Fri Aug 26 11:16:53 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.042745	94.146564	0.000000
0.795227	101.369931	0.005005
0.675280	82.748499	0.010010
0.335873	84.525697	0.015014
0.488736	88.814121	0.020019
0.182933	81.028683	0.025024
-0.235093	72.896901	0.030029
0.269160	61.650857	0.035034
-0.434271	60.302097	0.040038
-0.731580	55.033614	0.045043
-1.190882	45.452992	0.050048
-1.802007	50.439305	0.055053
-1.834678	47.562469	0.060058
-1.902252	43.346516	0.065062
-2.743516	35.669777	0.070067
-2.137375	34.284795	0.075072
-2.950222	25.278068	0.080077
-2.996058	21.087209	0.085082
-3.611104	25.998199	0.090086
-3.849485	20.957825	0.095091
-3.840932	21.136982	0.100096
-4.070302	20.147835	0.105101
-4.289455	16.512290	0.110106
-4.853950	26.616440	0.115110
-4.951772	16.255078	0.120115
-4.961848	17.905066	0.125120
-5.663345	32.225542	0.130125
-6.386722	21.313027	0.135130
-7.028587	8.524441	0.140134
-6.353050	21.108797	0.145139
-6.228746	15.429845	0.150144
-7.012749	19.057390	0.155149
-6.677857	19.707739	0.160154
-6.790727	34.300388	0.165158
-7.068918	24.245505	0.170163
-7.380917	22.234710	0.175168
-8.068174	23.952171	0.180173
-8.771613	23.751818	0.185178
-9.288457	19.795640	0.190182
-9.079761	22.544151	0.195187
-8.846057	27.133174	0.200192
-9.409100	35.003569	0.205197
-9.487791	20.456885	0.210202
-9.427591	24.911576	0.215206
-9.909568	30.080249	0.220211
-10.678486	17.925186	0.225216
-11.509661	16.289446	0.230221
-10.864979	14.480865	0.235226
-11.218539	17.819936	0.240230
-11.517958	24.734987	0.245235
-11.232595	13.643274	0.250240
-11.440833	15.194406	0.255245
-11.420846	13.932325	0.260250
-12.369152	19.426692	0.265254
-12.431521	20.021838	0.270259
-12.526201	26.098283	0.275264
-13.471841	24.986547	0.280269
-13.687157	17.984288	0.285274
-14.249691	14.364244	0.290278
-14.314685	23.640837	0.295283
-14.160361	16.410189	0.300288
-14.510033	14.987372	0.305293
-14.176110	12.834884	0.310298
-13.893798	26.049921	0.315302
-14.533261	22.438689	0.320307
-15.146200	11.850660	0.325312
-15.488383	20.952118	0.330317
-15.616706	18.890581	0.335322
-16.462485	14.365544	0.340326
-16.636291	20.773835	0.345331
-16.777727	15.585497	0.350336
-17.042863	21.232915	0.355341
-17.117134	17.138231	0.360346
-17.035553	17.394600	0.365350
-17.299661	18.846867	0.370355
-17.580786	16.404174	0.375360
-18.094087	28.765522	0.380365
-18.381160	29.009690	0.385370
-18.553010	19.295746	0.390374
-18.573589	17.097215	0.395379
-19.004087	21.992124	0.400384
-19.791315	25.531591	0.405389
-19.471233	26.614501	0.410394
-19.625600	23.721816	0.415398
-19.940751	27.627528	0.420403
-20.465610	18.762623	0.425408
-20.998745	24.309405	0.430413
-21.064961	22.962672	0.435418
-21.158048	22.433180	0.440422
-21.288135	27.550227	0.445427
-21.419064	9.066623	0.450432
-21.405956	22.203352	0.455437
-21.993458	15.211588	0.460442
-22.386755	16.857970	0.465446
-22.545998	15.364376	0.470451
-22.386705	18.326215	0.475456
-23.553682	19.447674	0.480461
-23.767620	18.070159	0.485466
-23.539882	19.556575	0.490470
-24.176888	24.379237	0.495475
-23.763937	16.054829	0.500480
-24.231389	26.314704	0.505485
-24.509365	20.166894	0.510490
-25.092059	31.004680	0.515494
-25.414371	21.826673	0.520499
-25.707709	22.407162	0.525504
-25.647909	26.153258	0.530509
-25.397800	18.246495	0.535514
-25.558306	28.069452	0.540518
-26.362380	26.786984	0.545523
-26.674238	16.629786	0.550528
-27.129710	29.728749	0.555533
-26.656601	19.778351	0.560538
-27.014518	22.032971	0.565542
-27.456986	22.408897	0.570547
-27.841194	12.541366	0.575552
-28.313531	25.307606	0.580557
-28.483602	25.337411	0.585562
-28.957779	26.787586	0.590566
-28.953153	27.533647	0.595571
-29.115519	25.439446	0.600576
-29.900705	23.049925	0.605581
-30.112662	21.365229	0.610586
-30.300123	22.970072	0.615590
-30.307140	32.645752	0.620595
-30.132556	25.152528	0.625600
-30.315067	29.926573	0.630605
-30.519390	24.760679	0.635610
-31.235784	16.782944	0.640614
-31.763828	13.492878	0.645619
-31.446268	16.581929	0.650624
-31.813488	25.677795	0.655629
-31.766932	30.409848	0.660634
-31.962552	21.765753	0.665638
-32.718642	23.772332	0.670643
-32.662289	9.122380	0.675648
-33.414049	18.328733	0.680653
-33.140579	20.674866	0.685658
-33.813132	15.879259	0.690662
-34.289348	20.148557	0.695667
-34.260174	10.577320	0.700672
-34.724492	15.692621	0.705677
-34.513687	21.237463	0.710682
-34.601537	20.960247	0.715686
-34.891830	19.335202	0.720691
-35.158283	21.670491	0.725696
-35.737481	21.722868	0.730701
-35.957177	27.603650	0.735706
-36.363628	34.832752	0.740710
-36.359000	28.501738	0.745715
-36.161233	21.340253	0.750720
-37.075234	20.176138	0.755725
-36.913335	13.615005	0.760730
-37.365036	13.647532	0.765734
-37.719043	20.121842	0.770739
-37.726839	10.145089	0.775744
-38.716135	20.963921	0.780749
-38.929940	22.139447	0.785754
-38.978954	18.752650	0.790758
-39.061538	20.587927	0.795763
-39.022465	9.857257	0.800768
-39.285770	23.903861	0.805773
-39.461390	13.842508	0.810778
-39.566719	14.675288	0.815782
-40.129344	24.459615	0.820787
-39.986739	8.704778	0.825792
-40.418745	10.711514	0.830797
-40.893143	6.878442	0.835802
-41.854209	10.119117	0.840806
-42.055616	20.783638	0.845811
-41.460054	14.170804	0.850816
-42.081561	21.537784	0.855821
-42.357072	13.940644	0.860826
-42.259481	17.721982	0.865830
-42.355354	19.356855	0.870835
-42.318672	13.621948	0.875840
-42.997423	22.573335	0.880845
-43.196698	15.479999	0.885850
-43.278708	15.527729	0.890854
-43.919841	21.021725	0.895859
-44.672248	20.468342	0.900864
-45.053728	29.212102	0.905869
-45.237822	16.826789	0.910874
-44.990831	22.821561	0.915878
-45.040505	28.470234	0.920883
-44.983246	28.714571	0.925888
-45.095641	32.974680	0.930893
-45.791728	26.268730	0.935898
-46.065466	30.348322	0.940902
-46.378513	23.706117	0.945907
-46.220033	23.327275	0.950912
-46.955479	26.577115	0.955917
-47.766368	26.463093	0.960922
-47.841911	16.579140	0.965926
-48.117111	27.660101	0.970931
-48.049269	24.517692	0.975936
-48.211068	24.751845	0.980941
-47.792311	21.425090	0.985946
-48.123361	25.728732	0.990950
-48.973936	30.869376	0.995955
-48.994746	26.139965	1.000960
-49.339062	22.701073	1.005965
-49.353455	21.849291	1.010970
-50.005421	22.270491	1.015974
-50.866348	22.638807	1.020979
-50.546979	20.118437	1.025984
-50.624373	27.865757	1.030989
-50.748320	26.097758	1.035994
-50.926579	18.551912	1.040998
-51.479870	22.159354	1.046003
-51.811683	16.861458	1.051008
-52.180597	19.139936	1.056013
-52.367674	22.804251	1.061018
-52.353392	21.375385	1.066022
-52.774559	28.540338	1.071027
-52.463987	22.826057	1.076032
-52.992967	28.811939	1.081037
-53.630760	22.549316	1.086042
-53.731674	23.564901	1.091046
-53.918257	28.817289	1.096051
-53.852282	24.264185	1.101056
-54.291264	23.146329	1.106061
-54.950423	22.777738	1.111066
-54.748347	18.956391	1.116070
-55.261782	25.142325	1.121075
-55.260841	25.544123	1.126080
-55.462373	17.634918	1.131085
-56.445881	21.774400	1.136090
-56.778628	22.645753	1.141094
-57.341558	29.070341	1.146099
-56.795477	15.922795	1.151104
-57.300720	28.656194	1.156109
-57.108566	25.823449	1.161114
-56.961518	27.509082	1.166118
-56.948195	32.496236	1.171123
-57.371980	18.996676	1.176128
-58.490212	21.385495	1.181133
-58.607000	22.235878	1.186138
-58.411655	28.441165	1.191142
-59.189099	33.301514	1.196147
-59.547908	23.967845	1.201152
-59.923584	28.873201	1.206157
-59.915350	27.113094	1.211162
-60.007695	22.780787	1.216166
-59.975023	34.272544	1.221171
-59.927598	39.608719	1.226176
-60.311676	22.543872	1.231181
-60.843394	18.624813	1.236186
-61.072018	20.780211	1.241190
-61.617104	21.105679	1.246195
-61.436409	23.399820	1.251200
-61.923384	23.830131	1.256205
-62.711825	24.364325	1.261210
-62.935332	20.362478	1.266214
-62.967318	22.136095	1.271219
-62.597290	21.085259	1.276224
-63.126696	22.407997	1.281229
-63.206495	19.336031	1.286234
-63.762420	29.141462	1.291238
-64.159221	29.611514	1.296243
-64.262416	26.204680	1.301248
-64.611231	29.891015	1.306253
-64.268179	26.873428	1.311258
-64.321088	22.079417	1.316262
-65.144657	26.908981	1.321267
-65.253168	15.495796	1.326272
-65.533885	19.449926	1.331277
-65.673600	30.601539	1.336282
-66.417649	23.786004	1.341286
-67.008640	25.551750	1.346291
-66.791740	23.547190	1.351296
-66.981654	28.844387	1.356301
-66.749048	17.922236	1.361306
-67.117956	14.461866	1.366310
-67.765998	26.651205	1.371315
-68.233082	7.039911	1.376320
-68.645649	23.637500	1.381325
-68.649041	26.922051	1.386330
-68.483185	19.680119	1.391334
-68.833735	25.138362	1.396339
-69.225654	15.651672	1.401344
-69.563573	20.699838	1.406349
-69.558644	19.123738	1.411354
-69.479986	11.044366	1.416358
-69.775370	20.353661	1.421363
-70.556087	18.143775	1.426368
-70.942920	16.701436	1.431373
-71.227079	16.416822	1.436378
-70.958261	24.315871	1.441382
-71.523222	26.102872	1.446387
-71.743428	16.589446	1.451392
-72.320261	28.416535	1.456397
-72.570187	17.294277	1.461402
-72.635730	25.561751	1.466406
-72.847590	22.494528	1.471411
-72.776183	17.991199	1.476416
-73.003453	20.465914	1.481421
-73.567795	19.956015	1.486426
-73.821761	13.061016	1.491430
-74.555686	19.050331	1.496435
-74.142376	23.503822	1.501440
-74.081924	17.559577	1.506445
-74.592877	22.311994	1.511450
-74.759718	24.748828	1.516454
-75.748748	21.065482	1.521459
-75.732431	23.274489	1.526464
-76.454837	24.234985	1.531469
-76.187224	28.103742	1.536474
-76.030333	20.784114	1.541478
-76.185621	27.964614	1.546483
-76.128712	19.894952	1.551488
-76.990294	23.737051	1.556493
-77.547741	21.027346	1.561498
-77.316648	29.599799	1.566502
-77.535654	32.696467	1.571507
-77.581692	20.808497	1.576512
-78.472888	25.411317	1.581517
-78.779587	28.031273	1.586522
-78.699253	22.590115	1.591526
-79.216520	20.288592	1.596531
-79.110800	24.052845	1.601536
-79.325833	24.991289	1.606541
-80.047240	30.833131	1.611546
-80.048797	27.663564	1.616550
-80.419314	27.044395	1.621555
-80.746313	21.644513	1.626560
-80.836786	18.302137	1.631565
-80.690451	28.017206	1.636570
-80.792316	24.110310	1.641574
-81.777838	22.255004	1.646579
-81.627811	28.226909	1.651584
-81.696159	26.260435	1.656589
-82.141280	25.554809	1.661594
-82.689766	18.234282	1.666598
-83.297741	27.079741	1.671603
-83.390212	18.523992	1.676608
-83.640608	32.147823	1.681613
-83.549981	23.038398	1.686618
-83.941778	24.080291	1.691622
-83.681886	23.878642	1.696627
-83.846902	28.251341	1.701632
-84.528129	30.451902	1.706637
-85.013668	24.273139	1.711642
-84.761731	20.700285	1.716646
-85.166363	31.994380	1.721651
-85.193368	19.100573	1.726656
-85.516254	24.769637	1.731661
-86.173485	30.399014	1.736666
-86.384805	29.280511	1.741670
-86.842299	33.638642	1.746675
-86.759735	24.160327	1.751680
-86.616038	21.148472	1.756685
-86.910573	25.171191	1.761690
-87.423247	24.222992	1.766694
-87.769378	27.124324	1.771699
-87.775050	13.335053	1.776704
-88.734456	22.722427	1.781709
-89.170192	26.197676	1.786714
-88.942937	27.639875	1.791718
-89.220706	23.197239	1.796723
-89.280228	23.504050	1.801728
-89.524899	17.980624	1.806733
-89.821867	20.023281	1.811738
-89.739532	26.208198	1.816742
-89.955295	24.131804	1.821747
-90.297937	18.563523	1.826752
-90.725595	24.954391	1.831757
-90.934390	20.725635	1.836762
-91.136474	23.205920	1.841766
-91.921592	31.686670	1.846771
-92.502730	20.116127	1.851776
-92.031545	19.049541	1.856781
-91.919961	25.422885	1.861786
-92.310727	30.434991	1.866790
-92.574492	40.403736	1.871795
-92.810911	22.670521	1.876800
-93.574753	23.738705	1.881805
-93.849948	36.651416	1.886810
-93.803470	29.086395	1.891814
-94.010397	32.905657	1.896819
-93.946008	24.002791	1.901824
-94.071302	31.197603	1.906829
-94.716475	28.191520	1.911834
-94.878585	28.270704	1.916838
-95.499387	30.718112	1.921843
-95.268931	30.454608	1.926848
-95.914383	33.582874	1.931853
-96.486682	37.130006	1.936858
-96.299643	27.097603	1.941862
-96.697041	36.609443	1.946867
-96.592936	35.017900	1.951872
-96.613127	32.490290	1.956877
-97.555685	33.545174	1.961882
-97.986424	34.564658	1.966886
-98.526322	35.433466	1.971891
-98.137383	22.769114	1.976896
-98.490353	32.318325	1.981901
-98.766621	31.757246	1.986906
-98.605523	26.053584	1.991910
-99.093176	25.889237	1.996915
-98.717815	27.021973	2.006912
-98.728390	23.352584	2.016909
-98.763334	32.392610	2.026906
-98.587378	24.104189	2.036902
-97.671491	27.953201	2.046899
-97.244339	25.118450	2.056896
-96.118538	22.206597	2.066893
-95.777833	18.986178	2.076890
-95.696883	20.779481	2.086886
-95.410943	23.934651	2.096883
-94.529587	18.596394	2.106880
-94.178161	28.038742	2.116877
-93.305074	29.813243	2.126874
-93.070718	30.626018	2.136870
-92.894827	26.123002	2.146867
-92.034676	28.688273	2.156864
-91.744862	25.821055	2.166861
-90.706661	23.166754	2.176858
-90.510845	22.569570	2.186854
-90.231243	29.621991	2.196851
-89.562537	25.409696	2.206848
-88.843795	27.078353	2.216845
-88.838577	23.349487	2.226842
-88.102320	20.878410	2.236838
-87.584812	21.390514	2.246835
-87.102140	22.300836	2.256832
-86.080037	22.724872	2.266829
-86.060296	19.548092	2.276826
-86.259808	25.499896	2.286822
-85.083625	28.117327	2.296819
-84.454592	22.859535	2.306816
-83.392416	19.089641	2.316813
-83.331947	21.747745	2.326810
-83.043530	17.626340	2.336806
-82.967795	22.996780	2.346803
-81.978011	20.543247	2.356800
-81.603159	23.500848	2.366797
-81.108705	26.617219	2.376794
-80.316834	23.861893	2.386790
-80.119218	20.758783	2.396787
-79.533658	25.264256	2.406784
-78.904042	26.167538	2.416781
-78.878338	29.939750	2.426778
-78.077305	33.116089	2.436774
-77.561104	29.003562	2.446771
-77.020738	29.968256	2.456768
-76.146533	26.873837	2.466765
-75.996535	32.362593	2.476762
-75.808381	26.530403	2.486758
-74.735718	29.119605	2.496755
-74.541453	29.298748	2.506752
-74.310827	27.321365	2.516749
-73.341234	19.435213	2.526746
-73.011905	21.243694	2.536742
-72.598911	22.811075	2.546739
-71.821040	26.247603	2.556736
-71.532685	24.429119	2.566733
-71.136186	23.170318	2.576730
-70.539638	23.559247	2.586726
-70.262652	22.173340	2.596723
-69.046194	22.082458	2.606720
-68.775943	26.450132	2.616717
-68.810681	19.410912	2.626714
-68.196266	26.119775	2.636710
-67.620520	22.656860	2.646707
-66.755618	27.315238	2.656704
-66.527207	30.213281	2.666701
-66.298773	19.341355	2.676698
-65.372636	23.160262	2.686694
-64.567591	27.647401	2.696691
-64.570672	21.426852	2.706688
-64.308629	23.347176	2.716685
-63.767969	25.515548	2.726682
-62.968054	29.981313	2.736678
-62.246327	28.880941	2.746675
-61.898902	24.994259	2.756672
-61.565461	21.835156	2.766669
-60.802338	26.328823	2.776666
-60.551643	25.216264	2.786662
-60.044121	22.679434	2.796659
-59.490567	24.395986	2.806656
-59.090509	27.653763	2.816653
-58.222494	25.732355	2.826650
-57.455354	24.792801	2.836646
-57.138244	23.850459	2.846643
-57.508007	22.318171	2.856640
-56.605588	27.110087	2.866637
-56.115646	32.298834	2.876634
-55.525175	25.627918	2.886630
-54.927124	29.969896	2.896627
-54.862069	28.623322	2.906624
-53.564466	28.389931	2.916621
-53.252621	33.701440	2.926618
-53.196724	27.718785	2.936614
-52.458196	29.127780	2.946611
-51.791144	35.134728	2.956608
-51.727958	25.729827	2.966605
-50.967256	31.281882	2.976602
-50.627388	30.750965	2.986598
-49.664744	27.348181	2.996595
-49.027521	28.250280	3.006592
-48.833456	28.879266	3.016589
-48.545011	34.669573	3.026586
-48.249513	30.002218	3.036582
-47.716495	29.738991	3.046579
-46.660473	31.602217	3.056576
-46.078206	32.816971	3.066573
-45.697982	34.823430	3.076570
-45.282471	30.615711	3.086566
-45.493427	35.346572	3.096563
-44.704398	28.055547	3.106560
-43.824165	22.850506	3.116557
-43.144720	28.586269	3.126554
-42.770630	31.075173	3.136550
-42.708030	30.140780	3.146547
-42.160076	32.000752	3.156544
-41.037716	23.526962	3.166541
-40.988045	25.926998	3.176538
-40.660982	24.441431	3.186534
-39.976231	24.306629	3.196531
-39.429480	25.156293	3.206528
-38.323821	19.653235	3.216525
-38.407005	21.323213	3.226522
-38.126526	23.554269	3.236518
-37.401465	27.556536	3.246515
-36.554659	28.131408	3.256512
-36.644675	21.582281	3.266509
-36.374820	25.544553	3.276506
-35.350446	26.684136	3.286502
-35.025983	26.554747	3.296499
-33.928617	23.314715	3.306496
-33.424816	31.364902	3.316493
-33.630673	31.020320	3.326490
-33.201097	28.552644	3.336486
-32.286186	27.466542	3.346483
-32.035755	25.238995	3.356480
-31.218545	21.336187	3.366477
-30.829113	20.433268	3.376474
-30.912084	21.884642	3.386470
-29.697078	26.051370	3.396467
-29.369312	25.557182	3.406464
-29.047114	24.829451	3.416461
-27.767011	26.046423	3.426458
-27.904861	26.980505	3.436454
-27.806630	29.452173	3.446451
-26.915215	29.069791	3.456448
-26.245907	25.592307	3.466445
-25.877642	29.070439	3.476442
-25.659793	24.655919	3.486438
-24.731575	27.707924	3.496435
-24.163809	23.942152	3.506432
-23.432663	25.748259	3.516429
-23.068179	26.071955	3.526426
-23.156303	30.527107	3.536422
-22.839151	30.471714	3.546419
-21.835251	27.648531	3.556416
-21.792477	27.974801	3.566413
-20.923207	24.523202	3.576410
-20.456834	30.045061	3.586406
-19.520857	25.997052	3.596403
-19.110725	34.587664	3.606400
-19.181625	22.827866	3.616397
-18.796558	29.201824	3.626394
-18.232484	26.849418	3.636390
-17.049789	28.857643	3.646387
-16.558123	27.796260	3.656384
-16.456380	20.466532	3.666381
-15.798187	22.771823	3.676378
-14.979206	24.044753	3.686374
-14.743115	23.292417	3.696371
-14.844969	26.023312	3.706368
-14.105393	23.054390	3.716365
-13.335796	19.266697	3.726362
-12.489116	23.737854	3.736358
-12.079706	24.361821	3.746355
-12.159254	25.388191	3.756352
-11.531425	26.228400	3.766349
-10.678609	16.941302	3.776346
-10.411056	21.290391	3.786342
-9.656956	8.616563	3.796339
-8.868711	15.200164	3.806336
-8.727875	17.018988	3.816333
-8.854978	16.386555	3.826330
-7.987922	18.336221	3.836326
-7.623007	18.282895	3.846323
-6.530192	19.307289	3.856320
-6.108027	20.622996	3.866317
-6.063388	13.150112	3.876314
-5.540687	19.379098	3.886310
-4.965695	25.305349	3.896307
-4.496860	27.912545	3.906304
-3.780671	40.041342	3.916301
-3.719586	47.096122	3.926298
-3.265647	48.603281	3.936294
-2.651774	66.256657	3.946291
-2.172744	67.794757	3.956288
-1.647278	85.465084	3.966285
-1.055217	91.179631	3.976282
-0.341723	105.719518	3.986278
0.000000	106.019553	3.991283
-0.718641	112.598125	3.996288
-0.316038	123.779256	4.001293
0.532337	119.673768	4.006298
0.211342	121.704359	4.011302
0.232640	123.393764	4.016307
0.170637	127.320193	4.021312
0.238739	123.263426	4.026317
0.264646	127.521008	4.031322
0.469291	115.676191	4.036326
0.484870	127.303550	4.041331
0.150527	124.957710	4.046336
0.619471	128.823619	4.051341
0.474748	138.970039	4.056346
0.695564	142.786002	4.061350
0.411327	126.373034	4.066355
0.638264	135.518815	4.071360
1.204713	130.814995	4.076365
0.590878	131.995865	4.081370
0.463480	126.991964	4.086374
0.638174	117.831432	4.091379
0.367803	124.476252	4.096384
0.585489	116.764312	4.101389
0.699780	130.049880	4.106394
0.707041	137.097555	4.111398
0.516196	131.268323	4.116403
0.760955	142.271567	4.121408
0.719963	132.034163	4.126413
0.522958	136.595365	4.131418
0.968654	132.315295	4.136422
1.155197	136.316920	4.141427
0.423918	130.018192	4.146432
0.460847	119.088475	4.151437
0.912929	132.251851	4.156442
0.897601	142.261072	4.161446
1.111347	131.930223	4.166451
0.661791	128.567803	4.171456
0.915507	117.373387	4.176461
0.733620	128.341813	4.181466
0.908584	131.285413	4.186470
1.113185	122.958593	4.191475
0.655434	124.415709	4.196480
0.709859	127.783025	4.201485
0.874940	132.490324	4.206490
1.239059	141.143363	4.211494
0.808739	133.168487	4.216499
1.240811	141.137086	4.221504
1.161899	127.235736	4.226509
0.945353	135.305319	4.231514
0.521825	127.462262	4.236518
1.093724	139.072611	4.241523
0.945271	140.604955	4.246528
1.142422	143.535611	4.251533
1.185734	133.984250	4.256538
1.001448	127.679449	4.261542
1.072666	125.748178	4.266547
0.920569	134.355040	4.271552
1.087961	122.012997	4.276557
0.978483	142.027725	4.281562
1.132646	144.572780	4.286566
0.822073	142.900262	4.291571
0.962430	148.626952	4.296576
1.525801	155.439358	4.301581
1.562075	150.963608	4.306586
1.137162	133.458926	4.311590
0.971296	123.528862	4.316595
0.530142	146.224240	4.321600
0.997863	143.538390	4.326605
1.203087	142.965611	4.331610
0.998071	147.904540	4.336614
1.476855	144.524124	4.341619
1.090747	146.270635	4.346624
1.340423	140.584778	4.351629
1.569667	142.760649	4.356634
1.428238	148.031353	4.361638
1.624230	146.422329	4.366643
1.440809	151.671099	4.371648
1.448087	152.900794	4.376653
1.429132	151.948479	4.381658
1.674262	152.783646	4.386662
1.267345	146.431246	4.391667
1.400836	145.104028	4.396672
1.840019	142.280257	4.401677
1.063887	133.748634	4.406682
0.987347	128.819069	4.411686
1.282530	144.838363	4.416691
1.078663	148.122515	4.421696
1.334748	139.474468	4.426701
1.343580	146.594667	4.431706
1.248193	140.143145	4.436710
1.808522	146.184087	4.441715
1.011479	146.687985	4.446720
1.446327	144.174927	4.451725
1.838115	146.565930	4.456730
1.550607	152.121963	4.461734
1.224179	151.514905	4.466739
1.335630	155.050513	4.471744
1.555056	135.503015	4.476749
1.585626	154.866383	4.481754
1.399115	145.508982	4.486758
1.498680	150.315070	4.491763
1.784696	163.668836	4.496768
1.512333	152.220958	4.501773
2.026914	158.253207	4.506778
1.927122	164.254568	4.511782
1.862416	160.085596	4.516787
1.493590	154.268250	4.521792
1.743720	142.318260	4.526797
1.860659	150.949679	4.531802
1.677963	151.107996	4.536806
1.349809	156.094571	4.541811
1.710518	150.995684	4.546816
2.003480	156.458178	4.551821
1.584794	156.713348	4.556826
1.399682	159.988254	4.561830
1.764302	162.712511	4.566835
2.010657	176.312901	4.571840
2.396662	168.413384	4.576845
1.738299	158.566309	4.581850
2.004309	156.642670	4.586854
1.731655	146.849439	4.591859
1.681732	150.188715	4.596864
2.103552	155.090159	4.601869
1.893592	154.056854	4.606874
1.710404	154.341794	4.611878
1.899072	158.165928	4.616883
1.836072	174.800986	4.621888
2.220696	172.020505	4.626893
2.148573	175.828301	4.631898
1.745397	165.634614	4.636902
1.996330	172.650691	4.641907
1.997992	188.968818	4.646912
2.153664	172.424042	4.651917
2.242414	174.647101	4.656922
1.773517	163.030504	4.661926
1.831889	161.075920	4.666931
1.786641	172.851980	4.671936
2.097653	160.000344	4.676941
2.187580	171.654119	4.681946
2.173740	164.974763	4.686950
2.590069	164.574754	4.691955
2.278006	165.664350	4.696960
2.342106	164.468154	4.701965
1.984857	156.924804	4.706970
2.015430	175.424513	4.711974
2.232339	164.770458	4.716979
1.816046	177.809651	4.721984
2.076986	174.026560	4.726989
2.215318	172.875753	4.731994
2.306453	172.257463	4.736998
2.585679	171.334649	4.742003
2.177046	173.768023	4.747008
2.258674	164.732686	4.752013
2.645047	180.740977	4.757018
2.200123	174.751979	4.762022
2.072038	176.907561	4.767027
2.392351	177.171054	4.772032
2.021988	166.924802	4.777037
2.226867	168.544500	4.782042
2.089799	172.378226	4.787046
2.442150	167.068669	4.792051
2.170553	179.161542	4.797056
2.361576	167.562415	4.802061
2.696010	168.086294	4.807066
2.306247	176.496068	4.812070
2.509749	172.082860	4.817075
2.267825	171.975159	4.822080
2.163843	167.711063	4.827085
2.544891	181.511942	4.832090
2.733137	177.825588	4.837094
2.482936	170.695824	4.842099
2.381875	179.019523	4.847104
2.458186	169.260530	4.852109
2.464461	171.208535	4.857114
2.539017	175.461718	4.862118
2.457970	169.900108	4.867123
2.404710	176.485835	4.872128
2.591583	174.685244	4.877133
2.281803	173.781372	4.882138
2.290285	176.244713	4.887142
2.992431	187.958199	4.892147
2.741877	188.607959	4.897152
2.700386	181.939229	4.902157
2.788003	172.498005	4.907162
2.271997	179.238036	4.912166
2.784805	179.819562	4.917171
2.708932	185.554621	4.922176
2.614792	181.750886	4.927181
2.754775	194.013799	4.932186
2.694048	188.316146	4.937190
3.071385	184.040380	4.942195
2.771979	181.243015	4.947200
3.067281	173.028597	4.952205
2.745457	170.709275	4.957210
2.436178	174.373666	4.962214
2.821447	174.804211	4.967219
2.673816	182.619484	4.972224
3.036807	193.749880	4.977229
3.094000	184.082439	4.982234
2.517029	180.954977	4.987238
3.098671	179.308051	4.992243
2.856778	188.564819	4.997248
3.002237	178.089556	5.002253
2.729398	180.232875	5.007258
3.052062	183.726113	5.012262
3.108440	178.260160	5.017267
2.926718	175.608984	5.022272
2.752780	163.819916	5.027277
3.125022	181.734938	5.032282
3.107587	183.316487	5.037286
3.266369	171.266807	5.042291
2.702424	179.804941	5.047296
2.999313	176.130145	5.052301
2.883596	179.906766	5.057306
3.093590	182.012874	5.062310
3.186100	184.643463	5.067315
2.826013	188.774501	5.072320
3.363518	183.252618	5.077325
3.080958	187.694280	5.082330
3.017888	189.896687	5.087334
3.047745	181.970360	5.092339
3.196029	189.631998	5.097344
3.318535	185.202923	5.102349
3.018914	184.123467	5.107354
3.216519	195.792130	5.112358
3.458699	185.172093	5.117363
3.021859	182.940277	5.122368
2.630176	178.689336	5.127373
2.596829	188.948155	5.132378
3.016105	198.086167	5.137382
3.064395	190.580899	5.142387
3.330735	194.858008	5.147392
3.083300	190.983228	5.152397
3.555801	193.320543	5.157402
2.963360	187.702512	5.162406
3.459499	190.766955	5.167411
3.522086	190.241693	5.172416
3.359240	191.197329	5.177421
3.504187	186.676177	5.182426
3.088420	191.372691	5.187430
3.377881	202.982766	5.192435
3.181121	199.334206	5.197440
3.480638	189.977037	5.202445
3.460022	199.632781	5.207450
3.267329	193.209046	5.212454
3.173171	190.724564	5.217459
3.244768	198.967606	5.222464
3.555720	199.311649	5.227469
3.602788	197.893482	5.232474
3.209456	194.152146	5.237478
3.571592	192.849436	5.242483
3.854315	205.507738	5.247488
3.546597	203.904370	5.252493
3.382121	200.620934	5.257498
3.339572	198.425801	5.262502
3.602011	194.648800	5.267507
3.965268	211.891388	5.272512
3.682509	192.513763	5.277517
3.769457	192.769299	5.282522
3.377847	196.512950	5.287526
3.401153	186.686272	5.292531
3.538569	186.725148	5.297536
3.902134	204.853511	5.302541
3.920801	198.520249	5.307546
3.168877	195.132129	5.312550
3.793171	196.044302	5.317555
3.832469	214.023850	5.322560
3.652506	211.068681	5.327565
3.904006	209.027077	5.332570
3.567144	209.778859	5.337574
3.867493	200.257043	5.342579
3.705487	218.391321	5.347584
3.392455	208.987148	5.352589
3.728547	216.698648	5.357594
3.697108	215.855838	5.362598
4.201332	210.683971	5.367603
3.706152	210.479662	5.372608
3.828376	212.615258	5.377613
4.167190	208.456213	5.382618
3.946292	213.865857	5.387622
4.444000	216.154958	5.392627
3.655841	208.514166	5.397632
3.429809	188.403230	5.402637
4.140836	204.221794	5.407642
4.002363	210.434832	5.412646
3.843680	202.851055	5.417651
3.794661	206.522386	5.422656
3.917928	205.930730	5.427661
4.096534	204.596484	5.432666
4.097370	213.780672	5.437670
4.213253	211.241339	5.442675
3.998594	218.102141	5.447680
3.866680	206.053407	5.452685
3.985424	215.149637	5.457690
3.851390	216.341228	5.462694
3.923609	216.482001	5.467699
3.746722	217.019055	5.472704
3.779912	213.568802	5.477709
4.034690	223.615106	5.482714
3.548830	214.199875	5.487718
3.754140	220.103132	5.492723
4.047628	219.162277	5.497728
3.996883	215.142975	5.502733
4.244176	219.372437	5.507738
4.050028	211.784687	5.512742
4.384411	219.059867	5.517747
4.116850	220.930293	5.522752
3.994512	212.660662	5.527757
4.277122	224.689423	5.532762
4.395730	231.700817	5.537766
4.510024	229.554026	5.542771
4.027106	226.683988	5.547776
4.154211	230.416486	5.552781
4.660700	240.002838	5.557786
4.493917	228.472035	5.562790
4.603648	217.878928	5.567795
4.210198	220.154923	5.572800
4.067098	210.120029	5.577805
3.947019	219.405302	5.582810
4.217078	226.747446	5.587814
4.368356	230.779893	5.592819
4.211387	245.483983	5.597824
4.272083	238.024219	5.602829
4.408431	236.987609	5.607834
4.280235	238.931249	5.612838
4.724697	240.779401	5.617843
4.241081	235.229831	5.622848
4.541722	242.915225	5.627853
4.542687	242.197080	5.632858
4.042004	251.497336	5.637862
4.623264	241.406590	5.642867
4.282933	244.164690	5.647872
4.572571	239.782345	5.652877
4.723419	242.960667	5.657882
4.198119	251.777549	5.662886
4.739162	236.615353	5.667891
4.379243	241.046926	5.672896
4.351954	243.262751	5.677901
4.323779	238.891924	5.682906
4.191522	240.386954	5.687910
4.498876	238.289194	5.692915
4.376883	258.685644	5.697920
4.720738	263.520165	5.702925
5.110570	262.548488	5.707930
4.903399	258.075815	5.712934
4.539142	257.253185	5.717939
4.450251	249.376953	5.722944
4.791063	256.439180	5.727949
5.212628	255.222124	5.732954
4.491993	250.965435	5.737958
4.524262	240.571032	5.742963
4.781548	247.959465	5.747968
4.866077	255.197633	5.752973
4.992349	260.597529	5.757978
4.726193	257.086309	5.762982
4.727559	245.921612	5.767987
5.106403	258.356183	5.772992
4.974545	260.338359	5.777997
4.688320	242.960669	5.783002
4.489171	244.516732	5.788006
4.942019	255.092187	5.793011
5.019987	259.594790	5.798016
5.311684	262.238669	5.803021
5.038969	245.270151	5.808026
4.868685	252.529009	5.813030
5.001226	236.389563	5.818035
4.988890	241.058077	5.823040
4.955067	246.482895	5.828045
5.243218	238.646039	5.833050
4.665887	237.299776	5.838054
5.029020	237.866644	5.843059
4.745627	251.255349	5.848064
5.131155	250.322308	5.853069
4.988673	242.049472	5.858074
4.682060	248.089390	5.863078
5.112667	257.288942	5.868083
5.175850	253.429060	5.873088
5.429217	259.872166	5.878093
5.374873	254.050114	5.883098
4.925806	243.477557	5.888102
5.190099	236.210716	5.893107
5.263991	241.577634	5.898112
4.892365	256.992183	5.903117
5.254505	248.615467	5.908122
5.209232	261.726665	5.913126
5.382685	250.984414	5.918131
4.999855	246.159451	5.923136
5.199023	256.850333	5.928141
5.239420	253.987395	5.933146
5.381158	259.315282	5.938150
5.281776	253.348386	5.943155
5.525256	255.136085	5.948160
4.847319	246.699848	5.953165
5.082404	252.845248	5.958170
4.825550	257.301906	5.963174
5.554586	261.329825	5.968179
5.421392	264.267644	5.973184
5.719771	263.835378	5.978189
5.408922	257.129465	5.983194
5.221147	258.009894	5.988198
5.509335	262.742353	5.993203
5.174674	265.730522	5.998208
5.420665	267.422920	6.003213
5.491078	251.675940	6.008218
5.354677	272.172722	6.013222
5.411257	259.446048	6.018227
5.298446	263.835990	6.023232
5.430156	262.860210	6.028237
5.323065	267.812398	6.033242
5.541168	268.278464	6.038246
5.303212	265.797378	6.043251
5.437525	264.330822	6.048256
5.555789	263.888636	6.053261
5.486641	267.316346	6.058266
4.943398	262.510027	6.063270
5.342432	260.280934	6.068275
5.237939	264.963803	6.073280
5.522681	269.089372	6.078285
5.637558	261.491451	6.083290
5.454182	267.287566	6.088294
5.574868	260.716939	6.093299
5.223208	254.627973	6.098304
5.011516	252.981177	6.103309
5.367277	262.505590	6.108314
5.449046	266.264136	6.113318
5.527041	264.281176	6.118323
5.334305	270.154678	6.123328
5.557874	263.115624	6.128333
5.749688	263.228287	6.133338
5.310591	256.070952	6.138342
5.057100	250.801916	6.143347
5.033427	249.429560	6.148352
5.472033	267.704488	6.153357
5.438564	258.063777	6.158362
5.611054	271.536538	6.163366
5.746751	257.228357	6.168371
5.336862	254.448183	6.173376
4.945288	243.110553	6.178381
4.990986	240.575816	6.183386
5.064816	261.710556	6.188390
5.363206	264.470449	6.193395
5.407300	254.855628	6.198400
5.303333	266.846532	6.203405
5.632119	264.960563	6.208410
5.377596	271.827593	6.213414
5.310195	262.973593	6.218419
5.399301	269.201837	6.223424
5.052703	266.490899	6.228429
5.282604	253.645496	6.233434
5.619508	252.239145	6.238438
5.379804	257.325870	6.243443
5.346678	273.143301	6.248448
5.480745	264.884344	6.253453
5.931723	259.916901	6.258458
5.496876	263.119980	6.263462
5.721601	272.841968	6.268467
5.724366	268.738394	6.273472
5.740564	284.915143	6.278477
6.021070	285.728991	6.283482
5.651456	281.471425	6.288486
5.670935	273.299906	6.293491
5.809911	280.080362	6.298496
5.678648	280.657770	6.303501
5.632676	248.234125	6.308506
5.045859	230.498296	6.313510
4.713037	223.166244	6.318515
4.645293	232.573086	6.323520
4.876013	244.233462	6.328525
5.081609	237.137107	6.333530
4.860477	249.228497	6.338534
5.081766	249.747849	6.343539
5.424185	265.598550	6.348544
5.438042	271.885966	6.353549
5.385901	263.371269	6.358554
5.361837	271.996228	6.363558
5.526290	265.539005	6.368563
5.308633	264.247469	6.373568
4.983239	266.275598	6.378573
5.372510	274.143355	6.383578
5.186411	276.383910	6.388582
5.504981	268.570778	6.393587
5.776804	271.534122	6.398592
5.300432	265.208310	6.403597
5.739395	261.555668	6.408602
5.183972	263.537356	6.413606
5.590765	254.789860	6.418611
5.308484	244.738652	6.423616
5.154703	247.493016	6.428621
5.406852	256.799446	6.433626
5.591842	262.199691	6.438630
5.422476	248.119345	6.443635
5.156798	257.794295	6.448640
4.809973	265.397013	6.453645
5.367855	264.563684	6.458650
5.406659	271.530572	6.463654
5.689801	261.068624	6.468659
5.509087	260.040250	6.473664
5.300017	264.293322	6.478669
5.517858	259.710184	6.483674
5.439025	258.077502	6.488678
5.443248	256.416070	6.493683
5.138415	246.466446	6.498688
5.039134	259.155790	6.503693
5.501111	264.762842	6.508698
5.712961	267.020529	6.513702
5.563540	261.909289	6.518707
5.231145	250.508658	6.523712
5.311903	250.072312	6.528717
5.627080	249.903181	6.533722
5.254754	255.573690	6.538726
5.236031	247.085435	6.543731
5.299760	253.706758	6.548736
5.416151	258.510255	6.553741
5.396157	266.280382	6.558746
5.728118	268.759809	6.563750
5.482451	257.269742	6.568755
5.705436	259.329545	6.573760
5.286110	258.920441	6.578765
5.546629	257.703149	6.583770
5.260379	252.803037	6.588774
5.585316	247.257285	6.593779
5.521045	252.503352	6.598784
5.422659	251.402050	6.603789
5.160973	245.808432	6.608794
5.285367	252.606967	6.613798
5.107079	249.512329	6.618803
5.415846	254.877482	6.623808
4.997037	242.506405	6.628813
4.828936	257.398896	6.633818
5.331319	275.629101	6.638822
5.710028	281.261777	6.643827
5.812658	275.013489	6.648832
5.541277	270.807069	6.653837
5.341812	258.847909	6.658842
5.312759	258.378040	6.663846
5.446629	249.223797	6.668851
5.396232	246.438271	6.673856
5.041953	255.446822	6.678861
5.290865	253.440416	6.683866
5.034959	269.716464	6.688870
5.512603	272.704708	6.693875
5.425607	275.398059	6.698880
5.353018	281.850796	6.703885
5.539220	261.254823	6.708890
5.251939	274.704261	6.713894
5.275886	271.097251	6.718899
5.652266	273.028772	6.723904
5.169653	276.830901	6.728909
5.563128	265.573504	6.733914
5.388837	275.060231	6.738918
5.645328	262.824438	6.743923
5.231167	264.730348	6.748928
5.184953	249.077457	6.753933
5.716431	268.480016	6.758938
5.455886	269.817855	6.763942
5.186654	259.384964	6.768947
4.867422	257.660000	6.773952
5.183882	269.923962	6.778957
5.611067	276.539324	6.783962
5.551997	275.884307	6.788966
5.500655	271.773339	6.793971
5.382167	262.873511	6.798976
5.576515	263.058543	6.803981
5.554279	254.311409	6.808986
5.459950	256.882515	6.813990
5.429367	248.326504	6.818995
4.910156	246.461838	6.824000
4.757704	257.058773	6.829005
5.832889	267.192498	6.834010
5.224974	279.435876	6.839014
5.262376	271.850013	6.844019
5.416383	278.140920	6.849024
5.260090	280.345198	6.854029
5.311290	280.093784	6.859034
5.440515	290.517171	6.864038
5.642746	282.437413	6.869043
5.731193	282.911012	6.874048
5.294013	268.492705	6.879053
5.475725	257.091117	6.884058
5.238531	259.516792	6.889062
5.173304	265.389422	6.894067
5.618498	278.633072	6.899072
5.489914	271.493823	6.904077
5.326424	260.234564	6.909082
5.254313	267.873604	6.914086
5.147561	270.218860	6.919091
5.643211	278.342134	6.924096
5.326112	285.851649	6.929101
5.497879	276.552289	6.934106
5.488778	270.894027	6.939110
5.422968	261.217222	6.944115
5.089657	251.433377	6.949120
5.405074	276.070684	6.954125
5.385603	272.293267	6.959130
5.488798	283.343950	6.964134
5.434902	271.697468	6.969139
5.280615	264.533751	6.974144
5.196197	262.069888	6.979149
5.407982	268.313832	6.984154
5.447704	278.159537	6.989158
5.635150	270.933120	6.994163
5.782178	263.323864	6.999168
5.349895	260.755979	7.004173
5.212329	257.439869	7.009178
5.354385	259.559728	7.014182
5.465244	253.781556	7.019187
5.575701	264.024356	7.024192
4.953913	260.514724	7.029197
5.239807	251.833508	7.034202
5.025069	255.635053	7.039206
5.302152	262.219997	7.044211
5.555630	272.083037	7.049216
5.589432	274.267208	7.054221
5.485767	261.650902	7.059226
5.209574	258.283611	7.064230
5.091128	253.800288	7.069235
5.383391	272.670633	7.074240
5.348250	277.731841	7.079245
5.680468	278.411090	7.084250
5.224918	269.658648	7.089254
5.349510	277.134191	7.094259
5.780862	275.200615	7.099264
5.085572	266.754415	7.104269
5.520760	261.435098	7.109274
5.322250	255.926551	7.114278
5.228784	250.771801	7.119283
5.684049	259.730240	7.124288
5.290806	259.446785	7.129293
5.300776	256.148833	7.134298
5.021651	255.645135	7.139302
5.519724	264.922771	7.144307
5.825300	270.025839	7.149312
5.368610	258.410443	7.154317
5.203467	255.171392	7.159322
5.330559	254.645575	7.164326
5.360333	256.314691	7.169331
5.721141	263.032129	7.174336
5.219003	254.878558	7.179341
5.081226	254.555329	7.184346
5.351747	259.262064	7.189350
5.583401	263.699611	7.194355
5.310760	264.798893	7.199360
5.137695	257.688722	7.204365
5.641447	260.536861	7.209370
5.492432	265.331064	7.214374
5.198207	251.308120	7.219379
5.529951	261.506973	7.224384
5.167288	266.495789	7.229389
5.348768	266.701807	7.234394
5.531052	279.872499	7.239398
5.094879	275.014706	7.244403
5.294125	276.331577	7.249408
4.913647	276.235956	7.254413
5.793933	283.995631	7.259418
5.671249	281.559870	7.264422
5.741875	281.672419	7.269427
5.449262	269.354439	7.274432
4.985375	263.349381	7.279437
5.314635	262.871179	7.284442
5.269596	275.941223	7.289446
5.249981	266.880469	7.294451
5.345423	277.150924	7.299456
5.097720	287.522266	7.304461
5.700600	282.629241	7.309466
5.140471	285.450041	7.314470
5.442927	279.863488	7.319475
5.886400	280.689927	7.324480
5.426768	275.174574	7.329485
5.556606	261.012832	7.334490
5.035457	264.953833	7.339494
4.925587	263.677153	7.344499
5.453206	268.293242	7.349504
5.618403	275.778281	7.354509
5.642148	273.003353	7.359514
5.147674	273.953680	7.364518
5.213708	268.248920	7.369523
5.570673	278.364764	7.374528
5.058293	275.910585	7.379533
5.406992	275.986166	7.384538
5.420553	275.579264	7.389542
5.573268	283.382618	7.394547
5.516662	267.297902	7.399552
5.389836	269.931017	7.404557
5.523945	268.657477	7.409562
5.329562	266.466993	7.414566
5.224453	276.025206	7.419571
5.252203	274.027922	7.424576
5.732229	276.968341	7.429581
5.351772	261.826214	7.434586
5.605775	256.066881	7.439590
5.168173	259.210279	7.444595
4.888765	257.558207	7.449600
5.073960	274.977274	7.454605
5.697977	277.098024	7.459610
5.860908	279.255764	7.464614
5.251880	271.868622	7.469619
5.407522	270.604384	7.474624
5.124111	275.457479	7.479629
5.348403	274.258481	7.484634
5.651294	283.016033	7.489638
5.511962	271.015866	7.494643
5.452444	256.469167	7.499648
5.248179	262.682975	7.504653
5.116982	250.700537	7.509658
5.305906	265.376099	7.514662
5.484725	269.189136	7.519667
5.612551	272.981640	7.524672
5.292457	272.338791	7.529677
5.306360	268.461269	7.534682
5.253532	266.463877	7.539686
5.289491	280.622277	7.544691
5.562382	271.588743	7.549696
5.701987	268.966616	7.554701
5.350786	254.031907	7.559706
5.496618	259.099734	7.564710
5.206232	260.116359	7.569715
5.355030	248.966669	7.574720
5.119764	257.393555	7.579725
5.490410	259.006435	7.584730
5.707641	271.073880	7.589734
5.175826	256.271692	7.594739
4.999916	264.281224	7.599744
5.076711	268.771357	7.604749
5.871337	268.910384	7.609754
5.781858	272.069183	7.614758
5.121156	252.307420	7.619763
5.280236	254.237971	7.624768
5.405953	273.820767	7.629773
5.598503	267.530009	7.634778
5.353973	267.055725	7.639782
5.355251	247.924874	7.644787
5.357802	250.034816	7.649792
5.181734	254.931303	7.654797
5.483559	270.750364	7.659802
5.003465	266.086068	7.664806
5.379701	274.518992	7.669811
5.477964	272.289271	7.674816
5.269363	271.534152	7.679821
5.781151	277.810482	7.684826
5.751092	275.708305	7.689830
5.419766	264.098696	7.694835
5.390937	257.820263	7.699840
4.954693	250.105678	7.704845
5.139636	253.670991	7.709850
5.540900	268.196439	7.714854
5.662886	262.881593	7.719859
5.458196	251.087764	7.724864
5.255261	266.643732	7.729869
5.146165	256.745883	7.734874
5.291707	261.108254	7.739878
5.504712	279.269625	7.744883
5.281791	263.650561	7.749888
4.987086	275.019448	7.754893
5.554118	272.814816	7.759898
5.613586	279.171062	7.764902
5.263373	279.618048	7.769907
5.683929	265.847628	7.774912
5.449008	264.368959	7.779917
5.452029	249.894784	7.784922
5.156599	253.500089	7.789926
5.262412	264.243474	7.794931
5.527854	265.179886	7.799936
5.556601	258.186986	7.804941
5.747389	257.562669	7.809946
5.391547	261.768991	7.814950
5.192253	265.112563	7.819955
5.341460	254.646162	7.824960
5.273609	256.121674	7.829965
5.268533	253.772007	7.834970
5.660626	276.565602	7.839974
5.483767	257.971830	7.844979
5.276630	259.858162	7.849984
4.841875	255.379795	7.854989
5.312248	260.694479	7.859994
5.462927	268.498144	7.864998
5.613021	273.185669	7.870003
5.528789	254.707190	7.875008
5.173919	258.897541	7.880013
5.676672	255.598792	7.885018
5.463354	258.919237	7.890022
5.279328	255.515450	7.895027
5.547894	255.774347	7.900032
5.511062	263.360436	7.905037
5.658256	253.919384	7.910042
5.646927	264.288711	7.915046
5.295275	262.470720	7.920051
5.655558	259.308046	7.925056
5.076847	260.935862	7.930061
5.534954	258.210364	7.935066
5.370796	264.145852	7.940070
5.399743	260.180569	7.945075
5.489453	264.557961	7.950080
5.695804	264.310863	7.955085
5.072650	257.745322	7.960090
5.126913	256.082427	7.965094
5.486664	266.197830	7.970099
5.280919	258.229059	7.975104
5.447685	260.860753	7.980109
5.798844	258.803626	7.985114
5.281550	265.319268	7.990118
5.345821	256.346156	7.995136
5.629959	262.364017	8.000154
5.288658	265.380443	8.005171
5.392850	258.074907	8.010189
5.368473	268.505023	8.015206
5.337761	267.449678	8.020224
5.798294	267.599030	8.025242
5.352463	264.639213	8.030259
5.486054	258.174805	8.035277
5.663551	255.812176	8.040294
5.604048	259.327491	8.045312
5.738280	255.428501	8.050330
5.116936	253.152381	8.055347
5.335994	257.870793	8.060365
5.524333	257.551314	8.065382
5.496115	261.768617	8.070400
5.617658	261.869768	8.075418
5.523968	260.871564	8.080435
5.500714	262.642491	8.085453
5.066039	262.808154	8.090470
5.168872	264.846612	8.095488
5.516520	254.353867	8.100506
5.167564	270.757610	8.105523
5.247373	260.063581	8.110541
5.273779	255.496611	8.115558
5.331778	263.840658	8.120576
5.595056	261.344758	8.125594
5.459880	264.657275	8.130611
5.693225	261.749494	8.135629
5.400662	256.424348	8.140646
5.406424	263.861400	8.145664
5.535735	253.771857	8.150682
5.561738	263.692383	8.155699
5.661443	263.651776	8.160717
5.753643	266.651196	8.165734
5.458582	269.316461	8.170752
5.563664	267.712986	8.175770
5.546340	269.808019	8.180787
5.452616	263.104463	8.185805
5.363416	261.461814	8.190822
5.538897	263.769810	8.195840
5.380673	263.160328	8.200858
5.458643	273.028589	8.205875
5.233718	262.391471	8.210893
5.433291	272.947658	8.215910
5.858577	280.107972	8.220928
5.735775	271.067471	8.225946
5.572155	268.208872	8.230963
5.668861	271.387462	8.235981
5.651494	265.445144	8.240998
5.214094	267.854875	8.246016
6.024842	280.871959	8.251034
6.103321	283.311819	8.256051
5.655676	269.228724	8.261069
5.492658	265.808333	8.266086
5.252972	260.323483	8.271104
5.768912	267.223539	8.276122
5.845608	272.588933	8.281139
5.289148	261.315510	8.286157
5.909337	270.477692	8.291174
5.540904	284.366297	8.296192
5.839535	276.361489	8.301210
5.735060	282.395684	8.306227
5.771751	281.626473	8.311245
5.595775	270.562032	8.316262
5.635495	278.912088	8.321280
5.956222	270.534635	8.326298
5.621226	268.422200	8.331315
6.038427	275.934045	8.336333
5.955935	270.064977	8.341350
5.482240	269.608747	8.346368
5.296974	261.521506	8.351386
5.367939	281.981116	8.356403
5.968735	282.263254	8.361421
5.978449	281.583445	8.366438
5.900857	292.419468	8.371456
5.817834	288.254512	8.376474
6.097279	285.491020	8.381491
5.820982	278.841129	8.386509
5.711428	268.956016	8.391526
5.458465	268.651601	8.396544
5.421411	268.310413	8.401562
5.977990	278.792085	8.406579
5.908982	281.226507	8.411597
5.953819	287.464661	8.416614
5.804513	289.110058	8.421632
5.953883	287.638533	8.426650
6.271973	284.963692	8.431667
5.866434	276.017700	8.436685
5.883380	265.147273	8.441702
5.606773	268.096825	8.446720
5.721291	264.295572	8.451738
5.558447	273.137884	8.456755
5.797059	284.278099	8.461773
6.008241	280.168319	8.466790
6.231912	290.196931	8.471808
6.050843	273.500497	8.476826
5.760608	266.511974	8.481843
5.634393	264.297609	8.486861
5.838725	276.452955	8.491878
6.184034	284.960550	8.496896
6.341704	288.265343	8.501914
6.016213	276.760301	8.506931
5.467628	271.967288	8.511949
5.655942	268.703621	8.516966
5.870888	280.365040	8.521984
5.852358	291.497962	8.527002
6.012614	293.050983	8.532019
6.126901	293.986349	8.537037
5.888489	289.586825	8.542054
5.794287	288.755947	8.547072
5.952020	287.444057	8.552090
5.753428	276.083349	8.557107
5.639421	290.279464	8.562125
6.009283	280.676286	8.567143
6.012740	286.097266	8.572160
6.033378	287.081923	8.577178
6.098874	292.401732	8.582195
5.710061	286.558263	8.587213
5.857521	283.348288	8.592231
5.760532	290.870773	8.597248
5.965993	288.582676	8.602266
5.869099	286.938067	8.607283
5.815116	288.391908	8.612301
6.091524	288.279610	8.617319
5.824136	289.463738	8.622336
5.914555	293.460617	8.627354
6.284882	282.500448	8.632371
6.304639	290.377119	8.637389
6.104343	279.215479	8.642407
6.479829	292.565412	8.647424
5.832322	291.312627	8.652442
6.130481	286.816939	8.657459
5.876811	286.427432	8.662477
6.118521	289.021748	8.667495
5.921512	295.868727	8.672512
5.677575	297.175429	8.677530
6.034536	290.288091	8.682547
6.382106	303.254237	8.687565
6.074123	297.773698	8.692583
6.165268	292.836897	8.697600
5.950483	287.995064	8.702618
6.006766	292.076148	8.707635
6.045949	304.919907	8.712653
6.331779	314.396087	8.717671
6.423632	306.761112	8.722688
6.512397	300.171132	8.727706
6.369470	291.837458	8.732723
6.079770	291.257912	8.737741
6.163851	280.784099	8.742759
6.058008	284.852556	8.747776
6.470705	286.839616	8.752794
6.528104	285.909399	8.757811
5.838032	289.627033	8.762829
6.041700	290.712575	8.767847
6.122908	290.472887	8.772864
6.223809	291.246244	8.777882
5.939608	289.504573	8.782899
5.669219	288.994600	8.787917
6.048166	300.551607	8.792935
6.096395	307.275206	8.797952
6.363323	307.527280	8.802970
6.327834	305.980400	8.807987
6.171849	315.638972	8.813005
6.512307	307.772797	8.818023
6.113049	310.204996	8.823040
6.294465	311.546453	8.828058
6.350678	314.059207	8.833075
6.315084	312.506031	8.838093
6.494053	313.399771	8.843111
6.233075	323.352389	8.848128
5.966621	319.032960	8.853146
6.432959	318.903713	8.858163
6.334343	321.128168	8.863181
6.021708	314.692193	8.868199
6.200738	320.164737	8.873216
6.231555	314.259079	8.878234
6.401802	307.372404	8.883251
6.307337	320.319028	8.888269
6.379527	312.466218	8.893287
6.389740	314.635860	8.898304
6.397839	319.750032	8.903322
6.406126	312.519363	8.908339
6.472393	304.326671	8.913357
6.835344	313.677241	8.918375
6.765963	310.444222	8.923392
6.372236	315.280147	8.928410
6.621284	311.748255	8.933427
6.494021	309.493025	8.938445
6.302337	307.184713	8.943463
6.144289	306.647781	8.948480
6.340341	318.050249	8.953498
6.555721	312.813249	8.958515
6.355651	316.161124	8.963533
6.119967	317.848373	8.968551
6.479233	317.896734	8.973568
6.330196	312.375665	8.978586
6.940676	315.739343	8.983603
6.468007	319.852299	8.988621
6.564479	306.400786	8.993639
6.359259	311.071668	8.998656
6.350218	313.913301	9.003674
6.428436	310.676234	9.008691
6.422975	320.680581	9.013709
6.407214	315.375433	9.018727
6.472325	316.548817	9.023744
6.467200	312.841915	9.028762
6.577061	314.506921	9.033779
6.128552	319.038969	9.038797
6.530184	312.801037	9.043815
6.519406	306.078240	9.048832
6.269701	314.217770	9.053850
6.514911	312.592473	9.058867
6.568479	321.035062	9.063885
6.448433	315.673570	9.068903
6.423299	321.417730	9.073920
6.432736	325.140063	9.078938
6.629389	319.735573	9.083955
6.706650	332.519777	9.088973
6.855690	329.786048	9.093991
6.733399	320.578194	9.099008
6.346915	322.471949	9.104026
6.280706	314.176810	9.109043
6.388807	321.926138	9.114061
6.663842	324.777188	9.119079
6.835246	335.669138	9.124096
6.727183	338.191695	9.129114
7.035219	330.617719	9.134131
6.165056	329.636270	9.139149
6.591278	327.872342	9.144167
7.005875	332.686554	9.149184
6.872698	339.479433	9.154202
6.585215	325.273533	9.159219
6.674048	336.077359	9.164237
6.864059	330.490873	9.169255
6.703722	320.850310	9.174272
6.426058	316.078216	9.179290
6.750492	325.084515	9.184307
6.867541	332.680984	9.189325
6.764095	339.434521	9.194343
6.868945	322.478942	9.199360
6.798172	322.884576	9.204378
6.681313	313.073155	9.209395
6.589105	321.292302	9.214413
6.583113	334.281963	9.219431
6.960700	335.738037	9.224448
6.503690	340.811028	9.229466
6.868077	330.189407	9.234483
6.873074	346.209925	9.239501
6.783878	332.588495	9.244519
6.753390	333.435957	9.249536
6.622447	335.334105	9.254554
6.708458	342.162282	9.259571
6.835321	348.725338	9.264589
6.866959	339.039097	9.269607
6.983316	339.683825	9.274624
6.659077	338.712045	9.279642
7.038397	329.646981	9.284659
6.887756	337.808965	9.289677
6.605653	345.120467	9.294695
6.865581	334.152210	9.299712
6.784530	340.791814	9.304730
6.868658	335.780359	9.309747
6.692437	338.884697	9.314765
6.694363	341.383818	9.319783
6.682838	338.078673	9.324800
6.514171	345.097973	9.329818
6.587010	339.580218	9.334835
6.621230	335.204504	9.339853
6.600404	356.700915	9.344871
7.118330	351.511467	9.349888
6.722853	361.557627	9.354906
7.216825	359.174111	9.359923
7.492449	355.931546	9.364941
6.871286	345.589588	9.369959
6.761826	335.944251	9.374976
6.993251	342.863390	9.379994
6.944319	338.491155	9.385011
6.708258	337.937967	9.390029
6.980068	354.292471	9.395047
7.419000	354.044421	9.400064
6.721673	342.341623	9.405082
6.710309	342.135283	9.410099
6.992438	356.235061	9.415117
7.192633	362.770927	9.420135
7.374186	358.498494	9.425152
6.917631	351.971310	9.430170
6.953595	348.381074	9.435187
7.250693	358.407758	9.440205
6.995697	352.546588	9.445223
7.135168	350.783125	9.450240
6.747107	347.918435	9.455258
7.273935	347.798704	9.460275
7.185211	351.186050	9.465293
6.948587	357.316581	9.470311
7.025423	349.576634	9.475328
7.329439	359.662199	9.480346
7.261915	353.355296	9.485363
7.124880	347.343224	9.490381
6.943045	344.146641	9.495399
7.129987	352.394919	9.500416
7.377351	354.369861	9.505434
7.035725	350.122085	9.510451
6.960849	354.886287	9.515469
7.040874	366.205872	9.520487
7.079501	352.801197	9.525504
7.073710	357.908075	9.530522
7.173275	360.499288	9.535539
7.193021	360.490064	9.540557
7.374429	369.117888	9.545575
7.228179	360.159883	9.550592
7.321147	363.121333	9.555610
7.056567	361.464957	9.560627
7.154369	359.032675	9.565645
7.130527	359.841236	9.570663
7.604965	359.975801	9.575680
7.098101	362.150220	9.580698
7.282169	355.838856	9.585715
7.290334	355.478004	9.590733
7.091683	364.966530	9.595751
7.387588	354.721611	9.600768
7.247138	363.446879	9.605786
7.092767	357.907692	9.610803
7.507804	361.629995	9.615821
7.324668	365.095156	9.620839
7.562896	363.754949	9.625856
7.331513	371.800139	9.630874
7.264090	362.299713	9.635891
7.270161	365.912131	9.640909
7.098841	367.122330	9.645927
7.343288	359.757048	9.650944
7.123624	362.319074	9.655962
7.272460	364.056906	9.660979
7.291681	361.248716	9.665997
7.043643	357.074725	9.671015
7.195557	357.357330	9.676032
7.266260	370.006890	9.681050
7.194447	362.659291	9.686067
7.385476	365.296222	9.691085
7.229120	368.214445	9.696103
7.287711	362.765169	9.701120
7.396908	359.987149	9.706138
7.269962	367.997143	9.711155
7.584127	371.252341	9.716173
7.174130	370.789346	9.721191
7.438244	374.749733	9.726208
7.435286	377.823945	9.731226
7.545738	374.247351	9.736243
7.557753	371.957806	9.741261
7.517555	368.070171	9.746279
7.477030	362.273430	9.751296
7.509912	366.130969	9.756314
7.371621	360.706036	9.761331
7.651138	359.084861	9.766349
7.192844	363.943474	9.771367
7.899831	366.891371	9.776384
7.586473	370.660816	9.781402
7.528114	355.213765	9.786419
7.691340	357.883424	9.791437
7.488162	361.888163	9.796455
7.420222	362.186065	9.801472
7.405298	366.533859	9.806490
7.267271	358.656958	9.811507
7.844500	361.836484	9.816525
7.612996	376.536929	9.821543
7.973562	363.514444	9.826560
7.546203	362.079062	9.831578
7.786770	359.693976	9.836595
7.573117	361.563981	9.841613
7.655151	367.796372	9.846631
7.656513	358.383063	9.851648
7.271941	352.172858	9.856666
7.326106	364.339022	9.861683
7.634116	361.305997	9.866701
7.670960	379.255990	9.871719
7.640648	378.897973	9.876736
7.871526	381.784308	9.881754
7.770356	386.978624	9.886771
7.741616	373.215213	9.891789
7.634837	368.893000	9.896807
7.878786	365.516517	9.901824
7.416839	367.418871	9.906842
7.253574	373.253978	9.911859
7.734014	377.202773	9.916877
7.926165	398.120149	9.921895
7.676434	387.925453	9.926912
7.685702	387.495004	9.931930
7.815488	386.932189	9.936947
8.032854	382.641551	9.941965
7.836722	387.304727	9.946983
7.818399	386.051797	9.952000
7.930838	384.059022	9.957018
7.959589	385.064512	9.962035
7.487666	363.739778	9.967053
7.621373	380.557597	9.972071
7.828682	375.646866	9.977088
7.830807	383.946023	9.982106
7.672735	388.798923	9.987123
7.884273	381.628095	9.992141
7.802870	388.330884	9.997159
7.883413	382.796138	10.002176
7.979124	383.264210	10.007194
7.545633	383.189861	10.012211
8.073948	380.741037	10.017229
7.851290	387.794006	10.022247
7.936036	381.763170	10.027264
7.875946	390.939818	10.032282
7.927174	390.597505	10.037299
8.169126	388.436251	10.042317
7.824175	388.912975	10.047335
7.917998	385.888049	10.052352
8.190396	386.962896	10.057370
8.128901	377.789725	10.062387
8.019682	375.354962	10.067405
7.971351	380.679897	10.072423
7.749255	366.517429	10.077440
7.663974	369.645481	10.082458
7.853640	380.140161	10.087475
7.856400	381.398992	10.092493
7.849087	386.342022	10.097511
7.951882	387.818796	10.102528
7.882221	379.372693	10.107546
7.422429	391.502137	10.112563
8.063002	383.636536	10.117581
7.633942	392.441465	10.122599
7.617611	382.929918	10.127616
7.873448	378.223059	10.132634
7.853288	403.089643	10.137651
8.415341	402.636240	10.142669
8.068938	394.473046	10.147687
7.830110	392.825281	10.152704
8.428233	395.689151	10.157722
7.884521	393.748046	10.162739
7.994825	387.261973	10.167757
7.956966	395.797723	10.172775
8.221114	405.674938	10.177792
8.322256	404.901998	10.182810
8.401563	401.197711	10.187827
8.173169	393.003522	10.192845
8.036307	388.354645	10.197863
7.859738	385.526445	10.202880
8.348422	395.860975	10.207898
8.232565	393.449332	10.212915
7.932074	387.942353	10.217933
8.266297	405.805049	10.222951
8.174031	400.887308	10.227968
8.320564	401.672499	10.232986
8.147481	410.254555	10.238003
8.169673	405.779716	10.243021
8.393700	417.452434	10.248039
8.167498	404.019530	10.253056
8.269257	396.881565	10.258074
8.096728	409.057809	10.263091
8.291987	408.368041	10.268109
8.096777	412.040208	10.273127
8.098127	405.858255	10.278144
8.480883	408.522142	10.283162
8.232001	412.019638	10.288179
8.575212	414.257360	10.293197
8.263651	413.147909	10.298215
8.463336	405.530815	10.303232
8.519139	412.710843	10.308250
8.307553	406.811339	10.313267
8.248769	383.023969	10.318285
8.355131	381.215168	10.323303
8.368077	395.659830	10.328320
8.331092	393.684008	10.333338
8.558256	412.977107	10.338355
8.428052	393.514608	10.343373
8.223696	396.026921	10.348391
8.090785	389.032789	10.353408
8.632226	402.445324	10.358426
8.370038	409.895755	10.363443
8.500871	405.741655	10.368461
8.492139	407.967904	10.373479
8.391606	400.558492	10.378496
8.565723	395.340515	10.383514
8.538167	396.522021	10.388531
8.284868	390.256652	10.393549
8.615399	387.715551	10.398567
8.326153	390.070675	10.403584
8.536778	390.072755	10.408602
8.471220	408.262772	10.413619
8.431619	405.959169	10.418637
8.754490	410.188112	10.423655
8.289726	403.614853	10.428672
8.628973	395.824562	10.433690
8.458224	408.931444	10.438707
8.042219	412.145707	10.443725
8.562219	402.601135	10.448743
8.299936	408.959729	10.453760
8.644889	404.292633	10.458778
8.711448	411.979044	10.463795
8.778049	409.318096	10.468813
8.654565	417.456954	10.473831
8.387569	410.370087	10.478848
8.945462	410.330721	10.483866
8.771516	409.521720	10.488883
8.602203	419.542167	10.493901
8.678515	414.560307	10.498919
8.624790	412.505043	10.503936
8.744641	413.430081	10.508954
8.376971	404.405548	10.513971
8.852986	408.661137	10.518989
8.760199	398.584002	10.524007
8.149101	412.352707	10.529024
8.956811	411.586515	10.534042
8.419058	414.185451	10.539059
8.634870	407.446270	10.544077
8.580960	405.760245	10.549095
8.311774	412.457569	10.554112
8.715309	408.194740	10.559130
8.781195	413.804844	10.564147
8.405993	412.364492	10.569165
8.691439	412.566351	10.574183
8.692200	422.096440	10.579200
8.677139	418.596181	10.584218
8.295990	415.370660	10.589235
8.447606	416.464313	10.594253
8.748914	417.648264	10.599271
9.086009	429.341253	10.604288
8.906016	417.327496	10.609306
8.292444	415.308907	10.614323
8.845863	429.988167	10.619341
8.971212	430.391669	10.624359
8.778093	434.584197	10.629376
9.003602	436.026090	10.634394
8.859600	444.158688	10.639411
9.172671	439.774245	10.644429
9.227663	421.428381	10.649447
8.984155	420.589187	10.654464
8.788740	415.264646	10.659482
9.010397	412.866719	10.664499
8.809108	417.581196	10.669517
8.907561	408.077009	10.674535
8.596841	418.110004	10.679552
9.027494	425.449413	10.684570
8.883634	436.078102	10.689587
9.128070	427.882858	10.694605
9.198531	426.694993	10.699623
8.736361	422.412322	10.704640
9.245890	404.529011	10.709658
8.883380	418.315818	10.714675
8.587512	419.166734	10.719693
9.230270	421.686006	10.724711
9.138120	427.008310	10.729728
9.049756	418.773373	10.734746
8.950905	416.977586	10.739763
8.667467	424.390308	10.744781
9.161317	431.237066	10.749799
9.196956	438.559092	10.754816
9.127899	427.193898	10.759834
8.788305	426.786209	10.764851
9.119734	435.062520	10.769869
9.362254	432.408890	10.774887
8.785683	430.346671	10.779904
9.168055	428.438090	10.784922
9.409193	435.816477	10.789939
9.113861	432.599681	10.794957
9.330075	420.997581	10.799975
8.951191	425.635575	10.804992
9.327650	419.950608	10.810010
9.316684	418.734398	10.815027
8.902212	420.162330	10.820045
9.399858	426.046023	10.825063
8.968984	420.303727	10.830080
9.453985	418.773624	10.835098
9.103062	417.294780	10.840115
9.027854	433.835923	10.845133
9.190751	424.340627	10.850151
9.142854	437.346355	10.855168
9.188490	428.737117	10.860186
9.299648	429.732934	10.865203
9.310938	436.162547	10.870221
9.594367	430.567796	10.875239
9.174258	443.483165	10.880256
9.442929	435.340946	10.885274
9.114906	437.654779	10.890291
9.032503	440.369005	10.895309
9.134546	441.640784	10.900327
9.141702	446.076673	10.905344
9.365268	431.740629	10.910362
9.160002	432.224008	10.915379
9.187098	442.523140	10.920397
9.284901	437.099293	10.925415
9.377438	439.641122	10.930432
9.472698	442.722143	10.935450
9.323179	441.155137	10.940467
9.297033	441.014210	10.945485
9.770702	437.138067	10.950503
9.642933	448.288095	10.955520
9.597074	445.035610	10.960538
9.776969	446.434116	10.965555
9.433835	433.650525	10.970573
9.626819	446.918542	10.975591
9.248236	444.115474	10.980608
9.621853	437.487404	10.985626
9.589147	441.702293	10.990643
9.286226	440.197039	10.995661
9.387500	443.860919	11.000679
9.679880	438.106990	11.005696
9.402688	435.376495	11.010714
9.317926	437.680854	11.015731
9.291819	447.294030	11.020749
9.431098	437.152341	11.025767
9.504080	437.977386	11.030784
9.199936	441.483493	11.035802
9.365020	435.522177	11.040819
9.353066	447.610334	11.045837
9.427954	434.790058	11.050855
9.277277	442.377768	11.055872
9.623799	449.540947	11.060890
10.000859	447.144065	11.065907
9.561178	454.098312	11.070925
9.577992	441.782511	11.075943
9.488577	445.056379	11.080960
9.533236	430.489428	11.085978
9.678542	447.838809	11.090995
9.614539	462.705741	11.096013
9.773550	459.484469	11.101031
9.829685	464.506000	11.106048
9.897988	443.693477	11.111066
9.624209	435.632561	11.116083
9.266603	439.825454	11.121101
9.571876	451.463455	11.126119
9.841725	457.426806	11.131136
9.979927	452.432144	11.136154
9.857752	451.324760	11.141171
9.742473	456.732722	11.146189
9.977551	453.575344	11.151207
10.100745	449.526559	11.156224
9.672091	442.761480	11.161242
9.474141	445.500008	11.166259
9.823285	444.852547	11.171277
10.073588	449.935357	11.176295
9.910207	446.164709	11.181312
9.453882	440.237031	11.186330
9.988968	458.027482	11.191347
9.740282	460.060735	11.196365
10.110020	461.193011	11.201383
10.287463	445.264221	11.206400
10.044766	438.738421	11.211418
9.905643	430.271552	11.216435
9.702412	442.929102	11.221453
9.579334	428.025369	11.226471
9.874580	447.535112	11.231488
9.446669	456.598657	11.236506
9.947483	458.288009	11.241523
9.944131	469.204094	11.246541
10.078660	457.447439	11.251559
9.779271	467.686971	11.256576
10.094491	462.639500	11.261594
10.174072	461.809957	11.266611
9.854670	463.765862	11.271629
9.954808	455.596228	11.276647
10.268400	463.209487	11.281664
10.052121	464.556074	11.286682
10.151060	458.141168	11.291699
10.140539	459.241135	11.296717
10.127188	458.520731	11.301735
9.905317	464.636379	11.306752
9.916616	460.144288	11.311770
9.575325	456.287735	11.316787
9.677655	469.598284	11.321805
10.108406	453.017852	11.326823
9.887197	456.955995	11.331840
9.918412	458.163066	11.336858
10.080736	466.913824	11.341875
9.813752	461.723482	11.346893
10.016837	466.119404	11.351911
10.297032	485.164495	11.356928
10.358153	488.336042	11.361946
10.571502	466.219713	11.366963
10.067930	468.422033	11.371981
10.315117	460.071720	11.376999
10.452110	466.260876	11.382016
10.440654	463.246017	11.387034
10.143887	460.972980	11.392051
10.157220	471.223782	11.397069
10.347201	462.068215	11.402087
10.469440	460.572500	11.407104
10.125369	466.120222	11.412122
10.466935	460.112487	11.417139
10.004096	467.849791	11.422157
10.215677	460.811462	11.427175
10.112801	456.804185	11.432192
9.824344	464.205083	11.437210
10.777682	467.610078	11.442227
10.670046	473.976173	11.447245
10.140909	458.693845	11.452263
10.190868	455.972368	11.457280
10.100777	462.092743	11.462298
10.485548	468.429505	11.467315
10.602824	487.332714	11.472333
10.541730	477.569322	11.477351
10.352326	464.708127	11.482368
10.297112	458.575986	11.487386
10.399251	466.711295	11.492403
10.410538	477.419989	11.497421
10.450702	479.540808	11.502439
10.559201	479.445186	11.507456
10.560314	484.850812	11.512474
10.496974	476.372122	11.517491
10.387155	481.334294	11.522509
10.388760	480.627339	11.527527
10.629600	474.496432	11.532544
10.555401	485.171106	11.537562
10.826444	472.503291	11.542579
10.491458	484.035882	11.547597
10.472406	478.043264	11.552615
10.716406	479.274009	11.557632
10.490994	485.844629	11.562650
10.655088	484.216169	11.567667
10.567930	486.820694	11.572685
10.556410	477.948945	11.577703
10.446568	484.025067	11.582720
10.567841	486.597141	11.587738
10.655578	477.151387	11.592755
10.479495	486.813181	11.597773
10.310551	484.334056	11.602791
10.704008	480.997387	11.607808
10.513525	485.684954	11.612826
10.639992	489.840359	11.617843
10.420991	487.009281	11.622861
10.565889	482.944487	11.627879
11.039683	485.237623	11.632896
10.864576	483.542060	11.637914
11.069034	483.485143	11.642931
10.587224	489.616025	11.647949
10.681989	487.275713	11.652967
10.963914	487.686394	11.657984
10.873799	488.082421	11.663002
10.786433	487.682794	11.668019
10.708479	486.843065	11.673037
10.590801	490.421130	11.678055
11.050560	481.239328	11.683072
10.956861	487.306627	11.688090
10.747212	484.795971	11.693107
10.855661	486.937716	11.698125
10.758445	487.855532	11.703143
10.667956	483.227812	11.708160
10.928005	489.770184	11.713178
11.190475	487.406916	11.718195
10.751877	481.930878	11.723213
10.701416	489.591363	11.728231
11.032058	489.186611	11.733248
10.974060	492.468219	11.738266
11.060958	486.623197	11.743283
10.732260	496.267734	11.748301
10.880091	486.124686	11.753319
11.281240	481.511934	11.758336
11.009531	491.538897	11.763354
11.407747	488.305622	11.768371
11.109225	485.477459	11.773389
10.873954	486.113826	11.778407
11.238224	484.078676	11.783424
11.066759	488.138463	11.788442
10.787053	483.590693	11.793459
11.228429	478.684514	11.798477
10.948711	483.139833	11.803495
11.352477	487.400379	11.808512
10.809742	491.615798	11.813530
10.900011	485.227478	11.818547
11.049958	483.250942	11.823565
10.815789	485.531234	11.828583
10.742740	485.997184	11.833600
10.976650	498.002915	11.838618
10.932492	502.677172	11.843635
11.303702	508.564800	11.848653
11.203731	495.112173	11.853671
11.168724	503.073201	11.858688
11.074828	502.052926	11.863706
11.260200	496.347195	11.868723
11.217352	505.025779	11.873741
11.104023	503.967505	11.878759
11.187030	495.645893	11.883776
11.130082	515.639716	11.888794
11.393752	502.326117	11.893811
11.161580	499.329838	11.898829
11.046324	502.554094	11.903847
11.585886	498.361580	11.908864
11.219490	509.012337	11.913882
11.382802	508.523189	11.918899
11.362120	508.782180	11.923917
11.220032	499.403754	11.928935
11.343014	501.123535	11.933952
11.325631	504.831147	11.938970
10.892164	502.771884	11.943987
11.370499	495.985484	11.949005
11.087116	501.571104	11.954023
11.220917	499.821132	11.959040
11.144806	516.671747	11.964058
11.259253	529.690134	11.969075
11.349490	522.938904	11.974093
11.438617	524.821742	11.979111
11.771064	526.366909	11.984128
11.600032	525.071476	11.989146
11.105822	521.156671	11.994163
11.258842	520.088483	11.999181
11.316177	521.427186	12.004199
11.580714	512.152693	12.009216
11.558686	512.326690	12.014234
11.582948	522.096160	12.019251
11.617382	526.912813	12.024269
11.667070	518.962435	12.029287
11.978880	523.092146	12.034304
11.992773	517.902235	12.039322
11.635705	526.140625	12.044339
11.601139	524.240147	12.049357
11.493284	524.418040	12.054375
11.582288	515.218211	12.059392
11.777479	525.358682	12.064410
11.394660	525.674056	12.069427
11.579830	522.297228	12.074445
11.495027	525.535681	12.079463
12.077476	522.358919	12.084480
12.066470	527.633907	12.089498
11.882686	521.061036	12.094515
11.907604	516.263867	12.099533
11.487661	532.899800	12.104551
12.003561	526.442040	12.109568
11.605563	517.570487	12.114586
11.921349	522.510584	12.119603
11.993980	511.000206	12.124621
11.544430	520.370096	12.129639
11.625954	527.625056	12.134656
11.771193	528.438856	12.139674
11.816883	525.279395	12.144691
11.709410	525.760173	12.149709
11.484594	533.274261	12.154727
11.754991	512.922476	12.159744
11.694191	522.449580	12.164762
11.795827	521.332591	12.169779
11.801111	519.892948	12.174797
11.957836	522.102917	12.179815
11.780860	516.021271	12.184832
11.817183	520.907053	12.189850
11.602294	516.904580	12.194867
11.937559	527.136848	12.199885
12.037693	534.366824	12.204903
12.101267	527.502984	12.209920
11.593921	532.972012	12.214938
11.708055	539.776952	12.219955
12.284972	546.595044	12.224973
12.113473	550.506534	12.229991
12.317517	552.349393	12.235008
12.032739	550.033454	12.240026
12.022370	549.546101	12.245043
12.231323	556.105921	12.250061
12.211860	551.148402	12.255079
12.262623	538.697865	12.260096
12.142497	533.916963	12.265114
11.947590	532.486398	12.270131
12.143969	537.688077	12.275149
11.801010	547.634650	12.280167
12.238011	543.786283	12.285184
12.312547	553.689947	12.290202
12.349648	548.897184	12.295219
12.360143	552.212318	12.300237
12.302513	553.048238	12.305255
12.270115	548.095889	12.310272
12.026259	542.172963	12.315290
12.242911	548.936699	12.320307
12.366052	541.148436	12.325325
11.963675	554.499762	12.330343
12.263444	552.357887	12.335360
12.591480	547.980554	12.340378
12.362355	548.720103	12.345395
12.828322	545.299552	12.350413
12.091939	536.856199	12.355431
12.049174	535.963654	12.360448
12.302816	540.787206	12.365466
12.438418	555.957638	12.370483
12.415892	549.432229	12.375501
12.196071	554.862808	12.380519
12.620290	547.510483	12.385536
12.167144	548.890800	12.390554
12.088578	545.854819	12.395571
12.711546	546.720465	12.400589
12.358519	546.232817	12.405607
12.558437	554.188847	12.410624
12.314825	547.562168	12.415642
12.267812	546.402052	12.420659
12.495193	547.742682	12.425677
12.520541	553.415943	12.430695
12.828942	541.922483	12.435712
12.656806	549.885948	12.440730
12.412194	552.742206	12.445747
12.831901	543.938977	12.450765
12.336994	550.605227	12.455783
12.178629	550.052559	12.460800
12.406442	551.383655	12.465818
12.370676	553.166026	12.470835
12.205575	546.419830	12.475853
12.320077	543.082403	12.480871
12.540732	552.745575	12.485888
12.962365	562.535244	12.490906
12.783148	558.580854	12.495923
12.615800	548.205988	12.500941
12.517599	555.580457	12.505959
12.641985	560.051770	12.510976
13.129028	561.721186	12.515994
12.947875	569.121198	12.521011
13.241096	550.365742	12.526029
12.768086	556.201800	12.531047
12.804085	549.979690	12.536064
13.001139	553.190042	12.541082
12.425997	550.171418	12.546099
12.984617	539.935979	12.551117
12.775047	545.387050	12.556135
12.734094	549.634804	12.561152
12.796895	546.668328	12.566170
12.639163	553.398841	12.571187
12.741125	549.492189	12.576205
12.645480	541.280418	12.581223
12.570946	560.532292	12.586240
12.883425	569.098782	12.591258
12.929409	579.246737	12.596275
13.015879	572.335135	12.601293
13.092990	575.377981	12.606311
12.992321	575.933437	12.611328
13.340957	574.389840	12.616346
13.008374	571.062059	12.621363
13.021610	557.566513	12.626381
13.069424	557.426692	12.631399
12.937429	556.718445	12.636416
13.033654	560.225352	12.641434
12.729928	570.364636	12.646451
13.009364	565.284840	12.651469
13.394668	574.843497	12.656487
13.036565	566.549508	12.661504
13.451925	568.580364	12.666522
13.061525	575.501740	12.671539
13.098779	572.753822	12.676557
13.211975	569.252498	12.681575
12.849281	569.927641	12.686592
12.994065	562.035018	12.691610
12.677617	574.318986	12.696627
13.303391	575.562878	12.701645
13.308272	578.348738	12.706663
13.157745	572.165129	12.711680
13.044359	577.203618	12.716698
12.909544	587.906725	12.721715
13.324407	575.967495	12.726733
13.324291	574.427706	12.731751
13.322797	572.436871	12.736768
13.478916	573.081728	12.741786
13.221821	577.173801	12.746803
13.234401	573.968997	12.751821
13.260711	578.360914	12.756839
13.140652	579.430607	12.761856
13.585245	564.252191	12.766874
13.385853	574.782316	12.771891
13.484477	576.698393	12.776909
13.466267	571.156874	12.781927
12.821801	576.177069	12.786944
13.643255	568.693463	12.791962
12.893886	575.528723	12.796979
13.261015	575.478036	12.801997
13.211591	585.552490	12.807015
13.528675	596.453475	12.812032
13.871880	604.065339	12.817050
13.393433	594.265881	12.822067
13.415444	588.443551	12.827085
13.668090	595.902261	12.832103
13.512375	591.758019	12.837120
13.796443	584.683109	12.842138
13.463207	584.583682	12.847155
13.291037	579.788781	12.852173
13.455291	590.028776	12.857191
13.494235	599.720266	12.862208
13.534297	599.480670	12.867226
13.580101	599.940740	12.872243
13.657818	598.354119	12.877261
13.862674	596.649876	12.882279
13.752234	601.567999	12.887296
13.992053	590.646895	12.892314
13.862383	598.111484	12.897331
13.958728	585.133132	12.902349
13.735770	586.790024	12.907367
13.279527	582.175045	12.912384
13.645987	586.242615	12.917402
13.970768	595.858042	12.922419
13.643741	589.111796	12.927437
13.836808	594.314007	12.932455
14.047644	597.108828	12.937472
14.024813	592.902873	12.942490
13.978914	592.506254	12.947507
13.909116	597.582143	12.952525
14.084815	586.431193	12.957543
13.786662	587.134156	12.962560
13.911781	573.466551	12.967578
14.006044	584.746189	12.972595
14.008153	574.051447	12.977613
14.040419	569.309921	12.982631
13.582117	575.440329	12.987648
14.257677	576.515529	12.992666
13.894179	576.657489	12.997683
13.932768	568.462675	13.002701
13.825850	574.459481	13.007719
13.871666	588.362717	13.012736
14.134242	593.490992	13.017754
14.077751	589.908790	13.022771
14.239706	589.785910	13.027789
14.140457	584.506303	13.032807
14.086336	593.713683	13.037824
14.180701	586.191801	13.042842
14.052711	589.228715	13.047859
14.109985	592.400880	13.052877
14.135150	586.896782	13.057895
13.799871	600.928788	13.062912
14.181137	595.694279	13.067930
14.176161	595.108259	13.072947
13.897904	590.434010	13.077965
14.107353	595.576868	13.082983
13.838759	595.517867	13.088000
13.899769	588.865833	13.093018
13.595349	597.187573	13.098035
13.807936	597.549095	13.103053
14.442394	609.221150	13.108071
14.233681	616.587605	13.113088
14.578067	617.992071	13.118106
14.271578	614.202646	13.123123
14.119847	618.120540	13.128141
14.534522	616.822267	13.133159
13.902027	626.324833	13.138176
14.416328	612.602915	13.143194
14.283263	616.596795	13.148211
14.537375	631.385936	13.153229
14.892532	620.229115	13.158247
14.632655	619.834254	13.163264
14.771103	601.528858	13.168282
14.345571	604.747795	13.173299
14.291700	590.155030	13.178317
14.363346	589.806380	13.183335
14.231647	607.101219	13.188352
14.221902	616.696161	13.193370
14.282973	619.113532	13.198387
14.459695	619.811985	13.203405
14.739318	624.622047	13.208423
14.317759	622.459933	13.213440
14.630624	620.426459	13.218458
14.668118	625.536142	13.223475
14.438919	617.868972	13.228493
14.688762	618.751693	13.233511
14.475600	623.900401	13.238528
14.605151	618.045539	13.243546
14.521052	613.886986	13.248563
14.376864	619.179582	13.253581
14.851580	612.163337	13.258599
14.609161	619.393036	13.263616
14.681017	622.045404	13.268634
14.754484	614.637213	13.273651
14.499290	629.887488	13.278669
14.368002	622.631089	13.283687
15.142862	635.669801	13.288704
14.756303	628.917030	13.293722
14.952402	634.683649	13.298739
14.517181	628.206687	13.303757
15.168415	637.326358	13.308775
14.809876	631.822030	13.313792
14.536009	637.175846	13.318810
14.871223	651.368575	13.323827
14.894794	645.205169	13.328845
15.076734	646.584439	13.333863
14.779302	657.170900	13.338880
15.078292	645.480030	13.343898
14.914928	643.164109	13.348915
15.086563	648.906139	13.353933
15.160998	648.538119	13.358951
14.982604	653.410033	13.363968
15.034151	651.149009	13.368986
15.293324	646.627745	13.374003
15.150040	645.192289	13.379021
15.399350	634.531603	13.384039
15.027531	630.149610	13.389056
14.886511	622.904194	13.394074
15.066760	631.513391	13.399091
15.241149	646.924005	13.404109
15.199841	624.092921	13.409127
14.825604	632.242517	13.414144
15.225466	634.708124	13.419162
15.347669	634.783929	13.424179
14.904957	645.427716	13.429197
15.246104	641.982401	13.434215
14.900668	634.213406	13.439232
15.494536	643.061156	13.444250
15.221782	642.554695	13.449267
15.041382	645.451462	13.454285
15.577491	637.927050	13.459303
15.045183	642.854065	13.464320
15.062894	650.122167	13.469338
15.416711	644.424875	13.474355
15.801108	640.414271	13.479373
15.341623	637.358690	13.484391
14.847994	645.946588	13.489408
15.286552	650.113397	13.494426
15.404038	650.003752	13.499443
15.372723	646.304014	13.504461
15.597711	643.246000	13.509479
15.407947	648.624593	13.514496
15.594424	634.303628	13.519514
15.533941	637.636141	13.524531
15.404270	637.833210	13.529549
15.598694	629.636193	13.534567
15.072158	637.768481	13.539584
15.151689	634.262919	13.544602
15.446810	631.380172	13.549619
15.144366	646.218112	13.554637
15.929716	657.093563	13.559655
15.886835	654.935600	13.564672
15.479313	652.484129	13.569690
15.665270	641.767032	13.574707
15.399327	645.595422	13.579725
15.702492	648.000349	13.584743
15.413534	656.600564	13.589760
15.472212	659.318103	13.594778
15.708757	666.277596	13.599795
15.639090	667.030191	13.604813
16.322757	664.730704	13.609831
15.871336	668.417570	13.614848
15.761557	665.812446	13.619866
16.158998	652.604135	13.624883
15.787947	645.826853	13.629901
15.937801	639.981445	13.634919
15.723357	634.864920	13.639936
15.718731	635.932423	13.644954
15.814664	649.215701	13.649971
15.637330	653.462625	13.654989
15.913221	660.182467	13.660007
15.934035	658.680437	13.665024
16.138954	659.633268	13.670042
16.241251	661.473046	13.675059
15.862867	652.260713	13.680077
16.105970	654.230041	13.685095
15.951219	644.519007	13.690112
15.796141	655.127482	13.695130
16.150750	660.033173	13.700147
15.806178	661.863635	13.705165
16.094172	654.425182	13.710183
16.077294	657.978119	13.715200
16.100989	657.766316	13.720218
16.030596	667.023602	13.725235
15.772546	672.592708	13.730253
15.858219	662.361411	13.735271
16.196564	658.111830	13.740288
15.835930	654.015257	13.745306
16.260380	657.329073	13.750323
16.194595	655.234634	13.755341
16.163479	660.755781	13.760359
16.024546	656.391169	13.765376
16.156907	662.230834	13.770394
16.152937	649.372191	13.775411
16.093052	654.929372	13.780429
15.963815	664.946872	13.785447
16.079941	662.215062	13.790464
16.023999	673.994652	13.795482
16.822450	677.912937	13.800499
16.495132	689.908353	13.805517
16.793750	669.346875	13.810535
16.419584	670.080611	13.815552
16.151289	665.357455	13.820570
16.446469	660.221533	13.825587
16.305215	664.772100	13.830605
16.419434	670.557789	13.835623
16.403270	663.917743	13.840640
16.843961	674.941537	13.845658
16.900806	658.450687	13.850675
16.568854	662.614393	13.855693
16.300280	651.819742	13.860711
16.620095	663.253654	13.865728
16.258156	661.552450	13.870746
16.569130	666.512271	13.875763
16.802841	666.958865	13.880781
16.448153	656.313313	13.885799
16.359096	666.987253	13.890816
16.517747	677.537429	13.895834
16.541134	681.361802	13.900851
16.722165	685.843261	13.905869
17.015814	686.122739	13.910887
17.303303	683.332687	13.915904
16.997023	682.108792	13.920922
16.895986	666.721762	13.925939
16.421059	672.312012	13.930957
16.252172	659.236051	13.935975
16.417406	674.149516	13.940992
16.378332	688.533089	13.946010
16.851556	678.525455	13.951027
16.764140	683.351656	13.956045
16.784251	681.758218	13.961063
16.774810	683.476545	13.966080
16.224856	686.493970	13.971098
16.849283	678.482437	13.976115
16.761755	685.454525	13.981133
16.640339	680.257233	13.986151
17.053637	702.674202	13.991168
16.792731	701.339102	13.996186
17.210059	704.366868	14.001203
17.467947	707.337411	14.006221
17.053768	688.265930	14.011239
17.052903	684.801277	14.016256
16.742300	690.088247	14.021274
17.140555	698.341654	14.026291
16.953646	707.626569	14.031309
17.383427	702.422344	14.036327
17.412291	705.980791	14.041344
17.326258	693.078091	14.046362
17.082423	677.908938	14.051379
16.874602	682.416226	14.056397
17.235454	689.589894	14.061415
17.433174	688.912354	14.066432
17.377632	686.210424	14.071450
17.524263	683.391813	14.076467
17.481714	685.273080	14.081485
17.404668	680.901982	14.086503
17.363477	673.224451	14.091520
17.160291	677.014674	14.096538
17.862793	672.541140	14.101555
17.524918	677.643011	14.106573
17.111185	667.300125	14.111591
17.566976	671.640975	14.116608
17.322484	677.665547	14.121626
17.286120	671.022331	14.126643
17.149811	671.453955	14.131661
17.332630	669.582730	14.136679
17.460360	673.570730	14.141696
17.039287	677.265495	14.146714
17.376900	678.759379	14.151731
17.605473	693.117064	14.156749
17.208527	694.517042	14.161767
17.838656	699.048498	14.166784
17.732496	708.869933	14.171802
17.578148	704.763320	14.176819
17.811199	707.813467	14.181837
17.484180	704.459549	14.186855
17.699316	700.800321	14.191872
17.640692	705.117133	14.196890
17.498288	700.850877	14.201907
17.482638	697.031930	14.206925
17.535374	701.372427	14.211943
17.971574	691.241167	14.216960
17.657735	704.064441	14.221978
17.518272	700.542471	14.226995
17.511025	688.681509	14.232013
17.523282	698.307783	14.237031
17.741712	696.184866	14.242048
17.528803	708.515919	14.247066
17.774857	703.517018	14.252083
17.723746	702.856130	14.257101
17.710838	699.749942	14.262119
17.705859	698.315038	14.267136
17.784339	708.458007	14.272154
18.156877	719.410392	14.277171
18.050452	726.981866	14.282189
17.947414	715.807964	14.287207
18.250385	713.693973	14.292224
17.953585	707.189119	14.297242
17.800016	711.142032	14.302259
18.150955	710.996039	14.307277
18.153204	721.185597	14.312295
18.486619	720.818277	14.317312
17.866863	721.703857	14.322330
17.711634	706.104332	14.327347
17.957235	714.839090	14.332365
18.058392	725.373000	14.337383
18.280774	721.759975	14.342400
18.009002	727.192384	14.347418
18.327784	716.968941	14.352435
18.240570	716.900633	14.357453
18.331036	722.096767	14.362471
18.316919	725.043393	14.367488
18.178429	723.850173	14.372506
18.263844	728.245547	14.377523
18.353714	723.091082	14.382541
17.896096	731.894313	14.387559
18.031522	724.766754	14.392576
18.348628	728.371843	14.397594
18.396711	721.923737	14.402611
18.365045	721.490187	14.407629
18.255246	716.357345	14.412647
18.308237	714.843988	14.417664
18.409017	716.728189	14.422682
18.331869	715.339232	14.427699
18.670011	719.411243	14.432717
18.446562	731.658749	14.437735
18.670089	718.916109	14.442752
18.478295	731.341717	14.447770
18.618329	721.840356	14.452787
18.888896	728.100322	14.457805
18.779221	726.138936	14.462823
18.699881	720.155623	14.467840
18.485485	723.701458	14.472858
18.490785	724.155215	14.477875
18.731681	714.297338	14.482893
18.391693	721.700054	14.487911
18.770826	718.608560	14.492928
18.715583	725.354739	14.497946
18.629140	719.896378	14.502963
18.952628	728.268733	14.507981
18.801036	728.481839	14.512999
18.545911	713.869816	14.518016
18.693491	718.990787	14.523034
19.010495	725.366594	14.528051
19.305011	738.240336	14.533069
18.989126	725.225082	14.538087
18.744731	715.660505	14.543104
19.089247	713.827214	14.548122
18.704534	722.821054	14.553139
18.707484	717.285662	14.558157
18.597929	734.536153	14.563175
18.616849	737.035839	14.568192
18.979540	741.176614	14.573210
19.086875	739.998766	14.578227
19.261936	737.185187	14.583245
19.143892	736.143412	14.588263
19.018341	732.369969	14.593280
19.001022	742.789796	14.598298
18.789055	744.470237	14.603315
19.270232	749.779110	14.608333
18.795429	752.118991	14.613351
18.874417	738.158650	14.618368
19.086056	743.850303	14.623386
19.047935	737.087420	14.628403
19.164246	740.187305	14.633421
19.116254	746.326468	14.638439
19.309347	746.141936	14.643456
19.108359	752.156604	14.648474
19.537541	760.130678	14.653491
19.710103	752.056927	14.658509
19.594111	739.427092	14.663527
19.239742	738.179123	14.668544
19.107470	745.710449	14.673562
19.180359	740.530222	14.678579
19.953081	739.709508	14.683597
19.590843	747.144100	14.688615
19.648847	733.682475	14.693632
19.491954	725.470688	14.698650
19.523507	743.961497	14.703667
19.629586	735.888637	14.708685
19.405579	742.837817	14.713703
19.171855	735.871867	14.718720
19.765217	743.832995	14.723738
19.027377	742.957145	14.728755
19.675086	751.458906	14.733773
19.765950	759.280534	14.738791
19.840106	757.978467	14.743808
19.759851	757.457810	14.748826
19.921136	760.392911	14.753843
19.693205	751.034029	14.758861
19.399104	746.393761	14.763879
19.701908	751.029841	14.768896
19.750628	760.410637	14.773914
20.021067	759.235794	14.778931
20.227879	746.577785	14.783949
19.836224	739.737405	14.788967
19.766474	729.751167	14.793984
20.077729	742.925254	14.799002
20.153274	736.706389	14.804019
19.864349	725.776010	14.809037
19.692797	731.704040	14.814055
19.909828	730.887797	14.819072
20.096171	740.143017	14.824090
19.876762	735.756202	14.829107
20.141049	737.479252	14.834125
19.922573	757.305998	14.839143
19.941270	753.838285	14.844160
20.475827	747.090373	14.849178
20.144363	741.073726	14.854195
20.269530	729.457200	14.859213
19.992253	737.127860	14.864231
19.661715	722.846297	14.869248
20.393440	731.770454	14.874266
20.142886	756.111689	14.879283
20.329319	744.880077	14.884301
20.114903	748.249199	14.889319
19.795728	750.148297	14.894336
20.029150	752.463115	14.899354
20.159385	751.016621	14.904371
20.446417	746.156490	14.909389
20.431645	757.680426	14.914407
20.010933	757.222244	14.919424
20.403138	754.286494	14.924442
20.191287	757.014611	14.929459
20.352629	748.936296	14.934477
20.354124	753.363677	14.939495
20.166604	755.529446	14.944512
20.458105	751.990858	14.949530
20.206955	755.293120	14.954547
20.270594	750.868544	14.959565
20.234350	765.576777	14.964583
20.182315	777.235911	14.969600
20.827592	772.651344	14.974618
20.836676	773.874506	14.979635
20.840657	764.353281	14.984653
20.525895	769.394777	14.989671
20.650446	778.675416	14.994688
20.926758	772.810276	14.999706
20.727416	773.393723	15.004723
20.708764	772.797204	15.009741
20.698325	774.159101	15.014759
20.945965	773.265509	15.019776
20.759979	768.939752	15.024794
20.645918	775.108146	15.029811
20.748418	772.697167	15.034829
21.073653	776.512432	15.039847
21.149886	769.561324	15.044864
21.156293	759.891405	15.049882
20.840664	755.121948	15.054899
21.014940	744.476034	15.059917
20.903296	740.463746	15.064935
20.598524	747.971440	15.069952
20.943111	751.774220	15.074970
20.751361	771.161333	15.079987
21.009901	771.982749	15.085005
21.042506	773.833390	15.090023
20.846375	767.565297	15.095040
21.002411	769.030658	15.100058
21.207622	773.473661	15.105075
21.302451	771.227973	15.110093
21.177552	770.638530	15.115111
21.019121	777.258787	15.120128
21.809321	765.652299	15.125146
21.403990	766.917893	15.130163
21.483183	769.010581	15.135181
21.051635	757.083096	15.140199
20.853501	759.525064	15.145216
20.904923	763.932052	15.150234
21.128902	762.048097	15.155251
21.349019	759.763969	15.160269
21.463571	770.661883	15.165287
21.389218	772.658560	15.170304
21.523924	765.051430	15.175322
21.394493	772.670685	15.180339
21.225374	767.745874	15.185357
21.279536	770.946956	15.190375
21.278234	765.364876	15.195392
21.562299	763.020300	15.200410
21.267091	770.636963	15.205427
21.830841	761.517720	15.210445
21.636001	761.646044	15.215463
21.413110	771.274256	15.220480
21.568850	756.017578	15.225498
20.950812	765.420140	15.230515
21.656224	766.695827	15.235533
21.512796	787.344027	15.240551
21.772055	787.584682	15.245568
21.816159	785.889672	15.250586
21.683965	792.408023	15.255603
21.576852	782.326589	15.260621
21.527683	790.176345	15.265639
21.299222	795.980717	15.270656
21.791291	786.998849	15.275674
21.786695	790.357402	15.280691
22.065661	795.006672	15.285709
21.996218	791.672592	15.290727
21.805751	793.314977	15.295744
22.155499	785.301982	15.300762
22.154720	793.210475	15.305779
22.147750	798.323974	15.310797
22.188058	789.043225	15.315815
22.023289	795.298414	15.320832
22.324920	787.965076	15.325850
21.955381	795.243040	15.330867
22.010033	794.259578	15.335885
22.161480	793.358872	15.340903
21.844637	794.007949	15.345920
22.055741	792.223823	15.350938
21.976942	803.540013	15.355955
22.015030	792.501876	15.360973
22.187351	797.738934	15.365991
21.891863	798.432023	15.371008
22.128576	791.604239	15.376026
22.116772	794.411665	15.381043
22.009948	793.585884	15.386061
22.227367	799.052599	15.391079
22.211807	812.365981	15.396096
22.599905	799.698643	15.401114
21.893477	818.490618	15.406131
22.726735	818.897517	15.411149
22.827388	808.427124	15.416167
22.588078	815.618550	15.421184
22.744493	804.997471	15.426202
22.823974	800.529391	15.431219
22.394493	781.469659	15.436237
22.417761	794.085882	15.441255
22.185039	795.583372	15.446272
22.410552	801.323375	15.451290
22.587304	816.512868	15.456307
22.471712	816.546806	15.461325
22.714054	820.693714	15.466343
22.727488	828.394888	15.471360
23.117260	820.075854	15.476378
22.884804	817.833781	15.481395
22.770947	812.900353	15.486413
23.063757	811.027767	15.491431
22.694801	802.173639	15.496448
22.697269	799.525773	15.501466
23.007866	809.323401	15.506483
22.949955	797.886808	15.511501
22.594432	789.103177	15.516519
22.189471	806.513337	15.521536
22.794028	812.197483	15.526554
23.094817	816.597215	15.531571
22.726977	820.261630	15.536589
22.676182	808.704006	15.541607
22.881433	825.040905	15.546624
23.156460	809.352210	15.551642
23.222772	812.623990	15.556659
23.111725	813.187379	15.561677
22.917390	817.219245	15.566695
22.956809	809.933035	15.571712
23.380593	807.768666	15.576730
23.080513	811.870641	15.581747
23.012756	820.767845	15.586765
23.052197	818.354055	15.591783
23.069202	820.194507	15.596800
23.456949	811.651736	15.601818
23.324423	824.175475	15.606835
22.989322	815.161440	15.611853
23.418326	815.811154	15.616871
23.064032	824.876047	15.621888
23.771248	836.240287	15.626906
23.259022	826.398623	15.631923
23.478368	837.633702	15.636941
23.626319	832.186148	15.641959
23.088178	837.407605	15.646976
23.512315	836.890463	15.651994
23.364675	839.879987	15.657011
23.222871	835.689342	15.662029
23.428060	829.917305	15.667047
23.812594	836.566653	15.672064
23.819112	827.316391	15.677082
23.844776	831.932527	15.682099
23.482634	841.087009	15.687117
23.820362	831.681038	15.692135
24.084623	837.743215	15.697152
23.927485	829.159043	15.702170
23.893382	826.756702	15.707187
23.804077	826.376303	15.712205
23.905678	828.547558	15.717223
23.713617	826.532718	15.722240
23.758430	828.766461	15.727258
23.898964	819.981317	15.732275
23.656611	838.385487	15.737293
23.851699	825.028678	15.742311
23.742750	824.815435	15.747328
23.577114	817.409675	15.752346
23.901663	820.467685	15.757363
23.749049	827.206972	15.762381
24.151163	828.409969	15.767399
23.900418	832.176073	15.772416
23.828547	829.205271	15.777434
23.744898	817.513905	15.782451
23.658631	838.847523	15.787469
24.375636	847.098707	15.792487
24.316963	853.220636	15.797504
24.413490	842.451072	15.802522
24.525155	848.650617	15.807539
24.124103	853.746596	15.812557
24.515143	842.896465	15.817575
24.289202	839.807642	15.822592
24.135528	837.120967	15.827610
24.629052	838.710509	15.832627
24.225035	837.978333	15.837645
24.418200	834.025861	15.842663
24.660353	851.168059	15.847680
24.440547	836.234864	15.852698
24.237968	838.153686	15.857715
24.220158	850.624870	15.862733
24.627599	845.878505	15.867751
24.443045	852.364006	15.872768
24.130117	851.589246	15.877786
24.667304	854.995998	15.882803
24.856809	846.607149	15.887821
24.978570	841.592848	15.892839
24.940934	842.195300	15.897856
24.727309	846.324847	15.902874
24.866638	844.012262	15.907891
24.560091	842.018401	15.912909
24.740472	849.737771	15.917927
24.870630	842.895000	15.922944
24.680367	848.825982	15.927962
25.085318	845.001476	15.932979
24.648008	847.789955	15.937997
24.654487	846.526820	15.943015
24.740218	845.806752	15.948032
24.690275	849.431145	15.953050
25.036770	849.219573	15.958067
24.745422	853.380157	15.963085
24.610264	850.431828	15.968103
24.732813	851.965524	15.973120
24.669552	853.152619	15.978138
24.674925	849.185203	15.983155
24.990843	868.439732	15.988173
25.036963	871.266554	15.993191
24.972440	867.281614	15.998208
25.066287	872.777059	16.003226
25.207852	877.965282	16.008243
24.883778	875.750090	16.013261
25.091197	868.942615	16.018279
25.323186	868.363873	16.023296
25.254484	870.814106	16.028314
25.457124	872.496276	16.033331
25.007740	873.137591	16.038349
25.292081	875.595972	16.043367
25.441199	868.456756	16.048384
25.444768	879.854842	16.053402
25.511002	865.113767	16.058419
25.180454	868.576731	16.063437
25.427454	865.127098	16.068455
25.626432	878.836306	16.073472
25.535529	889.131979	16.078490
25.832215	883.790637	16.083507
25.743168	886.954079	16.088525
25.737203	870.176173	16.093543
25.351201	870.391064	16.098560
25.600729	881.766635	16.103578
26.053320	880.146868	16.108595
25.763253	879.605227	16.113613
25.601493	868.077464	16.118631
25.825317	879.340273	16.123648
26.262591	886.978638	16.128666
26.090884	874.395251	16.133683
26.013951	872.356169	16.138701
25.743627	868.456919	16.143719
25.637637	872.585492	16.148736
25.526354	877.465952	16.153754
25.779209	874.917944	16.158771
25.973250	894.440779	16.163789
26.107510	890.724679	16.168807
25.970272	883.809918	16.173824
25.963925	897.295495	16.178842
26.330371	889.466042	16.183859
25.975787	895.678238	16.188877
25.984090	889.270977	16.193895
26.547961	883.357874	16.198912
25.995811	881.096142	16.203930
26.138657	888.852931	16.208947
26.143885	884.746677	16.213965
26.135603	889.705776	16.218983
26.666178	886.679035	16.224000
26.094959	880.011721	16.229018
26.273125	875.704979	16.234035
26.017596	881.762895	16.239053
26.109671	886.955670	16.244071
26.274786	883.525095	16.249088
26.324939	883.416464	16.254106
26.304359	887.317153	16.259123
26.204803	899.311961	16.264141
26.113913	904.236590	16.269159
26.767522	908.682396	16.274176
26.451445	905.430875	16.279194
26.636122	900.075410	16.284211
26.611742	910.505902	16.289229
26.878058	908.829930	16.294247
27.079113	916.038038	16.299264
26.688166	917.159394	16.304282
27.075848	910.898181	16.309299
27.153849	915.591395	16.314317
26.797748	897.473145	16.319335
27.010302	884.889881	16.324352
26.417551	887.080890	16.329370
26.804467	890.473177	16.334387
26.996605	906.749078	16.339405
26.909483	898.794585	16.344423
26.829739	893.183653	16.349440
26.802726	913.583506	16.354458
27.184788	904.880634	16.359475
26.870726	902.730149	16.364493
26.862848	900.894902	16.369511
26.881600	899.027108	16.374528
27.010111	904.460363	16.379546
27.353428	899.067576	16.384563
27.161379	903.862791	16.389581
26.983191	898.895175	16.394599
26.997478	891.849524	16.399616
26.832557	896.476416	16.404634
26.888268	899.147118	16.409651
27.150355	918.542624	16.414669
27.346401	921.873118	16.419687
27.749551	920.806988	16.424704
27.631100	913.939782	16.429722
27.398016	894.344433	16.434739
27.062101	907.253340	16.439757
27.611384	907.647651	16.444775
27.843395	906.390422	16.449792
27.366655	914.060656	16.454810
27.846864	906.595327	16.459827
27.592898	908.881911	16.464845
27.296543	908.726247	16.469863
27.580410	911.071100	16.474880
27.555820	921.280730	16.479898
27.737767	914.117451	16.484915
27.893850	913.575771	16.489933
27.539296	921.432107	16.494951
27.841422	910.135042	16.499968
28.105555	920.309185	16.504986
27.873547	908.180121	16.510003
27.924874	915.559860	16.515021
27.806199	916.408456	16.520039
27.658539	911.095264	16.525056
28.006418	921.379443	16.530074
27.856428	919.443247	16.535091
28.182351	918.272378	16.540109
27.813096	912.775942	16.545127
28.058276	911.687071	16.550144
28.039452	907.158533	16.555162
27.756533	909.203477	16.560179
28.243448	906.073080	16.565197
27.865802	918.426772	16.570215
28.488172	907.332306	16.575232
28.119327	917.261025	16.580250
28.314970	909.641190	16.585267
28.088134	905.981307	16.590285
28.122407	910.056493	16.595303
28.062490	906.477917	16.600320
27.811169	928.058242	16.605338
28.032885	921.952250	16.610355
28.815406	936.447941	16.615373
28.338440	934.303882	16.620391
28.437353	934.159258	16.625408
28.580869	934.380066	16.630426
28.398107	935.137658	16.635443
28.509017	934.514650	16.640461
28.856436	937.812112	16.645479
28.921535	928.334931	16.650496
28.838433	932.646142	16.655514
28.404428	913.416563	16.660531
28.430953	927.001183	16.665549
28.366615	937.182298	16.670567
28.401112	939.739546	16.675584
28.636626	939.602056	16.680602
28.713837	936.257738	16.685619
28.553965	928.431321	16.690637
28.794909	940.947486	16.695655
28.992243	925.030950	16.700672
28.791430	936.022246	16.705690
28.573054	927.412848	16.710707
28.712581	943.949434	16.715725
29.055217	955.957482	16.720743
29.152446	951.486601	16.725760
29.211097	953.623534	16.730778
29.414738	946.258052	16.735795
29.367197	936.953035	16.740813
29.201149	925.230246	16.745831
29.503902	933.205149	16.750848
29.217172	929.399956	16.755866
28.924941	927.833036	16.760883
29.398751	929.113238	16.765901
29.268174	937.303930	16.770919
29.424968	923.369198	16.775936
29.444330	922.848804	16.780954
29.422264	916.679787	16.785971
29.285521	926.941595	16.790989
29.373623	931.532257	16.796007
29.794607	928.582531	16.801024
29.112720	929.881727	16.806042
29.345964	940.698150	16.811059
29.821405	940.854657	16.816077
29.660982	948.879591	16.821095
29.673603	947.303074	16.826112
29.490334	955.912224	16.831130
29.402324	947.165757	16.836147
29.589281	949.866524	16.841165
29.626616	946.534724	16.846183
29.652716	947.931970	16.851200
29.763902	953.812896	16.856218
29.519610	947.220885	16.861235
29.968030	957.167546	16.866253
29.666377	964.608574	16.871271
29.666852	946.920740	16.876288
29.745943	948.155104	16.881306
29.795007	961.985545	16.886323
29.911623	945.033852	16.891341
29.825367	959.286139	16.896359
30.273502	964.887394	16.901376
30.621128	966.707942	16.906394
30.031552	950.128122	16.911411
30.100459	947.574030	16.916429
30.112890	954.716849	16.921447
29.922911	958.145321	16.926464
29.971630	968.176310	16.931482
30.226850	971.598584	16.936499
30.358063	969.706961	16.941517
30.114416	970.802231	16.946535
30.575769	973.700116	16.951552
30.372282	969.298141	16.956570
30.216471	971.518959	16.961587
30.632288	964.155148	16.966605
30.574788	971.346731	16.971623
30.872084	966.724778	16.976640
31.034585	966.178942	16.981658
30.483082	957.037584	16.986675
31.198625	949.664982	16.991693
30.151371	952.273894	16.996711
30.316568	950.181326	17.001728
30.464182	965.725771	17.006746
30.259882	962.097081	17.011763
30.697119	963.629128	17.016781
30.301758	960.737072	17.021799
30.505579	955.365987	17.026816
30.900667	962.524969	17.031834
30.769943	965.877946	17.036851
30.910399	957.471436	17.041869
30.992539	972.704196	17.046887
30.927731	961.590457	17.051904
31.051566	970.820817	17.056922
30.941794	967.328885	17.061939
31.157025	975.481532	17.066957
31.258143	979.480056	17.071975
31.196424	968.173332	17.076992
31.088054	968.291350	17.082010
30.996669	978.050674	17.087027
31.248989	978.510158	17.092045
31.005921	994.692957	17.097063
31.217482	991.801073	17.102080
31.366404	986.132419	17.107098
31.663958	986.127277	17.112115
31.663004	984.764305	17.117133
31.529636	991.267133	17.122151
31.700674	990.107752	17.127168
31.323842	978.373566	17.132186
31.166201	985.962591	17.137203
31.557323	980.748526	17.142221
31.707939	984.092416	17.147239
31.818388	982.683698	17.152256
31.918698	985.306444	17.157274
31.766057	974.771252	17.162291
31.341319	972.909384	17.167309
31.641520	978.511586	17.172327
31.579011	985.031781	17.177344
31.551025	987.709216	17.182362
31.705022	978.517962	17.187379
31.575096	975.357363	17.192397
31.722509	978.906875	17.197415
31.391205	980.867844	17.202432
31.422788	973.223033	17.207450
31.595076	997.142164	17.212467
31.886029	1002.856265	17.217485
31.904761	1007.445124	17.222503
32.102772	996.378805	17.227520
32.002095	1005.054014	17.232538
31.938826	1002.403730	17.237555
32.246806	997.155268	17.242573
32.431178	1008.878730	17.247591
32.010109	1006.517679	17.252608
32.658540	1001.474981	17.257626
32.117941	1008.997411	17.262643
32.466240	1000.072535	17.267661
32.262948	1006.393754	17.272679
32.494083	1004.120503	17.277696
32.516566	998.212760	17.282714
32.304019	1009.789742	17.287731
32.422333	1005.694255	17.292749
32.345716	1004.513472	17.297767
32.506923	1005.274316	17.302784
32.356714	1002.915274	17.307802
32.768018	1005.227676	17.312819
32.594720	1014.627395	17.317837
32.284355	1014.899937	17.322855
32.675370	1017.385910	17.327872
32.494049	1001.783876	17.332890
32.524332	1014.055186	17.337907
32.813181	1021.628358	17.342925
32.565698	1019.274992	17.347943
32.381552	1021.295103	17.352960
32.887235	1027.042050	17.357978
32.984894	1033.256463	17.362995
33.030162	1031.163624	17.368013
33.047462	1029.851454	17.373031
32.959678	1037.751512	17.378048
33.032629	1029.033591	17.383066
32.897896	1026.934064	17.388083
32.793713	1027.654179	17.393101
32.831208	1023.148400	17.398119
32.831788	1028.980302	17.403136
33.114480	1038.608834	17.408154
33.035020	1051.452670	17.413171
33.905156	1051.096452	17.418189
33.324397	1042.729609	17.423207
33.407122	1040.974914	17.428224
33.394726	1042.829434	17.433242
33.612178	1045.048948	17.438259
33.745593	1034.907832	17.443277
33.544071	1033.197394	17.448295
33.298790	1031.569507	17.453312
33.673460	1035.538075	17.458330
33.724428	1035.725958	17.463347
33.517624	1033.249494	17.468365
33.831071	1035.242626	17.473383
33.646215	1043.170422	17.478400
33.739667	1030.864371	17.483418
33.757587	1052.254606	17.488435
33.960707	1041.663983	17.493453
33.988143	1048.940201	17.498471
33.853794	1039.443522	17.503488
34.231696	1039.088205	17.508506
33.877830	1030.367310	17.513523
34.100871	1023.333286	17.518541
34.149195	1022.398133	17.523559
33.987415	1026.289279	17.528576
34.235595	1014.940587	17.533594
33.747218	1027.895409	17.538611
34.388037	1029.323182	17.543629
34.198559	1023.833433	17.548647
33.840050	1023.545436	17.553664
34.397378	1032.900836	17.558682
34.432404	1044.663353	17.563699
34.363339	1032.868590	17.568717
34.027365	1023.425401	17.573735
34.061491	1041.051444	17.578752
34.494808	1038.895030	17.583770
34.412934	1045.875846	17.588787
34.436695	1044.041970	17.593805
34.167208	1046.141642	17.598823
34.553727	1049.076437	17.603840
34.679696	1038.223278	17.608858
34.594427	1042.588501	17.613875
34.333872	1049.912714	17.618893
34.783652	1041.126650	17.623911
34.730751	1044.035187	17.628928
34.792378	1036.376204	17.633946
34.586083	1041.643881	17.638963
34.781592	1036.870504	17.643981
34.789118	1036.721173	17.648999
34.659262	1043.677902	17.654016
34.647901	1033.414162	17.659034
34.733455	1050.587246	17.664051
34.521537	1048.714325	17.669069
34.714354	1056.381358	17.674087
34.498446	1072.323316	17.679104
35.207002	1063.774658	17.684122
35.008839	1067.100285	17.689139
35.148984	1072.364524	17.694157
35.157316	1067.822250	17.699175
35.046586	1068.593878	17.704192
35.173799	1056.749605	17.709210
35.189068	1059.499210	17.714227
35.258004	1058.387279	17.719245
35.543417	1064.932227	17.724263
35.193840	1063.449962	17.729280
35.558765	1052.067291	17.734298
35.766262	1062.657427	17.739315
35.742553	1062.124801	17.744333
35.714947	1064.253086	17.749351
35.368641	1065.635741	17.754368
35.850668	1063.979817	17.759386
35.606177	1054.992576	17.764403
35.588967	1057.923961	17.769421
35.770927	1052.243830	17.774439
35.886493	1066.474247	17.779456
35.298336	1058.354697	17.784474
35.449941	1072.339670	17.789491
36.077985	1080.942482	17.794509
36.120360	1072.879387	17.799527
35.898846	1082.072057	17.804544
36.100906	1080.021071	17.809562
36.449395	1079.922794	17.814579
36.146678	1076.003295	17.819597
35.931410	1082.752434	17.824615
35.957390	1079.472869	17.829632
36.147000	1080.087285	17.834650
35.890663	1084.315053	17.839667
35.958976	1086.800787	17.844685
36.292721	1079.632742	17.849703
35.988592	1092.006665	17.854720
36.061155	1080.218221	17.859738
36.219505	1077.934203	17.864755
35.861230	1080.805086	17.869773
36.242487	1094.697517	17.874791
36.277375	1098.614862	17.879808
36.746359	1102.313145	17.884826
36.501976	1098.665421	17.889843
36.799879	1099.259821	17.894861
36.946685	1098.899459	17.899879
37.111525	1103.519242	17.904896
36.734752	1086.944031	17.909914
36.657848	1083.768845	17.914931
36.718716	1076.987265	17.919949
36.697704	1071.487051	17.924967
36.523990	1087.911597	17.929984
36.661261	1088.234364	17.935002
36.804680	1085.028031	17.940019
36.821004	1104.480939	17.945037
37.003898	1104.632504	17.950055
36.668174	1105.584330	17.955072
36.622380	1093.208398	17.960090
37.109535	1103.537269	17.965107
37.075167	1101.018169	17.970125
37.036145	1100.112390	17.975143
36.942408	1097.466836	17.980160
37.024345	1104.557868	17.985178
37.277907	1109.605647	17.990195
37.096634	1110.574451	17.995213
37.385091	1103.126272	18.000231
37.360912	1115.503961	18.005248
37.301241	1121.048631	18.010266
37.261501	1108.110020	18.015283
37.111727	1117.272604	18.020301
37.084333	1122.824872	18.025319
37.393478	1121.675538	18.030336
37.592966	1121.991775	18.035354
37.161684	1120.364437	18.040371
37.493807	1143.166982	18.045389
38.117726	1132.242548	18.050407
38.093983	1129.851176	18.055424
38.133419	1114.839514	18.060442
38.023467	1101.438474	18.065459
37.970979	1106.511812	18.070477
38.033279	1107.341708	18.075495
37.745649	1103.388296	18.080512
38.011251	1098.253699	18.085530
37.764492	1099.781801	18.090547
37.771741	1124.985950	18.095565
38.282592	1124.912886	18.100583
38.195437	1123.213034	18.105600
38.318690	1134.043545	18.110618
38.336594	1132.807012	18.115635
38.198916	1132.099626	18.120653
38.482206	1128.574866	18.125671
38.331291	1140.016105	18.130688
38.386515	1133.620386	18.135706
38.688650	1133.238995	18.140723
38.342502	1131.516351	18.145741
38.681576	1132.082251	18.150759
38.411523	1130.600221	18.155776
38.483272	1130.276791	18.160794
38.612558	1123.484540	18.165811
38.610945	1126.006413	18.170829
38.605557	1128.380552	18.175847
38.568316	1127.973106	18.180864
38.714951	1130.951575	18.185882
38.710499	1123.331245	18.190899
38.410382	1128.742942	18.195917
38.213857	1123.869635	18.200935
38.819294	1130.030270	18.205952
38.833097	1149.180665	18.210970
38.964683	1147.194292	18.215987
38.621853	1164.061801	18.221005
39.107763	1150.593197	18.226023
38.670706	1149.178193	18.231040
38.735378	1149.755259	18.236058
38.792373	1146.871636	18.241075
39.039526	1151.058899	18.246093
39.022009	1147.760848	18.251111
39.421906	1151.965354	18.256128
39.453267	1153.317616	18.261146
39.673559	1148.373094	18.266163
39.166787	1144.002517	18.271181
39.519005	1136.885221	18.276199
39.105793	1147.212291	18.281216
39.560925	1165.157912	18.286234
39.876586	1168.728603	18.291251
39.645890	1176.609948	18.296269
39.768257	1165.911905	18.301287
39.955908	1167.672175	18.306304
39.708388	1148.056704	18.311322
39.595505	1142.012200	18.316339
39.662102	1154.558817	18.321357
39.773506	1161.298149	18.326375
39.939744	1165.905109	18.331392
39.928894	1163.811524	18.336410
40.076188	1156.281161	18.341427
39.795818	1163.027843	18.346445
40.182630	1158.344568	18.351463
40.047508	1159.148399	18.356480
39.976353	1166.067634	18.361498
40.178389	1158.938998	18.366515
39.667004	1155.455909	18.371533
40.078958	1157.354824	18.376551
39.783770	1153.544587	18.381568
40.215252	1155.939074	18.386586
40.409660	1167.490666	18.391603
40.240410	1175.406624	18.396621
40.490683	1183.620183	18.401639
40.583963	1180.857137	18.406656
40.880412	1178.813534	18.411674
40.810653	1168.186428	18.416691
40.478351	1170.403191	18.421709
40.571387	1170.694977	18.426727
40.498004	1185.273641	18.431744
40.191819	1177.160628	18.436762
40.563873	1177.408973	18.441779
40.859224	1177.561964	18.446797
40.809080	1182.436145	18.451815
41.176376	1178.945631	18.456832
41.069571	1172.073357	18.461850
41.055475	1174.120657	18.466867
40.769217	1183.235098	18.471885
40.793728	1175.837452	18.476903
41.045386	1175.937286	18.481920
41.011149	1178.713552	18.486938
41.285323	1176.111689	18.491955
41.010460	1185.738748	18.496973
41.413145	1185.016656	18.501991
41.164165	1182.426817	18.507008
40.987558	1180.684083	18.512026
41.487386	1188.350709	18.517043
40.974581	1196.036146	18.522061
41.179213	1200.823328	18.527079
41.229708	1205.382046	18.532096
41.608067	1205.209691	18.537114
41.563996	1198.365508	18.542131
41.574621	1204.845995	18.547149
41.499411	1202.983330	18.552167
41.588904	1197.532144	18.557184
41.509300	1201.249588	18.562202
41.861066	1204.451751	18.567219
41.755939	1204.698652	18.572237
41.890168	1207.051064	18.577255
41.928476	1203.917880	18.582272
41.792234	1218.291764	18.587290
42.368900	1217.451064	18.592307
42.011914	1213.016123	18.597325
42.136742	1210.869851	18.602343
42.080051	1210.449652	18.607360
41.961529	1216.322249	18.612378
42.069358	1211.827562	18.617395
41.915139	1214.906535	18.622413
42.124970	1219.560370	18.627431
42.357041	1213.938657	18.632448
42.249720	1213.870322	18.637466
42.508202	1219.138271	18.642483
42.502741	1227.858723	18.647501
42.210263	1220.119095	18.652519
42.353813	1226.708281	18.657536
42.025635	1230.720052	18.662554
42.224415	1220.060572	18.667571
42.084545	1235.918255	18.672589
42.764570	1237.450395	18.677607
43.124730	1242.039804	18.682624
43.124474	1245.268380	18.687642
43.517142	1228.671067	18.692659
43.035701	1230.488182	18.697677
42.773415	1222.652333	18.702695
43.026703	1226.977513	18.707712
43.087145	1231.313785	18.712730
43.348368	1228.537206	18.717747
43.092204	1221.924851	18.722765
42.803851	1212.988540	18.727783
43.400934	1224.767808	18.732800
43.878633	1232.021334	18.737818
43.557602	1216.175777	18.742835
43.174757	1210.006025	18.747853
42.839130	1208.818219	18.752871
43.459360	1215.566712	18.757888
43.431823	1225.038521	18.762906
43.708900	1229.893326	18.767923
43.206593	1233.247403	18.772941
43.461196	1230.882108	18.777959
43.614498	1229.940066	18.782976
43.298440	1239.639840	18.787994
43.940733	1225.354729	18.793011
43.568690	1236.278196	18.798029
43.562639	1228.434008	18.803047
43.471711	1230.638444	18.808064
43.478137	1227.772149	18.813082
43.889246	1238.005643	18.818099
43.541661	1252.604963	18.823117
44.051141	1261.718627	18.828135
44.042288	1261.616025	18.833152
44.599265	1265.960204	18.838170
44.275942	1251.916931	18.843187
44.104741	1247.481458	18.848205
44.053977	1250.171946	18.853223
44.375747	1257.146804	18.858240
44.431012	1254.948241	18.863258
44.414668	1256.143836	18.868275
44.734808	1255.690212	18.873293
44.571421	1259.783630	18.878311
44.731347	1246.236321	18.883328
44.650267	1247.773353	18.888346
44.257073	1256.954973	18.893363
44.237831	1253.470980	18.898381
43.910522	1252.960370	18.903399
44.466269	1253.561968	18.908416
44.354506	1256.602780	18.913434
44.690598	1271.064112	18.918451
44.641806	1273.018996	18.923469
44.762813	1287.283457	18.928487
45.139572	1268.088206	18.933504
44.766695	1281.744750	18.938522
44.863580	1277.548395	18.943539
45.246625	1278.492462	18.948557
44.749348	1280.971609	18.953575
44.875766	1275.861787	18.958592
44.926640	1288.859070	18.963610
44.978815	1284.287824	18.968627
44.962651	1283.627784	18.973645
45.335858	1296.981986	18.978663
45.451574	1299.378318	18.983680
45.696989	1304.279099	18.988698
45.290297	1294.272420	18.993715
45.716503	1299.545838	18.998733
45.495539	1303.556712	19.003751
45.608670	1290.171289	19.008768
45.551600	1308.468201	19.013786
45.871000	1287.476742	19.018803
45.848141	1299.993208	19.023821
45.493224	1298.249822	19.028839
45.573216	1303.681286	19.033856
45.855676	1304.189735	19.038874
45.814138	1303.180196	19.043891
46.139392	1301.267794	19.048909
45.997897	1297.064369	19.053927
46.268954	1289.808170	19.058944
46.180297	1297.089942	19.063962
45.987018	1295.330857	19.068979
46.016563	1296.039629	19.073997
45.925125	1294.346740	19.079015
46.317194	1299.483461	19.084032
45.948487	1297.739066	19.089050
46.668469	1305.115846	19.094067
46.336510	1310.261157	19.099085
46.527087	1321.362166	19.104103
46.727542	1309.500010	19.109120
46.788780	1311.605025	19.114138
46.430103	1323.151313	19.119155
46.520983	1315.358267	19.124173
46.384366	1320.855019	19.129191
46.978773	1304.870010	19.134208
46.851530	1310.646166	19.139226
46.690285	1312.164127	19.144243
46.937968	1309.323373	19.149261
46.630813	1312.965817	19.154279
46.813990	1309.791123	19.159296
46.891897	1313.834362	19.164314
46.918696	1316.828364	19.169331
47.238092	1316.800888	19.174349
47.149851	1320.257770	19.179367
47.228679	1320.962026	19.184384
47.251059	1323.603268	19.189402
47.359570	1335.922581	19.194419
47.282442	1335.111085	19.199437
47.070113	1334.462651	19.204455
47.278605	1331.542788	19.209472
47.190532	1337.227647	19.214490
47.561720	1337.308872	19.219507
47.397630	1334.895143	19.224525
46.922033	1346.383910	19.229543
47.462113	1341.992305	19.234560
47.490592	1362.365098	19.239578
47.577102	1360.963234	19.244595
47.949581	1345.208402	19.249613
47.880808	1360.184123	19.254631
48.042380	1347.412810	19.259648
48.046854	1353.152693	19.264666
48.311214	1348.819794	19.269683
48.096108	1350.087368	19.274701
47.644778	1355.371197	19.279719
47.993909	1352.959611	19.284736
47.887129	1356.507749	19.289754
48.215003	1359.410702	19.294771
48.452250	1350.935287	19.299789
48.462811	1357.330633	19.304807
48.506845	1358.352733	19.309824
47.902590	1357.124689	19.314842
48.283555	1358.394132	19.319859
48.647150	1362.762132	19.324877
48.666220	1374.161277	19.329895
48.731337	1365.087804	19.334912
48.917704	1374.349663	19.339930
48.871740	1372.356195	19.344947
48.835242	1373.239356	19.349965
49.111018	1380.069944	19.354983
48.741459	1363.982502	19.360000
48.971760	1369.188611	19.365018
48.861186	1367.921573	19.370035
49.068808	1372.730426	19.375053
49.318433	1369.860958	19.380071
49.182073	1366.073283	19.385088
48.850542	1373.134124	19.390106
48.927235	1375.331414	19.395123
49.290702	1365.633976	19.400141
49.298738	1378.574878	19.405159
49.634419	1371.213910	19.410176
49.410027	1376.512906	19.415194
49.137914	1365.437504	19.420211
49.629477	1367.652251	19.425229
49.487464	1369.186158	19.430247
49.346467	1368.899002	19.435264
49.455842	1382.060815	19.440282
49.551062	1391.459951	19.445299
50.026950	1395.737892	19.450317
50.057819	1395.938375	19.455335
50.169579	1389.792539	19.460352
49.971887	1393.642019	19.465370
50.120875	1394.070266	19.470387
50.418486	1384.171631	19.475405
49.772385	1385.165483	19.480423
49.894015	1389.211399	19.485440
50.383833	1392.568827	19.490458
50.390457	1392.514308	19.495475
50.093062	1396.079509	19.500493
50.177212	1397.688660	19.505511
50.455783	1386.319221	19.510528
50.137528	1389.272285	19.515546
49.985481	1397.188818	19.520563
50.175238	1380.430452	19.525581
50.259636	1400.359080	19.530599
50.612534	1406.672740	19.535616
50.785491	1411.329210	19.540634
50.421487	1409.142257	19.545651
50.609389	1406.572728	19.550669
50.942009	1411.109665	19.555687
50.612701	1412.436050	19.560704
50.772380	1406.661445	19.565722
50.874956	1416.958858	19.570739
50.894610	1408.589879	19.575757
50.793139	1420.115118	19.580775
50.857117	1418.880860	19.585792
51.168770	1427.296415	19.590810
51.266249	1434.318887	19.595827
51.393367	1436.369478	19.600845
51.126137	1425.782431	19.605863
51.036007	1433.869222	19.610880
51.250038	1436.556381	19.615898
51.010160	1434.552072	19.620915
51.125572	1426.660484	19.625933
51.212336	1437.152875	19.630951
51.496722	1448.577032	19.635968
51.649410	1451.870195	19.640986
51.589987	1461.186147	19.646003
51.892374	1458.204307	19.651021
51.419714	1455.245308	19.656039
51.881016	1461.122385	19.661056
51.998492	1446.325513	19.666074
51.751450	1458.005986	19.671091
51.959931	1445.069509	19.676109
51.977973	1455.957622	19.681127
52.207832	1457.351586	19.686144
51.980784	1444.864774	19.691162
51.987147	1451.103015	19.696179
52.622909	1472.599533	19.701197
52.893731	1472.885736	19.706215
52.449598	1467.602757	19.711232
52.525399	1446.784738	19.716250
52.175120	1450.708480	19.721267
52.978815	1460.252969	19.726285
53.062452	1466.311925	19.731303
52.580597	1455.439537	19.736320
52.845992	1450.115522	19.741338
52.676187	1463.611198	19.746355
52.965270	1463.935583	19.751373
52.822103	1469.695334	19.756391
52.793036	1481.584885	19.761408
52.945870	1475.180157	19.766426
52.702421	1482.451391	19.771443
53.163988	1471.343744	19.776461
52.828704	1473.709331	19.781479
53.159444	1473.462337	19.786496
53.135231	1469.016546	19.791514
52.508491	1472.320612	19.796531
52.907143	1482.063877	19.801549
52.875601	1500.612634	19.806567
53.116418	1496.554766	19.811584
53.292873	1487.164093	19.816602
52.967065	1497.518782	19.821619
53.676799	1508.340260	19.826637
54.069257	1509.308121	19.831655
53.964564	1518.296632	19.836672
54.173648	1505.012876	19.841690
53.905708	1511.019287	19.846707
54.289762	1502.713450	19.851725
54.315421	1495.590050	19.856743
53.893522	1492.654700	19.861760
54.272303	1482.920100	19.866778
54.189660	1492.492150	19.871795
54.255052	1482.446578	19.876813
54.392400	1482.213914	19.881831
54.231104	1497.929998	19.886848
54.784968	1495.944113	19.891866
54.673544	1492.521762	19.896883
54.702379	1486.956854	19.901901
54.265627	1488.710230	19.906919
54.334070	1482.182939	19.911936
54.356686	1485.849814	19.916954
54.709659	1505.926095	19.921971
54.781213	1502.582551	19.926989
54.797313	1503.031491	19.932007
54.249619	1498.326366	19.937024
54.853337	1501.609277	19.942042
54.887736	1501.380018	19.947059
55.069475	1495.750275	19.952077
55.026473	1511.135525	19.957095
54.658466	1506.033188	19.962112
55.086058	1501.949395	19.967130
54.772237	1515.262403	19.972147
55.079500	1513.870338	19.977165
55.311950	1529.329484	19.982183
55.165638	1529.617516	19.987200
55.427830	1523.224148	19.992218
55.230174	1523.570667	19.997235
55.147240	1526.455556	20.002253
55.144285	1527.598592	20.007271
55.176232	1530.348829	20.012288
55.419224	1540.760153	20.017306
55.533173	1548.414430	20.022323
55.941513	1545.636989	20.027341
56.025856	1547.719500	20.032359
56.347287	1543.652226	20.037376
56.243152	1542.112770	20.042394
56.381416	1547.535236	20.047411
56.056225	1551.297302	20.052429
56.146938	1536.791704	20.057447
56.152948	1540.530603	20.062464
56.447208	1537.994990	20.067482
56.384177	1534.640837	20.072499
56.177061	1539.795178	20.077517
56.488076	1533.040750	20.082535
56.169440	1533.743781	20.087552
56.306773	1536.963611	20.092570
56.485876	1533.830538	20.097587
56.305691	1544.774815	20.102605
56.495909	1546.777725	20.107623
56.574064	1565.085405	20.112640
57.126222	1567.593706	20.117658
57.028086	1561.751893	20.122675
56.750012	1560.438335	20.127693
57.249054	1562.702437	20.132711
56.707354	1565.235876	20.137728
57.210549	1552.351267	20.142746
57.180034	1555.376324	20.147763
57.322020	1561.050682	20.152781
57.415427	1555.055971	20.157799
57.332706	1562.217005	20.162816
57.301758	1548.361509	20.167834
57.498943	1559.310157	20.172851
57.848758	1566.044082	20.177869
57.595890	1560.497764	20.182887
57.293160	1555.896497	20.187904
57.698258	1559.607979	20.192922
57.399839	1559.641979	20.197939
57.439406	1569.816745	20.202957
58.042291	1586.546878	20.207975
57.587713	1583.954276	20.212992
58.049941	1580.313204	20.218010
57.414022	1588.687017	20.223027
57.448509	1583.578797	20.228045
58.064234	1581.898856	20.233063
58.125270	1603.443989	20.238080
58.464136	1596.584213	20.243098
58.402456	1598.222399	20.248115
58.637090	1612.103349	20.253133
58.632600	1603.914765	20.258151
58.456432	1606.179856	20.263168
58.538591	1600.660259	20.268186
58.441292	1602.124107	20.273203
57.990454	1597.823604	20.278221
58.752203	1597.446385	20.283239
58.171507	1599.922783	20.288256
58.266026	1607.741060	20.293274
58.757749	1608.399977	20.298291
58.944854	1623.048897	20.303309
59.067262	1630.679802	20.308327
58.551576	1632.063623	20.313344
58.944469	1630.042824	20.318362
58.926014	1632.681002	20.323379
59.024357	1625.154908	20.328397
58.889367	1618.826500	20.333415
59.181784	1633.455876	20.338432
59.640866	1636.969619	20.343450
59.647479	1645.915617	20.348467
59.904703	1641.987709	20.353485
59.799682	1622.974387	20.358503
59.609943	1624.155978	20.363520
59.659076	1619.903861	20.368538
59.539445	1632.890072	20.373555
59.783408	1632.391494	20.378573
60.077178	1640.039905	20.383591
59.725560	1647.040863	20.388608
59.879814	1641.226002	20.393626
59.887991	1638.921112	20.398643
59.734191	1640.920788	20.403661
60.208341	1632.689228	20.408679
60.116416	1636.872592	20.413696
60.221810	1631.923736	20.418714
60.366311	1643.691694	20.423731
60.453040	1656.828833	20.428749
60.715164	1653.364071	20.433767
60.629912	1666.225031	20.438784
60.487385	1668.128279	20.443802
61.026551	1668.420044	20.448819
60.926870	1673.147433	20.453837
60.978861	1662.324348	20.458855
61.121051	1656.694400	20.463872
60.846821	1653.666602	20.468890
61.205977	1663.753793	20.473907
61.151914	1663.197472	20.478925
61.010587	1657.782082	20.483943
61.296176	1661.698389	20.488960
61.068040	1662.270567	20.493978
61.305575	1655.603275	20.498995
61.128445	1664.918724	20.504013
61.097733	1660.852601	20.509031
60.864594	1662.451214	20.514048
61.483002	1668.468005	20.519066
61.296027	1677.803929	20.524083
61.229353	1683.441384	20.529101
61.229583	1682.062395	20.534119
61.211184	1690.573645	20.539136
61.516339	1690.425308	20.544154
62.010376	1698.446514	20.549171
62.239681	1703.965309	20.554189
62.099657	1704.921410	20.559207
62.155014	1701.264764	20.564224
62.470372	1694.395988	20.569242
62.916404	1695.159855	20.574259
62.576869	1693.808518	20.579277
62.530386	1673.602577	20.584295
62.045630	1670.623333	20.589312
62.820750	1685.228092	20.594330
62.770866	1687.861703	20.599347
62.589956	1689.767774	20.604365
62.550753	1690.282134	20.609383
62.816796	1701.649348	20.614400
62.641707	1703.245238	20.619418
62.627538	1697.096812	20.624435
62.900386	1695.924691	20.629453
62.718574	1702.627828	20.634471
62.556515	1700.399928	20.639488
62.713351	1708.243261	20.644506
62.782383	1698.831331	20.649523
62.839990	1716.334463	20.654541
63.239568	1703.099797	20.659559
63.170231	1710.640667	20.664576
63.183736	1708.584252	20.669594
63.130112	1713.992462	20.674611
62.756241	1715.884396	20.679629
63.216552	1722.515969	20.684647
63.106158	1739.688666	20.689664
63.602968	1732.122578	20.694682
63.687112	1736.108136	20.699699
63.345017	1742.224003	20.704717
64.183026	1731.556214	20.709735
63.520189	1733.644622	20.714752
63.855904	1750.211374	20.719770
64.164904	1754.780480	20.724787
64.233851	1763.287632	20.729805
64.508145	1754.951430	20.734823
64.253139	1753.665824	20.739840
64.484451	1757.098285	20.744858
64.494370	1759.220811	20.749875
64.277594	1764.218926	20.754893
64.550927	1765.931203	20.759911
64.171065	1760.341476	20.764928
64.819067	1761.073901	20.769946
64.831301	1749.799349	20.774963
64.486858	1758.683294	20.779981
64.612733	1758.960510	20.784999
64.683785	1765.182478	20.790016
64.667373	1780.623781	20.795034
65.168701	1780.921439	20.800051
64.943832	1778.157341	20.805069
65.259039	1775.877216	20.810087
65.030209	1775.048292	20.815104
65.084775	1783.238949	20.820122
65.279424	1777.679693	20.825139
65.567154	1795.929733	20.830157
65.886730	1800.948497	20.835175
66.065291	1790.790455	20.840192
65.834726	1769.483258	20.845210
66.294012	1765.350289	20.850227
65.665895	1777.311214	20.855245
65.692502	1770.645160	20.860263
65.745431	1777.191854	20.865280
65.978841	1783.274937	20.870298
66.243250	1782.953058	20.875315
66.364523	1789.015732	20.880333
65.909335	1781.831380	20.885351
65.958357	1785.289072	20.890368
65.932239	1791.062262	20.895386
66.149836	1787.932619	20.900403
66.219312	1788.114473	20.905421
66.537322	1785.575127	20.910439
66.307443	1790.692058	20.915456
66.420672	1812.841559	20.920474
66.478774	1811.822790	20.925491
66.433425	1811.798453	20.930509
66.489899	1810.827275	20.935527
66.691381	1809.779870	20.940544
67.042751	1828.405054	20.945562
67.283677	1830.150785	20.950579
67.314444	1836.975514	20.955597
67.072192	1822.360574	20.960615
67.259867	1814.716347	20.965632
67.523507	1833.042761	20.970650
67.689623	1827.891887	20.975667
67.509615	1823.066309	20.980685
67.450541	1816.066431	20.985703
67.568663	1826.080785	20.990720
67.735590	1826.578836	20.995738
67.653712	1832.256576	21.000755
67.777827	1828.147374	21.005773
67.649427	1830.865816	21.010791
67.492799	1834.017856	21.015808
67.507623	1834.028333	21.020826
67.633566	1832.033295	21.025843
67.714499	1837.313293	21.030861
67.783153	1852.394266	21.035879
68.208115	1853.413892	21.040896
68.222669	1858.240314	21.045914
68.612423	1868.098788	21.050931
68.618964	1862.650846	21.055949
68.261567	1858.727063	21.060967
68.551713	1859.966501	21.065984
68.421499	1855.404570	21.071002
68.415388	1854.307430	21.076019
68.474613	1873.066511	21.081037
68.576090	1882.588013	21.086055
68.692654	1876.046774	21.091072
68.692401	1886.540354	21.096090
68.995757	1888.087017	21.101107
68.878850	1889.626526	21.106125
69.112436	1896.650081	21.111143
69.584439	1894.894657	21.116160
69.003875	1904.740117	21.121178
69.701455	1899.790507	21.126195
69.709271	1910.822506	21.131213
69.625216	1910.163546	21.136231
69.795264	1900.786277	21.141248
69.870698	1904.877373	21.146266
70.174629	1896.725845	21.151283
69.856225	1906.113910	21.156301
69.894634	1902.358873	21.161319
70.146785	1891.924220	21.166336
69.731305	1897.464566	21.171354
69.710435	1894.880134	21.176371
69.811748	1897.247231	21.181389
70.020235	1899.089541	21.186407
70.103877	1915.629419	21.191424
70.016102	1921.339664	21.196442
70.295015	1920.674686	21.201459
70.159665	1916.975102	21.206477
70.241715	1927.077184	21.211495
70.776914	1930.225672	21.216512
70.898706	1952.787438	21.221530
71.012414	1939.988439	21.226547
70.731043	1949.932514	21.231565
71.259020	1951.702995	21.236583
71.334956	1960.136567	21.241600
71.045471	1947.816919	21.246618
71.411232	1940.028142	21.251635
71.334752	1941.536115	21.256653
71.680477	1949.870871	21.261671
71.594046	1931.725359	21.266688
71.450022	1941.095760	21.271706
71.660380	1934.066510	21.276723
71.747002	1938.875420	21.281741
71.738304	1934.184093	21.286759
71.677486	1940.505550	21.291776
71.540370	1939.908501	21.296794
72.071688	1942.271773	21.301811
71.849594	1938.219604	21.306829
71.814620	1933.478718	21.311847
71.900641	1936.709765	21.316864
72.013336	1944.111935	21.321882
71.627959	1945.245108	21.326899
71.958724	1951.000656	21.331917
71.820676	1964.027845	21.336935
71.741900	1963.286007	21.341952
71.999601	1971.050633	21.346970
72.185099	1975.683208	21.351987
72.450265	1982.203244	21.357005
72.556273	1979.460185	21.362023
73.231745	1971.922987	21.367040
72.697493	1978.501212	21.372058
72.991716	1975.662575	21.377075
73.160751	1972.808715	21.382093
72.754099	1978.212006	21.387111
73.445193	1986.903278	21.392128
73.342710	1999.574649	21.397146
73.546485	1989.251617	21.402163
73.569824	1990.620971	21.407181
73.830729	2000.108245	21.412199
73.797489	1995.748939	21.417216
73.590137	1993.853114	21.422234
73.505166	1992.670410	21.427251
73.749342	1995.630682	21.432269
73.705771	1991.616981	21.437287
73.878507	1989.488404	21.442304
73.938473	1996.507471	21.447322
74.152937	1998.806469	21.452339
74.272229	2001.997633	21.457357
74.187762	1988.045983	21.462375
74.194230	2001.773406	21.467392
74.015553	2002.186409	21.472410
74.234945	2004.251103	21.477427
74.480940	2017.259565	21.482445
74.424021	2017.278056	21.487463
74.778853	2017.245064	21.492480
74.542125	2014.870954	21.497498
74.463660	2011.579076	21.502515
74.691247	2014.362047	21.507533
74.666825	2013.106796	21.512551
75.014951	2023.066515	21.517568
75.310473	2032.390621	21.522586
75.650907	2036.566726	21.527603
75.609420	2033.518405	21.532621
75.448837	2028.531952	21.537639
75.655786	2027.474215	21.542656
75.197556	2028.255805	21.547674
75.395438	2034.852611	21.552691
75.401993	2030.446073	21.557709
75.138838	2032.813127	21.562727
75.560994	2024.936635	21.567744
75.544750	2036.619423	21.572762
75.670620	2045.045261	21.577779
75.854954	2046.667275	21.582797
75.510587	2059.423687	21.587815
75.849261	2044.882227	21.592832
75.859114	2065.312373	21.597850
76.147226	2067.861857	21.602867
76.224023	2066.451982	21.607885
76.091349	2075.353607	21.612903
76.656435	2058.103806	21.617920
76.863059	2068.177104	21.622938
76.665226	2057.929184	21.627955
76.698977	2060.073282	21.632973
76.692799	2084.125804	21.637991
77.277716	2081.103030	21.643008
77.290234	2098.342146	21.648026
76.993230	2090.779574	21.653043
77.564205	2082.286571	21.658061
77.244163	2090.649306	21.663079
77.480173	2081.296388	21.668096
77.459875	2092.105648	21.673114
77.532666	2082.030184	21.678131
77.777324	2075.266949	21.683149
77.389886	2086.916040	21.688167
77.617046	2088.206329	21.693184
77.801035	2095.225060	21.698202
77.703627	2083.844287	21.703219
77.557893	2077.381684	21.708237
77.617913	2082.582956	21.713255
77.678668	2081.396493	21.718272
77.590442	2098.480873	21.723290
77.426086	2101.892949	21.728307
78.042600	2109.664890	21.733325
77.817569	2128.364350	21.738343
78.255610	2132.566308	21.743360
78.664873	2144.716273	21.748378
78.668485	2138.924705	21.753395
78.203227	2134.074024	21.758413
78.602414	2135.798301	21.763431
78.768736	2136.668857	21.768448
78.896970	2143.794123	21.773466
79.274764	2158.795663	21.778483
79.211211	2158.180841	21.783501
78.690110	2159.808552	21.788519
79.496236	2152.310900	21.793536
79.622540	2142.981343	21.798554
79.410926	2151.522894	21.803571
79.798529	2143.487621	21.808589
79.624254	2148.984178	21.813607
79.737203	2144.554735	21.818624
79.831293	2145.767912	21.823642
79.818478	2147.171311	21.828659
79.898789	2144.722575	21.833677
79.637184	2138.416852	21.838695
79.939030	2153.925698	21.843712
80.242428	2162.693197	21.848730
79.910038	2174.147573	21.853747
80.339028	2168.232959	21.858765
80.017302	2174.822350	21.863783
79.920063	2166.521710	21.868800
80.618361	2171.547889	21.873818
80.331125	2185.709363	21.878835
80.800159	2187.167138	21.883853
81.148020	2190.837171	21.888871
80.597635	2197.563161	21.893888
80.746489	2191.890980	21.898906
80.928176	2183.846722	21.903923
81.283539	2187.480870	21.908941
81.128680	2190.282385	21.913959
81.046645	2192.201517	21.918976
81.132206	2191.228946	21.923994
81.305416	2205.486013	21.929011
81.367177	2205.924705	21.934029
81.643646	2217.448423	21.939047
81.518348	2206.460097	21.944064
81.755782	2204.962082	21.949082
81.416908	2207.994231	21.954099
81.730607	2212.202944	21.959117
81.959672	2224.021239	21.964135
82.314330	2225.862917	21.969152
82.488669	2221.398650	21.974170
82.113934	2225.796605	21.979187
82.131227	2228.997379	21.984205
82.307801	2236.313981	21.989223
82.712785	2228.597872	21.994240
82.516922	2230.007685	21.999258
82.336207	2227.852055	22.004275
82.825674	2218.819384	22.009293
82.392081	2231.021736	22.014311
82.370573	2228.213281	22.019328
82.245537	2241.289141	22.024346
82.678405	2257.566669	22.029363
83.091467	2245.459342	22.034381
83.064407	2250.333376	22.039399
83.682878	2267.058567	22.044416
83.644917	2271.495624	22.049434
83.349016	2271.971067	22.054451
83.607043	2267.140290	22.059469
83.590015	2275.471714	22.064487
83.839393	2274.041265	22.069504
83.969030	2281.788094	22.074522
83.719948	2281.003326	22.079539
84.314362	2269.719861	22.084557
84.028102	2278.711774	22.089575
84.126522	2276.828276	22.094592
83.925483	2272.977891	22.099610
83.972831	2280.860615	22.104627
84.055249	2275.697395	22.109645
84.289563	2286.861628	22.114663
84.615011	2294.738931	22.119680
84.525580	2292.629044	22.124698
84.507563	2292.461588	22.129715
84.637133	2289.437087	22.134733
84.944166	2300.574227	22.139751
84.979740	2304.633749	22.144768
85.142500	2306.439038	22.149786
85.220373	2324.908495	22.154803
85.392756	2314.953102	22.159821
85.225610	2319.227237	22.164839
85.437973	2318.695690	22.169856
85.888382	2308.031101	22.174874
85.414506	2320.381804	22.179891
85.642827	2314.024989	22.184909
85.628450	2309.782596	22.189927
85.228287	2320.761596	22.194944
86.008992	2336.574763	22.199962
86.059836	2345.593124	22.204979
86.376963	2342.747708	22.209997
86.079744	2345.637688	22.215015
86.196141	2344.155350	22.220032
86.196924	2344.022838	22.225050
85.961572	2354.692160	22.230067
86.200484	2349.820152	22.235085
86.058524	2359.745904	22.240103
86.091782	2355.821151	22.245120
86.518518	2354.015923	22.250138
86.456535	2373.990520	22.255155
86.852005	2371.849312	22.260173
87.250932	2382.896452	22.265191
87.169154	2390.496352	22.270208
87.190322	2380.173123	22.275226
87.355380	2386.368046	22.280243
87.266229	2381.556576	22.285261
87.200294	2389.122449	22.290279
87.339050	2399.591532	22.295296
87.815426	2401.796153	22.300314
87.765973	2399.064610	22.305331
87.920056	2398.554759	22.310349
87.863286	2401.258979	22.315367
87.901331	2404.440773	22.320384
88.305820	2397.311684	22.325402
87.751116	2399.377018	22.330419
87.935592	2413.995437	22.335437
88.204931	2420.982072	22.340455
88.186323	2427.767373	22.345472
88.504587	2415.598948	22.350490
88.447378	2431.157624	22.355507
88.567614	2427.989378	22.360525
88.649337	2422.936684	22.365543
88.967164	2434.952751	22.370560
89.594394	2436.979246	22.375578
89.292201	2419.441224	22.380595
89.527007	2413.809244	22.385613
89.334572	2416.260016	22.390631
89.334723	2411.832290	22.395648
89.411492	2424.173076	22.400666
89.473333	2431.728541	22.405683
89.446252	2445.196423	22.410701
89.521430	2440.618144	22.415719
89.668214	2441.024669	22.420736
89.713189	2437.189598	22.425754
89.872345	2447.065359	22.430771
89.922697	2439.962987	22.435789
89.905782	2447.211965	22.440807
90.283806	2463.936905	22.445824
90.395635	2464.967449	22.450842
90.359695	2467.712620	22.455859
90.648552	2463.041103	22.460877
90.465996	2459.632797	22.465895
90.647744	2461.321528	22.470912
90.478597	2459.110417	22.475930
90.734589	2467.563535	22.480947
90.571080	2470.754629	22.485965
90.940664	2482.122000	22.490983
91.076394	2481.327807	22.496000
91.114037	2481.252676	22.501018
91.488076	2485.638264	22.506035
91.244226	2490.621860	22.511053
91.574047	2486.998066	22.516071
91.543002	2515.877424	22.521088
91.966495	2504.330070	22.526106
91.683243	2505.999678	22.531123
91.559198	2502.755835	22.536141
91.948665	2509.859510	22.541159
91.491288	2501.586382	22.546176
92.269982	2514.843651	22.551194
92.078761	2519.351970	22.556211
92.100499	2529.489030	22.561229
92.238465	2534.703545	22.566247
92.295767	2529.310618	22.571264
92.535281	2523.037199	22.576282
92.403642	2545.459276	22.581299
92.836833	2552.369956	22.586317
92.849276	2552.226159	22.591335
92.959824	2559.884556	22.596352
93.174365	2554.587069	22.601370
92.813441	2557.625865	22.606387
92.494849	2553.414999	22.611405
93.226797	2560.733635	22.616423
93.332221	2571.368965	22.621440
93.560061	2573.261985	22.626458
93.465939	2576.890450	22.631475
93.271967	2580.483966	22.636493
93.432531	2584.984872	22.641511
93.315387	2604.504377	22.646528
93.626053	2609.045040	22.651546
93.915005	2609.539895	22.656563
94.391501	2626.934514	22.661581
94.410483	2637.450788	22.666599
94.639790	2631.279914	22.671616
94.510429	2624.123392	22.676634
94.444554	2631.348506	22.681651
95.074779	2626.137769	22.686669
95.425545	2612.714360	22.691687
95.141085	2617.003674	22.696704
95.183176	2612.310573	22.701722
95.303061	2617.550020	22.706739
94.784236	2624.375404	22.711757
95.205220	2608.877019	22.716775
95.015253	2615.578609	22.721792
95.322584	2624.655015	22.726810
95.492891	2619.083509	22.731827
95.314127	2622.624169	22.736845
95.602406	2623.185406	22.741863
95.624177	2636.251321	22.746880
95.671245	2634.221135	22.751898
95.736773	2637.827912	22.756915
96.013270	2648.483994	22.761933
96.311562	2640.143645	22.766951
95.951349	2637.899138	22.771968
96.648495	2646.842275	22.776986
96.375662	2661.876104	22.782003
96.237150	2664.463693	22.787021
96.589355	2663.351744	22.792039
96.546054	2672.902519	22.797056
96.907893	2661.932751	22.802074
96.702040	2660.623645	22.807091
96.476722	2677.717297	22.812109
97.275047	2679.982290	22.817127
96.992951	2686.594101	22.822144
97.520982	2683.482249	22.827162
97.232844	2684.000678	22.832179
97.240052	2685.988026	22.837197
97.417236	2693.396246	22.842215
97.561628	2702.447563	22.847232
97.648886	2701.515729	22.852250
97.647442	2703.485489	22.857267
97.740964	2718.468639	22.862285
98.196387	2724.779431	22.867303
98.023861	2728.884073	22.872320
98.154592	2728.475686	22.877338
98.375276	2737.635073	22.882355
98.290508	2738.588937	22.887373
98.827170	2725.707747	22.892391
98.540010	2750.357218	22.897408
98.952038	2753.001127	22.902426
99.415521	2759.449543	22.907443
98.957258	2745.426101	22.912461
99.473490	2749.669686	22.917479
99.511295	2750.771738	22.922496
99.591813	2750.705710	22.927514
99.456404	2754.353264	22.932531
99.319211	2756.864915	22.937549
99.564690	2746.162540	22.942567
99.621323	2751.522337	22.947584
99.298256	2748.969051	22.952602
99.883540	2760.318796	22.957619
99.999641	2774.844005	22.962637
100.020781	2770.138345	22.967655
100.003958	2779.341043	22.972672
100.123543	2775.563717	22.977690
100.283770	2785.026055	22.982707
100.195075	2797.468605	22.987725
100.497643	2797.055555	22.992743
100.440021	2805.308331	22.997760
100.488425	2796.972100	23.002778
100.792120	2802.861537	23.007795
100.846656	2816.907175	23.012813
100.987636	2817.816427	23.017831
100.996597	2822.713412	23.022848
101.101956	2819.159217	23.027866
101.232796	2817.466291	23.032883
101.211108	2831.908848	23.037901
101.439702	2829.531615	23.042919
101.921394	2844.485995	23.047936
101.822711	2849.743759	23.052954
101.893137	2845.910950	23.057971
102.007072	2837.823295	23.062989
102.049462	2829.327025	23.068007
101.900285	2836.770336	23.073024
102.093038	2840.423623	23.078042
102.549740	2845.052072	23.083059
102.637053	2862.835746	23.088077
102.733414	2851.616837	23.093095
102.908685	2854.092477	23.098112
102.674349	2868.890092	23.103130
103.023393	2851.240786	23.108147
103.047196	2853.613766	23.113165
102.693799	2851.825801	23.118183
103.172061	2868.942647	23.123200
103.326992	2883.228348	23.128218
103.571490	2877.919790	23.133235
103.280237	2885.934399	23.138253
103.957578	2885.352535	23.143271
103.781064	2879.244760	23.148288
103.534645	2882.919090	23.153306
103.686888	2894.027046	23.158323
103.587820	2909.248641	23.163341
104.359804	2904.587005	23.168359
104.204699	2906.987847	23.173376
104.000576	2903.914202	23.178394
104.605823	2912.792879	23.183411
104.707201	2936.024996	23.188429
104.814056	2919.218134	23.193447
105.180275	2924.539249	23.198464
104.881360	2934.612842	23.203482
104.854721	2931.580994	23.208499
104.551182	2929.731605	23.213517
104.911788	2930.025948	23.218535
105.272739	2947.167446	23.223552
105.143050	2947.708554	23.228570
105.509826	2951.704033	23.233587
105.290327	2950.722107	23.238605
105.410024	2954.639280	23.243623
105.732619	2976.637692	23.248640
105.765616	2976.449662	23.253658
106.416337	2962.827800	23.258675
106.214451	2975.379623	23.263693
106.147424	2970.359403	23.268711
106.521999	2976.509286	23.273728
106.362634	2994.056916	23.278746
106.557481	2993.957307	23.283763
106.533117	2993.434193	23.288781
106.405973	2996.367230	23.293799
106.941937	3000.967599	23.298816
107.201688	3013.494916	23.303834
107.415055	3021.910748	23.308851
107.458425	3020.439724	23.313869
107.356597	3014.017289	23.318887
107.410079	3029.104770	23.323904
107.678382	3023.034998	23.328922
107.737712	3015.520707	23.333939
107.681137	3025.310444	23.338957
107.766744	3015.926804	23.343975
107.877924	3021.697950	23.348992
108.001037	3037.178579	23.354010
108.232151	3039.617146	23.359027
107.951161	3040.349087	23.364045
108.308414	3038.166410	23.369063
108.598626	3040.889294	23.374080
108.333245	3037.137132	23.379098
108.839624	3041.890455	23.384115
108.639237	3053.577326	23.389133
108.674955	3062.705711	23.394151
109.264297	3053.805411	23.399168
109.307149	3058.075430	23.404186
109.026676	3054.991554	23.409203
109.149525	3055.177736	23.414221
109.372982	3063.307966	23.419239
109.429954	3075.052621	23.424256
109.252189	3072.934302	23.429274
109.561935	3077.655126	23.434291
109.511109	3084.928577	23.439309
109.671846	3088.040892	23.444327
110.052719	3101.928636	23.449344
110.318916	3108.202747	23.454362
110.424890	3103.856214	23.459379
110.243285	3106.848246	23.464397
110.502131	3124.618097	23.469415
111.036831	3117.010815	23.474432
110.812869	3122.376535	23.479450
110.920931	3117.919209	23.484467
110.501538	3125.335275	23.489485
110.418761	3122.510970	23.494503
111.147612	3135.732276	23.499520
111.294184	3145.790281	23.504538
111.485532	3143.074788	23.509555
111.732267	3149.995793	23.514573
111.673724	3145.113073	23.519591
111.893881	3156.213774	23.524608
112.107673	3171.917111	23.529626
111.738434	3169.487729	23.534643
112.307476	3173.830502	23.539661
112.077282	3166.421192	23.544679
112.421763	3172.900910	23.549696
111.904745	3176.661616	23.554714
112.306642	3185.723584	23.559731
112.486219	3195.858538	23.564749
112.924366	3195.086665	23.569767
112.977151	3192.111842	23.574784
112.687395	3212.716187	23.579802
112.996867	3204.736793	23.584819
113.426759	3222.186589	23.589837
113.250523	3219.569345	23.594855
113.950676	3209.149395	23.599872
113.935048	3206.336715	23.604890
114.278517	3202.442383	23.609907
114.106970	3207.768407	23.614925
113.993315	3211.090739	23.619943
113.992975	3215.342271	23.624960
113.784142	3235.997166	23.629978
114.387764	3229.581597	23.634995
114.529619	3226.195227	23.640013
114.328737	3233.514194	23.645031
114.482180	3237.962718	23.650048
114.544687	3255.109946	23.655066
114.435181	3258.261209	23.660083
114.674178	3256.497749	23.665101
114.849653	3265.216271	23.670119
115.086141	3272.962674	23.675136
115.095708	3287.558538	23.680154
115.698313	3286.391787	23.685171
115.566188	3288.369333	23.690189
115.490122	3286.020537	23.695207
115.816856	3295.069013	23.700224
115.786837	3307.562747	23.705242
115.960806	3306.891968	23.710259
115.877698	3308.148593	23.715277
115.941993	3306.320800	23.720295
116.191256	3313.544465	23.725312
116.454077	3326.374514	23.730330
116.807677	3324.470115	23.735347
116.868123	3329.700087	23.740365
116.735296	3331.153825	23.745383
116.984087	3329.057436	23.750400
117.169166	3339.747099	23.755418
116.847411	3326.809761	23.760435
116.966489	3333.476127	23.765453
117.033200	3344.143191	23.770471
117.828282	3342.583511	23.775488
117.277974	3351.086834	23.780506
117.586295	3355.902638	23.785523
117.749659	3362.757802	23.790541
117.738338	3378.278592	23.795559
117.840130	3376.956252	23.800576
117.967216	3389.851665	23.805594
118.568306	3386.602073	23.810611
118.388788	3391.392843	23.815629
118.463846	3397.343323	23.820647
119.173968	3398.893070	23.825664
118.811834	3393.988114	23.830682
118.712965	3397.674294	23.835699
119.132827	3404.628410	23.840717
119.624708	3414.692771	23.845735
119.447580	3417.482162	23.850752
119.361094	3414.582641	23.855770
119.564753	3411.003556	23.860787
119.801362	3413.813747	23.865805
119.582393	3410.458271	23.870823
119.957019	3413.565747	23.875840
119.990440	3427.933923	23.880858
120.136659	3439.781700	23.885875
120.287318	3430.558149	23.890893
120.349681	3436.447495	23.895911
120.366829	3433.954763	23.900928
120.283241	3443.865711	23.905946
120.632201	3447.191810	23.910963
120.793302	3460.075666	23.915981
120.934946	3459.258417	23.920999
121.339455	3440.034435	23.926016
121.125750	3463.575095	23.931034
121.378918	3470.274290	23.936051
121.582810	3470.937067	23.941069
121.744085	3475.561178	23.946087
122.049530	3476.946691	23.951104
121.935447	3474.272390	23.956122
121.585622	3471.259206	23.961139
121.907393	3490.897552	23.966157
122.078794	3501.576815	23.971175
122.674311	3497.520087	23.976192
122.417731	3498.582801	23.981210
122.377597	3512.697377	23.986227
122.840549	3523.104016	23.991245
123.099690	3522.779774	23.996263
123.165533	3523.637637	24.001280
123.223238	3523.016513	24.006298
123.257717	3527.357383	24.011315
123.266347	3522.864939	24.016333
123.226213	3526.500971	24.021351
123.555634	3521.646119	24.026368
123.506523	3542.166030	24.031386
123.515559	3541.139021	24.036403
123.616657	3544.847753	24.041421
123.768584	3546.569638	24.046439
123.991945	3557.919427	24.051456
124.284531	3570.060121	24.056474
124.646502	3557.218164	24.061491
124.620744	3564.396375	24.066509
124.559444	3568.225082	24.071527
124.859460	3565.934476	24.076544
124.960111	3576.315492	24.081562
125.085615	3587.892001	24.086579
125.310576	3581.503702	24.091597
125.135375	3580.000382	24.096615
125.274027	3580.468168	24.101632
125.567372	3588.742410	24.106650
125.570469	3587.829946	24.111667
125.698120	3598.323550	24.116685
125.676390	3609.850405	24.121703
126.038024	3609.664858	24.126720
126.294618	3613.374645	24.131738
125.834014	3610.318717	24.136755
126.812573	3622.810296	24.141773
126.809948	3626.926564	24.146791
126.895971	3629.776016	24.151808
126.601790	3635.660970	24.156826
126.648544	3639.835834	24.161843
127.091790	3637.485044	24.166861
126.942897	3646.033318	24.171879
127.165011	3653.469658	24.176896
127.357137	3654.790767	24.181914
127.075909	3661.077708	24.186931
127.609109	3667.256789	24.191949
127.740726	3693.133241	24.196967
128.050770	3680.207751	24.201984
128.019789	3683.072271	24.207002
127.897884	3681.276586	24.212019
128.197112	3695.758246	24.217037
128.258484	3708.127561	24.222055
128.419758	3704.422456	24.227072
128.657864	3710.035188	24.232090
128.751325	3727.313763	24.237107
129.211227	3724.385935	24.242125
129.050575	3728.214363	24.247143
129.338036	3732.225523	24.252160
129.394243	3726.478911	24.257178
129.146193	3735.061602	24.262195
129.532379	3741.822250	24.267213
129.672486	3754.573868	24.272231
129.898879	3753.244726	24.277248
130.062740	3758.698596	24.282266
130.081124	3764.001525	24.287283
130.042690	3764.875635	24.292301
130.265590	3775.452356	24.297319
130.173392	3771.988700	24.302336
130.407393	3787.528459	24.307354
130.423779	3799.822779	24.312371
130.983392	3787.202386	24.317389
131.139675	3790.489110	24.322407
131.052321	3804.715422	24.327424
131.412700	3814.759451	24.332442
131.447993	3826.672096	24.337459
131.660457	3820.692813	24.342477
131.790855	3818.213959	24.347495
132.041596	3820.810546	24.352512
132.242536	3834.887840	24.357530
132.231920	3843.436773	24.362547
132.558472	3838.575971	24.367565
132.490912	3850.643520	24.372583
132.647225	3841.466224	24.377600
132.793093	3840.774550	24.382618
133.113580	3834.784758	24.387635
132.826426	3830.663381	24.392653
133.153404	3838.212877	24.397671
132.992119	3837.954087	24.402688
133.291559	3854.594715	24.407706
133.390456	3857.584230	24.412723
133.921156	3854.465453	24.417741
133.668719	3856.196667	24.422759
133.377313	3860.575730	24.427776
133.585844	3866.745460	24.432794
133.469655	3879.391881	24.437811
134.299375	3880.133989	24.442829
134.205979	3885.050355	24.447847
133.706981	3891.368125	24.452864
134.170966	3900.405007	24.457882
134.292584	3906.506219	24.462899
135.005585	3922.091456	24.467917
134.902082	3935.458725	24.472935
134.624168	3934.239650	24.477952
134.789290	3938.891687	24.482970
135.225384	3957.086111	24.487987
135.284485	3951.329507	24.493005
135.467515	3967.436017	24.498023
135.725109	3979.651873	24.503040
136.086432	3977.345358	24.508058
136.300616	3978.631495	24.513075
136.348457	3976.143378	24.518093
136.547607	3982.687049	24.523111
136.639758	3995.534678	24.528128
136.873254	3989.640441	24.533146
136.942790	3997.024928	24.538163
136.941004	4002.457317	24.543181
136.851403	4004.488289	24.548199
137.131648	4013.755837	24.553216
137.538747	4019.793703	24.558234
137.348780	4028.550554	24.563251
137.746120	4024.802318	24.568269
137.893963	4017.172829	24.573287
137.759757	4029.269811	24.578304
137.940802	4039.512325	24.583322
137.954865	4054.316424	24.588339
138.166102	4058.721436	24.593357
138.478803	4068.962407	24.598375
138.721784	4078.541949	24.603392
138.502458	4084.838337	24.608410
138.669828	4080.936516	24.613427
138.937043	4086.753149	24.618445
139.196496	4101.676897	24.623463
139.200961	4108.938995	24.628480
139.647879	4098.232866	24.633498
139.132734	4110.294522	24.638515
139.716955	4118.239654	24.643533
140.110331	4115.798723	24.648551
140.212682	4120.441643	24.653568
140.450734	4127.689476	24.658586
140.362747	4134.189529	24.663603
140.676509	4124.135376	24.668621
140.179991	4124.604221	24.673639
140.386130	4134.931260	24.678656
140.884455	4137.779726	24.683674
140.609647	4142.522403	24.688691
140.920031	4157.406704	24.693709
141.157346	4160.570410	24.698727
141.311204	4162.093206	24.703744
141.807022	4172.526667	24.708762
141.356599	4182.188971	24.713779
141.706464	4183.996883	24.718797
141.902903	4192.336991	24.723815
141.449055	4201.147635	24.728832
142.100008	4197.782824	24.733850
142.187111	4217.095521	24.738867
142.184170	4219.277153	24.743885
142.577587	4218.259700	24.748903
142.843604	4230.120908	24.753920
143.284105	4234.190417	24.758938
143.006900	4242.866265	24.763955
143.114724	4235.495420	24.768973
142.950249	4236.894186	24.773991
143.387269	4250.922424	24.779008
143.631334	4264.548299	24.784026
143.431972	4256.789699	24.789043
143.922127	4259.522673	24.794061
143.868753	4274.441610	24.799079
144.136741	4280.864200	24.804096
144.384006	4278.253460	24.809114
144.441411	4283.594654	24.814131
144.732020	4288.628098	24.819149
144.965183	4300.961604	24.824167
145.285144	4309.326723	24.829184
145.502663	4312.518788	24.834202
145.349832	4310.090275	24.839219
145.322938	4301.995484	24.844237
145.342689	4299.435945	24.849255
145.891710	4324.983185	24.854272
145.908951	4325.731869	24.859290
146.164607	4337.361192	24.864307
146.530692	4318.082291	24.869325
146.073612	4321.142661	24.874343
146.555172	4348.995092	24.879360
146.798138	4349.639194	24.884378
146.736358	4356.555040	24.889395
146.661020	4359.357134	24.894413
146.825941	4360.152266	24.899431
146.793522	4375.942330	24.904448
146.934260	4366.707223	24.909466
147.266920	4387.755734	24.914483
147.422355	4406.669765	24.919501
147.629109	4411.290192	24.924519
147.877998	4406.510771	24.929536
148.271804	4416.717218	24.934554
148.516086	4432.063395	24.939571
148.767445	4425.124640	24.944589
149.129250	4422.758024	24.949607
148.655044	4429.899083	24.954624
149.376160	4419.737156	24.959642
149.005568	4428.424475	24.964659
149.029682	4419.491569	24.969677
149.264280	4427.039914	24.974695
149.175274	4440.916627	24.979712
149.284241	4444.103522	24.984730
149.189570	4448.988676	24.989747
149.779505	4457.974666	24.994765
149.964670	4467.487664	24.999783
149.848566	4474.809714	25.004800
150.236246	4481.235835	25.009818
150.451167	4496.053212	25.014835
150.681235	4498.545801	25.019853
150.724197	4489.780369	25.024871
150.952755	4507.701493	25.029888
151.058088	4509.171903	25.034906
151.032011	4520.191839	25.039923
151.391885	4517.844450	25.044941
151.444145	4524.067142	25.049959
151.207753	4539.440901	25.054976
151.488161	4543.933109	25.059994
151.791805	4541.742821	25.065011
152.131848	4564.302290	25.070029
152.331008	4552.034186	25.075047
152.143738	4564.351264	25.080064
152.180195	4566.242730	25.085082
152.282830	4569.904089	25.090099
152.974218	4586.067727	25.095117
152.796682	4588.115612	25.100135
153.377129	4595.777469	25.105152
153.338784	4587.479168	25.110170
153.539595	4592.447769	25.115187
153.473308	4601.526529	25.120205
153.797560	4602.407340	25.125223
154.024757	4614.287470	25.130240
154.215114	4606.152406	25.135258
154.184004	4625.310342	25.140275
154.400267	4629.111841	25.145293
154.678523	4634.709142	25.150311
154.480845	4633.183982	25.155328
154.987054	4624.403178	25.160346
155.482665	4639.599928	25.165363
155.906838	4640.660880	25.170381
155.830440	4634.022429	25.175399
155.899324	4642.082747	25.180416
156.243593	4634.384540	25.185434
156.691214	4633.260778	25.190451
156.327284	4634.157199	25.195469
156.319365	4635.171793	25.200487
156.002140	4634.858359	25.205504
156.701473	4621.041461	25.210522
156.421216	4635.140639	25.215539
156.159394	4653.015155	25.220557
156.545493	4652.573281	25.225575
156.562571	4665.202659	25.230592
157.169476	4685.858461	25.235610
156.879909	4692.263842	25.240627
157.056046	4700.380085	25.245645
157.297659	4719.375717	25.250663
157.534028	4722.331347	25.255680
157.777920	4738.694206	25.260698
157.970983	4745.905103	25.265715
158.022133	4735.525355	25.270733
158.523038	4749.136858	25.275751
158.233044	4775.430862	25.280768
158.575080	4765.362483	25.285786
158.538657	4786.588865	25.290803
158.982355	4802.519810	25.295821
159.077543	4793.058002	25.300839
159.225404	4823.930147	25.305856
159.547695	4821.051980	25.310874
159.926307	4824.474725	25.315891
159.745582	4826.469473	25.320909
160.360391	4831.338964	25.325927
160.376328	4844.966072	25.330944
160.651649	4846.823536	25.335962
160.510763	4848.291274	25.340979
160.714243	4846.653136	25.345997
160.855470	4859.563180	25.351015
160.960466	4873.700411	25.356032
161.094678	4867.483610	25.361050
161.363688	4876.832261	25.366067
161.290054	4883.914288	25.371085
161.462005	4888.218300	25.376103
161.810995	4894.843135	25.381120
161.894288	4910.243190	25.386138
162.369112	4914.853575	25.391155
161.970897	4911.778239	25.396173
162.224764	4923.818554	25.401191
162.324766	4938.104965	25.406208
162.892565	4936.893034	25.411226
162.624857	4942.562806	25.416243
163.026409	4947.822208	25.421261
163.522707	4954.200023	25.426279
163.500284	4961.116284	25.431296
163.557812	4960.662431	25.436314
163.824943	4957.303582	25.441331
163.963233	4963.257359	25.446349
164.283656	4969.905608	25.451367
164.427685	4985.776051	25.456384
164.505839	4980.435962	25.461402
164.954994	4979.921136	25.466419
164.432753	4981.435631	25.471437
164.653652	4984.330584	25.476455
164.771967	5004.778739	25.481472
164.849046	5001.802993	25.486490
165.358390	5010.552448	25.491507
165.298305	5025.832883	25.496525
165.306542	5030.686389	25.501543
165.619565	5045.937160	25.506560
165.841787	5056.884044	25.511578
165.723697	5066.662366	25.516595
165.943054	5080.987124	25.521613
166.270760	5081.848483	25.526631
166.714087	5095.349267	25.531648
167.008602	5101.411338	25.536666
167.247544	5106.948621	25.541683
167.304748	5103.720279	25.546701
167.557228	5115.126488	25.551719
167.684546	5129.124715	25.556736
167.757295	5126.039146	25.561754
168.157611	5125.664492	25.566771
168.051155	5131.211366	25.571789
168.143243	5135.445803	25.576807
168.496936	5140.176112	25.581824
168.727666	5152.084453	25.586842
168.781043	5159.721291	25.591859
168.579212	5176.741046	25.596877
168.780815	5180.371337	25.601895
168.916967	5189.538820	25.606912
169.220055	5194.078163	25.611930
169.656900	5194.884658	25.616947
169.730501	5208.926031	25.621965
169.815339	5223.596963	25.626983
170.128451	5229.697217	25.632000
169.964445	5234.817487	25.637018
170.271594	5250.066188	25.642035
170.449610	5264.290206	25.647053
170.387584	5273.393891	25.652071
170.673003	5277.762399	25.657088
170.670808	5284.442053	25.662106
171.369699	5284.024068	25.667123
171.653746	5295.204520	25.672141
171.517238	5300.093259	25.677159
171.494169	5305.090599	25.682176
171.853182	5324.011770	25.687194
172.153124	5323.299210	25.692212
172.293876	5342.740484	25.697229
172.446098	5353.575341	25.702247
172.781756	5364.441619	25.707264
172.723384	5365.808169	25.712282
173.346303	5374.224466	25.717300
173.408766	5380.376420	25.722317
173.557519	5387.881714	25.727335
173.381356	5392.707209	25.732352
173.568181	5402.157309	25.737370
173.600718	5404.409317	25.742388
173.567791	5416.500923	25.747405
174.054363	5423.773715	25.752423
174.284838	5429.574406	25.757440
174.323289	5441.819056	25.762458
174.769020	5440.067393	25.767476
174.736371	5454.169689	25.772493
174.737436	5459.248540	25.777511
175.250075	5463.815300	25.782528
175.580079	5478.082110	25.787546
175.578146	5481.242262	25.792564
175.523402	5483.908748	25.797581
175.477150	5484.140224	25.802599
175.583387	5499.234179	25.807616
175.490063	5508.674290	25.812634
176.183083	5520.675039	25.817652
176.318155	5533.510763	25.822669
177.020086	5543.953965	25.827687
176.995037	5551.199140	25.832704
177.289975	5551.099721	25.837722
177.581782	5561.966632	25.842740
177.775029	5568.849546	25.847757
177.745131	5569.318375	25.852775
177.975194	5587.720127	25.857792
177.639686	5585.392484	25.862810
178.503890	5588.578790	25.867828
178.611711	5599.225000	25.872845
178.562933	5602.367214	25.877863
178.698799	5620.250206	25.882880
178.961709	5618.530147	25.887898
179.201821	5618.761233	25.892916
179.769740	5639.016997	25.897933
180.110483	5646.157911	25.902951
180.313540	5647.332266	25.907968
180.222699	5649.448840	25.912986
180.469050	5646.405601	25.918004
180.657119	5647.604384	25.923021
180.776532	5651.755773	25.928039
181.008183	5648.588559	25.933056
180.755912	5663.984678	25.938074
181.227064	5659.558584	25.943092
181.438258	5660.933692	25.948109
181.464817	5674.932244	25.953127
181.932030	5680.954997	25.958144
181.685904	5686.624795	25.963162
181.908758	5692.496202	25.968180
181.799182	5698.277321	25.973197
181.859238	5707.538983	25.978215
182.087137	5721.076929	25.983232
182.507381	5745.090032	25.988250
182.898523	5738.091137	25.993268
183.187614	5737.506516	25.998285
183.389718	5752.576285	26.003303
184.258340	5747.191819	26.008320
184.158771	5747.078063	26.013338
184.386354	5740.713852	26.018356
184.419814	5745.831931	26.023373
184.553104	5742.560065	26.028391
184.641805	5744.383545	26.033408
184.526855	5748.928138	26.038426
184.707051	5757.751296	26.043444
184.748225	5773.755234	26.048461
184.764890	5769.885986	26.053479
185.025125	5779.949857	26.058496
185.378702	5799.096487	26.063514
185.644774	5793.423871	26.068532
185.768560	5817.079181	26.073549
185.639585	5824.211224	26.078567
185.924573	5828.204299	26.083584
186.059495	5840.071189	26.088602
186.115443	5851.347472	26.093620
186.247516	5858.000119	26.098637
186.597039	5865.790012	26.103655
187.189924	5878.308488	26.108672
187.445555	5882.823828	26.113690
187.307427	5877.024720	26.118708
187.608740	5895.870242	26.123725
187.342261	5895.804567	26.128743
188.029939	5897.392761	26.133760
187.709353	5915.893202	26.138778
187.787482	5912.118522	26.143796
188.173041	5937.062164	26.148813
188.448444	5937.338266	26.153831
189.151793	5950.385688	26.158848
189.090923	5964.653760	26.163866
189.357125	5972.210455	26.168884
189.596062	5972.678476	26.173901
189.657126	5985.920619	26.178919
190.336307	5998.315261	26.183936
190.355237	6009.385911	26.188954
190.568520	6007.247398	26.193972
190.286747	6003.954877	26.198989
190.572588	6019.949349	26.204007
190.681402	6031.833055	26.209024
190.766388	6044.515949	26.214042
191.083074	6045.678952	26.219060
191.232626	6052.041696	26.224077
191.091120	6067.540861	26.229095
191.838451	6073.305483	26.234112
191.798506	6085.092432	26.239130
192.313905	6088.080604	26.244148
192.583062	6105.782333	26.249165
192.412601	6108.154418	26.254183
192.609142	6116.182888	26.259200
192.651540	6133.809465	26.264218
192.785223	6138.321758	26.269236
193.391372	6157.085367	26.274253
193.252005	6156.750525	26.279271
193.299414	6176.121991	26.284288
193.558694	6187.051160	26.289306
194.183050	6196.793413	26.294324
194.552010	6201.471118	26.299341
194.214679	6213.856864	26.304359
195.002422	6223.122292	26.309376
195.058890	6229.726869	26.314394
195.085767	6230.253166	26.319412
195.315065	6246.376592	26.324429
195.414209	6252.144330	26.329447
195.432757	6258.846365	26.334464
195.501919	6272.156902	26.339482
195.897399	6270.656050	26.344500
196.101829	6296.076630	26.349517
196.165926	6306.038748	26.354535
196.894953	6308.011971	26.359552
197.071336	6322.344398	26.364570
197.054864	6331.046933	26.369588
197.421744	6325.986637	26.374605
197.391118	6341.812851	26.379623
197.812141	6352.994725	26.384640
197.921710	6356.102945	26.389658
197.915064	6362.054493	26.394676
198.181102	6363.118075	26.399693
198.272626	6379.635558	26.404711
198.435882	6392.836833	26.409728
199.087274	6411.445296	26.414746
198.936923	6407.608229	26.419764
198.978215	6413.113549	26.424781
199.343347	6428.032228	26.429799
199.617232	6440.364005	26.434816
199.546245	6433.351564	26.439834
199.857068	6441.135103	26.444852
200.219036	6453.825666	26.449869
200.182966	6460.855105	26.454887
200.611915	6459.835160	26.459904
200.432888	6473.121349	26.464922
200.861141	6482.910071	26.469940
201.143077	6506.532181	26.474957
200.977201	6517.265733	26.479975
201.512361	6520.793855	26.484992
201.636727	6533.467801	26.490010
202.223265	6529.673819	26.495028
202.283522	6541.757977	26.500045
202.578197	6558.307127	26.505063
202.729009	6560.029475	26.510080
202.851736	6562.075024	26.515098
203.102933	6576.143464	26.520116
203.527391	6584.120873	26.525133
203.349821	6589.350962	26.530151
203.545531	6598.636151	26.535168
203.790714	6620.240669	26.540186
203.813483	6614.864531	26.545204
204.476741	6623.900164	26.550221
204.383264	6632.977855	26.555239
204.464221	6635.329805	26.560256
204.721886	6660.859404	26.565274
204.854966	6671.303433	26.570292
205.359484	6676.010663	26.575309
205.283676	6691.901035	26.580327
205.738394	6690.078410	26.585344
206.129244	6709.649510	26.590362
206.276340	6711.533445	26.595380
206.158057	6710.308264	26.600397
206.313937	6725.651201	26.605415
206.576485	6737.568253	26.610432
206.944866	6744.092887	26.615450
207.201679	6760.635488	26.620468
207.612278	6759.971941	26.625485
207.307842	6773.495688	26.630503
207.275110	6774.059692	26.635520
208.211445	6790.954257	26.640538
208.067803	6810.059402	26.645556
208.445246	6816.225938	26.650573
208.392020	6830.174660	26.655591
208.584384	6844.451343	26.660608
208.811763	6851.392564	26.665626
208.768166	6871.116709	26.670644
209.354083	6880.379171	26.675661
209.518016	6895.455828	26.680679
209.808698	6907.176047	26.685696
210.037571	6917.766298	26.690714
210.476474	6930.050617	26.695732
210.699430	6920.163748	26.700749
210.842502	6932.670906	26.705767
211.494945	6935.783096	26.710784
211.576514	6938.201282	26.715802
211.799012	6936.938814	26.720820
212.464095	6926.118150	26.725837
212.422062	6944.213229	26.730855
212.764709	6945.309115	26.735872
213.066644	6952.721756	26.740890
212.564561	6956.240984	26.745908
213.125126	6946.683511	26.750925
212.848353	6952.797264	26.755943
213.262795	6961.376187	26.760960
213.527384	6970.729762	26.765978
213.388919	6983.110319	26.770996
213.604101	6982.575050	26.776013
213.679116	6991.683508	26.781031
213.780910	7003.297454	26.786048
213.949470	7017.044479	26.791066
214.048997	7028.914496	26.796084
214.335709	7038.103663	26.801101
214.690529	7055.518334	26.806119
214.644519	7068.083434	26.811136
214.832436	7074.146977	26.816154
214.894187	7095.019823	26.821172
215.369691	7118.221143	26.826189
215.593473	7128.307218	26.831207
215.882119	7133.632188	26.836224
216.376825	7140.689741	26.841242
216.668344	7159.957950	26.846260
217.314423	7160.002738	26.851277
217.355783	7155.965198	26.856295
217.514819	7165.657301	26.861312
217.885637	7172.914093	26.866330
218.050103	7180.521854	26.871348
218.331560	7173.911998	26.876365
218.508743	7197.383998	26.881383
218.693301	7206.964817	26.886400
218.808349	7206.413563	26.891418
218.736647	7220.289695	26.896436
219.118501	7235.651543	26.901453
218.940010	7240.982979	26.906471
219.634095	7251.598858	26.911488
220.168094	7255.840752	26.916506
219.854750	7271.307708	26.921524
219.996006	7273.978664	26.926541
220.427696	7284.685924	26.931559
220.400049	7290.268534	26.936576
221.040487	7310.180241	26.941594
220.897417	7323.202585	26.946612
221.211189	7320.877807	26.951629
221.221960	7340.142561	26.956647
221.629912	7343.977924	26.961664
222.031210	7350.421887	26.966682
221.973270	7360.523540	26.971700
222.237568	7371.553656	26.976717
222.323694	7391.614888	26.981735
222.560458	7396.938542	26.986752
223.023081	7406.138390	26.991770
222.798941	7431.715662	26.996788
223.579373	7440.218890	27.001805
223.634854	7460.155536	27.006823
223.953120	7472.178040	27.011840
224.149308	7492.531621	27.016858
224.280264	7503.399477	27.021876
224.668200	7513.681190	27.026893
225.192270	7520.690122	27.031911
224.970569	7532.184296	27.036928
225.150608	7530.697946	27.041946
225.380105	7552.274436	27.046964
225.850410	7554.897361	27.051981
225.769354	7572.282521	27.056999
225.877678	7587.327364	27.062016
226.150356	7595.303591	27.067034
226.442265	7621.956210	27.072052
226.679597	7633.214821	27.077069
227.131017	7643.013188	27.082087
227.073063	7653.140258	27.087104
227.457120	7667.981237	27.092122
227.417249	7676.182946	27.097140
227.802461	7682.083385	27.102157
228.071121	7688.469195	27.107175
228.470415	7706.439491	27.112192
228.846072	7699.139202	27.117210
228.671587	7714.202923	27.122228
228.900187	7724.743173	27.127245
229.265828	7742.826080	27.132263
229.258783	7754.283816	27.137280
229.643607	7748.768899	27.142298
230.098423	7782.388976	27.147316
230.038628	7785.924737	27.152333
230.599042	7795.605195	27.157351
230.632324	7809.440170	27.162368
231.072966	7807.000872	27.167386
231.421724	7825.900978	27.172404
231.617352	7825.993803	27.177421
231.880057	7833.813840	27.182439
231.903298	7842.053152	27.187456
232.433963	7854.958351	27.192474
232.423028	7862.637900	27.197492
232.414507	7864.634577	27.202509
233.249804	7874.127061	27.207527
233.100793	7880.609533	27.212544
233.589413	7893.934866	27.217562
233.682353	7913.007481	27.222580
234.027816	7916.252874	27.227597
234.212484	7920.505113	27.232615
234.351086	7928.294001	27.237632
234.688050	7918.363592	27.242650
234.817307	7949.335465	27.247668
234.873682	7965.780925	27.252685
235.198338	7974.475326	27.257703
235.451733	7979.739735	27.262720
235.655766	7981.434991	27.267738
235.752598	8006.634765	27.272756
235.897534	8015.025684	27.277773
236.432795	8030.531635	27.282791
236.099350	8046.984188	27.287808
236.729526	8064.413773	27.292826
237.148265	8077.131352	27.297844
237.318871	8091.109322	27.302861
237.779870	8092.928744	27.307879
238.088895	8096.299807	27.312896
238.624946	8108.954946	27.317914
238.548382	8102.791964	27.322932
238.481684	8112.210327	27.327949
239.265403	8115.981038	27.332967
239.503730	8133.844220	27.337984
239.769475	8133.253692	27.343002
239.436953	8143.139649	27.348020
240.086807	8161.898514	27.353037
240.432052	8154.688020	27.358055
240.623469	8171.993440	27.363072
240.900063	8174.532963	27.368090
240.803289	8179.684626	27.373108
241.110100	8190.916977	27.378125
241.293074	8213.126572	27.383143
241.454000	8215.441020	27.388160
241.731757	8228.711028	27.393178
241.889221	8241.804041	27.398196
241.906979	8249.239351	27.403213
242.355910	8265.156724	27.408231
242.278192	8275.211445	27.413248
242.365884	8289.593944	27.418266
242.766292	8310.746932	27.423284
243.455062	8322.320839	27.428301
243.602357	8331.570246	27.433319
243.665252	8353.599812	27.438336
244.114327	8357.040673	27.443354
244.351980	8367.488329	27.448372
244.130554	8378.600985	27.453389
244.968302	8392.071218	27.458407
244.972475	8397.570285	27.463424
244.882254	8410.585168	27.468442
245.149198	8424.090622	27.473460
245.275019	8439.906912	27.478477
245.537404	8448.620704	27.483495
245.767544	8470.245526	27.488512
246.253237	8478.791971	27.493530
246.112043	8499.581194	27.498548
246.164850	8518.676469	27.503565
246.871401	8532.808114	27.508583
246.964343	8553.390465	27.513600
247.569525	8559.241155	27.518618
247.892024	8581.925130	27.523636
248.079172	8591.733578	27.528653
248.384239	8595.777805	27.533671
248.511890	8615.000438	27.538688
248.914546	8631.471506	27.543706
249.445601	8633.418989	27.548724
249.096909	8660.415938	27.553741
250.000230	8672.054534	27.558759
249.898198	8683.859128	27.563776
250.320643	8700.993322	27.568794
250.682968	8713.164476	27.573812
250.467600	8727.985978	27.578829
250.665902	8736.463630	27.583847
251.151512	8762.964616	27.588864
251.257326	8761.016160	27.593882
251.744657	8787.715811	27.598900
251.916584	8800.791182	27.603917
252.336307	8814.175266	27.608935
252.811772	8819.667383	27.613952
252.983393	8824.581699	27.618970
252.961811	8841.996679	27.623988
253.277568	8850.361384	27.629005
253.645695	8858.645326	27.634023
253.856543	8876.497720	27.639040
254.531908	8895.057620	27.644058
254.595381	8897.106342	27.649076
254.536702	8913.377973	27.654093
254.987396	8913.629994	27.659111
254.834210	8926.929712	27.664128
255.412483	8944.058815	27.669146
255.512718	8954.771296	27.674164
255.652579	8962.639353	27.679181
256.057164	8968.433006	27.684199
256.572574	8988.441770	27.689216
256.631930	8991.447756	27.694234
257.276456	9013.703270	27.699252
257.355919	9022.085898	27.704269
257.398158	9031.929768	27.709287
257.535122	9043.883655	27.714304
258.487125	9050.485580	27.719322
258.789888	9057.245415	27.724340
258.795081	9068.626289	27.729357
259.212663	9068.343595	27.734375
258.963820	9077.323548	27.739392
259.391911	9087.915607	27.744410
259.895347	9104.279850	27.749428
260.131733	9119.871136	27.754445
260.377829	9112.830408	27.759463
260.226137	9131.910796	27.764480
260.221562	9145.916839	27.769498
260.605848	9158.296398	27.774516
260.710434	9179.575366	27.779533
261.399168	9187.500139	27.784551
261.289674	9204.373485	27.789568
261.589002	9199.818603	27.794586
262.187095	9219.085438	27.799604
262.195620	9233.004263	27.804621
262.474426	9244.453148	27.809639
262.406514	9262.706075	27.814656
262.997429	9279.211556	27.819674
263.274024	9285.666144	27.824692
263.254169	9306.475268	27.829709
263.695953	9305.112202	27.834727
264.081449	9335.418224	27.839744
264.368048	9337.495401	27.844762
264.822260	9347.025882	27.849780
264.975907	9357.515591	27.854797
265.424233	9360.628411	27.859815
265.925922	9367.461577	27.864832
265.763588	9374.852762	27.869850
266.098133	9391.701348	27.874868
266.231313	9404.814751	27.879885
266.828772	9402.906503	27.884903
266.710167	9423.011288	27.889920
266.955793	9439.188647	27.894938
267.308277	9457.407887	27.899956
267.086996	9462.614019	27.904973
267.654798	9482.994029	27.909991
267.764647	9506.810958	27.915008
267.925732	9517.842643	27.920026
268.586845	9538.681771	27.925044
268.767295	9550.581856	27.930061
268.990595	9566.254487	27.935079
269.234736	9594.183441	27.940096
269.430220	9604.701507	27.945114
270.012478	9623.579731	27.950132
269.976568	9643.106733	27.955149
270.295498	9653.100448	27.960167
270.738062	9681.888987	27.965184
270.946397	9694.318399	27.970202
271.140114	9703.876990	27.975220
271.692262	9729.904886	27.980237
272.160427	9733.611404	27.985255
272.389304	9756.545033	27.990272
272.627989	9771.637662	27.995290
272.899289	9778.437389	28.000308
273.182233	9792.345483	28.005325
273.473363	9799.940921	28.010343
273.696127	9808.348954	28.015360
273.456587	9834.219253	28.020378
274.422463	9847.695866	28.025396
274.296787	9859.031296	28.030413
274.790251	9871.230156	28.035431
274.666201	9888.302140	28.040448
274.738592	9914.269222	28.045466
275.299569	9922.015294	28.050484
275.590854	9944.506889	28.055501
276.078244	9956.874089	28.060519
276.297480	9984.330754	28.065536
276.874581	9983.600136	28.070554
277.432192	9994.882945	28.075572
277.356059	10011.158255	28.080589
278.180322	10021.708115	28.085607
278.103022	10032.824579	28.090624
277.836602	10044.374630	28.095642
278.454371	10036.808407	28.100660
278.595308	10058.186914	28.105677
278.960714	10069.228162	28.110695
279.500931	10076.778620	28.115712
279.633345	10090.801935	28.120730
280.222846	10095.260023	28.125748
280.041447	10108.650226	28.130765
280.318287	10129.862420	28.135783
280.481682	10117.886654	28.140800
280.815560	10136.551484	28.145818
281.266740	10153.508898	28.150836
281.249793	10165.288557	28.155853
281.533677	10173.703027	28.160871
281.760713	10184.289128	28.165888
282.223656	10208.121446	28.170906
282.330474	10213.188300	28.175924
282.841521	10230.079631	28.180941
282.903269	10236.665878	28.185959
283.172256	10253.686478	28.190976
283.206707	10276.338440	28.195994
283.581208	10283.122286	28.201012
283.641693	10298.656700	28.206029
284.433945	10318.484879	28.211047
284.779374	10338.035332	28.216064
284.703803	10358.532255	28.221082
285.081420	10367.011154	28.226100
285.166311	10386.182290	28.231117
286.070475	10400.328806	28.236135
286.049915	10418.477615	28.241152
286.299120	10440.606949	28.246170
286.543743	10457.558909	28.251188
287.177427	10459.320115	28.256205
287.113080	10479.202891	28.261223
287.530460	10498.072944	28.266240
287.694617	10508.987916	28.271258
288.094342	10519.714665	28.276276
288.616449	10535.922555	28.281293
288.657456	10554.882835	28.286311
289.437058	10567.514375	28.291328
289.237214	10591.017805	28.296346
289.710845	10601.859391	28.301364
289.889875	10615.358029	28.306381
290.423070	10623.743361	28.311399
290.375573	10640.321031	28.316416
290.530958	10660.223466	28.321434
291.028930	10675.693241	28.326452
291.356145	10690.596018	28.331469
291.731157	10706.451224	28.336487
292.327357	10721.776290	28.341504
292.318692	10727.480120	28.346522
292.524369	10749.982860	28.351540
293.049740	10768.037543	28.356557
292.789066	10784.538019	28.361575
293.781898	10793.107622	28.366592
293.791787	10811.798310	28.371610
294.145979	10825.418230	28.376628
294.316770	10845.340566	28.381645
294.403525	10861.433385	28.386663
294.972265	10875.392519	28.391680
295.081200	10898.077844	28.396698
295.256554	10908.448223	28.401716
295.749661	10925.324034	28.406733
296.470154	10946.196546	28.411751
296.249389	10953.300650	28.416768
296.535323	10973.928257	28.421786
297.091934	10981.760706	28.426804
297.455687	11000.889058	28.431821
297.785776	11015.204357	28.436839
298.117433	11028.095398	28.441856
297.972546	11038.004194	28.446874
298.249966	11064.534565	28.451892
298.882126	11072.203730	28.456909
298.920693	11091.768016	28.461927
299.301458	11109.419282	28.466944
299.768937	11122.769182	28.471962
300.111236	11128.727930	28.476980
300.272558	11130.777453	28.481997
300.450222	11142.104325	28.487015
301.162806	11163.202494	28.492032
301.105202	11174.941757	28.497050
301.637756	11191.524335	28.502068
301.705432	11200.825458	28.507085
301.926080	11217.598706	28.512103
302.577694	11227.917220	28.517120
302.438469	11245.548529	28.522138
302.880961	11256.221682	28.527156
303.359090	11280.615046	28.532173
303.696358	11279.950141	28.537191
304.308702	11289.393853	28.542208
304.286455	11306.204996	28.547226
305.278639	11313.837157	28.552244
305.592620	11315.436667	28.557261
305.713229	11319.282869	28.562279
306.042713	11325.843606	28.567296
306.463799	11338.240994	28.572314
306.606670	11336.100207	28.577332
306.632730	11342.146147	28.582349
307.004102	11362.773514	28.587367
307.228319	11361.289458	28.592384
307.076467	11385.541066	28.597402
308.014037	11401.167192	28.602420
308.323555	11414.055631	28.607437
308.228300	11427.234440	28.612455
308.235434	11446.084069	28.617472
308.236591	11467.896434	28.622490
308.599264	11480.877686	28.627508
309.273913	11509.399259	28.632525
309.392268	11523.536354	28.637543
309.953040	11546.243690	28.642560
309.687610	11574.993816	28.647578
310.520771	11582.158264	28.652596
310.925760	11606.219266	28.657613
311.050496	11630.933342	28.662631
311.733060	11643.640717	28.667648
311.626966	11668.217112	28.672666
311.856006	11680.006792	28.677684
312.302419	11704.291974	28.682701
312.547575	11728.381173	28.687719
313.177836	11738.659089	28.692736
313.426956	11779.015706	28.697754
313.843378	11784.931548	28.702772
313.859501	11794.796731	28.707789
314.087969	11827.433152	28.712807
314.926054	11845.983305	28.717824
315.070571	11864.755128	28.722842
315.305075	11875.258929	28.727860
315.860245	11884.797101	28.732877
316.122213	11910.813227	28.737895
316.684506	11930.091606	28.742912
316.696927	11943.506624	28.747930
317.251622	11958.071864	28.752948
317.754638	11963.595365	28.757965
317.496956	11982.180469	28.762983
317.915999	11990.151594	28.768000
317.630485	12013.231230	28.773018
318.100092	12034.832387	28.778036
318.732174	12050.926586	28.783053
318.736236	12079.133460	28.788071
319.376280	12099.217742	28.793088
319.715385	12112.064164	28.798106
319.973673	12137.313864	28.803124
320.463480	12151.286242	28.808141
320.595240	12174.812657	28.813159
320.704753	12188.664281	28.818176
321.908468	12192.408352	28.823194
321.928704	12203.255147	28.828212
322.479066	12214.742525	28.833229
322.427676	12223.462732	28.838247
322.846975	12237.367210	28.843264
323.641397	12252.968972	28.848282
323.386879	12261.787133	28.853300
323.940046	12268.098655	28.858317
324.006783	12289.143918	28.863335
324.348018	12305.239409	28.868352
324.710094	12317.766626	28.873370
324.876721	12339.007960	28.878388
325.423841	12343.934218	28.883405
325.736994	12369.096745	28.888423
326.250674	12380.315215	28.893440
326.289682	12399.009267	28.898458
326.288673	12407.598566	28.903476
326.763091	12424.759678	28.908493
326.928123	12452.837846	28.913511
327.308069	12471.813611	28.918528
327.391400	12484.295919	28.923546
327.828774	12505.536340	28.928564
328.746813	12526.812474	28.933581
328.578731	12554.588988	28.938599
329.025955	12563.844328	28.943616
329.458520	12584.861388	28.948634
329.638594	12612.192225	28.953652
330.199961	12622.481354	28.958669
330.379326	12647.807181	28.963687
331.191271	12663.112887	28.968704
331.611219	12680.254293	28.973722
331.457936	12698.340711	28.978740
331.960054	12718.368185	28.983757
331.896977	12737.397400	28.988775
332.403763	12751.945455	28.993792
332.489852	12768.766302	28.998810
333.041637	12801.234082	29.003828
333.763367	12818.205479	29.008845
334.191451	12837.928828	29.013863
334.365517	12859.299060	29.018880
334.710488	12881.236373	29.023898
334.682062	12891.986933	29.028916
334.843478	12913.390773	29.033933
335.314341	12938.349514	29.038951
335.807158	12953.660931	29.043968
335.913546	12973.137671	29.048986
336.183735	12995.832003	29.054004
336.625476	13014.160816	29.059021
336.887904	13041.457349	29.064039
337.400963	13062.544514	29.069056
337.785870	13087.914721	29.074074
338.190216	13115.947145	29.079092
338.763351	13124.377913	29.084109
338.868670	13150.281195	29.089127
339.520081	13172.821655	29.094144
339.527803	13190.286646	29.099162
339.464577	13213.677347	29.104180
339.971968	13226.627804	29.109197
340.615026	13250.679110	29.114215
341.137825	13276.716516	29.119232
341.496330	13287.242853	29.124250
341.774695	13319.081469	29.129268
342.285444	13334.535666	29.134285
342.610778	13350.167161	29.139303
342.543490	13357.055643	29.144320
343.270382	13377.693032	29.149338
343.001268	13394.452893	29.154356
343.334228	13405.112746	29.159373
344.120655	13432.808265	29.164391
344.359249	13448.267030	29.169408
345.038540	13451.916166	29.174426
345.197135	13471.486345	29.179444
345.975854	13484.208423	29.184461
345.776772	13510.573273	29.189479
346.150147	13514.715311	29.194496
346.484731	13534.131840	29.199514
346.991677	13555.504720	29.204532
347.348812	13558.727188	29.209549
347.649425	13585.488034	29.214567
347.507329	13601.091455	29.219584
348.406073	13612.541243	29.224602
348.881593	13622.471652	29.229620
349.576015	13625.439515	29.234637
349.482186	13646.220760	29.239655
350.298447	13663.336099	29.244672
350.339033	13663.898368	29.249690
350.329133	13682.989730	29.254708
350.863986	13701.674193	29.259725
351.255006	13717.444189	29.264743
351.334598	13734.857440	29.269760
352.195561	13744.816330	29.274778
352.335833	13765.498101	29.279796
352.996144	13764.763875	29.284813
353.187707	13787.793510	29.289831
353.400665	13805.081851	29.294848
353.959966	13815.788806	29.299866
353.721608	13829.894744	29.304884
354.525250	13849.800689	29.309901
354.569151	13869.003864	29.314919
354.930844	13887.980738	29.319936
355.485199	13907.518177	29.324954
355.575950	13937.094359	29.329972
355.981611	13953.152806	29.334989
356.419726	13979.684377	29.340007
356.720615	13993.074889	29.345024
356.787086	14012.536808	29.350042
357.057153	14043.244218	29.355060
357.478354	14071.487022	29.360077
357.684170	14097.499116	29.365095
358.226972	14118.102815	29.370112
358.462464	14146.011471	29.375130
358.683014	14172.968776	29.380148
359.523251	14191.893560	29.385165
360.141627	14213.404579	29.390183
360.016361	14234.946128	29.395200
360.805737	14257.741153	29.400218
361.454942	14279.064282	29.405236
361.704852	14283.712048	29.410253
361.941688	14304.230947	29.415271
362.338792	14319.871019	29.420288
362.880946	14340.298211	29.425306
363.228984	14353.852173	29.430324
363.377912	14363.878030	29.435341
364.063949	14386.935626	29.440359
364.111281	14402.494425	29.445376
364.319462	14425.076961	29.450394
364.856574	14451.745367	29.455412
365.543556	14461.573821	29.460429
365.917556	14475.679645	29.465447
365.969647	14491.787278	29.470464
366.557882	14509.804195	29.475482
366.727007	14520.130164	29.480500
367.567974	14537.668790	29.485517
367.905119	14559.533476	29.490535
367.972626	14571.577495	29.495552
368.476442	14574.913101	29.500570
368.578442	14592.071004	29.505588
368.511788	14604.527532	29.510605
369.202114	14626.324678	29.515623
369.396069	14646.105314	29.520640
369.522120	14651.353542	29.525658
369.682590	14675.784970	29.530676
370.236381	14698.250864	29.535693
370.846680	14722.280721	29.540711
370.850398	14744.544919	29.545728
371.283881	14769.275039	29.550746
371.429646	14796.134337	29.555764
372.095135	14820.727345	29.560781
372.042192	14847.949253	29.565799
372.066833	14873.769547	29.570816
372.925718	14888.286542	29.575834
373.289504	14921.993636	29.580852
373.868807	14949.354120	29.585869
374.247033	14976.888063	29.590887
374.433865	15011.567149	29.595904
375.235187	15038.217352	29.600922
375.222654	15069.213594	29.605940
375.678269	15082.893445	29.610957
376.348811	15117.971143	29.615975
376.865315	15140.948672	29.620992
377.417872	15157.572689	29.626010
377.537382	15181.483727	29.631028
377.933452	15203.542103	29.636045
378.725361	15214.567355	29.641063
378.916784	15233.433122	29.646080
379.250384	15251.720933	29.651098
379.875613	15275.505985	29.656116
380.073949	15297.254169	29.661133
380.436945	15317.577660	29.666151
380.614506	15337.402623	29.671168
380.980651	15357.855153	29.676186
381.448706	15383.736592	29.681204
381.898103	15404.744690	29.686221
382.821401	15433.375607	29.691239
382.503717	15455.071660	29.696256
383.265478	15467.961945	29.701274
383.629602	15492.896455	29.706292
383.781214	15513.651000	29.711309
384.425396	15527.829240	29.716327
384.950628	15559.525799	29.721344
385.395860	15565.533097	29.726362
386.451694	15564.080323	29.731380
386.941774	15576.994029	29.736397
387.141868	15589.674965	29.741415
387.334602	15599.726236	29.746432
387.918258	15598.119575	29.751450
388.032229	15616.846185	29.756468
388.067147	15633.898613	29.761485
388.708521	15647.512053	29.766503
388.541418	15671.518857	29.771520
389.337214	15679.783460	29.776538
389.553245	15703.001099	29.781556
389.636372	15720.876723	29.786573
389.897613	15744.273711	29.791591
390.302088	15771.634170	29.796608
390.515428	15791.027666	29.801626
390.790085	15817.154565	29.806644
390.918408	15839.305892	29.811661
391.678400	15869.722054	29.816679
391.973243	15901.101318	29.821696
392.592705	15922.794127	29.826714
393.250527	15940.166750	29.831732
393.712601	15963.507474	29.836749
393.760086	15971.493914	29.841767
393.950422	16003.060164	29.846784
394.697016	16016.603796	29.851802
394.925342	16034.093902	29.856820
395.265438	16058.082236	29.861837
395.585108	16072.374570	29.866855
395.716396	16104.452353	29.871872
396.612143	16126.850905	29.876890
396.893308	16153.899483	29.881908
397.176228	16180.868867	29.886925
397.268193	16192.426875	29.891943
397.777826	16226.476775	29.896960
398.343565	16244.918899	29.901978
398.564709	16287.705605	29.906996
398.786449	16308.311127	29.912013
399.518926	16331.919724	29.917031
399.892487	16362.889536	29.922048
400.543836	16389.833440	29.927066
401.337809	16412.339765	29.932084
401.249854	16438.246025	29.937101
401.728521	16455.429079	29.942119
402.213438	16480.033390	29.947136
402.542225	16500.104478	29.952154
403.181870	16519.201782	29.957172
403.425571	16547.516947	29.962189
404.114219	16570.140924	29.967207
404.142716	16599.187676	29.972224
404.356564	16613.098928	29.977242
405.133263	16644.268582	29.982260
405.362702	16668.341234	29.987277
406.416882	16680.482491	29.992295
406.699139	16704.521699	29.997312
407.061492	16729.448620	30.002330
407.634910	16746.083409	30.007348
407.666729	16770.843910	30.012365
408.439942	16776.882652	30.017383
408.604485	16811.656904	30.022400
409.264812	16830.129085	30.027418
409.573247	16844.019462	30.032436
409.942377	16870.613173	30.037453
410.428923	16890.072636	30.042471
410.706186	16908.904582	30.047488
411.088230	16930.237529	30.052506
411.909390	16953.296148	30.057524
411.992688	16976.633906	30.062541
412.666849	16981.598461	30.067559
412.541873	17011.064537	30.072576
412.791404	17030.744233	30.077594
413.280420	17055.989816	30.082612
413.605902	17083.566589	30.087629
414.222712	17108.779713	30.092647
414.557443	17133.499839	30.097664
414.768665	17158.043398	30.102682
415.108431	17185.548606	30.107700
415.244719	17223.293838	30.112717
416.083647	17241.271151	30.117735
416.286523	17277.796411	30.122752
416.798276	17309.425317	30.127770
417.466700	17331.254234	30.132788
417.749744	17369.175891	30.137805
418.081286	17396.433156	30.142823
418.614349	17410.728010	30.147840
419.101014	17441.565086	30.152858
419.549637	17455.089799	30.157876
419.572120	17494.243039	30.162893
420.320697	17504.448826	30.167911
420.576735	17543.054119	30.172928
421.115218	17568.160014	30.177946
421.936589	17582.315355	30.182964
421.951563	17602.212189	30.187981
423.053734	17620.739530	30.192999
423.149275	17641.880976	30.198016
423.466020	17655.691681	30.203034
424.247594	17677.054857	30.208052
424.366402	17712.501158	30.213069
424.540831	17722.821713	30.218087
424.843632	17757.885691	30.223104
425.358789	17775.898117	30.228122
425.616991	17799.263337	30.233140
425.977629	17831.121934	30.238157
426.476190	17856.199674	30.243175
426.917713	17876.889530	30.248192
427.409192	17905.638752	30.253210
427.860668	17925.708020	30.258228
428.106617	17959.233486	30.263245
428.758685	17975.721276	30.268263
428.685940	18010.818908	30.273280
429.716284	18021.833939	30.278298
430.317767	18049.315428	30.283316
430.824184	18081.625540	30.288333
431.421153	18103.359063	30.293351
431.654371	18120.581819	30.298368
431.991136	18142.368528	30.303386
432.901792	18177.066991	30.308404
432.749867	18196.567158	30.313421
433.186738	18220.164082	30.318439
433.472094	18255.440150	30.323456
433.624660	18278.013772	30.328474
434.505912	18307.265158	30.333492
434.731681	18342.822309	30.338509
435.240746	18361.291083	30.343527
435.641560	18386.959612	30.348544
436.005043	18411.667424	30.353562
436.985608	18439.197848	30.358580
437.546523	18468.808903	30.363597
437.760240	18499.983922	30.368615
438.288802	18529.391630	30.373632
438.144645	18559.485318	30.378650
439.016203	18573.248212	30.383668
439.499511	18609.403822	30.388685
439.584792	18635.229200	30.393703
440.147258	18672.680324	30.398720
440.389451	18694.899333	30.403738
440.845566	18720.319631	30.408756
441.508290	18751.576773	30.413773
441.801444	18782.424004	30.418791
442.030295	18816.977056	30.423808
442.504499	18853.147173	30.428826
443.217064	18874.073872	30.433844
443.772328	18904.526708	30.438861
444.341328	18944.573862	30.443879
444.495841	18968.841097	30.448896
445.148332	18994.237499	30.453914
445.739332	19015.789766	30.458932
446.033918	19040.572281	30.463949
446.403706	19073.707656	30.468967
446.940797	19098.105022	30.473984
447.191811	19125.623647	30.479002
448.078827	19155.045994	30.484020
448.521726	19186.369649	30.489037
448.700420	19214.556695	30.494055
448.881083	19241.593657	30.499072
449.765178	19272.374939	30.504090
450.298499	19297.259604	30.509108
450.385376	19321.190335	30.514125
450.982477	19339.785326	30.519143
451.632681	19362.946097	30.524160
451.867890	19382.879966	30.529178
452.412306	19397.585177	30.534196
452.629060	19430.005809	30.539213
452.988849	19449.528651	30.544231
453.594672	19467.193698	30.549248
453.752504	19501.335732	30.554266
454.351882	19524.397206	30.559284
454.727354	19553.053212	30.564301
455.270974	19588.436804	30.569319
455.564502	19614.938655	30.574336
456.228334	19648.155588	30.579354
456.730678	19659.399068	30.584372
456.958917	19684.502305	30.589389
457.782257	19718.597975	30.594407
458.532800	19733.530383	30.599424
458.685408	19768.273893	30.604442
459.286972	19789.136729	30.609460
459.582143	19819.435636	30.614477
460.112983	19845.054261	30.619495
460.429238	19871.969903	30.624512
461.009092	19903.052264	30.629530
461.645385	19927.106696	30.634548
461.650989	19961.254280	30.639565
462.017279	19989.021531	30.644583
462.813027	20018.566800	30.649600
463.261617	20052.291775	30.654618
463.483451	20084.649524	30.659636
463.855956	20114.349280	30.664653
463.989764	20155.420687	30.669671
465.019063	20177.051322	30.674688
465.224289	20208.988557	30.679706
465.850748	20240.955038	30.684724
466.612252	20283.097825	30.689741
466.817924	20307.718889	30.694759
467.324796	20346.603445	30.699776
467.722342	20379.376590	30.704794
468.248115	20412.818495	30.709812
468.671567	20440.065725	30.714829
469.108466	20461.845764	30.719847
469.903462	20494.241323	30.724864
470.004328	20524.710569	30.729882
470.953886	20559.754730	30.734900
471.204814	20595.868068	30.739917
471.628381	20631.468101	30.744935
472.380486	20653.887960	30.749952
472.157801	20698.926931	30.754970
473.145606	20723.066622	30.759988
473.621041	20759.935082	30.765005
473.645272	20792.400580	30.770023
474.362500	20823.734701	30.775040
475.079814	20858.758689	30.780058
475.537955	20882.014348	30.785076
476.270079	20913.997070	30.790093
476.510175	20938.790478	30.795111
477.319117	20967.570624	30.800128
477.539186	20998.350597	30.805146
478.514232	21028.564489	30.810164
479.218899	21041.129378	30.815181
479.535924	21062.069463	30.820199
480.358088	21079.430607	30.825216
480.829508	21101.224938	30.830234
481.144189	21118.500845	30.835252
481.560234	21139.191821	30.840269
482.077457	21165.812588	30.845287
482.492767	21178.548979	30.850304
483.018680	21198.294122	30.855322
483.257238	21214.608944	30.860340
483.670862	21229.436994	30.865357
484.292621	21257.854971	30.870375
484.942563	21269.556598	30.875392
484.913914	21291.214167	30.880410
485.650952	21311.299338	30.885428
485.842295	21334.622343	30.890445
485.730711	21350.720098	30.895463
486.791462	21370.110462	30.900480
486.708352	21401.475327	30.905498
486.753873	21432.295791	30.910516
487.687584	21474.559657	30.915533
488.354961	21504.341982	30.920551
488.870538	21529.150115	30.925568
489.246943	21577.724606	30.930586
489.340236	21606.219039	30.935604
490.208985	21646.427257	30.940621
490.585782	21668.508642	30.945639
491.240274	21690.439408	30.950656
491.967688	21729.178639	30.955674
492.372353	21763.248276	30.960692
492.979183	21799.080955	30.965709
493.320022	21828.586044	30.970727
494.165798	21850.702039	30.975744
494.321901	21884.305099	30.980762
495.444227	21907.079462	30.985780
496.043894	21933.043944	30.990797
496.238136	21962.376180	30.995815
496.737020	21982.252691	31.000832
497.186753	22020.928310	31.005850
497.227145	22042.297937	31.010868
497.969146	22068.840705	31.015885
498.344800	22120.026228	31.020903
498.981363	22149.795372	31.025920
499.372977	22180.209282	31.030938
499.983799	22220.104983	31.035956
500.243780	22253.622995	31.040973
500.520234	22288.914043	31.045991
500.822868	22318.135154	31.051008
501.687945	22349.935231	31.056026
502.070787	22393.190399	31.061044
502.694634	22431.485869	31.066061
503.093866	22476.040321	31.071079
503.958076	22508.952885	31.076096
504.330865	22541.461782	31.081114
504.524824	22580.595351	31.086132
504.675714	22625.713257	31.091149
505.105984	22667.350355	31.096167
506.306906	22700.867974	31.101184
506.790271	22744.335737	31.106202
507.702469	22777.531943	31.111220
508.032222	22808.474593	31.116237
508.135847	22845.904028	31.121255
508.730862	22878.037665	31.126272
509.507782	22919.273791	31.131290
510.096334	22956.198260	31.136308
510.887532	22984.320638	31.141325
511.475926	23022.426886	31.146343
511.852790	23042.531984	31.151360
512.482769	23085.345781	31.156378
512.688524	23119.120137	31.161396
513.456933	23140.333381	31.166413
513.629804	23172.798610	31.171431
514.088498	23210.780076	31.176448
514.473335	23246.454051	31.181466
515.374850	23272.373303	31.186484
515.972736	23294.952883	31.191501
516.331232	23336.166549	31.196519
517.231514	23354.067297	31.201536
517.370165	23379.751586	31.206554
517.774942	23407.922085	31.211572
518.515416	23431.035696	31.216589
518.586319	23465.122309	31.221607
519.372456	23503.223973	31.226624
519.951953	23522.956784	31.231642
520.505192	23550.200749	31.236660
521.169624	23577.964562	31.241677
521.513754	23612.564971	31.246695
521.859523	23638.103607	31.251712
522.434768	23674.285831	31.256730
522.628965	23703.551141	31.261748
523.570755	23733.016068	31.266765
524.136651	23773.117783	31.271783
524.727398	23787.098696	31.276800
525.067776	23835.861271	31.281818
525.486739	23858.412474	31.286836
526.304147	23888.257187	31.291853
526.473552	23923.820575	31.296871
527.130890	23966.240222	31.301888
527.840621	23996.259840	31.306906
528.448450	24030.112172	31.311924
528.864069	24055.722620	31.316941
529.460893	24098.088776	31.321959
529.686190	24126.041784	31.326976
530.339951	24156.563258	31.331994
530.469145	24197.966068	31.337012
531.510679	24234.430600	31.342029
531.686964	24277.892649	31.347047
532.250476	24302.665202	31.352064
532.846432	24346.788788	31.357082
533.352730	24380.752312	31.362100
534.206135	24416.905222	31.367117
534.475117	24453.098624	31.372135
535.435267	24491.402588	31.377152
536.280086	24515.379608	31.382170
536.450543	24549.288272	31.387188
537.182800	24579.122000	31.392205
537.423284	24621.734324	31.397223
537.882075	24648.280403	31.402240
538.547655	24680.943120	31.407258
539.321305	24714.821357	31.412276
539.562708	24746.595981	31.417293
540.414611	24784.095832	31.422311
540.867264	24824.861876	31.427328
541.590864	24854.255001	31.432346
541.634954	24886.256468	31.437364
542.597086	24921.097871	31.442381
543.057855	24960.004995	31.447399
543.441836	24985.937537	31.452416
544.007102	25022.920022	31.457434
544.868868	25059.167587	31.462452
545.436017	25082.746149	31.467469
545.577269	25122.992518	31.472487
546.108507	25154.305579	31.477504
547.063052	25179.928364	31.482522
547.848973	25212.699608	31.487540
548.800490	25234.107770	31.492557
549.388316	25271.017686	31.497575
549.644404	25285.456205	31.502592
550.189202	25309.392412	31.507610
550.423484	25334.862100	31.512628
551.023299	25355.092816	31.517645
551.654439	25386.845702	31.522663
552.114841	25418.599939	31.527680
552.775480	25440.451743	31.532698
553.177145	25482.933372	31.537716
553.655229	25497.122616	31.542733
553.904976	25524.681951	31.547751
553.997398	25545.130880	31.552768
554.948070	25579.652911	31.557786
554.996605	25612.634399	31.562804
555.398744	25646.888035	31.567821
556.106950	25703.965219	31.572839
556.102123	25736.272683	31.577856
557.037690	25771.227139	31.582874
557.379745	25819.760455	31.587892
558.337637	25854.452470	31.592909
558.256657	25902.299786	31.597927
558.301892	25937.810241	31.602944
559.503536	25985.135771	31.607962
559.853247	26044.304714	31.612980
560.963407	26088.756559	31.617997
561.256896	26135.395917	31.623015
562.437606	26174.465073	31.628032
562.949843	26210.219302	31.633050
563.419910	26247.566457	31.638068
564.232770	26283.191858	31.643085
564.920622	26324.234008	31.648103
565.731863	26363.323128	31.653120
566.216591	26388.085246	31.658138
566.404554	26427.985676	31.663156
567.151565	26468.848271	31.668173
567.831710	26512.893997	31.673191
567.961232	26544.265441	31.678208
568.723300	26587.401136	31.683226
569.528278	26630.688243	31.688244
570.494109	26674.708808	31.693261
570.913362	26699.671103	31.698279
571.674501	26735.039913	31.703296
572.665667	26764.002338	31.708314
572.970647	26803.133203	31.713332
573.597084	26832.007144	31.718349
574.115229	26861.795439	31.723367
574.683269	26890.842877	31.728384
575.062288	26922.327750	31.733402
575.591828	26969.640142	31.738420
576.336350	27002.477631	31.743437
576.881498	27032.944551	31.748455
577.062109	27070.205566	31.753472
577.173563	27102.566635	31.758490
578.123918	27148.676303	31.763508
579.201391	27180.893433	31.768525
579.898968	27224.463982	31.773543
580.143700	27256.766628	31.778560
580.981405	27292.156094	31.783578
581.327400	27322.610212	31.788596
581.939946	27357.238493	31.793613
582.609399	27389.114977	31.798631
583.276789	27434.340267	31.803648
583.839003	27459.015793	31.808666
584.345977	27501.769691	31.813684
584.694473	27542.456325	31.818701
585.646997	27577.227986	31.823719
585.733044	27607.672436	31.828736
586.899086	27642.935559	31.833754
587.477775	27677.563338	31.838772
587.938982	27713.246005	31.843789
588.832075	27747.060194	31.848807
589.030951	27776.545595	31.853824
590.224923	27797.798661	31.858842
590.192490	27831.934042	31.863860
591.235529	27854.683319	31.868877
591.864903	27888.311262	31.873895
592.278779	27924.551547	31.878912
592.741185	27944.995869	31.883930
593.222857	27977.509274	31.888948
593.316430	28017.781473	31.893965
594.114625	28042.471537	31.898983
594.087188	28086.769890	31.904000
594.624589	28113.965629	31.909018
594.922141	28164.597260	31.914036
595.339027	28213.055139	31.919053
596.563845	28255.458694	31.924071
596.700031	28304.851686	31.929088
597.160685	28344.473252	31.934106
597.713578	28388.087784	31.939124
598.692109	28443.449340	31.944141
599.209164	28493.352350	31.949159
599.571799	28548.272818	31.954176
600.292415	28591.160084	31.959194
600.871579	28648.935649	31.964212
601.558495	28693.193638	31.969229
602.496149	28734.720078	31.974247
603.117720	28785.100545	31.979264
603.915772	28824.310239	31.984282
604.514242	28875.231786	31.989300
605.269047	28908.961983	31.994317
605.977369	28952.679940	31.999335
606.309084	29004.496636	32.004352
607.156450	29042.883695	32.009370
607.519124	29096.257038	32.014388
608.073300	29139.512689	32.019405
609.251407	29179.226454	32.024423
609.385013	29219.861397	32.029440
610.071039	29269.392352	32.034458
611.120930	29305.890047	32.039476
611.935917	29340.888403	32.044493
612.863869	29369.971849	32.049511
613.175791	29415.724621	32.054528
614.112974	29441.153253	32.059546
614.453811	29473.899557	32.064564
614.873381	29516.007590	32.069581
615.983274	29550.277736	32.074599
616.008088	29598.148878	32.079616
617.010608	29625.666125	32.084634
617.508177	29675.404387	32.089652
618.002328	29707.962852	32.094669
618.740929	29740.755118	32.099687
618.944343	29785.678593	32.104704
619.690513	29824.139761	32.109722
620.551824	29874.428698	32.114740
620.764010	29908.030099	32.119757
621.593570	29959.215455	32.124775
621.615819	29999.565866	32.129792
622.601092	30043.837220	32.134810
623.269020	30092.563882	32.139828
624.072729	30138.431339	32.144845
624.483968	30181.806258	32.149863
625.275779	30227.675767	32.154880
625.658886	30261.485020	32.159898
626.317256	30310.479174	32.164916
627.048106	30362.913531	32.169933
627.803337	30402.404725	32.174951
628.487724	30452.134747	32.179968
629.043917	30489.122285	32.184986
629.652325	30531.910980	32.190004
630.038299	30574.159156	32.195021
630.748923	30620.111712	32.200039
631.114063	30666.288827	32.205056
631.808276	30710.328791	32.210074
632.683463	30762.785945	32.215092
633.157664	30804.445619	32.220109
634.003498	30841.635232	32.225127
634.268104	30885.160884	32.230144
634.796437	30929.865596	32.235162
635.111128	30970.374663	32.240180
635.833838	31012.779921	32.245197
636.540945	31055.731337	32.250215
637.203076	31114.436488	32.255232
637.841115	31158.707403	32.260250
638.860150	31199.322201	32.265268
639.432242	31242.105378	32.270285
640.312104	31282.710398	32.275303
640.793779	31331.121300	32.280320
641.643677	31369.689317	32.285338
642.644723	31406.002383	32.290356
643.090646	31442.503075	32.295373
644.063026	31469.035008	32.300391
644.600756	31509.156404	32.305408
645.425665	31544.119038	32.310426
646.558947	31573.578222	32.315444
647.193003	31608.507460	32.320461
647.798926	31649.092629	32.325479
647.681942	31675.813376	32.330496
648.288229	31710.955722	32.335514
649.376450	31755.290587	32.340532
649.854305	31784.150403	32.345549
650.776394	31824.256827	32.350567
651.933003	31855.596629	32.355584
652.252729	31886.093222	32.360602
652.567748	31920.212906	32.365620
653.260939	31964.312596	32.370637
654.161079	31997.519503	32.375655
654.344282	32035.977610	32.380672
654.999643	32079.824244	32.385690
655.807290	32124.949540	32.390708
656.086747	32174.443298	32.395725
656.755077	32204.588970	32.400743
657.003014	32259.644656	32.405760
657.378667	32303.990473	32.410778
658.297777	32352.917267	32.415796
658.909068	32415.654680	32.420813
659.867420	32465.473328	32.425831
660.274837	32518.797978	32.430848
661.120132	32564.601127	32.435866
661.907957	32607.600090	32.440884
662.259452	32665.751089	32.445901
662.660110	32719.949726	32.450919
663.095948	32776.286160	32.455936
664.055901	32832.812999	32.460954
664.758169	32875.572956	32.465972
665.666242	32937.854813	32.470989
666.729075	32986.191745	32.476007
667.243489	33037.686655	32.481024
668.100389	33080.505146	32.486042
668.443025	33126.583762	32.491060
669.229904	33182.259729	32.496077
670.089400	33227.840853	32.501095
670.928001	33270.820636	32.506112
671.386374	33323.311217	32.511130
672.020394	33366.417875	32.516148
672.658618	33427.719019	32.521165
673.285412	33467.267656	32.526183
673.496360	33517.413797	32.531200
674.230845	33564.665197	32.536218
675.368083	33612.081604	32.541236
675.866405	33664.920865	32.546253
676.652769	33708.820075	32.551271
677.432564	33757.070086	32.556288
677.770387	33811.951489	32.561306
678.768474	33848.345152	32.566324
679.364148	33900.411181	32.571341
679.870674	33940.725462	32.576359
680.863646	33985.870189	32.581376
681.035595	34037.452481	32.586394
682.044027	34074.641537	32.591412
682.378422	34120.951225	32.596429
683.175933	34156.984664	32.601447
684.043156	34204.400190	32.606464
684.439057	34254.481365	32.611482
684.832833	34304.954979	32.616500
685.697730	34360.900117	32.621517
686.579518	34402.162128	32.626535
687.201375	34455.540519	32.631552
688.084998	34504.945736	32.636570
689.202353	34550.464307	32.641588
689.578703	34607.706389	32.646605
690.147717	34645.160858	32.651623
690.982835	34693.568794	32.656640
691.521782	34753.624763	32.661658
692.141388	34796.736603	32.666676
692.857644	34852.921155	32.671693
693.824787	34898.590314	32.676711
694.997763	34950.493203	32.681728
695.892329	34978.514884	32.686746
696.758652	35016.050183	32.691764
697.188870	35058.047649	32.696781
698.301141	35098.181335	32.701799
698.935197	35138.825803	32.706816
699.342702	35179.922911	32.711834
700.335769	35208.991770	32.716852
701.053302	35250.028108	32.721869
701.563257	35291.754397	32.726887
701.918082	35337.823317	32.731904
702.624969	35381.928074	32.736922
703.319016	35421.684892	32.741940
703.852379	35468.952911	32.746957
704.496001	35512.169961	32.751975
705.624306	35568.804417	32.756992
706.358867	35611.008516	32.762010
707.373497	35651.733828	32.767028
707.587569	35692.065372	32.772045
708.572298	35735.109644	32.777063
709.237602	35772.323503	32.782080
709.839227	35828.345132	32.787098
710.610521	35859.548595	32.792116
711.058508	35916.062263	32.797133
711.352440	35966.599650	32.802151
712.173926	36020.146929	32.807168
712.690389	36070.586692	32.812186
713.686889	36118.675596	32.817204
714.652072	36166.333200	32.822221
715.202593	36217.754391	32.827239
716.129984	36280.081071	32.832256
716.615691	36329.837035	32.837274
717.582819	36368.484534	32.842292
718.239415	36427.470998	32.847309
718.778182	36473.241859	32.852327
719.361899	36525.663988	32.857344
720.104930	36573.565750	32.862362
721.007204	36617.946170	32.867380
721.834876	36680.662610	32.872397
722.201387	36725.537658	32.877415
723.157893	36774.759786	32.882432
723.656920	36831.811731	32.887450
724.558524	36881.428363	32.892468
725.460143	36933.599668	32.897485
725.773464	36976.732007	32.902503
726.572989	37022.836526	32.907520
727.108954	37073.402094	32.912538
728.291329	37109.924454	32.917556
729.078445	37158.554162	32.922573
729.601388	37193.124266	32.927591
730.527591	37254.107133	32.932608
730.957969	37293.156032	32.937626
731.669140	37328.911124	32.942644
732.200102	37392.946827	32.947661
732.924399	37438.937489	32.952679
733.256668	37495.694678	32.957696
733.960077	37549.567704	32.962714
735.083126	37594.111814	32.967732
736.057366	37642.327769	32.972749
736.755257	37698.674471	32.977767
737.269367	37757.819583	32.982784
737.979941	37812.843018	32.987802
738.717237	37860.773856	32.992820
739.575864	37915.382454	32.997837
740.381280	37969.133158	33.002855
740.917367	38025.543848	33.007872
741.364383	38092.731161	33.012890
742.410637	38145.900996	33.017908
743.297755	38209.649726	33.022925
744.007468	38260.861348	33.027943
745.182106	38308.775696	33.032960
745.859943	38373.113965	33.037978
746.419406	38428.295297	33.042996
747.128561	38477.642058	33.048013
747.622718	38538.986725	33.053031
748.772283	38597.181538	33.058048
749.010200	38655.157973	33.063066
750.114662	38716.882418	33.068084
751.095795	38762.627256	33.073101
752.035229	38813.241624	33.078119
753.371824	38853.644693	33.083136
754.377034	38899.335485	33.088154
755.027921	38939.529271	33.093172
755.854802	38988.251797	33.098189
756.580541	39029.825329	33.103207
757.307539	39073.175732	33.108224
758.081288	39129.470111	33.113242
758.753199	39161.977607	33.118260
759.731074	39198.016813	33.123277
760.296287	39243.928602	33.128295
761.301410	39286.863033	33.133312
761.709315	39337.093409	33.138330
762.500751	39385.088780	33.143348
763.191038	39428.515175	33.148365
763.813031	39477.201138	33.153383
764.852863	39515.564755	33.158400
765.297724	39575.592020	33.163418
766.029317	39611.967482	33.168436
767.097968	39675.553166	33.173453
767.589145	39716.785097	33.178471
768.090376	39773.534635	33.183488
768.613263	39826.891277	33.188506
769.504366	39878.628696	33.193524
770.340085	39928.686339	33.198541
771.090453	39990.646623	33.203559
772.141218	40057.012476	33.208576
772.288655	40102.864640	33.213594
773.259882	40159.636887	33.218612
773.855973	40214.696923	33.223629
774.353559	40271.903670	33.228647
775.267574	40341.396836	33.233664
775.963929	40398.104985	33.238682
776.938654	40454.788921	33.243700
778.180752	40509.837682	33.248717
778.295374	40556.088010	33.253735
779.112944	40597.454209	33.258752
779.849333	40658.254913	33.263770
780.402129	40713.670786	33.268788
781.333753	40771.184413	33.273805
781.838773	40818.285224	33.278823
782.655787	40878.821021	33.283840
783.399210	40946.616137	33.288858
784.316495	40997.207439	33.293876
785.404441	41063.191115	33.298893
785.595232	41131.389051	33.303911
786.709188	41180.995181	33.308928
787.268901	41250.091044	33.313946
788.231708	41315.702849	33.318964
788.917196	41375.786166	33.323981
789.634798	41445.477866	33.328999
790.551403	41503.931788	33.334016
791.354983	41574.673032	33.339034
792.494297	41627.716772	33.344052
793.481881	41694.483249	33.349069
794.101512	41754.963657	33.354087
795.197128	41803.144702	33.359104
795.896145	41880.436514	33.364122
796.414502	41935.285308	33.369140
797.963676	41979.999814	33.374157
799.088878	42057.055141	33.379175
800.139272	42094.858775	33.384192
800.731270	42140.247558	33.389210
801.514584	42192.797838	33.394228
802.090393	42234.084604	33.399245
803.026842	42291.177725	33.404263
803.890272	42339.345497	33.409280
804.688489	42394.740076	33.414298
805.390328	42441.990838	33.419316
806.390903	42490.637250	33.424333
807.167652	42543.056570	33.429351
808.143313	42598.190022	33.434368
808.722642	42658.236457	33.439386
809.247727	42719.448947	33.444404
810.126434	42762.447864	33.449421
810.759369	42823.049316	33.454439
811.854948	42877.937107	33.459456
812.552243	42941.197973	33.464474
813.492488	42994.238059	33.469492
814.230187	43041.958898	33.474509
815.059861	43104.933979	33.479527
816.148857	43146.420870	33.484544
817.395397	43207.699510	33.489562
818.208409	43255.086512	33.494580
818.721616	43304.474716	33.499597
819.795244	43357.419013	33.504615
820.189403	43404.061932	33.509632
821.124978	43460.936848	33.514650
821.471691	43510.174327	33.519668
822.315520	43565.084043	33.524685
822.678039	43631.226318	33.529703
823.823512	43696.374042	33.534720
824.560219	43753.457771	33.539738
825.487289	43812.789074	33.544756
826.497962	43871.076517	33.549773
827.027755	43929.843783	33.554791
827.799792	43995.720991	33.559808
828.666922	44056.896592	33.564826
829.281425	44126.581202	33.569844
830.136680	44181.035248	33.574861
830.907933	44251.511810	33.579879
831.633094	44308.130693	33.584896
832.715901	44370.772684	33.589914
833.321121	44423.412927	33.594932
834.014519	44467.152447	33.599949
834.664658	44534.726447	33.604967
835.639415	44597.107580	33.609984
836.396823	44664.405935	33.615002
837.040518	44730.716452	33.620020
837.781462	44785.872922	33.625037
838.790373	44850.823904	33.630055
839.875001	44916.775366	33.635072
840.525762	44989.158014	33.640090
841.000248	45042.262856	33.645108
842.621339	45113.470127	33.650125
843.262693	45180.642620	33.655143
844.397082	45232.999986	33.660160
845.487711	45294.314990	33.665178
846.091319	45351.980194	33.670196
847.187499	45409.511940	33.675213
848.167775	45476.012652	33.680231
849.056699	45526.422668	33.685248
850.024044	45582.735088	33.690266
850.588889	45644.531417	33.695284
851.616111	45703.485283	33.700301
852.095808	45771.987811	33.705319
853.639443	45834.695023	33.710336
854.131452	45887.603048	33.715354
855.218850	45947.762735	33.720372
856.610960	46002.681680	33.725389
856.568722	46068.192028	33.730407
857.821504	46123.961640	33.735424
858.606445	46182.752056	33.740442
859.376690	46249.041051	33.745460
860.613611	46303.504127	33.750477
861.316924	46366.261400	33.755495
861.784682	46425.626875	33.760512
862.682973	46488.777975	33.765530
862.856513	46563.314899	33.770548
864.243909	46631.210632	33.775565
865.047198	46696.300196	33.780583
865.731881	46765.861914	33.785600
866.731325	46833.299916	33.790618
867.349963	46912.146314	33.795636
868.709122	46973.885913	33.800653
869.525508	47048.893719	33.805671
870.120577	47116.066558	33.810688
871.278593	47188.054707	33.815706
871.798543	47260.325868	33.820724
873.047328	47319.995971	33.825741
874.090770	47388.839518	33.830759
874.813737	47454.905353	33.835776
875.938751	47517.802627	33.840794
876.728498	47586.888707	33.845812
877.922266	47638.989396	33.850829
878.507113	47702.610219	33.855847
879.886822	47765.924027	33.860864
881.167174	47810.236636	33.865882
881.866520	47870.778183	33.870900
882.922669	47918.599049	33.875917
883.909611	47974.288099	33.880935
884.647838	48025.802652	33.885952
885.859962	48077.363754	33.890970
886.373845	48134.366804	33.895988
887.475539	48187.779999	33.901005
888.157676	48247.996259	33.906023
888.901265	48304.280726	33.911040
889.678796	48361.831665	33.916058
890.383597	48416.249820	33.921076
891.289945	48472.578959	33.926093
891.778404	48536.223450	33.931111
892.339014	48595.580166	33.936128
893.517750	48648.305515	33.941146
894.489059	48704.447974	33.946164
895.071174	48753.881741	33.951181
896.114233	48815.574348	33.956199
896.816408	48858.973084	33.961216
898.031392	48921.290854	33.966234
898.923846	48976.275838	33.971252
900.135897	49023.442102	33.976269
900.885428	49088.123023	33.981287
901.635019	49148.394431	33.986304
902.659026	49201.879042	33.991322
903.350163	49272.554614	33.996340
904.166523	49332.455494	34.001357
904.978808	49391.066511	34.006375
905.921855	49460.469738	34.011392
906.792747	49532.453077	34.016410
907.656048	49603.305328	34.021428
908.359706	49665.730033	34.026445
909.202469	49734.719479	34.031463
910.017283	49811.938385	34.036480
911.172979	49876.172371	34.041498
911.968373	49954.021138	34.046516
912.598205	50024.531420	34.051533
913.847311	50098.273485	34.056551
914.870709	50155.252883	34.061568
916.402147	50227.053331	34.066586
917.217932	50305.830180	34.071604
918.412750	50361.492703	34.076621
919.004121	50429.504724	34.081639
920.047441	50505.114963	34.086656
921.082692	50563.801832	34.091674
921.813581	50631.141044	34.096692
922.738176	50697.672069	34.101709
923.883297	50765.168642	34.106727
924.823266	50831.469884	34.111744
925.571622	50890.107336	34.116762
926.829369	50963.920431	34.121780
928.227366	51024.437503	34.126797
929.365151	51080.041045	34.131815
929.960372	51135.697541	34.136832
930.775846	51185.574766	34.141850
931.494169	51248.912606	34.146868
932.369457	51321.793004	34.151885
933.169038	51385.865187	34.156903
934.358829	51453.072093	34.161920
935.464019	51511.218993	34.166938
936.397861	51583.875974	34.171956
937.245020	51647.764312	34.176973
938.333567	51705.294211	34.181991
938.891220	51774.283529	34.187008
939.778657	51846.992850	34.192026
940.559405	51909.272431	34.197044
941.284983	51983.949895	34.202061
942.318385	52056.877596	34.207079
942.952747	52134.860024	34.212096
944.134051	52204.557132	34.217114
945.264365	52283.026006	34.222132
945.829429	52350.123950	34.227149
946.700459	52429.506879	34.232167
947.602763	52507.784210	34.237184
948.687599	52571.138212	34.242202
949.709062	52651.270448	34.247220
950.468758	52727.381358	34.252237
951.404792	52800.529031	34.257255
952.129037	52884.403689	34.262272
953.193509	52947.723919	34.267290
954.010425	53034.014527	34.272308
954.577422	53098.589561	34.277325
955.792044	53171.397628	34.282343
956.741235	53247.499719	34.287360
957.729558	53316.236731	34.292378
958.532928	53392.710023	34.297396
959.343126	53469.714041	34.302413
960.568029	53551.665428	34.307431
961.400910	53632.728942	34.312448
962.324842	53700.546906	34.317466
963.454389	53781.628034	34.322484
964.038379	53864.692750	34.327501
965.165408	53946.103892	34.332519
966.026287	54030.075288	34.337536
967.123551	54110.890475	34.342554
967.964110	54196.422320	34.347572
968.968462	54273.177270	34.352589
970.320021	54355.010499	34.357607
971.454671	54443.598225	34.362624
972.373760	54519.911629	34.367642
973.471279	54599.861502	34.372660
974.087493	54674.400045	34.377677
975.360077	54755.278749	34.382695
976.262013	54839.297265	34.387712
977.269095	54918.844635	34.392730
977.993438	55008.314693	34.397748
979.486591	55088.527380	34.402765
980.804488	55165.217442	34.407783
981.724181	55250.728136	34.412800
982.843199	55321.735190	34.417818
983.883314	55400.601907	34.422836
984.425428	55474.306505	34.427853
985.849418	55556.303491	34.432871
986.391728	55642.519840	34.437888
987.610009	55714.006236	34.442906
989.113519	55801.586040	34.447924
989.667443	55871.897975	34.452941
990.973861	55945.478736	34.457959
992.032832	56026.255808	34.462976
992.890594	56087.059935	34.467994
994.184781	56162.370965	34.473012
995.007735	56239.957933	34.478029
996.385046	56318.787871	34.483047
997.370958	56390.185901	34.488064
998.312061	56453.237311	34.493082
998.879558	56524.390770	34.498100
1000.204796	56614.172049	34.503117
1001.377504	56687.598716	34.508135
1001.859399	56764.531666	34.513152
1002.930143	56833.057234	34.518170
1004.336636	56909.504976	34.523188
1004.627846	56989.658030	34.528205
1005.805360	57052.667895	34.533223
1007.044269	57136.433229	34.538240
1007.932378	57216.614377	34.543258
1009.102623	57294.631705	34.548276
1010.239010	57370.762222	34.553293
1010.801820	57448.355636	34.558311
1011.786395	57531.174632	34.563328
1012.814025	57593.645978	34.568346
1014.306536	57682.139441	34.573364
1015.151024	57755.082512	34.578381
1016.265620	57825.445830	34.583399
1017.545270	57909.093601	34.588416
1018.730916	57979.636182	34.593434
1019.944290	58043.731668	34.598452
1020.951562	58113.916336	34.603469
1021.901690	58170.325330	34.608487
1022.804347	58239.172222	34.613504
1023.297351	58294.000763	34.618522
1024.520821	58355.152463	34.623540
1025.057523	58416.284637	34.628557
1025.801156	58482.593668	34.633575
1026.830103	58553.757266	34.638592
1027.871117	58617.988707	34.643610
1029.116359	58699.264795	34.648628
1029.936386	58779.145288	34.653645
1031.235635	58846.558732	34.658663
1032.166150	58930.264394	34.663680
1033.246752	58991.882999	34.668698
1034.120022	59069.325707	34.673716
1034.796396	59153.748940	34.678733
1036.181061	59233.492407	34.683751
1036.995402	59317.071915	34.688768
1038.191255	59394.522414	34.693786
1039.140333	59475.556058	34.698804
1040.116985	59553.028525	34.703821
1041.279061	59629.301424	34.708839
1042.135492	59722.015538	34.713856
1043.354921	59803.957620	34.718874
1044.411422	59884.248011	34.723892
1045.844490	59977.791126	34.728909
1047.221461	60044.284345	34.733927
1048.259069	60130.167512	34.738944
1048.877085	60214.926323	34.743962
1050.435987	60292.848533	34.748980
1051.216261	60367.746347	34.753997
1052.401651	60440.941942	34.759015
1053.541974	60525.196441	34.764032
1054.700955	60595.788771	34.769050
1056.206802	60662.567445	34.774068
1056.904615	60748.980412	34.779085
1057.876695	60816.868015	34.784103
1059.188701	60905.572259	34.789120
1059.928761	60972.420342	34.794138
1061.292354	61055.129085	34.799156
1062.080548	61136.630050	34.804173
1063.263857	61217.132960	34.809191
1064.120531	61296.667862	34.814208
1065.034370	61379.662925	34.819226
1066.185362	61457.348505	34.824244
1067.132436	61555.999288	34.829261
1068.298626	61634.695859	34.834279
1069.532149	61724.896501	34.839296
1070.238510	61806.779567	34.844314
1071.298595	61887.082301	34.849332
1071.930740	61978.561202	34.854349
1073.431779	62056.947468	34.859367
1074.720283	62156.762891	34.864384
1075.670647	62239.894430	34.869402
1076.922560	62323.935167	34.874420
1077.387867	62415.530278	34.879437
1078.984648	62495.542555	34.884455
1079.636896	62590.286982	34.889472
1080.987130	62677.643323	34.894490
1082.456558	62758.777742	34.899508
1083.535174	62851.595699	34.904525
1084.399533	62920.676977	34.909543
1085.840246	63003.405579	34.914560
1086.766487	63095.773392	34.919578
1088.105136	63178.885627	34.924596
1088.855644	63267.628799	34.929613
1090.086707	63352.701799	34.934631
1091.255850	63430.074236	34.939648
1092.174574	63503.136858	34.944666
1093.305492	63590.777442	34.949684
1093.819400	63671.671088	34.954701
1094.824242	63746.645497	34.959719
1095.903281	63825.862713	34.964736
1096.838924	63910.705060	34.969754
1098.321302	63987.251811	34.974772
1098.634154	64080.332821	34.979789
1100.207935	64156.827881	34.984807
1101.371036	64236.520775	34.989824
1102.245807	64330.515494	34.994842
1103.135025	64409.814756	34.999860
1104.472903	64502.440241	35.004877
1106.012191	64586.963016	35.009895
1107.124752	64678.377068	35.014912
1108.054319	64763.014336	35.019930
1109.454047	64850.250309	35.024948
1110.225913	64932.139800	35.029965
1111.641774	65020.247508	35.034983
1112.908965	65109.467577	35.040000
1114.169143	65195.529937	35.045018
1115.323101	65277.342084	35.050036
1115.728774	65362.423781	35.055053
1117.103528	65453.280703	35.060071
1118.307147	65547.602317	35.065088
1119.568250	65643.067581	35.070106
1121.179576	65719.637538	35.075124
1121.975417	65803.552060	35.080141
1123.089828	65900.484611	35.085159
1124.883269	65982.680671	35.090176
1125.814960	66064.966817	35.095194
1126.909070	66142.346643	35.100212
1127.659084	66240.134940	35.105229
1128.954537	66309.595312	35.110247
1130.515349	66394.469023	35.115264
1131.407373	66498.953617	35.120282
1132.928607	66564.549155	35.125300
1133.822660	66646.938019	35.130317
1134.900718	66732.001966	35.135335
1136.147546	66821.408530	35.140352
1136.629182	66915.056208	35.145370
1138.016459	66996.653993	35.150388
1138.626645	67104.990089	35.155405
1140.070978	67194.633139	35.160423
1141.249574	67286.400905	35.165440
1142.355356	67378.028382	35.170458
1143.771307	67467.727462	35.175476
1144.785721	67571.823853	35.180493
1145.848209	67663.212164	35.185511
1147.307089	67748.384848	35.190528
1148.586097	67848.851201	35.195546
1149.673887	67928.814392	35.200564
1150.414797	68020.912521	35.205581
1151.979387	68117.074306	35.210599
1153.202853	68206.983229	35.215616
1154.115277	68304.861803	35.220634
1155.189787	68390.805602	35.225652
1156.272348	68486.461287	35.230669
1157.359147	68588.277454	35.235687
1158.485325	68686.181194	35.240704
1159.284178	68785.035371	35.245722
1161.363571	68866.290784	35.250740
1162.387883	68963.255331	35.255757
1163.463572	69048.226041	35.260775
1164.849661	69143.343038	35.265792
1165.756535	69227.061575	35.270810
1167.006545	69320.402147	35.275828
1168.480110	69412.226585	35.280845
1169.577712	69504.192185	35.285863
1170.902968	69588.593942	35.290880
1171.665616	69669.214691	35.295898
1172.687061	69742.348946	35.300916
1173.489276	69834.602315	35.305933
1174.500889	69912.797888	35.310951
1176.055157	69993.011483	35.315968
1176.566168	70091.351903	35.320986
1177.705313	70176.455749	35.326004
1179.061352	70271.663889	35.331021
1179.717821	70368.576979	35.336039
1181.063783	70472.354860	35.341056
1182.469944	70567.587944	35.346074
1183.783846	70661.974551	35.351092
1185.274269	70758.195712	35.356109
1186.098001	70856.560001	35.361127
1187.376873	70942.771753	35.366144
1188.545062	71039.601353	35.371162
1189.590466	71139.844572	35.376180
1190.723483	71246.824864	35.381197
1192.085805	71352.452759	35.386215
1193.303327	71451.327908	35.391232
1194.539522	71556.317684	35.396250
1195.898454	71651.574738	35.401268
1197.074484	71745.302810	35.406285
1198.603842	71850.754735	35.411303
1200.478933	71929.366547	35.416320
1201.863961	72021.555927	35.421338
1203.185733	72102.622770	35.426356
1204.012534	72189.415600	35.431373
1205.410384	72284.833543	35.436391
1206.593990	72373.851194	35.441408
1207.686312	72468.215474	35.446426
1208.992511	72559.000486	35.451444
1210.242475	72660.319560	35.456461
1211.064501	72753.283070	35.461479
1212.607100	72853.126131	35.466496
1213.641153	72951.389533	35.471514
1214.963333	73035.245613	35.476532
1216.124348	73123.104069	35.481549
1217.192351	73221.477180	35.486567
1218.513402	73307.208826	35.491584
1220.154196	73416.424066	35.496602
1221.123227	73503.275068	35.501620
1222.137365	73610.486114	35.506637
1222.934104	73711.968419	35.511655
1224.698039	73806.435586	35.516672
1225.507387	73906.384083	35.521690
1227.031531	74004.651097	35.526708
1227.909012	74099.143289	35.531725
1229.194147	74209.962419	35.536743
1230.405360	74310.749180	35.541760
1231.570749	74416.293315	35.546778
1233.076337	74517.351693	35.551796
1234.516656	74618.610609	35.556813
1235.977514	74717.966746	35.561831
1237.029602	74810.964970	35.566848
1237.872601	74911.266649	35.571866
1239.350165	75007.378628	35.576884
1240.975656	75107.546579	35.581901
1242.223516	75210.915018	35.586919
1243.391597	75301.325554	35.591936
1244.584413	75394.341896	35.596954
1245.789331	75495.868768	35.601972
1246.793439	75598.453296	35.606989
1247.962559	75704.483260	35.612007
1249.590835	75793.633132	35.617024
1250.467266	75890.867861	35.622042
1251.413481	75998.707057	35.627060
1252.962630	76097.725211	35.632077
1254.128227	76197.968805	35.637095
1255.310948	76288.076362	35.642112
1256.171134	76385.581410	35.647130
1257.384104	76474.595498	35.652148
1258.462340	76576.209489	35.657165
1259.645750	76683.064444	35.662183
1260.772015	76777.286641	35.667200
1261.982849	76894.728114	35.672218
1263.076964	76995.188462	35.677236
1264.582252	77101.222244	35.682253
1265.625578	77210.773933	35.687271
1266.933697	77320.031495	35.692288
1268.191422	77436.720616	35.697306
1269.220393	77551.786366	35.702324
1270.793470	77658.318476	35.707341
1271.980357	77773.436587	35.712359
1273.370122	77885.597314	35.717376
1274.657693	77997.331030	35.722394
1275.979470	78115.545905	35.727412
1277.457499	78218.636623	35.732429
1278.771540	78344.619221	35.737447
1280.196438	78450.734097	35.742464
1281.385956	78571.897876	35.747482
1283.062428	78681.850967	35.752500
1284.592588	78783.643528	35.757517
1285.859629	78903.453859	35.762535
1287.440490	79003.731804	35.767552
1288.558287	79104.892974	35.772570
1290.001320	79213.617678	35.777588
1291.861470	79320.884342	35.782605
1292.821298	79424.300941	35.787623
1294.438028	79523.536366	35.792640
1295.563826	79631.159243	35.797658
1296.871318	79727.453715	35.802676
1298.464176	79824.147514	35.807693
1299.365194	79933.782887	35.812711
1300.603097	80032.014917	35.817728
1302.072827	80148.213793	35.822746
1303.330297	80254.260311	35.827764
1305.016188	80348.344311	35.832781
1305.979437	80448.064833	35.837799
1307.408685	80547.181076	35.842816
1308.069908	80663.051859	35.847834
1309.427515	80778.079913	35.852852
1311.086629	80880.632936	35.857869
1312.145926	81003.956064	35.862887
1313.637184	81103.102638	35.867904
1315.096194	81220.283197	35.872922
1315.942645	81335.481794	35.877940
1317.366271	81444.699688	35.882957
1318.647431	81558.235175	35.887975
1320.325308	81665.602603	35.892992
1321.403786	81774.343378	35.898010
1323.083851	81884.270581	35.903028
1324.535999	81990.787506	35.908045
1325.763260	82096.858383	35.913063
1327.082943	82203.194013	35.918080
1328.650563	82312.126799	35.923098
1330.143937	82424.517798	35.928116
1331.441465	82518.403472	35.933133
1332.537597	82630.274300	35.938151
1334.384700	82724.429880	35.943168
1335.376463	82828.981740	35.948186
1336.698072	82935.041083	35.953204
1338.055385	83021.367675	35.958221
1339.215636	83130.772472	35.963239
1340.722096	83240.402551	35.968256
1342.479532	83339.705628	35.973274
1343.222012	83432.793799	35.978292
1345.024708	83510.500014	35.983309
1345.844533	83602.601076	35.988327
1347.230685	83687.772190	35.993344
1348.451264	83781.243225	35.998362
1349.297600	83888.368410	36.003380
1351.174935	83982.650169	36.008397
1352.307955	84084.257733	36.013415
1353.757487	84183.104850	36.018432
1355.082166	84270.796087	36.023450
1356.122807	84372.951231	36.028468
1357.353983	84468.158774	36.033485
1358.601638	84574.767913	36.038503
1360.208505	84675.898356	36.043520
1361.141541	84782.797988	36.048538
1362.460262	84904.032338	36.053556
1364.195554	85010.998016	36.058573
1365.532401	85124.868549	36.063591
1367.261740	85239.489401	36.068608
1368.526662	85346.998377	36.073626
1369.922084	85459.163163	36.078644
1371.132058	85561.650974	36.083661
1372.252896	85687.430434	36.088679
1374.024503	85787.386043	36.093696
1375.591899	85900.552166	36.098714
1376.857625	86019.480567	36.103732
1378.165680	86128.252895	36.108749
1379.523004	86233.659971	36.113767
1380.543588	86358.114750	36.118784
1381.996727	86471.275543	36.123802
1383.259154	86601.624114	36.128820
1385.128452	86711.781205	36.133837
1386.646422	86833.562868	36.138855
1387.905064	86955.613499	36.143872
1389.558094	87065.666200	36.148890
1390.696705	87198.748529	36.153908
1392.281986	87312.158135	36.158925
1393.201371	87443.666339	36.163943
1394.970631	87557.314377	36.168960
1396.087252	87678.465059	36.173978
1397.121895	87803.836220	36.178996
1398.951368	87926.739809	36.184013
1400.348113	88056.516376	36.189031
1401.675072	88185.075144	36.194048
1403.400090	88303.396444	36.199066
1404.305768	88431.857117	36.204084
1405.937891	88547.836751	36.209101
1407.454234	88683.540949	36.214119
1408.901496	88814.466209	36.219136
1410.258418	88927.144553	36.224154
1411.447417	89062.622638	36.229172
1413.201458	89182.501711	36.234189
1414.743529	89309.929348	36.239207
1416.413720	89430.481470	36.244224
1418.103641	89550.790223	36.249242
1419.976987	89656.547487	36.254260
1422.292900	89745.824468	36.259277
1423.596626	89850.961386	36.264295
1425.262685	89955.814160	36.269312
1426.666735	90050.696166	36.274330
1427.980486	90153.931596	36.279348
1429.527420	90253.785312	36.284365
1430.454250	90355.269365	36.289383
1431.637169	90457.512333	36.294400
1433.100176	90555.593159	36.299418
1434.250393	90674.178136	36.304436
1435.212214	90782.387860	36.309453
1436.811777	90881.322978	36.314471
1438.336364	90984.236963	36.319488
1439.444419	91079.966748	36.324506
1440.598267	91190.074462	36.329524
1441.865919	91286.210972	36.334541
1443.181569	91400.932898	36.339559
1444.264970	91509.848727	36.344576
1445.706198	91613.779080	36.349594
1446.752287	91739.203059	36.354612
1448.078047	91860.046710	36.359629
1449.632207	91995.303800	36.364647
1450.917743	92116.522285	36.369664
1452.646182	92227.165384	36.374682
1454.127930	92363.031074	36.379700
1456.047333	92488.499668	36.384717
1457.494896	92610.518741	36.389735
1458.791240	92733.487074	36.394752
1460.101600	92855.579183	36.399770
1461.492989	92986.632744	36.404788
1462.709762	93110.717669	36.409805
1464.240415	93252.308634	36.414823
1465.895971	93378.873959	36.419840
1467.771321	93506.102710	36.424858
1469.207378	93633.222917	36.429876
1470.696393	93764.289966	36.434893
1472.260117	93895.865619	36.439911
1473.440542	94024.294726	36.444928
1475.031017	94155.398352	36.449946
1476.562390	94290.149484	36.454964
1478.029223	94427.788507	36.459981
1479.682110	94547.438441	36.464999
1481.040559	94692.966809	36.470016
1482.581172	94826.134438	36.475034
1484.425968	94954.920325	36.480052
1485.863573	95081.349122	36.485069
1487.426989	95212.930441	36.490087
1488.973360	95352.779406	36.495104
1490.621612	95479.303795	36.500122
1492.163960	95614.756143	36.505140
1493.632072	95747.495366	36.510157
1495.402279	95875.320654	36.515175
1496.844242	96003.970778	36.520192
1498.594546	96122.977837	36.525210
1500.058005	96253.919971	36.530228
1501.438446	96392.379729	36.535245
1503.100427	96511.909054	36.540263
1503.763837	96639.478751	36.545280
1505.510008	96768.604389	36.550298
1507.063434	96917.471964	36.555316
1508.606305	97055.592463	36.560333
1509.831485	97186.740367	36.565351
1511.396771	97327.900873	36.570368
1513.412139	97459.053685	36.575386
1514.632007	97586.667373	36.580404
1515.798350	97724.836730	36.585421
1517.846322	97852.056393	36.590439
1519.479670	98000.270134	36.595456
1521.238592	98126.154140	36.600474
1522.612113	98258.944041	36.605492
1524.062350	98392.140888	36.610509
1525.922072	98504.370535	36.615527
1527.646527	98641.569642	36.620544
1529.437905	98760.428140	36.625562
1530.931705	98884.163310	36.630580
1532.187819	99003.714519	36.635597
1533.798478	99126.025293	36.640615
1535.442617	99246.036772	36.645632
1537.365667	99364.116399	36.650650
1538.619895	99488.385603	36.655668
1540.015425	99593.351245	36.660685
1541.599611	99695.486193	36.665703
1542.840819	99807.499754	36.670720
1544.403439	99928.249081	36.675738
1545.184277	100042.756488	36.680756
1546.605076	100159.332537	36.685773
1548.462159	100276.411590	36.690791
1549.599625	100400.791232	36.695808
1551.162711	100522.442816	36.700826
1552.439627	100661.850048	36.705844
1553.801992	100788.959902	36.710861
1555.359433	100917.662643	36.715879
1556.764053	101059.853489	36.720896
1558.308561	101196.799913	36.725914
1559.609766	101339.870173	36.730932
1561.258601	101486.271969	36.735949
1562.947882	101622.918737	36.740967
1564.252971	101778.541547	36.745984
1565.975203	101919.152661	36.751002
1567.610642	102073.495681	36.756020
1569.299793	102210.943651	36.761037
1571.221836	102349.813954	36.766055
1572.485992	102496.482995	36.771072
1574.701648	102650.269321	36.776090
1576.134209	102794.618689	36.781108
1577.814326	102930.891980	36.786125
1579.604065	103064.308774	36.791143
1581.111298	103216.699256	36.796160
1582.713561	103362.229161	36.801178
1584.749795	103503.571574	36.806196
1585.997001	103650.273735	36.811213
1587.838868	103794.234112	36.816231
1589.090746	103941.545417	36.821248
1590.670630	104073.781763	36.826266
1592.223210	104225.307648	36.831284
1594.178529	104378.686078	36.836301
1595.744476	104506.120942	36.841319
1597.038750	104666.589772	36.846336
1599.374884	104805.418597	36.851354
1600.638818	104958.514238	36.856372
1602.206097	105098.909383	36.861389
1603.849296	105236.630627	36.866407
1605.467442	105399.055894	36.871424
1607.354378	105532.568874	36.876442
1609.444134	105672.137002	36.881460
1610.762527	105811.711647	36.886477
1612.774861	105960.929520	36.891495
1614.311212	106084.494998	36.896512
1615.770045	106221.729090	36.901530
1617.351692	106356.915852	36.906548
1618.797874	106503.979908	36.911565
1620.648167	106642.929956	36.916583
1621.861938	106787.140388	36.921600
1623.516341	106927.795843	36.926618
1625.513768	107072.608275	36.931636
1626.814220	107216.819711	36.936653
1628.262407	107354.415068	36.941671
1629.916376	107503.809607	36.946688
1631.601876	107644.057401	36.951706
1633.233518	107791.174215	36.956724
1634.482918	107938.008780	36.961741
1636.494520	108087.464319	36.966759
1638.232431	108238.979304	36.971776
1639.333667	108386.460186	36.976794
1641.202922	108530.132102	36.981812
1642.875554	108684.246046	36.986829
1644.797179	108822.407616	36.991847
1646.074649	108973.185916	36.996864
1647.793641	109096.746507	37.001882
1649.319526	109233.183311	37.006900
1650.324616	109366.569521	37.011917
1652.154460	109509.947287	37.016935
1653.750010	109646.387547	37.021952
1655.549208	109792.916139	37.026970
1657.190149	109936.071435	37.031988
1658.176370	110078.821970	37.037005
1660.089167	110212.957816	37.042023
1661.377676	110373.340131	37.047040
1663.266965	110527.390453	37.052058
1664.841362	110670.102572	37.057076
1666.533842	110839.263064	37.062093
1668.017381	110996.878671	37.067111
1669.490670	111152.594341	37.072128
1671.232210	111310.386775	37.077146
1673.200167	111470.719053	37.082164
1674.634153	111638.287660	37.087181
1676.676767	111800.296478	37.092199
1678.588362	111961.349922	37.097216
1680.650487	112115.469028	37.102234
1682.709621	112268.714211	37.107252
1684.053880	112427.435806	37.112269
1685.843572	112584.490836	37.117287
1687.561965	112745.324244	37.122304
1689.248376	112904.172247	37.127322
1690.839968	113064.240523	37.132340
1692.466449	113227.005409	37.137357
1694.160146	113391.637558	37.142375
1695.933295	113550.918796	37.147392
1697.598146	113718.968494	37.152410
1699.557634	113862.711448	37.157428
1701.709618	114014.808191	37.162445
1703.776572	114171.839666	37.167463
1705.846515	114325.954338	37.172480
1707.284312	114471.734032	37.177498
1708.987993	114622.698234	37.182516
1710.521386	114778.306117	37.187533
1712.530332	114927.334324	37.192551
1714.676376	115085.562301	37.197568
1716.082383	115239.847580	37.202586
1717.679788	115382.270434	37.207604
1718.924806	115544.597736	37.212621
1720.656074	115704.427590	37.217639
1722.182398	115864.011003	37.222656
1723.892580	116033.294558	37.227674
1725.672013	116192.205833	37.232692
1727.016781	116359.581837	37.237709
1729.095217	116523.521349	37.242727
1730.833726	116689.328230	37.247744
1732.310582	116858.727968	37.252762
1733.819997	117016.086666	37.257780
1735.769485	117188.331570	37.262797
1737.400484	117356.631466	37.267815
1739.458554	117528.746886	37.272832
1741.102932	117692.784461	37.277850
1743.045875	117855.837677	37.282868
1744.521739	118029.136819	37.287885
1746.338753	118202.129982	37.292903
1748.415201	118372.622853	37.297920
1749.715135	118540.269265	37.302938
1751.651369	118701.817772	37.307956
1753.277230	118874.628132	37.312973
1755.175200	119041.168943	37.317991
1757.049417	119213.840718	37.323008
1758.731063	119377.841750	37.328026
1760.814899	119532.965197	37.333044
1762.076121	119705.303332	37.338061
1763.587201	119862.825841	37.343079
1765.617933	120014.255614	37.348096
1766.739483	120170.495444	37.353114
1768.652771	120323.492245	37.358132
1769.880784	120485.995719	37.363149
1771.756841	120641.904390	37.368167
1773.478181	120811.765757	37.373184
1774.811818	120992.597250	37.378202
1776.829008	121156.680497	37.383220
1778.603496	121336.392127	37.388237
1780.208479	121508.278891	37.393255
1781.768165	121680.617445	37.398272
1783.902635	121855.772216	37.403290
1786.060225	122025.723215	37.408308
1787.667136	122207.253561	37.413325
1789.385902	122380.394987	37.418343
1790.843574	122567.075119	37.423360
1792.753944	122757.021966	37.428378
1794.742844	122938.369382	37.433396
1796.221594	123136.909933	37.438413
1798.098621	123328.932478	37.443431
1799.765518	123522.726604	37.448448
1801.569389	123722.196287	37.453466
1803.558106	123904.093641	37.458484
1805.409555	124102.974276	37.463501
1807.519372	124286.973079	37.468519
1809.203607	124491.564996	37.473536
1811.197652	124683.677344	37.478554
1813.083834	124874.082078	37.483572
1814.628634	125068.537010	37.488589
1816.488153	125267.460219	37.493607
1818.585830	125458.722839	37.498624
1820.478775	125657.756943	37.503642
1822.622855	125850.802978	37.508660
1823.943426	126048.113911	37.513677
1826.153200	126251.389664	37.518695
1828.536016	126440.481178	37.523712
1830.017715	126634.953432	37.528730
1831.898349	126828.197335	37.533748
1834.085039	127016.979493	37.538765
1836.130144	127208.042823	37.543783
1837.977288	127399.340841	37.548800
1839.512742	127595.636192	37.553818
1841.426818	127775.266163	37.558836
1843.490133	127964.592029	37.563853
1845.904321	128139.705247	37.568871
1847.820188	128328.827352	37.573888
1849.538483	128506.587869	37.578906
1851.667087	128686.784693	37.583924
1853.389745	128864.952051	37.588941
1854.910769	129049.355717	37.593959
1856.759994	129235.130114	37.598976
1858.259777	129429.270080	37.603994
1860.258125	129618.981485	37.609012
1862.455342	129818.432315	37.614029
1864.046547	130001.167133	37.619047
1866.155813	130198.781031	37.624064
1867.270001	130378.292883	37.629082
1869.175142	130572.463812	37.634100
1870.919126	130776.062498	37.639117
1872.887648	130966.558530	37.644135
1874.434113	131160.826018	37.649152
1876.382711	131370.092635	37.654170
1878.138938	131560.992300	37.659188
1880.069303	131769.680039	37.664205
1882.258964	131962.252315	37.669223
1883.962500	132164.544279	37.674240
1885.271943	132362.102289	37.679258
1887.196367	132547.422588	37.684276
1889.183396	132741.387525	37.689293
1890.735635	132936.030046	37.694311
1892.659360	133132.353964	37.699328
1893.899743	133319.230504	37.704346
1895.986749	133511.952488	37.709364
1897.494624	133720.753381	37.714381
1898.975135	133926.032007	37.719399
1901.154270	134132.319482	37.724416
1902.486794	134346.124687	37.729434
1904.969672	134557.150623	37.734452
1906.639193	134780.828326	37.739469
1908.415179	135010.911316	37.744487
1910.521623	135225.945344	37.749504
1912.607252	135440.780612	37.754522
1914.975835	135660.483662	37.759540
1916.554512	135879.955415	37.764557
1918.427044	136095.867505	37.769575
1920.786291	136322.732112	37.774592
1922.564588	136545.437240	37.779610
1924.780351	136768.379925	37.784628
1926.531112	136984.061388	37.789645
1928.322759	137208.671137	37.794663
1930.682688	137427.077019	37.799680
1932.507712	137655.820660	37.804698
1934.617069	137883.696333	37.809716
1936.765222	138109.155978	37.814733
1939.055338	138326.206452	37.819751
1941.092187	138543.804965	37.824768
1942.897338	138772.772943	37.829786
1945.052069	138990.875495	37.834804
1947.009900	139205.151836	37.839821
1949.150568	139426.862669	37.844839
1951.234945	139635.981658	37.849856
1953.631896	139842.654416	37.854874
1956.188554	140062.894847	37.859892
1958.334206	140267.933415	37.864909
1960.540012	140460.234731	37.869927
1962.311974	140667.427145	37.874944
1963.966671	140872.113237	37.879962
1965.793522	141075.821596	37.884980
1967.896196	141283.688587	37.889997
1969.652973	141498.501508	37.895015
1971.808104	141706.907873	37.900032
1973.349102	141928.850578	37.905050
1975.223064	142128.774108	37.910068
1977.258623	142333.749789	37.915085
1979.279879	142566.941208	37.920103
1980.978892	142779.598585	37.925120
1982.565892	143007.719710	37.930138
1984.586889	143231.611562	37.935156
1986.785129	143456.492166	37.940173
1987.898364	143692.914279	37.945191
1990.507118	143918.710345	37.950208
1992.539955	144141.982587	37.955226
1994.432159	144367.562227	37.960244
1996.671143	144593.672737	37.965261
1998.594536	144831.243342	37.970279
2000.759993	145059.385397	37.975296
2002.519970	145284.393221	37.980314
2004.446138	145516.102945	37.985332
2006.469595	145734.243465	37.990349
2008.047643	145969.474370	37.995367
2010.278342	146209.021666	38.000384
2012.229463	146441.950172	38.005402
2014.159906	146672.217573	38.010420
2016.254870	146909.098500	38.015437
2017.981909	147145.847391	38.020455
2019.973210	147361.207511	38.025472
2021.953799	147584.642634	38.030490
2023.960380	147798.897943	38.035508
2025.988079	148011.995818	38.040525
2027.663034	148243.376140	38.045543
2029.838165	148468.815598	38.050560
2031.566357	148695.734479	38.055578
2033.684849	148918.341491	38.060596
2035.313388	149157.158362	38.065613
2037.254675	149395.584923	38.070631
2039.356164	149630.725516	38.075648
2041.371052	149873.229908	38.080666
2043.013832	150115.234811	38.085684
2045.443282	150359.860100	38.090701
2047.219029	150610.325580	38.095719
2049.665218	150858.733110	38.100736
2051.486106	151106.261705	38.105754
2053.709281	151362.309564	38.110772
2056.013680	151614.080974	38.115789
2057.639374	151872.369403	38.120807
2059.823792	152118.373547	38.125824
2061.901083	152392.042228	38.130842
2063.879293	152653.084741	38.135860
2066.338440	152895.012977	38.140877
2068.210708	153167.562249	38.145895
2070.769823	153419.213363	38.150912
2073.057288	153673.294343	38.155930
2075.330772	153932.925922	38.160948
2077.583070	154178.814325	38.165965
2080.168875	154440.849576	38.170983
2082.359331	154678.320870	38.176000
2084.673611	154936.947843	38.181018
2086.517564	155178.778481	38.186036
2088.825661	155415.307834	38.191053
2091.552782	155653.410518	38.196071
2093.836426	155878.038239	38.201088
2096.251910	156120.342418	38.206106
2097.912788	156362.549235	38.211124
2099.882911	156596.876364	38.216141
2101.647684	156840.935090	38.221159
2103.915871	157088.940695	38.226176
2105.697053	157333.532078	38.231194
2108.124584	157580.131211	38.236212
2110.067650	157829.459986	38.241229
2111.545008	158089.348268	38.246247
2113.699846	158339.141304	38.251264
2115.787656	158591.662539	38.256282
2117.265620	158855.184797	38.261300
2119.890612	159122.465173	38.266317
2121.523765	159382.512487	38.271335
2123.770805	159644.331564	38.276352
2125.913679	159909.684560	38.281370
2128.480446	160177.829177	38.286388
2130.362120	160437.994610	38.291405
2132.358950	160700.402998	38.296423
2134.659054	160977.365113	38.301440
2137.113685	161229.713111	38.306458
2139.516019	161498.549154	38.311476
2141.554717	161748.729532	38.316493
2143.896856	162013.590692	38.321511
2146.017547	162279.680816	38.326528
2147.780127	162538.070637	38.331546
2150.098175	162805.452590	38.336564
2152.466914	163053.199876	38.341581
2154.217079	163317.523738	38.346599
2156.572982	163573.324247	38.351616
2158.621599	163833.858427	38.356634
2160.835827	164085.239360	38.361652
2162.903594	164329.610372	38.366669
2164.717966	164584.584967	38.371687
2166.469816	164833.666511	38.376704
2168.604501	165075.731828	38.381722
2170.569307	165323.893313	38.386740
2172.901385	165573.280892	38.391757
2174.810910	165828.346980	38.396775
2177.046751	166075.783438	38.401792
2179.028273	166339.969017	38.406810
2180.897069	166606.153827	38.411828
2183.051705	166874.783724	38.416845
2185.201354	167141.333184	38.421863
2187.736488	167416.838359	38.426880
2190.054596	167686.372819	38.431898
2191.829519	167968.892836	38.436916
2193.941505	168236.176054	38.441933
2196.127828	168510.901813	38.446951
2198.572627	168786.654955	38.451968
2200.706338	169072.894538	38.456986
2202.907159	169356.826645	38.462004
2205.394969	169640.118442	38.467021
2207.254199	169925.528024	38.472039
2209.538456	170219.138476	38.477056
2212.477000	170502.604727	38.482074
2214.275623	170795.658199	38.487092
2217.063862	171085.435262	38.492109
2219.292493	171371.199274	38.497127
2221.483711	171643.206134	38.502144
2224.058425	171922.671229	38.507162
2226.151409	172210.516542	38.512180
2228.438937	172497.608905	38.517197
2230.315505	172785.121838	38.522215
2232.601356	173075.238672	38.527232
2234.723792	173375.286285	38.532250
2237.276192	173668.601790	38.537268
2239.597820	173956.519627	38.542285
2241.736400	174252.111148	38.547303
2243.631164	174551.932044	38.552320
2246.232506	174845.764933	38.557338
2248.584579	175142.634436	38.562356
2250.717477	175436.390018	38.567373
2252.883875	175742.763407	38.572391
2255.144506	176045.809057	38.577408
2257.878560	176337.036283	38.582426
2259.793725	176641.356926	38.587444
2262.049437	176934.082909	38.592461
2264.487633	177233.384674	38.597479
2266.838878	177535.824851	38.602496
2269.221274	177832.242193	38.607514
2271.310499	178139.423736	38.612532
2273.893067	178431.773888	38.617549
2275.871032	178741.438423	38.622567
2278.049345	179051.377654	38.627584
2280.674679	179338.822540	38.632602
2282.759989	179651.927649	38.637620
2284.937374	179946.580921	38.642637
2286.991036	180255.604086	38.647655
2289.035079	180568.337883	38.652672
2291.601552	180879.950152	38.657690
2293.594520	181185.506455	38.662708
2295.961489	181502.206084	38.667725
2298.545039	181813.158535	38.672743
2300.677475	182121.515430	38.677760
2303.785433	182429.264359	38.682778
2305.634458	182731.419406	38.687796
2308.281155	183027.508054	38.692813
2310.737806	183333.050035	38.697831
2312.794444	183629.765747	38.702848
2314.973071	183921.764641	38.707866
2317.249897	184195.639853	38.712884
2319.144679	184481.385718	38.717901
2321.565653	184764.256649	38.722919
2323.382742	185060.988582	38.727936
2325.915011	185333.785838	38.732954
2327.852740	185637.206035	38.737972
2330.239921	185930.346738	38.742989
2332.406082	186232.971187	38.748007
2334.009223	186607.386367	38.753024
2336.741511	186909.594501	38.758042
2339.179362	187230.111539	38.763060
2341.037240	187540.356800	38.768077
2343.644940	187868.265998	38.773095
2345.525367	188184.554726	38.778112
2347.913207	188509.706127	38.783130
2349.937710	188838.623416	38.788148
2352.773572	189164.748429	38.793165
2355.386378	189488.394514	38.798183
2357.641230	189823.197066	38.803200
2360.085928	190157.818662	38.808218
2362.432353	190478.334017	38.813236
2365.071393	190802.132161	38.818253
2368.215579	191140.762599	38.823271
2370.727388	191467.782832	38.828288
2373.262304	191793.657349	38.833306
2375.281460	192118.241388	38.838324
2377.785202	192456.391023	38.843341
2380.694401	192767.782362	38.848359
2382.977543	193092.912126	38.853376
2385.693002	193414.165337	38.858394
2388.146302	193745.722127	38.863412
2390.423154	194081.015783	38.868429
2392.566281	194394.740256	38.873447
2394.807000	194732.301918	38.878464
2397.227821	195067.169301	38.883482
2399.566299	195399.738834	38.888500
2401.837812	195744.690037	38.893517
2404.210124	196081.980627	38.898535
2406.563106	196422.069211	38.903552
2409.080776	196748.340004	38.908570
2411.060334	197100.960477	38.913588
2413.453841	197449.326144	38.918605
2415.990249	197807.551659	38.923623
2418.359345	198162.019239	38.928640
2420.623342	198506.876756	38.933658
2423.278265	198863.282870	38.938676
2425.690124	199216.374601	38.943693
2428.088915	199571.425131	38.948711
2430.661066	199931.707710	38.953728
2433.187267	200271.422592	38.958746
2435.729431	200634.683478	38.963764
2437.885042	200986.371140	38.968781
2440.504308	201348.351510	38.973799
2442.829629	201712.207377	38.978816
2445.713641	202065.130283	38.983834
2448.113318	202427.578979	38.988852
2450.495179	202772.909955	38.993869
2452.787763	203128.035460	38.998887
2455.144055	203497.783617	39.003904
2457.474642	203844.547177	39.008922
2459.986685	204207.667849	39.013940
2462.354255	204562.835260	39.018957
2465.189961	204918.590948	39.023975
2467.384683	205281.051761	39.028992
2470.097459	205640.384276	39.034010
2472.742923	205998.483165	39.039028
2475.170313	206345.159902	39.044045
2477.772122	206675.552178	39.049063
2479.957974	207007.559282	39.054080
2482.309192	207326.661824	39.059098
2484.206002	207663.643096	39.064116
2486.584593	207995.647098	39.069133
2489.119590	208341.344940	39.074151
2491.651615	208686.992952	39.079168
2493.882138	209029.563791	39.084186
2495.920652	209382.986781	39.089204
2498.876226	209730.348594	39.094221
2501.441338	210083.690623	39.099239
2503.470994	210447.201598	39.104256
2506.035746	210809.181805	39.109274
2508.220020	211164.921656	39.114292
2510.941997	211541.663157	39.119309
2513.976068	211917.823113	39.124327
2516.196122	212283.593173	39.129344
2518.613981	212640.924318	39.134362
2521.164650	213015.026977	39.139380
2524.037123	213383.008534	39.144397
2527.100154	213744.101865	39.149415
2529.608144	214121.514907	39.154432
2531.929234	214493.444841	39.159450
2534.825538	214863.456576	39.164468
2537.851485	215235.836457	39.169485
2540.599096	215596.802914	39.174503
2542.772324	215975.438511	39.179520
2545.530335	216343.466269	39.184538
2548.253556	216710.991680	39.189556
2550.653677	217082.098813	39.194573
2553.061628	217447.133496	39.199591
2555.896194	217831.256601	39.204608
2558.648309	218194.129750	39.209626
2561.210091	218569.607714	39.214644
2563.214276	218948.983296	39.219661
2566.199471	219321.474404	39.224679
2568.467294	219707.287443	39.229696
2570.984477	220081.274447	39.234714
2573.548604	220464.526806	39.239732
2575.735487	220849.540136	39.244749
2578.720735	221237.909757	39.249767
2580.697234	221627.122441	39.254784
2583.447245	222020.914657	39.259802
2586.238296	222431.467313	39.264820
2588.688073	222830.717600	39.269837
2591.330862	223221.732452	39.274855
2594.056263	223635.598221	39.279872
2596.529025	224025.471132	39.284890
2599.284035	224430.517238	39.289908
2601.675443	224828.151182	39.294925
2604.637661	225229.608567	39.299943
2607.783511	225619.122877	39.304960
2610.736296	225998.912068	39.309978
2613.821705	226372.609035	39.314996
2616.530175	226753.401578	39.320013
2619.459489	227130.145875	39.325031
2622.138081	227511.933751	39.330048
2625.099799	227881.229505	39.335066
2627.525486	228256.883418	39.340084
2629.930581	228637.392630	39.345101
2632.504846	229003.699947	39.350119
2634.998986	229385.617723	39.355136
2637.900027	229757.081793	39.360154
2640.774891	230132.462028	39.365172
2643.109833	230499.364979	39.370189
2646.040745	230864.193518	39.375207
2647.983123	231240.759959	39.380224
2650.462784	231606.979385	39.385242
2653.472465	231959.220162	39.390260
2655.414971	232312.287331	39.395277
2658.178085	232653.439165	39.400295
2660.491920	233013.586656	39.405312
2662.837291	233373.119319	39.410330
2665.363688	233734.655884	39.415348
2667.724245	234099.469702	39.420365
2670.069222	234466.902274	39.425383
2672.452761	234856.074254	39.430400
2674.975054	235239.940311	39.435418
2677.557531	235622.247031	39.440436
2679.763539	236027.780233	39.445453
2682.240732	236419.705220	39.450471
2684.643275	236843.116640	39.455488
2687.024619	237241.381219	39.460506
2690.044795	237666.524634	39.465524
2692.335437	238096.379112	39.470541
2695.256414	238519.860255	39.475559
2698.123395	238949.141257	39.480576
2700.831122	239380.631154	39.485594
2703.781637	239801.641816	39.490612
2706.394767	240229.182257	39.495629
2709.180036	240667.059859	39.500647
2711.848548	241108.816249	39.505664
2714.768757	241546.569820	39.510682
2717.744697	241989.115203	39.515700
2720.111485	242435.539691	39.520717
2723.182516	242876.188862	39.525735
2725.689113	243323.148832	39.530752
2728.505551	243768.611753	39.535770
2731.303369	244221.926243	39.540788
2733.895920	244674.052408	39.545805
2737.011040	245121.472972	39.550823
2740.242124	245587.621876	39.555840
2742.950516	246033.732029	39.560858
2746.052890	246479.195622	39.565876
2748.701033	246934.127905	39.570893
2751.844634	247371.022337	39.575911
2754.470731	247817.319049	39.580928
2757.676050	248250.620063	39.585946
2760.745535	248694.711834	39.590964
2763.227304	249135.972684	39.595981
2766.546023	249568.211355	39.600999
2769.739394	250001.535343	39.606016
2772.760284	250433.945178	39.611034
2776.004022	250849.985622	39.616052
2778.594395	251284.289175	39.621069
2781.868170	251690.746196	39.626087
2785.119910	252102.362197	39.631104
2787.436621	252527.509409	39.636122
2790.559321	252932.030748	39.641140
2793.069495	253353.690893	39.646157
2795.990822	253757.885710	39.651175
2798.898498	254175.595187	39.656192
2801.516857	254592.713438	39.661210
2804.086339	255004.452960	39.666228
2806.407575	255423.621705	39.671245
2809.289703	255843.311523	39.676263
2811.889524	256273.509281	39.681280
2814.658615	256689.607087	39.686298
2817.414108	257116.501150	39.691316
2820.146341	257550.966927	39.696333
2822.583880	257974.707120	39.701351
2826.088044	258409.329263	39.706368
2828.323774	258841.327810	39.711386
2831.143658	259267.340999	39.716404
2833.653047	259696.855493	39.721421
2837.333194	260115.594279	39.726439
2839.934905	260530.638561	39.731456
2842.754229	260924.285887	39.736474
2845.475562	261315.356310	39.741492
2848.030264	261714.477766	39.746509
2850.455225	262111.179611	39.751527
2852.843550	262523.963907	39.756544
2855.667490	262938.253670	39.761562
2858.826658	263344.056997	39.766580
2861.508564	263765.858648	39.771597
2863.975307	264173.900184	39.776615
2867.322797	264604.992776	39.781632
2870.259505	265027.537156	39.786650
2873.110932	265452.429821	39.791668
2875.829068	265893.266720	39.796685
2878.571280	266327.672018	39.801703
2881.117364	266765.738005	39.806720
2883.629464	267218.919630	39.811738
2886.498154	267659.141161	39.816756
2889.329772	268122.402955	39.821773
2892.039334	268580.855820	39.826791
2895.268772	269031.250515	39.831808
2898.446976	269500.928250	39.836826
2901.147343	269965.014221	39.841844
2904.012907	270436.310561	39.846861
2907.165274	270904.156539	39.851879
2910.383198	271372.015294	39.856896
2913.252133	271832.509839	39.861914
2916.262071	272306.110500	39.866932
2919.100137	272782.529051	39.871949
2921.725954	273260.070095	39.876967
2924.923664	273735.005193	39.881984
2928.085985	274219.212991	39.887002
2931.127030	274690.078227	39.892020
2933.828568	275179.660094	39.897037
2936.986940	275657.307861	39.902055
2940.236361	276127.395990	39.907072
2943.188410	276621.298408	39.912090
2946.223559	277100.099675	39.917108
2948.918221	277588.245902	39.922125
2952.189260	278070.179068	39.927143
2955.029554	278561.445633	39.932160
2957.406366	279055.447711	39.937178
2960.907235	279545.817946	39.942196
2963.538666	280040.205744	39.947213
2966.746033	280530.208948	39.952231
2969.676658	281029.597221	39.957248
2972.697717	281522.670222	39.962266
2975.657064	282029.030719	39.967284
2978.661317	282521.185388	39.972301
2981.776185	283013.548024	39.977319
2984.842588	283508.327210	39.982336
2987.508412	284010.986494	39.987354
2990.806670	284500.567731	39.992372
2994.024037	285005.343252	39.997389
2996.866052	285499.635380	40.002407
3000.242170	286001.357101	40.007424
3002.799005	286510.617257	40.012442
3005.959586	286995.682153	40.017460
3009.021520	287501.047303	40.022477
3012.437917	288004.245889	40.027495
3015.367954	288501.015976	40.032512
3018.267057	288999.843811	40.037530
3021.410153	289493.475349	40.042548
3024.173802	289987.314479	40.047565
3027.309607	290480.964903	40.052583
3030.710183	290964.363116	40.057600
3033.731555	291460.486571	40.062618
3036.819666	291932.627036	40.067636
3039.707242	292403.068551	40.072653
3042.814690	292860.167810	40.077671
3045.830891	293309.711631	40.082688
3048.398890	293763.155706	40.087706
3051.547091	294224.122935	40.092724
3053.953354	294688.604230	40.097741
3056.841127	295151.356657	40.102759
3060.209992	295620.200094	40.107776
3063.301458	296096.902670	40.112794
3066.150392	296565.540125	40.117812
3068.790052	297047.281329	40.122829
3072.072462	297535.747860	40.127847
3074.814983	298030.768121	40.132864
3077.332876	298524.422677	40.137882
3080.160838	299033.688688	40.142900
3083.195232	299540.074552	40.147917
3086.133654	300058.732621	40.152935
3089.621888	300565.165375	40.157952
3092.305883	301088.295957	40.162970
3095.726522	301610.291406	40.167988
3098.903061	302142.067995	40.173005
3101.794321	302687.795067	40.178023
3105.185817	303211.962568	40.183040
3108.438156	303744.447474	40.188058
3111.418975	304282.452365	40.193076
3115.170190	304811.904079	40.198093
3118.476816	305347.334118	40.203111
3121.976274	305864.629637	40.208128
3125.143673	306399.054950	40.213146
3128.772949	306928.833684	40.218164
3131.665590	307460.549066	40.223181
3134.648242	307999.961243	40.228199
3137.939708	308526.425019	40.233216
3141.202152	309063.269153	40.238234
3144.159666	309595.053012	40.243252
3147.579774	310131.251686	40.248269
3150.634034	310674.760513	40.253287
3153.959313	311215.809778	40.258304
3156.471007	311758.730813	40.263322
3159.949271	312304.160209	40.268340
3162.958550	312839.859377	40.273357
3166.089341	313395.000166	40.278375
3169.496598	313945.522918	40.283392
3172.330256	314506.965484	40.288410
3176.078504	315046.458013	40.293428
3179.705694	315571.903011	40.298445
3183.140753	316110.746426	40.303463
3187.121604	316652.899183	40.308480
3190.441174	317186.646611	40.313498
3193.684370	317711.644178	40.318516
3197.804042	318226.830290	40.323533
3200.648652	318748.096317	40.328551
3203.658226	319268.848312	40.333568
3206.688694	319789.616210	40.338586
3209.852968	320310.509287	40.343604
3213.113960	320844.018278	40.348621
3216.475564	321373.673239	40.353639
3219.647092	321884.725655	40.358656
3222.549708	322420.985842	40.363674
3225.625688	322948.660936	40.368692
3228.646789	323473.216873	40.373709
3231.435633	324008.738599	40.378727
3234.656607	324540.456219	40.383744
3237.606840	325083.627171	40.388762
3240.992498	325624.261980	40.393780
3244.073758	326173.259265	40.398797
3246.934885	326711.550835	40.403815
3250.245899	327234.059882	40.408832
3252.726717	327768.311592	40.413850
3255.327989	328290.308378	40.418868
3258.517199	328809.872674	40.423885
3261.453258	329345.630715	40.428903
3264.906497	329871.025954	40.433920
3267.949679	330422.203204	40.438938
3271.063038	330958.292117	40.443956
3274.127316	331502.245746	40.448973
3277.347233	332057.507415	40.453991
3280.616450	332602.073172	40.459008
3284.137633	333173.076402	40.464026
3287.154423	333729.842040	40.469044
3290.725522	334298.613498	40.474061
3293.786071	334864.563929	40.479079
3297.184532	335429.387792	40.484096
3300.806158	336012.229163	40.489114
3303.781333	336577.989193	40.494132
3307.255663	337161.824563	40.499149
3310.996902	337750.986477	40.504167
3314.320130	338320.825241	40.509184
3317.703384	338902.008902	40.514202
3321.341063	339488.292454	40.519220
3325.171100	340063.858437	40.524237
3328.656033	340637.693400	40.529255
3331.991049	341214.129389	40.534272
3335.558138	341801.273434	40.539290
3338.916926	342383.443782	40.544308
3342.297607	342968.897992	40.549325
3345.388414	343555.985178	40.554343
3348.937993	344145.603132	40.559360
3352.122109	344735.851124	40.564378
3355.151011	345319.240612	40.569396
3358.850159	345910.960425	40.574413
3362.400551	346522.929348	40.579431
3365.725118	347111.871584	40.584448
3369.346711	347706.919217	40.589466
3372.460804	348288.316840	40.594484
3376.013032	348891.899528	40.599501
3379.934809	349490.519874	40.604519
3383.547986	350075.104730	40.609536
3386.909328	350672.979304	40.614554
3390.273672	351266.709547	40.619572
3394.273457	351857.743851	40.624589
3397.649076	352447.444612	40.629607
3401.736149	353019.022670	40.634624
3405.572453	353600.010239	40.639642
3408.753264	354177.007391	40.644660
3412.109456	354749.530071	40.649677
3415.424585	355327.752920	40.654695
3418.739825	355897.168146	40.659712
3421.966742	356494.599556	40.664730
3425.080050	357080.147795	40.669748
3428.326658	357671.469364	40.674765
3431.228526	358270.387383	40.679783
3434.806197	358864.397586	40.684800
3438.380473	359472.287742	40.689818
3441.463790	360067.897663	40.694836
3445.562338	360652.286363	40.699853
3448.936425	361259.031136	40.704871
3452.090492	361854.417294	40.709888
3455.845691	362450.838606	40.714906
3458.776001	363047.655113	40.719924
3462.375321	363653.327598	40.724941
3465.689034	364255.255753	40.729959
3469.494881	364858.793017	40.734976
3473.089520	365454.215440	40.739994
3476.148400	366059.795507	40.745012
3479.730930	366644.854058	40.750016
3483.065564	367200.467695	40.755021
3486.113571	367717.065831	40.760026
3489.218243	368193.707918	40.765031
3492.052794	368605.269999	40.770036
3494.541026	368980.245873	40.775040
3497.110472	369314.988369	40.780045
3499.307352	369596.689413	40.785050
3501.597566	369854.035792	40.790055
3503.187640	370052.170160	40.795060
3505.238022	370216.088555	40.800064
3506.450030	370363.420718	40.805069
3507.975510	370458.752656	40.810074
3509.352404	370523.241894	40.815079
3510.317295	370568.107255	40.820084
3511.568988	370584.653654	40.825088
3512.132268	370587.360564	40.830093
3513.394941	370547.940963	40.835098
3514.440218	370497.504513	40.840103
3515.070455	370436.107314	40.845108
3515.528191	370336.707237	40.850112
3516.060395	370226.219086	40.855117
3515.974948	370104.293160	40.860122
3516.592053	369974.940970	40.865127
3516.682447	369838.099660	40.870132
3517.261593	369689.571792	40.875136
3517.306669	369537.798250	40.880141
3517.323227	369374.138911	40.885146
3517.410743	369208.155739	40.890151
3517.300727	369025.434997	40.895156
3517.339333	368839.488894	40.900160
3517.482260	368663.890740	40.905165
3517.287313	368470.433168	40.910170
3517.097047	368281.571990	40.915175
3516.922472	368094.485534	40.920180
3517.374201	367901.533216	40.925184
3517.006831	367700.450032	40.930189
3516.764741	367498.329685	40.935194
3516.481303	367309.984723	40.940199
3516.105340	367121.729143	40.945204
3516.350338	366926.947751	40.950208
3515.992874	366745.318038	40.955213
3515.697681	366550.821422	40.960218
3515.275501	366356.419480	40.965223
3515.185913	366176.472210	40.970228
3515.139098	365982.517497	40.975232
3514.925937	365813.283865	40.980237
3514.633597	365626.174295	40.985242
3514.523113	365433.928167	40.990247
3513.911467	365271.232489	40.995252
3514.066910	365074.089604	41.000256
3513.974638	364905.619551	41.005261
3513.485007	364737.947217	41.010266
3513.490825	364560.871724	41.015271
3512.919775	364385.917662	41.020276
3513.016860	364216.499449	41.025280
3512.745166	364066.626680	41.030285
3512.894421	363901.924688	41.035290
3512.430180	363742.805740	41.040295
3512.198000	363588.935067	41.045300
3512.249998	363424.194722	41.050304
3511.791787	363272.212500	41.055309
3511.503906	363122.439092	41.060314
3511.331343	362968.860837	41.065319
3511.237407	362825.535391	41.070324
3511.216190	362675.489534	41.075328
3510.920221	362545.382282	41.080333
3510.934218	362393.830292	41.085338
3510.969683	362256.046941	41.090343
3510.194720	362110.308338	41.095348
3510.309731	361984.429158	41.100352
3510.051156	361859.801914	41.105357
3509.855901	361719.332979	41.110362
3509.863995	361585.692859	41.115367
3509.454224	361465.966518	41.120372
3509.359306	361335.949768	41.125376
3509.316598	361219.290970	41.130381
3509.156689	361093.628711	41.135386
3509.119966	360972.851286	41.140391
3508.594458	360859.518965	41.145396
3508.646991	360739.946500	41.150400
3508.702154	360628.200159	41.155405
3508.264502	360523.238978	41.160410
3508.434587	360413.710254	41.165415
3508.028773	360309.632814	41.170420
3508.146979	360199.171119	41.175424
3508.065139	360095.347480	41.180429
3508.278695	359988.732926	41.185434
3508.119175	359881.489902	41.190439
3507.693597	359781.174843	41.195444
3507.521414	359673.958469	41.200448
3507.540617	359567.830117	41.205453
3507.308521	359472.261619	41.210458
3507.335877	359372.510061	41.215463
3507.228443	359284.977625	41.220468
3507.327214	359188.086074	41.225472
3507.417396	359100.522357	41.230477
3507.255205	359010.837496	41.235482
3507.096531	358902.777654	41.240487
3506.812499	358822.971753	41.245492
3506.876449	358712.843487	41.250496
3506.650090	358627.614929	41.255501
3506.308036	358539.100305	41.260506
3506.392995	358464.598425	41.265511
3506.190774	358382.567614	41.270516
3506.139244	358292.278900	41.275520
3506.154669	358216.389451	41.280525
3506.520610	358133.024256	41.285530
3506.361166	358045.699686	41.290535
3506.184944	357983.207513	41.295540
3506.202861	357884.011696	41.300544
3505.908434	357813.659034	41.305549
3505.809178	357731.585048	41.310554
3506.087778	357655.399116	41.315559
3505.869938	357580.179770	41.320564
3506.022777	357499.031703	41.325568
3505.598249	357420.184376	41.330573
3505.387083	357358.662147	41.335578
3505.451135	357277.120672	41.340583
3505.199214	357211.614315	41.345588
3505.412091	357139.503771	41.350592
3505.274540	357068.591279	41.355597
3505.161389	356989.008185	41.360602
3505.203780	356928.106443	41.365607
3505.020381	356864.266107	41.370612
3505.111007	356801.984176	41.375616
3505.075750	356738.476346	41.380621
3505.080028	356673.538958	41.385626
3505.232015	356607.180586	41.390631
3504.964920	356542.361400	41.395636
3504.938550	356464.567977	41.400640
3504.911548	356399.380726	41.405645
3504.643179	356338.856595	41.410650
3504.688857	356273.124037	41.415655
3504.840842	356219.854059	41.420660
3505.174143	356158.143061	41.425664
3504.959575	356090.341083	41.430669
3504.618958	356029.497184	41.435674
3504.918585	355966.215246	41.440679
3504.654925	355916.338954	41.445684
3504.978711	355842.251096	41.450688
3504.848963	355774.053988	41.455693
3504.397485	355714.217965	41.460698
3504.691093	355650.758412	41.465703
3504.296627	355589.439124	41.470708
3504.458150	355537.157744	41.475712
3504.731376	355490.908046	41.480717
3504.612957	355427.969656	41.485722
3504.808262	355362.211901	41.490727
3504.748255	355303.712096	41.495732
3504.647442	355238.711831	41.500736
3504.221083	355191.452217	41.505741
3503.997319	355123.725828	41.510746
3504.117931	355064.282463	41.515751
3503.759790	355016.681550	41.520756
3504.302194	354962.484506	41.525760
3504.565285	354913.820919	41.530765
3504.319162	354857.662200	41.535770
3504.065008	354809.714370	41.540775
3504.061685	354753.873523	41.545780
3504.554347	354694.473234	41.550784
3504.440188	354644.825831	41.555789
3504.357990	354579.236711	41.560794
3504.359215	354527.385277	41.565799
3504.253455	354476.643356	41.570804
3504.387066	354409.520674	41.575808
3504.405245	354358.657607	41.580813
3503.995600	354310.250283	41.585818
3504.230254	354254.778203	41.590823
3504.015664	354192.258995	41.595828
3504.021835	354144.472987	41.600832
3504.161882	354095.013923	41.605837
3504.004915	354035.891413	41.610842
3504.466479	353974.130761	41.615847
3503.890917	353926.053682	41.620852
3503.834315	353876.446954	41.625856
3503.939875	353824.425627	41.630861
3504.069156	353774.688142	41.635866
3504.212925	353725.634612	41.640871
3503.660988	353678.290604	41.645876
3503.740929	353626.908392	41.650880
3503.840987	353575.421294	41.655885
3504.101284	353521.875724	41.660890
3503.982283	353465.338901	41.665895
3504.124654	353416.463039	41.670900
3504.069285	353367.007835	41.675904
3504.088918	353314.109406	41.680909
3503.555626	353261.754462	41.685914
3503.804125	353203.889068	41.690919
3503.773207	353172.705606	41.695924
3503.951498	353120.036351	41.700928
3504.087208	353067.907425	41.705933
3503.758621	353012.673341	41.710938
3503.751284	352959.626011	41.715943
3503.277253	352925.715213	41.720948
3503.264297	352869.948812	41.725952
3503.249395	352823.307944	41.730957
3503.470862	352779.375455	41.735962
3503.719180	352734.955769	41.740967
3503.502363	352686.490550	41.745972
3503.507048	352641.676527	41.750976
3503.641968	352604.213660	41.755981
3503.599830	352557.957929	41.760986
3503.956692	352511.055405	41.765991
3503.417742	352469.147245	41.770996
3503.536189	352423.628901	41.776000
3503.450981	352371.914508	41.781005
3503.411650	352330.513059	41.786010
3503.694714	352283.774202	41.791015
3503.508045	352226.483147	41.796020
3503.667830	352186.397746	41.801024
3503.625483	352147.538455	41.806029
3503.113820	352093.805595	41.811034
3503.318246	352041.206762	41.816039
3503.129384	352005.750874	41.821044
3503.302159	351961.494392	41.826048
3503.370346	351923.151438	41.831053
3503.330292	351877.962022	41.836058
3503.451414	351839.305698	41.841063
3503.132971	351796.065951	41.846068
3503.501769	351739.246823	41.851072
3503.138813	351700.411464	41.856077
3502.866103	351666.900143	41.861082
3503.334585	351620.080633	41.866087
3503.444560	351584.526940	41.871092
3503.286867	351539.075740	41.876096
3503.140301	351505.392102	41.881101
3503.212248	351467.378480	41.886106
3503.271653	351424.791194	41.891111
3503.377890	351377.519307	41.896116
3503.184242	351328.082485	41.901120
3503.011978	351291.708113	41.906125
3503.043070	351249.913022	41.911130
3503.286253	351215.761714	41.916135
3503.082241	351183.561042	41.921140
3503.193024	351134.178231	41.926144
3503.493538	351096.154026	41.931149
3503.286433	351055.310873	41.936154
3503.543719	351002.549608	41.941159
3503.501370	350960.206328	41.946164
3503.355451	350913.888133	41.951168
3503.104194	350874.983563	41.956173
3502.818369	350840.659979	41.961178
3503.142179	350793.556748	41.966183
3502.810651	350764.273421	41.971188
3503.173357	350713.528911	41.976192
3503.333202	350675.068538	41.981197
3503.075431	350639.596457	41.986202
3503.114636	350604.256068	41.991207
3503.017293	350568.962310	41.996212
3502.952959	350527.842074	42.001216
3503.429724	350485.391976	42.006221
3503.185079	350444.604740	42.011226
3503.272892	350391.436708	42.016231
3503.275686	350366.981763	42.021236
3503.301117	350321.678310	42.026240
3503.114941	350270.383007	42.031245
3503.178695	350227.818900	42.036250
3503.093182	350184.566182	42.041255
3502.782506	350152.838664	42.046260
3503.305286	350106.466106	42.051264
3503.350912	350074.861013	42.056269
3503.148572	350034.956414	42.061274
3503.620207	349984.448033	42.066279
3503.227268	349948.004817	42.071284
3503.234806	349900.974939	42.076288
3502.912062	349861.978602	42.081293
3503.111845	349815.172895	42.086298
3503.771300	349765.016265	42.091303
3503.313447	349738.014156	42.096308
3503.259745	349673.885042	42.101312
3503.241242	349644.043576	42.106317
3502.846187	349607.473206	42.111322
3503.289285	349553.841788	42.116327
3502.832731	349519.009537	42.121332
3503.122737	349483.679755	42.126336
3502.859457	349452.249239	42.131341
3503.238203	349413.041523	42.136346
3503.472100	349371.288736	42.141351
3502.932103	349326.249846	42.146356
3502.999428	349284.395762	42.151360
3502.745059	349251.718014	42.156365
3502.942355	349213.377207	42.161370
3503.068174	349163.582341	42.166375
3502.884477	349126.520957	42.171380
3503.249235	349086.501538	42.176384
3503.356432	349052.140342	42.181389
3503.219098	349013.953063	42.186394
3503.385486	348972.871242	42.191399
3503.015521	348934.974289	42.196404
3503.016793	348886.520318	42.201408
3502.895813	348855.753479	42.206413
3502.687204	348827.517011	42.211418
3502.968713	348780.392056	42.216423
3502.894685	348745.575728	42.221428
3502.838326	348713.807246	42.226432
3502.840807	348671.657413	42.231437
3502.603186	348634.273383	42.236442
3502.957355	348593.619466	42.241447
3502.798646	348560.671929	42.246452
3503.258076	348515.374721	42.251456
3502.921104	348476.048472	42.256461
3502.931317	348438.498544	42.261466
3503.245465	348399.375947	42.266471
3502.821893	348357.902147	42.271476
3502.607971	348326.335768	42.276480
3502.782059	348299.513788	42.281485
3502.514337	348256.032673	42.286490
3502.781860	348216.815427	42.291495
3502.810141	348193.727710	42.296500
3502.879753	348155.151325	42.301504
3502.800076	348116.801506	42.306509
3502.999471	348085.602762	42.311514
3502.746109	348048.296789	42.316519
3502.630814	348014.884350	42.321524
3502.508622	347976.947746	42.326528
3502.858729	347937.437673	42.331533
3502.638683	347905.032903	42.336538
3503.038812	347862.311715	42.341543
3502.621611	347838.632087	42.346548
3502.954996	347792.438297	42.351552
3502.958394	347762.413770	42.356557
3502.671541	347724.044893	42.361562
3502.845371	347682.909474	42.366567
3502.765661	347645.499759	42.371572
3502.809645	347611.070643	42.376576
3502.947635	347579.677600	42.381581
3502.673053	347548.170769	42.386586
3502.666390	347498.139794	42.391591
3502.186918	347469.893477	42.396596
3502.465313	347442.952886	42.401600
3502.583567	347410.901760	42.406605
3502.076640	347382.608796	42.411610
3502.691660	347343.666949	42.416615
3502.495104	347321.859343	42.421620
3502.773357	347286.478209	42.426624
3502.721319	347253.919549	42.431629
3502.551013	347212.760836	42.436634
3502.540516	347182.610835	42.441639
3502.695320	347147.248765	42.446644
3502.684181	347108.785431	42.451648
3502.575895	347081.421682	42.456653
3502.423725	347052.844426	42.461658
3502.484408	347005.954715	42.466663
3502.636853	346984.906124	42.471668
3502.559646	346950.342649	42.476672
3502.645124	346921.906263	42.481677
3502.546839	346885.007055	42.486682
3502.660867	346854.430609	42.491687
3502.293753	346827.412010	42.496692
3502.535465	346794.451266	42.501696
3502.378606	346767.399901	42.506701
3502.329096	346737.636923	42.511706
3502.257434	346698.089330	42.516711
3502.171225	346672.806537	42.521716
3502.037034	346642.293948	42.526720
3502.322343	346618.097360	42.531725
3502.416870	346595.989751	42.536730
3502.472732	346552.634033	42.541735
3502.564686	346537.416577	42.546740
3502.555859	346502.180987	42.551744
3502.822846	346469.266839	42.556749
3502.684763	346426.475036	42.561754
3502.535718	346385.540815	42.566759
3502.059367	346351.928667	42.571764
3502.598689	346323.929627	42.576768
3502.580015	346292.686881	42.581773
3502.404352	346269.222795	42.586778
3502.368325	346228.194525	42.591783
3502.187962	346203.663323	42.596788
3502.198143	346167.051538	42.601792
3502.394182	346139.944754	42.606797
3502.172048	346113.462347	42.611802
3502.470867	346089.288703	42.616807
3502.247680	346059.679273	42.621812
3501.989250	346029.897335	42.626816
3502.636784	345994.838742	42.631821
3502.342627	345974.570891	42.636826
3502.284474	345940.283080	42.641831
3502.130938	345910.077928	42.646836
3501.821935	345883.735980	42.651840
3502.222337	345858.783641	42.656845
3502.368964	345833.667382	42.661850
3502.628904	345800.016381	42.666855
3502.823859	345774.206105	42.671860
3502.764792	345736.511391	42.676864
3502.718666	345706.085950	42.681869
3502.349016	345668.439491	42.686874
3502.825234	345633.178366	42.691879
3502.618984	345615.057684	42.696884
3502.570586	345576.089918	42.701888
3502.570234	345542.224923	42.706893
3502.330280	345512.998991	42.711898
3502.293986	345475.122473	42.716903
3502.283373	345453.055904	42.721908
3502.439052	345423.793754	42.726912
3502.254191	345389.067464	42.731917
3502.514096	345356.356735	42.736922
3502.680424	345324.118178	42.741927
3502.517014	345297.956515	42.746932
3502.779085	345264.406352	42.751936
3502.675591	345218.734667	42.756941
3502.351158	345198.827008	42.761946
3502.348529	345160.792354	42.766951
3502.222721	345139.684219	42.771956
3502.194759	345111.314816	42.776960
3502.164792	345073.869087	42.781965
3502.178870	345050.400057	42.786970
3502.234104	345026.619509	42.791975
3502.118418	344996.611054	42.796980
3502.344319	344965.608701	42.801985
3502.872051	344945.085216	42.806989
3502.465144	344913.037172	42.811994
3502.445008	344884.717212	42.816999
3502.513569	344851.730678	42.822004
3502.287004	344809.687928	42.827009
3502.622960	344784.516009	42.832013
3502.215459	344759.764862	42.837018
3502.220287	344722.516733	42.842023
3502.253454	344681.806356	42.847028
3502.469618	344653.703684	42.852033
3502.436489	344626.072007	42.857037
3502.348316	344589.016180	42.862042
3502.585550	344561.520355	42.867047
3502.308970	344540.994664	42.872052
3502.240524	344500.249033	42.877057
3502.352268	344475.111778	42.882061
3501.967699	344451.602671	42.887066
3502.200545	344412.818639	42.892071
3502.121404	344392.592662	42.897076
3502.345596	344369.370146	42.902081
3502.410419	344343.858718	42.907085
3502.179808	344320.376414	42.912090
3502.246362	344286.169236	42.917095
3502.188218	344253.608648	42.922100
3502.311047	344222.875917	42.927105
3502.466501	344194.934869	42.932109
3502.167741	344166.428845	42.937114
3502.653881	344129.639108	42.942119
3502.614810	344101.677404	42.947124
3502.384795	344068.278921	42.952129
3502.705204	344032.328484	42.957133
3502.269478	344004.708106	42.962138
3502.424839	343976.080407	42.967143
3502.368976	343951.172255	42.972148
3502.687015	343921.705579	42.977153
3502.368526	343885.549302	42.982157
3502.182531	343852.220037	42.987162
3502.332561	343822.042079	42.992167
3502.284956	343798.937750	42.997172
3502.197802	343765.948980	43.002177
3502.304302	343741.701904	43.007181
3502.293975	343714.701589	43.012186
3502.498978	343681.006206	43.017191
3502.034426	343659.568487	43.022196
3502.129816	343627.008841	43.027201
3501.996307	343590.772619	43.032205
3501.630819	343581.447536	43.037210
3502.201357	343545.966185	43.042215
3502.160548	343527.589821	43.047220
3502.276156	343494.721794	43.052225
3502.360980	343463.231525	43.057229
3502.169672	343435.292971	43.062234
3502.214132	343400.783243	43.067239
3502.152117	343385.562918	43.072244
3502.221077	343350.032289	43.077249
3502.528463	343325.295994	43.082253
3501.978193	343294.718031	43.087258
3502.383886	343262.669128	43.092263
3502.132126	343237.867223	43.097268
3502.111423	343211.554634	43.102273
3502.017890	343186.092419	43.107277
3502.041345	343148.229464	43.112282
3502.147547	343128.940098	43.117287
3502.169550	343104.451463	43.122292
3501.993875	343086.248409	43.127297
3502.192998	343057.333453	43.132301
3501.888055	343031.598908	43.137306
3502.071304	343002.152426	43.142311
3502.262201	342978.349355	43.147316
3501.924694	342943.593496	43.152321
3501.792884	342931.002738	43.157325
3501.258415	342895.870661	43.162330
3501.644575	342885.436798	43.167335
3501.896697	342859.564587	43.172340
3501.828502	342836.640806	43.177345
3502.131881	342811.192831	43.182349
3501.945384	342785.846494	43.187354
3502.164316	342762.674572	43.192359
3502.062655	342738.637172	43.197364
3501.894412	342712.550576	43.202369
3502.188337	342692.926639	43.207373
3502.181647	342667.374250	43.212378
3502.401212	342639.447399	43.217383
3502.296626	342612.537174	43.222388
3501.903430	342587.095725	43.227393
3502.230553	342555.160104	43.232397
3502.211144	342522.769846	43.237402
3502.202388	342496.988816	43.242407
3502.397586	342476.795309	43.247412
3501.830229	342448.990759	43.252417
3501.981931	342431.168671	43.257421
3501.815332	342391.325763	43.262426
3502.383626	342367.310987	43.267431
3502.146130	342344.514934	43.272436
3502.076883	342324.565904	43.277441
3502.146556	342287.610184	43.282445
3501.756799	342262.269670	43.287450
3501.866944	342241.199325	43.292455
3501.678058	342231.973531	43.297460
3501.643632	342200.831225	43.302465
3502.031739	342169.928261	43.307469
3501.953116	342147.793881	43.312474
3501.868091	342122.761821	43.317479
3501.882793	342109.385162	43.322484
3501.690970	342083.352618	43.327489
3502.110830	342055.241570	43.332493
3501.808012	342047.940475	43.337498
3501.976168	342008.553578	43.342503
3501.737046	341997.733641	43.347508
3501.819486	341964.030243	43.352513
3501.829024	341943.534769	43.357517
3501.562687	341926.082600	43.362522
3501.802174	341906.288704	43.367527
3501.595765	341880.639685	43.372532
3501.977970	341869.392471	43.377537
3502.134001	341827.210282	43.382541
3502.087664	341812.037684	43.387546
3501.841875	341782.275532	43.392551
3501.947988	341763.163416	43.397556
3501.900717	341742.880082	43.402561
3502.069581	341712.544803	43.407565
3501.940018	341694.588118	43.412570
3502.066506	341664.386528	43.417575
3501.860117	341643.059955	43.422580
3502.079885	341612.106415	43.427585
3502.161966	341589.590694	43.432589
3502.019131	341570.262940	43.437594
3502.027956	341542.469717	43.442599
3501.705006	341523.093683	43.447604
3501.996861	341497.138002	43.452609
3502.284468	341473.573132	43.457613
3501.765381	341452.167966	43.462618
3502.194415	341424.029560	43.467623
3502.073801	341404.749111	43.472628
3502.001751	341363.364680	43.477633
3502.200352	341346.831541	43.482637
3501.923861	341322.642383	43.487642
3502.080217	341298.131578	43.492647
3502.202760	341272.329215	43.497652
3501.904494	341235.861912	43.502657
3501.987700	341215.456260	43.507661
3502.001217	341189.619949	43.512666
3502.172993	341162.182482	43.517671
3502.207491	341134.512081	43.522676
3501.744186	341118.437822	43.527681
3502.019395	341088.263451	43.532685
3502.112399	341075.306483	43.537690
3502.390136	341033.968945	43.542695
3501.796142	341010.591809	43.547700
3502.146603	340993.043195	43.552705
3502.513236	340957.107829	43.557709
3502.082370	340922.389920	43.562714
3502.082997	340891.800411	43.567719
3501.821325	340870.253123	43.572724
3501.963601	340850.346624	43.577729
3502.021297	340826.003410	43.582733
3501.825863	340798.470238	43.587738
3501.852345	340768.512294	43.592743
3501.887876	340742.265384	43.597748
3501.887239	340727.288632	43.602753
3502.131119	340694.347162	43.607757
3501.960512	340672.989006	43.612762
3502.019388	340654.137920	43.617767
3501.970248	340626.251285	43.622772
3502.269812	340599.708904	43.627777
3502.150498	340569.976903	43.632781
3501.917334	340542.881679	43.637786
3501.902327	340521.753499	43.642791
3501.990721	340502.312894	43.647796
3501.749314	340479.490813	43.652801
3501.966737	340457.589012	43.657805
3501.742998	340435.196430	43.662810
3502.058340	340411.117977	43.667815
3501.909786	340389.273084	43.672820
3502.152555	340357.679166	43.677825
3502.122230	340334.035872	43.682829
3501.625578	340313.999644	43.687834
3501.900219	340285.833505	43.692839
3501.559299	340270.121238	43.697844
3501.583761	340250.309021	43.702849
3501.889105	340222.672046	43.707853
3501.725560	340210.746385	43.712858
3501.711532	340185.040769	43.717863
3502.056330	340166.602640	43.722868
3501.909897	340137.027067	43.727873
3502.289611	340111.565266	43.732877
3502.178179	340093.986372	43.737882
3501.995508	340051.397063	43.742887
3501.906841	340029.288347	43.747892
3501.719038	340003.940211	43.752897
3502.166790	339984.595973	43.757901
3501.683767	339962.599439	43.762906
3501.871470	339936.455397	43.767911
3501.912519	339921.853245	43.772916
3501.697652	339892.186405	43.777921
3501.664829	339869.178903	43.782925
3501.773237	339849.836541	43.787930
3502.031533	339815.976591	43.792935
3501.803078	339803.018325	43.797940
3502.040368	339779.765305	43.802945
3501.924300	339758.372684	43.807949
3501.869339	339739.513400	43.812954
3502.118051	339705.629407	43.817959
3501.924782	339688.597049	43.822964
3501.768813	339664.133718	43.827969
3502.241999	339637.538175	43.832973
3502.027289	339617.152537	43.837978
3501.854008	339582.825523	43.842983
3501.836446	339552.847982	43.847988
3502.024264	339537.815975	43.852993
3502.083841	339512.327280	43.857997
3502.002464	339487.852221	43.863002
3502.024550	339470.175957	43.868007
3502.215106	339447.921715	43.873012
3501.869435	339422.521446	43.878017
3502.183786	339386.465490	43.883021
3501.760747	339359.653202	43.888026
3501.913952	339342.312474	43.893031
3501.635733	339315.477616	43.898036
3501.914459	339291.353250	43.903041
3501.704920	339262.371638	43.908045
3501.791268	339253.127665	43.913050
3501.695929	339216.448710	43.918055
3501.886454	339198.618956	43.923060
3501.780514	339184.013947	43.928065
3502.016453	339159.972438	43.933069
3501.654783	339134.294735	43.938074
3501.577004	339105.241635	43.943079
3501.758074	339093.236546	43.948084
3501.527656	339077.226839	43.953089
3501.901144	339051.129528	43.958093
3501.582941	339028.369328	43.963098
3501.684264	339010.985656	43.968103
3501.824299	338992.070205	43.973108
3501.539404	338981.205612	43.978113
3501.653225	338950.164529	43.983117
3501.892425	338935.302278	43.988122
3501.733644	338904.252718	43.993127
3501.879290	338886.328076	43.998132
3501.637881	338873.981791	44.003137
3501.721392	338844.242222	44.008141
3501.781606	338814.862264	44.013146
3501.869229	338795.217418	44.018151
3501.660178	338777.475064	44.023156
3501.512961	338770.403370	44.028161
3501.584989	338734.842197	44.033165
3501.583212	338723.018014	44.038170
3501.870098	338690.424019	44.043175
3502.050389	338676.486284	44.048180
3501.652711	338657.400040	44.053185
3501.535390	338636.769826	44.058189
3501.752949	338613.722557	44.063194
3501.929341	338585.773808	44.068199
3502.050500	338568.844565	44.073204
3501.905918	338559.992362	44.078209
3502.058608	338521.875486	44.083213
3501.879373	338498.584737	44.088218
3502.007123	338478.068873	44.093223
3502.169354	338447.909857	44.098228
3502.124928	338423.682620	44.103233
3501.880083	338403.377271	44.108237
3501.722752	338369.428060	44.113242
3501.964610	338349.250380	44.118247
3501.728819	338330.901657	44.123252
3501.946973	338311.897406	44.128257
3501.820146	338279.748864	44.133261
3501.729547	338261.504660	44.138266
3501.734083	338244.033962	44.143271
3501.629897	338219.815888	44.148276
3501.387299	338205.486046	44.153281
3501.704738	338177.209877	44.158285
3501.624387	338161.150980	44.163290
3501.682247	338141.713849	44.168295
3501.745797	338126.598874	44.173300
3501.539238	338103.871576	44.178305
3502.002801	338074.707977	44.183309
3501.981307	338051.722981	44.188314
3501.694805	338025.753064	44.193319
3501.746540	338008.096899	44.198324
3501.817550	337988.530490	44.203329
3502.046849	337954.215568	44.208333
3501.577385	337942.616487	44.213338
3501.745214	337904.750905	44.218343
3501.899301	337895.241745	44.223348
3501.699291	337870.758621	44.228353
3501.505705	337854.361191	44.233357
3501.491586	337836.689761	44.238362
3501.788075	337817.164462	44.243367
3501.910007	337795.199612	44.248372
3501.747135	337784.544539	44.253377
3501.966496	337757.020774	44.258381
3501.529392	337746.128633	44.263386
3501.938563	337721.067443	44.268391
3501.763896	337692.130004	44.273396
3501.519175	337673.324598	44.278401
3501.838628	337656.720094	44.283405
3501.587461	337636.847610	44.288410
3501.605759	337615.407379	44.293415
3501.852059	337584.598813	44.298420
3501.731315	337569.944596	44.303425
3501.861517	337541.035887	44.308429
3501.708832	337516.112847	44.313434
3501.577934	337497.340498	44.318439
3501.857399	337486.565644	44.323444
3501.447738	337455.681033	44.328449
3501.762529	337437.932797	44.333453
3501.694112	337425.050493	44.338458
3501.436360	337404.390570	44.343463
3501.677795	337381.567678	44.348468
3501.468786	337375.954850	44.353473
3501.685031	337343.319780	44.358477
3501.819747	337325.446929	44.363482
3501.485660	337304.798829	44.368487
3501.903917	337283.372456	44.373492
3501.461206	337266.250619	44.378497
3501.650857	337248.420043	44.383501
3501.661158	337229.015255	44.388506
3500.990363	337205.723879	44.393511
3501.443660	337193.599510	44.398516
3501.275226	337169.645039	44.403521
3501.651681	337153.311170	44.408525
3501.395608	337140.635980	44.413530
3501.427603	337124.075966	44.418535
3501.673341	337110.966652	44.423540
3501.589203	337088.524835	44.428545
3501.975943	337059.474103	44.433549
3501.865067	337053.871386	44.438554
3501.978850	337022.904954	44.443559
3501.489078	337010.927278	44.448564
3501.346239	336989.867782	44.453569
3501.678754	336959.350439	44.458573
3501.330983	336942.518843	44.463578
3501.605158	336919.639706	44.468583
3501.479189	336912.818650	44.473588
3500.979229	336897.663701	44.478593
3501.272729	336872.772513	44.483597
3501.272207	336868.907306	44.488602
3501.507442	336856.740468	44.493607
3501.702615	336831.355941	44.498612
3501.678588	336809.947254	44.503617
3501.963252	336791.389613	44.508621
3501.445237	336778.322738	44.513626
3501.719928	336747.432757	44.518631
3502.276450	336726.009974	44.523636
3501.799021	336705.917886	44.528641
3502.030026	336671.677787	44.533645
3501.877371	336658.910044	44.538650
3501.889387	336629.968146	44.543655
3501.728730	336603.545311	44.548660
3501.782346	336584.743781	44.553665
3502.065243	336558.379045	44.558669
3501.635040	336546.773409	44.563674
3501.686113	336521.716261	44.568679
3501.969524	336501.302218	44.573684
3501.846662	336480.417337	44.578689
3501.477301	336452.679035	44.583693
3501.387392	336430.441161	44.588698
3501.780139	336413.799259	44.593703
3501.670243	336394.895922	44.598708
3501.298728	336375.829839	44.603713
3501.681576	336363.283834	44.608717
3501.288022	336344.678922	44.613722
3501.682351	336323.128558	44.618727
3501.863550	336294.287224	44.623732
3501.464356	336282.600386	44.628737
3501.693871	336256.574344	44.633741
3501.694643	336246.630857	44.638746
3501.592664	336216.256804	44.643751
3501.543992	336197.903322	44.648756
3501.737663	336180.758241	44.653761
3501.339751	336151.676308	44.658765
3501.738666	336140.144971	44.663770
3501.835085	336122.099478	44.668775
3501.660149	336101.553089	44.673780
3501.533855	336084.915515	44.678785
3501.233096	336060.421427	44.683789
3501.514641	336035.887571	44.688794
3501.719381	336027.132981	44.693799
3501.975698	336004.205193	44.698804
3501.499811	335995.861684	44.703809
3501.565322	335971.590284	44.708813
3501.638883	335948.665470	44.713818
3501.575940	335929.195101	44.718823
3501.243778	335908.189878	44.723828
3501.607256	335893.383347	44.728833
3501.841040	335875.392651	44.733837
3501.571969	335856.437514	44.738842
3501.547796	335839.682213	44.743847
3501.649735	335828.044405	44.748852
3501.280405	335801.119409	44.753857
3501.434295	335785.023020	44.758861
3501.415931	335764.502943	44.763866
3501.412805	335749.270207	44.768871
3501.546858	335735.338549	44.773876
3501.202252	335717.412350	44.778881
3501.672851	335698.596344	44.783885
3501.559887	335676.234447	44.788890
3501.629060	335662.083975	44.793895
3501.455021	335635.382783	44.798900
3501.514831	335621.640656	44.803905
3501.517966	335603.482269	44.808909
3501.824027	335578.766276	44.813914
3501.400304	335569.905923	44.818919
3501.525804	335542.547696	44.823924
3501.431523	335541.265522	44.828929
3501.848918	335513.709263	44.833933
3501.651770	335503.567491	44.838938
3501.603763	335478.652213	44.843943
3501.772091	335460.722366	44.848948
3501.573731	335434.686035	44.853953
3501.906606	335421.766015	44.858957
3501.544815	335393.720560	44.863962
3501.369382	335379.404592	44.868967
3501.503076	335371.423852	44.873972
3501.327099	335341.620092	44.878977
3501.458221	335337.912261	44.883981
3501.313710	335318.454264	44.888986
3501.396076	335293.620301	44.893991
3501.228424	335283.804491	44.898996
3501.014979	335267.002090	44.904001
3501.309634	335253.757348	44.909005
3501.435468	335235.325370	44.914010
3501.872797	335218.497973	44.919015
3501.274996	335207.986128	44.924020
3501.359526	335184.931977	44.929025
3501.527073	335170.308239	44.934029
3501.544151	335168.754405	44.939034
3501.446971	335135.759248	44.944039
3501.682980	335122.040381	44.949044
3501.727213	335101.942538	44.954049
3501.517018	335080.383798	44.959053
3501.817532	335063.272440	44.964058
3501.365261	335045.210079	44.969063
3501.898708	335022.823494	44.974068
3501.402009	335004.640868	44.979073
3501.637920	334983.266971	44.984077
3501.699876	334961.742108	44.989082
3501.542054	334943.608446	44.994087
3501.386218	334924.991260	44.999092
3501.220716	334910.877021	45.004097
3501.549275	334888.267920	45.009101
3501.635318	334870.910096	45.014106
3501.486007	334854.072096	45.019111
3501.608246	334828.875572	45.024116
3501.443707	334818.067307	45.029121
3501.471087	334793.292431	45.034125
3501.480111	334789.527250	45.039130
3501.585913	334764.053487	45.044135
3501.932045	334740.322552	45.049140
3501.653460	334728.184109	45.054145
3501.386943	334700.631948	45.059149
3501.598421	334674.912791	45.064154
3501.385784	334660.856657	45.069159
3501.739467	334662.149682	45.074164
3501.559230	334632.142562	45.079169
3501.528156	334612.615680	45.084173
3501.597571	334589.258329	45.089178
3501.796268	334571.653947	45.094183
3501.825238	334543.699638	45.099188
3501.746624	334528.529014	45.104193
3501.937102	334509.043899	45.109197
3501.972866	334494.542133	45.114202
3501.972400	334471.373607	45.119207
3501.976029	334440.015245	45.124212
3501.544730	334423.627848	45.129217
3501.808839	334390.346922	45.134221
3501.429254	334379.571995	45.139226
3501.594557	334347.628886	45.144231
3501.836879	334328.262771	45.149236
3501.807860	334306.370204	45.154241
3501.557273	334294.939369	45.159245
3501.676960	334273.099939	45.164250
3501.722131	334247.635261	45.169255
3501.807491	334223.791985	45.174260
3501.909512	334207.626691	45.179265
3501.726831	334179.018371	45.184269
3501.355865	334167.580797	45.189274
3501.470392	334142.105255	45.194279
3501.704229	334118.772889	45.199284
3501.486219	334102.377594	45.204289
3501.618475	334073.720185	45.209293
3501.032993	334071.725989	45.214298
3501.267882	334051.521616	45.219303
3501.662714	334028.087844	45.224308
3501.592375	334024.284071	45.229313
3501.651361	334006.955491	45.234317
3501.489131	333995.892304	45.239322
3501.630564	333968.072661	45.244327
3501.558330	333950.611879	45.249332
3501.421670	333933.771497	45.254337
3501.797424	333918.835113	45.259341
3501.674146	333893.549004	45.264346
3501.646927	333872.418883	45.269351
3501.802824	333848.818719	45.274356
3501.485339	333833.354362	45.279361
3501.737261	333814.851200	45.284365
3501.720929	333795.499629	45.289370
3501.944206	333768.862441	45.294375
3501.772143	333747.805655	45.299380
3501.642968	333726.462423	45.304385
3501.641478	333703.598777	45.309389
3501.561947	333686.774827	45.314394
3501.362729	333666.815831	45.319399
3501.929613	333648.212710	45.324404
3501.351698	333637.188671	45.329409
3501.305855	333614.052112	45.334413
3501.287408	333589.334440	45.339418
3501.134269	333582.771328	45.344423
3501.814811	333561.912389	45.349428
3501.647348	333548.230301	45.354433
3501.567639	333531.762370	45.359437
3501.362483	333506.234414	45.364442
3501.531173	333491.940472	45.369447
3501.778380	333468.910820	45.374452
3501.410523	333458.235534	45.379457
3501.394994	333425.938291	45.384461
3501.415696	333417.135432	45.389466
3501.404358	333404.370016	45.394471
3501.379511	333382.857758	45.399476
3501.482053	333374.372782	45.404481
3501.472986	333343.981937	45.409485
3501.199217	333323.958061	45.414490
3501.127328	333320.637685	45.419495
3501.414078	333292.667767	45.424500
3501.303399	333284.928076	45.429505
3501.546561	333269.986637	45.434509
3501.260568	333253.474386	45.439514
3501.281882	333240.830999	45.444519
3501.815622	333221.342670	45.449524
3501.180251	333223.171152	45.454529
3501.060190	333202.792663	45.459533
3501.266126	333189.026907	45.464538
3501.433738	333171.655608	45.469543
3501.501965	333161.141276	45.474548
3501.584421	333136.127842	45.479553
3501.512429	333126.906977	45.484557
3501.389180	333102.434195	45.489562
3501.361609	333091.604119	45.494567
3501.524634	333075.556015	45.499572
3501.021363	333053.075258	45.504577
3501.273971	333041.921804	45.509581
3501.287910	333032.687544	45.514586
3501.052468	333013.649435	45.519591
3501.337569	332995.954574	45.524596
3501.531668	333000.629678	45.529601
3501.700427	332975.729875	45.534605
3501.226271	332954.338159	45.539610
3501.220832	332935.009886	45.544615
3501.713676	332904.845785	45.549620
3501.676325	332904.851758	45.554625
3501.502129	332882.828358	45.559629
3501.576445	332859.265708	45.564634
3501.372518	332841.748608	45.569639
3501.515097	332815.123307	45.574644
3501.546513	332806.700140	45.579649
3501.411604	332788.104074	45.584653
3501.380467	332777.427065	45.589658
3501.404412	332753.414386	45.594663
3501.576243	332732.837623	45.599668
3501.581948	332718.263553	45.604673
3501.520931	332704.539163	45.609677
3501.370676	332682.613655	45.614682
3501.245438	332666.483068	45.619687
3501.572454	332646.085577	45.624692
3501.223505	332637.721562	45.629697
3501.541796	332611.221377	45.634701
3501.393000	332609.057413	45.639706
3501.408329	332583.087590	45.644711
3501.445861	332565.049552	45.649716
3501.380221	332556.209062	45.654721
3501.593128	332534.608460	45.659725
3501.591399	332513.092112	45.664730
3501.691963	332498.096259	45.669735
3501.420049	332479.597663	45.674740
3501.386138	332468.361460	45.679745
3501.299196	332452.402859	45.684749
3501.500127	332438.179806	45.689754
3501.327476	332411.323508	45.694759
3501.608832	332405.481021	45.699764
3501.588287	332384.959440	45.704769
3501.707625	332368.180261	45.709773
3501.403036	332338.266972	45.714778
3501.187179	332329.780443	45.719783
3501.528048	332308.719342	45.724788
3501.410051	332302.532044	45.729793
3501.554510	332277.381231	45.734797
3501.564321	332257.210930	45.739802
3501.375665	332240.555923	45.744807
3501.712274	332219.291966	45.749812
3501.579351	332208.935841	45.754817
3501.728083	332175.238554	45.759821
3501.487370	332095.210565	45.764826
3500.884540	332004.047848	45.769831
3500.823086	331855.116430	45.774836
3500.155423	331656.351624	45.779841
3499.538326	331422.758419	45.784845
3498.823941	331146.474512	45.789850
3498.422686	330830.131199	45.794855
3497.605746	330475.468756	45.799860
3496.625614	330091.298283	45.804865
3495.684917	329651.821307	45.809869
3494.262865	329179.780278	45.814874
3492.919772	328677.198046	45.819879
3491.758868	328134.747692	45.824884
3489.835656	327572.135476	45.829889
3488.521903	326975.182131	45.834893
3486.831523	326347.346511	45.839898
3484.815870	325693.223513	45.844903
3483.425245	324999.766801	45.849908
3481.735933	324289.657004	45.854913
3479.513203	323547.411921	45.859917
3477.258599	322769.542957	45.864922
3475.487307	321978.431792	45.869927
3472.935216	321154.583414	45.874932
3470.458642	320314.094296	45.879937
3468.601548	319442.682481	45.884941
3466.191195	318568.438902	45.889946
3463.327088	317659.849948	45.894951
3461.110334	316732.593502	45.899956
3458.493619	315796.856441	45.904961
3456.019594	314828.738086	45.909965
3453.184592	313836.126560	45.914970
3450.560161	312859.389832	45.919975
3447.908564	311840.269418	45.924980
3444.810400	310815.267537	45.929985
3441.616430	309772.700176	45.934989
3438.916881	308718.098553	45.939994
3435.648435	307659.898306	45.944999
3432.769719	306579.270960	45.950004
3429.475075	305501.331931	45.955009
3426.578565	304394.600862	45.960013
3423.857162	303292.654508	45.965018
3420.439882	302185.677746	45.970023
3417.184939	301044.522436	45.975028
3413.872022	299913.940133	45.980033
3410.672639	298771.786971	45.985037
3407.718665	297630.692216	45.990042
3404.129485	296478.448393	45.995047
3400.832806	295314.172669	46.000052
3397.280847	294153.171749	46.005057
3394.060104	292974.176386	46.010061
3390.658103	291800.379264	46.015066
3386.695240	290624.687021	46.020071
3383.914348	289438.199006	46.025076
3379.912507	288254.475638	46.030081
3376.609868	287062.119256	46.035085
3373.286344	285873.308875	46.040090
3369.729889	284671.046517	46.045095
3366.021653	283469.143347	46.050100
3362.356606	282273.425067	46.055105
3358.953739	281066.927735	46.060109
3355.246582	279876.421432	46.065114
3351.519066	278670.139561	46.070119
3348.019055	277460.519000	46.075124
3344.167387	276268.400974	46.080129
3341.054369	275056.468691	46.085133
3337.390892	273843.025707	46.090138
3333.587059	272642.012798	46.095143
3330.140334	271428.552953	46.100148
3326.404321	270235.160976	46.105153
3322.859180	269008.799822	46.110157
3318.918705	267799.366612	46.115162
3315.453680	266584.777050	46.120167
3311.898174	265382.231388	46.125172
3308.156811	264183.800403	46.130177
3304.279106	262964.546957	46.135181
3300.759998	261768.983049	46.140186
3297.275577	260550.380517	46.145191
3293.366953	259347.288948	46.150196
3289.666823	258147.387194	46.155201
3286.192429	256939.697224	46.160205
3282.736435	255730.210624	46.165210
3278.775821	254529.832428	46.170215
3274.980230	253322.847997	46.175220
3271.129587	252118.969270	46.180225
3267.407269	250924.356717	46.185229
3263.583242	249719.869899	46.190234
3260.064494	248532.288397	46.195239
3256.453873	247338.677507	46.200244
3252.248404	246146.603326	46.205249
3248.745397	244962.868094	46.210253
3245.079353	243783.022794	46.215258
3241.044277	242602.668484	46.220263
3237.784248	241423.028278	46.225268
3233.614800	240236.494976	46.230273
3230.198621	239063.694343	46.235277
3226.462965	237885.386792	46.240282
3222.561913	236718.358024	46.245287
3219.031890	235536.776137	46.250292
3214.724090	234381.366569	46.255297
3211.274698	233218.281810	46.260301
3207.798327	232050.945469	46.265306
3203.821555	230895.120476	46.270311
3200.224795	229728.486744	46.275316
3196.503099	228580.208847	46.280321
3192.584592	227424.218073	46.285325
3189.095972	226274.323375	46.290330
3184.779427	225127.460822	46.295335
3181.368908	223973.224270	46.300340
3177.444819	222852.610952	46.305345
3173.817608	221713.181663	46.310349
3170.310439	220582.012400	46.315354
3166.528020	219447.653037	46.320359
3162.590619	218322.132019	46.325364
3158.886265	217189.598579	46.330369
3154.992983	216066.749898	46.335373
3151.776369	214946.498591	46.340378
3147.808708	213829.067155	46.345383
3144.126262	212709.964995	46.350388
3140.226323	211592.403319	46.355393
3136.253211	210474.220654	46.360397
3132.686136	209367.796741	46.365402
3128.709871	208265.847400	46.370407
3124.949165	207153.478775	46.375412
3121.515750	206064.902771	46.380417
3117.901592	204978.398024	46.385421
3114.014302	203876.788575	46.390426
3110.038372	202795.064013	46.395431
3106.544033	201709.680202	46.400436
3102.834687	200628.768060	46.405441
3098.934536	199544.862233	46.410445
3095.386410	198466.537317	46.415450
3091.315104	197392.758233	46.420455
3087.767911	196333.777957	46.425460
3084.111216	195264.152473	46.430465
3080.226807	194199.231237	46.435469
3076.428930	193139.856834	46.440474
3072.621127	192087.445029	46.445479
3069.315602	191025.491096	46.450484
3065.539847	189982.413157	46.455489
3061.415551	188942.047332	46.460493
3057.479106	187900.414266	46.465498
3053.872509	186860.700685	46.470503
3049.924379	185826.245223	46.475508
3046.084282	184801.306892	46.480513
3042.561692	183771.593462	46.485517
3039.022008	182757.069724	46.490522
3034.830160	181739.068023	46.495527
3030.992341	180716.337258	46.500532
3027.186664	179714.772334	46.505537
3023.425876	178721.054087	46.510541
3019.735852	177719.977721	46.515546
3015.748291	176729.398695	46.520551
3012.255379	175741.644332	46.525556
3008.464790	174758.582140	46.530561
3004.929370	173780.444410	46.535565
3001.025525	172808.435752	46.540570
2996.913974	171836.127963	46.545575
2993.212713	170867.358630	46.550580
2989.531510	169908.222430	46.555585
2985.356437	168948.653762	46.560589
2981.569516	167989.877644	46.565594
2977.448395	167058.496060	46.570599
2974.112679	166118.934549	46.575604
2970.272544	165191.391336	46.580609
2966.144326	164266.031406	46.585613
2962.396081	163335.992090	46.590618
2958.326292	162427.234091	46.595623
2954.609337	161519.324972	46.600628
2950.545064	160617.286812	46.605633
2946.601694	159718.921145	46.610637
2942.988290	158833.168384	46.615642
2938.700657	157962.615350	46.620647
2934.968707	157082.913953	46.625652
2931.052238	156223.630224	46.630657
2927.092339	155361.795025	46.635661
2923.230253	154513.244019	46.640666
2919.045257	153668.828300	46.645671
2915.056787	152830.745001	46.650676
2911.027898	152018.018135	46.655681
2906.894044	151199.720164	46.660685
2902.949414	150393.634371	46.665690
2898.646602	149601.423490	46.670695
2894.733967	148816.926053	46.675700
2890.402139	148043.130940	46.680705
2886.791660	147287.724322	46.685709
2883.153091	146531.251453	46.690714
2878.435612	145791.932176	46.695719
2874.404076	145057.415768	46.700724
2870.552253	144327.971757	46.705729
2866.423596	143621.968200	46.710733
2862.474649	142910.602713	46.715738
2858.148500	142223.468435	46.720743
2854.198804	141540.903878	46.725748
2850.361627	140869.082631	46.730753
2846.104924	140203.583128	46.735757
2842.276361	139560.075174	46.740762
2838.020449	138916.833327	46.745767
2834.208537	138287.297068	46.750772
2830.163857	137670.527981	46.755777
2825.988159	136970.851106	46.760781
2822.413713	136357.156102	46.765786
2818.504057	135762.057348	46.770791
2814.874888	135174.644869	46.775796
2810.597357	134579.351813	46.780801
2806.846779	133997.761973	46.785805
2803.334360	133426.764931	46.790810
2799.454525	132871.899186	46.795815
2795.909372	132311.887293	46.800820
2792.391832	131753.277582	46.805825
2788.475406	131197.293991	46.810829
2785.311895	130647.077251	46.815834
2781.334060	130106.432746	46.820839
2777.776151	129553.493019	46.825844
2773.988332	129020.744684	46.830849
2770.349572	128482.039760	46.835853
2766.457065	127950.389769	46.840858
2762.872237	127417.083320	46.845863
2759.684360	126881.699601	46.850868
2756.068422	126360.469535	46.855873
2752.586369	125842.735705	46.860877
2749.511850	125312.137197	46.865882
2746.083743	124790.160305	46.870887
2742.371558	124255.999209	46.875892
2739.009827	123727.526648	46.880897
2735.195980	123206.673301	46.885901
2731.590188	122681.724665	46.890906
2727.531124	122165.018376	46.895911
2724.104016	121630.543035	46.900916
2720.802561	121131.613466	46.905921
2716.792825	120607.938205	46.910925
2713.579296	120098.491042	46.915930
2709.868045	119588.059851	46.920935
2706.832813	119063.694395	46.925940
2703.217203	118563.804213	46.930945
2699.342079	118053.126589	46.935949
2696.150984	117535.024851	46.940954
2692.267634	117024.578628	46.945959
2689.078871	116504.659645	46.950964
2685.252852	115997.117786	46.955969
2682.029584	115493.456338	46.960973
2678.339669	114992.837075	46.965978
2674.782706	114478.369785	46.970983
2671.174409	113973.759170	46.975988
2667.532163	113474.640949	46.980993
2664.059435	112970.175768	46.985997
2660.144059	112466.892696	46.991002
2656.500823	111977.992394	46.996007
2653.093689	111480.848688	47.001012
2649.499002	110989.792974	47.006017
2645.748356	110493.771810	47.011021
2642.196187	110012.627117	47.016026
2638.038605	109518.704495	47.021031
2634.412339	109033.185926	47.026036
2630.481993	108573.211235	47.031041
2626.955201	108107.014066	47.036045
2623.364114	107627.980585	47.041050
2619.159961	107180.245891	47.046055
2615.627496	106715.390574	47.051060
2611.822046	106260.830150	47.056065
2608.042398	105815.602464	47.061069
2604.201050	105371.483458	47.066074
2600.759880	104938.202002	47.071079
2597.324812	104494.577938	47.076084
2593.254524	104065.918265	47.081089
2589.807395	103636.264621	47.086093
2586.056714	103219.057097	47.091098
2582.170197	102792.342753	47.096103
2578.538382	102374.733339	47.101108
2575.171215	101955.855109	47.106113
2571.378705	101546.466873	47.111117
2567.750146	101130.563284	47.116122
2564.178909	100721.697503	47.121127
2560.503759	100308.086798	47.126132
2557.254262	99915.818480	47.131137
2553.489134	99507.926022	47.136141
2550.463985	99098.665341	47.141146
2546.561399	98695.964651	47.146151
2543.173201	98287.279217	47.151156
2539.498981	97887.361927	47.156161
2536.040854	97492.042073	47.161165
2532.947002	97080.111029	47.166170
2529.255576	96678.534145	47.171175
2526.270809	96278.682425	47.176180
2522.434968	95873.668925	47.181185
2519.119513	95467.906164	47.186189
2515.842536	95055.610850	47.191194
2512.072540	94651.251100	47.196199
2508.953973	94247.862689	47.201204
2505.189267	93834.058395	47.206209
2501.490126	93422.066595	47.211213
2498.246540	93015.625945	47.216218
2494.903662	92603.056027	47.221223
2491.230404	92191.330923	47.226228
2487.955301	91786.652384	47.231233
2484.134167	91371.098644	47.236237
2481.174283	90960.206821	47.241242
2477.337235	90550.715008	47.246247
2474.136748	90126.149548	47.251252
2470.719533	89714.265960	47.256257
2467.052307	89294.435226	47.261261
2463.860932	88876.289697	47.266266
2460.166729	88466.855091	47.271271
2456.687333	88044.027136	47.276276
2453.139591	87625.255998	47.281281
2449.681275	87206.946983	47.286285
2446.437919	86780.111255	47.291290
2443.205690	86361.067714	47.296295
2439.681973	85939.865069	47.301300
2436.303002	85514.758639	47.306305
2432.697273	85084.307400	47.311309
2428.992932	84662.071665	47.316314
2425.069706	84243.077423	47.321319
2421.733387	83808.665347	47.326324
2418.145053	83389.085261	47.331329
2414.477774	82967.897697	47.336333
2411.704329	82529.848062	47.341338
2408.148472	82106.852190	47.346343
2404.615725	81680.277059	47.351348
2401.051395	81251.935038	47.356353
2397.618054	80829.803026	47.361357
2394.374243	80397.410436	47.366362
2390.386858	79958.078317	47.371367
2387.328571	79517.478147	47.376372
2383.659272	79091.103522	47.381377
2379.911008	78664.061924	47.386381
2376.820521	78234.422567	47.391386
2373.164397	77800.750337	47.396391
2369.753186	77360.950783	47.401396
2366.005410	76927.840062	47.406401
2362.516998	76487.012518	47.411405
2359.279568	76050.432818	47.416410
2355.574718	75631.623083	47.421415
2352.117137	75187.624362	47.426420
2349.031138	74753.823173	47.431425
2345.388719	74316.788522	47.436429
2341.968770	73876.818427	47.441434
2337.966256	73442.609695	47.446439
2334.465822	73006.475993	47.451444
2331.245254	72573.988296	47.456449
2327.585393	72137.398496	47.461453
2324.207822	71691.794879	47.466458
2320.740146	71257.424514	47.471463
2317.260716	70812.004045	47.476468
2313.764654	70363.990902	47.481473
2310.042087	69939.026975	47.486477
2306.957225	69486.552862	47.491482
2303.126988	69053.488148	47.496487
2299.774260	68617.601351	47.501492
2296.129986	68176.193860	47.506497
2292.933064	67728.503517	47.511501
2289.566892	67293.422043	47.516506
2285.614307	66851.285549	47.521511
2282.122061	66402.445664	47.526516
2278.942171	65963.650999	47.531521
2275.204269	65523.903481	47.536525
2271.657666	65075.793746	47.541530
2268.221707	64634.967457	47.546535
2265.007664	64186.060171	47.551540
2261.386284	63748.750050	47.556545
2257.933658	63291.784764	47.561549
2254.553907	62847.833268	47.566554
2250.846663	62399.745682	47.571559
2247.253891	61956.471581	47.576564
2244.176493	61504.576896	47.581569
2240.457450	61056.223584	47.586573
2236.970218	60603.362124	47.591578
2233.428923	60150.841084	47.596583
2229.908437	59703.642907	47.601588
2226.203857	59262.027654	47.606593
2222.894367	58813.905565	47.611597
2219.562928	58348.262890	47.616602
2216.093871	57913.564705	47.621607
2212.408081	57452.677256	47.626612
2208.921607	57004.108692	47.631617
2205.502317	56549.567510	47.636621
2201.819604	56092.474603	47.641626
2198.181672	55658.192555	47.646631
2194.475057	55198.493837	47.651636
2191.248212	54742.624838	47.656641
2187.974172	54293.300253	47.661645
2184.735360	53835.160333	47.666650
2181.116513	53385.900371	47.671655
2178.131070	52925.156729	47.676660
2174.330285	52466.553690	47.681665
2170.396564	52014.888625	47.686669
2167.406108	51548.920356	47.691674
2163.692843	51091.605845	47.696679
2160.271009	50632.973664	47.701684
2156.263137	50174.670152	47.706689
2152.889051	49716.987550	47.711693
2149.430970	49258.033182	47.716698
2145.935051	48792.573498	47.721703
2142.570776	48336.870524	47.726708
2139.204233	47873.261520	47.731713
2135.592287	47419.752894	47.736717
2132.312543	46962.998786	47.741722
2128.811557	46504.417398	47.746727
2125.126020	46034.756478	47.751732
2121.678715	45574.771396	47.756737
2118.231931	45113.438526	47.761741
2114.951153	44645.937945	47.766746
2111.121562	44199.859057	47.771751
2107.434745	43721.330742	47.776756
2103.912507	43264.607337	47.781761
2100.421939	42797.083171	47.786765
2096.923490	42328.993101	47.791770
2093.256448	41880.335854	47.796775
2090.041095	41407.161345	47.801780
2086.529668	40950.693478	47.806785
2083.177031	40498.547295	47.811789
2079.800660	40018.637282	47.816794
2075.942138	39563.000643	47.821799
2072.384480	39105.989005	47.826804
2069.089703	38637.363103	47.831809
2065.686413	38175.864799	47.836813
2062.340679	37709.796557	47.841818
2058.635954	37244.333156	47.846823
2055.530216	36771.369606	47.851828
2051.425712	36298.629015	47.856833
2048.062308	35846.334854	47.861837
2044.579363	35373.023641	47.866842
2040.798032	34919.895113	47.871847
2037.612865	34447.059013	47.876852
2034.069998	33985.311860	47.881857
2030.379351	33521.823090	47.886861
2026.816997	33054.730803	47.891866
2023.458800	32587.287577	47.896871
2019.789079	32121.329333	47.901876
2016.326089	31650.298094	47.906881
2012.586319	31187.920823	47.911885
2009.140814	30718.118504	47.916890
2005.615927	30263.054621	47.921895
2002.043289	29814.884121	47.926900
1998.938443	29345.079047	47.931905
1995.320394	28878.038785	47.936909
1992.099898	28416.834201	47.941914
1987.874795	27948.705631	47.946919
1984.278208	27487.650274	47.951924
1981.133444	27026.427329	47.956929
1977.614687	26572.287293	47.961933
1974.180845	26108.595720	47.966938
1970.595439	25649.082094	47.971943
1967.223948	25188.196126	47.976948
1963.642808	24723.450581	47.981953
1960.319849	24258.371517	47.986957
1957.240337	23789.945637	47.991962
1953.269421	23322.670444	47.996967
1949.662769	22853.227275	48.001972
1946.292430	22389.504197	48.006977
1942.068658	21933.767247	48.011981
1938.913753	21473.066464	48.016986
1935.510766	21013.149846	48.021991
1931.954293	20554.819773	48.026996
1928.366909	20088.346772	48.032001
1924.817908	19634.388628	48.037005
1921.381333	19171.201382	48.042010
1917.847571	18716.888496	48.047015
1914.511955	18256.709471	48.052020
1910.933144	17796.268861	48.057025
1907.404994	17329.833684	48.062029
1903.729367	16871.190809	48.067034
1900.207522	16424.871577	48.072039
1896.463587	15959.487907	48.077044
1893.236791	15504.825935	48.082049
1889.053194	15052.904175	48.087053
1885.998678	14606.535529	48.092058
1882.080989	14152.652820	48.097063
1878.735335	13706.923629	48.102068
1875.239808	13261.693624	48.107073
1871.199264	12816.910320	48.112077
1867.753777	12361.863583	48.117082
1863.934237	11930.040317	48.122087
1860.346741	11484.163734	48.127092
1856.541034	11050.500265	48.132097
1852.900663	10633.231205	48.137101
1849.466122	10205.420595	48.142106
1845.424556	9779.363430	48.147111
1841.794001	9357.167537	48.152116
1837.567922	8952.283352	48.157121
1833.376686	8560.509587	48.162125
1829.286552	8171.725740	48.167130
1825.286280	7797.587092	48.172135
1821.204622	7409.932067	48.177140
1817.369268	7036.713705	48.182145
1813.213520	6677.781977	48.187149
1809.421819	6325.696702	48.192154
1805.629506	5984.932222	48.197159
1801.982076	5639.967839	48.202164
1798.384897	5305.780844	48.207169
1794.428137	4976.510378	48.212173
1791.099360	4648.929749	48.217178
1787.258290	4326.842799	48.222183
1783.699132	4012.729938	48.227188
1779.621088	3699.190591	48.232193
1775.698354	3404.254337	48.237197
1772.183070	3097.947343	48.242202
1768.231591	2816.700995	48.247207
1764.273971	2532.330666	48.252212
1759.668061	2275.295877	48.257217
1755.171532	2033.615523	48.262221
1750.763036	1792.035468	48.267226
1746.713913	1571.193154	48.272231
1742.505169	1369.725838	48.277236
1738.704789	1155.813758	48.282241
1734.726702	962.424203	48.287245
1730.827109	768.265213	48.292250
1726.695122	596.385968	48.297255
1722.710589	431.932937	48.302260
1719.224856	272.478429	48.307265
1714.697322	127.930386	48.312269
1708.638978	40.625147	48.317274
1698.594473	100.413382	48.322279
1692.791500	97.178598	48.327284
1689.518132	92.756016	48.332289
1686.232808	109.323312	48.337293
1683.794457	103.356588	48.342298
1681.467955	112.320966	48.347303
1679.005999	111.755198	48.352308
1676.329090	104.215276	48.357313
1672.931521	105.399128	48.362317
1669.990893	105.986685	48.367322
1666.363432	106.045238	48.372327
1663.206244	103.028241	48.377332
1659.781155	100.046614	48.382337
1656.163250	105.981844	48.387341
1652.457659	105.055991	48.392346
1648.602209	104.517290	48.397351
1645.420705	105.733952	48.402356
1642.414769	102.899057	48.407361
1639.447883	109.337230	48.412365
1636.491604	100.695536	48.417370
1632.637317	100.153492	48.422375
1629.239343	98.395165	48.427380
1625.796544	103.439451	48.432385
1622.189265	103.137368	48.437389
1618.603946	100.085774	48.442394
1615.263498	98.663339	48.447399
1611.873360	109.887634	48.452404
1608.377303	104.942906	48.457409
1604.681207	107.906937	48.462413
1601.605696	98.948454	48.467418
1598.721663	102.858587	48.472423
1594.674703	111.923066	48.477428
1591.413187	99.861468	48.482433
1587.720105	104.315134	48.487437
1583.924650	93.766640	48.492442
1580.954219	102.922983	48.497447
1577.369833	104.619965	48.502452
1574.378124	104.253715	48.507457
1570.629000	101.316205	48.512461
1567.228156	99.994923	48.517466
1563.587485	103.295172	48.522471
1559.910681	107.720997	48.527476
1556.339484	103.208745	48.532481
1553.039291	113.131415	48.537485
1549.884113	108.693614	48.542490
1546.569706	106.219947	48.547495
1542.604184	97.842918	48.552500
1539.378518	105.564705	48.557505
1535.805117	103.580596	48.562509
1532.069867	103.665430	48.567514
1528.735557	111.771118	48.572519
1525.340587	105.266781	48.577524
1521.821172	105.922289	48.582529
1518.483036	106.464162	48.587533
1515.179645	102.400607	48.592538
1511.476328	103.280889	48.597543
1507.661393	98.661051	48.602548
1504.308490	98.967946	48.607553
1500.738491	104.351570	48.612557
1497.524145	95.493808	48.617562
1494.111485	88.264585	48.622567
1490.707495	103.100810	48.627572
1487.278999	98.841600	48.632577
1483.446189	104.098454	48.637581
1480.220919	91.290937	48.642586
1476.613882	98.186245	48.647591
1473.220645	102.457208	48.652596
1470.224263	102.373263	48.657601
1466.208934	104.162640	48.662605
1462.302409	97.462696	48.667610
1458.766368	87.332590	48.672615
1455.605135	103.510401	48.677620
1452.292205	98.530867	48.682625
1448.634600	94.433871	48.687629
1445.458420	95.921797	48.692634
1442.026275	89.246098	48.697639
1438.200248	102.050480	48.702644
1435.272762	85.204040	48.707649
1431.121514	98.176095	48.712653
1427.655117	92.714261	48.717658
1423.990698	95.787266	48.722663
1420.949223	91.069202	48.727668
1417.520110	97.712196	48.732673
1413.549295	95.410316	48.737677
1410.133311	98.055520	48.742682
1406.649109	96.541589	48.747687
1402.927317	94.694487	48.752692
1399.959906	101.303585	48.757697
1396.362988	101.139115	48.762701
1392.602233	96.884178	48.767706
1389.565116	97.328591	48.772711
1385.924852	95.316944	48.777716
1382.622455	86.631096	48.782721
1378.429236	98.932654	48.787725
1375.477194	96.658866	48.792730
1371.891770	95.081602	48.797735
1367.975340	111.357980	48.802740
1364.847819	100.879565	48.807745
1361.391063	99.525879	48.812749
1358.084886	95.741185	48.817754
1354.417585	93.692622	48.822759
1351.132382	100.395477	48.827764
1347.516225	93.824361	48.832769
1344.096939	98.374628	48.837773
1340.398877	93.195633	48.842778
1336.697084	95.613250	48.847783
1333.587433	98.248743	48.852788
1329.891341	89.080026	48.857793
1326.287158	93.399649	48.862797
1322.760574	91.493700	48.867802
1319.393765	95.463171	48.872807
1315.706206	97.353402	48.877812
1312.648800	90.619394	48.882817
1308.695191	92.924352	48.887821
1305.655043	97.611756	48.892826
1302.372129	91.384241	48.897831
1298.290745	93.392719	48.902836
1294.793242	88.217316	48.907841
1291.150657	97.247330	48.912845
1288.072624	86.346792	48.917850
1285.117977	95.348818	48.922855
1280.664261	99.060373	48.927860
1277.101130	94.186246	48.932865
1273.357916	98.065615	48.937869
1270.382608	100.075936	48.942874
1267.052309	95.295281	48.947879
1263.525990	102.674737	48.952884
1260.229369	92.871224	48.957889
1256.630212	100.815662	48.962893
1252.883145	96.330829	48.967898
1249.228223	92.717489	48.972903
1245.887330	98.173030	48.977908
1242.396741	92.616915	48.982913
1238.761808	98.134043	48.987917
1235.392240	93.577800	48.992922
1232.156723	94.872504	48.997927
1228.201824	95.121271	49.002932
1225.073253	82.415818	49.007937
1221.225992	91.037937	49.012941
1217.642026	88.520850	49.017946
1214.171602	92.332452	49.022951
1210.482551	87.221679	49.027956
1207.545843	89.330397	49.032961
1204.026990	95.914604	49.037965
1200.604000	88.111245	49.042970
1197.378138	87.158230	49.047975
1193.345592	90.560631	49.052980
1190.211896	83.575933	49.057985
1186.232298	93.034886	49.062989
1183.081692	89.909357	49.067994
1179.562803	90.947623	49.072999
1175.653328	89.484098	49.078004
1172.283158	83.055057	49.083009
1168.663616	93.065393	49.088013
1165.470061	89.731421	49.093018
1161.934141	91.816357	49.098023
1158.418740	96.096864	49.103028
1154.696121	86.865874	49.108033
1151.340842	92.304675	49.113037
1147.765426	84.211849	49.118042
1144.710728	78.844163	49.123047
1140.714620	80.434431	49.128052
1137.680673	82.485525	49.133057
1133.562384	88.625213	49.138061
1130.501733	89.127094	49.143066
1126.949238	81.185725	49.148071
1123.437443	92.830735	49.153076
1119.970535	91.541933	49.158081
1116.180784	91.277799	49.163085
1113.100477	81.190718	49.168090
1109.898960	82.176426	49.173095
1106.045456	86.104611	49.178100
1102.407579	78.692219	49.183105
1098.919588	92.279190	49.188109
1095.188295	83.628519	49.193114
1092.056844	88.988191	49.198119
1087.899431	92.492295	49.203124
1084.617396	83.369907	49.208129
1081.349985	86.045791	49.213133
1077.963059	89.126249	49.218138
1074.772022	86.639766	49.223143
1070.940354	87.448325	49.228148
1067.119150	79.109043	49.233153
1063.578499	87.202561	49.238157
1060.362826	77.566825	49.243162
1056.948146	87.741421	49.248167
1053.262293	97.050255	49.253172
1050.042708	88.244009	49.258177
1046.287720	88.724267	49.263181
1042.918723	78.666320	49.268186
1039.600505	90.382435	49.273191
1036.078537	90.510054	49.278196
1032.625678	79.202852	49.283201
1028.731963	94.127943	49.288205
1025.034782	93.520388	49.293210
1021.925087	82.963345	49.298215
1018.236730	88.653313	49.303220
1014.930741	81.031090	49.308225
1011.428255	80.105336	49.313229
1007.673356	77.538958	49.318234
1004.277649	86.872226	49.323239
1000.444271	94.214068	49.328244
997.213894	86.285854	49.333249
994.033949	87.435890	49.338253
990.304497	89.329510	49.343258
986.792563	84.896704	49.348263
983.296956	91.436175	49.353268
980.133568	83.171678	49.358273
976.325971	86.817489	49.363277
972.703212	90.039068	49.368282
969.446835	77.290293	49.373287
965.516101	83.419779	49.378292
962.162303	67.639553	49.383297
958.841874	84.715282	49.388301
955.495655	72.518325	49.393306
951.854032	74.167327	49.398311
948.065714	88.990588	49.403316
944.611416	88.759679	49.408321
941.488678	92.570963	49.413325
937.866540	90.208549	49.418330
934.370736	88.940087	49.423335
930.606729	84.650930	49.428340
927.363288	80.555982	49.433345
923.703564	76.801077	49.438349
920.159189	82.316780	49.443354
916.833437	81.287599	49.448359
913.553075	90.340331	49.453364
910.320112	84.788460	49.458369
905.906538	87.585829	49.463373
902.464568	91.706231	49.468378
899.195950	89.798145	49.473383
895.566870	93.808472	49.478388
892.101758	85.587794	49.483393
888.746056	80.811153	49.488397
885.029289	78.039546	49.493402
881.434558	71.553767	49.498407
878.353073	91.259285	49.503412
875.048032	81.191415	49.508417
871.185565	84.921704	49.513421
868.062097	79.137668	49.518426
864.253957	83.821259	49.523431
860.536660	89.477780	49.528436
857.286995	90.635519	49.533441
853.495284	87.407356	49.538445
850.028965	88.655767	49.543450
846.601161	83.583480	49.548455
843.110512	93.703473	49.553460
839.661522	77.871649	49.558465
836.425849	84.003677	49.563469
832.679319	78.576057	49.568474
829.253113	70.906148	49.573479
825.618475	84.699434	49.578484
822.451009	83.984138	49.583489
818.741520	88.921291	49.588493
815.274573	97.797436	49.593498
811.614228	92.505092	49.598503
807.855933	87.870225	49.603508
804.743848	86.263643	49.608513
801.106932	92.163914	49.613517
797.834680	83.628502	49.618522
794.163816	87.964872	49.623527
790.461148	84.185034	49.628532
787.435308	80.600386	49.633537
783.609397	82.594463	49.638541
780.546426	89.797408	49.643546
776.729314	81.773914	49.648551
772.797714	89.460081	49.653556
769.905134	77.186218	49.658561
766.056239	80.645492	49.663565
762.550271	80.767489	49.668570
759.657878	76.162351	49.673575
755.474776	84.590004	49.678580
752.534718	85.174388	49.683585
748.247151	86.006500	49.688589
744.772292	87.344836	49.693594
741.967292	79.261869	49.698599
737.987126	87.370040	49.703604
734.602668	81.629815	49.708609
730.893748	83.754379	49.713613
727.366589	82.544608	49.718618
724.319759	81.563777	49.723623
720.375831	80.921910	49.728628
717.597100	84.651185	49.733633
713.845784	85.744666	49.738637
710.115978	92.349085	49.743642
706.526271	85.786622	49.748647
703.007403	87.141304	49.753652
699.498983	83.422989	49.758657
695.921065	81.838319	49.763661
692.298008	88.729834	49.768666
688.892215	77.114832	49.773671
685.102267	86.025441	49.778676
682.460478	78.986400	49.783681
678.834881	89.083112	49.788685
674.806372	86.742870	49.793690
671.676579	80.855447	49.798695
668.228915	83.382262	49.803700
664.871346	74.841179	49.808705
660.823151	85.781940	49.813709
657.402596	99.399547	49.818714
654.216304	77.411491	49.823719
650.288307	90.911938	49.828724
647.066423	84.440919	49.833729
643.372802	81.384179	49.838733
640.368721	84.990357	49.843738
636.740852	80.746495	49.848743
632.919236	88.557916	49.853748
629.354789	78.346987	49.858753
625.435585	86.638659	49.863757
622.622420	89.667803	49.868762
619.181288	84.062967	49.873767
615.754429	80.986849	49.878772
612.221226	87.152555	49.883777
608.225682	83.934019	49.888781
604.730973	84.743963	49.893786
601.332603	81.508392	49.898791
597.997403	87.893205	49.903796
594.557531	77.188340	49.908801
590.712084	87.651467	49.913805
587.346605	84.455068	49.918810
583.994532	85.511723	49.923815
580.745760	84.904023	49.928820
577.304936	77.350327	49.933825
573.429658	87.324565	49.938829
569.454153	82.995631	49.943834
566.522640	83.186408	49.948839
562.735856	85.728063	49.953844
559.868980	72.032921	49.958849
556.313093	79.363227	49.963853
552.205815	79.249838	49.968858
548.855472	76.965391	49.973863
545.301034	78.572395	49.978868
541.910854	74.756608	49.983873
538.212210	78.164044	49.988877
534.692659	87.304643	49.993882
531.735471	75.205400	49.998887
528.300512	81.485527	50.003892
524.446978	83.202369	50.008897
520.643585	83.838922	50.013901
517.104027	77.328801	50.018906
513.936658	84.133568	50.023911
510.470961	89.991389	50.028916
507.070138	78.369326	50.033921
503.812366	80.037716	50.038925
499.886566	80.082739	50.043930
496.444775	77.078566	50.048935
492.905700	80.787023	50.053940
489.657968	77.667221	50.058945
485.659761	76.584598	50.063949
482.365095	78.638373	50.068954
479.292723	76.152480	50.073959
475.224949	76.289210	50.078964
472.035892	75.191351	50.083969
468.552424	85.417801	50.088973
464.779640	75.543056	50.093978
461.302351	70.446905	50.098983
457.589733	78.842463	50.103988
454.016914	70.679773	50.108993
450.656166	83.535106	50.113997
447.183854	83.803760	50.119002
444.028493	68.631834	50.124007
440.038852	82.989740	50.129012
437.024206	72.902066	50.134017
433.338109	81.147970	50.139021
429.583535	77.872970	50.144026
426.593292	74.494799	50.149031
422.855398	81.499120	50.154036
419.306398	80.653451	50.159041
415.808341	79.837815	50.164045
411.619591	79.329019	50.169050
408.452815	73.102562	50.174055
405.336703	79.459605	50.179060
402.274914	74.327251	50.184065
398.377747	80.435742	50.189069
394.894687	76.571165	50.194074
391.309936	78.458145	50.199079
387.696130	79.970010	50.204084
384.231751	86.574260	50.209089
380.711014	85.784305	50.214093
376.896051	85.074958	50.219098
373.625077	82.689597	50.224103
370.215794	82.654228	50.229108
367.139185	81.640113	50.234113
363.262463	80.032411	50.239117
359.808645	82.696255	50.244122
356.662907	77.722505	50.249127
352.621121	83.787079	50.254132
349.046720	85.416197	50.259137
345.495918	87.848376	50.264141
342.203061	77.475011	50.269146
339.075937	86.285615	50.274151
335.393476	90.946531	50.279156
331.557367	81.280983	50.284161
328.106938	83.226152	50.289165
324.708028	79.917945	50.294170
321.591962	72.753491	50.299175
317.658384	82.784274	50.304180
314.419477	75.986948	50.309185
310.709659	73.622465	50.314189
307.120215	75.108401	50.319194
303.937197	65.483557	50.324199
300.193210	74.124447	50.329204
296.775678	70.189577	50.334209
293.164274	72.115519	50.339213
289.262113	68.743304	50.344218
286.206821	72.503010	50.349223
282.344386	85.667401	50.354228
278.843872	87.164806	50.359233
275.774898	79.129346	50.364237
271.952072	81.085043	50.369242
268.881246	79.332908	50.374247
264.987058	88.240793	50.379252
261.742666	79.147509	50.384257
258.443655	81.129222	50.389261
254.454310	81.007011	50.394266
250.824465	70.104021	50.399271
247.232230	79.594461	50.404276
244.176677	78.545448	50.409281
240.446718	75.374215	50.414285
237.123870	84.129876	50.419290
233.874628	86.312645	50.424295
229.990765	83.266611	50.429300
226.824173	77.214157	50.434305
223.615051	75.875854	50.439309
219.618459	79.234803	50.444314
216.349028	73.685568	50.449319
212.499933	80.533217	50.454324
209.016722	75.896763	50.459329
205.713315	74.516195	50.464333
202.393499	79.898924	50.469338
198.709261	72.693242	50.474343
194.805055	84.070344	50.479348
191.219817	76.918848	50.484353
187.681046	82.712143	50.489357
184.354707	78.161998	50.494362
181.195864	74.405164	50.499367
177.783311	82.931193	50.504372
174.322522	80.812690	50.509377
170.689772	85.370973	50.514381
166.856354	79.833624	50.519386
163.905657	72.558035	50.524391
160.003102	80.318819	50.529396
156.672742	77.471353	50.534401
152.825697	76.153287	50.539405
149.678912	79.332484	50.544410
146.447742	69.961934	50.549415
142.583947	86.682494	50.554420
138.800331	80.226262	50.559425
135.667687	78.951992	50.564429
131.997639	71.854843	50.569434
128.603907	67.631569	50.574439
124.812232	81.272149	50.579444
121.341014	71.458101	50.584449
118.123341	74.850811	50.589453
114.241173	78.846837	50.594458
110.965322	73.833279	50.599463
107.469131	79.300421	50.604468
103.952419	72.337588	50.609473
100.764452	73.713590	50.614477
97.235502	72.390300	50.619482
93.664930	68.469802	50.624487
89.595521	75.117653	50.629492
86.500935	74.571433	50.634497
83.245701	79.216476	50.639501
79.507039	81.216042	50.644506
76.125699	78.708711	50.649511
72.424299	78.272788	50.654516
68.698598	81.137179	50.659521
64.969756	73.922652	50.664525
61.732740	78.226349	50.669530
59.006774	75.484110	50.674535
54.758035	78.936122	50.679540
51.462676	75.950350	50.684545
48.096045	76.730936	50.689549
44.775205	77.779630	50.694554
41.333847	73.930769	50.699559
37.527377	74.504598	50.704564
33.846827	71.787605	50.709569
30.026988	77.320964	50.714573
26.461234	73.330127	50.719578
23.623153	77.862772	50.724583
20.094482	76.877961	50.729588
16.446742	73.070728	50.734593
12.971558	82.169650	50.739597
9.433217	84.843532	50.744602
6.043629	77.291466	50.749607
2.422236	78.538817	50.754612