Fri Aug 26 11:10:54 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.170593	104.017431	0.000000
0.119805	104.867074	0.005005
0.109979	108.022978	0.010010
0.125452	110.735193	0.015014
0.085758	103.756204	0.020019
0.231528	98.570612	0.025024
0.079212	85.572898	0.030029
-0.019446	86.999452	0.035034
-0.307624	77.173904	0.040038
-0.410207	75.092572	0.045043
-1.168765	65.337103	0.050048
-1.148711	55.245285	0.055053
-1.510960	48.034973	0.060058
-1.920609	37.677884	0.065062
-2.109291	40.406058	0.070067
-2.342490	30.578303	0.075072
-2.845247	25.120395	0.080077
-3.066472	15.350893	0.085082
-3.540525	12.286565	0.090086
-2.947889	12.460240	0.095091
-3.463571	9.067048	0.100096
-3.814311	-4.219234	0.105101
-4.083393	-3.145790	0.110106
-4.640509	-5.324016	0.115110
-4.771804	-3.772169	0.120115
-5.430042	-3.236063	0.125120
-5.626210	-9.962862	0.130125
-6.186987	-5.022320	0.135130
-6.163622	-6.737289	0.140134
-6.011875	-4.169690	0.145139
-6.280655	-3.479094	0.150144
-6.456534	-3.416709	0.155149
-7.395077	0.291885	0.160154
-7.873077	-3.429864	0.165158
-7.646020	-5.103783	0.170163
-7.724272	3.526369	0.175168
-7.871236	-7.944068	0.180173
-7.881861	1.741702	0.185178
-8.705490	-2.116052	0.190182
-9.182808	-4.407939	0.195187
-9.309292	0.601022	0.200192
-9.227847	-6.684676	0.205197
-9.067851	0.168376	0.210202
-9.317262	-6.366643	0.215206
-10.131656	-2.104760	0.220211
-10.597528	2.292678	0.225216
-10.573311	-6.483677	0.230221
-10.695389	-1.497548	0.235226
-11.106456	2.166883	0.240230
-11.508193	-0.396191	0.245235
-12.032035	-0.497921	0.250240
-12.112345	-1.462782	0.255245
-12.403776	-8.174749	0.260250
-12.224705	0.598828	0.265254
-11.960588	1.092563	0.270259
-12.526701	0.453268	0.275264
-13.042666	-8.751491	0.280269
-13.419123	-0.144511	0.285274
-14.119402	-4.407434	0.290278
-13.904053	-7.541133	0.295283
-14.289151	-2.865217	0.300288
-14.266883	-12.460650	0.305293
-14.370849	4.313560	0.310298
-14.554654	-1.402800	0.315302
-14.888873	-2.255364	0.320307
-15.329040	6.905685	0.325312
-15.251023	-7.244588	0.330317
-15.976027	-6.407031	0.335322
-16.567070	-4.739312	0.340326
-16.663526	-4.056564	0.345331
-16.958127	-1.843398	0.350336
-16.616867	1.011058	0.355341
-16.808429	-4.400383	0.360346
-17.209235	-5.587416	0.365350
-17.116871	-7.930038	0.370355
-18.142168	-7.842964	0.375360
-18.113417	-8.116149	0.380365
-18.510462	-2.460807	0.385370
-18.154935	-2.000287	0.390374
-18.255374	-6.635004	0.395379
-19.203980	-2.402843	0.400384
-19.466072	-6.480899	0.405389
-19.580979	3.676672	0.410394
-19.556269	-3.514775	0.415398
-19.875747	-4.901126	0.420403
-20.823197	-2.750822	0.425408
-20.901343	-13.181639	0.430413
-21.090845	2.153773	0.435418
-21.644016	6.972915	0.440422
-21.292293	-1.041377	0.445427
-21.370276	0.204787	0.450432
-21.176265	0.298163	0.455437
-21.689527	0.093550	0.460442
-22.534117	-3.941267	0.465446
-22.361806	-4.167204	0.470451
-22.711294	-3.815206	0.475456
-23.080267	-1.565152	0.480461
-23.439182	4.571456	0.485466
-23.834603	-3.715634	0.490470
-23.795305	-4.939554	0.495475
-24.159822	-0.453497	0.500480
-23.729082	-8.571835	0.505485
-24.899617	-7.674400	0.510490
-25.335139	-3.471507	0.515494
-24.900657	-5.791469	0.520499
-25.586814	3.575552	0.525504
-25.550384	-1.558187	0.530509
-25.497826	5.843086	0.535514
-26.079175	8.325518	0.540518
-26.369822	-0.553669	0.545523
-26.556183	0.579659	0.550528
-26.219968	-14.582046	0.555533
-27.464202	0.234237	0.560538
-28.309895	-0.472254	0.565542
-27.501277	2.398017	0.570547
-27.743563	8.019775	0.575552
-28.233002	-1.435881	0.580557
-28.414436	6.992046	0.585562
-28.286840	1.037382	0.590566
-28.526688	3.071187	0.595571
-29.329159	4.436480	0.600576
-29.384554	3.372831	0.605581
-29.754933	4.816375	0.610586
-30.137243	15.123150	0.615590
-29.527396	7.710885	0.620595
-30.438420	-0.106799	0.625600
-30.836029	-0.557201	0.630605
-31.014639	8.227778	0.635610
-31.297845	5.481739	0.640614
-31.139084	5.767258	0.645619
-31.460029	6.709577	0.650624
-31.796561	-1.672100	0.655629
-32.327229	0.204511	0.660634
-32.899901	2.733046	0.665638
-32.887770	-1.163088	0.670643
-32.916176	7.870577	0.675648
-32.714677	0.895205	0.680653
-32.867709	-5.044236	0.685658
-33.444521	-0.446034	0.690662
-33.619362	2.090159	0.695667
-34.457601	2.388546	0.700672
-34.403969	-2.219541	0.705677
-34.161633	3.200214	0.710682
-35.154045	3.272678	0.715686
-35.735081	8.187904	0.720691
-35.746485	1.432335	0.725696
-35.764997	-7.821402	0.730701
-36.078844	-1.343813	0.735706
-35.882725	4.791795	0.740710
-35.802318	-5.154365	0.745715
-36.356007	7.428439	0.750720
-36.849739	-0.039779	0.755725
-37.345828	2.135158	0.760730
-37.299534	2.985499	0.765734
-37.179514	-0.471868	0.770739
-37.945062	5.977980	0.775744
-38.090730	0.534084	0.780749
-38.556592	-0.307474	0.785754
-38.618064	8.430793	0.790758
-38.742688	3.328457	0.795763
-38.951308	-0.280215	0.800768
-39.879712	-2.818232	0.805773
-40.136190	-2.635734	0.810778
-40.524668	-5.238835	0.815782
-40.396780	-2.578940	0.820787
-40.736517	-4.091846	0.825792
-40.673190	4.048041	0.830797
-40.661323	4.536759	0.835802
-40.450769	-0.206489	0.840806
-40.680164	-5.333637	0.845811
-41.725840	1.906445	0.850816
-41.851472	-6.960467	0.855821
-42.003738	-1.558366	0.860826
-42.645468	0.718339	0.865830
-42.984742	-4.926357	0.870835
-43.222904	-8.369081	0.875840
-43.226598	-3.758878	0.880845
-43.400542	-2.782501	0.885850
-43.113960	-1.235608	0.890854
-43.446410	-5.527327	0.895859
-44.434219	-0.207096	0.900864
-44.474230	-2.032415	0.905869
-44.511438	6.395200	0.910874
-44.682330	-0.873355	0.915878
-44.796941	-3.920879	0.920883
-45.713082	-1.357849	0.925888
-45.847213	-1.150109	0.930893
-46.000692	-13.457889	0.935898
-46.140648	-9.740764	0.940902
-46.074881	-10.984623	0.945907
-46.551535	-10.989299	0.950912
-47.191518	-6.821009	0.955917
-47.636203	-4.973604	0.960922
-47.771480	-1.614697	0.965926
-47.589957	-3.594727	0.970931
-48.109701	3.519177	0.975936
-48.268350	-5.086340	0.980941
-47.864446	-4.851644	0.985946
-48.308601	-0.634752	0.990950
-48.665324	-11.430303	0.995955
-49.080701	-7.553240	1.000960
-48.982059	-6.195377	1.005965
-49.834316	-3.224693	1.010970
-50.181081	-0.718677	1.015974
-50.113633	-7.040445	1.020979
-50.546200	-7.134240	1.025984
-50.819030	-5.288283	1.030989
-50.595096	-4.032182	1.035994
-50.973313	-2.258399	1.040998
-51.713243	-12.437483	1.046003
-51.937172	-5.755605	1.051008
-52.301242	-0.127543	1.056013
-52.120517	-5.236292	1.061018
-52.146038	-4.754407	1.066022
-52.414475	-7.619798	1.071027
-53.278061	-4.457531	1.076032
-53.853773	1.918467	1.081037
-53.918438	2.482374	1.086042
-53.763270	0.487465	1.091046
-53.280904	-1.520424	1.096051
-53.172587	-0.018540	1.101056
-53.677887	0.737356	1.106061
-54.447487	2.992843	1.111066
-54.842343	9.135047	1.116070
-55.199450	8.346157	1.121075
-55.827320	4.416797	1.126080
-56.128145	-4.799311	1.131085
-56.293535	1.376763	1.136090
-56.455491	5.182735	1.141094
-56.011484	-0.900283	1.146099
-56.405869	4.305408	1.151104
-56.601170	-0.618248	1.156109
-57.365601	-1.391173	1.161114
-57.874120	1.753775	1.166118
-57.445515	2.898917	1.171123
-57.300914	-1.106423	1.176128
-57.929356	6.834299	1.181133
-58.866944	-0.719827	1.186138
-59.429650	9.032920	1.191142
-58.935161	-1.825570	1.196147
-59.231955	0.834011	1.201152
-59.498394	-0.222087	1.206157
-59.457362	0.641727	1.211162
-59.568641	1.447001	1.216166
-60.095925	2.067119	1.221171
-60.554945	13.787329	1.226176
-60.739904	9.184751	1.231181
-60.652241	-3.078325	1.236186
-60.895548	11.313211	1.241190
-61.687259	-3.214154	1.246195
-62.088082	2.248794	1.251200
-62.401789	-5.392977	1.256205
-62.304116	0.887666	1.261210
-62.400904	-0.931977	1.266214
-62.267698	0.490105	1.271219
-62.912978	4.216312	1.276224
-63.220865	-0.708797	1.281229
-63.564546	-0.465266	1.286234
-64.153785	-2.967508	1.291238
-63.702633	-8.377779	1.296243
-64.062402	3.687625	1.301248
-64.554424	-1.056958	1.306253
-65.209136	-2.232930	1.311258
-65.430867	0.940128	1.316262
-65.326619	-1.859908	1.321267
-65.391642	3.285010	1.326272
-65.667416	8.703180	1.331277
-65.528288	4.059634	1.336282
-65.843784	3.650230	1.341286
-66.674798	3.064836	1.346291
-66.848949	2.997243	1.351296
-66.910287	-0.514140	1.356301
-66.999659	-3.233412	1.361306
-67.007841	2.212693	1.366310
-67.671548	-7.952951	1.371315
-68.214775	1.673377	1.376320
-68.673213	-2.086215	1.381325
-68.443914	-2.175498	1.386330
-68.945794	-6.893236	1.391334
-68.581537	1.845176	1.396339
-69.104667	-2.151107	1.401344
-69.700674	4.417870	1.406349
-69.919082	-8.256275	1.411354
-70.352969	1.235972	1.416358
-70.093583	-6.966411	1.421363
-70.421909	-5.054868	1.426368
-70.704231	4.689020	1.431373
-70.661957	-7.434113	1.436378
-71.435447	-10.970649	1.441382
-71.499233	-6.797164	1.446387
-71.755131	-10.047307	1.451392
-71.808525	-0.519394	1.456397
-72.040210	-3.131088	1.461402
-72.629040	-9.828382	1.466406
-72.716349	-11.099025	1.471411
-73.194763	-3.165849	1.476416
-73.328222	-4.903853	1.481421
-73.323659	-9.093024	1.486426
-73.700789	1.738097	1.491430
-73.500769	1.492027	1.496435
-74.339443	9.225046	1.501440
-74.408093	6.844221	1.506445
-74.035317	-6.402847	1.511450
-75.154444	-2.511118	1.516454
-75.619882	-4.235397	1.521459
-75.852677	0.094113	1.526464
-76.213432	9.894507	1.531469
-76.174283	0.163571	1.536474
-76.284700	1.193330	1.541478
-76.292345	-3.218560	1.546483
-75.976717	3.768439	1.551488
-77.078133	6.325518	1.556493
-76.956850	2.222571	1.561498
-77.470033	6.870976	1.566502
-77.159349	-6.037404	1.571507
-77.858464	3.695450	1.576512
-78.573964	8.710703	1.581517
-78.860345	0.887512	1.586522
-79.143692	10.349997	1.591526
-79.022586	6.383114	1.596531
-79.143944	3.159476	1.601536
-79.325414	6.183902	1.606541
-79.569033	5.820252	1.611546
-80.208304	7.928902	1.616550
-80.153794	3.896460	1.621555
-80.234903	3.301871	1.626560
-80.450525	-1.422475	1.631565
-80.976768	-5.554309	1.636570
-81.880692	-1.370232	1.641574
-81.630784	-3.930364	1.646579
-81.922027	0.765738	1.651584
-81.879670	-5.741941	1.656589
-82.080342	-3.299800	1.661594
-82.668134	-1.512368	1.666598
-82.394710	-5.044236	1.671603
-82.896819	3.408305	1.676608
-83.240229	-7.958773	1.681613
-83.414309	-2.996187	1.686618
-83.442079	1.994238	1.691622
-84.546932	-5.198493	1.696627
-84.827327	-7.837402	1.701632
-85.017293	-3.663253	1.706637
-84.961147	-5.829398	1.711642
-85.334888	-9.228865	1.716646
-84.761734	-10.229033	1.721651
-85.296866	-5.343104	1.726656
-84.932144	3.259198	1.731661
-85.260998	-5.506470	1.736666
-86.158048	-7.103436	1.741670
-86.400170	-5.088261	1.746675
-87.140458	3.078674	1.751680
-87.404256	1.746927	1.756685
-87.543697	-9.003361	1.761690
-87.783306	4.055697	1.766694
-87.492760	4.184660	1.771699
-87.783628	-4.492012	1.776704
-87.929498	-9.882089	1.781709
-88.502968	-8.637870	1.786714
-89.144555	-4.836313	1.791718
-88.989317	-4.670464	1.796723
-89.388110	-1.223074	1.801728
-89.388646	-0.571079	1.806733
-89.376494	-13.081808	1.811738
-90.271064	1.395302	1.816742
-90.600008	-9.743081	1.821747
-90.478025	-10.549619	1.826752
-91.101280	-5.909389	1.831757
-90.711253	-10.449631	1.836762
-90.893713	-0.066422	1.841766
-91.326355	4.031622	1.846771
-92.012240	-3.381362	1.851776
-92.509372	0.739378	1.856781
-92.212311	-9.607491	1.861786
-92.649405	-2.810169	1.866790
-92.301114	-0.576884	1.871795
-92.651471	-4.657012	1.876800
-93.591292	-3.975824	1.881805
-93.618573	-5.958143	1.886810
-93.896777	-2.026510	1.891814
-93.692726	-10.375292	1.896819
-94.513189	-11.468509	1.901824
-95.246736	1.060035	1.906829
-94.664322	-3.525983	1.911834
-94.974384	-2.711903	1.916838
-95.416899	-1.127418	1.921843
-95.062617	-11.530649	1.926848
-95.698761	-10.216562	1.931853
-96.069862	-9.854870	1.936858
-96.666771	-9.669984	1.941862
-97.082667	-3.477055	1.946867
-97.050125	-1.928573	1.951872
-97.222202	-9.301336	1.956877
-97.120481	-3.011837	1.961882
-97.489410	-3.346485	1.966886
-97.112163	-9.988559	1.971891
-98.025172	-1.405606	1.976896
-98.298389	-1.862720	1.981901
-98.189701	-9.295017	1.986906
-98.373403	-4.340425	1.991910
-98.999384	-1.265771	1.996915
-99.664993	-0.067964	2.006912
-98.686803	1.661741	2.016909
-98.169630	-8.684873	2.026906
-98.377904	-8.892787	2.036902
-98.126530	-1.782045	2.046899
-97.589022	-8.397115	2.056896
-96.722696	-5.778878	2.066893
-95.772622	-7.630623	2.076890
-95.170053	-7.505472	2.086886
-94.823262	-1.603805	2.096883
-94.618954	-1.381800	2.106880
-94.424753	0.609352	2.116877
-93.675543	-0.821492	2.126874
-93.026198	-8.648196	2.136870
-92.360720	-3.692607	2.146867
-91.426468	5.335970	2.156864
-91.630617	-3.137099	2.166861
-91.432002	1.184787	2.176858
-90.657682	2.113132	2.186854
-90.142573	4.301399	2.196851
-89.496600	-1.478453	2.206848
-88.801994	6.380547	2.216845
-88.731632	-1.346509	2.226842
-87.905093	1.987488	2.236838
-87.500219	-4.429542	2.246835
-87.171677	3.888750	2.256832
-86.515615	0.688997	2.266829
-86.096688	4.352546	2.276826
-85.562199	2.340602	2.286822
-84.760246	2.748310	2.296819
-84.557581	7.136090	2.306816
-84.631583	4.560007	2.316813
-83.720991	6.712039	2.326810
-82.981503	5.504446	2.336806
-82.218608	1.676695	2.346803
-81.760243	4.136715	2.356800
-81.593258	0.091313	2.366797
-81.142145	-3.751246	2.376794
-80.266489	1.592924	2.386790
-80.203723	-0.801721	2.396787
-79.604762	-0.657002	2.406784
-79.066591	3.089348	2.416781
-78.672141	-6.471579	2.426778
-77.510157	3.931163	2.436774
-77.272566	-6.172358	2.446771
-77.075291	4.934938	2.456768
-76.927052	-0.007171	2.466765
-75.934177	1.327455	2.476762
-75.769271	-3.053398	2.486758
-74.782889	1.842726	2.496755
-74.506210	-7.487628	2.506752
-74.397518	-5.198070	2.516749
-73.254204	-5.027237	2.526746
-73.040278	-6.403246	2.536742
-72.555107	-1.951753	2.546739
-71.808776	-4.962827	2.556736
-71.554250	-3.443551	2.566733
-71.215112	4.546821	2.576730
-70.502253	6.707467	2.586726
-70.160162	6.651437	2.596723
-69.146088	3.630350	2.606720
-68.741042	4.882279	2.616717
-68.831757	-1.178833	2.626714
-67.814959	-2.768545	2.636710
-67.506265	-6.173962	2.646707
-67.172056	-0.324185	2.656704
-66.206644	-3.816015	2.666701
-65.725620	-5.838641	2.676698
-65.458165	-2.271880	2.686694
-65.427720	-7.379372	2.696691
-64.806960	-5.046003	2.706688
-63.731275	0.276527	2.716685
-63.162055	1.867178	2.726682
-62.638393	2.543124	2.736678
-62.767749	-8.193821	2.746675
-62.097486	-0.156808	2.756672
-61.132040	-3.879885	2.766669
-61.385944	-0.437848	2.776666
-60.500184	-1.180390	2.786662
-59.931547	6.745742	2.796659
-59.721270	-0.176333	2.806656
-58.772947	-5.673820	2.816653
-58.471863	0.808319	2.826650
-57.692034	1.491896	2.836646
-57.187490	-0.328492	2.846643
-56.997082	2.027536	2.856640
-56.744048	-1.796854	2.866637
-55.838419	-4.259379	2.876634
-55.444487	-1.320507	2.886630
-55.196055	-5.163187	2.896627
-54.391283	4.018597	2.906624
-54.106165	-3.681711	2.916621
-53.120862	-2.843234	2.926618
-52.501403	1.742570	2.936614
-52.522664	-3.144638	2.946611
-52.540337	11.395067	2.956608
-51.529831	-3.615189	2.966605
-51.191151	-2.147027	2.976602
-50.377331	-1.158309	2.986598
-49.744283	4.372520	2.996595
-49.471836	3.576590	3.006592
-48.726077	2.317339	3.016589
-48.304514	5.590854	3.026586
-48.121766	6.551122	3.036582
-47.596107	-1.836017	3.046579
-47.072925	-4.406882	3.056576
-46.296063	1.659068	3.066573
-45.481332	2.153485	3.076570
-45.242296	-2.609532	3.086566
-45.508033	-0.648133	3.096563
-44.467735	-3.077774	3.106560
-44.152887	0.807882	3.116557
-43.118531	-5.602626	3.126554
-42.570500	-1.848308	3.136550
-42.675305	6.084481	3.146547
-42.101363	-1.217322	3.156544
-41.207854	-8.910988	3.166541
-40.887535	-2.653583	3.176538
-40.466272	3.401214	3.186534
-39.836288	-1.397332	3.196531
-39.485223	3.448833	3.206528
-39.043351	-3.385761	3.216525
-38.337664	-5.525726	3.226522
-37.972552	-3.234911	3.236518
-37.394933	-1.126065	3.246515
-36.455755	-3.777539	3.256512
-36.475632	-4.999940	3.266509
-35.960861	0.083653	3.276506
-35.113466	-3.297939	3.286502
-35.018027	0.438153	3.296499
-34.585188	-0.541135	3.306496
-33.644782	-3.690128	3.316493
-33.670698	-5.709848	3.326490
-33.174958	-5.891167	3.336486
-32.047954	-4.583758	3.346483
-31.964951	-1.076972	3.356480
-31.436334	-4.348744	3.366477
-30.792169	-3.549013	3.376474
-30.538952	-9.818891	3.386470
-29.351706	-7.516703	3.396467
-29.186162	-3.012275	3.406464
-28.928253	-0.422843	3.416461
-28.828314	-3.320604	3.426458
-27.951078	-6.456594	3.436454
-27.613698	-11.105045	3.446451
-26.453185	-5.726032	3.456448
-26.413105	-6.919757	3.466445
-26.288604	-8.085445	3.476442
-25.321760	-13.389416	3.486438
-24.798556	-2.367712	3.496435
-24.403758	-3.179523	3.506432
-23.617209	-0.425320	3.516429
-23.307606	-7.223480	3.526426
-23.085817	-3.190292	3.536422
-22.452127	3.167207	3.546419
-21.887869	-3.743460	3.556416
-21.493663	3.291200	3.566413
-20.796498	-0.773397	3.576410
-20.106494	1.976832	3.586406
-20.002338	-3.981579	3.596403
-19.203066	1.903494	3.606400
-19.000424	3.468863	3.616397
-18.497866	-1.046924	3.626394
-17.589718	-3.253257	3.636390
-17.480231	1.801577	3.646387
-17.075040	2.334417	3.656384
-16.226800	0.647411	3.666381
-15.926629	1.576726	3.676378
-14.735138	1.144534	3.686374
-14.882368	-0.520523	3.696371
-14.509522	-2.450281	3.706368
-13.850217	0.371250	3.716365
-13.033067	0.162063	3.726362
-12.922664	4.035205	3.736358
-12.694743	2.695029	3.746355
-11.581409	-4.041379	3.756352
-11.018769	-0.143619	3.766349
-11.008780	1.556279	3.776346
-10.292096	-2.416326	3.786342
-9.664083	-0.929858	3.796339
-9.507419	0.338571	3.806336
-8.854109	-3.057150	3.816333
-8.441014	-0.054738	3.826330
-7.812270	-4.311414	3.836326
-6.833712	-0.883877	3.846323
-6.620518	1.063140	3.856320
-6.363505	-5.226337	3.866317
-6.167989	-6.117990	3.876314
-5.612331	3.406683	3.886310
-5.419922	8.299727	3.896307
-4.753511	17.788159	3.906304
-4.192770	24.020814	3.916301
-3.676065	36.139581	3.926298
-3.184718	39.959755	3.936294
-2.540143	56.439561	3.946291
-2.266338	63.359949	3.956288
-1.505827	65.364304	3.966285
-1.282330	82.555908	3.976282
-0.916405	91.514641	3.986278
-0.307400	117.772436	3.996275
0.000000	124.591248	4.001280
0.096717	124.918066	4.006285
0.602753	132.631592	4.011290
0.647239	139.474210	4.016294
0.525331	148.392796	4.021299
0.592326	146.867168	4.026304
0.534346	160.600406	4.031309
1.179044	162.547126	4.036314
0.803672	170.862961	4.041318
1.241832	161.085625	4.046323
1.268851	160.638705	4.051328
1.070228	163.526628	4.056333
1.269016	167.826949	4.061338
1.004019	165.647509	4.066342
1.283176	164.386232	4.071347
1.636019	156.994937	4.076352
0.823342	149.592130	4.081357
1.103650	143.028362	4.086362
0.712295	150.944891	4.091366
1.065271	157.432609	4.096371
1.517704	164.119973	4.101376
0.734201	153.238909	4.106381
1.119491	151.894670	4.111386
0.893576	163.929857	4.116390
1.003248	160.423450	4.121395
0.799185	165.833668	4.126400
0.996484	166.252392	4.131405
1.673403	162.701957	4.136410
1.720123	162.932159	4.141414
1.260866	160.048994	4.146419
1.457501	165.656246	4.151424
1.193229	159.240536	4.156429
1.404994	154.734332	4.161434
1.627354	164.187768	4.166438
1.399572	158.737624	4.171443
1.244288	147.388601	4.176448
0.953948	143.814768	4.181453
1.113449	149.317068	4.186458
1.355497	166.331779	4.191462
1.515504	163.535689	4.196467
1.204313	165.653384	4.201472
1.128520	171.075270	4.206477
1.436822	164.462844	4.211482
0.976583	162.902247	4.216486
1.100746	168.780205	4.221491
1.455343	165.169226	4.226496
1.101760	165.053640	4.231501
1.621983	162.615907	4.236506
1.180532	172.346703	4.241510
1.304046	168.376243	4.246515
1.380626	165.684888	4.251520
1.376187	179.501551	4.256525
2.021609	177.648584	4.261530
1.497504	175.218428	4.266534
1.245212	169.063434	4.271539
1.354174	175.336056	4.276544
1.746791	190.204521	4.281549
2.152090	178.426520	4.286554
1.368110	180.924705	4.291558
1.369898	167.282858	4.296563
1.565374	174.994137	4.301568
1.733518	188.929466	4.306573
1.596293	183.044446	4.311578
1.560979	193.025222	4.316582
1.638787	194.949480	4.321587
1.877780	201.360051	4.326592
1.738449	199.471082	4.331597
2.025775	185.515850	4.336602
1.605218	180.462701	4.341606
1.511371	170.337932	4.346611
2.030973	188.862815	4.351616
1.702764	180.220331	4.356621
1.943098	162.729116	4.361626
1.705535	175.980975	4.366630
1.726595	172.450398	4.371635
2.060563	178.377949	4.376640
1.880079	173.705028	4.381645
1.935246	176.547111	4.386650
1.704241	179.468552	4.391654
1.626394	174.210189	4.396659
2.018813	180.688610	4.401664
2.121154	186.914812	4.406669
2.195968	176.181663	4.411674
1.477085	177.299841	4.416678
1.766545	179.437911	4.421683
1.936517	180.930213	4.426688
2.210789	192.011202	4.431693
2.388432	188.237949	4.436698
1.979366	187.419174	4.441702
2.069564	176.566573	4.446707
2.006104	173.397160	4.451712
1.679272	174.862411	4.456717
1.567379	181.539572	4.461722
2.105177	191.320387	4.466726
2.356120	201.908317	4.471731
2.257224	196.523514	4.476736
2.265277	188.784102	4.481741
1.999545	179.714285	4.486746
1.797467	183.937821	4.491750
2.099581	191.632504	4.496755
2.385671	194.511401	4.501760
2.014854	191.139909	4.506765
2.309284	184.409416	4.511770
2.204422	182.812468	4.516774
2.057404	189.438155	4.521779
2.312491	186.380491	4.526784
1.953722	195.990861	4.531789
2.141593	186.976963	4.536794
2.336745	194.909759	4.541798
2.560661	192.894633	4.546803
2.059242	189.027796	4.551808
2.271760	192.876742	4.556813
2.232546	187.938219	4.561818
2.335188	189.491623	4.566822
2.381954	199.918358	4.571827
2.486752	202.733736	4.576832
2.280903	194.992825	4.581837
2.249253	193.574298	4.586842
2.175091	198.518222	4.591846
2.204106	203.939618	4.596851
2.135904	199.106842	4.601856
2.102635	197.925843	4.606861
1.847603	194.675525	4.611866
1.884147	199.184607	4.616870
1.912329	197.054427	4.621875
2.404091	206.532377	4.626880
2.456015	220.789540	4.631885
2.810962	211.553467	4.636890
2.027475	209.847047	4.641894
2.597206	214.706542	4.646899
2.746253	223.756981	4.651904
2.720819	219.550279	4.656909
2.794716	205.935138	4.661914
2.609828	206.641154	4.666918
2.308336	198.576618	4.671923
2.656321	202.404475	4.676928
2.214797	211.205181	4.681933
2.583707	213.264447	4.686938
2.672547	229.347641	4.691942
2.871656	225.722895	4.696947
2.643662	211.904823	4.701952
2.312139	209.460495	4.706957
2.364245	214.565094	4.711962
2.822759	220.884546	4.716966
3.071621	222.775848	4.721971
2.888825	221.656092	4.726976
2.764548	215.591879	4.731981
2.368446	204.919378	4.736986
2.479406	215.342454	4.741990
2.811784	223.380444	4.746995
2.555771	227.235909	4.752000
2.595697	232.696743	4.757005
2.831898	222.615467	4.762010
3.158704	233.011274	4.767014
2.986457	230.725639	4.772019
3.000061	222.814508	4.777024
2.859197	231.707615	4.782029
3.082251	229.702111	4.787034
2.610529	216.165587	4.792038
2.707111	223.408241	4.797043
2.950614	225.515507	4.802048
2.849107	232.210053	4.807053
2.745965	233.387385	4.812058
3.105435	224.536572	4.817062
2.656183	225.429278	4.822067
3.104836	224.894563	4.827072
2.862069	229.690745	4.832077
3.082918	220.092741	4.837082
2.880712	230.143815	4.842086
2.863167	232.234780	4.847091
3.242579	226.794478	4.852096
2.801557	235.231294	4.857101
3.148903	225.338352	4.862106
2.999042	233.362846	4.867110
2.968055	228.473650	4.872115
2.858840	221.220707	4.877120
2.718021	230.022059	4.882125
3.091553	228.198766	4.887130
3.122617	223.948465	4.892134
2.826737	229.518527	4.897139
3.034238	225.398939	4.902144
2.902595	234.711382	4.907149
3.082215	228.482792	4.912154
3.112180	232.217804	4.917158
3.195160	232.372760	4.922163
3.152437	225.451142	4.927168
3.064692	232.485222	4.932173
3.037823	235.004737	4.937178
3.203317	241.812736	4.942182
2.849944	242.772771	4.947187
3.508581	253.078960	4.952192
3.544744	252.349045	4.957197
3.493817	237.184126	4.962202
3.647137	233.190029	4.967206
3.255634	230.033717	4.972211
3.299146	222.535537	4.977216
3.144423	231.497238	4.982221
3.065103	218.465916	4.987226
3.204031	231.681344	4.992230
3.324316	243.387441	4.997235
3.779258	248.068669	5.002240
3.510208	255.703615	5.007245
3.391040	239.635012	5.012250
3.399159	230.693371	5.017254
3.118802	244.012053	5.022259
3.542263	241.994327	5.027264
3.298547	246.974155	5.032269
3.676214	243.739211	5.037274
3.366369	251.519709	5.042278
3.508487	251.709750	5.047283
3.377586	255.893748	5.052288
3.491444	252.377180	5.057293
3.403890	251.312195	5.062298
3.418002	243.888184	5.067302
3.708592	253.201333	5.072307
3.917406	250.100243	5.077312
3.726632	249.288606	5.082317
3.771149	242.565365	5.087322
3.940081	247.642293	5.092326
3.287682	230.017930	5.097331
3.464839	236.862075	5.102336
3.455383	248.708596	5.107341
3.611933	243.828161	5.112346
3.896044	241.237357	5.117350
3.574526	253.714587	5.122355
3.730433	250.976068	5.127360
3.911187	252.985542	5.132365
4.052939	236.547294	5.137370
3.631335	240.438035	5.142374
3.617963	241.898778	5.147379
3.909354	241.467640	5.152384
4.008987	242.825369	5.157389
3.492820	231.367969	5.162394
3.720092	233.145577	5.167398
3.995695	244.356103	5.172403
3.992504	231.243317	5.177408
3.951219	234.518034	5.182413
3.618998	220.178357	5.187418
3.549363	236.001499	5.192422
3.918233	242.860089	5.197427
3.799256	250.414720	5.202432
3.669845	248.188851	5.207437
3.589427	250.425646	5.212442
3.668775	250.343891	5.217446
3.544248	247.351649	5.222451
4.065607	244.584704	5.227456
3.648588	248.091927	5.232461
3.957397	248.831805	5.237466
3.867954	244.685682	5.242470
3.593935	248.971053	5.247475
3.989946	244.629125	5.252480
3.840442	252.795939	5.257485
4.095070	259.017438	5.262490
4.406196	267.128359	5.267494
3.747055	254.411909	5.272499
4.347320	259.940528	5.277504
3.701061	256.181647	5.282509
4.132307	266.890237	5.287514
4.507432	268.527771	5.292518
4.244811	267.591281	5.297523
4.203297	255.892287	5.302528
4.007963	260.554544	5.307533
4.016840	251.812086	5.312538
4.122812	256.136370	5.317542
4.322137	266.871578	5.322547
4.485207	252.593961	5.327552
3.965834	254.620697	5.332557
4.057890	248.412060	5.337562
4.634836	263.716950	5.342566
4.024863	254.684874	5.347571
4.127133	254.197761	5.352576
4.316669	263.504504	5.357581
4.666277	263.453435	5.362586
4.657993	264.381888	5.367590
4.291350	253.511786	5.372595
4.397725	246.101882	5.377600
4.118253	248.644910	5.382605
4.305665	245.483880	5.387610
3.939277	249.321735	5.392614
4.005619	256.819042	5.397619
4.642635	262.364086	5.402624
4.774611	266.766580	5.407629
4.451745	258.360503	5.412634
4.362245	251.113970	5.417638
4.416560	258.445475	5.422643
4.595412	251.827862	5.427648
4.139870	253.506144	5.432653
4.336103	255.848560	5.437658
4.638762	265.675518	5.442662
4.696844	270.617854	5.447667
4.577331	258.883547	5.452672
4.522739	261.337781	5.457677
4.486266	257.344755	5.462682
4.466644	260.375664	5.467686
4.346650	266.535273	5.472691
4.929531	274.471010	5.477696
4.589568	273.467468	5.482701
4.909453	263.632563	5.487706
4.334906	264.551106	5.492710
4.641667	266.601073	5.497715
4.898316	268.139997	5.502720
4.526497	261.620774	5.507725
4.342277	259.915954	5.512730
4.812643	270.403324	5.517734
4.511504	279.843418	5.522739
4.442897	267.889212	5.527744
4.519174	280.595585	5.532749
4.554917	280.704114	5.537754
4.690223	271.587628	5.542758
4.676083	281.872036	5.547763
4.966373	264.353961	5.552768
4.651946	268.433661	5.557773
4.778233	283.356326	5.562778
4.864808	275.895710	5.567782
4.495678	278.142660	5.572787
4.864440	272.147192	5.577792
4.543151	277.949012	5.582797
4.353135	273.046599	5.587802
5.095243	280.169788	5.592806
4.775569	281.883865	5.597811
4.731864	272.209966	5.602816
4.710011	267.914111	5.607821
4.563407	268.136451	5.612826
4.808218	282.205445	5.617830
4.869395	288.245107	5.622835
5.608412	291.910862	5.627840
5.002685	288.955570	5.632845
4.967792	270.017001	5.637850
5.077926	271.806523	5.642854
4.676411	271.094133	5.647859
5.108601	272.415905	5.652864
4.970222	278.265175	5.657869
5.016238	282.048317	5.662874
5.187599	286.340282	5.667878
5.322824	285.101406	5.672883
5.309879	267.491338	5.677888
4.740297	274.337869	5.682893
4.540382	270.158321	5.687898
5.376848	284.897649	5.692902
5.467774	283.523304	5.697907
5.403484	274.937756	5.702912
4.826610	274.078667	5.707917
5.230438	272.538548	5.712922
5.131451	272.047970	5.717926
5.026470	278.616526	5.722931
5.481972	274.252674	5.727936
5.073448	277.268207	5.732941
5.328769	283.394696	5.737946
5.306064	275.656871	5.742950
4.951376	277.097994	5.747955
5.146411	284.410764	5.752960
5.070594	287.520028	5.757965
5.317996	297.051892	5.762970
5.421450	286.481893	5.767974
5.421451	293.347315	5.772979
5.539645	291.234746	5.777984
5.272837	293.952976	5.782989
5.493005	294.725640	5.787994
5.573388	293.647159	5.792998
5.162764	285.858999	5.798003
5.326043	274.166072	5.803008
4.919398	284.998802	5.808013
5.231675	283.735524	5.813018
5.398371	283.855300	5.818022
5.428633	294.284660	5.823027
5.734619	296.388534	5.828032
5.557208	301.424491	5.833037
5.277533	293.869034	5.838042
5.665371	287.661787	5.843046
5.414156	287.270839	5.848051
5.504525	281.866033	5.853056
5.488718	296.342605	5.858061
5.453963	295.130194	5.863066
5.744751	290.121279	5.868070
5.654390	301.312892	5.873075
5.994250	299.757421	5.878080
5.601413	290.473224	5.883085
5.521371	296.028684	5.888090
5.546746	295.012551	5.893094
5.455119	292.875704	5.898099
5.732411	292.997243	5.903104
5.686120	293.425423	5.908109
5.231920	299.700353	5.913114
5.759110	293.208820	5.918118
5.445410	295.617982	5.923123
5.513072	288.688643	5.928128
5.523332	288.538552	5.933133
5.291614	294.380215	5.938138
5.841460	290.586953	5.943142
5.599410	300.587324	5.948147
5.983653	286.781435	5.953152
5.687827	304.882917	5.958157
5.582186	294.766240	5.963162
5.781802	299.990264	5.968166
5.515187	293.964004	5.973171
5.842941	301.828746	5.978176
6.054966	305.813833	5.983181
6.070983	315.584209	5.988186
6.173866	302.726934	5.993190
5.585758	290.252495	5.998195
5.942175	291.374098	6.003200
5.645595	293.622408	6.008205
5.523366	299.105346	6.013210
5.866525	310.884352	6.018214
6.171911	317.831948	6.023219
6.104277	304.789252	6.028224
5.806054	296.819074	6.033229
5.472994	292.938655	6.038234
6.038557	293.720816	6.043238
5.828231	311.647644	6.048243
5.981061	311.421573	6.053248
5.990556	323.948553	6.058253
5.725721	313.717449	6.063258
5.828840	304.460427	6.068262
5.734912	314.213121	6.073267
6.025350	310.333696	6.078272
6.260037	314.005214	6.083277
5.747790	306.485963	6.088282
6.007069	297.195140	6.093286
5.823612	304.035347	6.098291
5.804938	293.810220	6.103296
5.570243	298.959497	6.108301
6.016556	299.902592	6.113306
6.367864	306.314695	6.118310
5.558167	303.204500	6.123315
5.798856	300.443282	6.128320
6.209988	315.593702	6.133325
5.910714	310.796873	6.138330
5.980639	291.411698	6.143334
5.461574	292.384878	6.148339
6.119800	299.027598	6.153344
5.645624	298.744129	6.158349
5.898066	313.628195	6.163354
6.288369	305.708996	6.168358
6.045651	297.967453	6.173363
5.890709	294.075120	6.178368
5.756967	289.148123	6.183373
5.684848	289.146898	6.188378
5.524780	294.863511	6.193382
5.747530	308.904325	6.198387
6.299385	310.311870	6.203392
6.091331	311.261937	6.208397
5.958074	306.436098	6.213402
6.075365	295.841793	6.218406
5.611928	294.870130	6.223411
6.101269	291.633608	6.228416
5.509897	295.759598	6.233421
5.682180	295.422932	6.238426
6.289290	314.064034	6.243430
5.833992	309.032075	6.248435
5.886413	301.719132	6.253440
5.740864	301.330714	6.258445
5.738985	302.739053	6.263450
6.172672	307.287567	6.268454
5.942936	297.803968	6.273459
5.589920	290.753469	6.278464
5.991069	299.290141	6.283469
5.866575	300.087995	6.288474
6.010856	304.314579	6.293478
5.866396	305.605915	6.298483
5.807746	290.885071	6.303488
5.723602	307.646990	6.308493
5.913269	307.478458	6.313498
6.000230	303.959740	6.318502
5.756908	311.574886	6.323507
6.043005	308.018835	6.328512
5.946135	312.937854	6.333517
5.709202	307.561854	6.338522
6.113509	294.350775	6.343526
5.723939	297.822096	6.348531
5.872002	300.915487	6.353536
5.984054	305.729210	6.358541
5.757142	302.170778	6.363546
6.125153	306.897194	6.368550
5.885628	297.703015	6.373555
5.566702	292.773213	6.378560
5.746572	301.268410	6.383565
5.659535	316.100932	6.388570
6.262845	314.264000	6.393574
6.286697	321.223793	6.398579
6.038245	310.591514	6.403584
5.589186	297.794868	6.408589
5.503736	299.165600	6.413594
6.064308	301.356384	6.418598
5.864948	315.997590	6.423603
5.937800	318.406680	6.428608
6.118461	316.104051	6.433613
5.689041	307.540537	6.438618
6.171022	300.375846	6.443622
5.843435	303.337653	6.448627
5.784935	288.531367	6.453632
5.905990	299.557187	6.458637
5.769196	301.805930	6.463642
6.147824	309.090125	6.468646
5.886826	296.115506	6.473651
5.923000	290.004140	6.478656
6.257963	284.953548	6.483661
5.711746	298.006786	6.488666
5.746995	294.818820	6.493670
6.050518	294.132696	6.498675
6.178973	292.717706	6.503680
5.870768	293.139210	6.508685
5.556832	290.448529	6.513690
5.836764	290.218487	6.518694
5.744617	296.838834	6.523699
5.777913	296.912943	6.528704
5.800653	289.591972	6.533709
5.684877	298.243929	6.538714
6.183792	298.792862	6.543718
6.081768	299.444851	6.548723
6.097707	298.654809	6.553728
5.541609	298.463188	6.558733
5.328792	295.867491	6.563738
6.470001	303.621400	6.568742
5.701040	299.198255	6.573747
5.663296	306.964885	6.578752
5.998560	310.313864	6.583757
6.235522	316.506497	6.588762
6.285811	293.312117	6.593766
6.029834	295.158644	6.598771
5.750322	288.776896	6.603776
5.806516	295.994231	6.608781
5.818177	300.545178	6.613786
5.998752	287.909931	6.618790
6.180576	290.998063	6.623795
5.973881	289.015171	6.628800
6.045638	292.329245	6.633805
5.812745	304.163136	6.638810
5.751996	293.852812	6.643814
5.862956	295.063251	6.648819
5.975576	288.667905	6.653824
5.661997	291.263705	6.658829
5.946844	298.565661	6.663834
5.943619	290.663448	6.668838
5.859688	300.784730	6.673843
5.531920	299.608449	6.678848
6.038681	289.608394	6.683853
5.924698	297.032556	6.688858
5.779891	291.730801	6.693862
5.804313	297.763533	6.698867
5.984516	291.661379	6.703872
6.308403	298.688342	6.708877
6.248688	301.314219	6.713882
6.098222	297.041545	6.718886
5.834322	298.016125	6.723891
5.978829	301.148034	6.728896
5.809925	306.745806	6.733901
5.813361	301.167871	6.738906
5.814884	287.842342	6.743910
5.652712	298.409231	6.748915
5.538128	294.175263	6.753920
6.010582	297.063125	6.758925
5.738873	301.866995	6.763930
5.793496	292.937064	6.768934
5.637927	291.585279	6.773939
5.789403	286.993517	6.778944
6.087578	291.860514	6.783949
5.675102	293.133468	6.788954
6.086199	295.277923	6.793958
5.940814	293.060862	6.798963
5.949026	290.576283	6.803968
6.388836	290.166327	6.808973
5.801899	294.639633	6.813978
6.149781	285.610262	6.818982
6.026439	299.107016	6.823987
6.006992	301.144503	6.828992
5.935887	288.826846	6.833997
6.203474	298.070835	6.839002
6.009380	295.535497	6.844006
5.868270	292.055456	6.849011
5.792406	287.113120	6.854016
5.569481	282.228483	6.859021
5.811008	293.007755	6.864026
5.860295	287.033551	6.869030
5.839751	291.693911	6.874035
6.116571	292.331207	6.879040
5.917885	299.623029	6.884045
5.923155	306.879934	6.889050
6.165440	287.638766	6.894054
5.961925	294.728861	6.899059
5.819274	291.973546	6.904064
5.905768	292.390543	6.909069
5.804851	301.761511	6.914074
5.950715	286.104010	6.919078
5.711774	300.817804	6.924083
5.712458	296.243191	6.929088
5.914463	294.547835	6.934093
5.902688	298.814534	6.939098
6.003230	292.569760	6.944102
5.800394	298.087393	6.949107
5.773127	296.475190	6.954112
5.877917	290.520816	6.959117
5.747580	293.572132	6.964122
5.584338	296.850030	6.969126
5.544843	298.688161	6.974131
5.457207	292.213263	6.979136
5.844240	289.543154	6.984141
5.625902	293.487679	6.989146
5.817346	296.836901	6.994150
5.787860	298.376087	6.999155
5.838668	306.078310	7.004160
6.335615	313.135281	7.009165
5.703966	305.438472	7.014170
5.840386	302.453046	7.019174
5.789891	300.142118	7.024179
5.707812	305.058832	7.029184
6.137923	313.970646	7.034189
5.952980	308.137305	7.039194
5.841286	304.766574	7.044198
5.773696	308.782542	7.049203
6.099622	306.371878	7.054208
5.960265	308.174939	7.059213
5.841049	295.415523	7.064218
6.067708	286.635976	7.069222
5.827659	292.849087	7.074227
5.783195	289.192651	7.079232
5.867087	302.315462	7.084237
5.817790	297.821395	7.089242
5.559426	302.942722	7.094246
6.034493	317.320738	7.099251
5.750781	320.196625	7.104256
5.849231	319.849309	7.109261
6.096309	322.528660	7.114266
6.118524	317.545736	7.119270
5.940088	305.769953	7.124275
5.959473	306.017068	7.129280
5.940246	297.111287	7.134285
5.925820	299.609892	7.139290
6.013604	298.302472	7.144294
5.966470	304.915814	7.149299
6.215886	303.349115	7.154304
6.127945	294.482508	7.159309
5.862107	302.120138	7.164314
6.154668	296.993888	7.169318
5.839355	292.557060	7.174323
5.624095	299.775533	7.179328
5.885057	295.903865	7.184333
5.460604	293.913749	7.189338
5.915334	282.520281	7.194342
5.824120	293.490563	7.199347
5.783766	297.046716	7.204352
5.894991	294.511296	7.209357
5.606306	297.688505	7.214362
5.973217	299.254556	7.219366
5.814120	293.812658	7.224371
5.989057	295.456054	7.229376
5.935932	291.117607	7.234381
5.655586	297.548961	7.239386
5.551274	298.277235	7.244390
5.959731	308.486370	7.249395
6.162770	312.653189	7.254400
5.966239	299.130701	7.259405
5.875891	291.650170	7.264410
5.933370	304.014644	7.269414
5.902959	302.260563	7.274419
5.852835	299.421239	7.279424
6.271536	301.362035	7.284429
5.882954	300.714068	7.289434
6.227123	290.109752	7.294438
6.015198	302.446569	7.299443
5.851673	297.286929	7.304448
5.762815	294.969319	7.309453
5.905448	294.561342	7.314458
5.789031	292.279661	7.319462
5.803395	296.352467	7.324467
5.822529	299.459604	7.329472
6.199594	297.866703	7.334477
6.072771	305.893971	7.339482
6.340568	294.570729	7.344486
5.833781	299.066357	7.349491
5.980978	295.747067	7.354496
6.040567	296.389711	7.359501
5.658401	297.914206	7.364506
5.929475	294.610430	7.369510
5.952595	289.744429	7.374515
6.132220	294.443225	7.379520
6.371754	285.848333	7.384525
5.969289	294.320301	7.389530
5.700972	298.342210	7.394534
6.273926	300.417173	7.399539
5.684429	284.504014	7.404544
5.876966	280.525946	7.409549
5.821655	291.490637	7.414554
5.990233	288.060454	7.419558
5.775918	289.745472	7.424563
6.040159	294.750628	7.429568
5.914012	281.919536	7.434573
5.867857	289.791871	7.439578
5.530121	273.614901	7.444582
5.855025	288.465518	7.449587
6.083823	290.195438	7.454592
6.272588	284.544361	7.459597
5.769220	283.275201	7.464602
5.708295	279.532745	7.469606
5.975926	279.472294	7.474611
5.765938	286.433682	7.479616
5.818062	281.003194	7.484621
6.049159	291.423428	7.489626
5.882957	282.401336	7.494630
5.739717	283.825356	7.499635
5.916109	288.774586	7.504640
6.128077	290.086355	7.509645
5.885034	281.281868	7.514650
5.910655	273.558666	7.519654
5.941424	272.899192	7.524659
5.767644	274.960705	7.529664
5.960224	272.396803	7.534669
5.575091	276.212272	7.539674
5.796368	277.123965	7.544678
5.923159	284.393578	7.549683
6.077311	298.457719	7.554688
5.937045	294.360625	7.559693
5.862664	301.886189	7.564698
5.835074	291.915547	7.569702
5.606316	289.050255	7.574707
5.459739	294.362978	7.579712
5.816845	289.176063	7.584717
5.802691	300.131187	7.589722
5.927251	299.646931	7.594726
6.060132	295.380760	7.599731
5.691139	294.780363	7.604736
5.787014	298.511455	7.609741
5.809123	298.239299	7.614746
5.795956	302.291083	7.619750
6.209510	303.593613	7.624755
5.884190	302.236619	7.629760
5.884126	296.586465	7.634765
6.045979	307.678703	7.639770
5.940607	297.666385	7.644774
5.803086	299.440686	7.649779
5.583867	302.575443	7.654784
6.036478	293.491799	7.659789
5.726296	299.798088	7.664794
5.799341	299.033956	7.669798
6.228587	294.459055	7.674803
5.844476	294.942997	7.679808
6.020490	289.929806	7.684813
5.674546	297.029423	7.689818
5.703298	296.117166	7.694822
5.599173	304.830585	7.699827
5.610167	305.142281	7.704832
6.011705	294.896019	7.709837
5.678157	299.494386	7.714842
5.953598	299.030929	7.719846
6.115690	295.070253	7.724851
5.897286	302.573950	7.729856
5.955550	291.507956	7.734861
5.887846	298.966042	7.739866
5.900039	296.664336	7.744870
5.952266	297.456820	7.749875
5.728399	302.386118	7.754880
6.489175	298.329064	7.759885
6.013312	298.846273	7.764890
5.951512	295.569014	7.769894
6.144447	292.508354	7.774899
5.977820	298.697380	7.779904
5.880403	296.352630	7.784909
5.771697	305.009816	7.789914
5.747667	299.281137	7.794918
6.180725	304.228374	7.799923
5.674368	306.363818	7.804928
5.979327	298.948283	7.809933
5.909769	299.826167	7.814938
5.775058	288.265047	7.819942
6.422571	294.042580	7.824947
5.957414	291.581084	7.829952
5.862325	284.151913	7.834957
5.635480	287.319491	7.839962
5.645572	291.364489	7.844966
5.972538	296.087801	7.849971
5.904202	295.165350	7.854976
6.042839	294.821269	7.859981
5.803541	295.674962	7.864986
5.897576	293.654738	7.869990
6.058579	298.302652	7.874995
5.843711	301.522151	7.880000
6.083928	292.202662	7.885005
5.613105	301.074412	7.890010
5.822917	294.265305	7.895014
5.439989	301.389664	7.900019
5.685918	301.006731	7.905024
5.838973	291.542628	7.910029
5.862857	299.723596	7.915034
5.803026	295.509576	7.920038
6.070598	296.423553	7.925043
5.752791	290.544467	7.930048
5.692065	291.762655	7.935053
5.251871	303.894573	7.940058
5.622920	294.396527	7.945062
5.562457	292.302283	7.950067
5.355452	301.873263	7.955072
6.060315	306.759199	7.960077
6.091884	320.576693	7.965082
5.950088	306.466721	7.970086
5.918910	312.245528	7.975091
5.688974	308.950153	7.980096
6.095796	302.926604	7.985101
6.252175	306.104120	7.990106
6.084731	303.425429	7.995110
6.214662	296.486392	8.000115
5.775087	298.570430	8.005133
6.129573	300.462461	8.010150
6.117216	301.468076	8.015168
5.699170	285.212467	8.020186
5.924320	295.859406	8.025203
5.738185	301.505605	8.030221
5.894317	298.398449	8.035238
5.263282	301.071893	8.040256
5.394085	298.596651	8.045274
5.809636	304.919142	8.050291
6.131147	315.039879	8.055309
6.078588	323.760960	8.060326
6.198762	315.607234	8.065344
5.845881	313.967805	8.070362
6.175443	299.861524	8.075379
5.716685	308.163031	8.080397
5.724782	305.457598	8.085414
6.290348	312.337371	8.090432
5.859167	308.453858	8.095450
6.163338	298.097264	8.100467
5.804331	304.862227	8.105485
6.216068	311.119047	8.110502
6.266257	309.959629	8.115520
6.202806	303.052571	8.120538
5.657476	294.866780	8.125555
5.556263	294.857495	8.130573
5.935904	304.375917	8.135590
5.757426	325.922149	8.140608
6.496572	321.928996	8.145626
6.395710	328.486526	8.150643
6.204325	308.929525	8.155661
6.312067	301.910612	8.160678
6.313933	302.689963	8.165696
6.106508	294.262223	8.170714
6.079603	289.728823	8.175731
5.993247	294.210836	8.180749
6.105295	287.771893	8.185766
5.990204	297.348406	8.190784
5.999071	305.075359	8.195802
6.451757	295.068007	8.200819
5.916820	294.955848	8.205837
5.805943	298.883135	8.210854
6.272681	299.252454	8.215872
6.166295	300.395778	8.220890
6.065767	292.816038	8.225907
6.005812	298.584593	8.230925
6.058204	298.365210	8.235942
6.032483	282.698578	8.240960
5.812569	298.394390	8.245978
6.110007	299.793559	8.250995
6.151510	302.109840	8.256013
6.319415	306.243017	8.261030
6.170232	299.769008	8.266048
5.947611	297.790581	8.271066
6.261601	303.283177	8.276083
6.347874	305.851250	8.281101
6.066298	298.640503	8.286118
6.073032	305.288564	8.291136
6.087916	312.099451	8.296154
6.676861	318.830428	8.301171
6.015112	312.161679	8.306189
6.102668	305.748632	8.311206
6.404815	315.689358	8.316224
6.401917	315.734189	8.321242
6.600583	304.737647	8.326259
6.322742	300.959642	8.331277
6.186909	302.205375	8.336294
6.522684	295.128871	8.341312
6.309040	306.194411	8.346330
6.387632	307.447783	8.351347
6.149927	305.919802	8.356365
5.982368	304.557616	8.361382
6.056211	307.399008	8.366400
6.170900	303.802870	8.371418
6.454537	301.590993	8.376435
6.311436	297.063060	8.381453
6.119744	304.628747	8.386470
6.630206	301.355975	8.391488
6.446432	302.492415	8.396506
6.198865	294.178216	8.401523
6.201513	303.868937	8.406541
6.133855	299.389214	8.411558
6.617549	291.929939	8.416576
6.351247	290.299121	8.421594
6.548749	294.673826	8.426611
6.306960	308.580658	8.431629
6.190856	300.085051	8.436646
6.405937	295.810602	8.441664
6.052057	300.015551	8.446682
6.197606	293.063334	8.451699
6.203803	302.497896	8.456717
6.170680	289.663009	8.461734
6.296002	296.655500	8.466752
6.290876	292.604675	8.471770
6.201981	291.476380	8.476787
6.441692	303.572645	8.481805
6.320581	313.216372	8.486822
6.769940	318.627939	8.491840
6.381681	308.215056	8.496858
6.213034	302.615030	8.501875
6.476153	308.301730	8.506893
6.206854	307.321437	8.511910
6.528939	312.872732	8.516928
6.734022	314.270503	8.521946
6.069113	305.371219	8.526963
6.732943	308.347957	8.531981
6.188024	307.035058	8.536998
6.361644	308.503995	8.542016
6.514531	321.935999	8.547034
6.656672	316.454828	8.552051
6.635779	317.856227	8.557069
6.217957	306.494947	8.562087
6.481790	313.106137	8.567104
6.627557	324.743699	8.572122
6.755508	309.589574	8.577139
6.654209	306.544588	8.582157
6.317194	310.156811	8.587175
6.321482	297.114133	8.592192
6.466703	311.768552	8.597210
6.578463	309.753839	8.602227
6.706468	307.316898	8.607245
6.139349	306.578624	8.612263
6.381036	308.737513	8.617280
6.384739	313.751433	8.622298
6.685912	319.227096	8.627315
6.651302	324.758197	8.632333
6.489328	322.915483	8.637351
6.871622	313.234644	8.642368
6.461514	322.787680	8.647386
6.749355	322.645241	8.652403
6.580529	323.388056	8.657421
6.434056	319.403411	8.662439
6.766982	315.460884	8.667456
6.526079	322.037061	8.672474
6.793101	326.760692	8.677491
6.715977	319.833667	8.682509
6.435494	305.519423	8.687527
6.849254	308.585587	8.692544
6.460478	309.681366	8.697562
6.494696	309.464813	8.702579
6.458805	314.566944	8.707597
6.544317	327.207913	8.712615
6.971648	313.610234	8.717632
6.834341	317.588974	8.722650
6.601250	309.184157	8.727667
6.994978	311.909476	8.732685
6.431560	295.856362	8.737703
6.704109	294.656013	8.742720
6.932350	301.474701	8.747738
6.550924	294.071231	8.752755
6.236201	298.210126	8.757773
6.375474	315.781274	8.762791
6.538485	316.232595	8.767808
6.784735	318.245615	8.772826
6.756018	320.544432	8.777843
6.766413	313.673207	8.782861
6.839593	310.143487	8.787879
6.681468	306.375242	8.792896
6.588473	316.866613	8.797914
6.501061	319.398617	8.802931
6.736213	311.753982	8.807949
6.567462	324.106351	8.812967
7.036917	310.918658	8.817984
6.788893	330.026955	8.823002
6.899139	323.130714	8.828019
6.650096	324.608658	8.833037
6.782393	315.941832	8.838055
6.746629	313.946932	8.843072
6.875212	328.099054	8.848090
6.800468	317.053560	8.853107
6.555272	314.472764	8.858125
6.634223	317.146115	8.863143
6.941193	313.592616	8.868160
7.231342	324.655463	8.873178
6.876271	324.827707	8.878195
6.859569	314.426393	8.883213
6.829361	321.843874	8.888231
7.003138	312.952853	8.893248
6.537810	321.776068	8.898266
6.854664	325.390624	8.903283
6.653259	320.101789	8.908301
6.538354	330.801696	8.913319
6.675867	323.885430	8.918336
6.945109	325.453083	8.923354
6.803835	323.256871	8.928371
6.899362	317.363259	8.933389
6.711661	329.134790	8.938407
6.773248	325.916124	8.943424
7.164582	333.217487	8.948442
6.981339	339.491219	8.953459
6.844266	327.183702	8.958477
6.681924	331.847960	8.963495
7.040873	339.353173	8.968512
7.134185	345.801586	8.973530
7.108175	335.632071	8.978547
6.891591	335.258917	8.983565
6.841757	325.487571	8.988583
7.166618	334.683197	8.993600
6.749703	334.975516	8.998618
6.799726	338.208765	9.003635
7.367952	339.133454	9.008653
6.794491	340.384215	9.013671
7.030007	339.921737	9.018688
7.204344	349.150273	9.023706
7.091754	341.537678	9.028723
7.114676	337.403585	9.033741
6.958307	332.473787	9.038759
6.757525	322.303090	9.043776
7.121522	335.320405	9.048794
7.179914	339.347570	9.053811
7.178691	347.587326	9.058829
6.961927	329.829810	9.063847
6.916960	334.270677	9.068864
7.399890	334.968818	9.073882
7.302313	330.894511	9.078899
6.821333	327.406891	9.083917
6.768252	338.882928	9.088935
7.269362	341.275970	9.093952
6.993900	350.053860	9.098970
7.303689	344.925254	9.103987
7.363796	334.833844	9.109005
7.337362	336.627406	9.114023
7.231397	331.797052	9.119040
6.980706	323.316078	9.124058
6.803193	319.841167	9.129075
6.981996	329.330915	9.134093
7.032450	339.613782	9.139111
7.456366	339.260818	9.144128
7.406971	352.342509	9.149146
7.158358	344.621709	9.154163
6.803802	335.853960	9.159181
7.005659	349.903176	9.164199
7.303486	341.548218	9.169216
7.301838	344.224655	9.174234
7.119171	349.772504	9.179251
7.546183	351.994057	9.184269
7.285794	357.348894	9.189287
7.600723	346.217465	9.194304
7.697325	340.740221	9.199322
7.112241	327.823997	9.204339
7.023535	330.378294	9.209357
7.056513	326.230015	9.214375
7.168616	324.811662	9.219392
6.981335	325.267033	9.224410
7.048045	342.802170	9.229427
7.194302	348.330363	9.234445
7.467609	346.470365	9.239463
7.353153	354.775088	9.244480
7.356315	348.043824	9.249498
7.251460	353.822544	9.254515
7.768022	349.684169	9.259533
7.321060	349.564623	9.264551
7.241505	338.949031	9.269568
7.061916	327.866208	9.274586
7.343041	348.425776	9.279603
7.629298	348.886309	9.284621
7.466449	343.660888	9.289639
7.502606	334.649279	9.294656
7.458847	330.901090	9.299674
7.200661	335.485602	9.304691
7.000528	330.430083	9.309709
7.403538	348.585015	9.314727
7.763871	350.974731	9.319744
7.507529	337.332010	9.324762
7.178018	335.341820	9.329779
7.445558	342.451034	9.334797
7.814134	339.257148	9.339815
7.464744	336.831420	9.344832
7.498788	335.040232	9.349850
6.798066	331.059833	9.354867
7.656443	337.890871	9.359885
7.614633	346.704959	9.364903
7.582277	330.199919	9.369920
7.440733	331.534902	9.374938
7.103394	329.593266	9.379955
7.315289	341.312056	9.384973
7.594645	351.300529	9.389991
7.629341	348.417388	9.395008
7.231717	352.455600	9.400026
7.644812	352.151655	9.405043
7.622048	347.888981	9.410061
7.510986	346.839869	9.415079
7.155440	352.023337	9.420096
7.481614	354.102809	9.425114
7.380042	353.314137	9.430131
7.390613	349.724734	9.435149
7.515812	351.617758	9.440167
7.616348	345.543485	9.445184
8.130601	346.239905	9.450202
7.675606	354.487202	9.455219
7.640314	347.916551	9.460237
7.358351	353.874316	9.465255
7.658019	350.388216	9.470272
7.758205	351.000791	9.475290
7.202145	347.165113	9.480307
7.786319	346.124514	9.485325
7.443431	345.660578	9.490343
7.634571	348.007213	9.495360
7.536148	338.353872	9.500378
7.761285	348.603236	9.505395
7.646574	350.789219	9.510413
7.439004	352.910770	9.515431
7.711733	347.933093	9.520448
7.745779	339.294176	9.525466
7.465213	343.743327	9.530483
7.822860	347.013883	9.535501
8.094957	342.017372	9.540519
7.530800	355.229702	9.545536
7.781810	352.215056	9.550554
7.513973	355.362106	9.555571
7.758263	352.746117	9.560589
7.901927	352.556701	9.565607
7.658121	351.897467	9.570624
7.622913	349.432287	9.575642
7.595680	359.023554	9.580659
7.868975	347.570421	9.585677
7.588978	347.030424	9.590695
7.875690	349.788190	9.595712
7.642710	349.711063	9.600730
7.655263	351.350241	9.605747
7.611782	352.603688	9.610765
7.943690	351.340448	9.615783
7.391266	349.211404	9.620800
7.427100	355.384763	9.625818
7.715511	352.607278	9.630835
7.616220	349.820733	9.635853
7.928885	349.844833	9.640871
7.633568	354.504555	9.645888
7.855522	345.678596	9.650906
7.498659	350.502526	9.655923
7.850277	347.446971	9.660941
8.231332	358.419950	9.665959
7.790914	360.817584	9.670976
7.879349	353.290444	9.675994
7.628554	357.842254	9.681011
8.011182	364.599061	9.686029
8.042072	352.227508	9.691047
7.722929	351.305463	9.696064
7.966573	347.414697	9.701082
7.599772	352.874458	9.706099
7.658510	366.043459	9.711117
8.137197	366.253138	9.716135
7.790391	366.354670	9.721152
7.996559	372.211196	9.726170
8.328996	368.394959	9.731187
8.236521	366.942186	9.736205
7.869544	357.144466	9.741223
7.860684	358.424080	9.746240
7.873296	357.380957	9.751258
8.050404	368.978956	9.756275
8.375981	369.262964	9.761293
8.306996	357.815782	9.766311
8.070720	360.692845	9.771328
7.834738	360.846547	9.776346
7.791441	359.379806	9.781363
7.871419	348.669945	9.786381
7.622875	349.576645	9.791399
7.991573	368.159794	9.796416
7.805087	372.152515	9.801434
7.777758	374.668861	9.806451
7.897472	371.712522	9.811469
8.122171	363.810729	9.816487
8.006138	375.908786	9.821504
8.078606	372.735752	9.826522
7.667688	373.431061	9.831539
7.871731	377.978328	9.836557
8.259627	362.442877	9.841575
8.184155	373.161914	9.846592
8.021751	376.879501	9.851610
8.177528	370.424253	9.856627
7.852186	377.411207	9.861645
8.111517	364.808428	9.866663
8.189735	375.790701	9.871680
7.921823	369.467689	9.876698
8.013858	372.056963	9.881715
7.840357	377.445612	9.886733
8.002987	381.014768	9.891751
8.110144	394.835781	9.896768
8.425573	397.671130	9.901786
8.591272	395.957262	9.906803
8.046206	391.936836	9.911821
8.376749	376.088427	9.916839
8.240266	375.639688	9.921856
8.098351	378.571486	9.926874
8.229705	376.279174	9.931891
8.076283	381.061970	9.936909
8.489718	381.578439	9.941927
8.422002	390.254579	9.946944
8.545284	381.658548	9.951962
8.668687	375.602794	9.956979
8.455786	379.403979	9.961997
8.025611	372.219495	9.967015
8.113299	375.592046	9.972032
8.179008	374.606923	9.977050
8.373483	370.070591	9.982067
8.293375	372.746626	9.987085
8.110681	364.024683	9.992103
7.970951	378.193375	9.997120
8.590730	389.324854	10.002138
8.354115	371.074952	10.007155
7.801602	377.885848	10.012173
8.382478	378.313134	10.017191
8.574796	395.623650	10.022208
8.768606	390.708739	10.027226
8.796695	385.434643	10.032243
8.192886	376.396428	10.037261
8.221651	361.219835	10.042279
7.840609	369.717542	10.047296
8.011842	383.446523	10.052314
8.572030	381.851107	10.057331
8.582876	389.470497	10.062349
8.517417	383.582994	10.067367
8.524131	390.060685	10.072384
8.298271	392.630034	10.077402
8.786288	395.346998	10.082419
8.760114	396.834427	10.087437
9.029299	386.546342	10.092455
8.659236	387.408850	10.097472
8.326677	376.116297	10.102490
8.311009	377.971299	10.107507
8.149174	376.276873	10.112525
8.666573	372.819981	10.117543
8.313342	382.562999	10.122560
8.432457	387.432745	10.127578
8.763221	398.082236	10.132595
8.571140	392.097685	10.137613
8.673835	395.389012	10.142631
8.583975	379.725970	10.147648
8.216060	378.003673	10.152666
8.530879	379.280227	10.157683
8.474514	386.206372	10.162701
8.592959	392.843384	10.167719
8.800937	394.013504	10.172736
8.907753	397.613443	10.177754
9.139420	399.079662	10.182771
8.508355	385.334309	10.187789
8.525336	375.763960	10.192807
8.168103	377.265065	10.197824
8.203222	394.701036	10.202842
8.859199	389.452249	10.207859
8.678224	397.814684	10.212877
8.938938	395.489606	10.217895
8.679767	398.619536	10.222912
8.696220	402.293502	10.227930
8.755938	395.332520	10.232947
8.880319	401.428995	10.237965
8.782028	391.939698	10.242983
8.632078	390.202397	10.248000
8.684379	399.143863	10.253018
8.595686	397.397024	10.258035
8.492200	394.876199	10.263053
8.674582	400.417718	10.268071
8.875748	397.253042	10.273088
8.752907	405.436025	10.278106
8.765412	394.771354	10.283123
8.556599	398.521416	10.288141
8.639895	394.857568	10.293159
8.694596	397.503149	10.298176
8.617870	394.268138	10.303194
8.584500	387.914914	10.308211
8.624135	399.098858	10.313229
8.574481	389.822885	10.318247
8.634142	394.948030	10.323264
8.646428	394.129006	10.328282
9.081429	391.492785	10.333299
8.535245	394.623222	10.338317
8.609411	394.469872	10.343335
9.275258	415.231535	10.348352
8.698196	404.649185	10.353370
9.053802	401.959056	10.358387
8.955422	405.259602	10.363405
8.876837	405.101634	10.368423
8.802398	401.784219	10.373440
8.747961	406.990245	10.378458
9.236039	407.236330	10.383475
8.747882	406.763453	10.388493
8.921415	407.342520	10.393511
8.891885	417.038313	10.398528
8.910059	418.124383	10.403546
9.309268	422.082725	10.408563
9.243705	407.211099	10.413581
8.979178	399.032030	10.418599
8.998177	402.958051	10.423616
8.451951	399.117676	10.428634
9.056908	405.902995	10.433651
8.835629	415.130049	10.438669
9.208862	428.067102	10.443687
9.020570	417.285365	10.448704
9.314684	426.195506	10.453722
9.135262	413.279172	10.458739
8.878735	406.843926	10.463757
9.240582	407.920666	10.468775
9.339602	402.313645	10.473792
9.144529	402.527246	10.478810
8.533826	397.229535	10.483827
8.642389	408.879256	10.488845
9.385831	409.139227	10.493863
9.148624	413.023095	10.498880
9.250193	418.138566	10.503898
9.587455	416.861865	10.508915
9.211138	410.132860	10.513933
9.015172	402.085118	10.518951
9.206940	400.613331	10.523968
8.883694	408.963211	10.528986
9.316734	406.617612	10.534003
9.145331	411.870252	10.539021
9.430579	416.919256	10.544039
9.273861	407.981820	10.549056
9.210902	406.073190	10.554074
8.802018	397.137153	10.559091
9.136169	423.245642	10.564109
9.256834	417.534266	10.569127
9.298017	412.153986	10.574144
9.240514	420.500363	10.579162
9.162128	413.958488	10.584179
9.546454	417.111300	10.589197
9.497642	410.855141	10.594215
9.594435	407.564710	10.599232
8.873750	408.649059	10.604250
9.286001	411.324176	10.609267
9.322056	414.916202	10.614285
9.540677	416.393920	10.619303
9.473635	416.025882	10.624320
9.262083	410.287342	10.629338
9.291410	408.951294	10.634355
9.231423	409.651922	10.639373
9.120482	406.220275	10.644391
9.285442	416.034101	10.649408
9.605840	420.478060	10.654426
9.320850	410.680168	10.659443
9.226920	422.184709	10.664461
9.353812	417.488482	10.669479
9.182539	420.342811	10.674496
9.238030	426.538380	10.679514
9.231558	415.131918	10.684531
8.968171	421.348732	10.689549
9.250738	423.422379	10.694567
9.257565	416.630561	10.699584
8.958377	426.037000	10.704602
9.558013	428.499917	10.709619
9.413313	435.076934	10.714637
9.344832	448.489855	10.719655
9.388865	435.699651	10.724672
9.498371	440.334234	10.729690
9.480780	431.283610	10.734707
9.797678	436.315070	10.739725
9.724081	444.780723	10.744743
10.218670	429.228601	10.749760
9.649116	428.850444	10.754778
9.839557	412.932302	10.759795
9.521626	422.407926	10.764813
9.274875	418.868040	10.769831
9.832991	409.879262	10.774848
9.396117	416.728970	10.779866
9.845387	407.791852	10.784883
9.592732	414.350958	10.789901
9.283987	411.868401	10.794919
9.679545	408.165399	10.799936
9.614281	414.288250	10.804954
9.406488	407.444649	10.809971
9.543616	412.207461	10.814989
9.250297	426.122407	10.820007
9.884867	434.831229	10.825024
10.085092	442.102435	10.830042
9.726084	437.526035	10.835059
9.759338	419.568564	10.840077
9.380771	419.264808	10.845095
9.704955	421.909459	10.850112
9.725125	446.583713	10.855130
10.011630	439.928214	10.860147
9.979039	422.394382	10.865165
9.450010	419.217167	10.870183
9.744662	411.657893	10.875200
9.814838	426.967843	10.880218
10.078808	434.595176	10.885235
10.090281	413.381315	10.890253
9.474737	425.882210	10.895271
9.818718	418.438325	10.900288
9.576744	427.577093	10.905306
9.591053	425.277754	10.910323
9.907207	434.364339	10.915341
10.005059	449.051491	10.920359
9.913648	437.131245	10.925376
9.535884	436.502332	10.930394
9.774208	438.339884	10.935411
10.150558	443.977441	10.940429
9.924332	463.738864	10.945447
10.234174	447.395021	10.950464
9.929106	434.564502	10.955482
9.661450	433.924756	10.960499
10.188429	430.769304	10.965517
9.914422	426.583596	10.970535
9.965601	418.528924	10.975552
9.690513	426.338008	10.980570
9.987186	432.268821	10.985587
10.078256	436.363501	10.990605
9.855162	449.431284	10.995623
10.185770	449.279029	11.000640
9.901775	449.247712	11.005658
9.865333	458.657439	11.010675
10.311917	452.743835	11.015693
9.720511	446.471162	11.020711
9.622234	452.987313	11.025728
10.024014	447.528789	11.030746
10.074560	451.430976	11.035763
10.230380	438.478206	11.040781
9.842903	443.805520	11.045799
9.957810	443.197724	11.050816
10.255776	445.474093	11.055834
10.166878	451.616416	11.060851
10.074250	448.544809	11.065869
10.016665	452.564813	11.070887
10.163992	445.053709	11.075904
10.262440	445.294191	11.080922
10.397777	451.287997	11.085939
10.385244	446.872234	11.090957
10.124350	451.734895	11.095975
10.537525	444.226579	11.100992
10.164357	443.811534	11.106010
10.228911	443.426161	11.111027
10.650243	440.984556	11.116045
9.974215	431.638836	11.121063
10.201567	425.061976	11.126080
9.921386	422.748531	11.131098
10.252380	441.706839	11.136115
10.702248	437.992219	11.141133
9.823641	438.930752	11.146151
10.126849	437.564683	11.151168
10.247291	443.204216	11.156186
10.415886	444.894843	11.161203
10.297907	439.504625	11.166221
10.127556	456.761219	11.171239
10.117202	450.552704	11.176256
9.808036	441.001544	11.181274
9.773246	440.694753	11.186291
10.189779	441.434792	11.191309
10.054122	445.744648	11.196327
10.179084	444.267481	11.201344
10.249384	449.280537	11.206362
10.458297	456.493595	11.211379
10.882416	444.843355	11.216397
10.386848	445.289926	11.221415
10.477815	439.756728	11.226432
10.579204	433.688603	11.231450
10.497323	441.189915	11.236467
10.631985	434.851535	11.241485
10.142961	445.300505	11.246503
10.406926	439.898154	11.251520
10.172497	442.071232	11.256538
9.986102	437.540537	11.261555
10.470625	454.307021	11.266573
10.507416	459.849137	11.271591
10.633521	464.424340	11.276608
10.663516	474.366504	11.281626
10.509598	474.576853	11.286643
10.500710	463.940717	11.291661
10.747961	474.436007	11.296679
10.492513	460.922433	11.301696
10.398950	458.223338	11.306714
10.194532	469.429546	11.311731
10.821505	469.818101	11.316749
10.589691	472.533549	11.321767
10.538518	472.708968	11.326784
10.639027	475.028707	11.331802
10.460533	472.440659	11.336819
10.728460	477.927859	11.341837
10.525380	474.056129	11.346855
10.444150	472.345988	11.351872
10.757165	477.450645	11.356890
10.201158	473.280431	11.361907
10.472891	463.458942	11.366925
10.278288	475.985847	11.371943
10.609230	471.746963	11.376960
10.780271	470.041724	11.381978
10.569360	469.860179	11.386995
10.822557	466.968244	11.392013
10.516147	479.054989	11.397031
10.592703	473.694429	11.402048
10.871116	464.196932	11.407066
10.662313	474.337215	11.412083
10.858111	465.663585	11.417101
10.831667	464.269947	11.422119
10.740968	463.750964	11.427136
10.699464	467.250940	11.432154
10.607562	477.262575	11.437171
10.929517	471.756515	11.442189
11.032342	489.327198	11.447207
11.071727	483.268710	11.452224
10.890077	472.880363	11.457242
10.915692	467.638184	11.462259
10.782254	462.591177	11.467277
10.244092	470.621113	11.472295
11.001062	479.112093	11.477312
10.986156	487.139458	11.482330
10.890029	487.643754	11.487347
11.429968	487.010803	11.492365
11.322248	483.761668	11.497383
10.833658	472.389210	11.502400
11.001603	468.753191	11.507418
10.559386	471.744383	11.512435
10.709489	465.738087	11.517453
11.318975	487.849765	11.522471
11.063592	484.039823	11.527488
11.195305	461.791060	11.532506
10.685850	471.624719	11.537523
10.648487	482.022322	11.542541
11.030097	490.398189	11.547559
11.124872	488.364011	11.552576
11.537861	491.067426	11.557594
11.307812	492.602384	11.562611
11.295368	480.953824	11.567629
10.768935	485.832593	11.572647
10.699188	476.976250	11.577664
10.927576	486.287956	11.582682
11.005435	496.279482	11.587699
11.459512	493.129058	11.592717
11.231830	490.785340	11.597735
11.038708	495.432344	11.602752
10.989646	496.942279	11.607770
10.854349	503.738754	11.612787
11.168542	499.433047	11.617805
10.967810	501.127536	11.622823
10.987193	491.458926	11.627840
11.356945	494.049158	11.632858
11.402286	496.601542	11.637875
11.683808	493.074060	11.642893
11.395958	493.693410	11.647911
11.185842	501.328317	11.652928
11.405141	501.026142	11.657946
11.299758	494.813474	11.662963
11.509146	493.383116	11.667981
11.355484	497.143546	11.672999
11.282131	497.208814	11.678016
11.379379	489.374144	11.683034
11.316872	487.203516	11.688051
11.376170	494.338902	11.693069
11.372082	492.701952	11.698087
10.919755	501.160330	11.703104
11.267398	496.871505	11.708122
10.988959	495.132109	11.713139
10.994312	497.062743	11.718157
11.127369	493.078716	11.723175
11.354796	495.975117	11.728192
11.753330	488.891921	11.733210
11.559203	484.217257	11.738227
11.512106	487.569792	11.743245
11.571466	493.726913	11.748263
11.091167	490.570498	11.753280
11.303982	494.684105	11.758298
11.300401	492.460122	11.763315
11.184627	492.920142	11.768333
11.569497	495.419662	11.773351
11.584878	493.113835	11.778368
11.773258	490.298257	11.783386
11.470838	501.885801	11.788403
11.476008	496.056689	11.793421
11.815752	492.602189	11.798439
11.765511	497.968527	11.803456
11.486108	487.892024	11.808474
11.244262	491.214923	11.813491
11.411083	493.675812	11.818509
11.624905	503.687197	11.823527
11.777316	517.008975	11.828544
11.975102	499.871524	11.833562
11.458489	493.659770	11.838579
11.634596	503.418262	11.843597
11.663853	490.248485	11.848615
11.626783	499.203915	11.853632
11.812947	507.449281	11.858650
11.675353	501.733909	11.863667
11.862661	504.055916	11.868685
11.864212	501.616548	11.873703
11.807888	491.783008	11.878720
11.823677	489.729571	11.883738
11.865084	490.102005	11.888755
11.759411	484.470027	11.893773
12.025591	487.256257	11.898791
11.807145	488.887234	11.903808
11.534074	481.753980	11.908826
11.812114	495.453795	11.913843
11.708199	490.367470	11.918861
11.460935	493.407204	11.923879
11.797357	511.563204	11.928896
12.191375	510.306060	11.933914
11.978480	503.400103	11.938931
11.806229	501.792490	11.943949
12.022188	489.786485	11.948967
11.805104	486.983546	11.953984
11.956824	476.887259	11.959002
12.127605	486.182689	11.964019
11.549470	491.198891	11.969037
12.100643	505.086551	11.974055
12.063817	508.421712	11.979072
11.940746	496.323328	11.984090
11.974166	504.545139	11.989107
11.793898	514.696780	11.994125
12.253534	518.819298	11.999143
12.031974	511.498139	12.004160
11.864131	494.660607	12.009178
12.128665	510.571500	12.014195
12.108660	514.901233	12.019213
12.149199	512.948077	12.024231
12.040734	512.684312	12.029248
12.486176	506.499481	12.034266
12.116499	502.729420	12.039283
11.689218	495.727463	12.044301
12.007728	502.030422	12.049319
11.848870	516.823868	12.054336
12.137314	512.493765	12.059354
12.094911	516.508264	12.064371
12.197999	522.223105	12.069389
12.494752	516.670465	12.074407
12.075366	514.186186	12.079424
12.240217	523.368955	12.084442
12.262951	520.680144	12.089459
12.229655	517.170117	12.094477
12.185162	523.012074	12.099495
12.372273	524.658801	12.104512
12.355634	517.766462	12.109530
12.364462	521.296479	12.114547
12.140962	520.208062	12.119565
12.098433	518.914750	12.124583
12.197663	517.807641	12.129600
11.932377	510.496446	12.134618
12.192720	520.465885	12.139635
12.026906	523.729617	12.144653
12.130477	518.216521	12.149671
11.999478	520.048471	12.154688
11.722233	515.920048	12.159706
12.132707	518.952049	12.164723
12.035775	531.539521	12.169741
12.322478	531.763316	12.174759
12.344788	542.751241	12.179776
12.462748	536.251330	12.184794
12.522444	538.744683	12.189811
12.630471	540.567820	12.194829
12.789496	534.891457	12.199847
12.768888	538.072627	12.204864
12.271137	524.278008	12.209882
12.664351	525.485565	12.214899
12.362604	526.103923	12.219917
12.621129	531.371707	12.224935
12.606627	519.991673	12.229952
12.379539	517.739373	12.234970
12.653084	523.112109	12.239987
12.153870	538.113192	12.245005
12.674446	539.865786	12.250023
12.858195	544.391010	12.255040
12.753132	535.827303	12.260058
12.432624	523.939513	12.265075
12.350574	535.625306	12.270093
12.890564	545.800517	12.275111
12.725826	544.131772	12.280128
12.776111	548.128691	12.285146
12.968370	545.467128	12.290163
12.562507	538.171498	12.295181
12.506917	524.945480	12.300199
12.564255	522.317551	12.305216
12.658567	552.427090	12.310234
12.845257	543.799019	12.315251
12.675023	554.192107	12.320269
12.941822	544.838382	12.325287
12.518877	550.325878	12.330304
12.678860	551.071154	12.335322
13.145594	550.408576	12.340339
12.648825	552.177563	12.345357
12.766611	555.861029	12.350375
12.948748	548.858837	12.355392
12.898106	540.488617	12.360410
13.029465	551.661531	12.365427
12.599191	552.994150	12.370445
12.920376	550.956270	12.375463
12.878870	555.314606	12.380480
12.516335	552.010462	12.385498
12.793142	548.294363	12.390515
12.855607	541.828336	12.395533
12.750516	550.210584	12.400551
12.801914	541.505753	12.405568
13.072347	539.422131	12.410586
12.859862	538.748545	12.415603
13.119374	540.548097	12.420621
13.005784	537.921533	12.425639
12.968307	535.930030	12.430656
12.579527	541.503719	12.435674
13.028477	543.696636	12.440691
13.054196	543.162680	12.445709
12.969193	544.078638	12.450727
13.158853	551.534563	12.455744
12.998512	553.042895	12.460762
12.884775	536.386239	12.465779
12.955109	537.057115	12.470797
13.020192	537.113452	12.475815
13.460039	544.044447	12.480832
13.029096	546.071416	12.485850
13.217172	543.438906	12.490867
13.542983	543.057035	12.495885
13.232170	547.479389	12.500903
13.289508	536.728760	12.505920
13.175410	543.241095	12.510938
12.941982	536.565531	12.515955
12.546160	548.098223	12.520973
12.832283	543.493931	12.525991
12.817433	558.463797	12.531008
12.956743	559.508926	12.536026
13.385879	562.847284	12.541043
13.045305	566.930308	12.546061
13.066484	565.857438	12.551079
13.318950	569.349532	12.556096
12.914080	568.617540	12.561114
13.739568	568.795316	12.566131
13.233661	576.223854	12.571149
13.282414	562.760665	12.576167
13.304951	567.737012	12.581184
13.262287	570.561874	12.586202
13.643094	562.380078	12.591219
13.380315	569.079667	12.596237
12.982150	563.704634	12.601255
13.260013	567.284287	12.606272
13.093579	572.640338	12.611290
13.463692	577.082908	12.616307
13.684080	591.924662	12.621325
13.433423	592.765432	12.626343
13.759772	587.246030	12.631360
13.696201	581.001576	12.636378
13.551271	574.135500	12.641395
13.392259	569.351210	12.646413
13.205732	572.135357	12.651431
13.714213	576.704701	12.656448
13.764480	593.138158	12.661466
13.888079	586.908740	12.666483
13.458477	579.623100	12.671501
13.192791	574.606118	12.676519
13.581528	577.931835	12.681536
13.711233	593.055941	12.686554
14.098833	595.447757	12.691571
13.848107	587.234895	12.696589
13.725918	575.934706	12.701607
13.893850	577.246767	12.706624
13.770232	575.432768	12.711642
13.594254	565.242291	12.716659
13.602111	561.094713	12.721677
13.489782	567.490022	12.726695
13.773811	563.230020	12.731712
13.627634	577.885848	12.736730
13.639193	586.003808	12.741747
13.860150	585.597237	12.746765
13.956889	595.459652	12.751783
13.927962	587.912816	12.756800
13.911237	597.868635	12.761818
13.863539	584.035454	12.766835
14.025674	589.886285	12.771853
13.837795	581.903471	12.776871
14.092017	571.623920	12.781888
13.760813	567.226187	12.786906
13.845407	558.620317	12.791923
13.572580	564.463125	12.796941
13.717033	576.388223	12.801959
14.221043	583.489117	12.806976
14.009469	593.819240	12.811994
14.312958	594.040421	12.817011
14.076899	597.327727	12.822029
13.919139	585.335665	12.827047
14.162364	576.525214	12.832064
13.763373	575.148548	12.837082
13.908290	576.524151	12.842099
13.731326	580.278760	12.847117
14.042261	589.978439	12.852135
14.430609	588.311935	12.857152
13.968741	593.392111	12.862170
14.035570	577.770767	12.867187
13.855677	587.808787	12.872205
14.106144	593.803650	12.877223
14.659073	593.932348	12.882240
14.157729	592.871407	12.887258
14.135283	587.971178	12.892275
14.273067	588.432746	12.897293
14.279708	592.275530	12.902311
14.151924	582.973753	12.907328
13.912959	583.948396	12.912346
13.830606	584.052935	12.917363
13.992242	584.274113	12.922381
13.848586	590.040016	12.927399
14.247176	584.992186	12.932416
14.092545	588.547667	12.937434
14.001693	584.699463	12.942451
14.343447	595.192734	12.947469
14.402587	597.941791	12.952487
14.112782	583.436278	12.957504
14.213697	598.842572	12.962522
14.439480	602.682795	12.967539
14.612263	604.770402	12.972557
14.345394	614.515877	12.977575
14.617289	603.526683	12.982592
14.212840	612.637197	12.987610
14.439330	600.951357	12.992627
14.762395	596.656868	12.997645
14.307848	601.417182	13.002663
14.620096	601.652778	13.007680
14.316145	612.874574	13.012698
14.529678	612.137812	13.017715
14.768825	607.850074	13.022733
14.344263	610.365188	13.027751
14.792315	607.733215	13.032768
14.593733	610.465599	13.037786
14.343202	605.282154	13.042803
14.841050	599.695022	13.047821
14.352893	610.528947	13.052839
14.664303	603.033253	13.057856
14.379799	608.925230	13.062874
14.672309	605.664248	13.067891
14.661549	609.033238	13.072909
14.619918	608.295180	13.077927
15.053061	604.056131	13.082944
14.820918	604.212392	13.087962
14.767027	597.420492	13.092979
14.647760	605.076010	13.097997
14.720058	600.110536	13.103015
14.755865	604.201236	13.108032
14.956689	605.795346	13.113050
14.599463	603.623255	13.118067
14.828345	608.321343	13.123085
14.572209	610.712407	13.128103
14.833399	603.174042	13.133120
14.885029	614.529817	13.138138
14.585731	606.393933	13.143155
14.988634	602.986381	13.148173
14.675129	609.794865	13.153191
14.900842	605.010622	13.158208
14.849476	604.286703	13.163226
14.617756	609.368918	13.168243
14.871511	609.859765	13.173261
14.803530	616.923502	13.178279
14.983407	609.312591	13.183296
14.756425	610.907040	13.188314
14.359701	616.112774	13.193331
14.672216	616.455622	13.198349
14.888452	622.285417	13.203367
15.002282	630.892384	13.208384
15.158173	634.481575	13.213402
14.826220	641.412859	13.218419
15.283828	635.920341	13.223437
15.099056	629.846213	13.228455
14.900604	631.676054	13.233472
15.063004	639.136259	13.238490
14.971826	644.064063	13.243507
15.037766	638.130772	13.248525
14.932216	644.222106	13.253543
15.111294	634.146716	13.258560
14.912314	641.095165	13.263578
14.960293	639.014609	13.268595
15.278906	636.999210	13.273613
15.250104	635.189376	13.278631
15.319303	640.483514	13.283648
15.503695	637.311941	13.288666
14.967997	642.741284	13.293683
15.058287	637.924471	13.298701
15.185166	641.597072	13.303719
15.244304	651.620001	13.308736
15.424679	664.180170	13.313754
15.294470	667.422606	13.318771
15.600473	652.786403	13.323789
15.555662	661.613737	13.328807
15.468449	650.699361	13.333824
15.417784	641.732671	13.338842
15.020489	646.793341	13.343859
15.344748	647.169074	13.348877
15.219697	656.557989	13.353895
15.630897	659.646703	13.358912
15.059178	663.358653	13.363930
15.239479	660.885121	13.368947
15.394296	658.497605	13.373965
15.564781	660.692869	13.378983
15.557247	657.396547	13.384000
15.992239	657.373201	13.389018
15.873307	664.571118	13.394035
16.005661	659.861354	13.399053
15.776501	661.961057	13.404071
16.084605	660.439580	13.409088
15.806827	650.523671	13.414106
15.412346	643.115776	13.419123
15.566792	640.829302	13.424141
15.349076	645.054155	13.429159
15.550931	652.710188	13.434176
16.132074	659.486690	13.439194
15.542127	656.678664	13.444211
16.216731	658.902732	13.449229
15.896130	662.796482	13.454247
15.665750	645.100729	13.459264
15.831414	651.806222	13.464282
15.498751	653.742165	13.469299
15.863731	649.857689	13.474317
15.704146	654.982332	13.479335
15.690462	666.550273	13.484352
16.015681	657.525052	13.489370
15.526771	663.445715	13.494387
15.944549	659.366830	13.499405
15.730409	654.515363	13.504423
15.709693	662.401706	13.509440
15.971156	654.535085	13.514458
15.526035	661.389326	13.519475
15.708392	657.798359	13.524493
15.771676	650.764141	13.529511
16.011802	656.066383	13.534528
15.877766	652.852871	13.539546
15.942646	665.074430	13.544563
15.757421	658.621679	13.549581
16.459935	664.890154	13.554599
15.759615	667.318827	13.559616
16.300306	660.289167	13.564634
16.132020	664.212849	13.569651
16.299420	659.538653	13.574669
15.845092	659.148861	13.579687
15.888845	666.804270	13.584704
16.547938	680.596372	13.589722
15.986282	676.363876	13.594739
16.032386	667.984844	13.599757
15.837251	673.014045	13.604775
16.353457	690.154504	13.609792
16.487036	685.132129	13.614810
16.450992	693.317507	13.619827
16.499660	682.804818	13.624845
16.063782	672.881956	13.629863
16.073510	682.735876	13.634880
16.466653	680.680467	13.639898
16.598889	692.670659	13.644915
16.422544	681.284164	13.649933
16.312840	676.227089	13.654951
16.532196	674.750985	13.659968
16.431487	675.221286	13.664986
16.067321	680.084310	13.670003
16.421103	678.287485	13.675021
16.616240	684.628653	13.680039
16.265599	686.172936	13.685056
16.665950	688.515445	13.690074
16.334732	683.710600	13.695091
16.636951	690.328577	13.700109
16.591907	686.365925	13.705127
16.565518	686.357613	13.710144
16.718363	683.853640	13.715162
16.762856	697.085062	13.720179
16.361174	679.059352	13.725197
16.858269	682.043182	13.730215
16.393580	684.416236	13.735232
17.058953	682.659256	13.740250
16.650746	674.688615	13.745267
16.363645	666.099541	13.750285
16.674601	679.829086	13.755303
16.646522	684.911173	13.760320
16.681050	687.925999	13.765338
16.524186	683.545273	13.770355
16.705694	683.151153	13.775373
16.643134	693.268790	13.780391
16.806963	689.964715	13.785408
16.659393	680.249415	13.790426
16.745785	683.442352	13.795443
16.420858	686.579414	13.800461
16.433008	683.040189	13.805479
16.652568	682.226749	13.810496
17.025765	676.236138	13.815514
16.560931	681.035943	13.820531
16.539309	676.195520	13.825549
16.661374	691.851056	13.830567
16.790243	706.940677	13.835584
17.386413	702.057705	13.840602
17.072454	710.409434	13.845619
17.099965	682.988649	13.850637
16.796839	685.497489	13.855655
16.855682	699.316793	13.860672
17.440954	702.974840	13.865690
16.807080	699.286895	13.870707
16.876827	697.284991	13.875725
17.049000	702.092916	13.880743
16.937347	715.471735	13.885760
17.185318	711.072150	13.890778
17.183926	714.947768	13.895795
17.522699	708.962507	13.900813
17.566365	708.668741	13.905831
16.912716	699.417221	13.910848
17.098275	692.632182	13.915866
17.009399	711.555169	13.920883
17.017901	713.172921	13.925901
17.472044	711.840133	13.930919
17.271640	714.149953	13.935936
17.272259	705.449793	13.940954
17.369126	715.914993	13.945971
17.485175	719.444134	13.950989
17.357586	714.664379	13.956007
17.236097	712.436637	13.961024
17.298674	708.526650	13.966042
17.296697	707.372173	13.971059
17.086296	711.715819	13.976077
17.035529	702.310473	13.981095
16.751439	714.636890	13.986112
17.296718	705.063003	13.991130
16.977538	713.380834	13.996147
17.200540	711.885225	14.001165
17.758006	720.700864	14.006183
17.631812	738.357941	14.011200
17.768122	735.146502	14.016218
17.528742	718.556574	14.021235
17.071025	718.312470	14.026253
17.725472	725.156477	14.031271
17.617416	737.752139	14.036288
17.347039	734.837541	14.041306
17.441011	731.850438	14.046323
17.649545	731.284858	14.051341
17.784308	731.380838	14.056359
17.677067	741.063660	14.061376
17.717915	729.728522	14.066394
18.012990	739.093092	14.071411
17.857605	736.883247	14.076429
17.926563	737.103078	14.081447
17.984220	749.234304	14.086464
17.775161	726.946752	14.091482
17.736745	722.771629	14.096499
17.467485	721.898600	14.101517
17.597998	731.989353	14.106535
17.813511	731.362728	14.111552
17.764584	723.194120	14.116570
17.865910	730.086379	14.121587
17.425922	735.860599	14.126605
17.818113	732.079162	14.131623
17.738705	737.194501	14.136640
17.974228	733.320695	14.141658
17.694403	731.341658	14.146675
17.684194	740.450813	14.151693
18.026568	731.542800	14.156711
17.508250	748.591931	14.161728
17.980799	744.659128	14.166746
18.143127	746.921943	14.171763
17.990507	756.927410	14.176781
17.992977	751.581457	14.181799
18.181826	764.301319	14.186816
17.831237	752.481174	14.191834
18.243145	746.254146	14.196851
18.225138	757.702903	14.201869
18.697409	754.328702	14.206887
17.917798	755.400155	14.211904
18.466365	751.657480	14.216922
18.165956	744.023464	14.221939
17.993415	755.600418	14.226957
18.345280	744.601842	14.231975
18.341455	758.260541	14.236992
18.391372	754.229443	14.242010
18.420867	760.896220	14.247027
18.232012	756.782380	14.252045
18.722391	755.462881	14.257063
18.620460	754.525929	14.262080
18.595864	744.302313	14.267098
18.064557	747.774466	14.272115
18.032472	741.840624	14.277133
18.377666	748.032222	14.282151
18.375154	755.215205	14.287168
18.387107	759.338057	14.292186
18.506640	765.735205	14.297203
18.574053	762.203138	14.302221
18.695932	757.709568	14.307239
18.187147	762.317428	14.312256
18.097259	762.309535	14.317274
18.464351	755.278464	14.322291
18.201796	754.035172	14.327309
18.185233	753.403655	14.332327
18.574154	763.861280	14.337344
18.482269	765.923843	14.342362
18.317056	769.471540	14.347379
18.675126	783.692432	14.352397
18.634399	779.432451	14.357415
18.766798	791.526823	14.362432
18.980611	786.390944	14.367450
18.654722	785.031281	14.372467
18.453515	789.158927	14.377485
19.123968	784.523136	14.382503
18.920799	781.241471	14.387520
18.392153	782.169712	14.392538
18.677004	779.058210	14.397555
18.400537	785.542267	14.402573
18.556221	771.377482	14.407591
18.266705	786.854194	14.412608
18.326749	785.232477	14.417626
18.775170	788.937094	14.422643
18.856565	802.124980	14.427661
18.942448	800.350920	14.432679
19.387271	807.192884	14.437696
19.391435	804.443807	14.442714
19.497988	789.765963	14.447731
18.636891	782.550578	14.452749
18.806908	782.694717	14.457767
19.090065	791.524699	14.462784
19.420581	798.854658	14.467802
19.314317	790.761216	14.472819
19.130030	792.260673	14.477837
19.376452	791.821732	14.482855
19.021205	792.517854	14.487872
19.333710	776.006043	14.492890
18.799478	788.103222	14.497907
19.215136	790.844137	14.502925
19.134600	804.628421	14.507943
19.161493	807.521383	14.512960
19.215955	810.435300	14.517978
19.418393	802.823949	14.522995
19.695807	810.954266	14.528013
19.212292	797.942991	14.533031
19.316695	801.461339	14.538048
18.956023	801.038027	14.543066
19.171496	799.638255	14.548083
19.247924	805.442542	14.553101
19.441723	802.493532	14.558119
19.566224	807.722306	14.563136
19.272198	805.704447	14.568154
19.814592	803.411198	14.573171
19.745184	811.617604	14.578189
19.534579	804.603879	14.583207
19.512464	812.724029	14.588224
19.415973	808.602108	14.593242
19.636228	800.419955	14.598259
18.930142	807.087671	14.603277
19.453408	810.124251	14.608295
19.496999	810.407991	14.613312
19.719259	815.104009	14.618330
19.929946	805.746261	14.623347
19.736125	813.912080	14.628365
19.983210	808.300813	14.633383
20.006897	806.485945	14.638400
19.688086	808.927818	14.643418
19.742745	795.198453	14.648435
19.825670	804.046995	14.653453
19.899007	803.420413	14.658471
19.690034	796.564222	14.663488
19.583107	809.039841	14.668506
19.751022	805.476339	14.673523
19.649518	806.249717	14.678541
19.477370	805.494103	14.683559
19.619885	813.178378	14.688576
20.096476	822.549444	14.693594
19.924017	819.635366	14.698611
19.889712	831.821990	14.703629
19.635840	833.092450	14.708647
20.193393	827.423371	14.713664
20.025160	831.662654	14.718682
20.355840	832.681159	14.723699
19.818056	830.284694	14.728717
20.034170	832.949390	14.733735
20.216741	824.022032	14.738752
20.024792	836.353121	14.743770
20.409756	828.221048	14.748787
20.489721	831.658003	14.753805
20.134948	829.479190	14.758823
20.529412	825.653200	14.763840
20.021997	823.021640	14.768858
20.484353	822.596414	14.773875
20.214194	824.582602	14.778893
20.245422	830.349755	14.783911
20.212577	831.920308	14.788928
20.320445	824.235312	14.793946
20.358890	823.267033	14.798963
20.031901	828.805944	14.803981
20.249571	832.849447	14.808999
20.531478	829.003112	14.814016
19.978446	834.864390	14.819034
20.285443	825.308604	14.824051
20.178307	828.153012	14.829069
19.966472	830.227947	14.834087
20.020817	820.761992	14.839104
20.443328	842.300481	14.844122
20.929097	841.871608	14.849139
20.876988	841.135172	14.854157
20.543961	838.009412	14.859175
20.386032	828.696421	14.864192
20.099138	825.882207	14.869210
20.618371	844.899998	14.874227
20.792469	857.196199	14.879245
20.877800	858.025694	14.884263
20.904286	852.751709	14.889280
20.741893	846.165951	14.894298
20.647764	841.810130	14.899315
20.761917	835.878734	14.904333
20.763360	842.849703	14.909351
21.088210	836.715092	14.914368
20.335819	843.194376	14.919386
21.118814	846.745930	14.924403
21.250034	847.517788	14.929421
20.570499	836.136957	14.934439
20.801497	830.843760	14.939456
20.718350	845.360609	14.944474
20.874615	852.913376	14.949491
21.014162	856.915401	14.954509
20.825921	854.988361	14.959527
20.795419	852.086888	14.964544
20.662141	861.246823	14.969562
20.688893	854.798866	14.974579
21.019310	849.931986	14.979597
20.962069	863.520189	14.984615
20.860704	852.898219	14.989632
20.887349	851.155467	14.994650
20.670518	855.096217	14.999667
21.226227	864.022651	15.004685
20.809217	874.498528	15.009703
21.383073	881.339364	15.014720
21.441587	883.848728	15.019738
21.007849	876.465782	15.024755
21.416608	876.765250	15.029773
21.483455	876.291151	15.034791
21.415039	880.372897	15.039808
21.128257	889.518878	15.044826
21.057505	889.508005	15.049843
21.400993	879.665648	15.054861
21.179617	888.419602	15.059879
21.204050	870.147477	15.064896
21.150342	886.720468	15.069914
21.495790	886.427048	15.074931
21.562351	888.023154	15.079949
21.044180	885.304899	15.084967
21.513841	879.681045	15.089984
21.030492	880.867320	15.095002
21.472502	893.342734	15.100019
21.724498	897.153695	15.105037
21.439472	893.594427	15.110055
21.633683	902.652903	15.115072
21.736811	911.290073	15.120090
21.750761	907.144622	15.125107
22.027032	897.896532	15.130125
21.536962	891.999233	15.135143
21.606645	883.714257	15.140160
21.704816	894.996693	15.145178
21.707245	897.429587	15.150195
22.017527	904.185241	15.155213
21.746253	905.190178	15.160231
22.015620	898.420414	15.165248
21.856648	894.825741	15.170266
21.336218	886.790429	15.175283
21.620329	899.277809	15.180301
21.893940	906.468353	15.185319
22.003249	906.378954	15.190336
21.647336	906.261004	15.195354
21.853060	914.743350	15.200371
22.249841	908.001081	15.205389
22.133957	909.950635	15.210407
22.043363	899.592042	15.215424
21.946565	915.966646	15.220442
21.834040	916.757522	15.225459
22.109096	912.079121	15.230477
21.937622	906.763361	15.235495
22.043675	913.184750	15.240512
21.711649	914.041360	15.245530
22.135405	912.997306	15.250547
21.956775	912.372082	15.255565
21.871401	908.462996	15.260583
22.499109	917.289887	15.265600
22.040615	916.654590	15.270618
22.224118	919.548433	15.275635
22.599456	929.181467	15.280653
22.413470	916.754928	15.285671
22.264645	909.542198	15.290688
22.124202	914.001231	15.295706
22.387093	929.805460	15.300723
22.440573	931.264754	15.305741
22.402315	934.467676	15.310759
22.497334	932.812098	15.315776
22.783809	931.382327	15.320794
22.648448	927.600938	15.325811
22.890527	914.902629	15.330829
22.307040	912.175605	15.335847
22.254664	907.907939	15.340864
22.553124	924.413511	15.345882
22.467263	932.382698	15.350899
22.636270	929.207158	15.355917
22.040945	930.060582	15.360935
22.185014	927.371753	15.365952
22.794003	924.462218	15.370970
22.533532	923.101827	15.375987
22.703078	934.455225	15.381005
22.644828	933.170642	15.386023
22.653795	925.949117	15.391040
22.773454	935.306389	15.396058
22.607210	940.908667	15.401075
22.738291	934.264561	15.406093
22.731637	959.779973	15.411111
23.021835	953.256250	15.416128
22.826712	962.952875	15.421146
23.085580	955.802880	15.426163
23.078165	959.748916	15.431181
22.659708	956.219877	15.436199
23.133362	953.306163	15.441216
23.060510	959.203169	15.446234
22.994111	957.541164	15.451251
23.038458	958.878808	15.456269
23.236095	962.158614	15.461287
23.040250	956.193394	15.466304
23.232085	949.909044	15.471322
23.121572	956.938513	15.476339
23.243847	952.725694	15.481357
23.128461	953.892551	15.486375
23.260889	952.038647	15.491392
23.355903	950.821717	15.496410
23.028172	956.338692	15.501427
23.031578	942.705555	15.506445
23.091141	955.518265	15.511463
22.935413	945.220278	15.516480
23.177174	949.193786	15.521498
22.855581	955.476651	15.526515
23.633186	963.841579	15.531533
23.604967	974.547309	15.536551
23.312785	966.264987	15.541568
23.401897	967.018161	15.546586
23.426163	982.648155	15.551603
23.623962	976.195613	15.556621
23.520014	982.709683	15.561639
23.538122	975.164828	15.566656
23.563361	975.808028	15.571674
23.483495	982.690727	15.576691
23.728900	977.666638	15.581709
23.330092	980.591196	15.586727
23.514563	980.483782	15.591744
23.258269	983.168405	15.596762
23.352424	983.027716	15.601779
23.346625	980.535780	15.606797
23.228193	988.648916	15.611815
23.582565	998.525089	15.616832
23.899534	996.617202	15.621850
23.980788	1003.891383	15.626867
24.446178	1004.043183	15.631885
23.940382	998.369200	15.636903
24.075458	982.238268	15.641920
23.616632	973.707339	15.646938
23.784571	992.552769	15.651955
24.105136	1005.476353	15.656973
24.072434	1010.180562	15.661991
23.822061	1001.875936	15.667008
24.153612	1008.861844	15.672026
24.226921	1009.150428	15.677043
24.367005	1013.578431	15.682061
24.038368	1015.987148	15.687079
23.936282	1016.637551	15.692096
23.994168	1008.644683	15.697114
24.135529	1013.940319	15.702131
24.459227	1004.561716	15.707149
24.277991	1015.344942	15.712167
24.372700	1015.806916	15.717184
24.309916	1005.844712	15.722202
24.308517	1007.808010	15.727219
24.231257	1005.630148	15.732237
24.834556	1007.698108	15.737255
24.460305	1006.402761	15.742272
24.246626	1006.171149	15.747290
24.322578	1005.875507	15.752307
24.641754	1003.190960	15.757325
24.672005	997.231549	15.762343
24.461403	1004.099898	15.767360
24.606938	995.702075	15.772378
24.654696	998.131081	15.777395
24.496674	1007.171869	15.782413
24.436919	1006.543912	15.787431
24.301283	1002.027260	15.792448
24.311422	993.956627	15.797466
24.257258	999.465735	15.802483
24.526089	1002.967990	15.807501
24.280190	1007.096332	15.812519
24.289022	997.792002	15.817536
24.783422	1006.418790	15.822554
24.375893	1029.986504	15.827571
24.720872	1029.787828	15.832589
24.760587	1026.067521	15.837607
24.962939	1028.257869	15.842624
24.717795	1026.813033	15.847642
24.448462	1038.253764	15.852659
24.552573	1031.244597	15.857677
24.710972	1036.032666	15.862695
24.665672	1033.647856	15.867712
24.932831	1038.570469	15.872730
25.055284	1052.178175	15.877747
25.203030	1051.760902	15.882765
24.842958	1050.542238	15.887783
25.055702	1062.097272	15.892800
25.089640	1063.730031	15.897818
24.898507	1060.096151	15.902835
25.474966	1060.473652	15.907853
25.585521	1061.529599	15.912871
25.136562	1058.914149	15.917888
25.376071	1048.153783	15.922906
25.001433	1045.066022	15.927923
25.346542	1050.595031	15.932941
25.156489	1051.644133	15.937959
25.266726	1063.170947	15.942976
25.481065	1058.066467	15.947994
25.653004	1057.796904	15.953011
25.484937	1044.591169	15.958029
25.655039	1053.555647	15.963047
25.522841	1055.204804	15.968064
25.546598	1056.886483	15.973082
25.033492	1054.281020	15.978099
25.156458	1054.249454	15.983117
25.529923	1052.885023	15.988135
25.315385	1067.409887	15.993152
25.395141	1057.797840	15.998170
25.333802	1058.413498	16.003187
25.834190	1055.710197	16.008205
25.653611	1050.638805	16.013223
25.286090	1056.404999	16.018240
25.886409	1057.384692	16.023258
25.944940	1053.235422	16.028275
25.347455	1050.264406	16.033293
25.619943	1059.282372	16.038311
25.829528	1071.383851	16.043328
26.139379	1078.587757	16.048346
26.033242	1086.055247	16.053363
25.806279	1074.114655	16.058381
25.823244	1074.415169	16.063399
26.077257	1078.266879	16.068416
26.331136	1078.536818	16.073434
25.824758	1075.299151	16.078451
26.134443	1075.137528	16.083469
26.018865	1074.120634	16.088487
25.851849	1082.329738	16.093504
26.065702	1076.060851	16.098522
26.363336	1081.187011	16.103539
26.132014	1077.537295	16.108557
26.291276	1077.607372	16.113575
26.503422	1089.077311	16.118592
26.175686	1082.621349	16.123610
26.205928	1078.817300	16.128627
26.123745	1085.627817	16.133645
26.092981	1081.965808	16.138663
26.029514	1080.208662	16.143680
26.519002	1079.211168	16.148698
26.462241	1078.368150	16.153715
26.132775	1085.633730	16.158733
26.217865	1080.322151	16.163751
26.285457	1077.291761	16.168768
26.407166	1081.485960	16.173786
26.622582	1074.229075	16.178803
26.633330	1077.342343	16.183821
26.069043	1075.319195	16.188839
26.346261	1078.088022	16.193856
26.592420	1089.309671	16.198874
26.891708	1099.895058	16.203891
26.783640	1098.608752	16.208909
26.790252	1086.688589	16.213927
26.472214	1088.631768	16.218944
26.994200	1088.279302	16.223962
26.940149	1082.443439	16.228979
26.616672	1078.584011	16.233997
26.746875	1081.612410	16.239015
26.972235	1095.519703	16.244032
27.201667	1092.517760	16.249050
26.972485	1074.108191	16.254067
26.809732	1074.218938	16.259085
26.733710	1073.410477	16.264103
26.624146	1086.663018	16.269120
26.996799	1097.404236	16.274138
27.314776	1096.057909	16.279155
27.077451	1091.796905	16.284173
27.248250	1094.452916	16.289191
26.869195	1102.969596	16.294208
27.027062	1088.939917	16.299226
26.967692	1088.182511	16.304243
27.232417	1097.766588	16.309261
27.231591	1096.233214	16.314279
27.177898	1109.776872	16.319296
27.227616	1099.307955	16.324314
27.026378	1089.152668	16.329331
27.031221	1100.014270	16.334349
27.087996	1093.176549	16.339367
26.935108	1097.716459	16.344384
27.295911	1108.854000	16.349402
27.912945	1114.261796	16.354419
27.509967	1110.755562	16.359437
27.335673	1096.957473	16.364455
27.596214	1110.206056	16.369472
27.247581	1114.325172	16.374490
27.339010	1122.632910	16.379507
27.127461	1122.195838	16.384525
27.337968	1116.848943	16.389543
27.274928	1113.166707	16.394560
27.522668	1119.733367	16.399578
27.675240	1119.075503	16.404595
27.185970	1121.168421	16.409613
27.928873	1118.152800	16.414631
27.951776	1137.579537	16.419648
27.606374	1136.730964	16.424666
28.281789	1137.200357	16.429683
27.843545	1137.514942	16.434701
27.891728	1117.714626	16.439719
27.619654	1133.132118	16.444736
28.076727	1142.878774	16.449754
28.123396	1140.432294	16.454771
27.947589	1135.218124	16.459789
28.404232	1132.142929	16.464807
28.143939	1129.984082	16.469824
27.731864	1121.581502	16.474842
27.895034	1126.239466	16.479859
28.131998	1131.693820	16.484877
28.302372	1134.987370	16.489895
28.096841	1147.314477	16.494912
28.135596	1142.735923	16.499930
28.200969	1137.730352	16.504947
28.036651	1140.542688	16.509965
28.229702	1140.815787	16.514983
28.550967	1139.951778	16.520000
28.050850	1137.650390	16.525018
28.340922	1134.815723	16.530035
28.108087	1138.462383	16.535053
28.201482	1140.060645	16.540071
27.992273	1140.715108	16.545088
28.394187	1148.103522	16.550106
28.947995	1157.027245	16.555123
28.490698	1151.187872	16.560141
28.341880	1138.607070	16.565159
28.618331	1156.814091	16.570176
28.470819	1164.070307	16.575194
28.577743	1161.488212	16.580211
28.987021	1156.075644	16.585229
28.984335	1154.839198	16.590247
28.955345	1161.313261	16.595264
28.821859	1152.703189	16.600282
28.548639	1147.747177	16.605299
28.857197	1161.606855	16.610317
28.923835	1159.204600	16.615335
28.738932	1165.554618	16.620352
28.652382	1165.489400	16.625370
28.939826	1158.931317	16.630387
28.782120	1166.476297	16.635405
28.845734	1156.437525	16.640423
28.967351	1155.901243	16.645440
28.807980	1155.658017	16.650458
29.209519	1154.604785	16.655475
28.900950	1159.623382	16.660493
29.200941	1156.837660	16.665511
29.192985	1162.936066	16.670528
29.030301	1161.834984	16.675546
29.257779	1155.475585	16.680563
29.201772	1162.316770	16.685581
29.179458	1148.166776	16.690599
29.182889	1163.134304	16.695616
28.874660	1163.198274	16.700634
29.405864	1165.375308	16.705651
29.239699	1176.367722	16.710669
29.428638	1179.522691	16.715687
29.693008	1179.560626	16.720704
29.718141	1189.611243	16.725722
29.675310	1177.796546	16.730739
29.345370	1182.364043	16.735757
29.494958	1185.326326	16.740775
29.935082	1178.305810	16.745792
29.608479	1180.262956	16.750810
29.887017	1179.544452	16.755827
29.641698	1186.348849	16.760845
29.653327	1178.719711	16.765863
29.780481	1180.366368	16.770880
29.254498	1173.130203	16.775898
29.585781	1175.966366	16.780915
29.678043	1177.908788	16.785933
29.435114	1173.730687	16.790951
29.757003	1184.236866	16.795968
29.713918	1179.986623	16.800986
29.645480	1172.133270	16.806003
29.313856	1186.483957	16.811021
29.970571	1194.858350	16.816039
29.939922	1197.807672	16.821056
30.011087	1199.608215	16.826074
30.139551	1205.262520	16.831091
30.118275	1201.438064	16.836109
30.315953	1200.586983	16.841127
30.580496	1200.921535	16.846144
29.893374	1198.450441	16.851162
30.118989	1193.681835	16.856179
30.255043	1205.536079	16.861197
30.389536	1200.415588	16.866215
30.422983	1195.336077	16.871232
30.080192	1201.657042	16.876250
30.677458	1199.364668	16.881267
30.368166	1205.181804	16.886285
30.440886	1198.313158	16.891303
30.268009	1203.272771	16.896320
30.056818	1210.879745	16.901338
30.538396	1201.561664	16.906355
30.480567	1210.549086	16.911373
30.266142	1205.167339	16.916391
30.920481	1200.552887	16.921408
30.513788	1208.313375	16.926426
30.692120	1206.386026	16.931443
30.586710	1217.526796	16.936461
30.933076	1219.707369	16.941479
30.937994	1207.967268	16.946496
30.706982	1213.522912	16.951514
30.900821	1223.130716	16.956531
30.598374	1224.023759	16.961549
30.603838	1232.146118	16.966567
31.016639	1219.054941	16.971584
30.844975	1236.766927	16.976602
30.513851	1230.443982	16.981619
30.505013	1229.325253	16.986637
30.642166	1225.084807	16.991655
30.667511	1228.296814	16.996672
31.005290	1247.011928	17.001690
31.373036	1245.774606	17.006707
31.251054	1247.295958	17.011725
31.384516	1237.183149	17.016743
31.656413	1243.124403	17.021760
31.337148	1232.324694	17.026778
31.487004	1210.163692	17.031795
31.141703	1225.564263	17.036813
30.823211	1229.255836	17.041831
31.374119	1233.515789	17.046848
31.559940	1243.124852	17.051866
31.652165	1243.003398	17.056883
31.753733	1246.645351	17.061901
31.547374	1237.317596	17.066919
31.311667	1219.760956	17.071936
31.273572	1237.385875	17.076954
31.594953	1247.204208	17.081971
31.409185	1244.374182	17.086989
31.332505	1254.715242	17.092007
31.531123	1242.364294	17.097024
31.542846	1252.293957	17.102042
31.920331	1251.679966	17.107059
31.482038	1250.580763	17.112077
31.607512	1248.320814	17.117095
31.507619	1249.280151	17.122112
31.166641	1256.462385	17.127130
31.926724	1265.085804	17.132147
31.921292	1275.115981	17.137165
31.901272	1267.924077	17.142183
32.039438	1275.984769	17.147200
32.036102	1275.622573	17.152218
32.156214	1282.161827	17.157235
32.326068	1274.315509	17.162253
31.942700	1273.264557	17.167271
32.345319	1279.901837	17.172288
32.288010	1278.651796	17.177306
32.155817	1267.024523	17.182323
32.394568	1271.910598	17.187341
32.129239	1275.322505	17.192359
32.456296	1264.384277	17.197376
32.221290	1274.074658	17.202394
32.407770	1283.863521	17.207411
32.448286	1273.197119	17.212429
32.101194	1278.278552	17.217447
32.451450	1267.125272	17.222464
32.362382	1278.080498	17.227482
32.447975	1273.690278	17.232499
32.308048	1274.965118	17.237517
32.572361	1272.986506	17.242535
32.317362	1275.194444	17.247552
32.464275	1280.088509	17.252570
32.700013	1289.289039	17.257587
32.832894	1295.094164	17.262605
32.683531	1300.700238	17.267623
32.935275	1296.277832	17.272640
32.552397	1296.170389	17.277658
32.969569	1293.587307	17.282675
33.032618	1296.654600	17.287693
32.731764	1298.418401	17.292711
32.745984	1295.872810	17.297728
32.702408	1303.292781	17.302746
33.070911	1298.624977	17.307763
33.131807	1292.954185	17.312781
32.965012	1295.580738	17.317799
33.169004	1281.464832	17.322816
33.028857	1296.861924	17.327834
33.029519	1296.628493	17.332851
33.394747	1292.526089	17.337869
33.522319	1301.891790	17.342887
33.317695	1292.724681	17.347904
33.144301	1294.863112	17.352922
33.348243	1297.952650	17.357939
33.355232	1288.487509	17.362957
32.999760	1293.005362	17.367975
33.289196	1284.827996	17.372992
33.309555	1292.667197	17.378010
33.244984	1297.818256	17.383027
33.490429	1310.270920	17.388045
33.301836	1324.845602	17.393063
33.148514	1316.560432	17.398080
33.485099	1325.912537	17.403098
33.398622	1322.489527	17.408115
33.582917	1311.633458	17.413133
33.374976	1318.293230	17.418151
33.831381	1316.145850	17.423168
33.358697	1324.380566	17.428186
33.611972	1335.500277	17.433203
33.980144	1339.836045	17.438221
33.651713	1338.378904	17.443239
34.278702	1329.902808	17.448256
33.925223	1337.702404	17.453274
34.009665	1331.339967	17.458291
34.146641	1330.450994	17.463309
34.066302	1334.850280	17.468327
34.257750	1327.224639	17.473344
34.474758	1332.622202	17.478362
34.242515	1332.077894	17.483379
34.478523	1334.969942	17.488397
33.958381	1338.052303	17.493415
34.114213	1334.518981	17.498432
34.389032	1334.410122	17.503450
34.354934	1339.979327	17.508467
34.227461	1328.531160	17.513485
34.279225	1337.918149	17.518503
34.393172	1329.635542	17.523520
34.358325	1337.770537	17.528538
34.056175	1344.902579	17.533555
34.240089	1339.086387	17.538573
34.134048	1332.027770	17.543591
34.565551	1337.139474	17.548608
34.566360	1347.515859	17.553626
34.459200	1360.013990	17.558643
34.456265	1360.986639	17.563661
34.664249	1367.543802	17.568679
34.867916	1354.295738	17.573696
35.061688	1352.498514	17.578714
34.903044	1370.249631	17.583731
34.767283	1355.277690	17.588749
35.034355	1364.678508	17.593767
35.069024	1359.292646	17.598784
35.429246	1357.510532	17.603802
35.090830	1353.997353	17.608819
35.247348	1346.740060	17.613837
34.707142	1337.773501	17.618855
35.287615	1344.720785	17.623872
35.257811	1351.750467	17.628890
34.866821	1352.461642	17.633907
35.198004	1345.467490	17.638925
34.973118	1351.375674	17.643943
35.312685	1358.830688	17.648960
35.202006	1353.136098	17.653978
34.990617	1351.935288	17.658995
35.041618	1345.316120	17.664013
34.971673	1350.950871	17.669031
35.177856	1354.052693	17.674048
35.208961	1356.437003	17.679066
35.494134	1379.884703	17.684083
35.738581	1375.523374	17.689101
35.497977	1382.289242	17.694119
35.525830	1378.775836	17.699136
35.990193	1375.904527	17.704154
35.863045	1382.832612	17.709171
35.920607	1385.329572	17.714189
35.637067	1381.536443	17.719207
35.902600	1386.961181	17.724224
36.017322	1382.904072	17.729242
35.793506	1378.757660	17.734259
36.131847	1370.708341	17.739277
36.079742	1380.004227	17.744295
35.814039	1383.940078	17.749312
36.250936	1376.345629	17.754330
35.923553	1372.786547	17.759347
36.028260	1381.060780	17.764365
36.207851	1378.334795	17.769383
35.841764	1384.189234	17.774400
36.349226	1370.811807	17.779418
36.045020	1368.366277	17.784435
35.984402	1371.809445	17.789453
36.105647	1375.230610	17.794471
35.927553	1374.576884	17.799488
36.386915	1367.597480	17.804506
36.023892	1372.239605	17.809523
36.139068	1379.461320	17.814541
36.422748	1397.130973	17.819559
36.288225	1401.062182	17.824576
36.418414	1397.715877	17.829594
36.338610	1397.835802	17.834611
36.953576	1397.598243	17.839629
36.752682	1400.208030	17.844647
36.311784	1402.372343	17.849664
36.670673	1401.123766	17.854682
36.311018	1400.526709	17.859699
36.343074	1397.372409	17.864717
36.734778	1401.909657	17.869735
36.596765	1420.519151	17.874752
37.204725	1408.208498	17.879770
36.558702	1417.786223	17.884787
36.994779	1416.967443	17.889805
37.053448	1416.396773	17.894823
37.061801	1410.402763	17.899840
37.243589	1406.278401	17.904858
37.132145	1414.299124	17.909875
37.360771	1412.076743	17.914893
37.275504	1420.342703	17.919911
37.469697	1423.481118	17.924928
37.429756	1416.787720	17.929946
37.484363	1420.064634	17.934963
37.336885	1412.059378	17.939981
37.358029	1408.493362	17.944999
37.100464	1416.035060	17.950016
37.435605	1422.086448	17.955034
37.094760	1411.876974	17.960051
37.735467	1408.700491	17.965069
37.474933	1416.406754	17.970087
37.305314	1410.560375	17.975104
37.627148	1395.971592	17.980122
37.473804	1412.314429	17.985139
37.429646	1409.563315	17.990157
37.689037	1408.888810	17.995175
37.496046	1418.140379	18.000192
37.558550	1418.452743	18.005210
37.780124	1431.404673	18.010227
38.255729	1435.780542	18.015245
37.837147	1435.429346	18.020263
37.850188	1441.868564	18.025280
38.430803	1435.078541	18.030298
38.075597	1445.248480	18.035315
38.029267	1437.647189	18.040333
38.388134	1437.089740	18.045351
38.013692	1445.318683	18.050368
38.249937	1432.138074	18.055386
38.063084	1438.520050	18.060403
38.000759	1440.458167	18.065421
38.127132	1435.979506	18.070439
38.067043	1439.432072	18.075456
38.625659	1433.876248	18.080474
38.397508	1440.747497	18.085491
38.266258	1431.502621	18.090509
38.806905	1434.088476	18.095527
38.226333	1429.928170	18.100544
38.415013	1430.624835	18.105562
38.452248	1436.145094	18.110579
38.287732	1428.644260	18.115597
38.720303	1443.182287	18.120615
38.505364	1453.137886	18.125632
38.700683	1451.674929	18.130650
38.671174	1466.666774	18.135667
38.843750	1459.801415	18.140685
39.016301	1465.815016	18.145703
38.608112	1467.554519	18.150720
38.585264	1454.256441	18.155738
38.753618	1463.319229	18.160755
38.852305	1456.695751	18.165773
39.313955	1460.120738	18.170791
39.012678	1468.698065	18.175808
39.005238	1467.348728	18.180826
38.926349	1459.222318	18.185843
38.690047	1468.281838	18.190861
39.086070	1467.611304	18.195879
39.121765	1480.273471	18.200896
39.331001	1473.216205	18.205914
39.379684	1480.643976	18.210931
39.517800	1470.855362	18.215949
39.847652	1470.602233	18.220967
39.608120	1477.566787	18.225984
39.559832	1471.742523	18.231002
39.551492	1470.055651	18.236019
39.400955	1474.579511	18.241037
39.829436	1474.424637	18.246055
39.560815	1483.331405	18.251072
39.453955	1478.759658	18.256090
39.594258	1473.363626	18.261107
39.889987	1477.208929	18.266125
39.943956	1471.286692	18.271143
39.694500	1474.150205	18.276160
39.808622	1475.145662	18.281178
39.839053	1469.899283	18.286195
39.994846	1472.011728	18.291213
39.851900	1470.973825	18.296231
40.032629	1472.394416	18.301248
40.058029	1476.995027	18.306266
39.850294	1491.995707	18.311283
40.103786	1486.875542	18.316301
40.541813	1488.587437	18.321319
40.269061	1490.144907	18.326336
41.006195	1487.859123	18.331354
40.730934	1477.115531	18.336371
40.711030	1472.041092	18.341389
40.424819	1459.036482	18.346407
40.232382	1464.822885	18.351424
40.083241	1462.062862	18.356442
40.406867	1466.137350	18.361459
40.570346	1483.027377	18.366477
40.780920	1481.423186	18.371495
40.615620	1485.535933	18.376512
40.669183	1481.706076	18.381530
40.866481	1476.077106	18.386547
40.702702	1475.651522	18.391565
41.016638	1476.013104	18.396583
40.625144	1482.843528	18.401600
40.930882	1486.131847	18.406618
40.894082	1478.071459	18.411635
40.614273	1486.045844	18.416653
40.807036	1477.725649	18.421671
40.680484	1486.449352	18.426688
40.768977	1479.047962	18.431706
40.304755	1496.196679	18.436723
40.639215	1503.835588	18.441741
41.170010	1504.542107	18.446759
41.125792	1513.028939	18.451776
40.746591	1513.873985	18.456794
41.032644	1516.120791	18.461811
41.142304	1524.757242	18.466829
41.740139	1525.456480	18.471847
42.011561	1530.880345	18.476864
41.796686	1526.158143	18.481882
41.422962	1514.123339	18.486899
41.727960	1522.101363	18.491917
42.041030	1505.169064	18.496935
41.843037	1500.040293	18.501952
42.111359	1491.137121	18.506970
41.912767	1488.703533	18.511987
41.861832	1496.298301	18.517005
42.084898	1488.528811	18.522023
41.926084	1490.999514	18.527040
41.694846	1490.350901	18.532058
41.823312	1497.513790	18.537075
41.858288	1500.926321	18.542093
42.227484	1488.703280	18.547111
42.001369	1496.199089	18.552128
41.739218	1498.790025	18.557146
42.611417	1509.488429	18.562163
42.302612	1516.006187	18.567181
42.382812	1519.632589	18.572199
42.351461	1511.151610	18.577216
42.465667	1512.623588	18.582234
42.283059	1501.098686	18.587251
42.152662	1510.028129	18.592269
42.597762	1512.783508	18.597287
42.753333	1516.413954	18.602304
42.308927	1523.003320	18.607322
42.506327	1518.027580	18.612339
42.566462	1523.935626	18.617357
42.888915	1521.383038	18.622375
42.688076	1518.097718	18.627392
42.496408	1515.498944	18.632410
42.712118	1510.040667	18.637427
42.699110	1511.914308	18.642445
42.967718	1511.209962	18.647463
43.232230	1505.652569	18.652480
42.769245	1510.266111	18.657498
42.707193	1503.957979	18.662515
42.686384	1506.252561	18.667533
43.077992	1506.731439	18.672551
42.742500	1510.599288	18.677568
42.847336	1512.849061	18.682586
43.280997	1532.499457	18.687603
43.257475	1543.640303	18.692621
43.692468	1539.886749	18.697639
43.137341	1548.099689	18.702656
43.464735	1539.089465	18.707674
43.476088	1540.994030	18.712691
43.541323	1549.318669	18.717709
43.469645	1542.803737	18.722727
43.462946	1542.965929	18.727744
43.293253	1550.512938	18.732762
43.650731	1539.708663	18.737779
43.387728	1541.005840	18.742797
43.730898	1542.353808	18.747815
43.349036	1542.309320	18.752832
43.420997	1551.721681	18.757850
43.723578	1551.924083	18.762867
43.783103	1559.053549	18.767885
43.562597	1566.658969	18.772903
43.672671	1574.257104	18.777920
43.970168	1564.743430	18.782938
43.691780	1556.395568	18.787955
43.782795	1567.685857	18.792973
43.765228	1564.138461	18.797991
44.101297	1584.820292	18.803008
44.231861	1587.577318	18.808026
44.245842	1582.087311	18.813043
44.198238	1592.212596	18.818061
44.076413	1589.555599	18.823079
44.357917	1579.312249	18.828096
44.046715	1588.907364	18.833114
44.689296	1585.449688	18.838131
44.194493	1587.833858	18.843149
44.682562	1576.292850	18.848167
44.691493	1586.036939	18.853184
44.383365	1588.414136	18.858202
45.126492	1604.109479	18.863219
45.008520	1607.214478	18.868237
44.789054	1591.355951	18.873255
44.817781	1580.321966	18.878272
44.809169	1591.365845	18.883290
45.129453	1593.373798	18.888307
44.943045	1611.041113	18.893325
44.994254	1604.866793	18.898343
45.245630	1605.061390	18.903360
44.934641	1604.605073	18.908378
45.244937	1599.431849	18.913395
45.218984	1607.524556	18.918413
45.264487	1606.346849	18.923431
45.221403	1612.349891	18.928448
45.190345	1615.898959	18.933466
45.333855	1602.814715	18.938483
45.213552	1615.072069	18.943501
45.327204	1604.611837	18.948519
45.374527	1599.795143	18.953536
45.472238	1598.763945	18.958554
45.802715	1604.977070	18.963571
45.412043	1604.369056	18.968589
45.226683	1608.822631	18.973607
45.752619	1617.561575	18.978624
46.028200	1627.721770	18.983642
46.034500	1632.464253	18.988659
45.787439	1630.094997	18.993677
45.724756	1640.869610	18.998695
46.399283	1632.761519	19.003712
45.794769	1633.673209	19.008730
45.738822	1626.272155	19.013747
45.507152	1636.956309	19.018765
45.990871	1630.702016	19.023783
45.892435	1627.022028	19.028800
46.086088	1638.315317	19.033818
46.066376	1635.421504	19.038835
46.350869	1633.960428	19.043853
46.382781	1645.212630	19.048871
46.595880	1651.399865	19.053888
46.509075	1657.173039	19.058906
46.410923	1654.850025	19.063923
46.423275	1658.392342	19.068941
46.778111	1645.186800	19.073959
47.002906	1639.102209	19.078976
47.199379	1637.913618	19.083994
47.270147	1641.162809	19.089011
47.107313	1625.150265	19.094029
46.658769	1615.405574	19.099047
46.780329	1614.146596	19.104064
46.649419	1617.253611	19.109082
47.239445	1632.534152	19.114099
47.283375	1633.007205	19.119117
46.902782	1623.356073	19.124135
47.378138	1628.486281	19.129152
47.273390	1646.197722	19.134170
47.612872	1638.255405	19.139187
47.202423	1619.248633	19.144205
46.955093	1628.319419	19.149223
47.071415	1621.929824	19.154240
47.209006	1631.590789	19.159258
47.354773	1634.522183	19.164275
47.489664	1635.470233	19.169293
47.266130	1636.508802	19.174311
47.321902	1636.819062	19.179328
47.251609	1643.567979	19.184346
47.546009	1641.540460	19.189363
47.596150	1660.597446	19.194381
47.596259	1666.174050	19.199399
47.991748	1653.990986	19.204416
48.012390	1662.979041	19.209434
48.145638	1665.931325	19.214451
48.261161	1658.787589	19.219469
48.089698	1658.748213	19.224487
48.052185	1653.395592	19.229504
47.966956	1662.002491	19.234522
47.892545	1661.591392	19.239539
47.962833	1659.172722	19.244557
47.817598	1663.342347	19.249575
47.842174	1657.620289	19.254592
47.895359	1663.532618	19.259610
48.302760	1681.410513	19.264627
48.407846	1687.229561	19.269645
48.381032	1689.559816	19.274663
48.715543	1689.211283	19.279680
48.196418	1693.177191	19.284698
48.304849	1686.318576	19.289715
48.626670	1689.967355	19.294733
48.508337	1688.016715	19.299751
49.311961	1686.459029	19.304768
48.877059	1693.040666	19.309786
48.872417	1689.516479	19.314803
48.760148	1689.764539	19.319821
48.631299	1687.036036	19.324839
49.259833	1685.612911	19.329856
48.639294	1695.464533	19.334874
48.563774	1690.001051	19.339891
48.960818	1702.294683	19.344909
49.032009	1716.460000	19.349927
49.510379	1703.172064	19.354944
49.105725	1718.538117	19.359962
49.260600	1710.741278	19.364979
49.790841	1714.528029	19.369997
49.584771	1718.694515	19.375015
49.548112	1706.929001	19.380032
49.546906	1715.775314	19.385050
49.389816	1714.572337	19.390067
49.687312	1713.629950	19.395085
49.328686	1705.796296	19.400103
49.544663	1703.667369	19.405120
49.525241	1717.726871	19.410138
49.902728	1710.977838	19.415155
49.773638	1717.496091	19.420173
49.883188	1725.722392	19.425191
50.374537	1720.479918	19.430208
49.762199	1731.242332	19.435226
50.121888	1738.063197	19.440243
50.297144	1736.335091	19.445261
50.083424	1735.058877	19.450279
50.440829	1725.709363	19.455296
50.411054	1733.960517	19.460314
50.703817	1733.504871	19.465331
50.252249	1728.080992	19.470349
50.391962	1732.648091	19.475367
50.239367	1730.150502	19.480384
50.224350	1731.125052	19.485402
50.471345	1730.256801	19.490419
50.394570	1730.508803	19.495437
50.327525	1736.319953	19.500455
50.677958	1724.020776	19.505472
50.800219	1740.611344	19.510490
50.708562	1741.758778	19.515507
51.096933	1752.804066	19.520525
50.869789	1752.287353	19.525543
51.071298	1760.707641	19.530560
51.252921	1756.725240	19.535578
51.222042	1752.643378	19.540595
51.597453	1742.568355	19.545613
51.000218	1747.493200	19.550631
50.945939	1742.098980	19.555648
51.261964	1750.504590	19.560666
51.532271	1745.782530	19.565683
51.321987	1736.136380	19.570701
51.221944	1736.306796	19.575719
51.287768	1741.106313	19.580736
51.460023	1743.030031	19.585754
51.361506	1745.709136	19.590771
51.236698	1740.881333	19.595789
51.583470	1755.795901	19.600807
51.953453	1760.854188	19.605824
51.951213	1765.781077	19.610842
51.451455	1765.638177	19.615859
51.694930	1765.398493	19.620877
51.548426	1773.383809	19.625895
51.491477	1764.988749	19.630912
52.101633	1772.969868	19.635930
51.665203	1771.905056	19.640947
52.229283	1767.471775	19.645965
52.230195	1767.380314	19.650983
52.138156	1755.178410	19.656000
52.115090	1760.701846	19.661018
52.115039	1774.509062	19.666035
52.469762	1777.373232	19.671053
52.462343	1790.307426	19.676071
52.253284	1785.050904	19.681088
52.124755	1792.796738	19.686106
52.699812	1786.941593	19.691123
52.604122	1776.908339	19.696141
52.414258	1790.142346	19.701159
52.869462	1781.503431	19.706176
52.553057	1783.515859	19.711194
52.548506	1779.808599	19.716211
52.835634	1789.133934	19.721229
52.500379	1804.255719	19.726247
52.954420	1809.704887	19.731264
53.013568	1807.758160	19.736282
52.844298	1813.159205	19.741299
52.957146	1803.888754	19.746317
52.989209	1813.771381	19.751335
52.918917	1813.883515	19.756352
53.069265	1819.209551	19.761370
53.528237	1831.051806	19.766387
53.555362	1827.074508	19.771405
53.600615	1833.029155	19.776423
53.792896	1831.471965	19.781440
53.793134	1825.671588	19.786458
53.290427	1816.446476	19.791475
53.970709	1821.898294	19.796493
53.737059	1822.626015	19.801511
53.609895	1814.380723	19.806528
54.140253	1811.114051	19.811546
53.700854	1815.335823	19.816563
53.722697	1820.426240	19.821581
53.916002	1817.461361	19.826599
53.785225	1817.513483	19.831616
54.168427	1822.658095	19.836634
53.973495	1836.401024	19.841651
54.443798	1838.843254	19.846669
54.614938	1845.141234	19.851687
54.621482	1839.131582	19.856704
54.633749	1836.857626	19.861722
54.501212	1837.859947	19.866739
54.551441	1832.367375	19.871757
54.497529	1839.921726	19.876775
54.405307	1834.498671	19.881792
54.722531	1831.965790	19.886810
54.634508	1832.683461	19.891827
54.494417	1829.123529	19.896845
54.727800	1839.665968	19.901863
54.542209	1833.657829	19.906880
54.737286	1830.572748	19.911898
54.659596	1845.480892	19.916915
55.245513	1848.713033	19.921933
55.180341	1853.555067	19.926951
55.162670	1860.904962	19.931968
55.294710	1856.232804	19.936986
55.227784	1855.173575	19.942003
55.372140	1853.668026	19.947021
55.263284	1860.770178	19.952039
55.163629	1854.814927	19.957056
55.505858	1857.870409	19.962074
55.511599	1866.510582	19.967091
55.492545	1852.463667	19.972109
55.348680	1859.656479	19.977127
55.409717	1850.510839	19.982144
56.066609	1850.153137	19.987162
55.535278	1860.956666	19.992179
55.903512	1857.765723	19.997197
55.970990	1876.368945	20.002215
56.239575	1884.084549	20.007232
55.891213	1867.456868	20.012250
55.984094	1873.959553	20.017267
56.224615	1877.071901	20.022285
56.502849	1882.384357	20.027303
56.364672	1888.036211	20.032320
56.498090	1873.126070	20.037338
56.265032	1878.436077	20.042355
56.728695	1877.704504	20.047373
56.373737	1878.331189	20.052391
56.588644	1877.073439	20.057408
56.700702	1873.234391	20.062426
56.715696	1880.049016	20.067443
56.581275	1873.698371	20.072461
56.253202	1877.009703	20.077479
56.644217	1874.664149	20.082496
56.655571	1869.938191	20.087514
56.465656	1873.429990	20.092531
56.755559	1888.549189	20.097549
57.203212	1895.889769	20.102567
57.034749	1903.947991	20.107584
57.184174	1906.421254	20.112602
57.032502	1905.703431	20.117619
57.142350	1898.585729	20.122637
57.270355	1898.566001	20.127655
56.960818	1898.589149	20.132672
57.373610	1892.254287	20.137690
57.451945	1894.489300	20.142707
57.356910	1899.392803	20.147725
57.680225	1910.132727	20.152743
57.957612	1922.918529	20.157760
58.095449	1922.906737	20.162778
57.675132	1914.180004	20.167795
58.046461	1915.927574	20.172813
57.508968	1918.517256	20.177831
57.471161	1917.810107	20.182848
57.607478	1916.776036	20.187866
57.434470	1929.433145	20.192883
57.652199	1932.372320	20.197901
58.218114	1944.406290	20.202919
57.946402	1945.973104	20.207936
58.419392	1940.067526	20.212954
58.317225	1948.756098	20.217971
58.142948	1944.062179	20.222989
58.647208	1944.687640	20.228007
58.353135	1949.918802	20.233024
58.647195	1935.772577	20.238042
58.411769	1937.046552	20.243059
58.581971	1933.681294	20.248077
58.538867	1942.710974	20.253095
58.665506	1951.625865	20.258112
59.051258	1950.407784	20.263130
58.807558	1962.239604	20.268147
58.877383	1955.194386	20.273165
59.509258	1959.344077	20.278183
59.468758	1964.235950	20.283200
59.432405	1951.211014	20.288218
59.561532	1954.937188	20.293235
59.497265	1957.323804	20.298253
59.610554	1953.806451	20.303271
59.167154	1953.815725	20.308288
59.514004	1942.299626	20.313306
59.530059	1965.168281	20.318323
59.220331	1955.515403	20.323341
59.644507	1962.774455	20.328359
59.482254	1959.265287	20.333376
59.761694	1955.330730	20.338394
59.531945	1958.292241	20.343411
59.397102	1959.411697	20.348429
59.687871	1951.637778	20.353447
59.743884	1961.737672	20.358464
59.838012	1967.886734	20.363482
59.738562	1979.052298	20.368499
59.799946	1977.982551	20.373517
59.675660	1978.301916	20.378535
59.972296	1986.808490	20.383552
60.182619	1997.294649	20.388570
60.342715	2010.294443	20.393587
60.357675	2012.899114	20.398605
60.871531	2006.961904	20.403623
60.711575	1996.288412	20.408640
60.867267	2000.133541	20.413658
60.851012	2000.802174	20.418675
60.825076	2006.076815	20.423693
61.000855	1999.258089	20.428711
60.875999	2005.207720	20.433728
61.022772	1998.235715	20.438746
61.171627	1992.658308	20.443763
61.051588	2005.225169	20.448781
61.185656	1995.436898	20.453799
61.043147	2009.531574	20.458816
60.817142	2000.083396	20.463834
61.021295	1996.608694	20.468851
61.091633	2000.299848	20.473869
61.693903	2001.658006	20.478887
61.515885	2012.352966	20.483904
61.650314	2025.580838	20.488922
61.598734	2022.265874	20.493939
61.686443	2023.290721	20.498957
61.760761	2014.960315	20.503975
61.754267	2019.414547	20.508992
62.048520	2014.944319	20.514010
62.097963	2004.184569	20.519027
61.939038	2008.769832	20.524045
62.339101	1996.049315	20.529063
62.147762	2006.440221	20.534080
62.351120	2001.135203	20.539098
62.365259	2003.885173	20.544115
62.413804	2000.482037	20.549133
62.543330	1996.356209	20.554151
62.488154	2001.730079	20.559168
62.617114	2004.724114	20.564186
62.651978	2003.235601	20.569203
62.219408	2005.521769	20.574221
62.579654	1998.873147	20.579239
62.168295	1995.519525	20.584256
62.428371	1996.747917	20.589274
63.056180	2003.707027	20.594291
63.070656	2013.696649	20.599309
63.466394	2022.033169	20.604327
63.307163	2022.736688	20.609344
63.052246	1998.185570	20.614362
63.473023	2005.202163	20.619379
63.379922	2014.785640	20.624397
63.372104	1997.082294	20.629415
63.307954	2003.082436	20.634432
63.218220	2005.504582	20.639450
63.639712	2010.021569	20.644467
63.591568	2013.093675	20.649485
63.660097	2014.629613	20.654503
63.598884	2011.975739	20.659520
63.714748	2011.011122	20.664538
63.660648	2009.312388	20.669555
63.836063	2029.104530	20.674573
63.915063	2015.686031	20.679591
63.912925	2021.266252	20.684608
63.753796	2024.544995	20.689626
63.875518	2014.859626	20.694643
63.847057	2010.427020	20.699661
63.852043	2008.387714	20.704679
63.977821	2030.579781	20.709696
64.192837	2034.895382	20.714714
64.177016	2034.266860	20.719731
64.078456	2043.434619	20.724749
64.277692	2036.113590	20.729767
64.139609	2041.566654	20.734784
64.269267	2054.501789	20.739802
64.457772	2058.165089	20.744819
64.495273	2064.231479	20.749837
64.467047	2066.814478	20.754855
64.834315	2068.584787	20.759872
64.873461	2068.582049	20.764890
65.022532	2075.839797	20.769907
64.964995	2084.436276	20.774925
65.460465	2067.604440	20.779943
65.206585	2074.334764	20.784960
65.293694	2070.575301	20.789978
65.711249	2065.227447	20.794995
65.350037	2075.976215	20.800013
65.679837	2073.561268	20.805031
66.031066	2080.039584	20.810048
65.921634	2066.467341	20.815066
65.676705	2065.558894	20.820083
65.694622	2066.528336	20.825101
65.980002	2069.977731	20.830119
66.077223	2071.231484	20.835136
66.226079	2072.931653	20.840154
66.383864	2063.190147	20.845171
66.098926	2070.872087	20.850189
66.236925	2060.925372	20.855207
66.143073	2063.881521	20.860224
65.962206	2065.724548	20.865242
66.077834	2064.807303	20.870259
66.007814	2071.638394	20.875277
66.368969	2079.866712	20.880295
66.323614	2092.541933	20.885312
66.452802	2099.575558	20.890330
66.565428	2084.561175	20.895347
66.728917	2096.986123	20.900365
66.909101	2088.213148	20.905383
66.859210	2098.197058	20.910400
66.252914	2084.156182	20.915418
66.827673	2098.439067	20.920435
67.240036	2114.388341	20.925453
67.388222	2123.631338	20.930471
67.185965	2125.695462	20.935488
67.095720	2121.865767	20.940506
67.619986	2117.170345	20.945523
67.118150	2121.102093	20.950541
67.191509	2112.980084	20.955559
67.131153	2116.735794	20.960576
67.118031	2118.622140	20.965594
67.232054	2127.545395	20.970611
67.294011	2150.353489	20.975629
67.640463	2136.880634	20.980647
67.699816	2136.669614	20.985664
67.738981	2141.763737	20.990682
67.805428	2141.479025	20.995699
67.821179	2156.404440	21.000717
68.209559	2153.172437	21.005735
68.353485	2149.767046	21.010752
68.251201	2157.609942	21.015770
68.692600	2149.922943	21.020787
68.715165	2156.566073	21.025805
69.072562	2151.363267	21.030823
68.892224	2138.240686	21.035840
68.979192	2129.207636	21.040858
68.768185	2116.048819	21.045875
68.474485	2122.854792	21.050893
68.743781	2135.386374	21.055911
68.761151	2129.750497	21.060928
68.812209	2145.061743	21.065946
69.062141	2143.713311	21.070963
69.133685	2158.043032	21.075981
69.269522	2147.506442	21.080999
69.380617	2139.192344	21.086016
68.890212	2147.196654	21.091034
68.912151	2140.550157	21.096051
69.067459	2152.020163	21.101069
69.582826	2159.145172	21.106087
69.407905	2168.978167	21.111104
69.301575	2168.016576	21.116122
69.853428	2166.113025	21.121139
69.607420	2182.963323	21.126157
69.705879	2170.624173	21.131175
69.353329	2167.242426	21.136192
69.457412	2182.147797	21.141210
69.990452	2181.730475	21.146227
69.899265	2196.675729	21.151245
69.936507	2200.482535	21.156263
70.082807	2192.974014	21.161280
70.003945	2197.382750	21.166298
70.431337	2206.598099	21.171315
70.313909	2210.937099	21.176333
70.525512	2216.534599	21.181351
70.872375	2211.017818	21.186368
70.850066	2219.943410	21.191386
71.036160	2211.545014	21.196403
70.881834	2216.328440	21.201421
71.248303	2221.857646	21.206439
71.426816	2214.508211	21.211456
71.049407	2212.080272	21.216474
71.293561	2211.386019	21.221491
71.263982	2216.459307	21.226509
71.257979	2224.422948	21.231527
71.525608	2207.575960	21.236544
70.821317	2217.125309	21.241562
71.342178	2204.502608	21.246579
71.227283	2215.538174	21.251597
71.109155	2221.063929	21.256615
71.364134	2230.798465	21.261632
71.540634	2243.300388	21.266650
71.695703	2237.074963	21.271667
71.530861	2241.288802	21.276685
71.641292	2243.073870	21.281703
72.177960	2247.386783	21.286720
72.109427	2269.631491	21.291738
71.983019	2270.329908	21.296755
71.992261	2270.044633	21.301773
72.215605	2262.855465	21.306791
72.144565	2264.665632	21.311808
72.225900	2265.189686	21.316826
72.174485	2274.369158	21.321843
72.882108	2278.308305	21.326861
72.780749	2274.246765	21.331879
72.728614	2271.607220	21.336896
73.162591	2283.062326	21.341914
73.099349	2276.760418	21.346931
72.737546	2274.977016	21.351949
72.966916	2278.406769	21.356967
73.316428	2281.716825	21.361984
72.870960	2288.366599	21.367002
72.864654	2274.266873	21.372019
73.298577	2283.263482	21.377037
73.049359	2280.648308	21.382055
73.272784	2275.008707	21.387072
73.101260	2292.156796	21.392090
73.105498	2299.954766	21.397107
73.321052	2296.800142	21.402125
73.367727	2312.538270	21.407143
73.913864	2300.063054	21.412160
73.887656	2305.022227	21.417178
74.115454	2302.187606	21.422195
74.280424	2316.370357	21.427213
74.227493	2311.900459	21.432231
74.314592	2312.874922	21.437248
74.677131	2320.932714	21.442266
74.587863	2317.064952	21.447283
74.598579	2301.214140	21.452301
74.370908	2293.782738	21.457319
74.857702	2307.609246	21.462336
74.697407	2319.406223	21.467354
75.105450	2313.018302	21.472371
74.962291	2314.921759	21.477389
74.880375	2319.018558	21.482407
75.037878	2314.560079	21.487424
74.888472	2323.398207	21.492442
74.922348	2309.131242	21.497459
74.778412	2318.363014	21.502477
75.165895	2310.750617	21.507495
75.123200	2309.974782	21.512512
74.979286	2318.736309	21.517530
75.078688	2328.466717	21.522547
74.945633	2339.461002	21.527565
75.464571	2345.461997	21.532583
75.333582	2342.487560	21.537600
75.124361	2356.110028	21.542618
75.631374	2362.223346	21.547635
75.627291	2362.924813	21.552653
75.963475	2369.162566	21.557671
76.272051	2361.111127	21.562688
75.749521	2362.543448	21.567706
76.249358	2369.112348	21.572723
76.550164	2376.173014	21.577741
76.401892	2390.653918	21.582759
76.831442	2379.326646	21.587776
76.807816	2380.832780	21.592794
76.563714	2383.373691	21.597811
76.899580	2389.393737	21.602829
76.846886	2375.039206	21.607847
77.274709	2374.013376	21.612864
76.954090	2385.870074	21.617882
76.886099	2385.855613	21.622899
77.094108	2383.683663	21.627917
76.978322	2381.738863	21.632935
77.314594	2379.035672	21.637952
77.298238	2382.254380	21.642970
77.350640	2387.397008	21.647987
77.316022	2381.160039	21.653005
77.351791	2384.708323	21.658023
77.171836	2378.077391	21.663040
77.251384	2379.826253	21.668058
77.407318	2394.976208	21.673075
77.473158	2402.114495	21.678093
77.274174	2399.324214	21.683111
77.701059	2396.537481	21.688128
78.109593	2418.480865	21.693146
78.361885	2426.764166	21.698163
78.440265	2416.949619	21.703181
78.315194	2427.156870	21.708199
78.544714	2417.467124	21.713216
78.314767	2421.848942	21.718234
78.434106	2417.374288	21.723251
78.581241	2407.350214	21.728269
78.484406	2416.262259	21.733287
78.561578	2417.418166	21.738304
78.901436	2420.594043	21.743322
78.658999	2419.801962	21.748339
79.053875	2425.648721	21.753357
78.809218	2418.387180	21.758375
79.345111	2426.216044	21.763392
78.926824	2444.346344	21.768410
79.192853	2452.962054	21.773427
79.328913	2434.506838	21.778445
78.958059	2443.104930	21.783463
79.186326	2441.482121	21.788480
78.989947	2453.152251	21.793498
79.512635	2464.293842	21.798515
79.649633	2460.646458	21.803533
79.433871	2466.168554	21.808551
79.616922	2457.243464	21.813568
79.891798	2473.189217	21.818586
79.969784	2482.127728	21.823603
80.242996	2477.449209	21.828621
80.407748	2490.366571	21.833639
80.292457	2483.577200	21.838656
80.466510	2487.302803	21.843674
80.377694	2493.007127	21.848691
80.356733	2478.275163	21.853709
80.537460	2493.888431	21.858727
80.407051	2473.278076	21.863744
80.838100	2489.767611	21.868762
80.669310	2501.862696	21.873779
81.092504	2498.988153	21.878797
81.405586	2506.536143	21.883815
81.125156	2498.740459	21.888832
81.450903	2503.414501	21.893850
81.424583	2492.555792	21.898867
81.498148	2493.658614	21.903885
81.287266	2498.826486	21.908903
81.480969	2503.890340	21.913920
81.770946	2497.123078	21.918938
81.557014	2504.541666	21.923955
81.905648	2500.870792	21.928973
81.779345	2508.190526	21.933991
81.772325	2523.747839	21.939008
82.272497	2519.198086	21.944026
82.550842	2519.016086	21.949043
82.487374	2520.645207	21.954061
82.241536	2524.505625	21.959079
81.990253	2521.505702	21.964096
82.451327	2516.662214	21.969114
82.365119	2524.846774	21.974131
82.609201	2517.269241	21.979149
82.597111	2520.509401	21.984167
82.357386	2523.908088	21.989184
82.720785	2531.984777	21.994202
82.417959	2545.025474	21.999219
83.202463	2545.840872	22.004237
82.796421	2539.466003	22.009255
83.035128	2535.367238	22.014272
83.129887	2539.635409	22.019290
82.781048	2549.741860	22.024307
83.131333	2543.842566	22.029325
83.078343	2563.225861	22.034343
83.363587	2572.987431	22.039360
83.330163	2562.006702	22.044378
83.050001	2570.994707	22.049395
83.589750	2567.284596	22.054413
83.580447	2584.414019	22.059431
84.046746	2587.093680	22.064448
84.270970	2595.495046	22.069466
84.187004	2593.633636	22.074483
84.401277	2588.572917	22.079501
83.906787	2582.218116	22.084519
84.285172	2590.270406	22.089536
84.556065	2589.814991	22.094554
84.735877	2603.844169	22.099571
84.790147	2607.607383	22.104589
84.849806	2615.778741	22.109607
84.650543	2618.019193	22.114624
84.783603	2613.270934	22.119642
84.585258	2616.672664	22.124659
84.823048	2618.046591	22.129677
84.777107	2614.989434	22.134695
84.972913	2619.276608	22.139712
85.234898	2621.451558	22.144730
85.159338	2634.857753	22.149747
85.341289	2632.636178	22.154765
85.670442	2623.880777	22.159783
85.513580	2631.145354	22.164800
85.889731	2630.840820	22.169818
85.806746	2651.825836	22.174835
86.133616	2655.338318	22.179853
85.839724	2658.628690	22.184871
85.938743	2660.368236	22.189888
86.190136	2653.360751	22.194906
86.210057	2657.596418	22.199923
86.195669	2647.041895	22.204941
86.325040	2649.673030	22.209959
86.373194	2654.548133	22.214976
86.714102	2663.991794	22.219994
86.469793	2687.454216	22.225011
86.786171	2678.590316	22.230029
86.543989	2679.404611	22.235047
86.875228	2675.464990	22.240064
86.744075	2678.789993	22.245082
86.765246	2684.805483	22.250099
86.950583	2691.852691	22.255117
87.233598	2700.096618	22.260135
87.199819	2693.887814	22.265152
87.456855	2695.059920	22.270170
87.632846	2703.263703	22.275187
87.625268	2701.545036	22.280205
87.943678	2702.521380	22.285223
87.952645	2716.047029	22.290240
88.092866	2711.739478	22.295258
87.767021	2724.603994	22.300275
88.206686	2721.329189	22.305293
87.853863	2728.905204	22.310311
88.143120	2733.222041	22.315328
88.242079	2720.326969	22.320346
88.261876	2720.961612	22.325363
88.544325	2717.294686	22.330381
88.907434	2722.767762	22.335399
89.083515	2718.602960	22.340416
89.101985	2720.181470	22.345434
89.087649	2715.295174	22.350451
89.004818	2707.951511	22.355469
88.926871	2707.951224	22.360487
89.122206	2715.110503	22.365504
89.311553	2714.358488	22.370522
89.489360	2717.436563	22.375539
89.197134	2717.169813	22.380557
89.545241	2714.792960	22.385575
89.458137	2726.045436	22.390592
89.418625	2712.054685	22.395610
89.491755	2715.101717	22.400627
89.858914	2709.483787	22.405645
90.155477	2723.147716	22.410663
89.876384	2729.550824	22.415680
90.159889	2735.967335	22.420698
90.688900	2735.165592	22.425715
90.820017	2732.813052	22.430733
90.841187	2723.004090	22.435751
90.018106	2725.104975	22.440768
90.616256	2727.398026	22.445786
90.421269	2732.197388	22.450803
90.668836	2734.993184	22.455821
90.734189	2733.916463	22.460839
90.759968	2740.126929	22.465856
90.849677	2733.116183	22.470874
90.830447	2734.807869	22.475891
90.906407	2750.803776	22.480909
91.018533	2757.988652	22.485927
91.209009	2758.404202	22.490944
91.379956	2748.041688	22.495962
91.381561	2759.397148	22.500979
91.857203	2768.879853	22.505997
91.620286	2779.685434	22.511015
91.762188	2782.286232	22.516032
92.047659	2776.434827	22.521050
91.794845	2775.615940	22.526067
91.960971	2777.035755	22.531085
91.898756	2773.371983	22.536103
92.084352	2791.462264	22.541120
92.429801	2790.562855	22.546138
92.506883	2803.244763	22.551155
92.530162	2805.472682	22.556173
92.841496	2799.869727	22.561191
92.690534	2800.029144	22.566208
92.956091	2808.556730	22.571226
92.589268	2799.843325	22.576243
93.067764	2806.832311	22.581261
93.196731	2805.575254	22.586279
93.383529	2818.912334	22.591296
93.306040	2819.060311	22.596314
93.423762	2813.130861	22.601331
93.422356	2821.097208	22.606349
93.763794	2816.673089	22.611367
93.816972	2815.781310	22.616384
93.840306	2810.627170	22.621402
93.949335	2812.674467	22.626419
93.919715	2815.683860	22.631437
94.146534	2811.432236	22.636455
94.173080	2830.866557	22.641472
94.639890	2835.569221	22.646490
94.551492	2838.070173	22.651507
94.624029	2843.591683	22.656525
94.592243	2839.168858	22.661543
94.674809	2837.890617	22.666560
94.942667	2841.822615	22.671578
94.880366	2837.044749	22.676595
94.707902	2844.485425	22.681613
95.109840	2838.413878	22.686631
94.750458	2839.622000	22.691648
94.899851	2832.377841	22.696666
94.929418	2838.499382	22.701683
94.870019	2850.161067	22.706701
95.211495	2854.223629	22.711719
95.321395	2859.234354	22.716736
95.526328	2855.768835	22.721754
95.470388	2856.235377	22.726771
95.490109	2868.787395	22.731789
95.455937	2881.114262	22.736807
95.453722	2891.551979	22.741824
95.780827	2884.147575	22.746842
96.156888	2895.186021	22.751859
96.515231	2906.369256	22.756877
96.661300	2903.424179	22.761895
96.586600	2903.552786	22.766912
96.603898	2896.354416	22.771930
96.904258	2894.960204	22.776947
96.803182	2904.636924	22.781965
96.884226	2896.352404	22.786983
96.752943	2908.479796	22.792000
96.528342	2896.566020	22.797018
96.846152	2915.453267	22.802035
96.781249	2925.077025	22.807053
97.454038	2916.517311	22.812071
97.060023	2923.670593	22.817088
97.415120	2919.534683	22.822106
97.755023	2934.877378	22.827123
97.571875	2949.351538	22.832141
97.851774	2952.094993	22.837159
97.612773	2943.311119	22.842176
98.173104	2944.290841	22.847194
98.251683	2948.637375	22.852211
98.098707	2948.323691	22.857229
98.428688	2949.291936	22.862247
98.643239	2966.806632	22.867264
98.523086	2966.295316	22.872282
98.489284	2963.337204	22.877299
98.481377	2969.546682	22.882317
98.704894	2965.065140	22.887335
98.873935	2964.518267	22.892352
99.119695	2968.810372	22.897370
98.915748	2976.540054	22.902387
98.979050	2980.428183	22.907405
99.612508	2978.038430	22.912423
99.463160	2989.288137	22.917440
99.742104	2989.241753	22.922458
99.611939	2986.510099	22.927475
99.686542	2992.179670	22.932493
99.627170	2982.824960	22.937511
100.062011	2995.025229	22.942528
99.784723	3007.626743	22.947546
100.382796	3009.064539	22.952563
100.147468	3015.173728	22.957581
99.925444	3010.076668	22.962599
100.039170	3014.499805	22.967616
100.029833	3022.928268	22.972634
100.566869	3034.790730	22.977651
100.554634	3034.041682	22.982669
100.680066	3035.587785	22.987687
100.861089	3034.180582	22.992704
100.899639	3041.799946	22.997722
101.391419	3042.582043	23.002739
101.136262	3056.691922	23.007757
101.428616	3056.993779	23.012775
101.326637	3052.641796	23.017792
101.652888	3051.028926	23.022810
101.779263	3045.984920	23.027827
101.724819	3046.236618	23.032845
101.888289	3035.875103	23.037863
101.948253	3041.307104	23.042880
101.997895	3044.496718	23.047898
102.131519	3036.933008	23.052915
102.127300	3041.327173	23.057933
102.157915	3043.001660	23.062951
102.788398	3054.496102	23.067968
102.180051	3056.734020	23.072986
102.419769	3050.873869	23.078003
102.448793	3065.141502	23.083021
102.812110	3062.550776	23.088039
102.788643	3068.437631	23.093056
103.065584	3083.957531	23.098074
102.883581	3085.649344	23.103091
103.353565	3090.035969	23.108109
103.241140	3095.024564	23.113127
103.045240	3090.289524	23.118144
103.464963	3092.957578	23.123162
103.233108	3090.188086	23.128179
103.231407	3105.801886	23.133197
103.597486	3109.668152	23.138215
103.687745	3115.471037	23.143232
103.783751	3133.521958	23.148250
104.372614	3128.166057	23.153267
104.108005	3134.434495	23.158285
104.394802	3136.447840	23.163303
103.879885	3141.540143	23.168320
104.266512	3140.246102	23.173338
104.730081	3145.492207	23.178355
105.020732	3147.713258	23.183373
105.210788	3148.138351	23.188391
105.293333	3150.334992	23.193408
105.085338	3157.806579	23.198426
105.622323	3153.544457	23.203443
105.334488	3158.563536	23.208461
105.509701	3145.470075	23.213479
105.458175	3148.438749	23.218496
105.467649	3154.109043	23.223514
105.541397	3165.557679	23.228531
105.779453	3174.793539	23.233549
105.511651	3171.616177	23.238567
105.973427	3172.538666	23.243584
106.154743	3184.885846	23.248602
106.017001	3189.597512	23.253619
106.349470	3208.075644	23.258637
106.261859	3208.136828	23.263655
106.400696	3209.403119	23.268672
106.507382	3208.237874	23.273690
106.884938	3214.829283	23.278707
106.718330	3224.226012	23.283725
106.744071	3224.528352	23.288743
107.027507	3226.425452	23.293760
106.649917	3223.363016	23.298778
107.055959	3235.870923	23.303795
107.447873	3244.123396	23.308813
107.281381	3236.603173	23.313831
107.503351	3245.289248	23.318848
107.424765	3250.828099	23.323866
108.118228	3258.105722	23.328883
107.931904	3273.350736	23.333901
108.063112	3271.910241	23.338919
108.145877	3272.383604	23.343936
108.164306	3278.327128	23.348954
108.116244	3271.157721	23.353971
108.449868	3277.923269	23.358989
108.582123	3290.858892	23.364007
109.378128	3295.194809	23.369024
108.924644	3300.384900	23.374042
109.163271	3287.524488	23.379059
109.355646	3297.439784	23.384077
109.296474	3281.261279	23.389095
109.557724	3283.903536	23.394112
109.157194	3288.637206	23.399130
109.511296	3280.758170	23.404147
109.281129	3295.347237	23.409165
109.150059	3286.925129	23.414183
109.899431	3290.630762	23.419200
109.512861	3304.660299	23.424218
109.727486	3310.289232	23.429235
109.591367	3311.749835	23.434253
109.944507	3308.791389	23.439271
110.294306	3325.136536	23.444288
110.351797	3337.446288	23.449306
110.360622	3336.927505	23.454323
110.369558	3339.182972	23.459341
110.502881	3342.713100	23.464359
111.049298	3343.145839	23.469376
111.064731	3358.075458	23.474394
111.009501	3362.887946	23.479411
110.784065	3367.796370	23.484429
111.179234	3363.136509	23.489447
111.289979	3366.477631	23.494464
111.481227	3377.579866	23.499482
111.894529	3386.068944	23.504499
111.985303	3385.928765	23.509517
111.999738	3381.678512	23.514535
111.895797	3391.507436	23.519552
111.845064	3383.902848	23.524570
112.217708	3385.580926	23.529587
112.065972	3382.978817	23.534605
112.633904	3395.363789	23.539623
112.759373	3389.792747	23.544640
112.818580	3405.728722	23.549658
112.813974	3408.544949	23.554675
113.089572	3402.821126	23.559693
112.768231	3398.679958	23.564711
113.110675	3410.067978	23.569728
113.006402	3415.639285	23.574746
113.476155	3422.462598	23.579763
113.428398	3419.601269	23.584781
113.326146	3423.054468	23.589799
113.303464	3425.229652	23.594816
113.625721	3430.147506	23.599834
114.009788	3439.575390	23.604851
113.859473	3438.620578	23.609869
114.041867	3443.692772	23.614887
114.048161	3443.745648	23.619904
114.294938	3456.950773	23.624922
114.558599	3461.202336	23.629939
114.708063	3463.044572	23.634957
114.785236	3468.934826	23.639975
114.867015	3461.975530	23.644992
114.519809	3468.916587	23.650010
114.990098	3482.803386	23.655027
115.436250	3488.708791	23.660045
115.069916	3494.330392	23.665063
115.336234	3494.768870	23.670080
115.217811	3492.701267	23.675098
115.264176	3496.462742	23.680115
115.491724	3509.841334	23.685133
115.386854	3526.229047	23.690151
115.798466	3516.724982	23.695168
115.686135	3536.699304	23.700186
115.904422	3539.935341	23.705203
116.356145	3541.121379	23.710221
116.122393	3541.473594	23.715239
116.707050	3534.334977	23.720256
116.954448	3534.113601	23.725274
116.932085	3519.179005	23.730291
117.084202	3533.260566	23.735309
117.474389	3538.376183	23.740327
117.832661	3530.101864	23.745344
117.778197	3527.389904	23.750362
117.593365	3520.595186	23.755379
117.882681	3520.392533	23.760397
117.621939	3521.885180	23.765415
117.644981	3513.041292	23.770432
117.534821	3531.023711	23.775450
117.773818	3535.626313	23.780467
118.168712	3537.749122	23.785485
117.765381	3548.903004	23.790503
117.906365	3542.897100	23.795520
118.731466	3560.778122	23.800538
118.144387	3570.006937	23.805555
118.506369	3566.936605	23.810573
118.510588	3572.636254	23.815591
118.556124	3567.790905	23.820608
118.951169	3592.288040	23.825626
118.921550	3587.586947	23.830643
119.261437	3584.217057	23.835661
119.270629	3596.013732	23.840679
119.613593	3587.558710	23.845696
119.227475	3598.081858	23.850714
119.638146	3608.013838	23.855731
120.028176	3617.090547	23.860749
119.982737	3622.425510	23.865767
119.977432	3621.075678	23.870784
119.858282	3625.162790	23.875802
120.055587	3639.998046	23.880819
120.109312	3644.017215	23.885837
119.788384	3644.373536	23.890855
120.629868	3668.864391	23.895872
120.449529	3669.549164	23.900890
120.803002	3676.232867	23.905907
121.130595	3658.737629	23.910925
121.327332	3681.558246	23.915943
121.715369	3688.852035	23.920960
121.812754	3687.265275	23.925978
121.969988	3691.760710	23.930995
121.965734	3685.742653	23.936013
121.606420	3690.135450	23.941031
121.733367	3685.899170	23.946048
121.930005	3692.446329	23.951066
121.849168	3686.859973	23.956083
122.266473	3690.380675	23.961101
122.321989	3699.803036	23.966119
122.320046	3703.067079	23.971136
122.362876	3713.902257	23.976154
122.630752	3719.156906	23.981171
122.448081	3729.850453	23.986189
122.855481	3741.206477	23.991207
122.809392	3740.137578	23.996224
123.045670	3745.485529	24.001242
123.105617	3752.675770	24.006259
123.296670	3753.069161	24.011277
123.491258	3758.158483	24.016295
123.387726	3758.600895	24.021312
124.040286	3769.079208	24.026330
123.752124	3779.615616	24.031347
124.074915	3777.084756	24.036365
123.999175	3789.324029	24.041383
124.439785	3783.896332	24.046400
124.465132	3782.207154	24.051418
124.551869	3786.303277	24.056435
124.589674	3793.070890	24.061453
124.785350	3812.887094	24.066471
124.780459	3806.645002	24.071488
125.125097	3802.990270	24.076506
124.982239	3809.565079	24.081523
125.228406	3814.608511	24.086541
125.263756	3828.639044	24.091559
125.318247	3836.047950	24.096576
125.587308	3830.384979	24.101594
125.279393	3836.142777	24.106611
125.384605	3843.079819	24.111629
125.530838	3857.604424	24.116647
125.843265	3856.552294	24.121664
126.316084	3860.301105	24.126682
126.113754	3870.729515	24.131699
126.461610	3869.201586	24.136717
126.474935	3881.505961	24.141735
126.735321	3888.702925	24.146752
127.566521	3883.766731	24.151770
127.483636	3901.738960	24.156787
127.422361	3906.438908	24.161805
127.239250	3904.097265	24.166823
127.477957	3892.192758	24.171840
127.634746	3900.583141	24.176858
127.426841	3891.355241	24.181875
127.726071	3898.520911	24.186893
127.768717	3922.562047	24.191911
128.324557	3920.503042	24.196928
128.364714	3915.295466	24.201946
128.297082	3914.526600	24.206963
128.380282	3910.297079	24.211981
128.623587	3928.344800	24.216999
128.658109	3933.765250	24.222016
129.082997	3936.483128	24.227034
128.755276	3947.616014	24.232051
129.114451	3939.716965	24.237069
128.964145	3947.063113	24.242087
129.217958	3951.584609	24.247104
129.431844	3959.161280	24.252122
129.590447	3968.419388	24.257139
129.839242	3969.930584	24.262157
129.853352	3982.803035	24.267175
130.044109	3992.144524	24.272192
130.283088	3993.177497	24.277210
130.136116	3995.138535	24.282227
130.631577	3985.498076	24.287245
130.573205	3988.026074	24.292263
130.710322	4001.539050	24.297280
131.074670	4004.051737	24.302298
130.963468	4017.044724	24.307315
131.208485	4008.358566	24.312333
130.972206	4016.721825	24.317351
131.379969	4005.996623	24.322368
131.575930	4012.847007	24.327386
131.485668	4020.969751	24.332403
131.847774	4013.635188	24.337421
131.634703	4031.201716	24.342439
132.012160	4027.396641	24.347456
132.278087	4024.382220	24.352474
132.263268	4038.423884	24.357491
132.320409	4050.592145	24.362509
132.783723	4048.781097	24.367527
132.592712	4051.320286	24.372544
132.816804	4050.045177	24.377562
132.506993	4054.651294	24.382579
132.949196	4065.970542	24.387597
132.569151	4076.701336	24.392615
133.277790	4081.404555	24.397632
133.456279	4077.636759	24.402650
133.069166	4082.179168	24.407667
133.327561	4106.212207	24.412685
133.594602	4110.173019	24.417703
133.930111	4114.969059	24.422720
134.175843	4107.854580	24.427738
134.043063	4124.423933	24.432755
134.567771	4124.980015	24.437773
134.318849	4125.034753	24.442791
134.408385	4122.044622	24.447808
134.785159	4112.555139	24.452826
134.779334	4130.856478	24.457843
134.985690	4139.387602	24.462861
135.029262	4139.974404	24.467879
134.818615	4142.204189	24.472896
135.321187	4144.464966	24.477914
135.082008	4160.545909	24.482931
135.536944	4165.020363	24.487949
135.782004	4175.085756	24.492967
135.754438	4176.542152	24.497984
136.009570	4176.089155	24.503002
136.297572	4185.200974	24.508019
136.355191	4182.509340	24.513037
136.554840	4178.785574	24.518055
136.365560	4185.342496	24.523072
136.799352	4192.534678	24.528090
136.932884	4200.177619	24.533107
137.095032	4197.438145	24.538125
137.355929	4198.294120	24.543143
137.583537	4210.322321	24.548160
137.783645	4202.687803	24.553178
138.113539	4210.811500	24.558195
138.308568	4219.754746	24.563213
138.423875	4216.571209	24.568231
138.376976	4222.462088	24.573248
138.435023	4208.647521	24.578266
138.461180	4225.024937	24.583283
138.782895	4220.628799	24.588301
138.597297	4216.608341	24.593319
138.275362	4217.848597	24.598336
138.930755	4222.332889	24.603354
138.672949	4245.493274	24.608371
139.119030	4242.880029	24.613389
139.215086	4246.536078	24.618407
138.812788	4253.826893	24.623424
139.011508	4256.460093	24.628442
139.211503	4275.581742	24.633459
139.395755	4295.813734	24.638477
139.698899	4293.263768	24.643495
139.605287	4304.013227	24.648512
139.704574	4318.321413	24.653530
139.945994	4328.403239	24.658547
140.123877	4335.486974	24.663565
140.446293	4345.953898	24.668583
140.392793	4356.274194	24.673600
141.156649	4350.508775	24.678618
141.247093	4375.231153	24.683635
141.349567	4379.744755	24.688653
141.733657	4373.621818	24.693671
141.859084	4385.713389	24.698688
141.927027	4372.645211	24.703706
141.971845	4371.385366	24.708723
142.195834	4370.766771	24.713741
142.377509	4369.201547	24.718759
142.118466	4369.368333	24.723776
142.834455	4377.198424	24.728794
142.726700	4387.135797	24.733811
142.700367	4392.755241	24.738829
142.814492	4391.298379	24.743847
142.551331	4392.854599	24.748864
143.026108	4386.351402	24.753882
142.825368	4390.142067	24.758899
142.943900	4404.901838	24.763917
143.335922	4412.656129	24.768935
143.195323	4416.184928	24.773952
143.970945	4420.710522	24.778970
143.751077	4433.875387	24.783987
143.581223	4446.492738	24.789005
144.045766	4439.710200	24.794023
144.071095	4452.398170	24.799040
144.861424	4460.036810	24.804058
144.710795	4469.075028	24.809075
144.606033	4472.595102	24.814093
144.817113	4473.196868	24.819111
144.861263	4475.841540	24.824128
145.281974	4477.142945	24.829146
145.172283	4485.174231	24.834163
144.922124	4497.516891	24.839181
145.447776	4500.736812	24.844199
145.369111	4514.962386	24.849216
145.364309	4512.390894	24.854234
145.830099	4522.592559	24.859251
146.091134	4536.673726	24.864269
146.019965	4539.115415	24.869287
145.884602	4551.850568	24.874304
146.741152	4554.570776	24.879322
146.661857	4561.495787	24.884339
146.711852	4567.425352	24.889357
147.019233	4584.665189	24.894375
147.139717	4594.027399	24.899392
147.236441	4591.863045	24.904410
147.385752	4593.206713	24.909427
147.599853	4609.166980	24.914445
148.127873	4609.804629	24.919463
147.888770	4613.935889	24.924480
148.000944	4617.668413	24.929498
148.570892	4639.071731	24.934515
148.472314	4647.764200	24.939533
148.576940	4638.995438	24.944551
148.679077	4639.484760	24.949568
148.993290	4639.215094	24.954586
149.085380	4648.887924	24.959603
149.247038	4643.938985	24.964621
149.586404	4644.284055	24.969639
149.481194	4648.908969	24.974656
149.523508	4653.943342	24.979674
149.877902	4668.092143	24.984691
149.971794	4674.589372	24.989709
149.993255	4677.041909	24.994727
149.561392	4682.443660	24.999744
150.121991	4682.760600	25.004762
150.107364	4687.431393	25.009779
150.272181	4701.410882	25.014797
151.226064	4714.036534	25.019815
150.833489	4728.147014	25.024832
151.394595	4722.750782	25.029850
151.503842	4723.785057	25.034867
151.408116	4718.854076	25.039885
151.733593	4729.655326	25.044903
151.906365	4740.991695	25.049920
151.974601	4739.968065	25.054938
152.084019	4743.442219	25.059955
152.348399	4741.652609	25.064973
152.581951	4736.051700	25.069991
152.620122	4735.039065	25.075008
152.777988	4742.388057	25.080026
152.760056	4753.024995	25.085043
152.509957	4761.163486	25.090061
153.181592	4752.303234	25.095079
152.794431	4759.001646	25.100096
152.975214	4779.351506	25.105114
153.451803	4777.405753	25.110131
153.414240	4792.859303	25.115149
153.575610	4795.340576	25.120167
153.676017	4810.633779	25.125184
153.901562	4812.278081	25.130202
153.865913	4822.191840	25.135219
154.145551	4838.243110	25.140237
154.664206	4838.178344	25.145255
154.981837	4835.799651	25.150272
154.895356	4842.328179	25.155290
155.340328	4842.221225	25.160307
155.142057	4862.658602	25.165325
155.329326	4851.856756	25.170343
155.321399	4851.255314	25.175360
155.648995	4861.254580	25.180378
155.758542	4866.827763	25.185395
155.800010	4876.767423	25.190413
155.903316	4877.278665	25.195431
156.307234	4896.811121	25.200448
156.235136	4895.326397	25.205466
156.301124	4899.871062	25.210483
156.100377	4913.061705	25.215501
156.696752	4924.878302	25.220519
156.987107	4938.759518	25.225536
156.987830	4943.753100	25.230554
157.626985	4957.949330	25.235571
157.169628	4956.537208	25.240589
157.301360	4963.956645	25.245607
157.586891	4978.716135	25.250624
157.504062	4992.058925	25.255642
158.076362	5012.881531	25.260659
157.962457	5015.418319	25.265677
158.636044	5009.751973	25.270695
158.673135	5018.818055	25.275712
158.513668	5041.872607	25.280730
159.123944	5049.223886	25.285747
159.176493	5045.346084	25.290765
159.237190	5057.265107	25.295783
159.526562	5066.487635	25.300800
159.484629	5067.144596	25.305818
159.774529	5065.470927	25.310835
159.838905	5079.018127	25.315853
160.123232	5087.635410	25.320871
160.531923	5084.374479	25.325888
160.630473	5083.705948	25.330906
160.963092	5093.947609	25.335923
161.091625	5105.202713	25.340941
161.607383	5103.695890	25.345959
161.528576	5104.071355	25.350976
161.561348	5106.156038	25.355994
162.042383	5101.993716	25.361011
161.396238	5104.995314	25.366029
161.864266	5100.743479	25.371047
161.568301	5101.313734	25.376064
161.870506	5117.828896	25.381082
162.186765	5119.714778	25.386099
161.823511	5136.115766	25.391117
162.318670	5140.293807	25.396135
162.840503	5144.827535	25.401152
162.969557	5156.754920	25.406170
163.017655	5145.520034	25.411187
162.820251	5162.068831	25.416205
163.380340	5165.195130	25.421223
163.433432	5169.432534	25.426240
163.062433	5174.790233	25.431258
163.785084	5180.365909	25.436275
163.746335	5200.112810	25.441293
164.190461	5202.808949	25.446311
164.410643	5200.227583	25.451328
164.133077	5203.790484	25.456346
164.451870	5216.234440	25.461363
164.400361	5229.623031	25.466381
165.097090	5213.022088	25.471399
165.278717	5226.573239	25.476416
165.295549	5239.143135	25.481434
165.679052	5233.644988	25.486451
165.523462	5232.889760	25.491469
165.768594	5228.978778	25.496487
166.179914	5237.601613	25.501504
166.440752	5257.270368	25.506522
166.493478	5253.256765	25.511539
166.908279	5249.783368	25.516557
166.755565	5256.325513	25.521575
166.915877	5257.307679	25.526592
166.999036	5254.690822	25.531610
167.345659	5263.478410	25.536627
167.605042	5279.425904	25.541645
167.391701	5280.554627	25.546663
167.538411	5273.436171	25.551680
167.236312	5282.621479	25.556698
167.842964	5286.362381	25.561715
167.999478	5298.579139	25.566733
168.329863	5312.672208	25.571751
168.100530	5324.387198	25.576768
168.152677	5335.010408	25.581786
168.306341	5335.810535	25.586803
168.907408	5356.720598	25.591821
168.932853	5353.137350	25.596839
169.212858	5367.001566	25.601856
169.313479	5372.468973	25.606874
169.640988	5375.416877	25.611891
169.870555	5378.468413	25.616909
169.932791	5397.802085	25.621927
170.566902	5398.208604	25.626944
170.255491	5402.256604	25.631962
170.797318	5396.588559	25.636979
170.859083	5401.673772	25.641997
170.690273	5415.364850	25.647015
171.005231	5417.958028	25.652032
170.911518	5423.742950	25.657050
171.285553	5431.213236	25.662067
171.255133	5450.135258	25.667085
171.310679	5450.325673	25.672103
171.783795	5457.556431	25.677120
171.487238	5474.045191	25.682138
171.987764	5469.677733	25.687156
172.531243	5505.006521	25.692173
172.718353	5502.256653	25.697191
172.767487	5499.010594	25.702208
172.846444	5496.457488	25.707226
173.354352	5514.992737	25.712244
173.223864	5525.000559	25.717261
173.589049	5531.777824	25.722279
173.571002	5529.804838	25.727296
173.476639	5538.171952	25.732314
173.935094	5540.285107	25.737332
174.304054	5549.785892	25.742349
174.271474	5549.491294	25.747367
174.458693	5562.789302	25.752384
174.504353	5571.412407	25.757402
174.982428	5577.512395	25.762420
174.996723	5571.838044	25.767437
174.954806	5577.163564	25.772455
175.724928	5583.745229	25.777472
175.194207	5602.303384	25.782490
175.457742	5600.769503	25.787508
175.797441	5605.890416	25.792525
175.520102	5608.323311	25.797543
175.918573	5615.512092	25.802560
176.185109	5624.025077	25.807578
176.214057	5628.200060	25.812596
176.626676	5632.558365	25.817613
176.607728	5630.673891	25.822631
177.279216	5637.466640	25.827648
177.358197	5648.351007	25.832666
177.150860	5650.286899	25.837684
177.569745	5653.242718	25.842701
177.797628	5666.102020	25.847719
177.718177	5676.310312	25.852736
177.828582	5683.616571	25.857754
178.067424	5690.820765	25.862772
178.114690	5702.439270	25.867789
177.844878	5714.634298	25.872807
178.506840	5727.006237	25.877824
178.459707	5743.405902	25.882842
178.819123	5751.683525	25.887860
179.229145	5756.537848	25.892877
179.494020	5760.893934	25.897895
179.903659	5782.781268	25.902912
180.036917	5783.114260	25.907930
180.114141	5793.235093	25.912948
180.141060	5791.412907	25.917965
180.564793	5815.712878	25.922983
180.886356	5809.406645	25.928000
180.688221	5810.905510	25.933018
181.345256	5816.033895	25.938036
181.098567	5828.190675	25.943053
181.279912	5838.914016	25.948071
181.686136	5831.903299	25.953088
181.971811	5841.742334	25.958106
182.136476	5850.306008	25.963124
182.175679	5852.162501	25.968141
182.324667	5864.690157	25.973159
182.637368	5866.055832	25.978176
183.036234	5879.545239	25.983194
182.962515	5889.626494	25.988212
183.325596	5876.040951	25.993229
183.223948	5888.484538	25.998247
183.413555	5881.188710	26.003264
183.208207	5899.677569	26.008282
183.493041	5905.851946	26.013300
183.738880	5921.972569	26.018317
183.813260	5933.290279	26.023335
184.283531	5924.659682	26.028352
184.411993	5952.351817	26.033370
184.585954	5948.533836	26.038388
185.170505	5965.772869	26.043405
184.526864	5970.245200	26.048423
184.992221	5978.935733	26.053440
185.220059	5988.692310	26.058458
185.690671	5992.868060	26.063476
185.794557	6011.510911	26.068493
185.647545	6017.531596	26.073511
185.931154	6021.029382	26.078528
186.150655	6032.482391	26.083546
186.403836	6034.567588	26.088564
186.398144	6047.469839	26.093581
186.519810	6053.448705	26.098599
186.771358	6067.788226	26.103616
186.615978	6075.136022	26.108634
187.071196	6088.708353	26.113652
187.220045	6088.682223	26.118669
187.202148	6113.796316	26.123687
187.614399	6107.810467	26.128704
188.387932	6125.863054	26.133722
188.343369	6141.823902	26.138740
188.488445	6138.218717	26.143757
188.414862	6145.029802	26.148775
188.725180	6148.826492	26.153792
188.933685	6163.021270	26.158810
188.954320	6163.283418	26.163828
189.312799	6177.328591	26.168845
189.697236	6187.818492	26.173863
189.968680	6196.826577	26.178880
190.139901	6209.625638	26.183898
189.894149	6227.376146	26.188916
189.891326	6217.206011	26.193933
190.303219	6233.133754	26.198951
190.235960	6247.194757	26.203968
190.544189	6252.393356	26.208986
191.000045	6268.989813	26.214004
191.361529	6271.039236	26.219021
191.009473	6287.404789	26.224039
191.370118	6296.054957	26.229056
192.032524	6310.845241	26.234074
192.144647	6322.008952	26.239092
192.184609	6323.205628	26.244109
192.470658	6337.678883	26.249127
192.809622	6340.476798	26.254144
192.985943	6346.718727	26.259162
193.118144	6351.966857	26.264180
193.580653	6364.682797	26.269197
193.427898	6370.837073	26.274215
193.749991	6372.927364	26.279232
194.392187	6382.146137	26.284250
194.420386	6381.191784	26.289268
194.890074	6389.613522	26.294285
194.306564	6386.105939	26.299303
194.772104	6393.837008	26.304320
195.333394	6402.449675	26.309338
195.071293	6408.589422	26.314356
195.302104	6407.717163	26.319373
195.493295	6409.903600	26.324391
195.726436	6419.779537	26.329408
195.649739	6428.317926	26.334426
195.543663	6438.477125	26.339444
195.956741	6454.625846	26.344461
195.722365	6456.888015	26.349479
196.202901	6478.503139	26.354496
196.504194	6489.890038	26.359514
196.670783	6507.683947	26.364532
197.142409	6512.456279	26.369549
197.002346	6527.030750	26.374567
197.386840	6537.868083	26.379584
197.956526	6544.257180	26.384602
197.967092	6560.380273	26.389620
198.425246	6561.713887	26.394637
198.784305	6559.653667	26.399655
198.853119	6564.141486	26.404672
199.049995	6569.944663	26.409690
198.910269	6578.919093	26.414708
199.758379	6574.383620	26.419725
199.569463	6588.650073	26.424743
199.665712	6583.420375	26.429760
200.219247	6597.943738	26.434778
200.208454	6597.292176	26.439796
200.192824	6590.264775	26.444813
200.317961	6604.299255	26.449831
200.234589	6600.505419	26.454848
200.797091	6612.505170	26.459866
200.434376	6617.413741	26.464884
201.231439	6637.729709	26.469901
201.093592	6648.080217	26.474919
201.419472	6648.616836	26.479936
201.502435	6653.055123	26.484954
201.461563	6674.682210	26.489972
202.544308	6677.484335	26.494989
202.316079	6693.329049	26.500007
202.733999	6695.328697	26.505024
202.706105	6710.261503	26.510042
202.766652	6712.452533	26.515060
203.030419	6716.307098	26.520077
203.094638	6727.633195	26.525095
203.225393	6741.136572	26.530112
203.799321	6745.069125	26.535130
203.780544	6756.105113	26.540148
204.187074	6761.203321	26.545165
204.533540	6776.860774	26.550183
204.736870	6776.829319	26.555200
205.265891	6786.694113	26.560218
204.894461	6803.666084	26.565236
205.353578	6786.841859	26.570253
205.801657	6814.782276	26.575271
205.579743	6814.993806	26.580288
206.272235	6813.367788	26.585306
205.775477	6817.978448	26.590324
206.207583	6839.131182	26.595341
206.320498	6839.738844	26.600359
206.681474	6849.497251	26.605376
206.988697	6863.181591	26.610394
206.961114	6871.071714	26.615412
207.118629	6878.355333	26.620429
207.383563	6892.301977	26.625447
207.529755	6895.909716	26.630464
207.963475	6910.205753	26.635482
207.714989	6932.951401	26.640500
208.051998	6938.003661	26.645517
208.199616	6950.102952	26.650535
208.213967	6960.155300	26.655552
208.737468	6961.605042	26.660570
208.620863	6991.524563	26.665588
209.035521	7000.719097	26.670605
209.364532	7005.718954	26.675623
209.597264	7025.864357	26.680640
210.069724	7023.467594	26.685658
210.316191	7052.740366	26.690676
210.659553	7057.936882	26.695693
210.663928	7056.481114	26.700711
211.179938	7061.155133	26.705728
211.379852	7073.962960	26.710746
211.247808	7080.398362	26.715764
211.454956	7073.815927	26.720781
211.911308	7086.309195	26.725799
212.020751	7098.790189	26.730816
212.258280	7101.430390	26.735834
212.527728	7112.996260	26.740852
212.998251	7120.051304	26.745869
213.207598	7127.907808	26.750887
212.922634	7130.288423	26.755904
213.390513	7132.147755	26.760922
213.138962	7146.029790	26.765940
213.403223	7151.279688	26.770957
213.527823	7155.279129	26.775975
213.621002	7175.036036	26.780992
213.959076	7177.764770	26.786010
214.053341	7187.432295	26.791028
214.545208	7198.676319	26.796045
214.568002	7194.625912	26.801063
214.954014	7216.837484	26.806080
215.393671	7215.440208	26.811098
215.511802	7225.315545	26.816116
215.939780	7235.079511	26.821133
216.461722	7231.342832	26.826151
216.321501	7240.857482	26.831168
216.660019	7239.709556	26.836186
216.515640	7257.966156	26.841204
216.517654	7256.097192	26.846221
216.899820	7258.399214	26.851239
216.893334	7273.531183	26.856256
217.327732	7286.940336	26.861274
217.314865	7306.271935	26.866292
217.664210	7315.792482	26.871309
217.932056	7315.596297	26.876327
218.094254	7331.724872	26.881344
218.626137	7345.999654	26.886362
218.958193	7357.142383	26.891380
219.274124	7364.366806	26.896397
219.196457	7372.258628	26.901415
219.138722	7380.737684	26.906432
219.709152	7388.765377	26.911450
219.636023	7401.063491	26.916468
219.843081	7418.649946	26.921485
220.195466	7427.020976	26.926503
220.064950	7435.953351	26.931520
220.391531	7444.353662	26.936538
220.718860	7470.950109	26.941556
221.232504	7482.550802	26.946573
221.628309	7483.275445	26.951591
221.630427	7495.110472	26.956608
221.956376	7504.779977	26.961626
222.028132	7504.254434	26.966644
222.215528	7526.711973	26.971661
222.760111	7535.728704	26.976679
222.480909	7544.532750	26.981696
223.294867	7552.648876	26.986714
223.144651	7572.295730	26.991732
223.105159	7582.382056	26.996749
223.571105	7586.659923	27.001767
223.566920	7603.180842	27.006784
223.875980	7607.896693	27.011802
224.072246	7625.674441	27.016820
224.014160	7641.913350	27.021837
224.356045	7644.761524	27.026855
224.796987	7659.028610	27.031872
225.096145	7677.346005	27.036890
225.499989	7687.265503	27.041908
225.455601	7692.374194	27.046925
225.803337	7708.565765	27.051943
226.001361	7726.254942	27.056960
226.152554	7729.735791	27.061978
226.608372	7740.158647	27.066996
226.745849	7744.531887	27.072013
227.585407	7753.278660	27.077031
227.831756	7770.420521	27.082048
227.785725	7776.246115	27.087066
227.790696	7785.157566	27.092084
227.841756	7783.009416	27.097101
228.343881	7777.662521	27.102119
228.498502	7800.188635	27.107136
228.634033	7807.172979	27.112154
228.740458	7817.362995	27.117172
228.976306	7835.175823	27.122189
229.401732	7828.915870	27.127207
228.910928	7841.831770	27.132224
229.556318	7841.472622	27.137242
230.145956	7863.798495	27.142260
230.084209	7870.021184	27.147277
230.036467	7873.488834	27.152295
230.244789	7891.779545	27.157312
230.896485	7900.009484	27.162330
231.016165	7908.732660	27.167348
231.091422	7927.754438	27.172365
231.430025	7923.705213	27.177383
231.721833	7942.617525	27.182400
232.011537	7955.680331	27.187418
231.733921	7951.654428	27.192436
231.971253	7967.364616	27.197453
232.360701	7994.760333	27.202471
232.367859	8009.786603	27.207488
233.066177	8020.888498	27.212506
233.202700	8030.603556	27.217524
233.403635	8036.921155	27.222541
233.771466	8043.345364	27.227559
233.818852	8057.323608	27.232576
233.782208	8065.348247	27.237594
234.286831	8080.293968	27.242612
234.791624	8104.104498	27.247629
234.930906	8105.307926	27.252647
235.270310	8122.359861	27.257664
235.662053	8128.272102	27.262682
235.904842	8148.060430	27.267700
235.958595	8156.582468	27.272717
236.558328	8149.341857	27.277735
236.512805	8168.701544	27.282752
236.757675	8181.335824	27.287770
237.271031	8180.327944	27.292788
237.166211	8205.909882	27.297805
237.887053	8209.242151	27.302823
237.644560	8217.362045	27.307840
238.349234	8222.853070	27.312858
238.779313	8226.590510	27.317876
238.419347	8244.266033	27.322893
238.607771	8237.089424	27.327911
239.259108	8254.440188	27.332928
239.337106	8254.286180	27.337946
239.625256	8261.060673	27.342964
239.644204	8286.326694	27.347981
239.848977	8288.407062	27.352999
239.821674	8302.577069	27.358016
240.149590	8307.305951	27.363034
240.196185	8318.588418	27.368052
240.376825	8330.835014	27.373069
240.957640	8346.902464	27.378087
240.980694	8358.390670	27.383104
241.583076	8376.491073	27.388122
241.761491	8382.060922	27.393140
242.100728	8391.122675	27.398157
242.326621	8400.628278	27.403175
242.581199	8409.056026	27.408192
242.952601	8433.632812	27.413210
243.380574	8431.972075	27.418228
243.144124	8442.758830	27.423245
243.683112	8447.887402	27.428263
243.823997	8454.460743	27.433280
243.833217	8463.223478	27.438298
244.386206	8467.323835	27.443316
244.445638	8478.190827	27.448333
244.483118	8492.079387	27.453351
244.966765	8505.582790	27.458368
245.176535	8511.378261	27.463386
245.543695	8514.481516	27.468404
245.703994	8540.878206	27.473421
245.816581	8534.268932	27.478439
245.680764	8544.992722	27.483456
246.101970	8561.587182	27.488474
246.397140	8566.330701	27.493492
246.590123	8586.010441	27.498509
247.146676	8583.426751	27.503527
247.274684	8604.628865	27.508544
247.282851	8616.353172	27.513562
247.639753	8625.639600	27.518580
247.561012	8644.004163	27.523597
247.984247	8657.832791	27.528615
248.278920	8678.346054	27.533632
248.230068	8687.449430	27.538650
249.022394	8696.450264	27.543668
249.156222	8702.803796	27.548685
249.340978	8712.401206	27.553703
249.451445	8733.154734	27.558720
249.757452	8748.340290	27.563738
250.226750	8753.107260	27.568756
250.452882	8772.428444	27.573773
251.218966	8787.267735	27.578791
250.726578	8797.245281	27.583808
250.838794	8811.078246	27.588826
251.303629	8824.133344	27.593844
251.444203	8841.400012	27.598861
251.921655	8851.914846	27.603879
252.272453	8870.856812	27.608896
252.410057	8881.222517	27.613914
252.700498	8898.011280	27.618932
253.013917	8918.506105	27.623949
252.921901	8927.669991	27.628967
253.593717	8933.914587	27.633984
253.578986	8949.481742	27.639002
254.129909	8962.479336	27.644020
254.468408	8976.059353	27.649037
254.654382	8984.731674	27.654055
254.927361	8991.069955	27.659072
255.134579	9009.485075	27.664090
255.604749	9011.890434	27.669108
255.633481	9033.433681	27.674125
255.832341	9044.377170	27.679143
256.155347	9054.272106	27.684160
256.020628	9069.422356	27.689178
256.484642	9074.726949	27.694196
256.609378	9090.711353	27.699213
256.937219	9111.273605	27.704231
257.953521	9110.158961	27.709248
257.680144	9126.050677	27.714266
257.888238	9139.079669	27.719284
258.393387	9153.101131	27.724301
258.692267	9170.368717	27.729319
259.343222	9169.784526	27.734336
259.053424	9183.408841	27.739354
259.502330	9191.115272	27.744372
259.882970	9196.426567	27.749389
259.990159	9205.553262	27.754407
260.332274	9214.277154	27.759424
260.512435	9225.807740	27.764442
260.598879	9235.966921	27.769460
261.179576	9242.118465	27.774477
261.067955	9255.377274	27.779495
261.593298	9264.776716	27.784512
261.526481	9275.338641	27.789530
261.689842	9282.369728	27.794548
261.811048	9285.511406	27.799565
262.083355	9300.279599	27.804583
262.394848	9316.737116	27.809600
262.452089	9324.293048	27.814618
262.944950	9341.508493	27.819636
262.894203	9359.746276	27.824653
263.411374	9374.798441	27.829671
263.628035	9383.977639	27.834688
263.741677	9397.542458	27.839706
264.053279	9422.350873	27.844724
264.141461	9436.529026	27.849741
264.600345	9456.629250	27.854759
265.028834	9463.666486	27.859776
264.969622	9497.120374	27.864794
265.548542	9500.430778	27.869812
265.977218	9514.805402	27.874829
266.489718	9526.369679	27.879847
266.461555	9540.755459	27.884864
266.581256	9546.486348	27.889882
267.315074	9564.763205	27.894900
267.236833	9573.123327	27.899917
267.490183	9591.140345	27.904935
267.921179	9595.957700	27.909952
267.782439	9613.353819	27.914970
268.570383	9613.941728	27.919988
268.860488	9634.450448	27.925005
268.709665	9634.051059	27.930023
268.967863	9655.862400	27.935040
269.157623	9671.546714	27.940058
269.707518	9682.625365	27.945076
269.965937	9701.427858	27.950093
269.989671	9719.272369	27.955111
270.701464	9727.891591	27.960128
270.716249	9744.793498	27.965146
271.270450	9751.549220	27.970164
271.559666	9767.849586	27.975181
271.971263	9775.306331	27.980199
272.447303	9796.455625	27.985216
272.297717	9807.706396	27.990234
272.523247	9810.516194	27.995252
272.889772	9822.914804	28.000269
272.825598	9835.462566	28.005287
273.527717	9841.829047	28.010304
273.522570	9856.849260	28.015322
273.997654	9872.426178	28.020340
274.454720	9884.649712	28.025357
274.513714	9903.050908	28.030375
274.820986	9904.657694	28.035392
275.021990	9932.761284	28.040410
275.370927	9929.180456	28.045428
275.869605	9946.603941	28.050445
275.983156	9950.302610	28.055463
276.450361	9956.816209	28.060480
276.470197	9986.952975	28.065498
276.835228	9988.440270	28.070516
277.541906	10003.485544	28.075533
277.400555	10012.174576	28.080551
277.651324	10015.043623	28.085568
278.127809	10024.413171	28.090586
278.433776	10032.281131	28.095604
278.719538	10040.524802	28.100621
278.854340	10053.748973	28.105639
279.245521	10053.041022	28.110656
279.416764	10069.599977	28.115674
279.212722	10087.631855	28.120692
279.853612	10091.046383	28.125709
279.935234	10110.009423	28.130727
280.558132	10108.949662	28.135744
280.714732	10128.677751	28.140762
280.952202	10139.312772	28.145780
281.114629	10134.327513	28.150797
281.215261	10155.523033	28.155815
281.397101	10162.024300	28.160832
281.370929	10182.484988	28.165850
282.032902	10202.623865	28.170868
282.204492	10208.002729	28.175885
282.591024	10220.461638	28.180903
282.990633	10231.601904	28.185920
282.712454	10255.957032	28.190938
283.058672	10271.115475	28.195956
283.710820	10291.003388	28.200973
283.638455	10306.653272	28.205991
284.204418	10318.648595	28.211008
284.576368	10336.941508	28.216026
284.615131	10352.994059	28.221044
285.176690	10362.884130	28.226061
285.478190	10386.773454	28.231079
286.034948	10388.928714	28.236096
286.159815	10402.978755	28.241114
286.500909	10405.919050	28.246132
286.761835	10421.896027	28.251149
286.945006	10444.585097	28.256167
287.426577	10454.749734	28.261184
287.682918	10468.552024	28.266202
287.711542	10487.968892	28.271220
288.387035	10487.961807	28.276237
288.361020	10509.606853	28.281255
288.417856	10524.412723	28.286272
288.626492	10541.992431	28.291290
288.846700	10560.624928	28.296308
289.152575	10573.848094	28.301325
289.828455	10595.987029	28.306343
290.248825	10610.168036	28.311360
290.261574	10636.072861	28.316378
290.628620	10645.784977	28.321396
291.141406	10656.911036	28.326413
291.554855	10680.660168	28.331431
291.843839	10691.278013	28.336448
292.292178	10707.980683	28.341466
292.565110	10703.814787	28.346484
292.946330	10720.944700	28.351501
292.719882	10734.945491	28.356519
293.297340	10742.847263	28.361536
293.518709	10756.168966	28.366554
293.502930	10776.183487	28.371572
293.921802	10783.528997	28.376589
294.188365	10810.733305	28.381607
294.678432	10822.355562	28.386624
295.360822	10833.654241	28.391642
295.469591	10842.873061	28.396660
295.726687	10858.184786	28.401677
295.850009	10869.343188	28.406695
296.241054	10884.179407	28.411712
296.366592	10897.115132	28.416730
296.558300	10919.879230	28.421748
296.541217	10924.943512	28.426765
297.020359	10956.285953	28.431783
297.596751	10974.266648	28.436800
297.882200	10978.485003	28.441818
298.041759	10998.961875	28.446836
298.719750	11006.235556	28.451853
298.588520	11028.696426	28.456871
298.732156	11037.556275	28.461888
299.359094	11056.372229	28.466906
299.263355	11076.794208	28.471924
299.648701	11083.128342	28.476941
300.157765	11105.173870	28.481959
300.262754	11114.036614	28.486976
300.711537	11142.523399	28.491994
300.435712	11144.565243	28.497012
301.007097	11174.078124	28.502029
301.398220	11180.430337	28.507047
301.701363	11198.087518	28.512064
302.208946	11218.182066	28.517082
302.499620	11231.019690	28.522100
303.141749	11243.673148	28.527117
303.381780	11249.243741	28.532135
303.537936	11263.046429	28.537152
303.941551	11277.183190	28.542170
304.285147	11289.955780	28.547188
304.897590	11294.546408	28.552205
304.992626	11313.685404	28.557223
305.242845	11324.363322	28.562240
305.422090	11334.815482	28.567258
305.186872	11341.918873	28.572276
305.728945	11360.284188	28.577293
306.288277	11385.887086	28.582311
306.290434	11393.367180	28.587328
306.672080	11411.628063	28.592346
306.892459	11423.535813	28.597364
307.714716	11438.040104	28.602381
307.907144	11455.534785	28.607399
308.152969	11478.006957	28.612416
308.741463	11478.060786	28.617434
308.683029	11504.802020	28.622452
309.185942	11507.935170	28.627469
309.073423	11528.290786	28.632487
309.390427	11543.517964	28.637504
309.869236	11554.179372	28.642522
310.237939	11588.062968	28.647540
310.451481	11605.516611	28.652557
310.906098	11626.668162	28.657575
310.928646	11642.613829	28.662592
311.255061	11658.726918	28.667610
311.457985	11680.501870	28.672628
312.092662	11699.127812	28.677645
312.442530	11722.082980	28.682663
312.647449	11746.510084	28.687680
312.988795	11759.532796	28.692698
313.180039	11779.620361	28.697716
313.791449	11792.329496	28.702733
314.038461	11813.513580	28.707751
314.172004	11827.380199	28.712768
314.828255	11852.554999	28.717786
314.938081	11856.469345	28.722804
315.628737	11875.794057	28.727821
315.832974	11886.602603	28.732839
316.376207	11904.207284	28.737856
316.854978	11907.271635	28.742874
316.827608	11927.554432	28.747892
317.297586	11928.507697	28.752909
317.638897	11943.756678	28.757927
317.467898	11949.798806	28.762944
318.193964	11964.059556	28.767962
318.314471	11987.303369	28.772980
318.324562	11996.045526	28.777997
318.972577	12015.449647	28.783015
319.276928	12031.607542	28.788032
319.226382	12046.633423	28.793050
319.759939	12071.404493	28.798068
319.810972	12081.990706	28.803085
320.400232	12105.853216	28.808103
320.401234	12129.990483	28.813120
320.854828	12140.387749	28.818138
321.154754	12160.904033	28.823156
321.826707	12176.992193	28.828173
322.006074	12187.447967	28.833191
321.885230	12199.598795	28.838208
322.549006	12220.481628	28.843226
322.661617	12230.186816	28.848244
323.190017	12248.801432	28.853261
323.488830	12267.053942	28.858279
323.405234	12287.364826	28.863296
323.885765	12293.583508	28.868314
323.913016	12311.262587	28.873332
324.181720	12334.486914	28.878349
324.997474	12348.658210	28.883367
325.415126	12372.929859	28.888384
325.951821	12388.890846	28.893402
326.479566	12407.335206	28.898420
326.470733	12413.241715	28.903437
326.765872	12430.500274	28.908455
327.161073	12448.715849	28.913472
327.380016	12461.189716	28.918490
327.647375	12480.047297	28.923508
328.033766	12512.246738	28.928525
328.129099	12521.392689	28.933543
328.258903	12542.330592	28.938560
329.195074	12554.901270	28.943578
328.975416	12582.007014	28.948596
329.124624	12599.256869	28.953613
330.044860	12622.076974	28.958631
330.637848	12645.614341	28.963648
331.102506	12648.279978	28.968666
331.468327	12672.594818	28.973684
331.965536	12686.613867	28.978701
332.249333	12698.948326	28.983719
332.209923	12712.684636	28.988736
332.653570	12727.185720	28.993754
332.729253	12744.586097	28.998772
333.042711	12757.778049	29.003789
333.396490	12778.343463	29.008807
333.710759	12799.552922	29.013824
334.149133	12820.537829	29.018842
334.707297	12840.294675	29.023860
334.577835	12861.314347	29.028877
334.809382	12873.224438	29.033895
335.138916	12891.747498	29.038912
335.682686	12909.460405	29.043930
336.123489	12939.517432	29.048948
336.222489	12954.615489	29.053965
336.961265	12968.227677	29.058983
337.303354	12990.557201	29.064000
338.135314	13001.767597	29.069018
337.986513	13018.202147	29.074036
338.348518	13039.682334	29.079053
338.784096	13048.292423	29.084071
338.808887	13065.543128	29.089088
339.055796	13079.077238	29.094106
339.844655	13099.193170	29.099124
340.050914	13118.218794	29.104141
340.217001	13122.074120	29.109159
340.448540	13148.362023	29.114176
341.123499	13156.647531	29.119194
341.351754	13183.937032	29.124212
341.485133	13196.674177	29.129229
341.926472	13207.910774	29.134247
342.385613	13234.943353	29.139264
342.733613	13245.900824	29.144282
343.228677	13262.342714	29.149300
343.424800	13288.582642	29.154317
343.847077	13297.475967	29.159335
343.838847	13321.234094	29.164352
344.297337	13324.308155	29.169370
343.950172	13346.830670	29.174388
344.652408	13357.982529	29.179405
344.951353	13378.181347	29.184423
344.784979	13405.336816	29.189440
345.861766	13426.172480	29.194458
346.143628	13437.708779	29.199476
346.688070	13452.213676	29.204493
347.529298	13467.243959	29.209511
347.565348	13482.112238	29.214528
348.269808	13488.413299	29.219546
348.627295	13503.335764	29.224564
348.947745	13504.950290	29.229581
349.372100	13525.347637	29.234599
349.253949	13539.147332	29.239616
349.852076	13549.314457	29.244634
350.147004	13569.210946	29.249652
350.483730	13578.544041	29.254669
350.666346	13590.907468	29.259687
350.748980	13603.415944	29.264704
350.727311	13620.213331	29.269722
351.208723	13642.585096	29.274740
351.521885	13677.845324	29.279757
352.024936	13696.777957	29.284775
352.601258	13726.799350	29.289792
352.613649	13742.941008	29.294810
353.287114	13766.723041	29.299828
353.339327	13789.746019	29.304845
353.687827	13811.952357	29.309863
354.005185	13837.545740	29.314880
354.137484	13852.459327	29.319898
354.760734	13881.374690	29.324916
355.178435	13901.612422	29.329933
355.551681	13929.161484	29.334951
355.828947	13956.558156	29.339968
356.294751	13978.901168	29.344986
356.760821	14003.925294	29.350004
357.072929	14023.753268	29.355021
357.608160	14044.320234	29.360039
357.944505	14074.360591	29.365056
358.166878	14080.260048	29.370074
358.953535	14099.799478	29.375092
358.898776	14122.807934	29.380109
359.477577	14140.203901	29.385127
359.507890	14166.979300	29.390144
359.849687	14194.688386	29.395162
360.451465	14219.682196	29.400180
360.604243	14235.840313	29.405197
361.147524	14254.678817	29.410215
361.443581	14273.423190	29.415232
361.553963	14307.765593	29.420250
362.339844	14332.955110	29.425268
362.450365	14359.525653	29.430285
362.918969	14371.589264	29.435303
363.425799	14399.301379	29.440320
363.855536	14413.925931	29.445338
364.121240	14433.628920	29.450356
364.402013	14451.036833	29.455373
365.263428	14475.327366	29.460391
365.345469	14496.745419	29.465408
365.915254	14516.792754	29.470426
366.521188	14528.370849	29.475444
366.869640	14543.440812	29.480461
367.343373	14551.265606	29.485479
367.536915	14561.729962	29.490496
367.866872	14576.095421	29.495514
368.215003	14580.885918	29.500532
368.650104	14601.724883	29.505549
368.875755	14600.022487	29.510567
368.910030	14628.730666	29.515584
369.261815	14629.860383	29.520602
369.616931	14650.459207	29.525620
369.703622	14666.008993	29.530637
370.263768	14680.941891	29.535655
370.674074	14704.257618	29.540672
370.633744	14724.747549	29.545690
371.213189	14752.707840	29.550708
371.408768	14778.810958	29.555725
371.666395	14795.199562	29.560743
372.123948	14820.841924	29.565760
372.446454	14847.342248	29.570778
373.065582	14870.486711	29.575796
373.492311	14892.454750	29.580813
373.937186	14915.190574	29.585831
374.050659	14938.868614	29.590848
374.518824	14959.364903	29.595866
375.080800	14977.948563	29.600884
375.374830	15008.502288	29.605901
375.495281	15020.797371	29.610919
376.254829	15045.862452	29.615936
376.597379	15060.990591	29.620954
376.925654	15077.895852	29.625972
377.173552	15107.758964	29.630989
378.019783	15124.618369	29.636007
378.234723	15157.212191	29.641024
378.850087	15168.002825	29.646042
379.645879	15178.440083	29.651060
379.756297	15197.097416	29.656077
380.451304	15212.477148	29.661095
380.748803	15219.189550	29.666112
380.945699	15236.895477	29.671130
381.666737	15250.129936	29.676148
381.546434	15269.909677	29.681165
382.246216	15275.536215	29.686183
382.437351	15298.558340	29.691200
382.868017	15318.050230	29.696218
383.093216	15330.351313	29.701236
383.280046	15354.485863	29.706253
383.852754	15366.865514	29.711271
384.101093	15399.508239	29.716288
383.921888	15417.989802	29.721306
384.634431	15426.602075	29.726324
384.474217	15458.509476	29.731341
385.015747	15484.843943	29.736359
385.355500	15510.309763	29.741376
385.671967	15543.791694	29.746394
386.076532	15572.232043	29.751412
386.870026	15595.252337	29.756429
387.240627	15619.222807	29.761447
387.845462	15660.126157	29.766464
388.179490	15688.056547	29.771482
388.848718	15699.786577	29.776500
388.874967	15721.637899	29.781517
389.050996	15746.178883	29.786535
389.933541	15772.561722	29.791552
390.198151	15797.524825	29.796570
390.955986	15812.854204	29.801588
391.116667	15834.678410	29.806605
391.488379	15852.803011	29.811623
391.650676	15873.966927	29.816640
391.979353	15891.832968	29.821658
392.957208	15906.278588	29.826676
393.381816	15938.149433	29.831693
393.545714	15950.545733	29.836711
393.891530	15966.488926	29.841728
394.153994	15979.261531	29.846746
394.504910	15988.647295	29.851764
395.062093	16008.581308	29.856781
395.287126	16020.601772	29.861799
395.891862	16033.479043	29.866816
395.923167	16059.786353	29.871834
396.569060	16074.113232	29.876852
396.826201	16090.041908	29.881869
397.014286	16111.694772	29.886887
397.591868	16135.403108	29.891904
397.517485	16160.795301	29.896922
398.228738	16177.016562	29.901940
398.222925	16206.652430	29.906957
398.810741	16233.467110	29.911975
399.264946	16256.297831	29.916992
399.567294	16281.006179	29.922010
400.334905	16305.777935	29.927028
400.795852	16335.057082	29.932045
400.885535	16359.220657	29.937063
401.481779	16374.120840	29.942080
401.476192	16404.805560	29.947098
402.276757	16417.883165	29.952116
402.448123	16454.563454	29.957133
403.009247	16478.660102	29.962151
403.443299	16502.185941	29.967168
403.708520	16536.678798	29.972186
404.653274	16548.679140	29.977204
405.513565	16573.654745	29.982221
405.482797	16583.791915	29.987239
405.787614	16614.507606	29.992256
405.957675	16632.809626	29.997274
406.658545	16655.934057	30.002292
406.666968	16683.663915	30.007309
406.981905	16709.782672	30.012327
407.540062	16734.056975	30.017344
407.701385	16757.410813	30.022362
408.602035	16785.033499	30.027380
409.382347	16817.469485	30.032397
409.362334	16828.375771	30.037415
409.821070	16849.052430	30.042432
409.833363	16871.829502	30.047450
410.646064	16897.125625	30.052468
411.039296	16918.561112	30.057485
411.268415	16935.515037	30.062503
411.809041	16964.454260	30.067520
412.046271	16987.682856	30.072538
412.925823	17012.551804	30.077556
412.967334	17038.808330	30.082573
413.534701	17065.049354	30.087591
413.882598	17089.328413	30.092608
414.463955	17115.447305	30.097626
414.474343	17137.106879	30.102644
414.680987	17168.811557	30.107661
415.445653	17196.168582	30.112679
415.821040	17218.178872	30.117696
416.473835	17243.689857	30.122714
416.795421	17269.827291	30.127732
417.701385	17301.047451	30.132749
418.104923	17312.399754	30.137767
418.533069	17326.597228	30.142784
418.599108	17346.650156	30.147802
419.135006	17373.089170	30.152820
419.364291	17388.874810	30.157837
419.276107	17413.357984	30.162855
420.289699	17432.881302	30.167872
420.441045	17468.713832	30.172890
420.931625	17485.747562	30.177908
421.338240	17513.239744	30.182925
421.885281	17537.548379	30.187943
422.210933	17558.357069	30.192960
422.668164	17576.751099	30.197978
422.844835	17603.716982	30.202996
423.421694	17622.818905	30.208013
423.768257	17639.733056	30.213031
424.167486	17665.085085	30.218048
424.502898	17688.236069	30.223066
425.141290	17718.617316	30.228084
425.340966	17730.001603	30.233101
425.678950	17761.939497	30.238119
426.272608	17779.383852	30.243136
426.572379	17804.618886	30.248154
426.885606	17830.369872	30.253172
427.508958	17849.496368	30.258189
427.803577	17882.041349	30.263207
428.324279	17896.288007	30.268224
428.585569	17940.645221	30.273242
428.999481	17961.933353	30.278260
429.418199	17996.322801	30.283277
429.464359	18030.643965	30.288295
430.265155	18061.278430	30.293312
431.000699	18089.585697	30.298330
431.281717	18119.776837	30.303348
431.871496	18155.510797	30.308365
432.752193	18179.348194	30.313383
433.883748	18191.491058	30.318400
433.780224	18202.291090	30.323418
434.132310	18220.626295	30.328436
434.645792	18241.633906	30.333453
434.834608	18265.117953	30.338471
435.459714	18280.789003	30.343488
436.051090	18302.643716	30.348506
435.810910	18313.566164	30.353524
436.738896	18342.064949	30.358541
436.763738	18376.175253	30.363559
437.554156	18391.845927	30.368576
437.604776	18424.751994	30.373594
438.004370	18447.931800	30.378612
438.826604	18469.618097	30.383629
438.785753	18508.053670	30.388647
439.940911	18524.059350	30.393664
440.598434	18540.281500	30.398682
441.202933	18561.420590	30.403700
441.556006	18572.452984	30.408717
441.662877	18594.850949	30.413735
441.900483	18617.835065	30.418752
442.282434	18640.322925	30.423770
442.756828	18666.271045	30.428788
443.258583	18691.279949	30.433805
443.302972	18721.224577	30.438823
443.730076	18740.407779	30.443840
444.536041	18768.326025	30.448858
444.837439	18788.868162	30.453876
445.189235	18818.322855	30.458893
445.520342	18853.801450	30.463911
445.971304	18879.917761	30.468928
446.458862	18902.913843	30.473946
446.998382	18926.982170	30.478964
447.612835	18958.468353	30.483981
447.817703	18990.157340	30.488999
448.803218	19017.927959	30.494016
448.982794	19036.992049	30.499034
449.302486	19065.959341	30.504052
449.798531	19092.568012	30.509069
450.120753	19120.119840	30.514087
450.358351	19134.999027	30.519104
451.335791	19166.087885	30.524122
451.679291	19193.301667	30.529140
451.896003	19207.956726	30.534157
452.399254	19236.023856	30.539175
453.074639	19252.180646	30.544192
453.203116	19273.167183	30.549210
453.162237	19296.441847	30.554228
454.058538	19321.409094	30.559245
454.427025	19356.731162	30.564263
454.834543	19377.421661	30.569280
455.194771	19406.124123	30.574298
455.007476	19444.729652	30.579316
455.810104	19469.560046	30.584333
456.111473	19510.553558	30.589351
456.786069	19548.456513	30.594368
457.299509	19577.602891	30.599386
457.123208	19608.360330	30.604404
458.164193	19646.572870	30.609421
458.201487	19683.002165	30.614439
459.154885	19709.755287	30.619456
459.875105	19744.934851	30.624474
460.239197	19775.570517	30.629492
461.127597	19805.265377	30.634509
461.528064	19833.229330	30.639527
462.057737	19849.649382	30.644544
462.432963	19883.954177	30.649562
462.429491	19910.629095	30.654580
463.776299	19939.425150	30.659597
463.822543	19974.886956	30.664615
464.239118	19994.862776	30.669632
465.160750	20022.846953	30.674650
465.383632	20050.908361	30.679668
465.388655	20076.451270	30.684685
466.369449	20119.204086	30.689703
466.793628	20141.769242	30.694720
467.316798	20168.653152	30.699738
467.901873	20197.523950	30.704756
468.386533	20218.500280	30.709773
468.598804	20235.431284	30.714791
469.399952	20259.909109	30.719808
469.845079	20290.097025	30.724826
470.284517	20310.019064	30.729844
470.725072	20332.638753	30.734861
471.154407	20353.270031	30.739879
471.524881	20386.616105	30.744896
472.095208	20416.077101	30.749914
472.218060	20447.484273	30.754932
472.975198	20473.435013	30.759949
473.371097	20506.941604	30.764967
473.356215	20539.722439	30.769984
474.186318	20565.263900	30.775002
474.405483	20598.210577	30.780020
474.823052	20623.102388	30.785037
475.361461	20668.844256	30.790055
475.990251	20693.273640	30.795072
476.360277	20718.962745	30.800090
476.819281	20757.861974	30.805108
477.037169	20787.795396	30.810125
477.343268	20826.901794	30.815143
477.920232	20861.341169	30.820160
478.673534	20898.438398	30.825178
479.034466	20937.397478	30.830196
479.783815	20967.191574	30.835213
480.045907	21001.737079	30.840231
480.683464	21038.024900	30.845248
481.643194	21072.487196	30.850266
481.668417	21098.565345	30.855284
482.341756	21128.024012	30.860301
482.726785	21156.308174	30.865319
483.254204	21185.928648	30.870336
483.675542	21203.535593	30.875354
484.031493	21227.616383	30.880372
484.842818	21254.374787	30.885389
485.329236	21288.209812	30.890407
485.423197	21310.549715	30.895424
486.516911	21329.562187	30.900442
486.472868	21359.366662	30.905460
487.374090	21378.238551	30.910477
487.389751	21401.797558	30.915495
488.203994	21434.109615	30.920512
488.851864	21450.468384	30.925530
489.103265	21484.346652	30.930548
489.765162	21506.307716	30.935565
490.510344	21539.805924	30.940583
490.559022	21572.989285	30.945600
490.904827	21593.382134	30.950618
491.329129	21617.098928	30.955636
492.643740	21637.612695	30.960653
493.186336	21666.726054	30.965671
493.863650	21673.312074	30.970688
494.247963	21687.645931	30.975706
494.559970	21725.710648	30.980724
494.656062	21738.010629	30.985741
495.256208	21760.057412	30.990759
496.176984	21791.557342	30.995776
496.402087	21819.968453	31.000794
496.776678	21844.325112	31.005812
497.134831	21868.981331	31.010829
497.709045	21905.185837	31.015847
498.152562	21928.653592	31.020864
499.017135	21957.489789	31.025882
499.458861	21989.904983	31.030900
499.484692	22016.489739	31.035917
500.134550	22048.670433	31.040935
500.651058	22076.202493	31.045952
501.009587	22103.980337	31.050970
501.716153	22135.065544	31.055988
501.690540	22167.231534	31.061005
502.425534	22205.338744	31.066023
502.722520	22236.178259	31.071040
503.547189	22269.204074	31.076058
503.571781	22309.842127	31.081076
504.178084	22339.780629	31.086093
504.588431	22377.963987	31.091111
505.071725	22420.078938	31.096128
506.249450	22445.126423	31.101146
506.490846	22488.132204	31.106164
507.020765	22516.743294	31.111181
507.508914	22556.450340	31.116199
507.853860	22585.911764	31.121216
508.590363	22618.907658	31.126234
508.758409	22651.075880	31.131252
509.401239	22694.803145	31.136269
510.230451	22718.799444	31.141287
510.691596	22749.083423	31.146304
511.363781	22779.770594	31.151322
511.699567	22817.707336	31.156340
512.072588	22857.698300	31.161357
513.073146	22891.203281	31.166375
513.095261	22916.437587	31.171392
513.947394	22944.784294	31.176410
514.401600	22975.031786	31.181428
515.256677	23005.646602	31.186445
515.829933	23034.017895	31.191463
516.193654	23061.973206	31.196480
516.797217	23074.321395	31.201498
517.079980	23105.145521	31.206516
517.816913	23126.205742	31.211533
518.082705	23147.674235	31.216551
518.343663	23176.024840	31.221568
518.954013	23186.173048	31.226586
519.253564	23222.226838	31.231604
519.680102	23253.388993	31.236621
520.147218	23276.709339	31.241639
520.369664	23315.422957	31.246656
521.034674	23348.311136	31.251674
521.360226	23391.103566	31.256692
522.011923	23434.761575	31.261709
522.467154	23459.568959	31.266727
523.215500	23496.002031	31.271744
523.889710	23525.944395	31.276762
524.536737	23563.954173	31.281780
525.217297	23591.924096	31.286797
525.415417	23622.496801	31.291815
525.785650	23653.541968	31.296832
526.455719	23692.426760	31.301850
527.162846	23721.296363	31.306868
527.865022	23759.215781	31.311885
528.519478	23797.401786	31.316903
529.106854	23826.340738	31.321920
529.585453	23854.393024	31.326938
529.633660	23895.833180	31.331956
530.607343	23908.674040	31.336973
531.054357	23943.954199	31.341991
531.300948	23985.426850	31.347008
532.235998	24016.169800	31.352026
532.568048	24053.724012	31.357044
532.952199	24084.616023	31.362061
533.913884	24111.196915	31.367079
533.937279	24153.172285	31.372096
534.773859	24180.227732	31.377114
535.305044	24212.468333	31.382132
535.931578	24249.098688	31.387149
536.344739	24274.077940	31.392167
536.667280	24317.372053	31.397184
537.205273	24357.018065	31.402202
537.732198	24393.935924	31.407220
538.375912	24434.165968	31.412237
538.778934	24472.145953	31.417255
539.559404	24510.490649	31.422272
540.109075	24540.302263	31.427290
540.564994	24578.185744	31.432308
541.083963	24601.663875	31.437325
541.712018	24630.787245	31.442343
542.082573	24667.900579	31.447360
543.021490	24702.593628	31.452378
543.721841	24741.279851	31.457396
544.296301	24776.636434	31.462413
544.837431	24804.478101	31.467431
545.151701	24836.260560	31.472448
545.600404	24869.519859	31.477466
546.348005	24906.126254	31.482484
546.835476	24937.964064	31.487501
547.347058	24964.458179	31.492519
547.661243	25015.073106	31.497536
548.346456	25040.977853	31.502554
549.353448	25080.438536	31.507572
549.546135	25108.638209	31.512589
550.214640	25132.384385	31.517607
550.427343	25175.008620	31.522624
551.267554	25203.524716	31.527642
551.685673	25237.307594	31.532660
552.086434	25272.793208	31.537677
552.857939	25300.662898	31.542695
553.274783	25348.153429	31.547712
553.659925	25370.073388	31.552730
554.411026	25404.032217	31.557748
555.034585	25433.233292	31.562765
555.507392	25460.353426	31.567783
555.966132	25501.246380	31.572800
556.074014	25542.775448	31.577818
556.723782	25579.170795	31.582836
557.311593	25606.342740	31.587853
557.937752	25622.430272	31.592871
558.551966	25669.056633	31.597888
558.644447	25709.659442	31.602906
559.547670	25743.007427	31.607924
559.691707	25788.557064	31.612941
560.367756	25823.659527	31.617959
561.199419	25862.068361	31.622976
561.754184	25905.190717	31.627994
562.596436	25939.584969	31.633012
563.059790	25981.362956	31.638029
564.045896	26009.364539	31.643047
564.822628	26031.167380	31.648064
565.292064	26060.791512	31.653082
566.140382	26090.590540	31.658100
566.632523	26122.195668	31.663117
567.492882	26145.293830	31.668135
567.697596	26173.063372	31.673152
568.237602	26205.647083	31.678170
568.885373	26237.544159	31.683188
568.984197	26275.764513	31.688205
569.539614	26302.620127	31.693223
569.871518	26345.961399	31.698240
570.247781	26380.346789	31.703258
570.981968	26427.683027	31.708276
571.423383	26468.568003	31.713293
572.239566	26510.589200	31.718311
572.572251	26547.876222	31.723328
573.328274	26592.940564	31.728346
574.000260	26630.048516	31.733364
574.196643	26670.207321	31.738381
574.959669	26711.143842	31.743399
575.698511	26744.917243	31.748416
576.486048	26783.587508	31.753434
577.452881	26816.181601	31.758452
577.918252	26848.853812	31.763469
579.030199	26889.925981	31.768487
579.066752	26928.119341	31.773504
579.606915	26955.951500	31.778522
580.314980	26979.270253	31.783540
580.983866	27021.555611	31.788557
581.648245	27051.846069	31.793575
582.018892	27084.217397	31.798592
582.502299	27121.368250	31.803610
583.008411	27150.204568	31.808628
583.603202	27187.812218	31.813645
584.163400	27227.277150	31.818663
584.678248	27263.525897	31.823680
585.085266	27305.511321	31.828698
585.715592	27345.610231	31.833716
586.115298	27390.643337	31.838733
586.547618	27426.633452	31.843751
587.446603	27467.866354	31.848768
587.865843	27510.507611	31.853786
588.894250	27563.741804	31.858804
588.920664	27600.775067	31.863821
589.397536	27630.659478	31.868839
590.218004	27674.774465	31.873856
590.818561	27705.398175	31.878874
591.914939	27748.383265	31.883892
592.463242	27781.025108	31.888909
593.125369	27812.682261	31.893927
593.860840	27833.185152	31.898944
594.357378	27863.648322	31.903962
594.833505	27892.262829	31.908980
595.473843	27925.269802	31.913997
595.949599	27955.489849	31.919015
596.389956	27989.817431	31.924032
596.948770	28023.551468	31.929050
597.496487	28053.962714	31.934068
598.163501	28088.963073	31.939085
598.604111	28124.510699	31.944103
598.879330	28160.596096	31.949120
599.465900	28210.885882	31.954138
600.616240	28242.120074	31.959156
600.821297	28287.078018	31.964173
601.325544	28325.536186	31.969191
601.638558	28365.812919	31.974208
602.405075	28418.647682	31.979226
603.233566	28447.688482	31.984244
603.765812	28508.005620	31.989261
604.064957	28566.165961	31.994279
604.510929	28602.383574	31.999296
605.347044	28649.007539	32.004314
606.152374	28694.587169	32.009332
606.867953	28740.819264	32.014349
607.311500	28780.185277	32.019367
608.273861	28828.901116	32.024384
608.723108	28885.610517	32.029402
609.094403	28917.011268	32.034420
609.483710	28967.074475	32.039437
610.689896	29010.266367	32.044455
611.367038	29054.059013	32.049472
612.102628	29105.775268	32.054490
612.657623	29146.812293	32.059508
613.195090	29192.668605	32.064525
613.580900	29235.160654	32.069543
614.194542	29274.292550	32.074560
615.011846	29327.526293	32.079578
615.620335	29367.752682	32.084596
615.946559	29415.759876	32.089613
616.299108	29470.311558	32.094631
617.341402	29508.523848	32.099648
618.117673	29562.567348	32.104666
618.929686	29612.477836	32.109684
619.136598	29646.263015	32.114701
620.025624	29688.854654	32.119719
621.052629	29737.094841	32.124736
621.455345	29783.769899	32.129754
622.555513	29812.239383	32.134772
622.877451	29852.542937	32.139789
623.817525	29897.307821	32.144807
624.125503	29933.795793	32.149824
624.787237	29961.316045	32.154842
625.199429	30009.431345	32.159860
626.108565	30052.608471	32.164877
627.036594	30080.744823	32.169895
628.309862	30106.671969	32.174912
629.069045	30141.579323	32.179930
629.460050	30166.455517	32.184948
630.504708	30186.571304	32.189965
630.911452	30218.796600	32.194983
631.541734	30240.848009	32.200000
631.776318	30271.222804	32.205018
631.860935	30290.318730	32.210036
632.836278	30334.554420	32.215053
633.289415	30368.593231	32.220071
633.791169	30408.351544	32.225088
633.991128	30433.769820	32.230106
634.837260	30478.424172	32.235124
635.082210	30515.099981	32.240141
635.602441	30542.794751	32.245159
636.220636	30580.259619	32.250176
636.823777	30625.957198	32.255194
637.640610	30669.820045	32.260212
638.223113	30705.754625	32.265229
639.034678	30737.216048	32.270247
639.662642	30769.964044	32.275264
639.886524	30818.761646	32.280282
640.733009	30854.611141	32.285300
641.395294	30908.814994	32.290317
641.443802	30949.517257	32.295335
642.200548	30987.688255	32.300352
642.869552	31044.552722	32.305370
643.438121	31092.298529	32.310388
644.414121	31145.208846	32.315405
644.640120	31189.999205	32.320423
645.606503	31234.484759	32.325440
646.496600	31271.535588	32.330458
647.244959	31322.016422	32.335476
648.104729	31362.251844	32.340493
648.810919	31406.133480	32.345511
649.804162	31442.846163	32.350528
650.196464	31496.745902	32.355546
650.807412	31527.778290	32.360564
651.814698	31576.537904	32.365581
652.511536	31604.832442	32.370599
652.961113	31652.092339	32.375616
653.280076	31688.158155	32.380634
653.917764	31725.577815	32.385652
654.627166	31769.086745	32.390669
655.368992	31821.542160	32.395687
655.739488	31860.090979	32.400704
656.546624	31905.494120	32.405722
657.240550	31953.159181	32.410740
657.859113	31998.180971	32.415757
658.121861	32042.442749	32.420775
659.075810	32089.840064	32.425792
659.676717	32151.092801	32.430810
660.047890	32202.247704	32.435828
660.716244	32237.160097	32.440845
661.436932	32301.479652	32.445863
662.466447	32343.220427	32.450880
663.355240	32390.976271	32.455898
664.016200	32436.409651	32.460916
665.133364	32481.576134	32.465933
665.252510	32526.891757	32.470951
666.183460	32564.583369	32.475968
666.893913	32612.734153	32.480986
667.450423	32651.925602	32.486004
668.051994	32691.312410	32.491021
668.756268	32744.111060	32.496039
669.309813	32780.875596	32.501056
670.205602	32831.223353	32.506074
670.625383	32869.513492	32.511092
671.632168	32917.770577	32.516109
671.793238	32961.626563	32.521127
672.579139	33004.373853	32.526144
673.101726	33056.310175	32.531162
674.096819	33097.944027	32.536180
674.973992	33139.229641	32.541197
675.929987	33184.852639	32.546215
676.493133	33220.908385	32.551232
677.181602	33265.049587	32.556250
677.932526	33305.710332	32.561268
678.453747	33340.887720	32.566285
678.966814	33374.783047	32.571303
680.210044	33396.046969	32.576320
680.507923	33438.763644	32.581338
681.130064	33466.914292	32.586356
682.014156	33499.146241	32.591373
682.266613	33537.457329	32.596391
682.891770	33569.242888	32.601408
683.512132	33611.909715	32.606426
683.832470	33650.052387	32.611444
684.950108	33693.217288	32.616461
685.282990	33741.461063	32.621479
686.043649	33794.898457	32.626496
686.542715	33831.736545	32.631514
686.852446	33881.236050	32.636532
687.559228	33927.443178	32.641549
688.062657	33976.160403	32.646567
688.623832	34031.677877	32.651584
689.436715	34096.981209	32.656602
689.613200	34146.084807	32.661620
690.942679	34202.026850	32.666637
691.361505	34261.632368	32.671655
692.358598	34313.403103	32.676672
692.892616	34371.770779	32.681690
693.487413	34431.305127	32.686708
694.376917	34480.722112	32.691725
695.141067	34551.711998	32.696743
695.623424	34606.996683	32.701760
696.408404	34672.382016	32.706778
697.147466	34724.908374	32.711796
698.305795	34782.111495	32.716813
698.809285	34836.343951	32.721831
700.015803	34880.439519	32.726848
700.452886	34931.464374	32.731866
701.416145	34984.057638	32.736884
702.083569	35037.430510	32.741901
703.073587	35095.741850	32.746919
703.601801	35143.035325	32.751936
704.182475	35190.548354	32.756954
705.361340	35234.661614	32.761972
705.673805	35288.197861	32.766989
706.727967	35336.699723	32.772007
707.571215	35381.769682	32.777024
708.365086	35430.761192	32.782042
708.778981	35474.987715	32.787060
709.630889	35515.200746	32.792077
710.072199	35568.546931	32.797095
710.683342	35609.663842	32.802112
711.308789	35669.810221	32.807130
712.164388	35726.696307	32.812148
713.116765	35768.987033	32.817165
713.237951	35830.034333	32.822183
714.293848	35876.867933	32.827200
715.131354	35922.331955	32.832218
715.553614	35977.326081	32.837236
716.048795	36022.951098	32.842253
716.726711	36073.896955	32.847271
717.573146	36125.986444	32.852288
718.661526	36181.288394	32.857306
719.233336	36240.186473	32.862324
720.332307	36282.480696	32.867341
720.712411	36338.980867	32.872359
721.526866	36384.253455	32.877376
722.044038	36442.578883	32.882394
722.582800	36487.768148	32.887412
723.747877	36537.798317	32.892429
724.207444	36588.602353	32.897447
725.051116	36643.709647	32.902464
725.885924	36695.524127	32.907482
726.487245	36754.241988	32.912500
727.404717	36796.103901	32.917517
727.695241	36842.097660	32.922535
728.246765	36885.401484	32.927552
729.101830	36925.483912	32.932570
729.835141	36982.474598	32.937588
730.560498	37026.624249	32.942605
731.312966	37079.217587	32.947623
731.852025	37120.860824	32.952640
732.743539	37163.189095	32.957658
733.451909	37226.741519	32.962676
734.293785	37274.363984	32.967693
734.760041	37327.723343	32.972711
735.654754	37379.131791	32.977728
736.789579	37416.433601	32.982746
737.811058	37467.126964	32.987764
738.404791	37516.635011	32.992781
739.492027	37558.155826	32.997799
739.916592	37598.780787	33.002816
740.576059	37647.741418	33.007834
741.102450	37700.181777	33.012852
742.016049	37746.927825	33.017869
742.523339	37800.237710	33.022887
743.403479	37842.663950	33.027904
744.338802	37894.054668	33.032922
744.904367	37946.717177	33.037940
745.639606	38001.693093	33.042957
746.677746	38049.204526	33.047975
747.150160	38104.904559	33.052992
747.699664	38144.638459	33.058010
748.538704	38204.929475	33.063028
749.497215	38253.775380	33.068045
750.389310	38313.135200	33.073063
750.938566	38374.844020	33.078080
751.435015	38415.117863	33.083098
752.282722	38479.999243	33.088116
753.166097	38534.504485	33.093133
753.887261	38596.661454	33.098151
754.285038	38651.868629	33.103168
755.036596	38712.054535	33.108186
756.039701	38765.782881	33.113204
756.508774	38828.213738	33.118221
757.618715	38881.622204	33.123239
758.156323	38953.363960	33.128256
759.364771	38993.926447	33.133274
760.103059	39047.639807	33.138292
761.214826	39094.003807	33.143309
762.203029	39149.702136	33.148327
762.878660	39194.395193	33.153344
763.899218	39236.909834	33.158362
764.720394	39283.281535	33.163380
765.298082	39322.981605	33.168397
766.206487	39383.783682	33.173415
767.180255	39428.051379	33.178432
768.035978	39464.167039	33.183450
768.467715	39506.033973	33.188468
769.078333	39547.721368	33.193485
769.785039	39601.143796	33.198503
770.449285	39642.045177	33.203520
770.975185	39697.785267	33.208538
771.707490	39749.389092	33.213556
772.984214	39790.941644	33.218573
773.488927	39835.409673	33.223591
774.099031	39895.760028	33.228608
775.049438	39944.332769	33.233626
775.528591	40002.155210	33.238644
776.382042	40057.054725	33.243661
777.403470	40104.845232	33.248679
777.556042	40153.017738	33.253696
778.212159	40200.359393	33.258714
778.964769	40257.773146	33.263732
780.153743	40292.472297	33.268749
781.019457	40329.757817	33.273767
781.878878	40376.631842	33.278784
782.605174	40424.026302	33.283802
783.176970	40466.176849	33.288820
784.009625	40526.247669	33.293837
784.719068	40584.181267	33.298855
785.092449	40629.929892	33.303872
786.008342	40682.816480	33.308890
786.779300	40746.957697	33.313908
787.534208	40801.134491	33.318925
788.487449	40851.043250	33.323943
788.863882	40905.298192	33.328960
789.716526	40955.924853	33.333978
790.440839	41023.660052	33.338996
791.187164	41078.717960	33.344013
792.253146	41138.450577	33.349031
793.232630	41206.330030	33.354048
794.019263	41267.516832	33.359066
794.675081	41324.587973	33.364084
795.409780	41382.323702	33.369101
796.244834	41438.994097	33.374119
796.758140	41504.613308	33.379136
798.129406	41572.085063	33.384154
798.501211	41627.050865	33.389172
799.373429	41690.135540	33.394189
800.258544	41751.049058	33.399207
801.001412	41821.686825	33.404224
802.395604	41877.284678	33.409242
802.966024	41933.472606	33.414260
803.750973	41999.398868	33.419277
804.597205	42052.249021	33.424295
805.082946	42121.523704	33.429312
806.148986	42181.727189	33.434330
806.971244	42256.357537	33.439348
808.222067	42307.247905	33.444365
809.047898	42370.885689	33.449383
809.680340	42427.583856	33.454400
810.586995	42484.587347	33.459418
811.169427	42537.840248	33.464436
811.911857	42601.282962	33.469453
813.024635	42651.386040	33.474471
813.494105	42706.016772	33.479488
814.808250	42773.330346	33.484506
815.526651	42832.906645	33.489524
816.156059	42888.847487	33.494541
817.123086	42950.118425	33.499559
818.023686	43005.561952	33.504576
818.955430	43053.689121	33.509594
819.342365	43120.129773	33.514612
820.328274	43174.586400	33.519629
821.226762	43232.567148	33.524647
822.279121	43302.282318	33.529664
822.747301	43352.240658	33.534682
823.809991	43421.062764	33.539700
824.369210	43474.878146	33.544717
825.098929	43538.085181	33.549735
825.747508	43600.406862	33.554752
826.709079	43650.788755	33.559770
827.409819	43715.291134	33.564788
828.437093	43772.981271	33.569805
829.599783	43829.088161	33.574823
829.536491	43896.853615	33.579840
830.799940	43954.994502	33.584858
831.573304	44025.862295	33.589876
832.582455	44080.766629	33.594893
833.580397	44130.188839	33.599911
834.329263	44188.239661	33.604928
835.163872	44227.680924	33.609946
836.011997	44279.606304	33.614964
836.767557	44338.029668	33.619981
837.459987	44387.879530	33.624999
838.358737	44440.777833	33.630016
838.846269	44498.920750	33.635034
840.244363	44553.284981	33.640052
840.488829	44616.608579	33.645069
841.320480	44665.026827	33.650087
842.249890	44739.522370	33.655104
842.962130	44794.455711	33.660122
843.934919	44856.502734	33.665140
844.621430	44916.095925	33.670157
845.507267	44980.288517	33.675175
846.059100	45046.000808	33.680192
847.103660	45110.548598	33.685210
848.273312	45183.452145	33.690228
848.978013	45246.636307	33.695245
850.074730	45308.254133	33.700263
850.509050	45380.981813	33.705280
851.471726	45448.301296	33.710298
852.342885	45512.712776	33.715316
853.122403	45582.616739	33.720333
854.336980	45639.181895	33.725351
855.282691	45711.268056	33.730368
855.964147	45770.320303	33.735386
856.975048	45843.029313	33.740404
857.527164	45909.104663	33.745421
858.655793	45977.431005	33.750439
859.218680	46046.883054	33.755456
860.069623	46116.581465	33.760474
861.137254	46184.532058	33.765492
861.821427	46253.225741	33.770509
862.771843	46328.431805	33.775527
863.683505	46393.971845	33.780544
864.609244	46461.002804	33.785562
865.768626	46528.035547	33.790580
866.580221	46604.763393	33.795597
867.549535	46663.697268	33.800615
868.365893	46734.351876	33.805632
869.579560	46798.087455	33.810650
870.834972	46861.671219	33.815668
871.390095	46926.970989	33.820685
872.742244	46967.614392	33.825703
873.330437	47029.923411	33.830720
874.551229	47085.485400	33.835738
875.695800	47141.457936	33.840756
876.041691	47200.895134	33.845773
877.259733	47245.241722	33.850791
877.713724	47301.094412	33.855808
878.800942	47355.412628	33.860826
879.796205	47417.551806	33.865844
880.202308	47476.417324	33.870861
881.034761	47531.313349	33.875879
881.802014	47595.493921	33.880896
882.596691	47659.379399	33.885914
883.807298	47719.537398	33.890932
884.576586	47791.695642	33.895949
885.564014	47842.937007	33.900967
886.297499	47904.245241	33.905984
887.069344	47962.719794	33.911002
888.433859	48028.681219	33.916020
888.698615	48085.495276	33.921037
890.064247	48143.232573	33.926055
890.747744	48209.623181	33.931072
891.066954	48281.245708	33.936090
892.379184	48333.279036	33.941108
892.937862	48392.458483	33.946125
893.689242	48452.829096	33.951143
894.455302	48514.772882	33.956160
895.032753	48579.371699	33.961178
896.357892	48631.846559	33.966196
896.983510	48696.773517	33.971213
898.009549	48758.120760	33.976231
899.069846	48817.545882	33.981248
899.728972	48890.218236	33.986266
900.822234	48949.455100	33.991284
901.633986	49021.452473	33.996301
902.578939	49092.954838	34.001319
903.585968	49161.025035	34.006336
904.258203	49222.548809	34.011354
905.335307	49281.934566	34.016372
906.006483	49352.891979	34.021389
907.032227	49433.828641	34.026407
908.058596	49498.062822	34.031424
908.733632	49576.783273	34.036442
909.849602	49647.412963	34.041460
910.457917	49716.109963	34.046477
911.259202	49792.799573	34.051495
912.359381	49860.673873	34.056512
913.286312	49945.132809	34.061530
914.858324	50002.013871	34.066548
915.784421	50072.269505	34.071565
917.079160	50133.420441	34.076583
918.073014	50198.781517	34.081600
919.072059	50258.068072	34.086618
920.051427	50323.210313	34.091636
920.886166	50395.796838	34.096653
922.173423	50449.642082	34.101671
922.780749	50515.671622	34.106688
923.514429	50582.896480	34.111706
924.043524	50645.578898	34.116724
924.983422	50714.100726	34.121741
925.948900	50783.884199	34.126759
927.259239	50853.500313	34.131776
927.665050	50927.338457	34.136794
928.887144	50987.440012	34.141812
929.557813	51074.189131	34.146829
930.628587	51140.939219	34.151847
931.374038	51212.181863	34.156864
932.168591	51286.618674	34.161882
933.364336	51365.106007	34.166900
933.887667	51441.091428	34.171917
935.453313	51511.473352	34.176935
936.184712	51591.096723	34.181952
936.736150	51668.027613	34.186970
937.982446	51735.264612	34.191988
938.905138	51814.707116	34.197005
939.626764	51895.427693	34.202023
940.786588	51965.507180	34.207040
941.475837	52040.962543	34.212058
942.763758	52100.632804	34.217076
943.851128	52183.752513	34.222093
944.798190	52253.612889	34.227111
945.531338	52321.646475	34.232128
946.310327	52399.404913	34.237146
947.701505	52466.602496	34.242164
948.501941	52548.749434	34.247181
949.543387	52622.380131	34.252199
950.569867	52685.566456	34.257216
951.601369	52759.344670	34.262234
952.419086	52831.023967	34.267252
953.283430	52896.254632	34.272269
953.992351	52959.529098	34.277287
954.828806	53036.293591	34.282304
955.768560	53110.568104	34.287322
957.040963	53167.952872	34.292340
957.822030	53238.215377	34.297357
958.589414	53305.771921	34.302375
959.953021	53370.711049	34.307392
960.504668	53441.351577	34.312410
961.257857	53502.943745	34.317428
961.741555	53581.872116	34.322445
963.004817	53663.204238	34.327463
964.155746	53726.006987	34.332480
964.797008	53817.257399	34.337498
966.156218	53888.070980	34.342516
967.169342	53963.539091	34.347533
968.181943	54036.197893	34.352551
968.823092	54113.091235	34.357568
969.698310	54192.391019	34.362586
970.786814	54263.241543	34.367604
972.158347	54342.154499	34.372621
973.174595	54419.173968	34.377639
974.200733	54506.506999	34.382656
974.807349	54577.306917	34.387674
975.922601	54651.445083	34.392692
977.127790	54731.796421	34.397709
977.951665	54808.574995	34.402727
979.171393	54890.386427	34.407744
979.851485	54977.566235	34.412762
981.288578	55044.960247	34.417780
982.154838	55126.821190	34.422797
983.259215	55195.722931	34.427815
984.371927	55266.876461	34.432832
984.949717	55351.561224	34.437850
986.551168	55427.670204	34.442868
987.664547	55503.114980	34.447885
988.444307	55573.239104	34.452903
989.854574	55643.701951	34.457920
990.732463	55714.849082	34.462938
992.025537	55791.095831	34.467956
992.607020	55865.434802	34.472973
993.887809	55928.887698	34.477991
995.233043	55986.812258	34.483008
995.891351	56069.544192	34.488026
996.773110	56137.306214	34.493044
997.519262	56207.247583	34.498061
998.569901	56288.394019	34.503079
999.621947	56352.554485	34.508096
1000.339296	56437.575797	34.513114
1001.291142	56510.042810	34.518132
1002.477133	56593.871556	34.523149
1003.328497	56674.347841	34.528167
1004.044071	56745.757482	34.533184
1004.915316	56828.604464	34.538202
1006.307784	56902.674871	34.543220
1008.006450	56965.230086	34.548237
1008.798638	57045.482668	34.553255
1009.985716	57108.750774	34.558272
1011.250029	57189.917645	34.563290
1012.205354	57263.702803	34.568308
1013.150169	57329.717957	34.573325
1014.101215	57397.896807	34.578343
1015.056996	57457.474119	34.583360
1015.717114	57536.729949	34.588378
1016.841566	57622.179429	34.593396
1017.712810	57694.833460	34.598413
1018.712792	57765.334801	34.603431
1019.596374	57848.575787	34.608448
1020.586101	57937.458701	34.613466
1021.155044	58006.540519	34.618484
1022.446440	58079.250564	34.623501
1022.987766	58158.875034	34.628519
1024.036300	58235.920814	34.633536
1025.086998	58306.928506	34.638554
1025.992699	58376.939983	34.643572
1027.084965	58457.251837	34.648589
1027.603130	58538.950808	34.653607
1028.958585	58616.456364	34.658624
1029.624129	58697.424057	34.663642
1030.828279	58769.795329	34.668660
1032.354512	58853.971421	34.673677
1033.408959	58931.759028	34.678695
1034.779047	59012.320630	34.683712
1035.800860	59086.195963	34.688730
1036.899113	59162.812895	34.693748
1038.040205	59233.290233	34.698765
1039.115478	59320.215471	34.703783
1040.140910	59385.609758	34.708800
1041.218620	59476.282193	34.713818
1042.360818	59542.880310	34.718836
1043.678588	59609.989286	34.723853
1044.558868	59691.901616	34.728871
1045.586173	59761.777910	34.733888
1046.712077	59846.399537	34.738906
1047.323547	59919.575407	34.743924
1048.605496	59987.032798	34.748941
1049.360016	60082.353072	34.753959
1050.612536	60158.828871	34.758976
1051.908309	60248.122031	34.763994
1052.803399	60314.678441	34.769012
1053.746279	60404.748686	34.774029
1054.531373	60500.439286	34.779047
1055.690270	60576.361294	34.784064
1056.540039	60668.681399	34.789082
1057.498404	60760.060801	34.794100
1058.886325	60842.277762	34.799117
1059.678412	60936.063707	34.804135
1061.122144	61011.588259	34.809152
1061.910924	61110.287342	34.814170
1062.826769	61199.060766	34.819188
1064.428839	61273.092943	34.824205
1065.626562	61367.785874	34.829223
1067.008844	61433.452931	34.834240
1068.517668	61507.456021	34.839258
1069.189144	61595.332081	34.844276
1070.359380	61673.692770	34.849293
1071.125491	61767.935366	34.854311
1072.251552	61845.670476	34.859328
1073.536696	61929.002175	34.864346
1074.390357	62004.672273	34.869364
1075.666218	62085.961327	34.874381
1076.611574	62173.030871	34.879399
1077.712793	62241.180937	34.884416
1078.478726	62323.373068	34.889434
1079.941384	62401.317073	34.894452
1081.213632	62490.337194	34.899469
1082.125640	62569.772752	34.904487
1083.182078	62640.266749	34.909504
1084.543599	62715.461165	34.914522
1085.387641	62802.301814	34.919540
1086.566510	62882.082983	34.924557
1087.608619	62972.254796	34.929575
1088.443242	63048.722345	34.934592
1089.629056	63126.262271	34.939610
1091.257705	63199.181950	34.944628
1092.588098	63250.320996	34.949645
1093.687966	63335.977886	34.954663
1094.688907	63398.917810	34.959680
1095.738024	63445.922945	34.964698
1096.171237	63524.201647	34.969716
1097.358566	63589.347701	34.974733
1098.047868	63657.692391	34.979751
1099.268320	63714.236776	34.984768
1100.327764	63789.658724	34.989786
1101.348707	63875.443706	34.994804
1102.114089	63941.302078	34.999821
1103.320471	64030.337973	35.004839
1104.531808	64110.339601	35.009856
1105.195718	64192.971619	35.014874
1106.298645	64274.807546	35.019892
1107.506235	64358.469681	35.024909
1108.561443	64457.507805	35.029927
1109.606792	64536.713642	35.034944
1110.838688	64616.099606	35.039962
1111.800207	64709.898781	35.044980
1113.042041	64798.678661	35.049997
1114.009472	64893.148666	35.055015
1114.621910	64972.575204	35.060032
1116.243523	65066.013397	35.065050
1117.330475	65163.156434	35.070068
1119.020464	65245.891770	35.075085
1119.988537	65349.030416	35.080103
1120.643382	65446.893895	35.085120
1121.798264	65535.955814	35.090138
1122.963962	65633.930431	35.095156
1124.360528	65720.454631	35.100173
1125.536134	65820.150470	35.105191
1126.798268	65903.777605	35.110208
1128.329001	65998.556601	35.115226
1128.978799	66100.120762	35.120244
1130.487776	66188.129546	35.125261
1131.410387	66282.535758	35.130279
1132.735815	66374.695357	35.135296
1134.079387	66454.240674	35.140314
1135.066407	66551.467918	35.145332
1136.032872	66642.937280	35.150349
1137.645194	66734.249459	35.155367
1138.425919	66820.898606	35.160384
1139.855826	66901.178981	35.165402
1140.758881	66999.522661	35.170420
1142.211142	67084.592972	35.175437
1143.261831	67176.285404	35.180455
1144.332601	67260.947163	35.185472
1145.647600	67350.060179	35.190490
1146.228423	67453.786843	35.195508
1147.827592	67535.448458	35.200525
1149.089429	67637.170418	35.205543
1150.195071	67726.133721	35.210560
1151.135771	67812.083861	35.215578
1152.239492	67905.771430	35.220596
1153.346195	68003.403467	35.225613
1154.502071	68101.199175	35.230631
1155.482229	68185.270264	35.235648
1156.829006	68281.093128	35.240666
1157.707679	68378.040275	35.245684
1159.128688	68467.374956	35.250701
1160.145325	68566.283166	35.255719
1161.662761	68661.093132	35.260736
1163.141791	68751.445516	35.265754
1163.734334	68852.060771	35.270772
1165.349785	68927.690074	35.275789
1166.290396	69024.724994	35.280807
1167.398038	69118.922926	35.285824
1168.822143	69218.985939	35.290842
1170.177431	69308.732681	35.295860
1171.168326	69396.871152	35.300877
1172.245872	69466.146175	35.305895
1173.009420	69543.993106	35.310912
1174.677441	69615.297833	35.315930
1175.622179	69703.742139	35.320948
1176.682405	69774.154115	35.325965
1177.798856	69861.179183	35.330983
1178.718191	69945.829034	35.336000
1180.056466	70035.327662	35.341018
1181.153396	70122.717575	35.346036
1182.312578	70211.662132	35.351053
1183.425496	70295.067219	35.356071
1184.545814	70382.612670	35.361088
1186.079944	70473.247444	35.366106
1186.960894	70566.346127	35.371124
1188.011728	70654.378226	35.376141
1189.142107	70750.250261	35.381159
1190.600832	70845.071037	35.386176
1191.502793	70944.804051	35.391194
1192.969326	71033.937873	35.396212
1194.541909	71133.415245	35.401229
1195.385427	71230.042919	35.406247
1196.274264	71325.954665	35.411264
1197.869144	71415.310443	35.416282
1199.210541	71516.902298	35.421300
1200.321954	71609.968827	35.426317
1201.717071	71707.411616	35.431335
1202.791960	71809.020757	35.436352
1204.091882	71898.981358	35.441370
1205.174403	71999.551509	35.446388
1206.196158	72093.887560	35.451405
1207.524409	72193.065026	35.456423
1208.958424	72301.016119	35.461440
1210.151398	72396.289165	35.466458
1211.508047	72485.622341	35.471476
1213.153595	72581.889506	35.476493
1214.471273	72672.622580	35.481511
1215.098214	72770.606837	35.486528
1216.314890	72871.476072	35.491546
1217.733252	72978.596447	35.496564
1218.798268	73071.308058	35.501581
1220.059032	73164.078185	35.506599
1221.333251	73271.260178	35.511616
1222.409924	73365.224914	35.516634
1223.510565	73477.957054	35.521652
1225.061563	73562.589915	35.526669
1226.543309	73657.100597	35.531687
1228.205370	73745.985180	35.536704
1229.574973	73835.054910	35.541722
1230.398332	73944.349029	35.546740
1231.399759	74029.271577	35.551757
1232.769623	74121.736747	35.556775
1233.911441	74229.690517	35.561792
1235.336022	74317.752672	35.566810
1236.389509	74426.404965	35.571828
1237.514114	74509.017265	35.576845
1239.060187	74607.599873	35.581863
1239.592006	74712.255946	35.586880
1241.168116	74801.575422	35.591898
1242.469363	74913.509748	35.596916
1243.769119	75010.371531	35.601933
1244.798476	75104.552425	35.606951
1246.001374	75213.995321	35.611968
1247.157771	75303.280465	35.616986
1248.688495	75408.619774	35.622004
1249.664160	75515.996585	35.627021
1250.750342	75617.086518	35.632039
1251.893096	75721.664095	35.637056
1253.315148	75818.497086	35.642074
1254.563395	75913.520762	35.647092
1255.635476	76004.569404	35.652109
1256.772596	76090.782065	35.657127
1257.880279	76193.707540	35.662144
1259.721846	76281.318551	35.667162
1260.874780	76372.963874	35.672180
1261.999549	76463.283828	35.677197
1263.537079	76554.388546	35.682215
1264.570410	76646.864120	35.687232
1266.250899	76734.843691	35.692250
1267.367631	76837.858879	35.697268
1268.489001	76927.737549	35.702285
1269.785720	77012.091516	35.707303
1270.836927	77120.527008	35.712320
1272.329818	77221.002253	35.717338
1273.582426	77324.340160	35.722356
1274.436792	77418.923715	35.727373
1276.340712	77525.467281	35.732391
1277.518748	77614.452655	35.737408
1278.394215	77713.353668	35.742426
1279.941665	77829.644815	35.747444
1281.115368	77935.518231	35.752461
1282.402145	78037.776744	35.757479
1283.454148	78131.419907	35.762496
1284.697657	78247.076062	35.767514
1286.260106	78354.132061	35.772532
1287.438097	78472.168307	35.777549
1288.835721	78568.888213	35.782567
1289.784621	78681.577013	35.787584
1291.687217	78800.971408	35.792602
1293.010022	78899.756396	35.797620
1293.979732	79010.467033	35.802637
1295.677831	79121.850186	35.807655
1296.925602	79224.410563	35.812672
1298.439004	79334.632481	35.817690
1299.685622	79435.660921	35.822708
1300.695797	79550.738108	35.827725
1302.434644	79657.797057	35.832743
1303.715367	79772.452992	35.837760
1304.834018	79875.517295	35.842778
1306.585620	79981.245280	35.847796
1307.671939	80081.857618	35.852813
1309.182274	80188.054689	35.857831
1310.676360	80300.513199	35.862848
1311.736361	80394.403507	35.867866
1313.058933	80499.528783	35.872884
1314.514298	80610.284240	35.877901
1315.809213	80704.899181	35.882919
1317.119859	80813.701574	35.887936
1318.549781	80916.429891	35.892954
1319.924941	81024.957010	35.897972
1321.106692	81134.173465	35.902989
1322.537285	81229.161815	35.908007
1323.436169	81341.489116	35.913024
1324.797994	81443.178399	35.918042
1326.410285	81562.275112	35.923060
1327.921022	81659.786371	35.928077
1329.219036	81766.035162	35.933095
1330.280403	81867.734741	35.938112
1331.671809	81977.948098	35.943130
1333.106676	82080.477196	35.948148
1334.127282	82179.358871	35.953165
1335.797025	82287.464925	35.958183
1336.994629	82387.992213	35.963200
1338.165657	82496.911554	35.968218
1339.947350	82603.772403	35.973236
1341.147089	82701.804472	35.978253
1342.341751	82797.519030	35.983271
1343.712934	82898.844679	35.988288
1344.625944	82986.570805	35.993306
1346.450845	83082.048856	35.998324
1347.567956	83168.464077	36.003341
1349.026753	83256.093415	36.008359
1350.469747	83349.085066	36.013376
1351.640342	83441.384534	36.018394
1352.778510	83537.414475	36.023412
1353.709927	83644.386253	36.028429
1355.146249	83742.182364	36.033447
1356.215001	83844.470743	36.038464
1357.310554	83958.615072	36.043482
1358.738187	84066.955658	36.048500
1359.837287	84184.800191	36.053517
1361.828877	84298.540324	36.058535
1363.015641	84424.519546	36.063552
1363.678161	84541.065043	36.068570
1365.310596	84660.146298	36.073588
1366.669416	84780.068910	36.078605
1368.153849	84901.543688	36.083623
1369.840749	85028.892223	36.088640
1371.093470	85150.518159	36.093658
1372.834445	85258.903177	36.098676
1373.929303	85389.703341	36.103693
1375.453597	85500.036361	36.108711
1376.925759	85623.796942	36.113728
1378.294737	85742.518197	36.118746
1379.624390	85860.245012	36.123764
1381.403303	85986.354316	36.128781
1382.589018	86104.776123	36.133799
1383.925886	86233.971155	36.138816
1385.261843	86346.060066	36.143834
1387.249828	86466.677404	36.148852
1388.445409	86581.374115	36.153869
1389.796019	86699.531917	36.158887
1391.409851	86818.371528	36.163904
1392.933316	86939.253207	36.168922
1394.420047	87051.802905	36.173940
1395.665162	87170.878752	36.178957
1397.561068	87286.381624	36.183975
1399.432338	87384.008337	36.188992
1401.188787	87491.246121	36.194010
1402.455383	87593.288879	36.199028
1403.360508	87697.352463	36.204045
1405.493707	87799.666569	36.209063
1406.835908	87901.293116	36.214080
1407.678226	88008.700422	36.219098
1409.182896	88113.166388	36.224116
1410.610667	88228.467045	36.229133
1411.865104	88339.017565	36.234151
1413.070555	88448.929821	36.239168
1414.352643	88562.353564	36.244186
1415.803688	88668.223842	36.249204
1417.129443	88782.211906	36.254221
1418.448786	88892.247486	36.259239
1419.964519	89014.380851	36.264256
1421.098909	89127.829754	36.269274
1422.946538	89247.352490	36.274292
1424.260695	89356.642897	36.279309
1426.007687	89465.587528	36.284327
1427.573866	89579.984799	36.289344
1429.155983	89693.543600	36.294362
1430.463550	89796.284622	36.299380
1431.807670	89903.037732	36.304397
1433.438070	90002.801695	36.309415
1434.762027	90110.293737	36.314432
1436.219365	90235.761629	36.319450
1437.749513	90338.824732	36.324468
1438.709507	90434.284127	36.329485
1440.082360	90518.577560	36.334503
1441.316007	90624.146459	36.339520
1442.347331	90731.622915	36.344538
1443.625730	90834.726909	36.349556
1445.113330	90946.759001	36.354573
1446.099884	91058.096399	36.359591
1447.806866	91178.535927	36.364608
1448.718518	91294.537142	36.369626
1450.014190	91409.275012	36.374644
1451.558482	91530.793205	36.379661
1452.928858	91663.732882	36.384679
1454.345271	91791.634378	36.389696
1455.736840	91926.599761	36.394714
1457.479321	92056.340068	36.399732
1458.676289	92189.397764	36.404749
1459.748327	92312.995131	36.409767
1461.581747	92451.341481	36.414784
1463.045404	92588.275785	36.419802
1464.798068	92721.046528	36.424820
1466.229837	92854.171984	36.429837
1467.743748	92991.049580	36.434855
1469.268761	93116.087976	36.439872
1470.758161	93262.831451	36.444890
1472.393337	93388.601622	36.449908
1474.216599	93522.087322	36.454925
1475.812981	93653.986539	36.459943
1477.494091	93784.909845	36.464960
1478.908783	93918.346789	36.469978
1480.163747	94043.392980	36.474996
1482.306549	94177.744397	36.480013
1483.610263	94296.243705	36.485031
1485.256502	94423.372630	36.490048
1486.518388	94556.633323	36.495066
1488.884030	94667.249576	36.500084
1490.405268	94782.941019	36.505101
1491.765970	94913.386630	36.510119
1493.536719	95027.316305	36.515136
1494.783332	95150.302191	36.520154
1495.925770	95268.374012	36.525172
1497.596623	95396.035475	36.530189
1499.137040	95525.644455	36.535207
1500.930319	95648.078229	36.540224
1502.250982	95777.316840	36.545242
1503.842120	95893.888844	36.550260
1505.484203	96009.426615	36.555277
1506.651202	96135.382246	36.560295
1508.576143	96255.326123	36.565312
1509.802705	96386.724129	36.570330
1511.207449	96505.203465	36.575348
1512.924538	96625.979702	36.580365
1514.294841	96746.594887	36.585383
1515.691112	96869.589607	36.590400
1517.208811	97007.004092	36.595418
1518.613057	97127.881656	36.600436
1520.124538	97252.786732	36.605453
1521.301587	97385.971303	36.610471
1523.117461	97509.308856	36.615488
1524.735000	97644.530240	36.620506
1526.766662	97766.859126	36.625524
1528.584482	97880.804541	36.630541
1529.470555	98013.846898	36.635559
1531.317605	98132.301537	36.640576
1532.452702	98271.099440	36.645594
1534.480756	98383.568797	36.650612
1535.756596	98518.885124	36.655629
1537.485968	98638.374110	36.660647
1538.540779	98757.676969	36.665664
1539.779517	98874.593734	36.670682
1540.873657	98985.511865	36.675700
1542.654504	99093.509199	36.680717
1543.914355	99219.538724	36.685735
1545.753023	99333.917118	36.690752
1546.510651	99457.236780	36.695770
1548.037801	99581.844315	36.700788
1549.401093	99723.452705	36.705805
1550.757429	99853.133434	36.710823
1552.468793	99980.464823	36.715840
1553.658101	100131.343896	36.720858
1555.177560	100268.860920	36.725876
1557.175423	100407.280241	36.730893
1558.305879	100553.086748	36.735911
1560.101862	100689.751157	36.740928
1561.729380	100849.604545	36.745946
1563.626843	100982.501790	36.750964
1565.664423	101118.382415	36.755981
1566.925178	101265.325524	36.760999
1568.512740	101406.500681	36.766016
1570.453452	101551.741832	36.771034
1571.718244	101696.708490	36.776052
1573.739147	101829.906933	36.781069
1575.038928	101967.439981	36.786087
1576.962043	102107.057241	36.791104
1578.340093	102255.774174	36.796122
1580.231112	102392.836637	36.801140
1582.183497	102523.588973	36.806157
1584.075173	102666.738093	36.811175
1586.009446	102791.979202	36.816192
1587.205750	102926.705074	36.821210
1589.016485	103058.546577	36.826228
1590.560483	103188.934045	36.831245
1591.739767	103318.960397	36.836263
1593.835872	103450.036362	36.841280
1595.204842	103586.120026	36.846298
1597.038634	103728.902394	36.851316
1598.964956	103852.627300	36.856333
1599.660529	103991.860365	36.861351
1601.738344	104125.198693	36.866368
1603.708290	104250.148149	36.871386
1605.843869	104374.527094	36.876404
1607.194163	104502.870500	36.881421
1608.649989	104626.240419	36.886439
1610.499173	104753.150466	36.891456
1612.562215	104880.053068	36.896474
1614.051064	105006.868010	36.901492
1615.852232	105133.774293	36.906509
1617.130374	105255.234240	36.911527
1618.663383	105382.183198	36.916544
1620.099068	105521.003119	36.921562
1621.621656	105640.816113	36.926580
1623.072872	105769.744592	36.931597
1624.531163	105912.138249	36.936615
1625.986845	106036.489696	36.941632
1627.564615	106171.498945	36.946650
1628.782728	106304.954375	36.951668
1630.660334	106450.429622	36.956685
1631.748811	106597.435783	36.961703
1633.412848	106733.765230	36.966720
1635.276923	106886.991906	36.971738
1636.635488	107044.482372	36.976756
1638.475780	107187.126237	36.981773
1639.672567	107338.366574	36.986791
1641.366212	107490.214980	36.991808
1642.801006	107647.544194	36.996826
1644.219551	107793.844750	37.001844
1646.180988	107940.555968	37.006861
1647.909949	108087.861935	37.011879
1649.258391	108222.661370	37.016896
1651.200738	108356.341771	37.021914
1652.604992	108494.265678	37.026932
1654.291149	108616.041827	37.031949
1655.776171	108771.859356	37.036967
1657.248780	108916.736017	37.041984
1658.719421	109066.001152	37.047002
1660.494415	109208.143632	37.052020
1662.177027	109356.121614	37.057037
1663.593848	109499.259418	37.062055
1665.322913	109664.350798	37.067072
1667.132253	109812.095413	37.072090
1668.732467	109971.894924	37.077108
1670.764881	110125.071716	37.082125
1672.225014	110280.899860	37.087143
1673.788972	110432.223353	37.092160
1675.798484	110582.146606	37.097178
1677.580123	110749.263928	37.102196
1679.899347	110892.241604	37.107213
1681.187871	111049.431413	37.112231
1683.134621	111195.220181	37.117248
1685.069257	111343.281447	37.122266
1686.514694	111506.295098	37.127284
1688.231419	111644.296909	37.132301
1690.355176	111788.145622	37.137319
1692.097092	111932.333347	37.142336
1694.117157	112087.841348	37.147354
1695.695464	112224.624126	37.152372
1697.606475	112378.349529	37.157389
1699.313214	112536.951934	37.162407
1700.964950	112678.785163	37.167424
1703.057725	112830.962366	37.172442
1704.448130	112973.192533	37.177460
1706.036006	113119.476218	37.182477
1707.469025	113270.553151	37.187495
1709.333373	113425.101967	37.192512
1710.718331	113577.024699	37.197530
1712.448434	113731.836688	37.202548
1714.290994	113886.061121	37.207565
1715.903427	114047.665247	37.212583
1717.509351	114208.510147	37.217600
1719.263925	114362.382500	37.222618
1720.942559	114521.074088	37.227636
1722.667061	114671.743691	37.232653
1724.131850	114845.372275	37.237671
1725.971597	115004.586252	37.242688
1727.768298	115174.004737	37.247706
1729.317616	115337.831237	37.252724
1731.515927	115496.534952	37.257741
1733.411689	115660.334335	37.262759
1735.283023	115817.809329	37.267776
1736.971343	115975.097864	37.272794
1738.443484	116142.440532	37.277812
1740.055601	116300.769659	37.282829
1741.994062	116463.462504	37.287847
1743.803154	116618.325122	37.292864
1745.664798	116781.145465	37.297882
1746.458414	116961.395115	37.302900
1748.501176	117114.498460	37.307917
1750.541303	117283.698461	37.312935
1752.291854	117444.065664	37.317952
1754.324780	117608.334272	37.322970
1756.188512	117776.676086	37.327988
1758.011566	117929.334971	37.333005
1759.834093	118089.122952	37.338023
1761.401976	118240.072423	37.343040
1763.088237	118395.468869	37.348058
1764.602438	118545.108770	37.353076
1766.416831	118689.362502	37.358093
1768.215537	118837.411808	37.363111
1769.731120	118973.582540	37.368128
1771.718509	119117.113340	37.373146
1773.073915	119267.782866	37.378164
1774.564995	119421.970825	37.383181
1776.434374	119581.998809	37.388199
1778.034264	119733.925940	37.393216
1780.063674	119895.845694	37.398234
1781.527092	120061.456657	37.403252
1783.041199	120227.111184	37.408269
1784.596923	120397.580149	37.413287
1785.987478	120564.435037	37.418304
1787.946755	120741.654452	37.423322
1789.790343	120922.025859	37.428340
1791.871137	121097.502843	37.433357
1793.815347	121265.707988	37.438375
1795.304975	121450.310315	37.443392
1797.309342	121629.454903	37.448410
1799.061954	121812.013761	37.453428
1801.139619	121998.696334	37.458445
1802.495777	122178.921094	37.463463
1804.354776	122371.474725	37.468480
1806.101738	122550.790448	37.473498
1808.090866	122739.494626	37.478516
1810.217307	122929.370780	37.483533
1812.028534	123109.300635	37.488551
1813.807886	123299.067672	37.493568
1816.026887	123476.576195	37.498586
1817.578894	123664.515561	37.503604
1819.748431	123847.386847	37.508621
1821.933478	124022.162945	37.513639
1823.384340	124216.552415	37.518656
1825.401069	124402.634209	37.523674
1826.653267	124576.631837	37.528692
1829.182005	124768.534673	37.533709
1830.836329	124954.472451	37.538727
1832.596189	125145.596031	37.543744
1834.705904	125333.215385	37.548762
1835.975907	125515.320859	37.553780
1838.575052	125707.788093	37.558797
1840.844911	125882.990416	37.563815
1842.501175	126069.567340	37.568832
1844.418612	126240.550684	37.573850
1846.083940	126428.485307	37.578868
1847.907419	126603.582588	37.583885
1849.635835	126800.935338	37.588903
1851.356120	126991.705831	37.593920
1853.481754	127178.544617	37.598938
1855.226886	127364.149401	37.603956
1856.946901	127550.380593	37.608973
1858.751198	127733.402364	37.613991
1860.216900	127929.761064	37.619008
1862.681183	128124.975677	37.624026
1864.234071	128314.509605	37.629044
1866.128268	128498.738731	37.634061
1867.654727	128702.767438	37.639079
1869.724366	128892.743747	37.644096
1871.290003	129085.818978	37.649114
1873.063590	129285.637878	37.654132
1874.882636	129481.339868	37.659149
1877.051049	129679.843115	37.664167
1878.975055	129874.642456	37.669184
1880.898750	130067.945584	37.674202
1883.142422	130266.731688	37.679220
1885.050486	130455.116131	37.684237
1887.150240	130630.999323	37.689255
1889.020110	130807.350410	37.694272
1890.943392	130960.233719	37.699290
1892.609547	131139.130111	37.704308
1894.331479	131308.388265	37.709325
1896.389218	131473.090514	37.714343
1897.534571	131653.630749	37.719360
1899.597198	131827.621387	37.724378
1901.259627	132016.710705	37.729396
1902.763347	132193.390912	37.734413
1904.528050	132389.977473	37.739431
1906.553148	132597.296949	37.744448
1908.140999	132783.254454	37.749466
1909.821069	132984.703904	37.754484
1911.588722	133189.338200	37.759501
1913.621666	133395.797407	37.764519
1915.314412	133607.830163	37.769536
1917.239170	133816.579478	37.774554
1919.445239	134031.402062	37.779572
1921.206133	134248.870840	37.784589
1923.636414	134459.244832	37.789607
1925.129636	134674.980885	37.794624
1927.242217	134882.652784	37.799642
1929.054051	135105.041212	37.804660
1931.348440	135321.835794	37.809677
1933.716572	135533.696475	37.814695
1935.950161	135749.995010	37.819712
1937.957017	135960.353124	37.824730
1940.015366	136168.382017	37.829748
1941.986414	136366.667153	37.834765
1944.002370	136578.815953	37.839783
1945.422881	136790.449305	37.844800
1947.717468	137006.376332	37.849818
1949.873370	137222.046784	37.854836
1951.594260	137439.765576	37.859853
1953.580095	137649.309906	37.864871
1955.672287	137864.269958	37.869888
1957.447528	138071.425188	37.874906
1959.568011	138280.418440	37.879924
1961.724452	138500.028716	37.884941
1964.024351	138720.404496	37.889959
1965.570395	138950.340226	37.894976
1967.771614	139157.408608	37.899994
1970.070344	139375.084606	37.905012
1971.427866	139600.801572	37.910029
1973.353449	139807.306570	37.915047
1974.726123	140029.977500	37.920064
1976.932585	140253.116170	37.925082
1978.982479	140490.125823	37.930100
1980.750545	140720.708220	37.935117
1982.827855	140938.387783	37.940135
1984.974793	141175.804531	37.945152
1987.064712	141392.113573	37.950170
1989.132983	141617.640631	37.955188
1991.074894	141845.840842	37.960205
1993.593064	142077.011005	37.965223
1995.286945	142299.007912	37.970240
1997.471496	142515.903731	37.975258
1999.467810	142736.548363	37.980276
2001.571179	142963.421477	37.985293
2003.372757	143176.648567	37.990311
2005.437004	143406.258469	37.995328
2007.393192	143618.765376	38.000346
2009.489205	143852.750988	38.005364
2011.276962	144078.650329	38.010381
2013.328961	144295.777676	38.015399
2015.861740	144509.543978	38.020416
2017.567210	144735.116420	38.025434
2019.644040	144940.731226	38.030452
2021.501098	145154.364295	38.035469
2023.364153	145345.672156	38.040487
2025.792755	145549.026294	38.045504
2027.926662	145737.437779	38.050522
2030.298090	145928.668723	38.055540
2031.689777	146132.732337	38.060557
2033.591706	146335.486211	38.065575
2035.365009	146542.792046	38.070592
2037.688018	146751.117398	38.075610
2039.526689	146956.079341	38.080628
2041.202197	147170.713731	38.085645
2042.959144	147378.901252	38.090663
2044.694859	147608.847903	38.095680
2046.546706	147826.478383	38.100698
2048.716154	148054.442918	38.105716
2050.636536	148296.675720	38.110733
2053.075944	148527.494233	38.115751
2054.752775	148782.066452	38.120768
2057.013582	149015.885017	38.125786
2058.912189	149253.010373	38.130804
2060.501873	149499.641138	38.135821
2062.844973	149734.935138	38.140839
2065.108510	149985.525046	38.145856
2067.139061	150233.309116	38.150874
2069.609841	150476.989371	38.155892
2071.364828	150727.217614	38.160909
2073.647392	150982.734184	38.165927
2075.750739	151224.685225	38.170944
2077.966671	151464.055741	38.175962
2080.157595	151713.738320	38.180980
2081.844975	151976.650930	38.185997
2084.399191	152219.348578	38.191015
2086.525695	152474.426723	38.196032
2088.786555	152720.129848	38.201050
2090.859994	152968.211577	38.206068
2092.970960	153225.123484	38.211085
2094.805527	153480.416683	38.216103
2096.884202	153734.581368	38.221120
2099.153109	153992.094201	38.226138
2101.143132	154245.170597	38.231156
2102.933038	154502.214445	38.236173
2105.683923	154766.599465	38.241191
2107.565416	155027.693562	38.246208
2109.725513	155283.528125	38.251226
2111.895799	155541.075975	38.256244
2113.670356	155812.599642	38.261261
2115.877637	156062.806674	38.266279
2117.745142	156330.471863	38.271296
2120.092468	156599.345753	38.276314
2122.525178	156866.074883	38.281332
2124.538064	157127.945009	38.286349
2126.742776	157390.890882	38.291367
2128.893363	157668.775449	38.296384
2130.928122	157924.209400	38.301402
2133.362877	158185.828094	38.306420
2135.151976	158451.153784	38.311437
2137.629746	158703.792675	38.316455
2139.654954	158970.302618	38.321472
2141.739108	159235.243050	38.326490
2144.132626	159499.209733	38.331508
2146.167799	159771.434458	38.336525
2148.272917	160033.061606	38.341543
2150.763904	160300.672803	38.346560
2152.256234	160568.504050	38.351578
2154.455425	160823.683306	38.356596
2156.760468	161089.841456	38.361613
2158.710273	161369.665683	38.366631
2161.030570	161621.414215	38.371648
2163.182950	161874.878405	38.376666
2165.297829	162111.743419	38.381684
2166.839919	162366.751856	38.386701
2169.473506	162597.367789	38.391719
2171.302045	162848.055060	38.396736
2173.279728	163098.364606	38.401754
2175.650228	163352.524343	38.406772
2177.356125	163617.313511	38.411789
2179.387726	163874.486196	38.416807
2181.720510	164135.485333	38.421824
2183.442465	164398.967447	38.426842
2185.606767	164674.493969	38.431860
2187.732166	164952.643119	38.436877
2190.021235	165217.398713	38.441895
2192.222165	165497.214283	38.446912
2193.910308	165792.194189	38.451930
2196.138245	166064.783627	38.456948
2198.141260	166366.992113	38.461965
2200.425282	166654.633284	38.466983
2202.909626	166949.430788	38.472000
2205.271033	167251.485806	38.477018
2207.785709	167544.554366	38.482036
2210.027933	167837.323742	38.487053
2212.188802	168131.135446	38.492071
2214.906046	168410.590444	38.497088
2217.374721	168697.322501	38.502106
2219.784021	168992.597352	38.507124
2221.976089	169283.044246	38.512141
2223.924170	169563.778890	38.517159
2226.696641	169848.576390	38.522176
2228.792575	170149.389918	38.527194
2231.375176	170435.235036	38.532212
2233.814841	170706.463495	38.537229
2235.957532	170986.576537	38.542247
2238.584866	171273.535305	38.547264
2240.393855	171555.581638	38.552282
2242.729856	171835.858242	38.557300
2245.203972	172136.214637	38.562317
2247.773902	172419.732970	38.567335
2249.808331	172701.304071	38.572352
2252.229619	172984.669864	38.577370
2254.305221	173270.490372	38.582388
2256.823736	173555.011318	38.587405
2259.315712	173844.667362	38.592423
2261.291481	174120.970444	38.597440
2263.402338	174419.525652	38.602458
2265.653439	174698.454470	38.607476
2267.784948	174990.837389	38.612493
2269.971593	175280.698576	38.617511
2271.994956	175573.202028	38.622528
2274.387726	175867.020448	38.627546
2276.710782	176158.450813	38.632564
2278.925339	176459.308508	38.637581
2280.819447	176754.439441	38.642599
2283.414758	177049.144838	38.647616
2285.560194	177355.603810	38.652634
2287.730341	177665.463235	38.657652
2289.856898	177965.654331	38.662669
2292.170701	178278.566670	38.667687
2294.440706	178575.308980	38.672704
2296.617722	178883.749513	38.677722
2299.028278	179187.608675	38.682740
2301.147255	179493.698448	38.687757
2303.402058	179803.323800	38.692775
2305.802874	180106.501918	38.697792
2307.802652	180423.153457	38.702810
2310.184231	180738.959362	38.707828
2312.618335	181044.091095	38.712845
2314.685351	181337.597926	38.717863
2317.046262	181629.586874	38.722880
2318.954768	181928.276057	38.727898
2321.294265	182210.415707	38.732916
2323.744134	182502.037980	38.737933
2325.836805	182789.043453	38.742951
2328.416525	183089.765337	38.747968
2330.544708	183393.682456	38.752986
2332.865754	183691.373268	38.758004
2335.063279	184002.951886	38.763021
2337.462710	184309.267938	38.768039
2339.867335	184611.748917	38.773056
2341.847630	184930.882335	38.778074
2344.305110	185240.697284	38.783092
2346.465443	185559.423703	38.788109
2348.613394	185880.896159	38.793127
2350.860397	186231.055328	38.798144
2353.533223	186600.681488	38.803162
2356.009592	186925.814394	38.808180
2358.688143	187250.815246	38.813197
2361.214706	187579.549085	38.818215
2363.428628	187899.671321	38.823232
2365.892735	188232.277627	38.828250
2367.975047	188555.216255	38.833268
2370.962796	188888.784465	38.838285
2373.351365	189212.540959	38.843303
2376.311699	189532.297812	38.848320
2378.332473	189864.292231	38.853338
2381.071981	190181.824685	38.858356
2383.751037	190511.280131	38.863373
2385.888297	190847.196308	38.868391
2388.331942	191170.238587	38.873408
2390.469550	191498.206264	38.878426
2392.682580	191833.351450	38.883444
2394.945084	192160.056884	38.888461
2397.006306	192499.850452	38.893479
2399.755412	192828.590206	38.898496
2401.808000	193186.624728	38.903514
2404.423083	193531.643701	38.908532
2406.770674	193873.707937	38.913549
2409.122895	194230.377940	38.918567
2411.586875	194573.518171	38.923584
2414.335067	194922.254124	38.928602
2416.548263	195260.659768	38.933620
2419.215322	195611.645464	38.938637
2421.305101	195963.255341	38.943655
2423.963713	196307.030174	38.948672
2426.583187	196664.223920	38.953690
2428.771901	197013.788957	38.958708
2431.333587	197353.364795	38.963725
2433.606367	197702.003982	38.968743
2436.361073	198049.603742	38.973760
2439.289868	198395.424512	38.978778
2441.980394	198747.735228	38.983796
2444.276341	199079.735871	38.988813
2447.217475	199421.035544	38.993831
2449.592737	199759.909239	38.998848
2451.912662	200090.028576	39.003866
2454.564128	200430.765883	39.008884
2457.074647	200771.195621	39.013901
2459.479412	201111.921952	39.018919
2462.604746	201435.110906	39.023936
2465.048827	201773.546275	39.028954
2467.646560	202100.019303	39.033972
2470.172400	202408.417635	39.038989
2472.438531	202753.106212	39.044007
2474.727731	203071.627307	39.049024
2477.174105	203380.674765	39.054042
2479.611023	203680.985736	39.059060
2481.936802	203983.676936	39.064077
2484.009052	204282.546878	39.069095
2486.097344	204588.349732	39.074112
2488.733541	204903.416012	39.079130
2490.527494	205221.230360	39.084148
2492.934526	205534.021663	39.089165
2494.870018	205855.498404	39.094183
2497.410718	206179.066115	39.099200
2499.875599	206528.760351	39.104218
2501.879769	206862.853224	39.109236
2504.631989	207213.062731	39.114253
2506.913103	207558.925981	39.119271
2509.254152	207906.228416	39.124288
2511.682962	208266.879774	39.129306
2514.007593	208627.217664	39.134324
2516.780267	208987.105326	39.139341
2519.309959	209347.996661	39.144359
2521.790675	209714.230835	39.149376
2524.246160	210079.021476	39.154394
2526.692021	210444.068162	39.159412
2529.184324	210828.897369	39.164429
2531.492670	211205.779071	39.169447
2534.233486	211577.056025	39.174464
2536.848704	211975.255312	39.179482
2538.968934	212356.079941	39.184500
2542.022326	212735.642071	39.189517
2544.590828	213131.335196	39.194535
2547.315060	213507.570799	39.199552
2550.258073	213895.052005	39.204570
2553.073500	214284.839837	39.209588
2555.796101	214656.783736	39.214605
2558.128195	215045.733078	39.219623
2560.927050	215429.046757	39.224640
2563.481150	215820.274075	39.229658
2565.974454	216201.476723	39.234676
2568.839185	216594.485502	39.239693
2571.118118	216992.183892	39.244711
2573.733724	217377.636370	39.249728
2576.810654	217757.149064	39.254746
2579.099813	218145.853834	39.259764
2582.113098	218528.933546	39.264781
2585.035839	218917.311633	39.269799
2587.966123	219285.492648	39.274816
2590.566783	219670.974481	39.279834
2592.845263	220051.044817	39.284852
2595.990780	220431.767952	39.289869
2598.146900	220820.139437	39.294887
2600.958164	221192.811077	39.299904
2603.461241	221567.588562	39.304922
2605.948226	221955.553402	39.309940
2608.351822	222343.988634	39.314957
2611.463504	222726.166017	39.319975
2613.733670	223104.308202	39.324992
2616.813644	223487.684719	39.330010
2618.946382	223872.174086	39.335028
2621.433721	224258.107182	39.340045
2624.468790	224641.414687	39.345063
2627.364734	225027.487529	39.350080
2629.884259	225410.799124	39.355098
2632.428464	225792.481031	39.360116
2634.788643	226173.962940	39.365133
2637.242618	226560.307827	39.370151
2639.831274	226946.885770	39.375168
2642.310046	227335.767140	39.380186
2644.488836	227743.138504	39.385204
2647.567778	228127.836288	39.390221
2650.074171	228516.281276	39.395239
2652.196357	228887.968462	39.400256
2655.156260	229255.308103	39.405274
2657.788293	229624.959616	39.410292
2660.690459	229984.000880	39.415309
2662.973595	230360.794152	39.420327
2665.390861	230729.411700	39.425344
2668.558058	231098.623693	39.430362
2670.856681	231478.437126	39.435380
2673.307500	231847.760232	39.440397
2675.569463	232232.532738	39.445415
2678.316887	232625.079285	39.450432
2681.254844	233020.644398	39.455450
2683.152889	233412.230227	39.460468
2686.046082	233806.455335	39.465485
2688.632232	234221.914757	39.470503
2691.313584	234626.486159	39.475520
2694.116195	235024.407935	39.480538
2696.159173	235445.412615	39.485556
2699.087627	235854.466319	39.490573
2701.864653	236288.184823	39.495591
2704.597604	236714.771257	39.500608
2707.620998	237130.134377	39.505626
2710.087165	237562.477177	39.510644
2712.899295	237978.329446	39.515661
2715.778644	238418.481991	39.520679
2718.691373	238847.451172	39.525696
2721.231888	239274.445407	39.530714
2723.780405	239713.250424	39.535732
2726.832442	240149.969554	39.540749
2729.594038	240595.421183	39.545767
2732.139752	241035.723401	39.550784
2735.097080	241481.778205	39.555802
2737.705952	241926.844937	39.560820
2740.539908	242370.097633	39.565837
2743.389398	242811.848326	39.570855
2746.183083	243257.773009	39.575872
2749.192349	243705.314496	39.580890
2751.665410	244157.917548	39.585908
2754.767981	244608.059236	39.590925
2757.584666	245048.210316	39.595943
2760.440430	245499.607886	39.600960
2763.257650	245941.459003	39.605978
2766.033109	246397.541216	39.610996
2769.634168	246835.457966	39.616013
2772.760342	247269.332398	39.621031
2775.440083	247715.062125	39.626048
2778.240622	248147.359442	39.631066
2781.229018	248586.485174	39.636084
2784.051084	249012.324844	39.641101
2786.877865	249453.099339	39.646119
2789.727835	249884.876688	39.651136
2792.589626	250313.043980	39.656154
2795.210668	250751.840341	39.661172
2798.212006	251175.157271	39.666189
2801.325049	251612.807852	39.671207
2804.341875	252040.031990	39.676224
2807.245114	252455.130526	39.681242
2809.576622	252900.062443	39.686260
2812.084758	253324.009120	39.691277
2815.272821	253760.397204	39.696295
2817.549681	254194.258616	39.701312
2820.217082	254617.363904	39.706330
2823.207975	255064.955381	39.711348
2825.949395	255497.191021	39.716365
2828.746160	255935.055774	39.721383
2831.375575	256375.459873	39.726400
2834.314628	256809.972079	39.731418
2836.461234	257238.484523	39.736436
2839.343402	257650.726083	39.741453
2841.880170	258071.986575	39.746471
2845.055278	258491.901688	39.751488
2847.902591	258909.046923	39.756506
2850.471048	259333.092305	39.761524
2853.120360	259752.526135	39.766541
2855.996418	260171.415207	39.771559
2858.613179	260600.579490	39.776576
2861.362333	261023.574741	39.781594
2863.875062	261464.004344	39.786612
2866.707716	261912.764483	39.791629
2869.493720	262355.129313	39.796647
2872.107779	262807.425089	39.801664
2874.849339	263259.013376	39.806682
2877.895679	263720.636018	39.811700
2880.611196	264185.432303	39.816717
2883.720702	264638.913306	39.821735
2886.185353	265114.488498	39.826752
2889.057141	265588.905990	39.831770
2892.099630	266071.701813	39.836788
2894.938353	266545.612018	39.841805
2897.875539	267029.207009	39.846823
2901.311634	267517.344560	39.851840
2904.341217	267989.897418	39.856858
2906.839441	268473.502785	39.861876
2909.612545	268961.939407	39.866893
2913.185607	269448.191766	39.871911
2916.023639	269944.943781	39.876928
2919.341468	270427.268643	39.881946
2922.202347	270906.284166	39.886964
2925.542842	271394.695837	39.891981
2929.038287	271877.950434	39.896999
2931.839842	272355.265803	39.902016
2934.531852	272839.986212	39.907034
2937.727659	273321.374687	39.912052
2940.681424	273807.852121	39.917069
2944.199258	274275.521553	39.922087
2947.282741	274756.208273	39.927104
2950.381633	275232.216865	39.932122
2952.906751	275717.073745	39.937140
2955.984636	276197.956111	39.942157
2959.239508	276684.319022	39.947175
2961.944556	277162.841023	39.952192
2964.895397	277647.239102	39.957210
2967.802323	278133.621890	39.962228
2970.925720	278616.844319	39.967245
2973.947978	279104.523636	39.972263
2976.896022	279607.042137	39.977280
2980.094160	280081.710931	39.982298
2982.453529	280586.346116	39.987316
2985.360651	281070.272227	39.992333
2989.035241	281551.612473	39.997351
2991.604658	282037.463955	40.002368
2994.930099	282523.677023	40.007386
2998.180865	283018.710116	40.012404
3001.073527	283507.726392	40.017421
3004.153568	283993.662897	40.022439
3006.895599	284481.984825	40.027456
3009.955238	284970.710977	40.032474
3013.017002	285465.705413	40.037492
3015.781680	285954.140356	40.042509
3019.399534	286441.575661	40.047527
3021.844396	286937.721844	40.052544
3024.894984	287425.060521	40.057562
3027.798356	287921.254971	40.062580
3030.448001	288407.480742	40.067597
3033.641438	288910.706891	40.072615
3036.579324	289396.321779	40.077632
3039.557428	289866.717319	40.082650
3042.322619	290340.138672	40.087668
3044.914830	290805.305943	40.092685
3047.901421	291271.144725	40.097703
3050.594040	291751.879262	40.102720
3053.803781	292230.117502	40.107738
3056.598985	292720.349910	40.112756
3059.084289	293213.876516	40.117773
3062.205431	293702.856942	40.122791
3065.169288	294206.888479	40.127808
3068.030454	294703.619604	40.132826
3071.392055	295217.431733	40.137844
3073.991491	295724.528358	40.142861
3077.577607	296240.276902	40.147879
3080.304332	296756.129196	40.152896
3083.912907	297282.781952	40.157914
3086.794317	297798.651557	40.162932
3089.777433	298311.834922	40.167949
3093.489003	298827.413609	40.172967
3096.311859	299365.136603	40.177984
3099.420092	299898.519563	40.183002
3102.918339	300431.125831	40.188020
3105.973723	300965.319012	40.193037
3109.144345	301493.243973	40.198055
3112.341210	302036.543612	40.203072
3115.542762	302569.708076	40.208090
3118.799535	303098.517670	40.213108
3121.771876	303644.678972	40.218125
3125.361348	304172.867504	40.223143
3128.519145	304711.449435	40.228160
3132.200353	305242.328957	40.233178
3135.515169	305773.767683	40.238196
3138.725993	306317.832872	40.243213
3142.078560	306834.811156	40.248231
3145.089958	307375.697626	40.253248
3148.268638	307912.262459	40.258266
3151.643989	308450.034646	40.263284
3154.501678	308991.942736	40.268301
3157.760182	309516.877845	40.273319
3161.177198	310061.149113	40.278336
3163.901708	310602.958463	40.283354
3167.160062	311135.465163	40.288372
3170.328528	311684.503052	40.293389
3173.541884	312227.283907	40.298407
3176.579794	312772.623873	40.303424
3179.797319	313313.361089	40.308442
3183.137060	313860.900221	40.313460
3186.435540	314406.789615	40.318477
3190.096250	314943.504958	40.323495
3193.172517	315486.522821	40.328512
3196.788869	316029.653177	40.333530
3200.080929	316566.254436	40.338548
3202.817360	317110.549194	40.343565
3206.104208	317642.138861	40.348583
3209.557011	318193.034029	40.353600
3212.978987	318737.049878	40.358618
3216.365500	319258.250633	40.363636
3219.425100	319797.208910	40.368653
3222.900964	320325.057012	40.373671
3226.452571	320861.463946	40.378688
3229.359224	321398.091405	40.383706
3232.851052	321916.097028	40.388724
3235.813852	322450.139548	40.393741
3239.115116	322981.838904	40.398759
3242.380032	323516.810467	40.403776
3245.323053	324042.030857	40.408794
3248.798941	324557.722631	40.413812
3251.671229	325085.528894	40.418829
3254.337112	325599.430642	40.423847
3257.536204	326099.668492	40.428864
3260.323203	326606.205937	40.433882
3263.985862	327107.044258	40.438900
3266.531912	327622.765770	40.443917
3269.731699	328131.579332	40.448935
3272.503395	328661.257382	40.453952
3275.414223	329190.069454	40.458970
3278.561339	329731.497536	40.463988
3281.664252	330268.409125	40.469005
3285.093779	330799.884091	40.474023
3288.576078	331354.607340	40.479040
3291.321964	331907.762845	40.484058
3295.434259	332451.209843	40.489076
3298.553607	333005.356847	40.494093
3302.119063	333560.314221	40.499111
3305.224916	334112.975771	40.504128
3308.630734	334673.573189	40.509146
3312.128860	335235.745945	40.514164
3315.426692	335813.440270	40.519181
3318.908090	336364.969965	40.524199
3322.072775	336931.810818	40.529216
3325.497130	337500.276596	40.534234
3329.465703	338069.993151	40.539252
3332.639646	338649.970194	40.544269
3335.591785	339218.862958	40.549287
3339.167492	339796.425494	40.554304
3342.909406	340377.376856	40.559322
3346.593448	340952.468899	40.564340
3349.563999	341537.148152	40.569357
3353.336817	342113.221928	40.574375
3356.639218	342695.370109	40.579392
3359.669433	343277.576266	40.584410
3363.324651	343851.813547	40.589428
3366.890885	344442.387138	40.594445
3370.580369	345024.030060	40.599463
3373.946869	345600.337120	40.604480
3377.199984	346182.611406	40.609498
3380.912130	346764.550636	40.614516
3384.204606	347355.319006	40.619533
3387.636974	347936.926410	40.624551
3391.525434	348515.435165	40.629568
3394.740869	349101.468087	40.634586
3398.391640	349675.480011	40.639604
3401.623767	350272.722325	40.644621
3404.835980	350855.098537	40.649639
3408.340906	351446.293005	40.654656
3411.250796	352039.394787	40.659674
3415.241064	352619.665858	40.664692
3418.204672	353214.284186	40.669709
3421.567245	353814.026731	40.674727
3425.458241	354403.610726	40.679744
3428.800291	355003.764929	40.684762
3432.342736	355595.611853	40.689780
3435.936493	356189.366293	40.694797
3439.045237	356767.543504	40.699815
3442.022918	357366.948481	40.704832
3445.698321	357963.951774	40.709850
3449.794567	358559.889362	40.714868
3453.065302	359153.865201	40.719885
3456.580997	359750.503603	40.724903
3459.867776	360346.557542	40.729920
3463.329211	360954.511086	40.734938
3467.033946	361543.252338	40.739956
3470.112972	362135.754577	40.744973
3473.674670	362740.209144	40.749991
3477.071717	363326.022933	40.755008
3480.323333	363906.896563	40.760013
3483.761731	364455.278981	40.765018
3487.098675	364975.488772	40.770023
3490.017148	365428.016157	40.775028
3493.238799	365839.633503	40.780032
3495.452705	366206.913247	40.785037
3497.755554	366526.358059	40.790042
3500.272440	366806.918727	40.795047
3502.358592	367050.322750	40.800052
3504.517969	367254.637962	40.805056
3506.171738	367407.480689	40.810061
3508.466710	367523.917127	40.815066
3509.889238	367607.054175	40.820071
3510.821769	367652.818420	40.825076
3512.225715	367671.934310	40.830080
3513.039430	367680.496822	40.835085
3514.288375	367642.294911	40.840090
3515.034011	367593.322776	40.845095
3515.613177	367523.035111	40.850100
3516.255149	367435.334084	40.855104
3516.502586	367331.332371	40.860109
3517.369508	367205.587417	40.865114
3517.514691	367075.736701	40.870119
3517.548196	366931.903579	40.875124
3518.130582	366776.652789	40.880128
3518.292931	366617.706266	40.885133
3518.328648	366444.143955	40.890138
3518.854224	366262.907536	40.895143
3518.565057	366080.323124	40.900148
3518.798527	365888.204526	40.905152
3518.449259	365699.300520	40.910157
3518.230633	365505.649040	40.915162
3519.004054	365306.887274	40.920167
3518.367413	365093.276334	40.925172
3518.448233	364881.864376	40.930176
3518.113931	364684.846091	40.935181
3518.103486	364476.214970	40.940186
3518.049698	364268.757934	40.945191
3518.094035	364064.866889	40.950196
3518.173350	363846.866668	40.955200
3517.448631	363642.762050	40.960205
3517.813318	363423.799542	40.965210
3517.193478	363208.012424	40.970215
3517.080998	363005.383558	40.975220
3516.853188	362807.421372	40.980224
3516.633160	362600.003890	40.985229
3516.710392	362395.765880	40.990234
3516.685075	362190.703864	40.995239
3516.167860	361988.690092	41.000244
3516.198409	361781.837790	41.005248
3515.765045	361587.507898	41.010253
3515.681458	361392.537846	41.015258
3515.663185	361189.094215	41.020263
3514.948963	361013.761552	41.025268
3514.902104	360816.012133	41.030272
3514.657180	360629.600729	41.035277
3514.568658	360447.992207	41.040282
3514.496788	360267.980999	41.045287
3514.030848	360077.737860	41.050292
3513.948551	359890.661272	41.055296
3513.474832	359733.428592	41.060301
3513.476696	359552.537616	41.065306
3513.273016	359385.731150	41.070311
3512.899760	359211.681891	41.075316
3512.610559	359053.629165	41.080320
3512.417298	358886.055934	41.085325
3512.441743	358729.807931	41.090330
3512.135270	358579.252545	41.095335
3511.846945	358426.431734	41.100340
3511.817074	358262.768862	41.105344
3511.881787	358121.963393	41.110349
3511.513096	357964.095315	41.115354
3511.590941	357816.221155	41.120359
3510.918339	357672.859825	41.125364
3511.405189	357530.638978	41.130368
3510.880552	357391.497606	41.135373
3510.870970	357248.336110	41.140378
3510.537763	357111.120653	41.145383
3510.222653	356969.123682	41.150388
3510.531984	356840.778667	41.155392
3510.174990	356719.729421	41.160397
3509.955718	356578.884868	41.165402
3510.323157	356453.858670	41.170407
3510.070455	356331.012575	41.175412
3509.907838	356198.138074	41.180416
3509.544785	356076.121460	41.185421
3509.429700	355943.289309	41.190426
3509.124336	355828.048876	41.195431
3509.313260	355711.917777	41.200436
3509.250749	355592.597478	41.205440
3509.278196	355471.356483	41.210445
3509.020461	355352.472316	41.215450
3508.977202	355252.235657	41.220455
3508.886338	355136.400134	41.225460
3508.950794	355017.922068	41.230464
3508.575542	354906.349168	41.235469
3508.988486	354792.391094	41.240474
3508.707634	354679.608097	41.245479
3508.519204	354567.827007	41.250484
3508.509139	354461.406257	41.255488
3508.173264	354356.586316	41.260493
3508.319416	354247.471701	41.265498
3508.658052	354133.802411	41.270503
3507.902407	354031.791826	41.275508
3508.124503	353920.859608	41.280512
3508.243045	353823.338365	41.285517
3507.907190	353716.737052	41.290522
3508.005194	353614.922722	41.295527
3507.601134	353518.218992	41.300532
3507.756890	353412.582304	41.305536
3507.672673	353325.334640	41.310541
3507.595400	353230.307630	41.315546
3507.658591	353130.937339	41.320551
3507.364133	353037.519497	41.325556
3507.505672	352942.864279	41.330560
3507.481389	352849.175077	41.335565
3507.318843	352755.430860	41.340570
3507.085826	352667.391156	41.345575
3506.983826	352572.086432	41.350580
3507.166401	352479.990773	41.355584
3506.987093	352398.830520	41.360589
3507.068731	352300.954509	41.365594
3506.964615	352202.903754	41.370599
3506.975222	352119.705126	41.375604
3506.937834	352030.413110	41.380608
3506.709354	351951.623380	41.385613
3506.843973	351858.592888	41.390618
3506.836934	351777.531360	41.395623
3506.843193	351683.834012	41.400628
3507.116008	351590.120332	41.405632
3506.934082	351519.431184	41.410637
3506.825018	351438.257584	41.415642
3507.022088	351352.943541	41.420647
3506.330733	351261.971777	41.425652
3506.469724	351173.285446	41.430656
3506.347751	351105.712729	41.435661
3506.473476	351012.147369	41.440666
3506.693491	350932.421082	41.445671
3505.979569	350855.178598	41.450676
3506.189887	350773.902796	41.455680
3506.124478	350692.669698	41.460685
3505.978974	350614.575577	41.465690
3505.888459	350539.929902	41.470695
3505.947704	350476.369539	41.475700
3506.272058	350389.507931	41.480704
3506.130222	350318.911617	41.485709
3506.045502	350237.909178	41.490714
3505.650024	350167.682477	41.495719
3505.963261	350093.455949	41.500724
3506.191762	350025.546826	41.505728
3505.757880	349944.877626	41.510733
3505.723629	349872.001140	41.515738
3505.854956	349793.404401	41.520743
3505.623912	349730.218237	41.525748
3505.758673	349658.713140	41.530752
3505.386692	349585.990259	41.535757
3505.526156	349507.696626	41.540762
3505.611885	349457.476353	41.545767
3505.289186	349394.380071	41.550772
3505.855713	349323.976442	41.555776
3505.765808	349258.581164	41.560781
3506.017613	349174.600262	41.565786
3505.693179	349094.903386	41.570791
3505.581411	349024.375876	41.575796
3505.647461	348953.312109	41.580800
3505.801321	348885.488516	41.585805
3505.781739	348810.319437	41.590810
3506.080249	348739.371568	41.595815
3505.715676	348678.009122	41.600820
3505.849721	348590.485988	41.605824
3505.838306	348513.815066	41.610829
3505.678060	348446.014030	41.615834
3506.101371	348374.995118	41.620839
3505.698707	348312.163434	41.625844
3506.080855	348238.837213	41.630848
3505.576444	348163.996338	41.635853
3505.714675	348093.402522	41.640858
3505.570134	348016.878282	41.645863
3505.865785	347943.793674	41.650868
3506.144958	347859.169621	41.655872
3505.956291	347794.117317	41.660877
3505.934096	347725.047621	41.665882
3505.571648	347656.818833	41.670887
3504.792301	347585.680315	41.675892
3505.234040	347512.699145	41.680896
3505.210280	347454.611798	41.685901
3505.406158	347390.871705	41.690906
3505.661671	347325.647677	41.695911
3505.079644	347250.740562	41.700916
3505.293428	347179.980521	41.705920
3505.175590	347119.847963	41.710925
3505.387344	347054.020062	41.715930
3505.481687	346996.167775	41.720935
3505.236087	346928.071859	41.725940
3505.682310	346864.444348	41.730944
3505.248812	346792.614744	41.735949
3505.008543	346731.305643	41.740954
3505.524155	346666.751718	41.745959
3505.023823	346595.974457	41.750964
3505.218053	346533.783830	41.755968
3505.167094	346470.766840	41.760973
3504.963980	346413.671702	41.765978
3505.204811	346350.761624	41.770983
3504.813620	346281.568413	41.775988
3504.796001	346213.816933	41.780992
3504.899931	346150.749819	41.785997
3505.087158	346097.330713	41.791002
3504.849567	346037.647066	41.796007
3504.733244	345974.486778	41.801012
3505.003809	345912.308554	41.806016
3505.094871	345854.912455	41.811021
3504.991709	345788.114127	41.816026
3505.398652	345737.609464	41.821031
3504.772992	345668.832849	41.826036
3505.071084	345612.675336	41.831040
3504.825336	345553.602289	41.836045
3504.278337	345493.279374	41.841050
3504.529752	345432.755836	41.846055
3504.675738	345390.274530	41.851060
3505.252776	345320.649020	41.856064
3505.053451	345258.593571	41.861069
3504.546109	345188.755167	41.866074
3504.587260	345140.442207	41.871079
3504.742794	345092.823269	41.876084
3505.286303	345025.693993	41.881088
3505.358493	344960.671908	41.886093
3505.038026	344893.117472	41.891098
3505.173793	344830.068381	41.896103
3504.770786	344766.187717	41.901108
3505.040651	344710.643310	41.906112
3504.577263	344655.848541	41.911117
3504.631355	344589.506468	41.916122
3504.584105	344523.434288	41.921127
3504.590111	344486.084083	41.926132
3504.456210	344414.457076	41.931136
3504.866922	344360.771647	41.936141
3504.545629	344302.725201	41.941146
3504.702212	344248.646913	41.946151
3504.605932	344207.345977	41.951156
3504.694325	344141.328230	41.956160
3504.334861	344083.719584	41.961165
3504.383518	344021.267348	41.966170
3504.424332	343966.647272	41.971175
3504.540928	343922.744893	41.976180
3504.373865	343860.732743	41.981184
3504.456296	343817.979698	41.986189
3504.569575	343758.898536	41.991194
3504.881720	343706.041047	41.996199
3504.511722	343648.560441	42.001204
3504.775463	343589.557279	42.006208
3504.536936	343531.750911	42.011213
3504.449686	343478.497560	42.016218
3504.458186	343416.965811	42.021223
3504.502711	343365.395316	42.026228
3504.513801	343309.151566	42.031232
3504.674159	343250.138487	42.036237
3504.207940	343198.392962	42.041242
3504.446832	343137.613072	42.046247
3504.572195	343097.115380	42.051252
3504.582902	343032.912861	42.056256
3504.246248	342979.417866	42.061261
3504.574590	342922.081646	42.066266
3504.443662	342876.792588	42.071271
3504.402767	342825.056599	42.076276
3504.377814	342763.249207	42.081280
3504.379926	342707.514409	42.086285
3504.134730	342658.683149	42.091290
3504.106743	342603.817368	42.096295
3503.869373	342562.892396	42.101300
3504.498661	342499.558843	42.106304
3504.399768	342464.358612	42.111309
3503.808813	342411.690541	42.116314
3503.846866	342347.762197	42.121319
3503.637127	342302.179536	42.126324
3503.987671	342262.383207	42.131328
3504.036193	342217.650184	42.136333
3504.031002	342178.265091	42.141338
3503.879280	342123.087261	42.146343
3504.039376	342065.470694	42.151348
3503.951147	342022.030045	42.156352
3503.702473	341983.648846	42.161357
3503.904829	341933.119603	42.166362
3504.013508	341891.962007	42.171367
3503.844287	341848.228622	42.176372
3504.118133	341793.441736	42.181376
3503.959443	341743.476945	42.186381
3503.843974	341703.040540	42.191386
3503.949991	341654.992322	42.196391
3503.815159	341611.405854	42.201396
3504.455191	341565.842564	42.206400
3504.684618	341517.012136	42.211405
3504.064076	341458.956651	42.216410
3503.861124	341410.269641	42.221415
3503.948256	341357.240192	42.226420
3504.264896	341313.710237	42.231424
3504.526616	341258.746414	42.236429
3504.454020	341207.597802	42.241434
3504.427807	341156.162194	42.246439
3504.239385	341100.225643	42.251444
3504.482199	341043.815056	42.256448
3504.050351	340995.747928	42.261453
3504.037084	340941.106107	42.266458
3504.577930	340887.140807	42.271463
3504.416956	340839.997570	42.276468
3504.096110	340780.190670	42.281472
3504.364398	340733.031348	42.286477
3504.221650	340686.953040	42.291482
3504.335392	340630.434740	42.296487
3504.134616	340588.738938	42.301492
3504.181477	340534.239700	42.306496
3504.181517	340485.265548	42.311501
3504.031821	340434.763517	42.316506
3504.034757	340373.888424	42.321511
3504.048662	340332.082629	42.326516
3503.761167	340289.331987	42.331520
3504.144852	340229.490809	42.336525
3503.869103	340185.059953	42.341530
3503.794501	340132.689545	42.346535
3503.944958	340099.584126	42.351540
3503.866595	340044.264491	42.356544
3503.378363	339994.679079	42.361549
3503.616489	339954.617935	42.366554
3504.137714	339914.588978	42.371559
3503.775850	339863.534298	42.376564
3503.494676	339819.485257	42.381568
3503.115186	339777.511171	42.386573
3503.586743	339740.846315	42.391578
3503.653144	339696.997321	42.396583
3503.761310	339661.228075	42.401588
3503.630920	339612.247591	42.406592
3503.861009	339570.814121	42.411597
3503.789133	339522.587269	42.416602
3503.757194	339475.625575	42.421607
3503.794783	339438.799082	42.426612
3503.988378	339385.724697	42.431616
3503.911803	339342.533238	42.436621
3503.770866	339296.325707	42.441626
3503.961116	339249.939435	42.446631
3503.872769	339213.717173	42.451636
3503.801788	339161.955075	42.456640
3503.595590	339115.401461	42.461645
3503.422512	339075.021888	42.466650
3503.778706	339019.556759	42.471655
3503.691201	338985.139600	42.476660
3503.748103	338940.223137	42.481664
3503.725942	338901.625353	42.486669
3503.585700	338867.114570	42.491674
3503.693192	338810.009495	42.496679
3503.434436	338771.728110	42.501684
3503.444730	338725.801463	42.506688
3503.934546	338689.259840	42.511693
3503.675115	338643.603925	42.516698
3503.976971	338591.248973	42.521703
3503.847534	338545.598135	42.526708
3503.797782	338506.343056	42.531712
3503.780157	338469.142722	42.536717
3503.550970	338420.582860	42.541722
3503.652707	338370.623673	42.546727
3503.731079	338337.731284	42.551732
3504.035767	338290.181640	42.556736
3503.946142	338238.192252	42.561741
3503.758007	338187.794757	42.566746
3503.889861	338143.908257	42.571751
3503.769787	338103.087044	42.576756
3503.859888	338047.610973	42.581760
3503.761849	338013.321676	42.586765
3504.074300	337968.567678	42.591770
3503.994496	337920.492496	42.596775
3503.588814	337871.577916	42.601780
3503.707693	337821.361006	42.606784
3503.825367	337788.385714	42.611789
3503.490703	337738.773295	42.616794
3503.482914	337686.261782	42.621799
3503.684833	337643.584416	42.626804
3503.398995	337597.524412	42.631808
3503.528138	337566.912131	42.636813
3503.685535	337530.395641	42.641818
3503.826924	337484.014710	42.646823
3503.482672	337444.855172	42.651828
3503.580460	337401.049368	42.656832
3503.431313	337363.410624	42.661837
3503.566112	337317.996857	42.666842
3503.969761	337274.931644	42.671847
3503.412827	337231.888708	42.676852
3503.581149	337188.351407	42.681856
3503.928469	337159.357807	42.686861
3503.825713	337114.438500	42.691866
3503.652156	337055.823147	42.696871
3503.073727	337023.489526	42.701876
3503.349756	336977.417597	42.706880
3503.717998	336941.478042	42.711885
3503.509498	336904.763561	42.716890
3503.912817	336851.017069	42.721895
3503.691727	336810.693309	42.726900
3503.821470	336762.304258	42.731904
3503.582196	336724.322853	42.736909
3503.451357	336683.221988	42.741914
3503.750896	336640.731708	42.746919
3503.958608	336602.172005	42.751924
3503.967393	336551.411007	42.756928
3503.585180	336507.907707	42.761933
3503.696677	336468.091294	42.766938
3503.380701	336422.110793	42.771943
3503.735140	336384.112940	42.776948
3503.584005	336340.853224	42.781952
3503.283184	336295.099084	42.786957
3503.403374	336262.325475	42.791962
3503.658928	336217.069572	42.796967
3503.254483	336177.027960	42.801972
3503.246815	336122.530566	42.806977
3502.976153	336094.980141	42.811981
3503.357887	336060.843236	42.816986
3503.589169	336022.253828	42.821991
3503.661546	335985.647309	42.826996
3503.671816	335951.110346	42.832001
3503.296430	335901.806952	42.837005
3503.248567	335870.991922	42.842010
3503.471706	335816.407298	42.847015
3503.195101	335788.526963	42.852020
3503.376354	335747.045883	42.857025
3503.228436	335713.932039	42.862029
3503.257280	335675.399203	42.867034
3503.310168	335633.276754	42.872039
3503.356930	335601.658401	42.877044
3503.482669	335558.659862	42.882049
3503.265622	335515.485731	42.887053
3503.344025	335472.062122	42.892058
3503.604174	335427.211444	42.897063
3503.607682	335389.623223	42.902068
3503.209857	335352.046552	42.907073
3503.892770	335310.563215	42.912077
3503.494828	335267.111765	42.917082
3503.744330	335233.961081	42.922087
3503.326715	335198.447303	42.927092
3503.313346	335145.755013	42.932097
3503.364921	335114.110065	42.937101
3503.218658	335072.450312	42.942106
3503.524794	335024.616471	42.947111
3503.435369	334990.551902	42.952116
3503.428473	334944.979244	42.957121
3503.465725	334909.699589	42.962125
3503.126756	334874.809062	42.967130
3503.571221	334823.392965	42.972135
3503.281230	334794.369528	42.977140
3503.106712	334752.510358	42.982145
3503.344264	334721.446506	42.987149
3503.397760	334683.341152	42.992154
3503.493861	334643.779500	42.997159
3503.124130	334610.215981	43.002164
3503.152184	334581.117454	43.007169
3503.419262	334527.643120	43.012173
3503.552611	334487.744889	43.017178
3503.612424	334444.857054	43.022183
3503.299172	334413.497175	43.027188
3503.423391	334380.517824	43.032193
3503.537868	334335.612208	43.037197
3503.598000	334292.088342	43.042202
3503.478076	334246.608719	43.047207
3503.443758	334214.874647	43.052212
3503.294047	334176.622373	43.057217
3503.460985	334133.234297	43.062221
3503.349567	334096.044146	43.067226
3503.373825	334058.832845	43.072231
3503.378263	334016.766979	43.077236
3503.439712	333983.695318	43.082241
3503.571046	333949.570017	43.087245
3503.403092	333903.309044	43.092250
3503.755084	333851.880576	43.097255
3503.396678	333820.094873	43.102260
3503.395090	333776.122227	43.107265
3503.080953	333736.063939	43.112269
3503.158510	333692.587533	43.117274
3503.340133	333656.470388	43.122279
3503.314799	333627.710057	43.127284
3502.940747	333588.830845	43.132289
3503.318150	333547.647432	43.137293
3502.536574	333523.786077	43.142298
3502.954949	333477.433342	43.147303
3503.272627	333448.390602	43.152308
3503.220367	333401.068260	43.157313
3503.387883	333372.226859	43.162317
3503.287255	333340.502370	43.167322
3503.564548	333301.496072	43.172327
3503.580497	333271.304798	43.177332
3503.590986	333224.989793	43.182337
3503.130146	333183.453198	43.187341
3502.940355	333154.692666	43.192346
3502.984472	333113.535213	43.197351
3503.243540	333079.567283	43.202356
3503.009687	333044.709566	43.207361
3503.374211	333001.365745	43.212365
3503.547691	332963.214550	43.217370
3503.340852	332926.673928	43.222375
3503.201719	332895.183958	43.227380
3502.846361	332852.943887	43.232385
3503.318311	332807.624764	43.237389
3502.946220	332770.931674	43.242394
3503.042507	332735.361032	43.247399
3502.701482	332713.312681	43.252404
3502.775197	332671.412575	43.257409
3503.210459	332642.757857	43.262413
3503.087413	332613.121793	43.267418
3502.910676	332576.576150	43.272423
3502.881354	332554.046832	43.277428
3503.116718	332516.012727	43.282433
3503.223155	332474.972053	43.287437
3502.961277	332448.180590	43.292442
3502.994901	332410.559277	43.297447
3502.752982	332379.618981	43.302452
3502.900894	332345.489660	43.307457
3503.551002	332308.535323	43.312461
3503.003042	332278.965121	43.317466
3502.851719	332232.597789	43.322471
3502.807037	332195.420823	43.327476
3502.990392	332161.947100	43.332481
3503.048207	332128.289413	43.337485
3502.769841	332110.046031	43.342490
3502.797376	332076.749084	43.347495
3502.923362	332042.851809	43.352500
3502.783738	332004.494041	43.357505
3503.159594	331973.380982	43.362509
3502.788580	331947.623506	43.367514
3503.015732	331909.437474	43.372519
3503.202961	331878.684332	43.377524
3502.897858	331855.459933	43.382529
3502.936089	331803.390809	43.387533
3502.671726	331783.313843	43.392538
3503.017148	331746.762456	43.397543
3502.732411	331712.470991	43.402548
3503.101318	331679.552957	43.407553
3502.870690	331651.331764	43.412557
3502.743892	331611.750771	43.417562
3503.012217	331581.951270	43.422567
3502.901555	331555.466295	43.427572
3503.085631	331519.677391	43.432577
3503.118254	331476.205453	43.437581
3503.065934	331452.559962	43.442586
3503.200434	331405.994548	43.447591
3502.877784	331383.840835	43.452596
3502.834188	331342.745995	43.457601
3503.305486	331312.685792	43.462605
3502.803328	331281.378159	43.467610
3502.876095	331257.077223	43.472615
3503.068550	331227.212952	43.477620
3502.908124	331185.093315	43.482625
3503.078071	331157.496155	43.487629
3502.971748	331117.097567	43.492634
3502.894272	331077.457482	43.497639
3502.660451	331052.135879	43.502644
3502.711547	331022.318881	43.507649
3503.002446	330993.609098	43.512653
3503.174361	330961.204363	43.517658
3502.771560	330928.354909	43.522663
3502.766704	330893.535905	43.527668
3502.749063	330863.347962	43.532673
3503.399069	330830.080248	43.537677
3502.785623	330803.240608	43.542682
3502.526675	330762.738227	43.547687
3502.633088	330739.194772	43.552692
3502.504171	330704.725556	43.557697
3502.909721	330674.420743	43.562701
3502.739358	330642.577700	43.567706
3502.962440	330603.806012	43.572711
3502.898247	330582.094881	43.577716
3502.505364	330554.712050	43.582721
3502.957035	330514.175133	43.587725
3502.357749	330497.405278	43.592730
3502.846719	330459.914684	43.597735
3502.716623	330437.399811	43.602740
3502.705223	330402.581386	43.607745
3503.014922	330368.552317	43.612749
3502.758670	330342.725042	43.617754
3502.935911	330313.625484	43.622759
3503.066220	330273.697896	43.627764
3502.549834	330256.889601	43.632769
3502.876075	330208.970294	43.637773
3502.769000	330184.035362	43.642778
3502.646368	330160.552634	43.647783
3502.669010	330123.083414	43.652788
3502.757161	330095.930626	43.657793
3502.795620	330063.469607	43.662797
3502.977043	330031.240665	43.667802
3502.657963	329994.969081	43.672807
3502.604828	329978.190319	43.677812
3502.812013	329957.250537	43.682817
3502.890188	329908.174008	43.687821
3502.671444	329885.850658	43.692826
3502.921263	329858.163842	43.697831
3502.944237	329817.413126	43.702836
3502.916723	329788.650265	43.707841
3502.773549	329756.522479	43.712845
3502.768089	329735.997199	43.717850
3502.470701	329698.221277	43.722855
3502.685181	329667.055178	43.727860
3502.265651	329645.856659	43.732865
3502.594448	329610.272398	43.737869
3502.634637	329591.800209	43.742874
3502.535217	329565.515612	43.747879
3502.932839	329538.848426	43.752884
3503.251869	329514.075679	43.757889
3503.176646	329469.931525	43.762893
3502.795050	329435.678558	43.767898
3502.702330	329392.503591	43.772903
3503.070789	329371.818191	43.777908
3502.836139	329338.559697	43.782913
3502.821960	329304.936203	43.787917
3503.050561	329275.191992	43.792922
3502.961645	329247.964429	43.797927
3502.966608	329219.679375	43.802932
3502.999622	329185.895821	43.807937
3502.929822	329146.608682	43.812941
3503.084280	329118.580086	43.817946
3502.932310	329076.126193	43.822951
3502.668274	329051.036915	43.827956
3502.759417	329021.390211	43.832961
3503.034796	328987.950310	43.837965
3503.125817	328956.802861	43.842970
3503.287881	328922.286796	43.847975
3503.054217	328888.798845	43.852980
3502.683807	328865.328464	43.857985
3502.937271	328814.646268	43.862989
3502.865012	328790.747908	43.867994
3502.921622	328748.159461	43.872999
3502.638672	328719.893416	43.878004
3503.084477	328693.701446	43.883009
3502.850920	328652.150055	43.888013
3502.682263	328634.345819	43.893018
3502.739319	328596.971534	43.898023
3502.915719	328580.894106	43.903028
3502.985249	328549.978606	43.908033
3502.836232	328507.727133	43.913037
3502.800095	328487.485774	43.918042
3502.586530	328452.188359	43.923047
3502.872918	328424.647465	43.928052
3502.253890	328399.384089	43.933057
3502.746024	328366.901947	43.938061
3502.363388	328343.458596	43.943066
3502.505433	328302.738659	43.948071
3502.497942	328281.042869	43.953076
3502.344168	328257.029691	43.958081
3503.036849	328227.390531	43.963085
3502.831633	328199.824236	43.968090
3502.859851	328160.800667	43.973095
3502.333359	328126.696294	43.978100
3502.452107	328115.994728	43.983105
3502.507819	328073.456570	43.988109
3502.563038	328058.949410	43.993114
3503.171921	328029.399453	43.998119
3502.663487	327999.311122	44.003124
3502.359262	327967.359562	44.008129
3502.648123	327947.957633	44.013133
3502.512954	327926.866558	44.018138
3502.725620	327888.856917	44.023143
3502.706393	327874.056036	44.028148
3502.400154	327836.534079	44.033153
3502.697174	327805.175615	44.038157
3502.547066	327786.045409	44.043162
3502.982192	327744.567071	44.048167
3502.401425	327716.066853	44.053172
3502.633400	327686.549858	44.058177
3502.512883	327647.498058	44.063181
3502.971173	327636.463723	44.068186
3502.753454	327601.624061	44.073191
3502.859207	327568.056743	44.078196
3502.563888	327547.956987	44.083201
3502.515833	327519.271984	44.088205
3502.470293	327493.410055	44.093210
3502.533684	327458.195845	44.098215
3502.528777	327434.820364	44.103220
3502.490957	327410.966690	44.108225
3502.561765	327381.856103	44.113229
3502.930972	327353.563914	44.118234
3502.439908	327325.380138	44.123239
3502.717634	327306.437496	44.128244
3502.435505	327274.787187	44.133249
3502.384738	327233.205872	44.138253
3502.178445	327211.286069	44.143258
3502.653380	327192.261810	44.148263
3502.566275	327171.010236	44.153268
3502.697338	327147.893236	44.158273
3502.776934	327103.824111	44.163277
3502.781522	327083.270459	44.168282
3502.377439	327043.397337	44.173287
3502.657055	327028.524203	44.178292
3502.116957	326995.463903	44.183297
3502.547915	326969.298553	44.188301
3502.478580	326950.893056	44.193306
3502.679770	326917.513841	44.198311
3502.709611	326894.437884	44.203316
3502.874006	326864.854491	44.208321
3502.732075	326840.711434	44.213325
3502.674137	326816.962287	44.218330
3502.652386	326785.398261	44.223335
3502.506394	326751.055444	44.228340
3502.527776	326721.341577	44.233345
3502.759811	326699.556783	44.238349
3502.599511	326667.658103	44.243354
3502.437283	326637.870997	44.248359
3502.927826	326608.567349	44.253364
3502.847946	326581.590934	44.258369
3502.980888	326553.843698	44.263373
3502.800248	326524.237435	44.268378
3502.638200	326482.748976	44.273383
3502.639643	326458.888629	44.278388
3502.380289	326427.056047	44.283393
3502.608115	326402.346440	44.288397
3502.569796	326378.619420	44.293402
3502.448569	326353.200974	44.298407
3502.352320	326324.064745	44.303412
3502.491010	326302.268826	44.308417
3502.765728	326276.254530	44.313421
3502.409498	326252.347969	44.318426
3502.596129	326228.891108	44.323431
3502.477996	326200.775700	44.328436
3502.294564	326175.010696	44.333441
3502.616486	326146.190831	44.338445
3502.494876	326124.155508	44.343450
3502.284755	326086.337147	44.348455
3502.578467	326061.591642	44.353460
3502.452805	326037.191196	44.358465
3502.478351	326006.127957	44.363469
3502.444550	325982.959634	44.368474
3502.842548	325963.387141	44.373479
3502.483971	325933.706385	44.378484
3502.602490	325899.906755	44.383489
3502.818969	325876.953802	44.388493
3502.747319	325848.347599	44.393498
3502.434428	325814.538717	44.398503
3502.364606	325790.129434	44.403508
3502.097632	325778.775011	44.408513
3502.587999	325744.586696	44.413517
3502.521857	325728.520433	44.418522
3502.551067	325696.235368	44.423527
3502.412982	325673.998862	44.428532
3502.377930	325655.078683	44.433537
3502.598440	325617.956014	44.438541
3502.238506	325600.587206	44.443546
3502.560295	325565.051321	44.448551
3502.795005	325538.788400	44.453556
3502.515025	325516.802831	44.458561
3502.602928	325488.400489	44.463565
3502.263917	325470.188914	44.468570
3502.478835	325433.779213	44.473575
3502.726879	325420.105995	44.478580
3502.339716	325387.402155	44.483585
3502.820684	325354.563197	44.488589
3502.477379	325334.469807	44.493594
3502.392646	325306.730157	44.498599
3502.669134	325271.938775	44.503604
3502.173089	325251.105966	44.508609
3502.601037	325220.488275	44.513613
3502.481921	325193.466169	44.518618
3502.768321	325163.277474	44.523623
3502.849763	325145.178394	44.528628
3502.772642	325124.025947	44.533633
3502.692365	325088.246957	44.538637
3502.534234	325050.266916	44.543642
3502.489932	325031.525956	44.548647
3502.699520	325008.395521	44.553652
3502.384105	324975.273173	44.558657
3502.556928	324945.407253	44.563661
3502.351009	324923.613348	44.568666
3502.780606	324897.548635	44.573671
3502.829055	324863.428354	44.578676
3502.556582	324838.643023	44.583681
3502.926742	324808.441034	44.588685
3502.785541	324783.711558	44.593690
3502.850495	324750.606155	44.598695
3502.761860	324710.605343	44.603700
3502.589424	324684.659618	44.608705
3502.638276	324657.585583	44.613709
3502.642540	324624.591277	44.618714
3502.368624	324607.056030	44.623719
3502.539251	324573.730532	44.628724
3502.393112	324558.006962	44.633729
3502.715296	324521.681517	44.638733
3502.585263	324498.171187	44.643738
3502.623496	324466.163577	44.648743
3502.540922	324448.064275	44.653748
3502.555202	324425.574434	44.658753
3502.335493	324389.485831	44.663757
3502.392424	324364.572639	44.668762
3502.439696	324337.167936	44.673767
3502.437590	324314.299003	44.678772
3502.139404	324292.086663	44.683777
3502.371005	324271.165564	44.688781
3502.499562	324244.333244	44.693786
3502.215891	324214.029054	44.698791
3502.312768	324186.870921	44.703796
3502.242124	324164.979248	44.708801
3502.396523	324144.044660	44.713805
3502.496738	324123.296566	44.718810
3502.352829	324095.260042	44.723815
3502.747423	324063.298421	44.728820
3502.515150	324053.210068	44.733825
3502.750713	324013.895861	44.738829
3502.759706	323994.128579	44.743834
3502.876988	323968.035564	44.748839
3502.753309	323938.800154	44.753844
3502.655834	323907.754473	44.758849
3502.792293	323877.333782	44.763853
3502.664556	323847.488401	44.768858
3502.601690	323814.402140	44.773863
3502.699900	323789.812888	44.778868
3502.531832	323762.110606	44.783873
3502.469683	323734.569898	44.788877
3502.405778	323704.434651	44.793882
3502.487440	323680.661963	44.798887
3502.478266	323655.351606	44.803892
3502.179423	323635.326786	44.808897
3502.687911	323602.405838	44.813901
3502.066452	323585.509342	44.818906
3502.187093	323558.805008	44.823911
3502.434946	323536.787123	44.828916
3502.463070	323517.143833	44.833921
3502.561449	323486.983176	44.838925
3502.483332	323460.843933	44.843930
3502.333070	323441.152048	44.848935
3502.540335	323418.300920	44.853940
3502.103647	323391.301615	44.858945
3502.581900	323363.015145	44.863949
3502.509163	323334.839837	44.868954
3502.445355	323306.256089	44.873959
3502.411330	323284.409133	44.878964
3502.520254	323262.819754	44.883969
3502.561864	323228.419359	44.888973
3502.259485	323206.741319	44.893978
3502.241069	323183.340074	44.898983
3502.203895	323151.215988	44.903988
3502.147751	323132.603211	44.908993
3502.301558	323108.488257	44.913997
3502.660876	323090.370479	44.919002
3502.607016	323077.659293	44.924007
3502.325959	323040.383407	44.929012
3502.199184	323025.190474	44.934017
3502.443124	322979.590416	44.939021
3502.680826	322963.043323	44.944026
3502.220802	322942.585339	44.949031
3502.338914	322909.597397	44.954036
3502.197630	322900.741147	44.959041
3502.409582	322866.771861	44.964045
3502.311024	322849.234024	44.969050
3502.151241	322823.285169	44.974055
3502.514128	322799.773495	44.979060
3502.235149	322780.152209	44.984065
3502.259343	322759.644224	44.989069
3502.595892	322725.121201	44.994074
3502.413779	322701.083727	44.999079
3502.529518	322677.203407	45.004084
3502.501836	322644.416023	45.009089
3502.581374	322624.891513	45.014093
3502.477059	322602.291945	45.019098
3502.327275	322571.177093	45.024103
3502.422561	322541.092556	45.029108
3502.414759	322518.274406	45.034113
3502.268490	322487.108064	45.039117
3502.557992	322459.435477	45.044122
3502.562465	322441.728797	45.049127
3502.786300	322402.313144	45.054132
3502.619373	322382.801435	45.059137
3502.606440	322369.371347	45.064141
3502.731169	322341.469924	45.069146
3502.110780	322310.224591	45.074151
3502.428314	322293.664813	45.079156
3502.194297	322262.639161	45.084161
3502.283916	322239.525859	45.089165
3502.332149	322214.561861	45.094170
3501.915543	322193.638834	45.099175
3502.433471	322166.261230	45.104180
3502.259182	322147.513761	45.109185
3502.518102	322118.192103	45.114189
3502.484870	322110.463678	45.119194
3502.405699	322077.709305	45.124199
3502.359233	322044.975258	45.129204
3502.300872	322023.818319	45.134209
3502.181732	321990.739377	45.139213
3502.409988	321982.614075	45.144218
3502.417406	321948.548678	45.149223
3502.717473	321931.151950	45.154228
3502.331225	321913.200567	45.159233
3502.232596	321881.848285	45.164237
3502.487874	321865.043625	45.169242
3502.349259	321832.527276	45.174247
3502.577840	321798.452783	45.179252
3502.239671	321781.180751	45.184257
3502.296649	321757.919625	45.189261
3502.332711	321722.399490	45.194266
3502.485479	321701.234976	45.199271
3502.424654	321685.878655	45.204276
3502.663996	321659.943298	45.209281
3502.368940	321634.091083	45.214285
3502.159962	321610.565977	45.219290
3502.369588	321593.463030	45.224295
3502.634864	321550.554796	45.229300
3502.469558	321540.887905	45.234305
3502.133370	321518.781769	45.239309
3502.305519	321490.261835	45.244314
3501.885737	321464.352605	45.249319
3502.217326	321449.342182	45.254324
3501.850557	321431.692851	45.259329
3502.235766	321401.918558	45.264333
3502.148499	321380.994762	45.269338
3502.055936	321363.684341	45.274343
3502.498527	321331.687739	45.279348
3502.477346	321315.561899	45.284353
3502.264933	321286.694622	45.289357
3502.063649	321259.123066	45.294362
3502.232639	321244.773891	45.299367
3502.485360	321218.251048	45.304372
3502.134181	321200.828160	45.309377
3502.385902	321183.286007	45.314381
3502.327975	321152.537430	45.319386
3502.500487	321125.034823	45.324391
3502.369312	321103.812435	45.329396
3502.279030	321082.812640	45.334401
3502.318386	321049.428454	45.339405
3502.339132	321038.435018	45.344410
3502.137647	321014.755772	45.349415
3502.437244	320989.573854	45.354420
3502.633539	320969.470718	45.359425
3502.484099	320943.773511	45.364429
3502.360445	320910.999722	45.369434
3502.109005	320900.862713	45.374439
3502.380749	320870.317040	45.379444
3502.111661	320852.728592	45.384449
3502.273245	320820.037551	45.389453
3502.277578	320802.610061	45.394458
3502.522811	320783.211568	45.399463
3502.407080	320745.933378	45.404468
3502.203526	320733.371987	45.409473
3501.969393	320707.815023	45.414477
3502.041121	320686.459090	45.419482
3501.786989	320667.748835	45.424487
3501.945136	320638.441842	45.429492
3502.196719	320630.770592	45.434497
3502.207496	320610.925126	45.439501
3502.404753	320594.128996	45.444506
3502.608948	320570.437259	45.449511
3502.701778	320541.776391	45.454516
3502.287662	320517.621138	45.459521
3502.172176	320480.724295	45.464525
3502.303684	320462.818938	45.469530
3501.990025	320436.663601	45.474535
3502.335838	320417.630908	45.479540
3502.106144	320398.026293	45.484545
3502.311209	320370.848873	45.489549
3502.510466	320353.543515	45.494554
3502.447182	320330.020475	45.499559
3502.830421	320307.674555	45.504564
3502.653547	320293.226236	45.509569
3502.531346	320246.204637	45.514573
3502.590026	320224.774182	45.519578
3502.311289	320201.182833	45.524583
3502.078136	320173.666422	45.529588
3502.389027	320158.175386	45.534593
3502.118070	320135.600442	45.539597
3502.237474	320116.602849	45.544602
3501.949836	320090.748548	45.549607
3502.055908	320065.265468	45.554612
3502.029615	320048.020528	45.559617
3501.830250	320030.573541	45.564621
3502.341021	320004.416857	45.569626
3502.202316	319998.256387	45.574631
3502.267048	319955.123354	45.579636
3502.396766	319950.396709	45.584641
3502.453438	319921.639290	45.589645
3502.370688	319897.788305	45.594650
3502.043748	319862.424884	45.599655
3502.311965	319838.061305	45.604660
3502.415084	319812.375004	45.609665
3502.052901	319792.536316	45.614669
3502.516787	319774.655277	45.619674
3502.052034	319751.448810	45.624679
3502.252951	319726.459602	45.629684
3502.468981	319707.014287	45.634689
3502.217964	319684.690420	45.639693
3502.257758	319663.517043	45.644698
3501.994576	319631.501800	45.649703
3502.192096	319613.305961	45.654708
3502.322732	319601.506368	45.659713
3502.200937	319577.228775	45.664717
3502.084205	319557.657084	45.669722
3501.828016	319537.827227	45.674727
3502.117848	319509.491203	45.679732
3502.338626	319496.252821	45.684737
3502.283172	319473.643997	45.689741
3501.900572	319458.871229	45.694746
3501.649256	319429.296393	45.699751
3502.119698	319408.768245	45.704756
3501.903319	319385.217631	45.709761
3501.857474	319365.202313	45.714765
3502.177975	319361.896095	45.719770
3501.858648	319339.226496	45.724775
3502.021483	319311.011872	45.729780
3502.192062	319299.587609	45.734785
3502.058094	319290.933006	45.739789
3502.143850	319261.585463	45.744794
3501.928497	319237.729309	45.749799
3502.239056	319216.793439	45.754804
3502.461568	319200.959631	45.759809
3502.753349	319184.428107	45.764813
3502.518751	319145.844060	45.769818
3502.118313	319067.291098	45.774823
3501.866266	318947.575219	45.779828
3501.451635	318798.829466	45.784833
3501.108877	318606.667667	45.789837
3500.707076	318360.729153	45.794842
3499.877903	318086.665498	45.799847
3499.345510	317753.832284	45.804852
3497.695269	317400.689005	45.809857
3497.051887	316994.108383	45.814861
3496.093100	316564.928559	45.819866
3495.010444	316095.613884	45.824871
3493.787646	315587.310637	45.829876
3491.902001	315054.296747	45.834881
3490.439283	314477.166360	45.839885
3488.844350	313873.128642	45.844890
3486.763645	313250.558192	45.849895
3485.060359	312587.640380	45.854900
3482.851602	311904.613248	45.859905
3480.957525	311193.307337	45.864909
3479.287475	310451.827073	45.869914
3476.731770	309689.123092	45.874919
3474.535127	308896.603119	45.879924
3472.289990	308110.414423	45.884929
3469.829401	307274.571610	45.889933
3468.055995	306414.686043	45.894938
3464.860343	305543.605926	45.899943
3462.889483	304645.241929	45.904948
3459.782705	303734.415834	45.909953
3456.867734	302806.415803	45.914957
3454.753504	301864.429551	45.919962
3451.477648	300905.682289	45.924967
3448.676052	299927.399027	45.929972
3445.654315	298939.460722	45.934977
3442.725299	297938.000482	45.939981
3440.302506	296924.531590	45.944986
3437.011833	295894.813089	45.949991
3433.829742	294848.641514	45.954996
3431.003262	293808.225180	45.960001
3427.901731	292747.673176	45.965005
3424.467923	291670.710146	45.970010
3420.854167	290600.604038	45.975015
3417.538333	289527.785907	45.980020
3414.511980	288442.074507	45.985025
3411.388192	287350.785029	45.990029
3407.805806	286237.680811	45.995034
3404.325553	285143.686814	46.000039
3401.033259	284027.930069	46.005044
3397.480421	282918.077098	46.010049
3394.203909	281801.544465	46.015053
3390.638242	280670.553162	46.020058
3387.134348	279553.054325	46.025063
3384.070462	278422.332981	46.030068
3380.253688	277290.923020	46.035073
3376.628077	276153.993003	46.040077
3373.219901	275013.906888	46.045082
3369.331538	273889.284234	46.050087
3365.652542	272741.901819	46.055092
3362.439640	271610.116632	46.060097
3358.799395	270464.862795	46.065101
3355.294263	269318.911527	46.070106
3351.593303	268181.201420	46.075111
3348.051004	267035.788582	46.080116
3344.370506	265893.210495	46.085121
3340.548466	264748.833633	46.090125
3336.982606	263601.323181	46.095130
3333.306150	262458.987105	46.100135
3329.677284	261319.254801	46.105140
3326.076281	260179.736036	46.110145
3322.297649	259034.784323	46.115149
3318.880670	257895.342669	46.120154
3315.177857	256752.471890	46.125159
3311.466258	255616.875922	46.130164
3307.776792	254473.779929	46.135169
3303.988109	253320.987372	46.140173
3300.316761	252182.072508	46.145178
3296.227639	251051.822133	46.150183
3292.681093	249919.849505	46.155188
3288.849852	248786.614759	46.160193
3285.131005	247664.051659	46.165197
3281.633471	246528.637093	46.170202
3278.146861	245402.892057	46.175207
3274.218855	244273.007390	46.180212
3270.205154	243154.361711	46.185217
3266.671841	242038.844941	46.190221
3262.964225	240920.930838	46.195226
3259.105330	239812.102402	46.200231
3255.416040	238693.590759	46.205236
3251.470438	237584.258274	46.210241
3247.676537	236477.521893	46.215245
3244.024275	235371.702595	46.220250
3239.926232	234283.752507	46.225255
3236.708319	233185.144327	46.230260
3232.824973	232095.908195	46.235265
3228.871801	230999.269608	46.240269
3225.516169	229909.947971	46.245274
3221.507203	228834.632887	46.250279
3217.821215	227742.508026	46.255284
3214.027818	226667.616384	46.260289
3210.472352	225585.683460	46.265293
3206.799182	224505.857358	46.270298
3203.250881	223443.000036	46.275303
3199.439837	222369.207081	46.280308
3195.455821	221295.722152	46.285313
3191.687037	220237.919341	46.290317
3188.289192	219161.340645	46.295322
3184.167704	218106.372165	46.300327
3180.491795	217050.572360	46.305332
3176.862947	215994.003538	46.310337
3172.977618	214948.887271	46.315341
3169.847747	213896.244956	46.320346
3165.741782	212842.458849	46.325351
3162.034950	211788.333983	46.330356
3158.655589	210745.648186	46.335361
3154.500923	209711.415151	46.340365
3150.874543	208662.332569	46.345370
3146.770933	207634.339990	46.350375
3143.264569	206598.083947	46.355380
3139.866425	205564.974102	46.360385
3135.533490	204538.993135	46.365389
3131.897201	203521.848326	46.370394
3128.060351	202508.051114	46.375399
3124.494761	201490.881325	46.380404
3121.107290	200473.740892	46.385409
3117.025370	199468.200505	46.390413
3113.507964	198454.378478	46.395418
3109.460049	197464.762721	46.400423
3106.197831	196459.777101	46.405428
3102.156477	195468.697188	46.410433
3098.068216	194475.849231	46.415437
3094.568821	193471.177435	46.420442
3090.814233	192495.609602	46.425447
3087.382132	191514.218680	46.430452
3083.701971	190537.228980	46.435457
3079.806443	189557.607196	46.440461
3075.965233	188584.428048	46.445466
3072.241025	187624.633658	46.450471
3068.442090	186650.803192	46.455476
3064.870318	185698.081634	46.460481
3060.921068	184735.344038	46.465485
3057.508952	183779.585575	46.470490
3053.463975	182830.198960	46.475495
3049.486770	181878.621446	46.480500
3045.636179	180939.459810	46.485505
3042.098801	180008.534440	46.490509
3038.259822	179061.267997	46.495514
3034.560666	178140.877934	46.500519
3031.056350	177218.252256	46.505524
3026.790595	176299.981787	46.510529
3023.296442	175378.227851	46.515533
3019.378696	174461.387880	46.520538
3015.412668	173562.961255	46.525543
3011.859362	172653.800128	46.530548
3007.985676	171759.861030	46.535553
3004.503615	170874.718799	46.540557
3000.758604	169970.011561	46.545562
2996.791909	169088.543215	46.550567
2993.011706	168204.077958	46.555572
2989.035054	167324.593236	46.560577
2985.151142	166460.800085	46.565581
2981.267780	165596.075748	46.570586
2977.507712	164748.565228	46.575591
2973.572859	163890.578838	46.580596
2969.921995	163039.012716	46.585601
2965.784753	162218.984923	46.590605
2962.207136	161379.584736	46.595610
2958.203289	160560.206635	46.600615
2953.973854	159730.221240	46.605620
2950.279169	158920.120617	46.610625
2946.066008	158119.720622	46.615629
2942.132067	157312.605995	46.620634
2937.976492	156528.763688	46.625639
2934.493414	155743.223566	46.630644
2930.750717	154978.619000	46.635649
2926.969481	154203.391167	46.640653
2923.505884	153436.727484	46.645658
2919.039687	152680.016705	46.650663
2915.544010	151924.755911	46.655668
2911.153423	151188.555354	46.660673
2907.218329	150455.704314	46.665677
2903.154185	149718.454788	46.670682
2898.951642	149024.223200	46.675687
2895.121139	148310.575040	46.680692
2891.111519	147627.440857	46.685697
2887.218810	146939.385629	46.690701
2883.207882	146244.422996	46.695706
2879.082683	145588.590012	46.700711
2875.269942	144928.072474	46.705716
2871.160978	144269.683727	46.710721
2867.750281	143629.784785	46.715725
2863.439443	142991.115700	46.720730
2859.441391	142357.508428	46.725735
2855.324171	141736.320641	46.730740
2851.875008	141133.065874	46.735745
2847.773119	140522.413540	46.740749
2844.094005	139928.065067	46.745754
2839.788734	139336.722297	46.750759
2836.503707	138757.900028	46.755764
2832.485904	138168.410193	46.760769
2828.843424	137606.591587	46.765773
2825.160310	137036.631158	46.770778
2821.211673	136477.952751	46.775783
2817.607080	135908.604811	46.780788
2813.967837	135359.140864	46.785793
2810.116709	134824.117499	46.790797
2806.545743	134187.068784	46.795802
2802.639982	133647.730002	46.800807
2799.273217	133108.504738	46.805812
2795.397460	132578.130070	46.810817
2791.985261	132047.448005	46.815821
2788.508998	131507.674372	46.820826
2784.597127	130991.724514	46.825831
2781.344136	130462.894331	46.830836
2777.626710	129939.065695	46.835841
2774.169757	129425.518961	46.840845
2770.933316	128896.107854	46.845850
2766.633918	128381.496551	46.850855
2763.243045	127855.264401	46.855860
2759.874748	127353.533040	46.860865
2756.008835	126841.569859	46.865869
2752.608982	126319.772232	46.870874
2749.116520	125822.530553	46.875879
2745.477714	125307.842071	46.880884
2742.223183	124798.213222	46.885889
2738.550740	124293.705091	46.890893
2735.048527	123782.588719	46.895898
2731.206270	123280.803355	46.900903
2728.123248	122767.561719	46.905908
2724.504004	122264.953283	46.910913
2720.761648	121768.869165	46.915917
2717.450123	121263.720288	46.920922
2713.843305	120770.552794	46.925927
2710.548550	120266.864047	46.930932
2706.940030	119755.638643	46.935937
2703.439821	119252.974351	46.940941
2700.008381	118751.056256	46.945946
2696.285204	118250.589004	46.950951
2692.713609	117742.513121	46.955956
2689.119722	117247.011146	46.960961
2685.372409	116745.715664	46.965965
2681.826890	116248.451866	46.970970
2678.004039	115760.380452	46.975975
2674.321284	115258.115894	46.980980
2671.018229	114773.269963	46.985985
2667.459413	114291.839767	46.990989
2663.846013	113804.168640	46.995994
2660.228941	113318.767870	47.000999
2656.436627	112831.290255	47.006004
2653.223474	112347.950317	47.011009
2649.311438	111892.582722	47.016013
2646.074479	111397.155300	47.021018
2642.004119	110936.459197	47.026023
2638.105272	110456.035993	47.031028
2634.429196	109989.722232	47.036033
2630.507059	109527.521267	47.041037
2626.834584	109066.457183	47.046042
2622.615234	108630.948726	47.051047
2618.975072	108180.252581	47.056052
2615.473825	107738.477803	47.061057
2612.026406	107301.213308	47.066061
2608.312983	106861.084622	47.071066
2604.559587	106438.510841	47.076071
2600.678550	106008.220455	47.081076
2597.066987	105580.181752	47.086081
2593.304491	105155.400768	47.091085
2589.757824	104745.476949	47.096090
2585.977720	104330.141213	47.101095
2582.443061	103920.784922	47.106100
2578.786416	103514.986362	47.111105
2575.261597	103109.655265	47.116109
2571.510363	102698.796982	47.121114
2567.780790	102300.333436	47.126119
2564.236262	101900.956177	47.131124
2560.924710	101509.847454	47.136129
2557.171690	101111.796026	47.141133
2553.575370	100718.275309	47.146138
2550.376180	100327.684407	47.151143
2547.062355	99932.044829	47.156148
2543.852182	99526.302481	47.161153
2540.048295	99142.085907	47.166157
2536.828671	98736.380427	47.171162
2532.939204	98344.751761	47.176167
2529.763967	97950.347856	47.181172
2526.272325	97555.972670	47.186177
2522.698063	97154.206058	47.191181
2519.333282	96757.253927	47.196186
2515.678928	96359.665613	47.201191
2511.994315	95960.231642	47.206196
2508.990638	95555.003578	47.211201
2505.242760	95163.430537	47.216205
2501.643942	94752.523429	47.221210
2498.618113	94362.411183	47.226215
2495.063258	93962.779367	47.231220
2491.793555	93558.914960	47.236225
2487.980785	93157.173516	47.241229
2484.656214	92754.789559	47.246234
2480.875161	92359.330897	47.251239
2477.372225	91950.250734	47.256244
2474.086433	91540.977112	47.261249
2470.744018	91147.854795	47.266253
2467.092705	90746.450475	47.271258
2463.612997	90337.413961	47.276263
2460.307654	89934.734184	47.281268
2456.812944	89525.571340	47.286273
2453.311719	89117.850842	47.291277
2449.858190	88702.950066	47.296282
2446.459042	88306.545198	47.301287
2442.554422	87888.524380	47.306292
2439.456731	87473.483870	47.311297
2435.723775	87065.599101	47.316301
2432.687729	86645.504326	47.321306
2428.958101	86234.264000	47.326311
2425.659290	85824.918860	47.331316
2422.047538	85411.613799	47.336321
2418.091624	85004.758131	47.341325
2414.923359	84584.586758	47.346330
2411.088084	84177.088849	47.351335
2407.947710	83766.007951	47.356340
2404.434549	83350.100371	47.361345
2400.584682	82935.762887	47.366349
2397.885721	82518.051305	47.371354
2394.037346	82104.462483	47.376359
2390.434877	81688.961536	47.381364
2387.579849	81263.544494	47.386369
2383.674478	80849.843259	47.391373
2380.378395	80420.989256	47.396378
2376.730841	80009.419611	47.401383
2373.310549	79592.397278	47.406388
2369.665645	79167.554252	47.411393
2365.847519	78743.608365	47.416397
2362.910521	78318.058600	47.421402
2358.908358	77900.733247	47.426407
2355.439425	77486.646022	47.431412
2352.108522	77059.018059	47.436417
2348.637625	76646.937780	47.441421
2345.448132	76209.954072	47.446426
2341.775177	75799.340465	47.451431
2338.164742	75364.874201	47.456436
2334.941108	74936.678861	47.461441
2330.943781	74519.950804	47.466445
2327.717917	74097.763046	47.471450
2324.108020	73674.460769	47.476455
2320.738229	73241.147044	47.481460
2317.208082	72818.620563	47.486465
2313.246949	72408.294315	47.491469
2309.840113	71979.209973	47.496474
2306.630501	71552.552526	47.501479
2303.192053	71130.127697	47.506484
2299.527827	70701.510587	47.511489
2296.008537	70272.363733	47.516493
2292.825685	69854.655651	47.521498
2289.149019	69420.100510	47.526503
2285.831858	68992.460554	47.531508
2282.376557	68555.504951	47.536513
2278.826475	68140.452621	47.541517
2275.562920	67705.677971	47.546522
2271.926624	67271.685990	47.551527
2268.097310	66843.234748	47.556532
2264.553923	66397.119360	47.561537
2261.231896	65975.738300	47.566541
2257.657452	65553.844973	47.571546
2253.980689	65122.142918	47.576551
2250.510287	64688.372402	47.581556
2247.137881	64251.636463	47.586561
2243.479738	63834.684785	47.591565
2240.232590	63399.962489	47.596570
2236.829784	62980.180107	47.601575
2233.015296	62542.559140	47.606580
2229.891309	62110.670735	47.611585
2226.421526	61676.546343	47.616589
2223.156152	61245.056809	47.621594
2219.511904	60815.975487	47.626599
2215.835668	60371.695496	47.631604
2212.266306	59936.145099	47.636609
2208.636978	59501.912673	47.641613
2205.205307	59065.588575	47.646618
2201.872402	58626.445911	47.651623
2198.260812	58195.273567	47.656628
2195.325401	57756.186368	47.661633
2191.391545	57317.154690	47.666637
2188.087109	56877.899837	47.671642
2184.111156	56434.094059	47.676647
2180.543613	56003.905927	47.681652
2177.253881	55555.555668	47.686657
2173.312991	55122.675303	47.691661
2170.083553	54683.119311	47.696666
2166.726149	54251.756510	47.701671
2163.168680	53818.542168	47.706676
2159.957620	53379.845032	47.711681
2156.543315	52937.425770	47.716685
2153.276392	52503.663938	47.721690
2149.623426	52058.748233	47.726695
2145.994230	51604.994379	47.731700
2142.455478	51159.824357	47.736705
2138.935302	50726.160469	47.741709
2135.663665	50279.043793	47.746714
2132.198066	49841.753371	47.751719
2128.460904	49394.491635	47.756724
2125.039546	48946.098507	47.761729
2121.382438	48503.199261	47.766733
2118.055654	48063.022582	47.771738
2114.408252	47611.811321	47.776743
2111.043739	47169.368192	47.781748
2107.712254	46721.201537	47.786753
2103.744088	46285.123098	47.791757
2100.089609	45830.428629	47.796762
2096.711738	45380.564513	47.801767
2093.162113	44942.538107	47.806772
2089.709533	44499.406536	47.811777
2085.920880	44064.123407	47.816781
2082.638418	43617.989724	47.821786
2079.014412	43179.400808	47.826791
2075.813243	42734.641961	47.831796
2072.140122	42288.868536	47.836801
2068.692280	41844.831828	47.841805
2065.363317	41396.163214	47.846810
2062.146305	40954.543431	47.851815
2058.238787	40516.013707	47.856820
2054.675111	40066.838265	47.861825
2050.915905	39620.409793	47.866829
2047.576473	39175.992037	47.871834
2044.035448	38737.783536	47.876839
2040.897675	38291.716866	47.881844
2037.380004	37846.891394	47.886849
2033.582564	37399.677947	47.891853
2029.985016	36957.267013	47.896858
2026.618986	36511.805362	47.901863
2023.210963	36060.388070	47.906868
2019.976478	35620.965774	47.911873
2015.906435	35170.215572	47.916877
2012.567831	34720.635216	47.921882
2008.884605	34285.861675	47.926887
2005.622684	33837.733394	47.931892
2002.035530	33390.761811	47.936897
1998.397302	32955.159438	47.941901
1995.093052	32502.439364	47.946906
1991.524336	32060.126459	47.951911
1987.729660	31622.231201	47.956916
1984.357742	31178.816297	47.961921
1980.935467	30738.403692	47.966925
1977.494313	30296.482422	47.971930
1974.221891	29844.918041	47.976935
1970.026787	29400.395620	47.981940
1967.068424	28953.402686	47.986945
1963.464690	28512.939172	47.991949
1959.783052	28071.293292	47.996954
1956.485799	27621.106131	48.001959
1952.625481	27173.943991	48.006964
1949.182309	26734.507755	48.011969
1945.652573	26302.121329	48.016973
1942.284687	25854.335079	48.021978
1939.103400	25410.451639	48.026983
1935.443685	24967.038928	48.031988
1932.281703	24525.896383	48.036993
1928.411230	24082.732426	48.041997
1924.848626	23632.909961	48.047002
1921.511829	23182.992810	48.052007
1917.591708	22742.197716	48.057012
1914.429540	22291.652723	48.062017
1910.724521	21858.458345	48.067021
1907.188743	21411.919079	48.072026
1903.787379	20972.336926	48.077031
1899.922214	20534.882765	48.082036
1896.276387	20092.058155	48.087041
1892.722532	19656.260036	48.092045
1889.449055	19211.535184	48.097050
1885.685733	18776.948393	48.102055
1882.242942	18341.827396	48.107060
1878.743883	17913.362397	48.112065
1875.131470	17470.307152	48.117069
1871.540902	17035.187820	48.122074
1868.146236	16590.871213	48.127079
1864.398177	16166.853506	48.132084
1861.462646	15728.216650	48.137089
1857.896026	15304.569718	48.142093
1854.154922	14862.294317	48.147098
1850.684582	14429.795812	48.152103
1846.777844	14005.869687	48.157108
1843.615337	13569.679637	48.162113
1839.785402	13137.361476	48.167117
1836.040706	12700.832463	48.172122
1832.793699	12274.388827	48.177127
1829.186305	11857.254884	48.182132
1825.714673	11424.378848	48.187137
1821.937581	10998.708245	48.192141
1818.314848	10573.308184	48.197146
1814.918549	10145.888322	48.202151
1811.285383	9727.786511	48.207156
1807.643638	9306.656723	48.212161
1803.987608	8895.642140	48.217165
1800.829783	8473.610806	48.222170
1797.039495	8048.522427	48.227175
1793.434825	7640.297175	48.232180
1789.700004	7213.560918	48.237185
1785.993121	6808.943226	48.242189
1782.059902	6397.432405	48.247194
1778.725314	5992.357019	48.252199
1774.827887	5594.324652	48.257204
1771.526906	5194.511903	48.262209
1767.532932	4805.223932	48.267213
1764.071109	4409.086344	48.272218
1759.946759	4022.711926	48.277223
1755.459314	3653.122598	48.282228
1750.372000	3331.136280	48.287233
1742.902527	3074.140011	48.292237
1737.514444	2802.201766	48.297242
1733.156479	2539.166239	48.302247
1728.149216	2313.749154	48.307252
1724.247765	2093.143029	48.312257
1719.839114	1900.939750	48.317261
1716.044313	1710.329406	48.322266
1712.273344	1528.832757	48.327271
1708.314767	1358.260567	48.332276
1705.138249	1191.684524	48.337281
1701.358212	1034.360220	48.342285
1698.260045	872.115805	48.347290
1694.806966	720.362379	48.352295
1691.160022	572.601490	48.357300
1687.592003	423.171733	48.362305
1684.188266	286.787078	48.367309
1680.394291	143.437594	48.372314
1676.820822	22.150182	48.377319
1666.823609	44.004649	48.382324
1659.202943	68.823792	48.387329
1654.429858	77.615350	48.392333
1651.737180	76.541378	48.397338
1649.657367	71.594557	48.402343
1647.373797	77.461350	48.407348
1644.738193	75.220580	48.412353
1641.816456	82.629350	48.417357
1638.909302	74.350207	48.422362
1635.663992	67.436636	48.427367
1631.961108	86.410100	48.432372
1628.846912	62.078920	48.437377
1624.762358	77.166645	48.442381
1620.977438	85.155847	48.447386
1618.396993	71.362141	48.452391
1614.741562	82.466417	48.457396
1611.715076	78.979878	48.462401
1608.415409	77.497355	48.467405
1604.947342	80.641067	48.472410
1601.559147	68.472684	48.477415
1597.821184	79.751153	48.482420
1594.624427	71.643640	48.487425
1591.490850	75.105444	48.492429
1587.503270	83.499506	48.497434
1584.641701	75.877653	48.502439
1581.089427	85.782650	48.507444
1577.263707	75.441384	48.512449
1573.823874	69.820415	48.517453
1570.174676	73.922448	48.522458
1567.153293	71.903079	48.527463
1563.481506	80.807964	48.532468
1560.152762	75.947975	48.537473
1556.834774	79.922530	48.542477
1553.306605	79.725240	48.547482
1550.007431	80.416109	48.552487
1546.438327	84.135526	48.557492
1543.314937	76.889782	48.562497
1539.890629	84.547617	48.567501
1535.959430	87.564106	48.572506
1532.362197	81.939163	48.577511
1528.582162	81.812715	48.582516
1526.012912	83.791496	48.587521
1522.282588	84.248922	48.592525
1518.716097	86.724601	48.597530
1515.100847	76.704922	48.602535
1511.737523	86.852590	48.607540
1508.627383	81.370132	48.612545
1504.873927	85.099264	48.617549
1500.887866	85.593334	48.622554
1497.891221	69.814354	48.627559
1494.227590	84.735329	48.632564
1490.840012	77.565513	48.637569
1487.369374	71.231190	48.642573
1484.349645	74.808155	48.647578
1480.823284	71.317181	48.652583
1476.687117	79.313601	48.657588
1473.526260	82.188046	48.662593
1469.806870	83.406228	48.667597
1466.439250	82.896061	48.672602
1463.294194	70.458909	48.677607
1459.417617	79.851244	48.682612
1456.192223	72.864997	48.687617
1452.654914	77.987316	48.692621
1448.731214	82.720533	48.697626
1445.919426	74.812546	48.702631
1442.311529	82.008585	48.707636
1438.694002	76.209650	48.712641
1435.368257	71.115099	48.717645
1431.446539	74.272485	48.722650
1428.232108	70.846860	48.727655
1424.315536	82.115167	48.732660
1420.871393	74.685253	48.737665
1417.657781	72.113700	48.742669
1414.127178	72.919694	48.747674
1411.299553	76.052319	48.752679
1407.038576	84.795821	48.757684
1403.570999	67.403913	48.762689
1400.594819	80.446212	48.767693
1396.833142	73.916761	48.772698
1393.510566	72.042365	48.777703
1389.913102	71.004843	48.782708
1386.248090	67.497499	48.787713
1382.473754	68.683113	48.792717
1379.043349	71.871597	48.797722
1375.916070	76.632711	48.802727
1372.281056	72.329775	48.807732
1368.617961	69.935755	48.812737
1365.087826	70.634116	48.817741
1361.683629	70.325803	48.822746
1358.234905	61.650123	48.827751
1354.886264	72.159323	48.832756
1351.377800	65.808765	48.837761
1347.966886	70.329296	48.842765
1344.429512	71.974730	48.847770
1341.055991	62.357221	48.852775
1337.401310	76.618745	48.857780
1333.837513	68.906921	48.862785
1330.364363	68.596689	48.867789
1326.433674	69.980648	48.872794
1323.076704	72.730607	48.877799
1319.694721	72.975650	48.882804
1316.350320	60.300650	48.887809
1312.777338	65.222887	48.892813
1309.136351	70.364514	48.897818
1305.710932	79.847979	48.902823
1302.423186	77.287976	48.907828
1299.401090	79.827629	48.912833
1295.752353	65.567534	48.917837
1292.077333	72.511437	48.922842
1288.529727	65.926541	48.927847
1284.579424	82.695435	48.932852
1281.308930	72.198207	48.937857
1277.824376	72.756607	48.942861
1274.099592	69.866010	48.947866
1271.029287	65.266388	48.952871
1267.662392	77.610211	48.957876
1264.375638	68.254449	48.962881
1260.449543	59.542363	48.967885
1256.503743	67.528140	48.972890
1253.199912	66.375328	48.977895
1249.723379	77.733327	48.982900
1246.544859	74.197732	48.987905
1242.778462	75.881988	48.992909
1239.194322	75.503621	48.997914
1235.927396	72.269685	49.002919
1232.829493	65.358541	49.007924
1229.260028	71.346401	49.012929
1225.564142	63.332463	49.017933
1221.446324	77.283268	49.022938
1218.564894	63.973085	49.027943
1214.596027	76.157512	49.032948
1211.513241	73.303032	49.037953
1207.805117	65.395403	49.042957
1204.233089	74.370188	49.047962
1200.993696	62.472952	49.052967
1197.174397	63.409325	49.057972
1194.256775	65.388567	49.062977
1190.454167	74.161966	49.067981
1187.239349	74.789119	49.072986
1183.463336	70.735943	49.077991
1179.582487	73.402946	49.082996
1176.271204	74.130535	49.088001
1173.069126	69.560927	49.093005
1169.291998	64.818245	49.098010
1165.814856	67.324334	49.103015
1162.159011	75.100474	49.108020
1158.928932	66.618580	49.113025
1155.550391	65.863379	49.118029
1151.978188	75.300091	49.123034
1148.366890	63.460755	49.128039
1144.715532	67.202493	49.133044
1141.223284	75.759910	49.138049
1138.141696	66.704424	49.143053
1134.208746	76.152998	49.148058
1131.163168	74.181734	49.153063
1127.499756	74.628787	49.158068
1124.181756	65.059622	49.163073
1120.442920	64.009338	49.168077
1116.564269	69.434739	49.173082
1113.423966	69.502982	49.178087
1109.716330	74.987186	49.183092
1106.550751	74.958125	49.188097
1103.052708	68.403509	49.193101
1099.043224	71.081052	49.198106
1096.178913	67.534533	49.203111
1092.219349	74.516412	49.208116
1088.745051	68.378873	49.213121
1085.444202	63.277336	49.218125
1081.709138	60.856594	49.223130
1078.567318	58.147361	49.228135
1074.836290	67.301917	49.233140
1071.222425	65.941127	49.238145
1067.871111	58.050752	49.243149
1064.240285	68.452022	49.248154
1060.958863	56.757510	49.253159
1057.344623	65.691411	49.258164
1053.726223	64.116199	49.263169
1050.471811	70.706748	49.268173
1047.000607	68.007661	49.273178
1043.301247	64.116580	49.278183
1039.980322	61.441558	49.283188
1036.373039	54.198462	49.288193
1032.895571	65.373107	49.293197
1029.320879	67.312276	49.298202
1025.989121	64.790799	49.303207
1022.477260	57.643579	49.308212
1018.957913	64.300676	49.313217
1015.344861	68.485706	49.318221
1011.470332	65.393836	49.323226
1008.247572	57.436006	49.328231
1004.721630	59.683956	49.333236
1001.408108	59.845611	49.338241
997.656323	72.442327	49.343245
994.199143	58.592244	49.348250
991.134615	55.665352	49.353255
987.366917	68.160141	49.358260
984.055670	64.774955	49.363265
980.192563	65.028489	49.368269
976.636048	71.681886	49.373274
973.556775	54.843413	49.378279
969.828416	57.375970	49.383284
966.638395	61.517299	49.388289
962.984641	60.254480	49.393293
959.214669	67.149907	49.398298
955.827282	54.592409	49.403303
952.323259	60.927592	49.408308
949.122279	58.252894	49.413313
945.658397	59.912236	49.418317
941.364579	64.699940	49.423322
938.037041	60.959800	49.428327
934.270133	70.847596	49.433332
931.108905	62.889689	49.438337
927.892895	66.835755	49.443341
923.697891	67.258017	49.448346
920.986428	58.426527	49.453351
917.578378	66.524763	49.458356
913.645504	69.775681	49.463361
910.516722	72.505972	49.468365
906.570818	74.534575	49.473370
903.029112	67.955153	49.478375
899.843225	66.382236	49.483380
896.293030	66.254885	49.488385
892.643955	62.501530	49.493389
889.324117	68.229095	49.498394
885.985414	66.157960	49.503399
882.495270	69.561422	49.508404
878.595424	63.243396	49.513409
875.013556	60.912729	49.518413
871.422359	63.161360	49.523418
868.232147	65.644958	49.528423
864.826808	59.351196	49.533428
861.377052	61.501882	49.538433
857.812266	67.381471	49.543437
854.152704	69.647074	49.548442
850.745186	66.900137	49.553447
847.124954	71.263466	49.558452
843.846675	68.566012	49.563457
840.384415	62.009038	49.568461
836.504407	79.646481	49.573466
833.250782	54.676051	49.578471
829.609939	62.585907	49.583476
826.192048	60.330959	49.588481
822.834424	59.901564	49.593485
818.697306	59.141105	49.598490
816.044360	64.391547	49.603495
812.234709	62.773375	49.608500
808.935529	59.981107	49.613505
805.501572	62.160976	49.618509
801.419510	60.034732	49.623514
797.956772	50.744427	49.628519
794.522248	63.041823	49.633524
791.428183	65.478824	49.638529
787.925599	63.496487	49.643533
783.995144	67.436724	49.648538
780.839750	62.464449	49.653543
777.291725	56.632666	49.658548
773.562643	56.299066	49.663553
769.793468	62.276914	49.668557
766.383549	55.164491	49.673562
763.623860	51.101872	49.678567
759.740098	55.990270	49.683572
756.190217	61.506886	49.688577
752.569205	54.939842	49.693581
748.768650	49.602948	49.698586
745.470564	57.054499	49.703591
741.818301	56.155301	49.708596
738.649810	55.911604	49.713601
735.257597	57.480720	49.718605
731.351812	54.172305	49.723610
728.481743	59.307856	49.728615
724.514210	50.266987	49.733620
721.083124	60.368258	49.738625
718.001209	60.576146	49.743629
714.110328	56.531441	49.748634
710.700751	54.088560	49.753639
707.419830	60.303609	49.758644
703.734570	55.603653	49.763649
700.159530	52.781582	49.768653
696.330798	59.347659	49.773658
693.045866	58.359648	49.778663
689.777523	54.841280	49.783668
686.169114	55.384226	49.788673
682.617168	50.021296	49.793677
679.034856	59.064134	49.798682
675.554688	55.781218	49.803687
672.157135	52.548717	49.808692
668.281625	60.849444	49.813697
664.950649	57.397775	49.818701
661.194346	63.035116	49.823706
658.141759	61.283295	49.828711
654.710002	58.891329	49.833716
651.267281	53.818277	49.838721
647.882008	47.932711	49.843725
644.339292	60.531681	49.848730
640.441533	59.800425	49.853735
636.930033	62.697882	49.858740
633.481675	65.430490	49.863745
629.898288	57.756653	49.868749
626.287738	69.923275	49.873754
623.088598	57.697205	49.878759
619.672218	56.941633	49.883764
616.117294	61.639654	49.888769
612.654621	63.631030	49.893773
608.603102	60.155502	49.898778
605.319003	54.820488	49.903783
601.721041	56.681069	49.908788
597.798204	62.426596	49.913793
594.733233	65.042578	49.918797
591.260184	69.617129	49.923802
588.472645	60.136331	49.928807
584.783542	61.960484	49.933812
580.717224	59.778043	49.938817
577.432295	56.170528	49.943821
573.889896	70.224745	49.948826
570.488212	64.132939	49.953831
566.900647	65.166188	49.958836
563.800581	65.636340	49.963841
560.261464	67.383365	49.968845
556.152812	65.982617	49.973850
553.238289	66.449195	49.978855
549.628496	59.266690	49.983860
546.119750	61.170335	49.988865
542.620417	57.697440	49.993869
538.674931	65.097935	49.998874
535.719677	51.910129	50.003879
532.114353	66.948550	50.008884
528.421819	59.044958	50.013889
524.973943	46.765894	50.018893
520.907480	64.318453	50.023898
518.288768	62.562378	50.028903
514.359467	55.973773	50.033908
510.703147	61.402578	50.038913
507.949934	61.831393	50.043917
503.624730	63.181959	50.048922
500.061601	60.108134	50.053927
496.556431	65.004059	50.058932
493.740176	67.938826	50.063937
489.964846	57.763963	50.068941
486.067502	65.093694	50.073946
483.105556	69.237519	50.078951
479.252092	70.505158	50.083956
475.825200	66.967212	50.088961
472.407326	59.261311	50.093965
469.067457	69.895711	50.098970
465.497513	64.731765	50.103975
461.909319	67.410233	50.108980
458.065024	63.845525	50.113985
454.797669	62.266367	50.118989
451.109825	67.437502	50.123994
447.956784	67.735586	50.128999
444.633659	59.031039	50.134004
440.684474	70.668272	50.139009
437.200618	63.621201	50.144013
433.579900	76.105782	50.149018
430.801067	61.419422	50.154023
426.962869	66.424146	50.159028
423.159364	67.272739	50.164033
419.521247	62.239635	50.169037
415.865798	69.667753	50.174042
412.910004	61.475485	50.179047
409.549256	61.767946	50.184052
405.924210	66.103591	50.189057
402.687392	59.305963	50.194061
399.016342	63.557025	50.199066
395.346273	58.468791	50.204071
391.934441	54.801970	50.209076
388.120044	58.610290	50.214081
384.634788	56.663280	50.219085
381.082371	59.462733	50.224090
377.767060	59.302047	50.229095
374.122252	56.452924	50.234100
370.692454	62.618411	50.239105
367.254804	53.472982	50.244109
363.598788	70.854083	50.249114
360.604489	66.318690	50.254119
356.995806	57.560546	50.259124
353.173942	63.707981	50.264129
349.914989	57.195376	50.269133
346.174949	70.657124	50.274138
342.773317	56.893465	50.279143
339.166085	61.564856	50.284148
336.215148	62.081418	50.289153
332.624215	56.724620	50.294157
328.879442	62.923329	50.299162
325.278961	58.684791	50.304167
321.416134	52.898940	50.309172
317.427354	66.687304	50.314177
314.886823	50.749033	50.319181
310.938133	49.880230	50.324186
307.006851	51.492192	50.329191
304.252730	56.239570	50.334196
301.120195	56.534478	50.339201
297.911379	52.801266	50.344205
293.455396	57.753492	50.349210
289.677288	55.712888	50.354215
286.279014	56.096626	50.359220
283.110161	56.631302	50.364225
279.845838	53.542631	50.369229
276.249179	58.497111	50.374234
272.775237	59.806929	50.379239
269.126810	50.520336	50.384244
265.633145	57.622727	50.389249
262.547833	58.280436	50.394253
258.459145	48.530895	50.399258
255.283167	57.782570	50.404263
251.722016	55.502558	50.409268
248.238424	56.601916	50.414273
244.794685	50.652762	50.419277
240.609798	60.450644	50.424282
237.494167	54.947101	50.429287
234.422896	64.679174	50.434292
230.878256	59.109549	50.439297
227.310547	63.543851	50.444301
223.643713	66.171318	50.449306
220.338697	57.853130	50.454311
216.593653	66.763151	50.459316
213.125083	55.597824	50.464321
209.481295	55.149789	50.469325
206.033793	57.455216	50.474330
202.520794	60.223245	50.479335
198.969701	59.498196	50.484340
195.371781	55.803434	50.489345
192.097817	55.424370	50.494349
188.589549	64.465202	50.499354
184.974537	50.934121	50.504359
181.509008	68.070433	50.509364
178.002205	58.689043	50.514369
174.542939	59.471422	50.519373
171.123908	66.995625	50.524378
167.706033	62.032680	50.529383
164.094139	64.066323	50.534388
160.790488	64.916222	50.539393
157.493677	56.274077	50.544397
153.347083	56.733212	50.549402
149.975674	60.700375	50.554407
146.599327	63.937502	50.559412
142.849596	58.039168	50.564417
139.638412	53.977330	50.569421
136.294206	60.635696	50.574426
132.383376	54.999722	50.579431
128.751146	56.558823	50.584436
125.380258	64.417208	50.589441
122.289680	60.336594	50.594445
118.238775	63.283291	50.599450
115.390671	65.128423	50.604455
111.539452	62.058389	50.609460
107.529277	59.263033	50.614465
104.337134	55.172927	50.619469
100.894487	66.092253	50.624474
97.409155	64.082026	50.629479
94.327295	59.111071	50.634484
90.609708	60.854305	50.639489
87.238485	50.983609	50.644493
83.344912	55.914737	50.649498
79.854209	53.060654	50.654503
76.515526	48.594749	50.659508
73.170807	62.105679	50.664513
69.758985	54.503322	50.669517
65.892642	56.060918	50.674522
62.678202	54.207832	50.679527
59.005414	51.394759	50.684532
55.220733	55.344020	50.689537
52.198640	51.594432	50.694541
48.721140	61.617542	50.699546
44.573742	50.130857	50.704551
41.350159	52.913953	50.709556
37.735005	57.827046	50.714561
34.694875	51.261452	50.719565
31.037466	57.981245	50.724570
27.611628	60.827470	50.729575
24.094707	56.053976	50.734580
20.172552	53.823883	50.739585
16.827018	45.195688	50.744589
13.231429	55.838278	50.749594
10.351750	60.921592	50.754599
6.557665	58.798107	50.759604
2.821653	66.697533	50.764609