Fri Aug 26 11:22:53 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.684299	102.953013	0.000000
1.481579	99.270544	0.005005
1.033845	95.173820	0.010010
1.096210	77.257899	0.015014
1.073595	81.677998	0.020019
0.709659	83.538056	0.025024
0.966352	73.561145	0.030029
0.365194	73.354305	0.035034
-0.364425	55.394041	0.040038
-0.514914	57.809304	0.045043
-0.597361	43.696533	0.050048
-0.733785	41.550780	0.055053
-1.270782	39.014993	0.060058
-1.299021	33.900710	0.065062
-1.353283	35.408838	0.070067
-1.697282	26.113918	0.075072
-1.745798	18.702823	0.080077
-2.469329	11.937813	0.085082
-2.597926	0.138561	0.090086
-2.986995	-4.925858	0.095091
-3.442417	2.731579	0.100096
-3.383652	-9.270839	0.105101
-3.931021	1.238703	0.110106
-3.999541	-7.728944	0.115110
-4.305310	-6.700498	0.120115
-5.068579	-11.102397	0.125120
-5.025247	-20.093780	0.130125
-5.549096	-3.694037	0.135130
-5.461051	-14.910099	0.140134
-5.716616	-14.016016	0.145139
-5.734991	-10.147074	0.150144
-5.714673	-17.246179	0.155149
-6.652221	-12.237578	0.160154
-6.735313	-19.269964	0.165158
-6.386330	-11.380284	0.170163
-7.251923	-10.153948	0.175168
-7.788394	-21.203170	0.180173
-7.931761	-12.025159	0.185178
-8.490716	-16.237412	0.190182
-8.261462	-18.497038	0.195187
-8.422098	-11.628960	0.200192
-8.272153	-12.743654	0.205197
-8.747548	-4.320671	0.210202
-9.144113	-8.080500	0.215206
-9.598796	-7.655271	0.220211
-9.946850	-10.309050	0.225216
-9.838683	-19.781910	0.230221
-10.105541	-10.856743	0.235226
-10.176424	-15.951718	0.240230
-10.728671	-14.286968	0.245235
-11.326632	-5.816430	0.250240
-11.056342	-14.738752	0.255245
-11.461615	-12.644484	0.260250
-11.362777	-19.312904	0.265254
-12.097751	-23.902696	0.270259
-12.286289	-16.498784	0.275264
-12.682927	-14.529243	0.280269
-12.566238	-12.554208	0.285274
-12.833153	-13.148433	0.290278
-13.170895	-8.992493	0.295283
-14.068889	-7.175838	0.300288
-13.633789	-18.363678	0.305293
-14.114362	-14.555647	0.310298
-14.189373	-5.606567	0.315302
-14.151612	-13.742901	0.320307
-14.422185	-14.732012	0.325312
-14.861234	-22.411303	0.330317
-15.146956	-20.949396	0.335322
-15.220137	-22.301423	0.340326
-15.505371	-17.745551	0.345331
-16.095497	-16.346977	0.350336
-16.489931	-14.697307	0.355341
-16.679507	-11.421784	0.360346
-17.072321	-6.798541	0.365350
-16.678087	-1.181072	0.370355
-16.917998	-10.783233	0.375360
-17.464167	-15.880133	0.380365
-18.325351	-11.804041	0.385370
-18.342711	-12.104939	0.390374
-18.359555	-1.013636	0.395379
-18.332096	-3.330427	0.400384
-18.096084	4.437648	0.405389
-18.847538	0.726745	0.410394
-19.472154	-3.427833	0.415398
-19.691853	-5.244249	0.420403
-20.088945	-1.692814	0.425408
-19.656529	1.887651	0.430413
-19.902346	4.748005	0.435418
-20.510083	-5.736491	0.440422
-20.797159	-3.692262	0.445427
-21.140033	3.900197	0.450432
-21.213331	1.073928	0.455437
-21.129859	-5.079593	0.460442
-21.265169	-7.282458	0.465446
-21.831188	-2.860029	0.470451
-22.445090	-0.787059	0.475456
-22.079366	-9.297150	0.480461
-23.226776	3.197676	0.485466
-23.930753	0.333566	0.490470
-23.166565	3.400483	0.495475
-23.900771	0.367079	0.500480
-23.513055	-12.287644	0.505485
-23.968089	-3.592595	0.510490
-24.165954	-1.508474	0.515494
-23.867427	-9.312100	0.520499
-25.085100	-3.231698	0.525504
-24.963877	-5.626359	0.530509
-25.480602	3.916663	0.535514
-25.820429	-1.421168	0.540518
-25.775902	-5.528075	0.545523
-26.129173	-4.115759	0.550528
-25.553482	-6.900709	0.555533
-26.560706	-11.448114	0.560538
-27.115917	-12.756727	0.565542
-27.006788	-8.534328	0.570547
-27.195806	-4.211725	0.575552
-27.175750	-16.790219	0.580557
-27.999992	-13.887263	0.585562
-28.288849	-9.973045	0.590566
-28.593820	-10.678399	0.595571
-28.476849	-11.215340	0.600576
-28.876127	-17.179803	0.605581
-28.950010	-9.189484	0.610586
-28.643647	-14.684868	0.615590
-29.233379	-12.065189	0.620595
-30.039919	-7.703385	0.625600
-29.964628	-10.783733	0.630605
-29.939391	-2.233061	0.635610
-30.784021	-14.657945	0.640614
-31.317045	-8.475342	0.645619
-31.782682	-7.671933	0.650624
-31.693287	-14.971611	0.655629
-31.969397	-9.120065	0.660634
-31.858356	-16.223804	0.665638
-31.624010	-23.365720	0.670643
-31.850356	-6.718086	0.675648
-31.813448	-23.437244	0.680653
-32.620983	-11.064947	0.685658
-32.923283	-14.741377	0.690662
-33.192112	-14.237520	0.695667
-33.524689	-20.766004	0.700672
-33.515009	-20.732602	0.705677
-34.049547	-15.577950	0.710682
-34.656964	-11.829260	0.715686
-34.312284	-16.644099	0.720691
-34.506302	-16.661236	0.725696
-35.142292	-15.315630	0.730701
-36.000415	-15.703914	0.735706
-36.065331	-10.647688	0.740710
-35.725468	-18.900655	0.745715
-35.884922	-11.994799	0.750720
-35.808962	-17.919363	0.755725
-36.088064	-17.211434	0.760730
-36.700818	-7.061865	0.765734
-37.132629	-18.829709	0.770739
-37.404900	-13.143271	0.775744
-37.467652	-19.055729	0.780749
-37.403000	-8.147958	0.785754
-38.168677	-17.750506	0.790758
-38.459982	-18.764862	0.795763
-38.737948	-15.823578	0.800768
-39.086046	-20.853243	0.805773
-38.999760	-11.657208	0.810778
-39.190856	-8.084066	0.815782
-39.070337	-6.944828	0.820787
-39.930152	-6.269864	0.825792
-40.168907	-11.484229	0.830797
-40.498822	-8.104601	0.835802
-40.303176	-5.129492	0.840806
-40.686216	-10.960448	0.845811
-41.622536	-6.780911	0.850816
-41.787434	-15.540562	0.855821
-41.972907	-19.564200	0.860826
-41.915362	-9.012814	0.865830
-41.569077	-12.780738	0.870835
-42.165089	-14.443652	0.875840
-42.231937	-13.230951	0.880845
-42.649009	-3.042247	0.885850
-43.362008	-8.711102	0.890854
-43.222976	-10.545407	0.895859
-43.385546	-18.172835	0.900864
-43.362802	-6.568865	0.905869
-44.300243	-11.260007	0.910874
-44.880772	-11.311875	0.915878
-44.932095	-27.008088	0.920883
-45.151491	-4.309492	0.925888
-44.763503	-6.239506	0.930893
-44.650810	-5.307850	0.935898
-45.282926	-6.503252	0.940902
-45.859548	-7.723111	0.945907
-46.556506	-4.751390	0.950912
-46.487925	-10.491316	0.955917
-46.524892	-4.132857	0.960922
-46.576379	-5.576844	0.965926
-46.768836	-10.833216	0.970931
-47.425610	-7.896225	0.975936
-47.628140	-2.644571	0.980941
-48.029733	-7.324236	0.985946
-48.270667	-4.303298	0.990950
-48.059761	-4.661882	0.995955
-48.775233	0.223563	1.000960
-48.856295	-10.830131	1.005965
-49.200575	-5.679789	1.010970
-49.346931	4.397167	1.015974
-49.075715	-6.268468	1.020979
-49.550843	-9.959117	1.025984
-49.622626	-6.154624	1.030989
-50.501538	-2.961590	1.035994
-50.886213	-7.621743	1.040998
-50.227562	-8.970661	1.046003
-51.289996	2.913004	1.051008
-51.844969	-4.726097	1.056013
-52.229472	-3.299427	1.061018
-51.746264	-3.773173	1.066022
-52.126840	-7.203307	1.071027
-52.353386	-4.886938	1.076032
-52.626030	-4.195832	1.081037
-52.634989	-1.372358	1.086042
-52.533191	-5.434399	1.091046
-53.368054	-6.990524	1.096051
-53.619750	1.074937	1.101056
-53.753972	-9.682589	1.106061
-54.007559	-9.402560	1.111066
-54.464592	-1.064692	1.116070
-54.969409	-14.535864	1.121075
-55.348393	-18.779300	1.126080
-55.187970	-15.004636	1.131085
-55.394657	-11.489177	1.136090
-55.742111	-12.390389	1.141094
-55.582328	-17.189093	1.146099
-55.695485	-3.245013	1.151104
-56.044614	-15.145949	1.156109
-56.842473	-12.069937	1.161114
-56.964441	-9.845779	1.166118
-57.084043	-14.923675	1.171123
-56.965392	-7.716282	1.176128
-57.338302	-9.322187	1.181133
-58.107391	-7.440183	1.186138
-58.583313	-6.072043	1.191142
-58.602551	-20.387581	1.196147
-58.531885	-10.385550	1.201152
-58.582681	-2.069807	1.206157
-58.451771	-11.242499	1.211162
-59.470594	-12.592817	1.216166
-59.613625	-8.293194	1.221171
-60.114766	-16.238053	1.226176
-60.206455	-6.884598	1.231181
-60.133844	-20.265343	1.236186
-60.462116	-14.962479	1.241190
-60.837976	-19.649310	1.246195
-61.719884	-14.858173	1.251200
-61.713757	-12.005413	1.256205
-61.309661	-16.873793	1.261210
-61.552125	-20.398192	1.266214
-61.608865	-23.325106	1.271219
-62.329464	-9.153580	1.276224
-62.553519	-16.723980	1.281229
-62.778066	-21.165461	1.286234
-63.125154	-16.346868	1.291238
-63.508405	-20.377674	1.296243
-63.922113	-7.829423	1.301248
-64.016898	-7.058445	1.306253
-64.055135	-10.576680	1.311258
-64.408848	-15.421979	1.316262
-63.897251	-18.117857	1.321267
-64.903129	-9.960284	1.326272
-64.974442	-10.724164	1.331277
-65.167127	-10.130926	1.336282
-65.771855	-8.780695	1.341286
-65.654581	-15.749366	1.346291
-66.969860	-9.046349	1.351296
-66.720526	-12.194922	1.356301
-66.992205	-10.178400	1.361306
-66.899610	-2.704366	1.366310
-66.944332	-17.025428	1.371315
-67.108235	-6.740110	1.376320
-66.769836	-11.531826	1.381325
-67.902630	-3.104562	1.386330
-68.402249	-3.982083	1.391334
-68.441917	-9.562790	1.396339
-68.496627	-9.690199	1.401344
-68.466075	-7.496116	1.406349
-69.179436	-6.037226	1.411354
-69.953054	-9.567507	1.416358
-70.208740	-16.183890	1.421363
-70.311356	-2.956435	1.426368
-70.434412	-10.105980	1.431373
-70.487404	-11.312459	1.436378
-70.757025	-2.905700	1.441382
-70.147198	-17.901293	1.446387
-70.402887	-8.876633	1.451392
-70.843870	-10.285283	1.456397
-71.162674	-8.460734	1.461402
-72.045756	-8.509784	1.466406
-72.449420	-18.583131	1.471411
-72.959839	-8.759535	1.476416
-72.802697	-13.659065	1.481421
-72.846482	-17.644653	1.486426
-73.238002	-8.738044	1.491430
-72.838687	-18.442886	1.496435
-73.212518	-5.078296	1.501440
-74.003335	-9.301901	1.506445
-74.352061	-16.587143	1.511450
-74.551636	-9.478896	1.516454
-74.504192	-11.729196	1.521459
-74.625852	-15.667859	1.526464
-75.363020	-16.236319	1.531469
-75.368061	-15.036406	1.536474
-75.724707	-6.261771	1.541478
-75.879455	-17.911404	1.546483
-76.182777	-6.984306	1.551488
-76.249367	-6.050046	1.556493
-76.738272	-13.534918	1.561498
-77.520609	-7.917754	1.566502
-77.234680	-16.390104	1.571507
-77.686513	-8.919888	1.576512
-77.803308	-13.802075	1.581517
-77.439998	-16.623555	1.586522
-77.695422	-7.250935	1.591526
-77.936299	-11.980930	1.596531
-78.606126	-15.704534	1.601536
-78.817196	-19.436293	1.606541
-79.000838	-16.769115	1.611546
-79.766544	-21.480664	1.616550
-80.058497	-22.570844	1.621555
-80.665908	-12.972586	1.626560
-80.350407	-11.423963	1.631565
-80.546863	-22.747570	1.636570
-80.891893	-20.267229	1.641574
-80.728216	-19.188494	1.646579
-81.002859	-9.705319	1.651584
-80.894378	-15.812110	1.656589
-81.213121	-15.360590	1.661594
-82.216935	-15.004878	1.666598
-82.069659	-17.748430	1.671603
-82.182682	-9.609658	1.676608
-82.544481	-11.492529	1.681613
-83.367638	-14.565859	1.686618
-83.881973	-13.343593	1.691622
-83.467840	-13.322547	1.696627
-83.960002	-7.617690	1.701632
-84.172554	-10.514019	1.706637
-83.901665	-12.697873	1.711642
-83.805085	-2.288602	1.716646
-84.052235	-17.372217	1.721651
-85.029350	-9.345669	1.726656
-85.236890	-11.341140	1.731661
-85.059954	-15.585714	1.736666
-85.414656	-7.023346	1.741670
-86.367773	-4.362905	1.746675
-86.567478	-2.749881	1.751680
-86.720585	-5.671284	1.756685
-86.403783	-16.166844	1.761690
-86.689474	-7.700641	1.766694
-86.545433	-7.836850	1.771699
-87.328905	-0.299177	1.776704
-88.221782	-9.091008	1.781709
-87.852894	-7.474769	1.786714
-88.183695	4.908725	1.791718
-88.050894	-7.870814	1.796723
-88.934685	1.792629	1.801728
-89.765722	-0.029837	1.806733
-89.437202	-1.846192	1.811738
-90.038391	3.075242	1.816742
-89.575945	-5.965579	1.821747
-89.790399	5.020452	1.826752
-90.090466	7.553906	1.831757
-89.748286	-1.025283	1.836762
-90.648714	4.879182	1.841766
-91.086777	-2.490228	1.846771
-91.604870	-5.917931	1.851776
-91.414230	-0.746476	1.856781
-91.222180	2.033045	1.861786
-91.715802	0.417462	1.866790
-92.168707	2.607730	1.871795
-92.689833	-2.243141	1.876800
-92.462471	-4.559419	1.881805
-92.246128	-6.038779	1.886810
-93.205163	1.459794	1.891814
-94.026889	-2.885545	1.896819
-94.117687	1.507183	1.901824
-94.103158	-9.662627	1.906829
-94.103259	0.717407	1.911834
-94.114524	-0.410150	1.916838
-94.104155	-1.759367	1.921843
-95.065191	0.551144	1.926848
-95.560167	-4.974490	1.931853
-95.774817	-10.929733	1.936858
-95.929167	-10.921410	1.941862
-95.936618	-7.898864	1.946867
-95.849856	-1.208506	1.951872
-96.165422	-2.991013	1.956877
-96.437681	-13.224020	1.961882
-97.216086	-1.390912	1.966886
-97.217037	-1.729164	1.971891
-97.658736	-3.295886	1.976896
-97.311549	-3.928781	1.981901
-97.952108	-8.874945	1.986906
-98.504230	-7.808141	1.991910
-98.423019	-7.792204	1.996915
-98.434367	-5.062727	2.006912
-98.740628	-6.855254	2.016909
-98.098072	-2.209879	2.026906
-97.478397	-5.407317	2.036902
-96.980470	-9.545609	2.046899
-96.220545	-3.331495	2.056896
-96.113326	-7.842928	2.066893
-95.898764	-5.322957	2.076890
-95.130090	-5.448759	2.086886
-94.509405	-5.285432	2.096883
-93.448002	-3.540357	2.106880
-93.593270	-11.696502	2.116877
-93.187512	-6.665813	2.126874
-92.503642	-2.913825	2.136870
-92.170618	-2.940118	2.146867
-91.128431	-4.980612	2.156864
-90.988329	-4.061403	2.166861
-90.678404	-5.915026	2.176858
-89.669739	-16.160957	2.186854
-89.242089	-13.940252	2.196851
-89.302374	-8.086257	2.206848
-88.643817	-5.575230	2.216845
-87.544340	-7.434582	2.226842
-87.724195	-7.539404	2.236838
-86.950133	-12.800873	2.246835
-86.408653	-11.354969	2.256832
-85.989110	-1.698426	2.266829
-84.996975	-17.219159	2.276826
-85.077284	-10.132983	2.286822
-84.898563	-10.958850	2.296819
-83.930026	-12.297319	2.306816
-83.344502	-12.074666	2.316813
-82.722621	-11.224136	2.326810
-82.148690	-11.826446	2.336806
-82.211722	-16.780187	2.346803
-81.767895	-7.852829	2.356800
-81.135574	-9.858015	2.366797
-80.394427	-17.214537	2.376794
-79.885306	-11.059573	2.386790
-79.402129	-7.051431	2.396787
-78.701075	-7.334591	2.406784
-77.940787	-9.635290	2.416781
-78.078726	-16.177053	2.426778
-77.775650	-9.223426	2.436774
-76.640856	-5.465621	2.446771
-76.218047	-10.875133	2.456768
-76.120912	-12.350345	2.466765
-75.577420	-8.006316	2.476762
-74.752743	-8.033134	2.486758
-74.493764	-10.236774	2.496755
-73.819047	-7.775779	2.506752
-73.532536	-9.283645	2.516749
-73.365607	-9.879603	2.526746
-72.406128	-12.071938	2.536742
-71.892674	-9.177202	2.546739
-71.094432	-9.488165	2.556736
-70.938156	-15.581577	2.566733
-70.731778	-13.364432	2.576730
-69.542699	-16.226053	2.586726
-69.301118	-12.569921	2.596723
-69.278351	-11.562755	2.606720
-68.202024	-15.797438	2.616717
-67.691137	-13.535841	2.626714
-67.570255	-14.460405	2.636710
-66.433515	-10.398805	2.646707
-66.329616	-9.093837	2.656704
-66.197515	-11.436106	2.666701
-65.320952	-9.427841	2.676698
-64.833929	-14.967722	2.686694
-64.796629	-17.719701	2.696691
-63.869968	-12.950674	2.706688
-63.694504	-15.160316	2.716685
-62.971088	-17.803720	2.726682
-62.220024	-12.472013	2.736678
-62.040843	-15.892292	2.746675
-61.367700	-4.833933	2.756672
-61.130931	-8.906222	2.766669
-59.792970	-11.090965	2.776666
-59.648225	-5.256219	2.786662
-59.426368	-14.457848	2.796659
-59.295689	-10.087555	2.806656
-58.298368	-10.185602	2.816653
-58.207967	-9.328344	2.826650
-56.938033	-11.822432	2.836646
-56.472659	-7.909715	2.846643
-56.490259	-8.305886	2.856640
-56.274844	-5.903253	2.866637
-55.223141	-12.003042	2.876634
-54.738417	-10.535629	2.886630
-54.715078	-9.595073	2.896627
-53.750582	-11.984585	2.906624
-53.172512	-8.250967	2.916621
-53.173588	-15.102302	2.926618
-52.226122	-10.010240	2.936614
-51.881603	-9.936956	2.946611
-51.595634	-7.722699	2.956608
-50.853070	-10.179023	2.966605
-50.208172	-4.751590	2.976602
-49.156098	-6.594058	2.986598
-49.478323	-7.927952	2.996595
-49.144204	-4.203866	3.006592
-48.510058	-6.215671	3.016589
-47.522298	-3.594347	3.026586
-47.442664	-6.717204	3.036582
-46.791106	-8.579671	3.046579
-46.121895	-9.497746	3.056576
-45.895204	-10.533815	3.066573
-45.618087	-15.692568	3.076570
-45.059898	-6.466242	3.086566
-44.177275	-7.804004	3.096563
-43.266011	-11.078518	3.106560
-43.578718	-6.376271	3.116557
-43.082305	-7.638062	3.126554
-41.792433	-7.553583	3.136550
-41.713796	-8.677470	3.146547
-41.734746	-12.887022	3.156544
-40.866076	-8.809024	3.166541
-39.849596	-16.148230	3.176538
-40.035306	-17.503380	3.186534
-39.440659	-14.453397	3.196531
-38.514216	-11.150976	3.206528
-38.617750	-10.415572	3.216525
-37.895669	-14.705968	3.226522
-37.103902	-18.513054	3.236518
-37.276445	-12.746113	3.246515
-36.380807	-13.230623	3.256512
-35.830475	-12.261250	3.266509
-35.328020	-16.343227	3.276506
-34.359862	-13.421089	3.286502
-34.339144	-8.092869	3.296499
-34.370078	-11.426584	3.306496
-33.358917	-9.559647	3.316493
-32.789904	-9.898271	3.326490
-31.814717	-14.788758	3.336486
-31.760577	-15.386161	3.346483
-31.596551	-10.533234	3.356480
-30.914033	-9.860031	3.366477
-30.366764	-10.024215	3.376474
-29.939052	1.344786	3.386470
-28.877922	-11.525835	3.396467
-28.818763	-8.645892	3.406464
-28.554797	-6.542244	3.416461
-27.698760	-3.035629	3.426458
-27.563962	-14.580470	3.436454
-26.224234	-12.327548	3.446451
-26.266068	-5.231518	3.456448
-25.971306	-3.151671	3.466445
-25.587428	-6.625998	3.476442
-24.352506	-3.016821	3.486438
-23.858046	-2.634274	3.496435
-24.547299	-3.391522	3.506432
-23.272963	-8.452127	3.516429
-22.617452	-9.478938	3.526426
-22.184952	-8.937863	3.536422
-21.326189	-12.755381	3.546419
-20.903579	-7.445386	3.556416
-20.585072	-4.574145	3.566413
-20.740456	-1.407381	3.576410
-20.061187	-7.458688	3.586406
-19.553438	-8.104543	3.596403
-18.442939	-4.406305	3.606400
-17.946742	-4.033531	3.616397
-17.908133	-5.952613	3.626394
-17.558143	-0.612303	3.636390
-17.064347	-2.513561	3.646387
-16.397505	-6.636974	3.656384
-15.557143	-5.351640	3.666381
-15.748835	-7.443932	3.676378
-14.345498	-5.036191	3.686374
-14.027317	-6.425449	3.696371
-13.973656	-0.047512	3.706368
-13.442717	-0.278843	3.716365
-12.593901	3.862438	3.726362
-12.454315	3.140862	3.736358
-11.477083	-2.845969	3.746355
-10.939206	-0.205279	3.756352
-10.602598	-4.327960	3.766349
-10.623563	-3.152431	3.776346
-9.807978	-2.243361	3.786342
-9.167572	-7.506196	3.796339
-8.520352	-1.936575	3.806336
-7.852382	-6.972460	3.816333
-8.174675	-6.380387	3.826330
-7.397747	-8.582310	3.836326
-6.281635	-3.741407	3.846323
-6.381162	-3.975941	3.856320
-6.156286	2.571736	3.866317
-5.254405	1.044082	3.876314
-4.922088	5.522365	3.886310
-4.709323	14.843667	3.896307
-3.923836	24.725182	3.906304
-3.683903	31.413072	3.916301
-2.873804	44.639027	3.926298
-2.737664	45.888297	3.936294
-2.209173	66.063711	3.946291
-1.696714	79.260009	3.956288
-0.891414	81.935100	3.966285
-0.608402	91.717494	3.976282
-0.388559	104.268809	3.986278
0.000000	116.649588	3.991283
0.303659	128.864792	3.996288
0.485031	137.327950	4.001293
0.721167	140.179724	4.006298
0.979148	141.980922	4.011302
0.673125	137.074370	4.016307
0.722026	143.944685	4.021312
1.047680	154.593629	4.026317
1.021464	151.646113	4.031322
0.982085	154.455367	4.036326
0.925565	151.265803	4.041331
1.493639	160.874123	4.046336
0.842039	156.350393	4.051341
1.016339	155.605210	4.056346
1.835746	164.772614	4.061350
1.069436	168.979503	4.066355
1.017419	153.571127	4.071360
0.960901	152.520205	4.076365
1.027848	160.150161	4.081370
1.471926	168.781234	4.086374
1.241792	164.862580	4.091379
1.242318	162.638544	4.096384
0.838056	157.734627	4.101389
1.327290	164.969815	4.106394
1.700500	176.927457	4.111398
1.556513	175.121379	4.116403
0.970916	157.932670	4.121408
1.152491	167.278476	4.126413
0.989530	170.638471	4.131418
1.364231	174.471562	4.136422
1.435331	177.437620	4.141427
1.285730	164.790500	4.146432
1.529549	169.419068	4.151437
1.505346	170.587177	4.156442
1.618980	171.619934	4.161446
1.485715	181.793031	4.166451
1.215103	166.269986	4.171456
1.509630	174.683906	4.176461
1.499609	167.415449	4.181466
1.444929	171.685542	4.186470
1.363924	179.756147	4.191475
1.197275	165.425441	4.196480
1.446426	175.459901	4.201485
1.317631	170.481455	4.206490
1.433438	174.022669	4.211494
1.823130	172.513140	4.216499
1.777713	170.685388	4.221504
1.495512	169.555711	4.226509
1.613782	166.244020	4.231514
1.562905	173.193154	4.236518
1.375981	177.556603	4.241523
1.599849	171.950622	4.246528
1.683861	173.734619	4.251533
1.549779	179.972229	4.256538
1.878785	177.706539	4.261542
1.618184	175.586431	4.266547
1.724405	165.303874	4.271552
1.612734	176.213905	4.276557
1.240501	178.597272	4.281562
1.109576	168.452874	4.286566
1.247014	178.011196	4.291571
1.777568	169.886634	4.296576
1.565948	178.218014	4.301581
1.730428	175.690046	4.306586
1.574177	171.842143	4.311590
1.430907	178.245694	4.316595
2.394290	185.501977	4.321600
2.178554	179.138718	4.326605
1.909822	178.494150	4.331610
1.889291	169.961857	4.336614
1.518689	173.154870	4.341619
1.757764	173.130410	4.346624
1.627383	176.036092	4.351629
1.846073	171.788135	4.356634
2.074635	179.506829	4.361638
1.744344	187.995892	4.366643
1.951416	183.414391	4.371648
2.213952	193.035499	4.376653
1.644888	178.343504	4.381658
1.958567	173.951046	4.386662
2.148385	192.524027	4.391667
2.235508	183.585833	4.396672
1.857825	181.869923	4.401677
1.847292	181.836871	4.406682
2.070725	178.173454	4.411686
2.193041	197.623799	4.416691
2.147766	183.726586	4.421696
1.860041	185.717155	4.426701
1.806590	174.674861	4.431706
2.414169	187.554613	4.436710
2.080598	200.672656	4.441715
2.191218	192.948816	4.446720
2.057395	196.095477	4.451725
2.071108	188.067196	4.456730
1.751606	195.545370	4.461734
2.172441	202.243905	4.466739
2.212779	194.958104	4.471744
2.493770	201.093132	4.476749
2.172138	200.403017	4.481754
2.554509	193.614443	4.486758
2.147210	198.635454	4.491763
2.203895	190.793466	4.496768
1.874499	185.064819	4.501773
2.070875	187.736135	4.506778
2.650643	188.746936	4.511782
2.295922	189.741886	4.516787
2.540521	189.384380	4.521792
2.431977	196.396285	4.526797
2.030064	184.860922	4.531802
2.440875	193.395948	4.536806
2.627777	197.875202	4.541811
2.284301	179.595269	4.546816
1.984811	182.188768	4.551821
2.074245	190.267642	4.556826
2.399481	197.259464	4.561830
2.281383	188.454458	4.566835
2.304463	185.689082	4.571840
2.318171	194.380847	4.576845
2.098656	197.718015	4.581850
2.227110	197.179281	4.586854
2.217045	194.925253	4.591859
2.432098	198.166288	4.596864
2.908414	199.965135	4.601869
2.674844	196.486761	4.606874
2.864749	196.887562	4.611878
2.455196	202.130383	4.616883
2.587047	195.440924	4.621888
2.678814	199.925499	4.626893
2.381117	208.574009	4.631898
3.240438	197.702789	4.636902
2.672221	197.810350	4.641907
2.466718	199.905174	4.646912
2.724673	194.692503	4.651917
2.601294	198.805624	4.656922
2.628701	188.671363	4.661926
2.694633	202.189103	4.666931
2.702599	193.225264	4.671936
2.663516	193.943286	4.676941
2.959140	203.166952	4.681946
3.105200	199.126444	4.686950
2.899665	200.642321	4.691955
2.582366	195.784963	4.696960
2.557637	189.221124	4.701965
2.637108	191.300051	4.706970
3.044919	196.197315	4.711974
2.433023	200.528863	4.716979
2.813824	206.094708	4.721984
2.626141	203.188142	4.726989
2.539017	200.569633	4.731994
2.832150	201.492188	4.736998
2.537597	200.851639	4.742003
2.662065	203.784084	4.747008
2.961171	206.043947	4.752013
2.880872	210.131381	4.757018
2.646983	203.647556	4.762022
2.507717	202.040053	4.767027
2.382202	201.426968	4.772032
2.654856	207.952429	4.777037
2.656881	217.943134	4.782042
3.194040	217.185744	4.787046
3.172861	226.661223	4.792051
3.375464	222.665690	4.797056
3.107030	220.992876	4.802061
2.796566	215.106251	4.807066
2.844961	213.776405	4.812070
2.634867	228.052134	4.817075
3.007747	220.534217	4.822080
3.193632	227.047885	4.827085
3.233734	225.804749	4.832090
3.554175	226.963494	4.837094
3.111759	224.653394	4.842099
3.213704	228.494163	4.847104
3.167096	212.550231	4.852109
2.586141	214.564312	4.857114
3.414545	228.678350	4.862118
3.377441	220.079012	4.867123
3.295295	217.788748	4.872128
3.405644	218.322157	4.877133
3.203918	211.577064	4.882138
3.324684	202.845589	4.887142
2.954445	192.450542	4.892147
3.108930	207.128224	4.897152
3.189413	218.327895	4.902157
3.466985	218.019038	4.907162
3.203942	217.778534	4.912166
3.307877	227.066858	4.917171
3.311186	222.918860	4.922176
3.689044	221.303604	4.927181
3.097227	212.686235	4.932186
3.153023	203.408067	4.937190
3.022785	216.526100	4.942195
3.082115	225.679003	4.947200
3.249214	226.485144	4.952205
3.380176	230.786458	4.957210
3.551377	230.459361	4.962214
3.541584	231.302535	4.967219
3.493352	224.606303	4.972224
3.479587	236.608418	4.977229
3.267387	236.239777	4.982234
3.542511	225.829650	4.987238
3.380630	233.884399	4.992243
3.477568	234.454697	4.997248
3.628263	225.645786	5.002253
3.421477	223.877954	5.007258
3.733816	224.528607	5.012262
3.495963	234.328884	5.017267
3.298778	228.143050	5.022272
3.638381	226.116144	5.027277
3.203179	224.589515	5.032282
3.337517	235.850414	5.037286
3.547039	252.085588	5.042291
3.760232	237.838049	5.047296
3.361541	235.065569	5.052301
3.369957	231.201506	5.057306
3.725539	228.286279	5.062310
3.140968	229.386620	5.067315
3.464810	229.099031	5.072320
3.618484	251.828459	5.077325
3.364957	259.979745	5.082330
3.908530	254.969354	5.087334
3.876387	252.089182	5.092339
3.708311	250.248882	5.097344
4.022507	257.043134	5.102349
3.745860	252.511619	5.107354
3.926272	244.476340	5.112358
3.639013	239.528874	5.117363
4.123056	249.447712	5.122368
3.733088	238.011693	5.127373
3.647654	233.083424	5.132378
4.023642	233.066121	5.137382
3.958774	239.286648	5.142387
3.762468	226.627773	5.147392
3.866386	233.166860	5.152397
3.764248	239.791815	5.157402
3.887180	229.085848	5.162406
4.105612	247.641778	5.167411
3.961907	237.126014	5.172416
4.124711	232.810815	5.177421
3.611439	228.439532	5.182426
3.911352	228.016467	5.187430
4.062639	238.164274	5.192435
4.287982	239.255571	5.197440
3.987551	227.226663	5.202445
3.634401	236.646269	5.207450
4.267639	236.357963	5.212454
3.954319	240.250736	5.217459
4.068850	243.776344	5.222464
4.111411	233.329656	5.227469
4.207983	241.919959	5.232474
3.820471	235.643536	5.237478
3.932090	244.563685	5.242483
4.008743	241.783632	5.247488
3.815791	234.844178	5.252493
3.886374	248.702908	5.257498
4.343029	240.548692	5.262502
4.423199	242.089689	5.267507
4.335188	245.314645	5.272512
4.165856	244.914021	5.277517
3.639389	246.150845	5.282522
4.198924	241.783365	5.287526
4.082449	237.230080	5.292531
4.522219	240.777813	5.297536
4.320434	248.718562	5.302541
3.814687	250.293839	5.307546
4.533674	232.348293	5.312550
4.251797	239.776335	5.317555
3.979050	241.157150	5.322560
4.211795	245.015522	5.327565
4.274013	244.749685	5.332570
4.398890	244.939155	5.337574
4.423940	246.589973	5.342579
4.355697	237.489284	5.347584
4.438895	242.402302	5.352589
4.437879	241.548373	5.357594
4.677775	237.961473	5.362598
4.146459	250.177052	5.367603
4.413001	246.434145	5.372608
4.417410	239.441815	5.377613
4.135809	242.889897	5.382618
4.512385	247.270030	5.387622
4.136277	248.179730	5.392627
4.318907	246.851128	5.397632
4.297777	248.942562	5.402637
4.555758	263.392208	5.407642
4.563538	262.945026	5.412646
4.892060	268.085604	5.417651
4.530127	258.214399	5.422656
4.707326	250.391584	5.427661
4.705776	236.250246	5.432666
4.656743	243.366796	5.437670
4.446104	239.233123	5.442675
4.292216	241.797634	5.447680
4.528089	252.254976	5.452685
4.111603	270.928766	5.457690
4.880486	257.540636	5.462694
5.016001	261.094618	5.467699
4.837280	262.115952	5.472704
4.882651	265.547930	5.477709
4.937815	244.466106	5.482714
4.970527	240.648877	5.487718
4.737129	240.251900	5.492723
4.602520	238.539266	5.497728
4.682458	239.045773	5.502733
4.320433	237.501422	5.507738
4.763737	238.052593	5.512742
4.704272	264.105457	5.517747
4.772182	264.670785	5.522752
5.428214	262.297221	5.527757
4.996655	257.546219	5.532762
5.141521	248.826788	5.537766
4.704378	242.390414	5.542771
4.528079	243.923888	5.547776
4.668610	239.159747	5.552781
4.796498	247.897035	5.557786
4.824481	250.752763	5.562790
4.784154	258.456410	5.567795
5.065770	260.991081	5.572800
5.171168	267.143980	5.577805
4.692361	263.472825	5.582810
4.915899	251.463559	5.587814
5.016466	257.421058	5.592819
4.357884	265.980254	5.597824
4.827940	253.309357	5.602829
4.925466	257.207767	5.607834
5.178567	262.992825	5.612838
5.080258	265.387337	5.617843
4.790620	265.622363	5.622848
5.235704	254.904188	5.627853
5.079538	264.381722	5.632858
5.248945	257.145401	5.637862
5.091991	262.627315	5.642867
5.068545	262.495036	5.647872
5.260959	255.954309	5.652877
5.086039	263.729533	5.657882
5.094367	270.970039	5.662886
5.059083	261.516200	5.667891
4.797518	268.384282	5.672896
5.214711	259.024507	5.677901
5.169763	260.970957	5.682906
5.512538	257.750842	5.687910
5.209474	261.053576	5.692915
5.011349	267.456208	5.697920
5.120668	263.623883	5.702925
4.839781	260.070608	5.707930
5.127612	255.960559	5.712934
5.213325	263.128902	5.717939
5.270323	272.661835	5.722944
5.439760	271.366922	5.727949
5.278066	268.544882	5.732954
5.420894	266.899779	5.737958
5.156542	266.700606	5.742963
5.424910	273.451380	5.747968
5.452363	284.649859	5.752973
5.626946	276.919188	5.757978
5.323621	260.603902	5.762982
5.230360	257.401057	5.767987
5.200801	275.707731	5.772992
5.740158	264.569919	5.777997
5.724751	278.568608	5.783002
5.489103	268.098778	5.788006
5.532490	264.358975	5.793011
5.588347	261.604302	5.798016
5.470941	256.766424	5.803021
5.265905	255.779748	5.808026
5.290157	262.454633	5.813030
5.531387	274.413908	5.818035
5.536516	276.482275	5.823040
5.866958	279.714850	5.828045
5.644393	286.573703	5.833050
5.461218	271.220447	5.838054
5.619535	279.522750	5.843059
5.237224	281.907700	5.848064
5.844705	274.005226	5.853069
5.559393	279.086359	5.858074
5.399533	282.452220	5.863078
6.002187	290.634728	5.868083
6.012051	292.873199	5.873088
5.659277	285.249941	5.878093
5.749052	285.365784	5.883098
5.627287	285.176047	5.888102
5.768080	284.388620	5.893107
5.226106	284.704063	5.898112
5.582106	279.887382	5.903117
5.561643	287.072266	5.908122
5.816464	285.991844	5.913126
5.847810	288.334535	5.918131
5.736982	292.841186	5.923136
5.590232	286.270999	5.928141
5.850959	289.875092	5.933146
5.933457	289.976249	5.938150
5.691536	277.267494	5.943155
5.720154	286.352444	5.948160
5.913647	286.654615	5.953165
5.630964	282.190470	5.958170
5.576726	280.648813	5.963174
5.833039	293.510569	5.968179
5.887640	284.697608	5.973184
5.917807	284.256430	5.978189
5.815561	288.309335	5.983194
5.924219	280.870495	5.988198
5.641957	284.350325	5.993203
6.216981	293.799450	5.998208
6.722224	290.898876	6.003213
6.225108	298.341473	6.008218
6.123591	287.224337	6.013222
6.035206	286.482083	6.018227
5.864845	285.565935	6.023232
6.438020	288.213400	6.028237
5.917927	286.329830	6.033242
6.154974	276.017349	6.038246
6.162871	273.406180	6.043251
6.067761	279.042983	6.048256
6.528728	276.203087	6.053261
6.060548	284.482716	6.058266
6.027339	273.664995	6.063270
6.080842	282.689122	6.068275
5.849190	280.080449	6.073280
6.072945	289.280549	6.078285
5.799147	283.546378	6.083290
5.957779	281.149017	6.088294
5.931669	280.558416	6.093299
5.825338	290.638798	6.098304
6.048954	285.548503	6.103309
5.702939	287.117896	6.108314
5.979348	288.498632	6.113318
5.540504	284.818088	6.118323
6.013197	282.093423	6.123328
5.935621	277.730219	6.128333
5.624303	284.900278	6.133338
5.883169	280.013300	6.138342
5.807988	281.790457	6.143347
5.862307	283.825856	6.148352
6.101270	282.320804	6.153357
5.841494	283.253521	6.158362
5.997429	274.465916	6.163366
5.864364	281.019773	6.168371
5.857996	279.084692	6.173376
5.838258	278.606992	6.178381
5.815612	289.300756	6.183386
6.274647	280.681087	6.188390
5.950023	287.679216	6.193395
5.734518	288.130486	6.198400
6.151550	279.953948	6.203405
5.887739	289.812080	6.208410
5.987695	282.422050	6.213414
6.210771	289.338067	6.218419
6.105912	288.332628	6.223424
6.286878	282.622563	6.228429
5.975860	281.048121	6.233434
6.062797	279.554084	6.238438
6.046855	280.483638	6.243443
5.871044	285.968495	6.248448
6.523541	277.173177	6.253453
6.112207	287.462394	6.258458
6.207579	281.098116	6.263462
6.223401	280.421894	6.268467
6.300347	285.842089	6.273472
6.279169	270.245315	6.278477
5.718904	266.001559	6.283482
5.791628	262.722251	6.288486
5.952057	279.015714	6.293491
6.109602	285.647709	6.298496
5.984846	268.943951	6.303501
5.763315	264.520908	6.308506
6.075402	273.182074	6.313510
6.197874	272.612632	6.318515
5.638047	266.208005	6.323520
6.211760	273.778091	6.328525
5.990692	275.713999	6.333530
5.753933	275.178342	6.338534
5.779324	277.860474	6.343539
5.791325	290.396442	6.348544
5.825496	283.662048	6.353549
5.956262	293.072777	6.358554
6.087287	289.110519	6.363558
5.937824	283.679686	6.368563
6.089658	289.521648	6.373568
6.228355	284.571123	6.378573
5.986982	291.119701	6.383578
5.809952	284.687104	6.388582
5.915294	294.165066	6.393587
5.803554	298.137195	6.398592
5.810814	285.016321	6.403597
5.676374	294.107681	6.408602
5.260103	288.348235	6.413606
5.969391	278.455763	6.418611
5.737614	286.597347	6.423616
5.990626	280.350891	6.428621
6.056421	285.788640	6.433626
6.011642	282.040414	6.438630
6.345254	286.218442	6.443635
5.966656	286.318626	6.448640
6.076138	284.302232	6.453645
5.855851	285.747648	6.458650
5.706584	288.710071	6.463654
5.875132	289.193293	6.468659
5.292281	291.770816	6.473664
5.906935	296.522010	6.478669
6.363139	312.633413	6.483674
6.057178	309.087195	6.488678
5.799884	296.912320	6.493683
5.707028	290.757676	6.498688
6.212653	298.445939	6.503693
5.882929	306.859042	6.508698
6.206163	295.795988	6.513702
5.849915	283.978209	6.518707
5.988608	294.890460	6.523712
5.774937	288.675535	6.528717
6.104691	303.569612	6.533722
6.322372	298.777625	6.538726
6.143100	287.185385	6.543731
6.029181	298.301482	6.548736
6.217782	284.389922	6.553741
6.139399	288.499222	6.558746
6.229628	291.778691	6.563750
6.143079	291.649909	6.568755
5.820005	282.905243	6.573760
5.822231	290.137215	6.578765
6.094416	285.396856	6.583770
6.077700	287.231348	6.588774
5.780034	284.879721	6.593779
5.867794	291.810480	6.598784
6.343320	292.204778	6.603789
6.304772	291.850227	6.608794
6.091455	291.140080	6.613798
6.072627	287.770620	6.618803
6.318189	288.067847	6.623808
6.317618	290.393362	6.628813
6.432011	288.841267	6.633818
5.607961	275.650519	6.638822
6.078406	277.206684	6.643827
5.649203	276.954085	6.648832
6.274148	278.694999	6.653837
5.871660	279.007706	6.658842
5.892441	280.839523	6.663846
6.391867	278.857328	6.668851
5.718485	280.585256	6.673856
5.949514	270.950745	6.678861
5.851162	277.502360	6.683866
5.948296	274.469180	6.688870
6.133709	283.861905	6.693875
5.777145	279.317516	6.698880
6.018666	288.983077	6.703885
6.026142	291.712292	6.708890
5.781314	295.746271	6.713894
6.309181	292.161979	6.718899
5.795116	290.650786	6.723904
5.893938	282.957217	6.728909
6.118468	284.608618	6.733914
5.913227	279.316182	6.738918
6.154256	292.322684	6.743923
5.921209	287.148468	6.748928
5.877840	283.150090	6.753933
5.935430	284.643988	6.758938
5.908866	292.889663	6.763942
6.344325	278.711887	6.768947
5.648944	273.441983	6.773952
6.092288	288.704333	6.778957
5.947872	288.179608	6.783962
6.117229	281.686753	6.788966
5.942820	265.512739	6.793971
5.528403	267.829921	6.798976
5.582536	278.163717	6.803981
5.717428	293.679737	6.808986
5.810004	289.691828	6.813990
6.108123	272.938045	6.818995
6.162823	283.423613	6.824000
5.696858	279.348666	6.829005
5.925485	288.231638	6.834010
5.922323	295.097462	6.839014
6.175502	294.086896	6.844019
5.208120	288.590424	6.849024
5.351368	293.392868	6.854029
5.655767	301.786330	6.859034
6.012698	309.893212	6.864038
6.764444	304.866213	6.869043
5.893168	297.203459	6.874048
6.095292	292.243057	6.879053
5.978434	301.309537	6.884058
6.021635	285.297773	6.889062
6.108092	288.195022	6.894067
5.937562	287.402284	6.899072
6.117787	290.028674	6.904077
5.941405	288.297230	6.909082
6.041248	290.347687	6.914086
6.309869	284.380369	6.919091
5.887720	293.374158	6.924096
5.663657	283.731404	6.929101
5.687654	289.416103	6.934106
5.956801	284.325047	6.939110
6.028339	285.775645	6.944115
5.992787	291.428488	6.949120
6.072203	278.622245	6.954125
6.048484	283.963201	6.959130
5.946723	279.761948	6.964134
6.242752	287.542949	6.969139
6.170649	293.017989	6.974144
6.028761	282.723375	6.979149
6.039738	285.094547	6.984154
6.181665	286.325382	6.989158
6.406378	281.396266	6.994163
6.136375	285.639802	6.999168
6.119656	281.267122	7.004173
6.025522	289.450551	7.009178
6.016158	292.865747	7.014182
6.051678	289.646009	7.019187
6.019619	287.025241	7.024192
6.313995	283.328611	7.029197
5.878852	271.602216	7.034202
5.533250	269.776900	7.039206
5.711626	273.314720	7.044211
5.511525	283.026890	7.049216
5.578215	278.318528	7.054221
5.659834	287.461665	7.059226
6.102188	286.060984	7.064230
6.046360	283.200313	7.069235
5.954831	286.387860	7.074240
5.962749	279.021652	7.079245
5.986947	298.446255	7.084250
5.929180	287.034410	7.089254
5.983060	289.092024	7.094259
5.561107	294.267201	7.099264
5.908759	287.291012	7.104269
5.817353	292.807022	7.109274
5.682889	290.376201	7.114278
5.810827	288.299987	7.119283
6.075677	303.802109	7.124288
5.998907	305.968650	7.129293
6.068098	307.615765	7.134298
5.862277	307.341041	7.139302
6.165057	297.976913	7.144307
5.729637	296.874247	7.149312
6.251811	298.463488	7.154317
5.719199	288.194904	7.159322
5.925986	311.403348	7.164326
6.294340	314.019433	7.169331
6.241028	308.481875	7.174336
6.287631	292.953621	7.179341
5.922175	287.122990	7.184346
5.801511	291.802011	7.189350
6.276288	287.052255	7.194355
5.926597	295.759521	7.199360
6.253294	300.697917	7.204365
6.102954	302.379212	7.209370
5.827183	293.946709	7.214374
6.274919	290.783011	7.219379
5.605583	290.634237	7.224384
5.858789	288.497392	7.229389
5.656416	290.968220	7.234394
5.488667	292.329527	7.239398
5.804629	293.666141	7.244403
6.149459	315.261757	7.249408
6.280197	303.516837	7.254413
6.163144	294.116840	7.259418
5.540130	294.957419	7.264422
5.672702	299.897566	7.269427
5.966845	313.806958	7.274432
6.001406	312.719700	7.279437
6.173786	316.679234	7.284442
5.789260	306.137651	7.289446
6.007501	309.653452	7.294451
6.244828	316.779229	7.299456
6.060991	295.247346	7.304461
6.068929	297.910053	7.309466
5.871276	293.299791	7.314470
6.427879	290.308964	7.319475
5.839784	295.658703	7.324480
5.853194	300.876827	7.329485
5.968877	290.744581	7.334490
5.806567	297.081538	7.339494
5.802614	286.673698	7.344499
6.096969	301.443574	7.349504
6.147928	296.272592	7.354509
6.047450	295.076649	7.359514
5.720103	294.877793	7.364518
5.829972	289.944409	7.369523
5.586140	298.413737	7.374528
6.424608	306.992963	7.379533
6.218704	302.168851	7.384538
6.174952	290.153719	7.389542
6.007730	291.957862	7.394547
6.024565	298.254272	7.399552
5.931803	292.124923	7.404557
5.781921	297.817714	7.409562
5.532355	292.687197	7.414566
6.017807	300.865812	7.419571
5.998999	310.954724	7.424576
6.401506	306.760371	7.429581
6.127261	293.132836	7.434586
5.524177	295.466742	7.439590
6.344449	294.583013	7.444595
5.892295	298.022859	7.449600
6.046934	299.969876	7.454605
5.706445	296.274015	7.459610
5.859926	298.822314	7.464614
6.110840	297.413475	7.469619
5.898293	293.662894	7.474624
5.781459	293.896325	7.479629
6.185629	306.086511	7.484634
6.382924	302.000039	7.489638
5.705907	294.284895	7.494643
5.731246	290.427675	7.499648
5.935434	299.336603	7.504653
6.080896	300.997151	7.509658
6.026959	312.350686	7.514662
6.058035	291.449724	7.519667
5.619732	294.615335	7.524672
6.145321	297.728947	7.529677
6.310523	308.118232	7.534682
5.911890	298.793711	7.539686
6.002348	290.686997	7.544691
5.793508	299.236296	7.549696
5.882367	297.969745	7.554701
6.223931	286.457761	7.559706
6.058525	298.986556	7.564710
6.088950	291.601020	7.569715
6.066407	293.733808	7.574720
5.725011	285.852519	7.579725
5.687828	282.767486	7.584730
5.466546	290.274699	7.589734
6.361392	307.156181	7.594739
6.386662	312.650867	7.599744
6.224254	296.471793	7.604749
5.867387	290.820154	7.609754
5.450242	291.951377	7.614758
5.874456	297.905955	7.619763
6.038019	304.287088	7.624768
6.288547	308.152196	7.629773
5.982676	302.710909	7.634778
5.655679	303.742677	7.639782
6.192340	302.925251	7.644787
6.108727	299.281142	7.649792
5.798142	292.556131	7.654797
5.847512	292.276475	7.659802
5.853673	304.278696	7.664806
6.268107	307.510854	7.669811
5.965692	309.086116	7.674816
6.135022	299.862986	7.679821
5.952505	287.692294	7.684826
5.906364	296.953401	7.689830
6.025000	287.984939	7.694835
5.979140	300.112314	7.699840
6.071491	293.362531	7.704845
5.702828	299.304518	7.709850
5.812659	300.660572	7.714854
5.777618	314.504161	7.719859
6.036529	325.385059	7.724864
6.048067	319.562158	7.729869
6.265792	319.825756	7.734874
5.880244	324.182201	7.739878
6.417126	315.638979	7.744883
6.244833	295.016445	7.749888
5.840555	292.482103	7.754893
5.619540	298.385283	7.759898
5.505092	297.488902	7.764902
6.048480	300.571270	7.769907
6.173727	319.948527	7.774912
6.174186	304.788109	7.779917
6.188129	297.370337	7.784922
6.247706	297.889507	7.789926
6.269325	281.760886	7.794931
6.145514	291.021429	7.799936
5.995167	289.716194	7.804941
5.849240	283.854548	7.809946
6.079799	294.230486	7.814950
5.935519	284.220976	7.819955
5.788636	282.200206	7.824960
5.983975	284.381325	7.829965
5.868203	281.634389	7.834970
5.564578	295.057881	7.839974
5.661827	279.154765	7.844979
5.787878	294.567759	7.849984
5.812314	302.587203	7.854989
6.480540	314.612898	7.859994
6.008056	302.360795	7.864998
6.209740	290.566873	7.870003
5.973217	295.131059	7.875008
6.173486	295.808655	7.880013
6.098678	288.695764	7.885018
5.773143	290.445463	7.890022
5.723816	292.579257	7.895027
5.867017	295.331632	7.900032
5.777904	292.618508	7.905037
5.712268	295.444528	7.910042
5.570503	313.828821	7.915046
6.080798	308.747668	7.920051
6.327513	311.882556	7.925056
6.215631	313.994455	7.930061
5.887199	306.753369	7.935066
6.034424	317.101167	7.940070
5.979728	307.261191	7.945075
5.866686	308.908206	7.950080
6.123732	307.020693	7.955085
6.001134	305.068905	7.960090
5.501517	311.518495	7.965094
6.080088	312.371305	7.970099
6.136108	318.930536	7.975104
6.412757	315.976966	7.980109
6.097092	304.412278	7.985114
6.015323	307.152227	7.990118
5.931429	298.876466	7.995136
5.787814	290.867864	8.000154
5.999676	290.424755	8.005171
5.888147	294.115379	8.010189
5.601071	302.036632	8.015206
6.200181	307.377454	8.020224
5.976076	320.792330	8.025242
6.035608	316.188571	8.030259
6.289838	325.685417	8.035277
6.073036	307.397687	8.040294
5.636837	295.338631	8.045312
6.269505	313.710132	8.050330
6.225402	310.564633	8.055347
5.888914	304.466811	8.060365
5.839516	304.645015	8.065382
5.927862	309.945449	8.070400
6.196808	320.358289	8.075418
6.207116	311.404268	8.080435
6.053148	303.157445	8.085453
5.997341	314.229881	8.090470
6.395568	313.779845	8.095488
5.820867	300.893485	8.100506
5.922103	301.146060	8.105523
6.370586	306.399888	8.110541
6.215203	313.379198	8.115558
6.153422	291.305837	8.120576
5.642881	297.138144	8.125594
5.806609	306.406087	8.130611
6.271227	308.883606	8.135629
6.237887	306.440137	8.140646
6.304900	318.074088	8.145664
6.121711	320.826030	8.150682
6.185552	320.639484	8.155699
6.458919	313.020360	8.160717
6.073426	313.033155	8.165734
5.880402	299.976922	8.170752
5.827700	304.627167	8.175770
6.109156	311.178720	8.180787
6.433910	317.903405	8.185805
5.868656	320.957816	8.190822
5.920185	322.313135	8.195840
6.119392	321.105178	8.200858
6.204900	315.200410	8.205875
6.333760	318.762097	8.210893
5.935419	317.117031	8.215910
6.246052	313.613359	8.220928
6.263978	321.051656	8.225946
6.386456	319.641062	8.230963
6.357474	314.678720	8.235981
6.174016	320.103522	8.240998
6.286100	317.467006	8.246016
6.216642	318.654980	8.251034
6.323045	321.396545	8.256051
6.254044	315.686238	8.261069
6.198191	330.696919	8.266086
6.023684	313.519692	8.271104
6.433933	314.030251	8.276122
6.091993	317.554794	8.281139
5.945421	315.034285	8.286157
6.073458	316.822636	8.291174
6.185411	322.782081	8.296192
6.280798	320.627820	8.301210
6.148685	323.169849	8.306227
6.513194	322.620926	8.311245
6.041491	324.079801	8.316262
6.091110	320.493697	8.321280
6.406986	323.174247	8.326298
6.328076	312.492208	8.331315
6.154592	312.714977	8.336333
6.348259	316.818809	8.341350
6.202267	321.900126	8.346368
6.038449	328.438967	8.351386
6.157126	340.184803	8.356403
6.648799	340.061026	8.361421
6.616262	347.551369	8.366438
6.577707	334.805558	8.371456
6.476778	312.807691	8.376474
6.142479	324.343192	8.381491
6.086836	317.990210	8.386509
6.263816	334.308942	8.391526
6.562137	341.754081	8.396544
6.483383	339.948806	8.401562
6.370715	346.984591	8.406579
6.433956	335.816527	8.411597
6.055298	346.308122	8.416614
6.266362	341.904814	8.421632
6.415669	345.179316	8.426650
6.379060	347.564475	8.431667
6.385835	346.957647	8.436685
6.732836	358.342915	8.441702
6.406837	351.142125	8.446720
6.587349	346.718327	8.451738
6.207527	356.332843	8.456755
6.628822	349.072505	8.461773
6.540989	345.763404	8.466790
6.520444	353.204548	8.471808
6.642927	351.784484	8.476826
6.527167	353.677065	8.481843
6.546179	346.548786	8.486861
6.238836	350.976771	8.491878
6.388945	351.578325	8.496896
6.542756	349.266649	8.501914
6.442923	349.866095	8.506931
6.425424	348.224842	8.511949
6.418564	354.799212	8.516966
6.369500	357.514497	8.521984
6.506010	345.135877	8.527002
6.618679	344.963818	8.532019
6.793504	340.373658	8.537037
6.747681	354.133166	8.542054
6.342920	351.861123	8.547072
6.768980	349.175717	8.552090
6.604737	354.427134	8.557107
6.508830	353.586998	8.562125
6.722907	351.919155	8.567143
6.552825	354.956224	8.572160
6.902197	350.275773	8.577178
6.538050	352.260673	8.582195
6.744548	346.946095	8.587213
6.999632	351.958663	8.592231
6.709249	336.143757	8.597248
6.674148	333.801540	8.602266
6.430690	330.996328	8.607283
6.519849	324.627111	8.612301
6.846711	338.890283	8.617319
6.262610	336.680877	8.622336
6.569288	334.462161	8.627354
6.491694	347.434546	8.632371
6.836641	348.611646	8.637389
6.700020	348.200705	8.642407
6.832370	362.307998	8.647424
7.036999	353.891716	8.652442
6.428198	353.421754	8.657459
6.709065	357.303747	8.662477
6.656646	353.907084	8.667495
6.288381	354.513612	8.672512
6.666115	351.879909	8.677530
6.503132	365.509352	8.682547
6.425255	356.606906	8.687565
6.539711	362.263033	8.692583
6.749363	360.469654	8.697600
6.911425	366.020545	8.702618
6.418091	365.002458	8.707635
6.656804	359.585035	8.712653
6.803033	352.348588	8.717671
6.586184	361.508566	8.722688
7.002995	351.247912	8.727706
6.689442	356.554133	8.732723
6.605119	354.131218	8.737741
6.666116	360.701336	8.742759
6.483285	361.881720	8.747776
6.648822	361.975970	8.752794
6.441510	369.588204	8.757811
6.909130	369.483950	8.762829
6.671839	367.807491	8.767847
6.684553	372.848335	8.772864
7.236253	377.483386	8.777882
6.890654	383.406798	8.782899
6.749028	370.137395	8.787917
6.833845	367.110662	8.792935
6.831820	368.288140	8.797952
6.926900	350.504044	8.802970
6.610885	369.070644	8.807987
6.415715	369.921607	8.813005
6.808286	373.091971	8.818023
7.026091	376.365280	8.823040
7.059663	383.715965	8.828058
7.006878	383.613845	8.833075
7.015430	376.887949	8.838093
6.885403	380.814987	8.843111
6.981020	386.108001	8.848128
7.206653	379.067453	8.853146
6.845902	375.116064	8.858163
6.816972	364.492481	8.863181
6.619761	370.067755	8.868199
6.457898	375.473433	8.873216
7.161065	377.235357	8.878234
7.295172	390.395707	8.883251
6.781560	383.555458	8.888269
7.038440	392.670094	8.893287
6.970723	388.666767	8.898304
7.317428	379.060764	8.903322
7.107262	378.487712	8.908339
6.578872	372.994071	8.913357
7.173766	377.369945	8.918375
6.959676	382.294633	8.923392
7.182168	376.406385	8.928410
7.063161	370.688067	8.933427
6.911825	363.589460	8.938445
6.950075	367.566031	8.943463
6.903731	377.665095	8.948480
7.032343	382.366021	8.953498
7.180778	377.555910	8.958515
7.203432	385.583602	8.963533
7.252910	376.295263	8.968551
6.687352	369.908052	8.973568
6.968983	370.769982	8.978586
6.973922	380.031129	8.983603
6.707682	379.618279	8.988621
6.931957	375.509535	8.993639
6.843153	373.286121	8.998656
7.025697	381.468789	9.003674
6.765618	373.863271	9.008691
6.791161	372.265805	9.013709
6.967210	377.839767	9.018727
7.084503	380.172568	9.023744
7.006793	375.637496	9.028762
6.690475	388.823795	9.033779
7.499269	394.974555	9.038797
7.140240	382.663595	9.043815
6.946075	388.342537	9.048832
7.106825	380.488467	9.053850
6.944529	396.162683	9.058867
7.228398	403.875172	9.063885
7.568820	394.655128	9.068903
7.408430	385.787604	9.073920
7.132081	389.134699	9.078938
7.418847	381.649152	9.083955
6.956729	382.740484	9.088973
7.216298	378.569443	9.093991
7.019193	384.359289	9.099008
7.196573	384.492718	9.104026
7.127017	392.074047	9.109043
7.076855	396.130658	9.114061
7.345489	394.776194	9.119079
7.328009	402.926901	9.124096
7.267043	391.191191	9.129114
7.518147	390.486363	9.134131
6.981480	385.943856	9.139149
7.438607	377.977374	9.144167
7.529950	386.903197	9.149184
7.257118	380.650277	9.154202
7.367519	384.372634	9.159219
7.494126	380.048734	9.164237
7.452083	383.040627	9.169255
7.319911	388.050387	9.174272
7.459581	381.108425	9.179290
7.312795	388.843780	9.184307
7.225629	380.993598	9.189325
7.432754	379.768626	9.194343
7.011646	375.564716	9.199360
6.849705	383.264561	9.204378
7.351938	391.943385	9.209395
7.330606	401.814519	9.214413
7.460344	395.072903	9.219431
7.253209	388.437386	9.224448
7.588799	394.866938	9.229466
7.539251	394.915785	9.234483
7.150626	394.777596	9.239501
7.508650	381.771200	9.244519
7.146266	393.478368	9.249536
7.476735	398.608594	9.254554
7.696081	408.205584	9.259571
7.370876	388.726036	9.264589
7.298865	384.761246	9.269607
7.215921	387.488123	9.274624
7.464810	409.592646	9.279642
8.003769	407.015880	9.284659
7.324616	391.015315	9.289677
7.239063	383.571959	9.294695
7.178077	399.659571	9.299712
7.330246	405.546514	9.304730
7.356685	404.296026	9.309747
7.492394	411.473037	9.314765
7.706191	413.787661	9.319783
7.722497	415.063269	9.324800
7.375293	413.722640	9.329818
7.575452	415.742757	9.334835
7.525407	407.811047	9.339853
7.986214	404.454382	9.344871
7.819603	396.487181	9.349888
7.271934	392.359774	9.354906
6.944189	384.162059	9.359923
7.124340	404.611099	9.364941
7.365987	408.287781	9.369959
7.335618	415.929287	9.374976
7.601241	413.972561	9.379994
7.588932	403.873359	9.385011
7.500988	410.829584	9.390029
7.479579	415.512853	9.395047
7.539779	410.426151	9.400064
7.589896	412.469629	9.405082
7.513779	413.510330	9.410099
7.333142	417.353743	9.415117
7.757640	414.163667	9.420135
7.791128	407.575881	9.425152
7.197127	416.396997	9.430170
7.783490	407.918099	9.435187
7.665783	416.482029	9.440205
7.784280	417.476652	9.445223
7.408937	413.641130	9.450240
7.277667	406.801300	9.455258
7.688090	408.037634	9.460275
7.356968	421.765879	9.465293
7.944402	416.915807	9.470311
7.967364	426.464493	9.475328
7.658077	424.518386	9.480346
7.597763	416.607205	9.485363
7.624243	424.034746	9.490381
8.111204	423.296351	9.495399
8.204909	419.592916	9.500416
7.589986	417.038021	9.505434
7.914290	414.409472	9.510451
7.683160	413.874395	9.515469
7.983808	407.693115	9.520487
7.976984	401.584955	9.525504
7.734105	413.860480	9.530522
8.037187	406.870975	9.535539
7.918864	405.980680	9.540557
7.614779	408.164508	9.545575
7.691041	412.416023	9.550592
7.838775	420.976495	9.555610
8.089485	408.665253	9.560627
7.587192	409.532479	9.565645
7.614153	404.671849	9.570663
7.799649	411.228913	9.575680
7.810174	409.532801	9.580698
7.726867	404.862900	9.585715
7.404085	418.794961	9.590733
7.711489	408.289390	9.595751
7.914619	416.765500	9.600768
7.952241	430.120774	9.605786
7.907220	419.193564	9.610803
7.873916	426.507344	9.615821
7.892720	411.672974	9.620839
8.175177	414.945692	9.625856
7.860191	419.908189	9.630874
8.163905	410.801144	9.635891
7.520498	418.411872	9.640909
7.876690	406.718493	9.645927
7.903769	411.025001	9.650944
7.589492	419.913013	9.655962
7.875111	418.357097	9.660979
8.249245	434.042495	9.665997
8.185515	426.766128	9.671015
8.234973	421.150946	9.676032
7.737340	414.620606	9.681050
7.660244	411.849437	9.686067
7.872538	426.786893	9.691085
8.124790	428.489647	9.696103
8.429451	433.519764	9.701120
8.069678	428.675162	9.706138
7.934129	416.073777	9.711155
7.818067	418.783725	9.716173
7.686064	426.232786	9.721191
8.256003	430.514734	9.726208
7.868608	436.460450	9.731226
8.245863	431.371713	9.736243
7.954351	435.121944	9.741261
8.087909	439.121560	9.746279
8.148800	440.349205	9.751296
8.058560	431.593807	9.756314
8.370195	434.000492	9.761331
8.324945	436.566880	9.766349
8.317261	427.691338	9.771367
7.960917	402.952998	9.776384
7.831190	412.689543	9.781402
8.355332	423.719086	9.786419
8.127623	431.299809	9.791437
8.058903	416.479062	9.796455
8.018415	422.986113	9.801472
7.963599	432.931901	9.806490
7.997094	429.749054	9.811507
8.408670	427.185807	9.816525
8.086993	436.340055	9.821543
8.092362	431.492247	9.826560
7.929906	437.655393	9.831578
8.311978	434.686503	9.836595
7.934165	430.658868	9.841613
7.925868	435.832382	9.846631
8.433580	436.551822	9.851648
7.873613	433.508709	9.856666
8.241689	435.663622	9.861683
8.181283	434.562347	9.866701
8.351460	429.868752	9.871719
8.342109	428.387161	9.876736
8.368344	426.474016	9.881754
8.153270	432.935673	9.886771
8.202830	424.767553	9.891789
8.475680	431.651834	9.896807
8.714176	432.230162	9.901824
8.665178	436.308691	9.906842
8.502968	430.865311	9.911859
8.443264	437.548920	9.916877
8.536675	440.630180	9.921895
8.427378	434.298134	9.926912
8.358809	424.087765	9.931930
8.456800	431.901787	9.936947
8.679005	434.499113	9.941965
8.255030	418.714401	9.946983
8.362393	411.629141	9.952000
7.674781	418.101253	9.957018
8.181298	426.337636	9.962035
8.568021	441.850676	9.967053
8.560855	430.870231	9.972071
8.903970	428.879348	9.977088
8.484724	437.401879	9.982106
8.770076	426.549453	9.987123
8.463633	413.356170	9.992141
8.176595	416.493505	9.997159
8.484564	406.997655	10.002176
8.366099	420.497138	10.007194
8.459365	416.601278	10.012211
8.654923	427.397973	10.017229
7.985182	424.842146	10.022247
8.266638	420.071270	10.027264
8.670854	435.862433	10.032282
8.516455	432.749864	10.037299
8.362541	432.941187	10.042317
8.332346	438.096021	10.047335
8.793866	432.249430	10.052352
8.740499	440.364719	10.057370
8.499513	434.532835	10.062387
8.692017	438.614787	10.067405
8.545509	436.816895	10.072423
8.837761	430.759985	10.077440
8.438125	425.495578	10.082458
8.555189	433.846247	10.087475
8.491112	433.032708	10.092493
8.161433	441.307777	10.097511
8.676791	432.505424	10.102528
8.245923	435.422171	10.107546
8.327937	436.078509	10.112563
8.747635	432.018217	10.117581
8.394857	435.197348	10.122599
8.564647	427.644793	10.127616
8.601969	440.318501	10.132634
8.888773	438.317451	10.137651
8.687498	435.133288	10.142669
8.527782	439.875965	10.147687
8.679794	433.042509	10.152704
8.822963	442.398926	10.157722
8.619741	440.543596	10.162739
8.539864	440.126972	10.167757
8.456930	442.620338	10.172775
8.609048	433.435903	10.177792
8.442371	443.339156	10.182810
8.351480	436.313155	10.187827
8.502453	441.600722	10.192845
8.873733	449.959153	10.197863
8.749792	453.039545	10.202880
8.822213	446.379414	10.207898
8.956704	448.728479	10.212915
8.848023	437.530317	10.217933
8.432552	444.701645	10.222951
8.687289	437.801702	10.227968
8.780006	450.179628	10.232986
8.921491	457.775460	10.238003
8.976826	451.307327	10.243021
8.795022	457.053790	10.248039
8.960750	465.747176	10.253056
8.774565	455.249003	10.258074
8.648517	442.239040	10.263091
8.906937	445.285143	10.268109
9.120875	455.015539	10.273127
8.746461	448.888859	10.278144
8.754035	452.242250	10.283162
8.867943	461.988224	10.288179
9.372415	449.315566	10.293197
9.070266	446.339602	10.298215
8.691055	437.626037	10.303232
8.851639	442.287288	10.308250
8.855525	443.182998	10.313267
9.074026	451.054001	10.318285
8.933906	446.310888	10.323303
8.848088	438.968531	10.328320
9.091792	446.229722	10.333338
8.957743	440.030909	10.338355
9.040463	435.000652	10.343373
8.990718	438.009532	10.348391
9.148660	431.711613	10.353408
8.959924	429.737270	10.358426
9.072344	430.063841	10.363443
8.893591	433.127518	10.368461
9.092070	442.999163	10.373479
9.027463	431.491200	10.378496
8.916084	430.176965	10.383514
8.790783	433.838205	10.388531
9.143605	437.437626	10.393549
9.232717	449.759311	10.398567
8.892823	450.676990	10.403584
9.166865	455.822329	10.408602
8.967224	457.702736	10.413619
9.607538	454.176108	10.418637
9.182174	447.148533	10.423655
8.838511	438.934337	10.428672
8.755985	443.816468	10.433690
8.999968	449.663885	10.438707
9.400992	454.530689	10.443725
8.782553	457.934215	10.448743
9.315400	450.703802	10.453760
9.353974	454.677186	10.458778
9.126658	461.042934	10.463795
9.615292	451.193898	10.468813
9.026678	448.376139	10.473831
9.297227	452.385985	10.478848
8.911844	442.764550	10.483866
9.097782	454.850267	10.488883
9.431952	454.293442	10.493901
9.047597	457.149305	10.498919
9.346755	450.744191	10.503936
9.355354	456.107575	10.508954
9.082580	463.625904	10.513971
9.172843	457.616212	10.518989
9.191656	458.793608	10.524007
9.133990	453.706311	10.529024
8.809554	452.990110	10.534042
8.898807	454.768735	10.539059
9.111082	457.566417	10.544077
9.155414	452.586310	10.549095
9.185924	457.299374	10.554112
9.169149	453.139785	10.559130
9.475857	458.778633	10.564147
9.316026	451.141695	10.569165
9.092917	463.199591	10.574183
9.095493	460.731576	10.579200
9.444528	459.724333	10.584218
9.529853	464.659227	10.589235
9.461825	459.138062	10.594253
9.212570	460.653826	10.599271
9.400779	467.983625	10.604288
9.649860	466.414459	10.609306
9.051041	463.490994	10.614323
9.537184	474.652710	10.619341
9.505570	478.586538	10.624359
9.482692	477.870718	10.629376
9.529446	469.971245	10.634394
9.369313	472.126356	10.639411
9.353065	462.639932	10.644429
9.797039	477.355175	10.649447
9.395664	471.718656	10.654464
9.273456	465.988184	10.659482
9.494591	482.268620	10.664499
9.292687	484.187250	10.669517
9.085283	482.360967	10.674535
9.587394	481.462428	10.679552
9.904742	485.913099	10.684570
9.346698	485.643504	10.689587
9.647439	477.783374	10.694605
9.669260	485.981647	10.699623
9.565631	487.332735	10.704640
9.733881	483.715506	10.709658
9.672111	484.914917	10.714675
9.729101	486.676479	10.719693
9.769607	479.945568	10.724711
9.199096	480.031349	10.729728
9.608692	480.365298	10.734746
9.341510	488.668527	10.739763
9.806396	482.931843	10.744781
9.468064	491.624830	10.749799
9.467708	488.182168	10.754816
9.814214	488.172506	10.759834
9.445874	489.773083	10.764851
9.087809	486.212554	10.769869
9.345946	485.765392	10.774887
9.616994	480.229295	10.779904
9.575815	484.697919	10.784922
9.567793	497.656426	10.789939
10.023680	493.675688	10.794957
9.799873	493.022709	10.799975
9.526141	487.495694	10.804992
9.737805	474.631934	10.810010
9.913565	485.917719	10.815027
9.856080	476.620736	10.820045
9.563642	486.493103	10.825063
9.434749	489.003097	10.830080
10.035076	495.779614	10.835098
10.096839	507.446064	10.840115
10.166775	484.386322	10.845133
10.526430	487.148440	10.850151
10.092838	494.436212	10.855168
10.085070	471.407520	10.860186
9.725807	490.116673	10.865203
9.778844	486.747745	10.870221
9.685077	488.892525	10.875239
9.557415	496.634416	10.880256
9.874757	481.860799	10.885274
10.117126	481.536007	10.890291
10.164003	487.281587	10.895309
10.353600	484.143850	10.900327
9.813251	492.293961	10.905344
10.159242	481.776027	10.910362
9.911621	486.005408	10.915379
10.162264	478.964082	10.920397
9.871797	480.618803	10.925415
9.623281	486.426153	10.930432
9.993617	481.073403	10.935450
9.978432	487.627028	10.940467
9.682831	484.590080	10.945485
9.735929	488.154131	10.950503
9.960326	489.362633	10.955520
10.026780	488.225824	10.960538
9.741182	487.623489	10.965555
9.983225	481.325082	10.970573
10.095656	479.922351	10.975591
9.979711	485.601768	10.980608
10.061090	476.841716	10.985626
9.857018	484.377759	10.990643
10.098675	478.852549	10.995661
10.015410	483.286703	11.000679
9.832084	494.641025	11.005696
10.309577	498.101132	11.010714
10.142576	511.854383	11.015731
10.139245	501.539143	11.020749
9.788709	505.784551	11.025767
10.262570	513.303413	11.030784
10.653735	507.332057	11.035802
10.283802	502.709913	11.040819
9.956975	488.390020	11.045837
10.049587	490.934952	11.050855
10.081034	498.046184	11.055872
10.632523	502.908509	11.060890
10.295381	505.372037	11.065907
9.861965	493.072583	11.070925
9.983500	496.329347	11.075943
10.234076	504.596149	11.080960
10.142665	504.806142	11.085978
10.134761	510.689641	11.090995
9.995020	514.589821	11.096013
10.298761	518.471443	11.101031
10.349453	511.672666	11.106048
10.705200	509.856525	11.111066
10.703935	508.231664	11.116083
10.277633	515.256390	11.121101
10.295328	513.754802	11.126119
10.192072	510.725771	11.131136
10.285854	501.099124	11.136154
10.203150	509.326304	11.141171
10.179290	510.362031	11.146189
10.522856	513.243417	11.151207
10.263980	514.549254	11.156224
10.142475	512.968359	11.161242
10.306919	507.347870	11.166259
10.292598	510.676280	11.171277
10.576264	514.529471	11.176295
10.233790	510.770857	11.181312
10.435460	503.790793	11.186330
10.426248	507.803186	11.191347
10.414424	510.411716	11.196365
10.695384	506.852670	11.201383
10.484240	513.357923	11.206400
10.557472	507.215172	11.211418
10.678918	504.239515	11.216435
10.463695	503.301189	11.221453
10.638679	508.872203	11.226471
10.236111	510.960928	11.231488
10.447249	507.699918	11.236506
10.354601	509.314374	11.241523
10.378767	515.603118	11.246541
10.721985	507.853121	11.251559
10.335509	509.816269	11.256576
10.087481	511.868310	11.261594
10.442085	520.671164	11.266611
10.702317	529.715925	11.271629
10.798825	519.766965	11.276647
10.532727	510.937927	11.281664
10.826405	508.232085	11.286682
10.637836	508.697036	11.291699
10.541199	507.604553	11.296717
10.851780	506.142568	11.301735
10.160054	505.650800	11.306752
10.328669	515.624960	11.311770
10.614687	522.040187	11.316787
10.405737	535.484421	11.321805
10.558286	528.007088	11.326823
10.364356	536.630279	11.331840
10.651531	529.832544	11.336858
10.733847	526.253931	11.341875
10.687562	530.890613	11.346893
10.940134	524.906118	11.351911
10.546417	539.426804	11.356928
10.578800	532.914880	11.361946
10.914605	530.802053	11.366963
10.884857	532.072217	11.371981
11.110304	533.747598	11.376999
10.893509	537.448350	11.382016
11.025252	536.320307	11.387034
10.987394	546.115201	11.392051
10.529243	544.173324	11.397069
10.933517	537.417312	11.402087
11.056212	531.301564	11.407104
11.068411	528.396558	11.412122
10.714181	532.118707	11.417139
10.872685	532.823098	11.422157
11.085090	530.874645	11.427175
11.245407	530.518448	11.432192
11.178497	538.146761	11.437210
11.020780	529.483868	11.442227
10.640505	534.645902	11.447245
11.197135	536.282341	11.452263
11.111143	537.835806	11.457280
11.204304	538.853315	11.462298
11.146897	537.309772	11.467315
11.218586	535.534700	11.472333
11.015437	525.408340	11.477351
10.775675	532.725907	11.482368
11.130972	532.023786	11.487386
11.062861	530.087452	11.492403
10.969376	542.137842	11.497421
11.041452	527.834700	11.502439
11.055464	538.186379	11.507456
10.775626	535.680277	11.512474
10.799207	530.741247	11.517491
10.624866	539.083691	11.522509
10.970262	543.649925	11.527527
11.207017	539.166832	11.532544
10.944791	529.431504	11.537562
10.913850	529.455365	11.542579
10.844087	540.653185	11.547597
10.979275	532.421193	11.552615
11.160586	538.590808	11.557632
11.049793	540.589928	11.562650
11.240269	534.413135	11.567667
11.119832	546.937920	11.572685
11.188778	547.015653	11.577703
11.142220	556.259665	11.582720
11.285429	555.707324	11.587738
11.314949	558.766996	11.592755
11.220924	560.785598	11.597773
11.578689	557.713180	11.602791
11.102657	547.503067	11.607808
11.171554	551.099383	11.612826
11.089522	549.648032	11.617843
11.181066	551.763967	11.622861
11.399079	558.050946	11.627879
11.435317	556.865191	11.632896
11.479818	550.692186	11.637914
11.483961	555.564010	11.642931
11.285586	550.634287	11.647949
11.354519	550.525838	11.652967
11.393673	547.995313	11.657984
11.714073	553.187109	11.663002
11.349482	540.870594	11.668019
11.211873	550.122468	11.673037
11.423260	542.519209	11.678055
11.445895	559.133565	11.683072
11.474838	551.593420	11.688090
11.821856	546.720788	11.693107
11.258556	547.547028	11.698125
11.464970	547.966261	11.703143
11.941380	549.324870	11.708160
11.420410	537.515523	11.713178
11.134718	528.762107	11.718195
11.254121	548.681151	11.723213
11.599592	553.313645	11.728231
11.243678	552.709633	11.733248
11.477734	554.692932	11.738266
11.864460	545.636007	11.743283
11.432040	564.678506	11.748301
11.926444	552.064146	11.753319
11.660964	555.248640	11.758336
11.518626	560.708136	11.763354
11.842519	559.127315	11.768371
11.549635	560.268044	11.773389
11.365079	559.760423	11.778407
11.599783	556.388442	11.783424
11.593112	555.742677	11.788442
11.577145	558.304524	11.793459
11.720652	562.927442	11.798477
11.370237	556.882191	11.803495
11.650912	553.042325	11.808512
11.199011	559.326315	11.813530
11.676451	552.640952	11.818547
11.543967	553.781953	11.823565
11.398540	553.236683	11.828583
11.576434	544.228052	11.833600
11.679234	562.089043	11.838618
11.683844	555.767619	11.843635
11.648945	557.079611	11.848653
11.384001	565.388838	11.853671
11.729332	570.942816	11.858688
12.048824	579.233635	11.863706
11.992392	579.371913	11.868723
11.726908	584.913704	11.873741
11.984575	574.087590	11.878759
11.948540	579.167638	11.883776
12.115185	581.757858	11.888794
12.143481	568.244109	11.893811
11.858228	562.242357	11.898829
11.447363	557.411986	11.903847
11.898348	560.251410	11.908864
12.136559	568.889381	11.913882
11.928956	582.841505	11.918899
11.893847	565.339386	11.923917
11.966753	573.315160	11.928935
12.015337	571.373275	11.933952
11.990578	582.112852	11.938970
11.890663	569.622570	11.943987
11.807309	580.645814	11.949005
12.073204	578.581735	11.954023
12.116749	571.758802	11.959040
11.799703	578.050203	11.964058
11.906123	571.359486	11.969075
11.641947	572.789224	11.974093
11.778931	571.439466	11.979111
11.973194	575.855677	11.984128
11.868852	575.638512	11.989146
11.886449	571.341005	11.994163
11.828572	572.659732	11.999181
11.627881	581.552229	12.004199
12.440965	590.488854	12.009216
12.369874	590.023524	12.014234
12.297704	578.892169	12.019251
12.356992	586.746997	12.024269
12.160600	579.131475	12.029287
12.003027	578.300929	12.034304
12.181794	583.574744	12.039322
12.316235	564.228557	12.044339
12.053181	571.107972	12.049357
12.000340	576.032853	12.054375
12.521144	582.219050	12.059392
12.467915	585.140138	12.064410
12.024755	578.642279	12.069427
12.289695	592.167401	12.074445
11.968086	600.958819	12.079463
12.373400	595.976116	12.084480
12.470362	604.995844	12.089498
12.447512	605.078403	12.094515
12.445596	601.550758	12.099533
11.881011	608.578116	12.104551
12.367330	595.037214	12.109568
12.332201	602.152542	12.114586
12.503384	601.438060	12.119603
12.171263	606.889251	12.124621
12.317830	605.822009	12.129639
12.343841	603.930971	12.134656
12.388105	598.234494	12.139674
12.584586	607.405980	12.144691
12.669884	597.651219	12.149709
12.444867	599.197934	12.154727
12.541343	600.426360	12.159744
12.266751	606.016911	12.164762
12.802700	601.149561	12.169779
12.657157	597.417071	12.174797
12.487144	606.503612	12.179815
12.701851	601.238171	12.184832
12.897421	596.632093	12.189850
12.339606	580.069689	12.194867
12.566585	596.425056	12.199885
12.422416	599.562269	12.204903
12.459523	601.339560	12.209920
12.379565	607.067059	12.214938
12.345722	609.473912	12.219955
12.660003	600.402993	12.224973
12.176572	604.344081	12.229991
12.801087	606.575849	12.235008
12.407717	602.869320	12.240026
12.243886	602.585680	12.245043
12.657626	596.352015	12.250061
12.107304	604.560531	12.255079
12.489695	604.387499	12.260096
12.719931	627.479770	12.265114
13.015332	623.044327	12.270131
13.107930	616.428327	12.275149
12.971062	600.046507	12.280167
12.676698	596.021619	12.285184
12.617261	599.817799	12.290202
12.438678	602.748940	12.295219
12.871852	614.928811	12.300237
12.841838	622.500925	12.305255
13.226018	615.760634	12.310272
13.027421	602.509394	12.315290
12.838283	602.185515	12.320307
13.046529	611.979997	12.325325
12.579162	606.659811	12.330343
13.446608	601.134957	12.335360
12.913928	595.853345	12.340378
12.859000	592.340267	12.345395
13.378805	601.597104	12.350413
13.040857	606.089875	12.355431
13.061537	592.634095	12.360448
12.775714	604.869102	12.365466
13.076007	600.054222	12.370483
13.135588	604.971073	12.375501
12.798452	606.345904	12.380519
13.327305	599.643052	12.385536
12.951972	601.964223	12.390554
12.755884	602.502927	12.395571
13.197982	602.819197	12.400589
12.970251	606.802521	12.405607
13.015079	596.984636	12.410624
12.867795	598.014339	12.415642
12.886619	598.529049	12.420659
12.993154	592.892304	12.425677
12.861774	604.860278	12.430695
13.073594	593.615272	12.435712
12.940458	591.995156	12.440730
12.896950	612.662288	12.445747
13.324900	616.698156	12.450765
13.070581	620.423701	12.455783
13.169729	627.423462	12.460800
12.987288	622.680580	12.465818
13.173678	620.193390	12.470835
12.932517	621.966674	12.475853
13.212517	627.603422	12.480871
13.256521	625.204670	12.485888
13.306378	621.145117	12.490906
13.268361	620.144481	12.495923
13.619341	624.025084	12.500941
13.353552	628.462446	12.505959
12.999691	623.746253	12.510976
13.343452	625.393754	12.515994
13.163270	619.337756	12.521011
13.731231	624.828687	12.526029
13.610438	636.779255	12.531047
13.633050	616.039831	12.536064
13.242320	621.370769	12.541082
13.409749	615.768715	12.546099
13.698198	616.048949	12.551117
13.305225	625.864465	12.556135
13.231384	621.707410	12.561152
13.542141	623.322182	12.566170
13.346965	616.265011	12.571187
13.305616	625.776482	12.576205
13.041704	630.948827	12.581223
13.640418	621.738942	12.586240
13.538107	618.312128	12.591258
13.157934	619.412805	12.596275
13.475981	624.185282	12.601293
13.244470	636.153088	12.606311
13.358451	618.403650	12.611328
13.353238	619.972946	12.616346
13.280271	629.883802	12.621363
13.576051	632.599086	12.626381
13.979085	646.074346	12.631399
13.569870	639.643761	12.636416
13.624424	627.473358	12.641434
13.531576	636.538433	12.646451
13.454701	644.007403	12.651469
13.358698	652.542822	12.656487
13.705484	649.636194	12.661504
13.758021	648.766620	12.666522
13.487225	642.914063	12.671539
13.607863	647.114546	12.676557
13.796366	649.805511	12.681575
13.922063	650.085840	12.686592
13.932165	647.954286	12.691610
13.756886	657.313062	12.696627
14.141757	641.714630	12.701645
14.210492	649.271381	12.706663
13.957445	643.611713	12.711680
13.987136	637.567212	12.716698
13.596062	638.455000	12.721715
13.669916	637.695712	12.726733
13.825330	640.950384	12.731751
14.079438	639.383577	12.736768
14.148906	645.046798	12.741786
13.850518	647.144564	12.746803
14.178815	629.923459	12.751821
13.922481	631.692795	12.756839
13.793463	620.339899	12.761856
13.942936	628.423692	12.766874
13.478227	638.089444	12.771891
14.337771	640.893671	12.776909
14.099060	650.375925	12.781927
14.272585	646.262399	12.786944
14.066282	637.092640	12.791962
13.756920	635.064474	12.796979
14.206614	638.573117	12.801997
13.987102	644.281332	12.807015
14.256205	641.364710	12.812032
14.003747	633.458104	12.817050
13.690407	645.583818	12.822067
14.070848	638.418083	12.827085
14.194820	646.423807	12.832103
13.875186	653.182679	12.837120
13.940804	646.454107	12.842138
14.034900	648.598058	12.847155
14.040993	641.875600	12.852173
13.753948	648.645175	12.857191
13.939558	649.853416	12.862208
14.467573	645.902439	12.867226
14.024192	650.951260	12.872243
14.250109	646.138480	12.877261
13.954406	646.711629	12.882279
13.941856	649.490699	12.887296
14.236564	663.115378	12.892314
14.352312	672.394138	12.897331
14.029338	676.430175	12.902349
14.510326	674.203213	12.907367
14.185395	677.021457	12.912384
14.352229	674.963323	12.917402
14.442880	679.294710	12.922419
14.510083	672.603750	12.927437
14.795786	671.325500	12.932455
14.591808	667.977620	12.937472
14.593908	649.150545	12.942490
14.056414	654.131972	12.947507
14.367544	653.935322	12.952525
14.753199	661.136632	12.957543
14.576356	659.728435	12.962560
14.637237	654.780408	12.967578
14.753770	647.529531	12.972595
14.447718	647.214387	12.977613
14.710162	643.509880	12.982631
14.291460	644.509263	12.987648
14.482104	643.132210	12.992666
14.282467	644.356253	12.997683
14.707538	663.129654	13.002701
14.995052	663.359544	13.007719
14.771316	651.226142	13.012736
14.825655	639.699524	13.017754
14.272714	656.125886	13.022771
14.659225	638.103631	13.027789
14.444467	651.615126	13.032807
14.659095	656.129169	13.037824
14.802310	654.929908	13.042842
14.754395	669.235919	13.047859
14.715452	659.828660	13.052877
14.838364	656.489844	13.057895
14.643758	659.189968	13.062912
14.765824	662.459303	13.067930
14.745871	674.274279	13.072947
14.898401	669.192063	13.077965
14.732978	669.950048	13.082983
14.737090	674.670436	13.088000
14.401153	673.640446	13.093018
14.695862	670.164431	13.098035
14.319438	669.961225	13.103053
14.947421	666.338650	13.108071
14.645992	682.422930	13.113088
14.797500	669.126598	13.118106
14.727765	670.434555	13.123123
14.484050	664.704002	13.128141
14.715425	670.562922	13.133159
14.978449	680.661326	13.138176
15.268842	690.736541	13.143194
14.939930	679.073916	13.148211
14.888916	678.419272	13.153229
14.856710	683.962641	13.158247
14.899955	690.349459	13.163264
15.353810	682.336016	13.168282
15.167060	699.245027	13.173299
14.946483	695.539976	13.178317
15.296663	681.789838	13.183335
14.757000	682.129583	13.188352
14.772685	687.425664	13.193370
14.907173	690.216560	13.198387
15.119352	685.311237	13.203405
15.327261	688.731308	13.208423
15.045652	689.538941	13.213440
15.254955	692.523310	13.218458
15.252899	682.649564	13.223475
15.217109	689.802898	13.228493
15.266170	687.551668	13.233511
15.146447	692.657401	13.238528
15.170646	693.322751	13.243546
15.268153	694.844503	13.248563
14.853240	693.605910	13.253581
15.257377	692.271350	13.258599
15.359548	684.464136	13.263616
15.587548	682.112465	13.268634
15.289355	692.793700	13.273651
14.991125	682.173987	13.278669
15.445680	690.500633	13.283687
14.979186	692.826541	13.288704
15.196824	689.400390	13.293722
14.692574	700.129490	13.298739
15.474103	711.289546	13.303757
15.477149	720.491207	13.308775
15.270867	721.536414	13.313792
15.452224	719.286672	13.318810
15.544377	722.112566	13.323827
15.699353	723.682176	13.328845
15.814227	713.124354	13.333863
15.423728	720.762103	13.338880
15.330082	718.384770	13.343898
15.649635	719.083027	13.348915
15.466101	722.507248	13.353933
15.636022	709.574081	13.358951
15.461650	722.246236	13.363968
15.675427	724.188531	13.368986
15.979082	721.421146	13.374003
15.466639	714.978205	13.379021
15.477953	712.773873	13.384039
15.581660	713.650898	13.389056
15.535661	715.362248	13.394074
15.505769	709.222861	13.399091
15.625692	715.711355	13.404109
15.927395	718.769701	13.409127
15.180426	715.667294	13.414144
15.500784	716.040389	13.419162
15.638607	726.480194	13.424179
15.692943	722.442010	13.429197
16.164212	734.530828	13.434215
15.776982	727.935846	13.439232
15.536613	721.709309	13.444250
15.841218	738.627059	13.449267
15.768256	743.823353	13.454285
16.387982	735.992338	13.459303
15.710304	731.304443	13.464320
15.870677	734.047136	13.469338
16.090543	732.791755	13.474355
15.866300	731.927402	13.479373
16.090298	734.802195	13.484391
16.250685	727.901053	13.489408
15.962649	719.334094	13.494426
16.203336	722.815338	13.499443
15.861933	719.460443	13.504461
15.980567	707.153780	13.509479
16.023717	717.365331	13.514496
15.928602	712.580427	13.519514
16.329473	714.790227	13.524531
16.009656	720.198513	13.529549
16.140690	714.295992	13.534567
16.145727	731.699020	13.539584
15.875758	723.331211	13.544602
16.029743	726.242150	13.549619
16.190886	740.269523	13.554637
16.561378	731.852485	13.559655
15.985484	742.024738	13.564672
15.914844	737.447448	13.569690
16.003050	744.748752	13.574707
16.078329	744.134400	13.579725
16.457141	740.875643	13.584743
16.062100	739.643419	13.589760
16.091661	739.629459	13.594778
16.219496	744.185439	13.599795
15.817208	741.632102	13.604813
16.509091	738.453985	13.609831
16.246118	744.093261	13.614848
16.451464	740.672170	13.619866
16.092193	739.071471	13.624883
16.217210	742.210977	13.629901
16.386888	737.886596	13.634919
16.075101	756.516055	13.639936
16.287953	761.380685	13.644954
16.462068	762.502363	13.649971
16.665605	757.784553	13.654989
16.737627	769.881910	13.660007
16.827534	772.285296	13.665024
16.873294	769.368714	13.670042
16.722462	744.575811	13.675059
16.330479	753.040600	13.680077
16.573633	736.627887	13.685095
16.703806	746.125339	13.690112
16.604249	744.455802	13.695130
16.538915	744.014817	13.700147
16.513077	752.422598	13.705165
16.697679	740.692603	13.710183
16.630149	752.764340	13.715200
16.702705	758.452362	13.720218
16.436359	746.896712	13.725235
16.855805	764.749631	13.730253
16.840445	755.408075	13.735271
16.699830	762.543046	13.740288
16.869552	764.116676	13.745306
17.018354	762.433713	13.750323
16.961803	755.111914	13.755341
17.047497	746.704498	13.760359
16.798866	745.884965	13.765376
16.027601	739.646409	13.770394
16.911655	751.374333	13.775411
16.758570	761.007410	13.780429
16.870512	756.316485	13.785447
16.949218	760.817004	13.790464
16.861155	762.446548	13.795482
16.830810	756.786883	13.800499
16.854675	766.455528	13.805517
16.931290	758.895250	13.810535
16.868244	761.142573	13.815552
16.857366	761.646133	13.820570
16.896088	754.426262	13.825587
16.882715	757.353796	13.830605
16.770731	755.316974	13.835623
16.907001	763.522801	13.840640
16.992865	753.278732	13.845658
17.165217	756.858981	13.850675
17.120162	772.070318	13.855693
17.294335	755.551567	13.860711
17.126492	755.375844	13.865728
16.927717	762.775483	13.870746
17.358995	770.430468	13.875763
17.082993	764.294668	13.880781
17.391638	760.740728	13.885799
17.443927	769.773807	13.890816
16.834586	772.241883	13.895834
17.152117	762.457186	13.900851
16.914045	773.861233	13.905869
17.301526	775.495630	13.910887
17.311509	786.214144	13.915904
17.579725	794.910667	13.920922
17.589168	787.685874	13.925939
17.149359	793.485239	13.930957
17.567533	777.550153	13.935975
17.337641	788.836175	13.940992
17.507939	786.051675	13.946010
17.764098	779.965554	13.951027
17.426385	777.774532	13.956045
17.658473	767.681252	13.961063
17.461006	759.213778	13.966080
17.277144	767.778710	13.971098
17.575783	757.520444	13.976115
16.891103	763.623004	13.981133
17.447706	776.247658	13.986151
17.511079	780.636964	13.991168
17.628383	786.381143	13.996186
17.414486	784.697846	14.001203
17.418459	787.559570	14.006221
17.464602	790.929109	14.011239
17.542099	792.933655	14.016256
17.599881	784.353846	14.021274
17.664753	778.265951	14.026291
17.449013	786.466637	14.031309
17.743055	792.028670	14.036327
17.741352	780.381303	14.041344
17.687729	779.171656	14.046362
17.932771	777.581002	14.051379
17.792570	780.253739	14.056397
17.873844	783.892354	14.061415
17.929675	784.344505	14.066432
17.500966	777.774898	14.071450
18.105113	775.677066	14.076467
17.997328	781.055513	14.081485
18.039530	783.119199	14.086503
17.930173	782.025524	14.091520
17.726566	789.684695	14.096538
18.063522	782.516206	14.101555
17.986672	787.365990	14.106573
18.022200	783.753586	14.111591
17.927467	782.692346	14.116608
17.820441	797.026598	14.121626
17.799742	776.350534	14.126643
18.160382	788.283048	14.131661
17.948069	790.698779	14.136679
18.501170	785.541539	14.141696
18.080490	789.624371	14.146714
18.049500	780.553471	14.151731
17.652654	787.198187	14.156749
17.825454	784.113505	14.161767
18.076987	793.904503	14.166784
18.496417	810.940139	14.171802
18.351437	800.088218	14.176819
18.302947	786.261220	14.181837
17.880056	790.066694	14.186855
18.253423	791.507636	14.191872
18.157233	805.543570	14.196890
18.371149	795.459415	14.201907
18.319351	804.707527	14.206925
18.629449	800.815692	14.211943
18.404399	784.889231	14.216960
18.015896	787.670055	14.221978
18.228794	782.616275	14.226995
18.491822	798.271959	14.232013
18.759942	799.470519	14.237031
18.561517	784.581300	14.242048
18.611867	786.164050	14.247066
18.611663	774.510142	14.252083
18.803951	774.126873	14.257101
18.270521	779.934498	14.262119
18.515271	778.287087	14.267136
18.137758	787.942499	14.272154
18.236041	776.585671	14.277171
18.658871	787.678550	14.282189
18.599272	800.986125	14.287207
18.786003	804.235951	14.292224
18.657802	796.587629	14.297242
18.548419	786.355005	14.302259
18.635141	789.784497	14.307277
18.653396	801.912336	14.312295
19.082093	795.928730	14.317312
18.700830	785.082049	14.322330
18.654462	776.843499	14.327347
18.499083	779.092577	14.332365
18.878024	791.189497	14.337383
18.849291	795.555279	14.342400
18.247822	793.815564	14.347418
18.683107	790.683701	14.352435
18.853887	798.906262	14.357453
18.577826	800.792291	14.362471
18.699872	800.899627	14.367488
18.741548	798.457034	14.372506
19.074921	800.809894	14.377523
18.976579	792.431110	14.382541
18.667029	798.670930	14.387559
18.922798	797.214300	14.392576
18.640976	800.789534	14.397594
18.442475	795.244399	14.402611
18.872295	809.028029	14.407629
18.994235	805.714583	14.412647
19.212182	808.303160	14.417664
19.169960	808.442383	14.422682
19.679204	800.596984	14.427699
19.426866	801.627276	14.432717
19.161790	805.051586	14.437735
19.222381	804.534191	14.442752
19.342647	799.652615	14.447770
19.331732	791.894518	14.452787
19.354085	798.177333	14.457805
19.087978	800.670866	14.462823
19.463670	794.474613	14.467840
19.393133	795.460820	14.472858
19.395347	789.228047	14.477875
19.679436	792.260747	14.482893
19.433717	799.929635	14.487911
19.616420	793.072328	14.492928
19.072907	777.791888	14.497946
19.343806	789.463829	14.502963
19.413407	789.519371	14.507981
19.332037	801.486002	14.512999
19.497271	792.375077	14.518016
19.346827	793.518889	14.523034
19.290894	795.219171	14.528051
19.599504	793.665954	14.533069
19.094590	789.244626	14.538087
19.539654	796.480922	14.543104
19.523462	795.640976	14.548122
19.405504	792.084025	14.553139
19.450927	790.483426	14.558157
19.266115	792.610860	14.563175
19.086336	797.921629	14.568192
19.455500	790.675540	14.573210
19.211696	796.652665	14.578227
19.417316	798.245954	14.583245
19.378673	810.679296	14.588263
19.920212	813.905438	14.593280
19.273148	822.343705	14.598298
19.691649	812.388629	14.603315
19.938960	806.477441	14.608333
19.869378	813.247933	14.613351
19.674020	824.923066	14.618368
19.805401	822.179332	14.623386
19.559474	819.790982	14.628403
19.718220	812.757522	14.633421
19.441016	817.995105	14.638439
19.706551	814.533071	14.643456
19.924149	815.256674	14.648474
19.509233	820.417872	14.653491
19.499007	823.035665	14.658509
19.588793	835.515298	14.663527
19.966371	836.662106	14.668544
20.178769	832.397321	14.673562
19.913380	837.087131	14.678579
20.412028	832.484295	14.683597
20.351426	841.383513	14.688615
20.162222	825.789097	14.693632
19.877109	820.339487	14.698650
19.909158	825.610972	14.703667
20.012860	831.417241	14.708685
20.115054	836.608382	14.713703
20.411080	836.713876	14.718720
20.359252	832.982523	14.723738
20.093425	833.844508	14.728755
20.495448	833.980834	14.733773
20.137449	832.597673	14.738791
20.180161	820.176524	14.743808
20.310196	832.949682	14.748826
20.234838	831.822308	14.753843
20.351091	821.930065	14.758861
20.163382	832.199716	14.763879
20.566807	827.393963	14.768896
20.529731	825.790427	14.773914
20.189307	839.271138	14.778931
20.474395	826.843804	14.783949
20.112997	833.113799	14.788967
20.103339	833.954834	14.793984
20.269338	824.386194	14.799002
20.151756	840.167445	14.804019
20.514291	828.655834	14.809037
20.458231	838.516838	14.814055
20.743891	835.206298	14.819072
20.757074	831.401708	14.824090
20.394573	838.167324	14.829107
20.467502	831.355496	14.834125
20.686159	843.641505	14.839143
20.916418	840.203893	14.844160
20.812992	836.007215	14.849178
20.402638	843.581837	14.854195
20.571422	834.640748	14.859213
20.582824	847.009520	14.864231
20.520498	833.067878	14.869248
20.393303	826.183071	14.874266
20.481256	840.619540	14.879283
20.980904	850.476078	14.884301
20.923048	862.006753	14.889319
20.784111	857.657812	14.894336
21.031726	851.355251	14.899354
20.680668	857.677292	14.904371
20.944264	861.517905	14.909389
20.971745	862.031274	14.914407
20.614787	866.047399	14.919424
20.866387	859.255078	14.924442
20.832168	859.844324	14.929459
20.898159	857.290643	14.934477
21.007707	861.881058	14.939495
21.055728	859.573165	14.944512
21.017115	861.043543	14.949530
21.073480	865.560190	14.954547
21.154288	860.088309	14.959565
21.100165	863.725932	14.964583
21.112636	866.901918	14.969600
21.421893	861.710040	14.974618
21.171078	865.886359	14.979635
21.393685	863.649111	14.984653
21.062194	861.185717	14.989671
21.101187	859.835415	14.994688
21.640694	860.082877	14.999706
21.389857	866.013784	15.004723
21.162846	860.842287	15.009741
20.939137	862.960007	15.014759
20.844975	866.950994	15.019776
21.287211	853.776513	15.024794
20.964166	870.754243	15.029811
21.580271	888.150643	15.034829
21.754508	895.451236	15.039847
21.337321	883.985252	15.044864
21.326209	869.353970	15.049882
21.137468	878.692869	15.054899
21.310760	885.744302	15.059917
21.304357	891.189047	15.064935
21.438424	890.556070	15.069952
21.866740	885.986262	15.074970
21.693351	898.604742	15.079987
21.630784	886.427151	15.085005
21.768965	889.321643	15.090023
21.655810	885.987982	15.095040
21.803182	878.407170	15.100058
21.643320	881.925563	15.105075
21.808295	885.519610	15.110093
21.802217	884.330955	15.115111
21.619191	888.436766	15.120128
21.879352	884.189779	15.125146
21.773563	890.060242	15.130163
21.783667	889.635910	15.135181
22.082785	889.548423	15.140199
21.826882	890.648701	15.145216
22.203028	884.196732	15.150234
21.946204	891.412963	15.155251
22.001403	876.888113	15.160269
21.957066	877.624099	15.165287
21.828290	888.219114	15.170304
22.153004	885.457892	15.175322
22.088586	884.890532	15.180339
21.827817	888.456195	15.185357
21.775038	886.624729	15.190375
21.957534	883.604791	15.195392
22.565992	882.957913	15.200410
22.018718	884.800973	15.205427
21.984591	879.864520	15.210445
22.065575	889.003642	15.215463
21.751488	880.797259	15.220480
22.076499	877.868739	15.225498
21.668449	877.408528	15.230515
21.921106	876.842293	15.235533
22.280546	887.771540	15.240551
22.394721	901.702214	15.245568
22.362537	899.719222	15.250586
22.493780	901.314633	15.255603
22.525259	907.084836	15.260621
22.352427	897.000880	15.265639
22.015832	886.573207	15.270656
22.291384	892.794543	15.275674
22.365785	898.002652	15.280691
22.517633	896.647399	15.285709
22.989030	892.269693	15.290727
22.377027	903.877207	15.295744
22.968928	897.019264	15.300762
22.531719	890.327864	15.305779
22.370404	888.626904	15.310797
22.471972	890.368942	15.315815
22.891180	893.121852	15.320832
22.743518	877.151702	15.325850
22.482379	882.311065	15.330867
22.527283	885.384177	15.335885
22.890370	895.220977	15.340903
22.871980	898.562716	15.345920
22.881881	892.988258	15.350938
22.762975	898.374784	15.355955
22.892513	898.253741	15.360973
22.708207	889.313951	15.365991
22.633419	894.311763	15.371008
22.898500	885.570245	15.376026
23.199135	898.480986	15.381043
22.872418	900.996593	15.386061
22.949437	892.205459	15.391079
22.874872	891.627055	15.396096
22.924421	895.668256	15.401114
22.707339	900.344248	15.406131
22.859914	900.954905	15.411149
22.991897	889.744233	15.416167
23.239040	902.559167	15.421184
22.907495	892.503080	15.426202
22.843141	897.578162	15.431219
23.071639	899.805356	15.436237
23.181565	896.159256	15.441255
23.010161	908.010590	15.446272
23.070099	889.991592	15.451290
22.915803	898.192230	15.456307
22.935377	899.132856	15.461325
23.123832	897.876043	15.466343
22.748280	903.804290	15.471360
23.283984	906.535908	15.476378
23.519876	921.763590	15.481395
23.580822	923.956915	15.486413
23.723504	914.647473	15.491431
22.833895	912.069001	15.496448
23.441843	912.876996	15.501466
23.397761	915.452739	15.506483
23.794326	915.829751	15.511501
23.944197	915.225871	15.516519
23.493368	909.050969	15.521536
23.318845	902.561657	15.526554
23.419794	901.694000	15.531571
23.349941	922.469733	15.536589
23.451600	914.198604	15.541607
23.757704	923.226956	15.546624
23.721298	915.794659	15.551642
23.546557	915.294966	15.556659
23.338099	915.759868	15.561677
23.829722	916.033720	15.566695
23.456849	913.822909	15.571712
24.143734	912.573696	15.576730
23.765995	915.819912	15.581747
23.681591	911.620254	15.586765
23.822714	912.052817	15.591783
23.657794	919.699709	15.596800
23.793346	912.464697	15.601818
24.006099	919.254386	15.606835
23.360388	920.898186	15.611853
23.941111	914.174518	15.616871
23.697664	917.503965	15.621888
24.114981	915.706600	15.626906
23.963567	920.492292	15.631923
24.036350	917.394757	15.636941
24.019621	919.338250	15.641959
24.026261	920.284046	15.646976
23.932921	924.126599	15.651994
24.029416	921.694388	15.657011
23.999141	926.366549	15.662029
24.787405	926.909790	15.667047
24.498642	922.120266	15.672064
24.034342	920.658976	15.677082
24.155581	907.212548	15.682099
23.883489	916.532886	15.687117
23.958966	916.382392	15.692135
24.164665	927.020026	15.697152
24.417926	934.870053	15.702170
24.066444	948.011748	15.707187
24.196056	941.970520	15.712205
24.393911	943.931098	15.717223
24.281370	944.494672	15.722240
24.439481	940.449749	15.727258
24.827818	938.906197	15.732275
24.287695	948.448161	15.737293
24.408614	945.901693	15.742311
24.381761	948.645168	15.747328
24.625213	943.624455	15.752346
24.473831	937.658536	15.757363
24.088022	937.592485	15.762381
24.634622	940.767371	15.767399
24.503214	955.342227	15.772416
24.627877	936.117077	15.777434
24.642007	949.441685	15.782451
24.675342	960.263962	15.787469
25.068711	959.559054	15.792487
24.965542	962.323880	15.797504
24.712773	944.539702	15.802522
24.887685	944.724013	15.807539
25.044592	959.115130	15.812557
25.306431	936.987426	15.817575
24.930787	942.022626	15.822592
24.896337	937.515388	15.827610
25.140346	933.520207	15.832627
25.091351	945.920542	15.837645
24.794546	942.681735	15.842663
25.049536	941.089518	15.847680
24.601896	942.424775	15.852698
24.848142	943.358513	15.857715
24.705217	961.516935	15.862733
24.777120	955.689811	15.867751
25.100588	954.361481	15.872768
24.837464	959.208757	15.877786
25.173645	956.606682	15.882803
25.160084	965.681671	15.887821
25.118883	965.060201	15.892839
24.874882	960.301567	15.897856
25.349890	958.974889	15.902874
25.212685	953.934546	15.907891
25.082553	956.763528	15.912909
25.651253	946.737656	15.917927
25.684998	958.023763	15.922944
25.457760	957.999293	15.927962
25.650422	953.248412	15.932979
25.283489	957.531192	15.937997
25.423668	959.213579	15.943015
25.332014	960.537592	15.948032
25.627133	952.214235	15.953050
25.674637	948.805056	15.958067
25.355066	956.043706	15.963085
25.787257	957.207265	15.968103
25.959775	956.410512	15.973120
25.273431	953.598419	15.978138
25.224354	954.407728	15.983155
25.292403	972.962494	15.988173
25.740295	969.014456	15.993191
26.192033	977.893931	15.998208
25.977655	972.026170	16.003226
26.119799	968.924138	16.008243
25.942356	960.787960	16.013261
25.836815	945.426561	16.018279
25.992390	947.523107	16.023296
25.822228	954.321935	16.028314
25.951769	950.776910	16.033331
25.669932	953.721028	16.038349
26.087537	971.874237	16.043367
26.074022	963.116099	16.048384
26.293863	971.978029	16.053402
26.276241	951.982922	16.058419
25.941367	959.261825	16.063437
26.303791	950.344176	16.068455
25.761664	956.620262	16.073472
25.769115	960.860532	16.078490
25.953258	962.674926	16.083507
26.197550	973.290801	16.088525
26.202146	964.432013	16.093543
26.384042	974.590553	16.098560
26.407264	972.936590	16.103578
26.297052	961.788828	16.108595
26.422472	968.409099	16.113613
26.240731	967.159428	16.118631
26.141762	976.913582	16.123648
26.200603	976.052478	16.128666
26.463493	966.998842	16.133683
26.296880	973.109172	16.138701
26.310876	972.169845	16.143719
26.258832	968.438497	16.148736
26.382151	978.407347	16.153754
26.494698	972.943112	16.158771
26.233525	990.129069	16.163789
26.513919	1000.786675	16.168807
26.582547	1000.656181	16.173824
26.494792	1000.379624	16.178842
26.789384	988.196847	16.183859
26.515805	993.219326	16.188877
26.741642	990.943690	16.193895
26.778907	1002.671082	16.198912
26.490964	1004.145578	16.203930
27.034298	998.904593	16.208947
26.942253	994.810245	16.213965
27.009105	997.592785	16.218983
26.936593	1001.668793	16.224000
26.835483	1004.161911	16.229018
26.664738	988.611814	16.234035
26.754314	989.121831	16.239053
26.950142	994.285817	16.244071
27.173287	984.572497	16.249088
26.874210	991.855306	16.254106
27.252845	987.709766	16.259123
26.945285	995.501974	16.264141
26.947813	986.504644	16.269159
27.077833	988.201238	16.274176
26.973037	1006.615696	16.279194
27.236641	994.428272	16.284211
27.159113	988.229935	16.289229
27.108372	993.861492	16.294247
27.325117	992.246824	16.299264
27.433477	1010.120022	16.304282
27.956659	999.662558	16.309299
27.509498	986.134157	16.314317
27.295318	974.522900	16.319335
27.631184	979.611430	16.324352
27.520518	981.124594	16.329370
27.354051	972.835225	16.334387
27.331157	982.621719	16.339405
27.567929	973.654196	16.344423
27.655907	970.093547	16.349440
27.972928	976.964852	16.354458
27.358680	981.702703	16.359475
27.601053	974.785544	16.364493
27.534562	976.436995	16.369511
27.873141	978.665994	16.374528
27.729218	978.297199	16.379546
27.875888	980.038536	16.384563
27.762079	978.860336	16.389581
27.568160	970.329094	16.394599
28.132791	976.363442	16.399616
27.820129	981.530856	16.404634
27.763625	977.528806	16.409651
27.795333	978.142505	16.414669
28.002412	992.440632	16.419687
28.209941	985.961232	16.424704
28.077124	995.439805	16.429722
28.156210	995.127804	16.434739
28.040111	981.642534	16.439757
27.816239	984.713330	16.444775
27.989296	988.612248	16.449792
28.097069	996.544914	16.454810
28.383470	999.040812	16.459827
28.011886	992.736780	16.464845
27.918398	992.596813	16.469863
27.844426	994.675456	16.474880
27.839124	998.131939	16.479898
27.866237	1001.094234	16.484915
27.988363	1000.412620	16.489933
28.084852	1005.693060	16.494951
28.498450	1010.283510	16.499968
28.323958	1025.950711	16.504986
28.492559	1022.090325	16.510003
28.684536	1026.838360	16.515021
28.280469	1025.654857	16.520039
28.783952	1025.529239	16.525056
28.721455	1023.039720	16.530074
28.797333	1018.243889	16.535091
28.397926	1004.105290	16.540109
28.518244	1006.185242	16.545127
28.740596	1010.672927	16.550144
28.716360	1012.882682	16.555162
28.467107	1003.444871	16.560179
28.610071	1008.538197	16.565197
28.597778	1019.777863	16.570215
29.046821	1004.352157	16.575232
28.949251	1026.694424	16.580250
29.153502	1018.650267	16.585267
29.236260	1012.919263	16.590285
28.797096	999.209729	16.595303
28.871796	990.570383	16.600320
28.574676	1000.775117	16.605338
28.753016	1001.590045	16.610355
29.214191	1015.978016	16.615373
29.223181	1016.926607	16.620391
28.889021	1013.147657	16.625408
28.991497	1016.713593	16.630426
28.741576	1016.519088	16.635443
28.665710	1018.752661	16.640461
28.880012	1020.316217	16.645479
29.018286	1019.401718	16.650496
29.080389	1016.078615	16.655514
29.087954	1011.328136	16.660531
29.101239	1020.572539	16.665549
29.035439	1028.109372	16.670567
29.376994	1030.375784	16.675584
29.505165	1038.980626	16.680602
29.234714	1040.944700	16.685619
29.335061	1037.868099	16.690637
29.646969	1041.505573	16.695655
29.389990	1030.203896	16.700672
29.181007	1040.896695	16.705690
29.483156	1044.816551	16.710707
29.700430	1037.660282	16.715725
29.669127	1048.659933	16.720743
29.733299	1040.558681	16.725760
29.551700	1041.369693	16.730778
29.907912	1036.766893	16.735795
30.070132	1034.983987	16.740813
29.677195	1048.084874	16.745831
30.044713	1034.549513	16.750848
29.588057	1043.422134	16.755866
29.623387	1036.578212	16.760883
29.825588	1034.773303	16.765901
29.523502	1039.730806	16.770919
29.565577	1034.356419	16.775936
29.637512	1039.372452	16.780954
29.578167	1053.661617	16.785971
29.837906	1055.407447	16.790989
29.886911	1060.114635	16.796007
30.110546	1054.342749	16.801024
30.113417	1055.560536	16.806042
30.044742	1065.212193	16.811059
30.584920	1055.616729	16.816077
30.250227	1062.731546	16.821095
30.323402	1056.503409	16.826112
30.305970	1059.425313	16.831130
30.515123	1066.802590	16.836147
30.482128	1060.881313	16.841165
30.246465	1066.579553	16.846183
30.225687	1056.743228	16.851200
30.271153	1056.770971	16.856218
29.981944	1061.407744	16.861235
30.011880	1060.222937	16.866253
30.163488	1067.694380	16.871271
30.302140	1065.811001	16.876288
30.545155	1061.680248	16.881306
30.203356	1062.913829	16.886323
30.819785	1061.126474	16.891341
30.303433	1074.606352	16.896359
30.878167	1080.541335	16.901376
30.669800	1084.657448	16.906394
30.726187	1083.149789	16.911411
31.310707	1085.974820	16.916429
30.710920	1065.615796	16.921447
30.952254	1060.144106	16.926464
30.717875	1058.571267	16.931482
30.608008	1054.848904	16.936499
30.854301	1066.177725	16.941517
30.764237	1086.331954	16.946535
31.079398	1071.283637	16.951552
31.145938	1078.541114	16.956570
31.042959	1076.004242	16.961587
31.193343	1077.375785	16.966605
31.340161	1085.239296	16.971623
31.167916	1072.254999	16.976640
31.107764	1054.172482	16.981658
30.863531	1053.497415	16.986675
31.527603	1063.300070	16.991693
31.256182	1074.677944	16.996711
31.328900	1078.983819	17.001728
31.009143	1081.659311	17.006746
31.598074	1086.137277	17.011763
31.393821	1073.899567	17.016781
31.540168	1080.141086	17.021799
31.308730	1073.540654	17.026816
31.071542	1074.164664	17.031834
31.006261	1083.866296	17.036851
31.219850	1074.037651	17.041869
31.239367	1089.841958	17.046887
31.428139	1076.637349	17.051904
31.529775	1079.108377	17.056922
31.415343	1079.599668	17.061939
31.618477	1081.060827	17.066957
31.277709	1082.155396	17.071975
31.270544	1090.620389	17.076992
31.809829	1099.915480	17.082010
31.557021	1095.656792	17.087027
32.013777	1084.695230	17.092045
31.879159	1096.701906	17.097063
32.026895	1088.196308	17.102080
32.461402	1090.101121	17.107098
32.373066	1097.606779	17.112115
32.327302	1083.876954	17.117133
31.908225	1065.032965	17.122151
31.881144	1081.267391	17.127168
32.162242	1071.081103	17.132186
31.903169	1081.488240	17.137203
32.064857	1091.460646	17.142221
32.476317	1096.496415	17.147239
32.167695	1099.129151	17.152256
32.478284	1089.383225	17.157274
32.221995	1080.754344	17.162291
32.543399	1078.448039	17.167309
32.278396	1077.201855	17.172327
31.790384	1080.806093	17.177344
32.415835	1085.136363	17.182362
32.114249	1083.100621	17.187379
32.557303	1085.010415	17.192397
32.452044	1088.315222	17.197415
32.889769	1086.350563	17.202432
32.657161	1084.010596	17.207450
32.493558	1086.229435	17.212467
32.337565	1083.915408	17.217485
32.353340	1088.394251	17.222503
32.532234	1084.475446	17.227520
32.561535	1091.612496	17.232538
32.552315	1091.576171	17.237555
32.556825	1084.386739	17.242573
32.004443	1093.823393	17.247591
32.781755	1094.747037	17.252608
33.099938	1095.464458	17.257626
32.915686	1104.995279	17.262643
32.902899	1086.015427	17.267661
32.816283	1101.836268	17.272679
32.956222	1110.634970	17.277696
33.484197	1101.521059	17.282714
32.932285	1101.891117	17.287731
32.828110	1086.141224	17.292749
32.834685	1093.417511	17.297767
33.086033	1103.404367	17.302784
33.479084	1098.881021	17.307802
33.569749	1116.454128	17.312819
33.990178	1096.718856	17.317837
33.528448	1082.589898	17.322855
33.271220	1082.891985	17.327872
33.160040	1081.151642	17.332890
33.241361	1084.282234	17.337907
32.978503	1078.317845	17.342925
33.263197	1089.369306	17.347943
33.089379	1101.117004	17.352960
33.683470	1099.989523	17.357978
33.383265	1103.097470	17.362995
33.883191	1099.639913	17.368013
33.693559	1103.683687	17.373031
33.601826	1106.011259	17.378048
33.575711	1099.580818	17.383066
33.542148	1106.976967	17.388083
34.171781	1105.092879	17.393101
33.870921	1107.156368	17.398119
33.531066	1105.132894	17.403136
34.012865	1104.158595	17.408154
33.977007	1103.747725	17.413171
33.781382	1101.821714	17.418189
33.979747	1101.500608	17.423207
33.726667	1108.893067	17.428224
33.691750	1103.394948	17.433242
33.750692	1099.983960	17.438259
33.948444	1097.681125	17.443277
33.996335	1099.273753	17.448295
33.702203	1101.348818	17.453312
33.981520	1106.487214	17.458330
33.988504	1125.556571	17.463347
34.045065	1126.052798	17.468365
34.299720	1118.101733	17.473383
33.927812	1120.974697	17.478400
34.507981	1128.032305	17.483418
34.182721	1124.176207	17.488435
34.021055	1111.830856	17.493453
34.444149	1121.393354	17.498471
34.084574	1128.884452	17.503488
34.253052	1122.928630	17.508506
34.307227	1134.183265	17.513523
34.380486	1146.173389	17.518541
34.722287	1137.492385	17.523559
34.852455	1144.462275	17.528576
35.260426	1138.746867	17.533594
34.877155	1130.570074	17.538611
34.640079	1129.038675	17.543629
34.630990	1116.555957	17.548647
34.434482	1115.327508	17.553664
34.741286	1124.914426	17.558682
34.966880	1141.955315	17.563699
35.070926	1137.685237	17.568717
34.994875	1130.877555	17.573735
34.598522	1142.880833	17.578752
34.944709	1138.254321	17.583770
34.910892	1147.228415	17.588787
35.075448	1150.828893	17.593805
35.241531	1144.106582	17.598823
34.869910	1146.401998	17.603840
35.427958	1141.919223	17.608858
35.139770	1140.225368	17.613875
35.171155	1148.539222	17.618893
35.653780	1137.157037	17.623911
35.405424	1137.662869	17.628928
35.446422	1134.232578	17.633946
35.097632	1141.737781	17.638963
35.480343	1144.647890	17.643981
35.594162	1134.727450	17.648999
35.135265	1150.192890	17.654016
35.227357	1141.187849	17.659034
35.126670	1145.391352	17.664051
35.142198	1144.167757	17.669069
35.491048	1137.423304	17.674087
35.427928	1140.450164	17.679104
36.201703	1156.168652	17.684122
35.649620	1148.529370	17.689139
35.555053	1140.919844	17.694157
35.926800	1145.027700	17.699175
35.945024	1159.143928	17.704192
35.749675	1156.662451	17.709210
35.764698	1166.279042	17.714227
35.682115	1165.054942	17.719245
36.068954	1159.926638	17.724263
36.001693	1172.516165	17.729280
36.093541	1157.161720	17.734298
35.979741	1163.437461	17.739315
35.921515	1161.376443	17.744333
35.957001	1162.557601	17.749351
36.133946	1165.108434	17.754368
36.221981	1162.510251	17.759386
36.159919	1164.489231	17.764403
35.997058	1160.942352	17.769421
36.132802	1148.639032	17.774439
36.331331	1164.879433	17.779456
36.118858	1167.361510	17.784474
36.308472	1171.933228	17.789491
36.298240	1175.204321	17.794509
36.569851	1173.316009	17.799527
36.423910	1180.603454	17.804544
36.567059	1179.353676	17.809562
36.545527	1179.145700	17.814579
36.378633	1180.885384	17.819597
36.582505	1178.745688	17.824615
36.566054	1183.980649	17.829632
36.653967	1177.349391	17.834650
36.959422	1178.955573	17.839667
36.707467	1176.183107	17.844685
36.657691	1169.406032	17.849703
36.635500	1179.066293	17.854720
36.558386	1180.369124	17.859738
36.914478	1178.811638	17.864755
36.919547	1198.717655	17.869773
37.069031	1193.137149	17.874791
37.042319	1202.861242	17.879808
37.181823	1200.138277	17.884826
37.139802	1209.274625	17.889843
37.122413	1208.901902	17.894861
37.010894	1197.148284	17.899879
37.103084	1214.026977	17.904896
37.164330	1198.958126	17.909914
37.022526	1195.619400	17.914931
36.720773	1203.521246	17.919949
37.247046	1192.274241	17.924967
37.365629	1200.186380	17.929984
37.531162	1199.699972	17.935002
37.778731	1194.599653	17.940019
37.403519	1198.937428	17.945037
37.393469	1194.789242	17.950055
37.276526	1216.326882	17.955072
37.417079	1220.271937	17.960090
37.612456	1220.374170	17.965107
37.624210	1226.696656	17.970125
37.838681	1222.172681	17.975143
37.757711	1222.207487	17.980160
37.780547	1222.825732	17.985178
37.945667	1223.806830	17.990195
37.852684	1224.569339	17.995213
38.104351	1214.482226	18.000231
38.135702	1216.023791	18.005248
38.167275	1224.605892	18.010266
38.476135	1217.908661	18.015283
37.758043	1219.080919	18.020301
37.748544	1217.037555	18.025319
37.801266	1215.596727	18.030336
37.766016	1216.533282	18.035354
38.205062	1230.975365	18.040371
38.025958	1236.611205	18.045389
38.435604	1235.682847	18.050407
38.559395	1240.662461	18.055424
38.646154	1256.863544	18.060442
38.654494	1247.357094	18.065459
38.598703	1239.141887	18.070477
38.410357	1221.795524	18.075495
38.486554	1227.697724	18.080512
38.621341	1233.770684	18.085530
38.650494	1234.151261	18.090547
38.478424	1245.384388	18.095565
38.789216	1241.451324	18.100583
38.856109	1240.525837	18.105600
39.235497	1237.487808	18.110618
39.218703	1234.429411	18.115635
38.975399	1221.402420	18.120653
38.870913	1208.404317	18.125671
38.802834	1206.597292	18.130688
38.686179	1218.153132	18.135706
39.168291	1217.645835	18.140723
38.981652	1229.158929	18.145741
38.915214	1227.064469	18.150759
39.159877	1231.198443	18.155776
38.963698	1232.081161	18.160794
39.356643	1233.137241	18.165811
38.987201	1240.677259	18.170829
39.464048	1235.740046	18.175847
39.189685	1235.025482	18.180864
38.998734	1237.848199	18.185882
39.221235	1238.855078	18.190899
39.257913	1233.165891	18.195917
39.531909	1232.716243	18.200935
39.458640	1233.166415	18.205952
39.304560	1235.563671	18.210970
39.324376	1236.024597	18.215987
39.139423	1249.935846	18.221005
39.693463	1252.424824	18.226023
39.784316	1257.232846	18.231040
39.412948	1260.714816	18.236058
39.745052	1250.498394	18.241075
39.237870	1251.148669	18.246093
39.414334	1253.598604	18.251111
39.487445	1258.620827	18.256128
39.762568	1268.742930	18.261146
40.086437	1278.844825	18.266163
39.926660	1290.498944	18.271181
40.351670	1274.240459	18.276199
40.252209	1282.827211	18.281216
40.349310	1279.413403	18.286234
40.168546	1256.943960	18.291251
40.182983	1266.238804	18.296269
40.038841	1255.386474	18.301287
39.902923	1267.204120	18.306304
40.110399	1271.328114	18.311322
40.081535	1269.325629	18.316339
40.176847	1275.688771	18.321357
40.162132	1275.953103	18.326375
40.372052	1275.620727	18.331392
40.427544	1269.922288	18.336410
40.436578	1272.066935	18.341427
40.448767	1280.513226	18.346445
40.551745	1281.377771	18.351463
40.864919	1291.926307	18.356480
40.778883	1296.746102	18.361498
41.061431	1280.907423	18.366515
40.806900	1279.855254	18.371533
41.031555	1272.710365	18.376551
41.117658	1278.254434	18.381568
40.579674	1276.804586	18.386586
40.957623	1277.717837	18.391603
40.878864	1292.139604	18.396621
41.003657	1294.477669	18.401639
41.484517	1306.104637	18.406656
41.158886	1313.227609	18.411674
41.311247	1298.049814	18.416691
41.306915	1298.710161	18.421709
41.171394	1296.266687	18.426727
41.578630	1295.894122	18.431744
41.292879	1292.300079	18.436762
41.307217	1284.692470	18.441779
41.554167	1292.808726	18.446797
41.801798	1284.603061	18.451815
41.460874	1270.155343	18.456832
41.227227	1274.146047	18.461850
41.284029	1275.235532	18.466867
41.206847	1287.571065	18.471885
41.462347	1291.842222	18.476903
41.426408	1293.514191	18.481920
41.201649	1298.753216	18.486938
41.467923	1280.834240	18.491955
41.410025	1293.933635	18.496973
41.617264	1309.011476	18.501991
41.933172	1310.887442	18.507008
41.771249	1319.562832	18.512026
42.147960	1314.193064	18.517043
41.992848	1319.080424	18.522061
42.058093	1309.053840	18.527079
42.006316	1310.551552	18.532096
41.958280	1308.416347	18.537114
41.925889	1312.823850	18.542131
42.236829	1317.155809	18.547149
42.373426	1313.202514	18.552167
42.349081	1309.854946	18.557184
41.865057	1309.491758	18.562202
42.246141	1318.249862	18.567219
42.582347	1335.750242	18.572237
42.465656	1335.402445	18.577255
42.440180	1330.682271	18.582272
42.331707	1337.411680	18.587290
42.354261	1334.107298	18.592307
42.499027	1331.768503	18.597325
42.365226	1339.776804	18.602343
42.853752	1340.783295	18.607360
42.631721	1342.913433	18.612378
42.766547	1342.075195	18.617395
42.684160	1336.603330	18.622413
42.767404	1344.233856	18.627431
42.724920	1332.702930	18.632448
42.720117	1336.443424	18.637466
42.758605	1333.546817	18.642483
42.662298	1337.961123	18.647501
43.193200	1350.192556	18.652519
43.449375	1355.470328	18.657536
43.123539	1352.949179	18.662554
43.406956	1350.342640	18.667571
43.690233	1347.802395	18.672589
43.575699	1350.404949	18.677607
43.428532	1329.353455	18.682624
43.462079	1328.000810	18.687642
43.580731	1319.752094	18.692659
43.447016	1320.745011	18.697677
43.349977	1325.768499	18.702695
43.664834	1330.607936	18.707712
43.472467	1348.225339	18.712730
43.536140	1344.337039	18.717747
43.371782	1341.632960	18.722765
43.335362	1346.404018	18.727783
43.411171	1346.887786	18.732800
43.412021	1352.789136	18.737818
43.333792	1344.773034	18.742835
43.873815	1356.722184	18.747853
43.991154	1372.476797	18.752871
44.103336	1377.167922	18.757888
44.095184	1368.367723	18.762906
44.020859	1375.628318	18.767923
44.433540	1369.937351	18.772941
44.259710	1376.130994	18.777959
44.648315	1364.510838	18.782976
44.337953	1369.087867	18.787994
44.501293	1363.593514	18.793011
44.532174	1363.727671	18.798029
44.478532	1362.969268	18.803047
44.431484	1349.021687	18.808064
44.318202	1359.810230	18.813082
43.945212	1357.113385	18.818099
44.273806	1362.695465	18.823117
44.280731	1376.753665	18.828135
44.275596	1367.691063	18.833152
44.242315	1368.321206	18.838170
44.048893	1380.138412	18.843187
44.758617	1385.942028	18.848205
44.808979	1393.498800	18.853223
44.792264	1389.427345	18.858240
44.861563	1392.458877	18.863258
45.018920	1393.586362	18.868275
45.278673	1392.782320	18.873293
45.113531	1394.635361	18.878311
45.353824	1393.846972	18.883328
45.155846	1402.376537	18.888346
45.319300	1400.075848	18.893363
45.325999	1388.079635	18.898381
44.936110	1394.594103	18.903399
45.309619	1390.083194	18.908416
45.319976	1391.078930	18.913434
45.093743	1388.141479	18.918451
45.136658	1389.217353	18.923469
45.160888	1398.592793	18.928487
45.555734	1407.841106	18.933504
45.783053	1410.343106	18.938522
45.295507	1403.968619	18.943539
45.532448	1407.103441	18.948557
45.413309	1414.853870	18.953575
45.965055	1401.018148	18.958592
45.550323	1411.471802	18.963610
45.353368	1414.535325	18.968627
45.796287	1411.004533	18.973645
46.163979	1415.567523	18.978663
45.986060	1415.399672	18.983680
46.019898	1415.391357	18.988698
45.879041	1407.151447	18.993715
46.054393	1402.646140	18.998733
45.961457	1408.435877	19.003751
45.960674	1406.274368	19.008768
45.972442	1411.716443	19.013786
46.588594	1430.460907	19.018803
46.491806	1422.580204	19.023821
46.170011	1437.617444	19.028839
46.510270	1439.972475	19.033856
46.567889	1429.596714	19.038874
46.395681	1430.191684	19.043891
46.866308	1426.400954	19.048909
46.541045	1426.357030	19.053927
46.819132	1419.027037	19.058944
46.887096	1421.096255	19.063962
46.644223	1429.632822	19.068979
46.767558	1415.440909	19.073997
46.457077	1426.446389	19.079015
46.727478	1426.366528	19.084032
46.604700	1428.140393	19.089050
46.727296	1423.122584	19.094067
46.787301	1415.242719	19.099085
46.712058	1432.889307	19.104103
47.108536	1446.363042	19.109120
47.456948	1443.102581	19.114138
47.195012	1452.140748	19.119155
47.246746	1446.480707	19.124173
47.277082	1448.347501	19.129191
47.328687	1442.946260	19.134208
47.449383	1453.913028	19.139226
47.436414	1452.823238	19.144243
47.739464	1442.172570	19.149261
47.540641	1448.966581	19.154279
47.713181	1439.185153	19.159296
47.718524	1451.062979	19.164314
47.729861	1442.404877	19.169331
47.882675	1442.362259	19.174349
47.971166	1446.129276	19.179367
47.822440	1443.577383	19.184384
48.257321	1442.881773	19.189402
47.850421	1446.640713	19.194419
48.436448	1439.928647	19.199437
47.973762	1444.314815	19.204455
48.066306	1435.486282	19.209472
48.071905	1429.110745	19.214490
47.951192	1447.061074	19.219507
48.174962	1441.702456	19.224525
48.445308	1448.792652	19.229543
48.004915	1447.283413	19.234560
48.275696	1442.813731	19.239578
48.165964	1446.709442	19.244595
48.176125	1427.577329	19.249613
48.145157	1436.831994	19.254631
48.223792	1449.197029	19.259648
48.748724	1450.955258	19.264666
48.624904	1459.725770	19.269683
48.821001	1451.998271	19.274701
48.338057	1468.682726	19.279719
48.494420	1466.032836	19.284736
48.527011	1465.100055	19.289754
48.259631	1461.509429	19.294771
48.516627	1453.614656	19.299789
48.831316	1465.220263	19.304807
49.072731	1476.733144	19.309824
49.496037	1477.816071	19.314842
49.432036	1469.128660	19.319859
49.367082	1453.795217	19.324877
49.252310	1456.227408	19.329895
48.926103	1448.656971	19.334912
49.338788	1449.391252	19.339930
48.971224	1453.137757	19.344947
49.605860	1465.930637	19.349965
49.658013	1473.329372	19.354983
49.606420	1469.967082	19.360000
49.729109	1470.323633	19.365018
49.649039	1480.520093	19.370035
49.864693	1466.815544	19.375053
49.726661	1465.319187	19.380071
49.584128	1474.960475	19.385088
49.871622	1464.432137	19.390106
49.990828	1468.977024	19.395123
50.020768	1469.070303	19.400141
49.845901	1469.204936	19.405159
49.677083	1465.576872	19.410176
49.726925	1469.902183	19.415194
49.916023	1475.534420	19.420211
49.777370	1465.233379	19.425229
50.023931	1469.019972	19.430247
49.742735	1465.481989	19.435264
50.048980	1484.574565	19.440282
50.205591	1497.890024	19.445299
50.214385	1493.035082	19.450317
50.630200	1492.430802	19.455335
50.073112	1496.856927	19.460352
50.272754	1499.142339	19.465370
50.077218	1498.929893	19.470387
50.361303	1498.854213	19.475405
50.261962	1509.328248	19.480423
50.375020	1518.260726	19.485440
50.662123	1520.699784	19.490458
50.682132	1521.845506	19.495475
50.797554	1517.712423	19.500493
50.713237	1517.163920	19.505511
50.895906	1515.560822	19.510528
50.848866	1512.497620	19.515546
50.758062	1528.556180	19.520563
51.145292	1540.876387	19.525581
51.172136	1545.666051	19.530599
51.420634	1550.070906	19.535616
51.425671	1541.612555	19.540634
51.262983	1548.811239	19.545651
51.548258	1540.586972	19.550669
51.597082	1544.170835	19.555687
51.416399	1547.809367	19.560704
51.518193	1544.426336	19.565722
51.386253	1544.639495	19.570739
51.593619	1534.044695	19.575757
51.788372	1535.210548	19.580775
51.460030	1529.978892	19.585792
51.554402	1538.661822	19.590810
51.696176	1532.489111	19.595827
51.705725	1536.811244	19.600845
51.908430	1533.188439	19.605863
51.569545	1535.147442	19.610880
51.790901	1540.395976	19.615898
52.006288	1554.377677	19.620915
52.249243	1556.618484	19.625933
52.143884	1557.963610	19.630951
52.472644	1558.755145	19.635968
52.161301	1553.082171	19.640986
52.259531	1564.951923	19.646003
52.286910	1559.052638	19.651021
52.535775	1553.964639	19.656039
52.621957	1558.290624	19.661056
52.382698	1550.394177	19.666074
52.485654	1559.224106	19.671091
52.366193	1547.515674	19.676109
52.542824	1550.937627	19.681127
52.394439	1554.965613	19.686144
52.610051	1564.222978	19.691162
52.827457	1588.277875	19.696179
53.518261	1580.252387	19.701197
53.366286	1578.631958	19.706215
52.785562	1566.824914	19.711232
53.183716	1571.840800	19.716250
52.951820	1577.645916	19.721267
52.888001	1572.653932	19.726285
52.883635	1576.375473	19.731303
53.108954	1580.540944	19.736320
53.400558	1573.133044	19.741338
53.093553	1578.877269	19.746355
53.326572	1575.981894	19.751373
53.490917	1567.422987	19.756391
53.707526	1572.337750	19.761408
53.618485	1567.125629	19.766426
53.348296	1581.110368	19.771443
53.725533	1592.475943	19.776461
53.705777	1599.614522	19.781479
53.521143	1606.021369	19.786496
53.915184	1595.324885	19.791514
53.863145	1594.133870	19.796531
53.949198	1591.879922	19.801549
54.029120	1592.482980	19.806567
54.013549	1601.940465	19.811584
53.849303	1584.246007	19.816602
53.888146	1590.476041	19.821619
53.813927	1589.610377	19.826637
54.071129	1607.397885	19.831655
54.117181	1621.014676	19.836672
54.524679	1613.547688	19.841690
54.911406	1627.742616	19.846707
54.853216	1622.393129	19.851725
54.992156	1619.755396	19.856743
54.516574	1614.417249	19.861760
54.894469	1611.218440	19.866778
55.288611	1617.639322	19.871795
54.674360	1610.880537	19.876813
54.775838	1595.735658	19.881831
54.513500	1613.894400	19.886848
54.850123	1610.083469	19.891866
54.618056	1616.226300	19.896883
54.634385	1620.885075	19.901901
54.657131	1622.756225	19.906919
54.707591	1619.220224	19.911936
54.933121	1624.253534	19.916954
55.116483	1627.898520	19.921971
55.296854	1639.023371	19.926989
55.513327	1634.382213	19.932007
55.292014	1650.013070	19.937024
55.225004	1633.871890	19.942042
55.568619	1637.028015	19.947059
55.385692	1641.941884	19.952077
55.473393	1627.629116	19.957095
55.668699	1636.034442	19.962112
55.827915	1635.384901	19.967130
55.378039	1642.760882	19.972147
55.589195	1655.379987	19.977165
56.126412	1652.702330	19.982183
55.888857	1650.580812	19.987200
56.229191	1653.459734	19.992218
56.190537	1651.364054	19.997235
56.052497	1658.852439	20.002253
56.240030	1648.386895	20.007271
56.259453	1648.781619	20.012288
56.221354	1650.706428	20.017306
56.347580	1641.859925	20.022323
56.530952	1651.261214	20.027341
56.520093	1652.149813	20.032359
56.222726	1655.923300	20.037376
56.339604	1652.518966	20.042394
56.590873	1648.831771	20.047411
56.539059	1657.023113	20.052429
56.667815	1641.621478	20.057447
56.530142	1650.940206	20.062464
56.921161	1670.455292	20.067482
57.136330	1666.713753	20.072499
57.116572	1673.855518	20.077517
57.212920	1664.268870	20.082535
56.985136	1668.467037	20.087552
57.011169	1673.812295	20.092570
57.244996	1674.867930	20.097587
57.293612	1671.389011	20.102605
57.597066	1671.502824	20.107623
57.361820	1673.095404	20.112640
57.503320	1680.092142	20.117658
57.433086	1668.044600	20.122675
57.266161	1668.313701	20.127693
57.434960	1667.100922	20.132711
57.099602	1674.812543	20.137728
57.206215	1669.920232	20.142746
57.738783	1677.834402	20.147763
57.605153	1686.761191	20.152781
57.532332	1691.859907	20.157799
57.912248	1691.684098	20.162816
57.605935	1689.617462	20.167834
58.082821	1697.947418	20.172851
57.543358	1696.794416	20.177869
58.331211	1703.775738	20.182887
58.242045	1711.849841	20.187904
58.118942	1717.679090	20.192922
58.222970	1716.889812	20.197939
58.173288	1718.892172	20.202957
58.577955	1721.593827	20.207975
58.149632	1710.435162	20.212992
58.423799	1714.185951	20.218010
58.396154	1715.509522	20.223027
58.293427	1719.066521	20.228045
58.460702	1732.446768	20.233063
58.495545	1740.694085	20.238080
58.726896	1733.024094	20.243098
58.874707	1735.311296	20.248115
58.726264	1741.583165	20.253133
58.839154	1725.634805	20.258151
59.009074	1735.865074	20.263168
58.988680	1731.238679	20.268186
58.802854	1746.646338	20.273203
58.900530	1758.775087	20.278221
59.369901	1749.647882	20.283239
59.584773	1754.629238	20.288256
59.294537	1763.157559	20.293274
59.562924	1766.072948	20.298291
59.508173	1759.400569	20.303309
59.922442	1761.501117	20.308327
59.908879	1769.721269	20.313344
59.808051	1757.078812	20.318362
59.768315	1754.793935	20.323379
59.728412	1761.396060	20.328397
59.972863	1745.272560	20.333415
59.831309	1757.858288	20.338432
59.832462	1751.609563	20.343450
60.130365	1752.358574	20.348467
59.820494	1755.903650	20.353485
59.913860	1751.215356	20.358503
60.156615	1764.350339	20.363520
60.086732	1784.095104	20.368538
60.697688	1775.270899	20.373555
60.402749	1790.850223	20.378573
60.431515	1780.895328	20.383591
60.637441	1787.525462	20.388608
60.584745	1780.376214	20.393626
60.566045	1776.850950	20.398643
60.560032	1778.947506	20.403661
60.928576	1775.021114	20.408679
61.090040	1771.597192	20.413696
60.665037	1774.737307	20.418714
60.849961	1762.230243	20.423731
60.593745	1781.170862	20.428749
60.690568	1782.181560	20.433767
61.239749	1785.318330	20.438784
61.545024	1792.491590	20.443802
61.301138	1785.914921	20.448819
61.080628	1786.460617	20.453837
61.375049	1787.336407	20.458855
61.451067	1791.477834	20.463872
61.626387	1792.836084	20.468890
61.352288	1778.917205	20.473907
61.230484	1790.695129	20.478925
61.543032	1790.592926	20.483943
61.498882	1788.797895	20.488960
62.059085	1798.115344	20.493978
62.180403	1788.190217	20.498995
62.244498	1806.771716	20.504013
62.285967	1804.546774	20.509031
62.343636	1791.728133	20.514048
62.095589	1790.693858	20.519066
62.288765	1796.745296	20.524083
62.079387	1803.241275	20.529101
62.048099	1803.940552	20.534119
62.784105	1801.137247	20.539136
62.064169	1800.473097	20.544154
62.019553	1803.030115	20.549171
62.240344	1806.868131	20.554189
62.182529	1801.619521	20.559207
62.676712	1812.361097	20.564224
62.631020	1829.684730	20.569242
62.778968	1831.915117	20.574259
62.763695	1827.521436	20.579277
63.047593	1828.285254	20.584295
63.023986	1833.502585	20.589312
63.017539	1826.207259	20.594330
63.201717	1824.603899	20.599347
62.881083	1828.927016	20.604365
62.989781	1826.928297	20.609383
63.290738	1830.984217	20.614400
63.092221	1824.949597	20.619418
63.353999	1838.741256	20.624435
63.536952	1847.284309	20.629453
63.202587	1849.353099	20.634471
63.418938	1843.263347	20.639488
63.480477	1850.922717	20.644506
63.736493	1847.809117	20.649523
63.929650	1849.410754	20.654541
63.620674	1847.306644	20.659559
63.608933	1846.109338	20.664576
63.823876	1851.598811	20.669594
64.080289	1847.049214	20.674611
63.906306	1861.423148	20.679629
64.182193	1865.599748	20.684647
64.549058	1862.263753	20.689664
64.536982	1863.875254	20.694682
64.543598	1861.024551	20.699699
64.721569	1860.078583	20.704717
64.388580	1858.536805	20.709735
64.714837	1861.383238	20.714752
64.965866	1858.838475	20.719770
64.874756	1857.965960	20.724787
64.455797	1863.538353	20.729805
64.777523	1861.765247	20.734823
64.814898	1858.751960	20.739840
64.807918	1864.919794	20.744858
65.169819	1858.690607	20.749875
65.133847	1859.349589	20.754893
64.924780	1857.949468	20.759911
64.900430	1850.972510	20.764928
64.785941	1858.163813	20.769946
65.299072	1870.145901	20.774963
65.395049	1881.833171	20.779981
65.300677	1884.492625	20.784999
65.502236	1880.838369	20.790016
65.269718	1877.384246	20.795034
65.557656	1868.149525	20.800051
65.313471	1872.208277	20.805069
65.660990	1883.414558	20.810087
65.795078	1897.977249	20.815104
65.991930	1900.746003	20.820122
65.907371	1904.729415	20.825139
65.665058	1906.540874	20.830157
66.199416	1905.362685	20.835175
66.547901	1900.741932	20.840192
66.415432	1904.556072	20.845210
66.479861	1905.369843	20.850227
66.739908	1901.469784	20.855245
66.317563	1898.840501	20.860263
66.630450	1892.943993	20.865280
66.196395	1899.841073	20.870298
66.652093	1892.868256	20.875315
66.843162	1902.928065	20.880333
66.462284	1900.955067	20.885351
66.785930	1903.044495	20.890368
67.068101	1918.603508	20.895386
67.088799	1919.869072	20.900403
67.085296	1924.644627	20.905421
66.638898	1927.576653	20.910439
66.979077	1923.108672	20.915456
67.013472	1931.614933	20.920474
67.021985	1929.887430	20.925491
66.862021	1922.631746	20.930509
66.868814	1944.652789	20.935527
67.200436	1936.348540	20.940544
67.187198	1947.125017	20.945562
67.561447	1946.135861	20.950579
67.631253	1942.397961	20.955597
67.433858	1944.584297	20.960615
67.946999	1960.621800	20.965632
67.784733	1969.300714	20.970650
68.116107	1972.398842	20.975667
68.384461	1981.604031	20.980685
68.377869	1975.665715	20.985703
68.648135	1966.297990	20.990720
68.291999	1958.874011	20.995738
68.258812	1947.975580	21.000755
68.147411	1943.644176	21.005773
68.028317	1961.537963	21.010791
68.299606	1959.529695	21.015808
68.461667	1971.383466	21.020826
68.426857	1965.657838	21.025843
68.304618	1960.980966	21.030861
68.367755	1975.497961	21.035879
68.680359	1980.435762	21.040896
68.845493	1986.785131	21.045914
69.266443	1983.475409	21.050931
69.211620	1981.858752	21.055949
69.383540	1992.382357	21.060967
69.011982	1988.220841	21.065984
69.045874	1976.567150	21.071002
69.339647	1990.095159	21.076019
69.124428	1989.017890	21.081037
69.286730	1982.860765	21.086055
69.153355	1978.434940	21.091072
69.481077	1990.124071	21.096090
69.490296	1993.613201	21.101107
69.805777	1997.502790	21.106125
69.523357	2008.968180	21.111143
69.855029	2008.269684	21.116160
69.652416	2003.999806	21.121178
69.990220	2004.505921	21.126195
70.208344	1989.538215	21.131213
70.045526	1998.034185	21.136231
70.389648	2009.635565	21.141248
70.279064	2017.135605	21.146266
70.249835	2028.892960	21.151283
70.528182	2023.036503	21.156301
70.608367	2021.203154	21.161319
70.795593	2021.426588	21.166336
70.293239	2028.719375	21.171354
70.373926	2022.675932	21.176371
70.420870	2020.194481	21.181389
70.425012	2015.450579	21.186407
70.644427	2035.529292	21.191424
71.193604	2051.772715	21.196442
71.298810	2048.641533	21.201459
71.111233	2038.455079	21.206477
70.988427	2049.658949	21.211495
71.225747	2050.818209	21.216512
71.401925	2047.057414	21.221530
71.121222	2050.594850	21.226547
71.808220	2040.691969	21.231565
71.210863	2045.790399	21.236583
71.669848	2050.225726	21.241600
71.388496	2059.762704	21.246618
71.801694	2075.601268	21.251635
72.247747	2069.986939	21.256653
72.137063	2067.422721	21.261671
72.452581	2059.490167	21.266688
72.272754	2059.455155	21.271706
72.106049	2062.037531	21.276723
72.636102	2071.214644	21.281741
72.087973	2068.283014	21.286759
72.095829	2063.380724	21.291776
72.311307	2065.682680	21.296794
72.366957	2062.038482	21.301811
72.404988	2058.570604	21.306829
72.083827	2065.841507	21.311847
72.094418	2062.097022	21.316864
72.250134	2076.599685	21.321882
71.943815	2081.766426	21.326899
72.837174	2079.673916	21.331917
72.723987	2085.962508	21.336935
73.256412	2082.490237	21.341952
73.501708	2092.289235	21.346970
73.426902	2090.227535	21.351987
73.356855	2073.518360	21.357005
73.201833	2081.596572	21.362023
73.513889	2081.658554	21.367040
73.619917	2085.224151	21.372058
73.761360	2101.123984	21.377075
73.908472	2095.852850	21.382093
73.872461	2089.319447	21.387111
73.900445	2078.152625	21.392128
74.097575	2076.534603	21.397146
73.752153	2088.281264	21.402163
74.267955	2093.686099	21.407181
74.284108	2089.719825	21.412199
74.393893	2096.248273	21.417216
74.240321	2093.940048	21.422234
74.105428	2093.184797	21.427251
74.719156	2086.174677	21.432269
74.342917	2097.982949	21.437287
74.339472	2101.142697	21.442304
74.629393	2092.674447	21.447322
74.320466	2095.566161	21.452339
74.306501	2089.196591	21.457357
74.246949	2091.260492	21.462375
74.597237	2105.511969	21.467392
74.819582	2109.479203	21.472410
74.302686	2118.469034	21.477427
74.833995	2120.014892	21.482445
74.715928	2123.448122	21.487463
75.474274	2134.641093	21.492480
75.586076	2132.859618	21.497498
75.384332	2140.736837	21.502515
75.571133	2135.620466	21.507533
75.656524	2134.281780	21.512551
75.502239	2129.335285	21.517568
75.544698	2140.743865	21.522586
75.691109	2148.636314	21.527603
75.757059	2140.856194	21.532621
75.704807	2152.478353	21.537639
75.667697	2162.251927	21.542656
75.958056	2164.457027	21.547674
76.018995	2169.049036	21.552691
76.218018	2160.014210	21.557709
76.064154	2158.501324	21.562727
76.184622	2168.038917	21.567744
76.424807	2171.176526	21.572762
76.448757	2173.637711	21.577779
76.779100	2188.236359	21.582797
76.958966	2177.323553	21.587815
76.924828	2183.075982	21.592832
77.101156	2190.998507	21.597850
77.039307	2182.048469	21.602867
77.322472	2184.747022	21.607885
77.250304	2180.614590	21.612903
77.024726	2177.361309	21.617920
77.312295	2179.377488	21.622938
77.201735	2184.254991	21.627955
77.237492	2176.145025	21.632973
76.934857	2185.685383	21.637991
77.170773	2174.060074	21.643008
77.266697	2178.596143	21.648026
77.443137	2202.330025	21.653043
78.015391	2197.260926	21.658061
77.846228	2195.983960	21.663079
77.811505	2195.850612	21.668096
78.256502	2200.928816	21.673114
77.903924	2200.033874	21.678131
78.101200	2193.000185	21.683149
78.207948	2196.199601	21.688167
78.054549	2199.098676	21.693184
78.416137	2196.536653	21.698202
78.189746	2203.243719	21.703219
78.419351	2217.072240	21.708237
78.684920	2222.042678	21.713255
78.827985	2227.865368	21.718272
79.053662	2220.473777	21.723290
78.418495	2229.097050	21.728307
78.585536	2220.745706	21.733325
78.798942	2218.654898	21.738343
78.593541	2226.996652	21.743360
78.508284	2221.032630	21.748378
78.915654	2245.993003	21.753395
78.892145	2240.751547	21.758413
79.182400	2243.171279	21.763431
79.476185	2247.941662	21.768448
79.419029	2250.128291	21.773466
79.431141	2262.583146	21.778483
79.780136	2262.121798	21.783501
79.823775	2264.330607	21.788519
79.914488	2259.409051	21.793536
80.129570	2267.009979	21.798554
79.748783	2272.712260	21.803571
79.883658	2263.273937	21.808589
79.938920	2262.975092	21.813607
80.344198	2270.959841	21.818624
80.200350	2270.146013	21.823642
80.115538	2291.301228	21.828659
80.233565	2285.627445	21.833677
80.102998	2292.673094	21.838695
80.256981	2290.559970	21.843712
80.554989	2296.292282	21.848730
80.558165	2312.936550	21.853747
81.046295	2313.646501	21.858765
80.957257	2308.828661	21.863783
80.981471	2313.113983	21.868800
81.442936	2302.801078	21.873818
81.416041	2311.386494	21.878835
81.440755	2308.043724	21.883853
81.419943	2303.821212	21.888871
81.282236	2301.627262	21.893888
81.357598	2303.461887	21.898906
81.103573	2312.622339	21.903923
81.507740	2316.848505	21.908941
82.162039	2329.228669	21.913959
82.106153	2336.571995	21.918976
82.209624	2329.439242	21.923994
82.216218	2328.557804	21.929011
82.053578	2322.779375	21.934029
82.355032	2323.123892	21.939047
82.045238	2332.002686	21.944064
82.594301	2324.380813	21.949082
82.507872	2328.241526	21.954099
82.443298	2319.392835	21.959117
82.301035	2325.241044	21.964135
82.253329	2341.880637	21.969152
82.598494	2353.579915	21.974170
82.577668	2347.886703	21.979187
83.027034	2355.365980	21.984205
82.851399	2344.789305	21.989223
82.517922	2352.712375	21.994240
83.089770	2350.622552	21.999258
83.217262	2365.789447	22.004275
83.383177	2374.237569	22.009293
83.673697	2370.155929	22.014311
83.774820	2368.363469	22.019328
84.287514	2344.547539	22.024346
83.992846	2340.058369	22.029363
83.943077	2339.655948	22.034381
84.189064	2323.727361	22.039399
83.816194	2333.035722	22.044416
84.120431	2332.735984	22.049434
84.410029	2320.237481	22.054451
84.435468	2324.853993	22.059469
84.407947	2323.785351	22.064487
83.861115	2330.807458	22.069504
84.546805	2340.074095	22.074522
84.328196	2347.666836	22.079539
84.380067	2357.360387	22.084557
84.507776	2348.791032	22.089575
83.992838	2363.433060	22.094592
84.880318	2353.754429	22.099610
84.420307	2374.636780	22.104627
84.447504	2380.013627	22.109645
84.925400	2374.271163	22.114663
84.918047	2376.481613	22.119680
85.236809	2387.973573	22.124698
85.365290	2401.379297	22.129715
85.587300	2390.219945	22.134733
86.018411	2381.840036	22.139751
85.789975	2387.061014	22.144768
86.315859	2385.196108	22.149786
86.030170	2378.136549	22.154803
85.988236	2371.042197	22.159821
86.179882	2368.228882	22.164839
85.809928	2375.333927	22.169856
86.258112	2386.259748	22.174874
86.350471	2387.671988	22.179891
86.282205	2387.060994	22.184909
86.335816	2385.364298	22.189927
86.264445	2397.163172	22.194944
86.191510	2391.563271	22.199962
86.161852	2395.408848	22.204979
86.359156	2405.868782	22.209997
86.490694	2407.603148	22.215015
86.552688	2420.356478	22.220032
86.674564	2415.117583	22.225050
86.583658	2415.314894	22.230067
86.853456	2431.305496	22.235085
87.189810	2431.136465	22.240103
87.007046	2441.652438	22.245120
87.160752	2432.406766	22.250138
87.538109	2432.120891	22.255155
87.598805	2448.327113	22.260173
88.403349	2444.837655	22.265191
87.860938	2435.725610	22.270208
87.707033	2422.301945	22.275226
88.035606	2434.707648	22.280243
87.720150	2445.910200	22.285261
87.826253	2443.997029	22.290279
88.173811	2451.356489	22.295296
88.223961	2454.874052	22.300314
87.929939	2445.230992	22.305331
87.979710	2457.844232	22.310349
88.556830	2468.333435	22.315367
88.583632	2472.362755	22.320384
88.743468	2464.542630	22.325402
88.926424	2466.928602	22.330419
88.948737	2466.253007	22.335437
88.949739	2469.711949	22.340455
89.163727	2472.039439	22.345472
89.080072	2462.647658	22.350490
88.887506	2469.245408	22.355507
89.178213	2475.496501	22.360525
89.760486	2481.033126	22.365543
89.758549	2492.508807	22.370560
89.805719	2484.239124	22.375578
89.683354	2477.008921	22.380595
89.611993	2485.150033	22.385613
89.952467	2480.599812	22.390631
89.951920	2488.228094	22.395648
89.894902	2489.704627	22.400666
90.276915	2483.541527	22.405683
90.185371	2475.602734	22.410701
90.112879	2483.652496	22.415719
90.351385	2488.687188	22.420736
90.045670	2482.113576	22.425754
90.444273	2487.669331	22.430771
90.364496	2502.164821	22.435789
90.648639	2500.167116	22.440807
90.635846	2502.567790	22.445824
90.577588	2509.305601	22.450842
90.844986	2511.078789	22.455859
91.097449	2527.327814	22.460877
91.346802	2526.493783	22.465895
91.446312	2528.788607	22.470912
91.372070	2535.636221	22.475930
91.392863	2532.868417	22.480947
91.220008	2535.745327	22.485965
91.476322	2537.024748	22.490983
91.133808	2536.907759	22.496000
91.366294	2549.066552	22.501018
91.811031	2546.816605	22.506035
91.516830	2560.184108	22.511053
91.799394	2561.348982	22.516071
92.147201	2578.703600	22.521088
92.075433	2571.834736	22.526106
92.229042	2580.322744	22.531123
92.597210	2581.758335	22.536141
92.173420	2575.704881	22.541159
92.515187	2591.883252	22.546176
92.267055	2600.348605	22.551194
92.611175	2602.412837	22.556211
92.930365	2601.315447	22.561229
93.012554	2589.931568	22.566247
92.926492	2598.608390	22.571264
93.084245	2613.136420	22.576282
93.649141	2614.964293	22.581299
93.890867	2613.995736	22.586317
93.581579	2616.051239	22.591335
93.636124	2613.773665	22.596352
93.832556	2614.017766	22.601370
94.284882	2609.642617	22.606387
94.089815	2609.900331	22.611405
94.058957	2605.666688	22.616423
94.170657	2603.683196	22.621440
94.296598	2605.503666	22.626458
94.176646	2597.502965	22.631475
94.301675	2601.147765	22.636493
94.624789	2603.966403	22.641511
94.596756	2601.139914	22.646528
94.336194	2603.241481	22.651546
94.722649	2596.121372	22.656563
94.877967	2622.361836	22.661581
94.754273	2619.278817	22.666599
94.894993	2621.475712	22.671616
94.921485	2620.783680	22.676634
95.176979	2607.248795	22.681651
94.761778	2627.196587	22.686669
95.090890	2619.517310	22.691687
95.395602	2631.560764	22.696704
95.514542	2646.315787	22.701722
95.756930	2650.870201	22.706739
95.781442	2648.149140	22.711757
95.718207	2651.794857	22.716775
96.051693	2646.062166	22.721792
95.626917	2654.794907	22.726810
95.948527	2646.513981	22.731827
95.981475	2649.586103	22.736845
96.030514	2657.465532	22.741863
96.330441	2667.322616	22.746880
96.512961	2677.008623	22.751898
96.378977	2669.486638	22.756915
96.636057	2670.958468	22.761933
96.736883	2663.784965	22.766951
96.682619	2672.579958	22.771968
96.714161	2685.306657	22.776986
97.192326	2689.777032	22.782003
97.008115	2695.256322	22.787021
97.336322	2685.759271	22.792039
97.573618	2688.528164	22.797056
97.547692	2685.335230	22.802074
97.365317	2682.223465	22.807091
97.548600	2689.958921	22.812109
97.646496	2697.840229	22.817127
97.885359	2704.746465	22.822144
97.571822	2726.619512	22.827162
98.054550	2718.976240	22.832179
97.720185	2711.516996	22.837197
97.821070	2721.547123	22.842215
97.863838	2726.574484	22.847232
97.880299	2736.750317	22.852250
98.261274	2732.692385	22.857267
98.216412	2744.919741	22.862285
98.351246	2751.409811	22.867303
98.751075	2759.038993	22.872320
98.861841	2768.123944	22.877338
99.009395	2757.301031	22.882355
98.992480	2772.863169	22.887373
99.507833	2767.970042	22.892391
99.911924	2767.506417	22.897408
99.532134	2775.840859	22.902426
99.533068	2770.671188	22.907443
99.643608	2776.145641	22.912461
99.518020	2776.843857	22.917479
99.819976	2765.334126	22.922496
99.410391	2777.665630	22.927514
100.162653	2773.852864	22.932531
99.951798	2777.449000	22.937549
100.434987	2794.981581	22.942567
100.437254	2794.842471	22.947584
100.083920	2801.578991	22.952602
100.494933	2793.476599	22.957619
100.692259	2795.582645	22.962637
100.535425	2796.762293	22.967655
100.762190	2799.005779	22.972672
100.972464	2820.759514	22.977690
101.150559	2814.716419	22.982707
101.290546	2820.741770	22.987725
101.318178	2819.692916	22.992743
101.602871	2813.207156	22.997760
101.242079	2816.681464	23.002778
101.357725	2809.593966	23.007795
101.304518	2808.788093	23.012813
101.248819	2812.539975	23.017831
101.334008	2815.263136	23.022848
101.479202	2842.947823	23.027866
101.554140	2839.874870	23.032883
101.868268	2830.966966	23.037901
101.706139	2848.937772	23.042919
102.237374	2859.977196	23.047936
101.995929	2867.229698	23.052954
102.220402	2859.948496	23.057971
102.427638	2864.902948	23.062989
102.540212	2887.909159	23.068007
102.807735	2889.038525	23.073024
102.971658	2895.947034	23.078042
102.934089	2888.454131	23.083059
102.867790	2889.029502	23.088077
103.155964	2891.408619	23.093095
103.057252	2889.240085	23.098112
103.243428	2907.450237	23.103130
103.795875	2918.199190	23.108147
103.837618	2906.035543	23.113165
103.697898	2915.535142	23.118183
103.932648	2903.953727	23.123200
103.781109	2916.989987	23.128218
104.041432	2909.428603	23.133235
103.904022	2910.030827	23.138253
103.988715	2926.792373	23.143271
104.226361	2926.739702	23.148288
104.043638	2938.423712	23.153306
104.646507	2921.034570	23.158323
104.497933	2925.144950	23.163341
104.927894	2948.016609	23.168359
105.344181	2942.857967	23.173376
105.279878	2946.065212	23.178394
105.188519	2949.074680	23.183411
105.115329	2949.531194	23.188429
105.588442	2949.179907	23.193447
105.980202	2948.601422	23.198464
105.446587	2954.084692	23.203482
105.320646	2952.273873	23.208499
105.426000	2946.103192	23.213517
105.571408	2960.324128	23.218535
105.828397	2963.926363	23.223552
105.766855	2975.512629	23.228570
106.133417	2968.878354	23.233587
106.352098	2966.562556	23.238605
106.399895	2970.945358	23.243623
106.587915	2963.878092	23.248640
106.307429	2969.656503	23.253658
106.937888	2984.130174	23.258675
107.112365	2982.979546	23.263693
106.890169	2984.437651	23.268711
107.130832	2985.201941	23.273728
107.381050	2980.539403	23.278746
107.126079	2981.901616	23.283763
107.364341	2982.549504	23.288781
106.998979	2985.519580	23.293799
107.482119	2985.223540	23.298816
107.670908	2995.865043	23.303834
107.519735	2994.692525	23.308851
108.059004	3004.667181	23.313869
107.752842	2998.285970	23.318887
108.343811	2996.808540	23.323904
108.275366	3000.174245	23.328922
108.322157	3008.707492	23.333939
108.492064	3010.713681	23.338957
108.582277	3017.936700	23.343975
109.009649	3022.055270	23.348992
108.697613	3035.545835	23.354010
108.761217	3030.126467	23.359027
108.860761	3030.448782	23.364045
108.444016	3023.702890	23.369063
108.988658	3016.094039	23.374080
108.914892	3029.459131	23.379098
108.964795	3042.675578	23.384115
109.380974	3034.755328	23.389133
109.413883	3043.896727	23.394151
109.730993	3045.302432	23.399168
109.989779	3051.738596	23.404186
109.598200	3043.196105	23.409203
109.787966	3050.820245	23.414221
109.735643	3063.850632	23.419239
110.088989	3062.280792	23.424256
110.003833	3063.143154	23.429274
110.014060	3065.688657	23.434291
110.109452	3077.736597	23.439309
110.227989	3089.042409	23.444327
110.034911	3078.231307	23.449344
110.629262	3088.819189	23.454362
111.178188	3103.659136	23.459379
111.248692	3101.549447	23.464397
110.670638	3109.706607	23.469415
111.141213	3105.691452	23.474432
111.348890	3119.407308	23.479450
111.370789	3126.192836	23.484467
111.861902	3133.066276	23.489485
112.235147	3130.625397	23.494503
112.277670	3120.326755	23.499520
112.165115	3126.375746	23.504538
112.098005	3127.282644	23.509555
112.217549	3121.819822	23.514573
111.827558	3130.193889	23.519591
112.538482	3148.852816	23.524608
112.425655	3153.093396	23.529626
112.401733	3164.705487	23.534643
112.588354	3150.824273	23.539661
112.736700	3157.470193	23.544679
112.807990	3157.850564	23.549696
112.907868	3178.678236	23.554714
113.114249	3172.750551	23.559731
113.606677	3167.595772	23.564749
113.625970	3162.486252	23.569767
114.012352	3157.941339	23.574784
113.883887	3154.966280	23.579802
113.888670	3159.204330	23.584819
114.222375	3166.140164	23.589837
114.448966	3166.411140	23.594855
114.632276	3167.496825	23.599872
114.411929	3175.503638	23.604890
114.436562	3173.186465	23.609907
114.758677	3173.366821	23.614925
114.437531	3181.752286	23.619943
114.770400	3178.386627	23.624960
114.917661	3174.374452	23.629978
114.978965	3187.245212	23.634995
115.162482	3177.439035	23.640013
115.127275	3184.675336	23.645031
115.303808	3183.918892	23.650048
115.433421	3200.664232	23.655066
115.304364	3207.852031	23.660083
115.575336	3209.602640	23.665101
115.401883	3210.210485	23.670119
115.519493	3204.129335	23.675136
115.727408	3217.592738	23.680154
115.487244	3228.664119	23.685171
115.678328	3224.253749	23.690189
115.713212	3242.920188	23.695207
116.004772	3254.817770	23.700224
116.682841	3259.029923	23.705242
116.479327	3261.807569	23.710259
116.586897	3254.209857	23.715277
116.784088	3266.242074	23.720295
116.755181	3279.268971	23.725312
116.910391	3280.318007	23.730330
117.043564	3276.901361	23.735347
117.421492	3274.308238	23.740365
117.396488	3291.077735	23.745383
117.092925	3283.531396	23.750400
117.901064	3296.409047	23.755418
117.938803	3300.597814	23.760435
117.928816	3295.672716	23.765453
118.251624	3292.125545	23.770471
118.273004	3304.229346	23.775488
118.426500	3297.375631	23.780506
118.208520	3294.010496	23.785523
118.444261	3294.595666	23.790541
118.722154	3314.161722	23.795559
118.701011	3308.881712	23.800576
119.052747	3304.790331	23.805594
118.853915	3313.595520	23.810611
118.894853	3314.166833	23.815629
119.019293	3311.966661	23.820647
119.445898	3333.277035	23.825664
119.512049	3340.519710	23.830682
119.266618	3342.656881	23.835699
119.514637	3343.707253	23.840717
119.696120	3343.751698	23.845735
119.672693	3351.592215	23.850752
119.880891	3360.435053	23.855770
119.815014	3360.151895	23.860787
120.124830	3347.526442	23.865805
120.340004	3356.317693	23.870823
120.505024	3379.881323	23.875840
120.791517	3380.969893	23.880858
120.802575	3383.565810	23.885875
121.121464	3379.100786	23.890893
121.156610	3375.005025	23.895911
121.167077	3388.404612	23.900928
121.536979	3382.634457	23.905946
121.455390	3403.298116	23.910963
121.811916	3404.180102	23.915981
121.905589	3405.349193	23.920999
121.678651	3406.634480	23.926016
122.085694	3412.122931	23.931034
122.285085	3410.570719	23.936051
122.051222	3402.609488	23.941069
121.960120	3405.088754	23.946087
122.456526	3403.783824	23.951104
122.561625	3419.100280	23.956122
122.633272	3426.900779	23.961139
122.658717	3421.250521	23.966157
122.747342	3424.393011	23.971175
122.489904	3425.941855	23.976192
123.154647	3429.906786	23.981210
122.738812	3449.508406	23.986227
122.868608	3442.159649	23.991245
123.143577	3443.423607	23.996263
123.145227	3464.620396	24.001280
123.464362	3472.073076	24.006298
123.533938	3471.399553	24.011315
124.060367	3465.444037	24.016333
124.445390	3479.482893	24.021351
124.106473	3487.451494	24.026368
124.599541	3485.348562	24.031386
124.263140	3485.716665	24.036403
124.696947	3485.803887	24.041421
125.015339	3482.131119	24.046439
124.625655	3482.782106	24.051456
124.666331	3471.691347	24.056474
124.799244	3484.415454	24.061491
124.777615	3495.929560	24.066509
125.227294	3505.975256	24.071527
125.231728	3505.993612	24.076544
125.441836	3506.109351	24.081562
125.209618	3516.021348	24.086579
125.518591	3526.912730	24.091597
125.697939	3519.048079	24.096615
125.920376	3523.590042	24.101632
126.126731	3533.140240	24.106650
126.087759	3552.822170	24.111667
126.266970	3548.868062	24.116685
126.648874	3561.029528	24.121703
126.884754	3558.149173	24.126720
126.728163	3554.736558	24.131738
126.682898	3562.624753	24.136755
126.869553	3575.435244	24.141773
127.274581	3569.577500	24.146791
127.286529	3571.463160	24.151808
127.801948	3558.250056	24.156826
127.369377	3582.860165	24.161843
127.652401	3576.794167	24.166861
127.829099	3591.771377	24.171879
127.861676	3599.660094	24.176896
128.317008	3596.275292	24.181914
128.126079	3600.162016	24.186931
128.323599	3604.717347	24.191949
128.279664	3601.176715	24.196967
128.024927	3624.897548	24.201984
128.851540	3619.311866	24.207002
128.779395	3622.791887	24.212019
128.716089	3622.707166	24.217037
129.493685	3622.775583	24.222055
129.572398	3631.847024	24.227072
130.163253	3627.737280	24.232090
130.299173	3635.524705	24.237107
130.161874	3617.473703	24.242125
129.861154	3614.894663	24.247143
129.974988	3611.250561	24.252160
130.050051	3624.842264	24.257178
130.040110	3635.006935	24.262195
129.772894	3632.356395	24.267213
129.998967	3633.485950	24.272231
130.089651	3654.116763	24.277248
130.439027	3650.723197	24.282266
130.565670	3648.409017	24.287283
130.693474	3671.360204	24.292301
130.819647	3667.632107	24.297319
130.910100	3673.327741	24.302336
131.090000	3676.986310	24.307354
131.527096	3694.264982	24.312371
131.732227	3697.932252	24.317389
132.038990	3693.588975	24.322407
131.864360	3702.721990	24.327424
132.055934	3708.913199	24.332442
132.007590	3699.003965	24.337459
131.842102	3703.754713	24.342477
132.092714	3718.471178	24.347495
132.282184	3729.725318	24.352512
132.130010	3723.244124	24.357530
132.452192	3734.685917	24.362547
132.473340	3739.555959	24.367565
132.412909	3738.211452	24.372583
132.249843	3760.359011	24.377600
132.620482	3757.647018	24.382618
132.999280	3764.282534	24.387635
132.999281	3774.237423	24.392653
133.498246	3784.553352	24.397671
133.533326	3794.067230	24.402688
133.736235	3793.417124	24.407706
133.773992	3804.634962	24.412723
134.090682	3805.677827	24.417741
134.955197	3799.404440	24.422759
134.550292	3803.296116	24.427776
134.424203	3810.297473	24.432794
134.686696	3816.442960	24.437811
134.701691	3817.154046	24.442829
135.095054	3826.747879	24.447847
134.842753	3837.237616	24.452864
135.252213	3834.740505	24.457882
135.190111	3843.152227	24.462899
135.146107	3841.243341	24.467917
135.657753	3846.311640	24.472935
135.601704	3855.874457	24.477952
135.660266	3853.712883	24.482970
135.889527	3867.514324	24.487987
136.350330	3882.952544	24.493005
136.534463	3874.307398	24.498023
136.373642	3887.680367	24.503040
136.574586	3881.769079	24.508058
136.765394	3883.298673	24.513075
136.815567	3892.141126	24.518093
137.184577	3888.643458	24.523111
136.889302	3896.109910	24.528128
136.756516	3896.184349	24.533146
137.429353	3909.724230	24.538163
137.616774	3913.324864	24.543181
137.900411	3912.905218	24.548199
137.722365	3915.814717	24.553216
137.944232	3915.751877	24.558234
138.069180	3927.530658	24.563251
138.079085	3936.925436	24.568269
138.517591	3945.641173	24.573287
138.595796	3953.384065	24.578304
138.555472	3948.390918	24.583322
138.951578	3953.369923	24.588339
138.748447	3974.580256	24.593357
139.340100	3970.429280	24.598375
139.196627	3973.481751	24.603392
139.456149	3976.600887	24.608410
139.588312	3978.227996	24.613427
139.458869	3990.860743	24.618445
139.868755	3986.889564	24.623463
139.889624	3989.326227	24.628480
139.856545	3989.732334	24.633498
140.343576	3999.570490	24.638515
140.648264	4006.675294	24.643533
140.948135	4004.596071	24.648551
140.803126	4011.786672	24.653568
141.016928	4004.550860	24.658586
141.122629	3999.648590	24.663603
141.379964	4010.996497	24.668621
141.386919	3999.557160	24.673639
141.318082	4006.679087	24.678656
141.421622	4024.919017	24.683674
141.572605	4024.624179	24.688691
141.647101	4036.152070	24.693709
141.991897	4032.765459	24.698727
141.932833	4038.304578	24.703744
142.136748	4041.861638	24.708762
142.222317	4050.064243	24.713779
142.255562	4062.182487	24.718797
142.149788	4055.277319	24.723815
142.138108	4062.500839	24.728832
142.381859	4077.922520	24.733850
142.805934	4081.088649	24.738867
142.811372	4085.301565	24.743885
143.231108	4101.851071	24.748903
143.412359	4104.329061	24.753920
143.313055	4112.285880	24.758938
143.307846	4109.562914	24.763955
143.340637	4120.664939	24.768973
143.741002	4128.480844	24.773991
143.623777	4132.283612	24.779008
143.463975	4138.046761	24.784026
144.310304	4144.489687	24.789043
144.515848	4150.568404	24.794061
144.814028	4165.782837	24.799079
145.201759	4171.069369	24.804096
145.284965	4173.306973	24.809114
145.506214	4164.873695	24.814131
145.327063	4174.042370	24.819149
145.572251	4170.557615	24.824167
145.834681	4165.952842	24.829184
145.931261	4166.894276	24.834202
146.581581	4175.485615	24.839219
146.109062	4183.667855	24.844237
146.503987	4193.605679	24.849255
146.628323	4193.359175	24.854272
146.269946	4190.978406	24.859290
146.460315	4197.040563	24.864307
146.446752	4199.690932	24.869325
146.788723	4214.163167	24.874343
147.009711	4219.942809	24.879360
146.910874	4224.607564	24.884378
147.159090	4224.480651	24.889395
147.364372	4241.354054	24.894413
147.945979	4245.369989	24.899431
147.390659	4248.903261	24.904448
147.513536	4260.130224	24.909466
147.993872	4262.867836	24.914483
147.933415	4273.754061	24.919501
147.868529	4282.807154	24.924519
148.169413	4296.474676	24.929536
147.811341	4298.610556	24.934554
148.412995	4303.813320	24.939571
148.505086	4320.578167	24.944589
148.957438	4332.022167	24.949607
148.973872	4338.625935	24.954624
148.915156	4353.088069	24.959642
149.253899	4360.765321	24.964659
149.431853	4370.490828	24.969677
149.826014	4373.844735	24.974695
150.232991	4373.595257	24.979712
150.245144	4389.403616	24.984730
150.339758	4390.859852	24.989747
150.257810	4402.166138	24.994765
150.384663	4394.965802	24.999783
150.461549	4408.564123	25.004800
150.413161	4418.624748	25.009818
150.996263	4417.744985	25.014835
151.189145	4439.538103	25.019853
151.655411	4446.049781	25.024871
151.629761	4443.358354	25.029888
151.693179	4446.678547	25.034906
152.254263	4432.094153	25.039923
151.997325	4433.422058	25.044941
152.354281	4440.187479	25.049959
152.732937	4463.867612	25.054976
152.635110	4462.443651	25.059994
153.093267	4457.805176	25.065011
152.883735	4458.424990	25.070029
152.871184	4461.188869	25.075047
153.187537	4464.040420	25.080064
152.969119	4465.962039	25.085082
153.072295	4455.429091	25.090099
153.280043	4467.384714	25.095117
153.276793	4471.008833	25.100135
153.434302	4474.150251	25.105152
153.407775	4486.899888	25.110170
154.147954	4486.289209	25.115187
154.030652	4493.014858	25.120205
154.050872	4497.396013	25.125223
154.495479	4507.884951	25.130240
154.824028	4524.206001	25.135258
154.940126	4515.208159	25.140275
154.725291	4523.864922	25.145293
155.167561	4541.812752	25.150311
155.426983	4548.596555	25.155328
155.281307	4557.955906	25.160346
155.559798	4550.772933	25.165363
155.432454	4553.624138	25.170381
155.671097	4564.110456	25.175399
155.746450	4572.867255	25.180416
155.806438	4591.392298	25.185434
156.183188	4597.510794	25.190451
156.468537	4597.573794	25.195469
156.354013	4612.215269	25.200487
156.671273	4621.818217	25.205504
156.867299	4625.572317	25.210522
157.178310	4640.617865	25.215539
157.497295	4645.918396	25.220557
157.643336	4648.689176	25.225575
158.007060	4657.126513	25.230592
157.893191	4659.975637	25.235610
158.136769	4656.105960	25.240627
158.292690	4664.783976	25.245645
158.126434	4677.867985	25.250663
158.150412	4678.798655	25.255680
158.478637	4686.155732	25.260698
158.872940	4691.614996	25.265715
158.981986	4702.285703	25.270733
158.901868	4703.510345	25.275751
158.911108	4703.114465	25.280768
159.058315	4727.083489	25.285786
159.386990	4723.490938	25.290803
159.595698	4730.118572	25.295821
159.844060	4745.132927	25.300839
160.413714	4743.399857	25.305856
160.417141	4752.278416	25.310874
160.415338	4753.222573	25.315891
160.642759	4753.013672	25.320909
160.990050	4767.378204	25.325927
161.142819	4769.958571	25.330944
160.916159	4767.386771	25.335962
161.291384	4762.672751	25.340979
161.496702	4768.385567	25.345997
161.388612	4793.252970	25.351015
161.509019	4789.118364	25.356032
161.819792	4794.388653	25.361050
162.057273	4796.520249	25.366067
162.033571	4811.318190	25.371085
162.135709	4810.784744	25.376103
162.506010	4817.207336	25.381120
162.188445	4820.410153	25.386138
162.423764	4826.866389	25.391155
162.627408	4841.275440	25.396173
162.607941	4847.604060	25.401191
162.782226	4859.344202	25.406208
162.955518	4860.453646	25.411226
163.344771	4864.695367	25.416243
163.991991	4876.825884	25.421261
163.643326	4875.917565	25.426279
164.143458	4872.509772	25.431296
164.415057	4885.980287	25.436314
164.659258	4889.651188	25.441331
164.528861	4895.387904	25.446349
164.483883	4909.958818	25.451367
164.594709	4904.458939	25.456384
164.863144	4900.301261	25.461402
165.197776	4917.754880	25.466419
165.181546	4928.729305	25.471437
165.287946	4935.076237	25.476455
165.615592	4937.840883	25.481472
165.741624	4960.109032	25.486490
165.792090	4952.124943	25.491507
166.280608	4952.494054	25.496525
166.477104	4969.442102	25.501543
166.515053	4976.014344	25.506560
166.555135	4981.954966	25.511578
166.976454	4980.257595	25.516595
167.034706	4984.939121	25.521613
167.180022	5004.360360	25.526631
167.304303	5005.319621	25.531648
167.378668	5009.645122	25.536666
167.617603	5022.356962	25.541683
167.737110	5025.592774	25.546701
167.801741	5022.435831	25.551719
168.304543	5037.666488	25.556736
168.192812	5053.125407	25.561754
168.233992	5057.512902	25.566771
168.554844	5050.989151	25.571789
168.560067	5080.233102	25.576807
168.715349	5075.019802	25.581824
168.792299	5094.922095	25.586842
169.364228	5102.383440	25.591859
169.479281	5106.614249	25.596877
169.498120	5115.257006	25.601895
170.137654	5120.558275	25.606912
170.099115	5135.295661	25.611930
170.520895	5128.844549	25.616947
170.613145	5136.544727	25.621965
170.669332	5148.350790	25.626983
171.042130	5142.112471	25.632000
171.100636	5159.334699	25.637018
171.179217	5148.600007	25.642035
170.891702	5152.634671	25.647053
171.181494	5165.887921	25.652071
171.975360	5178.040001	25.657088
171.719518	5179.260467	25.662106
171.878417	5190.987437	25.667123
172.158620	5195.400882	25.672141
171.979497	5208.742952	25.677159
172.487700	5211.697327	25.682176
172.880276	5221.951732	25.687194
172.885059	5222.131016	25.692212
173.405828	5225.411712	25.697229
173.477578	5226.628527	25.702247
173.340603	5223.906968	25.707264
173.443092	5244.929161	25.712282
173.966997	5239.374339	25.717300
173.710397	5240.822195	25.722317
173.562281	5248.405174	25.727335
173.898636	5254.956310	25.732352
173.921343	5262.067634	25.737370
174.194360	5276.365222	25.742388
174.637745	5291.962028	25.747405
174.568485	5285.360044	25.752423
174.997792	5284.194851	25.757440
175.263390	5294.724743	25.762458
175.352848	5305.020075	25.767476
175.853505	5307.896728	25.772493
175.936835	5299.430737	25.777511
176.297201	5289.842094	25.782528
176.383603	5303.682656	25.787546
176.565562	5315.074682	25.792564
176.630651	5317.637213	25.797581
176.680637	5326.234187	25.802599
176.869444	5317.300385	25.807616
177.137346	5317.025203	25.812634
176.748443	5320.393883	25.817652
177.577467	5330.510956	25.822669
178.010555	5335.058458	25.827687
177.991915	5332.242704	25.832704
178.034178	5332.116286	25.837722
178.136533	5340.364210	25.842740
178.425649	5339.160866	25.847757
178.179690	5353.113185	25.852775
178.324812	5351.335677	25.857792
178.544772	5358.817206	25.862810
178.680715	5371.333839	25.867828
179.041138	5383.888131	25.872845
179.061218	5394.330045	25.877863
179.276779	5398.630500	25.882880
179.423985	5411.940852	25.887898
179.573437	5421.185255	25.892916
180.076044	5422.322377	25.897933
179.902206	5438.984460	25.902951
180.229319	5444.362874	25.907968
180.704552	5451.053443	25.912986
180.530200	5462.324270	25.918004
180.740196	5471.770761	25.923021
180.743851	5479.125032	25.928039
181.296389	5480.945665	25.933056
181.594997	5498.418078	25.938074
181.388252	5517.572710	25.943092
182.004731	5516.012204	25.948109
181.969647	5518.060059	25.953127
182.028300	5531.788323	25.958144
182.471731	5539.415057	25.963162
182.166931	5542.903258	25.968180
182.613737	5543.780768	25.973197
182.796529	5565.927187	25.978215
183.205437	5554.897773	25.983232
183.301038	5561.685367	25.988250
183.384125	5563.339199	25.993268
184.289465	5566.560085	25.998285
184.199165	5577.214995	26.003303
184.409976	5572.419043	26.008320
184.581632	5575.555295	26.013338
185.164651	5582.535317	26.018356
184.671816	5585.595100	26.023373
184.954631	5595.731074	26.028391
185.089883	5602.152662	26.033408
185.191970	5594.472754	26.038426
184.746456	5599.580091	26.043444
185.428686	5609.006793	26.048461
185.811378	5615.124711	26.053479
186.090793	5625.005549	26.058496
185.947475	5634.737561	26.063514
185.965916	5650.170406	26.068532
186.497312	5646.173640	26.073549
186.573334	5667.948549	26.078567
186.525448	5663.940956	26.083584
187.055091	5654.682460	26.088602
186.836219	5669.842925	26.093620
187.211033	5680.599094	26.098637
187.344865	5692.216654	26.103655
187.167828	5690.662882	26.108672
187.910087	5697.706541	26.113690
187.883205	5717.575176	26.118708
187.988426	5714.752704	26.123725
188.288700	5735.760454	26.128743
188.714420	5732.417752	26.133760
188.893028	5743.690619	26.138778
188.681971	5745.355541	26.143796
189.048888	5757.366148	26.148813
189.232417	5763.291006	26.153831
189.201157	5775.016392	26.158848
189.638656	5773.149132	26.163866
189.459652	5792.637489	26.168884
189.545494	5802.905256	26.173901
190.004268	5814.750084	26.178919
189.799222	5828.137678	26.183936
190.360632	5841.573252	26.188954
190.742766	5855.030435	26.193972
190.422770	5868.776868	26.198989
191.229861	5876.675414	26.204007
191.571436	5897.449644	26.209024
192.104865	5884.711859	26.214042
192.161195	5892.610503	26.219060
192.536297	5878.852534	26.224077
192.716758	5883.644686	26.229095
192.808970	5892.727785	26.234112
193.057495	5898.519459	26.239130
192.777347	5912.357576	26.244148
193.096060	5904.631185	26.249165
193.173601	5903.479685	26.254183
193.234669	5931.851399	26.259200
193.564896	5938.321665	26.264218
193.860335	5941.634419	26.269236
193.956297	5944.501580	26.274253
194.202672	5951.600446	26.279271
194.265158	5960.451460	26.284288
194.985453	5963.129880	26.289306
194.905124	5971.804267	26.294324
195.121996	5968.172061	26.299341
195.773262	5955.314869	26.304359
195.708949	5969.179402	26.309376
195.862921	5977.113387	26.314394
195.825459	5980.275952	26.319412
195.817875	5988.074106	26.324429
196.156161	5990.628921	26.329447
196.083733	6000.400597	26.334464
196.715232	6010.397287	26.339482
196.234354	6029.273159	26.344500
197.018637	6040.691818	26.349517
197.200080	6039.678808	26.354535
197.243591	6046.263197	26.359552
197.561624	6063.016572	26.364570
197.470169	6064.631336	26.369588
197.715672	6065.783276	26.374605
197.965877	6091.546817	26.379623
197.895326	6092.214492	26.384640
198.543664	6099.992647	26.389658
198.761882	6112.717946	26.394676
198.712627	6117.858433	26.399693
198.807457	6137.970577	26.404711
199.368040	6141.990214	26.409728
199.430609	6142.119475	26.414746
199.705880	6159.687699	26.419764
199.893424	6167.657576	26.424781
199.816554	6172.189986	26.429799
199.854998	6179.924236	26.434816
200.415037	6193.382382	26.439834
200.449348	6199.327456	26.444852
200.507997	6203.662002	26.449869
200.984821	6210.693525	26.454887
200.872630	6230.459202	26.459904
201.197674	6233.631664	26.464922
201.302732	6250.831893	26.469940
201.310093	6258.690969	26.474957
201.863546	6267.143712	26.479975
201.809202	6275.615327	26.484992
202.361263	6290.065982	26.490010
202.347535	6302.878032	26.495028
202.340622	6316.822278	26.500045
202.287112	6313.999175	26.505063
202.591759	6336.361153	26.510080
203.624134	6346.696516	26.515098
203.745938	6360.573406	26.520116
203.751780	6370.187886	26.525133
204.335082	6368.376785	26.530151
204.023977	6386.118593	26.535168
204.257147	6389.703129	26.540186
204.777384	6397.002598	26.545204
205.033243	6390.725242	26.550221
205.553408	6403.091221	26.555239
205.686666	6415.457468	26.560256
205.846939	6412.515834	26.565274
206.005057	6407.680518	26.570292
206.151726	6420.180418	26.575309
206.750132	6426.470211	26.580327
206.572309	6437.792687	26.585344
206.955792	6435.567594	26.590362
207.418602	6435.359911	26.595380
207.133693	6422.521876	26.600397
207.635840	6432.425297	26.605415
207.626599	6447.174965	26.610432
208.105571	6441.604681	26.615450
208.150518	6446.604326	26.620468
208.160626	6453.891695	26.625485
208.246174	6458.989193	26.630503
208.060266	6478.776086	26.635520
208.365461	6476.739952	26.640538
208.803982	6487.464584	26.645556
208.843112	6498.750163	26.650573
209.250476	6506.322943	26.655591
209.548233	6532.647913	26.660608
209.550414	6530.971464	26.665626
209.874643	6539.867240	26.670644
210.380630	6551.518952	26.675661
210.823081	6547.545310	26.680679
210.553395	6559.235716	26.685696
211.407991	6557.656995	26.690714
211.590682	6555.030677	26.695732
211.252667	6570.516640	26.700749
211.891756	6572.065061	26.705767
211.911064	6577.854759	26.710784
211.900904	6580.751169	26.715802
212.010802	6596.198986	26.720820
211.952933	6605.510992	26.725837
212.184346	6603.429511	26.730855
212.044358	6626.574491	26.735872
212.410406	6641.483702	26.740890
212.657536	6657.178527	26.745908
212.592509	6675.456831	26.750925
213.299988	6669.674125	26.755943
213.270237	6699.983628	26.760960
213.584794	6706.627072	26.765978
213.785577	6712.107607	26.770996
213.894441	6730.055845	26.776013
214.103547	6733.227504	26.781031
214.438777	6746.023416	26.786048
214.944087	6761.195152	26.791066
214.428188	6772.573625	26.796084
215.005177	6784.738454	26.801101
215.548701	6791.305244	26.806119
215.619261	6806.702541	26.811136
215.719657	6814.844107	26.816154
215.928086	6825.791010	26.821172
216.156994	6838.786633	26.826189
216.199303	6839.866085	26.831207
216.357144	6858.280339	26.836224
216.669889	6876.474774	26.841242
217.244374	6884.675146	26.846260
217.319396	6895.428199	26.851277
217.831267	6905.835450	26.856295
217.637051	6911.838432	26.861312
218.114591	6922.232096	26.866330
218.596415	6935.829240	26.871348
218.439019	6946.283889	26.876365
219.118904	6948.233219	26.881383
219.196671	6963.553762	26.886400
219.529348	6962.646586	26.891418
220.145435	6957.408362	26.896436
219.974159	6977.648093	26.901453
220.344641	6973.451963	26.906471
220.322770	6980.940241	26.911488
220.287584	6988.954624	26.916506
220.606712	7000.600990	26.921524
220.627793	7017.609822	26.926541
220.977270	7028.894763	26.931559
220.829825	7042.978243	26.936576
221.201183	7055.004800	26.941594
221.987682	7057.919312	26.946612
221.822610	7077.514198	26.951629
222.281173	7082.664284	26.956647
222.010710	7089.670435	26.961664
222.356873	7096.249122	26.966682
222.739353	7115.777742	26.971700
223.058504	7118.613497	26.976717
223.662202	7132.185500	26.981735
223.540467	7144.269943	26.986752
223.557541	7152.389906	26.991770
223.977122	7162.338148	26.996788
223.725899	7178.571905	27.001805
224.132662	7183.988945	27.006823
224.726066	7194.405765	27.011840
224.796676	7200.080339	27.016858
225.258061	7214.792079	27.021876
225.476629	7223.669913	27.026893
225.488062	7224.457452	27.031911
225.824580	7247.342775	27.036928
225.830300	7250.356778	27.041946
225.896192	7255.628029	27.046964
226.054953	7272.217899	27.051981
226.472593	7282.207547	27.056999
227.108368	7295.623148	27.062016
227.016518	7306.986440	27.067034
227.383352	7323.805982	27.072052
227.327848	7339.504313	27.077069
227.704987	7329.296408	27.082087
228.016430	7350.989316	27.087104
228.113280	7361.101558	27.092122
228.211196	7376.785506	27.097140
228.338584	7387.656969	27.102157
228.956867	7390.708216	27.107175
228.952296	7403.393334	27.112192
229.321053	7410.811501	27.117210
229.621307	7411.879240	27.122228
229.366771	7433.868714	27.127245
229.911649	7433.746110	27.132263
230.145303	7451.618802	27.137280
229.946053	7454.614240	27.142298
230.628343	7470.024189	27.147316
230.564244	7483.867735	27.152333
230.977273	7494.540104	27.157351
231.265899	7511.166796	27.162368
231.406853	7515.665624	27.167386
231.716697	7525.163929	27.172404
231.692439	7543.199982	27.177421
232.184145	7545.873193	27.182439
232.169890	7558.026410	27.187456
232.347957	7577.312697	27.192474
232.672332	7581.502022	27.197492
232.718297	7603.520680	27.202509
233.231006	7603.993425	27.207527
233.598472	7625.778955	27.212544
233.607712	7639.939519	27.217562
234.036803	7648.885805	27.222580
234.005034	7668.678393	27.227597
234.629324	7680.508137	27.232615
235.114518	7688.946915	27.237632
235.027454	7696.079431	27.242650
235.561940	7719.982619	27.247668
235.398248	7723.746012	27.252685
235.965517	7734.508157	27.257703
236.580737	7740.738965	27.262720
236.088825	7742.971841	27.267738
236.432416	7754.744312	27.272756
236.624710	7778.536691	27.277773
237.211524	7792.156010	27.282791
237.615792	7785.930841	27.287808
237.609796	7791.835354	27.292826
237.984570	7808.436275	27.297844
238.241247	7822.864680	27.302861
238.218863	7824.314153	27.307879
238.473032	7837.126606	27.312896
238.825046	7849.822812	27.317914
239.132433	7854.415776	27.322932
238.939886	7867.521941	27.327949
239.405850	7873.359315	27.332967
239.416617	7891.314489	27.337984
239.518645	7911.411674	27.343002
240.394283	7918.078700	27.348020
240.419716	7929.386233	27.353037
240.670610	7942.975881	27.358055
241.059747	7951.833827	27.363072
241.437291	7962.480424	27.368090
241.538941	7970.925376	27.373108
241.810275	7992.852588	27.378125
241.994460	7982.589126	27.383143
242.265194	7991.383443	27.388160
242.479344	8001.433578	27.393178
242.886803	8003.826375	27.398196
242.957820	8020.042274	27.403213
242.949796	8019.945766	27.408231
243.455236	8028.589909	27.413248
243.403058	8047.899908	27.418266
243.857060	8041.733207	27.423284
243.899377	8062.070312	27.428301
244.020934	8073.284043	27.433319
244.255222	8090.781576	27.438336
244.234586	8115.693545	27.443354
244.891256	8112.690144	27.448372
245.123974	8138.677118	27.453389
245.645741	8133.510076	27.458407
245.781967	8139.784025	27.463424
245.971678	8155.495386	27.468442
246.219401	8155.756843	27.473460
246.514115	8174.804606	27.478477
246.656494	8174.552087	27.483495
246.896717	8185.747412	27.488512
246.754175	8196.194142	27.493530
247.040492	8207.644336	27.498548
247.300260	8225.545284	27.503565
247.526613	8233.882547	27.508583
248.020305	8246.146558	27.513600
247.912139	8262.520004	27.518618
248.311069	8281.138082	27.523636
248.486729	8288.150999	27.528653
248.850721	8312.236195	27.533671
249.267133	8320.717544	27.538688
248.999119	8347.786705	27.543706
249.440234	8354.152169	27.548724
249.949931	8368.014385	27.553741
250.025688	8377.966304	27.558759
250.913446	8378.465923	27.563776
250.836373	8395.349242	27.568794
251.587478	8401.246575	27.573812
251.877148	8397.447866	27.578829
252.443037	8413.422899	27.583847
252.463496	8423.553933	27.588864
252.357678	8428.164016	27.593882
252.633926	8437.513329	27.598900
252.726007	8442.424096	27.603917
253.083515	8459.167203	27.608935
253.505991	8453.611428	27.613952
253.825047	8463.588657	27.618970
253.934312	8484.850292	27.623988
254.264925	8475.993905	27.629005
254.118995	8498.340271	27.634023
254.387326	8498.705865	27.639040
254.630747	8520.218161	27.644058
255.124264	8526.878605	27.649076
255.484682	8545.941779	27.654093
255.299680	8556.979380	27.659111
255.727983	8556.900180	27.664128
255.733218	8584.425962	27.669146
256.155324	8587.754208	27.674164
256.478884	8601.572967	27.679181
256.588249	8622.850530	27.684199
256.801310	8638.748093	27.689216
257.268018	8650.246247	27.694234
257.712660	8654.091915	27.699252
258.158214	8668.100099	27.704269
257.995499	8679.926732	27.709287
258.206205	8700.752930	27.714304
258.388986	8707.452346	27.719322
258.814903	8724.355527	27.724340
258.775520	8737.757329	27.729357
258.805850	8746.977758	27.734375
259.836631	8758.546017	27.739392
259.644409	8771.605415	27.744410
259.744851	8788.262559	27.749428
260.262811	8803.629757	27.754445
260.475346	8823.584446	27.759463
260.883984	8829.475251	27.764480
260.957046	8848.678189	27.769498
260.942920	8858.644361	27.774516
261.336105	8878.106887	27.779533
261.445897	8890.620524	27.784551
262.087324	8906.448469	27.789568
262.077946	8921.256968	27.794586
262.577291	8934.489798	27.799604
262.627746	8941.342500	27.804621
263.034723	8959.123370	27.809639
263.448808	8964.830257	27.814656
263.605594	8983.938214	27.819674
263.863802	8997.088659	27.824692
264.130217	8998.531148	27.829709
263.999727	9022.725828	27.834727
264.446595	9034.350440	27.839744
264.963463	9050.643059	27.844762
265.241712	9060.522777	27.849780
265.667261	9071.130972	27.854797
265.347435	9089.855453	27.859815
265.813676	9102.758898	27.864832
266.285186	9118.607165	27.869850
266.615377	9135.891857	27.874868
266.755113	9146.089960	27.879885
266.977019	9157.377127	27.884903
267.303890	9162.469377	27.889920
267.417319	9180.769738	27.894938
267.697621	9186.336505	27.899956
268.384262	9200.809551	27.904973
268.999150	9217.330160	27.909991
269.326958	9212.638180	27.915008
269.483955	9222.347432	27.920026
269.530857	9235.881391	27.925044
270.101266	9239.925448	27.930061
270.026889	9248.193174	27.935079
270.459609	9257.537485	27.940096
270.781798	9270.507675	27.945114
270.250492	9277.517375	27.950132
271.187369	9284.835224	27.955149
271.223419	9297.600563	27.960167
271.684001	9308.796992	27.965184
272.115612	9325.074712	27.970202
272.110990	9341.284603	27.975220
272.515977	9349.389341	27.980237
272.365561	9363.560296	27.985255
273.011861	9371.431729	27.990272
273.212680	9386.810901	27.995290
273.437644	9407.834579	28.000308
273.664685	9414.217954	28.005325
273.743619	9437.739656	28.010343
274.185781	9442.769833	28.015360
274.505401	9467.311769	28.020378
274.453815	9479.216327	28.025396
275.442964	9489.253962	28.030413
275.459239	9517.388756	28.035431
275.798407	9523.814700	28.040448
275.810922	9516.238663	28.045466
276.139024	9545.865681	28.050484
276.338806	9549.203458	28.055501
276.576046	9569.224564	28.060519
276.887202	9583.522732	28.065536
277.390594	9597.942531	28.070554
277.858680	9607.429904	28.075572
278.367186	9618.903213	28.080589
278.083609	9625.227238	28.085607
278.374855	9645.322106	28.090624
278.860491	9650.317157	28.095642
279.323823	9658.832863	28.100660
279.513322	9659.627513	28.105677
279.722526	9674.090015	28.110695
280.067597	9694.192343	28.115712
280.184830	9697.195700	28.120730
280.267752	9713.389128	28.125748
280.992852	9721.021120	28.130765
280.659265	9734.684139	28.135783
281.268312	9756.333543	28.140800
281.379551	9752.492879	28.145818
281.386720	9761.600600	28.150836
281.765930	9778.066841	28.155853
281.874133	9793.782813	28.160871
282.127021	9804.781397	28.165888
282.845899	9827.651439	28.170906
282.901117	9845.320589	28.175924
283.148205	9857.434629	28.180941
283.562379	9881.671923	28.185959
283.596453	9895.400955	28.190976
284.219782	9901.132388	28.195994
284.205080	9918.026326	28.201012
284.430081	9926.162497	28.206029
284.909237	9943.506841	28.211047
285.447923	9955.442941	28.216064
285.609164	9969.319567	28.221082
285.967834	9986.644822	28.226100
286.430682	9988.028392	28.231117
286.816964	10001.929996	28.236135
286.987085	10025.656100	28.241152
287.341594	10028.622570	28.246170
287.334861	10052.265735	28.251188
287.963484	10052.357416	28.256205
288.190074	10066.527044	28.261223
287.862118	10086.027336	28.266240
288.576885	10097.686686	28.271258
288.649432	10120.297778	28.276276
289.254689	10123.468340	28.281293
288.962229	10148.381157	28.286311
289.229388	10157.824318	28.291328
289.607803	10181.906546	28.296346
289.974392	10202.031333	28.301364
290.221324	10214.903394	28.306381
290.897343	10224.456590	28.311399
291.032627	10237.601794	28.316416
291.419275	10256.997327	28.321434
291.582752	10273.901736	28.326452
291.943248	10283.317801	28.331469
291.872983	10311.811421	28.336487
292.369629	10329.102885	28.341504
293.189061	10335.015468	28.346522
293.591735	10355.330560	28.351540
294.253238	10358.621859	28.356557
294.320951	10370.360016	28.361575
294.347388	10365.547327	28.366592
294.964355	10383.217939	28.371610
294.992303	10400.642429	28.376628
295.355175	10404.463308	28.381645
296.024576	10425.362113	28.386663
295.958548	10426.329189	28.391680
295.924049	10434.657538	28.396698
296.315675	10452.464334	28.401716
296.641142	10459.824167	28.406733
296.735704	10471.160376	28.411751
297.306046	10493.482877	28.416768
297.753929	10495.314010	28.421786
297.891623	10499.798288	28.426804
298.707455	10503.112947	28.431821
298.547745	10509.291690	28.436839
298.968916	10528.593725	28.441856
299.252828	10539.234285	28.446874
299.222069	10540.937866	28.451892
299.054913	10556.656305	28.456909
299.663099	10568.588295	28.461927
299.841285	10601.467208	28.466944
300.057118	10608.926262	28.471962
300.239686	10635.824409	28.476980
300.531581	10642.277046	28.481997
301.024093	10658.890616	28.487015
300.825556	10680.218472	28.492032
301.226961	10694.111925	28.497050
301.548278	10711.929915	28.502068
301.829633	10733.044193	28.507085
302.101142	10761.649478	28.512103
302.285256	10772.618295	28.517120
303.022041	10800.071357	28.522138
302.868115	10824.426740	28.527156
303.103939	10844.566265	28.532173
303.746765	10867.512578	28.537191
303.878332	10875.269028	28.542208
304.600793	10894.994997	28.547226
304.677978	10925.253722	28.552244
305.557264	10939.353974	28.557261
306.037591	10949.970505	28.562279
305.910583	10967.362814	28.567296
306.560014	10980.330615	28.572314
306.753452	10995.134449	28.577332
307.061812	10994.148779	28.582349
307.345094	11012.923381	28.587367
307.753405	11034.652889	28.592384
308.513092	11040.533954	28.597402
308.378710	11053.835386	28.602420
308.779618	11072.607523	28.607437
308.861340	11089.515927	28.612455
308.704923	11102.148277	28.617472
309.427866	11121.590237	28.622490
309.814500	11129.957529	28.627508
309.547183	11162.319491	28.632525
310.167838	11167.363399	28.637543
310.193905	11197.115848	28.642560
310.995533	11209.251791	28.647578
310.949304	11221.128208	28.652596
311.842473	11249.905846	28.657613
312.050682	11258.938794	28.662631
312.367136	11278.172654	28.667648
313.008982	11290.513505	28.672666
313.007565	11304.596427	28.677684
313.251963	11320.886098	28.682701
313.493871	11331.880980	28.687719
313.700488	11350.096341	28.692736
314.298684	11370.543135	28.697754
314.571269	11391.040643	28.702772
314.658590	11396.328681	28.707789
315.158706	11402.518665	28.712807
315.376923	11434.142420	28.717824
315.355738	11445.377254	28.722842
315.840122	11470.833974	28.727860
315.915400	11490.576077	28.732877
316.802066	11504.577725	28.737895
316.635286	11534.499665	28.742912
317.217915	11538.577063	28.747930
317.565103	11560.578778	28.752948
317.776321	11573.668895	28.757965
318.170230	11597.062186	28.762983
318.273211	11622.622697	28.768000
319.083724	11623.478632	28.773018
319.390271	11645.638338	28.778036
319.677296	11664.030942	28.783053
320.216960	11673.568224	28.788071
320.151212	11688.728717	28.793088
320.689744	11700.103912	28.798106
321.070270	11722.233245	28.803124
320.712232	11741.632584	28.808141
321.515722	11743.285335	28.813159
321.851960	11768.149790	28.818176
322.257279	11771.096001	28.823194
322.632802	11793.390394	28.828212
322.776509	11797.870890	28.833229
323.192547	11816.202510	28.838247
323.914523	11818.849978	28.843264
324.372588	11801.512917	28.848282
324.341087	11822.888693	28.853300
325.040797	11827.904688	28.858317
325.348194	11820.553363	28.863335
325.237867	11842.879247	28.868352
325.518480	11839.861188	28.873370
326.018278	11855.735806	28.878388
326.193131	11877.780512	28.883405
326.294900	11880.300354	28.888423
326.500090	11896.902921	28.893440
327.104092	11906.247164	28.898458
327.120334	11929.327066	28.903476
327.319878	11944.806435	28.908493
327.968158	11958.510829	28.913511
327.804869	11987.425659	28.918528
328.226975	11992.573331	28.923546
328.656410	12025.879805	28.928564
328.942993	12043.470806	28.933581
330.015747	12052.991600	28.938599
329.977722	12074.356047	28.943616
329.809622	12095.121867	28.948634
330.253775	12113.342039	28.953652
330.413745	12136.260882	28.958669
330.817673	12148.661446	28.963687
331.022458	12175.930952	28.968704
331.839142	12192.170178	28.973722
331.905448	12214.671095	28.978740
332.006523	12242.774685	28.983757
332.397451	12260.415956	28.988775
332.924157	12282.027435	28.993792
333.404967	12305.303877	28.998810
334.195847	12317.508530	29.003828
333.768968	12342.239934	29.008845
334.578864	12354.097460	29.013863
334.526770	12392.036125	29.018880
335.142278	12409.677308	29.023898
335.284336	12425.611261	29.028916
335.594422	12447.597688	29.033933
336.003872	12463.319528	29.038951
336.298242	12484.841102	29.043968
336.829731	12510.181380	29.048986
337.267899	12532.485844	29.054004
337.346675	12552.957956	29.059021
338.008328	12567.172268	29.064039
338.815077	12578.509399	29.069056
338.817972	12597.885004	29.074074
339.237253	12610.444528	29.079092
339.708777	12628.559892	29.084109
339.725401	12636.107608	29.089127
339.987626	12665.197222	29.094144
340.408612	12676.063965	29.099162
340.666195	12692.175940	29.104180
340.988603	12707.519971	29.109197
341.294824	12718.843536	29.114215
341.734173	12749.724581	29.119232
342.106249	12764.647259	29.124250
341.999499	12772.949999	29.129268
342.451095	12800.320927	29.134285
342.983209	12817.381814	29.139303
342.920211	12834.949035	29.144320
343.302740	12857.230969	29.149338
343.984466	12884.010420	29.154356
344.113882	12893.770085	29.159373
344.351788	12912.206295	29.164391
344.563425	12933.940204	29.169408
344.657997	12946.376825	29.174426
345.457887	12975.127430	29.179444
345.709420	13000.139330	29.184461
345.987052	13013.419054	29.189479
346.285329	13051.566596	29.194496
346.748311	13072.674180	29.199514
347.003873	13100.123430	29.204532
347.584126	13121.771748	29.209549
347.984989	13132.881883	29.214567
348.300243	13154.423076	29.219584
348.484332	13177.307851	29.224602
348.989293	13193.899630	29.229620
349.146079	13215.939241	29.234637
349.459330	13236.353485	29.239655
349.736694	13260.029093	29.244672
349.975340	13284.493908	29.249690
350.900996	13299.409773	29.254708
350.985855	13329.781698	29.259725
352.149786	13349.248897	29.264743
352.631713	13352.192908	29.269760
352.878727	13371.704985	29.274778
353.197109	13369.236592	29.279796
353.484979	13399.959127	29.284813
353.936533	13408.200491	29.289831
354.341291	13425.464913	29.294848
354.437862	13430.275243	29.299866
354.938437	13444.963718	29.304884
355.000121	13463.453164	29.309901
355.216522	13484.890123	29.314919
355.921662	13509.033131	29.319936
355.884729	13522.851661	29.324954
356.308734	13544.881634	29.329972
356.077331	13566.527349	29.334989
356.787871	13582.020090	29.340007
357.309021	13612.952971	29.345024
357.270621	13632.487645	29.350042
357.586044	13649.870392	29.355060
358.213070	13680.382686	29.360077
358.339208	13688.368515	29.365095
358.658821	13719.427684	29.370112
359.154603	13748.435237	29.375130
359.809995	13779.180120	29.380148
359.925395	13796.868884	29.385165
360.344669	13818.527273	29.390183
360.904774	13843.940681	29.395200
361.212936	13870.504948	29.400218
361.626368	13880.303014	29.405236
361.789347	13910.104747	29.410253
362.503334	13925.811976	29.415271
362.722548	13944.852118	29.420288
363.133127	13963.360368	29.425306
363.530872	13981.415885	29.430324
363.734378	14007.251354	29.435341
364.304105	14022.861119	29.440359
364.932069	14046.404179	29.445376
365.153530	14066.094639	29.450394
365.390770	14079.709833	29.455412
366.019120	14098.632748	29.460429
366.332708	14114.146671	29.465447
366.799972	14131.499906	29.470464
367.003921	14139.540130	29.475482
367.921683	14156.280075	29.480500
367.966171	14173.411788	29.485517
368.551051	14172.660817	29.490535
368.758584	14187.455495	29.495552
369.399073	14199.466884	29.500570
369.639486	14201.179107	29.505588
369.991591	14212.044829	29.510605
369.860408	14225.073248	29.515623
370.366755	14238.791930	29.520640
371.470906	14234.808408	29.525658
372.279012	14221.873771	29.530676
371.817908	14227.096399	29.535693
372.317250	14241.346722	29.540711
372.322563	14243.686100	29.545728
372.654735	14262.522652	29.550746
373.149268	14272.475671	29.555764
373.264544	14293.427163	29.560781
373.327447	14311.418277	29.565799
374.028054	14328.489039	29.570816
373.837575	14353.685232	29.575834
374.142504	14375.621020	29.580852
374.501673	14394.646142	29.585869
374.910174	14420.143929	29.590887
375.650486	14441.329872	29.595904
375.544550	14470.665904	29.600922
376.276790	14493.653259	29.605940
376.682176	14515.968329	29.610957
376.943759	14537.241541	29.615975
377.614610	14548.326269	29.620992
377.687824	14570.967869	29.626010
378.073550	14585.713009	29.631028
378.740116	14613.299426	29.636045
378.830310	14639.882915	29.641063
379.229619	14663.013891	29.646080
379.457188	14696.432296	29.651098
379.838413	14703.699849	29.656116
380.457465	14733.179224	29.661133
380.868553	14753.958846	29.666151
381.766954	14779.147146	29.671168
381.984090	14792.109094	29.676186
382.327644	14807.918941	29.681204
382.589822	14832.729485	29.686221
382.821221	14854.213029	29.691239
382.995709	14868.533346	29.696256
383.237718	14904.561641	29.701274
383.816486	14922.337222	29.706292
384.151450	14947.837691	29.711309
384.772803	14973.170440	29.716327
385.193218	14997.372307	29.721344
385.485777	15020.959320	29.726362
385.956929	15039.197064	29.731380
386.345419	15066.865329	29.736397
386.753473	15092.026163	29.741415
387.251532	15105.279355	29.746432
387.847448	15141.464599	29.751450
387.960406	15151.865940	29.756468
388.119432	15185.984357	29.761485
388.351999	15205.146852	29.766503
389.052786	15229.681190	29.771520
389.411561	15255.759470	29.776538
389.573116	15279.683018	29.781556
389.899137	15303.817856	29.786573
390.419249	15335.941191	29.791591
390.748289	15358.322824	29.796608
391.015103	15378.383410	29.801626
391.847322	15413.325944	29.806644
392.162594	15431.553591	29.811661
392.179093	15449.426674	29.816679
392.568111	15472.853951	29.821696
393.048125	15507.238793	29.826714
393.572504	15527.205747	29.831732
394.306476	15550.295175	29.836749
394.083592	15572.804041	29.841767
394.482727	15592.708447	29.846784
394.686779	15611.525224	29.851802
395.217492	15634.681138	29.856820
395.615932	15665.832279	29.861837
395.997115	15689.523177	29.866855
396.427079	15717.593345	29.871872
396.757401	15747.924600	29.876890
397.069174	15768.029128	29.881908
397.969702	15783.336181	29.886925
398.368817	15817.645744	29.891943
399.027061	15844.461462	29.896960
399.128748	15866.496932	29.901978
399.649590	15875.154956	29.906996
400.319157	15904.817778	29.912013
400.317416	15925.764013	29.917031
401.141647	15945.713149	29.922048
400.979342	15975.758252	29.927066
401.523958	15996.199451	29.932084
402.018712	16011.430895	29.937101
402.399857	16039.723902	29.942119
402.786060	16060.256156	29.947136
403.134502	16086.709862	29.952154
403.669387	16108.637112	29.957172
403.834001	16134.178319	29.962189
404.376216	16169.290560	29.967207
404.977591	16184.815061	29.972224
405.307013	16204.772016	29.977242
405.464422	16230.377640	29.982260
406.410506	16252.740059	29.987277
406.631350	16270.980049	29.992295
407.237084	16292.365875	29.997312
407.256788	16325.033057	30.002330
407.712572	16341.992141	30.007348
408.399096	16362.001052	30.012365
408.789800	16384.693282	30.017383
409.192101	16403.682111	30.022400
409.392135	16436.564603	30.027418
409.448045	16463.001203	30.032436
410.038554	16488.081778	30.037453
410.371106	16510.363144	30.042471
410.720750	16538.083804	30.047488
411.004077	16568.009922	30.052506
411.498512	16601.917566	30.057524
412.303009	16638.515349	30.062541
412.394778	16656.630513	30.067559
412.720795	16679.355272	30.072576
413.209105	16711.602730	30.077594
413.873197	16736.893266	30.082612
413.989709	16764.849529	30.087629
414.765366	16801.963781	30.092647
415.062702	16826.799863	30.097664
415.496156	16855.689195	30.102682
415.826119	16880.169679	30.107700
416.313274	16895.895729	30.112717
416.674457	16929.259330	30.117735
417.337811	16953.053153	30.122752
417.881391	16983.157335	30.127770
417.735520	17003.227017	30.132788
418.465334	17033.536013	30.137805
418.697362	17054.712398	30.142823
419.573624	17079.348132	30.147840
420.755009	17087.025813	30.152858
420.931726	17092.462606	30.157876
421.791907	17115.869078	30.162893
421.521084	17119.821571	30.167911
422.189713	17139.309769	30.172928
423.236570	17141.493671	30.177946
423.274269	17158.310105	30.182964
423.830719	17168.495049	30.187981
423.897453	17173.506796	30.192999
424.438902	17186.066125	30.198016
424.871559	17200.098473	30.203034
425.192722	17203.229205	30.208052
425.577542	17220.196957	30.213069
425.710730	17232.810399	30.218087
425.945221	17252.075715	30.223104
426.302810	17259.679569	30.228122
426.817341	17280.038385	30.233140
427.091754	17301.284247	30.238157
427.244762	17332.302585	30.243175
427.422546	17353.607768	30.248192
427.432465	17385.078028	30.253210
428.002695	17411.205286	30.258228
428.776048	17438.479097	30.263245
428.820913	17469.669260	30.268263
429.431365	17504.893346	30.273280
430.000570	17524.302657	30.278298
430.576937	17552.093715	30.283316
430.929483	17579.442714	30.288333
431.768799	17616.823426	30.293351
431.866166	17637.471823	30.298368
432.324267	17672.833643	30.303386
432.763628	17700.270372	30.308404
433.397143	17713.810670	30.313421
433.713885	17760.300286	30.318439
434.339606	17774.656760	30.323456
434.466783	17803.374093	30.328474
434.727077	17834.243873	30.333492
435.372010	17863.733518	30.338509
435.588488	17885.848188	30.343527
436.563534	17907.352045	30.348544
437.020219	17933.788282	30.353562
437.445103	17958.713361	30.358580
437.946224	17987.530684	30.363597
438.395284	18009.091271	30.368615
438.750233	18033.161865	30.373632
439.051970	18060.626848	30.378650
439.504583	18088.365297	30.383668
440.039310	18113.172397	30.388685
440.318322	18143.464880	30.393703
440.517133	18182.291994	30.398720
440.938325	18201.336513	30.403738
441.533441	18239.893572	30.408756
442.138972	18257.197443	30.413773
442.763145	18288.630401	30.418791
443.291325	18313.268209	30.423808
443.617216	18336.566665	30.428826
443.814670	18372.760018	30.433844
444.469354	18401.231863	30.438861
444.702289	18424.942894	30.443879
445.456843	18450.967057	30.448896
445.556040	18476.966931	30.453914
445.866295	18503.698394	30.458932
446.490179	18536.591131	30.463949
447.004409	18566.872927	30.468967
447.447150	18591.903439	30.473984
448.148269	18619.212278	30.479002
448.249838	18648.825616	30.484020
449.004373	18673.201213	30.489037
449.088895	18703.278467	30.494055
449.648777	18735.454991	30.499072
450.161733	18751.807135	30.504090
450.470321	18787.030012	30.509108
450.908046	18810.968653	30.514125
451.272957	18848.153948	30.519143
451.951113	18868.934355	30.524160
452.081887	18890.697096	30.529178
452.655014	18915.252862	30.534196
453.412171	18945.345809	30.539213
453.667162	18984.734365	30.544231
453.869209	19003.409462	30.549248
454.780804	19028.399135	30.554266
454.824300	19048.634141	30.559284
455.549620	19073.867671	30.564301
456.006337	19108.474212	30.569319
456.153822	19136.665992	30.574336
456.775350	19159.344506	30.579354
457.233927	19190.236117	30.584372
457.650797	19215.429403	30.589389
458.319533	19251.026656	30.594407
458.384764	19268.282873	30.599424
459.090512	19304.196663	30.604442
459.193877	19335.800847	30.609460
459.843782	19358.942687	30.614477
460.362172	19394.260357	30.619495
460.782815	19414.064282	30.624512
461.273474	19460.290821	30.629530
461.861846	19492.116687	30.634548
462.326994	19509.892094	30.639565
462.369825	19538.530357	30.644583
463.064413	19581.585497	30.649600
463.722073	19618.594016	30.654618
464.276958	19649.496635	30.659636
464.857909	19677.545902	30.664653
465.189711	19705.166477	30.669671
465.344984	19736.434701	30.674688
466.346670	19763.451962	30.679706
466.484818	19795.765393	30.684724
467.105205	19834.504904	30.689741
467.477727	19862.959641	30.694759
468.083637	19886.955557	30.699776
468.867809	19918.846407	30.704794
468.938479	19947.082907	30.709812
469.451412	19973.228860	30.714829
470.113708	20006.579315	30.719847
470.160658	20036.411757	30.724864
470.817739	20067.128543	30.729882
471.245104	20096.029976	30.734900
471.906255	20126.329236	30.739917
472.397097	20158.967440	30.744935
472.736190	20194.314471	30.749952
473.252109	20217.080158	30.754970
473.631414	20250.418223	30.759988
474.203043	20274.457860	30.765005
474.624699	20304.510370	30.770023
475.220273	20344.082417	30.775040
475.920481	20374.066398	30.780058
476.556363	20399.018622	30.785076
477.133878	20413.232927	30.790093
477.993730	20440.595431	30.795111
478.086332	20463.111402	30.800128
478.783709	20487.637173	30.805146
478.892442	20512.172479	30.810164
479.296186	20541.432061	30.815181
480.012174	20568.381190	30.820199
480.151290	20589.569578	30.825216
480.578234	20618.711938	30.830234
480.882315	20645.270393	30.835252
481.672593	20674.697452	30.840269
482.062026	20700.452925	30.845287
482.615010	20735.483319	30.850304
482.793706	20755.288363	30.855322
483.453185	20781.943312	30.860340
483.710206	20809.216952	30.865357
484.010582	20831.195543	30.870375
484.493680	20865.459910	30.875392
485.148982	20897.694651	30.880410
485.179693	20929.161082	30.885428
485.617761	20957.506116	30.890445
486.206510	20992.588265	30.895463
486.880050	21026.924358	30.900480
487.489690	21048.728683	30.905498
487.850775	21089.855127	30.910516
488.431420	21115.448694	30.915533
489.151939	21141.544938	30.920551
489.255235	21167.326615	30.925568
489.773529	21200.429836	30.930586
490.176246	21231.364964	30.935604
490.597140	21268.369237	30.940621
491.049745	21297.875075	30.945639
491.663037	21332.543318	30.950656
492.626703	21370.101441	30.955674
492.670448	21415.997798	30.960692
493.154055	21432.148255	30.965709
493.612991	21466.790218	30.970727
494.312031	21515.958823	30.975744
495.508056	21544.565814	30.980762
495.503307	21573.037539	30.985780
496.276920	21596.276506	30.990797
496.692987	21631.392998	30.995815
497.120087	21659.443785	31.000832
497.544162	21681.119740	31.005850
498.203993	21708.887946	31.010868
498.483172	21743.526788	31.015885
498.996463	21775.974633	31.020903
499.450278	21814.244828	31.025920
500.159991	21842.112872	31.030938
500.690953	21874.798234	31.035956
500.751194	21901.421621	31.040973
501.661856	21932.803215	31.045991
502.168537	21973.131656	31.051008
502.922748	21998.162275	31.056026
503.390572	22030.074220	31.061044
503.625923	22064.960556	31.066061
504.385573	22094.122814	31.071079
504.566860	22139.215933	31.076096
505.311552	22158.447743	31.081114
505.972277	22186.197528	31.086132
506.238296	22222.109305	31.091149
506.895490	22248.141054	31.096167
506.991049	22288.774252	31.101184
507.458754	22311.088612	31.106202
508.094547	22342.431507	31.111220
508.277014	22389.458532	31.116237
509.041964	22421.343810	31.121255
509.438157	22459.839064	31.126272
510.327048	22494.776066	31.131290
510.880195	22528.362637	31.136308
511.109220	22561.993404	31.141325
511.609902	22589.301082	31.146343
512.260155	22621.324596	31.151360
512.940762	22651.144498	31.156378
514.372915	22667.590619	31.161396
514.827815	22687.480983	31.166413
515.561121	22705.350240	31.171431
515.928597	22729.949127	31.176448
516.386816	22749.851675	31.181466
516.973360	22762.966806	31.186484
517.220973	22789.006162	31.191501
517.761567	22809.597336	31.196519
517.792037	22841.989403	31.201536
518.532740	22858.802400	31.206554
518.270872	22882.715914	31.211572
519.134162	22908.293086	31.216589
519.526526	22931.131704	31.221607
519.915930	22965.250018	31.226624
520.023882	22988.183529	31.231642
520.919757	23022.109355	31.236660
521.109458	23058.337838	31.241677
521.809049	23089.254938	31.246695
522.135586	23117.967983	31.251712
523.036811	23141.429027	31.256730
523.625066	23173.665294	31.261748
524.000724	23212.790784	31.266765
524.554653	23235.465584	31.271783
524.789082	23270.322592	31.276800
525.358116	23305.652048	31.281818
525.920977	23343.901909	31.286836
526.004781	23388.994091	31.291853
526.881605	23419.504974	31.296871
527.158427	23463.019113	31.301888
527.855499	23501.804460	31.306906
528.476060	23539.963568	31.311924
528.733780	23589.111248	31.316941
529.398654	23623.086703	31.321959
529.802503	23667.358762	31.326976
530.124427	23710.898017	31.331994
531.046309	23749.484553	31.337012
531.447241	23792.739965	31.342029
532.475060	23834.842579	31.347047
532.974106	23877.324601	31.352064
533.436154	23912.583323	31.357082
534.078380	23941.526456	31.362100
534.505411	23993.460818	31.367117
535.143093	24021.210444	31.372135
535.702872	24067.613973	31.377152
536.245993	24095.473212	31.382170
537.009588	24133.510083	31.387188
537.617313	24166.970865	31.392205
538.464510	24194.909291	31.397223
538.557991	24226.661874	31.402240
539.385009	24260.676369	31.407258
540.107310	24295.174853	31.412276
540.242992	24325.682439	31.417293
540.870511	24359.867185	31.422311
541.480652	24386.806415	31.427328
541.800186	24426.808777	31.432346
542.514829	24456.923105	31.437364
543.209074	24506.409527	31.442381
543.727450	24529.363071	31.447399
544.126706	24561.883785	31.452416
544.374132	24605.089023	31.457434
545.299278	24634.500992	31.462452
545.864823	24670.718131	31.467469
546.099404	24704.256863	31.472487
547.049144	24731.219524	31.477504
547.683327	24763.267951	31.482522
548.177347	24786.307736	31.487540
548.847831	24832.563100	31.492557
549.421214	24853.340873	31.497575
549.649754	24891.039079	31.502592
550.160197	24923.252375	31.507610
551.023661	24953.274770	31.512628
551.543833	24984.684072	31.517645
552.373723	25014.996164	31.522663
552.579024	25039.168147	31.527680
553.062239	25067.341407	31.532698
553.656007	25103.959389	31.537716
553.516437	25139.522479	31.542733
554.278508	25158.887210	31.547751
555.190861	25185.477130	31.552768
555.158056	25219.481762	31.557786
556.013266	25248.696977	31.562804
556.262605	25277.823285	31.567821
556.880248	25313.862849	31.572839
557.323777	25363.346184	31.577856
557.739736	25398.955964	31.582874
558.388375	25428.311033	31.587892
558.596595	25476.238723	31.592909
559.274357	25511.656274	31.597927
559.743516	25561.332017	31.602944
560.176525	25604.219811	31.607962
561.162154	25639.065123	31.612980
561.673405	25685.372523	31.617997
562.680587	25728.354470	31.623015
563.010472	25760.805772	31.628032
563.287319	25796.665425	31.633050
564.295159	25837.277585	31.638068
564.786864	25881.325993	31.643085
565.404274	25911.887395	31.648103
566.288599	25955.628373	31.653120
566.782015	25991.764331	31.658138
567.479174	26028.102470	31.663156
567.530158	26064.288474	31.668173
568.154576	26097.358054	31.673191
568.955368	26136.713797	31.678208
569.447730	26166.612505	31.683226
570.154336	26203.366604	31.688244
570.520821	26241.096426	31.693261
571.406020	26283.567677	31.698279
572.079533	26314.929909	31.703296
572.553018	26356.447897	31.708314
573.355522	26382.342352	31.713332
573.609869	26422.933956	31.718349
574.330508	26456.520024	31.723367
575.127281	26493.247976	31.728384
575.396882	26537.635755	31.733402
576.234444	26571.462933	31.738420
576.700348	26623.878374	31.743437
576.845127	26648.895957	31.748455
577.841387	26679.804031	31.753472
578.501665	26714.531216	31.758490
578.900940	26757.451996	31.763508
579.553947	26791.725400	31.768525
580.238840	26826.752311	31.773543
581.207617	26862.499823	31.778560
581.432672	26897.604762	31.783578
582.303894	26928.260917	31.788596
582.561589	26969.472470	31.793613
582.772104	27005.793328	31.798631
583.362870	27036.385865	31.803648
583.711164	27084.396690	31.808666
584.612777	27132.751266	31.813684
584.719059	27165.321798	31.818701
585.245383	27209.911255	31.823719
586.145820	27240.051397	31.828736
586.527675	27298.125636	31.833754
587.580214	27339.195244	31.838772
588.218677	27392.540172	31.843789
588.398868	27425.428271	31.848807
589.524383	27470.626575	31.853824
590.152500	27504.803937	31.858842
590.539648	27538.159306	31.863860
591.375844	27577.000399	31.868877
591.700867	27625.066690	31.873895
592.242963	27654.871373	31.878912
592.772513	27687.477977	31.883930
593.560687	27721.624468	31.888948
593.865531	27758.608270	31.893965
594.438745	27791.574827	31.898983
594.948621	27826.453742	31.904000
595.237307	27862.100320	31.909018
596.243158	27907.463597	31.914036
596.717475	27941.867892	31.919053
597.203522	27984.329009	31.924071
597.990638	28025.561416	31.929088
598.237356	28069.905548	31.934106
599.084498	28110.503055	31.939124
599.986073	28151.363951	31.944141
600.344973	28189.591583	31.949159
600.726462	28216.729549	31.954176
601.394623	28259.649571	31.959194
602.065621	28299.901965	31.964212
602.661506	28347.605448	31.969229
603.486647	28388.510322	31.974247
604.367875	28434.519915	31.979264
604.681894	28480.415651	31.984282
605.475598	28511.964837	31.989300
606.058218	28552.989964	31.994317
606.384763	28601.709349	31.999335
607.856911	28628.545343	32.004352
607.953831	28672.794012	32.009370
608.427981	28719.171011	32.014388
608.896958	28748.881229	32.019405
609.775712	28791.099592	32.024423
610.540248	28828.285565	32.029440
610.997793	28867.794860	32.034458
612.000102	28909.261029	32.039476
611.976676	28951.942528	32.044493
612.510155	28992.666472	32.049511
613.382367	29037.281937	32.054528
613.717979	29090.621573	32.059546
614.523688	29124.609669	32.064564
615.707995	29176.458434	32.069581
616.196150	29208.372305	32.074599
617.045260	29237.050647	32.079616
617.286844	29282.498038	32.084634
617.769475	29322.680639	32.089652
618.479314	29364.054202	32.094669
618.876564	29405.413301	32.099687
619.698634	29441.668581	32.104704
619.741678	29491.628871	32.109722
620.541080	29538.279461	32.114740
621.375442	29578.698573	32.119757
621.776509	29631.517429	32.124775
622.842485	29671.837459	32.129792
623.114397	29726.326442	32.134810
623.899690	29764.775086	32.139828
624.631816	29800.216951	32.144845
624.793737	29842.915697	32.149863
625.584294	29897.653089	32.154880
626.351087	29949.967036	32.159898
626.730138	29995.167046	32.164916
627.532914	30043.278429	32.169933
628.018163	30092.216853	32.174951
628.982696	30147.022643	32.179968
629.236795	30187.198265	32.184986
630.359298	30235.266646	32.190004
630.749391	30272.551459	32.195021
631.662369	30311.923106	32.200039
632.610085	30347.654734	32.205056
633.257649	30391.258801	32.210074
634.034445	30424.273768	32.215092
634.451572	30451.889561	32.220109
634.960912	30490.850294	32.225127
635.949748	30517.492204	32.230144
636.070691	30540.533396	32.235162
636.526223	30582.265065	32.240180
637.233179	30611.751297	32.245197
637.437747	30668.459381	32.250215
638.193099	30696.579124	32.255232
638.827578	30744.092538	32.260250
639.313057	30784.694760	32.265268
639.942973	30822.044375	32.270285
640.365401	30880.685062	32.275303
641.706924	30922.703026	32.280320
642.109536	30965.018952	32.285338
642.452013	31005.808227	32.290356
643.350459	31045.196181	32.295373
643.857906	31096.137418	32.300391
644.630941	31135.690461	32.305408
645.089409	31192.177134	32.310426
645.985223	31227.848835	32.315444
646.476036	31275.189869	32.320461
647.072206	31331.832489	32.325479
648.007720	31371.322760	32.330496
648.168045	31413.184242	32.335514
648.597991	31463.259756	32.340532
649.747652	31513.855506	32.345549
649.904729	31568.006899	32.350567
650.922896	31619.988837	32.355584
651.329573	31682.092151	32.360602
652.300358	31724.422325	32.365620
653.357919	31770.980889	32.370637
654.199905	31817.244391	32.375655
654.844475	31860.339971	32.380672
655.377212	31909.231054	32.385690
656.249920	31951.968905	32.390708
656.666165	31985.522945	32.395725
657.274166	32033.580784	32.400743
658.006072	32069.936910	32.405760
658.729044	32118.805194	32.410778
659.373985	32165.479451	32.415796
660.314800	32203.497518	32.420813
661.045321	32251.012082	32.425831
661.641100	32286.226572	32.430848
662.035480	32327.079905	32.435866
662.865854	32386.135478	32.440884
663.435287	32416.581322	32.445901
664.334162	32473.970163	32.450919
665.097120	32508.109579	32.455936
665.342594	32554.701492	32.460954
665.542041	32602.204703	32.465972
666.564466	32647.127014	32.470989
667.084348	32702.280636	32.476007
667.644588	32743.203794	32.481024
668.349204	32801.622642	32.486042
668.814477	32852.770732	32.491060
669.638120	32897.041756	32.496077
670.479288	32954.738037	32.501095
670.833184	33007.541239	32.506112
671.750611	33059.207393	32.511130
672.426552	33110.885980	32.516148
673.320620	33152.453397	32.521165
674.111016	33205.138571	32.526183
675.150087	33242.384594	32.531200
675.912487	33285.022236	32.536218
676.410672	33333.865142	32.541236
677.344613	33369.288026	32.546253
677.473588	33415.141340	32.551271
678.533422	33450.146469	32.556288
678.794823	33494.303976	32.561306
679.292520	33530.414614	32.566324
680.112688	33574.434729	32.571341
680.865128	33614.299160	32.576359
681.566150	33650.839874	32.581376
682.278419	33690.628515	32.586394
682.901116	33744.207295	32.591412
683.194553	33766.984963	32.596429
684.118260	33819.081930	32.601447
684.200257	33864.317637	32.606464
684.915112	33908.177824	32.611482
685.567960	33967.745997	32.616500
686.209199	34012.572528	32.621517
686.777875	34074.272078	32.626535
687.547517	34119.249551	32.631552
688.283394	34173.210115	32.636570
689.275595	34225.423876	32.641588
689.829623	34277.187542	32.646605
690.431816	34324.853246	32.651623
691.420777	34379.280733	32.656640
692.209736	34433.277959	32.661658
692.568072	34484.149523	32.666676
693.796763	34536.371499	32.671693
694.410210	34585.363759	32.676711
695.028394	34625.529200	32.681728
695.865768	34676.244463	32.686746
696.177834	34736.234568	32.691764
697.210911	34765.764437	32.696781
697.928318	34830.357737	32.701799
698.567130	34877.336156	32.706816
699.275806	34932.377737	32.711834
699.626614	34988.682787	32.716852
700.789695	35025.931644	32.721869
701.124471	35090.711757	32.726887
702.035469	35143.307149	32.731904
702.795217	35197.260298	32.736922
703.300404	35248.762079	32.741940
704.012303	35300.181225	32.746957
704.926063	35359.295419	32.751975
705.380755	35403.047475	32.756992
706.598767	35462.639382	32.762010
707.426942	35516.197006	32.767028
708.303388	35558.378914	32.772045
708.660255	35596.380237	32.777063
709.884270	35643.149128	32.782080
710.680038	35686.045680	32.787098
710.884793	35735.907226	32.792116
711.764250	35785.828252	32.797133
712.512749	35836.617044	32.802151
713.312977	35889.705750	32.807168
713.947403	35935.909492	32.812186
714.234100	35975.484168	32.817204
715.407075	36036.671749	32.822221
715.824374	36082.327902	32.827239
716.491842	36129.823121	32.832256
717.413175	36177.987099	32.837274
717.744825	36240.931235	32.842292
718.312613	36284.439878	32.847309
719.054285	36340.997501	32.852327
719.782201	36398.259270	32.857344
720.595718	36453.364360	32.862362
721.210883	36516.473836	32.867380
722.423566	36569.980589	32.872397
722.995768	36614.772804	32.877415
723.586334	36667.459800	32.882432
724.688620	36716.115322	32.887450
725.162530	36768.080923	32.892468
725.784175	36816.760912	32.897485
726.513533	36862.610440	32.902503
727.009486	36916.836661	32.907520
727.783041	36956.893813	32.912538
728.460773	37010.118204	32.917556
729.766045	37047.588768	32.922573
730.368254	37092.908466	32.927591
731.051424	37135.490343	32.932608
731.769512	37176.675755	32.937626
732.134126	37231.454374	32.942644
732.962935	37272.173783	32.947661
733.496985	37322.322914	32.952679
734.446203	37374.525842	32.957696
735.146770	37425.679994	32.962714
735.428176	37477.190391	32.967732
736.350557	37537.390592	32.972749
737.168584	37587.268498	32.977767
737.652517	37646.070237	32.982784
738.325988	37697.804685	32.987802
739.247702	37758.296488	32.992820
739.821695	37812.481215	32.997837
740.294256	37869.799330	33.002855
741.244229	37931.716324	33.007872
742.284407	37993.448721	33.012890
742.842525	38052.157819	33.017908
743.851332	38107.565600	33.022925
744.197078	38174.813231	33.027943
745.108446	38234.599752	33.032960
746.047876	38297.056944	33.037978
746.535892	38362.544031	33.042996
747.572899	38412.655361	33.048013
748.036206	38481.226254	33.053031
748.900028	38541.741926	33.058048
749.615656	38603.861753	33.063066
750.459074	38675.162830	33.068084
751.081061	38731.909822	33.073101
752.519791	38794.353971	33.078119
753.006282	38846.189853	33.083136
754.129685	38885.785110	33.088154
754.911997	38942.880802	33.093172
755.506323	39002.200261	33.098189
756.395103	39057.066357	33.103207
757.515416	39106.742641	33.108224
758.058775	39159.873131	33.113242
758.520459	39221.446153	33.118260
759.858421	39279.562912	33.123277
760.398313	39323.335025	33.128295
761.181132	39373.032841	33.133312
761.868232	39415.062126	33.138330
762.887234	39476.890610	33.143348
763.583186	39533.413183	33.148365
764.385266	39578.947322	33.153383
764.646385	39629.713476	33.158400
765.585791	39681.259520	33.163418
766.339242	39749.397188	33.168436
767.426664	39800.604274	33.173453
768.130588	39847.653051	33.178471
768.805252	39906.020204	33.183488
769.920466	39940.293825	33.188506
770.065793	40005.086676	33.193524
770.843774	40047.805015	33.198541
771.664556	40106.636917	33.203559
772.281474	40167.227199	33.208576
773.082986	40232.854552	33.213594
773.925540	40285.068495	33.218612
774.382711	40341.586077	33.223629
775.053994	40401.612022	33.228647
775.680139	40477.246989	33.233664
776.782919	40532.178375	33.238682
777.565801	40579.741360	33.243700
778.210407	40639.500172	33.248717
778.619163	40689.012588	33.253735
779.414807	40744.542534	33.258752
780.299042	40798.857212	33.263770
780.916753	40861.782975	33.268788
781.726086	40922.143027	33.273805
782.832184	40972.224239	33.278823
783.084732	41039.330838	33.283840
784.435093	41084.156673	33.288858
785.182261	41145.273299	33.293876
785.631128	41204.722613	33.298893
786.704955	41269.608690	33.303911
787.198638	41328.273456	33.308928
788.073524	41394.063647	33.313946
788.962894	41453.641125	33.318964
789.990907	41512.337049	33.323981
791.362712	41569.309938	33.328999
792.135115	41618.211296	33.334016
792.731427	41672.939794	33.339034
793.598233	41732.622738	33.344052
794.120540	41789.873906	33.349069
794.970895	41838.263978	33.354087
795.709554	41906.183009	33.359104
796.372705	41955.589124	33.364122
797.278398	42026.379212	33.369140
797.983584	42089.585825	33.374157
799.006772	42151.592023	33.379175
799.463692	42213.888936	33.384192
800.226579	42267.296421	33.389210
801.245713	42337.007298	33.394228
801.651501	42405.865157	33.399245
802.576030	42467.362649	33.404263
803.345961	42536.752439	33.409280
804.198809	42598.697868	33.414298
805.478575	42667.407848	33.419316
806.313016	42737.857129	33.424333
807.331458	42790.992085	33.429351
808.002381	42851.549773	33.434368
808.622646	42912.128162	33.439386
809.484875	42972.959999	33.444404
810.244121	43039.310743	33.449421
811.120666	43095.561425	33.454439
811.942661	43166.488386	33.459456
812.757289	43227.258760	33.464474
813.427833	43288.184555	33.469492
814.519221	43350.031714	33.474509
815.648179	43414.017393	33.479527
816.104729	43479.714498	33.484544
816.905671	43538.704187	33.489562
817.766661	43599.942751	33.494580
818.440656	43666.024018	33.499597
819.514716	43710.215123	33.504615
820.390183	43779.440588	33.509632
821.624750	43836.175063	33.514650
822.466839	43887.183226	33.519668
822.686330	43949.262664	33.524685
824.168349	44003.492216	33.529703
824.604427	44074.545415	33.534720
825.531772	44130.639017	33.539738
826.419889	44190.932528	33.544756
827.041054	44245.543365	33.549773
828.007933	44298.145999	33.554791
829.021743	44362.924033	33.559808
829.829517	44419.954153	33.564826
830.262146	44468.313818	33.569844
830.680819	44525.271945	33.574861
831.854165	44588.248372	33.579879
832.407489	44651.081127	33.584896
833.487291	44707.987410	33.589914
834.351294	44773.656545	33.594932
834.889797	44824.505380	33.599949
835.553576	44869.072610	33.604967
835.989997	44936.921494	33.609984
836.839855	44996.558969	33.615002
837.992083	45039.171829	33.620020
838.246429	45126.886477	33.625037
839.565825	45182.055103	33.630055
840.180477	45258.796265	33.635072
841.123247	45322.829081	33.640090
841.895223	45386.306711	33.645108
842.816715	45460.287109	33.650125
843.444157	45526.925155	33.655143
844.100322	45597.942623	33.660160
845.321862	45658.289414	33.665178
846.363576	45734.851868	33.670196
847.094182	45803.404021	33.675213
848.159147	45864.395665	33.680231
848.857223	45941.353907	33.685248
849.581911	46009.312989	33.690266
850.641054	46081.977226	33.695284
851.552582	46150.641446	33.700301
852.630874	46200.055653	33.705319
853.332084	46291.817101	33.710336
854.280489	46359.312258	33.715354
855.435749	46423.979364	33.720372
855.905555	46489.556750	33.725389
857.032119	46552.387848	33.730407
858.025969	46614.898177	33.735424
858.765525	46678.523682	33.740442
859.967008	46746.973787	33.745460
860.529761	46805.288027	33.750477
861.616876	46873.224933	33.755495
862.182089	46945.089529	33.760512
863.042574	47015.915196	33.765530
864.187133	47081.914335	33.770548
864.937495	47145.874761	33.775565
865.746092	47207.580526	33.780583
866.806733	47280.008006	33.785600
868.026636	47338.341526	33.790618
869.307473	47394.185847	33.795636
870.152169	47454.577148	33.800653
871.025498	47513.958284	33.805671
871.709713	47575.444019	33.810688
872.209180	47633.308434	33.815706
873.190485	47687.150401	33.820724
874.186997	47753.952681	33.825741
875.245814	47808.655899	33.830759
875.703949	47869.766417	33.835776
876.310678	47945.853709	33.840794
877.614211	48003.650842	33.845812
878.351729	48072.366978	33.850829
879.321749	48136.390906	33.855847
880.005932	48201.009907	33.860864
880.552306	48262.145704	33.865882
882.120304	48332.966581	33.870900
882.965663	48400.736937	33.875917
883.655430	48460.655244	33.880935
884.689710	48529.756770	33.885952
885.196915	48594.973824	33.890970
885.809253	48657.757963	33.895988
886.430657	48729.037426	33.901005
887.346309	48791.951863	33.906023
888.183923	48876.977412	33.911040
888.739610	48955.606665	33.916058
889.934726	49028.588191	33.921076
890.805176	49102.499895	33.926093
891.511846	49155.293581	33.931111
892.725573	49220.288563	33.936128
893.070118	49296.104844	33.941146
894.601965	49356.558730	33.946164
895.405624	49427.970172	33.951181
896.329064	49485.273484	33.956199
897.169985	49543.152868	33.961216
898.076998	49617.009930	33.966234
899.169338	49675.362982	33.971252
899.768799	49741.663488	33.976269
900.792859	49807.335002	33.981287
901.776924	49875.708177	33.986304
902.825164	49938.991073	33.991322
903.957312	50002.811524	33.996340
904.479837	50075.287378	34.001357
905.356520	50140.305806	34.006375
906.502880	50212.666005	34.011392
907.122603	50280.148055	34.016410
908.277421	50344.630261	34.021428
909.068978	50410.301731	34.026445
910.345243	50482.718484	34.031463
911.435290	50544.509688	34.036480
912.154799	50614.729456	34.041498
913.456860	50673.817979	34.046516
914.096858	50741.165356	34.051533
914.934402	50814.549896	34.056551
916.057646	50878.715831	34.061568
916.823329	50950.675727	34.066586
917.618775	51008.641809	34.071604
918.364848	51089.773282	34.076621
919.173006	51168.282230	34.081639
920.206396	51243.852178	34.086656
920.538425	51320.759039	34.091674
922.025726	51377.979298	34.096692
922.979156	51463.179883	34.101709
923.691611	51534.283041	34.106727
924.173780	51615.001868	34.111744
925.287706	51692.332402	34.116762
926.799649	51764.336849	34.121780
927.527842	51851.668290	34.126797
928.422716	51926.047163	34.131815
929.519363	51998.471321	34.136832
930.396477	52080.901977	34.141850
931.397142	52155.473924	34.146868
932.275297	52237.556961	34.151885
932.957597	52311.058994	34.156903
934.489846	52390.680583	34.161920
935.094865	52459.841755	34.166938
936.047049	52531.777529	34.171956
936.750519	52608.067675	34.176973
938.014058	52686.555167	34.181991
939.138043	52758.534502	34.187008
939.872998	52838.452578	34.192026
941.136256	52915.396930	34.197044
942.133406	52987.662479	34.202061
943.031708	53063.917461	34.207079
944.026959	53123.680112	34.212096
945.133669	53204.509719	34.217114
945.975423	53271.902636	34.222132
946.950635	53352.873453	34.227149
947.798378	53424.625746	34.232167
948.657101	53493.756816	34.237184
949.300371	53578.431258	34.242202
950.702677	53639.859377	34.247220
951.729172	53714.533534	34.252237
952.592339	53778.248055	34.257255
953.416103	53847.322330	34.262272
954.457641	53922.868065	34.267290
955.447884	53984.177719	34.272308
956.470349	54039.470911	34.277325
957.419482	54106.988731	34.282343
958.311414	54162.194955	34.287360
958.519345	54232.283789	34.292378
959.994499	54287.760223	34.297396
960.615911	54347.071613	34.302413
961.841447	54411.674330	34.307431
962.958936	54487.482167	34.312448
963.415477	54556.520767	34.317466
964.555950	54623.320516	34.322484
965.616111	54698.688656	34.327501
966.369982	54769.769897	34.332519
967.369972	54833.187537	34.337536
968.173708	54910.659269	34.342554
969.486735	54985.103010	34.347572
970.392634	55061.464545	34.352589
971.415443	55129.549700	34.357607
972.272753	55201.723591	34.362624
973.180984	55280.319366	34.367642
974.251276	55356.143667	34.372660
974.922302	55431.454479	34.377677
976.005304	55510.662980	34.382695
977.018784	55592.743012	34.387712
977.842682	55676.371666	34.392730
978.772773	55763.287542	34.397748
979.911681	55846.722206	34.402765
980.937892	55931.737848	34.407783
981.609897	56004.708778	34.412800
983.005508	56095.901109	34.417818
984.178112	56173.003120	34.422836
984.766820	56249.765926	34.427853
985.946572	56337.081711	34.432871
987.152174	56416.963968	34.437888
987.909449	56504.181584	34.442906
988.866216	56582.957643	34.447924
989.989239	56667.353288	34.452941
990.798284	56759.753318	34.457959
991.656568	56839.608781	34.462976
992.521619	56933.007034	34.467994
993.870493	57020.735681	34.473012
995.164194	57097.669940	34.478029
996.345966	57173.343445	34.483047
997.745987	57250.350250	34.488064
998.773259	57324.845800	34.493082
999.667495	57395.172559	34.498100
1000.786610	57475.052831	34.503117
1001.861774	57550.471978	34.508135
1002.925933	57622.133675	34.513152
1003.808832	57700.994532	34.518170
1004.967851	57770.293855	34.523188
1005.835336	57854.220812	34.528205
1007.008610	57919.955110	34.533223
1008.080082	57997.673678	34.538240
1008.700910	58069.646222	34.543258
1009.735999	58139.801339	34.548276
1010.788793	58237.719736	34.553293
1011.560903	58301.479545	34.558311
1012.623214	58375.656443	34.563328
1013.639564	58455.404068	34.568346
1014.351557	58536.724670	34.573364
1015.418808	58613.515489	34.578381
1016.356489	58699.807921	34.583399
1017.572502	58779.025526	34.588416
1018.391337	58858.963460	34.593434
1019.760826	58937.201973	34.598452
1020.631088	59023.449090	34.603469
1021.518283	59099.902381	34.608487
1022.801319	59161.591186	34.613504
1023.472883	59241.338109	34.618522
1024.185566	59307.603599	34.623540
1025.194755	59370.000149	34.628557
1026.251343	59456.637546	34.633575
1027.318791	59537.039044	34.638592
1028.107141	59614.433443	34.643610
1028.979818	59689.055301	34.648628
1030.111750	59770.295686	34.653645
1030.686909	59858.553857	34.658663
1032.088076	59940.651697	34.663680
1033.243409	60027.123847	34.668698
1034.534295	60111.948494	34.673716
1035.410754	60195.825206	34.678733
1036.653630	60280.005959	34.683751
1037.830155	60361.108452	34.688768
1038.848591	60437.817696	34.693786
1039.742644	60524.794349	34.698804
1040.686596	60608.674632	34.703821
1041.780727	60696.038512	34.708839
1042.635236	60768.875181	34.713856
1043.847271	60853.809627	34.718874
1045.043655	60942.557357	34.723892
1046.139397	61026.750926	34.728909
1047.246467	61108.930124	34.733927
1048.335358	61208.139829	34.738944
1049.652979	61289.552591	34.743962
1050.502228	61369.114229	34.748980
1051.932529	61455.985396	34.753997
1052.616466	61528.819223	34.759015
1053.549659	61627.902939	34.764032
1054.785941	61703.594756	34.769050
1056.102192	61791.706556	34.774068
1057.294617	61871.336672	34.779085
1057.857272	61958.129447	34.784103
1058.928004	62049.084612	34.789120
1060.091003	62134.309643	34.794138
1061.412180	62218.231656	34.799156
1062.396170	62295.749667	34.804173
1063.760323	62389.597612	34.809191
1064.695477	62470.257218	34.814208
1065.864483	62543.968070	34.819226
1066.519662	62633.160632	34.824244
1067.858983	62710.542340	34.829261
1068.742823	62807.479847	34.834279
1070.194151	62889.965894	34.839296
1071.311985	62977.979875	34.844314
1072.167547	63061.015012	34.849332
1073.363136	63135.812311	34.854349
1074.344969	63225.937367	34.859367
1075.249184	63310.554697	34.864384
1076.626612	63399.529972	34.869402
1077.161379	63483.331795	34.874420
1078.204548	63563.440052	34.879437
1079.521406	63671.727409	34.884455
1080.219296	63753.827162	34.889472
1081.696509	63836.730140	34.894490
1083.056744	63934.395536	34.899508
1084.105642	64008.699184	34.904525
1084.809048	64107.739949	34.909543
1086.273515	64189.987700	34.914560
1087.168392	64266.316575	34.919578
1087.996704	64352.848458	34.924596
1089.573459	64434.952923	34.929613
1090.491255	64525.225586	34.934631
1091.412044	64617.688551	34.939648
1092.475952	64705.052293	34.944666
1093.391604	64794.484265	34.949684
1094.615823	64871.612047	34.954701
1095.734441	64958.778231	34.959719
1096.473436	65028.429326	34.964736
1097.712845	65108.746228	34.969754
1098.704510	65182.903997	34.974772
1100.438634	65273.286526	34.979789
1101.277644	65349.716026	34.984807
1102.232837	65426.355588	34.989824
1103.033365	65506.685097	34.994842
1104.150545	65596.398770	34.999860
1105.339608	65681.214019	35.004877
1106.285163	65774.589049	35.009895
1107.119864	65860.979513	35.014912
1108.715486	65945.219550	35.019930
1109.403719	66042.124055	35.024948
1110.790518	66126.612458	35.029965
1111.977697	66223.876844	35.034983
1113.134327	66320.779149	35.040000
1114.327175	66411.034748	35.045018
1115.270155	66495.036318	35.050036
1116.885796	66578.066081	35.055053
1118.185474	66673.966126	35.060071
1118.817838	66762.733732	35.065088
1120.063620	66846.505725	35.070106
1121.514353	66945.586930	35.075124
1122.409413	67041.234775	35.080141
1123.688454	67122.596581	35.085159
1124.565210	67208.871124	35.090176
1125.591713	67306.930767	35.095194
1126.852186	67395.374877	35.100212
1127.874393	67484.856754	35.105229
1129.255797	67585.135224	35.110247
1130.217623	67675.019720	35.115264
1131.548531	67770.558136	35.120282
1132.636098	67868.673747	35.125300
1133.978337	67955.771108	35.130317
1134.899296	68056.066112	35.135335
1135.870166	68147.698386	35.140352
1137.204552	68235.500733	35.145370
1138.068740	68342.738865	35.150388
1139.552804	68434.342935	35.155405
1140.758900	68533.265761	35.160423
1141.569282	68633.776517	35.165440
1143.108603	68720.693837	35.170458
1143.979794	68821.721400	35.175476
1145.389521	68916.757935	35.180493
1146.799315	69008.242642	35.185511
1148.047532	69093.534926	35.190528
1149.357264	69175.778607	35.195546
1150.585051	69271.433637	35.200564
1151.756831	69355.712915	35.205581
1152.947176	69438.134315	35.210599
1153.923183	69531.720958	35.215616
1155.206185	69615.046636	35.220634
1156.008673	69707.394524	35.225652
1157.298808	69792.821896	35.230669
1158.761008	69884.162244	35.235687
1159.691532	69975.034781	35.240704
1161.318343	70062.709186	35.245722
1162.257199	70158.013543	35.250740
1163.075976	70236.335109	35.255757
1164.534567	70333.262558	35.260775
1165.600530	70417.777056	35.265792
1167.437989	70494.072838	35.270810
1168.270595	70565.421477	35.275828
1169.815008	70642.155907	35.280845
1170.608853	70727.834576	35.285863
1171.477947	70807.942063	35.290880
1172.874684	70881.635357	35.295898
1173.406627	70957.464484	35.300916
1174.645048	71038.186417	35.305933
1175.867203	71118.771819	35.310951
1176.352791	71190.138187	35.315968
1177.783546	71272.844605	35.320986
1178.618012	71365.079411	35.326004
1179.714371	71449.168247	35.331021
1180.642339	71551.381755	35.336039
1181.617930	71645.229357	35.341056
1182.663387	71735.684858	35.346074
1183.407333	71836.978245	35.351092
1185.012677	71941.760168	35.356109
1185.948617	72050.876875	35.361127
1187.156201	72162.902751	35.366144
1188.684990	72269.040409	35.371162
1189.724147	72381.207418	35.376180
1191.109994	72489.419999	35.381197
1192.261382	72587.030549	35.386215
1193.261414	72685.450280	35.391232
1194.756060	72787.289075	35.396250
1196.237426	72912.700989	35.401268
1197.722127	73015.555460	35.406285
1198.966155	73118.929088	35.411303
1199.861388	73220.140907	35.416320
1201.255027	73315.069298	35.421338
1202.280960	73430.168610	35.426356
1203.671749	73529.974563	35.431373
1205.300251	73630.073204	35.436391
1206.251254	73744.970222	35.441408
1207.436300	73837.387085	35.446426
1208.600473	73949.629937	35.451444
1209.818907	74055.303756	35.456461
1211.271339	74152.366564	35.461479
1212.161410	74264.881399	35.466496
1213.440800	74357.513374	35.471514
1215.014238	74473.709939	35.476532
1216.018215	74583.839782	35.481549
1217.627502	74694.623181	35.486567
1218.589309	74795.349296	35.491584
1219.915718	74888.659782	35.496602
1220.879109	75005.168942	35.501620
1222.341836	75112.354237	35.506637
1223.653295	75220.133507	35.511655
1224.937292	75330.374831	35.516672
1226.418093	75426.424506	35.521690
1227.572986	75528.643332	35.526708
1229.056394	75625.541990	35.531725
1230.475693	75725.073029	35.536743
1231.502163	75827.806990	35.541760
1233.071365	75912.343030	35.546778
1233.974422	76018.884365	35.551796
1235.349245	76105.059982	35.556813
1236.850490	76201.679259	35.561831
1237.946910	76295.790453	35.566848
1239.424058	76392.464831	35.571866
1240.491381	76489.735371	35.576884
1241.402699	76583.268347	35.581901
1243.139123	76679.396700	35.586919
1244.325375	76776.320405	35.591936
1245.839399	76864.300882	35.596954
1246.803350	76949.846432	35.601972
1247.844223	77047.186425	35.606989
1249.372867	77142.981403	35.612007
1250.651229	77239.461726	35.617024
1251.458704	77322.233256	35.622042
1252.806356	77429.445653	35.627060
1254.148997	77509.271547	35.632077
1255.291086	77588.394160	35.637095
1255.758619	77687.687848	35.642112
1256.839649	77784.834207	35.647130
1258.232780	77874.306240	35.652148
1259.293210	77969.657617	35.657165
1260.662025	78066.494155	35.662183
1261.888211	78171.106090	35.667200
1263.363305	78251.179565	35.672218
1263.962668	78360.919026	35.677236
1265.203760	78462.008005	35.682253
1266.519139	78564.263939	35.687271
1267.635079	78678.193459	35.692288
1268.680247	78775.779634	35.697306
1270.412794	78900.812916	35.702324
1271.667863	79008.882018	35.707341
1272.927864	79106.676626	35.712359
1274.016582	79229.087884	35.717376
1275.424801	79344.140170	35.722394
1276.881516	79444.401071	35.727412
1278.517626	79547.750911	35.732429
1279.902661	79661.047177	35.737447
1281.064311	79762.026600	35.742464
1282.934922	79863.301444	35.747482
1284.312125	79959.623911	35.752500
1285.244193	80076.197606	35.757517
1286.839578	80175.083992	35.762535
1288.239969	80286.188688	35.767552
1289.460934	80389.124861	35.772570
1290.822160	80496.841182	35.777588
1292.297312	80596.609283	35.782605
1293.614445	80687.128472	35.787623
1295.109225	80785.982014	35.792640
1296.294841	80881.387300	35.797658
1297.854337	80984.247640	35.802676
1298.903174	81084.729981	35.807693
1300.269570	81186.974984	35.812711
1301.246492	81290.598610	35.817728
1302.854098	81400.167821	35.822746
1304.051241	81498.867499	35.827764
1304.907375	81606.565359	35.832781
1306.293809	81705.401006	35.837799
1307.503379	81825.765049	35.842816
1308.701062	81939.365795	35.847834
1310.243075	82043.829138	35.852852
1311.094955	82159.233032	35.857869
1312.458620	82264.535826	35.862887
1313.939754	82389.256474	35.867904
1315.486935	82492.935139	35.872922
1316.345588	82602.587599	35.877940
1317.822820	82716.236653	35.882957
1319.149717	82831.049880	35.887975
1320.613807	82953.811793	35.892992
1321.876261	83063.276484	35.898010
1323.324686	83175.664838	35.903028
1324.747894	83287.297339	35.908045
1326.060138	83408.272990	35.913063
1327.752692	83514.492196	35.918080
1329.403579	83621.440505	35.923098
1330.663078	83716.273713	35.928116
1331.898490	83832.182226	35.933133
1333.205360	83935.168672	35.938151
1334.567835	84048.764896	35.943168
1335.409746	84151.621762	35.948186
1337.206352	84254.343071	35.953204
1338.240667	84368.815249	35.958221
1339.916465	84473.038638	35.963239
1341.182746	84572.093045	35.968256
1342.412026	84680.175304	35.973274
1344.237567	84758.730335	35.978292
1345.352058	84848.939602	35.983309
1346.637147	84939.718141	35.988327
1347.681730	85040.215165	35.993344
1349.012066	85130.062269	35.998362
1350.355370	85215.510716	36.003380
1351.248716	85316.361697	36.008397
1352.468408	85419.214989	36.013415
1353.504511	85525.974662	36.018432
1355.023846	85641.225396	36.023450
1356.482205	85738.986783	36.028468
1357.369118	85862.231157	36.033485
1358.851865	85967.643120	36.038503
1360.493837	86092.101463	36.043520
1361.184414	86192.670270	36.048538
1362.862501	86307.784904	36.053556
1363.980351	86431.097125	36.058573
1365.581031	86544.387340	36.063591
1366.775846	86673.074130	36.068608
1368.461154	86803.547917	36.073626
1369.679082	86920.916175	36.078644
1371.309805	87034.482405	36.083661
1372.805862	87160.412644	36.088679
1374.203591	87284.571960	36.093696
1375.444745	87418.843239	36.098714
1376.965700	87537.231272	36.103732
1377.666847	87652.515949	36.108749
1379.815882	87781.718059	36.113767
1381.126701	87906.311725	36.118784
1382.521422	88024.987495	36.123802
1383.968248	88143.224770	36.128820
1385.489139	88271.779128	36.133837
1386.819426	88401.859084	36.138855
1388.290571	88523.617089	36.143872
1389.800692	88642.353422	36.148890
1391.507605	88764.899453	36.153908
1392.638811	88888.967629	36.158925
1394.253733	89003.532415	36.163943
1395.553223	89124.293110	36.168960
1396.852182	89250.009515	36.173978
1398.473767	89367.679553	36.178996
1399.839120	89501.003180	36.184013
1401.594357	89608.882422	36.189031
1402.837392	89725.117367	36.194048
1404.453373	89841.180658	36.199066
1406.325675	89953.972819	36.204084
1407.491985	90076.469005	36.209101
1408.999417	90185.820996	36.214119
1410.470419	90294.000428	36.219136
1412.163386	90398.736541	36.224154
1413.927810	90505.261538	36.229172
1415.310462	90611.098597	36.234189
1416.127028	90721.890803	36.239207
1417.705172	90830.321645	36.244224
1419.189583	90935.928559	36.249242
1421.115471	91037.855116	36.254260
1422.339900	91150.220332	36.259277
1423.225541	91260.712277	36.264295
1424.661717	91373.742431	36.269312
1425.737137	91495.675563	36.274330
1427.268643	91604.103780	36.279348
1428.619954	91709.518669	36.284365
1430.312547	91832.979376	36.289383
1431.418126	91951.931249	36.294400
1432.568648	92072.727022	36.299418
1434.392210	92182.353925	36.304436
1435.253890	92296.528910	36.309453
1436.496049	92419.694564	36.314471
1437.856784	92529.217318	36.319488
1439.077111	92651.297314	36.324506
1440.720822	92752.563810	36.329524
1442.079209	92867.272000	36.334541
1443.594922	92974.389429	36.339559
1444.993853	93082.552053	36.344576
1446.199169	93207.615143	36.349594
1447.724538	93323.477800	36.354612
1449.304565	93438.140964	36.359629
1450.146677	93571.779501	36.364647
1452.076203	93689.012889	36.369664
1453.284022	93813.900618	36.374682
1454.760384	93935.299473	36.379700
1456.108324	94068.950168	36.384717
1457.371878	94196.974179	36.389735
1459.238920	94323.903459	36.394752
1460.095517	94459.673017	36.399770
1461.797226	94587.427650	36.404788
1463.341717	94728.174082	36.409805
1464.744783	94849.030232	36.414823
1466.587614	94986.625952	36.419840
1468.214736	95121.112350	36.424858
1469.648680	95255.654749	36.429876
1471.183660	95387.989138	36.434893
1472.739246	95514.452084	36.439911
1474.716879	95646.186300	36.444928
1476.122081	95782.319909	36.449946
1477.651332	95902.957710	36.454964
1479.060579	96035.352448	36.459981
1480.604546	96165.800048	36.464999
1482.271133	96289.219331	36.470016
1483.706278	96422.866594	36.475034
1485.328550	96542.795209	36.480052
1486.913649	96668.180775	36.485069
1488.257038	96799.765052	36.490087
1489.650867	96935.157556	36.495104
1490.984663	97073.475517	36.500122
1492.633058	97192.971558	36.505140
1494.331420	97325.415475	36.510157
1495.674124	97464.938018	36.515175
1497.336614	97590.353241	36.520192
1498.649640	97728.968866	36.525210
1500.496141	97854.711439	36.530228
1501.989864	97983.475740	36.535245
1503.734942	98116.131201	36.540263
1505.538237	98228.444747	36.545280
1506.893006	98362.087383	36.550298
1508.615280	98480.131639	36.555316
1509.855141	98608.430915	36.560333
1511.073343	98738.711673	36.565351
1512.943200	98863.643284	36.570368
1514.384377	98989.998543	36.575386
1515.920220	99114.869032	36.580404
1517.626947	99242.629141	36.585421
1518.693310	99378.146420	36.590439
1520.403764	99498.072496	36.595456
1521.681036	99634.851106	36.600474
1523.382556	99758.912328	36.605492
1524.769170	99885.989539	36.610509
1526.075058	100021.167993	36.615527
1527.778347	100144.355686	36.620544
1529.509450	100280.445207	36.625562
1530.803124	100410.822424	36.630580
1531.741071	100538.365041	36.635597
1533.601593	100681.510207	36.640615
1535.044398	100815.694494	36.645632
1536.662170	100957.129137	36.650650
1538.577029	101076.141821	36.655668
1540.536211	101190.989708	36.660685
1541.421336	101310.962229	36.665703
1543.038825	101425.065417	36.670720
1544.382727	101546.945160	36.675738
1545.450300	101664.405698	36.680756
1547.224510	101775.354246	36.685773
1548.451888	101903.706598	36.690791
1549.990287	102031.339101	36.695808
1551.408994	102168.727610	36.700826
1552.801520	102288.269753	36.705844
1554.717323	102430.704013	36.710861
1556.055588	102560.144690	36.715879
1557.599629	102693.851836	36.720896
1559.142552	102836.713565	36.725914
1560.542760	102968.580475	36.730932
1562.452650	103115.671642	36.735949
1563.673234	103257.811969	36.740967
1565.320062	103386.434464	36.745984
1566.836726	103538.419298	36.751002
1568.707893	103687.243342	36.756020
1570.095594	103836.942071	36.761037
1571.695794	103974.043587	36.766055
1573.219695	104121.135896	36.771072
1574.754261	104277.089839	36.776090
1576.283258	104414.901598	36.781108
1578.200051	104567.462806	36.786125
1579.769615	104721.587580	36.791143
1581.079469	104859.942448	36.796160
1582.737766	105012.469841	36.801178
1584.746992	105157.411762	36.806196
1586.693816	105302.224548	36.811213
1587.948683	105447.221732	36.816231
1589.905533	105600.491452	36.821248
1591.280285	105747.094246	36.826266
1592.821536	105899.022573	36.831284
1594.817511	106041.371030	36.836301
1596.167137	106182.273756	36.841319
1597.872913	106315.095320	36.846336
1599.584467	106479.058234	36.851354
1601.339261	106621.218427	36.856372
1603.476380	106761.595232	36.861389
1604.540777	106906.336663	36.866407
1606.004879	107053.742714	36.871424
1607.538939	107204.346586	36.876442
1609.317194	107348.864664	36.881460
1611.132507	107496.446203	36.886477
1612.706688	107641.453767	36.891495
1614.241873	107780.863300	36.896512
1615.996335	107936.026367	36.901530
1617.970481	108083.294058	36.906548
1618.998364	108226.233436	36.911565
1620.197764	108380.876233	36.916583
1622.390840	108527.426994	36.921600
1623.924008	108683.097047	36.926618
1625.773373	108826.646529	36.931636
1627.434305	108966.497785	36.936653
1628.115347	109121.757158	36.941671
1630.190665	109270.814836	36.946688
1631.938710	109424.451187	36.951706
1633.715424	109578.109115	36.956724
1635.700863	109731.608423	36.961741
1637.118481	109856.512114	36.966759
1639.290257	109996.909371	36.971776
1641.167067	110132.851273	36.976794
1642.762121	110273.250631	36.981812
1644.568239	110405.374853	36.986829
1645.681578	110548.399226	36.991847
1647.793603	110669.253833	36.996864
1649.400619	110794.029932	37.001882
1650.801600	110909.733234	37.006900
1653.030113	111039.130982	37.011917
1653.706821	111153.248483	37.016935
1655.440586	111276.814493	37.021952
1657.143527	111404.722859	37.026970
1658.464163	111535.519210	37.031988
1660.133439	111661.835848	37.037005
1661.404654	111792.793018	37.042023
1662.576579	111942.142121	37.047040
1663.847986	112091.717323	37.052058
1665.666598	112238.481363	37.057076
1667.566379	112380.300071	37.062093
1668.762929	112550.319561	37.067111
1670.501023	112699.989537	37.072128
1671.725110	112858.516202	37.077146
1673.604069	113025.717747	37.082164
1675.170658	113175.302256	37.087181
1676.921572	113342.563248	37.092199
1678.684316	113503.012723	37.097216
1680.602693	113661.358765	37.102234
1682.289118	113835.683523	37.107252
1684.540675	113998.189778	37.112269
1685.777572	114161.894659	37.117287
1687.352077	114332.066634	37.122304
1689.299849	114486.556164	37.127322
1691.201571	114658.162615	37.132340
1692.945724	114813.801309	37.137357
1695.200201	114984.517322	37.142375
1696.634181	115138.810553	37.147392
1698.507552	115299.136581	37.152410
1700.025664	115460.710811	37.157428
1701.901104	115625.159941	37.162445
1703.603054	115794.253490	37.167463
1705.143440	115951.463386	37.172480
1706.987943	116118.380080	37.177498
1708.594704	116295.113404	37.182516
1710.143012	116455.533100	37.187533
1711.771317	116626.316124	37.192551
1713.648056	116780.204847	37.197568
1715.371279	116951.380463	37.202586
1717.218010	117128.270652	37.207604
1719.154912	117289.584734	37.212621
1720.728534	117457.767232	37.217639
1722.345543	117630.624063	37.222656
1724.607323	117802.518833	37.227674
1726.218282	117966.410649	37.232692
1728.089750	118129.400121	37.237709
1729.692144	118301.856423	37.242727
1731.201075	118476.256042	37.247744
1733.000552	118637.559242	37.252762
1734.722488	118815.973521	37.257780
1736.398037	118976.358818	37.262797
1738.039488	119148.039151	37.267815
1739.693037	119326.174728	37.272832
1741.319725	119502.425335	37.277850
1742.734638	119663.640526	37.282868
1744.714171	119849.325823	37.287885
1746.947756	120034.579257	37.292903
1748.398631	120208.488452	37.297920
1750.174721	120376.779217	37.302938
1751.681669	120551.594536	37.307956
1753.304373	120733.001438	37.312973
1755.463966	120908.579366	37.317991
1757.293000	121096.628123	37.323008
1759.012805	121259.045665	37.328026
1760.676473	121444.052067	37.333044
1762.484977	121602.093567	37.338061
1764.120787	121763.942773	37.343079
1765.741336	121921.405932	37.348096
1767.352719	122074.367873	37.353114
1768.801324	122244.506329	37.358132
1770.648581	122399.817675	37.363149
1772.466377	122573.109500	37.368167
1773.766827	122757.531684	37.373184
1775.483060	122919.195542	37.378202
1776.975519	123098.806981	37.383220
1779.070951	123276.853851	37.388237
1780.620540	123459.160081	37.393255
1782.093321	123636.798046	37.398272
1784.215937	123826.590196	37.403290
1785.755545	124023.337067	37.408308
1787.721775	124212.800189	37.413325
1789.444407	124401.173066	37.418343
1791.300015	124594.968465	37.423360
1792.996483	124776.204905	37.428378
1794.781105	124975.721958	37.433396
1796.806640	125162.808013	37.438413
1798.241910	125368.699147	37.443431
1800.069242	125568.313971	37.448448
1802.392468	125763.247414	37.453466
1804.393383	125957.458078	37.458484
1806.074853	126156.844767	37.463501
1808.196702	126344.822031	37.468519
1810.008056	126543.797110	37.473536
1812.014716	126732.720215	37.478554
1813.660071	126924.656452	37.483572
1815.601547	127122.789445	37.488589
1817.470964	127309.757410	37.493607
1819.307781	127512.348993	37.498624
1821.497271	127704.698968	37.503642
1822.829409	127913.156359	37.508660
1824.568922	128101.632514	37.513677
1826.763777	128298.907036	37.518695
1828.108064	128498.674709	37.523712
1830.508490	128698.240902	37.528730
1832.222075	128905.920709	37.533748
1834.302023	129095.008109	37.538765
1835.906665	129304.470404	37.543783
1837.416074	129508.962331	37.548800
1839.612173	129714.401451	37.553818
1841.135510	129923.029395	37.558836
1842.843351	130127.290424	37.563853
1844.713041	130340.142298	37.568871
1846.495363	130553.008834	37.573888
1848.632133	130764.260645	37.578906
1850.080095	130967.576484	37.583924
1852.025345	131175.307480	37.588941
1854.100064	131391.253949	37.593959
1856.238783	131600.504844	37.598976
1858.465532	131801.178459	37.603994
1860.178115	132003.176487	37.609012
1862.152452	132213.788211	37.614029
1864.154936	132415.616155	37.619047
1865.957288	132618.135987	37.624064
1867.820173	132816.142891	37.629082
1869.572512	133012.594505	37.634100
1871.803401	133219.973622	37.639117
1873.630825	133422.125301	37.644135
1875.347768	133618.267915	37.649152
1877.064656	133809.805350	37.654170
1878.850951	134019.224201	37.659188
1880.867814	134227.174301	37.664205
1883.003520	134433.127387	37.669223
1884.681783	134634.292694	37.674240
1886.409978	134833.598520	37.679258
1888.414067	135018.053981	37.684276
1889.658320	135196.080799	37.689293
1891.806263	135389.842011	37.694311
1893.470734	135590.696529	37.699328
1895.218446	135769.256349	37.704346
1897.268433	135958.352855	37.709364
1898.941898	136147.356477	37.714381
1901.087070	136351.616493	37.719399
1902.457000	136560.312561	37.724416
1904.377632	136745.841310	37.729434
1906.162547	136953.789348	37.734452
1907.357787	137167.489762	37.739469
1909.993584	137369.228839	37.744487
1911.463009	137599.207764	37.749504
1913.138844	137813.508947	37.754522
1915.162819	138026.094545	37.759540
1917.110898	138254.542879	37.764557
1918.759853	138473.927346	37.769575
1920.613597	138705.933137	37.774592
1922.827516	138931.615017	37.779610
1924.901674	139158.005017	37.784628
1926.614828	139390.289887	37.789645
1928.819031	139615.684690	37.794663
1930.355502	139861.235552	37.799680
1932.521515	140087.983750	37.804698
1934.620775	140320.936467	37.809716
1936.520570	140554.403616	37.814733
1938.762214	140783.719578	37.819751
1940.576552	141018.522137	37.824768
1942.813800	141257.156138	37.829786
1945.010446	141498.475439	37.834804
1946.801770	141735.823277	37.839821
1949.248484	141956.749519	37.844839
1950.762976	142190.906440	37.849856
1952.980698	142435.158786	37.854874
1954.888013	142665.182966	37.859892
1957.086846	142906.293168	37.864909
1959.154652	143128.007094	37.869927
1960.720003	143367.682491	37.874944
1962.825760	143597.768993	37.879962
1964.852066	143838.707544	37.884980
1966.587236	144072.166429	37.889997
1968.947673	144313.309112	37.895015
1970.652470	144551.458208	37.900032
1972.714688	144777.305197	37.905050
1975.114145	145016.985638	37.910068
1977.086112	145253.738453	37.915085
1978.978507	145483.435315	37.920103
1981.064059	145718.065753	37.925120
1983.560642	145951.541782	37.930138
1985.582383	146171.397925	37.935156
1987.396211	146413.739931	37.940173
1989.882868	146632.688013	37.945191
1991.799232	146852.703095	37.950208
1993.740970	147080.305221	37.955226
1995.673626	147304.952422	37.960244
1997.484180	147535.902392	37.965261
1999.691997	147764.354587	37.970279
2001.614750	147995.542985	37.975296
2003.174863	148228.705439	37.980314
2005.800086	148455.090248	37.985332
2007.077842	148694.213525	37.990349
2009.323790	148928.249684	37.995367
2010.896524	149166.529540	38.000384
2012.830162	149399.067849	38.005402
2015.147423	149637.018160	38.010420
2016.761348	149867.298140	38.015437
2018.907769	150101.951522	38.020455
2020.858125	150324.539843	38.025472
2022.447788	150551.183586	38.030490
2024.758803	150762.560234	38.035508
2025.969606	150987.716186	38.040525
2028.231825	151209.091820	38.045543
2029.724543	151439.714694	38.050560
2031.619157	151670.783731	38.055578
2033.414818	151907.162350	38.060596
2035.187827	152162.103555	38.065613
2037.535209	152409.467285	38.070631
2039.505468	152659.581879	38.075648
2041.567168	152916.906125	38.080666
2043.676331	153160.984501	38.085684
2045.220992	153418.848502	38.090701
2047.373852	153683.169107	38.095719
2049.598961	153950.767455	38.100736
2051.448123	154204.030502	38.105754
2053.761711	154472.303019	38.110772
2055.750877	154738.507358	38.115789
2058.036915	154996.326614	38.120807
2059.847896	155269.961893	38.125824
2061.953064	155539.287379	38.130842
2063.842441	155811.719750	38.135860
2065.922104	156087.652849	38.140877
2068.256808	156361.135596	38.145895
2070.007255	156632.488994	38.150912
2072.349996	156909.438669	38.155930
2074.793052	157192.746779	38.160948
2076.729578	157463.592633	38.165965
2079.340511	157740.885295	38.170983
2081.135175	158016.033893	38.176000
2083.468320	158284.371623	38.181018
2085.561826	158565.455546	38.186036
2087.355707	158847.476059	38.191053
2089.287161	159130.453994	38.196071
2091.844339	159410.187452	38.201088
2093.592346	159680.818678	38.206106
2095.918399	159964.081819	38.211124
2098.083796	160263.684798	38.216141
2100.291145	160542.512986	38.221159
2102.460606	160838.411036	38.226176
2104.850420	161112.325610	38.231194
2106.872731	161396.289999	38.236212
2108.652094	161688.317122	38.241229
2110.937028	161979.873339	38.246247
2112.876237	162272.893923	38.251264
2114.988152	162556.709889	38.256282
2117.277248	162836.208326	38.261300
2119.528804	163133.373854	38.266317
2121.974331	163400.865421	38.271335
2124.405601	163687.861420	38.276352
2126.355622	163965.589246	38.281370
2128.761452	164234.004510	38.286388
2130.937280	164520.421781	38.291405
2133.057364	164793.924176	38.296423
2135.078313	165076.038518	38.301440
2137.352002	165358.317856	38.306458
2139.771936	165621.277071	38.311476
2141.765297	165904.694211	38.316493
2144.225464	166174.594276	38.321511
2146.632424	166450.712308	38.326528
2148.362878	166724.206964	38.331546
2150.470354	166986.153548	38.336564
2152.546833	167254.822507	38.341581
2154.768488	167527.063094	38.346599
2157.046150	167802.736861	38.351616
2159.239357	168087.033326	38.356634
2161.032028	168351.725756	38.361652
2163.074745	168603.873758	38.366669
2165.004531	168854.592771	38.371687
2166.947584	169107.773825	38.376704
2168.511340	169369.280605	38.381722
2170.623137	169632.112424	38.386740
2172.474940	169905.829053	38.391757
2174.002241	170175.940409	38.396775
2176.451092	170459.368456	38.401792
2178.248383	170748.003323	38.406810
2180.304354	171033.665964	38.411828
2182.589504	171333.451666	38.416845
2184.864827	171621.825067	38.421863
2186.932198	171918.980533	38.426880
2188.549544	172210.671061	38.431898
2190.958569	172514.480011	38.436916
2192.943767	172829.149156	38.441933
2195.181165	173136.999750	38.446951
2197.553736	173449.046195	38.451968
2199.921076	173776.801926	38.456986
2201.996528	174086.230615	38.462004
2204.088120	174397.143665	38.467021
2206.299375	174730.311578	38.472039
2208.300244	175050.282268	38.477056
2210.783612	175383.156590	38.482074
2213.330629	175697.305319	38.487092
2215.411288	176035.095681	38.492109
2217.741676	176364.150275	38.497127
2220.316694	176681.714252	38.502144
2222.181120	177013.320113	38.507162
2224.288924	177341.117992	38.512180
2226.408750	177679.937525	38.517197
2228.970744	178009.953037	38.522215
2231.589633	178344.278477	38.527232
2233.746395	178682.461320	38.532250
2236.238440	179011.628065	38.537268
2238.543916	179341.307641	38.542285
2240.849609	179670.175703	38.547303
2243.045551	179998.096963	38.552320
2245.424008	180328.987951	38.557338
2247.812114	180665.288380	38.562356
2250.109050	181004.982165	38.567373
2252.207459	181330.155095	38.572391
2254.720319	181670.503497	38.577408
2257.100146	182005.006891	38.582426
2259.750295	182330.783229	38.587444
2261.561674	182662.913820	38.592461
2264.093960	182997.092248	38.597479
2266.059314	183320.591125	38.602496
2268.095860	183652.232952	38.607514
2270.627761	183984.763975	38.612532
2272.967449	184331.193758	38.617549
2275.330191	184662.712062	38.622567
2277.631540	184997.288901	38.627584
2279.637117	185338.796018	38.632602
2282.055684	185656.568079	38.637620
2284.464450	186075.736142	38.642637
2286.654152	186415.872067	38.647655
2289.423384	186743.473240	38.652672
2291.804181	187080.381285	38.657690
2294.127679	187406.529934	38.662708
2296.246758	187739.797883	38.667725
2298.645626	188072.312136	38.672743
2301.078242	188397.938832	38.677760
2303.025166	188735.732400	38.682778
2305.414773	189058.395976	38.687796
2307.258762	189399.306380	38.692813
2310.258098	189738.742617	38.697831
2312.440684	190051.332056	38.702848
2314.712445	190354.307206	38.707866
2317.131509	190659.876455	38.712884
2319.284485	190963.506696	38.717901
2321.126011	191269.827834	38.722919
2323.651323	191568.956628	38.727936
2325.485888	191883.662584	38.732954
2328.085855	192199.698081	38.737972
2330.310917	192518.155007	38.742989
2332.188644	192836.209603	38.748007
2334.579353	193156.979269	38.753024
2336.406990	193501.333170	38.758042
2338.140413	193832.570399	38.763060
2340.633016	194183.731715	38.768077
2342.776697	194524.660864	38.773095
2345.066660	194871.130985	38.778112
2347.178716	195234.318281	38.783130
2348.999883	195590.566492	38.788148
2351.783178	195950.272899	38.793165
2354.018521	196324.442716	38.798183
2356.582567	196689.316261	38.803200
2358.705994	197057.282110	38.808218
2361.024743	197444.345913	38.813236
2363.771045	197819.989680	38.818253
2365.845596	198184.638406	38.823271
2368.537555	198562.680296	38.828288
2370.768147	198963.199374	38.833306
2373.060181	199336.936326	38.838324
2375.598941	199710.940613	38.843341
2377.691055	200112.551114	38.848359
2380.403229	200505.454822	38.853376
2382.589438	200897.247440	38.858394
2385.112841	201288.378867	38.863412
2387.797132	201690.536171	38.868429
2390.165698	202088.602984	38.873447
2392.515129	202476.106298	38.878464
2394.841638	202871.437996	38.883482
2397.287120	203273.356712	38.888500
2400.103472	203665.311603	38.893517
2402.317581	204067.979349	38.898535
2405.072874	204458.014816	38.903552
2407.731216	204859.853035	38.908570
2410.423868	205242.914089	38.913588
2412.985624	205631.229238	38.918605
2415.483152	206035.127093	38.923623
2418.082937	206412.870215	38.928640
2420.572499	206803.408864	38.933658
2422.954070	207189.290876	38.938676
2425.735852	207571.961306	38.943693
2428.118059	207967.523143	38.948711
2430.356419	208344.436737	38.953728
2432.727424	208744.345587	38.958746
2435.385339	209130.949970	38.963764
2437.730438	209518.314939	38.968781
2440.466359	209905.289443	38.973799
2443.289478	210285.442865	38.978816
2445.691411	210668.837808	38.983834
2447.851862	211041.855476	38.988852
2450.908706	211424.819319	38.993869
2452.948763	211792.903053	38.998887
2455.237966	212172.608694	39.003904
2458.000691	212552.368145	39.008922
2460.091381	212930.149557	39.013940
2462.965737	213303.643271	39.018957
2465.090827	213698.440653	39.023975
2467.817322	214067.842851	39.028992
2470.082095	214446.564243	39.034010
2472.105897	214822.478319	39.039028
2474.938736	215206.218244	39.044045
2476.804353	215573.952277	39.049063
2479.306317	215939.098048	39.054080
2481.921761	216301.584485	39.059098
2483.935759	216666.197135	39.064116
2486.015086	217028.335743	39.069133
2488.392309	217404.247984	39.074151
2490.263071	217774.955324	39.079168
2492.670119	218159.729457	39.084186
2495.277935	218547.368672	39.089204
2497.839216	218931.179402	39.094221
2499.841027	219330.040384	39.099239
2502.803610	219711.426586	39.104256
2505.114143	220119.842716	39.109274
2507.517489	220527.990596	39.114292
2510.073062	220939.138082	39.119309
2512.382900	221349.993760	39.124327
2514.602232	221748.822191	39.129344
2517.545247	222173.272468	39.134362
2519.755457	222580.943245	39.139380
2522.633113	223002.050656	39.144397
2524.924975	223424.062284	39.149415
2527.741684	223847.719817	39.154432
2530.515222	224270.342588	39.159450
2532.727376	224702.147457	39.164468
2535.586615	225115.459112	39.169485
2538.425883	225544.549850	39.174503
2540.882346	225966.841067	39.179520
2543.676586	226399.546202	39.184538
2546.224000	226833.204270	39.189556
2548.788599	227252.480901	39.194573
2551.378424	227687.199231	39.199591
2554.181641	228123.916594	39.204608
2556.663616	228549.302817	39.209626
2559.287091	228975.835486	39.214644
2562.333236	229400.701783	39.219661
2564.688776	229842.721513	39.224679
2567.671722	230265.971445	39.229696
2570.014883	230706.900333	39.234714
2572.748898	231130.137780	39.239732
2575.291608	231556.681882	39.244749
2577.844236	231991.175631	39.249767
2580.352469	232418.385067	39.254784
2583.093048	232844.389470	39.259802
2585.684157	233288.758456	39.264820
2588.247851	233716.999869	39.269837
2590.896918	234157.345294	39.274855
2593.875376	234597.334218	39.279872
2596.522549	235020.836384	39.284890
2599.058851	235459.115014	39.289908
2601.636855	235884.227542	39.294925
2604.118306	236324.927154	39.299943
2606.912967	236752.621624	39.304960
2609.597064	237179.748526	39.309978
2612.000987	237618.045328	39.314996
2614.970460	238051.553892	39.320013
2617.406634	238486.999349	39.325031
2619.990779	238918.534445	39.330048
2622.716658	239347.379517	39.335066
2625.265247	239792.992473	39.340084
2627.848233	240220.131085	39.345101
2630.369755	240659.370646	39.350119
2633.045618	241094.978208	39.355136
2635.126556	241541.296237	39.360154
2637.960515	241978.833793	39.365172
2640.936092	242400.090476	39.370189
2643.439435	242857.848117	39.375207
2645.994818	243291.311374	39.380224
2648.896516	243725.405818	39.385242
2651.240069	244140.762630	39.390260
2654.150819	244542.185761	39.395277
2656.884873	244947.877945	39.400295
2659.149047	245342.820840	39.405312
2661.572112	245756.256953	39.410330
2664.430116	246155.170344	39.415348
2667.116153	246572.272681	39.420365
2670.054186	246984.610013	39.425383
2672.505488	247400.781803	39.430400
2675.010690	247820.145017	39.435418
2677.480656	248245.050520	39.440436
2680.169728	248664.256182	39.445453
2682.781844	249084.057092	39.450471
2685.389540	249521.436117	39.455488
2688.051284	249954.792058	39.460506
2690.408095	250391.420426	39.465524
2693.056193	250837.477322	39.470541
2695.824488	251289.356772	39.475559
2698.242441	251739.104897	39.480576
2700.770296	252184.059070	39.485594
2703.532382	252648.585754	39.490612
2706.516555	253107.589674	39.495629
2709.535638	253572.276735	39.500647
2712.308939	254025.900066	39.505664
2715.015754	254480.827801	39.510682
2717.684886	254940.992650	39.515700
2720.673351	255405.729345	39.520717
2723.014418	255874.680233	39.525735
2725.669775	256344.418832	39.530752
2728.636018	256820.051262	39.535770
2731.633180	257292.883051	39.540788
2734.327175	257747.141414	39.545805
2737.394838	258223.921358	39.550823
2740.057323	258691.084869	39.555840
2743.115747	259180.461372	39.560858
2745.864872	259653.094294	39.565876
2748.804543	260118.354983	39.570893
2751.465849	260594.274517	39.575911
2754.238104	261075.508905	39.580928
2757.001393	261553.085069	39.585946
2759.652128	262026.104748	39.590964
2762.184458	262503.662055	39.595981
2765.013227	262986.632140	39.600999
2767.779960	263465.444205	39.606016
2770.523356	263953.731831	39.611034
2773.069615	264446.213421	39.616052
2776.109973	264928.583084	39.621069
2778.944853	265418.830854	39.626087
2781.275425	265907.656226	39.631104
2784.225278	266402.224646	39.636122
2787.001621	266909.212276	39.641140
2789.904981	267384.225955	39.646157
2792.929761	267887.893464	39.651175
2795.550490	268376.864726	39.656192
2798.557359	268868.846604	39.661210
2801.186299	269372.771102	39.666228
2804.248846	269848.966913	39.671245
2807.087857	270347.418263	39.676263
2810.003398	270840.318272	39.681280
2812.776941	271325.059651	39.686298
2815.628918	271829.926441	39.691316
2818.315417	272317.215725	39.696333
2821.352738	272803.660396	39.701351
2823.790903	273302.995717	39.706368
2826.925537	273779.718060	39.711386
2829.444692	274283.733487	39.716404
2832.734291	274769.873745	39.721421
2835.450100	275256.278234	39.726439
2837.860464	275728.327657	39.731456
2841.130845	276177.739475	39.736474
2843.964229	276632.194434	39.741492
2846.490275	277086.466085	39.746509
2849.454761	277552.958474	39.751527
2852.047661	278022.858152	39.756544
2854.743239	278482.631626	39.761562
2857.297201	278955.960118	39.766580
2860.010084	279434.187625	39.771597
2862.679997	279915.161473	39.776615
2865.457463	280399.696190	39.781632
2868.493695	280880.302112	39.786650
2870.953025	281385.398814	39.791668
2873.711885	281872.694793	39.796685
2876.375584	282369.093428	39.801703
2878.956574	282886.984826	39.806720
2882.159121	283389.336320	39.811738
2884.870981	283906.768239	39.816756
2887.802026	284424.873252	39.821773
2890.571133	284947.697358	39.826791
2893.522487	285478.284803	39.831808
2896.778126	286006.814746	39.836826
2899.323297	286536.187513	39.841844
2902.314338	287061.423936	39.846861
2905.626542	287588.180556	39.851879
2908.223145	288125.988301	39.856896
2911.627866	288657.927319	39.861914
2914.667242	289203.147861	39.866932
2917.820355	289733.568291	39.871949
2920.839315	290262.557890	39.876967
2923.655132	290795.332545	39.881984
2927.095033	291327.751652	39.887002
2929.887755	291867.858689	39.892020
2932.592674	292408.380910	39.897037
2935.914728	292946.872679	39.902055
2938.775844	293483.222484	39.907072
2941.972752	294025.786503	39.912090
2944.721483	294563.210514	39.917108
2947.677040	295113.139722	39.922125
2950.880497	295639.438890	39.927143
2953.902754	296189.804621	39.932160
2957.091691	296728.866707	39.937178
2959.931407	297272.217918	39.942196
2962.693076	297817.277096	39.947213
2966.174313	298360.441911	39.952231
2968.616613	298908.282125	39.957248
2971.756945	299444.380977	39.962266
2974.616365	300001.716494	39.967284
2977.686718	300547.792598	39.972301
2980.893962	301090.973262	39.977319
2983.895642	301644.411115	39.982336
2986.804718	302190.470367	39.987354
2989.766652	302741.136006	39.992372
2992.706320	303295.632588	39.997389
2996.195597	303840.315279	40.002407
2998.835009	304394.009260	40.007424
3001.753246	304940.444707	40.012442
3004.986474	305489.769927	40.017460
3007.542336	306051.099793	40.022477
3010.773364	306597.215027	40.027495
3013.651383	307153.278861	40.032512
3016.942257	307708.383865	40.037530
3019.937624	308258.249005	40.042548
3023.080415	308813.720043	40.047565
3026.346276	309352.337116	40.052583
3029.096233	309919.329581	40.057600
3032.106160	310456.958960	40.062618
3035.192670	310999.519817	40.067636
3038.264579	311513.218304	40.072653
3041.283704	312022.325496	40.077671
3043.759972	312549.379702	40.082688
3046.776125	313057.663987	40.087706
3049.703065	313575.169619	40.092724
3052.687199	314102.533349	40.097741
3055.776686	314628.529540	40.102759
3058.419397	315160.832528	40.107776
3061.577224	315682.313833	40.112794
3064.494241	316219.256856	40.117812
3066.995120	316770.647778	40.122829
3070.131916	317317.111124	40.127847
3072.551595	317879.971870	40.132864
3076.215935	318438.698270	40.137882
3078.951116	319003.728794	40.142900
3081.786655	319568.711023	40.147917
3085.333254	320130.555457	40.152935
3088.334129	320710.672167	40.157952
3091.734150	321291.505572	40.162970
3094.845297	321873.594040	40.167988
3097.589864	322460.349822	40.173005
3100.804087	323035.351987	40.178023
3103.953238	323624.236156	40.183040
3107.372411	324211.623659	40.188058
3110.236388	324798.759364	40.193076
3113.766674	325392.557664	40.198093
3116.673017	325988.956351	40.203111
3120.037902	326585.503285	40.208128
3123.288045	327171.073129	40.213146
3126.880275	327756.987150	40.218164
3129.740724	328356.123464	40.223181
3133.601848	328952.557918	40.228199
3136.365345	329542.557799	40.233216
3140.012291	330137.662976	40.238234
3143.094552	330727.011881	40.243252
3146.487213	331325.411173	40.248269
3149.805248	331914.223283	40.253287
3152.855205	332509.435614	40.258304
3155.682503	333104.444993	40.263322
3159.072687	333691.747078	40.268340
3161.886976	334285.167104	40.273357
3165.329298	334891.772371	40.278375
3168.469413	335490.475033	40.283392
3171.487907	336100.576414	40.288410
3175.080435	336691.198872	40.293428
3178.073954	337294.993605	40.298445
3181.532055	337894.089623	40.303463
3184.586898	338506.631012	40.308480
3188.009178	339093.334835	40.313498
3191.603648	339699.811372	40.318516
3194.825633	340304.205056	40.323533
3198.008568	340892.108656	40.328551
3201.268585	341496.247827	40.333568
3204.324540	342082.883207	40.338586
3207.980956	342673.828232	40.343604
3210.880274	343277.663070	40.348621
3214.131745	343868.929738	40.353639
3217.406287	344461.957889	40.358656
3220.660159	345057.337464	40.363674
3224.175727	345645.590643	40.368692
3227.408248	346229.160899	40.373709
3230.941519	346819.622511	40.378727
3233.690296	347416.763570	40.383744
3237.171417	348005.741633	40.388762
3240.846748	348592.270115	40.393780
3243.646508	349184.198659	40.398797
3246.614592	349769.802021	40.403815
3249.556218	350361.484444	40.408832
3252.592379	350928.445293	40.413850
3255.797567	351479.878070	40.418868
3258.699233	352040.527014	40.423885
3262.076620	352598.886365	40.428903
3265.140383	353178.835376	40.433920
3267.662352	353738.677040	40.438938
3271.207370	354316.705009	40.443956
3274.407136	354892.646549	40.448973
3277.391051	355476.242028	40.453991
3279.999674	356069.974860	40.459008
3283.516830	356668.549126	40.464026
3286.954081	357269.735370	40.469044
3290.316614	357858.804327	40.474061
3293.722337	358460.707403	40.479079
3297.045765	359067.377038	40.484096
3300.092847	359676.612437	40.489114
3303.276794	360289.515090	40.494132
3306.297799	360920.680716	40.499149
3309.786747	361539.264325	40.504167
3312.909450	362176.749735	40.509184
3316.214112	362814.674756	40.514202
3319.373091	363459.806739	40.519220
3322.178465	364099.378492	40.524237
3325.527073	364753.196501	40.529255
3329.269719	365411.069549	40.534272
3332.139539	366069.849169	40.539290
3335.628712	366728.061262	40.544308
3338.837553	367396.717383	40.549325
3342.624908	368075.252286	40.554343
3346.111921	368747.736072	40.559360
3349.686115	369428.577875	40.564378
3353.099796	370092.349577	40.569396
3356.710817	370773.710639	40.574413
3360.359460	371435.614964	40.579431
3363.745007	372118.650622	40.584448
3367.435685	372772.408596	40.589466
3371.263591	373421.417192	40.594484
3374.604019	374103.777368	40.599501
3378.010012	374770.782646	40.604519
3382.115282	375423.779524	40.609536
3385.340851	376085.789728	40.614554
3389.248471	376746.537574	40.619572
3392.533182	377403.566224	40.624589
3395.751803	378054.610694	40.629607
3399.196483	378716.319223	40.634624
3403.106881	379378.166752	40.639642
3406.672578	380032.933592	40.644660
3410.338638	380691.493252	40.649677
3413.857445	381347.247770	40.654695
3417.068840	381992.598439	40.659712
3420.468872	382640.005898	40.664730
3423.672295	383297.178587	40.669748
3427.033264	383949.016807	40.674765
3430.611073	384611.770685	40.679783
3434.238754	385275.816492	40.684800
3437.602392	385934.871839	40.689818
3441.113357	386596.014286	40.694836
3444.477027	387249.160270	40.699853
3447.547893	387911.298910	40.704871
3451.396133	388562.866551	40.709888
3454.320618	389225.702098	40.714906
3457.838142	389889.136615	40.719924
3460.948052	390558.009807	40.724941
3464.585083	391217.566715	40.729959
3468.144396	391881.320776	40.734976
3471.618669	392549.120811	40.739994
3475.347608	393215.799557	40.745012
3478.703210	393863.959826	40.750016
3481.942125	394475.431788	40.755021
3485.280300	395064.690969	40.760026
3488.186625	395583.550685	40.765031
3491.285697	396061.560452	40.770036
3494.009980	396491.958933	40.775040
3496.508460	396875.943640	40.780045
3498.861716	397207.616739	40.785050
3500.992452	397514.196597	40.790055
3503.270131	397754.617931	40.795060
3504.864593	397970.121909	40.800064
3506.557519	398143.128680	40.805069
3508.339254	398276.381308	40.810074
3509.396192	398373.610478	40.815079
3510.173077	398451.698592	40.820084
3511.583515	398506.697285	40.825088
3512.091561	398528.390865	40.830093
3513.411909	398521.943040	40.835098
3514.308607	398510.485956	40.840103
3515.154587	398459.145768	40.845108
3515.918673	398396.246741	40.850112
3516.443432	398302.527424	40.855117
3517.124460	398193.760678	40.860122
3516.731395	398092.316707	40.865127
3517.737041	397957.208425	40.870132
3517.474807	397816.561542	40.875136
3517.662749	397668.027706	40.880141
3518.338028	397512.311544	40.885146
3517.911209	397367.576523	40.890151
3518.186172	397187.203162	40.895156
3518.260620	397020.512738	40.900160
3518.340485	396840.370115	40.905165
3518.365020	396649.626768	40.910170
3517.943489	396462.910288	40.915175
3517.880585	396274.309295	40.920180
3518.100849	396081.196123	40.925184
3517.774195	395886.186953	40.930189
3517.629561	395697.035775	40.935194
3517.250246	395509.645399	40.940199
3517.497284	395303.984478	40.945204
3516.983006	395123.058427	40.950208
3517.044483	394924.732431	40.955213
3516.975211	394734.039127	40.960218
3516.502021	394544.219329	40.965223
3516.239209	394351.522695	40.970228
3515.916602	394152.793248	40.975232
3515.767534	393962.918425	40.980237
3515.668681	393781.663821	40.985242
3515.117911	393607.432612	40.990247
3514.995433	393427.194269	40.995252
3514.509647	393245.132887	41.000256
3514.427726	393071.890885	41.005261
3514.530701	392891.765766	41.010266
3514.125885	392730.094945	41.015271
3514.135083	392542.113387	41.020276
3513.950299	392388.782198	41.025280
3513.346503	392219.422691	41.030285
3513.182912	392055.983837	41.035290
3513.325444	391901.431041	41.040295
3513.336857	391733.444635	41.045300
3513.387158	391581.899376	41.050304
3512.737669	391417.567300	41.055309
3512.772470	391265.616361	41.060314
3512.492331	391115.439583	41.065319
3512.534794	390961.251798	41.070324
3511.908970	390811.533095	41.075328
3511.739364	390663.620919	41.080333
3511.771260	390514.864197	41.085338
3511.147412	390378.647025	41.090343
3511.498798	390244.308111	41.095348
3511.287664	390103.557500	41.100352
3510.800435	389958.432073	41.105357
3510.812800	389825.184418	41.110362
3510.536732	389702.642712	41.115367
3510.663126	389569.020541	41.120372
3510.425097	389443.679248	41.125376
3510.181735	389323.770664	41.130381
3510.029498	389193.464568	41.135386
3509.806756	389078.552576	41.140391
3509.586813	388951.936693	41.145396
3509.519947	388838.446334	41.150400
3509.244973	388727.678777	41.155405
3509.491381	388611.371540	41.160410
3509.324573	388495.381926	41.165415
3509.245339	388374.351609	41.170420
3508.878721	388275.020245	41.175424
3508.731071	388171.313277	41.180429
3508.538701	388063.703261	41.185434
3508.445210	387953.741795	41.190439
3508.297552	387850.922043	41.195444
3508.150404	387752.316062	41.200448
3508.316655	387660.236228	41.205453
3508.064213	387551.516320	41.210458
3507.859828	387456.599252	41.215463
3507.970459	387361.480480	41.220468
3507.908810	387265.474200	41.225472
3508.189020	387172.283174	41.230477
3507.642619	387071.375585	41.235482
3507.668286	386979.569012	41.240487
3507.637633	386880.890706	41.245492
3507.457526	386801.098664	41.250496
3507.199575	386717.357920	41.255501
3507.367336	386629.234640	41.260506
3507.139104	386539.268543	41.265511
3507.096455	386442.773793	41.270516
3506.828048	386365.989958	41.275520
3506.796730	386286.960182	41.280525
3506.723451	386203.747548	41.285530
3506.803343	386132.595881	41.290535
3506.806120	386047.314404	41.295540
3506.369261	385975.074818	41.300544
3506.469466	385885.106064	41.305549
3506.414495	385811.511743	41.310554
3506.502367	385742.718929	41.315559
3506.117276	385677.731750	41.320564
3506.371329	385601.956035	41.325568
3506.224371	385525.658541	41.330573
3506.231835	385448.448155	41.335578
3506.176655	385378.762594	41.340583
3506.142731	385313.669059	41.345588
3505.981413	385239.048654	41.350592
3505.775568	385172.356569	41.355597
3505.951958	385100.120623	41.360602
3505.179957	385034.328752	41.365607
3505.499049	384967.173594	41.370612
3505.848106	384906.386496	41.375616
3505.782547	384848.735974	41.380621
3505.708819	384782.123869	41.385626
3505.418615	384714.047254	41.390631
3505.598227	384651.940236	41.395636
3505.576465	384579.098895	41.400640
3505.560805	384517.605916	41.405645
3505.104797	384454.886399	41.410650
3504.974621	384393.004693	41.415655
3505.304076	384325.186083	41.420660
3505.175367	384281.305816	41.425664
3504.911076	384222.466055	41.430669
3505.012153	384163.899384	41.435674
3504.726431	384120.881171	41.440679
3505.022352	384060.811277	41.445684
3505.135577	384009.351806	41.450688
3504.824893	383947.344768	41.455693
3505.145264	383891.587140	41.460698
3504.649740	383835.499316	41.465703
3504.829991	383782.581668	41.470708
3505.148066	383727.052562	41.475712
3505.371340	383672.706086	41.480717
3504.805068	383617.669836	41.485722
3504.777799	383561.076894	41.490727
3504.733837	383506.466955	41.495732
3505.300224	383443.687433	41.500736
3504.857043	383394.573158	41.505741
3504.736790	383328.548523	41.510746
3504.563274	383290.538994	41.515751
3504.855013	383235.343017	41.520756
3504.712035	383180.747797	41.525760
3504.431808	383125.869117	41.530765
3504.612152	383073.635577	41.535770
3504.545403	383033.196829	41.540775
3504.748648	382976.160462	41.545780
3504.645883	382927.500162	41.550784
3504.487377	382876.918650	41.555789
3504.833693	382814.628902	41.560794
3504.535677	382765.668583	41.565799
3504.187747	382719.712219	41.570804
3504.782633	382667.971980	41.575808
3504.025760	382622.536140	41.580813
3504.316167	382575.235963	41.585818
3504.215681	382528.123490	41.590823
3503.866596	382487.093013	41.595828
3503.962619	382445.612320	41.600832
3503.851443	382422.497184	41.605837
3503.934847	382369.617105	41.610842
3504.068196	382329.374652	41.615847
3504.100976	382276.553045	41.620852
3504.484456	382238.506079	41.625856
3504.250072	382194.003887	41.630861
3504.232546	382137.990345	41.635866
3503.991657	382090.797355	41.640871
3504.124966	382057.613687	41.645876
3504.510908	382009.408864	41.650880
3504.053892	381963.544312	41.655885
3504.174078	381915.609206	41.660890
3504.087946	381872.937081	41.665895
3503.942538	381829.309174	41.670900
3503.941025	381793.606843	41.675904
3504.016042	381746.160924	41.680909
3504.132968	381702.999845	41.685914
3503.759286	381665.806269	41.690919
3503.831110	381621.255446	41.695924
3504.138729	381577.912126	41.700928
3503.933700	381538.381332	41.705933
3504.005244	381491.773470	41.710938
3503.955140	381454.681600	41.715943
3504.065121	381407.966033	41.720948
3504.042233	381367.035388	41.725952
3504.081062	381330.031075	41.730957
3503.973149	381280.327355	41.735962
3503.741184	381246.691624	41.740967
3503.869854	381207.083006	41.745972
3503.965856	381161.283346	41.750976
3503.659224	381119.964775	41.755981
3503.847118	381073.566605	41.760986
3503.705063	381038.062867	41.765991
3503.792877	381004.275488	41.770996
3503.928979	380960.272201	41.776000
3503.465794	380918.901491	41.781005
3503.682358	380874.479235	41.786010
3503.575171	380848.619531	41.791015
3503.695050	380805.659663	41.796020
3503.786252	380772.074609	41.801024
3503.918897	380739.346464	41.806029
3503.984683	380695.531433	41.811034
3503.562711	380650.243183	41.816039
3503.560865	380602.121504	41.821044
3503.633888	380570.875293	41.826048
3503.554290	380536.072196	41.831053
3503.420882	380492.871893	41.836058
3503.621120	380464.526111	41.841063
3503.920846	380425.626132	41.846068
3503.887427	380384.822562	41.851072
3503.559383	380350.565770	41.856077
3503.669548	380309.587373	41.861082
3503.585269	380270.188239	41.866087
3503.480619	380241.000851	41.871092
3503.778256	380200.170873	41.876096
3503.597052	380165.332306	41.881101
3503.600568	380116.954957	41.886106
3503.587387	380087.143691	41.891111
3503.754264	380042.651577	41.896116
3503.642063	380014.607878	41.901120
3503.530141	379980.774079	41.906125
3503.536815	379940.039765	41.911130
3503.384881	379901.615614	41.916135
3503.583234	379868.317471	41.921140
3503.673113	379826.909766	41.926144
3503.717720	379793.178343	41.931149
3503.659651	379751.082480	41.936154
3503.431495	379716.809318	41.941159
3503.352286	379677.738645	41.946164
3503.828004	379639.267232	41.951168
3503.664989	379606.431315	41.956173
3503.364395	379566.125167	41.961178
3503.168751	379534.868745	41.966183
3503.289427	379494.674700	41.971188
3503.760661	379465.168279	41.976192
3503.206550	379429.447141	41.981197
3503.516249	379394.150233	41.986202
3503.789923	379361.119081	41.991207
3503.670035	379322.282772	41.996212
3503.761075	379279.426485	42.001216
3503.300815	379240.058924	42.006221
3503.380876	379202.588081	42.011226
3503.512060	379170.162963	42.016231
3503.737736	379133.685189	42.021236
3503.415038	379100.949680	42.026240
3503.434986	379066.814837	42.031245
3503.660106	379029.702113	42.036250
3503.539062	378990.560748	42.041255
3503.332124	378958.340361	42.046260
3503.534071	378915.237664	42.051264
3503.241757	378893.265022	42.056269
3503.335304	378848.883894	42.061274
3503.410240	378812.937055	42.066279
3503.023777	378786.483886	42.071284
3503.290717	378753.833966	42.076288
3503.179479	378720.379388	42.081293
3503.272124	378677.801236	42.086298
3503.591537	378660.583865	42.091303
3503.357173	378618.666011	42.096308
3503.786849	378580.682756	42.101312
3503.445693	378548.228795	42.106317
3503.663752	378499.942085	42.111322
3503.445240	378462.084922	42.116327
3503.233395	378430.956700	42.121332
3503.412593	378397.583502	42.126336
3503.331253	378362.777814	42.131341
3503.253166	378317.101894	42.136346
3502.663735	378297.943207	42.141351
3503.022673	378267.970401	42.146356
3503.263200	378235.806489	42.151360
3503.017863	378207.984766	42.156365
3503.218122	378176.106411	42.161370
3502.895716	378147.153771	42.166375
3502.819585	378115.013593	42.171380
3503.079222	378071.671983	42.176384
3502.877319	378052.935352	42.181389
3503.185075	378024.138485	42.186394
3503.254611	378000.737372	42.191399
3502.929848	377962.540479	42.196404
3502.980246	377914.608958	42.201408
3502.741148	377907.458967	42.206413
3503.014824	377870.057706	42.211418
3503.019064	377847.276146	42.216423
3502.864814	377819.592225	42.221428
3503.152349	377792.855406	42.226432
3503.099540	377762.920710	42.231437
3503.418020	377718.782064	42.236442
3502.824887	377693.071085	42.241447
3502.952779	377671.590779	42.246452
3502.908456	377657.832571	42.251456
3502.668682	377618.885445	42.256461
3502.692852	377579.795600	42.261466
3502.825784	377565.679599	42.266471
3502.496917	377540.054334	42.271476
3503.006226	377515.517681	42.276480
3502.804361	377491.472632	42.281485
3502.886313	377465.046847	42.286490
3502.927313	377435.909899	42.291495
3502.938970	377400.910704	42.296500
3503.285403	377374.138906	42.301504
3503.036908	377345.656445	42.306509
3503.197956	377312.818062	42.311514
3503.104676	377286.190793	42.316519
3503.147015	377257.866161	42.321524
3503.149982	377224.544321	42.326528
3503.171872	377196.121216	42.331533
3503.141396	377158.156751	42.336538
3503.063122	377120.707622	42.341543
3503.109522	377091.239291	42.346548
3503.176217	377071.774439	42.351552
3503.122748	377043.159718	42.356557
3503.199392	377007.286377	42.361562
3503.265777	376977.103675	42.366567
3502.961236	376936.844954	42.371572
3503.219855	376902.517817	42.376576
3502.805026	376877.845014	42.381581
3503.135560	376845.360653	42.386586
3502.858536	376817.237641	42.391591
3502.759883	376798.738043	42.396596
3503.007698	376761.593241	42.401600
3502.921732	376737.783460	42.406605
3503.000820	376700.512442	42.411610
3502.617223	376677.053697	42.416615
3502.466837	376649.494957	42.421620
3502.865997	376620.199798	42.426624
3502.890949	376598.734653	42.431629
3502.788277	376571.701768	42.436634
3503.064807	376555.632635	42.441639
3502.758325	376521.875513	42.446644
3503.136912	376490.983332	42.451648
3502.948634	376472.040289	42.456653
3503.090914	376436.613142	42.461658
3503.048459	376401.671863	42.466663
3502.728278	376373.504306	42.471668
3503.104376	376350.206440	42.476672
3502.685495	376323.171715	42.481677
3502.885386	376297.259796	42.486682
3502.883895	376265.004192	42.491687
3502.807039	376241.294148	42.496692
3503.022551	376204.204403	42.501696
3503.166644	376177.361309	42.506701
3503.021809	376141.318092	42.511706
3503.167186	376117.141582	42.516711
3502.995268	376098.627506	42.521716
3503.208013	376054.858166	42.526720
3502.990692	376028.579137	42.531725
3503.168019	375990.225109	42.536730
3503.230804	375958.517908	42.541735
3503.021048	375938.917468	42.546740
3502.842697	375894.014988	42.551744
3502.816349	375873.090623	42.556749
3503.137639	375839.031768	42.561754
3503.073843	375817.986194	42.566759
3502.872050	375787.691501	42.571764
3503.263238	375744.681256	42.576768
3502.970080	375717.423169	42.581773
3503.290240	375685.624800	42.586778
3503.046256	375655.971499	42.591783
3502.827876	375625.704604	42.596788
3503.079033	375592.342126	42.601792
3502.894656	375570.832543	42.606797
3503.502634	375544.348419	42.611802
3503.521410	375503.834056	42.616807
3503.173703	375474.018902	42.621812
3503.427244	375432.401136	42.626816
3503.247579	375404.083706	42.631821
3503.090823	375367.457133	42.636826
3503.295215	375333.415835	42.641831
3502.929135	375308.073628	42.646836
3503.129369	375276.242644	42.651840
3502.848619	375244.232477	42.656845
3502.774506	375215.034847	42.661850
3502.934847	375199.313183	42.666855
3502.652589	375163.340849	42.671860
3502.854864	375134.404916	42.676864
3502.546693	375116.241564	42.681869
3502.336054	375073.984296	42.686874
3502.543662	375057.061418	42.691879
3502.164926	375032.609907	42.696884
3502.319459	375012.799712	42.701888
3502.307142	374990.856501	42.706893
3502.978141	374968.298947	42.711898
3502.516251	374949.651413	42.716903
3502.712666	374931.561815	42.721908
3503.086551	374891.753270	42.726912
3502.811901	374868.479200	42.731917
3502.914193	374840.625301	42.736922
3502.849729	374816.556487	42.741927
3502.612074	374795.181579	42.746932
3502.871623	374752.012452	42.751936
3502.957553	374728.097955	42.756941
3503.135386	374706.175725	42.761946
3503.389416	374680.152240	42.766951
3502.718120	374638.931177	42.771956
3502.826854	374611.279241	42.776960
3503.033822	374584.297790	42.781965
3503.037960	374553.868077	42.786970
3502.468409	374529.852207	42.791975
3502.498220	374510.010256	42.796980
3502.946811	374481.289301	42.801985
3502.590333	374459.424618	42.806989
3502.979989	374425.581959	42.811994
3502.946446	374399.856958	42.816999
3502.520396	374382.803666	42.822004
3502.589008	374343.803832	42.827009
3502.563529	374319.398311	42.832013
3502.787899	374303.843970	42.837018
3502.760500	374270.193018	42.842023
3502.515444	374246.177204	42.847028
3502.625388	374216.975265	42.852033
3502.589819	374201.410514	42.857037
3502.897320	374170.501362	42.862042
3502.808210	374151.236463	42.867047
3502.766359	374121.194430	42.872052
3502.871442	374094.736359	42.877057
3502.776243	374076.310569	42.882061
3502.659308	374039.422011	42.887066
3502.769164	374013.013920	42.892071
3502.418035	373985.686918	42.897076
3502.448650	373962.491575	42.902081
3502.316388	373938.813546	42.907085
3502.426453	373925.943838	42.912090
3502.575087	373906.590970	42.917095
3502.454872	373883.241226	42.922100
3502.802540	373854.865529	42.927105
3502.628950	373832.717879	42.932109
3502.630799	373805.996188	42.937114
3502.634854	373787.072145	42.942119
3502.493758	373764.487571	42.947124
3502.892801	373730.185381	42.952129
3502.468217	373708.457699	42.957133
3502.626930	373688.137879	42.962138
3502.638463	373658.620449	42.967143
3502.323781	373649.118814	42.972148
3502.620629	373607.237523	42.977153
3502.703164	373591.857255	42.982157
3502.717509	373562.821902	42.987162
3502.844702	373534.886598	42.992167
3502.496729	373512.588019	42.997172
3502.794982	373489.706243	43.002177
3502.572569	373460.529817	43.007181
3502.404332	373431.167122	43.012186
3502.367728	373406.330702	43.017191
3502.537186	373397.668080	43.022196
3502.865014	373367.974113	43.027201
3502.464093	373339.917585	43.032205
3502.623861	373322.721669	43.037210
3502.870759	373299.619116	43.042215
3502.468263	373272.096187	43.047220
3502.545139	373248.842241	43.052225
3502.475835	373223.985344	43.057229
3502.783135	373209.179516	43.062234
3502.879587	373180.791415	43.067239
3502.655880	373156.822128	43.072244
3503.094806	373122.131956	43.077249
3502.550361	373095.011959	43.082253
3502.558387	373062.039852	43.087258
3502.481215	373038.962109	43.092263
3502.224342	373019.392304	43.097268
3502.964556	372995.349083	43.102273
3502.845649	372966.765661	43.107277
3502.514214	372949.772958	43.112282
3502.455959	372922.881952	43.117287
3502.582164	372884.709336	43.122292
3502.832430	372873.189002	43.127297
3502.601285	372842.285974	43.132301
3502.673858	372810.192578	43.137306
3502.847275	372792.740192	43.142311
3502.247411	372770.912037	43.147316
3502.778536	372735.876812	43.152321
3502.607976	372719.011342	43.157325
3502.847382	372698.678237	43.162330
3502.786802	372673.819488	43.167335
3502.789108	372648.798519	43.172340
3502.491844	372628.015438	43.177345
3502.345493	372598.496041	43.182349
3502.149024	372572.388256	43.187354
3502.266033	372549.991138	43.192359
3502.262614	372529.441678	43.197364
3502.148434	372494.023929	43.202369
3502.229970	372486.746406	43.207373
3502.211767	372460.001129	43.212378
3502.560884	372447.042728	43.217383
3502.226142	372422.709052	43.222388
3502.436070	372408.121165	43.227393
3502.655129	372395.335390	43.232397
3502.451528	372359.067716	43.237402
3502.890870	372333.140188	43.242407
3502.595338	372314.998414	43.247412
3502.556748	372282.794695	43.252417
3502.488221	372269.469366	43.257421
3502.524489	372237.584172	43.262426
3502.265960	372212.603399	43.267431
3502.249986	372192.741501	43.272436
3502.442051	372166.776090	43.277441
3502.444155	372152.626844	43.282445
3502.584129	372125.297781	43.287450
3502.582053	372103.807913	43.292455
3501.948736	372079.977639	43.297460
3502.455749	372059.145182	43.302465
3502.637292	372042.884969	43.307469
3502.129586	372017.307737	43.312474
3501.913513	372013.835947	43.317479
3501.653152	371996.882402	43.322484
3502.401396	371970.728651	43.327489
3502.106467	371973.187880	43.332493
3502.382918	371941.569800	43.337498
3502.650515	371919.809203	43.342503
3502.153182	371908.379403	43.347508
3502.400747	371872.599740	43.352513
3502.436796	371853.364566	43.357517
3502.401369	371847.984860	43.362522
3502.739778	371815.442506	43.367527
3502.284538	371799.205034	43.372532
3502.516664	371772.496348	43.377537
3502.330296	371747.122889	43.382541
3502.517620	371740.235150	43.387546
3502.862585	371702.433307	43.392551
3502.648208	371681.611216	43.397556
3502.709326	371649.746884	43.402561
3502.143122	371624.280004	43.407565
3502.087998	371612.933684	43.412570
3502.742180	371578.639935	43.417575
3502.422015	371557.427768	43.422580
3502.522810	371540.417744	43.427585
3502.625103	371520.409948	43.432589
3502.461848	371496.785456	43.437594
3502.537738	371476.375292	43.442599
3502.496618	371453.595454	43.447604
3502.606301	371425.787765	43.452609
3502.184317	371415.438360	43.457613
3502.484144	371389.404650	43.462618
3502.745910	371371.454970	43.467623
3502.504350	371348.299789	43.472628
3502.770964	371317.165189	43.477633
3502.540445	371300.714635	43.482637
3502.082554	371272.334637	43.487642
3502.514534	371247.169336	43.492647
3502.410342	371231.029322	43.497652
3502.565519	371203.824006	43.502657
3502.326128	371185.926790	43.507661
3502.204125	371166.156868	43.512666
3502.359628	371140.043773	43.517671
3502.059981	371124.899432	43.522676
3502.113876	371108.353701	43.527681
3501.809119	371086.859343	43.532685
3502.187894	371068.662632	43.537690
3502.832633	371049.764039	43.542695
3502.506870	371032.769277	43.547700
3502.367855	370997.302683	43.552705
3502.550626	370985.563443	43.557709
3502.594192	370963.506722	43.562714
3502.424760	370943.515394	43.567719
3502.167595	370908.829172	43.572724
3502.658947	370891.402331	43.577729
3502.475252	370877.255947	43.582733
3502.676452	370848.722149	43.587738
3502.831616	370818.925314	43.592743
3502.587512	370799.987044	43.597748
3502.385747	370771.388856	43.602753
3502.542805	370756.122440	43.607757
3502.599753	370731.726334	43.612762
3502.750356	370705.816824	43.617767
3502.431200	370680.844112	43.622772
3502.404415	370659.052135	43.627777
3502.027692	370638.432353	43.632781
3502.069264	370622.980607	43.637786
3502.273911	370593.658501	43.642791
3502.270379	370586.419124	43.647796
3502.209708	370563.489182	43.652801
3502.092897	370548.163656	43.657805
3502.208352	370525.384101	43.662810
3502.052394	370503.739122	43.667815
3502.098307	370489.201160	43.672820
3502.301434	370466.407914	43.677825
3502.110012	370458.994513	43.682829
3502.261991	370441.671012	43.687834
3502.341769	370416.102506	43.692839
3502.224288	370387.287581	43.697844
3502.132657	370373.939538	43.702849
3502.322122	370354.044364	43.707853
3502.218744	370336.277862	43.712858
3502.158445	370310.858077	43.717863
3501.813209	370306.644056	43.722868
3502.081652	370284.932867	43.727873
3501.735832	370279.270909	43.732877
3501.906995	370260.216846	43.737882
3502.136915	370236.174452	43.742887
3501.722318	370222.393920	43.747892
3502.767869	370204.372335	43.752897
3502.358035	370181.064548	43.757901
3502.399277	370171.506332	43.762906
3502.244010	370141.503047	43.767911
3502.189614	370121.721868	43.772916
3502.243717	370105.632786	43.777921
3502.127182	370099.350819	43.782925
3501.971491	370069.322118	43.787930
3502.124043	370053.471728	43.792935
3501.896321	370047.130839	43.797940
3501.643880	370017.828454	43.802945
3502.089407	370018.775399	43.807949
3502.067967	370001.122956	43.812954
3502.355373	369979.865856	43.817959
3501.958389	369965.752203	43.822964
3502.247104	369952.344774	43.827969
3501.963961	369932.980121	43.832973
3502.137293	369913.950891	43.837978
3502.310560	369889.815401	43.842983
3502.376749	369868.745067	43.847988
3502.340474	369858.081019	43.852993
3502.632658	369835.120980	43.857997
3502.190408	369812.097378	43.863002
3502.813501	369787.637758	43.868007
3502.336289	369766.499482	43.873012
3502.463046	369733.327137	43.878017
3502.695330	369715.025326	43.883021
3502.388799	369695.333893	43.888026
3502.531648	369663.124330	43.893031
3502.268337	369651.199906	43.898036
3502.549937	369623.236658	43.903041
3502.495542	369600.838450	43.908045
3502.249928	369579.689399	43.913050
3502.129475	369559.435419	43.918055
3502.155447	369538.548929	43.923060
3502.460550	369521.150227	43.928065
3502.471247	369503.771922	43.933069
3501.847579	369492.055935	43.938074
3502.033046	369454.860196	43.943079
3502.073780	369454.168041	43.948084
3502.157509	369436.397260	43.953089
3502.337853	369419.043314	43.958093
3501.986897	369404.464932	43.963098
3502.088068	369372.744213	43.968103
3501.836056	369370.497113	43.973108
3502.002074	369340.798646	43.978113
3502.209109	369332.865657	43.983117
3501.789691	369319.136242	43.988122
3502.194631	369300.070557	43.993127
3501.687084	369289.886108	43.998132
3501.860224	369273.854243	44.003137
3501.858205	369258.357723	44.008141
3501.813910	369255.011287	44.013146
3502.051249	369237.064049	44.018151
3501.778898	369223.159273	44.023156
3502.208112	369214.861414	44.028161
3502.223318	369183.230075	44.033165
3501.997634	369176.304360	44.038170
3502.181446	369159.864292	44.043175
3502.272357	369139.069022	44.048180
3502.358487	369116.496133	44.053185
3502.328048	369102.883918	44.058189
3502.183479	369090.737540	44.063194
3502.326235	369052.607936	44.068199
3502.177013	369043.663294	44.073204
3502.280598	369014.964997	44.078209
3502.472384	368994.789050	44.083213
3501.816796	368982.366476	44.088218
3502.485279	368958.712042	44.093223
3502.084845	368944.522199	44.098228
3502.177373	368921.363843	44.103233
3501.733249	368897.730063	44.108237
3501.906060	368884.975295	44.113242
3502.359225	368874.133094	44.118247
3502.178577	368853.024200	44.123252
3501.785964	368840.636856	44.128257
3501.905883	368822.885465	44.133261
3501.812241	368817.920722	44.138266
3501.977027	368795.919660	44.143271
3502.171438	368782.704190	44.148276
3502.347001	368768.805705	44.153281
3502.214137	368739.356362	44.158285
3502.260584	368731.600626	44.163290
3502.514417	368707.705646	44.168295
3502.183453	368691.523250	44.173300
3502.222527	368666.238956	44.178305
3502.416215	368646.621384	44.183309
3502.543257	368626.836332	44.188314
3502.560212	368596.067851	44.193319
3502.161476	368577.609448	44.198324
3502.238434	368557.679709	44.203329
3502.199132	368531.264246	44.208333
3502.076491	368519.749348	44.213338
3502.153817	368504.316286	44.218343
3502.138288	368488.796043	44.223348
3502.382513	368470.161301	44.228353
3502.596633	368452.420426	44.233357
3502.183363	368421.159782	44.238362
3502.283273	368409.406964	44.243367
3502.362187	368380.330782	44.248372
3502.576117	368360.354186	44.253377
3502.272615	368332.861803	44.258381
3501.995327	368324.470381	44.263386
3502.052424	368304.137065	44.268391
3502.449805	368284.487547	44.273396
3502.193445	368263.898112	44.278401
3502.111190	368247.498921	44.283405
3502.169706	368236.540050	44.288410
3502.229907	368208.254184	44.293415
3501.951662	368200.904511	44.298420
3501.983791	368177.297645	44.303425
3502.291981	368161.574414	44.308429
3502.059369	368154.547904	44.313434
3502.414110	368127.715067	44.318439
3502.014325	368112.229009	44.323444
3501.764724	368088.589692	44.328449
3502.337976	368066.981811	44.333453
3501.661563	368056.086423	44.338458
3502.159044	368035.989258	44.343463
3501.776185	368021.542159	44.348468
3501.695252	367997.266777	44.353473
3501.855366	367985.479010	44.358477
3501.651055	367994.250563	44.363482
3502.356553	367961.113121	44.368487
3501.654308	367959.139217	44.373492
3501.758711	367942.761617	44.378497
3502.075535	367921.981116	44.383501
3502.049335	367912.102357	44.388506
3502.101207	367893.497172	44.393511
3502.258459	367878.711892	44.398516
3502.268254	367860.519730	44.403521
3502.235931	367844.569847	44.408525
3502.379882	367824.984858	44.413530
3502.287414	367800.228388	44.418535
3502.481529	367773.648870	44.423540
3502.386384	367755.117285	44.428545
3502.340176	367727.685906	44.433549
3502.135068	367717.987357	44.438554
3502.094428	367695.992008	44.443559
3502.098308	367680.036400	44.448564
3502.056482	367667.390708	44.453569
3502.235327	367637.332783	44.458573
3502.006933	367629.721143	44.463578
3501.870174	367606.317930	44.468583
3502.081478	367595.080975	44.473588
3502.158178	367580.028607	44.478593
3502.258291	367557.401497	44.483597
3501.974626	367551.297411	44.488602
3502.075810	367522.166079	44.493607
3502.065982	367520.541709	44.498612
3502.160243	367494.790476	44.503617
3502.386487	367471.991233	44.508621
3501.597962	367468.125237	44.513626
3502.079066	367438.909294	44.518631
3501.999069	367430.207437	44.523636
3502.264090	367419.698842	44.528641
3502.041781	367407.767096	44.533645
3501.894838	367397.754510	44.538650
3501.994960	367363.770543	44.543655
3501.788934	367355.037462	44.548660
3502.044177	367349.255976	44.553665
3502.613482	367323.329040	44.558669
3501.831630	367309.604239	44.563674
3501.926649	367286.698236	44.568679
3502.233221	367273.337584	44.573684
3502.158242	367257.216166	44.578689
3502.298331	367237.504344	44.583693
3502.142494	367224.342659	44.588698
3502.340429	367194.484554	44.593703
3502.137266	367180.898300	44.598708
3502.375752	367161.526807	44.603713
3502.427137	367137.789055	44.608717
3502.280075	367127.141225	44.613722
3502.184418	367100.911057	44.618727
3502.431074	367075.669276	44.623732
3502.566720	367055.246630	44.628737
3502.431740	367033.519522	44.633741
3502.052545	367012.618013	44.638746
3502.382374	366983.272708	44.643751
3502.277244	366966.393613	44.648756
3501.690710	366955.433003	44.653761
3501.528137	366941.789506	44.658765
3501.957048	366932.347726	44.663770
3501.895697	366911.650752	44.668775
3502.129690	366899.520753	44.673780
3502.219610	366883.322651	44.678785
3502.132105	366871.318890	44.683789
3501.910208	366856.820748	44.688794
3502.166878	366833.355684	44.693799
3501.924998	366819.572028	44.698804
3502.078984	366806.082462	44.703809
3502.093591	366782.629617	44.708813
3502.069564	366765.788598	44.713818
3501.929431	366736.922687	44.718823
3502.122593	366735.800234	44.723828
3501.883512	366712.056517	44.728833
3502.184196	366704.362299	44.733837
3502.199743	366686.879898	44.738842
3502.154420	366669.889695	44.743847
3502.197043	366648.846059	44.748852
3502.112748	366626.932907	44.753857
3502.135849	366614.403684	44.758861
3502.107639	366594.590576	44.763866
3502.099886	366579.220533	44.768871
3501.920430	366549.623745	44.773876
3501.800491	366547.533717	44.778881
3501.847252	366530.427472	44.783885
3501.534945	366511.827250	44.788890
3501.987180	366492.371232	44.793895
3501.726735	366496.527850	44.798900
3501.952293	366469.866014	44.803905
3501.579015	366457.195146	44.808909
3501.725531	366450.795217	44.813914
3501.750038	366445.049457	44.818919
3502.079786	366420.226097	44.823924
3501.933076	366413.236606	44.828929
3502.066880	366393.880889	44.833933
3501.819444	366374.635299	44.838938
3502.178576	366364.314935	44.843943
3502.175693	366345.310751	44.848948
3502.104124	366333.710806	44.853953
3501.855197	366308.723325	44.858957
3501.932481	366292.501451	44.863962
3501.755384	366283.484060	44.868967
3501.705475	366270.432493	44.873972
3501.662320	366258.701058	44.878977
3501.683024	366249.220949	44.883981
3501.588799	366250.658540	44.888986
3501.579052	366226.192734	44.893991
3501.875078	366215.602654	44.898996
3501.845572	366206.231974	44.904001
3501.793524	366191.351361	44.909005
3501.661717	366180.726215	44.914010
3501.915379	366166.763504	44.919015
3501.625961	366161.701728	44.924020
3501.847960	366152.622192	44.929025
3502.096351	366125.651595	44.934029
3501.949972	366123.235352	44.939034
3501.868557	366089.455987	44.944039
3501.692925	366078.380286	44.949044
3501.393140	366078.350822	44.954049
3501.500164	366052.367646	44.959053
3501.200376	366051.474322	44.964058
3501.858894	366039.887686	44.969063
3501.623184	366039.060613	44.974068
3501.319228	366036.033691	44.979073
3501.831304	366005.058350	44.984077
3501.683688	366001.625981	44.989082
3501.913801	365988.530711	44.994087
3501.898659	365970.493683	44.999092
3501.970090	365972.083364	45.004097
3502.325343	365950.329970	45.009101
3501.965197	365934.074334	45.014106
3501.744085	365919.753454	45.019111
3501.985564	365914.456573	45.024116
3502.129769	365886.511062	45.029121
3501.824903	365873.092465	45.034125
3502.249460	365860.144735	45.039130
3501.890606	365845.667397	45.044135
3502.062793	365826.305328	45.049140
3501.763877	365812.326804	45.054145
3502.142645	365795.879882	45.059149
3501.966149	365783.914926	45.064154
3502.032220	365751.738324	45.069159
3502.141424	365749.307685	45.074164
3501.852671	365728.086276	45.079169
3501.871940	365718.860296	45.084173
3501.896401	365711.462880	45.089178
3502.155340	365687.818679	45.094183
3502.279870	365671.309618	45.099188
3502.067536	365655.132456	45.104193
3502.211004	365641.745618	45.109197
3502.038345	365616.872712	45.114202
3501.944362	365596.891301	45.119207
3501.691574	365595.330038	45.124212
3501.717686	365576.778184	45.129217
3501.788635	365561.014233	45.134221
3501.781348	365564.775875	45.139226
3501.591724	365552.025214	45.144231
3502.176518	365519.538963	45.149236
3502.017574	365523.934005	45.154241
3502.019820	365496.416741	45.159245
3501.794935	365479.174291	45.164250
3501.992463	365457.978645	45.169255
3501.869112	365442.651397	45.174260
3501.905912	365434.997908	45.179265
3502.061766	365428.240587	45.184269
3502.033463	365410.357708	45.189274
3501.916964	365397.900500	45.194279
3501.866437	365381.723415	45.199284
3501.782177	365358.869193	45.204289
3501.995297	365341.380645	45.209293
3501.642529	365327.816800	45.214298
3502.232983	365314.538113	45.219303
3502.305012	365307.082375	45.224308
3501.925548	365291.083468	45.229313
3501.971140	365268.463052	45.234317
3501.989253	365258.932206	45.239322
3502.196724	365237.912712	45.244327
3502.385443	365225.611201	45.249332
3502.078511	365198.878612	45.254337
3502.332339	365181.968027	45.259341
3502.045327	365165.116185	45.264346
3502.283690	365146.861339	45.269351
3502.161314	365126.096360	45.274356
3501.666765	365109.988219	45.279361
3502.128193	365086.972643	45.284365
3502.163587	365080.386438	45.289370
3502.144295	365066.287816	45.294375
3502.295242	365044.921259	45.299380
3501.715322	365032.078655	45.304385
3502.021715	365011.221464	45.309389
3501.729003	364998.791506	45.314394
3501.550369	364982.380048	45.319399
3502.072268	364971.881412	45.324404
3501.573087	364950.209416	45.329409
3501.955478	364935.235148	45.334413
3501.604616	364936.179158	45.339418
3501.747059	364917.862869	45.344423
3501.816864	364907.002614	45.349428
3501.795632	364908.124008	45.354433
3502.049701	364888.113358	45.359437
3501.734770	364875.635988	45.364442
3501.753823	364858.990429	45.369447
3501.914140	364846.794813	45.374452
3501.986165	364833.240861	45.379457
3502.085838	364812.364879	45.384461
3501.689178	364794.996302	45.389466
3501.600658	364785.024538	45.394471
3501.956723	364772.112393	45.399476
3501.723114	364765.339298	45.404481
3502.185368	364738.054642	45.409485
3501.840133	364743.444325	45.414490
3501.787701	364723.227170	45.419495
3501.940947	364697.261002	45.424500
3501.931251	364696.246266	45.429505
3501.866894	364664.114169	45.434509
3501.624274	364664.024988	45.439514
3501.757270	364647.158307	45.444519
3501.806351	364632.388204	45.449524
3501.437259	364622.688725	45.454529
3501.646075	364612.060818	45.459533
3501.856565	364605.066125	45.464538
3502.151265	364591.020048	45.469543
3502.267898	364575.477137	45.474548
3501.963968	364564.547868	45.479553
3501.841437	364532.754997	45.484557
3501.824270	364525.744893	45.489562
3501.797670	364507.073518	45.494567
3501.543774	364483.304875	45.499572
3501.641375	364482.273434	45.504577
3501.824106	364475.842029	45.509581
3501.950593	364463.270383	45.514586
3502.033683	364443.286036	45.519591
3502.432671	364432.628471	45.524596
3501.810676	364407.113002	45.529601
3501.774886	364395.481307	45.534605
3501.889177	364386.367166	45.539610
3502.163419	364367.877569	45.544615
3501.860748	364359.666806	45.549620
3501.642902	364338.814488	45.554625
3502.025509	364323.407918	45.559629
3501.855086	364328.084426	45.564634
3502.026851	364292.993125	45.569639
3502.065942	364281.629233	45.574644
3501.631615	364274.175800	45.579649
3502.003662	364247.616184	45.584653
3501.985420	364246.247033	45.589658
3502.014945	364233.080555	45.594663
3502.094682	364211.953156	45.599668
3502.143780	364195.404182	45.604673
3502.007527	364175.352148	45.609677
3501.965847	364160.672159	45.614682
3501.894931	364146.022123	45.619687
3502.019525	364129.385135	45.624692
3501.977590	364117.830515	45.629697
3501.958401	364098.293808	45.634701
3502.118536	364088.206884	45.639706
3502.207838	364079.350631	45.644711
3502.046313	364056.634462	45.649716
3501.829660	364043.861940	45.654721
3501.801231	364018.380813	45.659725
3501.717776	364007.874397	45.664730
3501.602416	364005.351512	45.669735
3501.924404	363989.064870	45.674740
3501.465945	363973.179171	45.679745
3501.678035	363965.599659	45.684749
3501.819939	363957.954839	45.689754
3501.816189	363939.813146	45.694759
3501.817695	363912.904337	45.699764
3502.038634	363918.155248	45.704769
3502.298933	363886.556199	45.709773
3502.002597	363885.738497	45.714778
3501.968573	363862.722832	45.719783
3501.657641	363841.376455	45.724788
3501.935275	363831.804761	45.729793
3501.732221	363818.877567	45.734797
3501.687069	363799.802075	45.739802
3501.618876	363783.194892	45.744807
3501.752200	363781.370169	45.749812
3501.785567	363761.393097	45.754817
3501.791367	363731.129377	45.759821
3501.589827	363686.388940	45.764826
3501.359509	363584.938259	45.769831
3500.943769	363422.557661	45.774836
3500.562341	363248.253494	45.779841
3499.943540	363013.127613	45.784845
3499.684631	362754.286670	45.789850
3498.956529	362428.991064	45.794855
3498.040650	362068.425104	45.799860
3497.558206	361673.126139	45.804865
3496.573666	361238.816733	45.809869
3495.441314	360760.840466	45.814874
3494.042033	360249.785483	45.819879
3493.003952	359703.671822	45.824884
3491.349579	359140.261357	45.829889
3489.822071	358520.274426	45.834893
3488.384294	357871.745780	45.839898
3486.802454	357199.996420	45.844903
3485.259393	356496.075522	45.849908
3483.004547	355753.972439	45.854913
3481.747892	354994.514548	45.859917
3479.636861	354201.238787	45.864922
3477.714905	353376.115484	45.869927
3475.578966	352530.719809	45.874932
3472.990983	351665.875358	45.879937
3470.769535	350765.743573	45.884941
3468.454199	349861.584985	45.889946
3466.036823	348913.895298	45.894951
3463.580421	347964.099863	45.899956
3461.331564	346988.237078	45.904961
3458.961448	345982.872974	45.909965
3456.188723	344967.422619	45.914970
3453.401665	343930.154628	45.919975
3451.020246	342874.383645	45.924980
3448.044297	341810.460173	45.929985
3445.069678	340726.543367	45.934989
3442.443244	339623.035440	45.939994
3439.303795	338521.938234	45.944999
3436.728140	337395.543820	45.950004
3433.633733	336261.260885	45.955009
3430.792363	335108.440192	45.960013
3427.397180	333953.381073	45.965018
3424.667791	332776.488256	45.970023
3421.754970	331589.897191	45.975028
3418.001777	330395.312017	45.980033
3415.126857	329197.679285	45.985037
3411.873913	327981.118785	45.990042
3408.827757	326753.907076	45.995047
3405.713430	325530.636988	46.000052
3402.345535	324299.381946	46.005057
3399.113772	323053.186927	46.010061
3395.728888	321796.904301	46.015066
3392.244497	320533.171185	46.020071
3389.007146	319276.766066	46.025076
3385.336542	318007.416462	46.030081
3381.977171	316723.352086	46.035085
3378.729071	315450.505304	46.040090
3375.172772	314177.034730	46.045095
3371.965221	312878.283770	46.050100
3368.390261	311591.004704	46.055105
3365.027868	310291.036075	46.060109
3361.571030	308999.673815	46.065114
3357.383679	307694.725549	46.070119
3354.454863	306395.298658	46.075124
3350.423864	305093.515864	46.080129
3347.213019	303778.821987	46.085133
3343.189856	302473.052871	46.090138
3339.625563	301168.325599	46.095143
3336.317182	299862.636224	46.100148
3332.539547	298552.636526	46.105153
3328.910921	297231.510907	46.110157
3325.353868	295920.779613	46.115162
3321.566972	294610.639999	46.120167
3317.975315	293292.753680	46.125172
3314.333244	291978.257492	46.130177
3310.921572	290672.810645	46.135181
3307.052816	289361.501928	46.140186
3303.208864	288047.820515	46.145191
3299.897736	286728.225548	46.150196
3295.864637	285420.249390	46.155201
3292.405078	284104.190480	46.160205
3288.898902	282781.316538	46.165210
3284.991947	281474.265351	46.170215
3281.582955	280162.963406	46.175220
3277.562850	278851.682729	46.180225
3274.201399	277537.094608	46.185229
3270.399005	276224.615545	46.190234
3266.814749	274914.245478	46.195239
3263.144868	273603.664373	46.200244
3259.356430	272302.120718	46.205249
3255.324938	270990.308651	46.210253
3251.549198	269690.736382	46.215258
3247.745466	268385.471962	46.220263
3244.071498	267077.826902	46.225268
3239.834001	265792.889803	46.230273
3236.284993	264490.029769	46.235277
3232.980407	263213.267852	46.240282
3229.147548	261917.474451	46.245287
3225.553909	260617.248930	46.250292
3221.768362	259332.572837	46.255297
3218.235852	258054.999698	46.260301
3214.214509	256771.938121	46.265306
3210.569389	255479.535758	46.270311
3206.671775	254201.956600	46.275316
3202.938088	252932.006065	46.280321
3199.509648	251658.737526	46.285325
3195.453793	250386.396761	46.290330
3191.538348	249109.491192	46.295335
3187.987983	247849.786490	46.300340
3184.075642	246585.316136	46.305345
3180.974901	245323.614670	46.310349
3177.232335	244068.245124	46.315354
3173.267067	242809.133881	46.320359
3169.318815	241545.785634	46.325364
3165.316033	240301.999444	46.330369
3161.618574	239040.714295	46.335373
3158.012060	237804.063443	46.340378
3154.334119	236546.738604	46.345383
3150.669051	235306.497142	46.350388
3147.084187	234081.011536	46.355393
3143.179801	232844.366269	46.360397
3139.417931	231604.079575	46.365402
3135.678028	230372.268438	46.370407
3132.374116	229137.484266	46.375412
3128.444100	227913.620611	46.380417
3124.858233	226678.929190	46.385421
3120.831259	225454.340879	46.390426
3116.832180	224231.607577	46.395431
3113.394383	223016.402729	46.400436
3109.477405	221813.498567	46.405441
3105.500502	220600.926908	46.410445
3101.751885	219394.179433	46.415450
3097.749769	218182.787393	46.420455
3094.023863	216974.487753	46.425460
3090.309753	215786.284264	46.430465
3087.292960	214597.084299	46.435469
3083.065700	213407.592655	46.440474
3079.498980	212223.631033	46.445479
3075.873241	211030.794763	46.450484
3071.751328	209849.628897	46.455489
3068.358663	208656.588686	46.460493
3064.254906	207488.216267	46.465498
3060.783149	206318.783817	46.470503
3057.638414	205153.356352	46.475508
3053.021694	203989.794721	46.480513
3049.756189	202815.588381	46.485517
3045.946953	201657.773439	46.490522
3042.050213	200500.234688	46.495527
3038.577479	199345.006655	46.500532
3034.592766	198191.471320	46.505537
3031.116228	197042.424382	46.510541
3027.663475	195894.681799	46.515546
3023.563008	194756.523017	46.520551
3019.553195	193608.657463	46.525556
3015.511562	192483.726286	46.530561
3012.042262	191346.238310	46.535565
3008.082330	190220.958984	46.540570
3004.244293	189105.246499	46.545575
3000.446503	187990.990401	46.550580
2996.910059	186870.975626	46.555585
2993.227914	185759.780573	46.560589
2989.438441	184655.489538	46.565594
2985.773523	183558.015613	46.570599
2982.395369	182459.567363	46.575604
2978.128818	181367.839587	46.580609
2974.461700	180261.339544	46.585613
2970.626390	179175.631094	46.590618
2966.817752	178099.378336	46.595623
2962.921026	177016.812844	46.600628
2959.163710	175951.336935	46.605633
2955.215907	174871.251700	46.610637
2951.566984	173825.035368	46.615642
2947.745036	172760.604825	46.620647
2943.958682	171715.609405	46.625652
2939.963576	170676.911259	46.630657
2936.587164	169628.151357	46.635661
2932.601934	168585.700554	46.640666
2928.035429	167565.860756	46.645671
2924.378118	166522.803759	46.650676
2920.285358	165522.052009	46.655681
2916.433459	164516.313363	46.660685
2912.499752	163514.357530	46.665690
2908.674707	162524.822923	46.670695
2904.908117	161536.809032	46.675700
2900.753589	160561.382411	46.680705
2897.161039	159586.481737	46.685709
2892.975778	158625.065326	46.690714
2888.775834	157667.128236	46.695719
2885.308680	156720.165009	46.700724
2881.263689	155794.382636	46.705729
2877.271300	154866.175972	46.710733
2873.293317	153939.763746	46.715738
2869.059859	153027.188961	46.720743
2865.724933	152117.365291	46.725748
2861.077253	151223.350053	46.730753
2856.957598	150328.032861	46.735757
2853.011521	149452.606107	46.740762
2848.875805	148589.783030	46.745767
2844.570737	147741.608754	46.750772
2840.546523	146902.171956	46.755777
2836.368141	146068.753357	46.760781
2832.349063	145254.181158	46.765786
2827.836438	144455.095190	46.770791
2824.199853	143662.540300	46.775796
2819.759696	142898.840806	46.780801
2815.676227	142123.391912	46.785805
2811.314987	141386.525158	46.790810
2807.058301	140557.219049	46.795815
2803.068105	139815.674657	46.800820
2798.655296	139109.538935	46.805825
2794.376855	138409.499777	46.810829
2790.295931	137717.862654	46.815834
2786.250095	137044.003419	46.820839
2782.165312	136374.345698	46.825844
2777.831583	135734.365871	46.830849
2773.951696	135094.120922	46.835853
2770.461697	134458.938483	46.840858
2766.043612	133848.309099	46.845863
2762.520732	133225.311030	46.850868
2757.937351	132625.015732	46.855873
2754.799198	132030.520730	46.860877
2750.917865	131439.304240	46.865882
2747.040273	130869.440264	46.870887
2743.633510	130286.879295	46.875892
2739.763547	129716.825960	46.880897
2735.893432	129156.790946	46.885901
2732.463669	128588.490562	46.890906
2728.485453	128033.842382	46.895911
2725.304797	127481.913915	46.900916
2721.492373	126937.404722	46.905921
2717.895848	126388.671809	46.910925
2714.311926	125839.193866	46.915930
2710.625603	125303.539173	46.920935
2707.657827	124754.730419	46.925940
2703.907349	124220.817077	46.930945
2700.499846	123673.452390	46.935949
2696.608769	123141.317752	46.940954
2693.157487	122604.467043	46.945959
2689.697827	122070.600902	46.950964
2686.118246	121547.392604	46.955969
2682.568785	121008.378857	46.960973
2678.632220	120475.015705	46.965978
2675.120655	119957.769907	46.970983
2672.329187	119422.271969	46.975988
2668.262227	118906.067833	46.980993
2664.950044	118383.013459	46.985997
2661.368479	117853.421139	46.991002
2657.919935	117334.102967	46.996007
2654.553514	116808.726372	47.001012
2650.932232	116289.487723	47.006017
2647.171868	115769.782062	47.011021
2643.710834	115243.831961	47.016026
2639.787317	114725.933849	47.021031
2636.586840	114205.387513	47.026036
2632.693081	113688.186095	47.031041
2629.131846	113176.471227	47.036045
2625.686368	112657.409273	47.041050
2622.294854	112149.509666	47.046055
2618.755202	111641.042749	47.051060
2614.828839	111130.736161	47.056065
2611.255414	110627.578039	47.061069
2608.011476	110128.940024	47.066074
2604.157200	109623.373491	47.071079
2600.730190	109124.727383	47.076084
2596.806846	108630.831371	47.081089
2592.802106	108127.115224	47.086093
2588.900520	107643.857940	47.091098
2585.234958	107168.808481	47.096103
2581.519950	106687.747610	47.101108
2577.993224	106211.380462	47.106113
2574.477620	105748.493057	47.111117
2570.376822	105282.436090	47.116122
2566.482983	104824.526997	47.121127
2562.554481	104363.184710	47.126132
2559.110776	103918.526938	47.131137
2555.384569	103473.029273	47.136141
2551.955021	103033.300364	47.141146
2548.021916	102591.304149	47.146151
2544.181924	102155.070029	47.151156
2540.500338	101732.010592	47.156161
2536.667945	101299.104125	47.161165
2533.167080	100877.692679	47.166170
2529.445849	100463.171705	47.171175
2526.043237	100035.591525	47.176180
2522.285545	99625.268511	47.181185
2518.753470	99214.292848	47.186189
2515.570277	98806.928461	47.191194
2511.662213	98393.136812	47.196199
2508.308674	97972.617396	47.201204
2504.708011	97570.023426	47.206209
2501.349205	97171.997501	47.211213
2498.081780	96759.245834	47.216218
2494.230674	96353.300456	47.221223
2491.289638	95935.374617	47.226228
2487.545495	95539.221203	47.231233
2484.095098	95120.623052	47.236237
2480.933735	94707.195732	47.241242
2477.360724	94291.537921	47.246247
2474.024919	93872.760891	47.251252
2470.617093	93461.917372	47.256257
2467.204582	93044.078492	47.261261
2463.608242	92623.097208	47.266266
2459.757616	92216.697788	47.271271
2456.789690	91792.453517	47.276276
2453.155242	91374.329020	47.281281
2449.633043	90949.179029	47.286285
2446.317028	90544.713748	47.291290
2442.564646	90130.347744	47.296295
2439.592201	89699.196280	47.301300
2436.092959	89281.550007	47.306305
2432.368491	88860.336348	47.311309
2429.370506	88434.174968	47.316314
2425.554188	88013.013074	47.321319
2422.390736	87589.659317	47.326324
2418.694691	87158.543127	47.331329
2414.990886	86717.931623	47.336333
2411.517695	86299.396163	47.341338
2408.185519	85868.725160	47.346343
2404.933094	85439.572599	47.351348
2401.261184	85013.337301	47.356353
2397.881673	84582.286310	47.361357
2394.451379	84148.836072	47.366362
2390.646694	83720.544582	47.371367
2387.534334	83279.868107	47.376372
2383.631593	82857.155997	47.381377
2380.108979	82412.415745	47.386381
2376.805778	81982.573509	47.391386
2373.605418	81553.572857	47.396391
2370.178932	81110.349720	47.401396
2366.578428	80678.363557	47.406401
2363.118756	80232.822368	47.411405
2359.819117	79799.482032	47.416410
2355.874068	79361.054153	47.421415
2352.644954	78917.860573	47.426420
2349.155603	78484.925953	47.431425
2345.478058	78040.025473	47.436429
2342.440784	77594.181644	47.441434
2338.605568	77147.516754	47.446439
2334.832307	76707.161366	47.451444
2331.430889	76268.964980	47.456449
2327.899740	75828.929046	47.461453
2324.770519	75386.767746	47.466458
2320.869026	74942.879824	47.471463
2317.610780	74494.124372	47.476468
2314.422517	74062.445175	47.481473
2310.885548	73612.579610	47.486477
2307.197654	73160.815006	47.491482
2303.591348	72714.645196	47.496487
2300.519809	72264.133232	47.501492
2296.757853	71820.453401	47.506497
2293.350747	71370.732686	47.511501
2290.123401	70925.283324	47.516506
2285.844978	70474.678773	47.521511
2282.668343	70031.223823	47.526516
2279.244886	69582.641035	47.531521
2275.664053	69126.466406	47.536525
2272.097808	68681.558915	47.541530
2268.805707	68225.494920	47.546535
2265.343147	67782.376934	47.551540
2261.921064	67327.777362	47.556545
2258.319770	66874.178591	47.561549
2254.661959	66420.641120	47.566554
2251.463428	65969.598240	47.571559
2248.130007	65510.225086	47.576564
2244.698058	65059.951977	47.581569
2241.176046	64605.321502	47.586573
2237.730204	64144.086647	47.591578
2233.623702	63686.529977	47.596583
2230.181092	63223.007725	47.601588
2227.073542	62773.271031	47.606593
2223.195569	62316.694017	47.611597
2219.968280	61855.784830	47.616602
2216.500782	61397.479134	47.621607
2213.003247	60943.914452	47.626612
2209.373453	60490.264502	47.631617
2205.523427	60029.213579	47.636621
2202.326840	59565.569459	47.641626
2198.668724	59122.184946	47.646631
2195.492175	58651.625749	47.651636
2192.038970	58204.634587	47.656641
2188.236643	57743.340437	47.661645
2185.217001	57279.915572	47.666650
2181.492813	56814.680418	47.671655
2178.042123	56350.610915	47.676660
2174.524243	55898.019476	47.681665
2171.097910	55431.413480	47.686669
2167.703090	54959.520442	47.691674
2164.378879	54499.883120	47.696679
2160.976976	54027.242111	47.701684
2157.414190	53565.909105	47.706689
2153.791926	53095.021341	47.711693
2150.191906	52618.334950	47.716698
2146.676662	52155.024013	47.721703
2143.345116	51687.849477	47.726708
2139.834156	51218.828243	47.731713
2136.204302	50740.846485	47.736717
2132.799527	50274.980496	47.741722
2128.997937	49818.947695	47.746727
2126.139522	49332.977929	47.751732
2122.215512	48863.935699	47.756737
2118.695220	48390.121299	47.761741
2115.378856	47910.912859	47.766746
2111.664318	47449.947549	47.771751
2108.389800	46983.437039	47.776756
2104.528964	46505.712969	47.781761
2101.510749	46025.286675	47.786765
2097.975492	45553.607798	47.791770
2094.102937	45087.629166	47.796775
2090.641682	44603.763556	47.801780
2087.110401	44140.567249	47.806785
2083.884852	43666.622435	47.811789
2080.659930	43186.340072	47.816794
2076.790486	42714.424537	47.821799
2073.448426	42229.659989	47.826804
2069.955824	41763.799810	47.831809
2066.311689	41282.038964	47.836813
2063.215016	40797.426355	47.841818
2059.207738	40325.678717	47.846823
2055.600468	39845.078756	47.851828
2052.095752	39366.451582	47.856833
2048.577178	38887.101696	47.861837
2045.431459	38409.834598	47.866842
2041.811005	37932.759722	47.871847
2038.486280	37458.318361	47.876852
2034.918915	36988.324814	47.881857
2031.408312	36498.883845	47.886861
2027.943200	36016.857468	47.891866
2024.369658	35546.205682	47.896871
2020.744757	35063.699652	47.901876
2017.164273	34580.804706	47.906881
2013.699860	34099.214818	47.911885
2010.240795	33629.132998	47.916890
2006.540479	33147.817109	47.921895
2003.230399	32655.746442	47.926900
1999.772776	32188.802384	47.931905
1995.980242	31701.468698	47.936909
1992.593788	31240.042416	47.941914
1988.735696	30756.011366	47.946919
1985.543586	30280.094921	47.951924
1982.002453	29808.584786	47.956929
1978.343332	29329.100039	47.961933
1975.099681	28856.659221	47.966938
1971.290175	28382.644440	47.971943
1967.654907	27902.181816	47.976948
1964.540481	27432.180749	47.981953
1960.818489	26954.934903	47.986957
1957.810153	26472.475880	47.991962
1954.111441	26005.196648	47.996967
1950.458343	25522.993685	48.001972
1946.794083	25049.845155	48.006977
1943.590453	24573.335214	48.011981
1939.743191	24094.782709	48.016986
1936.248871	23617.941612	48.021991
1932.922266	23148.048167	48.026996
1928.894837	22677.216939	48.032001
1925.275567	22202.773157	48.037005
1921.837362	21730.200307	48.042010
1918.149147	21267.160524	48.047015
1914.421137	20794.300452	48.052020
1910.768936	20333.937471	48.057025
1907.165858	19868.485011	48.062029
1904.009973	19415.109914	48.067034
1900.324683	18959.908584	48.072039
1896.709068	18500.039122	48.077044
1892.838347	18049.587534	48.082049
1889.378078	17593.369814	48.087053
1885.689130	17146.929456	48.092058
1881.306901	16718.567975	48.097063
1877.571764	16286.530858	48.102068
1873.174148	15873.747494	48.107073
1869.098264	15464.342592	48.112077
1865.205051	15052.660462	48.117082
1861.303621	14657.142472	48.122087
1857.776903	14258.009291	48.127092
1853.859214	13877.150275	48.132097
1849.932035	13498.997819	48.137101
1846.097736	13117.757979	48.142106
1842.286044	12746.814608	48.147111
1839.238980	12372.957760	48.152116
1835.588911	12009.880299	48.157121
1831.874435	11646.452643	48.162125
1828.235328	11276.438912	48.167130
1824.638590	10937.720849	48.172135
1821.245593	10568.736926	48.177140
1817.581004	10207.285707	48.182145
1813.856515	9857.239932	48.187149
1810.360615	9502.461456	48.192154
1807.015254	9161.520768	48.197159
1803.501042	8805.568298	48.202164
1799.978173	8465.332728	48.207169
1796.352734	8119.798829	48.212173
1793.228240	7774.747310	48.217178
1789.439499	7427.912962	48.222183
1786.006946	7087.426035	48.227188
1782.644448	6742.712570	48.232193
1778.812636	6414.133720	48.237197
1775.256644	6068.428149	48.242202
1771.832325	5731.443177	48.247207
1768.221462	5394.148509	48.252212
1764.584231	5066.063618	48.257217
1760.824717	4728.491113	48.262221
1757.079786	4400.808396	48.267226
1753.820711	4077.226668	48.272231
1750.419087	3757.441647	48.277236
1746.814765	3434.681411	48.282241
1742.874649	3111.909590	48.287245
1739.404717	2790.810668	48.292250
1735.714250	2480.392759	48.297255
1731.816182	2164.320346	48.302260
1728.440436	1861.426284	48.307265
1724.400045	1557.131569	48.312269
1720.828130	1249.633674	48.317274
1716.720148	970.629651	48.322279
1712.789418	679.592564	48.327284
1709.070034	408.585593	48.332289
1704.443611	156.959327	48.337293
1698.173125	-52.760816	48.342298
1682.332664	41.227140	48.347303
1672.186619	56.979774	48.352308
1667.683260	56.111597	48.357313
1665.054663	63.408205	48.362317
1664.156161	60.836866	48.367322
1662.782839	64.227078	48.372327
1660.732481	58.468837	48.377332
1658.408467	62.554338	48.382337
1655.164008	66.071266	48.387341
1652.063332	64.263450	48.392346
1648.424138	71.097267	48.397351
1644.910912	66.775244	48.402356
1642.440189	59.174718	48.407361
1638.868139	58.215377	48.412365
1635.355272	61.277380	48.417370
1632.120581	66.286057	48.422375
1628.667289	67.937269	48.427380
1625.246130	58.576962	48.432385
1621.094729	61.298595	48.437389
1618.214480	60.731447	48.442394
1614.107543	73.734519	48.447399
1611.346492	72.987470	48.452404
1608.060339	68.494069	48.457409
1604.682342	60.750026	48.462413
1601.755554	64.299770	48.467418
1598.682477	61.165237	48.472423
1594.861564	64.430210	48.477428
1591.419284	68.196227	48.482433
1587.900307	64.359153	48.487437
1584.433393	55.860176	48.492442
1580.847920	67.772862	48.497447
1577.562155	67.360579	48.502452
1573.938002	64.874959	48.507457
1570.256110	71.316799	48.512461
1567.105900	67.472950	48.517466
1563.560308	71.916262	48.522471
1560.112675	76.205127	48.527476
1556.819646	68.093528	48.532481
1553.208715	73.148115	48.537485
1549.887085	71.501247	48.542490
1546.746885	71.581994	48.547495
1542.776427	71.412323	48.552500
1539.456061	61.530150	48.557505
1535.930931	65.296410	48.562509
1532.298338	63.451176	48.567514
1529.047531	59.445824	48.572519
1525.393498	61.862266	48.577524
1522.374505	57.763888	48.582529
1518.451543	60.696743	48.587533
1515.563837	54.164031	48.592538
1512.154544	68.437886	48.597543
1508.495954	65.888032	48.602548
1504.889164	59.173018	48.607553
1501.100176	66.397142	48.612557
1497.908954	56.893504	48.617562
1494.499033	68.260019	48.622567
1490.594560	61.613486	48.627572
1487.218985	55.042819	48.632577
1483.802766	68.998218	48.637581
1480.529235	61.465721	48.642586
1477.066681	66.430778	48.647591
1473.228241	56.164193	48.652596
1469.894152	56.550367	48.657601
1466.548004	53.537446	48.662605
1463.102855	60.856746	48.667610
1459.701338	58.295360	48.672615
1456.007135	55.459998	48.677620
1452.860033	59.695761	48.682625
1448.824003	59.194628	48.687629
1445.825555	57.266520	48.692634
1442.294285	56.671005	48.697639
1438.163641	60.218312	48.702644
1435.098466	66.456600	48.707649
1431.410595	61.339229	48.712653
1428.097839	58.400206	48.717658
1424.676117	62.884355	48.722663
1420.921029	65.259589	48.727668
1417.967242	53.804974	48.732673
1414.394524	52.478773	48.737677
1410.861844	56.651168	48.742682
1407.161258	67.911067	48.747687
1403.848542	57.046984	48.752692
1400.221824	56.760553	48.757697
1396.569821	54.092634	48.762701
1393.319268	59.062660	48.767706
1389.652310	58.070662	48.772711
1386.184375	62.198182	48.777716
1383.173984	52.764495	48.782721
1379.299930	55.113956	48.787725
1375.883165	52.611901	48.792730
1372.025946	58.242657	48.797735
1368.837637	53.844791	48.802740
1365.514429	47.519091	48.807745
1361.559842	55.847812	48.812749
1358.050769	61.658494	48.817754
1354.707779	58.145230	48.822759
1351.135554	63.652537	48.827764
1348.024323	57.613374	48.832769
1344.174995	64.910171	48.837773
1341.241780	52.930359	48.842778
1337.388848	59.924001	48.847783
1333.621034	68.524209	48.852788
1330.465406	61.223316	48.857793
1326.556292	70.984448	48.862797
1323.453977	61.669476	48.867802
1320.170025	64.154879	48.872807
1316.576575	62.420635	48.877812
1313.140248	56.280222	48.882817
1309.410508	60.802830	48.887821
1306.164755	59.375129	48.892826
1302.217943	54.022844	48.897831
1298.349098	60.674123	48.902836
1294.890795	53.382387	48.907841
1291.488362	56.961888	48.912845
1288.297547	54.487948	48.917850
1285.056919	61.167992	48.922855
1281.581894	65.777504	48.927860
1278.522063	61.280559	48.932865
1274.274075	67.212588	48.937869
1270.815615	59.759529	48.942874
1267.252055	68.558896	48.947879
1263.930388	62.036817	48.952884
1260.316869	60.596763	48.957889
1256.807633	71.943939	48.962893
1253.359921	65.153583	48.967898
1250.148537	64.049562	48.972903
1246.806588	58.115927	48.977908
1242.968940	62.693301	48.982913
1238.885676	63.629534	48.987917
1235.701078	62.448580	48.992922
1232.361880	62.269272	48.997927
1228.731533	58.958937	49.002932
1225.780746	56.137601	49.007937
1222.171616	64.093028	49.012941
1218.505760	55.419441	49.017946
1214.889310	58.440651	49.022951
1211.349400	60.703317	49.027956
1207.842547	54.747902	49.032961
1204.221620	63.654272	49.037965
1200.876103	53.007304	49.042970
1197.451313	54.008723	49.047975
1193.571447	62.977544	49.052980
1190.672846	46.477794	49.057985
1186.975290	52.770228	49.062989
1183.726918	50.580501	49.067994
1180.208298	47.993087	49.072999
1176.462353	54.024141	49.078004
1172.960514	51.750484	49.083009
1169.277936	64.510332	49.088013
1165.811503	58.051932	49.093018
1162.418660	54.103538	49.098023
1158.630152	50.662813	49.103028
1155.484273	52.579419	49.108033
1151.771158	63.259150	49.113037
1148.526301	52.583870	49.118042
1144.942327	54.353538	49.123047
1141.494771	57.955893	49.128052
1137.943873	56.746548	49.133057
1134.308099	62.504199	49.138061
1130.651021	48.941369	49.143066
1127.471047	53.982678	49.148071
1123.830022	59.415287	49.153076
1120.653239	58.290077	49.158081
1116.684969	56.965371	49.163085
1113.438894	55.458650	49.168090
1109.932107	57.507366	49.173095
1106.212785	57.709936	49.178100
1102.911215	52.475542	49.183105
1099.256581	56.711234	49.188109
1095.991258	53.325118	49.193114
1092.836723	57.701261	49.198119
1088.840084	50.869836	49.203124
1085.367826	48.053760	49.208129
1081.239265	55.893895	49.213133
1078.394424	53.590748	49.218138
1074.778961	51.891599	49.223143
1071.286943	61.938980	49.228148
1067.952228	54.343313	49.233153
1064.217852	54.753871	49.238157
1060.638149	50.113259	49.243162
1057.879303	48.726852	49.248167
1054.105116	48.140721	49.253172
1050.899745	46.937713	49.258177
1046.848004	58.495876	49.263181
1043.490059	55.092547	49.268186
1040.088888	55.546152	49.273191
1036.664832	57.945821	49.278196
1032.733309	46.311292	49.283201
1029.007389	54.806910	49.288205
1025.799065	41.357751	49.293210
1022.175547	48.613083	49.298215
1018.813778	49.807186	49.303220
1015.102822	52.580538	49.308225
1011.458543	62.116959	49.313229
1008.315585	64.077415	49.318234
1004.833582	48.212674	49.323239
1001.187651	57.119777	49.328244
998.147069	52.762241	49.333249
994.470567	59.313998	49.338253
990.989564	54.851016	49.343258
987.228067	58.097301	49.348263
983.805227	59.867213	49.353268
980.329917	64.198385	49.358273
977.041076	64.340289	49.363277
973.608606	57.724777	49.368282
970.079889	57.692054	49.373287
966.006060	59.838542	49.378292
962.408568	56.383930	49.383297
959.169881	64.885969	49.388301
955.707875	63.270512	49.393306
952.341034	61.763626	49.398311
949.008341	63.981407	49.403316
945.630313	56.655089	49.408321
941.783388	66.691284	49.413325
938.348525	57.029524	49.418330
934.881223	51.656443	49.423335
931.141248	50.989073	49.428340
928.009773	55.317345	49.433345
924.360900	59.121894	49.438349
920.686833	57.049082	49.443354
917.277085	52.125778	49.448359
913.750467	48.587378	49.453364
910.372279	53.105911	49.458369
906.734946	61.163816	49.463373
903.059047	48.334780	49.468378
899.782934	48.373473	49.473383
896.051774	56.357399	49.478388
892.909609	41.407878	49.483393
889.400382	57.753659	49.488397
885.994670	45.828511	49.493402
882.148294	42.422148	49.498407
878.472737	49.615988	49.503412
875.468119	42.914916	49.508417
871.932590	52.219279	49.513421
868.094382	50.235300	49.518426
865.088369	41.471729	49.523431
861.072187	48.804013	49.528436
857.435418	46.766534	49.533441
853.863384	53.972735	49.538445
850.824043	48.169227	49.543450
847.542535	47.370391	49.548455
843.526526	45.164164	49.553460
840.114391	47.653742	49.558465
836.608815	45.640135	49.563469
833.486922	50.118776	49.568474
829.657157	59.839097	49.573479
826.053724	56.391758	49.578484
822.943864	43.158264	49.583489
819.478965	43.444648	49.588493
815.670980	48.007946	49.593498
812.418183	45.160911	49.598503
808.932616	60.901911	49.603508
805.304399	50.118703	49.608513
801.589307	49.286129	49.613517
798.267268	45.981650	49.618522
794.470259	55.219156	49.623527
790.902786	57.710775	49.628532
787.714602	43.040517	49.633537
784.209804	47.338328	49.638541
780.353658	52.345715	49.643546
777.283399	54.266401	49.648551
773.872814	58.074998	49.653556
770.418488	51.829913	49.658561
767.041968	46.249746	49.663565
762.983084	50.877416	49.668570
759.509068	44.170341	49.673575
755.593431	52.540485	49.678580
752.631075	47.402036	49.683585
749.311947	45.504946	49.688589
745.707889	42.348778	49.693594
742.351157	44.488063	49.698599
738.923117	48.062103	49.703604
735.373079	43.483365	49.708609
731.621086	46.810449	49.713613
728.098276	41.800378	49.718618
725.018420	43.241684	49.723623
720.837254	46.423613	49.728628
717.376160	50.828519	49.733633
714.165460	40.980062	49.738637
710.684087	44.246039	49.743642
707.442237	43.801706	49.748647
703.065107	44.220619	49.753652
699.970886	40.766799	49.758657
696.510387	42.346454	49.763661
693.104721	38.447585	49.768666
689.711959	37.238993	49.773671
686.246418	48.187066	49.778676
682.269999	47.281298	49.783681
678.905518	53.952177	49.788685
675.171352	45.260864	49.793690
672.137551	47.179047	49.798695
668.562985	59.653171	49.803700
665.310322	50.826791	49.808705
661.506375	54.731433	49.813709
658.383784	47.188241	49.818714
654.220849	50.898837	49.823719
650.750525	55.887303	49.828724
647.696124	42.142192	49.833729
644.006858	48.873122	49.838733
640.910843	55.369337	49.843738
637.305876	52.390491	49.848743
633.708897	45.819636	49.853748
630.167795	47.563703	49.858753
626.155810	43.743412	49.863757
622.750635	55.688142	49.868762
619.778859	50.152555	49.873767
615.914314	47.831039	49.878772
612.798258	45.427804	49.883777
609.038166	53.479524	49.888781
605.434345	44.644551	49.893786
602.152603	47.702296	49.898791
598.238297	40.503824	49.903796
595.114294	47.029705	49.908801
591.259305	54.071170	49.913805
587.806619	51.780452	49.918810
584.571054	50.319616	49.923815
581.178697	56.327307	49.928820
577.904714	42.524649	49.933825
573.818905	51.813453	49.938829
570.341041	46.771101	49.943834
567.288546	54.918307	49.948839
563.473980	56.546770	49.953844
560.041721	41.879765	49.958849
556.785599	46.777945	49.963853
552.909351	46.698139	49.968858
549.315332	37.504161	49.973863
545.786983	52.226783	49.978868
542.673880	43.771000	49.983873
538.924883	46.702180	49.988877
535.349446	51.128067	49.993882
531.830314	38.891639	49.998887
528.502128	41.902838	50.003892
524.872953	34.523958	50.008897
521.631548	46.167950	50.013901
517.794148	49.906976	50.018906
514.368361	39.149272	50.023911
511.061861	59.098541	50.028916
507.837048	40.159940	50.033921
503.997428	45.012923	50.038925
499.819669	52.886069	50.043930
496.651650	44.669790	50.048935
492.967255	54.399133	50.053940
489.937972	38.710822	50.058945
486.699825	36.826472	50.063949
483.508444	49.127049	50.068954
479.850140	41.316123	50.073959
475.604472	53.303119	50.078964
472.575897	47.045592	50.083969
468.740997	51.783954	50.088973
465.339511	46.970168	50.093978
462.061446	33.601604	50.098983
458.152304	56.447693	50.103988
454.835332	37.596221	50.108993
451.202733	45.805265	50.113997
447.993484	44.530172	50.119002
444.822455	43.796444	50.124007
440.393753	49.291620	50.129012
437.540215	41.061197	50.134017
434.291489	47.467303	50.139021
430.234265	47.210051	50.144026
427.060325	49.222840	50.149031
423.082725	47.621290	50.154036
419.650513	43.150810	50.159041
416.401289	48.997026	50.164045
412.674975	44.236984	50.169050
409.381449	40.156192	50.174055
406.071833	48.185249	50.179060
402.375633	46.495602	50.184065
398.691230	45.829148	50.189069
395.383554	43.683559	50.194074
392.085037	41.580836	50.199079
388.103558	50.878720	50.204084
384.720637	49.092849	50.209089
381.023350	43.088138	50.214093
377.411155	46.501062	50.219098
374.203813	45.336411	50.224103
371.040958	44.171161	50.229108
367.605793	45.933566	50.234113
364.287012	37.642714	50.239117
360.238929	40.256656	50.244122
356.337300	41.190040	50.249127
353.180309	42.184661	50.254132
349.853655	44.123159	50.259137
346.449476	52.483309	50.264141
342.439311	43.101067	50.269146
339.578710	39.414782	50.274151
335.686784	50.527324	50.279156
331.992984	50.137580	50.284161
328.798563	48.660884	50.289165
325.306326	47.376082	50.294170
321.775413	38.795570	50.299175
318.060563	48.415769	50.304180
314.889238	53.566516	50.309185
311.302244	53.236075	50.314189
307.864670	43.894408	50.319194
304.110883	43.292552	50.324199
300.323650	49.861598	50.329204
297.287958	47.398440	50.334209
293.778655	45.970772	50.339213
290.197506	51.033468	50.344218
286.574367	53.309189	50.349223
283.140300	47.700101	50.354228
279.826094	42.796834	50.359233
276.442248	47.911069	50.364237
272.510215	50.788523	50.369242
269.023092	44.298710	50.374247
265.641476	51.763200	50.379252
262.204126	49.384726	50.384257
259.010909	49.078406	50.389261
255.356999	56.778274	50.394266
251.891424	44.280480	50.399271
247.993090	46.826833	50.404276
244.925384	53.609721	50.409281
241.119003	51.652524	50.414285
237.458195	55.158453	50.419290
234.231910	47.153771	50.424295
230.357280	56.200923	50.429300
227.024977	45.751420	50.434305
223.928462	53.971933	50.439309
220.374759	61.200638	50.444314
217.107885	53.651515	50.449319
213.050195	53.289970	50.454324
209.461174	52.194254	50.459329
206.335246	48.593586	50.464333
202.501500	51.193163	50.469338
199.574353	40.595173	50.474343
195.344428	50.225971	50.479348
191.760246	51.046683	50.484353
188.473703	50.558756	50.489357
184.948651	52.610417	50.494362
181.701719	46.690648	50.499367
178.063021	48.965641	50.504372
174.495779	48.069015	50.509377
170.966215	46.786884	50.514381
167.638504	50.430780	50.519386
164.252927	46.835744	50.524391
160.563185	48.928866	50.529396
157.346307	48.477552	50.534401
153.588515	51.634769	50.539405
149.862773	53.448770	50.544410
147.097775	35.979391	50.549415
142.949113	49.615386	50.554420
139.379418	45.701017	50.559425
135.915733	55.234673	50.564429
132.396136	56.010537	50.569434
129.139846	48.491423	50.574439
125.522889	48.494696	50.579444
122.278035	50.066156	50.584449
118.878469	41.310218	50.589453
115.033981	47.638266	50.594458
111.496296	42.690732	50.599463
107.912376	49.955783	50.604468
104.635991	41.867183	50.609473
101.046302	43.773899	50.614477
97.372342	50.157655	50.619482
94.356461	49.377672	50.624487
90.363754	56.029349	50.629492
87.022566	45.676171	50.634497
83.359804	50.776905	50.639501
80.046439	51.466885	50.644506
76.781028	39.096158	50.649511
73.025714	48.365180	50.654516
69.570460	43.417474	50.659521
66.029191	45.807022	50.664525
62.361904	47.896662	50.669530
58.883410	37.732547	50.674535
55.200701	49.935629	50.679540
51.931002	45.914460	50.684545
48.660975	46.945699	50.689549
44.716804	43.282636	50.694554
41.387883	42.984819	50.699559
38.040382	53.819635	50.704564
34.710295	50.298236	50.709569
31.112460	46.891289	50.714573
27.363263	46.775965	50.719578
24.141975	53.804237	50.724583
20.212263	48.800700	50.729588
16.871467	44.603950	50.734593
13.225432	49.986816	50.739597
9.967316	48.440991	50.744602
6.605213	49.075297	50.749607
2.730436	51.687617	50.754612