Fri Aug 26 11:25:52 2022

Number of Points = 9912

Depth (nm)	Load (N)	Time (s)
8.521508	100.276410	0.000000
7.923495	103.523842	0.005005
8.056907	92.281712	0.010010
7.734716	95.081249	0.015014
7.236360	95.889799	0.020019
7.404978	84.714957	0.025024
7.108717	78.073260	0.030029
6.243264	86.228036	0.035034
6.316146	91.288188	0.040038
5.645803	78.117994	0.045043
5.095020	79.251072	0.050048
4.916294	83.255770	0.055053
4.707445	78.100038	0.060058
4.782770	71.419470	0.065062
4.629658	84.392314	0.070067
4.899633	76.362192	0.075072
4.193181	69.224397	0.080077
3.607964	69.616213	0.085082
3.577140	66.799182	0.090086
3.665521	67.636596	0.095091
3.043577	56.012239	0.100096
2.955172	53.321230	0.105101
2.270641	55.269208	0.110106
2.444487	54.407087	0.115110
2.012213	59.963483	0.120115
1.508305	53.910929	0.125120
1.223971	58.779924	0.130125
1.500551	49.097358	0.135130
1.077955	44.727866	0.140134
1.056030	58.816017	0.145139
0.760026	39.041968	0.150144
-0.045963	49.357735	0.155149
0.047323	51.735083	0.160154
0.150898	41.889639	0.165158
-0.250289	48.690834	0.170163
-0.834038	40.388704	0.175168
-0.900294	43.100930	0.180173
-1.066664	35.901205	0.185178
-1.061839	40.617609	0.190182
-1.592897	38.969927	0.195187
-1.890170	44.663482	0.200192
-2.030486	45.549157	0.205197
-2.566152	33.417853	0.210202
-3.520857	23.518899	0.215206
-3.473589	30.962085	0.220211
-3.037119	33.083524	0.225216
-3.418547	36.151695	0.230221
-3.459123	33.775935	0.235226
-3.396968	25.366918	0.240230
-4.139458	29.962402	0.245235
-4.738890	29.486426	0.250240
-4.608200	24.527773	0.255245
-4.734173	26.293872	0.260250
-5.003685	13.959795	0.265254
-5.710846	15.813220	0.270259
-5.808288	9.997942	0.275264
-5.795005	18.148743	0.280269
-5.952008	15.357693	0.285274
-6.677400	13.835181	0.290278
-7.113128	9.632252	0.295283
-6.776010	17.871833	0.300288
-7.096717	20.538254	0.305293
-7.508566	14.847855	0.310298
-7.989086	1.698783	0.315302
-8.284096	13.380755	0.320307
-8.759376	1.322326	0.325312
-8.932983	6.468285	0.330317
-8.634123	7.889836	0.335322
-8.778715	3.628924	0.340326
-8.763031	22.399712	0.345331
-9.359318	11.378812	0.350336
-9.948239	10.692400	0.355341
-9.586443	4.479766	0.360346
-10.154603	4.470306	0.365350
-10.548248	11.222857	0.370355
-10.747913	-1.128411	0.375360
-10.951114	10.086864	0.380365
-11.135975	0.688135	0.385370
-11.366200	-3.021623	0.390374
-12.148152	8.802599	0.395379
-12.066594	-4.788310	0.400384
-12.185086	5.372933	0.405389
-12.832280	5.581416	0.410394
-12.395146	-1.807168	0.415398
-13.072705	-0.198790	0.420403
-13.261643	-2.083226	0.425408
-13.726057	-1.362220	0.430413
-13.797516	-6.010989	0.435418
-13.835638	-7.292505	0.440422
-14.246961	-8.436823	0.445427
-15.059348	-4.690976	0.450432
-15.044817	-4.822797	0.455437
-15.478964	-4.438685	0.460442
-15.282419	-14.744646	0.465446
-15.205834	-8.109607	0.470451
-15.555907	-10.297973	0.475456
-15.513602	-8.358768	0.480461
-16.696625	-3.375175	0.485466
-16.255389	1.149887	0.490470
-16.926296	-0.665835	0.495475
-17.240739	-11.993185	0.500480
-18.262605	-7.154903	0.505485
-17.301430	-13.100198	0.510490
-17.619706	-16.331188	0.515494
-18.417499	-7.260042	0.520499
-18.437426	-7.446607	0.525504
-18.094741	-4.813879	0.530509
-18.821253	-1.432567	0.535514
-19.062890	-16.567621	0.540518
-19.705987	-11.440314	0.545523
-19.675739	-4.880315	0.550528
-20.096117	-5.023511	0.555533
-20.139282	-0.286993	0.560538
-19.577280	-5.126137	0.565542
-20.332781	-2.230676	0.570547
-20.693928	-3.670698	0.575552
-20.872682	-5.986974	0.580557
-21.181806	-3.521670	0.585562
-21.573380	-11.575294	0.590566
-22.068753	-6.939205	0.595571
-22.588637	-9.183386	0.600576
-22.476348	-13.348252	0.605581
-22.762621	-9.671668	0.610586
-22.497723	-17.261209	0.615590
-22.868337	-10.255997	0.620595
-23.550502	-1.503398	0.625600
-24.191776	-5.775556	0.630605
-24.368619	-7.623910	0.635610
-24.346269	-11.398300	0.640614
-24.080479	-0.430056	0.645619
-24.453689	-5.360861	0.650624
-24.263984	-5.219410	0.655629
-25.061471	-3.772688	0.660634
-25.166505	-5.733460	0.665638
-25.507241	-4.927310	0.670643
-25.865427	-4.988444	0.675648
-25.991918	3.838986	0.680653
-27.068499	2.753956	0.685658
-26.739872	-6.152097	0.690662
-27.177058	-5.204384	0.695667
-27.116839	-14.467261	0.700672
-27.288522	-4.996908	0.705677
-27.595580	-5.357058	0.710682
-27.219347	-13.950992	0.715686
-28.021300	-16.613145	0.720691
-28.352720	-13.011787	0.725696
-28.814998	-11.990567	0.730701
-28.717293	-4.128159	0.735706
-28.357722	-8.103746	0.740710
-29.277670	-2.439803	0.745715
-29.589830	-6.725239	0.750720
-29.924384	-4.986776	0.755725
-30.122182	-3.253788	0.760730
-30.484644	-10.166706	0.765734
-31.091685	-11.106550	0.770739
-31.068758	-16.681141	0.775744
-31.521015	-2.491239	0.780749
-31.597073	-2.855719	0.785754
-31.576812	-7.809824	0.790758
-31.706111	-14.562897	0.795763
-31.536660	-10.122068	0.800768
-32.425659	-1.217046	0.805773
-32.737300	-4.173834	0.810778
-32.869976	-5.029354	0.815782
-33.153767	-6.070146	0.820787
-33.416170	-2.982551	0.825792
-33.146754	-10.857526	0.830797
-33.962546	-10.635447	0.835802
-33.893692	-14.255731	0.840806
-34.302139	-2.859819	0.845811
-34.109798	-13.149307	0.850816
-35.307743	-12.143253	0.855821
-35.295844	-5.513961	0.860826
-35.416139	-11.638873	0.865830
-35.575783	-8.026295	0.870835
-35.556608	-10.594843	0.875840
-35.835532	-17.723237	0.880845
-36.840961	-7.651690	0.885850
-37.135095	-19.905978	0.890854
-37.369009	-11.033358	0.895859
-37.267444	-10.685202	0.900864
-37.313384	-11.740881	0.905869
-37.322377	-7.876523	0.910874
-37.192318	-6.476147	0.915878
-37.782807	2.357089	0.920883
-38.467734	-8.532939	0.925888
-38.345954	-5.995526	0.930893
-39.231579	0.080674	0.935898
-39.548473	-10.338327	0.940902
-39.759864	-6.670238	0.945907
-40.222921	-14.317274	0.950912
-40.182076	-11.824206	0.955917
-40.216017	-11.818770	0.960922
-39.768178	-9.044234	0.965926
-40.229789	-3.306127	0.970931
-40.671464	-11.522785	0.975936
-41.329723	-8.265992	0.980941
-42.032129	-1.304027	0.985946
-41.672956	-6.032499	0.990950
-42.390448	-11.944208	0.995955
-41.945046	-13.089044	1.000960
-42.148290	-7.505057	1.005965
-42.208507	-15.556488	1.010970
-42.914728	-18.091182	1.015974
-43.348059	-18.782834	1.020979
-43.213689	-15.519746	1.025984
-43.322782	-10.412311	1.030989
-43.965507	-12.504491	1.035994
-44.104358	-16.199998	1.040998
-44.437272	-7.625163	1.046003
-44.910555	-11.714674	1.051008
-44.812884	-15.795008	1.056013
-44.595007	-13.785069	1.061018
-45.336739	-16.168706	1.066022
-45.904203	-13.501833	1.071027
-45.827603	-22.555292	1.076032
-45.880570	-17.905835	1.081037
-46.210466	-12.577366	1.086042
-46.539403	-16.876005	1.091046
-47.091561	-18.684903	1.096051
-47.055301	-11.094497	1.101056
-47.244075	-10.239243	1.106061
-47.644701	-14.643775	1.111066
-48.082008	-13.572661	1.116070
-48.566902	-7.486094	1.121075
-48.925152	-13.115226	1.126080
-48.899158	-8.335697	1.131085
-49.184063	-6.244309	1.136090
-49.129188	-13.399368	1.141094
-48.714904	-12.087537	1.146099
-49.235687	-14.742849	1.151104
-49.834170	-9.337761	1.156109
-50.483078	-13.368290	1.161114
-50.329913	-12.366967	1.166118
-50.469463	-12.512761	1.171123
-50.867152	-11.855925	1.176128
-51.386837	-13.268097	1.181133
-51.785654	-14.205560	1.186138
-51.972356	-9.990842	1.191142
-52.045778	0.451269	1.196147
-51.995867	-4.485306	1.201152
-51.757258	-19.970365	1.206157
-52.547994	-9.524137	1.211162
-52.944923	-18.728487	1.216166
-53.809575	-7.992349	1.221171
-53.704379	-10.855855	1.226176
-53.346861	-9.104930	1.231181
-53.885170	-11.162749	1.236186
-53.778785	-18.544116	1.241190
-54.711454	-7.753098	1.246195
-54.888117	-8.832714	1.251200
-55.003883	-7.928719	1.256205
-54.861688	-3.626009	1.261210
-55.055882	-17.186624	1.266214
-56.033173	-5.154836	1.271219
-56.542208	-9.637399	1.276224
-56.293101	-13.149712	1.281229
-56.734085	-8.753038	1.286234
-56.842557	-8.941634	1.291238
-56.934118	-11.685922	1.296243
-56.401551	-13.122730	1.301248
-57.033964	-16.263679	1.306253
-57.849455	-10.014911	1.311258
-57.889467	-15.421519	1.316262
-58.147917	-13.533561	1.321267
-58.173935	-15.019434	1.326272
-58.806827	-4.983744	1.331277
-59.303201	-8.860859	1.336282
-59.576678	-10.535985	1.341286
-59.870690	-8.829144	1.346291
-59.925534	-4.701392	1.351296
-59.600356	-13.888467	1.356301
-59.693310	-7.847107	1.361306
-60.473832	-3.201420	1.366310
-61.074184	-8.334130	1.371315
-61.199882	-2.547088	1.376320
-61.325965	-15.264125	1.381325
-61.914145	-8.759695	1.386330
-61.668548	-15.115573	1.391334
-62.030338	-15.328001	1.396339
-61.761408	-8.390731	1.401344
-61.980232	-1.586315	1.406349
-63.042501	-11.183765	1.411354
-62.572168	-19.672128	1.416358
-63.112565	-3.152723	1.421363
-63.601340	-11.070991	1.426368
-63.609943	-11.838265	1.431373
-64.056897	-2.533853	1.436378
-64.030055	-14.445827	1.441382
-64.658876	-8.229287	1.446387
-64.379217	-1.344303	1.451392
-64.634684	-12.899121	1.456397
-65.233158	-11.268258	1.461402
-65.394643	-14.846349	1.466406
-65.839067	-11.024924	1.471411
-65.820216	-12.520946	1.476416
-66.248601	-10.581219	1.481421
-67.173501	-8.994440	1.486426
-67.021625	-16.794164	1.491430
-67.194303	-5.691221	1.496435
-67.274273	-8.481604	1.501440
-66.950882	-19.259709	1.506445
-67.355708	-8.968478	1.511450
-68.046589	-8.164755	1.516454
-68.687832	-6.628468	1.521459
-68.749761	-9.953152	1.526464
-68.385127	-10.285012	1.531469
-68.944487	-8.271110	1.536474
-68.726440	-18.861976	1.541478
-69.411212	-15.275202	1.546483
-69.511479	-4.879534	1.551488
-69.681436	-16.773518	1.556493
-70.121562	-12.747125	1.561498
-70.455373	-25.415992	1.566502
-71.201301	-23.059843	1.571507
-71.805599	-7.384676	1.576512
-71.827740	-18.975819	1.581517
-71.737931	-12.497862	1.586522
-71.144684	-16.320012	1.591526
-71.396890	-3.113519	1.596531
-71.560646	-13.274795	1.601536
-72.307254	-24.968260	1.606541
-72.931436	-17.268699	1.611546
-72.839612	-8.826435	1.616550
-72.958903	-12.841352	1.621555
-73.549667	-15.871731	1.626560
-74.348933	-14.307677	1.631565
-74.896749	-12.007682	1.636570
-73.975125	-14.580704	1.641574
-74.435991	-14.021595	1.646579
-74.754342	-13.054420	1.651584
-74.509950	-21.744875	1.656589
-74.805160	-19.310212	1.661594
-75.686402	-22.089725	1.666598
-75.950805	-15.528146	1.671603
-76.224090	-25.033306	1.676608
-76.236772	-17.425793	1.681613
-75.858351	-16.026124	1.686618
-76.599237	-25.853932	1.691622
-77.538509	-18.121130	1.696627
-77.336073	-25.773704	1.701632
-77.249327	-24.094512	1.706637
-77.770657	-16.505875	1.711642
-77.397423	-10.948376	1.716646
-78.161384	-18.295465	1.721651
-78.479618	-11.981757	1.726656
-78.490501	-15.896498	1.731661
-78.894503	-15.343079	1.736666
-79.698721	-16.464183	1.741670
-80.101771	-13.955783	1.746675
-80.056260	-15.674247	1.751680
-80.261859	-14.721465	1.756685
-81.002813	-16.241548	1.761690
-80.360272	-20.210572	1.766694
-80.741531	-16.743819	1.771699
-80.779415	-18.686570	1.776704
-80.478835	-15.791036	1.781709
-80.958351	-13.659857	1.786714
-81.138356	-16.785828	1.791718
-81.425669	-15.348940	1.796723
-82.731199	-10.558238	1.801728
-82.391202	-14.771211	1.806733
-83.293015	-12.311698	1.811738
-83.247464	-16.466171	1.816742
-83.211843	-13.393345	1.821747
-83.244953	-12.679383	1.826752
-83.559102	-22.871018	1.831757
-84.395481	-15.730017	1.836762
-84.285102	-25.778950	1.841766
-85.091125	-15.966239	1.846771
-85.032112	-18.139205	1.851776
-85.132572	-19.759013	1.856781
-85.231065	-9.040934	1.861786
-84.998446	-19.048794	1.866790
-85.474597	-15.915266	1.871795
-86.177298	-8.896314	1.876800
-86.234214	-22.019567	1.881805
-86.378263	-18.681494	1.886810
-86.489240	-20.464174	1.891814
-87.105341	-15.132273	1.896819
-87.523086	-8.894816	1.901824
-87.361527	-24.529215	1.906829
-87.907665	-8.379070	1.911834
-87.695569	-16.960097	1.916838
-87.686949	-20.909509	1.921843
-88.742304	-23.921330	1.926848
-88.878733	-14.620984	1.931853
-89.123103	-19.397843	1.936858
-89.238500	-16.405904	1.941862
-89.550736	-19.055721	1.946867
-89.731917	-12.105316	1.951872
-89.989509	-20.837829	1.956877
-90.986952	-13.108622	1.961882
-90.804928	-17.863289	1.966886
-90.682184	-15.180502	1.971891
-91.165632	-16.908351	1.976896
-90.917357	-19.917513	1.981901
-91.291055	-16.328556	1.986906
-91.760528	-16.884871	1.991910
-92.296441	-27.155864	1.996915
-92.104549	-21.729672	2.006912
-92.364020	-17.716688	2.016909
-91.833693	-19.937149	2.026906
-91.151413	-19.488734	2.036902
-90.133993	-15.712576	2.046899
-89.906997	-22.260387	2.056896
-89.818371	-15.333476	2.066893
-89.436171	-18.424163	2.076890
-88.652139	-12.435462	2.086886
-87.606163	-14.935776	2.096883
-87.261371	-10.307312	2.106880
-87.090873	-13.618452	2.116877
-86.998658	-13.008473	2.126874
-86.133573	-10.884303	2.136870
-85.442147	-14.324068	2.146867
-84.693806	-13.458300	2.156864
-84.492456	-12.222272	2.166861
-84.503865	-8.463312	2.176858
-83.367715	-15.893922	2.186854
-83.086323	-9.655903	2.196851
-82.535647	-16.073556	2.206848
-81.764451	-12.870423	2.216845
-81.786152	-14.041955	2.226842
-81.143320	-20.812898	2.236838
-80.193176	-17.450735	2.246835
-80.153995	-14.535923	2.256832
-79.817999	-18.230780	2.266829
-78.783122	-17.732730	2.276826
-78.755166	-10.805874	2.286822
-78.018275	-17.645314	2.296819
-77.776213	-11.844648	2.306816
-76.505656	-9.717088	2.316813
-76.576158	-15.556534	2.326810
-76.130480	-16.696304	2.336806
-75.657346	-12.284220	2.346803
-74.608259	-12.504281	2.356800
-74.360140	-15.808500	2.366797
-74.741363	-12.330903	2.376794
-73.475177	-9.138318	2.386790
-73.047051	-12.895036	2.396787
-72.099074	-15.408600	2.406784
-71.553772	-21.309081	2.416781
-71.599477	-15.856404	2.426778
-71.343896	-17.137631	2.436774
-70.564208	-15.389790	2.446771
-70.325206	-12.243171	2.456768
-69.372006	-5.878509	2.466765
-68.830679	-3.599394	2.476762
-68.546448	-12.215121	2.486758
-67.822172	-11.545170	2.496755
-67.389706	-8.305134	2.506752
-67.294525	-12.108210	2.516749
-66.307465	-13.614199	2.526746
-65.912186	-14.682768	2.536742
-65.795313	-17.485063	2.546739
-64.644425	-11.930435	2.556736
-64.328880	-14.120623	2.566733
-64.414472	-15.307549	2.576730
-63.571178	-16.997052	2.586726
-63.061136	-11.507363	2.596723
-62.090064	-10.369008	2.606720
-61.507180	-17.187637	2.616717
-61.558748	-12.022305	2.626714
-61.720206	-13.070711	2.636710
-60.511358	-18.108362	2.646707
-59.820767	-17.119565	2.656704
-59.526827	-20.468930	2.666701
-58.688727	-26.738103	2.676698
-58.612428	-22.790069	2.686694
-58.137635	-20.966247	2.696691
-57.359685	-18.423045	2.706688
-57.211268	-24.480300	2.716685
-56.056164	-10.956420	2.726682
-55.996998	-19.055613	2.736678
-56.031965	-17.073227	2.746675
-54.821121	-15.094754	2.756672
-54.516538	-20.846886	2.766669
-53.432814	-12.057091	2.776666
-53.110933	-14.875468	2.786662
-53.138193	-6.438526	2.796659
-52.891122	-19.385036	2.806656
-51.932472	-10.883032	2.816653
-51.901281	-12.990933	2.826650
-50.690103	-13.771570	2.836646
-50.044167	-8.531112	2.846643
-49.938183	-10.552461	2.856640
-49.520449	-14.434269	2.866637
-48.280348	-17.493811	2.876634
-48.770643	-18.557539	2.886630
-48.055291	-17.258995	2.896627
-46.960714	-14.020683	2.906624
-46.741482	-14.374452	2.916621
-46.956203	-14.426246	2.926618
-45.811027	-17.163742	2.936614
-45.411664	-12.591289	2.946611
-45.348724	-10.218682	2.956608
-44.454258	-9.442186	2.966605
-44.003112	-7.215550	2.976602
-42.980357	-6.535052	2.986598
-42.811939	-7.324387	2.996595
-42.676513	-13.968815	3.006592
-42.111209	-16.175716	3.016589
-41.395039	-8.098438	3.026586
-40.880733	-11.019634	3.036582
-39.912663	-16.520291	3.046579
-39.805934	-13.799722	3.056576
-39.754755	-14.922416	3.066573
-39.127139	-15.000827	3.076570
-38.050053	-0.267400	3.086566
-37.987707	-10.426095	3.096563
-37.508234	-11.640816	3.106560
-37.007710	-13.140739	3.116557
-36.346570	-12.483130	3.126554
-36.052132	-11.825444	3.136550
-35.123296	-20.085387	3.146547
-35.348591	-16.384988	3.156544
-34.276060	-17.375279	3.166541
-34.099504	-8.263675	3.176538
-33.147394	-10.939435	3.186534
-32.237951	-20.916415	3.196531
-32.491042	-15.244552	3.206528
-32.353408	-16.425054	3.216525
-31.429354	-18.085951	3.226522
-30.892325	-14.931884	3.236518
-30.581967	-11.571468	3.246515
-29.541931	-11.210429	3.256512
-29.368284	-7.423262	3.266509
-29.326468	-8.471642	3.276506
-28.317898	-13.148671	3.286502
-27.993075	-14.047885	3.296499
-27.268654	-9.285296	3.306496
-26.272506	-9.899409	3.316493
-26.366273	-7.638614	3.326490
-26.427895	-11.547153	3.336486
-25.495817	-18.907977	3.346483
-24.745330	-15.432363	3.356480
-23.972875	-11.494518	3.366477
-23.761093	-13.624202	3.376474
-23.482984	-8.795291	3.386470
-23.411644	-15.486759	3.396467
-22.286770	-15.085079	3.406464
-21.685868	-20.813660	3.416461
-21.648815	-18.123422	3.426458
-20.921691	-11.856601	3.436454
-20.200633	-13.828003	3.446451
-19.251268	-18.812581	3.456448
-19.531175	-6.082090	3.466445
-19.141296	-17.818606	3.476442
-18.208235	-25.787777	3.486438
-17.663997	-13.600577	3.496435
-17.756824	-11.510983	3.506432
-16.893033	-11.322067	3.516429
-16.338829	-8.550795	3.526426
-16.202852	-4.463166	3.536422
-15.301020	1.155590	3.546419
-14.773290	-4.669305	3.556416
-14.238913	-3.193699	3.566413
-13.498327	3.441652	3.576410
-13.418513	-3.463377	3.586406
-13.324484	1.951714	3.596403
-12.478063	0.458120	3.606400
-11.727563	5.511249	3.616397
-11.338402	9.610145	3.626394
-11.159933	13.006940	3.636390
-10.773878	14.312411	3.646387
-10.247719	22.593514	3.656384
-9.135363	25.021305	3.666381
-9.054449	29.646521	3.676378
-8.779428	28.469966	3.686374
-7.858359	34.503875	3.696371
-6.923935	46.224901	3.706368
-6.805455	47.999676	3.716365
-6.649250	44.459507	3.726362
-6.056820	54.700618	3.736358
-5.653471	50.821036	3.746355
-4.881582	59.475698	3.756352
-4.447457	68.689788	3.766349
-3.928668	68.153165	3.776346
-3.548012	73.422284	3.786342
-3.104898	75.602667	3.796339
-2.213845	80.595922	3.806336
-2.035805	82.510309	3.816333
-1.460643	86.133616	3.826330
-1.238799	100.176688	3.836326
0.000000	96.891495	3.841331
-0.062038	102.092875	3.846336
0.254640	96.823678	3.851341
0.188125	89.988023	3.856346
0.165224	97.673109	3.861350
-0.232010	95.713529	3.866355
-0.148863	93.520972	3.871360
-0.555732	92.195624	3.876365
0.243228	96.813707	3.881370
0.066836	97.445582	3.886374
0.148875	94.256643	3.891379
0.380946	92.186428	3.896384
-0.256584	90.337026	3.901389
-0.173866	94.573095	3.906394
0.105950	100.689329	3.911398
0.229762	98.569531	3.916403
0.100352	99.276346	3.921408
0.502351	89.381247	3.926413
-0.118508	94.033737	3.931418
0.116732	101.476158	3.936422
0.316011	84.658896	3.941427
-0.262135	95.783912	3.946432
-0.369090	90.356055	3.951437
0.139136	92.497966	3.956442
0.067061	101.494138	3.961446
0.182422	90.783152	3.966451
0.310956	98.068185	3.971456
0.068037	92.946226	3.976461
0.113922	97.156394	3.981466
0.294209	100.330100	3.986470
0.574825	95.854270	3.991475
0.320646	107.893768	3.996480
0.057980	112.702458	4.001485
0.210212	108.793927	4.006490
0.085985	105.776304	4.011494
0.409146	108.320343	4.016499
0.535141	101.404092	4.021504
0.202986	95.454492	4.026509
0.384450	97.131603	4.031514
-0.061547	106.369489	4.036518
0.137497	107.373168	4.041523
0.084974	110.469233	4.046528
0.492135	100.959291	4.051533
0.532686	107.913187	4.056538
0.437813	107.880655	4.061542
0.537110	107.662871	4.066547
0.377507	107.491725	4.071552
0.263036	104.883859	4.076557
0.572197	96.439514	4.081562
0.243337	101.252180	4.086566
0.466009	91.631767	4.091571
0.430874	92.725688	4.096576
0.410491	91.735623	4.101581
0.911085	95.008150	4.106586
0.444712	101.294346	4.111590
0.785459	101.013660	4.116595
0.582207	99.884393	4.121600
0.408154	99.266257	4.126605
0.350591	101.730373	4.131610
0.629440	109.782922	4.136614
0.703263	101.175906	4.141619
0.793580	113.133298	4.146624
0.608585	101.409242	4.151629
0.928745	95.819973	4.156634
0.449014	96.476932	4.161638
0.544381	97.477770	4.166643
0.875585	96.575328	4.171648
0.892598	102.406623	4.176653
0.735945	102.975315	4.181658
0.706025	101.993062	4.186662
0.783201	98.032946	4.191667
0.546058	99.351304	4.196672
0.492075	96.797294	4.201677
1.193968	112.405239	4.206682
1.011316	103.063058	4.211686
1.315858	96.147482	4.216691
0.900747	101.232996	4.221696
1.197624	97.653114	4.226701
0.820747	97.601216	4.231706
0.432533	108.446738	4.236710
0.922230	100.524760	4.241715
1.108976	100.635036	4.246720
0.627909	100.320958	4.251725
0.734500	101.582633	4.256730
0.793099	103.715460	4.261734
0.732227	103.370758	4.266739
0.910191	101.767697	4.271744
0.813187	94.215472	4.276749
1.101484	103.294737	4.281754
1.074500	101.796350	4.286758
0.880911	93.335375	4.291763
1.488743	96.777861	4.296768
0.759960	103.272589	4.301773
0.821104	103.101873	4.306778
1.153522	111.554195	4.311782
1.546255	115.267451	4.316787
1.080023	107.345614	4.321792
0.924733	99.188711	4.326797
0.917303	102.496047	4.331802
0.715045	109.446621	4.336806
1.572952	105.216253	4.341811
1.271900	104.535635	4.346816
0.836080	100.269425	4.351821
1.208045	102.888120	4.356826
1.425065	109.928433	4.361830
1.453640	97.136610	4.366835
1.270659	105.159826	4.371840
0.919762	96.849888	4.376845
1.098234	91.874285	4.381850
1.133351	108.838853	4.386854
1.513440	106.565260	4.391859
1.683295	106.184635	4.396864
1.192433	94.397479	4.401869
1.134501	88.174239	4.406874
0.858213	112.726299	4.411878
1.708581	109.866971	4.416883
1.491595	104.927628	4.421888
0.831386	113.942613	4.426893
1.180528	100.942693	4.431898
1.541661	114.515679	4.436902
1.326273	108.522585	4.441907
1.568835	106.681682	4.446912
1.420328	108.736027	4.451917
1.599301	114.969204	4.456922
1.586954	104.331876	4.461926
1.069026	107.047999	4.466931
1.362666	113.797982	4.471936
1.177712	113.558018	4.476941
1.877465	106.887780	4.481946
1.940321	111.645786	4.486950
1.636650	109.348943	4.491955
1.202205	111.969814	4.496960
1.257149	112.201849	4.501965
1.599360	102.569145	4.506970
1.676405	107.869091	4.511974
1.735351	108.451669	4.516979
1.457898	98.918612	4.521984
1.706658	104.815063	4.526989
1.850527	103.710841	4.531994
1.436365	107.752201	4.536998
1.359606	105.979997	4.542003
1.857653	101.498785	4.547008
1.601962	115.917599	4.552013
1.729698	105.521043	4.557018
1.730532	112.006575	4.562022
1.925240	109.477116	4.567027
1.439421	106.667647	4.572032
1.761405	110.926576	4.577037
2.040833	101.116992	4.582042
1.853509	99.618261	4.587046
0.624062	106.848984	4.592051
1.528497	105.313141	4.597056
1.642334	112.005699	4.602061
2.044764	105.536773	4.607066
1.685877	108.490718	4.612070
1.905950	107.928273	4.617075
1.738763	111.355393	4.622080
1.315257	109.020263	4.627085
1.654145	109.676310	4.632090
1.706560	105.327754	4.637094
1.698653	103.589122	4.642099
1.882390	113.576825	4.647104
1.848764	115.078625	4.652109
1.687938	108.567686	4.657114
1.558086	112.514162	4.662118
2.017078	123.379641	4.667123
2.934096	119.826582	4.672128
2.462509	122.823386	4.677133
2.147215	117.848726	4.682138
1.831400	111.134134	4.687142
1.783077	108.183783	4.692147
1.704813	105.779081	4.697152
1.642206	114.903496	4.702157
1.664808	106.987804	4.707162
1.942390	111.152409	4.712166
2.101685	115.183576	4.717171
2.403497	120.372602	4.722176
2.696822	118.973034	4.727181
2.592255	110.479208	4.732186
2.093828	113.388443	4.737190
1.637074	113.285708	4.742195
1.957719	112.084362	4.747200
2.017250	113.853224	4.752205
2.329402	102.861661	4.757210
1.946252	110.425677	4.762214
1.647713	111.573265	4.767219
2.251090	110.647428	4.772224
2.596738	116.209267	4.777229
2.717983	118.582272	4.782234
2.516484	116.940217	4.787238
2.392192	112.979830	4.792243
2.130227	103.741743	4.797248
1.814751	107.916430	4.802253
2.170683	104.903138	4.807258
2.068352	117.001256	4.812262
2.608303	109.688364	4.817267
2.480676	113.681949	4.822272
2.117696	110.467386	4.827277
2.532480	105.641642	4.832282
2.136709	117.026169	4.837286
2.651865	119.461225	4.842291
2.467225	113.450688	4.847296
2.088082	107.859567	4.852301
2.409440	114.870982	4.857306
2.897929	125.440812	4.862310
2.495161	118.043748	4.867315
2.392094	116.617315	4.872320
2.295839	111.421898	4.877325
2.464811	99.740805	4.882330
2.304219	112.683197	4.887334
2.924601	119.739803	4.892339
2.546486	110.377432	4.897344
2.122058	116.739358	4.902349
2.996832	113.490263	4.907354
2.672331	116.859623	4.912358
2.304190	113.683827	4.917363
2.651494	108.008072	4.922368
2.428425	123.801171	4.927373
2.982897	122.579235	4.932378
2.300952	116.576526	4.937382
2.406180	117.136080	4.942387
3.458114	114.311805	4.947392
2.662833	118.618145	4.952397
2.536491	109.545595	4.957402
2.228473	120.865842	4.962406
2.733644	120.777848	4.967411
2.821326	118.299852	4.972416
2.423056	123.113839	4.977421
2.962706	121.546209	4.982426
2.962582	126.307697	4.987430
2.236795	127.442717	4.992435
2.977534	118.067485	4.997440
2.961053	121.268668	5.002445
2.891735	121.962964	5.007450
2.526064	123.487991	5.012454
2.731495	126.075673	5.017459
3.071121	121.188862	5.022464
3.012750	125.481706	5.027469
2.668732	113.690656	5.032474
2.677406	122.275644	5.037478
2.764224	124.739429	5.042483
3.248411	118.852539	5.047488
2.936635	124.190882	5.052493
3.286702	125.414650	5.057498
2.659800	122.858093	5.062502
2.882085	119.156946	5.067507
3.206173	124.140030	5.072512
2.733968	124.514251	5.077517
2.857093	116.915088	5.082522
3.020017	122.473742	5.087526
3.046402	124.557805	5.092531
3.522066	120.722297	5.097536
2.645206	124.740792	5.102541
3.031259	116.113629	5.107546
3.295478	127.085363	5.112550
3.061251	129.418805	5.117555
2.832759	120.498192	5.122560
2.713655	124.582199	5.127565
3.054267	119.008720	5.132570
2.889324	131.442453	5.137574
3.184855	121.348785	5.142579
3.385167	128.176577	5.147584
2.733156	140.705134	5.152589
2.928102	121.635980	5.157594
3.264816	121.931709	5.162598
3.113807	121.275184	5.167603
3.186767	119.966872	5.172608
3.184357	117.945816	5.177613
3.299440	112.720657	5.182618
3.223026	126.966038	5.187622
3.208385	123.058177	5.192627
3.383666	122.325539	5.197632
2.892210	127.356511	5.202637
3.084872	111.568446	5.207642
3.238856	116.369211	5.212646
3.143382	119.892733	5.217651
3.176425	122.371217	5.222656
3.151524	131.486606	5.227661
3.773330	126.059164	5.232666
3.334134	129.177472	5.237670
3.243844	113.120258	5.242675
3.472226	119.076832	5.247680
2.992765	118.325918	5.252685
3.716186	129.453941	5.257690
3.380838	130.736972	5.262694
3.289773	130.583627	5.267699
3.899071	128.536929	5.272704
3.449894	125.911572	5.277709
3.351778	120.580404	5.282714
3.598331	125.113665	5.287718
4.010335	128.637266	5.292723
3.380995	124.097469	5.297728
3.343307	121.085350	5.302733
3.509090	123.710842	5.307738
3.480302	128.818470	5.312742
3.372021	124.751186	5.317747
3.956258	122.486934	5.322752
3.658919	130.866479	5.327757
3.432183	110.293813	5.332762
3.412923	119.693047	5.337766
3.976753	123.968107	5.342771
4.156266	122.269893	5.347776
3.581936	133.454447	5.352781
3.609037	126.822495	5.357786
3.383978	123.887004	5.362790
3.833168	119.660160	5.367795
3.704748	124.596643	5.372800
3.321945	132.961023	5.377805
3.989124	134.901026	5.382810
3.766104	133.670433	5.387814
3.572085	129.920210	5.392819
3.874044	124.109145	5.397824
3.666992	130.573269	5.402829
4.056412	130.212240	5.407834
3.960650	129.382602	5.412838
3.638086	125.449919	5.417843
3.544721	127.109713	5.422848
4.183586	137.051877	5.427853
4.219154	125.053025	5.432858
3.615123	129.873742	5.437862
3.853490	125.929651	5.442867
3.791179	131.033008	5.447872
3.729286	133.159290	5.452877
3.986129	129.965274	5.457882
4.429035	139.381144	5.462886
3.818908	134.329001	5.467891
3.808788	117.952425	5.472896
3.502372	130.778334	5.477901
3.934762	137.873708	5.482906
4.370107	141.203857	5.487910
4.255845	131.104386	5.492915
4.128754	117.099791	5.497920
4.041511	132.650293	5.502925
3.921710	128.059633	5.507930
3.909337	129.042448	5.512934
4.075821	128.339653	5.517939
4.349498	128.752762	5.522944
3.725482	125.344728	5.527949
4.296675	129.675588	5.532954
4.543639	134.458718	5.537958
3.697131	129.819857	5.542963
4.005005	128.459151	5.547968
4.450235	136.226387	5.552973
4.407084	124.644741	5.557978
3.874672	128.252113	5.562982
4.510308	136.084613	5.567987
4.360542	121.801978	5.572992
3.884869	131.250136	5.577997
4.153581	125.099408	5.583002
4.120925	124.661730	5.588006
4.285048	133.393359	5.593011
4.276101	128.165361	5.598016
4.301892	133.365730	5.603021
4.638234	138.479784	5.608026
4.098963	126.026282	5.613030
4.268141	133.431548	5.618035
4.831226	139.630238	5.623040
4.198042	134.417174	5.628045
4.200763	117.206554	5.633050
4.277457	134.136200	5.638054
3.957094	134.796819	5.643059
4.526466	134.417263	5.648064
4.319403	140.473279	5.653069
4.829306	140.356075	5.658074
4.269285	141.984128	5.663078
3.868795	142.663550	5.668083
4.494867	147.131399	5.673088
4.194603	146.365238	5.678093
4.222041	138.417142	5.683098
4.580815	133.369164	5.688102
4.214339	141.639259	5.693107
4.755917	130.225990	5.698112
4.590251	137.461935	5.703117
4.504072	143.815498	5.708122
4.433969	140.938134	5.713126
4.371930	140.356338	5.718131
4.564597	129.918022	5.723136
4.586362	139.741139	5.728141
4.747386	132.180360	5.733146
4.410538	140.958356	5.738150
4.428812	134.416358	5.743155
4.613449	126.753832	5.748160
4.596203	145.194529	5.753165
4.674967	131.420456	5.758170
4.391047	141.452516	5.763174
4.989996	151.970363	5.768179
5.099680	137.194915	5.773184
4.776345	144.224464	5.778189
4.460359	144.270650	5.783194
4.281604	136.553970	5.788198
5.057085	142.324132	5.793203
5.317756	144.118626	5.798208
5.078138	141.378383	5.803213
4.856369	129.716981	5.808218
4.619938	130.671407	5.813222
4.583755	136.859000	5.818227
4.837946	137.044195	5.823232
4.568402	136.102412	5.828237
4.543437	135.919794	5.833242
5.128236	135.537836	5.838246
5.078700	138.225327	5.843251
5.157557	135.191897	5.848256
4.715474	146.219831	5.853261
4.380245	141.264086	5.858266
4.679500	147.503857	5.863270
5.357076	148.151464	5.868275
5.699477	141.366014	5.873280
4.888452	144.368216	5.878285
4.558970	134.773639	5.883290
4.624388	133.124825	5.888294
4.483492	142.017841	5.893299
4.994624	130.875060	5.898304
4.633815	141.947284	5.903309
4.666867	129.199032	5.908314
5.282224	142.890641	5.913318
4.947247	142.784764	5.918323
4.893443	134.944229	5.923328
4.400278	136.315106	5.928333
4.944534	134.544282	5.933338
5.143269	150.743117	5.938342
5.550621	140.657336	5.943347
4.681539	137.885390	5.948352
4.958885	138.674404	5.953357
4.741516	135.778841	5.958362
5.052655	125.964306	5.963366
4.483428	131.649613	5.968371
5.014298	126.018036	5.973376
4.458623	130.948279	5.978381
5.042996	133.128958	5.983386
5.352363	139.711992	5.988390
4.679297	142.284600	5.993395
4.993783	128.559247	5.998400
4.378573	132.812245	6.003405
4.886536	138.503839	6.008410
5.369888	135.581431	6.013414
4.875931	134.892882	6.018419
5.042183	130.798671	6.023424
4.931457	140.190013	6.028429
4.690927	138.417995	6.033434
4.788283	127.089711	6.038438
4.536297	133.234974	6.043443
5.009829	128.314658	6.048448
4.950258	142.718777	6.053453
4.804874	131.238464	6.058458
5.031178	145.212107	6.063462
4.889260	144.367509	6.068467
5.121987	129.212252	6.073472
4.583136	134.127222	6.078477
4.443335	139.973454	6.083482
5.208996	143.748871	6.088486
5.370414	136.684725	6.093491
5.087522	135.447636	6.098496
5.018534	132.054421	6.103501
4.878625	127.191654	6.108506
5.184393	126.834158	6.113510
5.005057	129.703205	6.118515
5.029671	139.399331	6.123520
4.745443	138.478817	6.128525
4.559428	123.433053	6.133530
4.546888	134.602903	6.138534
4.335214	141.526482	6.143539
4.818291	136.794498	6.148544
4.636790	145.709657	6.153549
5.224158	137.617435	6.158554
4.928217	132.060807	6.163558
4.785622	135.569523	6.168563
5.302956	133.230267	6.173568
4.807963	140.827528	6.178573
4.601680	129.043495	6.183578
4.802259	130.413922	6.188582
4.606310	145.304335	6.193587
5.279249	139.372231	6.198592
5.163530	138.827267	6.203597
5.059486	127.141209	6.208602
4.831945	129.166734	6.213606
4.745378	138.652387	6.218611
4.877186	129.969892	6.223616
4.972434	130.356999	6.228621
4.591531	134.061001	6.233626
4.814254	129.916870	6.238630
4.800074	137.296904	6.243635
5.009361	126.609236	6.248640
4.823603	137.609909	6.253645
4.953159	133.217699	6.258650
4.701377	125.458612	6.263654
4.561871	142.067597	6.268659
5.431837	135.601794	6.273664
5.159571	136.675692	6.278669
5.091963	131.807993	6.283674
4.888527	132.108731	6.288678
4.543135	136.126735	6.293683
4.882769	124.159634	6.298688
4.606298	124.864037	6.303693
4.547902	130.061695	6.308698
4.981883	130.981340	6.313702
5.231690	150.430802	6.318707
5.363583	140.508129	6.323712
4.737507	137.786930	6.328717
4.776153	145.766166	6.333722
5.031194	132.470834	6.338726
4.634453	141.928853	6.343731
5.036994	138.250256	6.348736
4.935490	135.409418	6.353741
4.815633	141.853643	6.358746
5.052996	126.640720	6.363750
5.009812	134.832003	6.368755
5.001239	128.215096	6.373760
4.828724	126.011722	6.378765
4.958656	127.507039	6.383770
4.642233	132.282976	6.388774
4.571605	134.524510	6.393779
4.759159	126.386980	6.398784
4.790454	136.645197	6.403789
4.858071	134.239923	6.408794
5.076328	134.101691	6.413798
4.434377	138.925150	6.418803
4.944584	131.559934	6.423808
4.900079	141.965994	6.428813
4.813295	127.464747	6.433818
5.132234	129.041365	6.438822
4.689316	144.954131	6.443827
4.972355	126.858320	6.448832
4.681977	136.524397	6.453837
5.128371	132.326458	6.458842
4.923713	134.427513	6.463846
5.093722	127.105777	6.468851
4.993232	121.379519	6.473856
4.801275	134.924744	6.478861
4.969917	141.687872	6.483866
4.608737	139.365179	6.488870
4.588297	135.701820	6.493875
4.815641	136.454328	6.498880
5.052616	153.292600	6.503885
5.165867	140.379997	6.508890
5.016274	139.460666	6.513894
4.701866	135.491910	6.518899
4.775872	132.734475	6.523904
4.636569	130.728404	6.528909
4.862621	127.210161	6.533914
5.477047	132.910487	6.538918
4.951252	140.417634	6.543923
5.103588	135.449252	6.548928
4.608440	149.570027	6.553933
4.746652	145.217594	6.558938
4.869012	131.651863	6.563942
4.559605	140.817881	6.568947
4.577741	134.120885	6.573952
5.035504	144.243106	6.578957
4.712771	141.288020	6.583962
5.661705	139.691463	6.588966
4.922291	145.355816	6.593971
4.711632	127.542511	6.598976
4.727886	136.607204	6.603981
4.458370	133.896927	6.608986
5.010897	138.717901	6.613990
5.273153	140.553275	6.618995
4.745526	145.941052	6.624000
4.568637	146.917845	6.629005
4.791229	144.105637	6.634010
5.179493	147.560174	6.639014
4.937815	142.513936	6.644019
4.619822	132.433530	6.649024
4.527141	143.008438	6.654029
4.981925	142.165845	6.659034
5.447031	149.170711	6.664038
4.641766	152.868025	6.669043
5.362880	139.057207	6.674048
4.669115	139.541853	6.679053
4.399977	135.006080	6.684058
5.239495	133.736599	6.689062
4.853063	142.285041	6.694067
4.756528	137.004240	6.699072
4.805332	139.236670	6.704077
4.882817	140.230804	6.709082
5.313629	140.420136	6.714086
4.702670	145.166007	6.719091
4.985594	136.083503	6.724096
4.853411	144.260175	6.729101
4.577269	138.308167	6.734106
4.951651	133.536161	6.739110
4.935027	144.304867	6.744115
5.509929	144.436964	6.749120
4.726169	144.109904	6.754125
4.752397	138.582205	6.759130
4.651677	142.315349	6.764134
4.693985	135.045129	6.769139
4.852843	141.025190	6.774144
5.166339	138.277921	6.779149
5.375375	140.301910	6.784154
4.824600	133.718802	6.789158
4.691925	133.881976	6.794163
5.066989	125.816487	6.799168
4.924391	131.258203	6.804173
4.737729	142.569060	6.809178
4.822493	138.218623	6.814182
4.764534	136.759856	6.819187
5.093826	130.482638	6.824192
5.325235	137.672578	6.829197
4.711077	129.324522	6.834202
5.302914	126.217550	6.839206
5.059538	136.135729	6.844211
4.691959	133.326828	6.849216
4.667991	140.148417	6.854221
4.816905	137.955106	6.859226
4.976080	129.806173	6.864230
4.720504	140.131204	6.869235
4.964955	130.877528	6.874240
4.834600	134.754486	6.879245
4.510470	133.950914	6.884250
4.966789	128.751711	6.889254
4.203393	135.900392	6.894259
4.723276	138.100604	6.899264
5.440150	142.839044	6.904269
4.694946	142.948895	6.909274
5.277182	136.338071	6.914278
4.692813	142.101666	6.919283
4.970824	129.565204	6.924288
4.873642	137.787042	6.929293
5.001593	143.458712	6.934298
5.127437	130.639066	6.939302
4.737772	137.299299	6.944307
4.524152	133.548963	6.949312
4.916382	138.708098	6.954317
5.037406	132.314614	6.959322
4.664399	137.792206	6.964326
4.722196	145.173690	6.969331
4.983244	136.999402	6.974336
5.016978	142.593996	6.979341
5.080282	138.961889	6.984346
5.257671	134.230046	6.989350
4.950543	140.121313	6.994355
5.133193	143.718591	6.999360
5.077183	138.146750	7.004365
4.761776	140.676326	7.009370
4.676745	141.733727	7.014374
4.584000	134.658537	7.019379
4.664819	142.479349	7.024384
4.428364	136.843857	7.029389
4.760603	136.023508	7.034394
4.796966	137.217028	7.039398
5.200924	144.199775	7.044403
5.013776	144.485322	7.049408
5.054677	146.029304	7.054413
5.017342	146.807204	7.059418
4.865021	136.992058	7.064422
4.433275	144.272598	7.069427
5.092212	133.780664	7.074432
5.151916	133.277987	7.079437
4.606463	143.043892	7.084442
5.089615	136.875590	7.089446
4.594364	136.851613	7.094451
4.998608	140.904758	7.099456
5.112536	138.419509	7.104461
4.657810	136.604913	7.109466
5.069078	136.034844	7.114470
4.969008	144.677902	7.119475
4.989322	137.483870	7.124480
4.931359	140.103073	7.129485
4.816491	140.639951	7.134490
4.974633	142.912304	7.139494
4.720812	137.731920	7.144499
4.969030	148.791578	7.149504
4.855278	138.742642	7.154509
4.839619	148.223587	7.159514
5.200623	133.361557	7.164518
5.200553	148.297403	7.169523
5.274624	135.128319	7.174528
4.742349	138.672398	7.179533
5.053464	144.970431	7.184538
5.103990	145.256936	7.189542
4.815763	144.836904	7.194547
5.098236	147.583433	7.199552
5.044571	142.248500	7.204557
4.796478	140.392241	7.209562
5.359933	131.927268	7.214566
4.531565	137.918673	7.219571
4.697055	135.561434	7.224576
5.126815	133.567998	7.229581
4.633840	144.414034	7.234586
4.940388	134.568573	7.239590
4.522345	141.005442	7.244595
5.087072	141.990150	7.249600
5.107924	140.360929	7.254605
4.862945	150.700133	7.259610
4.899405	138.416404	7.264614
4.955512	142.109312	7.269619
4.991228	140.740361	7.274624
4.647342	136.390227	7.279629
4.957934	138.379423	7.284634
4.948697	141.658574	7.289638
4.555029	141.973112	7.294643
5.046062	142.966130	7.299648
5.216792	135.055835	7.304653
4.556727	134.978428	7.309658
4.491636	131.932611	7.314662
4.728139	142.642922	7.319667
5.130859	135.819609	7.324672
5.087059	142.887890	7.329677
4.673970	144.771469	7.334682
4.605255	142.545604	7.339686
4.989791	151.954750	7.344691
4.932249	141.093488	7.349696
5.090097	136.883528	7.354701
4.751755	140.938400	7.359706
4.916525	137.451843	7.364710
4.562630	143.053008	7.369715
4.745474	136.621424	7.374720
4.881380	137.736172	7.379725
4.998707	143.020365	7.384730
4.968184	135.530536	7.389734
4.900172	146.465428	7.394739
5.024746	141.539331	7.399744
4.927573	140.747876	7.404749
4.988423	148.021322	7.409754
5.112312	141.896300	7.414758
4.854108	145.695093	7.419763
5.175811	140.456737	7.424768
4.912330	140.029689	7.429773
4.706209	145.272497	7.434778
5.059119	141.029001	7.439782
4.933933	149.350115	7.444787
4.636102	140.076465	7.449792
4.910652	147.313474	7.454797
4.590709	149.274297	7.459802
4.974283	148.395336	7.464806
4.879850	148.764521	7.469811
5.202398	142.266892	7.474816
4.833766	155.061378	7.479821
5.042564	152.846086	7.484826
4.778110	140.441532	7.489830
4.407770	143.371957	7.494835
4.843559	150.526916	7.499840
5.212942	146.113181	7.504845
5.045818	154.121295	7.509850
4.900319	139.230557	7.514854
4.721691	144.756978	7.519859
5.039548	136.285952	7.524864
4.766691	136.831610	7.529869
4.922422	142.853286	7.534874
5.184033	137.409157	7.539878
4.475999	128.088653	7.544883
5.109841	144.653160	7.549888
4.574566	145.628807	7.554893
4.841076	141.740441	7.559898
5.127450	134.112690	7.564902
4.994512	140.157165	7.569907
4.757170	140.149978	7.574912
4.709714	135.892892	7.579917
4.580988	142.297370	7.584922
5.165586	139.314907	7.589926
4.968804	131.449180	7.594931
5.120549	135.161997	7.599936
4.802944	142.086251	7.604941
4.522308	148.549184	7.609946
5.173641	132.702341	7.614950
4.977795	143.100328	7.619955
4.935863	138.291903	7.624960
4.432650	129.986683	7.629965
4.461307	147.876085	7.634970
4.504592	142.295110	7.639974
4.621605	143.922151	7.644979
5.185803	143.394707	7.649984
5.031323	131.042638	7.654989
4.669188	140.697743	7.659994
5.001777	137.466624	7.664998
5.010148	143.444807	7.670003
4.858879	149.520612	7.675008
4.930767	150.784530	7.680013
5.029116	153.322451	7.685018
5.362846	143.096276	7.690022
5.064457	151.004607	7.695027
5.064385	139.166315	7.700032
4.627161	136.194256	7.705037
4.583199	149.156480	7.710042
5.052858	145.767979	7.715046
4.860687	151.388257	7.720051
5.202648	150.835306	7.725056
5.044246	145.042129	7.730061
4.750594	135.764668	7.735066
4.513061	128.427292	7.740070
4.466090	149.979344	7.745075
4.558247	144.979202	7.750080
5.018010	137.817985	7.755085
4.608773	147.635448	7.760090
5.118877	144.332397	7.765094
4.775275	145.841335	7.770099
4.742034	141.645307	7.775104
5.067136	138.178078	7.780109
4.985851	143.955091	7.785114
5.162996	139.068265	7.790118
5.059939	142.760646	7.795123
4.958007	142.919033	7.800128
4.858038	150.717378	7.805133
4.545959	146.805204	7.810138
4.782123	138.913192	7.815142
5.094207	144.559358	7.820147
5.058924	155.802363	7.825152
5.140666	146.782814	7.830157
5.150549	147.809620	7.835162
4.990748	144.171121	7.840166
4.744599	144.338211	7.845184
4.807911	138.247665	7.850202
4.877916	134.371310	7.855219
4.898528	152.143743	7.860237
5.148865	143.152480	7.865254
4.498230	141.054482	7.870272
4.785752	156.406041	7.875290
5.108742	136.933186	7.880307
4.823811	146.573877	7.885325
5.004542	143.248288	7.890342
5.132001	146.683976	7.895360
4.737911	141.955286	7.900378
5.106786	144.384617	7.905395
4.759392	143.911872	7.910413
5.529450	136.483760	7.915430
4.815071	137.301993	7.920448
4.567033	139.821064	7.925466
4.993023	133.147068	7.930483
5.081487	140.000027	7.935501
5.045261	142.820614	7.940518
4.932104	146.300076	7.945536
4.844576	142.536603	7.950554
5.399216	135.823641	7.955571
4.480349	142.208632	7.960589
4.995531	138.130428	7.965606
4.936789	145.170400	7.970624
4.894071	143.665670	7.975642
4.958163	136.230719	7.980659
4.713709	147.180993	7.985677
4.850566	143.142758	7.990694
4.620834	144.308383	7.995712
5.011504	144.171974	8.000730
5.466270	134.861726	8.005747
5.207363	136.470521	8.010765
5.460782	140.757542	8.015782
5.391723	139.373671	8.020800
5.148137	146.022729	8.025818
5.209913	140.655054	8.030835
5.136138	146.564508	8.035853
5.061329	142.363582	8.040870
4.944600	133.543076	8.045888
4.871668	140.758814	8.050906
5.181290	143.535020	8.055923
4.706904	149.188133	8.060941
5.096502	143.504346	8.065958
5.329295	137.762929	8.070976
4.785165	143.376410	8.075994
4.683664	139.356354	8.081011
4.911197	144.988535	8.086029
5.092844	142.609483	8.091046
5.359799	141.832816	8.096064
4.835890	143.754253	8.101082
5.211099	137.577279	8.106099
5.056045	146.860100	8.111117
5.032354	139.139034	8.116134
5.288189	139.235043	8.121152
5.187921	144.287142	8.126170
4.983507	152.933910	8.131187
4.987970	146.382340	8.136205
5.028073	142.693662	8.141222
5.205293	141.691141	8.146240
5.223640	148.608666	8.151258
5.335646	145.770272	8.156275
5.253710	142.577092	8.161293
5.686885	143.330255	8.166310
5.274860	139.853976	8.171328
5.264446	147.672169	8.176346
5.222321	140.708160	8.181363
5.376324	145.540801	8.186381
5.160041	145.233822	8.191398
5.357023	143.167943	8.196416
5.193536	147.093870	8.201434
5.428829	140.840856	8.206451
5.127190	145.435191	8.211469
5.352837	140.524809	8.216486
5.445734	135.947501	8.221504
5.071290	133.591920	8.226522
5.593459	136.694769	8.231539
5.379526	137.883179	8.236557
5.208155	144.117076	8.241574
5.618283	141.393201	8.246592
5.373724	144.432405	8.251610
5.228277	143.902973	8.256627
5.127431	139.639833	8.261645
5.345472	139.044340	8.266662
5.576375	145.202981	8.271680
4.991567	139.222814	8.276698
5.427024	137.119804	8.281715
5.560746	147.260165	8.286733
5.249137	140.600029	8.291750
5.227715	144.364990	8.296768
5.280770	146.183974	8.301786
5.711351	135.031466	8.306803
5.565132	145.019764	8.311821
5.523362	139.696612	8.316838
5.476929	134.083873	8.321856
5.053244	142.177834	8.326874
5.599006	135.699769	8.331891
5.287062	133.555349	8.336909
5.364315	134.411261	8.341926
5.266888	135.704600	8.346944
5.241350	153.686179	8.351962
5.523992	140.552894	8.356979
5.096597	134.699688	8.361997
5.239737	142.026942	8.367014
5.472339	133.890456	8.372032
5.397830	135.713522	8.377050
5.918016	132.953579	8.382067
5.712777	132.991997	8.387085
5.138955	139.869183	8.392102
5.332418	138.217236	8.397120
5.360926	142.334161	8.402138
4.910070	135.541082	8.407155
5.222267	146.628735	8.412173
5.172860	143.332666	8.417190
5.744256	141.571385	8.422208
5.419390	141.123533	8.427226
5.497691	136.466452	8.432243
5.562487	149.631142	8.437261
5.557904	144.078151	8.442278
5.516836	139.701570	8.447296
5.557358	145.432292	8.452314
5.466606	132.092080	8.457331
5.440290	144.791302	8.462349
5.932588	149.306202	8.467366
5.978973	140.747456	8.472384
5.060957	146.065724	8.477402
5.299929	142.068390	8.482419
5.152347	147.304571	8.487437
5.572636	144.557024	8.492454
6.250338	144.924999	8.497472
5.712336	142.336124	8.502490
5.649549	130.329533	8.507507
5.113749	135.307440	8.512525
5.519817	138.778637	8.517542
5.936118	146.785995	8.522560
5.571305	151.446968	8.527578
5.627547	139.626953	8.532595
5.777361	141.086910	8.537613
5.622913	143.815458	8.542630
5.446175	136.209733	8.547648
5.510126	144.013191	8.552666
5.813576	145.032688	8.557683
5.961699	143.252109	8.562701
5.689056	137.930192	8.567719
5.460650	134.516837	8.572736
5.449932	138.242263	8.577754
6.059284	137.705756	8.582771
5.785762	139.269493	8.587789
5.457525	131.248731	8.592807
5.326863	135.336792	8.597824
5.684562	144.094837	8.602842
5.914766	141.610402	8.607859
6.062587	141.713762	8.612877
5.287664	151.440214	8.617895
5.821278	140.628243	8.622912
5.821388	141.713904	8.627930
5.981117	139.155240	8.632947
5.714254	129.537656	8.637965
5.587267	136.746031	8.642983
5.385013	132.523927	8.648000
5.916423	147.487235	8.653018
5.996152	151.940147	8.658035
6.006280	136.410016	8.663053
5.778229	142.542292	8.668071
5.127005	133.072908	8.673088
5.455722	150.223049	8.678106
5.806014	146.019047	8.683123
6.260032	148.248941	8.688141
6.159347	148.577174	8.693159
6.129910	147.007264	8.698176
5.808892	143.564149	8.703194
5.434345	147.182133	8.708211
5.655873	142.603730	8.713229
5.826024	147.620037	8.718247
6.274996	152.037549	8.723264
5.886181	151.924680	8.728282
5.533162	153.939424	8.733299
5.586159	142.839389	8.738317
5.953003	155.531050	8.743335
6.201609	146.584233	8.748352
6.026430	147.397404	8.753370
6.027739	145.873197	8.758387
5.690233	137.800230	8.763405
5.800699	146.590460	8.768423
6.289437	143.481984	8.773440
5.534380	144.669445	8.778458
5.908968	137.384952	8.783475
6.219373	146.718371	8.788493
5.829291	154.696660	8.793511
5.651771	144.168967	8.798528
5.644237	151.781599	8.803546
6.162105	147.677729	8.808563
6.260765	147.173402	8.813581
6.073208	150.737028	8.818599
5.732851	153.279942	8.823616
5.721585	145.708406	8.828634
6.149681	157.475407	8.833651
6.271916	149.564368	8.838669
5.937858	155.536440	8.843687
5.948315	146.825505	8.848704
5.774583	148.165436	8.853722
6.111833	151.884021	8.858739
6.363522	143.608869	8.863757
5.972398	153.670015	8.868775
5.653005	148.901293	8.873792
5.657924	151.693385	8.878810
5.960759	150.311567	8.883827
6.041949	145.003980	8.888845
6.089750	157.757939	8.893863
6.467941	149.680825	8.898880
6.724503	145.762797	8.903898
5.844876	147.799576	8.908915
5.932061	139.903466	8.913933
5.866768	144.233798	8.918951
6.083702	143.502786	8.923968
6.413905	148.282749	8.928986
6.234723	151.974452	8.934003
6.123331	139.745064	8.939021
5.546509	144.713582	8.944039
6.022359	143.235403	8.949056
6.267850	147.141831	8.954074
6.108065	150.287750	8.959091
6.327609	144.977555	8.964109
6.196019	154.767935	8.969127
6.291049	144.857327	8.974144
6.083826	153.564489	8.979162
6.259990	154.673228	8.984179
6.106188	143.289831	8.989197
6.177298	151.092177	8.994215
6.154134	150.221833	8.999232
5.955160	149.482998	9.004250
6.236103	152.569764	9.009267
6.667452	152.704714	9.014285
6.062880	151.419998	9.019303
6.276213	151.052440	9.024320
5.719697	139.340453	9.029338
6.122031	154.983384	9.034355
6.193698	149.491098	9.039373
6.212544	154.770791	9.044391
6.550853	150.177359	9.049408
6.222906	155.249133	9.054426
6.319363	161.501292	9.059443
6.781555	152.729487	9.064461
6.211892	147.864041	9.069479
5.865680	147.801339	9.074496
6.114187	154.648320	9.079514
6.179926	153.748357	9.084531
6.475860	152.067830	9.089549
6.349548	155.574588	9.094567
6.419885	150.391758	9.099584
6.777556	146.817726	9.104602
6.396916	151.080403	9.109619
5.985809	139.569823	9.114637
5.962076	150.309020	9.119655
6.295878	149.171673	9.124672
6.556371	154.697746	9.129690
6.255306	161.775454	9.134707
6.357740	146.672727	9.139725
6.567333	155.924023	9.144743
6.528745	157.056733	9.149760
6.523819	144.069198	9.154778
6.359667	146.761390	9.159795
6.788072	148.938472	9.164813
6.055372	143.656627	9.169831
5.699914	138.155113	9.174848
6.063740	133.807004	9.179866
6.220958	144.388644	9.184883
6.215503	147.204440	9.189901
6.316297	146.491511	9.194919
6.333647	151.560011	9.199936
6.449482	142.346709	9.204954
6.434773	145.078744	9.209971
6.760751	145.488859	9.214989
6.563317	148.293523	9.220007
6.410931	151.596070	9.225024
6.416829	145.807932	9.230042
6.213738	152.232951	9.235059
6.367257	142.650887	9.240077
6.368014	149.921423	9.245095
6.136028	143.838986	9.250112
6.417728	138.361336	9.255130
6.358860	149.071291	9.260147
6.821290	152.429581	9.265165
6.642983	152.448028	9.270183
6.340123	152.858229	9.275200
6.682849	142.208513	9.280218
6.196842	148.447221	9.285235
6.955307	144.555184	9.290253
6.601108	147.217009	9.295271
6.106863	153.053085	9.300288
6.567847	154.600286	9.305306
6.762644	165.239199	9.310323
7.430419	160.682824	9.315341
6.738617	152.658702	9.320359
6.482942	150.578098	9.325376
6.593159	149.396672	9.330394
6.573579	149.264181	9.335411
6.606096	143.869505	9.340429
6.688390	139.132912	9.345447
6.605069	154.305539	9.350464
6.435331	143.167604	9.355482
6.292785	148.160020	9.360499
6.641188	151.583398	9.365517
6.904730	149.516621	9.370535
6.569043	142.077644	9.375552
6.567174	144.984394	9.380570
6.912804	155.448348	9.385587
6.567006	149.427808	9.390605
6.501043	151.252700	9.395623
7.032285	156.727152	9.400640
7.146372	146.097255	9.405658
7.056745	150.163152	9.410675
6.752179	154.839991	9.415693
6.635195	156.142687	9.420711
6.303261	152.521399	9.425728
6.806913	148.006359	9.430746
7.046842	146.372420	9.435763
6.872657	148.188918	9.440781
6.834678	149.813805	9.445799
6.633907	147.538473	9.450816
7.062476	147.680167	9.455834
6.485914	155.542333	9.460851
6.737813	154.111644	9.465869
7.184008	148.062460	9.470887
6.854179	154.119074	9.475904
6.840936	140.031533	9.480922
6.931023	153.040820	9.485939
6.623791	155.783690	9.490957
6.948928	151.681427	9.495975
6.540079	155.311065	9.500992
6.638396	153.569794	9.506010
6.731875	157.231667	9.511027
6.793663	147.140053	9.516045
6.726983	154.244377	9.521063
6.408467	158.402715	9.526080
7.066201	157.044529	9.531098
6.974507	162.253078	9.536115
6.850213	156.381073	9.541133
7.514737	157.259152	9.546151
6.934290	156.863715	9.551168
6.880849	144.540099	9.556186
6.765267	150.090014	9.561203
6.754481	150.319048	9.566221
7.170123	144.905743	9.571239
6.576183	151.839711	9.576256
7.169525	152.987632	9.581274
6.860218	154.964014	9.586291
6.986065	147.522599	9.591309
7.037113	146.946794	9.596327
6.488767	153.289878	9.601344
7.426229	148.454846	9.606362
7.241855	156.975427	9.611379
7.036136	153.911963	9.616397
6.831650	144.322527	9.621415
6.746498	159.523844	9.626432
7.026618	160.840446	9.631450
7.349935	163.368385	9.636467
7.080946	157.146547	9.641485
6.960039	152.618302	9.646503
6.928515	157.785926	9.651520
7.531410	165.470769	9.656538
7.319261	153.471640	9.661555
6.944528	158.096292	9.666573
6.648603	153.611075	9.671591
6.704658	156.694988	9.676608
7.246730	158.674504	9.681626
7.753898	160.378606	9.686643
7.260175	172.001982	9.691661
7.000175	159.126731	9.696679
6.519733	170.258920	9.701696
6.975442	161.418697	9.706714
7.131099	169.570781	9.711731
6.978079	160.894759	9.716749
7.601944	159.115840	9.721767
7.730720	166.757746	9.726784
7.334885	157.816593	9.731802
7.087244	155.479134	9.736819
6.595177	163.366015	9.741837
7.217529	153.288098	9.746855
7.344743	164.265716	9.751872
7.477410	163.270130	9.756890
6.900408	155.130309	9.761907
7.089901	159.711292	9.766925
7.830187	152.868439	9.771943
7.116004	160.758346	9.776960
7.080884	155.595090	9.781978
7.542387	159.527845	9.786995
7.264302	158.889684	9.792013
6.792811	159.386097	9.797031
7.261094	159.584719	9.802048
7.312708	160.012308	9.807066
7.679120	168.658563	9.812083
7.360715	160.626790	9.817101
7.176296	151.501255	9.822119
7.051016	155.935598	9.827136
7.348444	150.840479	9.832154
7.586162	158.329728	9.837171
7.346182	156.054188	9.842189
7.718842	156.049962	9.847207
7.305547	160.235679	9.852224
6.840142	162.233211	9.857242
6.775513	152.628306	9.862259
7.368626	153.167231	9.867277
7.643797	149.852181	9.872295
7.669925	159.586451	9.877312
7.474462	159.086894	9.882330
7.512246	160.251892	9.887347
7.354202	169.528879	9.892365
7.606141	146.867293	9.897383
7.206386	159.870806	9.902400
7.522479	151.847537	9.907418
7.492343	161.502211	9.912435
7.511795	162.367125	9.917453
7.463601	157.070213	9.922471
7.432006	161.310102	9.927488
7.418107	162.423190	9.932506
7.378506	155.966834	9.937523
7.552296	163.535461	9.942541
7.697114	149.776730	9.947559
7.576995	154.144003	9.952576
7.600738	161.808570	9.957594
7.483309	153.530928	9.962611
7.125657	158.181321	9.967629
7.627184	161.126453	9.972647
7.745100	158.650031	9.977664
7.713471	167.658042	9.982682
7.902963	157.713786	9.987699
7.251978	158.007786	9.992717
7.133566	154.261742	9.997735
7.306129	153.386169	10.002752
7.711735	159.072675	10.007770
7.938352	158.422200	10.012787
7.280794	163.958680	10.017805
7.392947	162.751707	10.022823
7.379324	153.482821	10.027840
7.314157	161.192788	10.032858
7.431597	157.959095	10.037875
7.387317	160.004660	10.042893
7.679224	156.980474	10.047911
7.796640	157.000212	10.052928
8.096444	155.060323	10.057946
7.660067	151.562588	10.062963
7.285710	168.257362	10.067981
7.459609	159.369505	10.072999
7.435926	156.545924	10.078016
7.133333	155.564463	10.083034
7.712551	162.527202	10.088051
7.911372	169.179966	10.093069
8.021467	159.055579	10.098087
7.533954	163.814550	10.103104
7.531465	165.396046	10.108122
7.967390	168.351394	10.113139
8.087301	167.439839	10.118157
8.007166	162.779019	10.123175
7.855764	166.248662	10.128192
7.926666	165.922215	10.133210
7.863166	160.040742	10.138227
7.884297	160.110183	10.143245
8.082075	160.944176	10.148263
7.907108	166.459163	10.153280
7.609867	166.953690	10.158298
7.982444	158.997358	10.163315
7.820652	166.368944	10.168333
7.944432	156.864081	10.173351
7.809346	164.670137	10.178368
7.685466	169.079021	10.183386
7.421590	158.826680	10.188403
7.635474	165.265672	10.193421
7.634662	165.205994	10.198439
8.011828	176.062656	10.203456
7.997219	157.655291	10.208474
8.233794	169.142871	10.213491
8.150061	161.847682	10.218509
7.844596	154.643820	10.223527
8.179735	161.736074	10.228544
7.910639	159.143196	10.233562
7.940134	154.449530	10.238579
7.986845	161.479402	10.243597
8.111136	154.372719	10.248615
8.291159	155.887931	10.253632
8.037221	151.610757	10.258650
7.964965	151.704205	10.263667
7.896612	161.083980	10.268685
8.039875	151.503509	10.273703
7.946802	158.615099	10.278720
7.861553	164.608391	10.283738
8.010716	153.269329	10.288755
7.724254	158.274688	10.293773
7.770339	156.298568	10.298791
7.776085	147.821881	10.303808
8.240250	155.834413	10.308826
8.172418	149.215208	10.313843
7.732522	160.448368	10.318861
8.142902	150.390834	10.323879
8.554887	157.423788	10.328896
8.201421	162.673095	10.333914
8.015918	150.799199	10.338931
7.839389	159.867634	10.343949
7.980396	153.730275	10.348967
7.980505	150.757833	10.353984
8.393866	171.277621	10.359002
8.470744	160.921735	10.364019
7.895638	166.719915	10.369037
7.830014	170.643234	10.374055
8.511068	168.593494	10.379072
8.458469	172.748299	10.384090
8.103961	158.928459	10.389107
7.833536	158.140792	10.394125
8.558005	163.490493	10.399143
8.409951	166.890192	10.404160
7.532446	164.669733	10.409178
8.133781	160.306728	10.414195
8.206081	173.848940	10.419213
8.754608	172.327887	10.424231
8.970204	170.647245	10.429248
8.119524	162.420652	10.434266
7.910913	161.080597	10.439283
8.463981	163.509652	10.444301
8.600625	165.031619	10.449319
8.332857	154.013075	10.454336
7.537867	161.549514	10.459354
8.652542	160.628235	10.464371
8.843855	156.871833	10.469389
7.887438	161.833191	10.474407
8.332882	164.979547	10.479424
8.693680	168.833316	10.484442
8.577107	161.618975	10.489459
8.059049	162.507621	10.494477
7.867003	159.874345	10.499495
8.751707	172.106716	10.504512
8.646478	174.256441	10.509530
8.390131	155.779424	10.514547
8.159827	160.643505	10.519565
8.443355	158.352723	10.524583
8.993063	167.932898	10.529600
8.811606	166.983065	10.534618
8.443633	154.664236	10.539635
8.334672	157.653929	10.544653
8.296188	149.603823	10.549671
8.279000	148.107740	10.554688
7.897758	157.842324	10.559706
8.761086	161.116108	10.564723
8.937193	173.241069	10.569741
8.301441	168.919205	10.574759
8.709401	162.636143	10.579776
8.235614	160.024645	10.584794
8.431646	159.435733	10.589811
8.869175	165.808348	10.594829
8.485185	163.943368	10.599847
9.035672	153.589480	10.604864
8.497089	157.706347	10.609882
8.503679	152.028545	10.614899
8.051322	158.908916	10.619917
8.436940	169.316163	10.624935
8.521518	155.311203	10.629952
8.508335	169.093925	10.634970
8.997349	164.379201	10.639987
9.105015	166.805026	10.645005
8.881959	156.319128	10.650023
8.668339	149.823600	10.655040
8.177971	149.177469	10.660058
8.311218	152.792126	10.665075
8.272185	159.302050	10.670093
8.724245	170.800259	10.675111
9.087285	154.786002	10.680128
9.082779	161.044414	10.685146
9.033216	157.202448	10.690163
8.322777	157.382636	10.695181
8.857451	165.832290	10.700199
8.736743	163.897917	10.705216
8.644874	160.908239	10.710234
8.674185	163.421998	10.715251
9.469972	166.955591	10.720269
8.759974	161.121131	10.725287
8.635540	157.237177	10.730304
8.573916	161.065202	10.735322
8.630819	155.616236	10.740339
8.847764	156.150618	10.745357
8.622024	166.630962	10.750375
8.917093	164.549808	10.755392
8.625778	170.496295	10.760410
9.249224	164.649868	10.765427
8.942073	171.072162	10.770445
8.918443	168.141281	10.775463
8.990993	170.714576	10.780480
8.494176	167.368251	10.785498
8.960608	164.654540	10.790515
9.208611	161.832836	10.795533
8.782179	167.715159	10.800551
9.262794	166.763222	10.805568
8.662727	166.923070	10.810586
8.856472	161.721022	10.815603
9.307749	163.465383	10.820621
8.944871	156.980470	10.825639
8.695657	153.724975	10.830656
8.843421	160.142704	10.835674
8.995588	163.098053	10.840691
9.557256	162.647859	10.845709
9.071490	153.862713	10.850727
8.555659	147.518375	10.855744
8.898903	160.623942	10.860762
9.095959	162.262726	10.865779
9.194638	165.355783	10.870797
8.865297	172.352696	10.875815
8.867984	166.363093	10.880832
9.085057	159.163073	10.885850
8.919208	160.757381	10.890867
9.179688	170.376278	10.895885
8.806059	165.735909	10.900903
9.268180	168.011878	10.905920
9.145780	173.521839	10.910938
8.825879	170.400416	10.915955
9.298516	168.525129	10.920973
9.086315	173.720889	10.925991
9.006255	170.830349	10.931008
8.977458	169.474919	10.936026
8.552194	165.113971	10.941043
9.102124	163.138294	10.946061
8.799337	158.909747	10.951079
8.889272	165.601552	10.956096
9.148439	172.077674	10.961114
9.502749	176.942249	10.966131
9.405704	171.911697	10.971149
8.924553	170.563586	10.976167
8.984783	166.366873	10.981184
9.733165	173.899688	10.986202
9.442211	166.087686	10.991219
9.279163	161.010613	10.996237
9.589329	168.267694	11.001255
9.318602	159.105103	11.006272
9.024635	156.465608	11.011290
8.809244	162.485473	11.016307
9.259938	163.684005	11.021325
9.727728	176.634501	11.026343
9.183049	173.920436	11.031360
9.502987	168.471535	11.036378
9.477896	173.590828	11.041395
9.277280	167.796970	11.046413
9.016270	169.541786	11.051431
9.274584	176.655475	11.056448
9.960352	177.154730	11.061466
9.079972	172.337655	11.066483
9.637060	168.442254	11.071501
9.570311	175.896870	11.076519
9.410267	162.034127	11.081536
9.372414	169.815579	11.086554
9.135534	167.318662	11.091571
10.082567	172.851451	11.096589
9.367971	167.020860	11.101607
9.175019	168.761391	11.106624
9.610555	169.722458	11.111642
9.404516	171.569162	11.116659
9.856974	168.813447	11.121677
9.661203	180.251592	11.126695
9.415272	168.933013	11.131712
9.261489	170.112059	11.136730
9.519195	163.271760	11.141747
10.323701	171.168197	11.146765
9.421450	172.911874	11.151783
9.313401	165.528957	11.156800
9.425071	169.992679	11.161818
9.562497	163.540314	11.166835
9.770106	162.877020	11.171853
9.541260	170.164380	11.176871
9.609015	164.808389	11.181888
9.673999	170.973940	11.186906
9.809792	173.559478	11.191923
9.550563	155.073445	11.196941
9.577017	169.070887	11.201959
9.985344	172.314536	11.206976
9.647976	166.516725	11.211994
9.149688	165.682490	11.217011
10.266852	162.151140	11.222029
9.712610	172.578499	11.227047
9.409336	159.277667	11.232064
9.607686	169.013528	11.237082
10.231373	169.528760	11.242099
9.972749	163.081258	11.247117
9.368874	167.435496	11.252135
9.441759	164.637902	11.257152
9.823922	161.448193	11.262170
9.837142	178.196234	11.267187
10.192556	166.967052	11.272205
10.044884	174.513156	11.277223
9.773570	168.231719	11.282240
9.420902	160.984715	11.287258
9.528944	175.480667	11.292275
9.841422	170.635647	11.297293
9.949582	172.928861	11.302311
9.340101	172.683102	11.307328
9.871235	167.491634	11.312346
9.995980	167.172581	11.317363
10.208539	161.096657	11.322381
10.049444	170.121360	11.327399
10.006323	174.763809	11.332416
9.932359	175.491799	11.337434
10.114363	180.313779	11.342451
10.591076	164.736222	11.347469
9.577295	169.665489	11.352487
9.909577	168.588334	11.357504
10.445817	173.702275	11.362522
9.736902	171.465033	11.367539
10.022151	158.684757	11.372557
10.073745	170.264250	11.377575
9.792211	170.320859	11.382592
10.106539	165.623866	11.387610
9.972294	166.828270	11.392627
10.387447	170.310682	11.397645
10.024192	169.919296	11.402663
10.259080	164.912800	11.407680
10.115896	156.004890	11.412698
9.575011	159.377394	11.417715
9.890083	175.198020	11.422733
9.784106	180.979964	11.427751
9.885921	176.947177	11.432768
10.513557	176.404667	11.437786
10.301158	179.643984	11.442803
10.042650	174.458702	11.447821
9.986137	181.526742	11.452839
9.963516	175.509520	11.457856
10.304947	178.785675	11.462874
9.978613	188.312923	11.467891
9.922875	178.444704	11.472909
10.112999	180.488487	11.477927
10.249232	177.277110	11.482944
10.022620	167.918309	11.487962
9.792185	182.015716	11.492979
10.685696	185.622454	11.497997
10.346922	185.628018	11.503015
10.290283	188.672683	11.508032
10.377240	180.382139	11.513050
10.242214	181.226927	11.518067
10.123922	174.457788	11.523085
10.383737	183.272117	11.528103
10.189757	181.724668	11.533120
10.435458	170.903861	11.538138
10.261106	190.571651	11.543155
10.228070	180.813498	11.548173
10.585105	180.445655	11.553191
11.100462	183.524329	11.558208
10.663862	179.818353	11.563226
10.192964	181.248733	11.568243
10.450607	181.802024	11.573261
10.271100	174.171470	11.578279
10.188717	185.756055	11.583296
10.301370	170.304600	11.588314
10.084285	178.640948	11.593331
10.612348	184.510355	11.598349
10.864003	188.065561	11.603367
10.474310	187.555222	11.608384
10.284448	170.080789	11.613402
10.112563	176.908031	11.618419
10.708676	190.267721	11.623437
11.174440	191.034745	11.628455
10.645601	182.489806	11.633472
10.550015	170.907990	11.638490
10.445502	186.793956	11.643507
10.325291	181.725986	11.648525
10.488962	186.673890	11.653543
10.544136	186.179488	11.658560
11.191681	179.584580	11.663578
10.673499	188.188705	11.668595
10.364885	175.308388	11.673613
10.371059	177.942509	11.678631
10.356554	195.865612	11.683648
10.867644	189.099455	11.688666
11.159865	192.080336	11.693683
10.528260	190.774581	11.698701
10.797455	180.189937	11.703719
10.695204	184.715371	11.708736
10.624219	179.699693	11.713754
10.657656	186.567550	11.718771
10.647268	193.050937	11.723789
10.889940	193.631805	11.728807
10.769508	197.339614	11.733824
10.983362	182.692849	11.738842
11.005385	197.217990	11.743859
10.474314	188.010718	11.748877
10.776043	188.213184	11.753895
10.788671	193.749461	11.758912
11.161062	187.244725	11.763930
10.588465	194.206943	11.768947
10.919955	193.862011	11.773965
10.943904	192.570945	11.778983
10.687944	194.255021	11.784000
11.084335	181.630982	11.789018
10.750436	190.900650	11.794035
10.911821	193.797767	11.799053
11.186278	194.058125	11.804071
10.956180	193.377779	11.809088
10.799578	187.586528	11.814106
10.986692	182.615866	11.819123
10.670574	195.000506	11.824141
11.461358	186.758155	11.829159
10.777187	191.866469	11.834176
11.064392	186.501549	11.839194
10.761493	201.080438	11.844211
10.599871	201.695853	11.849229
11.263630	194.296890	11.854247
10.847774	196.539160	11.859264
11.184054	194.095002	11.864282
11.356115	200.000909	11.869299
11.064442	199.390107	11.874317
11.529551	186.512383	11.879335
11.183446	195.193855	11.884352
10.825473	185.517847	11.889370
10.580372	190.911226	11.894387
11.122913	195.604497	11.899405
11.195966	188.199684	11.904423
11.153676	195.451696	11.909440
11.233778	194.461138	11.914458
11.355756	194.549588	11.919475
11.382092	197.884274	11.924493
11.300544	197.114531	11.929511
11.239175	198.294969	11.934528
11.521984	193.602876	11.939546
10.991238	188.015036	11.944563
11.234508	198.084724	11.949581
11.409782	201.623425	11.954599
11.168393	193.396620	11.959616
11.476204	195.538838	11.964634
11.114164	193.140295	11.969651
11.253164	197.217940	11.974669
11.306220	194.549653	11.979687
11.391243	204.445181	11.984704
11.555602	194.129299	11.989722
11.508989	201.268385	11.994739
10.683423	196.856154	11.999757
11.159274	193.260557	12.004775
11.241652	199.044736	12.009792
11.172172	198.282581	12.014810
10.949079	200.687331	12.019827
11.365659	194.693232	12.024845
10.999023	189.736207	12.029863
11.151845	203.136525	12.034880
11.025155	192.007635	12.039898
11.734942	207.728967	12.044915
11.449821	209.398651	12.049933
11.713409	200.200181	12.054951
11.510406	211.355467	12.059968
11.528894	198.761854	12.064986
11.760987	195.289411	12.070003
11.724980	196.172428	12.075021
11.749318	189.188585	12.080039
11.309166	193.438448	12.085056
11.529819	198.314372	12.090074
11.568999	190.706562	12.095091
11.544682	199.407357	12.100109
11.347389	195.935501	12.105127
11.670629	192.436245	12.110144
11.501633	202.241941	12.115162
11.780738	194.063476	12.120179
11.568644	204.595363	12.125197
11.679173	206.853500	12.130215
11.689579	202.733960	12.135232
12.186837	199.065606	12.140250
11.604083	201.977606	12.145267
11.306236	203.245353	12.150285
11.866594	203.931382	12.155303
11.713261	198.224820	12.160320
11.581623	196.352102	12.165338
11.767858	195.704758	12.170355
12.129785	195.601224	12.175373
11.765260	193.256713	12.180391
11.418085	188.265102	12.185408
12.410490	201.152869	12.190426
12.057660	194.432863	12.195443
11.700991	196.034795	12.200461
11.410914	194.369771	12.205479
11.863857	188.944334	12.210496
12.061279	196.266314	12.215514
12.008346	190.831283	12.220531
11.574901	186.152887	12.225549
11.935268	197.075291	12.230567
12.256983	202.181618	12.235584
11.914638	204.194706	12.240602
12.293952	190.046005	12.245619
11.351215	193.471615	12.250637
12.119732	198.145480	12.255655
12.126000	192.470871	12.260672
12.007600	190.189019	12.265690
11.911102	184.489391	12.270707
11.624603	202.375959	12.275725
12.097971	203.965415	12.280743
12.026021	207.504742	12.285760
12.459612	204.032480	12.290778
11.870476	194.493439	12.295795
11.981110	201.456573	12.300813
12.275373	197.791424	12.305831
11.800014	192.324339	12.310848
11.926104	206.839596	12.315866
12.612451	203.419494	12.320883
12.224045	206.099276	12.325901
11.980934	198.320834	12.330919
12.242696	193.417436	12.335936
12.089808	195.580895	12.340954
12.488199	196.484634	12.345971
12.089772	203.394493	12.350989
12.008554	200.680843	12.356007
12.120354	204.245205	12.361024
12.213627	208.109080	12.366042
12.487687	204.680590	12.371059
12.341025	207.638295	12.376077
12.135929	192.207892	12.381095
12.602436	197.907018	12.386112
12.151474	197.065413	12.391130
12.199853	192.425598	12.396147
11.974379	198.948787	12.401165
12.290662	205.517009	12.406183
12.460624	202.587536	12.411200
12.026778	205.548931	12.416218
12.323786	199.813274	12.421235
12.505368	199.497993	12.426253
12.796480	204.486017	12.431271
12.455721	204.608648	12.436288
11.777414	200.331268	12.441306
12.375379	194.611867	12.446323
12.301331	205.762849	12.451341
12.263038	199.893217	12.456359
12.527394	193.436856	12.461376
12.501742	200.746236	12.466394
12.518990	204.950131	12.471411
12.290696	201.940663	12.476429
12.772470	197.192346	12.481447
12.609636	200.228302	12.486464
12.130263	198.943023	12.491482
12.490401	195.794605	12.496499
12.487332	194.905353	12.501517
12.475328	200.988232	12.506535
12.338298	206.052385	12.511552
12.366555	196.571840	12.516570
12.301960	199.715569	12.521587
12.494700	212.128284	12.526605
13.377716	212.817723	12.531623
12.973391	205.023355	12.536640
12.547185	205.096177	12.541658
12.517850	197.549522	12.546675
12.619004	202.746991	12.551693
12.796222	203.256004	12.556711
12.526985	203.496878	12.561728
12.465706	207.914959	12.566746
12.949725	211.071096	12.571763
13.446078	206.014412	12.576781
12.838802	197.491144	12.581799
12.666591	195.135624	12.586816
12.251616	202.663403	12.591834
12.954500	200.572394	12.596851
13.228018	222.587685	12.601869
12.396952	211.852457	12.606887
12.751855	208.278844	12.611904
13.046997	219.952986	12.616922
12.963986	207.147966	12.621939
12.934642	212.441492	12.626957
12.990265	214.897516	12.631975
12.877131	203.791752	12.636992
12.637337	205.618470	12.642010
13.063704	207.836900	12.647027
13.083746	208.162114	12.652045
13.073340	206.349410	12.657063
12.843623	197.849403	12.662080
12.832093	202.985527	12.667098
13.047035	201.336540	12.672115
12.840035	216.209760	12.677133
13.385998	210.438494	12.682151
12.912374	214.318056	12.687168
13.035624	207.161024	12.692186
13.384271	210.972516	12.697203
13.348216	224.345457	12.702221
12.762368	209.293039	12.707239
12.958293	203.797167	12.712256
12.857124	213.207325	12.717274
12.919056	209.240697	12.722291
13.191215	213.247124	12.727309
13.079874	215.864835	12.732327
13.587204	207.657141	12.737344
13.310930	211.928827	12.742362
13.425235	209.629675	12.747379
13.393330	205.513566	12.752397
13.412285	207.157995	12.757415
13.298678	205.332958	12.762432
12.845830	212.532143	12.767450
13.226413	204.394674	12.772467
13.377406	213.336408	12.777485
12.932418	215.712596	12.782503
13.552122	207.335936	12.787520
13.155240	217.988114	12.792538
13.435995	211.854221	12.797555
13.823091	215.694439	12.802573
13.320359	217.530542	12.807591
13.426923	210.199392	12.812608
13.064266	219.284216	12.817626
13.593750	208.864142	12.822643
13.263381	207.006587	12.827661
13.395168	207.778278	12.832679
13.423127	204.236637	12.837696
13.455427	213.379876	12.842714
13.929310	206.256610	12.847731
13.814246	204.564335	12.852749
13.077834	212.000162	12.857767
13.602436	209.633972	12.862784
13.701622	206.803875	12.867802
13.561999	207.863962	12.872819
13.778602	220.844133	12.877837
13.694430	206.089126	12.882855
13.841577	204.561141	12.887872
13.514336	209.266769	12.892890
13.326134	199.576944	12.897907
13.238380	201.600882	12.902925
13.412020	202.214587	12.907943
13.572326	198.298912	12.912960
13.724993	215.432350	12.917978
13.685141	211.184942	12.922995
13.628416	210.338754	12.928013
13.448550	205.986923	12.933031
13.671571	210.830925	12.938048
13.169044	200.719852	12.943066
13.228575	208.606072	12.948083
13.400214	209.163288	12.953101
13.690058	216.262617	12.958119
14.474661	206.945155	12.963136
14.591530	211.057806	12.968154
13.866404	206.598377	12.973171
14.138344	207.199933	12.978189
13.881771	210.957342	12.983207
14.203025	208.231517	12.988224
13.898030	209.257395	12.993242
13.593633	211.438134	12.998259
13.774414	219.778822	13.003277
13.542230	210.657537	13.008295
13.632330	196.298257	13.013312
13.632789	201.814342	13.018330
13.700958	212.510868	13.023347
13.949548	218.998121	13.028365
14.303932	220.741795	13.033383
14.477291	217.218536	13.038400
13.512130	214.828693	13.043418
13.966792	219.008665	13.048435
14.285102	213.197108	13.053453
14.077854	210.828107	13.058471
13.894646	210.806294	13.063488
14.205517	214.958163	13.068506
14.028428	219.365877	13.073523
14.198607	218.354981	13.078541
14.190529	218.937023	13.083559
14.313693	203.408167	13.088576
14.145675	218.306876	13.093594
14.263560	218.462232	13.098611
14.313857	212.553557	13.103629
13.805215	216.804623	13.108647
14.471278	211.229238	13.113664
14.412090	215.309345	13.118682
14.071853	213.955068	13.123699
14.237634	212.124397	13.128717
14.238268	224.983573	13.133735
14.550181	222.565295	13.138752
13.981236	214.938556	13.143770
14.541188	222.863626	13.148787
14.872531	214.920000	13.153805
14.081012	213.326736	13.158823
14.183998	215.930011	13.163840
14.079410	211.878863	13.168858
14.259862	215.322091	13.173875
14.553186	223.370721	13.178893
14.544708	214.495453	13.183911
14.461096	216.783819	13.188928
14.635060	234.059118	13.193946
14.710235	213.009087	13.198963
14.567544	211.229601	13.203981
14.149735	207.962479	13.208999
14.605640	216.070993	13.214016
14.550763	208.323195	13.219034
14.516517	213.377657	13.224051
14.605453	218.012179	13.229069
14.420386	232.392878	13.234087
14.718915	207.167912	13.239104
14.688424	227.573847	13.244122
14.466131	223.881829	13.249139
14.981723	210.911026	13.254157
15.018509	218.349539	13.259175
14.420574	216.562043	13.264192
14.424289	214.712427	13.269210
14.491845	225.996000	13.274227
15.037832	214.415244	13.279245
14.885330	227.983032	13.284263
14.882132	216.453070	13.289280
14.561989	218.926577	13.294298
14.288420	221.203497	13.299315
14.965634	210.422771	13.304333
14.746890	223.565396	13.309351
14.714587	220.244560	13.314368
14.758322	226.391349	13.319386
15.299152	225.767685	13.324403
15.263360	213.185668	13.329421
14.643705	218.725730	13.334439
14.582904	218.126315	13.339456
14.830654	217.961668	13.344474
14.916770	225.887936	13.349491
14.964224	223.526610	13.354509
15.200667	222.259259	13.359527
14.860564	225.761450	13.364544
14.825475	223.526579	13.369562
14.629543	229.294144	13.374579
14.842068	230.132155	13.379597
14.685782	224.558580	13.384615
14.904509	226.455912	13.389632
14.946902	224.603429	13.394650
14.848582	228.525539	13.399667
15.181384	217.236734	13.404685
14.831283	226.846593	13.409703
15.150805	224.382951	13.414720
14.880587	225.084698	13.419738
14.652697	236.859220	13.424755
15.320162	224.426461	13.429773
15.472977	243.828790	13.434791
15.448559	247.815133	13.439808
15.130733	221.294485	13.444826
14.847129	231.673430	13.449843
15.653795	232.513603	13.454861
15.055489	228.047046	13.459879
15.211505	225.021917	13.464896
15.307602	228.156410	13.469914
15.342988	238.820188	13.474931
15.648288	227.835442	13.479949
15.070959	227.998061	13.484967
15.149691	231.245705	13.489984
15.776844	233.625368	13.495002
15.308539	233.477541	13.500019
15.230118	226.878889	13.505037
15.670228	228.546104	13.510055
15.127662	237.602147	13.515072
15.495796	229.157355	13.520090
15.075533	235.922312	13.525107
15.810141	228.098918	13.530125
15.623335	234.843305	13.535143
15.609276	230.718100	13.540160
15.670247	226.325610	13.545178
15.268990	234.182605	13.550195
15.553248	234.296279	13.555213
15.284650	229.835188	13.560231
15.363830	232.401149	13.565248
15.879748	231.816075	13.570266
15.534452	239.077415	13.575283
15.689534	235.143612	13.580301
15.662690	242.273325	13.585319
15.798844	237.092845	13.590336
16.026990	237.035385	13.595354
15.414184	234.215160	13.600371
16.080508	237.743681	13.605389
16.181755	235.279310	13.610407
15.771269	230.821376	13.615424
15.198761	225.400963	13.620442
15.057663	236.032261	13.625459
15.662702	227.509561	13.630477
15.704078	233.031908	13.635495
15.823502	233.530987	13.640512
16.288230	239.385028	13.645530
15.877830	237.319037	13.650547
15.922619	227.895859	13.655565
15.982999	232.591631	13.660583
15.785262	231.496015	13.665600
15.707162	232.587547	13.670618
15.776671	234.836297	13.675635
15.890198	240.079186	13.680653
16.014774	226.642263	13.685671
16.040043	231.472883	13.690688
16.121456	229.358719	13.695706
16.019903	230.346611	13.700723
16.128606	230.919938	13.705741
15.808611	228.606357	13.710759
15.790944	231.698606	13.715776
16.169009	231.598871	13.720794
15.850069	237.003760	13.725811
15.843915	221.772717	13.730829
15.868790	231.235839	13.735847
15.616902	236.516687	13.740864
16.098948	235.725460	13.745882
16.316622	248.279477	13.750899
16.645590	244.236552	13.755917
16.466700	239.635266	13.760935
15.591492	236.600291	13.765952
16.109093	246.753520	13.770970
16.657203	243.329688	13.775987
16.530189	236.902690	13.781005
16.246663	235.583760	13.786023
15.954813	232.536849	13.791040
16.685065	232.148763	13.796058
16.472370	227.205626	13.801075
16.079035	233.104907	13.806093
16.101365	232.060229	13.811111
16.098449	249.669177	13.816128
16.711023	240.397416	13.821146
16.699579	246.429734	13.826163
16.392182	243.277950	13.831181
16.857193	238.311339	13.836199
16.428314	247.346530	13.841216
16.487245	239.767180	13.846234
16.269666	233.695091	13.851251
16.193544	242.369262	13.856269
16.817599	237.062326	13.861287
16.718789	235.339118	13.866304
16.906988	236.543813	13.871322
16.816974	238.811090	13.876339
16.155379	227.364697	13.881357
16.525140	231.052993	13.886375
17.012750	235.593890	13.891392
16.724921	225.998452	13.896410
16.488690	231.800692	13.901427
16.504275	228.219950	13.906445
16.899369	229.323008	13.911463
16.665113	235.449971	13.916480
16.783009	225.330642	13.921498
16.454890	231.570042	13.926515
16.463555	240.546572	13.931533
16.810155	240.129863	13.936551
17.030089	241.970208	13.941568
16.929172	232.923142	13.946586
16.884620	239.140482	13.951603
16.945825	230.434227	13.956621
17.066160	241.507633	13.961639
16.886554	251.371810	13.966656
16.940540	245.992694	13.971674
16.688562	240.765353	13.976691
16.840754	244.749442	13.981709
17.033784	235.864879	13.986727
16.707103	249.055884	13.991744
16.747156	240.772614	13.996762
16.690157	248.380368	14.001779
16.646863	239.690378	14.006797
16.969767	242.647557	14.011815
16.942846	244.374867	14.016832
17.142918	240.850600	14.021850
16.774956	244.934610	14.026867
17.154172	239.971889	14.031885
16.824372	234.829246	14.036903
17.212830	254.333744	14.041920
17.047940	240.320224	14.046938
17.073579	242.061440	14.051955
17.215582	251.465313	14.056973
17.464532	248.693938	14.061991
17.698440	255.066733	14.067008
17.053776	243.728140	14.072026
17.127711	240.971393	14.077043
16.877903	248.072711	14.082061
17.652848	246.557423	14.087079
17.113650	256.345054	14.092096
17.585443	247.862024	14.097114
17.374710	249.037320	14.102131
17.463027	255.552696	14.107149
17.906592	242.201788	14.112167
17.270297	245.106353	14.117184
17.201105	235.432690	14.122202
17.483202	234.530592	14.127219
17.410863	247.177097	14.132237
17.866020	244.402017	14.137255
17.740412	248.836435	14.142272
17.403848	239.696675	14.147290
17.681275	246.428743	14.152307
17.094915	240.922124	14.157325
17.559802	235.778818	14.162343
17.673777	256.581991	14.167360
17.945724	243.289358	14.172378
17.511202	231.766585	14.177395
17.230217	238.181674	14.182413
17.554356	240.166730	14.187431
17.303246	239.827305	14.192448
17.529254	240.631662	14.197466
17.799140	240.220586	14.202483
17.765613	247.253517	14.207501
17.816675	242.379756	14.212519
17.601945	248.983337	14.217536
18.120711	242.073961	14.222554
18.113654	250.869919	14.227571
17.835368	251.888485	14.232589
18.434323	249.138350	14.237607
17.646584	251.709911	14.242624
17.718058	251.313949	14.247642
17.808306	246.061722	14.252659
17.995523	259.488284	14.257677
17.845613	243.935642	14.262695
18.108331	248.246486	14.267712
17.860690	242.677662	14.272730
18.356526	239.959361	14.277747
17.865694	251.307801	14.282765
18.201773	248.645930	14.287783
18.282762	249.520200	14.292800
17.858140	246.828454	14.297818
17.634284	244.973244	14.302835
17.922779	254.998057	14.307853
18.171515	252.655879	14.312871
18.000492	253.045554	14.317888
17.720721	248.699800	14.322906
18.141669	244.468995	14.327923
17.989188	259.485233	14.332941
17.944078	254.213057	14.337959
17.990732	262.214908	14.342976
18.119360	250.932625	14.347994
17.767952	263.146094	14.353011
18.267795	271.004809	14.358029
18.720938	270.552577	14.363047
18.105412	260.976585	14.368064
18.015161	260.725717	14.373082
18.650106	264.846074	14.378099
18.274628	263.869643	14.383117
18.790559	263.275099	14.388135
18.126835	259.705448	14.393152
18.511350	265.092333	14.398170
18.474275	264.262018	14.403187
18.578871	271.557460	14.408205
18.307738	266.386738	14.413223
18.439792	262.784700	14.418240
18.707057	273.175724	14.423258
18.627895	262.070946	14.428275
18.421956	270.323556	14.433293
18.661715	264.568391	14.438311
18.295109	270.848508	14.443328
18.341798	281.987052	14.448346
18.659657	269.397267	14.453363
18.866038	269.712404	14.458381
19.069071	269.886059	14.463399
19.201385	272.601535	14.468416
18.511647	262.936116	14.473434
18.567731	255.710632	14.478451
18.510232	265.599984	14.483469
18.860373	274.775814	14.488487
19.136232	265.629045	14.493504
18.480332	271.837447	14.498522
18.632464	264.619094	14.503539
18.530952	264.026016	14.508557
18.652225	275.146632	14.513575
18.729802	270.237179	14.518592
18.761239	275.981980	14.523610
18.834093	261.713689	14.528627
18.718517	270.229924	14.533645
19.137921	260.117277	14.538663
18.940948	261.120028	14.543680
18.704954	270.289291	14.548698
19.057573	270.663706	14.553715
18.572047	263.061825	14.558733
18.679773	261.319079	14.563751
19.179301	267.675767	14.568768
19.726768	273.674719	14.573786
19.562307	267.988801	14.578803
19.104645	270.900269	14.583821
19.088363	262.673095	14.588839
19.130314	261.063659	14.593856
18.954138	263.637827	14.598874
19.384101	265.956684	14.603891
18.965161	263.008445	14.608909
19.337800	265.440363	14.613927
19.168882	265.249077	14.618944
19.237621	271.177406	14.623962
19.306158	262.340613	14.628979
19.218860	273.490546	14.633997
19.125011	270.605293	14.639015
19.638242	270.071126	14.644032
19.406773	279.593120	14.649050
19.529085	262.353996	14.654067
19.355795	274.113731	14.659085
19.331798	263.366415	14.664103
19.470414	271.215104	14.669120
19.628061	267.287207	14.674138
19.199318	265.779457	14.679155
19.403256	272.049633	14.684173
19.800891	272.571664	14.689191
19.962078	261.347418	14.694208
19.443213	278.323557	14.699226
19.538503	258.075024	14.704243
19.407943	266.644081	14.709261
19.791483	269.711737	14.714279
19.853590	264.116769	14.719296
19.297282	261.530725	14.724314
19.292185	259.354292	14.729331
19.684350	266.327264	14.734349
19.983583	269.625785	14.739367
20.044409	277.063735	14.744384
19.797148	276.285079	14.749402
19.880402	271.560923	14.754419
19.918764	281.618384	14.759437
19.957172	270.855036	14.764455
19.717172	264.530822	14.769472
19.750986	278.126441	14.774490
19.663680	270.487800	14.779507
19.791362	273.708897	14.784525
19.554625	263.420712	14.789543
19.948887	261.286236	14.794560
19.973067	280.689700	14.799578
20.256137	272.081417	14.804595
19.745885	273.110855	14.809613
19.881830	268.353252	14.814631
20.034772	272.766396	14.819648
19.920992	277.902683	14.824666
20.182987	272.765711	14.829683
20.167124	265.197996	14.834701
20.294606	271.811416	14.839719
20.281283	267.922760	14.844736
20.118542	283.369780	14.849754
20.162507	266.407924	14.854771
20.065187	275.378884	14.859789
20.226527	267.909802	14.864807
20.479634	269.868054	14.869824
20.456665	267.536622	14.874842
20.716315	270.083957	14.879859
20.564206	272.171568	14.884877
20.357891	279.461776	14.889895
20.254756	267.369861	14.894912
20.563950	275.961966	14.899930
20.474719	268.326781	14.904947
20.922047	275.240678	14.909965
19.863534	284.698950	14.914983
20.283515	267.665925	14.920000
20.185780	281.954177	14.925018
20.517877	271.451197	14.930035
20.516593	279.599368	14.935053
20.041493	275.498601	14.940071
20.584277	273.132727	14.945088
20.244919	281.324069	14.950106
20.289857	281.433982	14.955123
20.620966	284.661274	14.960141
20.816215	290.790807	14.965159
21.174892	278.415554	14.970176
20.232033	276.019074	14.975194
21.112404	275.440367	14.980211
20.833116	279.734628	14.985229
20.371879	273.122983	14.990247
20.668916	273.335647	14.995264
21.059566	279.923874	15.000282
20.884408	283.876894	15.005299
21.125024	271.712521	15.010317
20.526868	273.964250	15.015335
21.068569	269.279162	15.020352
20.969978	277.373059	15.025370
20.628352	280.695627	15.030387
21.348971	285.077189	15.035405
21.225501	272.196375	15.040423
20.813348	264.213862	15.045440
20.780158	275.913917	15.050458
20.869141	269.563724	15.055475
21.132308	283.240395	15.060493
21.151693	278.898546	15.065511
21.022106	289.363991	15.070528
21.380136	280.207577	15.075546
20.898290	283.397351	15.080563
21.443592	282.410092	15.085581
20.959951	293.893132	15.090599
21.291360	279.212205	15.095616
21.361538	288.034024	15.100634
21.497833	283.860152	15.105651
20.766732	275.488661	15.110669
20.863526	291.766232	15.115687
21.727418	285.901262	15.120704
21.234769	292.532352	15.125722
21.217015	288.104770	15.130739
21.346013	297.457047	15.135757
21.175661	303.978003	15.140775
21.615396	289.538964	15.145792
21.377498	292.895874	15.150810
21.349597	296.368404	15.155827
21.446165	290.446187	15.160845
21.123214	294.882942	15.165863
21.310830	288.498451	15.170880
21.016037	293.460967	15.175898
21.021944	289.790205	15.180915
21.858757	295.561088	15.185933
21.563059	295.279094	15.190951
21.928253	291.454568	15.195968
21.827031	294.764954	15.200986
21.504661	291.413532	15.206003
21.448818	291.791587	15.211021
21.946069	302.929416	15.216039
21.634800	298.317170	15.221056
21.889653	294.648670	15.226074
21.806098	303.226204	15.231091
22.106987	295.738538	15.236109
21.743632	296.574703	15.241127
21.573024	291.852200	15.246144
21.909761	302.418607	15.251162
22.069314	293.611806	15.256179
22.422752	304.327085	15.261197
21.835984	293.197184	15.266215
22.129440	285.404584	15.271232
21.263302	294.097648	15.276250
22.072159	302.144937	15.281267
21.938562	298.192955	15.286285
22.305311	310.919455	15.291303
22.040959	294.740837	15.296320
22.359144	299.462756	15.301338
22.286690	300.581814	15.306355
21.861024	287.568169	15.311373
21.738890	305.776370	15.316391
22.228131	300.029685	15.321408
22.234010	294.919960	15.326426
22.307329	303.015503	15.331443
22.140832	298.191378	15.336461
21.888254	310.392647	15.341479
22.148255	297.710870	15.346496
22.352512	299.717755	15.351514
21.882582	301.722317	15.356531
22.397013	293.674415	15.361549
22.336632	305.905713	15.366567
22.368781	304.244154	15.371584
22.256827	302.734413	15.376602
22.158524	302.557377	15.381619
22.414920	299.008550	15.386637
22.520747	306.837116	15.391655
22.623552	308.743039	15.396672
22.706768	302.175994	15.401690
22.144377	307.678766	15.406707
23.016537	315.419576	15.411725
22.884006	321.085786	15.416743
22.807712	307.875726	15.421760
22.602470	305.963966	15.426778
22.408717	302.870213	15.431795
22.622510	301.189839	15.436813
22.745907	305.718039	15.441831
23.109406	312.127479	15.446848
22.765151	306.810349	15.451866
22.391038	315.483617	15.456883
22.816141	305.313256	15.461901
22.731346	317.223333	15.466919
23.074718	314.096439	15.471936
23.261328	305.241241	15.476954
22.848748	304.942733	15.481971
22.628040	285.027376	15.486989
22.842616	309.349249	15.492007
22.930366	311.661437	15.497024
23.324490	315.371202	15.502042
23.411640	320.596132	15.507059
23.004051	303.688767	15.512077
22.412703	304.708745	15.517095
22.979045	307.593321	15.522112
23.252827	311.157729	15.527130
23.390271	316.441095	15.532147
23.471337	313.531756	15.537165
23.277658	315.417574	15.542183
22.993438	317.390068	15.547200
23.197575	307.030060	15.552218
23.069791	317.520487	15.557235
23.301714	308.216443	15.562253
22.926615	306.892832	15.567271
23.049203	308.123525	15.572288
23.266184	304.984755	15.577306
23.695698	318.903783	15.582323
23.502857	307.573692	15.587341
23.373390	309.036124	15.592359
23.287993	312.747969	15.597376
23.518975	317.294133	15.602394
23.350362	313.281330	15.607411
23.517490	308.130718	15.612429
23.654498	313.859095	15.617447
23.604131	315.678420	15.622464
23.366223	311.357688	15.627482
23.476758	315.755356	15.632499
23.597321	317.832075	15.637517
23.587605	314.422503	15.642535
23.649475	316.997483	15.647552
23.821422	313.108371	15.652570
23.438392	312.044755	15.657587
23.955349	308.142951	15.662605
23.613904	318.145966	15.667623
23.832807	317.146412	15.672640
24.023788	318.142408	15.677658
24.158109	324.543356	15.682675
23.766891	313.998344	15.687693
23.865513	319.783189	15.692711
23.657784	317.288023	15.697728
24.075146	310.851975	15.702746
24.218933	315.203443	15.707763
24.429016	318.383317	15.712781
24.073390	318.495640	15.717799
23.826605	309.916189	15.722816
24.204786	311.539410	15.727834
23.896656	308.334082	15.732851
23.832247	313.235488	15.737869
24.122451	307.466144	15.742887
24.302055	322.667403	15.747904
24.098702	306.930532	15.752922
24.429649	310.921517	15.757939
24.315871	313.485977	15.762957
24.114614	315.780051	15.767975
24.189361	321.022690	15.772992
24.716674	323.550447	15.778010
24.291350	323.945006	15.783027
24.082143	316.069719	15.788045
24.028992	316.191749	15.793063
24.636758	327.911958	15.798080
24.630496	327.423961	15.803098
24.543719	329.835904	15.808115
25.036007	320.999373	15.813133
24.081631	320.444413	15.818151
24.324125	325.900764	15.823168
24.313947	317.003619	15.828186
24.544472	321.824395	15.833203
24.491557	322.542802	15.838221
24.733509	326.519246	15.843239
24.201298	321.868814	15.848256
24.417670	316.745244	15.853274
24.283146	331.951242	15.858291
24.671723	326.460049	15.863309
24.766658	334.492283	15.868327
24.687323	329.499953	15.873344
24.482405	325.439154	15.878362
24.975285	326.315567	15.883379
24.799242	330.322381	15.888397
25.699093	333.991277	15.893415
25.554821	325.954405	15.898432
25.008804	320.917980	15.903450
24.655953	331.291987	15.908467
24.861593	325.621005	15.913485
25.055396	319.693107	15.918503
24.554477	332.804011	15.923520
25.131646	317.466285	15.928538
24.761634	334.381434	15.933555
25.337017	335.437495	15.938573
25.094033	331.221684	15.943591
25.120432	343.837107	15.948608
25.625228	332.423624	15.953626
25.316024	328.158168	15.958643
25.502266	319.400845	15.963661
25.453460	320.020788	15.968679
25.107825	327.499955	15.973696
25.209153	315.268881	15.978714
24.850330	324.977976	15.983731
25.352820	324.158318	15.988749
25.462062	320.673422	15.993767
25.634007	336.024200	15.998784
25.646244	331.446778	16.003802
25.113866	335.247155	16.008819
25.312950	329.012335	16.013837
25.447615	338.575179	16.018855
25.576311	340.843128	16.023872
25.986984	335.398982	16.028890
25.592228	334.700088	16.033907
25.608518	337.831248	16.038925
26.312770	333.953923	16.043943
25.195427	330.233990	16.048960
25.641892	333.979789	16.053978
25.670841	339.358945	16.058995
25.591279	333.536717	16.064013
25.809430	330.413538	16.069031
25.626138	335.667957	16.074048
25.756731	332.646768	16.079066
25.666486	336.649691	16.084083
25.589000	333.512585	16.089101
25.603082	330.162417	16.094119
25.536828	333.836574	16.099136
25.754997	341.789668	16.104154
25.829206	330.799815	16.109171
25.661013	342.183280	16.114189
25.943590	335.645140	16.119207
26.788005	342.708665	16.124224
26.329282	337.664955	16.129242
26.069462	336.986075	16.134259
25.879319	325.169584	16.139277
25.932609	325.246641	16.144295
26.261020	334.530022	16.149312
26.923688	336.039527	16.154330
26.274198	339.419506	16.159347
25.808482	332.123763	16.164365
26.347029	338.262975	16.169383
26.216618	336.052397	16.174400
26.703403	336.734110	16.179418
26.537107	329.363349	16.184435
25.847862	334.687076	16.189453
26.583130	333.954244	16.194471
26.885001	338.195902	16.199488
26.640045	341.765348	16.204506
26.349070	342.066410	16.209523
26.458728	343.946024	16.214541
27.083214	335.915680	16.219559
26.632226	337.838406	16.224576
26.760694	321.544957	16.229594
26.458673	336.458318	16.234611
26.089446	338.977352	16.239629
26.596411	334.344991	16.244647
26.602636	343.287241	16.249664
26.521547	351.416314	16.254682
26.785937	343.858576	16.259699
26.931343	345.404439	16.264717
27.253759	338.045940	16.269735
26.797723	343.011485	16.274752
27.070327	345.736685	16.279770
26.970161	344.152525	16.284787
27.004207	345.321272	16.289805
27.208096	336.106782	16.294823
26.977691	347.970127	16.299840
26.857906	347.158996	16.304858
27.054537	342.843180	16.309875
27.095489	347.936463	16.314893
27.287409	340.008177	16.319911
27.273712	344.560887	16.324928
26.956719	337.702709	16.329946
27.049789	339.423969	16.334963
26.826907	345.429284	16.339981
27.448512	336.967065	16.344999
26.895482	347.656256	16.350016
27.331986	341.842033	16.355034
27.051975	346.070154	16.360051
27.014721	340.679970	16.365069
27.368130	348.905484	16.370087
27.585687	347.615820	16.375104
27.307743	346.639976	16.380122
27.470330	342.673424	16.385139
27.579072	350.233327	16.390157
27.923188	341.359899	16.395175
27.776257	338.852108	16.400192
27.203370	341.383917	16.405210
27.300369	347.642370	16.410227
27.578992	354.358515	16.415245
27.729215	348.194408	16.420263
28.093288	359.242562	16.425280
27.557465	362.866766	16.430298
27.512518	347.433381	16.435315
27.913983	352.079236	16.440333
28.090149	361.556740	16.445351
27.484970	357.084907	16.450368
27.403963	357.997028	16.455386
28.171811	358.575024	16.460403
27.778908	363.136290	16.465421
27.749723	348.019171	16.470439
28.137170	353.777992	16.475456
27.674936	354.039450	16.480474
28.300319	357.044223	16.485491
27.988959	357.509397	16.490509
28.257448	351.159627	16.495527
28.130722	358.030398	16.500544
27.703421	346.339176	16.505562
27.992128	351.267659	16.510579
27.913904	357.083207	16.515597
27.926770	355.737054	16.520615
28.165381	365.122791	16.525632
27.915317	362.022016	16.530650
28.561352	361.549216	16.535667
28.414419	367.164037	16.540685
28.553529	365.703558	16.545703
28.506664	355.388913	16.550720
28.035751	359.971791	16.555738
28.559444	363.989580	16.560755
28.864456	368.577876	16.565773
28.720536	350.215687	16.570791
28.246963	350.074990	16.575808
28.792087	356.749642	16.580826
28.636094	360.611337	16.585843
28.184868	358.728403	16.590861
28.387231	355.771771	16.595879
28.754504	371.107946	16.600896
29.006316	371.829401	16.605914
29.206353	360.065740	16.610931
28.984512	365.054784	16.615949
28.865757	352.564476	16.620967
28.616352	356.478582	16.625984
28.872309	351.475065	16.631002
28.939744	358.735305	16.636019
29.034385	362.658958	16.641037
29.236499	349.519123	16.646055
28.842222	347.422207	16.651072
28.948101	353.231179	16.656090
29.343218	344.507590	16.661107
28.791732	355.089253	16.666125
28.911855	360.189147	16.671143
29.367750	359.196870	16.676160
28.830177	359.687798	16.681178
29.069665	346.166625	16.686195
29.009395	347.914915	16.691213
28.869895	345.929802	16.696231
29.495713	362.604728	16.701248
29.367477	356.039029	16.706266
29.212796	354.068901	16.711283
29.176895	360.076665	16.716301
29.498701	360.569482	16.721319
29.328279	361.233607	16.726336
29.211444	355.802163	16.731354
29.414901	369.251526	16.736371
29.537194	358.045896	16.741389
29.152313	352.542584	16.746407
29.151750	359.674564	16.751424
29.426998	373.147464	16.756442
29.766654	364.867979	16.761459
29.978256	362.455833	16.766477
29.741028	362.956799	16.771495
29.760206	366.081203	16.776512
29.848841	374.537293	16.781530
29.898471	362.276368	16.786547
29.609777	368.904132	16.791565
29.935805	365.442275	16.796583
30.066978	359.984838	16.801600
29.341416	359.918086	16.806618
29.642710	366.816888	16.811635
30.181784	356.748667	16.816653
29.981518	375.855840	16.821671
30.512552	362.424954	16.826688
30.151010	370.929044	16.831706
30.247146	362.460269	16.836723
29.994464	359.675466	16.841741
30.135363	358.271510	16.846759
30.178876	371.067315	16.851776
29.671232	366.188995	16.856794
29.830783	359.108297	16.861811
29.887381	367.102336	16.866829
30.230860	364.426673	16.871847
30.109906	359.753222	16.876864
30.392027	367.816285	16.881882
30.285625	367.586863	16.886899
30.337179	364.300278	16.891917
30.111272	363.527760	16.896935
30.467667	364.296043	16.901952
30.773652	377.417041	16.906970
31.151611	372.243051	16.911987
30.959636	370.064144	16.917005
30.780344	368.804710	16.922023
30.291072	361.585202	16.927040
30.401038	378.668646	16.932058
30.355684	368.322202	16.937075
30.495820	371.222657	16.942093
31.023314	376.628339	16.947111
31.301124	369.380909	16.952128
30.840105	371.472450	16.957146
30.646998	368.993933	16.962163
30.385892	367.456918	16.967181
30.970467	371.746082	16.972199
31.330222	371.781734	16.977216
31.179536	376.349470	16.982234
31.151779	369.701853	16.987251
30.723006	373.975232	16.992269
30.864850	379.873282	16.997287
31.342733	371.240930	17.002304
31.240326	379.262887	17.007322
31.264095	380.471105	17.012339
31.161766	382.781340	17.017357
31.046642	377.343311	17.022375
31.304250	375.028137	17.027392
30.971273	384.310385	17.032410
31.196947	381.754041	17.037427
31.599915	379.561393	17.042445
31.137761	383.492851	17.047463
31.545168	373.492455	17.052480
31.045990	376.464050	17.057498
31.623883	381.300182	17.062515
31.299693	380.700747	17.067533
31.315788	384.649257	17.072551
31.407357	378.904505	17.077568
31.204279	388.033993	17.082586
31.149698	386.950790	17.087603
31.636770	377.894148	17.092621
32.036058	382.209007	17.097639
32.130126	388.777184	17.102656
31.361619	376.283887	17.107674
31.916323	382.833987	17.112691
31.736662	385.089995	17.117709
31.775503	393.124679	17.122727
32.385765	386.863687	17.127744
31.849146	389.920005	17.132762
31.567240	387.026144	17.137779
32.098821	383.835222	17.142797
32.268890	398.034537	17.147815
31.890837	383.779550	17.152832
32.204768	392.550846	17.157850
31.907568	392.890746	17.162867
32.051816	389.706483	17.167885
32.135999	392.325335	17.172903
32.580676	387.282957	17.177920
32.673444	390.468488	17.182938
32.129827	378.669128	17.187955
31.989125	384.424989	17.192973
32.162428	387.241392	17.197991
31.988287	388.499357	17.203008
32.167445	395.420343	17.208026
32.578323	394.507654	17.213043
32.757594	390.730988	17.218061
32.238370	386.135318	17.223079
32.645479	390.837105	17.228096
32.453602	395.726824	17.233114
32.528424	390.994482	17.238131
32.716910	391.227205	17.243149
32.569835	392.417844	17.248167
32.217300	385.678784	17.253184
32.590080	387.236584	17.258202
32.448007	389.322647	17.263219
32.732646	389.578267	17.268237
33.204006	392.291463	17.273255
33.203455	390.212131	17.278272
32.888358	393.861932	17.283290
32.884180	386.213453	17.288307
32.811269	387.597662	17.293325
33.046928	400.335171	17.298343
33.400719	401.835972	17.303360
32.902160	399.499678	17.308378
33.374804	396.441000	17.313395
33.083195	386.237023	17.318413
33.271085	399.628876	17.323431
33.275941	394.216340	17.328448
32.925427	393.901855	17.333466
33.380280	397.362354	17.338483
33.727571	393.057780	17.343501
33.257171	398.514702	17.348519
33.198815	392.159004	17.353536
33.460379	410.143479	17.358554
33.353421	398.844136	17.363571
34.009234	385.901863	17.368589
33.294635	388.884911	17.373607
33.037790	385.655806	17.378624
33.783797	402.179520	17.383642
33.410074	389.943467	17.388659
33.972995	388.618961	17.393677
33.364288	396.722911	17.398695
33.450215	394.999325	17.403712
33.738092	399.681811	17.408730
33.914786	393.368408	17.413747
33.791379	398.294801	17.418765
33.436490	403.740050	17.423783
33.803174	388.643307	17.428800
33.847774	394.351386	17.433818
33.582579	394.787283	17.438835
33.881375	391.948168	17.443853
33.783239	395.914466	17.448871
33.964134	392.737119	17.453888
33.868146	399.457961	17.458906
34.203672	409.283045	17.463923
34.317459	391.802138	17.468941
33.999555	399.993350	17.473959
34.395053	403.349488	17.478976
34.642422	404.210484	17.483994
33.846138	397.673046	17.489011
34.389242	393.672483	17.494029
34.384951	399.927791	17.499047
34.425719	403.042529	17.504064
34.571813	407.068629	17.509082
34.622979	403.277194	17.514099
34.364070	393.061810	17.519117
34.115828	396.133186	17.524135
34.301871	403.176173	17.529152
34.925393	411.870877	17.534170
34.687566	414.625070	17.539187
34.693801	405.599099	17.544205
34.699942	415.137817	17.549223
34.262588	411.554978	17.554240
34.667913	413.423279	17.559258
34.396797	413.090120	17.564275
34.448142	401.674614	17.569293
34.694563	404.217717	17.574311
34.673618	406.168163	17.579328
35.295742	408.258316	17.584346
35.213906	406.974238	17.589363
34.948131	407.924596	17.594381
35.002969	405.338046	17.599399
35.211448	410.039209	17.604416
35.310637	413.848562	17.609434
34.598651	410.311639	17.614451
35.529238	418.844933	17.619469
35.886343	418.855753	17.624487
35.323497	406.816384	17.629504
35.170323	400.967726	17.634522
34.960320	412.613355	17.639539
35.533322	404.385878	17.644557
35.554451	418.141363	17.649575
35.604438	415.426185	17.654592
35.421641	404.927558	17.659610
35.274726	408.144098	17.664627
35.488849	412.244810	17.669645
35.457643	413.133402	17.674663
36.026333	413.534135	17.679680
36.144911	409.552331	17.684698
35.427015	408.853256	17.689715
35.737160	401.701758	17.694733
35.705651	419.652983	17.699751
35.553267	415.003345	17.704768
35.945806	413.812657	17.709786
35.450818	426.332601	17.714803
36.096734	416.317135	17.719821
35.867017	414.816253	17.724839
35.656745	422.081890	17.729856
36.103045	409.323692	17.734874
35.873523	420.041449	17.739891
36.175267	417.725708	17.744909
35.902447	421.864369	17.749927
36.060209	417.302134	17.754944
36.174873	409.609897	17.759962
36.023319	418.043447	17.764979
36.149381	414.694762	17.769997
36.328390	424.698851	17.775015
36.503908	418.817946	17.780032
36.714252	417.229613	17.785050
36.251358	415.137060	17.790067
36.470476	413.736700	17.795085
36.223717	416.826783	17.800103
36.391036	420.720200	17.805120
36.981532	429.016131	17.810138
36.479900	420.842360	17.815155
36.573749	424.005639	17.820173
36.727224	429.942918	17.825191
37.007500	434.449881	17.830208
36.968440	419.845453	17.835226
36.438685	418.978235	17.840243
36.731592	422.583868	17.845261
36.986118	422.172024	17.850279
37.178293	429.567500	17.855296
36.764098	420.259860	17.860314
36.956017	423.464671	17.865331
37.252422	427.555730	17.870349
37.280284	431.691758	17.875367
37.006384	429.225812	17.880384
36.822501	410.639420	17.885402
37.175923	422.721169	17.890419
37.447159	426.929750	17.895437
37.587603	435.421982	17.900455
37.357744	435.271739	17.905472
37.041051	420.300302	17.910490
37.145443	435.074734	17.915507
37.215058	425.587627	17.920525
37.544243	430.796995	17.925543
37.146053	431.790060	17.930560
37.371691	427.823140	17.935578
37.132633	439.870922	17.940595
37.568356	426.688345	17.945613
37.028232	423.048925	17.950631
37.303096	436.244237	17.955648
37.781131	429.047655	17.960666
38.105857	434.841514	17.965683
37.876085	436.865501	17.970701
37.859824	417.694452	17.975719
37.676775	434.195598	17.980736
38.053481	431.341190	17.985754
38.080921	438.459376	17.990771
37.732939	429.431742	17.995789
37.943071	434.252568	18.000807
38.025422	445.455087	18.005824
38.167570	439.213315	18.010842
38.243575	439.599245	18.015859
38.511712	443.385455	18.020877
38.528537	434.121147	18.025895
37.617160	436.125032	18.030912
37.764134	430.917565	18.035930
38.418558	439.803121	18.040947
38.287593	438.684473	18.045965
38.533440	440.249419	18.050983
38.533369	442.764637	18.056000
38.618814	442.009906	18.061018
38.503900	432.510502	18.066035
38.711744	431.862941	18.071053
38.482692	427.531335	18.076071
38.227218	439.285041	18.081088
38.505348	439.112507	18.086106
38.127952	428.647320	18.091123
38.789862	432.394309	18.096141
38.798681	428.884003	18.101159
38.627571	435.181075	18.106176
38.723680	439.170786	18.111194
38.643472	436.125598	18.116211
38.770202	444.692549	18.121229
39.338173	444.840944	18.126247
39.490217	451.292825	18.131264
39.024372	445.473901	18.136282
38.989123	445.899242	18.141299
39.126566	450.352712	18.146317
39.110263	438.531168	18.151335
39.149789	446.695152	18.156352
39.085439	440.356148	18.161370
39.336041	446.088972	18.166387
39.287689	444.938527	18.171405
39.480504	449.989261	18.176423
39.417904	448.699029	18.181440
39.688651	446.198772	18.186458
39.296862	446.562866	18.191475
39.395918	452.139415	18.196493
39.707305	451.062341	18.201511
39.867800	455.360752	18.206528
39.245479	445.990833	18.211546
39.352946	437.094244	18.216563
39.756427	451.433978	18.221581
40.032094	441.873757	18.226599
39.969554	443.240577	18.231616
39.921572	451.607526	18.236634
39.826466	449.079028	18.241651
39.943767	458.341698	18.246669
39.926299	449.918970	18.251687
39.583393	455.308723	18.256704
40.198236	451.047681	18.261722
39.933114	453.455853	18.266739
39.783855	444.687590	18.271757
40.188632	447.887666	18.276775
40.044639	454.016428	18.281792
39.973551	452.604448	18.286810
40.039239	449.050572	18.291827
40.117355	457.183307	18.296845
40.746245	456.886736	18.301863
40.478501	457.272541	18.306880
40.173780	458.311012	18.311898
40.777203	459.369027	18.316915
40.429359	461.597584	18.321933
40.773033	463.696385	18.326951
40.813825	465.697183	18.331968
40.461841	459.961507	18.336986
40.517846	456.753104	18.342003
40.576297	464.895216	18.347021
40.877260	458.811737	18.352039
40.729868	461.693862	18.357056
40.657084	453.415438	18.362074
41.155856	454.985184	18.367091
41.078488	457.155850	18.372109
41.202362	457.976119	18.377127
40.816491	464.448644	18.382144
40.711753	457.248116	18.387162
40.880140	462.006026	18.392179
41.263906	460.857725	18.397197
41.163184	462.508189	18.402215
40.903280	458.537967	18.407232
41.024780	468.166045	18.412250
41.186237	466.481182	18.417267
40.891130	464.958919	18.422285
40.953384	465.706736	18.427303
41.609765	469.205296	18.432320
41.594882	469.930411	18.437338
41.736767	469.349920	18.442355
41.781519	475.824826	18.447373
42.048272	468.282445	18.452391
41.434520	461.637672	18.457408
41.427033	464.879849	18.462426
41.650775	470.058311	18.467443
41.564054	467.212939	18.472461
41.976544	463.971120	18.477479
41.860905	460.619035	18.482496
41.942788	465.279966	18.487514
41.876101	471.948938	18.492531
41.888485	477.337027	18.497549
41.771388	470.062683	18.502567
41.982543	471.778193	18.507584
41.957113	470.302300	18.512602
42.117750	469.188739	18.517619
42.040993	468.642290	18.522637
42.012365	465.655336	18.527655
42.050177	475.539433	18.532672
41.492332	474.834369	18.537690
42.788380	477.204592	18.542707
42.851284	483.279062	18.547725
42.488968	464.862398	18.552743
42.513488	469.488082	18.557760
42.040352	470.114139	18.562778
42.390476	470.861315	18.567795
42.864510	484.514780	18.572813
43.037272	478.602727	18.577831
42.986219	477.294917	18.582848
42.320446	474.028483	18.587866
42.573003	476.927231	18.592883
42.899813	473.654572	18.597901
42.929284	473.719559	18.602919
42.581873	474.218749	18.607936
42.523873	477.831694	18.612954
43.407790	466.939739	18.617971
42.964294	475.816384	18.622989
42.961923	472.888453	18.628007
43.303917	471.304863	18.633024
43.371171	473.809603	18.638042
43.440499	470.242533	18.643059
43.266415	475.640720	18.648077
43.305477	468.493535	18.653095
43.217269	471.398003	18.658112
43.129117	479.108532	18.663130
43.471812	466.505273	18.668147
43.508281	481.855182	18.673165
43.367585	471.555078	18.678183
43.410763	476.903660	18.683200
43.291703	471.844894	18.688218
43.955779	476.210064	18.693235
43.656515	481.283776	18.698253
44.120377	476.819027	18.703271
43.768082	472.976791	18.708288
43.280334	472.689983	18.713306
43.963058	477.370971	18.718323
44.043444	493.790133	18.723341
44.031688	495.101716	18.728359
44.375626	475.527399	18.733376
44.216856	481.712118	18.738394
44.502688	478.761404	18.743411
43.776850	484.482174	18.748429
44.148612	477.434656	18.753447
44.345103	485.615243	18.758464
43.887623	486.551274	18.763482
44.089331	483.228666	18.768499
44.075104	485.632490	18.773517
44.196128	478.264266	18.778535
44.143565	482.756795	18.783552
44.486441	483.258958	18.788570
44.479170	477.523252	18.793587
44.195189	481.521660	18.798605
44.406008	482.842766	18.803623
44.796808	480.036647	18.808640
44.395428	487.382557	18.813658
45.185280	482.340056	18.818675
44.618234	494.246446	18.823693
44.747791	487.552202	18.828711
44.797125	488.497682	18.833728
45.145672	505.231693	18.838746
45.262249	484.746066	18.843763
45.233284	492.475787	18.848781
45.239360	486.545504	18.853799
44.745957	486.234330	18.858816
44.875293	494.299150	18.863834
45.380371	491.399501	18.868851
45.290768	496.879211	18.873869
45.440001	490.156656	18.878887
45.357423	488.853754	18.883904
45.515206	494.736739	18.888922
45.247875	492.787290	18.893939
45.037434	501.226892	18.898957
45.334237	486.380776	18.903975
45.423244	491.542355	18.908992
45.010940	487.393892	18.914010
45.750463	486.843421	18.919027
45.738896	496.536412	18.924045
45.639595	494.699650	18.929063
46.333935	493.048577	18.934080
45.545126	493.051628	18.939098
46.067990	488.991082	18.944115
46.014656	499.296464	18.949133
46.050369	499.915876	18.954151
46.252740	497.195895	18.959168
46.067648	510.286158	18.964186
46.336058	497.091711	18.969203
46.116630	499.779940	18.974221
46.490559	497.594955	18.979239
46.164436	489.059325	18.984256
45.912827	494.346518	18.989274
46.330529	494.376304	18.994291
46.488238	504.683543	18.999309
46.567128	505.289922	19.004327
46.805154	494.306017	19.009344
46.619141	502.186421	19.014362
46.790958	496.886707	19.019379
46.719538	498.270692	19.024397
46.713674	498.268601	19.029415
46.911851	492.396766	19.034432
46.286018	499.408414	19.039450
46.872855	495.208524	19.044467
47.040632	497.347338	19.049485
46.935187	496.041684	19.054503
46.915762	496.234200	19.059520
46.723726	503.121508	19.064538
46.209234	500.954931	19.069555
46.816819	496.931683	19.074573
47.253554	506.343451	19.079591
47.245015	510.409429	19.084608
47.648454	514.821500	19.089626
47.319112	511.436409	19.094643
47.605256	504.664131	19.099661
47.199257	499.864617	19.104679
47.574850	494.571045	19.109696
47.323052	506.642947	19.114714
47.339273	515.258695	19.119731
47.933712	511.461543	19.124749
47.427286	511.108217	19.129767
47.700404	498.758754	19.134784
47.388314	506.605143	19.139802
47.467545	512.086971	19.144819
47.608892	509.811970	19.149837
47.391648	508.343850	19.154855
47.719301	505.323506	19.159872
47.657627	519.271836	19.164890
47.755248	518.748726	19.169907
48.178700	520.538480	19.174925
48.672009	529.651130	19.179943
48.471681	521.704943	19.184960
48.132786	511.776486	19.189978
48.074593	506.367421	19.194995
48.208964	515.908318	19.200013
48.567243	526.439951	19.205031
49.012540	515.531054	19.210048
48.315385	513.222510	19.215066
48.214173	510.928472	19.220083
48.277526	512.263074	19.225101
48.486601	516.654917	19.230119
48.613069	516.357680	19.235136
48.746898	515.869956	19.240154
49.026531	512.506809	19.245171
49.070935	522.673916	19.250189
48.478192	519.913632	19.255207
48.937691	516.932717	19.260224
48.930117	520.137050	19.265242
48.951342	513.614289	19.270259
49.396390	513.463101	19.275277
49.079163	513.200233	19.280295
49.091905	505.691073	19.285312
49.013166	520.216392	19.290330
49.129809	518.409119	19.295347
49.299737	514.542367	19.300365
49.041538	518.681930	19.305383
49.171739	517.330119	19.310400
49.307910	524.128466	19.315418
49.539395	526.017534	19.320435
49.945726	531.921791	19.325453
49.585721	528.519381	19.330471
50.220059	521.661327	19.335488
49.492299	518.148927	19.340506
49.587788	523.814412	19.345523
50.274642	521.990940	19.350541
49.813181	517.184278	19.355559
50.030006	521.253038	19.360576
49.694882	525.363556	19.365594
50.177550	526.487712	19.370611
50.038912	521.037521	19.375629
50.292691	525.573878	19.380647
50.566641	532.726301	19.385664
50.232350	525.766605	19.390682
50.008742	516.501820	19.395699
50.292415	515.962365	19.400717
50.429069	517.733658	19.405735
50.358321	522.901185	19.410752
50.717664	520.626954	19.415770
50.241438	524.828866	19.420787
50.577508	514.602822	19.425805
50.413030	532.833630	19.430823
50.671640	522.152603	19.435840
50.869696	524.438178	19.440858
50.672716	527.100826	19.445875
50.726374	522.179248	19.450893
50.565418	527.597496	19.455911
50.277948	520.176096	19.460928
50.526347	519.657911	19.465946
50.885233	532.616161	19.470963
51.413727	535.490891	19.475981
51.265961	537.394829	19.480999
50.936399	532.728565	19.486016
51.459122	532.183447	19.491034
51.084308	536.593625	19.496051
51.505162	526.067208	19.501069
51.213468	538.416730	19.506087
51.322247	536.314047	19.511104
51.548648	537.478103	19.516122
51.288567	533.621496	19.521139
51.484098	536.469175	19.526157
51.578078	536.820752	19.531175
51.382540	533.178148	19.536192
51.695574	539.532416	19.541210
51.264697	534.247637	19.546227
51.554861	535.048331	19.551245
51.878854	538.292558	19.556263
52.074061	546.492307	19.561280
52.329104	541.880181	19.566298
52.356780	540.197207	19.571315
51.955127	523.478045	19.576333
52.060036	530.183436	19.581351
52.090033	540.100343	19.586368
52.415169	537.212925	19.591386
52.519833	548.683424	19.596403
52.351031	543.502999	19.601421
52.337607	544.300470	19.606439
52.161546	551.286290	19.611456
52.800844	546.279835	19.616474
52.636109	544.077731	19.621491
52.496890	541.496130	19.626509
52.740556	545.106300	19.631527
52.862349	540.697950	19.636544
52.893974	536.887439	19.641562
52.486893	547.692876	19.646579
52.940017	539.099010	19.651597
52.695420	543.596207	19.656615
52.850812	537.390206	19.661632
52.851806	542.691729	19.666650
52.457870	538.108068	19.671667
52.961886	548.055314	19.676685
53.045463	550.835223	19.681703
53.559712	554.639941	19.686720
53.492163	551.482314	19.691738
53.854561	554.651140	19.696755
53.918748	556.884982	19.701773
53.540762	547.966095	19.706791
53.489255	550.341020	19.711808
54.015137	550.117288	19.716826
53.250129	544.985510	19.721843
53.624182	549.421100	19.726861
53.682663	556.228401	19.731879
54.099080	555.015052	19.736896
53.969326	552.308905	19.741914
53.858134	553.298316	19.746931
53.995162	549.840605	19.751949
53.872648	548.468180	19.756967
53.681429	543.237599	19.761984
54.139950	546.511372	19.767002
54.148905	554.699100	19.772019
54.075683	554.123697	19.777037
54.147146	554.844838	19.782055
53.918629	557.739609	19.787072
54.196737	547.610929	19.792090
54.548708	568.001892	19.797107
54.820898	563.939334	19.802125
54.611648	552.236114	19.807143
54.335419	552.455991	19.812160
54.552876	548.433515	19.817178
54.626851	561.227872	19.822195
54.698212	561.295804	19.827213
54.934456	562.445707	19.832231
55.163583	560.942796	19.837248
55.118676	549.261325	19.842266
54.923257	560.762776	19.847283
55.078381	551.249664	19.852301
55.122739	559.160494	19.857319
54.870510	559.038978	19.862336
55.257667	564.201492	19.867354
55.324212	562.575577	19.872371
55.062146	559.899495	19.877389
54.760957	556.607838	19.882407
54.914992	562.308400	19.887424
55.975028	565.403321	19.892442
55.369334	570.550013	19.897459
55.906929	569.137924	19.902477
55.808503	580.286628	19.907495
55.756662	566.230000	19.912512
55.964664	565.945313	19.917530
55.850926	575.231394	19.922547
56.038895	566.924940	19.927565
55.950493	570.634152	19.932583
55.827780	572.010351	19.937600
56.322399	558.237861	19.942618
56.138246	575.417782	19.947635
56.346133	565.104373	19.952653
56.151240	566.573857	19.957671
56.161265	570.700072	19.962688
56.602099	564.474864	19.967706
56.200761	570.833075	19.972723
56.386641	572.262208	19.977741
56.384037	576.210517	19.982759
56.265456	568.466167	19.987776
56.541707	565.049890	19.992794
56.305474	564.351550	19.997811
56.202094	567.454048	20.002829
56.981462	570.652626	20.007847
57.118664	579.246414	20.012864
57.317039	580.477951	20.017882
57.259504	580.373456	20.022899
56.856212	577.384858	20.027917
57.080076	569.530388	20.032935
57.103468	573.635588	20.037952
57.416321	579.731134	20.042970
57.344678	580.698610	20.047987
57.241789	584.956013	20.053005
57.364734	573.974198	20.058023
57.552572	581.749095	20.063040
57.601515	567.881892	20.068058
57.288712	573.061876	20.073075
57.500384	582.751713	20.078093
57.476378	563.035779	20.083111
57.228767	583.807279	20.088128
57.601405	576.769053	20.093146
57.225252	582.122997	20.098163
57.898572	578.780590	20.103181
58.136193	590.006362	20.108199
58.850839	591.220632	20.113216
58.494249	587.366416	20.118234
57.872896	587.696830	20.123251
57.620092	575.252479	20.128269
58.177939	577.803922	20.133287
57.940351	593.490078	20.138304
58.641609	581.297950	20.143322
58.703852	588.918842	20.148339
58.806617	584.958395	20.153357
58.807023	581.818583	20.158375
58.478296	593.410235	20.163392
58.616607	585.253510	20.168410
58.690984	581.859194	20.173427
58.659214	585.793112	20.178445
58.585258	583.905060	20.183463
58.764175	583.448183	20.188480
59.405443	576.683699	20.193498
58.915125	587.227577	20.198515
58.860482	587.962042	20.203533
59.466525	580.262649	20.208551
58.948410	588.052793	20.213568
59.165693	581.609930	20.218586
59.101887	587.846171	20.223603
59.069389	587.892406	20.228621
59.347459	575.930266	20.233639
59.069248	590.786489	20.238656
59.936277	602.280332	20.243674
60.059900	599.777715	20.248691
59.487383	600.955715	20.253709
59.642353	589.404037	20.258727
59.561080	596.592859	20.263744
60.037988	594.325560	20.268762
60.245092	605.035406	20.273779
60.055901	604.711578	20.278797
60.197130	596.279849	20.283815
60.356122	606.394452	20.288832
60.201547	604.591530	20.293850
59.999310	599.794975	20.298867
59.803951	598.556960	20.303885
60.494199	600.062196	20.308903
60.019830	601.786626	20.313920
60.148945	603.047882	20.318938
60.138417	597.625056	20.323955
60.660941	600.948833	20.328973
60.902755	596.313508	20.333991
60.867912	597.843278	20.339008
60.644527	600.077720	20.344026
61.075542	604.536012	20.349043
60.922188	599.006040	20.354061
61.203621	597.422401	20.359079
60.691396	603.040525	20.364096
60.912266	610.586238	20.369114
61.386159	609.225088	20.374131
61.402063	613.987846	20.379149
61.226654	601.487247	20.384167
61.305065	607.764465	20.389184
61.668366	617.705258	20.394202
61.924455	596.064889	20.399219
61.522024	610.785841	20.404237
61.633772	606.388506	20.409255
61.387277	608.673882	20.414272
61.511569	607.187289	20.419290
61.359252	606.207649	20.424307
61.340854	604.557087	20.429325
61.769235	600.820484	20.434343
61.343354	605.588910	20.439360
61.688649	612.427312	20.444378
62.097778	618.129199	20.449395
62.081408	618.191858	20.454413
62.789355	620.009909	20.459431
62.080624	615.532041	20.464448
62.005358	622.246586	20.469466
62.606052	616.715967	20.474483
62.580541	618.174861	20.479501
62.648012	616.624533	20.484519
62.524837	617.634748	20.489536
62.558853	609.042987	20.494554
62.778468	611.195834	20.499571
62.947357	615.199499	20.504589
62.842399	594.735612	20.509607
63.025444	598.427813	20.514624
62.771326	603.986817	20.519642
62.879037	599.328190	20.524659
62.860909	608.463709	20.529677
63.103963	597.936530	20.534695
63.200904	601.995574	20.539712
62.926732	603.846618	20.544730
62.912269	607.361297	20.549747
63.404266	608.061144	20.554765
63.714679	604.948798	20.559783
63.802345	612.597299	20.564800
63.492841	607.953138	20.569818
63.644413	609.188808	20.574835
63.909351	614.739581	20.579853
63.808797	605.985745	20.584871
63.722808	609.565206	20.589888
64.101717	609.885045	20.594906
64.110103	605.106187	20.599923
63.985732	613.207408	20.604941
64.050319	612.509564	20.609959
63.786898	606.109980	20.614976
64.049591	612.945465	20.619994
64.054884	603.878515	20.625011
64.063883	609.415489	20.630029
64.227781	611.649592	20.635047
64.061779	612.174187	20.640064
63.896833	614.648831	20.645082
65.081973	610.863826	20.650099
65.048035	621.696415	20.655117
65.375243	616.845825	20.660135
64.854881	619.694530	20.665152
64.498650	612.747681	20.670170
64.849374	617.931663	20.675187
64.851805	619.076949	20.680205
65.507641	615.491114	20.685223
65.348310	615.923156	20.690240
65.084593	619.514513	20.695258
65.508594	605.961256	20.700275
65.263363	616.823584	20.705293
65.564361	610.746359	20.710311
65.046056	607.128748	20.715328
65.133884	611.460601	20.720346
65.201157	617.149444	20.725363
65.434805	622.231739	20.730381
65.744437	620.047283	20.735399
66.301987	632.217313	20.740416
65.774958	613.554747	20.745434
66.073468	624.638523	20.750451
65.787609	626.986833	20.755469
66.142390	627.480836	20.760487
66.256879	629.148299	20.765504
66.259970	629.188993	20.770522
66.395452	633.112660	20.775539
66.623036	629.167481	20.780557
66.516203	630.616948	20.785575
66.475662	627.082731	20.790592
66.333878	633.242769	20.795610
66.619372	624.192140	20.800627
66.282468	626.463194	20.805645
66.555067	611.784835	20.810663
66.630716	629.148412	20.815680
66.645226	630.288663	20.820698
66.676978	626.654832	20.825715
66.481656	633.451187	20.830733
67.067333	631.690793	20.835751
67.606837	630.158485	20.840768
66.803911	628.298722	20.845786
67.351735	638.980786	20.850803
67.152358	642.129800	20.855821
67.233585	634.231240	20.860839
67.535664	632.196276	20.865856
67.306870	637.751348	20.870874
67.677930	632.196519	20.875891
67.784021	638.264319	20.880909
67.716828	632.462155	20.885927
67.874843	633.857763	20.890944
67.526539	639.046449	20.895962
67.654735	627.621986	20.900979
67.653718	626.259039	20.905997
67.959802	635.025369	20.911015
68.366993	632.017866	20.916032
68.620210	632.811695	20.921050
68.168731	621.417530	20.926067
68.038063	630.138254	20.931085
68.917754	632.844716	20.936103
68.711061	638.651957	20.941120
68.388005	637.799881	20.946138
68.812948	639.261224	20.951155
68.470917	634.249748	20.956173
68.875762	637.648657	20.961191
68.908952	634.986552	20.966208
68.879114	629.068124	20.971226
68.856313	637.289236	20.976243
69.302695	640.545984	20.981261
69.132095	641.923332	20.986279
69.324122	644.762107	20.991296
69.018787	644.800331	20.996314
68.962965	645.323551	21.001331
69.094709	633.002316	21.006349
69.286807	635.913660	21.011367
69.393751	631.513911	21.016384
69.555141	637.917071	21.021402
69.864040	638.493955	21.026419
70.250969	646.951069	21.031437
69.309416	652.156388	21.036455
69.710341	645.445078	21.041472
69.647082	640.535359	21.046490
70.165062	641.455217	21.051507
70.501530	647.597601	21.056525
70.063564	647.429265	21.061543
70.330395	642.158894	21.066560
69.905076	652.818918	21.071578
70.334576	642.392067	21.076595
70.531267	650.654748	21.081613
70.209512	643.986531	21.086631
70.430125	634.327484	21.091648
70.985930	646.381035	21.096666
70.631707	649.289081	21.101683
71.209905	650.969552	21.106701
71.353953	657.861396	21.111719
71.069908	648.871028	21.116736
70.512050	648.879144	21.121754
70.744288	651.452893	21.126771
71.138277	661.824420	21.131789
71.147242	661.444492	21.136807
71.283096	655.440300	21.141824
71.530450	657.279576	21.146842
71.520183	650.051637	21.151859
71.766138	652.550670	21.156877
71.622064	650.673528	21.161895
71.705403	656.296768	21.166912
71.257158	659.153186	21.171930
71.375557	659.204328	21.176947
71.779962	655.799638	21.181965
71.386652	659.291263	21.186983
72.144383	662.493228	21.192000
72.169480	669.820149	21.197018
72.429879	664.380365	21.202035
72.161728	656.302670	21.207053
72.060634	656.312250	21.212071
72.564829	658.310346	21.217088
72.872367	656.703704	21.222106
72.511784	656.722128	21.227123
72.298530	654.483384	21.232141
72.952422	664.025524	21.237159
72.832368	652.579737	21.242176
73.128375	669.120123	21.247194
72.733435	667.528181	21.252211
73.227088	669.240751	21.257229
73.093900	665.039322	21.262247
72.947787	664.244898	21.267264
73.090318	667.119784	21.272282
72.769271	661.593812	21.277299
72.856836	666.673619	21.282317
72.857380	667.106016	21.287335
73.591275	663.915102	21.292352
73.540529	676.085200	21.297370
74.085592	672.661763	21.302387
74.284442	674.262449	21.307405
73.611351	662.972186	21.312423
73.739716	652.286112	21.317440
73.884882	670.197464	21.322458
73.715657	662.189567	21.327475
74.361195	660.022233	21.332493
74.234071	668.272225	21.337511
74.238305	668.164424	21.342528
73.963885	666.632610	21.347546
74.042380	668.693832	21.352563
74.307945	668.529564	21.357581
74.227707	665.086723	21.362599
74.470058	660.694286	21.367616
74.554540	666.383621	21.372634
75.024242	668.768928	21.377651
75.079823	669.205379	21.382669
75.123583	668.917860	21.387687
75.373271	664.603172	21.392704
74.665506	667.720895	21.397722
74.863983	674.556936	21.402739
75.515751	674.256802	21.407757
75.399155	674.915713	21.412775
75.600792	672.653394	21.417792
75.562544	679.491581	21.422810
75.384457	679.800317	21.427827
75.588810	670.610824	21.432845
75.765342	674.313522	21.437863
75.800392	669.644100	21.442880
75.725406	678.138434	21.447898
75.532446	671.642651	21.452915
75.545627	664.114420	21.457933
75.552642	677.039204	21.462951
76.035855	676.989368	21.467968
76.276382	685.440893	21.472986
76.348644	681.156981	21.478003
76.751673	677.960776	21.483021
76.667712	677.472245	21.488039
76.788153	675.156298	21.493056
76.412995	668.187128	21.498074
76.534397	670.361585	21.503091
76.724945	665.699511	21.508109
76.457654	667.858749	21.513127
76.530725	675.638933	21.518144
76.981221	670.917451	21.523162
76.774592	676.579533	21.528179
77.075432	674.273368	21.533197
76.855875	672.448999	21.538215
77.325475	670.132337	21.543232
76.875550	668.842436	21.548250
77.565588	680.079876	21.553267
77.790881	679.672578	21.558285
77.523525	679.181043	21.563303
77.640241	672.346721	21.568320
77.698951	679.138255	21.573338
77.557054	681.019204	21.578355
78.417078	670.777762	21.583373
77.798628	681.846556	21.588391
78.004405	674.730132	21.593408
78.165012	678.012447	21.598426
78.212177	674.975788	21.603443
78.268261	670.347270	21.608461
78.471251	679.066560	21.613479
78.514597	678.539273	21.618496
78.068866	674.626335	21.623514
78.298938	676.846987	21.628531
78.253431	677.895604	21.633549
78.984166	685.339877	21.638567
78.973271	678.083623	21.643584
79.259374	684.953360	21.648602
78.946202	686.741060	21.653619
78.810675	679.513677	21.658637
78.856902	686.477566	21.663655
79.311329	682.241445	21.668672
79.393286	683.579475	21.673690
79.365194	688.273366	21.678707
79.748380	685.872330	21.683725
79.246534	692.224144	21.688743
79.564525	692.815393	21.693760
79.690803	683.104736	21.698778
79.866660	683.036484	21.703795
79.678206	682.696760	21.708813
79.816347	682.176804	21.713831
80.385308	692.126644	21.718848
80.083095	686.313718	21.723866
80.147001	690.624070	21.728883
80.687549	687.289692	21.733901
80.780589	697.884816	21.738919
80.546289	687.703295	21.743936
80.302096	680.849424	21.748954
80.231180	688.039828	21.753971
80.631678	681.798769	21.758989
80.748736	685.826299	21.764007
80.668409	686.829846	21.769024
80.958967	687.573683	21.774042
80.819344	690.031772	21.779059
81.123913	689.899300	21.784077
80.881527	698.239833	21.789095
80.843905	692.281572	21.794112
81.611189	701.676694	21.799130
81.798691	710.597220	21.804147
81.830408	696.136170	21.809165
81.796286	701.345383	21.814183
81.559517	699.091360	21.819200
81.826367	693.814660	21.824218
81.739686	692.562872	21.829235
82.141957	694.964993	21.834253
82.253875	695.380050	21.839271
81.983957	701.496948	21.844288
82.147133	691.310343	21.849306
82.265143	696.215011	21.854323
82.416606	694.064639	21.859341
82.297555	697.059150	21.864359
81.995793	697.393453	21.869376
82.166505	688.594184	21.874394
82.282626	693.855739	21.879411
82.067990	694.788683	21.884429
82.719536	702.248448	21.889447
82.824540	706.874287	21.894464
83.475414	695.803887	21.899482
83.212579	701.856569	21.904499
83.344587	700.141556	21.909517
83.734900	705.947385	21.914535
83.094074	691.408020	21.919552
83.351771	695.034971	21.924570
83.320233	702.345477	21.929587
83.759528	694.618350	21.934605
83.710924	698.867329	21.939623
83.615369	694.413888	21.944640
83.322291	691.054671	21.949658
82.946756	699.990273	21.954675
83.275084	698.090066	21.959693
83.529089	707.391543	21.964711
83.923003	696.162341	21.969728
84.766033	705.428912	21.974746
84.423576	700.572113	21.979763
84.351183	706.655103	21.984781
84.740302	703.521018	21.989799
84.694023	705.898307	21.994816
84.743440	701.567455	21.999834
84.526537	691.209659	22.004851
84.527441	693.273497	22.009869
84.559813	698.879442	22.014887
85.340798	716.811765	22.019904
85.854658	703.610503	22.024922
85.180195	710.374195	22.029939
85.062836	705.065795	22.034957
85.718678	703.954011	22.039975
85.642671	703.795589	22.044992
85.751132	706.426486	22.050010
85.793497	711.071546	22.055027
85.741020	706.175908	22.060045
86.000998	704.393635	22.065063
85.752084	707.821764	22.070080
85.645414	703.366896	22.075098
86.046527	696.557710	22.080115
85.921919	695.059371	22.085133
85.970401	693.455190	22.090151
85.841564	695.283617	22.095168
85.944539	699.695182	22.100186
86.418579	713.979968	22.105203
86.622353	703.619782	22.110221
87.197163	704.688581	22.115239
86.967556	718.237197	22.120256
87.048050	708.186527	22.125274
87.080343	708.393083	22.130291
86.844631	704.011952	22.135309
87.085224	700.815789	22.140327
87.225150	702.722287	22.145344
87.095153	708.580726	22.150362
86.798020	710.542650	22.155379
87.307967	706.670252	22.160397
87.405551	708.185726	22.165415
87.227817	706.484225	22.170432
87.725483	701.739612	22.175450
88.485150	718.939979	22.180467
88.239586	715.876307	22.185485
87.881175	705.294391	22.190503
87.784782	705.505203	22.195520
87.958320	705.172233	22.200538
88.326647	709.435193	22.205555
88.127524	709.254915	22.210573
88.455536	711.851631	22.215591
88.396974	714.423330	22.220608
88.677310	710.835982	22.225626
88.914392	708.681745	22.230643
88.560111	710.144499	22.235661
88.599457	708.428134	22.240679
88.526402	701.295154	22.245696
88.645109	703.318561	22.250714
88.708303	713.545969	22.255731
89.224666	710.319491	22.260749
89.869835	722.030989	22.265767
89.458690	714.732898	22.270784
89.757063	713.339110	22.275802
89.850517	711.144121	22.280819
89.351021	703.979707	22.285837
89.773745	706.337621	22.290855
89.790859	712.747494	22.295872
89.478070	704.544185	22.300890
89.691890	711.718668	22.305907
90.042477	710.427200	22.310925
90.232885	703.720242	22.315943
89.813093	720.981175	22.320960
90.542305	718.519948	22.325978
90.821046	725.397160	22.330995
90.605155	722.407760	22.336013
90.967964	711.852400	22.341031
90.787706	726.523081	22.346048
91.412891	717.290132	22.351066
90.734740	717.282262	22.356083
90.707276	711.524377	22.361101
90.923198	724.546055	22.366119
90.959968	717.724162	22.371136
91.521901	713.149414	22.376154
91.435153	723.352838	22.381171
91.564446	717.674682	22.386189
91.497647	722.182112	22.391207
91.381603	716.160314	22.396224
91.262292	720.732722	22.401242
91.801089	727.162359	22.406259
92.365773	733.764688	22.411277
92.765079	725.040259	22.416295
92.376672	725.268136	22.421312
92.052827	718.003787	22.426330
91.821252	713.887088	22.431347
92.040365	725.018004	22.436365
92.344584	720.063671	22.441383
92.550242	726.895459	22.446400
92.822447	723.978383	22.451418
92.868033	723.037349	22.456435
93.130793	727.253635	22.461453
92.959544	722.190298	22.466471
92.893807	724.359186	22.471488
92.987845	725.704805	22.476506
93.628774	718.773069	22.481523
93.206380	731.603810	22.486541
93.457057	725.357660	22.491559
93.596731	743.594981	22.496576
93.748618	736.553192	22.501594
93.940847	735.188551	22.506611
93.976002	729.887955	22.511629
94.162669	730.240883	22.516647
94.276604	734.546613	22.521664
94.006689	727.368535	22.526682
94.012841	716.799276	22.531699
93.994354	732.205299	22.536717
94.135113	727.112317	22.541735
94.570916	728.341611	22.546752
94.676998	721.631997	22.551770
94.554048	727.921676	22.556787
94.479160	727.655785	22.561805
94.669650	713.952614	22.566823
94.644787	726.506870	22.571840
94.347348	727.774589	22.576858
95.181677	731.447465	22.581875
95.150467	739.594199	22.586893
95.275316	734.898154	22.591911
95.411737	727.792507	22.596928
95.438603	733.938946	22.601946
95.486872	729.986950	22.606963
95.744752	733.493964	22.611981
96.076779	738.134957	22.616999
96.115600	735.121676	22.622016
95.523543	735.832526	22.627034
96.008283	732.184946	22.632051
95.800079	735.613054	22.637069
96.315310	733.620629	22.642087
96.488535	747.822895	22.647104
96.326313	740.091574	22.652122
96.888696	731.228145	22.657139
96.862534	744.028762	22.662157
97.169919	734.466598	22.667175
97.270119	738.881761	22.672192
97.262327	730.545750	22.677210
97.247632	728.108829	22.682227
97.413138	732.311858	22.687245
97.129169	733.353425	22.692263
97.376545	730.083619	22.697280
97.332886	719.730389	22.702298
97.364171	731.363909	22.707315
97.093236	729.850481	22.712333
97.609227	726.343200	22.717351
97.264924	728.555460	22.722368
97.984157	733.281328	22.727386
98.764906	736.403987	22.732403
98.402003	740.537814	22.737421
98.814291	736.229349	22.742439
98.416818	730.620581	22.747456
98.207949	731.527383	22.752474
98.676153	729.327692	22.757491
98.647128	741.011632	22.762509
98.929002	735.659998	22.767527
98.868427	737.976403	22.772544
98.538999	744.635896	22.777562
98.828502	726.164803	22.782579
98.606878	735.691823	22.787597
98.820811	733.042586	22.792615
99.521972	752.331707	22.797632
99.297353	744.546984	22.802650
99.662946	741.495448	22.807667
99.737784	755.807710	22.812685
99.931411	742.252347	22.817703
99.942356	745.611623	22.822720
99.657773	739.107989	22.827738
99.974987	732.984017	22.832755
99.834409	746.518795	22.837773
99.820557	737.691433	22.842791
100.065510	739.916089	22.847808
100.841816	748.520907	22.852826
101.106377	739.107415	22.857843
100.540657	743.765110	22.862861
100.868883	734.644656	22.867879
100.785491	732.357282	22.872896
100.755346	729.607196	22.877914
101.428464	737.445459	22.882931
101.132156	739.423037	22.887949
101.781685	741.852938	22.892967
100.904588	732.210113	22.897984
101.227728	743.312222	22.903002
101.188717	737.985302	22.908019
101.389081	743.880677	22.913037
101.562517	738.858340	22.918055
101.695232	738.105705	22.923072
101.632248	738.396521	22.928090
102.354145	747.233865	22.933107
102.212332	758.531446	22.938125
102.262444	750.681856	22.943143
102.865830	745.785075	22.948160
102.487673	748.131993	22.953178
102.609374	731.570978	22.958195
102.503355	748.025716	22.963213
102.793814	744.329490	22.968231
103.187069	745.609590	22.973248
102.767221	744.545366	22.978266
102.816588	741.606179	22.983283
102.936381	742.114682	22.988301
103.144549	740.315227	22.993319
103.444243	739.527127	22.998336
103.457011	739.026689	23.003354
103.448846	738.277053	23.008371
103.576448	756.945445	23.013389
103.893427	759.641714	23.018407
103.868058	747.553135	23.023424
104.003643	756.667956	23.028442
104.458344	750.718226	23.033459
103.986152	753.859245	23.038477
104.150025	748.727944	23.043495
104.573961	743.379435	23.048512
104.082778	753.718427	23.053530
104.993809	751.790605	23.058547
105.016893	753.746858	23.063565
104.820797	757.952545	23.068583
105.105840	751.199278	23.073600
105.200705	755.817242	23.078618
105.006113	755.945517	23.083635
105.436119	756.847522	23.088653
105.300531	758.897906	23.093671
105.521588	761.896279	23.098688
105.519332	757.453541	23.103706
105.846572	762.294095	23.108723
105.812601	758.216045	23.113741
105.773641	766.894158	23.118759
105.795433	760.743590	23.123776
105.949114	758.255204	23.128794
106.322700	761.690563	23.133811
106.581518	766.557550	23.138829
106.411055	764.602454	23.143847
106.605330	769.006134	23.148864
106.695793	759.768056	23.153882
106.710089	766.045847	23.158899
106.930519	766.882656	23.163917
106.868161	763.566396	23.168935
106.874781	758.046178	23.173952
106.565374	775.088013	23.178970
107.343080	772.395174	23.183987
107.620833	767.400767	23.189005
107.707064	774.538339	23.194023
107.901300	770.042915	23.199040
108.135409	774.307854	23.204058
108.200419	769.800993	23.209075
108.318834	760.672167	23.214093
107.735624	758.793958	23.219111
108.567485	759.393563	23.224128
107.836334	766.500607	23.229146
108.215417	763.437500	23.234163
108.094011	760.849936	23.239181
107.770698	760.379733	23.244199
108.586908	760.000349	23.249216
108.555338	765.228118	23.254234
109.132865	771.897889	23.259251
109.019515	767.519780	23.264269
109.395163	768.124145	23.269287
109.433393	766.726676	23.274304
109.587291	765.734063	23.279322
109.532853	768.169433	23.284339
109.751845	759.059662	23.289357
109.642566	772.621144	23.294375
109.733548	762.777086	23.299392
109.628456	770.957427	23.304410
109.907867	762.011812	23.309427
109.983009	760.760070	23.314445
110.041488	767.605323	23.319463
110.925610	763.327528	23.324480
110.620407	765.751449	23.329498
111.294205	770.373952	23.334515
110.813364	766.835676	23.339533
110.270050	756.339318	23.344551
111.220432	761.710839	23.349568
111.317450	773.573988	23.354586
111.489533	759.091029	23.359603
111.622856	766.969170	23.364621
111.330443	766.257477	23.369639
111.694808	769.770010	23.374656
111.544040	759.199910	23.379674
111.301080	758.351134	23.384691
111.381372	758.345097	23.389709
111.480800	767.525512	23.394727
111.932110	767.963467	23.399744
112.188795	776.257893	23.404762
111.994406	773.400832	23.409779
112.786428	773.971928	23.414797
112.541715	772.135685	23.419815
112.836143	769.723212	23.424832
112.604841	772.066202	23.429850
112.605065	778.696474	23.434867
112.531615	765.277345	23.439885
112.940661	771.146550	23.444903
113.605666	781.400219	23.449920
113.704740	772.905541	23.454938
113.507072	773.611791	23.459955
113.576531	769.189441	23.464973
113.516300	781.711376	23.469991
113.854125	772.463179	23.475008
114.281243	772.766049	23.480026
113.616928	772.721312	23.485043
114.204418	768.044744	23.490061
113.773001	764.628158	23.495079
114.243160	762.440782	23.500096
114.030174	767.485365	23.505114
114.659336	779.306690	23.510131
115.134632	771.125812	23.515149
114.851730	779.387489	23.520167
115.233641	782.881515	23.525184
115.385826	778.484151	23.530202
115.224691	776.028999	23.535219
115.329752	772.023971	23.540237
115.276970	778.839215	23.545255
115.137530	770.621508	23.550272
114.905320	776.057239	23.555290
115.424182	769.895547	23.560307
115.964314	773.361781	23.565325
115.174077	776.082120	23.570343
115.961527	770.430861	23.575360
115.903798	784.789034	23.580378
116.244422	783.420219	23.585395
116.735049	775.584080	23.590413
116.583939	778.517327	23.595431
116.648049	771.968858	23.600448
116.739185	774.864389	23.605466
116.867017	777.911992	23.610483
117.226740	769.777510	23.615501
116.856496	768.213269	23.620519
116.832738	767.863680	23.625536
117.246441	776.837384	23.630554
117.753755	774.969260	23.635571
118.091958	768.829385	23.640589
118.015658	776.714921	23.645607
118.061440	767.483794	23.650624
117.993211	768.633781	23.655642
118.205456	768.332652	23.660659
118.348112	767.818301	23.665677
118.624168	769.668901	23.670695
118.448605	772.334563	23.675712
118.619146	775.911987	23.680730
118.523673	778.741901	23.685747
118.708863	773.118138	23.690765
118.568406	769.921330	23.695783
118.501286	764.150667	23.700800
118.709543	772.253821	23.705818
119.429323	782.246506	23.710835
119.496797	775.385095	23.715853
119.559342	787.786937	23.720871
119.661250	784.962635	23.725888
120.131440	782.740539	23.730906
120.043608	781.192286	23.735923
120.235456	779.357499	23.740941
119.858632	774.909960	23.745959
120.145988	768.702263	23.750976
120.332807	770.513109	23.755994
119.851018	780.800163	23.761011
120.804878	766.694083	23.766029
120.611493	792.812638	23.771047
120.877103	780.928033	23.776064
121.393355	784.079260	23.781082
121.117611	785.491924	23.786099
121.632619	779.160420	23.791117
120.972067	781.156844	23.796135
121.335148	769.528463	23.801152
121.509381	769.788657	23.806170
120.887886	782.186546	23.811187
121.593558	776.368141	23.816205
122.030379	778.465103	23.821223
122.540430	784.189203	23.826240
122.725505	788.638501	23.831258
122.732646	791.483997	23.836275
122.415936	774.763986	23.841293
122.272225	772.085221	23.846311
122.107922	775.740025	23.851328
122.862459	778.459687	23.856346
122.398297	784.906651	23.861363
122.689856	777.357118	23.866381
123.032636	781.321126	23.871399
123.642307	795.625890	23.876416
123.752034	798.546932	23.881434
123.959240	794.011613	23.886451
123.854466	783.797244	23.891469
123.510360	788.085942	23.896487
123.828701	782.564518	23.901504
124.205893	787.621359	23.906522
124.278906	790.851064	23.911539
124.457721	782.381834	23.916557
124.393873	785.882148	23.921575
124.813601	790.534747	23.926592
124.251706	783.768166	23.931610
124.549814	791.563860	23.936627
124.526290	783.687850	23.941645
124.691980	783.507575	23.946663
124.260123	786.695967	23.951680
125.072277	799.271434	23.956698
125.284831	792.169684	23.961715
125.701336	789.801315	23.966733
125.484052	797.216520	23.971751
125.851918	785.868241	23.976768
126.093607	787.418089	23.981786
125.627916	780.018010	23.986803
126.311653	784.964009	23.991821
126.704351	791.517402	23.996839
126.494021	793.573116	24.001856
126.691735	783.441036	24.006874
126.986976	805.529424	24.011891
126.752947	785.710235	24.016909
126.925349	780.662802	24.021927
127.002074	790.582046	24.026944
127.272220	788.242776	24.031962
127.250855	780.751429	24.036979
127.391345	782.657849	24.041997
127.731073	782.693467	24.047015
127.544293	786.610542	24.052032
128.225458	782.174998	24.057050
127.740203	786.312107	24.062067
127.687907	782.312641	24.067085
127.764474	781.859072	24.072103
128.320526	781.775806	24.077120
128.822968	791.205904	24.082138
128.410891	795.227483	24.087155
129.008212	796.422169	24.092173
129.013502	782.656259	24.097191
129.124404	789.007380	24.102208
129.145680	787.956521	24.107226
128.922121	788.029348	24.112243
128.816059	789.150513	24.117261
129.544921	794.095801	24.122279
129.481189	798.003187	24.127296
129.637320	788.941055	24.132314
129.506891	790.047080	24.137331
129.411288	789.064910	24.142349
130.042285	799.241836	24.147367
130.284452	802.625083	24.152384
131.118944	793.880199	24.157402
131.011719	795.399166	24.162419
131.229735	800.048460	24.167437
130.992487	792.003756	24.172455
131.391487	798.158550	24.177472
131.501283	783.846209	24.182490
131.328684	792.317930	24.187507
131.156081	783.480547	24.192525
131.554156	787.637914	24.197543
131.754452	799.292503	24.202560
131.802632	780.994617	24.207578
131.184850	783.549256	24.212595
131.195514	789.398445	24.217613
131.892065	779.658903	24.222631
132.154429	792.256851	24.227648
132.812104	796.989166	24.232666
132.658265	799.370591	24.237683
133.106191	796.624955	24.242701
132.920490	794.738498	24.247719
133.047310	801.756157	24.252736
133.068467	796.880585	24.257754
133.230792	798.957172	24.262771
133.522728	791.754703	24.267789
133.550160	790.579812	24.272807
133.353050	804.025611	24.277824
133.599290	796.063415	24.282842
133.342836	794.566660	24.287859
133.153224	791.948686	24.292877
133.999220	788.655093	24.297895
134.013870	810.051893	24.302912
134.590151	798.838410	24.307930
134.459073	798.458193	24.312947
134.504139	799.218168	24.317965
135.010016	794.756265	24.322983
134.880350	794.543082	24.328000
134.794977	791.908878	24.333018
134.667079	802.273387	24.338035
135.309114	799.816256	24.343053
135.994387	795.345357	24.348071
135.665710	807.006572	24.353088
135.991704	811.661148	24.358106
135.948522	802.686843	24.363123
135.810927	798.659630	24.368141
136.210540	793.131861	24.373159
136.210738	791.049208	24.378176
135.964695	791.172871	24.383194
136.564989	799.937662	24.388211
136.856469	805.203508	24.393229
137.329441	797.073470	24.398247
137.334751	802.084076	24.403264
137.398961	795.134806	24.408282
137.729851	794.067299	24.413299
137.175987	801.525442	24.418317
137.582834	797.785838	24.423335
137.601945	797.858751	24.428352
137.774982	796.692748	24.433370
137.237112	783.494228	24.438387
137.969326	792.916955	24.443405
138.655894	795.495729	24.448423
138.759899	804.959468	24.453440
138.936047	798.428257	24.458458
138.949309	804.428522	24.463475
138.742774	807.420895	24.468493
139.180508	795.152884	24.473511
138.997190	798.110084	24.478528
139.701062	793.671002	24.483546
139.463297	800.322558	24.488563
139.134200	799.127439	24.493581
139.224965	792.735752	24.498599
139.227718	796.232011	24.503616
139.466604	797.005989	24.508634
140.274987	806.132850	24.513651
140.163482	805.938929	24.518669
140.846965	800.805606	24.523687
140.495455	800.598560	24.528704
140.770905	792.606572	24.533722
140.949054	801.534916	24.538739
140.786745	785.775437	24.543757
140.931044	798.685253	24.548775
140.967283	793.797866	24.553792
141.139286	808.603119	24.558810
141.549258	808.892882	24.563827
141.761432	812.419653	24.568845
142.012938	801.644886	24.573863
141.910951	794.172396	24.578880
141.844951	795.552405	24.583898
142.117091	797.605583	24.588915
142.144816	799.053049	24.593933
142.362971	793.828078	24.598951
142.186680	786.146260	24.603968
142.395724	794.224058	24.608986
143.030631	786.403319	24.614003
143.657589	802.182276	24.619021
143.498575	786.030974	24.624039
143.102896	785.417407	24.629056
143.411994	795.022773	24.634074
143.866990	793.582504	24.639091
144.006858	793.977434	24.644109
144.229058	785.368907	24.649127
144.172099	786.198413	24.654144
144.144931	785.391775	24.659162
143.982693	790.011910	24.664179
143.719316	789.929994	24.669197
144.312628	778.925304	24.674215
144.627713	782.761085	24.679232
144.823038	789.632379	24.684250
145.443840	792.716840	24.689267
145.300934	794.165625	24.694285
145.301091	793.446249	24.699303
145.044061	796.919839	24.704320
145.241701	802.582137	24.709338
145.977285	800.621668	24.714355
145.636805	803.994647	24.719373
146.414296	811.450634	24.724391
146.318776	809.215628	24.729408
146.167239	806.329799	24.734426
146.369976	800.302518	24.739443
146.223566	800.205547	24.744461
146.676642	798.983321	24.749479
147.309045	803.041095	24.754496
147.562970	808.609427	24.759514
148.098698	799.680687	24.764531
147.490680	799.494643	24.769549
147.497353	791.730688	24.774567
147.446700	794.058179	24.779584
148.067590	804.681640	24.784602
147.997124	797.668131	24.789619
148.201495	807.195139	24.794637
147.931018	799.919287	24.799655
148.665515	800.795979	24.804672
148.080671	795.099598	24.809690
148.602396	798.568705	24.814707
149.122359	807.061993	24.819725
149.851576	806.532056	24.824743
149.680526	808.026249	24.829760
149.556753	806.483589	24.834778
150.035199	802.436199	24.839795
149.946905	802.210262	24.844813
149.672564	795.815460	24.849831
149.788534	796.756894	24.854848
149.908468	800.676710	24.859866
149.957643	794.083220	24.864883
150.553157	797.954238	24.869901
150.576727	796.382327	24.874919
150.738891	791.753038	24.879936
150.914548	802.048198	24.884954
151.415028	794.993134	24.889971
151.576729	804.974895	24.894989
151.413648	783.472127	24.900007
151.358023	792.960714	24.905024
151.499502	799.124047	24.910042
151.590255	790.630653	24.915059
151.509291	789.428459	24.920077
151.655923	790.204178	24.925095
152.177306	796.942661	24.930112
151.904338	799.342634	24.935130
152.611684	800.450765	24.940147
152.413330	803.732190	24.945165
152.431200	809.498216	24.950183
153.088164	796.116815	24.955200
152.985241	799.702109	24.960218
153.362862	795.247551	24.965235
153.040642	796.288766	24.970253
153.533224	803.542962	24.975271
153.779451	801.431470	24.980288
154.166446	807.099002	24.985306
154.324373	797.692611	24.990323
154.350365	804.322038	24.995341
154.339604	798.495251	25.000359
154.658405	796.429263	25.005376
154.731730	806.970725	25.010394
154.290176	798.841063	25.015411
154.272530	798.231752	25.020429
154.567279	802.146442	25.025447
154.968791	808.505972	25.030464
155.267989	800.743805	25.035482
156.030777	795.131090	25.040499
155.619485	803.879816	25.045517
155.683464	803.175748	25.050535
156.623237	810.966222	25.055552
156.637733	807.016310	25.060570
156.940944	804.918035	25.065587
157.008937	801.534136	25.070605
157.051918	801.555997	25.075623
156.587825	794.445988	25.080640
157.029592	797.712955	25.085658
157.044245	798.367214	25.090675
157.453156	791.222269	25.095693
157.820736	800.881650	25.100711
157.847686	791.268442	25.105728
157.655651	806.064102	25.110746
157.638525	799.282122	25.115763
157.862787	794.920867	25.120781
158.493419	806.013016	25.125799
158.890679	797.159482	25.130816
158.827429	800.937410	25.135834
158.938311	797.313311	25.140851
159.141129	798.847122	25.145869
159.064663	802.756493	25.150887
159.219996	794.268821	25.155904
159.453441	801.481314	25.160922
159.242110	803.758085	25.165939
159.541171	801.843489	25.170957
160.027075	807.732301	25.175975
160.457280	791.372494	25.180992
160.018301	802.444983	25.186010
160.315071	808.748240	25.191027
160.817688	805.167288	25.196045
160.923021	797.886573	25.201063
160.934906	789.534843	25.206080
160.693959	804.637911	25.211098
160.818493	804.931090	25.216115
160.965156	806.085491	25.221133
161.262388	808.260993	25.226151
161.782703	803.929381	25.231168
161.875977	814.139547	25.236186
161.945261	811.383433	25.241203
162.288947	814.529978	25.246221
162.619349	821.793654	25.251239
163.338240	812.719628	25.256256
162.557359	809.600430	25.261274
162.916362	791.951550	25.266291
162.519147	799.464197	25.271309
163.195462	813.099060	25.276327
163.418893	806.349050	25.281344
163.137253	806.175306	25.286362
163.176648	808.668656	25.291379
163.572666	806.164622	25.296397
163.178686	809.769988	25.301415
163.860851	800.376647	25.306432
164.191145	804.651866	25.311450
164.292748	802.269409	25.316467
164.632135	798.410923	25.321485
164.267701	807.714074	25.326503
165.187376	807.668867	25.331520
165.448774	808.818028	25.336538
165.792771	813.065871	25.341555
166.366352	803.803039	25.346573
166.065617	792.625119	25.351591
165.996353	786.829533	25.356608
165.463380	788.913389	25.361626
165.489259	791.494045	25.366643
166.154303	787.704776	25.371661
166.088211	804.005039	25.376679
166.541058	793.069544	25.381696
166.436792	800.394575	25.386714
166.995311	798.805647	25.391731
167.756467	803.818494	25.396749
167.771668	813.643195	25.401767
167.981487	804.616873	25.406784
167.721910	803.713879	25.411802
167.936505	805.665568	25.416819
167.960970	799.527190	25.421837
167.945895	799.119445	25.426855
168.220966	796.880390	25.431872
168.245449	802.254076	25.436890
168.221503	801.197634	25.441907
168.845040	804.095485	25.446925
169.110451	804.070093	25.451943
169.055053	811.813542	25.456960
169.117807	800.951399	25.461978
169.101202	799.754962	25.466995
169.621418	801.864190	25.472013
169.885875	813.373108	25.477031
170.286481	811.130284	25.482048
170.545344	809.237725	25.487066
170.483759	801.339228	25.492083
170.344347	803.248206	25.497101
171.023942	804.177627	25.502119
171.082458	809.918392	25.507136
170.739996	806.689911	25.512154
170.831445	804.946490	25.517171
171.749076	804.131606	25.522189
171.891141	816.852444	25.527207
172.177889	806.668616	25.532224
172.531675	806.973439	25.537242
172.380829	807.795473	25.542259
172.365155	807.088028	25.547277
172.228082	810.732289	25.552295
172.432220	802.170744	25.557312
172.539538	804.618805	25.562330
172.515326	799.601975	25.567347
172.963501	802.530284	25.572365
173.318917	804.283328	25.577383
173.576914	816.746281	25.582400
173.757350	807.260642	25.587418
173.522485	808.884687	25.592435
174.295236	804.873524	25.597453
173.906756	806.843370	25.602471
174.056598	798.025200	25.607488
174.303714	795.897791	25.612506
174.314955	798.887815	25.617523
174.819533	796.373193	25.622541
175.107575	801.787894	25.627559
175.341029	802.606899	25.632576
175.255974	809.566035	25.637594
175.502725	797.905250	25.642611
175.507210	810.344555	25.647629
175.506832	809.625261	25.652647
176.184921	806.758583	25.657664
175.894050	801.698065	25.662682
176.259673	806.359095	25.667699
176.998896	805.695060	25.672717
176.583685	801.878320	25.677735
176.971097	800.388614	25.682752
177.165549	802.012088	25.687770
176.954458	807.192086	25.692788
177.462171	806.977495	25.697805
177.462205	805.649083	25.702823
177.840591	805.318931	25.707840
178.070667	810.976183	25.712858
177.772093	806.986652	25.717876
178.551222	805.650547	25.722893
178.393102	800.054979	25.727911
178.839329	807.761353	25.732928
179.265604	802.977334	25.737946
179.084776	802.589084	25.742964
179.748333	802.508016	25.747981
179.636947	809.300842	25.752999
179.411554	804.372136	25.758016
179.828311	805.367724	25.763034
179.542977	809.966006	25.768052
180.166060	807.855799	25.773069
180.474138	816.413640	25.778087
180.761737	812.465386	25.783104
180.928975	816.343129	25.788122
180.968994	812.461823	25.793140
181.446307	802.279885	25.798157
181.311875	807.899216	25.803175
180.989416	809.325466	25.808192
181.609658	809.484665	25.813210
181.692424	821.697201	25.818228
182.365958	808.306896	25.823245
182.223697	807.770634	25.828263
182.381288	806.992033	25.833280
182.484582	804.880704	25.838298
182.236300	810.221123	25.843316
183.335938	819.337363	25.848333
183.891091	826.288347	25.853351
183.673140	810.528036	25.858368
183.891164	813.997095	25.863386
184.102858	819.218567	25.868404
184.452910	806.077437	25.873421
184.309515	796.257222	25.878439
183.952370	807.802956	25.883456
184.423586	808.973098	25.888474
184.301487	813.662729	25.893492
184.323107	804.236529	25.898509
184.524556	798.938419	25.903527
184.955278	817.793219	25.908544
185.235328	811.204800	25.913562
185.012685	808.888602	25.918580
185.630570	811.863072	25.923597
186.288022	822.966838	25.928615
186.508501	819.391941	25.933632
186.267839	806.487943	25.938650
186.017539	811.576219	25.943668
186.734116	815.857572	25.948685
186.612942	807.573884	25.953703
186.839708	813.455709	25.958720
187.271808	804.113920	25.963738
187.097853	806.646798	25.968756
187.093567	813.744836	25.973773
187.614407	812.136527	25.978791
187.917026	819.445555	25.983808
188.419272	813.968069	25.988826
188.335260	814.767075	25.993844
188.653097	808.964860	25.998861
188.663361	811.772007	26.003879
188.720608	813.432623	26.008896
188.831895	805.608192	26.013914
188.931880	810.976438	26.018932
189.644002	819.483998	26.023949
189.845802	815.848896	26.028967
189.841091	819.945910	26.033984
190.263603	810.545651	26.039002
190.059901	820.167760	26.044020
190.359462	802.376646	26.049037
190.517046	804.832660	26.054055
191.105496	814.312500	26.059072
191.459938	809.097862	26.064090
191.557357	819.815461	26.069108
191.326691	809.361901	26.074125
191.682086	808.871232	26.079143
191.733293	814.486908	26.084160
191.791989	806.834762	26.089178
191.593146	802.031307	26.094196
192.236088	816.744318	26.099213
192.599282	812.635975	26.104231
192.606239	816.923671	26.109248
193.184737	809.960592	26.114266
193.243514	814.981814	26.119284
193.128116	817.164758	26.124301
193.583052	811.372755	26.129319
193.892720	818.289375	26.134336
193.938637	823.151660	26.139354
194.220816	825.591435	26.144372
194.477436	815.412291	26.149389
194.528700	815.783148	26.154407
194.565594	812.811176	26.159424
194.817507	810.550479	26.164442
194.856139	816.294343	26.169460
195.317318	815.989170	26.174477
195.859652	827.044592	26.179495
195.646265	821.804750	26.184512
196.293343	820.145230	26.189530
196.094139	819.475825	26.194548
195.945296	819.249847	26.199565
196.114572	826.778449	26.204583
196.407335	830.298990	26.209600
197.171367	821.448298	26.214618
197.416449	830.934271	26.219636
197.460369	817.332722	26.224653
197.808353	820.778394	26.229671
197.602171	820.801179	26.234688
197.816154	813.134320	26.239706
197.954691	822.898802	26.244724
198.449838	821.616378	26.249741
198.819621	822.104898	26.254759
198.607738	822.406274	26.259776
198.752734	820.323163	26.264794
199.072915	812.434649	26.269812
199.118477	820.146606	26.274829
199.564572	822.223198	26.279847
199.354184	821.886885	26.284864
199.635971	815.714749	26.289882
199.720489	816.096208	26.294900
199.873144	823.292889	26.299917
200.604899	827.051188	26.304935
200.348106	824.128094	26.309952
200.869946	817.596700	26.314970
200.931853	821.493999	26.319988
200.786535	813.141485	26.325005
201.425293	812.540428	26.330023
201.437087	826.834174	26.335040
201.787334	820.421010	26.340058
202.131580	818.524623	26.345076
201.985511	820.655540	26.350093
202.526391	819.899312	26.355111
202.497841	823.122748	26.360128
202.858351	822.280996	26.365146
203.208533	823.918096	26.370164
203.523410	823.228613	26.375181
204.266827	821.229054	26.380199
203.974954	819.371746	26.385216
204.033150	813.366961	26.390234
203.792030	813.313137	26.395252
203.941110	821.034225	26.400269
204.315422	817.192386	26.405287
204.438085	819.571791	26.410304
204.922814	823.330680	26.415322
205.560547	832.080198	26.420340
205.275685	824.752924	26.425357
205.566039	820.712723	26.430375
205.626033	815.392451	26.435392
205.900299	815.940022	26.440410
206.614734	826.362752	26.445428
206.312984	830.133639	26.450445
206.608759	828.730779	26.455463
206.782081	833.961387	26.460480
206.756076	823.109890	26.465498
207.046391	825.355899	26.470516
207.030688	830.047904	26.475533
208.217769	828.187548	26.480551
207.948063	837.166708	26.485568
208.281599	829.762088	26.490586
208.591560	832.932823	26.495604
208.397879	835.951602	26.500621
208.870053	822.917674	26.505639
208.552923	824.289448	26.510656
208.906962	829.996835	26.515674
209.218193	833.836386	26.520692
209.438442	835.481094	26.525709
209.852733	830.200328	26.530727
209.970875	835.212315	26.535744
210.080636	829.180563	26.540762
210.317291	829.027107	26.545780
210.585742	837.581664	26.550797
211.309725	834.931894	26.555815
211.176345	832.418763	26.560832
211.463063	835.242831	26.565850
211.687670	828.388488	26.570868
211.466067	834.198121	26.575885
211.820507	817.938439	26.580903
211.617514	829.520149	26.585920
211.751631	822.689364	26.590938
212.553020	833.575075	26.595956
212.436273	839.718670	26.600973
212.968627	829.335646	26.605991
212.749771	836.492347	26.611008
213.384999	833.405126	26.616026
213.989336	836.492162	26.621044
213.934737	835.339506	26.626061
214.131733	833.661698	26.631079
214.159524	838.634105	26.636096
213.810706	826.788318	26.641114
214.361503	819.312008	26.646132
214.232461	832.289660	26.651149
214.834767	826.395814	26.656167
215.309361	824.166715	26.661184
215.651988	824.059876	26.666202
215.975643	824.678652	26.671220
215.688796	827.491034	26.676237
216.170569	829.947071	26.681255
216.064682	826.558679	26.686272
216.085288	829.004466	26.691290
216.684152	827.223067	26.696308
216.780851	831.279051	26.701325
217.124972	830.329400	26.706343
217.735190	825.740793	26.711360
217.258605	826.635633	26.716378
217.985456	826.213360	26.721396
218.389967	841.171795	26.726413
218.667508	833.706464	26.731431
219.028382	831.769618	26.736448
219.120522	831.042230	26.741466
219.402493	818.997258	26.746484
219.248514	826.440492	26.751501
219.183033	820.953565	26.756519
219.275929	827.913407	26.761536
219.413212	831.230943	26.766554
219.455910	826.500325	26.771572
219.918279	832.272896	26.776589
220.327982	830.009720	26.781607
220.675758	823.259276	26.786624
220.919592	842.786973	26.791642
221.522709	844.081746	26.796660
221.571010	836.699440	26.801677
222.017783	834.957499	26.806695
222.257194	825.046108	26.811712
222.111805	830.919612	26.816730
222.444065	822.691548	26.821748
222.310418	823.905371	26.826765
222.217651	820.366619	26.831783
222.901829	833.668931	26.836800
223.171060	825.725227	26.841818
223.675554	834.968851	26.846836
223.713536	837.317262	26.851853
223.681558	831.774623	26.856871
223.995409	831.921567	26.861888
224.753787	841.226650	26.866906
224.986762	830.502081	26.871924
225.140244	835.442296	26.876941
225.469671	838.881394	26.881959
225.591738	832.854036	26.886976
225.698673	821.581063	26.891994
225.884898	827.563879	26.897012
225.633469	834.167087	26.902029
225.446485	823.757207	26.907047
226.189201	832.525095	26.912064
226.349692	840.348555	26.917082
226.700184	823.480426	26.922100
226.799275	831.105163	26.927117
226.903459	834.746582	26.932135
227.499398	828.187868	26.937152
227.874022	834.292829	26.942170
228.270025	830.157284	26.947188
227.904176	837.775517	26.952205
228.015265	831.674130	26.957223
228.458266	825.098204	26.962240
228.540528	838.787715	26.967258
229.256001	835.536526	26.972276
229.155009	834.750846	26.977293
229.368096	825.307445	26.982311
229.444902	831.727009	26.987328
229.765579	841.983843	26.992346
230.059497	829.820240	26.997364
230.313070	827.540347	27.002381
230.888560	841.149914	27.007399
231.091943	835.501205	27.012416
231.220627	836.355458	27.017434
231.611212	826.382662	27.022452
231.233642	834.542348	27.027469
231.690007	825.638569	27.032487
232.199515	837.093578	27.037504
232.313256	836.173483	27.042522
232.671206	833.075784	27.047540
232.423333	835.118414	27.052557
232.339673	832.392419	27.057575
233.211933	831.556198	27.062592
233.735229	847.745815	27.067610
233.675926	835.454168	27.072628
233.883313	829.075864	27.077645
233.942270	833.333380	27.082663
234.567509	825.974861	27.087680
234.691441	835.268268	27.092698
235.305952	834.396438	27.097716
235.607748	839.865817	27.102733
235.738867	837.352529	27.107751
236.183428	819.990085	27.112768
236.142604	836.412682	27.117786
236.292174	825.877820	27.122804
236.593760	832.410709	27.127821
236.537314	826.597332	27.132839
236.442754	819.357192	27.137856
236.692577	823.095853	27.142874
237.215549	829.042021	27.147892
237.407152	823.862196	27.152909
237.685420	835.747673	27.157927
237.684007	831.535148	27.162944
238.200722	842.727114	27.167962
238.492714	831.873436	27.172980
238.362144	844.879739	27.177997
238.437037	838.660911	27.183015
239.483782	837.182158	27.188032
239.475119	842.977576	27.193050
240.062165	835.883770	27.198068
240.156998	843.695364	27.203085
240.003822	841.797524	27.208103
240.403263	839.819960	27.213120
240.646448	842.941135	27.218138
241.159604	843.508319	27.223156
241.768050	848.819508	27.228173
241.649505	849.538687	27.233191
241.858050	832.304492	27.238208
241.755187	844.874147	27.243226
241.636139	840.395918	27.248244
242.109374	840.372884	27.253261
242.503065	840.491619	27.258279
243.020201	839.313065	27.263296
243.077346	846.344752	27.268314
243.314136	841.296740	27.273332
243.771415	834.257850	27.278349
243.540610	844.067227	27.283367
244.118471	841.888319	27.288384
244.649217	845.589560	27.293402
244.840398	836.133784	27.298420
245.015211	827.538919	27.303437
244.645786	831.765301	27.308455
245.098893	822.167770	27.313472
245.310917	832.854916	27.318490
245.427666	829.570713	27.323508
245.564740	827.782317	27.328525
245.869873	836.236493	27.333543
246.186241	832.918055	27.338560
246.229146	837.623029	27.343578
247.389879	842.939748	27.348596
247.934797	840.993182	27.353613
247.413667	831.563102	27.358631
247.687488	828.197642	27.363648
247.908719	824.755166	27.368666
248.214458	836.068336	27.373684
248.240526	830.592397	27.378701
247.987061	830.941271	27.383719
249.257206	835.458334	27.388736
249.625252	842.823459	27.393754
249.554002	843.718308	27.398772
250.044865	831.583999	27.403789
250.083906	830.328404	27.408807
249.916261	832.964443	27.413824
250.022346	829.407352	27.418842
250.989558	832.441049	27.423860
251.377501	829.969826	27.428877
251.048802	835.941298	27.433895
251.536615	825.208611	27.438912
251.428560	828.255083	27.443930
251.675932	825.168290	27.448948
252.193961	829.742488	27.453965
252.266944	840.829973	27.458983
252.817560	830.295784	27.464000
253.158129	841.067061	27.469018
253.816499	837.316690	27.474036
254.240880	835.363645	27.479053
253.789724	838.921116	27.484071
254.051043	827.201234	27.489088
254.289141	834.324663	27.494106
254.154290	830.842951	27.499124
254.942039	823.575894	27.504141
255.254435	842.991939	27.509159
255.392252	829.034937	27.514176
255.304442	839.509999	27.519194
255.726962	832.514389	27.524212
256.335675	831.605594	27.529229
256.533166	838.220962	27.534247
257.067718	840.583581	27.539264
257.095056	835.135844	27.544282
257.314531	836.938460	27.549300
257.662796	821.424482	27.554317
257.762494	830.005312	27.559335
257.726169	824.801013	27.564352
258.114219	834.551907	27.569370
258.484332	841.026795	27.574388
259.003828	829.222536	27.579405
259.298046	827.457011	27.584423
259.359411	822.635125	27.589440
259.170333	823.406310	27.594458
259.401182	830.063818	27.599476
260.217375	825.856543	27.604493
260.079404	839.731821	27.609511
260.584502	832.985280	27.614528
260.971108	832.799013	27.619546
260.901534	832.043154	27.624564
261.217673	827.733855	27.629581
261.763091	839.839670	27.634599
262.186144	835.015118	27.639616
262.322083	837.016927	27.644634
262.467954	832.421718	27.649652
262.533210	818.106800	27.654669
262.327435	821.884835	27.659687
262.679455	820.059819	27.664704
262.678106	817.431461	27.669722
262.994899	831.501013	27.674740
263.470440	825.046248	27.679757
263.870962	831.484842	27.684775
264.605765	825.993234	27.689792
264.872841	835.308538	27.694810
264.640866	847.835184	27.699828
265.335990	835.908905	27.704845
265.036005	838.107968	27.709863
265.419624	831.718003	27.714880
266.203885	839.860909	27.719898
266.049850	839.856640	27.724916
266.722635	831.752275	27.729933
266.767679	842.244524	27.734951
267.457340	845.539181	27.739968
267.694591	841.554577	27.744986
267.865997	837.460308	27.750004
268.261231	829.673703	27.755021
268.127229	828.754310	27.760039
268.000670	826.426304	27.765056
268.316648	835.298505	27.770074
269.195334	841.829912	27.775092
269.488492	837.079230	27.780109
269.926690	833.451498	27.785127
269.775250	836.807676	27.790144
269.971164	830.986565	27.795162
269.820565	834.800192	27.800180
270.770445	834.182256	27.805197
270.640985	845.569501	27.810215
271.018362	839.489767	27.815232
271.483662	840.073869	27.820250
271.957828	843.471502	27.825268
272.617881	837.764315	27.830285
273.008691	839.486610	27.835303
273.159187	834.000764	27.840320
273.237030	829.608645	27.845338
273.279220	835.115286	27.850356
273.410855	827.555909	27.855373
273.100144	825.505875	27.860391
273.573472	834.224194	27.865408
274.046529	835.782208	27.870426
274.260714	841.997359	27.875444
274.943532	827.150795	27.880461
275.233167	828.393391	27.885479
275.742046	828.711938	27.890496
276.271253	831.170060	27.895514
275.919963	840.944549	27.900532
275.600288	837.557880	27.905549
276.263411	830.228173	27.910567
276.236611	836.562889	27.915584
276.989802	830.547721	27.920602
277.327386	830.473225	27.925620
277.535391	829.797224	27.930637
277.872232	832.493573	27.935655
277.745330	833.835732	27.940672
278.177301	835.207644	27.945690
278.425051	842.559943	27.950708
278.571250	837.759558	27.955725
279.280625	840.009755	27.960743
279.827348	834.629475	27.965760
280.502307	836.821915	27.970778
280.335834	835.992782	27.975796
280.869271	828.733757	27.980813
281.149800	834.938576	27.985831
280.620710	828.198416	27.990848
281.016533	821.424711	27.995866
280.946553	823.180874	28.000884
280.841808	817.649566	28.005901
281.714293	829.205852	28.010919
281.925943	829.810509	28.015936
282.295753	839.122446	28.020954
282.014597	832.498314	28.025972
282.867750	832.659123	28.030989
283.530491	828.068649	28.036007
283.475754	835.925619	28.041024
284.110701	825.731743	28.046042
284.209468	832.138425	28.051060
284.631106	838.157178	28.056077
285.438762	835.399710	28.061095
285.176121	843.304830	28.066112
285.499454	829.606114	28.071130
285.498757	832.093088	28.076148
285.758966	830.591626	28.081165
286.157180	826.547252	28.086183
286.476237	842.803383	28.091200
287.049648	836.939276	28.096218
286.983948	833.554092	28.101236
287.014011	834.433167	28.106253
287.873005	839.863136	28.111271
288.312000	848.416398	28.116288
288.828922	835.283971	28.121306
288.306400	838.688455	28.126324
288.735357	838.647070	28.131341
289.180254	830.906379	28.136359
289.280754	838.988486	28.141376
289.602373	826.164175	28.146394
289.870281	838.164878	28.151412
290.740428	839.074106	28.156429
290.979015	837.607567	28.161447
291.049568	836.466983	28.166464
291.358245	832.414457	28.171482
291.512939	836.319408	28.176500
291.574957	830.639059	28.181517
292.343275	827.013580	28.186535
292.468513	838.048752	28.191552
293.164197	831.190490	28.196570
293.266047	841.071153	28.201588
292.931385	837.857226	28.206605
293.399922	830.147568	28.211623
293.903256	839.511300	28.216640
294.533115	831.426239	28.221658
294.520312	834.798703	28.226676
294.419801	835.549787	28.231693
294.824583	826.963296	28.236711
295.644491	833.383936	28.241728
295.866857	836.552534	28.246746
295.846057	840.084030	28.251764
295.861282	836.616820	28.256781
296.464500	834.323515	28.261799
296.832785	837.109642	28.266816
297.591954	839.197456	28.271834
297.698737	837.505291	28.276852
297.651483	834.880920	28.281869
298.405673	829.171703	28.286887
298.246911	832.150334	28.291904
298.639275	825.089994	28.296922
298.769971	839.769184	28.301940
298.883419	843.150395	28.306957
299.462915	833.750924	28.311975
300.171319	844.515433	28.316992
300.118965	840.749481	28.322010
300.641814	841.504501	28.327028
300.589979	839.483588	28.332045
300.516138	831.612223	28.337063
300.632022	838.896691	28.342080
301.002658	825.228480	28.347098
301.489898	831.937591	28.352116
301.808356	831.894475	28.357133
302.458267	825.059120	28.362151
302.977586	834.597082	28.367168
303.758217	835.753770	28.372186
303.854592	839.475302	28.377204
303.482833	844.935943	28.382221
304.023623	835.293193	28.387239
304.078266	836.663891	28.392256
304.567530	836.559470	28.397274
305.148667	838.889591	28.402292
305.167365	833.402173	28.407309
305.620172	831.315318	28.412327
305.836484	836.984196	28.417344
306.048292	839.251900	28.422362
306.440613	835.091679	28.427380
306.434568	837.999199	28.432397
306.904178	833.344119	28.437415
307.158548	841.225552	28.442432
308.002778	842.975084	28.447450
308.148699	830.642015	28.452468
307.969321	839.525071	28.457485
308.898879	831.557449	28.462503
309.172823	845.021477	28.467520
309.542057	838.255060	28.472538
309.645213	832.915435	28.477556
309.840391	838.060598	28.482573
310.101352	835.763774	28.487591
310.638452	840.385501	28.492608
311.176019	837.013690	28.497626
311.452384	834.301068	28.502644
311.843797	839.040147	28.507661
312.254910	826.637392	28.512679
312.274297	835.394830	28.517696
312.105903	825.083029	28.522714
312.267017	837.157164	28.527732
312.796707	849.760890	28.532749
313.102498	839.350012	28.537767
313.643513	846.214855	28.542784
314.356657	845.677957	28.547802
314.483966	839.760226	28.552820
314.451029	843.164228	28.557837
315.110373	844.939389	28.562855
315.424488	850.630915	28.567872
315.801782	846.173236	28.572890
315.978610	836.240018	28.577908
315.862735	839.874677	28.582925
316.317733	844.370335	28.587943
317.150491	845.604115	28.592960
317.719253	838.945485	28.597978
317.931659	834.475611	28.602996
317.593554	839.347201	28.608013
318.190393	832.182443	28.613031
318.485532	842.875596	28.618048
318.712473	833.736133	28.623066
319.055802	835.371149	28.628084
319.261139	838.835882	28.633101
319.575328	830.266648	28.638119
320.244238	843.334679	28.643136
320.884067	841.591082	28.648154
321.226927	843.314532	28.653172
321.282427	840.841417	28.658189
321.264906	830.319936	28.663207
321.251676	835.399716	28.668224
321.417562	831.950075	28.673242
322.436318	836.405298	28.678260
322.275913	836.420955	28.683277
322.768183	831.251120	28.688295
322.892410	834.719012	28.693312
323.167360	832.943862	28.698330
323.887249	840.172167	28.703348
323.975984	834.796917	28.708365
324.381395	827.428439	28.713383
324.434741	836.969523	28.718400
325.245343	841.706457	28.723418
325.363890	841.126433	28.728436
325.228013	837.240943	28.733453
325.885368	833.437083	28.738471
326.624028	829.898269	28.743488
326.754811	836.524027	28.748506
326.966754	828.078006	28.753524
327.210220	840.697888	28.758541
327.831805	832.894974	28.763559
328.159303	833.049261	28.768576
328.829016	834.298956	28.773594
329.033965	823.364156	28.778612
328.934295	834.169263	28.783629
329.696524	838.733851	28.788647
330.194554	837.277412	28.793664
330.068028	836.514641	28.798682
330.242924	828.759181	28.803700
330.754516	837.421058	28.808717
331.476998	829.889608	28.813735
331.564027	834.780215	28.818752
331.775975	838.963426	28.823770
331.908474	832.319071	28.828788
332.349434	832.433604	28.833805
332.576384	832.297439	28.838823
333.107850	839.106965	28.843840
333.657381	843.606841	28.848858
334.306093	835.099130	28.853876
334.775056	839.791424	28.858893
334.616874	840.693496	28.863911
334.734158	829.166439	28.868928
334.915349	839.650120	28.873946
335.651941	842.454647	28.878964
335.878302	841.576977	28.883981
336.175659	827.771850	28.888999
336.588468	828.985803	28.894016
336.909478	837.437516	28.899034
337.356498	828.023956	28.904052
337.554141	829.792104	28.909069
337.753720	830.045200	28.914087
338.544142	828.164553	28.919104
338.942562	827.774481	28.924122
339.572313	826.401675	28.929140
339.881698	832.213850	28.934157
340.013167	837.485694	28.939175
339.787529	826.674730	28.944192
339.922740	834.309632	28.949210
340.591274	828.579036	28.954228
340.954504	834.152461	28.959245
341.360495	834.253504	28.964263
341.405017	825.495885	28.969280
341.763926	833.935385	28.974298
342.467600	819.581023	28.979316
342.621382	833.098467	28.984333
342.986948	829.939623	28.989351
343.561605	834.328290	28.994368
343.784255	839.608030	28.999386
344.033166	836.243289	29.004404
344.467605	835.970683	29.009421
344.879196	834.306801	29.014439
345.458559	830.578197	29.019456
344.840275	825.716955	29.024474
345.128885	823.437918	29.029492
345.629164	829.119390	29.034509
346.283742	825.868216	29.039527
346.433116	828.729449	29.044544
346.746592	840.508476	29.049562
347.380079	835.354522	29.054580
347.599234	840.139356	29.059597
348.085555	837.577079	29.064615
348.264647	836.870866	29.069632
349.037788	842.453059	29.074650
349.081163	836.419010	29.079668
349.141734	829.385076	29.084685
349.517333	835.938008	29.089703
350.540959	845.501607	29.094720
350.675857	839.219784	29.099738
350.728046	820.697143	29.104756
351.219568	838.355974	29.109773
351.713770	836.960091	29.114791
352.341565	830.377478	29.119808
351.976195	834.221389	29.124826
352.927949	828.298380	29.129844
353.362173	840.696067	29.134861
353.493426	843.635862	29.139879
353.421826	829.099239	29.144896
353.906189	836.903843	29.149914
354.873542	830.839553	29.154932
355.181664	832.805091	29.159949
355.508142	838.516780	29.164967
355.522348	828.747733	29.169984
355.921457	842.245927	29.175002
356.390090	833.359161	29.180020
357.027285	834.550806	29.185037
356.729093	823.249376	29.190055
357.552621	825.948850	29.195072
357.768089	837.702111	29.200090
358.315839	832.204908	29.205108
358.404027	833.516737	29.210125
359.154799	831.686443	29.215143
359.801598	831.882537	29.220160
359.899829	840.510944	29.225178
360.078726	834.436862	29.230196
360.460022	831.777330	29.235213
360.365969	830.674996	29.240231
361.260696	832.287283	29.245248
361.577365	843.721842	29.250266
361.723664	826.642490	29.255284
362.071207	831.344220	29.260301
362.557547	841.016711	29.265319
363.216807	831.084123	29.270336
363.459872	834.751261	29.275354
363.531258	838.205292	29.280372
363.625443	826.672363	29.285389
364.269351	835.676552	29.290407
364.825315	836.262319	29.295424
365.051311	828.691402	29.300442
365.856308	840.479114	29.305460
366.226554	837.893883	29.310477
366.126176	834.450980	29.315495
367.086375	831.470953	29.320512
366.527966	827.667024	29.325530
366.722672	822.953760	29.330548
367.592547	827.447942	29.335565
367.880892	837.539411	29.340583
368.121003	831.070801	29.345600
368.139121	830.604239	29.350618
368.700795	839.059512	29.355636
369.082356	830.552368	29.360653
369.482146	835.681457	29.365671
369.844379	832.867105	29.370688
370.398589	838.063670	29.375706
371.174090	837.387680	29.380724
371.237790	831.173747	29.385741
371.039575	833.517908	29.390759
371.721418	833.705391	29.395776
372.626155	833.170223	29.400794
372.765430	842.783142	29.405812
372.890931	835.846390	29.410829
372.980293	841.673890	29.415847
374.278899	839.067202	29.420864
374.228487	838.866923	29.425882
374.292481	838.702481	29.430900
374.752380	835.383786	29.435917
375.006429	847.938916	29.440935
375.625498	833.910129	29.445952
376.147313	837.565429	29.450970
376.493643	841.106042	29.455988
376.893657	837.253883	29.461005
377.068043	834.882177	29.466023
377.868484	841.324792	29.471040
378.014990	843.119838	29.476058
378.105736	840.189964	29.481076
379.095537	839.351226	29.486093
379.525068	844.125402	29.491111
379.631645	839.078723	29.496128
380.207144	839.431081	29.501146
380.396974	837.217913	29.506164
381.140937	837.613470	29.511181
381.017036	837.743362	29.516199
381.583690	834.385957	29.521216
381.936104	831.342766	29.526234
382.343607	840.794008	29.531252
383.056784	843.475954	29.536269
383.071482	853.064093	29.541287
383.386455	835.421995	29.546304
383.722255	836.070440	29.551322
384.237701	842.658409	29.556340
384.647750	834.610719	29.561357
384.815629	838.415794	29.566375
385.273788	838.196298	29.571392
385.669725	837.181778	29.576410
386.164261	838.502928	29.581428
386.926243	848.504889	29.586445
386.905323	856.110463	29.591463
387.349910	839.158223	29.596480
387.703136	847.999396	29.601498
388.459233	848.803310	29.606516
388.828800	843.807203	29.611533
388.934365	841.651332	29.616551
389.563522	842.216239	29.621568
389.525320	837.286772	29.626586
390.160500	835.657507	29.631604
390.576738	840.518956	29.636621
391.091968	837.087507	29.641639
390.822091	834.560907	29.646656
391.705306	841.492399	29.651674
391.969761	847.623994	29.656692
392.235985	839.302055	29.661709
392.720296	838.838652	29.666727
393.300600	835.223507	29.671744
393.791166	834.459336	29.676762
393.970266	833.607959	29.681780
394.236632	828.003088	29.686797
394.425381	831.833314	29.691815
395.317627	832.937916	29.696832
395.622707	831.694550	29.701850
395.898611	834.422481	29.706868
395.986692	831.057532	29.711885
396.356490	832.265561	29.716903
396.630720	832.349249	29.721920
396.929129	839.100391	29.726938
397.498680	836.676631	29.731956
398.652656	833.331930	29.736973
398.858448	838.412330	29.741991
398.624435	834.791419	29.747008
399.428396	835.868742	29.752026
399.634327	841.100596	29.757044
400.229806	848.070575	29.762061
400.368571	839.904174	29.767079
401.107964	843.809619	29.772096
401.659518	841.221407	29.777114
401.860569	839.088540	29.782132
402.159067	835.400505	29.787149
402.634745	837.693401	29.792167
402.916667	846.176455	29.797184
403.407119	836.266986	29.802202
403.884429	843.652983	29.807220
404.632867	841.485389	29.812237
405.148109	844.097167	29.817255
405.293192	833.364174	29.822272
405.536038	837.574134	29.827290
406.129137	840.776536	29.832308
406.807040	830.462356	29.837325
406.831859	828.590450	29.842343
406.892701	837.319352	29.847360
407.412395	831.681352	29.852378
408.198334	836.545204	29.857396
408.490472	838.314421	29.862413
408.985915	844.144975	29.867431
409.857676	842.245353	29.872448
410.343447	833.595752	29.877466
410.145935	838.524350	29.882484
410.447159	835.189333	29.887501
410.749218	836.180695	29.892519
411.563831	842.390739	29.897536
412.054599	833.390073	29.902554
412.432582	842.056982	29.907572
412.824268	833.595593	29.912589
412.641885	841.876381	29.917607
413.053576	840.297687	29.922624
414.287051	832.730861	29.927642
414.497104	845.381204	29.932660
414.719612	833.976607	29.937677
415.242104	840.768603	29.942695
415.605605	842.867530	29.947712
416.407715	833.868886	29.952730
416.146792	846.125503	29.957748
416.625857	832.292075	29.962765
417.170081	831.390166	29.967783
417.639450	835.025231	29.972800
417.894641	831.063079	29.977818
418.758878	845.789033	29.982836
419.148980	832.597445	29.987853
419.601759	836.020504	29.992871
419.453091	835.100236	29.997888
420.325735	826.601843	30.002906
420.549170	837.981494	30.007924
420.963736	836.680057	30.012941
421.061312	835.118709	30.017959
421.452983	840.211197	30.022976
422.187929	832.829278	30.027994
422.581720	829.189523	30.033012
422.905393	833.885506	30.038029
423.162761	831.365184	30.043047
423.663928	840.811316	30.048064
424.246045	837.394699	30.053082
424.264670	832.926589	30.058100
424.690973	843.712941	30.063117
425.202841	832.408460	30.068135
425.139283	837.275179	30.073152
426.110302	834.646911	30.078170
426.429893	837.453246	30.083188
427.140493	848.820177	30.088205
427.882698	841.096304	30.093223
427.884301	848.616323	30.098240
428.657877	839.183470	30.103258
429.252942	836.452787	30.108276
429.656659	845.323971	30.113293
430.021019	837.191875	30.118311
430.071480	838.648431	30.123328
430.909435	827.886465	30.128346
431.042286	834.158464	30.133364
431.667219	835.090095	30.138381
431.885546	826.090821	30.143399
432.283371	847.399666	30.148416
432.756099	833.895418	30.153434
433.274643	844.828354	30.158452
433.848238	842.236709	30.163469
434.428849	833.540785	30.168487
434.557901	840.349853	30.173504
435.529862	839.356108	30.178522
435.717492	833.725622	30.183540
436.520673	836.238926	30.188557
436.733723	830.522435	30.193575
436.654549	842.845429	30.198592
437.579674	834.897426	30.203610
437.919032	837.823758	30.208628
438.083706	832.496641	30.213645
438.683575	840.772410	30.218663
438.756281	840.786489	30.223680
439.611776	835.705265	30.228698
440.274647	845.833111	30.233716
440.793964	846.478234	30.238733
441.454444	842.765401	30.243751
441.071218	842.799967	30.248768
441.836522	842.090853	30.253786
442.096231	835.366728	30.258804
442.585052	844.546549	30.263821
442.848507	842.325073	30.268839
443.826498	838.133630	30.273856
444.210882	834.334395	30.278874
444.387122	835.225428	30.283892
445.048775	835.400278	30.288909
445.393724	838.521396	30.293927
445.503951	835.452792	30.298944
446.296750	847.674755	30.303962
447.165068	843.784401	30.308980
447.141950	843.567250	30.313997
447.285873	840.354547	30.319015
448.159512	835.680745	30.324032
448.823182	836.344419	30.329050
449.101224	834.303705	30.334068
449.152333	838.114338	30.339085
449.908862	831.461188	30.344103
450.319584	833.688461	30.349120
450.715900	837.748302	30.354138
450.950557	846.027284	30.359156
451.800771	843.048600	30.364173
452.291361	832.892961	30.369191
452.080026	836.469903	30.374208
452.606151	833.841470	30.379226
452.996866	842.471687	30.384244
453.744646	837.284158	30.389261
453.970046	833.673773	30.394279
454.433779	842.548237	30.399296
454.601549	826.131389	30.404314
455.213140	836.122051	30.409332
455.997031	839.468318	30.414349
456.678698	839.315012	30.419367
456.967182	836.972877	30.424384
457.302499	837.555129	30.429402
457.906106	831.834638	30.434420
458.122495	849.255472	30.439437
458.645978	832.881067	30.444455
459.026084	843.693549	30.449472
459.728148	835.963304	30.454490
460.414564	833.619179	30.459508
461.025265	837.289047	30.464525
461.273589	826.397972	30.469543
461.785691	831.519047	30.474560
461.855444	834.455795	30.479578
462.476765	835.312251	30.484596
463.170062	834.005291	30.489613
463.503814	834.953852	30.494631
463.846838	824.212133	30.499648
464.579711	827.717816	30.504666
464.980306	829.485928	30.509684
465.083970	839.779725	30.514701
466.404215	834.951189	30.519719
466.570754	836.222421	30.524736
466.736509	833.277714	30.529754
467.158730	835.282296	30.534772
467.713707	840.567109	30.539789
468.485672	831.027214	30.544807
469.116030	833.772548	30.549824
469.745042	835.571371	30.554842
470.003234	826.597445	30.559860
470.128808	827.988660	30.564877
470.565903	830.672564	30.569895
471.113229	842.926430	30.574912
471.681004	836.776024	30.579930
472.166063	839.064307	30.584948
472.389414	832.525718	30.589965
473.118735	838.057938	30.594983
473.185350	823.720689	30.600000
473.956287	830.628638	30.605018
474.657956	833.646887	30.610036
474.828987	838.798973	30.615053
475.311629	832.658665	30.620071
475.933909	835.108618	30.625088
476.251377	835.898771	30.630106
476.665911	829.541855	30.635124
477.440974	831.011835	30.640141
477.897221	821.341218	30.645159
478.615137	830.232911	30.650176
478.953201	829.464081	30.655194
479.177531	832.335740	30.660212
479.288853	830.541883	30.665229
480.419189	827.888814	30.670247
480.838122	830.957389	30.675264
480.843387	828.157586	30.680282
481.641699	828.999111	30.685300
482.366740	842.519162	30.690317
482.528432	830.590710	30.695335
483.203034	832.757968	30.700352
483.945842	830.673302	30.705370
484.147643	823.996063	30.710388
484.239614	821.924359	30.715405
484.565904	819.661546	30.720423
484.739964	822.414800	30.725440
485.633893	829.114259	30.730458
485.622807	827.317368	30.735476
486.055526	832.182566	30.740493
486.879917	832.956917	30.745511
487.287739	838.141566	30.750528
488.381113	832.821343	30.755546
488.531464	835.445750	30.760564
488.983906	839.219151	30.765581
489.809106	828.762117	30.770599
490.281529	830.493801	30.775616
490.617313	832.398234	30.780634
491.541169	833.277018	30.785652
491.844774	835.924902	30.790669
491.894849	822.761004	30.795687
492.543701	827.437923	30.800704
493.193493	829.596421	30.805722
493.781654	833.781028	30.810740
494.501083	835.695161	30.815757
495.076964	836.385127	30.820775
495.378038	828.468006	30.825792
495.581572	823.059102	30.830810
496.448034	824.170878	30.835828
496.628755	824.761419	30.840845
497.343041	828.200572	30.845863
497.793989	824.933762	30.850880
498.537642	830.697275	30.855898
498.831223	824.709475	30.860916
499.090085	835.465094	30.865933
499.966666	823.652564	30.870951
500.303444	820.602341	30.875968
500.885934	829.316307	30.880986
501.250508	814.377266	30.886004
501.599468	825.311353	30.891021
502.770245	823.649200	30.896039
503.193525	828.616851	30.901056
503.068603	825.061004	30.906074
503.803958	825.180201	30.911092
504.548846	827.661558	30.916109
504.415363	819.805780	30.921127
505.702463	826.311491	30.926144
506.027121	818.602136	30.931162
506.593745	827.163941	30.936180
507.229532	822.722825	30.941197
507.679832	822.725456	30.946215
508.178746	820.404212	30.951232
508.247371	822.845684	30.956250
508.979789	819.238418	30.961268
509.833118	819.099413	30.966285
509.970468	814.767452	30.971303
510.661920	823.054208	30.976320
511.068517	820.504344	30.981338
511.693790	810.769548	30.986356
512.456675	825.946770	30.991373
512.703729	819.865232	30.996391
513.222362	817.761819	31.001408
513.282615	829.239460	31.006426
513.991454	828.267745	31.011444
514.686712	819.544508	31.016461
515.334425	831.363031	31.021479
515.986710	821.832303	31.026496
516.364751	816.860126	31.031514
516.711996	816.496957	31.036532
517.066459	822.264254	31.041549
517.372785	813.551076	31.046567
518.012563	817.263752	31.051584
518.079732	826.695401	31.056602
518.902505	822.619642	31.061620
519.720880	810.424870	31.066637
520.221112	810.669031	31.071655
520.404834	808.299029	31.076672
520.659738	825.101641	31.081690
521.348492	814.435486	31.086708
521.716952	823.075476	31.091725
522.419743	819.264544	31.096743
523.264584	830.648445	31.101760
523.408493	829.285006	31.106778
524.158507	821.878652	31.111796
524.491011	832.171537	31.116813
525.269600	837.247976	31.121831
525.590248	838.264849	31.126848
526.139976	848.167328	31.131866
526.743364	842.235431	31.136884
527.414181	846.918405	31.141901
527.419550	847.981204	31.146919
528.401616	847.408757	31.151936
528.867981	848.156798	31.156954
529.909040	856.231358	31.161972
530.330358	858.598996	31.166989
530.725372	852.301911	31.172007
531.051596	862.750423	31.177024
531.359438	862.617446	31.182042
531.841045	870.176361	31.187060
532.624918	871.386204	31.192077
533.219636	877.905053	31.197095
533.751424	874.452083	31.202112
534.417254	886.586555	31.207130
535.373006	875.721011	31.212148
535.557723	886.816404	31.217165
536.012842	896.809378	31.222183
536.276390	895.506203	31.227200
537.225140	907.874351	31.232218
537.472767	895.780996	31.237236
538.058201	914.899050	31.242253
538.684560	913.018693	31.247271
539.101475	914.588619	31.252288
539.732153	922.288448	31.257306
540.546497	923.897489	31.262324
541.135505	929.243306	31.267341
541.545276	931.827343	31.272359
542.554863	930.344908	31.277376
542.484795	948.586762	31.282394
542.841252	944.460496	31.287412
543.529312	949.907663	31.292429
543.855917	956.209509	31.297447
544.432575	957.350634	31.302464
545.178606	960.639708	31.307482
545.784359	967.447203	31.312500
546.265122	972.267095	31.317517
546.868559	983.713925	31.322535
547.720378	981.138908	31.327552
547.746312	995.926085	31.332570
548.308958	983.761538	31.337588
548.892116	999.140461	31.342605
549.545086	1002.172635	31.347623
550.167031	1007.693228	31.352640
550.642415	1018.790792	31.357658
551.534971	1020.696931	31.362676
551.945516	1027.563241	31.367693
551.854952	1031.080397	31.372711
553.029950	1032.500760	31.377728
553.397668	1039.746123	31.382746
554.210555	1048.241300	31.387764
554.208141	1052.016133	31.392781
554.425722	1054.630108	31.397799
555.181142	1064.500689	31.402816
555.443524	1077.581720	31.407834
555.873952	1068.053840	31.412852
556.571117	1083.878987	31.417869
557.148258	1102.127541	31.422887
557.586530	1103.059848	31.427904
558.534779	1112.354487	31.432922
559.170726	1120.782571	31.437940
559.849704	1119.865984	31.442957
560.362639	1130.266655	31.447975
561.213897	1125.501589	31.452992
561.653853	1141.941184	31.458010
561.650609	1152.520054	31.463028
562.109355	1152.164768	31.468045
562.724191	1160.627716	31.473063
563.385149	1165.132432	31.478080
563.863747	1181.225222	31.483098
564.308216	1192.722183	31.488116
565.021982	1205.407991	31.493133
565.936150	1218.005806	31.498151
566.742963	1216.895745	31.503168
567.363481	1222.164164	31.508186
567.650320	1228.794191	31.513204
568.692853	1236.688820	31.518221
569.092333	1253.971109	31.523239
569.513771	1257.553771	31.528256
569.957857	1272.626378	31.533274
570.615728	1277.355667	31.538292
571.652221	1277.863494	31.543309
571.639737	1294.278990	31.548327
571.951902	1299.983602	31.553344
572.925021	1311.963234	31.558362
573.291016	1321.014111	31.563380
574.068753	1325.828895	31.568397
574.589148	1341.527158	31.573415
575.723396	1345.431218	31.578432
576.172514	1350.685334	31.583450
576.428402	1363.309992	31.588468
577.010026	1369.711142	31.593485
577.470158	1378.873627	31.598503
578.251571	1391.154559	31.603520
578.844008	1405.513058	31.608538
579.550990	1402.300961	31.613556
579.929607	1413.350721	31.618573
580.524521	1429.624448	31.623591
581.173990	1435.797308	31.628608
581.688956	1440.103914	31.633626
582.068761	1448.357434	31.638644
583.293543	1457.725974	31.643661
583.535660	1474.553288	31.648679
583.909002	1474.952918	31.653696
584.950593	1484.905421	31.658714
585.065073	1495.343091	31.663732
585.822610	1496.503433	31.668749
586.511698	1512.626874	31.673767
586.778825	1523.589916	31.678784
587.590712	1534.790057	31.683802
587.872792	1544.138139	31.688820
588.924015	1547.515519	31.693837
589.060487	1564.337273	31.698855
589.500788	1575.926653	31.703872
590.121633	1583.473668	31.708890
590.851270	1594.396311	31.713908
592.087989	1604.432117	31.718925
592.329491	1620.584309	31.723943
592.636864	1620.937406	31.728960
593.429523	1628.422979	31.733978
593.660866	1635.961223	31.738996
593.893658	1647.033830	31.744013
594.422469	1659.079712	31.749031
594.754962	1667.492182	31.754048
595.647159	1686.380276	31.759066
595.906671	1698.023127	31.764084
597.155313	1713.210708	31.769101
598.167994	1716.830814	31.774119
598.412171	1736.220640	31.779136
598.993336	1731.882483	31.784154
599.759544	1751.815926	31.789172
600.035376	1759.549275	31.794189
600.324234	1771.667303	31.799207
601.179477	1785.212001	31.804224
601.975158	1809.227818	31.809242
601.995048	1820.046489	31.814260
602.995791	1840.091849	31.819277
603.990235	1853.668580	31.824295
604.673181	1867.846100	31.829312
605.260738	1866.407206	31.834330
605.470282	1887.781351	31.839348
606.214977	1900.639577	31.844365
606.926566	1914.986251	31.849383
607.461176	1919.147901	31.854400
608.469111	1933.438990	31.859418
608.916047	1952.851138	31.864436
609.480864	1965.626956	31.869453
610.032732	1982.226642	31.874471
610.786950	1993.647500	31.879488
611.078309	2004.439802	31.884506
611.613546	2024.946019	31.889524
612.392961	2034.210625	31.894541
613.126610	2054.853254	31.899559
613.687094	2073.960667	31.904576
614.788377	2079.949803	31.909594
614.556824	2105.823841	31.914612
615.382626	2112.146222	31.919629
615.772596	2142.212511	31.924647
616.595226	2150.817165	31.929664
617.521294	2170.751441	31.934682
617.475669	2200.074552	31.939700
618.652698	2208.513605	31.944717
619.317933	2230.779794	31.949735
619.609481	2241.433347	31.954752
620.600017	2253.136338	31.959770
620.994706	2273.358590	31.964788
621.833131	2279.997823	31.969805
622.504531	2305.387578	31.974823
623.045340	2311.599754	31.979840
624.296224	2327.797436	31.984858
624.960791	2338.579181	31.989876
625.698991	2344.855320	31.994893
625.778976	2349.523374	31.999911
626.066613	2363.731271	32.004928
626.817800	2380.268739	32.009946
627.084463	2405.131469	32.014964
627.776948	2411.326381	32.019981
628.622415	2430.089989	32.024999
629.404540	2451.864856	32.030016
629.944060	2469.909221	32.035034
630.264446	2489.370058	32.040052
630.842492	2509.251586	32.045069
632.116987	2527.415140	32.050087
632.095571	2543.684841	32.055104
633.320733	2548.850065	32.060122
633.896206	2565.964211	32.065140
634.400189	2567.864745	32.070157
634.991566	2588.116699	32.075175
635.306714	2605.422898	32.080192
636.369666	2614.577393	32.085210
636.560256	2636.845390	32.090228
636.968477	2640.572415	32.095245
637.764889	2654.631906	32.100263
637.862903	2683.703056	32.105280
638.770158	2697.095177	32.110298
638.933240	2721.649397	32.115316
640.136646	2729.039936	32.120333
640.702699	2757.533372	32.125351
640.914735	2781.076421	32.130368
641.758299	2805.262868	32.135386
642.679878	2823.699434	32.140404
643.311180	2841.755135	32.145421
644.170914	2865.778187	32.150439
644.740903	2890.496532	32.155456
645.405732	2902.821912	32.160474
645.822406	2922.265075	32.165492
646.995983	2939.021356	32.170509
648.142286	2955.030745	32.175527
648.263486	2969.899411	32.180544
649.221510	2980.462276	32.185562
649.583340	3004.136948	32.190580
650.417967	3014.330841	32.195597
651.124542	3037.958203	32.200615
651.450394	3057.706014	32.205632
652.078636	3081.938980	32.210650
652.508233	3107.294927	32.215668
653.283123	3117.577081	32.220685
654.318301	3138.742131	32.225703
654.683696	3164.095527	32.230720
655.449879	3172.943022	32.235738
655.605026	3212.541363	32.240756
656.748312	3229.113264	32.245773
657.522763	3250.811395	32.250791
657.712124	3278.796191	32.255808
658.924107	3284.058372	32.260826
659.450036	3301.796388	32.265844
659.959129	3337.773431	32.270861
661.102270	3344.823275	32.275879
661.613114	3362.727821	32.280896
662.362291	3377.129791	32.285914
662.777343	3409.110106	32.290932
663.547533	3429.303614	32.295949
664.362312	3449.726918	32.300967
664.625793	3469.055648	32.305984
665.400619	3490.283737	32.311002
666.097276	3514.992694	32.316020
666.978169	3536.349511	32.321037
667.373829	3557.179054	32.326055
667.749411	3589.651891	32.331072
668.680894	3609.110343	32.336090
669.335884	3629.700757	32.341108
669.971194	3651.708251	32.346125
670.359707	3678.696859	32.351143
671.304842	3712.469997	32.356160
671.864104	3726.643001	32.361178
672.469713	3749.968238	32.366196
673.139902	3778.778490	32.371213
674.006834	3803.253023	32.376231
674.635992	3839.310221	32.381248
674.950005	3871.452273	32.386266
676.046094	3883.591256	32.391284
676.668869	3911.418032	32.396301
677.282635	3937.753332	32.401319
677.888271	3961.700626	32.406336
678.717712	3984.653599	32.411354
679.252779	4006.737102	32.416372
679.819391	4022.124369	32.421389
680.660250	4040.268595	32.426407
680.684116	4067.598617	32.431424
681.740183	4079.655588	32.436442
682.599201	4092.589133	32.441460
683.253733	4125.126823	32.446477
683.641199	4137.969680	32.451495
684.251512	4174.257736	32.456512
684.978682	4183.320125	32.461530
685.740334	4223.126118	32.466548
686.522126	4243.672245	32.471565
687.019904	4265.758714	32.476583
687.740567	4303.077755	32.481600
688.372237	4317.265204	32.486618
689.374564	4346.185633	32.491636
690.019209	4385.678782	32.496653
690.401058	4401.849507	32.501671
691.271940	4430.585370	32.506688
692.066038	4449.292809	32.511706
692.886728	4478.292228	32.516724
693.652626	4508.812130	32.521741
694.460274	4536.462742	32.526759
695.031959	4569.452867	32.531776
695.744296	4586.604450	32.536794
696.940825	4603.522854	32.541812
697.453318	4631.184837	32.546829
698.249566	4652.076385	32.551847
698.510512	4682.359546	32.556864
699.018697	4714.144602	32.561882
699.893829	4738.104633	32.566900
700.638833	4770.370576	32.571917
701.581002	4794.935750	32.576935
701.784989	4829.356638	32.581952
702.564681	4855.089818	32.586970
703.467343	4887.710199	32.591988
703.878847	4922.035829	32.597005
704.788990	4952.786543	32.602023
705.533662	4978.250738	32.607040
706.092525	4998.996565	32.612058
707.368445	5033.528740	32.617076
708.105246	5049.019806	32.622093
709.195606	5074.922734	32.627111
710.181434	5090.741221	32.632128
710.871039	5116.583492	32.637146
711.613906	5134.122248	32.642164
712.001866	5149.737147	32.647181
712.789590	5161.849248	32.652199
712.703780	5189.377954	32.657216
713.414144	5214.251244	32.662234
714.194978	5239.082032	32.667252
715.070169	5289.011407	32.672269
715.654652	5301.032135	32.677287
716.390951	5343.325564	32.682304
716.824424	5371.941625	32.687322
717.775284	5400.085778	32.692340
718.318326	5434.530788	32.697357
719.355416	5461.793564	32.702375
720.059021	5502.378447	32.707392
720.570098	5516.913895	32.712410
721.481675	5550.746201	32.717428
722.283198	5574.583068	32.722445
723.276890	5595.609111	32.727463
723.619866	5628.965052	32.732480
724.160514	5651.718889	32.737498
724.870998	5680.083978	32.742516
725.596524	5715.255537	32.747533
726.435859	5748.215612	32.752551
726.873363	5778.896100	32.757568
727.531647	5802.304170	32.762586
728.398593	5826.383712	32.767604
728.818009	5856.145416	32.772621
729.648562	5879.889779	32.777639
730.500796	5911.105687	32.782656
730.979847	5936.562072	32.787674
732.443387	5952.846733	32.792692
732.935893	5982.928713	32.797709
733.346006	6000.434879	32.802727
734.261417	6023.288674	32.807744
735.083263	6056.558226	32.812762
735.886512	6080.701684	32.817780
736.430121	6120.337446	32.822797
737.524256	6136.007410	32.827815
738.014879	6168.381728	32.832832
738.878158	6202.248020	32.837850
739.571440	6232.097129	32.842868
740.109827	6265.468009	32.847885
740.651037	6288.048937	32.852903
741.626461	6324.994713	32.857920
742.480282	6347.568088	32.862938
743.446801	6373.817293	32.867956
743.894522	6403.875372	32.872973
744.946801	6442.214159	32.877991
745.478988	6468.070232	32.883008
745.989278	6505.335005	32.888026
747.214226	6532.311294	32.893044
747.640010	6565.293032	32.898061
748.186317	6598.098231	32.903079
749.120577	6633.586311	32.908096
749.485887	6678.352350	32.913114
750.775465	6710.167623	32.918132
751.127810	6747.410126	32.923149
752.043775	6780.909419	32.928167
752.543637	6822.548598	32.933184
753.550531	6862.312728	32.938202
754.161276	6889.823953	32.943220
754.638100	6931.864722	32.948237
755.370029	6970.974239	32.953255
756.466519	7019.257619	32.958272
757.548011	7056.579810	32.963290
758.248253	7086.801738	32.968308
758.768597	7129.338121	32.973325
759.680874	7170.715010	32.978343
760.917531	7193.109876	32.983360
761.374886	7232.726752	32.988378
762.367361	7267.957610	32.993396
762.485444	7305.297694	32.998413
763.835717	7337.091985	33.003431
764.840352	7364.545764	33.008448
765.187938	7400.634918	33.013466
766.468664	7428.273109	33.018484
767.321191	7466.095841	33.023501
768.058496	7494.551126	33.028519
769.069424	7523.835167	33.033536
769.641416	7561.812259	33.038554
770.672149	7576.385262	33.043572
771.186704	7605.472051	33.048589
771.795558	7628.726000	33.053607
772.705572	7651.156493	33.058624
773.249359	7687.859682	33.063642
774.157284	7724.351569	33.068660
774.434291	7762.412879	33.073677
775.269581	7791.020690	33.078695
775.990707	7825.294108	33.083712
776.728491	7874.740516	33.088730
777.657824	7893.976610	33.093748
778.205531	7925.871603	33.098765
778.699442	7950.807578	33.103783
779.681281	7995.692372	33.108800
780.217214	8027.336815	33.113818
780.726711	8061.226895	33.118836
781.425994	8100.186052	33.123853
782.016675	8145.479373	33.128871
782.713206	8179.226902	33.133888
783.360317	8211.637295	33.138906
784.525512	8257.554945	33.143924
785.325151	8302.203659	33.148941
786.675399	8335.442454	33.153959
787.571713	8363.962731	33.158976
788.474942	8400.541933	33.163994
789.533194	8434.505128	33.169012
790.045811	8475.078980	33.174029
790.431037	8505.705874	33.179047
791.749058	8527.739277	33.184064
792.616714	8570.070230	33.189082
793.521421	8590.226443	33.194100
793.971927	8632.758232	33.199117
794.318048	8674.245583	33.204135
795.505802	8712.078680	33.209152
796.044508	8747.919724	33.214170
796.949650	8783.757467	33.219188
797.657771	8838.628696	33.224205
798.091201	8879.503061	33.229223
799.173930	8914.609372	33.234240
800.505201	8955.959785	33.239258
800.812004	8991.793202	33.244276
801.599515	9038.522994	33.249293
802.207989	9080.753393	33.254311
803.349231	9120.741444	33.259328
804.362154	9171.938618	33.264346
805.778823	9200.903281	33.269364
806.856454	9236.850812	33.274381
807.400550	9278.712821	33.279399
808.224709	9303.264552	33.284416
809.050295	9342.563434	33.289434
809.620725	9378.542838	33.294452
810.395222	9410.180931	33.299469
811.291931	9441.992644	33.304487
811.778304	9479.175604	33.309504
812.635095	9525.611690	33.314522
813.194474	9558.394874	33.319540
813.792583	9600.833293	33.324557
814.831863	9648.775708	33.329575
815.659650	9690.168253	33.334592
816.667658	9732.015900	33.339610
817.024153	9775.370054	33.344628
817.920153	9819.821154	33.349645
818.810900	9861.052730	33.354663
820.076952	9913.387065	33.359680
820.626947	9951.681913	33.364698
821.418198	9989.809834	33.369716
822.050664	10042.975663	33.374733
822.994579	10096.781461	33.379751
823.972577	10129.636254	33.384768
824.389542	10174.383787	33.389786
826.063096	10213.855622	33.394804
826.906715	10245.995874	33.399821
827.522990	10287.807876	33.404839
828.133802	10328.534683	33.409856
828.479719	10376.353264	33.414874
829.892662	10410.119638	33.419892
830.673076	10461.845962	33.424909
831.374172	10504.415654	33.429927
831.967960	10537.586727	33.434944
833.105695	10581.509462	33.439962
833.414322	10613.803094	33.444980
834.060717	10661.509326	33.449997
834.747625	10701.151573	33.455015
835.922356	10743.215510	33.460032
836.811027	10777.610404	33.465050
837.582985	10823.560903	33.470068
838.882580	10865.280460	33.475085
838.892676	10924.285971	33.480103
839.690131	10958.313341	33.485120
840.356723	11009.872612	33.490138
841.481771	11047.941267	33.495156
842.570075	11098.566823	33.500173
843.352295	11151.507263	33.505191
844.303696	11193.989043	33.510208
844.976680	11243.956571	33.515226
845.915165	11288.249845	33.520244
847.326634	11329.084701	33.525261
847.873735	11382.766530	33.530279
848.382236	11435.968255	33.535296
849.230513	11482.596845	33.540314
849.916466	11530.267560	33.545332
850.714191	11576.724271	33.550349
851.627487	11636.687110	33.555367
853.041685	11683.307045	33.560384
853.777281	11732.154650	33.565402
855.080646	11757.970703	33.570420
856.711570	11802.116355	33.575437
857.247456	11850.385935	33.580455
858.348473	11879.198676	33.585472
859.148053	11927.165321	33.590490
859.956951	11956.074176	33.595508
860.750320	12005.747123	33.600525
861.294964	12055.408397	33.605543
862.187407	12093.228043	33.610560
862.786365	12150.159563	33.615578
863.766203	12182.746127	33.620596
864.376162	12221.550997	33.625613
865.538391	12277.394230	33.630631
866.120140	12318.546713	33.635648
867.205312	12376.577902	33.640666
867.605102	12430.115140	33.645684
868.568182	12470.513894	33.650701
869.412217	12516.792048	33.655719
871.022361	12556.812380	33.660736
872.041047	12598.923732	33.665754
872.583686	12656.525523	33.670772
873.610180	12695.484418	33.675789
874.298597	12754.285877	33.680807
875.092049	12783.738395	33.685824
876.003655	12841.738039	33.690842
876.506036	12887.160841	33.695860
877.486455	12931.603043	33.700877
878.086821	12992.256801	33.705895
879.361358	13031.414618	33.710912
880.378051	13085.757671	33.715930
880.947832	13134.625258	33.720948
882.456212	13171.460680	33.725965
882.695632	13232.439814	33.730983
883.501265	13276.663725	33.736000
884.086195	13332.170481	33.741018
885.032466	13393.902206	33.746036
886.636800	13443.657971	33.751053
887.438071	13491.059916	33.756071
888.382562	13522.043769	33.761088
889.679219	13562.171885	33.766106
890.780180	13611.216969	33.771124
891.643919	13653.916911	33.776141
892.080924	13692.802260	33.781159
893.039582	13725.549535	33.786176
893.488109	13771.447064	33.791194
894.359428	13811.461917	33.796212
895.072087	13842.539228	33.801229
895.917441	13892.426956	33.806247
896.738437	13932.222523	33.811264
897.386843	13981.064269	33.816282
898.257172	14035.113879	33.821300
899.117512	14083.392353	33.826317
899.472025	14141.763771	33.831335
900.266924	14196.864572	33.836352
901.396079	14258.763290	33.841370
902.648400	14309.176159	33.846388
903.481807	14369.715945	33.851405
904.394655	14439.244055	33.856423
906.236135	14476.551256	33.861440
906.980022	14525.543760	33.866458
907.437789	14583.082516	33.871476
908.468655	14631.705338	33.876493
909.182201	14693.742806	33.881511
909.885448	14744.614961	33.886528
910.759655	14808.626885	33.891546
911.941172	14860.378655	33.896564
912.876981	14923.137068	33.901581
913.527417	14983.056709	33.906599
915.012618	15038.425158	33.911616
916.118112	15083.421415	33.916634
917.083618	15146.504391	33.921652
918.245332	15196.295766	33.926669
918.946791	15249.092889	33.931687
919.779465	15312.102344	33.936704
921.043529	15362.456175	33.941722
921.825499	15413.971615	33.946740
923.066991	15456.256770	33.951757
923.943129	15504.507970	33.956775
924.695325	15561.495369	33.961792
925.698959	15607.235118	33.966810
926.092170	15669.894113	33.971828
927.536622	15713.351548	33.976845
928.624406	15763.427525	33.981863
929.652013	15811.927537	33.986880
930.546860	15863.609800	33.991898
931.295650	15914.152680	33.996916
931.973696	15970.079013	34.001933
932.893010	16023.087553	34.006951
933.592577	16077.201124	34.011968
934.688415	16145.159381	34.016986
935.594773	16204.354494	34.022004
936.770519	16247.346477	34.027021
937.431669	16306.188437	34.032039
938.166495	16360.666850	34.037056
939.453905	16418.675765	34.042074
940.186510	16478.044056	34.047092
940.791945	16539.700069	34.052109
941.829080	16609.639963	34.057127
942.881007	16673.624151	34.062144
943.779149	16736.877622	34.067162
945.103809	16786.161374	34.072180
946.158858	16835.348249	34.077197
947.440294	16890.813800	34.082215
948.303167	16943.918950	34.087232
948.842538	16999.917248	34.092250
949.704424	17054.579994	34.097268
950.720966	17105.254892	34.102285
951.628681	17161.891195	34.107303
952.952643	17211.820487	34.112320
954.076069	17255.315605	34.117338
954.944224	17315.524503	34.122356
955.981356	17352.128697	34.127373
956.889702	17401.112441	34.132391
957.550498	17446.631995	34.137408
958.384026	17491.957364	34.142426
958.888143	17543.370165	34.147444
959.759707	17594.656415	34.152461
960.645691	17654.904660	34.157479
961.492521	17707.148956	34.162496
962.333638	17768.680618	34.167514
963.135335	17834.767036	34.172532
964.272540	17886.467554	34.177549
965.291521	17957.757592	34.182567
966.222335	18017.722029	34.187584
967.109894	18067.149753	34.192602
968.185571	18135.020259	34.197620
969.372669	18198.653652	34.202637
970.399876	18268.579001	34.207655
971.512903	18334.365968	34.212672
972.566948	18387.142098	34.217690
973.137163	18461.473043	34.222708
974.259700	18518.578965	34.227725
975.230391	18582.196765	34.232743
976.237373	18646.251351	34.237760
977.750319	18700.788983	34.242778
978.881444	18762.247073	34.247796
979.832771	18819.544790	34.252813
980.550709	18884.940261	34.257831
981.605599	18939.562503	34.262848
982.493745	19000.414772	34.267866
983.711985	19056.060642	34.272884
984.602589	19117.601521	34.277901
985.983748	19166.121281	34.282919
986.640658	19235.507577	34.287936
988.150688	19290.457974	34.292954
988.872766	19355.367918	34.297972
989.704494	19414.448660	34.302989
990.849514	19471.882412	34.308007
991.739998	19538.453601	34.313024
992.871655	19592.572940	34.318042
993.474920	19667.073929	34.323060
994.678416	19724.429828	34.328077
995.564639	19784.956320	34.333095
996.797048	19840.349514	34.338112
998.243858	19888.317519	34.343130
999.392565	19938.909765	34.348148
1000.667790	20000.210342	34.353165
1001.487920	20050.803481	34.358183
1002.074534	20111.415532	34.363200
1003.100445	20165.818279	34.368218
1003.967229	20216.764713	34.373236
1005.106786	20282.288785	34.378253
1006.288399	20337.596527	34.383271
1006.665313	20401.413790	34.388288
1007.821880	20461.729710	34.393306
1008.752641	20520.071801	34.398324
1009.794222	20584.872916	34.403341
1011.035985	20650.521311	34.408359
1012.098563	20701.274257	34.413376
1013.221765	20764.382625	34.418394
1014.123277	20817.700863	34.423412
1015.145669	20880.559932	34.428429
1016.543165	20929.492228	34.433447
1016.763470	21000.721865	34.438464
1018.130691	21046.222020	34.443482
1018.779951	21110.946942	34.448500
1019.584252	21180.898483	34.453517
1020.869085	21229.697426	34.458535
1021.724638	21298.542014	34.463552
1022.820990	21348.021384	34.468570
1023.610206	21409.515759	34.473588
1024.250895	21470.370010	34.478605
1025.347814	21527.766743	34.483623
1026.126138	21598.178740	34.488640
1027.151370	21661.930771	34.493658
1027.979920	21728.133616	34.498676
1029.161523	21800.069508	34.503693
1030.334651	21872.645156	34.508711
1030.987995	21940.455627	34.513728
1032.246748	22007.199028	34.518746
1032.991794	22080.644540	34.523764
1034.077901	22146.878204	34.528781
1035.189257	22223.199080	34.533799
1036.191835	22300.996802	34.538816
1037.744601	22371.783869	34.543834
1038.822975	22447.523104	34.548852
1039.743361	22522.623751	34.553869
1041.164854	22588.364376	34.558887
1041.805023	22665.847138	34.563904
1043.145239	22719.317078	34.568922
1044.246000	22796.311611	34.573940
1045.831846	22868.093687	34.578957
1046.669164	22932.390900	34.583975
1047.479585	22998.076353	34.588992
1048.801064	23058.595724	34.594010
1049.821099	23138.144366	34.599028
1050.242700	23198.267127	34.604045
1051.701249	23279.416288	34.609063
1053.016898	23354.231075	34.614080
1054.205179	23411.404213	34.619098
1055.275601	23487.338232	34.624116
1056.280771	23564.464371	34.629133
1057.316533	23619.943055	34.634151
1058.013545	23694.703762	34.639168
1059.241268	23759.416819	34.644186
1060.713304	23825.760321	34.649204
1061.459747	23897.070140	34.654221
1063.056540	23951.539815	34.659239
1064.000631	24021.144718	34.664256
1065.063638	24095.262269	34.669274
1066.397768	24152.636011	34.674292
1067.384705	24216.503335	34.679309
1068.860816	24285.135324	34.684327
1069.880326	24346.185892	34.689344
1070.784128	24407.065076	34.694362
1071.449671	24469.239092	34.699380
1072.527264	24539.191546	34.704397
1073.673457	24598.283107	34.709415
1074.790015	24677.987181	34.714432
1075.639495	24739.273959	34.719450
1076.634072	24807.293877	34.724468
1077.561913	24877.738469	34.729485
1079.237761	24939.371192	34.734503
1080.490609	25001.373288	34.739520
1081.148018	25066.135123	34.744538
1082.810410	25140.991118	34.749556
1083.217602	25212.465871	34.754573
1084.328031	25271.451235	34.759591
1085.574397	25342.618876	34.764608
1086.435136	25413.714083	34.769626
1087.520863	25489.912443	34.774644
1088.431614	25558.548331	34.779661
1089.578764	25638.693846	34.784679
1090.913893	25705.153379	34.789696
1091.289941	25784.806486	34.794714
1092.720243	25853.033877	34.799732
1093.488333	25922.988779	34.804749
1094.683145	25981.356389	34.809767
1095.710293	26051.043897	34.814784
1096.300014	26115.491015	34.819802
1097.232447	26180.814021	34.824820
1098.235326	26259.101126	34.829837
1099.505492	26336.139814	34.834855
1100.538752	26416.432552	34.839872
1101.506097	26491.907372	34.844890
1102.286970	26567.310379	34.849908
1103.639166	26662.128479	34.854925
1104.878242	26745.980294	34.859943
1106.182083	26825.809094	34.864960
1107.266136	26906.873250	34.869978
1108.623351	26988.287062	34.874996
1109.616218	27062.224236	34.880013
1110.561622	27134.829181	34.885031
1111.649644	27228.635581	34.890048
1113.105142	27324.995490	34.895066
1114.277693	27402.344169	34.900084
1115.412013	27477.948363	34.905101
1116.607317	27551.078409	34.910119
1118.003942	27634.606003	34.915136
1119.899160	27703.039056	34.920154
1121.216496	27763.819779	34.925172
1122.115494	27836.516625	34.930189
1123.489207	27901.909229	34.935207
1124.529005	27975.406314	34.940224
1125.468992	28050.827995	34.945242
1126.592123	28112.411093	34.950260
1127.441553	28182.000870	34.955277
1128.275719	28256.769807	34.960295
1129.440672	28333.168808	34.965312
1130.488473	28419.952147	34.970330
1131.986232	28497.842192	34.975348
1132.705248	28577.294866	34.980365
1134.094094	28658.135269	34.985383
1135.099684	28742.998740	34.990400
1135.796979	28826.804422	34.995418
1137.210349	28908.071807	35.000436
1138.208759	29001.312494	35.005453
1140.236696	29070.772424	35.010471
1141.195089	29156.390816	35.015488
1141.973459	29241.000963	35.020506
1143.477230	29309.196949	35.025524
1144.117768	29399.119794	35.030541
1145.725675	29470.991529	35.035559
1147.067105	29547.127403	35.040576
1148.015541	29632.528099	35.045594
1149.015046	29711.657070	35.050612
1150.239190	29800.605889	35.055629
1151.282875	29870.923380	35.060647
1152.705990	29953.565070	35.065664
1153.736965	30034.713137	35.070682
1154.603654	30116.455999	35.075700
1155.590228	30207.333580	35.080717
1156.818203	30286.985465	35.085735
1157.771691	30371.408658	35.090752
1158.821508	30463.933687	35.095770
1159.867048	30542.673092	35.100788
1161.073986	30649.839860	35.105805
1162.806158	30736.558081	35.110823
1163.831690	30822.255136	35.115840
1165.255188	30902.169747	35.120858
1166.246453	30986.355685	35.125876
1167.752265	31065.897797	35.130893
1169.420988	31133.897162	35.135911
1170.593608	31195.899037	35.140928
1171.606116	31276.776720	35.145946
1173.178770	31323.747407	35.150964
1173.924508	31400.374791	35.155981
1174.962307	31456.070574	35.160999
1175.825749	31520.858781	35.166016
1176.530699	31590.950391	35.171034
1178.442731	31656.144746	35.176052
1179.046949	31724.368646	35.181069
1180.201379	31800.510344	35.186087
1181.385924	31877.918292	35.191104
1182.916822	31952.668075	35.196122
1184.389245	32029.601904	35.201140
1185.370387	32111.878508	35.206157
1186.532771	32173.480310	35.211175
1187.397907	32256.913463	35.216192
1188.633159	32331.881319	35.221210
1189.995030	32415.895260	35.226228
1190.757568	32496.032695	35.231245
1191.651905	32583.015500	35.236263
1193.160825	32650.292413	35.241280
1194.141497	32755.096630	35.246298
1195.513347	32844.168304	35.251316
1196.918348	32925.433849	35.256333
1197.801059	33013.368558	35.261351
1198.728839	33107.485911	35.266368
1199.917685	33202.751603	35.271386
1201.228964	33294.376102	35.276404
1202.687318	33386.401693	35.281421
1203.400520	33480.611024	35.286439
1204.785814	33578.187049	35.291456
1205.731148	33669.946019	35.296474
1207.582339	33759.794159	35.301492
1209.140407	33848.992861	35.306509
1210.563717	33940.280311	35.311527
1211.988430	34019.751505	35.316544
1213.266122	34110.347938	35.321562
1214.496039	34192.884840	35.326580
1215.877423	34269.632455	35.331597
1216.952309	34357.821076	35.336615
1218.390359	34434.794404	35.341632
1219.535646	34521.961162	35.346650
1220.801754	34601.427631	35.351668
1221.852069	34683.343195	35.356685
1222.848883	34769.927127	35.361703
1224.070939	34854.118032	35.366720
1225.176215	34951.282470	35.371738
1226.593165	35031.877798	35.376756
1227.500466	35120.797508	35.381773
1228.776996	35214.357875	35.386791
1230.058979	35296.600152	35.391808
1231.442434	35394.804514	35.396826
1232.671113	35493.811124	35.401844
1233.646151	35586.218739	35.406861
1234.968898	35677.308069	35.411879
1236.307579	35756.331313	35.416896
1237.361486	35851.016677	35.421914
1238.797247	35939.326446	35.426932
1239.845551	36038.363676	35.431949
1240.921661	36118.788572	35.436967
1243.032866	36213.102321	35.441984
1244.487694	36296.908647	35.447002
1245.890303	36368.197505	35.452020
1247.038437	36446.993737	35.457037
1247.964120	36535.473904	35.462055
1249.993058	36602.233579	35.467072
1250.901784	36686.809339	35.472090
1252.230551	36762.227367	35.477108
1253.381280	36837.629112	35.482125
1254.531545	36910.533536	35.487143
1255.620388	36972.970209	35.492160
1256.492205	37045.399933	35.497178
1257.405065	37118.759354	35.502196
1258.408228	37193.021847	35.507213
1259.913804	37264.164890	35.512231
1261.398041	37334.571664	35.517248
1262.655656	37426.848438	35.522266
1263.411763	37501.517212	35.527284
1264.813585	37584.546433	35.532301
1265.651316	37673.190443	35.537319
1267.225962	37765.880942	35.542336
1268.337145	37852.168749	35.547354
1269.840607	37929.846481	35.552372
1270.753372	38029.331398	35.557389
1271.635614	38130.946240	35.562407
1273.257261	38220.488585	35.567424
1274.165049	38325.230540	35.572442
1276.013818	38418.665319	35.577460
1277.188432	38528.741824	35.582477
1278.131394	38625.113553	35.587495
1279.532983	38720.440473	35.592512
1280.925019	38826.722043	35.597530
1282.034412	38920.621895	35.602548
1283.607827	39029.380449	35.607565
1284.780724	39129.652056	35.612583
1286.277885	39228.362250	35.617600
1287.809072	39325.290583	35.622618
1288.994636	39432.543211	35.627636
1290.458808	39525.890882	35.632653
1291.924321	39623.463170	35.637671
1293.596188	39718.733458	35.642688
1294.609740	39819.488394	35.647706
1295.987864	39903.055143	35.652724
1297.460491	39998.958462	35.657741
1298.797797	40106.127565	35.662759
1300.024817	40191.692074	35.667776
1301.212384	40291.220526	35.672794
1302.641916	40378.322646	35.677812
1304.328101	40477.407536	35.682829
1305.470583	40574.667579	35.687847
1306.717540	40660.022128	35.692864
1308.069581	40761.943012	35.697882
1309.542289	40847.977808	35.702900
1310.773123	40938.528245	35.707917
1311.831828	41038.649365	35.712935
1313.094452	41127.601890	35.717952
1314.651005	41233.597698	35.722970
1315.964924	41327.552023	35.727988
1317.208062	41424.553534	35.733005
1318.177364	41515.115447	35.738023
1319.767552	41617.167695	35.743040
1321.077379	41723.678625	35.748058
1322.034317	41828.682817	35.753076
1323.877277	41933.796264	35.758093
1324.575360	42026.483319	35.763111
1326.095711	42118.593723	35.768128
1326.899813	42224.705125	35.773146
1328.573619	42318.430590	35.778164
1330.312692	42435.250783	35.783181
1331.631582	42543.143086	35.788199
1332.713974	42633.559191	35.793216
1334.512111	42742.902168	35.798234
1335.303536	42845.615747	35.803252
1337.086635	42928.719916	35.808269
1338.189224	43032.587672	35.813287
1340.075649	43122.077361	35.818304
1341.466513	43219.114403	35.823322
1342.459801	43301.969739	35.828340
1344.022606	43386.476135	35.833357
1344.814391	43470.046573	35.838375
1346.227349	43547.922909	35.843392
1347.455073	43646.891083	35.848410
1348.766670	43729.160837	35.853428
1350.233512	43817.656026	35.858445
1351.386905	43913.012622	35.863463
1352.107689	44002.674662	35.868480
1353.647290	44106.637569	35.873498
1354.971592	44215.650445	35.878516
1355.806001	44313.898478	35.883533
1357.282128	44424.381526	35.888551
1358.325341	44536.216563	35.893568
1359.948211	44659.638688	35.898586
1361.431382	44756.098801	35.903604
1363.056550	44851.740218	35.908621
1364.306264	44970.206033	35.913639
1365.602546	45086.780213	35.918656
1367.196917	45189.436591	35.923674
1368.895255	45301.502426	35.928692
1370.460142	45400.350016	35.933709
1372.210033	45504.476487	35.938727
1373.558988	45607.046470	35.943744
1375.020732	45708.701113	35.948762
1376.350863	45814.532729	35.953780
1377.752779	45920.549770	35.958797
1378.585275	46036.600137	35.963815
1379.659663	46132.370718	35.968832
1381.487342	46238.171170	35.973850
1382.448529	46361.547533	35.978868
1384.305866	46470.488443	35.983885
1385.613558	46585.607351	35.988903
1386.745593	46694.845694	35.993920
1388.313398	46812.683416	35.998938
1389.861530	46932.447942	36.003956
1390.899987	47041.677227	36.008973
1392.274381	47169.814191	36.013991
1393.871449	47279.141135	36.019008
1395.080138	47396.139482	36.024026
1396.806182	47520.434303	36.029044
1398.376037	47629.172509	36.034061
1399.563606	47746.289826	36.039079
1400.979525	47868.116958	36.044096
1402.237169	47992.316463	36.049114
1404.261704	48112.436952	36.054132
1405.407934	48225.362444	36.059149
1407.125126	48340.002670	36.064167
1407.581319	48460.419721	36.069184
1409.194581	48575.925064	36.074202
1410.754227	48695.817322	36.079220
1412.353436	48821.834529	36.084237
1414.194360	48937.496068	36.089255
1415.144309	49051.835414	36.094272
1416.992331	49167.990497	36.099290
1418.240686	49286.017319	36.104308
1419.588838	49389.129696	36.109325
1421.484743	49507.316268	36.114343
1422.611832	49620.422467	36.119360
1424.453274	49722.333391	36.124378
1426.096212	49828.704482	36.129396
1427.701554	49939.270332	36.134413
1429.147455	50035.992883	36.139431
1430.671567	50147.211399	36.144448
1432.228043	50250.118070	36.149466
1433.336453	50355.942103	36.154484
1434.608325	50461.159092	36.159501
1436.204212	50573.557985	36.164519
1437.130513	50670.844939	36.169536
1438.559009	50753.875027	36.174554
1440.074461	50855.443111	36.179572
1440.761194	50946.738733	36.184589
1442.362570	51056.443745	36.189607
1443.429622	51155.988635	36.194624
1444.672560	51253.772905	36.199642
1445.922901	51376.802367	36.204660
1447.634549	51492.496898	36.209677
1448.895229	51612.539500	36.214695
1449.785234	51739.062731	36.219712
1451.350616	51849.011217	36.224730
1452.738637	51978.330892	36.229748
1454.337325	52112.553950	36.234765
1455.903060	52233.064807	36.239783
1457.502504	52360.664249	36.244800
1458.949396	52472.646297	36.249818
1460.037649	52599.725492	36.254836
1462.166310	52734.976987	36.259853
1463.694218	52862.811782	36.264871
1465.099075	52989.211048	36.269888
1466.763296	53104.952623	36.274906
1468.171101	53235.402537	36.279924
1469.229939	53364.154681	36.284941
1470.890960	53492.396165	36.289959
1472.472487	53613.886186	36.294976
1474.405319	53735.910656	36.299994
1475.756458	53869.581187	36.305012
1477.644776	53991.999924	36.310029
1479.483093	54121.020906	36.315047
1480.834436	54244.454760	36.320064
1482.601412	54353.890067	36.325082
1483.824867	54481.249512	36.330100
1485.473580	54588.286965	36.335117
1487.029082	54714.273398	36.340135
1488.387054	54838.766142	36.345152
1490.119051	54954.999887	36.350170
1491.261324	55090.665289	36.355188
1492.640643	55199.652265	36.360205
1493.856517	55326.371953	36.365223
1495.505597	55452.657845	36.370240
1496.920502	55578.379656	36.375258
1498.110308	55708.630383	36.380276
1499.915664	55844.544958	36.385293
1501.384487	55977.474989	36.390311
1502.800431	56099.914885	36.395328
1504.606415	56223.035149	36.400346
1505.952831	56359.694932	36.405364
1507.628892	56495.532090	36.410381
1509.491591	56624.170538	36.415399
1510.535716	56756.550803	36.420416
1512.518788	56871.881481	36.425434
1514.501376	57000.281788	36.430452
1515.317263	57119.776153	36.435469
1517.111660	57251.232286	36.440487
1518.417599	57379.018449	36.445504
1520.272709	57502.371831	36.450522
1521.817002	57627.229889	36.455540
1523.159605	57746.784632	36.460557
1525.030636	57860.352728	36.465575
1527.027706	57978.996645	36.470592
1528.858866	58083.660671	36.475610
1529.961279	58205.628491	36.480628
1531.731750	58328.360044	36.485645
1532.891362	58439.332719	36.490663
1534.271950	58556.290600	36.495680
1536.024958	58678.279802	36.500698
1537.318537	58792.714340	36.505716
1538.642619	58900.429269	36.510733
1540.084101	59002.930018	36.515751
1541.135519	59116.758185	36.520768
1542.984560	59222.107936	36.525786
1543.939012	59337.800417	36.530804
1545.229615	59460.017435	36.535821
1546.618998	59578.947346	36.540839
1547.907718	59708.843579	36.545856
1549.578874	59824.217949	36.550874
1551.346003	59961.320055	36.555892
1552.741011	60089.334546	36.560909
1554.657517	60207.723423	36.565927
1555.854658	60347.726783	36.570944
1558.030334	60480.242491	36.575962
1559.292870	60609.248774	36.580980
1560.833778	60732.895388	36.585997
1562.436482	60867.369662	36.591015
1563.974489	61010.653247	36.596032
1565.605108	61131.135637	36.601050
1566.979817	61264.204359	36.606068
1567.902264	61412.276570	36.611085
1569.844777	61550.892135	36.616103
1571.772199	61703.360949	36.621120
1573.433189	61839.483612	36.626138
1575.008133	61973.689737	36.631156
1576.938093	62110.848153	36.636173
1578.188374	62253.848261	36.641191
1579.557835	62398.027056	36.646208
1581.595224	62533.234050	36.651226
1583.563844	62678.074522	36.656244
1585.184113	62816.576433	36.661261
1586.888008	62941.652077	36.666279
1588.249473	63074.378114	36.671296
1590.296684	63214.683261	36.676314
1591.669440	63351.587100	36.681332
1593.464424	63491.489934	36.686349
1595.070629	63622.959020	36.691367
1596.416636	63761.730452	36.696384
1598.278252	63902.017715	36.701402
1599.896661	64028.979656	36.706420
1601.581137	64162.136010	36.711437
1603.357118	64296.715899	36.716455
1605.078530	64443.092829	36.721472
1606.311666	64565.609977	36.726490
1608.047074	64706.883674	36.731508
1609.260840	64856.114917	36.736525
1611.325769	64989.438031	36.741543
1612.765372	65114.888571	36.746560
1614.950624	65246.345697	36.751578
1616.687377	65375.176323	36.756596
1618.286167	65501.616969	36.761613
1619.989238	65634.531328	36.766631
1621.882668	65767.233158	36.771648
1623.009194	65885.157974	36.776666
1624.954068	66021.892375	36.781684
1626.441778	66159.059545	36.786701
1627.795125	66283.168117	36.791719
1629.446810	66416.037600	36.796736
1630.919721	66543.661664	36.801754
1632.400727	66674.507737	36.806772
1634.141148	66814.418556	36.811789
1635.935766	66953.264371	36.816807
1637.597658	67086.977846	36.821824
1639.265962	67222.976670	36.826842
1640.796373	67358.567143	36.831860
1642.394178	67493.843934	36.836877
1644.310283	67606.632968	36.841895
1645.750104	67733.869259	36.846912
1647.469724	67858.308393	36.851930
1649.201058	67966.676670	36.856948
1650.339905	68093.467726	36.861965
1652.089553	68197.148710	36.866983
1653.647531	68326.940215	36.872000
1654.691700	68442.743236	36.877018
1656.187885	68572.906509	36.882036
1657.988354	68708.652047	36.887053
1659.300428	68832.146247	36.892071
1661.027709	68982.018262	36.897088
1662.992019	69117.715128	36.902106
1664.746139	69250.608718	36.907124
1666.189908	69385.773814	36.912141
1668.212764	69526.453302	36.917159
1669.268243	69675.395452	36.922176
1671.196316	69813.051874	36.927194
1673.143814	69950.256426	36.932212
1674.726840	70096.237778	36.937229
1676.574662	70238.911338	36.942247
1678.269969	70381.064849	36.947264
1679.522505	70526.935420	36.952282
1681.397055	70678.744654	36.957300
1682.960581	70822.915754	36.962317
1684.758736	70968.532900	36.967335
1686.316778	71120.710584	36.972352
1688.175015	71264.762264	36.977370
1690.507629	71407.512408	36.982388
1692.407834	71553.053601	36.987405
1694.525105	71685.630809	36.992423
1696.155574	71832.773336	36.997440
1697.683307	71968.597342	37.002458
1699.308169	72108.041857	37.007476
1700.866394	72242.418694	37.012493
1702.756810	72390.068487	37.017511
1704.698274	72527.046857	37.022528
1706.207405	72679.089194	37.027546
1707.891719	72811.422821	37.032564
1709.497503	72969.366610	37.037581
1711.268417	73113.062029	37.042599
1713.040140	73269.829201	37.047616
1714.417697	73410.117023	37.052634
1716.411476	73562.975612	37.057652
1717.832194	73713.986372	37.062669
1719.606989	73860.851736	37.067687
1721.689554	74016.878301	37.072704
1722.976564	74159.476740	37.077722
1725.472010	74311.514240	37.082740
1727.084164	74466.932672	37.087757
1728.810519	74603.068584	37.092775
1730.492125	74751.561989	37.097792
1732.117822	74889.032338	37.102810
1734.701253	75030.458318	37.107828
1736.443482	75167.316625	37.112845
1738.216676	75301.776792	37.117863
1740.090175	75442.606100	37.122880
1741.983525	75580.849010	37.127898
1743.497559	75721.089710	37.132916
1745.113503	75857.591175	37.137933
1746.953969	75990.460932	37.142951
1748.582979	76127.189733	37.147968
1749.924900	76276.745128	37.152986
1751.930912	76411.909292	37.158004
1752.892013	76560.410802	37.163021
1754.737390	76715.945256	37.168039
1756.260400	76865.602386	37.173056
1758.134086	77009.860052	37.178074
1760.057028	77149.208445	37.183092
1761.497022	77307.165552	37.188109
1763.062720	77437.526287	37.193127
1764.855214	77579.582749	37.198144
1766.091995	77729.656541	37.203162
1767.992847	77864.185558	37.208180
1769.557187	78012.892455	37.213197
1771.171581	78158.970073	37.218215
1773.122438	78314.763254	37.223232
1774.669232	78463.285302	37.228250
1776.957906	78598.542994	37.233268
1778.882624	78749.376739	37.238285
1780.308053	78902.683353	37.243303
1782.065228	79047.565307	37.248320
1783.630599	79207.376112	37.253338
1785.587065	79351.772577	37.258356
1787.325367	79518.107950	37.263373
1789.195135	79679.001621	37.268391
1791.144483	79835.589095	37.273408
1792.903871	79999.098919	37.278426
1794.831131	80151.637556	37.283444
1796.455271	80316.601895	37.288461
1798.476857	80469.887742	37.293479
1800.398299	80635.466494	37.298496
1801.722582	80796.451530	37.303514
1803.977700	80955.898988	37.308532
1806.035011	81120.699309	37.313549
1807.951152	81281.506335	37.318567
1809.877827	81439.829405	37.323584
1811.482080	81597.380023	37.328602
1813.692125	81752.746734	37.333620
1815.735117	81923.964887	37.338637
1817.392484	82067.687120	37.343655
1819.694832	82230.948107	37.348672
1821.337736	82392.019401	37.353690
1823.411178	82540.455883	37.358708
1825.232451	82695.520868	37.363725
1826.786460	82849.006512	37.368743
1829.011196	83003.807669	37.373760
1830.685041	83157.504398	37.378778
1832.722413	83311.854923	37.383796
1834.215586	83465.923541	37.388813
1835.997638	83627.601053	37.393831
1838.426031	83784.224668	37.398848
1839.940756	83950.494376	37.403866
1841.533676	84106.628928	37.408884
1843.436107	84262.779515	37.413901
1845.318100	84425.332949	37.418919
1847.070790	84577.783309	37.423936
1848.806281	84745.683175	37.428954
1851.055384	84915.240031	37.433972
1853.021286	85078.797797	37.438989
1855.189977	85231.972499	37.444007
1857.144346	85373.384355	37.449024
1859.231919	85532.718879	37.454042
1860.789110	85689.019647	37.459060
1862.610469	85834.699409	37.464077
1864.151148	85993.449998	37.469095
1866.138542	86145.783422	37.474112
1868.218161	86307.417023	37.479130
1869.833139	86458.302111	37.484148
1871.962990	86617.483961	37.489165
1873.572861	86769.587959	37.494183
1875.617771	86927.454169	37.499200
1877.854535	87083.048415	37.504218
1879.609299	87237.552671	37.509236
1881.283859	87390.270771	37.514253
1883.100287	87555.690560	37.519271
1885.007952	87709.096363	37.524288
1886.461807	87864.094288	37.529306
1888.373260	88006.539416	37.534324
1889.993199	88155.176787	37.539341
1891.580826	88301.589560	37.544359
1893.442741	88433.184041	37.549376
1895.201815	88590.571439	37.554394
1896.885652	88752.622302	37.559412
1898.361774	88907.280080	37.564429
1900.323162	89066.590146	37.569447
1902.259636	89223.991322	37.574464
1903.848605	89389.063933	37.579482
1906.015886	89559.572944	37.584500
1908.156097	89719.543033	37.589517
1909.704381	89888.414037	37.594535
1911.714138	90063.842341	37.599552
1913.652759	90237.457773	37.604570
1915.631550	90415.351606	37.609588
1917.715439	90585.043006	37.614605
1919.880093	90757.232180	37.619623
1921.676946	90936.640241	37.624640
1923.561741	91106.771137	37.629658
1925.723648	91279.838226	37.634676
1927.903972	91461.863922	37.639693
1929.222332	91639.069327	37.644711
1931.409840	91802.490501	37.649728
1933.540397	91984.489070	37.654746
1935.795721	92158.243733	37.659764
1937.668204	92336.875213	37.664781
1939.737201	92523.449351	37.669799
1941.826991	92681.858740	37.674816
1943.727239	92870.248366	37.679834
1945.532554	93040.085627	37.684852
1947.661068	93224.322665	37.689869
1949.722304	93402.031110	37.694887
1952.157395	93572.267628	37.699904
1953.890495	93743.831136	37.704922
1955.788009	93915.484089	37.709940
1958.116303	94083.661371	37.714957
1959.559052	94266.300266	37.719975
1962.126914	94443.593661	37.724992
1963.804409	94619.505616	37.730010
1966.039927	94781.781802	37.735028
1968.290315	94956.237576	37.740045
1970.200285	95123.116685	37.745063
1971.917944	95300.851526	37.750080
1973.894153	95473.020580	37.755098
1976.010708	95641.226610	37.760116
1978.275015	95822.175027	37.765133
1979.906229	95999.420279	37.770151
1982.310445	96165.252015	37.775168
1984.100656	96337.099862	37.780186
1985.831294	96516.753678	37.785204
1988.134120	96685.646197	37.790221
1990.117120	96866.581054	37.795239
1991.964457	97030.082887	37.800256
1993.976315	97214.247690	37.805274
1996.006700	97381.690543	37.810292
1998.351695	97544.192214	37.815309
2000.072549	97726.402418	37.820327
2002.136478	97897.252763	37.825344
2004.460522	98065.540894	37.830362
2006.080570	98237.932648	37.835380
2007.960758	98396.479834	37.840397
2009.826122	98582.982567	37.845415
2011.491976	98756.244701	37.850432
2013.938654	98939.388400	37.855450
2015.358198	99111.866791	37.860468
2017.499711	99294.527581	37.865485
2019.619590	99472.147250	37.870503
2021.385339	99640.074193	37.875520
2023.398023	99808.090355	37.880538
2025.134913	99959.973954	37.885556
2027.229047	100127.510043	37.890573
2028.647859	100296.901603	37.895591
2030.694491	100455.027380	37.900608
2033.580370	100629.415526	37.905626
2034.906541	100791.610506	37.910644
2037.317048	100963.919223	37.915661
2039.736281	101139.561773	37.920679
2041.386569	101306.044705	37.925696
2043.914374	101480.974915	37.930714
2045.754936	101645.667727	37.935732
2047.689549	101832.584159	37.940749
2049.502834	102005.701307	37.945767
2051.515120	102185.026103	37.950784
2054.024541	102367.190525	37.955802
2056.039803	102548.862336	37.960820
2058.137152	102724.018319	37.965837
2059.965334	102922.811891	37.970855
2061.804688	103110.523806	37.975872
2063.793769	103301.104226	37.980890
2065.591389	103490.739274	37.985908
2067.896886	103673.880873	37.990925
2069.894474	103870.029245	37.995943
2072.013621	104066.235929	38.000960
2074.389190	104267.881213	38.005978
2076.439290	104467.537027	38.010996
2078.598256	104649.895331	38.016013
2080.905695	104853.215724	38.021031
2082.678573	105044.714629	38.026048
2085.222667	105233.051538	38.031066
2087.454212	105432.837011	38.036084
2089.660398	105623.789954	38.041101
2091.855398	105822.049192	38.046119
2093.721978	106013.361500	38.051136
2095.838683	106211.952199	38.056154
2097.804235	106417.034316	38.061172
2100.207604	106603.879178	38.066189
2102.365780	106800.006951	38.071207
2104.609617	107004.542096	38.076224
2106.757609	107202.563100	38.081242
2108.411392	107404.669117	38.086260
2110.982345	107602.157436	38.091277
2112.945365	107797.928212	38.096295
2115.362651	108005.257377	38.101312
2117.548616	108203.164117	38.106330
2119.315945	108399.095568	38.111348
2121.468370	108601.967927	38.116365
2123.776684	108799.808318	38.121383
2125.932095	108992.487180	38.126400
2127.923551	109178.344949	38.131418
2130.154947	109385.026538	38.136436
2132.630102	109588.932314	38.141453
2135.133791	109776.869330	38.146471
2137.178282	109963.116139	38.151488
2139.185449	110150.181346	38.156506
2141.161023	110346.040611	38.161524
2143.283971	110536.640622	38.166541
2145.585729	110743.788486	38.171559
2147.638467	110937.521229	38.176576
2149.987705	111129.737824	38.181594
2151.860565	111327.761711	38.186612
2154.258826	111510.601000	38.191629
2156.444050	111709.136397	38.196647
2158.664745	111892.081374	38.201664
2160.353232	112088.324685	38.206682
2162.408921	112271.284605	38.211700
2164.422113	112451.576160	38.216717
2166.258435	112626.607706	38.221735
2168.020710	112816.692698	38.226752
2169.934122	112994.453391	38.231770
2171.089452	113189.999405	38.236788
2173.863132	113382.491807	38.241805
2176.324981	113596.403704	38.246823
2178.514848	113791.766604	38.251840
2180.717922	113989.284542	38.256858
2182.646834	114190.739802	38.261876
2184.809713	114386.642774	38.266893
2186.970653	114589.928493	38.271911
2189.233023	114799.540996	38.276928
2191.328103	114990.321193	38.281946
2193.538896	115214.605585	38.286964
2195.823771	115413.932171	38.291981
2197.913732	115633.240785	38.296999
2200.205778	115847.281074	38.302016
2202.627757	116062.951213	38.307034
2204.717756	116274.552175	38.312052
2206.917589	116492.111159	38.317069
2209.117782	116714.186699	38.322087
2211.316178	116933.422714	38.327104
2213.388319	117156.294516	38.332122
2215.679135	117378.778468	38.337140
2218.256842	117609.666528	38.342157
2220.519882	117826.880986	38.347175
2222.611535	118046.368435	38.352192
2225.014444	118273.076687	38.357210
2227.129288	118505.919518	38.362228
2229.174316	118730.200116	38.367245
2231.782511	118967.027947	38.372263
2233.942775	119194.756165	38.377280
2236.472905	119430.952128	38.382298
2238.409128	119659.961065	38.387316
2241.180269	119884.503302	38.392333
2243.296113	120117.863206	38.397351
2245.730686	120343.132792	38.402368
2248.098969	120574.401248	38.407386
2249.969818	120804.721028	38.412404
2252.130765	121033.221133	38.417421
2254.994409	121265.063558	38.422439
2256.839354	121505.400033	38.427456
2259.403452	121727.422803	38.432474
2261.732889	121957.614616	38.437492
2263.966837	122185.184090	38.442509
2266.317263	122416.732666	38.447527
2268.312842	122659.044392	38.452544
2270.936337	122877.131922	38.457562
2273.103475	123121.817362	38.462580
2275.201764	123349.922102	38.467597
2277.411042	123582.615824	38.472615
2279.808539	123811.133335	38.477632
2282.587090	124057.048714	38.482650
2284.546313	124282.922343	38.487668
2286.493784	124517.209953	38.492685
2289.032430	124759.361154	38.497703
2291.396317	124998.318704	38.502720
2293.369396	125232.111727	38.507738
2295.471988	125487.934899	38.512756
2297.482880	125724.008430	38.517773
2300.040624	125963.702697	38.522791
2302.027085	126213.712701	38.527808
2304.596287	126451.365506	38.532826
2306.385633	126698.364342	38.537844
2308.558664	126951.521509	38.542861
2311.050730	127195.749733	38.547879
2313.116237	127442.253327	38.552896
2315.553698	127663.935335	38.557914
2317.572450	127911.083351	38.562932
2319.959567	128141.466442	38.567949
2322.351041	128364.060138	38.572967
2324.319364	128611.029846	38.577984
2326.655268	128841.094898	38.583002
2328.327618	129083.381041	38.588020
2330.448536	129333.160565	38.593037
2333.256364	129585.968516	38.598055
2335.188267	129843.735634	38.603072
2337.500827	130096.534898	38.608090
2339.391247	130352.598708	38.613108
2341.920244	130612.840517	38.618125
2344.697131	130878.133236	38.623143
2346.816458	131144.862184	38.628160
2349.205420	131400.385215	38.633178
2351.512145	131682.923197	38.638196
2353.691386	131953.225916	38.643213
2356.652741	132220.541016	38.648231
2358.430979	132498.954004	38.653248
2360.995751	132765.991584	38.658266
2363.770673	133047.006379	38.663284
2365.919692	133318.781462	38.668301
2368.699868	133590.295044	38.673319
2371.066653	133876.010074	38.678336
2373.556899	134141.925603	38.683354
2375.790918	134429.898127	38.688372
2378.327084	134710.059731	38.693389
2380.893202	134997.425913	38.698407
2383.200379	135279.390522	38.703424
2385.767327	135564.361926	38.708442
2387.958619	135844.216290	38.713460
2389.789579	136123.316330	38.718477
2392.749452	136417.622223	38.723495
2395.321444	136709.198647	38.728512
2397.510423	137002.549661	38.733530
2400.044019	137293.184048	38.738548
2402.836017	137575.772701	38.743565
2406.183769	137851.715855	38.748583
2408.379352	138140.327021	38.753600
2410.874404	138428.741093	38.758618
2413.183814	138709.990466	38.763636
2415.323868	138977.016646	38.768653
2417.828406	139271.297374	38.773671
2420.089883	139543.460184	38.778688
2422.813444	139825.933526	38.783706
2425.204793	140114.044133	38.788724
2427.793986	140397.607805	38.793741
2430.589899	140664.516069	38.798759
2432.888069	140955.311327	38.803776
2435.267522	141225.498317	38.808794
2437.821311	141504.860667	38.813812
2439.759841	141786.109826	38.818829
2442.357937	142070.430758	38.823847
2444.467744	142360.096201	38.828864
2446.951339	142642.940730	38.833882
2449.314166	142938.941260	38.838900
2451.633638	143240.801078	38.843917
2454.291261	143511.960084	38.848935
2456.717710	143809.834285	38.853952
2459.404345	144096.666102	38.858970
2461.997314	144370.137050	38.863988
2464.448687	144666.819472	38.869005
2466.708850	144950.498835	38.874023
2469.150372	145246.234318	38.879040
2471.380709	145528.665069	38.884058
2473.878801	145819.990964	38.889076
2476.411421	146113.724667	38.894093
2478.708480	146378.850315	38.899111
2480.708190	146645.457840	38.904128
2483.271806	146918.921718	38.909146
2485.479741	147182.440754	38.914164
2487.834057	147465.256347	38.919181
2490.257835	147737.730910	38.924199
2492.540264	148030.283273	38.929216
2494.978250	148312.976206	38.934234
2497.025747	148602.928238	38.939252
2499.227510	148902.910598	38.944269
2501.835316	149200.140566	38.949287
2504.262602	149504.470290	38.954304
2506.589753	149813.945334	38.959322
2508.847512	150120.742016	38.964340
2511.079754	150446.165373	38.969357
2513.639691	150769.343750	38.974375
2515.697632	151099.837398	38.979392
2518.463150	151430.070610	38.984410
2521.274751	151753.050637	38.989428
2523.612477	152095.895635	38.994445
2526.462480	152428.787351	38.999463
2529.464415	152761.746276	39.004480
2532.057171	153093.793441	39.009498
2534.832375	153416.814200	39.014516
2537.279737	153750.220734	39.019533
2539.836972	154077.772868	39.024551
2542.550453	154419.278812	39.029568
2545.076828	154754.151459	39.034586
2547.746156	155082.821701	39.039604
2550.514798	155421.583065	39.044621
2553.466180	155758.566143	39.049639
2556.247221	156088.278346	39.054656
2558.658576	156411.131402	39.059674
2561.518115	156745.036987	39.064692
2563.872855	157078.223253	39.069709
2566.548997	157408.505048	39.074727
2569.164752	157737.553976	39.079744
2572.000213	158073.171880	39.084762
2574.646584	158402.613233	39.089780
2577.290149	158739.470732	39.094797
2579.923174	159068.041819	39.099815
2582.347934	159401.052318	39.104832
2584.997957	159733.864529	39.109850
2588.277211	160055.205595	39.114868
2590.631409	160385.807583	39.119885
2592.977809	160728.600188	39.124903
2595.777384	161058.755563	39.129920
2598.225355	161392.509460	39.134938
2600.929812	161723.406763	39.139956
2603.287247	162055.642061	39.144973
2605.890482	162393.414291	39.149991
2608.580716	162736.519717	39.155008
2611.514845	163062.157490	39.160026
2617.945359	163298.253902	39.165044
2621.895665	163558.618378	39.170061
2625.116540	163821.268437	39.175079
2627.549324	164084.803959	39.180096
2630.110253	164344.143547	39.185114
2632.441627	164610.553585	39.190132
2634.482931	164865.608570	39.195149
2636.631987	165132.125240	39.200167
2638.610343	165390.175654	39.205184
2640.571026	165676.682506	39.210202
2643.293718	165953.232207	39.215220
2645.268041	166232.476890	39.220237
2647.258674	166533.710670	39.225255
2649.583745	166829.599220	39.230272
2651.389358	167118.980288	39.235290
2653.901430	167410.830061	39.240308
2655.602486	167699.785425	39.245325
2658.048853	168000.154741	39.250343
2660.176594	168295.102550	39.255360
2662.560684	168596.271298	39.260378
2665.229586	168919.515206	39.265396
2667.244966	169243.573311	39.270413
2669.448309	169575.501240	39.275431
2671.917104	169913.661794	39.280448
2674.290368	170261.031596	39.285466
2677.241810	170599.069417	39.290484
2679.661492	170963.754449	39.295501
2682.134324	171314.897528	39.300519
2684.729874	171683.164781	39.305536
2687.280644	172057.027728	39.310554
2690.147368	172422.818450	39.315572
2692.222059	172803.793635	39.320589
2695.018239	173190.397809	39.325607
2697.979474	173582.260515	39.330624
2700.111423	173978.850874	39.335642
2703.396055	174369.549774	39.340660
2705.960059	174757.302525	39.345677
2708.593762	175164.283881	39.350695
2711.575267	175555.886524	39.355712
2714.477522	175957.052428	39.360730
2717.444935	176357.092713	39.365748
2719.922574	176774.988798	39.370765
2723.306404	177171.590459	39.375783
2726.220093	177576.241779	39.380800
2728.750477	177994.592873	39.385818
2731.639756	178386.705734	39.390836
2734.307265	178792.645592	39.395853
2737.077590	179203.600024	39.400871
2740.372219	179611.096928	39.405888
2742.837958	180016.134151	39.410906
2745.901169	180421.308814	39.415924
2748.673524	180834.607073	39.420941
2751.724041	181245.425725	39.425959
2754.543439	181654.936090	39.430976
2757.523204	182049.717780	39.435994
2760.815502	182451.310035	39.441012
2763.202451	182862.797870	39.446029
2765.835312	183259.187918	39.451047
2769.359560	183656.507626	39.456064
2771.954402	184058.037390	39.461082
2774.762548	184455.116218	39.466100
2777.557496	184862.205862	39.471117
2780.498154	185267.445765	39.476135
2782.960659	185666.132544	39.481152
2785.638771	186074.845415	39.486170
2788.529672	186487.971676	39.491188
2790.967268	186913.285638	39.496205
2793.961738	187382.938409	39.501223
2796.646534	187786.399236	39.506240
2799.119763	188212.601844	39.511258
2802.299584	188629.069636	39.516276
2804.606268	189037.445316	39.521293
2807.314440	189461.203216	39.526311
2810.031532	189889.736545	39.531328
2813.222991	190304.964169	39.536346
2815.964323	190718.993328	39.541364
2818.720277	191144.604252	39.546381
2821.593877	191566.464538	39.551399
2824.588348	191986.808874	39.556416
2827.427877	192414.570371	39.561434
2829.864610	192830.483106	39.566452
2833.047695	193257.051035	39.571469
2835.792052	193658.668807	39.576487
2838.314912	194056.867786	39.581504
2841.160102	194452.909549	39.586522
2844.202518	194836.932494	39.591540
2847.211131	195229.699829	39.596557
2849.905564	195618.859429	39.601575
2852.403557	195994.333993	39.606592
2855.017775	196407.944423	39.611610
2858.184275	196809.556840	39.616628
2860.297248	197215.678018	39.621645
2863.114757	197624.383284	39.626663
2865.896614	198040.309335	39.631680
2868.514793	198461.977434	39.636698
2871.130952	198888.625800	39.641716
2874.271068	199319.258136	39.646733
2876.718361	199756.019763	39.651751
2879.698506	200188.533745	39.656768
2882.412664	200635.417097	39.661786
2885.729898	201080.734500	39.666804
2888.675646	201526.822178	39.671821
2891.281059	201971.185837	39.676839
2894.322473	202417.769013	39.681856
2896.750231	202868.106783	39.686874
2899.905259	203326.994777	39.691892
2903.186337	203795.796730	39.696909
2905.563926	204263.444929	39.701927
2908.962519	204723.771827	39.706944
2912.249767	205171.873004	39.711962
2915.178075	205629.379297	39.716980
2918.082834	206101.115909	39.721997
2921.132315	206561.044103	39.727015
2924.313325	207023.416915	39.732032
2927.189838	207493.814655	39.737050
2930.216434	207958.169493	39.742068
2933.142531	208422.388493	39.747085
2936.167766	208898.329265	39.752103
2939.358009	209362.686812	39.757120
2941.911785	209824.984989	39.762138
2944.870153	210304.825564	39.767156
2948.136426	210776.159764	39.772173
2950.912397	211252.321524	39.777191
2954.126620	211724.732385	39.782208
2956.826896	212212.796355	39.787226
2959.627513	212693.707098	39.792244
2963.148318	213162.236568	39.797261
2966.066193	213649.989484	39.802279
2968.477381	214130.124641	39.807296
2971.660086	214617.583682	39.812314
2974.538922	215105.598734	39.817332
2978.323590	215583.108704	39.822349
2981.143962	216071.997787	39.827367
2984.062276	216547.281144	39.832384
2987.110952	217033.493790	39.837402
2990.327853	217507.842551	39.842420
2993.345090	218001.606023	39.847437
2996.037919	218486.605277	39.852455
2999.581735	218961.641192	39.857472
3002.527959	219442.410162	39.862490
3005.311124	219920.537445	39.867508
3008.260331	220405.930167	39.872525
3010.836683	220902.177931	39.877543
3014.299860	221381.114854	39.882560
3016.935486	221872.654194	39.887578
3020.256755	222356.211807	39.892596
3023.513840	222825.070646	39.897613
3026.791384	223308.660826	39.902631
3029.859117	223787.634849	39.907648
3032.692820	224267.890203	39.912666
3035.614819	224730.450651	39.917684
3038.721606	225186.275715	39.922701
3041.482652	225644.618810	39.927719
3045.085560	226067.366782	39.932736
3048.276262	226504.938668	39.937754
3050.527176	226954.520477	39.942772
3053.852380	227400.124436	39.947789
3056.403740	227853.876431	39.952807
3059.131043	228314.256808	39.957824
3062.101815	228778.155735	39.962842
3064.667561	229254.565522	39.967860
3067.555109	229715.835032	39.972877
3070.185353	230196.197405	39.977895
3073.724811	230674.868394	39.982912
3076.731774	231170.998313	39.987930
3080.149187	231656.165722	39.992948
3082.715289	232140.169666	39.997965
3085.621337	232645.713703	40.002983
3089.091261	233139.890216	40.008000
3091.944799	233651.690902	40.013018
3095.359656	234144.249206	40.018036
3098.813150	234649.934792	40.023053
3101.991774	235148.168467	40.028071
3105.258518	235645.625745	40.033088
3108.352504	236160.561693	40.038106
3111.463593	236678.720578	40.043124
3114.686448	237185.277268	40.048141
3117.492521	237712.043197	40.053159
3120.609894	238226.616943	40.058176
3124.137439	238745.724098	40.063194
3126.897970	239268.353829	40.068212
3130.504168	239780.588048	40.073229
3133.325553	240304.984727	40.078247
3136.736955	240833.708801	40.083264
3139.812901	241362.306221	40.088282
3142.927614	241885.536447	40.093300
3146.482707	242418.096259	40.098317
3149.196071	242957.568548	40.103335
3151.988142	243492.531012	40.108352
3155.509448	244029.614222	40.113370
3158.638267	244558.145601	40.118388
3161.983018	245092.560976	40.123405
3165.026797	245648.106216	40.128423
3168.436015	246182.330941	40.133440
3171.771245	246730.054603	40.138458
3174.625255	247279.883822	40.143476
3178.012470	247816.774764	40.148493
3181.368246	248356.742745	40.153511
3184.612730	248909.249831	40.158528
3187.635150	249458.741460	40.163546
3190.961484	250010.165419	40.168564
3194.682693	250555.327990	40.173581
3197.874963	251090.257812	40.178599
3201.613952	251623.576659	40.183616
3205.122283	252151.087153	40.188634
3208.051422	252697.584950	40.193652
3211.423337	253221.963154	40.198669
3214.793565	253756.779852	40.203687
3217.591875	254291.632785	40.208704
3220.501591	254829.590763	40.213722
3223.926476	255367.466512	40.218740
3227.641317	255894.499499	40.223757
3230.244688	256440.017642	40.228775
3233.776346	256973.171180	40.233792
3236.974272	257514.604389	40.238810
3239.932213	258047.918988	40.243828
3242.725154	258582.095238	40.248845
3245.786954	259124.177755	40.253863
3249.277945	259661.923794	40.258880
3252.569174	260181.461019	40.263898
3255.113145	260709.214948	40.268916
3257.939793	261213.782932	40.273933
3261.035632	261727.374642	40.278951
3264.565417	262256.720674	40.283968
3267.600194	262789.265409	40.288986
3270.409599	263326.084394	40.294004
3273.588077	263857.255386	40.299021
3276.699796	264402.149838	40.304039
3279.811261	264951.130811	40.309056
3282.795648	265496.318785	40.314074
3285.591803	266069.649906	40.319092
3289.272242	266616.603104	40.324109
3292.478359	267195.654960	40.329127
3295.648630	267769.172092	40.334144
3298.991964	268351.192790	40.339162
3302.248488	268934.899748	40.344180
3306.064609	269516.128595	40.349197
3309.281441	270093.434194	40.354215
3312.684119	270680.637802	40.359232
3316.395303	271272.284991	40.364250
3319.926746	271858.571977	40.369268
3323.417641	272449.610688	40.374285
3327.186751	273039.662413	40.379303
3330.168064	273625.515209	40.384320
3333.458444	274212.103184	40.389338
3336.840101	274809.187070	40.394356
3340.224458	275403.599623	40.399373
3343.926372	276006.161450	40.404391
3347.102463	276606.261024	40.409408
3350.519645	277201.442585	40.414426
3354.045796	277807.395886	40.419444
3357.343297	278415.335534	40.424461
3360.362734	279022.374057	40.429479
3363.643118	279630.002040	40.434496
3367.364013	280244.184659	40.439514
3370.928374	280875.172466	40.444532
3374.209210	281477.046194	40.449549
3377.650150	282086.533726	40.454567
3381.452609	282704.162137	40.459584
3384.787981	283320.765975	40.464602
3387.894837	283930.315199	40.469620
3391.886346	284537.969320	40.474637
3395.586013	285145.282635	40.479655
3399.239734	285758.565062	40.484672
3402.815856	286357.659523	40.489690
3406.018070	286981.386727	40.494708
3409.275267	287593.495296	40.499725
3413.088058	288196.929240	40.504743
3415.951577	288807.208745	40.509760
3420.013525	289416.864348	40.514778
3422.980504	290024.754802	40.519796
3426.643086	290628.316281	40.524813
3429.982484	291241.062932	40.529831
3433.436080	291855.943977	40.534848
3437.123647	292464.714212	40.539866
3440.625570	293081.454343	40.544884
3444.274196	293689.253564	40.549901
3447.898952	294296.237880	40.554919
3451.359142	294908.141732	40.559936
3454.337642	295520.063412	40.564954
3458.162552	296119.304957	40.569972
3461.466892	296737.180256	40.574989
3465.338611	297334.396206	40.580007
3468.350506	297928.667756	40.585024
3471.806903	298540.203636	40.590042
3475.081122	299152.700519	40.595060
3478.584826	299745.921017	40.600064
3481.854819	300309.553078	40.605069
3484.846185	300841.128361	40.610074
3488.010359	301301.840690	40.615079
3490.948226	301730.465052	40.620084
3494.047624	302100.320209	40.625088
3496.614619	302435.515404	40.630093
3498.736096	302731.405752	40.635098
3501.071098	302970.888432	40.640103
3503.106219	303178.858225	40.645108
3504.503348	303337.400206	40.650112
3506.308698	303469.562641	40.655117
3507.480921	303563.469835	40.660122
3508.496872	303628.973353	40.665127
3509.786329	303680.283954	40.670132
3510.334062	303692.491286	40.675136
3511.793497	303683.789436	40.680141
3512.337548	303661.512402	40.685146
3513.156895	303613.615105	40.690151
3513.653342	303558.362004	40.695156
3514.339713	303472.080909	40.700160
3514.653512	303368.780509	40.705165
3514.985162	303271.636110	40.710170
3515.418743	303133.704141	40.715175
3515.260563	303017.725845	40.720180
3515.516065	302882.773186	40.725184
3515.517303	302743.584050	40.730189
3515.792885	302591.142965	40.735194
3515.819264	302433.064708	40.740199
3515.853528	302274.043075	40.745204
3515.881725	302114.945558	40.750208
3515.934515	301947.648530	40.755213
3515.694114	301775.484551	40.760218
3515.728824	301595.514613	40.765223
3515.668050	301419.020298	40.770228
3515.334090	301246.487417	40.775232
3515.191739	301063.972677	40.780237
3515.054558	300901.639533	40.785242
3514.919146	300728.794141	40.790247
3514.866620	300545.398329	40.795252
3514.666744	300364.570001	40.800256
3514.507308	300187.450746	40.805261
3514.056690	300006.685707	40.810266
3514.307771	299829.119635	40.815271
3513.659867	299674.930597	40.820276
3513.583017	299501.817704	40.825280
3513.604305	299322.529567	40.830285
3512.912048	299162.873781	40.835290
3512.974423	298992.104693	40.840295
3512.659606	298838.854139	40.845300
3512.316550	298672.321359	40.850304
3512.353224	298514.586486	40.855309
3512.102582	298367.280553	40.860314
3511.914974	298199.424095	40.865319
3511.539151	298059.187235	40.870324
3511.527616	297904.563392	40.875328
3511.448757	297745.062644	40.880333
3511.036446	297607.172009	40.885338
3511.158121	297472.150496	40.890343
3511.125346	297323.382573	40.895348
3510.656386	297188.045047	40.900352
3510.812211	297038.788877	40.905357
3510.222715	296907.338334	40.910362
3509.638120	296759.112972	40.915367
3509.217494	296635.246079	40.920372
3509.307112	296514.633923	40.925376
3509.204646	296391.887857	40.930381
3509.034979	296265.766663	40.935386
3509.102984	296154.371309	40.940391
3509.144405	296026.384085	40.945396
3508.559033	295908.497431	40.950400
3508.869073	295789.147605	40.955405
3508.880180	295679.058337	40.960410
3508.903813	295547.407479	40.965415
3508.756379	295450.069390	40.970420
3508.055095	295333.803210	40.975424
3508.291827	295220.674401	40.980429
3508.002057	295107.169132	40.985434
3507.931723	294998.643959	40.990439
3507.339599	294904.734110	40.995444
3507.299310	294795.414808	41.000448
3507.705479	294685.236748	41.005453
3507.102847	294589.673507	41.010458
3507.532989	294487.356726	41.015463
3507.127028	294393.468006	41.020468
3506.892607	294292.221570	41.025472
3507.189734	294196.950409	41.030477
3506.994515	294105.370250	41.035482
3506.747472	294003.208926	41.040487
3506.628064	293912.609402	41.045492
3506.385749	293819.305223	41.050496
3506.555251	293729.016829	41.055501
3506.092284	293650.612245	41.060506
3506.196063	293550.508296	41.065511
3506.291587	293465.169237	41.070516
3505.801370	293383.713972	41.075520
3506.263481	293298.546725	41.080525
3506.184276	293220.845509	41.085530
3506.079284	293130.191656	41.090535
3506.001610	293060.762843	41.095540
3505.788082	292976.158470	41.100544
3505.618717	292886.939749	41.105549
3505.369526	292819.599207	41.110554
3505.267476	292737.013557	41.115559
3505.003689	292665.729579	41.120564
3505.368256	292587.296664	41.125568
3505.209657	292516.657976	41.130573
3505.001237	292446.256057	41.135578
3504.954370	292373.639768	41.140583
3504.875033	292308.410470	41.145588
3505.003048	292238.312332	41.150592
3505.111839	292164.806093	41.155597
3504.616197	292105.546996	41.160602
3504.977355	292031.314032	41.165607
3505.166633	291965.126177	41.170612
3504.585700	291889.843240	41.175616
3505.018352	291828.708453	41.180621
3504.301187	291763.425099	41.185626
3504.583462	291696.102443	41.190631
3504.457137	291623.701278	41.195636
3504.609067	291563.322668	41.200640
3504.708305	291503.690411	41.205645
3504.168610	291436.622661	41.210650
3504.439650	291369.097753	41.215655
3504.055146	291306.434995	41.220660
3504.356604	291259.167946	41.225664
3504.219959	291190.840794	41.230669
3504.236700	291141.861517	41.235674
3504.396850	291074.633560	41.240679
3504.437655	291020.253821	41.245684
3504.166383	290959.584101	41.250688
3504.090938	290891.807126	41.255693
3504.066794	290839.142878	41.260698
3503.845258	290775.792375	41.265703
3503.980792	290723.790491	41.270708
3503.826882	290671.680870	41.275712
3504.139724	290612.981849	41.280717
3503.771450	290555.356091	41.285722
3503.960973	290496.523416	41.290727
3503.838747	290439.470209	41.295732
3503.599113	290395.748730	41.300736
3503.815139	290335.358962	41.305741
3503.918734	290285.321804	41.310746
3503.514532	290225.435744	41.315751
3503.505367	290186.413093	41.320756
3503.138291	290122.906389	41.325760
3503.394618	290071.725225	41.330765
3503.498507	290035.052312	41.335770
3503.362164	289988.794317	41.340775
3503.471186	289939.239709	41.345780
3503.542669	289895.876771	41.350784
3503.812360	289834.536295	41.355789
3503.440081	289782.307185	41.360794
3503.426068	289725.949272	41.365799
3503.414551	289671.576515	41.370804
3503.398467	289634.183807	41.375808
3503.548163	289576.527470	41.380813
3502.969883	289532.578075	41.385818
3503.363563	289493.568681	41.390823
3503.331598	289440.853576	41.395828
3503.084547	289395.401527	41.400832
3503.340845	289346.892713	41.405837
3503.511789	289302.546550	41.410842
3503.273529	289248.234174	41.415847
3503.501183	289197.718641	41.420852
3502.964940	289153.406053	41.425856
3503.228819	289101.942916	41.430861
3503.047386	289065.644783	41.435866
3503.012993	289022.144991	41.440871
3502.986333	288971.897965	41.445876
3503.052279	288939.608866	41.450880
3503.141833	288879.288318	41.455885
3502.994129	288843.544857	41.460890
3502.906179	288806.010111	41.465895
3502.999167	288755.387905	41.470900
3503.037443	288720.888271	41.475904
3503.459980	288668.636399	41.480909
3503.369948	288623.057545	41.485914
3503.247943	288576.898128	41.490919
3502.876259	288532.203112	41.495924
3502.822487	288481.247135	41.500928
3503.015307	288433.256650	41.505933
3503.065426	288403.846368	41.510938
3503.256357	288350.917491	41.515943
3503.126991	288301.169608	41.520948
3502.720604	288266.586187	41.525952
3502.979254	288226.451483	41.530957
3503.089505	288179.670135	41.535962
3503.228037	288126.901972	41.540967
3503.158517	288083.025163	41.545972
3502.644323	288046.065447	41.550976
3503.078447	287999.411770	41.555981
3502.896699	287964.615034	41.560986
3502.915036	287913.316452	41.565991
3502.990367	287873.591914	41.570996
3502.790148	287833.884774	41.576000
3502.722252	287788.505549	41.581005
3502.744828	287749.654686	41.586010
3502.573163	287712.132339	41.591015
3502.640545	287669.124949	41.596020
3502.285562	287632.012939	41.601024
3502.506026	287586.283217	41.606029
3502.326145	287559.963206	41.611034
3502.187844	287524.599418	41.616039
3502.494875	287480.129011	41.621044
3502.439586	287448.774501	41.626048
3502.726600	287407.718425	41.631053
3502.235026	287383.941654	41.636058
3502.279499	287339.664753	41.641063
3502.435892	287300.003628	41.646068
3502.032242	287276.518624	41.651072
3502.729321	287236.722408	41.656077
3502.493896	287202.900999	41.661082
3502.440074	287169.484088	41.666087
3502.651329	287136.942374	41.671092
3502.510498	287097.047349	41.676096
3502.506022	287059.982305	41.681101
3502.515757	287026.759090	41.686106
3502.544266	286986.506701	41.691111
3502.738503	286950.505341	41.696116
3502.353608	286904.334746	41.701120
3502.829547	286867.347581	41.706125
3502.577767	286825.254862	41.711130
3502.451102	286791.034458	41.716135
3502.598567	286747.428488	41.721140
3502.859006	286715.922672	41.726144
3502.590794	286676.174505	41.731149
3502.554184	286636.237528	41.736154
3502.522608	286587.975133	41.741159
3502.535475	286551.976325	41.746164
3502.469901	286520.266573	41.751168
3502.843923	286475.225005	41.756173
3502.539452	286437.366199	41.761178
3502.786857	286401.407186	41.766183
3502.559253	286366.769494	41.771188
3502.705649	286328.789551	41.776192
3502.673361	286278.464977	41.781197
3502.617312	286252.990740	41.786202
3502.499246	286199.828198	41.791207
3502.852152	286163.012537	41.796212
3502.570300	286134.849420	41.801216
3502.754280	286085.356610	41.806221
3502.356276	286041.860523	41.811226
3502.449507	286015.166453	41.816231
3502.447508	285974.892749	41.821236
3502.572215	285949.772137	41.826240
3502.386083	285897.587344	41.831245
3502.807258	285862.873893	41.836250
3502.737791	285822.381477	41.841255
3502.384195	285778.140033	41.846260
3502.246586	285745.753766	41.851264
3502.619621	285707.916413	41.856269
3502.482399	285669.521993	41.861274
3502.422952	285633.406660	41.866279
3502.545933	285589.065474	41.871284
3502.265174	285568.310203	41.876288
3502.604200	285520.014834	41.881293
3502.224408	285480.206953	41.886298
3502.188161	285451.750754	41.891303
3502.121531	285418.665922	41.896308
3501.850906	285395.083186	41.901312
3502.204517	285351.622445	41.906317
3502.292378	285329.562297	41.911322
3502.144795	285301.428857	41.916327
3502.329230	285271.079808	41.921332
3502.337959	285232.891554	41.926336
3502.562602	285186.650393	41.931341
3502.172901	285150.968068	41.936346
3501.999271	285115.633971	41.941351
3502.198950	285087.930110	41.946356
3501.994501	285044.479641	41.951360
3502.204074	285022.273164	41.956365
3502.317785	284992.113204	41.961370
3502.288938	284956.705580	41.966375
3502.473850	284927.145507	41.971380
3502.090237	284894.109749	41.976384
3502.474779	284847.207024	41.981389
3501.859086	284823.168625	41.986394
3501.778834	284789.423697	41.991399
3502.328587	284760.010444	41.996404
3502.169219	284724.928511	42.001408
3502.638387	284688.399464	42.006413
3502.617411	284659.049524	42.011418
3501.694742	284618.536417	42.016423
3502.116049	284588.786664	42.021428
3502.211832	284562.218923	42.026432
3502.241494	284524.892602	42.031437
3502.363820	284490.581380	42.036442
3502.265793	284453.147599	42.041447
3501.962019	284415.643981	42.046452
3501.897709	284392.741631	42.051456
3501.857297	284354.305955	42.056461
3502.103648	284321.324643	42.061466
3502.041394	284292.566514	42.066471
3502.236053	284256.589126	42.071476
3502.219526	284234.035705	42.076480
3502.007293	284193.946424	42.081485
3502.047467	284166.114265	42.086490
3502.096737	284132.297946	42.091495
3502.417895	284107.527969	42.096500
3501.962789	284077.965296	42.101504
3502.171446	284040.152610	42.106509
3502.141842	284001.027679	42.111514
3501.829297	283977.578276	42.116519
3502.474352	283936.311644	42.121524
3502.003385	283907.082328	42.126528
3502.276749	283865.415240	42.131533
3502.198805	283848.854010	42.136538
3502.036991	283814.306628	42.141543
3502.394496	283773.517442	42.146548
3501.850076	283748.194652	42.151552
3501.805823	283711.337654	42.156557
3502.294485	283679.413053	42.161562
3501.405947	283649.994024	42.166567
3502.256387	283615.619987	42.171572
3501.972387	283602.222174	42.176576
3502.092358	283558.669378	42.181581
3501.811965	283535.443952	42.186586
3502.031763	283507.609039	42.191591
3501.930640	283478.983918	42.196596
3501.930876	283456.911354	42.201600
3501.802966	283411.233052	42.206605
3502.026425	283388.285594	42.211610
3501.568686	283353.529449	42.216615
3502.269371	283330.049452	42.221620
3501.589081	283311.392377	42.226624
3501.674788	283271.841758	42.231629
3501.656333	283247.913549	42.236634
3501.764881	283215.869679	42.241639
3502.075118	283192.883195	42.246644
3501.897099	283166.332075	42.251648
3501.997089	283136.580793	42.256653
3501.750234	283103.828413	42.261658
3502.236321	283076.181023	42.266663
3502.349618	283041.615912	42.271668
3502.043933	283010.552928	42.276672
3501.770172	282984.525816	42.281677
3501.644751	282953.052872	42.286682
3501.348070	282925.781821	42.291687
3501.583650	282900.388267	42.296692
3501.640335	282877.899397	42.301696
3501.716552	282855.585693	42.306701
3501.795156	282830.242001	42.311706
3501.565130	282795.221018	42.316711
3501.897827	282756.089939	42.321716
3501.659043	282738.586038	42.326720
3501.401157	282701.736301	42.331725
3501.685424	282688.835442	42.336730
3501.685699	282659.710493	42.341735
3501.966739	282634.080640	42.346740
3501.546479	282618.539832	42.351744
3501.654973	282582.244036	42.356749
3501.753942	282550.175899	42.361754
3501.513179	282524.423534	42.366759
3501.996264	282503.650325	42.371764
3501.888866	282477.113419	42.376768
3501.545942	282439.436632	42.381773
3501.764028	282413.281856	42.386778
3501.519987	282395.829608	42.391783
3501.916557	282377.182928	42.396788
3502.064703	282347.907547	42.401792
3501.961538	282307.672932	42.406797
3502.095578	282285.681021	42.411802
3501.760092	282251.439958	42.416807
3501.922015	282230.360220	42.421812
3501.580588	282201.899278	42.426816
3501.603573	282169.206317	42.431821
3501.619942	282140.155031	42.436826
3501.758403	282113.681569	42.441831
3501.397881	282085.045338	42.446836
3501.228494	282069.134404	42.451840
3501.397141	282038.964636	42.456845
3501.325156	282020.950880	42.461850
3501.638664	281991.420489	42.466855
3501.616180	281963.342628	42.471860
3501.852463	281951.365637	42.476864
3501.523846	281922.571621	42.481869
3501.839648	281889.323784	42.486874
3501.776930	281873.701718	42.491879
3501.498531	281848.235021	42.496884
3501.484491	281807.629830	42.501888
3501.700428	281793.619237	42.506893
3501.876892	281758.279903	42.511898
3501.538549	281738.474457	42.516903
3501.714386	281713.980859	42.521908
3501.511909	281686.643761	42.526912
3501.492035	281667.297923	42.531917
3501.825036	281631.043093	42.536922
3501.691936	281614.057119	42.541927
3501.817279	281573.710161	42.546932
3502.030604	281557.077617	42.551936
3501.758467	281526.059691	42.556941
3501.698471	281511.099068	42.561946
3501.497197	281479.611827	42.566951
3501.776897	281445.325571	42.571956
3501.744881	281426.719882	42.576960
3501.522072	281397.323628	42.581965
3501.433980	281372.285420	42.586970
3501.580802	281345.657622	42.591975
3501.897988	281315.744495	42.596980
3501.414264	281299.831388	42.601984
3501.474428	281264.280779	42.606989
3501.418088	281242.878288	42.611994
3501.332154	281222.244180	42.616999
3501.635652	281194.420810	42.622004
3501.470699	281167.026761	42.627008
3501.310761	281143.552683	42.632013
3501.460542	281126.700794	42.637018
3501.338590	281114.448438	42.642023
3501.858604	281086.082145	42.647028
3501.779659	281054.957579	42.652032
3501.532786	281030.962344	42.657037
3501.827351	280997.462813	42.662042
3501.410846	280980.520795	42.667047
3501.312344	280945.783969	42.672052
3501.568129	280922.703402	42.677056
3501.399503	280904.398895	42.682061
3501.682369	280880.346636	42.687066
3501.385499	280860.432661	42.692071
3501.922443	280829.594054	42.697076
3501.768631	280815.666272	42.702080
3501.571537	280787.156860	42.707085
3501.505934	280760.740125	42.712090
3501.758104	280734.426688	42.717095
3501.580913	280702.731690	42.722100
3501.483697	280672.399056	42.727104
3501.408072	280658.179022	42.732109
3501.679082	280632.550029	42.737114
3501.069493	280605.912374	42.742119
3501.492361	280580.005134	42.747124
3501.129018	280564.862386	42.752128
3501.455701	280533.394424	42.757133
3501.577236	280518.099834	42.762138
3501.234328	280501.324472	42.767143
3501.819519	280475.137339	42.772148
3501.653614	280443.542314	42.777152
3501.497368	280426.636049	42.782157
3501.701890	280390.986178	42.787162
3501.295623	280371.878347	42.792167
3501.635628	280336.436505	42.797172
3501.702501	280325.834982	42.802177
3501.865283	280297.804036	42.807181
3501.531756	280269.239277	42.812186
3501.517930	280241.286712	42.817191
3501.714284	280206.274519	42.822196
3501.527225	280193.446568	42.827201
3501.591679	280163.266787	42.832205
3501.419521	280139.819755	42.837210
3501.084875	280116.983576	42.842215
3501.355433	280097.490295	42.847220
3501.254945	280077.189112	42.852225
3501.077043	280053.895706	42.857229
3501.096349	280028.560273	42.862234
3501.393978	280015.962386	42.867239
3501.550152	279990.682022	42.872244
3501.653383	279963.169416	42.877249
3501.484992	279939.161617	42.882253
3501.650979	279907.336500	42.887258
3501.877806	279897.702962	42.892263
3501.647605	279866.525058	42.897268
3501.482044	279841.218330	42.902273
3501.527428	279817.788264	42.907277
3501.384362	279789.346444	42.912282
3501.253156	279774.676612	42.917287
3501.188399	279748.310308	42.922292
3501.265341	279731.520358	42.927297
3501.190508	279713.099124	42.932301
3501.131792	279686.859159	42.937306
3501.141128	279666.642616	42.942311
3501.310411	279645.662837	42.947316
3501.275881	279633.829455	42.952321
3501.355462	279602.170415	42.957325
3501.497751	279581.118439	42.962330
3501.454521	279560.528148	42.967335
3501.596915	279529.674025	42.972340
3501.717175	279512.571766	42.977345
3501.403833	279497.701082	42.982349
3501.343917	279462.524743	42.987354
3501.429340	279443.594764	42.992359
3501.334181	279421.357610	42.997364
3501.171147	279406.692660	43.002369
3501.260905	279377.348811	43.007373
3501.148541	279352.899286	43.012378
3500.926822	279333.533333	43.017383
3501.254967	279309.600827	43.022388
3501.635488	279293.400043	43.027393
3501.143435	279274.967247	43.032397
3501.487114	279248.740893	43.037402
3501.428064	279229.273220	43.042407
3501.198913	279204.714519	43.047412
3501.408805	279193.199476	43.052417
3501.293195	279175.242740	43.057421
3501.817761	279140.382662	43.062426
3501.516595	279123.829638	43.067431
3501.308542	279089.338144	43.072436
3501.687662	279075.938155	43.077441
3501.301941	279042.772757	43.082445
3501.453991	279018.765723	43.087450
3501.036731	279001.594233	43.092455
3501.234097	278969.789301	43.097460
3501.396518	278959.045417	43.102465
3501.388582	278932.389925	43.107469
3501.935680	278915.246571	43.112474
3501.310667	278888.941693	43.117479
3501.505459	278857.926384	43.122484
3501.549936	278838.926246	43.127489
3501.412700	278816.262639	43.132493
3501.471008	278799.246242	43.137498
3501.137723	278776.307607	43.142503
3501.526537	278741.773998	43.147508
3501.466548	278728.544120	43.152513
3501.525324	278702.743818	43.157517
3501.607183	278673.502771	43.162522
3501.552028	278656.707682	43.167527
3501.509091	278628.555372	43.172532
3501.391648	278600.312804	43.177537
3501.159407	278586.294975	43.182541
3501.486209	278566.792551	43.187546
3501.124249	278554.118841	43.192551
3501.080911	278521.536449	43.197556
3500.909833	278502.035104	43.202561
3501.057363	278490.555120	43.207565
3501.434430	278459.460365	43.212570
3501.185621	278448.933165	43.217575
3501.143926	278423.530312	43.222580
3500.938909	278405.638229	43.227585
3501.203374	278386.120000	43.232589
3501.451084	278371.340013	43.237594
3501.301930	278354.203040	43.242599
3501.216131	278328.068665	43.247604
3501.588815	278304.867270	43.252609
3501.256459	278283.557813	43.257613
3501.494243	278261.599500	43.262618
3501.118799	278240.143974	43.267623
3501.240825	278218.636490	43.272628
3501.355295	278200.032671	43.277633
3501.432854	278183.751498	43.282637
3501.467364	278149.807429	43.287642
3501.348937	278140.100095	43.292647
3501.827553	278108.200122	43.297652
3501.276236	278091.456659	43.302657
3501.080933	278061.112787	43.307661
3501.596900	278042.573756	43.312666
3501.380547	278028.171445	43.317671
3501.700698	277999.300432	43.322676
3501.340712	277972.215643	43.327681
3501.498283	277950.244264	43.332685
3501.264665	277931.134416	43.337690
3500.999123	277917.452635	43.342695
3501.288683	277886.982324	43.347700
3501.535597	277872.049604	43.352705
3501.077513	277845.845697	43.357709
3501.531320	277819.092510	43.362714
3501.019156	277799.033011	43.367719
3501.229034	277784.055116	43.372724
3501.578143	277755.688719	43.377729
3501.153284	277732.789487	43.382733
3501.164265	277710.153414	43.387738
3501.050619	277703.093189	43.392743
3501.039838	277673.407891	43.397748
3501.395912	277663.372052	43.402753
3500.954380	277643.301522	43.407757
3501.129977	277623.644167	43.412762
3500.866327	277600.948956	43.417767
3501.005906	277586.185648	43.422772
3501.431945	277572.243425	43.427777
3501.023436	277541.932530	43.432781
3501.658353	277522.661966	43.437786
3501.204387	277503.917293	43.442791
3501.044276	277481.664228	43.447796
3501.103246	277463.323479	43.452801
3501.127037	277440.354346	43.457805
3501.251058	277417.471452	43.462810
3501.125677	277410.336644	43.467815
3501.123643	277377.110829	43.472820
3501.219390	277358.458804	43.477825
3501.490481	277351.847892	43.482829
3501.215466	277321.363375	43.487834
3501.199402	277305.733108	43.492839
3501.383827	277287.601942	43.497844
3501.683813	277260.694277	43.502849
3501.333630	277227.955410	43.507853
3501.236806	277216.895176	43.512858
3501.275109	277196.291570	43.517863
3501.339783	277166.543418	43.522868
3500.977563	277152.647401	43.527873
3501.196073	277134.358132	43.532877
3501.158480	277101.621491	43.537882
3500.989337	277095.690125	43.542887
3500.903681	277077.117183	43.547892
3501.131900	277059.462907	43.552897
3501.241370	277048.243244	43.557901
3501.168336	277023.608641	43.562906
3501.129670	277006.097727	43.567911
3501.351610	276993.154676	43.572916
3501.555774	276961.704323	43.577921
3500.820529	276944.861932	43.582925
3501.291804	276918.920472	43.587930
3501.104661	276900.159595	43.592935
3501.039726	276881.125087	43.597940
3501.181646	276857.322654	43.602945
3501.159653	276843.959241	43.607949
3501.084817	276824.671651	43.612954
3501.419234	276811.736528	43.617959
3501.133227	276780.566068	43.622964
3501.537203	276772.381312	43.627969
3501.212309	276743.126461	43.632973
3501.318470	276714.110052	43.637978
3501.333782	276708.099031	43.642983
3501.110788	276683.436736	43.647988
3501.349815	276672.069555	43.652993
3500.990954	276654.073710	43.657997
3501.086520	276624.447854	43.663002
3500.972241	276612.550041	43.668007
3500.810466	276587.521736	43.673012
3501.047412	276568.109184	43.678017
3501.120732	276542.866054	43.683021
3501.039904	276536.437144	43.688026
3501.355846	276517.725196	43.693031
3501.207965	276498.041517	43.698036
3501.408366	276479.347540	43.703041
3501.277426	276466.764849	43.708045
3501.187024	276429.784156	43.713050
3501.098927	276416.965641	43.718055
3501.459526	276392.645281	43.723060
3501.176367	276375.834264	43.728065
3500.735248	276348.837929	43.733069
3501.004171	276335.225472	43.738074
3501.156239	276323.388013	43.743079
3500.982934	276297.877652	43.748084
3500.985081	276275.471696	43.753089
3500.930881	276263.742709	43.758093
3501.502289	276246.798684	43.763098
3501.619225	276225.877058	43.768103
3501.249519	276198.182109	43.773108
3501.129336	276178.035743	43.778113
3501.118068	276169.380859	43.783117
3500.827539	276142.895706	43.788122
3500.851849	276128.481062	43.793127
3500.999616	276119.139435	43.798132
3501.364009	276087.230967	43.803137
3501.401313	276073.858199	43.808141
3501.567750	276049.848023	43.813146
3501.416691	276033.907519	43.818151
3501.421132	276011.271983	43.823156
3501.628847	275983.181573	43.828161
3501.193476	275953.408941	43.833165
3501.349188	275938.642819	43.838170
3501.172799	275921.916938	43.843175
3501.009981	275898.976402	43.848180
3501.289636	275870.874758	43.853185
3501.358036	275857.217042	43.858189
3501.017965	275829.542817	43.863194
3501.076136	275824.136132	43.868199
3501.084109	275810.131353	43.873204
3501.273069	275794.265198	43.878209
3501.214325	275770.697360	43.883213
3501.439664	275743.979034	43.888218
3501.154193	275715.226900	43.893223
3501.061412	275701.314166	43.898228
3501.248688	275677.478866	43.903233
3501.346904	275671.327561	43.908237
3501.216618	275637.382608	43.913242
3501.447144	275622.961246	43.918247
3500.956102	275602.515988	43.923252
3501.219168	275593.640125	43.928257
3501.096644	275571.202453	43.933261
3501.202091	275550.587977	43.938266
3501.152141	275529.488452	43.943271
3501.027923	275510.437385	43.948276
3500.826053	275482.766999	43.953281
3500.972675	275472.228793	43.958285
3501.104212	275460.470787	43.963290
3500.903344	275440.387717	43.968295
3500.839769	275428.227225	43.973300
3500.579268	275410.572257	43.978305
3500.899201	275403.928125	43.983309
3500.938459	275384.902514	43.988314
3500.704986	275373.354064	43.993319
3500.873504	275357.389160	43.998324
3501.019846	275343.922921	44.003329
3500.790954	275322.341959	44.008333
3500.902928	275308.728294	44.013338
3500.722898	275302.773028	44.018343
3500.812176	275275.260957	44.023348
3500.880298	275266.517240	44.028353
3500.746278	275253.120075	44.033357
3500.852951	275237.903153	44.038362
3500.590553	275224.042193	44.043367
3500.942101	275215.203443	44.048372
3500.548350	275186.773511	44.053377
3500.802864	275181.921843	44.058381
3500.861713	275158.590145	44.063386
3500.765661	275140.756760	44.068391
3500.897127	275141.347529	44.073396
3500.843749	275115.767213	44.078401
3500.822584	275100.748389	44.083405
3501.076183	275080.288972	44.088410
3500.811961	275065.715348	44.093415
3501.058825	275055.237875	44.098420
3501.160129	275037.679294	44.103425
3501.053896	275020.153005	44.108429
3501.165664	274992.128110	44.113434
3500.870313	274990.111839	44.118439
3500.820031	274976.650676	44.123444
3500.860481	274943.035329	44.128449
3500.891861	274937.148985	44.133453
3501.016445	274914.010682	44.138458
3500.946444	274898.133729	44.143463
3501.006432	274891.708238	44.148468
3501.343648	274869.682603	44.153473
3501.205214	274855.522214	44.158477
3500.987534	274828.083223	44.163482
3500.688391	274812.725680	44.168487
3501.238919	274795.682759	44.173492
3501.543270	274770.504978	44.178497
3501.406162	274761.538528	44.183501
3501.180032	274741.408296	44.188506
3500.918318	274725.306527	44.193511
3500.669927	274701.742434	44.198516
3501.054950	274686.991328	44.203521
3500.937170	274678.607479	44.208525
3501.244960	274657.884909	44.213530
3501.329372	274628.769299	44.218535
3501.133813	274612.020673	44.223540
3501.209132	274586.267398	44.228545
3501.394748	274582.317573	44.233549
3501.054905	274553.318880	44.238554
3500.943637	274540.630986	44.243559
3500.911556	274521.285276	44.248564
3500.730695	274494.324216	44.253569
3501.104638	274490.396005	44.258573
3500.945866	274461.980183	44.263578
3500.999753	274452.933055	44.268583
3500.908888	274440.420202	44.273588
3501.408309	274421.831997	44.278593
3501.090901	274408.997928	44.283597
3500.696021	274380.211433	44.288602
3500.753422	274360.648068	44.293607
3500.857420	274350.778357	44.298612
3500.704008	274325.595291	44.303617
3500.716853	274328.878004	44.308621
3500.928490	274304.274668	44.313626
3501.429919	274280.797469	44.318631
3500.775837	274262.948886	44.323636
3501.394024	274250.096512	44.328641
3500.879108	274237.293152	44.333645
3501.129894	274211.996230	44.338650
3501.321243	274193.965149	44.343655
3500.942417	274168.817113	44.348660
3501.137143	274151.880353	44.353665
3501.091097	274136.050451	44.358669
3501.122516	274123.111134	44.363674
3501.450820	274108.445138	44.368679
3501.178551	274088.169158	44.373684
3501.467931	274054.565642	44.378689
3500.853286	274045.036881	44.383693
3500.995255	274024.620039	44.388698
3501.069851	274011.648524	44.393703
3501.042413	274003.072316	44.398708
3500.884835	273971.397031	44.403713
3500.822962	273965.423283	44.408717
3501.063719	273940.127841	44.413722
3501.075464	273926.427700	44.418727
3500.770320	273907.378960	44.423732
3501.213979	273891.320037	44.428737
3500.961768	273878.883132	44.433741
3501.314910	273845.931619	44.438746
3501.249386	273841.155137	44.443751
3501.198940	273821.048269	44.448756
3501.136094	273794.348701	44.453761
3500.808231	273772.782741	44.458765
3500.924905	273761.103195	44.463770
3501.278901	273741.264377	44.468775
3500.742285	273734.371475	44.473780
3501.268752	273716.619148	44.478785
3501.351384	273698.910422	44.483789
3501.157204	273673.300654	44.488794
3500.662881	273652.448038	44.493799
3501.093338	273641.865433	44.498804
3500.934599	273611.641524	44.503809
3501.050104	273610.146910	44.508813
3500.919603	273580.122290	44.513818
3501.179359	273567.401976	44.518823
3500.809986	273546.020651	44.523828
3500.811261	273523.614089	44.528833
3500.787247	273525.629471	44.533837
3501.108708	273501.976367	44.538842
3501.111228	273483.185199	44.543847
3501.181784	273473.931677	44.548852
3500.961552	273456.830194	44.553857
3500.570592	273448.106803	44.558861
3500.735572	273418.290766	44.563866
3500.629390	273407.638869	44.568871
3500.320357	273398.113402	44.573876
3500.944381	273390.148692	44.578881
3500.828184	273372.496301	44.583885
3501.237173	273354.278403	44.588890
3501.076759	273336.123645	44.593895
3500.869154	273328.644809	44.598900
3501.000641	273303.035176	44.603905
3500.574127	273288.690195	44.608909
3500.890587	273282.886684	44.613914
3500.979169	273268.970785	44.618919
3500.960258	273252.932800	44.623924
3501.298555	273225.253998	44.628929
3500.808764	273202.312680	44.633933
3500.981630	273204.679363	44.638938
3500.969307	273177.207879	44.643943
3500.652468	273161.496322	44.648948
3501.274367	273147.319177	44.653953
3501.010070	273136.386306	44.658957
3501.081560	273115.674670	44.663962
3500.865314	273087.114560	44.668967
3500.604097	273076.995988	44.673972
3501.083809	273066.431111	44.678977
3500.940619	273048.706468	44.683981
3500.866058	273034.102979	44.688986
3501.054342	273012.609281	44.693991
3500.836545	273001.974702	44.698996
3501.035212	272990.231368	44.704001
3500.916769	272971.840844	44.709005
3500.802855	272947.007693	44.714010
3500.806695	272924.702425	44.719015
3500.877471	272922.858289	44.724020
3500.655830	272898.983987	44.729025
3501.238705	272884.380017	44.734029
3500.831404	272870.846765	44.739034
3500.841484	272857.859652	44.744039
3500.755260	272837.809046	44.749044
3501.000549	272817.401301	44.754049
3500.829005	272810.171430	44.759053
3500.786737	272792.889349	44.764058
3500.613828	272784.030110	44.769063
3500.415647	272779.503372	44.774068
3500.707801	272754.301431	44.779073
3500.791125	272750.902146	44.784077
3500.325214	272728.160682	44.789082
3500.381158	272699.303466	44.794087
3500.186325	272702.032928	44.799092
3500.508949	272691.747072	44.804097
3500.464786	272696.566451	44.809101
3500.912240	272680.761334	44.814106
3501.011414	272666.589067	44.819111
3500.707390	272662.740811	44.824116
3500.854577	272649.324937	44.829121
3500.888756	272626.505626	44.834125
3500.947144	272610.200872	44.839130
3500.985721	272590.792805	44.844135
3500.746385	272577.895388	44.849140
3500.878595	272571.764030	44.854145
3500.645201	272556.574084	44.859149
3500.711395	272539.478772	44.864154
3500.899659	272526.743967	44.869159
3500.782405	272514.693259	44.874164
3500.684238	272496.732337	44.879169
3500.956372	272492.387019	44.884173
3500.922153	272473.830509	44.889178
3500.777766	272451.522723	44.894183
3501.042371	272446.542018	44.899188
3501.039232	272423.371990	44.904193
3500.820161	272415.283765	44.909197
3500.647114	272389.262930	44.914202
3500.931743	272375.621928	44.919207
3500.477704	272373.604826	44.924212
3500.729734	272337.969469	44.929217
3500.907711	272335.344770	44.934221
3500.922737	272324.673878	44.939226
3500.958832	272296.277938	44.944231
3501.104368	272290.526422	44.949236
3501.220311	272271.590029	44.954241
3500.893960	272253.104394	44.959245
3500.794341	272234.558010	44.964250
3500.722811	272213.893878	44.969255
3500.830723	272208.402834	44.974260
3501.164067	272190.629324	44.979265
3500.870186	272179.573624	44.984269
3500.725318	272169.564153	44.989274
3501.091872	272136.813602	44.994279
3500.781594	272141.114250	44.999284
3500.756287	272118.685999	45.004289
3500.918712	272102.695971	45.009293
3500.704161	272092.544561	45.014298
3501.157083	272074.523258	45.019303
3500.626195	272058.793885	45.024308
3500.764485	272038.759083	45.029313
3500.473039	272027.193737	45.034317
3500.730114	272014.600925	45.039322
3500.961599	272000.000563	45.044327
3500.457049	271987.398954	45.049332
3500.759471	271968.688102	45.054337
3500.797699	271973.520161	45.059341
3500.760450	271957.535716	45.064346
3501.091620	271938.005587	45.069351
3501.001332	271925.212192	45.074356
3501.146710	271900.593020	45.079361
3500.749135	271888.534923	45.084365
3500.980229	271872.101306	45.089370
3501.015366	271851.726039	45.094375
3500.564587	271843.190032	45.099380
3501.092147	271816.270668	45.104385
3501.164782	271803.731990	45.109389
3500.747798	271789.512591	45.114394
3500.825111	271776.336619	45.119399
3500.910218	271769.372274	45.124404
3500.599816	271739.044002	45.129409
3500.840435	271725.358823	45.134413
3500.486307	271720.576210	45.139418
3501.024931	271710.765878	45.144423
3500.891697	271687.081188	45.149428
3500.788528	271683.481720	45.154433
3500.663798	271649.763477	45.159437
3501.044506	271634.044947	45.164442
3500.972412	271624.100477	45.169447
3500.860941	271611.819583	45.174452
3500.886284	271603.184000	45.179457
3500.650211	271588.121616	45.184461
3500.796410	271556.627341	45.189466
3501.003065	271551.579216	45.194471
3500.481820	271539.234766	45.199476
3500.874185	271516.766830	45.204481
3500.859353	271508.264802	45.209485
3500.656371	271502.007292	45.214490
3500.871873	271482.749688	45.219495
3501.000822	271475.294709	45.224500
3500.965180	271456.967370	45.229505
3501.281642	271452.029465	45.234509
3500.871063	271418.024602	45.239514
3500.551378	271398.417398	45.244519
3500.602670	271398.918819	45.249524
3500.697290	271384.263267	45.254529
3500.845263	271368.402669	45.259533
3500.554691	271353.348726	45.264538
3500.852204	271349.686893	45.269543
3500.765646	271336.409044	45.274548
3500.965443	271314.556664	45.279553
3501.044148	271299.470710	45.284557
3500.610728	271275.399760	45.289562
3501.041432	271259.087745	45.294567
3500.678785	271246.056546	45.299572
3500.890380	271227.639761	45.304577
3500.816461	271227.447714	45.309581
3500.991012	271206.388577	45.314586
3501.090638	271189.567891	45.319591
3500.723212	271180.866073	45.324596
3500.933216	271148.190445	45.329601
3500.836725	271143.444097	45.334605
3500.888115	271121.080048	45.339610
3501.317288	271103.469647	45.344615
3500.652491	271103.573249	45.349620
3501.008265	271075.814666	45.354625
3501.229372	271060.171797	45.359629
3501.150650	271036.452990	45.364634
3501.176122	271017.097544	45.369639
3501.013248	270999.502865	45.374644
3501.126132	270989.300376	45.379649
3500.903802	270962.446524	45.384653
3500.834690	270947.408976	45.389658
3500.654494	270940.918717	45.394663
3500.318337	270926.355588	45.399668
3500.576550	270909.739336	45.404673
3501.017934	270896.481118	45.409677
3500.816119	270887.015081	45.414682
3501.097875	270859.064248	45.419687
3500.678765	270863.050877	45.424692
3501.181290	270842.602649	45.429697
3500.782673	270825.655726	45.434701
3500.602981	270816.415405	45.439706
3501.045704	270794.372320	45.444711
3500.928181	270785.478799	45.449716
3500.807988	270768.845018	45.454721
3500.723964	270747.011204	45.459725
3500.914133	270736.567495	45.464730
3501.168411	270716.488885	45.469735
3500.709897	270706.859073	45.474740
3501.097300	270688.211119	45.479745
3500.930252	270668.503615	45.484749
3500.842061	270657.619421	45.489754
3501.066049	270630.110373	45.494759
3501.147648	270624.928881	45.499764
3501.051379	270592.708116	45.504769
3500.652428	270582.534304	45.509773
3500.659179	270574.461697	45.514778
3500.904117	270549.521108	45.519783
3500.587937	270545.572799	45.524788
3501.018694	270533.512935	45.529793
3500.914852	270520.797837	45.534797
3500.739348	270503.179564	45.539802
3501.179128	270486.153039	45.544807
3500.761619	270479.088567	45.549812
3500.531082	270459.059881	45.554817
3500.521396	270451.600929	45.559821
3500.471571	270429.379774	45.564826
3500.826340	270411.475264	45.569831
3500.311646	270415.680489	45.574836
3500.556381	270402.478263	45.579841
3500.354414	270371.521549	45.584845
3500.285884	270368.400432	45.589850
3500.867083	270359.754620	45.594855
3500.889406	270359.776760	45.599860
3501.156843	270333.432154	45.604865
3500.962787	270305.835285	45.609869
3500.904754	270251.201115	45.614874
3500.519868	270143.145653	45.619879
3500.138229	269992.846511	45.624884
3499.516714	269805.255679	45.629889
3499.330467	269586.786416	45.634893
3498.117847	269314.519959	45.639898
3497.727444	269005.635957	45.644903
3496.821984	268659.654645	45.649908
3495.639128	268270.351028	45.654913
3494.452627	267859.580640	45.659917
3493.177180	267407.876801	45.664922
3492.107709	266906.942806	45.669927
3490.639131	266389.033027	45.674932
3489.006079	265834.783505	45.679937
3487.726143	265252.643649	45.684941
3485.951973	264643.279642	45.689946
3484.243839	263998.658951	45.694951
3482.355580	263334.199961	45.699956
3480.746793	262619.120278	45.704961
3478.598182	261896.556879	45.709965
3476.309320	261148.545523	45.714970
3474.624836	260373.136436	45.719975
3472.135883	259578.188072	45.724980
3469.740267	258759.664204	45.729985
3467.571983	257918.944262	45.734989
3464.758874	257052.445628	45.739994
3462.419334	256165.570995	45.744999
3460.170143	255264.568084	45.750004
3457.372996	254347.218670	45.755009
3454.779946	253410.553322	45.760013
3451.842240	252457.203946	45.765018
3449.068522	251497.634623	45.770023
3446.132736	250507.524125	45.775028
3443.284136	249516.604626	45.780033
3440.604608	248504.922593	45.785037
3437.665610	247503.233058	45.790042
3434.409045	246456.917196	45.795047
3431.338414	245417.137553	45.800052
3428.420896	244361.487783	45.805057
3425.057033	243309.620729	45.810061
3422.251872	242239.528598	45.815066
3418.887545	241159.204179	45.820071
3415.472504	240078.475745	45.825076
3412.066438	238980.805243	45.830081
3408.696836	237872.224591	45.835085
3405.332439	236774.285385	45.840090
3402.148061	235660.677084	45.845095
3398.859229	234555.665014	45.850100
3395.525283	233429.467211	45.855105
3392.050882	232301.098542	45.860109
3388.511860	231168.790186	45.865114
3385.211154	230027.070437	45.870119
3381.621199	228895.836629	45.875124
3377.786447	227751.574292	45.880129
3374.298342	226617.368580	45.885133
3370.742545	225470.565927	45.890138
3367.475316	224327.080365	45.895143
3363.841488	223193.738038	45.900148
3360.469703	222033.103865	45.905153
3356.575392	220882.587002	45.910157
3352.723052	219738.916323	45.915162
3349.500436	218587.941861	45.920167
3345.755513	217439.725216	45.925172
3341.853709	216281.348137	45.930177
3338.634670	215129.744461	45.935181
3334.992991	213983.736684	45.940186
3331.038879	212813.738981	45.945191
3327.347829	211671.847307	45.950196
3323.528611	210529.470691	45.955201
3319.905929	209374.869053	45.960205
3316.044376	208226.906160	45.965210
3312.543433	207079.147470	45.970215
3308.961661	205931.178154	45.975220
3304.831360	204793.360322	45.980225
3301.706265	203646.071568	45.985229
3297.201383	202513.928529	45.990234
3293.993280	201376.166453	45.995239
3290.029961	200241.305517	46.000244
3286.292133	199106.799523	46.005249
3282.581304	197975.073577	46.010253
3278.469408	196842.654744	46.015258
3274.934698	195722.200700	46.020263
3271.460440	194598.563207	46.025268
3267.289332	193475.374825	46.030273
3263.839062	192362.423261	46.035277
3259.628258	191247.588394	46.040282
3256.085269	190125.326136	46.045287
3251.889473	189023.522871	46.050292
3248.058525	187910.622090	46.055297
3244.402300	186815.912596	46.060301
3240.342533	185720.386067	46.065306
3236.484375	184626.724239	46.070311
3232.777943	183551.079012	46.075316
3229.112199	182460.390619	46.080321
3225.318306	181377.144483	46.085325
3220.897658	180309.489907	46.090330
3217.369424	179243.797045	46.095335
3213.332636	178190.647179	46.100340
3209.431534	177129.239508	46.105345
3205.336351	176077.461659	46.110349
3201.418414	175043.988916	46.115354
3197.803231	174001.520132	46.120359
3193.879123	172978.119377	46.125364
3189.680195	171943.916197	46.130369
3186.035960	170922.612512	46.135373
3181.926058	169910.076935	46.140378
3178.048087	168894.349633	46.145383
3174.164835	167902.415896	46.150388
3170.257563	166908.208585	46.155393
3166.259652	165917.886496	46.160397
3161.888040	164944.006141	46.165402
3158.527992	163961.288863	46.170407
3154.180887	163006.665922	46.175412
3150.211969	162040.899125	46.180417
3146.152061	161084.096115	46.185421
3141.946438	160142.145482	46.190426
3138.248227	159199.468308	46.195431
3134.423982	158273.167276	46.200436
3129.936386	157348.320015	46.205441
3126.419258	156445.162973	46.210445
3122.274855	155534.863080	46.215450
3118.468896	154641.425786	46.220455
3114.365278	153752.604794	46.225460
3109.946223	152870.057245	46.230465
3106.195507	152011.102818	46.235469
3101.537689	151152.264706	46.240474
3097.476268	150292.061980	46.245479
3093.091980	149466.091076	46.250484
3088.797137	148638.935561	46.255489
3084.955005	147825.351091	46.260493
3080.503825	147044.144358	46.265498
3076.393038	146255.770603	46.270503
3072.398970	145485.574112	46.275508
3067.892651	144723.027253	46.280513
3063.594761	143961.426548	46.285517
3059.676160	143220.060394	46.290522
3055.345043	142498.325950	46.295527
3051.120330	141790.161621	46.300532
3046.863303	141085.053535	46.305537
3043.258121	140388.238919	46.310541
3038.688870	139704.243884	46.315546
3035.038281	139033.322059	46.320551
3030.747994	138362.407576	46.325556
3026.832073	137714.484868	46.330561
3023.460952	137065.252387	46.335565
3019.006825	136434.644669	46.340570
3015.124203	135761.490931	46.345575
3011.225773	135087.064764	46.350580
3007.331792	134473.482482	46.355585
3003.292442	133855.962185	46.360589
2999.481011	133258.501810	46.365594
2995.883554	132657.657887	46.370599
2992.000124	132075.782642	46.375604
2988.108647	131497.987059	46.380609
2984.586309	130923.003876	46.385613
2980.477256	130349.328126	46.390618
2977.112064	129777.744921	46.395623
2973.477702	129212.431389	46.400628
2969.552264	128644.181564	46.405633
2966.235644	128085.409893	46.410637
2962.325209	127531.800480	46.415642
2959.074880	126970.260625	46.420647
2954.973328	126431.373805	46.425652
2951.337259	125885.973100	46.430657
2948.018631	125329.248692	46.435661
2944.115363	124798.568962	46.440666
2940.923592	124248.351645	46.445671
2937.327903	123713.148748	46.450676
2933.551972	123167.323276	46.455681
2930.248027	122628.808283	46.460685
2926.598726	122091.689746	46.465690
2922.913195	121553.274280	46.470695
2919.523382	121021.687636	46.475700
2915.972564	120491.443197	46.480705
2912.462292	119953.264250	46.485709
2909.121299	119422.645773	46.490714
2905.326154	118902.456755	46.495719
2901.505574	118367.222381	46.500724
2898.082946	117837.706879	46.505729
2894.269372	117308.742867	46.510733
2890.732451	116794.239538	46.515738
2887.368308	116268.094115	46.520743
2883.825157	115744.577995	46.525748
2879.810720	115222.426892	46.530753
2876.506339	114707.522152	46.535757
2872.847675	114193.798714	46.540762
2869.304826	113673.694295	46.545767
2865.624359	113160.395721	46.550772
2861.463111	112648.425289	46.555777
2857.994990	112139.202314	46.560781
2854.149760	111644.730216	46.565786
2850.401372	111150.529617	46.570791
2847.003290	110655.454984	46.575796
2843.196818	110151.691095	46.580801
2839.408086	109674.299522	46.585805
2835.912775	109191.580035	46.590810
2831.954806	108718.385124	46.595815
2828.040251	108237.600235	46.600820
2824.136421	107778.101651	46.605825
2821.106122	107304.374905	46.610829
2816.732894	106845.508476	46.615834
2813.236141	106387.350826	46.620839
2809.454571	105937.646400	46.625844
2805.612804	105481.626733	46.630849
2801.891200	105040.009723	46.635853
2798.097790	104599.655423	46.640858
2794.424960	104166.775208	46.645863
2790.473752	103729.533092	46.650868
2786.982359	103311.126658	46.655873
2783.290206	102875.609602	46.660877
2779.540616	102462.147807	46.665882
2775.966262	102034.567791	46.670887
2772.403764	101629.450973	46.675892
2769.166825	101209.252155	46.680897
2765.407115	100787.907214	46.685901
2761.754590	100379.934713	46.690906
2758.462431	99971.504555	46.695911
2755.079739	99560.094159	46.700916
2751.293004	99149.908467	46.705921
2748.036187	98722.398926	46.710925
2744.479642	98322.902010	46.715930
2741.050819	97906.957419	46.720935
2737.885403	97487.215451	46.725940
2734.052541	97081.359166	46.730945
2730.932821	96665.128609	46.735949
2727.044898	96253.280415	46.740954
2724.155616	95833.250628	46.745959
2720.405015	95411.060367	46.750964
2716.599788	94988.833498	46.755969
2713.280848	94566.892510	46.760973
2710.094148	94150.680497	46.765978
2706.602529	93739.096198	46.770983
2703.210443	93313.549428	46.775988
2699.163169	92901.058968	46.780993
2695.889634	92467.932128	46.785997
2692.291381	92059.106279	46.791002
2688.838023	91641.978756	46.796007
2685.594870	91217.912036	46.801012
2682.238688	90791.632586	46.806017
2678.973628	90369.055133	46.811021
2675.151800	89945.185352	46.816026
2671.657425	89518.665979	46.821031
2668.117366	89096.810001	46.826036
2664.708331	88664.838969	46.831041
2661.369431	88234.248175	46.836045
2657.799940	87812.592947	46.841050
2654.301266	87385.749235	46.846055
2650.820502	86952.734566	46.851060
2647.025313	86534.867952	46.856065
2643.847001	86098.871483	46.861069
2640.037934	85672.571178	46.866074
2636.441819	85239.841323	46.871079
2633.241378	84820.674585	46.876084
2629.867644	84387.922908	46.881089
2626.901029	83953.615425	46.886093
2623.057368	83537.273304	46.891098
2619.675323	83090.251691	46.896103
2616.317152	82653.763836	46.901108
2612.527751	82213.526389	46.906113
2609.074436	81785.285182	46.911117
2605.439669	81345.951766	46.916122
2601.898803	80909.049355	46.921127
2598.638398	80464.273224	46.926132
2594.889653	80033.691436	46.931137
2591.732735	79601.779489	46.936141
2588.028253	79168.867191	46.941146
2584.593106	78719.929432	46.946151
2581.192329	78291.771821	46.951156
2577.224288	77845.674576	46.956161
2573.843996	77408.053059	46.961165
2570.762179	76978.951897	46.966170
2567.270483	76535.684802	46.971175
2563.363254	76090.470371	46.976180
2559.845546	75646.993253	46.981185
2556.504855	75209.324787	46.986189
2553.094643	74774.569618	46.991194
2549.517367	74319.135814	46.996199
2546.000941	73886.189405	47.001204
2542.650877	73444.322594	47.006209
2539.319743	72996.822205	47.011213
2535.503115	72565.048745	47.016218
2531.967721	72117.188667	47.021223
2528.685284	71673.321929	47.026228
2524.940969	71235.743527	47.031233
2521.661606	70779.029085	47.036237
2518.096077	70331.216847	47.041242
2514.412516	69890.978810	47.046247
2511.463937	69443.739699	47.051252
2507.703921	68993.555756	47.056257
2504.464801	68540.245211	47.061261
2500.725053	68101.855522	47.066266
2497.125615	67651.504988	47.071271
2493.909021	67200.353765	47.076276
2489.978519	66754.793187	47.081281
2486.562502	66289.787993	47.086285
2483.223479	65847.458266	47.091290
2479.854238	65399.752191	47.096295
2476.640374	64942.426726	47.101300
2472.363743	64493.697388	47.106305
2469.271223	64033.354757	47.111309
2465.684149	63585.924313	47.116314
2462.174771	63132.435111	47.121319
2459.105185	62682.509583	47.126324
2455.565478	62234.842181	47.131329
2452.065475	61765.580300	47.136333
2448.202355	61318.385984	47.141338
2444.792356	60858.468913	47.146343
2441.289613	60400.288288	47.151348
2437.642914	59953.478600	47.156353
2434.232424	59497.959421	47.161357
2430.704934	59040.664828	47.166362
2427.308724	58586.759580	47.171367
2423.561623	58127.511222	47.176372
2420.100662	57678.049460	47.181377
2416.698501	57209.976774	47.186381
2413.154564	56755.443715	47.191386
2409.464971	56297.509386	47.196391
2406.569413	55831.649907	47.201396
2402.460696	55388.416516	47.206401
2399.341216	54924.468620	47.211405
2395.603973	54478.263277	47.216410
2392.214320	54007.739199	47.221415
2388.942309	53546.576464	47.226420
2384.962316	53089.440858	47.231425
2381.752371	52622.754660	47.236429
2378.274930	52172.670229	47.241434
2374.935142	51705.787855	47.246439
2371.553801	51245.398027	47.251444
2367.863397	50778.138488	47.256449
2364.427133	50325.977461	47.261453
2360.890921	49861.427386	47.266458
2357.462278	49396.013653	47.271463
2354.046514	48921.873253	47.276468
2350.433281	48464.809964	47.281473
2346.913853	48002.762297	47.286477
2343.261572	47544.746786	47.291482
2339.642714	47067.270689	47.296487
2336.185839	46603.618143	47.301492
2332.644364	46142.854906	47.306497
2329.302056	45672.671344	47.311501
2325.755682	45223.698355	47.316506
2322.350523	44752.909680	47.321511
2319.053050	44278.803880	47.326516
2315.577647	43820.462568	47.331521
2312.151161	43342.858281	47.336525
2308.438509	42871.288522	47.341530
2304.689284	42401.503661	47.346535
2301.245615	41929.195637	47.351540
2297.595306	41466.409324	47.356545
2294.254992	40994.358954	47.361549
2290.869076	40529.566683	47.366554
2286.905103	40054.913612	47.371559
2283.624626	39586.637866	47.376564
2280.328378	39129.653645	47.381569
2276.525275	38655.652831	47.386573
2273.383465	38193.788955	47.391578
2269.588297	37716.764446	47.396583
2266.334094	37248.979079	47.401588
2262.532959	36785.041949	47.406593
2259.123539	36311.215439	47.411597
2255.736018	35849.174084	47.416602
2251.762323	35383.316519	47.421607
2248.663793	34908.946734	47.426612
2244.950711	34449.414300	47.431617
2241.406301	33976.307495	47.436621
2238.101553	33513.556309	47.441626
2234.369187	33044.055569	47.446631
2231.149202	32566.683398	47.451636
2227.174344	32103.757074	47.456641
2223.845592	31638.401822	47.461645
2220.417074	31177.331433	47.466650
2216.946914	30715.200390	47.471655
2213.418165	30239.127492	47.476660
2209.734923	29782.386558	47.481665
2206.414869	29303.292591	47.486669
2202.905003	28842.261666	47.491674
2199.287734	28371.803287	47.496679
2196.051498	27898.267502	47.501684
2192.317588	27443.063041	47.506689
2188.740066	26969.316822	47.511693
2185.381870	26505.324347	47.516698
2181.692912	26040.329517	47.521703
2178.393499	25560.369944	47.526708
2174.832852	25110.576516	47.531713
2171.707077	24630.916200	47.536717
2167.717518	24161.798346	47.541722
2164.348013	23700.830962	47.546727
2160.712278	23226.795435	47.551732
2157.114130	22768.666346	47.556737
2153.337142	22281.219671	47.561741
2149.773986	21825.273460	47.566746
2146.846736	21363.385613	47.571751
2142.898092	20893.173021	47.576756
2139.160975	20440.440459	47.581761
2135.560945	19966.122826	47.586765
2132.224732	19509.016806	47.591770
2128.611332	19055.213891	47.596775
2125.282412	18597.627700	47.601780
2121.856031	18134.183551	47.606785
2118.182718	17672.885258	47.611789
2114.443990	17214.404273	47.616794
2110.756866	16765.432152	47.621799
2107.358450	16302.876160	47.626804
2103.506694	15854.853341	47.631809
2099.638574	15402.483483	47.636813
2096.411608	14952.424555	47.641818
2092.391309	14510.329677	47.646823
2088.837729	14075.223359	47.651828
2084.361845	13643.341596	47.656833
2080.101143	13223.710656	47.661837
2076.337828	12815.488016	47.666842
2072.310026	12414.356180	47.671847
2068.598943	12011.493061	47.676852
2064.449723	11629.309166	47.681857
2060.842105	11235.807558	47.686861
2057.090454	10865.185757	47.691866
2053.130716	10489.314100	47.696871
2049.788161	10114.493512	47.701876
2045.427894	9746.650761	47.706881
2042.210858	9391.995041	47.711885
2038.254868	9027.420858	47.716890
2034.561244	8683.583097	47.721895
2031.407304	8330.340029	47.726900
2027.651011	7993.095696	47.731905
2024.080487	7643.215958	47.736909
2021.003444	7289.721289	47.741914
2016.996330	6955.139752	47.746919
2013.381501	6617.673877	47.751924
2009.690721	6273.003964	47.756929
2006.378242	5947.308065	47.761933
2002.983657	5611.123998	47.766938
1999.225560	5285.091516	47.771943
1996.015414	4949.375123	47.776948
1991.954888	4619.243388	47.781953
1988.721068	4287.419420	47.786957
1984.636932	3967.606667	47.791962
1981.226252	3644.049428	47.796967
1977.516201	3322.718431	47.801972
1973.689314	3019.308212	47.806977
1970.235630	2711.627167	47.811981
1966.490588	2402.727911	47.816986
1962.556127	2098.157082	47.821991
1958.177856	1814.830929	47.826996
1953.445706	1554.639173	47.832001
1948.778195	1305.125728	47.837005
1944.109697	1063.427557	47.842010
1939.556554	845.161965	47.847015
1935.587114	636.286978	47.852020
1931.153704	442.375377	47.857025
1926.827487	266.985581	47.862029
1922.757569	96.505678	47.867034
1915.456623	23.984676	47.872039
1906.042754	41.730387	47.877044
1899.450958	52.839195	47.882049
1895.780972	48.032232	47.887053
1892.948889	42.977806	47.892058
1890.023459	50.839496	47.897063
1887.866806	41.358328	47.902068
1884.948525	48.902534	47.907073
1881.979904	62.500422	47.912077
1879.617535	53.788409	47.917082
1876.576843	56.862372	47.922087
1873.102423	53.951671	47.927092
1869.213002	57.376025	47.932097
1865.548733	68.576531	47.937101
1862.394339	49.095148	47.942106
1858.949511	58.388581	47.947111
1856.176693	42.609467	47.952116
1852.825292	50.319159	47.957121
1849.030314	49.378721	47.962125
1846.418784	52.439674	47.967130
1842.497027	59.700309	47.972135
1839.583931	52.522994	47.977140
1835.802105	57.322634	47.982145
1832.079777	51.786682	47.987149
1828.452869	54.853811	47.992154
1825.289854	61.091538	47.997159
1822.055158	49.959029	48.002164
1818.384763	54.317390	48.007169
1814.774607	58.511355	48.012173
1811.663612	57.961167	48.017178
1808.153889	60.817073	48.022183
1804.720061	42.986365	48.027188
1801.150736	57.206077	48.032193
1797.315674	56.183298	48.037197
1794.544523	46.497228	48.042202
1791.097876	53.459294	48.047207
1787.705622	49.007746	48.052212
1784.008980	52.607742	48.057217
1780.403045	46.528509	48.062221
1777.093446	49.581055	48.067226
1773.643171	50.111880	48.072231
1770.067763	45.147848	48.077236
1766.583350	50.220735	48.082241
1763.241880	43.546696	48.087245
1759.792110	40.935889	48.092250
1756.047977	47.589921	48.097255
1752.867442	42.232246	48.102260
1749.244282	48.348602	48.107265
1745.668839	50.344722	48.112269
1742.313537	39.164567	48.117274
1738.381890	50.251655	48.122279
1735.554018	44.952986	48.127284
1731.831422	43.979149	48.132289
1728.697845	53.050134	48.137293
1725.192711	52.124707	48.142298
1721.149645	43.411719	48.147303
1717.910083	45.694079	48.152308
1714.710896	52.883383	48.157313
1710.912372	49.390405	48.162317
1707.290834	47.246091	48.167322
1703.927957	42.954496	48.172327
1700.694412	39.791195	48.177332
1697.062901	48.876403	48.182337
1693.927859	42.056353	48.187341
1690.220065	51.428677	48.192346
1686.396948	48.765256	48.197351
1683.324592	46.940422	48.202356
1679.567807	44.937382	48.207361
1675.812109	46.082054	48.212365
1672.294297	39.900541	48.217370
1668.449970	48.784759	48.222375
1664.981640	44.117282	48.227380
1661.842355	48.914998	48.232385
1658.437221	43.355014	48.237389
1655.171255	35.179142	48.242394
1651.266098	48.862665	48.247399
1648.431917	39.990011	48.252404
1644.867680	46.815360	48.257409
1641.119108	41.448036	48.262413
1637.918959	43.866633	48.267418
1634.241931	49.004306	48.272423
1630.783372	41.060887	48.277428
1627.647380	45.927692	48.282433
1623.653800	47.884499	48.287437
1620.291468	42.637393	48.292442
1616.289239	51.808777	48.297447
1613.556903	44.498960	48.302452
1610.061973	45.641015	48.307457
1606.084699	48.057185	48.312461
1603.063653	42.314045	48.317466
1599.062296	42.206171	48.322471
1595.411761	43.245899	48.327476
1592.332816	41.330353	48.332481
1588.700137	44.037733	48.337485
1585.739015	37.279215	48.342490
1581.858402	45.523688	48.347495
1578.730797	36.832755	48.352500
1574.614191	47.942303	48.357505
1571.096047	51.062121	48.362509
1567.674942	41.151391	48.367514
1564.089067	52.159354	48.372519
1560.512981	48.464099	48.377524
1557.241826	39.093170	48.382529
1553.991152	42.405472	48.387533
1550.296056	45.223808	48.392538
1546.783345	51.262873	48.397543
1543.353004	39.477514	48.402548
1540.211228	36.986471	48.407553
1536.462208	38.917875	48.412557
1533.125909	42.740205	48.417562
1529.090862	55.314509	48.422567
1526.022507	47.588776	48.427572
1522.231113	38.947384	48.432577
1518.511594	46.426482	48.437581
1515.243234	37.121565	48.442586
1511.303143	50.427718	48.447591
1507.865791	42.196285	48.452596
1505.140892	47.502138	48.457601
1501.416677	50.745782	48.462605
1497.983654	45.845047	48.467610
1494.487523	55.045229	48.472615
1491.038888	48.362599	48.477620
1487.440313	45.575671	48.482625
1483.636236	49.916894	48.487629
1480.625765	35.690265	48.492634
1476.548600	39.608929	48.497639
1473.445619	36.675265	48.502644
1469.668837	43.052820	48.507649
1466.205465	38.628205	48.512653
1463.113015	48.176832	48.517658
1458.852860	45.461244	48.522663
1456.074166	47.883857	48.527668
1452.767995	43.260771	48.532673
1448.690357	38.014297	48.537677
1445.563229	31.139274	48.542682
1441.758780	37.780558	48.547687
1438.246496	28.557917	48.552692
1434.685220	38.040309	48.557697
1431.241979	35.963188	48.562701
1428.068214	27.965990	48.567706
1424.518390	36.472183	48.572711
1420.933164	43.848125	48.577716
1417.632003	29.049840	48.582721
1413.667871	42.840610	48.587725
1410.036467	28.182313	48.592730
1406.657998	29.420151	48.597735
1403.421999	28.437051	48.602740
1400.129518	35.675678	48.607745
1396.527479	37.840476	48.612749
1392.839583	36.250684	48.617754
1389.093127	41.038515	48.622759
1385.321030	39.866782	48.627764
1382.270858	38.057509	48.632769
1379.088430	41.574330	48.637773
1375.292318	34.879371	48.642778
1371.648742	36.873470	48.647783
1368.431652	31.534195	48.652788
1365.211874	32.968795	48.657793
1361.547646	41.255522	48.662797
1358.046486	36.703930	48.667802
1353.910693	47.598174	48.672807
1350.034041	39.441475	48.677812
1347.118445	37.396128	48.682817
1343.890713	43.333897	48.687821
1340.670564	31.190008	48.692826
1336.891114	37.890680	48.697831
1333.436569	34.122758	48.702836
1329.778887	38.222909	48.707841
1326.354563	29.457986	48.712845
1322.738596	33.621245	48.717850
1319.098869	43.166472	48.722855
1315.748890	36.155314	48.727860
1312.313981	39.546926	48.732865
1308.806278	39.428685	48.737869
1305.478223	40.658685	48.742874
1301.967946	47.216227	48.747879
1298.525726	47.584493	48.752884
1294.500223	39.109295	48.757889
1290.961662	40.951018	48.762893
1288.007308	48.260407	48.767898
1284.118265	51.877731	48.772903
1280.999554	46.589587	48.777908
1277.501876	40.870062	48.782913
1273.704336	47.722250	48.787917
1270.027933	38.809912	48.792922
1266.581648	54.427789	48.797927
1262.800124	46.041164	48.802932
1259.740109	50.345680	48.807937
1256.146749	40.120143	48.812941
1252.904348	33.446584	48.817946
1249.097393	43.236137	48.822951
1245.790180	41.384632	48.827956
1242.507759	42.654991	48.832961
1238.568383	43.492945	48.837965
1235.526163	50.012436	48.842970
1231.540968	50.936615	48.847975
1228.484707	44.797218	48.852980
1225.201406	43.214071	48.857985
1221.131715	50.592668	48.862989
1218.023088	45.613006	48.867994
1214.031929	44.067277	48.872999
1210.837513	40.189278	48.878004
1207.208021	40.602522	48.883009
1203.512166	39.820732	48.888013
1200.403580	36.163489	48.893018
1196.556852	39.113022	48.898023
1193.146978	45.174061	48.903028
1189.677046	35.271005	48.908033
1185.822135	47.665411	48.913037
1182.779661	39.040385	48.918042
1179.237376	43.179532	48.923047
1176.063500	41.126951	48.928052
1172.522829	43.997210	48.933057
1168.598005	54.656150	48.938061
1165.092913	44.378925	48.943066
1161.535599	47.305558	48.948071
1158.299752	45.212006	48.953076
1154.537083	44.535532	48.958081
1151.171713	49.621560	48.963085
1147.896264	45.620144	48.968090
1144.119455	52.067326	48.973095
1141.080431	43.830900	48.978100
1137.109750	37.979386	48.983105
1133.509135	49.214267	48.988109
1129.934083	44.781773	48.993114
1126.718967	62.559265	48.998119
1122.693297	47.041758	49.003124
1119.626379	49.139106	49.008129
1115.965168	55.090581	49.013133
1112.820490	35.838844	49.018138
1109.006251	43.924312	49.023143
1105.657611	44.211594	49.028148
1102.194947	48.202316	49.033153
1098.878883	48.617404	49.038157
1095.183702	38.822191	49.043162
1091.942100	40.459524	49.048167
1088.030222	46.883441	49.053172
1084.517572	51.081258	49.058177
1080.888763	52.519443	49.063181
1077.594066	47.084720	49.068186
1074.284195	43.246857	49.073191
1070.628642	47.283425	49.078196
1067.028515	42.684005	49.083201
1063.564412	45.282934	49.088205
1060.315102	38.803464	49.093210
1056.550160	43.752382	49.098215
1053.019080	37.237682	49.103220
1049.660514	43.306560	49.108225
1045.912026	45.462550	49.113229
1042.856804	39.430587	49.118234
1038.977657	40.442683	49.123239
1035.318729	42.176619	49.128244
1032.206000	36.061864	49.133249
1028.547482	49.279896	49.138253
1025.443982	36.115024	49.143258
1021.857020	45.566629	49.148263
1018.075318	39.828084	49.153268
1014.682208	35.623547	49.158273
1010.727233	47.707673	49.163277
1007.459840	36.476016	49.168282
1003.937815	46.309810	49.173287
1000.369165	40.142644	49.178292
997.392432	36.116899	49.183297
993.891479	44.204225	49.188301
990.037631	38.277604	49.193306
986.085516	46.473125	49.198311
982.874139	43.281152	49.203316
979.743075	39.731838	49.208321
975.537410	48.681820	49.213325
972.172390	33.653135	49.218330
968.630891	40.620504	49.223335
965.202219	39.471295	49.228340
962.151887	29.996505	49.233345
958.779632	42.806150	49.238349
955.556211	35.734224	49.243354
951.841423	44.180698	49.248359
948.315809	42.480282	49.253364
944.393964	46.023651	49.258369
940.997942	44.116407	49.263373
937.382842	43.989616	49.268378
933.988025	36.036398	49.273383
930.447484	42.007063	49.278388
926.872593	35.882010	49.283393
923.273692	41.317607	49.288397
919.902111	25.679374	49.293402
916.598336	40.256342	49.298407
913.026011	34.659227	49.303412
909.510327	29.534176	49.308417
906.106983	39.153347	49.313421
902.531518	34.186295	49.318426
898.579639	34.178371	49.323431
895.402974	37.105884	49.328436
891.842449	38.796044	49.333441
888.199875	30.413181	49.338445
884.775536	32.398510	49.343450
881.400110	36.514869	49.348455
878.094004	35.507940	49.353460
874.516171	38.864889	49.358465
870.690394	38.638028	49.363469
867.423510	43.882744	49.368474
863.946305	39.144003	49.373479
860.388881	39.194901	49.378484
857.145773	37.675143	49.383489
853.384035	35.249052	49.388493
850.212247	36.318733	49.393498
846.823314	38.070770	49.398503
843.040611	39.672138	49.403508
839.241966	35.008750	49.408513
835.488196	36.684707	49.413517
832.176846	32.201722	49.418522
828.816647	38.191774	49.423527
825.811051	39.362134	49.428532
822.182697	40.667402	49.433537
818.132574	42.870372	49.438541
814.979406	36.648054	49.443546
811.209471	33.283635	49.448551
807.780625	40.692209	49.453556
804.520192	33.594436	49.458561
800.833738	46.272665	49.463565
796.930885	33.763777	49.468570
793.347958	39.902395	49.473575
790.281783	38.130482	49.478580
787.101099	36.854109	49.483585
783.407366	44.949311	49.488589
779.844146	40.334702	49.493594
776.484612	45.473628	49.498599
773.053495	41.417408	49.503604
769.611796	28.754487	49.508609
765.848787	33.905601	49.513613
762.674673	31.239357	49.518618
758.803438	44.734105	49.523623
755.154975	37.959328	49.528628
751.670500	29.972650	49.533633
748.236787	26.378738	49.538637
745.400682	35.261058	49.543642
741.538216	43.502747	49.548647
737.776783	30.010105	49.553652
734.309246	35.203809	49.558657
730.883355	44.734752	49.563661
727.134905	35.137732	49.568666
723.454779	35.236221	49.573671
719.774012	37.397523	49.578676
716.543425	31.554261	49.583681
713.139175	29.161126	49.588685
709.878938	27.583944	49.593690
706.376668	34.640130	49.598695
702.850993	32.091896	49.603700
699.206785	32.627710	49.608705
695.565473	42.125752	49.613709
692.432241	27.880450	49.618714
688.883301	33.235521	49.623719
684.953196	38.162725	49.628724
681.884112	31.810286	49.633729
677.842183	31.955613	49.638733
675.088095	22.187999	49.643738
671.595193	24.206168	49.648743
667.708744	29.559998	49.653748
664.362129	29.859670	49.658753
660.590774	35.714427	49.663757
657.343732	27.105528	49.668762
653.637743	30.808306	49.673767
649.950705	32.423278	49.678772
646.505459	29.856204	49.683777
642.947169	39.872819	49.688781
640.021284	38.556799	49.693786
636.339035	31.534214	49.698791
632.702703	35.321061	49.703796
629.086442	36.064499	49.708801
625.396008	44.314216	49.713805
622.221484	31.723628	49.718810
618.318545	33.106466	49.723815
615.013759	25.560066	49.728820
612.199238	28.611555	49.733825
608.422893	30.756112	49.738829
604.863640	29.893028	49.743834
601.094325	28.142018	49.748839
597.574757	26.598896	49.753844
594.257205	21.215273	49.758849
590.456670	20.218915	49.763853
587.091337	20.831550	49.768858
583.751435	19.896357	49.773863
580.359776	22.471398	49.778868
576.859191	16.790417	49.783873
573.265645	25.499595	49.788877
569.571439	20.399233	49.793882
565.883764	18.701958	49.798887
562.328747	23.795399	49.803892
559.087227	17.485649	49.808897
555.549393	26.695505	49.813901
552.210010	25.795036	49.818906
548.673105	29.743578	49.823911
545.209221	25.037621	49.828916
541.746886	19.290581	49.833921
537.957502	33.035168	49.838925
534.201525	19.418354	49.843930
530.867774	23.445998	49.848935
527.427152	30.622307	49.853940
524.492739	19.731222	49.858945
520.410896	23.691836	49.863949
517.454825	21.747799	49.868954
513.779076	18.346625	49.873959
510.201517	28.745879	49.878964
507.003538	22.767869	49.883969
502.828313	30.817822	49.888973
499.373812	21.206736	49.893978
496.027313	18.197220	49.898983
492.654662	19.288718	49.903988
489.107162	15.007067	49.908993
485.625171	24.356925	49.913997
481.978805	18.141851	49.919002
478.303831	19.245616	49.924007
474.663755	15.111254	49.929012
471.730924	19.174560	49.934017
468.321696	28.335928	49.939021
464.651673	21.555080	49.944026
461.256668	20.982812	49.949031
457.370292	21.834762	49.954036
453.863065	26.101385	49.959041
450.497380	23.515629	49.964045
446.652719	21.017097	49.969050
443.714453	21.117186	49.974055
440.025082	18.746335	49.979060
436.294052	19.542466	49.984065
432.886466	31.592004	49.989069
429.228617	32.278670	49.994074
425.618623	27.127258	49.999079
422.495418	31.938360	50.004084
419.026330	32.662078	50.009089
415.503001	29.079006	50.014093
412.193103	31.729921	50.019098
408.346307	29.643001	50.024103
404.794131	28.114475	50.029108
401.745016	25.362387	50.034113
397.934532	28.765094	50.039117
394.362905	23.376769	50.044122
390.817464	27.133672	50.049127
387.293054	25.657772	50.054132
384.203767	27.173390	50.059137
380.444908	28.027644	50.064141
377.011684	31.061582	50.069146
373.512694	31.397667	50.074151
370.216893	33.034020	50.079156
366.189192	26.789750	50.084161
362.687340	27.015554	50.089165
359.268753	33.805644	50.094170
355.757352	26.554044	50.099175
352.417525	26.928626	50.104180
349.320550	30.334149	50.109185
345.657995	28.547578	50.114189
341.886579	31.969519	50.119194
338.331958	21.235139	50.124199
334.522310	28.019673	50.129204
331.829602	25.743603	50.134209
327.926744	30.169907	50.139213
324.282379	32.717883	50.144218
320.761431	26.730077	50.149223
316.763210	26.438397	50.154228
313.640410	22.555713	50.159233
310.201636	16.520319	50.164237
306.745472	29.722666	50.169242
303.788765	13.855504	50.174247
300.072359	26.234687	50.179252
296.754277	23.432742	50.184257
292.784129	23.332843	50.189261
289.169281	35.098289	50.194266
286.264637	24.617055	50.199271
282.024662	23.806215	50.204276
278.786547	21.498009	50.209281
275.220543	30.266195	50.214285
271.866417	24.252427	50.219290
268.355995	17.133570	50.224295
264.844515	27.057491	50.229300
261.558140	19.745570	50.234305
258.011249	23.951952	50.239309
254.090793	30.506982	50.244314
250.858471	26.986197	50.249319
247.077345	26.056471	50.254324
243.961728	17.775200	50.259329
240.085571	19.944834	50.264333
237.031816	22.419851	50.269338
233.411429	17.314388	50.274343
229.709728	24.420637	50.279348
226.440873	21.437039	50.284353
222.682983	26.457698	50.289357
219.176299	34.447885	50.294362
215.639873	16.057820	50.299367
211.937232	21.436861	50.304372
208.685191	27.669537	50.309377
205.132496	29.336414	50.314381
201.555016	29.026703	50.319386
198.252017	16.804229	50.324391
194.973828	23.044139	50.329396
191.240333	19.307174	50.334401
187.202978	28.658098	50.339405
184.479611	23.397166	50.344410
181.377512	17.755454	50.349415
177.206931	21.252216	50.354420
173.707907	12.356797	50.359425
170.138169	17.237438	50.364429
166.490948	22.212399	50.369434
163.251765	12.618488	50.374439
159.419638	19.147117	50.379444
156.309811	20.979159	50.384449
152.834759	21.707005	50.389453
149.094941	19.170056	50.394458
146.095411	13.819257	50.399463
142.140991	22.100609	50.404468
138.883375	11.823061	50.409473
135.174108	21.391815	50.414477
131.541251	21.682339	50.419482
128.164755	15.456957	50.424487
124.322778	22.072543	50.429492
121.115322	22.891603	50.434497
117.479583	27.118161	50.439501
113.816945	20.124271	50.444506
110.251433	16.196658	50.449511
106.805966	27.783881	50.454516
103.830589	12.308809	50.459521
100.693525	16.831037	50.464525
96.940868	18.209532	50.469530
93.069253	20.840373	50.474535
89.585548	22.297214	50.479540
86.466836	19.723683	50.484545
82.796640	19.169006	50.489549
79.159987	23.243855	50.494554
75.867834	18.172737	50.499559
72.029533	18.454129	50.504564
68.277623	14.527073	50.509569
65.132549	14.586643	50.514573
61.242180	22.794758	50.519578
58.121776	8.671015	50.524583
54.388055	24.618334	50.529588
51.282852	19.097347	50.534593
47.712837	23.282043	50.539597
43.785009	21.628571	50.544602
40.761116	21.371893	50.549607
37.047170	19.438357	50.554612
33.644027	20.126551	50.559617
30.066428	30.924458	50.564621
26.896822	16.387611	50.569626
23.026391	15.617356	50.574631
19.745463	22.158253	50.579636
15.725432	24.824868	50.584641
12.431874	25.385275	50.589645
8.906920	28.936558	50.594650
6.002658	26.576413	50.599655
2.093891	30.064074	50.604660