Fri Aug 26 11:01:54 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.755291	107.205859	0.000000
0.759996	121.207729	0.005005
0.678902	113.384175	0.010010
0.665433	110.336719	0.015014
0.668597	102.117248	0.020019
0.761509	104.820588	0.025024
0.351230	108.836104	0.030029
0.516716	84.333304	0.035034
0.233621	81.656854	0.040038
-0.621324	80.372867	0.045043
-0.739455	64.067006	0.050048
-1.172190	61.534076	0.055053
-1.165505	47.559393	0.060058
-1.434425	45.700127	0.065062
-1.864948	41.107318	0.070067
-2.223211	36.952498	0.075072
-2.511329	24.602395	0.080077
-2.345963	23.279772	0.085082
-2.578818	21.987514	0.090086
-3.467897	28.099132	0.095091
-3.360422	17.541340	0.100096
-3.543571	22.555985	0.105101
-3.546295	19.035489	0.110106
-4.161301	11.804456	0.115110
-4.652725	10.444893	0.120115
-4.884066	4.201295	0.125120
-5.615125	12.078927	0.130125
-5.730895	6.282390	0.135130
-5.720541	16.274958	0.140134
-5.858103	12.462255	0.145139
-5.477095	7.853829	0.150144
-6.246807	7.486690	0.155149
-6.601946	10.180685	0.160154
-6.706593	2.509539	0.165158
-6.843220	2.616450	0.170163
-7.573918	9.361440	0.175168
-8.259965	19.225163	0.180173
-8.024983	5.173842	0.185178
-8.412643	8.160792	0.190182
-8.534631	10.514776	0.195187
-8.273968	1.707949	0.200192
-8.647256	10.475806	0.205197
-9.228911	3.476857	0.210202
-9.419374	8.334455	0.215206
-9.862240	12.380332	0.220211
-9.541887	2.770136	0.225216
-9.970468	8.481028	0.230221
-10.464724	3.809571	0.235226
-11.064015	8.506203	0.240230
-11.369062	12.672986	0.245235
-11.106640	12.565911	0.250240
-11.299420	9.195226	0.255245
-11.149036	9.731997	0.260250
-11.617032	10.010720	0.265254
-12.596279	2.703530	0.270259
-12.706068	5.321360	0.275264
-12.904762	7.351941	0.280269
-12.754093	9.030743	0.285274
-12.838380	9.319324	0.290278
-13.208526	13.107114	0.295283
-13.628324	9.629411	0.300288
-14.233968	14.187834	0.305293
-14.482210	14.109650	0.310298
-14.424733	14.123066	0.315302
-14.423379	10.595609	0.320307
-15.058108	-4.291531	0.325312
-15.736635	10.313319	0.330317
-15.584135	-3.038642	0.335322
-15.896737	1.028078	0.340326
-16.137051	8.683772	0.345331
-16.310333	-4.294773	0.350336
-16.350091	3.427766	0.355341
-16.234479	-1.117190	0.360346
-16.945350	7.212861	0.365350
-17.293479	1.072867	0.370355
-17.170073	6.239087	0.375360
-17.854732	10.395374	0.380365
-17.377478	7.511968	0.385370
-17.959185	6.460683	0.390374
-18.795002	3.534957	0.395379
-18.694065	5.180375	0.400384
-19.182508	14.870965	0.405389
-19.039587	12.096560	0.410394
-19.392406	7.624535	0.415398
-20.073716	15.820278	0.420403
-20.515070	19.033881	0.425408
-20.655849	19.103475	0.430413
-20.396042	7.047713	0.435418
-20.547623	8.779903	0.440422
-20.341129	10.722087	0.445427
-21.101452	7.563151	0.450432
-21.803474	12.165052	0.455437
-21.837963	-4.584022	0.460442
-22.003552	3.297308	0.465446
-22.199674	8.563897	0.470451
-21.702144	-1.016937	0.475456
-22.730570	8.017431	0.480461
-22.868450	-0.281268	0.485466
-23.093308	3.066298	0.490470
-23.430228	0.689297	0.495475
-23.623417	-3.766451	0.500480
-24.701190	6.639130	0.505485
-24.661305	0.448214	0.510490
-24.654766	4.133062	0.515494
-24.644794	5.023877	0.520499
-24.604053	-0.303497	0.525504
-25.017851	13.643227	0.530509
-25.129731	3.521382	0.535514
-25.640018	8.476230	0.540518
-26.073419	7.389199	0.545523
-26.068546	10.973071	0.550528
-26.252734	9.534037	0.555533
-26.504696	6.419332	0.560538
-27.177122	8.045961	0.565542
-27.680893	17.131519	0.570547
-27.568724	4.450199	0.575552
-27.925646	4.145336	0.580557
-28.085309	6.400785	0.585562
-27.960809	11.940146	0.590566
-28.464560	17.988601	0.595571
-28.613811	3.066995	0.600576
-29.339368	5.268189	0.605581
-29.110022	11.442936	0.610586
-29.501733	5.249617	0.615590
-29.595166	6.479225	0.620595
-30.012713	1.147278	0.625600
-30.451651	8.580805	0.630605
-30.650622	5.410396	0.635610
-30.785266	5.232270	0.640614
-30.711763	5.559556	0.645619
-30.716709	7.341678	0.650624
-31.855991	3.412871	0.655629
-32.184098	8.310881	0.660634
-32.298172	10.733233	0.665638
-32.274572	7.521842	0.670643
-32.386897	10.089449	0.675648
-32.742314	12.365886	0.680653
-32.306429	11.102381	0.685658
-33.161895	10.938414	0.690662
-33.433851	15.027280	0.695667
-33.642498	13.636345	0.700672
-33.902469	14.553373	0.705677
-34.206682	10.905819	0.710682
-34.753338	10.820316	0.715686
-35.194502	21.228022	0.720691
-35.209805	10.493208	0.725696
-35.180469	6.958232	0.730701
-34.967459	7.200523	0.735706
-35.369572	3.397378	0.740710
-36.267730	11.674335	0.745715
-36.319246	-3.173899	0.750720
-36.912450	4.732883	0.755725
-36.568970	4.524605	0.760730
-37.024124	11.188729	0.765734
-36.934084	16.170327	0.770739
-37.299650	11.317486	0.775744
-37.696340	4.397305	0.780749
-37.875857	10.360474	0.785754
-37.829413	12.485760	0.790758
-38.952033	7.048463	0.795763
-39.126824	8.278083	0.800768
-39.349113	10.169973	0.805773
-39.430503	2.545826	0.810778
-39.614166	10.800120	0.815782
-39.554251	9.139588	0.820787
-39.392549	4.362836	0.825792
-40.206817	16.410454	0.830797
-40.379305	7.035174	0.835802
-40.789705	0.104475	0.840806
-41.219818	7.517646	0.845811
-40.753280	-2.349417	0.850816
-41.731291	5.962117	0.855821
-42.224814	12.423414	0.860826
-41.977829	3.656682	0.865830
-42.370189	11.035503	0.870835
-42.326018	6.343487	0.875840
-42.437091	7.490422	0.880845
-42.995772	6.846826	0.885850
-43.320160	1.987577	0.890854
-43.844732	1.737289	0.895859
-44.126765	10.788318	0.900864
-43.864042	12.990657	0.905869
-43.798811	8.627545	0.910874
-44.623110	11.619206	0.915878
-45.213921	7.073511	0.920883
-45.299743	1.028714	0.925888
-45.850933	17.148108	0.930893
-45.443030	8.546138	0.935898
-45.414357	6.121705	0.940902
-45.429343	15.336794	0.945907
-46.155632	10.767901	0.950912
-46.726610	14.802088	0.955917
-46.968022	13.795892	0.960922
-47.166773	10.650757	0.965926
-47.333108	20.066578	0.970931
-47.118490	9.776841	0.975936
-47.909198	16.360338	0.980941
-48.235267	3.089216	0.985946
-48.052430	4.693409	0.990950
-48.583347	3.222943	0.995955
-48.542066	-1.481275	1.000960
-48.949861	10.423959	1.005965
-50.112610	6.267861	1.010970
-49.781327	7.466140	1.015974
-50.209542	16.482986	1.020979
-50.095998	7.673756	1.025984
-50.022739	14.692190	1.030989
-49.858209	13.888536	1.035994
-50.152586	12.700768	1.040998
-51.338968	11.449412	1.046003
-51.273692	0.344567	1.051008
-51.952496	11.899706	1.056013
-51.967787	0.500532	1.061018
-51.599068	-0.075495	1.066022
-51.804836	-0.324801	1.071027
-52.456712	-0.175630	1.076032
-53.125799	4.171213	1.081037
-53.262125	3.101201	1.086042
-53.112659	6.694195	1.091046
-53.328347	5.063920	1.096051
-53.670221	8.201924	1.101056
-53.997230	6.905346	1.106061
-54.058745	14.852730	1.111066
-54.122687	9.646054	1.116070
-55.014276	12.464702	1.121075
-55.295282	8.775573	1.126080
-55.576377	14.270520	1.131085
-55.358472	16.897439	1.136090
-55.696965	15.422321	1.141094
-55.628007	10.457535	1.146099
-56.261797	3.400271	1.151104
-56.993554	12.638377	1.156109
-56.949212	2.881340	1.161114
-56.958849	-2.030078	1.166118
-57.435885	6.690655	1.171123
-57.125655	3.665583	1.176128
-57.724211	7.827445	1.181133
-57.857817	9.683381	1.186138
-58.130893	9.865319	1.191142
-58.474828	3.851220	1.196147
-59.224683	5.996088	1.201152
-59.347807	10.900146	1.206157
-59.472883	9.847364	1.211162
-59.769632	8.504948	1.216166
-60.347476	10.702125	1.221171
-60.047957	-0.492972	1.226176
-60.173168	5.585121	1.231181
-60.034742	2.950618	1.236186
-60.373923	1.152917	1.241190
-60.945715	7.329016	1.246195
-61.323813	7.267887	1.251200
-61.148839	-2.651850	1.256205
-61.932119	-0.732724	1.261210
-62.524068	2.893452	1.266214
-62.946652	4.778563	1.271219
-63.224720	3.597748	1.276224
-63.022298	7.160351	1.281229
-62.925359	11.397416	1.286234
-63.167728	10.631807	1.291238
-63.283791	11.064535	1.296243
-63.421580	7.789691	1.301248
-64.144504	15.492055	1.306253
-64.395009	9.564644	1.311258
-64.270544	3.120123	1.316262
-64.504026	14.596435	1.321267
-64.795603	4.638609	1.326272
-65.635029	14.700209	1.331277
-65.898224	15.291882	1.336282
-65.757172	9.113687	1.341286
-65.647257	6.043876	1.346291
-66.141247	7.345341	1.351296
-67.044222	15.683158	1.356301
-67.181011	2.268678	1.361306
-67.244457	10.225850	1.366310
-67.644465	21.642677	1.371315
-67.199750	8.564743	1.376320
-67.379384	10.956175	1.381325
-67.872734	8.413711	1.386330
-68.367491	11.259154	1.391334
-68.781909	5.841303	1.396339
-68.673212	-2.084510	1.401344
-69.224032	8.498443	1.406349
-69.402179	11.351535	1.411354
-69.408475	5.332320	1.416358
-69.930541	5.999100	1.421363
-70.458470	4.461733	1.426368
-70.823309	-3.858569	1.431373
-70.510286	5.492097	1.436378
-70.367910	11.449437	1.441382
-70.741603	5.832263	1.446387
-71.100209	-5.522942	1.451392
-71.946257	0.259273	1.456397
-72.283909	-10.555045	1.461402
-72.449713	-0.658446	1.466406
-72.286558	4.036526	1.471411
-71.933431	-8.948043	1.476416
-72.717458	6.559045	1.481421
-73.123130	-4.330105	1.486426
-73.116228	-12.306499	1.491430
-73.666122	-5.051849	1.496435
-73.617076	-4.502465	1.501440
-74.402547	9.619175	1.506445
-74.684917	-1.143646	1.511450
-74.912578	0.214423	1.516454
-75.178471	9.016172	1.521459
-74.772431	-7.988137	1.526464
-75.179184	0.658376	1.531469
-75.104021	-0.438236	1.536474
-75.912146	-1.875030	1.541478
-76.462407	1.200508	1.546483
-76.355421	1.405525	1.551488
-76.754537	1.641888	1.556493
-76.691399	6.374579	1.561498
-76.871828	4.802088	1.566502
-77.547053	11.949713	1.571507
-77.457619	5.029773	1.576512
-78.185996	6.380386	1.581517
-77.829583	6.951514	1.586522
-77.903981	4.669676	1.591526
-78.421960	4.497454	1.596531
-78.935161	2.059319	1.601536
-79.262863	6.950937	1.606541
-79.513534	4.611127	1.611546
-79.474034	1.530135	1.616550
-80.198342	12.121119	1.621555
-80.477851	-5.418671	1.626560
-80.815460	-2.784353	1.631565
-80.744198	-0.156751	1.636570
-80.817241	0.854553	1.641574
-81.096398	5.118538	1.646579
-80.470154	1.028734	1.651584
-81.428140	11.064500	1.656589
-81.948438	9.760054	1.661594
-82.217269	10.953698	1.666598
-82.614778	15.289895	1.671603
-82.365532	4.257642	1.676608
-82.583912	6.148923	1.681613
-83.540506	2.489059	1.686618
-83.712299	4.449013	1.691622
-84.114475	2.050538	1.696627
-84.158828	-1.159761	1.701632
-84.519877	-2.216928	1.706637
-84.467532	-2.054021	1.711642
-83.870212	-3.833026	1.716646
-84.475718	1.320136	1.721651
-84.923320	-3.678107	1.726656
-85.535196	2.004375	1.731661
-85.534842	0.049409	1.736666
-85.734688	-4.898828	1.741670
-85.690787	4.863885	1.746675
-86.702713	7.729742	1.751680
-86.805317	10.425544	1.756685
-86.993439	5.181260	1.761690
-87.017201	4.517651	1.766694
-87.546647	7.608931	1.771699
-87.324343	7.365738	1.776704
-88.150105	7.013656	1.781709
-88.171667	6.450941	1.786714
-88.403083	-3.509919	1.791718
-88.756637	5.536423	1.796723
-88.450801	2.195671	1.801728
-88.811084	0.692311	1.806733
-89.503166	-4.014774	1.811738
-89.532396	-4.459240	1.816742
-89.746694	2.360359	1.821747
-89.828711	3.749534	1.826752
-90.359198	8.511380	1.831757
-91.269786	-3.276718	1.836762
-91.504904	0.173680	1.841766
-91.520936	3.770294	1.846771
-91.235576	-1.493927	1.851776
-91.788747	4.274325	1.856781
-91.459394	5.545667	1.861786
-91.846596	0.237473	1.866790
-92.230997	5.403664	1.871795
-92.448918	-0.889471	1.876800
-92.916637	-1.623156	1.881805
-92.699474	-2.741878	1.886810
-93.350259	3.006772	1.891814
-93.898849	-1.232291	1.896819
-93.911057	0.930597	1.901824
-94.343720	8.537145	1.906829
-94.286799	5.972278	1.911834
-94.308517	7.867739	1.916838
-95.330810	12.696670	1.921843
-95.201590	0.348051	1.926848
-96.038273	7.115867	1.931853
-95.796987	4.041421	1.936858
-95.961218	5.044777	1.941862
-96.440633	3.499858	1.946867
-95.922264	-1.199551	1.951872
-96.192862	10.640027	1.956877
-96.885056	6.638449	1.961882
-97.491112	3.971172	1.966886
-97.267585	2.974841	1.971891
-97.678705	5.231477	1.976896
-97.589859	8.900345	1.981901
-98.357696	3.594470	1.986906
-98.699127	-8.570133	1.991910
-99.005771	8.713354	1.996915
-98.947410	-0.195030	2.006912
-98.880831	1.480256	2.016909
-97.991888	10.433567	2.026906
-98.019349	9.836420	2.036902
-97.129539	5.691181	2.046899
-96.590494	2.829623	2.056896
-96.274304	4.453373	2.066893
-95.286198	-3.768151	2.076890
-95.007896	-0.402607	2.086886
-95.043640	3.119538	2.096883
-94.229309	8.961120	2.106880
-93.725230	6.086000	2.116877
-93.166828	10.025635	2.126874
-92.617409	8.971214	2.136870
-92.039475	5.615776	2.146867
-91.894137	8.374821	2.156864
-91.084545	-1.602321	2.166861
-90.797804	7.216679	2.176858
-90.313846	7.686609	2.186854
-89.909651	8.659951	2.196851
-89.128114	5.662437	2.206848
-88.157694	5.201347	2.216845
-88.268475	3.198046	2.226842
-88.000786	6.992884	2.236838
-87.198397	6.089137	2.246835
-86.833152	-1.088268	2.256832
-85.685147	4.074157	2.266829
-85.525746	10.692433	2.276826
-85.433408	6.357760	2.286822
-84.749130	4.759672	2.296819
-83.995462	12.685542	2.306816
-83.926541	11.189601	2.316813
-83.017753	3.126137	2.326810
-82.534580	0.697750	2.336806
-82.365005	2.642091	2.346803
-81.383570	5.327974	2.356800
-80.875226	10.944780	2.366797
-80.875917	11.315947	2.376794
-79.904397	10.024749	2.386790
-79.363884	11.619909	2.396787
-79.441953	5.350965	2.406784
-78.654841	5.022950	2.416781
-78.018413	5.811251	2.426778
-78.272986	8.290453	2.436774
-77.208786	4.954333	2.446771
-76.527774	6.511778	2.456768
-75.617699	1.739349	2.466765
-75.383463	5.080080	2.476762
-75.203422	-2.306066	2.486758
-75.162606	4.552411	2.496755
-74.151416	7.252668	2.506752
-73.504166	1.235077	2.516749
-72.942744	2.041392	2.526746
-72.526183	6.256528	2.536742
-72.362038	6.199733	2.546739
-71.530128	2.830092	2.556736
-70.955485	0.815101	2.566733
-70.932208	3.475947	2.576730
-70.168902	8.761627	2.586726
-69.905464	6.082358	2.596723
-68.723497	8.125655	2.606720
-68.065183	11.995885	2.616717
-67.858661	5.964553	2.626714
-67.613095	11.346685	2.636710
-67.606480	12.774725	2.646707
-66.892648	12.077997	2.656704
-66.071059	3.210843	2.666701
-64.934728	8.999125	2.676698
-64.770434	9.300257	2.686694
-64.878251	11.861143	2.696691
-64.573491	7.471220	2.706688
-63.628115	9.906136	2.716685
-63.029887	7.561200	2.726682
-62.108415	8.666238	2.736678
-62.047433	12.116307	2.746675
-61.915754	8.751156	2.756672
-61.168993	14.143949	2.766669
-60.272163	14.967731	2.776666
-60.191525	12.377110	2.786662
-59.756585	14.660260	2.796659
-59.193058	5.326455	2.806656
-58.775471	10.336524	2.816653
-57.859270	8.287358	2.826650
-57.496867	12.700990	2.836646
-57.332713	9.644385	2.846643
-56.249534	16.232870	2.856640
-56.134256	0.817193	2.866637
-55.999451	9.669357	2.876634
-55.547685	7.939583	2.886630
-54.324494	5.627216	2.896627
-53.746594	-0.008956	2.906624
-53.643040	5.021497	2.916621
-53.340791	6.976860	2.926618
-52.790211	8.975918	2.936614
-52.165576	8.403947	2.946611
-51.237738	5.038376	2.956608
-50.946015	2.079115	2.966605
-50.747119	4.250134	2.976602
-49.817801	12.104311	2.986598
-49.351800	9.197106	2.996595
-49.202559	3.782891	3.006592
-48.684907	4.044843	3.016589
-47.827249	4.548452	3.026586
-47.835700	6.916476	3.036582
-46.735291	1.474538	3.046579
-46.447987	3.074278	3.056576
-46.555974	2.733581	3.066573
-45.527939	1.021785	3.076570
-45.309203	5.812567	3.086566
-44.254463	3.510590	3.096563
-43.842751	6.383380	3.106560
-43.540577	1.436346	3.116557
-43.058067	3.534698	3.126554
-42.145052	0.706776	3.136550
-41.839379	7.869297	3.146547
-41.941508	6.111728	3.156544
-41.008241	4.221458	3.166541
-40.260407	7.412535	3.176538
-40.206614	4.430132	3.186534
-39.640604	5.913622	3.196531
-38.918050	4.290569	3.206528
-38.749952	4.755828	3.216525
-37.686857	4.061740	3.226522
-37.475423	8.232791	3.236518
-37.122162	5.244942	3.246515
-36.707711	6.964264	3.256512
-35.836540	4.161864	3.266509
-35.716661	0.817558	3.276506
-34.421990	7.354107	3.286502
-34.579621	-0.834745	3.296499
-34.165779	7.264410	3.306496
-33.895869	7.409719	3.316493
-32.967545	10.113378	3.326490
-32.508327	10.761385	3.336486
-31.723489	8.707331	3.346483
-31.243222	14.920872	3.356480
-31.098722	10.213789	3.366477
-30.862058	7.947322	3.376474
-30.115960	4.600545	3.386470
-29.538847	4.973612	3.396467
-29.192789	7.619047	3.406464
-28.439648	-0.356829	3.416461
-27.771391	1.934341	3.426458
-26.989105	5.237259	3.436454
-26.827593	-4.721341	3.446451
-26.675374	-4.035038	3.456448
-26.399861	-3.269734	3.466445
-25.511563	4.419773	3.476442
-25.040148	-1.041435	3.486438
-24.332779	-3.314668	3.496435
-23.967567	0.541011	3.506432
-23.643707	4.666049	3.516429
-22.709464	4.647736	3.526426
-22.684444	6.193283	3.536422
-22.231826	3.988224	3.546419
-21.418289	3.871500	3.556416
-20.915348	-2.364368	3.566413
-20.384032	2.064144	3.576410
-19.402510	3.913746	3.586406
-19.385636	-0.573898	3.596403
-19.366946	1.609340	3.606400
-18.884848	-6.083588	3.616397
-17.988017	3.717443	3.626394
-17.150400	4.211503	3.636390
-16.626902	-1.251480	3.646387
-16.313172	-0.029642	3.656384
-16.408694	3.432123	3.666381
-15.432449	4.284722	3.676378
-14.948669	0.117175	3.686374
-14.821914	0.221419	3.696371
-13.492434	-2.037805	3.706368
-13.309713	2.502001	3.716365
-13.093382	-1.779121	3.726362
-12.508859	-0.238328	3.736358
-11.855421	3.889246	3.746355
-11.700048	-2.568095	3.756352
-10.539885	4.499397	3.766349
-10.469089	-6.708989	3.776346
-10.071650	0.375889	3.786342
-9.519783	-0.811954	3.796339
-8.632321	1.403907	3.806336
-8.593731	3.080385	3.816333
-7.949105	-4.986297	3.826330
-7.777953	6.384863	3.836326
-7.291440	4.950612	3.846323
-6.595546	3.426742	3.856320
-5.840681	9.996658	3.866317
-5.138486	16.707821	3.876314
-4.948515	21.148306	3.886310
-4.834191	15.210516	3.896307
-4.440564	18.564448	3.906304
-3.731116	32.465165	3.916301
-3.312999	50.180821	3.926298
-2.581552	51.654396	3.936294
-2.073548	62.871779	3.946291
-1.788972	72.850538	3.956288
-1.431932	83.473736	3.966285
-1.060327	98.893757	3.976282
-0.694368	115.084426	3.986278
0.000000	127.967764	3.991283
0.140452	135.089679	3.996288
0.480951	140.968764	4.001293
0.550386	147.310824	4.006298
0.386302	141.638821	4.011302
0.654032	147.883569	4.016307
0.804092	160.663807	4.021312
1.027851	155.782441	4.026317
1.006726	169.335965	4.031322
1.109437	154.156705	4.036326
0.880420	150.544869	4.041331
0.693900	148.141266	4.046336
1.040750	142.180909	4.051341
0.845296	151.427334	4.056346
0.895878	146.582425	4.061350
1.094452	161.835429	4.066355
0.588196	154.305838	4.071360
1.321972	155.473098	4.076365
0.939788	152.622245	4.081370
1.233145	160.150622	4.086374
0.795677	150.784883	4.091379
0.925055	157.753511	4.096384
0.895962	158.292922	4.101389
0.892183	162.887384	4.106394
1.122025	157.846887	4.111398
1.356586	156.880466	4.116403
1.204927	169.888017	4.121408
1.448165	163.788765	4.126413
0.899898	157.078778	4.131418
0.849104	143.337590	4.136422
1.071394	155.546608	4.141427
1.212695	174.481564	4.146432
1.490614	164.852577	4.151437
1.067750	169.379417	4.156442
1.166645	162.476920	4.161446
1.228883	165.843090	4.166451
1.095189	166.936611	4.171456
1.442889	164.851616	4.176461
1.118078	172.697703	4.181466
1.108528	169.105475	4.186470
1.413043	169.545489	4.191475
1.348064	166.803429	4.196480
1.243358	153.665397	4.201485
1.457650	165.575119	4.206490
1.135741	156.681754	4.211494
1.321591	159.427579	4.216499
1.472364	165.851891	4.221504
1.540581	168.410394	4.226509
0.958402	162.619987	4.231514
1.262564	156.688417	4.236518
1.572533	167.020389	4.241523
1.550797	167.640910	4.246528
1.432285	165.176097	4.251533
1.156694	177.728399	4.256538
1.609502	166.784565	4.261542
1.713041	162.817235	4.266547
1.246315	164.573197	4.271552
1.536760	165.489953	4.276557
1.673820	168.461669	4.281562
1.362987	153.068394	4.286566
1.356285	161.364808	4.291571
1.198810	170.133942	4.296576
1.896351	159.930273	4.301581
1.396674	171.834106	4.306586
1.593012	168.829902	4.311590
1.625862	162.352129	4.316595
1.398152	165.988064	4.321600
1.446436	166.597683	4.326605
1.428910	174.883133	4.331610
1.508035	171.065132	4.336614
1.843099	171.952795	4.341619
1.508401	166.978047	4.346624
1.656878	159.767282	4.351629
1.568989	169.607558	4.356634
1.713755	170.246446	4.361638
1.429147	173.812150	4.366643
1.173130	169.302866	4.371648
1.660165	167.961786	4.376653
1.331847	173.815304	4.381658
1.468790	171.231625	4.386662
1.910422	188.215303	4.391667
1.856071	189.736223	4.396672
2.039817	179.963707	4.401677
1.711417	180.834450	4.406682
1.845724	172.800167	4.411686
1.637892	172.921328	4.416691
1.882015	182.637154	4.421696
2.292251	179.428806	4.426701
1.601032	183.279277	4.431706
1.780424	174.924769	4.436710
2.051091	169.938022	4.441715
1.772436	169.102126	4.446720
1.927001	168.372781	4.451725
1.810964	174.680454	4.456730
1.925637	183.612861	4.461734
2.212327	180.891973	4.466739
1.641243	175.422530	4.471744
2.010536	178.829477	4.476749
1.996671	190.085058	4.481754
2.363824	181.476691	4.486758
2.253735	179.962832	4.491763
2.033534	177.586615	4.496768
1.954721	166.273148	4.501773
1.655534	174.763800	4.506778
1.691859	184.496161	4.511782
2.094935	197.107320	4.516787
1.983175	197.862078	4.521792
2.251329	201.120266	4.526797
2.564051	198.657908	4.531802
2.381271	198.851098	4.536806
2.237988	180.309160	4.541811
2.048926	181.487231	4.546816
1.885483	172.170563	4.551821
2.009138	191.016537	4.556826
2.571323	188.198972	4.561830
2.314357	185.154614	4.566835
2.036203	188.463058	4.571840
2.293358	180.479245	4.576845
2.004306	184.782779	4.581850
2.483644	185.758708	4.586854
2.419828	189.910119	4.591859
1.832197	187.300050	4.596864
2.299653	184.373851	4.601869
1.974694	191.014608	4.606874
2.148277	197.922587	4.611878
2.704360	204.309117	4.616883
2.444920	202.138318	4.621888
2.642641	197.656455	4.626893
2.345389	193.055511	4.631898
2.760521	189.492067	4.636902
2.250876	182.728602	4.641907
2.073956	170.987491	4.646912
2.336166	181.415491	4.651917
2.383497	194.866629	4.656922
2.405103	194.366787	4.661926
2.347919	191.044556	4.666931
2.234528	197.421427	4.671936
2.351443	191.791076	4.676941
2.222919	200.555717	4.681946
2.265119	195.534934	4.686950
2.226191	193.228565	4.691955
2.234081	199.789029	4.696960
2.415698	204.139506	4.701965
2.371615	190.912916	4.706970
2.503829	192.211804	4.711974
2.629057	192.901191	4.716979
2.614730	200.793859	4.721984
2.617968	194.997713	4.726989
2.565103	206.626363	4.731994
2.471419	197.605696	4.736998
2.912434	210.897477	4.742003
2.698590	211.029066	4.747008
2.459674	195.045604	4.752013
2.586337	199.085104	4.757018
2.460609	210.405569	4.762022
3.057519	217.054660	4.767027
2.827026	214.458583	4.772032
2.987722	207.473682	4.777037
2.416841	204.810383	4.782042
2.762674	200.245349	4.787046
2.480411	197.616207	4.792051
2.900678	215.305573	4.797056
3.113581	208.122722	4.802061
2.697154	212.205655	4.807066
2.893337	214.231724	4.812070
2.585117	201.542949	4.817075
2.752641	215.639763	4.822080
3.212398	222.971420	4.827085
2.712977	214.627672	4.832090
3.145347	213.472266	4.837094
2.808424	207.583549	4.842099
2.648475	208.004133	4.847104
3.096580	207.115190	4.852109
2.912154	214.888819	4.857114
2.733820	206.833597	4.862118
3.071907	217.974287	4.867123
2.757239	225.473976	4.872128
3.008037	215.409433	4.877133
3.188539	228.855681	4.882138
3.109903	218.687407	4.887142
3.249726	222.996941	4.892147
2.750997	212.198067	4.897152
2.861518	208.419461	4.902157
2.794883	217.351641	4.907162
3.010085	220.368146	4.912166
3.228586	221.716876	4.917171
2.967150	221.393977	4.922176
3.124236	221.198900	4.927181
2.862831	218.455778	4.932186
3.310988	219.180306	4.937190
3.080205	224.670650	4.942195
3.202583	228.916464	4.947200
3.062812	215.998976	4.952205
3.139753	227.487209	4.957210
3.287994	222.895987	4.962214
3.003122	230.201218	4.967219
3.050837	227.232799	4.972224
3.204058	218.898164	4.977229
2.752434	219.822895	4.982234
2.858526	220.186239	4.987238
3.067958	224.877232	4.992243
2.722575	226.687072	4.997248
3.395810	238.085634	5.002253
3.454114	255.110076	5.007258
3.217934	237.512668	5.012262
3.556040	239.396423	5.017267
3.396516	247.115570	5.022272
3.628539	244.153252	5.027277
3.209412	239.052427	5.032282
3.035107	235.590239	5.037286
3.544717	239.285393	5.042291
3.398763	244.094997	5.047296
3.655111	244.805098	5.052301
3.019436	245.208005	5.057306
3.501196	239.198138	5.062310
3.660808	262.258949	5.067315
3.636240	255.033960	5.072320
3.375531	245.321117	5.077325
3.094261	250.142300	5.082330
3.298453	249.016092	5.087334
3.915339	247.240345	5.092339
3.459498	248.232172	5.097344
3.411462	247.199017	5.102349
3.084843	245.576500	5.107354
3.108800	245.304076	5.112358
3.307198	237.968451	5.117363
3.407887	250.639384	5.122368
4.076845	244.220726	5.127373
3.790785	251.111707	5.132378
3.776152	248.678165	5.137382
3.811654	245.689499	5.142387
3.441824	244.067381	5.147392
3.616980	238.611442	5.152397
3.574044	241.105005	5.157402
3.664359	242.141508	5.162406
3.903304	241.633135	5.167411
3.309063	246.442936	5.172416
3.955076	243.884387	5.177421
3.628225	246.368374	5.182426
3.422397	247.836955	5.187430
3.868681	237.514177	5.192435
3.869502	246.416887	5.197440
3.579060	245.133579	5.202445
3.648216	247.315467	5.207450
3.565876	242.197005	5.212454
3.936436	256.588098	5.217459
3.695070	256.008979	5.222464
4.174893	248.515639	5.227469
3.846787	246.646585	5.232474
3.674299	244.481224	5.237478
3.924191	251.886697	5.242483
3.964567	248.368935	5.247488
3.838309	248.312885	5.252493
4.059611	254.140965	5.257498
3.990877	259.122045	5.262502
3.939125	246.007337	5.267507
3.794772	250.617382	5.272512
4.056712	256.442299	5.277517
3.977749	253.575856	5.282522
3.924739	253.913353	5.287526
4.011245	272.648141	5.292531
4.297146	269.152258	5.297536
4.087168	253.401514	5.302541
3.794426	257.360798	5.307546
4.198041	268.472335	5.312550
4.307611	247.299896	5.317555
3.730798	246.415508	5.322560
4.426822	259.847951	5.327565
4.243932	257.469078	5.332570
4.421244	242.986794	5.337574
4.212165	242.165371	5.342579
4.063664	247.563819	5.347584
4.024778	240.670089	5.352589
3.958574	253.885854	5.357594
3.969917	244.532443	5.362598
4.410142	264.556717	5.367603
4.139076	263.333664	5.372608
4.456045	256.457288	5.377613
4.495098	252.370267	5.382618
4.022250	262.071219	5.387622
3.825886	250.829783	5.392627
4.049753	268.897788	5.397632
4.571783	268.130208	5.402637
4.752180	268.706606	5.407642
4.317759	260.950653	5.412646
4.152190	255.025749	5.417651
4.152001	262.732750	5.422656
4.476722	256.649253	5.427661
4.674706	262.151943	5.432666
4.256988	255.731634	5.437670
4.163261	255.800229	5.442675
4.168558	265.616559	5.447680
4.750170	264.700500	5.452685
4.080453	268.633060	5.457690
4.081003	268.427555	5.462694
4.497287	263.639568	5.467699
4.182778	268.671571	5.472704
4.569641	259.250193	5.477709
4.627233	271.266640	5.482714
4.775285	259.335672	5.487718
4.795866	266.887583	5.492723
4.616138	268.693781	5.497728
4.742263	264.590037	5.502733
4.811654	272.308354	5.507738
4.526121	267.208866	5.512742
4.409031	271.115495	5.517747
4.460926	264.720140	5.522752
4.587218	268.215559	5.527757
4.308624	268.537560	5.532762
4.313482	266.793829	5.537766
4.328303	267.639611	5.542771
4.201402	267.580496	5.547776
4.320882	261.111346	5.552781
4.285322	264.290285	5.557786
4.246278	283.873520	5.562790
4.767819	286.443715	5.567795
4.683159	296.900479	5.572800
5.030515	290.367365	5.577805
5.141587	287.420708	5.582810
4.517115	274.414133	5.587814
4.854912	268.986644	5.592819
4.755268	285.608609	5.597824
4.902122	282.504525	5.602829
4.736898	274.387120	5.607834
4.611846	289.500799	5.612838
5.069552	282.286131	5.617843
4.838946	292.351172	5.622848
5.057959	286.676421	5.627853
4.846108	275.956227	5.632858
4.654206	282.595283	5.637862
4.794075	290.245688	5.642867
4.766439	294.948301	5.647872
4.978131	291.476622	5.652877
5.134535	295.008486	5.657882
5.156800	301.123831	5.662886
5.237632	288.105506	5.667891
4.875620	282.850245	5.672896
4.983277	280.299584	5.677901
4.650532	278.700163	5.682906
4.916697	287.229392	5.687910
4.985725	291.170321	5.692915
5.196727	295.513081	5.697920
4.948392	293.429126	5.702925
4.918270	302.029802	5.707930
4.944269	295.961165	5.712934
4.983124	296.986701	5.717939
4.837546	299.970808	5.722944
5.174205	295.748858	5.727949
4.617148	299.951781	5.732954
5.107053	293.099083	5.737958
5.118608	296.188437	5.742963
4.978120	304.860081	5.747968
5.012948	293.569967	5.752973
5.210279	304.669353	5.757978
5.043161	300.124048	5.762982
5.200201	289.302119	5.767987
4.854599	303.766791	5.772992
5.144873	296.457965	5.777997
5.222531	302.868401	5.783002
5.276853	312.847963	5.788006
5.494712	296.400992	5.793011
5.192371	293.607285	5.798016
5.164406	289.100428	5.803021
5.425796	305.251755	5.808026
5.533772	302.277105	5.813030
5.511913	289.420298	5.818035
4.935318	287.877825	5.823040
5.259603	292.535135	5.828045
5.501270	308.888849	5.833050
5.441600	306.462311	5.838054
5.378250	303.890815	5.843059
5.322492	316.801286	5.848064
5.517221	308.014064	5.853069
5.536821	304.664038	5.858074
5.442478	299.316478	5.863078
5.483436	292.922816	5.868083
4.922041	299.581443	5.873088
5.232746	302.662185	5.878093
5.384906	310.177810	5.883098
5.527778	303.673364	5.888102
5.860498	301.112968	5.893107
5.711330	312.133432	5.898112
5.708697	302.424668	5.903117
5.722490	305.542147	5.908122
5.467957	306.632346	5.913126
5.505504	315.636938	5.918131
5.771695	319.183350	5.923136
5.826897	314.964089	5.928141
5.141526	309.240319	5.933146
5.447478	311.964304	5.938150
5.791754	309.664694	5.943155
5.537800	312.599240	5.948160
5.754287	313.907163	5.953165
5.186393	312.546827	5.958170
5.641171	313.763866	5.963174
5.382897	307.967271	5.968179
5.562887	313.434814	5.973184
5.465020	313.633766	5.978189
5.560576	310.195985	5.983194
5.505434	310.938769	5.988198
5.668840	310.973657	5.993203
5.436083	310.326757	5.998208
5.673215	328.889459	6.003213
5.916350	339.304703	6.008218
5.948212	332.444214	6.013222
5.775446	319.895614	6.018227
5.638736	322.726486	6.023232
5.627554	327.543603	6.028237
5.877216	337.771171	6.033242
5.733859	340.172817	6.038246
6.297234	328.990210	6.043251
5.959409	335.402073	6.048256
5.713059	317.980172	6.053261
5.590686	316.370139	6.058266
5.658294	311.573154	6.063270
5.756980	316.885681	6.068275
5.472066	321.909927	6.073280
5.908285	329.580646	6.078285
6.020387	323.716889	6.083290
5.801295	320.400860	6.088294
5.914553	318.871197	6.093299
5.749132	314.578720	6.098304
5.794915	313.543609	6.103309
5.867955	316.753105	6.108314
5.760962	317.405887	6.113318
5.743421	307.063538	6.118323
5.604765	315.931052	6.123328
5.704096	311.806159	6.128333
5.425548	318.037947	6.133338
5.966997	324.543856	6.138342
5.937373	302.554641	6.143347
6.080189	316.965425	6.148352
5.933952	311.401318	6.153357
6.091548	315.337954	6.158362
5.748626	315.859793	6.163366
5.955607	308.946738	6.168371
5.856921	317.646682	6.173376
5.799319	315.374842	6.178381
5.756925	325.359978	6.183386
5.937655	320.124604	6.188390
5.981165	319.349271	6.193395
5.746467	319.367050	6.198400
5.814397	311.352530	6.203405
5.943464	326.240016	6.208410
5.709370	320.335251	6.213414
5.851636	313.327868	6.218419
5.498138	325.139442	6.223424
5.735334	315.051651	6.228429
5.571592	330.345392	6.233434
5.801551	319.078664	6.238438
6.160132	307.254087	6.243443
5.619440	313.890514	6.248448
6.025299	308.512527	6.253453
5.821707	307.437151	6.258458
5.628667	315.920834	6.263462
5.837482	308.985347	6.268467
5.686760	318.610866	6.273472
5.876362	319.435765	6.278477
6.004671	317.827829	6.283482
5.491643	316.528552	6.288486
5.883359	310.915488	6.293491
5.709365	316.045848	6.298496
5.981515	313.251275	6.303501
6.040544	307.813395	6.308506
5.556936	321.442206	6.313510
5.814312	310.664751	6.318515
5.901663	321.493375	6.323520
5.771381	317.900932	6.328525
5.993492	316.540979	6.333530
5.564292	301.555140	6.338534
5.793153	306.635428	6.343539
5.664817	311.375870	6.348544
6.080014	312.412412	6.353549
5.765327	309.003704	6.358554
5.599135	311.184279	6.363558
5.695341	307.733742	6.368563
5.897117	314.874654	6.373568
5.615738	303.823589	6.378573
5.834087	314.704577	6.383578
5.793861	317.564718	6.388582
5.852259	304.382198	6.393587
5.643370	297.815467	6.398592
5.555380	302.922941	6.403597
5.791671	309.871819	6.408602
5.903798	319.181171	6.413606
6.156791	307.736860	6.418611
5.576825	299.424595	6.423616
5.806267	290.907218	6.428621
5.756908	295.951729	6.433626
5.693115	291.906022	6.438630
5.492882	294.835364	6.443635
5.464558	310.775544	6.448640
5.889276	310.567270	6.453645
6.074737	322.462604	6.458650
5.845066	308.138545	6.463654
6.029915	298.312009	6.468659
5.670333	293.986493	6.473664
5.749620	281.699228	6.478669
5.862156	289.762005	6.483674
5.706865	292.013646	6.488678
5.575690	292.138691	6.493683
5.603831	294.007438	6.498688
5.841328	303.904693	6.503693
5.856692	318.246737	6.508698
5.660957	311.750718	6.513702
6.111857	305.498864	6.518707
5.669900	297.797852	6.523712
5.585667	298.823570	6.528717
5.841001	301.780057	6.533722
5.745942	317.594596	6.538726
5.944658	307.911426	6.543731
5.597336	308.658573	6.548736
5.851896	303.943211	6.553741
5.806761	300.539991	6.558746
5.694172	299.089785	6.563750
5.559660	292.593731	6.568755
5.783282	306.008014	6.573760
5.984774	311.358316	6.578765
5.935140	295.936904	6.583770
5.469072	300.220571	6.588774
5.917390	299.559378	6.593779
5.769513	311.000412	6.598784
5.630964	299.496848	6.603789
5.709428	303.866574	6.608794
5.456617	314.166034	6.613798
5.796241	311.519141	6.618803
5.803188	321.680088	6.623808
5.665979	313.286225	6.628813
5.710178	321.210963	6.633818
5.943505	316.717199	6.638822
5.953905	322.758469	6.643827
5.837279	322.735720	6.648832
5.776611	323.162994	6.653837
5.668770	316.934857	6.658842
6.228826	319.037159	6.663846
5.970133	301.854474	6.668851
5.585271	302.626448	6.673856
5.529197	307.377783	6.678861
5.657662	314.890772	6.683866
5.715693	320.456398	6.688870
6.131881	313.719573	6.693875
5.852097	304.623425	6.698880
5.764767	309.268898	6.703885
5.785652	300.989630	6.708890
5.653541	301.484974	6.713894
5.526164	299.587824	6.718899
5.595988	303.440049	6.723904
5.793561	313.197994	6.728909
6.045576	316.360642	6.733914
5.871309	310.459219	6.738918
5.843641	299.355999	6.743923
5.280139	306.366128	6.748928
5.761927	312.748446	6.753933
6.101496	322.006569	6.758938
5.624004	302.817361	6.763942
5.757840	301.306641	6.768947
5.954021	305.484036	6.773952
5.874698	295.616376	6.778957
5.903835	300.639176	6.783962
5.432521	289.896096	6.788966
5.804206	296.896654	6.793971
5.425820	306.589250	6.798976
5.561063	310.197176	6.803981
6.036279	312.784079	6.808986
6.191387	313.332779	6.813990
5.764667	297.245589	6.818995
6.024109	295.848189	6.824000
5.720187	298.145117	6.829005
5.793663	284.827389	6.834010
5.580600	293.472363	6.839014
5.957716	290.683597	6.844019
5.787010	298.888553	6.849024
5.879847	290.810054	6.854029
6.007280	297.171610	6.859034
5.828935	293.422143	6.864038
5.619495	306.185694	6.869043
5.623780	298.083015	6.874048
5.736807	298.945145	6.879053
5.543646	299.953022	6.884058
5.572419	296.054250	6.889062
5.956195	299.243835	6.894067
5.544014	296.970257	6.899072
5.749617	291.525379	6.904077
5.795474	294.846669	6.909082
5.477332	298.136049	6.914086
6.088088	303.697869	6.919091
6.004326	303.780731	6.924096
5.967510	302.179524	6.929101
5.788171	296.987565	6.934106
5.628943	298.964578	6.939110
5.519620	292.698716	6.944115
5.344570	295.010380	6.949120
5.609739	305.532902	6.954125
5.898168	310.278056	6.959130
5.814363	315.378555	6.964134
5.810661	317.457902	6.969139
5.883543	320.768662	6.974144
6.065774	306.314034	6.979149
5.798630	304.963820	6.984154
5.899089	301.155123	6.989158
5.741768	296.529202	6.994163
5.496687	304.021253	6.999168
5.403345	303.105879	7.004173
5.527747	311.454715	7.009178
5.581190	317.615830	7.014182
5.877117	319.803549	7.019187
5.753545	321.234019	7.024192
5.997714	322.075732	7.029197
6.050895	320.400401	7.034202
5.675176	329.690804	7.039206
5.538805	324.767388	7.044211
5.733282	323.990695	7.049216
6.084475	324.584794	7.054221
5.924831	326.106302	7.059226
5.632883	314.104601	7.064230
5.775601	316.702144	7.069235
5.964103	319.725987	7.074240
5.671770	306.136173	7.079245
5.758597	306.432917	7.084250
5.493069	305.281764	7.089254
5.719523	309.599976	7.094259
5.688796	321.127179	7.099264
5.719336	316.481494	7.104269
5.987952	316.465201	7.109274
5.908466	311.425366	7.114278
5.751734	306.694948	7.119283
5.508929	317.783778	7.124288
5.869102	318.857361	7.129293
6.064397	313.227423	7.134298
5.767975	313.390852	7.139302
5.590919	298.701110	7.144307
5.740272	309.899716	7.149312
6.020575	314.171581	7.154317
5.650984	306.060672	7.159322
5.252858	312.776140	7.164326
5.787546	316.932469	7.169331
5.871487	322.785123	7.174336
6.076818	320.886789	7.179341
6.002775	310.967680	7.184346
5.648053	311.288880	7.189350
5.980256	304.827721	7.194355
5.485869	298.843269	7.199360
5.754389	309.096358	7.204365
5.821868	314.635202	7.209370
5.595432	315.929830	7.214374
6.027775	313.980333	7.219379
6.067066	306.846620	7.224384
5.743267	300.218686	7.229389
5.964846	303.566400	7.234394
5.614642	297.853724	7.239398
5.813546	296.801100	7.244403
5.818937	305.570253	7.249408
5.864713	299.403625	7.254413
5.883536	299.321821	7.259418
5.690519	298.111924	7.264422
5.414687	301.486464	7.269427
5.205366	303.075815	7.274432
5.501950	313.169515	7.279437
5.794875	320.074779	7.284442
5.980071	326.493789	7.289446
5.981930	319.596849	7.294451
5.784099	332.731928	7.299456
5.690607	323.110064	7.304461
6.054393	321.032038	7.309466
5.793286	310.395421	7.314470
5.777042	305.393197	7.319475
5.534707	306.962378	7.324480
5.635292	320.914676	7.329485
6.144624	324.318830	7.334490
5.913338	319.229864	7.339494
5.615259	301.050418	7.344499
5.631776	302.149033	7.349504
5.786786	304.393490	7.354509
5.691094	306.034751	7.359514
5.462815	315.947585	7.364518
6.300457	306.057371	7.369523
5.766486	310.617364	7.374528
5.744234	301.762690	7.379533
5.780097	299.982492	7.384538
5.646484	300.050970	7.389542
5.696997	306.070172	7.394547
5.582262	307.410682	7.399552
6.000881	312.537356	7.404557
6.173902	309.641161	7.409562
5.999272	299.747210	7.414566
6.087733	297.417829	7.419571
5.547964	306.714780	7.424576
5.442229	299.920019	7.429581
5.512732	297.052443	7.434586
5.540883	308.121225	7.439590
6.119316	300.058863	7.444595
6.031946	298.993866	7.449600
5.857031	302.536188	7.454605
6.113324	296.286164	7.459610
5.627282	309.636940	7.464614
6.006190	292.968748	7.469619
5.935987	297.456530	7.474624
6.068911	294.550762	7.479629
5.807396	294.379731	7.484634
5.648669	306.078711	7.489638
5.875375	295.097237	7.494643
5.873057	311.134607	7.499648
5.747875	292.197436	7.504653
6.110627	300.123186	7.509658
5.970315	300.936176	7.514662
6.142771	303.459486	7.519667
5.969096	295.729359	7.524672
5.654314	286.508958	7.529677
5.443366	280.417108	7.534682
5.683558	302.291694	7.539686
6.029847	293.607430	7.544691
5.755945	304.485962	7.549696
5.876291	301.218326	7.554701
6.032346	290.864776	7.559706
5.721281	278.499086	7.564710
5.800951	274.453192	7.569715
5.520673	272.994296	7.574720
5.287079	278.099123	7.579725
5.645888	296.051235	7.584730
5.539901	298.981722	7.589734
5.816661	295.756172	7.594739
5.792769	300.046922	7.599744
5.790662	298.721881	7.604749
6.111757	304.828664	7.609754
5.843881	298.508394	7.614758
5.989891	299.453972	7.619763
5.750524	300.662029	7.624768
5.806294	297.667035	7.629773
5.921631	303.774217	7.634778
5.542191	296.490571	7.639782
5.992664	292.377449	7.644787
5.473128	289.086058	7.649792
5.746405	294.327103	7.654797
5.790413	294.484984	7.659802
5.840726	301.975334	7.664806
6.061838	295.319508	7.669811
5.449263	289.397752	7.674816
5.565686	291.401448	7.679821
5.691621	294.969692	7.684826
5.487074	300.307281	7.689830
5.509447	300.845010	7.694835
5.423758	303.709064	7.699840
5.813142	298.254552	7.704845
5.768326	292.927756	7.709850
5.826651	304.121549	7.714854
5.966664	300.977399	7.719859
5.620958	305.141089	7.724864
5.688848	305.140230	7.729869
5.824874	295.172603	7.734874
5.594849	306.433439	7.739878
5.889317	304.461118	7.744883
5.752925	303.226586	7.749888
5.855764	304.093466	7.754893
5.837112	301.119550	7.759898
5.411050	303.878414	7.764902
5.937744	305.150692	7.769907
5.854214	302.838599	7.774912
5.691259	304.980705	7.779917
6.105614	298.905383	7.784922
5.934057	299.593527	7.789926
5.857328	293.759180	7.794931
6.156301	300.147812	7.799936
6.084277	291.120562	7.804941
6.351812	284.473330	7.809946
5.797145	281.105155	7.814950
5.923557	277.286096	7.819955
5.432280	275.591138	7.824960
5.214921	279.532362	7.829965
5.707254	279.405308	7.834970
5.712181	297.251171	7.839974
6.063608	293.729262	7.844979
6.047651	290.941586	7.849984
5.609844	280.304025	7.854989
5.670478	278.089709	7.859994
5.082052	278.339730	7.864998
5.985846	285.820574	7.870003
5.914388	300.109684	7.875008
5.907372	298.095720	7.880013
6.079492	294.212595	7.885018
5.633421	288.951437	7.890022
5.822164	280.342328	7.895027
5.606647	279.528233	7.900032
6.031992	287.286047	7.905037
5.981248	277.088087	7.910042
5.341772	290.013492	7.915046
5.812877	274.871683	7.920051
5.802442	276.907783	7.925056
5.463109	275.189167	7.930061
6.265106	288.766482	7.935066
5.761823	281.274338	7.940070
5.975236	274.790557	7.945075
5.927045	283.074505	7.950080
5.401842	279.967493	7.955085
5.759281	275.141210	7.960090
5.682163	280.164729	7.965094
5.439206	269.898625	7.970099
5.448994	289.815943	7.975104
5.704882	305.604302	7.980109
5.915383	297.010780	7.985114
5.805286	304.301484	7.990118
6.142380	306.054643	7.995136
5.716473	298.705450	8.000154
5.891073	296.065627	8.005171
5.873191	286.320902	8.010189
5.583070	280.329584	8.015206
5.607735	283.456344	8.020224
5.779851	293.057579	8.025242
5.725529	293.949833	8.030259
6.152473	298.901027	8.035277
5.904096	287.065297	8.040294
5.940359	284.961380	8.045312
5.617758	268.425872	8.050330
5.510947	272.911084	8.055347
5.680742	280.736059	8.060365
5.677096	295.994297	8.065382
6.216555	289.810699	8.070400
6.142553	291.775774	8.075418
5.618642	288.998569	8.080435
5.840842	287.411626	8.085453
5.913211	301.436806	8.090470
5.924707	298.601483	8.095488
5.980025	292.398595	8.100506
5.831388	297.328957	8.105523
6.020833	281.041898	8.110541
5.426933	295.896604	8.115558
5.574894	291.777784	8.120576
5.947431	291.751558	8.125594
5.540539	291.931888	8.130611
5.831675	304.338885	8.135629
6.256250	300.337932	8.140646
5.965369	300.143614	8.145664
6.143493	305.001013	8.150682
5.829924	305.693804	8.155699
6.207549	291.854605	8.160717
6.260838	295.055800	8.165734
6.059013	290.432896	8.170752
5.903987	291.672169	8.175770
5.694874	295.422276	8.180787
6.107215	293.859373	8.185805
5.704636	302.309931	8.190822
6.046284	297.753878	8.195840
5.986735	303.112159	8.200858
5.874031	314.676374	8.205875
6.106933	301.740121	8.210893
5.928165	308.325571	8.215910
5.820562	311.614933	8.220928
5.853659	308.571129	8.225946
5.507229	309.748692	8.230963
5.959010	300.744987	8.235981
5.962324	305.717961	8.240998
6.015962	303.087503	8.246016
5.897314	303.226111	8.251034
5.989762	309.390658	8.256051
6.211590	306.838149	8.261069
6.249342	306.889293	8.266086
6.126048	303.058843	8.271104
6.001419	299.758748	8.276122
6.118461	305.502922	8.281139
6.261470	297.812700	8.286157
6.331380	304.135381	8.291174
6.053358	300.467870	8.296192
6.202476	305.799974	8.301210
6.034624	305.741127	8.306227
6.393654	301.927094	8.311245
5.971080	306.306852	8.316262
6.009474	308.711995	8.321280
5.952502	302.283604	8.326298
5.602330	306.667867	8.331315
6.125815	305.478957	8.336333
5.926095	308.624879	8.341350
6.219364	308.210230	8.346368
6.035099	307.822597	8.351386
6.081260	316.723973	8.356403
5.939194	300.813541	8.361421
5.923615	305.713722	8.366438
5.811516	305.374810	8.371456
5.956324	306.280239	8.376474
6.018341	322.825240	8.381491
6.117154	330.377282	8.386509
6.189824	330.751175	8.391526
6.178323	329.206926	8.396544
6.208049	322.424220	8.401562
6.161858	333.577327	8.406579
6.247355	332.254648	8.411597
6.261281	324.773851	8.416614
6.250621	326.467150	8.421632
6.549537	326.524966	8.426650
5.991378	324.223276	8.431667
6.214264	317.628237	8.436685
6.387288	330.119909	8.441702
6.416442	330.472177	8.446720
6.121042	316.213912	8.451738
5.791161	320.225811	8.456755
6.380656	331.825866	8.461773
6.265547	325.315004	8.466790
6.278598	324.076185	8.471808
6.567234	320.736986	8.476826
6.417879	327.103281	8.481843
6.412085	309.653765	8.486861
6.397412	304.398992	8.491878
6.272110	311.856540	8.496896
6.130140	310.512477	8.501914
6.065709	312.586511	8.506931
6.180539	316.551258	8.511949
6.204848	318.037151	8.516966
6.325352	321.562383	8.521984
6.409434	325.421473	8.527002
5.879793	326.188929	8.532019
5.970632	321.668764	8.537037
6.466280	318.404626	8.542054
6.259720	324.748270	8.547072
6.283876	319.266553	8.552090
6.143901	322.488378	8.557107
6.464052	323.921898	8.562125
6.252008	326.261901	8.567143
6.386547	317.118243	8.572160
6.316944	322.048929	8.577178
5.881726	328.828942	8.582195
6.426372	321.896641	8.587213
6.306677	323.701585	8.592231
6.100449	321.894181	8.597248
6.108535	327.592214	8.602266
6.364163	340.856785	8.607283
6.743834	341.536311	8.612301
6.745905	346.216016	8.617319
6.703001	339.031224	8.622336
6.596297	315.494418	8.627354
6.299695	327.169320	8.632371
6.549419	324.438905	8.637389
6.597699	322.257378	8.642407
6.039060	324.338936	8.647424
6.240240	313.244192	8.652442
6.179158	325.090694	8.657459
6.472098	339.665354	8.662477
6.585015	353.873600	8.667495
6.846731	343.413161	8.672512
6.850622	323.491262	8.677530
6.498240	330.794835	8.682547
6.494546	317.059165	8.687565
6.550567	320.143181	8.692583
6.520990	322.880784	8.697600
6.392559	320.982377	8.702618
6.114703	324.468653	8.707635
6.487886	331.492009	8.712653
6.549797	338.197779	8.717671
6.386863	344.130716	8.722688
6.767852	345.595789	8.727706
6.621580	349.004782	8.732723
6.865555	339.162457	8.737741
6.455628	321.027967	8.742759
6.237117	339.721466	8.747776
6.855291	341.878562	8.752794
6.584203	348.513113	8.757811
6.603521	338.803591	8.762829
6.474510	338.277974	8.767847
6.860485	342.393004	8.772864
6.480973	339.785802	8.777882
6.172536	335.346733	8.782899
6.725337	339.271695	8.787917
6.766914	344.506952	8.792935
6.604617	349.379498	8.797952
7.072817	347.113654	8.802970
6.637151	342.807996	8.807987
6.440146	340.522654	8.813005
6.743869	340.163177	8.818023
6.925951	345.234555	8.823040
6.581656	335.935079	8.828058
6.368419	332.317432	8.833075
6.904221	337.728188	8.838093
6.795060	335.788912	8.843111
6.440486	338.065905	8.848128
6.706997	345.822204	8.853146
6.374904	351.904552	8.858163
6.783237	356.006637	8.863181
7.374099	356.107356	8.868199
7.168686	346.893543	8.873216
6.676990	336.149647	8.878234
6.534470	327.348907	8.883251
6.389879	332.531099	8.888269
6.706714	336.319240	8.893287
6.486819	343.024709	8.898304
6.628718	342.901856	8.903322
6.545216	348.039830	8.908339
6.969351	356.472144	8.913357
7.122719	353.305470	8.918375
6.863562	350.193560	8.923392
7.211658	343.225585	8.928410
6.827054	332.408215	8.933427
6.463614	336.160270	8.938445
6.453713	337.831362	8.943463
6.594132	349.867402	8.948480
6.720733	353.820858	8.953498
6.606772	358.487076	8.958515
6.643899	351.233017	8.963533
6.807073	352.624713	8.968551
6.663448	359.296224	8.973568
6.856951	357.139416	8.978586
6.870968	359.103417	8.983603
6.676647	358.505920	8.988621
6.898184	355.682065	8.993639
6.714987	358.077537	8.998656
6.711430	345.992222	9.003674
6.729621	358.858297	9.008691
6.469186	361.082768	9.013709
6.592114	359.119976	9.018727
7.031833	370.822268	9.023744
7.265073	365.765550	9.028762
6.714390	364.765971	9.033779
6.560888	362.742081	9.038797
7.062718	365.513711	9.043815
6.908885	371.423150	9.048832
7.395854	371.833520	9.053850
7.298593	361.066064	9.058867
7.113521	352.451808	9.063885
7.112587	353.515624	9.068903
6.616794	354.817425	9.073920
7.104328	351.314716	9.078938
6.568145	366.447656	9.083955
6.476697	362.236714	9.088973
6.758334	366.478443	9.093991
6.641935	381.154737	9.099008
7.180407	386.145392	9.104026
6.994036	387.402175	9.109043
7.092413	386.200556	9.114061
7.395344	381.224498	9.119079
7.457964	387.368472	9.124096
7.328486	377.508536	9.129114
7.233516	358.952603	9.134131
7.131342	358.653168	9.139149
7.131025	361.692318	9.144167
6.902009	357.761558	9.149184
6.905416	358.913056	9.154202
7.067106	358.566227	9.159219
7.073162	357.842863	9.164237
7.233501	355.066404	9.169255
6.936126	367.214798	9.174272
7.105620	364.736697	9.179290
7.048716	374.856447	9.184307
7.183643	375.419454	9.189325
6.929513	373.161935	9.194343
7.184094	374.192280	9.199360
7.286485	383.144892	9.204378
7.454444	373.254426	9.209395
7.091011	375.065769	9.214413
7.115459	357.450560	9.219431
7.277013	362.723943	9.224448
7.167108	359.064957	9.229466
6.952817	354.131568	9.234483
6.976539	349.732293	9.239501
7.370500	365.682882	9.244519
7.177185	370.560263	9.249536
7.269752	366.219689	9.254554
7.276170	367.765174	9.259571
7.060938	361.721144	9.264589
7.396357	354.224991	9.269607
7.432686	360.332026	9.274624
7.395269	356.289389	9.279642
7.254950	356.989918	9.284659
6.813933	364.884787	9.289677
7.015649	360.205345	9.294695
7.067089	373.094655	9.299712
7.157937	365.775424	9.304730
7.540688	383.611691	9.309747
7.188163	386.279670	9.314765
7.395693	391.362877	9.319783
7.391664	391.985387	9.324800
7.563716	381.396882	9.329818
7.566666	376.189835	9.334835
7.010589	376.778382	9.339853
7.240389	371.330899	9.344871
7.282431	376.493513	9.349888
7.351860	375.649835	9.354906
7.118911	383.862592	9.359923
7.054050	388.934563	9.364941
7.199748	380.789474	9.369959
7.506237	391.796192	9.374976
7.516414	384.543160	9.379994
7.610157	381.486746	9.385011
7.297697	390.652268	9.390029
7.138284	387.616334	9.395047
7.040033	388.455475	9.400064
7.580417	380.854819	9.405082
7.617406	387.353059	9.410099
7.521328	389.406784	9.415117
7.785145	391.218292	9.420135
7.414355	387.634631	9.425152
7.457275	377.779410	9.430170
7.352148	379.323329	9.435187
7.297938	380.846697	9.440205
7.549323	381.211700	9.445223
7.298940	388.357412	9.450240
7.480588	388.521844	9.455258
7.887355	387.417370	9.460275
7.480381	383.050433	9.465293
7.478871	370.936382	9.470311
7.521634	378.077471	9.475328
7.460846	377.998798	9.480346
7.635732	372.865962	9.485363
7.296391	377.185443	9.490381
7.721628	375.074600	9.495399
7.367908	373.927595	9.500416
7.276485	387.419796	9.505434
7.435371	375.356504	9.510451
7.270272	385.190165	9.515469
7.541771	372.705419	9.520487
7.562885	388.281756	9.525504
7.627742	387.170559	9.530522
7.638454	381.413220	9.535539
7.165124	387.624861	9.540557
6.997458	374.571051	9.545575
7.248951	375.576632	9.550592
7.423166	377.985882	9.555610
7.683354	379.782176	9.560627
7.213420	386.687529	9.565645
7.629301	377.193940	9.570663
7.433843	388.496547	9.575680
7.699748	405.167661	9.580698
7.800083	401.333928	9.585715
7.486212	399.202466	9.590733
7.448441	404.210266	9.595751
7.817668	408.242717	9.600768
7.938195	405.948950	9.605786
7.791344	395.113459	9.610803
7.417597	392.738869	9.615821
7.822433	398.277327	9.620839
7.923069	395.125168	9.625856
7.342078	391.211335	9.630874
7.712903	392.258294	9.635891
7.400230	407.839283	9.640909
8.020549	408.279382	9.645927
7.799412	408.052114	9.650944
7.775812	412.524405	9.655962
7.856586	402.467626	9.660979
7.529051	410.338535	9.665997
8.262365	401.253078	9.671015
7.880437	399.839077	9.676032
7.357528	388.847557	9.681050
7.768014	395.063597	9.686067
7.944676	407.340174	9.691085
7.817148	399.783544	9.696103
7.801959	405.400023	9.701120
7.766033	402.439530	9.706138
7.914557	398.481536	9.711155
7.725953	405.914267	9.716173
8.058415	399.630323	9.721191
7.963483	401.103233	9.726208
7.533941	394.385695	9.731226
7.651166	396.128513	9.736243
7.676463	401.413656	9.741261
7.909623	408.496712	9.746279
8.394569	408.465607	9.751296
8.085222	402.631867	9.756314
7.922243	395.819180	9.761331
7.973882	390.342629	9.766349
7.815622	390.774569	9.771367
7.811650	386.792986	9.776384
7.727223	385.651386	9.781402
7.735833	386.022632	9.786419
8.209250	401.560114	9.791437
8.164109	397.566005	9.796455
8.050620	392.945098	9.801472
7.519719	391.519580	9.806490
7.623395	388.919187	9.811507
8.028362	408.954659	9.816525
8.201238	407.198669	9.821543
7.908267	410.538999	9.826560
7.837871	411.708303	9.831578
8.131045	403.360371	9.836595
8.227514	413.033407	9.841613
8.330082	399.814433	9.846631
7.631198	396.398612	9.851648
7.809531	394.638618	9.856666
8.222306	408.042866	9.861683
8.084264	408.036178	9.866701
7.974944	398.286695	9.871719
8.117183	406.258020	9.876736
8.180620	412.051599	9.881754
8.240368	390.356920	9.886771
8.085990	390.299130	9.891789
7.719648	386.373967	9.896807
8.034944	399.449421	9.901824
8.074823	410.219964	9.906842
7.947549	411.139360	9.911859
8.084884	415.656019	9.916877
7.978149	414.637806	9.921895
8.542955	411.886721	9.926912
8.290563	421.765549	9.931930
8.367779	405.776703	9.936947
8.025556	408.155918	9.941965
8.134295	410.616391	9.946983
8.435320	400.897687	9.952000
7.886664	398.190585	9.957018
8.208651	396.386135	9.962035
8.169966	410.280376	9.967053
8.383029	403.229266	9.972071
8.312684	397.878997	9.977088
8.053049	396.789921	9.982106
8.188568	402.158884	9.987123
8.183684	407.486595	9.992141
8.133767	401.066537	9.997159
7.846205	411.768148	10.002176
8.061514	415.840343	10.007194
8.308683	418.007878	10.012211
8.478265	415.996792	10.017229
8.496722	416.994480	10.022247
8.438938	411.547582	10.027264
8.250068	408.175421	10.032282
8.387241	410.877608	10.037299
8.242183	417.845994	10.042317
8.364187	413.882659	10.047335
8.287772	406.769326	10.052352
8.611035	413.749997	10.057370
8.270577	405.327158	10.062387
8.077044	395.666524	10.067405
8.570056	406.025704	10.072423
8.452348	403.854232	10.077440
7.701061	402.358891	10.082458
8.105281	396.723306	10.087475
8.260248	411.963259	10.092493
8.414780	409.465392	10.097511
8.600360	408.613094	10.102528
8.350822	403.372771	10.107546
8.514490	398.857025	10.112563
8.433075	401.530130	10.117581
8.265132	403.576113	10.122599
8.537669	394.578179	10.127616
8.145386	407.243125	10.132634
8.360333	406.263185	10.137651
8.364674	405.975565	10.142669
8.348844	406.457909	10.147687
8.644018	401.596656	10.152704
8.445965	402.473425	10.157722
8.656755	402.964664	10.162739
8.745771	407.223770	10.167757
8.662989	413.914229	10.172775
9.129199	411.998963	10.177792
8.685201	411.516075	10.182810
8.352957	402.280957	10.187827
8.146381	393.894080	10.192845
8.426734	410.332588	10.197863
8.378484	406.995335	10.202880
8.168855	413.270064	10.207898
8.402197	413.360180	10.212915
8.522741	412.530630	10.217933
8.525604	415.411511	10.222951
8.812199	406.534453	10.227968
8.627217	404.796313	10.232986
8.360239	407.911701	10.238003
8.230035	407.203239	10.243021
8.108375	419.138127	10.248039
8.432501	405.998256	10.253056
8.562963	419.982928	10.258074
8.264816	425.331060	10.263091
8.728404	428.446308	10.268109
8.734131	429.663718	10.273127
8.918383	431.894697	10.278144
8.671137	434.688297	10.283162
8.423299	422.410601	10.288179
8.716515	434.299838	10.293197
8.757668	436.108151	10.298215
9.027188	435.498391	10.303232
8.669904	423.509121	10.308250
8.594563	424.300518	10.313267
8.516665	418.869372	10.318285
8.904223	445.064267	10.323303
8.941406	433.209224	10.328320
8.735819	426.693479	10.333338
8.621594	426.967091	10.338355
8.832853	417.322312	10.343373
8.656191	426.536133	10.348391
8.930449	423.937576	10.353408
8.870229	432.132929	10.358426
8.609319	429.529337	10.363443
8.734994	432.340609	10.368461
8.629923	439.331179	10.373479
8.879671	435.701383	10.378496
8.728462	447.697692	10.383514
8.764534	442.984062	10.388531
8.681888	439.134631	10.393549
8.566473	442.642973	10.398567
8.874673	436.116654	10.403584
8.941802	441.799219	10.408602
8.845622	438.494668	10.413619
8.870395	436.058024	10.418637
8.622297	437.131926	10.423655
8.915521	433.605809	10.428672
8.367647	441.312231	10.433690
8.495018	436.666434	10.438707
8.827430	428.558522	10.443725
8.596411	427.133646	10.448743
8.884727	442.406508	10.453760
8.876774	452.802690	10.458778
8.991069	463.615326	10.463795
9.383694	454.652311	10.468813
8.958033	444.658580	10.473831
8.698023	429.773050	10.478848
9.124440	447.766676	10.483866
9.066236	449.577837	10.488883
9.233038	442.432932	10.493901
8.995390	434.587335	10.498919
8.951951	435.957560	10.503936
8.950849	440.779789	10.508954
9.086628	447.982159	10.513971
9.227123	436.767404	10.518989
8.940443	440.785226	10.524007
9.005688	432.482235	10.529024
8.979635	441.003616	10.534042
8.823807	460.741471	10.539059
8.914066	455.672278	10.544077
9.064969	465.138061	10.549095
9.404114	462.601976	10.554112
9.370497	462.938775	10.559130
8.813398	463.423347	10.564147
9.087194	466.239963	10.569165
8.750105	469.473570	10.574183
8.870303	460.780175	10.579200
9.194065	462.273103	10.584218
9.025755	454.997341	10.589235
9.173033	454.602264	10.594253
9.055629	444.977085	10.599271
9.494555	462.552232	10.604288
9.358906	459.042393	10.609306
9.210648	455.727014	10.614323
9.104860	457.305754	10.619341
9.320158	453.914836	10.624359
9.740381	451.574403	10.629376
9.424951	458.544086	10.634394
9.369007	452.626697	10.639411
9.643310	451.009537	10.644429
8.982623	452.043543	10.649447
9.184984	442.015146	10.654464
9.479825	450.227805	10.659482
9.219247	457.652829	10.664499
9.468059	461.672484	10.669517
9.330335	462.953255	10.674535
9.235988	453.845164	10.679552
9.570217	458.574164	10.684570
9.516511	459.731405	10.689587
9.351492	445.231840	10.694605
8.789140	438.254111	10.699623
9.297335	445.202846	10.704640
9.428440	449.774130	10.709658
9.093097	452.938037	10.714675
9.375431	444.241496	10.719693
9.583645	464.216150	10.724711
9.683041	462.903920	10.729728
9.613775	453.684633	10.734746
9.532885	455.732845	10.739763
9.507467	453.575399	10.744781
9.083396	463.503070	10.749799
9.440363	469.386659	10.754816
9.741982	459.554227	10.759834
9.383566	460.733665	10.764851
9.657079	458.343492	10.769869
9.645831	463.564919	10.774887
9.480266	447.591746	10.779904
9.299503	444.044755	10.784922
9.440855	456.143836	10.789939
9.468843	450.699350	10.794957
9.586956	463.288024	10.799975
9.581702	466.148087	10.804992
9.683134	461.190757	10.810010
9.112851	461.734183	10.815027
9.108823	453.798557	10.820045
9.288794	462.881134	10.825063
9.363204	461.916761	10.830080
9.640843	452.343675	10.835098
9.377512	465.061164	10.840115
9.702226	470.425936	10.845133
9.331005	471.121397	10.850151
9.372223	464.456763	10.855168
9.326060	455.874475	10.860186
9.536963	464.911214	10.865203
9.635893	461.749842	10.870221
9.602172	469.350979	10.875239
9.707682	479.126780	10.880256
9.926167	471.074455	10.885274
9.813052	467.841959	10.890291
9.529778	470.391877	10.895309
9.492540	463.853062	10.900327
9.691942	467.870944	10.905344
9.696054	475.526151	10.910362
9.462573	484.799339	10.915379
9.714568	476.675525	10.920397
9.610944	482.056500	10.925415
9.796502	480.178613	10.930432
9.846705	476.507297	10.935450
9.866337	484.993185	10.940467
9.766388	483.879241	10.945485
9.691890	483.411400	10.950503
9.724711	487.553049	10.955520
9.873498	476.867129	10.960538
9.785767	479.124682	10.965555
10.119405	483.112201	10.970573
9.918254	481.411282	10.975591
9.870699	488.020549	10.980608
9.872361	481.324199	10.985626
10.124008	484.166356	10.990643
10.050218	478.005596	10.995661
9.633629	483.662507	11.000679
9.936186	489.280031	11.005696
10.177392	478.993112	11.010714
9.855813	487.137669	11.015731
9.651716	482.773832	11.020749
9.978615	489.545693	11.025767
10.022878	480.854645	11.030784
10.206973	481.264839	11.035802
9.834950	484.844699	11.040819
9.951591	483.908462	11.045837
9.826307	479.346170	11.050855
10.100913	486.321823	11.055872
10.126337	485.150491	11.060890
9.648761	486.367418	11.065907
9.969109	487.204502	11.070925
9.810136	489.914941	11.075943
9.770441	484.654544	11.080960
10.080984	481.999839	11.085978
10.181936	488.911016	11.090995
9.921188	480.204344	11.096013
10.014385	487.867775	11.101031
9.919324	482.966278	11.106048
10.093794	482.519631	11.111066
9.808703	487.206216	11.116083
9.835131	472.474859	11.121101
10.201854	482.591826	11.126119
9.922361	486.775789	11.131136
10.330710	483.159158	11.136154
10.040894	480.610549	11.141171
10.045286	486.637397	11.146189
9.929031	484.124878	11.151207
10.115473	484.329589	11.156224
10.289284	491.617569	11.161242
10.487111	490.444639	11.166259
10.067747	489.244733	11.171277
10.119365	489.372611	11.176295
10.139299	484.850821	11.181312
10.173679	482.450543	11.186330
10.269621	488.687189	11.191347
10.624937	489.534607	11.196365
10.362393	482.279817	11.201383
9.996958	489.796917	11.206400
10.045196	474.225912	11.211418
10.220746	500.280336	11.216435
10.282438	505.288457	11.221453
10.407758	506.458851	11.226471
10.328025	510.043697	11.231488
10.112010	499.569190	11.236506
10.182975	506.349349	11.241523
10.147191	500.539253	11.246541
10.561721	511.724875	11.251559
10.523230	516.032261	11.256576
10.343867	514.176475	11.261594
10.467463	517.082754	11.266611
10.541477	511.350229	11.271629
10.663234	499.753361	11.276647
10.688827	500.383885	11.281664
10.705305	489.510284	11.286682
10.564757	481.466519	11.291699
10.375365	476.996258	11.296717
10.066833	481.077448	11.301735
10.332020	490.421314	11.306752
10.463835	483.521671	11.311770
10.302842	503.105750	11.316787
10.600501	507.398664	11.321805
10.515072	510.397444	11.326823
10.463599	508.799445	11.331840
10.548272	510.837664	11.336858
10.843747	504.739316	11.341875
10.709550	497.682278	11.346893
10.470392	495.419257	11.351911
10.329204	495.927432	11.356928
10.724962	492.252801	11.361946
10.434360	496.195510	11.366963
10.703767	511.859523	11.371981
10.695817	506.420615	11.376999
10.205295	496.951327	11.382016
10.803550	498.754954	11.387034
10.743242	515.038325	11.392051
10.624050	504.924264	11.397069
10.627474	491.496606	11.402087
10.438434	508.352255	11.407104
10.618807	507.223065	11.412122
10.442200	510.763037	11.417139
10.687444	507.802929	11.422157
10.774258	509.837659	11.427175
10.283989	511.839168	11.432192
10.881788	510.919529	11.437210
10.783248	510.622681	11.442227
10.701882	504.639808	11.447245
10.836561	499.497417	11.452263
10.393621	515.717293	11.457280
10.430064	501.703844	11.462298
10.809254	504.213736	11.467315
10.407795	508.056948	11.472333
10.934919	503.677082	11.477351
10.736744	505.008292	11.482368
10.864488	498.121899	11.487386
10.377391	510.678610	11.492403
10.931593	503.691105	11.497421
11.290437	505.614056	11.502439
10.875732	508.780862	11.507456
11.113737	508.961767	11.512474
11.060339	499.235079	11.517491
10.821019	501.787624	11.522509
11.245637	506.915955	11.527527
11.194702	501.032482	11.532544
11.053403	502.405327	11.537562
11.146075	501.280325	11.542579
10.810084	507.871393	11.547597
11.123164	500.788894	11.552615
10.709934	501.008080	11.557632
10.899759	502.149497	11.562650
11.085691	505.516262	11.567667
11.127489	511.382667	11.572685
11.000049	503.431521	11.577703
10.815663	506.701317	11.582720
11.278282	501.069229	11.587738
11.043974	503.220225	11.592755
10.720182	510.014514	11.597773
11.365481	497.944831	11.602791
10.897228	507.248272	11.607808
10.996161	504.724336	11.612826
11.003310	508.443972	11.617843
10.641192	507.613831	11.622861
11.141048	496.810126	11.627879
11.077905	506.145163	11.632896
10.856139	503.320880	11.637914
10.628337	508.718042	11.642931
10.714929	513.977896	11.647949
11.199452	521.006083	11.652967
10.921132	530.115870	11.657984
11.241846	532.148897	11.663002
11.618034	531.894895	11.668019
11.335869	537.142746	11.673037
11.366071	519.356075	11.678055
10.994523	519.202714	11.683072
11.677879	522.570927	11.688090
11.406366	513.572438	11.693107
11.216852	505.706692	11.698125
11.095156	502.952032	11.703143
10.944782	509.855013	11.708160
11.250195	527.088110	11.713178
11.244065	525.284243	11.718195
11.128100	528.606503	11.723213
11.563867	527.481727	11.728231
11.417298	537.681800	11.733248
11.543473	534.576131	11.738266
11.127163	524.483073	11.743283
11.188736	534.862167	11.748301
11.529513	523.934897	11.753319
11.371101	534.080009	11.758336
11.662782	533.217498	11.763354
11.591735	521.783173	11.768371
11.441759	524.252386	11.773389
11.254050	505.505621	11.778407
10.990028	517.033570	11.783424
11.330388	519.132962	11.788442
11.297715	535.973758	11.793459
11.364668	537.945314	11.798477
11.558066	526.596039	11.803495
11.679720	531.891464	11.808512
11.493794	525.833349	11.813530
11.460783	528.164436	11.818547
11.805469	525.892556	11.823565
11.835712	524.922433	11.828583
11.692214	536.251756	11.833600
11.411105	525.484424	11.838618
11.520882	534.426495	11.843635
11.397499	534.616332	11.848653
11.683302	530.324523	11.853671
11.857236	531.380057	11.858688
11.778136	529.420301	11.863706
11.678045	514.042762	11.868723
11.474702	519.076373	11.873741
11.968183	514.181058	11.878759
11.397982	518.612253	11.883776
11.298263	511.688691	11.888794
11.609757	518.687014	11.893811
11.401805	530.799507	11.898829
11.930347	531.288611	11.903847
11.421837	528.912895	11.908864
11.325842	526.091116	11.913882
12.117478	525.090806	11.918899
11.772632	526.501655	11.923917
11.925449	521.877119	11.928935
11.380592	523.748280	11.933952
11.396311	532.361027	11.938970
11.320596	529.192122	11.943987
11.368480	526.950674	11.949005
12.073188	529.753855	11.954023
11.838550	528.929111	11.959040
11.748072	524.699045	11.964058
11.703233	527.798801	11.969075
11.540932	540.159802	11.974093
12.046543	539.453322	11.979111
11.820755	542.530763	11.984128
11.758061	543.481135	11.989146
12.070603	553.518220	11.994163
11.855591	547.452003	11.999181
11.897484	543.930284	12.004199
11.827303	553.222261	12.009216
11.632018	560.107009	12.014234
12.058709	555.105322	12.019251
12.017831	560.123116	12.024269
12.338486	551.796081	12.029287
12.092729	549.893827	12.034304
12.179703	542.625618	12.039322
12.189125	531.961364	12.044339
11.729126	538.442369	12.049357
12.002011	519.131592	12.054375
11.804100	534.691668	12.059392
11.958637	544.806996	12.064410
12.019838	550.796619	12.069427
11.840553	553.917313	12.074445
11.962777	554.008952	12.079463
12.119066	553.991150	12.084480
12.095830	559.444835	12.089498
12.195299	551.357358	12.094515
11.806145	564.810846	12.099533
12.177162	555.863767	12.104551
12.418990	555.674864	12.109568
11.855793	552.512429	12.114586
11.945394	553.252905	12.119603
11.923234	557.838613	12.124621
12.138415	554.258354	12.129639
11.972868	561.987348	12.134656
12.106156	555.352525	12.139674
12.348245	556.993871	12.144691
12.026195	557.091568	12.149709
12.131844	558.889852	12.154727
12.034796	555.392918	12.159744
12.188460	552.068380	12.164762
12.395763	550.341728	12.169779
12.278194	555.803789	12.174797
12.528731	555.307429	12.179815
12.207020	562.426447	12.184832
12.119523	555.444163	12.189850
12.355407	562.009326	12.194867
12.321968	579.314166	12.199885
12.550677	570.711116	12.204903
12.504283	567.723824	12.209920
12.213553	565.926396	12.214938
12.672586	572.179120	12.219955
12.550753	563.706388	12.224973
12.396209	553.919681	12.229991
12.100213	555.597470	12.235008
12.033430	570.714301	12.240026
12.866870	572.954670	12.245043
12.251613	583.215119	12.250061
12.441252	574.678108	12.255079
12.885663	583.650150	12.260096
13.107265	574.076256	12.265114
12.697835	564.120955	12.270131
11.968770	566.708737	12.275149
12.396727	563.025923	12.280167
12.522875	572.167427	12.285184
12.476294	578.536744	12.290202
12.640874	572.846901	12.295219
12.455083	576.571345	12.300237
12.514569	574.441689	12.305255
12.679973	565.390925	12.310272
12.698753	577.080000	12.315290
12.705530	574.059183	12.320307
12.725589	583.403396	12.325325
13.009193	577.310027	12.330343
12.716788	583.354716	12.335360
12.696787	591.322983	12.340378
12.583546	579.144139	12.345395
12.355809	582.054639	12.350413
12.689394	580.810076	12.355431
12.701684	574.036300	12.360448
12.853742	580.769150	12.365466
13.115147	577.790735	12.370483
12.803392	585.103864	12.375501
12.930157	581.461630	12.380519
13.105941	579.673613	12.385536
12.526940	576.886005	12.390554
12.942018	574.792499	12.395571
12.688558	577.599711	12.400589
12.391027	580.634682	12.405607
12.580282	572.223959	12.410624
12.550530	579.802436	12.415642
12.674582	579.874856	12.420659
12.597634	578.530116	12.425677
12.894725	581.611357	12.430695
12.933363	582.889922	12.435712
12.588984	579.087524	12.440730
12.723901	586.520449	12.445747
12.575571	589.973987	12.450765
13.047883	605.817921	12.455783
13.179194	602.067682	12.460800
13.232558	598.064502	12.465818
13.240160	595.532683	12.470835
13.140082	588.896313	12.475853
12.653606	583.730695	12.480871
12.718934	586.172706	12.485888
13.069918	603.818487	12.490906
13.320852	598.468627	12.495923
13.014206	602.833563	12.500941
13.385453	598.351717	12.505959
13.229168	581.351383	12.510976
13.095344	588.305464	12.515994
13.392149	577.842580	12.521011
13.281821	588.497768	12.526029
13.207053	588.355002	12.531047
12.934497	579.085253	12.536064
12.692705	588.075778	12.541082
13.418819	586.577602	12.546099
13.116841	585.671824	12.551117
13.200175	575.844913	12.556135
13.574833	575.878315	12.561152
13.042200	587.943573	12.566170
13.164911	581.073711	12.571187
13.156641	588.894989	12.576205
13.447632	598.831318	12.581223
13.054524	585.320167	12.586240
13.376721	599.581229	12.591258
13.479843	601.515604	12.596275
13.397206	596.788859	12.601293
13.248726	587.493476	12.606311
13.517667	587.410799	12.611328
13.299094	597.874572	12.616346
13.144878	599.410374	12.621363
13.147831	607.031105	12.626381
13.449584	606.993811	12.631399
13.452643	613.118735	12.636416
13.140169	609.248249	12.641434
13.504440	610.804307	12.646451
13.486895	615.572341	12.651469
13.357089	619.837166	12.656487
13.581919	610.865486	12.661504
13.489613	614.354485	12.666522
13.423608	606.952284	12.671539
13.560604	618.357903	12.676557
13.413575	612.148540	12.681575
13.189528	608.961692	12.686592
13.283807	615.533144	12.691610
13.572421	612.468439	12.696627
13.376016	616.671053	12.701645
13.373744	619.555922	12.706663
13.330286	615.615148	12.711680
13.516437	627.745238	12.716698
13.545637	635.279847	12.721715
13.907709	641.875884	12.726733
13.637446	631.655888	12.731751
13.857316	623.622213	12.736768
13.474884	618.061703	12.741786
13.606023	616.154406	12.746803
13.891547	622.907515	12.751821
13.823383	629.876635	12.756839
13.633289	614.825435	12.761856
13.737796	630.032408	12.766874
13.594586	625.595942	12.771891
13.714569	632.526301	12.776909
13.720621	630.098857	12.781927
13.780787	635.378640	12.786944
13.902679	645.120425	12.791962
13.642017	633.024455	12.796979
13.830874	635.466174	12.801997
13.932312	632.638884	12.807015
14.192918	637.679185	12.812032
13.747234	637.767731	12.817050
14.425929	631.010093	12.822067
13.717060	627.845080	12.827085
13.641541	631.770110	12.832103
13.595591	627.037644	12.837120
13.905382	643.866245	12.842138
14.169655	636.652441	12.847155
13.922262	637.161377	12.852173
14.186309	641.948688	12.857191
14.323365	633.770118	12.862208
14.169569	632.323734	12.867226
13.978378	627.380361	12.872243
14.024645	629.228921	12.877261
14.075382	632.405329	12.882279
14.150287	633.447886	12.887296
13.860451	634.136994	12.892314
13.600688	637.570022	12.897331
13.892028	634.615338	12.902349
13.960391	638.902961	12.907367
14.023967	632.443058	12.912384
14.221933	639.342345	12.917402
14.140422	638.566335	12.922419
14.010839	638.747671	12.927437
13.970424	635.992957	12.932455
14.270064	635.050310	12.937472
14.265210	642.028511	12.942490
14.096530	637.409822	12.947507
14.227750	637.266540	12.952525
14.264837	640.363028	12.957543
14.168002	640.501397	12.962560
14.326970	644.541393	12.967578
14.290374	642.918976	12.972595
14.050862	633.442090	12.977613
14.144868	634.784619	12.982631
13.946986	639.157875	12.987648
13.990735	655.027556	12.992666
14.398379	656.043554	12.997683
14.743261	655.097017	13.002701
14.337137	656.277584	13.007719
14.823378	655.608828	13.012736
14.812958	654.253724	13.017754
14.281756	636.286111	13.022771
14.382187	632.906733	13.027789
14.057329	633.052203	13.032807
14.333848	643.271666	13.037824
14.329336	657.053486	13.042842
14.455397	652.467795	13.047859
14.850323	647.906514	13.052877
14.568973	650.872708	13.057895
14.801084	660.070340	13.062912
14.860427	653.734161	13.067930
14.723086	641.625296	13.072947
14.853831	640.932998	13.077965
14.479942	643.525449	13.082983
14.652398	629.787358	13.088000
14.921947	635.122900	13.093018
14.129946	629.878610	13.098035
14.303517	633.588139	13.103053
14.799201	653.177433	13.108071
14.905221	661.722536	13.113088
14.583319	664.938035	13.118106
14.617132	659.609339	13.123123
14.843228	661.799119	13.128141
14.710740	658.165677	13.133159
14.580479	647.936497	13.138176
14.496004	655.015460	13.143194
14.465036	659.034541	13.148211
14.923460	653.036999	13.153229
14.854361	656.099531	13.158247
14.853339	648.355847	13.163264
15.023524	651.993326	13.168282
14.677570	654.543561	13.173299
14.731342	655.927069	13.178317
14.853220	662.061911	13.183335
15.025100	653.325664	13.188352
14.537392	656.175671	13.193370
14.645446	661.081946	13.198387
14.582120	647.251168	13.203405
14.568190	654.628404	13.208423
14.683374	657.252004	13.213440
14.955988	662.662814	13.218458
14.906121	662.768625	13.223475
15.316612	670.928668	13.228493
15.239489	666.936322	13.233511
15.332366	652.143980	13.238528
15.154018	646.539063	13.243546
15.003270	654.609763	13.248563
14.804210	651.927083	13.253581
14.918521	658.650060	13.258599
14.987896	651.715894	13.263616
15.355926	661.804360	13.268634
15.046743	652.628635	13.273651
15.260718	649.114814	13.278669
14.830049	656.815703	13.283687
15.134935	666.986583	13.288704
15.241455	679.024969	13.293722
15.483157	670.965783	13.298739
15.187997	670.750036	13.303757
15.131616	682.387769	13.308775
15.165178	681.625397	13.313792
15.370864	681.855515	13.318810
15.281170	687.603600	13.323827
15.325954	677.659563	13.328845
15.103352	687.193085	13.333863
14.989924	683.727078	13.338880
15.574453	688.625444	13.343898
15.016374	680.984257	13.348915
15.133186	690.834151	13.353933
15.148881	685.164298	13.358951
15.290954	681.497569	13.363968
15.331652	678.013878	13.368986
15.113532	685.000055	13.374003
15.455125	670.743310	13.379021
15.500854	687.142867	13.384039
15.360723	684.889649	13.389056
15.758956	680.561365	13.394074
15.481531	684.019242	13.399091
15.410609	675.967705	13.404109
15.303490	685.338083	13.409127
15.288172	681.373980	13.414144
15.472153	691.431159	13.419162
15.587259	708.542589	13.424179
15.939921	703.164237	13.429197
15.756980	696.692202	13.434215
15.553136	687.531614	13.439232
15.620349	687.489813	13.444250
15.946628	688.887698	13.449267
15.654255	683.309989	13.454285
15.535112	682.931142	13.459303
15.544487	690.541442	13.464320
15.501237	694.098556	13.469338
15.516073	708.543255	13.474355
15.722647	711.275706	13.479373
15.482210	711.344919	13.484391
15.615889	712.059604	13.489408
15.782697	712.614502	13.494426
15.731873	719.126536	13.499443
15.944597	715.975803	13.504461
16.053746	715.056499	13.509479
15.860928	716.143900	13.514496
15.896345	710.388919	13.519514
15.770601	709.307379	13.524531
16.168608	701.369005	13.529549
16.196335	713.132513	13.534567
16.329653	711.575150	13.539584
15.777662	696.034291	13.544602
16.162707	696.479473	13.549619
16.242693	689.928636	13.554637
16.020992	682.257164	13.559655
15.614910	683.560799	13.564672
15.810849	689.595760	13.569690
15.695914	710.106981	13.574707
15.890581	708.846170	13.579725
16.056429	711.105295	13.584743
16.196664	710.689219	13.589760
15.969368	708.219203	13.594778
16.256902	710.743395	13.599795
16.305828	711.553324	13.604813
16.467633	704.147170	13.609831
15.837967	705.984218	13.614848
15.862130	706.693865	13.619866
15.839421	704.248798	13.624883
16.203317	706.136272	13.629901
16.295582	708.182799	13.634919
16.289581	703.980562	13.639936
16.327422	698.938396	13.644954
16.453484	705.905706	13.649971
16.161934	704.455519	13.654989
16.058569	704.389784	13.660007
15.776628	703.401988	13.665024
15.670417	704.324431	13.670042
16.039678	714.090853	13.675059
16.353993	726.156876	13.680077
16.895291	721.481271	13.685095
16.317121	716.367758	13.690112
16.474684	714.450026	13.695130
16.019903	708.124450	13.700147
16.088724	713.207255	13.705165
16.736776	717.483534	13.710183
16.666178	725.040030	13.715200
16.642796	720.089438	13.720218
16.469962	718.213680	13.725235
16.873040	722.382939	13.730253
16.530256	710.242900	13.735271
16.414582	709.128234	13.740288
16.620340	709.216335	13.745306
16.713177	707.766258	13.750323
16.809530	701.850319	13.755341
16.595520	711.739110	13.760359
16.395970	706.181655	13.765376
16.370569	702.061332	13.770394
16.619685	717.252175	13.775411
16.887280	714.310642	13.780429
16.890958	710.643366	13.785447
16.604494	709.927664	13.790464
16.987378	711.490301	13.795482
16.525286	707.804028	13.800499
16.887039	705.210743	13.805517
16.630036	709.318675	13.810535
16.576666	704.022473	13.815552
16.596054	717.491360	13.820570
16.826743	726.114910	13.825587
16.924427	733.367508	13.830605
16.726770	728.302041	13.835623
16.723360	728.113450	13.840640
16.610408	721.769360	13.845658
16.399124	727.915073	13.850675
16.488536	727.112446	13.855693
16.579606	722.563742	13.860711
16.529692	729.823540	13.865728
16.579237	730.677554	13.870746
16.915268	744.662032	13.875763
16.943319	744.654729	13.880781
17.154486	738.632542	13.885799
16.705681	745.591546	13.890816
17.225386	741.749248	13.895834
16.993803	741.006066	13.900851
17.081116	745.256051	13.905869
17.044217	747.019745	13.910887
16.919831	745.145908	13.915904
17.152048	741.515624	13.920922
17.303869	746.591828	13.925939
17.066973	741.926930	13.930957
17.412230	734.252367	13.935975
17.227241	739.999527	13.940992
17.361153	737.684700	13.946010
17.374924	749.125367	13.951027
17.144798	745.895261	13.956045
17.005199	753.699191	13.961063
16.882061	746.548816	13.966080
17.520588	750.198600	13.971098
17.410029	744.627277	13.976115
17.311067	748.590695	13.981133
17.302200	744.344715	13.986151
17.219632	748.889386	13.991168
17.296001	739.947067	13.996186
17.131889	751.213466	14.001203
16.956221	752.011030	14.006221
17.524865	748.688114	14.011239
17.191929	750.005610	14.016256
17.486794	750.707824	14.021274
17.444104	752.074801	14.026291
17.517288	751.214742	14.031309
17.582211	742.062772	14.036327
17.336550	745.730303	14.041344
17.659891	750.656730	14.046362
17.396678	759.268836	14.051379
17.422650	767.056459	14.056397
17.507478	771.142741	14.061415
17.947143	781.286391	14.066432
17.754805	760.447841	14.071450
17.359389	760.733681	14.076467
17.632029	765.671162	14.081485
18.098476	766.744282	14.086503
17.482454	771.873773	14.091520
17.420333	764.616065	14.096538
17.872522	767.250324	14.101555
17.658787	771.237928	14.106573
17.827807	766.942156	14.111591
17.880442	772.314668	14.116608
18.163259	765.028499	14.121626
17.753191	765.524898	14.126643
17.933341	766.992877	14.131661
17.925948	756.375286	14.136679
17.510815	748.607675	14.141696
17.906679	758.439405	14.146714
17.962717	766.629434	14.151731
17.469144	776.489207	14.156749
17.903307	770.470157	14.161767
17.813622	782.618054	14.166784
17.920046	770.464837	14.171802
18.099310	774.347073	14.176819
17.892102	774.048205	14.181837
17.915541	771.715861	14.186855
17.825430	772.307607	14.191872
17.679161	760.294722	14.196890
17.739679	771.504070	14.201907
17.880348	767.225335	14.206925
18.252119	773.049917	14.211943
17.881542	772.214769	14.216960
17.916637	775.018108	14.221978
18.286325	772.814885	14.226995
17.903100	777.381129	14.232013
18.295096	784.253418	14.237031
18.027156	800.818679	14.242048
18.423473	803.114514	14.247066
18.110683	804.138552	14.252083
18.274761	799.032522	14.257101
18.720688	793.447123	14.262119
18.200495	783.174438	14.267136
18.188094	780.005097	14.272154
18.407018	795.263822	14.277171
18.300066	795.952862	14.282189
18.779729	782.362476	14.287207
18.487504	783.967118	14.292224
18.308765	776.143754	14.297242
18.286213	773.812259	14.302259
18.038658	779.341962	14.307277
18.607303	779.016968	14.312295
18.304690	794.981725	14.317312
18.336469	797.570996	14.322330
18.258585	802.373720	14.327347
18.300136	807.451331	14.332365
18.631525	802.275071	14.337383
18.388111	804.228710	14.342400
18.522984	798.707518	14.347418
18.640966	796.597129	14.352435
18.327495	796.201200	14.357453
18.494863	792.644117	14.362471
18.595941	790.328084	14.367488
18.572003	795.901868	14.372506
18.507372	797.941277	14.377523
18.575777	805.141659	14.382541
18.488677	792.652494	14.387559
18.902057	805.744533	14.392576
18.814697	812.385362	14.397594
18.665222	806.782210	14.402611
18.859889	825.206767	14.407629
18.955730	818.391488	14.412647
18.847205	823.511405	14.417664
18.690381	816.565058	14.422682
18.962230	815.601482	14.427699
18.477346	827.116682	14.432717
18.895263	823.432223	14.437735
18.839044	826.615851	14.442752
19.034150	824.910007	14.447770
19.205455	828.881854	14.452787
18.945475	822.895126	14.457805
19.096309	811.123119	14.462823
19.282456	824.556656	14.467840
18.992415	825.854856	14.472858
19.053471	822.513130	14.477875
19.083485	822.003762	14.482893
19.202107	818.612049	14.487911
19.215966	819.395886	14.492928
19.203016	821.389382	14.497946
19.259415	807.681846	14.502963
18.880379	798.305488	14.507981
18.678897	806.661859	14.512999
18.965781	819.906143	14.518016
19.028291	813.228597	14.523034
19.030656	819.031816	14.528051
19.209079	820.746214	14.533069
19.360025	819.874044	14.538087
19.220949	816.361513	14.543104
18.855800	817.500997	14.548122
19.001263	813.262529	14.553139
18.998969	822.821781	14.558157
19.596870	823.028704	14.563175
19.201096	828.944407	14.568192
19.086450	837.536574	14.573210
19.813566	833.223319	14.578227
19.323471	833.766892	14.583245
19.596015	831.200101	14.588263
19.532688	829.133716	14.593280
19.123331	833.123390	14.598298
19.353545	830.724132	14.603315
19.333776	841.863975	14.608333
19.590473	844.039547	14.613351
19.287533	842.685793	14.618368
19.225446	849.903354	14.623386
19.913126	839.114379	14.628403
19.711739	842.573071	14.633421
19.763846	837.449751	14.638439
19.505953	841.406377	14.643456
19.564292	839.005476	14.648474
19.913215	832.349599	14.653491
19.231076	841.998932	14.658509
19.685519	834.357818	14.663527
19.728053	836.188046	14.668544
19.426416	836.721212	14.673562
19.493957	842.656299	14.678579
19.702168	856.026465	14.683597
20.180776	851.824479	14.688615
19.946541	845.041648	14.693632
19.845868	836.593892	14.698650
19.891568	840.007801	14.703667
19.923732	841.186410	14.708685
19.804082	836.897698	14.713703
19.968316	852.231257	14.718720
20.123974	856.909273	14.723738
20.126365	848.543293	14.728755
19.897511	848.752710	14.733773
19.844994	849.878234	14.738791
20.022202	864.506057	14.743808
19.810085	873.167065	14.748826
20.200541	865.371802	14.753843
20.291362	870.738399	14.758861
20.480117	867.619772	14.763879
20.270885	867.942897	14.768896
19.979275	851.200054	14.773914
20.267086	854.680408	14.778931
20.056418	864.508805	14.783949
20.355431	862.698418	14.788967
20.504388	858.746567	14.793984
20.019680	860.062455	14.799002
20.483345	854.729889	14.804019
20.422794	869.786044	14.809037
20.518855	862.317479	14.814055
20.234110	848.315897	14.819072
20.183442	851.091577	14.824090
20.687171	844.566223	14.829107
20.655309	848.232045	14.834125
20.257694	835.579762	14.839143
20.776343	834.508334	14.844160
20.168574	834.880886	14.849178
20.286533	833.458444	14.854195
20.388342	842.730106	14.859213
20.519800	851.959287	14.864231
20.701164	862.553445	14.869248
20.283238	865.282169	14.874266
20.385041	856.597757	14.879283
20.328743	864.429790	14.884301
20.757662	866.985639	14.889319
20.752602	860.473226	14.894336
20.673197	867.030788	14.899354
20.860767	861.362520	14.904371
20.354803	872.461319	14.909389
20.462366	871.510697	14.914407
20.488757	866.908912	14.919424
20.717665	860.921790	14.924442
20.893941	865.435657	14.929459
20.284141	870.725150	14.934477
20.251894	867.246467	14.939495
20.864417	867.523696	14.944512
20.227663	873.243409	14.949530
20.811740	880.786401	14.954547
20.688209	884.469658	14.959565
20.578068	891.107753	14.964583
21.074236	886.230853	14.969600
21.108345	889.081700	14.974618
21.443102	884.665424	14.979635
21.264879	885.002655	14.984653
21.288191	883.992567	14.989671
21.102976	888.474362	14.994688
21.151330	885.295544	14.999706
20.983819	875.974571	15.004723
20.936902	886.222442	15.009741
21.187173	882.642966	15.014759
21.151122	885.918137	15.019776
21.045448	887.900832	15.024794
21.342145	889.227601	15.029811
21.344900	891.041938	15.034829
21.351727	896.904447	15.039847
21.329598	896.507335	15.044864
21.072139	888.039786	15.049882
21.284983	888.082605	15.054899
21.541762	895.020170	15.059917
20.983849	893.431562	15.064935
21.315678	892.304013	15.069952
21.074022	904.851186	15.074970
21.034767	893.358025	15.079987
21.019514	881.561340	15.085005
21.077993	887.223304	15.090023
21.650477	879.238752	15.095040
20.951576	884.324376	15.100058
21.127816	884.205641	15.105075
21.320119	897.095488	15.110093
21.650601	907.218341	15.115111
21.709356	905.486382	15.120128
21.529839	918.891718	15.125146
21.718492	916.836582	15.130163
22.188510	904.797073	15.135181
21.356752	900.931635	15.140199
21.425112	898.598592	15.145216
21.485195	906.403056	15.150234
21.547812	912.133810	15.155251
21.549680	907.807226	15.160269
21.856610	908.990396	15.165287
22.033506	904.993159	15.170304
21.789493	915.836611	15.175322
22.320059	913.614635	15.180339
21.858261	907.605653	15.185357
21.476569	913.585462	15.190375
21.914151	908.017105	15.195392
21.893546	904.785905	15.200410
21.824601	904.755835	15.205427
21.614070	905.962768	15.210445
21.599622	915.015888	15.215463
21.643257	902.667234	15.220480
21.909068	918.063927	15.225498
21.967396	907.988268	15.230515
22.046366	907.537546	15.235533
21.945723	913.574580	15.240551
21.948348	909.872713	15.245568
21.986712	914.269212	15.250586
22.022152	910.180393	15.255603
22.098096	913.857844	15.260621
21.907076	917.112969	15.265639
22.677983	933.049558	15.270656
22.186688	915.656105	15.275674
21.921727	910.638934	15.280691
21.903706	919.566383	15.285709
21.923154	925.856117	15.290727
22.376180	929.190845	15.295744
21.725916	930.904892	15.300762
22.280772	930.799789	15.305779
22.508116	927.728792	15.310797
22.650299	938.183931	15.315815
22.692053	928.953423	15.320832
22.175667	931.154700	15.325850
22.464284	929.819286	15.330867
22.444060	945.077505	15.335885
22.257377	943.080805	15.340903
22.351333	935.975447	15.345920
22.258840	931.060803	15.350938
22.434600	934.684849	15.355955
22.237129	932.658273	15.360973
22.421216	952.570961	15.365991
22.540361	961.827363	15.371008
22.401619	968.337398	15.376026
22.432994	955.693975	15.381043
22.428021	964.193390	15.386061
22.443136	967.599462	15.391079
22.505409	958.403613	15.396096
22.682365	963.700023	15.401114
22.707493	963.336577	15.406131
22.670780	959.804923	15.411149
22.743762	962.561369	15.416167
22.823659	957.048687	15.421184
22.841420	959.441352	15.426202
22.987804	959.141076	15.431219
23.143611	946.841196	15.436237
23.036128	953.721892	15.441255
23.307075	950.296970	15.446272
22.655926	958.480432	15.451290
22.732876	963.568355	15.456307
23.120537	958.165542	15.461325
23.374860	967.665982	15.466343
23.463797	957.121635	15.471360
23.154322	953.853353	15.476378
23.427992	955.249983	15.481395
23.356224	950.808624	15.486413
22.976482	956.519905	15.491431
23.088886	954.230489	15.496448
23.305229	953.698418	15.501466
23.032803	956.335076	15.506483
23.095905	956.391742	15.511501
23.043940	962.187689	15.516519
23.159864	954.570828	15.521536
23.112237	961.101387	15.526554
23.105791	966.344304	15.531571
23.372742	972.835356	15.536589
23.611069	979.460252	15.541607
23.611150	975.714588	15.546624
23.148051	966.739386	15.551642
23.390769	976.989550	15.556659
23.750773	977.489131	15.561677
23.652661	977.179585	15.566695
23.773317	966.302096	15.571712
23.705247	964.091270	15.576730
23.419517	947.558855	15.581747
23.398061	951.803734	15.586765
23.206063	963.216617	15.591783
23.905582	966.853795	15.596800
23.791658	978.058875	15.601818
23.582151	983.844644	15.606835
24.039059	975.786527	15.611853
23.914980	962.166932	15.616871
24.150724	959.413352	15.621888
23.631965	957.152779	15.626906
23.637698	961.355558	15.631923
23.608320	949.785085	15.636941
23.618667	959.089982	15.641959
23.905885	972.750887	15.646976
23.913084	976.372784	15.651994
24.344990	974.039932	15.657011
24.522428	971.958134	15.662029
23.784626	953.217652	15.667047
23.912311	948.391796	15.672064
23.853548	950.455554	15.677082
23.556485	948.031080	15.682099
24.098613	955.422848	15.687117
24.277908	974.654667	15.692135
24.425279	970.671480	15.697152
23.930995	967.589757	15.702170
23.843913	977.092866	15.707187
24.166152	972.694296	15.712205
24.149154	972.728720	15.717223
23.961054	978.911935	15.722240
23.990151	972.321580	15.727258
24.209782	973.985397	15.732275
24.288909	969.157628	15.737293
24.231143	977.785187	15.742311
24.454265	973.108564	15.747328
24.190778	975.620759	15.752346
24.248667	979.471445	15.757363
24.273363	973.553950	15.762381
24.283682	971.791657	15.767399
24.522709	982.367441	15.772416
24.520265	971.262967	15.777434
24.305437	988.545954	15.782451
24.210033	970.626913	15.787469
24.567553	992.781625	15.792487
24.558169	994.702003	15.797504
24.848925	995.515318	15.802522
24.500361	986.137272	15.807539
24.716782	994.223541	15.812557
24.817057	1003.359828	15.817575
24.609109	988.913840	15.822592
24.747483	983.458316	15.827610
24.534225	1003.805306	15.832627
24.883823	997.524797	15.837645
25.179259	1004.380649	15.842663
25.014594	984.869255	15.847680
24.685393	987.035082	15.852698
24.316057	986.474280	15.857715
24.686340	990.377315	15.862733
24.918327	1001.556954	15.867751
25.030723	994.366653	15.872768
25.125884	1003.036685	15.877786
24.868399	1005.734138	15.882803
24.920798	1003.665494	15.887821
24.705775	1009.572049	15.892839
24.738935	998.493571	15.897856
25.161706	1000.315107	15.902874
24.955348	999.586921	15.907891
25.057295	992.331976	15.912909
24.851951	1002.197488	15.917927
24.944046	1000.741191	15.922944
25.239237	995.037190	15.927962
24.875955	986.857464	15.932979
25.008851	989.364749	15.937997
24.992841	1018.655999	15.943015
25.156729	1008.166223	15.948032
25.571639	1014.586917	15.953050
25.042772	1016.278915	15.958067
25.362560	1016.570167	15.963085
25.395413	1017.657163	15.968103
25.601258	1018.445831	15.973120
25.822581	1018.225402	15.978138
25.474234	1024.455673	15.983155
25.637615	1018.188371	15.988173
25.821830	1022.448581	15.993191
25.513853	1018.959151	15.998208
25.450887	1026.861720	16.003226
25.669111	1025.565661	16.008243
25.739610	1013.610373	16.013261
25.665477	1025.879088	16.018279
25.946723	1024.749939	16.023296
25.563727	998.667528	16.028314
25.215573	1013.068006	16.033331
25.447713	1017.525877	16.038349
25.441836	1022.058677	16.043367
25.869194	1026.473533	16.048384
25.651859	1016.465978	16.053402
25.357137	1023.259090	16.058419
25.604002	1028.001845	16.063437
25.845991	1024.953797	16.068455
25.706131	1024.070091	16.073472
25.761651	1039.291352	16.078490
25.939186	1044.291055	16.083507
25.923818	1041.279918	16.088525
26.033254	1044.289473	16.093543
26.003613	1042.656469	16.098560
26.179641	1046.179512	16.103578
26.072989	1038.773992	16.108595
26.123675	1042.272369	16.113613
26.445499	1038.066349	16.118631
26.279167	1048.626391	16.123648
26.195393	1040.172752	16.128666
26.138828	1042.974626	16.133683
26.330996	1039.031786	16.138701
26.599899	1042.909592	16.143719
26.534684	1049.749030	16.148736
26.608428	1039.645650	16.153754
26.183819	1027.906291	16.158771
26.272298	1035.608563	16.163789
26.258635	1047.369268	16.168807
26.502075	1037.785414	16.173824
26.198076	1034.680364	16.178842
26.003525	1043.064168	16.183859
26.172462	1053.496275	16.188877
26.482576	1046.186807	16.193895
26.328521	1038.394198	16.198912
26.378792	1044.433026	16.203930
26.518436	1049.277686	16.208947
26.356062	1040.369232	16.213965
26.444816	1046.023378	16.218983
26.289652	1057.348536	16.224000
26.880038	1058.298237	16.229018
26.676121	1070.653461	16.234035
26.821856	1059.462745	16.239053
26.714937	1066.924057	16.244071
26.706750	1073.723068	16.249088
26.949919	1065.751837	16.254106
26.572531	1066.741766	16.259123
27.109172	1067.794508	16.264141
26.827380	1071.398304	16.269159
26.728216	1068.911444	16.274176
26.752460	1065.824708	16.279194
27.027590	1076.290787	16.284211
26.900325	1064.760726	16.289229
26.687689	1072.519362	16.294247
26.975879	1070.126824	16.299264
26.978309	1067.456890	16.304282
26.736275	1077.539592	16.309299
27.140711	1078.177424	16.314317
27.604944	1091.848728	16.319335
27.593896	1078.700589	16.324352
27.245522	1068.079099	16.329370
27.080936	1066.801614	16.334387
27.272215	1069.344001	16.339405
27.501152	1058.392793	16.344423
27.110209	1064.241550	16.349440
27.458209	1069.082177	16.354458
27.689736	1093.169025	16.359475
27.623434	1075.011820	16.364493
27.783673	1067.760392	16.369511
27.070168	1068.641709	16.374528
27.421470	1070.941433	16.379546
27.483776	1070.881461	16.384563
27.552491	1084.955163	16.389581
27.778389	1088.852298	16.394599
27.623930	1091.921883	16.399616
27.473905	1074.998996	16.404634
27.657551	1082.752742	16.409651
27.681198	1079.363144	16.414669
27.864228	1077.226816	16.419687
27.990055	1082.966718	16.424704
27.926126	1085.949624	16.429722
27.943371	1078.035654	16.434739
27.722450	1065.141105	16.439757
27.872503	1072.486671	16.444775
27.803394	1089.037020	16.449792
27.910002	1084.867653	16.454810
28.045475	1083.723328	16.459827
27.837574	1081.796187	16.464845
27.803443	1084.651379	16.469863
27.902120	1085.863829	16.474880
27.995361	1079.765215	16.479898
27.853319	1080.033700	16.484915
28.002311	1086.290698	16.489933
28.458903	1071.182606	16.494951
28.280024	1084.370219	16.499968
28.418472	1076.847628	16.504986
28.166970	1083.400507	16.510003
28.363367	1070.147493	16.515021
28.758563	1070.660532	16.520039
28.272169	1071.029969	16.525056
28.442011	1068.318190	16.530074
28.296583	1069.366676	16.535091
28.277385	1066.955727	16.540109
28.192898	1069.553672	16.545127
28.089297	1067.168487	16.550144
28.341345	1068.183489	16.555162
28.305459	1063.424095	16.560179
28.284610	1067.309150	16.565197
28.394420	1060.160249	16.570215
28.128405	1079.269013	16.575232
28.427380	1061.727128	16.580250
28.231730	1070.593948	16.585267
28.681942	1083.008279	16.590285
28.875308	1099.991138	16.595303
28.563807	1103.751043	16.600320
28.613144	1094.333078	16.605338
28.659897	1097.355557	16.610355
28.470285	1090.723473	16.615373
28.546069	1088.092607	16.620391
28.519622	1090.766724	16.625408
28.660984	1084.262990	16.630426
28.587251	1092.946739	16.635443
28.731348	1088.888297	16.640461
29.222288	1093.220687	16.645479
29.048733	1101.749571	16.650496
28.983669	1091.598346	16.655514
28.997553	1105.595397	16.660531
29.082795	1105.869521	16.665549
28.972900	1101.525577	16.670567
28.904036	1109.457503	16.675584
29.184841	1109.432938	16.680602
29.438358	1119.277564	16.685619
29.308947	1114.602144	16.690637
29.314205	1108.416234	16.695655
29.198302	1115.232032	16.700672
29.530318	1110.547886	16.705690
29.302602	1113.594167	16.710707
29.145995	1112.826672	16.715725
29.371878	1106.704241	16.720743
29.404918	1120.253357	16.725760
29.514583	1118.743822	16.730778
29.600249	1108.758466	16.735795
29.415613	1109.286046	16.740813
29.782897	1104.444933	16.745831
29.485301	1103.712013	16.750848
29.643382	1109.333294	16.755866
29.302140	1114.603135	16.760883
29.230831	1114.589212	16.765901
29.393795	1114.510411	16.770919
29.118003	1113.594217	16.775936
29.307443	1113.830027	16.780954
29.784289	1120.682925	16.785971
29.508230	1122.225119	16.790989
29.774043	1126.946016	16.796007
29.704712	1132.173526	16.801024
29.507062	1133.914950	16.806042
29.543350	1144.175261	16.811059
29.440035	1130.520746	16.816077
29.785205	1139.959797	16.821095
30.038671	1152.048207	16.826112
30.066615	1159.103555	16.831130
30.005259	1162.499480	16.836147
30.283398	1158.398062	16.841165
30.657728	1148.667539	16.846183
30.199862	1139.464219	16.851200
29.993793	1139.430252	16.856218
30.094955	1142.305413	16.861235
30.449029	1154.475989	16.866253
30.717877	1149.277809	16.871271
30.498845	1139.658609	16.876288
30.361547	1132.147370	16.881306
30.193579	1129.286209	16.886323
30.149793	1122.142263	16.891341
30.428789	1131.730467	16.896359
30.342161	1136.897557	16.901376
30.676825	1147.669986	16.906394
30.700465	1136.166875	16.911411
30.096303	1135.683654	16.916429
30.174686	1131.064239	16.921447
30.301675	1144.109600	16.926464
30.456024	1146.714552	16.931482
30.713330	1147.059716	16.936499
30.621815	1158.362405	16.941517
30.987864	1149.794497	16.946535
30.654297	1156.394894	16.951552
30.776060	1151.655111	16.956570
30.657568	1153.592494	16.961587
30.594682	1153.416314	16.966605
30.931028	1158.687967	16.971623
30.455282	1145.665778	16.976640
30.581187	1153.819861	16.981658
31.002736	1150.194729	16.986675
30.669055	1167.291269	16.991693
31.054051	1171.741159	16.996711
31.233109	1175.844420	17.001728
31.171657	1189.058008	17.006746
31.380769	1177.977271	17.011763
30.935541	1176.222769	17.016781
31.012210	1171.824515	17.021799
31.184060	1175.367169	17.026816
31.023832	1180.769790	17.031834
31.222918	1183.749632	17.036851
31.022777	1183.411787	17.041869
31.373908	1172.804399	17.046887
31.126024	1174.253848	17.051904
31.211059	1183.073867	17.056922
31.471900	1177.419336	17.061939
31.310842	1181.058005	17.066957
31.179751	1176.960338	17.071975
31.554290	1174.301880	17.076992
31.500194	1172.590621	17.082010
31.594915	1175.728721	17.087027
31.536866	1172.509614	17.092045
31.809895	1176.708697	17.097063
32.023483	1174.002714	17.102080
31.887978	1175.952216	17.107098
31.880244	1169.222357	17.112115
31.567195	1174.787625	17.117133
31.709519	1173.635916	17.122151
31.749641	1174.305227	17.127168
31.773145	1168.422566	17.132186
32.081686	1167.055631	17.137203
31.849415	1170.648581	17.142221
32.218876	1171.519078	17.147239
31.959281	1176.706798	17.152256
31.965432	1176.008633	17.157274
32.095330	1169.973707	17.162291
31.800795	1178.941183	17.167309
32.061801	1183.012752	17.172327
32.303553	1194.787436	17.177344
32.097020	1195.463593	17.182362
32.228296	1193.947532	17.187379
31.970278	1198.762630	17.192397
32.448531	1206.025594	17.197415
32.529813	1205.236835	17.202432
32.539751	1196.964190	17.207450
32.440769	1192.609058	17.212467
32.365770	1197.619721	17.217485
32.100593	1197.285690	17.222503
32.260333	1201.306758	17.227520
32.466726	1202.937944	17.232538
32.693342	1193.858396	17.237555
32.546936	1198.141723	17.242573
32.835201	1191.551962	17.247591
32.480153	1190.408263	17.252608
32.224096	1198.145313	17.257626
32.615253	1183.220883	17.262643
32.492315	1198.754085	17.267661
32.456527	1197.005260	17.272679
32.474116	1200.385746	17.277696
33.090606	1196.225328	17.282714
32.700760	1183.814582	17.287731
33.009000	1194.177746	17.292749
33.052286	1198.573549	17.297767
33.131911	1199.388188	17.302784
32.671155	1197.879098	17.307802
32.910570	1192.508764	17.312819
32.746771	1197.135623	17.317837
32.860189	1185.769980	17.322855
33.259425	1188.062257	17.327872
32.836619	1201.139612	17.332890
33.164349	1208.034696	17.337907
33.136705	1216.095950	17.342925
33.106728	1221.550887	17.347943
33.444237	1217.017337	17.352960
33.298712	1227.665763	17.357978
33.421396	1216.595302	17.362995
32.774560	1220.366417	17.368013
33.442330	1221.250430	17.373031
33.535404	1216.347841	17.378048
33.416111	1223.306218	17.383066
33.469977	1228.363097	17.388083
33.556300	1229.687933	17.393101
33.653783	1228.587384	17.398119
33.989046	1216.994677	17.403136
33.604163	1223.962848	17.408154
33.726673	1210.459303	17.413171
33.542509	1219.662078	17.418189
33.690863	1219.929533	17.423207
33.732474	1213.558046	17.428224
33.417036	1221.755630	17.433242
33.501366	1219.792442	17.438259
33.324583	1223.004379	17.443277
33.413364	1220.696517	17.448295
34.283773	1227.895277	17.453312
34.081080	1236.933689	17.458330
34.093336	1236.644824	17.463347
34.039920	1230.363866	17.468365
33.990722	1235.326341	17.473383
34.077392	1238.737103	17.478400
33.665975	1236.093709	17.483418
33.862666	1234.242413	17.488435
34.011772	1241.777544	17.493453
33.836158	1243.720674	17.498471
34.304625	1239.971455	17.503488
33.968629	1240.936014	17.508506
34.564826	1232.234404	17.513523
33.968806	1230.203574	17.518541
34.067387	1229.475237	17.523559
34.333563	1245.459135	17.528576
34.323434	1251.649448	17.533594
34.417023	1249.353456	17.538611
34.154461	1253.197291	17.543629
34.330625	1257.102206	17.548647
34.537882	1264.284311	17.553664
34.361701	1264.151017	17.558682
34.490743	1254.483873	17.563699
34.619058	1253.971811	17.568717
34.634037	1250.378403	17.573735
34.629666	1251.256615	17.578752
34.309563	1255.945696	17.583770
35.052021	1258.067778	17.588787
34.913148	1247.066424	17.593805
34.666022	1248.916548	17.598823
35.365863	1265.893292	17.603840
34.982961	1258.410771	17.608858
35.084316	1248.284039	17.613875
34.847463	1249.697064	17.618893
35.233294	1246.929539	17.623911
35.309917	1243.269731	17.628928
34.744350	1250.281823	17.633946
35.242385	1249.652237	17.638963
35.624228	1252.082929	17.643981
35.214827	1251.604095	17.648999
35.189204	1248.351523	17.654016
35.234145	1247.726211	17.659034
34.881582	1254.440054	17.664051
35.310135	1258.217311	17.669069
35.167867	1268.126798	17.674087
35.355128	1265.241864	17.679104
34.876072	1268.232630	17.684122
35.669650	1263.956263	17.689139
35.648548	1264.710849	17.694157
35.737652	1271.598929	17.699175
35.606981	1265.585606	17.704192
35.528560	1262.035140	17.709210
36.081364	1268.248265	17.714227
35.556569	1267.515998	17.719245
35.623755	1267.755066	17.724263
35.726278	1265.987856	17.729280
35.382647	1267.458532	17.734298
35.539411	1272.944371	17.739315
36.299274	1287.756379	17.744333
35.923349	1283.217126	17.749351
36.180411	1276.789981	17.754368
36.011747	1281.941483	17.759386
36.165682	1272.762758	17.764403
36.081022	1267.357653	17.769421
35.920751	1271.340199	17.774439
36.159053	1272.698180	17.779456
35.886607	1283.041353	17.784474
36.272633	1288.873354	17.789491
36.241574	1286.650413	17.794509
36.066400	1293.058942	17.799527
36.686774	1289.494344	17.804544
36.615622	1285.952209	17.809562
36.361184	1287.876059	17.814579
36.491523	1284.173165	17.819597
36.259990	1290.773503	17.824615
36.552709	1272.932584	17.829632
36.168246	1278.408017	17.834650
36.202646	1279.611554	17.839667
36.796137	1277.404983	17.844685
36.483353	1278.359618	17.849703
36.716852	1278.626440	17.854720
36.553778	1274.738858	17.859738
36.870932	1281.831276	17.864755
36.769111	1276.305763	17.869773
36.449177	1278.082019	17.874791
36.928382	1277.471143	17.879808
36.695125	1287.732478	17.884826
36.826853	1298.580777	17.889843
37.506830	1293.476334	17.894861
36.944600	1291.020514	17.899879
37.307701	1282.380418	17.904896
36.997043	1281.434930	17.909914
36.965034	1275.977442	17.914931
37.100778	1281.362415	17.919949
37.108199	1298.232403	17.924967
37.233353	1300.624172	17.929984
37.533568	1294.748880	17.935002
37.432316	1290.864291	17.940019
37.150020	1285.392121	17.945037
37.232697	1291.230327	17.950055
37.279610	1294.792458	17.955072
37.443290	1292.652805	17.960090
37.247993	1300.367816	17.965107
37.729394	1296.439847	17.970125
37.378282	1290.615472	17.975143
37.608150	1295.367257	17.980160
37.778071	1301.924029	17.985178
37.939392	1297.228542	17.990195
37.998067	1301.012904	17.995213
37.820946	1302.968899	18.000231
38.027113	1296.505490	18.005248
37.615476	1301.129938	18.010266
37.806171	1300.797511	18.015283
38.198643	1305.296764	18.020301
37.888724	1308.860805	18.025319
38.274573	1302.432534	18.030336
38.153562	1309.186085	18.035354
37.803342	1303.715018	18.040371
38.021832	1301.487935	18.045389
37.355200	1310.166272	18.050407
37.710860	1304.642106	18.055424
37.934573	1307.157386	18.060442
37.663151	1308.601044	18.065459
38.199213	1320.285807	18.070477
38.165317	1318.388353	18.075495
38.233050	1320.530289	18.080512
38.663893	1321.239758	18.085530
38.141466	1326.881853	18.090547
38.565988	1323.546559	18.095565
38.348971	1323.785696	18.100583
38.413114	1319.629197	18.105600
38.047466	1323.407046	18.110618
38.142855	1320.722600	18.115635
38.363234	1318.141772	18.120653
38.426782	1344.268519	18.125671
38.543163	1347.734636	18.130688
38.469992	1347.799898	18.135706
38.363892	1352.970082	18.140723
38.850120	1344.954572	18.145741
38.703285	1353.722413	18.150759
38.688163	1352.355365	18.155776
38.801665	1348.958037	18.160794
38.324048	1346.915070	18.165811
39.074462	1359.254452	18.170829
38.953939	1365.884872	18.175847
39.142522	1374.269139	18.180864
39.192872	1371.601166	18.185882
39.316827	1371.257038	18.190899
39.193433	1374.217692	18.195917
39.262935	1371.537270	18.200935
38.930690	1369.263382	18.205952
39.268309	1369.876914	18.210970
39.281450	1365.466413	18.215987
39.740456	1359.487481	18.221005
39.767282	1367.284702	18.226023
39.531919	1359.501455	18.231040
39.687980	1362.333391	18.236058
39.736954	1365.412374	18.241075
39.681280	1356.155789	18.246093
39.751575	1359.805810	18.251111
40.026088	1354.852842	18.256128
40.147293	1354.234587	18.261146
39.844372	1354.278815	18.266163
39.704758	1336.195875	18.271181
39.795149	1348.429729	18.276199
39.846239	1353.051574	18.281216
39.850431	1353.489800	18.286234
39.866098	1353.014209	18.291251
40.116648	1345.073263	18.296269
40.001347	1351.740734	18.301287
39.927647	1353.507062	18.306304
40.142917	1354.515185	18.311322
39.512480	1353.897192	18.316339
40.213392	1357.856128	18.321357
40.269480	1361.252741	18.326375
39.938805	1351.770729	18.331392
40.180724	1359.379823	18.336410
40.485855	1361.222869	18.341427
40.087809	1364.541866	18.346445
40.035229	1354.445352	18.351463
40.334934	1368.423355	18.356480
40.533983	1372.993766	18.361498
40.291580	1373.726007	18.366515
40.188623	1380.950147	18.371533
40.068047	1380.199121	18.376551
40.617919	1373.688482	18.381568
40.763558	1378.541766	18.386586
40.707617	1388.002376	18.391603
40.928739	1375.168166	18.396621
40.353304	1384.128986	18.401639
40.515783	1389.102728	18.406656
40.869231	1399.566271	18.411674
40.572511	1404.106581	18.416691
40.898670	1403.046157	18.421709
40.926835	1410.303542	18.426727
41.096007	1402.962224	18.431744
41.027012	1390.182641	18.436762
41.122173	1402.718749	18.441779
41.098111	1395.271819	18.446797
41.154045	1395.768263	18.451815
41.250358	1392.307331	18.456832
41.268363	1397.638086	18.461850
41.256757	1403.358464	18.466867
41.629357	1400.551951	18.471885
41.456822	1398.676073	18.476903
41.209493	1403.268654	18.481920
41.726960	1411.301930	18.486938
41.132942	1420.413985	18.491955
41.626105	1421.003301	18.496973
41.697004	1425.372770	18.501991
41.670844	1422.549443	18.507008
42.150516	1423.169262	18.512026
41.738197	1428.926791	18.517043
41.695701	1420.267728	18.522061
42.299990	1414.679571	18.527079
42.215774	1415.440834	18.532096
42.178116	1405.449266	18.537114
41.850369	1404.437003	18.542131
42.137078	1402.909347	18.547149
41.860985	1407.266565	18.552167
41.858396	1412.496389	18.557184
42.104343	1416.548266	18.562202
42.100090	1413.980307	18.567219
42.087418	1411.565139	18.572237
42.040619	1418.143073	18.577255
42.197423	1415.215521	18.582272
42.546989	1409.275702	18.587290
42.401719	1409.989666	18.592307
42.504919	1413.508343	18.597325
42.368148	1412.838732	18.602343
42.411505	1414.744632	18.607360
42.527759	1409.910964	18.612378
42.653662	1421.508174	18.617395
42.664935	1404.790236	18.622413
42.388815	1415.616898	18.627431
42.420957	1405.936357	18.632448
42.668322	1409.934363	18.637466
42.605034	1420.611126	18.642483
43.111617	1423.464236	18.647501
42.966955	1425.525644	18.652519
42.533426	1430.273455	18.657536
42.707356	1428.820161	18.662554
42.457936	1440.160238	18.667571
42.612672	1428.961577	18.672589
42.938730	1426.395838	18.677607
42.852013	1445.634869	18.682624
43.099806	1449.206779	18.687642
43.529065	1456.527968	18.692659
43.301538	1443.975003	18.697677
43.462835	1439.336287	18.702695
43.067523	1447.656863	18.707712
43.435169	1448.133178	18.712730
43.566013	1451.988387	18.717747
43.660302	1462.419733	18.722765
43.793309	1457.883248	18.727783
43.675526	1443.198788	18.732800
43.871731	1424.154594	18.737818
43.109708	1433.602085	18.742835
43.393669	1440.141153	18.747853
43.882180	1442.773016	18.752871
44.097061	1456.335102	18.757888
43.976381	1451.721350	18.762906
43.684779	1459.281009	18.767923
44.076018	1451.722057	18.772941
43.907079	1448.425490	18.777959
43.766925	1446.393086	18.782976
44.098453	1444.871072	18.787994
43.766650	1447.687461	18.793011
43.678817	1451.614587	18.798029
43.747128	1448.965897	18.803047
43.640039	1456.108659	18.808064
43.783544	1469.511452	18.813082
43.824072	1474.721958	18.818099
44.286974	1478.086812	18.823117
44.522683	1475.449925	18.828135
44.297604	1472.117913	18.833152
44.638020	1473.147584	18.838170
44.646035	1472.143000	18.843187
44.542682	1472.881999	18.848205
44.855572	1469.917512	18.853223
44.909696	1471.682885	18.858240
44.879118	1465.499275	18.863258
44.903042	1473.325396	18.868275
44.823845	1474.742294	18.873293
44.740005	1474.963853	18.878311
44.614480	1472.124431	18.883328
44.947637	1472.053845	18.888346
44.829034	1474.625602	18.893363
44.810478	1473.921805	18.898381
45.170305	1488.543799	18.903399
45.383423	1497.504979	18.908416
45.131852	1487.679215	18.913434
44.892300	1484.624012	18.918451
45.239780	1490.354782	18.923469
45.553595	1499.234012	18.928487
45.535567	1497.046887	18.933504
45.397460	1481.504016	18.938522
45.419737	1488.345779	18.943539
45.155948	1501.673154	18.948557
45.342508	1493.363404	18.953575
45.242740	1498.056112	18.958592
45.620830	1495.195080	18.963610
45.384765	1503.778070	18.968627
45.408114	1497.349364	18.973645
45.680278	1491.121766	18.978663
45.416894	1497.007608	18.983680
45.560365	1483.955034	18.988698
45.438005	1506.873075	18.993715
45.722056	1514.952207	18.998733
45.960439	1518.096403	19.003751
45.836135	1520.514418	19.008768
46.038018	1517.715531	19.013786
45.901242	1512.346868	19.018803
45.894854	1521.108703	19.023821
46.127311	1514.925148	19.028839
45.769795	1524.660005	19.033856
46.145112	1517.933492	19.038874
45.851174	1523.527451	19.043891
45.921159	1543.417540	19.048909
46.170188	1539.175399	19.053927
45.982996	1553.557562	19.058944
46.071235	1543.786160	19.063962
46.387154	1548.032303	19.068979
45.876496	1555.768121	19.073997
46.476318	1555.075340	19.079015
46.275877	1573.489603	19.084032
46.554889	1562.126342	19.089050
46.646868	1564.343428	19.094067
46.825637	1566.057845	19.099085
47.113751	1563.447500	19.104103
46.983381	1566.443987	19.109120
47.227332	1559.952509	19.114138
46.969281	1559.872985	19.119155
47.103349	1556.642832	19.124173
47.327871	1563.765565	19.129191
47.214286	1565.067901	19.134208
47.366078	1563.829486	19.139226
47.077220	1556.262768	19.144243
47.320183	1563.085980	19.149261
47.415697	1543.902699	19.154279
47.387415	1560.295648	19.159296
47.355446	1561.815655	19.164314
47.419362	1550.631059	19.169331
47.367764	1561.242969	19.174349
47.933541	1573.238857	19.179367
47.590546	1575.533137	19.184384
47.893916	1568.085649	19.189402
47.986441	1563.864713	19.194419
47.580716	1559.405769	19.199437
47.911988	1566.111089	19.204455
47.998617	1579.885744	19.209472
48.166361	1570.278676	19.214490
48.049025	1554.906079	19.219507
47.592830	1560.036155	19.224525
48.325429	1570.421832	19.229543
47.914757	1579.492798	19.234560
48.364531	1571.691149	19.239578
48.613878	1565.321908	19.244595
48.373977	1561.673446	19.249613
48.401840	1545.148455	19.254631
47.984123	1543.919815	19.259648
48.590122	1549.499899	19.264666
48.263028	1546.089081	19.269683
48.244774	1562.111237	19.274701
48.614715	1566.358440	19.279719
48.464673	1564.412770	19.284736
48.422043	1563.292989	19.289754
48.882517	1565.115027	19.294771
48.713147	1564.384213	19.299789
48.807775	1567.724371	19.304807
48.754262	1575.319593	19.309824
48.687623	1575.150305	19.314842
48.788769	1572.730018	19.319859
48.534279	1576.222365	19.324877
48.504063	1557.333204	19.329895
48.875838	1570.965625	19.334912
48.733049	1578.688359	19.339930
48.900192	1583.973859	19.344947
49.125994	1597.098843	19.349965
49.185414	1583.566969	19.354983
49.359382	1594.888561	19.360000
49.093521	1599.941677	19.365018
49.088400	1595.259402	19.370035
49.226436	1598.428703	19.375053
49.309604	1599.444784	19.380071
49.250194	1607.709980	19.385088
49.530678	1604.747361	19.390106
49.936832	1613.593336	19.395123
49.781417	1615.331386	19.400141
49.770498	1602.776142	19.405159
49.436314	1606.482878	19.410176
49.555444	1611.308795	19.415194
49.876824	1616.412498	19.420211
49.866800	1623.246718	19.425229
50.070125	1607.944073	19.430247
49.825569	1616.383269	19.435264
49.545799	1619.516636	19.440282
50.002361	1616.545536	19.445299
49.628320	1620.807600	19.450317
50.125184	1615.535913	19.455335
50.579541	1636.660165	19.460352
50.442565	1642.381203	19.465370
50.637245	1636.881999	19.470387
50.381619	1637.294412	19.475405
50.845393	1626.107474	19.480423
50.688258	1627.432375	19.485440
50.439032	1620.392800	19.490458
50.826794	1617.890011	19.495475
50.886795	1632.079114	19.500493
50.788047	1623.602283	19.505511
50.592433	1625.078344	19.510528
50.378306	1629.567981	19.515546
50.989974	1632.808715	19.520563
50.564247	1628.333932	19.525581
50.851011	1628.646117	19.530599
50.831531	1640.487017	19.535616
50.895928	1632.622265	19.540634
51.143717	1627.234717	19.545651
50.791154	1629.186504	19.550669
51.192336	1636.000889	19.555687
51.160490	1650.750271	19.560704
51.251766	1656.732428	19.565722
51.388844	1652.195260	19.570739
51.597310	1667.049254	19.575757
51.510147	1667.277645	19.580775
51.582335	1666.080019	19.585792
51.115200	1661.409699	19.590810
51.495807	1658.671329	19.595827
51.087405	1665.327745	19.600845
51.892888	1658.979183	19.605863
51.767866	1650.203466	19.610880
51.493356	1659.284831	19.615898
51.563506	1649.967476	19.620915
51.974609	1671.174243	19.625933
51.964551	1677.863320	19.630951
52.093841	1684.622224	19.635968
52.062082	1685.933921	19.640986
52.260543	1681.649126	19.646003
52.320111	1679.162712	19.651021
52.412822	1676.286123	19.656039
52.401336	1687.756571	19.661056
52.290798	1683.387339	19.666074
52.415559	1675.670963	19.671091
52.191610	1685.678607	19.676109
52.264147	1678.863473	19.681127
52.618221	1681.913944	19.686144
52.178867	1683.932899	19.691162
52.386315	1685.421952	19.696179
52.666854	1689.632611	19.701197
52.079780	1681.367484	19.706215
52.213970	1689.025051	19.711232
52.389409	1699.762644	19.716250
52.845729	1705.419732	19.721267
52.756754	1701.782457	19.726285
52.581465	1704.325203	19.731303
52.852483	1710.891633	19.736320
52.908045	1715.134170	19.741338
53.282934	1717.420840	19.746355
53.050297	1728.114686	19.751373
53.298398	1727.243125	19.756391
53.478282	1726.524201	19.761408
53.456731	1726.461503	19.766426
53.358456	1722.809892	19.771443
53.525751	1724.592385	19.776461
53.443253	1721.477973	19.781479
53.183446	1724.254792	19.786496
53.204509	1723.257631	19.791514
53.433835	1737.044904	19.796531
53.403047	1747.325473	19.801549
53.222447	1747.224421	19.806567
53.540582	1737.647499	19.811584
54.042230	1746.576505	19.816602
54.184050	1738.762770	19.821619
53.652396	1736.889119	19.826637
53.606338	1746.045415	19.831655
54.428006	1751.206967	19.836672
54.095374	1769.979693	19.841690
54.520437	1759.426722	19.846707
54.496650	1771.536628	19.851725
54.749209	1766.031529	19.856743
54.767510	1756.223561	19.861760
54.067994	1746.262266	19.866778
54.502044	1751.752419	19.871795
54.891757	1759.698444	19.876813
54.462811	1766.351785	19.881831
54.896840	1764.823253	19.886848
54.246091	1766.439618	19.891866
54.707290	1771.332243	19.896883
54.582134	1770.095906	19.901901
54.932499	1763.884441	19.906919
54.906359	1768.505794	19.911936
54.864976	1772.589865	19.916954
54.710403	1768.571459	19.921971
54.961764	1764.821220	19.926989
55.135666	1786.980264	19.932007
55.324515	1783.312340	19.937024
55.324041	1795.222967	19.942042
55.374172	1787.436110	19.947059
55.442955	1794.548468	19.952077
55.193527	1796.458968	19.957095
55.437245	1790.453451	19.962112
55.312233	1793.206137	19.967130
55.823842	1787.998379	19.972147
55.646741	1783.033554	19.977165
55.859450	1789.839472	19.982183
56.002126	1788.659267	19.987200
55.559992	1789.163838	19.992218
55.974890	1788.891172	19.997235
55.572517	1789.247538	20.002253
55.601365	1787.229809	20.007271
55.619380	1784.626771	20.012288
55.861661	1787.057176	20.017306
55.987879	1797.827739	20.022323
56.149041	1810.382260	20.027341
55.912491	1813.704597	20.032359
56.140337	1812.915084	20.037376
56.180982	1814.474300	20.042394
56.241686	1811.858300	20.047411
56.088740	1809.931990	20.052429
56.172350	1813.491666	20.057447
56.724892	1822.911418	20.062464
56.564727	1834.566061	20.067482
56.651978	1833.413417	20.072499
57.011573	1838.489143	20.077517
56.717662	1838.860181	20.082535
56.773388	1837.213814	20.087552
56.784369	1838.837613	20.092570
57.086362	1831.175629	20.097587
57.058157	1842.494141	20.102605
56.854913	1833.118269	20.107623
56.898540	1826.572675	20.112640
57.030099	1830.298464	20.117658
56.969588	1831.560997	20.122675
57.236345	1844.951195	20.127693
57.141916	1852.003778	20.132711
57.709369	1860.490238	20.137728
57.226470	1863.140861	20.142746
57.468169	1862.462801	20.147763
57.577517	1860.975346	20.152781
57.603088	1857.594768	20.157799
57.717995	1857.400367	20.162816
57.603994	1855.884568	20.167834
57.545585	1857.863166	20.172851
57.868076	1858.630556	20.177869
57.682664	1869.001542	20.182887
58.043848	1879.461008	20.187904
57.650591	1872.273339	20.192922
58.117423	1883.675754	20.197939
58.164206	1879.376656	20.202957
57.998416	1880.242161	20.207975
58.091857	1871.631143	20.212992
58.165967	1872.370931	20.218010
58.224023	1874.410295	20.223027
58.572953	1880.494428	20.228045
58.346382	1884.392755	20.233063
59.079736	1889.927872	20.238080
58.904037	1895.418328	20.243098
59.006279	1887.178330	20.248115
58.904632	1878.070647	20.253133
58.711189	1876.901741	20.258151
58.907360	1866.510580	20.263168
58.670496	1878.372859	20.268186
59.025433	1881.644144	20.273203
58.948289	1878.730849	20.278221
58.569519	1893.272505	20.283239
59.175683	1882.539781	20.288256
59.132511	1887.848649	20.293274
59.045660	1881.241297	20.298291
59.174176	1882.070447	20.303309
58.864609	1887.859462	20.308327
59.650729	1899.761304	20.313344
59.794708	1900.259832	20.318362
60.054837	1899.099204	20.323379
59.946159	1877.094414	20.328397
59.987908	1878.587190	20.333415
59.965254	1877.303328	20.338432
59.882468	1881.393870	20.343450
60.053859	1874.566426	20.348467
59.962140	1871.702740	20.353485
59.546325	1868.545522	20.358503
59.917757	1876.273532	20.363520
59.579304	1880.997191	20.368538
59.927867	1897.233943	20.373555
60.160720	1902.701818	20.378573
59.960038	1902.742751	20.383591
60.403781	1887.588634	20.388608
60.605135	1896.362491	20.393626
60.809249	1900.256885	20.398643
60.942060	1895.922298	20.403661
60.619902	1897.146675	20.408679
60.706447	1890.777419	20.413696
60.734534	1891.780002	20.418714
60.723732	1892.681338	20.423731
60.897868	1898.764288	20.428749
60.897944	1899.947963	20.433767
60.718246	1884.764678	20.438784
60.764977	1898.542635	20.443802
60.725244	1910.664586	20.448819
61.271608	1913.852422	20.453837
61.200949	1916.795488	20.458855
61.370033	1926.136137	20.463872
61.276607	1917.913966	20.468890
61.339391	1920.555380	20.473907
61.626774	1925.440395	20.478925
61.363080	1927.409936	20.483943
61.426482	1930.739244	20.488960
61.670165	1925.888753	20.493978
62.026290	1923.160466	20.498995
61.886960	1910.893251	20.504013
61.509973	1921.003752	20.509031
61.632479	1918.665301	20.514048
61.699263	1918.440522	20.519066
62.007166	1938.555950	20.524083
61.694439	1940.599400	20.529101
61.684757	1941.614178	20.534119
62.130087	1931.853241	20.539136
62.063069	1941.846062	20.544154
61.964223	1939.756675	20.549171
61.892337	1932.743016	20.554189
62.038112	1949.336449	20.559207
62.274678	1955.084638	20.564224
62.034077	1963.498134	20.569242
62.209130	1968.820388	20.574259
62.566710	1964.466569	20.579277
62.249380	1977.427078	20.584295
62.906778	1983.636795	20.589312
62.930013	1981.291701	20.594330
62.904669	1987.528821	20.599347
63.055086	1994.625393	20.604365
63.148034	1996.419489	20.609383
63.209713	1986.080757	20.614400
63.152544	1986.004669	20.619418
63.270734	1990.802431	20.624435
63.369197	1981.780309	20.629453
63.183663	1988.105488	20.634471
63.530344	1989.292011	20.639488
63.262046	1978.427125	20.644506
63.482804	1994.185229	20.649523
63.551986	1975.687265	20.654541
63.522644	1983.499812	20.659559
63.700017	1983.971052	20.664576
63.809071	1979.870526	20.669594
63.683152	1995.124008	20.674611
63.806424	1987.833780	20.679629
63.995945	2003.590443	20.684647
64.303265	2009.046757	20.689664
64.188027	2000.370334	20.694682
63.960060	2003.410492	20.699699
64.366159	1999.374170	20.704717
64.344884	2009.025379	20.709735
64.170879	1998.496108	20.714752
64.395804	2000.787228	20.719770
64.370144	2001.236430	20.724787
64.369777	1991.109335	20.729805
64.606870	1996.664945	20.734823
64.405845	1990.750697	20.739840
64.527060	1998.271555	20.744858
64.512737	2008.568647	20.749875
64.732381	2018.854563	20.754893
64.389330	2019.277439	20.759911
64.673767	2018.507510	20.764928
65.109194	2022.788811	20.769946
64.778258	2018.236052	20.774963
65.324005	2028.243975	20.779981
65.411827	2042.003020	20.784999
65.319630	2045.653234	20.790016
65.477332	2027.700035	20.795034
65.530491	2038.469494	20.800051
65.655597	2032.646472	20.805069
65.562035	2036.461005	20.810087
65.303893	2043.577025	20.815104
65.614781	2037.835534	20.820122
65.420849	2034.634271	20.825139
65.809263	2028.748163	20.830157
65.750859	2036.060308	20.835175
65.828153	2045.415312	20.840192
66.111229	2048.227581	20.845210
65.907436	2054.479884	20.850227
66.390119	2058.823267	20.855245
66.452896	2056.345770	20.860263
66.538309	2056.736652	20.865280
66.557985	2059.586777	20.870298
66.517628	2062.042290	20.875315
66.424280	2057.723940	20.880333
66.042751	2058.285357	20.885351
66.075979	2059.063077	20.890368
66.520556	2048.901389	20.895386
66.355073	2067.967153	20.900403
66.790525	2071.989675	20.905421
66.816313	2076.950177	20.910439
66.618205	2080.815712	20.915456
66.636519	2077.830715	20.920474
66.909788	2085.069149	20.925491
67.160198	2077.689659	20.930509
67.065729	2093.585296	20.935527
67.144160	2101.308528	20.940544
67.455740	2106.170890	20.945562
67.350932	2115.358613	20.950579
67.464122	2108.338162	20.955597
67.615729	2108.141201	20.960615
67.909875	2108.076688	20.965632
67.550487	2099.867439	20.970650
67.479789	2101.384053	20.975667
67.507830	2095.847535	20.980685
67.614101	2100.738705	20.985703
67.726592	2100.465780	20.990720
68.252023	2116.889799	20.995738
67.880671	2127.898984	21.000755
68.476648	2116.201986	21.005773
68.291050	2122.003334	21.010791
68.007316	2116.322839	21.015808
68.335863	2114.425676	21.020826
68.328133	2118.810713	21.025843
68.286306	2114.364402	21.030861
68.287397	2112.234187	21.035879
68.212944	2119.548866	21.040896
68.840391	2118.728683	21.045914
68.477491	2135.085891	21.050931
68.683763	2138.961066	21.055949
68.748984	2142.937101	21.060967
68.854012	2145.609842	21.065984
69.032442	2135.631561	21.071002
68.825843	2135.935360	21.076019
69.192698	2132.097632	21.081037
69.246428	2137.874348	21.086055
69.366423	2142.706585	21.091072
69.581851	2139.182781	21.096090
69.446490	2146.570072	21.101107
69.125431	2144.499478	21.106125
69.867380	2153.463863	21.111143
69.627093	2163.158721	21.116160
70.129365	2159.795390	21.121178
70.310892	2159.887274	21.126195
70.288893	2161.784493	21.131213
70.135041	2147.954022	21.136231
70.072327	2144.198953	21.141248
70.253158	2152.742592	21.146266
70.040040	2147.467678	21.151283
70.348734	2159.822742	21.156301
70.463337	2160.035504	21.161319
70.179814	2176.819069	21.166336
70.620718	2160.756247	21.171354
70.224987	2170.876118	21.176371
70.038204	2157.221189	21.181389
70.363679	2158.265851	21.186407
69.971079	2174.321591	21.191424
70.801242	2183.171266	21.196442
70.388327	2190.642816	21.201459
70.779878	2191.980166	21.206477
70.674723	2188.376870	21.211495
70.561242	2186.876741	21.216512
70.744170	2197.433578	21.221530
70.666984	2209.141820	21.226547
70.873487	2211.704093	21.231565
71.500681	2203.492676	21.236583
71.150663	2219.964726	21.241600
71.003849	2221.581568	21.246618
71.470691	2232.599177	21.251635
71.220992	2238.647241	21.256653
71.563579	2236.069347	21.261671
71.686445	2238.158626	21.266688
71.842822	2231.210301	21.271706
71.869080	2232.664492	21.276723
71.986494	2243.304143	21.281741
72.288448	2254.596760	21.286759
72.246655	2258.851427	21.291776
72.834205	2256.973888	21.296794
72.822305	2243.380032	21.301811
72.332205	2228.907537	21.306829
72.609984	2217.941704	21.311847
72.392612	2224.590675	21.316864
72.626012	2225.356173	21.321882
72.625232	2223.115778	21.326899
72.539721	2222.375035	21.331917
72.840309	2238.111457	21.336935
73.000323	2241.435249	21.341952
73.464174	2234.694685	21.346970
73.126707	2230.764614	21.351987
72.602019	2224.058037	21.357005
72.973534	2228.459798	21.362023
73.124758	2241.019325	21.367040
73.013855	2243.990802	21.372058
72.991285	2236.117233	21.377075
73.109953	2244.465457	21.382093
73.209801	2252.794522	21.387111
73.344094	2261.130852	21.392128
74.020669	2258.160109	21.397146
73.317481	2269.312568	21.402163
73.675049	2271.655659	21.407181
73.505031	2264.474102	21.412199
73.536363	2273.539719	21.417216
73.683687	2268.868249	21.422234
73.829316	2291.335293	21.427251
74.081617	2287.679479	21.432269
74.108282	2289.603852	21.437287
74.004845	2298.823015	21.442304
74.275177	2288.420064	21.447322
74.589387	2291.896593	21.452339
74.155684	2299.633371	21.457357
74.525906	2305.556535	21.462375
74.631810	2320.177719	21.467392
75.048091	2314.009453	21.472410
74.983032	2319.435472	21.477427
75.008908	2312.668390	21.482445
75.504711	2315.207727	21.487463
74.807580	2321.937742	21.492480
74.490448	2316.275006	21.497498
74.890582	2316.938805	21.502515
74.572230	2312.005292	21.507533
74.833188	2324.203791	21.512551
75.118488	2331.367864	21.517568
75.474972	2346.369801	21.522586
75.865726	2340.120289	21.527603
75.891055	2330.809559	21.532621
76.128450	2331.937378	21.537639
75.995823	2338.339654	21.542656
76.061062	2332.869859	21.547674
75.844380	2340.273047	21.552691
75.600859	2338.875207	21.557709
76.151720	2341.497500	21.562727
76.335392	2354.427618	21.567744
76.388166	2358.910597	21.572762
76.632111	2353.999986	21.577779
76.455495	2360.866738	21.582797
76.678906	2363.858771	21.587815
76.368375	2359.539447	21.592832
76.345267	2357.447686	21.597850
76.807413	2347.071645	21.602867
76.706965	2354.803900	21.607885
76.858762	2349.106016	21.612903
76.606119	2347.334034	21.617920
77.196002	2345.951613	21.622938
77.194534	2344.017441	21.627955
76.783941	2349.812865	21.632973
77.279690	2349.477109	21.637991
77.248059	2364.002970	21.643008
77.306171	2362.946354	21.648026
77.292040	2368.149850	21.653043
77.255461	2370.320778	21.658061
77.580499	2364.561200	21.663079
77.539336	2366.698124	21.668096
78.134910	2367.205256	21.673114
77.934467	2356.676734	21.678131
77.779967	2361.460245	21.683149
77.909107	2359.139641	21.688167
77.694617	2364.721491	21.693184
78.100575	2378.999343	21.698202
78.187017	2383.120459	21.703219
78.330810	2383.590627	21.708237
78.291959	2380.033777	21.713255
78.374215	2393.169072	21.718272
78.365448	2389.784273	21.723290
78.697041	2388.249547	21.728307
78.353197	2390.850192	21.733325
78.686139	2389.185861	21.738343
78.681330	2403.777010	21.743360
78.776130	2404.661931	21.748378
78.968338	2409.940618	21.753395
78.807188	2415.612015	21.758413
79.100323	2407.758649	21.763431
79.003302	2402.001652	21.768448
79.385412	2410.914888	21.773466
79.651066	2416.302070	21.778483
79.403349	2426.496875	21.783501
79.838735	2430.282789	21.788519
79.815875	2429.620652	21.793536
79.828035	2431.670382	21.798554
79.878725	2423.419229	21.803571
79.754114	2434.112456	21.808589
79.690958	2437.224862	21.813607
80.129384	2430.011628	21.818624
80.266318	2432.862492	21.823642
80.407946	2424.827568	21.828659
80.108006	2433.121126	21.833677
80.185533	2421.694010	21.838695
80.296296	2421.254081	21.843712
80.071695	2438.492650	21.848730
80.360345	2448.815411	21.853747
80.458945	2453.442767	21.858765
80.789759	2444.914446	21.863783
80.858627	2450.165008	21.868800
80.827541	2446.054635	21.873818
81.431226	2440.844978	21.878835
81.249855	2445.872552	21.883853
81.397299	2441.825907	21.888871
81.386205	2443.737239	21.893888
81.643836	2450.839392	21.898906
81.655595	2444.276443	21.903923
81.566616	2443.400523	21.908941
81.556425	2453.776127	21.913959
81.913384	2458.224395	21.918976
81.560193	2461.107390	21.923994
82.044912	2459.315273	21.929011
81.749255	2456.470622	21.934029
81.729129	2451.197130	21.939047
82.034867	2457.303965	21.944064
81.656466	2461.819386	21.949082
82.096020	2464.982925	21.954099
81.920800	2479.531235	21.959117
81.877602	2486.806481	21.964135
82.553695	2478.653603	21.969152
82.366937	2483.754614	21.974170
82.603278	2480.158054	21.979187
82.401437	2485.681164	21.984205
82.872401	2495.142379	21.989223
83.021918	2498.508882	21.994240
83.218907	2508.568219	21.999258
83.152185	2503.406115	22.004275
82.780450	2512.559856	22.009293
83.002148	2499.734220	22.014311
82.938493	2501.704238	22.019328
82.870201	2509.097016	22.024346
83.078647	2501.594489	22.029363
82.919948	2519.902233	22.034381
83.294616	2524.243612	22.039399
83.490002	2526.599364	22.044416
83.334940	2532.497083	22.049434
83.900634	2533.955679	22.054451
83.906836	2560.547599	22.059469
83.545333	2551.587336	22.064487
83.986592	2549.208645	22.069504
84.123002	2556.323402	22.074522
84.386960	2546.498846	22.079539
84.398501	2545.506278	22.084557
84.272761	2540.691046	22.089575
84.548566	2542.693429	22.094592
84.223250	2548.018016	22.099610
84.733436	2574.907058	22.104627
84.632151	2577.457340	22.109645
84.383995	2573.109315	22.114663
84.617255	2572.685027	22.119680
84.963639	2579.678732	22.124698
85.277568	2591.026506	22.129715
85.100027	2595.018345	22.134733
85.189730	2601.184114	22.139751
85.088375	2603.232601	22.144768
85.409539	2600.752671	22.149786
85.349524	2599.935355	22.154803
85.469031	2606.620387	22.159821
85.637243	2601.699407	22.164839
86.035635	2614.665715	22.169856
86.004943	2625.174008	22.174874
86.331953	2618.066414	22.179891
86.234366	2624.561174	22.184909
86.373867	2619.931859	22.189927
86.265479	2623.420597	22.194944
86.128065	2622.050399	22.199962
86.300604	2625.381781	22.204979
86.155405	2626.957379	22.209997
86.362732	2630.258097	22.215015
86.416106	2624.559670	22.220032
86.612355	2646.163992	22.225050
86.795028	2645.706549	22.230067
86.620840	2645.557151	22.235085
86.653057	2648.364390	22.240103
86.903951	2643.275880	22.245120
86.842119	2660.214743	22.250138
87.317924	2664.294239	22.255155
87.429052	2672.119932	22.260173
87.583991	2671.067158	22.265191
87.797872	2661.477572	22.270208
87.515083	2673.748343	22.275226
87.789402	2662.255719	22.280243
87.588574	2669.808064	22.285261
87.335520	2674.607002	22.290279
87.844188	2673.306636	22.295296
87.975309	2689.719986	22.300314
87.955104	2683.745794	22.305331
88.157398	2685.775419	22.310349
88.273968	2690.848198	22.315367
88.555326	2679.401808	22.320384
88.319244	2674.436449	22.325402
88.672820	2676.900146	22.330419
88.354154	2691.379436	22.335437
89.011503	2705.993979	22.340455
89.131843	2700.105207	22.345472
89.077562	2709.001322	22.350490
88.974909	2708.506245	22.355507
88.989805	2706.152886	22.360525
88.913740	2706.834033	22.365543
89.359670	2703.056463	22.370560
88.844886	2713.043683	22.375578
89.185945	2709.089920	22.380595
89.403163	2726.424091	22.385613
89.121555	2723.274227	22.390631
89.835738	2729.506927	22.395648
89.723317	2716.878335	22.400666
90.071277	2721.378568	22.405683
90.015682	2725.840639	22.410701
89.978053	2724.328655	22.415719
89.882020	2716.797699	22.420736
90.154357	2730.459113	22.425754
90.526613	2737.511973	22.430771
90.575732	2742.465871	22.435789
90.308643	2741.945897	22.440807
90.506525	2744.244480	22.445824
90.486261	2746.305606	22.450842
90.475021	2739.948117	22.455859
90.944129	2746.313661	22.460877
91.132229	2754.910110	22.465895
90.902361	2765.755632	22.470912
90.852222	2769.361572	22.475930
90.972791	2760.020010	22.480947
90.916721	2761.581743	22.485965
91.186540	2762.306878	22.490983
91.577644	2778.531496	22.496000
91.403152	2784.331329	22.501018
91.460110	2793.080768	22.506035
91.698413	2789.647957	22.511053
91.497511	2790.279110	22.516071
92.074552	2801.403000	22.521088
92.422008	2822.327530	22.526106
92.565857	2817.785858	22.531123
92.739545	2814.123241	22.536141
92.263438	2808.153712	22.541159
92.597445	2801.837130	22.546176
92.751442	2809.952880	22.551194
92.690527	2813.071315	22.556211
92.795239	2814.046238	22.561229
92.570450	2817.297495	22.566247
92.690903	2810.543904	22.571264
92.554869	2813.680347	22.576282
92.644403	2818.905707	22.581299
92.685884	2829.507032	22.586317
93.038629	2838.358777	22.591335
93.100452	2825.393685	22.596352
93.551920	2838.806366	22.601370
93.515793	2851.408116	22.606387
93.782520	2857.041438	22.611405
93.697614	2856.139615	22.616423
93.826903	2842.630629	22.621440
93.613635	2852.795063	22.626458
93.902795	2843.092665	22.631475
93.898027	2841.124236	22.636493
94.004724	2860.385170	22.641511
94.567663	2860.569168	22.646528
94.581393	2861.621381	22.651546
94.479266	2872.264027	22.656563
94.547419	2859.266364	22.661581
94.619113	2868.717351	22.666599
94.766165	2863.764878	22.671616
94.908448	2874.126454	22.676634
94.651393	2865.509565	22.681651
94.831267	2861.034863	22.686669
94.952308	2884.992993	22.691687
94.950450	2890.898538	22.696704
95.055043	2887.836852	22.701722
95.449482	2887.990274	22.706739
95.869109	2885.277207	22.711757
95.956077	2883.654284	22.716775
96.327490	2867.377570	22.721792
96.234540	2879.994498	22.726810
96.091138	2873.468174	22.731827
96.400147	2873.079427	22.736845
96.242481	2864.264011	22.741863
96.267269	2866.952509	22.746880
96.121539	2868.076891	22.751898
95.954855	2869.166662	22.756915
96.633978	2874.738939	22.761933
96.128514	2874.821013	22.766951
96.666522	2886.146711	22.771968
96.799206	2900.729482	22.776986
97.146698	2891.854339	22.782003
96.853566	2896.110417	22.787021
96.855529	2899.938665	22.792039
97.357811	2891.345563	22.797056
97.082898	2892.117641	22.802074
97.068047	2892.767171	22.807091
97.375817	2905.558435	22.812109
97.154753	2911.406588	22.817127
97.262546	2910.291707	22.822144
97.563642	2915.888136	22.827162
97.480076	2923.431799	22.832179
97.771882	2935.625912	22.837197
97.811883	2946.407434	22.842215
98.028689	2948.965053	22.847232
98.012709	2949.731537	22.852250
97.839116	2944.308209	22.857267
98.433898	2967.280580	22.862285
98.328661	2973.868183	22.867303
98.331700	2971.478763	22.872320
98.499243	2975.410647	22.877338
98.660255	2978.065329	22.882355
98.639557	2990.194514	22.887373
98.846192	2993.407036	22.892391
99.020189	2993.632655	22.897408
99.306317	2998.783274	22.902426
99.312826	2997.371703	22.907443
99.390813	2997.236693	22.912461
98.984868	3009.050295	22.917479
99.408265	3010.796200	22.922496
99.708413	3017.866711	22.927514
99.784557	3022.488242	22.932531
99.751346	3016.844201	22.937549
99.583290	3026.449375	22.942567
100.033886	3033.076705	22.947584
100.055688	3041.096365	22.952602
99.800842	3043.456005	22.957619
100.194953	3040.860507	22.962637
100.000349	3061.831839	22.967655
100.632968	3064.356296	22.972672
100.887106	3074.858379	22.977690
100.594657	3068.961163	22.982707
101.399054	3062.839524	22.987725
101.181667	3070.953248	22.992743
101.170510	3065.498280	22.997760
100.944878	3064.637293	23.002778
101.565329	3070.745838	23.007795
101.457545	3061.881529	23.012813
101.525779	3069.269062	23.017831
101.426426	3081.634639	23.022848
101.650702	3078.459603	23.027866
101.583597	3086.676181	23.032883
101.562716	3082.478858	23.037901
101.560380	3090.625386	23.042919
101.784179	3088.192112	23.047936
102.029276	3104.367167	23.052954
102.159336	3103.876876	23.057971
102.336738	3106.071386	23.062989
102.266316	3113.644643	23.068007
102.361812	3112.948273	23.073024
102.738755	3119.448233	23.078042
103.061287	3131.195838	23.083059
102.708563	3125.361642	23.088077
102.977118	3138.064493	23.093095
102.989970	3135.736646	23.098112
103.274145	3129.399304	23.103130
103.066290	3131.499149	23.108147
103.327040	3124.931903	23.113165
103.602960	3143.235736	23.118183
104.025267	3153.171983	23.123200
104.016732	3152.744298	23.128218
103.891076	3159.290963	23.133235
104.336172	3158.104614	23.138253
104.019797	3156.181510	23.143271
104.161589	3154.272288	23.148288
104.261814	3153.748767	23.153306
104.113260	3151.092561	23.158323
104.497250	3149.069883	23.163341
104.334219	3160.814203	23.168359
104.117743	3170.310215	23.173376
104.154014	3173.574544	23.178394
104.412506	3190.785960	23.183411
104.597935	3198.972739	23.188429
104.557640	3215.627875	23.193447
105.082791	3210.341856	23.198464
105.061604	3213.602513	23.203482
105.248828	3235.963268	23.208499
105.425169	3231.085038	23.213517
105.148264	3234.319233	23.218535
105.555386	3235.256566	23.223552
106.015169	3238.944171	23.228570
106.015641	3259.238350	23.233587
106.196487	3253.052766	23.238605
105.908874	3248.811717	23.243623
105.906540	3255.241375	23.248640
106.253837	3246.148315	23.253658
106.429173	3255.264599	23.258675
106.815390	3257.142564	23.263693
107.375778	3269.992597	23.268711
106.869718	3269.711806	23.273728
107.130824	3258.804747	23.278746
107.060960	3274.460886	23.283763
107.321763	3268.224975	23.288781
107.429858	3264.591417	23.293799
107.287538	3264.014127	23.298816
107.586596	3264.087720	23.303834
107.249775	3283.358193	23.308851
107.483907	3265.193021	23.313869
107.327789	3271.454103	23.318887
107.237115	3289.139744	23.323904
107.882389	3292.937352	23.328922
107.908848	3294.855552	23.333939
108.092578	3294.675671	23.338957
108.316124	3309.670708	23.343975
108.382000	3314.716839	23.348992
108.570738	3313.084346	23.354010
108.624640	3314.900434	23.359027
108.525231	3316.456338	23.364045
108.712019	3321.720358	23.369063
108.693266	3314.549546	23.374080
108.824601	3315.368857	23.379098
108.929324	3335.814167	23.384115
109.106449	3337.506920	23.389133
108.815895	3343.205067	23.394151
108.868515	3338.810027	23.399168
109.468207	3356.527120	23.404186
109.573263	3363.252558	23.409203
109.639961	3363.018306	23.414221
109.794055	3365.191228	23.419239
109.875837	3360.469713	23.424256
109.840788	3358.711093	23.429274
110.142546	3377.790715	23.434291
110.061879	3385.731797	23.439309
110.233476	3395.912364	23.444327
110.466793	3387.304093	23.449344
110.965316	3387.368725	23.454362
110.407374	3387.468438	23.459379
110.602043	3401.798939	23.464397
111.302480	3405.291302	23.469415
110.959648	3408.321173	23.474432
111.305232	3405.666900	23.479450
111.197907	3401.864858	23.484467
111.346523	3403.009725	23.489485
111.584564	3412.561346	23.494503
111.720933	3420.440247	23.499520
111.942882	3425.582044	23.504538
111.966148	3420.617130	23.509555
112.235188	3430.236526	23.514573
112.344619	3425.861025	23.519591
112.116179	3423.315058	23.524608
112.194056	3421.482039	23.529626
111.964392	3429.515774	23.534643
112.553056	3439.988080	23.539661
112.682599	3440.331092	23.544679
112.435721	3444.485411	23.549696
112.851374	3437.379476	23.554714
112.853271	3456.748895	23.559731
113.077244	3469.402110	23.564749
113.047173	3467.317617	23.569767
113.294623	3473.891522	23.574784
113.535012	3462.703509	23.579802
113.152573	3472.389641	23.584819
113.725678	3490.660183	23.589837
113.780110	3491.848125	23.594855
113.953677	3496.382018	23.599872
114.366267	3491.558466	23.604890
113.992385	3500.391108	23.609907
114.386874	3493.888123	23.614925
114.258469	3496.931966	23.619943
114.322193	3509.496537	23.624960
114.510599	3516.884480	23.629978
115.139841	3522.190139	23.634995
115.023546	3521.129046	23.640013
115.347749	3512.670688	23.645031
115.058137	3522.459173	23.650048
115.124387	3509.641240	23.655066
115.189050	3517.761750	23.660083
115.680487	3524.745867	23.665101
115.581745	3534.804480	23.670119
115.624418	3542.817958	23.675136
115.985507	3543.412137	23.680154
115.694087	3533.913384	23.685171
115.611133	3547.709642	23.690189
115.843461	3537.024673	23.695207
115.764521	3549.639889	23.700224
115.693053	3557.582771	23.705242
116.138310	3561.266393	23.710259
116.194342	3565.032708	23.715277
116.280380	3574.276680	23.720295
116.446539	3591.493387	23.725312
116.438157	3581.126772	23.730330
116.640576	3596.876515	23.735347
116.810649	3608.190518	23.740365
117.253547	3605.682032	23.745383
117.126818	3613.715603	23.750400
117.159714	3611.536072	23.755418
117.532952	3617.370830	23.760435
117.373518	3631.747177	23.765453
117.698309	3637.314894	23.770471
117.602427	3636.515739	23.775488
118.051023	3636.310399	23.780506
118.085071	3652.373620	23.785523
118.087155	3658.528144	23.790541
118.590213	3651.058176	23.795559
118.868312	3652.852018	23.800576
118.897029	3651.967183	23.805594
119.027576	3643.248542	23.810611
119.072034	3648.121353	23.815629
119.488494	3636.006297	23.820647
119.329392	3639.869248	23.825664
119.645231	3635.739307	23.830682
119.956126	3629.514410	23.835699
119.603271	3633.082435	23.840717
119.927115	3628.995436	23.845735
119.758475	3638.664151	23.850752
119.692885	3637.203787	23.855770
120.022216	3647.823902	23.860787
119.880997	3656.156433	23.865805
119.754801	3659.480863	23.870823
119.936293	3665.727393	23.875840
120.599807	3678.287072	23.880858
120.728462	3690.475537	23.885875
120.743894	3687.699034	23.890893
120.837845	3683.688846	23.895911
120.750534	3685.861518	23.900928
121.018539	3682.808974	23.905946
121.097561	3691.747945	23.910963
121.036182	3704.123818	23.915981
121.323087	3712.923121	23.920999
121.481137	3716.831397	23.926016
121.449443	3704.079075	23.931034
121.946709	3726.401636	23.936051
121.760566	3730.196223	23.941069
121.740429	3726.860285	23.946087
121.979962	3717.831110	23.951104
122.494345	3725.828040	23.956122
122.418855	3736.675359	23.961139
122.368700	3750.570821	23.966157
122.635251	3752.997718	23.971175
122.604575	3758.112662	23.976192
123.025215	3748.995306	23.981210
122.828092	3750.777928	23.986227
122.721283	3768.188802	23.991245
123.209024	3765.695406	23.996263
123.213414	3774.728100	24.001280
123.069371	3776.931708	24.006298
123.094783	3784.158921	24.011315
123.415285	3799.606395	24.016333
123.720221	3797.605424	24.021351
123.473440	3810.953952	24.026368
123.679055	3815.618655	24.031386
123.891475	3828.715797	24.036403
123.895553	3828.314538	24.041421
124.068457	3838.476215	24.046439
123.953565	3857.712747	24.051456
124.667703	3841.605891	24.056474
125.372548	3837.882464	24.061491
125.148065	3840.445792	24.066509
125.429316	3843.870945	24.071527
125.459592	3837.304605	24.076544
125.945017	3829.610060	24.081562
126.053786	3827.216690	24.086579
125.944343	3830.630074	24.091597
125.656052	3822.977088	24.096615
126.077217	3825.663985	24.101632
126.139430	3822.425677	24.106650
126.353344	3821.199531	24.111667
126.458876	3835.124475	24.116685
126.600517	3839.754957	24.121703
126.490921	3855.673442	24.126720
126.881164	3847.226739	24.131738
126.936759	3846.309303	24.136755
126.706215	3846.222324	24.141773
127.026671	3845.295214	24.146791
126.553524	3854.209765	24.151808
126.745477	3856.455759	24.156826
127.235540	3878.445068	24.161843
127.141051	3880.628349	24.166861
127.374909	3885.746331	24.171879
127.378156	3898.778246	24.176896
127.226246	3903.653292	24.181914
127.529162	3900.996122	24.186931
127.553478	3922.401496	24.191949
127.798478	3926.637156	24.196967
128.148080	3936.124342	24.201984
128.503178	3947.889505	24.207002
128.540492	3957.425324	24.212019
128.252471	3961.636666	24.217037
128.866145	3956.005241	24.222055
128.903090	3967.561137	24.227072
129.260667	3975.443715	24.232090
129.103501	3972.848697	24.237107
128.863535	3984.324621	24.242125
129.177400	3985.885677	24.247143
129.373939	4005.717759	24.252160
129.862989	4006.418283	24.257178
129.869787	3999.508349	24.262195
129.830506	4006.205998	24.267213
129.877116	4016.838787	24.272231
130.235076	4028.881310	24.277248
130.353719	4017.872879	24.282266
130.863264	4019.539192	24.287283
130.416346	4034.834909	24.292301
130.999330	4049.503160	24.297319
130.839389	4056.951873	24.302336
131.028514	4058.866923	24.307354
131.461485	4052.733345	24.312371
131.201314	4064.161965	24.317389
131.393613	4070.646831	24.322407
131.846833	4081.591950	24.327424
131.705143	4079.291199	24.332442
131.984815	4087.605743	24.337459
132.108089	4079.323593	24.342477
131.966730	4076.359969	24.347495
132.199080	4086.430466	24.352512
132.197362	4099.333891	24.357530
132.675947	4100.859842	24.362547
132.388009	4101.684498	24.367565
132.398815	4102.380577	24.372583
132.529390	4117.595921	24.377600
132.389218	4119.533840	24.382618
132.690020	4127.756736	24.387635
132.667222	4143.008606	24.392653
132.867910	4140.209502	24.397671
133.676357	4145.945111	24.402688
133.715950	4151.778332	24.407706
134.182037	4156.049064	24.412723
134.115753	4157.464161	24.417741
134.314740	4153.576394	24.422759
134.306448	4159.293977	24.427776
134.031066	4170.958599	24.432794
134.547364	4163.416923	24.437811
134.671954	4170.057556	24.442829
134.635105	4179.380941	24.447847
134.831263	4178.369008	24.452864
134.643233	4191.263630	24.457882
135.170226	4181.599239	24.462899
134.899046	4207.116284	24.467917
135.364486	4209.048300	24.472935
135.476892	4212.875413	24.477952
135.254246	4209.173219	24.482970
135.734425	4223.150604	24.487987
135.718377	4234.320380	24.493005
135.941331	4239.433848	24.498023
136.152337	4239.978823	24.503040
136.333371	4260.441707	24.508058
136.569889	4261.115277	24.513075
136.838629	4262.200465	24.518093
136.722795	4265.756960	24.523111
137.097025	4263.262233	24.528128
137.197895	4269.186954	24.533146
137.516500	4276.706442	24.538163
137.295756	4289.527319	24.543181
137.501085	4281.951944	24.548199
137.560632	4280.841335	24.553216
137.712484	4278.122409	24.558234
138.059089	4294.497360	24.563251
137.887108	4308.462719	24.568269
138.212266	4299.666118	24.573287
138.164541	4309.123828	24.578304
138.146471	4315.133365	24.583322
138.205415	4318.656347	24.588339
138.336048	4332.906025	24.593357
138.432250	4331.044810	24.598375
139.091817	4340.496577	24.603392
139.491419	4342.918621	24.608410
139.774730	4339.055562	24.613427
139.638249	4347.943189	24.618445
139.773500	4345.895982	24.623463
139.681226	4339.998745	24.628480
139.884180	4345.737155	24.633498
140.343711	4352.019544	24.638515
140.313899	4365.246322	24.643533
140.416078	4368.342789	24.648551
140.435462	4365.799135	24.653568
140.510831	4371.358568	24.658586
140.507978	4375.402510	24.663603
140.540637	4395.109030	24.668621
140.808806	4391.137845	24.673639
140.888786	4393.470780	24.678656
141.283291	4408.449584	24.683674
141.303297	4407.228338	24.688691
141.356181	4416.234864	24.693709
141.234124	4422.812989	24.698727
141.688483	4424.891946	24.703744
141.857751	4453.273016	24.708762
142.221255	4446.351564	24.713779
142.079886	4455.593516	24.718797
142.107907	4454.181638	24.723815
142.864802	4463.567814	24.728832
142.646469	4466.846766	24.733850
142.808016	4471.288086	24.738867
142.717285	4471.504440	24.743885
142.906034	4472.485310	24.748903
142.817817	4474.951758	24.753920
142.946470	4495.094801	24.758938
143.194543	4486.587871	24.763955
143.518531	4494.706322	24.768973
143.268065	4504.243045	24.773991
143.840312	4506.859178	24.779008
143.798514	4520.725522	24.784026
144.457711	4519.824550	24.789043
144.233793	4534.697734	24.794061
144.300254	4545.236207	24.799079
144.511261	4544.083063	24.804096
144.169519	4552.949089	24.809114
144.522344	4552.411452	24.814131
144.698223	4565.862019	24.819149
144.860292	4574.614896	24.824167
145.244532	4584.024434	24.829184
145.227156	4593.354469	24.834202
145.735521	4591.037666	24.839219
145.602966	4602.124804	24.844237
145.984182	4612.235546	24.849255
146.262514	4607.003334	24.854272
146.278276	4609.564086	24.859290
146.332585	4612.298750	24.864307
146.819697	4617.175502	24.869325
147.070815	4631.485566	24.874343
147.659547	4619.990095	24.879360
147.558410	4622.821559	24.884378
148.024349	4614.397436	24.889395
147.734502	4605.936324	24.894413
147.903538	4610.177660	24.899431
148.031928	4615.227047	24.904448
148.186165	4627.661517	24.909466
148.222350	4615.702863	24.914483
148.405196	4612.874901	24.919501
148.055722	4608.507435	24.924519
148.424182	4608.393475	24.929536
148.226342	4608.345587	24.934554
148.235673	4623.981095	24.939571
149.084647	4625.206385	24.944589
148.809172	4640.011929	24.949607
148.831883	4641.088100	24.954624
149.048065	4647.146498	24.959642
149.274906	4649.655454	24.964659
149.587364	4662.658716	24.969677
149.562163	4662.808054	24.974695
149.608718	4670.565759	24.979712
149.686969	4687.494184	24.984730
150.238033	4688.633291	24.989747
150.503399	4683.232631	24.994765
150.301533	4690.590283	24.999783
150.885568	4700.066624	25.004800
150.473791	4712.415673	25.009818
150.580249	4717.452722	25.014835
150.895451	4711.059497	25.019853
151.109208	4731.176927	25.024871
151.180520	4729.448960	25.029888
151.070586	4737.240527	25.034906
151.774320	4742.140402	25.039923
151.723222	4754.269192	25.044941
151.675799	4762.259360	25.049959
151.614187	4758.386787	25.054976
152.098904	4776.855468	25.059994
152.545593	4778.484294	25.065011
152.703700	4778.690317	25.070029
152.767804	4782.389345	25.075047
153.045915	4778.476501	25.080064
152.976001	4784.355383	25.085082
152.945329	4780.891478	25.090099
153.154278	4788.797554	25.095117
153.472218	4804.975420	25.100135
153.162895	4807.195416	25.105152
153.394060	4819.472845	25.110170
153.620133	4822.670045	25.115187
153.647557	4828.877837	25.120205
153.618002	4833.882435	25.125223
154.341561	4847.740344	25.130240
154.189202	4847.050933	25.135258
154.298149	4848.827042	25.140275
154.426216	4858.813201	25.145293
154.550982	4875.188496	25.150311
154.572621	4872.202520	25.155328
154.578570	4887.538921	25.160346
155.032527	4893.907590	25.165363
155.079101	4905.696162	25.170381
155.661946	4918.225078	25.175399
155.847230	4914.386630	25.180416
155.883748	4921.457902	25.185434
156.180063	4935.300329	25.190451
156.764238	4950.313182	25.195469
156.622342	4949.243364	25.200487
157.129030	4938.779998	25.205504
157.125153	4941.659498	25.210522
156.897696	4950.097586	25.215539
157.234346	4963.334031	25.220557
157.479625	4969.656306	25.225575
157.472872	4962.233613	25.230592
157.545317	4971.729775	25.235610
157.463955	4976.527840	25.240627
157.755448	4977.972522	25.245645
158.062237	4997.204583	25.250663
158.341078	4991.631285	25.255680
158.222391	5005.790895	25.260698
158.303611	5014.648110	25.265715
158.196409	5018.680034	25.270733
158.672017	5039.561935	25.275751
159.016782	5032.933573	25.280768
159.284820	5042.547674	25.285786
159.271963	5050.330574	25.290803
159.142444	5058.753464	25.295821
159.409373	5070.157467	25.300839
159.853841	5080.542705	25.305856
160.027330	5096.449770	25.310874
160.288228	5088.237271	25.315891
160.410183	5090.762619	25.320909
160.810823	5095.905482	25.325927
161.001868	5095.112092	25.330944
160.813946	5095.539286	25.335962
161.278246	5106.511712	25.340979
161.332373	5111.973672	25.345997
161.308032	5116.608228	25.351015
161.702826	5108.829406	25.356032
161.835256	5111.599331	25.361050
161.528075	5124.920350	25.366067
161.981046	5124.944741	25.371085
161.822938	5139.808174	25.376103
162.135345	5135.400660	25.381120
162.564769	5148.916349	25.386138
162.366045	5156.601973	25.391155
162.608625	5159.986052	25.396173
162.443243	5166.277637	25.401191
162.875220	5164.411408	25.406208
163.230617	5182.130456	25.411226
163.231230	5186.521252	25.416243
163.409850	5184.893325	25.421261
163.344097	5195.714749	25.426279
163.626734	5206.112630	25.431296
163.494713	5204.334206	25.436314
163.714866	5223.677847	25.441331
164.033687	5228.069615	25.446349
163.924249	5241.492506	25.451367
164.375636	5241.485579	25.456384
164.460476	5257.021494	25.461402
164.395708	5268.871827	25.466419
164.953751	5274.760421	25.471437
165.053617	5286.790306	25.476455
165.492569	5293.890606	25.481472
165.764145	5310.363384	25.486490
165.823146	5312.930129	25.491507
166.027028	5311.304571	25.496525
166.227679	5314.212260	25.501543
166.452460	5326.661478	25.506560
166.737852	5337.980706	25.511578
166.483624	5346.634632	25.516595
166.474528	5342.611714	25.521613
166.717665	5354.313156	25.526631
166.958972	5356.829428	25.531648
167.248016	5370.266129	25.536666
167.158188	5382.568663	25.541683
167.563506	5383.092892	25.546701
167.589121	5391.636983	25.551719
167.938998	5399.650802	25.556736
168.104104	5404.293815	25.561754
168.110233	5406.000760	25.566771
168.642731	5411.836559	25.571789
168.546799	5426.286510	25.576807
168.897315	5430.240949	25.581824
169.047308	5431.931812	25.586842
169.139107	5438.691651	25.591859
169.783718	5454.077453	25.596877
169.409007	5455.793192	25.601895
169.497526	5465.047213	25.606912
169.841271	5462.424497	25.611930
170.014514	5482.053492	25.616947
170.151879	5481.599880	25.621965
170.551760	5480.808683	25.626983
170.596417	5490.874463	25.632000
170.898859	5504.713215	25.637018
171.107148	5503.273190	25.642035
171.343604	5503.729017	25.647053
171.068023	5508.194457	25.652071
170.858709	5523.770084	25.657088
171.607074	5529.891124	25.662106
171.762540	5535.839325	25.667123
172.318903	5544.060957	25.672141
172.257780	5557.391331	25.677159
172.541479	5550.065222	25.682176
172.788970	5541.084410	25.687194
172.955229	5537.864319	25.692212
173.120394	5537.261177	25.697229
172.718131	5547.399726	25.702247
172.885938	5555.000044	25.707264
173.577077	5562.127474	25.712282
173.447099	5571.020998	25.717300
173.467440	5575.771821	25.722317
173.933240	5583.805552	25.727335
173.648215	5589.383589	25.732352
173.906859	5588.712230	25.737370
173.682055	5606.790332	25.742388
174.204420	5610.661237	25.747405
174.172981	5621.995248	25.752423
174.401770	5642.288115	25.757440
174.850397	5642.284777	25.762458
174.783347	5646.487355	25.767476
174.986019	5658.646682	25.772493
175.027485	5664.821007	25.777511
175.513589	5674.641392	25.782528
175.835893	5675.532091	25.787546
176.029706	5689.567821	25.792564
176.352863	5683.829585	25.797581
176.232151	5700.947759	25.802599
176.500872	5711.385975	25.807616
176.951661	5714.346326	25.812634
176.873347	5721.382125	25.817652
177.250064	5727.984077	25.822669
177.608085	5732.802317	25.827687
177.655626	5740.099464	25.832704
178.346096	5720.768612	25.837722
178.265437	5721.788339	25.842740
178.508129	5714.500114	25.847757
178.347763	5714.585277	25.852775
178.631099	5721.918308	25.857792
179.021008	5728.474014	25.862810
179.212321	5741.096026	25.867828
179.399606	5743.361923	25.872845
179.769645	5748.342438	25.877863
179.669699	5744.690270	25.882880
179.594984	5744.740002	25.887898
179.398449	5749.297361	25.892916
179.812549	5754.359403	25.897933
180.105370	5757.069732	25.902951
179.948694	5757.908745	25.907968
179.927438	5771.996962	25.912986
179.818088	5788.008643	25.918004
180.284621	5796.960923	25.923021
180.580572	5810.538922	25.928039
180.746685	5826.678206	25.933056
181.150305	5841.574705	25.938074
181.007318	5855.066402	25.943092
181.220646	5869.474869	25.948109
181.536874	5882.964537	25.953127
181.882081	5890.092293	25.958144
181.975895	5895.832405	25.963162
181.998832	5911.451118	25.968180
182.592071	5908.492774	25.973197
182.823993	5926.607409	25.978215
182.639748	5934.411057	25.983232
183.299489	5938.036526	25.988250
183.040992	5941.056838	25.993268
183.866292	5945.404650	25.998285
184.277044	5944.337117	26.003303
183.897354	5939.683622	26.008320
184.082412	5946.627998	26.013338
184.238795	5946.266113	26.018356
184.247996	5955.958876	26.023373
184.757908	5958.458667	26.028391
185.003097	5963.745932	26.033408
184.940272	5957.995102	26.038426
185.220553	5981.733673	26.043444
185.565170	5977.207305	26.048461
185.793058	5985.843291	26.053479
185.410099	5986.651254	26.058496
185.840803	5997.067572	26.063514
186.203055	6006.301347	26.068532
186.481169	6010.185114	26.073549
186.643344	6012.372882	26.078567
186.657866	6016.348195	26.083584
186.618310	6021.648242	26.088602
186.730094	6036.628218	26.093620
186.899004	6024.275492	26.098637
186.906941	6031.357958	26.103655
187.158133	6054.618189	26.108672
187.288361	6056.261682	26.113690
187.529770	6069.756823	26.118708
187.752006	6076.856449	26.123725
188.182465	6084.561301	26.128743
188.200850	6103.504832	26.133760
188.575765	6106.477061	26.138778
188.757105	6113.156921	26.143796
188.823607	6113.797057	26.148813
188.971306	6131.880816	26.153831
189.148876	6145.887861	26.158848
189.319287	6149.378061	26.163866
189.120546	6161.540244	26.168884
189.465867	6170.180131	26.173901
189.776995	6181.265442	26.178919
189.850371	6193.420003	26.183936
189.992055	6209.405596	26.188954
190.374545	6218.001839	26.193972
190.648680	6235.422056	26.198989
190.874265	6237.113853	26.204007
190.944282	6248.921740	26.209024
191.405502	6264.488303	26.214042
191.538635	6270.175061	26.219060
191.224330	6274.956070	26.224077
191.670248	6292.223329	26.229095
191.878970	6309.445460	26.234112
192.033018	6310.340291	26.239130
192.603080	6317.401641	26.244148
192.941194	6327.621066	26.249165
193.558539	6331.969783	26.254183
193.610517	6341.106828	26.259200
194.031550	6332.578425	26.264218
193.796829	6335.762404	26.269236
194.064318	6337.150957	26.274253
194.189218	6348.603130	26.279271
194.097717	6355.448668	26.284288
194.481552	6351.522187	26.289306
194.919664	6363.222333	26.294324
194.894046	6367.832153	26.299341
195.186011	6376.796114	26.304359
195.127757	6383.948999	26.309376
195.059288	6395.472344	26.314394
195.283686	6403.616627	26.319412
195.474256	6408.549505	26.324429
196.214789	6421.320076	26.329447
195.914354	6439.666468	26.334464
196.416360	6440.699691	26.339482
196.438789	6441.280409	26.344500
196.835157	6458.328258	26.349517
196.976789	6460.083654	26.354535
196.761747	6470.575525	26.359552
196.992553	6480.253005	26.364570
197.404837	6486.025795	26.369588
197.765166	6498.079062	26.374605
198.181390	6503.254625	26.379623
198.068622	6517.733314	26.384640
198.639801	6515.529608	26.389658
198.833086	6517.823079	26.394676
198.733232	6533.878129	26.399693
199.266428	6533.350239	26.404711
199.014647	6542.591497	26.409728
198.878188	6552.209396	26.414746
199.273114	6564.017410	26.419764
199.343866	6566.655107	26.424781
199.436326	6570.839377	26.429799
199.647230	6598.273450	26.434816
200.205316	6596.359036	26.439834
200.155762	6609.230650	26.444852
200.315524	6611.987079	26.449869
200.682100	6616.052920	26.454887
200.849004	6633.000918	26.459904
201.243202	6638.350413	26.464922
201.283506	6647.931371	26.469940
201.506682	6660.460670	26.474957
201.783038	6659.552918	26.479975
201.604769	6675.923347	26.484992
202.136161	6683.729539	26.490010
202.473900	6692.806486	26.495028
202.494652	6705.948173	26.500045
203.092580	6714.934114	26.505063
202.820126	6719.907597	26.510080
203.095683	6733.448421	26.515098
203.414819	6735.201462	26.520116
203.509063	6739.246596	26.525133
204.055221	6752.003467	26.530151
204.226339	6768.452166	26.535168
204.238520	6766.834230	26.540186
204.263390	6774.097439	26.545204
204.413973	6787.080073	26.550221
204.892428	6785.585260	26.555239
204.885261	6801.894439	26.560256
205.088447	6801.313748	26.565274
205.395991	6810.196578	26.570292
205.355607	6843.052430	26.575309
205.752690	6838.795479	26.580327
205.980418	6855.292264	26.585344
205.828219	6864.906464	26.590362
206.528490	6871.565789	26.595380
206.854419	6889.717253	26.600397
207.167908	6891.856315	26.605415
207.625710	6901.703869	26.610432
207.743197	6918.363087	26.615450
208.331667	6915.035984	26.620468
208.397891	6922.027644	26.625485
208.201195	6912.288238	26.630503
208.480954	6917.655632	26.635520
208.508500	6928.346756	26.640538
208.750310	6931.674464	26.645556
208.750616	6939.033111	26.650573
209.525701	6952.603657	26.655591
209.315073	6965.159665	26.660608
209.461805	6970.222636	26.665626
209.659929	6968.212701	26.670644
209.761850	6982.604666	26.675661
210.109127	6987.835298	26.680679
210.256120	7010.150144	26.685696
210.276378	7017.429952	26.690714
210.833493	7020.089854	26.695732
210.712002	7032.085903	26.700749
210.764289	7039.758491	26.705767
210.802691	7053.576392	26.710784
211.286805	7060.064248	26.715802
211.879645	7061.294873	26.720820
212.424039	7074.844604	26.725837
212.733385	7070.083543	26.730855
212.853509	7081.262275	26.735872
212.968329	7090.200501	26.740890
213.691966	7093.860454	26.745908
213.410040	7108.324906	26.750925
213.974408	7108.486649	26.755943
214.129740	7105.350064	26.760960
213.711930	7097.378077	26.765978
213.984455	7100.101240	26.770996
213.966193	7107.125065	26.776013
214.155985	7114.507946	26.781031
214.754619	7122.581659	26.786048
214.621284	7127.214754	26.791066
214.912720	7142.650659	26.796084
214.843630	7154.547082	26.801101
214.745413	7163.029203	26.806119
214.996634	7173.246846	26.811136
214.911145	7195.244548	26.816154
215.450478	7198.162949	26.821172
215.691851	7222.294323	26.826189
215.744725	7234.579041	26.831207
216.725971	7249.358350	26.836224
216.403363	7259.529636	26.841242
217.178164	7258.099139	26.846260
217.012898	7281.624649	26.851277
217.338411	7280.516647	26.856295
217.594315	7310.280848	26.861312
217.873918	7317.059498	26.866330
218.154407	7321.852350	26.871348
218.070629	7338.925265	26.876365
218.489100	7345.262442	26.881383
218.703282	7364.899714	26.886400
219.105746	7371.349883	26.891418
219.125992	7375.444561	26.896436
219.189929	7386.158697	26.901453
219.609439	7393.850025	26.906471
219.935023	7407.598227	26.911488
220.124212	7417.270055	26.916506
221.076748	7420.566123	26.921524
221.087306	7427.762369	26.926541
221.212012	7425.290284	26.931559
221.589399	7425.588476	26.936576
221.476352	7431.604356	26.941594
222.187920	7431.200204	26.946612
222.086030	7449.163122	26.951629
222.265215	7447.370752	26.956647
222.438177	7453.525209	26.961664
222.521954	7444.477405	26.966682
223.084295	7462.235903	26.971700
223.043313	7464.805890	26.976717
223.050995	7476.043408	26.981735
223.368805	7485.651051	26.986752
223.392637	7500.990019	26.991770
224.082614	7502.669615	26.996788
223.825882	7521.963662	27.001805
224.087451	7526.497492	27.006823
224.191590	7539.680461	27.011840
224.371377	7554.887858	27.016858
224.481137	7553.191522	27.021876
224.712719	7580.440747	27.026893
224.885932	7590.809672	27.031911
225.367441	7604.079152	27.036928
225.438412	7619.360368	27.041946
225.621526	7637.765262	27.046964
225.877045	7642.413712	27.051981
225.833202	7658.413670	27.056999
226.348000	7672.132612	27.062016
226.310074	7682.935389	27.067034
227.130106	7704.615933	27.072052
227.326736	7726.829215	27.077069
227.250139	7737.884285	27.082087
227.732130	7747.415993	27.087104
227.615004	7765.438417	27.092122
228.088053	7770.801225	27.097140
228.012126	7782.658078	27.102157
228.566145	7800.389786	27.107175
228.655011	7802.368199	27.112192
228.827902	7822.596422	27.117210
229.635333	7818.963574	27.122228
229.553021	7831.383388	27.127245
229.962295	7826.612889	27.132263
230.192451	7837.670772	27.137280
230.092508	7844.666556	27.142298
230.780318	7841.731070	27.147316
230.992806	7859.004583	27.152333
230.743638	7864.009474	27.157351
231.336935	7871.083598	27.162368
231.326962	7892.577892	27.167386
231.459816	7900.377202	27.172404
231.962688	7900.504334	27.177421
232.021531	7910.922815	27.182439
232.243752	7912.801553	27.187456
232.354838	7935.227293	27.192474
232.661701	7951.343381	27.197492
232.674956	7966.640185	27.202509
233.003585	7969.203209	27.207527
233.288806	7972.284421	27.212544
233.423609	8000.600605	27.217562
233.809051	7999.612667	27.222580
234.206007	8026.991498	27.227597
234.368248	8037.264517	27.232615
234.740627	8046.772406	27.237632
235.138034	8055.266170	27.242650
235.476024	8051.750563	27.247668
235.649768	8063.647650	27.252685
235.848795	8079.799581	27.257703
236.026218	8075.346087	27.262720
235.864581	8093.296836	27.267738
236.698685	8097.621705	27.272756
236.847129	8110.223613	27.277773
236.845657	8125.636494	27.282791
237.322509	8122.582273	27.287808
237.311911	8138.043940	27.292826
237.794971	8149.343609	27.297844
237.662281	8149.443413	27.302861
237.837746	8166.467262	27.307879
238.665453	8164.760119	27.312896
238.592025	8170.110258	27.317914
238.852882	8191.742684	27.322932
239.064215	8201.278884	27.327949
239.054439	8218.950394	27.332967
239.603040	8224.026914	27.337984
239.811412	8230.706497	27.343002
239.814063	8238.302073	27.348020
240.508854	8247.602021	27.353037
240.643595	8256.566126	27.358055
241.092844	8266.974539	27.363072
241.147214	8270.498997	27.368090
241.148059	8270.571698	27.373108
241.432562	8287.319807	27.378125
241.621780	8293.977139	27.383143
241.847176	8322.936375	27.388160
242.008254	8339.833186	27.393178
242.046647	8339.761131	27.398196
242.214284	8361.957594	27.403213
242.137701	8384.110023	27.408231
242.939065	8375.161565	27.413248
242.773721	8400.942639	27.418266
243.180191	8419.395623	27.423284
243.668047	8435.054598	27.428301
243.650929	8442.782776	27.433319
244.269870	8457.114344	27.438336
244.654007	8459.634068	27.443354
244.540794	8483.945427	27.448372
245.165894	8488.962755	27.453389
245.245369	8491.106871	27.458407
245.429661	8500.344358	27.463424
245.633041	8518.090309	27.468442
245.880198	8531.163323	27.473460
246.471818	8533.120369	27.478477
246.341633	8548.970374	27.483495
246.684436	8545.933799	27.488512
246.810908	8569.301877	27.493530
247.090208	8566.919226	27.498548
247.274953	8576.753367	27.503565
247.500154	8597.334203	27.508583
247.704476	8602.922204	27.513600
248.121457	8619.649990	27.518618
248.656005	8627.399698	27.523636
248.959005	8629.234364	27.528653
248.913310	8644.218885	27.533671
249.089171	8651.692953	27.538688
249.517623	8658.546795	27.543706
249.453335	8655.463082	27.548724
249.788333	8666.119977	27.553741
249.843808	8687.355597	27.558759
250.530070	8696.224580	27.563776
250.692579	8708.988876	27.568794
250.862332	8726.756048	27.573812
251.212676	8729.640980	27.578829
251.336238	8752.409895	27.583847
251.778020	8756.818103	27.588864
252.121098	8764.386153	27.593882
252.112454	8777.868548	27.598900
252.656304	8792.521465	27.603917
252.425856	8809.716445	27.608935
252.976599	8822.578232	27.613952
252.955050	8835.525969	27.618970
253.458824	8843.170060	27.623988
253.670968	8855.828860	27.629005
253.728044	8867.012178	27.634023
254.212667	8872.913377	27.639040
254.511645	8892.876888	27.644058
254.838972	8901.331441	27.649076
255.140006	8916.328501	27.654093
255.065424	8931.898664	27.659111
255.705259	8946.707245	27.664128
255.748371	8958.622091	27.669146
256.075239	8963.714396	27.674164
257.425829	8946.768378	27.679181
257.207047	8950.471249	27.684199
257.699375	8957.899328	27.689216
258.039218	8970.888767	27.694234
258.071203	8973.788574	27.699252
258.264824	8974.885748	27.704269
257.991912	8976.336541	27.709287
258.479126	8978.575091	27.714304
259.346217	8981.802669	27.719322
259.362287	8994.473147	27.724340
259.628391	8994.103596	27.729357
259.386948	9005.001974	27.734375
259.746911	9007.099324	27.739392
259.974193	9015.837863	27.744410
259.839526	9014.934006	27.749428
260.316439	9023.864155	27.754445
260.289674	9044.674146	27.759463
260.725427	9060.322823	27.764480
260.709793	9074.504253	27.769498
261.011309	9083.199694	27.774516
261.358703	9095.878645	27.779533
261.345649	9115.395303	27.784551
261.806636	9130.910667	27.789568
261.923508	9136.449301	27.794586
261.739483	9160.153769	27.799604
262.393044	9174.755181	27.804621
262.435584	9191.671226	27.809639
262.535875	9201.029486	27.814656
263.004044	9214.823141	27.819674
263.353183	9235.584294	27.824692
263.753719	9249.931541	27.829709
263.723185	9275.708629	27.834727
264.186356	9294.365193	27.839744
264.392964	9304.840386	27.844762
264.640827	9322.119233	27.849780
265.193242	9337.917313	27.854797
265.349097	9352.451121	27.859815
265.471593	9369.661129	27.864832
265.466095	9390.771288	27.869850
266.074654	9412.944568	27.874868
266.275980	9414.068984	27.879885
266.678948	9434.272625	27.884903
267.545476	9450.909076	27.889920
267.302496	9468.715960	27.894938
267.560858	9478.712767	27.899956
267.971379	9491.527394	27.904973
267.986227	9516.495816	27.909991
268.528168	9524.348940	27.915008
268.594902	9545.568005	27.920026
268.629445	9551.065908	27.925044
269.449220	9572.338256	27.930061
269.458153	9598.428529	27.935079
269.989840	9609.876230	27.940096
270.828859	9610.449892	27.945114
271.083027	9613.422555	27.950132
271.168281	9616.453088	27.955149
271.533215	9624.930533	27.960167
271.714030	9619.538439	27.965184
272.026437	9634.761634	27.970202
272.326950	9646.785238	27.975220
272.524183	9642.615596	27.980237
272.335239	9671.212063	27.985255
272.564554	9676.345011	27.990272
272.887639	9683.064091	27.995290
273.123290	9699.514833	28.000308
273.638485	9709.484409	28.005325
273.661477	9729.302354	28.010343
273.813266	9743.414028	28.015360
274.348875	9751.754455	28.020378
274.343802	9776.300097	28.025396
274.852965	9787.628281	28.030413
274.895988	9814.509184	28.035431
275.092073	9823.777069	28.040448
275.642928	9843.613989	28.045466
275.263868	9866.254142	28.050484
275.980188	9869.808454	28.055501
276.475448	9894.172165	28.060519
276.852953	9898.947431	28.065536
277.074826	9914.904813	28.070554
277.348219	9932.776984	28.075572
277.862527	9944.543329	28.080589
277.786363	9959.407363	28.085607
278.169641	9968.276773	28.090624
278.785183	9971.638413	28.095642
278.907023	9998.317872	28.100660
278.774340	9998.774458	28.105677
279.081812	10022.176178	28.110695
279.257131	10035.716093	28.115712
279.949333	10046.839131	28.120730
280.038660	10072.361864	28.125748
280.125437	10080.920711	28.130765
280.457087	10093.242861	28.135783
280.698868	10101.736541	28.140800
281.189577	10120.875879	28.145818
280.996515	10132.847192	28.150836
281.580008	10143.560971	28.155853
281.466716	10164.136257	28.160871
281.671481	10180.049170	28.165888
282.570687	10195.724531	28.170906
282.391205	10211.804643	28.175924
282.810061	10226.648655	28.180941
282.927179	10249.499344	28.185959
282.955013	10269.705465	28.190976
283.577534	10285.272425	28.195994
283.641697	10307.146332	28.201012
284.168653	10324.922571	28.206029
284.641838	10348.286272	28.211047
285.486349	10360.923426	28.216064
285.508805	10368.538893	28.221082
285.591669	10391.998147	28.226100
286.053091	10388.769153	28.231117
286.555366	10415.007937	28.236135
286.763409	10422.019889	28.241152
286.990740	10433.512327	28.246170
287.365061	10446.623730	28.251188
287.908269	10445.412193	28.256205
288.271656	10470.971740	28.261223
288.464284	10473.044794	28.266240
288.452016	10479.206997	28.271258
288.598850	10493.184243	28.276276
288.908908	10506.305692	28.281293
288.856559	10516.158831	28.286311
289.153051	10537.134868	28.291328
289.594719	10540.015341	28.296346
289.638710	10567.752836	28.301364
290.280998	10586.455435	28.306381
290.807007	10602.520771	28.311399
291.118717	10616.630311	28.316416
291.709391	10621.612541	28.321434
291.943916	10638.863115	28.326452
292.183114	10645.055687	28.331469
292.439357	10650.787780	28.336487
292.804929	10671.566926	28.341504
293.000148	10673.608025	28.346522
292.906637	10692.308459	28.351540
293.555872	10699.068698	28.356557
293.742946	10718.044375	28.361575
293.823587	10723.465985	28.366592
293.889626	10743.739293	28.371610
294.364259	10763.396458	28.376628
294.748223	10777.602225	28.381645
295.403999	10798.067948	28.386663
294.925594	10820.317412	28.391680
295.564616	10828.023366	28.396698
296.141597	10851.851472	28.401716
296.549406	10861.645783	28.406733
296.943384	10872.326341	28.411751
296.776711	10887.827225	28.416768
297.342572	10898.127402	28.421786
297.280033	10914.647744	28.426804
297.409123	10922.568897	28.431821
297.696843	10949.334403	28.436839
297.978319	10965.453910	28.441856
298.375888	10980.740728	28.446874
298.583506	11001.052265	28.451892
298.748723	11023.479625	28.456909
299.532322	11042.817440	28.461927
299.670100	11045.363249	28.466944
299.979940	11060.455396	28.471962
300.260611	11081.191381	28.476980
300.852144	11083.227660	28.481997
301.314186	11083.759029	28.487015
301.354818	11095.940858	28.492032
301.958967	11104.242809	28.497050
301.850154	11120.764222	28.502068
302.461540	11133.873934	28.507085
302.631523	11143.133911	28.512103
302.789357	11165.553119	28.517120
303.338493	11170.996646	28.522138
303.420134	11188.135757	28.527156
303.757803	11200.710305	28.532173
303.958110	11215.734378	28.537191
304.348468	11229.828981	28.542208
304.455968	11241.738421	28.547226
304.851921	11252.999874	28.552244
304.983857	11274.949616	28.557261
305.858777	11287.787909	28.562279
305.906246	11304.294626	28.567296
306.097909	11307.905643	28.572314
306.471842	11324.225778	28.577332
306.834746	11334.112582	28.582349
307.640048	11340.744560	28.587367
307.845002	11344.555597	28.592384
308.186362	11356.618154	28.597402
308.274346	11368.789632	28.602420
308.835127	11376.463790	28.607437
309.007531	11392.676428	28.612455
309.024302	11407.170342	28.617472
309.576276	11412.755589	28.622490
309.656054	11424.628413	28.627508
309.748471	11435.861452	28.632525
310.039767	11459.153821	28.637543
310.064243	11475.803202	28.642560
310.717827	11499.045533	28.647578
311.161545	11512.920486	28.652596
310.984060	11533.740932	28.657613
311.524860	11556.328331	28.662631
311.837392	11582.143608	28.667648
312.440627	11587.626199	28.672666
312.488416	11608.424286	28.677684
312.838846	11625.714564	28.682701
313.160603	11641.440000	28.687719
313.315895	11674.318151	28.692736
313.939840	11683.592976	28.697754
313.949697	11705.701163	28.702772
314.388160	11732.030675	28.707789
314.847830	11743.797194	28.712807
314.793001	11772.950679	28.717824
315.492101	11778.033174	28.722842
315.594458	11796.600015	28.727860
316.230262	11813.662897	28.732877
316.599388	11841.566378	28.737895
316.626099	11849.248095	28.742912
317.337722	11867.003372	28.747930
317.443871	11881.202709	28.752948
317.723798	11899.192579	28.757965
318.032680	11908.977581	28.762983
318.380213	11930.370359	28.768000
318.991483	11940.818769	28.773018
319.748056	11946.460738	28.778036
319.739148	11961.966366	28.783053
319.885425	11979.465582	28.788071
320.141204	11999.698079	28.793088
320.384420	12006.493589	28.798106
320.762511	12020.552807	28.803124
320.919958	12040.778554	28.808141
321.337580	12044.120868	28.813159
321.560336	12061.845079	28.818176
321.770007	12077.462025	28.823194
322.296404	12094.640084	28.828212
322.338165	12107.788641	28.833229
322.686037	12120.163286	28.838247
322.932046	12134.448401	28.843264
323.613890	12150.105574	28.848282
323.504386	12162.415674	28.853300
323.415758	12186.320688	28.858317
323.837626	12210.534653	28.863335
323.853125	12237.429637	28.868352
324.509948	12254.931726	28.873370
324.913382	12274.667878	28.878388
324.803312	12299.463687	28.883405
325.471897	12321.514252	28.888423
326.171477	12356.137169	28.893440
326.084953	12370.903683	28.898458
326.525762	12390.883597	28.903476
327.138328	12409.933686	28.908493
327.221278	12421.048794	28.913511
328.138372	12446.799559	28.918528
328.404681	12464.848930	28.923546
328.671382	12477.185925	28.928564
329.136065	12500.635742	28.933581
329.853058	12511.601670	28.938599
330.115001	12520.175413	28.943616
330.476043	12525.522313	28.948634
330.899633	12539.038021	28.953652
331.059702	12543.753090	28.958669
331.512308	12560.731495	28.963687
331.445031	12565.709321	28.968704
332.531987	12577.653430	28.973722
332.816376	12587.837319	28.978740
332.677748	12597.322894	28.983757
333.302754	12611.672521	28.988775
333.085995	12628.941505	28.993792
333.678952	12641.186764	28.998810
334.071806	12658.124036	29.003828
334.164939	12676.519506	29.008845
334.596283	12693.185565	29.013863
334.647024	12700.377593	29.018880
335.035910	12716.687140	29.023898
335.073222	12734.882944	29.028916
335.649148	12765.989163	29.033933
336.047296	12778.561671	29.038951
336.563548	12795.754583	29.043968
336.967276	12808.098882	29.048986
337.242435	12827.328235	29.054004
336.890279	12851.843523	29.059021
337.705968	12866.451017	29.064039
337.826201	12884.214069	29.069056
338.149318	12912.517871	29.074074
338.467241	12922.927240	29.079092
338.733702	12951.628330	29.084109
339.305276	12966.393904	29.089127
339.397067	13003.976773	29.094144
339.566464	13017.475558	29.099162
340.467592	13039.493922	29.104180
340.282655	13069.165446	29.109197
340.983218	13086.292036	29.114215
341.182063	13105.176718	29.119232
341.365487	13123.192257	29.124250
342.406105	13135.579720	29.129268
343.256431	13133.240229	29.134285
343.846786	13128.683357	29.139303
344.569356	13149.602301	29.144320
344.475452	13150.188710	29.149338
345.025989	13159.709379	29.154356
344.995980	13162.777379	29.159373
345.128498	13162.194873	29.164391
345.243190	13168.338192	29.169408
345.468455	13178.316872	29.174426
345.852709	13192.792845	29.179444
345.838025	13211.492985	29.184461
346.230884	13219.045627	29.189479
346.524156	13237.429432	29.194496
346.881217	13251.227586	29.199514
347.269316	13264.660922	29.204532
347.541836	13279.770139	29.209549
347.692813	13296.483540	29.214567
348.201706	13324.601145	29.219584
348.311833	13339.877796	29.224602
349.171688	13358.814560	29.229620
349.107029	13380.187896	29.234637
349.388551	13397.010535	29.239655
349.771574	13420.392107	29.244672
350.014076	13439.191380	29.249690
350.292384	13461.158780	29.254708
350.477461	13484.887038	29.259725
351.030266	13499.548585	29.264743
351.578947	13523.747654	29.269760
351.681509	13565.514185	29.274778
352.227269	13576.058973	29.279796
352.184813	13607.663907	29.284813
353.072295	13627.951388	29.289831
353.171177	13646.867964	29.294848
353.432704	13674.980390	29.299866
353.932742	13687.196587	29.304884
354.139286	13729.496772	29.309901
354.825343	13743.379858	29.314919
354.827533	13772.688609	29.319936
355.010784	13803.077659	29.324954
355.893054	13823.959857	29.329972
355.965405	13857.369474	29.334989
356.823109	13863.751037	29.340007
357.152615	13885.556219	29.345024
357.454436	13906.806776	29.350042
357.834230	13930.249482	29.355060
357.961160	13952.859983	29.360077
358.709190	13973.109544	29.365095
359.155618	13991.647085	29.370112
359.204136	14019.799501	29.375130
359.562351	14029.836882	29.380148
360.052512	14059.054317	29.385165
360.461097	14074.427206	29.390183
360.875465	14097.520515	29.395200
360.949792	14117.985646	29.400218
361.513930	14135.541812	29.405236
361.646430	14168.017316	29.410253
362.250372	14185.898923	29.415271
362.748342	14194.155620	29.420288
362.718659	14231.924053	29.425306
363.442191	14247.206996	29.430324
363.626936	14255.768284	29.435341
363.696765	14274.731064	29.440359
364.420591	14295.003687	29.445376
364.416805	14322.552035	29.450394
365.191160	14342.488407	29.455412
365.551105	14372.661378	29.460429
366.022712	14387.588899	29.465447
366.447018	14401.974296	29.470464
366.485424	14424.425447	29.475482
367.097640	14448.075779	29.480500
367.402764	14462.751369	29.485517
368.208044	14475.507955	29.490535
368.627954	14480.479913	29.495552
368.457710	14490.145050	29.500570
368.959494	14502.806790	29.505588
369.329412	14524.833797	29.510605
369.481580	14535.986743	29.515623
370.126622	14548.863067	29.520640
370.457146	14565.893864	29.525658
371.070766	14578.190856	29.530676
371.059493	14592.211552	29.535693
371.542611	14603.215114	29.540711
371.596013	14623.320867	29.545728
371.974615	14640.849542	29.550746
372.513664	14659.790186	29.555764
372.430099	14685.744011	29.560781
372.718440	14697.355883	29.565799
373.644657	14726.086432	29.570816
373.570525	14749.888208	29.575834
373.951077	14771.452761	29.580852
374.520545	14799.642079	29.585869
375.030141	14827.998665	29.590887
375.103523	14845.436088	29.595904
375.604218	14871.239202	29.600922
376.160103	14900.675087	29.605940
376.327492	14915.685125	29.610957
376.546043	14941.952292	29.615975
377.115802	14970.432366	29.620992
377.409615	14996.618413	29.626010
377.867251	15009.328420	29.631028
378.354900	15029.306992	29.636045
378.511474	15047.091678	29.641063
379.606334	15069.909689	29.646080
379.701606	15088.360854	29.651098
380.039185	15113.172762	29.656116
380.259833	15136.540673	29.661133
380.672777	15150.783130	29.666151
381.282777	15179.171981	29.671168
381.101913	15203.840489	29.676186
381.850421	15219.243499	29.681204
381.831066	15248.355753	29.686221
382.235773	15282.294078	29.691239
383.118777	15301.747132	29.696256
383.156603	15332.439186	29.701274
383.306588	15351.409508	29.706292
384.131320	15373.616190	29.711309
384.420155	15398.849784	29.716327
385.070630	15425.179860	29.721344
385.292611	15437.320464	29.726362
385.910017	15459.929035	29.731380
386.069307	15478.294813	29.736397
386.719855	15502.347903	29.741415
387.687667	15520.891040	29.746432
387.630824	15543.967877	29.751450
388.053287	15550.777816	29.756468
388.625666	15580.303772	29.761485
388.886739	15593.351122	29.766503
389.305437	15602.981981	29.771520
389.527198	15633.361642	29.776538
390.323722	15647.314202	29.781556
390.311319	15655.878389	29.786573
390.675521	15685.348485	29.791591
391.202752	15686.024609	29.796608
391.168299	15712.755432	29.801626
391.504432	15736.216637	29.806644
392.112175	15758.902867	29.811661
392.491231	15774.960759	29.816679
392.977968	15797.267929	29.821696
393.497384	15821.945069	29.826714
394.040819	15818.733984	29.831732
394.490189	15842.054518	29.836749
394.988904	15848.988499	29.841767
395.128516	15859.360919	29.846784
395.418469	15875.963361	29.851802
395.712212	15894.419148	29.856820
396.287037	15895.094187	29.861837
396.514620	15923.919520	29.866855
396.847848	15937.991795	29.871872
396.817861	15951.075228	29.876890
397.479698	15967.411405	29.881908
397.999698	15990.515834	29.886925
398.316098	16015.101655	29.891943
398.807349	16027.124914	29.896960
398.564222	16057.978729	29.901978
398.794775	16081.084113	29.906996
399.217036	16101.421405	29.912013
400.145636	16135.930302	29.917031
400.246309	16162.463850	29.922048
400.677118	16193.358247	29.927066
401.180269	16212.028090	29.932084
401.513259	16244.810700	29.937101
401.460757	16271.845157	29.942119
402.348624	16292.893440	29.947136
402.855855	16323.131843	29.952154
403.008884	16346.976040	29.957172
403.614095	16373.728219	29.962189
404.096869	16389.015629	29.967207
404.720639	16415.736552	29.972224
405.222210	16445.303293	29.977242
405.579383	16472.387955	29.982260
405.988216	16493.890043	29.987277
406.710508	16517.769007	29.992295
407.006788	16532.684448	29.997312
407.035167	16560.205746	30.002330
407.591523	16582.026074	30.007348
408.265507	16600.935008	30.012365
409.304333	16606.272302	30.017383
410.592974	16596.186071	30.022400
410.887751	16592.899869	30.027418
411.557476	16603.632341	30.032436
411.888309	16620.617550	30.037453
411.898524	16618.667437	30.042471
412.436038	16616.682610	30.047488
412.103663	16630.306294	30.052506
412.739302	16646.201795	30.057524
412.410274	16658.274193	30.062541
413.044274	16678.307511	30.067559
413.168867	16699.882507	30.072576
413.637309	16727.591369	30.077594
413.653697	16734.085939	30.082612
414.256220	16760.709582	30.087629
414.535085	16791.830739	30.092647
415.298020	16820.438263	30.097664
415.560342	16836.635241	30.102682
415.265761	16857.612397	30.107700
415.607966	16894.308010	30.112717
416.262167	16928.832630	30.117735
416.364875	16954.529961	30.122752
417.010949	16986.879765	30.127770
417.503597	17020.425305	30.132788
418.045418	17044.797319	30.137805
418.359092	17072.331787	30.142823
418.979590	17103.975109	30.147840
419.481310	17128.820930	30.152858
419.676412	17164.361838	30.157876
420.303374	17187.801653	30.162893
420.629255	17214.080496	30.167911
420.901240	17230.901687	30.172928
421.342207	17255.722386	30.177946
421.894667	17286.062656	30.182964
422.207555	17309.823148	30.187981
422.545707	17340.932805	30.192999
423.305388	17356.822219	30.198016
423.599848	17380.787814	30.203034
424.379710	17398.123891	30.208052
424.600559	17426.339770	30.213069
424.717105	17448.592787	30.218087
425.302204	17462.118443	30.223104
425.498633	17499.520151	30.228122
425.835777	17527.512766	30.233140
426.523894	17553.012367	30.238157
426.836650	17583.482020	30.243175
427.212203	17598.755501	30.248192
427.831910	17638.469991	30.253210
428.255024	17658.303427	30.258228
428.532274	17690.339118	30.263245
428.892940	17712.241734	30.268263
429.593100	17734.255769	30.273280
429.798381	17769.398223	30.278298
429.894988	17806.882397	30.283316
430.690724	17832.394041	30.288333
431.478628	17855.354773	30.293351
431.725324	17878.412424	30.298368
432.067829	17904.493784	30.303386
432.495256	17933.082547	30.308404
433.610046	17951.387221	30.313421
433.558811	17985.091760	30.318439
434.943736	18001.629810	30.323456
435.371196	18019.018151	30.328474
435.324109	18034.136669	30.333492
435.709663	18052.592870	30.338509
435.922006	18077.911383	30.343527
436.602864	18104.711051	30.348544
436.820645	18125.158127	30.353562
437.115996	18157.033841	30.358580
437.742128	18171.529637	30.363597
438.187667	18204.222254	30.368615
438.043513	18227.827605	30.373632
438.717300	18245.632652	30.378650
439.080920	18287.390949	30.383668
439.647847	18310.980460	30.388685
439.862473	18350.178276	30.393703
440.417542	18380.554606	30.398720
441.128555	18409.245225	30.403738
441.196534	18434.112872	30.408756
442.088016	18467.380886	30.413773
442.352848	18490.423807	30.418791
443.159931	18514.140432	30.423808
443.084725	18548.190825	30.428826
443.381658	18580.136481	30.433844
444.410900	18603.736503	30.438861
444.800943	18638.333737	30.443879
445.149530	18659.588604	30.448896
445.443390	18671.104105	30.453914
446.164451	18706.534378	30.458932
446.683245	18719.670079	30.463949
446.999656	18755.763602	30.468967
447.714520	18775.514861	30.473984
448.248962	18796.380845	30.479002
448.329023	18830.963505	30.484020
449.098158	18843.586500	30.489037
449.073066	18868.090139	30.494055
449.967077	18893.373089	30.499072
450.055186	18924.081988	30.504090
450.387917	18949.414485	30.509108
450.979253	18969.918014	30.514125
451.613126	18998.179283	30.519143
451.830247	19012.265565	30.524160
452.172373	19034.677973	30.529178
451.879911	19067.385855	30.534196
452.945990	19091.151315	30.539213
453.222288	19118.950381	30.544231
453.521359	19147.939978	30.549248
454.087800	19177.304961	30.554266
454.281612	19201.996059	30.559284
455.254556	19230.685024	30.564301
455.508322	19270.750446	30.569319
455.974451	19294.078868	30.574336
456.427537	19326.987004	30.579354
457.111187	19349.422419	30.584372
457.881110	19378.762347	30.589389
458.548507	19395.122687	30.594407
458.785594	19416.458919	30.599424
459.268051	19430.516833	30.604442
459.718561	19460.873226	30.609460
460.346786	19485.054811	30.614477
460.298384	19517.156853	30.619495
460.953045	19538.851503	30.624512
461.417113	19565.686943	30.629530
461.869039	19604.799804	30.634548
462.563074	19615.508065	30.639565
463.077852	19638.481847	30.644583
463.309009	19663.970080	30.649600
463.462021	19697.386759	30.654618
463.829393	19736.670994	30.659636
464.319457	19761.480945	30.664653
464.863656	19804.736993	30.669671
465.228316	19834.014341	30.674688
465.867398	19859.028661	30.679706
466.027318	19897.928536	30.684724
466.736757	19917.738664	30.689741
467.362030	19953.874777	30.694759
468.131595	19985.945017	30.699776
468.661153	20010.692276	30.704794
468.795789	20042.488696	30.709812
469.607207	20065.265170	30.714829
470.549559	20091.186587	30.719847
470.956032	20114.689547	30.724864
471.566305	20123.604190	30.729882
471.502506	20156.265660	30.734900
472.148635	20174.089423	30.739917
472.303348	20200.259964	30.744935
472.620304	20227.630975	30.749952
473.181036	20258.666432	30.754970
474.202526	20284.796917	30.759988
475.066579	20298.404335	30.765005
475.763661	20312.334704	30.770023
475.852450	20323.699886	30.775040
476.400496	20333.597291	30.780058
476.804528	20364.366681	30.785076
477.342416	20392.872370	30.790093
477.668314	20406.879546	30.795111
478.069237	20426.289639	30.800128
478.370366	20451.028792	30.805146
478.491736	20484.717102	30.810164
479.031907	20506.948738	30.815181
479.345389	20535.502206	30.820199
479.782006	20555.576590	30.825216
480.421719	20582.215495	30.830234
480.739855	20607.899917	30.835252
481.552750	20634.467706	30.840269
482.027400	20661.682095	30.845287
482.287343	20691.400346	30.850304
482.903271	20711.592293	30.855322
483.048972	20739.293953	30.860340
483.789178	20770.814055	30.865357
484.260115	20793.669659	30.870375
484.337319	20822.854239	30.875392
485.091603	20844.882336	30.880410
485.159218	20872.659522	30.885428
485.666436	20897.367155	30.890445
486.030079	20923.183906	30.895463
486.444950	20965.338010	30.900480
486.964946	20997.518266	30.905498
487.486418	21034.468636	30.910516
487.953314	21066.069671	30.915533
488.357724	21092.701675	30.920551
489.047808	21131.445645	30.925568
489.678243	21164.910552	30.930586
489.767779	21214.464033	30.935604
490.456078	21241.563828	30.940621
490.941654	21272.915873	30.945639
491.363393	21314.222998	30.950656
492.325735	21341.122310	30.955674
492.393709	21379.123274	30.960692
492.664971	21409.820199	30.965709
493.588036	21448.168375	30.970727
494.008787	21489.962540	30.975744
494.740225	21513.587187	30.980762
495.178463	21553.862344	30.985780
495.549414	21589.333403	30.990797
496.233901	21617.881235	30.995815
496.762331	21646.971517	31.000832
498.076694	21653.938578	31.005850
498.853483	21677.385763	31.010868
499.334223	21692.077422	31.015885
500.258901	21715.899694	31.020903
500.709129	21722.786479	31.025920
501.246238	21738.404534	31.030938
501.580628	21760.814954	31.035956
502.168314	21772.210722	31.040973
502.585814	21780.871803	31.045991
502.554983	21805.481105	31.051008
503.231291	21827.705684	31.056026
503.545570	21848.956728	31.061044
503.817189	21872.754487	31.066061
503.971311	21910.452412	31.071079
504.154802	21932.090382	31.076096
504.935610	21970.708149	31.081114
505.328496	22009.095728	31.086132
505.727136	22040.696319	31.091149
506.395101	22066.119673	31.096167
506.848691	22109.843532	31.101184
507.291564	22134.474278	31.106202
507.754863	22172.939675	31.111220
508.288993	22218.572101	31.116237
508.885018	22245.712921	31.121255
509.201718	22286.374978	31.126272
509.757712	22317.667176	31.131290
510.042571	22355.105487	31.136308
510.787235	22389.502498	31.141325
511.814844	22427.387681	31.146343
511.963453	22466.262806	31.151360
512.423698	22482.335728	31.156378
513.050374	22520.687905	31.161396
513.501821	22556.078665	31.166413
514.399292	22585.125519	31.171431
514.431643	22624.695161	31.176448
515.318634	22654.767391	31.181466
515.778705	22687.932831	31.186484
516.037647	22725.110488	31.191501
516.642012	22753.419687	31.196519
516.754654	22784.459384	31.201536
517.624039	22822.527928	31.206554
517.730443	22849.530960	31.211572
518.432036	22880.915123	31.216589
518.956377	22912.731337	31.221607
519.361013	22947.194891	31.226624
520.084262	22971.094273	31.231642
520.662430	23002.068158	31.236660
521.221750	23034.713217	31.241677
521.689863	23056.327064	31.246695
522.305647	23094.650455	31.251712
522.825144	23115.801405	31.256730
523.030158	23158.340406	31.261748
523.418670	23188.181421	31.266765
524.042239	23224.456509	31.271783
524.537360	23266.274449	31.276800
525.188952	23294.766640	31.281818
525.801477	23330.620269	31.286836
526.252268	23368.243189	31.291853
527.013586	23402.487713	31.296871
527.463669	23445.393594	31.301888
527.962783	23473.239961	31.306906
528.534508	23505.353064	31.311924
528.917071	23533.817970	31.316941
529.575394	23574.827588	31.321959
530.120606	23614.079235	31.326976
530.641480	23659.116729	31.331994
531.232935	23686.102259	31.337012
531.813139	23718.220705	31.342029
532.606107	23756.770556	31.347047
533.059317	23798.810991	31.352064
533.550396	23825.597485	31.357082
534.033449	23866.938311	31.362100
534.527145	23901.364379	31.367117
535.172635	23930.547224	31.372135
535.367929	23971.749808	31.377152
536.052612	23997.191999	31.382170
537.071837	24034.316938	31.387188
537.471266	24072.625344	31.392205
537.606536	24097.470716	31.397223
538.036653	24138.535981	31.402240
538.844930	24161.962257	31.407258
539.668161	24187.661171	31.412276
540.507260	24238.255631	31.417293
541.348065	24259.920197	31.422311
541.590858	24294.935784	31.427328
541.922239	24318.360654	31.432346
542.835249	24349.417219	31.437364
542.928327	24379.078516	31.442381
543.937864	24401.551121	31.447399
544.390352	24433.722201	31.452416
545.032142	24457.503350	31.457434
545.311477	24491.085418	31.462452
546.189099	24521.951860	31.467469
546.611321	24540.452693	31.472487
547.037925	24581.291918	31.477504
547.317523	24609.420504	31.482522
547.879555	24630.364224	31.487540
548.118330	24660.350826	31.492557
548.542068	24707.573372	31.497575
549.299736	24739.002296	31.502592
549.685078	24772.290277	31.507610
550.250403	24816.691520	31.512628
550.581141	24857.091230	31.517645
551.455277	24890.259077	31.522663
551.860864	24930.255474	31.527680
552.395906	24970.029573	31.532698
553.473263	24997.674301	31.537716
553.845787	25018.647930	31.542733
554.522431	25047.859158	31.547751
555.134385	25072.821121	31.552768
555.750094	25102.503242	31.557786
556.065273	25131.353772	31.562804
556.871481	25150.920277	31.567821
556.871161	25171.124245	31.572839
557.897664	25212.364295	31.577856
558.748644	25234.211606	31.582874
559.241326	25248.701819	31.587892
559.557053	25279.258771	31.592909
559.838046	25309.353524	31.597927
560.559838	25340.978570	31.602944
561.121169	25378.847178	31.607962
561.517594	25403.318575	31.612980
561.779382	25439.009409	31.617997
562.191473	25458.536456	31.623015
563.075800	25505.752378	31.628032
563.382444	25542.902581	31.633050
564.048255	25577.330022	31.638068
564.471360	25620.958903	31.643085
565.480247	25660.616369	31.648103
566.226767	25690.879373	31.653120
567.184917	25716.192708	31.658138
567.772183	25744.704735	31.663156
567.676357	25770.150617	31.668173
568.395481	25809.960924	31.673191
569.249831	25844.252035	31.678208
570.171869	25857.727879	31.683226
571.170611	25875.476619	31.688244
571.678287	25908.096502	31.693261
572.019603	25929.347695	31.698279
571.967485	25945.888688	31.703296
572.366123	25976.060924	31.708314
573.401313	26005.243011	31.713332
573.970982	26051.182033	31.718349
574.712836	26075.827991	31.723367
575.048890	26106.111282	31.728384
575.362922	26150.409240	31.733402
575.989169	26188.964458	31.738420
575.986425	26230.107714	31.743437
576.828731	26257.234623	31.748455
577.463007	26296.047913	31.753472
577.619327	26340.421399	31.758490
579.016059	26370.609486	31.763508
579.314753	26407.408605	31.768525
579.822644	26446.077540	31.773543
580.432321	26483.479344	31.778560
580.559890	26522.934432	31.783578
581.535054	26556.196749	31.788596
582.452187	26585.176857	31.793613
583.214301	26621.714624	31.798631
583.880970	26652.636151	31.803648
584.149610	26689.491024	31.808666
585.010877	26719.099388	31.813684
585.206584	26747.787553	31.818701
586.037784	26786.052884	31.823719
587.213529	26819.391853	31.828736
587.244264	26854.508114	31.833754
587.913991	26877.194407	31.838772
588.475843	26932.420909	31.843789
588.834543	26949.859430	31.848807
589.217260	26992.208259	31.853824
589.630418	27032.460462	31.858842
590.076593	27073.187938	31.863860
590.741346	27111.422916	31.868877
591.312441	27158.906364	31.873895
591.674890	27198.035473	31.878912
592.294148	27237.162601	31.883930
592.747089	27265.229993	31.888948
593.241973	27302.524779	31.893965
594.250352	27349.940601	31.898983
594.438674	27391.916030	31.904000
595.133207	27436.701115	31.909018
595.928177	27450.539109	31.914036
596.019266	27504.190857	31.919053
596.826921	27537.291260	31.924071
597.562226	27583.365988	31.929088
597.996798	27632.319155	31.934106
598.660005	27668.122088	31.939124
599.389666	27721.207293	31.944141
599.826009	27755.042136	31.949159
600.705270	27800.728365	31.954176
600.464813	27844.212530	31.959194
601.576951	27886.727772	31.964212
602.052200	27931.156218	31.969229
602.856813	27980.261192	31.974247
603.260970	28024.846281	31.979264
603.472693	28074.966570	31.984282
604.511107	28124.642263	31.989300
605.547920	28180.537721	31.994317
606.073832	28220.212199	31.999335
607.028458	28271.424543	32.004352
607.589394	28312.294654	32.009370
607.834075	28353.580671	32.014388
608.770307	28393.539243	32.019405
609.514676	28440.031661	32.024423
610.394420	28484.840788	32.029440
610.730278	28517.150311	32.034458
611.402135	28552.479407	32.039476
612.003717	28598.337068	32.044493
612.616997	28630.673110	32.049511
613.239545	28677.090223	32.054528
613.939444	28722.439845	32.059546
614.500113	28758.734712	32.064564
614.665953	28800.659658	32.069581
615.403834	28852.450786	32.074599
616.595278	28887.585804	32.079616
617.015917	28928.447386	32.084634
618.085440	28960.257831	32.089652
618.480573	29004.075332	32.094669
619.043508	29035.863625	32.099687
619.963175	29077.305181	32.104704
620.682656	29117.014478	32.109722
620.896073	29152.630889	32.114740
621.553870	29194.694965	32.119757
622.106429	29235.239544	32.124775
622.717469	29279.845734	32.129792
623.359993	29312.987375	32.134810
623.812051	29357.131776	32.139828
624.172194	29397.137749	32.144845
624.699599	29450.239978	32.149863
625.550479	29488.975084	32.154880
626.156529	29536.717791	32.159898
626.843649	29566.951588	32.164916
627.555914	29617.712005	32.169933
628.090505	29653.886102	32.174951
629.045444	29696.113543	32.179968
629.525867	29741.923098	32.184986
630.529455	29775.704591	32.190004
631.159943	29820.523845	32.195021
631.635791	29868.199098	32.200039
632.775270	29888.154467	32.205056
633.233933	29938.449473	32.210074
633.756458	29967.028080	32.215092
634.510021	29998.762909	32.220109
635.069662	30029.940113	32.225127
635.693681	30052.535928	32.230144
636.009200	30087.847297	32.235162
636.183484	30110.348839	32.240180
636.975296	30153.588712	32.245197
637.249227	30188.818232	32.250215
638.112465	30235.138196	32.255232
638.205665	30276.894151	32.260250
638.717295	30319.564836	32.265268
639.698087	30366.416739	32.270285
640.099852	30409.509270	32.275303
641.214883	30452.282255	32.280320
641.574841	30518.049439	32.285338
642.447505	30550.278599	32.290356
642.912457	30594.910388	32.295373
643.325515	30642.040937	32.300391
644.245892	30686.589385	32.305408
644.902297	30743.619361	32.310426
645.253939	30788.262886	32.315444
646.106097	30827.632451	32.320461
647.332348	30866.931212	32.325479
648.577385	30893.995293	32.330496
649.413239	30929.947738	32.335514
650.013598	30965.190982	32.340532
650.809909	31002.553056	32.345549
651.267520	31035.726262	32.350567
652.041583	31066.517659	32.355584
652.502509	31090.492786	32.360602
653.126692	31124.891846	32.365620
653.678052	31168.019567	32.370637
654.419802	31207.230044	32.375655
655.367578	31239.581342	32.380672
655.491844	31282.320642	32.385690
656.171399	31321.458839	32.390708
657.188413	31365.152951	32.395725
657.550064	31407.425693	32.400743
658.189413	31434.275020	32.405760
658.865698	31473.104258	32.410778
659.389760	31511.628546	32.415796
659.965759	31557.882410	32.420813
660.809477	31598.809864	32.425831
661.587452	31641.169990	32.430848
662.123620	31684.256900	32.435866
662.235214	31723.591741	32.440884
662.807360	31771.129966	32.445901
663.500826	31818.984462	32.450919
664.359028	31861.452661	32.455936
665.216405	31913.732303	32.460954
665.462553	31968.983595	32.465972
666.553891	32010.505484	32.470989
666.941071	32064.426483	32.476007
667.323820	32105.319228	32.481024
668.057058	32159.085454	32.486042
668.707275	32208.483763	32.491060
669.290310	32254.030046	32.496077
669.893008	32310.478450	32.501095
670.600816	32355.455535	32.506112
671.642903	32412.689260	32.511130
672.748898	32462.314347	32.516148
673.603957	32498.702734	32.521165
674.552944	32550.286958	32.526183
675.167710	32584.348525	32.531200
675.754022	32618.231243	32.536218
676.153391	32652.964965	32.541236
676.905069	32693.099703	32.546253
677.699689	32740.080793	32.551271
678.199441	32774.957139	32.556288
678.571792	32830.684180	32.561306
679.401622	32865.212162	32.566324
679.815004	32896.833705	32.571341
680.469405	32938.374892	32.576359
681.317993	32977.900827	32.581376
681.807694	33014.441821	32.586394
682.437032	33062.764345	32.591412
683.104011	33102.350397	32.596429
683.756744	33139.093824	32.601447
684.739522	33184.586234	32.606464
685.061208	33229.625314	32.611482
685.907306	33275.031723	32.616500
687.023873	33310.546305	32.621517
687.694075	33349.297808	32.626535
688.785672	33370.806603	32.631552
689.381642	33398.765270	32.636570
690.351623	33439.000225	32.641588
691.226933	33479.262640	32.646605
691.261567	33514.572989	32.651623
692.426227	33543.688786	32.656640
692.778695	33586.005312	32.661658
693.568820	33625.364553	32.666676
694.140817	33663.948584	32.671693
694.386710	33706.054344	32.676711
695.329622	33742.949649	32.681728
696.436296	33781.615040	32.686746
696.721826	33817.436876	32.691764
697.505356	33858.428722	32.696781
697.938312	33903.787010	32.701799
698.983803	33947.646496	32.706816
699.247716	33993.220961	32.711834
699.999917	34047.090255	32.716852
700.771612	34087.736664	32.721869
701.079572	34134.524788	32.726887
701.848817	34180.937734	32.731904
702.357461	34232.076226	32.736922
703.160365	34285.887661	32.741940
704.308022	34334.126109	32.746957
704.637708	34391.141067	32.751975
705.533853	34442.245037	32.756992
706.318364	34490.793274	32.762010
706.594793	34545.275316	32.767028
707.849049	34592.024629	32.772045
708.699376	34647.637835	32.777063
709.254182	34679.050377	32.782080
709.638446	34733.832245	32.787098
710.336051	34785.347307	32.792116
711.540967	34832.503155	32.797133
711.859656	34880.625324	32.802151
712.595411	34941.726160	32.807168
713.700017	34979.578469	32.812186
714.444318	35033.046871	32.817204
715.254286	35080.561919	32.822221
715.622410	35129.865614	32.827239
716.639723	35173.599270	32.832256
717.433637	35213.308643	32.837274
718.157196	35268.361536	32.842292
718.554715	35307.405684	32.847309
718.668615	35358.949785	32.852327
719.702432	35402.769865	32.857344
720.727992	35459.249436	32.862362
721.702552	35517.267204	32.867380
722.727980	35555.139195	32.872397
723.643000	35600.008789	32.877415
724.105360	35638.208847	32.882432
725.040704	35689.676461	32.887450
725.781827	35726.404330	32.892468
726.160540	35762.733436	32.897485
726.792942	35815.102095	32.902503
727.493660	35842.055019	32.907520
727.888997	35882.927873	32.912538
728.057854	35936.209932	32.917556
728.799491	35964.636196	32.922573
728.947011	36027.102638	32.927591
729.710921	36084.414972	32.932608
730.977099	36143.691582	32.937626
731.755400	36196.285065	32.942644
732.239457	36237.935161	32.947661
733.082684	36297.663743	32.952679
733.783556	36340.671346	32.957696
735.154511	36391.838902	32.962714
735.533970	36440.454671	32.967732
736.418742	36488.403847	32.972749
737.066960	36550.863437	32.977767
738.165457	36597.780545	32.982784
739.085012	36633.299794	32.987802
739.467126	36694.226781	32.992820
740.775891	36728.579057	32.997837
741.158462	36791.175553	33.002855
741.805850	36838.150769	33.007872
742.671358	36880.027283	33.012890
742.972939	36938.425594	33.017908
743.821391	36980.930957	33.022925
744.249154	37036.894437	33.027943
744.884310	37098.908719	33.032960
745.823780	37156.070145	33.037978
746.604301	37218.087438	33.042996
747.314236	37269.265157	33.048013
748.048834	37344.126215	33.053031
748.862605	37403.647491	33.058048
750.117320	37453.039874	33.063066
750.561482	37515.742724	33.068084
751.611866	37574.013559	33.073101
752.014713	37637.760229	33.078119
752.855155	37679.186930	33.083136
753.634751	37740.965594	33.088154
754.281993	37802.493132	33.093172
755.437751	37848.031894	33.098189
756.387412	37896.941622	33.103207
757.094205	37954.476547	33.108224
758.164137	37999.491497	33.113242
758.408355	38054.569303	33.118260
759.278157	38096.169299	33.123277
760.008913	38150.893380	33.128295
761.101388	38210.550573	33.133312
761.737076	38248.854798	33.138330
762.255188	38311.447285	33.143348
763.106452	38367.398904	33.148365
764.018881	38422.993347	33.153383
764.706288	38478.989735	33.158400
765.478834	38518.031971	33.163418
766.049003	38576.601614	33.168436
766.635220	38633.139018	33.173453
767.685047	38692.273000	33.178471
768.564956	38734.359584	33.183488
769.386766	38788.716987	33.188506
769.676462	38852.080154	33.193524
771.019063	38907.646830	33.198541
771.527724	38963.425675	33.203559
772.043999	39014.289897	33.208576
773.323405	39052.830509	33.213594
774.606117	39116.988444	33.218612
774.859417	39152.229838	33.223629
775.634530	39197.388050	33.228647
775.817437	39263.899351	33.233664
777.157155	39315.439229	33.238682
777.585210	39383.430466	33.243700
778.308904	39418.061538	33.248717
778.929660	39465.729634	33.253735
779.810246	39526.751483	33.258752
780.385144	39565.212963	33.263770
781.132487	39624.725435	33.268788
781.779113	39671.352827	33.273805
782.767645	39720.956289	33.278823
783.389288	39772.463587	33.283840
784.163501	39832.377183	33.288858
784.872660	39899.137364	33.293876
785.768838	39955.661599	33.298893
786.227023	40009.819392	33.303911
787.021536	40062.660147	33.308928
787.946445	40118.440416	33.313946
788.904492	40187.414123	33.318964
789.891637	40245.879110	33.323981
790.811104	40301.831449	33.328999
791.687854	40347.014184	33.334016
792.901487	40389.791973	33.339034
793.816972	40448.154825	33.344052
794.570874	40501.527880	33.349069
795.419707	40540.726328	33.354087
796.246163	40588.175145	33.359104
797.051017	40635.020300	33.364122
797.828403	40695.144485	33.369140
798.374163	40738.728923	33.374157
799.647559	40786.203463	33.379175
799.967509	40844.141491	33.384192
800.572505	40898.986970	33.389210
801.191439	40967.200100	33.394228
801.951383	41011.554936	33.399245
802.926217	41078.454464	33.404263
803.272721	41136.989952	33.409280
804.451221	41193.049722	33.414298
805.254633	41264.327707	33.419316
806.175648	41312.180795	33.424333
807.329020	41366.126229	33.429351
807.982673	41433.247603	33.434368
808.990898	41471.657652	33.439386
809.744183	41532.401373	33.444404
810.710807	41591.745953	33.449421
811.638651	41646.612624	33.454439
812.088823	41703.609274	33.459456
813.160424	41748.049908	33.464474
813.672918	41811.001217	33.469492
814.402808	41859.290030	33.474509
815.460817	41920.632504	33.479527
816.239770	41978.634902	33.484544
817.484218	42038.278977	33.489562
817.877178	42092.452094	33.494580
818.799475	42152.039107	33.499597
819.738460	42203.173866	33.504615
820.105040	42258.995926	33.509632
820.809500	42305.354314	33.514650
822.319712	42364.938933	33.519668
823.032517	42423.838272	33.524685
823.748341	42471.548744	33.529703
824.716362	42529.959578	33.534720
825.742043	42581.752154	33.539738
826.064725	42633.458215	33.544756
826.782817	42701.572763	33.549773
827.704901	42759.953411	33.554791
827.781826	42822.880549	33.559808
828.997775	42886.402197	33.564826
829.741676	42953.185275	33.569844
830.737870	43006.008078	33.574861
831.529280	43066.288387	33.579879
832.189716	43126.456424	33.584896
833.286298	43183.027387	33.589914
833.525857	43249.352245	33.594932
834.446146	43303.654979	33.599949
834.912095	43357.136742	33.604967
835.474755	43421.697734	33.609984
837.259841	43482.551881	33.615002
838.186089	43552.040819	33.620020
838.523807	43606.371734	33.625037
839.266312	43664.852307	33.630055
839.801877	43737.229975	33.635072
841.056986	43796.054885	33.640090
841.923607	43855.516018	33.645108
843.166283	43916.032007	33.650125
844.279531	43976.346927	33.655143
845.097222	44039.174862	33.660160
846.468721	44086.128934	33.665178
847.083503	44141.898140	33.670196
847.913815	44193.686960	33.675213
848.514087	44244.113820	33.680231
849.319329	44300.941730	33.685248
850.422827	44355.047742	33.690266
850.881321	44419.223034	33.695284
851.966934	44483.768968	33.700301
852.839067	44540.897021	33.705319
853.512283	44603.584583	33.710336
854.432645	44660.085546	33.715354
855.331581	44725.932650	33.720372
855.992569	44795.479426	33.725389
856.845451	44850.327782	33.730407
858.191484	44909.710785	33.735424
859.175147	44964.260743	33.740442
859.973371	45021.464791	33.745460
860.670184	45076.540415	33.750477
861.821672	45139.211964	33.755495
862.387141	45206.485042	33.760512
863.375085	45261.110967	33.765530
864.182298	45321.856713	33.770548
864.595147	45387.155202	33.775565
865.285980	45458.951320	33.780583
866.467694	45527.400890	33.785600
867.187951	45594.505550	33.790618
867.817003	45662.263504	33.795636
868.745008	45734.985094	33.800653
870.212280	45802.144887	33.805671
870.507923	45866.406620	33.810688
871.732884	45942.960349	33.815706
872.471448	46001.852523	33.820724
873.236187	46074.145172	33.825741
874.531590	46132.318427	33.830759
875.386516	46201.725522	33.835776
876.734086	46263.022291	33.840794
877.694881	46311.936426	33.845812
878.716965	46377.509864	33.850829
879.555871	46417.542665	33.855847
880.405523	46476.058214	33.860864
881.213794	46542.139860	33.865882
882.417938	46607.609719	33.870900
883.044301	46656.355254	33.875917
884.120177	46711.521389	33.880935
884.629714	46767.889196	33.885952
885.768702	46824.911958	33.890970
886.653655	46879.058105	33.895988
886.994026	46945.454160	33.901005
888.077155	46999.911355	33.906023
888.773401	47064.493714	33.911040
889.671510	47120.719677	33.916058
890.673312	47187.019808	33.921076
891.522102	47246.068887	33.926093
892.486570	47293.801597	33.931111
893.079326	47348.804104	33.936128
894.013558	47402.874249	33.941146
894.882252	47458.245271	33.946164
895.316857	47516.271423	33.951181
896.433056	47579.031194	33.956199
896.856812	47635.983882	33.961216
897.801846	47702.009679	33.966234
898.393690	47768.754908	33.971252
899.312561	47841.997156	33.976269
900.409129	47910.543149	33.981287
901.311603	47979.638324	33.986304
902.303234	48035.889963	33.991322
903.661278	48113.151555	33.996340
904.549640	48175.258869	34.001357
905.220894	48227.201964	34.006375
906.539048	48297.467051	34.011392
907.564485	48359.224557	34.016410
908.603803	48425.465537	34.021428
909.037552	48488.277120	34.026445
910.395021	48550.021418	34.031463
910.870869	48613.744138	34.036480
911.355494	48682.261188	34.041498
912.575006	48755.200194	34.046516
913.598108	48829.859206	34.051533
914.920039	48887.099097	34.056551
915.627705	48956.550223	34.061568
916.410614	49018.644622	34.066586
917.775718	49091.441835	34.071604
918.371697	49165.086574	34.076621
919.604254	49222.771435	34.081639
920.586983	49294.439401	34.086656
921.432763	49344.731912	34.091674
922.570307	49410.669438	34.096692
923.344392	49477.574784	34.101709
924.646869	49534.743410	34.106727
925.456210	49597.777959	34.111744
926.140281	49655.182338	34.116762
927.352423	49728.005392	34.121780
927.925779	49788.071955	34.126797
928.938996	49851.290579	34.131815
929.797095	49923.441776	34.136832
930.571531	49992.714828	34.141850
932.006906	50055.412763	34.146868
932.535712	50134.543863	34.151885
933.516510	50190.435542	34.156903
934.311027	50257.833489	34.161920
935.108758	50331.703650	34.166938
935.918898	50400.535811	34.171956
937.029726	50480.102643	34.176973
937.868480	50542.875801	34.181991
938.901149	50623.606820	34.187008
939.904209	50682.754676	34.192026
940.853686	50755.368793	34.197044
941.522185	50833.714970	34.202061
942.743379	50899.808260	34.207079
943.689963	50971.360545	34.212096
944.296963	51052.361795	34.217114
946.063974	51112.271317	34.222132
946.978122	51186.398166	34.227149
948.277691	51245.836656	34.232167
949.073834	51316.122670	34.237184
949.998837	51372.867431	34.242202
950.948618	51438.099711	34.247220
951.838939	51495.014681	34.252237
953.077783	51555.172080	34.257255
954.728416	51613.709007	34.262272
955.642347	51648.373733	34.267290
956.980679	51687.578773	34.272308
957.311427	51740.386406	34.277325
957.929283	51773.540872	34.282343
959.137700	51820.688256	34.287360
959.817691	51867.582639	34.292378
960.317392	51918.244693	34.297396
960.996655	51970.473423	34.302413
962.020447	52028.798932	34.307431
962.722931	52097.792113	34.312448
963.707713	52170.101458	34.317466
964.480203	52230.219310	34.322484
965.044314	52308.143799	34.327501
966.248380	52372.681063	34.332519
967.043995	52448.045290	34.337536
967.822189	52521.716677	34.342554
968.717336	52587.194814	34.347572
969.565558	52662.266802	34.352589
970.510081	52745.948636	34.357607
971.465446	52829.451907	34.362624
972.296084	52909.621211	34.367642
973.561688	52984.882375	34.372660
974.538846	53080.291925	34.377677
975.637696	53152.453680	34.382695
976.922702	53227.219040	34.387712
977.829331	53312.383177	34.392730
978.934180	53387.202403	34.397748
979.626478	53467.667251	34.402765
981.183951	53552.180426	34.407783
981.784940	53625.243761	34.412800
982.978121	53702.733274	34.417818
983.871415	53772.062392	34.422836
984.943618	53858.930267	34.427853
986.030813	53931.305060	34.432871
986.916331	54004.603717	34.437888
988.132740	54095.898604	34.442906
989.386688	54165.444849	34.447924
990.042720	54254.884874	34.452941
990.723162	54321.736506	34.457959
991.951386	54401.918633	34.462976
992.993027	54482.497109	34.467994
994.032009	54560.234937	34.473012
995.027671	54637.340620	34.478029
996.211650	54708.892736	34.483047
997.389962	54794.374332	34.488064
998.373995	54871.121881	34.493082
999.667222	54943.942335	34.498100
1000.406307	55021.715710	34.503117
1001.552162	55090.465166	34.508135
1002.614527	55173.991760	34.513152
1003.473518	55243.311564	34.518170
1004.530961	55308.753046	34.523188
1005.683195	55381.134825	34.528205
1007.130795	55449.319430	34.533223
1008.543030	55506.124946	34.538240
1009.180746	55572.132435	34.543258
1010.064457	55632.064491	34.548276
1011.324093	55701.272644	34.553293
1012.289105	55768.476437	34.558311
1013.256211	55824.624233	34.563328
1014.572207	55894.248185	34.568346
1015.545541	55949.572602	34.573364
1016.386427	56016.517964	34.578381
1017.353009	56080.634073	34.583399
1018.281109	56127.979317	34.588416
1019.210452	56209.397539	34.593434
1019.964170	56282.141544	34.598452
1021.021576	56356.439642	34.603469
1021.797221	56412.435099	34.608487
1022.825241	56478.441308	34.613504
1023.709753	56541.628464	34.618522
1024.742027	56606.457232	34.623540
1025.551987	56666.099598	34.628557
1026.474728	56728.971193	34.633575
1027.584575	56798.231171	34.638592
1028.215987	56868.806260	34.643610
1029.272481	56948.890832	34.648628
1030.232543	57023.598544	34.653645
1031.245520	57096.988188	34.658663
1032.214908	57171.125316	34.663680
1032.899340	57253.528218	34.668698
1034.132726	57334.251076	34.673716
1035.317900	57413.361511	34.678733
1036.073861	57490.779578	34.683751
1037.723890	57565.710686	34.688768
1038.356673	57653.395013	34.693786
1039.349592	57735.162957	34.698804
1040.573587	57829.160834	34.703821
1041.862093	57900.813874	34.708839
1043.193736	57979.105917	34.713856
1043.913778	58057.461771	34.718874
1045.279159	58124.217468	34.723892
1045.973188	58209.457588	34.728909
1046.975323	58294.377897	34.733927
1048.366083	58374.934186	34.738944
1049.220971	58460.188128	34.743962
1050.373204	58536.123810	34.748980
1051.451197	58612.166225	34.753997
1052.673417	58691.806753	34.759015
1054.183757	58757.801122	34.764032
1054.881692	58854.650770	34.769050
1056.234254	58914.511736	34.774068
1057.047437	58992.064964	34.779085
1058.357530	59075.819796	34.784103
1059.816983	59138.297683	34.789120
1060.482400	59221.514103	34.794138
1062.071819	59295.497965	34.799156
1063.158472	59360.806733	34.804173
1064.299594	59433.753151	34.809191
1065.300450	59503.360684	34.814208
1065.833404	59588.732007	34.819226
1066.900056	59663.975649	34.824244
1067.662893	59733.918378	34.829261
1068.584203	59825.439331	34.834279
1070.464219	59904.645991	34.839296
1070.969428	59992.200415	34.844314
1072.107820	60072.421861	34.849332
1073.038528	60149.922514	34.854349
1073.974277	60235.847380	34.859367
1075.483252	60307.916308	34.864384
1076.475327	60399.073940	34.869402
1077.513432	60478.191978	34.874420
1078.738784	60555.344230	34.879437
1079.552651	60631.294828	34.884455
1081.034516	60703.900845	34.889472
1081.604084	60810.772954	34.894490
1082.861803	60887.338875	34.899508
1083.974849	60967.206407	34.904525
1084.998177	61046.708374	34.909543
1086.058950	61118.868451	34.914560
1087.147189	61207.950590	34.919578
1088.041111	61290.771365	34.924596
1089.427738	61376.319887	34.929613
1090.470373	61455.984753	34.934631
1091.686051	61532.432634	34.939648
1092.318191	61620.916289	34.944666
1093.600017	61699.740803	34.949684
1094.469163	61770.229848	34.954701
1095.756282	61843.660810	34.959719
1096.769558	61917.584052	34.964736
1097.750635	61997.405844	34.969754
1098.806949	62077.766904	34.974772
1099.689510	62156.749982	34.979789
1100.445520	62228.568286	34.984807
1101.374229	62306.905315	34.989824
1102.926449	62404.338694	34.994842
1103.949785	62488.763882	34.999860
1105.094591	62566.878192	35.004877
1105.889449	62659.562511	35.009895
1107.224871	62743.237330	35.014912
1108.368893	62843.179467	35.019930
1109.387199	62926.537108	35.024948
1110.622940	63014.298763	35.029965
1111.662921	63102.515335	35.034983
1112.590856	63188.103554	35.040000
1113.443097	63284.832731	35.045018
1114.649993	63375.695730	35.050036
1116.375623	63475.024451	35.055053
1117.378452	63569.199106	35.060071
1118.927358	63647.709713	35.065088
1119.865844	63746.687255	35.070106
1120.969660	63829.097692	35.075124
1122.174939	63918.557539	35.080141
1123.298127	64016.893336	35.085159
1124.831060	64112.817076	35.090176
1125.630179	64195.428086	35.095194
1126.784794	64287.315450	35.100212
1128.041093	64368.608727	35.105229
1129.249182	64469.750250	35.110247
1130.147852	64545.199534	35.115264
1131.219083	64651.592287	35.120282
1132.221902	64730.887688	35.125300
1133.877254	64821.781106	35.130317
1134.702852	64921.648188	35.135335
1136.209343	65005.664833	35.140352
1137.514614	65111.339372	35.145370
1138.534096	65192.229020	35.150388
1139.573789	65284.771017	35.155405
1140.707867	65375.304413	35.160423
1141.757196	65462.799798	35.165440
1142.840400	65552.695991	35.170458
1144.184576	65646.059267	35.175476
1145.294650	65730.007084	35.180493
1146.324193	65824.850812	35.185511
1147.649895	65916.483253	35.190528
1148.645210	66013.112050	35.195546
1149.852902	66117.033282	35.200564
1151.160081	66200.578445	35.205581
1152.266911	66304.433842	35.210599
1153.072983	66383.701755	35.215616
1154.424630	66470.444476	35.220634
1155.409653	66570.514856	35.225652
1156.932460	66664.398574	35.230669
1158.427828	66755.089606	35.235687
1159.418741	66828.790255	35.240704
1160.886498	66921.379242	35.245722
1161.604434	67013.034274	35.250740
1163.319280	67097.766215	35.255757
1164.356963	67184.705867	35.260775
1165.801435	67258.527105	35.265792
1166.920751	67350.063890	35.270810
1168.187673	67420.538575	35.275828
1169.785804	67494.805109	35.280845
1170.413952	67575.453036	35.285863
1171.723106	67651.024974	35.290880
1172.774559	67719.982803	35.295898
1173.938552	67793.260416	35.300916
1174.881308	67863.590505	35.305933
1175.725246	67940.483031	35.310951
1176.317306	68008.563407	35.315968
1177.560388	68100.590145	35.320986
1178.232672	68195.447666	35.326004
1179.294240	68266.627804	35.331021
1180.917479	68360.153891	35.336039
1182.112836	68448.700544	35.341056
1183.509860	68532.467311	35.346074
1184.864661	68621.508944	35.351092
1186.270342	68702.634576	35.356109
1187.142713	68779.575845	35.361127
1188.811605	68871.450421	35.366144
1189.837505	68957.701428	35.371162
1191.496869	69032.526425	35.376180
1192.805596	69095.894869	35.381197
1193.658702	69189.474198	35.386215
1195.300332	69267.550902	35.391232
1196.401616	69357.191750	35.396250
1197.551550	69429.602412	35.401268
1198.429613	69516.353194	35.406285
1199.691261	69601.233609	35.411303
1201.005012	69683.503733	35.416320
1201.585908	69770.630887	35.421338
1203.106800	69860.467779	35.426356
1203.991786	69957.958139	35.431373
1205.360308	70045.242231	35.436391
1206.317692	70147.319142	35.441408
1207.790782	70237.278759	35.446426
1208.799728	70336.980164	35.451444
1210.407773	70424.373888	35.456461
1211.133387	70528.603326	35.461479
1212.165191	70630.404596	35.466496
1213.482737	70727.209949	35.471514
1214.795802	70834.717941	35.476532
1216.299689	70925.200723	35.481549
1217.021285	71031.484467	35.486567
1218.076956	71134.259168	35.491584
1219.345953	71233.112978	35.496602
1220.354755	71344.849808	35.501620
1221.864899	71449.594047	35.506637
1223.130095	71557.391089	35.511655
1224.866547	71652.956829	35.516672
1225.974018	71754.674708	35.521690
1227.423927	71858.150787	35.526708
1228.654751	71954.695550	35.531725
1229.733101	72055.722546	35.536743
1231.126557	72159.373246	35.541760
1232.158557	72254.974836	35.546778
1233.187953	72364.407717	35.551796
1234.744328	72459.548469	35.556813
1236.041134	72558.972885	35.561831
1237.624998	72651.703622	35.566848
1238.627496	72750.414640	35.571866
1239.957219	72858.105643	35.576884
1241.533511	72950.116669	35.581901
1242.618625	73046.802103	35.586919
1243.511885	73143.188444	35.591936
1245.469012	73248.959519	35.596954
1246.431542	73332.112720	35.601972
1248.802570	73393.274386	35.606989
1249.923306	73475.200158	35.612007
1251.443313	73559.394562	35.617024
1252.585543	73634.097916	35.622042
1253.885007	73719.834403	35.627060
1255.183413	73781.442575	35.632077
1255.927961	73858.057696	35.637095
1256.834347	73937.358389	35.642112
1258.053772	74006.275040	35.647130
1258.964252	74075.683272	35.652148
1259.737513	74148.722907	35.657165
1260.752303	74240.306494	35.662183
1261.751837	74337.440597	35.667200
1262.930587	74424.046782	35.672218
1263.820595	74534.016959	35.677236
1265.351334	74630.119466	35.682253
1266.413342	74727.650587	35.687271
1267.617169	74831.759238	35.692288
1268.538678	74934.316252	35.697306
1269.065075	75051.641087	35.702324
1271.006816	75155.547471	35.707341
1272.288543	75273.135705	35.712359
1273.771953	75380.926983	35.717376
1275.233737	75491.952098	35.722394
1276.387735	75609.713687	35.727412
1277.851767	75714.988612	35.732429
1279.395756	75819.694158	35.737447
1280.663966	75945.052284	35.742464
1281.759989	76046.205665	35.747482
1282.819818	76160.766879	35.752500
1284.328982	76273.624571	35.757517
1285.578181	76397.024340	35.762535
1287.283363	76507.167041	35.767552
1288.555628	76609.878508	35.772570
1289.818427	76723.789812	35.777588
1291.163389	76833.153859	35.782605
1292.658945	76947.093208	35.787623
1294.256079	77053.834724	35.792640
1295.648178	77168.462484	35.797658
1296.805592	77279.212951	35.802676
1298.231518	77380.484637	35.807693
1299.498914	77495.234524	35.812711
1301.182950	77592.793177	35.817728
1302.856918	77686.832086	35.822746
1304.151497	77792.496152	35.827764
1305.680609	77874.840461	35.832781
1306.984714	77973.549053	35.837799
1308.029399	78067.433862	35.842816
1309.671934	78156.842788	35.847834
1311.352826	78268.187193	35.852852
1312.438629	78356.112580	35.857869
1313.719306	78456.980147	35.862887
1315.235583	78541.887436	35.867904
1316.865517	78625.611817	35.872922
1317.860716	78721.672842	35.877940
1319.197346	78809.763334	35.882957
1320.534055	78898.145469	35.887975
1321.776610	78990.520433	35.892992
1323.085403	79068.443329	35.898010
1324.091554	79178.414235	35.903028
1325.560948	79275.847596	35.908045
1326.712245	79361.726363	35.913063
1327.894098	79471.354372	35.918080
1329.487314	79564.120079	35.923098
1330.695852	79666.498210	35.928116
1332.332375	79762.285673	35.933133
1333.333792	79852.965431	35.938151
1334.363396	79957.488184	35.943168
1336.171003	80051.438367	35.948186
1337.565846	80157.311275	35.953204
1338.244031	80256.606890	35.958221
1339.670170	80358.497620	35.963239
1340.902882	80456.592759	35.968256
1342.224491	80550.493586	35.973274
1343.452391	80643.598487	35.978292
1344.557542	80732.389925	35.983309
1345.636479	80835.286635	35.988327
1347.023136	80924.934389	35.993344
1348.298560	81026.863692	35.998362
1349.365424	81128.534432	36.003380
1350.771835	81224.388087	36.008397
1351.997407	81332.166883	36.013415
1352.837955	81445.846688	36.018432
1354.108228	81556.001264	36.023450
1355.468242	81671.488900	36.028468
1356.876794	81782.104287	36.033485
1358.045545	81894.189118	36.038503
1359.357887	82025.383466	36.043520
1360.805183	82132.662039	36.048538
1362.320697	82261.621307	36.053556
1363.677644	82388.958748	36.058573
1365.431346	82509.849310	36.063591
1366.608778	82627.941304	36.068608
1368.058161	82746.662981	36.073626
1370.153675	82871.987120	36.078644
1371.048251	82988.059401	36.083661
1372.372840	83094.942610	36.088679
1373.856454	83228.003757	36.093696
1375.161946	83339.084747	36.098714
1376.775506	83469.060559	36.103732
1378.292227	83584.658328	36.108749
1379.892962	83690.791248	36.113767
1381.132366	83822.119307	36.118784
1383.061469	83931.585071	36.123802
1384.307513	84038.902185	36.128820
1385.836763	84158.859061	36.133837
1387.283405	84273.013390	36.138855
1387.984690	84390.667312	36.143872
1389.876248	84512.026427	36.148890
1391.650613	84626.105813	36.153908
1392.874909	84744.718802	36.158925
1394.278123	84855.790483	36.163943
1395.395577	84981.744965	36.168960
1396.747711	85095.917280	36.173978
1398.427274	85214.461347	36.178996
1399.873097	85330.875492	36.184013
1401.149843	85433.023159	36.189031
1402.367590	85561.410132	36.194048
1404.369103	85688.053739	36.199066
1405.491368	85813.985765	36.204084
1406.648340	85927.824277	36.209101
1408.176452	86043.518881	36.214119
1409.415941	86164.276844	36.219136
1410.675101	86279.748147	36.224154
1412.573259	86402.140604	36.229172
1414.138009	86521.785001	36.234189
1415.797954	86630.314527	36.239207
1417.072333	86748.611149	36.244224
1418.562433	86861.641157	36.249242
1420.291353	86972.340800	36.254260
1421.487800	87094.452558	36.259277
1423.006610	87199.686094	36.264295
1423.898262	87316.511266	36.269312
1425.680185	87428.167471	36.274330
1427.408013	87528.680946	36.279348
1428.548036	87651.690870	36.284365
1430.162858	87753.756055	36.289383
1431.682262	87866.126425	36.294400
1433.589984	87977.131525	36.299418
1435.343555	88072.840006	36.304436
1436.498281	88166.538370	36.309453
1438.291890	88263.242370	36.314471
1439.548788	88353.884014	36.319488
1440.860243	88429.373646	36.324506
1441.957813	88525.832011	36.329524
1443.314843	88612.340247	36.334541
1444.774565	88692.585088	36.339559
1446.283470	88787.396193	36.344576
1447.835485	88870.136364	36.349594
1448.992141	88963.139955	36.354612
1450.277232	89070.799071	36.359629
1451.971459	89157.928085	36.364647
1452.907720	89272.004044	36.369664
1453.866929	89369.500537	36.374682
1455.466239	89470.256085	36.379700
1456.755810	89584.126175	36.384717
1458.004658	89702.742807	36.389735
1459.138673	89821.327092	36.394752
1460.628009	89938.690603	36.399770
1462.192610	90061.999326	36.404788
1463.611682	90191.934041	36.409805
1465.058602	90311.016526	36.414823
1466.221552	90443.362131	36.419840
1467.237830	90585.895336	36.424858
1469.332976	90711.519461	36.429876
1470.056995	90838.637563	36.434893
1472.100637	90971.215958	36.439911
1473.433109	91116.313252	36.444928
1475.099929	91245.732371	36.449946
1476.827144	91382.835694	36.454964
1478.401923	91512.777242	36.459981
1479.864720	91645.157512	36.464999
1481.367949	91791.955144	36.470016
1482.694780	91934.243609	36.475034
1484.413971	92059.513631	36.480052
1485.900922	92191.094059	36.485069
1487.574568	92323.457153	36.490087
1489.057995	92470.755453	36.495104
1490.438427	92602.506336	36.500122
1491.998728	92736.625264	36.505140
1493.331450	92871.160440	36.510157
1494.506128	93014.453584	36.515175
1496.338785	93147.074352	36.520192
1498.317888	93275.224092	36.525210
1500.348802	93411.009168	36.530228
1501.543009	93542.057958	36.535245
1503.305789	93672.739966	36.540263
1504.817837	93802.270117	36.545280
1506.034439	93932.125649	36.550298
1508.068621	94057.659052	36.555316
1509.348101	94198.457121	36.560333
1510.937875	94321.360984	36.565351
1512.269989	94447.461554	36.570368
1513.862052	94580.062589	36.575386
1515.663441	94712.213330	36.580404
1517.077231	94829.366686	36.585421
1518.664145	94954.669151	36.590439
1520.354207	95084.950182	36.595456
1521.949664	95211.760732	36.600474
1523.657316	95334.941813	36.605492
1524.855956	95451.814122	36.610509
1526.541638	95574.581280	36.615527
1528.019729	95709.017499	36.620544
1529.726665	95825.114935	36.625562
1531.105282	95938.234396	36.630580
1532.764488	96064.049788	36.635597
1534.541507	96176.309527	36.640615
1536.012668	96301.445296	36.645632
1537.429724	96418.832298	36.650650
1539.006198	96534.306202	36.655668
1540.275044	96640.739684	36.660685
1541.939348	96728.490801	36.665703
1543.595783	96844.080162	36.670720
1545.015383	96949.591222	36.675738
1546.562148	97046.995418	36.680756
1547.525613	97158.916283	36.685773
1549.059139	97264.296580	36.690791
1550.641661	97379.075451	36.695808
1552.295542	97486.554709	36.700826
1553.649841	97608.963097	36.705844
1554.804895	97729.298673	36.710861
1556.420474	97853.518108	36.715879
1558.363467	97977.065917	36.720896
1559.511028	98095.198324	36.725914
1561.101672	98222.795072	36.730932
1562.834607	98348.709533	36.735949
1564.294793	98470.787850	36.740967
1565.738281	98606.877135	36.745984
1567.522859	98746.450765	36.751002
1568.641178	98857.199924	36.756020
1570.489177	98995.040708	36.761037
1572.377006	99118.804370	36.766055
1573.907635	99243.308670	36.771072
1575.582032	99373.546499	36.776090
1577.350791	99509.145300	36.781108
1578.582198	99641.367421	36.786125
1580.055296	99773.653886	36.791143
1582.142320	99904.590285	36.796160
1583.416540	100047.849386	36.801178
1585.244442	100170.536175	36.806196
1586.942537	100308.773578	36.811213
1588.662064	100436.523895	36.816231
1590.354822	100572.126324	36.821248
1591.900835	100704.963074	36.826266
1593.884670	100824.737571	36.831284
1595.342650	100968.948335	36.836301
1596.853276	101095.009587	36.841319
1598.210569	101230.603593	36.846336
1599.716459	101355.829853	36.851354
1601.580389	101484.829615	36.856372
1603.170829	101617.409621	36.861389
1605.170613	101750.801241	36.866407
1606.659467	101893.819555	36.871424
1607.934498	102025.436058	36.876442
1609.657337	102162.029325	36.881460
1611.128369	102307.549831	36.886477
1612.646094	102434.325131	36.891495
1614.294098	102575.318470	36.896512
1615.632971	102715.219467	36.901530
1617.380016	102850.987733	36.906548
1619.196642	102995.138926	36.911565
1620.604638	103137.908989	36.916583
1622.080410	103287.059163	36.921600
1623.550304	103428.578337	36.926618
1625.359139	103571.604850	36.931636
1626.602852	103725.560334	36.936653
1628.216794	103870.215999	36.941671
1629.986250	104031.267319	36.946688
1631.502858	104176.535376	36.951706
1633.167459	104319.169146	36.956724
1634.624726	104471.877651	36.961741
1636.508317	104620.032074	36.966759
1638.261264	104760.333689	36.971776
1639.887315	104914.184431	36.976794
1641.723420	105050.429629	36.981812
1643.227034	105206.342138	36.986829
1644.856127	105343.406865	36.991847
1646.832855	105480.202493	36.996864
1648.592306	105613.292029	37.001882
1650.444659	105730.581542	37.006900
1651.811852	105862.668028	37.011917
1653.196208	105989.781923	37.016935
1655.020720	106108.484527	37.021952
1656.053720	106240.332867	37.026970
1658.199464	106373.669587	37.031988
1659.925919	106516.442520	37.037005
1661.306476	106645.233206	37.042023
1662.951133	106773.044956	37.047040
1664.163130	106920.172805	37.052058
1666.025635	107054.989124	37.057076
1667.700745	107200.930256	37.062093
1669.033200	107341.041736	37.067111
1670.951521	107498.497935	37.072128
1672.324495	107638.731128	37.077146
1674.191000	107794.611714	37.082164
1675.322165	107948.223538	37.087181
1676.698208	108103.522478	37.092199
1678.685135	108258.536831	37.097216
1680.216508	108428.116689	37.102234
1682.203025	108582.726783	37.107252
1684.124177	108735.648527	37.112269
1686.112736	108897.906172	37.117287
1687.928559	109050.135575	37.122304
1689.731521	109210.863830	37.127322
1691.245734	109369.203030	37.132340
1693.416640	109514.696352	37.137357
1695.528633	109658.107080	37.142375
1697.669592	109800.157014	37.147392
1699.332426	109948.762002	37.152410
1700.964009	110088.267390	37.157428
1702.784881	110240.171489	37.162445
1704.368492	110386.355863	37.167463
1706.167718	110528.106859	37.172480
1707.479673	110674.372755	37.177498
1709.543876	110820.027602	37.182516
1711.135617	110973.796658	37.187533
1713.184877	111113.165013	37.192551
1714.753690	111261.929677	37.197568
1716.453036	111413.756294	37.202586
1717.780251	111555.965329	37.207604
1719.663756	111705.913003	37.212621
1721.589170	111859.684697	37.217639
1723.577100	111998.939260	37.222656
1725.355307	112149.425148	37.227674
1726.920125	112290.408034	37.232692
1729.002597	112440.074191	37.237709
1730.411734	112588.653655	37.242727
1732.227282	112731.907396	37.247744
1733.826212	112881.599927	37.252762
1735.543203	113032.999491	37.257780
1737.428259	113177.169993	37.262797
1739.310388	113325.070136	37.267815
1741.395339	113461.842227	37.272832
1743.090345	113614.186150	37.277850
1745.310243	113743.557124	37.282868
1746.809280	113882.197545	37.287885
1748.539957	114009.476898	37.292903
1750.444238	114144.795828	37.297920
1751.397796	114295.431714	37.302938
1753.119934	114443.323277	37.307956
1754.964429	114589.103737	37.312973
1756.365819	114740.610288	37.317991
1757.734084	114882.851433	37.323008
1759.615334	115042.832816	37.328026
1761.571467	115194.229540	37.333044
1762.884589	115347.553325	37.338061
1764.294695	115486.492707	37.343079
1765.996997	115628.532557	37.348096
1767.464776	115772.600715	37.353114
1769.148149	115914.568514	37.358132
1770.834691	116067.494728	37.363149
1772.089014	116224.585564	37.368167
1773.639893	116374.781875	37.373184
1775.260727	116538.767501	37.378202
1777.312706	116712.034496	37.383220
1779.115532	116881.612105	37.388237
1780.494930	117055.441985	37.393255
1782.361036	117209.892355	37.398272
1784.162982	117392.118053	37.403290
1785.859686	117563.402211	37.408308
1788.026719	117728.246654	37.413325
1789.232701	117914.905524	37.418343
1791.291047	118099.910581	37.423360
1793.360982	118283.367289	37.428378
1795.133969	118453.349853	37.433396
1797.448326	118623.794341	37.438413
1799.356971	118806.606431	37.443431
1801.465560	118972.074246	37.448448
1803.323064	119149.746133	37.453466
1805.137381	119321.869807	37.458484
1807.016268	119499.590735	37.463501
1808.804381	119670.223294	37.468519
1811.013135	119834.601082	37.473536
1813.155000	120010.190501	37.478554
1814.981150	120174.806879	37.483572
1817.125696	120344.258029	37.488589
1818.415939	120509.999397	37.493607
1820.347539	120671.062432	37.498624
1821.869755	120856.912707	37.503642
1823.370246	121032.264114	37.508660
1825.683784	121212.360817	37.513677
1827.661708	121391.457729	37.518695
1829.515281	121547.272247	37.523712
1831.345063	121722.207648	37.528730
1833.348145	121898.169737	37.533748
1835.127511	122066.492836	37.538765
1836.935881	122243.767997	37.543783
1838.895265	122420.880918	37.548800
1840.440129	122591.526140	37.553818
1842.431847	122767.950577	37.558836
1844.593568	122953.749355	37.563853
1846.294876	123132.009285	37.568871
1848.200985	123294.089265	37.573888
1849.898248	123474.888505	37.578906
1852.013862	123642.950346	37.583924
1854.065675	123816.883690	37.588941
1855.931484	123988.461794	37.593959
1857.910036	124149.214652	37.598976
1859.349334	124330.057923	37.603994
1861.470410	124498.198636	37.609012
1863.543707	124664.774411	37.614029
1865.127463	124843.973693	37.619047
1867.327427	125009.503604	37.624064
1868.675161	125190.073213	37.629082
1870.727874	125369.468257	37.634100
1872.504607	125551.520447	37.639117
1873.863782	125717.919929	37.644135
1875.748918	125902.620978	37.649152
1877.134081	126088.783515	37.654170
1878.946194	126279.663310	37.659188
1880.816270	126468.238687	37.664205
1882.218443	126657.166864	37.669223
1884.269286	126849.230089	37.674240
1886.098415	127035.581573	37.679258
1887.466464	127222.437016	37.684276
1889.797568	127395.707919	37.689293
1891.137779	127588.621037	37.694311
1892.782952	127761.632305	37.699328
1894.823312	127958.041307	37.704346
1896.386105	128139.085244	37.709364
1898.091505	128332.541281	37.714381
1899.752200	128536.827453	37.719399
1902.059689	128736.890562	37.724416
1903.722010	128938.425282	37.729434
1905.505694	129132.240769	37.734452
1907.605189	129336.779735	37.739469
1909.479644	129546.531267	37.744487
1911.311088	129745.150749	37.749504
1913.507601	129956.211773	37.754522
1915.100988	130176.160365	37.759540
1917.394327	130380.699584	37.764557
1919.000226	130604.632434	37.769575
1921.230583	130811.683046	37.774592
1922.836070	131036.937777	37.779610
1924.806639	131250.019707	37.784628
1927.101739	131466.820577	37.789645
1929.091018	131680.155488	37.794663
1931.011147	131903.957390	37.799680
1933.184945	132116.402930	37.804698
1935.346860	132337.542946	37.809716
1937.430337	132547.555783	37.814733
1939.680309	132766.780998	37.819751
1941.810434	132973.020117	37.824768
1944.003186	133179.339282	37.829786
1946.057006	133381.455687	37.834804
1948.569453	133582.283517	37.839821
1950.337130	133789.940584	37.844839
1952.725225	133985.104991	37.849856
1954.244700	134182.879796	37.854874
1956.706151	134394.745978	37.859892
1958.926131	134591.017784	37.864909
1960.802075	134776.329817	37.869927
1963.040918	134966.078116	37.874944
1965.388365	135162.484867	37.879962
1967.319561	135341.116092	37.884980
1969.232576	135527.199511	37.889997
1971.173413	135724.217642	37.895015
1973.360462	135906.313570	37.900032
1974.969806	136094.058150	37.905050
1976.983449	136288.174198	37.910068
1979.229861	136471.798598	37.915085
1981.002397	136663.821918	37.920103
1982.950600	136858.876932	37.925120
1984.404599	137050.672279	37.930138
1986.246313	137267.343625	37.935156
1988.260598	137452.200937	37.940173
1990.026161	137660.497967	37.945191
1991.751679	137865.083998	37.950208
1993.464975	138073.835177	37.955226
1995.541436	138287.035769	37.960244
1997.777448	138498.372432	37.965261
1999.198475	138712.260728	37.970279
2001.213452	138930.143842	37.975296
2003.688187	139141.700070	37.980314
2005.685707	139353.103095	37.985332
2007.077496	139557.735799	37.990349
2009.067812	139785.779094	37.995367
2010.997756	140000.203193	38.000384
2013.079224	140218.462635	38.005402
2014.889940	140447.552317	38.010420
2017.339111	140651.809437	38.015437
2019.163761	140872.992651	38.020455
2020.881794	141070.169654	38.025472
2022.788789	141279.729782	38.030490
2024.728819	141482.902119	38.035508
2026.877882	141687.286501	38.040525
2028.731068	141893.938735	38.045543
2030.569986	142106.685819	38.050560
2032.569207	142314.814673	38.055578
2034.169697	142536.827245	38.060596
2036.093441	142757.673682	38.065613
2037.600913	142983.814745	38.070631
2040.122847	143211.689987	38.075648
2042.370672	143441.931488	38.080666
2044.255596	143684.389044	38.085684
2046.061859	143905.258910	38.090701
2047.665317	144152.255387	38.095719
2049.893645	144387.517520	38.100736
2051.999150	144628.574641	38.105754
2054.110043	144877.488339	38.110772
2056.740557	145105.203056	38.115789
2059.031202	145354.370360	38.120807
2060.724193	145594.138264	38.125824
2063.204475	145835.460129	38.130842
2065.165661	146074.947412	38.135860
2067.668604	146312.993438	38.140877
2069.371176	146561.420491	38.145895
2071.594616	146813.448458	38.150912
2073.964092	147058.778731	38.155930
2075.765805	147303.145056	38.160948
2078.452063	147545.331375	38.165965
2080.451275	147794.682821	38.170983
2082.212245	148044.135999	38.176000
2084.584000	148283.874246	38.181018
2086.719169	148530.352182	38.186036
2088.928708	148774.268442	38.191053
2090.905998	149020.125904	38.196071
2092.877169	149276.964844	38.201088
2095.205294	149519.050987	38.206106
2097.415383	149765.954571	38.211124
2099.469385	150007.730186	38.216141
2101.671307	150255.931995	38.221159
2104.083734	150496.524333	38.226176
2106.230130	150750.817114	38.231194
2108.261075	150996.954545	38.236212
2110.376734	151232.392067	38.241229
2112.434061	151484.658504	38.246247
2114.675386	151734.346072	38.251264
2116.578521	151975.113056	38.256282
2118.701790	152233.567128	38.261300
2120.938017	152470.679445	38.266317
2122.991406	152718.077767	38.271335
2125.211551	152964.105694	38.276352
2127.897283	153215.203253	38.281370
2129.461890	153453.515943	38.286388
2131.312047	153701.508772	38.291405
2133.897703	153960.927083	38.296423
2135.711739	154226.762930	38.301440
2138.084746	154470.069803	38.306458
2139.958127	154728.434608	38.311476
2142.372268	154966.989570	38.316493
2144.396855	155215.799666	38.321511
2146.767015	155450.745605	38.326528
2149.354851	155702.326366	38.331546
2151.280921	155960.625019	38.336564
2153.910060	156201.944394	38.341581
2156.036464	156431.168924	38.346599
2157.788096	156675.622733	38.351616
2159.985689	156906.577200	38.356634
2162.260081	157151.357853	38.361652
2164.034179	157371.754570	38.366669
2165.970973	157598.956590	38.371687
2167.847600	157821.535216	38.376704
2170.191449	158040.474689	38.381722
2172.062938	158274.709717	38.386740
2174.058434	158507.504516	38.391757
2176.233798	158732.680580	38.396775
2178.238309	158974.349608	38.401792
2180.018371	159217.717590	38.406810
2181.654227	159468.383332	38.411828
2184.009515	159708.464551	38.416845
2186.029161	159971.932905	38.421863
2188.373125	160239.960323	38.426880
2190.394206	160488.107353	38.431898
2192.490721	160756.721410	38.436916
2194.553473	161025.862390	38.441933
2196.831823	161301.179104	38.446951
2198.706124	161576.597987	38.451968
2201.130472	161851.145331	38.456986
2203.215218	162136.614263	38.462004
2205.232202	162413.601528	38.467021
2207.491704	162699.617080	38.472039
2209.333605	162998.953419	38.477056
2211.591007	163270.231873	38.482074
2213.924257	163571.995487	38.487092
2216.176208	163859.909029	38.492109
2218.783346	164159.106201	38.497127
2220.709477	164455.033526	38.502144
2223.170393	164743.527815	38.507162
2225.302424	165048.262321	38.512180
2227.970465	165338.821834	38.517197
2229.918002	165644.908179	38.522215
2232.336539	165953.068311	38.527232
2234.633131	166247.752405	38.532250
2237.181239	166548.696131	38.537268
2239.746727	166850.425662	38.542285
2241.960229	167142.295173	38.547303
2243.893006	167449.636147	38.552320
2246.507643	167739.350769	38.557338
2249.037408	168045.712677	38.562356
2251.508110	168332.671532	38.567373
2253.839206	168613.761888	38.572391
2257.070450	168900.693556	38.577408
2261.095867	169141.983835	38.582426
2263.426361	169394.216960	38.587444
2265.877841	169644.692630	38.592461
2268.385256	169903.223172	38.597479
2270.499812	170160.838086	38.602496
2273.023093	170401.172795	38.607514
2275.419609	170635.890411	38.612532
2277.752899	170886.337938	38.617549
2280.115206	171115.589841	38.622567
2281.749396	171368.725363	38.627584
2284.336734	171604.571810	38.632602
2286.297122	171848.896930	38.637620
2288.533385	172100.646072	38.642637
2290.467714	172350.005099	38.647655
2292.087185	172601.597938	38.652672
2293.978526	172863.866139	38.657690
2296.303897	173131.032500	38.662708
2298.269302	173397.163796	38.667725
2300.819531	173658.760753	38.672743
2302.462387	173932.575463	38.677760
2304.873814	174214.804509	38.682778
2306.830389	174475.836285	38.687796
2308.996558	174760.048231	38.692813
2311.261250	175034.239802	38.697831
2313.781022	175309.916382	38.702848
2315.863289	175574.678115	38.707866
2318.093897	175833.665359	38.712884
2320.084980	176090.874859	38.717901
2321.981196	176348.277706	38.722919
2324.254962	176626.701751	38.727936
2326.696788	176884.605479	38.732954
2328.714114	177163.960117	38.737972
2330.723421	177439.482014	38.742989
2333.290367	177713.952948	38.748007
2335.221652	178013.158771	38.753024
2337.772262	178291.850014	38.758042
2339.894157	178597.783840	38.763060
2341.907828	178889.055984	38.768077
2344.347233	179181.685099	38.773095
2346.313055	179496.891010	38.778112
2348.794570	179797.185648	38.783130
2350.905724	180122.250806	38.788148
2353.143771	180432.541341	38.793165
2355.731118	180746.461265	38.798183
2357.815266	181082.404350	38.803200
2360.110736	181404.423099	38.808218
2363.272469	181736.924551	38.813236
2365.045778	182061.769849	38.818253
2367.758027	182392.895909	38.823271
2369.776985	182725.273955	38.828288
2372.331107	183054.141098	38.833306
2374.688925	183388.627595	38.838324
2377.298502	183730.543261	38.843341
2379.902921	184066.390653	38.848359
2382.472892	184404.530450	38.853376
2384.750206	184739.211913	38.858394
2387.397008	185065.836338	38.863412
2390.001509	185399.199153	38.868429
2392.928900	185723.343744	38.873447
2395.051758	186093.536300	38.878464
2397.107978	186462.826187	38.883482
2399.895051	186800.229043	38.888500
2402.549323	187129.652831	38.893517
2405.022768	187466.598650	38.898535
2407.075026	187805.058861	38.903552
2409.650811	188144.429254	38.908570
2412.208262	188483.295569	38.913588
2414.490122	188812.198288	38.918605
2417.288253	189154.839198	38.923623
2419.541752	189480.827327	38.928640
2422.462482	189807.068166	38.933658
2424.747964	190134.170810	38.938676
2427.232740	190464.621603	38.943693
2430.008445	190782.327927	38.948711
2432.543064	191118.030686	38.953728
2435.342598	191441.932781	38.958746
2437.919995	191764.981313	38.963764
2440.191409	192104.131490	38.968781
2443.004439	192417.721496	38.973799
2445.035235	192741.899129	38.978816
2447.506848	193058.490388	38.983834
2450.317607	193393.292866	38.988852
2452.318698	193702.541938	38.993869
2454.565200	194026.028906	38.998887
2457.258311	194355.518031	39.003904
2459.626958	194679.114635	39.008922
2461.764797	195004.399032	39.013940
2464.366872	195340.305890	39.018957
2466.883335	195664.720140	39.023975
2469.211527	195991.501390	39.028992
2471.554130	196309.441494	39.034010
2474.037181	196628.097115	39.039028
2476.210764	196960.188217	39.044045
2478.875351	197263.296708	39.049063
2481.266686	197561.114027	39.054080
2484.089789	197860.084048	39.059098
2486.318745	198158.766119	39.064116
2488.248506	198471.948966	39.069133
2490.614720	198773.455914	39.074151
2492.598033	199097.452909	39.079168
2495.293228	199421.238199	39.084186
2497.850067	199731.557246	39.089204
2500.284891	200057.238726	39.094221
2502.521719	200389.073591	39.099239
2505.078823	200725.050654	39.104256
2507.348045	201054.595654	39.109274
2510.101708	201395.293714	39.114292
2512.013817	201739.933779	39.119309
2514.432868	202083.657375	39.124327
2517.048039	202437.258073	39.129344
2519.510464	202785.345525	39.134362
2521.836581	203146.156124	39.139380
2524.749941	203508.425613	39.144397
2527.106022	203863.161766	39.149415
2529.631565	204230.852977	39.154432
2531.989137	204602.660878	39.159450
2534.298651	204958.854288	39.164468
2536.826898	205346.462965	39.169485
2539.584588	205710.285032	39.174503
2541.904107	206102.982815	39.179520
2544.150295	206482.076782	39.184538
2547.049231	206858.275520	39.189556
2549.743586	207247.665520	39.194573
2552.530049	207633.180610	39.199591
2555.279585	208024.163779	39.204608
2558.619889	208394.174284	39.209626
2562.161684	208743.526626	39.214644
2564.317041	209118.422260	39.219661
2567.230968	209468.711668	39.224679
2570.210298	209829.559164	39.229696
2572.815945	210194.199615	39.234714
2575.512424	210550.595747	39.239732
2578.021693	210913.982022	39.244749
2580.601663	211281.650958	39.249767
2583.063217	211643.521409	39.254784
2585.670473	212005.293430	39.259802
2588.684532	212366.596131	39.264820
2590.931834	212725.503633	39.269837
2593.541592	213072.085207	39.274855
2595.789956	213443.720561	39.279872
2598.539322	213808.546399	39.284890
2601.175404	214174.635039	39.289908
2603.608856	214543.829443	39.294925
2606.422701	214913.422294	39.299943
2608.920479	215284.131655	39.304960
2611.322557	215656.456702	39.309978
2614.644581	216019.874619	39.314996
2617.014301	216396.371599	39.320013
2619.536454	216766.290992	39.325031
2622.015951	217128.824803	39.330048
2624.476744	217501.955224	39.335066
2627.673569	217867.401024	39.340084
2630.242234	218236.475984	39.345101
2633.004427	218604.377903	39.350119
2635.697702	218952.399493	39.355136
2638.819502	219310.465377	39.360154
2641.570045	219663.762486	39.365172
2643.917991	220022.050810	39.370189
2646.429797	220384.759517	39.375207
2648.860579	220737.903695	39.380224
2651.300736	221095.771718	39.385242
2654.172225	221432.106352	39.390260
2656.703952	221772.584034	39.395277
2659.216051	222115.097209	39.400295
2661.415313	222439.952544	39.405312
2664.317732	222786.698464	39.410330
2666.401690	223125.493347	39.415348
2668.586277	223475.526654	39.420365
2671.237268	223821.524412	39.425383
2673.758355	224181.997372	39.430400
2676.288013	224539.268134	39.435418
2679.173276	224901.691437	39.440436
2681.470866	225275.765087	39.445453
2684.315515	225628.515797	39.450471
2686.898070	226007.752966	39.455488
2689.461729	226385.824480	39.460506
2691.742623	226767.521956	39.465524
2694.680356	227165.096356	39.470541
2697.060847	227562.808229	39.475559
2700.098218	227955.540228	39.480576
2702.384002	228358.068061	39.485594
2705.596005	228739.950569	39.490612
2708.052715	229171.971115	39.495629
2710.287253	229561.829946	39.500647
2713.091469	229981.551354	39.505664
2716.145491	230395.263760	39.510682
2718.961664	230812.925208	39.515700
2721.278398	231228.606440	39.520717
2724.105148	231646.951705	39.525735
2726.810516	232068.745147	39.530752
2729.352633	232496.177997	39.535770
2732.434057	232919.792242	39.540788
2735.216229	233353.893756	39.545805
2737.757023	233789.404296	39.550823
2740.594231	234216.815309	39.555840
2743.650142	234657.986204	39.560858
2746.625207	235089.185554	39.565876
2749.289113	235522.541420	39.570893
2752.242981	235957.274327	39.575911
2755.004059	236390.766579	39.580928
2757.714576	236830.032857	39.585946
2760.792775	237249.731361	39.590964
2763.548064	237697.652283	39.595981
2766.082848	238132.930526	39.600999
2769.323081	238568.047608	39.606016
2771.619007	238997.087180	39.611034
2774.890343	239438.726933	39.616052
2777.586127	239888.940365	39.621069
2780.659138	240310.972782	39.626087
2783.861978	240741.545311	39.631104
2786.381135	241170.445320	39.636122
2789.395233	241598.657935	39.641140
2792.356629	242034.321204	39.646157
2795.308806	242452.939581	39.651175
2798.808462	242878.661149	39.656192
2801.621655	243315.132705	39.661210
2804.641173	243732.112561	39.666228
2806.895262	244148.499484	39.671245
2809.924729	244554.425941	39.676263
2812.595683	244978.062489	39.681280
2815.213064	245403.052885	39.686298
2818.539505	245814.925810	39.691316
2820.947772	246238.295841	39.696333
2823.823744	246659.204333	39.701351
2826.729239	247074.086888	39.706368
2829.000706	247503.978561	39.711386
2831.899325	247908.470686	39.716404
2835.081898	248338.752103	39.721421
2837.633451	248753.685999	39.726439
2840.797051	249137.050102	39.731456
2843.634625	249517.314209	39.736474
2846.465883	249892.066161	39.741492
2849.161428	250284.899394	39.746509
2851.989139	250668.642557	39.751527
2854.417196	251059.356393	39.756544
2857.187125	251454.664659	39.761562
2859.649483	251855.023998	39.766580
2862.252884	252258.052970	39.771597
2864.755879	252674.483293	39.776615
2867.479440	253089.912883	39.781632
2869.727567	253517.989153	39.786650
2872.617074	253946.269189	39.791668
2875.523887	254380.819453	39.796685
2877.847484	254834.357857	39.801703
2880.488260	255276.846634	39.806720
2883.160041	255732.918876	39.811738
2885.933179	256179.930983	39.816756
2889.246283	256653.020753	39.821773
2892.098324	257110.812945	39.826791
2895.481663	257578.198616	39.831808
2898.267567	258052.991008	39.836826
2901.069510	258517.491811	39.841844
2904.117361	258991.173062	39.846861
2907.291863	259472.097345	39.851879
2910.368847	259939.801247	39.856896
2913.568894	260408.906590	39.861914
2916.804536	260870.308244	39.866932
2920.151892	261340.199743	39.871949
2923.515902	261798.605894	39.876967
2926.960534	262234.798071	39.881984
2929.730893	262704.265708	39.887002
2933.341949	263155.134900	39.892020
2936.352341	263599.694989	39.897037
2939.349179	264053.221400	39.902055
2942.256860	264494.999814	39.907072
2945.148866	264946.506763	39.912090
2948.052010	265410.557241	39.917108
2950.920026	265868.540708	39.922125
2953.302274	266327.334280	39.927143
2956.491725	266789.530592	39.932160
2959.122151	267253.157886	39.937178
2962.218285	267712.875330	39.942196
2965.256491	268183.470184	39.947213
2968.111080	268650.586333	39.952231
2971.194208	269115.759757	39.957248
2974.146567	269595.936135	39.962266
2977.139470	270061.118905	39.967284
2980.117100	270537.832342	39.972301
2982.978649	271009.710382	39.977319
2986.244034	271474.741948	39.982336
2989.138231	271954.457805	39.987354
2992.376527	272423.501423	39.992372
2995.242107	272890.289381	39.997389
2998.448432	273376.577540	40.002407
3001.485339	273830.939975	40.007424
3004.898295	274302.841436	40.012442
3007.763269	274767.739859	40.017460
3011.040409	275231.809654	40.022477
3013.805674	275702.610340	40.027495
3016.461934	276159.584343	40.032512
3019.582109	276632.991020	40.037530
3022.778752	277104.706874	40.042548
3025.861314	277567.549164	40.047565
3028.814143	278031.094605	40.052583
3031.779439	278487.169087	40.057600
3034.911232	278962.159879	40.062618
3037.988915	279410.821369	40.067636
3040.826605	279845.270955	40.072653
3043.459278	280279.800734	40.077671
3046.276446	280711.150335	40.082688
3049.057807	281155.987523	40.087706
3052.109639	281598.596016	40.092724
3055.305972	282039.858839	40.097741
3057.826813	282496.892260	40.102759
3060.748151	282935.779963	40.107776
3063.496327	283400.492004	40.112794
3066.668108	283867.776013	40.117812
3069.726118	284343.759175	40.122829
3072.167922	284817.625761	40.127847
3075.215138	285290.176019	40.132864
3078.127669	285775.008758	40.137882
3081.204224	286264.662528	40.142900
3084.476179	286758.091218	40.147917
3087.043470	287256.805965	40.152935
3090.602195	287751.249153	40.157952
3093.724282	288267.542884	40.162970
3096.300324	288775.944490	40.167988
3100.038966	289288.020706	40.173005
3102.958608	289791.536439	40.178023
3106.692899	290296.927324	40.183040
3109.321531	290810.865242	40.188058
3112.235617	291324.906873	40.193076
3115.790973	291831.354258	40.198093
3119.133079	292363.804979	40.203111
3123.425734	292847.227185	40.208128
3127.766491	293342.393592	40.213146
3131.105002	293826.819713	40.218164
3134.580802	294304.466944	40.223181
3137.677013	294805.273672	40.228199
3140.865268	295290.701438	40.233216
3144.163986	295777.809050	40.238234
3147.172053	296252.695095	40.243252
3150.405559	296724.419380	40.248269
3153.303702	297228.130388	40.253287
3156.603526	297702.146627	40.258304
3159.613756	298193.086859	40.263322
3162.721289	298686.825690	40.268340
3165.951987	299170.766863	40.273357
3169.015566	299680.472377	40.278375
3172.239235	300177.810239	40.283392
3174.613150	300680.556247	40.288410
3177.628483	301182.715458	40.293428
3180.799246	301694.010232	40.298445
3183.765819	302218.253357	40.303463
3188.020102	302694.286583	40.308480
3191.603707	303210.452789	40.313498
3194.766902	303702.563396	40.318516
3198.034455	304193.840813	40.323533
3200.963037	304700.701799	40.328551
3204.156368	305208.481222	40.333568
3207.180027	305708.819057	40.338586
3210.064387	306215.722729	40.343604
3213.179511	306724.590736	40.348621
3216.313694	307248.477649	40.353639
3219.590652	307746.014471	40.358656
3222.733480	308264.990400	40.363674
3225.853396	308787.289574	40.368692
3229.047648	309306.221146	40.373709
3232.058899	309832.155764	40.378727
3235.371836	310355.651835	40.383744
3238.263003	310883.700392	40.388762
3241.640317	311404.738378	40.393780
3245.227792	311917.742930	40.398797
3248.401648	312445.933210	40.403815
3251.735595	312939.270636	40.408832
3255.871046	313420.219484	40.413850
3258.593533	313891.434285	40.418868
3262.131741	314367.060313	40.423885
3264.853419	314849.635552	40.428903
3268.192618	315326.069363	40.433920
3270.938257	315809.595126	40.438938
3274.132700	316292.233766	40.443956
3277.088254	316777.899050	40.448973
3279.806331	317292.450884	40.453991
3283.116120	317796.905851	40.459008
3286.544497	318306.082203	40.464026
3289.135137	318830.507829	40.469044
3292.562653	319345.965791	40.474061
3295.684454	319882.400893	40.479079
3298.624824	320420.836927	40.484096
3302.060474	320945.587651	40.489114
3305.036540	321491.109964	40.494132
3308.275729	322044.552178	40.499149
3311.665445	322601.490846	40.504167
3315.022294	323158.173506	40.509184
3318.065286	323714.643854	40.514202
3321.344036	324292.917019	40.519220
3324.513782	324856.177903	40.524237
3328.151568	325435.140378	40.529255
3331.559528	326016.312478	40.534272
3334.982483	326594.581464	40.539290
3338.274097	327179.890687	40.544308
3341.801132	327757.289500	40.549325
3345.649718	328346.808188	40.554343
3349.357130	328922.157692	40.559360
3352.800435	329503.857196	40.564378
3356.188606	330082.842039	40.569396
3360.678909	330635.388943	40.574413
3364.160207	331204.143909	40.579431
3367.683201	331770.550043	40.584448
3370.916661	332338.413530	40.589466
3374.626664	332913.018518	40.594484
3378.290864	333475.825811	40.599501
3381.582475	334035.638581	40.604519
3384.656234	334606.638513	40.609536
3388.299901	335180.432864	40.614554
3391.125684	335748.993308	40.619572
3394.740427	336327.796976	40.624589
3398.094525	336907.646727	40.629607
3401.857823	337485.470492	40.634624
3405.289546	338056.513532	40.639642
3408.655614	338638.895712	40.644660
3412.472110	339198.624363	40.649677
3415.518388	339778.577531	40.654695
3419.170104	340351.350711	40.659712
3423.127891	340902.178869	40.664730
3426.946339	341484.672474	40.669748
3430.089662	342035.482843	40.674765
3433.287277	342603.141588	40.679783
3437.070736	343163.750936	40.684800
3440.808425	343730.749259	40.689818
3444.018819	344288.868088	40.694836
3447.316965	344840.446665	40.699853
3450.969724	345410.575083	40.704871
3454.424177	345973.573516	40.709888
3458.129774	346531.426392	40.714906
3461.127541	347088.847646	40.719924
3464.767017	347645.145457	40.724941
3468.205533	348212.647904	40.729959
3471.868050	348765.779071	40.734976
3475.439096	349328.753578	40.739994
3478.665964	349901.204503	40.745012
3481.884996	350439.580405	40.750016
3484.920111	350955.498176	40.755021
3487.930912	351424.130695	40.760026
3491.530048	351855.196574	40.765031
3494.069551	352239.319868	40.770036
3496.618357	352576.971380	40.775040
3499.134540	352868.209928	40.780045
3501.673962	353130.490576	40.785050
3503.516321	353320.562490	40.790055
3505.418104	353492.195842	40.795060
3507.143919	353615.154631	40.800064
3508.778435	353725.214809	40.805069
3510.357149	353781.931048	40.810074
3511.402834	353813.617227	40.815079
3512.616032	353820.164408	40.820084
3513.631320	353788.717158	40.825088
3514.449456	353748.302592	40.830093
3514.828665	353688.409820	40.835098
3515.829825	353595.325800	40.840103
3516.334934	353499.243101	40.845108
3517.105706	353386.851084	40.850112
3517.196581	353248.078533	40.855117
3517.577565	353111.319132	40.860122
3518.142562	352955.695327	40.865127
3518.050171	352797.631190	40.870132
3518.473840	352627.005304	40.875136
3518.492073	352448.460034	40.880141
3518.370796	352264.368686	40.885146
3518.911637	352065.404632	40.890151
3518.676741	351878.100504	40.895156
3518.573810	351680.886524	40.900160
3518.690931	351473.037051	40.905165
3518.452100	351265.673774	40.910170
3518.329307	351054.935660	40.915175
3518.115185	350859.259190	40.920180
3518.011019	350645.312570	40.925184
3517.669080	350443.400065	40.930189
3517.510282	350225.239374	40.935194
3517.430749	350020.512561	40.940199
3516.877077	349820.459464	40.945204
3516.439427	349621.429364	40.950208
3516.556230	349422.947312	40.955213
3515.978015	349235.325523	40.960218
3515.938948	349029.976127	40.965223
3515.615750	348838.600833	40.970228
3515.799035	348646.815131	40.975232
3515.667704	348461.890405	40.980237
3515.340573	348279.257699	40.985242
3515.382017	348076.991384	40.990247
3514.852637	347900.819941	40.995252
3514.812343	347708.402632	41.000256
3514.649810	347523.909737	41.005261
3514.363162	347344.112964	41.010266
3514.223001	347153.284225	41.015271
3513.964293	346987.438478	41.020276
3513.461454	346810.570736	41.025280
3513.593795	346637.747253	41.030285
3513.074059	346475.473468	41.035290
3513.160486	346311.553726	41.040295
3512.779601	346146.536410	41.045300
3512.939852	345971.137361	41.050304
3512.899454	345819.082553	41.055309
3512.196074	345662.731840	41.060314
3512.166114	345508.131591	41.065319
3511.740362	345357.787266	41.070324
3511.492330	345207.262074	41.075328
3511.728477	345063.372991	41.080333
3511.546089	344911.615895	41.085338
3511.263158	344767.170719	41.090343
3511.058838	344624.365327	41.095348
3510.877792	344481.276041	41.100352
3510.778250	344341.021099	41.105357
3510.607057	344201.793748	41.110362
3510.209537	344071.805056	41.115367
3510.120913	343937.648870	41.120372
3510.469253	343808.534714	41.125376
3510.232341	343675.926123	41.130381
3509.477335	343548.660786	41.135386
3509.646657	343426.692285	41.140391
3509.458732	343306.965581	41.145396
3509.719746	343181.422311	41.150400
3509.554085	343059.936890	41.155405
3509.147609	342926.919572	41.160410
3508.858664	342813.716008	41.165415
3509.099061	342706.710031	41.170420
3508.746694	342592.040883	41.175424
3508.910024	342486.419253	41.180429
3508.974990	342371.531878	41.185434
3508.859673	342254.104079	41.190439
3508.339871	342146.985841	41.195444
3508.269930	342033.949082	41.200448
3508.196759	341929.989897	41.205453
3508.154182	341829.432868	41.210458
3508.168477	341724.238964	41.215463
3507.826668	341625.990932	41.220468
3507.926958	341518.138598	41.225472
3507.485430	341427.304868	41.230477
3507.272123	341334.782606	41.235482
3507.435768	341222.418856	41.240487
3507.217591	341142.254609	41.245492
3507.347910	341059.010063	41.250496
3507.620144	340957.282741	41.255501
3507.219593	340869.161958	41.260506
3507.518742	340769.464128	41.265511
3507.600836	340686.658484	41.270516
3507.361394	340583.560323	41.275520
3507.544069	340488.126295	41.280525
3507.171490	340405.161895	41.285530
3507.480387	340298.188792	41.290535
3506.642984	340212.677174	41.295540
3506.773840	340112.647694	41.300544
3506.739528	340029.604350	41.305549
3506.699897	339953.707024	41.310554
3506.811090	339867.690967	41.315559
3506.256563	339789.889996	41.320564
3506.189713	339699.476675	41.325568
3506.514959	339618.283568	41.330573
3506.314086	339548.030202	41.335578
3506.419625	339471.575259	41.340583
3506.520627	339388.483941	41.345588
3506.491464	339310.854463	41.350592
3506.621284	339230.352039	41.355597
3506.210573	339142.482856	41.360602
3506.490249	339066.889968	41.365607
3506.354050	338985.996099	41.370612
3506.159904	338910.146036	41.375616
3506.047189	338827.671549	41.380621
3505.846187	338751.567927	41.385626
3505.657062	338681.387326	41.390631
3505.594534	338611.136029	41.395636
3505.975347	338534.890553	41.400640
3505.564726	338462.557065	41.405645
3505.568212	338391.201601	41.410650
3506.111517	338318.159931	41.415655
3505.571549	338253.144435	41.420660
3505.841270	338184.366384	41.425664
3505.954678	338110.501155	41.430669
3505.917402	338035.133439	41.435674
3506.274339	337956.016898	41.440679
3505.965335	337883.819019	41.445684
3505.669291	337802.286199	41.450688
3505.636534	337743.192322	41.455693
3505.467676	337658.664082	41.460698
3505.635433	337592.189479	41.465703
3505.310268	337527.876730	41.470708
3505.504852	337460.990832	41.475712
3505.249727	337394.505384	41.480717
3505.495616	337334.986032	41.485722
3505.494434	337264.239409	41.490727
3505.593642	337197.825616	41.495732
3505.300243	337124.097982	41.500736
3505.287031	337055.590702	41.505741
3505.126320	336988.810090	41.510746
3505.526124	336919.093912	41.515751
3505.212951	336868.332611	41.520756
3505.108238	336791.675861	41.525760
3505.098986	336735.323204	41.530765
3504.938136	336668.821768	41.535770
3504.942963	336598.276370	41.540775
3504.993055	336549.797730	41.545780
3504.849312	336477.011877	41.550784
3504.827959	336418.677012	41.555789
3504.855801	336361.453361	41.560794
3504.860474	336301.690129	41.565799
3504.883138	336246.094686	41.570804
3505.115103	336184.744604	41.575808
3505.292695	336121.292101	41.580813
3504.734151	336065.507087	41.585818
3505.093593	336003.195915	41.590823
3504.905276	335942.750061	41.595828
3504.604810	335880.541372	41.600832
3504.802809	335816.423957	41.605837
3504.546183	335754.691429	41.610842
3504.868999	335702.786869	41.615847
3505.063564	335645.536165	41.620852
3504.769464	335577.578476	41.625856
3505.087660	335512.221121	41.630861
3504.525126	335461.801866	41.635866
3504.785255	335403.472461	41.640871
3504.436773	335344.779903	41.645876
3504.380636	335287.059027	41.650880
3504.723637	335222.714570	41.655885
3504.661904	335181.423280	41.660890
3504.892102	335120.987256	41.665895
3504.579094	335063.789210	41.670900
3504.322972	335010.651320	41.675904
3504.477153	334945.140470	41.680909
3504.622478	334899.086314	41.685914
3504.720561	334835.796579	41.690919
3504.557362	334787.959194	41.695924
3504.725827	334727.048932	41.700928
3504.636092	334673.681214	41.705933
3504.622402	334614.859113	41.710938
3504.645590	334552.979321	41.715943
3504.323498	334499.113437	41.720948
3504.152352	334445.351147	41.725952
3504.301443	334386.528789	41.730957
3504.564246	334348.161653	41.735962
3504.344111	334282.402705	41.740967
3503.954738	334238.287503	41.745972
3503.849737	334186.650869	41.750976
3504.419447	334139.334416	41.755981
3504.240792	334088.370353	41.760986
3504.352691	334034.105644	41.765991
3504.307309	333983.680215	41.770996
3504.010010	333933.471948	41.776000
3504.021465	333874.110690	41.781005
3504.253583	333829.033587	41.786010
3503.978297	333781.059765	41.791015
3504.043627	333732.651386	41.796020
3504.246865	333679.872485	41.801024
3504.211880	333634.836715	41.806029
3504.163350	333583.724556	41.811034
3504.190719	333529.192514	41.816039
3504.209956	333481.325077	41.821044
3504.083114	333422.747617	41.826048
3504.471702	333381.562302	41.831053
3503.989397	333321.692054	41.836058
3504.100450	333281.338242	41.841063
3504.068785	333229.663454	41.846068
3503.782559	333178.257106	41.851072
3504.189293	333133.075703	41.856077
3503.870838	333082.411801	41.861082
3504.028647	333034.954600	41.866087
3504.049379	332991.079321	41.871092
3504.051235	332940.441685	41.876096
3504.380423	332889.753045	41.881101
3504.088651	332840.712398	41.886106
3504.164251	332781.364880	41.891111
3504.024529	332738.073812	41.896116
3504.069115	332681.401469	41.901120
3504.479861	332637.795727	41.906125
3504.092558	332591.287537	41.911130
3504.273221	332539.146401	41.916135
3504.302843	332491.454135	41.921140
3503.811226	332432.753879	41.926144
3504.339833	332382.974576	41.931149
3504.084557	332336.877902	41.936154
3504.309236	332284.856738	41.941159
3503.610257	332234.149188	41.946164
3503.916660	332188.880546	41.951168
3504.278343	332139.533842	41.956173
3504.028347	332088.985136	41.961178
3503.711706	332030.333334	41.966183
3504.063967	331991.975332	41.971188
3503.835049	331935.929425	41.976192
3504.115307	331891.452951	41.981197
3503.590982	331859.767749	41.986202
3504.166404	331799.272702	41.991207
3504.064709	331756.737626	41.996212
3503.929415	331713.317540	42.001216
3504.078374	331664.359406	42.006221
3503.814143	331610.861930	42.011226
3503.977476	331569.811454	42.016231
3503.718374	331526.130646	42.021236
3503.918791	331473.756081	42.026240
3504.007967	331416.057561	42.031245
3503.715528	331385.811070	42.036250
3503.742370	331327.969513	42.041255
3503.939930	331293.526339	42.046260
3503.683373	331244.757948	42.051264
3504.103507	331185.863036	42.056269
3503.845098	331150.397010	42.061274
3504.015341	331096.398825	42.066279
3503.699037	331051.912479	42.071284
3503.321304	331014.201226	42.076288
3503.834465	330963.888369	42.081293
3503.531422	330925.173459	42.086298
3503.935486	330874.852029	42.091303
3503.951423	330829.220038	42.096308
3503.520749	330790.906373	42.101312
3503.772189	330743.838727	42.106317
3503.611614	330698.615571	42.111322
3503.690993	330648.293503	42.116327
3504.177209	330614.338938	42.121332
3503.668685	330571.128257	42.126336
3503.999627	330519.546005	42.131341
3503.578943	330473.472843	42.136346
3503.507291	330429.329235	42.141351
3502.899378	330394.629083	42.146356
3503.246820	330352.811055	42.151360
3503.715178	330310.058508	42.156365
3503.625310	330279.652456	42.161370
3503.781280	330222.781123	42.166375
3503.534640	330183.853216	42.171380
3503.614686	330141.796787	42.176384
3503.463312	330093.010582	42.181389
3503.531437	330057.340134	42.186394
3503.625251	330011.313538	42.191399
3503.366619	329977.169105	42.196404
3503.684980	329939.399359	42.201408
3503.720827	329885.369538	42.206413
3503.467322	329852.317914	42.211418
3503.497007	329798.390674	42.216423
3503.552440	329768.902720	42.221428
3503.296999	329719.648972	42.226432
3503.842689	329683.700386	42.231437
3503.451321	329650.568304	42.236442
3503.595051	329600.718146	42.241447
3503.503319	329558.331725	42.246452
3503.231229	329511.827338	42.251456
3502.943709	329476.109962	42.256461
3503.434569	329438.974215	42.261466
3503.465180	329393.668926	42.266471
3503.214753	329357.080860	42.271476
3503.382268	329318.138516	42.276480
3503.821812	329273.659700	42.281485
3503.529825	329240.766164	42.286490
3503.504321	329185.498579	42.291495
3503.522461	329158.152571	42.296500
3503.288432	329108.843854	42.301504
3503.457601	329066.594355	42.306509
3503.445295	329031.189849	42.311514
3503.460899	328980.112489	42.316519
3503.378889	328949.704184	42.321524
3503.712645	328907.327159	42.326528
3503.484648	328866.029506	42.331533
3503.187978	328836.392159	42.336538
3503.356649	328786.409911	42.341543
3503.120919	328746.614059	42.346548
3503.451472	328702.787461	42.351552
3503.579942	328659.017699	42.356557
3503.486644	328627.618896	42.361562
3503.460671	328584.636167	42.366567
3503.661446	328540.269991	42.371572
3503.336711	328503.921623	42.376576
3503.615717	328466.309207	42.381581
3503.226776	328427.452578	42.386586
3503.504317	328384.040858	42.391591
3503.411966	328343.764437	42.396596
3503.233925	328295.946734	42.401600
3503.091942	328262.418570	42.406605
3503.269049	328226.983871	42.411610
3503.638339	328185.109273	42.416615
3503.554285	328143.076249	42.421620
3503.236731	328115.934379	42.426624
3503.094998	328069.687810	42.431629
3503.322350	328035.008215	42.436634
3503.470184	327992.659147	42.441639
3503.263781	327951.815039	42.446644
3503.331031	327910.038026	42.451648
3503.502274	327874.985475	42.456653
3503.693585	327838.200083	42.461658
3503.514596	327785.294598	42.466663
3503.451067	327748.472470	42.471668
3503.321760	327707.921354	42.476672
3503.625505	327662.724206	42.481677
3503.502219	327622.350123	42.486682
3503.329455	327583.179227	42.491687
3503.316279	327539.913575	42.496692
3503.355531	327494.782832	42.501696
3503.491131	327457.700518	42.506701
3503.094763	327419.734351	42.511706
3503.423076	327385.623530	42.516711
3503.282392	327360.844688	42.521716
3503.308418	327320.345320	42.526720
3503.162933	327284.222315	42.531725
3503.235153	327245.598015	42.536730
3503.499708	327197.608376	42.541735
3503.313454	327153.122828	42.546740
3503.635185	327122.573990	42.551744
3503.140714	327085.309572	42.556749
3503.231113	327041.747458	42.561754
3503.314815	327004.596491	42.566759
3503.667674	326957.177878	42.571764
3503.391754	326920.082795	42.576768
3503.277595	326871.057901	42.581773
3503.112093	326836.565589	42.586778
3503.407288	326799.737644	42.591783
3503.387359	326767.359348	42.596788
3503.373602	326728.747932	42.601792
3503.326262	326683.985876	42.606797
3503.357766	326659.586805	42.611802
3503.360506	326615.910686	42.616807
3503.137761	326577.204460	42.621812
3503.367251	326535.629708	42.626816
3503.531120	326490.885447	42.631821
3503.140234	326461.159249	42.636826
3503.336696	326416.689646	42.641831
3503.254834	326390.349368	42.646836
3503.138663	326339.238268	42.651840
3503.455350	326300.447834	42.656845
3503.456693	326265.674697	42.661850
3503.427433	326224.903019	42.666855
3503.213530	326185.966104	42.671860
3503.148308	326146.420949	42.676864
3503.070219	326102.934919	42.681869
3502.894767	326076.125685	42.686874
3503.125237	326041.316700	42.691879
3503.177328	326010.656357	42.696884
3503.326139	325976.826658	42.701888
3503.271748	325936.567357	42.706893
3502.982019	325902.653212	42.711898
3502.771105	325865.597923	42.716903
3502.941577	325827.720115	42.721908
3502.490261	325789.684652	42.726912
3503.173015	325754.525225	42.731917
3502.893054	325722.898821	42.736922
3503.075704	325684.230410	42.741927
3503.103824	325657.872543	42.746932
3502.906217	325636.968072	42.751936
3503.151476	325588.292705	42.756941
3502.825795	325557.334675	42.761946
3502.983901	325512.768301	42.766951
3502.873632	325480.403038	42.771956
3502.580779	325456.231785	42.776960
3502.776278	325425.904819	42.781965
3502.497985	325397.050656	42.786970
3502.671271	325371.000709	42.791975
3502.820851	325342.614125	42.796980
3503.062543	325305.437020	42.801985
3502.900483	325271.044596	42.806989
3502.944528	325238.146364	42.811994
3502.966984	325196.933161	42.816999
3503.042503	325163.928219	42.822004
3503.300473	325129.979080	42.827009
3503.357645	325087.412136	42.832013
3502.851488	325045.594206	42.837018
3503.150086	325017.667537	42.842023
3502.997206	324989.353214	42.847028
3502.824978	324951.731432	42.852033
3502.715417	324919.696314	42.857037
3502.813043	324895.718351	42.862042
3502.702098	324844.630005	42.867047
3502.798567	324822.967079	42.872052
3502.614010	324795.166321	42.877057
3503.031060	324761.624578	42.882061
3502.917796	324728.267086	42.887066
3502.656163	324690.531784	42.892071
3502.829682	324653.542768	42.897076
3502.448574	324641.798792	42.902081
3502.852824	324605.053652	42.907085
3502.708525	324577.907886	42.912090
3502.795841	324544.875173	42.917095
3502.666729	324512.664711	42.922100
3502.503469	324485.038500	42.927105
3502.780962	324453.934899	42.932109
3502.629013	324429.868309	42.937114
3502.652962	324397.888326	42.942119
3502.602905	324373.398828	42.947124
3502.647614	324333.936572	42.952129
3502.692157	324308.770906	42.957133
3502.819371	324273.620348	42.962138
3502.604804	324243.000180	42.967143
3502.641065	324225.670911	42.972148
3502.308889	324197.231312	42.977153
3502.370895	324156.341619	42.982157
3502.681430	324148.178512	42.987162
3502.506532	324115.898549	42.992167
3502.869796	324093.048974	42.997172
3502.876558	324050.056343	43.002177
3502.687105	324029.429614	43.007181
3502.677774	323998.548377	43.012186
3503.025392	323958.987750	43.017191
3502.791817	323926.233429	43.022196
3502.722779	323899.558848	43.027201
3502.980864	323860.139255	43.032205
3502.526887	323831.794676	43.037210
3502.641987	323797.307016	43.042215
3502.866467	323769.238404	43.047220
3502.726856	323739.700082	43.052225
3502.977432	323703.079814	43.057229
3502.519347	323666.366277	43.062234
3502.911904	323638.169665	43.067239
3502.809535	323603.970078	43.072244
3502.994648	323576.085537	43.077249
3503.084660	323528.932817	43.082253
3502.899818	323506.066455	43.087258
3502.883695	323477.424545	43.092263
3502.496131	323451.536983	43.097268
3502.483298	323415.440799	43.102273
3502.579355	323385.000616	43.107277
3502.602319	323368.080088	43.112282
3502.734544	323328.145351	43.117287
3502.483578	323301.371501	43.122292
3502.304784	323276.011010	43.127297
3502.758050	323238.112262	43.132301
3502.519862	323218.077821	43.137306
3502.689207	323192.052558	43.142311
3502.881599	323155.720698	43.147316
3503.008108	323126.344047	43.152321
3503.266285	323092.851121	43.157325
3502.936055	323063.138467	43.162330
3502.863458	323024.380093	43.167335
3502.725870	322999.521813	43.172340
3502.546372	322965.969696	43.177345
3502.775841	322934.032927	43.182349
3502.534876	322907.333587	43.187354
3502.799004	322875.900173	43.192359
3503.057373	322850.751233	43.197364
3502.791049	322819.781918	43.202369
3502.939963	322783.125785	43.207373
3502.804109	322746.946410	43.212378
3502.623526	322712.071392	43.217383
3502.089055	322691.981047	43.222388
3502.472061	322661.063209	43.227393
3502.708392	322633.729746	43.232397
3502.442604	322610.417575	43.237402
3503.115709	322579.708932	43.242407
3503.060800	322549.215316	43.247412
3503.115075	322515.931739	43.252417
3502.814322	322481.380509	43.257421
3502.615634	322447.805524	43.262426
3502.671014	322417.549049	43.267431
3502.909787	322387.950892	43.272436
3502.649469	322353.698544	43.277441
3502.690872	322318.228977	43.282445
3502.863021	322298.817124	43.287450
3502.785050	322263.824007	43.292455
3502.969869	322239.144069	43.297460
3502.609096	322196.333928	43.302465
3503.096720	322163.033520	43.307469
3502.717947	322142.257240	43.312474
3502.989456	322102.172465	43.317479
3502.744171	322071.021244	43.322484
3502.710403	322046.248007	43.327489
3502.611643	322006.576922	43.332493
3502.464520	321987.697973	43.337498
3502.755405	321960.355586	43.342503
3502.584976	321922.629032	43.347508
3502.566527	321907.367978	43.352513
3502.793277	321859.047297	43.357517
3502.794237	321835.515106	43.362522
3502.366135	321794.699380	43.367527
3502.595938	321765.585551	43.372532
3502.580598	321739.740773	43.377537
3502.692260	321719.981903	43.382541
3502.827630	321688.593084	43.387546
3502.962455	321653.057542	43.392551
3503.055600	321614.475605	43.397556
3502.626394	321579.358497	43.402561
3502.897526	321549.627518	43.407565
3502.933080	321520.620071	43.412570
3503.031858	321489.974573	43.417575
3502.898261	321456.261471	43.422580
3502.407291	321421.611774	43.427585
3502.784056	321390.083408	43.432589
3502.804291	321365.530336	43.437594
3502.646826	321335.916785	43.442599
3502.839699	321301.236896	43.447604
3502.685212	321274.395865	43.452609
3502.601720	321241.717862	43.457613
3502.755222	321217.703661	43.462618
3502.689672	321181.435687	43.467623
3502.574981	321150.059943	43.472628
3502.683458	321118.344161	43.477633
3502.575426	321083.252987	43.482637
3502.380880	321068.451527	43.487642
3502.596567	321040.509675	43.492647
3502.755063	321010.872171	43.497652
3502.756504	320980.266896	43.502657
3502.737241	320943.940636	43.507661
3502.431651	320920.811815	43.512666
3502.315912	320884.551400	43.517671
3502.738105	320859.045057	43.522676
3502.160270	320837.535890	43.527681
3502.542064	320814.274605	43.532685
3502.189865	320793.595295	43.537690
3502.553130	320762.882678	43.542695
3502.583790	320733.188553	43.547700
3502.260509	320703.549485	43.552705
3502.671784	320685.041003	43.557709
3502.510978	320651.636792	43.562714
3502.614000	320622.974411	43.567719
3502.497552	320600.350246	43.572724
3502.452963	320575.399752	43.577729
3502.666234	320540.945044	43.582733
3502.422255	320514.168344	43.587738
3502.428511	320489.642387	43.592743
3502.948993	320456.081125	43.597748
3502.504687	320433.711420	43.602753
3502.756738	320405.483644	43.607757
3502.662035	320374.282311	43.612762
3502.639876	320342.001137	43.617767
3502.505808	320305.743085	43.622772
3502.539339	320280.780264	43.627777
3502.503963	320243.514595	43.632781
3502.421527	320220.070817	43.637786
3502.717594	320191.963259	43.642791
3502.731399	320173.287437	43.647796
3502.318815	320145.951596	43.652801
3502.725547	320107.726567	43.657805
3502.542737	320076.436964	43.662810
3502.555157	320046.567115	43.667815
3502.659112	320025.638362	43.672820
3502.227034	319998.890614	43.677825
3502.327241	319974.985778	43.682829
3502.384351	319941.267252	43.687834
3502.272391	319920.143074	43.692839
3502.224082	319875.577411	43.697844
3502.288749	319869.512502	43.702849
3502.585630	319837.155863	43.707853
3502.194799	319814.319568	43.712858
3502.706959	319786.050912	43.717863
3502.966182	319762.680928	43.722868
3502.551769	319731.147258	43.727873
3502.818731	319693.172588	43.732877
3502.371611	319675.560499	43.737882
3502.359574	319636.128142	43.742887
3502.519609	319612.137472	43.747892
3502.543348	319590.177886	43.752897
3502.331184	319556.500963	43.757901
3502.478367	319534.649347	43.762906
3502.247243	319509.218432	43.767911
3502.415156	319495.657554	43.772916
3502.447182	319464.105103	43.777921
3502.552665	319426.155328	43.782925
3502.340910	319409.117105	43.787930
3502.306638	319377.498583	43.792935
3502.526235	319353.956454	43.797940
3502.761133	319336.467071	43.802945
3502.641698	319305.853978	43.807949
3502.373061	319276.027336	43.812954
3502.173233	319250.845818	43.817959
3502.438143	319210.861143	43.822964
3502.282068	319195.925845	43.827969
3502.646592	319171.419716	43.832973
3502.383510	319149.682634	43.837978
3502.614977	319122.474903	43.842983
3503.053014	319089.714115	43.847988
3502.282575	319065.028355	43.852993
3502.270969	319029.971393	43.857997
3502.177234	319005.561925	43.863002
3502.386689	318987.465755	43.868007
3502.452448	318953.032742	43.873012
3502.124520	318934.435009	43.878017
3502.496622	318893.899082	43.883021
3502.546028	318885.190440	43.888026
3502.430255	318852.490213	43.893031
3502.583588	318827.940430	43.898036
3502.235119	318808.531694	43.903041
3502.378660	318781.744506	43.908045
3502.499734	318759.743914	43.913050
3502.364187	318725.571027	43.918055
3502.634448	318699.323797	43.923060
3502.425953	318679.257168	43.928065
3502.490480	318644.671452	43.933069
3502.200061	318612.150875	43.938074
3502.494206	318587.884353	43.943079
3502.463217	318558.427315	43.948084
3502.202995	318538.826630	43.953089
3502.775023	318505.154078	43.958093
3502.157315	318484.845732	43.963098
3502.290226	318466.226971	43.968103
3502.343965	318430.523305	43.973108
3502.363451	318407.469769	43.978113
3502.237245	318386.906797	43.983117
3502.068872	318368.640187	43.988122
3502.342970	318333.843519	43.993127
3502.289422	318317.212772	43.998132
3502.443667	318298.692390	44.003137
3502.418379	318263.942255	44.008141
3502.119724	318240.912696	44.013146
3502.446021	318213.435221	44.018151
3502.665143	318189.968869	44.023156
3502.803312	318161.706479	44.028161
3502.767390	318125.533112	44.033165
3502.523753	318114.656424	44.038170
3502.297488	318084.746050	44.043175
3502.694292	318054.153520	44.048180
3502.540599	318029.218547	44.053185
3502.533884	318000.088111	44.058189
3502.286716	317974.455262	44.063194
3502.118317	317944.891983	44.068199
3502.636378	317916.163240	44.073204
3502.243091	317894.751109	44.078209
3502.542358	317861.985561	44.083213
3502.314714	317845.305400	44.088218
3502.174943	317813.473185	44.093223
3502.581550	317787.713049	44.098228
3502.483668	317771.597849	44.103233
3502.209143	317730.856165	44.108237
3501.961651	317710.235423	44.113242
3502.342710	317677.965866	44.118247
3502.443704	317666.450256	44.123252
3502.037549	317637.610724	44.128257
3502.491137	317618.254751	44.133261
3502.530219	317585.682144	44.138266
3502.315575	317550.859144	44.143271
3502.580397	317531.125423	44.148276
3502.285293	317507.102659	44.153281
3502.468912	317475.219878	44.158285
3501.978906	317459.598112	44.163290
3502.289676	317436.117100	44.168295
3502.257648	317409.610831	44.173300
3502.056981	317380.001312	44.178305
3502.077017	317365.445074	44.183309
3502.216345	317343.593595	44.188314
3501.978839	317325.693513	44.193319
3502.110506	317301.705999	44.198324
3502.000641	317278.137702	44.203329
3502.323065	317251.423523	44.208333
3502.189705	317238.188706	44.213338
3501.879201	317214.422611	44.218343
3502.376569	317188.673448	44.223348
3502.034792	317172.468768	44.228353
3502.013624	317154.789383	44.233357
3502.049997	317125.015593	44.238362
3502.008529	317117.389352	44.243367
3502.457632	317076.458134	44.248372
3502.018384	317058.818326	44.253377
3502.302382	317030.405309	44.258381
3502.182790	317013.199159	44.263386
3502.184635	316994.880052	44.268391
3502.525259	316962.310951	44.273396
3502.522459	316944.552295	44.278401
3502.301185	316919.500000	44.283405
3502.240595	316892.514448	44.288410
3502.313717	316862.556662	44.293415
3502.536808	316839.877720	44.298420
3502.102735	316819.743578	44.303425
3501.977560	316791.012433	44.308429
3502.322097	316772.436361	44.313434
3502.021484	316755.945249	44.318439
3502.505383	316729.205632	44.323444
3501.858742	316713.531649	44.328449
3501.650257	316695.194262	44.333453
3501.875522	316670.784752	44.338458
3501.921353	316649.151029	44.343463
3502.570708	316619.663165	44.348468
3502.294695	316613.320060	44.353473
3502.144338	316576.476273	44.358477
3502.357526	316555.274442	44.363482
3502.063673	316523.516170	44.368487
3502.388429	316501.737199	44.373492
3502.077687	316479.319249	44.378497
3502.269475	316454.660398	44.383501
3502.586196	316435.859525	44.388506
3502.423836	316407.312025	44.393511
3502.226660	316389.049084	44.398516
3502.373406	316367.195974	44.403521
3502.668711	316332.750653	44.408525
3502.299729	316303.751814	44.413530
3502.141514	316283.498173	44.418535
3502.325686	316263.598340	44.423540
3502.565853	316230.331924	44.428545
3502.171406	316210.369446	44.433549
3502.241565	316183.719332	44.438554
3502.543640	316159.297593	44.443559
3502.344932	316128.389319	44.448564
3501.896703	316111.259407	44.453569
3502.490494	316085.545496	44.458573
3502.090441	316068.942387	44.463578
3501.885041	316040.070585	44.468583
3501.904114	316022.206386	44.473588
3501.817506	316009.727241	44.478593
3502.025436	315978.094050	44.483597
3501.980407	315966.244515	44.488602
3501.866586	315941.861933	44.493607
3502.357564	315925.399997	44.498612
3502.112050	315901.699423	44.503617
3502.107007	315878.826505	44.508621
3502.081256	315858.094073	44.513626
3501.930816	315839.747305	44.518631
3501.889406	315807.567589	44.523636
3501.852416	315802.332144	44.528641
3502.001983	315773.964698	44.533645
3501.828117	315752.720946	44.538650
3502.062515	315741.463965	44.543655
3502.130402	315714.992035	44.548660
3501.747193	315696.121667	44.553665
3502.044120	315662.795113	44.558669
3502.176488	315663.588938	44.563674
3502.192662	315637.557556	44.568679
3502.506767	315619.621844	44.573684
3502.340072	315603.236690	44.578689
3502.205794	315562.165884	44.583693
3502.552900	315538.449233	44.588698
3502.304398	315515.486797	44.593703
3502.291527	315498.670565	44.598708
3502.050243	315470.872629	44.603713
3502.195410	315437.340530	44.608717
3502.381075	315432.782827	44.613722
3502.071039	315415.936475	44.618727
3502.428294	315391.124075	44.623732
3502.063750	315361.106180	44.628737
3502.218954	315330.193176	44.633741
3502.380403	315298.134196	44.638746
3502.184702	315279.539804	44.643751
3502.149056	315264.635336	44.648756
3501.902475	315249.178472	44.653761
3501.988887	315223.186812	44.658765
3501.917685	315193.861037	44.663770
3501.763053	315168.186740	44.668775
3501.894706	315166.919710	44.673780
3501.651547	315155.965896	44.678785
3501.945867	315131.341258	44.683789
3501.859316	315108.277082	44.688794
3502.072239	315091.094789	44.693799
3501.966651	315067.702780	44.698804
3501.696512	315051.358968	44.703809
3502.073227	315035.626930	44.708813
3502.293016	315006.459308	44.713818
3501.959985	314991.092142	44.718823
3502.278426	314960.993146	44.723828
3502.376268	314947.925233	44.728833
3502.521525	314922.942015	44.733837
3502.397147	314894.362208	44.738842
3502.098838	314873.264632	44.743847
3502.369734	314845.742835	44.748852
3502.260134	314829.501183	44.753857
3502.446609	314793.646749	44.758861
3502.464166	314772.703529	44.763866
3502.142444	314760.031628	44.768871
3502.285240	314730.366924	44.773876
3502.172070	314702.065141	44.778881
3502.276807	314669.098546	44.783885
3502.388982	314649.183767	44.788890
3502.117382	314630.524589	44.793895
3502.146034	314613.574347	44.798900
3502.160927	314590.977569	44.803905
3502.047905	314572.853468	44.808909
3502.083029	314542.085840	44.813914
3502.096168	314520.379858	44.818919
3502.162489	314499.657925	44.823924
3502.163006	314485.739912	44.828929
3502.087517	314456.261666	44.833933
3502.573272	314434.532987	44.838938
3502.209055	314414.336015	44.843943
3502.232904	314385.173044	44.848948
3501.710194	314368.639290	44.853953
3502.044074	314338.206704	44.858957
3502.091596	314327.156569	44.863962
3501.826829	314303.559939	44.868967
3502.161825	314281.371200	44.873972
3502.277539	314266.595521	44.878977
3502.346723	314234.041262	44.883981
3502.339994	314210.175429	44.888986
3502.109032	314194.028772	44.893991
3502.196303	314161.955096	44.898996
3501.978461	314149.241417	44.904001
3502.239407	314115.435888	44.909005
3502.182718	314102.468115	44.914010
3502.185354	314086.056067	44.919015
3502.238545	314065.412317	44.924020
3502.056771	314040.784848	44.929025
3502.038776	314008.905560	44.934029
3502.328141	313989.828046	44.939034
3501.863364	313974.379262	44.944039
3502.027962	313943.005856	44.949044
3502.045954	313933.410576	44.954049
3502.309724	313902.683276	44.959053
3502.376714	313893.716485	44.964058
3502.019660	313870.541112	44.969063
3502.087386	313836.536443	44.974068
3501.966386	313816.912038	44.979073
3502.042196	313793.796492	44.984077
3501.886382	313779.215581	44.989082
3501.927324	313766.486971	44.994087
3502.276824	313741.471330	44.999092
3502.333701	313721.310307	45.004097
3501.973187	313687.601172	45.009101
3502.083168	313665.090924	45.014106
3502.164731	313642.686867	45.019111
3502.207555	313628.812902	45.024116
3502.223194	313615.197613	45.029121
3502.100272	313584.581167	45.034125
3502.312028	313561.876916	45.039130
3502.271263	313538.881164	45.044135
3502.446128	313521.882324	45.049140
3502.119355	313493.129583	45.054145
3502.227101	313467.235392	45.059149
3502.215511	313446.983124	45.064154
3501.855090	313422.688467	45.069159
3502.235936	313397.820434	45.074164
3501.806529	313377.963940	45.079169
3502.311967	313349.157943	45.084173
3502.529393	313334.315249	45.089178
3502.059012	313308.256482	45.094183
3501.958540	313280.740653	45.099188
3502.029693	313266.938507	45.104193
3501.998177	313245.518773	45.109197
3501.944783	313228.580792	45.114202
3501.720814	313211.542121	45.119207
3502.139850	313181.858883	45.124212
3501.876498	313170.271608	45.129217
3502.092699	313136.930344	45.134221
3501.853584	313125.746410	45.139226
3502.044774	313108.388645	45.144231
3502.241478	313089.605080	45.149236
3502.054543	313067.446091	45.154241
3502.085515	313055.456752	45.159245
3502.228623	313029.531370	45.164250
3502.282327	313008.734399	45.169255
3502.000461	312975.699534	45.174260
3502.074974	312952.558327	45.179265
3502.350078	312930.581827	45.184269
3502.209860	312910.120334	45.189274
3501.883414	312891.189089	45.194279
3501.995391	312876.031869	45.199284
3502.204154	312847.093612	45.204289
3501.947625	312825.352464	45.209293
3501.903619	312794.875891	45.214298
3501.845253	312791.373721	45.219303
3502.119202	312763.850214	45.224308
3501.865442	312755.772817	45.229313
3502.060158	312737.472884	45.234317
3502.221956	312711.697091	45.239322
3502.139813	312695.526755	45.244327
3501.733918	312668.796013	45.249332
3501.905576	312658.209629	45.254337
3501.851098	312631.220616	45.259341
3502.070342	312615.359591	45.264346
3501.975652	312600.717907	45.269351
3502.220722	312573.351456	45.274356
3501.947537	312552.630596	45.279361
3501.880237	312534.702150	45.284365
3501.927066	312511.946718	45.289370
3501.729285	312504.496707	45.294375
3501.994170	312470.663927	45.299380
3502.056488	312458.822232	45.304385
3501.707014	312430.962966	45.309389
3501.740644	312416.275812	45.314394
3501.815413	312398.732336	45.319399
3501.909921	312374.875255	45.324404
3501.709979	312369.130419	45.329409
3501.802078	312351.838686	45.334413
3501.924009	312326.374234	45.339418
3501.902927	312316.377572	45.344423
3502.026961	312290.200293	45.349428
3501.940824	312270.671597	45.354433
3502.246384	312256.730895	45.359437
3501.873770	312232.386625	45.364442
3502.009940	312219.464655	45.369447
3502.186403	312192.286779	45.374452
3501.911513	312174.975752	45.379457
3501.940492	312141.662917	45.384461
3501.842727	312134.044608	45.389466
3502.036517	312112.360284	45.394471
3502.109984	312096.547215	45.399476
3502.000089	312080.024744	45.404481
3502.093997	312053.877469	45.409485
3501.917296	312038.306876	45.414490
3501.830229	312023.256693	45.419495
3501.642836	311995.906312	45.424500
3501.739549	311977.239646	45.429505
3501.880966	311969.533200	45.434509
3501.760106	311943.521067	45.439514
3501.870192	311933.020440	45.444519
3501.899573	311906.755895	45.449524
3501.792139	311892.294096	45.454529
3502.034296	311876.861838	45.459533
3502.055396	311855.814972	45.464538
3501.834492	311843.991749	45.469543
3501.770901	311816.901905	45.474548
3501.747891	311800.289479	45.479553
3501.740688	311779.119753	45.484557
3501.977668	311760.074931	45.489562
3501.328320	311748.089341	45.494567
3501.679601	311731.723998	45.499572
3501.982842	311718.928570	45.504577
3502.108553	311700.740758	45.509581
3502.211258	311681.436893	45.514586
3502.106748	311666.363865	45.519591
3502.179108	311635.308622	45.524596
3501.874441	311618.205593	45.529601
3501.815788	311596.076841	45.534605
3502.205176	311575.939493	45.539610
3501.835232	311551.492672	45.544615
3502.080802	311530.105378	45.549620
3501.698237	311513.447018	45.554625
3501.722201	311501.509267	45.559629
3501.870297	311483.063427	45.564634
3501.602276	311457.252051	45.569639
3502.148645	311439.965634	45.574644
3502.120562	311434.372064	45.579649
3501.904443	311412.980223	45.584653
3502.218292	311392.930890	45.589658
3501.827718	311370.471991	45.594663
3502.166357	311345.354984	45.599668
3501.798062	311345.539746	45.604673
3502.208149	311321.531242	45.609677
3502.296834	311301.466017	45.614682
3501.625587	311274.801224	45.619687
3501.962946	311250.498646	45.624692
3502.010366	311239.651370	45.629697
3501.992765	311218.330335	45.634701
3502.316442	311194.335213	45.639706
3501.811548	311179.706031	45.644711
3501.800063	311162.735340	45.649716
3502.116100	311140.929764	45.654721
3502.233394	311120.376531	45.659725
3502.103132	311086.985951	45.664730
3501.772028	311073.881920	45.669735
3502.112957	311044.184050	45.674740
3501.883128	311037.120491	45.679745
3501.622881	311015.837124	45.684749
3502.154720	310998.807274	45.689754
3501.759843	310981.463590	45.694759
3502.330428	310951.526354	45.699764
3501.899208	310944.901262	45.704769
3501.680698	310919.565374	45.709773
3501.968299	310914.482440	45.714778
3501.705273	310891.774449	45.719783
3501.830919	310861.499252	45.724788
3501.932854	310854.205913	45.729793
3501.985533	310833.713504	45.734797
3502.020204	310804.724753	45.739802
3501.787325	310781.070497	45.744807
3501.911266	310769.040666	45.749812
3502.078057	310755.095673	45.754817
3501.994004	310724.420430	45.759821
3501.988152	310663.018969	45.764826
3501.493373	310551.360060	45.769831
3501.452288	310396.345415	45.774836
3500.948028	310205.904025	45.779841
3499.953752	309967.392512	45.784845
3499.198392	309697.033777	45.789850
3498.697231	309376.477439	45.794855
3497.909299	309025.528476	45.799860
3496.502520	308634.593259	45.804865
3495.629084	308198.961827	45.809869
3494.429129	307740.016006	45.814874
3492.942586	307232.885904	45.819879
3491.632731	306701.419721	45.824884
3489.889492	306136.982678	45.829889
3488.554834	305546.084938	45.834893
3486.944066	304922.724295	45.839898
3484.446915	304267.452689	45.844903
3482.755891	303590.007518	45.849908
3480.973923	302889.407773	45.854913
3479.305121	302157.120262	45.859917
3477.096002	301388.511534	45.864922
3474.374823	300605.642285	45.869927
3472.287428	299805.763055	45.874932
3469.876235	298978.128634	45.879937
3467.509675	298124.996785	45.884941
3465.160716	297266.402318	45.889946
3462.434318	296375.680422	45.894951
3459.946603	295470.144380	45.899956
3457.133100	294547.005185	45.904961
3454.445023	293610.442926	45.909965
3451.524620	292643.890652	45.914970
3449.006503	291680.824236	45.919975
3445.840499	290681.288955	45.924980
3442.947815	289694.499777	45.929985
3439.968173	288681.055689	45.934989
3436.944298	287670.682959	45.939994
3433.769954	286635.929862	45.944999
3430.754167	285591.283909	45.950004
3427.399142	284539.495508	45.955009
3424.298350	283477.519056	45.960013
3421.347442	282417.743729	45.965018
3417.815723	281339.355968	45.970023
3414.554852	280251.566472	45.975028
3411.350875	279170.499272	45.980033
3407.977350	278070.118618	45.985037
3404.760496	276976.674349	45.990042
3401.048634	275875.450049	45.995047
3397.310294	274761.917034	46.000052
3394.096846	273657.708362	46.005057
3390.954178	272533.308272	46.010061
3387.439557	271404.546553	46.015066
3383.821772	270285.131521	46.020071
3380.507067	269159.799123	46.025076
3376.675840	268033.209538	46.030081
3373.362310	266899.701952	46.035085
3370.059565	265759.584544	46.040090
3366.169134	264635.002717	46.045095
3363.070685	263479.040503	46.050100
3359.291452	262347.796440	46.055105
3355.572865	261200.080982	46.060109
3351.817126	260057.936792	46.065114
3348.302685	258922.594350	46.070119
3344.377073	257768.206017	46.075124
3341.118634	256629.568792	46.080129
3337.281391	255488.872663	46.085133
3333.918271	254346.234222	46.090138
3329.907837	253208.678846	46.095143
3326.742315	252047.833865	46.100148
3322.548685	250905.552906	46.105153
3318.986255	249771.493483	46.110157
3315.264837	248625.099526	46.115162
3311.348791	247484.484171	46.120167
3307.892402	246348.068943	46.125172
3304.282684	245214.166913	46.130177
3300.561067	244072.304675	46.135181
3296.668092	242935.913436	46.140186
3292.947373	241811.765658	46.145191
3289.632062	240669.441806	46.150196
3285.256447	239544.214721	46.155201
3281.915430	238423.967009	46.160205
3278.408423	237303.690293	46.165210
3274.453843	236180.805455	46.170215
3270.736963	235055.180712	46.175220
3266.865230	233936.937676	46.180225
3263.350865	232829.384400	46.185229
3259.183101	231703.822242	46.190234
3255.952333	230590.745046	46.195239
3251.898696	229487.447189	46.200244
3248.351058	228379.943486	46.205249
3244.467406	227278.705729	46.210253
3240.649924	226162.965316	46.215258
3237.077645	225076.450574	46.220263
3233.271818	223969.979154	46.225268
3229.108944	222879.660259	46.230273
3225.669242	221787.319482	46.235277
3222.225326	220698.316951	46.240282
3218.381263	219613.198492	46.245287
3214.789920	218528.271690	46.250292
3211.027046	217450.173841	46.255297
3207.116892	216373.120019	46.260301
3203.556386	215295.836162	46.265306
3199.292358	214218.410061	46.270311
3195.965357	213144.992795	46.275316
3192.238541	212087.966597	46.280321
3188.395870	211016.215957	46.285325
3185.224088	209950.834001	46.290330
3180.741544	208893.097113	46.295335
3176.969635	207828.454276	46.300340
3173.212157	206783.908374	46.305345
3169.266249	205730.406712	46.310349
3165.482033	204668.226308	46.315354
3161.709152	203641.042368	46.320359
3158.257132	202597.846140	46.325364
3154.698829	201558.263495	46.330369
3150.705138	200529.731314	46.335373
3147.113872	199492.789884	46.340378
3143.444138	198468.320813	46.345383
3139.906905	197443.838128	46.350388
3135.737052	196418.111437	46.355393
3131.784384	195405.091601	46.360397
3128.517068	194389.171472	46.365402
3124.470098	193388.252621	46.370407
3121.246529	192366.128049	46.375412
3117.276928	191360.629675	46.380417
3113.433734	190355.094674	46.385421
3110.080505	189354.050410	46.390426
3106.015565	188351.597940	46.395431
3102.187486	187361.620870	46.400436
3098.266936	186366.880120	46.405441
3094.467082	185377.401173	46.410445
3091.086004	184401.438910	46.415450
3086.908162	183425.355640	46.420455
3083.600654	182454.086672	46.425460
3079.677954	181492.344733	46.430465
3075.911007	180510.142028	46.435469
3072.358344	179545.409345	46.440474
3068.188161	178584.500758	46.445479
3064.577850	177634.362462	46.450484
3060.839650	176680.651889	46.455489
3056.972817	175744.031321	46.460493
3053.273475	174799.133338	46.465498
3049.328078	173863.234216	46.470503
3045.608483	172917.368806	46.475508
3041.833033	171993.686653	46.480513
3037.669839	171063.762050	46.485517
3034.112530	170144.702305	46.490522
3029.949728	169243.085951	46.495527
3026.307987	168321.681918	46.500532
3022.331552	167429.899200	46.505537
3018.462861	166543.940993	46.510541
3014.762845	165647.275636	46.515546
3010.966198	164774.261703	46.520551
3007.134133	163893.894818	46.525556
3003.357604	163012.309110	46.530561
2999.320363	162145.655225	46.535565
2995.424585	161285.265967	46.540570
2991.522658	160429.509583	46.545575
2987.629870	159581.756505	46.550580
2983.985922	158744.845678	46.555585
2979.863908	157911.940776	46.560589
2976.175284	157087.227187	46.565594
2971.954838	156262.658711	46.570599
2968.540303	155437.569144	46.575604
2964.008725	154636.794881	46.580609
2960.341231	153838.353542	46.585613
2956.529425	153032.768264	46.590618
2952.179449	152250.579828	46.595623
2948.429192	151468.449076	46.600628
2944.455582	150705.860089	46.605633
2940.309844	149949.162359	46.610637
2936.747366	149193.148031	46.615642
2932.469886	148459.219441	46.620647
2928.641052	147715.827433	46.625652
2924.935703	146991.908561	46.630657
2920.696309	146276.328521	46.635661
2917.140440	145563.553286	46.640666
2912.996801	144863.043980	46.645671
2909.027312	144165.087592	46.650676
2904.690901	143475.455923	46.655681
2900.438075	142798.964548	46.660685
2897.018650	142128.180224	46.665690
2892.898745	141470.708373	46.670695
2889.104332	140814.976071	46.675700
2884.930370	140180.699369	46.680705
2880.851060	139551.314725	46.685709
2877.080349	138918.264444	46.690714
2872.994525	138313.554124	46.695719
2869.403996	137693.673021	46.700724
2865.484317	137092.807650	46.705729
2861.494933	136494.060133	46.710733
2858.200200	135913.722820	46.715738
2854.033658	135264.220305	46.720743
2850.508198	134653.237450	46.725748
2846.552151	134079.781856	46.730753
2842.774429	133515.185366	46.735757
2839.402568	132946.233198	46.740762
2835.428877	132389.390640	46.745767
2832.104911	131831.029354	46.750772
2828.245104	131292.004954	46.755777
2824.197934	130735.589409	46.760781
2820.366977	130185.278629	46.765786
2816.632595	129656.800412	46.770791
2813.210070	129121.398744	46.775796
2809.593255	128590.282535	46.780801
2805.962567	128047.040661	46.785805
2802.626013	127521.847218	46.790810
2798.683996	127003.190636	46.795815
2795.420847	126483.633628	46.800820
2791.673030	125966.473486	46.805825
2788.178360	125442.336012	46.810829
2784.877746	124919.803101	46.815834
2780.877539	124396.508245	46.820839
2777.135983	123885.656670	46.825844
2773.973865	123378.689534	46.830849
2770.052889	122859.993745	46.835853
2766.555702	122356.462100	46.840858
2763.216021	121851.945840	46.845863
2760.082852	121336.237937	46.850868
2756.502073	120830.704110	46.855873
2752.839068	120324.553808	46.860877
2749.689925	119814.184421	46.865882
2745.950107	119308.898750	46.870887
2742.253376	118793.223506	46.875892
2738.665569	118278.937122	46.880897
2734.921849	117782.751935	46.885901
2731.682900	117267.407726	46.890906
2727.785723	116770.649405	46.895911
2724.429957	116267.493664	46.900916
2720.879688	115775.297773	46.905921
2717.134751	115274.415887	46.910925
2714.076982	114770.255045	46.915930
2710.105874	114272.549990	46.920935
2706.824928	113770.764533	46.925940
2702.876888	113274.163030	46.930945
2699.323319	112773.718000	46.935949
2695.830810	112279.932802	46.940954
2692.162682	111791.559881	46.945959
2688.478973	111300.589677	46.950964
2684.811216	110819.578789	46.955969
2681.336255	110331.208597	46.960973
2677.640746	109842.523516	46.965978
2673.785089	109370.944281	46.970983
2670.498869	108887.039945	46.975988
2666.795936	108423.179417	46.980993
2663.267203	107941.321955	46.985997
2659.461961	107472.036280	46.991002
2655.757519	107009.008614	46.996007
2651.687219	106536.535292	47.001012
2648.201225	106078.380512	47.006017
2644.211200	105625.560420	47.011021
2640.707396	105178.963097	47.016026
2636.587030	104730.776987	47.021031
2632.940975	104293.493098	47.026036
2629.244647	103850.006893	47.031041
2625.450002	103427.769588	47.036045
2622.190032	102997.293959	47.041050
2618.362052	102563.798160	47.046055
2614.356779	102137.479068	47.051060
2610.985041	101722.379298	47.056065
2607.051899	101317.184574	47.061069
2603.340528	100911.718874	47.066074
2599.493091	100497.890759	47.071079
2596.122772	100093.500687	47.076084
2593.103653	99690.560770	47.081089
2589.253188	99283.192525	47.086093
2585.593365	98887.378072	47.091098
2581.907183	98493.161277	47.096103
2578.810786	98090.583934	47.101108
2575.160560	97694.210882	47.106113
2571.407640	97295.736398	47.111117
2568.303268	96886.859307	47.116122
2564.777170	96505.833874	47.121127
2561.158231	96098.661082	47.126132
2557.663669	95704.334879	47.131137
2554.062331	95310.869002	47.136141
2551.117525	94905.678264	47.141146
2547.279804	94507.481204	47.146151
2543.884831	94116.857581	47.151156
2540.642437	93709.568545	47.156161
2537.024448	93313.551081	47.161165
2533.680673	92903.403991	47.166170
2530.110204	92509.016041	47.171175
2526.968432	92098.098637	47.176180
2522.981669	91700.164563	47.181185
2519.435105	91297.440461	47.186189
2515.882041	90893.947668	47.191194
2512.333627	90496.050200	47.196199
2509.120968	90089.402268	47.201204
2505.761044	89699.490715	47.206209
2502.016420	89292.301139	47.211213
2498.672368	88875.233600	47.216218
2494.722495	88475.011569	47.221223
2491.453231	88077.954215	47.226228
2488.316001	87675.710814	47.231233
2484.597481	87269.955271	47.236237
2481.501909	86858.429519	47.241242
2477.566895	86450.025702	47.246247
2474.178239	86041.390139	47.251252
2470.886482	85635.311435	47.256257
2467.748616	85228.934996	47.261261
2464.329857	84803.578087	47.266266
2460.450416	84405.408115	47.271271
2457.086223	83985.784035	47.276276
2453.749318	83567.267022	47.281281
2450.120482	83159.713289	47.286285
2446.843385	82751.183367	47.291290
2442.949340	82342.983985	47.296295
2439.584613	81918.093574	47.301300
2435.929324	81502.336758	47.306305
2432.468723	81095.815461	47.311309
2429.532561	80663.179982	47.316314
2425.320442	80252.901169	47.321319
2422.069691	79837.664992	47.326324
2418.668793	79428.554922	47.331329
2415.037144	79015.790832	47.336333
2411.893298	78591.081804	47.341338
2407.886312	78170.590522	47.346343
2404.828634	77746.516148	47.351348
2401.455562	77330.104812	47.356353
2397.689603	76907.118891	47.361357
2394.498369	76480.544964	47.366362
2390.826875	76071.133389	47.371367
2387.522752	75645.771221	47.376372
2384.254697	75222.594396	47.381377
2380.308489	74785.408512	47.386381
2376.906908	74363.954944	47.391386
2373.377615	73946.362852	47.396391
2370.100805	73516.445985	47.401396
2366.772352	73092.728099	47.406401
2362.756258	72661.949648	47.411405
2359.518183	72229.127073	47.416410
2355.930361	71803.400459	47.421415
2352.193263	71373.501147	47.426420
2349.300844	70951.755948	47.431425
2345.443086	70518.727851	47.436429
2342.160702	70082.697154	47.441434
2338.267798	69660.373070	47.446439
2334.459352	69222.877000	47.451444
2331.394202	68790.509779	47.456449
2327.592909	68379.326804	47.461453
2324.269261	67939.237873	47.466458
2320.725496	67521.725150	47.471463
2317.224649	67090.520747	47.476468
2313.808469	66660.598996	47.481473
2310.209887	66229.906771	47.486477
2306.907829	65798.433074	47.491482
2303.139466	65370.942818	47.496487
2299.434770	64940.327130	47.501492
2296.184796	64513.938592	47.506497
2292.670628	64088.588520	47.511501
2289.308766	63654.577688	47.516506
2285.788845	63224.070609	47.521511
2282.314846	62794.236557	47.526516
2279.062521	62361.424355	47.531521
2275.350755	61932.003990	47.536525
2271.992141	61496.881661	47.541530
2268.449347	61073.726330	47.546535
2264.868373	60639.453373	47.551540
2261.363615	60199.039793	47.556545
2257.684779	59769.931298	47.561549
2254.309151	59338.238565	47.566554
2250.816252	58908.323111	47.571559
2247.427553	58468.322537	47.576564
2243.860114	58030.318480	47.581569
2240.104438	57600.752698	47.586573
2237.101859	57154.281975	47.591578
2233.587216	56720.785847	47.596583
2229.899768	56291.328059	47.601588
2226.549516	55845.862189	47.606593
2222.878104	55409.755826	47.611597
2219.568597	54970.638272	47.616602
2215.973186	54533.692372	47.621607
2212.476302	54099.714676	47.626612
2209.180308	53654.313291	47.631617
2205.658321	53216.162320	47.636621
2202.288243	52765.251005	47.641626
2198.748832	52326.649944	47.646631
2194.917123	51885.742782	47.651636
2191.804458	51445.417176	47.656641
2187.898193	51000.427809	47.661645
2184.516880	50557.014561	47.666650
2180.911502	50109.248882	47.671655
2177.134592	49663.072655	47.676660
2173.840156	49225.329533	47.681665
2170.257726	48788.863758	47.686669
2166.853924	48341.209056	47.691674
2163.193200	47909.440504	47.696679
2159.830805	47462.887553	47.701684
2156.478820	47030.745172	47.706689
2153.089716	46585.399693	47.711693
2149.497812	46141.794239	47.716698
2145.667251	45705.343991	47.721703
2142.248960	45254.613371	47.726708
2138.806751	44821.500079	47.731713
2135.262246	44382.893941	47.736717
2131.995944	43930.657087	47.741722
2128.097096	43492.795833	47.746727
2124.732390	43045.183445	47.751732
2121.816912	42601.137288	47.756737
2118.177492	42155.373863	47.761741
2114.416522	41709.720816	47.766746
2110.913746	41265.279407	47.771751
2107.196397	40818.914843	47.776756
2104.097947	40382.106857	47.781761
2100.021235	39941.871269	47.786765
2096.711521	39480.184252	47.791770
2093.266298	39045.663463	47.796775
2089.579690	38601.343103	47.801780
2086.423341	38152.219900	47.806785
2082.646725	37717.891538	47.811789
2079.202647	37260.361985	47.816794
2075.895497	36822.016511	47.821799
2072.455736	36371.700478	47.826804
2068.965196	35923.848754	47.831809
2065.456818	35485.371903	47.836813
2062.277502	35022.340595	47.841818
2058.530356	34583.330056	47.846823
2054.541796	34125.154002	47.851828
2051.233067	33680.871037	47.856833
2047.677348	33233.327309	47.861837
2044.443113	32789.330504	47.866842
2040.336762	32345.954204	47.871847
2037.067288	31907.273887	47.876852
2034.108268	31462.089974	47.881857
2030.256347	31012.814691	47.886861
2026.774597	30556.317504	47.891866
2023.405402	30117.855315	47.896871
2019.736735	29665.944447	47.901876
2016.228077	29219.037567	47.906881
2012.486417	28770.883944	47.911885
2009.377663	28321.443972	47.916890
2005.779338	27887.931732	47.921895
2002.057679	27430.077627	47.926900
1998.794025	26991.925727	47.931905
1995.163003	26543.651775	47.936909
1991.567805	26092.733681	47.941914
1987.787609	25652.904370	47.946919
1984.442448	25201.992613	47.951924
1980.527893	24757.451912	47.956929
1976.784528	24319.324999	47.961933
1973.570074	23876.335794	47.966938
1970.272425	23443.074989	47.971943
1966.611271	23003.766777	47.976948
1963.183848	22559.642644	47.981953
1959.514233	22124.973394	47.986957
1955.983431	21678.275144	47.991962
1952.164285	21248.057403	47.996967
1948.846938	20817.707612	48.001972
1945.398156	20369.753035	48.006977
1942.076623	19942.387516	48.011981
1938.771558	19494.329229	48.016986
1934.777699	19071.305829	48.021991
1931.311842	18629.442607	48.026996
1927.916086	18191.689004	48.032001
1924.065045	17757.556523	48.037005
1920.751340	17321.355157	48.042010
1917.148068	16892.472829	48.047015
1913.500012	16459.348057	48.052020
1910.133637	16025.821887	48.057025
1906.270205	15608.540824	48.062029
1902.683352	15179.412350	48.067034
1899.529051	14752.879482	48.072039
1896.111855	14329.290924	48.077044
1892.552283	13893.177259	48.082049
1888.831512	13461.850871	48.087053
1885.241760	13039.622308	48.092058
1881.339522	12614.830460	48.097063
1877.980807	12194.414688	48.102068
1874.122413	11770.537278	48.107073
1870.735152	11356.830665	48.112077
1867.177473	10937.803517	48.117082
1863.327875	10530.106746	48.122087
1859.534055	10114.021747	48.127092
1856.457989	9701.281413	48.132097
1851.967709	9312.867830	48.137101
1848.532217	8907.696499	48.142106
1844.266722	8516.729232	48.147111
1840.655698	8133.115867	48.152116
1836.569984	7758.588899	48.157121
1832.382396	7391.507277	48.162125
1828.096908	7041.678048	48.167130
1823.238121	6713.912036	48.172135
1818.676920	6410.468297	48.177140
1813.717902	6114.433755	48.182145
1809.001734	5821.923351	48.187149
1804.925662	5558.828513	48.192154
1800.529596	5306.309647	48.197159
1796.087113	5063.741458	48.202164
1792.995036	4830.466282	48.207169
1788.671528	4600.806584	48.212173
1785.183922	4387.373639	48.217178
1781.605245	4180.976081	48.222183
1778.132312	3973.491691	48.227188
1774.685472	3759.803485	48.232193
1770.861358	3561.403226	48.237197
1767.662915	3357.354450	48.242202
1764.086203	3167.995182	48.247207
1760.520417	2972.488131	48.252212
1756.981175	2777.662537	48.257217
1753.411113	2595.288451	48.262221
1750.606837	2411.993344	48.267226
1746.946809	2225.064872	48.272231
1743.527409	2031.557639	48.277236
1740.131670	1836.697778	48.282241
1736.432862	1660.668618	48.287245
1733.443522	1476.415228	48.292250
1730.000969	1285.991861	48.297255
1726.202362	1105.775691	48.302260
1722.292585	923.556943	48.307265
1718.646706	755.222978	48.312269
1714.851924	571.680110	48.317274
1711.247783	410.103944	48.322279
1707.480536	257.843364	48.327284
1703.817130	94.827137	48.332289
1697.315445	12.558020	48.337293
1686.365632	70.819930	48.342298
1680.018779	76.104296	48.347303
1676.304200	73.072874	48.352308
1673.308479	72.893959	48.357313
1671.474021	89.286121	48.362317
1669.036097	76.767357	48.367322
1666.006891	78.472894	48.372327
1663.309362	78.503828	48.377332
1659.978834	75.055135	48.382337
1656.940260	79.327895	48.387341
1653.517236	65.200282	48.392346
1649.633565	74.416566	48.397351
1646.028232	72.760174	48.402356
1642.967183	72.233930	48.407361
1639.598094	79.541505	48.412365
1635.878402	66.561039	48.417370
1632.461780	62.806217	48.422375
1629.597850	68.791829	48.427380
1626.425961	68.210074	48.432385
1622.749743	75.536977	48.437389
1619.495127	68.552110	48.442394
1615.650172	68.612943	48.447399
1612.236234	70.963649	48.452404
1609.155692	65.457613	48.457409
1605.264002	76.370890	48.462413
1602.032782	66.803967	48.467418
1598.568913	74.360407	48.472423
1594.870539	72.519189	48.477428
1591.704462	67.855357	48.482433
1587.999610	73.161949	48.487437
1584.440984	71.435021	48.492442
1581.058466	67.728679	48.497447
1577.949485	68.159012	48.502452
1574.751324	61.617776	48.507457
1571.078310	70.848728	48.512461
1567.551363	65.124282	48.517466
1563.984246	70.706824	48.522471
1560.354612	73.945305	48.527476
1557.103015	68.067273	48.532481
1553.360637	66.248728	48.537485
1549.920338	65.889087	48.542490
1546.802649	73.432775	48.547495
1543.250023	70.192668	48.552500
1539.824842	73.209507	48.557505
1535.960569	71.640885	48.562509
1533.023745	72.231085	48.567514
1529.629018	63.075597	48.572519
1525.872301	72.778315	48.577524
1522.520271	65.751679	48.582529
1518.654928	73.883127	48.587533
1515.445782	66.944982	48.592538
1511.870680	69.981993	48.597543
1508.203669	81.961271	48.602548
1504.731611	66.253145	48.607553
1500.951661	77.092085	48.612557
1498.149241	66.949083	48.617562
1494.847533	69.921396	48.622567
1490.846300	71.325829	48.627572
1487.430465	69.912038	48.632577
1484.064272	72.154084	48.637581
1480.798418	62.624212	48.642586
1476.821237	60.968772	48.647591
1473.261849	66.312837	48.652596
1470.456969	67.458297	48.657601
1466.513990	68.211434	48.662605
1462.967760	70.490995	48.667610
1459.580115	69.778325	48.672615
1456.032599	64.500014	48.677620
1452.572338	67.990545	48.682625
1449.101700	75.073489	48.687629
1445.814121	74.680596	48.692634
1442.691764	67.048758	48.697639
1438.637084	74.134024	48.702644
1435.131061	65.634941	48.707649
1431.360887	71.128876	48.712653
1427.818505	60.873277	48.717658
1424.824468	62.345570	48.722663
1421.746950	67.171719	48.727668
1418.010707	66.190614	48.732673
1413.893301	70.991964	48.737677
1410.783640	65.715110	48.742682
1407.263541	65.586199	48.747687
1403.541115	62.113118	48.752692
1400.476687	61.261562	48.757697
1396.739548	71.049818	48.762701
1393.411553	66.357432	48.767706
1389.953572	70.413915	48.772711
1386.160080	62.010206	48.777716
1382.793265	62.322502	48.782721
1378.983373	64.962641	48.787725
1375.734359	60.495244	48.792730
1372.122653	57.375087	48.797735
1368.718057	70.667574	48.802740
1365.908433	60.396008	48.807745
1361.808699	71.230938	48.812749
1358.234533	58.287998	48.817754
1354.612811	60.272439	48.822759
1351.016385	57.558023	48.827764
1347.737250	66.724506	48.832769
1344.394038	70.740982	48.837773
1340.716567	59.073274	48.842778
1337.285554	64.068341	48.847783
1333.509354	69.654967	48.852788
1330.892220	60.894164	48.857793
1327.015463	73.127543	48.862797
1323.238534	68.030489	48.867802
1320.024879	66.702305	48.872807
1316.317859	66.229183	48.877812
1312.682555	59.730719	48.882817
1309.305954	68.640298	48.887821
1305.476386	66.737280	48.892826
1302.316482	72.854391	48.897831
1298.846655	60.069225	48.902836
1295.234033	59.331481	48.907841
1292.089424	63.661887	48.912845
1288.639646	55.584343	48.917850
1284.825406	71.708821	48.922855
1281.161632	64.999661	48.927860
1277.749057	56.258280	48.932865
1274.206043	66.813570	48.937869
1270.998604	56.319212	48.942874
1267.587820	58.577706	48.947879
1263.641898	56.594731	48.952884
1260.462958	58.054689	48.957889
1256.563688	62.733512	48.962893
1253.415292	55.112090	48.967898
1250.019483	52.603739	48.972903
1246.552524	53.985144	48.977908
1242.971955	63.053018	48.982913
1239.396407	59.614045	48.987917
1235.656259	56.251314	48.992922
1232.459644	53.800542	48.997927
1228.904173	67.964377	49.002932
1225.606392	57.053828	49.007937
1221.672889	65.512264	49.012941
1218.305672	60.379929	49.017946
1215.156565	62.262345	49.022951
1211.361034	61.825158	49.027956
1207.710326	63.118113	49.032961
1203.902627	65.719963	49.037965
1200.437705	62.864876	49.042970
1196.891113	72.898720	49.047975
1193.531075	72.776554	49.052980
1190.689421	63.648931	49.057985
1186.769298	70.419043	49.062989
1183.689440	65.061652	49.067994
1180.236647	58.050759	49.072999
1176.195198	68.882949	49.078004
1172.604829	62.051653	49.083009
1169.287583	65.149792	49.088013
1165.838333	63.187595	49.093018
1162.363958	66.730963	49.098023
1159.196010	65.750014	49.103028
1155.173780	68.309334	49.108033
1151.787260	63.002846	49.113037
1148.281036	66.886524	49.118042
1145.015349	58.236194	49.123047
1141.224038	65.340589	49.128052
1137.979166	52.381246	49.133057
1134.042304	58.426314	49.138061
1130.705415	57.642506	49.143066
1127.352236	58.927121	49.148071
1123.599293	70.603401	49.153076
1120.451386	62.232127	49.158081
1116.986152	61.547390	49.163085
1113.345599	60.143313	49.168090
1110.036085	60.921271	49.173095
1106.006555	71.830701	49.178100
1102.904095	65.394859	49.183105
1099.311591	83.104635	49.188109
1095.707556	66.651537	49.193114
1092.422137	69.403050	49.198119
1088.684544	70.209679	49.203124
1085.750634	66.560122	49.208129
1081.898217	66.141296	49.213133
1078.506209	63.474189	49.218138
1074.592873	68.319730	49.223143
1071.218059	76.352699	49.228148
1067.918727	68.485882	49.233153
1064.250374	66.668532	49.238157
1060.720527	66.060296	49.243162
1057.434955	68.957365	49.248167
1053.531437	68.344022	49.253172
1050.049588	62.650601	49.258177
1046.883444	61.998408	49.263181
1043.344533	65.466412	49.268186
1039.895903	60.074700	49.273191
1036.055574	63.950282	49.278196
1032.370510	60.927011	49.283201
1029.065154	62.064989	49.288205
1026.156962	62.160402	49.293210
1022.655050	59.168733	49.298215
1018.700553	61.420137	49.303220
1015.335586	65.841808	49.308225
1011.617749	58.429284	49.313229
1008.601878	60.158103	49.318234
1004.748914	54.715446	49.323239
1001.408254	54.090423	49.328244
998.127088	60.014454	49.333249
994.230122	69.273955	49.338253
990.764066	65.068181	49.343258
987.129226	56.342469	49.348263
983.267252	51.638357	49.353268
980.270972	52.956013	49.358273
976.416734	65.366216	49.363277
973.309094	52.578532	49.368282
969.964249	51.881400	49.373287
966.124500	62.856199	49.378292
962.983423	53.911268	49.383297
959.149424	61.408286	49.388301
955.130527	57.908657	49.393306
952.098548	55.618950	49.398311
948.862980	57.698340	49.403316
945.221723	46.512297	49.408321
941.375730	61.002916	49.413325
938.339592	54.949077	49.418330
934.977320	50.195661	49.423335
930.923863	52.149273	49.428340
927.691606	51.301746	49.433345
924.205606	53.511869	49.438349
921.019565	53.511342	49.443354
917.364216	52.128577	49.448359
913.490185	66.455889	49.453364
910.520139	60.031105	49.458369
907.047719	56.354671	49.463373
903.003473	54.795169	49.468378
899.231216	50.510529	49.473383
895.841239	54.224273	49.478388
892.122031	61.716081	49.483393
888.780725	53.621726	49.488397
885.657306	57.439506	49.493402
882.434303	51.598259	49.498407
878.593202	61.285653	49.503412
875.516626	61.328201	49.508417
871.477104	56.759309	49.513421
868.515902	58.871926	49.518426
864.838260	51.003935	49.523431
860.990192	60.221026	49.528436
857.536694	51.853083	49.533441
854.082747	56.560692	49.538445
850.826006	51.591550	49.543450
847.349249	55.204914	49.548455
843.806773	61.603055	49.553460
840.133701	48.084028	49.558465
836.479735	58.074479	49.563469
833.183158	65.304355	49.568474
829.444554	61.365654	49.573479
826.040972	66.220448	49.578484
822.619892	58.815547	49.583489
818.971351	53.426521	49.588493
815.624260	49.002946	49.593498
812.349420	48.323410	49.598503
808.636510	53.197881	49.603508
805.029645	51.946786	49.608513
801.369089	53.143243	49.613517
797.969338	48.275464	49.618522
794.898234	49.750314	49.623527
790.919047	57.361690	49.628532
787.600580	54.325681	49.633537
784.207735	59.362298	49.638541
780.678936	56.134410	49.643546
776.939111	54.445283	49.648551
773.426423	54.555731	49.653556
770.378560	49.481322	49.658561
766.526106	55.592371	49.663565
762.980165	52.832215	49.668570
759.452394	50.882297	49.673575
756.023962	53.140421	49.678580
752.483365	52.119456	49.683585
748.873793	53.140309	49.688589
745.213308	45.918226	49.693594
742.198329	49.114873	49.698599
738.349046	58.578926	49.703604
735.061143	59.435814	49.708609
731.396580	57.861525	49.713613
728.182458	52.999659	49.718618
725.108673	50.358993	49.723623
721.039002	63.947988	49.728628
717.483627	52.403783	49.733633
713.730084	58.135617	49.738637
710.565499	45.581481	49.743642
706.986978	48.422943	49.748647
703.385354	57.142945	49.753652
699.791676	47.948992	49.758657
696.483421	59.363067	49.763661
692.964035	51.600184	49.768666
689.998140	50.303107	49.773671
686.384870	56.677478	49.778676
682.847018	58.231326	49.783681
679.120788	50.228570	49.788685
675.429553	59.301037	49.793690
672.162380	46.592040	49.798695
668.472936	59.656783	49.803700
664.969832	40.543282	49.808705
661.476224	49.464761	49.813709
657.937836	50.392288	49.818714
654.470222	48.448839	49.823719
650.680659	53.724388	49.828724
647.632314	60.251259	49.833729
643.622389	55.174778	49.838733
640.522027	55.376074	49.843738
636.763512	45.983175	49.848743
633.162007	56.572892	49.853748
630.090831	47.345069	49.858753
626.334004	57.342050	49.863757
623.206309	46.927159	49.868762
619.844803	48.219450	49.873767
615.758409	58.682178	49.878772
612.451642	49.690344	49.883777
608.741133	52.248653	49.888781
605.319249	48.529599	49.893786
601.673731	53.216432	49.898791
598.161920	58.394967	49.903796
594.929623	53.754245	49.908801
591.531527	54.982634	49.913805
587.828543	56.391362	49.918810
584.276330	52.752710	49.923815
580.432507	61.909048	49.928820
577.520093	52.492006	49.933825
574.026382	53.722628	49.938829
570.373497	66.765868	49.943834
566.605018	55.229561	49.948839
562.749268	68.067109	49.953844
559.860524	63.654473	49.958849
556.264212	58.687620	49.963853
552.908305	52.553914	49.968858
549.683380	55.931955	49.973863
545.962848	60.026211	49.978868
542.442966	58.805903	49.983873
539.037186	63.873028	49.988877
535.057293	54.511447	49.993882
531.873401	60.255853	49.998887
528.310425	57.144054	50.003892
525.301834	62.092400	50.008897
521.652024	62.610194	50.013901
517.705033	60.810992	50.018906
514.206436	58.445289	50.023911
510.553953	58.912882	50.028916
507.418414	52.153272	50.033921
503.772903	59.136938	50.038925
499.826577	49.412647	50.043930
496.829822	51.761779	50.048935
493.265798	52.870483	50.053940
489.848107	46.262368	50.058945
486.438227	54.247033	50.063949
482.896133	48.841497	50.068954
479.105074	58.075044	50.073959
475.676626	57.995250	50.078964
472.296399	59.391710	50.083969
468.581841	50.795575	50.088973
464.899911	54.244769	50.093978
462.031684	57.007318	50.098983
458.242244	53.918132	50.103988
455.157658	52.225121	50.108993
451.335520	45.591395	50.113997
448.114220	51.050572	50.119002
444.271644	56.767817	50.124007
440.743715	59.149030	50.129012
437.038690	46.859420	50.134017
433.886344	44.677103	50.139021
429.985991	48.954384	50.144026
426.849384	42.381615	50.149031
423.308350	54.619685	50.154036
420.068171	52.337150	50.159041
416.112433	55.765704	50.164045
412.675908	48.461364	50.169050
409.235439	42.290234	50.174055
405.613496	58.191772	50.179060
402.033416	52.165757	50.184065
398.370055	49.968090	50.189069
395.256420	51.313564	50.194074
392.090671	49.987528	50.199079
388.248658	52.468262	50.204084
384.656588	54.941721	50.209089
381.000052	47.690622	50.214093
377.148778	54.946769	50.219098
374.224539	53.700191	50.224103
370.836210	52.870705	50.229108
367.523884	56.759064	50.234113
363.699494	50.302871	50.239117
360.406636	55.238536	50.244122
356.783212	52.911275	50.249127
352.858242	53.414984	50.254132
349.552349	55.138398	50.259137
345.950686	56.303599	50.264141
342.677739	60.676199	50.269146
339.409168	53.826602	50.274151
335.693742	64.016468	50.279156
332.124649	58.972654	50.284161
328.834123	48.273135	50.289165
324.979715	49.452378	50.294170
322.096997	44.899645	50.299175
318.187931	49.776228	50.304180
314.720842	44.748178	50.309185
311.235610	44.126770	50.314189
307.276297	48.134842	50.319194
303.873969	42.179250	50.324199
300.158544	52.210929	50.329204
297.314699	42.153704	50.334209
293.890386	38.210463	50.339213
290.000453	43.526981	50.344218
286.798309	43.231652	50.349223
283.190663	45.353218	50.354228
279.788746	45.427504	50.359233
276.241903	57.400738	50.364237
272.473854	44.678070	50.369242
268.765069	52.497319	50.374247
265.326060	46.952393	50.379252
262.099981	42.516399	50.384257
258.476243	54.115636	50.389261
254.588489	52.187039	50.394266
251.604803	51.974758	50.399271
247.759277	54.747115	50.404276
244.712976	56.094778	50.409281
240.975008	47.761759	50.414285
237.558270	50.394595	50.419290
234.301959	48.731514	50.424295
230.375536	53.829103	50.429300
227.169039	49.810832	50.434305
223.374676	54.258293	50.439309
219.900076	56.238935	50.444314
216.744274	50.776470	50.449319
212.879773	55.307617	50.454324
209.807410	57.706513	50.459329
206.058688	55.477875	50.464333
202.556039	65.447967	50.469338
199.109081	54.526064	50.474343
195.670497	57.456527	50.479348
192.067283	52.149143	50.484353
188.319187	52.353265	50.489357
184.622902	55.750945	50.494362
181.269439	50.774827	50.499367
177.920804	62.657100	50.504372
174.642248	52.964958	50.509377
171.085930	52.506493	50.514381
167.300206	55.380278	50.519386
164.589687	45.438358	50.524391
160.450287	60.613730	50.529396
156.953162	43.577973	50.534401
153.213151	47.634177	50.539405
149.450099	54.354605	50.544410
146.635181	49.424357	50.549415
143.051985	54.822849	50.554420
139.581029	49.804923	50.559425
136.282467	40.220312	50.564429
132.399821	55.479089	50.569434
128.992106	55.244259	50.574439
125.441069	60.697856	50.579444
122.047396	46.354093	50.584449
118.377455	49.785642	50.589453
114.639374	50.178036	50.594458
111.391992	51.503239	50.599463
107.929361	52.849300	50.604468
104.694334	43.419313	50.609473
100.881082	49.442065	50.614477
97.012806	45.096594	50.619482
93.736892	41.433994	50.624487
90.030270	45.931081	50.629492
86.741077	40.960796	50.634497
83.432931	47.192800	50.639501
79.783521	51.563927	50.644506
76.562792	47.513097	50.649511
72.868858	54.959904	50.654516
69.954932	46.495462	50.659521
66.155662	52.516042	50.664525
62.168866	44.867194	50.669530
58.927162	40.237522	50.674535
55.617779	58.902886	50.679540
51.872931	59.805692	50.684545
48.385130	53.993163	50.689549
44.680356	54.168417	50.694554
41.351782	47.359859	50.699559
37.934873	49.410633	50.704564
34.211634	51.958341	50.709569
30.630972	53.221553	50.714573
27.162254	45.393976	50.719578
23.815392	43.811462	50.724583
20.797351	48.837243	50.729588
16.919783	43.117046	50.734593
13.293124	46.092631	50.739597
10.102420	41.673319	50.744602
6.350927	46.693078	50.749607
2.536181	41.561034	50.754612