Fri Aug 26 11:19:54 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.042410	94.757104	0.000000
0.889060	97.153840	0.005005
0.629566	98.001090	0.010010
0.714126	88.892509	0.015014
0.184026	80.506039	0.020019
0.236954	75.094382	0.025024
0.419504	79.125047	0.030029
-0.053270	65.579222	0.035034
-0.269377	57.646896	0.040038
-0.381646	59.733520	0.045043
-0.477475	43.936609	0.050048
-0.732881	34.469713	0.055053
-1.625417	20.543204	0.060058
-1.261633	16.494152	0.065062
-2.049471	13.222335	0.070067
-2.250246	10.627881	0.075072
-2.159642	10.639197	0.080077
-2.661864	0.293291	0.085082
-2.963551	-2.952979	0.090086
-3.282689	-7.506279	0.095091
-3.564647	-20.853965	0.100096
-4.048113	-12.784053	0.105101
-4.748437	-6.796852	0.110106
-4.719020	-19.183817	0.115110
-4.760934	-8.034829	0.120115
-4.726354	-14.462295	0.125120
-4.652962	-20.952747	0.130125
-5.886595	-11.494253	0.135130
-5.676624	-16.892369	0.140134
-5.991085	-14.293400	0.145139
-6.131299	-7.089986	0.150144
-6.535600	-18.068037	0.155149
-7.097823	0.552236	0.160154
-7.422115	-16.819345	0.165158
-7.627909	-11.291943	0.170163
-7.466172	-15.356983	0.175168
-7.535997	-10.306316	0.180173
-7.898659	-4.071141	0.185178
-8.022161	-15.719315	0.190182
-8.514160	-11.770300	0.195187
-8.807212	-7.842769	0.200192
-8.705058	-8.870927	0.205197
-9.608718	-7.974006	0.210202
-9.947612	-15.842889	0.215206
-10.214043	-11.375357	0.220211
-10.111885	-11.340532	0.225216
-10.074570	-11.456956	0.230221
-10.338160	-5.601026	0.235226
-10.181663	-16.758138	0.240230
-11.037692	-8.269563	0.245235
-11.261719	-12.546615	0.250240
-11.378929	-15.135094	0.255245
-11.644516	-7.209831	0.260250
-11.948437	-13.458048	0.265254
-12.609403	-10.071163	0.270259
-12.812372	-5.471147	0.275264
-13.037334	-14.730791	0.280269
-13.095426	-8.717039	0.285274
-12.701388	-10.755553	0.290278
-13.675742	-11.122573	0.295283
-13.965789	-8.261658	0.300288
-14.285988	-17.512800	0.305293
-14.215697	-8.595831	0.310298
-14.758457	-20.928507	0.315302
-15.160206	-10.837098	0.320307
-14.898549	-12.718964	0.325312
-14.668717	-6.224876	0.330317
-15.865519	-6.452860	0.335322
-15.417708	-14.067759	0.340326
-15.776406	-3.733121	0.345331
-16.494513	-8.372993	0.350336
-16.727029	-22.655321	0.355341
-17.345036	-12.384714	0.360346
-17.436086	-2.797239	0.365350
-17.409150	-6.797002	0.370355
-17.519270	-1.490131	0.375360
-17.556705	-11.079520	0.380365
-17.773505	-9.441685	0.385370
-17.961923	-2.866657	0.390374
-19.003322	-4.279895	0.395379
-19.026553	-1.140993	0.400384
-19.063739	-11.869333	0.405389
-19.075275	-1.269218	0.410394
-19.161617	-13.951362	0.415398
-20.018439	-4.867897	0.420403
-20.024737	-7.742555	0.425408
-20.476481	-14.186047	0.430413
-20.052509	-7.779132	0.435418
-20.570070	-12.633719	0.440422
-21.023240	-8.295294	0.445427
-21.504774	-9.998174	0.450432
-21.497157	-14.137291	0.455437
-21.813690	-7.343008	0.460442
-22.532613	-15.231812	0.465446
-22.880746	-11.861999	0.470451
-23.296319	-7.507282	0.475456
-22.571556	-12.681841	0.480461
-23.032784	-7.642997	0.485466
-23.102372	-13.766352	0.490470
-23.272758	-3.397761	0.495475
-23.513894	-9.206516	0.500480
-24.129836	-15.877533	0.505485
-24.615789	-8.512726	0.510490
-25.204616	-10.920211	0.515494
-24.880415	-9.160972	0.520499
-24.886666	-7.843810	0.525504
-25.075806	-11.594801	0.530509
-25.811985	-6.155655	0.535514
-26.211998	-7.845919	0.540518
-26.549719	-7.932424	0.545523
-26.407819	-7.489349	0.550528
-26.203907	-6.170109	0.555533
-26.105527	-12.091834	0.560538
-26.675900	-12.192733	0.565542
-27.068939	-9.616329	0.570547
-27.797469	-8.749838	0.575552
-27.776465	-8.813104	0.580557
-28.439883	-4.698198	0.585562
-28.573240	-14.604833	0.590566
-29.006946	-15.951340	0.595571
-29.329133	-7.033373	0.600576
-28.853381	-8.037445	0.605581
-29.346829	-10.295271	0.610586
-29.032374	-15.193981	0.615590
-29.837312	-13.385483	0.620595
-30.656894	-9.920120	0.625600
-30.733194	-16.108865	0.630605
-30.920182	-6.370420	0.635610
-30.675326	-15.181211	0.640614
-30.864756	-8.270682	0.645619
-31.072468	-10.427469	0.650624
-31.386772	-13.200388	0.655629
-32.135149	-10.309240	0.660634
-32.141218	-19.640924	0.665638
-32.214291	-13.646988	0.670643
-32.127793	-7.807604	0.675648
-32.504427	-8.027250	0.680653
-33.209001	0.026473	0.685658
-33.347542	-11.287177	0.690662
-33.542641	-6.315077	0.695667
-33.865396	-9.102499	0.700672
-34.543259	-3.903378	0.705677
-34.839471	-3.218089	0.710682
-34.921511	-9.706489	0.715686
-35.255762	-4.064177	0.720691
-35.376637	-7.218377	0.725696
-35.090765	-15.595808	0.730701
-35.333088	-6.576385	0.735706
-35.459786	-6.439490	0.740710
-36.186187	-11.052759	0.745715
-36.593727	-7.711659	0.750720
-36.538403	-10.222601	0.755725
-36.815753	-8.907521	0.760730
-36.852319	-10.157680	0.765734
-37.395357	-7.238393	0.770739
-38.078368	-7.786810	0.775744
-38.048712	-7.376877	0.780749
-38.113566	-0.890688	0.785754
-38.207949	-12.897723	0.790758
-38.317828	-10.833625	0.795763
-38.818463	-11.951420	0.800768
-38.899868	-11.138231	0.805773
-39.610446	-5.598671	0.810778
-39.678622	-6.606636	0.815782
-39.663335	-8.307779	0.820787
-39.966514	-3.524488	0.825792
-40.310206	-13.471136	0.830797
-40.835118	-1.155488	0.835802
-40.988140	-8.774912	0.840806
-40.921266	-7.823463	0.845811
-41.446364	-6.915882	0.850816
-41.729138	-7.162797	0.855821
-42.484338	4.097254	0.860826
-42.392154	-1.659001	0.865830
-42.760715	-2.560087	0.870835
-42.698600	-0.019748	0.875840
-42.418943	-4.343587	0.880845
-42.736394	2.643824	0.885850
-43.033031	-6.291461	0.890854
-43.618699	-3.764155	0.895859
-43.800235	-4.903161	0.900864
-44.040073	-5.972981	0.905869
-44.267914	-2.545967	0.910874
-45.245858	-6.550616	0.915878
-45.562640	-7.105436	0.920883
-45.590482	-2.877525	0.925888
-45.478464	-10.389522	0.930893
-45.441978	-8.218504	0.935898
-45.567260	-4.045021	0.940902
-45.595910	-2.702226	0.945907
-46.265823	-4.537122	0.950912
-46.912681	-12.421327	0.955917
-46.956110	-6.795823	0.960922
-46.752007	-2.047224	0.965926
-47.352375	-13.795148	0.970931
-47.889261	-8.769833	0.975936
-48.212751	-11.965250	0.980941
-48.720694	-7.624624	0.985946
-48.763282	-4.109401	0.990950
-49.076289	-4.917900	0.995955
-49.387410	-13.569361	1.000960
-48.882119	-7.773038	1.005965
-49.526605	-6.672868	1.010970
-48.902598	5.033642	1.015974
-49.468086	-1.490215	1.020979
-49.825736	-9.618760	1.025984
-50.061533	-9.971061	1.030989
-50.976615	0.450205	1.035994
-51.208641	-5.514987	1.040998
-51.109643	-7.127927	1.046003
-51.623975	-4.134018	1.051008
-51.500547	-4.482141	1.056013
-51.771428	-4.923889	1.061018
-51.451862	-8.121356	1.066022
-52.511255	-9.167972	1.071027
-52.675714	3.322502	1.076032
-52.812055	-2.935989	1.081037
-53.083448	5.790582	1.086042
-53.531969	2.484921	1.091046
-54.132666	-4.707308	1.096051
-54.454820	-7.127841	1.101056
-54.521329	-10.388579	1.106061
-54.889645	-2.092993	1.111066
-54.963091	-8.829495	1.116070
-55.042778	-1.157795	1.121075
-54.688709	0.100102	1.126080
-54.785737	-5.098362	1.131085
-55.614469	-6.895874	1.136090
-55.910725	-6.482651	1.141094
-55.907463	-6.413446	1.146099
-56.270320	-4.104323	1.151104
-56.478375	-8.516733	1.156109
-57.180287	-9.040061	1.161114
-57.477290	-5.415625	1.166118
-57.214971	-7.022358	1.171123
-57.606141	-8.271087	1.176128
-57.740172	-15.289208	1.181133
-58.196275	-6.622466	1.186138
-58.433496	-3.893157	1.191142
-58.631831	-5.035875	1.196147
-58.793694	0.345488	1.201152
-58.512317	-13.248090	1.206157
-59.603152	-10.449148	1.211162
-60.109202	-9.408496	1.216166
-59.974950	-4.427567	1.221171
-59.973728	-4.560517	1.226176
-60.077126	-6.224199	1.231181
-61.170073	4.885965	1.236186
-61.386090	-5.226093	1.241190
-61.453699	-4.570070	1.246195
-61.755557	-6.215507	1.251200
-61.431281	-4.086133	1.256205
-62.127244	1.093661	1.261210
-61.824358	-2.408084	1.266214
-61.777429	1.789205	1.271219
-62.481850	-2.672468	1.276224
-62.846427	-3.324247	1.281229
-63.180545	-5.347461	1.286234
-63.514951	-3.150331	1.291238
-64.135815	-5.287081	1.296243
-64.700696	-2.222028	1.301248
-64.247820	-9.483387	1.306253
-64.350947	-8.900925	1.311258
-64.362316	-9.553916	1.316262
-64.586876	-10.069312	1.321267
-64.941270	-4.733901	1.326272
-65.355244	-8.323339	1.331277
-66.154915	-8.176572	1.336282
-66.236511	-4.816621	1.341286
-66.168878	-14.397054	1.346291
-66.352658	-3.510708	1.351296
-66.680637	-7.945573	1.356301
-66.961087	-5.269644	1.361306
-67.269841	-6.600806	1.366310
-67.558162	-8.957005	1.371315
-67.922887	-0.940380	1.376320
-67.679615	-10.102089	1.381325
-68.276484	-3.014230	1.386330
-68.683531	-11.018027	1.391334
-69.132110	-11.564980	1.396339
-69.326608	-8.364615	1.401344
-69.208463	-13.378286	1.406349
-69.206159	-3.897098	1.411354
-69.657897	-7.547092	1.416358
-69.231892	-13.779245	1.421363
-70.440050	-7.747776	1.426368
-70.733851	-12.412580	1.431373
-71.148516	-12.025212	1.436378
-70.782723	-13.714492	1.441382
-70.919199	-14.964913	1.446387
-71.132107	-13.280229	1.451392
-71.788014	-2.896156	1.456397
-72.611194	-4.726168	1.461402
-72.343507	-5.542826	1.466406
-72.515585	-5.411520	1.471411
-72.580864	-9.406414	1.476416
-72.522453	-9.329977	1.481421
-73.283398	-9.040548	1.486426
-73.697612	-9.757361	1.491430
-73.601565	-11.274932	1.496435
-74.080780	-7.283616	1.501440
-73.853990	-14.984317	1.506445
-74.317233	-11.666181	1.511450
-74.872878	-18.232690	1.516454
-75.352007	-6.911233	1.521459
-75.786482	4.203969	1.526464
-75.496089	-4.553805	1.531469
-75.591327	-4.314245	1.536474
-75.534677	-2.431094	1.541478
-75.933181	-3.289554	1.546483
-76.267788	-0.646319	1.551488
-76.749987	-15.304206	1.556493
-76.882939	-10.101349	1.561498
-77.120045	-8.197769	1.566502
-77.661295	-13.766810	1.571507
-78.474449	-11.181940	1.576512
-78.309340	-11.612480	1.581517
-78.481726	-7.640465	1.586522
-78.686376	0.246836	1.591526
-78.811890	-4.497954	1.596531
-78.990465	-5.710185	1.601536
-78.617274	2.833767	1.606541
-78.976014	0.422095	1.611546
-79.649922	-11.608595	1.616550
-79.799251	-17.339893	1.621555
-80.134462	-8.549612	1.626560
-80.330385	-13.400492	1.631565
-81.022654	-4.548287	1.636570
-81.221653	-2.388058	1.641574
-81.258090	-8.589338	1.646579
-81.443120	0.114292	1.651584
-81.742093	-7.881023	1.656589
-81.903592	-0.405387	1.661594
-82.586848	-1.428311	1.666598
-82.105115	-8.447399	1.671603
-82.610739	-0.427818	1.676608
-82.639081	-5.257337	1.681613
-83.107265	5.201912	1.686618
-83.808781	-1.057162	1.691622
-84.034682	-6.555086	1.696627
-84.392333	3.440879	1.701632
-84.331818	-1.984587	1.706637
-84.189408	5.706315	1.711642
-84.130993	3.413182	1.716646
-85.104858	-2.344759	1.721651
-85.487162	-4.936253	1.726656
-85.262009	3.247948	1.731661
-85.470619	-5.558676	1.736666
-85.864373	-7.949077	1.741670
-86.635211	-1.046095	1.746675
-87.304350	6.565529	1.751680
-87.488595	-2.564418	1.756685
-87.014553	3.205135	1.761690
-87.110997	-7.839829	1.766694
-87.057632	-1.748523	1.771699
-87.660874	1.072575	1.776704
-87.700067	-7.966062	1.781709
-88.040041	-0.760020	1.786714
-88.505715	3.849263	1.791718
-88.534835	-4.134288	1.796723
-89.065522	-2.495034	1.801728
-89.146774	2.981341	1.806733
-89.678236	2.105619	1.811738
-90.024511	-2.063815	1.816742
-90.081510	-5.686688	1.821747
-90.293102	4.973046	1.826752
-90.223959	-2.718932	1.831757
-90.678554	1.800044	1.836762
-91.156080	0.355959	1.841766
-91.197996	-1.950024	1.846771
-91.817796	8.956762	1.851776
-92.091878	1.112587	1.856781
-92.095349	-3.341168	1.861786
-92.270447	-5.487214	1.866790
-92.093407	-9.244599	1.871795
-93.002063	4.788546	1.876800
-93.065650	-0.434106	1.881805
-93.294056	-0.471194	1.886810
-93.434506	0.047479	1.891814
-93.269772	-5.441667	1.896819
-93.844793	5.012071	1.901824
-94.514834	-9.293880	1.906829
-94.766795	-4.404674	1.911834
-94.475064	-9.470682	1.916838
-94.648122	-8.409113	1.921843
-95.405414	-0.258602	1.926848
-95.584720	-5.760617	1.931853
-95.660123	-6.194837	1.936858
-96.095558	-6.775473	1.941862
-96.019915	-9.052304	1.946867
-96.879455	-3.056132	1.951872
-97.052602	-16.588424	1.956877
-97.437773	-7.186109	1.961882
-97.489003	-9.708932	1.966886
-97.403823	-19.497729	1.971891
-97.747997	0.641928	1.976896
-97.446874	-11.439337	1.981901
-98.030533	-11.310383	1.986906
-98.715009	-7.208018	1.991910
-98.704514	-7.899213	1.996915
-99.158876	-10.405548	2.006912
-98.888025	-13.992140	2.016909
-98.534462	-10.388281	2.026906
-98.065286	-9.640674	2.036902
-97.109568	-9.323604	2.046899
-96.622089	-9.152199	2.056896
-96.683488	-10.821289	2.066893
-95.965955	-20.663929	2.076890
-95.033008	-11.451606	2.086886
-94.871749	-8.774448	2.096883
-94.201359	-5.802773	2.106880
-93.835165	-6.641984	2.116877
-93.604747	-5.901550	2.126874
-92.840563	-9.311540	2.136870
-92.414271	-5.326210	2.146867
-91.487909	-6.496551	2.156864
-91.086603	-9.789855	2.166861
-90.971587	-3.180725	2.176858
-90.594150	-11.269366	2.186854
-89.493543	-6.875861	2.196851
-89.701481	-6.035497	2.206848
-88.660407	-7.369414	2.216845
-88.010742	-4.933019	2.226842
-87.953275	-6.313352	2.236838
-86.915739	-0.766488	2.246835
-86.979163	-1.608497	2.256832
-86.655634	0.777312	2.266829
-85.570397	2.075208	2.276826
-85.360710	-7.596504	2.286822
-84.870451	-8.207952	2.296819
-84.046358	-5.057476	2.306816
-83.555614	-5.988936	2.316813
-83.508621	-5.932673	2.326810
-82.918241	-5.840644	2.336806
-82.456807	-6.045306	2.346803
-81.341100	-13.314426	2.356800
-81.034706	-10.308251	2.366797
-81.064246	-14.373909	2.376794
-80.597107	-19.118761	2.386790
-79.789800	-17.315110	2.396787
-79.080064	-15.942910	2.406784
-78.302378	-14.932905	2.416781
-78.175520	-12.263061	2.426778
-77.976993	-14.397092	2.436774
-77.751595	-9.797628	2.446771
-76.942841	-5.504394	2.456768
-75.774651	-10.234862	2.466765
-75.679046	-8.104994	2.476762
-75.501943	-10.061468	2.486758
-75.039892	-15.112794	2.496755
-74.336819	-5.525732	2.506752
-73.641302	-4.626471	2.516749
-72.671068	0.357520	2.526746
-72.698935	-7.915097	2.536742
-72.428597	-15.119114	2.546739
-72.092042	-8.069325	2.556736
-71.606788	-12.113771	2.566733
-70.481970	-7.454781	2.576730
-69.747410	-3.118317	2.586726
-69.634040	-5.631885	2.596723
-69.554263	-7.870968	2.606720
-69.097181	-5.955767	2.616717
-68.245787	-9.233621	2.626714
-67.870878	-12.608342	2.636710
-66.899712	-8.356235	2.646707
-67.032010	-5.718895	2.656704
-66.130826	-4.328988	2.666701
-65.282911	-6.842887	2.676698
-65.395665	-6.622373	2.686694
-64.991049	-2.057146	2.696691
-64.134698	-3.416151	2.706688
-63.949213	6.622128	2.716685
-62.892257	-0.245056	2.726682
-62.465983	-7.888323	2.736678
-62.612877	-2.014496	2.746675
-61.650239	-4.033092	2.756672
-60.879519	-2.245915	2.766669
-60.842439	-3.369658	2.776666
-60.485558	-4.330959	2.786662
-59.705227	0.977197	2.796659
-59.446577	1.098704	2.806656
-58.731983	-1.733381	2.816653
-58.203323	-9.950104	2.826650
-57.615036	-7.016327	2.836646
-56.892283	-3.846903	2.846643
-56.828131	-1.205305	2.856640
-56.671627	-5.255586	2.866637
-55.791940	-4.312143	2.876634
-55.363689	-4.939277	2.886630
-54.489340	-5.319099	2.896627
-54.429340	-2.094000	2.906624
-53.353809	-3.968620	2.916621
-52.801325	-9.616885	2.926618
-52.728996	-4.667313	2.936614
-52.493290	-2.606773	2.946611
-51.472956	0.193214	2.956608
-51.214467	2.161512	2.966605
-51.108391	-2.900915	2.976602
-49.726717	-2.532959	2.986598
-49.465630	-12.405904	2.996595
-49.720617	-12.356473	3.006592
-48.945608	-1.893652	3.016589
-48.139133	-6.526622	3.026586
-47.168654	-13.142760	3.036582
-46.783260	-7.377152	3.046579
-46.478251	-3.848090	3.056576
-46.718004	0.472189	3.066573
-45.904050	-9.664230	3.076570
-45.031108	-10.576005	3.086566
-44.853840	-14.737218	3.096563
-44.049552	-13.031293	3.106560
-43.782955	-3.236888	3.116557
-42.685387	-4.883697	3.126554
-42.606271	-7.065660	3.136550
-42.244448	-5.401711	3.146547
-42.054115	-3.730068	3.156544
-40.933803	-8.373890	3.166541
-40.776676	-6.779437	3.176538
-40.544615	-10.483531	3.186534
-39.341553	-10.730806	3.196531
-39.378164	-8.178055	3.206528
-38.494124	-11.708072	3.216525
-37.836940	-13.675940	3.226522
-37.786679	-3.832013	3.236518
-37.161961	-8.642583	3.246515
-36.544522	-3.397759	3.256512
-36.442725	-10.398148	3.266509
-35.658759	-9.161044	3.276506
-34.762155	-8.828431	3.286502
-34.433834	-10.700748	3.296499
-34.435441	-10.589403	3.306496
-33.447743	-11.823143	3.316493
-33.204318	-11.426844	3.326490
-32.957853	-12.389958	3.336486
-32.050290	-12.499362	3.346483
-31.871058	-7.050100	3.356480
-31.125483	-11.578556	3.366477
-30.559614	-11.479541	3.376474
-30.173690	-11.425365	3.386470
-29.314630	-2.879413	3.396467
-29.150694	-6.303647	3.406464
-28.993920	-11.491171	3.416461
-27.888978	-10.342055	3.426458
-27.597454	-2.949473	3.436454
-27.356757	-9.094037	3.446451
-26.449066	-8.120109	3.456448
-26.185276	-6.821020	3.466445
-25.834205	-7.832098	3.476442
-24.708558	-3.651554	3.486438
-24.831736	-5.583449	3.496435
-24.199263	-3.942634	3.506432
-23.476336	-11.594078	3.516429
-23.136925	-4.291312	3.526426
-22.703886	-10.703400	3.536422
-21.988356	-11.701535	3.546419
-21.667565	-5.979717	3.556416
-21.227673	-8.715180	3.566413
-20.231993	-13.121024	3.576410
-20.008186	-14.425889	3.586406
-19.858278	-14.233600	3.596403
-18.710940	-15.824803	3.606400
-18.805902	-7.697329	3.616397
-18.222513	-10.173209	3.626394
-17.259413	-17.390059	3.636390
-16.709634	-13.775567	3.646387
-17.104947	-13.324166	3.656384
-16.280287	-10.512718	3.666381
-15.257612	-10.937806	3.676378
-15.276627	-4.542213	3.686374
-14.614695	-6.837093	3.696371
-13.851433	-0.699508	3.706368
-13.551406	-8.769766	3.716365
-13.527839	-5.589676	3.726362
-12.678978	-5.243294	3.736358
-12.534459	-9.922080	3.746355
-11.523678	-11.403326	3.756352
-10.961410	-6.346309	3.766349
-10.032721	-15.033947	3.776346
-10.023677	-14.129169	3.786342
-9.719044	-14.236560	3.796339
-9.257626	-13.845692	3.806336
-8.201742	-2.739209	3.816333
-8.299738	-1.209566	3.826330
-7.727629	-12.385347	3.836326
-6.835590	-2.447573	3.846323
-6.793461	-11.504010	3.856320
-6.216478	-8.818719	3.866317
-5.342510	-7.348546	3.876314
-5.387570	-14.082157	3.886310
-4.481554	-1.827807	3.896307
-4.235581	5.774605	3.906304
-3.611211	14.962140	3.916301
-3.149297	14.389951	3.926298
-3.146646	20.573113	3.936294
-2.602573	34.394834	3.946291
-2.163972	46.341869	3.956288
-1.519347	68.022876	3.966285
-1.202705	75.462265	3.976282
-0.598313	96.734601	3.986278
0.008109	106.872125	3.996275
0.000000	122.900748	4.001280
0.438581	127.818515	4.006285
0.476418	139.303183	4.011290
0.817307	140.126557	4.016294
1.175568	141.776108	4.021299
0.995504	146.391580	4.026304
1.064957	159.567066	4.031309
1.194534	157.057193	4.036314
1.649972	157.834260	4.041318
1.441837	161.811880	4.046323
1.006719	158.013731	4.051328
1.105799	162.715455	4.056333
1.253683	169.016729	4.061338
1.048188	162.999891	4.066342
1.466539	170.027827	4.071347
1.362932	171.287396	4.076352
1.579672	167.362443	4.081357
1.448300	168.442841	4.086362
1.278245	166.324460	4.091366
1.212107	158.210556	4.096371
1.469426	169.120082	4.101376
1.337733	169.128044	4.106381
1.476617	171.143941	4.111386
1.501990	165.347414	4.116390
1.565539	168.691128	4.121395
1.404050	165.511582	4.126400
1.409586	169.819759	4.131405
1.675991	169.841667	4.136410
1.420657	172.440949	4.141414
1.775778	157.658866	4.146419
1.090466	164.007608	4.151424
1.259906	151.835998	4.156429
1.475320	169.633037	4.161434
1.280260	166.101223	4.166438
1.801946	164.014341	4.171443
1.750371	168.771160	4.176448
1.549775	170.953805	4.181453
1.771391	175.490925	4.186458
1.555540	177.758201	4.191462
1.364085	172.587040	4.196467
1.225588	177.632634	4.201472
1.377136	176.818233	4.206477
1.393769	178.217265	4.211482
1.310863	171.713113	4.216486
1.339434	168.734923	4.221491
1.367749	174.409425	4.226496
1.910031	182.768961	4.231501
1.802464	187.876180	4.236506
1.990970	173.999527	4.241510
1.675169	169.186240	4.246515
1.470874	172.767806	4.251520
1.945961	178.815663	4.256525
1.561676	178.768043	4.261530
2.077220	182.753213	4.266534
1.769020	170.450319	4.271539
1.692675	178.678386	4.276544
2.073207	179.925850	4.281549
2.264338	180.082861	4.286554
1.848190	174.124127	4.291558
1.670759	171.329867	4.296563
1.582615	169.088003	4.301568
1.719450	174.131856	4.306573
1.997446	187.613407	4.311578
2.131174	181.088177	4.316582
2.017149	171.042389	4.321587
1.570813	186.677286	4.326592
2.109056	187.046002	4.331597
2.174898	190.088814	4.336602
1.687834	187.760366	4.341606
2.039000	196.317338	4.346611
1.918506	201.350646	4.351616
2.264086	197.082931	4.356621
2.376512	189.450563	4.361626
1.869948	183.695723	4.366630
2.041435	172.574122	4.371635
1.721208	189.040415	4.376640
2.194225	195.158201	4.381645
2.055901	199.213543	4.386650
2.073147	203.886892	4.391654
2.352794	204.852679	4.396659
2.087425	200.948999	4.401664
2.137057	198.059272	4.406669
2.103456	204.363505	4.411674
1.958423	205.338468	4.416678
2.290101	196.947477	4.421683
2.027193	199.693471	4.426688
2.153858	201.508797	4.431693
2.514199	202.645514	4.436698
2.225710	205.556840	4.441702
2.189977	197.055378	4.446707
1.885484	200.478547	4.451712
2.428671	186.676373	4.456717
2.134981	198.060840	4.461722
2.168575	196.606757	4.466726
2.538756	192.847729	4.471731
2.201172	198.171093	4.476736
2.290100	206.680318	4.481741
2.304917	203.783355	4.486746
2.158357	202.028299	4.491750
2.357594	205.686244	4.496755
2.077390	201.455850	4.501760
2.115825	204.031543	4.506765
2.162540	199.905270	4.511770
2.226220	200.202346	4.516774
2.151450	204.852057	4.521779
2.028140	205.662289	4.526784
2.678626	213.169780	4.531789
2.564647	217.816108	4.536794
2.684820	221.900809	4.541798
2.769831	218.319051	4.546803
2.175102	204.194171	4.551808
2.544317	209.866227	4.556813
2.390237	220.792383	4.561818
2.412023	220.241787	4.566822
2.756056	220.567977	4.571827
2.605944	231.272064	4.576832
2.527230	221.954724	4.581837
2.777419	219.486174	4.586842
2.321791	222.205231	4.591846
2.742279	217.251983	4.596851
2.514917	223.254205	4.601856
3.017345	217.693426	4.606861
2.704129	221.848768	4.611866
2.448569	219.753184	4.616870
2.570243	221.907805	4.621875
2.669993	218.845759	4.626880
2.838768	218.933487	4.631885
2.944815	225.987924	4.636890
2.739188	231.161042	4.641894
2.910725	228.296621	4.646899
2.514683	222.619472	4.651904
3.043021	226.517240	4.656909
2.705827	216.490355	4.661914
2.660905	217.582606	4.666918
2.840233	211.777912	4.671923
2.897601	221.484766	4.676928
2.771943	212.848605	4.681933
2.672822	222.703208	4.686938
2.717184	217.283350	4.691942
2.724079	218.231495	4.696947
2.522966	223.375435	4.701952
2.951875	215.080026	4.706957
2.891512	217.484446	4.711962
2.447494	218.838147	4.716966
2.719339	218.267599	4.721971
2.552185	224.273102	4.726976
2.812261	222.600260	4.731981
2.802577	218.780150	4.736986
2.867778	220.535448	4.741990
2.967100	225.828760	4.746995
3.171728	231.776380	4.752000
3.136824	231.687017	4.757005
2.957075	230.525570	4.762010
2.521490	238.796943	4.767014
3.307471	232.439054	4.772019
2.886111	243.327746	4.777024
3.316449	242.460444	4.782029
3.229333	248.232034	4.787034
2.922796	247.811648	4.792038
3.149337	244.859569	4.797043
3.236658	250.369887	4.802048
3.200760	240.912997	4.807053
3.263619	246.493560	4.812058
3.193637	247.137307	4.817062
3.130358	238.447130	4.822067
3.132540	251.392717	4.827072
3.519369	249.266713	4.832077
3.111279	244.113442	4.837082
3.119198	240.227313	4.842086
3.454149	243.079541	4.847091
3.203777	246.889753	4.852096
3.390421	244.668370	4.857101
3.420436	250.586236	4.862106
2.692239	250.130263	4.867110
3.131419	241.434618	4.872115
2.892548	247.742353	4.877120
3.349954	248.449517	4.882125
2.911763	249.716894	4.887130
3.139872	258.198145	4.892134
3.387056	245.672688	4.897139
3.203864	254.183176	4.902144
3.219355	251.653089	4.907149
3.632734	253.635747	4.912154
3.261926	254.054255	4.917158
3.195300	249.913980	4.922163
3.122963	255.053698	4.927168
3.345043	260.166559	4.932173
3.589180	273.017544	4.937178
3.617232	274.291422	4.942182
3.518438	271.921492	4.947187
3.300210	273.154623	4.952192
3.256663	277.280646	4.957197
3.456649	273.443698	4.962202
3.538313	263.699577	4.967206
3.932536	271.427322	4.972211
3.944360	276.231245	4.977216
3.895100	270.569689	4.982221
3.624188	252.465047	4.987226
3.392637	252.273426	4.992230
3.561304	250.864745	4.997235
3.542502	261.640153	5.002240
3.765833	275.823130	5.007245
3.724772	261.263995	5.012250
3.018844	266.834551	5.017254
3.594405	271.639284	5.022259
3.818609	279.361868	5.027264
3.928655	278.421048	5.032269
3.658648	270.291379	5.037274
3.896906	281.830353	5.042278
4.033124	276.326575	5.047283
3.501748	272.407349	5.052288
3.721872	276.289842	5.057293
3.849876	279.500158	5.062298
3.898276	276.718175	5.067302
4.055972	275.181490	5.072307
3.690006	273.413131	5.077312
3.827678	278.928274	5.082317
3.512794	274.845629	5.087322
3.702972	278.198121	5.092326
3.947193	270.956479	5.097331
4.004730	279.897724	5.102336
3.908056	283.785252	5.107341
4.105089	270.856306	5.112346
3.958982	282.546872	5.117350
4.205290	276.488124	5.122355
3.925318	283.574213	5.127360
3.969638	274.595188	5.132365
3.846065	279.787181	5.137370
3.733763	280.007256	5.142374
3.985029	279.458893	5.147379
4.034780	283.187584	5.152384
3.967680	282.995668	5.157389
3.873012	280.729496	5.162394
3.662969	281.445671	5.167398
3.946977	284.837338	5.172403
3.838314	289.992212	5.177408
3.712883	280.043049	5.182413
4.036960	278.932867	5.187418
3.877657	276.518574	5.192422
3.724825	272.948527	5.197427
3.872330	291.366854	5.202432
4.026294	299.223766	5.207437
4.286267	296.475277	5.212442
4.019630	303.673191	5.217446
4.686289	301.775690	5.222451
4.364035	301.288148	5.227456
4.407389	294.884513	5.232461
4.117976	295.353623	5.237466
4.048969	291.046033	5.242470
4.534771	295.390194	5.247475
4.266616	296.624772	5.252480
4.120083	287.311630	5.257485
4.122585	290.190317	5.262490
4.327173	290.648950	5.267494
4.347630	293.828557	5.272499
4.858530	301.759608	5.277504
4.468266	287.302276	5.282509
4.263678	270.895685	5.287514
3.987289	287.956346	5.292518
4.234484	280.337756	5.297523
4.404384	293.820400	5.302528
4.351453	299.358898	5.307533
4.736191	300.346293	5.312538
4.591198	301.881229	5.317542
4.798666	286.938533	5.322547
4.580767	281.724001	5.327552
4.567086	276.686479	5.332557
4.418256	282.894788	5.337562
4.621046	284.593869	5.342566
4.438800	275.782993	5.347571
4.571824	278.381934	5.352576
4.628219	284.893643	5.357581
4.684271	277.092848	5.362586
4.194196	281.845205	5.367590
4.374535	273.591634	5.372595
4.517671	289.179134	5.377600
4.597117	279.372075	5.382605
4.531875	276.319890	5.387610
4.469643	291.246518	5.392614
4.690631	284.619080	5.397619
4.571978	287.254044	5.402624
4.400526	296.923800	5.407629
4.809852	295.876273	5.412634
4.783767	307.073614	5.417638
5.003500	295.672345	5.422643
4.561680	294.548535	5.427648
4.353517	287.004004	5.432653
4.594587	286.280061	5.437658
4.946899	301.768566	5.442662
4.906886	305.039847	5.447667
4.684904	306.064760	5.452672
4.425744	312.878706	5.457677
4.593690	305.841910	5.462682
4.512872	305.658457	5.467686
4.805269	307.701087	5.472691
4.549801	312.916789	5.477696
4.533761	310.666845	5.482701
4.782988	310.770521	5.487706
4.437002	311.036471	5.492710
4.881226	299.546465	5.497715
4.829997	299.750703	5.502720
4.691240	307.453882	5.507725
4.778550	311.059675	5.512730
4.980505	322.999791	5.517734
4.872446	320.517403	5.522739
5.184453	333.266118	5.527744
4.942320	320.810466	5.532749
5.120336	311.418306	5.537754
4.712947	310.428337	5.542758
4.855268	321.858890	5.547763
5.057189	323.583419	5.552768
5.185822	323.822928	5.557773
5.379258	318.519032	5.562778
5.036786	312.396923	5.567782
5.229358	306.463588	5.572787
4.659811	313.098074	5.577792
4.792223	314.994774	5.582797
5.183612	318.110305	5.587802
4.752179	330.066786	5.592806
5.302827	324.068204	5.597811
5.098306	328.953281	5.602816
5.011177	329.390896	5.607821
4.839438	325.279625	5.612826
4.821072	324.039262	5.617830
5.567779	321.252950	5.622835
5.210329	331.372457	5.627840
5.157357	329.064987	5.632845
5.700995	324.446870	5.637850
5.242602	328.612186	5.642854
5.534382	323.748550	5.647859
5.208167	331.822606	5.652864
5.102938	328.608961	5.657869
5.479271	325.196955	5.662874
5.311102	330.228230	5.667878
5.801982	325.064680	5.672883
5.419725	330.372893	5.677888
4.849319	327.367715	5.682893
5.663275	315.861260	5.687898
5.456951	331.205818	5.692902
5.180213	327.961930	5.697907
5.356778	328.975412	5.702912
5.111987	332.974595	5.707917
5.599408	323.157775	5.712922
5.115390	331.648700	5.717926
5.544065	330.044509	5.722931
5.413406	325.623126	5.727936
5.616564	328.945134	5.732941
5.504752	326.681625	5.737946
5.360072	331.658625	5.742950
5.644784	330.646316	5.747955
5.337714	325.714569	5.752960
5.361136	325.106769	5.757965
5.447950	321.777805	5.762970
4.938032	334.499470	5.767974
5.533558	317.386139	5.772979
5.615983	332.476936	5.777984
5.354693	330.262010	5.782989
5.751683	325.606616	5.787994
5.471439	338.374781	5.792998
5.583461	335.412043	5.798003
5.424283	328.030708	5.803008
5.572055	324.062676	5.808013
5.419976	321.767473	5.813018
5.429192	344.215798	5.818022
5.402120	337.889551	5.823027
5.703802	353.718173	5.828032
5.473107	363.381371	5.833037
5.747970	350.569961	5.838042
5.467328	348.921186	5.843046
5.509560	344.118544	5.848051
5.545009	354.382531	5.853056
5.452290	355.289246	5.858061
6.073235	352.263087	5.863066
5.545583	349.668857	5.868070
5.713399	358.536025	5.873075
5.642362	367.073396	5.878080
5.580298	357.664809	5.883085
5.889614	356.942893	5.888090
5.464202	369.496404	5.893094
5.679947	385.354253	5.898099
6.083888	384.582802	5.903104
6.011220	382.882660	5.908109
6.693775	373.848505	5.913114
6.168508	364.980263	5.918118
5.988459	359.272603	5.923123
5.831044	351.150677	5.928128
5.577745	357.166472	5.933133
5.763418	351.534750	5.938138
5.849123	369.921652	5.943142
6.123355	380.657835	5.948147
5.804151	376.851081	5.953152
6.016347	368.526069	5.958157
6.435750	370.042737	5.963162
6.305371	384.129015	5.968166
6.010923	360.592668	5.973171
6.223473	368.272813	5.978176
5.903438	363.985307	5.983181
5.988120	364.921349	5.988186
6.315147	372.915861	5.993190
6.164748	365.118698	5.998195
6.124081	351.698363	6.003200
5.973876	356.369349	6.008205
6.326980	358.921381	6.013210
5.628380	375.317046	6.018214
6.106055	371.281820	6.023219
6.103000	375.844480	6.028224
6.545670	378.398389	6.033229
6.458967	364.485345	6.038234
5.978006	365.142465	6.043238
5.828657	366.814124	6.048243
5.963232	374.455792	6.053248
5.681825	379.479403	6.058253
6.196602	377.947223	6.063258
6.353498	377.372422	6.068262
6.524738	384.752125	6.073267
6.427125	384.087238	6.078272
6.180400	370.097865	6.083277
6.123720	356.778094	6.088282
5.644466	372.022815	6.093286
6.544156	379.754165	6.098291
6.352863	372.747966	6.103296
5.999991	370.711807	6.108301
6.031419	361.804346	6.113306
6.174548	374.408544	6.118310
6.318060	364.604118	6.123315
6.392797	364.216114	6.128320
6.013314	362.690293	6.133325
5.752606	354.170001	6.138330
5.471699	365.691787	6.143334
6.501152	386.877183	6.148339
6.317692	382.419715	6.153344
6.323102	383.766727	6.158349
6.425363	385.968682	6.163354
6.211717	378.244635	6.168358
5.840820	367.903376	6.173363
6.009661	369.152176	6.178368
5.958841	382.466775	6.183373
6.473808	380.985184	6.188378
6.083198	378.999192	6.193382
5.990014	363.049727	6.198387
6.053967	370.945995	6.203392
6.223718	375.301419	6.208397
6.594898	369.558552	6.213402
5.960108	371.252010	6.218406
5.899918	365.380156	6.223411
6.129444	377.891812	6.228416
6.271049	379.401114	6.233421
6.335300	369.131307	6.238426
5.849643	374.253155	6.243430
6.035546	376.087750	6.248435
6.355876	383.336674	6.253440
6.111978	390.262166	6.258445
6.445328	375.970504	6.263450
5.746859	376.889277	6.268454
5.975055	380.061865	6.273459
6.297731	385.617839	6.278464
6.232181	385.751543	6.283469
6.147516	375.691576	6.288474
5.765615	379.430548	6.293478
6.040993	381.444198	6.298483
6.118792	380.074966	6.303488
6.209409	394.424232	6.308493
6.415408	386.495640	6.313498
6.158808	392.897935	6.318502
6.130275	386.923070	6.323507
6.477028	377.109140	6.328512
5.739566	372.877134	6.333517
6.235094	376.846482	6.338522
6.071174	386.448676	6.343526
6.282529	382.590952	6.348531
6.166715	379.546623	6.353536
5.862100	383.846195	6.358541
6.157320	390.102461	6.363546
5.995357	391.934272	6.368550
6.087843	387.117467	6.373555
6.373829	395.343004	6.378560
6.189272	393.723556	6.383565
6.439218	386.392391	6.388570
6.258420	377.040245	6.393574
5.846766	360.362094	6.398579
5.897666	378.507656	6.403584
6.066478	383.454842	6.408589
6.200697	393.308010	6.413594
6.160981	386.771745	6.418598
6.380456	382.529947	6.423603
6.214181	391.271981	6.428608
5.967028	381.996601	6.433613
6.412550	374.986163	6.438618
5.937410	380.501839	6.443622
6.195756	368.370022	6.448627
6.200944	370.375121	6.453632
6.110168	370.180562	6.458637
5.990540	365.978911	6.463642
6.030861	377.640514	6.468646
6.390699	383.867735	6.473651
5.950245	379.791961	6.478656
5.726794	388.894068	6.483661
6.331752	384.845349	6.488666
6.540023	393.370882	6.493670
6.262209	387.991643	6.498675
6.288927	378.006081	6.503680
6.255134	375.907587	6.508685
6.492351	355.467999	6.513690
5.782816	375.519450	6.518694
5.905299	365.133012	6.523699
6.143715	367.576353	6.528704
5.800075	370.860119	6.533709
5.892708	380.533095	6.538714
6.130979	389.053956	6.543718
6.593376	389.434486	6.548723
6.326788	376.387825	6.553728
6.135345	385.968994	6.558733
6.304133	368.466481	6.563738
5.785774	368.284713	6.568742
5.852995	366.857018	6.573747
6.174237	377.209398	6.578752
6.375016	380.791210	6.583757
6.297128	372.603108	6.588762
5.941055	373.326204	6.593766
6.189676	372.930108	6.598771
6.395393	368.563908	6.603776
6.183416	368.859613	6.608781
6.152560	360.243420	6.613786
5.767595	371.183471	6.618790
6.143790	371.264215	6.623795
6.254907	375.252286	6.628800
6.039323	379.120385	6.633805
6.308492	364.841888	6.638810
6.094666	369.690461	6.643814
6.352156	359.915748	6.648819
6.175277	358.152741	6.653824
5.956338	371.085388	6.658829
6.374209	354.667224	6.663834
6.225523	361.441842	6.668838
6.258927	364.012014	6.673843
5.990973	359.912551	6.678848
5.877349	362.559398	6.683853
6.382318	354.932279	6.688858
6.171887	357.920060	6.693862
6.233421	368.939285	6.698867
6.073523	354.427048	6.703872
5.788536	360.609128	6.708877
5.812848	351.579396	6.713882
6.132343	374.210399	6.718886
6.309954	381.487871	6.723891
6.433164	371.575872	6.728896
6.007324	369.342270	6.733901
6.372876	360.711813	6.738906
6.188175	368.593012	6.743910
6.185831	368.520725	6.748915
5.903633	363.126358	6.753920
5.896076	364.051451	6.758925
5.947610	362.287681	6.763930
6.131967	372.142522	6.768934
6.318134	378.808064	6.773939
6.314896	372.595151	6.778944
5.796242	369.145315	6.783949
6.544570	371.265660	6.788954
6.162196	357.522041	6.793958
5.837439	357.537917	6.798963
6.189020	360.349610	6.803968
6.222464	372.695642	6.808973
6.521826	368.311697	6.813978
6.198911	357.570673	6.818982
5.825253	363.466008	6.823987
6.208913	362.757825	6.828992
5.890474	358.065119	6.833997
5.994512	349.427929	6.839002
6.131312	362.476022	6.844006
6.182961	379.552134	6.849011
6.278273	381.296432	6.854016
6.298924	381.087688	6.859021
6.014410	372.181958	6.864026
6.268466	366.488964	6.869030
5.814797	367.417077	6.874035
6.254530	362.770837	6.879040
5.918170	374.848585	6.884045
6.397152	373.556093	6.889050
6.197330	372.467364	6.894054
6.338810	368.228223	6.899059
6.553224	366.609933	6.904064
6.270063	368.495413	6.909069
6.038446	357.718028	6.914074
6.000868	359.761421	6.919078
6.047328	357.859239	6.924083
6.097962	362.394555	6.929088
6.015982	363.464111	6.934093
6.401855	360.474550	6.939098
5.799139	365.089445	6.944102
6.150292	374.541836	6.949107
6.014353	362.465085	6.954112
6.037320	372.196360	6.959117
5.971433	361.434297	6.964122
6.172449	372.039507	6.969126
6.304377	373.619917	6.974131
6.367050	370.576273	6.979136
5.873243	370.571014	6.984141
6.218301	359.646895	6.989146
5.852128	365.569538	6.994150
6.016853	377.835022	6.999155
6.182362	383.175023	7.004160
6.017248	388.522211	7.009165
6.416655	381.392401	7.014170
6.339331	397.789430	7.019174
6.126400	380.064768	7.024179
6.123934	377.021774	7.029184
5.814667	372.413055	7.034189
5.944035	376.967753	7.039194
6.399599	382.442925	7.044198
5.937789	384.011377	7.049203
6.186019	391.897945	7.054208
6.002923	385.213164	7.059213
6.359470	384.736990	7.064218
6.383105	387.988885	7.069222
6.157648	380.959529	7.074227
6.299770	360.221534	7.079232
5.834127	372.670581	7.084237
6.186448	371.217479	7.089242
5.963217	380.737157	7.094246
6.229660	378.981053	7.099251
6.518386	386.013439	7.104256
5.951076	368.454694	7.109261
6.037732	371.225380	7.114266
5.707388	377.487293	7.119270
6.120522	389.182605	7.124275
6.622362	388.244053	7.129280
6.360177	385.032690	7.134285
6.275538	367.205809	7.139290
5.852260	371.634582	7.144294
5.873950	363.990957	7.149299
6.051192	368.791296	7.154304
5.784143	381.952902	7.159309
6.465208	384.036265	7.164314
6.288448	388.891726	7.169318
6.164967	392.609447	7.174323
6.463025	383.334600	7.179328
6.319697	378.750662	7.184333
6.249974	368.805431	7.189338
6.199651	366.769622	7.194342
6.029599	373.421023	7.199347
6.157552	363.666476	7.204352
5.936489	365.849167	7.209357
6.179997	372.037550	7.214362
6.022776	364.814081	7.219366
5.938013	373.375738	7.224371
6.181018	380.570262	7.229376
6.106666	380.525004	7.234381
6.221676	382.728137	7.239386
6.248337	373.498714	7.244390
6.001434	363.938571	7.249395
5.881510	368.256838	7.254400
6.279645	389.167213	7.259405
6.429355	383.680283	7.264410
6.225380	373.755951	7.269414
6.290761	378.368068	7.274419
6.272096	359.512208	7.279424
5.937930	362.702749	7.284429
6.257008	358.097441	7.289434
6.504135	367.762175	7.294438
6.150321	362.037278	7.299443
5.921366	362.433702	7.304448
5.908453	367.216191	7.309453
5.961435	365.126334	7.314458
6.026818	362.876360	7.319462
6.065078	361.304480	7.324467
6.313541	362.297278	7.329472
6.088144	367.577916	7.334477
6.566719	360.027670	7.339482
6.459742	362.879123	7.344486
6.076909	359.696040	7.349491
6.607013	362.438810	7.354496
5.784440	361.298348	7.359501
6.168557	371.890868	7.364506
6.156511	365.938753	7.369510
6.111781	370.286441	7.374515
6.382944	355.877929	7.379520
5.769858	369.232605	7.384525
6.126993	367.794572	7.389530
5.837040	363.768135	7.394534
6.062646	359.905033	7.399539
6.276505	371.182113	7.404544
6.036618	374.800898	7.409549
6.340319	358.523891	7.414554
6.538164	367.759706	7.419558
6.356794	371.764843	7.424563
6.412406	361.202160	7.429568
6.235207	370.148361	7.434573
6.493443	370.237980	7.439578
6.172774	364.431992	7.444582
5.849597	357.857616	7.449587
6.317233	360.616439	7.454592
6.040525	365.452655	7.459597
6.246614	361.200292	7.464602
6.259064	372.037338	7.469606
6.040319	365.298005	7.474611
6.296197	367.529822	7.479616
6.458378	360.028838	7.484621
6.410007	360.302234	7.489626
6.231573	343.008829	7.494630
6.099301	344.595571	7.499635
6.107650	331.708613	7.504640
5.660997	351.390082	7.509645
6.258887	347.763244	7.514650
5.979358	358.671052	7.519654
6.152501	358.599916	7.524659
6.392778	369.749497	7.529664
6.019723	370.794771	7.534669
6.032194	358.878411	7.539674
6.158761	365.179909	7.544678
6.185007	365.137972	7.549683
6.348767	352.976600	7.554688
6.255861	368.398443	7.559693
6.463318	359.052294	7.564698
6.272543	349.511893	7.569702
5.905676	338.825179	7.574707
5.894298	342.892426	7.579712
5.553431	345.131732	7.584717
5.902193	349.509897	7.589722
5.948077	363.543405	7.594726
6.226181	362.677654	7.599731
5.980884	363.190515	7.604736
6.120103	367.756332	7.609741
6.113560	357.440607	7.614746
6.270959	363.360823	7.619750
5.924469	369.985910	7.624755
6.148005	374.336124	7.629760
5.981533	371.685656	7.634765
6.365320	373.938688	7.639770
6.328551	366.437040	7.644774
5.772858	370.642824	7.649779
6.186936	359.451698	7.654784
6.283212	360.768743	7.659789
6.366929	360.205336	7.664794
6.158891	357.121587	7.669798
6.098460	377.445294	7.674803
6.450654	364.675616	7.679808
5.873671	363.465279	7.684813
6.187680	363.210861	7.689818
6.145613	361.376245	7.694822
6.165175	371.917959	7.699827
6.407016	361.512939	7.704832
5.529470	359.115553	7.709837
5.844228	355.434721	7.714842
6.430286	352.973970	7.719846
6.571259	359.605413	7.724851
6.371132	357.627730	7.729856
6.084084	358.931692	7.734861
5.882973	362.778551	7.739866
6.229493	360.500624	7.744870
6.146276	360.399800	7.749875
6.074833	358.392591	7.754880
5.957765	372.214198	7.759885
6.190821	366.736443	7.764890
6.392244	366.458425	7.769894
6.103152	368.851022	7.774899
6.316306	368.466776	7.779904
6.059526	366.874395	7.784909
6.659025	368.388333	7.789914
6.484182	363.837780	7.794918
5.711128	349.155263	7.799923
6.154810	356.967092	7.804928
6.023176	361.135323	7.809933
6.176666	362.443460	7.814938
6.185392	360.588281	7.819942
6.261101	364.898234	7.824947
5.905398	355.880211	7.829952
5.977155	363.810061	7.834957
6.241526	361.911915	7.839962
6.576799	361.344143	7.844966
5.830140	357.293904	7.849971
5.954287	359.865765	7.854976
5.941437	362.376700	7.859981
6.283890	364.376743	7.864986
6.546582	366.908052	7.869990
6.129245	369.095993	7.874995
6.088443	356.374855	7.880000
6.163559	361.441025	7.885005
6.124263	363.494177	7.890010
6.316478	368.988201	7.895014
5.727404	362.819049	7.900019
6.311374	367.533915	7.905024
5.992697	370.601825	7.910029
5.893073	360.461940	7.915034
6.174503	364.300107	7.920038
6.360120	367.564743	7.925043
6.258452	369.868048	7.930048
6.026061	359.995604	7.935053
6.475925	363.586087	7.940058
5.986770	354.063667	7.945062
6.293713	363.870943	7.950067
6.378254	350.731666	7.955072
5.629718	355.581231	7.960077
6.560608	348.906515	7.965082
6.374667	351.339996	7.970086
6.199585	345.125375	7.975091
6.133136	341.488081	7.980096
6.126607	355.786003	7.985101
5.670270	345.980072	7.990106
5.801888	350.107312	7.995110
6.110356	368.222251	8.000115
6.555614	359.011476	8.005133
6.393303	350.185297	8.010150
6.325962	345.481375	8.015168
5.998295	342.935417	8.020186
5.883583	347.910895	8.025203
5.930077	347.212685	8.030221
6.139302	365.789019	8.035238
6.587109	365.211352	8.040256
6.224843	349.152026	8.045274
5.632158	347.035473	8.050291
6.262370	354.381612	8.055309
6.398905	367.020890	8.060326
6.210772	366.879890	8.065344
6.139544	358.408736	8.070362
6.341885	369.166476	8.075379
6.536284	355.630188	8.080397
5.971489	349.025132	8.085414
6.028137	348.751352	8.090432
6.515540	348.700823	8.095450
6.161915	354.896864	8.100467
6.222336	342.375472	8.105485
5.920831	354.401325	8.110502
5.789010	364.955483	8.115520
6.341893	367.094241	8.120538
6.270647	375.755057	8.125555
6.354314	363.974762	8.130573
6.463021	360.887513	8.135590
6.221600	370.505737	8.140608
6.252970	370.775507	8.145626
6.397509	375.316172	8.150643
6.769055	364.617618	8.155661
6.394009	366.635777	8.160678
6.087160	348.955291	8.165696
6.352640	347.563458	8.170714
6.035299	361.340004	8.175731
6.219338	361.683828	8.180749
6.081157	358.669732	8.185766
6.111589	365.730583	8.190784
6.358546	372.319090	8.195802
6.336445	377.157086	8.200819
6.238173	372.334903	8.205837
6.244378	378.481239	8.210854
6.042709	373.782446	8.215872
6.137029	364.203129	8.220890
6.310013	368.275485	8.225907
6.306055	368.459242	8.230925
6.315685	374.166409	8.235942
6.296419	377.394588	8.240960
6.297009	372.544389	8.245978
6.281356	371.751718	8.250995
6.208663	368.134163	8.256013
6.282980	365.648684	8.261030
6.226153	377.532321	8.266048
6.550407	373.575265	8.271066
6.409283	376.235467	8.276083
6.404048	368.713348	8.281101
6.607578	379.871676	8.286118
6.236218	382.854889	8.291136
6.488191	375.993274	8.296154
6.404228	385.082087	8.301171
6.500289	381.854799	8.306189
6.525806	385.281124	8.311206
6.133181	390.186280	8.316224
6.679902	395.033543	8.321242
6.531208	396.161283	8.326259
6.712473	397.991849	8.331277
6.442528	380.450746	8.336294
6.222014	379.459609	8.341312
6.872236	387.181323	8.346330
6.631942	384.287257	8.351347
6.224246	373.811004	8.356365
6.407922	366.117469	8.361382
5.950379	392.929730	8.366400
6.558275	388.912731	8.371418
6.551022	393.975627	8.376435
6.687184	396.034110	8.381453
6.948131	397.300032	8.386470
6.604769	386.387742	8.391488
6.294317	374.845519	8.396506
5.918583	388.072628	8.401523
6.291354	387.746472	8.406541
6.360669	387.142533	8.411558
6.447605	394.683722	8.416576
7.104314	390.075328	8.421594
6.833600	403.778378	8.426611
7.058296	394.835120	8.431629
6.829882	389.124369	8.436646
6.570030	394.355975	8.441664
6.635171	380.300178	8.446682
6.662040	374.398214	8.451699
6.498846	373.963012	8.456717
6.524886	374.634379	8.461734
6.692314	375.927482	8.466752
6.724919	378.642682	8.471770
6.725492	388.358930	8.476787
6.404464	375.739122	8.481805
6.610031	377.480700	8.486822
6.568418	386.720702	8.491840
6.516395	386.858297	8.496858
6.285813	398.093693	8.501875
6.457618	393.412481	8.506893
6.625687	396.841857	8.511910
6.753919	398.945755	8.516928
7.067758	394.450701	8.521946
6.932255	393.774514	8.526963
7.069911	393.914133	8.531981
6.850798	379.006391	8.536998
6.428398	382.120621	8.542016
6.747947	376.889417	8.547034
6.849392	393.242056	8.552051
6.583383	393.261497	8.557069
6.790714	385.065680	8.562087
6.829495	394.876963	8.567104
6.687961	384.463399	8.572122
6.567185	397.720243	8.577139
6.747779	392.558005	8.582157
6.787129	386.698272	8.587175
6.581792	403.439495	8.592192
7.117580	396.814534	8.597210
6.992486	389.424672	8.602227
6.642123	396.150368	8.607245
6.770036	388.632755	8.612263
6.396762	391.168166	8.617280
6.892666	393.353666	8.622298
6.211618	396.126336	8.627315
6.345000	398.614420	8.632333
6.827144	384.077149	8.637351
6.844384	395.296047	8.642368
6.902791	395.350180	8.647386
6.658907	394.933852	8.652403
6.587942	391.492740	8.657421
6.638936	394.618469	8.662439
6.664325	402.361738	8.667456
6.618325	400.926884	8.672474
6.814290	390.669041	8.677491
7.021117	395.234726	8.682509
7.015255	388.539475	8.687527
6.707908	395.577194	8.692544
6.588079	391.765012	8.697562
6.869791	393.602027	8.702579
6.607081	409.250868	8.707597
7.038808	415.188961	8.712615
6.993357	416.502589	8.717632
7.001926	420.483797	8.722650
7.097632	406.211792	8.727667
6.665565	400.876711	8.732685
6.341575	399.952174	8.737703
6.868480	418.570615	8.742720
7.299482	425.960423	8.747738
7.021304	424.669008	8.752755
7.084983	422.942533	8.757773
7.076702	409.330469	8.762791
6.958326	419.282993	8.767808
7.131109	410.934760	8.772826
7.283399	391.639634	8.777843
7.049925	398.826790	8.782861
7.023912	391.184826	8.787879
6.759075	394.631114	8.792896
7.031187	395.579733	8.797914
7.038197	394.770910	8.802931
6.763891	394.286739	8.807949
7.012615	393.067916	8.812967
6.937002	416.021352	8.817984
7.120228	413.503131	8.823002
7.072908	412.570229	8.828019
7.069378	415.316306	8.833037
6.961070	396.797014	8.838055
6.928015	404.306399	8.843072
7.049680	415.057794	8.848090
7.282981	410.275489	8.853107
6.951325	408.651592	8.858125
7.365084	410.559564	8.863143
6.891505	408.528595	8.868160
6.997807	414.312238	8.873178
7.303069	422.696717	8.878195
6.750504	413.214936	8.883213
7.219212	415.079641	8.888231
7.195293	407.522547	8.893248
6.924423	415.340350	8.898266
7.268941	415.955820	8.903283
7.343319	415.057616	8.908301
6.771909	404.581589	8.913319
7.235164	414.787518	8.918336
6.934577	416.854047	8.923354
7.188624	425.293836	8.928371
6.953294	428.284278	8.933389
7.262023	411.568185	8.938407
7.265349	420.264748	8.943424
7.114370	424.251864	8.948442
7.289512	430.422406	8.953459
7.004779	425.357853	8.958477
7.654380	416.588257	8.963495
7.145287	411.634376	8.968512
7.666269	412.181348	8.973530
7.296707	403.444213	8.978547
6.916254	402.383308	8.983565
7.327713	415.516275	8.988583
7.184222	419.489601	8.993600
6.962988	424.850896	8.998618
7.350244	423.556856	9.003635
7.221553	428.064341	9.008653
7.341111	424.647204	9.013671
7.351748	427.485747	9.018688
7.536372	428.583682	9.023706
7.383105	414.277855	9.028723
6.724050	411.960199	9.033741
7.379212	407.453022	9.038759
7.511360	417.328672	9.043776
7.194421	409.564748	9.048794
7.673513	415.669027	9.053811
7.385129	415.556258	9.058829
6.956108	397.074278	9.063847
6.845398	406.867819	9.068864
7.288740	415.009901	9.073882
7.541512	414.674027	9.078899
6.931570	422.484668	9.083917
7.408540	416.802931	9.088935
7.484922	421.729742	9.093952
7.212195	421.933257	9.098970
7.598184	427.875319	9.103987
7.394265	424.252939	9.109005
7.505802	415.507161	9.114023
7.710811	420.290876	9.119040
7.239451	417.666298	9.124058
7.565888	416.615246	9.129075
7.563908	415.192470	9.134093
7.392164	411.126449	9.139111
7.257882	411.854334	9.144128
7.377776	418.238591	9.149146
7.248429	417.432063	9.154163
7.346928	418.303578	9.159181
7.379309	415.483811	9.164199
7.511930	422.702335	9.169216
7.234332	423.884859	9.174234
7.237089	420.255546	9.179251
6.974683	418.838606	9.184269
7.300883	425.313814	9.189287
7.112555	425.990158	9.194304
6.934590	417.267364	9.199322
7.499899	418.709950	9.204339
7.086373	425.019479	9.209357
7.503905	433.916632	9.214375
7.770656	444.093216	9.219392
7.484285	446.577237	9.224410
7.774755	447.358906	9.229427
7.546611	449.442561	9.234445
7.749237	439.543397	9.239463
7.611771	433.815316	9.244480
7.250024	426.544331	9.249498
7.589661	431.152460	9.254515
7.460503	448.774913	9.259533
7.475427	446.030440	9.264551
7.433991	447.649544	9.269568
7.276588	455.506499	9.274586
7.793263	452.914267	9.279603
7.589065	456.903365	9.284621
7.256546	448.027903	9.289639
7.555707	451.730355	9.294656
7.224521	446.174436	9.299674
7.573729	445.104058	9.304691
7.333504	450.405205	9.309709
7.786889	449.577371	9.314727
7.632570	451.053112	9.319744
7.658499	453.655759	9.324762
7.684424	452.206547	9.329779
7.765509	450.505760	9.334797
7.400094	449.287883	9.339815
7.813980	446.885216	9.344832
7.874650	455.878966	9.349850
7.685368	442.004738	9.354867
7.549435	447.744060	9.359885
7.805474	445.788827	9.364903
7.910223	446.558389	9.369920
7.578256	443.416667	9.374938
7.812329	444.573173	9.379955
7.446627	448.631594	9.384973
7.481381	453.246175	9.389991
7.670018	439.480357	9.395008
7.638206	446.857030	9.400026
7.765621	440.977257	9.405043
7.579373	455.872655	9.410061
7.454629	453.768435	9.415079
7.926274	454.035926	9.420096
7.834626	458.405113	9.425114
7.794690	456.382358	9.430131
7.812176	448.941870	9.435149
7.734087	451.626981	9.440167
7.868507	446.699123	9.445184
7.550870	450.589123	9.450202
8.247070	454.204513	9.455219
7.511117	456.711199	9.460237
7.753820	454.070109	9.465255
7.776594	455.931669	9.470272
8.089879	457.034819	9.475290
8.070700	459.874853	9.480307
7.853563	452.767526	9.485325
7.827457	448.303297	9.490343
8.296224	438.514168	9.495360
7.909857	444.147321	9.500378
7.885225	442.078005	9.505395
7.695309	446.569782	9.510413
7.779404	451.246104	9.515431
7.721430	447.468459	9.520448
7.553212	457.507656	9.525466
8.129024	460.390746	9.530483
8.032025	475.461604	9.535501
8.013293	470.355623	9.540519
7.947081	456.979749	9.545536
7.820376	472.474932	9.550554
7.934408	478.187968	9.555571
7.964640	475.605201	9.560589
8.022812	478.265944	9.565607
8.160459	478.853669	9.570624
8.129426	472.701924	9.575642
7.973310	458.749938	9.580659
7.623723	450.028604	9.585677
8.101567	472.308989	9.590695
8.309478	469.152629	9.595712
7.880758	460.323696	9.600730
8.386486	463.170363	9.605747
8.134204	453.045388	9.610765
7.981062	449.175268	9.615783
8.055123	450.407178	9.620800
7.893469	453.515535	9.625818
7.990893	455.043595	9.630835
8.152193	458.549773	9.635853
8.320185	461.281775	9.640871
8.142998	461.473570	9.645888
8.079815	457.428502	9.650906
8.214931	458.376365	9.655923
8.104031	454.442864	9.660941
8.203990	454.534707	9.665959
8.112756	444.397285	9.670976
8.086511	461.369442	9.675994
7.989255	450.879520	9.681011
7.677943	456.867047	9.686029
7.917965	464.292917	9.691047
8.086777	472.651329	9.696064
8.458946	470.116306	9.701082
8.099788	470.061891	9.706099
8.466229	472.359072	9.711117
8.184807	464.087844	9.716135
7.946863	448.154232	9.721152
7.662160	460.127049	9.726170
8.068494	474.750327	9.731187
8.261564	480.545728	9.736205
8.039356	479.731566	9.741223
8.097949	474.499941	9.746240
8.118342	487.106896	9.751258
8.434730	477.515032	9.756275
8.183582	478.800734	9.761293
8.311608	475.120350	9.766311
8.387605	475.260102	9.771328
8.341931	480.010283	9.776346
7.983316	468.611191	9.781363
8.442096	469.817915	9.786381
8.328772	477.358762	9.791399
8.163493	468.908511	9.796416
8.413817	476.462164	9.801434
8.235615	469.279343	9.806451
8.519646	467.767853	9.811469
7.937203	474.220458	9.816487
8.201629	470.881738	9.821504
8.174184	474.439396	9.826522
8.264372	482.103187	9.831539
8.200665	482.952625	9.836557
8.329024	486.514428	9.841575
8.212372	476.346233	9.846592
7.969816	480.536960	9.851610
8.082296	474.605855	9.856627
8.215725	490.682216	9.861645
8.906881	491.139583	9.866663
8.707197	488.876620	9.871680
8.485769	482.442105	9.876698
8.238218	481.874874	9.881715
8.413827	473.220074	9.886733
7.950507	479.518440	9.891751
8.428568	490.040829	9.896768
8.207916	496.373999	9.901786
8.957948	498.766087	9.906803
8.408201	488.340283	9.911821
8.135420	489.077113	9.916839
8.560417	490.099759	9.921856
8.675556	503.644984	9.926874
8.668966	494.772399	9.931891
8.793092	486.068806	9.936909
8.291462	484.992050	9.941927
8.371413	481.284437	9.946944
8.441109	484.195840	9.951962
8.502889	483.062920	9.956979
9.020176	489.296971	9.961997
8.237285	482.015798	9.967015
8.230510	479.924763	9.972032
8.381687	493.205605	9.977050
8.680615	505.071805	9.982067
8.768931	502.372698	9.987085
8.264773	501.864354	9.992103
8.501355	505.696476	9.997120
8.693071	511.422673	10.002138
8.736623	509.983333	10.007155
8.903343	505.858280	10.012173
8.895639	503.060519	10.017191
8.860438	478.956858	10.022208
8.679175	475.116355	10.027226
8.395984	484.703276	10.032243
8.704489	471.644572	10.037261
8.374221	461.683206	10.042279
8.764786	483.055742	10.047296
8.405842	484.282492	10.052314
8.670834	501.184096	10.057331
8.838172	492.830362	10.062349
8.415700	487.746213	10.067367
8.555520	484.843439	10.072384
8.667183	492.942527	10.077402
8.603191	496.714154	10.082419
8.787572	488.897386	10.087437
8.647616	499.260395	10.092455
8.663062	490.772528	10.097472
8.854922	494.712592	10.102490
8.916811	496.994080	10.107507
9.172423	489.484944	10.112525
8.718599	491.748901	10.117543
8.877779	495.864459	10.122560
9.120080	493.605261	10.127578
8.721652	484.459189	10.132595
8.946815	476.935864	10.137613
8.533890	474.343204	10.142631
8.825531	477.488281	10.147648
8.562436	486.207422	10.152666
8.900632	486.006564	10.157683
9.199393	488.377398	10.162701
8.881338	489.253814	10.167719
8.649123	478.103267	10.172736
8.659727	490.197376	10.177754
8.226434	487.948696	10.182771
8.774188	493.518472	10.187789
8.979172	497.286088	10.192807
8.805203	500.232276	10.197824
8.619685	500.627331	10.202842
8.641992	496.155552	10.207859
8.993796	493.958196	10.212877
8.601812	499.497571	10.217895
8.942871	491.646940	10.222912
8.880726	490.012630	10.227930
8.425966	500.989518	10.232947
8.815277	495.804220	10.237965
8.933988	491.519395	10.242983
8.963746	511.042121	10.248000
9.094459	518.017994	10.253018
9.180909	509.007845	10.258035
9.080606	493.071696	10.263053
8.983442	500.777288	10.268071
8.947919	497.620958	10.273088
9.001508	495.984406	10.278106
8.876265	502.570954	10.283123
9.048822	500.448840	10.288141
9.193799	506.895493	10.293159
9.267919	504.163883	10.298176
9.136646	499.299468	10.303194
8.837604	499.125245	10.308211
9.190633	505.378565	10.313229
9.179622	497.226158	10.318247
9.126984	497.095618	10.323264
8.884082	486.801913	10.328282
8.690239	498.719586	10.333299
9.223835	503.325937	10.338317
9.033704	520.001788	10.343335
9.009834	527.307832	10.348352
9.491478	520.621832	10.353370
9.311019	523.509076	10.358387
9.423349	507.836441	10.363405
9.012854	504.871030	10.368423
9.184407	501.764505	10.373440
9.301810	494.753390	10.378458
9.152487	502.691155	10.383475
8.959841	497.893098	10.388493
8.951120	506.320191	10.393511
9.128061	508.896179	10.398528
9.357110	508.990013	10.403546
9.132777	525.888935	10.408563
9.315711	522.891083	10.413581
9.594234	517.861878	10.418599
9.165437	511.746804	10.423616
9.263696	494.934020	10.428634
8.878987	500.882498	10.433651
9.216354	515.592285	10.438669
9.318306	515.330382	10.443687
9.164573	522.899631	10.448704
9.404482	515.380306	10.453722
9.562309	530.108590	10.458739
9.753397	512.085339	10.463757
9.235667	505.160485	10.468775
9.194964	497.830018	10.473792
9.184698	504.004208	10.478810
9.487223	514.875820	10.483827
9.370712	511.691073	10.488845
9.150264	514.407825	10.493863
9.036259	511.983204	10.498880
9.596211	522.442371	10.503898
9.498955	521.567729	10.508915
9.298142	526.477771	10.513933
9.666749	519.317086	10.518951
9.556952	520.871104	10.523968
9.342925	506.685111	10.528986
9.489863	514.340080	10.534003
9.303795	513.056407	10.539021
9.418936	515.910249	10.544039
9.286015	518.616530	10.549056
9.129412	522.948511	10.554074
9.657447	520.300854	10.559091
9.451622	517.066899	10.564109
9.767580	523.729922	10.569127
9.515991	527.174173	10.574144
9.810123	521.492469	10.579162
9.214679	521.881924	10.584179
9.584997	527.113279	10.589197
9.669535	527.699807	10.594215
9.560637	531.301715	10.599232
9.762135	526.227698	10.604250
9.604609	521.932228	10.609267
9.697191	512.413060	10.614285
9.366780	511.284399	10.619303
9.309251	525.209959	10.624320
9.482109	525.265206	10.629338
9.387494	528.729196	10.634355
9.796234	528.501575	10.639373
9.896777	529.776703	10.644391
9.679560	529.024875	10.649408
9.771983	522.601437	10.654426
9.633882	532.033254	10.659443
9.765342	528.112494	10.664461
9.486344	519.051946	10.669479
9.330740	525.018407	10.674496
9.865123	522.499144	10.679514
9.633869	526.950042	10.684531
9.787730	525.887985	10.689549
10.028900	523.755185	10.694567
9.731875	513.558251	10.699584
9.947452	514.095975	10.704602
9.566852	507.121369	10.709619
9.665959	504.856063	10.714637
9.715543	506.101255	10.719655
9.804364	522.484379	10.724672
9.795054	519.907763	10.729690
9.439176	516.706637	10.734707
9.831002	515.686422	10.739725
10.082294	528.573023	10.744743
9.722610	526.786228	10.749760
10.014739	525.323963	10.754778
10.022769	517.989056	10.759795
9.369941	507.901168	10.764813
9.535798	506.783598	10.769831
9.672430	522.868958	10.774848
9.802857	515.884207	10.779866
9.980505	534.358342	10.784883
10.110776	520.633105	10.789901
9.663171	518.790576	10.794919
9.750003	524.832895	10.799936
9.958190	526.469942	10.804954
9.867801	528.106143	10.809971
9.571588	523.765997	10.814989
9.878052	528.900002	10.820007
9.709473	526.834155	10.825024
9.877086	520.282251	10.830042
9.877829	522.604820	10.835059
9.886386	518.703197	10.840077
10.044067	521.755535	10.845095
9.823606	525.993322	10.850112
10.109411	520.082551	10.855130
9.889274	519.182862	10.860147
9.719693	519.121020	10.865165
10.239905	526.992420	10.870183
9.800046	529.105891	10.875200
9.693740	526.456016	10.880218
9.903785	527.584712	10.885235
9.828731	525.053043	10.890253
9.962274	522.949624	10.895271
10.131021	538.067518	10.900288
10.358522	538.694901	10.905306
9.851229	534.829411	10.910323
9.598883	534.445954	10.915341
10.125191	542.092359	10.920359
10.007621	550.429128	10.925376
9.873946	544.381698	10.930394
10.139477	545.249302	10.935411
10.183615	550.121212	10.940429
10.497432	551.877510	10.945447
10.201294	549.736850	10.950464
10.363159	540.361508	10.955482
10.448301	548.928635	10.960499
10.213149	539.375276	10.965517
10.391489	525.904472	10.970535
9.987975	527.993350	10.975552
10.229796	539.947356	10.980570
10.451988	530.676231	10.985587
10.167209	531.465421	10.990605
9.921322	529.275916	10.995623
10.354648	536.517092	11.000640
10.327126	540.014817	11.005658
10.461393	555.699804	11.010675
9.986525	540.629784	11.015693
10.555253	544.656343	11.020711
10.281307	539.381804	11.025728
10.254382	536.340888	11.030746
10.186654	535.613120	11.035763
9.695500	550.338329	11.040781
9.901841	552.035624	11.045799
10.199982	560.777868	11.050816
10.169017	540.169951	11.055834
10.317748	547.016804	11.060851
10.269469	548.428708	11.065869
10.560994	544.542980	11.070887
10.463916	537.328567	11.075904
10.471854	538.084805	11.080922
10.139495	546.619109	11.085939
9.919725	549.474610	11.090957
10.411297	543.882074	11.095975
10.084258	552.892059	11.100992
10.344367	550.923558	11.106010
10.495098	543.512776	11.111027
10.448029	548.701830	11.116045
10.566663	540.939455	11.121063
10.479462	552.228360	11.126080
10.343524	551.135687	11.131098
10.446922	543.921614	11.136115
10.416795	557.331714	11.141133
10.831300	563.745889	11.146151
10.747146	553.124485	11.151168
10.428756	548.254478	11.156186
10.817612	549.970691	11.161203
10.233967	550.907396	11.166221
10.314773	544.422645	11.171239
10.656183	559.172862	11.176256
10.659482	549.970519	11.181274
10.587842	546.166580	11.186291
10.265078	558.593494	11.191309
10.395730	559.709308	11.196327
10.573244	575.034143	11.201344
11.219441	576.514640	11.206362
11.065400	560.757204	11.211379
10.621411	561.082055	11.216397
10.824671	550.135048	11.221415
10.222079	557.120973	11.226432
10.280213	549.816119	11.231450
10.695460	563.295730	11.236467
10.559636	575.652527	11.241485
11.193171	566.762288	11.246503
10.805544	566.570299	11.251520
10.603489	559.429024	11.256538
10.658527	553.399544	11.261555
10.545950	564.146476	11.266573
10.699621	566.457863	11.271591
10.639789	574.943437	11.276608
10.653444	571.318708	11.281626
11.135400	577.482555	11.286643
11.007376	576.376025	11.291661
11.510918	570.787927	11.296679
10.819822	566.480852	11.301696
11.013649	559.012863	11.306714
10.618674	558.127770	11.311731
10.506827	554.803440	11.316749
10.767258	554.330678	11.321767
10.581925	556.278297	11.326784
10.592753	564.932738	11.331802
11.147735	564.180595	11.336819
11.137094	573.242310	11.341837
10.978613	559.312703	11.346855
11.126395	549.251612	11.351872
10.742006	559.895701	11.356890
10.803248	549.153835	11.361907
10.643779	553.230661	11.366925
11.120643	565.943318	11.371943
10.919086	559.515148	11.376960
11.067216	575.046521	11.381978
11.358349	563.612473	11.386995
10.845696	556.140877	11.392013
10.896677	553.737897	11.397031
10.589456	561.794944	11.402048
10.904077	567.287436	11.407066
10.982653	580.011626	11.412083
10.989855	583.948904	11.417101
10.861089	573.640534	11.422119
10.770896	569.754275	11.427136
10.898287	572.047664	11.432154
11.116346	569.120072	11.437171
10.868373	572.169309	11.442189
10.897249	566.099718	11.447207
11.078364	572.941538	11.452224
10.578578	567.951451	11.457242
10.945366	572.340804	11.462259
10.590651	578.350907	11.467277
11.111587	583.710301	11.472295
11.128040	590.091791	11.477312
11.322052	601.488415	11.482330
11.620610	594.654175	11.487347
11.115578	582.198564	11.492365
10.711821	582.422480	11.497383
11.259082	586.212560	11.502400
11.046550	597.887066	11.507418
11.301720	598.106216	11.512435
11.090430	602.806479	11.517453
11.578345	597.268142	11.522471
11.197164	597.860914	11.527488
10.977397	606.052681	11.532506
11.426598	596.294914	11.537523
11.163403	607.986781	11.542541
11.476740	605.363073	11.547559
11.328938	606.837812	11.552576
11.309494	600.589548	11.557594
11.535349	600.024342	11.562611
11.287254	603.102004	11.567629
11.111682	603.265148	11.572647
11.315850	611.233127	11.577664
11.204369	603.544422	11.582682
11.527838	604.806936	11.587699
11.528298	598.290496	11.592717
11.343223	603.781909	11.597735
11.338559	599.819213	11.602752
11.224463	612.961573	11.607770
11.392212	599.514452	11.612787
11.392201	608.688134	11.617805
11.368957	607.902946	11.622823
11.280786	605.527936	11.627840
11.265258	602.990143	11.632858
11.460600	593.773656	11.637875
11.345196	599.273154	11.642893
11.494839	599.597094	11.647911
11.380375	609.628007	11.652928
11.191746	606.836310	11.657946
11.496286	594.021122	11.662963
11.268639	615.834040	11.667981
11.208018	612.861471	11.672999
11.757227	610.194725	11.678016
11.550603	622.660404	11.683034
12.306174	619.343013	11.688051
11.806108	620.891534	11.693069
11.622173	610.421326	11.698087
11.871890	598.892722	11.703104
11.834141	600.400817	11.708122
11.973348	601.294404	11.713139
11.473414	605.357981	11.718157
11.363448	608.742329	11.723175
11.896972	596.197588	11.728192
11.489351	609.915801	11.733210
12.083745	606.860184	11.738227
11.625680	606.051181	11.743245
11.828004	603.176524	11.748263
11.718318	609.419876	11.753280
11.726606	613.966038	11.758298
11.856451	606.864583	11.763315
12.189031	604.013825	11.768333
11.861558	615.381203	11.773351
12.070942	608.860632	11.778368
11.646790	611.397684	11.783386
11.648197	599.996099	11.788403
11.752160	618.797361	11.793421
11.724968	610.306608	11.798439
11.579579	603.535175	11.803456
11.762455	608.991390	11.808474
11.494533	609.831606	11.813491
11.636584	608.241228	11.818509
11.348650	606.146620	11.823527
12.008556	602.228769	11.828544
11.773477	597.440447	11.833562
11.751883	604.683055	11.838579
11.712324	609.384983	11.843597
11.540634	621.873623	11.848615
12.304600	625.917139	11.853632
11.938345	630.638381	11.858650
12.216087	633.163980	11.863667
11.704761	625.600633	11.868685
11.926235	634.010880	11.873703
12.031192	629.024446	11.878720
11.676593	634.371855	11.883738
12.043423	633.765765	11.888755
12.191339	629.422714	11.893773
11.976958	628.976541	11.898791
12.143748	621.509580	11.903808
11.840678	640.068137	11.908826
12.080802	634.047680	11.913843
12.100352	628.250909	11.918861
12.185480	634.924669	11.923879
12.207348	627.268837	11.928896
12.241229	645.815962	11.933914
12.436141	632.118444	11.938931
12.305927	627.695625	11.943949
11.766985	614.450038	11.948967
12.060664	611.605336	11.953984
11.747938	633.232713	11.959002
12.137885	628.709973	11.964019
11.724241	629.680171	11.969037
11.588896	635.094426	11.974055
12.025156	635.193866	11.979072
11.913223	630.970164	11.984090
12.357545	635.464222	11.989107
12.375639	631.725184	11.994125
11.998981	633.529037	11.999143
12.227198	635.077773	12.004160
12.073969	633.940451	12.009178
12.294169	646.181906	12.014195
12.606833	653.457695	12.019213
12.347888	639.761410	12.024231
12.364949	635.309348	12.029248
12.060115	639.869556	12.034266
12.325740	644.400905	12.039283
12.265053	642.627503	12.044301
11.954067	645.172186	12.049319
12.696578	641.474987	12.054336
12.353040	654.406957	12.059354
12.390303	650.586039	12.064371
12.473409	647.625799	12.069389
12.387428	651.129492	12.074407
12.546966	651.969425	12.079424
12.588290	643.445899	12.084442
12.615179	642.207951	12.089459
12.546545	636.664740	12.094477
12.112594	639.563070	12.099495
12.489435	634.752045	12.104512
12.462247	643.993090	12.109530
12.456125	643.801660	12.114547
12.571075	640.631343	12.119565
12.319779	646.903068	12.124583
12.609264	641.332499	12.129600
12.561042	658.014785	12.134618
12.230020	647.412827	12.139635
12.601800	644.388708	12.144653
12.343430	651.343164	12.149671
12.305341	646.905997	12.154688
12.474962	643.181233	12.159706
12.417662	639.122586	12.164723
12.581994	646.191101	12.169741
12.349609	645.630971	12.174759
12.484274	653.256354	12.179776
12.654059	644.289964	12.184794
12.562057	640.385036	12.189811
13.151284	649.167207	12.194829
12.908127	654.333175	12.199847
12.843857	643.055394	12.204864
12.410778	643.138714	12.209882
12.438774	645.242469	12.214899
12.833858	636.648088	12.219917
12.749497	644.818790	12.224935
12.797582	643.078944	12.229952
12.844480	649.913290	12.234970
12.877745	648.958362	12.239987
13.131641	638.479926	12.245005
12.567287	636.513555	12.250023
12.971387	637.672002	12.255040
12.817068	638.500843	12.260058
12.650584	637.154153	12.265075
12.921954	644.518416	12.270093
12.899993	661.685749	12.275111
12.642793	655.613333	12.280128
12.665674	660.466493	12.285146
13.044024	662.256934	12.290163
13.127120	663.806177	12.295181
12.999056	667.906540	12.300199
12.860401	668.609872	12.305216
12.779272	672.242197	12.310234
13.007672	664.664643	12.315251
12.784353	670.764768	12.320269
12.758637	662.740803	12.325287
13.297243	662.694926	12.330304
13.085779	667.524616	12.335322
12.814696	665.493646	12.340339
13.150334	666.362964	12.345357
12.771549	664.295116	12.350375
12.846337	657.666100	12.355392
12.922140	665.464749	12.360410
12.773549	662.957132	12.365427
12.814545	661.716987	12.370445
12.689685	667.318960	12.375463
13.267694	676.308011	12.380480
13.192768	678.004931	12.385498
12.545701	674.113837	12.390515
13.544193	682.100181	12.395533
13.531834	693.314409	12.400551
13.490847	680.139560	12.405568
13.147314	672.755188	12.410586
12.935838	667.565555	12.415603
13.456368	670.542491	12.420621
13.160820	672.343186	12.425639
12.897346	670.696025	12.430656
13.203849	686.234394	12.435674
13.222933	693.552753	12.440691
13.561718	687.699948	12.445709
13.424174	686.396084	12.450727
13.614957	683.308623	12.455744
13.378121	670.703899	12.460762
12.943739	671.680484	12.465779
13.282508	675.051780	12.470797
13.390668	683.751083	12.475815
13.201912	686.125267	12.480832
13.347564	686.954741	12.485850
13.336297	690.213288	12.490867
13.244133	689.839600	12.495885
13.166226	697.072080	12.500903
13.304494	691.294673	12.505920
13.499105	689.314265	12.510938
12.902525	705.419277	12.515955
13.413838	690.495376	12.520973
13.246793	693.263798	12.525991
13.327884	681.723527	12.531008
13.432236	680.940559	12.536026
13.367103	683.784628	12.541043
13.616814	676.973741	12.546061
13.343473	692.709689	12.551079
13.360531	692.110720	12.556096
13.862281	710.635558	12.561114
13.720305	702.377220	12.566131
13.899488	692.569926	12.571149
13.523324	687.393306	12.576167
13.397235	685.835203	12.581184
13.626681	688.563982	12.586202
13.233986	691.657862	12.591219
13.839321	706.057850	12.596237
13.600135	710.547897	12.601255
13.764603	709.651430	12.606272
13.761016	706.527959	12.611290
13.887189	718.528492	12.616307
14.039417	705.777963	12.621325
13.465037	697.356585	12.626343
13.617090	702.053949	12.631360
13.592614	702.663768	12.636378
14.066586	708.352393	12.641395
13.959853	710.612828	12.646413
13.693000	706.103970	12.651431
13.441403	711.905564	12.656448
13.637333	711.562758	12.661466
13.846292	717.008635	12.666483
14.533237	718.659519	12.671501
14.205145	704.112444	12.676519
13.618762	700.032021	12.681536
13.789118	690.137743	12.686554
13.904766	705.235645	12.691571
13.996722	697.401620	12.696589
13.942119	706.754260	12.701607
14.039486	705.196076	12.706624
14.226498	701.317119	12.711642
13.868615	696.768790	12.716659
13.579019	683.885102	12.721677
13.662989	697.151315	12.726695
13.787204	715.204781	12.731712
13.854934	707.731117	12.736730
13.734352	709.690760	12.741747
13.888127	709.875207	12.746765
13.639765	719.040278	12.751783
13.747895	713.052969	12.756800
14.034338	713.355611	12.761818
14.048922	708.515765	12.766835
13.944124	709.684026	12.771853
14.089819	729.662295	12.776871
14.474950	729.652937	12.781888
14.055497	719.790516	12.786906
14.228397	720.625216	12.791923
14.414796	718.185351	12.796941
14.307172	712.610318	12.801959
13.980548	717.142382	12.806976
13.940400	713.188341	12.811994
14.141973	722.933435	12.817011
14.250108	722.923023	12.822029
14.500852	730.934296	12.827047
14.166373	734.505098	12.832064
14.075043	729.041128	12.837082
14.355180	731.058300	12.842099
14.564572	733.073864	12.847117
14.309875	732.037538	12.852135
14.256058	732.339511	12.857152
14.477001	722.153326	12.862170
14.222310	734.140588	12.867187
14.557272	737.007576	12.872205
14.413208	726.086137	12.877223
14.475316	718.528140	12.882240
14.493811	714.202063	12.887258
14.562447	715.602088	12.892275
14.351889	710.712091	12.897293
14.498142	710.339151	12.902311
14.144816	722.322828	12.907328
14.329367	730.846164	12.912346
14.379807	741.495240	12.917363
14.406049	744.757424	12.922381
14.779478	750.625814	12.927399
15.131935	741.375321	12.932416
14.675341	723.077169	12.937434
14.641153	726.225686	12.942451
14.054173	726.970421	12.947469
14.074304	725.995443	12.952487
14.478616	740.202703	12.957504
14.802340	735.623976	12.962522
14.689252	732.852054	12.967539
14.457020	742.882444	12.972557
14.813045	740.599197	12.977575
14.655752	735.189676	12.982592
15.002047	737.404824	12.987610
14.568208	741.350847	12.992627
14.650396	746.854339	12.997645
14.610813	741.555873	13.002663
14.583304	742.888822	13.007680
14.714608	737.576373	13.012698
14.481931	741.443740	13.017715
14.288082	744.812773	13.022733
14.441983	743.248939	13.027751
14.740237	742.161233	13.032768
14.679438	735.909893	13.037786
14.469795	740.729852	13.042803
15.204558	750.836900	13.047821
15.026585	740.832731	13.052839
14.512164	745.428754	13.057856
15.239518	750.263770	13.062874
14.882549	752.645218	13.067891
15.054467	750.744074	13.072909
14.967364	740.672110	13.077927
14.591991	745.240173	13.082944
14.695919	750.863354	13.087962
14.938763	758.645503	13.092979
15.031307	764.595498	13.097997
15.336518	751.092149	13.103015
14.904434	768.411799	13.108032
14.983471	760.980532	13.113050
14.936121	764.162661	13.118067
15.019321	755.032977	13.123085
15.011635	753.052502	13.128103
14.976295	765.987059	13.133120
15.338684	761.449641	13.138138
15.372539	761.883127	13.143155
14.773445	762.273155	13.148173
14.795852	773.204317	13.153191
14.711954	774.890020	13.158208
14.718403	775.419289	13.163226
14.583217	764.266078	13.168243
14.610873	770.043147	13.173261
15.175353	778.744030	13.178279
15.196902	793.102443	13.183296
15.391663	785.482739	13.188314
15.462665	794.976811	13.193331
15.382443	786.106077	13.198349
15.579702	771.994688	13.203367
14.907015	772.948423	13.208384
15.403557	774.752031	13.213402
15.281727	780.489264	13.218419
15.530927	789.879850	13.223437
15.510446	777.370749	13.228455
14.998901	775.358271	13.233472
15.283993	772.167752	13.238490
15.413545	792.801838	13.243507
15.486602	794.340033	13.248525
15.493199	790.725825	13.253543
15.038946	791.039655	13.258560
15.269338	783.332356	13.263578
15.568748	793.399917	13.268595
15.666426	794.426208	13.273613
15.468780	797.691703	13.278631
15.579646	797.775538	13.283648
15.660560	791.508425	13.288666
15.797921	799.089271	13.293683
15.462481	801.798724	13.298701
15.885778	789.154249	13.303719
15.326879	795.713753	13.308736
15.687151	793.915819	13.313754
15.649794	795.067273	13.318771
15.387710	799.396810	13.323789
15.183318	789.652340	13.328807
15.121393	788.216778	13.333824
15.460171	790.720274	13.338842
15.270201	795.092229	13.343859
15.155001	794.835731	13.348877
15.765338	800.525245	13.353895
15.781311	827.318080	13.358912
15.759471	818.166849	13.363930
15.907389	811.901920	13.368947
15.711364	804.229447	13.373965
15.771039	803.677486	13.378983
15.617886	811.145783	13.384000
16.125285	817.529808	13.389018
15.629997	817.196793	13.394035
15.931234	816.130707	13.399053
15.797443	810.521849	13.404071
15.709638	823.013348	13.409088
15.899109	814.005939	13.414106
16.083201	811.055194	13.419123
15.915030	813.934261	13.424141
16.236891	812.016077	13.429159
15.395043	812.734227	13.434176
15.937862	820.091011	13.439194
16.127608	807.968867	13.444211
16.075477	823.064590	13.449229
15.857073	812.489179	13.454247
16.108476	814.056411	13.459264
16.420725	814.052089	13.464282
16.331439	814.757206	13.469299
15.785325	813.911410	13.474317
15.928555	810.181254	13.479335
15.722383	826.225589	13.484352
15.537828	816.560065	13.489370
16.005576	814.401421	13.494387
15.788157	818.099176	13.499405
16.084181	813.780356	13.504423
16.116060	827.354569	13.509440
16.322863	823.652381	13.514458
16.329681	818.100521	13.519475
16.050671	819.945991	13.524493
16.334359	832.177690	13.529511
16.269908	821.685598	13.534528
15.932174	826.844252	13.539546
16.014063	817.130932	13.544563
16.174303	825.976826	13.549581
16.378277	821.306272	13.554599
16.066889	830.411786	13.559616
16.190421	842.141422	13.564634
16.184297	846.443742	13.569651
16.322758	859.092536	13.574669
16.546886	840.830284	13.579687
16.714476	851.435941	13.584704
16.258381	857.351471	13.589722
16.498319	844.874358	13.594739
16.509693	855.002578	13.599757
16.301304	857.310416	13.604775
16.699483	856.219767	13.609792
16.589486	855.173527	13.614810
16.609152	851.497314	13.619827
16.460922	851.681448	13.624845
16.695226	852.610733	13.629863
16.399520	857.709205	13.634880
16.520598	855.967440	13.639898
16.866568	850.290184	13.644915
16.486844	866.544609	13.649933
16.698549	856.457613	13.654951
17.017729	852.210916	13.659968
16.629102	842.239488	13.664986
16.493672	826.870229	13.670003
16.533114	829.808489	13.675021
16.651029	833.750675	13.680039
16.699505	843.841556	13.685056
16.302526	842.666433	13.690074
16.712572	846.269656	13.695091
16.754419	851.877289	13.700109
16.762682	839.587724	13.705127
16.584076	849.442572	13.710144
16.614825	855.446399	13.715162
16.901953	854.174230	13.720179
16.422641	849.670013	13.725197
16.522554	849.648259	13.730215
16.474409	855.061627	13.735232
16.713456	849.069667	13.740250
16.918253	868.830613	13.745267
16.857650	876.716862	13.750285
17.028119	877.290023	13.755303
17.210807	877.362676	13.760320
17.033662	864.202579	13.765338
16.874550	852.166278	13.770355
17.043217	852.922751	13.775373
16.860391	861.812610	13.780391
16.959294	863.596089	13.785408
17.288557	872.100118	13.790426
17.454800	867.444893	13.795443
16.986884	862.588613	13.800461
16.779373	851.598082	13.805479
16.843363	863.576838	13.810496
17.279821	866.936117	13.815514
16.990060	876.173984	13.820531
17.114299	880.077327	13.825549
17.242744	878.776215	13.830567
17.330163	881.514515	13.835584
17.206487	885.595310	13.840602
17.373271	868.531669	13.845619
17.081197	875.769165	13.850637
17.115924	876.808418	13.855655
17.284194	887.123662	13.860672
17.227324	887.116852	13.865690
17.223800	882.371294	13.870707
17.030554	875.550404	13.875725
17.532231	877.141789	13.880743
17.472390	884.788088	13.885760
17.229472	881.345252	13.890778
17.579673	887.513942	13.895795
17.410460	884.993726	13.900813
17.344476	880.986868	13.905831
17.329722	885.448326	13.910848
17.341120	896.169844	13.915866
17.414686	883.011723	13.920883
16.867976	889.335839	13.925901
16.907999	886.622103	13.930919
17.573813	881.611389	13.935936
17.407231	883.874852	13.940954
17.498436	868.353509	13.945971
17.241053	885.504064	13.950989
17.567568	891.808985	13.956007
17.980067	900.984861	13.961024
17.567208	895.870696	13.966042
17.824278	885.681949	13.971059
17.431343	879.195099	13.976077
17.393844	883.407640	13.981095
17.657693	890.864692	13.986112
17.898439	901.995463	13.991130
18.026123	898.157258	13.996147
17.343607	892.889423	14.001165
17.397937	894.692468	14.006183
17.866755	903.865889	14.011200
17.538489	916.587392	14.016218
17.467258	914.310687	14.021235
17.541302	910.884765	14.026253
17.610329	911.505278	14.031271
17.608235	898.343147	14.036288
17.417222	913.558398	14.041306
17.787957	907.514359	14.046323
17.506377	917.060235	14.051341
17.351298	925.598674	14.056359
18.158201	927.811558	14.061376
17.830201	933.587252	14.066394
18.285134	928.214891	14.071411
18.163773	939.635589	14.076429
18.156067	940.687764	14.081447
18.339841	924.912123	14.086464
17.985891	919.747754	14.091482
18.213576	905.278080	14.096499
18.177422	907.013165	14.101517
17.945260	906.850614	14.106535
18.357586	900.983134	14.111552
18.077643	902.336463	14.116570
18.386476	898.697267	14.121587
18.320219	898.442615	14.126605
18.086581	898.879883	14.131623
18.159717	903.681104	14.136640
17.985514	901.306827	14.141658
18.208127	905.314776	14.146675
18.209684	901.306864	14.151693
18.101087	901.093517	14.156711
18.154987	903.114376	14.161728
18.438894	923.891835	14.166746
18.485715	913.568553	14.171763
18.007257	915.258898	14.176781
17.826030	923.725670	14.181799
18.258690	919.082600	14.186816
18.664148	934.435369	14.191834
18.412977	927.617167	14.196851
18.297001	925.915460	14.201869
18.122937	930.316529	14.206887
18.308962	921.366406	14.211904
18.007105	929.145077	14.216922
18.421584	915.125984	14.221939
18.467814	924.365210	14.226957
18.112005	927.194616	14.231975
18.604475	917.922233	14.236992
18.056743	926.925742	14.242010
18.406147	928.493505	14.247027
18.489405	934.852094	14.252045
18.511524	945.931726	14.257063
18.744040	946.807648	14.262080
18.593200	954.988842	14.267098
18.872246	950.009927	14.272115
18.818649	946.449240	14.277133
18.480175	930.423553	14.282151
18.843866	942.532421	14.287168
18.941357	948.850930	14.292186
18.293717	939.443628	14.297203
18.727654	951.270171	14.302221
18.797667	951.417171	14.307239
18.918259	947.015182	14.312256
18.704722	957.263683	14.317274
19.056695	956.473707	14.322291
19.056257	956.028929	14.327309
18.993743	948.928886	14.332327
18.864257	936.629145	14.337344
18.853613	937.359891	14.342362
18.840598	927.869566	14.347379
18.921445	942.897350	14.352397
18.861230	953.428085	14.357415
19.012439	949.134935	14.362432
19.046722	960.682889	14.367450
19.067953	957.082148	14.372467
19.319183	960.927867	14.377485
18.886399	945.216646	14.382503
19.396198	935.490285	14.387520
18.729213	935.272360	14.392538
19.009044	941.546698	14.397555
19.375592	948.157824	14.402573
19.089285	952.191374	14.407591
19.094235	954.008425	14.412608
19.128143	954.763793	14.417626
19.259791	949.195613	14.422643
19.386588	941.362367	14.427661
19.118839	949.744794	14.432679
19.632940	958.772340	14.437696
19.774151	949.254835	14.442714
19.196297	934.923179	14.447731
19.178721	931.991191	14.452749
19.051845	944.823367	14.457767
19.031767	937.918688	14.462784
19.267538	942.757713	14.467802
18.990073	951.977926	14.472819
19.215979	955.174348	14.477837
19.595019	957.961928	14.482855
19.695087	955.279857	14.487872
19.435258	961.073347	14.492890
19.442547	960.564251	14.497907
18.953286	957.563690	14.502925
19.293448	951.328739	14.507943
19.369512	947.069380	14.512960
19.610433	954.006175	14.517978
19.525765	955.092424	14.522995
19.546509	964.007442	14.528013
19.589779	959.503882	14.533031
19.804876	948.838805	14.538048
19.626549	953.855913	14.543066
19.791666	953.808228	14.548083
19.660097	949.306646	14.553101
19.449413	956.411584	14.558119
19.833070	954.455361	14.563136
19.439158	957.609434	14.568154
19.398376	962.829188	14.573171
19.323350	954.891662	14.578189
19.289370	963.606921	14.583207
20.191755	963.816824	14.588224
19.782018	969.977633	14.593242
19.451224	978.556079	14.598259
19.605395	983.089090	14.603277
19.497075	988.088996	14.608295
19.271262	988.903738	14.613312
19.712478	985.322807	14.618330
19.425537	982.928202	14.623347
19.905611	970.243202	14.628365
19.715701	986.455559	14.633383
19.906467	1001.153859	14.638400
20.078393	1006.940101	14.643418
20.262054	1006.567642	14.648435
20.210454	1005.638530	14.653453
19.843209	1006.967591	14.658471
19.579318	1003.572177	14.663488
20.040644	1013.848179	14.668506
20.085802	1013.904376	14.673523
20.253866	1007.749849	14.678541
19.950402	1013.392362	14.683559
20.297515	1006.938563	14.688576
20.490164	1006.331179	14.693594
19.943237	1013.927140	14.698611
19.897125	1006.297510	14.703629
19.934977	1006.859765	14.708647
20.349886	1005.880110	14.713664
20.303994	1011.274240	14.718682
20.118374	1010.571119	14.723699
20.290472	997.631098	14.728717
20.076441	1008.223683	14.733735
20.550945	1002.191856	14.738752
20.152607	1011.200549	14.743770
19.975478	1014.248298	14.748787
20.177145	1018.474125	14.753805
20.482052	1029.105844	14.758823
20.622399	1028.370905	14.763840
20.571295	1027.732045	14.768858
20.274994	1033.581729	14.773875
20.732959	1036.476951	14.778893
20.433559	1039.120870	14.783911
20.763991	1037.816700	14.788928
20.696084	1032.522557	14.793946
20.749189	1046.181993	14.798963
20.627779	1030.766195	14.803981
20.441329	1029.798118	14.808999
20.684021	1032.982474	14.814016
20.665209	1032.950803	14.819034
20.301317	1037.188952	14.824051
20.511145	1025.950302	14.829069
20.450120	1039.595945	14.834087
20.612293	1030.475915	14.839104
20.581647	1030.386127	14.844122
20.387933	1039.243056	14.849139
20.731102	1037.899034	14.854157
20.644247	1039.298048	14.859175
20.504177	1039.187428	14.864192
20.877086	1041.202815	14.869210
20.923791	1050.776543	14.874227
20.855533	1042.979934	14.879245
20.673448	1048.884422	14.884263
21.051680	1049.018148	14.889280
21.259498	1047.998152	14.894298
20.992661	1049.422034	14.899315
21.194744	1043.413674	14.904333
21.389993	1041.884403	14.909351
20.813941	1036.549456	14.914368
21.022213	1036.545544	14.919386
21.305648	1036.687717	14.924403
20.889807	1028.547606	14.929421
20.906867	1036.709008	14.934439
21.132314	1044.888461	14.939456
21.357273	1041.221270	14.944474
21.261197	1053.578520	14.949491
21.264328	1043.643813	14.954509
21.230270	1046.959621	14.959527
21.468702	1040.282893	14.964544
21.285931	1039.437318	14.969562
21.035903	1032.890293	14.974579
21.465679	1036.594623	14.979597
21.511375	1043.912138	14.984615
21.191683	1043.747434	14.989632
21.583620	1035.711922	14.994650
21.106740	1041.709643	14.999667
21.203829	1042.423621	15.004685
21.387113	1054.778401	15.009703
21.273085	1060.719634	15.014720
21.310488	1044.439664	15.019738
21.118249	1055.047817	15.024755
21.770593	1053.065530	15.029773
21.477819	1054.850051	15.034791
21.247489	1050.587880	15.039808
21.464703	1047.234314	15.044826
21.258958	1063.266172	15.049843
21.630481	1049.461942	15.054861
21.579020	1049.536339	15.059879
21.593432	1053.803953	15.064896
21.630216	1053.296574	15.069914
21.289819	1055.000149	15.074931
21.858025	1063.981456	15.079949
21.727067	1075.997018	15.084967
21.479547	1081.533013	15.089984
21.848306	1073.258099	15.095002
21.981832	1073.770748	15.100019
21.993296	1070.468146	15.105037
22.008203	1067.546857	15.110055
22.202258	1067.551470	15.115072
22.090744	1048.798473	15.120090
21.654388	1047.702050	15.125107
21.897382	1047.506542	15.130125
21.675564	1048.020868	15.135143
21.822810	1054.221216	15.140160
22.338938	1052.585180	15.145178
22.042198	1059.094494	15.150195
22.507464	1064.494260	15.155213
22.426961	1047.415302	15.160231
22.103936	1043.653552	15.165248
22.236812	1035.421693	15.170266
22.213851	1044.968396	15.175283
22.255800	1043.535575	15.180301
22.275923	1043.220135	15.185319
21.985878	1047.027073	15.190336
22.263142	1033.010317	15.195354
22.056570	1049.411515	15.200371
22.085968	1039.097185	15.205389
22.207519	1043.468034	15.210407
22.436911	1034.997089	15.215424
22.185432	1040.969183	15.220442
21.907999	1051.398098	15.225459
22.404838	1043.668137	15.230477
21.923596	1050.692162	15.235495
22.089572	1055.769299	15.240512
22.281281	1060.252304	15.245530
22.343327	1073.556924	15.250547
22.228849	1068.856993	15.255565
22.413351	1072.362836	15.260583
21.988555	1064.817387	15.265600
22.719774	1070.311444	15.270618
22.762141	1075.310004	15.275635
22.658385	1060.494182	15.280653
22.475925	1065.647663	15.285671
22.283480	1072.819233	15.290688
22.550329	1066.381065	15.295706
22.814156	1062.994993	15.300723
22.689758	1069.584774	15.305741
22.602223	1068.064815	15.310759
22.735943	1063.701779	15.315776
22.580268	1064.660236	15.320794
22.258083	1067.768447	15.325811
22.347209	1080.989962	15.330829
22.644676	1078.722102	15.335847
22.536025	1085.236855	15.340864
22.671702	1081.447859	15.345882
22.728287	1086.863925	15.350899
22.820564	1087.158937	15.355917
22.670941	1087.554726	15.360935
22.634106	1090.864663	15.365952
22.828097	1082.449700	15.370970
22.619715	1093.707322	15.375987
22.466230	1104.606114	15.381005
23.132236	1106.515914	15.386023
22.821614	1114.068814	15.391040
23.189628	1109.640886	15.396058
23.415056	1112.092649	15.401075
23.406340	1108.752157	15.406093
23.327847	1122.066072	15.411111
23.287084	1103.093721	15.416128
23.451911	1097.861152	15.421146
22.960747	1088.602975	15.426163
23.042595	1088.593501	15.431181
23.368459	1099.427124	15.436199
23.389785	1109.317257	15.441216
23.491529	1105.637679	15.446234
23.324199	1097.203226	15.451251
23.317918	1088.566980	15.456269
22.956360	1092.189404	15.461287
23.240302	1103.291485	15.466304
23.784776	1097.551687	15.471322
23.439449	1117.657335	15.476339
23.477611	1112.684321	15.481357
23.592410	1099.566957	15.486375
23.733156	1105.307593	15.491392
23.415681	1087.877332	15.496410
23.652423	1093.991177	15.501427
23.650168	1102.310250	15.506445
23.448883	1096.165862	15.511463
23.478133	1094.697144	15.516480
23.660341	1098.948111	15.521498
23.789218	1107.691733	15.526515
24.041380	1106.693231	15.531533
23.609516	1089.549019	15.536551
23.224384	1095.005460	15.541568
23.856891	1107.274556	15.546586
23.645455	1104.760882	15.551603
23.494358	1117.508591	15.556621
23.646480	1115.244422	15.561639
23.611909	1115.735906	15.566656
23.362555	1113.606828	15.571674
23.498724	1119.736341	15.576691
23.500551	1116.899130	15.581709
23.499866	1118.016494	15.586727
22.976987	1122.812743	15.591744
23.775848	1129.826837	15.596762
24.164437	1134.695770	15.601779
23.798183	1138.943778	15.606797
23.753625	1140.812737	15.611815
24.029998	1143.332311	15.616832
23.923262	1142.380220	15.621850
23.968582	1141.473881	15.626867
23.929437	1142.136490	15.631885
24.220739	1135.744983	15.636903
24.062898	1136.331400	15.641920
24.408921	1130.575153	15.646938
24.083548	1134.494906	15.651955
23.880096	1146.364014	15.656973
23.873817	1152.686129	15.661991
24.111258	1161.677959	15.667008
24.257685	1168.667420	15.672026
24.368131	1160.836624	15.677043
24.483792	1159.464899	15.682061
24.649123	1154.295351	15.687079
24.335815	1162.299966	15.692096
24.722029	1161.659284	15.697114
24.764719	1166.654663	15.702131
24.577008	1170.338398	15.707149
24.830191	1158.108310	15.712167
24.708520	1147.697518	15.717184
24.580292	1143.561437	15.722202
24.347120	1134.714344	15.727219
24.349306	1137.144065	15.732237
24.774543	1146.520055	15.737255
24.749946	1162.545888	15.742272
24.515744	1144.430426	15.747290
24.216153	1150.009263	15.752307
24.301386	1159.050036	15.757325
24.627835	1156.746096	15.762343
24.607203	1157.787673	15.767360
24.558550	1158.016267	15.772378
24.789931	1160.107351	15.777395
24.783250	1156.545629	15.782413
24.853266	1156.689474	15.787431
24.875671	1155.231285	15.792448
24.903858	1160.162649	15.797466
24.950868	1161.433534	15.802483
24.789021	1167.678891	15.807501
25.046606	1159.897769	15.812519
24.658350	1158.771759	15.817536
24.731608	1165.258219	15.822554
25.225066	1169.006310	15.827571
25.203517	1177.224280	15.832589
24.898288	1169.281475	15.837607
25.174857	1178.466036	15.842624
25.144063	1182.731252	15.847642
25.317059	1182.966361	15.852659
25.004039	1176.713111	15.857677
25.558479	1178.621355	15.862695
25.166028	1173.273559	15.867712
25.073163	1169.586399	15.872730
24.976453	1176.156130	15.877747
25.223892	1180.330689	15.882765
25.637253	1186.319238	15.887783
25.465002	1188.577310	15.892800
25.529098	1188.807284	15.897818
25.598108	1190.750084	15.902835
25.372325	1178.452545	15.907853
25.414710	1165.674609	15.912871
25.048567	1179.528809	15.917888
25.337865	1187.193461	15.922906
25.706513	1184.497941	15.927923
25.486135	1187.252653	15.932941
25.476272	1186.206582	15.937959
25.489096	1186.169985	15.942976
25.488431	1189.811978	15.947994
25.689860	1188.114475	15.953011
25.225442	1178.359785	15.958029
25.487880	1188.019918	15.963047
25.775155	1195.457672	15.968064
25.687065	1193.120440	15.973082
25.782352	1193.168833	15.978099
25.440012	1183.354108	15.983117
25.625647	1184.388818	15.988135
25.698687	1188.959759	15.993152
25.640662	1197.884002	15.998170
26.253997	1213.034234	16.003187
26.186939	1207.534781	16.008205
25.993945	1193.780464	16.013223
25.793895	1194.139926	16.018240
25.497129	1193.637138	16.023258
26.279437	1200.647527	16.028275
25.974285	1213.495029	16.033293
26.114726	1210.014531	16.038311
26.055974	1216.761403	16.043328
25.807125	1208.913944	16.048346
26.283070	1204.942555	16.053363
25.953122	1205.183388	16.058381
26.210567	1213.929134	16.063399
25.895449	1205.457680	16.068416
25.892742	1204.419961	16.073434
26.348158	1207.309297	16.078451
26.132607	1212.805642	16.083469
26.363960	1196.788824	16.088487
26.655147	1209.016459	16.093504
26.434959	1210.534076	16.098522
26.286029	1201.629652	16.103539
26.661793	1212.493444	16.108557
26.450360	1205.265007	16.113575
26.358153	1208.596211	16.118592
26.491695	1211.649271	16.123610
26.496543	1205.974521	16.128627
26.429245	1206.941316	16.133645
26.497973	1215.006393	16.138663
26.569378	1219.214681	16.143680
26.294337	1207.107828	16.148698
26.773676	1211.101122	16.153715
26.714175	1216.137672	16.158733
26.663578	1217.259657	16.163751
26.324903	1225.760553	16.168768
26.576104	1230.751888	16.173786
26.991453	1224.006522	16.178803
27.201610	1237.771040	16.183821
26.998112	1221.938669	16.188839
26.917778	1219.480306	16.193856
26.697986	1216.144256	16.198874
27.507630	1208.034164	16.203891
27.101916	1210.180266	16.208909
26.782672	1204.827375	16.213927
26.774812	1194.644987	16.218944
26.532791	1199.217648	16.223962
27.018381	1222.128924	16.228979
27.080648	1226.231339	16.233997
27.230192	1230.837716	16.239015
27.173476	1225.175702	16.244032
27.186698	1228.402132	16.249050
27.119279	1224.266031	16.254067
27.040474	1222.170346	16.259085
26.931373	1228.511653	16.264103
27.103875	1227.598130	16.269120
27.122663	1238.504895	16.274138
26.889264	1220.916247	16.279155
27.222823	1228.769685	16.284173
27.229083	1229.463098	16.289191
27.316134	1224.394079	16.294208
26.962956	1230.265306	16.299226
27.301440	1225.062466	16.304243
27.515272	1242.379837	16.309261
27.508870	1233.342754	16.314279
27.516498	1238.141642	16.319296
27.483682	1258.634290	16.324314
27.488718	1250.447483	16.329331
27.744910	1254.008472	16.334349
27.764755	1246.128629	16.339367
27.457559	1240.401467	16.344384
27.770030	1244.692147	16.349402
27.331894	1253.113868	16.354419
27.364563	1252.073794	16.359437
27.333085	1258.134783	16.364455
27.761060	1244.949617	16.369472
27.336508	1256.127390	16.374490
27.472153	1254.973453	16.379507
27.707834	1255.097817	16.384525
27.679033	1262.644771	16.389543
28.160028	1275.944273	16.394560
28.036494	1273.530499	16.399578
28.086165	1257.510355	16.404595
27.927442	1250.450418	16.409613
27.992039	1253.312248	16.414631
28.177247	1254.990812	16.419648
28.326981	1261.358102	16.424666
28.125882	1249.059827	16.429683
28.009012	1243.151553	16.434701
28.095922	1248.626063	16.439719
28.318535	1249.238455	16.444736
28.031195	1258.517167	16.449754
28.066327	1261.102721	16.454771
28.258893	1270.508691	16.459789
28.396436	1272.188366	16.464807
28.273313	1268.095642	16.469824
28.183009	1269.331110	16.474842
28.196004	1263.822331	16.479859
27.878922	1274.661491	16.484877
27.602678	1269.017863	16.489895
28.222497	1272.493838	16.494912
28.447786	1275.021385	16.499930
28.484221	1278.420935	16.504947
28.911396	1282.870490	16.509965
28.153699	1272.280942	16.514983
28.397344	1275.929095	16.520000
28.123551	1297.443917	16.525018
28.513512	1298.516249	16.530035
28.793966	1301.650593	16.535053
28.770400	1290.817344	16.540071
29.323110	1288.301434	16.545088
29.169685	1295.009427	16.550106
28.939991	1290.737631	16.555123
28.669360	1272.583528	16.560141
28.787940	1278.842067	16.565159
28.953483	1287.576912	16.570176
29.209082	1294.038184	16.575194
28.962350	1282.804185	16.580211
28.576529	1273.586315	16.585229
28.738599	1286.487356	16.590247
29.046078	1289.008420	16.595264
28.761888	1287.070937	16.600282
29.171783	1297.440317	16.605299
29.163611	1288.308808	16.610317
29.010323	1290.040077	16.615335
28.960864	1289.741778	16.620352
28.998524	1301.377789	16.625370
28.996048	1297.099017	16.630387
29.497050	1290.696896	16.635405
29.123409	1291.102322	16.640423
29.093895	1292.808009	16.645440
29.070335	1294.361290	16.650458
29.108973	1297.201923	16.655475
29.304094	1297.010711	16.660493
28.831850	1294.556552	16.665511
28.950394	1298.751207	16.670528
29.436380	1319.387212	16.675546
29.379743	1312.708987	16.680563
29.853634	1322.055404	16.685581
29.487262	1330.794192	16.690599
29.720586	1317.894900	16.695616
29.535714	1322.944688	16.700634
29.267371	1318.593696	16.705651
29.524167	1317.960536	16.710669
29.243434	1315.091548	16.715687
29.516300	1322.288601	16.720704
29.575898	1334.082164	16.725722
29.385459	1322.265018	16.730739
29.801884	1328.767535	16.735757
29.992857	1343.500800	16.740775
30.084595	1339.750148	16.745792
29.667008	1332.070918	16.750810
29.942503	1337.004852	16.755827
30.204798	1335.206340	16.760845
29.531009	1340.827718	16.765863
29.706543	1341.125550	16.770880
30.029803	1342.653240	16.775898
30.178119	1339.887860	16.780915
30.304023	1349.029695	16.785933
29.974940	1345.814779	16.790951
30.082846	1350.553902	16.795968
29.845008	1351.667179	16.800986
30.120016	1341.115617	16.806003
30.262647	1343.308904	16.811021
30.048368	1339.839428	16.816039
30.195216	1337.446663	16.821056
30.122145	1332.427791	16.826074
30.256191	1337.683550	16.831091
30.552843	1338.565285	16.836109
30.233566	1339.249426	16.841127
30.396306	1333.714155	16.846144
30.121505	1346.339276	16.851162
30.527399	1358.517597	16.856179
30.364647	1366.135943	16.861197
30.405046	1359.256399	16.866215
30.547711	1361.809446	16.871232
30.882952	1367.381028	16.876250
30.518680	1373.837855	16.881267
30.894009	1369.983083	16.886285
30.752175	1371.248671	16.891303
31.015361	1367.029506	16.896320
30.872514	1361.557584	16.901338
30.849252	1366.146720	16.906355
31.078058	1361.219694	16.911373
30.626724	1355.836830	16.916391
31.113021	1351.279973	16.921408
30.565364	1358.352327	16.926426
30.174940	1364.746951	16.931443
30.830784	1369.504909	16.936461
30.663258	1374.914931	16.941479
30.796812	1364.483210	16.946496
30.879628	1367.032952	16.951514
30.833636	1361.508080	16.956531
30.820410	1358.209270	16.961549
30.758131	1376.709011	16.966567
30.952974	1386.269322	16.971584
31.466277	1398.667634	16.976602
31.354958	1401.102439	16.981619
31.794765	1388.852605	16.986637
31.254633	1395.406248	16.991655
31.385993	1392.782356	16.996672
31.466456	1387.427138	17.001690
31.494780	1393.797599	17.006707
31.322680	1390.826478	17.011725
31.481684	1389.773038	17.016743
31.717887	1385.015268	17.021760
31.665382	1390.378983	17.026778
31.470371	1381.715175	17.031795
31.819896	1366.629708	17.036813
31.389707	1376.454588	17.041831
31.598105	1376.860913	17.046848
31.748420	1383.995021	17.051866
31.790769	1384.329369	17.056883
31.961233	1378.739233	17.061901
31.704256	1385.636952	17.066919
31.681910	1384.119440	17.071936
31.653003	1382.685000	17.076954
31.459413	1389.563384	17.081971
31.826883	1381.765058	17.086989
31.593643	1388.428707	17.092007
31.758296	1385.695491	17.097024
32.118497	1381.962993	17.102042
31.640295	1379.440321	17.107059
31.850958	1376.598957	17.112077
31.724654	1383.782445	17.117095
31.966995	1382.353110	17.122112
32.453228	1395.030190	17.127130
32.127832	1395.336588	17.132147
32.243259	1384.607874	17.137165
31.949717	1391.530223	17.142183
31.587416	1401.309833	17.147200
32.088116	1404.075386	17.152218
32.330173	1404.924598	17.157235
32.454695	1395.245352	17.162253
32.044774	1396.164516	17.167271
32.263336	1407.879728	17.172288
31.974766	1407.211555	17.177306
32.120645	1408.467064	17.182323
32.350761	1414.389546	17.187341
32.422055	1419.036558	17.192359
32.621620	1427.920810	17.197376
32.646551	1433.168340	17.202394
32.564174	1427.737476	17.207411
32.878450	1425.012516	17.212429
32.785310	1423.793203	17.217447
32.691915	1425.647705	17.222464
32.957396	1431.807685	17.227482
32.743648	1431.332990	17.232499
32.985050	1417.889566	17.237517
32.828899	1426.838668	17.242535
32.784654	1421.452363	17.247552
32.903489	1418.016214	17.252570
32.807500	1425.914527	17.257587
33.322740	1426.752766	17.262605
32.942077	1419.597927	17.267623
33.004761	1425.221431	17.272640
33.133304	1420.111183	17.277658
33.121533	1424.376651	17.282675
33.067398	1415.043948	17.287693
33.009203	1427.297728	17.292711
32.983869	1423.205522	17.297728
32.965801	1420.614360	17.302746
32.776081	1436.849186	17.307763
33.100421	1426.608632	17.312781
33.088217	1433.663921	17.317799
33.409211	1435.889410	17.322816
33.120178	1435.928213	17.327834
33.135239	1452.364701	17.332851
33.630139	1462.036128	17.337869
33.659395	1455.000491	17.342887
33.484942	1464.640433	17.347904
33.557303	1454.757835	17.352922
33.463755	1459.484171	17.357939
33.676479	1451.883478	17.362957
33.586574	1450.392258	17.367975
33.460555	1455.720101	17.372992
33.626522	1458.698727	17.378010
33.876474	1450.603085	17.383027
33.669632	1444.863388	17.388045
33.739009	1453.133600	17.393063
33.670645	1451.310820	17.398080
34.414459	1449.446794	17.403098
33.669002	1450.030035	17.408115
33.925975	1449.908087	17.413133
34.009071	1440.358343	17.418151
34.003318	1451.613044	17.423168
33.964556	1448.299258	17.428186
33.917878	1448.846286	17.433203
33.880877	1454.409580	17.438221
33.942460	1455.608789	17.443239
33.808244	1459.161176	17.448256
34.097075	1469.710454	17.453274
33.896351	1475.034156	17.458291
34.143232	1464.101889	17.463309
34.225420	1466.629652	17.468327
34.137194	1472.039980	17.473344
34.651852	1465.926007	17.478362
34.039926	1473.904670	17.483379
34.378660	1478.487967	17.488397
34.485944	1479.130947	17.493415
34.589065	1469.505486	17.498432
34.687034	1466.334511	17.503450
34.269129	1470.814703	17.508467
34.774878	1463.922627	17.513485
34.734913	1471.351486	17.518503
34.734088	1474.245629	17.523520
34.670312	1472.008717	17.528538
34.768784	1473.817572	17.533555
34.903287	1490.349109	17.538573
35.047629	1472.240647	17.543591
34.705379	1470.763468	17.548608
34.844733	1469.896121	17.553626
34.812418	1486.393666	17.558643
35.039147	1492.682779	17.563661
34.896952	1503.213978	17.568679
34.894296	1499.294951	17.573696
34.736221	1493.705438	17.578714
34.881641	1495.030453	17.583731
35.021740	1500.796564	17.588749
35.107680	1504.156891	17.593767
34.794577	1502.312248	17.598784
35.109326	1495.443587	17.603802
35.099969	1500.011657	17.608819
35.251303	1484.376274	17.613837
35.128797	1501.487485	17.618855
35.182053	1497.966856	17.623872
35.203896	1484.380839	17.628890
35.039177	1502.552673	17.633907
35.347804	1518.189270	17.638925
35.554381	1518.185623	17.643943
35.463878	1518.957230	17.648960
35.721170	1515.209168	17.653978
35.506737	1518.234407	17.658995
35.359194	1512.315040	17.664013
35.348488	1519.793012	17.669031
35.417353	1529.729626	17.674048
35.709290	1521.674752	17.679066
35.689445	1520.497670	17.684083
35.716241	1511.114446	17.689101
35.924081	1517.135106	17.694119
35.630501	1516.215240	17.699136
36.031206	1515.922589	17.704154
36.224239	1528.901038	17.709171
36.018479	1530.612097	17.714189
35.879490	1523.186057	17.719207
36.287797	1539.968503	17.724224
36.147477	1526.653858	17.729242
36.128031	1523.826207	17.734259
35.954389	1532.481436	17.739277
36.099952	1525.825299	17.744295
36.330421	1534.471261	17.749312
36.326379	1545.081962	17.754330
36.242501	1539.228414	17.759347
36.071825	1540.668920	17.764365
36.050931	1543.301108	17.769383
35.888208	1544.225973	17.774400
36.260527	1534.656395	17.779418
36.399519	1539.646353	17.784435
35.966918	1543.800643	17.789453
36.218995	1548.561554	17.794471
36.805968	1561.993096	17.799488
36.502158	1565.070128	17.804506
36.945144	1559.737311	17.809523
36.833908	1566.063290	17.814541
37.240381	1557.873801	17.819559
36.895422	1553.683005	17.824576
36.837565	1542.813916	17.829594
36.740795	1543.293005	17.834611
37.035129	1555.883311	17.839629
37.050630	1544.721929	17.844647
36.511892	1545.680092	17.849664
37.024705	1550.750708	17.854682
36.942636	1551.539938	17.859699
36.535971	1560.250396	17.864717
36.937404	1551.878655	17.869735
36.751735	1565.348444	17.874752
37.000454	1563.574114	17.879770
37.369810	1558.438957	17.884787
37.354232	1552.789368	17.889805
37.409755	1553.926410	17.894823
36.991084	1559.072628	17.899840
37.043058	1554.911550	17.904858
37.215577	1557.617769	17.909875
36.921802	1565.632146	17.914893
37.320549	1578.666966	17.919911
37.055904	1580.579705	17.924928
36.851805	1587.302009	17.929946
37.064443	1585.653217	17.934963
36.948737	1590.016959	17.939981
37.388685	1598.030724	17.944999
37.351180	1611.865649	17.950016
37.909986	1602.977068	17.955034
37.961696	1606.610991	17.960051
37.924309	1608.668234	17.965069
37.898125	1602.641578	17.970087
37.993326	1605.224141	17.975104
37.812191	1607.701403	17.980122
38.155789	1607.057874	17.985139
37.954340	1611.684283	17.990157
38.187802	1599.384380	17.995175
37.811253	1602.794642	18.000192
37.928340	1600.936660	18.005210
37.979996	1606.602965	18.010227
37.625032	1610.663130	18.015245
37.959045	1601.399287	18.020263
37.953451	1613.831201	18.025280
38.222769	1598.010088	18.030298
37.882248	1612.513896	18.035315
38.392601	1624.436290	18.040333
38.641312	1625.246607	18.045351
38.591723	1639.736699	18.050368
38.257550	1630.002508	18.055386
38.662112	1636.756298	18.060403
38.796254	1635.204932	18.065421
38.641308	1625.060979	18.070439
38.609677	1615.604745	18.075456
38.620052	1622.176902	18.080474
38.799148	1622.205936	18.085491
38.403441	1629.728118	18.090509
38.686973	1626.307314	18.095527
38.864699	1631.856166	18.100544
38.902964	1637.369928	18.105562
38.674765	1630.727763	18.110579
38.790553	1636.384092	18.115597
38.736415	1624.703317	18.120615
38.604738	1632.575719	18.125632
38.385505	1626.598047	18.130650
38.869081	1635.857913	18.135667
38.797570	1637.974122	18.140685
39.064984	1650.117398	18.145703
39.108853	1664.517218	18.150720
39.303870	1657.073833	18.155738
39.483403	1659.223543	18.160755
39.407782	1656.092186	18.165773
39.484969	1652.378449	18.170791
39.453369	1653.121955	18.175808
39.243336	1656.531548	18.180826
39.327669	1658.620339	18.185843
39.130846	1667.033085	18.190861
39.604286	1664.078178	18.195879
39.699624	1657.836918	18.200896
39.603210	1656.318291	18.205914
39.749101	1654.998629	18.210931
39.419447	1658.022895	18.215949
39.484885	1655.365047	18.220967
39.742921	1665.531064	18.225984
39.429273	1662.622962	18.231002
39.525518	1645.591654	18.236019
39.366785	1665.252289	18.241037
39.709055	1666.628722	18.246055
39.790852	1681.698007	18.251072
39.750107	1687.905754	18.256090
40.098386	1679.617971	18.261107
39.906821	1685.208557	18.266125
40.069515	1686.193219	18.271143
39.623519	1682.917547	18.276160
39.752044	1688.325751	18.281178
40.206460	1676.180746	18.286195
39.864389	1685.868996	18.291213
40.257144	1688.241138	18.296231
40.359668	1700.548979	18.301248
40.442062	1708.227134	18.306266
40.689831	1697.673292	18.311283
40.158833	1697.667715	18.316301
40.512453	1703.066124	18.321319
40.484580	1702.341570	18.326336
40.324058	1702.918955	18.331354
40.486799	1698.466037	18.336371
40.383449	1699.703565	18.341389
40.724134	1699.764247	18.346407
40.558501	1700.089957	18.351424
40.480105	1699.515283	18.356442
40.693761	1696.692338	18.361459
40.498994	1705.906374	18.366477
40.719724	1699.626642	18.371495
40.928360	1707.487118	18.376512
40.616265	1714.081113	18.381530
41.031496	1723.020299	18.386547
40.892436	1728.555386	18.391565
40.920016	1727.866379	18.396583
41.080312	1723.388588	18.401600
41.033860	1729.038648	18.406618
41.040869	1721.823329	18.411635
40.915429	1731.326392	18.416653
41.053444	1726.094659	18.421671
41.040236	1721.262021	18.426688
40.994547	1736.073483	18.431706
41.111059	1743.919916	18.436723
41.160834	1756.983952	18.441741
41.522762	1748.763441	18.446759
41.534538	1756.168583	18.451776
41.315611	1755.985026	18.456794
41.711322	1752.452056	18.461811
41.335654	1756.436580	18.466829
41.802350	1752.015221	18.471847
41.764857	1748.511829	18.476864
41.492193	1753.196701	18.481882
41.752441	1749.110451	18.486899
41.449099	1760.856660	18.491917
41.566804	1767.812957	18.496935
42.078627	1769.974062	18.501952
42.005494	1773.835745	18.506970
42.026965	1772.324001	18.511987
41.901162	1772.078607	18.517005
42.067298	1781.148126	18.522023
42.083773	1769.535160	18.527040
41.783726	1773.192325	18.532058
42.282214	1759.699150	18.537075
42.059619	1774.973700	18.542093
42.189033	1760.436582	18.547111
42.264370	1769.618065	18.552128
42.172907	1775.082638	18.557146
42.503256	1766.964868	18.562163
42.374395	1787.798133	18.567181
42.563519	1794.071116	18.572199
42.698407	1788.682056	18.577216
42.378785	1794.718660	18.582234
42.597963	1796.890617	18.587251
42.454080	1797.320243	18.592269
42.434659	1795.079540	18.597287
42.277554	1791.171873	18.602304
42.585199	1795.756937	18.607322
42.521016	1797.748944	18.612339
42.540015	1802.893361	18.617357
43.010114	1801.504275	18.622375
42.871502	1805.073194	18.627392
42.983799	1818.357921	18.632410
43.256000	1814.099377	18.637427
43.495714	1814.317796	18.642445
43.316551	1804.076523	18.647463
43.243865	1795.712213	18.652480
43.181010	1798.470895	18.657498
43.000445	1791.246881	18.662515
43.054315	1799.967806	18.667533
43.414800	1811.528639	18.672551
43.635470	1812.213940	18.677568
43.105988	1815.572311	18.682586
43.695255	1818.687068	18.687603
43.469840	1825.703122	18.692621
43.626212	1821.809759	18.697639
43.542178	1820.964552	18.702656
43.265139	1823.280045	18.707674
43.429910	1817.122597	18.712691
43.472837	1816.522719	18.717709
43.323610	1821.866908	18.722727
43.835314	1813.373732	18.727744
43.738579	1822.967052	18.732762
44.020317	1827.852812	18.737779
44.269175	1817.267171	18.742797
43.566464	1822.918448	18.747815
44.145959	1821.853165	18.752832
44.025045	1832.349685	18.757850
44.304500	1830.898758	18.762867
44.237034	1834.327214	18.767885
44.128797	1843.196479	18.772903
44.235110	1836.814589	18.777920
44.056731	1850.867299	18.782938
44.370246	1840.296825	18.787955
44.159279	1844.280972	18.792973
44.029982	1843.326043	18.797991
44.624666	1845.660455	18.803008
44.269507	1843.459396	18.808026
44.025056	1834.036181	18.813043
44.354749	1840.703874	18.818061
44.287379	1852.489144	18.823079
44.302636	1859.344659	18.828096
44.284527	1864.100383	18.833114
44.419209	1859.339360	18.838131
44.655677	1864.771838	18.843149
44.931578	1877.059118	18.848167
44.961606	1862.281763	18.853184
45.067492	1864.878480	18.858202
45.088685	1866.917164	18.863219
44.850124	1865.805671	18.868237
44.993079	1872.073246	18.873255
45.210467	1874.624200	18.878272
45.164231	1872.144658	18.883290
45.490067	1873.277505	18.888307
45.241429	1867.948135	18.893325
45.384924	1877.627162	18.898343
44.951651	1872.610569	18.903360
45.356891	1884.663115	18.908378
45.630604	1882.944826	18.913395
45.484215	1886.028962	18.918413
45.432583	1888.997357	18.923431
45.708632	1881.752708	18.928448
45.399963	1887.251133	18.933466
45.643172	1881.769439	18.938483
45.556494	1885.355535	18.943501
45.209652	1890.244502	18.948519
45.652471	1888.278970	18.953536
45.209156	1896.076927	18.958554
45.421769	1890.006683	18.963571
45.723318	1905.723619	18.968589
45.773823	1909.635512	18.973607
45.887794	1920.003991	18.978624
45.785448	1921.364459	18.983642
45.973592	1916.137489	18.988659
46.013718	1916.008274	18.993677
46.132480	1914.232053	18.998695
46.259558	1913.350817	19.003712
46.163393	1919.450504	19.008730
45.811086	1915.601605	19.013747
46.006206	1921.431871	19.018765
46.452875	1940.414706	19.023783
47.024350	1933.174535	19.028800
46.727893	1933.697349	19.033818
46.691931	1926.703240	19.038835
46.705077	1908.709442	19.043853
46.501529	1911.745676	19.048871
46.722847	1912.209965	19.053888
46.515476	1929.091792	19.058906
46.515205	1936.435765	19.063923
47.021140	1937.572135	19.068941
46.732241	1930.462766	19.073959
46.928018	1928.996456	19.078976
46.900937	1927.539597	19.083994
46.992913	1939.360077	19.089011
47.127655	1936.192762	19.094029
46.724586	1931.468106	19.099047
46.838239	1928.793243	19.104064
46.919913	1935.139812	19.109082
46.669407	1935.254670	19.114099
47.086774	1947.002402	19.119117
47.061831	1957.730215	19.124135
47.384427	1957.437096	19.129152
47.619408	1958.154889	19.134170
47.336665	1956.901941	19.139187
47.294792	1941.848526	19.144205
47.387001	1965.816121	19.149223
47.714505	1948.653841	19.154240
47.897375	1959.964704	19.159258
47.623080	1953.998651	19.164275
47.849349	1951.618687	19.169293
47.740795	1957.057573	19.174311
47.644517	1950.555701	19.179328
47.771155	1956.541813	19.184346
47.468023	1971.481919	19.189363
48.009116	1967.935739	19.194381
47.871214	1984.825738	19.199399
48.068368	1978.256079	19.204416
48.106719	1971.632249	19.209434
47.742169	1973.450126	19.214451
48.051679	1973.253722	19.219469
47.962948	1984.149278	19.224487
48.098359	1983.920018	19.229504
48.151721	1980.834796	19.234522
47.959183	1989.852963	19.239539
48.346590	1998.250645	19.244557
48.191212	2004.132353	19.249575
48.673048	2002.814011	19.254592
48.434876	2003.053186	19.259610
48.352646	2006.932116	19.264627
48.818638	2000.746642	19.269645
48.622059	2005.018930	19.274663
48.796633	2003.634814	19.279680
48.629059	2003.979766	19.284698
48.734509	2013.866770	19.289715
48.961479	2016.286860	19.294733
48.729737	2036.158093	19.299751
48.617562	2032.375926	19.304768
48.916716	2035.150868	19.309786
48.961157	2036.441152	19.314803
49.255916	2030.477996	19.319821
49.419016	2041.782521	19.324839
49.307138	2034.200562	19.329856
49.351952	2039.233726	19.334874
48.981761	2035.655839	19.339891
49.472252	2037.978096	19.344909
48.973959	2035.789830	19.349927
48.900568	2038.237752	19.354944
49.706956	2052.860005	19.359962
49.331467	2057.952302	19.364979
49.580486	2060.097554	19.369997
49.617796	2058.763208	19.375015
49.762827	2059.605468	19.380032
49.855972	2052.203028	19.385050
49.874978	2059.471464	19.390067
49.670595	2061.605254	19.395085
49.684304	2058.945932	19.400103
49.932976	2055.801885	19.405120
49.764074	2056.235412	19.410138
49.394007	2055.185409	19.415155
49.818258	2068.570082	19.420173
49.849875	2079.689966	19.425191
50.014887	2073.917417	19.430208
50.269870	2078.034207	19.435226
50.418372	2077.919677	19.440243
50.348942	2078.217791	19.445261
50.485543	2084.590576	19.450279
50.588807	2075.334012	19.455296
50.152468	2083.052066	19.460314
50.103061	2086.058018	19.465331
50.839313	2092.817147	19.470349
50.794392	2102.026991	19.475367
50.869298	2103.101088	19.480384
50.804134	2107.690626	19.485402
50.741223	2109.272196	19.490419
50.913350	2099.960715	19.495437
50.894287	2101.705878	19.500455
50.909393	2098.819105	19.505472
51.165403	2093.827681	19.510490
51.093037	2100.210915	19.515507
51.170572	2091.535887	19.520525
51.090597	2113.349730	19.525543
51.318601	2107.507400	19.530560
51.287159	2106.007022	19.535578
51.242006	2112.048338	19.540595
51.376274	2101.925360	19.545613
51.348903	2107.032900	19.550631
50.982922	2104.218084	19.555648
51.384649	2108.144767	19.560666
51.404061	2125.931942	19.565683
51.756402	2121.746059	19.570701
51.659675	2118.703118	19.575719
51.677414	2123.589035	19.580736
52.002517	2127.278333	19.585754
51.706745	2122.353875	19.590771
51.832684	2121.621136	19.595789
51.986975	2125.109799	19.600807
52.058364	2125.307090	19.605824
52.088059	2120.817976	19.610842
51.862625	2131.274137	19.615859
51.966235	2127.953838	19.620877
52.041467	2119.610530	19.625895
51.850847	2122.433337	19.630912
52.203363	2123.243296	19.635930
52.107367	2140.114292	19.640947
52.221447	2138.944722	19.645965
52.046251	2141.913460	19.650983
51.719552	2146.256536	19.656000
52.292292	2139.937625	19.661018
52.233499	2153.804687	19.666035
52.261940	2158.023041	19.671053
52.728101	2161.138091	19.676071
52.567905	2163.394408	19.681088
52.609694	2156.523810	19.686106
52.552590	2166.369931	19.691123
52.818545	2158.596542	19.696141
52.659384	2175.669920	19.701159
52.453660	2176.847677	19.706176
53.019986	2193.836521	19.711194
52.826213	2200.822547	19.716211
53.001239	2199.185868	19.721229
53.028705	2197.016715	19.726247
53.035629	2197.025218	19.731264
53.305275	2188.926177	19.736282
53.117604	2193.970334	19.741299
53.496629	2204.616463	19.746317
53.865205	2216.495052	19.751335
53.671673	2206.325217	19.756352
53.779054	2200.810922	19.761370
53.018855	2202.295927	19.766387
53.587194	2209.276913	19.771405
53.561330	2211.155697	19.776423
53.487085	2221.080260	19.781440
53.549575	2224.112997	19.786458
53.485178	2232.297095	19.791475
53.330336	2229.616651	19.796493
54.159966	2231.996591	19.801511
54.285969	2243.111349	19.806528
54.067132	2245.496733	19.811546
54.081111	2261.325030	19.816563
54.145120	2242.934793	19.821581
54.189128	2247.658856	19.826599
54.351333	2246.011545	19.831616
54.547177	2237.371678	19.836634
54.363024	2245.426097	19.841651
54.519998	2251.675843	19.846669
54.250426	2244.367669	19.851687
54.047061	2255.786193	19.856704
54.743298	2267.784224	19.861722
54.333743	2269.801652	19.866739
54.716574	2269.849464	19.871757
54.857301	2276.098592	19.876775
54.737832	2279.844515	19.881792
55.003129	2270.398512	19.886810
54.990013	2274.787475	19.891827
54.988492	2264.322610	19.896845
54.980318	2272.292834	19.901863
55.004346	2285.124566	19.906880
55.121882	2279.182609	19.911898
54.896417	2277.721893	19.916915
55.337838	2281.588784	19.921933
55.352957	2289.577481	19.926951
55.501842	2295.547619	19.931968
55.872385	2300.078837	19.936986
55.659143	2297.044538	19.942003
55.487767	2297.711998	19.947021
55.635197	2294.406938	19.952039
55.669260	2304.055893	19.957056
55.787112	2292.565668	19.962074
55.968223	2303.135366	19.967091
55.797265	2296.338866	19.972109
55.922720	2299.144049	19.977127
55.925999	2289.341178	19.982144
56.188691	2295.157890	19.987162
55.944870	2304.111612	19.992179
56.233055	2301.696714	19.997197
56.366859	2298.065553	20.002215
55.993254	2302.356005	20.007232
56.002844	2297.888912	20.012250
56.179416	2303.425529	20.017267
56.073689	2301.917765	20.022285
56.290690	2296.288538	20.027303
56.151307	2301.378858	20.032320
56.407389	2316.995931	20.037338
56.428198	2321.086117	20.042355
56.553662	2326.226732	20.047373
56.454770	2313.185934	20.052391
56.219861	2323.981373	20.057408
56.308850	2319.552408	20.062426
56.891826	2333.408056	20.067443
56.775736	2341.934787	20.072461
56.833938	2343.071463	20.077479
56.924162	2340.662134	20.082496
56.884711	2335.937564	20.087514
57.484982	2319.909645	20.092531
57.536062	2320.110100	20.097549
57.800588	2311.787726	20.102567
57.764645	2316.508475	20.107584
57.635098	2311.971518	20.112602
57.700954	2317.253963	20.117619
58.011804	2315.905413	20.122637
58.319443	2310.931139	20.127655
57.669145	2301.441470	20.132672
57.728252	2297.989205	20.137690
57.991939	2285.359061	20.142707
57.855151	2296.801962	20.147725
57.734453	2293.806906	20.152743
57.750923	2302.514962	20.157760
57.739999	2310.428824	20.162778
58.122985	2316.378302	20.167795
57.903187	2319.824256	20.172813
58.054101	2315.966352	20.177831
58.020178	2315.791856	20.182848
57.990128	2320.483284	20.187866
57.835701	2324.660718	20.192883
57.904783	2327.553582	20.197901
58.434080	2338.037531	20.202919
58.041120	2354.734046	20.207936
58.290241	2348.790515	20.212954
58.476200	2353.514597	20.217971
58.436949	2350.955001	20.222989
58.878370	2343.507685	20.228007
58.205562	2357.442099	20.233024
58.488256	2363.025332	20.238042
58.948502	2373.510584	20.243059
59.048247	2373.652968	20.248077
59.381743	2367.421722	20.253095
58.786262	2381.050608	20.258112
59.021899	2373.000964	20.263130
58.994156	2379.920181	20.268147
58.602014	2373.814535	20.273165
59.070826	2383.843997	20.278183
59.029271	2392.520103	20.283200
59.059503	2395.295944	20.288218
59.464525	2401.645986	20.293235
59.073608	2400.785412	20.298253
59.185844	2406.303673	20.303271
59.473035	2411.444381	20.308288
59.469265	2415.311183	20.313306
59.880907	2423.601143	20.318323
59.724950	2432.332953	20.323341
59.977436	2425.650367	20.328359
59.593686	2427.982551	20.333376
60.127517	2431.759343	20.338394
60.187111	2434.817814	20.343411
59.888804	2431.304400	20.348429
59.955321	2428.851409	20.353447
59.892435	2429.735527	20.358464
59.678691	2427.910033	20.363482
59.917841	2434.857150	20.368499
59.973099	2453.639522	20.373517
60.363666	2455.339879	20.378535
60.216347	2451.711428	20.383552
60.016695	2445.645220	20.388570
60.290858	2461.452121	20.393587
60.337725	2474.570786	20.398605
60.993583	2477.798378	20.403623
61.047060	2477.054815	20.408640
60.664452	2472.396260	20.413658
60.834639	2472.114240	20.418675
60.974450	2473.579067	20.423693
61.075234	2467.797456	20.428711
61.213234	2470.105220	20.433728
61.125459	2472.022074	20.438746
61.351383	2468.654265	20.443763
61.140892	2469.084808	20.448781
61.177000	2470.799326	20.453799
61.098418	2496.233362	20.458816
61.517111	2493.207945	20.463834
61.606734	2495.425407	20.468851
61.763080	2496.101814	20.473869
62.133210	2492.506407	20.478887
61.819851	2491.299215	20.483904
61.878193	2497.501283	20.488922
62.211566	2492.380931	20.493939
61.936160	2491.802189	20.498957
61.956538	2492.054767	20.503975
61.757282	2497.804603	20.508992
61.728604	2496.758228	20.514010
62.093848	2493.526524	20.519027
62.140070	2506.654781	20.524045
62.509331	2506.079815	20.529063
62.098664	2507.081205	20.534080
62.391072	2514.411406	20.539098
62.323308	2508.586592	20.544115
62.461160	2524.020269	20.549133
62.706861	2521.933871	20.554151
62.496950	2517.993237	20.559168
62.687122	2517.080056	20.564186
62.505380	2514.523686	20.569203
62.266860	2516.921638	20.574221
62.612712	2525.966710	20.579239
63.002435	2524.662674	20.584256
62.798598	2538.931339	20.589274
62.926270	2535.600906	20.594291
62.895264	2540.494527	20.599309
63.005499	2541.253859	20.604327
63.114483	2545.156786	20.609344
63.180240	2542.943757	20.614362
63.587113	2556.511394	20.619379
63.379402	2568.479942	20.624397
63.800739	2560.177224	20.629415
63.294714	2569.313922	20.634432
63.532513	2565.717012	20.639450
63.835960	2556.959245	20.644467
63.943917	2568.048611	20.649485
63.993343	2559.589187	20.654503
63.998841	2559.670501	20.659520
63.771896	2557.086447	20.664538
63.947083	2555.361342	20.669555
63.686920	2555.076891	20.674573
64.035009	2560.293373	20.679591
64.188008	2559.117716	20.684608
63.748751	2554.865619	20.689626
64.057468	2564.216315	20.694643
64.518350	2580.726448	20.699661
64.367168	2579.471907	20.704679
64.357748	2583.522675	20.709696
64.493040	2590.609107	20.714714
64.885531	2585.700447	20.719731
64.946536	2578.883504	20.724749
64.703127	2577.583358	20.729767
64.802278	2572.294309	20.734784
64.432684	2578.149593	20.739802
64.739486	2571.878248	20.744819
64.737846	2580.892238	20.749837
64.800199	2592.114960	20.754855
64.902423	2593.292138	20.759872
64.442576	2603.065494	20.764890
65.328082	2600.043124	20.769907
64.996020	2609.935454	20.774925
65.296973	2620.707604	20.779943
65.698926	2620.821874	20.784960
65.654545	2628.946227	20.789978
65.985195	2623.084594	20.794995
65.814596	2627.526566	20.800013
65.855329	2633.033938	20.805031
66.043199	2629.034504	20.810048
65.854797	2631.667683	20.815066
65.866556	2623.075228	20.820083
65.932436	2633.019231	20.825101
66.124150	2635.441739	20.830119
66.022776	2628.637434	20.835136
66.111626	2631.763973	20.840154
66.206141	2630.401742	20.845171
66.083279	2632.794326	20.850189
66.078306	2636.715016	20.855207
66.442857	2645.788797	20.860224
66.223987	2649.711232	20.865242
66.523256	2655.304600	20.870259
66.551425	2654.725928	20.875277
66.663668	2660.452566	20.880295
66.789116	2650.245439	20.885312
66.318388	2662.103509	20.890330
66.659022	2661.716047	20.895347
66.490178	2670.342673	20.900365
66.936115	2679.769902	20.905383
67.077011	2688.266254	20.910400
67.063417	2681.208403	20.915418
67.413084	2685.847119	20.920435
67.434079	2686.790778	20.925453
67.064777	2685.854235	20.930471
67.411702	2684.219153	20.935488
67.276311	2696.274364	20.940506
67.720249	2703.931373	20.945523
67.357493	2701.658799	20.950541
67.507116	2703.604993	20.955559
67.716014	2698.387190	20.960576
67.579574	2704.843736	20.965594
67.749957	2707.386348	20.970611
67.833121	2719.536945	20.975629
67.727276	2729.154259	20.980647
67.841227	2725.907986	20.985664
68.051973	2726.187737	20.990682
68.228314	2728.360166	20.995699
67.995518	2724.640818	21.000717
68.190119	2718.727746	21.005735
68.324884	2727.515428	21.010752
68.011932	2739.371077	21.015770
68.460531	2740.273412	21.020787
68.514403	2752.854660	21.025805
68.581619	2758.203300	21.030823
68.794909	2748.907167	21.035840
68.944397	2752.409325	21.040858
69.124797	2749.458839	21.045875
69.303491	2751.204837	21.050893
68.926341	2752.914290	21.055911
69.209120	2751.731039	21.060928
69.095050	2755.990658	21.065946
69.342972	2749.264479	21.070963
69.410793	2754.900225	21.075981
68.938307	2752.944555	21.080999
69.322331	2760.711910	21.086016
69.347929	2780.670142	21.091034
69.455987	2764.197713	21.096051
69.478417	2771.891973	21.101069
69.381396	2773.908137	21.106087
69.807506	2763.354308	21.111104
69.639961	2784.983769	21.116122
69.509368	2794.923734	21.121139
70.025072	2786.906046	21.126157
70.033939	2793.933341	21.131175
70.410066	2788.209753	21.136192
70.367934	2797.605727	21.141210
70.251126	2796.222733	21.146227
70.476564	2793.849100	21.151245
70.349257	2788.235454	21.156263
70.271119	2788.187768	21.161280
70.352343	2798.019011	21.166298
70.500377	2806.782574	21.171315
70.571462	2824.063736	21.176333
70.779678	2823.210853	21.181351
70.793970	2820.242033	21.186368
70.763362	2820.060703	21.191386
71.007700	2819.438901	21.196403
70.921619	2819.029503	21.201421
70.520526	2827.998503	21.206439
71.343819	2831.013884	21.211456
71.182143	2843.041725	21.216474
71.311476	2831.268477	21.221491
71.284644	2847.693831	21.226509
71.289013	2848.750550	21.231527
71.676521	2831.174109	21.236544
71.360825	2837.816415	21.241562
71.394160	2850.211564	21.246579
71.564113	2855.118167	21.251597
71.241232	2864.586292	21.256615
71.955809	2868.464436	21.261632
71.807039	2873.493257	21.266650
72.016483	2867.192784	21.271667
71.866492	2863.331115	21.276685
72.224151	2881.293614	21.281703
72.649589	2879.150786	21.286720
72.488793	2883.430335	21.291738
72.653880	2881.608934	21.296755
72.651671	2893.043885	21.301773
72.810289	2883.421649	21.306791
72.914841	2880.378801	21.311808
73.054951	2879.552299	21.316826
73.032080	2880.572232	21.321843
73.016667	2865.605449	21.326861
72.773004	2866.505109	21.331879
72.905383	2862.324898	21.336896
72.760167	2873.071984	21.341914
72.565421	2872.559572	21.346931
73.056654	2878.438730	21.351949
72.612074	2884.577211	21.356967
72.807896	2881.576961	21.361984
73.167714	2904.633066	21.367002
72.840752	2905.154342	21.372019
73.137865	2906.954508	21.377037
73.405813	2904.444843	21.382055
73.386499	2916.308544	21.387072
73.485716	2921.371359	21.392090
73.591829	2929.103154	21.397107
73.577079	2927.136163	21.402125
73.467353	2929.116449	21.407143
73.689115	2937.095354	21.412160
73.811493	2941.375013	21.417178
73.699597	2959.025653	21.422195
74.459690	2952.279622	21.427213
74.018410	2946.254020	21.432231
74.402433	2959.601439	21.437248
74.360574	2974.223960	21.442266
74.505010	2981.211284	21.447283
74.915634	2985.187275	21.452301
74.759299	2985.243290	21.457319
74.980533	2981.453199	21.462336
74.846201	2982.187506	21.467354
74.914138	2983.534165	21.472371
75.037291	2980.491560	21.477389
75.088983	2979.050755	21.482407
75.355836	2974.887455	21.487424
75.207858	2981.106032	21.492442
75.241445	2971.405378	21.497459
75.472783	2985.890691	21.502477
75.080677	2999.314792	21.507495
75.102155	3004.853681	21.512512
75.396730	3006.606910	21.517530
75.146932	3004.162061	21.522547
75.606207	3013.249687	21.527565
75.607663	3024.409569	21.532583
75.625530	3021.774707	21.537600
75.527649	3028.285331	21.542618
75.620049	3028.810753	21.547635
75.812707	3033.426664	21.552653
76.105770	3049.537283	21.557671
76.408412	3049.698580	21.562688
76.475995	3052.396116	21.567706
76.874177	3047.271830	21.572723
77.061375	3051.263686	21.577741
76.711677	3052.132522	21.582759
77.071592	3052.559484	21.587776
76.992486	3043.539120	21.592794
76.973213	3044.845709	21.597811
76.845055	3041.993714	21.602829
76.932778	3052.729888	21.607847
76.761326	3048.167707	21.612864
76.982378	3040.470365	21.617882
76.891851	3048.090802	21.622899
76.881713	3053.148587	21.627917
77.193423	3073.873720	21.632935
77.362389	3070.716658	21.637952
77.373218	3071.040166	21.642970
77.221090	3077.644469	21.647987
77.369329	3078.312692	21.653005
77.639467	3104.573851	21.658023
77.574147	3092.568781	21.663040
77.883704	3099.214831	21.668058
77.758552	3105.316276	21.673075
78.091151	3101.158491	21.678093
78.238061	3099.781756	21.683111
77.871224	3109.266321	21.688128
78.238857	3106.236128	21.693146
78.100068	3111.175090	21.698163
78.210736	3121.134483	21.703181
78.363383	3124.105993	21.708199
78.420608	3126.353827	21.713216
78.755499	3120.178916	21.718234
78.518090	3128.223084	21.723251
78.525042	3124.115995	21.728269
78.350652	3127.349884	21.733287
78.731426	3136.310925	21.738304
79.094453	3145.489350	21.743322
78.788578	3150.852009	21.748339
79.109946	3144.357270	21.753357
79.377404	3142.201135	21.758375
79.369743	3150.856549	21.763392
79.340871	3143.138108	21.768410
79.356795	3161.494955	21.773427
79.480345	3173.914155	21.778445
79.713067	3175.165738	21.783463
80.055609	3169.087459	21.788480
80.010172	3167.772227	21.793498
79.651774	3180.683077	21.798515
79.986286	3164.793627	21.803533
79.768895	3169.789028	21.808551
79.763549	3166.116235	21.813568
80.069505	3179.330789	21.818586
79.848217	3194.044548	21.823603
80.091178	3190.853852	21.828621
80.235082	3196.133873	21.833639
80.231195	3196.172465	21.838656
80.494295	3205.514817	21.843674
80.063095	3220.778887	21.848691
80.698855	3219.225035	21.853709
80.471408	3224.231485	21.858727
80.774607	3241.252824	21.863744
81.246355	3243.382479	21.868762
81.205338	3257.386495	21.873779
81.305834	3242.581253	21.878797
81.461081	3249.121981	21.883815
81.887557	3253.711013	21.888832
81.683326	3241.575976	21.893850
81.405260	3252.460749	21.898867
81.566501	3241.455521	21.903885
81.957303	3242.133328	21.908903
81.618444	3242.684871	21.913920
81.642556	3244.451828	21.918938
81.623653	3242.236114	21.923955
81.824984	3253.466015	21.928973
82.324139	3258.943236	21.933991
82.317073	3268.330840	21.939008
82.001197	3264.823152	21.944026
82.195117	3269.921818	21.949043
82.310820	3263.402247	21.954061
82.244119	3263.775702	21.959079
82.130070	3265.627296	21.964096
82.516584	3269.963750	21.969114
82.514233	3288.096328	21.974131
82.491161	3297.426473	21.979149
82.639151	3296.033773	21.984167
82.646252	3290.560008	21.989184
83.123167	3302.034243	21.994202
83.129296	3311.546062	21.999219
83.362851	3307.933885	22.004237
83.457427	3310.529416	22.009255
83.689564	3319.374820	22.014272
83.248182	3319.497308	22.019290
83.281822	3318.886202	22.024307
83.667534	3318.630580	22.029325
83.320957	3321.357921	22.034343
83.270067	3312.345654	22.039360
83.946380	3316.725372	22.044378
83.817054	3346.991123	22.049395
84.009323	3324.391580	22.054413
83.923251	3329.297145	22.059431
83.998229	3336.453229	22.064448
84.821420	3336.369364	22.069466
84.555228	3331.193785	22.074483
84.089157	3337.499884	22.079501
84.529912	3329.578842	22.084519
84.505331	3343.422557	22.089536
84.855934	3345.612117	22.094554
84.876304	3341.395580	22.099571
85.174766	3350.584162	22.104589
85.337386	3357.568802	22.109607
85.073353	3354.273956	22.114624
85.537477	3353.712602	22.119642
85.450132	3357.314876	22.124659
85.263901	3351.078995	22.129677
85.566043	3348.418762	22.134695
85.392968	3351.791357	22.139712
85.475471	3344.323763	22.144730
85.349128	3347.666989	22.149747
85.397545	3345.939455	22.154765
85.645968	3355.359918	22.159783
85.770243	3366.766009	22.164800
85.951325	3372.532655	22.169818
85.806759	3377.254813	22.174835
85.802751	3373.045220	22.179853
85.848169	3376.888789	22.184871
86.084550	3398.632843	22.189888
86.317172	3392.618946	22.194906
86.214449	3413.932920	22.199923
86.332427	3393.674116	22.204941
86.545896	3393.252784	22.209959
86.553142	3410.579167	22.214976
86.927244	3419.232083	22.219994
86.591138	3423.668457	22.225011
86.818606	3424.542135	22.230029
87.043544	3417.860316	22.235047
87.026231	3426.148093	22.240064
86.985244	3429.613760	22.245082
87.494085	3442.257213	22.250099
87.725414	3440.542222	22.255117
87.661769	3437.793742	22.260135
87.527331	3450.909785	22.265152
87.433836	3446.710951	22.270170
87.809688	3441.176572	22.275187
87.959000	3443.990845	22.280205
87.690640	3448.918511	22.285223
87.505035	3459.599642	22.290240
87.802363	3468.927334	22.295258
87.991224	3464.911780	22.300275
87.795221	3476.503521	22.305293
88.530860	3478.153409	22.310311
88.461144	3488.188432	22.315328
88.761120	3492.008174	22.320346
88.695347	3500.571805	22.325363
89.009363	3498.765030	22.330381
89.136490	3493.780662	22.335399
89.385555	3494.228051	22.340416
89.106267	3488.079203	22.345434
88.860041	3492.779345	22.350451
89.149100	3493.633968	22.355469
89.534297	3491.011282	22.360487
88.957701	3490.201654	22.365504
89.108623	3478.039567	22.370522
89.415611	3488.792363	22.375539
89.406338	3512.430640	22.380557
89.714190	3513.758923	22.385575
89.228106	3514.737388	22.390592
89.502088	3519.448074	22.395610
89.438551	3519.903103	22.400627
89.761011	3535.207907	22.405645
90.387489	3533.251482	22.410663
90.017745	3537.813056	22.415680
90.122581	3539.138232	22.420698
90.318470	3538.176768	22.425715
90.249380	3537.124000	22.430733
90.697457	3550.506072	22.435751
90.415767	3564.550953	22.440768
90.738258	3554.353668	22.445786
90.589524	3563.129086	22.450803
90.520057	3560.476180	22.455821
91.224423	3568.029889	22.460839
91.447205	3585.556442	22.465856
91.397637	3587.151844	22.470874
91.112017	3586.176972	22.475891
91.244463	3587.876598	22.480909
91.796763	3585.467753	22.485927
91.470393	3587.093628	22.490944
91.381395	3585.655742	22.495962
91.578550	3590.078568	22.500979
91.774990	3607.047438	22.505997
92.058935	3613.006456	22.511015
92.224441	3607.173374	22.516032
92.362934	3607.899947	22.521050
92.577820	3599.524741	22.526067
92.344528	3598.020947	22.531085
92.831751	3601.757903	22.536103
92.311610	3600.273519	22.541120
92.479619	3600.979716	22.546138
92.418752	3603.577397	22.551155
92.784139	3612.793569	22.556173
92.987601	3621.065999	22.561191
92.769264	3616.378412	22.566208
92.847976	3620.775500	22.571226
93.122629	3620.306763	22.576243
93.407428	3621.995296	22.581261
93.531159	3620.600036	22.586279
93.171120	3624.128040	22.591296
93.260165	3634.375142	22.596314
93.606611	3645.980379	22.601331
93.337541	3654.020241	22.606349
93.691729	3645.440265	22.611367
93.818102	3655.012449	22.616384
93.637976	3659.213129	22.621402
93.860367	3670.256951	22.626419
93.985261	3674.021930	22.631437
93.988926	3674.990433	22.636455
94.104535	3680.647435	22.641472
94.470658	3694.597870	22.646490
94.607215	3696.631425	22.651507
94.396771	3714.212928	22.656525
94.771973	3708.296665	22.661543
94.601935	3703.652036	22.666560
94.715690	3705.960578	22.671578
94.953633	3704.506499	22.676595
95.318866	3715.108331	22.681613
95.149457	3720.323662	22.686631
95.192022	3726.029926	22.691648
95.378077	3720.799604	22.696666
95.575570	3725.834719	22.701683
95.332070	3723.783319	22.706701
95.337302	3717.769999	22.711719
95.441016	3725.407824	22.716736
95.500977	3730.319167	22.721754
95.878063	3742.876034	22.726771
95.753899	3746.765022	22.731789
96.080374	3742.087266	22.736807
96.182666	3748.721640	22.741824
95.697096	3752.486992	22.746842
96.170728	3767.171929	22.751859
96.139383	3771.021221	22.756877
96.266813	3761.378124	22.761895
96.758813	3776.107552	22.766912
96.693919	3791.034165	22.771930
96.959909	3793.145423	22.776947
97.007755	3798.339577	22.781965
97.376765	3788.138073	22.786983
97.269800	3796.544133	22.792000
97.314618	3790.259502	22.797018
97.484463	3792.650853	22.802035
97.412294	3794.969417	22.807053
97.577313	3798.245269	22.812071
97.374372	3814.285454	22.817088
97.678061	3822.040528	22.822106
97.799332	3814.238455	22.827123
97.785591	3818.375391	22.832141
97.910223	3818.605444	22.837159
98.182816	3827.615236	22.842176
97.903344	3838.699424	22.847194
98.215911	3839.607217	22.852211
98.605504	3834.645016	22.857229
98.932144	3832.211305	22.862247
99.239290	3832.630723	22.867264
99.176885	3828.250210	22.872282
99.529856	3826.828712	22.877299
98.936968	3823.689136	22.882317
99.348299	3831.275955	22.887335
99.488650	3826.156874	22.892352
99.262600	3827.685088	22.897370
98.943224	3821.068930	22.902387
99.356870	3842.202014	22.907405
99.569322	3845.552552	22.912423
99.730796	3855.280346	22.917440
99.541575	3853.498231	22.922458
99.665538	3850.793072	22.927475
99.647433	3858.311045	22.932493
99.855305	3859.276170	22.937511
100.064661	3870.745083	22.942528
99.884093	3878.171577	22.947546
100.305930	3871.380029	22.952563
100.194331	3877.075624	22.957581
100.347617	3878.588969	22.962599
100.618291	3903.632896	22.967616
100.632540	3895.623355	22.972634
100.739933	3900.612579	22.977651
100.722801	3904.260842	22.982669
100.827608	3903.730167	22.987687
101.070880	3914.512075	22.992704
101.300820	3929.506524	22.997722
101.311592	3924.814749	23.002739
101.069411	3931.016756	23.007757
101.454081	3928.428810	23.012775
101.618907	3918.839776	23.017792
101.771256	3934.417594	23.022810
101.462156	3945.089832	23.027827
101.992572	3953.365166	23.032845
102.200840	3943.065508	23.037863
102.161517	3948.330089	23.042880
102.162584	3956.204931	23.047898
102.430983	3945.390906	23.052915
102.080368	3946.929054	23.057933
102.299041	3954.309201	23.062951
102.390173	3959.108440	23.067968
102.405569	3965.911080	23.072986
102.602824	3966.091952	23.078003
102.648140	3978.486012	23.083021
102.948071	3984.581541	23.088039
103.556589	3982.066048	23.093056
103.405026	3984.718937	23.098074
103.331565	3986.838881	23.103091
103.464884	3994.506929	23.108109
103.706766	3989.472996	23.113127
103.521816	3993.466189	23.118144
103.510705	3993.196593	23.123162
103.997351	3994.938955	23.128179
103.755774	4003.773230	23.133197
103.880320	4018.083468	23.138215
104.017183	4013.533008	23.143232
104.202668	4013.949279	23.148250
104.211154	4001.856361	23.153267
104.156935	4018.520609	23.158285
104.293836	4027.365407	23.163303
104.767706	4031.568508	23.168320
104.858433	4041.026508	23.173338
105.088033	4041.742070	23.178355
104.826658	4037.995335	23.183373
105.280806	4055.985016	23.188391
105.460687	4064.406511	23.193408
105.500611	4062.781232	23.198426
105.549259	4057.821552	23.203443
105.233748	4066.762057	23.208461
105.549752	4066.807660	23.213479
105.569266	4072.003147	23.218496
105.787630	4083.859017	23.223514
105.868947	4089.474142	23.228531
106.088926	4089.973420	23.233549
106.144913	4091.078989	23.238567
106.462203	4083.849133	23.243584
106.283251	4084.397897	23.248602
106.272205	4087.631775	23.253619
106.801058	4097.564475	23.258637
106.815391	4103.713979	23.263655
107.101662	4104.638505	23.268672
106.749246	4109.762501	23.273690
107.150848	4105.192895	23.278707
106.884964	4111.528063	23.283725
107.113756	4107.663965	23.288743
107.315832	4123.871777	23.293760
107.566495	4132.077123	23.298778
107.300355	4132.721526	23.303795
107.572874	4129.077870	23.308813
107.889889	4133.093943	23.313831
107.785763	4131.320645	23.318848
107.735072	4139.216251	23.323866
107.961502	4157.825404	23.328883
108.262429	4165.581057	23.333901
107.726260	4162.495715	23.338919
108.570351	4156.954500	23.343936
108.573096	4167.461533	23.348954
108.617272	4170.592139	23.353971
108.439883	4178.273922	23.358989
108.289451	4181.437985	23.364007
108.728919	4184.327140	23.369024
108.893998	4184.080610	23.374042
109.032358	4203.057029	23.379059
109.024007	4212.877739	23.384077
109.111313	4208.013002	23.389095
109.238527	4209.937600	23.394112
109.364473	4216.322270	23.399130
109.594274	4220.923235	23.404147
109.751177	4229.973335	23.409165
109.606733	4234.203312	23.414183
110.036029	4232.208075	23.419200
109.748180	4238.414142	23.424218
109.982144	4245.596335	23.429235
110.225886	4246.480146	23.434253
110.348750	4260.099603	23.439271
110.732484	4239.318714	23.444288
110.669709	4244.224055	23.449306
110.863449	4245.251373	23.454323
110.934042	4240.455512	23.459341
110.862441	4255.099483	23.464359
111.408437	4265.840782	23.469376
111.445536	4268.372805	23.474394
111.437404	4270.482611	23.479411
111.456928	4268.175566	23.484429
111.289084	4269.164491	23.489447
111.805703	4266.596986	23.494464
111.648082	4270.661737	23.499482
111.728840	4281.462854	23.504499
112.093607	4288.141782	23.509517
111.936831	4295.435332	23.514535
112.713080	4288.755735	23.519552
112.407201	4288.459432	23.524570
112.287351	4292.467806	23.529587
112.418851	4302.503516	23.534605
112.439365	4317.035350	23.539623
113.030960	4311.858502	23.544640
112.691205	4309.174972	23.549658
112.813002	4309.534883	23.554675
113.003134	4309.442267	23.559693
113.027107	4325.823181	23.564711
113.338504	4335.319574	23.569728
113.194226	4336.219612	23.574746
113.660534	4334.846714	23.579763
113.598426	4342.479054	23.584781
113.689087	4353.789999	23.589799
113.993547	4351.716340	23.594816
113.660625	4352.683625	23.599834
113.982979	4354.170689	23.604851
114.274407	4359.557492	23.609869
114.268415	4370.646771	23.614887
114.396081	4371.245651	23.619904
114.384375	4385.208101	23.624922
114.909971	4379.886849	23.629939
115.134781	4372.885909	23.634957
114.950374	4378.125858	23.639975
115.368116	4387.072299	23.644992
115.216133	4391.830596	23.650010
115.149534	4399.249027	23.655027
115.616018	4394.754468	23.660045
115.542624	4390.956297	23.665063
115.482081	4397.382692	23.670080
115.438388	4404.964845	23.675098
115.563503	4408.742568	23.680115
115.765990	4404.260703	23.685133
115.842359	4413.149834	23.690151
115.885327	4413.140101	23.695168
116.374233	4436.086536	23.700186
116.318913	4443.613701	23.705203
116.546077	4441.529972	23.710221
116.787914	4445.598853	23.715239
116.911917	4438.130659	23.720256
116.807539	4439.415879	23.725274
117.006817	4441.569164	23.730291
117.167736	4438.536217	23.735309
117.269338	4453.415360	23.740327
117.466555	4463.968040	23.745344
117.277892	4476.004324	23.750362
117.266699	4473.544218	23.755379
117.707138	4465.764768	23.760397
117.376597	4473.931349	23.765415
118.156335	4480.634118	23.770432
118.281002	4487.451505	23.775450
118.424568	4484.910488	23.780467
118.492574	4485.294559	23.785485
118.361662	4490.889194	23.790503
118.684974	4491.542839	23.795520
118.475756	4481.601416	23.800538
118.331844	4488.817289	23.805555
118.725005	4500.109636	23.810573
118.821145	4506.669493	23.815591
119.157056	4516.130602	23.820608
119.340351	4515.609784	23.825626
119.423882	4504.619044	23.830643
119.657638	4508.818609	23.835661
119.714828	4522.921944	23.840679
120.014108	4525.668850	23.845696
120.132941	4528.970964	23.850714
120.127290	4531.680124	23.855731
120.371160	4522.709739	23.860749
120.332094	4529.805144	23.865767
120.046034	4525.345653	23.870784
120.064554	4531.463087	23.875802
120.202130	4551.172271	23.880819
120.553507	4545.957005	23.885837
120.250681	4559.204228	23.890855
120.867638	4561.734392	23.895872
121.200584	4563.658560	23.900890
121.080500	4565.984682	23.905907
121.304308	4559.504628	23.910925
121.877008	4562.448855	23.915943
121.559167	4563.379083	23.920960
121.791267	4570.681639	23.925978
121.449242	4568.228839	23.930995
121.700555	4578.807884	23.936013
121.802849	4586.534673	23.941031
122.101401	4590.743106	23.946048
121.969582	4592.158864	23.951066
122.397671	4605.036656	23.956083
122.672278	4602.604632	23.961101
122.339938	4617.560940	23.966119
122.656669	4616.848900	23.971136
122.843564	4619.613318	23.976154
122.751626	4625.738512	23.981171
123.205915	4630.702336	23.986189
123.034928	4639.024063	23.991207
123.176258	4634.763140	23.996224
123.419762	4634.444423	24.001242
123.449770	4653.943207	24.006259
123.691838	4653.719405	24.011277
123.664972	4660.790867	24.016295
124.011873	4657.271250	24.021312
124.430040	4655.356612	24.026330
123.880009	4664.936794	24.031347
124.353894	4669.847076	24.036365
124.498051	4688.374893	24.041383
124.931873	4691.296574	24.046400
124.791762	4681.704111	24.051418
124.554202	4676.466870	24.056435
124.918787	4680.993310	24.061453
124.905070	4688.072204	24.066471
125.082066	4695.670622	24.071488
124.998493	4703.454807	24.076506
125.295002	4707.695150	24.081523
125.580628	4705.902147	24.086541
125.204480	4702.820204	24.091559
125.494131	4713.506990	24.096576
125.800360	4723.329502	24.101594
125.816715	4733.992565	24.106611
126.350440	4719.746789	24.111629
126.104938	4731.672149	24.116647
126.407080	4746.037379	24.121664
126.771144	4747.764182	24.126682
126.719721	4748.987519	24.131699
126.767635	4746.148874	24.136717
126.724726	4742.535267	24.141735
126.722325	4755.208739	24.146752
126.998834	4754.117873	24.151770
127.371512	4774.333600	24.156787
127.300465	4766.901952	24.161805
127.640444	4775.526114	24.166823
127.536500	4786.198469	24.171840
127.766468	4792.005305	24.176858
127.404032	4801.054481	24.181875
127.686547	4799.501841	24.186893
127.930870	4812.528336	24.191911
128.001663	4822.314960	24.196928
128.515058	4813.239340	24.201946
128.378896	4819.055843	24.206963
128.629943	4826.548094	24.211981
128.917946	4846.101609	24.216999
129.014988	4843.810831	24.222016
129.523649	4836.083731	24.227034
129.203270	4843.990068	24.232051
129.539480	4837.918533	24.237069
129.491530	4842.032621	24.242087
129.337400	4858.760544	24.247104
129.844086	4856.911014	24.252122
129.741275	4860.607530	24.257139
130.018068	4855.107084	24.262157
130.017111	4880.507141	24.267175
130.065350	4877.873593	24.272192
130.322996	4881.583434	24.277210
130.049004	4897.013822	24.282227
130.778847	4898.390142	24.287245
130.793181	4917.800113	24.292263
130.829201	4916.509948	24.297280
131.047009	4912.000321	24.302298
130.564263	4920.421218	24.307315
131.436870	4929.050908	24.312333
131.344408	4937.070153	24.317351
131.465376	4939.753348	24.322368
131.962262	4933.347433	24.327386
132.057104	4941.018718	24.332403
132.016354	4947.199179	24.337421
132.147281	4954.773314	24.342439
132.573697	4965.268508	24.347456
132.597777	4962.622926	24.352474
132.337828	4964.503720	24.357491
132.666055	4962.217967	24.362509
132.765359	4967.596987	24.367527
132.690513	4968.401022	24.372544
132.921197	4986.047649	24.377562
132.805067	4989.648415	24.382579
133.113950	4989.269011	24.387597
132.846000	5001.804080	24.392615
132.859546	5013.379960	24.397632
133.385363	5007.076835	24.402650
133.228078	5028.827326	24.407667
133.449799	5038.309643	24.412685
133.557617	5043.128667	24.417703
134.135998	5049.541042	24.422720
133.918052	5060.657429	24.427738
134.190569	5066.287280	24.432755
134.437881	5058.382980	24.437773
134.830755	5065.395562	24.442791
134.811023	5077.873100	24.447808
135.118541	5081.085966	24.452826
135.224452	5069.617930	24.457843
135.466876	5073.415406	24.462861
135.577839	5066.173094	24.467879
135.539824	5072.015431	24.472896
136.168098	5070.402624	24.477914
135.698594	5076.694073	24.482931
135.929454	5092.285916	24.487949
136.318606	5098.838246	24.492967
136.218387	5092.212751	24.497984
136.473210	5090.462384	24.503002
136.332884	5091.336592	24.508019
136.563830	5107.398748	24.513037
136.887162	5109.144554	24.518055
136.842100	5113.040458	24.523072
137.035712	5110.955564	24.528090
137.183926	5113.476719	24.533107
137.541801	5112.865575	24.538125
137.880735	5125.113698	24.543143
137.757567	5134.656075	24.548160
137.719398	5133.320629	24.553178
137.934416	5133.978534	24.558195
137.876461	5127.302254	24.563213
138.163639	5129.498754	24.568231
138.221228	5144.741999	24.573248
138.180986	5153.113047	24.578266
138.188662	5159.535403	24.583283
138.697458	5162.922118	24.588301
138.870554	5161.449613	24.593319
138.420186	5182.709317	24.598336
139.003239	5174.033017	24.603354
139.222880	5190.684113	24.608371
139.592589	5202.128906	24.613389
139.707675	5211.239668	24.618407
139.694431	5216.087056	24.623424
139.734817	5211.200948	24.628442
139.542026	5208.993126	24.633459
140.093989	5225.289492	24.638477
140.102945	5233.858090	24.643495
140.121857	5239.196047	24.648512
140.461205	5232.019120	24.653530
140.457049	5246.280924	24.658547
140.559810	5256.088056	24.663565
141.063798	5262.044928	24.668583
140.503391	5262.125979	24.673600
140.900348	5270.836201	24.678618
141.247702	5289.999019	24.683635
141.227837	5282.208819	24.688653
141.702105	5286.869847	24.693671
141.943640	5303.583925	24.698688
142.247980	5314.243527	24.703706
142.463316	5306.363038	24.708723
142.408220	5299.954553	24.713741
142.890117	5303.263413	24.718759
142.576735	5301.835072	24.723776
142.807944	5298.996212	24.728794
142.718038	5303.391553	24.733811
142.791118	5306.262178	24.738829
142.977272	5302.208764	24.743847
143.013315	5326.539941	24.748864
143.301724	5327.360036	24.753882
143.586913	5322.858756	24.758899
143.571537	5320.206639	24.763917
143.514129	5319.704336	24.768935
143.792534	5337.324936	24.773952
143.838563	5345.108156	24.778970
144.117718	5346.901898	24.783987
143.850596	5342.991646	24.789005
144.254386	5355.589670	24.794023
144.383193	5367.207804	24.799040
144.096291	5367.138951	24.804058
144.334854	5380.179377	24.809075
144.785034	5401.163397	24.814093
145.009784	5396.488430	24.819111
144.749435	5408.545962	24.824128
145.061578	5413.235420	24.829146
145.474561	5423.278432	24.834163
145.486102	5442.291675	24.839181
145.967321	5444.192855	24.844199
145.865390	5448.252354	24.849216
146.121838	5452.903147	24.854234
145.936869	5454.715499	24.859251
146.410670	5471.027411	24.864269
146.592368	5465.197526	24.869287
146.480729	5473.699786	24.874304
146.871657	5487.650901	24.879322
147.370613	5492.582758	24.884339
147.326113	5493.852415	24.889357
147.753625	5491.532200	24.894375
147.408135	5493.776741	24.899392
147.864250	5500.552376	24.904410
147.958272	5498.331430	24.909427
147.935132	5507.997317	24.914445
148.217203	5511.242630	24.919463
148.214675	5520.321354	24.924480
148.462162	5515.952159	24.929498
148.135828	5523.086363	24.934515
148.350181	5541.995535	24.939533
148.558786	5544.595731	24.944551
148.871044	5552.915238	24.949568
149.041987	5555.341376	24.954586
149.302498	5565.348231	24.959603
149.249954	5562.386210	24.964621
149.297907	5581.296077	24.969639
149.482368	5596.895577	24.974656
149.734764	5592.762341	24.979674
150.278122	5598.523802	24.984691
150.096586	5612.497853	24.989709
150.530414	5613.812997	24.994727
150.247373	5614.772579	24.999744
150.477524	5616.848599	25.004762
150.578600	5634.743308	25.009779
150.586362	5639.499154	25.014797
150.881555	5644.525908	25.019815
150.822684	5653.575592	25.024832
151.376034	5664.597515	25.029850
151.766296	5667.494573	25.034867
151.634521	5667.070126	25.039885
152.177197	5664.580445	25.044903
152.140853	5678.197345	25.049920
152.074517	5685.063860	25.054938
152.435624	5680.610648	25.059955
152.355239	5690.979990	25.064973
152.758392	5690.772134	25.069991
153.101799	5678.944768	25.075008
153.173622	5664.659691	25.080026
153.597953	5667.870258	25.085043
153.148607	5676.324180	25.090061
153.661549	5677.914259	25.095079
153.724434	5684.501816	25.100096
153.767014	5698.330561	25.105114
153.687848	5695.139077	25.110131
153.737972	5698.799326	25.115149
154.445610	5698.995454	25.120167
154.276248	5691.607144	25.125184
154.410843	5712.624875	25.130202
154.836217	5711.188807	25.135219
154.805816	5720.830685	25.140237
155.321847	5719.033279	25.145255
154.986433	5717.567299	25.150272
155.103895	5720.020725	25.155290
155.528417	5728.846827	25.160307
155.256667	5738.652553	25.165325
155.162929	5735.299189	25.170343
155.730648	5740.280383	25.175360
155.897453	5744.149749	25.180378
156.473169	5752.175804	25.185395
156.372163	5766.781379	25.190413
156.448811	5761.671673	25.195431
156.368428	5759.411560	25.200448
156.640989	5770.366784	25.205466
156.867098	5777.333005	25.210483
156.823051	5787.744094	25.215501
157.028015	5791.228738	25.220519
157.188399	5797.460244	25.225536
157.289524	5799.651071	25.230554
157.612904	5794.954334	25.235571
157.703966	5812.137387	25.240589
157.867527	5816.294523	25.245607
157.893605	5823.345568	25.250624
158.059836	5834.569912	25.255642
158.340507	5845.564954	25.260659
157.765535	5849.218387	25.265677
158.762269	5864.590643	25.270695
158.687718	5874.836074	25.275712
158.949851	5883.766449	25.280730
159.242879	5879.888821	25.285747
158.884722	5896.731534	25.290765
159.447163	5908.440331	25.295783
159.538129	5917.261638	25.300800
159.690794	5922.039191	25.305818
159.972435	5927.033410	25.310835
160.122221	5944.201132	25.315853
160.052414	5955.651697	25.320871
160.696859	5950.519826	25.325888
160.716526	5960.554926	25.330906
160.792555	5956.259670	25.335923
161.263819	5968.307833	25.340941
161.862666	5964.543562	25.345959
161.995588	5961.539974	25.350976
161.647057	5970.884286	25.355994
161.886242	5966.468927	25.361011
162.207051	5966.501165	25.366029
162.212568	5966.550926	25.371047
162.215010	5964.407314	25.376064
162.100923	5965.381645	25.381082
162.788522	5979.621553	25.386099
162.559795	5987.637222	25.391117
162.422232	5985.726898	25.396135
162.924048	6002.773578	25.401152
162.839014	6018.794193	25.406170
163.429778	6008.105527	25.411187
163.251806	6014.500269	25.416205
163.467606	6017.929607	25.421223
163.907079	6019.777373	25.426240
163.670486	6038.602594	25.431258
163.991417	6038.183415	25.436275
163.909151	6033.054182	25.441293
164.279688	6055.774879	25.446311
164.588466	6060.840671	25.451328
164.400133	6066.135377	25.456346
164.707200	6060.721399	25.461363
165.065175	6081.616392	25.466381
165.268830	6076.827741	25.471399
165.440419	6079.487441	25.476416
165.500843	6082.233894	25.481434
165.953084	6088.502134	25.486451
165.618895	6110.003672	25.491469
165.681817	6104.760272	25.496487
165.989976	6099.731223	25.501504
166.314790	6122.354953	25.506522
166.482264	6125.545617	25.511539
166.410145	6129.853157	25.516557
166.295670	6139.085354	25.521575
166.934901	6147.632014	25.526592
166.796904	6155.352689	25.531610
167.032211	6164.053786	25.536627
167.220684	6176.370238	25.541645
167.697410	6167.473275	25.546663
168.034523	6183.687157	25.551680
168.320280	6190.315958	25.556698
168.650729	6194.191508	25.561715
168.499167	6200.591673	25.566733
169.119965	6204.093729	25.571751
169.026932	6202.523682	25.576768
168.368445	6209.937146	25.581786
168.957798	6214.081745	25.586803
169.255332	6218.975714	25.591821
169.268643	6218.838019	25.596839
169.609638	6240.556570	25.601856
169.540848	6249.753301	25.606874
169.906607	6251.464204	25.611891
170.084084	6263.318396	25.616909
170.093605	6271.615920	25.621927
170.630020	6269.133448	25.626944
170.448600	6277.489112	25.631962
170.571014	6280.967763	25.636979
171.088093	6283.788357	25.641997
171.112121	6297.083809	25.647015
171.281785	6300.823424	25.652032
170.911853	6320.850293	25.657050
171.480882	6315.603796	25.662067
171.765332	6322.504323	25.667085
172.124011	6334.532378	25.672103
172.031410	6350.920638	25.677120
172.326493	6347.465588	25.682138
172.493759	6338.247391	25.687156
172.613289	6363.324558	25.692173
172.676656	6365.966425	25.697191
172.834249	6360.907083	25.702208
173.113035	6368.443004	25.707226
173.658283	6375.691221	25.712244
173.662928	6388.822453	25.717261
173.753926	6388.824183	25.722279
174.437930	6381.460566	25.727296
174.437270	6390.012264	25.732314
174.465827	6376.497286	25.737332
174.723359	6394.245271	25.742349
174.503814	6403.547623	25.747367
174.745994	6399.377917	25.752384
174.698158	6407.305629	25.757402
174.665771	6406.155434	25.762420
175.319887	6412.796413	25.767437
175.562008	6429.710307	25.772455
175.569934	6427.723622	25.777472
175.497704	6425.399023	25.782490
175.840157	6426.254949	25.787508
176.165831	6447.622583	25.792525
176.169470	6450.358992	25.797543
176.468570	6445.940503	25.802560
176.443741	6458.337706	25.807578
176.696454	6462.411662	25.812596
176.762264	6468.512915	25.817613
176.853443	6478.208868	25.822631
177.352689	6489.991014	25.827648
177.280609	6496.565154	25.832666
177.580448	6505.003830	25.837684
178.180741	6512.139360	25.842701
177.872227	6522.680430	25.847719
178.211921	6524.357538	25.852736
178.359363	6530.196721	25.857754
178.567734	6533.330582	25.862772
179.034846	6534.946815	25.867789
178.740527	6539.342711	25.872807
179.061084	6530.523551	25.877824
179.051108	6544.231694	25.882842
179.337936	6555.595543	25.887860
179.749416	6553.179835	25.892877
179.513410	6556.673303	25.897895
180.445376	6566.828709	25.902912
180.234206	6576.909556	25.907930
180.068090	6580.739388	25.912948
180.000026	6586.552163	25.917965
180.064804	6604.557647	25.922983
180.929214	6611.639469	25.928000
181.445442	6626.272746	25.933018
181.318489	6619.799223	25.938036
182.024636	6619.544186	25.943053
182.057051	6625.909543	25.948071
182.298904	6615.779924	25.953088
182.499939	6615.410968	25.958106
182.404566	6621.931958	25.963124
182.754758	6630.438615	25.968141
182.559034	6642.995132	25.973159
183.017072	6649.729861	25.978176
183.145382	6649.987791	25.983194
183.058414	6655.528895	25.988212
183.542159	6659.412247	25.993229
183.490062	6675.216808	25.998247
183.921401	6669.038312	26.003264
183.843864	6667.910914	26.008282
184.044799	6680.579321	26.013300
184.446556	6692.496733	26.018317
183.988203	6694.860006	26.023335
184.283809	6710.503134	26.028352
184.522698	6718.503140	26.033370
184.592095	6730.055631	26.038388
184.680932	6733.962601	26.043405
184.836532	6749.381333	26.048423
185.245050	6765.319448	26.053440
185.537162	6784.318818	26.058458
185.478701	6782.901177	26.063476
185.694034	6786.245501	26.068493
186.074405	6804.145225	26.073511
186.283552	6807.881954	26.078528
186.468536	6816.733253	26.083546
186.668753	6829.348210	26.088564
187.144226	6825.192595	26.093581
186.924853	6826.208618	26.098599
187.244809	6839.796165	26.103616
187.539797	6846.846776	26.108634
187.570632	6843.751609	26.113652
187.647804	6854.516931	26.118669
188.129467	6867.937269	26.123687
188.243004	6876.783937	26.128704
188.430472	6881.313251	26.133722
188.547186	6889.367079	26.138740
188.563682	6895.697126	26.143757
188.750188	6904.718697	26.148775
189.044509	6909.897464	26.153792
189.468787	6927.279073	26.158810
189.385154	6935.556677	26.163828
189.743670	6930.437486	26.168845
189.881218	6947.525979	26.173863
190.159935	6952.470429	26.178880
190.340981	6956.154742	26.183898
190.003796	6962.599856	26.188916
190.801963	6979.247750	26.193933
190.810458	6985.964204	26.198951
190.681053	6980.958844	26.203968
191.061513	6990.786812	26.208986
191.030364	7000.846178	26.214004
191.661924	7013.990742	26.219021
191.906759	7026.374756	26.224039
192.249332	7023.840287	26.229056
192.369419	7028.575850	26.234074
192.145797	7044.925151	26.239092
192.695648	7050.562950	26.244109
192.815718	7057.258901	26.249127
192.753446	7064.314709	26.254144
193.381083	7067.989495	26.259162
193.208187	7074.443794	26.264180
193.508166	7079.659611	26.269197
193.856513	7097.460433	26.274215
194.100696	7100.885557	26.279232
194.283984	7095.386372	26.284250
194.094861	7110.120383	26.289268
194.723168	7107.970744	26.294285
195.145119	7110.992533	26.299303
195.064969	7115.080578	26.304320
195.263904	7124.927408	26.309338
195.527564	7135.613353	26.314356
195.923104	7125.781522	26.319373
196.034398	7138.053816	26.324391
196.324000	7151.409560	26.329408
196.323796	7148.353898	26.334426
196.218826	7157.796635	26.339444
196.926885	7149.762879	26.344461
196.902507	7169.383309	26.349479
196.929442	7184.787715	26.354496
196.928546	7184.614342	26.359514
196.938863	7185.976601	26.364532
197.257729	7199.425685	26.369549
197.226159	7205.618109	26.374567
197.573519	7217.490667	26.379584
198.129774	7227.253510	26.384602
198.247313	7243.511990	26.389620
198.399239	7257.959416	26.394637
198.429672	7268.078791	26.399655
198.652800	7274.903992	26.404672
198.951630	7286.285369	26.409690
199.042269	7295.157901	26.414708
198.923164	7296.284612	26.419725
199.255707	7317.472253	26.424743
199.598665	7321.254549	26.429760
199.889438	7330.140136	26.434778
200.003458	7333.115197	26.439796
200.496244	7323.710081	26.444813
200.776253	7337.866139	26.449831
201.087586	7351.632194	26.454848
201.626208	7344.909575	26.459866
201.332270	7351.253385	26.464884
201.360937	7347.792275	26.469901
201.407357	7370.868129	26.474919
201.755574	7382.753289	26.479936
201.906425	7370.045637	26.484954
201.892430	7394.785123	26.489972
202.177474	7399.305689	26.494989
202.645297	7400.470459	26.500007
202.511155	7419.044381	26.505024
203.082665	7426.566734	26.510042
203.147615	7435.474903	26.515060
203.387343	7442.486995	26.520077
203.659491	7451.407109	26.525095
203.652186	7454.637845	26.530112
203.943895	7475.570005	26.535130
203.986230	7474.512286	26.540148
204.071544	7479.919482	26.545165
204.445505	7495.952007	26.550183
204.736227	7505.383828	26.555200
205.265961	7520.520822	26.560218
205.262918	7531.699955	26.565236
205.928104	7524.755526	26.570253
205.884600	7532.992425	26.575271
206.243234	7552.086413	26.580288
206.415949	7545.935263	26.585306
206.637496	7549.521841	26.590324
206.715473	7550.778885	26.595341
206.954421	7561.712007	26.600359
206.702899	7572.850929	26.605376
207.403270	7572.139035	26.610394
207.509974	7584.620697	26.615412
208.055528	7594.663211	26.620429
207.965834	7588.944357	26.625447
207.835693	7598.653262	26.630464
207.980543	7605.017238	26.635482
208.259552	7609.216791	26.640500
208.197959	7619.183372	26.645517
208.794100	7636.100088	26.650535
208.666963	7645.148756	26.655552
209.209298	7662.490586	26.660570
209.091582	7668.314590	26.665588
209.489280	7677.328917	26.670605
210.084585	7688.651759	26.675623
210.328730	7692.408477	26.680640
210.209914	7685.027274	26.685658
210.642626	7701.896886	26.690676
210.958044	7696.187536	26.695693
211.404672	7695.284688	26.700711
211.554139	7707.396731	26.705728
212.339066	7711.552268	26.710746
212.161005	7726.165087	26.715764
212.199516	7718.850927	26.720781
212.331990	7727.723470	26.725799
211.997124	7725.389083	26.730816
212.514056	7733.434640	26.735834
212.806742	7750.089328	26.740852
212.314555	7756.227372	26.745869
212.735206	7762.996748	26.750887
212.962613	7774.133837	26.755904
213.119657	7780.293932	26.760922
213.269757	7800.557141	26.765940
213.653334	7802.315931	26.770957
214.097378	7819.644801	26.775975
214.101802	7831.081823	26.780992
214.240101	7828.733738	26.786010
214.130439	7853.959121	26.791028
214.679088	7867.906446	26.796045
214.857171	7875.853287	26.801063
215.068370	7887.103461	26.806080
215.469646	7889.629800	26.811098
215.465306	7905.330119	26.816116
215.442217	7915.309806	26.821133
215.913726	7929.067143	26.826151
215.899463	7950.492611	26.831168
216.261608	7949.978583	26.836186
216.883849	7962.888511	26.841204
217.102110	7963.656512	26.846221
217.692083	7971.141491	26.851239
217.582924	7978.242832	26.856256
218.007153	7989.860837	26.861274
218.217727	7988.461199	26.866292
218.320987	7989.654355	26.871309
218.861957	7997.374276	26.876327
218.735631	8010.350268	26.881344
218.855960	8005.864532	26.886362
218.867140	8021.976097	26.891380
218.751043	8032.039781	26.896397
219.267513	8041.903965	26.901415
219.140950	8058.990414	26.906432
219.599601	8057.829963	26.911450
220.048780	8076.256904	26.916468
220.059930	8087.721451	26.921485
220.544600	8093.581242	26.926503
220.719018	8111.650058	26.931520
220.990382	8107.639588	26.936538
221.065247	8126.472125	26.941556
221.350343	8131.586379	26.946573
221.517256	8133.644122	26.951591
221.684433	8152.503354	26.956608
222.151724	8164.885073	26.961626
222.671119	8175.550752	26.966644
222.672351	8176.469360	26.971661
223.284236	8178.464145	26.976679
222.959066	8184.086993	26.981696
223.338120	8189.366584	26.986714
223.800979	8186.229186	26.991732
223.902001	8193.831421	26.996749
224.493502	8209.215085	27.001767
224.738864	8215.497327	27.006784
224.560870	8210.909607	27.011802
224.877534	8216.233647	27.016820
225.022593	8231.405862	27.021837
225.694177	8232.557908	27.026855
226.279951	8238.651409	27.031872
226.079575	8225.761073	27.036890
225.954650	8234.642364	27.041908
225.796308	8242.101893	27.046925
226.153663	8248.638213	27.051943
226.286175	8264.942620	27.056960
226.471716	8268.481276	27.061978
226.716728	8286.807621	27.066996
226.735807	8290.975188	27.072013
227.096559	8307.196743	27.077031
227.414401	8318.089619	27.082048
227.885687	8332.137739	27.087066
227.869208	8332.746567	27.092084
227.983026	8350.067366	27.097101
228.499406	8350.318574	27.102119
228.627032	8359.065894	27.107136
228.754623	8373.448531	27.112154
229.103636	8388.762759	27.117172
229.279221	8382.689810	27.122189
229.759911	8395.271650	27.127207
229.962305	8405.336465	27.132224
230.125073	8411.631633	27.137242
230.839687	8402.077782	27.142260
230.496627	8409.433540	27.147277
231.016192	8417.665255	27.152295
231.088715	8425.998142	27.157312
231.105341	8431.435255	27.162330
231.277278	8431.162350	27.167348
231.546015	8449.125259	27.172365
231.624152	8442.808585	27.177383
231.745275	8465.637402	27.182400
232.175501	8477.519975	27.187418
232.354549	8481.858417	27.192436
232.465991	8495.163951	27.197453
232.977054	8503.078165	27.202471
233.142558	8516.744673	27.207488
233.911875	8517.420592	27.212506
233.915606	8528.532978	27.217524
233.688852	8543.561285	27.222541
234.362388	8552.425758	27.227559
234.378815	8567.889784	27.232576
234.539074	8573.004655	27.237594
234.753824	8588.753529	27.242612
234.747072	8592.802060	27.247629
235.305755	8597.927521	27.252647
235.281664	8614.828048	27.257664
235.622274	8635.204584	27.262682
236.126571	8640.834186	27.267700
235.618043	8657.494465	27.272717
236.098870	8667.266665	27.277735
236.507049	8678.543484	27.282752
237.001304	8694.630940	27.287770
237.216769	8702.749116	27.292788
237.193689	8708.426116	27.297805
237.830373	8714.840188	27.302823
238.073554	8726.802557	27.307840
238.331292	8730.835197	27.312858
238.763374	8742.247245	27.317876
239.040567	8742.892450	27.322893
239.410316	8738.812856	27.327911
239.435646	8749.098009	27.332928
239.638268	8765.148846	27.337946
240.045778	8764.296240	27.342964
240.109673	8774.057638	27.347981
240.710609	8782.655701	27.352999
240.730203	8796.281990	27.358016
240.732464	8791.719733	27.363034
241.341818	8794.826283	27.368052
241.126446	8816.817619	27.373069
241.496052	8817.956735	27.378087
241.659918	8818.651157	27.383104
241.492269	8833.787311	27.388122
242.134925	8838.985008	27.393140
241.692593	8851.186782	27.398157
242.416570	8865.789507	27.403175
242.702849	8888.501578	27.408192
242.611209	8894.773377	27.413210
243.026703	8904.287520	27.418228
243.385697	8921.949540	27.423245
243.729704	8934.063673	27.428263
243.821531	8939.962797	27.433280
244.124093	8951.085740	27.438298
244.405541	8963.351704	27.443316
244.728698	8976.510966	27.448333
244.959375	8977.548593	27.453351
245.078389	8992.630775	27.458368
245.483479	8990.436751	27.463386
245.324820	9014.332718	27.468404
245.922913	9028.008028	27.473421
246.122878	9033.764060	27.478439
246.202531	9044.113534	27.483456
246.234501	9054.173665	27.488474
246.336278	9066.710770	27.493492
246.796770	9081.897718	27.498509
247.345608	9090.093607	27.503527
247.453387	9107.103497	27.508544
247.610516	9116.575887	27.513562
248.106683	9125.474567	27.518580
247.981483	9132.310489	27.523597
248.430766	9144.458885	27.528615
249.024053	9157.494134	27.533632
248.563375	9169.121210	27.538650
249.115965	9179.880177	27.543668
249.078776	9192.802078	27.548685
249.722214	9201.409506	27.553703
249.681353	9230.660927	27.558720
249.856380	9232.802774	27.563738
250.675664	9244.742088	27.568756
250.624078	9271.049590	27.573773
251.287006	9281.346274	27.578791
251.757520	9288.285255	27.583808
251.471526	9292.071165	27.588826
251.943847	9299.890725	27.593844
251.708967	9306.304937	27.598861
252.247936	9323.137393	27.603879
252.328416	9328.627972	27.608896
252.778565	9353.190477	27.613914
253.243706	9354.617845	27.618932
253.193618	9375.573805	27.623949
253.754074	9380.898114	27.628967
253.566037	9391.207371	27.633984
253.606688	9406.807243	27.639002
254.004928	9418.562801	27.644020
254.402514	9440.187925	27.649037
254.865112	9458.052175	27.654055
255.552927	9469.109137	27.659072
255.258933	9473.903484	27.664090
255.987232	9482.106337	27.669108
255.966352	9494.078741	27.674125
256.142006	9502.039291	27.679143
256.501942	9517.226466	27.684160
256.364924	9526.287063	27.689178
257.177598	9542.085736	27.694196
257.250966	9555.811558	27.699213
258.047271	9555.564565	27.704231
258.293415	9556.088345	27.709248
258.345732	9567.190632	27.714266
258.884360	9581.106089	27.719284
258.824047	9586.770211	27.724301
258.867607	9589.491400	27.729319
259.596253	9590.180012	27.734336
259.611812	9609.954680	27.739354
260.139894	9607.731966	27.744372
259.723408	9617.167627	27.749389
260.130002	9625.509032	27.754407
260.598408	9629.430141	27.759424
260.637486	9643.470776	27.764442
261.055066	9648.463796	27.769460
261.299035	9659.337393	27.774477
261.227662	9674.923359	27.779495
261.682457	9681.460807	27.784512
261.819456	9696.547076	27.789530
262.477705	9704.082124	27.794548
262.700199	9714.251870	27.799565
262.663289	9716.553061	27.804583
263.042832	9724.437762	27.809600
262.718069	9739.810651	27.814618
263.508163	9748.821735	27.819636
263.508148	9764.005165	27.824653
263.740527	9772.812621	27.829671
264.076022	9778.269945	27.834688
263.961125	9795.510886	27.839706
264.813610	9807.300161	27.844724
264.645329	9819.807203	27.849741
264.731485	9832.359886	27.854759
265.012379	9839.161260	27.859776
265.318713	9866.992526	27.864794
265.616456	9879.048179	27.869812
266.142964	9890.493596	27.874829
266.271036	9914.879664	27.879847
266.835231	9923.932318	27.884864
266.916126	9933.312804	27.889882
267.073122	9943.726514	27.894900
267.454644	9963.937122	27.899917
267.578459	9975.224275	27.904935
268.037510	9988.047369	27.909952
268.078814	10008.983500	27.914970
268.635642	10021.652474	27.919988
268.988775	10036.793775	27.925005
269.094130	10050.975951	27.930023
269.802888	10056.419448	27.935040
270.244131	10074.265517	27.940058
270.789476	10065.397053	27.945076
271.271937	10067.585855	27.950093
271.102714	10070.195005	27.955111
271.281941	10074.890572	27.960128
271.474201	10090.761047	27.965146
271.699809	10094.082275	27.970164
272.045743	10095.383025	27.975181
272.515662	10111.961735	27.980199
273.147093	10114.777760	27.985216
273.339883	10110.971691	27.990234
273.334301	10106.899717	27.995252
273.218878	10133.957195	28.000269
273.228217	10134.498915	28.005287
273.649667	10146.147131	28.010304
274.009738	10165.410939	28.015322
274.291687	10185.539413	28.020340
274.496250	10182.587137	28.025357
274.569338	10201.595715	28.030375
274.779716	10215.051263	28.035392
274.966588	10233.786414	28.040410
275.256049	10256.228133	28.045428
276.008105	10265.226450	28.050445
275.896387	10269.032785	28.055463
276.460163	10285.615981	28.060480
276.490006	10302.509649	28.065498
276.531584	10323.114567	28.070516
277.280466	10334.405660	28.075533
277.183332	10352.702069	28.080551
277.629941	10367.342852	28.085568
277.680270	10385.856296	28.090586
278.084921	10398.375564	28.095604
278.226293	10407.737401	28.100621
278.295691	10432.632148	28.105639
278.786913	10438.952649	28.110656
278.596356	10469.662777	28.115674
279.254498	10479.026289	28.120692
279.670932	10496.238833	28.125709
279.879697	10511.434571	28.130727
280.379439	10527.263862	28.135744
280.415686	10545.691250	28.140762
280.979479	10549.427206	28.145780
281.164831	10565.005522	28.150797
281.315906	10585.360035	28.155815
281.672259	10584.051177	28.160832
281.589510	10604.180049	28.165850
282.160779	10620.793952	28.170868
282.828427	10628.078480	28.175885
283.146976	10646.307303	28.180903
283.538391	10651.292039	28.185920
283.966114	10669.702806	28.190938
283.883843	10677.745062	28.195956
284.188419	10694.599470	28.200973
284.008714	10700.172008	28.205991
284.926386	10710.616120	28.211008
284.828676	10722.781249	28.216026
285.337126	10734.492067	28.221044
285.858471	10748.025885	28.226061
285.969614	10756.214879	28.231079
286.325687	10763.617432	28.236096
286.807462	10780.311718	28.241114
287.159767	10789.688270	28.246132
287.575550	10793.040009	28.251149
287.761167	10798.899862	28.256167
288.311471	10800.973995	28.261184
287.963310	10808.694597	28.266202
288.369164	10814.359138	28.271220
288.842495	10823.123264	28.276237
289.067538	10846.450338	28.281255
289.125932	10839.851753	28.286272
289.483097	10861.563762	28.291290
289.348883	10866.039944	28.296308
289.868685	10879.684609	28.301325
289.949853	10906.946253	28.306343
290.360412	10926.752388	28.311360
290.452169	10936.690561	28.316378
290.807165	10950.329361	28.321396
290.869593	10968.412083	28.326413
291.350767	10988.687227	28.331431
292.113139	10997.728500	28.336448
292.264623	11021.562969	28.341466
292.408433	11035.275757	28.346484
292.774923	11038.562593	28.351501
293.092431	11059.548469	28.356519
293.744365	11077.147990	28.361536
293.711488	11090.421017	28.366554
293.763214	11106.364756	28.371572
294.254647	11117.481698	28.376589
294.682819	11130.547202	28.381607
294.972371	11139.813716	28.386624
295.037167	11160.226493	28.391642
295.354654	11177.410866	28.396660
295.753954	11187.437065	28.401677
295.843032	11214.296921	28.406695
296.395412	11223.610968	28.411712
296.071643	11240.525803	28.416730
296.583310	11257.847367	28.421748
297.100372	11274.230323	28.426765
297.455372	11299.874301	28.431783
297.796656	11305.002791	28.436800
298.392511	11320.918836	28.441818
298.469653	11328.200847	28.446836
298.832596	11350.379841	28.451853
298.960064	11358.683387	28.456871
299.737282	11372.342016	28.461888
299.760399	11386.215941	28.466906
299.977918	11399.147080	28.471924
300.543817	11407.988640	28.476941
300.593203	11418.770416	28.481959
300.877911	11430.251272	28.486976
301.069922	11433.195908	28.491994
301.446364	11447.008556	28.497012
301.645070	11450.476307	28.502029
301.707642	11468.707895	28.507047
302.345520	11472.524075	28.512064
302.743129	11491.312934	28.517082
302.738101	11511.815905	28.522100
303.327308	11531.212804	28.527117
303.391649	11539.485210	28.532135
303.349354	11555.964969	28.537152
303.997685	11566.498862	28.542170
304.176178	11582.571677	28.547188
304.598621	11602.645074	28.552205
304.698622	11622.010871	28.557223
304.945226	11627.514156	28.562240
305.375738	11642.799439	28.567258
305.471735	11663.965729	28.572276
306.035881	11690.689155	28.577293
306.295685	11709.824920	28.582311
306.923136	11727.034167	28.587328
307.232048	11735.934838	28.592346
307.454610	11760.845399	28.597364
307.626583	11767.487611	28.602381
307.925879	11782.566088	28.607399
308.440024	11796.067055	28.612416
308.803148	11810.857749	28.617434
308.736738	11829.327643	28.622452
309.293543	11848.063658	28.627469
309.534362	11857.227598	28.632487
309.871557	11869.294186	28.637504
310.425303	11892.227208	28.642522
310.557604	11902.014330	28.647540
310.896332	11911.447241	28.652557
311.072818	11941.180608	28.657575
311.364416	11957.750831	28.662592
311.654603	11964.728365	28.667610
311.747638	11998.033479	28.672628
312.228389	12006.632811	28.677645
312.878075	12023.722036	28.682663
313.308263	12048.253312	28.687680
313.664472	12054.630119	28.692698
313.744345	12070.807120	28.697716
314.357812	12080.497322	28.702733
314.605478	12097.175553	28.707751
314.732264	12110.932829	28.712768
315.320822	12120.570091	28.717786
315.134012	12145.431219	28.722804
315.318497	12156.820763	28.727821
315.608716	12174.449214	28.732839
316.002253	12190.735370	28.737856
316.570819	12211.680294	28.742874
316.709768	12228.943951	28.747892
317.100170	12241.444572	28.752909
317.510116	12255.530478	28.757927
317.738736	12272.417080	28.762944
318.162165	12275.382659	28.767962
318.929284	12296.767265	28.772980
319.110775	12313.935961	28.777997
319.546107	12328.210589	28.783015
320.006594	12328.353736	28.788032
320.538016	12339.692536	28.793050
320.294037	12350.223695	28.798068
320.760820	12360.685255	28.803085
321.081774	12367.598153	28.808103
321.308203	12377.528755	28.813120
321.680768	12389.328081	28.818138
321.688718	12401.859931	28.823156
321.775238	12404.107500	28.828173
321.801888	12429.330485	28.833191
322.229562	12448.229302	28.838208
322.616170	12460.632770	28.843226
322.766733	12484.649233	28.848244
323.044243	12500.960037	28.853261
323.719883	12513.741679	28.858279
323.627826	12534.900334	28.863296
324.444431	12549.197874	28.868314
324.721693	12576.712453	28.873332
324.808176	12597.874961	28.878349
325.141579	12608.376371	28.883367
325.700941	12632.370430	28.888384
326.177248	12641.365466	28.893402
325.897050	12661.593595	28.898420
326.796696	12674.242582	28.903437
327.157183	12699.729733	28.908455
327.399902	12717.558712	28.913472
327.971237	12725.541139	28.918490
327.688025	12747.939219	28.923508
327.903886	12766.391350	28.928525
328.463034	12781.411229	28.933543
328.610363	12799.059353	28.938560
329.149452	12812.452964	28.943578
329.426436	12848.674001	28.948596
330.060447	12858.484562	28.953613
330.472252	12869.337059	28.958631
330.715730	12901.069871	28.963648
330.978797	12911.181361	28.968666
331.315097	12935.390527	28.973684
331.897588	12948.486960	28.978701
331.935976	12967.582690	28.983719
332.088213	12988.264884	28.988736
332.291717	13009.390688	28.993754
332.817507	13039.557714	28.998772
333.316625	13062.696456	29.003789
333.320287	13080.594574	29.008807
333.325170	13097.548327	29.013824
333.955417	13115.124722	29.018842
334.328499	13133.221162	29.023860
334.882043	13159.913594	29.028877
335.290122	13173.744694	29.033895
335.463016	13196.365976	29.038912
336.423632	13207.272173	29.043930
336.576652	13228.538711	29.048948
337.446727	13237.700096	29.053965
337.348743	13254.003696	29.058983
337.507961	13267.156774	29.064000
337.667527	13283.897141	29.069018
338.036136	13306.671242	29.074036
338.448175	13325.226008	29.079053
338.964069	13344.389883	29.084071
339.035457	13358.718796	29.089088
339.715929	13376.723404	29.094106
339.779320	13396.769355	29.099124
340.231034	13412.201199	29.104141
340.623522	13426.407542	29.109159
341.190854	13443.975093	29.114176
341.599822	13454.342054	29.119194
341.330960	13459.992444	29.124212
341.654641	13486.354808	29.129229
342.566776	13514.855075	29.134247
342.521734	13520.969586	29.139264
343.186415	13541.035764	29.144282
343.126515	13555.243159	29.149300
343.411184	13573.783262	29.154317
343.880215	13593.778902	29.159335
344.356384	13599.288080	29.164352
344.973678	13601.096315	29.169370
345.348859	13623.386614	29.174388
345.324466	13633.164293	29.179405
345.579764	13642.797381	29.184423
345.783586	13659.676455	29.189440
346.354712	13680.177350	29.194458
346.615808	13694.274875	29.199476
346.648786	13714.774324	29.204493
347.248542	13736.685578	29.209511
347.235946	13748.776251	29.214528
347.610862	13766.039316	29.219546
348.017396	13795.433471	29.224564
348.084910	13812.807595	29.229581
348.636485	13829.604259	29.234599
349.101180	13860.653704	29.239616
349.569168	13885.333071	29.244634
349.946727	13904.386416	29.249652
349.965931	13929.527297	29.254669
350.845864	13937.939052	29.259687
350.701497	13952.999916	29.264704
351.223334	13981.969032	29.269722
351.455968	14002.901932	29.274740
352.134652	14024.144371	29.279757
352.369396	14042.572702	29.284775
352.563465	14068.482357	29.289792
352.782668	14083.521461	29.294810
353.008580	14106.981921	29.299828
353.746995	14140.237707	29.304845
354.027576	14149.642898	29.309863
354.012912	14180.855920	29.314880
354.623938	14207.468249	29.319898
355.372600	14227.951572	29.324916
355.622001	14256.897203	29.329933
355.822291	14275.511132	29.334951
356.545654	14303.565116	29.339968
356.948594	14313.851380	29.344986
357.211158	14332.108285	29.350004
357.326521	14355.494680	29.355021
358.029552	14364.272078	29.360039
358.121478	14390.213864	29.365056
359.019179	14398.493580	29.370074
359.479119	14415.980855	29.375092
359.970801	14422.230003	29.380109
360.346561	14441.925254	29.385127
360.559027	14452.257037	29.390144
360.977561	14467.129617	29.395162
361.554689	14479.359483	29.400180
361.343713	14497.652373	29.405197
361.682940	14508.839236	29.410215
361.838508	14534.474453	29.415232
362.087433	14550.687261	29.420250
362.686528	14572.305886	29.425268
362.936513	14588.329076	29.430285
363.318357	14606.788742	29.435303
363.569548	14631.963913	29.440320
364.236787	14643.421916	29.445338
364.425360	14664.719270	29.450356
364.521539	14685.800490	29.455373
365.066726	14707.332918	29.460391
365.540638	14741.657321	29.465408
365.470112	14748.625725	29.470426
365.836135	14779.038306	29.475444
366.468935	14801.577271	29.480461
367.072058	14815.811871	29.485479
367.444370	14843.716029	29.490496
367.549390	14854.399520	29.495514
367.961719	14874.433762	29.500532
367.895385	14897.855427	29.505549
368.741769	14921.068705	29.510567
368.927536	14935.782085	29.515584
368.998223	14952.607240	29.520602
369.727447	14963.901038	29.525620
369.973874	14986.629859	29.530637
370.359234	15010.079243	29.535655
371.071585	15037.141209	29.540672
371.542268	15044.338122	29.545690
371.910442	15055.268149	29.550708
371.845803	15080.436235	29.555725
372.381559	15092.821373	29.560743
372.658458	15125.064326	29.565760
373.216067	15144.924644	29.570778
373.535316	15148.788034	29.575796
373.951908	15180.450337	29.580813
374.504442	15193.767750	29.585831
374.496586	15215.860580	29.590848
374.961494	15242.118126	29.595866
375.418238	15256.439008	29.600884
375.455437	15275.148786	29.605901
375.988353	15303.085462	29.610919
376.450669	15329.179305	29.615936
376.949320	15351.345032	29.620954
377.417233	15363.895660	29.625972
377.262221	15393.142845	29.630989
377.608272	15417.078898	29.636007
378.184562	15440.293803	29.641024
378.461607	15467.765239	29.646042
379.080772	15490.676657	29.651060
378.991266	15521.676133	29.656077
379.473881	15538.238706	29.661095
379.978402	15568.811005	29.666112
380.416619	15601.793944	29.671130
380.896431	15630.822647	29.676148
380.853933	15655.817498	29.681165
381.752613	15677.987651	29.686183
382.157378	15703.361407	29.691200
382.564716	15723.804736	29.696218
383.502243	15735.110781	29.701236
383.504658	15771.354873	29.706253
384.103665	15786.648864	29.711271
384.374839	15803.822550	29.716288
384.464104	15817.768380	29.721306
384.885687	15837.571641	29.726324
385.494970	15864.016012	29.731341
385.966784	15882.725047	29.736359
386.422857	15916.002629	29.741376
386.764858	15927.085671	29.746394
387.200418	15941.002946	29.751412
387.597585	15965.964495	29.756429
388.226465	15984.068048	29.761447
388.520139	15992.875193	29.766464
388.412955	16008.683567	29.771482
389.034157	16027.372645	29.776500
389.022607	16053.001177	29.781517
389.897153	16073.833261	29.786535
389.996008	16102.012389	29.791552
390.322890	16131.141461	29.796570
391.210828	16143.402972	29.801588
391.228701	16169.077611	29.806605
391.374377	16189.277924	29.811623
391.756980	16216.617144	29.816640
391.766047	16240.628799	29.821658
392.660384	16260.238881	29.826676
392.926746	16287.703683	29.831693
393.288044	16308.830695	29.836711
393.646335	16335.971735	29.841728
394.090020	16363.867003	29.846746
394.737366	16367.998560	29.851764
395.100248	16399.456474	29.856781
395.117088	16420.987816	29.861799
395.580904	16442.465389	29.866816
396.141261	16464.891265	29.871834
396.492327	16478.866303	29.876852
396.762908	16510.755677	29.881869
397.164219	16526.826422	29.886887
397.722499	16553.630270	29.891904
397.941678	16573.750060	29.896922
398.230011	16594.124411	29.901940
398.805311	16622.874447	29.906957
398.955227	16646.814147	29.911975
399.621317	16672.385386	29.916992
399.744342	16698.710790	29.922010
400.572077	16719.459272	29.927028
401.005726	16751.611077	29.932045
401.370770	16758.853513	29.937063
401.684319	16778.920924	29.942080
401.407600	16815.535762	29.947098
402.357036	16835.978005	29.952116
402.697406	16865.800951	29.957133
403.561013	16896.430014	29.962151
404.242984	16906.977453	29.967168
404.950715	16926.835205	29.972186
405.041270	16932.651751	29.977204
405.359986	16952.465863	29.982221
405.940991	16979.273085	29.987239
406.585903	16993.278556	29.992256
407.041086	17023.083872	29.997274
407.342842	17030.775293	30.002292
407.219801	17057.717499	30.007309
407.719064	17075.182140	30.012327
407.849605	17096.124850	30.017344
408.343043	17118.817747	30.022362
408.935395	17149.934792	30.027380
408.973032	17173.567302	30.032397
409.483046	17194.384713	30.037415
410.218423	17218.957280	30.042432
410.369753	17248.440703	30.047450
410.885039	17270.287053	30.052468
411.186611	17296.136968	30.057485
411.366736	17318.364038	30.062503
411.940878	17336.445807	30.067520
412.255202	17372.132675	30.072538
413.326065	17383.712690	30.077556
413.190475	17413.256826	30.082573
413.607549	17437.282260	30.087591
414.356380	17455.968656	30.092608
414.381133	17488.880233	30.097626
415.155610	17511.754099	30.102644
415.374636	17534.149082	30.107661
415.817211	17556.657742	30.112679
416.368632	17567.519617	30.117696
416.452117	17608.050206	30.122714
417.105877	17625.636590	30.127732
417.266061	17642.352255	30.132749
417.357932	17682.388955	30.137767
418.054693	17704.365476	30.142784
418.583802	17731.592443	30.147802
418.980929	17759.124270	30.152820
418.958949	17788.477569	30.157837
419.651079	17819.513832	30.162855
420.709585	17847.751426	30.167872
420.696745	17873.174111	30.172890
420.837315	17895.066871	30.177908
421.479382	17926.003706	30.182925
421.571422	17950.930053	30.187943
422.270987	17972.040977	30.192960
422.803413	17996.083894	30.197978
423.234611	18007.754395	30.202996
423.545997	18034.365004	30.208013
423.827442	18054.031277	30.213031
424.446173	18080.682544	30.218048
424.514875	18103.237412	30.223066
425.248881	18136.668247	30.228084
425.742290	18159.296043	30.233101
426.175278	18181.964858	30.238119
426.250541	18196.325218	30.243136
426.712744	18222.040812	30.248154
427.114213	18251.846914	30.253172
427.365958	18289.156147	30.258189
427.826579	18317.184275	30.263207
428.722445	18345.428967	30.268224
429.074509	18379.380852	30.273242
429.040651	18413.854050	30.278260
429.989330	18433.088327	30.283277
430.137156	18461.474913	30.288295
430.491476	18487.491940	30.293312
430.954903	18523.416735	30.298330
431.534515	18548.672263	30.303348
432.316909	18582.841797	30.308365
431.948862	18614.177052	30.313383
432.858765	18643.948827	30.318400
433.330647	18679.683071	30.323418
433.607657	18700.753178	30.328436
434.109890	18725.483994	30.333453
434.645351	18759.376406	30.338471
435.068490	18779.722603	30.343488
435.160741	18820.304902	30.348506
435.951500	18854.271451	30.353524
436.673544	18874.230065	30.358541
437.057776	18911.778890	30.363559
437.304160	18937.131024	30.368576
437.799318	18959.967964	30.373594
438.467226	18987.749992	30.378612
439.194310	19013.071614	30.383629
439.602514	19043.812892	30.388647
440.325324	19062.697585	30.393664
440.361378	19096.579887	30.398682
440.889017	19104.167476	30.403700
441.454228	19124.011776	30.408717
441.734864	19153.275804	30.413735
442.309295	19173.750485	30.418752
442.555556	19204.289792	30.423770
443.304997	19221.774288	30.428788
443.906612	19237.159070	30.433805
443.825810	19267.408239	30.438823
444.394226	19285.786499	30.443840
444.473710	19315.284252	30.448858
444.657473	19341.227892	30.453876
445.437197	19375.064399	30.458893
445.455807	19405.279351	30.463911
445.883014	19437.888345	30.468928
446.230155	19470.825747	30.473946
446.719898	19506.040674	30.478964
447.566968	19541.016820	30.483981
447.778102	19578.202176	30.488999
448.221602	19597.731064	30.494016
448.939959	19622.372517	30.499034
449.106702	19659.015288	30.504052
449.527776	19689.338605	30.509069
450.131687	19724.593014	30.514087
450.787830	19743.002275	30.519104
451.345223	19767.188813	30.524122
452.047334	19793.071312	30.529140
452.102907	19809.558732	30.534157
452.316088	19849.303024	30.539175
452.755797	19872.149668	30.544192
453.177276	19884.757864	30.549210
453.711432	19912.802118	30.554228
454.114384	19936.975002	30.559245
454.649301	19968.001273	30.564263
455.490464	19996.440108	30.569280
455.626881	20024.123140	30.574298
456.036534	20051.612043	30.579316
456.731117	20077.161240	30.584333
456.909855	20102.038938	30.589351
457.238780	20125.819232	30.594368
457.678164	20162.193055	30.599386
457.977699	20195.056957	30.604404
458.643368	20215.891293	30.609421
459.225808	20255.370431	30.614439
459.810700	20284.165482	30.619456
460.231435	20308.576144	30.624474
460.282041	20349.787275	30.629492
461.126952	20373.992986	30.634509
461.220160	20409.694585	30.639527
462.524708	20420.200734	30.644544
463.271915	20435.241578	30.649562
463.831754	20462.537091	30.654580
464.571966	20476.580800	30.659597
465.026698	20497.075508	30.664615
465.576328	20516.519296	30.669632
466.072131	20527.290406	30.674650
466.830696	20545.564437	30.679668
467.212413	20542.421888	30.684685
467.250285	20565.401401	30.689703
467.464466	20583.899216	30.694720
468.057907	20612.143744	30.699738
467.769411	20624.357495	30.704756
468.565650	20643.352339	30.709773
468.688351	20671.922963	30.714791
469.316833	20700.364344	30.719808
469.724848	20730.760812	30.724826
470.143373	20768.206780	30.729844
470.622873	20789.967895	30.734861
470.900454	20827.360100	30.739879
471.041832	20865.070536	30.744896
472.079426	20893.075733	30.749914
472.230406	20925.509076	30.754932
472.769341	20959.316317	30.759949
473.192231	20993.615551	30.764967
473.535644	21024.900769	30.769984
474.059681	21059.159099	30.775002
474.407930	21096.844093	30.780020
475.501364	21122.471567	30.785037
475.602796	21161.882095	30.790055
476.099155	21200.087604	30.795072
476.610573	21231.959875	30.800090
476.943458	21273.173228	30.805108
477.884318	21297.598925	30.810125
478.221243	21330.951742	30.815143
478.683294	21352.943659	30.820160
479.162263	21394.450443	30.825178
479.537060	21419.981676	30.830196
480.079457	21451.407193	30.835213
480.435082	21502.215139	30.840231
480.460584	21530.441992	30.845248
481.246962	21562.840653	30.850266
481.389657	21592.578412	30.855284
482.118723	21629.908176	30.860301
482.465421	21660.012341	30.865319
483.353601	21689.368816	30.870336
483.730205	21724.371563	30.875354
484.323571	21753.085314	30.880372
485.401497	21772.991496	30.885389
485.754179	21806.140473	30.890407
486.121362	21818.000147	30.895424
487.062971	21835.235925	30.900442
487.288299	21858.269906	30.905460
487.448009	21870.698986	30.910477
488.099366	21898.727838	30.915495
488.529253	21922.317673	30.920512
488.965469	21952.105059	30.925530
489.042206	21986.712656	30.930548
490.010540	22013.093726	30.935565
490.409809	22040.504892	30.940583
490.450708	22064.938960	30.945600
490.940578	22095.419574	30.950618
491.431992	22129.457376	30.955636
492.348261	22162.070592	30.960653
492.446269	22197.850512	30.965671
492.677326	22227.866131	30.970688
493.335259	22260.563957	30.975706
493.829558	22294.841705	30.980724
494.669724	22336.338473	30.985741
494.967914	22375.013101	30.990759
495.078647	22414.058197	30.995776
495.711548	22455.694900	31.000794
496.029034	22485.779599	31.005812
496.746266	22512.181473	31.010829
497.371441	22552.138797	31.015847
497.585983	22596.557990	31.020864
498.484290	22627.658268	31.025882
499.032958	22663.792231	31.030900
499.736989	22694.120372	31.035917
500.480454	22737.080041	31.040935
500.356991	22772.686957	31.045952
501.396342	22806.286770	31.050970
501.928901	22824.515966	31.055988
502.865991	22850.517573	31.061005
503.223765	22882.119445	31.066023
503.369626	22910.917185	31.071040
504.011658	22941.849332	31.076058
504.396085	22986.792695	31.081076
505.299153	23008.863138	31.086093
505.781744	23036.837734	31.091111
506.401655	23057.600067	31.096128
506.762135	23083.375800	31.101146
506.884872	23113.213737	31.106164
507.580575	23140.327523	31.111181
507.532034	23168.580878	31.116199
508.296632	23207.481512	31.121216
508.817261	23241.251284	31.126234
509.093811	23279.109578	31.131252
509.451061	23321.214387	31.136269
509.883960	23351.522554	31.141287
510.450414	23399.724399	31.146304
511.283809	23438.197720	31.151322
511.664935	23483.559777	31.156340
512.206548	23502.597027	31.161357
512.540314	23545.179895	31.166375
512.840800	23577.821801	31.171392
513.172022	23613.921837	31.176410
513.902714	23656.607447	31.181428
514.560554	23707.639408	31.186445
515.226567	23741.046163	31.191463
515.369540	23780.569181	31.196480
516.078742	23823.820899	31.201498
516.440013	23858.981466	31.206516
516.910605	23894.510547	31.211533
517.539044	23927.007183	31.216551
518.347567	23959.785478	31.221568
518.950736	23988.184987	31.226586
519.519237	24022.706938	31.231604
519.937451	24047.501774	31.236621
520.566026	24072.459789	31.241639
520.973165	24108.049682	31.246656
521.934719	24134.175552	31.251674
522.141324	24163.881942	31.256692
522.563861	24208.544084	31.261709
523.233683	24238.033128	31.266727
523.599842	24272.018276	31.271744
524.226136	24295.561402	31.276762
525.007513	24341.330732	31.281780
525.336205	24362.177682	31.286797
525.915507	24396.351036	31.291815
525.738768	24435.830333	31.296832
526.572815	24466.065110	31.301850
527.193169	24513.724113	31.306868
527.732052	24543.240313	31.311885
528.435128	24575.050213	31.316903
528.639214	24621.169149	31.321920
529.175011	24643.791503	31.326938
529.893259	24693.274646	31.331956
530.465846	24722.261350	31.336973
530.947122	24754.283009	31.341991
531.036047	24810.632546	31.347008
532.042089	24842.610569	31.352026
532.588591	24876.846727	31.357044
533.264568	24914.671223	31.362061
533.500206	24956.848971	31.367079
534.282974	24986.839739	31.372096
535.185270	25021.886532	31.377114
535.497920	25057.277961	31.382132
536.104579	25098.311286	31.387149
536.868892	25127.515194	31.392167
536.942194	25164.966337	31.397184
537.599093	25197.043518	31.402202
538.275253	25243.539088	31.407220
538.738604	25266.230301	31.412237
539.776253	25306.444924	31.417255
539.984048	25347.957949	31.422272
540.527368	25379.174674	31.427290
540.938561	25416.820151	31.432308
541.457517	25447.478326	31.437325
542.281518	25479.725856	31.442343
542.804341	25523.446327	31.447360
543.196441	25542.919583	31.452378
543.393305	25582.728475	31.457396
543.615321	25623.885953	31.462413
544.556401	25650.895440	31.467431
545.001862	25694.824239	31.472448
545.472676	25738.629112	31.477466
546.116338	25777.092242	31.482484
546.489473	25823.149705	31.487501
547.451818	25859.528411	31.492519
547.662421	25900.587113	31.497536
548.376348	25933.351774	31.502554
549.296990	25958.203478	31.507572
549.541671	26002.271643	31.512589
550.406485	26038.912330	31.517607
550.844148	26067.814548	31.522624
551.409428	26100.615262	31.527642
551.950329	26136.522888	31.532660
552.834422	26169.779674	31.537677
553.411199	26193.743537	31.542695
553.989368	26220.500613	31.547712
554.753892	26246.426084	31.552730
555.041554	26278.063201	31.557748
555.161973	26306.819231	31.562765
555.949968	26327.179606	31.567783
556.241371	26359.271304	31.572800
556.699947	26393.100299	31.577818
557.188482	26428.100203	31.582836
557.600400	26462.442175	31.587853
558.257388	26490.198538	31.592871
558.437582	26518.155564	31.597888
559.000118	26561.846828	31.602906
559.904051	26597.287959	31.607924
559.970613	26637.953465	31.612941
560.615610	26669.131083	31.617959
560.865378	26725.562061	31.622976
561.480997	26767.918293	31.627994
562.247359	26805.447874	31.633012
562.790515	26853.200287	31.638029
563.243137	26896.612341	31.643047
563.813129	26941.927538	31.648064
564.905824	26984.216274	31.653082
565.305360	27028.565938	31.658100
565.674097	27075.998420	31.663117
566.602161	27112.327845	31.668135
567.348497	27162.514232	31.673152
567.995622	27208.778690	31.678170
568.471269	27245.608560	31.683188
568.884666	27284.116731	31.688205
569.346112	27321.056392	31.693223
570.037849	27362.567746	31.698240
570.894525	27402.814732	31.703258
571.209296	27436.231759	31.708276
571.871581	27484.144083	31.713293
572.640211	27521.510312	31.718311
573.020323	27567.014475	31.723328
573.843383	27597.135591	31.728346
574.808371	27631.722106	31.733364
575.011244	27665.156931	31.738381
575.594313	27700.896442	31.743399
576.467053	27747.221813	31.748416
576.512199	27781.003721	31.753434
577.307405	27810.484810	31.758452
578.045687	27842.781069	31.763469
579.131588	27878.246682	31.768487
579.333253	27906.176998	31.773504
580.200689	27936.348594	31.778522
581.267042	27964.201264	31.783540
581.614366	28000.932393	31.788557
582.455580	28014.757147	31.793575
583.232851	28043.716768	31.798592
583.296473	28075.492697	31.803610
584.054761	28102.337994	31.808628
584.449229	28129.037706	31.813645
584.869224	28157.850853	31.818663
585.455877	28182.624564	31.823680
586.058387	28208.059492	31.828698
586.415528	28250.041904	31.833716
586.929172	28283.644264	31.838733
587.470659	28320.946197	31.843751
587.771635	28357.571414	31.848768
588.045215	28401.615014	31.853786
589.232569	28443.948948	31.858804
589.706970	28483.379024	31.863821
590.647307	28505.260112	31.868839
590.956595	28548.426224	31.873856
591.070845	28595.358294	31.878874
592.268378	28618.229731	31.883892
592.358090	28657.859085	31.888909
593.051035	28690.479782	31.893927
593.832013	28714.041922	31.898944
594.354723	28737.056469	31.903962
595.005855	28767.136559	31.908980
595.624768	28807.846831	31.913997
596.174408	28829.536261	31.919015
596.486483	28872.076871	31.924032
596.717542	28908.574905	31.929050
597.501792	28942.559716	31.934068
598.127466	28995.063847	31.939085
598.545636	29029.731548	31.944103
599.055249	29068.891801	31.949120
599.553337	29114.595961	31.954138
600.321776	29146.137418	31.959156
600.795967	29197.407807	31.964173
601.609165	29248.783571	31.969191
601.844248	29294.396338	31.974208
602.369159	29332.992157	31.979226
602.903620	29378.861909	31.984244
603.817566	29441.650651	31.989261
604.482772	29488.669664	31.994279
604.790883	29527.805274	31.999296
605.608608	29581.096412	32.004314
606.240411	29622.040173	32.009332
606.520044	29675.257297	32.014349
607.572627	29721.299997	32.019367
608.092223	29769.701336	32.024384
608.779139	29818.999612	32.029402
609.629515	29865.339597	32.034420
610.059763	29912.351910	32.039437
610.404652	29962.854209	32.044455
611.333920	30008.151899	32.049472
611.711576	30061.089277	32.054490
612.624630	30109.240533	32.059508
613.026415	30158.520800	32.064525
613.973112	30202.646796	32.069543
614.530046	30247.807023	32.074560
615.040281	30303.176994	32.079578
615.671169	30336.796080	32.084596
616.222747	30392.033431	32.089613
617.104249	30429.577049	32.094631
617.734943	30470.244540	32.099648
618.576044	30521.492721	32.104666
619.365744	30559.126722	32.109684
620.029538	30609.941274	32.114701
620.777266	30631.614418	32.119719
621.492003	30672.749642	32.124736
622.312962	30708.141314	32.129754
622.979854	30736.913332	32.134772
623.462788	30784.323998	32.139789
624.173149	30811.072851	32.144807
624.402954	30851.436864	32.149824
624.972771	30886.760476	32.154842
625.791710	30925.149157	32.159860
626.182565	30974.692252	32.164877
626.501598	31015.858154	32.169895
627.395421	31055.872663	32.174912
627.645102	31107.739046	32.179930
628.164452	31146.452919	32.184948
628.737651	31197.333592	32.189965
629.423837	31242.027051	32.194983
630.113810	31293.730536	32.200000
630.394822	31332.475539	32.205018
631.384393	31389.663931	32.210036
631.718019	31453.769200	32.215053
632.310078	31493.755675	32.220071
632.877658	31541.749124	32.225088
633.610078	31601.430896	32.230106
634.191247	31644.339923	32.235124
635.002136	31697.410021	32.240141
635.525101	31737.085319	32.245159
636.196533	31771.452702	32.250176
636.820625	31824.381520	32.255194
638.015989	31862.890349	32.260212
638.482221	31895.753721	32.265229
638.986184	31941.716103	32.270247
639.457046	31974.970823	32.275264
639.888199	32027.177912	32.280282
640.945810	32068.901029	32.285300
641.597954	32111.648254	32.290317
642.467134	32157.990459	32.295335
643.282523	32190.338456	32.300352
643.650833	32234.868600	32.305370
644.398656	32260.614659	32.310388
645.269055	32297.682947	32.315405
645.811038	32345.056382	32.320423
646.811374	32372.729350	32.325440
646.854634	32416.760488	32.330458
647.956148	32451.814343	32.335476
648.659060	32498.151582	32.340493
649.070763	32538.692859	32.345511
650.011223	32574.214523	32.350528
650.702216	32613.094069	32.355546
651.493154	32647.450621	32.360564
651.756190	32699.483268	32.365581
651.939941	32737.240847	32.370599
652.881103	32782.536444	32.375616
653.613588	32824.020884	32.380634
653.827362	32865.428105	32.385652
654.656628	32917.727179	32.390669
655.482455	32960.398534	32.395687
655.883256	33010.336898	32.400704
656.565743	33054.263548	32.405722
657.308373	33100.791926	32.410740
657.782591	33162.813269	32.415757
658.415289	33216.262693	32.420775
659.388632	33261.598576	32.425792
659.833669	33312.510697	32.430810
660.847365	33353.288592	32.435828
661.396764	33405.006566	32.440845
661.850949	33450.929448	32.445863
662.899637	33502.810179	32.450880
663.116684	33554.207252	32.455898
664.020273	33597.556919	32.460916
664.539346	33654.616149	32.465933
665.256065	33705.632343	32.470951
666.394236	33748.440028	32.475968
666.609293	33800.394370	32.480986
667.308726	33843.751039	32.486004
668.463006	33893.827105	32.491021
668.708064	33937.684615	32.496039
669.486669	33988.280915	32.501056
670.321758	34031.218550	32.506074
671.142457	34069.486318	32.511092
671.624330	34116.272504	32.516109
672.255361	34164.141986	32.521127
673.032285	34210.623236	32.526144
673.570343	34256.787720	32.531162
674.553614	34305.159059	32.536180
674.742191	34349.184280	32.541197
675.572422	34390.732478	32.546215
676.055383	34433.219957	32.551232
676.566496	34499.191025	32.556250
677.523545	34538.911553	32.561268
678.406851	34585.219009	32.566285
678.713147	34630.168541	32.571303
679.657943	34670.397024	32.576320
680.450529	34708.777816	32.581338
680.893886	34749.425926	32.586356
681.499668	34784.586159	32.591373
682.092731	34836.180731	32.596391
683.104555	34867.857395	32.601408
683.352101	34910.641710	32.606426
684.097524	34956.946158	32.611444
684.549406	35011.231267	32.616461
684.771003	35056.156956	32.621479
685.657571	35098.367978	32.626496
686.170175	35157.335401	32.631514
686.896068	35216.984246	32.636532
687.882627	35269.859027	32.641549
688.327703	35319.973021	32.646567
689.103028	35376.864251	32.651584
689.763492	35438.913892	32.656602
690.153052	35488.107485	32.661620
691.259666	35539.421502	32.666637
691.845067	35611.764146	32.671655
693.247089	35651.411180	32.676672
693.400552	35707.363165	32.681690
694.444798	35768.481482	32.686708
695.296470	35819.658826	32.691725
695.684219	35870.137125	32.696743
696.563160	35918.054191	32.701760
697.259591	35976.647521	32.706778
697.818143	36029.584506	32.711796
698.694066	36070.686295	32.716813
699.251515	36131.628522	32.721831
700.063166	36172.803744	32.726848
700.864171	36234.416521	32.731866
701.559687	36271.708744	32.736884
702.636019	36327.733682	32.741901
703.034044	36388.366343	32.746919
703.999622	36439.400991	32.751936
704.991142	36485.107723	32.756954
705.685589	36523.924408	32.761972
706.419509	36567.028380	32.766989
707.204862	36606.159863	32.772007
707.540178	36660.309263	32.777024
708.805695	36700.984886	32.782042
709.019241	36746.199944	32.787060
709.727342	36791.628975	32.792077
710.060597	36853.771627	32.797095
710.984699	36898.806843	32.802112
711.952290	36945.896739	32.807130
712.353469	36990.608868	32.812148
712.988474	37046.040465	32.817165
713.409653	37103.313933	32.822183
714.309034	37145.697764	32.827200
715.140374	37198.677394	32.832218
715.865090	37256.188567	32.837236
716.904921	37307.725923	32.842253
717.233926	37366.595267	32.847271
717.905451	37418.095373	32.852288
718.775991	37468.647740	32.857306
719.255982	37529.960129	32.862324
720.291319	37579.152876	32.867341
721.302162	37625.643144	32.872359
722.127777	37666.110862	32.877376
723.142124	37705.398417	32.882394
723.386141	37758.142045	32.887412
724.331221	37807.690834	32.892429
725.118061	37850.220052	32.897447
725.426460	37893.911468	32.902464
726.615369	37941.089253	32.907482
726.895556	37996.799869	32.912500
727.996358	38026.488151	32.917517
727.980907	38076.870025	32.922535
729.050055	38107.233639	32.927552
729.752888	38148.334764	32.932570
730.139904	38193.993818	32.937588
731.204977	38231.244585	32.942605
731.798980	38293.293911	32.947623
732.465402	38334.293560	32.952640
733.036899	38379.361491	32.957658
733.614925	38436.044980	32.962676
734.646873	38482.091169	32.967693
734.922204	38537.886150	32.972711
735.708019	38579.335630	32.977728
736.731055	38636.791422	32.982746
737.272018	38705.407846	32.987764
737.751327	38751.875798	32.992781
738.499741	38809.368476	32.997799
739.323050	38870.258147	33.002816
740.192895	38931.197660	33.007834
741.170250	38983.520270	33.012852
741.792846	39039.509118	33.017869
742.018572	39107.859706	33.022887
743.143040	39162.480689	33.027904
743.939082	39223.451488	33.032922
744.291472	39280.064816	33.037940
744.981467	39330.864684	33.042957
745.658082	39396.844103	33.047975
746.748897	39460.457341	33.052992
747.423511	39524.015400	33.058010
748.288116	39592.508375	33.063028
749.490988	39648.737317	33.068045
750.110941	39708.351945	33.073063
751.128785	39766.051864	33.078080
752.084091	39817.956221	33.083098
752.816633	39877.699241	33.088116
753.570255	39923.608439	33.093133
754.288578	39979.186403	33.098151
755.084245	40030.275018	33.103168
755.955081	40084.659556	33.108186
756.649233	40142.252764	33.113204
757.334945	40186.263207	33.118221
758.440994	40239.713492	33.123239
758.953308	40285.509241	33.128256
760.157589	40335.194245	33.133274
761.088248	40386.705379	33.138292
761.330001	40434.213144	33.143309
762.138916	40491.909574	33.148327
762.998880	40541.926917	33.153344
764.055469	40575.489706	33.158362
764.595356	40634.834752	33.163380
765.826478	40674.682136	33.168397
766.321258	40728.551318	33.173415
767.120134	40773.753275	33.178432
767.652433	40819.110660	33.183450
768.525084	40870.840673	33.188468
769.136242	40911.265649	33.193485
769.885038	40962.667322	33.198503
770.757486	41016.111612	33.203520
771.610561	41063.677372	33.208538
771.907990	41123.459927	33.213556
772.684361	41170.803858	33.218573
773.556130	41219.195546	33.223591
774.229314	41277.655145	33.228608
774.840411	41327.681411	33.233626
775.829556	41387.255820	33.238644
776.446059	41432.917597	33.243661
777.300893	41501.481353	33.248679
777.903174	41543.837858	33.253696
778.662282	41587.561430	33.258714
779.326801	41653.517957	33.263732
780.323845	41699.487878	33.268749
780.797336	41754.811231	33.273767
781.281282	41803.391075	33.278784
782.305156	41869.969047	33.283802
782.572408	41921.473235	33.288820
783.554217	41981.208519	33.293837
784.448437	42041.020847	33.298855
785.127951	42096.344614	33.303872
785.102353	42150.285655	33.308890
785.889998	42215.535315	33.313908
787.509005	42280.769598	33.318925
788.379538	42341.642664	33.323943
789.557186	42401.190487	33.328960
790.739655	42451.541486	33.333978
791.422996	42520.717006	33.338996
792.074643	42557.141445	33.344013
792.888704	42618.549029	33.349031
793.571414	42670.116794	33.354048
794.703135	42718.572527	33.359066
795.464363	42782.227793	33.364084
795.855744	42841.323641	33.369101
796.742914	42892.607105	33.374119
797.544297	42954.517267	33.379136
799.057895	43009.289723	33.384154
799.736686	43072.604463	33.389172
800.166040	43112.859402	33.394189
801.003435	43171.450283	33.399207
801.493084	43227.616049	33.404224
802.241980	43293.671888	33.409242
802.967099	43353.204182	33.414260
804.128856	43406.944489	33.419277
804.792117	43476.031256	33.424295
805.586810	43544.092088	33.429312
806.435891	43597.388175	33.434330
807.143157	43660.466138	33.439348
807.884583	43721.761597	33.444365
808.689066	43785.722954	33.449383
809.444917	43856.384110	33.454400
810.834236	43912.658249	33.459418
811.072437	43978.137808	33.464436
812.010169	44036.184043	33.469453
813.068934	44089.119760	33.474471
813.882117	44149.462770	33.479488
814.912006	44215.528220	33.484506
815.557824	44277.940700	33.489524
816.675112	44338.357065	33.494541
817.444715	44388.877961	33.499559
817.943074	44452.180456	33.504576
818.847140	44500.359269	33.509594
819.726663	44574.450786	33.514612
820.660185	44636.281828	33.519629
821.401535	44699.983655	33.524647
821.642788	44760.676696	33.529664
822.959687	44822.885034	33.534682
823.384207	44883.220956	33.539700
824.258966	44950.571509	33.544717
825.349326	45022.879535	33.549735
825.800078	45082.275737	33.554752
826.931681	45133.501036	33.559770
827.743206	45196.421641	33.564788
828.762887	45268.033002	33.569805
829.547614	45325.752187	33.574823
830.390792	45388.067472	33.579840
831.721813	45442.330365	33.584858
832.379748	45511.108001	33.589876
833.160324	45561.275612	33.594893
833.892229	45611.343374	33.599911
834.802709	45662.730824	33.604928
835.458792	45708.616671	33.609946
836.082846	45765.761061	33.614964
836.972807	45813.989190	33.619981
837.473616	45856.186302	33.624999
838.103826	45922.926301	33.630016
838.871386	45977.708358	33.635034
839.678586	46045.091703	33.640052
840.407410	46106.092044	33.645069
841.192496	46172.637881	33.650087
842.081596	46238.092327	33.655104
842.877368	46295.730057	33.660122
843.835680	46378.190747	33.665140
844.452365	46451.848632	33.670157
845.313841	46503.460719	33.675175
846.266146	46597.531240	33.680192
847.274005	46653.492123	33.685210
848.543517	46717.667836	33.690228
849.481741	46793.566796	33.695245
850.526278	46854.773064	33.700263
851.367033	46916.112437	33.705280
852.617977	46967.677615	33.710298
852.996576	47028.115021	33.715316
853.752840	47088.867038	33.720333
855.091267	47149.686750	33.725351
855.538873	47218.957834	33.730368
856.598286	47279.245650	33.735386
857.267705	47343.693692	33.740404
858.029605	47412.530548	33.745421
859.061463	47476.005251	33.750439
859.706540	47539.350554	33.755456
860.662120	47603.406849	33.760474
861.402916	47680.560488	33.765492
862.059172	47753.337109	33.770509
863.196117	47817.928818	33.775527
863.580154	47886.427378	33.780544
864.623936	47963.471553	33.785562
865.244250	48039.455816	33.790580
866.490133	48109.484723	33.795597
867.439007	48181.869218	33.800615
868.052218	48246.746120	33.805632
869.070760	48327.945593	33.810650
869.966877	48407.114639	33.815668
870.672593	48479.790992	33.820685
871.543308	48549.664557	33.825703
872.494499	48626.054783	33.830720
873.434273	48703.389698	33.835738
874.457621	48769.456903	33.840756
875.811327	48849.391364	33.845773
876.583211	48910.867062	33.850791
877.385527	48979.329107	33.855808
878.157980	49055.565123	33.860826
879.136302	49119.843587	33.865844
879.846473	49192.698666	33.870861
881.229049	49250.613195	33.875879
881.982620	49322.993758	33.880896
882.859542	49391.723801	33.885914
883.716949	49448.822186	33.890932
884.387492	49515.515879	33.895949
885.397044	49579.234018	33.900967
886.128821	49648.860524	33.905984
887.072069	49716.809349	33.911002
888.045246	49786.746673	33.916020
888.936658	49856.614689	33.921037
889.664051	49914.854330	33.926055
890.652358	49987.624355	33.931072
891.660345	50061.410182	33.936090
892.210048	50123.777860	33.941108
893.261720	50180.639040	33.946125
894.383197	50239.185124	33.951143
894.824583	50301.766282	33.956160
895.684142	50353.811324	33.961178
896.710111	50418.313788	33.966196
897.070670	50492.258723	33.971213
897.844276	50546.601643	33.976231
898.633702	50621.701355	33.981248
899.668540	50695.554636	33.986266
900.327261	50765.822282	33.991284
901.283056	50845.325807	33.996301
902.210611	50920.335393	34.001319
903.032962	51005.206690	34.006336
903.751498	51076.547920	34.011354
904.889612	51149.184408	34.016372
905.726871	51231.751109	34.021389
906.774184	51315.519224	34.026407
907.945746	51386.575764	34.031424
908.898503	51462.355115	34.036442
909.930256	51536.907572	34.041460
910.758287	51618.648210	34.046477
911.999975	51686.505772	34.051495
912.540742	51766.867991	34.056512
914.160911	51836.672860	34.061530
915.251278	51892.836226	34.066548
915.901785	51974.061592	34.071565
916.772297	52043.907850	34.076583
917.812268	52117.144781	34.081600
918.890445	52184.415488	34.086618
919.999274	52247.087838	34.091636
920.544372	52323.990158	34.096653
921.649865	52391.636865	34.101671
922.658809	52455.255476	34.106688
923.374416	52532.606511	34.111706
924.341653	52600.199415	34.116724
925.396413	52670.999656	34.121741
926.581164	52733.092011	34.126759
927.443697	52814.698604	34.131776
927.975712	52882.163915	34.136794
928.921860	52944.306630	34.141812
929.629755	53015.225187	34.146829
930.699863	53082.018836	34.151847
932.244947	53160.135046	34.156864
932.989121	53230.251311	34.161882
934.181831	53302.721514	34.166900
934.986948	53374.670117	34.171917
935.973586	53428.062763	34.176935
936.716848	53503.900357	34.181952
937.513558	53575.502853	34.186970
938.915435	53633.457011	34.191988
939.520094	53707.753850	34.197005
940.415431	53776.278896	34.202023
941.757238	53853.473547	34.207040
942.322660	53924.651171	34.212058
943.384891	53982.431256	34.217076
944.390708	54056.831282	34.222093
945.251382	54121.705144	34.227111
945.870694	54198.956443	34.232128
947.017935	54267.595585	34.237146
947.850538	54334.512040	34.242164
948.722334	54410.680599	34.247181
949.793819	54483.527695	34.252199
950.820155	54558.628536	34.257216
951.514152	54632.167667	34.262234
952.532126	54699.094272	34.267252
953.537981	54775.236813	34.272269
954.720913	54836.594627	34.277287
955.554356	54906.195740	34.282304
956.194150	54980.782225	34.287322
957.252847	55034.616612	34.292340
957.952900	55109.409285	34.297357
959.099792	55161.711444	34.302375
960.473582	55224.179652	34.307392
960.905094	55283.206534	34.312410
962.607757	55337.485608	34.317428
963.184086	55401.584567	34.322445
964.020973	55458.359169	34.327463
965.038063	55532.344421	34.332480
965.974804	55605.943722	34.337498
967.137809	55670.793766	34.342516
967.733930	55743.022613	34.347533
968.428683	55816.894389	34.352551
969.513925	55884.364455	34.357568
970.068607	55977.623743	34.362586
970.981476	56048.323339	34.367604
972.045254	56133.403460	34.372621
972.930037	56219.480022	34.377639
974.099706	56292.570547	34.382656
975.045930	56380.802511	34.387674
975.936558	56454.360987	34.392692
976.742810	56550.178102	34.397709
977.816652	56623.360503	34.402727
979.025433	56711.514849	34.407744
979.603547	56811.672053	34.412762
980.709354	56884.970526	34.417780
982.166437	56970.631617	34.422797
982.715143	57054.440840	34.427815
983.923276	57135.363025	34.432832
984.875964	57222.369299	34.437850
986.226932	57306.364636	34.442868
987.340894	57398.232336	34.447885
988.123484	57479.177620	34.452903
989.402766	57559.653468	34.457920
989.783597	57641.554218	34.462938
991.348185	57712.992717	34.467956
992.301595	57811.950135	34.472973
993.019221	57889.242419	34.477991
994.207847	57973.651434	34.483008
995.148927	58060.346099	34.488026
996.403948	58135.732751	34.493044
997.272385	58221.224117	34.498061
998.216495	58299.741958	34.503079
999.462312	58381.118174	34.508096
1000.407976	58477.174448	34.513114
1001.931408	58534.855831	34.518132
1003.135240	58613.884907	34.523149
1003.992513	58686.531353	34.528167
1005.167064	58763.135049	34.533184
1006.291596	58829.790824	34.538202
1007.620885	58902.883448	34.543220
1008.622988	58971.653668	34.548237
1009.412437	59029.178325	34.553255
1010.566678	59102.210188	34.558272
1011.258708	59181.852453	34.563290
1012.286462	59254.790537	34.568308
1013.106729	59325.906623	34.573325
1013.936301	59398.186082	34.578343
1015.190774	59463.316974	34.583360
1015.660808	59554.704482	34.588378
1016.643875	59637.138537	34.593396
1017.507652	59725.262678	34.598413
1018.587604	59796.573911	34.603431
1019.973436	59865.040082	34.608448
1021.078664	59958.020220	34.613466
1021.853849	60020.113063	34.618484
1022.740520	60090.429851	34.623501
1023.299686	60162.589104	34.628519
1024.950742	60241.699452	34.633536
1025.513752	60308.763179	34.638554
1026.687976	60377.263729	34.643572
1027.867096	60454.036622	34.648589
1028.519147	60526.961046	34.653607
1029.890112	60604.248903	34.658624
1030.470063	60678.716799	34.663642
1031.598605	60761.290255	34.668660
1032.621905	60842.070050	34.673677
1033.503195	60918.093205	34.678695
1034.675560	60994.280173	34.683712
1035.243216	61088.639578	34.688730
1036.377626	61168.561283	34.693748
1037.772203	61246.442503	34.698765
1038.393164	61325.748354	34.703783
1039.693710	61412.082521	34.708800
1040.552912	61499.257948	34.713818
1041.887753	61585.365838	34.718836
1043.017197	61679.595754	34.723853
1043.706592	61767.760725	34.728871
1044.908088	61859.732954	34.733888
1045.788388	61941.291901	34.738906
1046.994524	62032.605724	34.743924
1048.390063	62126.770611	34.748941
1049.122785	62221.583423	34.753959
1050.549015	62303.394087	34.758976
1051.349143	62395.785280	34.763994
1052.413011	62473.437001	34.769012
1053.565380	62571.800388	34.774029
1054.624167	62660.069301	34.779047
1055.805796	62742.489215	34.784064
1056.887216	62845.257949	34.789082
1058.022597	62926.508237	34.794100
1059.109953	63024.307480	34.799117
1060.496309	63100.056175	34.804135
1061.519788	63197.555854	34.809152
1062.699092	63276.977299	34.814170
1063.855245	63360.593352	34.819188
1064.801564	63440.526367	34.824205
1065.625437	63525.524094	34.829223
1067.129296	63602.332213	34.834240
1067.981741	63692.529735	34.839258
1069.022881	63771.125973	34.844276
1070.366882	63854.790413	34.849293
1071.166505	63951.802454	34.854311
1072.607690	64025.525975	34.859328
1073.383627	64109.324006	34.864346
1074.437587	64184.260446	34.869364
1075.666862	64273.508789	34.874381
1076.706450	64365.179980	34.879399
1077.762007	64437.388400	34.884416
1079.127606	64531.282180	34.889434
1080.227634	64607.852378	34.894452
1081.279753	64687.836226	34.899469
1082.197898	64774.431544	34.904487
1083.339394	64857.940938	34.909504
1084.370709	64942.600982	34.914522
1085.248409	65019.846460	34.919540
1086.400230	65105.957056	34.924557
1087.486391	65196.161601	34.929575
1088.626697	65276.956616	34.934592
1089.788183	65370.429480	34.939610
1091.008238	65455.536693	34.944628
1091.844025	65531.986234	34.949645
1092.479049	65620.502506	34.954663
1093.909344	65713.751202	34.959680
1095.291064	65775.637433	34.964698
1095.979264	65846.381300	34.969716
1096.970843	65920.376638	34.974733
1098.262187	65996.262851	34.979751
1099.188576	66069.116511	34.984768
1100.385038	66154.672933	34.989786
1101.102130	66227.426673	34.994804
1102.302202	66307.076074	34.999821
1103.398752	66398.182325	35.004839
1104.383110	66482.829522	35.009856
1105.514388	66562.110559	35.014874
1106.263272	66650.422772	35.019892
1107.771951	66724.681859	35.024909
1108.580285	66827.382783	35.029927
1110.448923	66909.601824	35.034944
1111.504131	66995.784547	35.039962
1112.583127	67079.545275	35.044980
1113.584468	67162.564929	35.049997
1114.677395	67250.730702	35.055015
1116.021400	67329.018644	35.060032
1117.025116	67419.794778	35.065050
1117.843802	67518.210478	35.070068
1119.287009	67603.644730	35.075085
1120.258401	67701.923401	35.080103
1121.182214	67789.604505	35.085120
1122.365290	67868.248392	35.090138
1123.501302	67979.121325	35.095156
1124.661916	68066.601898	35.100173
1125.779484	68173.116056	35.105191
1126.847460	68251.994313	35.110208
1128.261925	68355.924020	35.115226
1129.212325	68458.444760	35.120244
1130.296333	68542.272816	35.125261
1131.525680	68629.959890	35.130279
1132.650042	68722.108513	35.135296
1133.926658	68815.468469	35.140314
1134.971489	68918.799480	35.145332
1136.651824	69008.367848	35.150349
1137.559166	69102.926059	35.155367
1138.929829	69199.597002	35.160384
1139.969571	69286.074771	35.165402
1141.094424	69375.623236	35.170420
1142.148978	69472.490040	35.175437
1143.273804	69568.567434	35.180455
1144.654792	69659.292755	35.185472
1145.760559	69748.370581	35.190490
1146.819729	69831.757120	35.195508
1147.998810	69924.731017	35.200525
1149.357268	70010.705689	35.205543
1150.653629	70101.350749	35.210560
1152.000897	70195.122612	35.215578
1153.269053	70279.864800	35.220596
1154.162749	70366.185275	35.225613
1155.246278	70455.990861	35.230631
1156.256462	70548.011788	35.235648
1157.184888	70633.276593	35.240666
1158.182619	70727.003465	35.245684
1159.742696	70821.415681	35.250701
1160.620399	70914.845296	35.255719
1162.074651	71008.514784	35.260736
1163.231706	71095.847851	35.265754
1164.088345	71189.724993	35.270772
1165.720029	71278.631211	35.275789
1166.489987	71383.768891	35.280807
1167.486484	71475.763556	35.285824
1168.580792	71566.096875	35.290842
1169.593054	71670.020148	35.295860
1170.874685	71761.160872	35.300877
1171.647498	71846.010576	35.305895
1172.881424	71936.260113	35.310912
1174.299647	72020.895935	35.315930
1175.005915	72108.986463	35.320948
1176.016166	72205.819653	35.325965
1177.175453	72298.323800	35.330983
1178.613997	72393.989136	35.336000
1179.943263	72478.576951	35.341018
1181.128032	72569.621565	35.346036
1182.762883	72650.337407	35.351053
1184.099976	72745.133226	35.356071
1184.732758	72842.217491	35.361088
1186.100658	72933.057535	35.366106
1187.031285	73026.258437	35.371124
1188.591665	73110.647650	35.376141
1189.909975	73204.814758	35.381159
1191.038500	73300.949604	35.386176
1192.271254	73380.463687	35.391194
1193.125448	73483.798083	35.396212
1194.801289	73583.382537	35.401229
1195.683565	73680.038391	35.406247
1196.832601	73774.791171	35.411264
1198.470036	73870.392890	35.416282
1199.721196	73965.662428	35.421300
1200.700018	74063.254603	35.426317
1201.902450	74165.688811	35.431335
1203.011718	74265.642665	35.436352
1203.994884	74361.892635	35.441370
1205.109842	74466.836872	35.446388
1206.746385	74552.320780	35.451405
1207.934931	74654.214369	35.456423
1209.280395	74753.702626	35.461440
1210.949575	74843.235654	35.466458
1211.897132	74944.547201	35.471476
1212.915899	75035.930097	35.476493
1214.583126	75132.443693	35.481511
1215.856411	75230.133624	35.486528
1217.162956	75316.380672	35.491546
1218.218088	75420.691953	35.496564
1219.836721	75500.063620	35.501581
1220.945446	75602.606577	35.506599
1222.122377	75692.206392	35.511616
1223.639617	75784.730269	35.516634
1224.626908	75868.216716	35.521652
1225.481354	75962.744418	35.526669
1226.736899	76065.088943	35.531687
1227.659778	76156.123222	35.536704
1229.288930	76256.776260	35.541722
1229.883652	76360.174799	35.546740
1231.288512	76458.190715	35.551757
1232.654763	76559.886517	35.556775
1233.728467	76673.256877	35.561792
1234.920184	76767.000183	35.566810
1236.296704	76877.461426	35.571828
1237.530193	76981.902979	35.576845
1238.686629	77076.564906	35.581863
1239.632145	77192.136202	35.586880
1240.959672	77290.091155	35.591898
1242.463922	77399.001849	35.596916
1243.363766	77507.437007	35.601933
1244.647278	77613.887371	35.606951
1246.160347	77719.415669	35.611968
1247.634240	77818.565851	35.616986
1248.950805	77919.628406	35.622004
1250.206177	78017.470521	35.627021
1251.351668	78119.979258	35.632039
1252.799477	78218.032830	35.637056
1254.732704	78302.963027	35.642074
1255.288091	78398.723873	35.647092
1256.014327	78472.884505	35.652109
1257.513092	78562.456352	35.657127
1258.111130	78665.863109	35.662144
1259.360954	78755.563012	35.667162
1260.623953	78857.650827	35.672180
1262.081919	78963.496533	35.677197
1263.312775	79049.450492	35.682215
1264.517317	79155.349049	35.687232
1266.033793	79238.890130	35.692250
1267.162431	79343.458358	35.697268
1268.633645	79452.597715	35.702285
1270.058270	79551.242405	35.707303
1270.941748	79648.793485	35.712320
1272.429391	79748.797294	35.717338
1273.547138	79842.524625	35.722356
1274.836515	79946.259305	35.727373
1275.983916	80054.285900	35.732391
1277.106990	80164.508435	35.737408
1279.052601	80264.316130	35.742426
1279.917565	80374.883731	35.747444
1281.172717	80480.462749	35.752461
1282.792721	80588.278497	35.757479
1283.864095	80698.283147	35.762496
1285.463075	80792.255506	35.767514
1286.685442	80901.515308	35.772532
1287.987675	81010.269001	35.777549
1289.488928	81112.581420	35.782567
1290.803510	81219.484272	35.787584
1292.348834	81318.040425	35.792602
1293.434483	81424.561601	35.797620
1294.828297	81527.538407	35.802637
1296.356271	81632.027735	35.807655
1297.320965	81744.257620	35.812672
1298.878144	81844.600206	35.817690
1299.952497	81958.296235	35.822708
1301.639020	82062.927196	35.827725
1302.794066	82161.585068	35.832743
1304.130433	82268.995321	35.837760
1305.296455	82370.692999	35.842778
1306.714471	82480.954764	35.847796
1307.698436	82585.304247	35.852813
1309.467307	82685.895622	35.857831
1310.626668	82792.803274	35.862848
1311.945345	82896.975107	35.867866
1312.803138	82999.812663	35.872884
1314.097612	83120.143660	35.877901
1316.011804	83227.163527	35.882919
1317.237633	83344.097834	35.887936
1318.472884	83443.495247	35.892954
1319.934932	83548.952215	35.897972
1320.944885	83666.884409	35.902989
1322.289670	83774.501787	35.908007
1323.618622	83881.095715	35.913024
1325.051480	83997.240242	35.918042
1326.160027	84111.281694	35.923060
1327.436167	84227.147451	35.928077
1328.925229	84333.806843	35.933095
1330.174316	84444.850101	35.938112
1331.728111	84549.916362	35.943130
1332.726275	84669.172303	35.948148
1334.447598	84778.382083	35.953165
1335.749675	84881.651438	35.958183
1337.366338	84990.624894	35.963200
1338.552362	85090.605898	35.968218
1340.210474	85197.216847	35.973236
1341.519549	85295.608179	35.978253
1342.975641	85393.964292	35.983271
1344.574534	85485.658725	35.988288
1345.685827	85573.349157	35.993306
1347.049877	85665.169414	35.998324
1348.105006	85758.039093	36.003341
1349.407470	85839.630943	36.008359
1350.363645	85937.167043	36.013376
1351.810675	86034.411653	36.018394
1352.802360	86140.584938	36.023412
1354.144841	86232.600429	36.028429
1355.501062	86341.492807	36.033447
1356.211483	86442.034041	36.038464
1357.835909	86547.451396	36.043482
1359.387078	86660.369608	36.048500
1360.353652	86775.520804	36.053517
1362.000737	86870.557508	36.058535
1363.389917	86987.683949	36.063552
1364.760173	87102.216034	36.068570
1365.954895	87223.884943	36.073588
1367.256932	87341.875400	36.078605
1368.908782	87446.011850	36.083623
1370.259953	87567.366376	36.088640
1371.196127	87685.744644	36.093658
1372.519073	87804.177241	36.098676
1373.978868	87929.178669	36.103693
1375.452631	88050.807579	36.108711
1377.291164	88177.778710	36.113728
1378.777043	88301.485065	36.118746
1380.037725	88423.579550	36.123764
1381.388953	88549.715704	36.128781
1383.179029	88665.227706	36.133799
1384.030525	88782.178871	36.138816
1385.456299	88906.948961	36.143834
1386.961363	89032.024058	36.148852
1388.348214	89151.161801	36.153869
1389.942699	89273.955545	36.158887
1391.137107	89401.741884	36.163904
1392.362487	89525.291136	36.168922
1393.818250	89658.233868	36.173940
1395.339681	89788.594311	36.178957
1397.098396	89905.953646	36.183975
1398.650240	90021.609398	36.188992
1400.165046	90139.463856	36.194010
1401.834774	90257.066544	36.199028
1402.872978	90383.538025	36.204045
1404.507535	90500.057226	36.209063
1405.991081	90616.803162	36.214080
1407.708711	90737.302528	36.219098
1409.596910	90851.679800	36.224116
1410.763835	90968.374998	36.229133
1412.106517	91072.001999	36.234151
1413.647899	91187.296346	36.239168
1414.875867	91291.322172	36.244186
1416.330221	91395.997511	36.249204
1417.555921	91516.221700	36.254221
1419.085387	91624.434845	36.259239
1420.419422	91736.430309	36.264256
1421.998462	91851.467855	36.269274
1423.341544	91975.122951	36.274292
1424.526144	92091.515564	36.279309
1426.148709	92198.372810	36.284327
1427.566499	92318.646336	36.289344
1428.815521	92432.850258	36.294362
1430.081138	92544.022852	36.299380
1431.525618	92666.955221	36.304397
1432.320648	92783.170307	36.309415
1433.857411	92911.906883	36.314432
1435.448722	93040.521440	36.319450
1436.739803	93155.545374	36.324468
1438.020567	93275.717263	36.329485
1439.826992	93373.804498	36.334503
1440.965575	93484.683426	36.339520
1442.301738	93595.316531	36.344538
1444.229347	93700.027548	36.349556
1445.247902	93817.606008	36.354573
1446.089800	93935.377188	36.359591
1448.054535	94061.517000	36.364608
1449.075602	94174.546111	36.369626
1450.782573	94297.761052	36.374644
1451.917330	94415.995492	36.379661
1453.634566	94544.140451	36.384679
1455.313766	94662.253069	36.389696
1456.551170	94786.278212	36.394714
1458.181226	94904.107872	36.399732
1459.344029	95041.708268	36.404749
1460.784000	95171.521434	36.409767
1462.097465	95301.557641	36.414784
1463.918139	95429.309901	36.419802
1465.489524	95552.196027	36.424820
1467.043402	95691.170775	36.429837
1468.535243	95829.344554	36.434855
1469.927056	95948.799724	36.439872
1471.159433	96080.917957	36.444890
1473.358293	96212.239851	36.449908
1474.779387	96335.228511	36.454925
1476.310508	96459.569534	36.459943
1477.712921	96588.519804	36.464960
1478.973115	96712.916677	36.469978
1480.822496	96845.170270	36.474996
1482.240492	96980.064828	36.480013
1483.584989	97117.253127	36.485031
1485.122528	97240.100446	36.490048
1486.674417	97377.777327	36.495066
1487.869246	97508.969364	36.500084
1489.157611	97643.062969	36.505101
1491.135974	97780.738610	36.510119
1492.568128	97917.194180	36.515136
1493.883276	98055.506658	36.520154
1495.524919	98183.107844	36.525172
1497.170588	98324.222299	36.530189
1499.014149	98457.269503	36.535207
1500.695017	98590.507384	36.540224
1502.005915	98721.065201	36.545242
1503.662460	98838.816765	36.550260
1505.519957	98975.134610	36.555277
1507.017100	99086.079005	36.560295
1508.506222	99217.828107	36.565312
1509.835398	99354.584758	36.570330
1511.476095	99471.859389	36.575348
1512.995516	99605.976003	36.580365
1514.622081	99738.643968	36.585383
1516.073864	99861.185143	36.590400
1517.075940	100000.011147	36.595418
1518.995808	100113.948551	36.600436
1520.479622	100251.762530	36.605453
1521.846640	100378.489756	36.610471
1523.533202	100502.036381	36.615488
1525.185603	100644.389724	36.620506
1526.881766	100771.194036	36.625524
1528.311125	100904.734215	36.630541
1529.897924	101018.536481	36.635559
1531.367047	101148.420272	36.640576
1532.527690	101279.620384	36.645594
1534.390460	101394.319176	36.650612
1536.143140	101529.751322	36.655629
1537.423597	101661.365373	36.660647
1538.953897	101773.277367	36.665664
1540.646384	101904.663453	36.670682
1541.750389	102006.208499	36.675700
1543.356960	102119.897429	36.680717
1544.794272	102228.731972	36.685735
1546.166326	102335.396366	36.690752
1546.859850	102470.769049	36.695770
1548.937842	102588.329194	36.700788
1550.289973	102715.080497	36.705805
1551.752919	102845.567873	36.710823
1553.209961	102964.620643	36.715840
1554.555419	103108.655344	36.720858
1556.298370	103243.665005	36.725876
1556.984683	103373.286409	36.730893
1558.641169	103524.856369	36.735911
1560.109818	103663.029405	36.740928
1561.555496	103813.555797	36.745946
1563.222123	103962.159322	36.750964
1565.105308	104107.293805	36.755981
1566.696352	104260.614325	36.760999
1568.305816	104408.582108	36.766016
1570.072615	104559.061887	36.771034
1571.988599	104705.094083	36.776052
1573.325613	104847.324499	36.781069
1575.367539	105000.958614	36.786087
1576.856241	105137.207375	36.791104
1578.428667	105290.041011	36.796122
1580.122134	105439.559839	36.801140
1581.990936	105583.625202	36.806157
1583.631052	105719.675240	36.811175
1585.427736	105865.401377	36.816192
1586.739661	106011.888294	36.821210
1588.684106	106144.000010	36.826228
1590.233037	106292.302492	36.831245
1591.669077	106448.776337	36.836263
1593.495248	106578.346824	36.841280
1595.008711	106726.124165	36.846298
1596.608333	106861.931490	36.851316
1598.569878	107013.051256	36.856333
1599.932956	107158.267143	36.861351
1601.338943	107301.295980	36.866368
1603.129591	107446.928391	36.871386
1604.806865	107581.001977	36.876404
1606.968507	107719.565615	36.881421
1608.497417	107850.886358	36.886439
1610.534606	107985.438082	36.891456
1612.145785	108116.493426	36.896474
1613.765369	108253.178110	36.901492
1615.546206	108386.338401	36.906509
1616.910775	108515.024335	36.911527
1618.379927	108658.695695	36.916544
1620.117590	108806.738750	36.921562
1621.152378	108927.387244	36.926580
1623.062734	109069.748923	36.931597
1624.658407	109223.408096	36.936615
1626.294985	109348.732397	36.941632
1627.744157	109485.955702	36.946650
1629.101412	109633.757143	36.951668
1631.114603	109774.064052	36.956685
1632.249033	109926.593409	36.961703
1633.725365	110063.472364	36.966720
1635.138987	110219.751214	36.971738
1637.039135	110362.982080	36.976756
1638.658671	110516.135967	36.981773
1640.112601	110662.569794	36.986791
1642.150655	110817.181619	36.991808
1643.926285	110965.595666	36.996826
1645.059822	111105.841901	37.001844
1646.995874	111251.175925	37.006861
1648.787057	111388.404154	37.011879
1650.741820	111501.131778	37.016896
1652.415244	111626.927691	37.021914
1654.074880	111746.271169	37.026932
1655.995185	111876.290619	37.031949
1657.213012	112001.575403	37.036967
1658.760496	112118.109527	37.041984
1660.551242	112249.101646	37.047002
1661.864611	112374.347504	37.052020
1663.544703	112514.590318	37.057037
1664.737785	112664.459105	37.062055
1666.594242	112799.513968	37.067072
1667.938865	112945.543014	37.072090
1669.376079	113076.707322	37.077108
1671.290236	113229.243649	37.082125
1672.798370	113384.177368	37.087143
1674.188868	113529.085591	37.092160
1675.438981	113688.334745	37.097178
1677.169804	113851.098936	37.102196
1679.177852	114007.441373	37.107213
1680.805905	114182.220764	37.112231
1682.444709	114335.958730	37.117248
1683.861166	114505.407827	37.122266
1685.550851	114679.457095	37.127284
1687.621834	114846.358123	37.132301
1689.085008	115019.898902	37.137319
1691.063983	115171.685003	37.142336
1692.809352	115345.310231	37.147354
1694.146198	115518.048630	37.152372
1696.303258	115682.441494	37.157389
1697.854734	115859.320846	37.162407
1699.771276	116026.631770	37.167424
1701.620848	116199.420390	37.172442
1703.044219	116372.580551	37.177460
1704.965568	116535.555306	37.182477
1706.654213	116707.749851	37.187495
1708.461810	116882.260456	37.192512
1710.530417	117047.510260	37.197530
1711.927686	117226.868067	37.202548
1713.986576	117392.222378	37.207565
1715.488573	117562.268312	37.212583
1717.150990	117732.340784	37.217600
1718.969828	117910.012713	37.222618
1720.564367	118088.684372	37.227636
1722.918594	118249.620521	37.232653
1724.250308	118424.427996	37.237671
1725.894407	118600.671704	37.242688
1727.911393	118760.432155	37.247706
1729.477432	118934.152723	37.252724
1731.486082	119109.365368	37.257741
1732.848143	119279.669128	37.262759
1734.688547	119449.873830	37.267776
1736.785766	119620.140797	37.272794
1738.263140	119800.119878	37.277812
1740.611510	119970.184415	37.282829
1741.899104	120140.326012	37.287847
1743.634476	120301.240308	37.292864
1745.881541	120464.866286	37.297882
1747.234442	120647.659357	37.302900
1749.039606	120804.949719	37.307917
1750.500219	120972.924316	37.312935
1752.565993	121149.063382	37.317952
1754.270111	121311.001547	37.322970
1755.746978	121493.563668	37.327988
1757.578331	121658.591326	37.333005
1758.980984	121834.785964	37.338023
1760.394927	122011.715384	37.343040
1762.367446	122182.634622	37.348058
1763.769867	122361.089652	37.353076
1765.523394	122516.720492	37.358093
1767.171313	122690.787707	37.363111
1768.653968	122862.407733	37.368128
1770.176341	123018.457098	37.373146
1771.891584	123193.835356	37.378164
1773.668043	123373.632175	37.383181
1775.270284	123558.962546	37.388199
1777.010067	123725.903305	37.393216
1779.085245	123907.964870	37.398234
1780.471655	124091.517231	37.403252
1783.036164	124266.463581	37.408269
1784.482469	124462.288363	37.413287
1786.258041	124644.095446	37.418304
1788.161003	124836.032461	37.423322
1789.808785	125027.591460	37.428340
1791.853531	125199.616137	37.433357
1793.428497	125408.314764	37.438375
1794.792728	125594.592317	37.443392
1796.995025	125783.379076	37.448410
1798.471097	125984.167016	37.453428
1800.221412	126174.040857	37.458445
1801.989987	126384.376307	37.463463
1804.153953	126582.256379	37.468480
1806.087394	126773.994826	37.473498
1807.819036	126979.353178	37.478516
1810.168994	127179.008713	37.483533
1811.800505	127376.315762	37.488551
1813.567846	127576.825118	37.493568
1815.519389	127772.244630	37.498586
1817.187769	127974.864683	37.503604
1819.210894	128170.871229	37.508621
1821.101585	128382.834513	37.513639
1822.490171	128576.036338	37.518656
1824.523430	128780.798428	37.523674
1826.878616	128988.531028	37.528692
1828.465055	129188.251608	37.533709
1830.264171	129396.288457	37.538727
1832.382139	129596.194685	37.543744
1833.996908	129797.601197	37.548762
1836.178486	130001.546816	37.553780
1838.198796	130209.197981	37.558797
1839.780804	130414.951756	37.563815
1841.532915	130609.337034	37.568832
1843.984502	130794.707363	37.573850
1845.505208	131006.221188	37.578868
1848.030318	131198.268427	37.583885
1850.169123	131390.554282	37.588903
1851.760354	131583.243425	37.593920
1853.732666	131771.572792	37.598938
1855.506786	131967.940165	37.603956
1857.329264	132158.248539	37.608973
1858.886847	132355.780635	37.613991
1860.572756	132554.321426	37.619008
1862.831763	132742.115533	37.624026
1864.204335	132949.411241	37.629044
1865.780316	133147.375469	37.634061
1867.623439	133353.559382	37.639079
1869.377943	133559.212435	37.644096
1871.468550	133764.217762	37.649114
1873.122301	133969.901099	37.654132
1874.963026	134178.005263	37.659149
1876.718137	134390.349177	37.664167
1878.712434	134605.575370	37.669184
1880.788542	134808.278363	37.674202
1882.492393	135022.688909	37.679220
1884.210172	135231.286626	37.684237
1885.767745	135434.035086	37.689255
1887.565263	135623.055269	37.694272
1889.448772	135814.930673	37.699290
1891.543843	136020.516688	37.704308
1893.678975	136209.042645	37.709325
1895.546209	136393.448893	37.714343
1897.169765	136599.516982	37.719360
1899.427629	136789.168314	37.724378
1901.095120	136985.993204	37.729396
1902.925104	137171.233228	37.734413
1904.977404	137369.852590	37.739431
1906.831702	137561.359200	37.744448
1909.034435	137758.332516	37.749466
1910.692173	137970.518013	37.754484
1912.415486	138163.379959	37.759501
1914.773774	138371.828898	37.764519
1916.303560	138582.742713	37.769536
1918.280388	138777.192095	37.774554
1919.830732	138985.464956	37.779572
1922.009740	139202.993704	37.784589
1924.486206	139410.159847	37.789607
1925.912260	139626.665603	37.794624
1928.012320	139833.866810	37.799642
1929.903010	140057.078973	37.804660
1931.520940	140268.088152	37.809677
1933.427663	140489.091675	37.814695
1935.262567	140722.100183	37.819712
1937.247868	140942.738235	37.824730
1939.167950	141164.770761	37.829748
1940.963080	141398.435982	37.834765
1943.094108	141621.744954	37.839783
1944.771626	141861.027456	37.844800
1947.026832	142087.339728	37.849818
1948.916079	142322.022742	37.854836
1950.875984	142551.429018	37.859853
1952.758227	142785.518863	37.864871
1954.888127	143025.599686	37.869888
1956.562360	143254.393762	37.874906
1958.534940	143503.512323	37.879924
1960.174874	143743.977497	37.884941
1962.711245	143977.400077	37.889959
1964.142986	144230.617017	37.894976
1966.468546	144468.669101	37.899994
1968.019723	144717.960864	37.905012
1970.314667	144963.800147	37.910029
1972.772187	145207.521160	37.915047
1974.690413	145450.832295	37.920064
1976.955627	145682.020452	37.925082
1978.959278	145925.561719	37.930100
1980.844686	146163.385691	37.935117
1983.079407	146395.686054	37.940135
1985.024321	146642.831783	37.945152
1986.883424	146875.091236	37.950170
1989.059641	147129.539481	37.955188
1991.127609	147360.435908	37.960205
1993.139887	147587.889665	37.965223
1995.052631	147830.921010	37.970240
1997.133161	148057.985419	37.975258
1999.526674	148295.245107	37.980276
2001.749615	148535.565981	37.985293
2003.776207	148769.597493	37.990311
2005.575644	149008.844083	37.995328
2007.358990	149230.641491	38.000346
2009.526513	149466.672322	38.005364
2011.612074	149705.585580	38.010381
2013.023344	149927.951518	38.015399
2014.945562	150178.354162	38.020416
2017.297917	150410.704763	38.025434
2019.209344	150652.543383	38.030452
2020.997148	150872.163645	38.035469
2023.043898	151084.864696	38.040487
2025.024247	151298.249663	38.045504
2027.035229	151503.100695	38.050522
2029.086718	151732.368489	38.055540
2030.931821	151951.171788	38.060557
2032.779739	152174.316732	38.065575
2034.428992	152416.457824	38.070592
2036.070859	152642.302391	38.075610
2038.096989	152868.925860	38.080628
2039.616741	153124.824845	38.085645
2042.069917	153354.836542	38.090663
2044.283100	153596.234905	38.095680
2046.596707	153838.989623	38.100698
2049.099927	154076.219355	38.105716
2050.690722	154319.799492	38.110733
2052.762267	154571.671295	38.115751
2054.529496	154827.894904	38.120768
2056.472900	155073.492532	38.125786
2058.762569	155331.591995	38.130804
2060.775510	155599.332626	38.135821
2062.615344	155846.574539	38.140839
2064.899749	156105.846157	38.145856
2066.739760	156377.869935	38.150874
2069.024439	156629.349380	38.155892
2070.736997	156907.526938	38.160909
2072.997217	157172.595792	38.165927
2074.663904	157447.114250	38.170944
2076.909225	157709.674254	38.175962
2078.842274	157990.704290	38.180980
2080.702481	158267.113323	38.185997
2083.148271	158534.558680	38.191015
2085.234188	158826.664255	38.196032
2087.247967	159107.128338	38.201050
2089.636702	159385.161355	38.206068
2091.493319	159668.534277	38.211085
2094.015701	159950.281453	38.216103
2095.910211	160243.071026	38.221120
2098.266034	160528.388758	38.226138
2100.612479	160798.817467	38.231156
2102.495578	161089.073693	38.236173
2104.859515	161365.672149	38.241191
2106.892500	161645.738449	38.246208
2108.891786	161934.914044	38.251226
2111.182644	162220.858939	38.256244
2113.038894	162507.126665	38.261261
2115.534884	162785.196139	38.266279
2117.693213	163077.094434	38.271296
2119.685565	163354.013228	38.276314
2122.451080	163631.625416	38.281332
2124.271789	163909.690527	38.286349
2126.596401	164176.899372	38.291367
2129.621979	164449.688098	38.296384
2132.391513	164707.447359	38.301402
2135.259474	164958.145863	38.306420
2137.045841	165219.145308	38.311437
2139.605069	165466.008681	38.316455
2141.489797	165709.714949	38.321472
2143.273833	165960.801718	38.326490
2145.481096	166206.465615	38.331508
2147.193104	166467.278295	38.336525
2148.985899	166736.827362	38.341543
2150.879872	166991.189222	38.346560
2152.946925	167262.030804	38.351578
2154.733442	167518.747515	38.356596
2156.533415	167800.882085	38.361613
2158.663653	168082.483909	38.366631
2160.323288	168362.280954	38.371648
2162.399868	168618.601020	38.376666
2164.706635	168870.569205	38.381684
2166.197808	169134.283007	38.386701
2168.399798	169403.994454	38.391719
2170.849219	169667.738836	38.396736
2172.591567	169937.498411	38.401754
2174.751203	170213.402991	38.406772
2176.667189	170487.797460	38.411789
2178.818181	170765.089461	38.416807
2180.977521	171056.424505	38.421824
2182.894691	171333.336006	38.426842
2185.113706	171622.987916	38.431860
2186.586196	171926.991051	38.436877
2188.951951	172219.784101	38.441895
2191.359218	172526.005909	38.446912
2193.706272	172832.974780	38.451930
2195.726166	173138.560948	38.456948
2197.651220	173452.746783	38.461965
2200.214395	173756.892175	38.466983
2202.619985	174071.945357	38.472000
2204.441999	174377.935412	38.477018
2207.087798	174695.125044	38.482036
2209.138782	175024.852580	38.487053
2211.576283	175325.163349	38.492071
2214.223528	175632.744018	38.497088
2217.224709	175927.267838	38.502106
2219.152259	176234.746918	38.507124
2221.701255	176549.241465	38.512141
2223.795405	176852.189033	38.517159
2226.396479	177153.014376	38.522176
2228.452377	177465.557389	38.527194
2230.547846	177758.666764	38.532212
2232.709969	178075.893929	38.537229
2235.035205	178391.649254	38.542247
2236.933151	178699.903874	38.547264
2239.553389	179015.513985	38.552282
2241.784918	179321.255362	38.557300
2243.619096	179640.444105	38.562317
2246.046847	179957.687605	38.567335
2248.261102	180277.378239	38.572352
2250.748250	180603.935729	38.577370
2253.445109	180911.972150	38.582388
2255.944223	181229.437618	38.587405
2258.055423	181540.132498	38.592423
2260.703881	181841.398321	38.597440
2263.122365	182149.507621	38.602458
2265.590417	182451.514647	38.607476
2267.534987	182767.903369	38.612493
2269.597051	183076.807730	38.617511
2272.169674	183387.792506	38.622528
2273.754381	183711.377339	38.627546
2276.377395	184006.888538	38.632564
2278.239887	184335.003975	38.637581
2280.419372	184657.534231	38.642599
2282.889390	184975.524717	38.647616
2284.984843	185311.836381	38.652634
2287.228381	185653.891713	38.657652
2289.171471	186019.539981	38.662669
2291.761975	186343.738816	38.667687
2294.227486	186680.124400	38.672704
2296.556132	186999.235372	38.677722
2298.980461	187319.069009	38.682740
2300.768995	187644.184069	38.687757
2303.433475	187962.178898	38.692775
2306.044252	188278.659042	38.697792
2308.286910	188609.141880	38.702810
2310.492585	188923.248559	38.707828
2312.815702	189238.684051	38.712845
2315.121808	189534.996882	38.717863
2317.588372	189827.932714	38.722880
2319.178548	190129.260736	38.727898
2321.316400	190419.226632	38.732916
2323.474012	190741.092915	38.737933
2325.599704	191038.606136	38.742951
2327.738971	191364.820451	38.747968
2330.172591	191672.498314	38.752986
2332.951332	191978.650029	38.758004
2335.160019	192297.261331	38.763021
2337.245613	192613.809768	38.768039
2339.827077	192931.018473	38.773056
2341.845234	193263.581535	38.778074
2344.048902	193588.115337	38.783092
2346.876419	193913.924534	38.788109
2349.319758	194217.797093	38.793127
2351.841393	194556.787838	38.798144
2353.888835	194893.338550	38.803162
2356.279214	195225.442346	38.808180
2358.074540	195562.313405	38.813197
2360.594533	195899.199536	38.818215
2363.431715	196229.966210	38.823232
2365.660167	196579.854086	38.828250
2367.522133	196922.941471	38.833268
2369.614279	197277.297562	38.838285
2372.177190	197632.063900	38.843303
2374.915462	197982.307719	38.848320
2377.291859	198335.555296	38.853338
2379.400342	198692.503269	38.858356
2381.396177	199060.189208	38.863373
2383.899484	199417.229857	38.868391
2386.330504	199782.614432	38.873408
2388.244880	200160.628875	38.878426
2390.892698	200546.430130	38.883444
2393.589699	200923.511710	38.888461
2395.334374	201300.107309	38.893479
2398.615234	201671.435040	38.898496
2400.555207	202063.421146	38.903514
2403.065504	202435.988167	38.908532
2405.563676	202829.845125	38.913549
2408.130112	203205.808969	38.918567
2411.141334	203581.120119	38.923584
2413.692834	203953.353659	38.928602
2415.614517	204329.013705	38.933620
2418.341486	204701.831082	38.938637
2420.601573	205088.007481	38.943655
2423.316977	205458.999109	38.948672
2425.862112	205843.430630	38.953690
2428.349146	206217.329713	38.958708
2430.662137	206584.931220	38.963725
2433.160741	206970.007138	38.968743
2436.324851	207341.999223	38.973760
2438.453405	207714.254706	38.978778
2441.215808	208082.220647	38.983796
2443.344193	208447.135854	38.988813
2445.892006	208821.563361	38.993831
2448.541711	209193.105031	38.998848
2450.944628	209570.503020	39.003866
2453.402408	209925.233284	39.008884
2456.216399	210292.178420	39.013901
2458.808988	210658.777475	39.018919
2461.532264	211022.486105	39.023936
2463.587797	211385.968888	39.028954
2465.759825	211748.519484	39.033972
2468.416053	212114.069006	39.038989
2470.909486	212483.226212	39.044007
2473.164252	212850.160088	39.049024
2475.830407	213199.527288	39.054042
2478.035095	213539.465725	39.059060
2480.352013	213867.980804	39.064077
2482.550664	214226.160698	39.069095
2484.856356	214565.982824	39.074112
2487.239168	214918.723765	39.079130
2489.247665	215270.354718	39.084148
2491.636939	215635.390734	39.089165
2494.055251	215999.558835	39.094183
2496.238016	216365.592988	39.099200
2498.468433	216732.483766	39.104218
2500.633126	217116.583488	39.109236
2503.170162	217499.838059	39.114253
2505.370895	217882.103706	39.119271
2507.949999	218268.807250	39.124288
2510.251594	218667.671936	39.129306
2512.692355	219070.554473	39.134324
2515.541478	219462.958100	39.139341
2517.500568	219878.516490	39.144359
2520.284144	220286.122391	39.149376
2522.443542	220702.107363	39.154394
2525.303225	221109.193779	39.159412
2527.870864	221537.563613	39.164429
2530.275703	221954.730385	39.169447
2533.097333	222370.613067	39.174464
2535.949452	222791.419539	39.179482
2538.779565	223210.425880	39.184500
2541.978380	223611.795329	39.189517
2544.266098	224032.334316	39.194535
2547.104176	224438.256591	39.199552
2549.681793	224864.593542	39.204570
2552.884532	225261.948794	39.209588
2555.469199	225671.746646	39.214605
2557.636292	226085.293083	39.219623
2560.379660	226490.493497	39.224640
2563.284064	226902.832778	39.229658
2565.824918	227314.796723	39.234676
2568.512142	227713.857955	39.239693
2571.124553	228131.831393	39.244711
2574.028605	228538.276706	39.249728
2576.446595	228949.395687	39.254746
2578.803042	229357.196186	39.259764
2581.451014	229766.704052	39.264781
2584.234058	230172.939021	39.269799
2586.979072	230575.623168	39.274816
2589.660519	230998.106747	39.279834
2592.195103	231398.206627	39.284852
2595.366451	231811.264844	39.289869
2597.214011	232223.766702	39.294887
2599.903293	232632.606154	39.299904
2602.605739	233051.579449	39.304922
2605.338854	233462.138966	39.309940
2608.040124	233868.892538	39.314957
2610.604279	234279.655532	39.319975
2613.355322	234697.908633	39.324992
2615.473754	235105.310752	39.330010
2617.810364	235513.923327	39.335028
2620.717938	235926.028585	39.340045
2623.209470	236343.761591	39.345063
2625.958634	236769.608651	39.350080
2628.847817	237180.623080	39.355098
2631.204645	237608.054444	39.360116
2633.749082	238014.701313	39.365133
2636.015477	238444.635258	39.370151
2638.784098	238862.271357	39.375168
2641.527661	239283.314872	39.380186
2643.653911	239712.989447	39.385204
2646.709077	240134.846990	39.390221
2649.049286	240561.311577	39.395239
2651.379478	240961.078109	39.400256
2653.805058	241365.960680	39.405274
2656.190391	241781.213441	39.410292
2659.085840	242176.292160	39.415309
2661.927291	242576.332286	39.420327
2664.392855	242984.711689	39.425344
2666.664184	243393.400053	39.430362
2669.633683	243814.883821	39.435380
2672.467744	244235.219343	39.440397
2674.334328	244658.041704	39.445415
2677.170456	245074.387025	39.450432
2679.950175	245497.040226	39.455450
2682.514003	245932.097349	39.460468
2685.485019	246363.178143	39.465485
2687.672223	246805.430168	39.470503
2690.463958	247238.162719	39.475520
2693.582616	247675.822325	39.480538
2696.498613	248113.283821	39.485556
2698.996389	248563.891640	39.490573
2701.693981	248998.031861	39.495591
2704.200229	249441.371043	39.500608
2707.066377	249888.717449	39.505626
2709.847814	250359.090279	39.510644
2712.638229	250793.389317	39.515661
2715.690872	251256.325355	39.520679
2718.184909	251700.193866	39.525696
2720.844189	252160.368865	39.530714
2723.416723	252624.213867	39.535732
2726.194074	253073.775178	39.540749
2729.373044	253546.286592	39.545767
2732.693396	253993.601472	39.550784
2735.028964	254458.392082	39.555802
2737.560975	254914.387099	39.560820
2740.377451	255378.007585	39.565837
2743.204314	255843.479194	39.570855
2746.245578	256312.827630	39.575872
2749.293923	256778.515558	39.580890
2751.563922	257253.492739	39.585908
2754.686578	257713.780756	39.590925
2757.646320	258187.021501	39.595943
2760.095981	258648.807909	39.600960
2763.108892	259108.650701	39.605978
2765.928563	259570.985695	39.610996
2768.963402	260045.249055	39.616013
2771.943219	260501.332434	39.621031
2774.560265	260972.075649	39.626048
2777.730479	261427.312977	39.631066
2780.435688	261898.775297	39.636084
2783.459333	262344.735346	39.641101
2786.414487	262811.582950	39.646119
2788.745978	263261.609406	39.651136
2791.968126	263725.312803	39.656154
2794.363354	264201.487055	39.661172
2797.329152	264655.193504	39.666189
2799.498093	265124.490173	39.671207
2802.414097	265590.366573	39.676224
2805.621790	266053.960347	39.681242
2808.693570	266511.121818	39.686260
2811.776474	266964.342654	39.691277
2814.730632	267426.267817	39.696295
2817.090208	267872.002828	39.701312
2820.213524	268333.998963	39.706330
2822.778485	268792.320808	39.711348
2825.268051	269250.601377	39.716365
2828.719226	269703.269473	39.721383
2831.344752	270166.451628	39.726400
2834.549733	270619.966284	39.731418
2836.957723	271072.586799	39.736436
2839.934899	271510.944602	39.741453
2842.155670	271936.566834	39.746471
2844.602838	272368.272552	39.751488
2847.138661	272802.273498	39.756506
2849.666001	273242.902240	39.761524
2852.542443	273687.969665	39.766541
2855.158018	274133.557902	39.771559
2857.652120	274589.702325	39.776576
2860.528432	275040.476900	39.781594
2863.262974	275516.388151	39.786612
2865.830444	275979.548316	39.791629
2868.539613	276454.315222	39.796647
2871.139810	276930.239107	39.801664
2874.183316	277416.579645	39.806682
2876.537785	277908.738443	39.811700
2879.503882	278403.465497	39.816717
2882.787970	278899.054144	39.821735
2885.662632	279401.610797	39.826752
2888.584633	279897.198533	39.831770
2891.077668	280406.689956	39.836788
2894.045626	280912.904273	39.841805
2896.992328	281431.358581	39.846823
2899.608798	281944.070712	39.851840
2902.906105	282469.446522	39.856858
2905.825027	282989.950959	39.861876
2908.620057	283510.191546	39.866893
2911.706138	284044.476442	39.871911
2914.440690	284571.320924	39.876928
2917.744830	285103.506910	39.881946
2920.524429	285639.350817	39.886964
2923.402066	286170.960057	39.891981
2926.687782	286700.394027	39.896999
2929.595479	287245.829049	39.902016
2933.134261	287767.419710	39.907034
2935.986359	288303.637301	39.912052
2938.913694	288843.926851	39.917069
2942.541573	289371.635628	39.922087
2945.181690	289904.292738	39.927104
2948.290184	290438.345189	39.932122
2951.503142	290971.843655	39.937140
2954.644611	291496.563520	39.942157
2957.798851	292018.407840	39.947175
2960.623113	292545.097848	39.952192
2964.246553	293066.022363	39.957210
2967.302726	293590.788371	39.962228
2970.221630	294113.336878	39.967245
2973.010193	294638.897043	39.972263
2975.799123	295170.748997	39.977280
2979.008212	295687.754406	39.982298
2981.745874	296215.568014	39.987316
2984.714435	296745.143461	39.992333
2987.861629	297275.143220	39.997351
2990.700824	297798.915152	40.002368
2993.910962	298336.029249	40.007386
2996.822434	298865.593826	40.012404
2999.550047	299398.406174	40.017421
3002.702635	299924.191221	40.022439
3005.735403	300444.937919	40.027456
3009.199355	300970.588315	40.032474
3012.298507	301492.457054	40.037492
3015.535251	302010.948367	40.042509
3019.054456	302524.542011	40.047527
3021.982881	303044.416699	40.052544
3024.903740	303553.473304	40.057562
3028.135880	304066.842756	40.062580
3030.943538	304575.907017	40.067597
3034.456170	305084.983488	40.072615
3037.228888	305579.904075	40.077632
3040.352820	306046.182743	40.082650
3042.950488	306538.024405	40.087668
3045.694895	307009.074659	40.092685
3049.056990	307482.029657	40.097703
3051.476391	307982.489864	40.102720
3054.197827	308448.504248	40.107738
3057.169074	308944.604522	40.112756
3059.691962	309446.683635	40.117773
3062.339051	309950.489612	40.122791
3065.140068	310466.043561	40.127808
3068.028394	310971.171966	40.132826
3070.359887	311502.067542	40.137844
3073.436338	312030.531595	40.142861
3076.567392	312573.194433	40.147879
3079.551101	313128.437225	40.152896
3082.264014	313674.832518	40.157914
3085.123865	314238.304487	40.162932
3088.127265	314794.387179	40.167949
3090.916849	315359.632891	40.172967
3094.248405	315932.603928	40.177984
3097.150509	316510.938641	40.183002
3100.175450	317099.880255	40.188020
3103.635854	317694.253325	40.193037
3106.911616	318270.705260	40.198055
3109.799961	318872.612492	40.203072
3113.035077	319463.697713	40.208090
3116.129892	320059.313748	40.213108
3120.001553	320654.242411	40.218125
3123.357129	321252.288233	40.223143
3126.500730	321851.424427	40.228160
3129.908627	322442.340260	40.233178
3133.327386	323034.235730	40.238196
3136.580056	323622.291781	40.243213
3140.017991	324203.002987	40.248231
3142.624493	324807.635890	40.253248
3146.329950	325399.021671	40.258266
3149.326800	325998.831471	40.263284
3152.119737	326600.034268	40.268301
3155.657561	327183.935271	40.273319
3159.432120	327777.482958	40.278336
3163.112748	328369.666381	40.283354
3166.204848	328953.255668	40.288372
3169.236085	329547.476091	40.293389
3172.843224	330129.775365	40.298407
3175.661591	330717.313405	40.303424
3179.302631	331296.342600	40.308442
3183.207224	331875.753366	40.313460
3186.282119	332457.922841	40.318477
3189.554583	333025.592738	40.323495
3192.847907	333606.391503	40.328512
3196.051114	334182.476988	40.333530
3199.340171	334751.183794	40.338548
3202.106492	335331.530544	40.343565
3205.748772	335896.055487	40.348583
3208.895888	336472.672348	40.353600
3211.719995	337041.999771	40.358618
3214.952964	337617.418457	40.363636
3218.166907	338191.030103	40.368653
3221.822455	338760.911466	40.373671
3224.754760	339342.766711	40.378688
3228.181911	339916.089428	40.383706
3231.311742	340491.528973	40.388724
3234.223085	341070.417157	40.393741
3237.612469	341638.797529	40.398759
3240.538980	342218.831139	40.403776
3243.761721	342793.964973	40.408794
3247.189843	343370.376111	40.413812
3250.221706	343939.890481	40.418829
3252.995100	344492.824675	40.423847
3256.158056	345047.160200	40.428864
3259.378206	345588.899524	40.433882
3262.309462	346134.047913	40.438900
3265.019619	346691.267267	40.443917
3268.722249	347238.306455	40.448935
3271.878438	347793.663023	40.453952
3275.078659	348365.358989	40.458970
3278.548015	348919.532294	40.463988
3281.257700	349498.156758	40.469005
3284.422372	350071.730450	40.474023
3287.700358	350662.163283	40.479040
3290.893201	351236.979892	40.484058
3294.389563	351822.033079	40.489076
3297.092896	352428.598020	40.494093
3300.477798	353022.089682	40.499111
3303.522231	353627.285803	40.504128
3306.646703	354242.015946	40.509146
3309.958256	354851.279649	40.514164
3313.180932	355474.108600	40.519181
3316.687338	356084.230734	40.524199
3320.300763	356708.216508	40.529216
3323.523768	357347.257844	40.534234
3326.994868	357970.124925	40.539252
3330.251774	358612.886504	40.544269
3333.631524	359233.511409	40.549287
3337.253061	359874.085745	40.554304
3340.575930	360508.736323	40.559322
3344.043559	361147.862801	40.564340
3347.606840	361788.836430	40.569357
3351.257455	362426.563771	40.574375
3354.622921	363057.377146	40.579392
3358.054470	363700.484423	40.584410
3361.735043	364344.780780	40.589428
3364.769869	364987.693521	40.594445
3368.477536	365632.844316	40.599463
3371.465964	366265.294646	40.604480
3374.963092	366922.208500	40.609498
3378.698331	367569.136419	40.614516
3381.767352	368218.129992	40.619533
3385.504431	368868.601279	40.624551
3388.764404	369520.297529	40.629568
3392.240884	370179.141391	40.634586
3395.767032	370812.699471	40.639604
3399.224455	371462.951686	40.644621
3403.178995	372117.520088	40.649639
3406.487200	372766.422151	40.654656
3409.851405	373414.768191	40.659674
3413.229226	374063.831558	40.664692
3416.554817	374716.586581	40.669709
3420.376121	375366.968728	40.674727
3423.884152	376022.146793	40.679744
3427.331753	376673.062386	40.684762
3430.986530	377320.307419	40.689780
3434.082216	377973.348839	40.694797
3437.970754	378613.483867	40.699815
3441.435753	379260.559335	40.704832
3444.985179	379906.795258	40.709850
3448.612265	380551.812741	40.714868
3452.094353	381198.154014	40.719885
3455.251794	381845.821541	40.724903
3458.703514	382486.158099	40.729920
3462.040529	383147.239491	40.734938
3465.790453	383792.562652	40.739956
3469.080312	384447.286369	40.744973
3472.682760	385099.868015	40.749991
3476.094997	385748.461265	40.755008
3479.793325	386390.633566	40.760013
3482.730100	386979.362026	40.765018
3486.034225	387543.520720	40.770023
3488.876279	388059.325899	40.775028
3491.972292	388524.384324	40.780032
3494.576014	388953.513403	40.785037
3497.212440	389315.561342	40.790042
3499.164147	389649.634472	40.795047
3501.305028	389929.908366	40.800052
3503.140193	390179.612718	40.805056
3505.017122	390395.546704	40.810061
3506.721905	390554.517860	40.815066
3508.194944	390697.202033	40.820071
3509.384276	390788.806053	40.825076
3510.991270	390867.754281	40.830080
3512.113894	390910.478609	40.835085
3513.041972	390916.578752	40.840090
3513.519276	390923.053647	40.845095
3514.373524	390889.261709	40.850100
3515.421546	390837.823065	40.855104
3515.702127	390771.019447	40.860109
3516.573314	390684.171785	40.865114
3517.028835	390590.280903	40.870119
3516.996156	390460.800563	40.875124
3517.564538	390336.607533	40.880128
3517.664618	390202.459806	40.885133
3517.781530	390053.839383	40.890138
3518.013914	389894.995333	40.895143
3518.139887	389729.998229	40.900148
3518.042085	389558.028495	40.905152
3517.881988	389397.236885	40.910157
3518.308959	389209.520214	40.915162
3518.061884	389034.244552	40.920167
3517.750403	388856.921407	40.925172
3517.708321	388669.476738	40.930176
3517.514845	388489.949399	40.935181
3517.833983	388291.072554	40.940186
3517.366045	388112.600675	40.945191
3517.193651	387916.209082	40.950196
3517.576472	387725.187800	40.955200
3517.239867	387541.410873	40.960205
3516.834387	387342.715418	40.965210
3516.739858	387157.222426	40.970215
3516.168142	386963.855889	40.975220
3516.312683	386778.297515	40.980224
3516.254366	386595.409732	40.985229
3515.926782	386415.406039	40.990234
3515.476206	386227.524315	40.995239
3515.027394	386052.690812	41.000244
3515.183047	385866.717795	41.005248
3515.014659	385699.835778	41.010253
3514.886038	385517.103479	41.015258
3515.046280	385354.230361	41.020263
3514.465102	385178.929035	41.025268
3514.145493	385005.667773	41.030272
3513.808103	384825.222699	41.035277
3514.175033	384663.353997	41.040282
3514.066447	384495.515343	41.045287
3513.707722	384336.804349	41.050292
3513.489856	384167.685630	41.055296
3512.953701	384005.293139	41.060301
3513.050207	383842.521868	41.065306
3512.957755	383694.759804	41.070311
3512.758650	383535.231883	41.075316
3512.740658	383376.385754	41.080320
3512.319002	383231.008278	41.085325
3512.186882	383070.984617	41.090330
3511.712942	382927.238642	41.095335
3511.520063	382794.519099	41.100340
3511.533830	382650.670301	41.105344
3511.462011	382514.858020	41.110349
3511.316997	382376.263240	41.115354
3510.793495	382246.156980	41.120359
3511.178154	382120.352484	41.125364
3511.059328	381984.341599	41.130368
3510.755784	381849.628399	41.135373
3510.472837	381715.596912	41.140378
3510.296285	381595.590674	41.145383
3510.319774	381465.446175	41.150388
3510.090544	381335.645075	41.155392
3509.665542	381212.679299	41.160397
3509.472964	381099.427987	41.165402
3509.406595	380998.955060	41.170407
3508.895275	380888.114064	41.175412
3509.361472	380775.444473	41.180416
3509.095879	380664.284956	41.185421
3508.945322	380561.207849	41.190426
3508.684411	380452.027458	41.195431
3508.469199	380350.026147	41.200436
3508.676115	380231.630018	41.205440
3508.354973	380145.211292	41.210445
3508.574466	380037.427315	41.215450
3508.180508	379942.232649	41.220455
3507.900371	379858.422275	41.225460
3508.086386	379749.550346	41.230464
3507.808168	379664.520092	41.235469
3508.229370	379566.810077	41.240474
3507.800925	379470.806427	41.245479
3507.513307	379376.659777	41.250484
3507.587374	379280.577240	41.255488
3507.339299	379198.943798	41.260493
3507.557620	379110.075942	41.265498
3507.611642	379030.528210	41.270503
3507.490415	378931.605075	41.275508
3507.199163	378843.856853	41.280512
3507.321621	378757.415348	41.285517
3507.331967	378671.879873	41.290522
3507.009054	378594.243405	41.295527
3506.925002	378511.693457	41.300532
3507.446659	378433.772718	41.305536
3507.088501	378350.731602	41.310541
3506.992849	378265.211313	41.315546
3506.888213	378186.320656	41.320551
3506.937354	378113.043892	41.325556
3506.834485	378038.469952	41.330560
3506.768793	377955.839235	41.335565
3506.570364	377870.003514	41.340570
3506.452986	377795.659725	41.345575
3506.455196	377722.033634	41.350580
3506.457177	377643.632722	41.355584
3506.353489	377579.419641	41.360589
3506.234946	377497.811618	41.365594
3506.440040	377436.267647	41.370599
3506.112648	377367.593547	41.375604
3506.296741	377286.115567	41.380608
3505.906948	377220.117531	41.385613
3506.431310	377147.246724	41.390618
3505.958199	377085.629702	41.395623
3505.666030	377015.425362	41.400628
3505.862302	376952.332395	41.405632
3505.925125	376884.840827	41.410637
3505.863502	376801.926542	41.415642
3505.686562	376750.751991	41.420647
3505.803003	376676.343316	41.425652
3505.638559	376612.391356	41.430656
3505.719251	376549.290032	41.435661
3505.622541	376489.441736	41.440666
3505.628836	376418.986209	41.445671
3505.745289	376359.383835	41.450676
3505.553098	376298.584838	41.455680
3505.186132	376240.149556	41.460685
3505.430959	376181.136373	41.465690
3505.283014	376114.717013	41.470695
3505.502061	376064.520879	41.475700
3505.607396	376000.982663	41.480704
3505.293172	375939.998660	41.485709
3504.974726	375878.735789	41.490714
3505.119644	375828.499956	41.495719
3505.134988	375773.966387	41.500724
3505.351692	375719.731560	41.505728
3505.276235	375658.379581	41.510733
3505.300256	375599.577285	41.515738
3505.313491	375536.179306	41.520743
3505.233811	375474.548178	41.525748
3505.265682	375425.345155	41.530752
3505.222897	375360.583928	41.535757
3505.308503	375302.482583	41.540762
3504.990241	375241.726230	41.545767
3504.932404	375196.600650	41.550772
3504.907708	375141.894246	41.555776
3504.781765	375092.537383	41.560781
3504.782673	375034.601043	41.565786
3504.987702	374985.395678	41.570791
3505.240531	374935.674793	41.575796
3505.159504	374866.270205	41.580800
3504.823000	374818.444193	41.585805
3504.561612	374767.812431	41.590810
3504.766569	374719.622590	41.595815
3504.820907	374648.164394	41.600820
3504.533480	374605.994552	41.605824
3504.581051	374566.388713	41.610829
3504.797320	374514.767752	41.615834
3504.783604	374477.355724	41.620839
3504.604567	374421.655890	41.625844
3504.796243	374365.136250	41.630848
3504.724885	374320.011323	41.635853
3504.990383	374261.524165	41.640858
3504.781999	374206.946073	41.645863
3504.637257	374154.186794	41.650868
3504.824839	374107.598802	41.655872
3504.692938	374057.072575	41.660877
3504.646171	374001.148099	41.665882
3504.573722	373963.439702	41.670887
3504.305562	373902.799574	41.675892
3504.481997	373854.079235	41.680896
3504.322741	373812.904251	41.685901
3504.074545	373757.696442	41.690906
3504.089497	373724.012832	41.695911
3504.356039	373679.139078	41.700916
3504.659929	373637.205937	41.705920
3504.455734	373586.461485	41.710925
3504.719748	373541.410093	41.715930
3504.424826	373493.295884	41.720935
3504.246316	373437.416162	41.725940
3504.478619	373398.211707	41.730944
3504.083277	373361.644976	41.735949
3504.597653	373311.347023	41.740954
3504.414701	373259.989035	41.745959
3504.132083	373216.927265	41.750964
3504.287711	373160.969585	41.755968
3504.161574	373133.809937	41.760973
3504.076846	373075.298551	41.765978
3504.432733	373038.411279	41.770983
3504.315487	372990.852776	41.775988
3504.520736	372936.842830	41.780992
3504.294527	372896.108719	41.785997
3504.168591	372847.611464	41.791002
3504.234306	372805.739524	41.796007
3504.224178	372767.257743	41.801012
3504.159077	372718.344368	41.806016
3503.843797	372685.650740	41.811021
3503.905120	372645.582764	41.816026
3504.321471	372595.933807	41.821031
3503.799134	372556.896394	41.826036
3504.041699	372522.464646	41.831040
3503.991369	372477.155612	41.836045
3504.303077	372438.775704	41.841050
3504.070921	372386.382269	41.846055
3503.852052	372343.182207	41.851060
3504.102718	372304.760808	41.856064
3503.777982	372269.172324	41.861069
3503.977998	372225.627471	41.866074
3503.598954	372189.615499	41.871079
3503.721976	372152.636275	41.876084
3503.820537	372111.367828	41.881088
3503.543186	372079.582063	41.886093
3503.610740	372043.627416	41.891098
3503.573912	372001.846426	41.896103
3503.844639	371965.174199	41.901108
3504.086322	371918.548693	41.906112
3504.125702	371890.091947	41.911117
3503.816443	371842.739169	41.916122
3504.176919	371797.542917	41.921127
3503.704289	371762.027602	41.926132
3503.931048	371714.718208	41.931136
3503.375547	371685.312316	41.936141
3504.293002	371645.338296	41.941146
3504.156930	371598.796441	41.946151
3503.777006	371566.289373	41.951156
3504.086324	371511.752406	41.956160
3503.805420	371482.710014	41.961165
3504.023244	371439.313578	41.966170
3504.046251	371397.369954	41.971175
3503.582634	371360.404757	41.976180
3503.730989	371314.631062	41.981184
3503.671946	371278.898353	41.986189
3503.790357	371243.290402	41.991194
3503.884506	371202.122908	41.996199
3504.001197	371166.464321	42.001204
3504.203187	371117.227133	42.006208
3503.956391	371089.754020	42.011213
3503.914694	371038.522360	42.016218
3503.834446	370998.092994	42.021223
3503.923002	370959.390129	42.026228
3503.946132	370916.328019	42.031232
3503.490414	370883.628722	42.036237
3503.621584	370839.076285	42.041242
3503.910372	370802.044073	42.046247
3503.951646	370777.650449	42.051252
3503.739376	370724.742726	42.056256
3503.865254	370694.264425	42.061261
3504.065470	370659.913180	42.066266
3503.753559	370612.634939	42.071271
3503.801764	370578.739111	42.076276
3503.923140	370538.074477	42.081280
3503.650143	370496.709043	42.086285
3503.477115	370456.039296	42.091290
3503.284003	370431.986690	42.096295
3503.337125	370398.724974	42.101300
3503.364262	370353.756091	42.106304
3503.402597	370334.367096	42.111309
3503.636222	370300.365867	42.116314
3503.507915	370261.848211	42.121319
3503.437194	370232.898834	42.126324
3503.556905	370192.945272	42.131328
3503.686234	370170.391909	42.136333
3503.338726	370126.268487	42.141338
3503.837021	370088.059551	42.146343
3503.676669	370055.186305	42.151348
3504.054990	370007.443980	42.156352
3503.923693	369968.799368	42.161357
3503.626423	369932.365293	42.166362
3503.486411	369890.216146	42.171367
3503.327965	369863.998297	42.176372
3503.450738	369825.771229	42.181376
3503.547184	369802.689199	42.186381
3503.402348	369755.358114	42.191386
3503.551996	369719.209880	42.196391
3503.424672	369695.298833	42.201396
3503.634692	369658.785465	42.206400
3503.315233	369630.966569	42.211405
3503.530813	369592.927980	42.216410
3503.939460	369552.572886	42.221415
3503.533754	369525.402421	42.226420
3503.661804	369487.961618	42.231424
3503.915040	369437.417882	42.236429
3503.951401	369400.169063	42.241434
3503.606295	369351.242564	42.246439
3503.312647	369315.416844	42.251444
3503.919049	369281.686643	42.256448
3503.415277	369249.145352	42.261453
3503.751800	369214.339254	42.266458
3503.916567	369179.356602	42.271463
3503.701573	369138.005553	42.276468
3503.679341	369102.797857	42.281472
3503.684767	369069.846858	42.286477
3503.453198	369025.881509	42.291482
3503.589359	368996.644622	42.296487
3503.572378	368967.507751	42.301492
3503.228192	368914.998237	42.306496
3503.524523	368896.025402	42.311501
3503.206305	368851.768405	42.316506
3503.494526	368814.123952	42.321511
3503.364437	368788.764472	42.326516
3503.090072	368752.757203	42.331520
3503.208272	368723.675262	42.336525
3503.535953	368680.384512	42.341530
3503.505637	368650.004528	42.346535
3503.058394	368620.426147	42.351540
3503.295173	368586.219127	42.356544
3503.367693	368560.396023	42.361549
3503.281642	368526.340788	42.366554
3503.507683	368486.571517	42.371559
3503.164472	368460.025443	42.376564
3503.670130	368429.765065	42.381568
3503.577749	368402.265305	42.386573
3503.514504	368364.471705	42.391578
3503.686283	368328.546908	42.396583
3503.217904	368300.241766	42.401588
3503.496079	368260.006764	42.406592
3503.473352	368228.405675	42.411597
3503.574838	368194.371673	42.416602
3503.330312	368147.536130	42.421607
3503.222567	368128.955940	42.426612
3503.164958	368084.250702	42.431616
3503.254895	368052.377828	42.436621
3503.404052	368028.549383	42.441626
3503.341357	367985.292921	42.446631
3503.086156	367958.935932	42.451636
3503.518018	367917.507857	42.456640
3503.186132	367890.121092	42.461645
3503.489263	367855.801248	42.466650
3503.544297	367830.056422	42.471655
3503.275599	367798.416916	42.476660
3503.210863	367767.965131	42.481664
3503.058746	367736.942569	42.486669
3503.560360	367708.663741	42.491674
3503.174400	367673.409255	42.496679
3503.176096	367648.790441	42.501684
3503.295724	367609.874917	42.506688
3503.144678	367588.049107	42.511693
3502.775159	367548.701491	42.516698
3503.219444	367516.442597	42.521703
3503.005550	367492.085855	42.526708
3503.227953	367458.718135	42.531712
3503.256079	367431.833850	42.536717
3503.382143	367407.957670	42.541722
3503.188140	367363.882289	42.546727
3502.810490	367346.029567	42.551732
3503.121057	367313.410155	42.556736
3503.226095	367276.630601	42.561741
3503.192317	367251.432616	42.566746
3503.071517	367225.816237	42.571751
3503.026308	367192.947172	42.576756
3503.466953	367160.993326	42.581760
3503.120471	367123.547044	42.586765
3502.837329	367099.861320	42.591770
3503.123665	367072.961925	42.596775
3503.117971	367043.059133	42.601780
3503.340281	367024.706341	42.606784
3503.141238	366978.496979	42.611789
3502.901800	366961.613378	42.616794
3502.925167	366918.951681	42.621799
3502.831313	366897.014818	42.626804
3503.324109	366862.816716	42.631808
3503.258887	366837.699482	42.636813
3503.004580	366805.192804	42.641818
3503.047893	366772.360298	42.646823
3502.816200	366754.814787	42.651828
3502.807856	366720.618279	42.656832
3502.791915	366693.765569	42.661837
3503.116266	366670.213622	42.666842
3503.053137	366637.422934	42.671847
3502.969472	366608.192409	42.676852
3503.121746	366581.618305	42.681856
3502.864175	366558.258450	42.686861
3502.860617	366534.554161	42.691866
3503.053265	366516.205662	42.696871
3502.908764	366486.527151	42.701876
3503.275387	366452.576864	42.706880
3503.138030	366425.183837	42.711885
3502.598603	366411.624143	42.716890
3503.026101	366378.045406	42.721895
3503.010698	366353.605998	42.726900
3502.861284	366316.305853	42.731904
3502.978506	366289.177970	42.736909
3503.243096	366267.388111	42.741914
3503.269961	366234.303478	42.746919
3502.991978	366208.151689	42.751924
3503.419240	366162.834455	42.756928
3503.254602	366139.408985	42.761933
3502.820160	366106.040284	42.766938
3503.173287	366085.125777	42.771943
3502.960588	366060.996308	42.776948
3503.016593	366023.714635	42.781952
3503.288106	366001.161267	42.786957
3503.120737	365964.879772	42.791962
3503.239277	365931.628082	42.796967
3503.179332	365912.530866	42.801972
3503.114831	365882.483577	42.806977
3502.905766	365853.703738	42.811981
3503.028028	365813.006832	42.816986
3502.817816	365796.118001	42.821991
3502.762309	365769.016512	42.826996
3503.214441	365741.124579	42.832001
3502.592052	365717.287248	42.837005
3502.724049	365689.394267	42.842010
3502.930338	365661.210211	42.847015
3503.005005	365636.324246	42.852020
3503.198328	365600.926265	42.857025
3502.901196	365578.181569	42.862029
3502.639883	365552.712613	42.867034
3503.351256	365526.228396	42.872039
3502.953934	365501.491988	42.877044
3503.090743	365463.104471	42.882049
3503.101659	365442.725510	42.887053
3502.722038	365422.712206	42.892058
3502.885992	365386.734146	42.897063
3502.782636	365362.866572	42.902068
3502.751493	365330.653819	42.907073
3502.889657	365307.002699	42.912077
3502.703880	365291.837538	42.917082
3503.131568	365265.727539	42.922087
3502.801257	365242.174675	42.927092
3502.861831	365213.199792	42.932097
3502.973887	365184.191461	42.937101
3502.870719	365151.227464	42.942106
3502.856172	365120.714263	42.947111
3502.798379	365103.420184	42.952116
3502.881363	365076.728444	42.957121
3502.999869	365052.267103	42.962125
3502.702179	365022.788794	42.967130
3502.941127	364991.219667	42.972135
3502.932491	364970.690968	42.977140
3503.046327	364940.741999	42.982145
3503.227998	364923.410550	42.987149
3502.554390	364900.825543	42.992154
3502.870145	364853.465522	42.997159
3502.949814	364830.788651	43.002164
3502.730243	364802.085633	43.007169
3502.806380	364786.472912	43.012173
3502.599484	364765.568380	43.017178
3502.929844	364727.378456	43.022183
3503.072370	364714.194614	43.027188
3502.720399	364689.475868	43.032193
3503.118664	364654.171892	43.037197
3503.053375	364633.550136	43.042202
3503.085606	364598.455507	43.047207
3503.133137	364583.355308	43.052212
3503.235233	364553.331543	43.057217
3502.969851	364524.660791	43.062221
3502.996378	364490.507053	43.067226
3503.189666	364463.899225	43.072231
3503.189662	364426.979954	43.077236
3502.999876	364394.536766	43.082241
3503.059065	364363.096572	43.087245
3503.051755	364340.788584	43.092250
3503.245324	364305.770135	43.097255
3502.725630	364276.300210	43.102260
3502.817406	364252.960368	43.107265
3502.964132	364233.118435	43.112269
3502.883375	364207.671027	43.117274
3503.333436	364168.216695	43.122279
3502.909084	364146.075094	43.127284
3502.869278	364110.254220	43.132289
3503.157628	364091.533573	43.137293
3503.225766	364056.153205	43.142298
3503.115043	364031.320133	43.147303
3502.497205	364006.235632	43.152308
3502.499225	363973.990816	43.157313
3502.826535	363954.984516	43.162317
3502.899987	363936.017707	43.167322
3503.191116	363910.867906	43.172327
3502.985072	363875.174252	43.177332
3503.070658	363845.025285	43.182337
3503.144279	363826.591981	43.187341
3502.651495	363793.026436	43.192346
3502.775197	363763.405057	43.197351
3502.421025	363750.069388	43.202356
3502.839082	363719.665278	43.207361
3502.775319	363693.376261	43.212365
3502.721075	363677.707012	43.217370
3503.216117	363652.093293	43.222375
3502.923180	363626.195615	43.227380
3502.971356	363590.614516	43.232385
3503.225832	363565.495534	43.237389
3502.994029	363532.473506	43.242394
3503.059821	363505.274816	43.247399
3503.237915	363482.886508	43.252404
3503.034206	363441.652607	43.257409
3503.038267	363417.538044	43.262413
3502.797977	363396.256585	43.267418
3502.896229	363364.326457	43.272423
3502.903220	363341.329417	43.277428
3503.006570	363313.159125	43.282433
3502.881547	363286.396487	43.287437
3502.620351	363263.314070	43.292442
3502.703441	363237.281305	43.297447
3503.087514	363217.274704	43.302452
3502.733580	363189.505785	43.307457
3502.667396	363158.464969	43.312461
3502.451080	363133.723804	43.317466
3502.848674	363105.863269	43.322471
3502.939239	363081.455460	43.327476
3502.818853	363061.120690	43.332481
3502.920619	363042.225132	43.337485
3502.561054	363006.528908	43.342490
3502.578553	362975.601930	43.347495
3502.546207	362957.133753	43.352500
3502.770188	362939.794554	43.357505
3502.653669	362917.832820	43.362509
3502.532652	362897.015238	43.367514
3502.771938	362866.511020	43.372519
3502.703996	362838.112827	43.377524
3502.721994	362814.910382	43.382529
3503.097127	362795.336866	43.387533
3502.482345	362767.633553	43.392538
3502.890712	362744.395717	43.397543
3502.498251	362729.134343	43.402548
3502.356569	362698.181026	43.407553
3502.649068	362685.989363	43.412557
3502.413306	362664.376335	43.417562
3502.767185	362637.589410	43.422567
3502.807652	362615.679254	43.427572
3502.388864	362589.393682	43.432577
3502.862549	362556.768997	43.437581
3502.571362	362550.055175	43.442586
3502.645026	362519.322268	43.447591
3502.727626	362489.909297	43.452596
3502.565608	362469.097795	43.457601
3502.263197	362441.218514	43.462605
3502.720050	362432.660327	43.467610
3503.013665	362396.429742	43.472615
3502.816862	362387.617508	43.477620
3502.920640	362357.718306	43.482625
3502.705519	362327.970341	43.487629
3503.066389	362306.391263	43.492634
3502.831813	362283.278529	43.497639
3502.620941	362245.906541	43.502644
3502.618243	362224.841377	43.507649
3502.905564	362202.943327	43.512653
3502.615323	362176.891496	43.517658
3502.877002	362147.831487	43.522663
3502.902449	362128.921814	43.527668
3502.512191	362107.510300	43.532673
3502.747733	362082.748767	43.537677
3502.301292	362065.538797	43.542682
3502.593935	362043.461923	43.547687
3502.396054	362028.957656	43.552692
3502.653287	361998.322701	43.557697
3503.162191	361979.871338	43.562701
3502.294811	361954.925570	43.567706
3502.626691	361920.670528	43.572711
3502.526424	361906.328889	43.577716
3502.382333	361878.449856	43.582721
3502.711755	361858.704960	43.587725
3502.314882	361843.545463	43.592730
3502.560220	361812.276887	43.597735
3502.376504	361795.610338	43.602740
3502.194503	361780.747719	43.607745
3502.759847	361755.832949	43.612749
3502.494730	361741.466061	43.617754
3502.709662	361712.565371	43.622759
3502.909514	361690.273975	43.627764
3502.661608	361661.546905	43.632769
3503.009189	361642.993381	43.637773
3502.490195	361616.493839	43.642778
3502.481540	361589.025456	43.647783
3502.312870	361574.541833	43.652788
3502.711764	361550.186436	43.657793
3502.794617	361528.116418	43.662797
3502.407086	361513.463531	43.667802
3502.538518	361477.104600	43.672807
3502.787678	361469.594925	43.677812
3502.667248	361431.902905	43.682817
3502.599077	361417.047804	43.687821
3502.683514	361396.171790	43.692826
3502.545098	361366.537990	43.697831
3502.525399	361344.585442	43.702836
3502.805067	361324.034763	43.707841
3502.539020	361294.954400	43.712845
3502.583349	361281.021961	43.717850
3502.539855	361262.173293	43.722855
3502.859516	361232.290195	43.727860
3502.478961	361216.772075	43.732865
3502.280978	361194.618454	43.737869
3502.306659	361173.497310	43.742874
3502.542205	361146.981584	43.747879
3502.722749	361135.391187	43.752884
3502.689440	361105.766186	43.757889
3503.013743	361080.558010	43.762893
3502.850613	361057.611094	43.767898
3502.877315	361027.468438	43.772903
3502.442368	361004.716251	43.777908
3502.869915	360976.264596	43.782913
3502.663358	360947.708292	43.787917
3502.699154	360933.395839	43.792922
3502.892628	360908.157054	43.797927
3502.549055	360889.329436	43.802932
3502.647709	360866.189164	43.807937
3502.837873	360827.507805	43.812941
3502.536969	360814.060879	43.817946
3502.530631	360788.065309	43.822951
3502.771384	360777.304007	43.827956
3502.965477	360752.573240	43.832961
3502.818981	360728.632407	43.837965
3502.691876	360711.270315	43.842970
3502.792179	360670.874705	43.847975
3502.372698	360654.701631	43.852980
3502.435281	360626.941747	43.857985
3502.657482	360610.541734	43.862989
3502.577048	360593.172312	43.867994
3502.401634	360560.773528	43.872999
3502.373363	360554.221642	43.878004
3502.482069	360532.782181	43.883009
3502.603855	360496.525217	43.888013
3502.714226	360474.373907	43.893018
3502.833045	360456.261851	43.898023
3502.862054	360436.334059	43.903028
3502.697329	360404.365456	43.908033
3503.149102	360374.562601	43.913037
3502.749081	360350.000193	43.918042
3502.663269	360326.811976	43.923047
3502.534365	360303.452558	43.928052
3502.531292	360278.777497	43.933057
3502.988658	360262.213638	43.938061
3502.156127	360226.892646	43.943066
3502.671068	360207.702292	43.948071
3502.689867	360188.131704	43.953076
3502.253795	360171.122333	43.958081
3502.851514	360145.133862	43.963085
3502.564682	360131.455726	43.968090
3502.900665	360099.459710	43.973095
3502.774436	360082.961155	43.978100
3502.627276	360056.859805	43.983105
3502.532211	360040.839221	43.988109
3502.276002	360016.508292	43.993114
3502.480974	359991.826035	43.998119
3502.252184	359978.952011	44.003124
3502.580466	359954.504664	44.008129
3502.391439	359918.803633	44.013133
3502.038118	359910.752001	44.018138
3502.255911	359892.700445	44.023143
3502.251816	359879.664348	44.028148
3501.943275	359859.687052	44.033153
3502.482302	359842.042912	44.038157
3502.722449	359835.982775	44.043162
3502.489469	359805.320223	44.048167
3502.446855	359790.816126	44.053172
3502.319603	359769.387430	44.058177
3502.247755	359736.590451	44.063181
3502.183713	359721.327263	44.068186
3502.587262	359707.719396	44.073191
3502.671129	359685.368329	44.078196
3502.492357	359658.814120	44.083201
3502.408536	359636.006261	44.088205
3502.390889	359630.011612	44.093210
3502.703602	359598.323647	44.098215
3502.792177	359576.149659	44.103220
3502.325903	359563.719025	44.108225
3502.244655	359528.788573	44.113229
3502.509141	359504.579512	44.118234
3502.389980	359490.519210	44.123239
3502.505380	359481.860846	44.128244
3502.690621	359462.619675	44.133249
3502.960991	359431.878419	44.138253
3502.522562	359409.989625	44.143258
3502.585318	359386.243889	44.148263
3502.474370	359356.629257	44.153268
3502.725568	359335.446324	44.158273
3502.747564	359313.841601	44.163277
3502.529570	359296.823216	44.168282
3502.791400	359275.308212	44.173287
3502.550696	359249.627341	44.178292
3502.933370	359221.943429	44.183297
3502.930755	359198.970125	44.188301
3502.594773	359176.302815	44.193306
3502.674257	359144.396537	44.198311
3502.560069	359123.880242	44.203316
3502.241254	359107.004508	44.208321
3502.302199	359077.286614	44.213325
3502.126483	359069.918703	44.218330
3502.557406	359047.792712	44.223335
3502.503418	359031.612722	44.228340
3502.552238	359009.571577	44.233345
3502.997170	358989.959319	44.238349
3502.687279	358956.105753	44.243354
3502.382919	358933.001308	44.248359
3502.620506	358906.762858	44.253364
3502.323238	358891.281410	44.258369
3502.674324	358863.093813	44.263373
3502.445974	358861.553804	44.268378
3502.314087	358823.224973	44.273383
3502.313951	358817.100370	44.278388
3502.198447	358794.855917	44.283393
3502.356622	358784.386314	44.288397
3502.074799	358760.693712	44.293402
3502.159920	358732.344072	44.298407
3502.233523	358723.539513	44.303412
3502.182094	358705.732461	44.308417
3501.905616	358680.946166	44.313421
3502.279909	358674.382060	44.318426
3502.357554	358652.259930	44.323431
3502.251631	358645.745131	44.328436
3501.944098	358629.858523	44.333441
3502.557589	358600.232081	44.338445
3502.156668	358585.325715	44.343450
3502.361702	358560.515221	44.348455
3502.205077	358550.729877	44.353460
3502.113690	358525.609685	44.358465
3502.416667	358518.624603	44.363469
3502.239746	358497.965165	44.368474
3502.397541	358480.404980	44.373479
3502.058194	358456.619437	44.378484
3502.015950	358441.377631	44.383489
3502.684769	358424.957771	44.388493
3502.205735	358404.904395	44.393498
3502.268613	358387.892625	44.398503
3502.315472	358366.283363	44.403508
3502.077354	358358.111735	44.408513
3502.295524	358338.432692	44.413517
3502.350864	358322.540285	44.418522
3502.575114	358310.764112	44.423527
3502.550652	358287.869766	44.428532
3502.214735	358265.074699	44.433537
3502.333518	358233.949200	44.438541
3502.557822	358230.788445	44.443546
3502.722728	358205.983910	44.448551
3502.297488	358186.506549	44.453556
3502.201251	358171.959199	44.458561
3502.333675	358160.654717	44.463565
3502.411900	358141.734342	44.468570
3502.504845	358121.286800	44.473575
3502.585303	358094.411333	44.478580
3502.198489	358075.715770	44.483585
3502.398700	358050.956445	44.488589
3502.116314	358032.752895	44.493594
3502.029876	358017.797316	44.498599
3502.475632	357996.532353	44.503604
3502.011970	357984.990176	44.508609
3502.498531	357968.471363	44.513613
3502.119550	357954.171225	44.518618
3502.428174	357931.529756	44.523623
3502.419474	357907.641506	44.528628
3502.158715	357883.690802	44.533633
3502.116594	357864.712741	44.538637
3502.271533	357858.970450	44.543642
3502.354820	357836.033586	44.548647
3502.320400	357828.694217	44.553652
3502.304297	357810.017050	44.558657
3502.607730	357782.928710	44.563661
3501.942406	357769.969194	44.568666
3502.343644	357742.662282	44.573671
3502.350059	357735.646928	44.578676
3502.084596	357709.765300	44.583681
3502.238617	357699.753441	44.588685
3502.220710	357679.449930	44.593690
3502.124166	357656.795065	44.598695
3502.184588	357638.588767	44.603700
3502.042438	357624.277036	44.608705
3502.258101	357603.505076	44.613709
3502.296942	357592.697830	44.618714
3502.166155	357572.233909	44.623719
3502.472134	357562.732072	44.628724
3502.034140	357545.213236	44.633729
3502.298096	357520.316490	44.638733
3502.277317	357505.757083	44.643738
3502.537281	357501.929918	44.648743
3502.727921	357482.356272	44.653748
3502.365575	357467.062135	44.658753
3502.585946	357427.278924	44.663757
3502.335069	357420.201877	44.668762
3502.045152	357388.275013	44.673767
3502.219597	357375.794613	44.678772
3502.247078	357358.050746	44.683777
3502.374729	357324.889745	44.688781
3502.179999	357322.404068	44.693786
3502.229969	357307.655652	44.698791
3502.414816	357291.818807	44.703796
3502.245649	357274.842531	44.708801
3502.181772	357247.912542	44.713805
3502.309841	357243.572151	44.718810
3502.436830	357216.968245	44.723815
3502.326683	357198.839061	44.728820
3502.440733	357186.774626	44.733825
3502.727091	357165.051009	44.738829
3502.264672	357139.682441	44.743834
3502.349076	357117.126099	44.748839
3502.567153	357099.377840	44.753844
3502.150543	357084.447771	44.758849
3502.309087	357048.816385	44.763853
3502.309839	357048.765551	44.768858
3502.306175	357020.911043	44.773863
3502.360691	356998.816742	44.778868
3502.185345	356990.711228	44.783873
3502.295695	356969.472339	44.788877
3502.239289	356959.874217	44.793882
3502.185341	356940.999090	44.798887
3502.489848	356918.738753	44.803892
3502.188004	356903.689076	44.808897
3502.563418	356873.945536	44.813901
3502.423551	356859.429773	44.818906
3502.522426	356839.336277	44.823911
3502.538803	356820.246809	44.828916
3501.966534	356811.338888	44.833921
3502.422436	356787.224981	44.838925
3502.064352	356766.897560	44.843930
3502.245823	356753.450026	44.848935
3502.233816	356727.451889	44.853940
3502.258680	356712.325864	44.858945
3502.149942	356696.610647	44.863949
3502.146752	356676.532928	44.868954
3502.119252	356664.947798	44.873959
3502.293666	356637.700626	44.878964
3501.852952	356636.091887	44.883969
3502.052548	356611.687326	44.888973
3502.011486	356596.698582	44.893978
3502.268279	356581.765143	44.898983
3502.136768	356562.749363	44.903988
3502.024799	356552.626031	44.908993
3502.379927	356535.542348	44.913997
3502.384173	356511.930579	44.919002
3502.149617	356502.741274	44.924007
3502.428796	356482.289085	44.929012
3502.258094	356463.152264	44.934017
3502.393413	356434.716456	44.939021
3502.419551	356420.530475	44.944026
3502.186919	356405.749361	44.949031
3502.562179	356384.163859	44.954036
3502.138135	356370.149574	44.959041
3502.037048	356341.750468	44.964045
3502.076791	356331.755952	44.969050
3502.166422	356326.658938	44.974055
3502.204703	356300.398459	44.979060
3502.260794	356299.576534	44.984065
3502.192427	356280.754082	44.989069
3502.301229	356254.762166	44.994074
3502.400004	356240.971457	44.999079
3502.364344	356209.944205	45.004084
3501.867965	356205.395850	45.009089
3502.573744	356181.344256	45.014093
3502.792399	356172.033495	45.019098
3502.270343	356149.926649	45.024103
3502.765200	356127.280302	45.029108
3502.335933	356099.287869	45.034113
3502.216779	356083.472300	45.039117
3502.671828	356068.914423	45.044122
3502.280605	356042.466402	45.049127
3502.401631	356021.682696	45.054132
3502.196943	356012.946089	45.059137
3502.316302	355981.538662	45.064141
3502.488863	355966.719702	45.069146
3502.351865	355945.594854	45.074151
3502.230044	355922.027673	45.079156
3502.253235	355908.502741	45.084161
3501.865010	355886.527379	45.089165
3501.944225	355873.476623	45.094170
3502.131433	355860.764883	45.099175
3502.184499	355846.803199	45.104180
3502.024800	355840.550339	45.109185
3502.375008	355816.731711	45.114189
3502.317481	355805.888008	45.119194
3502.170806	355784.052900	45.124199
3502.374464	355761.121190	45.129204
3502.526168	355754.870687	45.134209
3502.117075	355725.781877	45.139213
3502.248695	355712.595817	45.144218
3502.077722	355693.128151	45.149223
3502.006356	355677.686186	45.154228
3501.954563	355666.714461	45.159233
3502.225203	355650.253437	45.164237
3502.346364	355633.561501	45.169242
3502.167284	355622.457068	45.174247
3502.182748	355597.343291	45.179252
3501.967461	355587.998218	45.184257
3502.577976	355561.698905	45.189261
3502.549054	355550.342332	45.194266
3502.183925	355526.660216	45.199271
3502.350982	355506.275670	45.204276
3501.973248	355499.955004	45.209281
3502.286675	355467.703532	45.214285
3502.229877	355470.228727	45.219290
3502.484045	355456.184741	45.224295
3502.071339	355436.068285	45.229300
3502.260771	355418.908111	45.234305
3502.119989	355392.268069	45.239309
3502.297224	355378.566437	45.244314
3502.497856	355350.348230	45.249319
3502.151697	355336.702610	45.254324
3502.045137	355317.504271	45.259329
3502.261110	355291.749046	45.264333
3502.293737	355293.370754	45.269338
3502.206125	355265.934411	45.274343
3502.116817	355251.486282	45.279348
3502.047188	355236.933416	45.284353
3502.115546	355220.300311	45.289357
3502.064425	355213.217092	45.294362
3502.251805	355190.567083	45.299367
3502.663372	355172.253868	45.304372
3502.048702	355148.711965	45.309377
3502.032544	355134.506568	45.314381
3502.227243	355124.258801	45.319386
3502.014287	355089.318414	45.324391
3502.402158	355081.760182	45.329396
3502.142138	355066.804777	45.334401
3502.002362	355046.874352	45.339405
3502.269346	355038.597830	45.344410
3502.386637	355020.050733	45.349415
3502.435339	354997.371332	45.354420
3502.331302	354985.339985	45.359425
3502.541294	354969.803055	45.364429
3502.452488	354944.755816	45.369434
3502.077924	354925.116020	45.374439
3501.997557	354904.998340	45.379444
3502.428599	354889.604892	45.384449
3502.388951	354875.275947	45.389453
3502.138305	354865.122815	45.394458
3502.098483	354852.013907	45.399463
3502.198240	354844.983377	45.404468
3502.107569	354827.154791	45.409473
3502.460537	354806.537525	45.414477
3502.165556	354785.614401	45.419482
3501.934415	354776.576559	45.424487
3502.143716	354764.165945	45.429492
3502.129050	354739.996607	45.434497
3502.681704	354723.872473	45.439501
3502.519727	354699.497272	45.444506
3502.047066	354685.896471	45.449511
3502.545501	354655.216664	45.454516
3502.148598	354645.365810	45.459521
3502.299809	354624.398563	45.464525
3502.203710	354606.087768	45.469530
3502.119380	354600.000853	45.474535
3501.989154	354559.226442	45.479540
3502.338282	354551.521609	45.484545
3502.509463	354535.100898	45.489549
3502.660571	354519.572910	45.494554
3502.155809	354499.521013	45.499559
3502.276077	354475.889657	45.504564
3502.284011	354461.476869	45.509569
3502.495062	354439.458073	45.514573
3502.215698	354424.810383	45.519578
3502.355456	354410.173717	45.524583
3502.267582	354386.752607	45.529588
3502.216605	354361.063582	45.534593
3502.174969	354341.117438	45.539597
3502.240980	354330.050663	45.544602
3502.171008	354313.565693	45.549607
3502.618685	354291.942071	45.554612
3501.874577	354279.552542	45.559617
3502.003896	354270.966815	45.564621
3502.327767	354250.099539	45.569626
3502.209914	354232.554440	45.574631
3502.569209	354209.749889	45.579636
3502.386133	354194.426250	45.584641
3502.360975	354170.308945	45.589645
3502.124861	354148.537456	45.594650
3502.062977	354138.558057	45.599655
3502.512833	354119.551998	45.604660
3502.226210	354110.700523	45.609665
3502.276809	354087.715162	45.614669
3502.135892	354062.217814	45.619674
3501.945980	354055.333857	45.624679
3501.918808	354039.604616	45.629684
3502.050841	354013.378475	45.634689
3502.364860	354003.493045	45.639693
3502.016169	353996.659201	45.644698
3502.203831	353976.931325	45.649703
3502.201052	353959.520674	45.654708
3502.089034	353944.262111	45.659713
3502.146121	353923.131122	45.664717
3502.202829	353906.244960	45.669722
3501.780908	353884.502203	45.674727
3502.251011	353877.337575	45.679732
3502.290038	353867.901581	45.684737
3502.560658	353849.736626	45.689741
3502.146442	353832.644110	45.694746
3502.254547	353814.148572	45.699751
3502.120121	353793.987763	45.704756
3502.217080	353775.976879	45.709761
3502.255567	353763.262021	45.714765
3502.097571	353739.648001	45.719770
3502.077725	353726.713444	45.724775
3502.457175	353709.827792	45.729780
3502.356469	353691.135914	45.734785
3502.144200	353674.011887	45.739789
3502.194431	353651.763391	45.744794
3501.939120	353642.220625	45.749799
3502.263146	353627.148235	45.754804
3502.018318	353604.488096	45.759809
3501.621286	353591.408834	45.764813
3501.941098	353577.785909	45.769818
3501.960344	353518.940034	45.774823
3501.722242	353408.687597	45.779828
3501.487542	353254.994278	45.784833
3501.065876	353064.396218	45.789837
3500.223794	352839.750560	45.794842
3499.655398	352557.080215	45.799847
3499.099591	352241.385927	45.804852
3498.124127	351882.286596	45.809857
3497.348586	351487.081522	45.814861
3496.563639	351045.278044	45.819866
3494.814488	350578.071025	45.824871
3493.684267	350074.104115	45.829876
3492.331919	349545.149478	45.834881
3491.005363	348972.482398	45.839885
3489.621289	348370.960172	45.844890
3487.936909	347740.339410	45.849895
3486.521499	347065.479414	45.854900
3484.504689	346371.504540	45.859905
3482.802536	345643.092857	45.864909
3481.053972	344888.053000	45.869914
3478.765259	344108.316190	45.874919
3477.023865	343292.803882	45.879924
3474.392934	342466.757057	45.884929
3472.638866	341594.708950	45.889933
3470.268401	340718.819241	45.894938
3467.859711	339813.925332	45.899943
3465.559313	338886.995415	45.904948
3463.060203	337943.314299	45.909953
3460.598230	336980.377419	45.914957
3458.065343	335990.164034	45.919962
3455.332564	334979.482562	45.924967
3453.057029	333966.566213	45.929972
3449.838344	332925.029800	45.934977
3447.087065	331869.657774	45.939981
3444.531173	330806.417891	45.944986
3441.203395	329721.801528	45.949991
3438.817095	328632.608199	45.954996
3435.303405	327518.072706	45.960001
3432.601475	326384.556120	45.965005
3429.728641	325253.756295	45.970010
3426.476126	324111.638584	45.975015
3424.092181	322958.898551	45.980020
3419.757951	321795.465551	45.985025
3416.713275	320622.564890	45.990029
3413.754055	319445.395596	45.995034
3410.420460	318262.935256	46.000039
3407.106616	317063.774900	46.005044
3403.686302	315866.710743	46.010049
3400.139758	314653.731790	46.015053
3397.141108	313441.831420	46.020058
3393.644796	312233.284866	46.025063
3390.361896	310999.075035	46.030068
3387.184246	309777.667762	46.035073
3383.285234	308542.447564	46.040077
3380.147858	307304.405800	46.045082
3376.486789	306061.732280	46.050087
3373.198703	304807.212606	46.055092
3369.732331	303557.245770	46.060097
3366.192474	302306.217091	46.065101
3362.383814	301055.149976	46.070106
3358.859123	299795.025234	46.075111
3355.477814	298535.918375	46.080116
3351.828578	297282.882781	46.085121
3348.191002	296016.276492	46.090125
3344.660148	294755.149546	46.095130
3341.317331	293498.090123	46.100135
3337.420178	292222.966563	46.105140
3333.524185	290967.493694	46.110145
3330.157641	289694.730231	46.115149
3326.864802	288426.333959	46.120154
3323.173321	287161.462677	46.125159
3319.464124	285871.188654	46.130164
3315.699472	284609.208357	46.135169
3311.875129	283335.197866	46.140173
3308.443965	282068.842894	46.145178
3304.601376	280799.423753	46.150183
3301.058145	279526.601036	46.155188
3296.872415	278265.034119	46.160193
3293.346523	277009.276439	46.165197
3289.595584	275741.974565	46.170202
3286.193052	274478.545374	46.175207
3282.684731	273214.247892	46.180212
3278.641953	271946.501191	46.185217
3274.957483	270696.784588	46.190221
3271.913724	269427.344491	46.195226
3267.564229	268168.072034	46.200231
3264.346857	266908.988890	46.205236
3260.137282	265646.428272	46.210241
3256.396472	264396.103917	46.215245
3253.281807	263146.354882	46.220250
3248.979195	261890.104583	46.225255
3245.241133	260631.307802	46.230260
3241.365842	259385.811863	46.235265
3237.766645	258140.565777	46.240269
3234.368826	256890.794036	46.245274
3230.349663	255665.274585	46.250279
3226.691810	254415.010864	46.255284
3222.612479	253183.901810	46.260289
3219.337896	251943.489253	46.265293
3215.612339	250706.320402	46.270298
3211.817363	249475.774507	46.275303
3208.053449	248245.113116	46.280308
3204.324963	247023.020475	46.285313
3200.478415	245794.240394	46.290317
3196.747334	244578.550941	46.295322
3192.846475	243360.334286	46.300327
3189.098742	242144.328611	46.305332
3185.611515	240939.558944	46.310337
3181.775508	239714.947288	46.315341
3178.295568	238502.882036	46.320346
3174.020596	237296.207930	46.325351
3170.475031	236085.977921	46.330356
3166.652231	234904.439761	46.335361
3163.039694	233701.344555	46.340365
3159.162474	232500.121483	46.345370
3155.534628	231313.170783	46.350375
3152.147354	230120.628484	46.355380
3147.941749	228945.454547	46.360385
3144.212653	227750.797954	46.365389
3140.836153	226563.293538	46.370394
3136.681793	225388.924583	46.375399
3133.310749	224210.842714	46.380404
3129.480998	223038.817975	46.385409
3125.686102	221859.937554	46.390413
3122.014245	220687.610307	46.395418
3118.251164	219522.048230	46.400423
3114.442864	218353.948368	46.405428
3110.391213	217200.915461	46.410433
3106.687015	216037.363597	46.415437
3103.119562	214885.127243	46.420442
3099.061595	213740.916959	46.425447
3095.240050	212587.123030	46.430452
3091.961708	211455.126242	46.435457
3088.053955	210306.957619	46.440461
3084.575787	209167.564597	46.445466
3080.631853	208036.399112	46.450471
3077.248413	206906.298008	46.455476
3073.241260	205774.848187	46.460481
3069.431923	204647.423200	46.465485
3066.058599	203528.010134	46.470490
3062.158773	202409.577172	46.475495
3058.574843	201280.023960	46.480500
3054.681272	200165.959593	46.485505
3050.994526	199054.392031	46.490509
3047.228985	197938.719202	46.495514
3043.289687	196837.444972	46.500519
3039.235448	195735.636952	46.505524
3035.382567	194639.409048	46.510529
3032.186188	193544.259561	46.515533
3028.087232	192462.807690	46.520538
3024.317607	191384.166224	46.525543
3020.553811	190296.646298	46.530548
3017.056589	189226.029319	46.535553
3012.738880	188153.869600	46.540557
3009.333778	187090.745635	46.545562
3005.595439	186030.408887	46.550567
3001.978713	184962.781473	46.555572
2998.126700	183902.179085	46.560577
2994.396523	182852.111084	46.565581
2990.705641	181798.432794	46.570586
2986.901077	180759.145141	46.575591
2983.218245	179718.399082	46.580596
2979.481059	178681.263855	46.585601
2975.553221	177637.626995	46.590605
2971.748705	176613.703744	46.595610
2967.623524	175592.809244	46.600615
2964.094259	174571.949385	46.605620
2960.303465	173560.232714	46.610625
2956.617677	172549.162022	46.615629
2952.689195	171542.648821	46.620634
2948.755607	170549.134250	46.625639
2944.941150	169549.758863	46.630644
2941.082230	168560.333107	46.635649
2937.534162	167580.788789	46.640653
2933.333680	166603.409051	46.645658
2929.479813	165635.701372	46.650663
2925.653865	164671.465354	46.655668
2921.604474	163716.849882	46.660673
2917.356670	162763.564702	46.665677
2913.731811	161818.571741	46.670682
2909.976489	160890.299454	46.675687
2906.050494	159960.921921	46.680692
2902.147632	159048.062414	46.685697
2898.132727	158132.510299	46.690701
2894.257870	157216.161193	46.695706
2890.218528	156331.580262	46.700711
2886.525535	155430.948391	46.705716
2882.674525	154544.799821	46.710721
2878.381864	153668.316695	46.715725
2874.623894	152804.235657	46.720730
2870.750983	151940.669448	46.725735
2866.685558	151086.716531	46.730740
2862.658024	150253.666589	46.735745
2858.520200	149417.948861	46.740749
2854.724976	148592.701955	46.745754
2850.493424	147791.802532	46.750759
2846.513351	146983.648512	46.755764
2842.076707	146195.174155	46.760769
2838.135297	145416.114599	46.765773
2834.300386	144640.676852	46.770778
2829.979396	143891.818267	46.775783
2825.675933	143146.352777	46.780788
2821.319404	142406.390728	46.785793
2817.081125	141679.590318	46.790797
2813.367413	140968.585169	46.795802
2809.225320	140285.317328	46.800807
2805.135722	139602.407352	46.805812
2801.070375	138925.063322	46.810817
2796.905589	138216.459671	46.815821
2792.901833	137519.711750	46.820826
2788.724573	136886.828722	46.825831
2784.946431	136251.945848	46.830836
2781.003306	135624.768795	46.835841
2776.947205	135016.013608	46.840845
2773.485542	134404.744358	46.845850
2769.339198	133811.692531	46.850855
2765.240439	133216.631292	46.855860
2761.487991	132640.796554	46.860865
2757.432379	132057.969222	46.865869
2753.898780	131493.106403	46.870874
2749.977939	130936.490528	46.875879
2746.830021	130374.724324	46.880884
2743.000806	129826.300534	46.885889
2739.212478	129269.240569	46.890893
2735.827874	128725.938898	46.895898
2731.794778	128189.537499	46.900903
2728.290578	127639.819655	46.905908
2724.613614	127107.358001	46.910913
2721.077488	126585.272890	46.915917
2717.939960	126050.616852	46.920922
2714.126788	125532.086023	46.925927
2710.830512	124991.121879	46.930932
2707.243567	124470.419976	46.935937
2703.629604	123945.684580	46.940941
2700.221246	123412.949757	46.945946
2696.850848	122898.237628	46.950951
2693.403728	122370.304824	46.955956
2689.802201	121841.207666	46.960961
2686.331323	121320.223827	46.965965
2683.086084	120788.478386	46.970970
2679.427912	120277.520799	46.975975
2675.877228	119741.945821	46.980980
2672.445761	119227.774924	46.985985
2668.895590	118706.202885	46.990989
2665.081563	118173.984493	46.995994
2661.536425	117665.206069	47.000999
2658.038338	117143.227841	47.006004
2654.284373	116625.938035	47.011009
2650.796356	116109.275242	47.016013
2647.243822	115598.453437	47.021018
2643.783140	115084.699853	47.026023
2640.217330	114569.431264	47.031028
2636.605239	114067.833135	47.036033
2632.731006	113551.380839	47.041037
2628.945217	113037.083641	47.046042
2625.323850	112539.703965	47.051047
2622.052019	112037.203746	47.056052
2618.794821	111538.547997	47.061057
2614.753841	111043.720984	47.066061
2611.506427	110543.984267	47.071066
2607.590181	110048.325372	47.076071
2604.240381	109551.301258	47.081076
2600.315705	109065.853777	47.086081
2596.736977	108580.664340	47.091085
2593.065587	108094.262954	47.096090
2589.316823	107611.681575	47.101095
2585.242133	107134.293574	47.106100
2581.968646	106660.804665	47.111105
2577.762648	106197.179596	47.116109
2574.149584	105739.837329	47.121114
2570.258050	105284.832717	47.126119
2566.630420	104828.255056	47.131124
2562.936511	104380.236081	47.136129
2559.014999	103933.555085	47.141133
2555.514584	103492.941348	47.146138
2551.711537	103063.973034	47.151143
2547.601260	102629.833915	47.156148
2543.994605	102199.867517	47.161153
2540.155481	101791.423772	47.166157
2536.806937	101369.778925	47.171162
2532.965885	100965.476678	47.176167
2529.729830	100545.642550	47.181172
2525.740264	100134.866192	47.186177
2522.089685	99730.206535	47.191181
2518.852220	99324.407355	47.196186
2515.538492	98925.005310	47.201191
2512.031759	98515.534403	47.206196
2508.345654	98108.676615	47.211201
2505.082910	97706.168156	47.216205
2501.902701	97300.118916	47.221210
2497.852769	96895.798820	47.226215
2494.666019	96483.546584	47.231220
2491.129933	96083.210969	47.236225
2487.818584	95684.777137	47.241229
2484.498473	95278.381852	47.246234
2481.009596	94863.402244	47.251239
2477.365684	94451.438611	47.256244
2473.918090	94047.430208	47.261249
2470.627652	93635.968872	47.266253
2467.246585	93220.194017	47.271258
2463.696082	92816.294063	47.276263
2460.223816	92392.272426	47.281268
2456.968174	91994.119067	47.286273
2453.356809	91582.176260	47.291277
2449.764643	91163.641520	47.296282
2446.353971	90741.005689	47.301287
2443.226020	90335.205262	47.306292
2439.707066	89915.075567	47.311297
2435.971843	89492.533264	47.316301
2432.873020	89076.098146	47.321306
2429.264652	88657.334176	47.326311
2425.493872	88231.270607	47.331316
2422.174770	87811.139585	47.336321
2418.450730	87391.636588	47.341325
2415.226996	86971.858462	47.346330
2411.564885	86553.247155	47.351335
2407.959594	86132.168420	47.356340
2404.784105	85709.504429	47.361345
2401.353049	85285.006222	47.366349
2398.092775	84856.054136	47.371354
2394.131592	84437.748612	47.376359
2390.581248	84000.673464	47.381364
2387.093078	83585.965277	47.386369
2383.825831	83161.472984	47.391373
2380.390774	82728.819955	47.396378
2377.285122	82307.910108	47.401383
2373.424752	81880.074241	47.406388
2369.869880	81450.660381	47.411393
2366.458833	81012.987205	47.416397
2363.412991	80584.358406	47.421402
2359.679510	80157.405475	47.426407
2356.020002	79727.475485	47.431412
2352.657216	79293.073307	47.436417
2349.157581	78858.457926	47.441421
2345.906451	78407.376071	47.446426
2341.961908	77985.696753	47.451431
2338.835266	77539.524847	47.456436
2334.934478	77109.101747	47.461441
2331.400845	76676.367731	47.466445
2328.222135	76237.133949	47.471450
2324.740256	75808.228306	47.476455
2320.927676	75369.742216	47.481460
2317.823417	74936.296133	47.486465
2313.982154	74493.460320	47.491469
2310.452264	74058.354919	47.496474
2306.857770	73626.441260	47.501479
2303.488309	73181.128380	47.506484
2299.974565	72754.003542	47.511489
2296.677133	72315.728668	47.516493
2293.519649	71872.931651	47.521498
2289.627950	71431.818117	47.526503
2286.212321	70991.031517	47.531508
2283.005955	70544.487108	47.536513
2279.247632	70111.856608	47.541517
2275.894800	69657.243340	47.546522
2272.072226	69216.867486	47.551527
2268.571800	68776.842569	47.556532
2265.450583	68334.836372	47.561537
2261.784615	67886.784209	47.566541
2258.433094	67434.507799	47.571546
2254.988483	66995.609199	47.576551
2251.442565	66543.626369	47.581556
2247.753696	66101.182173	47.586561
2244.107817	65660.878030	47.591565
2240.726645	65204.831171	47.596570
2237.214151	64763.239794	47.601575
2233.775511	64322.273020	47.606580
2230.361103	63871.104561	47.611585
2226.732694	63426.863706	47.616589
2223.270330	62977.832293	47.621594
2219.711373	62522.788532	47.626599
2216.233226	62081.315383	47.631604
2212.813822	61630.810277	47.636609
2209.525599	61184.976419	47.641613
2206.014272	60733.550111	47.646618
2202.431016	60278.799022	47.651623
2199.168596	59831.551575	47.656628
2195.599585	59373.699345	47.661633
2191.800086	58914.679607	47.666637
2188.565427	58456.037519	47.671642
2184.898496	58006.837051	47.676647
2181.236910	57548.824324	47.681652
2178.300518	57105.294734	47.686657
2174.342388	56640.188258	47.691661
2171.151159	56190.167296	47.696666
2167.744120	55732.175058	47.701671
2164.081107	55270.754648	47.706676
2160.452985	54812.903358	47.711681
2156.692043	54359.192719	47.716685
2153.165979	53911.062524	47.721690
2149.715034	53462.269385	47.726695
2145.892772	53005.580942	47.731700
2142.914844	52551.383664	47.736705
2139.920951	52090.232306	47.741709
2136.411362	51635.342643	47.746714
2132.345194	51184.506830	47.751719
2129.013431	50709.479846	47.756724
2125.221252	50255.403432	47.761729
2122.050125	49795.448077	47.766733
2118.452710	49326.751563	47.771738
2114.988065	48881.956429	47.776743
2111.281782	48421.223940	47.781748
2108.066744	47969.018499	47.786753
2104.295884	47507.363166	47.791757
2101.245794	47048.129300	47.796762
2097.627602	46582.815876	47.801767
2094.054594	46117.346464	47.806772
2090.749216	45661.078878	47.811777
2087.112974	45189.835654	47.816781
2083.489870	44724.935629	47.821786
2080.264954	44271.366369	47.826791
2076.921089	43811.591256	47.831796
2073.408046	43335.237857	47.836801
2069.933371	42869.744751	47.841805
2066.697716	42396.126794	47.846810
2062.829465	41933.923229	47.851815
2059.152359	41456.741852	47.856820
2055.685045	40987.451270	47.861825
2052.003558	40526.243794	47.866829
2048.498428	40055.787113	47.871834
2044.947576	39596.817120	47.876839
2041.411275	39131.825180	47.881844
2038.198167	38663.464474	47.886849
2034.764105	38196.422610	47.891853
2031.388046	37731.683137	47.896858
2027.539741	37268.713525	47.901863
2023.930472	36793.614866	47.906868
2020.404955	36315.648405	47.911873
2016.771568	35847.940728	47.916877
2013.491526	35390.077104	47.921882
2010.015794	34929.375998	47.926887
2006.529489	34462.683849	47.931892
2003.238218	33981.760686	47.936897
1999.133432	33523.901054	47.941901
1996.071762	33053.225246	47.946906
1992.306967	32592.626603	47.951911
1989.113358	32114.684606	47.956916
1985.912676	31647.104321	47.961921
1981.817800	31186.632486	47.966925
1978.395898	30716.407735	47.971930
1974.909703	30247.223995	47.976935
1971.365393	29781.881325	47.981940
1967.889165	29317.698267	47.986945
1964.262973	28855.836681	47.991949
1960.967850	28384.130923	47.996954
1957.573321	27914.891137	48.001959
1954.045722	27443.623488	48.006964
1950.576160	26968.923408	48.011969
1946.924829	26509.121183	48.016973
1943.287007	26041.483224	48.021978
1939.712587	25575.265476	48.026983
1936.184983	25104.255036	48.031988
1932.639096	24632.301796	48.036993
1928.717582	24172.290847	48.041997
1925.326962	23704.643443	48.047002
1921.734489	23244.938411	48.052007
1918.074926	22785.862602	48.057012
1915.142804	22324.017189	48.062017
1911.413926	21860.197063	48.067021
1908.014004	21394.917669	48.072026
1904.264710	20941.498400	48.077031
1900.765471	20472.221196	48.082036
1897.498595	20012.489971	48.087041
1894.037060	19546.795179	48.092045
1890.671231	19094.435718	48.097050
1886.786130	18635.181469	48.102055
1883.175733	18177.352032	48.107060
1879.838957	17707.944979	48.112065
1876.031387	17258.455211	48.117069
1872.759312	16791.834290	48.122074
1868.606899	16341.542411	48.127079
1865.400019	15885.373214	48.132084
1861.774321	15422.215945	48.137089
1858.529193	14978.768109	48.142093
1855.068708	14512.437725	48.147098
1851.211687	14062.957670	48.152103
1847.620854	13616.695161	48.157108
1844.591146	13156.371766	48.162113
1840.968023	12708.777454	48.167117
1837.423963	12261.054804	48.172122
1833.363383	11815.930436	48.177127
1830.164144	11354.794106	48.182132
1826.439389	10912.532277	48.187137
1822.495592	10470.004760	48.192141
1818.878253	10021.653667	48.197146
1815.179032	9562.937399	48.202151
1811.949788	9129.582799	48.207156
1808.596934	8687.138588	48.212161
1804.225777	8262.948977	48.217165
1800.676800	7838.574670	48.222170
1796.991177	7410.465051	48.227175
1793.361663	6982.704787	48.232180
1789.675761	6565.388234	48.237185
1785.524612	6146.533220	48.242189
1782.092688	5737.370587	48.247194
1778.544270	5340.824135	48.252199
1773.706134	4947.537669	48.257204
1769.444459	4575.343619	48.262209
1765.290962	4213.089336	48.267213
1761.156108	3846.583309	48.272218
1756.861463	3503.712143	48.277223
1752.794814	3167.592986	48.282228
1749.109487	2835.012100	48.287233
1744.812910	2522.912688	48.292237
1741.557375	2208.558878	48.297242
1737.057621	1905.471989	48.302247
1733.355630	1616.336267	48.307252
1729.455821	1332.228680	48.312257
1725.072178	1068.060585	48.317261
1721.172042	797.044214	48.322266
1716.755646	555.098941	48.327271
1709.793655	391.846596	48.332276
1703.831275	242.113839	48.337281
1697.631850	125.571778	48.342285
1690.574571	72.963164	48.347290
1683.260448	79.910221	48.352295
1678.490958	81.712507	48.357300
1675.101081	76.292460	48.362305
1672.562613	81.961562	48.367309
1670.284928	86.827623	48.372314
1667.957824	74.345287	48.377319
1664.762922	76.424514	48.382324
1662.320524	69.961675	48.387329
1659.167709	75.324603	48.392333
1655.794118	76.422420	48.397338
1652.311771	79.100034	48.402343
1648.663629	78.196831	48.407348
1646.148795	76.130161	48.412353
1642.927316	76.302648	48.417357
1639.604768	68.303202	48.422362
1635.729513	77.065661	48.427367
1631.351478	82.296591	48.432372
1628.915442	69.945112	48.437377
1625.509240	79.359056	48.442381
1622.041217	73.849942	48.447386
1618.852852	80.259264	48.452391
1615.648963	77.205202	48.457396
1612.376462	68.916401	48.462401
1608.837665	77.528419	48.467405
1605.396887	73.815214	48.472410
1601.833337	67.375026	48.477415
1597.777110	69.733846	48.482420
1595.028111	73.309707	48.487425
1591.475115	73.764747	48.492429
1587.928628	82.922122	48.497434
1584.858029	79.891608	48.502439
1581.194749	78.819928	48.507444
1577.933023	72.535241	48.512449
1574.213470	84.481465	48.517453
1570.788739	77.902614	48.522458
1567.368815	77.805443	48.527463
1564.083809	74.896888	48.532468
1560.610157	72.346720	48.537473
1556.727341	84.941604	48.542477
1553.257299	74.554384	48.547482
1550.227783	75.902371	48.552487
1546.751932	82.103346	48.557492
1543.376028	84.587234	48.562497
1539.751936	79.595959	48.567501
1536.309747	70.647057	48.572506
1532.991390	68.930085	48.577511
1529.211494	76.228730	48.582516
1525.773346	70.344828	48.587521
1521.968054	62.632509	48.592525
1518.577978	76.140931	48.597530
1515.224447	75.824627	48.602535
1511.963767	71.697431	48.607540
1508.730435	68.246176	48.612545
1505.192823	78.041235	48.617549
1501.738055	72.957175	48.622554
1497.948912	79.172113	48.627559
1494.591456	75.721194	48.632564
1491.286963	76.548846	48.637569
1487.663919	79.071204	48.642573
1483.907662	63.204733	48.647578
1481.035668	70.593016	48.652583
1477.438179	77.192568	48.657588
1473.852784	70.955112	48.662593
1470.407381	72.371000	48.667597
1466.434316	69.854284	48.672602
1462.914217	75.865999	48.677607
1459.436102	82.206532	48.682612
1456.396429	68.645595	48.687617
1453.223742	76.017409	48.692621
1449.457926	70.171864	48.697626
1445.836998	73.823335	48.702631
1442.101210	75.961455	48.707636
1438.786609	67.619126	48.712641
1435.007006	68.729536	48.717645
1431.856499	75.996660	48.722650
1428.670028	65.081286	48.727655
1424.836291	66.500675	48.732660
1421.404742	66.889373	48.737665
1417.602665	72.157217	48.742669
1414.523944	64.135677	48.747674
1410.739497	64.177515	48.752679
1407.195759	67.158925	48.757684
1404.142537	67.143896	48.762689
1400.267295	70.929864	48.767693
1396.824385	66.812066	48.772698
1393.506061	69.540097	48.777703
1389.988139	74.134140	48.782708
1386.345699	74.147549	48.787713
1382.791072	63.504620	48.792717
1379.897318	67.618703	48.797722
1376.339517	70.453611	48.802727
1372.426258	67.184131	48.807732
1369.039949	72.051913	48.812737
1365.287948	75.764920	48.817741
1361.924970	72.175676	48.822746
1358.541964	69.921466	48.827751
1355.111959	77.643377	48.832756
1351.542638	71.156669	48.837761
1348.107232	69.208004	48.842765
1344.339949	74.483093	48.847770
1340.899904	64.796754	48.852775
1337.362840	74.107683	48.857780
1334.448560	73.106107	48.862785
1330.655305	76.474368	48.867789
1327.140775	67.388071	48.872794
1323.668271	62.373238	48.877799
1319.789165	72.626404	48.882804
1316.687728	70.280917	48.887809
1313.152321	72.372040	48.892813
1309.216308	75.626485	48.897818
1306.258249	68.952895	48.902823
1302.514716	72.272290	48.907828
1299.133025	72.811424	48.912833
1295.758733	59.093808	48.917837
1291.930522	65.666004	48.922842
1288.909387	65.740901	48.927847
1285.076063	70.719394	48.932852
1281.494109	73.409376	48.937857
1277.958087	72.776658	48.942861
1274.324139	72.314204	48.947866
1270.608062	68.042793	48.952871
1267.392973	74.554360	48.957876
1264.342200	60.887631	48.962881
1260.666531	65.436632	48.967885
1256.792707	65.796114	48.972890
1254.141304	73.931498	48.977895
1250.175640	76.241456	48.982900
1246.631612	68.991543	48.987905
1243.163571	67.718673	48.992909
1239.615997	64.357493	48.997914
1235.764322	66.501014	49.002919
1232.127014	70.819426	49.007924
1229.059489	66.709658	49.012929
1226.127903	74.100896	49.017933
1222.348232	72.016010	49.022938
1218.611895	70.069910	49.027943
1214.772076	78.184639	49.032948
1211.612322	71.937918	49.037953
1207.912244	73.747804	49.042957
1204.739873	68.806490	49.047962
1201.656266	61.475431	49.052967
1197.660610	68.048387	49.057972
1194.157691	65.778063	49.062977
1190.335484	67.616451	49.067981
1186.929344	72.503149	49.072986
1183.852944	61.216358	49.077991
1180.083658	73.992876	49.082996
1176.524244	72.379903	49.088001
1173.137140	70.695818	49.093005
1169.403070	66.892286	49.098010
1166.158905	71.393112	49.103015
1162.501692	65.859735	49.108020
1158.943773	66.616135	49.113025
1155.654896	68.637261	49.118029
1152.235134	70.469958	49.123034
1148.892707	72.913863	49.128039
1144.801365	70.364984	49.133044
1141.915040	57.337062	49.138049
1138.044717	66.870706	49.143053
1134.268290	62.017102	49.148058
1130.746571	62.910236	49.153063
1127.197151	73.213328	49.158068
1124.193349	67.663668	49.163073
1121.101148	62.738362	49.168077
1117.225927	66.919811	49.173082
1114.317988	66.882195	49.178087
1110.024046	68.009426	49.183092
1106.425531	71.220846	49.188097
1102.751435	67.145402	49.193101
1099.464903	66.733293	49.198106
1096.311606	67.553265	49.203111
1092.313806	74.385986	49.208116
1089.262904	62.383414	49.213121
1085.557958	62.033272	49.218125
1081.774908	64.634352	49.223130
1078.778971	68.406861	49.228135
1075.090735	64.751230	49.233140
1071.765242	59.577514	49.238145
1067.990199	69.947362	49.243149
1064.470892	65.313168	49.248154
1061.121351	56.457504	49.253159
1057.434733	63.997906	49.258164
1054.301299	64.748353	49.263169
1050.660302	68.750984	49.268173
1046.489768	68.311971	49.273178
1043.797077	58.983913	49.278183
1040.254036	71.215861	49.283188
1037.043519	64.262078	49.288193
1033.342907	68.795998	49.293197
1029.420715	61.737866	49.298202
1025.881143	55.477538	49.303207
1022.073158	69.699554	49.308212
1019.139422	68.868714	49.313217
1015.860900	59.473666	49.318221
1012.015485	63.220223	49.323226
1008.377804	66.858517	49.328231
1005.034708	65.072693	49.333236
1001.444029	62.822382	49.338241
997.980145	62.083558	49.343245
994.625032	64.864802	49.348250
991.126056	63.482886	49.353255
987.196421	68.223298	49.358260
983.854333	66.848598	49.363265
980.247790	63.923731	49.368269
976.779590	63.935375	49.373274
974.051367	56.916022	49.378279
969.956943	62.896940	49.383284
966.246534	58.918919	49.388289
962.740977	68.674195	49.393293
959.505188	70.823114	49.398298
956.348077	62.127333	49.403303
952.442844	66.791186	49.408308
949.343082	65.476843	49.413313
945.757234	64.601990	49.418317
941.886764	61.294279	49.423322
938.351818	59.202978	49.428327
934.606252	62.557521	49.433332
931.680664	52.724750	49.438337
928.165764	61.276115	49.443341
924.377891	63.087042	49.448346
921.128632	52.083475	49.453351
917.267169	54.962526	49.458356
913.759394	57.520773	49.463361
910.522755	62.520303	49.468365
906.816751	62.698683	49.473370
903.544850	58.377172	49.478375
899.824289	62.097978	49.483380
896.501076	52.577039	49.488385
893.225299	55.915403	49.493389
889.407389	56.705977	49.498394
886.033732	58.455592	49.503399
881.949636	60.720750	49.508404
878.872519	61.497247	49.513409
875.746952	52.521336	49.518413
871.757148	60.744843	49.523418
868.821308	57.763044	49.528423
865.011639	67.967450	49.533428
861.378184	47.399789	49.538433
857.864534	55.922488	49.543437
854.499606	55.051222	49.548442
850.870220	64.604318	49.553447
847.336142	65.287440	49.558452
844.007108	55.818035	49.563457
840.815244	54.435788	49.568461
836.898384	65.346562	49.573466
833.623415	49.655280	49.578471
829.761489	63.727506	49.583476
826.304907	57.770661	49.588481
822.603545	58.675975	49.593485
819.328964	61.615536	49.598490
816.221977	57.366441	49.603495
812.330881	61.604171	49.608500
808.985549	59.223949	49.613505
805.491905	55.825966	49.618509
801.710429	54.658890	49.623514
798.281482	58.084379	49.628519
794.627895	61.288580	49.633524
791.254225	59.387324	49.638529
787.936043	58.916903	49.643533
784.523865	58.537044	49.648538
781.242411	50.230808	49.653543
777.165032	60.992567	49.658548
773.477139	55.717129	49.663553
770.373582	58.085919	49.668557
766.669586	56.014630	49.673562
763.642765	57.843141	49.678567
760.086690	63.888967	49.683572
756.445930	59.618570	49.688577
752.895578	58.994475	49.693581
749.031928	53.616692	49.698586
745.937322	57.774730	49.703591
742.241338	59.087331	49.708596
738.568544	52.224549	49.713601
735.884838	56.672955	49.718605
731.626187	57.848526	49.723610
728.226781	46.115422	49.728615
724.486537	58.757705	49.733620
721.446217	56.826711	49.738625
718.045555	57.204349	49.743629
714.487298	55.698825	49.748634
711.252969	55.882896	49.753639
707.005131	58.423495	49.758644
703.587360	54.377817	49.763649
700.203490	56.831377	49.768653
696.410151	62.113732	49.773658
693.342671	56.662636	49.778663
689.562351	61.326049	49.783668
686.414715	63.097447	49.788673
683.260982	56.305727	49.793677
679.372946	52.965995	49.798682
676.070467	59.662029	49.803687
671.865451	62.129529	49.808692
668.569115	63.667819	49.813697
665.014889	60.823439	49.818701
661.582665	63.056747	49.823706
658.176391	61.878738	49.828711
654.657651	72.063175	49.833716
651.503557	56.903596	49.838721
647.929600	51.142222	49.843725
644.231715	56.903254	49.848730
640.635447	54.967070	49.853735
636.926466	65.351958	49.858740
633.635322	59.176408	49.863745
630.565329	60.486482	49.868749
626.984309	66.814605	49.873754
623.285289	52.413730	49.878759
619.655895	58.170429	49.883764
616.148930	62.509728	49.888769
612.869303	64.728777	49.893773
609.062763	64.081309	49.898778
605.729434	61.319606	49.903783
601.936887	65.415470	49.908788
598.116976	58.189646	49.913793
595.296685	62.162628	49.918797
591.923211	66.012925	49.923802
588.637814	57.795919	49.928807
584.696758	59.994555	49.933812
581.053130	55.022301	49.938817
577.489691	62.796651	49.943821
574.007840	67.400957	49.948826
570.819251	51.183779	49.953831
566.962884	60.920914	49.958836
563.821692	53.709659	49.963841
560.000955	60.144704	49.968845
556.435608	65.404235	49.973850
553.460975	62.969504	49.978855
549.999873	60.657959	49.983860
546.365776	68.633134	49.988865
542.674549	60.586878	49.993869
538.928900	66.342703	49.998874
535.611010	61.503238	50.003879
532.149195	67.047203	50.008884
528.601635	59.870741	50.013889
525.273919	57.845312	50.018893
521.564523	67.379244	50.023898
518.671634	58.904999	50.028903
514.442338	67.232255	50.033908
511.013510	68.557077	50.038913
507.601696	63.254524	50.043917
503.704952	64.278877	50.048922
500.458719	53.936135	50.053927
496.978486	59.103327	50.058932
493.672291	56.134943	50.063937
490.283389	58.023011	50.068941
486.471435	61.346810	50.073946
483.240877	51.153488	50.078951
479.428363	64.246782	50.083956
475.997153	57.596369	50.088961
472.674744	56.620460	50.093965
468.846832	60.114419	50.098970
465.708761	64.620923	50.103975
461.907866	66.323205	50.108980
458.749613	56.653289	50.113985
455.351385	54.774885	50.118989
451.462292	64.264031	50.123994
448.028945	56.854676	50.128999
444.093868	60.678524	50.134004
440.850617	60.734306	50.139009
437.835028	60.824246	50.144013
434.491213	59.933929	50.149018
430.681396	53.206430	50.154023
426.954176	63.309437	50.159028
423.609432	69.373010	50.164033
420.073815	59.417009	50.169037
416.162994	58.149907	50.174042
412.964051	57.689444	50.179047
409.673198	53.497510	50.184052
406.504531	52.814041	50.189057
402.404442	49.744646	50.194061
398.692497	54.419587	50.199066
395.462136	45.874527	50.204071
392.076216	55.715596	50.209076
388.446669	58.719950	50.214081
385.646270	54.904069	50.219085
381.597643	52.187323	50.224090
377.898348	51.029663	50.229095
374.126467	62.088725	50.234100
371.093062	56.075571	50.239105
367.414892	48.701187	50.244109
363.454185	56.366559	50.249114
360.553761	55.404060	50.254119
356.986680	49.916909	50.259124
353.449093	55.760576	50.264129
350.346792	52.741489	50.269133
346.424552	57.787688	50.274138
343.253699	51.080952	50.279143
339.528652	48.364457	50.284148
335.913349	52.521336	50.289153
332.292420	49.393176	50.294157
328.262888	58.347386	50.299162
325.489812	47.972150	50.304167
321.870899	50.854636	50.309172
318.629502	60.919977	50.314177
314.850251	55.098878	50.319181
311.270365	54.147258	50.324186
307.859198	53.235809	50.329191
304.347892	61.947996	50.334196
300.875323	59.622457	50.339201
297.884822	55.703310	50.344205
293.589657	56.599902	50.349210
290.500289	54.300126	50.354215
286.713841	49.590601	50.359220
283.182054	54.110960	50.364225
280.002909	50.385697	50.369229
276.522430	62.389623	50.374234
273.072096	51.559866	50.379239
269.467160	51.181611	50.384244
265.631890	51.392858	50.389249
262.820895	47.199006	50.394253
258.424098	55.742178	50.399258
255.185233	39.254520	50.404263
251.967851	44.270080	50.409268
248.459174	55.104675	50.414273
245.263418	50.129193	50.419277
240.975738	50.395060	50.424282
237.823065	46.592919	50.429287
234.455574	56.798111	50.434292
230.684323	51.124478	50.439297
227.718201	47.802644	50.444301
224.274517	53.296354	50.449306
220.474079	45.260851	50.454311
216.544547	51.678062	50.459316
212.899606	58.981086	50.464321
209.555793	49.074368	50.469325
206.657712	49.949611	50.474330
203.073453	54.867278	50.479335
199.476308	51.159651	50.484340
195.925405	53.329232	50.489345
192.385267	46.325689	50.494349
188.621569	51.204857	50.499354
185.403444	51.335851	50.504359
181.946007	56.243266	50.509364
178.234610	58.577039	50.514369
174.798063	57.343703	50.519373
171.172252	56.263217	50.524378
167.656000	44.852147	50.529383
164.283702	45.019802	50.534388
160.574481	52.899130	50.539393
156.860896	54.211384	50.544397
153.612086	47.937588	50.549402
150.581689	54.164202	50.554407
147.038432	56.130125	50.559412
143.323685	52.782492	50.564417
139.989675	52.479131	50.569421
135.977623	51.174057	50.574426
132.571399	42.469777	50.579431
129.344981	51.403363	50.584436
125.818319	49.045149	50.589441
122.269598	47.626813	50.594445
118.364671	51.699098	50.599450
115.278505	53.514768	50.604455
111.735067	45.989753	50.609460
108.128966	54.805291	50.614465
105.020002	50.237088	50.619469
101.067008	48.242639	50.624474
98.084798	42.702443	50.629479
94.019121	48.998500	50.634484
90.462188	43.522477	50.639489
87.182445	41.976850	50.644493
84.090823	46.055386	50.649498
80.547107	44.522385	50.654503
76.954325	46.726975	50.659508
72.943371	40.274475	50.664513
69.786640	40.642691	50.669517
66.123918	51.314621	50.674522
62.883311	38.981169	50.679527
59.191990	47.531574	50.684532
55.501850	42.718520	50.689537
52.279921	43.963731	50.694541
48.689977	46.689885	50.699546
45.244326	45.135295	50.704551
41.531843	45.896918	50.709556
37.801914	51.264375	50.714561
34.446872	49.746297	50.719565
30.791467	54.627604	50.724570
27.566035	47.635206	50.729575
24.197429	47.460632	50.734580
20.317297	52.414893	50.739585
17.082118	49.840477	50.744589
13.388150	50.013945	50.749594
10.267015	48.209523	50.754599
6.554592	51.059154	50.759604
3.108623	51.437612	50.764609