Fri Aug 26 11:13:54 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.955209	100.124172	0.000000
1.247182	91.578153	0.005005
1.033464	95.452307	0.010010
0.945235	80.245875	0.015014
0.725563	91.957338	0.020019
0.664028	92.805484	0.025024
0.369458	85.211306	0.030029
0.216302	81.340884	0.035034
0.101536	70.131129	0.040038
-0.442121	75.059529	0.045043
-0.379238	59.826423	0.050048
-0.622260	50.300732	0.055053
-1.162875	49.578368	0.060058
-1.119320	44.067028	0.065062
-1.897362	40.053471	0.070067
-2.318241	25.117170	0.075072
-1.685483	23.601533	0.080077
-2.598644	22.361391	0.085082
-3.054479	13.900204	0.090086
-3.066289	12.601980	0.095091
-3.209864	16.579087	0.100096
-3.354736	9.433017	0.105101
-4.188628	8.908173	0.110106
-4.198836	6.976971	0.115110
-4.876525	5.026312	0.120115
-4.915233	9.088327	0.125120
-4.638819	0.994010	0.130125
-5.071707	3.016737	0.135130
-5.338712	5.893130	0.140134
-5.869153	4.137836	0.145139
-6.170579	-7.938117	0.150144
-6.004514	-2.152166	0.155149
-7.165074	-0.832363	0.160154
-7.374818	1.326457	0.165158
-7.554173	-3.283323	0.170163
-7.607390	-2.778150	0.175168
-7.462044	1.796190	0.180173
-7.466793	-0.123207	0.185178
-7.404320	-8.326572	0.190182
-8.132727	3.957569	0.195187
-8.525974	-1.707203	0.200192
-8.551388	-4.088437	0.205197
-8.809029	6.429860	0.210202
-9.507968	1.793412	0.215206
-10.385049	4.761628	0.220211
-10.032376	7.440303	0.225216
-10.362398	6.492170	0.230221
-10.583530	5.289810	0.235226
-10.304139	0.656058	0.240230
-10.168199	2.606039	0.245235
-10.800514	5.748110	0.250240
-11.557561	-3.314718	0.255245
-11.932955	5.690709	0.260250
-11.981886	-0.445273	0.265254
-12.184705	4.164293	0.270259
-12.212110	3.624609	0.275264
-11.915386	-2.891045	0.280269
-12.657518	7.731159	0.285274
-12.923432	-0.984209	0.290278
-13.315416	-1.868912	0.295283
-13.688204	5.361306	0.300288
-13.668957	-2.544277	0.305293
-14.107088	3.788148	0.310298
-14.792145	-5.213123	0.315302
-15.057702	-1.134773	0.320307
-15.115666	4.366533	0.325312
-14.650745	4.338633	0.330317
-14.780665	2.239415	0.335322
-15.000024	-7.856219	0.340326
-16.087472	-3.067793	0.345331
-16.334557	4.788236	0.350336
-16.041185	0.892600	0.355341
-16.349172	2.399188	0.360346
-16.506121	4.641534	0.365350
-17.164832	3.181449	0.370355
-17.685194	0.193930	0.375360
-17.546511	-1.852199	0.380365
-17.832157	3.409319	0.385370
-17.714751	2.344069	0.390374
-18.129808	0.263938	0.395379
-18.795741	-0.881821	0.400384
-18.729898	2.597621	0.405389
-19.391215	6.152318	0.410394
-19.390928	1.448130	0.415398
-19.302113	-1.156526	0.420403
-19.789927	1.061408	0.425408
-19.839697	-1.034470	0.430413
-20.058583	-2.420670	0.435418
-20.024180	-3.352778	0.440422
-21.125797	-0.384403	0.445427
-21.714755	2.475679	0.450432
-21.705553	-7.842196	0.455437
-21.528113	2.810830	0.460442
-21.724753	3.224443	0.465446
-21.887695	-0.109781	0.470451
-22.114913	0.599648	0.475456
-22.712555	-2.309402	0.480461
-22.962585	2.025950	0.485466
-23.217556	5.311742	0.490470
-23.017353	3.439526	0.495475
-23.474836	4.589754	0.500480
-23.882160	-1.145590	0.505485
-24.476708	9.912365	0.510490
-24.477146	6.660403	0.515494
-24.422957	7.085580	0.520499
-24.710268	4.340176	0.525504
-24.412842	3.025442	0.530509
-25.477959	6.544936	0.535514
-25.979485	2.361790	0.540518
-26.321764	8.410383	0.545523
-26.308771	6.579969	0.550528
-25.891078	2.807341	0.555533
-26.093374	4.471473	0.560538
-26.665133	7.680044	0.565542
-27.485984	10.206087	0.570547
-27.679665	4.927843	0.575552
-27.495074	6.411520	0.580557
-27.518582	1.296600	0.585562
-27.720409	-3.116698	0.590566
-28.361607	3.547890	0.595571
-28.944597	5.018205	0.600576
-28.602875	5.528323	0.605581
-29.140104	4.837072	0.610586
-29.016624	-0.462079	0.615590
-29.668088	4.457777	0.620595
-30.036399	13.939815	0.625600
-30.560219	9.152719	0.630605
-30.728292	16.737031	0.635610
-30.965409	6.410045	0.640614
-30.726207	2.807571	0.645619
-30.976630	8.591934	0.650624
-30.959941	8.156112	0.655629
-31.668528	11.620097	0.660634
-31.778398	-2.054851	0.665638
-32.174188	5.394075	0.670643
-32.424808	10.289486	0.675648
-32.648517	2.292021	0.680653
-33.424348	2.900213	0.685658
-33.657846	4.626149	0.690662
-33.608901	5.248289	0.695667
-33.855516	-0.432984	0.700672
-33.766196	7.509867	0.705677
-33.903266	6.879694	0.710682
-33.895383	3.484073	0.715686
-34.354966	4.172735	0.720691
-34.992213	7.480084	0.725696
-35.056454	1.333831	0.730701
-35.198522	1.916112	0.735706
-35.255061	-0.776641	0.740710
-36.069137	0.916308	0.745715
-36.464742	-3.131473	0.750720
-36.500325	0.907907	0.755725
-36.334213	9.332332	0.760730
-36.422841	8.890762	0.765734
-36.930789	-5.962350	0.770739
-37.350288	12.926838	0.775744
-37.720760	-1.096663	0.780749
-37.850779	4.105824	0.785754
-38.058454	4.122536	0.790758
-38.325636	2.088982	0.795763
-39.319608	1.895936	0.800768
-39.330341	0.806346	0.805773
-39.420105	8.210789	0.810778
-39.644425	8.524312	0.815782
-39.658939	6.422944	0.820787
-39.876343	5.760987	0.825792
-39.425855	-10.734587	0.830797
-40.170810	8.746252	0.835802
-40.642823	-2.319248	0.840806
-40.703732	4.160080	0.845811
-41.005417	11.141955	0.850816
-40.796436	-4.253038	0.855821
-41.913565	2.336959	0.860826
-41.774332	-0.629875	0.865830
-42.144384	8.738539	0.870835
-42.319749	3.928828	0.875840
-42.803768	7.459083	0.880845
-43.380938	9.804822	0.885850
-43.487015	7.198873	0.890854
-43.682966	1.566656	0.895859
-43.692298	3.460163	0.900864
-43.594480	5.539461	0.905869
-43.718539	1.829037	0.910874
-43.724879	7.379250	0.915878
-44.870346	5.754516	0.920883
-45.184454	2.453320	0.925888
-45.219518	2.886067	0.930893
-45.409884	5.586017	0.935898
-45.319399	5.616416	0.940902
-45.825365	1.845236	0.945907
-46.656575	5.970531	0.950912
-46.914908	-2.167068	0.955917
-46.920428	11.814127	0.960922
-46.935356	1.544296	0.965926
-46.881485	5.164803	0.970931
-46.767760	1.996303	0.975936
-47.252373	-6.545808	0.980941
-48.468763	5.156272	0.985946
-48.253060	4.369936	0.990950
-48.444775	6.130494	0.995955
-48.473176	12.737637	1.000960
-48.519765	-4.705569	1.005965
-49.811845	0.693666	1.010970
-49.951993	0.029172	1.015974
-49.782418	10.718225	1.020979
-50.169879	5.653645	1.025984
-50.694424	0.926774	1.030989
-50.342418	6.076356	1.035994
-49.890580	-0.096466	1.040998
-50.510090	3.407429	1.046003
-51.058264	12.515687	1.051008
-50.908576	3.624883	1.056013
-51.367438	5.094853	1.061018
-52.588737	4.813821	1.066022
-52.717551	-1.161030	1.071027
-53.000470	2.394859	1.076032
-52.644108	-0.105926	1.081037
-53.104817	9.352530	1.086042
-52.811044	-0.813508	1.091046
-53.064343	9.065055	1.096051
-53.322231	3.910702	1.101056
-53.677121	-4.145425	1.106061
-54.171550	3.122711	1.111066
-54.446230	3.915457	1.116070
-54.121470	12.334162	1.121075
-54.994524	2.302342	1.126080
-55.221831	2.625820	1.131085
-55.403717	-0.259379	1.136090
-55.615786	0.871619	1.141094
-55.589341	7.704330	1.146099
-56.264506	4.285349	1.151104
-56.698677	6.320931	1.156109
-56.803221	7.305479	1.161114
-57.252711	-3.083342	1.166118
-57.131734	4.300940	1.171123
-57.396809	4.105135	1.176128
-57.403438	2.306250	1.181133
-58.226809	1.352678	1.186138
-58.658954	0.844375	1.191142
-58.632046	2.678458	1.196147
-59.257714	4.414836	1.201152
-58.443219	-6.784531	1.206157
-59.024906	2.332103	1.211162
-58.978171	-0.993639	1.216166
-59.630740	0.126854	1.221171
-60.066202	-0.596060	1.226176
-60.463489	-0.749134	1.231181
-60.409269	7.948964	1.236186
-60.346996	6.329169	1.241190
-60.727837	1.564106	1.246195
-62.148346	4.955444	1.251200
-61.585280	-2.835498	1.256205
-61.932599	-9.719089	1.261210
-62.130115	0.457657	1.266214
-62.023177	-3.722150	1.271219
-62.316173	3.729750	1.276224
-62.109068	-1.528637	1.281229
-63.319919	5.496719	1.286234
-63.259804	-0.165875	1.291238
-63.047792	-1.315455	1.296243
-63.492439	6.277114	1.301248
-63.524245	-2.158336	1.306253
-64.244464	-0.897601	1.311258
-64.847376	2.499310	1.316262
-64.916718	-8.850333	1.321267
-64.961355	7.307203	1.326272
-64.843903	5.020780	1.331277
-65.382395	0.846556	1.336282
-66.135356	5.472177	1.341286
-65.843945	-0.865484	1.346291
-66.104358	11.064227	1.351296
-65.956677	7.235566	1.356301
-66.381642	5.900435	1.361306
-67.041801	-1.102124	1.366310
-66.960858	4.282643	1.371315
-67.649561	2.738648	1.376320
-67.470022	-3.746103	1.381325
-68.367035	4.695153	1.386330
-68.679970	7.910879	1.391334
-68.525999	0.711960	1.396339
-68.965503	11.755263	1.401344
-69.037284	7.217316	1.406349
-69.057889	15.588558	1.411354
-68.780203	7.984409	1.416358
-69.446865	11.005283	1.421363
-70.102973	9.633376	1.426368
-70.016426	-0.905342	1.431373
-70.550515	0.924342	1.436378
-70.434639	1.355733	1.441382
-71.092291	-5.704159	1.446387
-71.595088	0.176439	1.451392
-71.608135	-7.208435	1.456397
-71.814571	10.973717	1.461402
-72.109357	1.683901	1.466406
-72.228311	6.438590	1.471411
-72.150875	-1.093248	1.476416
-72.675245	-1.334100	1.481421
-73.356021	-1.550599	1.486426
-73.327673	0.612277	1.491430
-73.243739	-3.848675	1.496435
-73.500916	2.914301	1.501440
-73.553164	-0.838938	1.506445
-74.440349	-6.638762	1.511450
-74.850184	-0.491074	1.516454
-74.947655	5.222017	1.521459
-75.376877	2.587293	1.526464
-75.046290	0.565067	1.531469
-75.386944	5.680130	1.536474
-75.635228	3.017233	1.541478
-76.453230	-1.233689	1.546483
-76.486722	8.063338	1.551488
-76.716348	-6.203537	1.556493
-76.776077	8.649765	1.561498
-76.630483	10.693151	1.566502
-76.762747	-3.557250	1.571507
-77.343468	8.238839	1.576512
-77.692985	4.095301	1.581517
-78.344457	1.435071	1.586522
-78.301842	0.128375	1.591526
-78.379097	-2.238459	1.596531
-78.615267	4.942012	1.601536
-78.660175	-1.491975	1.606541
-79.208278	0.137417	1.611546
-79.572557	4.316556	1.616550
-78.979664	-0.888006	1.621555
-80.030297	-1.948556	1.626560
-80.286395	-5.894673	1.631565
-80.744316	2.832543	1.636570
-80.987389	1.114764	1.641574
-80.713816	-4.081207	1.646579
-81.322297	-1.654668	1.651584
-81.538216	-4.120130	1.656589
-82.268886	7.895451	1.661594
-82.611372	1.919070	1.666598
-82.374282	4.770756	1.671603
-82.743742	10.753979	1.676608
-82.399664	0.576946	1.681613
-82.445618	-3.332290	1.686618
-82.802091	10.738342	1.691622
-83.405893	-6.675043	1.696627
-83.752011	3.186330	1.701632
-83.846670	7.567091	1.706637
-83.999244	-2.257375	1.711642
-85.002744	-6.909667	1.716646
-85.168247	-3.941517	1.721651
-85.485348	5.731848	1.726656
-85.661432	-0.558332	1.731661
-85.643338	-4.882487	1.736666
-85.657354	-2.187851	1.741670
-85.682659	-1.335860	1.746675
-85.774067	2.759666	1.751680
-86.059238	0.203749	1.756685
-86.891672	-1.656375	1.761690
-86.933796	-1.655948	1.766694
-87.131119	1.114684	1.771699
-87.682039	5.642412	1.776704
-88.032455	2.691707	1.781709
-88.522872	10.038311	1.786714
-88.997779	-4.206192	1.791718
-88.701401	2.160557	1.796723
-89.133973	-3.137430	1.801728
-88.968642	-3.311668	1.806733
-88.954864	0.780134	1.811738
-89.168102	0.895785	1.816742
-89.130105	-2.105903	1.821747
-89.899533	-3.561400	1.826752
-90.047233	-2.772607	1.831757
-89.680627	0.451204	1.836762
-90.927289	-1.527916	1.841766
-91.229745	-3.986231	1.846771
-91.391705	5.188432	1.851776
-91.549360	-5.173059	1.856781
-91.527121	-0.867447	1.861786
-92.181153	1.689567	1.866790
-92.716529	-10.919404	1.871795
-93.171241	4.087138	1.876800
-93.053096	-14.400393	1.881805
-93.095456	-0.214168	1.886810
-93.381761	2.519700	1.891814
-93.098972	5.202925	1.896819
-93.421985	2.950282	1.901824
-93.748698	-5.613247	1.906829
-94.294944	0.742336	1.911834
-94.699566	-3.234438	1.916838
-94.861655	-5.793699	1.921843
-94.830545	-5.519947	1.926848
-95.057452	-4.399293	1.931853
-95.164391	-3.294155	1.936858
-95.875385	2.887770	1.941862
-95.820752	-6.611462	1.946867
-96.101933	0.664595	1.951872
-96.756040	1.045037	1.956877
-97.433610	3.798698	1.961882
-97.766278	0.734504	1.966886
-97.606396	-0.552487	1.971891
-97.664499	0.564030	1.976896
-97.739723	-1.350720	1.981901
-97.745926	6.714564	1.986906
-97.796177	5.836764	1.991910
-98.128493	-7.142335	1.996915
-98.700514	-2.956537	2.006912
-98.920950	6.242308	2.016909
-97.994377	4.197815	2.026906
-97.560074	1.992393	2.036902
-96.815241	4.601028	2.046899
-96.469594	3.404064	2.056896
-96.398058	-1.880890	2.066893
-95.775868	0.648642	2.076890
-95.178839	-2.047768	2.086886
-94.443595	-5.978923	2.096883
-93.609206	0.502525	2.106880
-93.781152	0.437825	2.116877
-93.354436	-0.302943	2.126874
-92.748593	0.192309	2.136870
-91.828830	2.818055	2.146867
-91.052346	3.087173	2.156864
-90.941768	0.374641	2.166861
-90.946320	0.556299	2.176858
-90.488647	7.410006	2.186854
-89.721221	3.711415	2.196851
-88.892193	4.656573	2.206848
-88.309661	8.259794	2.216845
-88.057142	6.519816	2.226842
-87.290409	2.510900	2.236838
-86.711688	1.518391	2.246835
-86.564480	0.624746	2.256832
-86.667875	3.941971	2.266829
-85.946701	-2.030156	2.276826
-84.412063	-7.289499	2.286822
-84.236209	-1.551290	2.296819
-84.113044	-7.981483	2.306816
-83.986647	-2.213401	2.316813
-82.916627	4.361237	2.326810
-82.511246	1.076966	2.336806
-82.208058	-0.525186	2.346803
-81.096221	5.878221	2.356800
-81.136199	5.697943	2.366797
-80.843114	5.427794	2.376794
-79.587933	3.804124	2.386790
-79.622029	2.153120	2.396787
-79.271092	4.164206	2.406784
-78.265350	11.071959	2.416781
-77.994538	7.523547	2.426778
-77.601872	6.521995	2.436774
-76.843996	6.154137	2.446771
-76.724131	11.479764	2.456768
-76.004787	11.171756	2.466765
-75.131563	5.571914	2.476762
-75.036755	0.308677	2.486758
-74.773545	12.400352	2.496755
-73.564743	10.730051	2.506752
-73.469851	11.520262	2.516749
-73.524556	11.614698	2.526746
-72.579330	9.190345	2.536742
-72.038882	8.463546	2.546739
-71.135935	16.172896	2.556736
-70.975776	9.350477	2.566733
-70.585457	4.706443	2.576730
-69.998091	-0.389574	2.586726
-69.194090	10.449021	2.596723
-69.210190	5.193547	2.606720
-68.651188	0.843187	2.616717
-68.324566	8.835496	2.626714
-67.336665	6.274624	2.636710
-66.773199	-2.916666	2.646707
-66.822599	4.798413	2.656704
-65.877386	3.967413	2.666701
-65.537627	0.924601	2.676698
-65.198657	7.613066	2.686694
-64.180494	12.995227	2.696691
-63.686346	6.234844	2.706688
-63.737967	8.736247	2.716685
-63.188984	11.153640	2.726682
-62.511308	11.691560	2.736678
-61.965716	2.664602	2.746675
-61.483289	12.492091	2.756672
-61.209440	2.699681	2.766669
-60.122927	6.791451	2.776666
-59.417231	0.650677	2.786662
-59.422871	1.504055	2.796659
-59.316241	3.717900	2.806656
-58.624768	2.432247	2.816653
-57.946098	-1.347554	2.826650
-57.729213	-1.035653	2.836646
-57.157231	4.976657	2.846643
-56.298136	2.917330	2.856640
-55.775115	5.386280	2.866637
-55.508551	6.317649	2.876634
-55.195622	2.480756	2.886630
-53.849849	4.720238	2.896627
-53.816355	6.254913	2.906624
-53.888217	8.471208	2.916621
-52.817066	3.464586	2.926618
-52.375294	3.899856	2.936614
-52.051042	4.457959	2.946611
-51.029707	7.710935	2.956608
-50.760052	9.981758	2.966605
-50.638440	13.349480	2.976602
-50.347528	8.293283	2.986598
-49.556481	8.303552	2.996595
-48.901297	10.580870	3.006592
-47.897307	9.940284	3.016589
-47.590102	8.993218	3.026586
-47.514400	11.715543	3.036582
-47.420022	9.699256	3.046579
-46.654229	13.470343	3.056576
-45.616561	12.431719	3.066573
-45.059044	11.616735	3.076570
-44.658739	4.269102	3.086566
-44.721149	5.381567	3.096563
-44.234166	7.042032	3.106560
-43.504233	9.611811	3.116557
-43.072751	9.858622	3.126554
-41.847002	5.369604	3.136550
-41.740047	9.097557	3.146547
-41.749808	9.181828	3.156544
-40.896134	7.158189	3.166541
-40.284889	12.198244	3.176538
-39.906050	8.107174	3.186534
-39.349937	5.841605	3.196531
-38.957568	8.381582	3.206528
-38.858828	5.800767	3.216525
-37.786652	3.844474	3.226522
-37.328452	1.315394	3.236518
-36.782190	5.678175	3.246515
-35.911498	13.218326	3.256512
-35.804517	16.686525	3.266509
-35.763108	15.055441	3.276506
-35.308599	10.262031	3.286502
-34.459315	15.575459	3.296499
-33.814476	15.044643	3.306496
-32.888075	12.464837	3.316493
-32.827666	13.602528	3.326490
-32.666330	12.424758	3.336486
-32.018101	11.133167	3.346483
-31.310396	8.688778	3.356480
-30.826964	9.580046	3.366477
-30.071048	9.421563	3.376474
-29.804196	11.778351	3.386470
-29.833214	1.668810	3.396467
-28.873443	2.980074	3.406464
-28.288668	8.464559	3.416461
-28.007618	2.386732	3.426458
-26.983507	4.631951	3.436454
-26.649392	7.434414	3.446451
-27.009685	5.663142	3.456448
-25.669776	4.146654	3.466445
-25.411539	5.937765	3.476442
-24.986344	14.760508	3.486438
-23.925978	13.620152	3.496435
-23.598620	9.990077	3.506432
-23.455510	11.165575	3.516429
-23.169958	7.253750	3.526426
-22.221062	11.712229	3.536422
-21.816629	16.154115	3.546419
-21.718841	15.065431	3.556416
-21.271202	13.564327	3.566413
-20.459799	2.709400	3.576410
-19.678924	10.219188	3.586406
-19.482645	8.484799	3.596403
-18.678569	11.869804	3.606400
-18.122039	17.903534	3.616397
-18.083873	8.176323	3.626394
-16.827112	4.420550	3.636390
-16.244917	8.274075	3.646387
-16.572499	7.131248	3.656384
-16.551892	11.705750	3.666381
-15.520276	1.852374	3.676378
-14.813329	10.485534	3.686374
-14.135728	9.578997	3.696371
-13.951329	14.020296	3.706368
-13.520891	14.124725	3.716365
-12.338987	8.647876	3.726362
-12.200219	12.944231	3.736358
-11.765148	6.364100	3.746355
-11.587439	7.882657	3.756352
-10.699199	11.454123	3.766349
-10.547697	7.664536	3.776346
-9.737257	9.341162	3.786342
-8.947270	7.723402	3.796339
-8.857220	15.901435	3.806336
-8.587090	12.619213	3.816333
-7.356309	10.090215	3.826330
-7.205125	7.798997	3.836326
-7.205386	9.693710	3.846323
-6.478837	6.650861	3.856320
-6.278878	9.600921	3.866317
-5.227802	12.222067	3.876314
-4.930848	17.105159	3.886310
-4.355758	18.286257	3.896307
-4.021509	21.114044	3.906304
-3.857124	29.765167	3.916301
-3.209838	35.487010	3.926298
-2.444677	45.809012	3.936294
-2.128232	57.211382	3.946291
-1.718814	73.442707	3.956288
-1.139087	76.099239	3.966285
-0.739268	87.713554	3.976282
-0.502664	107.085676	3.986278
0.000000	118.170759	3.991283
0.502628	117.165744	3.996288
0.605796	127.235641	4.001293
0.945471	125.085440	4.006298
0.887801	130.419065	4.011302
0.972133	129.725943	4.016307
0.887181	126.398533	4.021312
0.903727	138.041611	4.026317
0.799409	129.940078	4.031322
0.888384	136.462558	4.036326
0.912204	142.773727	4.041331
0.960341	133.670882	4.046336
0.727117	136.909021	4.051341
1.138759	127.562926	4.056346
1.405384	132.418965	4.061350
1.149121	129.868017	4.066355
1.257425	132.024789	4.071360
1.055002	132.815782	4.076365
1.502793	131.971159	4.081370
0.959197	137.848667	4.086374
0.904737	129.046528	4.091379
1.378663	124.369801	4.096384
1.038274	137.046025	4.101389
1.103827	124.615458	4.106394
0.939074	127.649951	4.111398
0.999751	129.472462	4.116403
1.235897	136.348504	4.121408
1.144257	138.681936	4.126413
1.031667	123.975956	4.131418
1.203425	142.605555	4.136422
1.226304	146.297355	4.141427
1.758457	153.117824	4.146432
1.278187	142.075661	4.151437
1.240993	134.533135	4.156442
0.878232	138.803817	4.161446
1.594411	140.846964	4.166451
1.339165	141.405742	4.171456
1.316060	144.051199	4.176461
1.238979	132.054112	4.181466
1.275611	140.603162	4.186470
1.630835	140.146264	4.191475
1.609776	135.698458	4.196480
1.555945	142.357066	4.201485
1.520696	129.423348	4.206490
1.175954	143.090482	4.211494
1.269209	139.982090	4.216499
1.327044	138.059261	4.221504
1.545967	153.875356	4.226509
1.956302	144.788877	4.231514
1.914645	134.599055	4.236518
1.537484	137.875423	4.241523
1.531752	128.062815	4.246528
1.330687	133.637061	4.251533
1.459817	139.150406	4.256538
1.199107	137.349939	4.261542
1.179217	142.566957	4.266547
1.565670	143.734487	4.271552
1.879386	154.711228	4.276557
1.733141	153.092249	4.281562
1.722542	146.798391	4.286566
1.557866	144.106634	4.291571
1.637659	142.417661	4.296576
1.798169	148.824606	4.301581
1.882372	137.245318	4.306586
1.732785	134.807470	4.311590
1.389734	143.162543	4.316595
1.440227	146.065453	4.321600
1.726975	158.254917	4.326605
2.147299	156.408523	4.331610
1.376514	161.438746	4.336614
1.361509	156.455331	4.341619
1.743592	153.077347	4.346624
1.854036	162.314086	4.351629
1.906598	159.363883	4.356634
2.132368	165.773328	4.361638
2.274455	164.232838	4.366643
1.779011	149.244769	4.371648
1.536004	146.115967	4.376653
1.723235	143.230218	4.381658
2.062796	156.528233	4.386662
2.124085	156.699216	4.391667
1.905165	149.545636	4.396672
1.633173	152.090644	4.401677
2.044897	145.797469	4.406682
2.144928	160.429886	4.411686
1.709601	155.515078	4.416691
2.032559	150.795412	4.421696
2.179622	161.165371	4.426701
1.849424	144.025590	4.431706
1.785785	150.796457	4.436710
2.331439	150.120089	4.441715
2.068261	149.610782	4.446720
1.834743	140.792225	4.451725
2.136581	143.377598	4.456730
2.232586	160.487795	4.461734
1.728186	156.339859	4.466739
1.707498	151.363658	4.471744
1.799482	164.728699	4.476749
1.806194	162.605026	4.481754
1.890482	165.214783	4.486758
1.866473	156.806512	4.491763
2.119493	163.369897	4.496768
2.053489	152.794723	4.501773
1.615147	155.409923	4.506778
2.024417	170.528861	4.511782
1.881961	169.902683	4.516787
2.661163	178.573412	4.521792
2.466200	177.300528	4.526797
2.099211	162.801799	4.531802
1.928365	163.875771	4.536806
2.242647	172.865649	4.541811
2.364402	179.199547	4.546816
2.334332	185.914582	4.551821
2.580761	178.653737	4.556826
2.328852	171.467321	4.561830
2.446248	162.726991	4.566835
2.268263	156.860977	4.571840
2.083190	172.028163	4.576845
2.164921	163.249094	4.581850
2.329182	184.230514	4.586854
2.494796	184.075213	4.591859
2.462434	187.443436	4.596864
2.116533	181.992690	4.601869
2.788317	181.961056	4.606874
2.523801	183.698166	4.611878
2.605071	187.200553	4.616883
2.529346	186.636749	4.621888
2.102532	176.911822	4.626893
2.638321	180.321294	4.631898
2.669795	173.897493	4.636902
2.431060	176.794821	4.641907
2.564543	176.818525	4.646912
2.648601	180.102183	4.651917
2.566124	179.754561	4.656922
2.416778	178.335373	4.661926
2.422156	180.593596	4.666931
2.502940	186.139793	4.671936
2.596739	184.945333	4.676941
3.039477	180.498068	4.681946
2.807081	182.075157	4.686950
2.580905	174.859424	4.691955
2.348431	167.378925	4.696960
2.129354	170.826834	4.701965
2.524508	180.958866	4.706970
2.793812	180.673529	4.711974
2.508245	178.003753	4.716979
2.790549	176.153537	4.721984
2.814382	184.581217	4.726989
2.637593	181.679374	4.731994
2.660833	178.648314	4.736998
2.885536	186.551187	4.742003
3.072493	184.861344	4.747008
2.853130	185.449337	4.752013
2.993201	182.798709	4.757018
2.703844	184.280266	4.762022
2.861022	189.422274	4.767027
2.825442	188.725673	4.772032
2.723326	188.004631	4.777037
3.037625	181.960724	4.782042
2.811258	180.268798	4.787046
2.715732	183.513979	4.792051
2.895278	177.570147	4.797056
2.721928	184.937060	4.802061
2.831647	183.407936	4.807066
2.908175	188.464426	4.812070
2.621508	184.994410	4.817075
2.558420	178.873224	4.822080
2.332757	190.778669	4.827085
3.024243	183.062560	4.832090
2.932390	187.964937	4.837094
2.670907	193.279695	4.842099
3.156774	209.307371	4.847104
3.314169	212.301213	4.852109
3.321219	198.357973	4.857114
2.919627	196.481360	4.862118
3.052788	184.075025	4.867123
3.119236	175.428041	4.872128
3.058325	187.671655	4.877133
3.280543	190.044811	4.882138
3.178556	188.637230	4.887142
3.160585	186.156738	4.892147
3.062609	184.871917	4.897152
2.992560	190.315052	4.902157
3.349778	197.665801	4.907162
3.405027	191.485058	4.912166
3.363995	193.332903	4.917171
3.391605	182.847537	4.922176
2.947004	193.477310	4.927181
2.857753	196.174201	4.932186
3.159889	196.022954	4.937190
3.232009	204.538036	4.942195
3.401280	203.284369	4.947200
3.382792	209.124433	4.952205
3.713281	204.564928	4.957210
3.318587	204.322863	4.962214
3.025095	190.711154	4.967219
3.176869	192.731454	4.972224
3.124804	203.357063	4.977229
3.467728	217.863126	4.982234
3.965315	220.955859	4.987238
3.639696	205.798936	4.992243
3.460696	190.388248	4.997248
3.268131	187.102892	5.002253
3.025385	187.735654	5.007258
3.247382	196.334962	5.012262
3.247664	203.643212	5.017267
4.050587	201.746735	5.022272
3.488462	196.658673	5.027277
3.347031	187.123418	5.032282
3.562017	187.457128	5.037286
3.623264	191.785189	5.042291
3.745969	184.002617	5.047296
3.238432	190.621154	5.052301
3.321108	193.240657	5.057306
3.591225	195.188750	5.062310
3.695934	200.680608	5.067315
3.661536	200.834852	5.072320
3.522385	200.670056	5.077325
3.483511	196.272463	5.082330
3.884510	208.222716	5.087334
3.400279	205.305463	5.092339
3.741793	194.771217	5.097344
3.644509	201.316393	5.102349
3.771228	199.009519	5.107354
3.919555	200.422931	5.112358
3.103449	194.064650	5.117363
3.796390	197.376894	5.122368
3.859269	199.297143	5.127373
3.713926	207.659428	5.132378
4.154689	203.949603	5.137382
3.698332	196.080017	5.142387
3.679448	192.853037	5.147392
3.352453	204.666703	5.152397
3.696016	202.465269	5.157402
3.838882	208.799054	5.162406
3.472207	207.385228	5.167411
3.675852	200.823882	5.172416
3.531414	201.159770	5.177421
3.567141	199.945878	5.182426
3.655288	197.626027	5.187430
3.541257	198.659518	5.192435
3.830786	200.791246	5.197440
3.695491	207.918132	5.202445
3.949462	219.442042	5.207450
4.077677	225.072613	5.212454
4.290848	226.466440	5.217459
4.197160	209.530212	5.222464
4.021392	219.801776	5.227469
3.774166	211.817367	5.232474
3.796526	204.547106	5.237478
3.767911	216.067556	5.242483
4.035331	218.696263	5.247488
4.031426	226.017830	5.252493
4.146992	225.228094	5.257498
3.836732	226.504105	5.262502
3.812224	226.808666	5.267507
3.593712	230.196389	5.272512
3.944121	234.662933	5.277517
3.778562	234.160570	5.282522
4.353489	226.174695	5.287526
4.019749	231.329876	5.292531
4.285375	234.547310	5.297536
4.242257	231.994798	5.302541
4.389196	220.753692	5.307546
4.823008	225.805184	5.312550
4.052214	236.191547	5.317555
4.567758	223.735140	5.322560
4.321466	227.168315	5.327565
4.560777	220.433733	5.332570
4.412158	228.916759	5.337574
4.183133	222.463897	5.342579
4.099724	217.336095	5.347584
4.282853	214.729377	5.352589
4.517263	221.010950	5.357594
4.211701	219.318695	5.362598
4.147751	230.781382	5.367603
4.374427	224.668848	5.372608
4.553146	233.455242	5.377613
4.274988	235.251428	5.382618
4.597028	229.804236	5.387622
4.291344	234.357113	5.392627
4.437460	228.190683	5.397632
4.424314	234.922083	5.402637
4.401085	232.239927	5.407642
4.382575	223.337234	5.412646
4.182380	229.737095	5.417651
4.757791	225.500111	5.422656
4.154044	219.852223	5.427661
4.075804	232.032128	5.432666
4.389895	222.764446	5.437670
4.256806	226.977244	5.442675
4.714607	223.486219	5.447680
4.160473	228.134724	5.452685
4.432348	223.783652	5.457690
4.209640	226.343142	5.462694
4.302167	236.696327	5.467699
4.640980	224.707188	5.472704
4.549313	229.663331	5.477709
4.502820	223.144085	5.482714
4.331527	232.181123	5.487718
4.404032	239.712256	5.492723
4.953526	244.230062	5.497728
4.626254	249.093181	5.502733
4.980152	256.659602	5.507738
5.108315	243.105585	5.512742
4.377885	242.419094	5.517747
4.439069	236.800548	5.522752
5.135083	237.404206	5.527757
4.780406	236.637065	5.532762
4.807168	229.562258	5.537766
4.422152	232.463388	5.542771
5.040596	230.677886	5.547776
4.749187	231.542848	5.552781
4.966316	237.023541	5.557786
4.762478	234.635254	5.562790
4.528772	231.758083	5.567795
5.147567	246.629333	5.572800
4.740607	242.836356	5.577805
4.839541	246.592264	5.582810
4.948971	242.212697	5.587814
4.682873	239.821448	5.592819
5.243764	245.552335	5.597824
4.695663	243.701692	5.602829
4.898856	238.690608	5.607834
5.262698	233.012286	5.612838
4.796854	241.538380	5.617843
5.338238	240.846856	5.622848
4.715254	234.018740	5.627853
4.622632	228.240650	5.632858
5.187647	245.439254	5.637862
5.273213	246.995316	5.642867
5.013401	238.889470	5.647872
4.981483	246.727924	5.652877
5.029227	238.197714	5.657882
4.890594	248.140816	5.662886
5.467353	251.284502	5.667891
4.946513	237.347493	5.672896
4.972055	243.430644	5.677901
4.877044	241.572730	5.682906
5.402854	240.307840	5.687910
5.096729	248.527502	5.692915
5.445750	246.344195	5.697920
5.237592	239.305960	5.702925
4.804306	238.655460	5.707930
5.259638	246.750238	5.712934
4.911426	240.768334	5.717939
4.825999	239.032312	5.722944
5.538469	253.449231	5.727949
5.277008	246.498385	5.732954
5.183563	244.507352	5.737958
5.402914	255.403937	5.742963
5.515250	256.788157	5.747968
5.163366	254.720304	5.752973
5.359211	251.760432	5.757978
5.391245	244.643670	5.762982
5.230553	253.052658	5.767987
5.461783	252.836521	5.772992
5.301458	248.723575	5.777997
5.242931	253.196847	5.783002
5.602367	255.048784	5.788006
5.258215	254.232549	5.793011
5.496020	251.797643	5.798016
5.613952	254.421157	5.803021
5.483690	253.622239	5.808026
5.218112	245.045898	5.813030
5.471465	258.452323	5.818035
5.578429	248.074784	5.823040
5.449296	258.734571	5.828045
5.781984	250.856002	5.833050
5.850037	250.146427	5.838054
5.112685	245.936664	5.843059
5.139292	249.033131	5.848064
5.510355	245.846667	5.853069
5.567429	251.662325	5.858074
5.668952	251.311363	5.863078
5.468269	248.612542	5.868083
5.456810	245.539417	5.873088
5.464178	251.533654	5.878093
5.151487	257.881439	5.883098
5.584645	244.526703	5.888102
5.711960	261.176551	5.893107
5.875378	257.487751	5.898112
5.660949	257.204963	5.903117
5.271597	261.916404	5.908122
5.600231	247.141624	5.913126
5.283239	253.303420	5.918131
5.569203	240.066515	5.923136
5.578463	255.352208	5.928141
5.752128	259.245176	5.933146
5.812418	269.132009	5.938150
5.339766	259.765342	5.943155
5.758734	269.004720	5.948160
5.988031	269.655736	5.953165
5.947762	269.333177	5.958170
6.316186	260.927030	5.963174
5.884655	262.332655	5.968179
5.747789	245.165839	5.973184
5.691573	249.303400	5.978189
5.675912	252.276737	5.983194
5.829350	258.687986	5.988198
5.906531	268.442478	5.993203
5.883040	269.926939	5.998208
5.834367	267.982715	6.003213
5.998923	276.375874	6.008218
6.074161	265.797625	6.013222
5.727074	268.708674	6.018227
6.129221	264.868810	6.023232
5.901026	249.892828	6.028237
5.784085	254.814948	6.033242
5.619974	253.559401	6.038246
5.520455	261.788030	6.043251
5.879764	269.037244	6.048256
5.900268	270.834388	6.053261
5.869716	276.369475	6.058266
6.296097	277.214428	6.063270
5.761966	277.212366	6.068275
5.903472	276.839360	6.073280
6.102699	277.618442	6.078285
6.034785	275.360844	6.083290
6.100251	259.677921	6.088294
5.553092	259.798108	6.093299
6.285883	264.012138	6.098304
5.888032	265.788999	6.103309
5.359840	260.338137	6.108314
5.743538	259.316831	6.113318
5.722984	272.718458	6.118323
6.231095	264.632239	6.123328
6.546880	270.413951	6.128333
6.016793	257.819771	6.133338
5.813338	253.593319	6.138342
5.639104	255.221469	6.143347
5.974005	250.417661	6.148352
6.178306	249.193337	6.153357
5.900269	244.098994	6.158362
5.887730	253.902247	6.163366
5.715604	259.459371	6.168371
6.005246	250.011987	6.173376
5.798869	247.342525	6.178381
5.769399	248.783624	6.183386
5.940622	249.203240	6.188390
5.968670	259.060287	6.193395
5.807619	251.682525	6.198400
5.924696	257.302186	6.203405
5.709233	253.087095	6.208410
5.782163	250.981573	6.213414
5.574071	254.956124	6.218419
6.106974	258.369226	6.223424
6.458018	270.362099	6.228429
5.977793	267.352465	6.233434
6.061768	253.659790	6.238438
6.251020	258.527911	6.243443
5.996756	260.541837	6.248448
6.324094	260.149389	6.253453
5.756994	260.500466	6.258458
5.908508	255.541716	6.263462
5.861819	270.418526	6.268467
5.945499	254.742262	6.273472
5.241921	261.644444	6.278477
5.053685	252.056332	6.283482
5.946361	259.273118	6.288486
5.841598	258.270917	6.293491
6.014740	257.851857	6.298496
6.274155	248.633802	6.303501
5.746567	259.978874	6.308506
5.559605	258.986307	6.313510
5.476633	261.340552	6.318515
5.617852	272.901033	6.323520
5.992050	288.522233	6.328525
6.071966	284.447802	6.333530
6.180297	286.769101	6.338534
6.036039	279.670282	6.343539
5.902077	268.909471	6.348544
5.799686	261.449808	6.353549
5.700926	259.801279	6.358554
6.210057	265.964166	6.363558
6.111235	264.439030	6.368563
5.892321	261.553224	6.373568
6.193693	256.080769	6.378573
5.909462	264.875985	6.383578
6.097987	250.407749	6.388582
6.053985	259.481929	6.393587
6.149457	256.873034	6.398592
5.762725	261.058894	6.403597
5.935294	266.929341	6.408602
5.890230	258.837505	6.413606
5.984565	260.645299	6.418611
5.835132	260.681415	6.423616
5.983242	258.459786	6.428621
5.793013	262.286028	6.433626
6.140627	259.919444	6.438630
6.006674	255.141178	6.443635
5.884587	250.209210	6.448640
5.849332	249.718196	6.453645
5.572691	255.123916	6.458650
5.974591	254.561674	6.463654
5.697577	251.710225	6.468659
5.791004	251.904677	6.473664
5.949340	250.877332	6.478669
5.844821	252.175094	6.483674
6.166527	243.969214	6.488678
5.662183	248.261966	6.493683
6.069183	249.290266	6.498688
6.033618	244.060096	6.503693
6.201749	247.447733	6.508698
6.183508	248.507440	6.513702
5.810000	248.964415	6.518707
6.020184	250.548530	6.523712
5.881732	242.123236	6.528717
6.010774	253.818476	6.533722
6.000582	248.211040	6.538726
5.719598	264.873843	6.543731
5.779626	256.208837	6.548736
6.062676	245.370458	6.553741
5.837319	254.083738	6.558746
6.118834	242.672972	6.563750
5.901673	245.282220	6.568755
6.237277	245.075143	6.573760
5.712500	235.150305	6.578765
5.672195	235.330778	6.583770
6.108795	228.809080	6.588774
5.813819	242.591925	6.593779
5.635159	234.641121	6.598784
6.132351	232.532820	6.603789
5.781493	238.484753	6.608794
5.865178	232.657065	6.613798
5.574142	246.705049	6.618803
5.856283	245.402169	6.623808
6.162328	244.943435	6.628813
5.889538	260.219264	6.633818
5.855712	241.438745	6.638822
5.685314	249.754332	6.643827
6.095071	243.553176	6.648832
5.810076	248.090180	6.653837
5.657689	257.035704	6.658842
6.159280	250.200164	6.663846
5.858613	256.074687	6.668851
6.024174	251.958456	6.673856
6.248897	245.896838	6.678861
5.591448	242.196644	6.683866
6.025198	237.731782	6.688870
5.609155	233.456178	6.693875
5.402879	249.446125	6.698880
6.263453	248.211369	6.703885
5.883835	260.887461	6.708890
6.166198	258.711367	6.713894
5.901076	254.795066	6.718899
6.150098	245.357172	6.723904
5.967482	233.316338	6.728909
5.534581	235.965502	6.733914
5.775212	228.522046	6.738918
5.678780	246.222260	6.743923
6.063432	245.434918	6.748928
5.701765	257.146452	6.753933
5.551493	258.002095	6.758938
5.914912	256.601139	6.763942
5.579337	262.209022	6.768947
5.937806	253.133727	6.773952
6.009753	260.282149	6.778957
5.994547	252.271088	6.783962
6.184603	245.243615	6.788966
5.907198	264.392519	6.793971
5.623425	256.198649	6.798976
5.831400	252.553531	6.803981
5.614493	266.014197	6.808986
6.030792	262.374606	6.813990
5.868408	260.878350	6.818995
5.831127	255.651607	6.824000
6.173893	257.623197	6.829005
5.803357	257.494426	6.834010
6.437765	258.936563	6.839014
6.273164	262.088112	6.844019
5.621641	253.394691	6.849024
5.734053	252.054963	6.854029
5.840822	257.499062	6.859034
6.274172	257.479242	6.864038
5.938798	250.467137	6.869043
5.919309	242.662386	6.874048
5.771428	238.737326	6.879053
5.596111	251.748590	6.884058
5.962008	251.821528	6.889062
6.053111	261.165732	6.894067
6.084818	250.847365	6.899072
5.996540	238.950022	6.904077
5.280922	241.212944	6.909082
5.857256	243.277877	6.914086
5.610036	251.352331	6.919091
5.716291	261.896378	6.924096
5.771051	259.053381	6.929101
5.795115	251.374721	6.934106
5.822109	256.483235	6.939110
5.677919	264.035462	6.944115
5.653736	263.476286	6.949120
5.809182	263.085291	6.954125
5.645158	271.728920	6.959130
6.013285	254.910567	6.964134
5.943451	261.423018	6.969139
5.985633	270.018721	6.974144
5.993518	261.905986	6.979149
6.250720	266.114972	6.984154
6.612288	249.772199	6.989158
6.250953	257.816968	6.994163
6.229029	251.024973	6.999168
5.857036	242.664514	7.004173
5.499526	245.203867	7.009178
5.874481	248.809234	7.014182
6.053496	254.431905	7.019187
5.876673	246.879435	7.024192
5.971071	245.346363	7.029197
5.697452	247.708143	7.034202
6.067038	246.404303	7.039206
5.569618	249.281809	7.044211
5.800180	251.258212	7.049216
5.958479	254.163337	7.054221
6.022799	262.205108	7.059226
6.016652	257.938443	7.064230
5.872663	255.015663	7.069235
5.685134	255.158949	7.074240
5.654599	264.730897	7.079245
5.711684	259.166764	7.084250
5.988545	256.849161	7.089254
5.814478	261.786505	7.094259
5.793124	256.427571	7.099264
6.064640	272.302020	7.104269
6.015748	256.219298	7.109274
5.801857	257.002590	7.114278
5.729520	262.949130	7.119283
5.852988	254.929131	7.124288
6.020349	259.000247	7.129293
6.045035	262.508295	7.134298
6.291046	260.594120	7.139302
5.921037	258.766365	7.144307
5.661960	252.191624	7.149312
5.628444	252.079982	7.154317
5.734780	263.750291	7.159322
6.074707	262.824382	7.164326
5.945718	261.623477	7.169331
5.591464	262.580480	7.174336
5.963006	261.864780	7.179341
5.819369	256.524886	7.184346
5.938176	256.968482	7.189350
5.730958	264.340702	7.194355
5.556127	263.089987	7.199360
6.278751	262.775196	7.204365
6.016447	266.511423	7.209370
5.729667	256.185693	7.214374
5.691651	261.430877	7.219379
5.455202	254.609008	7.224384
5.868807	257.642059	7.229389
5.855283	264.484258	7.234394
6.263797	252.838582	7.239398
6.420606	258.509003	7.244403
6.017962	253.582751	7.249408
6.264818	248.049186	7.254413
5.727248	261.784397	7.259418
6.339265	255.709931	7.264422
5.931675	251.246348	7.269427
5.605168	242.359962	7.274432
5.859099	239.394212	7.279437
5.777909	250.185731	7.284442
5.934432	256.213693	7.289446
6.010410	264.516236	7.294451
6.120801	251.787540	7.299456
5.760987	235.572915	7.304461
5.365131	240.434056	7.309466
5.913756	243.692849	7.314470
5.777680	261.380268	7.319475
6.003572	264.338144	7.324480
6.308177	257.973025	7.329485
5.711675	255.617399	7.334490
5.999490	250.036327	7.339494
5.949796	256.991721	7.344499
5.708672	257.374301	7.349504
5.555483	258.708115	7.354509
5.839335	264.055044	7.359514
5.689618	261.658327	7.364518
5.403830	262.424340	7.369523
5.615554	257.712473	7.374528
5.906406	258.274813	7.379533
5.989469	262.694406	7.384538
5.921778	261.920545	7.389542
5.811320	264.807406	7.394547
5.686346	258.790739	7.399552
6.163029	252.262791	7.404557
5.768800	253.653116	7.409562
6.157882	251.507862	7.414566
5.813878	257.683356	7.419571
5.783797	262.920978	7.424576
5.905454	255.521344	7.429581
5.417812	257.489350	7.434586
5.785008	257.321646	7.439590
5.918345	260.211676	7.444595
5.623596	256.610029	7.449600
5.657182	253.248321	7.454605
5.610026	264.129460	7.459610
5.971781	260.697674	7.464614
6.128381	265.286148	7.469619
5.781910	261.822265	7.474624
5.926161	258.531909	7.479629
5.754694	258.913135	7.484634
5.582585	263.150999	7.489638
5.890040	281.088914	7.494643
6.076000	278.608294	7.499648
6.480008	267.403063	7.504653
5.731204	273.021505	7.509658
5.893235	270.177623	7.514662
5.721613	271.511144	7.519667
5.604081	262.614358	7.524672
5.847252	266.806547	7.529677
5.878181	272.831924	7.534682
6.211570	274.909377	7.539686
6.034846	265.015751	7.544691
5.959764	261.876601	7.549696
5.971811	255.943002	7.554701
5.824909	266.561268	7.559706
5.975198	257.410818	7.564710
6.092323	270.648642	7.569715
5.964670	268.061831	7.574720
6.104521	268.426222	7.579725
5.863389	262.823100	7.584730
5.561629	258.668899	7.589734
5.528483	250.530920	7.594739
5.720370	264.703041	7.599744
6.065100	258.673353	7.604749
6.199465	263.151396	7.609754
6.402764	257.286094	7.614758
6.166390	254.599156	7.619763
6.072421	260.729394	7.624768
6.287304	253.128588	7.629773
6.114829	252.095802	7.634778
6.122982	251.376571	7.639782
6.211427	261.322290	7.644787
5.839015	255.730119	7.649792
5.905356	248.797835	7.654797
5.767960	248.550510	7.659802
5.797664	244.809766	7.664806
6.026758	257.223405	7.669811
6.094125	256.172259	7.674816
5.585926	249.743872	7.679821
5.500017	259.473132	7.684826
6.040279	262.097329	7.689830
5.878922	255.975598	7.694835
6.003937	254.077098	7.699840
5.938372	266.198107	7.704845
5.986017	264.938063	7.709850
6.058762	261.918263	7.714854
5.753923	254.705253	7.719859
5.343664	260.296290	7.724864
5.988527	265.900217	7.729869
6.009384	268.064294	7.734874
5.975588	267.013078	7.739878
5.770757	264.251626	7.744883
5.959835	256.822512	7.749888
5.990981	254.055958	7.754893
5.641332	264.449531	7.759898
5.992133	260.636644	7.764902
6.062777	271.676614	7.769907
6.136914	265.442285	7.774912
6.256640	249.260551	7.779917
6.093266	240.313966	7.784922
6.106661	239.612902	7.789926
6.122747	242.960937	7.794931
5.773673	235.916170	7.799936
6.173414	234.313413	7.804941
5.700431	239.113797	7.809946
5.501581	239.179753	7.814950
5.886778	237.943084	7.819955
5.579194	236.864897	7.824960
5.737204	234.559474	7.829965
5.576548	245.898026	7.834970
5.598343	252.402534	7.839974
5.853395	250.834957	7.844979
5.805495	265.990357	7.849984
6.193210	251.361396	7.854989
6.025728	264.991533	7.859994
5.791050	256.983003	7.864998
6.140477	253.132368	7.870003
6.070222	254.057808	7.875008
5.885225	239.919814	7.880013
5.543803	239.432177	7.885018
5.998882	245.676238	7.890022
6.182722	257.723609	7.895027
5.872500	250.131796	7.900032
5.882893	241.075901	7.905037
5.190882	238.134047	7.910042
5.796642	250.359325	7.915046
6.056083	259.304003	7.920051
6.110759	264.987165	7.925056
6.077029	257.374447	7.930061
6.011608	253.990190	7.935066
5.914566	242.261885	7.940070
5.641178	244.161731	7.945075
5.593569	251.876082	7.950080
6.188485	265.428645	7.955085
6.077086	262.696938	7.960090
5.957098	256.780733	7.965094
5.854895	240.159007	7.970099
5.751234	244.025549	7.975104
6.048979	241.518039	7.980109
5.495362	245.771006	7.985114
6.146080	254.882547	7.990118
6.008881	257.109608	7.995136
5.638736	253.614208	8.000154
5.432176	256.231016	8.005171
5.560416	264.150784	8.010189
5.980412	263.198859	8.015206
5.855233	267.024223	8.020224
5.899127	268.122052	8.025242
6.072240	264.753493	8.030259
6.085117	271.447912	8.035277
6.134596	263.087477	8.040294
5.924508	266.774591	8.045312
5.819301	268.495203	8.050330
6.201426	260.338582	8.055347
6.536000	261.132392	8.060365
5.996647	256.568337	8.065382
5.792217	248.512514	8.070400
5.370251	255.880508	8.075418
6.073797	261.826798	8.080435
6.112348	265.273240	8.085453
6.312908	261.739471	8.090470
6.355188	263.074223	8.095488
6.047799	256.347164	8.100506
5.741794	243.860891	8.105523
5.635598	244.780128	8.110541
6.088725	260.083945	8.115558
6.199674	262.395713	8.120576
5.844638	263.741836	8.125594
6.380714	256.596291	8.130611
5.823138	258.551426	8.135629
5.768442	260.794317	8.140646
5.956464	267.369951	8.145664
6.201490	270.676956	8.150682
6.390455	271.733264	8.155699
6.136240	268.327103	8.160717
5.728703	258.381125	8.165734
6.193800	262.786731	8.170752
6.114757	273.960664	8.175770
6.416420	265.538875	8.180787
6.037854	259.643358	8.185805
5.681244	252.381198	8.190822
5.946936	259.462257	8.195840
5.858369	271.511778	8.200858
6.185256	260.956019	8.205875
6.153270	262.460115	8.210893
6.142367	260.918911	8.215910
6.273612	263.255920	8.220928
5.895355	264.012402	8.225946
6.555491	258.870293	8.230963
5.825349	262.625754	8.235981
6.049757	264.411804	8.240998
6.596694	254.784251	8.246016
6.164336	254.927499	8.251034
6.436266	260.224663	8.256051
6.119879	252.681702	8.261069
5.623893	254.166527	8.266086
5.664091	258.168100	8.271104
5.889606	264.794697	8.276122
5.932735	262.292083	8.281139
5.775070	261.609968	8.286157
6.347195	266.595323	8.291174
6.363005	265.927222	8.296192
6.136133	268.764932	8.301210
6.287930	270.615933	8.306227
6.172512	269.883061	8.311245
6.168676	262.758464	8.316262
6.479361	264.512147	8.321280
5.971587	270.546057	8.326298
6.363451	274.978847	8.331315
5.766718	266.955694	8.336333
5.839033	265.085971	8.341350
5.777825	271.801391	8.346368
6.356444	285.391122	8.351386
6.574549	289.522784	8.356403
6.220127	290.922458	8.361421
6.887272	296.776603	8.366438
6.750858	270.906147	8.371456
6.583955	270.313828	8.376474
6.489083	268.892988	8.381491
6.446297	271.260250	8.386509
6.394494	268.144447	8.391526
6.491974	273.664426	8.396544
6.309444	273.326989	8.401562
6.234071	260.486078	8.406579
6.241578	262.315365	8.411597
6.367633	274.820594	8.416614
6.287169	263.823357	8.421632
6.318945	269.918420	8.426650
6.114974	265.860689	8.431667
6.291492	266.799022	8.436685
6.643947	262.402209	8.441702
6.597586	254.173458	8.446720
6.337065	264.447889	8.451738
6.403304	267.034847	8.456755
6.198437	267.120586	8.461773
6.501540	263.088042	8.466790
6.513972	262.975856	8.471808
6.529493	263.955033	8.476826
6.611577	268.628545	8.481843
6.170451	262.793258	8.486861
6.189046	268.312894	8.491878
6.676127	261.888146	8.496896
6.349759	267.893812	8.501914
6.557272	268.196194	8.506931
6.459023	273.958074	8.511949
6.261976	265.670733	8.516966
6.257133	262.913671	8.521984
6.644997	272.355052	8.527002
6.416447	264.864677	8.532019
6.664086	267.006850	8.537037
6.482310	269.225349	8.542054
6.424462	265.586654	8.547072
6.350655	272.487062	8.552090
6.584114	273.489109	8.557107
6.584378	268.213066	8.562125
6.697792	269.656656	8.567143
6.811543	264.867843	8.572160
6.482196	267.424880	8.577178
6.462172	265.525355	8.582195
6.533278	263.081497	8.587213
6.325967	267.841090	8.592231
6.607775	261.931112	8.597248
6.302875	261.129918	8.602266
6.524985	257.892579	8.607283
6.729989	263.001361	8.612301
6.319462	275.706892	8.617319
5.942353	269.890036	8.622336
5.887149	265.026549	8.627354
6.063889	262.099212	8.632371
6.201960	256.129569	8.637389
6.163261	282.175974	8.642407
6.413984	284.989817	8.647424
6.467640	292.861253	8.652442
6.293947	284.898452	8.657459
6.474812	297.666547	8.662477
6.459103	294.191689	8.667495
6.646982	288.870650	8.672512
6.358208	298.572021	8.677530
6.750346	289.205224	8.682547
6.912133	299.082582	8.687565
6.488420	299.678894	8.692583
6.814723	292.644887	8.697600
6.635173	291.906221	8.702618
6.276068	290.059487	8.707635
6.446868	285.331210	8.712653
6.401770	292.747834	8.717671
6.547293	272.302179	8.722688
6.375672	289.912228	8.727706
6.776029	297.029137	8.732723
6.961469	300.004617	8.737741
7.026051	300.988780	8.742759
6.770639	289.501243	8.747776
6.898680	295.682307	8.752794
6.476384	288.739610	8.757811
6.705630	289.190080	8.762829
6.635077	295.140147	8.767847
6.803602	284.274534	8.772864
6.665862	282.648940	8.777882
6.743557	292.892818	8.782899
6.688449	286.126469	8.787917
6.475569	284.493640	8.792935
6.880013	281.726497	8.797952
7.111859	284.458077	8.802970
6.748103	289.131586	8.807987
6.792813	284.751127	8.813005
6.880366	290.244255	8.818023
7.024376	288.003625	8.823040
6.815586	291.018395	8.828058
6.515149	291.122169	8.833075
6.674677	277.941733	8.838093
6.557595	284.811016	8.843111
6.648086	284.642497	8.848128
7.091888	293.374631	8.853146
7.013482	295.577039	8.858163
7.035695	285.737694	8.863181
6.769173	287.492891	8.868199
7.058842	287.668880	8.873216
7.037575	288.041596	8.878234
7.127097	295.582420	8.883251
6.999217	287.918580	8.888269
7.194515	289.993170	8.893287
7.385650	283.078036	8.898304
7.080988	295.050771	8.903322
7.130832	282.755206	8.908339
6.972063	281.928103	8.913357
6.948254	292.301387	8.918375
7.057486	291.634517	8.923392
7.135075	288.195625	8.928410
6.636089	272.801493	8.933427
6.692361	273.730147	8.938445
6.737980	281.000106	8.943463
6.666398	287.726614	8.948480
6.600487	292.943853	8.953498
6.871794	291.576445	8.958515
7.067555	286.525563	8.963533
6.944428	293.727131	8.968551
6.991758	288.809806	8.973568
6.735611	292.687123	8.978586
6.881180	291.604365	8.983603
7.203284	290.402607	8.988621
6.891362	292.313187	8.993639
6.841703	282.772197	8.998656
6.615744	290.194890	9.003674
7.024172	299.554192	9.008691
7.196351	285.229444	9.013709
6.994059	292.134086	9.018727
6.750188	292.197497	9.023744
6.806582	295.660101	9.028762
6.760293	298.832597	9.033779
7.441777	305.514441	9.038797
6.918014	299.480581	9.043815
6.740370	291.938090	9.048832
7.468493	294.488268	9.053850
6.887610	305.424793	9.058867
6.963864	301.449649	9.063885
7.180153	308.573132	9.068903
7.055037	307.352647	9.073920
7.119723	295.515483	9.078938
7.139352	308.160375	9.083955
7.134318	303.431069	9.088973
6.716393	299.078458	9.093991
7.395444	303.141511	9.099008
7.578725	309.156197	9.104026
7.110667	300.740631	9.109043
7.356391	292.605233	9.114061
7.330996	283.063620	9.119079
7.255819	295.057427	9.124096
7.191471	292.445317	9.129114
7.207829	289.186362	9.134131
6.979754	283.523012	9.139149
7.171464	291.063702	9.144167
6.946564	294.229294	9.149184
7.079339	288.377223	9.154202
6.668723	293.777512	9.159219
7.245870	310.314845	9.164237
7.070578	317.306807	9.169255
6.930633	315.388080	9.174272
7.443266	307.460413	9.179290
7.290970	316.989074	9.184307
7.512899	313.048048	9.189325
7.390566	316.522705	9.194343
7.575523	307.853993	9.199360
7.340044	302.674601	9.204378
6.980543	298.625300	9.209395
7.106914	294.251057	9.214413
7.417051	302.660044	9.219431
7.236588	309.305688	9.224448
7.477894	312.146247	9.229466
7.183260	304.704011	9.234483
7.338317	304.954605	9.239501
7.183503	306.906994	9.244519
7.638463	313.207567	9.249536
7.205442	300.564316	9.254554
6.934037	308.663085	9.259571
7.304585	312.761550	9.264589
7.209406	312.593539	9.269607
6.966627	312.183436	9.274624
7.020261	321.380252	9.279642
7.156986	321.523253	9.284659
7.715823	311.619278	9.289677
7.327641	319.606853	9.294695
7.346716	316.685122	9.299712
7.406242	310.891782	9.304730
7.304868	313.280795	9.309747
7.269211	315.713221	9.314765
7.312990	308.489679	9.319783
7.201331	316.484689	9.324800
7.405565	312.660021	9.329818
7.207478	319.706022	9.334835
6.975135	306.334127	9.339853
7.194186	325.890364	9.344871
7.753368	341.161959	9.349888
7.825712	323.201657	9.354906
7.060715	325.469945	9.359923
7.129069	312.922182	9.364941
7.343262	324.025246	9.369959
7.621663	336.263814	9.374976
7.849453	339.412578	9.379994
7.396343	334.450087	9.385011
7.384473	326.291668	9.390029
7.480605	331.944411	9.395047
7.720232	336.432475	9.400064
7.828644	327.144545	9.405082
7.585410	329.779696	9.410099
7.730858	321.883948	9.415117
7.702958	314.144573	9.420135
7.631427	315.424469	9.425152
7.392278	306.042350	9.430170
7.532821	319.501509	9.435187
7.614128	308.627372	9.440205
7.064989	312.086433	9.445223
7.272763	316.999150	9.450240
7.695024	324.349332	9.455258
7.651784	335.533508	9.460275
7.777055	330.581947	9.465293
7.450577	335.306466	9.470311
7.595851	327.331851	9.475328
7.872873	327.150068	9.480346
7.485336	312.896665	9.485363
7.223122	318.860803	9.490381
7.648622	324.437017	9.495399
7.861957	345.164904	9.500416
8.140316	339.103967	9.505434
7.652637	325.462560	9.510451
7.533789	312.347530	9.515469
7.626807	308.622225	9.520487
7.492280	323.657850	9.525504
7.818539	325.693121	9.530522
7.634772	332.531782	9.535539
7.742342	339.678516	9.540557
7.798174	328.874601	9.545575
7.664496	327.248371	9.550592
7.638547	330.572331	9.555610
7.667334	339.438528	9.560627
7.637151	337.976054	9.565645
7.899316	335.013316	9.570663
7.846730	340.304230	9.575680
8.255524	332.903932	9.580698
7.679347	327.370501	9.585715
7.557065	318.986292	9.590733
7.810816	322.588577	9.595751
7.399154	321.955474	9.600768
7.811814	331.191065	9.605786
7.752007	341.945502	9.610803
7.891338	342.435218	9.615821
8.168293	332.982195	9.620839
7.519421	327.254967	9.625856
7.763076	334.588783	9.630874
7.954423	343.925106	9.635891
7.742144	339.805540	9.640909
8.013629	338.084670	9.645927
7.668672	350.265676	9.650944
7.952553	346.841988	9.655962
8.238140	336.586089	9.660979
7.447236	327.599116	9.665997
7.961846	326.622990	9.671015
7.588173	343.005453	9.676032
7.991837	331.967509	9.681050
8.006061	340.671881	9.686067
7.716778	332.790168	9.691085
7.920988	342.481075	9.696103
7.795397	343.706277	9.701120
8.255924	331.820081	9.706138
8.467580	338.805449	9.711155
7.809073	334.174724	9.716173
7.930400	317.014643	9.721191
7.816807	333.795236	9.726208
8.133962	326.033689	9.731226
8.030299	331.717539	9.736243
7.865139	327.423390	9.741261
7.986329	331.702688	9.746279
8.040858	335.048831	9.751296
7.881783	327.348808	9.756314
8.019994	333.714484	9.761331
8.033856	328.606709	9.766349
7.875802	327.202013	9.771367
7.973432	327.079717	9.776384
8.388008	336.548529	9.781402
8.113859	337.733749	9.786419
8.274185	330.012395	9.791437
7.940505	322.844460	9.796455
7.507552	319.898439	9.801472
7.867263	330.492883	9.806490
8.224906	329.620087	9.811507
8.173483	336.005822	9.816525
8.032303	339.335103	9.821543
7.973313	340.972791	9.826560
8.324086	332.675860	9.831578
8.396993	342.021156	9.836595
8.397544	342.156959	9.841613
8.495351	324.363095	9.846631
7.899980	323.225292	9.851648
7.893764	322.999251	9.856666
8.411830	320.671977	9.861683
7.985572	326.778417	9.866701
8.096328	320.500598	9.871719
7.996867	327.827876	9.876736
8.157961	335.032543	9.881754
7.923078	334.861038	9.886771
8.080181	338.289036	9.891789
8.147831	333.990194	9.896807
8.156886	340.420161	9.901824
7.920194	338.093640	9.906842
8.100363	339.429018	9.911859
7.809096	343.210833	9.916877
8.110050	337.708082	9.921895
8.076788	337.700834	9.926912
8.048446	333.410627	9.931930
8.239565	341.920209	9.936947
8.149135	348.075350	9.941965
8.038751	345.823831	9.946983
8.205787	351.620167	9.952000
8.573908	357.154835	9.957018
8.440364	343.287872	9.962035
8.014034	338.210764	9.967053
8.290183	351.106065	9.972071
8.322999	361.533686	9.977088
8.529051	361.129435	9.982106
8.410237	353.076012	9.987123
8.502242	344.749941	9.992141
8.347245	335.947963	9.997159
7.884249	349.261285	10.002176
7.928644	352.779414	10.007194
8.236865	363.312471	10.012211
8.426038	369.301015	10.017229
8.379753	363.700849	10.022247
8.364485	368.323276	10.027264
8.436702	360.022368	10.032282
8.908142	359.876583	10.037299
8.178106	370.246267	10.042317
8.346271	357.323189	10.047335
8.529169	362.394418	10.052352
8.493032	365.997668	10.057370
8.815984	364.388696	10.062387
8.542533	355.838668	10.067405
8.850975	352.890811	10.072423
8.327139	352.130012	10.077440
8.274716	336.571627	10.082458
8.590648	337.456701	10.087475
8.376438	344.467355	10.092493
8.553197	349.416466	10.097511
8.488377	357.580917	10.102528
8.150706	349.630995	10.107546
8.826069	359.797635	10.112563
8.586050	359.633241	10.117581
8.872831	350.412196	10.122599
8.582488	350.419730	10.127616
8.422241	336.512752	10.132634
8.526336	337.569656	10.137651
8.285261	341.015471	10.142669
8.654791	352.927455	10.147687
8.704015	368.594036	10.152704
8.652486	358.728265	10.157722
9.030439	351.443209	10.162739
8.657891	339.917075	10.167757
8.324934	327.668457	10.172775
8.273386	334.518089	10.177792
8.487679	340.291285	10.182810
8.561389	351.880117	10.187827
8.403972	355.401267	10.192845
8.672505	361.724573	10.197863
8.666987	363.735769	10.202880
8.400764	358.687373	10.207898
8.915495	355.335032	10.212915
8.233850	360.420952	10.217933
8.712975	354.098390	10.222951
8.733188	358.734225	10.227968
8.586190	362.796524	10.232986
8.733851	355.821862	10.238003
8.358164	371.952213	10.243021
8.387445	361.231303	10.248039
8.561888	369.743496	10.253056
8.466700	362.326985	10.258074
8.874086	366.722669	10.263091
8.671786	373.213955	10.268109
8.849368	370.318026	10.273127
8.905153	365.380430	10.278144
8.687067	375.010878	10.283162
8.753177	369.945448	10.288179
8.797731	371.008468	10.293197
9.092727	379.347269	10.298215
8.647516	376.968006	10.303232
8.689607	373.550403	10.308250
8.910504	380.439680	10.313267
8.853735	382.979539	10.318285
9.319082	383.263870	10.323303
8.970880	369.436620	10.328320
8.881066	362.599909	10.333338
8.865420	366.054809	10.338355
8.427983	369.720541	10.343373
8.670402	373.116328	10.348391
8.653996	388.565940	10.353408
8.931005	385.206427	10.358426
9.224611	386.278007	10.363443
8.937579	384.151812	10.368461
9.202020	386.474411	10.373479
8.949457	377.621334	10.378496
8.840862	368.370326	10.383514
8.996924	362.978483	10.388531
8.964164	372.655812	10.393549
9.047129	375.782952	10.398567
9.421456	376.605290	10.403584
8.813535	367.854881	10.408602
8.707025	373.245713	10.413619
8.853018	379.654373	10.418637
8.828406	385.007212	10.423655
9.319083	389.787545	10.428672
9.272755	381.921628	10.433690
9.007058	362.991490	10.438707
9.001454	372.872862	10.443725
9.008732	372.594229	10.448743
9.044162	368.603337	10.453760
9.287975	375.624737	10.458778
9.143531	370.087186	10.463795
9.048254	360.496455	10.468813
8.831956	360.135873	10.473831
9.417421	364.538542	10.478848
8.900431	375.736547	10.483866
9.391374	374.211867	10.488883
8.865670	367.992102	10.493901
8.860349	373.029526	10.498919
9.368794	388.236483	10.503936
9.557688	385.165230	10.508954
9.136694	368.127405	10.513971
8.939972	374.579956	10.518989
9.180833	373.823165	10.524007
8.955914	379.374438	10.529024
9.013071	385.803243	10.534042
8.596550	379.276156	10.539059
9.049606	389.818235	10.544077
9.303760	386.632685	10.549095
9.444225	375.238082	10.554112
9.410631	384.871368	10.559130
9.807198	381.622623	10.564147
9.265567	385.446584	10.569165
9.461222	390.017243	10.574183
9.397865	382.002507	10.579200
9.147787	389.984389	10.584218
9.295998	383.407242	10.589235
8.967494	393.891138	10.594253
8.938040	392.251830	10.599271
9.392290	389.505316	10.604288
9.370554	395.091228	10.609306
9.528072	382.939767	10.614323
9.312547	385.737861	10.619341
9.521778	389.451228	10.624359
9.463505	391.363349	10.629376
9.564857	395.983405	10.634394
9.587418	382.669589	10.639411
9.234505	392.586114	10.644429
9.346333	392.717214	10.649447
9.325009	386.362111	10.654464
9.005274	387.645945	10.659482
9.424191	384.800797	10.664499
9.285229	389.679162	10.669517
9.244271	388.814777	10.674535
9.599491	386.165730	10.679552
9.342495	392.804387	10.684570
9.577618	390.912457	10.689587
9.243430	400.576775	10.694605
9.159147	395.291768	10.699623
8.937276	395.389622	10.704640
9.173822	384.450244	10.709658
9.210933	386.076129	10.714675
9.776719	396.487057	10.719693
9.159643	407.968895	10.724711
9.625230	410.124487	10.729728
9.798976	415.329693	10.734746
9.760058	409.318131	10.739763
9.545317	395.154517	10.744781
8.901562	402.058512	10.749799
9.629659	405.956170	10.754816
9.664848	415.061237	10.759834
9.832538	413.564793	10.764851
9.726751	417.295657	10.769869
9.694432	419.036491	10.774887
9.561136	406.166625	10.779904
9.633894	400.847699	10.784922
9.579761	397.258890	10.789939
9.492691	399.472126	10.794957
9.391482	406.875444	10.799975
9.527547	410.906304	10.804992
9.788663	420.307541	10.810010
10.097556	411.546903	10.815027
9.884332	412.732108	10.820045
9.692998	401.565864	10.825063
9.629342	391.370621	10.830080
9.399162	393.975348	10.835098
9.604901	396.335489	10.840115
9.972427	405.417208	10.845133
9.897056	413.734799	10.850151
10.007540	409.069527	10.855168
9.845129	394.572734	10.860186
9.492273	388.553257	10.865203
9.582017	393.301345	10.870221
10.177626	405.638888	10.875239
9.920940	399.042729	10.880256
9.602494	391.332780	10.885274
9.604381	384.093640	10.890291
9.576765	401.226964	10.895309
9.765373	412.195219	10.900327
9.957271	412.522125	10.905344
9.880748	415.446897	10.910362
9.967237	412.382117	10.915379
10.108590	411.823845	10.920397
9.575874	414.706042	10.925415
9.848656	411.037929	10.930432
9.933988	418.409053	10.935450
9.748476	413.130334	10.940467
9.870145	417.094013	10.945485
9.500506	415.138458	10.950503
10.040998	415.212284	10.955520
9.976195	419.280732	10.960538
9.834081	426.400107	10.965555
10.127177	416.310242	10.970573
9.952486	414.400070	10.975591
10.162441	411.322378	10.980608
9.635190	425.721838	10.985626
9.763474	416.241428	10.990643
10.033826	408.455576	10.995661
9.761067	408.993676	11.000679
10.202648	407.643928	11.005696
10.214393	411.899261	11.010714
9.959713	408.133401	11.015731
10.239346	422.189489	11.020749
9.709377	419.577277	11.025767
10.157835	416.017504	11.030784
10.233839	417.246035	11.035802
10.158702	408.418965	11.040819
9.879719	412.640673	11.045837
9.986117	411.018079	11.050855
9.826456	417.742572	11.055872
10.142384	414.364372	11.060890
10.014772	418.133345	11.065907
10.083794	415.367915	11.070925
10.025244	412.063798	11.075943
10.079116	413.731255	11.080960
10.155699	412.946394	11.085978
10.496953	417.708975	11.090995
10.306671	409.139661	11.096013
10.072484	411.419984	11.101031
10.363791	414.741899	11.106048
10.226718	411.992779	11.111066
9.981467	418.014266	11.116083
9.963020	406.120549	11.121101
10.128846	414.126045	11.126119
10.077866	408.933674	11.131136
10.322886	420.600015	11.136154
10.258586	427.082457	11.141171
10.117837	426.981497	11.146189
10.585299	428.814923	11.151207
10.272810	427.358528	11.156224
10.438584	418.579146	11.161242
9.873645	413.861250	11.166259
10.618460	430.079115	11.171277
10.627100	432.848627	11.176295
10.450240	411.332751	11.181312
10.319689	413.069945	11.186330
10.275076	418.874010	11.191347
10.235807	412.922459	11.196365
10.125983	412.753571	11.201383
10.378773	419.783058	11.206400
10.427668	423.922163	11.211418
10.626854	435.756588	11.216435
10.611531	427.876357	11.221453
10.445510	418.886715	11.226471
10.616463	414.073178	11.231488
10.172913	417.130831	11.236506
10.331755	411.097945	11.241523
10.650937	427.508303	11.246541
10.656216	425.456505	11.251559
10.280223	411.835511	11.256576
10.522211	417.165785	11.261594
10.365527	432.473182	11.266611
10.805073	419.589853	11.271629
10.426720	432.066435	11.276647
10.568977	420.936599	11.281664
10.659136	416.517474	11.286682
10.820869	418.600461	11.291699
10.705466	403.509392	11.296717
10.521150	404.172570	11.301735
10.610795	403.133224	11.306752
10.358989	405.589850	11.311770
10.486327	408.905737	11.316787
10.569818	397.299095	11.321805
10.670023	427.943950	11.326823
10.991011	419.793620	11.331840
10.616633	409.141841	11.336858
10.300436	408.474936	11.341875
10.747065	416.913216	11.346893
10.463383	424.758342	11.351911
10.607757	435.903903	11.356928
10.845308	431.509160	11.361946
10.594791	433.097785	11.366963
10.826124	436.435354	11.371981
10.737381	435.792991	11.376999
10.837117	429.750368	11.382016
11.123194	433.915660	11.387034
10.690089	428.694420	11.392051
10.643294	409.146355	11.397069
10.329507	416.273521	11.402087
10.575459	425.434137	11.407104
11.138607	425.523369	11.412122
11.114743	432.157300	11.417139
10.695473	415.513617	11.422157
10.734095	427.158452	11.427175
10.831472	425.193296	11.432192
10.722812	429.325376	11.437210
10.609900	431.056670	11.442227
11.068235	432.332967	11.447245
11.022359	434.249475	11.452263
11.124730	434.909041	11.457280
11.025245	432.662126	11.462298
10.704975	429.237816	11.467315
10.656480	419.504077	11.472333
10.666569	433.485382	11.477351
10.980656	430.583968	11.482368
10.836983	426.923891	11.487386
10.389205	423.686685	11.492403
10.798633	423.364371	11.497421
11.298398	418.957207	11.502439
10.777970	425.690538	11.507456
11.056568	428.992346	11.512474
10.724910	429.744734	11.517491
10.853574	426.774366	11.522509
10.597430	422.513294	11.527527
10.731146	427.396548	11.532544
11.019979	423.697533	11.537562
10.924705	439.323562	11.542579
11.340489	446.602224	11.547597
10.994660	434.434427	11.552615
11.101645	433.988797	11.557632
11.244870	428.406439	11.562650
10.888221	432.750692	11.567667
11.215208	439.538272	11.572685
11.086002	447.775903	11.577703
11.067760	448.085037	11.582720
11.378818	442.479700	11.587738
11.195405	436.847214	11.592755
11.010865	432.827443	11.597773
11.090437	435.472308	11.602791
11.057919	439.747162	11.607808
11.221202	445.357930	11.612826
11.168594	454.965813	11.617843
11.784339	448.205400	11.622861
11.350695	442.135370	11.627879
11.464278	426.784578	11.632896
11.316645	427.195904	11.637914
11.157166	435.479266	11.642931
11.356499	433.551881	11.647949
11.559771	431.658595	11.652967
11.314177	422.971660	11.657984
11.143682	429.341255	11.663002
10.988575	429.949396	11.668019
11.143109	426.334404	11.673037
11.363415	438.260212	11.678055
11.099416	432.605563	11.683072
11.148184	437.426311	11.688090
11.261020	452.003829	11.693107
11.712709	447.118173	11.698125
11.457825	456.583990	11.703143
11.578154	451.898239	11.708160
11.491274	453.729619	11.713178
10.909004	443.050230	11.718195
11.473123	451.886780	11.723213
11.426281	450.177594	11.728231
11.221746	454.293051	11.733248
11.517906	457.532172	11.738266
11.264419	451.162702	11.743283
11.438729	447.333197	11.748301
11.324343	450.301738	11.753319
11.293776	457.088193	11.758336
11.814454	451.049448	11.763354
11.629734	461.498374	11.768371
11.587119	457.106222	11.773389
11.335175	452.995961	11.778407
11.217812	452.512681	11.783424
11.499305	450.452587	11.788442
11.357056	449.929003	11.793459
11.254358	445.129663	11.798477
11.539434	437.827476	11.803495
11.373377	452.211743	11.808512
11.713774	452.064271	11.813530
11.590897	454.485051	11.818547
11.522401	442.851554	11.823565
11.709625	444.192152	11.828583
11.595514	456.659166	11.833600
11.545244	450.901810	11.838618
11.726873	460.653099	11.843635
11.719018	462.207100	11.848653
12.081793	462.841902	11.853671
12.010737	457.823048	11.858688
11.752747	447.418199	11.863706
11.715709	453.893251	11.868723
11.585279	447.047054	11.873741
11.523098	443.948614	11.878759
11.300513	453.807013	11.883776
11.615086	459.129154	11.888794
12.044948	467.756253	11.893811
11.685274	465.104896	11.898829
11.729562	470.548015	11.903847
11.879900	475.968313	11.908864
12.167413	466.358949	11.913882
11.691800	463.842403	11.918899
11.773472	467.847033	11.923917
12.142844	462.128473	11.928935
11.855115	467.588572	11.933952
12.189228	471.885243	11.938970
11.825077	471.774886	11.943987
11.779807	469.699397	11.949005
11.980413	465.868950	11.954023
11.684947	470.557119	11.959040
11.910946	461.048850	11.964058
11.739953	461.359678	11.969075
11.720663	466.544464	11.974093
12.340017	464.968226	11.979111
11.870029	465.524413	11.984128
12.087021	454.789999	11.989146
11.737600	468.830462	11.994163
11.956837	464.081974	11.999181
11.874660	462.921061	12.004199
12.102932	465.542778	12.009216
12.112522	463.846894	12.014234
12.147281	463.551358	12.019251
11.984639	469.607335	12.024269
11.738618	466.262972	12.029287
11.892429	472.859788	12.034304
12.130450	466.457966	12.039322
11.839467	472.653842	12.044339
12.094404	469.834211	12.049357
12.231762	461.876547	12.054375
11.785278	468.017741	12.059392
12.290566	473.733051	12.064410
11.975462	478.572596	12.069427
12.337653	489.567518	12.074445
12.530560	486.385175	12.079463
12.199216	480.305515	12.084480
12.033362	473.543715	12.089498
11.917009	475.316572	12.094515
12.307286	486.793091	12.099533
12.589114	491.334581	12.104551
12.405461	478.055957	12.109568
12.290748	467.568831	12.114586
11.793288	471.332287	12.119603
12.155477	485.325081	12.124621
12.493307	486.891531	12.129639
12.322453	490.985974	12.134656
12.679083	490.444673	12.139674
12.510782	487.722493	12.144691
12.486710	473.608021	12.149709
12.475036	471.470500	12.154727
12.041209	464.908208	12.159744
11.932286	470.633945	12.164762
11.930434	481.773900	12.169779
12.199377	494.127654	12.174797
12.209202	482.554516	12.179815
12.179455	494.115370	12.184832
12.478412	487.274883	12.189850
12.708236	499.407524	12.194867
12.316178	495.675657	12.199885
12.396052	485.959762	12.204903
12.396280	495.505795	12.209920
12.403543	485.211097	12.214938
12.422008	488.427191	12.219955
12.687335	501.384244	12.224973
12.532344	482.944803	12.229991
12.221853	495.234146	12.235008
12.332469	491.162096	12.240026
12.552314	502.942859	12.245043
12.820540	512.242056	12.250061
13.163587	498.461708	12.255079
12.301340	491.240307	12.260096
12.378502	490.796164	12.265114
12.947518	494.336776	12.270131
12.865317	493.863799	12.275149
12.843774	484.955766	12.280167
12.834949	485.455930	12.285184
12.837029	483.388845	12.290202
12.678019	489.021406	12.295219
12.744754	487.411292	12.300237
12.775025	476.851097	12.305255
12.264501	476.810865	12.310272
12.667430	478.162061	12.315290
12.800551	480.817529	12.320307
12.506572	484.880650	12.325325
12.964910	481.881033	12.330343
12.978458	494.504915	12.335360
12.515526	486.075839	12.340378
13.230213	495.226624	12.345395
12.900266	491.267347	12.350413
12.955753	483.079435	12.355431
12.886979	493.377789	12.360448
12.694991	482.230531	12.365466
12.750367	481.319587	12.370483
12.841694	490.172966	12.375501
12.710640	483.932738	12.380519
13.024843	495.771386	12.385536
12.986487	502.316085	12.390554
13.304922	507.830135	12.395571
12.926533	498.564263	12.400589
13.278208	488.692444	12.405607
12.671709	487.338622	12.410624
12.854740	490.226151	12.415642
13.274861	488.194959	12.420659
12.722119	502.680496	12.425677
12.902787	503.454102	12.430695
13.135319	514.232552	12.435712
13.232779	505.476386	12.440730
13.176806	487.608476	12.445747
12.719733	497.604389	12.450765
13.050009	496.751624	12.455783
13.075579	505.640495	12.460800
12.772478	509.989052	12.465818
13.577431	511.561667	12.470835
12.903737	515.040160	12.475853
13.250834	512.613255	12.480871
13.267100	520.014108	12.485888
13.395515	512.628989	12.490906
13.579135	507.283303	12.495923
12.718357	507.597392	12.500941
13.161975	503.041166	12.505959
13.453366	514.968580	12.510976
13.504849	506.449936	12.515994
13.398978	502.648264	12.521011
12.830565	498.022401	12.526029
13.370849	506.010661	12.531047
13.198531	502.983005	12.536064
13.391446	507.910711	12.541082
13.179905	498.669351	12.546099
13.126897	517.201544	12.551117
13.512409	505.929643	12.556135
13.526315	508.430115	12.561152
13.308657	514.415782	12.566170
13.672059	514.015431	12.571187
13.032574	518.984383	12.576205
13.382075	519.018522	12.581223
13.202626	514.007061	12.586240
13.335919	519.739281	12.591258
13.847606	520.574952	12.596275
13.369230	515.878264	12.601293
13.296484	518.515300	12.606311
13.469705	521.357026	12.611328
13.505254	517.770007	12.616346
13.623509	511.677137	12.621363
12.977022	523.166784	12.626381
13.495676	524.389517	12.631399
13.455021	524.414977	12.636416
13.206368	526.757524	12.641434
13.584423	515.436288	12.646451
13.398582	516.793954	12.651469
13.771278	521.535890	12.656487
13.451923	514.990468	12.661504
13.164036	519.907834	12.666522
13.627773	512.098138	12.671539
13.460674	512.742861	12.676557
13.364448	517.444201	12.681575
13.659340	529.213297	12.686592
13.937321	531.404425	12.691610
14.151768	523.412641	12.696627
13.945811	519.891625	12.701645
13.825263	522.141645	12.706663
13.815724	515.519585	12.711680
13.628162	516.041268	12.716698
13.966136	510.699950	12.721715
13.649659	518.278835	12.726733
13.780497	517.592815	12.731751
13.509402	516.502336	12.736768
13.814988	516.076274	12.741786
13.970457	513.373105	12.746803
13.734088	525.139711	12.751821
14.140119	522.432241	12.756839
14.027424	520.733301	12.761856
13.734794	528.936456	12.766874
13.808287	524.286380	12.771891
13.738138	524.508928	12.776909
13.657862	522.751294	12.781927
13.704316	519.374007	12.786944
13.903828	525.645004	12.791962
14.138679	531.146830	12.796979
13.814515	526.949970	12.801997
14.065678	537.883317	12.807015
14.057375	536.698274	12.812032
13.913201	533.180258	12.817050
14.084496	526.832983	12.822067
13.848259	531.707598	12.827085
13.919489	543.129691	12.832103
14.310033	533.983911	12.837120
14.235091	537.804667	12.842138
13.946388	533.021641	12.847155
13.865962	543.962439	12.852173
13.748696	538.792973	12.857191
14.020275	539.464067	12.862208
13.846350	546.064602	12.867226
14.245688	532.799304	12.872243
14.256934	541.687267	12.877261
14.021037	540.752246	12.882279
14.381724	538.941732	12.887296
14.213442	542.379408	12.892314
14.321773	547.156199	12.897331
14.436979	548.230320	12.902349
14.113043	550.202755	12.907367
14.311748	535.854742	12.912384
14.098419	541.947036	12.917402
14.275641	548.972562	12.922419
14.332073	546.805493	12.927437
14.623305	547.296810	12.932455
14.691119	554.004870	12.937472
14.204445	555.854327	12.942490
14.110549	550.122666	12.947507
13.944060	553.181383	12.952525
14.095338	551.807399	12.957543
14.243311	552.765970	12.962560
14.188797	556.779201	12.967578
14.218646	549.627154	12.972595
14.276507	550.801718	12.977613
14.223320	546.815116	12.982631
14.371461	545.728787	12.987648
14.660185	565.987622	12.992666
14.569290	563.445874	12.997683
14.577246	562.879966	13.002701
14.298201	558.448865	13.007719
14.885988	558.023044	13.012736
14.321773	552.260471	13.017754
14.384450	554.706021	13.022771
14.712994	560.101754	13.027789
14.620680	560.826349	13.032807
14.998572	564.160057	13.037824
14.680957	558.406423	13.042842
14.502558	545.947405	13.047859
14.372608	542.414550	13.052877
14.298758	552.388695	13.057895
14.896301	569.863485	13.062912
14.595172	571.545206	13.067930
14.960611	567.502888	13.072947
14.755639	563.934374	13.077965
14.377407	571.664902	13.082983
14.765993	570.926127	13.088000
14.555689	579.091242	13.093018
14.757029	573.370407	13.098035
15.238479	571.619980	13.103053
14.913336	571.942188	13.108071
14.976579	565.772662	13.113088
14.865706	582.237498	13.118106
14.937376	563.276709	13.123123
14.785658	550.472721	13.128141
14.354959	559.666177	13.133159
14.645515	568.135141	13.138176
14.661520	576.271330	13.143194
14.726565	567.996687	13.148211
14.791339	575.440502	13.153229
14.914968	578.697040	13.158247
15.026248	578.645198	13.163264
14.631736	572.543785	13.168282
14.559982	571.059363	13.173299
14.778110	574.092913	13.178317
14.657091	567.661753	13.183335
14.757434	573.878783	13.188352
15.055698	587.884767	13.193370
15.555542	583.124114	13.198387
15.097378	584.603077	13.203405
14.671177	573.896153	13.208423
15.485978	567.546498	13.213440
15.492375	567.107060	13.218458
15.230870	572.487372	13.223475
14.990381	562.347964	13.228493
15.149845	573.677447	13.233511
15.274829	570.376282	13.238528
15.190842	569.196709	13.243546
15.383366	568.923943	13.248563
15.224484	559.330385	13.253581
15.226496	568.731018	13.258599
15.269278	560.298906	13.263616
15.140972	563.525242	13.268634
15.248346	567.222948	13.273651
15.197648	564.886373	13.278669
15.255198	564.546263	13.283687
15.301317	562.907795	13.288704
15.266601	563.027001	13.293722
15.148175	563.383293	13.298739
15.157769	567.452814	13.303757
15.207009	578.386068	13.308775
15.649909	574.849219	13.313792
15.316725	575.646030	13.318810
15.384428	578.942833	13.323827
15.634102	573.189228	13.328845
15.220176	578.975110	13.333863
15.698584	584.379074	13.338880
15.640422	582.217220	13.343898
15.391785	575.117989	13.348915
15.173900	565.947007	13.353933
15.201225	587.575104	13.358951
15.585787	584.839411	13.363968
15.388482	590.733576	13.368986
15.878679	592.014392	13.374003
15.971196	587.588546	13.379021
15.460303	586.986660	13.384039
15.658275	584.797549	13.389056
15.259641	592.281965	13.394074
15.295469	587.069714	13.399091
15.424504	582.294215	13.404109
15.296835	593.652638	13.409127
15.605060	583.036481	13.414144
15.946372	587.912703	13.419162
15.392424	583.631690	13.424179
15.559331	587.130791	13.429197
15.585821	587.338293	13.434215
15.796957	577.848054	13.439232
15.739623	584.720772	13.444250
15.455739	580.129479	13.449267
15.841035	577.851246	13.454285
15.611938	589.392709	13.459303
15.825316	585.894749	13.464320
15.750811	583.495609	13.469338
15.638747	590.367384	13.474355
16.059823	594.991358	13.479373
15.916349	595.629250	13.484391
16.116284	593.790113	13.489408
15.919856	588.737095	13.494426
15.575737	588.954964	13.499443
16.214912	583.462591	13.504461
15.850351	594.633845	13.509479
15.980035	591.767428	13.514496
16.044797	583.843102	13.519514
15.708025	598.228821	13.524531
16.016282	600.803393	13.529549
15.925181	612.784114	13.534567
15.996631	611.794925	13.539584
16.271098	613.538503	13.544602
16.401383	615.456003	13.549619
16.132711	595.831829	13.554637
15.830691	598.649735	13.559655
16.447171	604.341465	13.564672
16.049576	600.339049	13.569690
15.844974	600.090245	13.574707
16.317887	603.017862	13.579725
16.308227	614.168584	13.584743
16.065994	613.714208	13.589760
16.200074	612.958255	13.594778
16.181656	613.191683	13.599795
16.204603	607.015794	13.604813
16.043279	614.065655	13.609831
16.265071	608.704528	13.614848
16.235683	614.414772	13.619866
16.324692	613.583788	13.624883
16.435247	612.632690	13.629901
16.226884	620.759653	13.634919
16.408260	610.500887	13.639936
16.534273	613.053344	13.644954
16.121671	609.990501	13.649971
16.291989	611.586199	13.654989
15.994999	613.750098	13.660007
16.099567	613.440535	13.665024
16.550184	608.368817	13.670042
16.484446	616.656601	13.675059
16.295999	617.875830	13.680077
16.083113	617.517867	13.685095
16.342134	611.671280	13.690112
16.803488	623.181000	13.695130
16.263321	610.787729	13.700147
16.355448	612.272531	13.705165
16.521684	632.935506	13.710183
16.504598	632.641728	13.715200
16.391570	636.096063	13.720218
16.499236	640.923475	13.725235
16.767169	629.439438	13.730253
16.650277	646.179816	13.735271
16.879291	638.349808	13.740288
16.885475	632.135496	13.745306
16.622192	627.600942	13.750323
16.898404	631.840397	13.755341
16.529169	633.116176	13.760359
16.742104	626.014485	13.765376
16.886471	630.769910	13.770394
16.390699	635.198986	13.775411
16.825957	624.714499	13.780429
16.687264	638.880070	13.785447
16.891860	630.072450	13.790464
16.587174	626.888663	13.795482
16.583152	636.596373	13.800499
17.158518	630.239796	13.805517
16.750971	635.450368	13.810535
17.036347	624.354924	13.815552
16.944078	628.194175	13.820570
17.063633	640.243099	13.825587
17.121034	628.870734	13.830605
16.982782	625.263418	13.835623
16.864889	634.812138	13.840640
17.027726	630.848686	13.845658
16.783159	626.936043	13.850675
16.977580	629.711372	13.855693
16.993706	635.042166	13.860711
16.960852	639.774695	13.865728
16.994277	634.023183	13.870746
16.801492	638.357751	13.875763
17.350870	629.676323	13.880781
17.240322	630.094503	13.885799
16.916274	635.702314	13.890816
17.301599	631.234024	13.895834
17.228248	635.931834	13.900851
17.453805	633.520680	13.905869
16.945307	633.467509	13.910887
16.878155	636.031110	13.915904
17.232621	634.272047	13.920922
16.892020	638.140498	13.925939
17.488865	635.860877	13.930957
17.030929	644.572642	13.935975
17.217208	645.247554	13.940992
17.112297	651.922586	13.946010
16.826543	658.764628	13.951027
17.158216	654.916889	13.956045
17.520204	653.295504	13.961063
17.653108	657.674038	13.966080
17.697431	648.512680	13.971098
17.459604	652.923689	13.976115
17.805843	651.588767	13.981133
17.940870	659.845314	13.986151
17.351563	651.230716	13.991168
17.411535	643.695259	13.996186
17.382827	657.878433	14.001203
17.663731	659.365403	14.006221
17.662191	656.626700	14.011239
17.593019	657.672733	14.016256
17.438637	652.972898	14.021274
16.983576	652.939808	14.026291
17.507964	651.908497	14.031309
17.273590	652.194483	14.036327
17.515565	663.766788	14.041344
17.691027	650.586751	14.046362
17.506609	649.732067	14.051379
17.370950	653.338247	14.056397
17.619019	656.998288	14.061415
17.783699	652.769466	14.066432
17.929754	652.011646	14.071450
17.538781	654.000842	14.076467
17.077567	651.737637	14.081485
17.788093	666.888124	14.086503
18.035896	669.371136	14.091520
17.929020	670.782788	14.096538
17.608311	678.905180	14.101555
17.599212	676.319124	14.106573
17.463674	672.840760	14.111591
17.782705	679.314101	14.116608
17.976321	671.517992	14.121626
17.849600	677.984999	14.126643
18.397517	685.057000	14.131661
18.250509	674.587403	14.136679
18.049671	682.198845	14.141696
18.558072	674.877569	14.146714
18.067156	677.283100	14.151731
18.461090	670.137432	14.156749
18.030379	656.676242	14.161767
17.976056	660.519059	14.166784
18.188291	650.760377	14.171802
18.238028	658.137142	14.176819
17.911595	642.857827	14.181837
18.079274	645.886622	14.186855
17.686611	655.743211	14.191872
18.171645	660.521341	14.196890
18.174615	671.423988	14.201907
17.809850	674.229584	14.206925
18.097869	674.743495	14.211943
18.024142	668.008300	14.216960
17.859609	668.643162	14.221978
18.163305	674.146936	14.226995
18.060800	664.891669	14.232013
18.192068	676.178272	14.237031
17.983082	674.431196	14.242048
18.091213	681.107782	14.247066
18.546386	696.436903	14.252083
18.422299	693.572112	14.257101
18.617178	685.602237	14.262119
18.331670	684.678087	14.267136
18.461517	684.055329	14.272154
18.550848	678.089978	14.277171
18.517231	682.425020	14.282189
18.565439	675.541454	14.287207
18.549239	675.399011	14.292224
18.698186	666.934540	14.297242
18.367566	672.641212	14.302259
18.312684	678.030410	14.307277
18.590990	690.701568	14.312295
18.576983	694.083695	14.317312
19.057721	699.118115	14.322330
18.587086	692.384750	14.327347
18.570405	675.460398	14.332365
18.839911	672.808876	14.337383
18.575379	678.890255	14.342400
18.899588	681.424486	14.347418
18.542831	675.481255	14.352435
18.797981	681.658441	14.357453
18.738937	670.569258	14.362471
18.679162	687.026235	14.367488
18.777610	689.340006	14.372506
18.865308	699.042937	14.377523
18.816309	701.430158	14.382541
18.782785	698.948884	14.387559
18.642032	702.265543	14.392576
18.896801	699.370167	14.397594
19.149992	702.625490	14.402611
19.036076	698.017170	14.407629
19.167089	682.022838	14.412647
19.006674	690.240193	14.417664
18.410391	694.075884	14.422682
18.738923	690.743005	14.427699
18.776473	700.472679	14.432717
19.007269	695.069100	14.437735
18.848956	699.511921	14.442752
18.957570	694.319863	14.447770
19.143260	696.818861	14.452787
19.120466	695.112219	14.457805
19.384353	688.305517	14.462823
18.802957	691.867499	14.467840
19.175114	684.879845	14.472858
19.149316	693.884101	14.477875
19.156292	695.707204	14.482893
19.239022	698.670341	14.487911
19.080090	693.661947	14.492928
19.100177	695.987919	14.497946
19.473427	701.566077	14.502963
18.977970	697.014006	14.507981
19.144823	683.522871	14.512999
19.020177	687.121032	14.518016
19.798249	700.175117	14.523034
19.520743	695.857346	14.528051
19.563970	694.020508	14.533069
19.349592	692.577216	14.538087
19.298081	701.058478	14.543104
19.258792	691.506186	14.548122
19.531497	697.210447	14.553139
18.971479	696.925463	14.558157
19.945588	701.662169	14.563175
19.451399	704.620461	14.568192
19.505669	693.952262	14.573210
19.603299	696.405012	14.578227
19.231195	692.505901	14.583245
19.659384	698.523612	14.588263
19.599693	710.963397	14.593280
19.490235	704.281087	14.598298
19.746066	704.396081	14.603315
19.571665	711.296542	14.608333
19.706427	707.899158	14.613351
19.574275	715.178039	14.618368
19.883889	713.340747	14.623386
20.104851	712.000081	14.628403
19.699740	706.338913	14.633421
19.851357	703.226075	14.638439
19.849458	712.109859	14.643456
19.641502	699.532262	14.648474
19.714274	686.923589	14.653491
19.703573	707.424858	14.658509
19.740041	711.193592	14.663527
19.491225	707.221635	14.668544
19.850493	712.117186	14.673562
19.807036	708.763328	14.678579
19.899823	707.221720	14.683597
19.876004	702.006100	14.688615
19.756623	701.273827	14.693632
19.596454	703.441680	14.698650
19.948753	711.800117	14.703667
19.349930	715.790837	14.708685
19.967126	721.996872	14.713703
20.019372	727.776490	14.718720
20.570673	732.582190	14.723738
20.418016	729.986921	14.728755
19.580305	717.889202	14.733773
20.088834	723.146513	14.738791
20.147346	731.572791	14.743808
20.077521	727.295259	14.748826
20.492066	724.472828	14.753843
20.254334	732.323557	14.758861
20.637152	727.962928	14.763879
20.488275	730.422506	14.768896
19.942749	722.312280	14.773914
20.267565	719.576402	14.778931
20.254606	732.191956	14.783949
20.333747	722.665389	14.788967
20.365743	724.049112	14.793984
20.319779	733.192223	14.799002
20.524624	730.093182	14.804019
20.257140	738.655424	14.809037
20.448263	730.717670	14.814055
20.403552	735.644568	14.819072
20.390906	731.601122	14.824090
20.593242	733.734628	14.829107
20.509480	736.161978	14.834125
20.424019	735.575897	14.839143
20.698193	735.779550	14.844160
20.595576	740.213709	14.849178
20.962953	739.585523	14.854195
20.476303	745.846670	14.859213
20.630369	729.498423	14.864231
20.506536	736.599297	14.869248
20.558430	736.670306	14.874266
20.726415	735.028627	14.879283
20.458297	739.084624	14.884301
20.630245	738.710921	14.889319
20.605809	735.799051	14.894336
20.860786	741.045353	14.899354
20.707281	735.654261	14.904371
20.419519	744.150237	14.909389
20.600910	729.593331	14.914407
20.883534	731.925768	14.919424
20.824520	735.100322	14.924442
20.818433	721.572970	14.929459
21.101325	744.319609	14.934477
20.896644	735.026567	14.939495
20.768034	742.273350	14.944512
20.819542	749.744548	14.949530
21.061140	757.590084	14.954547
21.272636	761.713419	14.959565
21.093551	750.614474	14.964583
21.180099	747.868354	14.969600
21.249684	752.749060	14.974618
21.020627	736.192222	14.979635
20.642778	745.487995	14.984653
20.950622	752.111423	14.989671
21.232696	756.397331	14.994688
20.926148	757.139511	14.999706
20.940229	753.517919	15.004723
20.899898	749.472468	15.009741
21.018447	757.977770	15.014759
20.932078	754.289769	15.019776
20.870439	758.651283	15.024794
21.197317	752.648922	15.029811
21.642337	771.835962	15.034829
21.399404	765.925469	15.039847
21.308093	755.017977	15.044864
21.322004	752.163248	15.049882
21.530739	761.383479	15.054899
21.406523	770.747070	15.059917
21.563840	762.435880	15.064935
21.630891	753.999898	15.069952
21.418940	759.672343	15.074970
21.617155	752.945267	15.079987
21.526843	748.162851	15.085005
21.368354	758.298607	15.090023
21.696146	767.146865	15.095040
21.726263	775.066360	15.100058
21.871307	759.019282	15.105075
21.424215	757.568037	15.110093
21.511943	755.026853	15.115111
21.793977	758.539620	15.120128
21.753919	777.679119	15.125146
21.904098	773.168512	15.130163
21.788570	765.155415	15.135181
21.895110	760.907218	15.140199
21.777957	749.303185	15.145216
21.459873	750.665680	15.150234
21.683160	759.217790	15.155251
21.964233	773.419095	15.160269
21.630719	772.076394	15.165287
22.240129	773.556407	15.170304
22.106269	773.773098	15.175322
22.018635	761.710039	15.180339
21.716100	751.857885	15.185357
21.836749	756.806379	15.190375
22.052668	770.045868	15.195392
21.801578	772.966321	15.200410
21.829636	767.259781	15.205427
21.759750	766.522955	15.210445
21.693579	766.479807	15.215463
21.929768	769.324392	15.220480
21.707862	769.892453	15.225498
22.005287	769.562327	15.230515
21.839976	765.119777	15.235533
21.990537	776.308769	15.240551
22.436881	782.159585	15.245568
22.111279	792.570682	15.250586
22.517813	790.172354	15.255603
22.769693	782.162004	15.260621
22.187134	767.932287	15.265639
22.259450	761.366817	15.270656
22.517981	778.108825	15.275674
22.526156	775.396993	15.280691
22.191723	773.751486	15.285709
22.184263	772.591543	15.290727
22.579858	765.773772	15.295744
22.155620	767.998525	15.300762
22.284272	771.266940	15.305779
22.224413	784.896506	15.310797
22.605548	782.839795	15.315815
22.727875	790.634490	15.320832
22.723560	791.307525	15.325850
22.777868	788.048881	15.330867
22.340303	792.339548	15.335885
22.575824	793.742080	15.340903
22.829609	791.755688	15.345920
22.691280	790.644520	15.350938
22.759024	795.576017	15.355955
22.946831	792.350234	15.360973
22.791654	790.515875	15.365991
22.601462	783.880818	15.371008
22.745459	792.164431	15.376026
22.748946	794.123782	15.381043
22.611377	791.494598	15.386061
22.770541	794.029297	15.391079
23.023201	786.596318	15.396096
22.879971	797.427134	15.401114
22.803036	792.614222	15.406131
22.846339	794.046681	15.411149
22.642477	795.082135	15.416167
22.539561	789.638970	15.421184
22.935919	794.765448	15.426202
22.783165	798.775095	15.431219
22.807350	798.676854	15.436237
22.766895	796.587954	15.441255
23.036401	792.450073	15.446272
22.869599	800.182494	15.451290
23.374974	801.716576	15.456307
23.169319	796.289405	15.461325
23.248195	810.812547	15.466343
23.455680	805.646087	15.471360
22.972886	803.755442	15.476378
23.447232	810.264608	15.481395
23.213786	802.907308	15.486413
22.874407	806.876587	15.491431
23.281226	806.690371	15.496448
23.195573	809.051756	15.501466
23.631115	812.139857	15.506483
23.610860	813.692664	15.511501
23.358852	807.755168	15.516519
23.511422	804.878843	15.521536
23.472041	810.691689	15.526554
23.727382	806.663303	15.531571
23.221324	794.217258	15.536589
23.447022	798.590846	15.541607
23.763471	798.702714	15.546624
23.514776	805.807278	15.551642
23.397094	808.729056	15.556659
23.690806	800.223048	15.561677
23.710218	806.036206	15.566695
23.901680	806.407368	15.571712
23.387779	797.885096	15.576730
23.699980	807.348011	15.581747
23.984676	798.701400	15.586765
23.440219	801.049014	15.591783
23.898486	803.799069	15.596800
23.842643	803.624928	15.601818
23.815239	811.777451	15.606835
24.129879	808.667614	15.611853
23.590801	798.546157	15.616871
23.938993	809.786448	15.621888
24.053005	807.487310	15.626906
23.880472	798.886643	15.631923
24.082557	797.892882	15.636941
23.600550	808.536616	15.641959
23.693262	804.580888	15.646976
23.744838	810.635185	15.651994
23.826560	810.486962	15.657011
23.959186	805.808671	15.662029
23.913303	805.595111	15.667047
23.821262	801.702861	15.672064
23.762209	800.251156	15.677082
24.102958	804.142943	15.682099
23.963798	808.115762	15.687117
23.984967	819.608941	15.692135
24.463042	824.650124	15.697152
24.516201	829.460827	15.702170
24.465489	815.602690	15.707187
24.266795	807.154410	15.712205
23.663028	812.884720	15.717223
24.227388	821.951786	15.722240
24.240495	836.100191	15.727258
23.849405	824.188475	15.732275
24.447270	831.669314	15.737293
24.731232	834.755774	15.742311
24.587244	831.704716	15.747328
24.564202	835.198727	15.752346
24.431113	830.019017	15.757363
24.650058	838.922126	15.762381
24.642178	830.049662	15.767399
24.956107	828.792340	15.772416
24.554709	831.720426	15.777434
24.752232	832.582937	15.782451
24.540946	817.891443	15.787469
24.444692	835.679639	15.792487
24.851609	825.896861	15.797504
24.828814	826.758962	15.802522
24.860465	828.619261	15.807539
24.878091	829.667567	15.812557
24.845800	831.559912	15.817575
24.834603	827.825478	15.822592
24.921490	837.657996	15.827610
24.483687	824.671140	15.832627
24.707389	831.329789	15.837645
24.609547	820.865074	15.842663
24.764645	818.922445	15.847680
24.312324	829.413251	15.852698
24.580901	833.123782	15.857715
24.809840	842.135788	15.862733
25.033381	846.979927	15.867751
25.753134	844.375039	15.872768
25.471829	839.300452	15.877786
24.924801	827.968419	15.882803
24.974562	828.030294	15.887821
25.077225	820.851023	15.892839
25.196349	827.999310	15.897856
25.279852	823.006780	15.902874
25.245095	834.107900	15.907891
25.133767	823.036229	15.912909
25.033183	822.544014	15.917927
25.002945	830.807437	15.922944
25.354152	835.596984	15.927962
25.440401	850.554499	15.932979
25.566887	842.980201	15.937997
25.430791	846.592799	15.943015
25.404069	839.913335	15.948032
25.384676	838.887785	15.953050
25.718440	842.430383	15.958067
25.781544	839.754169	15.963085
25.407214	836.006847	15.968103
25.675114	827.391239	15.973120
25.764784	836.790989	15.978138
25.655416	822.225630	15.983155
25.678986	817.157228	15.988173
25.654389	825.255672	15.993191
25.807860	819.299222	15.998208
25.571024	813.371985	16.003226
25.432585	821.245163	16.008243
25.814778	832.050996	16.013261
25.911565	841.541156	16.018279
25.899765	844.784117	16.023296
25.937725	842.152842	16.028314
25.562125	847.143912	16.033331
25.658876	835.112054	16.038349
25.836906	845.245957	16.043367
25.600767	839.848765	16.048384
25.529149	846.850037	16.053402
25.616535	843.071850	16.058419
26.039739	834.712918	16.063437
25.681103	841.910351	16.068455
25.826600	837.362588	16.073472
26.067382	846.637833	16.078490
25.930609	856.735551	16.083507
26.103330	858.245694	16.088525
26.492397	863.644720	16.093543
26.429557	863.137161	16.098560
25.951035	844.350095	16.103578
25.978454	848.688297	16.108595
26.160413	853.744035	16.113613
26.335890	859.151068	16.118631
26.182969	860.494167	16.123648
26.388861	860.017349	16.128666
26.198559	867.280100	16.133683
26.395412	859.224635	16.138701
26.561721	863.509659	16.143719
26.457089	869.190675	16.148736
26.659881	870.210155	16.153754
26.470210	874.070936	16.158771
26.563874	872.491308	16.163789
26.625117	868.619358	16.168807
26.283436	874.185809	16.173824
26.748987	860.029511	16.178842
26.438443	871.953057	16.183859
26.662606	867.645497	16.188877
26.691226	868.086195	16.193895
26.488087	869.380310	16.198912
26.809865	866.326155	16.203930
26.494066	871.869641	16.208947
26.453466	864.936714	16.213965
26.249887	865.615530	16.218983
26.654506	868.774726	16.224000
26.767067	864.677042	16.229018
26.468281	877.242530	16.234035
26.647412	882.611133	16.239053
27.110476	891.817080	16.244071
26.855627	887.704013	16.249088
26.931235	885.890515	16.254106
27.164971	885.955303	16.259123
27.163954	884.737546	16.264141
26.957290	883.031111	16.269159
27.056064	888.547924	16.274176
27.009224	891.316677	16.279194
27.017291	893.524630	16.284211
27.291988	882.007820	16.289229
27.191011	887.006636	16.294247
27.251520	883.747009	16.299264
27.098573	880.864591	16.304282
26.575122	879.027603	16.309299
27.054090	876.308725	16.314317
27.369072	877.014099	16.319335
27.241668	885.049684	16.324352
27.431136	871.668492	16.329370
27.140549	884.725001	16.334387
27.255790	879.544482	16.339405
27.755529	870.564561	16.344423
27.299035	880.835145	16.349440
27.279606	876.032191	16.354458
27.114034	886.213304	16.359475
27.604611	898.977790	16.364493
28.006492	899.066891	16.369511
27.927728	896.624190	16.374528
27.885240	876.150311	16.379546
27.985112	881.610148	16.384563
27.560158	878.615450	16.389581
27.774603	873.864444	16.394599
27.873175	876.364408	16.399616
27.917998	865.994216	16.404634
27.541355	874.990074	16.409651
27.684482	871.335743	16.414669
27.801750	876.852829	16.419687
27.721255	874.666015	16.424704
27.730495	874.099897	16.429722
27.734739	888.016199	16.434739
28.136936	897.521953	16.439757
28.366444	897.066703	16.444775
28.102042	885.760056	16.449792
27.696860	888.332143	16.454810
28.166596	896.814391	16.459827
28.305041	900.172822	16.464845
28.230489	893.797423	16.469863
27.959079	895.651267	16.474880
28.285883	898.371314	16.479898
28.078849	892.698181	16.484915
28.131347	890.067791	16.489933
28.408836	894.780470	16.494951
28.193148	904.063701	16.499968
28.643240	894.750678	16.504986
28.569397	898.072735	16.510003
28.231424	895.790310	16.515021
28.495579	896.383680	16.520039
28.276927	898.339761	16.525056
28.487927	896.416822	16.530074
28.361863	900.059426	16.535091
28.586600	902.946841	16.540109
29.185512	895.961669	16.545127
28.833453	893.413200	16.550144
28.989020	871.081322	16.555162
28.483117	873.476589	16.560179
28.177681	871.545699	16.565197
28.415357	864.802970	16.570215
28.438307	884.494493	16.575232
28.746345	886.690454	16.580250
28.630465	900.111084	16.585267
28.775477	891.407284	16.590285
28.916673	893.540861	16.595303
28.691735	891.818336	16.600320
28.836634	892.534413	16.605338
28.847022	900.788388	16.610355
28.856303	897.574603	16.615373
28.830234	899.636395	16.620391
28.523949	897.904446	16.625408
28.541857	893.259772	16.630426
28.675438	906.133494	16.635443
28.572585	899.058771	16.640461
28.724083	902.825415	16.645479
28.999541	911.385255	16.650496
28.929980	914.697180	16.655514
28.816995	918.694351	16.660531
28.803893	920.050397	16.665549
28.973621	916.432940	16.670567
29.203297	915.857746	16.675584
29.342998	913.286357	16.680602
29.237031	919.494605	16.685619
29.257219	926.323828	16.690637
29.734940	931.030589	16.695655
29.340187	933.477984	16.700672
29.413804	916.403647	16.705690
29.327684	930.169954	16.710707
29.718879	938.380434	16.715725
29.542126	927.306261	16.720743
29.363972	925.017884	16.725760
29.931573	938.754997	16.730778
29.493119	932.177472	16.735795
29.672346	940.566120	16.740813
29.569139	929.281684	16.745831
29.829237	931.791221	16.750848
30.043716	938.946797	16.755866
29.823582	930.609092	16.760883
29.727690	924.577824	16.765901
30.014991	921.857224	16.770919
29.587236	914.407057	16.775936
29.716336	924.270918	16.780954
29.466775	938.867391	16.785971
30.082886	940.037113	16.790989
30.081183	932.277612	16.796007
29.549866	939.315781	16.801024
29.529838	935.923520	16.806042
29.868809	932.914012	16.811059
29.950044	933.532708	16.816077
30.052076	927.833534	16.821095
30.313508	935.158519	16.826112
29.814259	937.495956	16.831130
29.821001	939.786169	16.836147
30.440475	950.693984	16.841165
30.187155	953.564322	16.846183
30.122813	952.851871	16.851200
30.299962	954.064692	16.856218
30.292838	949.237712	16.861235
30.683437	951.376646	16.866253
31.040350	941.992902	16.871271
30.776632	940.427886	16.876288
30.272444	920.142603	16.881306
30.589655	927.944885	16.886323
30.559236	930.796293	16.891341
30.499535	916.952099	16.896359
30.719804	922.579391	16.901376
30.854377	918.077489	16.906394
30.966960	920.568967	16.911411
30.683857	926.132625	16.916429
31.120771	925.439959	16.921447
30.799093	923.697781	16.926464
30.757831	928.993417	16.931482
31.056781	924.784650	16.936499
30.810590	926.864939	16.941517
30.844000	916.657437	16.946535
30.759503	930.597056	16.951552
30.956484	926.142239	16.956570
30.624955	924.433151	16.961587
30.603440	926.368009	16.966605
30.546419	918.708642	16.971623
30.392770	924.924316	16.976640
30.690980	942.720630	16.981658
31.183809	944.370285	16.986675
30.873834	947.445098	16.991693
31.286035	946.790993	16.996711
31.256800	948.982669	17.001728
31.237561	948.288442	17.006746
31.377843	949.260856	17.011763
30.625255	947.491093	17.016781
31.198850	940.692878	17.021799
31.035225	942.911790	17.026816
31.004591	951.323650	17.031834
31.150335	950.565867	17.036851
31.255506	952.701904	17.041869
31.636964	957.944356	17.046887
31.454334	969.523011	17.051904
31.453460	971.438880	17.056922
32.076894	972.512792	17.061939
31.510718	952.830404	17.066957
31.632252	947.469007	17.071975
31.596165	949.254660	17.076992
31.349077	960.183794	17.082010
31.791897	962.434517	17.087027
31.645241	962.145128	17.092045
31.943691	975.403478	17.097063
32.233478	976.482001	17.102080
32.208772	967.264955	17.107098
31.884920	950.839438	17.112115
31.654260	946.870911	17.117133
31.687169	944.294054	17.122151
31.486231	954.644811	17.127168
31.789571	965.605011	17.132186
32.027992	970.210187	17.137203
32.111331	981.586496	17.142221
31.906738	971.239297	17.147239
31.876937	973.708770	17.152256
31.792407	968.256376	17.157274
31.969560	970.747275	17.162291
31.985372	970.508328	17.167309
32.199188	971.084293	17.172327
32.274795	977.399988	17.177344
32.132270	966.282593	17.182362
32.276628	969.794748	17.187379
32.556678	986.713480	17.192397
32.256370	973.443180	17.197415
32.629104	982.454959	17.202432
32.443013	984.276594	17.207450
32.720484	956.324177	17.212467
32.268417	972.899301	17.217485
32.444354	969.912015	17.222503
32.246319	986.643256	17.227520
32.653402	993.450136	17.232538
33.070312	987.020276	17.237555
32.865429	992.215176	17.242573
32.685578	979.633006	17.247591
32.457363	980.179965	17.252608
32.326649	978.152433	17.257626
32.758083	988.641432	17.262643
32.696156	986.303394	17.267661
32.829498	986.191312	17.272679
33.052666	984.528396	17.277696
32.566349	988.141903	17.282714
32.763965	983.917342	17.287731
32.892212	986.299095	17.292749
32.963146	984.214921	17.297767
33.182297	976.903843	17.302784
32.754682	985.409085	17.307802
33.218401	985.422288	17.312819
32.628039	980.752378	17.317837
33.039941	991.392740	17.322855
33.361742	1000.500819	17.327872
33.012769	1006.945745	17.332890
33.479563	1006.582934	17.337907
32.942192	1012.239855	17.342925
33.557181	1004.343281	17.347943
33.805086	1004.737218	17.352960
33.430763	1007.358164	17.357978
33.693475	1005.506056	17.362995
33.239347	1008.237257	17.368013
33.141617	1001.818092	17.373031
33.261145	1010.304429	17.378048
33.177122	1005.975392	17.383066
33.384871	1011.207037	17.388083
33.456566	1006.531869	17.393101
33.345449	1004.649603	17.398119
33.372084	1016.972021	17.403136
33.849347	1024.967174	17.408154
34.150988	1016.882700	17.413171
33.542050	1020.278623	17.418189
33.312237	1020.172591	17.423207
33.903421	1019.048811	17.428224
33.917128	1027.936634	17.433242
34.240250	1032.481302	17.438259
34.010375	1034.420210	17.443277
34.012155	1032.312084	17.448295
34.242881	1029.647612	17.453312
33.795703	1030.664159	17.458330
34.126976	1032.376845	17.463347
33.964709	1032.515912	17.468365
34.013050	1023.236973	17.473383
34.300186	1026.203053	17.478400
34.267881	1029.831086	17.483418
34.051175	1024.888396	17.488435
34.391101	1025.331121	17.493453
34.384866	1022.148132	17.498471
34.372976	1023.431415	17.503488
34.353431	1025.915078	17.508506
34.729504	1024.193638	17.513523
34.282730	1018.627218	17.518541
34.483460	1025.923823	17.523559
34.657350	1019.124696	17.528576
34.542199	1029.370622	17.533594
34.577085	1020.062222	17.538611
34.802309	1024.981886	17.543629
34.588236	1027.599976	17.548647
34.790701	1028.436482	17.553664
34.392015	1026.542183	17.558682
34.865942	1020.687248	17.563699
34.659951	1015.480965	17.568717
34.606862	1015.991192	17.573735
34.762626	1023.206436	17.578752
34.953331	1034.733318	17.583770
35.234114	1031.164817	17.588787
35.008478	1033.604830	17.593805
34.965632	1027.098217	17.598823
34.970784	1024.017594	17.603840
35.045835	1039.999478	17.608858
34.848813	1036.953486	17.613875
34.730980	1042.728130	17.618893
35.081458	1048.581338	17.623911
35.299742	1044.719613	17.628928
35.376374	1053.263141	17.633946
35.577650	1046.857366	17.638963
35.670945	1047.732961	17.643981
35.619305	1048.337635	17.648999
35.671049	1045.293935	17.654016
35.388798	1047.215753	17.659034
35.636329	1037.457675	17.664051
35.067774	1036.195728	17.669069
35.466233	1043.799222	17.674087
35.612276	1042.877288	17.679104
35.745099	1043.166069	17.684122
35.548771	1053.270016	17.689139
35.680181	1052.747986	17.694157
35.527184	1050.809120	17.699175
35.770741	1038.949925	17.704192
35.511658	1052.478171	17.709210
35.862581	1043.331989	17.714227
35.646500	1042.482215	17.719245
35.415271	1053.326887	17.724263
35.725085	1034.887087	17.729280
35.433549	1043.191291	17.734298
35.606425	1057.876722	17.739315
35.786519	1059.410980	17.744333
35.636190	1066.888491	17.749351
35.976994	1058.952533	17.754368
35.831849	1065.469885	17.759386
36.180240	1063.314101	17.764403
36.316030	1063.656068	17.769421
35.688765	1072.905638	17.774439
36.308412	1069.606258	17.779456
36.369181	1089.352080	17.784474
36.485062	1082.473599	17.789491
36.193868	1090.089815	17.794509
36.218301	1088.858614	17.799527
36.643329	1082.455857	17.804544
36.571309	1092.177559	17.809562
36.674831	1088.207461	17.814579
36.955264	1090.262580	17.819597
36.676654	1078.484657	17.824615
36.689550	1059.488309	17.829632
36.648623	1071.379478	17.834650
36.566572	1061.821022	17.839667
36.847045	1071.705578	17.844685
36.641905	1067.146079	17.849703
36.788742	1076.824229	17.854720
37.219697	1076.530113	17.859738
37.153368	1067.385767	17.864755
36.998279	1054.020214	17.869773
36.601425	1056.578405	17.874791
36.898155	1072.008258	17.879808
37.171891	1078.905360	17.884826
37.093719	1079.548880	17.889843
37.339150	1083.616514	17.894861
37.231659	1077.470237	17.899879
37.147824	1066.987417	17.904896
37.433662	1076.621836	17.909914
36.981551	1056.274641	17.914931
37.185539	1060.910448	17.919949
37.060150	1074.310600	17.924967
37.365343	1069.823120	17.929984
37.754796	1071.072322	17.935002
37.254002	1074.965807	17.940019
37.519851	1068.344845	17.945037
37.440953	1072.791173	17.950055
37.599382	1068.695768	17.955072
37.221268	1070.332716	17.960090
37.494319	1067.910954	17.965107
37.126872	1064.676900	17.970125
37.115009	1072.107609	17.975143
37.649576	1071.134650	17.980160
37.280769	1079.816971	17.985178
37.377297	1082.351996	17.990195
37.612627	1086.951372	17.995213
37.368140	1092.023081	18.000231
37.928792	1086.561716	18.005248
37.647901	1093.024475	18.010266
37.955793	1092.762141	18.015283
38.095548	1087.101223	18.020301
38.155665	1091.901448	18.025319
38.096343	1082.213211	18.030336
37.927007	1090.069227	18.035354
37.612899	1091.554202	18.040371
38.478602	1097.548113	18.045389
38.374015	1121.513731	18.050407
38.344084	1095.805375	18.055424
38.313217	1102.970815	18.060442
38.266092	1108.440985	18.065459
38.152891	1111.791299	18.070477
38.116144	1114.252406	18.075495
38.564955	1105.835713	18.080512
38.547567	1111.272852	18.085530
38.426654	1108.877709	18.090547
38.426020	1109.458666	18.095565
38.247030	1117.379312	18.100583
38.486467	1111.201099	18.105600
38.524956	1112.432365	18.110618
38.357056	1110.574707	18.115635
38.993729	1114.934880	18.120653
38.747294	1115.131234	18.125671
38.826396	1120.234619	18.130688
39.266014	1129.993446	18.135706
38.858754	1116.578746	18.140723
38.985681	1110.276041	18.145741
38.599176	1119.283025	18.150759
38.937923	1126.375148	18.155776
39.402420	1127.000450	18.160794
39.280263	1130.513107	18.165811
39.540602	1115.031575	18.170829
39.028126	1112.773135	18.175847
39.180454	1117.675773	18.180864
39.341855	1127.522096	18.185882
39.447038	1121.090230	18.190899
39.632044	1117.937407	18.195917
39.384122	1122.602565	18.200935
39.556373	1127.429521	18.205952
39.567822	1114.107422	18.210970
39.307812	1101.682810	18.215987
39.511651	1110.683081	18.221005
38.986887	1114.611865	18.226023
39.024751	1121.798169	18.231040
39.346642	1124.118233	18.236058
39.279482	1130.102764	18.241075
39.313023	1116.856117	18.246093
39.472221	1125.336333	18.251111
39.961548	1141.304299	18.256128
40.459988	1133.488930	18.261146
40.028920	1124.922045	18.266163
39.761596	1111.943149	18.271181
40.113750	1120.450124	18.276199
39.633712	1117.883679	18.281216
40.089881	1123.408035	18.286234
40.143040	1145.547180	18.291251
40.463795	1142.231207	18.296269
40.433438	1121.647861	18.301287
40.137203	1119.879610	18.306304
40.046684	1122.336467	18.311322
39.972751	1132.244679	18.316339
40.487007	1137.270851	18.321357
40.162870	1146.403836	18.326375
40.040897	1149.761835	18.331392
40.321255	1144.707008	18.336410
40.193427	1149.511263	18.341427
40.531064	1148.351213	18.346445
40.008020	1153.753485	18.351463
40.062481	1149.128300	18.356480
40.724178	1155.406455	18.361498
40.578604	1166.411428	18.366515
40.755661	1171.461708	18.371533
40.789087	1167.852798	18.376551
41.126780	1175.778232	18.381568
41.135698	1163.027686	18.386586
40.819934	1148.784525	18.391603
40.974400	1147.274301	18.396621
40.539164	1151.744570	18.401639
40.798204	1157.255449	18.406656
41.126388	1161.960307	18.411674
40.892062	1159.529167	18.416691
41.152143	1167.662339	18.421709
41.227033	1170.715138	18.426727
41.225831	1165.161348	18.431744
41.201072	1163.959891	18.436762
41.518904	1162.856572	18.441779
41.497427	1164.927148	18.446797
41.440443	1168.091996	18.451815
40.936826	1170.127187	18.456832
41.117137	1171.664577	18.461850
41.252691	1169.491425	18.466867
41.791656	1168.511466	18.471885
41.292350	1166.841099	18.476903
41.450664	1170.038698	18.481920
41.276533	1171.015896	18.486938
41.467776	1184.044943	18.491955
41.652217	1186.944989	18.496973
41.696505	1176.792448	18.501991
41.657062	1194.695234	18.507008
42.021915	1189.570434	18.512026
41.509471	1194.718605	18.517043
41.917749	1186.346054	18.522061
42.090362	1183.393964	18.527079
42.058308	1179.249297	18.532096
42.025192	1183.000563	18.537114
41.797871	1189.862112	18.542131
42.259830	1179.754992	18.547149
41.974365	1192.148215	18.552167
42.034574	1192.063298	18.557184
42.329053	1179.296682	18.562202
42.319886	1188.604710	18.567219
42.473270	1186.267836	18.572237
42.262880	1181.503998	18.577255
42.482780	1191.530595	18.582272
42.213562	1197.515050	18.587290
42.545712	1200.707680	18.592307
42.944467	1204.757782	18.597325
42.765192	1207.039122	18.602343
42.485655	1186.620728	18.607360
42.778036	1197.295602	18.612378
42.873529	1195.706194	18.617395
42.677656	1182.435256	18.622413
42.712926	1185.402709	18.627431
42.688704	1195.312683	18.632448
43.052352	1198.588771	18.637466
42.909515	1190.857442	18.642483
42.973828	1187.483559	18.647501
43.023369	1200.395825	18.652519
42.988065	1211.730794	18.657536
42.894842	1195.430088	18.662554
42.848189	1201.452475	18.667571
43.104625	1196.139427	18.672589
42.973415	1202.787203	18.677607
43.299223	1202.203344	18.682624
43.427917	1195.578444	18.687642
43.358392	1200.518802	18.692659
43.105606	1198.866854	18.697677
42.937808	1201.929042	18.702695
43.012532	1206.597636	18.707712
43.498337	1218.507878	18.712730
43.411770	1217.975601	18.717747
43.272526	1219.521723	18.722765
43.561344	1226.848877	18.727783
43.532200	1224.152254	18.732800
43.715146	1221.066006	18.737818
43.445946	1221.663534	18.742835
43.396503	1217.657264	18.747853
43.677294	1226.711885	18.752871
43.720770	1240.423540	18.757888
43.798557	1236.400612	18.762906
43.912240	1245.900981	18.767923
44.123430	1231.228573	18.772941
43.913994	1241.019087	18.777959
43.557710	1244.943758	18.782976
44.359966	1233.982054	18.787994
43.838533	1235.073288	18.793011
43.975717	1238.624483	18.798029
44.531155	1244.483715	18.803047
44.516912	1251.542485	18.808064
44.678483	1240.103018	18.813082
44.467441	1231.508136	18.818099
44.471161	1232.359816	18.823117
44.593325	1231.526798	18.828135
44.528951	1237.283714	18.833152
44.830255	1242.519797	18.838170
44.471528	1238.283966	18.843187
45.029603	1246.998781	18.848205
45.190839	1236.016959	18.853223
44.470363	1233.207066	18.858240
44.829412	1234.782905	18.863258
45.075524	1234.514410	18.868275
44.616649	1237.066503	18.873293
44.473515	1238.266095	18.878311
44.895463	1250.460855	18.883328
44.413053	1254.752303	18.888346
44.499836	1253.479825	18.893363
44.863634	1261.593736	18.898381
45.300469	1276.304522	18.903399
45.242077	1285.276282	18.908416
45.606011	1277.939384	18.913434
45.396167	1274.428289	18.918451
45.159224	1264.177474	18.923469
45.361781	1257.793514	18.928487
45.361560	1271.874913	18.933504
45.350428	1276.560048	18.938522
45.502180	1283.690816	18.943539
45.715399	1276.724522	18.948557
45.924934	1282.899554	18.953575
45.866840	1281.867381	18.958592
45.695648	1278.242970	18.963610
45.515791	1282.967000	18.968627
45.874167	1279.692482	18.973645
46.273995	1279.469481	18.978663
45.978276	1284.347250	18.983680
46.062063	1281.156510	18.988698
46.219741	1283.066662	18.993715
45.578785	1274.519760	18.998733
45.987702	1270.016081	19.003751
45.889607	1279.066603	19.008768
46.274812	1276.658910	19.013786
46.260562	1282.875095	19.018803
46.064650	1281.006001	19.023821
46.233171	1268.927962	19.028839
46.085169	1274.088842	19.033856
46.226709	1278.980581	19.038874
46.026096	1279.456979	19.043891
46.140116	1292.990434	19.048909
46.477066	1287.238790	19.053927
46.152414	1309.998695	19.058944
46.584227	1299.691074	19.063962
46.712532	1303.041692	19.068979
46.607008	1308.988075	19.073997
46.693835	1302.925075	19.079015
46.361493	1304.072079	19.084032
46.638096	1300.557825	19.089050
46.721471	1300.971074	19.094067
46.659811	1306.856978	19.099085
47.225376	1311.079949	19.104103
47.066600	1322.604625	19.109120
47.318672	1324.320204	19.114138
47.694661	1316.615339	19.119155
47.183924	1301.001235	19.124173
47.467235	1288.135295	19.129191
47.486819	1286.125352	19.134208
47.456633	1281.235601	19.139226
47.759583	1279.127892	19.144243
47.039727	1286.176615	19.149261
47.631200	1276.219690	19.154279
47.487342	1281.001231	19.159296
47.430381	1284.970825	19.164314
47.404245	1279.465063	19.169331
47.646091	1297.570309	19.174349
48.003888	1297.170815	19.179367
48.029939	1302.755884	19.184384
47.856295	1286.710612	19.189402
48.068193	1278.756757	19.194419
47.598741	1277.217430	19.199437
47.889786	1282.240527	19.204455
47.871792	1294.876200	19.209472
47.913046	1313.675412	19.214490
48.245968	1305.936232	19.219507
48.265397	1308.085662	19.224525
48.138835	1312.485821	19.229543
48.032148	1318.403986	19.234560
48.234072	1314.147118	19.239578
48.580364	1302.334868	19.244595
48.167410	1306.470347	19.249613
48.347816	1299.064185	19.254631
48.290370	1304.217286	19.259648
48.332792	1296.946217	19.264666
48.695395	1301.904529	19.269683
48.316370	1299.120358	19.274701
48.596248	1296.546025	19.279719
48.301546	1309.859106	19.284736
48.703847	1303.418784	19.289754
48.568108	1306.286650	19.294771
48.401881	1313.040904	19.299789
48.515881	1320.628845	19.304807
48.587193	1319.724845	19.309824
49.045102	1330.364560	19.314842
48.769482	1316.203377	19.319859
48.882699	1333.056896	19.324877
49.008729	1323.428033	19.329895
49.174302	1327.514468	19.334912
48.649574	1329.395173	19.339930
49.037892	1329.540038	19.344947
48.827363	1353.692876	19.349965
49.250368	1348.609470	19.354983
49.451671	1344.314823	19.360000
49.206902	1357.617009	19.365018
49.430301	1349.329972	19.370035
49.576224	1351.661685	19.375053
49.491744	1345.880962	19.380071
49.626970	1349.934258	19.385088
49.302963	1339.532852	19.390106
49.705848	1352.882522	19.395123
49.555332	1361.568862	19.400141
50.083812	1363.856793	19.405159
50.227313	1371.462254	19.410176
50.074273	1368.516654	19.415194
50.263604	1369.778102	19.420211
49.917306	1368.888625	19.425229
50.502590	1362.987840	19.430247
50.113252	1351.955968	19.435264
49.786520	1353.417683	19.440282
49.513787	1353.368824	19.445299
50.107298	1364.795335	19.450317
50.051229	1369.332856	19.455335
50.262447	1361.031931	19.460352
50.758241	1370.321395	19.465370
50.542327	1367.606492	19.470387
50.477820	1375.976489	19.475405
50.625594	1370.544608	19.480423
50.457486	1361.598994	19.485440
50.628818	1373.413135	19.490458
50.298283	1369.864007	19.495475
50.730253	1390.265583	19.500493
50.942736	1383.072143	19.505511
50.906342	1375.201085	19.510528
50.836623	1385.440142	19.515546
51.095402	1387.650146	19.520563
50.912759	1383.396333	19.525581
51.528127	1385.329911	19.530599
51.320117	1381.988923	19.535616
51.284537	1390.237658	19.540634
50.949791	1383.347170	19.545651
50.994260	1387.805927	19.550669
51.080352	1391.769052	19.555687
50.904333	1384.102765	19.560704
51.234017	1390.760903	19.565722
51.840942	1408.941966	19.570739
51.557397	1417.039971	19.575757
51.155667	1407.480608	19.580775
51.352905	1404.477311	19.585792
51.639409	1402.769781	19.590810
52.183462	1398.727871	19.595827
51.834526	1397.333873	19.600845
51.806817	1403.526949	19.605863
51.642373	1407.349203	19.610880
51.591631	1399.521393	19.615898
51.884505	1397.904391	19.620915
51.742146	1410.802507	19.625933
51.791136	1414.986009	19.630951
51.994268	1415.162863	19.635968
52.289156	1417.004330	19.640986
52.419518	1419.029204	19.646003
52.612152	1423.954053	19.651021
52.787128	1423.352646	19.656039
52.947200	1415.138555	19.661056
52.426795	1401.084845	19.666074
52.544073	1398.699915	19.671091
52.635458	1402.343480	19.676109
52.789663	1391.750823	19.681127
52.780748	1389.221440	19.686144
52.503880	1401.282108	19.691162
52.737333	1395.559167	19.696179
52.911859	1418.096322	19.701197
52.683186	1416.090303	19.706215
52.664916	1418.157253	19.711232
52.168093	1421.516860	19.716250
52.749034	1420.678676	19.721267
52.520406	1421.149972	19.726285
52.782604	1423.583513	19.731303
52.723082	1436.307802	19.736320
52.495628	1435.071613	19.741338
53.339772	1430.645300	19.746355
53.164689	1446.975764	19.751373
53.136941	1442.767248	19.756391
53.758664	1445.476178	19.761408
53.952152	1458.744919	19.766426
53.965478	1436.109429	19.771443
53.799995	1428.536158	19.776461
53.757694	1434.829348	19.781479
53.951291	1427.780843	19.786496
53.870045	1430.280480	19.791514
54.038564	1429.765285	19.796531
53.918488	1426.319079	19.801549
53.987934	1425.516351	19.806567
54.023854	1431.677439	19.811584
53.789112	1444.801403	19.816602
53.984507	1434.369567	19.821619
54.066442	1446.222922	19.826637
54.183981	1448.022576	19.831655
54.415063	1450.252680	19.836672
54.349646	1458.300963	19.841690
54.362178	1462.486997	19.846707
54.381088	1465.034162	19.851725
54.088899	1462.185952	19.856743
54.407324	1455.663960	19.861760
54.626677	1461.894330	19.866778
54.363345	1455.645953	19.871795
54.475297	1454.079205	19.876813
54.272750	1454.344468	19.881831
54.558194	1458.617400	19.886848
54.424009	1485.952233	19.891866
54.745325	1481.989165	19.896883
54.543920	1485.100815	19.901901
54.600852	1488.371062	19.906919
54.860069	1481.375436	19.911936
54.775281	1494.807452	19.916954
55.116257	1499.210604	19.921971
55.382910	1504.928691	19.926989
55.193924	1504.371325	19.932007
55.724367	1496.348843	19.937024
55.168532	1499.894378	19.942042
55.630212	1501.312250	19.947059
55.781932	1495.267483	19.952077
55.703772	1500.360749	19.957095
55.929723	1497.889458	19.962112
55.833287	1495.913335	19.967130
55.589788	1495.326586	19.972147
56.012075	1503.043334	19.977165
55.768965	1499.755126	19.982183
56.016880	1500.398384	19.987200
55.963605	1505.759179	19.992218
55.969494	1487.091674	19.997235
56.041834	1487.557138	20.002253
55.905814	1496.752533	20.007271
55.953702	1485.393725	20.012288
55.819913	1491.622283	20.017306
56.140178	1484.418333	20.022323
56.196503	1492.324599	20.027341
55.891949	1488.326429	20.032359
56.376395	1497.459935	20.037376
56.224868	1525.264592	20.042394
56.517766	1529.388056	20.047411
56.916334	1515.692955	20.052429
56.653860	1530.601194	20.057447
56.690929	1514.794312	20.062464
56.577602	1519.656371	20.067482
56.322885	1518.623238	20.072499
56.383715	1518.588717	20.077517
56.506870	1523.486542	20.082535
57.061367	1524.243016	20.087552
56.952199	1545.379126	20.092570
56.972127	1537.978915	20.097587
57.295115	1538.162356	20.102605
56.800912	1541.603629	20.107623
57.608544	1537.533274	20.112640
57.574676	1538.292990	20.117658
57.365063	1537.716744	20.122675
57.593436	1539.385540	20.127693
57.332343	1538.485945	20.132711
57.504529	1539.409242	20.137728
57.237114	1545.810105	20.142746
57.234627	1548.811899	20.147763
57.370149	1548.863580	20.152781
57.673774	1565.536192	20.157799
58.017293	1550.962841	20.162816
57.933250	1559.695733	20.167834
57.827836	1562.202307	20.172851
57.575285	1555.125383	20.177869
57.456916	1560.019796	20.182887
57.984136	1552.682610	20.187904
58.083314	1568.115250	20.192922
58.269141	1578.109500	20.197939
58.332979	1579.545137	20.202957
58.529571	1586.400798	20.207975
58.853234	1582.033394	20.212992
58.666131	1582.835905	20.218010
58.768165	1577.802408	20.223027
58.965402	1575.670097	20.228045
58.783240	1577.923531	20.233063
59.057046	1576.189560	20.238080
58.586223	1565.577347	20.243098
58.739412	1570.498912	20.248115
59.056797	1578.045829	20.253133
58.807627	1581.095504	20.258151
58.801043	1574.971214	20.263168
59.283666	1577.073807	20.268186
59.402811	1579.517018	20.273203
59.058807	1580.637452	20.278221
59.059044	1582.041967	20.283239
58.966841	1575.874202	20.288256
59.077212	1570.205083	20.293274
58.801247	1570.819454	20.298291
58.838664	1575.699084	20.303309
59.028089	1594.753238	20.308327
59.567576	1599.882914	20.313344
59.573991	1601.974444	20.318362
59.277892	1602.655069	20.323379
59.297466	1599.385905	20.328397
59.199123	1604.428694	20.333415
59.744470	1607.247371	20.338432
59.847640	1613.843028	20.343450
60.062090	1620.910521	20.348467
60.443228	1613.435105	20.353485
60.460800	1623.364057	20.358503
60.565783	1626.333353	20.363520
60.383648	1619.763001	20.368538
60.389882	1621.362248	20.373555
60.377324	1608.368570	20.378573
60.272790	1614.030873	20.383591
60.594025	1608.966395	20.388608
60.354882	1619.115198	20.393626
60.521181	1624.119944	20.398643
60.542674	1614.232639	20.403661
60.493789	1625.352231	20.408679
60.397225	1625.339059	20.413696
60.449963	1625.024925	20.418714
60.689206	1631.690923	20.423731
61.031388	1630.706864	20.428749
60.498995	1651.703862	20.433767
60.619641	1639.812911	20.438784
60.975360	1640.837029	20.443802
61.162325	1642.360801	20.448819
61.370006	1636.667043	20.453837
61.156899	1642.642910	20.458855
61.298324	1649.283118	20.463872
61.693776	1664.291009	20.468890
61.634913	1666.070812	20.473907
61.885246	1663.175972	20.478925
61.667237	1664.197897	20.483943
61.677464	1652.680742	20.488960
61.772988	1663.449663	20.493978
61.637969	1666.569944	20.498995
61.766962	1665.145695	20.504013
61.761190	1661.246137	20.509031
62.141296	1654.985874	20.514048
61.924886	1663.073537	20.519066
61.751777	1660.045806	20.524083
62.199948	1654.298820	20.529101
62.111881	1657.604296	20.534119
62.054332	1653.548696	20.539136
62.452946	1660.524414	20.544154
62.238087	1672.995340	20.549171
62.764101	1677.931473	20.554189
62.682596	1680.942436	20.559207
63.066591	1682.732187	20.564224
63.383668	1687.486253	20.569242
62.890665	1670.748727	20.574259
63.031641	1656.478230	20.579277
62.755589	1666.023723	20.584295
62.818982	1658.086510	20.589312
62.788326	1665.463586	20.594330
62.451764	1676.706896	20.599347
62.807898	1673.700905	20.604365
62.997751	1681.854715	20.609383
62.408259	1680.608602	20.614400
62.844798	1677.599560	20.619418
62.952963	1695.164279	20.624435
62.808059	1692.820131	20.629453
63.181595	1699.490492	20.634471
63.173179	1695.960576	20.639488
63.103341	1697.877793	20.644506
63.153078	1715.754593	20.649523
63.539328	1709.827877	20.654541
63.464432	1718.010300	20.659559
63.549852	1717.129330	20.664576
63.678835	1721.499271	20.669594
63.660335	1718.037193	20.674611
64.081982	1738.188305	20.679629
64.220156	1741.284999	20.684647
64.488268	1738.336885	20.689664
65.027469	1732.736651	20.694682
64.246190	1722.437774	20.699699
64.411754	1700.478851	20.704717
64.324438	1711.475089	20.709735
64.893885	1731.132956	20.714752
64.979276	1713.200779	20.719770
64.465599	1712.996923	20.724787
64.314853	1705.654775	20.729805
64.601601	1718.681967	20.734823
64.507010	1737.386008	20.739840
64.922252	1722.662492	20.744858
64.944671	1728.674303	20.749875
64.861283	1736.946421	20.754893
64.733918	1726.892878	20.759911
64.839297	1734.207776	20.764928
65.075540	1731.914736	20.769946
65.162692	1747.456703	20.774963
65.272155	1748.743236	20.779981
65.270771	1749.112886	20.784999
65.629911	1760.632950	20.790016
65.686342	1749.941692	20.795034
65.361772	1755.366891	20.800051
65.756316	1746.118883	20.805069
65.421666	1758.018369	20.810087
65.695483	1747.084979	20.815104
65.770280	1749.487780	20.820122
65.530915	1754.722984	20.825139
65.713132	1753.561848	20.830157
66.045061	1771.177012	20.835175
66.278778	1771.159755	20.840192
66.426149	1772.759132	20.845210
66.447999	1774.775695	20.850227
66.365829	1770.988996	20.855245
66.642336	1768.576070	20.860263
66.559633	1762.005965	20.865280
66.524017	1765.615728	20.870298
66.264518	1774.764216	20.875315
66.611707	1768.490103	20.880333
66.595114	1779.390163	20.885351
66.415383	1771.206722	20.890368
66.750631	1769.785067	20.895386
66.602550	1776.782830	20.900403
67.059343	1779.687908	20.905421
67.324055	1790.604139	20.910439
67.499299	1781.153564	20.915456
66.983585	1771.965211	20.920474
66.729280	1780.986658	20.925491
67.217606	1786.692414	20.930509
67.613578	1786.356397	20.935527
67.418320	1798.748618	20.940544
67.368164	1784.179565	20.945562
67.108246	1790.954898	20.950579
67.450067	1782.589260	20.955597
67.369413	1790.523297	20.960615
67.488725	1806.328559	20.965632
67.630744	1806.230902	20.970650
67.615788	1812.788219	20.975667
67.926615	1819.152799	20.980685
68.213878	1812.342032	20.985703
67.898662	1814.234348	20.990720
68.305402	1812.681634	20.995738
68.273406	1818.673545	21.000755
68.052488	1810.531213	21.005773
68.149260	1813.037902	21.010791
67.875052	1814.390487	21.015808
68.162285	1826.029089	21.020826
68.306290	1824.312148	21.025843
68.359218	1825.547527	21.030861
68.544154	1824.515354	21.035879
68.543214	1825.064823	21.040896
68.750869	1823.716679	21.045914
68.871983	1838.271954	21.050931
68.822057	1841.846090	21.055949
69.008686	1839.352471	21.060967
69.057164	1852.909179	21.065984
69.372594	1854.349850	21.071002
69.515171	1866.825224	21.076019
69.375864	1854.346578	21.081037
69.842699	1851.294920	21.086055
69.523380	1859.891014	21.091072
69.455034	1847.697980	21.096090
69.686026	1856.561854	21.101107
69.498810	1850.298331	21.106125
69.632245	1849.621324	21.111143
69.594232	1849.258198	21.116160
69.748640	1842.348180	21.121178
69.516239	1843.053610	21.126195
69.720139	1848.361844	21.131213
70.285603	1860.834490	21.136231
70.266539	1877.743834	21.141248
70.361987	1871.139639	21.146266
70.202312	1875.444103	21.151283
70.247656	1874.099135	21.156301
69.934861	1865.368306	21.161319
69.992039	1868.155730	21.166336
70.373661	1864.454597	21.171354
70.600007	1878.119335	21.176371
70.718131	1890.317656	21.181389
71.054685	1885.014023	21.186407
70.901835	1892.347099	21.191424
70.922010	1891.514150	21.196442
71.046136	1888.714666	21.201459
70.947728	1893.019063	21.206477
71.353173	1897.276573	21.211495
70.783179	1889.062318	21.216512
71.330643	1881.939604	21.221530
71.424468	1892.481703	21.226547
71.265868	1890.998068	21.231565
71.721574	1885.622233	21.236583
71.847259	1883.554677	21.241600
72.168562	1878.818327	21.246618
71.810206	1882.292164	21.251635
72.143028	1877.399381	21.256653
72.092954	1876.564747	21.261671
72.062891	1875.054789	21.266688
72.340649	1879.780313	21.271706
72.117513	1878.417184	21.276723
72.392484	1872.678159	21.281741
72.009782	1868.815150	21.286759
72.174766	1873.264733	21.291776
72.140214	1867.902114	21.296794
72.234576	1875.446011	21.301811
71.764875	1882.841039	21.306829
72.277943	1886.349620	21.311847
72.131008	1899.813708	21.316864
72.374631	1890.478666	21.321882
72.386960	1898.278349	21.326899
72.326028	1897.773619	21.331917
72.737963	1911.725078	21.336935
72.709800	1928.228774	21.341952
73.030997	1922.637177	21.346970
73.100948	1921.051681	21.351987
72.822837	1930.837485	21.357005
73.075522	1921.128618	21.362023
73.067496	1927.296720	21.367040
73.026637	1933.264801	21.372058
73.177111	1944.492413	21.377075
73.086522	1952.405977	21.382093
73.422937	1952.947108	21.387111
73.124244	1950.005153	21.392128
73.724160	1961.598317	21.397146
73.711227	1972.447429	21.402163
74.024732	1969.198709	21.407181
74.060809	1970.777562	21.412199
74.167940	1974.172630	21.417216
74.384120	1964.980683	21.422234
74.434415	1962.501962	21.427251
74.405769	1977.405727	21.432269
74.372456	1969.350883	21.437287
74.154406	1968.715973	21.442304
74.209392	1964.769018	21.447322
74.368825	1969.629758	21.452339
74.024560	1973.997700	21.457357
74.217343	1982.943328	21.462375
74.441976	1985.502720	21.467392
74.618515	1994.646550	21.472410
74.835707	2000.539762	21.477427
75.221266	2003.740003	21.482445
75.390387	1998.206774	21.487463
75.230266	2001.684484	21.492480
75.455774	2003.779822	21.497498
75.711987	2002.847000	21.502515
75.638787	1995.439007	21.507533
75.333885	1996.780605	21.512551
75.436457	1997.746325	21.517568
75.563043	2002.650059	21.522586
75.655490	2005.473041	21.527603
75.323558	2005.701649	21.532621
75.737898	2005.018773	21.537639
75.523552	2003.389167	21.542656
75.983641	2003.595452	21.547674
76.741997	2005.207026	21.552691
76.682552	2000.656161	21.557709
77.141353	1989.542338	21.562727
76.879956	2000.960347	21.567744
76.628801	1995.745028	21.572762
76.768119	1998.497593	21.577779
76.755320	1994.535938	21.582797
76.690309	1976.951974	21.587815
76.830461	1992.577424	21.592832
77.018509	1981.272222	21.597850
77.318879	1978.640951	21.602867
76.709581	1985.057327	21.607885
77.067059	1981.123235	21.612903
76.879153	1980.931772	21.617920
76.931734	1984.575186	21.622938
76.937673	1985.268761	21.627955
77.141975	1991.283902	21.632973
77.337243	1994.624226	21.637991
77.427889	1996.775275	21.643008
77.673836	2001.196504	21.648026
77.709066	1999.124082	21.653043
77.295660	2007.674934	21.658061
77.662877	2003.726697	21.663079
77.574937	2010.399594	21.668096
77.747454	1998.080590	21.673114
77.856630	1997.388420	21.678131
77.526934	2011.101961	21.683149
78.112958	2012.866604	21.688167
77.896070	2025.297064	21.693184
78.008447	2025.901483	21.698202
78.434846	2025.065244	21.703219
78.296162	2027.365615	21.708237
78.523292	2014.675164	21.713255
78.438012	2022.442760	21.718272
78.308418	2020.891479	21.723290
78.281768	2018.756104	21.728307
78.421245	2041.081744	21.733325
78.681329	2040.113602	21.738343
79.054667	2051.944081	21.743360
78.806233	2045.772075	21.748378
78.728160	2044.045506	21.753395
78.888880	2059.598383	21.758413
79.184871	2064.232751	21.763431
79.275410	2068.097501	21.768448
79.696623	2064.377539	21.773466
80.129221	2062.912302	21.778483
79.523840	2066.393074	21.783501
80.086656	2057.273348	21.788519
80.227648	2063.096390	21.793536
79.902905	2056.630134	21.798554
80.256520	2065.355095	21.803571
80.020339	2065.467805	21.808589
80.220582	2063.142458	21.813607
80.063220	2054.677681	21.818624
80.132674	2058.154375	21.823642
80.266936	2052.629712	21.828659
80.334499	2058.391599	21.833677
80.414519	2062.548331	21.838695
80.546510	2081.242702	21.843712
80.511203	2082.520240	21.848730
80.584443	2087.192452	21.853747
80.407139	2085.891601	21.858765
80.461514	2082.528565	21.863783
80.631856	2087.393951	21.868800
80.675171	2101.232530	21.873818
80.891664	2107.255280	21.878835
80.864249	2118.624311	21.883853
81.186438	2106.584900	21.888871
81.038111	2110.632022	21.893888
81.562015	2129.085536	21.898906
81.555785	2121.824862	21.903923
81.501945	2136.641159	21.908941
81.640344	2131.614469	21.913959
81.983785	2132.249191	21.918976
81.955396	2133.162721	21.923994
82.087596	2131.551735	21.929011
82.061025	2129.899194	21.934029
82.110473	2138.529530	21.939047
82.257672	2132.797692	21.944064
81.952255	2140.495467	21.949082
82.278661	2133.498594	21.954099
82.169621	2148.364523	21.959117
82.175239	2146.918417	21.964135
82.508687	2151.717399	21.969152
82.528740	2160.323918	21.974170
82.688923	2150.439972	21.979187
82.446271	2157.073893	21.984205
82.841410	2165.738787	21.989223
83.015680	2172.591837	21.994240
82.733200	2178.468225	21.999258
83.038572	2170.556228	22.004275
82.726071	2185.362343	22.009293
83.201162	2175.915371	22.014311
83.502876	2175.319455	22.019328
83.184252	2182.694240	22.024346
83.845337	2188.994953	22.029363
83.463688	2196.026088	22.034381
83.800055	2204.400335	22.039399
83.650784	2206.481460	22.044416
83.370615	2211.584288	22.049434
83.603915	2204.314691	22.054451
83.832596	2214.413084	22.059469
83.891926	2213.116409	22.064487
84.190972	2224.702937	22.069504
84.199901	2227.756719	22.074522
84.807644	2231.036024	22.079539
84.543629	2230.348297	22.084557
84.603808	2229.493324	22.089575
84.722626	2235.401930	22.094592
84.535351	2233.932198	22.099610
84.500654	2233.988292	22.104627
84.396293	2233.076882	22.109645
84.488379	2251.815516	22.114663
84.921785	2247.257286	22.119680
85.272959	2258.744197	22.124698
85.074556	2251.939446	22.129715
85.442526	2260.845314	22.134733
85.193625	2263.074508	22.139751
85.906042	2275.369924	22.144768
85.558777	2282.916475	22.149786
85.707110	2278.131208	22.154803
85.754304	2283.356666	22.159821
85.705746	2279.267964	22.164839
85.913098	2272.359005	22.169856
85.732477	2279.608196	22.174874
86.287353	2277.420121	22.179891
86.241910	2279.718632	22.184909
85.816551	2282.840039	22.189927
86.322566	2287.053582	22.194944
86.333927	2299.786385	22.199962
86.453120	2308.371228	22.204979
86.917001	2298.048575	22.209997
86.964329	2300.013890	22.215015
86.773338	2300.198465	22.220032
86.727501	2302.856822	22.225050
87.139791	2290.282523	22.230067
86.833982	2294.685583	22.235085
86.986516	2293.049325	22.240103
87.277438	2304.851776	22.245120
87.109474	2322.927189	22.250138
87.229727	2312.282466	22.255155
87.708446	2313.565202	22.260173
87.416815	2312.708192	22.265191
87.669771	2307.199687	22.270208
87.649359	2312.262101	22.275226
87.605228	2315.784933	22.280243
87.560021	2315.473413	22.285261
87.654317	2330.863288	22.290279
87.878991	2328.025989	22.295296
87.786281	2337.170887	22.300314
88.043378	2328.085999	22.305331
87.982129	2346.384675	22.310349
88.179868	2354.001047	22.315367
88.556997	2355.293290	22.320384
88.373478	2348.656609	22.325402
88.610509	2345.915219	22.330419
88.577871	2352.330310	22.335437
88.889078	2361.424958	22.340455
89.269370	2367.087758	22.345472
88.857871	2379.687627	22.350490
89.054278	2371.363292	22.355507
89.506889	2368.196991	22.360525
89.211386	2376.148958	22.365543
89.193864	2370.082907	22.370560
89.030117	2370.310581	22.375578
89.357508	2370.562780	22.380595
89.669285	2364.619041	22.385613
89.615940	2389.563051	22.390631
89.882453	2393.091185	22.395648
89.969059	2396.915589	22.400666
90.206686	2396.193937	22.405683
90.435564	2396.287895	22.410701
90.037412	2390.104363	22.415719
90.146039	2386.887466	22.420736
90.209896	2394.720371	22.425754
89.964492	2396.147414	22.430771
90.578219	2397.974060	22.435789
90.616541	2407.044941	22.440807
90.949993	2413.788088	22.445824
90.847306	2413.586508	22.450842
90.831442	2412.759146	22.455859
91.067326	2409.749665	22.460877
91.131127	2406.359852	22.465895
90.860440	2405.524825	22.470912
91.184412	2414.974140	22.475930
90.972143	2417.497470	22.480947
91.103995	2428.570484	22.485965
91.265056	2435.977993	22.490983
91.515664	2423.412995	22.496000
91.370389	2439.304195	22.501018
91.631616	2452.553661	22.506035
91.744852	2452.312151	22.511053
91.753329	2462.258764	22.516071
92.008563	2457.766094	22.521088
92.182070	2455.896168	22.526106
92.029308	2460.455332	22.531123
92.591400	2466.541168	22.536141
92.649635	2475.567955	22.541159
92.802721	2473.477130	22.546176
92.990303	2462.279002	22.551194
93.017941	2473.898480	22.556211
93.082877	2475.084694	22.561229
92.997121	2473.311939	22.566247
93.020710	2468.435583	22.571264
93.060343	2470.181194	22.576282
92.906030	2465.862746	22.581299
93.150347	2476.577431	22.586317
93.330202	2480.191663	22.591335
93.487381	2484.674173	22.596352
93.537401	2503.072458	22.601370
93.589019	2494.322455	22.606387
93.924781	2496.242885	22.611405
93.674919	2501.227459	22.616423
93.971742	2488.418518	22.621440
93.814298	2493.142532	22.626458
93.781738	2500.469753	22.631475
94.022700	2512.762990	22.636493
93.997902	2524.027722	22.641511
94.449009	2517.475221	22.646528
94.525634	2528.863030	22.651546
94.332329	2521.041145	22.656563
94.886001	2530.719864	22.661581
94.820176	2548.328290	22.666599
95.063033	2546.996706	22.671616
94.876018	2545.413290	22.676634
94.826364	2540.731367	22.681651
94.936770	2540.805898	22.686669
95.018584	2551.012561	22.691687
94.950715	2544.903794	22.696704
95.319151	2550.562186	22.701722
95.522682	2558.373417	22.706739
95.441483	2559.462460	22.711757
95.282801	2570.937428	22.716775
95.487207	2569.299381	22.721792
95.519210	2578.604879	22.726810
95.890891	2593.175409	22.731827
96.159608	2587.392946	22.736845
96.041413	2592.748394	22.741863
96.247810	2593.761102	22.746880
96.476526	2598.043141	22.751898
96.411835	2590.923932	22.756915
96.998880	2588.623508	22.761933
96.398421	2600.549156	22.766951
97.041247	2607.313642	22.771968
97.327008	2607.439773	22.776986
97.512321	2608.701936	22.782003
97.301757	2595.823582	22.787021
97.062272	2596.943583	22.792039
97.412672	2599.969513	22.797056
97.518715	2607.704418	22.802074
97.549281	2609.833335	22.807091
97.669009	2607.523609	22.812109
97.295223	2606.045012	22.817127
97.522703	2599.543078	22.822144
97.534820	2600.712276	22.827162
97.745858	2616.185213	22.832179
98.144398	2623.457989	22.837197
98.260736	2631.563714	22.842215
98.290871	2630.918542	22.847232
98.246401	2634.902271	22.852250
98.353588	2639.493597	22.857267
98.233706	2641.163067	22.862285
98.186735	2637.102441	22.867303
98.493495	2652.128129	22.872320
98.961209	2652.162810	22.877338
98.540817	2652.351544	22.882355
99.139929	2651.381083	22.887373
99.070075	2648.384447	22.892391
99.119966	2662.127754	22.897408
99.248932	2662.088935	22.902426
99.377442	2669.163912	22.907443
99.973127	2669.705729	22.912461
99.693087	2671.081377	22.917479
99.735770	2663.307901	22.922496
100.004478	2664.610736	22.927514
99.713549	2670.441258	22.932531
100.043193	2665.368863	22.937549
99.983038	2677.835338	22.942567
100.021499	2683.425218	22.947584
100.240968	2693.162371	22.952602
99.854657	2687.425051	22.957619
100.367376	2686.004100	22.962637
100.319070	2708.138885	22.967655
100.580617	2704.730853	22.972672
100.881282	2720.189926	22.977690
100.619664	2716.800223	22.982707
100.774681	2718.559455	22.987725
100.846830	2724.787938	22.992743
101.096420	2740.163454	22.997760
100.981006	2740.591907	23.002778
101.143374	2741.340058	23.007795
101.291820	2738.274702	23.012813
101.242954	2750.834151	23.017831
101.501296	2752.984431	23.022848
101.582078	2759.912227	23.027866
101.848362	2760.723102	23.032883
101.705104	2754.386139	23.037901
101.947846	2767.203180	23.042919
101.886152	2773.335744	23.047936
102.532874	2773.200534	23.052954
102.543707	2772.021832	23.057971
102.935294	2768.836558	23.062989
102.946476	2774.017269	23.068007
102.996979	2781.404261	23.073024
103.524302	2777.314155	23.078042
103.141802	2766.719034	23.083059
103.564956	2767.136225	23.088077
103.212010	2772.080114	23.093095
103.188935	2758.295067	23.098112
103.483213	2761.938882	23.103130
103.448911	2768.471156	23.108147
103.454823	2765.582634	23.113165
103.358756	2762.179772	23.118183
103.287947	2769.216387	23.123200
103.905093	2776.909663	23.128218
103.795973	2792.552529	23.133235
103.897246	2791.012578	23.138253
103.864299	2790.983187	23.143271
104.187923	2790.907749	23.148288
104.271723	2790.304713	23.153306
104.249637	2806.839833	23.158323
104.728487	2812.222320	23.163341
104.880253	2815.569571	23.168359
104.738712	2823.974331	23.173376
104.884338	2815.648229	23.178394
104.710647	2820.336986	23.183411
104.844887	2828.152810	23.188429
104.968451	2839.779682	23.193447
105.144929	2843.968919	23.198464
105.027343	2838.255989	23.203482
105.241160	2837.923069	23.208499
105.585801	2852.068793	23.213517
105.835050	2851.026551	23.218535
105.485002	2860.218093	23.223552
106.048131	2867.518996	23.228570
105.818413	2863.199568	23.233587
106.131497	2864.104155	23.238605
106.361919	2872.697200	23.243623
106.310234	2890.679334	23.248640
106.317977	2874.077329	23.253658
106.630790	2885.791541	23.258675
106.755310	2884.601444	23.263693
106.771983	2886.287549	23.268711
106.574573	2881.944149	23.273728
106.918164	2895.414670	23.278746
106.945250	2907.716229	23.283763
107.427772	2907.051112	23.288781
107.257358	2911.597357	23.293799
107.106287	2908.900526	23.298816
107.099351	2911.603413	23.303834
107.368505	2930.431964	23.308851
107.620872	2928.076297	23.313869
107.636959	2922.806474	23.318887
107.720291	2927.635139	23.323904
108.380167	2942.511410	23.328922
108.414183	2940.309669	23.333939
108.342690	2947.857748	23.338957
108.856861	2945.287733	23.343975
108.792244	2946.355281	23.348992
109.132570	2939.412739	23.354010
109.178950	2944.569083	23.359027
108.921140	2946.588289	23.364045
109.070251	2941.992090	23.369063
108.867667	2947.565928	23.374080
109.190151	2946.363941	23.379098
109.104282	2944.588001	23.384115
108.938532	2938.093515	23.389133
109.283970	2942.745664	23.394151
109.223911	2955.228096	23.399168
110.023380	2961.075155	23.404186
109.711333	2970.611163	23.409203
109.823930	2974.662040	23.414221
109.785704	2965.083118	23.419239
109.598247	2970.985997	23.424256
109.694674	2987.057821	23.429274
109.994507	2992.231527	23.434291
110.134991	2987.778685	23.439309
110.541696	3004.654363	23.444327
110.635464	3012.782711	23.449344
110.837930	3006.502297	23.454362
110.903785	3019.978280	23.459379
110.741489	3022.613845	23.464397
111.077206	3009.284034	23.469415
110.983989	3017.924380	23.474432
111.044230	3019.957198	23.479450
111.477770	3038.349974	23.484467
111.427808	3028.712879	23.489485
111.813476	3029.274783	23.494503
111.048910	3039.925954	23.499520
111.423818	3050.241918	23.504538
111.633505	3059.037115	23.509555
111.935258	3062.515710	23.514573
112.070414	3071.076340	23.519591
111.878552	3086.000125	23.524608
112.448645	3083.686499	23.529626
112.451891	3087.842797	23.534643
112.518681	3079.771869	23.539661
112.558897	3086.775542	23.544679
112.636580	3107.827592	23.549696
113.046438	3103.648393	23.554714
113.248943	3101.142662	23.559731
113.577314	3101.871295	23.564749
113.975157	3093.063940	23.569767
113.623425	3096.183491	23.574784
113.832097	3091.398082	23.579802
114.208003	3093.526943	23.584819
114.274200	3089.423346	23.589837
114.322442	3093.424303	23.594855
114.108331	3094.019624	23.599872
114.250493	3091.778934	23.604890
114.159911	3104.130509	23.609907
114.019556	3115.284202	23.614925
114.438905	3120.148975	23.619943
114.471167	3119.746476	23.624960
114.998598	3110.155155	23.629978
114.779232	3110.135851	23.634995
114.987106	3125.773839	23.640013
114.952904	3129.961227	23.645031
114.809294	3147.408763	23.650048
115.317783	3139.127013	23.655066
115.534904	3131.136809	23.660083
115.290056	3134.381751	23.665101
115.805814	3146.430648	23.670119
115.762908	3150.272221	23.675136
116.245890	3155.789884	23.680154
116.394610	3157.335523	23.685171
116.270440	3149.376353	23.690189
116.542634	3154.876336	23.695207
116.393055	3155.811942	23.700224
116.399911	3155.741636	23.705242
116.365591	3147.118316	23.710259
116.402144	3161.021888	23.715277
116.437495	3150.591880	23.720295
116.493067	3162.393666	23.725312
116.999722	3180.033513	23.730330
116.844116	3170.135050	23.735347
116.813225	3175.401331	23.740365
117.019892	3186.396887	23.745383
117.191873	3197.890208	23.750400
117.381910	3201.720774	23.755418
117.597930	3195.296157	23.760435
117.534386	3204.477985	23.765453
117.818582	3218.491384	23.770471
117.747117	3229.183094	23.775488
118.098747	3221.055130	23.780506
118.137592	3220.964063	23.785523
118.226430	3227.625670	23.790541
118.643740	3239.368030	23.795559
118.368248	3259.613616	23.800576
118.420114	3246.315199	23.805594
118.784592	3242.654330	23.810611
118.866578	3251.680966	23.815629
119.280307	3265.882540	23.820647
119.114485	3274.272353	23.825664
118.885334	3262.797745	23.830682
119.302361	3271.472394	23.835699
119.414425	3290.720299	23.840717
119.607203	3291.851946	23.845735
120.248550	3293.387177	23.850752
120.462737	3287.641387	23.855770
120.319799	3279.994385	23.860787
120.688374	3282.903981	23.865805
120.907073	3264.712788	23.870823
120.838783	3271.619805	23.875840
120.694805	3267.334272	23.880858
121.101402	3265.860365	23.885875
121.227736	3269.404186	23.890893
121.672818	3262.192718	23.895911
120.984913	3266.611316	23.900928
121.319717	3271.827002	23.905946
121.508875	3260.309361	23.910963
121.089863	3268.763840	23.915981
121.720979	3270.878239	23.920999
122.005717	3286.813703	23.926016
121.937013	3288.345862	23.931034
122.042480	3281.215668	23.936051
121.591659	3289.327932	23.941069
121.773190	3282.372109	23.946087
121.991910	3285.743741	23.951104
122.039362	3294.109827	23.956122
122.445810	3308.340974	23.961139
122.426540	3312.822759	23.966157
122.476050	3312.793153	23.971175
122.700291	3330.581272	23.976192
123.315668	3334.235179	23.981210
122.985556	3324.669948	23.986227
122.803662	3333.538871	23.991245
123.432882	3347.583870	23.996263
123.652095	3347.407909	24.001280
123.654793	3356.939304	24.006298
123.867030	3353.172712	24.011315
123.790825	3357.511876	24.016333
123.751605	3340.074057	24.021351
124.336432	3361.198941	24.026368
123.939930	3372.963940	24.031386
124.384587	3372.604539	24.036403
124.456839	3380.998365	24.041421
124.780940	3372.549534	24.046439
125.222806	3374.141081	24.051456
124.987507	3365.321703	24.056474
125.379388	3356.291060	24.061491
125.584087	3361.189318	24.066509
125.723619	3361.016294	24.071527
125.694759	3351.520924	24.076544
125.691311	3346.818972	24.081562
126.070420	3341.943838	24.086579
126.106467	3342.961019	24.091597
126.055531	3348.312531	24.096615
125.980554	3357.893894	24.101632
126.043122	3351.644609	24.106650
126.321962	3346.876614	24.111667
126.192192	3343.687195	24.116685
126.460327	3356.478611	24.121703
126.579234	3364.186591	24.126720
126.394840	3374.413075	24.131738
126.626692	3370.570834	24.136755
126.490417	3382.528881	24.141773
126.630413	3385.922258	24.146791
127.188671	3399.665885	24.151808
127.114445	3402.609723	24.156826
127.233943	3404.216744	24.161843
127.095553	3421.048279	24.166861
127.234455	3423.848472	24.171879
127.950788	3433.543388	24.176896
127.618659	3443.183770	24.181914
127.923903	3441.870814	24.186931
127.893149	3456.056524	24.191949
128.069399	3452.614290	24.196967
128.022849	3467.588359	24.201984
128.205977	3470.713073	24.207002
128.748088	3474.832907	24.212019
128.713271	3495.218033	24.217037
128.827201	3491.706589	24.222055
129.124447	3503.613001	24.227072
128.817294	3503.083435	24.232090
128.727652	3503.488955	24.237107
129.179287	3522.352840	24.242125
129.748513	3522.516908	24.247143
129.812177	3512.795582	24.252160
129.872839	3534.532519	24.257178
130.259147	3535.813955	24.262195
130.095232	3539.942728	24.267213
129.812586	3541.309377	24.272231
130.328570	3545.496419	24.277248
130.243854	3562.360760	24.282266
130.570526	3569.967044	24.287283
130.569559	3574.206172	24.292301
130.444225	3574.118571	24.297319
130.789850	3588.100601	24.302336
131.250134	3592.883381	24.307354
131.528175	3592.508887	24.312371
131.754278	3591.618548	24.317389
131.547157	3597.234323	24.322407
131.915629	3605.313857	24.327424
131.696459	3610.426518	24.332442
132.017854	3613.188860	24.337459
132.179100	3625.428991	24.342477
132.048091	3617.009872	24.347495
132.353982	3610.779426	24.352512
132.229212	3624.108793	24.357530
132.653304	3634.755151	24.362547
132.787256	3639.547720	24.367565
133.065333	3630.761907	24.372583
133.333935	3633.226318	24.377600
133.305165	3639.379300	24.382618
133.784707	3635.608908	24.387635
133.037653	3637.802204	24.392653
133.051826	3656.257749	24.397671
133.372528	3662.978105	24.402688
133.146012	3661.814204	24.407706
133.584431	3668.626702	24.412723
133.610872	3676.235587	24.417741
133.647663	3675.980714	24.422759
134.059021	3693.705340	24.427776
134.163026	3711.332650	24.432794
134.375288	3699.624915	24.437811
134.514482	3714.687050	24.442829
134.852339	3725.394231	24.447847
135.037846	3727.410783	24.452864
134.693958	3726.744899	24.457882
135.144747	3730.856918	24.462899
135.386135	3750.318740	24.467917
135.506556	3751.587932	24.472935
135.919486	3755.052510	24.477952
135.823241	3754.111351	24.482970
136.085222	3740.303265	24.487987
136.119602	3750.647400	24.493005
136.414382	3766.010447	24.498023
136.092355	3768.680457	24.503040
136.300003	3772.622028	24.508058
136.496432	3777.183970	24.513075
136.773162	3795.062219	24.518093
136.896206	3796.220537	24.523111
137.420995	3788.826015	24.528128
137.253010	3802.152772	24.533146
137.106368	3799.107930	24.538163
137.059624	3814.252754	24.543181
137.227534	3829.433608	24.548199
137.803821	3825.364052	24.553216
137.798792	3829.812185	24.558234
137.959426	3834.730058	24.563251
138.192121	3850.835093	24.568269
138.575354	3842.468369	24.573287
138.807456	3835.371897	24.578304
138.716946	3845.634530	24.583322
139.011106	3837.215395	24.588339
138.783938	3845.472993	24.593357
139.067375	3857.003038	24.598375
139.277135	3859.082110	24.603392
139.310766	3861.725167	24.608410
139.857556	3865.105801	24.613427
139.543187	3861.433717	24.618445
139.487539	3870.854530	24.623463
139.899489	3869.449181	24.628480
139.778988	3878.936907	24.633498
139.937965	3884.391616	24.638515
140.324837	3900.201253	24.643533
140.431094	3910.335444	24.648551
140.436347	3910.480011	24.653568
140.333973	3916.442546	24.658586
140.710074	3915.929685	24.663603
140.928272	3921.031151	24.668621
140.889012	3933.400553	24.673639
141.155217	3932.551299	24.678656
140.929632	3938.921245	24.683674
141.531859	3949.524275	24.688691
141.651773	3960.587468	24.693709
141.771976	3970.429145	24.698727
142.059027	3962.118371	24.703744
141.801962	3966.624716	24.708762
142.288886	3985.142714	24.713779
142.341834	3992.580323	24.718797
142.402198	3993.530629	24.723815
142.541984	3989.023992	24.728832
142.375531	3999.920324	24.733850
142.849316	4004.069857	24.738867
143.086368	4007.195738	24.743885
142.938276	4015.169661	24.748903
143.085890	4014.474587	24.753920
142.870332	4019.823522	24.758938
143.324206	4028.073015	24.763955
143.455173	4043.130393	24.768973
143.329622	4037.898077	24.773991
143.899852	4044.481882	24.779008
144.235759	4053.560918	24.784026
144.797636	4051.826053	24.789043
144.798769	4045.876472	24.794061
144.785954	4048.353192	24.799079
144.939547	4047.897064	24.804096
144.720822	4058.508034	24.809114
145.046167	4067.961165	24.814131
145.386254	4066.759523	24.819149
145.298670	4076.510513	24.824167
145.393372	4071.467992	24.829184
145.630568	4092.922457	24.834202
146.078769	4096.915024	24.839219
145.930397	4098.598532	24.844237
146.222814	4093.474723	24.849255
146.447709	4088.831715	24.854272
146.325862	4086.240626	24.859290
146.372948	4110.754753	24.864307
146.662623	4116.463781	24.869325
146.896491	4112.273878	24.874343
146.985508	4118.175118	24.879360
147.434488	4131.096744	24.884378
147.439969	4133.138214	24.889395
147.564047	4137.162315	24.894413
147.367308	4141.018581	24.899431
147.909914	4131.206575	24.904448
148.005705	4137.681214	24.909466
148.073584	4141.575189	24.914483
148.329686	4149.612494	24.919501
148.648183	4151.810392	24.924519
148.781282	4148.491528	24.929536
148.511605	4152.103491	24.934554
148.397077	4157.764992	24.939571
148.820419	4149.230911	24.944589
148.869266	4170.010936	24.949607
149.359566	4169.616009	24.954624
149.026489	4174.875972	24.959642
149.380406	4185.391549	24.964659
149.319759	4205.017670	24.969677
149.543841	4195.375160	24.974695
150.212483	4204.774915	24.979712
150.149870	4214.642031	24.984730
150.071264	4213.492941	24.989747
150.386536	4224.926733	24.994765
150.306339	4232.950151	24.999783
150.741344	4228.697343	25.004800
151.220037	4242.327750	25.009818
151.007791	4241.464596	25.014835
151.050928	4242.215593	25.019853
151.046934	4249.728456	25.024871
151.453271	4246.120840	25.029888
151.538349	4265.039417	25.034906
151.793074	4270.491961	25.039923
151.878983	4266.997355	25.044941
151.730037	4281.157926	25.049959
151.797244	4287.255153	25.054976
152.081843	4285.803318	25.059994
152.210650	4292.784197	25.065011
152.671822	4298.248796	25.070029
152.806752	4314.593567	25.075047
152.886727	4308.846254	25.080064
152.811853	4314.564758	25.085082
152.578177	4319.118049	25.090099
153.476022	4327.538439	25.095117
153.050596	4344.402896	25.100135
153.316112	4347.959980	25.105152
153.520026	4366.468775	25.110170
153.910919	4372.152657	25.115187
154.179410	4374.468840	25.120205
153.795555	4379.645233	25.125223
153.770079	4380.700459	25.130240
154.277091	4389.055473	25.135258
154.408388	4404.109944	25.140275
154.842119	4416.115651	25.145293
154.727154	4414.726014	25.150311
155.125232	4425.512614	25.155328
155.237476	4435.459943	25.160346
155.138380	4435.920614	25.165363
155.407753	4430.913926	25.170381
155.887668	4455.389539	25.175399
155.928602	4465.041820	25.180416
156.705839	4459.473132	25.185434
156.297254	4462.324006	25.190451
156.739163	4455.415572	25.195469
156.730220	4475.393761	25.200487
156.724675	4483.869653	25.205504
156.944263	4485.158177	25.210522
156.851302	4488.537530	25.215539
156.973414	4486.236664	25.220557
157.388312	4507.894369	25.225575
157.565957	4498.934391	25.230592
157.675372	4504.056116	25.235610
157.757519	4530.983130	25.240627
157.889710	4523.501086	25.245645
158.061209	4527.047592	25.250663
158.792346	4527.262220	25.255680
159.001586	4546.471084	25.260698
158.882785	4547.828079	25.265715
158.996318	4545.358096	25.270733
159.297713	4551.841906	25.275751
159.355539	4538.409043	25.280768
159.628923	4534.806288	25.285786
159.729900	4546.538783	25.290803
160.047401	4548.411779	25.295821
160.167630	4558.439998	25.300839
159.522296	4572.646516	25.305856
160.199076	4571.190414	25.310874
160.085714	4574.077408	25.315891
160.193390	4583.321657	25.320909
160.830520	4583.077464	25.325927
160.688454	4591.596756	25.330944
160.589116	4598.528052	25.335962
161.000655	4619.002770	25.340979
161.455403	4617.672768	25.345997
160.877684	4618.807674	25.351015
161.194901	4629.168248	25.356032
161.956606	4649.358067	25.361050
161.631462	4645.981043	25.366067
161.956159	4656.362563	25.371085
162.201462	4670.843981	25.376103
161.993235	4674.326537	25.381120
162.712077	4665.572606	25.386138
162.484308	4689.950394	25.391155
162.686828	4697.147215	25.396173
162.857418	4699.096758	25.401191
163.207825	4707.911887	25.406208
163.295323	4707.024137	25.411226
163.251428	4715.177842	25.416243
163.832038	4709.677568	25.421261
164.075865	4713.424330	25.426279
164.280242	4711.132722	25.431296
164.422627	4710.444749	25.436314
164.068071	4712.182509	25.441331
164.236626	4726.120393	25.446349
164.736086	4730.591209	25.451367
164.822996	4727.459345	25.456384
164.883438	4727.197619	25.461402
165.101429	4746.888263	25.466419
165.246229	4746.506085	25.471437
165.379811	4760.215866	25.476455
165.495430	4762.568526	25.481472
166.035728	4768.813210	25.486490
165.925140	4786.257185	25.491507
166.326210	4785.115444	25.496525
166.267038	4777.820909	25.501543
166.009990	4788.861232	25.506560
166.348143	4799.089231	25.511578
166.823859	4801.849826	25.516595
166.932728	4801.230196	25.521613
167.349790	4810.899856	25.526631
167.134561	4825.806618	25.531648
167.437595	4817.912770	25.536666
167.294466	4836.037334	25.541683
167.774970	4841.634815	25.546701
168.046174	4850.973686	25.551719
167.780787	4854.297884	25.556736
168.187186	4860.692860	25.561754
168.192956	4872.213125	25.566771
168.323314	4875.472557	25.571789
168.729633	4889.944864	25.576807
168.814575	4895.673390	25.581824
168.894836	4900.064317	25.586842
168.851886	4919.805244	25.591859
169.265657	4924.939675	25.596877
169.661249	4930.275794	25.601895
169.916864	4938.275650	25.606912
169.748626	4956.760921	25.611930
169.918363	4951.015213	25.616947
170.106986	4957.778711	25.621965
170.208855	4975.653788	25.626983
170.108347	4980.423245	25.632000
170.442325	4995.591849	25.637018
170.788459	5009.985241	25.642035
170.862022	5000.387835	25.647053
171.475743	5013.012990	25.652071
171.522212	5034.495109	25.657088
172.113478	5025.492570	25.662106
172.402217	5030.157247	25.667123
172.380033	5023.769071	25.672141
172.592871	5033.884142	25.677159
172.198125	5041.085707	25.682176
172.399645	5044.523478	25.687194
172.673232	5049.537730	25.692212
172.676048	5059.691826	25.697229
172.948324	5072.890999	25.702247
172.935258	5075.655137	25.707264
173.553061	5086.976088	25.712282
173.713783	5095.628393	25.717300
173.721855	5092.275162	25.722317
173.993716	5096.036578	25.727335
173.891904	5111.326787	25.732352
174.662499	5111.055498	25.737370
174.488942	5117.064231	25.742388
174.630031	5121.335265	25.747405
174.602403	5112.997204	25.752423
174.600590	5122.138829	25.757440
174.962219	5138.079740	25.762458
175.268768	5141.580089	25.767476
175.476108	5147.936716	25.772493
175.945686	5146.115115	25.777511
175.724458	5158.239069	25.782528
176.176386	5158.339354	25.787546
176.245072	5164.064182	25.792564
176.284956	5163.843528	25.797581
176.350072	5169.644669	25.802599
176.195719	5178.109331	25.807616
176.593803	5170.358357	25.812634
176.642166	5193.620626	25.817652
176.694567	5201.317649	25.822669
177.605541	5205.102687	25.827687
177.514665	5232.963592	25.832704
177.722793	5238.818246	25.837722
177.942899	5230.132225	25.842740
178.063484	5254.661707	25.847757
178.264217	5256.051075	25.852775
177.965619	5259.437334	25.857792
178.255894	5271.102948	25.862810
178.848980	5279.470228	25.867828
179.087643	5280.317087	25.872845
179.063306	5293.212228	25.877863
179.087167	5300.004663	25.882880
179.455056	5306.866643	25.887898
179.649903	5317.461305	25.892916
179.969306	5323.513304	25.897933
180.494982	5331.054628	25.902951
180.477477	5333.920505	25.907968
180.796168	5328.987963	25.912986
180.798539	5350.518356	25.918004
180.698474	5356.099065	25.923021
180.963821	5354.937387	25.928039
180.940296	5365.992206	25.933056
181.219362	5374.408420	25.938074
181.134919	5381.697537	25.943092
181.525373	5402.280589	25.948109
182.109129	5405.791493	25.953127
181.884550	5409.838595	25.958144
182.484812	5409.653798	25.963162
182.301603	5424.679168	25.968180
182.682141	5439.850365	25.973197
182.965914	5434.149881	25.978215
182.653501	5451.243976	25.983232
182.970599	5452.501607	25.988250
183.333435	5456.432013	25.993268
183.400558	5481.762414	25.998285
183.705288	5479.300417	26.003303
183.574047	5493.310818	26.008320
183.951351	5499.761055	26.013338
184.067478	5506.469758	26.018356
184.201335	5516.660526	26.023373
184.466639	5522.869372	26.028391
184.601253	5539.464662	26.033408
185.540665	5541.013667	26.038426
185.749799	5541.448472	26.043444
185.850895	5541.417146	26.048461
186.416656	5540.502244	26.053479
186.134729	5544.971812	26.058496
186.308819	5539.963873	26.063514
186.397494	5542.948983	26.068532
186.300071	5536.821708	26.073549
186.450123	5555.709418	26.078567
186.391047	5562.331783	26.083584
187.030178	5568.744438	26.088602
187.193588	5565.625773	26.093620
187.030832	5578.466909	26.098637
187.421519	5589.406870	26.103655
187.220675	5594.545642	26.108672
187.333982	5596.412662	26.113690
187.486243	5608.958563	26.118708
187.776213	5615.059434	26.123725
188.377680	5629.618743	26.128743
188.382685	5642.670548	26.133760
188.627079	5651.979284	26.138778
188.649964	5651.098392	26.143796
188.613632	5675.567644	26.148813
188.998782	5669.343097	26.153831
188.913169	5693.302368	26.158848
189.700482	5695.667368	26.163866
189.536005	5701.889526	26.168884
189.901298	5719.332907	26.173901
190.327279	5715.974472	26.178919
190.659793	5723.656514	26.183936
190.506138	5736.480562	26.188954
190.845864	5748.356588	26.193972
190.723960	5746.251383	26.198989
191.174793	5750.966769	26.204007
191.255952	5770.057979	26.209024
191.432802	5776.230178	26.214042
192.067852	5787.627798	26.219060
192.071069	5797.195118	26.224077
191.831850	5792.623936	26.229095
192.029406	5802.748128	26.234112
192.536421	5809.373989	26.239130
192.629688	5820.941208	26.244148
192.862447	5831.063092	26.249165
192.836384	5842.270111	26.254183
192.768307	5852.981779	26.259200
192.837827	5863.255359	26.264218
193.496861	5874.841853	26.269236
193.504779	5899.187722	26.274253
194.031354	5901.580717	26.279271
194.289176	5919.782825	26.284288
194.524679	5930.627201	26.289306
195.015830	5926.838753	26.294324
194.827326	5941.518145	26.299341
195.075896	5948.484174	26.304359
195.243132	5950.352303	26.309376
195.096761	5952.023042	26.314394
195.646752	5966.439118	26.319412
195.921208	5980.481429	26.324429
195.915224	5981.915664	26.329447
196.012740	5993.548619	26.334464
196.238504	6001.619881	26.339482
196.602034	6009.777023	26.344500
196.894206	6029.047146	26.349517
196.948236	6024.723816	26.354535
197.119782	6032.099604	26.359552
197.750617	6056.244532	26.364570
197.995977	6048.879978	26.369588
198.044973	6055.053238	26.374605
198.280620	6056.844438	26.379623
198.305393	6071.235042	26.384640
198.386552	6076.636238	26.389658
198.554082	6077.708863	26.394676
198.467584	6092.732352	26.399693
198.868820	6091.394797	26.404711
199.647335	6099.237996	26.409728
199.349679	6112.015280	26.414746
199.781059	6121.866497	26.419764
199.757296	6116.062163	26.424781
200.287305	6125.743352	26.429799
200.539667	6120.218005	26.434816
200.322263	6129.131698	26.439834
200.614457	6132.748115	26.444852
200.444288	6147.768893	26.449869
200.581274	6148.944133	26.454887
200.466231	6157.071681	26.459904
200.700671	6177.118015	26.464922
201.568156	6176.519125	26.469940
201.597874	6198.567110	26.474957
201.966105	6211.038765	26.479975
202.470129	6223.912281	26.484992
201.841763	6222.735015	26.490010
202.490550	6235.617567	26.495028
202.669559	6243.055412	26.500045
202.641235	6245.942056	26.505063
203.327663	6263.370685	26.510080
203.315680	6269.098949	26.515098
203.398876	6274.070579	26.520116
203.375823	6283.320263	26.525133
203.786255	6285.011671	26.530151
203.795257	6297.132102	26.535168
204.494554	6318.147922	26.540186
204.685767	6320.441666	26.545204
204.848156	6327.954737	26.550221
205.157930	6342.863073	26.555239
205.605267	6339.659036	26.560256
205.779900	6347.722628	26.565274
205.799102	6330.885236	26.570292
206.124253	6350.352592	26.575309
206.394718	6346.513186	26.580327
206.559949	6356.904724	26.585344
206.627548	6355.407596	26.590362
207.155788	6368.454219	26.595380
207.165867	6376.066783	26.600397
207.283210	6384.224542	26.605415
207.342408	6391.611653	26.610432
207.362104	6403.105464	26.615450
207.666227	6407.067316	26.620468
207.580112	6412.756660	26.625485
207.871606	6424.214482	26.630503
208.123540	6424.273313	26.635520
208.365745	6449.353674	26.640538
208.503928	6456.491762	26.645556
208.737899	6470.862738	26.650573
209.159135	6488.847413	26.655591
209.332910	6496.920675	26.660608
209.559198	6509.111590	26.665626
210.001164	6519.665322	26.670644
209.880505	6521.679348	26.675661
210.291262	6534.305597	26.680679
210.437214	6539.390641	26.685696
210.897347	6540.152574	26.690714
211.242446	6547.346871	26.695732
211.710609	6554.951325	26.700749
211.797005	6553.315516	26.705767
211.740518	6547.039475	26.710784
211.758490	6552.778948	26.715802
212.488221	6559.853390	26.720820
212.322392	6578.371494	26.725837
212.565829	6572.964200	26.730855
212.727058	6572.323734	26.735872
212.566633	6602.290466	26.740890
212.608084	6600.020833	26.745908
212.551722	6618.319904	26.750925
212.540414	6632.539791	26.755943
212.978109	6643.946579	26.760960
213.327827	6663.527243	26.765978
213.718216	6678.808426	26.770996
213.848302	6683.959115	26.776013
213.839767	6693.276194	26.781031
214.298010	6706.179276	26.786048
214.518872	6720.031625	26.791066
214.852554	6720.971091	26.796084
215.083188	6721.913973	26.801101
215.259044	6742.958112	26.806119
215.609406	6741.356952	26.811136
216.039633	6756.369986	26.816154
216.413034	6761.126103	26.821172
216.243199	6772.668595	26.826189
216.496149	6774.567660	26.831207
216.977778	6780.519127	26.836224
216.689369	6797.648622	26.841242
216.992779	6795.363435	26.846260
217.386842	6806.950741	26.851277
217.620282	6818.553590	26.856295
217.911747	6827.104288	26.861312
217.820941	6841.952283	26.866330
218.144205	6850.254970	26.871348
218.753850	6863.418701	26.876365
218.730985	6880.636359	26.881383
219.026775	6879.043683	26.886400
219.116699	6887.265914	26.891418
219.146137	6898.111380	26.896436
219.419417	6915.002010	26.901453
219.795387	6934.534683	26.906471
220.144965	6938.369616	26.911488
220.259733	6950.622383	26.916506
220.712397	6948.392861	26.921524
221.025300	6955.810150	26.926541
221.140926	6966.563318	26.931559
221.684985	6982.935179	26.936576
221.499020	6983.712488	26.941594
221.706187	6984.093971	26.946612
221.817946	7002.152589	26.951629
222.153877	7008.890760	26.956647
222.525677	7007.882875	26.961664
222.349322	7024.322737	26.966682
222.686739	7024.024170	26.971700
223.098993	7037.562851	26.976717
223.213880	7052.792535	26.981735
223.377702	7051.905417	26.986752
223.482714	7063.986154	26.991770
224.356422	7075.331644	26.996788
224.327722	7071.046203	27.001805
224.187613	7087.328951	27.006823
224.757276	7086.539645	27.011840
225.367543	7089.513253	27.016858
225.446882	7078.676385	27.021876
225.668863	7090.745243	27.026893
225.967319	7102.031939	27.031911
226.123079	7090.094066	27.036928
226.476850	7102.259215	27.041946
226.611762	7101.199815	27.046964
226.689627	7103.369248	27.051981
227.016555	7122.351001	27.056999
227.118440	7128.061806	27.062016
227.002486	7141.190335	27.067034
227.299378	7139.130256	27.072052
227.301535	7152.745497	27.077069
227.447783	7158.121095	27.082087
227.833776	7174.549305	27.087104
228.121101	7181.995924	27.092122
228.648561	7193.938369	27.097140
228.573429	7208.462224	27.102157
228.296089	7212.836776	27.107175
228.745587	7217.189718	27.112192
229.027859	7239.240675	27.117210
229.258575	7240.054141	27.122228
229.665910	7253.186515	27.127245
229.424584	7266.003184	27.132263
229.943993	7280.999609	27.137280
230.096096	7283.444779	27.142298
230.147188	7304.704712	27.147316
230.403429	7322.958975	27.152333
230.356146	7336.790401	27.157351
230.763847	7358.184289	27.162368
230.350349	7370.759502	27.167386
230.890158	7390.977448	27.172404
231.821785	7407.264094	27.177421
231.785432	7427.057212	27.182439
231.963433	7427.364325	27.187456
232.579248	7448.609112	27.192474
232.736666	7466.111782	27.197492
233.233749	7469.273546	27.202509
233.149288	7498.172358	27.207527
233.865905	7493.540329	27.212544
233.940506	7508.236835	27.217562
234.154360	7503.405271	27.222580
234.757284	7514.060796	27.227597
234.984600	7537.740151	27.232615
235.188579	7534.040283	27.237632
235.318057	7536.583717	27.242650
235.391515	7550.355466	27.247668
236.062081	7559.292607	27.252685
235.941750	7556.337743	27.257703
236.074344	7567.416939	27.262720
236.260757	7576.590467	27.267738
236.311173	7582.299956	27.272756
236.944695	7600.691485	27.277773
236.882106	7613.025974	27.282791
237.329565	7616.574318	27.287808
237.354746	7623.310586	27.292826
237.429879	7637.587245	27.297844
237.997821	7648.668164	27.302861
237.832056	7675.363761	27.307879
238.462299	7676.137145	27.312896
238.465895	7692.012912	27.317914
238.464634	7702.620550	27.322932
239.278740	7713.019171	27.327949
238.865810	7739.191410	27.332967
239.352013	7735.678019	27.337984
239.253440	7756.409314	27.343002
239.381944	7772.035247	27.348020
239.949736	7789.420667	27.353037
240.015151	7807.083203	27.358055
240.215623	7823.035768	27.363072
240.575585	7840.636695	27.368090
240.936809	7860.210533	27.373108
241.311892	7873.900840	27.378125
241.695880	7882.194541	27.383143
242.236738	7895.028776	27.388160
242.420978	7912.414044	27.393178
242.416555	7913.077890	27.398196
242.825014	7920.164999	27.403213
242.826029	7928.360498	27.408231
243.300599	7934.436564	27.413248
243.878370	7953.932592	27.418266
243.939895	7956.262519	27.423284
244.477873	7951.323551	27.428301
244.434130	7967.699411	27.433319
244.870893	7969.772031	27.438336
245.376085	7969.835639	27.443354
245.352118	7967.206658	27.448372
245.549164	7959.627876	27.453389
245.878491	7978.802716	27.458407
246.287929	7987.799664	27.463424
246.729438	7985.953750	27.468442
246.269319	7991.316659	27.473460
246.502509	7985.727444	27.478477
246.639637	7993.747090	27.483495
246.881130	8006.867940	27.488512
246.522344	8013.761996	27.493530
246.814345	8032.033494	27.498548
247.482205	8035.973800	27.503565
247.738951	8061.186694	27.508583
248.194890	8066.233373	27.513600
248.308181	8072.485697	27.518618
248.509196	8094.218849	27.523636
248.960516	8092.668154	27.528653
249.229737	8104.708225	27.533671
249.279196	8114.263240	27.538688
249.454774	8127.795377	27.543706
249.232315	8146.068159	27.548724
249.389655	8151.982168	27.553741
249.595669	8166.074696	27.558759
250.592808	8203.712119	27.563776
250.756180	8198.420997	27.568794
250.592242	8219.942769	27.573812
250.942634	8238.530554	27.578829
251.357298	8254.008164	27.583847
251.488323	8260.756599	27.588864
251.749854	8276.194928	27.593882
252.029559	8297.455143	27.598900
252.514779	8308.391489	27.603917
252.640652	8321.805226	27.608935
253.078494	8330.106531	27.613952
253.121659	8342.191423	27.618970
253.165275	8366.004625	27.623988
253.746692	8375.912628	27.629005
253.591124	8396.745069	27.634023
254.022425	8405.075840	27.639040
254.522911	8410.747087	27.644058
254.592507	8435.471875	27.649076
255.178050	8442.916777	27.654093
255.486169	8468.150644	27.659111
255.893318	8466.357389	27.664128
256.371479	8467.883766	27.669146
256.264608	8486.786084	27.674164
256.914363	8484.405730	27.679181
256.737492	8496.250315	27.684199
257.006748	8501.607157	27.689216
257.372022	8513.787237	27.694234
257.732614	8537.472385	27.699252
257.911004	8538.117263	27.704269
258.121807	8539.868380	27.709287
258.326732	8560.224992	27.714304
258.561797	8569.751347	27.719322
258.530652	8583.186562	27.724340
258.763515	8592.407035	27.729357
259.172763	8611.472223	27.734375
259.111596	8619.450400	27.739392
259.593421	8633.572958	27.744410
259.886768	8657.754920	27.749428
260.215716	8668.532699	27.754445
260.489310	8680.420926	27.759463
260.880889	8700.795990	27.764480
261.307384	8695.438505	27.769498
261.206443	8721.099468	27.774516
261.726176	8731.342447	27.779533
261.933282	8747.130610	27.784551
262.410390	8749.509592	27.789568
262.859860	8755.577212	27.794586
262.682655	8764.867928	27.799604
262.758281	8767.265218	27.804621
262.822528	8780.003791	27.809639
263.121301	8792.273336	27.814656
263.123104	8805.315259	27.819674
263.749133	8815.327053	27.824692
263.976979	8840.160344	27.829709
264.381549	8846.127642	27.834727
264.661279	8865.235356	27.839744
264.867324	8880.155590	27.844762
264.633956	8893.240502	27.849780
265.264489	8907.311705	27.854797
265.532776	8912.274176	27.859815
265.821299	8937.132879	27.864832
266.025964	8946.039050	27.869850
266.164828	8964.531056	27.874868
266.569125	8986.252552	27.879885
266.746106	8994.657914	27.884903
266.712856	9014.228093	27.889920
267.296925	9026.623864	27.894938
267.709276	9047.441234	27.899956
268.069051	9058.672229	27.904973
268.629987	9076.239891	27.909991
268.721477	9087.799973	27.915008
268.881236	9091.263955	27.920026
269.164107	9111.811097	27.925044
269.503637	9123.076855	27.930061
269.698491	9136.628830	27.935079
269.775848	9152.052365	27.940096
270.306214	9166.335105	27.945114
270.433653	9180.923688	27.950132
270.844070	9199.844071	27.955149
271.134402	9203.546634	27.960167
271.265282	9213.181099	27.965184
271.742144	9221.022099	27.970202
272.033874	9241.413305	27.975220
272.419798	9259.232548	27.980237
272.879493	9273.583203	27.985255
272.474050	9281.858368	27.990272
273.266039	9284.974538	27.995290
273.768825	9299.634224	28.000308
274.198351	9312.461525	28.005325
274.240109	9309.174896	28.010343
274.434194	9312.500973	28.015360
275.461351	9318.194694	28.020378
275.245161	9323.014856	28.025396
275.411948	9330.629501	28.030413
275.906848	9335.383161	28.035431
275.752215	9355.809256	28.040448
276.200933	9354.025233	28.045466
276.325669	9361.182329	28.050484
276.654909	9374.003186	28.055501
276.659550	9378.801611	28.060519
276.409895	9397.455567	28.065536
277.103151	9408.827447	28.070554
277.010328	9430.866808	28.075572
277.211399	9451.054512	28.080589
277.586062	9466.798259	28.085607
278.196893	9494.670036	28.090624
278.393072	9508.158933	28.095642
278.466131	9522.551032	28.100660
278.262515	9539.038417	28.105677
278.632529	9570.720694	28.110695
279.459346	9597.359249	28.115712
280.027208	9615.914563	28.120730
280.468867	9617.563541	28.125748
280.964856	9622.733863	28.130765
281.139685	9633.542515	28.135783
281.186457	9637.144165	28.140800
281.713248	9633.377838	28.145818
281.841057	9660.731502	28.150836
282.042292	9658.335586	28.155853
282.153720	9666.211568	28.160871
282.458940	9677.211482	28.165888
283.441313	9669.156127	28.170906
283.418975	9681.668848	28.175924
283.613860	9692.619646	28.180941
284.058026	9699.332485	28.185959
284.290553	9721.703567	28.190976
284.637151	9725.312229	28.195994
284.653880	9729.698419	28.201012
284.398858	9734.234264	28.206029
284.848144	9747.838636	28.211047
285.084531	9770.199704	28.216064
285.362057	9783.073097	28.221082
285.552845	9805.431834	28.226100
285.283899	9827.751668	28.231117
286.097348	9840.077545	28.236135
286.021349	9861.647519	28.241152
286.142553	9887.442845	28.246170
286.660576	9898.886511	28.251188
286.928863	9926.174493	28.256205
287.620541	9944.417232	28.261223
287.621793	9966.057390	28.266240
288.145752	9979.767127	28.271258
288.724709	10010.438860	28.276276
288.749307	10015.572175	28.281293
289.481245	10034.449670	28.286311
290.087925	10042.656002	28.291328
290.509086	10034.820472	28.296346
291.336884	10050.181595	28.301364
291.059191	10054.010650	28.306381
291.414227	10055.325849	28.311399
291.221754	10069.838644	28.316416
291.753690	10067.185965	28.321434
292.249635	10076.356749	28.326452
292.144951	10091.490516	28.331469
292.556585	10098.435893	28.336487
292.799064	10109.060637	28.341504
293.044845	10125.500678	28.346522
293.204192	10141.177486	28.351540
293.488132	10162.012944	28.356557
293.628315	10165.063406	28.361575
294.324002	10186.898812	28.366592
294.062191	10192.995553	28.371610
294.540469	10213.320896	28.376628
294.565114	10233.991576	28.381645
295.091860	10248.588294	28.386663
295.511015	10272.405467	28.391680
295.257858	10287.313077	28.396698
296.057469	10304.491124	28.401716
296.388954	10312.677273	28.406733
297.061847	10326.809269	28.411751
296.915274	10345.855426	28.416768
297.528937	10363.693952	28.421786
297.819933	10367.863937	28.426804
297.852045	10386.876002	28.431821
297.987519	10394.852743	28.436839
298.528927	10416.327238	28.441856
298.576277	10431.841756	28.446874
298.951585	10444.454109	28.451892
299.267945	10464.912287	28.456909
299.609522	10468.768154	28.461927
299.641479	10491.089295	28.466944
300.158616	10507.162216	28.471962
300.418101	10504.990771	28.476980
300.518958	10530.821731	28.481997
300.853924	10542.764747	28.487015
301.314046	10559.825385	28.492032
301.640229	10572.638075	28.497050
302.030000	10587.594227	28.502068
302.085124	10595.056276	28.507085
302.477416	10612.253818	28.512103
302.834419	10626.804640	28.517120
302.782435	10639.941474	28.522138
303.659009	10657.202589	28.527156
303.822477	10668.509327	28.532173
303.950415	10692.422895	28.537191
304.271615	10708.144445	28.542208
304.461557	10723.886444	28.547226
304.703669	10747.908605	28.552244
305.144003	10769.449762	28.557261
305.303538	10790.336866	28.562279
305.281071	10806.102530	28.567296
305.935661	10817.295009	28.572314
306.262214	10844.155325	28.577332
306.342495	10864.896977	28.582349
306.812024	10877.087643	28.587367
306.781245	10896.416291	28.592384
307.523703	10917.945316	28.597402
307.539318	10940.193759	28.602420
308.153586	10980.229809	28.607437
308.549718	10986.132808	28.612455
309.087100	10992.594794	28.617472
309.481422	11009.830277	28.622490
310.443697	11024.047210	28.627508
310.434829	11031.026827	28.632525
310.683584	11037.925293	28.637543
310.995450	11048.571346	28.642560
311.454265	11050.953480	28.647578
311.893473	11060.859808	28.652596
312.248381	11068.932132	28.657613
312.769742	11074.054708	28.662631
312.708895	11098.061336	28.667648
312.888483	11102.624574	28.672666
313.171416	11102.624927	28.677684
313.065647	11122.262288	28.682701
313.829209	11133.750586	28.687719
313.810927	11147.567707	28.692736
314.119816	11167.604714	28.697754
314.087124	11181.550405	28.702772
314.549991	11199.823686	28.707789
314.758526	11215.013796	28.712807
314.866904	11246.802809	28.717824
315.311407	11265.407395	28.722842
315.948892	11290.748540	28.727860
316.226542	11301.968420	28.732877
316.424034	11317.406620	28.737895
316.986082	11344.815137	28.742912
317.075749	11353.645640	28.747930
317.839322	11363.217451	28.752948
317.817226	11371.601204	28.757965
318.342148	11391.260646	28.762983
318.497476	11413.090048	28.768000
318.480713	11433.506424	28.773018
319.289598	11446.680308	28.778036
319.728692	11459.422351	28.783053
319.879227	11463.646027	28.788071
319.825787	11481.614742	28.793088
319.696735	11511.196141	28.798106
320.416747	11519.262341	28.803124
321.052179	11551.313991	28.808141
320.979694	11561.975969	28.813159
321.258184	11577.739635	28.818176
321.613795	11604.353385	28.823194
322.671418	11615.575170	28.828212
322.543218	11635.526005	28.833229
322.811184	11636.153891	28.838247
323.264856	11653.159697	28.843264
323.523443	11674.259713	28.848282
323.800739	11684.494709	28.853300
323.823006	11699.439501	28.858317
324.263995	11721.903674	28.863335
324.541620	11738.978015	28.868352
324.847651	11758.769807	28.873370
325.341143	11777.730402	28.878388
325.343499	11796.094906	28.883405
325.838367	11810.593612	28.888423
326.174331	11836.689745	28.893440
326.275195	11864.249762	28.898458
326.829285	11874.441769	28.903476
327.202040	11892.271900	28.908493
327.633512	11905.091217	28.913511
327.910932	11926.011757	28.918528
328.418619	11958.140829	28.923546
329.010771	11965.671384	28.928564
329.443271	11988.219297	28.933581
329.344306	11998.730920	28.938599
329.793751	12015.655615	28.943616
330.325189	12029.845663	28.948634
330.685742	12021.984010	28.953652
331.406315	12059.419703	28.958669
331.528183	12056.325367	28.963687
331.910975	12068.233496	28.968704
332.137297	12087.933842	28.973722
332.667629	12096.424532	28.978740
332.598830	12115.766672	28.983757
333.141869	12133.535788	28.988775
333.484949	12145.857488	28.993792
333.482543	12164.324139	28.998810
333.850641	12170.080311	29.003828
334.247403	12192.817179	29.008845
334.596298	12210.000846	29.013863
335.201351	12210.611008	29.018880
335.367838	12224.071758	29.023898
336.171627	12244.156019	29.028916
335.936981	12254.486816	29.033933
336.567441	12267.250140	29.038951
336.738505	12275.414762	29.043968
336.894718	12306.212922	29.048986
336.975743	12319.927030	29.054004
337.338791	12341.150472	29.059021
337.825587	12356.222402	29.064039
338.344433	12371.440925	29.069056
338.444115	12393.456963	29.074074
339.083482	12407.696807	29.079092
339.457246	12425.056789	29.084109
339.656028	12437.536927	29.089127
340.050705	12452.904314	29.094144
340.000483	12477.918365	29.099162
340.343826	12483.312191	29.104180
340.987112	12511.142377	29.109197
341.097749	12522.385832	29.114215
341.454264	12541.059066	29.119232
342.031078	12564.355693	29.124250
342.267253	12581.933020	29.129268
342.307092	12599.859862	29.134285
343.188548	12624.640644	29.139303
343.224507	12635.977895	29.144320
343.424628	12657.779667	29.149338
344.116906	12661.316141	29.154356
344.298918	12683.790207	29.159373
344.507349	12700.967770	29.164391
345.055827	12715.209367	29.169408
345.104852	12729.541363	29.174426
345.454722	12745.670672	29.179444
345.762238	12764.916999	29.184461
346.092262	12796.115199	29.189479
346.541285	12799.616942	29.194496
346.516317	12824.659099	29.199514
346.809443	12851.915903	29.204532
347.430621	12874.966016	29.209549
347.484173	12892.237337	29.214567
347.628598	12922.217311	29.219584
348.017261	12946.434203	29.224602
348.866126	12965.991182	29.229620
349.173628	12984.849325	29.234637
349.337022	13012.660229	29.239655
350.032133	13029.632854	29.244672
350.135975	13058.545703	29.249690
350.350205	13079.130002	29.254708
350.820578	13103.129116	29.259725
350.878964	13121.230405	29.264743
351.869021	13141.337154	29.269760
352.123277	13164.327905	29.274778
352.616750	13185.181473	29.279796
352.795193	13208.171448	29.284813
353.473728	13235.406699	29.289831
353.918034	13245.379707	29.294848
353.793269	13270.201152	29.299866
354.421827	13295.454818	29.304884
354.241009	13321.229257	29.309901
355.130912	13340.792869	29.314919
355.525206	13356.991575	29.319936
355.586785	13378.345224	29.324954
356.204530	13398.466001	29.329972
356.540003	13417.945482	29.334989
356.814091	13441.975586	29.340007
357.154143	13452.514407	29.345024
357.800651	13481.084471	29.350042
357.920817	13494.278602	29.355060
358.539364	13522.234134	29.360077
358.861282	13533.922142	29.365095
359.001712	13557.562673	29.370112
359.417933	13584.750845	29.375130
359.903632	13581.571197	29.380148
360.708194	13599.032563	29.385165
360.892241	13615.542119	29.390183
361.655277	13616.686691	29.395200
361.805691	13639.425764	29.400218
361.980350	13651.582038	29.405236
362.598650	13659.497632	29.410253
362.648366	13678.238704	29.415271
362.857152	13694.106576	29.420288
362.907224	13709.351793	29.425306
363.550664	13733.602664	29.430324
363.959627	13751.981561	29.435341
363.963177	13777.172119	29.440359
364.418729	13790.187925	29.445376
364.545633	13814.759320	29.450394
364.710369	13838.200624	29.455412
365.737357	13863.838294	29.460429
365.568537	13896.009675	29.465447
366.358769	13919.476862	29.470464
366.604320	13935.070784	29.475482
367.090263	13952.001014	29.480500
367.585383	13967.069781	29.485517
368.119195	13984.861031	29.490535
368.670407	14004.051734	29.495552
368.906134	14013.170228	29.500570
368.992807	14023.114059	29.505588
369.613882	14031.951511	29.510605
369.269685	14054.831244	29.515623
370.007857	14070.215950	29.520640
370.215440	14093.432997	29.525658
370.374644	14108.885764	29.530676
370.565460	14129.225369	29.535693
370.921379	14154.127878	29.540711
371.838644	14164.103534	29.545728
372.270123	14190.819658	29.550746
372.660048	14209.615663	29.555764
373.193185	14222.360731	29.560781
373.566368	14245.517446	29.565799
373.712511	14254.754217	29.570816
373.806581	14279.252374	29.575834
374.354651	14301.548211	29.580852
374.909007	14321.341931	29.585869
375.008020	14346.663653	29.590887
375.331203	14360.591027	29.595904
375.822234	14385.381222	29.600922
376.027009	14407.800106	29.605940
376.704732	14424.404045	29.610957
377.149616	14445.538162	29.615975
377.385262	14466.404861	29.620992
378.280974	14485.491891	29.626010
378.334141	14504.410093	29.631028
378.831993	14519.643095	29.636045
378.795385	14542.901866	29.641063
379.231370	14569.633613	29.646080
379.610485	14592.088734	29.651098
379.985640	14612.182251	29.656116
380.381993	14630.579754	29.661133
380.508317	14664.045514	29.666151
380.539105	14684.454840	29.671168
381.349685	14714.687648	29.676186
381.387173	14740.332124	29.681204
382.121630	14768.811488	29.686221
382.425555	14796.432593	29.691239
383.137647	14820.598374	29.696256
383.460099	14842.869967	29.701274
383.788422	14873.105469	29.706292
384.589106	14889.744362	29.711309
384.478858	14912.269729	29.716327
385.120356	14932.625301	29.721344
385.376113	14957.632885	29.726362
385.609339	14979.934320	29.731380
386.418872	15000.737527	29.736397
386.616410	15029.300870	29.741415
386.919350	15048.196518	29.746432
387.640377	15060.524446	29.751450
387.843178	15093.344264	29.756468
388.438185	15112.241878	29.761485
388.850077	15128.300400	29.766503
389.532004	15147.512968	29.771520
389.774394	15163.064176	29.776538
390.513442	15173.216548	29.781556
390.914180	15185.243863	29.786573
391.089634	15196.507238	29.791591
391.434412	15209.926565	29.796608
391.854012	15225.361807	29.801626
391.912180	15256.135810	29.806644
392.218926	15270.006404	29.811661
392.683263	15290.437313	29.816679
392.877074	15303.119082	29.821696
393.550950	15327.752555	29.826714
393.753876	15342.984760	29.831732
394.413405	15361.187247	29.836749
394.453527	15379.429333	29.841767
394.789311	15390.497319	29.846784
395.337635	15400.840575	29.851802
395.936667	15427.586042	29.856820
396.431886	15428.257640	29.861837
396.725473	15448.753200	29.866855
397.156761	15459.471587	29.871872
396.948981	15477.401798	29.876890
397.352054	15484.145225	29.881908
398.422095	15514.212582	29.886925
398.461421	15532.120166	29.891943
399.044183	15550.082126	29.896960
399.861209	15570.366840	29.901978
399.847808	15589.192259	29.906996
400.113995	15604.519047	29.912013
400.462164	15627.040213	29.917031
400.822814	15644.525204	29.922048
400.692367	15667.158829	29.927066
401.189504	15695.720743	29.932084
401.898980	15730.616713	29.937101
402.154978	15745.762020	29.942119
402.674330	15763.749845	29.947136
403.434533	15789.744326	29.952154
403.393473	15813.330640	29.957172
404.100352	15831.586213	29.962189
404.181476	15856.088412	29.967207
404.458658	15878.355630	29.972224
405.319450	15906.270644	29.977242
405.503747	15937.578810	29.982260
405.983426	15958.668132	29.987277
406.151960	15985.727750	29.992295
406.838885	16008.777758	29.997312
407.284992	16041.532902	30.002330
407.493123	16066.309320	30.007348
407.804061	16088.770503	30.012365
408.453903	16113.591916	30.017383
408.456657	16146.593127	30.022400
409.029593	16174.843915	30.027418
409.407086	16204.518002	30.032436
409.943848	16225.216572	30.037453
410.292564	16260.605525	30.042471
410.665157	16292.159733	30.047488
411.302024	16311.244680	30.052506
411.693046	16331.009069	30.057524
411.975811	16364.841931	30.062541
412.268360	16395.177004	30.067559
412.425417	16419.709160	30.072576
413.090339	16449.964240	30.077594
413.481164	16480.843183	30.082612
414.186431	16510.324588	30.087629
414.263466	16546.012193	30.092647
414.562151	16575.222203	30.097664
415.342404	16596.562326	30.102682
415.788196	16627.417155	30.107700
416.070015	16659.513555	30.112717
416.714489	16689.557423	30.117735
417.125118	16714.050479	30.122752
417.325849	16734.795596	30.127770
417.838433	16761.903816	30.132788
418.319239	16779.301652	30.137805
418.598061	16815.258395	30.142823
418.957731	16850.839395	30.147840
419.778996	16872.887252	30.152858
420.231658	16896.236951	30.157876
420.906803	16915.528159	30.162893
420.945592	16934.735264	30.167911
421.311128	16963.951250	30.172928
421.804026	16985.033328	30.177946
422.064271	16997.096291	30.182964
422.451988	17017.945260	30.187981
423.190250	17036.993037	30.192999
423.188006	17066.282227	30.198016
423.793790	17080.774022	30.203034
423.880903	17112.598274	30.208052
424.440731	17126.667702	30.213069
425.204866	17158.471911	30.218087
425.363839	17186.693880	30.223104
426.365473	17204.778537	30.228122
426.344896	17233.028526	30.233140
426.664830	17253.629305	30.238157
427.018456	17285.690301	30.243175
427.229509	17302.309391	30.248192
427.695965	17330.673213	30.253210
428.046989	17360.444804	30.258228
428.427463	17388.092474	30.263245
428.883099	17418.176356	30.268263
429.517851	17446.542576	30.273280
430.085740	17477.730361	30.278298
430.104473	17514.130035	30.283316
430.954075	17537.235521	30.288333
431.106909	17580.316921	30.293351
431.720174	17607.107435	30.298368
432.706899	17631.938381	30.303386
433.045460	17645.303529	30.308404
433.514075	17672.805225	30.313421
434.079211	17688.529340	30.318439
434.651055	17707.335210	30.323456
435.128694	17729.011136	30.328474
435.711778	17738.200519	30.333492
436.432960	17742.017739	30.338509
436.665600	17763.479157	30.343527
437.140639	17776.437799	30.348544
437.316424	17795.697081	30.353562
437.883812	17815.293403	30.358580
438.338125	17831.786637	30.363597
438.685219	17853.388268	30.368615
438.828630	17873.549715	30.373632
439.458100	17895.833916	30.378650
439.847153	17922.868245	30.383668
440.163617	17951.954389	30.388685
440.506834	17969.747442	30.393703
440.569998	18008.349017	30.398720
441.095063	18030.763339	30.403738
441.634328	18064.205486	30.408756
441.757406	18089.683177	30.413773
442.257446	18116.302507	30.418791
442.483788	18155.087442	30.423808
443.255211	18181.247669	30.428826
443.768725	18219.495274	30.433844
443.947400	18243.701042	30.438861
444.720674	18268.313345	30.443879
444.723448	18295.067191	30.448896
445.202176	18328.329698	30.453914
446.038197	18365.661901	30.458932
446.469973	18389.986384	30.463949
446.909515	18423.419407	30.468967
447.316923	18448.916480	30.473984
448.087343	18478.406551	30.479002
448.168547	18504.933685	30.484020
448.576045	18525.755934	30.489037
449.282489	18553.575637	30.494055
449.725711	18588.448754	30.499072
450.438326	18608.648702	30.504090
450.775915	18633.664125	30.509108
450.906389	18658.932935	30.514125
451.650694	18682.830082	30.519143
452.068017	18707.801599	30.524160
452.640297	18724.131928	30.529178
452.791286	18743.301250	30.534196
453.219506	18762.553782	30.539213
453.767026	18786.841792	30.544231
453.581306	18812.387458	30.549248
454.132321	18847.901285	30.554266
454.369658	18872.654650	30.559284
454.826582	18910.148002	30.564301
455.978941	18948.512389	30.569319
456.115173	18979.201214	30.574336
456.288831	18995.037879	30.579354
457.046520	19022.850279	30.584372
457.350768	19051.358754	30.589389
458.261249	19079.804482	30.594407
458.565965	19119.381483	30.599424
459.121663	19142.771559	30.604442
459.782291	19177.447630	30.609460
460.010177	19200.118053	30.614477
460.465903	19220.320727	30.619495
460.695864	19258.128062	30.624512
461.098309	19278.825553	30.629530
461.590458	19318.329555	30.634548
461.952124	19349.445061	30.639565
463.246240	19372.669917	30.644583
463.375819	19405.748552	30.649600
464.176259	19431.046739	30.654618
464.540170	19459.824506	30.659636
464.669379	19482.074695	30.664653
465.356585	19507.346384	30.669671
465.916559	19537.869038	30.674688
466.503309	19564.558989	30.679706
466.821146	19592.706028	30.684724
467.007547	19626.148941	30.689741
467.402643	19651.497883	30.694759
467.646670	19684.123243	30.699776
467.976964	19714.574527	30.704794
468.577051	19749.532709	30.709812
468.881879	19783.134354	30.714829
469.670481	19815.011779	30.719847
470.333352	19859.418242	30.724864
470.912851	19880.922771	30.729882
471.060896	19906.651671	30.734900
471.785281	19937.117766	30.739917
472.448776	19964.649236	30.744935
472.546289	20003.584271	30.749952
472.750842	20029.235038	30.754970
473.417457	20056.747199	30.759988
473.873338	20103.707304	30.765005
474.223273	20133.473843	30.770023
474.852413	20163.298049	30.775040
475.299445	20201.389317	30.780058
476.024124	20236.657512	30.785076
476.082290	20274.999002	30.790093
476.803411	20307.746989	30.795111
477.395104	20340.262459	30.800128
477.706926	20382.406040	30.805146
478.217821	20406.581731	30.810164
478.522268	20442.048396	30.815181
479.396863	20468.107192	30.820199
479.600167	20504.202571	30.825216
480.609505	20536.596486	30.830234
481.399538	20553.924305	30.835252
481.916320	20586.060123	30.840269
483.131327	20596.542479	30.845287
483.430430	20616.139170	30.850304
483.672035	20634.790794	30.855322
484.189307	20652.887750	30.860340
484.362455	20662.723614	30.865357
484.997715	20669.018879	30.870375
485.108147	20700.990692	30.875392
485.641854	20717.941564	30.880410
485.649425	20738.967441	30.885428
486.011258	20763.628006	30.890445
486.670122	20788.090724	30.895463
486.875573	20829.980146	30.900480
487.462355	20846.878640	30.905498
487.814361	20871.484006	30.910516
488.320573	20917.079811	30.915533
488.944289	20941.131190	30.920551
489.017634	20967.985123	30.925568
489.411360	21004.955287	30.930586
489.976951	21045.177948	30.935604
490.793786	21080.774505	30.940621
491.312907	21115.785645	30.945639
491.998133	21143.928269	30.950656
492.433763	21163.112518	30.955674
493.111019	21193.701639	30.960692
493.336032	21230.559490	30.965709
494.031737	21254.903326	30.970727
494.213290	21292.955908	30.975744
494.685588	21333.117861	30.980762
495.140441	21356.305148	30.985780
495.198479	21410.564853	30.990797
495.958456	21439.258599	30.995815
496.239944	21474.623293	31.000832
496.685122	21524.027370	31.005850
497.714612	21556.167100	31.010868
498.205011	21594.222730	31.015885
498.725630	21632.924531	31.020903
498.853330	21676.458021	31.025920
499.500866	21706.306987	31.030938
499.973078	21744.953359	31.035956
500.579122	21788.349444	31.040973
501.142969	21819.481630	31.045991
501.622036	21860.073264	31.051008
502.309171	21901.833113	31.056026
502.874482	21928.333751	31.061044
503.342862	21967.587737	31.066061
503.910056	21993.544774	31.071079
504.918983	22040.739344	31.076096
504.868323	22075.777708	31.081114
505.386147	22102.317567	31.086132
506.056555	22142.835765	31.091149
506.349589	22161.784124	31.096167
506.947723	22205.182358	31.101184
507.580592	22244.487112	31.106202
508.233945	22280.338764	31.111220
508.173420	22315.600242	31.116237
508.619765	22342.581221	31.121255
509.229206	22392.315747	31.126272
509.689263	22419.098816	31.131290
510.505847	22465.231209	31.136308
510.618459	22500.377600	31.141325
511.586531	22527.328161	31.146343
512.291378	22574.463927	31.151360
512.539439	22611.358682	31.156378
513.508714	22633.993482	31.161396
513.451872	22678.821664	31.166413
514.414861	22697.533546	31.171431
514.862330	22728.084998	31.176448
515.207084	22768.155989	31.181466
515.831972	22794.541097	31.186484
516.078894	22833.723859	31.191501
516.943879	22863.705015	31.196519
517.343229	22888.046456	31.201536
517.637926	22918.065925	31.206554
518.342433	22939.990349	31.211572
518.670389	22978.301415	31.216589
519.235058	23005.542910	31.221607
519.832308	23040.930757	31.226624
520.232083	23071.509120	31.231642
521.055988	23101.162129	31.236660
522.151015	23116.315257	31.241677
522.428213	23132.903733	31.246695
523.053715	23145.033698	31.251712
523.597456	23172.784196	31.256730
524.059158	23186.917518	31.261748
524.609428	23211.905672	31.266765
525.574996	23232.646049	31.271783
525.842841	23250.588339	31.276800
526.214616	23277.171468	31.281818
527.039891	23300.278099	31.286836
527.234757	23319.489291	31.291853
527.732967	23345.079703	31.296871
528.453993	23377.984474	31.301888
528.362390	23411.300162	31.306906
529.165437	23432.792738	31.311924
529.011807	23470.977517	31.316941
529.804505	23499.669169	31.321959
530.487633	23539.360451	31.326976
530.372294	23577.488921	31.331994
531.134101	23615.025939	31.337012
531.579520	23658.975618	31.342029
532.171652	23701.891495	31.347047
532.741969	23726.276861	31.352064
533.039093	23775.501076	31.357082
533.637067	23811.673760	31.362100
534.367314	23859.194095	31.367117
534.830564	23895.792331	31.372135
535.377637	23937.742578	31.377152
535.737238	23976.492985	31.382170
536.595485	24015.627143	31.387188
536.852804	24054.437859	31.392205
537.610765	24098.434641	31.397223
538.523520	24128.467148	31.402240
538.964210	24178.478872	31.407258
540.391364	24198.213152	31.412276
540.813900	24218.729455	31.417293
541.436694	24242.399525	31.422311
541.969679	24264.971408	31.427328
542.333641	24300.814892	31.432346
542.946424	24327.153368	31.437364
543.124080	24357.022608	31.442381
543.295001	24384.712770	31.447399
543.853290	24416.285937	31.452416
544.211631	24468.308120	31.457434
544.575765	24498.028472	31.462452
545.104230	24536.305003	31.467469
545.874073	24574.183826	31.472487
547.170946	24611.045403	31.477504
547.354633	24651.157900	31.482522
547.995120	24680.431060	31.487540
548.470125	24720.599455	31.492557
548.725097	24758.779961	31.497575
549.347924	24784.795187	31.502592
549.560676	24822.521066	31.507610
550.361801	24863.688013	31.512628
550.844561	24913.442248	31.517645
551.196910	24945.105186	31.522663
552.003372	24983.971248	31.527680
552.455464	25013.817703	31.532698
553.271114	25058.117277	31.537716
553.822470	25087.752484	31.542733
553.690889	25127.896055	31.547751
554.606982	25148.835726	31.552768
555.156287	25194.371463	31.557786
555.620510	25223.552786	31.562804
556.198037	25255.099004	31.567821
556.499954	25289.456170	31.572839
557.538435	25329.563347	31.577856
557.635889	25372.149047	31.582874
558.216332	25398.519250	31.587892
558.982288	25443.421459	31.592909
559.681039	25482.096707	31.597927
560.177803	25501.105008	31.602944
561.076976	25538.365153	31.607962
561.673341	25567.216740	31.612980
562.171077	25604.874447	31.617997
562.843651	25647.042572	31.623015
564.080145	25662.106112	31.628032
564.270777	25695.438541	31.633050
564.559912	25725.583174	31.638068
565.181271	25763.215613	31.643085
566.004472	25785.447005	31.648103
566.558590	25808.131097	31.653120
566.832025	25838.594332	31.658138
567.835214	25873.715459	31.663156
568.276797	25908.576486	31.668173
568.635417	25932.909025	31.673191
569.296540	25957.289299	31.678208
570.109128	25998.425193	31.683226
571.128944	26028.842043	31.688244
571.888099	26045.857179	31.693261
571.668975	26079.247712	31.698279
572.204049	26109.177677	31.703296
572.482860	26139.413015	31.708314
573.381852	26164.287381	31.713332
573.972292	26202.494247	31.718349
574.185585	26244.343290	31.723367
574.809256	26274.841142	31.728384
575.196919	26315.942717	31.733402
575.821708	26351.073026	31.738420
576.405447	26398.622197	31.743437
576.775877	26430.670179	31.748455
577.180868	26476.149126	31.753472
577.867299	26525.875647	31.758490
578.154873	26567.549476	31.763508
578.611677	26613.399868	31.768525
579.338504	26667.683513	31.773543
579.926819	26704.602370	31.778560
580.318625	26761.883572	31.783578
580.851957	26810.143087	31.788596
581.701055	26859.623902	31.793613
581.749133	26902.359562	31.798631
582.673371	26960.241012	31.803648
583.244420	27010.056207	31.808666
583.919018	27058.837858	31.813684
584.328828	27100.285189	31.818701
585.088501	27155.392974	31.823719
585.596352	27195.889849	31.828736
586.329795	27249.649448	31.833754
587.485190	27289.767615	31.838772
588.061596	27327.827107	31.843789
588.440489	27373.659748	31.848807
589.073714	27416.880545	31.853824
589.736999	27453.378279	31.858842
590.331951	27500.675482	31.863860
591.139046	27537.327949	31.868877
591.565096	27582.351040	31.873895
592.533416	27613.707388	31.878912
593.101973	27636.403930	31.883930
593.248118	27666.137613	31.888948
594.513951	27690.248875	31.893965
594.634386	27728.304258	31.898983
595.264914	27764.738128	31.904000
595.827043	27792.372072	31.909018
596.496485	27826.037980	31.914036
597.075304	27856.753774	31.919053
596.943094	27902.395396	31.924071
598.120165	27937.031656	31.929088
599.075276	27964.851155	31.934106
599.546737	27988.783055	31.939124
600.022912	28020.444184	31.944141
600.715130	28054.050040	31.949159
601.789737	28089.511534	31.954176
601.989365	28128.522372	31.959194
602.412389	28174.501642	31.964212
602.879938	28201.341840	31.969229
603.222187	28245.254391	31.974247
603.944898	28279.658582	31.979264
604.565024	28318.515836	31.984282
604.630212	28367.363898	31.989300
605.458687	28416.061650	31.994317
606.032506	28464.767558	31.999335
606.671299	28504.905345	32.004352
607.359971	28556.159765	32.009370
607.913498	28612.864793	32.014388
608.635713	28659.019802	32.019405
609.278642	28700.339295	32.024423
609.769912	28742.820206	32.029440
610.576238	28791.256833	32.034458
610.425212	28836.555833	32.039476
612.032759	28881.732867	32.044493
613.076906	28913.477626	32.049511
613.787787	28943.523464	32.054528
615.090169	28982.522285	32.059546
615.699776	29014.398055	32.064564
616.441079	29028.441399	32.069581
616.641104	29082.345768	32.074599
617.164117	29100.411568	32.079616
617.917824	29129.117324	32.084634
618.007359	29167.243409	32.089652
618.795080	29199.129664	32.094669
619.133077	29237.880890	32.099687
619.610335	29284.846590	32.104704
620.320360	29327.376833	32.109722
620.526165	29365.655851	32.114740
621.042168	29411.060871	32.119757
621.538939	29464.047764	32.124775
622.220323	29505.539884	32.129792
622.622345	29548.794874	32.134810
623.182578	29608.908608	32.139828
624.078499	29656.277736	32.144845
624.757709	29706.424020	32.149863
625.471961	29761.128739	32.154880
626.017171	29804.336693	32.159898
626.516386	29861.900653	32.164916
627.265273	29903.326180	32.169933
627.818103	29954.896018	32.174951
628.497050	30005.384411	32.179968
628.823868	30048.728014	32.184986
629.441144	30100.958222	32.190004
630.569753	30149.708196	32.195021
631.310708	30201.451642	32.200039
631.707925	30255.214610	32.205056
632.503909	30294.497043	32.210074
632.826730	30348.853385	32.215092
633.521409	30380.996169	32.220109
633.895367	30437.746840	32.225127
634.153175	30472.214449	32.230144
635.094266	30520.286516	32.235162
635.961733	30571.486535	32.240180
636.749996	30611.876996	32.245197
637.523174	30653.919739	32.250215
637.937734	30692.326758	32.255232
638.407080	30734.195718	32.260250
639.219237	30788.160976	32.265268
640.210834	30836.295452	32.270285
640.720596	30873.701860	32.275303
640.873310	30923.408398	32.280320
642.040243	30969.429840	32.285338
642.464060	31012.507514	32.290356
643.391361	31050.923880	32.295373
643.786147	31100.163304	32.300391
644.941039	31148.209873	32.305408
645.369757	31181.071702	32.310426
645.771572	31230.202876	32.315444
646.925535	31266.833316	32.320461
647.278698	31313.323566	32.325479
647.735558	31356.832995	32.330496
648.594983	31399.995380	32.335514
649.128823	31454.283851	32.340532
649.909293	31493.210656	32.345549
650.438584	31548.024768	32.350567
650.763570	31597.472208	32.355584
651.528145	31652.117215	32.360602
651.979437	31698.630982	32.365620
652.736567	31745.653546	32.370637
653.352307	31802.401930	32.375655
653.854199	31857.979722	32.380672
654.810553	31909.403120	32.385690
655.228700	31962.591996	32.390708
655.871976	32022.845229	32.395725
656.653936	32070.003739	32.400743
657.575041	32127.173281	32.405760
657.956828	32169.653016	32.410778
658.164027	32233.546529	32.415796
659.282975	32289.307574	32.420813
660.248781	32351.483947	32.425831
660.554821	32410.115523	32.430848
661.420636	32447.052103	32.435866
661.938137	32502.344705	32.440884
662.812832	32556.285867	32.445901
663.443985	32610.163931	32.450919
664.232353	32668.164823	32.455936
665.050231	32706.196692	32.460954
665.775374	32757.234613	32.465972
666.826893	32799.927471	32.470989
667.365658	32848.118148	32.476007
668.463912	32901.829422	32.481024
669.086370	32936.882879	32.486042
669.799317	32974.160292	32.491060
670.567425	33007.737137	32.496077
671.164345	33047.327628	32.501095
671.884831	33090.780680	32.506112
672.766002	33124.352756	32.511130
673.181180	33165.331000	32.516148
673.786194	33205.483193	32.521165
674.708651	33248.532131	32.526183
675.082529	33293.816064	32.531200
675.851245	33330.725073	32.536218
676.868992	33356.980567	32.541236
677.729726	33390.499355	32.546253
678.054015	33430.069791	32.551271
678.604058	33470.357493	32.556288
679.252242	33506.368866	32.561306
679.758642	33549.641247	32.566324
680.216909	33579.556137	32.571341
680.099497	33611.596428	32.576359
681.039002	33658.582276	32.581376
681.697815	33714.115297	32.586394
682.552807	33755.942952	32.591412
682.778765	33795.896074	32.596429
683.770005	33846.705566	32.601447
684.328026	33889.736689	32.606464
685.187901	33935.123377	32.611482
685.538367	33983.295403	32.616500
686.157269	34039.303347	32.621517
687.091747	34085.677672	32.626535
687.206282	34150.685227	32.631552
688.344016	34189.814350	32.636570
688.598498	34241.599329	32.641588
689.510197	34298.371647	32.646605
690.702818	34357.553481	32.651623
691.374198	34395.958963	32.656640
692.927895	34421.266192	32.661658
693.860105	34465.808208	32.666676
694.543646	34505.229909	32.671693
695.363956	34546.596679	32.676711
695.567128	34590.746651	32.681728
696.314399	34619.005803	32.686746
696.795920	34665.142118	32.691764
697.564293	34702.698492	32.696781
698.414050	34756.427919	32.701799
698.608414	34808.761067	32.706816
699.393602	34847.889395	32.711834
699.844096	34908.465461	32.716852
700.378403	34961.043228	32.721869
701.138894	35007.098928	32.726887
701.920071	35064.140212	32.731904
702.198175	35115.493723	32.736922
703.163907	35169.465377	32.741940
703.634457	35232.859152	32.746957
704.545552	35287.554074	32.751975
704.892892	35351.492167	32.756992
705.718030	35400.029806	32.762010
706.803844	35466.622639	32.767028
707.170132	35526.574988	32.772045
708.392870	35584.965237	32.777063
708.752814	35636.585474	32.782080
709.482639	35690.829125	32.787098
710.282558	35746.503607	32.792116
711.242957	35806.503365	32.797133
711.758108	35852.403091	32.802151
712.622030	35913.979916	32.807168
713.572059	35966.419591	32.812186
714.123906	36020.476814	32.817204
714.952847	36079.511436	32.822221
715.842719	36123.121425	32.827239
716.638144	36183.116316	32.832256
717.258426	36228.633759	32.837274
717.802278	36278.962337	32.842292
718.429736	36331.162271	32.847309
719.050362	36379.866773	32.852327
719.829688	36436.469430	32.857344
720.939627	36482.872293	32.862362
721.753852	36531.060130	32.867380
722.257731	36576.387777	32.872397
723.239751	36629.747279	32.877415
723.806649	36685.517405	32.882432
724.743192	36735.431840	32.887450
725.805717	36762.563531	32.892468
726.729272	36793.839571	32.897485
727.498962	36827.719451	32.902503
728.382211	36870.528967	32.907520
728.813540	36896.620920	32.912538
729.354534	36933.849906	32.917556
729.365095	36980.051927	32.922573
729.908432	37020.322152	32.927591
730.716615	37070.801149	32.932608
731.265732	37110.248627	32.937626
732.049796	37167.775681	32.942644
732.361801	37223.953643	32.947661
732.970181	37274.925825	32.952679
733.767252	37336.068220	32.957696
734.388235	37379.868079	32.962714
735.501854	37431.957090	32.967732
735.950802	37497.093566	32.972749
737.020359	37552.345076	32.977767
737.597174	37623.987736	32.982784
738.551110	37669.298232	32.987802
738.593411	37726.271979	32.992820
739.599660	37788.426467	32.997837
740.321998	37846.300097	33.002855
741.046796	37907.411112	33.007872
742.076627	37964.491026	33.012890
742.623030	38027.887635	33.017908
743.202323	38094.181805	33.022925
744.273199	38153.317298	33.027943
745.170182	38206.586477	33.032960
746.391258	38250.338966	33.037978
747.433123	38306.583208	33.042996
748.202664	38367.113121	33.048013
749.057299	38413.692722	33.053031
749.796256	38467.587891	33.058048
750.259491	38508.512070	33.063066
751.015475	38561.412014	33.068084
751.652406	38622.791688	33.073101
752.265885	38676.567794	33.078119
753.577175	38730.127904	33.083136
754.179719	38779.175840	33.088154
755.204607	38830.833080	33.093172
755.678259	38881.855348	33.098189
756.303884	38928.964966	33.103207
757.058234	38982.606079	33.108224
757.499258	39039.660357	33.113242
758.401795	39096.971781	33.118260
758.845396	39155.316020	33.123277
760.271945	39206.804131	33.128295
761.034325	39270.600801	33.133312
761.509908	39324.659266	33.138330
762.249990	39377.690167	33.143348
762.739499	39439.101437	33.148365
764.019556	39495.608930	33.153383
764.586139	39555.263129	33.158400
765.265305	39606.527046	33.163418
766.301282	39663.597863	33.168436
766.731395	39726.208100	33.173453
767.534817	39778.370060	33.178471
768.504931	39831.119627	33.183488
769.611496	39891.708863	33.188506
770.185842	39938.019186	33.193524
771.118401	39992.501460	33.198541
771.903410	40034.738116	33.203559
772.395404	40094.234660	33.208576
773.348568	40148.309375	33.213594
773.776752	40197.210596	33.218612
774.717243	40260.331070	33.223629
775.386324	40315.525530	33.228647
776.361890	40376.768930	33.233664
776.800935	40424.138518	33.238682
777.941907	40475.680433	33.243700
778.718025	40534.469911	33.248717
779.338675	40574.513400	33.253735
779.886285	40623.700553	33.258752
780.746472	40678.353920	33.263770
781.184390	40726.280878	33.268788
781.853763	40783.942951	33.273805
782.622549	40826.948915	33.278823
783.709000	40882.857734	33.283840
784.090653	40936.865269	33.288858
785.120802	40992.062158	33.293876
785.652059	41061.111343	33.298893
786.480619	41110.812406	33.303911
787.393808	41164.699816	33.308928
787.910765	41232.739864	33.313946
788.928464	41288.837511	33.318964
789.722890	41349.738704	33.323981
790.631305	41405.050456	33.328999
791.632904	41462.896613	33.334016
792.666420	41529.902177	33.339034
793.624461	41583.012047	33.344052
794.350717	41639.478514	33.349069
795.045387	41686.140649	33.354087
796.592010	41737.584457	33.359104
798.569875	41739.705403	33.364122
800.328117	41752.213872	33.369140
801.218746	41797.258272	33.374157
801.847460	41808.013602	33.379175
802.662843	41835.266063	33.384192
803.169634	41864.046555	33.389210
804.010929	41889.720222	33.394228
804.367139	41920.851689	33.399245
805.231783	41950.069910	33.404263
805.723156	41984.368044	33.409280
805.883113	42018.173902	33.414298
806.659821	42057.980783	33.419316
807.036433	42105.420661	33.424333
807.416161	42150.494721	33.429351
808.107461	42194.116286	33.434368
808.934240	42262.604635	33.439386
809.818950	42312.698149	33.444404
810.118541	42375.513401	33.449421
810.964823	42442.367487	33.454439
811.815740	42493.946673	33.459456
812.267872	42563.398724	33.464474
813.253872	42622.616534	33.469492
814.016788	42680.193146	33.474509
815.143158	42742.494929	33.479527
816.313359	42800.874963	33.484544
817.074215	42868.180057	33.489562
817.936668	42922.503460	33.494580
818.418958	42984.052323	33.499597
819.505403	43028.790472	33.504615
820.497739	43089.153368	33.509632
821.341814	43149.349758	33.514650
822.453386	43209.991697	33.519668
823.111184	43256.751460	33.524685
823.885694	43300.665867	33.529703
824.968885	43347.682180	33.534720
825.589504	43395.820558	33.539738
826.821775	43435.818346	33.544756
827.514170	43498.860279	33.549773
827.837611	43568.569555	33.554791
828.739051	43612.863307	33.559808
829.314274	43676.246566	33.564826
830.475568	43727.280639	33.569844
831.129022	43790.082783	33.574861
831.815752	43843.018968	33.579879
832.745166	43897.100314	33.584896
833.457406	43944.972617	33.589914
834.365842	43995.939143	33.594932
834.825012	44050.568456	33.599949
835.775867	44112.895103	33.604967
836.665069	44158.981901	33.609984
837.196975	44217.155103	33.615002
838.190076	44276.173834	33.620020
838.970577	44331.848097	33.625037
839.779323	44384.715979	33.630055
840.870216	44440.127135	33.635072
841.372154	44502.866327	33.640090
842.148592	44558.535465	33.645108
842.589865	44630.532172	33.650125
843.614464	44693.601693	33.655143
844.528198	44760.692654	33.660160
845.254249	44829.558859	33.665178
846.107549	44898.582583	33.670196
846.810966	44958.192209	33.675213
847.821606	45030.759430	33.680231
848.708192	45100.657844	33.685248
849.063259	45168.172250	33.690266
849.936112	45236.346350	33.695284
850.916479	45315.383947	33.700301
852.124143	45392.039637	33.705319
853.059931	45464.923550	33.710336
853.706586	45538.048805	33.715354
854.704557	45599.954787	33.720372
855.651651	45672.584590	33.725389
856.494015	45748.545609	33.730407
857.782457	45810.590404	33.735424
858.789220	45876.430391	33.740442
860.177001	45934.803782	33.745460
861.042199	45994.340382	33.750477
861.722843	46052.368698	33.755495
862.543567	46115.834544	33.760512
863.129660	46176.585351	33.765530
864.399752	46232.902964	33.770548
865.109776	46305.204821	33.775565
866.094957	46373.915251	33.780583
867.209778	46428.587489	33.785600
867.515599	46494.171499	33.790618
868.493744	46549.921738	33.795636
869.533793	46612.437583	33.800653
870.462279	46677.767052	33.805671
871.317189	46739.078503	33.810688
871.907458	46804.846875	33.815706
872.793254	46852.072118	33.820724
873.966050	46929.168661	33.825741
874.733165	46995.593274	33.830759
875.430213	47059.137968	33.835776
876.412067	47121.297372	33.840794
877.346384	47178.466712	33.845812
878.075521	47246.144220	33.850829
879.717835	47298.680466	33.855847
880.652737	47352.136702	33.860864
881.059572	47417.606453	33.865882
882.488764	47477.666499	33.870900
883.151191	47546.512988	33.875917
883.621634	47601.604691	33.880935
884.881595	47655.694280	33.885952
885.520163	47707.849994	33.890970
886.404312	47767.945045	33.895988
887.247422	47835.821671	33.901005
888.133142	47901.382759	33.906023
889.124192	47963.751818	33.911040
889.867652	48023.920059	33.916058
890.551681	48080.972483	33.921076
891.404526	48142.300716	33.926093
892.110316	48203.949347	33.931111
892.985044	48257.176684	33.936128
893.910993	48323.087009	33.941146
894.833711	48373.991674	33.946164
895.238369	48438.724515	33.951181
896.210150	48501.047438	33.956199
896.948687	48567.253357	33.961216
898.061199	48641.081657	33.966234
898.606805	48699.270649	33.971252
899.749365	48777.883911	33.976269
900.270314	48843.732256	33.981287
901.268291	48906.121804	33.986304
902.205500	48983.097516	33.991322
903.036405	49050.182513	33.996340
904.372801	49114.462231	34.001357
904.774264	49192.072463	34.006375
906.210010	49251.838833	34.011392
906.854270	49326.691249	34.016410
908.040678	49390.305479	34.021428
909.171826	49474.673922	34.026445
909.813307	49540.929407	34.031463
911.024417	49612.309694	34.036480
911.650737	49680.548231	34.041498
912.749237	49748.207323	34.046516
913.734766	49819.300702	34.051533
914.649883	49892.904377	34.056551
915.179524	49967.656518	34.061568
916.370239	50039.515828	34.066586
917.242634	50107.945101	34.071604
918.152082	50180.032115	34.076621
918.720752	50260.947915	34.081639
920.352745	50325.374832	34.086656
921.213974	50400.279229	34.091674
922.229350	50486.086665	34.096692
923.436049	50541.102491	34.101709
923.942970	50619.245260	34.106727
924.720566	50681.015933	34.111744
926.216713	50751.311424	34.116762
926.513421	50830.170958	34.121780
927.676524	50908.851606	34.126797
928.399352	50980.090702	34.131815
929.595420	51053.008984	34.136832
930.780749	51128.947249	34.141850
931.306026	51194.909227	34.146868
932.600531	51268.186173	34.151885
933.831278	51346.984331	34.156903
934.901453	51402.384119	34.161920
935.840214	51470.149069	34.166938
937.119725	51534.381147	34.171956
938.396821	51593.577216	34.176973
939.136221	51661.399068	34.181991
939.883879	51712.711712	34.187008
940.369451	51767.482056	34.192026
941.345350	51837.501177	34.197044
942.186720	51902.049247	34.202061
943.104441	51974.589826	34.207079
944.158338	52045.464294	34.212096
944.842808	52113.631375	34.217114
945.780647	52184.201631	34.222132
947.154794	52241.467016	34.227149
948.005892	52310.241487	34.232167
948.900424	52370.353309	34.237184
950.146315	52440.129739	34.242202
950.976095	52507.313564	34.247220
952.180434	52569.990971	34.252237
952.699234	52638.286619	34.257255
953.536830	52700.173563	34.262272
954.768708	52771.395870	34.267290
955.441012	52825.304387	34.272308
956.351868	52879.049341	34.277325
957.052474	52942.533847	34.282343
957.887128	53004.327140	34.287360
958.753221	53065.552534	34.292378
959.645600	53136.518744	34.297396
960.565795	53193.540749	34.302413
961.314889	53270.939707	34.307431
962.080228	53345.931823	34.312448
963.170730	53425.448590	34.317466
964.030171	53494.870695	34.322484
965.331418	53558.978426	34.327501
965.721413	53635.738422	34.332519
966.698153	53704.769544	34.337536
967.646994	53791.795527	34.342554
968.291058	53880.362673	34.347572
969.689045	53960.314316	34.352589
970.679726	54036.741656	34.357607
971.724628	54122.475655	34.362624
973.216892	54194.402142	34.367642
974.140545	54274.719781	34.372660
975.346052	54352.544851	34.377677
976.244982	54420.020822	34.382695
977.109438	54496.292117	34.387712
978.083222	54583.386757	34.392730
978.801912	54662.434024	34.397748
980.398283	54724.360078	34.402765
981.194162	54808.477354	34.407783
982.025633	54877.281402	34.412800
983.077474	54956.999215	34.417818
984.188603	55047.504099	34.422836
985.156143	55122.666582	34.427853
986.386872	55197.459262	34.432871
987.426068	55268.567263	34.437888
988.112660	55349.570951	34.442906
989.110846	55431.811073	34.447924
990.203120	55514.543107	34.452941
990.887383	55582.176053	34.457959
991.753908	55674.214914	34.462976
993.381131	55746.852899	34.467994
994.054366	55834.846943	34.473012
995.093069	55911.323503	34.478029
995.826529	55993.195426	34.483047
997.085567	56077.264095	34.488064
998.283725	56154.608942	34.493082
998.975536	56244.595109	34.498100
1000.519793	56316.108605	34.503117
1001.472153	56388.277698	34.508135
1002.241390	56471.278520	34.513152
1003.862492	56548.172764	34.518170
1004.256524	56622.612867	34.523188
1005.401966	56688.582341	34.528205
1006.625101	56781.835717	34.533223
1007.371876	56854.791342	34.538240
1008.751495	56932.515508	34.543258
1009.403569	57013.517574	34.548276
1010.694332	57084.174145	34.553293
1011.549703	57154.006332	34.558311
1012.720657	57241.674937	34.563328
1013.625133	57307.873496	34.568346
1014.525784	57404.078119	34.573364
1015.433097	57474.934767	34.578381
1016.039494	57557.509024	34.583399
1017.204113	57631.256380	34.588416
1018.726293	57714.125324	34.593434
1019.779335	57797.010619	34.598452
1021.359010	57862.928396	34.603469
1022.081331	57940.207523	34.608487
1023.117793	58002.995090	34.613504
1024.736872	58046.894794	34.618522
1025.395685	58105.076890	34.623540
1026.523850	58153.844321	34.628557
1027.579575	58207.382618	34.633575
1028.766049	58262.919671	34.638592
1029.515358	58318.518573	34.643610
1029.945580	58386.028107	34.648628
1031.213355	58451.356805	34.653645
1031.918132	58520.387283	34.658663
1032.946271	58591.760067	34.663680
1034.066473	58656.542663	34.668698
1034.954593	58737.602404	34.673716
1035.894357	58803.932503	34.678733
1037.049294	58880.951097	34.683751
1037.545055	58954.110398	34.688768
1038.670348	59024.671845	34.693786
1039.864894	59108.906758	34.698804
1040.250578	59189.457592	34.703821
1041.621728	59274.279539	34.708839
1042.091383	59361.419425	34.713856
1043.579756	59448.679547	34.718874
1044.618573	59543.959759	34.723892
1045.776420	59631.601119	34.728909
1047.034557	59706.099797	34.733927
1047.998045	59796.462044	34.738944
1049.318826	59874.666919	34.743962
1050.329592	59982.264182	34.748980
1051.391055	60066.288938	34.753997
1052.726612	60149.378843	34.759015
1053.322047	60229.191552	34.764032
1054.308008	60324.109596	34.769050
1055.420847	60406.019748	34.774068
1056.736408	60486.601032	34.779085
1057.913118	60584.813492	34.784103
1058.655232	60676.530041	34.789120
1059.916458	60760.931198	34.794138
1061.044726	60852.461703	34.799156
1062.155044	60933.475184	34.804173
1063.265497	61021.540355	34.809191
1064.210831	61107.536359	34.814208
1065.167384	61182.713146	34.819226
1066.424647	61276.845729	34.824244
1067.077954	61354.070495	34.829261
1069.263157	61446.597075	34.834279
1070.354851	61527.982557	34.839296
1071.696571	61596.435199	34.844314
1073.005888	61677.261911	34.849332
1073.971269	61743.469419	34.854349
1074.987364	61821.759598	34.859367
1075.846824	61898.618492	34.864384
1076.754045	61972.830545	34.869402
1077.798672	62057.719312	34.874420
1078.987260	62134.591012	34.879437
1080.595027	62212.802995	34.884455
1081.702005	62284.389533	34.889472
1083.914905	62308.954488	34.894490
1085.147804	62373.381251	34.899508
1086.091371	62431.744573	34.904525
1086.905129	62489.178705	34.909543
1087.988862	62556.161252	34.914560
1088.985204	62617.783199	34.919578
1089.836318	62680.504052	34.924596
1090.323316	62744.389539	34.929613
1091.118241	62813.297831	34.934631
1091.885297	62895.384047	34.939648
1093.159400	62967.370680	34.944666
1093.791606	63037.969804	34.949684
1094.731658	63106.457507	34.954701
1096.044054	63172.842725	34.959719
1096.293862	63261.809508	34.964736
1097.533462	63335.784000	34.969754
1098.320274	63417.970155	34.974772
1099.237634	63503.510405	34.979789
1100.181799	63593.066642	34.984807
1101.695201	63678.476731	34.989824
1103.037515	63751.341292	34.994842
1104.186612	63830.971855	34.999860
1105.934129	63907.027706	35.004877
1108.082245	63963.238325	35.009895
1109.073319	64034.316184	35.014912
1110.193101	64095.675691	35.019930
1111.324462	64164.851889	35.024948
1111.947918	64229.853134	35.029965
1112.960828	64300.301617	35.034983
1113.845746	64375.182715	35.040000
1115.065863	64448.359546	35.045018
1116.127110	64531.823441	35.050036
1116.853740	64612.832720	35.055053
1118.246994	64697.986448	35.060071
1118.875878	64784.000147	35.065088
1120.346814	64872.934528	35.070106
1121.158297	64965.745055	35.075124
1122.053530	65047.166319	35.080141
1123.106673	65135.736163	35.085159
1124.216293	65238.656037	35.090176
1125.157585	65319.589865	35.095194
1126.287110	65418.417592	35.100212
1127.376580	65513.510330	35.105229
1128.456732	65605.749594	35.110247
1129.228926	65720.873163	35.115264
1130.682857	65826.774411	35.120282
1131.854680	65917.196191	35.125300
1133.003645	66024.962759	35.130317
1134.541072	66118.322966	35.135335
1135.940041	66218.973240	35.140352
1137.018448	66310.069406	35.145370
1138.264002	66401.051245	35.150388
1139.631770	66491.045710	35.155405
1141.362160	66576.628151	35.160423
1142.238911	66668.542069	35.165440
1143.543675	66752.133690	35.170458
1144.244550	66841.859658	35.175476
1145.540816	66933.012788	35.180493
1146.932113	67009.171459	35.185511
1148.061116	67105.435323	35.190528
1149.290592	67197.321573	35.195546
1150.298117	67290.122772	35.200564
1151.193329	67387.348479	35.205581
1152.378245	67460.868754	35.210599
1153.449679	67565.241263	35.215616
1154.573844	67653.625239	35.220634
1155.667401	67746.034813	35.225652
1156.949044	67840.352901	35.230669
1158.414064	67927.943978	35.235687
1158.820124	68038.797894	35.240704
1160.381234	68120.910494	35.245722
1161.605554	68225.420189	35.250740
1162.145463	68316.771969	35.255757
1163.834690	68404.652693	35.260775
1165.014237	68492.511744	35.265792
1166.312139	68597.024162	35.270810
1167.799485	68684.411733	35.275828
1168.839977	68770.406511	35.280845
1170.031507	68852.857580	35.285863
1171.191699	68946.812400	35.290880
1172.330406	69016.646540	35.295898
1174.494645	69076.069948	35.300916
1175.656321	69138.720510	35.305933
1177.103885	69194.836531	35.310951
1177.675532	69274.852681	35.315968
1179.055185	69328.738066	35.320986
1180.063403	69395.953133	35.326004
1180.754860	69463.496286	35.331021
1181.791304	69541.813600	35.336039
1182.941748	69626.584712	35.341056
1184.005709	69704.955225	35.346074
1184.945833	69788.391888	35.351092
1186.028145	69881.273119	35.356109
1187.057405	69967.564909	35.361127
1187.768372	70064.107552	35.366144
1188.595709	70159.783935	35.371162
1190.287799	70254.021644	35.376180
1191.320092	70363.977548	35.381197
1192.280391	70457.899315	35.386215
1193.772446	70575.851779	35.391232
1194.999481	70658.588025	35.396250
1196.051338	70750.976856	35.401268
1197.263670	70861.426083	35.406285
1198.216025	70961.404581	35.411303
1199.513724	71068.497928	35.416320
1200.778472	71183.436328	35.421338
1202.282332	71280.062693	35.426356
1203.580984	71385.308129	35.431373
1205.334224	71480.984551	35.436391
1206.640862	71572.450086	35.441408
1208.167569	71661.766633	35.446426
1209.381796	71753.956425	35.451444
1210.708630	71853.272118	35.456461
1211.730049	71944.758017	35.461479
1212.634577	72042.443032	35.466496
1213.818786	72139.654260	35.471514
1215.621853	72236.541544	35.476532
1217.303072	72319.009699	35.481549
1219.149827	72398.286012	35.486567
1220.276273	72479.017212	35.491584
1221.540131	72549.974898	35.496602
1223.839974	72598.733648	35.501620
1225.400053	72664.174066	35.506637
1227.236092	72721.149135	35.511655
1228.343041	72776.426642	35.516672
1229.121993	72841.444468	35.521690
1230.542300	72895.647540	35.526708
1231.360265	72963.977977	35.531725
1232.292411	73017.801322	35.536743
1233.223690	73084.125927	35.541760
1234.270797	73153.738418	35.546778
1235.788791	73225.633625	35.551796
1236.593668	73304.694863	35.556813
1238.013664	73370.386821	35.561831
1238.834506	73462.289178	35.566848
1239.314647	73531.636267	35.571866
1240.299517	73612.190311	35.576884
1241.358893	73718.444918	35.581901
1242.284926	73797.932075	35.586919
1243.346800	73902.223795	35.591936
1244.350116	74008.754274	35.596954
1245.440318	74108.051943	35.601972
1246.557735	74214.894805	35.606989
1247.950493	74321.441913	35.612007
1249.030574	74426.391494	35.617024
1249.988679	74539.492278	35.622042
1251.578312	74641.348796	35.627060
1252.304778	74755.588525	35.632077
1254.017567	74848.281475	35.637095
1255.218318	74950.364365	35.642112
1256.220730	75048.501200	35.647130
1257.776909	75133.024221	35.652148
1258.728006	75249.042418	35.657165
1259.953495	75350.768312	35.662183
1261.258877	75451.519479	35.667200
1262.235634	75559.288939	35.672218
1263.865185	75660.269101	35.677236
1264.754980	75765.544877	35.682253
1266.305712	75873.580927	35.687271
1267.488607	75980.547298	35.692288
1268.752108	76081.674685	35.697306
1270.136922	76193.677307	35.702324
1271.202628	76314.293088	35.707341
1272.792815	76414.534836	35.712359
1274.581070	76519.344353	35.717376
1275.986607	76622.693766	35.722394
1278.012593	76708.301330	35.727412
1279.062721	76809.375977	35.732429
1280.483699	76906.441024	35.737447
1281.903560	77006.192106	35.742464
1282.911524	77102.549421	35.747482
1284.145909	77197.985102	35.752500
1285.478134	77301.766542	35.757517
1286.729963	77393.336558	35.762535
1288.046569	77500.845491	35.767552
1288.646135	77606.629626	35.772570
1290.188313	77705.477485	35.777588
1291.469892	77817.236845	35.782605
1292.791281	77932.030773	35.787623
1294.185142	78043.938266	35.792640
1295.373837	78161.173397	35.797658
1296.546449	78261.094233	35.802676
1298.149368	78370.297550	35.807693
1299.426365	78484.872677	35.812711
1301.277304	78578.874383	35.817728
1302.194415	78691.428795	35.822746
1304.003944	78795.990386	35.827764
1305.019118	78894.949902	35.832781
1306.085921	79000.856711	35.837799
1308.076946	79103.642976	35.842816
1309.482548	79208.218330	35.847834
1311.008921	79302.425051	35.852852
1312.967768	79382.717977	35.857869
1314.584401	79473.807424	35.862887
1315.708303	79562.047395	35.867904
1316.911948	79650.515942	35.872922
1318.466397	79730.872826	35.877940
1319.467618	79832.067577	35.882957
1320.746951	79928.911994	35.887975
1321.896934	80016.718613	35.892992
1323.058782	80123.856483	35.898010
1324.168210	80210.149752	35.903028
1325.343084	80313.219577	35.908045
1326.470537	80418.590270	35.913063
1327.790506	80515.620444	35.918080
1328.689449	80619.570515	35.923098
1330.266791	80721.489658	35.928116
1331.305515	80845.094129	35.933133
1332.311667	80939.146664	35.938151
1333.875878	81052.750181	35.943168
1334.905102	81169.566780	35.948186
1336.401949	81278.886765	35.953204
1337.336955	81394.312654	35.958221
1338.461613	81510.583700	35.963239
1340.129154	81629.874789	35.968256
1340.905389	81738.700588	35.973274
1342.481367	81842.689186	35.978292
1344.317673	81949.995142	35.983309
1345.594048	82049.647396	35.988327
1346.942785	82147.527627	35.993344
1347.660459	82258.151001	35.998362
1349.334155	82359.693676	36.003380
1350.640591	82475.496967	36.008397
1352.191221	82573.081182	36.013415
1354.042538	82673.368344	36.018432
1355.123654	82786.078464	36.023450
1356.322753	82887.582877	36.028468
1357.612876	82994.775099	36.033485
1358.912385	83103.017900	36.038503
1360.856796	83214.873147	36.043520
1362.098979	83333.186006	36.048538
1363.134754	83431.613541	36.053556
1364.544092	83557.516254	36.058573
1365.553104	83667.732338	36.063591
1367.262459	83774.912933	36.068608
1368.243259	83890.341885	36.073626
1369.799906	84008.469227	36.078644
1370.784448	84128.498024	36.083661
1372.480908	84246.921360	36.088679
1373.995709	84376.042327	36.093696
1375.364085	84498.775182	36.098714
1377.025343	84617.927775	36.103732
1378.745711	84743.331149	36.108749
1379.638370	84869.383418	36.113767
1381.351818	84979.393542	36.118784
1382.382245	85097.772007	36.123802
1384.282097	85210.947142	36.128820
1385.571895	85335.963956	36.133837
1387.028895	85459.029243	36.138855
1388.977737	85565.178225	36.143872
1390.646466	85675.223312	36.148890
1392.293450	85780.558412	36.153908
1394.028759	85887.552791	36.158925
1395.010275	85988.050331	36.163943
1396.791401	86085.712037	36.168960
1398.007348	86198.401928	36.173978
1399.111062	86305.610203	36.178996
1400.731648	86415.222088	36.184013
1401.826866	86521.798897	36.189031
1403.278741	86630.386094	36.194048
1404.095904	86747.461286	36.199066
1406.287660	86861.661886	36.204084
1407.169081	86972.125894	36.209101
1408.661800	87100.312076	36.214119
1409.816404	87204.056268	36.219136
1411.102363	87328.055822	36.224154
1412.303319	87442.488945	36.229172
1413.648149	87567.646194	36.234189
1414.738216	87695.872314	36.239207
1416.356890	87815.602266	36.244224
1417.732634	87938.424571	36.249242
1419.389675	88053.828230	36.254260
1420.950476	88170.083708	36.259277
1422.905029	88299.090327	36.264295
1424.463765	88394.120462	36.269312
1426.057653	88505.442469	36.274330
1427.834017	88617.078658	36.279348
1429.346534	88732.266691	36.284365
1430.383573	88838.379414	36.289383
1432.362658	88937.464536	36.294400
1433.374772	89054.696003	36.299418
1435.120689	89160.167284	36.304436
1436.239249	89259.653555	36.309453
1437.386681	89366.017119	36.314471
1438.868444	89465.764375	36.319488
1439.937627	89569.720292	36.324506
1441.154409	89675.693977	36.329524
1442.310152	89774.973416	36.334541
1443.626783	89870.806368	36.339559
1445.111144	89982.252359	36.344576
1446.483806	90092.702285	36.349594
1447.781158	90213.366418	36.354612
1449.313585	90317.911858	36.359629
1450.463069	90435.406198	36.364647
1451.902249	90547.292228	36.369664
1453.085799	90679.394807	36.374682
1454.937441	90801.217048	36.379700
1456.190306	90926.111299	36.384717
1457.392513	91057.997187	36.389735
1459.392536	91169.177231	36.394752
1460.361827	91306.436128	36.399770
1461.823525	91433.315123	36.404788
1463.623526	91562.955615	36.409805
1464.882831	91698.346105	36.414823
1466.292999	91816.781167	36.419840
1467.735789	91956.149258	36.424858
1469.247777	92092.414720	36.429876
1470.795037	92220.196243	36.434893
1472.121312	92367.353665	36.439911
1473.648567	92493.403073	36.444928
1475.396442	92638.772479	36.449946
1476.923622	92761.578364	36.454964
1478.729135	92893.403697	36.459981
1480.072289	93029.319403	36.464999
1481.673763	93162.584536	36.470016
1483.224782	93300.281566	36.475034
1485.151832	93429.555364	36.480052
1486.725116	93546.045212	36.485069
1488.234236	93683.180122	36.490087
1489.807918	93805.387248	36.495104
1491.277314	93933.695063	36.500122
1493.101083	94052.974363	36.505140
1494.407933	94188.457238	36.510157
1495.584861	94319.689422	36.515175
1498.641810	94415.227860	36.520192
1500.626844	94519.324405	36.525210
1502.291427	94625.816095	36.530228
1504.111897	94732.943003	36.535245
1505.128873	94847.255495	36.540263
1507.355011	94933.760602	36.545280
1508.754582	95027.049182	36.550298
1510.133567	95131.368874	36.555316
1511.456295	95235.330083	36.560333
1512.413811	95339.804803	36.565351
1513.674013	95442.597616	36.570368
1515.417376	95551.615342	36.575386
1516.188894	95673.067420	36.580404
1517.661729	95778.097188	36.585421
1518.850789	95896.557062	36.590439
1520.533815	96020.771369	36.595456
1521.657034	96142.969110	36.600474
1523.115269	96269.095417	36.605492
1524.495760	96400.773722	36.610509
1525.733667	96527.201556	36.615527
1527.606543	96661.390224	36.620544
1528.399556	96794.251759	36.625562
1529.846902	96929.331750	36.630580
1531.773492	97066.923678	36.635597
1533.098069	97204.546526	36.640615
1535.010246	97341.723582	36.645632
1536.149957	97478.083411	36.650650
1538.039247	97605.504363	36.655668
1539.625189	97717.368294	36.660685
1540.620473	97840.974280	36.665703
1542.558724	97953.303948	36.670720
1544.225095	98067.717267	36.675738
1545.782114	98203.051845	36.680756
1547.165575	98308.002561	36.685773
1549.019091	98436.940954	36.690791
1550.241708	98552.895594	36.695808
1551.848722	98673.240404	36.700826
1552.688239	98799.929486	36.705844
1554.382800	98933.559733	36.710861
1555.706695	99065.105815	36.715879
1557.213313	99201.872305	36.720896
1558.687299	99336.261159	36.725914
1560.330068	99478.332029	36.730932
1561.898074	99619.109410	36.735949
1563.694388	99771.793881	36.740967
1564.719194	99912.035902	36.745984
1565.855074	100052.109117	36.751002
1567.795266	100211.492304	36.756020
1569.547401	100360.408556	36.761037
1571.121738	100509.796883	36.766055
1573.086090	100660.190118	36.771072
1574.522542	100805.240160	36.776090
1576.376500	100957.097213	36.781108
1578.304607	101094.744284	36.786125
1579.680842	101258.581567	36.791143
1581.349951	101391.008886	36.796160
1583.042479	101536.111078	36.801178
1584.791011	101689.496638	36.806196
1586.485446	101830.847143	36.811213
1588.100866	101979.817450	36.816231
1589.557298	102119.621477	36.821248
1591.611693	102268.334599	36.826266
1593.334328	102421.081026	36.831284
1594.647197	102542.893306	36.836301
1596.214636	102699.164410	36.841319
1598.037380	102834.984154	36.846336
1599.842763	102974.090901	36.851354
1601.728890	103117.280852	36.856372
1603.965840	103243.427439	36.861389
1605.552203	103381.834631	36.866407
1607.445180	103493.759504	36.871424
1609.990842	103599.687539	36.876442
1611.400505	103720.842482	36.881460
1613.714998	103825.336476	36.886477
1615.421437	103943.618655	36.891495
1616.813234	104044.973113	36.896512
1618.185201	104157.120784	36.901530
1619.425936	104277.391160	36.906548
1620.891223	104387.027311	36.911565
1622.728068	104502.869476	36.916583
1624.187876	104613.597628	36.921600
1625.590089	104730.890259	36.926618
1626.755886	104857.133612	36.931636
1628.804518	104966.427284	36.936653
1630.507593	105084.371688	36.941671
1631.883088	105212.079900	36.946688
1633.521810	105315.644030	36.951706
1634.974528	105451.925107	36.956724
1636.424783	105572.028044	36.961741
1637.714848	105705.545967	36.966759
1638.917623	105839.902179	36.971776
1641.084956	105972.473121	36.976794
1642.003456	106109.296466	36.981812
1643.563855	106246.793922	36.986829
1645.165042	106392.426037	36.991847
1646.168636	106520.361914	36.996864
1648.047808	106664.138706	37.001882
1649.681606	106793.778076	37.006900
1650.871899	106921.344042	37.011917
1652.380711	107063.848760	37.016935
1653.639060	107200.217832	37.021952
1655.507528	107337.950708	37.026970
1657.126614	107488.948437	37.031988
1659.621363	107600.539700	37.037005
1661.950935	107743.287232	37.042023
1663.232188	107871.058146	37.047040
1664.400545	108002.131335	37.052058
1666.328236	108148.835992	37.057076
1668.126915	108281.929782	37.062093
1669.507572	108418.829918	37.067111
1671.136478	108568.106296	37.072128
1672.851922	108705.614853	37.077146
1674.090649	108860.799016	37.082164
1675.484446	109002.987285	37.087181
1677.388026	109160.618149	37.092199
1678.933404	109308.896247	37.097216
1680.663323	109467.620726	37.102234
1681.959622	109631.105394	37.107252
1683.840570	109782.376722	37.112269
1685.839246	109953.108602	37.117287
1687.414080	110124.554023	37.122304
1689.434527	110282.438067	37.127322
1690.811487	110439.979128	37.132340
1692.609431	110604.759842	37.137357
1694.298440	110767.060039	37.142375
1696.007857	110937.309101	37.147392
1697.548628	111101.143004	37.152410
1699.522852	111274.484818	37.157428
1701.213316	111432.704366	37.162445
1703.586601	111604.184887	37.167463
1704.973424	111763.340888	37.172480
1707.275714	111926.806445	37.177498
1708.457117	112097.029116	37.182516
1710.294685	112253.200313	37.187533
1711.939076	112423.530027	37.192551
1713.346666	112592.172643	37.197568
1715.421338	112748.258370	37.202586
1716.861548	112927.195379	37.207604
1718.744947	113091.505068	37.212621
1720.684626	113256.301358	37.217639
1722.289413	113428.379477	37.222656
1724.427634	113600.337344	37.227674
1726.036959	113760.380708	37.232692
1728.672495	113904.031406	37.237709
1730.972053	114051.095851	37.242727
1732.924451	114204.505517	37.247744
1734.558343	114343.164695	37.252762
1736.415094	114499.000202	37.257780
1737.865673	114644.575791	37.262797
1739.308187	114787.756157	37.267815
1740.626719	114940.798310	37.272832
1742.816119	115089.317260	37.277850
1744.070559	115247.646778	37.282868
1745.912408	115404.566517	37.287885
1747.652855	115558.547543	37.292903
1749.241925	115729.294556	37.297920
1750.844734	115882.512000	37.302938
1752.436231	116032.497605	37.307956
1754.352622	116197.957649	37.312973
1756.069422	116354.951626	37.317991
1757.555881	116525.705603	37.323008
1759.145308	116681.236821	37.328026
1760.849475	116849.776841	37.333044
1762.923416	116997.560422	37.338061
1764.797020	117146.986593	37.343079
1766.379600	117291.309073	37.348096
1767.958061	117434.402426	37.353114
1769.610541	117579.197119	37.358132
1771.324605	117728.992908	37.363149
1773.021082	117883.358237	37.368167
1774.427892	118036.779934	37.373184
1775.948880	118190.970894	37.378202
1777.503203	118355.317230	37.383220
1778.993249	118535.199648	37.388237
1780.394203	118699.127403	37.393255
1782.176094	118873.105913	37.398272
1783.914809	119055.806052	37.403290
1785.919225	119243.032084	37.408308
1787.483662	119414.497358	37.413325
1789.722329	119593.697472	37.418343
1791.342263	119779.362362	37.423360
1793.576106	119957.512115	37.428378
1795.400526	120144.199768	37.433396
1797.020089	120328.116889	37.438413
1799.076975	120508.630727	37.443431
1800.978886	120680.252091	37.448448
1802.810957	120861.703194	37.453466
1804.784637	121058.152095	37.458484
1806.100213	121237.440106	37.463501
1807.874048	121427.579473	37.468519
1809.810307	121613.965058	37.473536
1812.136793	121792.819220	37.478554
1813.946861	121988.714764	37.483572
1815.992540	122169.999186	37.488589
1818.008672	122337.487356	37.493607
1819.869677	122532.172580	37.498624
1821.876200	122714.214050	37.503642
1823.886073	122888.733308	37.508660
1825.781468	123070.857149	37.513677
1827.677773	123240.410193	37.518695
1829.240732	123440.981692	37.523712
1831.170769	123611.761590	37.528730
1832.951535	123804.042580	37.533748
1834.851852	123975.640560	37.538765
1837.179191	124150.369679	37.543783
1839.809924	124324.760565	37.548800
1841.634009	124477.178639	37.553818
1843.321035	124652.986436	37.558836
1845.018493	124829.110533	37.563853
1847.314215	124987.470385	37.568871
1849.138434	125162.206100	37.573888
1850.845720	125326.976632	37.578906
1852.509221	125493.454625	37.583924
1854.040641	125675.938761	37.588941
1856.226478	125841.918239	37.593959
1857.531692	126034.017487	37.598976
1858.734564	126210.249943	37.603994
1860.954170	126397.717536	37.609012
1862.499157	126592.053005	37.614029
1863.969858	126775.706004	37.619047
1865.401127	126971.773685	37.624064
1867.106858	127165.414448	37.629082
1869.117135	127365.973862	37.634100
1870.696731	127583.601886	37.639117
1872.513114	127781.795647	37.644135
1874.342281	127977.336752	37.649152
1876.177784	128179.234081	37.654170
1877.804485	128388.675749	37.659188
1879.819207	128602.587455	37.664205
1881.782118	128802.311124	37.669223
1883.671999	129018.198243	37.674240
1885.703987	129214.538260	37.679258
1887.592589	129408.452808	37.684276
1889.367111	129602.627067	37.689293
1891.087867	129783.488512	37.694311
1893.149408	129971.390140	37.699328
1894.481814	130172.652147	37.704346
1896.644656	130360.501668	37.709364
1898.698464	130560.105314	37.714381
1900.572390	130749.524066	37.719399
1902.239684	130958.502704	37.724416
1905.404987	131129.755899	37.729434
1907.915721	131305.083040	37.734452
1909.885403	131487.092965	37.739469
1911.885141	131654.799328	37.744487
1914.511664	131829.704562	37.749504
1916.364161	131997.955394	37.754522
1918.120871	132175.179795	37.759540
1919.500546	132355.661087	37.764557
1921.685891	132536.195377	37.769575
1923.195911	132721.581039	37.774592
1925.104567	132900.738782	37.779610
1926.890279	133088.341664	37.784628
1928.266459	133296.234903	37.789645
1930.052109	133478.840108	37.794663
1931.953607	133689.724132	37.799680
1933.146790	133898.816067	37.804698
1935.376665	134108.052180	37.809716
1937.168882	134329.906833	37.814733
1939.341036	134537.225222	37.819751
1942.707838	134709.996483	37.824768
1945.070808	134905.447937	37.829786
1947.203189	135092.738887	37.834804
1948.863559	135299.544074	37.839821
1951.099129	135490.411695	37.844839
1952.990333	135686.891679	37.849856
1954.676819	135895.979633	37.854874
1956.236139	136081.320882	37.859892
1957.777428	136295.407567	37.864909
1960.227382	136502.095373	37.869927
1962.168935	136703.863506	37.874944
1963.801349	136914.588842	37.879962
1966.006221	137116.241677	37.884980
1967.597444	137324.767287	37.889997
1969.538983	137541.830395	37.895015
1971.407999	137745.479819	37.900032
1973.218003	137969.582967	37.905050
1975.342142	138187.369402	37.910068
1977.208977	138415.361719	37.915085
1979.070637	138625.665797	37.920103
1980.731076	138854.923337	37.925120
1982.571337	139075.270779	37.930138
1984.853275	139303.761203	37.935156
1986.874056	139529.844123	37.940173
1988.541541	139745.145411	37.945191
1990.649648	139985.404922	37.950208
1992.614774	140212.350038	37.955226
1994.727414	140436.722449	37.960244
1996.631768	140675.583111	37.965261
1998.821192	140902.839259	37.970279
2000.845687	141139.069228	37.975296
2002.886449	141367.429439	37.980314
2004.935715	141598.695649	37.985332
2006.545881	141833.927464	37.990349
2008.618231	142060.572741	37.995367
2010.587980	142291.169313	38.000384
2012.532071	142521.288702	38.005402
2014.979666	142750.937384	38.010420
2016.563914	142990.227342	38.015437
2018.872599	143213.554125	38.020455
2020.918642	143434.333734	38.025472
2022.475282	143648.590896	38.030490
2024.721119	143859.949574	38.035508
2026.386997	144082.593445	38.040525
2028.853262	144292.967786	38.045543
2030.608658	144503.402881	38.050560
2031.912998	144728.200039	38.055578
2034.162002	144955.046877	38.060596
2036.320900	145174.661672	38.065613
2038.549128	145402.122970	38.070631
2040.592538	145636.797749	38.075648
2042.504945	145860.477260	38.080666
2044.565132	146092.359271	38.085684
2046.255570	146331.902515	38.090701
2048.435769	146564.491447	38.095719
2050.464422	146801.674256	38.100736
2052.151913	147051.540181	38.105754
2054.664662	147306.571631	38.110772
2056.066554	147566.460759	38.115789
2058.212607	147811.397746	38.120807
2060.378620	148070.040825	38.125824
2062.202302	148333.739385	38.130842
2064.283409	148588.590425	38.135860
2066.307032	148861.234296	38.140877
2068.098213	149122.644458	38.145895
2070.281047	149386.762018	38.150912
2072.202305	149668.958380	38.155930
2074.778091	149940.607954	38.160948
2076.734978	150205.653241	38.165965
2078.882836	150471.215920	38.170983
2081.245241	150743.308937	38.176000
2083.234279	151026.288847	38.181018
2085.244065	151282.940878	38.186036
2087.269310	151550.635021	38.191053
2090.233295	151803.396420	38.196071
2093.553403	152058.769210	38.201088
2096.376725	152303.507068	38.206106
2098.980787	152535.243711	38.211124
2100.420137	152778.371163	38.216141
2102.883880	153013.406623	38.221159
2105.138254	153261.004489	38.226176
2106.717486	153501.917280	38.231194
2108.990066	153743.446750	38.236212
2110.897799	154002.488312	38.241229
2113.087020	154250.925777	38.246247
2114.768901	154491.534840	38.251264
2116.431964	154754.248425	38.256282
2118.829113	155002.732967	38.261300
2120.463205	155261.226197	38.266317
2122.824641	155507.331946	38.271335
2125.051838	155766.103265	38.276352
2128.718259	155969.291205	38.281370
2131.307772	156197.719096	38.286388
2133.763239	156450.961212	38.291405
2135.618229	156670.758711	38.296423
2137.468591	156902.008331	38.301440
2139.032195	157133.227316	38.306458
2141.076529	157370.377006	38.311476
2142.729985	157615.167275	38.316493
2145.298200	157858.902153	38.321511
2147.062778	158094.194028	38.326528
2149.038426	158352.177958	38.331546
2151.054996	158599.251602	38.336564
2152.951978	158855.574181	38.341581
2154.582741	159121.320968	38.346599
2156.766887	159364.918569	38.351616
2158.773298	159624.693129	38.356634
2160.858109	159878.147029	38.361652
2162.824302	160134.578443	38.366669
2164.536905	160375.587405	38.371687
2166.643071	160622.337863	38.376704
2168.123843	160873.591958	38.381722
2170.399522	161123.352231	38.386740
2172.655983	161373.129182	38.391757
2175.082675	161637.861480	38.396775
2177.410116	161888.454634	38.401792
2179.660924	162148.404765	38.406810
2181.896514	162396.043405	38.411828
2184.083976	162658.709668	38.416845
2186.125442	162923.748462	38.421863
2188.837075	163187.046267	38.426880
2190.564467	163457.747729	38.431898
2192.422937	163724.443354	38.436916
2194.590476	164003.851544	38.441933
2196.464100	164287.013939	38.446951
2198.502053	164567.561943	38.451968
2200.914938	164855.810198	38.456986
2202.711104	165141.819553	38.462004
2205.008034	165424.273387	38.467021
2207.440400	165726.043985	38.472039
2209.939179	166010.500284	38.477056
2212.235856	166305.743190	38.482074
2214.304514	166586.624922	38.487092
2216.652601	166872.987353	38.492109
2218.931634	167184.221850	38.497127
2221.360058	167475.640252	38.502144
2223.294533	167790.283022	38.507162
2225.390223	168084.371284	38.512180
2227.644870	168390.536193	38.517197
2229.933375	168692.608730	38.522215
2232.209095	169005.603978	38.527232
2234.451369	169318.948618	38.532250
2236.302816	169616.128505	38.537268
2239.061748	169930.258794	38.542285
2240.996609	170234.119643	38.547303
2243.788432	170539.689493	38.552320
2246.150647	170855.180611	38.557338
2250.210006	171127.720297	38.562356
2252.941464	171404.213386	38.567373
2255.208681	171679.840131	38.572391
2257.799599	171964.648617	38.577408
2259.813812	172243.834015	38.582426
2262.214958	172508.675389	38.587444
2264.333499	172795.985752	38.592461
2266.666328	173070.413747	38.597479
2268.652797	173342.991955	38.602496
2270.670248	173630.206873	38.607514
2273.055778	173909.251634	38.612532
2275.179981	174192.401386	38.617549
2277.313256	174491.194613	38.622567
2279.726548	174765.920780	38.627584
2281.518738	175058.369431	38.632602
2284.372861	175330.057589	38.637620
2286.738721	175613.314453	38.642637
2288.475403	175900.987601	38.647655
2290.999104	176190.063067	38.652672
2292.968115	176484.660732	38.657690
2295.215418	176781.171677	38.662708
2297.199687	177072.594481	38.667725
2299.376434	177369.728021	38.672743
2301.839383	177663.795841	38.677760
2304.361306	177959.811072	38.682778
2306.651439	178250.961773	38.687796
2308.566029	178552.635532	38.692813
2310.392636	178857.701870	38.697831
2312.676206	179142.659679	38.702848
2314.821406	179440.948191	38.707866
2316.621807	179731.494347	38.712884
2319.350309	180022.277983	38.717901
2321.143173	180316.738454	38.722919
2323.405860	180601.755011	38.727936
2325.758578	180894.530190	38.732954
2327.793674	181188.346263	38.737972
2330.098402	181478.565602	38.742989
2332.064332	181789.664994	38.748007
2334.658448	182095.689632	38.753024
2337.130284	182414.001652	38.758042
2338.958905	182727.716163	38.763060
2341.514632	183049.700030	38.768077
2343.618330	183369.774251	38.773095
2346.228708	183682.963869	38.778112
2348.674125	184008.117542	38.783130
2351.117817	184332.891586	38.788148
2353.755070	184653.979151	38.793165
2355.979299	184978.611684	38.798183
2358.148330	185306.377939	38.803200
2360.832436	185645.164499	38.808218
2362.775486	185974.542832	38.813236
2365.223620	186333.636933	38.818253
2367.699825	186714.977733	38.823271
2370.449469	187046.723095	38.828288
2372.898381	187387.583927	38.833306
2374.571623	187725.417020	38.838324
2377.136833	188069.640080	38.843341
2379.351340	188415.569798	38.848359
2382.128138	188760.422515	38.853376
2384.389041	189108.887187	38.858394
2387.163623	189456.155411	38.863412
2389.658025	189805.144718	38.868429
2391.781080	190157.698111	38.873447
2394.206943	190508.859256	38.878464
2396.570361	190864.222235	38.883482
2399.088245	191211.510341	38.888500
2402.025814	191560.867794	38.893517
2404.488714	191912.662393	38.898535
2406.861048	192260.839830	38.903552
2409.674731	192596.350851	38.908570
2412.347513	192936.304445	38.913588
2415.483458	193272.376772	38.918605
2417.835785	193598.513208	38.923623
2420.496525	193931.613146	38.928640
2422.939187	194271.555358	38.933658
2425.212222	194597.605078	38.938676
2427.907171	194939.541862	38.943693
2429.791220	195280.107057	38.948711
2432.217449	195610.733055	38.953728
2434.563460	195954.682640	38.958746
2436.607268	196294.463491	38.963764
2439.542498	196638.399296	38.968781
2441.486098	196976.114491	38.973799
2443.788067	197323.528925	38.978816
2446.473948	197668.547506	38.983834
2448.681741	198019.153478	38.988852
2451.135714	198359.713687	38.993869
2453.567477	198713.588682	38.998887
2455.775522	199067.321513	39.003904
2458.381102	199420.891691	39.008922
2461.180223	199761.502948	39.013940
2464.000166	200090.858604	39.018957
2466.849629	200449.575170	39.023975
2469.367280	200780.147789	39.028992
2471.682215	201115.299621	39.034010
2473.982089	201460.716986	39.039028
2476.441184	201789.090744	39.044045
2478.636727	202108.615330	39.049063
2480.750746	202415.452000	39.054080
2483.086460	202737.902612	39.059098
2485.142453	203073.428819	39.064116
2487.536837	203390.359144	39.069133
2489.879056	203733.742223	39.074151
2492.117877	204061.417807	39.079168
2494.593740	204401.758409	39.084186
2496.850817	204738.932926	39.089204
2499.543080	205074.414529	39.094221
2501.955406	205424.242048	39.099239
2504.673850	205768.129079	39.104256
2506.990124	206125.720632	39.109274
2509.462471	206474.346680	39.114292
2512.175376	206825.196734	39.119309
2514.514203	207187.232099	39.124327
2516.890591	207553.021869	39.129344
2519.535739	207908.812399	39.134362
2521.541390	208270.469518	39.139380
2523.974317	208651.544945	39.144397
2526.946253	209033.883472	39.149415
2529.131714	209405.929658	39.154432
2531.723476	209786.550293	39.159450
2533.936241	210168.195805	39.164468
2536.907094	210548.682362	39.169485
2539.478732	210938.580043	39.174503
2542.377610	211314.201425	39.179520
2544.949599	211693.151228	39.184538
2547.746388	212079.077915	39.189556
2550.364219	212462.645020	39.194573
2553.141739	212833.562181	39.199591
2556.500551	213206.243781	39.204608
2558.616992	213594.005680	39.209626
2561.099563	213976.376284	39.214644
2563.797660	214355.716136	39.219661
2565.997456	214750.198344	39.224679
2568.730453	215136.113146	39.229696
2571.095805	215523.609778	39.234714
2573.464447	215918.447974	39.239732
2576.188050	216314.704731	39.244749
2578.511857	216710.973263	39.249767
2581.547763	217110.027368	39.254784
2584.589159	217493.000303	39.259802
2586.877489	217886.785773	39.264820
2589.721860	218287.953766	39.269837
2592.249943	218675.427746	39.274855
2594.820336	219076.257887	39.279872
2597.318399	219461.526915	39.284890
2599.818937	219868.770239	39.289908
2602.414350	220256.158515	39.294925
2604.934354	220664.466236	39.299943
2607.409731	221068.513236	39.304960
2610.805321	221454.456567	39.309978
2613.478833	221861.851829	39.314996
2616.164408	222242.596519	39.320013
2618.591049	222632.628712	39.325031
2621.121370	223038.065162	39.330048
2623.779741	223433.574207	39.335066
2626.190252	223836.997182	39.340084
2628.995895	224223.210985	39.345101
2631.260943	224637.783732	39.350119
2634.048303	225020.850379	39.355136
2636.660283	225423.708736	39.360154
2639.393311	225829.799997	39.365172
2642.331839	226227.958603	39.370189
2644.644101	226638.561045	39.375207
2646.943329	227043.220924	39.380224
2649.656760	227432.472226	39.385242
2652.229703	227808.103337	39.390260
2655.526266	228171.808871	39.395277
2658.368119	228527.201747	39.400295
2661.245128	228887.771499	39.405312
2664.020757	229251.837287	39.410330
2666.514896	229611.247020	39.415348
2669.187349	229976.395602	39.420365
2671.331757	230339.390668	39.425383
2673.656022	230710.232847	39.430400
2676.447681	231091.138326	39.435418
2678.463485	231477.473794	39.440436
2681.184671	231860.777825	39.445453
2683.685770	232264.794720	39.450471
2686.368306	232643.201342	39.455488
2689.736039	233026.962941	39.460506
2692.524662	233424.811962	39.465524
2695.503880	233805.635818	39.470541
2698.156644	234197.103612	39.475559
2700.323765	234598.554173	39.480576
2702.923371	234998.514469	39.485594
2705.800798	235395.992406	39.490612
2708.441488	235798.892417	39.495629
2711.410694	236208.904770	39.500647
2713.737270	236623.792603	39.505664
2716.499189	237035.004907	39.510682
2719.126280	237455.865722	39.515700
2721.823595	237874.200144	39.520717
2724.539952	238301.346141	39.525735
2727.237534	238718.434684	39.530752
2730.927243	239118.601941	39.535770
2733.804265	239542.876064	39.540788
2736.670951	239954.093804	39.545805
2739.590014	240371.628264	39.550823
2741.871258	240790.302900	39.555840
2744.866529	241193.445935	39.560858
2747.923599	241612.684448	39.565876
2750.752656	242033.685189	39.570893
2753.396675	242447.651921	39.575911
2755.963053	242866.964708	39.580928
2758.760107	243281.973135	39.585946
2761.176664	243723.586282	39.590964
2763.938186	244149.979268	39.595981
2766.832551	244576.985839	39.600999
2769.354503	245016.141335	39.606016
2771.984336	245436.455585	39.611034
2774.726670	245875.524185	39.616052
2777.495328	246326.196819	39.621069
2780.098293	246755.378100	39.626087
2782.690799	247203.815296	39.631104
2785.754085	247637.851099	39.636122
2789.003315	248073.889164	39.641140
2791.961562	248513.527824	39.646157
2795.109864	248950.417773	39.651175
2797.351312	249388.463860	39.656192
2800.418534	249828.107689	39.661210
2803.700274	250258.597594	39.666228
2806.825568	250688.983724	39.671245
2809.566228	251108.988315	39.676263
2812.793788	251547.535739	39.681280
2814.998766	251974.810197	39.686298
2817.657992	252406.127904	39.691316
2820.724672	252844.036271	39.696333
2823.467994	253273.865127	39.701351
2825.861270	253713.399854	39.706368
2828.391240	254144.173836	39.711386
2831.234113	254582.442092	39.716404
2833.763142	255033.458558	39.721421
2836.838222	255458.555403	39.726439
2839.053325	255890.439902	39.731456
2842.078639	256295.525672	39.736474
2844.717632	256708.214473	39.741492
2847.248592	257129.707561	39.746509
2850.174410	257543.187336	39.751527
2852.727683	257987.001613	39.756544
2855.528137	258404.994063	39.761562
2858.112393	258857.258920	39.766580
2860.459362	259293.124850	39.771597
2863.244648	259739.081221	39.776615
2866.201019	260196.058502	39.781632
2869.008411	260640.484045	39.786650
2871.797363	261099.312704	39.791668
2874.719983	261558.118742	39.796685
2877.507857	262021.007910	39.801703
2880.175207	262487.292122	39.806720
2883.078505	262965.043778	39.811738
2886.150424	263433.623224	39.816756
2888.776876	263928.152149	39.821773
2891.791369	264399.835080	39.826791
2894.667698	264890.231335	39.831808
2897.607955	265369.134885	39.836826
2900.864705	265854.666928	39.841844
2904.479001	266340.242613	39.846861
2907.663689	266821.742795	39.851879
2910.690971	267304.890662	39.856896
2913.916833	267785.820971	39.861914
2916.885564	268255.232598	39.866932
2920.307201	268719.720363	39.871949
2923.421542	269192.304926	39.876967
2926.632546	269666.929320	39.881984
2929.602692	270131.302586	39.887002
2932.426497	270590.769098	39.892020
2935.389810	271072.460000	39.897037
2938.634484	271540.897792	39.902055
2941.410752	272020.199940	39.907072
2944.584931	272484.021387	39.912090
2947.269546	272952.386463	39.917108
2950.109929	273429.562940	39.922125
2952.897915	273905.729038	39.927143
2955.769129	274394.323927	39.932160
2958.852473	274868.432287	39.937178
2962.037773	275351.385447	39.942196
2964.961948	275837.627140	39.947213
2968.042048	276306.369103	39.952231
2970.871821	276787.159621	39.957248
2974.188894	277273.458511	39.962266
2976.933191	277750.904259	39.967284
2979.998942	278236.576034	39.972301
2983.081845	278710.611016	39.977319
2986.093956	279203.929088	39.982336
2988.885869	279693.265820	39.987354
2992.054210	280172.941535	39.992372
2994.791617	280661.213880	39.997389
2998.250713	281142.971278	40.002407
3001.038133	281630.366033	40.007424
3003.951346	282116.290490	40.012442
3007.695311	282589.486949	40.017460
3010.367377	283061.298064	40.022477
3013.503565	283537.401555	40.027495
3016.869534	284018.544794	40.032512
3020.164116	284498.451560	40.037530
3023.365286	284961.254518	40.042548
3025.765851	285426.896013	40.047565
3029.452965	285892.207167	40.052583
3032.419632	286368.469927	40.057600
3035.178289	286837.981885	40.062618
3038.269863	287291.238420	40.067636
3041.431254	287726.528723	40.072653
3044.401852	288157.960861	40.077671
3047.214988	288587.459483	40.082688
3050.101337	289018.238848	40.087706
3052.839499	289442.411212	40.092724
3055.738646	289892.048621	40.097741
3058.949477	290332.366577	40.102759
3061.422538	290782.444845	40.107776
3063.848850	291236.640470	40.112794
3066.649877	291695.268610	40.117812
3069.292980	292175.423607	40.122829
3071.866021	292649.009690	40.127847
3075.169918	293142.561862	40.132864
3077.658385	293633.469416	40.137882
3080.424308	294129.712379	40.142900
3083.620020	294645.383373	40.147917
3086.410198	295148.875415	40.152935
3089.223697	295683.105508	40.157952
3092.590230	296201.376718	40.162970
3095.251505	296721.479455	40.167988
3098.502070	297252.148843	40.173005
3101.753350	297788.449319	40.178023
3104.757934	298340.523510	40.183040
3108.109344	298882.637184	40.188058
3111.452613	299424.645308	40.193076
3114.276079	299971.831803	40.198093
3117.975564	300506.970145	40.203111
3121.095211	301060.497134	40.208128
3124.402035	301616.781825	40.213146
3128.179315	302157.425949	40.218164
3131.188198	302705.216015	40.223181
3134.242113	303243.829264	40.228199
3137.432329	303798.357691	40.233216
3140.518383	304357.161110	40.238234
3143.986513	304921.635983	40.243252
3146.846662	305478.964738	40.248269
3149.832074	306028.246559	40.253287
3152.842398	306592.088872	40.258304
3156.012349	307158.235327	40.263322
3159.446079	307720.831451	40.268340
3162.389026	308297.229758	40.273357
3165.637362	308863.319228	40.278375
3168.799314	309438.070993	40.283392
3172.118833	310005.379899	40.288410
3175.569995	310568.448297	40.293428
3178.968945	311143.092169	40.298445
3182.660373	311695.094383	40.303463
3186.132663	312257.124333	40.308480
3189.239617	312828.722139	40.313498
3193.113833	313368.341357	40.318516
3196.204246	313929.801529	40.323533
3199.943222	314476.002307	40.328551
3203.199547	315028.261223	40.333568
3206.325269	315579.391726	40.338586
3210.209772	316119.103923	40.343604
3212.860300	316664.026612	40.348621
3215.923773	317195.707174	40.353639
3219.232472	317744.574770	40.358656
3222.569191	318291.401006	40.363674
3226.156959	318831.634071	40.368692
3229.265256	319363.611466	40.373709
3232.429458	319903.821044	40.378727
3235.560067	320442.658789	40.383744
3238.629872	320981.524625	40.388762
3242.124724	321506.538574	40.393780
3245.349425	322046.990889	40.398797
3248.284892	322586.263310	40.403815
3251.550565	323107.562934	40.408832
3254.264702	323631.606195	40.413850
3257.308302	324146.989799	40.418868
3259.878168	324663.328786	40.423885
3263.120776	325182.474553	40.428903
3266.186261	325701.311453	40.433920
3269.033893	326225.656159	40.438938
3271.837879	326758.272280	40.443956
3274.890310	327320.883219	40.448973
3278.069921	327861.342356	40.453991
3280.878162	328415.273406	40.459008
3284.068859	328984.182206	40.464026
3287.267153	329538.874070	40.469044
3290.366606	330116.609671	40.474061
3293.709471	330687.525083	40.479079
3296.931969	331281.942983	40.484096
3300.461803	331867.779883	40.489114
3303.882296	332445.506863	40.494132
3306.811719	333042.150184	40.499149
3310.304928	333632.912506	40.504167
3313.643446	334237.565691	40.509184
3316.963772	334840.461633	40.514202
3320.710732	335436.229502	40.519220
3324.447846	336031.837141	40.524237
3327.774341	336642.769329	40.529255
3331.740667	337228.911184	40.534272
3334.828313	337842.143418	40.539290
3338.615231	338436.080825	40.544308
3341.658532	339039.965494	40.549325
3345.494699	339641.763622	40.554343
3348.557137	340242.378485	40.559360
3352.203140	340843.881544	40.564378
3356.073320	341445.035135	40.569396
3359.501543	342052.765272	40.574413
3362.846507	342652.331368	40.579431
3366.200105	343252.139405	40.584448
3369.689679	343860.158133	40.589466
3373.496001	344447.093154	40.594484
3376.818592	345058.844619	40.599501
3380.184104	345660.536109	40.604519
3384.396747	346244.993166	40.609536
3388.039281	346837.389959	40.614554
3391.332752	347426.990517	40.619572
3394.906732	348010.628700	40.624589
3398.370374	348601.094893	40.629607
3402.076811	349179.290829	40.634624
3405.021077	349777.119557	40.639642
3408.775054	350353.563210	40.644660
3412.575882	350935.618281	40.649677
3416.248066	351519.356364	40.654695
3419.741939	352094.491136	40.659712
3423.614997	352667.350822	40.664730
3427.375544	353217.450266	40.669748
3431.112676	353781.462733	40.674765
3434.194694	354337.834555	40.679783
3437.731598	354896.280741	40.684800
3440.716704	355460.507036	40.689818
3444.351264	356027.461457	40.694836
3447.561462	356595.865908	40.699853
3450.665455	357167.977643	40.704871
3454.057550	357731.262888	40.709888
3457.055377	358317.540439	40.714906
3460.458812	358893.173144	40.719924
3463.420560	359473.502497	40.724941
3467.030640	360064.163256	40.729959
3470.377718	360639.746297	40.734976
3473.701788	361231.873521	40.739994
3477.552744	361811.918163	40.745012
3481.156171	362380.237273	40.750016
3484.500232	362903.277851	40.755021
3487.904725	363392.809436	40.760026
3490.486947	363851.054608	40.765031
3493.580421	364246.553927	40.770036
3496.119674	364608.543550	40.775040
3498.058373	364920.592516	40.780045
3500.877575	365175.611667	40.785050
3502.612942	365415.425260	40.790055
3504.373700	365602.739886	40.795060
3506.332310	365752.977756	40.800064
3507.587401	365872.402998	40.805069
3509.088428	365953.677849	40.810074
3509.983814	366003.795233	40.815079
3511.041856	366044.460968	40.820084
3512.024640	366051.549421	40.825088
3512.797534	366033.440700	40.830093
3513.706290	365995.772288	40.835098
3513.930934	365945.125283	40.840103
3514.637905	365881.750037	40.845108
3515.852759	365792.938539	40.850112
3516.580971	365693.200839	40.855117
3517.213162	365565.630468	40.860122
3517.407834	365428.345457	40.865127
3517.703923	365275.824414	40.870132
3518.100814	365121.508294	40.875136
3517.801288	364954.366735	40.880141
3518.192986	364785.134772	40.885146
3517.999711	364614.900276	40.890151
3518.451720	364432.368015	40.895156
3518.366635	364246.437130	40.900160
3518.015626	364055.744071	40.905165
3518.372542	363859.222456	40.910170
3518.169911	363659.712022	40.915175
3518.239389	363459.573468	40.920180
3517.915497	363258.275086	40.925184
3517.653976	363047.411363	40.930189
3517.529210	362851.847365	40.935194
3517.054090	362645.003460	40.940199
3517.065088	362453.633877	40.945204
3517.034052	362250.351865	40.950208
3516.656719	362059.090998	40.955213
3516.810980	361860.402319	40.960218
3516.707606	361656.085654	40.965223
3516.565585	361452.281841	40.970228
3516.306975	361262.649164	40.975232
3515.950023	361070.768928	40.980237
3516.123938	360867.674343	40.985242
3515.609086	360678.357389	40.990247
3515.454883	360480.597012	40.995252
3515.666660	360289.029896	41.000256
3515.046192	360102.419504	41.005261
3515.200883	359908.978320	41.010266
3514.282333	359733.949518	41.015271
3514.357395	359549.692561	41.020276
3514.010281	359365.195222	41.025280
3513.444925	359200.121262	41.030285
3513.591574	359025.380068	41.035290
3513.647035	358868.111359	41.040295
3513.192962	358692.496016	41.045300
3513.097218	358528.768532	41.050304
3512.953441	358364.259806	41.055309
3512.456509	358187.987471	41.060314
3512.294180	358047.496512	41.065319
3512.266334	357894.556238	41.070324
3512.217970	357741.643812	41.075328
3512.204756	357576.017720	41.080333
3511.869685	357432.882278	41.085338
3511.611275	357282.135122	41.090343
3511.780564	357128.423337	41.095348
3511.239456	356977.693275	41.100352
3511.568251	356840.881878	41.105357
3511.450927	356705.486328	41.110362
3510.763603	356562.757499	41.115367
3510.782875	356422.027574	41.120372
3510.595200	356292.969716	41.125376
3510.297919	356153.660298	41.130381
3510.655759	356012.850425	41.135386
3509.907026	355883.014030	41.140391
3510.305929	355763.902131	41.145396
3510.207508	355633.455176	41.150400
3509.744472	355513.307295	41.155405
3510.053940	355373.264571	41.160410
3509.719267	355265.117852	41.165415
3509.480454	355144.984502	41.170420
3509.577708	355017.554563	41.175424
3509.011900	354896.174882	41.180429
3508.987877	354775.727112	41.185434
3509.089416	354669.391336	41.190439
3508.767360	354558.698503	41.195444
3508.657822	354453.106531	41.200448
3508.495818	354339.897118	41.205453
3508.498379	354226.483768	41.210458
3508.040520	354130.019004	41.215463
3507.837596	354019.254910	41.220468
3508.197787	353913.867641	41.225472
3508.055224	353819.360879	41.230477
3508.002361	353715.587723	41.235482
3507.827176	353614.781761	41.240487
3507.647124	353515.857183	41.245492
3507.720094	353421.290281	41.250496
3507.267854	353337.150085	41.255501
3507.301517	353236.564611	41.260506
3507.235633	353149.237334	41.265511
3507.301979	353053.958658	41.270516
3507.395554	352969.656302	41.275520
3507.257889	352884.550891	41.280525
3507.399244	352785.828223	41.285530
3507.044240	352700.908658	41.290535
3506.857422	352605.922233	41.295540
3506.853179	352523.565761	41.300544
3507.297546	352445.257151	41.305549
3507.284385	352349.327859	41.310554
3506.741735	352259.301667	41.315559
3506.912454	352180.374097	41.320564
3506.676508	352088.545773	41.325568
3506.153052	352002.887997	41.330573
3506.698869	351925.833306	41.335578
3506.604898	351857.164744	41.340583
3506.408673	351769.650643	41.345588
3506.441204	351697.504997	41.350592
3506.402575	351609.762582	41.355597
3506.634266	351530.163023	41.360602
3506.149036	351457.919475	41.365607
3506.291635	351375.028824	41.370612
3506.506180	351300.057783	41.375616
3506.533541	351222.548279	41.380621
3506.692366	351124.656670	41.385626
3506.453614	351055.017554	41.390631
3506.156815	350982.819885	41.395636
3506.225825	350899.659851	41.400640
3505.754743	350836.640262	41.405645
3506.008185	350746.689340	41.410650
3506.120541	350679.791023	41.415655
3505.904165	350601.174049	41.420660
3505.921660	350534.671503	41.425664
3505.685668	350464.751069	41.430669
3505.489612	350401.331952	41.435674
3505.848310	350330.327285	41.440679
3505.411559	350268.445186	41.445684
3505.676673	350190.921651	41.450688
3505.686990	350120.453736	41.455693
3505.879950	350045.025594	41.460698
3505.649142	349983.060065	41.465703
3505.352043	349917.571215	41.470708
3505.883891	349830.930024	41.475712
3505.442853	349774.131870	41.480717
3505.373731	349708.988445	41.485722
3505.177106	349644.093523	41.490727
3505.376332	349585.797243	41.495732
3505.427865	349518.397594	41.500736
3505.986246	349450.232559	41.505741
3505.639948	349378.445792	41.510746
3505.318375	349306.070327	41.515751
3505.284900	349241.174643	41.520756
3505.373161	349171.861956	41.525760
3505.293148	349115.413229	41.530765
3505.587181	349048.101991	41.535770
3505.353265	348987.990853	41.540775
3505.333094	348903.466863	41.545780
3505.011201	348850.055093	41.550784
3505.000173	348794.357738	41.555789
3505.324384	348729.507077	41.560794
3504.946039	348674.705603	41.565799
3504.809742	348613.917624	41.570804
3504.923958	348549.404352	41.575808
3505.071733	348499.783083	41.580813
3504.993376	348429.554152	41.585818
3505.143271	348372.204028	41.590823
3505.296681	348314.802415	41.595828
3505.282366	348242.122587	41.600832
3505.018506	348185.192438	41.605837
3505.452194	348120.374397	41.610842
3505.040641	348056.958881	41.615847
3505.019234	347995.846823	41.620852
3505.008873	347934.453287	41.625856
3504.899243	347877.041006	41.630861
3504.785570	347808.519571	41.635866
3504.751238	347760.171247	41.640871
3505.109286	347700.931723	41.645876
3505.119028	347635.975330	41.650880
3504.953775	347584.240475	41.655885
3504.956634	347526.072825	41.660890
3505.078338	347465.776481	41.665895
3504.911260	347396.754054	41.670900
3504.955305	347338.223748	41.675904
3504.453416	347287.100123	41.680909
3504.453457	347232.822124	41.685914
3504.503541	347176.171901	41.690919
3504.458583	347127.265007	41.695924
3504.880052	347072.921170	41.700928
3504.728558	347018.971483	41.705933
3505.099644	346954.593121	41.710938
3504.775995	346906.441125	41.715943
3504.676589	346837.305324	41.720948
3504.646769	346785.166810	41.725952
3504.380501	346731.310792	41.730957
3504.808189	346673.253519	41.735962
3504.636487	346622.204618	41.740967
3504.603028	346557.278284	41.745972
3504.969442	346509.221726	41.750976
3504.225039	346448.448167	41.755981
3504.507760	346393.285844	41.760986
3504.432901	346340.492635	41.765991
3504.387062	346289.855848	41.770996
3504.704468	346237.738727	41.776000
3504.951208	346184.742687	41.781005
3504.749581	346124.621373	41.786010
3504.762027	346077.814207	41.791015
3504.782952	346014.047867	41.796020
3504.757732	345965.797241	41.801024
3504.461398	345908.385227	41.806029
3504.584472	345844.475552	41.811034
3504.291614	345794.944277	41.816039
3504.526096	345743.779993	41.821044
3504.259311	345677.871312	41.826048
3504.431363	345636.403213	41.831053
3504.346185	345574.584802	41.836058
3504.166744	345533.781457	41.841063
3504.078587	345477.048200	41.846068
3504.105274	345441.017875	41.851072
3504.283234	345403.438507	41.856077
3504.519301	345348.230896	41.861082
3504.323447	345293.141258	41.866087
3503.927802	345244.159089	41.871092
3504.391464	345190.924347	41.876096
3504.026668	345136.954003	41.881101
3504.446279	345088.938007	41.886106
3504.287925	345040.859334	41.891111
3504.080998	344993.957690	41.896116
3504.335411	344946.551969	41.901120
3504.138905	344891.894006	41.906125
3504.289162	344834.690358	41.911130
3504.383819	344790.970462	41.916135
3503.902677	344741.111004	41.921140
3504.498440	344705.474422	41.926144
3503.930426	344648.763609	41.931149
3504.054753	344603.284532	41.936154
3503.801169	344555.474246	41.941159
3503.915683	344507.810013	41.946164
3503.960854	344459.241199	41.951168
3503.871721	344415.803676	41.956173
3504.182941	344366.456001	41.961178
3503.996361	344321.609711	41.966183
3504.152917	344275.362427	41.971188
3504.244763	344228.540368	41.976192
3504.560286	344182.802154	41.981197
3504.044679	344126.845083	41.986202
3503.971761	344074.531145	41.991207
3503.982853	344042.646120	41.996212
3504.235178	343981.967308	42.001216
3504.300140	343942.674988	42.006221
3504.117445	343880.461884	42.011226
3503.822520	343841.174601	42.016231
3504.056675	343794.151827	42.021236
3504.219335	343733.079721	42.026240
3504.253357	343704.191044	42.031245
3504.207109	343644.778534	42.036250
3504.007363	343596.602577	42.041255
3503.967612	343552.113823	42.046260
3504.315261	343505.810345	42.051264
3504.243661	343466.564161	42.056269
3504.106453	343418.073113	42.061274
3503.939201	343373.832804	42.066279
3503.979723	343321.474647	42.071284
3504.148773	343265.943584	42.076288
3504.237508	343212.255607	42.081293
3504.388124	343160.439448	42.086298
3503.934582	343118.201172	42.091303
3504.063028	343067.100255	42.096308
3504.156025	343013.614717	42.101312
3504.158012	342965.915014	42.106317
3504.344419	342921.034291	42.111322
3504.133949	342875.986432	42.116327
3504.052095	342827.587650	42.121332
3504.055610	342780.319703	42.126336
3503.665254	342739.088189	42.131341
3504.053922	342697.989664	42.136346
3503.844407	342645.796530	42.141351
3503.978366	342601.991469	42.146356
3504.194943	342543.883780	42.151360
3504.111843	342497.976536	42.156365
3503.958359	342448.011926	42.161370
3503.751319	342409.192449	42.166375
3503.402236	342361.317710	42.171380
3504.276465	342314.015345	42.176384
3503.832371	342280.801064	42.181389
3503.405012	342234.184241	42.186394
3503.537443	342201.286999	42.191399
3503.673692	342150.285232	42.196404
3503.960982	342114.770273	42.201408
3504.062723	342082.182816	42.206413
3504.093690	342019.272032	42.211418
3503.956021	341973.448872	42.216423
3504.174571	341928.841569	42.221428
3504.565025	341882.427567	42.226432
3503.773298	341826.458900	42.231437
3503.832321	341778.977546	42.236442
3503.608379	341733.828602	42.241447
3503.428592	341691.978260	42.246452
3503.583572	341648.880697	42.251456
3503.632182	341605.647069	42.256461
3503.792505	341569.312218	42.261466
3503.444824	341527.360671	42.266471
3503.314603	341488.451938	42.271476
3503.746481	341443.810824	42.276480
3503.433949	341405.718617	42.281485
3503.687510	341360.011768	42.286490
3503.532072	341320.064250	42.291495
3503.558805	341282.198818	42.296500
3503.855481	341242.740262	42.301504
3503.571446	341201.744667	42.306509
3503.649490	341155.480033	42.311514
3503.534463	341114.102050	42.316519
3503.795646	341076.708466	42.321524
3503.649496	341025.164178	42.326528
3503.323326	340987.302491	42.331533
3503.632846	340953.562839	42.336538
3503.704904	340925.377923	42.341543
3503.392592	340876.376618	42.346548
3503.802826	340820.931289	42.351552
3503.705199	340790.992725	42.356557
3503.467960	340755.863155	42.361562
3503.462840	340713.653910	42.366567
3503.159523	340670.219623	42.371572
3503.735867	340628.911483	42.376576
3503.380791	340588.663642	42.381581
3503.459033	340546.364942	42.386586
3503.591964	340513.338907	42.391591
3503.423378	340468.281442	42.396596
3503.779773	340432.398045	42.401600
3503.277726	340393.825678	42.406605
3503.463367	340349.602924	42.411610
3503.682564	340325.513991	42.416615
3503.311800	340274.766409	42.421620
3503.375295	340228.807967	42.426624
3503.211443	340197.836652	42.431629
3503.179874	340154.435731	42.436634
3503.467735	340129.115424	42.441639
3503.243978	340084.472911	42.446644
3503.438957	340042.511443	42.451648
3503.466419	340015.400735	42.456653
3503.458811	339967.698464	42.461658
3503.407545	339927.046599	42.466663
3503.489545	339895.553623	42.471668
3503.212252	339849.800294	42.476672
3503.194767	339825.340999	42.481677
3503.331413	339779.650309	42.486682
3503.343854	339736.343746	42.491687
3503.172735	339704.203418	42.496692
3503.559973	339667.704167	42.501696
3503.536189	339632.285985	42.506701
3503.566171	339594.901394	42.511706
3503.024944	339559.665375	42.516711
3503.059580	339524.314281	42.521716
3502.971554	339486.515651	42.526720
3503.090091	339459.593780	42.531725
3502.873982	339409.253189	42.536730
3503.183020	339382.581332	42.541735
3503.531627	339355.293005	42.546740
3503.741525	339309.666604	42.551744
3503.582070	339269.030827	42.556749
3503.484098	339224.952532	42.561754
3503.309333	339192.252876	42.566759
3503.690535	339154.736884	42.571764
3503.701826	339104.131619	42.576768
3503.427636	339066.132655	42.581773
3503.595120	339024.199702	42.586778
3503.610686	338993.835151	42.591783
3503.272325	338943.716365	42.596788
3503.234380	338906.087335	42.601792
3502.872484	338877.739469	42.606797
3502.861430	338839.546743	42.611802
3503.252293	338810.623960	42.616807
3502.940394	338766.908973	42.621812
3503.051958	338732.994597	42.626816
3503.256662	338702.117212	42.631821
3503.438714	338664.199402	42.636826
3503.691962	338631.330915	42.641831
3503.450219	338595.615047	42.646836
3503.558184	338548.833793	42.651840
3503.173461	338526.007383	42.656845
3503.173505	338473.470346	42.661850
3503.103344	338447.924843	42.666855
3503.231263	338410.091480	42.671860
3503.241691	338361.214512	42.676864
3503.188999	338331.266898	42.681869
3503.060620	338293.040993	42.686874
3503.628662	338257.859948	42.691879
3502.980766	338226.580810	42.696884
3503.400286	338187.455785	42.701888
3503.026236	338155.498231	42.706893
3503.304396	338112.936686	42.711898
3503.276961	338081.332004	42.716903
3503.535930	338039.637971	42.721908
3503.569657	338001.742549	42.726912
3502.890377	337970.417214	42.731917
3503.245647	337927.182278	42.736922
3503.113346	337898.543616	42.741927
3503.143071	337860.801250	42.746932
3503.255922	337816.459560	42.751936
3503.233332	337786.506812	42.756941
3503.432355	337750.416363	42.761946
3503.288173	337713.260364	42.766951
3503.036844	337685.377527	42.771956
3503.328213	337632.971950	42.776960
3502.957290	337611.338027	42.781965
3503.249728	337568.137872	42.786970
3503.168164	337537.482054	42.791975
3503.176736	337512.381383	42.796980
3503.128512	337465.648469	42.801985
3503.175160	337430.700342	42.806989
3503.373660	337389.549008	42.811994
3503.044376	337345.707861	42.816999
3503.099295	337323.880351	42.822004
3503.173383	337293.378118	42.827009
3502.879143	337261.458218	42.832013
3502.897775	337224.963005	42.837018
3503.622750	337192.604709	42.842023
3502.811893	337155.729898	42.847028
3503.041886	337136.214627	42.852033
3502.898015	337096.692925	42.857037
3503.012489	337064.810975	42.862042
3503.434070	337039.009948	42.867047
3503.104683	336997.991181	42.872052
3503.087390	336964.425805	42.877057
3503.387953	336925.038203	42.882061
3503.060173	336893.021479	42.887066
3503.245214	336846.505780	42.892071
3502.966436	336820.304973	42.897076
3503.235920	336780.260856	42.902081
3503.023413	336745.403264	42.907085
3503.162629	336703.294020	42.912090
3503.461721	336679.063074	42.917095
3503.388973	336645.607759	42.922100
3503.182193	336597.550581	42.927105
3503.271650	336569.461277	42.932109
3503.028467	336532.268624	42.937114
3502.662688	336498.604465	42.942119
3502.755315	336467.666337	42.947124
3503.067455	336434.786707	42.952129
3503.093420	336405.435615	42.957133
3503.121058	336368.378669	42.962138
3503.466152	336330.661942	42.967143
3503.212530	336297.768506	42.972148
3503.290883	336259.610027	42.977153
3503.162805	336233.868540	42.982157
3502.945222	336191.712509	42.987162
3502.800843	336164.549372	42.992167
3502.860438	336132.497135	42.997172
3503.248783	336097.265687	43.002177
3502.848324	336066.658264	43.007181
3503.130115	336029.917464	43.012186
3502.767253	336002.635619	43.017191
3502.881722	335969.888061	43.022196
3503.037841	335931.488261	43.027201
3502.888463	335896.874354	43.032205
3502.508080	335867.992967	43.037210
3502.621279	335835.169193	43.042215
3502.552759	335811.579803	43.047220
3502.639967	335785.372170	43.052225
3502.891987	335768.039841	43.057229
3502.936178	335737.134070	43.062234
3503.005810	335708.564001	43.067239
3502.962653	335670.016920	43.072244
3503.049922	335640.197915	43.077249
3502.781897	335608.196206	43.082253
3502.786456	335580.653423	43.087258
3502.786412	335550.975090	43.092263
3502.935420	335520.688615	43.097268
3502.989240	335476.633036	43.102273
3502.868482	335458.061563	43.107277
3503.001368	335423.377858	43.112282
3503.268731	335382.340727	43.117287
3502.945958	335353.399110	43.122292
3503.060791	335312.945133	43.127297
3502.885722	335288.710769	43.132301
3502.810676	335243.276224	43.137306
3502.830107	335221.758173	43.142311
3502.587928	335196.516923	43.147316
3502.933924	335156.993210	43.152321
3502.821537	335127.789794	43.157325
3502.854473	335099.326694	43.162330
3502.941447	335066.608050	43.167335
3502.720135	335045.000200	43.172340
3503.088014	335007.075129	43.177345
3502.942524	334983.878669	43.182349
3502.810436	334950.456488	43.187354
3503.070860	334910.208305	43.192359
3502.883099	334891.290929	43.197364
3502.720058	334848.234767	43.202369
3502.807777	334827.112773	43.207373
3502.865991	334796.076878	43.212378
3502.985968	334772.381201	43.217383
3502.827526	334739.318980	43.222388
3502.898954	334710.646138	43.227393
3502.588496	334669.291226	43.232397
3502.583633	334649.251686	43.237402
3502.760128	334619.824894	43.242407
3502.502202	334587.693576	43.247412
3502.938450	334565.703370	43.252417
3502.730239	334532.725008	43.257421
3502.678122	334492.906495	43.262426
3502.626326	334473.382808	43.267431
3502.285907	334451.818582	43.272436
3502.853523	334422.712255	43.277441
3502.965008	334396.805056	43.282445
3502.761098	334370.056788	43.287450
3503.025674	334337.208140	43.292455
3502.643643	334303.773410	43.297460
3503.174136	334265.161043	43.302465
3502.774560	334236.281377	43.307469
3502.747651	334207.114805	43.312474
3502.648406	334178.671574	43.317479
3502.713425	334154.093924	43.322484
3502.925799	334113.979527	43.327489
3502.617031	334091.926951	43.332493
3502.672961	334066.333359	43.337498
3502.962401	334027.376771	43.342503
3502.717592	334004.780108	43.347508
3503.313526	333967.021959	43.352513
3502.781731	333935.619380	43.357517
3503.073939	333901.596153	43.362522
3503.056184	333870.698478	43.367527
3503.375593	333836.365769	43.372532
3503.489678	333803.514642	43.377537
3503.189678	333759.562967	43.382541
3502.877391	333727.973460	43.387546
3502.981709	333694.589670	43.392551
3502.875481	333674.005864	43.397556
3502.839991	333627.978253	43.402561
3502.875215	333600.174914	43.407565
3502.863565	333574.515206	43.412570
3502.900377	333537.428589	43.417575
3502.730620	333513.039652	43.422580
3502.925691	333476.996530	43.427585
3502.832423	333447.941429	43.432589
3502.994012	333413.429431	43.437594
3502.943376	333377.627912	43.442599
3502.664046	333353.408522	43.447604
3503.026515	333319.322972	43.452609
3502.816365	333285.860592	43.457613
3502.397105	333247.496712	43.462618
3502.694186	333227.282264	43.467623
3502.606125	333203.516242	43.472628
3502.718177	333169.494959	43.477633
3502.511333	333143.382105	43.482637
3502.899602	333120.508366	43.487642
3502.877229	333084.015478	43.492647
3502.587426	333067.656379	43.497652
3502.500692	333024.662557	43.502657
3502.453697	332999.898122	43.507661
3502.637022	332985.601754	43.512666
3502.306067	332953.836473	43.517671
3502.232246	332929.508531	43.522676
3502.511809	332899.835461	43.527681
3502.638155	332877.358401	43.532685
3502.833385	332854.082176	43.537690
3502.648159	332824.862874	43.542695
3502.355404	332799.577019	43.547700
3502.941625	332768.152092	43.552705
3502.970477	332746.987228	43.557709
3502.560394	332720.803976	43.562714
3502.892011	332688.223234	43.567719
3502.353803	332656.566255	43.572724
3502.607413	332624.709734	43.577729
3502.500079	332606.338232	43.582733
3502.261549	332575.550158	43.587738
3502.801197	332553.517262	43.592743
3502.412042	332527.356054	43.597748
3502.771534	332490.497971	43.602753
3503.099192	332464.962749	43.607757
3502.548914	332431.272776	43.612762
3502.513585	332415.458770	43.617767
3502.510309	332388.754180	43.622772
3502.460673	332364.040611	43.627777
3502.169374	332334.099863	43.632781
3502.568225	332313.614759	43.637786
3502.976154	332274.103829	43.642791
3502.440448	332254.018458	43.647796
3502.587904	332229.452168	43.652801
3502.857368	332205.146646	43.657805
3502.520845	332179.282214	43.662810
3502.700865	332140.188118	43.667815
3502.651211	332117.254757	43.672820
3502.530585	332084.464103	43.677825
3502.389574	332061.036248	43.682829
3502.345722	332029.988536	43.687834
3502.397718	332002.664663	43.692839
3502.437228	331986.355591	43.697844
3502.365220	331962.764334	43.702849
3502.468263	331939.781672	43.707853
3502.464404	331911.627107	43.712858
3502.858520	331891.015345	43.717863
3502.679882	331859.963035	43.722868
3502.379602	331835.771374	43.727873
3502.412392	331814.579947	43.732877
3502.237937	331786.502706	43.737882
3502.678047	331762.017746	43.742887
3502.508323	331733.202142	43.747892
3502.484569	331717.792992	43.752897
3502.426972	331688.934473	43.757901
3502.561133	331663.912076	43.762906
3502.481254	331635.998046	43.767911
3502.412107	331618.027073	43.772916
3502.553717	331585.958211	43.777921
3502.274175	331574.378496	43.782925
3502.247398	331548.440004	43.787930
3502.550444	331513.675371	43.792935
3502.336369	331500.279618	43.797940
3502.407187	331472.825270	43.802945
3502.712246	331446.250084	43.807949
3502.739528	331421.244161	43.812954
3502.698326	331391.874183	43.817959
3502.391054	331367.708749	43.822964
3502.512324	331329.207960	43.827969
3502.476534	331313.444441	43.832973
3502.606704	331282.445349	43.837978
3502.310169	331246.400323	43.842983
3502.392073	331233.416238	43.847988
3502.536301	331210.070649	43.852993
3502.178743	331194.001071	43.857997
3502.293039	331171.194240	43.863002
3502.456873	331145.276684	43.868007
3502.505957	331115.053109	43.873012
3502.949043	331084.615592	43.878017
3502.590290	331059.593204	43.883021
3502.398318	331042.124332	43.888026
3503.133972	331021.535262	43.893031
3502.686272	330989.455871	43.898036
3502.463618	330947.854338	43.903041
3502.492842	330926.815587	43.908045
3502.400285	330901.573630	43.913050
3502.489200	330869.334332	43.918055
3502.388749	330852.029174	43.923060
3502.418116	330825.471029	43.928065
3502.830947	330797.962981	43.933069
3502.545170	330780.534023	43.938074
3502.783176	330739.750796	43.943079
3502.780114	330711.747841	43.948084
3503.054464	330672.434102	43.953089
3503.039008	330653.513240	43.958093
3502.624327	330622.572971	43.963098
3502.754899	330583.790212	43.968103
3502.521069	330565.411986	43.973108
3502.365464	330543.257221	43.978113
3502.478901	330520.424707	43.983117
3502.247327	330489.684752	43.988122
3502.367098	330451.564849	43.993127
3502.481097	330439.821814	43.998132
3502.882220	330413.917716	44.003137
3502.514892	330387.726221	44.008141
3502.376158	330362.363926	44.013146
3502.627763	330332.769537	44.018151
3502.466147	330312.167110	44.023156
3502.824992	330288.813006	44.028161
3502.963648	330253.055426	44.033165
3502.506941	330229.395801	44.038170
3502.827105	330197.908448	44.043175
3502.365734	330184.448982	44.048180
3502.645400	330149.330675	44.053185
3502.743639	330121.998280	44.058189
3502.903262	330089.671028	44.063194
3502.650387	330052.676999	44.068199
3502.456396	330042.736798	44.073204
3502.735991	330006.015959	44.078209
3502.677145	329978.784213	44.083213
3502.535012	329950.624307	44.088218
3502.962252	329911.743844	44.093223
3502.519726	329894.618669	44.098228
3502.368629	329870.428000	44.103233
3502.050964	329848.730459	44.108237
3502.010389	329821.597503	44.113242
3502.419210	329798.616860	44.118247
3502.585168	329777.174681	44.123252
3502.550168	329748.489251	44.128257
3502.408319	329726.738848	44.133261
3502.131616	329709.486046	44.138266
3502.504312	329681.983458	44.143271
3502.396835	329656.921066	44.148276
3502.475670	329631.753358	44.153281
3502.374517	329606.257547	44.158285
3502.443742	329581.116739	44.163290
3502.415698	329564.689984	44.168295
3502.196081	329533.591319	44.173300
3502.505882	329506.251009	44.178305
3502.563126	329490.243355	44.183309
3502.281045	329461.062017	44.188314
3502.411103	329442.499459	44.193319
3502.374302	329415.670861	44.198324
3502.042485	329390.872129	44.203329
3502.267572	329368.072440	44.208333
3502.046969	329354.651527	44.213338
3502.174162	329314.774306	44.218343
3502.174901	329316.682059	44.223348
3502.375015	329272.291339	44.228353
3501.958387	329261.826000	44.233357
3502.160508	329236.104706	44.238362
3502.371229	329222.845551	44.243367
3502.325460	329207.845804	44.248372
3502.184817	329182.813706	44.253377
3502.224732	329153.480291	44.258381
3502.234428	329147.069170	44.263386
3502.635227	329108.726180	44.268391
3502.637604	329095.143302	44.273396
3502.495628	329067.542324	44.278401
3502.507558	329040.960246	44.283405
3502.173289	329024.555483	44.288410
3502.483748	328992.407343	44.293415
3502.192931	328980.701431	44.298420
3502.322623	328940.187545	44.303425
3502.138104	328936.604559	44.308429
3502.310562	328908.267772	44.313434
3502.510004	328880.053944	44.318439
3502.256134	328861.627164	44.323444
3501.982503	328842.592988	44.328449
3502.008350	328817.839982	44.333453
3502.222712	328792.065622	44.338458
3502.362512	328771.466355	44.343463
3502.247249	328758.486695	44.348468
3502.428362	328725.926054	44.353473
3502.554364	328712.857963	44.358477
3502.152330	328688.909105	44.363482
3502.435205	328656.968474	44.368487
3501.941474	328636.696645	44.373492
3502.413619	328615.307933	44.378497
3502.542459	328602.671778	44.383501
3502.390451	328572.452098	44.388506
3502.183728	328546.972030	44.393511
3501.989235	328527.569282	44.398516
3501.909893	328513.413889	44.403521
3502.211507	328491.975338	44.408525
3502.013516	328470.843447	44.413530
3502.569396	328429.423326	44.418535
3502.177893	328425.414651	44.423540
3502.331197	328400.488933	44.428545
3502.679276	328391.684900	44.433549
3502.233578	328370.438884	44.438554
3502.234295	328326.154441	44.443559
3502.080796	328312.875350	44.448564
3501.981801	328299.638645	44.453569
3502.037222	328268.954039	44.458573
3502.118569	328260.573029	44.463578
3502.189787	328239.297377	44.468583
3501.902088	328227.463574	44.473588
3502.434491	328192.863798	44.478593
3502.719003	328165.501061	44.483597
3502.152812	328149.691625	44.488602
3502.476443	328119.117784	44.493607
3502.060772	328101.504358	44.498612
3502.351315	328089.122677	44.503617
3502.240195	328052.155585	44.508621
3501.957662	328042.203221	44.513626
3502.085443	328010.744062	44.518631
3502.042154	327993.403314	44.523636
3502.203215	327981.753971	44.528641
3502.523402	327958.938673	44.533645
3502.109556	327935.932349	44.538650
3502.349976	327910.382292	44.543655
3502.116022	327892.257201	44.548660
3502.388296	327868.431846	44.553665
3502.154758	327848.602420	44.558669
3502.124075	327826.986293	44.563674
3502.349252	327786.558120	44.568679
3502.192886	327765.928109	44.573684
3502.693460	327749.621835	44.578689
3502.540836	327739.827236	44.583693
3502.282438	327709.521710	44.588698
3502.882003	327679.311581	44.593703
3502.693000	327656.778841	44.598708
3502.493085	327629.898108	44.603713
3502.358812	327606.084987	44.608717
3502.207901	327585.886459	44.613722
3502.426013	327546.502050	44.618727
3502.308498	327540.644638	44.623732
3502.106460	327509.287281	44.628737
3502.143715	327481.784496	44.633741
3502.228479	327465.695433	44.638746
3502.369316	327438.659799	44.643751
3501.980818	327417.302626	44.648756
3502.091223	327408.382742	44.653761
3502.380315	327384.071182	44.658765
3501.925716	327371.906981	44.663770
3502.329310	327345.415444	44.668775
3502.183152	327323.562645	44.673780
3502.138997	327293.121717	44.678785
3502.108411	327273.056929	44.683789
3502.087299	327254.109882	44.688794
3502.294373	327231.566143	44.693799
3501.931725	327215.215922	44.698804
3502.184898	327198.184814	44.703809
3502.285320	327174.334915	44.708813
3501.841214	327149.908375	44.713818
3502.279237	327139.182295	44.718823
3502.217665	327113.042799	44.723828
3502.168694	327084.383055	44.728833
3501.927850	327057.355685	44.733837
3502.102637	327045.296941	44.738842
3501.948038	327032.475462	44.743847
3502.105596	327020.851823	44.748852
3502.042963	327004.683764	44.753857
3502.392894	326982.575523	44.758861
3502.547375	326959.658258	44.763866
3502.350867	326939.924369	44.768871
3502.311814	326905.386971	44.773876
3502.308372	326875.524447	44.778881
3502.268239	326849.254257	44.783885
3502.087318	326834.986891	44.788890
3502.449517	326807.534828	44.793895
3502.042540	326796.965588	44.798900
3502.177623	326765.733252	44.803905
3502.352549	326747.289643	44.808909
3502.036736	326737.596505	44.813914
3502.143524	326714.101466	44.818919
3502.250848	326693.022873	44.823924
3502.569668	326674.684027	44.828929
3502.475563	326643.817946	44.833933
3502.048797	326620.482192	44.838938
3502.144480	326595.640631	44.843943
3502.153738	326585.744248	44.848948
3502.053459	326560.246350	44.853953
3502.035424	326537.762691	44.858957
3502.224740	326514.966940	44.863962
3502.809393	326504.980998	44.868967
3502.606192	326477.693007	44.873972
3502.504973	326451.457502	44.878977
3502.425807	326427.355296	44.883981
3502.361889	326407.651389	44.888986
3502.400091	326373.890078	44.893991
3502.145439	326357.904265	44.898996
3502.434943	326339.747892	44.904001
3502.092473	326313.575276	44.909005
3501.929289	326294.370075	44.914010
3502.190809	326270.240198	44.919015
3502.215331	326244.646368	44.924020
3502.253328	326222.637129	44.929025
3502.391802	326209.922409	44.934029
3502.322074	326190.499114	44.939034
3502.413357	326165.734288	44.944039
3502.171733	326142.013320	44.949044
3502.184816	326123.594612	44.954049
3502.566691	326097.792456	44.959053
3501.886419	326073.732704	44.964058
3502.442665	326046.402557	44.969063
3502.216929	326035.397910	44.974068
3502.381090	326016.675830	44.979073
3502.087085	325991.284034	44.984077
3501.966869	325969.019461	44.989082
3502.499603	325945.966450	44.994087
3502.216293	325934.080412	44.999092
3502.182578	325896.717730	45.004097
3501.815380	325878.129148	45.009101
3502.130673	325865.971875	45.014106
3502.116329	325845.700349	45.019111
3502.143113	325829.543344	45.024116
3502.155831	325797.896862	45.029121
3502.040834	325780.897013	45.034125
3501.894154	325762.706507	45.039130
3502.070324	325747.009543	45.044135
3502.124823	325722.529989	45.049140
3501.919023	325710.911641	45.054145
3502.152116	325693.908465	45.059149
3501.907011	325678.022651	45.064154
3502.432306	325658.506509	45.069159
3502.273972	325636.578380	45.074164
3502.335653	325614.310747	45.079169
3502.148204	325582.568056	45.084173
3502.190962	325575.464394	45.089178
3502.188719	325546.694540	45.094183
3501.736104	325535.801376	45.099188
3502.175385	325507.725929	45.104193
3502.439119	325491.379290	45.109197
3501.802052	325468.151912	45.114202
3502.186441	325451.277720	45.119207
3501.970733	325421.091025	45.124212
3502.302527	325400.358404	45.129217
3502.461701	325382.883277	45.134221
3502.346700	325373.743641	45.139226
3502.259969	325344.706973	45.144231
3502.453794	325323.359829	45.149236
3502.153922	325294.000158	45.154241
3502.452504	325286.475063	45.159245
3502.155848	325262.024439	45.164250
3501.960911	325228.680032	45.169255
3502.262816	325209.274754	45.174260
3502.114858	325189.278076	45.179265
3502.403087	325161.454842	45.184269
3502.167329	325146.941033	45.189274
3502.483766	325126.388732	45.194279
3502.534331	325108.904951	45.199284
3502.014512	325080.622324	45.204289
3502.482631	325066.405968	45.209293
3502.089166	325041.029058	45.214298
3502.357378	325015.727236	45.219303
3502.057142	324994.075228	45.224308
3501.945761	324979.440252	45.229313
3502.299403	324961.247848	45.234317
3502.088272	324948.078371	45.239322
3502.083354	324917.680435	45.244327
3502.230198	324903.056125	45.249332
3502.144014	324872.925186	45.254337
3502.205614	324858.670264	45.259341
3502.401309	324842.308516	45.264346
3501.811948	324813.527757	45.269351
3501.588482	324790.133878	45.274356
3502.270172	324775.375417	45.279361
3502.442584	324754.107626	45.284365
3501.987938	324742.044395	45.289370
3502.230755	324716.059500	45.294375
3502.057873	324697.058565	45.299380
3501.856470	324678.392760	45.304385
3502.351881	324655.828166	45.309389
3502.220072	324643.663791	45.314394
3502.499421	324615.281921	45.319399
3502.053876	324595.483894	45.324404
3501.790564	324573.266269	45.329409
3502.166654	324559.903535	45.334413
3502.005867	324534.159402	45.339418
3501.866045	324508.361114	45.344423
3501.890278	324492.941701	45.349428
3502.176825	324479.821823	45.354433
3502.150706	324463.036546	45.359437
3502.013351	324441.028197	45.364442
3502.305303	324419.716193	45.369447
3501.906960	324402.352846	45.374452
3502.273201	324384.259982	45.379457
3502.248946	324359.384851	45.384461
3501.925698	324350.608097	45.389466
3502.245958	324321.532812	45.394471
3502.031411	324322.176925	45.399476
3502.023043	324289.082550	45.404481
3502.363216	324271.655103	45.409485
3501.801922	324244.319591	45.414490
3502.338274	324224.495785	45.419495
3502.254844	324214.155352	45.424500
3502.093823	324190.624222	45.429505
3502.132766	324173.701508	45.434509
3502.170904	324157.516641	45.439514
3502.301265	324120.025055	45.444519
3502.064466	324104.976824	45.449524
3501.972940	324091.635828	45.454529
3502.240509	324057.150066	45.459533
3501.867841	324046.015115	45.464538
3502.094495	324014.842749	45.469543
3502.253196	324003.548782	45.474548
3501.772356	323983.679637	45.479553
3501.686492	323956.397146	45.484557
3501.611111	323964.854822	45.489562
3501.818486	323934.728395	45.494567
3502.060352	323911.515997	45.499572
3501.938459	323898.713885	45.504577
3502.001130	323879.701357	45.509581
3501.853622	323874.509500	45.514586
3501.906305	323848.426454	45.519591
3501.979201	323835.136107	45.524596
3501.878033	323826.248365	45.529601
3501.890630	323799.204840	45.534605
3501.698498	323790.789150	45.539610
3501.883824	323774.225082	45.544615
3502.019845	323755.073888	45.549620
3501.823700	323741.596424	45.554625
3501.835879	323712.772168	45.559629
3501.889365	323706.022664	45.564634
3501.880946	323687.860603	45.569639
3502.116357	323667.091235	45.574644
3501.848519	323651.309933	45.579649
3502.110908	323629.798610	45.584653
3502.116843	323619.571319	45.589658
3502.132558	323598.505394	45.594663
3502.103709	323579.328897	45.599668
3502.335834	323564.258378	45.604673
3502.206213	323535.506944	45.609677
3501.681530	323523.937601	45.614682
3501.866989	323496.638027	45.619687
3501.995448	323488.248705	45.624692
3501.767115	323475.463026	45.629697
3502.053791	323444.637043	45.634701
3502.027088	323441.232525	45.639706
3501.848041	323405.772710	45.644711
3502.149321	323396.338904	45.649716
3501.851476	323387.354477	45.654721
3501.943187	323369.583726	45.659725
3501.886798	323354.888740	45.664730
3501.699657	323328.639173	45.669735
3501.993563	323317.374860	45.674740
3501.878226	323298.440647	45.679745
3502.332769	323284.327552	45.684749
3501.935452	323266.658297	45.689754
3501.719980	323249.087933	45.694759
3501.986241	323226.812618	45.699764
3501.968633	323213.943188	45.704769
3502.107548	323193.366676	45.709773
3501.890528	323185.870558	45.714778
3502.068337	323154.679710	45.719783
3501.922726	323143.076713	45.724788
3501.773830	323122.341437	45.729793
3501.928032	323097.361463	45.734797
3501.619102	323093.975394	45.739802
3502.055475	323064.728528	45.744807
3501.919091	323056.482091	45.749812
3501.819692	323044.057809	45.754817
3502.193626	323013.192491	45.759821
3501.531481	322951.146775	45.764826
3501.348609	322846.567574	45.769831
3501.018548	322697.008078	45.774836
3500.790909	322510.976769	45.779841
3500.406631	322269.204496	45.784845
3499.584461	322000.303422	45.789850
3498.925794	321675.711661	45.794855
3497.843380	321335.842687	45.799860
3496.879311	320937.260634	45.804865
3496.329961	320504.850029	45.809869
3494.759951	320042.776646	45.814874
3493.497612	319537.654070	45.819879
3492.180370	318988.824879	45.824884
3490.663486	318417.961393	45.829889
3489.249806	317825.651737	45.834893
3487.655899	317198.657958	45.839898
3485.688217	316521.946284	45.844903
3483.969697	315837.196297	45.849908
3481.599409	315117.907860	45.854913
3479.941447	314362.722146	45.859917
3477.510580	313601.588401	45.864922
3474.773591	312812.525274	45.869927
3473.124615	311987.171834	45.874932
3470.699630	311163.884119	45.879937
3468.656018	310297.517802	45.884941
3466.310206	309406.728143	45.889946
3463.706680	308510.720083	45.894951
3460.720900	307591.699157	45.899956
3458.141817	306655.700081	45.904961
3455.700435	305691.210055	45.909965
3452.677066	304731.653247	45.914970
3449.943360	303735.359929	45.919975
3446.876103	302742.560825	45.924980
3444.104343	301733.612058	45.929985
3441.268127	300715.873578	45.934989
3438.110900	299669.608837	45.939994
3435.367601	298621.478176	45.944999
3432.068216	297554.528308	45.950004
3428.838219	296475.380846	45.955009
3425.916389	295391.328996	45.960013
3422.564578	294308.393092	45.965018
3419.406934	293201.759680	45.970023
3416.363472	292101.452100	45.975028
3412.703729	290988.620119	45.980033
3409.535424	289860.087181	45.985037
3405.835893	288741.672308	45.990042
3402.825968	287608.798447	45.995047
3399.251287	286476.400345	46.000052
3395.910096	285339.288019	46.005057
3392.806699	284188.830518	46.010061
3389.616865	283044.834070	46.015066
3385.859648	281885.733839	46.020071
3382.552944	280718.550697	46.025076
3379.070547	279554.151702	46.030081
3375.267546	278386.831323	46.035085
3371.910732	277220.035004	46.040090
3368.393627	276054.010305	46.045095
3364.577091	274877.627142	46.050100
3360.692407	273702.587415	46.055105
3357.310856	272531.807227	46.060109
3353.932782	271369.031512	46.065114
3350.886569	270193.839540	46.070119
3346.804923	269008.022719	46.075124
3343.444190	267819.710709	46.080129
3339.829970	266637.305753	46.085133
3335.509765	265455.836981	46.090138
3332.269035	264278.133646	46.095143
3328.913395	263101.148124	46.100148
3324.747571	261921.754976	46.105153
3321.443847	260734.499383	46.110157
3317.741246	259558.982459	46.115162
3314.236831	258375.095957	46.120167
3310.311455	257193.122786	46.125172
3306.515110	256016.466687	46.130177
3303.137461	254839.225848	46.135181
3299.079929	253671.096131	46.140186
3295.553958	252489.275075	46.145191
3292.067375	251307.260480	46.150196
3287.940984	250137.077095	46.155201
3284.436805	248959.199428	46.160205
3280.511142	247787.899163	46.165210
3276.959540	246620.659057	46.170215
3272.983765	245451.466038	46.175220
3269.563013	244295.576224	46.180225
3266.146527	243132.166584	46.185229
3262.078610	241970.890016	46.190234
3258.328019	240809.456840	46.195239
3254.423773	239656.650945	46.200244
3250.629494	238507.134325	46.205249
3246.951980	237344.682803	46.210253
3243.212919	236195.709981	46.215258
3239.504510	235053.554653	46.220263
3235.889822	233912.298647	46.225268
3232.028885	232772.351804	46.230273
3228.225240	231635.602900	46.235277
3224.259880	230503.614533	46.240282
3220.520657	229369.908528	46.245287
3217.369790	228239.140642	46.250292
3213.052486	227118.155329	46.255297
3209.527493	225997.250050	46.260301
3205.533197	224874.354730	46.265306
3201.998313	223747.415014	46.270311
3198.555025	222630.802096	46.275316
3194.381496	221527.191085	46.280321
3191.091399	220410.225455	46.285325
3187.264767	219316.063242	46.290330
3183.366260	218201.207886	46.295335
3179.393940	217093.064615	46.300340
3175.857604	215993.642826	46.305345
3172.066195	214894.161739	46.310349
3168.288628	213800.259338	46.315354
3164.592197	212712.332915	46.320359
3161.171082	211614.740350	46.325364
3156.837039	210527.430419	46.330369
3153.097298	209459.566552	46.335373
3149.599218	208374.427698	46.340378
3145.674918	207292.849294	46.345383
3142.072632	206214.409547	46.350388
3137.942399	205139.266452	46.355393
3134.150611	204069.220977	46.360397
3130.666833	203022.436371	46.365402
3126.667500	201963.793919	46.370407
3123.485458	200912.008807	46.375412
3119.440989	199856.035237	46.380417
3115.756836	198800.521999	46.385421
3112.042309	197763.254943	46.390426
3108.090027	196714.979817	46.395431
3104.644754	195674.961065	46.400436
3100.616694	194641.025489	46.405441
3096.798493	193610.656081	46.410445
3093.215249	192593.704323	46.415450
3089.594641	191568.057594	46.420455
3085.929582	190544.412869	46.425460
3082.697881	189522.110311	46.430465
3078.792439	188497.273531	46.435469
3074.786048	187477.784120	46.440474
3070.879004	186466.081052	46.445479
3067.374508	185461.582430	46.450484
3063.398292	184451.030400	46.455489
3059.487002	183450.944090	46.460493
3055.697796	182459.277471	46.465498
3052.497670	181464.626826	46.470503
3048.417327	180470.658600	46.475508
3044.507871	179492.817900	46.480513
3040.957782	178511.825728	46.485517
3036.719079	177533.116103	46.490522
3033.236230	176560.691011	46.495527
3029.339275	175599.430118	46.500532
3025.639065	174644.298774	46.505537
3021.819706	173673.513644	46.510541
3018.039487	172732.523006	46.515546
3014.181326	171791.810595	46.520551
3009.871850	170844.547866	46.525556
3006.262094	169919.045176	46.530561
3002.430237	168976.709424	46.535565
2998.505279	168058.026183	46.540570
2994.519382	167137.836850	46.545575
2991.052880	166230.995234	46.550580
2987.294139	165329.289897	46.555585
2983.496273	164413.766613	46.560589
2979.909335	163528.109623	46.565594
2975.379144	162629.806678	46.570599
2971.775022	161742.305587	46.575604
2967.469792	160867.768483	46.580609
2963.971102	160000.271054	46.585613
2959.579755	159139.135743	46.590618
2955.807003	158280.703587	46.595623
2951.894738	157429.165322	46.600628
2947.861726	156594.852280	46.605633
2944.101453	155761.539476	46.610637
2940.119131	154944.499711	46.615642
2936.057738	154122.240504	46.620647
2932.383788	153308.141378	46.625652
2928.186917	152516.240769	46.630657
2924.377239	151711.234295	46.635661
2920.416019	150939.833861	46.640666
2916.309393	150161.951446	46.645671
2912.219782	149393.710766	46.650676
2908.139910	148644.440276	46.655681
2904.377720	147887.063259	46.660685
2900.162397	147168.133313	46.665690
2896.026615	146425.113032	46.670695
2892.382377	145714.105592	46.675700
2887.729580	145002.743328	46.680705
2884.007948	144300.751160	46.685709
2879.667300	143617.722169	46.690714
2875.772454	142936.376374	46.695719
2872.216869	142266.260391	46.700724
2868.182382	141615.809602	46.705729
2864.122011	140955.561889	46.710733
2859.919171	140317.827240	46.715738
2855.897914	139687.528535	46.720743
2851.978646	139062.973068	46.725748
2847.885355	138444.916091	46.730753
2844.332056	137839.111362	46.735757
2840.139601	137231.912782	46.740762
2836.359663	136648.435735	46.745767
2832.692045	136080.431333	46.750772
2828.841673	135409.466538	46.755777
2825.720131	134823.302516	46.760781
2821.769862	134269.829416	46.765786
2817.862432	133700.391261	46.770791
2814.312610	133135.713386	46.775796
2810.463090	132584.637271	46.780801
2806.933876	132027.704833	46.785805
2802.772909	131482.619037	46.790810
2799.160877	130933.396850	46.795815
2795.853584	130390.278198	46.800820
2792.205440	129861.389802	46.805825
2788.559356	129316.353219	46.810829
2784.373150	128786.035587	46.815834
2781.055416	128264.315232	46.820839
2777.961374	127732.530850	46.825844
2774.024962	127208.948463	46.830849
2770.789048	126681.269862	46.835853
2766.700044	126167.658182	46.840858
2763.336375	125658.468016	46.845863
2760.308363	125125.575107	46.850868
2756.566234	124616.545949	46.855873
2753.285640	124092.787061	46.860877
2749.258472	123577.049245	46.865882
2745.674189	123058.667413	46.870887
2742.473200	122552.492800	46.875892
2739.173113	122045.615192	46.880897
2735.413132	121522.715217	46.885901
2731.931575	121003.619582	46.890906
2728.469607	120498.478671	46.895911
2724.904323	119980.249113	46.900916
2721.281330	119471.560494	46.905921
2718.087321	118955.728643	46.910925
2714.349752	118453.137312	46.915930
2710.946366	117931.400587	46.920935
2707.236494	117412.796099	46.925940
2703.168063	116913.748298	46.930945
2699.571802	116412.370254	46.935949
2696.210526	115908.597275	46.940954
2692.645904	115403.286066	46.945959
2689.188560	114893.807163	46.950964
2685.895324	114397.673469	46.955969
2681.797023	113895.848318	46.960973
2678.671070	113393.802488	46.965978
2674.960049	112901.339817	46.970983
2671.397710	112393.997489	46.975988
2667.524302	111906.901087	46.980993
2664.078113	111417.723296	46.985997
2660.509230	110924.744420	46.991002
2656.911341	110435.184221	46.996007
2653.204168	109954.979626	47.001012
2649.397254	109465.058620	47.006017
2645.926445	108991.899121	47.011021
2641.422977	108527.310119	47.016026
2637.799127	108059.119827	47.021031
2633.966239	107587.879213	47.026036
2629.985235	107128.134861	47.031041
2626.417237	106680.688880	47.036045
2622.993550	106220.946270	47.041050
2619.333673	105785.552139	47.046055
2615.860529	105334.651425	47.051060
2611.375198	104905.524235	47.056065
2607.829625	104471.235200	47.061069
2604.158677	104042.055879	47.066074
2600.540531	103621.174318	47.071079
2596.749266	103188.007962	47.076084
2593.029248	102787.045714	47.081089
2589.498088	102370.628041	47.086093
2585.687005	101956.686928	47.091098
2582.356740	101548.612003	47.096103
2578.841050	101144.193467	47.101108
2575.028144	100743.868033	47.106113
2571.840341	100335.176043	47.111117
2568.382962	99938.681771	47.116122
2564.789271	99538.820097	47.121127
2561.003075	99129.906040	47.126132
2557.254445	98733.700718	47.131137
2554.197614	98326.729623	47.136141
2550.796257	97928.218019	47.141146
2547.244516	97524.981695	47.146151
2544.141003	97121.401160	47.151156
2540.667029	96720.018476	47.156161
2537.370315	96320.189167	47.161165
2533.494594	95911.686380	47.166170
2530.072435	95506.892643	47.171175
2526.651273	95102.828360	47.176180
2523.190162	94704.125506	47.181185
2519.830184	94292.526565	47.186189
2516.349647	93880.837506	47.191194
2512.950121	93479.129234	47.196199
2509.488638	93060.827725	47.201204
2505.637492	92660.712608	47.206209
2502.521921	92247.870488	47.211213
2499.020563	91836.783984	47.216218
2495.244885	91421.552641	47.221223
2492.202974	91009.287716	47.226228
2488.185030	90604.079704	47.231233
2484.856428	90188.236726	47.236237
2481.502747	89781.005176	47.241242
2478.374048	89369.170185	47.246247
2475.115447	88944.719305	47.251252
2470.984587	88527.817344	47.256257
2467.756747	88112.394265	47.261261
2464.342085	87694.071306	47.266266
2460.825463	87283.659735	47.271271
2457.518008	86850.772630	47.276276
2453.727728	86447.275773	47.281281
2450.252892	86023.104007	47.286285
2446.933981	85603.081045	47.291290
2443.717238	85184.064575	47.296295
2440.004050	84759.694343	47.301300
2436.439363	84340.439406	47.306305
2432.852244	83928.866786	47.311309
2429.495368	83495.135710	47.316314
2425.724255	83075.232787	47.321319
2422.358354	82638.543718	47.326324
2418.569464	82218.465702	47.331329
2415.762072	81795.561024	47.336333
2411.929449	81372.542800	47.341338
2408.406252	80945.964394	47.346343
2405.268270	80525.162579	47.351348
2401.373915	80098.489744	47.356353
2398.018615	79667.052807	47.361357
2394.747711	79241.324905	47.366362
2390.557325	78811.136245	47.371367
2387.539140	78385.128188	47.376372
2384.132168	77961.663818	47.381377
2380.473159	77531.869686	47.386381
2377.125716	77103.240325	47.391386
2373.801957	76663.361957	47.396391
2369.928153	76237.634803	47.401396
2366.136985	75815.939897	47.406401
2362.758426	75382.821539	47.411405
2359.755837	74958.604450	47.416410
2356.395716	74530.906720	47.421415
2352.800167	74084.979128	47.426420
2349.263450	73655.100620	47.431425
2345.701293	73218.985486	47.436429
2342.479177	72782.481746	47.441434
2338.848620	72344.652004	47.446439
2335.214127	71906.157162	47.451444
2331.558096	71477.488042	47.456449
2328.118439	71035.536406	47.461453
2324.485239	70600.504096	47.466458
2321.102511	70172.004269	47.471463
2317.757840	69731.685100	47.476468
2314.140118	69299.046377	47.481473
2310.770549	68852.835872	47.486477
2307.148866	68413.642352	47.491482
2303.726918	67980.519162	47.496487
2300.330969	67531.942522	47.501492
2296.901469	67112.869984	47.506497
2293.403717	66658.300627	47.511501
2289.817002	66223.106439	47.516506
2286.191608	65776.526004	47.521511
2282.918462	65340.930018	47.526516
2279.038924	64892.202288	47.531521
2275.633083	64459.961692	47.536525
2271.930288	64030.002494	47.541530
2268.886405	63583.757616	47.546535
2265.775345	63140.615623	47.551540
2261.678019	62705.073113	47.556545
2258.009925	62253.503915	47.561549
2254.806181	61807.093673	47.566554
2251.225557	61356.840917	47.571559
2247.921596	60916.903743	47.576564
2244.378891	60470.399141	47.581569
2240.744344	60024.361180	47.586573
2237.635424	59575.273428	47.591578
2234.278495	59132.089528	47.596583
2230.448939	58684.640621	47.601588
2226.437890	58244.062173	47.606593
2223.495203	57785.006796	47.611597
2220.108589	57341.022758	47.616602
2216.532731	56892.958470	47.621607
2213.235370	56443.209550	47.626612
2209.301925	55987.699184	47.631617
2206.132303	55545.783073	47.636621
2202.292666	55093.631536	47.641626
2198.792476	54647.450288	47.646631
2195.340075	54183.823256	47.651636
2192.008576	53741.559981	47.656641
2188.405154	53290.757516	47.661645
2184.902757	52849.939661	47.666650
2180.743573	52392.097738	47.671655
2177.616051	51939.312399	47.676660
2174.101964	51494.544494	47.681665
2171.176262	51037.412671	47.686669
2167.652819	50591.667630	47.691674
2164.308250	50135.798676	47.696679
2160.889633	49674.767999	47.701684
2156.962096	49226.517969	47.706689
2153.442996	48763.523228	47.711693
2150.194197	48310.288884	47.716698
2146.351362	47849.912820	47.721703
2143.268014	47393.119171	47.726708
2139.371361	46935.389454	47.731713
2136.385947	46485.708577	47.736717
2132.592655	46027.752860	47.741722
2128.585052	45563.631101	47.746727
2125.794436	45105.049824	47.751732
2121.792735	44658.005283	47.756737
2118.399735	44194.945080	47.761741
2114.955022	43743.602410	47.766746
2111.685133	43286.242880	47.771751
2107.824236	42823.284104	47.776756
2104.255864	42367.118753	47.781761
2100.834218	41915.644930	47.786765
2097.270086	41458.197886	47.791770
2093.938087	41004.401806	47.796775
2090.467153	40544.467494	47.801780
2086.786070	40087.435075	47.806785
2083.548643	39622.012192	47.811789
2080.148853	39165.266061	47.816794
2076.639019	38708.286756	47.821799
2073.240972	38249.606999	47.826804
2069.327138	37792.329592	47.831809
2065.630239	37321.423543	47.836813
2062.571320	36864.362515	47.841818
2058.780054	36402.309460	47.846823
2055.793089	35945.339314	47.851828
2052.214354	35482.011664	47.856833
2048.574381	35013.119149	47.861837
2044.989369	34548.766973	47.866842
2041.466042	34090.652548	47.871847
2037.890404	33621.248493	47.876852
2034.323983	33171.216927	47.881857
2030.915750	32697.218573	47.886861
2026.888829	32240.566600	47.891866
2023.497940	31788.439605	47.896871
2020.114941	31324.552057	47.901876
2016.538069	30869.260780	47.906881
2013.041821	30417.813795	47.911885
2009.830341	29955.463882	47.916890
2006.052532	29498.941273	47.921895
2002.732224	29031.096720	47.926900
1998.971475	28579.705868	47.931905
1995.608613	28124.061795	47.936909
1991.943135	27668.563702	47.941914
1988.081891	27203.012301	47.946919
1984.955709	26748.420359	47.951924
1981.616046	26289.309798	47.956929
1978.141576	25836.744069	47.961933
1974.833833	25371.611171	47.966938
1971.221076	24920.139308	47.971943
1968.163397	24449.882215	47.976948
1964.238671	23997.142875	47.981953
1960.649921	23538.323967	47.986957
1957.165647	23074.120815	47.991962
1953.453140	22623.736314	47.996967
1950.549433	22145.204413	48.001972
1946.633382	21682.348980	48.006977
1943.211357	21220.555059	48.011981
1939.802263	20773.275746	48.016986
1936.010444	20309.527404	48.021991
1932.518812	19842.791609	48.026996
1928.622755	19385.713173	48.032001
1925.624462	18929.664804	48.037005
1921.705161	18471.325651	48.042010
1918.078799	18011.913019	48.047015
1914.911160	17557.797906	48.052020
1911.222540	17109.791092	48.057025
1907.501015	16654.177939	48.062029
1903.879012	16193.094761	48.067034
1900.360557	15744.871554	48.072039
1896.982492	15287.736468	48.077044
1893.360162	14843.296269	48.082049
1889.822502	14385.852969	48.087053
1886.229452	13936.350823	48.092058
1882.607690	13497.682043	48.097063
1879.365008	13042.574336	48.102068
1875.647468	12602.766617	48.107073
1872.152702	12151.069084	48.112077
1868.522404	11699.735869	48.117082
1865.193806	11260.779001	48.122087
1861.246008	10810.494748	48.127092
1857.564614	10369.632012	48.132097
1854.371620	9929.374732	48.137101
1850.786999	9488.612703	48.142106
1846.874828	9051.172317	48.147111
1843.239949	8620.804937	48.152116
1839.822776	8178.224799	48.157121
1836.712234	7742.811163	48.162125
1832.925016	7313.862040	48.167130
1828.960372	6883.928263	48.172135
1825.677000	6438.558632	48.177140
1821.362526	6018.697229	48.182145
1817.569456	5600.777045	48.187149
1814.121848	5174.597352	48.192154
1810.230151	4773.866760	48.197159
1805.639834	4385.234380	48.202164
1801.158208	4010.820533	48.207169
1796.668228	3644.674634	48.212173
1792.516532	3288.935085	48.217178
1788.137274	2952.144123	48.222183
1784.868436	2611.041590	48.227188
1780.435883	2297.727041	48.232193
1776.431355	1967.923638	48.237197
1772.776571	1660.093190	48.242202
1768.825523	1352.510303	48.247207
1764.695579	1058.682289	48.252212
1760.299322	783.959464	48.257217
1755.857570	542.916955	48.262221
1750.767898	312.437898	48.267226
1744.904301	124.985359	48.272231
1736.969389	28.898649	48.277236
1724.780867	70.247208	48.282241
1718.131125	77.926152	48.287245
1714.639230	75.056192	48.292250
1712.658255	83.495429	48.297255
1711.134721	71.084259	48.302260
1709.142786	74.273451	48.307265
1706.658317	84.293812	48.312269
1703.584265	76.110232	48.317274
1700.529309	81.698451	48.322279
1697.810305	78.578486	48.327284
1694.489626	82.366786	48.332289
1691.102689	77.860675	48.337293
1687.180357	83.080865	48.342298
1683.626061	85.459714	48.347303
1680.454343	77.487488	48.352308
1677.561610	87.372080	48.357313
1674.354264	79.525620	48.362317
1670.730766	75.521395	48.367322
1667.403392	80.168102	48.372327
1664.299469	69.787243	48.377332
1660.956739	73.370172	48.382337
1657.211953	76.003293	48.387341
1653.904376	73.471641	48.392346
1650.304357	71.627739	48.397351
1646.937774	78.422375	48.402356
1643.702873	76.502662	48.407361
1639.987185	81.200318	48.412365
1637.122446	71.228318	48.417370
1633.771170	74.629083	48.422375
1630.073399	74.097514	48.427380
1626.708923	76.468968	48.432385
1622.409611	75.831713	48.437389
1619.269922	74.814657	48.442394
1615.920911	81.606561	48.447399
1612.586227	73.681857	48.452404
1609.616379	72.037265	48.457409
1605.913609	80.640083	48.462413
1602.498795	70.835960	48.467418
1598.352856	80.728942	48.472423
1595.713817	73.309727	48.477428
1592.214140	93.153209	48.482433
1588.463954	79.693422	48.487437
1585.278093	80.028129	48.492442
1581.450903	82.145744	48.497447
1577.912233	77.204527	48.502452
1574.539504	78.770526	48.507457
1570.897669	80.375246	48.512461
1567.851955	77.435857	48.517466
1564.349457	70.600285	48.522471
1560.812123	73.508004	48.527476
1557.235879	83.081368	48.532481
1553.653312	79.504215	48.537485
1550.705316	73.863637	48.542490
1546.827668	82.284872	48.547495
1543.998625	77.802676	48.552500
1540.129726	75.889905	48.557505
1536.486096	78.412381	48.562509
1532.880375	66.578419	48.567514
1528.967656	76.704015	48.572519
1525.790981	71.298348	48.577524
1522.621769	75.252903	48.582529
1518.954563	82.356923	48.587533
1515.850205	73.855393	48.592538
1512.297936	79.359673	48.597543
1508.701182	78.511842	48.602548
1504.888598	83.626378	48.607553
1501.329004	73.927062	48.612557
1498.008452	71.242427	48.617562
1494.780361	75.481390	48.622567
1491.532550	70.033017	48.627572
1487.538709	80.307281	48.632577
1484.211423	77.285179	48.637581
1481.110429	75.195948	48.642586
1477.045653	80.928694	48.647591
1473.460420	75.542331	48.652596
1470.311278	78.965429	48.657601
1467.088997	81.090140	48.662605
1463.282611	69.303241	48.667610
1459.616052	78.520510	48.672615
1455.935243	69.735398	48.677620
1452.486522	76.593444	48.682625
1449.229086	71.007372	48.687629
1446.011316	71.679245	48.692634
1442.536152	77.788448	48.697639
1438.937492	71.534165	48.702644
1435.516293	78.315163	48.707649
1431.781807	77.159754	48.712653
1428.551507	71.923795	48.717658
1424.779687	81.799680	48.722663
1421.164676	73.472558	48.727668
1417.637761	74.274808	48.732673
1414.214495	75.972070	48.737677
1411.211121	75.440008	48.742682
1407.398261	69.181107	48.747687
1404.080922	65.265306	48.752692
1400.206684	78.431555	48.757697
1396.925882	76.348173	48.762701
1393.549465	68.774846	48.767706
1389.794442	83.893524	48.772711
1386.230377	69.866992	48.777716
1382.869181	76.660798	48.782721
1379.541937	74.790287	48.787725
1376.008496	72.382407	48.792730
1372.086693	74.704588	48.797735
1368.790052	69.811152	48.802740
1365.599047	69.539249	48.807745
1361.853353	67.455468	48.812749
1358.309758	73.018514	48.817754
1354.865131	80.148006	48.822759
1351.391965	71.969659	48.827764
1347.871068	73.495464	48.832769
1344.573380	77.950909	48.837773
1341.259711	72.183783	48.842778
1337.139952	71.303485	48.847783
1333.814088	75.064139	48.852788
1330.390148	68.396708	48.857793
1326.923438	71.872407	48.862797
1323.461384	63.996054	48.867802
1320.080655	73.083414	48.872807
1316.449784	63.072537	48.877812
1313.219643	69.358736	48.882817
1309.584881	68.668701	48.887821
1305.811149	66.469072	48.892826
1302.445993	83.823904	48.897831
1299.082795	76.232713	48.902836
1295.156456	78.498662	48.907841
1291.679371	81.485607	48.912845
1288.206985	66.998749	48.917850
1284.551911	66.840215	48.922855
1281.557473	65.620255	48.927860
1278.140369	74.213415	48.932865
1275.050315	71.584676	48.937869
1271.440407	69.568354	48.942874
1267.692777	69.202771	48.947879
1263.809265	67.687773	48.952884
1260.444945	70.087703	48.957889
1257.036181	66.160843	48.962893
1253.629562	60.212053	48.967898
1250.038805	68.961953	48.972903
1246.383016	64.703393	48.977908
1243.108736	58.832081	48.982913
1238.838131	71.180514	48.987917
1235.791768	66.899861	48.992922
1232.179366	66.519561	48.997927
1228.913657	65.528487	49.002932
1225.534896	76.399866	49.007937
1222.037221	74.641321	49.012941
1218.574889	60.538890	49.017946
1214.864254	64.463843	49.022951
1211.533340	66.358713	49.027956
1208.240708	62.951611	49.032961
1204.208123	64.300818	49.037965
1201.207314	60.076354	49.042970
1197.179176	72.216209	49.047975
1193.853905	62.974020	49.052980
1190.600383	65.575003	49.057985
1186.834670	65.117334	49.062989
1183.531485	64.214354	49.067994
1179.975333	70.905638	49.072999
1176.216059	67.881216	49.078004
1172.816155	65.443086	49.083009
1169.564686	64.184053	49.088013
1166.044342	55.797959	49.093018
1162.491674	68.205481	49.098023
1158.863096	72.174614	49.103028
1155.299170	67.686637	49.108033
1151.644536	61.080457	49.113037
1148.107148	65.418201	49.118042
1145.043886	67.913644	49.123047
1141.467148	59.789427	49.128052
1138.148108	69.227847	49.133057
1134.686516	69.877591	49.138061
1131.390881	62.041806	49.143066
1127.260530	66.272538	49.148071
1123.740866	65.327333	49.153076
1120.421902	66.571796	49.158081
1116.665152	65.451529	49.163085
1113.675152	64.186604	49.168090
1109.906474	58.724456	49.173095
1106.396591	61.665900	49.178100
1103.053600	65.846840	49.183105
1099.166184	67.233572	49.188109
1095.875696	68.366040	49.193114
1092.125062	67.561192	49.198119
1089.203170	67.430922	49.203124
1085.389912	63.690433	49.208129
1081.843651	70.851571	49.213133
1078.768321	64.579163	49.218138
1075.069442	71.656492	49.223143
1071.278424	70.082831	49.228148
1067.842616	67.995144	49.233153
1064.375801	69.433466	49.238157
1061.153332	69.248747	49.243162
1057.056067	74.382315	49.248167
1053.892851	65.807773	49.253172
1050.595450	68.020137	49.258177
1046.735243	60.961931	49.263181
1043.299654	65.736243	49.268186
1040.061347	63.861422	49.273191
1036.423624	65.952759	49.278196
1032.805361	63.292378	49.283201
1029.290722	66.361117	49.288205
1025.952675	64.498659	49.293210
1022.202353	60.931878	49.298215
1018.986851	66.257215	49.303220
1015.550348	61.309675	49.308225
1011.464317	73.401600	49.313229
1008.267113	58.413246	49.318234
1004.744222	66.349014	49.323239
1001.369609	63.043284	49.328244
997.806383	62.715467	49.333249
994.532219	68.106884	49.338253
991.195128	62.039747	49.343258
987.117510	63.462426	49.348263
984.053710	65.885200	49.353268
980.301608	54.517065	49.358273
976.683405	61.509074	49.363277
973.567934	57.321472	49.368282
969.709137	69.782976	49.373287
966.093568	65.856712	49.378292
962.876855	64.627093	49.383297
959.332799	64.796158	49.388301
956.233253	61.169214	49.393306
952.396333	61.551542	49.398311
948.791755	59.524944	49.403316
945.200430	64.285541	49.408321
941.619604	63.678903	49.413325
938.574190	62.587133	49.418330
934.998801	70.724064	49.423335
931.143522	68.154374	49.428340
928.131671	66.573338	49.433345
924.426068	61.193149	49.438349
920.997613	65.779703	49.443354
917.098403	68.069940	49.448359
913.933148	58.508675	49.453364
910.178235	56.679487	49.458369
906.001273	71.047599	49.463373
903.124354	66.465375	49.468378
899.456293	61.417860	49.473383
896.475596	68.664972	49.478388
892.965974	73.355911	49.483393
889.150587	64.522258	49.488397
885.812165	64.624521	49.493402
882.260951	69.347245	49.498407
878.809244	64.186962	49.503412
875.267353	71.176592	49.508417
871.661019	62.092109	49.513421
868.332926	53.312323	49.518426
864.569579	62.743982	49.523431
861.151791	65.696422	49.528436
858.120378	61.865901	49.533441
854.141960	60.141113	49.538445
850.384496	59.201323	49.543450
847.279207	67.850358	49.548455
844.291371	68.976867	49.553460
840.457887	63.328703	49.558465
836.521975	67.690545	49.563469
833.184997	61.496870	49.568474
829.573439	64.381402	49.573479
826.163300	62.701031	49.578484
822.960672	53.721393	49.583489
819.181182	63.142913	49.588493
815.769092	65.721156	49.593498
812.110325	62.076882	49.598503
808.328646	67.249928	49.603508
805.226925	69.637493	49.608513
801.536002	71.303713	49.613517
798.321985	63.085131	49.618522
794.372694	75.209561	49.623527
791.321178	69.718081	49.628532
788.189000	65.124990	49.633537
784.439852	70.691598	49.638541
781.015066	60.259619	49.643546
777.174120	63.793618	49.648551
773.514002	62.977887	49.653556
769.656970	65.410268	49.658561
766.145959	66.573933	49.663565
763.211145	66.496325	49.668570
759.730993	69.420519	49.673575
756.299337	70.998929	49.678580
752.864008	59.815643	49.683585
749.155041	63.797324	49.688589
745.540165	59.149671	49.693594
742.141140	58.771015	49.698599
738.759891	53.071457	49.703604
735.287404	54.428440	49.708609
731.431508	65.535443	49.713613
728.165479	54.762398	49.718618
724.654436	54.015214	49.723623
721.006556	59.910900	49.728628
717.702526	66.547144	49.733633
714.080330	59.186203	49.738637
710.723359	49.335296	49.743642
707.191197	63.049387	49.748647
702.906656	54.576707	49.753652
699.960912	67.686999	49.758657
696.556927	74.484336	49.763661
693.731914	61.390103	49.768666
690.021592	62.758806	49.773671
686.122953	60.028232	49.778676
682.511050	60.546405	49.783681
678.808949	66.539120	49.788685
675.341702	58.008816	49.793690
672.083189	62.224094	49.798695
668.611667	56.671474	49.803700
665.533074	52.857817	49.808705
661.585277	60.166903	49.813709
658.267115	53.821639	49.818714
654.395688	64.573568	49.823719
651.173817	58.121568	49.828724
647.758422	55.224026	49.833729
643.641535	63.628758	49.838733
640.646093	56.625833	49.843738
636.781184	61.264534	49.848743
633.498106	61.266465	49.853748
630.501168	54.336540	49.858753
626.189018	64.195322	49.863757
623.223932	50.325674	49.868762
619.416289	56.777735	49.873767
615.602776	54.476835	49.878772
612.204233	56.512001	49.883777
608.899288	57.207019	49.888781
605.766446	53.253123	49.893786
601.967388	57.609500	49.898791
598.648288	56.218701	49.903796
594.949177	56.570132	49.908801
591.394949	68.667865	49.913805
587.789627	62.490697	49.918810
584.618346	55.907451	49.923815
580.447709	61.163212	49.928820
577.504835	59.486062	49.933825
573.845588	67.307044	49.938829
570.613916	64.384075	49.943834
567.213839	64.587720	49.948839
563.414069	56.590083	49.953844
560.035123	56.258943	49.958849
556.611995	63.381959	49.963853
552.924830	53.452776	49.968858
549.349079	62.826775	49.973863
546.287377	60.323427	49.978868
542.503491	67.357078	49.983873
538.615993	70.509220	49.988877
535.666503	54.302372	49.993882
531.926966	65.663345	49.998887
528.747039	57.971005	50.003892
524.934646	61.877063	50.008897
521.360155	62.867146	50.013901
518.030783	57.229150	50.018906
514.183557	58.587551	50.023911
510.649546	53.784986	50.028916
507.249452	56.734705	50.033921
503.698274	54.715677	50.038925
500.327804	49.150522	50.043930
496.959173	49.260698	50.048935
493.370916	55.811490	50.053940
490.276954	51.250463	50.058945
486.474411	57.141773	50.063949
483.291345	50.107977	50.068954
479.481191	59.246394	50.073959
475.854721	55.638277	50.078964
472.262403	53.679441	50.083969
468.274544	62.260247	50.088973
465.425050	55.263105	50.093978
462.054671	65.006923	50.098983
458.406441	57.444448	50.103988
455.317267	62.452771	50.108993
451.585396	64.754977	50.113997
448.204002	58.552467	50.119002
444.287496	55.786752	50.124007
440.541483	60.372164	50.129012
437.302556	47.127307	50.134017
433.572140	58.372968	50.139021
430.460320	54.899867	50.144026
426.834161	58.925634	50.149031
423.191046	67.572995	50.154036
419.446028	61.094914	50.159041
415.852029	61.556553	50.164045
412.720529	52.904435	50.169050
409.769377	65.072794	50.174055
405.659409	58.835025	50.179060
402.125100	56.819714	50.184065
398.402394	59.136317	50.189069
395.710558	51.956461	50.194074
391.893919	61.570444	50.199079
388.571872	54.909467	50.204084
385.259995	54.435035	50.209089
381.101977	59.435761	50.214093
377.673578	58.634631	50.219098
374.248909	58.655474	50.224103
370.799611	66.396329	50.229108
367.311750	57.986353	50.234113
363.225922	66.231255	50.239117
360.303176	50.773243	50.244122
356.942301	64.014597	50.249127
353.245478	52.998662	50.254132
349.657051	55.911281	50.259137
346.103530	63.212795	50.264141
342.998248	58.033474	50.269146
339.486690	60.870854	50.274151
335.753898	57.405859	50.279156
332.258086	53.052947	50.284161
328.776273	56.679776	50.289165
325.159720	54.705755	50.294170
321.534662	58.712380	50.299175
318.159275	59.162143	50.304180
314.785385	62.101476	50.309185
311.573686	61.681058	50.314189
308.227367	58.861397	50.319194
304.535765	58.139218	50.324199
300.820972	63.371499	50.329204
297.308342	60.210747	50.334209
293.461882	60.332067	50.339213
290.306439	59.709910	50.344218
286.441163	67.047311	50.349223
282.781160	59.110229	50.354228
279.571793	58.300323	50.359233
276.108399	63.882597	50.364237
272.549069	61.444107	50.369242
269.436227	61.280379	50.374247
265.948252	66.597571	50.379252
262.313666	60.102330	50.384257
258.478719	61.110852	50.389261
255.268703	58.323761	50.394266
251.321625	55.768478	50.399271
247.911952	54.050154	50.404276
244.622827	60.911891	50.409281
240.819952	57.698263	50.414285
237.641121	54.918975	50.419290
234.402510	54.866578	50.424295
231.022621	58.328858	50.429300
227.529205	53.374496	50.434305
223.513194	56.787120	50.439309
220.172104	52.331049	50.444314
216.594976	53.207691	50.449319
212.796974	52.932350	50.454324
209.353709	54.743577	50.459329
205.683403	52.081939	50.464333
202.742846	59.180467	50.469338
199.338429	61.741763	50.474343
195.811062	61.259779	50.479348
192.254970	52.711773	50.484353
188.582576	61.737018	50.489357
185.052221	61.401029	50.494362
181.584735	57.939048	50.499367
177.912652	61.598681	50.504372
174.738423	56.825581	50.509377
171.322450	61.818369	50.514381
167.612079	60.934623	50.519386
163.868009	54.234994	50.524391
159.991740	60.700946	50.529396
157.181542	54.476000	50.534401
153.569771	56.398888	50.539405
150.495571	55.045952	50.544410
146.665410	53.045107	50.549415
143.022659	61.774684	50.554420
139.671283	54.928502	50.559425
136.108218	57.672687	50.564429
132.477132	49.686850	50.569434
128.728912	51.789167	50.574439
125.448566	56.925353	50.579444
122.079228	46.513369	50.584449
118.535018	66.876189	50.589453
115.165681	54.986774	50.594458
111.464664	52.987974	50.599463
108.166217	50.951808	50.604468
104.378621	45.049886	50.609473
101.041939	60.976582	50.614477
97.445547	48.603686	50.619482
93.987029	55.004603	50.624487
90.116413	53.392870	50.629492
86.864254	55.778617	50.634497
83.351744	53.478398	50.639501
80.055357	53.001597	50.644506
76.572392	57.678967	50.649511
72.961589	52.100689	50.654516
69.556123	48.246272	50.659521
66.013221	55.482879	50.664525
62.703933	53.315534	50.669530
59.036108	49.970187	50.674535
55.959380	51.534546	50.679540
52.220105	43.432700	50.684545
48.294049	50.197469	50.689549
44.711816	59.278286	50.694554
41.170910	58.073956	50.699559
37.866790	49.211519	50.704564
34.654856	53.716984	50.709569
31.054787	58.251245	50.714573
27.576224	54.607525	50.719578
23.759816	58.270665	50.724583
20.149901	60.398920	50.729588
16.979940	58.064361	50.734593
13.349852	55.355367	50.739597
9.781218	52.681097	50.744602
6.314036	48.048551	50.749607
3.002694	61.899111	50.754612