Fri Aug 26 11:07:53 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.274553	99.077133	0.000000
1.334806	94.154780	0.005005
1.210699	90.317798	0.010010
1.063753	92.716793	0.015014
0.881692	91.606424	0.020019
1.459299	78.988581	0.025024
0.615540	80.366639	0.030029
0.794360	69.177597	0.035034
0.193150	62.849174	0.040038
-0.204493	57.321102	0.045043
-0.133298	60.094241	0.050048
-0.360871	52.904078	0.055053
-0.545937	35.941090	0.060058
-0.860914	28.641162	0.065062
-1.563913	31.047635	0.070067
-1.433262	22.302137	0.075072
-1.852021	19.570870	0.080077
-2.080124	8.941916	0.085082
-2.534340	2.315391	0.090086
-2.513438	6.640214	0.095091
-2.814924	1.945046	0.100096
-3.451068	-1.799539	0.105101
-3.491455	-7.800817	0.110106
-3.586581	-0.569519	0.115110
-4.247025	-4.367266	0.120115
-3.959461	-15.266312	0.125120
-4.354617	-11.819481	0.130125
-4.457845	-20.749998	0.135130
-5.287432	-23.012347	0.140134
-5.956748	-19.130539	0.145139
-5.540203	-12.978624	0.150144
-5.875316	-14.071485	0.155149
-6.091991	-17.536539	0.160154
-6.645726	-20.167693	0.165158
-7.215561	-11.818485	0.170163
-6.858719	-11.877005	0.175168
-7.597072	-17.171678	0.180173
-7.470143	-19.551318	0.185178
-7.310695	-10.445654	0.190182
-8.363038	-10.022184	0.195187
-8.517698	-23.690164	0.200192
-8.604837	-13.565379	0.205197
-8.656960	-17.739401	0.210202
-8.785688	-16.178459	0.215206
-8.977039	-14.981077	0.220211
-9.722347	-18.781425	0.225216
-9.838098	-15.950718	0.230221
-9.998945	-14.242411	0.235226
-10.042520	-18.363982	0.240230
-10.421962	-27.457127	0.245235
-10.640242	-26.413735	0.250240
-11.539535	-14.175731	0.255245
-11.668642	-17.853729	0.260250
-11.894035	-12.658524	0.265254
-11.952071	-14.221617	0.270259
-11.842977	-23.593302	0.275264
-11.942448	-10.236513	0.280269
-12.367490	-24.577378	0.285274
-12.691708	-23.859165	0.290278
-13.221457	-11.621751	0.295283
-13.135863	-12.789606	0.300288
-13.334489	-17.184419	0.305293
-13.481879	-19.018327	0.310298
-13.973014	-20.343150	0.315302
-14.698000	-12.447497	0.320307
-14.567681	-23.546674	0.325312
-14.718136	-16.676915	0.330317
-14.791459	-13.172629	0.335322
-14.789268	-18.585766	0.340326
-15.983555	-11.553483	0.345331
-16.507347	-16.783489	0.350336
-16.429888	-8.544554	0.355341
-16.219985	-11.626789	0.360346
-16.134016	-19.764215	0.365350
-16.364876	-17.769770	0.370355
-16.825643	-22.158567	0.375360
-17.254909	-29.529257	0.380365
-17.513974	-17.849667	0.385370
-17.700293	-19.411768	0.390374
-18.040113	-22.193281	0.395379
-18.262294	-22.977869	0.400384
-19.029223	-26.116810	0.405389
-19.311649	-15.294093	0.410394
-19.315787	-26.267932	0.415398
-19.588973	-16.133164	0.420403
-19.286854	-24.250461	0.425408
-19.294445	-21.673868	0.430413
-19.211527	-19.639696	0.435418
-20.163961	-21.712080	0.440422
-20.789636	-20.988058	0.445427
-20.334433	-27.057000	0.450432
-20.794492	-20.195984	0.455437
-21.680986	-25.957953	0.460442
-21.713905	-23.950037	0.465446
-22.412786	-11.192761	0.470451
-22.168440	-20.158412	0.475456
-22.525024	-20.476000	0.480461
-22.522435	-18.324920	0.485466
-22.423305	-18.925426	0.490470
-23.060635	-12.239279	0.495475
-23.205113	-15.380227	0.500480
-23.413882	-21.329973	0.505485
-23.770978	-16.332556	0.510490
-24.106338	-26.726494	0.515494
-24.203131	-13.569436	0.520499
-24.528884	-19.814170	0.525504
-25.410681	-14.573711	0.530509
-25.630511	-14.042588	0.535514
-25.426511	-19.483982	0.540518
-25.678160	-19.827398	0.545523
-25.337615	-27.011073	0.550528
-25.460237	-20.493650	0.555533
-26.196330	-21.805643	0.560538
-26.371339	-19.392802	0.565542
-26.637713	-22.005423	0.570547
-26.761775	-24.393437	0.575552
-27.922123	-18.005497	0.580557
-28.229879	-12.436813	0.585562
-28.122601	-16.477471	0.590566
-28.095429	-19.556562	0.595571
-28.196900	-17.829027	0.600576
-28.418461	-13.400023	0.605581
-28.403476	-18.252022	0.610586
-28.514834	-18.610954	0.615590
-29.457709	-6.701507	0.620595
-29.591601	-14.931249	0.625600
-29.736869	-11.554962	0.630605
-29.800427	-14.708509	0.635610
-30.222805	-20.795834	0.640614
-31.078026	-13.142486	0.645619
-31.236894	-15.784502	0.650624
-30.937955	-12.005994	0.655629
-31.438211	-12.788413	0.660634
-31.340222	-19.902688	0.665638
-31.553507	-3.940314	0.670643
-31.938066	-16.215296	0.675648
-32.107935	-5.641045	0.680653
-32.822030	-5.244930	0.685658
-32.727678	-13.874028	0.690662
-32.882765	-9.714791	0.695667
-33.499323	1.362432	0.700672
-33.950439	-0.383060	0.705677
-34.265083	-8.236660	0.710682
-34.106171	-5.391771	0.715686
-34.309633	-3.926756	0.720691
-34.052436	-13.119030	0.725696
-34.577029	-1.859981	0.730701
-35.076418	-7.571499	0.735706
-35.202210	-9.060770	0.740710
-35.560508	-4.186544	0.745715
-35.654316	-8.562878	0.750720
-35.959152	-10.524128	0.755725
-36.670217	-12.086782	0.760730
-36.718313	-13.154730	0.765734
-37.192470	-8.025193	0.770739
-36.909882	-12.925186	0.775744
-37.297826	-13.478328	0.780749
-37.106866	-8.724422	0.785754
-37.677836	-6.066437	0.790758
-38.069731	-8.358970	0.795763
-38.199291	-14.738652	0.800768
-38.516840	-7.124727	0.805773
-38.916415	-8.198059	0.810778
-39.302332	-3.797244	0.815782
-39.805688	1.450733	0.820787
-39.827284	-5.037508	0.825792
-40.072630	-9.589556	0.830797
-39.987013	-5.470960	0.835802
-39.975711	-12.603377	0.840806
-40.121441	-3.785544	0.845811
-40.760437	-6.507823	0.850816
-41.131190	-4.137267	0.855821
-41.703015	-8.746048	0.860826
-41.176854	-15.167715	0.865830
-42.295029	3.276653	0.870835
-42.250017	-0.551840	0.875840
-42.740738	-5.556051	0.880845
-43.175054	-3.352762	0.885850
-43.012980	-10.704801	0.890854
-42.964911	-4.359478	0.895859
-43.182327	-10.972246	0.900864
-43.459124	-9.407232	0.905869
-43.690574	-4.666648	0.910874
-43.900540	-7.746782	0.915878
-44.526089	-0.904284	0.920883
-44.289167	-6.005969	0.925888
-44.462167	-5.864939	0.930893
-45.406234	-3.202645	0.935898
-45.792990	-1.810328	0.940902
-46.016819	-2.876224	0.945907
-46.151055	-4.607781	0.950912
-46.014160	-7.254719	0.955917
-45.758084	-12.520731	0.960922
-46.273767	-12.588928	0.965926
-46.551038	-7.281245	0.970931
-47.421023	-7.889043	0.975936
-47.658930	-3.726401	0.980941
-47.990489	-5.993528	0.985946
-47.771566	-16.040352	0.990950
-47.898334	-9.345117	0.995955
-48.049940	-5.907733	1.000960
-48.697733	-8.986134	1.005965
-49.520998	-3.789586	1.010970
-49.260952	-5.860933	1.015974
-49.437435	-8.174350	1.020979
-49.351058	-9.655528	1.025984
-49.578027	-14.719783	1.030989
-49.822167	-5.374119	1.035994
-49.963645	-17.259853	1.040998
-50.650032	-8.069951	1.046003
-50.617674	-7.597075	1.051008
-51.450242	-6.707965	1.056013
-51.546428	-1.169057	1.061018
-51.680939	-6.200256	1.066022
-51.616017	-3.777316	1.071027
-51.702208	-10.296624	1.076032
-51.924557	0.048527	1.081037
-52.973034	-1.626102	1.086042
-52.835009	-15.326998	1.091046
-53.218222	4.939088	1.096051
-53.700012	-7.798469	1.101056
-53.437568	-11.249539	1.106061
-53.687189	-8.717517	1.111066
-54.019370	-9.934215	1.116070
-54.512530	-1.214142	1.121075
-54.466103	-5.520565	1.126080
-54.631542	-8.696213	1.131085
-54.918523	-8.588054	1.136090
-55.850232	-12.536542	1.141094
-55.873798	-3.294820	1.146099
-56.139466	-10.450550	1.151104
-56.223366	-7.618474	1.156109
-56.279073	-17.242899	1.161114
-56.295518	-2.526015	1.166118
-56.702886	-3.155223	1.171123
-57.457309	-7.852628	1.176128
-57.344025	-8.724247	1.181133
-57.576126	-9.077034	1.186138
-57.478704	-13.154121	1.191142
-58.054519	-6.686352	1.196147
-58.768644	-14.180365	1.201152
-59.305906	-1.451414	1.206157
-59.353293	-1.567214	1.211162
-59.313606	-12.968647	1.216166
-59.425990	-10.382064	1.221171
-59.395256	-10.949775	1.226176
-59.601929	-7.295018	1.231181
-59.921971	-8.124477	1.236186
-60.114965	-9.324883	1.241190
-60.366422	-11.246989	1.246195
-60.673056	-22.819111	1.251200
-61.386460	-15.235302	1.256205
-62.167480	-15.132475	1.261210
-61.513994	-12.734740	1.266214
-62.412803	-2.916996	1.271219
-62.030975	-11.151107	1.276224
-61.954218	-18.904295	1.281229
-62.494731	-4.368398	1.286234
-62.300859	-21.346032	1.291238
-63.247161	-14.035997	1.296243
-63.604382	-15.498724	1.301248
-63.572426	-11.438211	1.306253
-63.626776	-19.914442	1.311258
-64.213590	-18.196758	1.316262
-64.962791	-11.423594	1.321267
-65.451163	-17.794861	1.326272
-64.850591	-15.664124	1.331277
-65.180463	-16.960272	1.336282
-64.915401	-9.819863	1.341286
-64.999105	-12.729836	1.346291
-65.976356	-19.354002	1.351296
-66.626767	-12.358947	1.356301
-66.539558	-13.805453	1.361306
-66.524511	-15.357779	1.366310
-66.551383	-13.429895	1.371315
-66.750426	-16.018199	1.376320
-67.295200	-5.790525	1.381325
-68.276511	-6.200660	1.386330
-68.245767	-15.145707	1.391334
-68.059398	-15.199831	1.396339
-68.226827	-12.443332	1.401344
-68.153137	-22.423248	1.406349
-68.787073	-16.863890	1.411354
-69.393043	-15.374169	1.416358
-70.065967	1.526609	1.421363
-69.569021	-10.047256	1.426368
-69.880316	-8.195305	1.431373
-69.888285	-3.144680	1.436378
-70.331561	-3.898007	1.441382
-71.333472	-11.075138	1.446387
-71.312303	-14.371586	1.451392
-71.204120	-9.127084	1.456397
-71.285824	0.468528	1.461402
-71.559683	-9.118770	1.466406
-71.433869	-7.638588	1.471411
-72.408691	-12.627529	1.476416
-72.660790	-6.589800	1.481421
-73.069488	-5.773015	1.486426
-72.662458	-12.169806	1.491430
-73.010693	-2.425132	1.496435
-73.046446	-6.519449	1.501440
-73.196919	-13.022419	1.506445
-74.243961	-7.262700	1.511450
-74.063856	-14.513143	1.516454
-74.439500	-15.944528	1.521459
-74.377197	-22.227533	1.526464
-74.946861	-18.532078	1.531469
-75.393868	-8.585374	1.536474
-75.753995	-13.831369	1.541478
-76.134991	-5.195200	1.546483
-75.899601	-10.309299	1.551488
-75.567430	-18.064291	1.556493
-76.427332	-1.289422	1.561498
-76.640993	-15.764433	1.566502
-77.109322	-8.376962	1.571507
-77.080434	-15.755714	1.576512
-77.238964	-3.354644	1.581517
-77.783502	-7.467815	1.586522
-78.240581	-8.218992	1.591526
-78.964930	-2.613916	1.596531
-79.082520	-8.663278	1.601536
-78.562040	-13.783802	1.606541
-78.656878	-14.983672	1.611546
-78.666329	-15.538798	1.616550
-79.131026	-0.192157	1.621555
-79.896648	-1.385659	1.626560
-80.243086	-6.137095	1.631565
-80.420164	-0.560283	1.636570
-80.215396	-3.793573	1.641574
-80.499116	1.224059	1.646579
-80.958903	-7.170068	1.651584
-80.987237	-12.170340	1.656589
-81.321185	-8.900713	1.661594
-81.421962	-18.790192	1.666598
-81.882569	-7.325985	1.671603
-81.878967	-17.272843	1.676608
-82.504909	-13.040296	1.681613
-83.266478	-11.168856	1.686618
-83.216094	-10.116676	1.691622
-83.529098	-5.445651	1.696627
-82.861205	-5.011619	1.701632
-83.212851	-5.978522	1.706637
-83.653325	-2.632198	1.711642
-84.496860	-2.019781	1.716646
-84.813451	-2.384722	1.721651
-84.927032	-8.944055	1.726656
-84.645254	-15.792726	1.731661
-85.184355	-4.382732	1.736666
-85.772065	-9.099764	1.741670
-86.406283	-6.501531	1.746675
-86.179617	-1.477949	1.751680
-86.162544	-2.799645	1.756685
-86.395444	-10.697603	1.761690
-86.495357	-9.239221	1.766694
-86.405673	-9.224508	1.771699
-86.690748	-10.692141	1.776704
-87.173617	-13.172980	1.781709
-87.406233	-4.708605	1.786714
-88.029929	-13.716264	1.791718
-88.763059	-8.043386	1.796723
-89.073077	-9.111680	1.801728
-88.897221	-6.177685	1.806733
-89.033173	-3.989216	1.811738
-89.013987	-10.607183	1.816742
-89.083706	-5.040762	1.821747
-89.295407	-13.334312	1.826752
-89.846901	-11.394345	1.831757
-90.425635	-8.750970	1.836762
-90.576199	-6.686771	1.841766
-90.571456	-6.060904	1.846771
-90.828731	-5.264531	1.851776
-91.407948	-13.861514	1.856781
-92.037034	-6.063048	1.861786
-92.109415	-6.741250	1.866790
-92.343671	-4.414092	1.871795
-92.481160	-8.144566	1.876800
-91.757994	-8.402488	1.881805
-92.417484	-0.643577	1.886810
-92.724396	-4.910801	1.891814
-93.636322	-13.775508	1.896819
-93.445973	-7.268851	1.901824
-93.761956	-10.104694	1.906829
-94.137359	-5.512535	1.911834
-93.920377	-7.064666	1.916838
-94.134434	-3.563777	1.921843
-95.037236	-9.880008	1.926848
-94.899123	-8.816178	1.931853
-95.042402	3.107973	1.936858
-95.035215	-16.580312	1.941862
-96.037461	-9.758258	1.946867
-96.397153	-12.369003	1.951872
-96.603772	-15.168090	1.956877
-96.693473	-7.769972	1.961882
-96.910009	-18.375392	1.966886
-96.594198	-16.405955	1.971891
-97.061772	-9.790532	1.976896
-97.341088	-11.388771	1.981901
-97.850655	5.299918	1.986906
-98.023469	-4.473951	1.991910
-98.281684	-1.991207	1.996915
-98.174963	-9.449901	2.006912
-98.562443	-7.140099	2.016909
-97.870814	-6.632847	2.026906
-97.153077	-2.990473	2.036902
-96.965396	-8.436051	2.046899
-96.371710	-11.543729	2.056896
-96.132411	-9.740150	2.066893
-95.023724	-10.530069	2.076890
-94.138718	-10.597770	2.086886
-94.004408	-6.478096	2.096883
-94.090789	-9.774483	2.106880
-93.655065	-10.798564	2.116877
-92.966834	-10.541031	2.126874
-92.066578	-11.054584	2.136870
-91.814998	-9.132545	2.146867
-91.337515	-11.284492	2.156864
-90.631021	-8.704713	2.166861
-90.331785	-10.055990	2.176858
-89.921756	-13.093892	2.186854
-88.864797	-10.327936	2.196851
-88.559765	-9.535584	2.206848
-88.607290	-8.596475	2.216845
-88.290045	-7.128138	2.226842
-87.419682	-5.308779	2.236838
-86.448718	-9.238615	2.246835
-86.207687	-10.875424	2.256832
-85.699566	-10.558171	2.266829
-84.914598	-10.201663	2.276826
-84.836824	-12.281871	2.286822
-84.509742	-16.529589	2.296819
-83.502922	-6.967453	2.306816
-83.529535	-9.668117	2.316813
-82.513866	-10.069763	2.326810
-81.793120	-14.904613	2.336806
-81.542504	-19.181604	2.346803
-81.396147	-17.683492	2.356800
-80.904489	-16.381690	2.366797
-80.273590	-13.362502	2.376794
-79.930973	-10.475819	2.386790
-78.753267	-11.805489	2.396787
-78.700306	-11.886186	2.406784
-78.632056	-13.578452	2.416781
-77.644099	-8.068030	2.426778
-77.246178	-9.577218	2.436774
-76.523836	-15.635047	2.446771
-76.212367	-17.808660	2.456768
-76.088899	-23.304422	2.466765
-75.327044	-22.557857	2.476762
-74.871823	-15.719585	2.486758
-73.612027	-13.602912	2.496755
-73.458053	-13.810205	2.506752
-73.352288	-14.149372	2.516749
-73.042076	-8.219822	2.526746
-72.037282	-11.866665	2.536742
-72.072534	-16.599643	2.546739
-71.164028	-15.612992	2.556736
-70.361503	-21.714980	2.566733
-70.403070	-18.540406	2.576730
-69.619321	-10.258132	2.586726
-69.032429	-10.982644	2.596723
-68.962682	-11.373221	2.606720
-68.163488	-11.867870	2.616717
-67.488287	-8.326574	2.626714
-67.247004	-7.204358	2.636710
-66.674811	-18.851967	2.646707
-65.923353	-18.265334	2.656704
-65.976413	-12.919098	2.666701
-65.132666	-7.231004	2.676698
-64.553236	-15.319250	2.686694
-63.981396	-14.444899	2.696691
-63.773303	-10.444415	2.706688
-63.033179	-10.768314	2.716685
-62.922775	-17.370739	2.726682
-62.181423	-14.565145	2.736678
-61.517213	-15.605794	2.746675
-61.382801	-19.155129	2.756672
-60.392480	-21.843072	2.766669
-60.023753	-13.816117	2.776666
-59.996927	-15.258021	2.786662
-59.209728	-16.796142	2.796659
-58.864188	-15.389228	2.806656
-57.906071	-15.655205	2.816653
-57.379126	-15.930074	2.826650
-57.270395	-14.030140	2.836646
-56.863610	-7.865378	2.846643
-55.828538	-12.248673	2.856640
-55.900568	-12.740715	2.866637
-55.219042	-9.105372	2.876634
-54.226577	-12.797810	2.886630
-53.938894	-12.389215	2.896627
-53.904668	-18.545804	2.906624
-53.568594	-14.710961	2.916621
-52.944145	-13.417162	2.926618
-51.882700	-12.140720	2.936614
-51.619839	-12.935153	2.946611
-51.275391	-21.762896	2.956608
-50.719675	-17.103806	2.966605
-50.149493	-17.337891	2.976602
-49.775220	-16.930107	2.986598
-48.683450	-13.181248	2.996595
-48.371115	-16.783628	3.006592
-48.686252	-9.153856	3.016589
-47.660652	-6.094754	3.026586
-47.176021	-2.583969	3.036582
-46.741976	-8.194616	3.046579
-45.967479	-12.331438	3.056576
-45.779672	-14.713872	3.066573
-45.037726	-10.391043	3.076570
-44.289683	-9.027791	3.086566
-44.335486	-9.409880	3.096563
-43.757500	-8.048660	3.106560
-42.948946	-13.752461	3.116557
-42.825486	-12.969850	3.126554
-41.854531	-12.141802	3.136550
-41.171535	-10.058858	3.146547
-40.889795	-12.104304	3.156544
-41.381845	-11.612317	3.166541
-40.382959	-17.922271	3.176538
-39.554387	-11.702808	3.186534
-38.668229	-10.563794	3.196531
-38.251209	-16.206632	3.206528
-38.235182	-14.713568	3.216525
-38.161884	-15.316933	3.226522
-37.597227	-11.295940	3.236518
-36.423063	-11.038040	3.246515
-35.664099	-11.063941	3.256512
-35.481422	-2.307949	3.266509
-35.414322	-7.037861	3.276506
-34.324007	-9.443611	3.286502
-33.836433	-5.958626	3.296499
-33.947667	-6.818353	3.306496
-32.982473	-11.333314	3.316493
-32.416166	-10.797045	3.326490
-32.118785	-8.258099	3.336486
-31.336834	-13.238690	3.346483
-30.956704	-11.811819	3.356480
-30.672031	-13.468094	3.366477
-30.530491	-13.420036	3.376474
-29.362692	-3.135379	3.386470
-29.197657	-12.948857	3.396467
-28.325081	-8.370775	3.406464
-27.770238	-14.709792	3.416461
-27.721729	-8.432226	3.426458
-27.347159	-14.112803	3.436454
-26.364591	-15.326560	3.446451
-26.220066	-12.228474	3.456448
-25.847326	-13.385294	3.466445
-25.119414	-10.241829	3.476442
-24.443816	-9.770091	3.486438
-23.693071	-11.936075	3.496435
-23.217623	-13.118390	3.506432
-23.327707	-7.706253	3.516429
-22.933988	-4.238332	3.526426
-22.128635	-6.587042	3.536422
-21.714211	-6.324888	3.546419
-20.744072	-10.093043	3.556416
-20.356514	-7.384410	3.566413
-20.496331	-16.120919	3.576410
-19.455127	-12.421203	3.586406
-18.906243	-16.234637	3.596403
-18.733703	-15.500848	3.606400
-18.052008	-17.092230	3.616397
-17.535811	-12.395307	3.626394
-17.243763	-8.376215	3.636390
-16.047741	-12.955625	3.646387
-16.063902	-20.054679	3.656384
-15.858855	-13.291488	3.666381
-15.101939	-11.207382	3.676378
-14.532186	-15.312326	3.686374
-13.954965	-14.818935	3.696371
-12.997655	-19.681114	3.706368
-12.696273	-21.865827	3.716365
-12.953473	-21.844381	3.726362
-12.315987	-15.674358	3.736358
-11.460701	-20.146863	3.746355
-10.858326	-24.228375	3.756352
-10.619612	-24.480539	3.766349
-9.958467	-19.898049	3.776346
-9.548854	-23.911536	3.786342
-9.182454	-27.348108	3.796339
-8.280479	-22.581377	3.806336
-8.327825	-17.964600	3.816333
-7.247512	-18.091216	3.826330
-6.807314	-17.158355	3.836326
-6.768578	-16.866216	3.846323
-6.336981	-13.540404	3.856320
-5.818674	-3.556917	3.866317
-5.500432	6.704806	3.876314
-4.827174	12.850264	3.886310
-4.290865	13.451392	3.896307
-3.763192	28.536609	3.906304
-3.276448	34.695276	3.916301
-2.963843	39.712174	3.926298
-2.326927	50.092194	3.936294
-1.741760	63.743021	3.946291
-1.603152	77.853015	3.956288
-0.858694	82.856538	3.966285
-0.677276	104.068242	3.976282
0.000000	109.216310	3.981286
0.371430	122.019003	3.986291
0.622491	127.760146	3.991296
0.675393	128.963799	3.996301
0.516333	133.727950	4.001306
0.658447	126.496016	4.006310
0.450658	140.401280	4.011315
0.787297	140.902713	4.016320
0.437821	133.146217	4.021325
0.639549	134.658885	4.026330
0.654616	127.073418	4.031334
0.767537	126.565671	4.036339
0.693749	129.918201	4.041344
0.644521	137.525213	4.046349
0.861255	146.970043	4.051354
1.261495	146.528288	4.056358
0.700159	148.773518	4.061363
0.838849	133.813254	4.066368
0.942869	148.748790	4.071373
1.081769	140.871960	4.076378
0.916798	145.668672	4.081382
1.120347	139.252887	4.086387
1.057724	135.494904	4.091392
0.450968	134.260835	4.096397
1.082419	149.636258	4.101402
1.248470	150.050359	4.106406
0.620690	143.703898	4.111411
0.998459	143.831941	4.116416
1.074056	158.594744	4.121421
1.415185	150.332092	4.126426
1.008477	139.781487	4.131430
0.998247	139.489062	4.136435
1.281708	141.096569	4.141440
0.950625	151.215138	4.146445
0.524519	141.091485	4.151450
1.450957	153.845752	4.156454
1.224239	163.378616	4.161459
1.559249	157.065740	4.166464
1.166683	152.742208	4.171469
0.900300	148.788163	4.176474
1.227349	147.247354	4.181478
1.123726	150.247038	4.186483
1.530764	159.576825	4.191488
1.209900	144.112315	4.196493
1.094456	146.958819	4.201498
1.398893	144.984944	4.206502
1.192619	150.499914	4.211507
1.460117	142.448042	4.216512
1.341176	141.571444	4.221517
1.148866	138.665699	4.226522
1.289340	134.499618	4.231526
0.780197	144.253611	4.236531
1.399318	145.707620	4.241536
1.463817	165.303090	4.246541
1.637714	154.956300	4.251546
1.227462	151.065782	4.256550
1.090614	160.492906	4.261555
1.937169	152.312907	4.266560
1.552559	160.585900	4.271565
1.029350	145.738174	4.276570
1.546647	153.200040	4.281574
1.653197	159.431917	4.286579
1.754635	147.166569	4.291584
1.561239	141.072008	4.296589
1.373130	135.767545	4.301594
1.262184	135.835641	4.306598
1.211336	135.106625	4.311603
1.391507	158.727254	4.316608
1.672829	157.968665	4.321613
1.509924	159.702619	4.326618
1.933274	152.486996	4.331622
1.681043	155.810369	4.336627
1.668822	144.280874	4.341632
1.106176	139.496620	4.346637
1.171452	153.251814	4.351642
1.640511	148.079139	4.356646
1.538508	159.626828	4.361651
1.653276	157.998850	4.366656
1.563591	162.704752	4.371661
1.516482	163.930307	4.376666
1.792207	156.573156	4.381670
1.395102	157.040139	4.386675
1.641670	155.907320	4.391680
1.548460	163.375662	4.396685
1.803620	163.064061	4.401690
1.841863	159.502335	4.406694
1.540940	153.244182	4.411699
1.710144	150.782010	4.416704
1.871347	164.538095	4.421709
1.386912	164.958565	4.426714
2.006286	160.550239	4.431718
1.614309	166.195366	4.436723
2.045109	163.588060	4.441728
1.383688	158.066225	4.446733
1.642115	151.221122	4.451738
1.796441	151.719304	4.456742
1.854243	161.343906	4.461747
1.916590	168.525445	4.466752
2.298755	170.797779	4.471757
2.000981	162.311901	4.476762
2.189489	156.398313	4.481766
1.962371	169.945951	4.486771
2.084206	162.973417	4.491776
2.052822	166.831868	4.496781
1.926352	169.651620	4.501786
2.088550	164.697556	4.506790
1.920992	169.092890	4.511795
2.245968	153.480360	4.516800
2.073788	154.472293	4.521805
1.826128	166.659582	4.526810
1.809485	162.258535	4.531814
1.624822	165.280331	4.536819
2.038891	165.908910	4.541824
2.158323	186.463937	4.546829
2.572055	173.621613	4.551834
2.390403	173.191365	4.556838
1.871885	165.464338	4.561843
2.000517	160.974236	4.566848
1.871569	157.387923	4.571853
1.963364	173.410524	4.576858
2.348607	180.032441	4.581862
2.333536	189.421638	4.586867
2.082011	173.111094	4.591872
2.178501	174.814153	4.596877
2.262100	187.291557	4.601882
2.429057	186.111021	4.606886
2.130474	185.888800	4.611891
2.565093	177.573615	4.616896
2.140174	172.786891	4.621901
2.089595	168.732804	4.626906
2.564765	181.566843	4.631910
2.493071	177.728008	4.636915
2.521845	169.738601	4.641920
2.497013	162.209951	4.646925
2.128191	161.413385	4.651930
2.247376	157.383488	4.656934
2.079452	166.154245	4.661939
2.291898	173.888205	4.666944
2.055902	185.469428	4.671949
2.240297	185.209973	4.676954
2.558268	184.679789	4.681958
2.529377	189.556563	4.686963
2.390257	172.659055	4.691968
2.676644	179.350146	4.696973
2.679915	182.494540	4.701978
2.847552	171.807036	4.706982
2.554990	177.977678	4.711987
2.496453	177.835138	4.716992
2.397306	180.884749	4.721997
2.560550	169.552540	4.727002
3.056808	176.011642	4.732006
2.466350	177.324959	4.737011
2.494735	156.823263	4.742016
2.303210	170.137574	4.747021
2.485998	177.809717	4.752026
2.688713	185.928004	4.757030
2.414981	185.733550	4.762035
2.669905	177.322960	4.767040
2.673172	182.833788	4.772045
2.869621	176.688008	4.777050
3.032178	179.162210	4.782054
2.911463	184.619579	4.787059
2.673793	164.178280	4.792064
2.380087	162.344987	4.797069
2.444001	172.180611	4.802074
3.121956	183.306328	4.807078
2.744882	186.579542	4.812083
2.729222	182.570634	4.817088
2.897324	179.314545	4.822093
2.787189	191.907536	4.827098
2.867299	184.998437	4.832102
2.809842	195.985568	4.837107
2.753342	188.126487	4.842112
2.821963	184.044346	4.847117
2.838743	180.751707	4.852122
3.125543	177.828306	4.857126
2.497079	190.201448	4.862131
2.684358	179.030002	4.867136
2.648449	177.792470	4.872141
2.623005	178.774213	4.877146
2.858903	179.689956	4.882150
2.709869	186.907577	4.887155
2.918410	179.301456	4.892160
2.720667	185.757886	4.897165
2.567551	188.920303	4.902170
2.430930	189.963648	4.907174
2.567042	196.238390	4.912179
3.143966	203.852342	4.917184
3.173266	201.671368	4.922189
3.465914	201.844301	4.927194
3.512969	197.379545	4.932198
3.068471	188.660241	4.937203
3.130079	186.170525	4.942208
3.058131	184.555797	4.947213
2.815308	186.852677	4.952218
3.213135	187.170582	4.957222
3.116442	205.677578	4.962227
3.461741	200.657032	4.967232
3.411533	190.073037	4.972237
2.988255	183.286606	4.977242
3.403565	181.437830	4.982246
3.127784	179.124029	4.987251
2.854267	185.788405	4.992256
3.109947	190.443706	4.997261
3.483045	200.778523	5.002266
3.530337	182.978805	5.007270
3.111307	186.774232	5.012275
3.052949	189.703601	5.017280
3.386192	189.072965	5.022285
3.207130	192.036947	5.027290
3.321557	192.591961	5.032294
3.003068	201.740510	5.037299
3.148907	206.783069	5.042304
3.350497	207.504843	5.047309
3.331113	209.013979	5.052314
3.681791	204.596859	5.057318
3.533318	209.406837	5.062323
3.533056	200.539269	5.067328
3.473022	202.532450	5.072333
3.381663	201.581954	5.077338
3.566068	200.019058	5.082342
3.278511	198.963071	5.087347
3.245683	206.137298	5.092352
3.429212	209.756657	5.097357
3.351884	206.466011	5.102362
3.476479	203.621644	5.107366
3.697065	207.725605	5.112371
3.471767	207.555247	5.117376
3.686511	209.622703	5.122381
3.585892	200.609412	5.127386
3.877807	204.180258	5.132390
3.377392	206.969654	5.137395
3.523134	206.418830	5.142400
3.542266	204.422932	5.147405
3.630006	212.480040	5.152410
3.604253	208.507498	5.157414
3.445005	213.856982	5.162419
3.467025	212.730648	5.167424
3.521691	211.909272	5.172429
3.088900	214.286352	5.177434
3.461164	220.502190	5.182438
3.234158	220.104312	5.187443
3.533883	222.199666	5.192448
3.582318	218.190262	5.197453
3.374247	220.437444	5.202458
4.237282	239.336039	5.207462
3.814208	228.493705	5.212467
3.621883	221.326459	5.217472
3.911746	219.997074	5.222477
3.554026	221.214047	5.227482
4.271859	227.407719	5.232486
3.657977	222.400471	5.237491
3.940593	220.559696	5.242496
3.770091	218.406665	5.247501
3.796869	223.625950	5.252506
3.692993	226.701615	5.257510
3.785270	239.832588	5.262515
4.037063	238.328799	5.267520
3.911164	241.290838	5.272525
4.088260	238.482582	5.277530
4.218895	229.562982	5.282534
3.724218	230.734843	5.287539
4.047546	226.356776	5.292544
3.887214	230.444121	5.297549
3.952085	231.076454	5.302554
4.249097	239.031390	5.307558
3.496258	236.266685	5.312563
3.951347	241.678711	5.317568
3.914679	233.167964	5.322573
4.119951	248.179566	5.327578
4.086537	236.162939	5.332582
3.943559	245.629026	5.337587
4.152023	239.465535	5.342592
3.970803	242.670302	5.347597
3.990691	243.879103	5.352602
4.287758	240.574450	5.357606
3.938175	238.379697	5.362611
4.018778	225.984664	5.367616
4.051476	232.870295	5.372621
4.071166	238.119161	5.377626
3.997607	230.506321	5.382630
4.007905	241.891048	5.387635
4.253186	233.690736	5.392640
4.316526	231.384238	5.397645
4.421430	239.840474	5.402650
4.395413	239.395484	5.407654
4.042301	238.685053	5.412659
4.048816	239.199923	5.417664
4.403964	238.066012	5.422669
4.075678	244.507988	5.427674
4.481237	239.873511	5.432678
4.316106	245.840841	5.437683
4.354948	233.793983	5.442688
4.522850	243.588145	5.447693
3.986019	243.751024	5.452698
4.476505	235.822575	5.457702
4.300771	242.417966	5.462707
4.606185	236.783536	5.467712
4.066050	236.478703	5.472717
4.345624	236.435377	5.477722
4.407837	240.241307	5.482726
4.368229	232.895257	5.487731
4.181520	240.647103	5.492736
4.276768	254.910227	5.497741
4.342212	264.043323	5.502746
4.746141	257.096433	5.507750
4.541782	261.775924	5.512755
4.383958	257.846080	5.517760
4.540831	256.470961	5.522765
4.897883	263.533888	5.527770
4.771258	265.372932	5.532774
4.511671	264.752340	5.537779
4.502147	249.970077	5.542784
4.468076	257.489361	5.547789
4.474965	258.757134	5.552794
4.513633	258.203997	5.557798
4.744078	258.025954	5.562803
4.644637	261.876040	5.567808
4.743267	250.512712	5.572813
4.561037	262.810099	5.577818
4.634611	258.686042	5.582822
4.600053	264.819706	5.587827
4.755675	260.372832	5.592832
4.853245	258.845597	5.597837
4.700247	266.914903	5.602842
4.953304	259.026574	5.607846
4.861666	260.562783	5.612851
4.670938	261.987873	5.617856
4.849191	258.154396	5.622861
4.716765	262.164639	5.627866
5.078275	262.883662	5.632870
4.506608	262.618538	5.637875
4.661255	260.766047	5.642880
4.748298	260.999466	5.647885
4.573044	259.989264	5.652890
4.926814	256.466976	5.657894
5.077525	261.198749	5.662899
4.873290	259.414790	5.667904
4.998077	255.115084	5.672909
4.728337	258.722770	5.677914
5.021053	265.194613	5.682918
4.737712	263.419806	5.687923
4.703224	260.195245	5.692928
4.895021	261.000802	5.697933
4.862166	263.942032	5.702938
4.732563	252.873660	5.707942
4.696320	254.230404	5.712947
4.805842	258.168175	5.717952
4.911397	268.753491	5.722957
5.019974	279.082084	5.727962
5.298501	279.206597	5.732966
5.109219	288.458458	5.737971
5.002141	279.284784	5.742976
5.374900	280.660106	5.747981
5.071122	281.814901	5.752986
5.353748	269.881920	5.757990
5.301820	268.953754	5.762995
4.770833	263.427396	5.768000
5.161208	271.798072	5.773005
4.975737	278.360191	5.778010
5.441404	287.060832	5.783014
5.328657	286.439522	5.788019
5.013443	281.528122	5.793024
5.074780	274.223284	5.798029
5.167808	288.211539	5.803034
5.308463	282.188303	5.808038
5.332253	292.314973	5.813043
5.106082	289.382838	5.818048
5.427264	280.512638	5.823053
4.980072	284.030901	5.828058
5.391545	288.579715	5.833062
5.366342	288.008049	5.838067
5.128978	285.811636	5.843072
5.498563	283.887713	5.848077
5.278711	294.900190	5.853082
5.601907	286.931328	5.858086
5.607445	286.829431	5.863091
5.187198	283.190372	5.868096
5.432897	293.019905	5.873101
5.248831	289.483275	5.878106
5.331145	288.670246	5.883110
5.140720	285.204208	5.888115
5.383343	288.539141	5.893120
5.524758	283.139035	5.898125
5.202507	290.586145	5.903130
5.359245	282.193956	5.908134
5.011791	285.598616	5.913139
5.499261	282.419332	5.918144
5.279208	284.617768	5.923149
5.412529	298.621903	5.928154
5.741940	300.946760	5.933158
5.818333	299.543039	5.938163
5.546808	283.137433	5.943168
5.459953	279.822948	5.948173
5.335148	285.524588	5.953178
5.643126	293.414567	5.958182
5.779735	306.203335	5.963187
5.899709	304.242344	5.968192
5.665211	286.881859	5.973197
5.374448	290.303003	5.978202
5.829188	294.921010	5.983206
5.531811	305.138820	5.988211
5.711982	307.331892	5.993216
5.821923	308.716499	5.998221
5.721305	311.918220	6.003226
5.883809	306.571770	6.008230
5.730692	296.013225	6.013235
5.544620	290.914039	6.018240
5.630109	291.897498	6.023245
5.348264	291.416409	6.028250
5.797776	301.562221	6.033254
5.889178	308.084406	6.038259
5.760311	301.116051	6.043264
6.149817	303.725775	6.048269
5.686164	294.076109	6.053274
6.038774	289.446699	6.058278
5.666273	289.995274	6.063283
5.492985	288.266603	6.068288
5.547515	283.000246	6.073293
5.554845	286.387632	6.078298
5.349978	283.293996	6.083302
5.524756	289.841157	6.088307
5.631786	297.904792	6.093312
5.847359	293.603596	6.098317
5.989944	297.868417	6.103322
5.619288	282.721581	6.108326
5.504179	288.538770	6.113331
5.333884	289.185573	6.118336
5.814848	303.094457	6.123341
5.734110	313.269051	6.128346
5.905097	305.747815	6.133350
5.825222	289.328182	6.138355
5.490369	284.248998	6.143360
5.742653	285.842392	6.148365
5.613189	286.498656	6.153370
5.715660	281.816447	6.158374
5.723571	283.185301	6.163379
5.647107	291.669801	6.168384
5.762716	277.431170	6.173389
5.623046	295.929133	6.178394
5.660593	296.761872	6.183398
5.680531	299.157058	6.188403
5.829027	297.387777	6.193408
5.998654	291.299916	6.198413
5.494105	293.346499	6.203418
5.758209	285.016685	6.208422
5.671769	292.018963	6.213427
5.447868	291.835732	6.218432
5.749026	288.071696	6.223437
6.021015	301.487941	6.228442
5.643640	286.702810	6.233446
5.770168	291.140969	6.238451
5.690490	292.763902	6.243456
5.777660	292.959338	6.248461
5.145978	295.247174	6.253466
5.485270	284.026685	6.258470
5.706356	297.852643	6.263475
5.934284	304.426335	6.268480
5.769242	291.563309	6.273485
5.588202	301.051171	6.278490
5.820175	294.390463	6.283494
5.565421	295.676830	6.288499
5.572647	286.409426	6.293504
5.698819	291.132373	6.298509
5.650391	306.784628	6.303514
5.785130	289.012316	6.308518
5.614764	295.160808	6.313523
5.844620	296.162918	6.318528
5.611579	280.175259	6.323533
5.733648	286.243416	6.328538
5.609753	284.766479	6.333542
5.889580	281.005767	6.338547
5.584790	286.112182	6.343552
5.848555	274.602906	6.348557
5.651032	289.190047	6.353562
5.777715	283.887146	6.358566
5.833245	283.052978	6.363571
5.467961	290.389731	6.368576
5.658867	291.261866	6.373581
5.850087	286.148229	6.378586
5.385298	282.629999	6.383590
5.612763	284.126017	6.388595
5.693905	293.161773	6.393600
5.521319	288.743847	6.398605
5.769174	302.407455	6.403610
5.997912	302.859255	6.408614
5.913622	284.766715	6.413619
5.712418	290.423305	6.418624
5.785823	284.923059	6.423629
5.667549	288.494513	6.428634
5.525664	276.051829	6.433638
5.917264	284.118606	6.438643
5.277892	292.997629	6.443648
6.055191	287.666193	6.448653
5.768148	288.362810	6.453658
5.621413	287.120380	6.458662
5.718197	288.238119	6.463667
5.749276	286.142277	6.468672
6.170754	285.687722	6.473677
5.663614	283.482694	6.478682
5.317579	282.761668	6.483686
5.719697	288.871643	6.488691
5.450699	288.205059	6.493696
5.545725	287.693766	6.498701
5.476482	290.741904	6.503706
5.670397	286.453574	6.508710
5.829060	283.429886	6.513715
5.515213	298.291405	6.518720
5.771913	284.834382	6.523725
5.799683	284.213340	6.528730
5.538027	284.083443	6.533734
5.381612	287.195772	6.538739
5.968417	295.213178	6.543744
5.715864	282.022105	6.548749
5.468928	289.751712	6.553754
5.772834	287.565936	6.558758
5.839407	282.221775	6.563763
5.140745	286.851687	6.568768
5.793769	293.836908	6.573773
6.136683	304.312524	6.578778
5.894605	302.110516	6.583782
5.479109	288.539854	6.588787
5.928493	286.935694	6.593792
5.985875	286.256259	6.598797
5.824073	287.278220	6.603802
5.554664	287.007164	6.608806
5.689537	279.899679	6.613811
5.428924	286.473500	6.618816
5.918525	282.464994	6.623821
5.775384	280.250749	6.628826
5.601788	286.213082	6.633830
5.703405	288.168450	6.638835
5.718697	288.065034	6.643840
5.752261	283.358752	6.648845
5.901387	290.618577	6.653850
5.778321	282.339554	6.658854
5.864727	283.848044	6.663859
5.632819	289.174063	6.668864
5.966748	289.751851	6.673869
5.653418	283.429145	6.678874
5.505885	282.066619	6.683878
5.679627	274.823373	6.688883
5.270254	283.521050	6.693888
5.514755	286.314697	6.698893
5.505971	289.562226	6.703898
5.803987	288.222075	6.708902
5.843621	290.025745	6.713907
5.649541	288.509116	6.718912
5.727685	285.963028	6.723917
5.870753	289.047711	6.728922
5.663548	279.266377	6.733926
6.002256	289.793259	6.738931
5.510098	286.994286	6.743936
5.952088	286.457445	6.748941
5.866331	296.379714	6.753946
5.966627	290.473488	6.758950
5.550084	287.786126	6.763955
5.439200	289.869491	6.768960
5.845123	288.155041	6.773965
6.151208	289.543908	6.778970
6.104856	288.181446	6.783974
5.903230	288.893238	6.788979
5.838191	273.885484	6.793984
5.745865	251.716222	6.798989
5.533624	257.580161	6.803994
5.486173	255.844556	6.808998
5.572073	268.868978	6.814003
5.874679	275.285503	6.819008
5.875587	263.649484	6.824013
5.669941	256.110981	6.829018
5.494565	256.628863	6.834022
5.595827	262.937529	6.839027
5.600701	274.667964	6.844032
5.722697	272.092905	6.849037
5.555048	277.522808	6.854042
5.616849	279.579285	6.859046
5.970916	278.252554	6.864051
5.951313	274.196784	6.869056
5.441860	267.186460	6.874061
5.629415	262.971891	6.879066
5.555159	271.114358	6.884070
5.662124	276.950750	6.889075
5.382577	286.235645	6.894080
5.614763	274.860998	6.899085
5.587297	279.886269	6.904090
5.609552	275.074184	6.909094
5.701341	279.751862	6.914099
5.206445	278.785099	6.919104
5.744298	279.236225	6.924109
5.665074	282.096094	6.929114
5.841725	276.750614	6.934118
5.947791	275.168272	6.939123
5.721476	288.601982	6.944128
5.818057	282.408441	6.949133
5.987665	284.505079	6.954138
5.692504	287.287840	6.959142
5.535471	279.631028	6.964147
5.450441	280.811876	6.969152
5.383080	278.380191	6.974157
5.728529	282.926629	6.979162
5.425203	281.034711	6.984166
5.603158	283.585623	6.989171
5.689024	288.318008	6.994176
5.560919	275.752959	6.999181
5.354594	274.719120	7.004186
5.609628	284.528212	7.009190
5.918157	281.455881	7.014195
5.658317	278.124037	7.019200
5.584464	276.028715	7.024205
5.691144	281.792388	7.029210
5.558899	286.081013	7.034214
5.818044	281.026404	7.039219
5.681242	286.926062	7.044224
5.945980	285.262068	7.049229
5.597987	281.811073	7.054234
5.738646	278.780698	7.059238
5.699980	276.838083	7.064243
5.659258	285.867499	7.069248
5.893510	273.790189	7.074253
5.483945	281.371110	7.079258
5.517234	273.570776	7.084262
5.784969	274.699862	7.089267
5.265292	282.993941	7.094272
5.642105	274.330214	7.099277
5.657063	282.825785	7.104282
5.485138	288.019080	7.109286
5.798653	276.688715	7.114291
5.356478	288.181885	7.119296
5.864607	277.555198	7.124301
5.599037	278.394002	7.129306
5.765936	280.978272	7.134310
5.797030	274.136880	7.139315
5.366019	279.164871	7.144320
5.614679	272.783142	7.149325
5.360791	283.914805	7.154330
5.853118	304.035429	7.159334
6.451232	308.086961	7.164339
5.955809	290.808225	7.169344
5.674532	287.046290	7.174349
6.004867	285.593541	7.179354
5.670195	290.442023	7.184358
5.722366	280.677251	7.189363
5.800391	286.299856	7.194368
6.031457	285.311809	7.199373
6.105186	290.308672	7.204378
5.751144	283.736046	7.209382
5.878893	289.376220	7.214387
5.989865	283.126655	7.219392
6.038464	281.148306	7.224397
5.814215	276.516968	7.229402
5.531043	265.184602	7.234406
5.343670	262.901317	7.239411
5.655295	273.144509	7.244416
5.678524	272.173004	7.249421
5.741210	277.389878	7.254426
5.401215	289.455587	7.259430
5.865760	277.465804	7.264435
5.560516	283.910534	7.269440
5.826747	280.759368	7.274445
5.751965	293.811991	7.279450
5.602654	285.932515	7.284454
5.748603	284.970376	7.289459
5.510814	290.483969	7.294464
5.976564	286.801873	7.299469
5.575130	271.688312	7.304474
5.659248	286.348657	7.309478
5.863069	286.472147	7.314483
5.784214	281.732750	7.319488
5.724830	260.988340	7.324493
5.496413	267.481212	7.329498
5.433234	271.262380	7.334502
5.916583	280.400019	7.339507
5.650047	287.028545	7.344512
5.726342	274.675277	7.349517
5.574524	274.809847	7.354522
5.834257	282.511184	7.359526
5.730490	275.719262	7.364531
5.343510	277.146435	7.369536
5.723184	280.982038	7.374541
5.645530	277.055526	7.379546
6.056326	288.532948	7.384550
5.958791	279.351461	7.389555
5.323372	262.534304	7.394560
5.501367	263.503358	7.399565
5.859346	279.003729	7.404570
5.670029	280.608931	7.409574
5.605179	266.082037	7.414579
5.284994	281.830365	7.419584
5.846289	272.698160	7.424589
5.586736	291.942435	7.429594
5.770127	293.910380	7.434598
5.899854	290.236310	7.439603
5.747851	292.455789	7.444608
5.911695	279.712405	7.449613
5.491504	273.175391	7.454618
5.492333	279.275077	7.459622
5.837645	283.666515	7.464627
5.817794	291.683464	7.469632
5.919356	268.667758	7.474637
5.596754	266.740878	7.479642
5.396598	266.873484	7.484646
5.756080	268.649498	7.489651
5.649593	288.091395	7.494656
6.307361	284.303475	7.499661
5.857122	270.121314	7.504666
5.637706	268.257462	7.509670
5.832688	264.620692	7.514675
5.353164	280.286261	7.519680
5.581250	261.031487	7.524685
5.571629	258.663580	7.529690
5.361584	269.785244	7.534694
5.579680	267.081330	7.539699
5.643509	281.374677	7.544704
5.759708	284.605909	7.549709
5.967534	288.294266	7.554714
5.814040	278.919015	7.559718
5.822922	266.127003	7.564723
5.277478	271.935260	7.569728
5.830683	268.049729	7.574733
5.588298	267.749156	7.579738
5.550954	286.101465	7.584742
6.008825	279.525811	7.589747
5.507261	269.815623	7.594752
5.362895	273.267753	7.599757
5.309545	278.613423	7.604762
5.692052	285.571158	7.609766
6.173210	290.302108	7.614771
5.794453	290.715618	7.619776
5.764437	288.407829	7.624781
5.891923	283.642632	7.629786
5.606670	271.541807	7.634790
5.263957	263.964532	7.639795
5.361494	273.864577	7.644800
5.690878	273.025736	7.649805
5.865592	283.559165	7.654810
5.332060	288.910000	7.659814
5.942006	289.659945	7.664819
5.604826	291.379917	7.669824
5.644692	284.571956	7.674829
5.752014	287.978574	7.679834
5.503260	289.485465	7.684838
6.195250	282.205818	7.689843
5.873963	291.367503	7.694848
6.025034	285.734943	7.699853
5.535760	269.451836	7.704858
5.666377	255.849954	7.709862
6.005862	257.319038	7.714867
5.588996	265.353497	7.719872
5.803560	262.640642	7.724877
5.607770	258.542706	7.729882
5.413766	259.446296	7.734886
5.620124	264.571195	7.739891
5.473919	279.846352	7.744896
5.592452	283.982038	7.749901
5.954843	290.015942	7.754906
5.735430	289.860486	7.759910
5.986092	271.329836	7.764915
5.483758	272.806607	7.769920
5.611563	271.689108	7.774925
5.854548	260.366571	7.779930
5.353279	271.932206	7.784934
5.685730	269.460418	7.789939
5.596213	290.547963	7.794944
5.943425	288.567412	7.799949
5.738853	277.165854	7.804954
5.609912	275.920654	7.809958
5.623282	278.588938	7.814963
5.778642	289.887836	7.819968
5.628434	284.444551	7.824973
5.559699	286.904161	7.829978
5.630058	288.567007	7.834982
5.947038	285.740128	7.839987
5.737934	278.686200	7.844992
5.596392	271.988745	7.849997
5.745419	290.166511	7.855002
5.875918	285.590667	7.860006
5.722317	265.496824	7.865011
5.556020	271.223903	7.870016
5.571421	262.970785	7.875021
5.557016	271.885367	7.880026
5.718830	276.492032	7.885030
6.043721	281.639609	7.890035
5.338620	276.425088	7.895040
5.800390	278.128230	7.900045
6.013913	265.706147	7.905050
5.523870	267.895998	7.910054
5.306505	266.003353	7.915059
5.208822	273.197196	7.920064
5.900464	286.548091	7.925069
6.051218	283.693310	7.930074
5.852519	286.913461	7.935078
5.896161	272.983427	7.940083
5.495104	261.833930	7.945088
5.582916	265.673844	7.950093
5.800237	265.592756	7.955098
5.425468	267.033846	7.960102
5.965021	260.442318	7.965107
5.446058	264.737366	7.970112
5.567229	271.315013	7.975117
5.553844	280.118711	7.980122
5.801489	283.696878	7.985139
6.159058	278.279995	7.990157
5.489661	266.219478	7.995174
5.744101	278.042071	8.000192
5.692074	279.088577	8.005210
5.377113	274.877721	8.010227
6.053917	276.296717	8.015245
5.570831	289.101945	8.020262
5.666019	286.086324	8.025280
5.635729	286.637168	8.030298
5.797420	293.232711	8.035315
5.667962	286.424286	8.040333
6.160776	286.344605	8.045350
5.931060	284.408306	8.050368
5.867311	264.638959	8.055386
5.521605	264.614098	8.060403
5.468194	259.661974	8.065421
5.509293	274.805943	8.070438
5.640781	282.365495	8.075456
6.098753	286.967881	8.080474
5.861343	287.803424	8.085491
6.287868	286.023712	8.090509
5.608212	283.573676	8.095526
5.533032	269.561973	8.100544
5.757336	278.580750	8.105562
5.808446	286.531494	8.110579
5.719838	291.891132	8.115597
5.627854	301.864832	8.120614
5.849794	294.228563	8.125632
6.050828	288.208079	8.130650
5.817928	286.654107	8.135667
5.912197	285.260623	8.140685
6.050117	291.717863	8.145702
5.972997	287.356370	8.150720
6.020640	288.343179	8.155738
5.632312	279.482880	8.160755
5.894864	280.641344	8.165773
5.688590	284.207969	8.170790
5.813565	292.604782	8.175808
5.999405	286.823336	8.180826
5.767002	290.261494	8.185843
6.042635	294.980630	8.190861
6.227432	294.279912	8.195878
5.869639	286.995826	8.200896
5.914377	289.942735	8.205914
5.757930	284.088358	8.210931
6.211656	283.497239	8.215949
5.682089	280.859743	8.220966
5.511333	290.792056	8.225984
5.869853	288.603233	8.231002
5.789228	292.109273	8.236019
6.002644	291.258940	8.241037
6.181760	301.064205	8.246054
6.128014	295.499931	8.251072
6.405320	282.332691	8.256090
5.656970	285.986872	8.261107
5.705872	280.605425	8.266125
5.893336	285.688561	8.271142
5.926279	280.795566	8.276160
5.755489	294.858605	8.281178
5.882349	298.417544	8.286195
5.982178	291.036961	8.291213
6.333369	289.609786	8.296230
5.977070	288.103427	8.301248
6.298319	290.966261	8.306266
5.774422	298.798266	8.311283
5.909425	297.616177	8.316301
6.005342	288.011484	8.321318
6.037032	295.245771	8.326336
6.357351	289.705304	8.331354
5.992408	293.728957	8.336371
5.569933	289.228741	8.341389
5.797343	296.953235	8.346406
5.752198	298.989540	8.351424
5.878617	289.746150	8.356442
5.939376	299.566686	8.361459
5.892993	295.528591	8.366477
5.961639	291.926999	8.371494
5.601931	291.894850	8.376512
6.247754	303.318870	8.381530
6.364640	316.990017	8.386547
6.640781	311.712028	8.391565
6.386744	295.768503	8.396582
6.132656	296.818069	8.401600
6.093481	286.060515	8.406618
5.887208	288.554227	8.411635
5.891338	283.769853	8.416653
5.977433	288.035686	8.421670
5.934187	290.977360	8.426688
6.391718	296.889405	8.431706
6.274629	299.769998	8.436723
6.110208	292.326421	8.441741
6.067030	295.776142	8.446758
5.699988	299.721232	8.451776
6.130428	302.724848	8.456794
6.293501	319.172074	8.461811
6.276405	313.005673	8.466829
6.494395	311.561368	8.471846
6.281202	313.355609	8.476864
6.303102	301.682869	8.481882
5.888263	295.594180	8.486899
5.979728	306.438675	8.491917
6.577981	306.307865	8.496934
6.234566	317.949028	8.501952
6.376798	307.229485	8.506970
6.283188	319.383992	8.511987
6.444643	313.622112	8.517005
6.271959	294.055876	8.522022
5.874791	299.880102	8.527040
6.255517	300.105035	8.532058
6.042152	311.224200	8.537075
6.257084	310.550345	8.542093
6.314207	321.870387	8.547110
6.410253	329.539613	8.552128
6.616688	325.121340	8.557146
6.503913	317.660244	8.562163
6.305684	306.204802	8.567181
5.979593	308.215426	8.572199
6.044067	319.587967	8.577216
6.344399	314.893158	8.582234
6.121460	315.439286	8.587251
6.160617	318.431247	8.592269
6.627769	313.868248	8.597287
6.019093	324.048633	8.602304
6.105069	315.723506	8.607322
5.995380	321.121147	8.612339
6.020473	322.947713	8.617357
6.464707	322.099309	8.622375
6.378259	310.736907	8.627392
6.232500	315.789887	8.632410
6.275832	314.707273	8.637427
6.599270	320.678071	8.642445
6.342558	323.340578	8.647463
6.239873	317.723959	8.652480
6.330701	318.082387	8.657498
6.024414	318.332239	8.662515
6.344770	319.775181	8.667533
6.721917	308.343755	8.672551
6.618348	324.595829	8.677568
6.445386	320.123025	8.682586
6.438537	316.340688	8.687603
6.331453	316.101958	8.692621
6.670754	310.444926	8.697639
6.563388	320.178048	8.702656
6.954308	314.560312	8.707674
6.691537	313.515890	8.712691
6.457930	318.077647	8.717709
6.517561	318.822764	8.722727
6.028645	320.196057	8.727744
6.024167	319.155599	8.732762
6.328916	316.104189	8.737779
6.455176	312.951189	8.742797
6.733015	315.183347	8.747815
6.246432	322.794969	8.752832
6.398010	313.266798	8.757850
6.420158	319.486467	8.762867
6.364256	335.980424	8.767885
6.972052	336.649661	8.772903
6.357651	330.910750	8.777920
6.740404	331.147990	8.782938
6.710229	326.122806	8.787955
6.253361	324.335472	8.792973
6.634114	325.579672	8.797991
6.140529	333.937120	8.803008
6.526449	337.247459	8.808026
6.691975	342.801062	8.813043
6.739812	340.834166	8.818061
6.903799	335.355893	8.823079
6.667386	341.467511	8.828096
6.618507	325.526729	8.833114
6.197992	325.658674	8.838131
6.328690	327.314172	8.843149
6.660297	329.989217	8.848167
6.577606	334.846200	8.853184
6.689687	338.028771	8.858202
6.871893	343.365194	8.863219
6.494915	337.245350	8.868237
6.663546	344.287931	8.873255
6.631471	341.352073	8.878272
6.767604	340.264475	8.883290
6.753837	336.849265	8.888307
6.627503	338.118772	8.893325
6.997387	331.166315	8.898343
7.086119	342.131172	8.903360
6.706008	332.013622	8.908378
6.800466	318.912692	8.913395
6.391341	321.706221	8.918413
6.914107	327.153708	8.923431
6.451509	330.839142	8.928448
6.763419	339.339408	8.933466
7.147520	335.385750	8.938483
6.622529	331.501056	8.943501
6.897142	315.383690	8.948519
6.653042	314.203824	8.953536
6.598090	317.036878	8.958554
6.867873	324.262507	8.963571
6.695111	336.495617	8.968589
7.141894	338.035635	8.973607
7.059364	326.533764	8.978624
6.940544	327.742143	8.983642
6.870441	317.901365	8.988659
6.652493	324.928393	8.993677
6.948643	310.637947	8.998695
6.468670	308.447136	9.003712
6.538165	311.702602	9.008730
6.889241	320.341920	9.013747
6.661763	317.562714	9.018765
6.729209	329.834155	9.023783
6.836386	338.120157	9.028800
7.060289	344.523005	9.033818
6.997301	336.915302	9.038835
6.627946	335.862228	9.043853
6.828958	327.105796	9.048871
6.752529	341.463433	9.053888
6.478457	338.647299	9.058906
6.766407	339.688210	9.063923
6.647289	344.699183	9.068941
6.989227	344.033954	9.073959
6.939333	342.524063	9.078976
6.764456	339.102381	9.083994
6.963403	338.112295	9.089011
6.965878	347.755750	9.094029
6.673766	338.041040	9.099047
7.014027	342.011707	9.104064
6.969972	344.006823	9.109082
7.444649	336.157625	9.114099
7.050900	340.700143	9.119117
6.868713	343.344738	9.124135
7.207342	343.737164	9.129152
6.957166	346.796268	9.134170
6.968142	343.714857	9.139187
7.011322	355.766044	9.144205
6.971887	351.300843	9.149223
6.997096	339.851614	9.154240
7.142867	340.015304	9.159258
7.367228	335.452233	9.164275
7.153240	348.884602	9.169293
7.160622	341.657240	9.174311
7.375698	341.125366	9.179328
6.904024	334.095664	9.184346
6.629497	325.776171	9.189363
6.520808	336.443576	9.194381
6.874927	337.928597	9.199399
6.622422	349.710253	9.204416
6.533803	351.027534	9.209434
6.689431	349.009142	9.214451
6.968367	349.688558	9.219469
6.818324	354.757995	9.224487
7.203507	358.046363	9.229504
7.153750	370.377104	9.234522
7.564975	359.858632	9.239539
7.188191	355.272394	9.244557
7.248526	349.690341	9.249575
7.020632	342.398630	9.254592
6.864839	348.702815	9.259610
7.174305	345.628576	9.264627
7.265783	356.018687	9.269645
7.602635	346.710948	9.274663
7.273324	351.095120	9.279680
7.079573	347.360810	9.284698
6.959085	345.918712	9.289715
6.728587	350.890227	9.294733
7.058364	344.824433	9.299751
7.594563	357.833910	9.304768
6.792958	359.795506	9.309786
7.457158	350.935388	9.314803
7.213487	358.304088	9.319821
7.522145	359.625784	9.324839
7.389056	343.827477	9.329856
6.942711	351.142528	9.334874
7.338574	342.907987	9.339891
7.110651	347.434154	9.344909
7.521177	337.670003	9.349927
7.101241	342.626831	9.354944
6.769056	349.554896	9.359962
7.279046	355.752268	9.364979
7.638780	362.900796	9.369997
7.843152	363.891608	9.375015
7.536693	351.866037	9.380032
6.924552	348.016998	9.385050
7.369923	332.068681	9.390067
7.386701	343.467597	9.395085
6.985091	341.494942	9.400103
7.446006	345.560427	9.405120
6.894345	347.549375	9.410138
7.405443	343.190954	9.415155
7.623717	357.859307	9.420173
7.649824	357.016045	9.425191
7.220457	344.485779	9.430208
7.405707	341.383547	9.435226
7.554755	341.407879	9.440243
7.154444	349.236442	9.445261
7.240511	349.068619	9.450279
7.247862	341.689791	9.455296
7.402689	357.952153	9.460314
7.304129	365.254084	9.465331
7.382160	358.921385	9.470349
7.398421	363.444249	9.475367
7.550030	365.402593	9.480384
7.641056	368.787253	9.485402
7.553193	357.686960	9.490419
7.306220	344.718062	9.495437
6.977825	360.528671	9.500455
7.314302	366.295494	9.505472
7.334009	366.706019	9.510490
7.730799	369.875824	9.515507
7.735172	365.460600	9.520525
7.387337	370.115891	9.525543
7.713989	363.245889	9.530560
7.449596	359.030295	9.535578
7.638241	359.401894	9.540595
7.728598	357.923811	9.545613
7.486774	345.133983	9.550631
7.750687	339.084758	9.555648
7.379114	347.811359	9.560666
7.545333	338.296673	9.565683
7.512236	334.625711	9.570701
6.961868	344.718138	9.575719
7.372636	357.775545	9.580736
7.290647	370.209128	9.585754
7.547502	368.654631	9.590771
7.747672	368.213436	9.595789
7.155371	365.951748	9.600807
7.642609	360.991154	9.605824
7.332314	367.328868	9.610842
7.636995	366.341252	9.615859
7.774103	364.373077	9.620877
7.627921	369.202087	9.625895
7.586527	368.012747	9.630912
7.263934	374.784702	9.635930
7.455574	362.536412	9.640947
7.355682	371.861320	9.645965
7.548072	372.011441	9.650983
7.594074	370.508707	9.656000
7.795996	388.158560	9.661018
7.474059	389.127182	9.666035
7.985727	387.697103	9.671053
7.980501	381.096506	9.676071
7.854146	367.225231	9.681088
7.785334	372.121087	9.686106
7.567526	367.746767	9.691123
7.742163	365.558164	9.696141
7.593995	370.510554	9.701159
7.764485	355.662155	9.706176
7.634957	375.720867	9.711194
7.546197	369.836989	9.716211
7.949455	382.094049	9.721229
7.692368	377.378721	9.726247
8.060468	376.564258	9.731264
7.659403	369.435190	9.736282
7.795796	377.022420	9.741299
7.794061	366.221120	9.746317
7.472958	376.426185	9.751335
8.138494	382.432099	9.756352
7.764280	379.546348	9.761370
7.416028	377.123592	9.766387
8.131226	382.803053	9.771405
7.844449	389.358009	9.776423
8.066957	388.503100	9.781440
7.779561	373.842736	9.786458
7.782262	374.483116	9.791475
7.948483	383.567791	9.796493
7.801436	394.616725	9.801511
7.961881	393.228708	9.806528
7.814755	389.468196	9.811546
7.749795	396.282093	9.816563
8.155816	390.400064	9.821581
8.130529	398.690940	9.826599
7.541011	388.508137	9.831616
7.863558	386.855052	9.836634
7.998446	394.887470	9.841651
8.383979	398.762742	9.846669
8.047680	389.752282	9.851687
7.932865	377.390758	9.856704
8.024924	379.566647	9.861722
7.868544	373.573382	9.866739
7.537383	373.319049	9.871757
7.678671	387.365128	9.876775
8.303524	385.788046	9.881792
8.232229	393.937767	9.886810
8.302650	386.574346	9.891827
8.143326	370.218396	9.896845
7.598649	373.844038	9.901863
7.641796	383.395978	9.906880
8.048314	384.857065	9.911898
8.094196	389.580442	9.916915
8.025473	394.084990	9.921933
8.406476	400.819987	9.926951
8.313640	398.382705	9.931968
8.056953	386.879510	9.936986
7.952356	389.363717	9.942003
8.416518	387.366706	9.947021
7.764111	387.070877	9.952039
8.072338	384.337634	9.957056
8.135609	392.128750	9.962074
8.338546	398.556971	9.967091
8.227102	386.721909	9.972109
7.990314	391.441962	9.977127
8.291162	387.002663	9.982144
7.576311	389.932161	9.987162
8.138440	388.929705	9.992179
8.418523	394.803142	9.997197
7.773725	410.719861	10.002215
8.154976	402.632728	10.007232
8.289181	403.050672	10.012250
7.923128	398.809874	10.017267
8.174802	400.989315	10.022285
8.108910	409.665196	10.027303
8.022442	395.134469	10.032320
8.353082	401.672190	10.037338
8.176476	400.636437	10.042355
8.209086	393.843761	10.047373
8.286741	396.602535	10.052391
8.550362	399.477514	10.057408
8.283917	396.799032	10.062426
8.052448	392.805511	10.067443
8.019402	388.604381	10.072461
8.209807	403.204530	10.077479
7.878194	403.638199	10.082496
8.468448	393.855501	10.087514
8.075441	402.683291	10.092531
8.587890	389.643455	10.097549
8.436304	403.353313	10.102567
8.088277	394.278408	10.107584
8.441948	392.601543	10.112602
8.274536	398.408962	10.117619
9.039029	391.246727	10.122637
8.529214	404.043577	10.127655
8.646091	400.200935	10.132672
8.877208	403.939313	10.137690
8.268189	395.763380	10.142707
8.782796	393.802694	10.147725
8.119990	398.907800	10.152743
8.201063	400.388003	10.157760
8.601584	401.872116	10.162778
8.189028	402.542439	10.167795
8.488520	405.307698	10.172813
8.398838	404.902163	10.177831
8.516061	397.588252	10.182848
8.563673	397.568420	10.187866
8.415108	401.602587	10.192883
8.471897	402.045207	10.197901
7.924070	413.465807	10.202919
7.558430	406.690953	10.207936
8.249630	407.981493	10.212954
8.022167	407.307091	10.217971
8.453305	410.206480	10.222989
8.314321	420.525219	10.228007
8.374969	433.135445	10.233024
8.663157	428.571880	10.238042
8.457203	435.556060	10.243059
8.846309	427.584452	10.248077
8.696405	440.069683	10.253095
8.365097	438.180741	10.258112
9.180110	433.683465	10.263130
8.414583	421.211796	10.268147
8.379896	407.676494	10.273165
8.498808	427.134876	10.278183
8.494099	430.405072	10.283200
8.445742	424.966144	10.288218
8.384684	429.106607	10.293235
8.371345	422.696598	10.298253
8.328319	429.260951	10.303271
8.331498	431.510643	10.308288
8.596238	426.802413	10.313306
8.838938	429.185217	10.318323
8.646075	421.960599	10.323341
8.462004	427.941027	10.328359
8.594360	421.580913	10.333376
8.819830	418.223109	10.338394
8.906927	431.390921	10.343411
8.312981	413.382768	10.348429
8.561818	422.306285	10.353447
8.421542	424.089184	10.358464
8.933335	424.763905	10.363482
8.778410	430.398985	10.368499
8.815974	432.513941	10.373517
8.608339	431.527197	10.378535
8.201345	432.193499	10.383552
8.847708	436.776060	10.388570
8.900487	449.516904	10.393587
9.365261	456.778497	10.398605
9.037713	443.304544	10.403623
8.712875	430.615938	10.408640
8.963872	421.962125	10.413658
8.587585	431.986474	10.418675
8.317523	434.404935	10.423693
8.668517	443.426160	10.428711
8.501141	448.520412	10.433728
8.957712	450.589065	10.438746
9.018573	449.945506	10.443763
8.705957	445.525971	10.448781
9.198135	455.282578	10.453799
8.722523	452.485183	10.458816
9.265869	450.567351	10.463834
9.045424	451.251944	10.468851
9.056357	438.634124	10.473869
8.864013	438.923039	10.478887
8.736847	433.729898	10.483904
9.002841	438.488441	10.488922
8.588995	439.600758	10.493939
9.077389	447.515046	10.498957
8.993642	451.062627	10.503975
8.854011	447.064262	10.508992
9.466213	450.481396	10.514010
9.089587	452.629286	10.519027
8.788814	434.146296	10.524045
8.981288	439.477993	10.529063
8.649614	447.942822	10.534080
9.058267	445.351718	10.539098
8.995590	448.239641	10.544115
8.836473	433.821174	10.549133
9.178271	444.131339	10.554151
8.902784	455.686280	10.559168
8.859864	448.567688	10.564186
8.961551	450.518035	10.569203
8.920766	446.185558	10.574221
9.147555	445.749683	10.579239
8.983575	453.244863	10.584256
9.075072	446.708074	10.589274
8.961295	458.783768	10.594291
8.910513	450.710233	10.599309
9.079139	450.068829	10.604327
8.843233	451.740394	10.609344
9.060307	453.843182	10.614362
9.004728	447.026349	10.619379
9.035512	450.941088	10.624397
9.149051	452.706562	10.629415
8.999382	461.515427	10.634432
9.346152	464.661481	10.639450
9.472838	469.214515	10.644467
9.211798	458.930037	10.649485
9.189921	444.578552	10.654503
9.184848	452.853684	10.659520
9.154668	456.178341	10.664538
9.262419	458.187702	10.669555
9.014213	456.446759	10.674573
9.318215	462.168179	10.679591
9.545693	474.894463	10.684608
9.458784	457.182846	10.689626
9.308728	454.789177	10.694643
9.181137	454.294874	10.699661
9.073910	456.261971	10.704679
9.118495	459.732771	10.709696
9.142359	461.878265	10.714714
9.740008	468.317636	10.719731
9.452812	465.654998	10.724749
9.527734	459.767695	10.729767
8.991226	461.375616	10.734784
9.274331	459.495147	10.739802
9.233853	472.723877	10.744819
9.299180	479.612190	10.749837
9.341836	483.944792	10.754855
9.549854	481.495369	10.759872
9.555953	468.711030	10.764890
9.560777	475.794946	10.769907
9.510016	481.151904	10.774925
9.752843	467.030575	10.779943
9.421060	461.171883	10.784960
9.308553	451.249274	10.789978
9.146331	453.729838	10.794995
9.087722	470.719781	10.800013
9.489287	466.271092	10.805031
9.386242	469.282063	10.810048
9.581273	470.570968	10.815066
9.624868	465.114556	10.820083
9.476796	465.809970	10.825101
9.582938	469.113405	10.830119
9.688986	474.527993	10.835136
9.785447	467.472895	10.840154
9.570644	466.493575	10.845171
9.531520	471.883431	10.850189
9.931364	462.752007	10.855207
9.640507	456.934279	10.860224
9.605169	449.618854	10.865242
9.467371	443.878281	10.870259
9.113600	450.778189	10.875277
9.687381	453.207273	10.880295
9.817462	469.359988	10.885312
10.062299	468.539467	10.890330
9.880638	448.744094	10.895347
9.410006	453.945521	10.900365
9.646361	450.844780	10.905383
9.472341	450.408196	10.910400
9.407830	443.491774	10.915418
9.326722	449.459334	10.920435
9.648066	467.109605	10.925453
9.718131	466.445678	10.930471
9.317981	475.656451	10.935488
9.423445	472.831694	10.940506
9.605600	470.575639	10.945523
9.314304	482.316087	10.950541
9.728190	472.043277	10.955559
9.763444	473.647381	10.960576
9.516409	481.751924	10.965594
9.656699	484.112813	10.970611
9.415442	478.309444	10.975629
9.818130	484.659262	10.980647
9.785156	484.803449	10.985664
9.928845	487.851743	10.990682
9.912280	487.251794	10.995699
9.927497	498.780435	11.000717
9.800504	478.913404	11.005735
9.456614	472.251899	11.010752
9.524118	488.471175	11.015770
9.911977	495.612222	11.020787
10.033323	501.008658	11.025805
10.072208	498.131150	11.030823
10.066414	504.213229	11.035840
10.155191	497.986100	11.040858
9.858145	484.018238	11.045875
9.783486	489.274783	11.050893
10.000822	491.282864	11.055911
10.084848	486.217764	11.060928
10.357941	478.920575	11.065946
9.895563	473.599740	11.070963
9.515901	483.529974	11.075981
9.999274	471.769494	11.080999
9.768981	481.029560	11.086016
9.999372	494.134085	11.091034
10.371234	491.147932	11.096051
9.619801	482.337754	11.101069
10.282732	481.590986	11.106087
10.346778	480.565094	11.111104
9.676717	481.780419	11.116122
10.253618	479.469213	11.121139
9.695302	484.703234	11.126157
10.186699	483.838013	11.131175
10.345752	500.207141	11.136192
9.891228	483.455254	11.141210
10.164340	482.747090	11.146227
9.917182	495.373728	11.151245
10.086288	498.048854	11.156263
9.995015	495.478777	11.161280
10.181146	494.254003	11.166298
10.434305	497.531397	11.171315
10.293515	499.270205	11.176333
10.100135	487.517258	11.181351
10.152841	489.071310	11.186368
10.349925	486.254376	11.191386
10.087931	482.581154	11.196403
10.091726	490.012359	11.201421
10.445423	486.151760	11.206439
9.984028	487.416644	11.211456
10.261272	494.483398	11.216474
10.269209	491.064779	11.221491
10.036206	501.253043	11.226509
10.387817	495.363672	11.231527
10.365618	500.684632	11.236544
10.369849	496.553409	11.241562
10.191213	500.216755	11.246579
10.223255	498.195498	11.251597
10.245681	490.602831	11.256615
10.206136	502.177869	11.261632
10.504225	496.419902	11.266650
10.640320	499.690278	11.271667
10.434299	498.892618	11.276685
9.888649	487.345991	11.281703
10.260256	491.497995	11.286720
10.175750	494.850052	11.291738
10.466159	491.409543	11.296755
10.278271	507.160537	11.301773
9.777892	502.363141	11.306791
10.031649	511.285936	11.311808
10.198924	503.083756	11.316826
10.505322	502.304140	11.321843
10.401099	496.340581	11.326861
10.503622	491.272599	11.331879
10.650361	500.836874	11.336896
10.768496	505.173507	11.341914
10.826269	492.958593	11.346931
10.669216	500.493738	11.351949
10.547908	504.965477	11.356967
10.473031	501.461925	11.361984
10.354870	493.865900	11.367002
10.336086	492.998064	11.372019
10.311910	502.917140	11.377037
10.529642	500.286329	11.382055
10.237476	488.958998	11.387072
10.419022	495.835535	11.392090
10.426088	503.140010	11.397107
10.420872	506.356652	11.402125
10.636166	508.601729	11.407143
10.770551	505.453741	11.412160
10.458888	501.475837	11.417178
10.545466	505.634355	11.422195
10.509264	516.937494	11.427213
10.984772	526.687269	11.432231
11.035648	509.449587	11.437248
10.921951	513.664535	11.442266
10.736565	499.821281	11.447283
10.833427	500.090414	11.452301
10.543218	498.106708	11.457319
10.710470	491.662245	11.462336
10.614566	503.271303	11.467354
10.825995	497.422692	11.472371
10.649563	512.070579	11.477389
10.766722	501.894443	11.482407
10.831844	497.005845	11.487424
11.018809	503.521795	11.492442
10.696076	499.873804	11.497459
10.555248	508.529844	11.502477
10.580767	498.386912	11.507495
11.124228	500.738676	11.512512
10.851922	507.635389	11.517530
11.101428	498.764030	11.522547
10.625810	507.730960	11.527565
10.489868	506.830874	11.532583
10.698425	498.600180	11.537600
10.432525	504.448213	11.542618
10.819189	511.204461	11.547635
11.013972	523.039661	11.552653
10.841913	513.119978	11.557671
10.938950	522.445860	11.562688
10.915232	518.618772	11.567706
10.715698	524.090421	11.572723
10.756191	520.562590	11.577741
10.408178	519.149591	11.582759
11.143553	517.422751	11.587776
10.612823	526.710684	11.592794
11.061122	514.327658	11.597811
10.897415	529.825610	11.602829
10.486374	523.395437	11.607847
11.155623	514.294622	11.612864
10.772788	521.798661	11.617882
10.887774	516.823402	11.622899
10.850246	532.061879	11.627917
11.133573	538.297762	11.632935
11.180665	544.879684	11.637952
11.084238	553.257444	11.642970
11.301457	541.816057	11.647987
11.017047	530.799905	11.653005
11.115989	530.330287	11.658023
11.168447	526.819526	11.663040
11.023583	532.216396	11.668058
11.189885	534.087267	11.673075
11.325774	536.912732	11.678093
11.341695	538.481983	11.683111
11.520119	522.739153	11.688128
11.130204	526.653142	11.693146
11.240297	520.772966	11.698163
11.308282	522.987333	11.703181
11.197199	515.560604	11.708199
11.319013	520.878082	11.713216
11.295680	533.813866	11.718234
11.331606	518.465596	11.723251
11.238720	521.686424	11.728269
11.089029	528.396805	11.733287
11.242994	521.585185	11.738304
11.015820	529.307978	11.743322
11.293759	524.509308	11.748339
11.370572	528.312761	11.753357
11.157969	525.067323	11.758375
11.289504	518.855619	11.763392
11.336017	525.525983	11.768410
11.396605	521.793060	11.773427
11.125659	532.599450	11.778445
11.401178	544.614589	11.783463
11.558412	545.164646	11.788480
11.404806	548.158257	11.793498
11.453276	535.518746	11.798515
11.318025	531.952006	11.803533
11.154747	546.165547	11.808551
12.010900	543.012468	11.813568
11.458420	549.608852	11.818586
11.152277	531.167621	11.823603
11.867679	543.732783	11.828621
11.339880	537.317629	11.833639
11.272438	529.634801	11.838656
11.439068	550.736305	11.843674
11.402336	546.636693	11.848691
11.480025	551.894781	11.853709
11.499479	560.295527	11.858727
11.484859	550.887776	11.863744
11.509925	552.127414	11.868762
11.243357	555.460493	11.873779
11.618594	552.571631	11.878797
11.401629	550.352462	11.883815
11.839714	553.269728	11.888832
11.622626	548.090554	11.893850
11.967775	558.337150	11.898867
12.014280	549.841341	11.903885
12.031952	550.687670	11.908903
11.418717	540.022498	11.913920
11.562051	545.920433	11.918938
11.621708	548.754613	11.923955
11.789236	561.859508	11.928973
11.619877	557.868902	11.933991
11.892974	547.573790	11.939008
11.445388	548.158057	11.944026
11.129522	552.369778	11.949043
11.636047	545.203468	11.954061
11.480446	554.111129	11.959079
11.567453	549.499964	11.964096
11.759910	555.298739	11.969114
11.453890	554.144276	11.974131
11.743625	548.204565	11.979149
11.600892	556.393884	11.984167
11.308808	546.183615	11.989184
11.788326	561.600380	11.994202
11.929686	566.315249	11.999219
12.049425	568.300667	12.004237
11.617680	576.759048	12.009255
11.662807	577.433853	12.014272
12.049456	582.725893	12.019290
11.925323	575.739811	12.024307
11.915441	568.401440	12.029325
11.980267	575.438185	12.034343
12.133696	573.334907	12.039360
12.418613	578.532337	12.044378
11.836084	564.397431	12.049395
12.124018	548.590193	12.054413
11.804647	555.320690	12.059431
11.957801	551.200980	12.064448
12.134415	562.171223	12.069466
12.035125	563.231416	12.074483
11.873591	555.992398	12.079501
11.755483	560.050260	12.084519
12.001450	570.230257	12.089536
12.092127	576.455124	12.094554
11.903905	577.049501	12.099571
12.155101	571.639625	12.104589
12.179166	573.598916	12.109607
12.119722	577.717072	12.114624
12.100136	579.951393	12.119642
11.935638	580.138148	12.124659
12.251075	584.166382	12.129677
12.281861	581.236474	12.134695
12.189715	577.628302	12.139712
12.237025	576.933202	12.144730
12.312021	577.527620	12.149747
12.299514	576.081313	12.154765
12.287722	578.551096	12.159783
12.083874	575.970134	12.164800
12.079402	578.552382	12.169818
12.189564	574.461449	12.174835
12.278587	581.854178	12.179853
11.891396	574.546149	12.184871
12.190274	575.553816	12.189888
11.772255	582.646808	12.194906
11.728621	578.239007	12.199923
12.329231	576.630970	12.204941
12.306288	576.170861	12.209959
12.270303	571.645110	12.214976
12.395966	573.115230	12.219994
12.020029	581.145218	12.225011
12.341857	587.144758	12.230029
12.351484	598.734292	12.235047
12.479447	590.901097	12.240064
12.122587	588.574322	12.245082
12.413235	597.917434	12.250099
12.666761	604.527195	12.255117
11.935886	602.697291	12.260135
12.340915	599.027484	12.265152
12.771429	599.986257	12.270170
12.433514	607.877798	12.275187
12.733081	600.453365	12.280205
12.528420	596.076942	12.285223
12.626088	607.349828	12.290240
12.691934	601.656389	12.295258
12.481635	601.499994	12.300275
12.692164	603.868897	12.305293
12.514611	601.514202	12.310311
12.433198	599.106671	12.315328
12.475527	604.095735	12.320346
12.325033	607.918817	12.325363
12.324446	597.174001	12.330381
12.625454	599.055463	12.335399
12.320887	600.977564	12.340416
12.316485	590.593095	12.345434
12.450775	594.908301	12.350451
12.692340	594.435409	12.355469
12.793394	600.434615	12.360487
12.887576	596.229405	12.365504
12.975260	601.170383	12.370522
12.776977	610.551759	12.375539
12.929210	601.004398	12.380557
12.929773	600.146168	12.385575
12.796026	596.348816	12.390592
12.837105	598.706233	12.395610
12.688817	602.181845	12.400627
13.099226	593.528374	12.405645
12.986967	594.439115	12.410663
12.710962	608.944801	12.415680
12.769492	589.228636	12.420698
12.777193	601.465387	12.425715
12.956968	593.927070	12.430733
12.737458	602.781591	12.435751
12.531880	603.233509	12.440768
12.929760	598.469793	12.445786
12.793224	604.954100	12.450803
12.992441	599.372434	12.455821
12.862384	602.094155	12.460839
12.681635	598.859522	12.465856
12.769320	603.156740	12.470874
12.872595	605.141570	12.475891
12.845555	599.831809	12.480909
12.869763	601.718499	12.485927
12.920850	593.468099	12.490944
12.854247	591.162401	12.495962
12.462717	604.931862	12.500979
13.125382	613.500720	12.505997
12.996369	625.039276	12.511015
12.909064	622.869335	12.516032
13.432734	619.054825	12.521050
12.897157	629.899320	12.526067
13.087078	629.866798	12.531085
13.273899	637.957509	12.536103
13.418690	632.605206	12.541120
13.295525	620.686609	12.546138
12.931084	613.419202	12.551155
13.063056	614.888343	12.556173
13.552106	615.525589	12.561191
13.157677	625.467668	12.566208
13.133535	614.575036	12.571226
12.881472	621.610647	12.576243
13.379017	620.652948	12.581261
13.171328	625.964957	12.586279
13.050153	631.235097	12.591296
13.494523	620.092797	12.596314
13.280652	629.643861	12.601331
13.554748	622.059290	12.606349
13.217699	629.928616	12.611367
13.435187	635.060825	12.616384
13.152363	619.796809	12.621402
13.067229	636.592231	12.626419
13.259106	627.729780	12.631437
13.347344	627.072484	12.636455
13.188188	629.404278	12.641472
13.349174	624.163061	12.646490
13.142256	625.154811	12.651507
12.993072	619.302349	12.656525
13.297524	620.283905	12.661543
13.274982	628.643886	12.666560
13.344827	619.440690	12.671578
13.079036	628.700048	12.676595
13.453571	627.221877	12.681613
13.687190	632.594561	12.686631
13.634449	642.549719	12.691648
13.591909	634.241297	12.696666
13.478688	631.942851	12.701683
13.402582	621.272893	12.706701
13.697303	623.328899	12.711719
13.429240	617.245646	12.716736
13.707731	626.530709	12.721754
13.507498	630.187977	12.726771
13.245780	630.658103	12.731789
13.975051	648.642660	12.736807
13.580085	644.904903	12.741824
13.628465	641.640899	12.746842
13.812430	646.891935	12.751859
13.830807	647.611932	12.756877
13.825056	635.006038	12.761895
13.467552	630.968972	12.766912
13.747962	624.440573	12.771930
12.987897	637.576343	12.776947
13.716416	643.165456	12.781965
14.202233	650.698398	12.786983
14.120938	651.689524	12.792000
14.056504	641.623630	12.797018
13.921566	638.710049	12.802035
13.522160	632.732444	12.807053
13.541663	634.193853	12.812071
13.556279	644.574010	12.817088
14.003305	644.372074	12.822106
14.108115	649.916292	12.827123
13.829824	646.539053	12.832141
14.163996	632.772587	12.837159
13.777256	635.247109	12.842176
13.692155	623.322584	12.847194
13.908753	634.939875	12.852211
14.154242	640.951320	12.857229
14.184867	638.557896	12.862247
13.774341	635.788206	12.867264
14.052747	629.421057	12.872282
13.808108	633.151510	12.877299
13.565756	650.056626	12.882317
14.092049	655.112360	12.887335
14.176450	654.004396	12.892352
13.972037	653.619875	12.897370
13.945776	653.381179	12.902387
13.962146	654.050997	12.907405
14.141068	656.345936	12.912423
14.226533	652.470262	12.917440
14.026910	654.050993	12.922458
14.021286	658.511070	12.927475
14.086341	656.323715	12.932493
14.210613	648.601519	12.937511
14.078770	663.447709	12.942528
14.217242	661.539246	12.947546
14.157135	656.932025	12.952563
13.933564	658.513329	12.957581
13.890518	657.844916	12.962599
13.884971	663.860742	12.967616
14.317084	653.499786	12.972634
14.056662	659.930821	12.977651
13.759528	657.462198	12.982669
13.908490	661.087194	12.987687
14.061480	677.826645	12.992704
14.372729	668.210310	12.997722
14.674377	680.152049	13.002739
14.536536	681.546444	13.007757
14.306540	677.587341	13.012775
14.464874	685.562593	13.017792
14.494588	674.942396	13.022810
14.343504	675.452101	13.027827
14.528100	676.663754	13.032845
14.348428	672.554811	13.037863
14.405449	680.021988	13.042880
14.243452	681.189778	13.047898
14.705597	673.418121	13.052915
14.164492	674.783787	13.057933
14.585767	674.554303	13.062951
14.850434	675.781890	13.067968
14.763084	672.845116	13.072986
14.635374	663.600075	13.078003
14.529666	654.398949	13.083021
14.514826	648.639165	13.088039
14.328842	656.939403	13.093056
14.333458	669.785730	13.098074
14.712236	678.001202	13.103091
14.399193	664.155606	13.108109
14.772004	667.196659	13.113127
14.735246	681.109751	13.118144
14.988588	672.057833	13.123162
15.194565	677.977616	13.128179
14.395852	654.428135	13.133197
14.755457	651.595338	13.138215
14.495237	652.488095	13.143232
14.659101	663.943207	13.148250
14.695265	668.434650	13.153267
14.640045	669.235531	13.158285
14.669460	668.618950	13.163303
14.620257	676.203647	13.168320
14.522425	671.349840	13.173338
14.900426	669.145315	13.178355
14.717040	676.526850	13.183373
15.023934	668.353348	13.188391
14.962751	662.477702	13.193408
14.849347	664.392137	13.198426
14.806095	676.109871	13.203443
14.558092	679.083488	13.208461
14.588804	673.521724	13.213479
14.595066	677.730656	13.218496
14.617888	675.120699	13.223514
14.781409	666.521411	13.228531
14.790654	670.751966	13.233549
14.948402	681.182441	13.238567
15.138740	689.941636	13.243584
15.443559	691.052524	13.248602
15.350335	684.680103	13.253619
15.057974	683.138509	13.258637
15.058023	674.542580	13.263655
14.824934	676.554542	13.268672
14.652149	680.052918	13.273690
14.942702	685.744947	13.278707
14.724303	692.803747	13.283725
15.439990	691.351347	13.288743
15.386033	707.160558	13.293760
15.321012	707.675798	13.298778
15.675144	691.842348	13.303795
15.078917	679.640772	13.308813
15.256491	675.652926	13.313831
14.906122	683.855698	13.318848
14.750050	681.298839	13.323866
15.042021	696.129560	13.328883
15.210577	709.963372	13.333901
15.204995	706.641488	13.338919
15.378756	709.637803	13.343936
15.248865	714.376011	13.348954
15.365746	710.747889	13.353971
15.282379	716.308804	13.358989
15.558896	704.955907	13.364007
15.379749	707.066769	13.369024
15.419530	707.101803	13.374042
15.702276	700.399449	13.379059
15.171563	703.855731	13.384077
15.415087	702.038202	13.389095
15.307742	712.147062	13.394112
15.235368	701.924585	13.399130
15.704976	697.834462	13.404147
15.638404	713.213311	13.409165
15.464214	713.534116	13.414183
15.454934	699.858942	13.419200
15.189193	708.799606	13.424218
15.613694	704.258928	13.429235
15.512565	706.856243	13.434253
15.591459	700.299234	13.439271
15.351187	706.411577	13.444288
15.096784	709.780660	13.449306
15.689200	707.687909	13.454323
15.424531	709.136766	13.459341
15.250363	705.351996	13.464359
15.289932	708.378671	13.469376
15.461971	724.654468	13.474394
15.636020	724.296224	13.479411
15.739573	726.154795	13.484429
16.120314	731.517226	13.489447
16.184893	725.151779	13.494464
15.772251	723.613130	13.499482
15.652499	705.720192	13.504499
15.502041	709.256121	13.509517
16.113306	710.095242	13.514535
15.719741	707.821501	13.519552
15.816174	713.442780	13.524570
15.969855	714.261630	13.529587
15.868975	706.309385	13.534605
15.466471	716.997518	13.539623
15.810371	722.485599	13.544640
15.715179	734.590143	13.549658
16.082661	721.780914	13.554675
16.041722	725.236680	13.559693
16.098380	721.242404	13.564711
16.286179	720.967223	13.569728
15.924643	721.351911	13.574746
16.156811	722.575094	13.579763
16.360611	712.751409	13.584781
16.244342	705.640978	13.589799
16.122474	702.031097	13.594816
15.609768	703.897256	13.599834
16.129695	697.318916	13.604851
15.758462	697.209667	13.609869
16.054490	712.910745	13.614887
16.323712	714.011397	13.619904
15.866217	724.771211	13.624922
16.185105	725.330817	13.629939
16.012974	737.141238	13.634957
16.044436	734.570951	13.639975
16.009987	731.676422	13.644992
16.609645	732.425835	13.650010
16.383604	723.757790	13.655027
16.078797	729.785518	13.660045
16.448570	728.219721	13.665063
16.361613	729.199110	13.670080
16.109389	734.410792	13.675098
16.368405	738.176454	13.680115
16.152527	732.277535	13.685133
16.200013	724.387386	13.690151
16.494918	726.298213	13.695168
16.295361	732.874427	13.700186
16.416095	731.590394	13.705203
16.115852	726.351533	13.710221
16.033434	728.731351	13.715239
16.440556	726.238272	13.720256
16.183968	728.844016	13.725274
16.089298	725.791612	13.730291
16.182872	714.678625	13.735309
16.318973	731.414445	13.740327
16.567398	739.470366	13.745344
16.421087	737.060297	13.750362
16.366569	747.574351	13.755379
16.667137	746.284407	13.760397
16.277772	745.660444	13.765415
16.614063	741.136646	13.770432
16.735069	748.931551	13.775450
16.687778	751.192297	13.780467
16.815227	755.297174	13.785485
16.750268	747.989395	13.790503
16.726995	744.338908	13.795520
16.897942	752.324849	13.800538
16.699587	734.901698	13.805555
16.745740	737.375104	13.810573
16.496644	744.239893	13.815591
16.857426	742.268408	13.820608
16.654092	750.410449	13.825626
17.094370	746.612052	13.830643
16.850586	740.714319	13.835661
16.668509	731.360947	13.840679
16.838206	737.570412	13.845696
16.964304	747.156967	13.850714
17.014522	727.388296	13.855731
16.612394	724.917076	13.860749
16.580232	731.347310	13.865767
16.818882	737.785873	13.870784
16.732531	748.244925	13.875802
16.837534	743.141773	13.880819
17.116163	738.260891	13.885837
16.841874	743.763180	13.890855
17.285874	743.426019	13.895872
16.828830	752.854070	13.900890
16.884558	743.662475	13.905907
16.835996	743.761756	13.910925
16.744616	746.316535	13.915943
16.981152	739.233208	13.920960
16.482156	744.467536	13.925978
16.849080	746.461823	13.930995
16.866372	760.899877	13.936013
16.942264	766.120440	13.941031
17.336525	773.314249	13.946048
16.903572	777.537941	13.951066
17.397580	765.712499	13.956083
17.388725	766.370470	13.961101
17.048597	768.623165	13.966119
17.317347	766.180026	13.971136
17.360385	762.055321	13.976154
17.216730	769.515912	13.981171
17.562753	769.692609	13.986189
17.300222	772.848379	13.991207
17.722831	769.535553	13.996224
17.490059	756.794510	14.001242
17.144235	746.276921	14.006259
17.367908	750.168005	14.011277
17.413522	764.197721	14.016295
17.479771	765.184816	14.021312
17.192623	765.400137	14.026330
17.111407	767.940714	14.031347
17.334593	762.112276	14.036365
16.969088	764.015481	14.041383
17.680618	762.768844	14.046400
17.551718	764.881357	14.051418
17.757935	764.767405	14.056435
18.028629	763.570471	14.061453
17.581367	764.119981	14.066471
17.709592	758.975340	14.071488
17.472425	763.149612	14.076506
17.405466	761.980004	14.081523
17.363670	757.742280	14.086541
17.508815	765.157904	14.091559
17.466481	759.856787	14.096576
17.438704	761.366592	14.101594
17.294763	752.720462	14.106611
17.350393	749.925510	14.111629
17.153421	772.286216	14.116647
17.507040	774.377250	14.121664
17.494001	781.479848	14.126682
17.649179	787.647410	14.131699
17.986610	789.400149	14.136717
18.027634	785.881650	14.141735
17.953266	787.341908	14.146752
17.805881	788.147677	14.151770
17.907646	776.051949	14.156787
17.973805	781.280343	14.161805
17.902044	790.143510	14.166823
18.021037	786.568692	14.171840
18.304067	789.355509	14.176858
17.870618	778.744249	14.181875
18.026579	781.206875	14.186893
17.996626	789.419767	14.191911
18.191038	779.130461	14.196928
18.028172	780.749660	14.201946
18.028515	780.759278	14.206963
18.523803	774.288884	14.211981
17.980067	769.564435	14.216999
18.037809	779.439353	14.222016
17.679138	778.147909	14.227034
17.917522	779.988650	14.232051
18.293909	779.740908	14.237069
18.079660	780.629670	14.242087
18.147790	779.565256	14.247104
17.884980	780.710880	14.252122
17.918714	783.861550	14.257139
18.064742	774.756863	14.262157
17.683142	779.767801	14.267175
18.248129	783.151328	14.272192
18.183370	788.273878	14.277210
17.957600	788.684765	14.282227
18.612447	794.749287	14.287245
18.109117	796.027032	14.292263
18.400082	805.180861	14.297280
18.648680	795.788801	14.302298
18.576406	794.771493	14.307315
18.424818	778.537036	14.312333
18.143084	786.953225	14.317351
18.143945	794.479686	14.322368
18.464416	800.858196	14.327386
18.223505	802.896637	14.332403
18.601368	804.188658	14.337421
18.349273	805.499868	14.342439
18.592337	803.754982	14.347456
18.604872	798.625187	14.352474
18.390009	804.591601	14.357491
18.895919	796.125129	14.362509
18.789433	809.645246	14.367527
18.876325	800.350942	14.372544
18.629623	805.845800	14.377562
18.616669	799.732232	14.382579
19.253605	804.417341	14.387597
19.129813	795.670226	14.392615
18.880971	787.908234	14.397632
18.607254	782.854570	14.402650
18.781829	789.359931	14.407667
19.091111	780.914614	14.412685
19.035780	777.657265	14.417703
18.877954	777.959745	14.422720
18.820292	768.246164	14.427738
18.809361	770.917806	14.432755
18.630225	764.874304	14.437773
18.549457	776.995566	14.442791
18.561408	774.958471	14.447808
19.032994	780.827467	14.452826
18.936394	795.103405	14.457843
18.860008	792.259575	14.462861
19.086298	793.912857	14.467879
18.901166	798.792228	14.472896
19.263554	792.333052	14.477914
18.874836	789.761908	14.482931
19.287044	792.717957	14.487949
18.745027	795.027333	14.492967
19.263918	799.945409	14.497984
19.091320	788.308945	14.503002
18.793727	794.868888	14.508019
18.979113	789.163088	14.513037
19.113269	805.088261	14.518055
18.676079	804.948256	14.523072
18.870738	798.016590	14.528090
18.765175	797.503069	14.533107
19.014725	799.250556	14.538125
19.240955	804.018545	14.543143
18.713368	805.694532	14.548160
19.392859	808.236593	14.553178
19.470293	807.382163	14.558195
19.253343	805.118779	14.563213
19.360226	803.527636	14.568231
19.267798	804.113417	14.573248
19.419036	809.397999	14.578266
19.509834	825.863257	14.583283
19.756521	812.599412	14.588301
19.128255	805.432961	14.593319
19.258554	801.916338	14.598336
19.567646	811.171487	14.603354
19.333375	826.655437	14.608371
19.667387	824.987905	14.613389
19.714110	820.764785	14.618407
19.356820	826.756538	14.623424
19.696641	830.579064	14.628442
19.133993	823.042637	14.633459
19.665536	813.991513	14.638477
19.924844	814.188022	14.643495
20.006670	819.732717	14.648512
19.894038	812.400776	14.653530
19.494960	801.894601	14.658547
19.679642	796.526570	14.663565
19.661155	807.252794	14.668583
19.628092	814.415326	14.673600
19.798010	817.194513	14.678618
19.773109	827.063390	14.683635
19.933291	820.660933	14.688653
20.233357	824.874647	14.693671
20.040569	807.643057	14.698688
20.128433	793.413057	14.703706
19.663169	799.380587	14.708723
19.681666	786.603556	14.713741
19.706559	792.040345	14.718759
20.396193	802.100907	14.723776
20.023943	795.030295	14.728794
19.656720	794.800504	14.733811
19.980046	795.687616	14.738829
20.058769	798.884931	14.743847
20.213347	809.464293	14.748864
20.006126	799.714023	14.753882
19.945911	805.369188	14.758899
19.910077	811.017403	14.763917
20.222227	812.234451	14.768935
20.057786	807.804378	14.773952
20.234029	811.832245	14.778970
20.039120	829.847271	14.783987
20.053722	816.092551	14.789005
20.230980	818.946333	14.794023
20.086768	828.373052	14.799040
20.496635	814.843962	14.804058
20.043360	824.631216	14.809075
19.869728	820.193103	14.814093
20.371854	825.716540	14.819111
20.014245	824.005216	14.824128
20.179016	820.398018	14.829146
20.185885	819.545106	14.834163
19.944863	826.717931	14.839181
20.044772	817.266962	14.844199
20.172080	825.291287	14.849216
20.418538	834.297431	14.854234
20.818500	847.208561	14.859251
20.355150	844.213538	14.864269
20.651952	839.134144	14.869287
20.253992	840.073602	14.874304
20.518613	834.778318	14.879322
20.440175	843.522634	14.884339
20.699525	842.352707	14.889357
20.556947	847.654645	14.894375
20.663315	845.599687	14.899392
21.131187	835.384534	14.904410
20.902115	830.630010	14.909427
20.311582	823.902634	14.914445
20.453243	830.807600	14.919463
20.521249	837.903914	14.924480
20.489481	835.419195	14.929498
20.713863	853.507815	14.934515
20.764786	851.149071	14.939533
20.713822	851.987167	14.944551
20.872557	846.342302	14.949568
20.725850	837.876437	14.954586
20.728933	849.725923	14.959603
21.028417	844.415742	14.964621
20.832165	842.234336	14.969639
20.646351	853.179139	14.974656
20.807454	837.451351	14.979674
20.671181	841.048213	14.984691
21.396057	843.071984	14.989709
21.208929	844.666565	14.994727
20.624337	850.220356	14.999744
20.825490	849.119448	15.004762
20.850046	849.885827	15.009779
20.956563	853.946650	15.014797
21.218534	857.374214	15.019815
21.163073	862.501650	15.024832
21.268499	850.998578	15.029850
21.083231	860.422239	15.034867
21.329331	864.798995	15.039885
21.074329	855.024577	15.044903
21.520173	864.062806	15.049920
21.120778	853.755460	15.054938
21.333294	855.164745	15.059955
21.604960	858.448792	15.064973
21.248289	842.454486	15.069991
21.033993	839.581629	15.075008
21.315219	842.561235	15.080026
21.704328	863.284497	15.085043
21.022214	856.031737	15.090061
21.360110	867.557713	15.095079
21.144174	864.757689	15.100096
21.130367	861.418123	15.105114
20.934573	863.881881	15.110131
21.185438	873.698381	15.115149
21.605388	865.242105	15.120167
21.392016	867.790649	15.125184
21.644513	853.175215	15.130202
21.792496	862.619572	15.135219
21.279818	868.250533	15.140237
21.521140	865.505545	15.145255
21.818089	865.267015	15.150272
21.594050	861.780304	15.155290
21.858441	863.361389	15.160307
21.606247	875.556744	15.165325
21.748691	864.858923	15.170343
21.492603	864.952647	15.175360
21.483490	862.918822	15.180378
21.764772	876.053574	15.185395
21.765397	883.624290	15.190413
21.936254	887.520472	15.195431
21.943652	890.741532	15.200448
22.280056	886.864605	15.205466
22.052231	874.482462	15.210483
21.643428	868.664028	15.215501
22.051280	857.460995	15.220519
21.702745	863.896355	15.225536
21.738729	868.750785	15.230554
21.926526	882.818416	15.235571
21.900604	889.168841	15.240589
22.096182	890.669127	15.245607
22.240537	893.897265	15.250624
22.361729	882.723070	15.255642
22.398708	883.875672	15.260659
21.997097	887.406559	15.265677
21.820684	877.193868	15.270695
21.837471	891.146123	15.275712
21.673846	881.445823	15.280730
21.974266	879.183926	15.285747
21.996408	876.652939	15.290765
22.103839	873.755231	15.295783
22.084413	876.308293	15.300800
21.746466	882.738855	15.305818
22.489550	904.164429	15.310835
22.261499	916.397077	15.315853
22.584149	916.507988	15.320871
22.497071	917.724088	15.325888
22.651629	909.315423	15.330906
22.704217	897.426080	15.335923
22.462711	894.229254	15.340941
22.532378	884.533655	15.345959
22.027059	882.072168	15.350976
22.284619	904.374893	15.355994
22.495704	900.949812	15.361011
22.570595	906.038030	15.366029
22.727407	902.529883	15.371047
22.684687	907.835225	15.376064
23.103447	907.539861	15.381082
23.165386	902.607467	15.386099
22.445487	902.486232	15.391117
22.942501	880.612375	15.396135
23.054138	883.416425	15.401152
22.723111	879.851695	15.406170
22.927802	881.088635	15.411187
22.935253	888.266979	15.416205
23.076677	877.686071	15.421223
22.664057	881.635229	15.426240
22.926175	880.496426	15.431258
22.731790	875.218949	15.436275
22.739469	878.733446	15.441293
22.713496	873.852617	15.446311
22.849830	883.074742	15.451328
22.520828	882.517113	15.456346
22.841729	899.811286	15.461363
22.927736	911.322861	15.466381
23.080494	912.716209	15.471399
23.309877	912.683854	15.476416
23.339966	907.301991	15.481434
22.948582	908.338256	15.486451
22.915898	907.043384	15.491469
23.117527	912.051913	15.496487
23.144893	908.267279	15.501504
23.170389	908.437079	15.506522
23.264066	902.682406	15.511539
22.991336	911.681064	15.516557
23.239322	909.512533	15.521575
22.854226	911.014868	15.526592
22.953154	907.591470	15.531610
23.085421	894.367468	15.536627
23.052200	903.341453	15.541645
22.858175	903.119407	15.546663
22.960036	922.053977	15.551680
23.064110	925.872205	15.556698
23.504120	932.901169	15.561715
23.558653	934.442353	15.566733
23.639082	933.376016	15.571751
23.765962	927.720306	15.576768
23.843349	927.818912	15.581786
23.929295	919.566089	15.586803
24.024181	922.729353	15.591821
23.746943	912.513404	15.596839
23.570447	903.960630	15.601856
23.468340	907.864603	15.606874
23.676239	903.329197	15.611891
23.395172	916.810306	15.616909
23.534666	916.293340	15.621927
23.658519	919.256437	15.626944
23.679601	923.336889	15.631962
23.927491	916.655660	15.636979
23.515729	929.791061	15.641997
24.060848	922.265149	15.647015
23.693521	923.083078	15.652032
23.854714	925.355566	15.657050
24.047156	927.143516	15.662067
24.129307	933.966271	15.667085
23.761719	929.103902	15.672103
24.087769	922.845993	15.677120
23.876780	930.247709	15.682138
24.170932	914.227744	15.687155
24.004322	926.529727	15.692173
23.822320	916.160096	15.697191
24.152019	921.208646	15.702208
23.351699	930.952163	15.707226
23.756419	922.813806	15.712243
23.695714	923.031741	15.717261
24.175678	944.671896	15.722279
24.371673	952.398412	15.727296
24.440168	945.902890	15.732314
24.200811	933.699222	15.737331
24.239158	945.161436	15.742349
24.386505	942.623569	15.747367
24.417472	936.982789	15.752384
24.798007	945.570490	15.757402
24.312834	932.742389	15.762419
23.919826	935.738625	15.767437
24.405371	946.859819	15.772455
24.270136	942.387295	15.777472
24.427083	949.731732	15.782490
24.623792	950.256721	15.787507
24.561389	953.870505	15.792525
24.420403	948.284896	15.797543
24.361978	947.792433	15.802560
24.381387	955.858863	15.807578
24.752258	941.647796	15.812595
24.408319	951.070963	15.817613
24.543505	955.534437	15.822631
24.789015	949.980168	15.827648
24.423420	960.804709	15.832666
24.754819	955.398009	15.837683
24.804599	953.616931	15.842701
24.823342	951.253717	15.847719
24.953328	947.727647	15.852736
24.637139	950.620409	15.857754
24.998636	946.389276	15.862771
24.995208	944.960460	15.867789
24.894143	945.493942	15.872807
24.906282	948.427101	15.877824
24.706551	944.857695	15.882842
25.210229	941.529059	15.887859
24.674916	946.437746	15.892877
24.730272	946.975275	15.897895
24.806852	939.705339	15.902912
24.867801	950.655962	15.907930
25.228037	955.150668	15.912947
25.247294	958.174236	15.917965
24.702983	961.834652	15.922983
25.110192	964.759950	15.928000
25.067174	965.741979	15.933018
25.135221	974.899046	15.938035
25.028376	971.596034	15.943053
25.133836	974.568315	15.948071
25.300635	974.185949	15.953088
25.101324	975.763504	15.958106
25.449183	965.024173	15.963123
25.495034	977.517170	15.968141
25.525043	973.792070	15.973159
25.382364	972.874074	15.978176
25.335488	974.727691	15.983194
25.269534	968.764327	15.988211
25.251699	970.701783	15.993229
25.272855	968.218273	15.998247
25.257170	964.998897	16.003264
25.062251	972.761039	16.008282
25.565520	982.225882	16.013299
25.917962	985.203891	16.018317
25.938744	992.449628	16.023335
25.806344	991.501629	16.028352
25.814275	985.100728	16.033370
25.543243	973.375328	16.038387
25.835628	983.131777	16.043405
25.957867	988.259983	16.048423
26.121201	980.051887	16.053440
26.086859	977.794763	16.058458
26.024482	965.746552	16.063475
26.132723	962.302759	16.068493
25.831583	968.664506	16.073511
25.880040	968.887535	16.078528
25.797751	960.096008	16.083546
25.878793	959.515559	16.088563
25.558820	966.123230	16.093581
25.964263	969.162411	16.098599
26.217575	977.732066	16.103616
25.843694	976.682813	16.108634
26.019954	989.240719	16.113651
26.019596	980.815116	16.118669
26.002842	991.282409	16.123687
26.528119	985.176494	16.128704
26.177076	988.058910	16.133722
25.871427	990.823807	16.138739
26.352213	983.670797	16.143757
26.278791	991.145792	16.148775
26.538298	986.043761	16.153792
26.442092	982.417204	16.158810
26.264223	985.159050	16.163827
26.447921	978.566686	16.168845
26.338187	984.889170	16.173863
26.508824	982.606443	16.178880
26.536385	987.840907	16.183898
26.205338	983.020170	16.188915
26.327466	987.943270	16.193933
26.240632	995.297280	16.198951
26.387358	990.582031	16.203968
26.465694	991.778692	16.208986
26.524471	989.324035	16.214003
26.493426	985.819873	16.219021
26.197148	990.154877	16.224039
26.603073	987.743998	16.229056
26.722477	994.478927	16.234074
26.625278	991.341665	16.239091
26.779523	1006.872577	16.244109
26.711764	1015.851997	16.249127
27.130493	1004.085454	16.254144
26.721609	1010.596533	16.259162
26.735033	1006.470071	16.264179
26.901960	1001.556017	16.269197
26.863922	1007.974643	16.274215
26.933470	1005.149083	16.279232
27.104296	1005.053263	16.284250
27.243912	994.674536	16.289267
27.317878	996.484095	16.294285
27.021507	1004.211554	16.299303
27.358982	988.800150	16.304320
26.886306	988.387962	16.309338
27.311903	993.680374	16.314355
27.062227	978.584455	16.319373
26.878619	992.590081	16.324391
27.160003	998.264703	16.329408
27.196292	1002.295470	16.334426
27.231878	996.612928	16.339443
27.405317	996.210593	16.344461
27.145121	997.665087	16.349479
27.247517	1002.490279	16.354496
27.450596	1006.532947	16.359514
27.293547	1002.489832	16.364531
27.565830	998.354626	16.369549
27.678223	998.798071	16.374567
27.553403	992.095949	16.379584
27.347504	995.511181	16.384602
26.950170	997.738097	16.389619
27.298711	986.926064	16.394637
27.160634	989.844749	16.399655
27.457405	994.683856	16.404672
27.850753	1009.091963	16.409690
27.656856	1014.162102	16.414707
27.896772	1001.628150	16.419725
27.477810	1001.775635	16.424743
27.849592	1011.841625	16.429760
28.018743	1023.652747	16.434778
27.826349	1004.975566	16.439795
27.964451	992.706778	16.444813
27.585783	1004.003587	16.449831
27.642422	1005.825312	16.454848
27.793453	1023.508965	16.459866
27.746325	1026.082141	16.464883
27.973458	1014.092961	16.469901
27.964604	1022.873868	16.474919
27.579967	1011.680520	16.479936
27.895928	1017.059435	16.484954
27.771978	1016.529836	16.489971
27.932114	1012.797090	16.494989
27.899376	1020.376214	16.500007
28.020059	1021.559973	16.505024
28.370912	1027.725555	16.510042
28.047222	1034.703054	16.515059
28.439976	1033.193613	16.520077
28.422765	1035.806312	16.525095
28.352680	1018.855210	16.530112
28.305700	1018.351496	16.535130
28.192247	1018.852195	16.540147
28.331237	1012.077434	16.545165
28.196343	1024.668032	16.550183
28.714534	1029.109761	16.555200
28.904013	1026.568478	16.560218
28.182262	1020.274862	16.565235
28.433737	1023.969177	16.570253
28.467111	1036.183294	16.575271
28.799844	1027.481749	16.580288
28.883342	1036.532302	16.585306
28.386842	1027.947241	16.590323
28.762185	1027.901629	16.595341
28.509408	1033.545823	16.600359
28.711254	1036.635649	16.605376
28.663374	1033.869393	16.610394
28.632818	1035.799369	16.615411
29.205460	1030.137338	16.620429
28.951297	1034.061858	16.625447
28.751577	1028.324424	16.630464
29.164723	1029.229122	16.635482
29.122329	1029.390559	16.640499
28.717566	1028.718490	16.645517
28.744657	1033.397627	16.650535
29.017680	1027.785403	16.655552
29.189484	1033.010045	16.660570
29.142117	1034.134764	16.665587
28.976849	1031.342604	16.670605
28.717904	1032.216246	16.675623
28.612263	1035.909361	16.680640
29.042637	1035.719483	16.685658
28.929040	1033.727152	16.690675
29.378274	1038.157530	16.695693
29.458661	1039.745190	16.700711
29.260618	1034.073765	16.705728
29.336329	1040.948056	16.710746
29.098519	1032.269069	16.715763
29.304669	1044.500472	16.720781
29.243463	1033.528149	16.725799
29.290755	1038.649105	16.730816
29.709829	1051.437489	16.735834
29.608263	1052.327654	16.740851
29.688173	1042.251682	16.745869
29.583962	1043.726074	16.750887
29.596954	1031.268457	16.755904
29.625829	1028.957304	16.760922
29.600002	1024.638136	16.765939
29.710838	1039.317468	16.770957
29.897947	1040.875889	16.775975
29.533094	1032.235616	16.780992
29.666117	1030.125994	16.786010
29.894215	1056.201478	16.791027
29.974664	1058.947296	16.796045
29.917798	1056.829367	16.801063
29.710119	1050.755499	16.806080
30.094444	1049.644995	16.811098
29.864035	1043.909178	16.816115
30.114880	1046.088829	16.821133
30.329185	1053.989261	16.826151
29.691278	1041.661382	16.831168
30.011096	1050.665680	16.836186
30.092762	1047.342771	16.841203
29.922204	1042.727401	16.846221
30.217443	1048.286275	16.851239
30.169254	1050.200065	16.856256
30.272910	1052.295337	16.861274
30.348127	1066.147115	16.866291
30.366425	1052.486310	16.871309
29.950467	1049.821539	16.876327
30.364108	1059.366649	16.881344
30.418594	1045.394106	16.886362
30.078188	1059.067595	16.891379
30.340675	1045.662262	16.896397
30.518090	1052.924662	16.901415
30.238213	1059.516657	16.906432
30.239198	1049.475059	16.911450
30.353637	1055.879429	16.916467
30.317278	1055.301477	16.921485
30.383638	1051.797916	16.926503
30.139205	1049.731282	16.931520
30.016944	1056.084144	16.936538
30.031318	1068.020378	16.941555
30.272225	1070.403549	16.946573
30.539397	1069.655263	16.951591
30.539978	1078.384235	16.956608
30.624904	1080.302548	16.961626
30.641514	1084.986486	16.966643
30.933872	1083.480049	16.971661
30.847150	1083.761996	16.976679
30.763207	1086.400872	16.981696
30.985404	1093.915088	16.986714
31.101138	1094.736709	16.991731
30.980977	1093.253473	16.996749
31.010529	1096.644688	17.001767
31.087819	1096.942124	17.006784
31.318279	1098.837780	17.011802
31.360070	1098.282373	17.016819
31.519081	1085.470627	17.021837
31.035996	1074.636546	17.026855
30.790139	1077.127062	17.031872
30.875088	1080.282434	17.036890
31.089959	1090.473884	17.041907
31.329078	1093.226561	17.046925
31.243106	1089.229163	17.051943
31.121248	1097.128305	17.056960
30.992081	1086.927072	17.061978
31.305882	1087.869330	17.066995
31.264596	1086.026680	17.072013
31.540829	1081.272309	17.077031
31.250006	1085.161522	17.082048
31.725413	1097.988506	17.087066
31.997156	1109.487070	17.092083
31.688227	1097.622323	17.097101
31.810615	1088.344433	17.102119
31.755422	1089.722836	17.107136
31.557185	1088.497907	17.112154
31.465870	1087.915887	17.117171
31.762486	1098.852000	17.122189
32.301778	1109.226477	17.127207
31.635526	1104.391625	17.132224
31.897018	1088.061012	17.137242
31.862973	1088.202215	17.142259
31.851156	1103.121600	17.147277
32.331685	1108.916730	17.152295
31.676855	1103.477347	17.157312
32.181175	1100.180140	17.162330
31.801267	1115.437710	17.167347
31.916253	1112.623992	17.172365
32.264180	1106.905407	17.177383
32.075631	1112.820490	17.182400
32.217349	1102.305675	17.187418
32.400495	1113.934800	17.192435
32.105495	1104.576722	17.197453
32.398028	1100.372068	17.202471
32.235493	1113.920077	17.207488
32.509838	1108.026757	17.212506
32.479396	1111.225346	17.217523
32.264137	1111.965959	17.222541
32.570186	1108.529208	17.227559
32.021237	1118.217910	17.232576
32.095750	1113.804204	17.237594
32.622093	1114.151644	17.242611
32.301512	1106.984501	17.247629
32.374484	1100.737532	17.252647
32.574221	1103.133428	17.257664
32.532623	1101.915668	17.262682
32.573710	1099.558423	17.267699
32.535790	1100.820529	17.272717
32.861161	1104.717948	17.277735
32.914374	1113.609155	17.282752
32.921080	1100.249917	17.287770
32.527011	1110.466761	17.292787
32.732884	1113.638025	17.297805
33.354805	1121.497113	17.302823
32.833475	1119.994285	17.307840
32.905741	1126.279016	17.312858
33.285726	1131.720581	17.317875
33.154408	1130.952286	17.322893
32.874143	1119.067282	17.327911
32.924793	1132.869289	17.332928
33.035410	1124.681957	17.337946
33.193783	1129.829825	17.342963
32.882794	1125.930569	17.347981
33.214221	1116.859957	17.352999
32.902767	1118.596994	17.358016
33.002186	1119.973417	17.363034
33.234688	1117.147714	17.368051
32.872082	1129.660232	17.373069
33.281506	1134.604913	17.378087
33.247711	1149.000743	17.383104
33.304975	1146.795606	17.388122
34.007891	1150.703681	17.393139
33.836005	1149.806002	17.398157
33.927638	1135.960147	17.403175
33.607309	1130.424494	17.408192
33.441736	1123.103824	17.413210
33.787028	1126.509000	17.418227
33.810580	1133.561861	17.423245
33.755221	1125.435084	17.428263
33.845019	1141.563123	17.433280
34.031933	1139.883751	17.438298
33.464055	1130.539744	17.443315
33.951061	1147.978709	17.448333
33.910147	1150.737126	17.453351
34.016111	1146.722454	17.458368
33.891356	1154.211821	17.463386
34.236482	1158.806761	17.468403
34.048858	1154.739969	17.473421
34.125283	1150.783544	17.478439
34.003721	1153.380950	17.483456
34.195127	1149.561257	17.488474
34.564401	1150.343405	17.493491
34.107336	1155.243121	17.498509
34.219829	1146.083506	17.503527
34.072332	1154.788234	17.508544
34.270098	1153.432218	17.513562
34.467299	1151.710218	17.518579
34.214205	1143.645778	17.523597
34.148774	1145.183568	17.528615
34.250933	1145.357213	17.533632
33.999055	1135.932444	17.538650
33.961151	1141.865107	17.543667
33.898293	1145.100307	17.548685
34.652538	1152.850445	17.553703
35.004392	1170.080102	17.558720
34.555626	1155.813444	17.563738
34.657040	1154.699645	17.568755
34.502687	1171.982872	17.573773
34.741025	1159.199749	17.578791
34.717048	1160.159888	17.583808
34.664097	1165.605755	17.588826
34.924705	1154.261362	17.593843
35.047364	1168.396165	17.598861
34.800176	1166.481423	17.603879
35.017837	1170.673336	17.608896
34.610579	1166.842708	17.613914
34.879813	1167.113416	17.618931
34.876396	1171.434424	17.623949
34.946727	1167.690382	17.628967
34.853849	1166.168179	17.633984
34.890567	1168.273887	17.639002
35.062989	1163.504099	17.644019
34.465769	1169.426025	17.649037
35.043021	1177.885381	17.654055
35.093203	1188.563273	17.659072
35.079861	1186.432241	17.664090
35.404263	1185.432044	17.669107
35.506994	1192.163332	17.674125
35.811097	1183.431455	17.679143
35.599552	1192.988770	17.684160
35.813549	1191.680716	17.689178
35.891767	1183.924433	17.694195
35.581531	1189.202083	17.699213
35.677257	1177.223786	17.704231
35.962135	1181.496755	17.709248
36.089560	1176.904381	17.714266
36.039763	1170.910031	17.719283
35.598354	1164.165618	17.724301
35.315245	1154.325983	17.729319
35.752838	1166.029133	17.734336
35.992965	1172.123644	17.739354
36.064627	1175.126467	17.744371
35.915393	1182.812160	17.749389
35.834908	1183.020554	17.754407
36.268728	1165.489086	17.759424
35.864795	1176.174560	17.764442
35.814338	1173.639055	17.769459
35.745291	1179.627071	17.774477
35.862600	1178.160504	17.779495
35.906946	1179.981005	17.784512
35.597976	1180.161857	17.789530
36.354754	1185.210260	17.794547
36.366559	1198.008513	17.799565
36.221826	1200.969294	17.804583
36.387905	1195.200099	17.809600
36.005478	1201.366302	17.814618
36.648439	1200.953976	17.819635
36.216898	1202.485657	17.824653
36.440835	1197.550050	17.829671
36.495591	1202.288040	17.834688
36.215021	1203.193459	17.839706
36.732298	1198.811780	17.844723
36.632998	1201.364701	17.849741
36.257790	1202.928637	17.854759
36.467878	1203.022362	17.859776
36.529713	1198.948278	17.864794
36.813000	1207.046321	17.869811
36.530617	1211.789467	17.874829
36.673570	1218.486101	17.879847
36.688190	1218.597637	17.884864
36.698335	1227.230520	17.889882
37.040044	1222.630018	17.894899
36.799705	1223.907870	17.899917
37.018046	1221.611373	17.904935
37.334766	1219.088122	17.909952
37.153060	1232.263665	17.914970
37.368131	1225.388615	17.919987
37.146028	1220.131129	17.925005
37.224909	1227.945427	17.930023
37.443162	1225.611074	17.935040
37.130875	1226.007037	17.940058
37.393563	1221.627122	17.945075
37.402760	1223.816016	17.950093
37.501374	1229.800036	17.955111
37.371034	1221.082133	17.960128
37.107905	1230.085767	17.965146
37.422238	1212.875813	17.970163
37.357431	1220.005581	17.975181
37.274651	1221.167383	17.980199
37.548229	1225.161255	17.985216
37.422975	1222.949812	17.990234
37.821838	1229.575048	17.995251
37.353441	1235.098243	18.000269
37.323560	1231.827381	18.005287
37.855930	1235.973466	18.010304
37.506883	1256.423952	18.015322
37.986100	1249.473053	18.020339
37.898673	1247.523961	18.025357
37.822945	1241.637765	18.030375
38.174876	1240.977261	18.035392
37.770592	1241.236070	18.040410
38.141312	1239.351347	18.045427
38.057012	1246.118087	18.050445
37.911016	1243.048338	18.055463
38.349898	1239.354196	18.060480
37.928548	1239.741894	18.065498
38.007058	1236.321612	18.070515
38.344007	1263.914170	18.075533
38.639327	1260.996613	18.080551
38.760145	1257.004851	18.085568
38.282652	1257.404446	18.090586
38.342283	1242.556790	18.095603
38.724630	1255.057551	18.100621
38.641157	1250.119299	18.105639
38.498578	1242.993814	18.110656
38.575912	1258.820943	18.115674
38.584510	1262.209141	18.120691
38.587677	1255.499615	18.125709
38.575837	1261.911098	18.130727
38.726160	1256.437826	18.135744
38.490900	1258.885692	18.140762
38.569973	1260.328409	18.145779
38.612031	1261.164664	18.150797
38.902125	1263.994639	18.155815
38.842210	1250.648816	18.160832
39.070664	1247.804788	18.165850
39.193784	1241.562585	18.170867
39.546470	1237.257016	18.175885
39.684625	1240.508273	18.180903
39.900370	1228.012640	18.185920
39.653994	1239.645605	18.190938
39.648353	1223.394330	18.195955
39.284538	1211.358171	18.200973
39.133675	1217.377874	18.205991
39.400380	1207.534655	18.211008
39.658180	1213.579092	18.216026
39.644589	1201.251727	18.221043
39.534138	1204.289221	18.226061
39.922167	1214.201319	18.231079
39.546665	1202.652978	18.236096
39.393801	1201.982708	18.241114
39.276043	1201.029262	18.246131
39.434948	1214.104424	18.251149
39.422800	1210.868674	18.256167
39.670689	1215.134787	18.261184
39.373019	1235.687703	18.266202
39.408847	1230.595182	18.271219
39.591364	1230.021016	18.276237
39.719417	1235.940494	18.281255
39.680414	1237.013431	18.286272
39.888700	1231.950863	18.291290
40.113027	1233.942163	18.296307
39.942915	1232.479316	18.301325
39.744266	1242.113544	18.306343
40.181622	1228.005507	18.311360
39.923084	1235.948082	18.316378
40.169526	1246.103147	18.321395
40.408407	1254.059803	18.326413
40.354586	1258.890452	18.331431
40.616290	1255.845586	18.336448
40.287391	1247.325842	18.341466
40.397671	1235.755494	18.346483
40.250459	1237.678409	18.351501
40.114831	1252.576171	18.356519
40.269888	1258.807033	18.361536
40.342779	1261.494099	18.366554
40.497508	1270.735653	18.371571
41.168914	1256.019952	18.376589
40.750824	1257.574789	18.381607
41.156550	1264.173723	18.386624
40.616121	1259.341329	18.391642
40.878209	1257.025393	18.396659
40.776986	1260.212939	18.401677
40.428705	1248.111220	18.406695
40.390234	1257.528014	18.411712
40.721527	1259.016669	18.416730
40.526519	1261.152155	18.421747
40.806095	1268.771121	18.426765
40.867391	1281.602754	18.431783
41.194562	1287.488092	18.436800
41.129023	1284.317446	18.441818
41.215855	1283.076522	18.446835
41.071467	1285.551268	18.451853
41.285234	1286.638501	18.456871
41.520853	1282.089216	18.461888
41.657491	1280.250402	18.466906
41.671615	1285.632213	18.471923
42.015467	1275.051111	18.476941
41.371286	1273.485346	18.481959
41.621693	1276.356215	18.486976
41.653918	1280.179394	18.491994
41.575153	1281.861283	18.497011
41.723924	1279.067526	18.502029
41.322882	1276.678109	18.507047
41.208169	1280.539945	18.512064
41.571945	1280.366746	18.517082
41.403679	1278.417614	18.522099
41.775237	1274.014423	18.527117
41.883459	1275.758717	18.532135
41.897082	1273.159572	18.537152
42.015085	1295.118444	18.542170
41.974554	1289.621228	18.547187
42.052113	1294.522950	18.552205
41.677763	1303.117904	18.557223
41.924992	1298.658325	18.562240
42.319727	1302.437691	18.567258
42.231068	1305.515991	18.572275
42.168155	1300.729159	18.577293
42.157093	1302.804452	18.582311
42.171298	1303.960627	18.587328
42.171913	1308.129561	18.592346
42.035025	1306.939247	18.597363
42.732360	1304.748043	18.602381
42.285662	1304.701031	18.607399
42.251527	1299.673033	18.612416
42.584736	1312.304561	18.617434
42.574858	1323.345337	18.622451
42.635917	1326.602302	18.627469
42.467035	1330.374752	18.632487
42.971437	1331.246323	18.637504
42.846064	1329.479856	18.642522
42.512017	1333.599916	18.647539
42.917380	1326.603680	18.652557
42.983534	1329.935592	18.657575
43.091635	1324.437315	18.662592
43.149711	1318.047422	18.667610
43.019147	1317.894385	18.672627
42.992970	1316.197681	18.677645
43.023814	1322.141791	18.682663
42.981321	1322.492594	18.687680
43.120677	1321.849406	18.692698
43.086119	1328.359123	18.697715
43.227300	1324.922755	18.702733
43.229729	1330.811331	18.707751
43.167265	1322.559338	18.712768
43.477825	1328.311576	18.717786
43.492830	1337.704307	18.722803
44.004499	1339.445752	18.727821
43.593375	1336.038568	18.732839
43.573820	1336.278503	18.737856
43.616926	1333.097245	18.742874
43.485255	1337.725441	18.747891
43.721069	1332.361912	18.752909
43.791442	1339.445434	18.757927
43.590465	1337.261546	18.762944
43.596633	1333.104580	18.767962
43.695930	1336.447112	18.772979
43.945030	1325.685071	18.777997
43.994384	1329.682320	18.783015
43.990171	1330.462666	18.788032
44.179202	1328.846064	18.793050
43.975704	1329.351324	18.798067
44.216195	1318.912521	18.803085
44.125778	1324.862888	18.808103
44.108173	1331.682393	18.813120
44.521584	1339.394162	18.818138
44.286581	1351.795449	18.823155
44.854577	1341.826352	18.828173
44.674978	1345.215464	18.833191
44.472759	1333.750512	18.838208
44.627245	1330.009113	18.843226
44.663707	1328.996935	18.848243
45.113984	1318.153084	18.853261
44.508376	1321.756843	18.858279
44.612863	1311.298194	18.863296
44.742519	1316.583131	18.868314
44.505871	1328.637520	18.873331
44.910925	1336.382146	18.878349
44.791492	1335.138619	18.883367
44.956548	1342.336789	18.888384
45.059389	1330.038544	18.893402
44.272449	1340.657516	18.898419
44.315833	1338.845838	18.903437
45.016512	1341.100655	18.908455
44.963918	1344.545733	18.913472
45.440812	1351.471292	18.918490
45.104858	1352.126564	18.923507
45.127159	1348.210081	18.928525
45.544445	1364.643941	18.933543
45.594826	1367.871018	18.938560
45.241935	1344.655150	18.943578
45.117893	1359.472303	18.948595
45.451422	1352.013869	18.953613
45.601120	1368.543044	18.958631
45.595062	1362.106315	18.963648
45.631761	1355.700802	18.968666
45.508360	1372.228319	18.973683
45.726475	1356.929856	18.978701
45.607297	1354.105222	18.983719
45.687497	1353.512269	18.988736
45.367621	1359.006065	18.993754
45.353762	1362.826970	18.998771
45.618610	1363.344518	19.003789
45.750254	1379.198013	19.008807
45.854008	1381.113427	19.013824
45.982819	1379.323158	19.018842
46.088793	1387.919108	19.023859
46.141828	1374.290517	19.028877
46.605309	1387.091166	19.033895
46.353907	1381.598351	19.038912
46.081307	1390.060739	19.043930
46.049911	1378.695394	19.048947
46.077117	1378.871244	19.053965
46.416435	1387.853744	19.058983
46.705947	1402.136325	19.064000
47.155790	1395.379292	19.069018
46.700596	1391.773830	19.074035
46.950006	1379.970286	19.079053
46.701185	1374.448670	19.084071
46.461458	1374.905923	19.089088
46.891365	1376.795802	19.094106
46.862906	1379.874210	19.099123
47.014243	1372.595613	19.104141
47.130756	1374.231328	19.109159
46.784062	1372.833832	19.114176
47.144666	1390.573585	19.119194
46.794665	1396.861039	19.124211
47.056572	1397.704097	19.129229
46.838630	1400.998203	19.134247
46.727480	1408.633883	19.139264
47.026096	1403.639254	19.144282
46.953712	1409.665737	19.149299
46.971063	1408.593414	19.154317
47.670586	1421.306843	19.159335
47.108469	1427.093998	19.164352
47.448164	1431.689855	19.169370
47.615175	1433.484972	19.174387
47.761673	1427.119142	19.179405
47.903885	1427.829358	19.184423
47.643391	1431.322601	19.189440
48.042081	1430.635875	19.194458
47.908831	1428.577132	19.199475
47.869414	1436.889626	19.204493
47.758565	1423.605253	19.209511
47.496694	1426.858866	19.214528
47.645268	1420.189756	19.219546
47.907121	1427.559084	19.224563
47.818799	1433.379772	19.229581
47.818735	1430.782735	19.234599
47.755492	1429.218025	19.239616
48.132758	1433.312567	19.244634
48.027202	1447.937564	19.249651
48.333897	1455.659687	19.254669
48.297860	1451.225239	19.259687
48.268145	1455.316878	19.264704
48.618155	1454.685069	19.269722
48.498575	1460.788346	19.274739
48.711951	1453.048773	19.279757
48.830757	1450.098707	19.284775
48.765767	1444.756732	19.289792
48.937887	1442.110794	19.294810
48.664211	1446.729570	19.299827
48.480533	1446.720502	19.304845
48.561457	1455.162592	19.309863
48.859740	1448.059904	19.314880
48.838129	1445.567206	19.319898
49.049864	1449.239396	19.324915
48.923482	1451.193804	19.329933
49.082292	1443.516380	19.334951
48.930486	1446.702367	19.339968
48.879542	1436.151079	19.344986
48.779849	1445.893088	19.350003
48.825399	1439.965853	19.355021
49.174360	1461.535517	19.360039
49.329125	1466.655642	19.365056
49.331319	1469.164397	19.370074
49.581786	1478.779321	19.375091
49.489760	1478.105879	19.380109
49.471574	1472.399999	19.385127
49.637754	1481.207528	19.390144
49.455051	1468.126816	19.395162
49.575256	1470.506743	19.400179
49.554771	1471.750381	19.405197
49.677056	1471.895650	19.410215
49.402968	1469.637921	19.415232
49.624371	1474.290076	19.420250
50.104719	1481.174122	19.425267
50.094327	1478.272569	19.430285
50.433287	1480.927711	19.435303
50.196810	1475.517751	19.440320
50.306290	1479.032296	19.445338
50.461541	1466.283979	19.450355
49.952474	1456.633993	19.455373
50.415516	1460.276525	19.460391
50.193693	1475.389867	19.465408
50.117023	1475.654475	19.470426
50.381734	1471.968469	19.475443
50.270599	1491.760482	19.480461
50.673165	1475.420174	19.485479
50.377111	1480.518974	19.490496
50.186929	1482.609553	19.495514
50.657987	1475.568317	19.500531
50.719243	1481.643446	19.505549
50.590496	1472.499133	19.510567
50.892351	1490.980288	19.515584
50.732970	1497.550527	19.520602
50.878939	1503.369474	19.525619
50.938993	1512.490192	19.530637
51.441717	1499.649882	19.535655
51.215242	1500.325984	19.540672
51.187061	1504.985448	19.545690
51.480014	1506.625262	19.550707
51.328927	1503.022922	19.555725
51.704340	1499.502714	19.560743
51.724228	1504.905785	19.565760
51.210391	1484.043808	19.570778
51.176614	1496.899866	19.575795
51.029634	1504.332879	19.580813
51.202888	1501.134483	19.585831
51.346959	1505.830246	19.590848
51.143263	1504.789176	19.595866
51.405248	1508.696554	19.600883
51.608019	1515.115740	19.605901
51.710673	1521.376943	19.610919
51.366341	1532.135401	19.615936
51.464009	1526.338881	19.620954
51.401443	1520.210699	19.625971
51.237744	1530.496057	19.630989
52.006338	1543.473380	19.636007
52.077421	1547.858620	19.641024
52.318753	1544.526539	19.646042
52.422240	1548.266096	19.651059
52.250607	1546.617264	19.656077
52.500713	1541.349279	19.661095
52.504718	1541.519275	19.666112
52.312721	1530.765827	19.671130
52.526712	1544.261851	19.676147
52.320672	1546.197114	19.681165
52.374054	1541.928605	19.686183
52.567440	1540.387046	19.691200
52.405344	1541.049970	19.696218
52.597818	1535.342829	19.701235
52.747311	1540.959265	19.706253
53.018152	1540.204077	19.711271
52.677556	1538.994970	19.716288
53.049319	1535.936077	19.721306
52.760660	1536.075899	19.726323
52.809633	1555.596899	19.731341
53.346711	1548.273952	19.736359
53.086390	1565.735008	19.741376
53.218260	1559.118941	19.746394
53.597402	1552.852547	19.751411
53.368732	1558.553114	19.756429
53.742798	1561.370062	19.761447
53.563973	1552.501752	19.766464
53.305875	1550.118445	19.771482
53.777796	1551.847166	19.776499
53.356433	1562.459842	19.781517
54.011111	1558.189230	19.786535
53.545359	1559.413837	19.791552
53.141475	1561.162151	19.796570
53.658203	1560.321341	19.801587
53.606163	1557.091740	19.806605
53.967549	1559.178504	19.811623
53.482469	1562.915025	19.816640
53.551126	1562.317550	19.821658
54.137315	1565.420214	19.826675
53.882359	1579.207031	19.831693
53.994764	1576.447293	19.836711
54.064549	1576.802711	19.841728
53.677177	1582.095642	19.846746
53.692186	1577.795228	19.851763
54.123259	1587.435741	19.856781
54.454249	1597.918677	19.861799
54.387914	1603.174253	19.866816
54.358717	1614.142476	19.871834
54.738622	1611.274811	19.876851
54.587548	1606.785650	19.881869
54.925208	1597.511849	19.886887
54.781554	1597.859474	19.891904
54.748041	1601.847594	19.896922
55.336590	1593.393128	19.901939
54.924824	1595.928482	19.906957
55.269989	1599.235939	19.911975
54.992146	1596.129851	19.916992
54.693374	1606.010242	19.922010
55.020351	1595.646177	19.927027
55.020282	1603.110007	19.932045
55.600016	1593.681751	19.937063
55.454271	1595.856945	19.942080
55.390662	1604.428909	19.947098
55.440603	1587.796255	19.952115
55.411538	1590.802208	19.957133
55.258051	1591.779379	19.962151
55.487824	1583.983547	19.967168
55.440824	1590.990768	19.972186
56.168776	1587.330445	19.977203
55.584560	1602.831683	19.982221
55.520429	1596.407068	19.987239
55.510419	1609.209012	19.992256
55.736505	1617.770593	19.997274
55.987266	1612.272107	20.002291
55.994350	1619.756921	20.007309
55.934401	1617.374313	20.012327
55.788626	1615.973918	20.017344
55.934992	1616.298478	20.022362
56.473841	1612.080602	20.027379
55.885136	1611.534980	20.032397
55.738641	1615.209329	20.037415
56.144042	1624.232153	20.042432
56.199071	1636.348635	20.047450
56.545582	1627.985487	20.052467
56.268241	1637.133552	20.057485
56.567304	1633.625205	20.062503
56.863399	1635.627468	20.067520
56.386736	1640.053830	20.072538
56.405672	1629.396872	20.077555
56.471061	1646.245550	20.082573
56.823404	1657.230136	20.087591
57.559744	1647.925796	20.092608
56.902677	1650.000722	20.097626
57.329353	1645.992811	20.102643
57.132307	1647.465927	20.107661
57.145843	1645.043471	20.112679
57.316220	1648.892557	20.117696
57.325683	1647.770954	20.122714
57.551294	1660.495223	20.127731
57.330823	1655.777009	20.132749
57.753182	1652.277864	20.137767
57.939503	1658.889015	20.142784
57.283435	1654.042957	20.147802
57.354488	1651.008773	20.152819
57.531070	1648.223252	20.157837
57.417988	1659.924102	20.162855
57.381700	1650.427623	20.167872
57.707788	1665.376922	20.172890
58.040290	1673.701050	20.177907
57.872449	1674.724642	20.182925
58.042004	1670.381210	20.187943
58.376203	1676.596950	20.192960
58.030592	1680.693642	20.197978
58.020623	1664.325871	20.202995
58.259528	1674.416082	20.208013
58.193795	1675.045072	20.213031
58.525518	1671.455891	20.218048
58.017082	1681.460487	20.223066
58.406293	1679.241473	20.228083
58.523306	1682.884276	20.233101
58.901835	1695.401722	20.238119
58.810029	1698.341720	20.243136
58.590991	1705.940674	20.248154
58.823673	1687.843549	20.253171
58.584535	1700.353021	20.258189
59.126792	1692.325449	20.263207
59.238218	1688.107829	20.268224
59.168394	1685.796178	20.273242
59.074687	1684.838961	20.278259
59.115226	1676.532897	20.283277
58.973355	1686.139589	20.288295
59.289360	1685.544625	20.293312
58.919442	1688.846667	20.298330
59.142480	1682.550883	20.303347
59.057432	1684.167514	20.308365
59.185323	1694.713688	20.313383
59.091851	1700.557355	20.318400
59.617912	1715.942632	20.323418
59.828214	1707.105181	20.328435
60.275334	1719.753978	20.333453
59.896400	1713.280502	20.338471
59.976248	1711.264288	20.343488
59.915774	1718.911145	20.348506
60.026821	1711.603969	20.353523
59.640932	1708.347422	20.358541
59.798396	1713.858527	20.363559
59.960085	1708.995589	20.368576
59.199358	1719.042643	20.373594
59.551048	1729.632890	20.378611
60.232622	1738.126767	20.383629
60.136597	1740.521461	20.388647
60.040599	1732.811000	20.393664
60.222589	1744.024139	20.398682
60.353668	1750.120047	20.403699
60.762379	1758.744783	20.408717
60.800643	1758.196216	20.413735
60.825429	1760.436399	20.418752
60.570170	1763.692199	20.423770
60.619817	1758.770951	20.428787
60.983331	1759.834899	20.433805
61.059870	1757.806571	20.438823
61.372041	1758.897449	20.443840
61.291736	1753.163279	20.448858
61.414318	1750.591283	20.453875
61.525046	1752.048047	20.458893
61.081060	1754.834599	20.463911
61.177931	1748.716230	20.468928
60.950187	1753.403674	20.473946
61.056786	1750.499642	20.478963
61.869340	1764.821003	20.483981
61.638845	1775.650248	20.488999
61.685937	1767.071714	20.494016
61.562058	1782.397290	20.499034
61.949681	1767.327712	20.504051
62.080145	1763.321712	20.509069
61.739814	1778.018247	20.514087
62.164229	1769.999520	20.519104
61.922684	1772.770335	20.524122
62.234142	1766.520717	20.529139
62.271857	1770.280029	20.534157
61.816581	1767.835870	20.539175
61.744510	1758.467985	20.544192
62.194881	1765.479889	20.549210
62.403599	1780.346570	20.554227
62.686492	1784.815659	20.559245
62.363596	1785.601460	20.564263
62.740147	1785.407333	20.569280
62.716078	1789.113150	20.574298
62.628823	1788.508384	20.579315
62.619229	1782.725325	20.584333
62.836441	1788.306048	20.589351
63.217751	1779.451404	20.594368
62.892875	1790.396341	20.599386
62.647820	1795.054932	20.604403
62.899927	1783.244390	20.609421
62.631058	1800.025332	20.614439
62.792197	1799.261968	20.619456
63.140732	1810.187279	20.624474
62.960975	1811.077031	20.629491
63.797227	1806.677102	20.634509
63.614680	1810.795774	20.639527
63.315963	1806.209626	20.644544
63.186875	1811.632829	20.649562
63.581496	1806.528464	20.654579
63.607402	1809.737341	20.659597
63.417460	1812.604272	20.664615
63.825143	1820.945167	20.669632
63.852495	1821.474459	20.674650
63.680699	1829.968698	20.679667
63.993470	1824.520455	20.684685
63.987248	1833.168803	20.689703
63.974403	1826.616195	20.694720
64.274664	1835.065343	20.699738
64.164440	1833.773008	20.704755
64.514508	1827.520513	20.709773
64.275388	1833.992835	20.714791
64.286957	1833.792415	20.719808
64.223030	1832.944166	20.724826
64.147438	1838.100264	20.729843
64.538602	1849.539687	20.734861
64.718933	1850.603758	20.739879
65.209001	1853.737219	20.744896
64.926604	1851.581723	20.749914
65.092313	1852.376663	20.754931
65.114266	1840.179027	20.759949
65.269963	1842.174769	20.764967
65.368975	1840.976092	20.769984
65.385530	1851.552317	20.775002
65.188797	1848.745991	20.780019
65.745590	1834.782988	20.785037
65.103825	1856.889247	20.790055
65.589363	1840.636676	20.795072
65.645481	1846.517063	20.800090
65.522945	1850.597998	20.805107
65.745812	1835.033290	20.810125
65.380849	1851.501027	20.815143
65.531251	1844.197138	20.820160
65.693041	1850.477653	20.825178
65.279646	1862.001323	20.830195
65.671132	1865.314242	20.835213
65.728250	1874.968951	20.840231
66.074294	1865.864126	20.845248
66.233655	1863.955440	20.850266
66.078241	1865.775554	20.855283
66.262940	1864.096460	20.860301
66.225370	1875.552157	20.865319
66.479011	1883.355313	20.870336
66.536758	1893.035181	20.875354
66.193017	1898.068938	20.880371
66.563350	1892.788443	20.885389
66.665584	1891.134810	20.890407
66.961534	1890.034861	20.895424
66.697501	1889.861571	20.900442
66.613557	1892.042958	20.905459
67.148344	1883.173835	20.910477
66.648544	1886.126892	20.915495
66.699723	1890.764633	20.920512
67.515167	1906.196540	20.925530
67.291485	1912.369830	20.930547
67.556315	1902.715877	20.935565
67.198418	1899.697942	20.940583
67.867639	1898.943833	20.945600
68.274030	1898.123344	20.950618
67.459520	1889.480076	20.955635
67.525388	1876.716980	20.960653
67.479355	1879.217522	20.965671
67.772050	1895.538723	20.970688
68.299133	1898.019466	20.975706
67.763192	1898.175699	20.980723
67.957561	1898.975647	20.985741
67.999609	1902.627011	20.990759
68.129594	1895.521946	20.995776
68.146403	1902.595096	21.000794
67.620943	1900.398540	21.005811
67.975647	1893.656134	21.010829
68.048885	1900.376502	21.015847
67.851637	1893.675849	21.020864
68.226503	1908.210645	21.025882
68.357167	1925.200907	21.030899
68.605327	1923.650788	21.035917
68.995058	1938.401052	21.040935
68.297433	1934.034775	21.045952
68.712250	1930.053895	21.050970
68.691100	1926.207169	21.055987
68.725799	1916.749991	21.061005
68.581859	1921.285570	21.066023
69.050826	1932.630879	21.071040
69.366726	1931.849725	21.076058
68.964623	1940.237858	21.081075
69.074884	1937.932851	21.086093
68.799698	1937.600345	21.091111
68.776844	1948.927561	21.096128
69.337655	1954.110844	21.101146
69.115334	1961.622051	21.106163
69.530349	1955.110082	21.111181
69.806688	1949.392908	21.116199
69.417805	1963.850993	21.121216
69.881974	1962.980479	21.126234
69.701445	1984.866754	21.131251
70.170945	1981.035146	21.136269
70.423963	1977.473939	21.141287
70.095474	1990.489850	21.146304
70.248910	1976.056186	21.151322
70.339365	1985.772039	21.156339
70.653534	1992.735809	21.161357
70.340547	1982.445912	21.166375
70.205669	1985.323233	21.171392
70.410299	1977.584795	21.176410
70.394491	1980.377302	21.181427
70.382221	1985.507804	21.186445
70.550006	2000.980668	21.191463
70.852084	2005.175416	21.196480
70.815948	1999.005083	21.201498
70.616903	2007.658289	21.206515
70.741699	2006.657568	21.211533
71.098272	2008.379046	21.216551
70.869594	2005.287323	21.221568
71.070675	2017.479158	21.226586
71.366455	2026.572905	21.231603
71.440862	2022.187395	21.236621
71.567832	2017.481264	21.241639
71.328737	2024.313426	21.246656
71.558265	2028.166010	21.251674
71.507445	2030.828270	21.256691
71.915846	2023.651404	21.261709
71.631918	2024.538449	21.266727
71.653344	2032.646079	21.271744
72.011862	2035.828458	21.276762
72.453783	2050.592780	21.281779
72.136113	2038.754012	21.286797
72.437460	2042.705875	21.291815
72.303778	2050.673554	21.296832
72.565314	2030.510760	21.301850
72.597024	2038.796681	21.306867
72.417380	2039.017367	21.311885
72.643628	2038.524734	21.316903
72.491100	2034.348129	21.321920
73.008220	2040.096842	21.326938
72.618747	2045.667958	21.331955
72.767025	2044.976016	21.336973
72.862530	2036.680162	21.341991
72.861130	2041.887886	21.347008
73.008055	2035.559645	21.352026
73.171378	2041.139371	21.357043
73.028878	2034.231317	21.362061
72.963678	2042.980471	21.367079
73.042212	2051.517894	21.372096
73.649046	2047.241993	21.377114
73.268868	2054.541121	21.382131
73.567192	2048.927795	21.387149
73.800895	2053.846442	21.392167
73.895435	2052.831493	21.397184
73.805467	2052.937227	21.402202
73.871610	2043.478242	21.407219
74.069240	2046.751947	21.412237
74.219802	2041.707607	21.417255
74.073081	2044.523662	21.422272
74.941617	2027.627443	21.427290
74.434888	2030.710995	21.432307
74.316623	2034.365255	21.437325
74.877837	2027.653765	21.442343
74.861026	2028.603367	21.447360
74.938452	2034.010264	21.452378
75.071993	2037.341285	21.457395
74.736773	2030.008782	21.462413
75.020596	2024.953166	21.467431
74.429253	2028.930399	21.472448
74.544868	2019.987610	21.477466
74.692982	2036.738567	21.482483
74.774115	2033.232513	21.487501
75.410743	2023.069310	21.492519
75.252743	2031.757165	21.497536
75.132608	2019.900277	21.502554
75.450116	2034.103265	21.507571
75.041912	2051.032373	21.512589
75.778345	2053.228069	21.517607
75.603557	2054.852394	21.522624
75.429875	2052.553709	21.527642
75.563897	2060.271420	21.532659
75.514171	2056.252382	21.537677
75.670260	2045.075182	21.542695
75.588588	2061.742014	21.547712
75.559968	2067.272733	21.552730
75.860637	2080.717796	21.557747
75.674559	2089.949718	21.562765
76.018388	2090.013160	21.567783
75.793836	2098.976508	21.572800
76.034904	2091.525852	21.577818
76.311828	2106.047654	21.582835
76.180258	2111.925791	21.587853
76.731736	2105.231568	21.592871
76.438975	2108.799396	21.597888
76.572524	2123.668599	21.602906
76.817153	2122.999524	21.607923
76.545783	2126.134815	21.612941
76.677826	2126.903450	21.617959
76.562562	2141.451627	21.622976
77.063157	2136.636798	21.627994
77.160124	2139.967220	21.633011
77.234633	2142.654168	21.638029
77.578735	2142.607109	21.643047
77.370350	2150.460225	21.648064
77.727210	2144.146600	21.653082
77.749690	2147.794749	21.658099
77.628285	2148.527102	21.663117
77.874040	2138.765534	21.668135
77.640498	2143.031083	21.673152
77.636504	2144.013412	21.678170
77.759294	2147.888952	21.683187
77.266950	2149.565883	21.688205
78.235486	2157.074807	21.693223
78.274899	2165.571037	21.698240
78.558074	2165.886932	21.703258
78.595069	2168.526073	21.708275
78.249931	2179.733190	21.713293
78.594677	2179.897481	21.718311
78.329148	2183.325377	21.723328
78.442021	2173.025874	21.728346
78.637405	2170.319400	21.733363
78.773038	2182.306932	21.738381
79.040623	2199.686414	21.743399
79.582042	2189.597904	21.748416
79.731410	2183.313414	21.753434
79.315673	2168.232872	21.758451
79.457591	2160.592487	21.763469
79.338525	2156.218130	21.768487
79.153580	2159.968008	21.773504
79.673284	2177.267187	21.778522
79.561456	2170.609937	21.783539
79.563662	2181.008701	21.788557
80.079335	2173.433201	21.793575
79.599949	2179.769477	21.798592
79.977128	2182.450334	21.803610
79.539805	2175.247283	21.808627
79.339794	2182.392173	21.813645
80.022370	2195.010962	21.818663
80.205276	2197.157151	21.823680
80.482827	2204.234007	21.828698
80.440008	2206.077653	21.833715
80.356034	2211.516044	21.838733
80.501274	2209.423318	21.843751
80.523661	2207.911483	21.848768
80.378198	2203.923097	21.853786
80.920101	2206.777137	21.858803
80.767841	2224.512360	21.863821
80.810759	2222.362976	21.868839
80.844966	2222.878590	21.873856
81.045868	2227.537291	21.878874
80.991053	2233.479261	21.883891
80.902409	2229.005470	21.888909
81.246114	2225.912959	21.893927
81.565956	2233.330400	21.898944
81.675403	2237.801360	21.903962
81.839970	2240.692063	21.908979
81.810756	2248.694061	21.913997
82.068207	2242.500026	21.919015
81.796541	2242.791849	21.924032
81.806605	2246.031674	21.929050
81.963752	2249.860860	21.934067
81.741072	2241.163146	21.939085
81.761363	2241.062355	21.944103
82.012254	2242.427906	21.949120
82.058138	2244.828976	21.954138
82.074919	2249.822480	21.959155
81.998026	2261.631703	21.964173
82.554845	2255.409990	21.969191
82.679606	2262.624274	21.974208
82.656106	2267.324236	21.979226
82.699873	2266.045765	21.984243
82.393717	2274.782052	21.989261
82.888737	2279.006788	21.994279
82.856628	2295.151695	21.999296
83.125574	2291.638441	22.004314
83.417582	2286.707717	22.009331
83.307437	2292.936048	22.014349
83.233211	2283.580847	22.019367
83.151296	2283.401290	22.024384
83.246704	2282.155805	22.029402
83.421824	2292.821219	22.034419
83.646291	2304.899150	22.039437
83.527393	2308.525159	22.044455
84.017835	2302.020258	22.049472
83.985813	2316.492497	22.054490
83.989815	2310.681903	22.059507
83.698971	2312.103400	22.064525
83.849858	2312.414647	22.069543
84.401449	2307.677045	22.074560
84.224258	2320.508683	22.079578
85.013048	2324.798152	22.084595
84.657844	2331.086742	22.089613
84.420045	2331.231273	22.094631
84.784173	2332.225730	22.099648
85.010364	2329.094690	22.104666
85.179485	2330.798046	22.109683
84.896740	2334.629462	22.114701
85.011724	2328.672187	22.119719
84.904754	2333.467217	22.124736
84.752327	2329.284216	22.129754
84.700623	2329.857392	22.134771
85.209296	2347.644477	22.139789
85.444065	2352.600913	22.144807
85.685483	2344.256951	22.149824
85.450903	2350.795027	22.154842
85.812290	2357.489640	22.159859
85.518006	2356.588864	22.164877
85.595671	2364.735228	22.169895
85.910155	2369.619294	22.174912
85.738906	2380.190355	22.179930
86.241318	2370.290866	22.184947
86.092204	2377.876061	22.189965
86.301575	2372.879279	22.194983
86.090769	2378.713032	22.200000
86.369427	2397.069342	22.205018
86.615984	2403.264266	22.210035
86.725229	2409.856136	22.215053
86.600691	2402.083553	22.220071
86.814062	2395.934201	22.225088
86.690318	2403.685881	22.230106
87.181005	2398.632670	22.235123
87.180406	2405.017564	22.240141
87.242702	2406.254690	22.245159
87.271165	2410.773019	22.250176
87.040974	2419.866802	22.255194
87.212683	2416.611676	22.260211
87.401144	2420.495987	22.265229
87.446646	2413.397559	22.270247
87.802877	2415.223279	22.275264
87.693822	2433.810416	22.280282
87.871129	2434.335316	22.285299
88.543176	2438.125403	22.290317
87.848895	2436.769313	22.295335
88.172625	2433.651473	22.300352
87.678938	2436.464802	22.305370
87.818313	2440.337823	22.310387
88.449732	2442.174354	22.315405
88.462793	2440.490370	22.320423
88.898259	2443.853359	22.325440
88.541118	2451.221648	22.330458
89.087235	2457.032259	22.335475
88.738884	2455.376139	22.340493
88.899063	2458.071888	22.345511
88.967977	2463.830558	22.350528
88.818737	2471.447372	22.355546
89.604624	2467.676863	22.360563
89.425389	2459.988516	22.365581
89.100939	2465.716906	22.370599
89.601093	2454.362798	22.375616
89.552920	2465.839460	22.380634
89.649031	2454.210566	22.385651
89.646556	2457.928940	22.390669
89.375468	2461.749100	22.395687
90.027476	2466.697415	22.400704
89.750296	2479.276473	22.405722
89.858453	2483.129116	22.410739
89.954107	2489.098240	22.415757
89.993358	2487.656344	22.420775
90.126016	2491.918612	22.425792
90.016634	2507.949500	22.430810
90.332665	2508.686350	22.435827
90.430222	2513.844087	22.440845
90.339567	2509.534653	22.445863
90.523349	2515.938220	22.450880
90.298432	2527.950559	22.455898
90.800022	2529.131923	22.460915
91.030595	2529.658001	22.465933
90.829075	2542.149579	22.470951
91.326079	2551.007123	22.475968
91.307003	2560.762434	22.480986
91.669970	2554.264665	22.486003
91.346918	2561.040670	22.491021
91.988159	2555.449541	22.496039
92.197680	2546.955806	22.501056
92.070638	2550.602068	22.506074
91.839551	2552.920061	22.511091
92.124339	2554.968374	22.516109
91.972474	2558.634283	22.521127
92.131936	2550.362950	22.526144
92.448024	2552.273836	22.531162
92.299329	2544.893144	22.536179
92.618470	2561.021475	22.541197
92.817488	2563.910023	22.546215
93.209474	2566.762216	22.551232
92.940556	2573.933770	22.556250
92.691383	2566.215237	22.561267
93.186788	2557.317198	22.566285
93.086457	2564.869629	22.571303
93.117589	2560.200369	22.576320
93.235107	2564.799552	22.581338
92.973449	2553.172644	22.586355
93.069570	2565.056123	22.591373
93.269541	2565.826826	22.596391
93.621626	2571.045944	22.601408
93.228372	2586.663475	22.606426
93.535743	2583.765922	22.611443
93.602616	2585.052845	22.616461
93.335572	2587.404845	22.621479
93.480229	2591.419099	22.626496
93.766005	2598.128731	22.631514
94.085017	2601.257398	22.636531
94.326744	2611.783234	22.641549
94.392129	2621.822096	22.646567
94.704495	2625.409429	22.651584
94.446793	2628.968744	22.656602
94.644012	2629.683069	22.661619
95.078451	2625.929374	22.666637
94.971416	2625.283473	22.671655
95.185050	2620.336457	22.676672
95.108258	2616.959027	22.681690
95.135967	2618.495065	22.686707
95.492917	2621.478964	22.691725
94.995216	2633.565404	22.696743
95.629581	2619.715958	22.701760
95.386604	2620.561939	22.706778
95.240601	2621.055125	22.711795
95.470140	2631.788013	22.716813
95.176837	2646.222297	22.721831
95.453689	2643.616686	22.726848
95.634506	2656.815735	22.731866
95.805630	2663.732606	22.736883
96.276792	2664.189670	22.741901
96.364647	2669.932832	22.746919
96.553135	2665.867100	22.751936
96.132715	2665.853860	22.756954
96.150306	2671.582714	22.761971
96.342166	2679.168601	22.766989
96.395271	2694.943966	22.772007
96.725352	2685.569791	22.777024
96.920029	2690.946007	22.782042
96.980338	2690.602280	22.787059
97.220394	2703.836325	22.792077
97.357824	2718.673857	22.797095
97.773642	2713.240863	22.802112
97.422310	2718.585323	22.807130
97.525275	2709.940830	22.812147
97.635713	2706.243876	22.817165
97.720841	2713.593910	22.822183
97.854359	2702.669145	22.827200
97.863129	2710.425574	22.832218
97.737663	2715.832705	22.837235
97.724934	2722.090202	22.842253
97.666668	2727.865602	22.847271
97.907892	2725.931456	22.852288
97.558391	2737.025981	22.857306
98.308595	2750.783442	22.862323
98.597475	2758.357414	22.867341
98.430981	2762.177133	22.872359
99.068777	2762.879677	22.877376
99.361480	2779.069129	22.882394
99.400326	2781.222038	22.887411
99.331595	2765.143300	22.892429
99.255106	2783.189195	22.897447
99.565125	2776.513383	22.902464
99.602329	2783.018768	22.907482
99.568269	2781.881777	22.912499
100.054975	2777.154156	22.917517
99.983137	2779.696713	22.922535
100.037069	2773.496310	22.927552
100.351969	2777.597719	22.932570
100.022177	2774.720436	22.937587
100.088031	2772.488514	22.942605
99.776651	2774.932655	22.947623
100.308805	2774.717451	22.952640
100.171685	2775.619547	22.957658
99.855623	2797.480573	22.962675
100.459853	2799.864221	22.967693
100.558814	2801.370245	22.972711
100.452378	2797.378806	22.977728
100.407250	2822.656738	22.982746
100.810359	2822.546839	22.987763
101.301677	2817.370326	22.992781
101.059014	2828.486146	22.997799
101.211183	2821.980073	23.002816
101.333519	2821.017562	23.007834
101.198788	2841.098786	23.012851
101.391109	2847.987179	23.017869
101.355393	2844.600155	23.022887
101.332919	2848.526869	23.027904
101.520592	2850.593493	23.032922
101.920467	2858.453209	23.037939
102.118969	2863.248162	23.042957
102.617273	2869.779627	23.047975
102.704672	2866.386055	23.052992
102.751014	2855.474770	23.058010
102.479421	2861.122466	23.063027
102.479324	2853.668013	23.068045
102.295453	2864.853604	23.073063
102.859443	2863.446755	23.078080
102.835147	2869.949123	23.083098
102.666357	2880.065618	23.088115
103.140132	2884.741972	23.093133
103.121507	2889.955780	23.098151
103.288855	2885.397784	23.103168
103.405926	2891.332147	23.108186
103.274078	2889.601248	23.113203
103.294095	2900.960264	23.118221
103.409046	2908.782305	23.123239
103.562056	2906.801908	23.128256
103.962578	2911.237187	23.133274
104.003259	2921.059136	23.138291
104.202365	2924.436924	23.143309
103.989053	2932.035504	23.148327
104.759643	2928.816444	23.153344
104.913244	2918.383929	23.158362
104.837377	2920.207544	23.163379
104.762486	2919.439852	23.168397
104.654982	2919.718750	23.173415
104.899772	2926.071936	23.178432
104.950702	2925.237313	23.183450
104.823418	2936.196367	23.188467
105.244553	2941.767796	23.193485
105.518593	2946.099688	23.198503
105.499540	2942.328163	23.203520
105.585617	2943.293356	23.208538
105.288114	2948.556913	23.213555
105.363895	2952.787117	23.218573
105.294957	2963.642421	23.223591
106.015262	2969.445017	23.228608
106.191926	2964.229081	23.233626
106.286617	2975.563893	23.238643
106.068761	2975.130912	23.243661
106.121446	2984.692227	23.248679
106.618364	2994.657798	23.253696
106.594611	2990.445140	23.258714
106.717746	2994.522801	23.263731
106.919639	2999.393009	23.268749
107.110898	2986.382362	23.273767
106.515724	2991.408227	23.278784
107.300908	3003.090030	23.283802
107.364977	3014.915676	23.288819
107.507121	3010.711901	23.293837
107.129737	3013.788103	23.298855
107.081732	3013.369706	23.303872
107.495645	3010.291380	23.308890
107.723493	3027.857751	23.313907
107.582714	3030.505761	23.318925
107.901797	3029.045502	23.323943
107.723951	3030.736668	23.328960
108.232704	3035.224562	23.333978
108.387874	3048.184871	23.338995
108.630427	3057.309524	23.344013
109.071456	3055.413670	23.349031
108.693976	3053.326484	23.354048
108.989891	3043.654456	23.359066
109.167170	3053.044915	23.364083
108.971517	3049.487074	23.369101
108.991366	3051.131681	23.374119
108.988293	3053.051284	23.379136
109.320235	3051.762608	23.384154
109.047901	3058.448843	23.389171
109.265584	3053.134968	23.394189
109.333632	3057.218064	23.399207
108.922582	3074.776644	23.404224
109.493561	3067.346811	23.409242
109.729441	3082.759511	23.414259
109.534291	3094.455136	23.419277
109.814573	3099.363665	23.424295
110.218318	3103.583873	23.429312
110.017560	3102.103548	23.434330
110.003914	3115.330056	23.439347
110.221686	3113.263807	23.444365
110.750834	3124.038714	23.449383
110.567461	3125.869619	23.454400
110.990289	3131.503966	23.459418
110.877294	3129.280909	23.464435
111.047833	3141.030094	23.469453
111.380666	3148.663666	23.474471
111.252361	3147.964247	23.479488
111.841554	3147.976871	23.484506
111.217766	3144.523542	23.489523
111.866453	3140.641701	23.494541
111.949877	3148.203640	23.499559
111.672944	3176.273465	23.504576
112.038610	3165.949816	23.509594
111.890031	3176.274792	23.514611
112.266318	3164.393512	23.519629
112.756662	3165.289464	23.524647
112.335877	3173.851508	23.529664
112.460963	3174.463465	23.534682
112.562006	3177.806070	23.539699
112.835242	3185.691960	23.544717
112.660647	3181.086132	23.549735
112.836954	3187.721501	23.554752
113.284343	3188.740919	23.559770
113.377422	3206.303198	23.564787
113.641036	3204.980964	23.569805
113.693444	3205.260218	23.574823
113.761043	3211.953551	23.579840
113.833789	3210.493758	23.584858
113.705025	3214.345571	23.589875
114.108688	3207.834921	23.594893
113.902024	3200.832253	23.599911
113.804644	3216.366388	23.604928
114.321438	3226.411055	23.609946
114.298512	3238.300890	23.614963
114.533738	3232.570775	23.619981
114.746563	3231.638341	23.624999
114.508743	3234.957968	23.630016
114.540189	3244.001962	23.635034
114.963110	3260.591344	23.640051
115.039703	3260.851052	23.645069
115.286604	3252.524753	23.650087
115.446465	3265.528676	23.655104
115.184961	3250.536829	23.660122
115.336548	3265.969122	23.665139
115.517887	3275.166539	23.670157
115.873640	3269.922632	23.675175
116.097461	3281.231220	23.680192
115.880886	3277.357819	23.685210
116.215986	3280.260015	23.690227
116.006723	3282.514735	23.695245
115.997519	3284.501596	23.700263
115.959009	3297.179780	23.705280
115.930148	3296.120851	23.710298
116.494779	3304.636844	23.715315
116.680672	3317.564159	23.720333
116.767729	3317.863269	23.725351
116.775494	3315.009091	23.730368
116.652262	3326.406459	23.735386
116.945396	3331.732820	23.740403
117.282469	3331.547985	23.745421
117.775896	3338.926236	23.750439
117.415839	3344.534200	23.755456
118.007419	3339.379803	23.760474
117.951825	3340.868906	23.765491
117.558067	3347.129133	23.770509
118.124829	3350.108894	23.775527
118.151044	3367.261969	23.780544
118.069676	3361.464326	23.785562
118.373895	3366.233486	23.790579
118.359181	3358.487576	23.795597
118.609244	3380.002361	23.800615
118.816292	3395.766997	23.805632
119.123822	3386.642153	23.810650
119.202885	3384.319726	23.815667
119.242745	3378.247553	23.820685
119.704851	3375.537247	23.825703
119.499794	3380.710788	23.830720
119.692886	3386.308392	23.835738
119.617661	3380.418257	23.840755
119.614577	3396.051488	23.845773
119.999856	3393.173240	23.850791
119.933008	3411.177233	23.855808
120.225543	3407.442316	23.860826
120.276973	3398.770798	23.865843
119.944876	3405.999861	23.870861
120.216832	3415.823946	23.875879
119.992279	3424.260871	23.880896
120.375157	3426.398168	23.885914
120.506802	3438.077854	23.890931
120.629847	3447.915673	23.895949
120.981751	3447.179352	23.900967
120.880651	3453.245709	23.905984
121.605875	3472.003865	23.911002
121.601164	3473.134719	23.916019
121.182423	3476.927581	23.921037
121.458395	3475.729652	23.926055
121.817972	3487.247635	23.931072
121.913686	3489.707394	23.936090
122.703717	3499.952701	23.941107
122.760538	3498.684735	23.946125
123.006072	3483.484348	23.951143
122.941097	3480.625688	23.956160
123.103052	3464.851277	23.961178
122.933194	3461.664924	23.966195
122.960866	3463.923808	23.971213
123.154320	3468.804927	23.976231
123.701058	3481.269030	23.981248
123.712040	3460.856430	23.986266
124.302896	3444.352460	23.991283
123.982054	3433.977732	23.996301
124.333130	3435.337248	24.001319
123.962498	3439.820129	24.006336
123.995384	3430.154128	24.011354
123.957120	3431.211299	24.016371
123.884062	3438.314827	24.021389
123.907721	3435.764306	24.026407
123.959982	3451.104912	24.031424
124.442513	3462.550081	24.036442
124.553185	3459.913416	24.041459
124.594264	3459.964036	24.046477
124.617069	3458.265815	24.051495
124.421594	3468.655071	24.056512
124.406641	3472.085228	24.061530
124.622335	3484.263162	24.066547
124.750507	3493.907680	24.071565
124.984508	3496.431127	24.076583
125.069576	3509.058658	24.081600
124.942117	3516.918706	24.086618
125.485260	3531.450715	24.091635
125.647605	3535.866421	24.096653
125.775600	3530.891458	24.101671
125.810750	3544.511521	24.106688
125.941598	3557.365518	24.111706
126.032816	3560.902253	24.116723
125.793303	3566.725077	24.121741
126.224465	3577.581794	24.126759
126.643787	3585.590302	24.131776
126.802003	3588.636867	24.136794
126.984136	3580.222660	24.141811
127.026163	3594.210966	24.146829
127.444548	3601.528416	24.151847
127.681234	3602.110388	24.156864
127.804933	3595.889371	24.161882
127.863706	3598.421177	24.166899
127.966791	3605.399504	24.171917
128.029354	3601.207982	24.176935
127.763595	3603.035980	24.181952
127.828852	3619.558287	24.186970
128.219828	3619.437651	24.191987
128.010988	3631.517658	24.197005
128.311845	3631.275335	24.202023
128.657549	3632.695670	24.207040
128.221427	3651.751607	24.212058
129.016204	3658.120423	24.217075
128.504842	3655.422765	24.222093
128.934738	3670.748950	24.227111
129.158194	3676.184105	24.232128
129.264612	3681.634329	24.237146
129.756511	3686.992975	24.242163
129.615149	3702.755313	24.247181
130.205303	3702.026075	24.252199
130.181848	3708.979956	24.257216
130.212074	3706.990183	24.262234
130.398943	3700.664609	24.267251
130.113411	3698.168501	24.272269
130.253927	3703.888014	24.277287
130.570919	3723.372800	24.282304
130.706902	3727.032004	24.287322
131.113784	3720.785793	24.292339
131.117128	3722.922248	24.297357
131.213025	3722.030088	24.302375
131.139599	3729.007538	24.307392
131.606226	3739.347521	24.312410
131.904302	3739.115099	24.317427
132.041474	3741.041346	24.322445
132.018978	3749.071371	24.327463
132.322596	3740.537174	24.332480
132.034221	3745.433416	24.337498
132.477451	3746.516641	24.342515
132.072184	3753.911889	24.347533
132.407626	3750.195471	24.352551
132.662858	3768.042364	24.357568
132.756569	3778.797085	24.362586
132.873128	3763.326169	24.367603
132.584528	3766.104612	24.372621
132.766039	3773.493730	24.377639
133.015205	3785.928626	24.382656
132.705774	3793.782406	24.387674
133.213945	3797.853959	24.392691
133.531032	3804.322451	24.397709
134.252537	3813.710639	24.402727
134.117864	3812.238903	24.407744
134.044475	3812.935440	24.412762
134.088164	3806.272308	24.417779
133.941422	3820.378554	24.422797
134.227931	3811.834363	24.427815
134.436391	3821.173025	24.432832
134.219626	3836.252844	24.437850
134.811866	3835.658996	24.442867
134.487815	3841.081600	24.447885
134.626702	3852.845647	24.452903
135.171905	3858.817829	24.457920
134.886737	3869.704187	24.462938
135.435209	3863.363289	24.467955
135.346921	3885.512108	24.472973
135.459307	3882.455332	24.477991
135.616017	3884.678397	24.483008
135.789180	3896.787482	24.488026
136.307185	3901.747595	24.493043
136.470150	3905.797168	24.498061
136.470915	3910.525343	24.503079
136.601811	3906.821802	24.508096
136.182152	3917.309345	24.513114
136.840842	3925.470113	24.518131
136.904318	3935.077596	24.523149
137.234906	3938.517168	24.528167
137.206424	3935.838974	24.533184
137.322534	3952.722952	24.538202
137.780723	3961.782929	24.543219
137.563634	3959.102533	24.548237
137.621887	3964.607685	24.553255
137.946951	3960.056427	24.558272
138.025911	3972.076072	24.563290
138.342861	3974.125855	24.568307
138.257821	3980.148857	24.573325
138.318335	3985.196003	24.578343
138.360803	3991.246501	24.583360
138.455090	3999.785554	24.588378
138.761250	4000.950104	24.593395
139.025749	4008.840873	24.598413
139.490778	4021.131853	24.603431
139.596238	4013.101823	24.608448
139.542994	4021.218819	24.613466
139.718380	4017.978616	24.618483
139.536708	4013.354737	24.623501
140.046987	4023.088394	24.628519
140.503113	4024.734604	24.633536
140.672923	4022.375872	24.638554
140.907557	4024.526853	24.643571
140.961019	4020.573373	24.648589
141.059925	4026.081683	24.653607
141.175583	4017.343056	24.658624
141.148806	4025.159242	24.663642
141.052223	4022.813579	24.668659
141.477007	4024.240572	24.673677
141.243161	4023.399736	24.678695
141.716066	4006.683210	24.683712
141.760519	4034.656988	24.688730
142.149746	4039.801316	24.693747
141.991997	4041.890295	24.698765
141.739926	4046.257021	24.703783
142.020241	4052.049568	24.708800
142.015510	4049.367659	24.713818
142.380210	4051.788773	24.718835
142.601274	4072.311511	24.723853
142.530921	4076.343791	24.728871
142.949343	4061.617853	24.733888
142.491267	4062.039724	24.738906
142.727796	4068.107379	24.743923
142.477143	4087.182241	24.748941
142.845443	4094.813852	24.753959
143.145002	4104.059570	24.758976
143.256794	4116.964277	24.763994
143.502200	4129.671437	24.769011
144.016770	4135.765264	24.774029
143.795329	4145.199433	24.779047
144.259831	4141.664846	24.784064
143.731243	4146.163024	24.789082
144.287833	4155.305625	24.794099
144.384587	4163.623430	24.799117
144.736381	4170.039305	24.804135
145.041690	4174.638070	24.809152
145.213578	4182.682212	24.814170
145.597979	4178.235288	24.819187
145.542242	4174.216712	24.824205
145.481150	4184.547580	24.829223
146.035339	4186.304791	24.834240
146.337590	4207.720905	24.839258
146.610751	4211.573481	24.844275
146.444545	4204.037017	24.849293
146.550940	4216.396591	24.854311
146.488946	4204.993189	24.859328
146.606500	4211.726462	24.864346
146.627897	4203.220206	24.869363
146.663629	4216.755465	24.874381
146.846902	4231.132596	24.879399
147.134986	4221.830449	24.884416
147.139501	4235.960815	24.889434
147.356157	4248.407404	24.894451
147.388186	4257.366594	24.899469
147.378300	4259.644051	24.904487
147.999035	4263.123734	24.909504
148.180793	4282.245107	24.914522
148.114363	4280.567015	24.919539
148.281755	4278.565292	24.924557
148.156102	4286.848341	24.929575
148.753849	4296.723189	24.934592
148.662084	4311.266301	24.939610
148.561531	4311.503104	24.944627
148.653642	4325.260079	24.949645
149.342746	4337.939338	24.954663
149.372930	4334.327143	24.959680
149.335063	4339.288701	24.964698
149.870268	4352.288628	24.969715
149.877565	4353.367166	24.974733
149.973920	4359.065356	24.979751
150.652912	4362.236135	24.984768
150.724241	4362.995383	24.989786
150.693351	4373.043898	24.994803
150.767434	4372.145633	24.999821
150.990635	4370.012114	25.004839
151.044056	4371.282323	25.009856
151.402392	4369.560184	25.014874
151.132202	4378.471797	25.019891
151.374448	4384.254597	25.024909
151.255110	4398.306526	25.029927
151.287391	4392.853837	25.034944
151.651456	4409.204090	25.039962
151.506747	4416.224466	25.044979
151.936503	4418.667065	25.049997
152.057468	4427.571461	25.055015
152.272156	4433.052400	25.060032
152.541004	4445.547813	25.065050
152.747577	4447.785280	25.070067
152.570923	4448.295911	25.075085
152.363814	4458.788549	25.080103
152.800217	4461.848766	25.085120
152.670646	4468.548013	25.090138
153.083731	4492.570150	25.095155
153.370351	4490.493027	25.100173
153.457269	4496.666185	25.105191
153.977228	4510.224121	25.110208
154.098400	4514.438157	25.115226
154.217322	4515.234190	25.120243
154.496507	4517.545583	25.125261
154.246685	4524.017375	25.130279
154.529348	4526.647021	25.135296
155.083728	4530.001363	25.140314
154.870400	4540.728589	25.145331
155.278904	4542.038217	25.150349
155.539479	4553.114622	25.155367
155.714052	4559.444599	25.160384
155.912714	4571.307125	25.165402
155.842411	4570.737499	25.170419
155.941382	4567.357589	25.175437
155.965666	4579.184141	25.180455
156.044715	4592.539336	25.185472
156.593110	4582.192745	25.190490
156.214845	4600.959752	25.195507
156.494361	4601.973828	25.200525
157.123918	4612.689809	25.205543
156.867481	4604.138242	25.210560
156.998027	4610.149984	25.215578
157.414249	4614.434893	25.220595
157.984166	4621.183111	25.225613
157.911438	4628.242865	25.230631
158.173941	4624.556565	25.235648
158.075634	4628.848988	25.240666
158.255963	4626.668455	25.245683
158.683632	4634.600379	25.250701
158.794396	4657.495624	25.255719
158.848443	4651.524977	25.260736
158.974903	4658.222308	25.265754
158.772398	4654.355888	25.270771
159.575307	4645.569930	25.275789
159.036703	4666.378905	25.280807
159.709593	4678.180294	25.285824
159.350863	4673.915234	25.290842
159.726726	4676.972288	25.295859
160.118565	4684.884561	25.300877
159.692971	4700.720427	25.305895
159.770641	4700.572813	25.310912
159.861626	4698.403026	25.315930
159.886883	4717.486096	25.320947
160.411500	4728.183763	25.325965
160.569693	4741.605656	25.330983
160.714233	4744.455693	25.336000
161.054728	4758.979212	25.341018
160.720096	4768.355572	25.346035
161.300200	4766.090687	25.351053
161.673265	4788.017273	25.356071
161.654294	4794.983499	25.361088
162.417866	4783.792093	25.366106
162.462318	4789.523750	25.371123
162.902293	4779.282309	25.376141
162.995213	4785.656642	25.381159
163.056418	4778.210789	25.386176
163.177528	4770.364217	25.391194
163.286088	4793.392547	25.396211
163.773994	4796.855139	25.401229
163.619585	4796.721562	25.406247
163.247775	4801.056608	25.411264
163.533021	4797.906480	25.416282
163.365202	4805.760744	25.421299
163.623071	4811.143539	25.426317
163.984303	4818.656613	25.431335
163.963966	4833.488885	25.436352
164.340420	4823.825465	25.441370
164.429863	4841.437246	25.446387
164.527028	4849.594325	25.451405
164.935401	4862.977356	25.456423
164.911752	4861.964870	25.461440
165.097142	4874.069550	25.466458
164.918187	4878.516627	25.471475
165.147135	4884.607833	25.476493
165.335012	4897.517032	25.481511
165.472372	4909.386167	25.486528
165.407438	4926.318179	25.491546
165.926674	4932.184288	25.496563
166.080775	4948.021652	25.501581
166.211342	4958.711365	25.506599
166.489205	4956.641867	25.511616
167.144605	4972.874673	25.516634
166.884436	4974.540956	25.521651
167.175188	4971.730839	25.526669
167.557562	4979.770973	25.531687
167.124523	4990.775718	25.536704
167.662428	5000.616079	25.541722
168.021766	4999.733345	25.546739
168.239921	5000.883256	25.551757
168.316431	5009.697009	25.556775
168.353311	5023.513616	25.561792
168.699225	5025.300183	25.566810
168.752001	5030.651845	25.571827
168.839826	5036.522025	25.576845
169.381633	5041.349335	25.581863
169.643383	5049.900689	25.586880
169.670406	5045.338748	25.591898
169.782643	5044.759626	25.596915
170.016739	5049.982057	25.601933
170.382717	5054.019221	25.606951
170.521328	5064.250056	25.611968
170.880126	5056.325320	25.616986
170.343109	5066.623468	25.622003
170.539710	5065.090583	25.627021
170.659855	5067.527815	25.632039
170.763105	5082.353674	25.637056
171.031483	5084.714170	25.642074
171.136572	5098.217193	25.647091
171.188902	5113.878003	25.652109
171.544918	5112.162471	25.657127
171.314787	5120.080231	25.662144
171.763553	5133.599216	25.667162
171.733650	5147.659895	25.672180
172.203848	5154.695298	25.677197
172.603053	5167.401338	25.682215
172.373979	5178.125077	25.687232
172.536640	5181.559469	25.692250
172.668765	5189.143089	25.697268
173.262241	5192.734520	25.702285
173.627931	5210.199486	25.707303
173.890932	5222.036638	25.712320
174.206925	5211.353409	25.717338
174.154123	5219.208883	25.722356
174.122003	5219.728597	25.727373
174.264484	5216.445957	25.732391
174.531535	5228.746488	25.737408
174.531216	5236.925231	25.742426
174.282960	5235.717268	25.747444
174.557044	5245.507299	25.752461
175.271572	5257.176324	25.757479
175.373801	5264.635214	25.762496
175.409391	5265.198048	25.767514
175.305429	5269.440998	25.772532
175.624438	5274.558735	25.777549
175.613592	5287.742203	25.782567
175.733128	5287.979474	25.787584
176.363918	5301.492340	25.792602
176.389363	5313.571711	25.797620
176.268458	5326.661864	25.802637
176.831618	5327.988508	25.807655
176.980312	5337.750763	25.812672
177.393069	5344.558444	25.817690
176.806631	5356.717325	25.822708
177.317623	5362.657458	25.827725
177.427092	5368.906315	25.832743
177.764004	5381.451751	25.837760
178.210512	5377.045374	25.842778
178.230557	5390.937481	25.847796
178.444303	5385.734017	25.852813
178.803893	5397.657255	25.857831
178.798294	5410.189750	25.862848
179.078611	5417.800898	25.867866
179.073405	5412.855629	25.872884
179.121103	5426.869720	25.877901
179.580382	5439.727581	25.882919
179.442436	5437.460774	25.887936
180.226702	5441.091996	25.892954
180.157018	5447.397181	25.897972
180.045526	5452.143235	25.902989
180.055133	5458.448706	25.908007
180.045695	5472.026655	25.913024
180.645881	5473.798932	25.918042
180.878252	5496.837286	25.923060
180.804915	5496.324921	25.928077
181.208465	5505.940265	25.933095
181.244468	5518.734664	25.938112
181.760534	5528.673410	25.943130
182.110442	5534.291459	25.948148
182.313588	5541.093970	25.953165
182.450385	5544.696599	25.958183
183.477258	5548.305853	25.963200
183.646829	5526.597301	25.968218
183.653309	5529.525775	25.973236
184.070523	5535.366930	25.978253
184.329196	5526.570589	25.983271
184.042348	5525.049804	25.988288
184.355158	5513.486216	25.993306
184.082381	5512.929145	25.998324
184.184676	5527.755516	26.003341
184.159100	5524.170704	26.008359
184.615941	5527.805572	26.013376
184.198086	5515.857006	26.018394
184.551069	5533.952415	26.023412
184.422212	5544.745994	26.028429
184.651659	5559.732518	26.033447
184.835927	5566.629518	26.038464
185.238886	5577.229838	26.043482
185.126647	5592.667313	26.048500
184.924405	5613.046211	26.053517
185.551717	5622.232209	26.058535
185.833693	5626.115281	26.063552
186.063721	5633.093566	26.068570
186.225559	5644.192324	26.073588
186.301744	5664.155456	26.078605
186.496629	5663.948550	26.083623
186.845633	5681.021995	26.088640
187.111564	5686.608974	26.093658
187.200702	5684.306781	26.098676
187.223633	5695.853335	26.103693
187.639945	5708.222494	26.108711
187.583307	5709.617255	26.113728
188.198547	5717.283708	26.118746
188.372638	5727.206361	26.123764
188.676046	5725.473711	26.128781
188.617258	5723.892149	26.133799
188.939347	5753.712988	26.138816
189.023868	5750.802284	26.143834
189.346538	5750.995309	26.148852
189.145218	5779.581382	26.153869
189.391827	5771.383398	26.158887
189.856418	5779.875107	26.163904
190.045329	5790.123773	26.168922
190.118115	5802.978933	26.173940
190.329855	5805.023213	26.178957
191.060827	5804.253039	26.183975
191.088703	5811.903655	26.188992
191.183914	5820.787492	26.194010
191.506566	5823.594187	26.199028
191.642304	5821.837127	26.204045
191.607972	5821.637497	26.209063
191.621687	5844.341012	26.214080
191.843733	5838.833093	26.219098
192.358102	5843.876384	26.224116
192.240203	5856.499272	26.229133
192.783806	5860.007062	26.234151
193.305661	5866.564366	26.239168
193.126919	5864.540602	26.244186
193.508300	5867.821121	26.249204
193.079895	5872.225205	26.254221
193.478919	5876.604636	26.259239
193.358927	5893.628191	26.264256
193.982363	5907.625618	26.269274
193.810828	5905.310319	26.274292
194.321026	5924.486456	26.279309
194.595875	5936.442181	26.284327
194.837587	5931.417293	26.289344
194.728781	5942.331093	26.294362
195.042964	5946.035605	26.299380
194.917481	5975.108924	26.304397
195.068950	5972.929569	26.309415
195.485097	5986.946703	26.314432
195.449277	5997.640836	26.319450
196.117537	6007.401475	26.324468
195.756523	6020.409556	26.329485
195.994022	6024.454314	26.334503
196.399879	6042.576720	26.339520
196.461639	6040.461831	26.344538
197.208005	6064.812958	26.349556
196.916502	6064.429243	26.354573
197.411129	6067.891036	26.359591
198.251170	6066.491483	26.364608
198.711544	6072.758553	26.369626
198.855712	6072.771035	26.374644
198.641502	6072.968735	26.379661
198.886918	6063.113568	26.384679
199.183818	6063.086487	26.389696
199.222792	6058.175201	26.394714
199.441544	6065.906689	26.399732
199.460219	6071.200834	26.404749
199.722027	6082.713599	26.409767
199.577142	6084.661914	26.414784
199.794328	6096.383661	26.419802
199.831544	6094.130537	26.424820
199.739295	6102.746971	26.429837
200.201527	6113.439390	26.434855
200.418903	6123.923717	26.439872
200.239265	6132.452758	26.444890
200.393447	6143.477253	26.449908
200.691141	6168.191942	26.454925
201.002019	6169.750486	26.459943
201.313936	6179.503564	26.464960
201.535895	6187.247231	26.469978
201.580724	6200.163844	26.474996
201.821017	6217.043221	26.480013
201.941191	6219.887815	26.485031
202.095937	6219.084229	26.490048
202.433181	6231.911145	26.495066
203.036283	6243.402443	26.500084
203.007338	6260.462671	26.505101
203.007316	6259.702119	26.510119
203.370452	6273.828742	26.515136
203.870023	6284.130332	26.520154
203.888975	6280.737311	26.525172
204.027576	6306.019904	26.530189
204.478321	6316.376465	26.535207
204.731285	6314.127605	26.540224
204.647139	6335.214959	26.545242
205.146303	6338.631905	26.550260
205.362882	6346.868921	26.555277
205.645707	6353.179514	26.560295
205.674679	6363.137733	26.565312
205.852908	6373.378920	26.570330
206.257109	6367.242711	26.575348
206.166202	6391.790922	26.580365
206.398022	6395.233717	26.585383
206.326375	6403.948100	26.590400
206.376434	6413.041284	26.595418
206.894129	6425.852870	26.600436
206.947631	6454.387698	26.605453
206.810581	6455.851855	26.610471
207.211679	6470.054794	26.615488
207.431689	6491.126541	26.620506
207.734310	6499.375484	26.625524
207.962713	6512.011199	26.630541
209.110858	6501.945804	26.635559
209.587502	6513.182326	26.640576
209.571008	6515.612616	26.645594
210.065034	6504.503169	26.650612
210.235757	6512.640071	26.655629
210.000461	6511.319518	26.660647
210.224331	6513.977551	26.665664
210.812018	6523.810991	26.670682
210.900402	6522.825164	26.675700
210.643769	6528.430625	26.680717
210.901773	6527.462584	26.685735
210.957328	6533.701295	26.690752
211.447680	6561.836822	26.695770
211.648112	6552.727071	26.700788
211.763367	6566.706265	26.705805
211.733114	6559.198164	26.710823
212.313682	6559.306854	26.715840
212.246264	6574.757120	26.720858
212.286907	6577.642563	26.725876
212.346104	6588.154940	26.730893
212.357645	6600.442515	26.735911
213.129734	6605.793137	26.740928
213.108540	6625.756697	26.745946
213.446729	6632.879521	26.750964
213.619683	6635.706492	26.755981
213.507147	6646.996945	26.760999
213.937252	6653.941315	26.766016
213.907254	6665.613523	26.771034
214.114580	6668.832898	26.776052
214.249812	6683.317308	26.781069
214.493403	6685.072622	26.786087
215.098282	6709.137278	26.791104
214.854527	6719.586411	26.796122
215.284267	6728.980510	26.801140
215.730167	6731.954407	26.806157
216.004655	6728.000654	26.811175
215.990922	6747.597001	26.816192
216.438750	6768.766184	26.821210
216.360227	6762.758663	26.826228
216.675340	6775.589408	26.831245
216.826648	6779.972901	26.836263
217.422475	6792.832559	26.841280
217.413642	6817.400130	26.846298
217.725126	6811.164565	26.851316
217.694937	6815.727848	26.856333
217.734303	6836.152568	26.861351
218.268334	6840.539625	26.866368
218.636884	6872.795249	26.871386
219.024250	6865.064164	26.876404
219.118896	6869.112410	26.881421
219.349941	6891.262520	26.886439
219.328788	6888.882645	26.891456
219.241805	6901.504596	26.896474
219.802801	6910.834159	26.901492
220.161608	6911.207824	26.906509
220.728134	6913.765216	26.911527
221.416745	6922.601398	26.916544
221.546062	6919.386796	26.921562
221.429135	6920.614255	26.926580
221.860512	6921.197598	26.931597
221.823270	6917.601702	26.936615
222.232956	6918.759800	26.941632
222.290222	6941.915632	26.946650
222.279767	6937.191743	26.951668
222.443940	6940.897718	26.956685
222.450221	6951.718438	26.961703
222.658604	6959.906498	26.966720
222.749219	6968.595888	26.971738
223.008958	6976.820155	26.976756
223.121913	6990.705328	26.981773
223.295540	7008.255588	26.986791
223.649316	7019.347398	26.991808
223.578995	7040.168239	26.996826
224.142227	7047.407715	27.001844
224.004204	7068.346460	27.006861
224.223381	7077.211608	27.011879
224.553775	7097.610250	27.016896
224.795883	7111.775305	27.021914
225.408970	7124.414690	27.026932
225.558241	7133.742175	27.031949
225.669332	7146.649140	27.036967
225.908780	7154.791412	27.041984
226.612247	7170.343140	27.047002
226.726594	7169.460569	27.052020
227.052231	7175.408060	27.057037
227.531742	7186.780296	27.062055
227.553252	7191.117802	27.067072
227.738913	7203.448123	27.072090
227.790271	7196.255366	27.077108
228.133108	7214.256161	27.082125
227.893193	7216.348820	27.087143
228.446133	7225.146293	27.092160
228.760426	7246.507288	27.097178
228.855383	7243.736781	27.102196
228.966317	7251.823341	27.107213
229.414785	7264.068591	27.112231
229.545500	7270.699928	27.117248
229.754837	7271.643008	27.122266
229.854570	7284.580249	27.127284
230.413943	7292.723284	27.132301
230.586649	7299.928956	27.137319
230.897159	7296.540864	27.142336
230.488736	7317.755598	27.147354
230.697521	7319.162825	27.152372
231.234390	7331.432239	27.157389
231.130181	7348.097962	27.162407
231.313027	7359.857435	27.167424
231.573142	7379.553881	27.172442
231.707853	7382.689982	27.177460
232.035414	7402.786346	27.182477
232.365045	7429.019379	27.187495
232.984993	7430.125835	27.192512
233.037095	7448.206850	27.197530
233.053222	7452.182214	27.202548
233.425622	7471.229901	27.207565
233.454103	7482.606246	27.212583
233.662443	7493.260081	27.217600
233.978276	7508.989253	27.222618
234.709291	7527.731772	27.227636
234.759507	7532.674170	27.232653
234.950962	7550.982985	27.237671
235.483033	7557.460389	27.242688
235.477316	7570.657331	27.247706
235.669729	7581.272657	27.252724
236.133037	7582.065721	27.257741
235.868436	7602.898505	27.262759
236.288223	7609.601765	27.267776
236.452224	7628.233779	27.272794
236.706879	7647.732477	27.277812
236.975740	7653.805769	27.282829
237.484668	7673.185985	27.287847
237.350735	7684.856079	27.292864
237.643466	7702.489480	27.297882
237.730553	7709.045688	27.302900
238.533610	7719.884874	27.307917
238.887906	7739.197683	27.312935
239.487096	7730.697693	27.317952
239.569123	7741.810151	27.322970
239.489184	7740.111744	27.327988
239.991408	7749.577164	27.333005
239.990233	7749.624905	27.338023
240.475242	7752.419251	27.343040
241.219037	7767.273841	27.348058
241.306539	7769.577614	27.353076
241.640800	7766.245720	27.358093
241.590838	7763.892315	27.363111
241.984713	7768.282477	27.368128
241.978591	7769.230715	27.373146
242.439005	7783.333889	27.378164
242.750703	7779.105779	27.383181
242.578557	7792.483481	27.388199
242.553245	7786.640972	27.393216
242.787368	7807.187984	27.398234
243.001002	7815.195663	27.403252
243.380560	7817.397147	27.408269
243.543969	7846.002266	27.413287
243.939159	7848.412835	27.418304
244.109903	7861.708791	27.423322
244.037223	7864.754142	27.428340
244.248445	7873.734564	27.433357
244.462097	7894.767875	27.438375
244.897656	7897.579414	27.443392
245.150076	7901.448634	27.448410
245.452652	7919.541628	27.453428
246.056589	7915.075414	27.458445
245.915053	7916.893964	27.463463
246.113781	7933.311008	27.468480
246.370482	7934.186766	27.473498
246.198206	7955.311800	27.478516
246.821235	7964.689071	27.483533
246.718383	7973.273306	27.488551
247.139227	7984.759353	27.493568
247.616946	7995.106354	27.498586
247.864779	8010.726578	27.503604
248.061506	8006.958293	27.508621
248.489297	8028.747662	27.513639
248.642931	8036.237563	27.518656
248.890110	8043.747631	27.523674
248.891819	8065.215070	27.528692
249.194552	8061.809108	27.533709
249.264808	8091.761360	27.538727
249.433689	8104.296946	27.543744
249.931952	8117.883051	27.548762
249.882384	8123.513584	27.553780
250.572186	8143.450181	27.558797
250.819473	8166.164403	27.563815
251.271319	8177.109053	27.568832
251.671764	8176.320801	27.573850
251.512890	8198.034386	27.578868
252.139238	8196.740569	27.583885
252.320098	8203.092933	27.588903
252.621149	8213.552802	27.593920
252.886800	8222.878507	27.598938
252.951200	8219.159193	27.603956
253.347391	8236.091927	27.608973
253.170743	8251.816326	27.613991
253.711932	8265.850469	27.619008
254.253743	8275.003768	27.624026
253.800426	8290.638678	27.629044
254.467813	8290.348714	27.634061
254.501156	8312.133532	27.639079
254.570260	8322.342285	27.644096
255.366444	8336.150518	27.649114
255.386833	8351.086636	27.654132
255.666286	8357.224811	27.659149
255.694525	8378.085490	27.664167
256.078220	8388.977735	27.669184
256.339931	8393.347583	27.674202
256.439533	8411.715753	27.679220
256.952701	8423.361338	27.684237
257.123583	8439.401165	27.689255
257.607282	8463.316511	27.694272
257.750621	8465.074979	27.699290
258.038067	8474.930960	27.704308
258.569814	8482.826264	27.709325
258.265305	8496.493432	27.714343
258.304974	8508.197003	27.719360
259.142711	8524.139397	27.724378
259.365561	8534.946273	27.729396
259.927615	8542.398052	27.734413
260.457846	8558.902953	27.739431
260.414757	8559.490766	27.744448
260.906796	8563.745869	27.749466
261.032898	8577.718591	27.754484
261.394562	8578.098165	27.759501
261.410713	8580.744641	27.764519
261.373417	8593.300031	27.769536
261.706858	8600.241250	27.774554
261.723151	8608.813546	27.779572
262.417944	8615.856367	27.784589
262.238996	8629.099979	27.789607
262.418228	8636.586140	27.794624
262.697286	8638.610789	27.799642
262.843386	8662.045405	27.804660
262.993206	8676.330219	27.809677
263.269118	8688.072894	27.814695
263.347181	8709.488152	27.819712
263.947267	8731.677738	27.824730
264.171328	8741.145935	27.829748
264.251968	8756.979090	27.834765
265.045931	8768.028684	27.839783
264.912020	8795.462920	27.844800
265.385896	8801.810915	27.849818
265.405963	8823.390033	27.854836
266.028350	8829.680188	27.859853
266.274950	8842.248375	27.864871
266.430038	8854.780305	27.869888
266.947260	8869.077524	27.874906
266.798438	8889.290721	27.879924
267.278954	8894.141235	27.884941
267.637943	8907.604380	27.889959
267.626941	8924.733741	27.894976
268.449617	8931.055892	27.899994
268.498662	8953.988218	27.905012
268.704166	8961.827178	27.910029
269.118211	8974.590386	27.915047
269.300755	8981.245842	27.920064
269.890215	8984.472434	27.925082
269.953370	8998.884646	27.930100
270.281003	9010.619474	27.935117
270.695793	9020.616937	27.940135
270.943051	9027.170778	27.945152
271.208624	9036.275906	27.950170
271.357086	9037.231714	27.955188
271.746452	9051.618438	27.960205
272.350569	9061.302302	27.965223
272.277962	9070.605327	27.970240
272.741113	9076.386798	27.975258
273.175534	9095.091851	27.980276
273.285343	9083.428188	27.985293
273.465985	9102.889435	27.990311
273.545884	9110.577525	27.995328
273.951537	9111.670097	28.000346
274.164430	9129.579340	28.005364
274.399206	9139.907981	28.010381
274.755352	9150.302976	28.015399
275.012303	9170.241775	28.020416
275.391390	9170.085088	28.025434
275.036951	9179.927721	28.030452
275.520248	9194.460949	28.035469
276.104119	9205.906592	28.040487
276.236653	9219.026358	28.045504
276.754566	9228.783719	28.050522
277.050864	9236.195068	28.055540
277.208491	9247.091445	28.060557
277.869818	9255.232112	28.065575
277.899759	9259.849782	28.070592
278.318116	9270.667695	28.075610
278.520797	9285.029993	28.080628
278.610431	9287.384139	28.085645
279.136375	9299.934406	28.090663
279.086677	9309.451830	28.095680
279.430067	9317.540993	28.100698
279.378153	9342.194407	28.105716
279.744335	9342.387020	28.110733
279.821991	9360.563803	28.115751
280.007667	9367.398872	28.120768
280.138965	9394.344381	28.125786
280.244518	9400.835171	28.130804
280.931636	9405.164288	28.135821
281.116229	9426.800582	28.140839
281.359776	9439.732732	28.145856
281.654966	9457.724196	28.150874
282.068234	9473.812429	28.155892
281.935326	9488.725973	28.160909
282.642028	9504.430726	28.165927
282.758792	9525.117896	28.170944
283.176198	9546.424460	28.175962
283.224499	9558.862989	28.180980
283.681384	9581.937818	28.185997
284.049800	9587.314286	28.191015
284.147939	9610.779671	28.196032
284.577140	9622.205451	28.201050
284.812666	9639.625445	28.206068
285.425046	9654.707245	28.211085
286.195183	9647.420574	28.216103
286.664089	9646.040672	28.221120
287.030793	9649.497812	28.226138
287.477305	9660.362086	28.231156
287.771529	9660.177564	28.236173
287.939641	9666.826043	28.241191
287.887313	9673.032097	28.246208
288.399537	9683.523069	28.251226
288.228639	9687.900589	28.256244
288.682560	9685.452704	28.261261
288.779668	9710.342302	28.266279
289.068590	9716.267919	28.271296
289.201273	9724.825768	28.276314
289.719841	9730.346236	28.281332
289.860731	9748.399892	28.286349
290.136628	9757.039650	28.291367
290.489033	9773.904838	28.296384
290.736493	9790.170710	28.301402
290.920637	9786.599775	28.306420
291.002915	9805.391944	28.311437
291.731917	9822.817373	28.316455
291.787977	9843.511191	28.321472
292.030239	9850.688089	28.326490
292.705952	9868.488103	28.331508
292.706092	9886.889008	28.336525
293.123307	9891.705441	28.341543
293.261588	9909.200817	28.346560
293.293778	9917.035591	28.351578
294.049843	9932.815114	28.356596
293.664989	9953.097787	28.361613
294.326419	9967.354463	28.366631
294.806343	9993.656148	28.371648
294.526408	10004.744228	28.376666
295.008016	10016.973524	28.381684
295.258548	10041.239788	28.386701
295.629161	10057.041538	28.391719
295.805490	10078.105244	28.396736
296.222834	10088.671207	28.401754
297.086019	10108.229316	28.406772
297.014491	10130.774571	28.411789
297.794381	10132.983474	28.416807
297.924933	10147.957564	28.421824
298.267561	10163.419611	28.426842
298.467626	10183.914577	28.431860
298.562506	10184.360983	28.436877
299.023710	10195.232756	28.441895
299.247937	10209.589258	28.446912
299.783001	10219.647579	28.451930
300.209587	10222.669263	28.456948
300.174453	10235.168593	28.461965
300.662604	10240.122469	28.466983
300.506362	10240.434318	28.472000
300.723224	10257.532590	28.477018
301.157920	10263.397800	28.482036
301.016721	10289.945000	28.487053
301.425482	10300.354553	28.492071
301.921773	10320.727774	28.497088
302.001782	10333.790201	28.502106
302.553869	10345.149936	28.507124
302.497423	10369.221301	28.512141
303.053488	10388.903298	28.517159
303.080811	10413.542638	28.522176
303.527472	10432.963863	28.527194
303.790254	10443.459370	28.532212
303.937421	10472.967774	28.537229
304.649449	10482.894493	28.542247
305.353660	10499.468765	28.547264
305.584352	10519.113148	28.552282
305.879193	10518.177061	28.557300
305.699826	10542.889796	28.562317
306.047831	10544.629229	28.567335
306.702615	10565.840017	28.572352
306.804481	10587.443180	28.577370
307.423100	10595.973138	28.582388
307.558689	10623.371270	28.587405
308.151758	10631.179014	28.592423
308.514674	10643.581916	28.597440
308.767664	10654.186419	28.602458
309.216236	10666.386555	28.607476
309.003194	10690.984747	28.612493
309.709151	10693.817772	28.617511
309.816330	10697.091337	28.622528
310.481727	10718.303805	28.627546
310.726166	10726.099560	28.632564
310.976112	10741.942780	28.637581
311.641682	10746.970210	28.642599
311.491672	10764.782813	28.647616
311.889665	10771.717958	28.652634
312.383593	10784.665740	28.657652
312.342986	10810.891748	28.662669
312.690634	10820.007077	28.667687
313.093073	10835.403538	28.672704
313.363779	10854.492647	28.677722
313.636129	10862.584073	28.682740
313.587446	10877.334056	28.687757
314.118316	10887.721770	28.692775
314.315516	10904.984729	28.697792
315.055971	10929.665284	28.702810
315.168006	10934.368470	28.707828
315.332211	10958.516755	28.712845
315.959733	10972.207980	28.717863
316.263201	10995.384229	28.722880
316.145375	11007.287555	28.727898
316.852225	11014.812519	28.732916
316.819716	11038.975745	28.737933
317.397295	11049.766752	28.742951
318.113361	11069.708734	28.747968
317.783988	11073.593419	28.752986
318.863616	11081.079320	28.758004
319.063219	11096.974885	28.763021
319.441933	11107.162227	28.768039
320.095936	11109.896052	28.773056
320.222251	11121.808804	28.778074
320.567204	11124.994907	28.783092
320.691623	11141.129555	28.788109
321.061157	11152.335069	28.793127
321.039033	11153.585935	28.798144
320.949301	11176.116341	28.803162
321.647499	11184.488936	28.808180
321.831381	11190.712397	28.813197
321.938128	11202.786124	28.818215
322.404017	11216.180626	28.823232
322.689839	11230.121004	28.828250
322.696002	11240.975823	28.833268
323.092874	11258.337481	28.838285
323.409355	11276.712609	28.843303
323.884053	11297.554419	28.848320
323.977706	11326.182077	28.853338
324.727591	11337.003261	28.858356
324.483916	11352.585992	28.863373
325.200530	11368.271838	28.868391
325.444057	11395.493262	28.873408
325.625878	11404.773627	28.878426
326.115561	11434.849106	28.883444
326.339968	11453.409251	28.888461
326.952849	11463.260363	28.893479
327.681795	11475.932064	28.898496
327.840090	11480.653447	28.903514
328.490395	11486.558102	28.908532
328.637956	11496.042773	28.913549
328.604752	11509.811998	28.918567
329.148546	11520.564333	28.923584
329.228749	11544.827494	28.928602
329.786090	11552.691712	28.933620
330.028984	11578.192620	28.938637
330.212883	11586.323392	28.943655
330.838724	11603.690773	28.948672
331.289118	11625.843974	28.953690
331.730385	11638.623725	28.958708
331.623818	11657.762917	28.963725
331.876388	11676.552561	28.968743
332.730932	11676.877578	28.973760
332.572014	11700.480338	28.978778
332.704039	11710.201199	28.983796
333.184356	11733.773951	28.988813
333.413365	11758.996239	28.993831
334.078355	11769.193054	28.998848
334.434423	11792.605239	29.003866
334.591414	11813.010812	29.008884
334.928075	11824.907053	29.013901
335.421664	11841.221652	29.018919
335.386949	11870.650060	29.023936
335.466272	11882.542194	29.028954
336.252046	11904.779291	29.033972
336.463109	11927.349026	29.038989
336.493514	11941.124452	29.044007
337.387706	11960.291294	29.049024
337.242527	11967.759835	29.054042
337.925861	11992.059140	29.059060
338.011526	12024.683539	29.064077
338.758346	12034.248859	29.069095
339.216796	12051.895330	29.074112
339.253767	12073.314535	29.079130
339.843442	12088.108183	29.084148
340.208085	12111.314182	29.089165
340.613545	12130.206784	29.094183
340.891464	12148.872962	29.099200
340.824819	12163.765691	29.104218
341.497591	12174.517269	29.109236
341.680017	12193.327823	29.114253
341.802914	12211.250880	29.119271
342.236412	12226.337356	29.124288
342.872642	12244.212103	29.129306
343.585112	12250.331521	29.134324
344.431604	12273.933202	29.139341
344.072385	12284.943397	29.144359
344.936710	12274.811757	29.149376
344.652328	12289.078523	29.154394
344.498737	12300.296699	29.159412
345.208502	12310.126862	29.164429
345.389833	12331.776504	29.169447
346.089596	12340.840917	29.174464
346.011968	12356.919650	29.179482
346.729187	12366.631847	29.184500
346.926772	12385.980203	29.189517
347.073120	12405.630225	29.194535
347.674594	12415.294154	29.199552
347.619302	12434.037754	29.204570
348.106185	12441.127043	29.209588
348.466644	12472.730542	29.214605
348.777549	12484.994351	29.219623
349.357349	12508.672583	29.224640
349.664186	12529.074551	29.229658
349.899613	12547.286711	29.234676
350.280564	12561.904817	29.239693
350.117728	12581.107390	29.244711
350.993561	12598.777813	29.249728
351.362092	12626.673110	29.254746
351.328222	12631.917311	29.259764
352.134165	12663.000216	29.264781
352.230849	12684.524499	29.269799
353.003057	12693.764114	29.274816
352.942148	12720.952754	29.279834
353.471864	12725.300849	29.284852
353.718936	12760.929703	29.289869
353.824227	12775.524578	29.294887
354.693229	12784.613384	29.299904
355.383053	12805.483378	29.304922
355.842167	12819.953732	29.309940
356.348543	12836.295627	29.314957
356.008087	12847.435855	29.319975
356.760923	12857.534329	29.324992
357.028974	12875.419631	29.330010
357.156619	12885.580717	29.335028
357.838256	12914.273986	29.340045
358.052512	12927.292058	29.345063
358.685448	12931.080989	29.350080
359.520283	12944.286662	29.355098
359.451717	12956.155131	29.360116
359.841750	12959.716627	29.365133
359.801510	12984.123551	29.370151
360.311340	12992.507341	29.375168
360.736433	13010.778839	29.380186
361.150208	13023.200666	29.385204
361.249884	13053.746816	29.390221
361.349218	13059.270392	29.395239
362.038267	13078.097693	29.400256
362.584200	13094.616809	29.405274
362.955110	13102.163343	29.410292
363.237202	13122.617176	29.415309
363.346771	13137.663237	29.420327
363.882279	13156.189261	29.425344
364.085143	13177.438634	29.430362
364.590592	13184.967414	29.435380
365.004973	13207.974394	29.440397
365.336637	13223.330154	29.445415
365.621125	13240.284833	29.450432
365.963606	13250.718981	29.455450
366.236839	13271.546982	29.460468
367.138862	13282.828767	29.465485
367.088540	13302.118765	29.470503
367.475049	13322.828135	29.475520
367.460727	13337.811539	29.480538
367.574487	13355.835001	29.485556
368.027918	13372.946654	29.490573
368.657931	13402.141334	29.495591
369.038189	13409.866537	29.500608
368.836503	13440.545493	29.505626
369.377335	13456.165720	29.510644
369.796333	13471.245979	29.515661
370.120354	13502.976878	29.520679
370.558422	13515.909986	29.525696
371.008596	13532.693869	29.530714
371.099304	13554.624288	29.535732
371.787185	13580.784953	29.540749
372.377618	13610.545069	29.545767
372.646554	13614.495020	29.550784
373.033642	13651.205872	29.555802
373.134758	13670.103190	29.560820
373.679867	13675.267017	29.565837
373.958526	13706.045307	29.570855
374.490655	13732.460960	29.575872
374.659910	13747.472950	29.580890
375.128124	13776.184968	29.585908
375.588100	13790.096976	29.590925
375.893874	13821.281766	29.595943
376.355760	13832.878725	29.600960
376.927172	13853.364097	29.605978
377.118314	13879.021443	29.610996
377.666331	13901.954778	29.616013
377.824989	13920.814966	29.621031
378.299117	13942.427188	29.626048
378.895416	13960.925591	29.631066
379.462575	13978.579052	29.636084
379.737067	13993.287477	29.641101
380.057750	14016.303712	29.646119
380.678404	14025.949697	29.651136
381.088089	14050.922707	29.656154
381.245325	14059.349234	29.661172
381.461443	14080.265967	29.666189
381.950700	14105.059286	29.671207
382.342542	14120.520094	29.676224
382.707971	14141.675764	29.681242
383.144804	14161.206596	29.686260
383.779095	14170.165243	29.691277
383.936784	14191.830172	29.696295
384.803319	14198.842074	29.701312
385.236322	14207.832076	29.706330
385.664482	14235.294132	29.711348
385.708831	14245.408914	29.716365
386.222211	14263.541560	29.721383
386.228590	14275.042329	29.726400
386.956175	14294.531191	29.731418
386.821365	14315.682826	29.736436
387.158843	14328.272134	29.741453
387.607080	14365.079063	29.746471
388.067772	14369.264597	29.751488
388.350587	14395.846312	29.756506
388.889464	14415.273093	29.761524
389.243186	14432.874939	29.766541
389.589671	14473.948670	29.771559
390.483483	14486.233566	29.776576
390.854740	14498.764041	29.781594
390.913857	14517.052918	29.786612
391.689348	14540.820084	29.791629
391.713653	14547.318989	29.796647
391.980712	14558.719343	29.801664
392.340313	14578.714235	29.806682
392.607120	14613.544508	29.811700
393.159953	14633.578852	29.816717
393.307236	14654.434298	29.821735
393.645208	14670.557668	29.826752
394.116131	14692.445999	29.831770
394.368359	14720.659353	29.836788
394.540009	14736.274952	29.841805
395.141508	14757.542988	29.846823
395.471955	14780.795489	29.851840
396.049555	14797.377486	29.856858
396.035751	14832.318166	29.861876
396.386129	14854.279138	29.866893
397.058652	14879.843945	29.871911
397.533470	14906.601761	29.876928
397.667385	14941.557541	29.881946
398.397778	14959.805500	29.886964
398.744251	14973.300225	29.891981
399.129654	15000.637402	29.896999
399.421188	15020.741258	29.902016
399.714623	15044.972556	29.907034
399.942159	15074.166150	29.912052
400.756777	15094.741329	29.917069
400.990516	15123.956140	29.922087
401.228361	15152.030254	29.927104
401.836179	15174.415770	29.932122
402.557792	15201.685103	29.937140
403.367717	15223.957099	29.942157
403.918027	15249.099282	29.947175
404.186079	15271.190406	29.952192
404.562089	15278.768600	29.957210
404.802098	15311.093550	29.962228
405.053680	15317.061496	29.967245
405.761011	15340.565511	29.972263
405.736572	15359.923047	29.977280
406.963055	15380.443891	29.982298
407.030560	15410.891460	29.987316
407.339992	15417.510501	29.992333
407.860694	15433.113387	29.997351
408.531552	15458.233921	30.002368
409.201126	15469.215277	30.007386
408.745704	15493.266854	30.012404
409.203504	15507.411014	30.017421
409.550545	15524.307464	30.022439
410.033765	15551.895497	30.027456
410.464238	15568.845321	30.032474
410.591879	15606.727834	30.037492
410.783276	15624.232881	30.042509
411.698960	15653.181265	30.047527
412.000163	15686.984866	30.052544
412.453174	15709.862536	30.057562
412.572860	15736.019883	30.062580
413.115077	15756.619237	30.067597
413.413498	15785.919739	30.072615
413.898780	15815.402802	30.077632
414.297918	15830.544878	30.082650
415.271935	15859.639252	30.087668
415.759398	15874.698130	30.092685
415.996407	15897.840208	30.097703
416.664204	15916.070406	30.102720
416.927282	15938.074643	30.107738
417.373078	15955.050849	30.112756
418.021556	15971.859710	30.117773
418.434920	15980.424080	30.122791
419.008453	16005.279396	30.127808
419.335231	16011.955952	30.132826
419.657168	16026.601713	30.137844
419.585055	16045.951573	30.142861
420.086362	16076.414783	30.147879
420.310705	16103.687022	30.152896
421.001677	16121.237925	30.157914
420.867945	16144.687527	30.162932
421.484411	16167.047596	30.167949
421.580898	16187.543097	30.172967
421.746131	16214.328835	30.177984
422.425383	16235.188465	30.183002
422.829646	16266.687236	30.188020
422.885308	16300.479612	30.193037
423.816341	16332.701867	30.198055
424.064432	16359.844439	30.203072
424.428482	16375.564077	30.208090
424.571280	16410.154785	30.213108
425.166857	16432.957432	30.218125
425.962499	16457.845085	30.223143
426.233974	16491.152549	30.228160
426.514511	16512.766243	30.233178
427.014217	16546.897358	30.238196
427.589473	16577.785714	30.243213
428.167739	16608.446244	30.248231
428.406403	16638.382720	30.253248
429.354043	16656.731139	30.258266
429.564660	16690.477969	30.263284
430.279372	16703.474409	30.268301
430.668160	16730.387144	30.273319
430.876261	16758.455611	30.278336
430.965537	16782.240810	30.283354
431.920810	16806.563970	30.288372
432.186417	16830.624989	30.293389
432.767961	16849.400127	30.298407
432.929860	16875.801974	30.303424
433.555350	16897.119198	30.308442
433.656504	16937.010928	30.313460
434.124127	16954.985860	30.318477
434.540753	16991.597470	30.323495
435.121476	17018.029064	30.328512
435.728024	17046.601290	30.333530
436.548459	17068.065230	30.338548
436.772531	17098.920658	30.343565
437.671367	17118.098328	30.348583
438.217637	17133.951304	30.353600
438.928236	17154.810215	30.358618
439.137857	17165.497769	30.363636
439.500008	17173.502115	30.368653
440.406162	17187.072357	30.373671
440.845587	17210.686709	30.378688
441.308316	17214.269282	30.383706
441.435735	17237.426877	30.388724
441.825860	17247.138819	30.393741
442.404767	17259.888306	30.398759
442.424494	17288.201651	30.403776
442.682659	17302.747767	30.408794
442.688906	17325.447394	30.413812
443.443734	17348.317935	30.418829
443.941915	17365.871567	30.423847
444.146287	17395.214436	30.428864
445.078218	17421.348701	30.433882
445.290772	17447.617105	30.438900
445.306125	17464.320536	30.443917
445.635628	17490.924550	30.448935
446.140458	17524.554392	30.453952
446.676116	17549.461826	30.458970
447.290680	17577.079703	30.463988
447.761782	17611.308760	30.469005
448.102291	17627.055198	30.474023
448.702201	17653.557326	30.479040
449.191185	17680.746382	30.484058
449.722703	17701.308431	30.489076
449.767913	17732.451724	30.494093
450.271061	17754.250101	30.499111
450.568317	17784.501415	30.504128
450.622603	17819.566432	30.509146
451.415899	17840.144730	30.514164
451.627150	17860.459897	30.519181
452.283189	17894.528002	30.524199
452.678365	17922.471123	30.529216
452.879426	17946.666770	30.534234
453.576261	17975.232636	30.539252
453.693788	18018.620672	30.544269
454.515843	18038.714590	30.549287
455.089032	18079.909211	30.554304
455.638741	18099.698139	30.559322
456.173516	18118.927170	30.564340
455.931088	18150.122231	30.569357
456.726631	18176.752555	30.574375
457.396652	18215.468623	30.579392
458.035908	18236.848362	30.584410
458.167641	18266.620808	30.589428
458.951347	18302.369134	30.594445
459.508146	18314.645799	30.599463
459.891211	18346.053351	30.604480
460.652300	18372.613501	30.609498
461.195274	18389.403002	30.614516
461.591525	18411.376699	30.619533
462.479054	18425.111812	30.624551
462.685686	18443.975302	30.629568
463.202355	18463.447557	30.634586
464.060564	18486.543419	30.639604
463.902957	18510.536593	30.644621
464.679150	18538.427605	30.649639
464.846833	18551.390428	30.654656
465.398442	18583.940860	30.659674
465.921355	18602.515201	30.664692
466.503101	18625.805889	30.669709
466.927200	18644.616766	30.674727
467.368971	18672.023045	30.679744
467.741837	18693.855400	30.684762
468.699421	18709.639323	30.689780
468.842703	18731.974959	30.694797
468.957468	18756.905253	30.699815
469.614262	18785.939731	30.704832
469.758225	18802.627453	30.709850
470.251408	18833.532201	30.714868
470.630624	18867.752515	30.719885
471.180312	18890.460978	30.724903
471.653006	18927.629792	30.729920
471.997479	18948.822460	30.734938
472.544318	18982.808400	30.739956
472.804129	19025.652175	30.744973
473.170840	19032.165625	30.749991
473.708022	19080.115209	30.755008
474.439583	19114.401140	30.760026
475.071703	19147.382220	30.765044
475.165183	19176.523932	30.770061
476.062406	19195.432265	30.775079
476.353601	19228.460240	30.780096
476.425698	19252.570193	30.785114
477.152414	19281.992544	30.790132
477.571871	19318.709202	30.795149
478.555147	19353.941934	30.800167
478.813079	19383.197344	30.805184
479.203216	19405.899660	30.810202
479.739384	19436.621778	30.815220
480.106548	19465.190623	30.820237
480.527222	19495.627561	30.825255
480.697899	19534.784112	30.830272
481.573858	19570.981614	30.835290
482.468849	19589.056730	30.840308
482.678937	19620.556450	30.845325
483.327750	19640.141989	30.850343
483.323515	19675.023612	30.855360
483.965937	19695.178808	30.860378
484.188645	19718.160266	30.865396
484.963017	19745.358334	30.870413
485.270224	19777.898271	30.875431
485.846881	19805.057705	30.880448
486.204391	19831.739545	30.885466
487.407655	19850.645099	30.890484
487.428413	19877.556327	30.895501
487.955548	19913.101165	30.900519
488.292079	19930.088406	30.905536
488.770748	19967.826889	30.910554
489.156721	19987.965451	30.915572
489.524347	20023.364737	30.920589
490.277488	20051.697451	30.925607
490.875885	20075.277912	30.930624
491.284417	20106.039909	30.935642
491.591247	20135.712140	30.940660
491.707702	20167.366314	30.945677
492.476253	20200.479571	30.950695
492.808690	20229.528792	30.955712
493.443268	20265.007000	30.960730
493.761562	20297.053270	30.965748
494.440103	20331.425415	30.970765
494.946948	20374.151558	30.975783
495.457829	20402.377180	30.980800
495.920628	20453.456531	30.985818
496.624366	20485.898008	30.990836
497.035497	20518.347182	30.995853
497.486494	20545.236576	31.000871
498.266571	20589.001050	31.005888
498.689018	20614.688220	31.010906
499.434950	20642.719643	31.015924
499.916878	20678.715182	31.020941
500.694854	20702.691761	31.025959
501.226965	20736.720960	31.030976
501.355815	20760.318483	31.035994
501.856989	20798.345701	31.041012
502.162955	20835.139741	31.046029
502.608353	20858.031007	31.051047
503.298410	20887.872173	31.056064
503.675058	20926.721442	31.061082
504.452190	20955.418191	31.066100
504.724715	20996.293011	31.071117
505.052237	21022.570456	31.076135
506.003984	21055.549231	31.081152
506.408484	21095.942478	31.086170
507.126873	21114.596197	31.091188
507.732965	21147.761622	31.096205
508.156674	21171.181050	31.101223
508.586865	21206.294728	31.106240
508.846180	21237.157551	31.111258
509.671134	21265.006969	31.116276
510.443713	21284.208428	31.121293
511.376722	21310.556275	31.126311
512.161631	21324.619023	31.131328
512.597915	21342.204843	31.136346
513.413310	21363.693286	31.141364
513.606113	21380.527247	31.146381
514.182727	21395.298541	31.151399
514.638676	21410.436142	31.156416
514.672564	21429.746424	31.161434
515.500647	21447.745225	31.166452
515.729293	21475.864689	31.171469
516.118802	21492.472253	31.176487
516.520811	21530.175133	31.181504
516.612264	21560.843452	31.186522
517.457550	21573.393190	31.191540
517.738794	21607.589323	31.196557
518.059363	21631.094860	31.201575
518.732360	21653.578833	31.206592
518.767332	21686.158001	31.211610
519.444415	21714.625016	31.216628
519.842412	21747.501606	31.221645
520.282182	21789.666289	31.226663
520.508759	21814.861085	31.231680
520.959418	21855.830012	31.236698
521.799495	21894.059334	31.241716
522.289955	21932.614856	31.246733
524.443546	21931.332011	31.251751
525.183916	21937.889362	31.256768
525.589915	21962.291869	31.261786
525.843989	21979.672839	31.266804
526.431093	22005.696355	31.271821
526.737448	22024.212889	31.276839
527.183764	22041.311242	31.281856
527.219996	22075.021886	31.286874
527.979421	22090.441335	31.291892
528.335240	22130.743188	31.296909
528.534036	22154.489459	31.301927
529.517695	22186.485779	31.306944
529.451876	22221.261454	31.311962
529.795295	22256.782271	31.316980
530.285092	22300.778991	31.321997
530.955872	22337.215748	31.327015
531.358968	22368.948897	31.332032
531.878063	22412.890756	31.337050
532.497757	22433.804240	31.342068
533.416352	22475.902166	31.347085
534.327307	22509.490013	31.352103
534.920020	22528.423710	31.357120
535.418620	22551.194928	31.362138
536.224840	22578.366698	31.367156
536.886698	22608.890977	31.372173
537.285485	22644.764042	31.377191
538.192892	22669.190466	31.382208
538.029222	22693.834213	31.387226
538.902933	22727.124926	31.392244
539.325983	22750.502104	31.397261
539.757986	22788.139530	31.402279
540.287459	22806.653658	31.407296
540.319539	22851.247323	31.412314
540.936811	22884.135902	31.417332
541.584762	22928.355833	31.422349
541.880729	22953.547597	31.427367
542.502591	22989.702504	31.432384
542.432826	23038.369180	31.437402
543.185783	23061.271998	31.442420
543.935861	23093.799029	31.447437
544.331051	23141.186657	31.452455
545.386437	23175.694676	31.457472
545.781750	23214.052665	31.462490
546.230354	23251.107039	31.467508
547.190343	23278.736077	31.472525
547.556684	23318.653251	31.477543
548.606240	23341.484945	31.482560
549.093522	23372.814818	31.487578
549.462134	23405.622911	31.492596
550.192629	23441.129827	31.497613
550.706271	23467.135109	31.502631
551.436156	23498.079864	31.507648
551.640854	23528.942131	31.512666
552.238335	23557.101922	31.517684
552.798377	23590.455556	31.522701
552.896276	23619.634754	31.527719
553.722827	23644.460436	31.532736
553.888864	23679.316314	31.537754
554.300302	23711.404185	31.542772
555.124596	23737.323545	31.547789
555.369471	23778.543336	31.552807
555.975919	23807.447746	31.557824
556.815853	23843.058407	31.562842
557.192237	23877.509055	31.567860
557.946112	23918.207554	31.572877
558.419826	23954.848583	31.577895
558.975828	23974.231724	31.582912
559.785541	24016.488896	31.587930
560.539335	24034.210943	31.592948
561.124823	24063.681401	31.597965
561.139445	24099.673772	31.602983
562.277352	24121.361466	31.608000
563.003865	24162.999976	31.613018
562.849103	24192.946062	31.618036
563.454681	24225.781811	31.623053
563.973980	24269.493933	31.628071
564.575141	24298.734804	31.633088
565.098603	24339.703848	31.638106
565.924416	24366.110381	31.643124
566.072219	24404.433363	31.648141
566.631879	24447.640364	31.653159
567.219809	24482.128636	31.658176
568.155116	24525.024551	31.663194
569.140777	24565.005794	31.668212
569.768698	24594.799040	31.673229
570.004467	24627.250660	31.678247
570.671270	24664.848764	31.683264
571.682435	24694.380276	31.688282
572.373001	24726.925563	31.693300
572.631188	24756.150983	31.698317
572.954503	24791.293971	31.703335
573.759771	24817.900205	31.708352
574.227175	24861.665939	31.713370
574.557658	24888.270345	31.718388
575.372885	24926.281881	31.723405
575.725774	24963.404895	31.728423
576.334873	24998.933487	31.733440
576.814309	25030.658999	31.738458
577.094383	25071.237703	31.743476
577.895664	25102.635165	31.748493
578.356788	25145.043788	31.753511
579.144861	25180.778665	31.758528
579.908004	25221.130800	31.763546
579.915917	25262.826594	31.768564
580.612390	25300.130571	31.773581
581.242552	25351.468238	31.778599
581.798339	25384.067174	31.783616
582.814333	25428.292234	31.788634
583.349584	25473.666579	31.793652
584.060379	25505.085079	31.798669
584.611669	25542.405788	31.803687
585.258845	25580.330972	31.808704
585.701596	25615.987669	31.813722
586.160892	25646.434385	31.818740
587.028728	25677.980382	31.823757
587.436055	25714.148348	31.828775
588.311524	25739.234456	31.833792
589.117584	25779.397761	31.838810
589.402824	25813.758494	31.843828
589.924826	25849.207354	31.848845
590.378741	25881.646003	31.853863
591.202791	25915.872474	31.858880
592.101348	25959.586122	31.863898
592.537487	25985.549870	31.868916
593.054069	25998.185195	31.873933
593.265638	26038.991393	31.878951
593.873862	26062.014994	31.883968
594.352601	26093.078707	31.888986
595.075368	26126.158445	31.894004
595.657264	26147.587309	31.899021
596.037474	26190.200331	31.904039
596.502744	26220.545868	31.909056
597.257310	26255.030210	31.914074
597.553317	26300.051827	31.919092
598.403831	26331.171791	31.924109
598.777686	26375.568422	31.929127
599.027654	26415.301328	31.934144
600.141495	26456.189108	31.939162
600.679279	26505.818743	31.944180
600.921215	26539.100413	31.949197
601.543179	26577.802445	31.954215
602.277762	26623.337951	31.959232
603.197019	26657.285419	31.964250
603.817289	26693.813838	31.969268
604.600132	26730.140051	31.974285
604.867786	26775.483146	31.979303
605.749559	26823.296704	31.984320
606.404237	26856.015353	31.989338
606.667268	26905.031448	31.994356
607.795039	26950.108313	31.999373
608.126833	26993.514265	32.004391
608.907707	27029.310430	32.009408
609.496660	27064.593000	32.014426
609.948717	27113.498010	32.019444
610.723546	27144.668934	32.024461
610.882477	27182.692102	32.029479
611.704251	27229.157112	32.034496
612.460533	27263.548107	32.039514
612.831036	27312.131320	32.044532
613.935726	27347.460501	32.049549
614.464179	27394.812151	32.054567
615.254393	27429.785933	32.059584
615.595709	27471.333258	32.064602
616.686840	27511.076415	32.069620
617.490590	27549.240060	32.074637
617.670408	27586.255799	32.079655
618.033195	27631.415349	32.084672
618.859472	27669.796927	32.089690
619.431474	27715.233792	32.094708
620.192196	27757.967850	32.099725
620.412287	27793.378635	32.104743
621.314247	27818.981485	32.109760
622.544948	27862.363128	32.114778
622.999988	27891.638291	32.119796
624.092625	27927.596085	32.124813
624.547792	27958.552566	32.129831
624.895436	27991.769600	32.134848
625.638163	28016.266123	32.139866
626.021491	28051.051499	32.144884
626.796938	28085.194406	32.149901
627.299621	28118.520243	32.154919
627.729798	28156.787431	32.159936
628.620575	28194.313010	32.164954
628.918223	28234.440251	32.169972
629.727991	28264.747865	32.174989
629.915142	28306.643244	32.180007
630.082953	28355.469083	32.185024
631.015426	28393.715407	32.190042
631.815078	28439.554572	32.195060
632.619702	28491.757940	32.200077
633.598922	28527.487949	32.205095
633.710694	28558.618891	32.210112
634.541222	28589.922420	32.215130
634.874244	28634.614779	32.220148
635.635701	28667.850665	32.225165
636.064660	28698.723861	32.230183
636.862990	28739.311411	32.235200
636.976687	28772.818966	32.240218
637.735235	28829.695060	32.245236
638.176569	28868.220996	32.250253
638.822646	28911.714851	32.255271
639.694287	28966.810229	32.260288
640.511804	29008.741654	32.265306
640.913583	29055.813489	32.270324
641.613399	29088.598237	32.275341
642.067068	29131.863360	32.280359
642.583535	29178.247614	32.285376
643.369474	29230.373608	32.290394
643.910745	29281.646579	32.295412
644.974031	29333.856079	32.300429
645.475055	29371.242230	32.305447
645.976691	29423.924968	32.310464
646.715714	29465.863228	32.315482
647.604377	29514.876700	32.320500
648.061893	29561.201468	32.325517
649.054990	29614.389716	32.330535
649.673904	29662.086522	32.335552
651.167615	29684.831008	32.340570
651.579949	29709.766582	32.345588
652.552934	29752.585554	32.350605
653.134674	29794.201315	32.355623
653.552153	29828.592496	32.360640
654.341959	29860.631233	32.365658
654.796882	29908.101298	32.370676
655.740741	29944.414508	32.375693
656.071075	29984.906715	32.380711
656.419796	30021.666690	32.385728
657.479146	30061.293349	32.390746
657.477217	30098.664305	32.395764
658.618691	30143.973673	32.400781
659.327651	30187.138069	32.405799
659.757475	30238.057830	32.410816
660.503820	30274.686825	32.415834
661.035839	30321.178702	32.420852
661.846981	30364.675228	32.425869
662.596831	30403.320372	32.430887
662.815479	30457.383589	32.435904
663.838207	30494.374509	32.440922
664.611604	30551.594414	32.445940
665.298865	30579.414989	32.450957
665.843120	30631.929835	32.455975
666.573715	30663.631370	32.460992
667.523567	30704.382543	32.466010
667.867456	30748.704855	32.471028
668.731939	30801.005926	32.476045
669.270583	30836.871766	32.481063
669.764707	30894.837768	32.486080
670.515928	30930.803428	32.491098
671.213226	30977.214162	32.496116
671.954184	31021.272961	32.501133
672.803781	31061.762306	32.506151
673.106663	31109.587520	32.511168
673.627818	31142.264289	32.516186
674.728969	31191.172820	32.521204
675.138551	31238.020860	32.526221
675.966141	31282.641985	32.531239
676.023399	31334.241954	32.536256
677.208594	31375.583645	32.541274
677.512506	31427.373023	32.546292
678.019881	31476.475807	32.551309
678.976071	31511.961742	32.556327
679.534670	31560.759639	32.561344
680.190350	31605.932913	32.566362
680.322780	31653.526732	32.571380
681.372584	31704.359915	32.576397
681.823487	31741.979427	32.581415
682.591020	31799.918044	32.586432
683.230286	31859.058940	32.591450
683.900432	31900.646222	32.596468
684.298943	31949.937759	32.601485
685.166848	32000.698838	32.606503
686.223540	32061.412652	32.611520
686.782322	32104.737188	32.616538
687.793136	32156.803966	32.621556
687.993957	32204.957359	32.626573
689.113207	32248.302415	32.631591
689.519351	32301.234943	32.636608
690.352715	32350.314334	32.641626
691.386744	32408.345919	32.646644
691.745736	32456.456305	32.651661
692.979211	32494.562253	32.656679
692.961668	32550.722297	32.661696
693.695670	32601.998795	32.666714
694.631835	32652.371526	32.671732
695.809407	32707.903416	32.676749
696.493723	32745.703354	32.681767
697.322484	32802.762806	32.686784
698.181675	32841.028806	32.691802
698.945680	32879.979823	32.696820
699.616242	32928.143946	32.701837
700.652769	32960.680129	32.706855
700.800688	32997.072033	32.711872
701.678130	33046.506558	32.716890
702.402846	33079.085144	32.721908
702.932306	33129.648781	32.726925
704.287364	33170.227928	32.731943
704.569814	33215.247847	32.736960
705.485758	33246.083644	32.741978
706.531841	33296.055173	32.746996
706.831389	33327.916394	32.752013
707.677727	33349.912233	32.757031
707.947628	33406.308002	32.762048
708.850279	33447.881146	32.767066
709.516274	33491.514304	32.772084
710.086407	33540.175956	32.777101
710.931117	33587.777105	32.782119
711.798329	33628.578497	32.787136
712.463265	33672.635784	32.792154
712.852466	33709.768998	32.797172
713.924565	33755.002231	32.802189
714.553639	33781.521135	32.807207
715.253691	33832.622594	32.812224
715.855253	33879.408753	32.817242
716.808673	33922.960132	32.822260
717.377434	33965.825451	32.827277
718.383431	34007.250851	32.832295
718.871439	34055.395409	32.837312
719.567066	34090.913660	32.842330
720.283929	34144.485296	32.847348
720.943647	34186.160948	32.852365
721.582675	34230.590138	32.857383
722.283071	34281.913921	32.862400
722.877928	34321.981406	32.867418
723.579162	34366.489714	32.872436
723.885097	34425.980597	32.877453
724.708521	34466.057033	32.882471
725.357760	34522.282942	32.887488
726.175149	34573.582902	32.892506
726.811172	34612.468551	32.897524
727.431009	34661.839506	32.902541
728.318036	34699.649352	32.907559
728.713067	34757.812218	32.912576
729.679324	34798.998788	32.917594
730.692450	34835.739705	32.922612
731.338911	34890.266260	32.927629
732.383998	34927.919136	32.932647
732.975560	34967.773396	32.937664
733.855881	35012.179319	32.942682
734.671400	35054.844056	32.947700
735.089690	35100.428548	32.952717
735.904757	35143.150438	32.957735
736.400746	35190.879054	32.962752
737.117082	35236.189826	32.967770
737.989930	35289.139437	32.972788
738.380699	35338.269436	32.977805
739.236184	35384.747535	32.982823
739.869329	35450.083146	32.987840
740.448520	35503.135911	32.992858
741.148094	35552.382727	32.997876
741.591662	35611.830233	33.002893
742.690112	35660.490416	33.007911
743.510758	35726.891538	33.012928
744.309796	35778.993961	33.017946
745.033356	35836.103319	33.022964
745.557084	35900.091612	33.027981
746.858497	35948.973779	33.032999
747.956188	36006.082260	33.038016
748.532354	36062.658757	33.043034
749.184446	36114.633129	33.048052
749.781516	36169.765026	33.053069
750.745368	36204.385160	33.058087
751.435075	36267.861856	33.063104
752.542439	36305.678215	33.068122
753.528549	36367.073061	33.073140
753.876606	36420.126161	33.078157
754.854563	36460.922121	33.083175
755.855378	36512.678783	33.088192
756.471213	36564.666223	33.093210
757.368012	36606.815589	33.098228
758.164682	36667.633777	33.103245
758.455687	36703.440717	33.108263
759.201134	36749.085316	33.113280
760.517485	36787.167188	33.118298
761.487107	36830.532350	33.123316
761.815526	36888.547027	33.128333
762.804419	36932.453189	33.133351
763.673430	36975.714169	33.138368
764.484541	37033.464404	33.143386
765.104887	37076.486076	33.148404
765.319202	37121.442720	33.153421
766.279290	37168.041229	33.158439
767.026688	37219.288935	33.163456
767.386178	37274.859042	33.168474
768.499579	37323.539679	33.173492
768.871860	37387.878507	33.178509
769.751745	37442.508070	33.183527
770.665739	37501.482928	33.188544
771.330734	37553.566298	33.193562
772.160134	37604.429084	33.198580
772.834824	37659.457899	33.203597
773.323603	37720.946710	33.208615
774.365240	37780.130109	33.213632
774.852194	37833.253625	33.218650
775.845362	37890.212696	33.223668
776.397365	37951.926295	33.228685
776.992921	38008.542873	33.233703
778.450221	38060.365022	33.238720
778.763218	38109.785428	33.243738
779.830031	38149.590639	33.248756
780.616104	38206.462641	33.253773
781.021287	38257.860958	33.258791
781.501065	38304.334357	33.263808
782.132591	38366.327653	33.268826
783.022004	38417.910241	33.273844
783.771529	38474.485108	33.278861
784.612736	38535.333290	33.283879
785.810233	38588.202620	33.288896
786.355412	38651.171377	33.293914
786.991535	38706.581977	33.298932
787.721714	38767.530307	33.303949
788.711399	38829.873903	33.308967
789.018611	38898.628708	33.313984
790.271810	38959.945152	33.319002
790.863983	39017.405974	33.324020
791.702007	39083.397448	33.329037
792.749244	39146.612011	33.334055
793.288326	39211.942143	33.339072
794.106289	39280.719839	33.344090
795.441944	39339.931326	33.349108
796.010151	39401.558022	33.354125
796.882800	39456.313985	33.359143
797.338053	39530.878415	33.364160
798.536196	39590.345981	33.369178
799.913519	39639.711719	33.374196
800.633267	39697.148165	33.379213
801.433164	39737.712477	33.384231
802.190922	39799.437278	33.389248
803.023887	39864.913355	33.394266
804.023249	39915.793090	33.399284
804.720759	39970.931766	33.404301
805.304474	40031.659822	33.409319
806.156797	40088.077460	33.414336
807.125321	40148.277956	33.419354
807.820650	40195.347958	33.424372
808.651980	40249.113144	33.429389
809.658366	40300.176088	33.434407
810.485220	40359.475895	33.439424
811.511522	40414.956617	33.444442
812.674823	40459.260233	33.449460
813.413180	40517.366321	33.454477
814.372020	40566.091002	33.459495
815.019413	40618.045378	33.464512
815.631015	40661.284272	33.469530
816.890061	40711.259023	33.474548
817.319451	40762.501414	33.479565
817.999739	40816.968218	33.484583
819.055903	40865.197770	33.489600
819.835088	40918.567972	33.494618
820.384230	40973.384449	33.499636
821.040960	41030.758339	33.504653
822.084600	41084.315458	33.509671
823.079925	41138.316614	33.514688
823.593822	41195.359004	33.519706
824.730708	41241.964096	33.524724
825.316893	41294.871956	33.529741
825.673273	41354.317277	33.534759
826.862970	41419.868993	33.539776
827.526139	41476.003449	33.544794
828.581187	41529.578859	33.549812
829.130128	41599.449317	33.554829
830.303450	41642.824075	33.559847
830.976411	41696.149468	33.564864
831.615872	41768.808163	33.569882
832.829680	41816.275301	33.574900
833.150833	41865.892729	33.579917
833.778330	41909.239139	33.584935
834.810869	41963.666618	33.589952
835.480550	42009.840104	33.594970
836.440465	42065.227840	33.599988
836.768007	42123.553945	33.605005
837.749318	42183.833967	33.610023
838.529498	42242.241719	33.615040
839.590464	42305.147088	33.620058
840.662541	42354.863770	33.625076
841.557124	42410.831778	33.630093
842.375782	42467.905937	33.635111
843.354567	42509.674574	33.640128
843.698511	42574.305156	33.645146
844.523763	42622.504958	33.650164
845.612358	42706.241214	33.655181
846.289442	42763.458350	33.660199
847.215904	42817.999334	33.665216
848.063765	42885.866634	33.670234
848.845167	42951.366313	33.675252
849.990875	43015.417986	33.680269
850.458731	43074.066314	33.685287
851.240705	43139.300813	33.690304
852.163288	43206.803270	33.695322
852.986136	43267.186828	33.700340
853.912986	43342.064015	33.705357
854.556447	43415.043775	33.710375
855.441164	43476.702264	33.715392
856.284897	43556.336931	33.720410
857.448479	43622.531796	33.725428
858.061721	43696.269876	33.730445
858.677395	43773.309563	33.735463
859.845880	43835.310713	33.740480
860.521099	43912.683175	33.745498
861.777101	43984.804111	33.750516
863.608325	44028.884470	33.755533
864.222393	44082.541069	33.760551
865.710542	44132.848495	33.765568
866.705203	44194.650001	33.770586
867.658427	44244.408420	33.775604
868.483226	44296.729721	33.780621
868.820092	44354.136765	33.785639
870.121344	44406.314578	33.790656
870.445071	44465.520354	33.795674
871.580336	44510.342548	33.800692
872.625095	44572.529481	33.805709
872.899766	44634.064763	33.810727
873.716009	44685.502753	33.815744
874.666869	44750.797936	33.820762
875.278304	44813.230108	33.825780
876.746175	44873.764328	33.830797
877.212762	44939.812276	33.835815
878.137613	44991.006348	33.840832
878.933696	45061.760155	33.845850
879.873321	45125.090943	33.850868
880.624274	45182.163662	33.855885
880.987781	45246.046240	33.860903
881.878032	45309.771098	33.865920
882.968570	45385.761979	33.870938
883.745614	45453.825275	33.875956
884.709583	45523.074208	33.880973
885.311649	45590.134073	33.885991
886.462370	45660.499311	33.891008
887.632128	45739.199114	33.896026
888.643503	45788.426895	33.901044
889.367569	45862.825424	33.906061
890.132093	45937.939042	33.911079
890.989032	45990.619883	33.916096
891.997152	46052.405466	33.921114
892.264143	46115.616033	33.926132
893.436895	46172.505428	33.931149
894.620894	46234.839787	33.936167
895.396654	46295.257866	33.941184
896.128094	46351.096729	33.946202
897.127900	46409.373714	33.951220
898.036292	46461.889505	33.956237
899.065795	46530.391215	33.961255
899.648125	46589.328292	33.966272
900.496402	46662.856131	33.971290
901.245815	46728.327613	33.976308
902.019997	46798.830946	33.981325
902.923437	46875.475949	33.986343
904.030375	46939.532291	33.991360
904.491363	47012.621798	33.996378
905.721846	47085.667672	34.001396
907.012164	47151.195358	34.006413
907.599826	47230.452801	34.011431
908.729172	47304.312221	34.016448
909.576097	47361.293299	34.021466
910.676289	47436.340685	34.026484
912.198970	47493.065077	34.031501
912.922969	47571.650893	34.036519
913.812611	47639.045345	34.041536
914.556926	47696.346900	34.046554
916.029907	47754.142499	34.051572
917.418302	47807.548301	34.056589
918.518442	47850.997188	34.061607
919.486047	47913.762109	34.066624
920.564769	47969.993762	34.071642
920.763109	48025.363032	34.076660
922.078132	48073.479389	34.081677
922.961493	48144.501339	34.086695
923.802061	48192.837311	34.091712
924.531180	48258.265772	34.096730
925.474244	48327.203930	34.101748
926.527886	48379.094230	34.106765
927.045212	48447.042504	34.111783
927.816975	48510.567107	34.116800
928.824174	48577.167887	34.121818
929.500279	48657.567977	34.126836
930.416104	48714.434180	34.131853
931.329860	48787.908113	34.136871
932.266576	48850.705738	34.141888
932.947216	48931.087106	34.146906
934.199332	48999.909602	34.151924
935.449142	49070.352288	34.156941
935.725428	49148.620995	34.161959
936.763389	49218.666902	34.166976
937.445548	49293.893051	34.171994
938.397075	49368.811795	34.177012
939.411682	49441.335775	34.182029
940.124810	49519.101202	34.187047
941.376331	49598.231924	34.192064
942.210662	49681.122727	34.197082
943.273776	49752.501314	34.202100
944.509188	49817.051923	34.207117
945.504662	49895.679420	34.212135
946.388106	49964.606496	34.217152
948.068936	50021.021543	34.222170
949.068715	50094.941825	34.227188
950.662539	50147.935200	34.232205
951.348220	50203.759024	34.237223
952.336321	50262.825941	34.242240
953.579754	50316.608180	34.247258
953.968104	50374.933580	34.252276
955.040054	50421.466688	34.257293
955.287594	50475.638422	34.262311
956.280329	50528.055576	34.267328
957.159407	50586.045714	34.272346
957.339945	50652.180141	34.277364
958.610195	50720.296350	34.282381
959.406678	50783.203353	34.287399
960.227176	50838.052334	34.292416
961.038424	50910.119093	34.297434
961.687913	50994.138002	34.302452
962.883697	51059.109537	34.307469
964.065915	51141.774290	34.312487
965.087071	51200.186763	34.317504
966.455935	51278.754535	34.322522
967.148592	51349.107453	34.327540
968.182559	51409.005371	34.332557
969.105093	51484.201267	34.337575
970.023121	51550.368993	34.342592
971.413595	51608.997086	34.347610
972.014547	51692.602155	34.352628
973.166605	51767.364617	34.357645
974.369570	51840.898205	34.362663
975.462152	51917.739476	34.367680
976.638910	51975.806987	34.372698
977.397565	52042.317298	34.377716
978.530125	52101.986528	34.382733
979.664420	52175.822932	34.387751
980.372315	52243.303502	34.392768
981.568840	52308.316394	34.397786
982.180492	52380.906020	34.402804
983.312806	52455.737049	34.407821
983.723302	52538.235840	34.412839
984.835107	52608.116034	34.417856
985.712640	52685.366648	34.422874
986.997174	52768.704659	34.427892
987.868062	52842.932203	34.432909
988.652824	52915.344681	34.437927
989.424784	53001.762646	34.442944
991.018539	53078.346233	34.447962
991.498166	53161.450256	34.452980
992.978064	53243.133312	34.457997
994.113400	53324.085639	34.463015
994.605578	53406.176126	34.468032
995.997262	53489.822750	34.473050
996.825019	53585.061559	34.478068
997.499457	53653.393021	34.483085
998.701146	53731.077552	34.488103
999.710278	53811.760124	34.493120
1001.441877	53878.902557	34.498138
1002.323671	53961.541824	34.503156
1003.378145	54038.408666	34.508173
1004.850785	54102.124298	34.513191
1005.989573	54159.121061	34.518208
1007.547240	54223.475576	34.523226
1008.621917	54286.215852	34.528244
1009.581020	54340.254171	34.533261
1010.559442	54400.370920	34.538279
1011.537020	54463.044518	34.543296
1012.243686	54512.591588	34.548314
1013.097577	54582.789933	34.553332
1013.872899	54648.071067	34.558349
1015.139232	54721.768389	34.563367
1015.999269	54807.641395	34.568384
1017.117964	54858.529921	34.573402
1017.375808	54933.966945	34.578420
1019.163457	54993.788381	34.583437
1020.290340	55060.579015	34.588455
1021.166561	55126.598832	34.593472
1022.058612	55204.387053	34.598490
1022.823131	55256.957949	34.603508
1023.667554	55318.673653	34.608525
1025.092126	55373.508870	34.613543
1025.784107	55437.052198	34.618560
1026.372618	55495.169375	34.623578
1027.441481	55561.154090	34.628596
1028.009734	55629.273655	34.633613
1029.313549	55700.417834	34.638631
1029.834142	55781.328743	34.643648
1031.103822	55855.851781	34.648666
1031.754062	55938.432753	34.653684
1032.479031	56019.882227	34.658701
1033.669829	56101.734112	34.663719
1034.854780	56183.258102	34.668736
1035.753686	56263.371317	34.673754
1036.940921	56348.952157	34.678772
1038.029025	56429.023821	34.683789
1039.488636	56512.449081	34.688807
1040.234240	56602.130939	34.693824
1042.298992	56681.272998	34.698842
1043.170318	56753.848324	34.703860
1043.904724	56826.831237	34.708877
1045.174987	56906.395164	34.713895
1046.069154	56996.087020	34.718912
1046.944730	57067.934826	34.723930
1048.631002	57146.181689	34.728948
1048.952760	57230.178962	34.733965
1050.284913	57311.576303	34.738983
1051.150047	57396.179424	34.744000
1052.159018	57485.918533	34.749018
1053.510745	57572.927476	34.754036
1054.598932	57656.465176	34.759053
1055.792608	57739.290557	34.764071
1057.000392	57815.841970	34.769088
1057.682810	57889.715945	34.774106
1058.709106	57974.973226	34.779124
1059.672804	58057.734237	34.784141
1060.832240	58138.585320	34.789159
1062.627331	58223.888371	34.794176
1063.941328	58291.051333	34.799194
1064.835769	58373.925477	34.804212
1065.913717	58447.113007	34.809229
1067.464275	58519.347434	34.814247
1068.294629	58590.681509	34.819264
1069.696115	58658.812907	34.824282
1070.390122	58729.383789	34.829300
1071.699144	58796.713496	34.834317
1073.005403	58861.847556	34.839335
1073.758701	58937.701105	34.844352
1075.425001	58984.551044	34.849370
1076.710484	59059.037283	34.854388
1077.331899	59127.348391	34.859405
1078.308922	59186.660929	34.864423
1078.887930	59259.814656	34.869440
1080.302176	59332.680357	34.874458
1081.339393	59413.972476	34.879476
1082.457777	59482.586994	34.884493
1083.612285	59554.221571	34.889511
1084.243903	59626.684631	34.894528
1084.831933	59706.345015	34.899546
1085.811512	59789.862693	34.904564
1086.630608	59870.114270	34.909581
1088.194121	59945.154929	34.914599
1089.606921	60039.543535	34.919616
1090.042315	60121.330462	34.924634
1091.480090	60198.049834	34.929652
1092.559150	60289.098670	34.934669
1093.696418	60358.782433	34.939687
1094.407673	60444.059462	34.944704
1095.419491	60506.205510	34.949722
1096.214619	60584.159149	34.954740
1096.975798	60680.563246	34.959757
1097.871651	60756.628146	34.964775
1099.147651	60843.932810	34.969792
1100.300751	60928.908550	34.974810
1100.949968	61018.754714	34.979828
1101.962324	61108.709259	34.984845
1102.849588	61191.676410	34.989863
1104.078938	61296.226258	34.994880
1105.243175	61387.803964	34.999898
1106.568894	61477.698423	35.004916
1107.786103	61570.882708	35.009933
1109.348179	61664.627677	35.014951
1110.633928	61748.072731	35.019968
1111.646251	61848.949309	35.024986
1112.989467	61934.044525	35.030004
1114.207665	62018.450522	35.035021
1115.593754	62109.876111	35.040039
1116.403897	62197.112504	35.045056
1117.959868	62279.124660	35.050074
1118.713076	62355.951012	35.055092
1119.898445	62448.884034	35.060109
1121.170024	62526.832970	35.065127
1122.402839	62619.961818	35.070144
1123.728242	62702.125213	35.075162
1125.094606	62793.999523	35.080180
1126.213774	62870.593259	35.085197
1127.559315	62955.976498	35.090215
1128.103107	63039.224887	35.095232
1129.393481	63113.241585	35.100250
1130.673492	63198.540903	35.105268
1131.705465	63288.291434	35.110285
1132.545901	63367.987690	35.115303
1134.063462	63451.807559	35.120320
1135.017895	63546.559504	35.125338
1136.318788	63621.569967	35.130356
1137.741683	63711.970194	35.135373
1138.763748	63788.062769	35.140391
1139.873094	63868.117593	35.145408
1141.195656	63966.529884	35.150426
1142.369570	64036.629822	35.155444
1143.525939	64121.616026	35.160461
1144.808612	64205.221766	35.165479
1145.665098	64292.508946	35.170496
1146.880425	64374.903913	35.175514
1148.254520	64455.520828	35.180532
1148.922716	64552.916744	35.185549
1149.835278	64627.458893	35.190567
1151.504802	64721.224007	35.195584
1152.208745	64802.642739	35.200602
1153.815621	64887.529765	35.205620
1154.886135	64974.874637	35.210637
1155.819583	65045.989785	35.215655
1157.051001	65139.349840	35.220672
1158.257140	65223.920526	35.225690
1159.342755	65310.365223	35.230708
1160.778410	65400.111142	35.235725
1161.444657	65479.986847	35.240743
1163.173539	65564.078457	35.245760
1164.384689	65648.168632	35.250778
1165.244200	65729.154628	35.255796
1166.161893	65818.115306	35.260813
1167.646847	65904.442901	35.265831
1168.767907	65986.788183	35.270848
1169.944734	66075.063657	35.275866
1171.462747	66152.118174	35.280884
1171.979882	66231.291382	35.285901
1172.801812	66303.187173	35.290919
1173.952436	66391.429840	35.295936
1174.634946	66478.884632	35.300954
1175.781210	66556.511075	35.305972
1176.713144	66657.533525	35.310989
1178.127958	66740.607950	35.316007
1179.610012	66819.582147	35.321024
1180.798073	66916.070522	35.326042
1182.235470	67002.656185	35.331060
1182.929893	67087.426716	35.336077
1184.372675	67173.600582	35.341095
1185.638216	67268.786627	35.346112
1186.810329	67357.662448	35.351130
1188.647332	67440.236572	35.356148
1189.702110	67525.028445	35.361165
1190.960308	67617.329773	35.366183
1192.289960	67701.414638	35.371200
1193.035937	67780.392421	35.376218
1194.561345	67867.980373	35.381236
1195.754138	67966.377790	35.386253
1196.817144	68057.166176	35.391271
1198.011304	68139.519711	35.396288
1199.337277	68231.489791	35.401306
1200.545421	68319.040026	35.406324
1201.255664	68407.592490	35.411341
1202.716753	68501.745943	35.416359
1203.799357	68594.723961	35.421376
1204.991190	68698.170745	35.426394
1205.934967	68798.604624	35.431412
1207.106804	68901.194210	35.436429
1208.458589	68994.593998	35.441447
1210.116040	69103.630615	35.446464
1211.336117	69179.499599	35.451482
1212.654703	69274.811472	35.456500
1214.283357	69375.248636	35.461517
1215.427533	69461.400687	35.466535
1216.575343	69553.206930	35.471552
1217.541755	69651.519386	35.476570
1219.067053	69731.971190	35.481588
1220.202213	69837.071356	35.486605
1221.134987	69924.809211	35.491623
1222.390951	70012.528717	35.496640
1224.003886	70122.621358	35.501658
1224.729419	70216.920886	35.506676
1226.120488	70319.361660	35.511693
1227.334676	70416.251699	35.516711
1228.811673	70512.987211	35.521728
1229.510181	70603.708307	35.526746
1231.029526	70703.572398	35.531764
1231.871210	70808.772831	35.536781
1233.324308	70902.594320	35.541799
1234.797935	71001.858768	35.546816
1235.571160	71105.867907	35.551834
1237.386085	71194.796197	35.556852
1238.781700	71299.950380	35.561869
1240.160747	71385.325022	35.566887
1241.411723	71484.993242	35.571904
1242.592052	71581.797889	35.576922
1243.384978	71667.986587	35.581940
1244.562892	71774.379736	35.586957
1245.925629	71867.927456	35.591975
1247.425810	71966.786146	35.596992
1248.477548	72068.210054	35.602010
1250.014951	72158.945278	35.607028
1251.065666	72254.696034	35.612045
1252.209638	72352.889698	35.617063
1254.323608	72418.623359	35.622080
1255.098547	72514.202672	35.627098
1256.851220	72579.511687	35.632116
1257.628671	72667.504561	35.637133
1258.853837	72748.436666	35.642151
1260.168638	72829.165083	35.647168
1260.849830	72906.116694	35.652186
1261.966042	72990.220234	35.657204
1263.372857	73084.525352	35.662221
1264.177055	73169.007334	35.667239
1265.515937	73265.780823	35.672256
1266.987869	73369.360835	35.677274
1268.004230	73456.103223	35.682292
1269.308721	73545.954858	35.687309
1270.508144	73657.861921	35.692327
1271.936214	73757.561824	35.697344
1272.933840	73857.721749	35.702362
1274.706470	73942.840750	35.707380
1276.185671	74044.079033	35.712397
1277.787920	74141.156703	35.717415
1279.160292	74227.529538	35.722432
1280.286930	74331.458367	35.727450
1281.127300	74427.249708	35.732468
1282.144155	74529.511774	35.737485
1283.602241	74637.798103	35.742503
1284.772227	74738.162499	35.747520
1286.106937	74846.152214	35.752538
1287.384796	74958.090518	35.757556
1288.422209	75061.060741	35.762573
1289.677942	75157.879373	35.767591
1291.065650	75268.851875	35.772608
1292.201053	75388.540852	35.777626
1294.141371	75489.054156	35.782644
1295.603517	75597.584397	35.787661
1296.623771	75702.675117	35.792679
1298.098601	75797.067897	35.797696
1299.049221	75915.749286	35.802714
1300.302293	76012.432069	35.807732
1301.742222	76127.605450	35.812749
1303.257781	76231.025073	35.817767
1304.544132	76334.392099	35.822784
1306.385468	76454.457279	35.827802
1307.754101	76551.732032	35.832820
1309.124730	76656.657918	35.837837
1310.131823	76761.096096	35.842855
1311.955637	76865.508891	35.847872
1312.887669	76971.568331	35.852890
1314.275483	77067.169833	35.857908
1315.568487	77162.976443	35.862925
1317.194055	77270.474547	35.867943
1318.524437	77366.909441	35.872960
1319.771884	77475.531297	35.877978
1320.987926	77575.937067	35.882996
1322.741622	77666.657292	35.888013
1323.875206	77770.990979	35.893031
1325.713487	77861.800030	35.898048
1326.542143	77964.636431	35.903066
1328.254051	78054.211661	35.908084
1331.319792	78127.614703	35.913101
1332.496879	78194.559819	35.918119
1334.289139	78257.013510	35.923136
1335.281005	78329.308396	35.928154
1336.600046	78402.604007	35.933172
1337.792066	78467.305198	35.938189
1338.635537	78550.949153	35.943207
1339.929638	78619.485963	35.948224
1340.784373	78700.430275	35.953242
1341.948868	78779.325010	35.958260
1342.857590	78872.879114	35.963277
1344.020173	78947.442036	35.968295
1345.302686	79033.198091	35.973312
1345.994602	79116.449294	35.978330
1347.076996	79209.331414	35.983348
1348.086702	79294.738020	35.988365
1349.427260	79401.820109	35.993383
1351.011334	79494.270379	35.998400
1352.337208	79598.036318	36.003418
1353.548204	79696.892372	36.008436
1355.391819	79768.551709	36.013453
1356.204679	79885.586813	36.018471
1357.516687	79988.304857	36.023488
1358.626637	80082.617206	36.028506
1360.105010	80195.850696	36.033524
1361.759056	80304.420429	36.038541
1362.804556	80408.828487	36.043559
1364.434488	80511.841047	36.048576
1365.717308	80631.707377	36.053594
1367.263113	80729.906872	36.058612
1368.729606	80844.639822	36.063629
1370.306975	80943.063202	36.068647
1371.634590	81046.200808	36.073664
1372.649689	81158.547444	36.078682
1374.155866	81274.961020	36.083700
1376.051163	81389.211369	36.088717
1377.260044	81499.489413	36.093735
1378.914622	81598.245160	36.098752
1380.165237	81696.582683	36.103770
1381.448022	81812.855888	36.108788
1383.371115	81925.925811	36.113805
1384.704575	82032.626348	36.118823
1386.245228	82125.928314	36.123840
1387.429381	82234.971444	36.128858
1388.524051	82342.103088	36.133876
1390.163288	82445.894181	36.138893
1391.482263	82569.171397	36.143911
1393.243618	82672.982328	36.148928
1394.514848	82775.932336	36.153946
1395.437225	82886.615168	36.158964
1397.366858	82999.802411	36.163981
1398.473373	83116.526540	36.168999
1400.148559	83218.794436	36.174016
1401.158639	83326.842569	36.179034
1402.593980	83453.577214	36.184052
1403.916651	83553.696522	36.189069
1405.564511	83673.671026	36.194087
1406.881006	83781.445121	36.199104
1408.170625	83902.502668	36.204122
1409.499555	84011.720155	36.209140
1411.116459	84118.751877	36.214157
1412.378625	84239.206928	36.219175
1413.928212	84357.298979	36.224192
1415.597607	84464.957372	36.229210
1416.849678	84589.723582	36.234228
1418.635608	84688.355614	36.239245
1419.476489	84806.331746	36.244263
1421.155371	84920.097828	36.249280
1422.829478	85031.381555	36.254298
1423.868774	85144.563832	36.259316
1425.525678	85260.577489	36.264333
1426.925904	85376.492179	36.269351
1428.654393	85487.667835	36.274368
1429.799327	85594.689824	36.279386
1431.250794	85706.403626	36.284404
1432.708348	85815.874054	36.289421
1433.930246	85927.548413	36.294439
1435.926214	86035.060478	36.299456
1437.560190	86137.256503	36.304474
1438.463416	86234.966801	36.309492
1439.813302	86338.449580	36.314509
1440.701542	86442.891606	36.319527
1442.033140	86539.471824	36.324544
1443.638756	86648.086009	36.329562
1444.628123	86754.515571	36.334580
1445.845527	86869.298873	36.339597
1446.983504	86992.167068	36.344615
1448.286460	87104.758392	36.349632
1450.027949	87229.523168	36.354650
1451.383731	87354.982119	36.359668
1452.730418	87477.541083	36.364685
1453.835277	87604.256692	36.369703
1455.522957	87732.478851	36.374720
1457.348087	87854.673459	36.379738
1458.709243	87992.325153	36.384756
1460.002044	88121.941082	36.389773
1461.492730	88254.340093	36.394791
1462.922894	88390.183401	36.399808
1465.098370	88520.588802	36.404826
1466.280214	88649.451288	36.409844
1467.325294	88774.812585	36.414861
1469.031613	88901.756983	36.419879
1470.468930	89043.228926	36.424896
1472.609908	89167.394809	36.429914
1474.216289	89297.397970	36.434932
1475.940139	89427.320051	36.439949
1478.190903	89539.722470	36.444967
1479.534784	89654.053385	36.449984
1481.178674	89772.494860	36.455002
1482.962858	89880.117346	36.460020
1484.617538	89989.103750	36.465037
1486.225905	90107.146538	36.470055
1487.862975	90205.731647	36.475072
1489.471674	90316.703455	36.480090
1490.675004	90439.956023	36.485108
1491.984590	90538.593201	36.490125
1493.389792	90645.529696	36.495143
1495.018886	90763.204315	36.500160
1496.521253	90877.527920	36.505178
1497.475069	91000.884997	36.510196
1499.018404	91107.865009	36.515213
1500.482814	91233.095330	36.520231
1501.855514	91350.862853	36.525248
1503.496530	91473.278430	36.530266
1505.155154	91590.672865	36.535284
1506.892002	91713.682854	36.540301
1508.338528	91829.121405	36.545319
1509.838703	91942.004545	36.550336
1511.553143	92061.217196	36.555354
1512.511166	92174.591161	36.560372
1514.188418	92294.963875	36.565389
1515.399070	92422.418597	36.570407
1516.895656	92548.194353	36.575424
1518.722574	92668.405835	36.580442
1519.775030	92793.820803	36.585460
1521.434413	92908.685327	36.590477
1522.661001	93040.994506	36.595495
1524.124802	93172.975820	36.600512
1526.011429	93305.791797	36.605530
1527.282206	93431.238775	36.610548
1528.970653	93563.959972	36.615565
1530.347503	93694.093871	36.620583
1531.933669	93818.086434	36.625600
1533.625185	93946.473989	36.630618
1535.061767	94076.169261	36.635636
1536.703771	94188.126037	36.640653
1538.069083	94325.070914	36.645671
1539.467694	94434.227241	36.650688
1541.139547	94543.455502	36.655706
1542.880587	94661.317907	36.660724
1544.286833	94763.895753	36.665741
1545.770168	94885.158077	36.670759
1546.870828	94999.382215	36.675776
1548.600691	95112.114542	36.680794
1549.959239	95242.498657	36.685812
1551.381739	95347.154686	36.690829
1553.172236	95477.497908	36.695847
1554.243530	95605.279056	36.700864
1556.035460	95729.792316	36.705882
1557.307365	95858.557334	36.710900
1558.929443	96002.124420	36.715917
1560.622105	96130.850424	36.720935
1561.610149	96260.979571	36.725952
1563.351766	96400.473590	36.730970
1564.982028	96549.327792	36.735988
1566.617552	96687.686084	36.741005
1568.250365	96833.220103	36.746023
1569.656638	96967.584297	36.751040
1571.569925	97107.891369	36.756058
1573.205119	97256.507304	36.761076
1574.788411	97384.368130	36.766093
1576.203380	97527.302579	36.771111
1578.175373	97673.193330	36.776128
1579.880882	97804.586249	36.781146
1581.727849	97951.423129	36.786164
1583.299588	98077.957516	36.791181
1585.764810	98202.375779	36.796199
1587.151985	98336.824825	36.801216
1589.075598	98458.552184	36.806234
1590.426241	98587.645694	36.811252
1591.908769	98726.759301	36.816269
1593.816475	98848.921642	36.821287
1595.117714	98988.077281	36.826304
1596.848068	99117.075802	36.831322
1598.117394	99254.133174	36.836340
1599.710760	99380.365114	36.841357
1601.859597	99519.695392	36.846375
1603.015870	99659.155406	36.851392
1604.566912	99791.214415	36.856410
1606.235284	99929.226745	36.861428
1607.684709	100061.923871	36.866445
1609.433895	100201.775694	36.871463
1611.061749	100338.122654	36.876480
1613.172414	100470.832642	36.881498
1614.755383	100606.896138	36.886516
1616.482727	100734.507071	36.891533
1618.127177	100864.945866	36.896551
1619.121755	100999.860171	36.901568
1621.237585	101128.020721	36.906586
1622.512219	101264.705467	36.911604
1624.297557	101395.479445	36.916621
1626.243997	101527.052942	36.921639
1627.916683	101670.612301	36.926656
1629.568623	101797.909513	36.931674
1631.096316	101932.250254	36.936692
1632.464430	102060.632272	36.941709
1634.116701	102192.089416	36.946727
1635.659453	102330.017389	36.951744
1637.405912	102455.565518	36.956762
1638.704169	102596.106368	36.961780
1640.695818	102721.211640	36.966797
1642.430330	102859.530377	36.971815
1644.044809	102989.120170	36.976832
1645.615850	103125.829932	36.981850
1647.474594	103251.236830	36.986868
1648.861180	103358.435000	36.991885
1650.848806	103471.524337	36.996903
1652.217601	103588.044897	37.001920
1653.455457	103708.567400	37.006938
1655.140032	103818.471985	37.011956
1656.342630	103947.013890	37.016973
1657.872766	104066.541280	37.021991
1658.975833	104204.418714	37.027008
1661.054273	104329.301009	37.032026
1663.235846	104457.134633	37.037044
1664.931380	104584.537228	37.042061
1666.676017	104710.373123	37.047079
1668.383799	104844.393352	37.052096
1670.519224	104971.526087	37.057114
1671.846711	105095.031962	37.062132
1673.730161	105218.540516	37.067149
1675.323148	105333.409308	37.072167
1676.998561	105477.542624	37.077184
1678.928923	105595.314125	37.082202
1680.785700	105730.468535	37.087220
1682.235389	105858.586244	37.092237
1683.828106	105989.230795	37.097255
1685.638165	106132.509090	37.102272
1687.446414	106251.836135	37.107290
1688.699190	106393.439777	37.112308
1689.883793	106520.865816	37.117325
1691.867981	106658.489358	37.122343
1693.453529	106804.924699	37.127360
1695.102244	106954.026328	37.132378
1696.875182	107100.585934	37.137396
1698.314357	107248.250568	37.142413
1700.339635	107400.922066	37.147431
1701.943092	107547.484603	37.152448
1703.956186	107689.660018	37.157466
1705.527981	107832.741612	37.162484
1707.579407	107978.564207	37.167501
1709.170581	108117.028289	37.172519
1710.431391	108289.008291	37.177536
1712.480816	108423.839050	37.182554
1714.396716	108582.454653	37.187572
1715.392409	108737.295865	37.192589
1717.406259	108888.162392	37.197607
1718.971334	109050.512162	37.202624
1720.816869	109201.583778	37.207642
1722.430498	109366.108575	37.212660
1724.134298	109522.453553	37.217677
1725.657353	109680.513941	37.222695
1727.448827	109846.649180	37.227712
1729.334780	110008.078468	37.232730
1731.361552	110161.434003	37.237748
1732.478513	110321.995286	37.242765
1735.144025	110478.017311	37.247783
1736.312133	110643.327603	37.252800
1738.197371	110801.184492	37.257818
1740.078610	110958.446678	37.262836
1741.653188	111120.715786	37.267853
1743.689561	111272.819190	37.272871
1745.366353	111442.137529	37.277888
1747.141695	111599.051273	37.282906
1748.914660	111751.261133	37.287924
1750.348808	111908.039116	37.292941
1752.127351	112069.431130	37.297959
1753.977702	112236.532266	37.302976
1755.518846	112391.685110	37.307994
1757.617014	112548.641563	37.313012
1759.606651	112705.666323	37.318029
1761.366142	112860.457478	37.323047
1763.179240	113010.332929	37.328064
1764.661420	113151.522408	37.333082
1766.519788	113279.527669	37.338100
1768.092943	113424.369253	37.343117
1769.635789	113558.220462	37.348135
1771.422947	113701.875750	37.353152
1772.992428	113845.514756	37.358170
1774.752428	113990.469033	37.363188
1776.364411	114148.408583	37.368205
1778.090134	114295.525462	37.373223
1779.669126	114444.415990	37.378240
1781.558841	114602.365014	37.383258
1783.498285	114752.811417	37.388276
1785.280533	114904.817536	37.393293
1786.965813	115062.635490	37.398311
1788.924235	115224.432127	37.403328
1790.221121	115384.886567	37.408346
1792.177907	115548.295634	37.413364
1793.659665	115724.868405	37.418381
1796.028202	115884.397240	37.423399
1797.837508	116053.729208	37.428416
1799.271962	116220.989489	37.433434
1801.115226	116394.972524	37.438452
1802.743420	116567.543931	37.443469
1804.888184	116736.776074	37.448487
1806.797418	116923.942192	37.453504
1808.465619	117100.758849	37.458522
1810.122582	117265.553931	37.463540
1811.654066	117446.109826	37.468557
1813.697699	117624.443312	37.473575
1815.589978	117803.397346	37.478592
1817.363287	117985.529052	37.483610
1819.617705	118169.717674	37.488628
1821.514610	118346.872439	37.493645
1823.447984	118522.779314	37.498663
1825.446702	118707.023037	37.503680
1827.158997	118881.875146	37.508698
1829.425762	119056.705186	37.513716
1831.013038	119233.468333	37.518733
1832.789675	119403.188339	37.523751
1834.607831	119582.707744	37.528768
1836.709833	119758.746304	37.533786
1839.305368	119932.387578	37.538804
1840.833417	120108.199957	37.543821
1842.683529	120272.737040	37.548839
1844.303934	120452.963585	37.553856
1846.139238	120621.715809	37.558874
1848.346873	120797.400194	37.563892
1850.331161	120971.306191	37.568909
1851.802061	121134.675527	37.573927
1854.108661	121305.526516	37.578944
1855.574160	121480.619138	37.583962
1857.445160	121644.245473	37.588980
1859.418384	121818.448742	37.593997
1861.286053	121990.969388	37.599015
1863.429272	122164.158289	37.604032
1865.295710	122337.492516	37.609050
1867.022539	122505.140787	37.614068
1868.294663	122682.082897	37.619085
1870.322617	122862.320581	37.624103
1871.974964	123049.505835	37.629120
1873.347578	123229.745705	37.634138
1875.473388	123408.664025	37.639156
1877.302735	123602.877613	37.644173
1879.192382	123782.303747	37.649191
1880.964299	123978.760816	37.654208
1882.711301	124158.160099	37.659226
1884.397021	124334.943716	37.664244
1886.203160	124529.546006	37.669261
1887.922432	124707.074522	37.674279
1889.859798	124867.697239	37.679296
1891.527106	125055.955216	37.684314
1893.343229	125236.338085	37.689332
1895.003416	125410.834183	37.694349
1896.585844	125594.502730	37.699367
1898.653176	125785.099576	37.704384
1899.986510	125977.359310	37.709402
1902.035490	126161.554075	37.714420
1903.777771	126365.030377	37.719437
1905.650322	126554.126049	37.724455
1907.556544	126755.371289	37.729472
1909.298296	126969.507573	37.734490
1911.659254	127167.740712	37.739508
1913.766072	127374.692245	37.744525
1915.932446	127570.534393	37.749543
1917.809271	127766.435218	37.754560
1919.446246	127970.075401	37.759578
1921.705264	128169.039684	37.764596
1924.025945	128376.876415	37.769613
1925.995105	128582.167987	37.774631
1927.600813	128776.796278	37.779648
1929.573845	128995.144607	37.784666
1931.382194	129193.092783	37.789684
1933.766608	129403.690570	37.794701
1935.882709	129624.087973	37.799719
1937.570263	129820.598813	37.804736
1939.313770	130026.160927	37.809754
1941.554625	130239.893725	37.814772
1943.545707	130442.729500	37.819789
1945.593580	130651.228920	37.824807
1947.468255	130864.971091	37.829824
1948.996204	131075.976911	37.834842
1951.536692	131288.424889	37.839860
1953.624973	131500.068809	37.844877
1955.636070	131707.614780	37.849895
1957.929769	131906.743468	37.854912
1959.903867	132110.630205	37.859930
1962.338307	132308.698388	37.864948
1964.317342	132514.032733	37.869965
1966.106628	132717.938392	37.874983
1968.553048	132915.956718	37.880000
1970.473590	133115.732690	37.885018
1972.587299	133305.442718	37.890036
1974.517210	133511.614156	37.895053
1976.501967	133710.075890	37.900071
1978.393030	133904.606847	37.905088
1979.961970	134105.837810	37.910106
1981.801224	134317.229591	37.915124
1983.740508	134522.554116	37.920141
1986.058741	134725.980684	37.925159
1987.874837	134927.214962	37.930176
1989.753778	135147.943755	37.935194
1991.563923	135348.622524	37.940212
1993.426299	135561.082490	37.945229
1995.220583	135771.955186	37.950247
1997.589760	135983.932207	37.955264
1999.497726	136201.666921	37.960282
2001.460449	136413.176245	37.965300
2003.637718	136625.922130	37.970317
2005.093605	136843.286134	37.975335
2007.222920	137059.137796	37.980352
2008.881812	137283.134436	37.985370
2011.131413	137494.819843	37.990388
2012.882854	137712.649562	37.995405
2014.885848	137939.374943	38.000423
2017.049831	138156.964889	38.005440
2019.213500	138373.071156	38.010458
2020.849877	138565.402893	38.015476
2023.213218	138778.015537	38.020493
2024.648010	138978.248313	38.025511
2026.630247	139181.924669	38.030528
2028.107385	139382.634814	38.035546
2030.271246	139607.249339	38.040564
2032.398283	139827.784307	38.045581
2034.377239	140043.368632	38.050599
2036.161900	140250.925604	38.055616
2037.969403	140482.833419	38.060634
2039.709946	140710.856711	38.065652
2042.300087	140934.408598	38.070669
2043.938318	141175.280469	38.075687
2045.939702	141406.743784	38.080704
2047.892939	141644.662746	38.085722
2049.838042	141891.975554	38.090740
2051.609882	142127.196532	38.095757
2053.682006	142373.337128	38.100775
2055.644463	142623.658774	38.105792
2057.862508	142882.698955	38.110810
2060.558622	143127.286725	38.115828
2062.128918	143382.051811	38.120845
2064.214544	143634.263156	38.125863
2066.599466	143884.297016	38.130880
2068.491255	144150.032333	38.135898
2070.775508	144407.039526	38.140916
2073.343643	144649.078296	38.145933
2075.189925	144897.919191	38.150951
2077.880433	145139.941282	38.155968
2079.872922	145395.526677	38.160986
2082.204685	145641.630365	38.166004
2084.518734	145886.913016	38.171021
2086.497763	146148.812279	38.176039
2089.042643	146375.543469	38.181056
2090.885143	146636.578020	38.186074
2093.536027	146883.945335	38.191092
2095.853510	147121.770255	38.196109
2097.926495	147372.771036	38.201127
2100.267486	147602.154005	38.206144
2102.114007	147853.205043	38.211162
2104.026087	148091.173648	38.216180
2106.500819	148330.718514	38.221197
2108.398188	148577.449587	38.226215
2110.378083	148814.776277	38.231232
2112.415019	149056.931144	38.236250
2114.776485	149298.884294	38.241268
2116.911467	149537.395911	38.246285
2118.814788	149794.908079	38.251303
2120.848023	150029.084003	38.256320
2123.026538	150283.547419	38.261338
2125.380591	150533.237446	38.266356
2127.703232	150764.109362	38.271373
2129.331956	151011.655072	38.276391
2131.782675	151264.430597	38.281408
2133.740757	151516.471581	38.286426
2135.647505	151765.310250	38.291444
2137.812362	152018.895356	38.296461
2139.498985	152275.754852	38.301479
2141.199169	152528.437201	38.306496
2143.605392	152790.531136	38.311514
2145.784590	153056.253985	38.316532
2148.004114	153302.765985	38.321549
2150.171582	153563.948658	38.326567
2152.817007	153823.864923	38.331584
2154.973372	154087.907896	38.336602
2156.718967	154343.434809	38.341620
2158.932148	154589.915323	38.346637
2161.217617	154847.086875	38.351655
2163.060245	155088.092523	38.356672
2164.810590	155326.054209	38.361690
2166.785844	155570.379839	38.366708
2168.965970	155807.971954	38.371725
2171.029592	156053.352195	38.376743
2172.886726	156304.884369	38.381760
2175.330230	156548.988892	38.386778
2177.130435	156816.743112	38.391796
2179.216837	157072.952603	38.396813
2181.770291	157331.248625	38.401831
2183.571932	157587.606212	38.406848
2185.419305	157855.446638	38.411866
2187.609758	158122.968274	38.416884
2189.971501	158385.246804	38.421901
2191.604646	158671.735046	38.426919
2193.921723	158955.553790	38.431936
2196.204342	159228.778762	38.436954
2198.213729	159514.463396	38.441972
2200.806408	159797.303707	38.446989
2202.789482	160091.170868	38.452007
2204.987224	160380.841924	38.457024
2207.380113	160663.425286	38.462042
2209.217302	160964.212900	38.467060
2211.783466	161261.460699	38.472077
2213.798401	161558.871859	38.477095
2216.029622	161861.849553	38.482112
2218.310737	162160.669412	38.487130
2220.395673	162463.101415	38.492148
2222.827380	162758.828236	38.497165
2224.830408	163069.045700	38.502183
2227.314184	163385.740958	38.507200
2229.401968	163678.351492	38.512218
2231.667679	163993.598191	38.517236
2234.216129	164294.874700	38.522253
2236.841029	164596.864366	38.527271
2239.363162	164899.874402	38.532288
2241.909740	165200.342739	38.537306
2244.210996	165494.540489	38.542324
2247.104790	165782.387957	38.547341
2249.100843	166078.959194	38.552359
2251.823660	166372.815822	38.557376
2254.046901	166667.564040	38.562394
2256.516763	166948.829370	38.567412
2258.738662	167234.692554	38.572429
2260.983646	167524.616285	38.577447
2262.992243	167816.292078	38.582464
2265.268299	168108.194091	38.587482
2267.396385	168403.662781	38.592500
2269.904597	168691.633113	38.597517
2271.934729	168996.667636	38.602535
2274.117883	169291.598157	38.607552
2276.568990	169578.882599	38.612570
2278.489329	169892.533957	38.617588
2281.373620	170184.413246	38.622605
2283.217631	170479.071235	38.627623
2285.513121	170771.526987	38.632640
2288.056982	171061.354973	38.637658
2290.017330	171367.908545	38.642676
2292.485027	171660.493358	38.647693
2294.436951	171967.545891	38.652711
2296.670218	172266.607191	38.657728
2299.181214	172562.756776	38.662746
2301.358984	172871.682453	38.667764
2303.296629	173171.567853	38.672781
2305.851065	173486.151353	38.677799
2308.020654	173799.043713	38.682816
2310.391654	174086.459400	38.687834
2312.461670	174394.811085	38.692852
2314.893934	174681.825766	38.697869
2316.860045	174968.761650	38.702887
2319.178936	175253.738947	38.707904
2321.398139	175536.942330	38.712922
2323.151379	175836.091926	38.717940
2325.474325	176117.439950	38.722957
2327.627486	176418.205600	38.727975
2329.970078	176725.711061	38.732992
2332.408881	177024.326540	38.738010
2334.369949	177336.426941	38.743028
2336.610158	177648.942202	38.748045
2338.684395	177956.786004	38.753063
2341.135424	178276.178742	38.758080
2343.514562	178613.488864	38.763098
2345.627539	178939.209774	38.768116
2348.116272	179259.539979	38.773133
2350.584276	179591.963771	38.778151
2352.714716	179924.898505	38.783168
2355.738335	180255.841456	38.788186
2357.928128	180590.064716	38.793204
2360.576766	180920.687507	38.798221
2363.093152	181253.617897	38.803239
2365.272839	181582.258836	38.808256
2367.795264	181921.413221	38.813274
2369.916251	182259.361407	38.818292
2372.089614	182589.987953	38.823309
2374.661514	182942.040668	38.828327
2376.484163	183289.055396	38.833344
2379.755585	183623.756194	38.838362
2382.498631	183964.407470	38.843380
2384.981539	184296.922026	38.848397
2387.211322	184649.237390	38.853415
2389.635380	184991.795985	38.858432
2392.281560	185331.679690	38.863450
2394.418334	185686.222897	38.868468
2397.402121	186002.917744	38.873485
2399.843002	186368.363038	38.878503
2402.023997	186767.097827	38.883520
2404.941184	187096.887059	38.888538
2407.584512	187431.647451	38.893556
2409.813400	187753.824393	38.898573
2412.454062	188093.184602	38.903591
2414.889415	188436.311591	38.908608
2417.733733	188768.504883	38.913626
2419.426206	189110.047802	38.918644
2421.577650	189446.262545	38.923661
2424.855264	189778.772426	38.928679
2427.493111	190116.386675	38.933696
2430.415500	190431.351451	38.938714
2432.742892	190758.805021	38.943732
2434.591317	191088.315279	38.948749
2437.704666	191420.753859	38.953767
2439.656588	191752.916909	38.958784
2442.337263	192082.351210	38.963802
2444.442992	192410.936060	38.968820
2446.461372	192742.812078	38.973837
2449.355766	193080.572642	38.978855
2451.529296	193424.390102	38.983872
2454.083352	193764.059734	38.988890
2456.003618	194098.393097	38.993908
2458.033856	194434.513688	38.998925
2460.822556	194779.636110	39.003943
2462.934702	195133.907543	39.008960
2465.754898	195472.473369	39.013978
2468.106581	195823.229381	39.018996
2470.632181	196168.294726	39.024013
2473.008812	196509.116678	39.029031
2475.257201	196863.117396	39.034048
2477.557715	197182.209153	39.039066
2480.252389	197508.962374	39.044084
2482.540745	197836.033584	39.049101
2485.015133	198159.190113	39.054119
2487.411549	198476.390066	39.059136
2489.926280	198802.132698	39.064154
2491.997226	199132.060202	39.069172
2494.574133	199469.555662	39.074189
2496.765627	199811.404775	39.079207
2499.057077	200159.538786	39.084224
2501.522263	200509.323060	39.089242
2503.852643	200870.661655	39.094260
2506.033917	201224.505195	39.099277
2508.962401	201589.435609	39.104295
2511.070928	201952.030392	39.109312
2513.464776	202320.068455	39.114330
2515.741033	202699.861525	39.119348
2517.537095	203074.243202	39.124365
2520.834799	203451.262456	39.129383
2523.492041	203841.972551	39.134400
2525.338965	204236.061111	39.139418
2528.032473	204623.668067	39.144436
2530.627258	205005.219907	39.149453
2534.026072	205402.244687	39.154471
2535.999901	205806.960454	39.159488
2538.853687	206192.259278	39.164506
2541.404226	206588.961126	39.169524
2544.235918	206971.826133	39.174541
2547.207162	207371.969571	39.179559
2549.596105	207768.063648	39.184576
2552.260780	208157.713919	39.189594
2554.822026	208564.553489	39.194612
2557.496651	208955.245069	39.199629
2560.202199	209344.814724	39.204647
2562.805244	209741.920319	39.209664
2565.235502	210135.496957	39.214682
2568.141338	210532.810684	39.219700
2571.198933	210926.494101	39.224717
2574.331305	211313.688567	39.229735
2576.478897	211693.212547	39.234752
2579.099756	212085.466745	39.239770
2581.783904	212473.393008	39.244788
2584.468896	212863.174091	39.249805
2586.889143	213254.800513	39.254823
2589.571897	213650.070083	39.259840
2592.184891	214032.420506	39.264858
2594.957530	214435.247289	39.269876
2597.574937	214828.851726	39.274893
2600.575449	215210.253967	39.279911
2603.277556	215601.000805	39.284928
2605.579734	215980.530976	39.289946
2608.440322	216369.043757	39.294964
2610.604576	216761.958501	39.299981
2613.488679	217143.456842	39.304999
2616.072338	217546.138282	39.310016
2618.593595	217922.892371	39.315034
2621.423131	218315.831867	39.320052
2623.522685	218711.044582	39.325069
2626.368606	219101.695725	39.330087
2628.928820	219497.015104	39.335104
2631.498771	219885.931403	39.340122
2634.166369	220278.973578	39.345140
2636.377462	220673.280992	39.350157
2639.356687	221065.538358	39.355175
2641.918460	221471.960109	39.360192
2644.550130	221866.075596	39.365210
2647.936190	222271.835914	39.370228
2649.732486	222653.532082	39.375245
2652.721842	223019.876465	39.380263
2654.895996	223394.883572	39.385280
2657.223323	223761.788426	39.390298
2659.781615	224125.380276	39.395316
2662.360517	224509.368460	39.400333
2664.786351	224886.623021	39.405351
2666.745570	225284.349720	39.410368
2668.875939	225678.772675	39.415386
2671.922773	226065.126935	39.420404
2674.414267	226479.486710	39.425421
2677.270609	226875.092264	39.430439
2679.771926	227288.154830	39.435456
2682.530665	227702.269648	39.440474
2685.379119	228096.555241	39.445492
2687.776398	228509.836995	39.450509
2691.044497	228934.567373	39.455527
2693.275333	229360.094132	39.460544
2695.883451	229781.065504	39.465562
2698.579542	230211.701951	39.470580
2701.111440	230644.802536	39.475597
2703.399472	231075.832315	39.480615
2706.200025	231523.193077	39.485632
2708.815315	231972.665515	39.490650
2711.771847	232416.038401	39.495668
2714.511262	232875.804894	39.500685
2717.401682	233317.180485	39.505703
2719.989095	233771.558861	39.510720
2723.175135	234208.899289	39.515738
2726.799360	234656.180250	39.520756
2729.293034	235100.588254	39.525773
2732.504911	235542.927948	39.530791
2735.699956	235985.218986	39.535808
2738.269594	236416.683250	39.540826
2741.533193	236843.466366	39.545844
2744.092247	237286.718606	39.550861
2747.222450	237715.121886	39.555879
2750.145976	238146.783053	39.560896
2752.542214	238580.278559	39.565914
2755.931983	239012.780548	39.570932
2758.562809	239441.233859	39.575949
2761.518936	239867.883093	39.580967
2764.439959	240296.315403	39.585984
2767.771478	240715.639567	39.591002
2770.535039	241132.206296	39.596020
2773.279883	241563.737844	39.601037
2775.887703	241982.308919	39.606055
2778.530702	242406.919796	39.611072
2780.883355	242832.032379	39.616090
2784.031015	243260.551528	39.621108
2786.946825	243689.690242	39.626125
2789.287347	244101.110133	39.631143
2792.146946	244532.669280	39.636160
2795.508035	244958.002015	39.641178
2798.492075	245383.748217	39.646196
2800.677949	245821.963544	39.651213
2803.484197	246245.195348	39.656231
2805.966730	246685.293246	39.661248
2808.413697	247117.647869	39.666266
2811.725449	247545.929530	39.671284
2814.340048	247984.098693	39.676301
2816.918800	248425.498508	39.681319
2820.011384	248862.117829	39.686336
2822.479531	249302.796017	39.691354
2825.436829	249743.828805	39.696372
2828.165066	250189.341491	39.701389
2830.920272	250632.181564	39.706407
2833.830229	251069.255485	39.711424
2836.353482	251500.723744	39.716442
2839.095724	251918.541294	39.721460
2841.591988	252351.205316	39.726477
2844.376555	252757.405346	39.731495
2847.219451	253179.776134	39.736512
2850.178993	253600.603471	39.741530
2853.151811	254020.132052	39.746548
2855.455614	254443.294341	39.751565
2858.082164	254872.653909	39.756583
2860.728697	255313.312671	39.761600
2863.413819	255753.227386	39.766618
2866.230320	256192.510606	39.771636
2868.766470	256651.115480	39.776653
2871.608705	257101.568197	39.781671
2874.684153	257554.269151	39.786688
2877.417654	258021.043003	39.791706
2880.457455	258492.288805	39.796724
2883.339198	258967.342126	39.801741
2886.283040	259431.969711	39.806759
2889.038463	259889.080893	39.811776
2892.141672	260371.866796	39.816794
2895.593323	260844.334788	39.821812
2898.272450	261324.998335	39.826829
2901.329760	261792.265982	39.831847
2904.843542	262262.305464	39.836864
2907.924172	262722.199634	39.841882
2911.546618	263185.182542	39.846900
2913.994041	263660.157172	39.851917
2916.825185	264121.989237	39.856935
2919.646152	264595.580812	39.861952
2922.409090	265077.688051	39.866970
2925.809304	265546.486305	39.871988
2927.987734	266031.219968	39.877005
2930.932128	266506.536104	39.882023
2934.200183	266991.705159	39.887040
2936.992566	267485.657610	39.892058
2940.215314	267954.878588	39.897076
2942.538847	268456.163064	39.902093
2945.674926	268953.076951	39.907111
2948.539106	269447.008155	39.912128
2951.518894	269945.058637	39.917146
2954.487089	270434.269769	39.922164
2958.289700	270932.796401	39.927181
2961.498576	271429.609446	39.932199
2964.751298	271916.101528	39.937216
2967.823905	272396.574395	39.942234
2970.964384	272875.967379	39.947252
2974.362803	273362.225572	39.952269
2977.367041	273833.888325	39.957287
2980.585967	274309.502342	39.962304
2983.238131	274801.354124	39.967322
2986.344650	275263.215237	39.972340
2989.317289	275749.830632	39.977357
2992.226796	276228.224587	39.982375
2995.064300	276705.712659	39.987392
2998.063017	277183.858486	39.992410
3000.874716	277671.452352	39.997428
3004.100762	278159.664394	40.002445
3006.506063	278638.807957	40.007463
3010.187534	279120.289480	40.012480
3012.660444	279602.438548	40.017498
3015.517507	280092.651146	40.022516
3018.786223	280590.668860	40.027533
3021.311272	281087.732396	40.032551
3024.429208	281580.967339	40.037568
3027.064959	282089.510536	40.042586
3029.927893	282584.048075	40.047604
3032.823557	283087.896672	40.052621
3035.589969	283585.464177	40.057639
3038.775003	284063.079891	40.062656
3041.174789	284545.461528	40.067674
3044.306428	285014.546860	40.072692
3046.766909	285510.294529	40.077709
3050.971963	285963.157948	40.082727
3054.116925	286425.019952	40.087744
3057.126456	286905.106270	40.092762
3060.391235	287375.068670	40.097780
3063.149504	287863.668192	40.102797
3066.133813	288344.103488	40.107815
3069.541448	288830.055548	40.112832
3072.168040	289319.959623	40.117850
3075.346998	289816.147230	40.122868
3077.981087	290306.855098	40.127885
3080.853421	290807.576899	40.132903
3083.992913	291316.098868	40.137920
3086.600269	291833.586176	40.142938
3089.715758	292347.740112	40.147956
3092.564248	292873.052147	40.152973
3095.458266	293402.948125	40.157991
3098.437172	293935.162086	40.163008
3101.718909	294487.280273	40.168026
3104.691394	295016.895849	40.173044
3107.447557	295578.758911	40.178061
3110.674024	296132.266664	40.183079
3114.230480	296671.398683	40.188096
3116.811140	297231.825889	40.193114
3120.470582	297797.182699	40.198132
3123.306626	298360.478651	40.203149
3126.657062	298936.788836	40.208167
3129.942991	299484.974082	40.213184
3132.941104	300061.530516	40.218202
3136.185344	300627.278641	40.223220
3139.846904	301202.171214	40.228237
3142.885923	301759.790426	40.233255
3146.084911	302332.965878	40.238272
3149.289194	302913.039219	40.243290
3152.658894	303480.413175	40.248308
3156.082443	304058.383563	40.253325
3159.292865	304632.598371	40.258343
3162.496822	305201.603987	40.263360
3165.712471	305764.712339	40.268378
3169.126353	306339.891748	40.273396
3172.604430	306906.728798	40.278413
3175.744999	307475.211121	40.283431
3179.012596	308038.285990	40.288448
3182.104454	308610.544984	40.293466
3185.343606	309175.108896	40.298484
3189.054859	309741.141130	40.303501
3192.089391	310307.576651	40.308519
3195.912990	310869.060225	40.313536
3199.709812	311419.932003	40.318554
3203.092626	311968.069915	40.323572
3206.470274	312519.704811	40.328589
3209.281285	313075.685310	40.333607
3212.617788	313614.217425	40.338624
3215.356708	314169.409290	40.343642
3218.523666	314719.553479	40.348660
3221.667365	315280.683865	40.353677
3224.546695	315840.427257	40.358695
3227.642139	316391.349110	40.363712
3230.991608	316955.878177	40.368730
3233.997956	317513.956756	40.373748
3237.545748	318066.284858	40.378765
3240.575759	318625.056319	40.383783
3243.866370	319198.219597	40.388800
3247.165922	319759.700702	40.393818
3250.388869	320310.198515	40.398836
3253.424528	320840.696787	40.403853
3256.039829	321360.900626	40.408871
3259.025880	321889.947175	40.413888
3262.835459	322422.132345	40.418906
3266.094187	322947.672208	40.423924
3269.262388	323481.364750	40.428941
3272.134411	324024.129717	40.433959
3274.878377	324565.740311	40.438976
3277.969140	325125.051203	40.443994
3280.929630	325678.082217	40.449012
3284.194773	326235.752269	40.454029
3287.045186	326820.449988	40.459047
3290.367655	327384.539836	40.464064
3293.805937	327966.668311	40.469082
3297.235683	328533.820572	40.474100
3300.765661	329118.886326	40.479117
3303.360700	329709.619646	40.484135
3306.790517	330299.579902	40.489152
3310.248781	330896.249770	40.494170
3313.789324	331493.709456	40.499188
3316.868769	332089.963175	40.504205
3320.307300	332704.721495	40.509223
3323.833777	333313.291747	40.514240
3327.442925	333925.365458	40.519258
3330.595267	334551.071796	40.524276
3334.019125	335156.533392	40.529293
3337.006161	335766.061009	40.534311
3340.664353	336390.998157	40.539328
3343.776676	337011.951135	40.544346
3347.142714	337628.288360	40.549364
3350.646807	338270.440320	40.554381
3354.011461	338894.137381	40.559399
3357.155334	339525.492498	40.564416
3360.387311	340173.841592	40.569434
3363.989597	340821.892974	40.574452
3368.002787	341459.825004	40.579469
3371.192873	342098.380782	40.584487
3374.745510	342725.227537	40.589504
3378.582588	343360.920469	40.594522
3382.285715	344006.310309	40.599540
3385.510812	344638.828761	40.604557
3389.058509	345266.517702	40.609575
3392.600165	345895.108936	40.614592
3396.374578	346516.780062	40.619610
3400.061676	347145.325384	40.624628
3403.743556	347768.788167	40.629645
3407.433578	348396.117686	40.634663
3411.199394	348994.668886	40.639680
3415.024978	349609.554789	40.644698
3418.653076	350229.784641	40.649716
3422.129477	350825.532984	40.654733
3425.291317	351432.779798	40.659751
3428.917990	352037.103177	40.664768
3432.328143	352636.073853	40.669786
3435.408799	353241.575107	40.674804
3439.014775	353836.334835	40.679821
3442.484498	354450.524687	40.684839
3445.944280	355050.785850	40.689856
3449.444287	355650.775774	40.694874
3452.447888	356259.526866	40.699892
3456.374881	356862.925493	40.704909
3459.912706	357475.549670	40.709927
3463.217156	358072.075642	40.714944
3466.874680	358676.165168	40.719962
3469.939496	359277.039667	40.724980
3473.439531	359887.416162	40.729997
3476.715021	360492.720430	40.735015
3479.988385	361081.896270	40.740020
3482.956863	361642.651837	40.745024
3485.832182	362168.191743	40.750029
3488.868828	362649.508269	40.755034
3491.485721	363099.602347	40.760039
3493.958803	363490.100440	40.765044
3496.302616	363832.919730	40.770048
3498.200693	364150.166403	40.775053
3500.387910	364420.586585	40.780058
3502.304923	364646.809493	40.785063
3504.546951	364839.110283	40.790068
3505.864877	365007.872833	40.795072
3506.943790	365135.459120	40.800077
3508.367262	365224.929511	40.805082
3509.573783	365304.143025	40.810087
3510.934222	365351.292568	40.815092
3511.740767	365351.726245	40.820096
3512.366574	365357.600006	40.825101
3513.114104	365323.360575	40.830106
3514.172743	365272.531871	40.835111
3514.737756	365199.293473	40.840116
3515.138007	365129.205771	40.845120
3515.232854	365038.991056	40.850125
3515.831645	364924.381590	40.855130
3515.996597	364796.931545	40.860135
3516.341760	364667.725101	40.865140
3516.543629	364533.636453	40.870144
3516.202791	364388.019689	40.875149
3516.794144	364241.164543	40.880154
3516.310665	364092.849723	40.885159
3516.620409	363918.416807	40.890164
3517.041985	363757.686666	40.895168
3516.676035	363589.861818	40.900173
3516.657445	363414.104882	40.905178
3516.544615	363240.953395	40.910183
3516.543039	363056.476024	40.915188
3516.559729	362874.738986	40.920192
3516.266137	362690.482652	40.925197
3516.709298	362511.014794	40.930202
3516.001060	362334.875975	40.935207
3515.671995	362152.629286	40.940212
3515.838779	361964.790097	40.945216
3515.536708	361795.750838	40.950221
3515.782250	361601.366399	40.955226
3515.335079	361430.187678	40.960231
3515.158449	361247.632224	40.965236
3515.208198	361064.354310	40.970240
3514.945637	360898.327863	40.975245
3514.719997	360713.438879	40.980250
3514.361709	360532.050901	40.985255
3513.998703	360359.226593	40.990260
3513.886661	360194.977141	40.995264
3513.639031	360031.383218	41.000269
3513.261938	359856.194836	41.005274
3513.060077	359703.163808	41.010279
3512.898582	359540.087506	41.015284
3512.905669	359388.902959	41.020288
3512.594272	359228.059271	41.025293
3512.500070	359076.126529	41.030298
3511.979798	358935.110997	41.035303
3511.860696	358771.896918	41.040308
3512.384686	358618.366283	41.045312
3511.779976	358483.918619	41.050317
3511.612144	358330.900826	41.055322
3511.737817	358184.266429	41.060327
3511.271098	358039.121312	41.065332
3511.180642	357898.898217	41.070336
3510.745619	357768.029883	41.075341
3510.877910	357622.992908	41.080346
3510.905144	357496.092442	41.085351
3510.849183	357360.182066	41.090356
3510.706974	357228.350937	41.095360
3510.261040	357096.617339	41.100365
3510.293960	356972.306195	41.105370
3509.758328	356836.722318	41.110375
3509.691278	356708.155874	41.115380
3509.669317	356590.637697	41.120384
3509.607441	356475.285626	41.125389
3509.532958	356348.497955	41.130394
3509.527672	356221.190681	41.135399
3509.276270	356121.878847	41.140404
3509.433589	356007.939652	41.145408
3508.847778	355876.730977	41.150413
3508.934396	355754.973658	41.155418
3508.588890	355656.259564	41.160423
3508.463573	355557.841309	41.165428
3508.203591	355448.641651	41.170432
3507.941310	355338.806554	41.175437
3508.025671	355232.907563	41.180442
3508.051317	355129.254035	41.185447
3508.045716	355036.610558	41.190452
3507.821266	354936.629934	41.195456
3507.546760	354840.774349	41.200461
3507.462500	354747.506835	41.205466
3507.327064	354657.983342	41.210471
3507.310695	354559.824601	41.215476
3507.346713	354472.078529	41.220480
3507.021334	354383.727598	41.225485
3506.962865	354289.488856	41.230490
3506.528175	354204.229954	41.235495
3506.681601	354123.378231	41.240500
3506.955797	354038.339001	41.245504
3506.739271	353962.653399	41.250509
3506.586787	353879.306879	41.255514
3506.344166	353802.582824	41.260519
3506.474984	353725.063352	41.265524
3506.475413	353636.939238	41.270528
3506.641554	353544.620522	41.275533
3506.516152	353469.936292	41.280538
3506.469012	353395.798910	41.285543
3506.543581	353312.974775	41.290548
3506.362075	353223.098547	41.295552
3505.959650	353161.445492	41.300557
3505.630625	353076.904259	41.305562
3506.151706	353004.202655	41.310567
3505.889300	352938.257063	41.315572
3506.164524	352859.009969	41.320576
3505.914081	352793.570590	41.325581
3505.740753	352711.774804	41.330586
3505.824124	352649.740141	41.335591
3505.688875	352573.809827	41.340596
3505.848627	352500.375323	41.345600
3505.605132	352438.492792	41.350605
3505.394835	352359.955493	41.355610
3505.553679	352300.551993	41.360615
3505.598950	352238.802076	41.365620
3505.906230	352164.377919	41.370624
3505.501868	352099.621978	41.375629
3505.781248	352027.769194	41.380634
3505.432335	351962.063832	41.385639
3505.403896	351895.901756	41.390644
3505.066579	351826.203462	41.395648
3505.418410	351774.369386	41.400653
3505.196794	351698.399609	41.405658
3505.180817	351640.471014	41.410663
3505.475578	351580.612905	41.415668
3504.922992	351510.388195	41.420672
3505.141331	351450.668837	41.425677
3504.908946	351384.893328	41.430682
3504.925445	351323.095297	41.435687
3504.637188	351271.334602	41.440692
3504.912801	351213.995368	41.445696
3504.999554	351147.813836	41.450701
3504.939512	351090.755397	41.455706
3504.935043	351023.774366	41.460711
3504.876001	350969.079627	41.465716
3504.925263	350907.199446	41.470720
3504.501816	350849.205745	41.475725
3504.839185	350781.789718	41.480730
3504.958832	350734.464086	41.485735
3504.559243	350687.219184	41.490740
3504.530059	350626.037026	41.495744
3504.530930	350572.806683	41.500749
3504.219046	350512.456338	41.505754
3504.413855	350467.508150	41.510759
3504.281315	350420.195885	41.515764
3504.385916	350353.221923	41.520768
3504.267028	350310.889820	41.525773
3504.453655	350250.893568	41.530778
3504.444527	350213.297931	41.535783
3504.417800	350161.164304	41.540788
3504.594172	350092.882181	41.545792
3504.427745	350052.260336	41.550797
3504.327741	349989.613597	41.555802
3504.240706	349949.894424	41.560807
3504.169991	349890.623923	41.565812
3504.325400	349837.215809	41.570816
3504.081626	349788.115046	41.575821
3504.058348	349732.573776	41.580826
3503.918780	349691.464303	41.585831
3503.748801	349643.114473	41.590836
3504.209733	349598.199945	41.595840
3504.184649	349551.505234	41.600845
3503.892468	349504.979127	41.605850
3503.714653	349454.850749	41.610855
3503.948880	349408.725596	41.615860
3504.174919	349359.779876	41.620864
3503.759079	349316.247049	41.625869
3504.332220	349267.679343	41.630874
3503.980619	349220.450279	41.635879
3503.909974	349178.490530	41.640884
3504.045211	349125.287772	41.645888
3503.902365	349082.881548	41.650893
3503.616335	349042.378753	41.655898
3503.846889	349003.600461	41.660903
3503.780982	348953.911498	41.665908
3504.018844	348905.751338	41.670912
3503.674792	348859.130704	41.675917
3503.707887	348824.348728	41.680922
3503.900231	348779.093555	41.685927
3503.714309	348729.473774	41.690932
3503.785710	348675.670101	41.695936
3503.862926	348640.779378	41.700941
3503.864504	348600.968524	41.705946
3503.959154	348551.279394	41.710951
3503.678446	348507.114343	41.715956
3503.482073	348461.817537	41.720960
3503.562046	348424.028039	41.725965
3503.914480	348380.577802	41.730970
3503.802771	348336.106582	41.735975
3504.207775	348301.825472	41.740980
3504.224950	348243.911138	41.745984
3503.830182	348205.356332	41.750989
3504.049214	348156.460769	41.755994
3504.101782	348103.675993	41.760999
3503.882869	348054.594206	41.766004
3504.316241	347997.606152	41.771008
3503.835412	347953.166436	41.776013
3504.090003	347906.451306	41.781018
3503.824182	347859.562868	41.786023
3503.711509	347811.786164	41.791028
3503.699714	347774.289857	41.796032
3503.865611	347732.189780	41.801037
3503.888572	347681.900363	41.806042
3503.646711	347637.702690	41.811047
3503.715046	347591.778785	41.816052
3503.677721	347545.133999	41.821056
3503.845854	347511.651622	41.826061
3503.415904	347457.949421	41.831066
3503.472961	347415.382847	41.836071
3503.329346	347375.389738	41.841076
3503.599601	347335.738946	41.846080
3503.522932	347311.065382	41.851085
3503.549350	347256.478305	41.856090
3503.468116	347221.737869	41.861095
3503.303956	347181.823996	41.866100
3503.271929	347123.711990	41.871104
3503.459203	347099.937853	41.876109
3503.862379	347067.562498	41.881114
3503.786960	347019.448365	41.886119
3503.483058	346971.064638	41.891124
3503.386613	346930.097575	41.896128
3503.567009	346895.646592	41.901133
3503.780568	346848.097403	41.906138
3503.659779	346804.337410	41.911143
3503.372838	346763.043860	41.916148
3503.602401	346713.153038	41.921152
3503.490348	346685.077780	41.926157
3503.548189	346645.306687	41.931162
3503.341756	346607.915635	41.936167
3503.309986	346563.251652	41.941172
3503.331776	346525.774147	41.946176
3503.246837	346486.228473	41.951181
3503.351771	346445.636261	41.956186
3503.527588	346414.236334	41.961191
3503.176948	346376.435262	41.966196
3503.623454	346328.950787	41.971200
3503.264818	346301.905106	41.976205
3503.279973	346250.648660	41.981210
3503.095491	346219.965637	41.986215
3503.106726	346178.294461	41.991220
3502.998789	346141.116378	41.996224
3503.070065	346111.995161	42.001229
3503.272045	346074.514539	42.006234
3503.016753	346036.240618	42.011239
3503.047994	346005.167896	42.016244
3503.194607	345969.348331	42.021248
3503.229712	345930.546046	42.026253
3503.173855	345891.300239	42.031258
3503.074092	345859.586744	42.036263
3502.952162	345829.452962	42.041268
3503.213254	345784.564410	42.046272
3503.319585	345754.267921	42.051277
3503.283760	345717.713755	42.056282
3503.237026	345683.779940	42.061287
3503.302648	345652.879515	42.066292
3503.025546	345604.998144	42.071296
3503.443985	345570.890132	42.076301
3503.474257	345527.791435	42.081306
3503.268529	345489.865126	42.086311
3502.906284	345450.844458	42.091316
3503.241665	345410.952453	42.096320
3503.178587	345386.148245	42.101325
3503.122501	345347.359484	42.106330
3503.200038	345315.312798	42.111335
3503.169283	345286.944060	42.116340
3503.313914	345247.234094	42.121344
3502.579331	345221.669826	42.126349
3502.806000	345178.438427	42.131354
3502.781604	345146.076924	42.136359
3503.022555	345116.165712	42.141364
3503.153322	345075.389869	42.146368
3503.100005	345044.151454	42.151373
3503.126079	345008.578457	42.156378
3503.184859	344977.398812	42.161383
3502.805090	344936.778524	42.166388
3503.349223	344901.709569	42.171392
3503.156295	344873.086051	42.176397
3502.860252	344838.656269	42.181402
3503.306853	344797.958072	42.186407
3502.933686	344772.057552	42.191412
3503.133321	344727.050047	42.196416
3503.004720	344694.551782	42.201421
3503.067905	344664.159339	42.206426
3503.375964	344621.321369	42.211431
3503.020327	344590.027884	42.216436
3503.056772	344549.418643	42.221440
3502.837742	344515.408777	42.226445
3502.957472	344485.363327	42.231450
3503.177335	344457.488829	42.236455
3502.914009	344421.324629	42.241460
3503.060818	344380.748864	42.246464
3502.578136	344349.627480	42.251469
3502.680091	344319.355824	42.256474
3503.111863	344288.244636	42.261479
3502.745979	344258.249130	42.266484
3502.544980	344218.718882	42.271488
3502.716526	344188.004051	42.276493
3502.739430	344163.134725	42.281498
3503.115920	344132.642207	42.286503
3503.021127	344104.079051	42.291508
3503.086779	344073.990807	42.296512
3502.919704	344030.310723	42.301517
3502.791483	344007.524262	42.306522
3503.346814	343960.528068	42.311527
3503.008275	343927.324407	42.316532
3502.762899	343904.123874	42.321536
3502.850597	343868.336701	42.326541
3502.775366	343843.406139	42.331546
3502.927542	343803.439072	42.336551
3503.074795	343769.829131	42.341556
3502.972735	343732.240702	42.346560
3502.972841	343703.230210	42.351565
3502.885586	343670.063476	42.356570
3502.861986	343640.471830	42.361575
3502.636177	343602.571981	42.366580
3502.869122	343570.346928	42.371584
3502.970335	343540.684922	42.376589
3503.035402	343511.765865	42.381594
3503.075290	343479.977582	42.386599
3502.664420	343448.335691	42.391604
3502.780373	343406.644844	42.396608
3502.943620	343379.439358	42.401613
3502.660402	343348.158900	42.406618
3502.631711	343316.533695	42.411623
3502.637665	343295.022607	42.416628
3502.719422	343265.007430	42.421632
3502.537915	343227.507092	42.426637
3502.815568	343192.249033	42.431642
3502.836805	343156.751153	42.436647
3502.501214	343135.979620	42.441652
3502.716125	343105.791027	42.446656
3502.752035	343074.104696	42.451661
3502.914423	343041.635869	42.456666
3502.878638	343005.002531	42.461671
3502.528406	342987.335180	42.466676
3502.707958	342956.312896	42.471680
3502.820281	342920.139519	42.476685
3502.913881	342895.232854	42.481690
3502.954100	342860.163963	42.486695
3502.561266	342837.824728	42.491700
3503.250844	342805.044807	42.496704
3502.463934	342779.436009	42.501709
3502.480252	342745.921730	42.506714
3503.227349	342708.047492	42.511719
3502.745328	342686.078008	42.516724
3502.655410	342648.639072	42.521728
3503.018530	342618.706685	42.526733
3502.656403	342582.072831	42.531738
3503.176710	342545.784724	42.536743
3502.754436	342520.373258	42.541748
3502.804108	342478.615333	42.546752
3502.321215	342459.264777	42.551757
3502.465407	342432.646328	42.556762
3502.521532	342401.541051	42.561767
3502.551531	342379.059443	42.566772
3502.981756	342346.675424	42.571776
3502.797698	342312.530816	42.576781
3502.694168	342283.992947	42.581786
3503.027253	342258.285759	42.586791
3502.663411	342239.043689	42.591796
3502.685783	342190.805849	42.596800
3502.778405	342165.237719	42.601805
3502.642370	342142.374967	42.606810
3502.555332	342106.155489	42.611815
3502.378255	342077.247493	42.616820
3502.764415	342045.734566	42.621824
3502.674906	342018.821619	42.626829
3502.618126	341987.530128	42.631834
3502.898739	341959.440756	42.636839
3502.715703	341924.125970	42.641844
3502.766067	341893.199127	42.646848
3502.719574	341874.492293	42.651853
3502.745606	341840.746792	42.656858
3502.783633	341800.464637	42.661863
3502.851911	341772.103032	42.666868
3502.778613	341745.924739	42.671872
3502.691317	341711.967905	42.676877
3502.822448	341677.443078	42.681882
3502.696717	341646.187439	42.686887
3502.462230	341629.137068	42.691892
3502.762019	341599.340802	42.696896
3502.824084	341567.699890	42.701901
3502.475965	341543.191553	42.706906
3502.964490	341511.128246	42.711911
3502.831447	341483.153717	42.716916
3503.116300	341439.603475	42.721920
3502.854947	341404.732619	42.726925
3502.437651	341370.241978	42.731930
3502.481319	341350.961433	42.736935
3502.323417	341330.822286	42.741940
3502.393204	341298.569672	42.746944
3502.360027	341273.300171	42.751949
3502.383612	341251.429098	42.756954
3502.778216	341216.989957	42.761959
3502.220219	341193.403999	42.766964
3502.119851	341162.906809	42.771968
3502.369798	341149.900079	42.776973
3502.227924	341121.265522	42.781978
3502.507389	341086.742461	42.786983
3502.616213	341065.417416	42.791988
3502.678803	341033.597949	42.796993
3502.659481	341012.903075	42.801997
3502.312894	340980.969241	42.807002
3502.563922	340949.222085	42.812007
3502.174294	340928.330509	42.817012
3502.497441	340898.936861	42.822017
3502.412854	340876.141564	42.827021
3502.001321	340841.471515	42.832026
3502.172747	340831.935061	42.837031
3502.243044	340807.386530	42.842036
3502.564239	340777.535385	42.847041
3502.550880	340758.873658	42.852045
3502.681027	340730.679583	42.857050
3502.428158	340687.568080	42.862055
3502.424914	340674.854855	42.867060
3502.554058	340640.812453	42.872065
3502.236191	340611.645456	42.877069
3502.317887	340593.095991	42.882074
3502.449897	340562.918114	42.887079
3501.759525	340543.191940	42.892084
3502.402801	340511.383354	42.897089
3502.367732	340496.005078	42.902093
3502.245753	340473.825612	42.907098
3502.497841	340440.831864	42.912103
3502.326970	340416.091738	42.917108
3502.622310	340389.956787	42.922113
3502.254745	340366.823775	42.927117
3502.439090	340345.410260	42.932122
3502.434219	340319.372830	42.937127
3502.466356	340287.379436	42.942132
3502.357115	340264.155303	42.947137
3502.513117	340240.966164	42.952141
3502.532804	340211.186890	42.957146
3502.557679	340182.373056	42.962151
3502.283326	340169.142417	42.967156
3502.250220	340134.133078	42.972161
3502.433262	340105.726850	42.977165
3502.786143	340073.581638	42.982170
3502.530745	340049.490118	42.987175
3502.356682	340033.751847	42.992180
3502.565270	339998.755621	42.997185
3502.362093	339964.459145	43.002189
3502.503850	339938.347763	43.007194
3502.544109	339914.540712	43.012199
3502.262036	339894.064073	43.017204
3502.560512	339863.401988	43.022209
3502.476812	339837.961327	43.027213
3502.317432	339805.946446	43.032218
3502.461207	339772.307793	43.037223
3502.386179	339757.443987	43.042228
3502.601279	339732.109325	43.047233
3502.662159	339699.348074	43.052237
3502.174364	339681.954753	43.057242
3502.575112	339650.055998	43.062247
3502.255121	339632.992542	43.067252
3502.432582	339596.551335	43.072257
3502.494128	339574.673323	43.077261
3502.353846	339548.961546	43.082266
3502.495460	339519.645867	43.087271
3502.400611	339492.070684	43.092276
3502.581118	339473.098400	43.097281
3502.711785	339443.860649	43.102285
3502.183257	339411.953717	43.107290
3502.468005	339390.422291	43.112295
3502.144677	339373.054084	43.117300
3502.370639	339343.445418	43.122305
3502.161691	339318.074736	43.127309
3502.053601	339288.187432	43.132314
3502.417650	339262.498685	43.137319
3502.613963	339251.177916	43.142324
3502.191901	339217.499650	43.147329
3502.264065	339185.727901	43.152333
3501.978012	339175.829903	43.157338
3502.410126	339150.130484	43.162343
3502.483733	339125.071701	43.167348
3502.417240	339096.627217	43.172353
3502.356470	339087.279005	43.177357
3501.859625	339054.832815	43.182362
3502.086234	339029.165289	43.187367
3501.979086	339008.737209	43.192372
3501.943604	338989.823710	43.197377
3501.760173	338968.390315	43.202381
3501.758372	338948.428960	43.207386
3502.040988	338929.415071	43.212391
3502.246161	338924.806106	43.217396
3502.001795	338904.831615	43.222401
3502.132534	338874.576224	43.227405
3502.084775	338845.314893	43.232410
3502.342465	338830.780365	43.237415
3502.340615	338805.682243	43.242420
3502.167416	338779.491883	43.247425
3502.317697	338762.507407	43.252429
3502.079281	338730.631011	43.257434
3502.454582	338699.015095	43.262439
3502.468517	338682.484096	43.267444
3502.119906	338658.965590	43.272449
3502.292478	338627.940603	43.277453
3502.032037	338617.428163	43.282458
3502.458112	338584.609066	43.287463
3502.335815	338565.683425	43.292468
3502.089460	338540.089150	43.297473
3502.159407	338525.838008	43.302477
3502.219351	338493.202951	43.307482
3502.568112	338466.676845	43.312487
3502.161046	338448.380333	43.317492
3502.411715	338425.200719	43.322497
3502.739268	338407.934197	43.327501
3502.310196	338373.442488	43.332506
3502.746458	338356.896480	43.337511
3502.152054	338320.624952	43.342516
3502.229941	338288.749804	43.347521
3502.161245	338266.458962	43.352525
3502.046120	338247.150594	43.357530
3502.501178	338215.699852	43.362535
3502.314668	338194.317335	43.367540
3502.217874	338173.251430	43.372545
3502.173005	338153.042042	43.377549
3502.587983	338129.328077	43.382554
3502.492002	338095.292863	43.387559
3502.521842	338068.765236	43.392564
3502.450573	338036.785928	43.397569
3502.555660	338006.355795	43.402573
3502.204601	337983.371255	43.407578
3502.172630	337952.199511	43.412583
3502.122722	337941.196375	43.417588
3502.104358	337908.115239	43.422593
3502.081778	337879.103507	43.427597
3501.909278	337868.093996	43.432602
3501.721406	337843.329312	43.437607
3502.064306	337837.249275	43.442612
3501.904761	337810.801789	43.447617
3502.260408	337786.206788	43.452621
3502.068398	337771.462085	43.457626
3502.280378	337754.111517	43.462631
3502.293996	337735.596601	43.467636
3502.341305	337709.905181	43.472641
3502.449390	337681.330697	43.477645
3502.227153	337651.129212	43.482650
3502.311044	337627.313862	43.487655
3502.075536	337607.947597	43.492660
3502.253946	337585.312723	43.497665
3502.153335	337554.431050	43.502669
3502.133421	337533.174800	43.507674
3502.240750	337510.474651	43.512679
3501.979077	337488.467662	43.517684
3501.590159	337475.762461	43.522689
3502.338189	337458.684358	43.527693
3501.891014	337438.588036	43.532698
3501.963835	337421.208104	43.537703
3502.132520	337396.209621	43.542708
3502.174189	337363.474672	43.547713
3502.220164	337340.453372	43.552717
3502.062584	337328.398736	43.557722
3501.888971	337303.911199	43.562727
3501.917696	337280.485661	43.567732
3501.930156	337255.562253	43.572737
3502.125018	337249.759458	43.577741
3502.182039	337229.075955	43.582746
3502.177352	337200.925529	43.587751
3502.139380	337179.137845	43.592756
3502.172353	337161.179093	43.597761
3502.499151	337141.928521	43.602765
3502.094622	337116.815603	43.607770
3502.454370	337090.998837	43.612775
3502.145721	337064.345139	43.617780
3502.120359	337033.044428	43.622785
3502.318256	337020.298613	43.627789
3502.333741	337005.902769	43.632794
3502.298588	336966.262333	43.637799
3502.288840	336948.233832	43.642804
3502.131606	336916.292350	43.647809
3501.826222	336893.579749	43.652813
3501.582963	336874.010856	43.657818
3501.915362	336847.918439	43.662823
3501.739305	336838.791033	43.667828
3501.729036	336819.185854	43.672833
3501.898366	336803.367308	43.677837
3501.755240	336780.731111	43.682842
3502.497181	336765.357485	43.687847
3501.947273	336749.167656	43.692852
3502.013602	336726.447970	43.697857
3502.314086	336691.764846	43.702861
3501.988920	336681.567085	43.707866
3502.370509	336655.695753	43.712871
3502.235943	336633.388732	43.717876
3501.966386	336615.807390	43.722881
3502.284787	336584.554525	43.727885
3501.971950	336568.022555	43.732890
3502.198355	336545.379571	43.737895
3501.999954	336516.368686	43.742900
3502.188625	336503.751282	43.747905
3502.125807	336489.774313	43.752909
3501.589772	336476.379594	43.757914
3502.165765	336450.859329	43.762919
3501.775283	336429.939843	43.767924
3501.587097	336409.294036	43.772929
3502.111845	336374.575715	43.777933
3501.701244	336387.787585	43.782938
3501.502070	336355.089214	43.787943
3501.773272	336337.957639	43.792948
3501.645805	336332.866061	43.797953
3501.868667	336301.602394	43.802957
3501.927561	336292.005963	43.807962
3502.148972	336266.261008	43.812967
3502.028004	336256.896006	43.817972
3501.935433	336227.385236	43.822977
3501.908300	336212.715972	43.827981
3501.777688	336199.080045	43.832986
3501.987298	336171.632982	43.837991
3502.125434	336156.251340	43.842996
3502.306863	336137.175450	43.848001
3502.018532	336108.279962	43.853005
3501.650157	336092.010731	43.858010
3501.678451	336066.829741	43.863015
3501.938605	336052.598899	43.868020
3502.166041	336036.618395	43.873025
3501.781824	336016.257184	43.878029
3501.628452	336003.641973	43.883034
3502.159607	335986.647801	43.888039
3501.922415	335966.289114	43.893044
3502.068314	335942.361298	43.898049
3501.999419	335923.960032	43.903053
3502.202311	335906.457418	43.908058
3502.146666	335878.135891	43.913063
3502.077455	335863.854504	43.918068
3501.973021	335841.491453	43.923073
3501.842044	335806.772913	43.928077
3502.143567	335791.823458	43.933082
3501.967214	335782.416091	43.938087
3502.142824	335759.271903	43.943092
3501.670402	335737.322090	43.948097
3501.916752	335718.413902	43.953101
3501.492080	335704.798121	43.958106
3501.833855	335674.786987	43.963111
3501.891234	335673.455830	43.968116
3502.053755	335650.313611	43.973121
3502.101749	335631.105637	43.978125
3502.116932	335606.841905	43.983130
3502.082648	335580.297025	43.988135
3501.705822	335567.843595	43.993140
3501.582871	335548.484159	43.998145
3501.866612	335520.236702	44.003149
3501.852721	335516.602364	44.008154
3501.990665	335490.259503	44.013159
3501.939297	335476.941588	44.018164
3501.483850	335454.200589	44.023169
3501.750584	335433.788623	44.028173
3501.667054	335425.460277	44.033178
3501.928381	335401.030950	44.038183
3501.964239	335393.879303	44.043188
3501.955925	335383.453854	44.048193
3501.636551	335348.586182	44.053197
3501.851130	335344.356779	44.058202
3502.053895	335315.765725	44.063207
3501.971938	335303.418910	44.068212
3501.612862	335274.660938	44.073217
3501.639247	335258.533364	44.078221
3501.825553	335248.026729	44.083226
3501.900160	335236.672795	44.088231
3502.137312	335221.326220	44.093236
3501.958980	335202.789036	44.098241
3502.415130	335177.871476	44.103245
3502.110106	335157.929807	44.108250
3502.315423	335125.981222	44.113255
3501.911357	335117.397506	44.118260
3501.829239	335083.560799	44.123265
3501.963844	335073.494500	44.128269
3501.883935	335043.090704	44.133274
3502.017386	335027.480437	44.138279
3501.825819	335010.979763	44.143284
3501.746696	335000.819544	44.148289
3502.221843	334965.827875	44.153293
3501.717621	334949.019780	44.158298
3501.863272	334929.948839	44.163303
3501.774007	334921.748432	44.168308
3501.838075	334907.039028	44.173313
3501.933577	334873.962880	44.178317
3501.813461	334865.512942	44.183322
3501.561992	334840.552679	44.188327
3501.926845	334820.226838	44.193332
3501.586211	334799.959904	44.198337
3501.888314	334771.632727	44.203341
3501.935626	334777.347767	44.208346
3501.759365	334759.903616	44.213351
3501.886796	334732.773463	44.218356
3501.840356	334716.580691	44.223361
3501.759259	334704.258975	44.228365
3501.752272	334692.052884	44.233370
3501.638399	334662.391593	44.238375
3501.701623	334651.115548	44.243380
3501.624234	334635.741384	44.248385
3501.865060	334618.283127	44.253389
3502.035743	334606.736026	44.258394
3501.858971	334575.482232	44.263399
3501.959868	334569.134133	44.268404
3501.688110	334552.467710	44.273409
3502.226512	334523.594932	44.278413
3501.944139	334515.068435	44.283418
3501.969550	334499.144142	44.288423
3502.078074	334465.328073	44.293428
3502.016672	334460.734602	44.298433
3502.003946	334422.486726	44.303437
3501.887234	334420.317919	44.308442
3501.593965	334394.321141	44.313447
3501.717907	334384.637801	44.318452
3501.568613	334368.231993	44.323457
3502.031954	334344.635237	44.328461
3501.886491	334332.781197	44.333466
3501.524984	334296.672916	44.338471
3502.211428	334294.557146	44.343476
3501.950351	334284.450479	44.348481
3501.867276	334260.379189	44.353485
3501.907059	334235.780118	44.358490
3502.057747	334215.360114	44.363495
3501.875194	334202.647103	44.368500
3501.805893	334185.058878	44.373505
3501.810171	334155.556827	44.378509
3501.896586	334136.291240	44.383514
3502.102595	334109.936815	44.388519
3502.153631	334090.753008	44.393524
3501.962471	334076.057562	44.398529
3501.996746	334053.748150	44.403533
3501.860788	334043.825408	44.408538
3501.769779	334010.319737	44.413543
3501.928256	333995.264662	44.418548
3502.036426	333976.987477	44.423553
3502.361176	333959.210664	44.428557
3502.074348	333938.655133	44.433562
3501.969382	333914.739623	44.438567
3502.073467	333889.799696	44.443572
3501.617638	333887.022381	44.448577
3501.729404	333860.682447	44.453581
3501.464409	333849.686131	44.458586
3502.020876	333834.416463	44.463591
3501.898286	333815.208669	44.468596
3501.883080	333793.262860	44.473601
3502.100487	333770.288967	44.478605
3501.644976	333764.256211	44.483610
3501.528681	333735.077786	44.488615
3501.534718	333714.273097	44.493620
3501.616125	333711.132408	44.498625
3501.808760	333695.817571	44.503629
3501.423559	333678.303700	44.508634
3501.939260	333669.525657	44.513639
3501.623429	333648.516691	44.518644
3501.484981	333638.339902	44.523649
3502.109369	333617.235474	44.528653
3501.695523	333602.040408	44.533658
3502.069413	333585.451113	44.538663
3502.008559	333557.077772	44.543668
3502.138095	333552.785104	44.548673
3502.040646	333522.560836	44.553677
3501.908310	333501.904727	44.558682
3502.020943	333479.938843	44.563687
3501.898433	333464.062564	44.568692
3502.036155	333442.525113	44.573697
3502.058592	333415.969873	44.578701
3501.686940	333403.642079	44.583706
3501.841641	333390.901747	44.588711
3501.730760	333361.366129	44.593716
3501.865680	333347.179181	44.598721
3501.835165	333325.311782	44.603725
3501.822848	333315.038979	44.608730
3501.866536	333293.973871	44.613735
3501.790835	333263.008454	44.618740
3501.398460	333265.078924	44.623745
3501.901790	333245.264779	44.628749
3501.721137	333229.626346	44.633754
3502.026948	333218.312124	44.638759
3502.072827	333193.736858	44.643764
3501.887607	333178.506044	44.648769
3502.044706	333142.646585	44.653773
3501.862363	333136.494920	44.658778
3502.192965	333099.158734	44.663783
3502.116125	333091.413791	44.668788
3501.956318	333071.601015	44.673793
3502.193455	333050.175037	44.678797
3502.193943	333030.871393	44.683802
3501.867929	332999.690381	44.688807
3501.846907	332977.160041	44.693812
3501.593405	332970.230993	44.698817
3502.025859	332949.944493	44.703821
3501.879392	332940.099396	44.708826
3502.005829	332908.847902	44.713831
3501.878807	332894.142016	44.718836
3501.797308	332874.774751	44.723841
3501.906280	332854.894603	44.728845
3501.956190	332833.599371	44.733850
3502.013712	332812.786176	44.738855
3501.887306	332803.828088	44.743860
3501.987355	332791.324959	44.748865
3501.753544	332763.334005	44.753869
3501.527128	332741.496754	44.758874
3502.083075	332730.753864	44.763879
3501.992172	332709.251575	44.768884
3501.618847	332698.526115	44.773889
3501.734995	332676.508352	44.778893
3501.829606	332659.173678	44.783898
3501.796833	332640.078479	44.788903
3501.724881	332623.430977	44.793908
3502.090396	332616.609005	44.798913
3502.127896	332580.869362	44.803917
3501.641553	332575.426183	44.808922
3501.677596	332549.580358	44.813927
3501.960673	332527.892603	44.818932
3501.709156	332523.099579	44.823937
3501.765063	332494.173171	44.828941
3502.064239	332485.657452	44.833946
3501.992353	332461.023738	44.838951
3502.094763	332454.268114	44.843956
3501.869547	332428.284827	44.848961
3502.094783	332411.463819	44.853965
3501.810428	332386.837687	44.858970
3501.755194	332372.527365	44.863975
3501.721946	332344.784663	44.868980
3501.658869	332335.689442	44.873985
3501.783954	332317.612296	44.878989
3501.959751	332301.943447	44.883994
3501.787492	332292.203930	44.888999
3502.373336	332260.931284	44.894004
3501.970266	332247.743258	44.899009
3502.007214	332226.195368	44.904013
3501.744870	332213.392371	44.909018
3501.798147	332181.871896	44.914023
3501.755291	332166.364186	44.919028
3501.440538	332144.947280	44.924033
3501.885215	332129.007616	44.929037
3501.326933	332123.473830	44.934042
3501.784834	332106.387579	44.939047
3501.714518	332076.870086	44.944052
3501.542566	332072.624167	44.949057
3501.807688	332044.961987	44.954061
3501.849876	332033.001725	44.959066
3501.446077	332016.914275	44.964071
3501.450968	331992.293746	44.969076
3501.391762	331985.054511	44.974081
3501.832373	331978.119005	44.979085
3501.748460	331967.068530	44.984090
3501.477240	331946.712962	44.989095
3501.757195	331933.011598	44.994100
3501.124932	331927.107788	44.999105
3501.733392	331911.676658	45.004109
3501.806970	331897.142643	45.009114
3501.981688	331881.015980	45.014119
3502.036313	331858.142567	45.019124
3501.680763	331838.919158	45.024129
3501.855364	331825.641094	45.029133
3501.911779	331809.659980	45.034138
3501.586779	331789.541603	45.039143
3501.852686	331768.161298	45.044148
3501.314828	331758.427669	45.049153
3501.611992	331747.826511	45.054157
3501.779686	331733.532129	45.059162
3501.704180	331714.392249	45.064167
3501.740055	331688.011755	45.069172
3501.498343	331666.227138	45.074177
3501.520647	331655.643292	45.079181
3502.048073	331652.204122	45.084186
3501.988102	331620.319299	45.089191
3501.910783	331611.785672	45.094196
3501.634257	331598.552296	45.099201
3501.650679	331575.303148	45.104205
3501.815645	331568.206990	45.109210
3502.000938	331546.635634	45.114215
3501.957353	331520.369126	45.119220
3501.674847	331504.262586	45.124225
3501.455563	331498.701391	45.129229
3501.557362	331473.098951	45.134234
3501.518270	331461.405501	45.139239
3501.692818	331444.744563	45.144244
3501.441483	331431.736117	45.149249
3501.456458	331414.871090	45.154253
3501.753919	331413.273516	45.159258
3501.938941	331391.371470	45.164263
3502.054485	331366.199202	45.169268
3501.469857	331348.791594	45.174273
3501.493244	331330.806112	45.179277
3501.867841	331331.994304	45.184282
3501.361887	331308.190426	45.189287
3501.678586	331289.930373	45.194292
3501.708837	331280.031915	45.199297
3501.799439	331267.224548	45.204301
3501.371407	331258.592812	45.209306
3501.786507	331254.687834	45.214311
3501.900927	331222.165119	45.219316
3501.792918	331217.425903	45.224321
3501.616390	331194.410025	45.229325
3501.649634	331168.055019	45.234330
3501.641416	331173.143382	45.239335
3501.619720	331145.855837	45.244340
3501.540644	331137.347813	45.249345
3501.562262	331116.793630	45.254349
3501.792975	331099.487942	45.259354
3501.746880	331091.330859	45.264359
3501.766561	331062.434445	45.269364
3501.454536	331045.162321	45.274369
3501.475363	331031.424657	45.279373
3501.747117	331017.546204	45.284378
3501.511380	331011.733154	45.289383
3501.819168	331000.824924	45.294388
3501.433259	330984.734258	45.299393
3501.830583	330960.535259	45.304397
3501.946423	330949.606015	45.309402
3501.608513	330937.857168	45.314407
3501.875744	330919.935288	45.319412
3501.717939	330899.612387	45.324417
3501.645921	330888.330840	45.329421
3501.938574	330867.556306	45.334426
3501.743055	330850.240531	45.339431
3501.928375	330832.102445	45.344436
3501.855905	330808.637757	45.349441
3501.703309	330790.984626	45.354445
3501.742723	330769.740753	45.359450
3501.567008	330759.060303	45.364455
3501.496881	330745.743647	45.369460
3501.756089	330727.288798	45.374465
3501.488197	330713.367038	45.379469
3501.621506	330700.654577	45.384474
3501.892827	330678.916743	45.389479
3501.622572	330661.866860	45.394484
3501.562754	330649.743999	45.399489
3501.579540	330627.511615	45.404493
3501.721558	330625.302329	45.409498
3501.498208	330620.021423	45.414503
3501.421714	330595.005711	45.419508
3501.628098	330592.328581	45.424513
3501.371844	330575.200177	45.429517
3501.397710	330554.873948	45.434522
3501.569635	330539.968031	45.439527
3501.806601	330529.350474	45.444532
3501.451454	330522.411365	45.449537
3501.361819	330502.738953	45.454541
3501.428431	330491.664632	45.459546
3501.333319	330472.476319	45.464551
3501.775610	330463.047666	45.469556
3501.485472	330456.098428	45.474561
3501.103132	330437.234578	45.479565
3501.418415	330429.656992	45.484570
3501.762262	330421.668002	45.489575
3501.736780	330411.549080	45.494580
3501.523701	330398.814118	45.499585
3501.424379	330376.701398	45.504589
3501.290378	330373.339609	45.509594
3501.429021	330348.213956	45.514599
3501.257310	330346.104344	45.519604
3501.675654	330341.817247	45.524609
3501.563530	330320.876495	45.529613
3501.602979	330316.139656	45.534618
3501.590448	330303.678675	45.539623
3501.936135	330271.068305	45.544628
3501.586210	330266.773577	45.549633
3501.494370	330250.636845	45.554637
3501.353951	330226.953465	45.559642
3501.467998	330216.990826	45.564647
3501.768369	330203.463719	45.569652
3501.669158	330188.981387	45.574657
3501.814968	330173.952219	45.579661
3502.200625	330154.765241	45.584666
3501.840329	330132.820169	45.589671
3501.654585	330109.042030	45.594676
3501.688070	330104.891101	45.599681
3501.389601	330085.810548	45.604685
3501.678658	330073.099081	45.609690
3501.380276	330059.080090	45.614695
3501.815025	330044.667224	45.619700
3501.833637	330031.870653	45.624705
3501.693511	330016.326346	45.629709
3501.718191	329997.500686	45.634714
3501.644726	329975.154798	45.639719
3501.834226	329959.126777	45.644724
3501.538530	329943.225122	45.649729
3501.712749	329933.329353	45.654733
3501.680218	329925.093608	45.659738
3501.591254	329900.588096	45.664743
3501.572114	329888.255186	45.669748
3501.788925	329878.683433	45.674753
3501.659706	329857.032906	45.679757
3501.685861	329846.600580	45.684762
3501.563370	329840.286461	45.689767
3501.846926	329811.526104	45.694772
3501.752906	329804.113832	45.699777
3501.432158	329770.258680	45.704781
3501.562587	329756.325464	45.709786
3501.262763	329758.279974	45.714791
3501.538475	329748.699024	45.719796
3501.634761	329735.864833	45.724801
3501.877608	329711.739969	45.729805
3501.305721	329693.286785	45.734810
3501.216350	329680.939304	45.739815
3501.895126	329661.859084	45.744820
3501.888215	329640.774418	45.749825
3501.548660	329576.475835	45.754829
3501.210060	329470.132115	45.759834
3501.272563	329332.032939	45.764839
3500.930172	329132.060325	45.769844
3500.166062	328898.627839	45.774849
3499.769981	328620.191207	45.779853
3499.317026	328303.683397	45.784858
3497.710761	327943.220239	45.789863
3496.998902	327537.260933	45.794868
3495.917311	327112.557089	45.799873
3494.638346	326635.020745	45.804877
3493.588682	326138.644663	45.809882
3491.901195	325595.225222	45.814887
3490.598256	325022.611824	45.819892
3488.966635	324425.976581	45.824897
3487.526748	323799.259334	45.829901
3485.860925	323135.858627	45.834906
3483.788090	322436.742237	45.839911
3482.275642	321715.317630	45.844916
3480.297178	320969.759101	45.849921
3477.904748	320189.346619	45.854925
3476.107390	319392.264864	45.859930
3473.862577	318570.610102	45.864935
3471.799757	317707.821710	45.869940
3469.293585	316845.441721	45.874945
3467.064779	315957.939921	45.879949
3464.499912	315041.237607	45.884954
3461.687400	314114.810096	45.889959
3459.232255	313155.916585	45.894964
3456.521428	312199.893076	45.899969
3453.915962	311213.807177	45.904973
3451.560940	310207.558937	45.909978
3448.663236	309194.630627	45.914983
3445.899338	308151.453857	45.919988
3442.818867	307109.118709	45.924993
3439.567438	306057.296026	45.929997
3436.740800	304981.157541	45.935002
3433.746947	303908.102032	45.940007
3430.905411	302802.653109	45.945012
3427.618247	301704.147689	45.950017
3424.656540	300574.110970	45.955021
3421.437214	299459.667619	45.960026
3418.349344	298324.895615	45.965031
3414.948378	297185.873292	45.970036
3411.561299	296034.913775	45.975041
3408.630610	294871.336963	45.980045
3405.396085	293704.195386	45.985050
3402.035681	292529.057787	45.990055
3398.843304	291342.416396	45.995060
3395.121057	290172.661324	46.000065
3391.580143	288984.858613	46.005069
3388.502475	287780.236657	46.010074
3384.677253	286590.168848	46.015079
3381.406866	285387.570088	46.020084
3377.882822	284183.182117	46.025089
3374.545790	282983.352325	46.030093
3371.079486	281763.180495	46.035098
3367.340733	280558.790182	46.040103
3364.058618	279335.876208	46.045108
3360.179428	278121.462941	46.050113
3356.742166	276902.226248	46.055117
3353.233094	275680.283202	46.060122
3349.979695	274462.406892	46.065127
3346.022693	273229.905314	46.070132
3342.297245	271999.157860	46.075137
3338.835168	270771.891578	46.080141
3335.182543	269555.358293	46.085146
3331.319406	268327.612516	46.090151
3327.520335	267090.470389	46.095156
3324.021087	265878.017158	46.100161
3320.829045	264638.840496	46.105165
3317.159245	263408.636176	46.110170
3313.047290	262191.219161	46.115175
3309.760451	260955.529289	46.120180
3306.451556	259733.581031	46.125185
3302.499905	258493.308645	46.130189
3298.605701	257267.326853	46.135194
3294.933589	256041.859148	46.140199
3291.132224	254816.196678	46.145204
3287.502386	253587.568150	46.150209
3283.963207	252352.090098	46.155213
3280.036703	251134.922250	46.160218
3276.343515	249923.668212	46.165223
3272.638786	248699.928239	46.170228
3268.794662	247485.853751	46.175233
3265.386670	246272.034622	46.180237
3261.619605	245065.394971	46.185242
3257.502201	243848.513851	46.190247
3254.204193	242633.918126	46.195252
3250.488818	241426.359556	46.200257
3246.751040	240215.844528	46.205261
3242.850977	239004.178001	46.210266
3238.869104	237804.693428	46.215271
3235.317930	236601.393675	46.220276
3231.831152	235407.121458	46.225281
3227.907489	234214.594788	46.230285
3224.143219	233017.124856	46.235290
3220.379330	231827.776897	46.240295
3216.418095	230634.255148	46.245300
3212.868026	229452.357982	46.250305
3209.116806	228270.414432	46.255309
3205.545084	227083.348262	46.260314
3201.482855	225915.663504	46.265319
3197.946313	224732.615432	46.270324
3194.153540	223562.138345	46.275329
3190.418747	222390.863415	46.280333
3186.582691	221213.212636	46.285338
3183.099385	220059.347448	46.290343
3179.324908	218898.245298	46.295348
3175.164985	217723.375778	46.300353
3171.691470	216560.856390	46.305357
3168.093094	215417.384606	46.310362
3163.970746	214265.465650	46.315367
3160.431917	213108.620578	46.320372
3156.873182	211975.188265	46.325377
3152.682477	210830.754400	46.330381
3148.660843	209680.212078	46.335386
3144.809188	208544.369089	46.340391
3141.189736	207400.651233	46.345396
3137.628971	206283.416716	46.350401
3133.784630	205161.316984	46.355405
3130.218087	204035.920501	46.360410
3125.919630	202934.125625	46.365415
3122.638115	201825.073890	46.370420
3119.048089	200702.707113	46.375425
3115.459999	199587.071018	46.380429
3111.706303	198489.320851	46.385434
3107.766759	197381.166339	46.390439
3103.763210	196269.719674	46.395444
3100.045083	195178.839623	46.400449
3096.223429	194085.336117	46.405453
3092.477434	192992.186613	46.410458
3088.876572	191912.800937	46.415463
3085.462220	190827.971770	46.420468
3081.523939	189751.586717	46.425473
3077.497795	188672.628127	46.430477
3073.675679	187596.729553	46.435482
3069.849350	186538.132688	46.440487
3066.271343	185476.681420	46.445492
3062.248734	184420.963392	46.450497
3058.509195	183363.404674	46.455501
3054.790311	182307.356667	46.460506
3051.042216	181272.459277	46.465511
3047.260483	180231.009418	46.470516
3043.604713	179190.239519	46.475521
3039.689093	178161.846016	46.480525
3035.958904	177126.612232	46.485530
3032.115058	176101.249717	46.490535
3028.025627	175077.185786	46.495540
3024.400924	174069.102820	46.500545
3020.303331	173058.241997	46.505549
3016.746348	172049.079703	46.510554
3012.881829	171051.117296	46.515559
3009.035387	170065.042231	46.520564
3005.050431	169075.055818	46.525569
3000.985217	168099.556049	46.530573
2997.392893	167111.394227	46.535578
2993.305735	166153.160219	46.540583
2989.359696	165177.428239	46.545588
2985.426891	164240.670703	46.550593
2981.787415	163286.544566	46.555597
2977.923058	162343.757332	46.560602
2973.814164	161412.489966	46.565607
2969.755968	160487.045030	46.570612
2966.110105	159564.616998	46.575617
2962.153402	158653.196806	46.580621
2958.364630	157726.287693	46.585626
2954.272172	156849.190553	46.590631
2950.567504	155941.475906	46.595636
2946.541088	155061.417027	46.600641
2942.389509	154187.385250	46.605645
2938.925974	153304.249530	46.610650
2935.007170	152443.520200	46.615655
2930.965460	151575.607678	46.620660
2926.792054	150728.548707	46.625665
2922.438809	149904.691469	46.630669
2918.783951	149065.709490	46.635674
2914.714257	148245.791268	46.640679
2910.636260	147437.441399	46.645684
2906.720106	146636.141148	46.650689
2902.509746	145844.964288	46.655693
2898.801469	145055.350281	46.660698
2894.478263	144288.429761	46.665703
2890.249400	143524.381936	46.670708
2886.561356	142776.560927	46.675713
2882.033537	142030.650565	46.680717
2877.911931	141311.840216	46.685722
2873.699536	140593.016528	46.690727
2869.465713	139885.059733	46.695732
2865.487248	139193.613485	46.700737
2860.977352	138517.234690	46.705741
2857.517595	137844.506295	46.710746
2853.444004	137102.928271	46.715751
2849.737396	136449.367510	46.720756
2845.970844	135796.703249	46.725761
2841.709574	135170.981003	46.730765
2837.752735	134538.337711	46.735770
2833.516833	133919.638576	46.740775
2829.814233	133304.935871	46.745780
2825.920294	132705.244190	46.750785
2822.059508	132110.707521	46.755789
2818.486980	131535.418711	46.760794
2814.452743	130959.420733	46.765799
2810.912718	130380.275238	46.770804
2807.058859	129808.144383	46.775809
2803.226062	129247.949347	46.780813
2799.760351	128675.353639	46.785818
2795.903302	128137.004448	46.790823
2792.285881	127578.591660	46.795828
2788.794911	127029.095696	46.800833
2784.952371	126494.339705	46.805837
2781.599699	125946.706398	46.810842
2778.078091	125399.768110	46.815847
2774.333966	124868.553954	46.820852
2770.494779	124337.234399	46.825857
2767.066434	123801.508268	46.830861
2763.554794	123273.420472	46.835866
2759.808476	122743.684722	46.840871
2756.040255	122222.264229	46.845876
2752.550118	121696.775874	46.850881
2748.828620	121174.331913	46.855885
2745.904141	120655.560695	46.860890
2742.096612	120144.640442	46.865895
2738.402302	119618.639714	46.870900
2735.333731	119107.643680	46.875905
2731.465592	118589.733896	46.880909
2728.136282	118075.498681	46.885914
2724.301850	117556.516877	46.890919
2721.183521	117041.207483	46.895924
2717.810309	116521.278094	46.900929
2714.184685	116013.538802	46.905933
2710.952995	115491.516407	46.910938
2707.005220	114983.523498	46.915943
2703.275910	114457.625994	46.920948
2700.316546	113950.955834	46.925953
2696.604566	113439.323898	46.930957
2693.019956	112915.536832	46.935962
2689.254569	112413.679901	46.940967
2686.011203	111901.958712	46.945972
2682.621154	111388.284269	46.950977
2678.460804	110884.323454	46.955981
2674.880687	110369.612648	46.960986
2671.429401	109877.150833	46.965991
2667.942932	109359.605098	46.970996
2664.266662	108868.171418	46.976001
2660.221062	108365.741792	46.981005
2656.753095	107872.420974	46.986010
2653.056706	107383.426937	46.991015
2649.127004	106886.848661	46.996020
2645.260207	106407.098935	47.001025
2641.517086	105935.561486	47.006029
2637.907490	105471.637002	47.011034
2634.180241	104995.571997	47.016039
2630.075413	104525.991856	47.021044
2626.509638	104072.147454	47.026049
2622.939540	103627.080678	47.031053
2619.481659	103163.583988	47.036058
2615.358405	102721.920315	47.041063
2611.520453	102277.904791	47.046068
2607.854889	101841.049921	47.051073
2603.958358	101416.337147	47.056077
2600.304619	100989.990617	47.061082
2596.674536	100554.685367	47.066087
2593.216516	100132.361440	47.071092
2589.629073	99716.265538	47.076097
2585.688829	99300.674747	47.081101
2582.271940	98880.724808	47.086106
2578.790690	98468.898911	47.091111
2574.927992	98054.977142	47.096116
2571.544676	97644.684461	47.101121
2568.145280	97239.749992	47.106125
2564.933642	96842.391249	47.111130
2561.202587	96432.333637	47.116135
2557.589427	96028.909472	47.121140
2554.289022	95609.709170	47.126145
2550.616132	95200.090728	47.131149
2547.319577	94789.059380	47.136154
2543.485424	94387.025190	47.141159
2540.145484	93983.991674	47.146164
2536.888767	93590.023489	47.151169
2533.003473	93189.093011	47.156173
2529.790170	92772.789436	47.161178
2526.295572	92371.313309	47.166183
2522.810497	91962.204316	47.171188
2519.601597	91553.934605	47.176193
2515.967633	91153.728804	47.181197
2512.531130	90739.876634	47.186202
2508.871918	90327.055882	47.191207
2505.878651	89921.201584	47.196212
2502.416402	89507.980306	47.201217
2498.966425	89097.253111	47.206221
2495.788551	88667.660097	47.211226
2492.371894	88253.902848	47.216231
2488.785838	87824.881100	47.221236
2485.456255	87410.842630	47.226241
2481.677344	86999.725739	47.231245
2477.953516	86567.999642	47.236250
2474.711267	86146.330189	47.241255
2470.872094	85731.162541	47.246260
2467.607421	85306.840943	47.251265
2464.082365	84891.280758	47.256269
2461.023410	84465.440498	47.261274
2457.740693	84048.902016	47.266279
2453.973579	83627.427281	47.271284
2450.514738	83194.503647	47.276289
2447.078109	82761.545035	47.281293
2443.255145	82331.981195	47.286298
2439.948910	81904.070972	47.291303
2436.076726	81470.386964	47.296308
2433.087676	81047.533921	47.301313
2429.531036	80625.245550	47.306317
2426.108372	80193.314984	47.311322
2422.538108	79770.762231	47.316327
2418.589373	79330.772701	47.321332
2415.760258	78904.040761	47.326337
2412.009594	78472.569060	47.331341
2408.678219	78039.616415	47.336346
2404.531637	77614.519245	47.341351
2401.718984	77176.978191	47.346356
2398.083159	76737.210076	47.351361
2394.430928	76312.170562	47.356365
2390.747805	75866.188360	47.361370
2387.527093	75436.079141	47.366375
2384.048190	75009.242528	47.371380
2380.884642	74570.883828	47.376385
2376.816481	74135.898536	47.381389
2373.221716	73683.932307	47.386394
2369.866356	73264.736049	47.391399
2366.513618	72827.400484	47.396404
2362.974247	72384.323665	47.401409
2359.422599	71948.582712	47.406413
2356.146833	71517.732627	47.411418
2352.586876	71084.115054	47.416423
2349.090069	70646.215942	47.421428
2345.630334	70205.436232	47.426433
2341.849128	69776.636085	47.431437
2338.782489	69330.204492	47.436442
2335.280814	68891.707201	47.441447
2332.036985	68448.993921	47.446452
2328.068837	67996.041283	47.451457
2324.617648	67560.186814	47.456461
2321.348918	67113.863167	47.461466
2317.589543	66679.226943	47.466471
2313.954452	66223.416531	47.471476
2310.737534	65782.255906	47.476481
2307.326156	65350.673052	47.481485
2303.935887	64896.073438	47.486490
2300.336969	64455.604758	47.491495
2296.996794	64015.116231	47.496500
2293.491612	63565.661455	47.501505
2290.047534	63115.107293	47.506509
2286.830776	62661.435156	47.511514
2283.059812	62208.847594	47.516519
2279.289330	61760.647162	47.521524
2276.210400	61300.949537	47.526529
2272.610416	60856.292859	47.531533
2269.201896	60395.654430	47.536538
2265.725030	59955.633798	47.541543
2262.208835	59493.810718	47.546548
2258.701793	59035.491383	47.551553
2254.918013	58587.109983	47.556557
2251.515792	58122.750714	47.561562
2247.997718	57669.985727	47.566567
2244.651104	57216.917039	47.571572
2241.166961	56744.665723	47.576577
2237.170207	56301.994355	47.581581
2233.926084	55847.641269	47.586586
2230.392637	55393.766964	47.591591
2226.672556	54938.325222	47.596596
2223.486220	54486.235129	47.601601
2220.056877	54027.409505	47.606605
2216.862973	53562.072482	47.611610
2212.923486	53110.785779	47.616615
2209.553763	52651.438502	47.621620
2206.019382	52186.042223	47.626625
2201.981470	51740.043591	47.631629
2198.714895	51283.270047	47.636634
2195.525194	50829.329027	47.641639
2191.986118	50367.782298	47.646644
2188.977251	49916.463524	47.651649
2185.130728	49441.199602	47.656653
2181.870246	48974.131761	47.661658
2178.228285	48513.881497	47.666663
2174.716404	48057.971304	47.671668
2171.232340	47591.194899	47.676673
2167.475374	47138.620356	47.681677
2164.212011	46672.297860	47.686682
2160.754004	46201.899268	47.691687
2156.792145	45743.093235	47.696692
2153.557507	45271.258747	47.701697
2150.091216	44817.823124	47.706701
2146.446210	44346.262261	47.711706
2143.480596	43892.241176	47.716711
2139.352584	43422.861384	47.721716
2136.203311	42962.020275	47.726721
2132.711806	42487.298088	47.731725
2129.081053	42025.169116	47.736730
2125.656444	41563.797687	47.741735
2121.943128	41099.830505	47.746740
2118.640969	40637.743026	47.751745
2115.082185	40173.460776	47.756749
2111.843143	39704.522976	47.761754
2107.779312	39232.502896	47.766759
2104.272949	38760.400006	47.771764
2101.161224	38293.235450	47.776769
2097.399363	37835.488854	47.781773
2094.182520	37363.491959	47.786778
2090.455661	36903.166923	47.791783
2087.042870	36438.638016	47.796788
2083.832968	35968.712063	47.801793
2080.264587	35495.061560	47.806797
2076.611124	35024.078168	47.811802
2072.833695	34555.571288	47.816807
2069.306230	34089.305107	47.821812
2066.022312	33617.294081	47.826817
2062.302003	33160.148794	47.831821
2059.125810	32673.906425	47.836826
2055.411938	32217.154678	47.841831
2052.054663	31742.928317	47.846836
2048.818359	31267.686239	47.851841
2044.851999	30801.808840	47.856845
2041.709974	30326.218767	47.861850
2038.044743	29854.732570	47.866855
2034.363982	29389.761484	47.871860
2031.008828	28912.057246	47.876865
2027.485106	28460.244711	47.881869
2023.917580	27983.146501	47.886874
2020.775701	27518.805722	47.891879
2017.050592	27044.915946	47.896884
2013.322726	26577.988544	47.901889
2009.684000	26117.394155	47.906893
2006.196963	25636.752306	47.911898
2002.642578	25162.335167	47.916903
1999.236532	24704.429576	47.921908
1995.738859	24230.298060	47.926913
1992.019099	23767.926458	47.931917
1988.788108	23289.359992	47.936922
1985.280961	22825.044916	47.941927
1981.543050	22363.025507	47.946932
1978.481426	21897.212096	47.951937
1974.789147	21431.222746	47.956941
1971.349478	20957.166624	47.961946
1967.410793	20492.473045	47.966951
1963.745975	20028.279913	47.971956
1960.612336	19559.897985	47.976961
1956.976167	19106.642131	47.981965
1953.603344	18635.051324	47.986970
1949.768007	18167.863431	47.991975
1946.249908	17705.716819	47.996980
1943.119303	17234.895000	48.001985
1939.384041	16777.497318	48.006989
1935.249985	16302.772706	48.011994
1932.167198	15850.526528	48.016999
1928.687118	15395.683613	48.022004
1925.030360	14925.554300	48.027009
1921.515135	14466.388512	48.032013
1917.931896	14013.975512	48.037018
1914.412695	13556.538813	48.042023
1910.542647	13111.049575	48.047028
1907.472377	12647.147551	48.052033
1903.855997	12198.369974	48.057037
1900.386797	11741.871622	48.062042
1896.806240	11284.474141	48.067047
1893.190583	10839.860030	48.072052
1889.785984	10382.653423	48.077057
1886.262015	9934.523353	48.082061
1882.337452	9478.496054	48.087066
1878.777914	9041.205828	48.092071
1874.886089	8593.146315	48.097076
1871.688619	8147.711571	48.102081
1867.295307	7712.462546	48.107085
1863.474836	7276.644066	48.112090
1860.000087	6847.463187	48.117095
1855.872039	6428.268253	48.122100
1852.434843	5996.088518	48.127105
1848.065632	5599.628685	48.132109
1844.116900	5205.653203	48.137114
1839.283101	4837.554910	48.142119
1834.022856	4491.067934	48.147124
1829.001766	4167.527279	48.152129
1823.830266	3866.463907	48.157133
1818.912761	3577.232247	48.162138
1814.732667	3308.888612	48.167143
1810.137951	3052.817959	48.172148
1806.322285	2814.292226	48.177153
1802.112886	2568.755890	48.182157
1798.610158	2367.340892	48.187162
1794.945277	2152.101049	48.192167
1791.016023	1936.746735	48.197172
1787.472059	1736.016023	48.202177
1784.303573	1546.132168	48.207181
1780.815050	1356.730435	48.212186
1777.501491	1156.612647	48.217191
1773.434047	981.317934	48.222196
1769.915827	798.494949	48.227201
1766.455884	616.879673	48.232205
1762.460565	447.425711	48.237210
1758.818217	281.009412	48.242215
1754.677234	133.331901	48.247220
1749.798027	7.929057	48.252225
1739.754597	44.593703	48.257229
1732.538864	49.516578	48.262234
1728.261631	48.708206	48.267239
1725.143197	56.796153	48.272244
1723.046430	48.716730	48.277249
1720.401538	45.572582	48.282253
1717.814638	45.848865	48.287258
1715.141346	45.157846	48.292263
1711.575725	50.401618	48.297268
1708.702347	35.400669	48.302273
1705.317340	54.925767	48.307277
1701.840615	47.440771	48.312282
1698.442039	44.173488	48.317287
1694.853875	58.326602	48.322292
1691.241143	49.540346	48.327297
1687.685803	56.655434	48.332301
1684.487865	49.443420	48.337306
1681.762880	44.916548	48.342311
1678.216314	50.802752	48.347316
1674.932663	51.035623	48.352321
1671.458102	55.369898	48.357325
1667.848682	59.361337	48.362330
1664.679754	43.586989	48.367335
1661.089103	49.179503	48.372340
1658.166198	49.906713	48.377345
1654.023477	44.214802	48.382349
1650.904644	46.677744	48.387354
1647.423130	48.431518	48.392359
1643.420014	49.231946	48.397364
1640.493311	44.654218	48.402369
1637.100234	43.202052	48.407373
1633.113658	42.440201	48.412378
1630.447130	29.966513	48.417383
1626.885956	54.720146	48.422388
1622.970479	41.808101	48.427393
1619.501121	52.168421	48.432397
1616.092613	52.446040	48.437402
1612.838346	54.218231	48.442407
1609.333715	53.783160	48.447412
1605.988273	50.994827	48.452417
1602.244483	51.156956	48.457421
1599.151470	58.418385	48.462426
1596.024016	54.276860	48.467431
1592.128925	48.862785	48.472436
1588.068728	48.855867	48.477441
1584.539800	54.210993	48.482445
1581.406756	54.777930	48.487450
1578.394008	46.018531	48.492455
1574.892935	55.621337	48.497460
1571.526501	51.858691	48.502465
1567.724353	44.247201	48.507469
1564.507185	48.089009	48.512474
1560.906221	50.123969	48.517479
1557.021868	53.073056	48.522484
1553.740467	53.938328	48.527489
1550.065258	47.575727	48.532493
1546.769658	48.547612	48.537498
1543.643235	45.225333	48.542503
1540.110816	44.819904	48.547508
1536.197008	46.115798	48.552513
1532.848767	41.787189	48.557517
1529.362255	52.321019	48.562522
1525.978025	41.569373	48.567527
1522.161101	49.206061	48.572532
1519.305052	38.071657	48.577537
1515.586323	50.429120	48.582541
1511.754855	51.253463	48.587546
1508.617010	50.669566	48.592551
1505.139749	55.181437	48.597556
1501.789871	58.158070	48.602561
1497.662884	45.402355	48.607565
1494.478377	60.394291	48.612570
1490.883758	46.995739	48.617575
1487.317588	56.728900	48.622580
1484.276876	45.316361	48.627585
1481.104659	43.051566	48.632589
1476.774832	47.243727	48.637594
1473.647059	45.721812	48.642599
1470.107195	49.215225	48.647604
1466.856618	38.271950	48.652609
1463.209406	52.861344	48.657613
1459.861041	51.582567	48.662618
1456.224956	43.733282	48.667623
1452.766369	49.801951	48.672628
1449.069998	46.182423	48.677633
1445.285145	43.908585	48.682637
1441.790385	47.122903	48.687642
1438.853757	40.474523	48.692647
1435.119120	47.389738	48.697652
1431.368243	39.855713	48.702657
1428.138815	50.017340	48.707661
1424.471339	43.897161	48.712666
1421.403035	34.263770	48.717671
1417.714442	44.711993	48.722676
1414.231212	43.504833	48.727681
1410.809473	39.893185	48.732685
1406.787336	42.139243	48.737690
1403.923856	41.303848	48.742695
1400.130367	47.171551	48.747700
1396.812447	46.637839	48.752705
1393.107984	52.150007	48.757709
1389.422562	49.500038	48.762714
1386.179737	48.056149	48.767719
1382.590712	51.437001	48.772724
1379.461955	48.273289	48.777729
1376.255112	49.860949	48.782733
1372.567859	49.751715	48.787738
1369.176290	48.486001	48.792743
1365.324852	56.286256	48.797748
1361.678690	50.789179	48.802753
1358.156541	49.040763	48.807757
1354.719266	53.337615	48.812762
1351.159641	45.634630	48.817767
1347.193539	56.844215	48.822772
1344.049558	38.595215	48.827777
1341.130287	50.530853	48.832781
1337.092098	45.319424	48.837786
1334.223303	42.817595	48.842791
1330.369525	57.043680	48.847796
1326.547726	48.454543	48.852801
1323.466056	43.024632	48.857805
1319.946723	53.357932	48.862810
1316.419031	45.143792	48.867815
1312.784035	46.677880	48.872820
1309.040249	43.682673	48.877825
1305.826523	47.432212	48.882829
1302.007078	50.156087	48.887834
1298.605950	41.435043	48.892839
1295.121396	46.065117	48.897844
1292.066196	38.698074	48.902849
1288.564144	41.869245	48.907853
1284.964196	39.452755	48.912858
1281.657828	32.058375	48.917863
1277.709753	39.677520	48.922868
1274.106911	44.294370	48.927873
1270.844625	46.165909	48.932877
1267.077455	53.076707	48.937882
1263.742033	34.047625	48.942887
1260.085810	41.083516	48.947892
1256.748230	45.149724	48.952897
1253.463173	54.291813	48.957901
1249.677853	47.671158	48.962906
1246.552414	50.135155	48.967911
1242.488824	49.426466	48.972916
1239.271618	51.012587	48.977921
1235.723234	43.836210	48.982925
1231.941345	52.150817	48.987930
1229.051317	39.424089	48.992935
1225.253546	41.360000	48.997940
1221.628995	33.445692	49.002945
1218.092208	44.237277	49.007949
1214.761817	40.045136	49.012954
1211.154764	37.623434	49.017959
1207.700727	43.295945	49.022964
1204.303756	42.780885	49.027969
1200.729654	45.131228	49.032973
1197.122118	46.759127	49.037978
1193.919592	42.847636	49.042983
1190.292743	44.098898	49.047988
1187.104493	36.863313	49.052993
1183.440510	45.779649	49.057997
1179.263917	42.010287	49.063002
1176.180910	38.535767	49.068007
1172.568471	44.805563	49.073012
1169.238997	48.465564	49.078017
1166.094352	49.122926	49.083021
1162.335736	35.468416	49.088026
1159.268405	39.103429	49.093031
1155.288803	45.955551	49.098036
1151.578602	38.067239	49.103041
1148.245871	48.067780	49.108045
1144.457999	43.570379	49.113050
1141.486293	40.176612	49.118055
1137.646728	50.499651	49.123060
1134.269959	42.103868	49.128065
1130.944740	43.684665	49.133069
1127.032937	40.218938	49.138074
1123.732495	36.888999	49.143079
1120.376993	39.455254	49.148084
1116.499491	46.690110	49.153089
1113.183179	40.955075	49.158093
1109.765520	47.042700	49.163098
1106.605586	31.406295	49.168103
1102.720368	34.339736	49.173108
1099.139354	32.534080	49.178113
1095.634330	47.427190	49.183117
1092.033064	35.080116	49.188122
1088.843639	35.874167	49.193127
1084.785425	45.377044	49.198132
1081.395939	31.851755	49.203137
1078.387281	43.007214	49.208141
1074.737909	44.727057	49.213146
1071.429849	36.788819	49.218151
1067.528995	42.603653	49.223156
1064.269076	43.354897	49.228161
1060.980664	41.718829	49.233165
1057.136568	40.877925	49.238170
1053.445988	33.979977	49.243175
1049.563111	40.737955	49.248180
1046.835078	42.374495	49.253185
1043.155613	42.928462	49.258189
1039.477064	48.249961	49.263194
1036.595770	43.377346	49.268199
1032.890306	39.851043	49.273204
1029.553952	43.762055	49.278209
1025.483334	38.220378	49.283213
1021.937551	35.052027	49.288218
1018.911221	36.779293	49.293223
1015.331562	39.975222	49.298228
1011.578467	38.123598	49.303233
1008.307530	37.294720	49.308237
1004.911229	41.695945	49.313242
1001.487464	33.491000	49.318247
997.248788	44.202026	49.323252
993.820291	39.689837	49.328257
990.600221	28.185104	49.333261
987.410219	31.181177	49.338266
983.792245	33.712371	49.343271
980.069192	36.715493	49.348276
976.382741	37.738779	49.353281
972.920690	32.115039	49.358285
969.538886	36.286223	49.363290
966.487506	33.252888	49.368295
962.310860	35.535698	49.373300
959.346434	38.018944	49.378305
955.834178	32.159418	49.383309
952.180305	30.083555	49.388314
948.643550	26.948612	49.393319
944.884181	33.671551	49.398324
941.402565	28.202719	49.403329
938.133959	34.469624	49.408333
934.481143	39.537192	49.413338
931.239012	28.399729	49.418343
927.338732	35.903889	49.423348
923.852991	43.599781	49.428353
920.911642	35.952492	49.433357
916.654206	47.517473	49.438362
913.821447	40.830858	49.443367
910.155237	41.268884	49.448372
906.551225	33.727915	49.453377
903.470894	29.784791	49.458381
899.628608	41.671115	49.463386
896.284349	34.371281	49.468391
892.306088	33.396264	49.473396
888.871583	40.606466	49.478401
885.789108	28.574147	49.483405
881.884159	45.029090	49.488410
878.723926	31.123320	49.493415
874.941284	34.474242	49.498420
871.262260	39.571205	49.503425
868.119934	39.706227	49.508429
864.481845	34.660387	49.513434
861.252530	31.158067	49.518439
857.910621	35.509706	49.523444
854.029911	34.709330	49.528449
850.466324	33.157253	49.533453
846.665239	40.016406	49.538458
843.520790	33.115739	49.543463
840.027482	41.205108	49.548468
836.536733	38.271820	49.553473
832.982583	39.995847	49.558477
829.197259	38.383379	49.563482
826.215919	36.870379	49.568487
822.574906	30.157744	49.573492
819.090698	41.441013	49.578497
815.672735	32.713193	49.583501
811.629014	39.733502	49.588506
808.518707	32.802217	49.593511
805.056709	38.466500	49.598516
801.613385	35.744129	49.603521
798.234726	34.663132	49.608525
794.636284	40.677679	49.613530
790.853856	32.572898	49.618535
787.791415	45.049658	49.623540
783.733488	38.569602	49.628545
780.711745	32.706513	49.633549
776.790598	42.612001	49.638554
773.392532	37.715468	49.643559
769.939575	38.566393	49.648564
766.518899	33.075448	49.653569
763.222900	29.681596	49.658573
759.373030	28.977671	49.663578
755.816843	40.964991	49.668583
752.114084	35.084535	49.673588
749.106834	38.634297	49.678593
745.876767	27.026771	49.683597
741.862155	32.875156	49.688602
738.130204	27.805988	49.693607
734.839787	32.260349	49.698612
731.260484	28.100704	49.703617
728.096935	32.057601	49.708621
724.476068	38.980455	49.713626
721.392844	35.680032	49.718631
717.408527	34.848349	49.723636
713.606683	38.822358	49.728641
710.332040	33.191633	49.733645
707.100102	36.051893	49.738650
703.236410	33.755635	49.743655
699.928257	36.545505	49.748660
695.994102	39.932687	49.753665
693.272181	38.100914	49.758669
689.356645	33.338735	49.763674
685.777742	36.468140	49.768679
682.457473	33.957579	49.773684
678.427340	35.765211	49.778689
675.606840	29.389933	49.783693
672.068462	42.301440	49.788698
668.763781	30.797291	49.793703
664.815381	41.969333	49.798708
660.951401	32.216345	49.803713
657.446312	32.192734	49.808717
653.707072	40.140068	49.813722
650.999091	41.697590	49.818727
647.699071	30.176902	49.823732
644.615092	30.986220	49.828737
640.955713	30.230511	49.833741
636.889750	32.913737	49.838746
633.449602	29.444271	49.843751
629.401663	26.490191	49.848756
626.149956	31.742108	49.853761
622.979167	33.526699	49.858765
619.241184	35.099038	49.863770
615.825757	39.351415	49.868775
611.869999	28.426351	49.873780
608.580629	33.032416	49.878785
605.416715	28.080481	49.883789
601.526987	35.159089	49.888794
598.203669	29.099375	49.893799
594.836756	33.799769	49.898804
591.020609	35.599410	49.903809
588.144755	26.540480	49.908813
584.268847	38.261208	49.913818
581.010378	37.234293	49.918823
576.828356	34.576334	49.923828
573.041397	36.093031	49.928833
570.141349	35.962586	49.933837
566.940793	41.462804	49.938842
563.777615	36.156427	49.943847
560.104331	26.003630	49.948852
556.487633	39.098167	49.953857
552.877241	34.769387	49.958861
549.246329	38.511164	49.963866
545.646412	28.327965	49.968871
542.144980	29.373120	49.973876
538.851809	34.656808	49.978881
535.222924	33.785639	49.983885
531.552081	36.147947	49.988890
528.328757	32.122736	49.993895
524.876338	34.406749	49.998900
521.663181	27.244761	50.003905
517.824574	36.602751	50.008909
513.942459	33.404582	50.013914
510.687211	30.836469	50.018919
507.075116	33.955241	50.023924
503.376490	40.925017	50.028929
500.014406	28.882528	50.033933
496.944695	37.782307	50.038938
493.771969	30.180606	50.043943
489.465140	35.005188	50.048948
485.680333	34.066553	50.053953
482.627861	27.199088	50.058957
478.861932	40.123876	50.063962
475.612610	33.524330	50.068967
472.510169	28.711539	50.073972
469.245491	36.274966	50.078977
465.587278	26.578576	50.083981
461.714217	28.175128	50.088986
457.849557	30.953584	50.093991
454.323214	28.649140	50.098996
450.990763	24.549186	50.104001
447.911881	36.990538	50.109005
443.917978	40.349087	50.114010
440.670903	32.774788	50.119015
437.239958	28.911625	50.124020
433.541360	35.011392	50.129025
430.313776	31.977088	50.134029
426.374868	35.833264	50.139034
422.964563	22.982078	50.144039
419.835229	29.584827	50.149044
416.156494	34.634329	50.154049
412.896688	25.514987	50.159053
408.879724	35.824541	50.164058
405.832426	26.795500	50.169063
402.295388	40.447100	50.174068
398.694851	36.028230	50.179073
394.846081	30.126284	50.184077
391.589773	29.111714	50.189082
388.119239	26.032985	50.194087
384.791962	32.732990	50.199092
381.041568	39.378650	50.204097
377.382889	25.528458	50.209101
373.742755	26.054241	50.214106
370.421279	25.075129	50.219111
367.253083	32.693141	50.224116
363.551684	27.059316	50.229121
360.381218	32.137260	50.234125
356.591058	30.990677	50.239130
352.849738	22.930213	50.244135
349.236138	32.284818	50.249140
345.777081	31.586549	50.254145
342.475215	24.976229	50.259149
338.966413	38.120410	50.264154
335.596234	30.302714	50.269159
332.444481	30.850543	50.274164
328.729657	38.357513	50.279169
325.199231	26.749388	50.284173
321.438784	31.735693	50.289178
317.917884	30.110611	50.294183
314.504620	16.870787	50.299188
311.423107	24.684105	50.304193
307.819147	27.020208	50.309197
303.916870	26.944589	50.314202
300.049313	25.205806	50.319207
297.083242	29.932402	50.324212
293.314794	21.733810	50.329217
289.871149	24.608088	50.334221
286.173007	33.855641	50.339226
282.901578	22.697575	50.344231
279.587120	30.303562	50.349236
275.742200	28.045581	50.354241
272.965575	25.102442	50.359245
268.753201	38.738965	50.364250
265.384853	30.974780	50.369255
262.069156	23.838297	50.374260
258.415599	28.890222	50.379265
255.181162	18.299029	50.384269
251.733144	25.255113	50.389274
247.672123	27.485217	50.394279
244.165428	22.646820	50.399284
241.068149	25.581070	50.404289
237.667971	24.917941	50.409293
234.045233	26.333188	50.414298
230.391711	30.432849	50.419303
226.677726	30.270981	50.424308
223.042384	34.127374	50.429313
219.756349	32.415123	50.434317
216.484497	33.348649	50.439322
213.377719	27.407149	50.444327
209.344995	32.151127	50.449332
205.652736	37.190103	50.454337
202.392177	32.319717	50.459341
198.410212	37.277252	50.464346
195.279740	26.733154	50.469351
192.213825	25.783879	50.474356
188.086609	30.934865	50.479361
184.952516	34.833443	50.484365
181.440734	40.072107	50.489370
177.730748	24.771509	50.494375
174.402224	26.757871	50.499380
170.949766	34.299934	50.504385
168.000906	29.773320	50.509389
164.274987	36.127296	50.514394
160.485660	30.643237	50.519399
156.472009	37.836090	50.524404
153.063339	36.307452	50.529409
149.893485	30.271382	50.534413
146.137634	41.625440	50.539418
143.343255	33.275222	50.544423
139.463778	31.089082	50.549428
135.834925	38.098645	50.554433
132.487542	29.261906	50.559437
128.609762	36.341861	50.564442
125.274412	36.076767	50.569447
121.931656	28.220046	50.574452
118.526167	33.556057	50.579457
114.959455	25.591842	50.584461
111.351833	35.881977	50.589466
107.787486	32.887501	50.594471
104.396747	35.171451	50.599476
100.542261	40.751374	50.604481
97.368174	30.745580	50.609485
93.556333	42.671490	50.614490
90.191479	34.213954	50.619495
86.684947	42.033356	50.624500
83.342267	32.999747	50.629505
79.715560	23.238434	50.634509
75.991012	37.963241	50.639514
72.906438	34.147449	50.644519
69.657909	33.058949	50.649524
65.849304	35.958440	50.654529
62.273086	35.870058	50.659533
58.585833	30.923768	50.664538
55.343816	28.227119	50.669543
51.619156	35.751463	50.674548
48.300603	42.070500	50.679553
44.758373	29.328527	50.684557
41.225374	36.630048	50.689562
37.931373	24.001288	50.694567
34.406393	27.951248	50.699572
30.411570	30.367225	50.704577
27.108477	31.789679	50.709581
23.582413	37.660150	50.714586
20.288908	39.005184	50.719591
16.590926	27.967371	50.724596
13.342354	31.646515	50.729601
10.024412	31.413528	50.734605
6.476518	31.194198	50.739610
2.835077	33.858869	50.744615