Fri Aug 26 11:28:52 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.565211	105.699445	0.000000
0.369335	102.189903	0.005005
0.079984	89.855657	0.010010
-0.154192	88.408458	0.015014
0.319537	88.907416	0.020019
0.119424	79.735595	0.025024
-0.221599	80.143115	0.030029
-0.236816	76.020174	0.035034
-0.552089	73.766216	0.040038
-0.808320	59.237587	0.045043
-1.127145	60.018125	0.050048
-1.555657	55.700118	0.055053
-1.832348	47.824678	0.060058
-2.445120	47.258977	0.065062
-1.862576	42.169807	0.070067
-2.845949	42.557120	0.075072
-3.153139	33.781632	0.080077
-3.140673	34.482115	0.085082
-3.490218	28.383342	0.090086
-3.821687	18.048801	0.095091
-3.971568	26.655198	0.100096
-3.886655	20.400202	0.105101
-4.612343	18.210151	0.110106
-5.224909	20.248098	0.115110
-5.520494	15.045730	0.120115
-5.186752	8.479923	0.125120
-5.267228	11.931426	0.130125
-5.313220	17.098583	0.135130
-6.325065	24.345944	0.140134
-6.688511	9.435431	0.145139
-6.961681	17.023345	0.150144
-6.892144	7.891832	0.155149
-6.703947	9.039499	0.160154
-7.296536	13.760267	0.165158
-7.689697	1.309374	0.170163
-7.686569	4.621313	0.175168
-8.283556	9.576874	0.180173
-8.385396	7.783221	0.185178
-9.149373	7.025937	0.190182
-9.524708	1.339298	0.195187
-9.734564	8.461786	0.200192
-9.625364	9.530007	0.205197
-9.606865	0.520336	0.210202
-10.004978	8.478863	0.215206
-9.655624	12.439226	0.220211
-10.256735	4.449808	0.225216
-10.861569	11.836267	0.230221
-11.235351	4.121492	0.235226
-11.603089	13.021220	0.240230
-11.606005	13.856970	0.245235
-11.302035	5.128705	0.250240
-11.750852	18.118993	0.255245
-12.086413	11.929467	0.260250
-12.369981	15.482191	0.265254
-12.519674	8.947363	0.270259
-12.870148	8.812207	0.275264
-13.024982	5.704404	0.280269
-13.159281	11.432618	0.285274
-13.702073	12.981990	0.290278
-13.478755	1.703734	0.295283
-13.766815	13.817970	0.300288
-14.223163	10.396456	0.305293
-14.870050	7.248210	0.310298
-15.487300	12.295508	0.315302
-15.181713	11.030021	0.320307
-15.661681	8.165822	0.325312
-15.443475	9.033580	0.330317
-15.998080	8.306970	0.335322
-16.822770	17.663811	0.340326
-16.802114	0.055025	0.345331
-16.823329	9.859382	0.350336
-17.274138	11.653851	0.355341
-16.821092	11.029770	0.360346
-16.916655	10.396197	0.365350
-17.227817	-1.953568	0.370355
-17.939574	6.433428	0.375360
-17.788425	3.268494	0.380365
-18.316029	0.168113	0.385370
-19.569283	5.482106	0.390374
-19.344999	7.250556	0.395379
-19.261411	9.414221	0.400384
-19.810893	5.744627	0.405389
-19.315570	3.867489	0.410394
-19.899323	-2.795898	0.415398
-19.825422	-1.174872	0.420403
-20.306919	10.608824	0.425408
-20.966403	8.278759	0.430413
-21.116277	-0.236477	0.435418
-21.159472	13.693527	0.440422
-21.002930	2.520577	0.445427
-21.871518	2.269944	0.450432
-22.258510	-0.184801	0.455437
-22.328408	2.901235	0.460442
-22.514182	-5.557790	0.465446
-22.652966	-4.982451	0.470451
-22.608766	-0.503198	0.475456
-23.327252	-0.891091	0.480461
-23.819166	-5.737029	0.485466
-24.148069	1.998755	0.490470
-23.726840	-5.488633	0.495475
-23.893126	1.478376	0.500480
-24.396471	-6.845785	0.505485
-25.295187	3.076211	0.510490
-25.695183	2.442583	0.515494
-24.921203	-5.299036	0.520499
-25.292515	3.518988	0.525504
-25.497030	-4.076610	0.530509
-25.275331	-7.859945	0.535514
-26.360543	1.556432	0.540518
-26.763811	-7.947529	0.545523
-26.807596	-0.759158	0.550528
-26.876066	-1.811385	0.555533
-27.045399	-11.661805	0.560538
-27.721216	-2.268045	0.565542
-28.326374	-7.188095	0.570547
-28.247120	-0.430153	0.575552
-28.555837	-5.424833	0.580557
-28.734088	-1.078618	0.585562
-28.748118	3.140793	0.590566
-28.536837	9.476400	0.595571
-28.663471	5.677697	0.600576
-29.513543	6.800365	0.605581
-29.935562	-3.523225	0.610586
-30.028625	4.564967	0.615590
-30.140603	5.936535	0.620595
-30.414640	0.547326	0.625600
-30.866069	-2.564913	0.630605
-31.126495	-3.691654	0.635610
-31.530330	4.020997	0.640614
-31.636298	-2.985689	0.645619
-31.593665	3.768466	0.650624
-31.539247	2.798341	0.655629
-31.692248	-7.155860	0.660634
-32.575067	8.518322	0.665638
-32.609786	-4.352192	0.670643
-32.921406	6.326250	0.675648
-33.422185	5.126205	0.680653
-33.642624	-0.584548	0.685658
-34.168889	-1.135243	0.690662
-34.279894	-2.990740	0.695667
-34.441580	-5.420454	0.700672
-34.657934	6.185919	0.705677
-34.309487	-5.905887	0.710682
-34.733166	5.530294	0.715686
-34.960375	4.797000	0.720691
-35.156323	4.716876	0.725696
-35.777318	5.819696	0.730701
-35.805740	1.774757	0.735706
-36.676432	1.369434	0.740710
-36.835153	-2.490707	0.745715
-37.088489	5.562330	0.750720
-37.294919	8.675951	0.755725
-37.227288	-0.948786	0.760730
-37.518111	14.835701	0.765734
-37.250909	-7.813178	0.770739
-37.872265	2.163705	0.775744
-38.470498	13.440413	0.780749
-38.407388	1.079829	0.785754
-38.861195	5.760004	0.790758
-38.586978	-3.295806	0.795763
-39.168706	0.673485	0.800768
-40.142345	0.394918	0.805773
-39.775290	-1.177520	0.810778
-40.397775	11.074199	0.815782
-40.385174	2.078103	0.820787
-40.440334	0.754893	0.825792
-40.602530	11.346800	0.830797
-40.402557	4.510768	0.835802
-41.294147	8.895287	0.840806
-41.815925	-1.871498	0.845811
-41.535271	-0.896409	0.850816
-41.877417	7.901257	0.855821
-42.347567	2.026910	0.860826
-42.976360	2.067961	0.865830
-42.898663	-8.630812	0.870835
-42.928604	-5.997073	0.875840
-43.523517	-3.256386	0.880845
-43.253184	-4.342382	0.885850
-43.307607	-4.567923	0.890854
-44.068890	-2.937079	0.895859
-44.547424	-4.026696	0.900864
-44.754691	5.060005	0.905869
-44.702753	-3.591049	0.910874
-44.860096	1.799075	0.915878
-45.228437	-0.601628	0.920883
-45.964150	1.512437	0.925888
-46.354266	2.620436	0.930893
-46.254882	-1.346328	0.935898
-46.441378	1.963497	0.940902
-46.033651	6.180514	0.945907
-46.180333	1.815478	0.950912
-47.069472	5.206232	0.955917
-47.510986	11.039223	0.960922
-47.879631	12.681699	0.965926
-47.688876	2.208917	0.970931
-47.616075	4.080042	0.975936
-47.991898	4.448689	0.980941
-48.238366	-3.561139	0.985946
-48.893437	5.819902	0.990950
-48.936707	5.133897	0.995955
-49.300384	-4.009246	1.000960
-50.135408	7.886435	1.005965
-49.722273	-4.082570	1.010970
-50.609919	-2.786378	1.015974
-50.432801	2.017016	1.020979
-50.523564	4.454590	1.025984
-50.999199	6.806561	1.030989
-50.855175	2.421572	1.035994
-50.903006	12.359781	1.040998
-51.219013	-4.962467	1.046003
-51.988423	1.848519	1.051008
-51.985755	15.072215	1.056013
-52.045029	5.710835	1.061018
-52.557215	-1.697657	1.066022
-53.429478	4.404871	1.071027
-53.687224	3.119532	1.076032
-54.012188	5.220261	1.081037
-53.517838	-2.598039	1.086042
-53.584146	5.748569	1.091046
-53.871832	3.101199	1.096051
-53.902281	2.900397	1.101056
-54.393575	6.823972	1.106061
-54.886772	-2.574242	1.111066
-55.390290	3.961237	1.116070
-55.486129	-8.286009	1.121075
-55.248118	-7.288463	1.126080
-55.638832	11.542336	1.131085
-55.412948	6.170200	1.136090
-56.306560	3.177426	1.141094
-56.708319	-3.435203	1.146099
-56.778178	1.096608	1.151104
-57.075626	-0.005386	1.156109
-57.626349	1.165584	1.161114
-58.008986	2.566637	1.166118
-58.032223	-3.491181	1.171123
-58.238946	-5.739883	1.176128
-58.327478	1.876219	1.181133
-58.057765	-8.289323	1.186138
-58.469922	-4.378072	1.191142
-58.993830	4.413092	1.196147
-59.210094	-2.092383	1.201152
-59.733163	-5.253576	1.206157
-59.460227	-6.880960	1.211162
-59.942285	-0.630388	1.216166
-60.521281	-0.283889	1.221171
-60.768929	3.949749	1.226176
-60.811443	0.258169	1.231181
-60.862790	6.311973	1.236186
-61.190114	-0.119265	1.241190
-61.286169	-6.788981	1.246195
-61.536671	1.440775	1.251200
-62.331086	6.528310	1.256205
-62.250098	-0.491666	1.261210
-62.558543	9.284645	1.266214
-63.322056	-1.817810	1.271219
-63.647545	5.648532	1.276224
-63.363380	4.462308	1.281229
-63.731578	0.777147	1.286234
-63.901520	6.773488	1.291238
-63.737044	-0.635960	1.296243
-63.626510	-5.936350	1.301248
-64.324989	3.859558	1.306253
-64.975139	-1.844397	1.311258
-65.558150	-6.495820	1.316262
-65.231019	1.235889	1.321267
-65.325484	0.383855	1.326272
-65.880182	5.057593	1.331277
-66.373937	3.685618	1.336282
-66.812986	10.030733	1.341286
-67.521173	1.580284	1.346291
-66.928670	4.227838	1.351296
-67.223148	9.636151	1.356301
-67.365888	5.985485	1.361306
-67.586944	6.513526	1.366310
-67.460636	0.707658	1.371315
-67.370594	-3.441142	1.376320
-68.012841	10.186671	1.381325
-68.221158	0.440391	1.386330
-69.129740	2.454826	1.391334
-69.641703	4.970635	1.396339
-69.849571	1.823638	1.401344
-70.228406	1.237335	1.406349
-69.603416	-5.864176	1.411354
-70.146113	-2.258455	1.416358
-70.127088	0.304388	1.421363
-70.189257	-6.038422	1.426368
-70.865705	-0.858530	1.431373
-71.249726	1.650013	1.436378
-71.660271	2.609339	1.441382
-71.426917	0.247826	1.446387
-71.396622	0.610186	1.451392
-71.772187	3.553994	1.456397
-72.128616	5.482459	1.461402
-72.408623	2.305566	1.466406
-72.691241	-2.927284	1.471411
-72.776785	6.434681	1.476416
-73.661327	5.376644	1.481421
-73.933555	-1.148589	1.486426
-73.838273	0.491252	1.491430
-74.353496	6.126917	1.496435
-74.545946	6.198103	1.501440
-74.562091	7.586386	1.506445
-74.391733	5.525736	1.511450
-75.040780	1.966557	1.516454
-75.572884	11.610018	1.521459
-75.352286	-0.148681	1.526464
-75.903570	10.171621	1.531469
-75.716790	-0.113884	1.536474
-76.891051	4.909410	1.541478
-77.573602	8.211054	1.546483
-77.244828	6.622429	1.551488
-77.387567	5.553293	1.556493
-76.966771	5.766270	1.561498
-77.264688	8.663189	1.566502
-77.380733	9.662080	1.571507
-78.006618	4.118856	1.576512
-78.496086	6.014254	1.581517
-78.827010	-3.861624	1.586522
-79.054136	4.978239	1.591526
-79.563566	6.335763	1.596531
-79.440752	9.644884	1.601536
-79.613178	11.642773	1.606541
-79.459591	5.218911	1.611546
-80.306614	7.973544	1.616550
-80.968399	12.803157	1.621555
-80.871974	1.873683	1.626560
-80.724686	5.903466	1.631565
-80.665380	6.049344	1.636570
-80.783683	4.928949	1.641574
-81.447320	5.971973	1.646579
-81.590416	-1.013112	1.651584
-82.255964	7.711524	1.656589
-82.488452	5.874943	1.661594
-83.252703	-4.445974	1.666598
-83.594387	10.640931	1.671603
-83.099532	10.867686	1.676608
-83.652279	12.598936	1.681613
-83.490517	9.941696	1.686618
-83.514955	9.505850	1.691622
-83.710080	4.240393	1.696627
-84.555114	11.835085	1.701632
-84.961554	9.351733	1.706637
-84.713325	-2.025303	1.711642
-84.599393	2.553819	1.716646
-84.993517	5.199971	1.721651
-85.425487	1.752521	1.726656
-86.353876	14.213214	1.731661
-86.504589	3.736656	1.736666
-86.269514	-0.820690	1.741670
-86.514865	-3.683449	1.746675
-86.544596	-4.988471	1.751680
-87.396501	7.808308	1.756685
-87.471826	5.846021	1.761690
-87.669753	1.590202	1.766694
-88.043249	-3.501951	1.771699
-87.868749	1.757412	1.776704
-88.371707	8.523749	1.781709
-88.953956	-1.898270	1.786714
-89.343237	1.784802	1.791718
-89.788297	4.625539	1.796723
-89.540149	-6.814752	1.801728
-89.830772	2.193177	1.806733
-89.651470	-2.153011	1.811738
-89.824475	-2.511944	1.816742
-89.661679	-7.994470	1.821747
-90.420751	-7.740151	1.826752
-90.829766	2.766794	1.831757
-90.709202	2.529826	1.836762
-91.893824	-2.369599	1.841766
-92.197949	2.606796	1.846771
-92.261511	9.235119	1.851776
-92.141681	8.966629	1.856781
-92.358186	2.271374	1.861786
-92.466726	1.336113	1.866790
-92.433121	1.495485	1.871795
-93.074337	3.057018	1.876800
-93.677531	4.046340	1.881805
-94.266621	-11.499701	1.886810
-94.328020	2.578646	1.891814
-94.032646	1.469768	1.896819
-94.188575	-7.876552	1.901824
-94.280206	2.119085	1.906829
-94.571666	-1.315441	1.911834
-94.781746	-6.404565	1.916838
-95.372810	-0.548295	1.921843
-95.290024	2.083711	1.926848
-96.503398	8.717061	1.931853
-96.677723	-8.257090	1.936858
-97.004700	-7.870740	1.941862
-96.881833	-0.303374	1.946867
-96.666380	-5.889009	1.951872
-97.026687	-2.963396	1.956877
-96.817400	-3.922833	1.961882
-97.225870	-3.685139	1.966886
-98.370937	3.051464	1.971891
-98.152827	1.353525	1.976896
-98.232920	4.226019	1.981901
-98.265503	-2.611761	1.986906
-99.035097	6.125909	1.991910
-99.783003	2.854197	1.996915
-99.665864	5.808493	2.006912
-98.619544	2.690315	2.016909
-98.516095	0.466518	2.026906
-98.598321	5.398930	2.036902
-98.033334	-0.729633	2.046899
-97.067487	1.277369	2.056896
-96.914354	-1.600373	2.066893
-96.092778	1.607472	2.076890
-95.811558	-0.314565	2.086886
-95.121089	5.096231	2.096883
-94.806412	9.466352	2.106880
-94.511319	-1.441411	2.116877
-93.511942	2.780919	2.126874
-93.186638	3.373499	2.136870
-92.920784	-5.321830	2.146867
-92.037203	1.778952	2.156864
-91.606235	1.556822	2.166861
-91.139593	1.908824	2.176858
-90.388569	-2.392438	2.186854
-90.110364	6.446633	2.196851
-90.136556	5.950406	2.206848
-89.196555	-2.758027	2.216845
-88.789132	1.569142	2.226842
-87.711126	6.263888	2.236838
-87.499758	8.157122	2.246835
-87.687767	5.665103	2.256832
-86.830146	2.997608	2.266829
-85.980527	-0.058266	2.276826
-85.996045	1.784766	2.286822
-84.912123	2.823077	2.296819
-84.697564	-1.657576	2.306816
-84.408954	-2.785673	2.316813
-83.409677	0.350156	2.326810
-83.248544	-0.498342	2.336806
-82.977980	5.529012	2.346803
-82.297073	5.074738	2.356800
-81.553929	1.275196	2.366797
-80.650712	2.116737	2.376794
-80.568263	4.717433	2.386790
-80.656837	8.500964	2.396787
-79.482232	0.167801	2.406784
-79.198721	0.465958	2.416781
-78.726248	1.650155	2.426778
-78.025198	4.458632	2.436774
-77.934405	4.308474	2.446771
-77.144888	-5.165283	2.456768
-76.009563	5.935109	2.466765
-76.145099	-0.337798	2.476762
-75.926163	0.059108	2.486758
-75.014072	-2.642208	2.496755
-74.799673	-1.744101	2.506752
-74.304722	1.669817	2.516749
-73.263441	0.868005	2.526746
-73.175481	4.243927	2.536742
-73.011901	0.449096	2.546739
-71.961958	-0.940087	2.556736
-71.699493	8.240381	2.566733
-71.233486	12.102284	2.576730
-70.445912	10.643082	2.586726
-70.127648	7.707951	2.596723
-69.595452	3.117654	2.606720
-68.964063	4.460835	2.616717
-68.910038	8.820857	2.626714
-68.168043	6.564159	2.636710
-67.593191	12.506127	2.646707
-67.131075	10.235987	2.656704
-66.173812	3.460322	2.666701
-65.956840	7.164602	2.676698
-65.916862	9.604024	2.686694
-65.216335	6.907138	2.696691
-64.532311	6.775483	2.706688
-64.231795	14.914195	2.716685
-63.435758	10.951199	2.726682
-62.854313	12.742466	2.736678
-62.789382	12.444285	2.746675
-62.396486	7.777478	2.756672
-61.846042	3.824213	2.766669
-61.364581	4.484343	2.776666
-60.755072	3.116220	2.786662
-59.786413	11.990340	2.796659
-59.260488	8.636418	2.806656
-59.002082	12.033318	2.816653
-59.011956	9.766977	2.826650
-58.400996	10.441789	2.836646
-57.659188	8.641267	2.846643
-56.858795	11.028814	2.856640
-56.200708	4.299730	2.866637
-56.167075	5.283002	2.876634
-56.031075	8.648277	2.886630
-55.390989	9.195014	2.896627
-54.221930	5.186611	2.906624
-53.862571	8.022949	2.916621
-53.594527	5.022781	2.926618
-53.381857	11.356916	2.936614
-52.673089	8.136078	2.946611
-52.126967	10.309800	2.956608
-51.342766	8.033859	2.966605
-50.510590	7.803113	2.976602
-50.466280	9.947265	2.986598
-50.389136	7.746568	2.996595
-49.944281	7.275197	3.006592
-49.090302	6.116090	3.016589
-48.367480	8.053232	3.026586
-47.900379	10.698573	3.036582
-47.616380	9.897466	3.046579
-47.479955	8.352754	3.056576
-46.412536	10.242578	3.066573
-46.319665	10.469052	3.076570
-45.131318	8.519812	3.086566
-44.781722	10.115937	3.096563
-44.654646	6.044863	3.106560
-44.450081	8.667727	3.116557
-43.572452	8.075122	3.126554
-43.198401	8.368686	3.136550
-42.407903	9.867653	3.146547
-41.737388	8.613571	3.156544
-41.530122	8.629005	3.166541
-41.157224	11.450566	3.176538
-40.367168	14.923074	3.186534
-40.284341	14.229313	3.196531
-39.567597	10.376862	3.206528
-38.629863	7.338945	3.216525
-38.310550	13.130641	3.226522
-38.751836	14.051646	3.236518
-37.721650	14.597832	3.246515
-37.131505	13.080675	3.256512
-36.058880	11.751315	3.266509
-35.881634	12.420799	3.276506
-35.858017	11.356134	3.286502
-35.194210	5.766527	3.296499
-34.420444	7.559527	3.306496
-34.191827	16.352479	3.316493
-33.375390	11.293453	3.326490
-33.027535	9.981908	3.336486
-32.874737	8.947812	3.346483
-31.771663	13.670339	3.356480
-31.197183	13.714125	3.366477
-31.364413	9.435458	3.376474
-30.575992	7.681530	3.386470
-30.140000	12.805683	3.396467
-29.437243	10.197144	3.406464
-28.522087	3.950704	3.416461
-28.665416	9.763749	3.426458
-28.270893	10.773191	3.436454
-27.542288	12.665087	3.446451
-26.987871	12.974915	3.456448
-26.505513	8.154799	3.466445
-25.718454	8.092631	3.476442
-25.176655	11.990252	3.486438
-25.298367	11.021071	3.496435
-24.633363	7.613817	3.506432
-23.839892	10.826044	3.516429
-23.497104	7.244053	3.526426
-23.172569	3.072546	3.536422
-22.435558	-0.444116	3.546419
-21.962161	7.750039	3.556416
-21.280705	5.128980	3.566413
-20.423672	8.841308	3.576410
-20.429606	7.480314	3.586406
-20.482801	-0.360753	3.596403
-19.959915	0.647709	3.606400
-19.059680	3.745113	3.616397
-18.058287	7.191053	3.626394
-17.419272	9.274288	3.636390
-17.475721	9.010844	3.646387
-17.616054	7.315994	3.656384
-16.655423	3.517434	3.666381
-16.202619	4.673019	3.676378
-15.361394	7.234769	3.686374
-15.079494	12.658504	3.696371
-14.780053	7.448732	3.706368
-13.559875	9.780425	3.716365
-13.499979	12.080536	3.726362
-13.220130	10.459642	3.736358
-12.685068	11.817823	3.746355
-12.078756	10.934856	3.756352
-10.856871	10.101759	3.766349
-10.865421	18.475492	3.776346
-10.544364	11.437762	3.786342
-10.248329	8.978077	3.796339
-9.286838	0.744615	3.806336
-8.937211	0.050495	3.816333
-8.601878	1.781883	3.826330
-7.569555	9.100262	3.836326
-7.516640	6.494705	3.846323
-7.249506	14.020919	3.856320
-6.264338	9.505807	3.866317
-6.418752	7.217622	3.876314
-5.577511	10.048625	3.886310
-5.110003	20.451586	3.896307
-4.486876	22.014628	3.906304
-3.693777	27.209894	3.916301
-4.069063	28.725654	3.926298
-3.507808	43.589989	3.936294
-3.065803	58.900542	3.946291
-2.133585	68.106644	3.956288
-1.705366	81.186133	3.966285
-1.329389	87.441021	3.976282
-1.022753	96.836403	3.986278
-0.575872	119.349620	3.996275
0.000000	119.460474	4.001280
0.241028	134.909170	4.006285
0.496329	123.739748	4.011290
0.614195	131.048534	4.016294
0.455489	134.594497	4.021299
0.714722	132.270064	4.026304
0.688477	132.210972	4.031309
0.952744	139.310311	4.036314
0.607352	149.095618	4.041318
0.541746	149.150219	4.046323
0.903287	149.979850	4.051328
1.330501	161.046375	4.056333
0.924666	154.203369	4.061338
0.834551	145.014388	4.066342
0.988922	157.923519	4.071347
0.948075	148.730028	4.076352
0.844038	147.034777	4.081357
1.254541	148.685665	4.086362
0.868545	153.143355	4.091366
0.795030	142.240247	4.096371
1.247596	153.369257	4.101376
0.715802	156.830948	4.106381
1.256036	145.987298	4.111386
0.937346	158.058947	4.116390
1.063604	156.081073	4.121395
1.129739	149.259495	4.126400
0.855549	155.439794	4.131405
1.067131	156.526885	4.136410
1.541539	160.600685	4.141414
0.720217	159.219587	4.146419
1.131687	155.723037	4.151424
1.024103	154.268776	4.156429
1.523266	158.095119	4.161434
1.400773	158.614145	4.166438
1.042865	153.804243	4.171443
1.024277	142.500288	4.176448
1.091368	152.401703	4.181453
1.706349	154.640834	4.186458
1.267688	150.045981	4.191462
0.847157	143.037593	4.196467
1.165579	146.139122	4.201472
1.349650	161.125323	4.206477
1.412282	163.665583	4.211482
1.075381	152.183398	4.216486
0.901429	150.236448	4.221491
1.729015	153.514959	4.226496
1.120902	157.532683	4.231501
1.620152	159.046372	4.236506
1.784902	166.619948	4.241510
1.218345	152.642584	4.246515
1.312142	139.976573	4.251520
1.060198	149.215835	4.256525
1.336991	155.468532	4.261530
1.333137	162.033838	4.266534
0.801579	163.739657	4.271539
1.418541	159.872599	4.276544
1.198386	164.652475	4.281549
1.664882	170.840840	4.286554
1.598050	165.207353	4.291558
1.430509	168.428840	4.296563
1.761121	158.933906	4.301568
1.586035	171.460920	4.306573
1.579642	167.684587	4.311578
1.480334	166.384057	4.316582
1.252910	168.779659	4.321587
1.540793	166.561489	4.326592
1.356506	165.789868	4.331597
1.684198	166.849391	4.336602
1.395190	163.465065	4.341606
1.330117	160.738718	4.346611
1.516806	156.565340	4.351616
1.195992	169.456717	4.356621
1.511874	164.361576	4.361626
1.825569	160.212715	4.366630
1.580142	169.267479	4.371635
1.869209	158.042160	4.376640
1.379218	172.143092	4.381645
1.232010	170.897474	4.386650
1.632320	182.439589	4.391654
1.844859	190.182901	4.396659
2.091975	189.176436	4.401664
1.512966	179.965482	4.406669
1.997984	200.090119	4.411674
1.717870	200.766562	4.416678
2.094482	189.878760	4.421683
2.013160	179.808890	4.426688
1.533407	172.575599	4.431693
1.572652	173.695850	4.436698
1.954950	185.920961	4.441702
1.834412	191.738837	4.446707
2.456603	186.203704	4.451712
2.191470	175.336736	4.456717
2.489390	180.463049	4.461722
2.135402	169.736466	4.466726
1.765717	171.556284	4.471731
2.024651	171.547700	4.476736
1.714551	175.860705	4.481741
1.907393	165.808267	4.486746
2.076684	171.369044	4.491750
1.759578	169.988532	4.496755
2.086038	161.089014	4.501760
1.660623	174.553487	4.506765
1.946052	165.464208	4.511770
1.979558	176.563569	4.516774
1.995404	176.073991	4.521779
1.995428	175.311637	4.526784
1.980924	177.905037	4.531789
1.942540	169.138248	4.536794
1.832819	178.168725	4.541798
1.731725	187.507903	4.546803
2.054104	181.200059	4.551808
2.023070	197.788964	4.556813
2.044551	196.311441	4.561818
2.141679	192.405093	4.566822
2.046212	188.136437	4.571827
2.580892	185.193323	4.576832
1.843912	187.978304	4.581837
2.098939	200.280186	4.586842
2.259905	185.436568	4.591846
1.908151	197.874050	4.596851
2.281864	184.003358	4.601856
1.877186	194.762841	4.606861
2.188297	187.643684	4.611866
2.095483	185.136782	4.616870
1.747160	195.852691	4.621875
2.043021	196.316073	4.626880
1.918208	220.964828	4.631885
2.691931	214.811321	4.636890
2.567325	214.628341	4.641894
2.602847	218.482592	4.646899
2.528451	207.411906	4.651904
2.172589	204.718172	4.656909
2.464243	196.244824	4.661914
2.308586	199.473958	4.666918
2.341274	215.208256	4.671923
2.660698	213.314193	4.676928
2.271226	208.866686	4.681933
2.455857	217.164835	4.686938
2.647182	214.003099	4.691942
2.381487	211.542092	4.696947
2.459378	211.197874	4.701952
2.644072	225.152673	4.706957
2.600991	211.856205	4.711962
2.251263	202.891107	4.716966
2.556603	215.884340	4.721971
3.043955	209.712148	4.726976
2.357782	212.406966	4.731981
2.574482	204.976643	4.736986
2.474898	208.940512	4.741990
2.745224	217.848563	4.746995
2.905415	215.694560	4.752000
2.481021	209.335302	4.757005
2.487016	205.199537	4.762010
2.581169	212.600632	4.767014
2.633187	217.306508	4.772019
3.078286	201.393606	4.777024
2.285979	213.083463	4.782029
2.547760	215.519959	4.787034
2.990130	221.772209	4.792038
2.775199	219.527919	4.797043
2.763840	214.758954	4.802048
2.845397	223.361049	4.807053
2.937400	218.139403	4.812058
2.849694	206.700638	4.817062
2.478034	213.111264	4.822067
2.892020	206.944168	4.827072
2.372753	215.117799	4.832077
2.720097	221.856232	4.837082
2.863695	217.116923	4.842086
2.628158	217.957264	4.847091
2.886287	219.559118	4.852096
2.819088	224.938440	4.857101
3.006418	219.486821	4.862106
3.063811	213.871941	4.867110
2.422229	217.989800	4.872115
2.768442	219.922780	4.877120
2.937585	218.713324	4.882125
2.608545	226.847851	4.887130
2.973206	221.229419	4.892134
2.686410	216.202790	4.897139
2.790652	214.348557	4.902144
2.794595	221.814320	4.907149
3.087836	228.804783	4.912154
3.121730	228.419958	4.917158
2.949029	227.820533	4.922163
3.098748	232.688368	4.927168
3.160250	247.130590	4.932173
3.094324	231.971090	4.937178
3.277574	227.396444	4.942182
2.911325	234.976796	4.947187
3.301647	229.661244	4.952192
3.124541	228.018490	4.957197
2.887450	229.823996	4.962202
3.147521	236.753189	4.967206
3.268979	241.593790	4.972211
3.325241	237.383754	4.977216
2.986462	239.505644	4.982221
3.224183	242.512189	4.987226
3.243592	248.605681	4.992230
3.232525	247.750140	4.997235
3.356242	240.574720	5.002240
3.199703	249.207570	5.007245
3.190910	243.590331	5.012250
3.170655	245.045710	5.017254
3.285602	248.343449	5.022259
3.517608	248.215674	5.027264
3.551564	244.278023	5.032269
3.266509	241.335982	5.037274
3.667702	252.406617	5.042278
3.085209	233.233735	5.047283
3.434283	234.372188	5.052288
3.213554	248.649551	5.057293
3.478288	243.682572	5.062298
3.521835	249.050985	5.067302
3.106475	246.255779	5.072307
3.158260	239.218107	5.077312
3.295016	252.019320	5.082317
3.079824	251.366399	5.087322
3.400743	246.697548	5.092326
3.158929	248.953036	5.097331
3.401698	249.573378	5.102336
3.584774	241.063132	5.107341
3.521557	242.977606	5.112346
3.484720	254.249317	5.117350
3.225522	254.428970	5.122355
3.693085	244.355859	5.127360
3.440999	246.805930	5.132365
3.383619	244.543434	5.137370
3.582228	243.307242	5.142374
3.257755	246.587977	5.147379
3.479014	257.458844	5.152384
3.663978	266.377047	5.157389
3.853128	264.996797	5.162394
3.851552	266.794111	5.167398
3.633744	254.236646	5.172403
4.006387	250.651212	5.177408
3.258993	253.902885	5.182413
3.132495	261.999566	5.187418
3.579234	262.515386	5.192422
3.534619	271.564247	5.197427
4.048105	270.535287	5.202432
3.926058	265.660159	5.207437
3.739507	268.555600	5.212442
4.249101	263.958606	5.217446
3.885281	275.246439	5.222451
3.865582	273.876560	5.227456
4.020424	268.284454	5.232461
3.577389	258.504970	5.237466
3.879486	269.420205	5.242470
3.694763	267.373681	5.247475
3.923099	271.159960	5.252480
3.997196	277.760628	5.257485
4.106798	267.331959	5.262490
4.030964	261.279072	5.267494
3.813955	264.258347	5.272499
3.869854	257.346574	5.277504
4.012299	269.909637	5.282509
3.825572	266.730825	5.287514
4.477060	270.729625	5.292518
3.878200	264.792971	5.297523
3.724085	248.011562	5.302528
3.980933	262.461346	5.307533
4.161762	267.441403	5.312538
4.018223	268.922306	5.317542
3.949699	271.596895	5.322547
4.295246	273.580605	5.327552
4.248307	266.928444	5.332557
3.963522	262.376041	5.337562
4.161621	254.236765	5.342566
3.959324	261.633417	5.347571
4.238077	259.476768	5.352576
4.041147	264.066397	5.357581
4.035562	273.881121	5.362586
4.247603	271.915188	5.367590
3.878209	279.356847	5.372595
4.343931	271.897215	5.377600
4.350092	275.142296	5.382605
4.443673	278.547768	5.387610
4.378498	269.598443	5.392614
3.887649	260.338920	5.397619
4.314860	268.213354	5.402624
4.218377	273.470703	5.407629
4.227648	277.778298	5.412634
4.424453	272.227114	5.417638
4.079434	276.542416	5.422643
4.131113	265.005984	5.427648
4.326352	269.012546	5.432653
4.311524	263.469004	5.437658
4.496336	272.051883	5.442662
4.280779	274.053353	5.447667
4.339314	269.368402	5.452672
4.584385	272.671195	5.457677
4.337366	267.340971	5.462682
4.321566	271.453156	5.467686
4.267935	270.044269	5.472691
4.626200	270.156258	5.477696
4.542145	268.122534	5.482701
4.479348	274.978627	5.487706
4.859885	268.889483	5.492710
4.438067	277.503541	5.497715
4.532972	272.477575	5.502720
4.291676	267.908909	5.507725
4.103987	269.010716	5.512730
4.324072	265.952059	5.517734
3.806981	271.907631	5.522739
4.225948	264.996273	5.527744
4.105161	267.881475	5.532749
4.386125	276.082397	5.537754
4.703007	285.489424	5.542758
4.503544	292.145344	5.547763
5.075373	286.032738	5.552768
4.703724	286.628525	5.557773
4.363694	284.606179	5.562778
4.741209	282.418332	5.567782
4.810859	291.275409	5.572787
4.666393	283.040762	5.577792
4.909022	282.234304	5.582797
4.674030	278.765617	5.587802
4.538013	272.054558	5.592806
4.667818	288.264173	5.597811
4.794745	286.453856	5.602816
4.924262	294.884006	5.607821
4.500180	290.891112	5.612826
4.885933	292.362373	5.617830
5.149286	295.089695	5.622835
4.839144	285.340124	5.627840
4.671628	280.794768	5.632845
4.605895	288.382136	5.637850
5.066710	291.170461	5.642854
4.769540	297.031690	5.647859
4.894729	280.918594	5.652864
5.204941	289.959674	5.657869
4.585561	283.504200	5.662874
5.050724	287.876856	5.667878
4.690794	295.449923	5.672883
4.593308	293.073444	5.677888
4.576157	291.105229	5.682893
5.042609	298.470540	5.687898
4.861198	297.508643	5.692902
4.809663	304.976752	5.697907
4.612411	293.501205	5.702912
4.404463	298.064084	5.707917
4.356816	300.966377	5.712922
4.896358	312.303404	5.717926
5.179544	317.776894	5.722931
5.375124	321.318351	5.727936
5.551027	318.374130	5.732941
5.122528	302.862904	5.737946
5.177041	288.870988	5.742950
4.955183	291.907969	5.747955
5.000644	288.095064	5.752960
4.713500	298.108661	5.757965
4.984659	305.358851	5.762970
5.079893	310.814147	5.767974
4.988191	315.504462	5.772979
5.465115	309.422442	5.777984
5.679953	317.931067	5.782989
5.553675	319.374486	5.787994
5.016367	302.140169	5.792998
5.183764	306.568682	5.798003
5.321611	310.549388	5.803008
5.331972	320.174997	5.808013
5.226395	309.131248	5.813018
5.417044	301.758724	5.818022
5.305382	310.596585	5.823027
5.233608	301.135753	5.828032
5.373038	293.812335	5.833037
5.241288	310.910563	5.838042
5.566299	307.490719	5.843046
5.180101	307.408577	5.848051
5.250530	309.779968	5.853056
5.316129	308.317713	5.858061
5.457790	313.667707	5.863066
5.554967	311.596269	5.868070
5.455790	312.171779	5.873075
5.539568	314.620185	5.878080
5.658656	317.135859	5.883085
5.223510	308.921148	5.888090
5.614269	310.021479	5.893094
5.778368	312.694657	5.898099
5.536327	299.331026	5.903104
5.637944	293.092315	5.908109
5.035299	295.147729	5.913114
5.337439	296.340949	5.918118
5.790868	305.122461	5.923123
5.584553	308.343682	5.928128
5.996491	316.568522	5.933133
5.515341	303.327537	5.938138
5.490485	296.418831	5.943142
4.992170	310.442075	5.948147
5.385408	309.153430	5.953152
5.633053	313.310028	5.958157
5.168272	315.527473	5.963162
5.648841	313.937334	5.968166
5.366218	313.408803	5.973171
5.664729	311.366129	5.978176
6.000199	321.086650	5.983181
5.788970	313.143953	5.988186
6.030156	308.370444	5.993190
6.155604	320.230685	5.998195
6.116548	320.088167	6.003200
5.767586	319.645893	6.008205
5.363925	316.576777	6.013210
5.890898	313.429202	6.018214
5.874077	314.014035	6.023219
5.783512	307.647057	6.028224
5.954318	313.400629	6.033229
5.830853	314.998631	6.038234
6.136303	312.575232	6.043238
5.611935	304.371252	6.048243
5.525913	297.487888	6.053248
5.583787	312.332517	6.058253
5.440923	316.100671	6.063258
6.180988	317.529424	6.068262
5.858047	316.668655	6.073267
5.701606	320.815404	6.078272
5.515220	327.020056	6.083277
5.632960	326.448172	6.088282
6.076137	317.606332	6.093286
5.597055	330.857820	6.098291
5.517119	317.370861	6.103296
5.984898	326.156477	6.108301
5.737205	315.742281	6.113306
5.780874	316.156348	6.118310
5.753069	314.075896	6.123315
5.859711	321.563675	6.128320
6.043919	325.144868	6.133325
5.748785	318.578787	6.138330
5.391612	294.074730	6.143334
5.440377	301.647441	6.148339
5.306052	310.615378	6.153344
5.689954	317.291209	6.158349
5.803510	324.445725	6.163354
5.740600	322.101823	6.168358
5.590879	316.452720	6.173363
5.810105	330.750233	6.178368
5.728072	329.383727	6.183373
5.757263	332.191805	6.188378
5.724004	315.530718	6.193382
5.578883	322.314228	6.198387
5.458095	315.774785	6.203392
5.233300	316.758988	6.208397
5.265781	322.413880	6.213402
5.354456	325.778997	6.218406
5.534110	342.107447	6.223411
5.949793	344.127700	6.228416
6.243065	335.856511	6.233421
5.644300	325.221729	6.238426
5.671361	324.151444	6.243430
5.497301	336.548702	6.248435
5.891986	330.441515	6.253440
6.123087	329.772888	6.258445
5.791948	333.310937	6.263450
5.937735	318.415788	6.268454
5.342992	320.944529	6.273459
5.653017	320.719186	6.278464
6.136138	326.452609	6.283469
5.722289	337.330663	6.288474
6.021016	319.649791	6.293478
5.881520	323.964742	6.298483
5.838570	322.187198	6.303488
5.957407	318.350208	6.308493
5.356147	326.201303	6.313498
5.883644	311.297348	6.318502
5.742270	326.008498	6.323507
5.673109	322.245070	6.328512
5.789751	316.586132	6.333517
5.530705	323.311451	6.338522
5.491638	313.124197	6.343526
5.458686	321.124083	6.348531
5.607464	325.947799	6.353536
5.989356	337.287242	6.358541
5.856466	331.176777	6.363546
5.770773	330.703004	6.368550
5.368073	336.207361	6.373555
5.601374	330.280323	6.378560
6.345528	344.094327	6.383565
5.637972	333.413204	6.388570
5.750297	319.038947	6.393574
5.825938	327.907764	6.398579
5.992906	316.916486	6.403584
5.881570	323.818121	6.408589
5.934267	317.314940	6.413594
5.823920	318.167431	6.418598
5.518217	319.673587	6.423603
5.559184	328.705988	6.428608
5.573391	317.570819	6.433613
5.928202	323.096432	6.438618
5.838198	314.536921	6.443622
5.693692	319.447426	6.448627
5.678173	323.426705	6.453632
5.892147	320.811907	6.458637
5.643302	321.698617	6.463642
5.680238	313.087706	6.468646
5.731072	319.306040	6.473651
5.601400	312.328228	6.478656
5.929441	316.130630	6.483661
6.093624	325.703819	6.488666
6.123539	317.211056	6.493670
5.931689	318.063582	6.498675
5.806621	318.371046	6.503680
5.690061	320.296997	6.508685
5.275927	319.966109	6.513690
5.808848	320.560261	6.518694
5.421065	321.933666	6.523699
5.735851	320.328211	6.528704
5.828611	318.308079	6.533709
5.709442	327.166099	6.538714
5.806373	315.948449	6.543718
5.783772	318.024284	6.548723
6.021378	327.908740	6.553728
5.977703	323.723734	6.558733
5.879603	323.432224	6.563738
6.445772	316.222686	6.568742
5.861626	318.974399	6.573747
5.390823	318.883284	6.578752
5.691820	320.437345	6.583757
5.556683	311.536856	6.588762
5.909073	316.977425	6.593766
5.750548	320.580342	6.598771
6.156717	324.493966	6.603776
6.387675	323.467863	6.608781
5.609716	322.931035	6.613786
5.642612	329.895635	6.618790
5.639431	324.192076	6.623795
5.774768	320.127894	6.628800
6.117541	324.026078	6.633805
5.587195	321.568297	6.638810
5.734283	315.635704	6.643814
5.734403	317.252429	6.648819
5.707322	317.152338	6.653824
6.013584	311.175982	6.658829
5.882257	317.574535	6.663834
5.853387	300.915942	6.668838
5.345272	297.480285	6.673843
5.114469	303.198309	6.678848
5.637714	318.644353	6.683853
5.558802	331.811391	6.688858
5.991412	323.540659	6.693862
6.095290	316.849179	6.698867
5.910091	315.751833	6.703872
6.097223	316.054980	6.708877
5.912647	312.426579	6.713882
5.439104	308.390763	6.718886
5.627243	309.250563	6.723891
5.814564	319.671181	6.728896
5.922213	308.436048	6.733901
5.658516	311.182159	6.738906
5.523885	311.336091	6.743910
5.713146	326.017909	6.748915
5.781061	319.708507	6.753920
5.908357	314.804034	6.758925
5.940187	330.329765	6.763930
5.770508	311.687300	6.768934
5.548623	306.207620	6.773939
5.708058	313.494191	6.778944
5.770822	320.700906	6.783949
6.070882	322.201330	6.788954
5.678010	297.339002	6.793958
5.369158	297.646607	6.798963
5.884926	304.485396	6.803968
6.303285	306.723523	6.808973
5.562926	304.456627	6.813978
5.529085	298.811633	6.818982
5.706731	288.954476	6.823987
5.571182	306.154529	6.828992
6.018045	304.933464	6.833997
5.443546	311.100464	6.839002
5.706660	303.596437	6.844006
5.936392	315.089268	6.849011
5.844586	317.631450	6.854016
5.747030	315.609313	6.859021
5.706344	314.442011	6.864026
6.174421	310.420935	6.869030
6.066417	302.519118	6.874035
5.673962	299.742483	6.879040
5.833212	293.690948	6.884045
4.999753	293.415857	6.889050
5.565434	291.034200	6.894054
5.851589	308.348927	6.899059
5.730292	320.177985	6.904064
5.709303	320.102255	6.909069
5.534358	321.202081	6.914074
5.584607	309.526640	6.919078
5.734623	320.658571	6.924083
5.591050	324.132613	6.929088
5.666175	319.897475	6.934093
5.827282	327.269211	6.939098
5.816500	317.273700	6.944102
5.722832	314.330323	6.949107
5.803528	323.799453	6.954112
5.842414	322.426776	6.959117
5.838913	319.719290	6.964122
5.963324	317.159566	6.969126
5.914037	319.486324	6.974131
5.849526	318.632774	6.979136
5.703548	302.925703	6.984141
5.316116	318.592629	6.989146
5.815397	308.495562	6.994150
5.666366	321.600744	6.999155
5.819002	316.353810	7.004160
5.856533	319.404192	7.009165
5.617794	328.568726	7.014170
5.423487	314.416218	7.019174
5.483148	316.476081	7.024179
5.818641	316.724492	7.029184
5.893314	318.104986	7.034189
5.253167	320.836946	7.039194
5.325992	320.771919	7.044198
5.593176	316.051306	7.049203
5.594536	313.691072	7.054208
5.518831	314.661553	7.059213
5.524300	322.073338	7.064218
5.690068	315.625318	7.069222
5.696460	322.261854	7.074227
5.914940	322.202622	7.079232
6.191161	319.758464	7.084237
5.561309	320.318524	7.089242
5.931488	317.597150	7.094246
6.028042	313.773121	7.099251
5.702130	314.570591	7.104256
5.641792	321.220680	7.109261
5.931245	320.587260	7.114266
5.707470	316.531535	7.119270
5.653252	322.509968	7.124275
5.610217	318.116060	7.129280
5.616565	317.131257	7.134285
5.481923	320.736783	7.139290
5.990243	321.480295	7.144294
5.759279	317.878098	7.149299
5.874980	318.600484	7.154304
5.803886	316.988671	7.159309
5.762196	323.401744	7.164314
5.748780	314.605686	7.169318
5.763440	326.340814	7.174323
5.719974	313.170878	7.179328
5.789940	319.468490	7.184333
5.653194	321.283692	7.189338
5.481980	315.350039	7.194342
5.654201	315.487832	7.199347
5.570959	315.896349	7.204352
5.808590	312.233849	7.209357
6.123623	321.701293	7.214362
6.083402	316.392639	7.219366
5.851300	319.994358	7.224371
5.813313	318.143277	7.229376
5.626064	309.579927	7.234381
5.562844	321.994718	7.239386
5.641728	314.310566	7.244390
5.635420	315.931455	7.249395
5.714177	311.929867	7.254400
5.925491	309.065553	7.259405
5.403061	317.337797	7.264410
5.707679	321.501344	7.269414
5.609642	324.297593	7.274419
5.945459	322.612934	7.279424
5.721792	321.553214	7.284429
5.765459	318.759292	7.289434
5.872753	320.014488	7.294438
6.123613	323.098094	7.299443
5.620594	319.535091	7.304448
6.101074	317.483066	7.309453
5.647416	321.014878	7.314458
5.650065	314.146174	7.319462
5.708749	328.228240	7.324467
5.952900	322.878472	7.329472
6.027161	320.801110	7.334477
5.672896	316.613845	7.339482
5.925555	311.598107	7.344486
6.336417	315.979225	7.349491
5.823704	326.663861	7.354496
5.928607	319.206606	7.359501
5.823123	327.255752	7.364506
6.070222	313.869736	7.369510
5.879050	318.505937	7.374515
5.796862	309.094178	7.379520
5.080965	299.464720	7.384525
5.554624	319.831703	7.389530
5.946351	310.216444	7.394534
6.073059	310.557472	7.399539
5.771586	318.384034	7.404544
6.177171	318.109012	7.409549
5.761796	313.833188	7.414554
5.819689	294.579516	7.419558
5.869237	304.227489	7.424563
5.203716	298.589099	7.429568
5.849809	299.032754	7.434573
5.521865	303.465624	7.439578
5.816859	316.811712	7.444582
6.060093	321.864324	7.449587
5.995099	305.053166	7.454592
5.652158	298.782432	7.459597
5.405702	303.462037	7.464602
5.711624	306.087823	7.469606
5.910416	311.346664	7.474611
5.931286	309.590822	7.479616
5.921747	303.537090	7.484621
5.399654	304.067718	7.489626
5.706621	291.966347	7.494630
6.001835	296.947585	7.499635
5.517603	297.367916	7.504640
5.348318	294.218020	7.509645
5.812988	294.436827	7.514650
6.091336	303.805571	7.519654
5.874566	312.514268	7.524659
5.676319	312.880581	7.529664
6.017718	293.820046	7.534669
5.339727	300.696005	7.539674
5.720280	297.789525	7.544678
5.910264	309.095555	7.549683
5.593642	310.163657	7.554688
5.814724	305.326841	7.559693
5.526728	303.334356	7.564698
5.817588	306.740756	7.569702
5.882733	315.184102	7.574707
5.747261	316.379020	7.579712
5.918609	305.194082	7.584717
5.561567	307.204931	7.589722
5.705131	307.464242	7.594726
5.809067	319.935262	7.599731
5.788062	319.891171	7.604736
5.719486	303.175484	7.609741
5.581577	307.531312	7.614746
5.580481	313.080699	7.619750
5.902998	320.218498	7.624755
5.742710	323.919765	7.629760
5.826498	322.707773	7.634765
5.455297	329.260734	7.639770
5.710702	324.108527	7.644774
5.665363	321.110168	7.649779
5.718462	326.654285	7.654784
5.790350	325.466291	7.659789
5.691059	329.268792	7.664794
5.916961	322.289396	7.669798
5.893405	329.275440	7.674803
5.946562	331.491339	7.679808
5.847249	315.846592	7.684813
5.724678	318.871283	7.689818
5.736151	308.492668	7.694822
5.798722	311.801737	7.699827
5.486698	318.880146	7.704832
5.925017	317.824922	7.709837
5.893005	325.872120	7.714842
5.625797	317.862208	7.719846
5.328625	309.803182	7.724851
5.516874	331.862901	7.729856
6.032494	317.577711	7.734861
5.813833	330.282461	7.739866
5.932051	330.896889	7.744870
6.112296	329.337690	7.749875
5.723652	314.655465	7.754880
5.779970	298.337944	7.759885
5.463576	301.949619	7.764890
5.749870	311.703102	7.769894
5.465063	316.398173	7.774899
5.740782	322.454947	7.779904
5.780566	318.858051	7.784909
5.553442	323.857349	7.789914
5.662606	320.088302	7.794918
5.830559	323.406275	7.799923
5.724971	324.593377	7.804928
5.901517	323.363779	7.809933
5.958469	323.130384	7.814938
5.597934	318.203790	7.819942
5.986458	318.848897	7.824947
5.706018	321.664053	7.829952
6.143353	311.440591	7.834957
5.662234	311.844618	7.839962
5.578054	298.064111	7.844966
5.670233	314.342882	7.849971
5.942908	309.564469	7.854976
6.024526	310.121321	7.859981
5.590055	302.270334	7.864986
5.634001	307.698813	7.869990
5.525190	299.268786	7.874995
5.534055	324.308151	7.880000
5.722879	320.156549	7.885005
5.747740	326.698463	7.890010
5.977158	324.255264	7.895014
6.468683	324.318032	7.900019
5.891330	310.272622	7.905024
5.882440	299.065132	7.910029
5.391813	306.706008	7.915034
5.381626	299.807672	7.920038
5.422944	295.498710	7.925043
5.589661	309.212771	7.930048
5.692688	318.789151	7.935053
5.606583	328.350691	7.940058
6.010208	325.997425	7.945062
6.213713	324.826903	7.950067
5.528767	315.838012	7.955072
6.127005	307.892671	7.960077
5.598188	304.090083	7.965082
5.382827	302.057817	7.970086
5.600885	308.623427	7.975091
5.678042	321.101781	7.980096
5.892331	315.500405	7.985101
6.027551	325.378655	7.990106
6.048698	324.568714	7.995110
5.812872	315.269456	8.000115
5.503923	302.734838	8.005133
5.577558	298.763161	8.010150
5.502828	307.146760	8.015168
6.115955	308.487202	8.020186
5.593048	310.963831	8.025203
5.391502	311.254068	8.030221
5.846894	312.495999	8.035238
5.764821	330.650571	8.040256
5.784833	330.089003	8.045274
5.927681	322.720556	8.050291
6.045409	334.185651	8.055309
6.207784	319.171234	8.060326
5.900521	314.889649	8.065344
5.536964	301.841041	8.070362
5.995955	293.962662	8.075379
5.459250	301.174871	8.080397
5.739495	310.863277	8.085414
6.016785	320.908734	8.090432
5.736873	316.619736	8.095450
5.908234	313.544816	8.100467
5.815580	320.388111	8.105485
6.050121	312.948590	8.110502
5.787557	318.404619	8.115520
5.819948	321.501652	8.120538
5.764051	319.566584	8.125555
5.904190	322.318655	8.130573
6.070389	318.029622	8.135590
5.901337	321.700786	8.140608
6.046603	317.187807	8.145626
5.660237	309.163346	8.150643
5.864339	323.076373	8.155661
5.861746	312.600193	8.160678
5.724727	327.412042	8.165696
5.790643	332.255231	8.170714
5.765987	324.884462	8.175731
5.795095	326.640865	8.180749
5.640393	325.115633	8.185766
5.670126	320.279834	8.190784
5.674963	324.857990	8.195802
5.803111	316.336875	8.200819
6.188819	323.200360	8.205837
5.893125	316.291493	8.210854
5.781294	320.679542	8.215872
5.264049	326.575991	8.220890
5.863381	319.609816	8.225907
6.005809	335.088179	8.230925
5.884970	334.419161	8.235942
6.091763	336.753780	8.240960
6.229646	343.375008	8.245978
6.106167	325.978412	8.250995
5.622211	320.417907	8.256013
5.891820	333.004847	8.261030
6.058324	335.370984	8.266048
6.035856	343.279430	8.271066
6.257042	344.605164	8.276083
5.940321	340.864659	8.281101
5.940532	336.961207	8.286118
5.791254	347.874624	8.291136
5.632510	348.233932	8.296154
6.057001	342.055478	8.301171
6.281128	350.745997	8.306189
6.318468	343.943048	8.311206
6.388551	337.674616	8.316224
6.165721	346.775531	8.321242
6.367630	335.803620	8.326259
5.913126	335.006681	8.331277
5.873585	328.348245	8.336294
6.518111	331.845405	8.341312
5.856884	325.943291	8.346330
6.017621	316.767042	8.351347
5.799743	333.270279	8.356365
5.785728	351.193381	8.361382
5.954763	347.001724	8.366400
5.845012	350.862466	8.371418
6.252556	343.752583	8.376435
6.241409	357.437233	8.381453
6.278122	348.898782	8.386470
6.299046	352.922205	8.391488
6.308941	344.391087	8.396506
6.344164	346.525216	8.401523
6.180544	354.499822	8.406541
5.911048	351.386244	8.411558
6.325742	354.761412	8.416576
6.000666	357.475474	8.421594
6.407670	353.795845	8.426611
6.420938	356.892705	8.431629
6.449618	346.045583	8.436646
6.458696	342.140749	8.441664
5.943445	341.053483	8.446682
6.039535	343.449519	8.451699
6.202425	350.480244	8.456717
6.454157	345.622496	8.461734
6.447524	346.646048	8.466752
6.424909	341.389227	8.471770
6.154809	329.228558	8.476787
6.186793	332.710642	8.481805
5.878399	337.956074	8.486822
6.216979	338.872231	8.491840
6.490451	353.348806	8.496858
6.160351	347.735937	8.501875
6.538559	348.235693	8.506893
6.260896	337.098620	8.511910
6.361955	332.333759	8.516928
6.236657	338.017717	8.521946
6.122981	331.781053	8.526963
6.262447	347.414514	8.531981
6.448974	351.825541	8.536998
6.380287	348.977328	8.542016
6.429911	345.596326	8.547034
6.212917	331.272091	8.552051
6.142576	343.911967	8.557069
6.279645	353.442818	8.562087
6.461507	345.818992	8.567104
6.258453	348.482498	8.572122
6.446294	349.409503	8.577139
6.577465	354.927309	8.582157
6.455667	346.347271	8.587175
6.567329	332.981665	8.592192
5.918560	327.374240	8.597210
5.694813	336.386935	8.602227
6.292525	343.132218	8.607245
6.393398	343.867647	8.612263
6.586125	339.296783	8.617280
6.199279	357.012866	8.622298
6.496648	352.113299	8.627315
6.684228	353.990190	8.632333
6.328935	353.682705	8.637351
6.449778	347.807132	8.642368
6.174576	354.609439	8.647386
6.670791	349.628422	8.652403
6.329438	351.565577	8.657421
6.234247	350.876787	8.662439
6.192475	345.903799	8.667456
6.131302	353.666805	8.672474
6.287411	351.184357	8.677491
6.187401	353.935956	8.682509
6.441078	355.871980	8.687527
6.155210	348.112705	8.692544
6.658809	362.976313	8.697562
6.909386	360.643248	8.702579
6.692325	358.203122	8.707597
6.622682	354.916423	8.712615
6.483581	343.338074	8.717632
6.893994	352.286752	8.722650
6.811003	344.716786	8.727667
7.023463	346.615047	8.732685
6.509710	353.640677	8.737703
6.630085	355.537499	8.742720
6.419471	364.134775	8.747738
6.513318	347.086153	8.752755
6.731994	349.800755	8.757773
6.362023	346.800647	8.762791
6.400381	351.209498	8.767808
6.577836	350.260519	8.772826
6.518897	347.145715	8.777843
6.368624	345.307385	8.782861
6.275841	347.707583	8.787879
6.488644	351.268809	8.792896
6.466858	359.524276	8.797914
6.612249	347.926874	8.802931
6.499641	353.867622	8.807949
6.593060	356.904669	8.812967
6.551566	352.016838	8.817984
6.211302	363.313432	8.823002
6.788567	363.952600	8.828019
6.731131	357.618814	8.833037
6.605196	369.917089	8.838055
6.824927	361.334358	8.843072
6.322907	358.780818	8.848090
6.982770	367.712754	8.853107
6.946306	353.619155	8.858125
6.647387	361.277178	8.863143
6.822505	350.262094	8.868160
7.025714	343.316562	8.873178
6.461236	353.508876	8.878195
6.648188	358.992754	8.883213
6.444404	353.928230	8.888231
6.430439	349.746131	8.893248
6.783166	364.459670	8.898266
6.781806	363.910896	8.903283
7.007454	372.550699	8.908301
6.682161	361.383159	8.913319
6.861415	347.650432	8.918336
6.826769	348.081932	8.923354
6.414364	351.109375	8.928371
6.895188	350.204676	8.933389
6.853558	356.058639	8.938407
7.184355	338.998377	8.943424
6.583835	351.837564	8.948442
6.589418	345.307788	8.953459
6.959474	345.875081	8.958477
6.895127	352.079699	8.963495
6.948261	349.584883	8.968512
6.864270	349.784238	8.973530
6.544138	349.872044	8.978547
6.910141	347.435807	8.983565
6.504839	347.581052	8.988583
6.855262	357.716124	8.993600
6.971551	365.650310	8.998618
7.058073	368.167753	9.003635
6.743783	354.647556	9.008653
6.875463	359.149171	9.013671
6.981008	352.035815	9.018688
6.996579	352.664612	9.023706
6.557534	354.490752	9.028723
7.194380	355.616077	9.033741
6.926405	353.089210	9.038759
7.204855	346.075160	9.043776
7.145355	349.423177	9.048794
6.983265	343.014177	9.053811
7.203731	353.687004	9.058829
6.936367	353.356362	9.063847
6.856104	343.536005	9.068864
6.632400	343.485728	9.073882
7.005560	347.031454	9.078899
6.663912	349.558757	9.083917
6.509797	354.120646	9.088935
6.511411	357.023672	9.093952
6.978275	366.092949	9.098970
7.272687	372.664571	9.103987
7.525110	369.419239	9.109005
7.037719	365.591699	9.114023
7.200146	346.629551	9.119040
7.146382	348.547174	9.124058
6.728010	353.254343	9.129075
7.277959	348.703593	9.134093
6.678850	347.821877	9.139111
6.797581	346.812617	9.144128
6.807670	351.355251	9.149146
6.826302	363.381718	9.154163
7.335506	369.389751	9.159181
7.109551	369.567030	9.164199
7.269123	357.595049	9.169216
7.162984	361.496254	9.174234
7.125508	357.971030	9.179251
6.999209	351.982464	9.184269
6.621404	353.325724	9.189287
7.069425	361.195637	9.194304
7.541366	360.967626	9.199322
6.923412	367.649743	9.204339
7.269851	350.072666	9.209357
7.260053	348.026282	9.214375
6.926203	349.271185	9.219392
7.023440	351.509261	9.224410
7.053005	370.299707	9.229427
7.074418	368.431488	9.234445
7.087916	384.744121	9.239463
6.951564	379.631224	9.244480
7.362063	378.153680	9.249498
7.353218	378.259288	9.254515
7.423617	376.702160	9.259533
7.252782	366.201653	9.264551
6.994828	358.163487	9.269568
7.456801	350.950458	9.274586
6.824718	356.833240	9.279603
7.363197	354.714112	9.284621
6.722471	366.133224	9.289639
7.263251	365.392749	9.294656
7.431494	372.615143	9.299674
7.213489	384.025251	9.304691
7.398780	377.877716	9.309709
7.409923	388.643112	9.314727
7.371694	372.953019	9.319744
7.280221	356.706372	9.324762
6.972702	367.249985	9.329779
7.480461	363.327460	9.334797
7.175106	372.958761	9.339815
7.226127	379.176983	9.344832
7.274692	373.640841	9.349850
7.024313	381.859330	9.354867
7.126297	371.612972	9.359885
6.989167	375.749367	9.364903
7.048779	379.952956	9.369920
7.147505	374.087129	9.374938
6.994209	378.932904	9.379955
7.331766	379.975448	9.384973
7.209618	380.212300	9.389991
7.143349	384.492290	9.395008
7.235179	379.384889	9.400026
7.178800	379.911286	9.405043
7.404776	377.212840	9.410061
7.245194	382.880060	9.415079
6.986250	381.733952	9.420096
7.473479	391.737295	9.425114
7.710415	401.520852	9.430131
7.539355	394.248584	9.435149
7.262357	378.573573	9.440167
7.308479	390.314926	9.445184
7.172251	391.150386	9.450202
7.171872	393.981149	9.455219
7.450499	400.075582	9.460237
7.230576	411.261956	9.465255
7.424671	405.453850	9.470272
7.577236	397.241303	9.475290
7.513875	399.551725	9.480307
7.339425	393.718957	9.485325
7.391923	401.256014	9.490343
7.641547	398.052136	9.495360
7.407214	397.467054	9.500378
7.189387	398.053301	9.505395
7.475052	397.333612	9.510413
7.807056	389.828394	9.515431
7.631760	397.009617	9.520448
7.758522	399.596534	9.525466
7.386583	402.665020	9.530483
7.553595	398.461043	9.535501
7.631677	401.620400	9.540519
7.517921	395.756092	9.545536
7.575123	398.158190	9.550554
7.215024	406.605201	9.555571
7.360951	393.294172	9.560589
7.361001	402.316235	9.565607
7.231051	408.329126	9.570624
7.680753	399.167801	9.575642
7.542889	404.127939	9.580659
7.098566	404.115166	9.585677
7.327666	408.844610	9.590695
7.386790	424.708387	9.595712
7.943106	414.905637	9.600730
7.574924	429.046698	9.605747
7.891141	415.724918	9.610765
7.877752	411.886680	9.615783
7.624836	413.639667	9.620800
7.517565	411.684186	9.625818
7.679892	414.928254	9.630835
7.337435	413.088282	9.635853
7.805204	424.836589	9.640871
8.039021	428.893151	9.645888
7.981116	420.290507	9.650906
7.986368	415.919217	9.655923
8.044582	413.092259	9.660941
7.651403	410.139932	9.665959
7.542533	414.587500	9.670976
7.388650	400.950779	9.675994
7.623536	413.764077	9.681011
7.608905	410.913749	9.686029
7.642802	410.570912	9.691047
7.562216	415.922902	9.696064
7.913015	426.591258	9.701082
7.912245	424.221583	9.706099
7.731199	424.101551	9.711117
7.754754	416.881020	9.716135
7.791209	430.012388	9.721152
8.083777	422.112530	9.726170
8.002915	414.983993	9.731187
7.997188	405.006838	9.736205
7.751640	404.843203	9.741223
7.550208	397.209608	9.746240
7.470882	402.820160	9.751258
7.807418	420.647729	9.756275
8.145495	424.498719	9.761293
8.090260	421.026738	9.766311
7.894863	410.296511	9.771328
8.136885	396.232098	9.776346
7.870321	408.400825	9.781363
7.743993	404.820001	9.786381
7.864798	404.151225	9.791399
7.995391	413.175058	9.796416
7.750609	405.923730	9.801434
7.848782	413.128650	9.806451
7.776724	409.545687	9.811469
7.721276	409.062134	9.816487
7.943992	428.482098	9.821504
8.187515	423.168038	9.826522
7.856782	428.003585	9.831539
8.192053	424.432935	9.836557
7.895075	412.396308	9.841575
7.516356	420.262430	9.846592
8.199602	417.262420	9.851610
8.165275	432.225617	9.856627
7.716511	435.751016	9.861645
7.977949	423.876734	9.866663
7.974581	432.684760	9.871680
7.964713	436.545747	9.876698
8.067045	438.852466	9.881715
7.970909	433.001181	9.886733
8.121013	428.001451	9.891751
7.862758	432.099916	9.896768
8.179601	427.140494	9.901786
8.146789	425.186042	9.906803
8.618098	431.569207	9.911821
8.494718	416.321502	9.916839
8.216965	410.485879	9.921856
8.096559	396.127619	9.926874
7.988200	402.544224	9.931891
7.857413	407.878782	9.936909
8.158876	400.564498	9.941927
7.931137	412.212813	9.946944
8.218528	418.514161	9.951962
8.148809	408.755239	9.956979
8.275598	416.842440	9.961997
8.196711	407.473091	9.967015
7.757581	398.566914	9.972032
8.050582	409.244259	9.977050
8.116940	418.331741	9.982067
8.179412	431.134028	9.987085
8.790659	429.625224	9.992103
8.183690	416.895282	9.997120
8.077723	408.057141	10.002138
7.898687	412.891155	10.007155
8.594127	418.620912	10.012173
8.325063	418.483028	10.017191
8.150370	415.058048	10.022208
8.104733	405.421605	10.027226
8.197920	417.471212	10.032243
8.093267	428.866856	10.037261
8.333972	418.292776	10.042279
7.988552	431.991661	10.047296
8.122254	419.414627	10.052314
8.436900	428.466612	10.057331
8.014972	432.587405	10.062349
8.318086	425.175029	10.067367
8.388366	431.548052	10.072384
8.148337	425.258449	10.077402
8.207644	431.570069	10.082419
7.896976	427.468859	10.087437
8.132018	427.151506	10.092455
8.365568	433.237191	10.097472
8.412540	425.760559	10.102490
8.276888	430.998057	10.107507
8.182307	434.641871	10.112525
8.583357	430.701234	10.117543
8.174703	423.869870	10.122560
8.378662	425.895689	10.127578
8.284074	423.357594	10.132595
8.276537	425.974892	10.137613
8.360783	426.422595	10.142631
7.893984	439.521877	10.147648
8.096737	447.805537	10.152666
8.599072	448.541578	10.157683
8.664204	447.262961	10.162701
8.872893	453.289411	10.167719
8.272560	450.574447	10.172736
8.368538	444.863652	10.177754
8.722537	452.552593	10.182771
8.176936	450.406592	10.187789
8.676584	450.748595	10.192807
8.704940	448.456429	10.197824
8.328348	444.589531	10.202842
8.755534	442.430919	10.207859
8.532630	438.426490	10.212877
8.821342	425.635978	10.217895
8.562512	436.222541	10.222912
8.445399	428.951327	10.227930
8.638995	433.970313	10.232947
8.348899	435.088495	10.237965
8.236115	434.755873	10.242983
8.554849	448.023176	10.248000
8.755017	450.153726	10.253018
9.004982	446.915073	10.258035
8.471058	437.651269	10.263053
8.788156	436.245064	10.268071
8.467195	430.507676	10.273088
8.416421	435.630979	10.278106
8.808853	444.655083	10.283123
8.388582	440.331106	10.288141
8.827936	445.460148	10.293159
8.672313	442.780082	10.298176
8.554513	434.319293	10.303194
8.741211	435.186523	10.308211
8.565275	454.756942	10.313229
8.782610	446.483798	10.318247
8.568572	448.890266	10.323264
8.867846	455.142442	10.328282
9.170120	450.907926	10.333299
8.562406	442.441364	10.338317
8.431994	438.908504	10.343335
8.687922	448.099023	10.348352
8.692126	449.881405	10.353370
8.903539	465.629994	10.358387
8.581815	462.701245	10.363405
8.667642	457.850363	10.368423
8.934441	461.750327	10.373440
9.041539	470.976653	10.378458
8.905218	468.363002	10.383475
8.712619	453.529965	10.388493
8.783911	446.554442	10.393511
8.979436	450.708485	10.398528
8.934092	438.134069	10.403546
8.735423	439.073922	10.408563
8.579601	439.783054	10.413581
8.807852	445.143769	10.418599
8.717118	450.708778	10.423616
8.727951	455.257633	10.428634
8.829793	460.253045	10.433651
8.968160	453.945540	10.438669
9.025526	454.738239	10.443687
8.917041	458.841792	10.448704
8.824884	460.200543	10.453722
9.236736	456.879882	10.458739
9.051938	451.013994	10.463757
9.150029	437.659890	10.468775
8.613633	442.527462	10.473792
8.739262	451.867652	10.478810
8.937487	449.552194	10.483827
9.131976	452.999533	10.488845
9.473358	446.183919	10.493863
8.753986	443.528514	10.498880
8.970436	448.136868	10.503898
9.120157	446.895571	10.508915
8.900788	439.454090	10.513933
8.997776	443.260574	10.518951
8.983865	444.951106	10.523968
8.799338	454.784534	10.528986
8.949484	447.566371	10.534003
8.741199	445.090154	10.539021
8.930533	452.650106	10.544039
9.316594	461.170307	10.549056
8.882615	454.349185	10.554074
9.148712	445.765506	10.559091
9.263804	447.764141	10.564109
9.114215	456.090042	10.569127
9.177180	452.094747	10.574144
8.822648	453.248207	10.579162
9.260044	450.756662	10.584179
8.865619	449.221409	10.589197
8.728767	455.150188	10.594215
9.148602	443.765601	10.599232
8.983490	458.140142	10.604250
8.851179	455.197681	10.609267
8.719855	448.360996	10.614285
8.686031	448.214886	10.619303
9.391408	458.862767	10.624320
9.350775	469.557382	10.629338
9.323558	472.436514	10.634355
9.228903	465.758207	10.639373
9.279953	458.243058	10.644391
9.524804	445.790704	10.649408
8.897502	445.945269	10.654426
9.282693	450.221253	10.659443
9.160248	472.629760	10.664461
9.271084	470.321594	10.669479
9.533731	463.937933	10.674496
8.961191	465.671266	10.679514
9.148894	468.589515	10.684531
9.283638	469.313365	10.689549
9.502728	478.042598	10.694567
9.270469	467.535817	10.699584
9.360943	480.737703	10.704602
9.391750	474.185019	10.709619
9.651371	473.639787	10.714637
9.319005	467.421347	10.719655
9.526984	463.545476	10.724672
8.753548	460.052771	10.729690
9.040355	459.831494	10.734707
9.083507	473.242705	10.739725
9.115885	471.237074	10.744743
9.389572	476.533923	10.749760
9.153526	482.572824	10.754778
9.505719	485.544358	10.759795
9.339361	478.694181	10.764813
9.099054	481.505512	10.769831
9.227216	474.884023	10.774848
9.341673	481.783492	10.779866
9.462564	478.167318	10.784883
9.499680	476.514382	10.789901
9.229511	476.234665	10.794919
9.704804	478.073085	10.799936
9.181483	493.749910	10.804954
9.380068	491.570083	10.809971
9.912300	490.846713	10.814989
9.668950	494.400099	10.820007
9.715713	476.232114	10.825024
9.337510	478.361203	10.830042
9.442532	470.373764	10.835059
9.779403	475.572417	10.840077
9.596926	481.303191	10.845095
9.647257	473.945930	10.850112
9.332018	476.418649	10.855130
9.384342	489.219402	10.860147
9.716516	494.412480	10.865165
9.774364	502.788152	10.870183
9.786038	494.117836	10.875200
9.368302	483.652546	10.880218
9.756753	493.163266	10.885235
9.712503	501.264513	10.890253
9.647369	503.486865	10.895271
9.660196	494.219951	10.900288
9.758061	506.316225	10.905306
9.658809	492.380608	10.910323
9.697846	493.722091	10.915341
9.485263	497.062413	10.920359
9.796896	501.034296	10.925376
9.718606	512.690964	10.930394
9.790131	496.062222	10.935411
9.879011	504.120653	10.940429
9.995692	505.506849	10.945447
10.169049	494.599242	10.950464
9.440098	495.072577	10.955482
9.550610	475.891168	10.960499
9.864637	483.835644	10.965517
9.604312	497.196297	10.970535
9.992138	495.138478	10.975552
9.723515	506.506055	10.980570
9.763709	500.620899	10.985587
10.096100	504.526437	10.990605
9.949168	494.290364	10.995623
9.775523	486.415730	11.000640
9.419913	476.903246	11.005658
10.201651	504.264241	11.010675
10.054461	504.157871	11.015693
9.494643	508.647273	11.020711
10.105106	504.869666	11.025728
9.981289	505.876760	11.030746
9.947427	498.756649	11.035763
9.732192	503.555300	11.040781
9.547243	506.323303	11.045799
9.947413	497.097060	11.050816
10.082618	506.729264	11.055834
9.647940	502.158218	11.060851
9.995979	500.406380	11.065869
9.743687	503.042862	11.070887
9.963525	503.226470	11.075904
9.872983	504.345142	11.080922
10.027342	503.658515	11.085939
10.040494	509.125320	11.090957
9.734805	509.163543	11.095975
9.950389	502.471631	11.100992
9.459419	505.577601	11.106010
10.062400	503.517838	11.111027
10.110920	509.824853	11.116045
9.758044	511.293625	11.121063
9.705657	505.968811	11.126080
10.197592	519.606815	11.131098
10.314216	518.970242	11.136115
10.290486	513.164459	11.141133
10.006201	520.602531	11.146151
9.892207	503.674477	11.151168
10.092654	520.418854	11.156186
10.496753	520.857782	11.161203
10.240049	514.154196	11.166221
9.869769	513.681792	11.171239
10.256554	517.339034	11.176256
10.538718	516.793447	11.181274
10.198094	519.181765	11.186291
10.294547	505.685861	11.191309
10.287466	501.837154	11.196327
10.364078	498.751709	11.201344
9.957362	501.282853	11.206362
10.028633	509.735330	11.211379
10.086545	512.427653	11.216397
10.490293	528.095861	11.221415
10.294625	516.620875	11.226432
10.016295	518.557702	11.231450
9.996048	516.683331	11.236467
10.243540	515.401561	11.241485
10.019414	526.228916	11.246503
10.199015	525.055542	11.251520
10.610132	526.840846	11.256538
10.002203	530.760257	11.261555
10.546608	528.984154	11.266573
10.454994	527.761493	11.271591
10.420233	524.573469	11.276608
10.019313	527.693823	11.281626
10.243836	532.395612	11.286643
10.469063	532.483710	11.291661
10.132578	533.432403	11.296679
10.684716	522.386914	11.301696
10.565826	529.351133	11.306714
10.220077	527.887186	11.311731
10.652251	526.873294	11.316749
10.376288	531.766610	11.321767
10.438428	533.268593	11.326784
10.271960	531.123509	11.331802
10.549971	536.318722	11.336819
10.421895	524.265188	11.341837
10.464042	532.422422	11.346855
10.479663	531.028437	11.351872
10.525545	537.910203	11.356890
10.212355	538.205203	11.361907
10.426833	523.898837	11.366925
10.331842	531.992219	11.371943
10.315431	528.428969	11.376960
10.806457	538.545408	11.381978
10.446724	540.479133	11.386995
10.680184	538.631527	11.392013
10.912854	541.356604	11.397031
10.378026	536.028003	11.402048
10.472064	538.686305	11.407066
10.525731	549.442022	11.412083
10.959672	544.252906	11.417101
10.842234	548.525124	11.422119
10.350953	543.063515	11.427136
10.550897	546.285971	11.432154
10.438605	551.377862	11.437171
10.918946	544.408037	11.442189
10.695451	565.084155	11.447207
10.514887	554.165347	11.452224
10.779563	559.539360	11.457242
10.682376	557.282505	11.462259
11.046836	554.101743	11.467277
10.718613	564.162722	11.472295
10.950089	553.037757	11.477312
10.576286	562.171755	11.482330
10.601865	563.723612	11.487347
11.027157	559.166973	11.492365
10.937672	561.162760	11.497383
10.922149	562.020459	11.502400
10.912722	549.187919	11.507418
10.790306	552.305938	11.512435
10.734463	540.648229	11.517453
10.603316	546.273205	11.522471
10.746903	550.252330	11.527488
10.742371	554.765735	11.532506
11.044497	558.739111	11.537523
11.045993	561.238263	11.542541
10.935363	557.664432	11.547559
11.198370	558.257866	11.552576
11.145838	552.582782	11.557594
10.690749	550.154444	11.562611
10.700412	548.284879	11.567629
10.833130	559.902414	11.572647
10.872465	548.684296	11.577664
11.091593	556.485796	11.582682
10.738873	551.444405	11.587699
10.965384	554.735306	11.592717
11.149903	555.691240	11.597735
10.676869	557.320730	11.602752
11.106843	551.946045	11.607770
10.693634	560.625450	11.612787
10.967060	552.558108	11.617805
10.982598	558.381148	11.622823
11.148469	559.030730	11.627840
11.009440	556.916083	11.632858
10.914908	558.537132	11.637875
10.760442	557.598798	11.642893
10.958115	560.237811	11.647911
11.114730	558.673555	11.652928
11.054642	556.357278	11.657946
10.579630	559.164139	11.662963
11.037861	563.510826	11.667981
10.896151	585.562728	11.672999
11.121008	594.297432	11.678016
11.233068	579.072888	11.683034
11.123448	589.503772	11.688051
11.491560	581.156599	11.693069
11.469706	580.999157	11.698087
11.245277	582.602564	11.703104
11.526846	575.130367	11.708122
11.384577	583.556168	11.713139
11.348334	562.182233	11.718157
11.351887	565.908621	11.723175
10.969781	566.435247	11.728192
11.430758	575.975743	11.733210
11.312466	577.467954	11.738227
11.510683	567.910216	11.743245
11.299707	572.092866	11.748263
11.201631	560.716262	11.753280
11.248349	558.449624	11.758298
11.074219	573.122295	11.763315
11.410331	570.444540	11.768333
11.696163	576.026694	11.773351
11.162415	580.499431	11.778368
11.401662	577.975606	11.783386
11.374285	578.611098	11.788403
11.493181	574.925790	11.793421
11.549591	569.726023	11.798439
11.100624	580.266539	11.803456
11.505204	582.097046	11.808474
11.730301	580.739867	11.813491
11.508108	578.937955	11.818509
11.234223	578.605168	11.823527
11.246553	590.418184	11.828544
11.201725	574.460709	11.833562
11.451816	579.521431	11.838579
11.431214	579.212322	11.843597
11.642787	572.211752	11.848615
11.322478	580.545357	11.853632
11.456730	579.265436	11.858650
11.487869	579.954931	11.863667
11.668794	577.418097	11.868685
11.526442	581.520639	11.873703
11.147985	579.664165	11.878720
11.571091	570.721480	11.883738
11.461651	581.647772	11.888755
11.693118	573.744737	11.893773
11.669035	578.901794	11.898791
11.447122	575.686097	11.903808
11.222146	573.682656	11.908826
11.671736	586.128149	11.913843
11.544439	598.366836	11.918861
12.059993	592.552799	11.923879
11.711486	595.532466	11.928896
11.919178	592.663272	11.933914
12.038675	583.076758	11.938931
12.058599	588.460485	11.943949
11.944103	580.226321	11.948967
11.744546	590.412443	11.953984
11.876352	580.139233	11.959002
11.402915	585.347321	11.964019
11.746797	585.079289	11.969037
11.826259	584.413787	11.974055
11.333727	594.481432	11.979072
11.612340	588.006883	11.984090
11.762228	597.974507	11.989107
12.022630	596.943176	11.994125
11.896103	608.282383	11.999143
11.647729	613.120935	12.004160
11.876971	604.328332	12.009178
11.703503	601.225004	12.014195
11.672269	600.384241	12.019213
11.893757	599.194873	12.024231
11.844634	608.707515	12.029248
12.168654	604.791456	12.034266
12.149194	609.247241	12.039283
11.974152	609.719540	12.044301
12.183111	595.770567	12.049319
11.846640	610.572682	12.054336
11.952456	604.203923	12.059354
11.952138	608.836602	12.064371
12.103138	608.674336	12.069389
11.884546	599.244591	12.074407
11.655381	603.480571	12.079424
11.735429	594.165270	12.084442
12.022713	601.971957	12.089459
11.661663	601.195167	12.094477
11.876392	607.539452	12.099495
11.737665	608.454203	12.104512
11.853257	614.154390	12.109530
12.230739	620.400759	12.114547
11.983115	622.881904	12.119565
12.393180	618.232950	12.124583
12.116717	624.549581	12.129600
12.118384	616.451942	12.134618
12.338864	629.456979	12.139635
12.532059	625.031131	12.144653
12.393685	607.715470	12.149671
12.199100	608.171877	12.154688
12.033779	599.030471	12.159706
12.323190	601.087186	12.164723
12.077914	604.429463	12.169741
12.026174	599.732500	12.174759
12.265693	613.119553	12.179776
12.356356	620.391995	12.184794
12.730416	624.297384	12.189811
12.624950	617.229399	12.194829
12.846845	605.399020	12.199847
12.251257	608.126837	12.204864
12.072797	598.981165	12.209882
12.299019	601.786146	12.214899
12.238923	610.596782	12.219917
12.255166	594.711827	12.224935
12.058994	595.136925	12.229952
12.318683	603.866211	12.234970
12.446372	605.884992	12.239987
12.292084	618.689606	12.245005
12.420189	626.287567	12.250023
12.276678	632.709728	12.255040
12.633624	623.193515	12.260058
12.600762	621.551462	12.265075
12.437362	619.248106	12.270093
12.530370	613.925867	12.275111
12.472093	621.663294	12.280128
12.671438	621.815381	12.285146
12.445201	631.305120	12.290163
12.535326	620.637605	12.295181
12.723450	619.301958	12.300199
12.778551	621.208971	12.305216
12.715384	609.239944	12.310234
12.432189	598.892488	12.315251
12.347751	604.040015	12.320269
12.502384	614.562309	12.325287
12.721817	616.200748	12.330304
13.038735	623.286492	12.335322
12.829869	618.118546	12.340339
12.200698	602.974676	12.345357
12.675017	618.313252	12.350375
12.725482	628.208014	12.355392
12.578427	616.504498	12.360410
12.768693	624.559821	12.365427
12.618336	628.433256	12.370445
12.844725	629.837093	12.375463
12.826738	635.192025	12.380480
12.832190	628.712657	12.385498
13.086393	623.415809	12.390515
12.937876	623.609434	12.395533
13.110470	615.942756	12.400551
12.715610	614.196125	12.405568
12.895855	595.713758	12.410586
12.693177	601.031166	12.415603
12.666139	605.046335	12.420621
12.566938	612.799597	12.425639
12.727432	618.862008	12.430656
12.758539	622.606207	12.435674
12.868802	632.557931	12.440691
12.572251	629.480073	12.445709
12.863672	623.246504	12.450727
12.633300	620.066829	12.455744
12.752231	625.716009	12.460762
12.736643	627.769723	12.465779
12.435297	629.580762	12.470797
12.450578	626.732053	12.475815
12.566902	638.661448	12.480832
12.987205	643.238114	12.485850
13.184667	650.575988	12.490867
12.968510	659.347831	12.495885
13.170553	658.590661	12.500903
13.102631	655.489824	12.505920
13.061270	655.247060	12.510938
13.478651	660.114507	12.515955
13.297328	650.710488	12.520973
13.014959	631.444921	12.525991
12.878998	635.158332	12.531008
13.180243	636.840838	12.536026
13.473010	644.154403	12.541043
13.124661	638.481170	12.546061
13.057798	631.981502	12.551079
12.885406	622.235294	12.556096
12.977420	640.053819	12.561114
13.088424	644.678642	12.566131
13.250935	639.657987	12.571149
13.595004	646.073663	12.576167
13.484722	646.501168	12.581184
13.046351	636.906812	12.586202
13.225134	648.271089	12.591219
13.040557	644.948585	12.596237
13.395186	649.257777	12.601255
13.243214	654.437923	12.606272
13.042398	652.184568	12.611290
13.471581	647.336978	12.616307
13.226593	656.722356	12.621325
13.341313	646.435990	12.626343
13.534034	649.795284	12.631360
13.610768	646.895980	12.636378
13.775832	645.529209	12.641395
13.241647	652.147898	12.646413
13.266608	651.945298	12.651431
13.712791	651.342613	12.656448
13.344946	651.541986	12.661466
13.434577	637.804056	12.666483
13.433396	648.006660	12.671501
13.715198	646.912036	12.676519
13.422729	651.265177	12.681536
13.291654	655.675239	12.686554
13.405777	639.532017	12.691571
13.360117	648.100591	12.696589
13.614889	645.940399	12.701607
13.333421	647.521136	12.706624
13.268860	646.887523	12.711642
13.600486	638.874195	12.716659
13.260544	651.852899	12.721677
13.250998	649.942135	12.726695
13.459803	652.115544	12.731712
13.463632	661.272844	12.736730
13.611033	647.585869	12.741747
13.467947	652.941350	12.746765
13.638346	646.676125	12.751783
13.853145	654.595103	12.756800
13.798531	658.636668	12.761818
13.941034	644.278297	12.766835
13.356348	642.501261	12.771853
13.313464	644.663365	12.776871
13.733255	657.744684	12.781888
13.618430	662.556145	12.786906
14.020658	663.118440	12.791923
13.976464	670.891564	12.796941
13.917601	665.056489	12.801959
14.057844	666.328581	12.806976
13.810189	658.610555	12.811994
13.618144	652.916137	12.817011
13.499217	655.677039	12.822029
13.725408	666.453300	12.827047
14.043352	669.565891	12.832064
13.704106	669.401063	12.837082
14.223962	674.224159	12.842099
13.883871	676.173774	12.847117
13.742453	658.751243	12.852135
14.012563	666.084124	12.857152
13.586388	671.411105	12.862170
14.078748	663.921830	12.867187
13.747973	668.179957	12.872205
13.539520	676.284759	12.877223
14.129568	675.757501	12.882240
13.917993	673.228117	12.887258
14.036766	661.031920	12.892275
13.910405	663.917052	12.897293
14.028950	672.690437	12.902311
13.907315	671.892147	12.907328
14.144920	670.523547	12.912346
14.242877	664.705080	12.917363
14.090814	665.580886	12.922381
13.771348	675.851996	12.927399
13.838846	665.569815	12.932416
13.581860	677.371174	12.937434
13.984392	694.844772	12.942451
14.196337	694.584658	12.947469
14.230896	694.844451	12.952487
14.316520	701.726404	12.957504
14.436029	699.811320	12.962522
14.397762	691.243355	12.967539
14.002002	694.069455	12.972557
14.597789	693.389829	12.977575
14.779972	691.761622	12.982592
14.280057	679.188386	12.987610
14.306115	665.895817	12.992627
14.457712	679.927748	12.997645
14.206059	673.797651	13.002663
14.357117	667.327155	13.007680
14.118519	671.195404	13.012698
14.363493	684.786782	13.017715
14.579227	685.283444	13.022733
14.567717	696.273451	13.027751
14.590596	690.406707	13.032768
14.135227	685.106714	13.037786
14.430143	679.364869	13.042803
14.518171	682.510105	13.047821
14.574664	692.315605	13.052839
14.435734	685.085551	13.057856
14.575547	693.199251	13.062874
14.566978	682.711161	13.067891
14.077602	681.111778	13.072909
14.618136	693.082455	13.077927
14.703136	692.453956	13.082944
14.573688	704.289121	13.087962
14.778021	690.410220	13.092979
14.656536	698.072318	13.097997
14.403461	692.860742	13.103015
14.561138	690.674638	13.108032
14.495838	692.799214	13.113050
14.603943	693.180094	13.118067
14.985668	692.660025	13.123085
14.498357	691.842931	13.128103
14.574362	688.691279	13.133120
14.448716	695.915382	13.138138
14.546635	695.089218	13.143155
14.654118	692.226143	13.148173
14.945807	691.445547	13.153191
14.957877	698.010759	13.158208
14.963616	700.569228	13.163226
14.965331	697.930896	13.168243
15.152493	694.891319	13.173261
15.094126	691.053712	13.178279
14.696997	678.666437	13.183296
14.652970	689.737239	13.188314
14.820606	695.410415	13.193331
14.816035	699.358993	13.198349
15.072654	703.339488	13.203367
15.200324	688.093486	13.208384
14.729751	685.847414	13.213402
14.694689	689.885942	13.218419
14.992362	691.026230	13.223437
14.781585	692.665390	13.228455
15.192866	690.938400	13.233472
14.831730	699.934800	13.238490
14.681542	690.648985	13.243507
14.960400	694.591302	13.248525
14.746062	704.849216	13.253543
14.937959	695.330262	13.258560
14.996391	696.343704	13.263578
15.048021	688.528577	13.268595
15.071451	695.874631	13.273613
14.949897	701.324600	13.278631
14.962510	694.197176	13.283648
15.032016	700.412632	13.288666
14.910703	696.619536	13.293683
14.997526	689.994937	13.298701
15.059771	702.399838	13.303719
15.134265	697.998764	13.308736
14.798867	701.670660	13.313754
14.979421	717.187599	13.318771
15.364871	711.570499	13.323789
15.240853	722.802094	13.328807
15.412668	715.416352	13.333824
15.296511	714.557248	13.338842
15.261662	722.016526	13.343859
15.274914	726.855398	13.348877
15.057685	718.750770	13.353895
15.093196	723.302163	13.358912
15.024107	719.115937	13.363930
14.936009	722.821914	13.368947
15.166281	722.659929	13.373965
15.213164	729.465877	13.378983
15.424156	720.218482	13.384000
15.591016	734.494224	13.389018
15.305763	730.392142	13.394035
15.372815	728.267479	13.399053
15.602778	732.785444	13.404071
15.532306	726.235812	13.409088
15.400940	722.677799	13.414106
15.365414	730.421197	13.419123
15.700051	742.887854	13.424141
15.363869	748.339697	13.429159
15.418449	743.812328	13.434176
15.716862	741.765247	13.439194
15.709629	748.901509	13.444211
15.693680	742.703133	13.449229
15.934258	746.717692	13.454247
15.688174	736.493761	13.459264
15.547601	725.925216	13.464282
15.227865	726.047673	13.469299
15.852113	738.750092	13.474317
15.495318	740.131133	13.479335
15.934655	738.488130	13.484352
15.911771	740.817539	13.489370
15.794370	737.746482	13.494387
15.664879	730.224615	13.499405
15.297893	746.006705	13.504423
15.766164	747.174082	13.509440
16.151515	736.201764	13.514458
15.677596	748.336737	13.519475
15.950246	742.904442	13.524493
15.838467	740.125990	13.529511
15.942911	751.249451	13.534528
15.844554	754.104992	13.539546
16.056866	743.500427	13.544563
16.188877	740.087590	13.549581
16.027245	724.627833	13.554599
15.543361	722.932920	13.559616
15.625776	730.894633	13.564634
15.941376	744.257317	13.569651
16.013880	733.794443	13.574669
15.968789	740.583158	13.579687
15.947901	744.903505	13.584704
15.978760	744.870393	13.589722
15.909135	750.943433	13.594739
16.381929	745.846037	13.599757
16.093758	751.637533	13.604775
15.986208	746.384350	13.609792
16.170916	745.263814	13.614810
15.676854	745.763696	13.619827
15.948268	742.161901	13.624845
15.802675	746.331256	13.629863
15.943294	739.376381	13.634880
16.047082	753.734540	13.639898
16.254134	754.503946	13.644915
16.450498	748.660663	13.649933
16.091495	744.841451	13.654951
15.646476	739.984784	13.659968
15.782602	756.117724	13.664986
16.153836	763.763094	13.670003
15.908388	765.088932	13.675021
15.935446	765.394073	13.680039
16.347416	769.770104	13.685056
16.469160	770.865208	13.690074
16.510897	768.305838	13.695091
16.483842	763.380933	13.700109
16.429340	766.983862	13.705127
16.600803	763.508075	13.710144
16.510580	764.197538	13.715162
16.238923	765.164550	13.720179
16.711305	761.960637	13.725197
16.743706	755.426536	13.730215
16.527922	766.435768	13.735232
16.781552	763.149153	13.740250
16.768834	762.027797	13.745267
16.417804	754.865450	13.750285
16.466009	761.806900	13.755303
16.577772	770.470940	13.760320
16.715610	760.745780	13.765338
16.507423	767.884936	13.770355
16.890105	753.921415	13.775373
16.617996	766.047068	13.780391
16.929481	766.061780	13.785408
16.671589	757.231342	13.790426
16.428585	749.181204	13.795443
16.753416	751.349183	13.800461
16.394299	763.781862	13.805479
16.470457	758.616833	13.810496
16.919857	759.073961	13.815514
16.878970	769.203924	13.820531
16.661261	755.005687	13.825549
16.760487	766.309844	13.830567
16.473555	751.459689	13.835584
16.766565	758.725929	13.840602
16.921598	767.386386	13.845619
16.940823	761.135191	13.850637
16.656890	755.458202	13.855655
16.498166	763.880338	13.860672
16.576655	760.677795	13.865690
16.310502	760.892893	13.870707
16.514534	763.429964	13.875725
16.854960	769.877810	13.880743
16.801451	775.768473	13.885760
16.837554	780.632204	13.890778
16.977647	787.335302	13.895795
17.310978	785.538391	13.900813
17.254696	783.514972	13.905831
17.004376	790.307259	13.910848
17.292403	779.337445	13.915866
17.226197	782.203764	13.920883
17.374222	763.641034	13.925901
17.172187	756.338728	13.930919
16.615696	762.039464	13.935936
16.590739	762.747167	13.940954
16.899944	780.569886	13.945971
16.935998	776.556618	13.950989
17.052731	789.170839	13.956007
16.825382	797.029337	13.961024
17.237958	782.035533	13.966042
16.894838	785.762295	13.971059
16.974402	787.245808	13.976077
17.022063	795.702097	13.981095
17.080487	793.102257	13.986112
17.662851	803.476018	13.991130
17.404354	799.486516	13.996147
17.406616	785.711584	14.001165
17.580550	782.850771	14.006183
17.677340	783.003049	14.011200
17.552880	777.594704	14.016218
17.216540	789.768242	14.021235
17.271427	780.993232	14.026253
17.162596	789.199336	14.031271
17.443489	790.787199	14.036288
17.492853	784.941545	14.041306
17.604303	796.370048	14.046323
17.319030	795.505714	14.051341
17.644143	803.524344	14.056359
17.331924	797.154333	14.061376
17.762757	794.578558	14.066394
17.271464	800.000920	14.071411
17.737353	799.319425	14.076429
17.886555	804.900834	14.081447
17.481824	802.149049	14.086464
17.946109	795.276299	14.091482
17.315805	790.057158	14.096499
17.466283	800.775863	14.101517
17.532513	806.922440	14.106535
17.431389	800.781485	14.111552
17.830664	805.768554	14.116570
17.661092	807.467578	14.121587
17.834555	805.764982	14.126605
17.957393	807.879213	14.131623
17.821014	811.778913	14.136640
18.089369	792.080297	14.141658
18.148100	802.967918	14.146675
17.928010	801.433891	14.151693
17.996272	799.668782	14.156711
17.980682	794.035205	14.161728
17.991453	786.958521	14.166746
18.021015	780.973945	14.171763
17.737464	770.683246	14.176781
18.033614	773.168108	14.181799
17.937905	786.323473	14.186816
17.830793	775.064899	14.191834
17.968619	784.381275	14.196851
18.141730	791.928120	14.201869
18.244370	794.269550	14.206887
17.822672	790.624186	14.211904
18.112628	790.967288	14.216922
17.933158	795.369140	14.221939
17.951539	797.644796	14.226957
18.030493	799.923645	14.231975
18.018455	799.578486	14.236992
18.339824	797.991713	14.242010
18.457653	806.279296	14.247027
18.405466	805.037854	14.252045
18.391649	802.266229	14.257063
17.702398	792.720318	14.262080
18.001435	791.354767	14.267098
17.896672	801.251703	14.272115
17.871626	794.871694	14.277133
18.366274	798.638430	14.282151
18.009211	796.914297	14.287168
18.320404	797.304584	14.292186
18.499109	801.997800	14.297203
18.096496	796.077351	14.302221
18.283982	792.182510	14.307239
18.001847	803.202095	14.312256
17.962899	796.208886	14.317274
18.820348	813.880009	14.322291
18.468925	814.547027	14.327309
18.500294	810.076903	14.332327
18.624447	822.169300	14.337344
18.704069	819.266363	14.342362
18.462496	801.082981	14.347379
18.355545	805.953213	14.352397
18.550036	822.875522	14.357415
18.554431	832.824906	14.362432
18.706081	835.647847	14.367450
19.078875	827.151512	14.372467
18.429097	821.985885	14.377485
18.763788	809.781214	14.382503
18.537668	814.963483	14.387520
18.314421	812.265489	14.392538
18.641009	830.154976	14.397555
18.845794	828.201356	14.402573
18.791159	825.871571	14.407591
18.571983	827.849712	14.412608
18.790093	822.533179	14.417626
18.620191	833.226049	14.422643
18.506852	833.351085	14.427661
18.761676	826.826506	14.432679
18.264862	827.263705	14.437696
18.789957	826.333157	14.442714
18.816925	827.458799	14.447731
18.709252	826.936031	14.452749
18.995347	815.773996	14.457767
19.004933	824.529708	14.462784
18.825507	819.868346	14.467802
18.846249	826.608976	14.472819
18.468864	833.903887	14.477837
19.261516	836.945753	14.482855
19.272805	843.362822	14.487872
19.450157	832.388117	14.492890
19.325842	828.611240	14.497907
18.816601	823.130250	14.502925
19.153516	819.726519	14.507943
19.070107	820.888280	14.512960
19.009416	824.687839	14.517978
18.891564	815.892371	14.522995
18.866395	840.952774	14.528013
19.398125	841.072046	14.533031
19.215289	842.586951	14.538048
19.318598	844.019437	14.543066
19.234762	836.417835	14.548083
19.260284	842.788508	14.553101
19.536281	835.370717	14.558119
19.155452	834.808429	14.563136
19.298699	841.618351	14.568154
19.349982	839.199492	14.573171
19.363765	851.738271	14.578189
19.733826	843.583171	14.583207
19.447622	846.925553	14.588224
19.386652	830.130941	14.593242
19.220681	836.376796	14.598259
19.419922	838.034179	14.603277
19.684290	838.491716	14.608295
19.709281	845.282183	14.613312
19.794514	835.003454	14.618330
19.756119	829.253499	14.623347
19.406783	836.427282	14.628365
19.688282	822.709828	14.633383
19.368938	825.454625	14.638400
19.563806	826.667731	14.643418
19.586492	820.974539	14.648435
19.854414	840.179637	14.653453
19.256741	827.804547	14.658471
19.458296	838.079833	14.663488
19.249140	837.108975	14.668506
19.445397	844.519698	14.673523
19.454616	855.288831	14.678541
20.011731	838.615721	14.683559
19.673281	841.111038	14.688576
19.699944	842.419760	14.693594
19.610178	845.182463	14.698611
19.345194	852.238981	14.703629
19.883057	844.367015	14.708647
19.879579	849.123321	14.713664
19.649833	840.828087	14.718682
19.906761	859.372217	14.723699
19.829414	868.065748	14.728717
20.071765	865.339433	14.733735
20.191458	869.899847	14.738752
20.189934	868.824077	14.743770
20.328615	859.127134	14.748787
19.895876	851.059155	14.753805
19.940359	850.061428	14.758823
20.249818	849.439000	14.763840
19.886494	837.794256	14.768858
19.755019	850.472411	14.773875
19.878486	862.015846	14.778893
20.148971	859.641748	14.783911
20.505259	861.514517	14.788928
20.083731	864.997890	14.793946
20.286873	863.767181	14.798963
19.823671	861.071826	14.803981
20.286616	860.094150	14.808999
20.109546	863.324872	14.814016
19.956514	871.468470	14.819034
20.478095	858.559343	14.824051
20.507696	865.958154	14.829069
20.547951	859.741519	14.834087
20.500611	866.325511	14.839104
20.529489	860.640808	14.844122
20.734447	859.838995	14.849139
20.078853	859.884361	14.854157
20.362695	857.719617	14.859175
20.623023	858.995116	14.864192
20.607246	855.229736	14.869210
20.543752	852.241781	14.874227
20.490234	851.098371	14.879245
20.567362	856.817246	14.884263
20.757148	866.273894	14.889280
20.501725	865.957160	14.894298
20.469611	858.113973	14.899315
20.107951	861.515443	14.904333
20.703670	854.814705	14.909351
20.897938	867.915514	14.914368
20.297753	855.641779	14.919386
20.647815	854.369262	14.924403
20.403951	857.856529	14.929421
20.711332	859.683265	14.934439
20.677652	848.776119	14.939456
20.555456	865.331221	14.944474
20.769549	855.019795	14.949491
20.824985	857.116125	14.954509
20.769377	859.936626	14.959527
20.626468	846.124291	14.964544
20.825445	864.977242	14.969562
20.903279	871.636419	14.974579
20.762086	877.253597	14.979597
21.398154	877.249330	14.984615
21.131811	867.574418	14.989632
20.533193	863.278104	14.994650
20.877121	867.863564	14.999667
20.867763	874.763529	15.004685
21.281147	875.478725	15.009703
21.091042	877.641689	15.014720
21.196599	881.415375	15.019738
21.218701	878.385688	15.024755
21.074024	876.656881	15.029773
20.970178	882.366073	15.034791
20.993202	885.824415	15.039808
21.403476	885.495551	15.044826
21.184133	880.963461	15.049843
21.159128	882.406460	15.054861
21.425676	887.057620	15.059879
21.391954	883.070971	15.064896
21.317845	886.569682	15.069914
21.590333	885.536453	15.074931
21.235035	883.048351	15.079949
21.319854	880.649511	15.084967
21.578305	882.692145	15.089984
21.192317	884.532166	15.095002
21.192267	885.636773	15.100019
21.009024	886.896132	15.105037
21.167516	890.140883	15.110055
21.455197	887.139271	15.115072
21.305420	883.429461	15.120090
21.471845	877.859034	15.125107
21.433413	885.003364	15.130125
21.546294	878.617629	15.135143
21.468303	886.247790	15.140160
21.280077	890.206071	15.145178
21.624112	887.956214	15.150195
21.415655	900.968276	15.155213
21.378662	907.370795	15.160231
22.062798	905.036427	15.165248
21.765717	905.982159	15.170266
21.636896	898.393847	15.175283
21.452373	901.142909	15.180301
21.809249	902.270839	15.185319
22.159573	901.121351	15.190336
22.018950	910.298114	15.195354
22.241899	896.381441	15.200371
21.693215	891.351528	15.205389
21.803006	876.190198	15.210407
21.825500	877.931907	15.215424
21.584403	891.693794	15.220442
22.180552	895.466838	15.225459
22.135096	896.357614	15.230477
21.850679	896.547155	15.235495
22.169722	892.789595	15.240512
21.785615	903.045654	15.245530
22.005404	899.079490	15.250547
22.190069	897.416166	15.255565
22.175579	905.819068	15.260583
22.276069	902.635164	15.265600
22.131486	905.630468	15.270618
22.149754	902.790717	15.275635
22.074608	896.610971	15.280653
21.975875	903.417568	15.285671
22.367606	901.075079	15.290688
21.952755	897.179324	15.295706
22.218571	902.013634	15.300723
22.328100	906.392608	15.305741
22.161129	905.232145	15.310759
22.323699	895.408389	15.315776
22.190660	904.161100	15.320794
22.218252	890.151774	15.325811
21.981137	903.641659	15.330829
22.145053	899.030957	15.335847
22.163753	891.908817	15.340864
22.137771	898.937609	15.345882
22.354167	910.305665	15.350899
22.788494	916.363412	15.355917
22.700685	917.560578	15.360935
22.923259	909.093903	15.365952
22.790585	908.142690	15.370970
22.577247	903.136300	15.375987
22.635766	899.921062	15.381005
22.287014	898.012593	15.386023
22.798931	894.827747	15.391040
22.740035	899.949292	15.396058
22.481919	898.175030	15.401075
22.683878	894.400987	15.406093
22.538869	910.640954	15.411111
23.087456	906.765603	15.416128
22.555611	920.190938	15.421146
22.715056	927.086731	15.426163
23.357474	923.584923	15.431181
22.926199	918.344223	15.436199
22.931050	905.158917	15.441216
22.942496	898.441837	15.446234
22.540641	900.603059	15.451251
22.802583	908.912432	15.456269
22.679511	925.934775	15.461287
22.968916	912.440078	15.466304
22.960408	917.638988	15.471322
23.089541	915.930660	15.476339
23.265298	921.400677	15.481357
22.777953	928.728525	15.486375
22.856889	920.363103	15.491392
22.801751	926.730586	15.496410
22.749663	917.382041	15.501427
22.932493	913.405850	15.506445
23.125845	918.301938	15.511463
23.203059	917.011939	15.516480
23.320533	917.681694	15.521498
23.037723	919.568769	15.526515
23.424386	919.675916	15.531533
23.113979	924.833472	15.536551
23.398018	928.052372	15.541568
23.479162	918.903984	15.546586
23.280254	917.729558	15.551603
23.259031	917.161770	15.556621
23.243244	921.964192	15.561639
23.799671	928.053425	15.566656
23.266076	924.034144	15.571674
23.295525	929.814114	15.576691
23.768862	934.991655	15.581709
23.549659	942.568089	15.586727
23.509587	928.417793	15.591744
23.814055	931.592488	15.596762
23.628350	930.718956	15.601779
23.579804	929.243414	15.606797
23.616202	919.631789	15.611815
23.666272	927.118955	15.616832
23.699588	924.096981	15.621850
23.463601	925.711685	15.626867
23.795867	938.888889	15.631885
23.688158	941.424031	15.636903
24.161444	935.379784	15.641920
24.028649	940.011085	15.646938
23.456415	924.166969	15.651955
23.674549	924.795805	15.656973
23.762863	932.718821	15.661991
23.825495	924.056141	15.667008
23.873512	930.521171	15.672026
23.604419	935.101109	15.677043
23.921443	932.394716	15.682061
23.922704	941.347437	15.687079
23.779218	938.084750	15.692096
23.652018	933.020759	15.697114
23.832390	935.886580	15.702131
23.976599	932.657995	15.707149
23.764345	939.157240	15.712167
24.266339	940.013274	15.717184
24.529962	950.307363	15.722202
24.103026	954.760407	15.727219
24.159359	930.919606	15.732237
24.327187	940.070450	15.737255
24.114657	936.007489	15.742272
24.285654	948.007473	15.747290
24.171117	960.351717	15.752307
24.453432	955.271296	15.757325
24.143564	969.176492	15.762343
24.713006	962.489273	15.767360
24.427626	969.085118	15.772378
24.253577	958.572138	15.777395
24.643052	963.743811	15.782413
24.460977	956.463560	15.787431
24.241965	946.989514	15.792448
24.615732	954.943835	15.797466
24.455242	968.169378	15.802483
24.629376	955.733990	15.807501
24.498976	958.777586	15.812519
24.366177	963.629796	15.817536
24.680350	957.439905	15.822554
24.621303	960.084236	15.827571
24.473775	956.572872	15.832589
24.634887	961.634935	15.837607
24.614114	961.022894	15.842624
24.480792	959.440631	15.847642
24.265920	955.147662	15.852659
24.725768	952.693577	15.857677
24.678295	955.481269	15.862695
24.709097	954.283699	15.867712
24.980202	945.768427	15.872730
24.694330	954.630163	15.877747
24.833175	962.557949	15.882765
24.941539	978.244143	15.887783
25.061264	971.850997	15.892800
25.524967	960.194170	15.897818
25.075788	957.632313	15.902835
25.341161	949.471374	15.907853
25.114701	941.642631	15.912871
24.916126	948.344871	15.917888
25.350298	943.613187	15.922906
25.003015	946.447557	15.927923
25.062041	937.520350	15.932941
25.145906	944.083942	15.937959
25.009706	946.762374	15.942976
25.345488	944.365476	15.947994
25.115235	956.730890	15.953011
24.949069	947.545255	15.958029
25.273694	962.973707	15.963047
25.624999	974.832030	15.968064
25.298930	968.571408	15.973082
25.669763	974.705331	15.978099
25.472367	958.749175	15.983117
25.400413	956.011824	15.988135
25.345033	952.391442	15.993152
25.382588	954.140280	15.998170
25.592853	968.803919	16.003187
25.664735	955.317811	16.008205
25.938706	963.082550	16.013223
25.759487	956.070093	16.018240
25.336852	945.078284	16.023258
25.373399	948.843795	16.028275
25.749519	954.020699	16.033293
25.826674	962.040139	16.038311
25.828812	966.461093	16.043328
25.895968	952.811624	16.048346
25.593021	960.562047	16.053363
26.072566	957.180263	16.058381
25.869934	953.832110	16.063399
25.701949	947.430121	16.068416
25.731745	950.808528	16.073434
25.619432	954.855987	16.078451
25.800552	953.237390	16.083469
25.938990	964.119011	16.088487
26.037631	959.294400	16.093504
26.161874	958.609290	16.098522
26.177467	975.436525	16.103539
26.055402	966.723687	16.108557
26.260658	968.329654	16.113575
25.995177	968.882313	16.118592
26.066156	973.014846	16.123610
26.154647	972.464686	16.128627
26.034076	965.250594	16.133645
26.076311	960.418986	16.138663
25.985461	972.822665	16.143680
26.061862	960.983147	16.148698
25.839437	960.894799	16.153715
26.246864	960.298139	16.158733
26.266058	963.084919	16.163751
25.955636	965.058348	16.168768
25.630824	960.984461	16.173786
26.134526	982.365178	16.178803
26.329857	990.359919	16.183821
26.440308	983.283416	16.188839
26.146351	990.789459	16.193856
26.586892	985.930543	16.198874
26.406736	989.123899	16.203891
26.418546	985.313171	16.208909
26.599233	979.860410	16.213927
26.552753	986.857715	16.218944
26.968339	981.911168	16.223962
26.806295	984.565227	16.228979
26.771656	988.392322	16.233997
26.707724	984.353550	16.239015
26.354565	983.979449	16.244032
26.856178	985.611859	16.249050
26.732858	986.031933	16.254067
26.967910	988.090846	16.259085
26.743005	984.200212	16.264103
26.227854	985.583836	16.269120
26.427028	980.551066	16.274138
26.458229	994.153874	16.279155
26.724122	1004.829487	16.284173
26.959581	1000.731475	16.289191
27.096241	1008.119988	16.294208
27.148259	1005.729394	16.299226
27.374154	1011.573477	16.304243
26.979952	1005.033122	16.309261
27.148812	1010.201288	16.314279
27.203064	1009.539696	16.319296
27.276837	1010.007978	16.324314
27.284260	998.731431	16.329331
27.288892	991.753449	16.334349
27.463630	986.661367	16.339367
26.655831	981.454025	16.344384
27.145625	991.340547	16.349402
27.087549	1004.007384	16.354419
27.680192	1002.646596	16.359437
27.649349	999.309556	16.364455
27.726835	1005.173589	16.369472
27.661971	1001.930207	16.374490
27.299640	982.929167	16.379507
27.427979	979.608372	16.384525
27.262215	983.932398	16.389543
27.269223	1000.622141	16.394560
27.483304	1005.947364	16.399578
27.617706	1002.467833	16.404595
27.441016	1007.061805	16.409613
27.395105	1010.142747	16.414631
27.221443	1011.672017	16.419648
27.430985	997.656368	16.424666
27.408851	998.698150	16.429683
27.159889	1002.536527	16.434701
27.669774	1014.764654	16.439719
27.912575	1022.909806	16.444736
27.814953	1027.273726	16.449754
27.978141	1031.821098	16.454771
28.171509	1034.129499	16.459789
28.214510	1029.263040	16.464807
28.090930	1014.601822	16.469824
27.788229	1008.820378	16.474842
28.020485	995.959354	16.479859
27.786004	1003.099543	16.484877
28.313523	1010.619702	16.489895
27.801893	1017.774646	16.494912
28.166362	1016.774426	16.499930
28.230729	1024.944205	16.504947
27.942365	1026.387195	16.509965
28.134639	1018.490066	16.514983
28.078688	1030.967246	16.520000
28.308594	1024.089875	16.525018
28.172361	1019.563744	16.530035
27.932029	1027.506414	16.535053
28.627882	1027.852596	16.540071
28.475616	1030.606123	16.545088
28.210032	1026.658698	16.550106
28.419557	1029.987046	16.555123
28.419363	1035.225721	16.560141
28.377454	1023.253106	16.565159
28.202061	1026.745523	16.570176
28.364115	1020.314212	16.575194
28.086017	1024.087703	16.580211
28.284011	1022.059381	16.585229
28.676744	1026.927613	16.590247
28.406610	1024.599797	16.595264
28.621633	1019.924304	16.600282
28.574695	1014.803613	16.605299
28.612211	1019.408417	16.610317
29.012903	1020.112973	16.615335
28.661762	1022.531397	16.620352
28.961444	1021.405565	16.625370
28.653070	1031.239659	16.630387
28.686235	1029.805034	16.635405
28.924442	1040.301946	16.640423
28.595815	1047.693492	16.645440
28.929781	1041.033439	16.650458
28.989867	1037.467644	16.655475
28.877598	1047.192319	16.660493
29.166561	1046.778200	16.665511
28.893650	1044.662250	16.670528
28.996709	1049.383088	16.675546
29.081599	1047.063108	16.680563
29.123637	1044.762424	16.685581
29.143635	1044.446985	16.690599
29.237981	1052.703626	16.695616
29.123985	1050.711253	16.700634
29.070384	1050.795432	16.705651
29.160767	1049.885220	16.710669
29.431645	1040.126570	16.715687
29.013100	1051.066563	16.720704
29.391061	1045.737699	16.725722
29.394234	1040.823789	16.730739
29.264312	1044.615239	16.735757
29.125164	1042.285962	16.740775
29.191585	1043.569574	16.745792
29.386212	1056.825099	16.750810
29.761521	1063.210817	16.755827
29.652889	1069.296350	16.760845
29.596494	1061.933373	16.765863
29.569839	1063.682752	16.770880
29.761977	1072.514303	16.775898
29.761206	1068.222685	16.780915
29.604911	1068.988718	16.785933
29.808746	1064.469587	16.790951
30.081238	1070.931276	16.795968
29.810816	1067.893453	16.800986
29.662863	1054.753917	16.806003
29.991004	1058.253148	16.811021
29.866614	1048.202591	16.816039
29.768873	1051.307389	16.821056
29.812995	1064.924019	16.826074
30.391203	1056.124197	16.831091
30.028198	1059.188247	16.836109
30.255456	1053.336899	16.841127
30.275528	1043.898159	16.846144
29.948735	1033.087029	16.851162
30.030067	1026.560988	16.856179
29.810977	1043.084005	16.861197
30.302546	1047.728574	16.866215
29.891843	1060.930029	16.871232
30.162647	1070.339458	16.876250
30.399603	1063.470442	16.881267
30.223165	1062.213614	16.886285
30.120407	1057.189962	16.891303
30.316821	1061.530201	16.896320
30.150726	1059.886760	16.901338
30.223253	1049.174391	16.906355
30.223542	1056.009810	16.911373
30.328154	1050.786618	16.916391
30.225364	1055.870862	16.921408
29.946523	1059.414106	16.926426
30.272800	1062.796866	16.931443
30.245556	1077.475484	16.936461
30.620706	1079.910221	16.941479
31.128751	1078.742477	16.946496
30.760557	1082.353286	16.951514
30.853549	1071.950138	16.956531
30.781769	1073.990562	16.961549
30.598335	1077.108706	16.966567
30.526993	1082.330070	16.971584
30.559619	1081.974796	16.976602
31.048105	1070.137316	16.981619
30.756758	1077.535694	16.986637
31.154212	1079.168550	16.991655
30.900897	1083.155943	16.996672
31.078649	1079.735919	17.001690
30.995581	1087.467940	17.006707
30.530682	1080.209583	17.011725
31.049438	1082.621961	17.016743
31.027906	1079.251900	17.021760
30.981251	1081.897475	17.026778
30.864426	1074.023201	17.031795
30.895758	1079.032921	17.036813
30.993292	1078.777992	17.041831
31.287333	1096.420356	17.046848
31.189311	1100.298368	17.051866
31.044180	1099.462691	17.056883
31.001679	1111.107867	17.061901
31.273994	1097.413722	17.066919
31.387148	1097.329928	17.071936
31.172841	1101.080880	17.076954
31.017246	1105.359172	17.081971
31.388064	1100.861370	17.086989
31.398368	1102.412497	17.092007
31.494199	1104.496256	17.097024
31.261428	1115.259042	17.102042
31.728749	1115.199000	17.107059
31.801155	1129.729604	17.112077
31.800971	1121.486858	17.117095
31.977177	1108.337837	17.122112
31.816125	1106.649426	17.127130
31.698727	1099.706181	17.132147
31.693502	1112.014576	17.137165
31.555426	1120.146492	17.142183
32.097901	1125.553163	17.147200
31.793151	1118.086821	17.152218
32.563131	1117.007680	17.157235
31.968503	1109.788443	17.162253
31.607432	1096.158201	17.167271
31.928241	1110.694295	17.172288
32.026298	1111.960364	17.177306
32.180694	1115.508749	17.182323
32.204555	1118.364254	17.187341
32.262372	1115.919094	17.192359
32.720592	1116.756707	17.197376
32.261340	1113.366429	17.202394
32.443382	1102.223572	17.207411
32.008861	1101.511846	17.212429
32.005990	1108.044823	17.217447
32.148514	1109.480691	17.222464
32.138813	1123.689562	17.227482
32.406479	1116.304510	17.232499
32.447483	1120.347071	17.237517
32.357871	1119.373363	17.242535
32.384922	1112.003684	17.247552
32.373212	1115.486413	17.252570
32.158685	1113.478128	17.257587
32.312227	1118.733916	17.262605
32.503040	1119.537425	17.267623
32.523780	1113.251157	17.272640
32.443892	1119.751949	17.277658
32.820902	1120.397081	17.282675
32.553435	1120.845913	17.287693
32.908732	1135.215713	17.292711
33.435972	1127.509378	17.297728
32.857414	1129.385718	17.302746
33.201549	1116.292595	17.307763
33.110748	1114.489105	17.312781
32.840849	1112.748214	17.317799
33.215936	1107.839496	17.322816
32.874038	1107.141750	17.327834
32.909558	1100.357731	17.332851
33.173817	1109.831315	17.337869
32.904793	1100.570098	17.342887
32.941087	1090.740649	17.347904
32.804471	1114.540706	17.352922
32.925214	1125.564035	17.357939
32.904104	1131.607560	17.362957
32.700077	1132.958533	17.367975
33.238150	1129.867403	17.372992
33.189352	1135.943642	17.378010
33.287089	1134.858713	17.383027
33.256778	1131.524722	17.388045
33.343722	1130.656066	17.393063
33.732124	1133.095059	17.398080
33.489139	1134.792921	17.403098
33.299775	1126.901515	17.408115
33.545215	1145.807491	17.413133
33.784767	1159.182328	17.418151
33.889032	1140.127408	17.423168
33.675666	1146.049394	17.428186
33.920166	1137.989448	17.433203
33.183076	1137.469995	17.438221
33.826345	1148.572927	17.443239
33.851616	1145.618440	17.448256
33.807026	1155.029683	17.453274
34.157559	1155.641069	17.458291
34.002975	1144.859863	17.463309
33.927121	1150.555316	17.468327
34.201289	1143.207109	17.473344
34.029303	1147.996043	17.478362
34.189478	1137.639200	17.483379
34.048394	1141.738518	17.488397
33.853085	1145.950421	17.493415
34.417916	1146.831396	17.498432
34.294059	1154.727586	17.503450
34.268666	1151.601107	17.508467
34.513792	1141.436161	17.513485
33.932217	1138.440459	17.518503
34.012342	1131.125625	17.523520
34.098004	1147.781169	17.528538
34.205074	1145.978426	17.533555
34.450329	1150.942237	17.538573
34.303893	1151.214437	17.543591
34.082879	1144.438784	17.548608
33.881526	1148.345518	17.553626
34.104016	1147.979616	17.558643
34.255914	1161.440685	17.563661
34.476470	1167.509712	17.568679
34.451581	1164.443111	17.573696
34.596208	1171.079377	17.578714
34.250895	1178.274761	17.583731
34.710160	1172.545040	17.588749
34.792861	1181.873363	17.593767
34.872890	1160.647862	17.598784
34.627907	1167.833933	17.603802
34.801104	1172.247240	17.608819
34.735488	1168.366478	17.613837
34.588161	1177.257246	17.618855
34.998375	1163.216535	17.623872
35.287911	1167.229878	17.628890
35.107835	1169.820501	17.633907
34.979761	1172.472455	17.638925
34.880556	1169.313284	17.643943
35.196002	1170.012184	17.648960
35.093791	1173.505859	17.653978
35.731353	1171.462730	17.658995
35.404750	1171.576791	17.664013
35.642974	1167.099617	17.669031
35.536613	1162.010225	17.674048
35.299413	1169.655828	17.679066
34.715496	1171.766534	17.684083
35.480786	1161.072469	17.689101
35.537540	1177.423276	17.694119
35.448726	1178.907792	17.699136
35.483253	1184.794351	17.704154
35.551980	1184.676448	17.709171
35.849355	1195.666009	17.714189
35.873515	1195.788573	17.719207
35.710870	1182.960497	17.724224
35.234196	1178.073923	17.729242
35.641253	1187.657858	17.734259
35.663944	1189.437436	17.739277
35.491192	1191.695565	17.744295
35.959525	1200.742952	17.749312
35.773893	1206.111534	17.754330
35.957366	1196.385342	17.759347
35.980076	1187.441574	17.764365
35.772488	1189.711437	17.769383
36.157109	1179.849796	17.774400
36.001618	1196.306249	17.779418
36.204740	1190.660583	17.784435
35.986358	1194.431124	17.789453
36.128238	1195.239100	17.794471
36.038358	1186.675776	17.799488
35.778293	1196.884288	17.804506
36.174955	1201.830851	17.809523
36.857572	1206.057556	17.814541
36.326893	1195.066634	17.819559
36.285681	1194.729165	17.824576
36.324275	1197.610791	17.829594
36.377478	1210.591807	17.834611
36.302960	1210.622438	17.839629
36.051061	1216.250647	17.844647
36.365311	1207.807428	17.849664
36.724855	1210.919951	17.854682
36.848935	1209.505870	17.859699
37.014893	1208.315642	17.864717
37.016325	1216.713057	17.869735
36.798400	1202.044283	17.874752
36.917315	1202.840055	17.879770
36.811969	1201.916129	17.884787
37.032537	1206.896422	17.889805
36.443961	1213.189271	17.894823
36.488001	1214.580522	17.899840
36.969101	1208.569681	17.904858
36.874801	1211.623478	17.909875
36.763560	1206.676844	17.914893
36.464975	1216.569475	17.919911
36.486848	1209.727579	17.924928
36.639956	1222.910797	17.929946
36.682620	1223.847830	17.934963
37.055049	1229.612366	17.939981
37.333568	1229.382906	17.944999
37.379091	1230.158548	17.950016
37.517236	1230.746202	17.955034
37.065978	1232.927777	17.960051
37.409355	1224.356939	17.965069
37.285144	1229.110054	17.970087
37.357653	1229.120950	17.975104
36.941089	1227.090459	17.980122
37.456851	1234.243318	17.985139
37.625619	1244.741694	17.990157
37.467313	1244.602336	17.995175
37.876151	1244.863823	18.000192
37.790810	1242.393598	18.005210
37.748690	1236.180190	18.010227
38.192225	1243.334830	18.015245
37.782204	1230.138138	18.020263
38.202399	1222.218056	18.025280
37.883112	1215.599687	18.030298
37.675981	1222.079302	18.035315
37.872933	1224.718527	18.040333
37.783203	1234.016920	18.045351
37.876333	1236.593418	18.050368
38.261444	1233.238909	18.055386
38.032461	1243.461543	18.060403
38.468728	1241.648562	18.065421
38.215426	1244.521994	18.070439
38.020103	1235.504851	18.075456
38.152647	1244.730773	18.080474
37.898428	1247.086799	18.085491
38.207793	1240.727146	18.090509
38.455483	1247.454691	18.095527
38.364727	1237.007472	18.100544
38.282143	1243.126878	18.105562
38.502419	1239.293106	18.110579
38.405716	1239.459735	18.115597
38.298925	1248.262177	18.120615
38.142608	1237.733647	18.125632
38.594893	1247.692424	18.130650
38.409993	1257.788283	18.135667
38.723406	1263.205415	18.140685
38.435367	1260.760435	18.145703
38.888816	1258.562925	18.150720
38.740447	1271.670043	18.155738
38.594633	1259.151714	18.160755
38.943555	1257.661598	18.165773
39.056602	1270.409278	18.170791
38.917172	1268.629123	18.175808
39.102369	1256.744066	18.180826
38.542342	1259.346522	18.185843
38.774421	1262.037088	18.190861
38.766931	1265.841081	18.195879
38.788741	1277.930787	18.200896
39.445693	1279.015177	18.205914
39.239188	1285.949152	18.210931
39.675522	1285.717210	18.215949
39.423509	1287.930887	18.220967
39.629828	1284.020384	18.225984
39.669942	1287.495078	18.231002
39.490048	1269.626660	18.236019
39.430690	1263.911385	18.241037
39.507329	1275.752713	18.246055
39.527744	1267.765468	18.251072
39.669507	1273.300846	18.256090
39.544777	1278.874561	18.261107
39.770217	1273.263265	18.266125
39.819672	1277.288767	18.271143
39.813658	1277.498080	18.276160
40.002375	1266.694908	18.281178
39.532076	1269.766231	18.286195
39.658905	1272.899218	18.291213
39.626162	1281.907898	18.296231
39.845201	1287.816256	18.301248
39.880522	1278.652728	18.306266
39.737165	1285.794621	18.311283
40.028078	1281.725780	18.316301
39.761536	1285.431255	18.321319
40.115406	1287.724168	18.326336
39.929746	1286.730690	18.331354
40.106445	1280.088723	18.336371
39.997537	1275.602453	18.341389
40.111006	1280.883463	18.346407
40.273404	1303.485351	18.351424
40.622575	1299.151816	18.356442
39.738666	1307.579820	18.361459
40.136096	1306.306209	18.366477
40.162853	1304.869404	18.371495
40.326834	1299.731571	18.376512
40.313757	1304.666218	18.381530
40.296227	1306.540433	18.386547
40.231019	1308.248501	18.391565
40.671256	1316.883756	18.396583
40.923222	1317.630416	18.401600
40.848630	1322.293779	18.406618
40.870575	1320.649439	18.411635
41.052712	1316.171494	18.416653
41.015321	1323.789209	18.421671
41.193812	1321.473555	18.426688
41.273433	1312.820664	18.431706
41.230674	1313.225047	18.436723
41.228777	1296.439731	18.441741
41.190522	1288.477390	18.446759
40.649246	1296.517528	18.451776
40.987010	1305.597921	18.456794
40.920518	1319.276149	18.461811
41.193385	1318.608910	18.466829
41.398659	1316.364827	18.471847
41.495951	1317.672055	18.476864
41.302226	1316.777662	18.481882
41.748155	1312.750951	18.486899
41.616594	1313.393222	18.491917
41.583492	1316.494313	18.496935
41.354055	1311.376705	18.501952
41.698312	1311.316889	18.506970
41.330126	1315.085532	18.511987
41.393728	1310.903753	18.517005
41.273647	1306.109947	18.522023
41.368366	1317.478273	18.527040
41.873177	1319.630924	18.532058
42.136091	1333.743870	18.537075
41.989443	1328.872142	18.542093
42.086908	1318.723774	18.547111
41.540503	1313.510348	18.552128
41.829085	1319.026038	18.557146
42.023046	1337.056607	18.562163
41.961369	1334.267104	18.567181
41.745589	1334.316574	18.572199
41.954756	1335.612697	18.577216
42.208424	1333.597762	18.582234
42.318528	1338.560577	18.587251
42.134468	1327.521917	18.592269
42.429978	1329.653508	18.597287
42.035284	1330.873235	18.602304
42.244907	1322.282150	18.607322
42.448540	1329.947548	18.612339
41.920358	1326.324963	18.617357
42.265010	1337.231511	18.622375
42.711441	1350.369155	18.627392
43.134000	1352.701875	18.632410
42.596830	1363.417530	18.637427
42.615445	1353.477079	18.642445
42.828245	1351.569491	18.647463
42.639551	1363.474279	18.652480
42.958333	1353.682754	18.657498
42.983842	1352.817341	18.662515
42.833640	1362.106281	18.667533
43.191851	1345.684574	18.672551
42.805323	1358.563748	18.677568
43.024188	1357.560932	18.682586
42.884560	1356.812749	18.687603
43.043796	1353.263012	18.692621
43.281307	1351.512523	18.697639
42.740114	1360.871805	18.702656
42.933678	1349.354614	18.707674
42.734219	1355.009416	18.712691
43.073549	1368.870651	18.717709
43.466207	1368.607639	18.722727
43.457810	1366.958551	18.727744
43.287387	1362.409253	18.732762
43.652947	1364.627772	18.737779
43.806158	1369.710116	18.742797
43.919955	1365.791910	18.747815
43.858102	1366.559030	18.752832
43.887796	1366.513476	18.757850
44.183947	1361.812639	18.762867
43.616284	1352.518892	18.767885
43.662689	1340.421860	18.772903
43.879553	1354.961714	18.777920
44.049858	1360.047706	18.782938
44.096138	1360.596018	18.787955
43.836221	1355.741919	18.792973
43.780136	1355.444632	18.797991
43.857441	1363.606241	18.803008
44.031319	1362.613585	18.808026
44.371104	1355.696889	18.813043
44.035763	1360.009539	18.818061
44.287414	1351.563375	18.823079
43.984870	1353.109584	18.828096
44.263096	1357.973645	18.833114
44.414591	1357.940685	18.838131
44.331841	1359.897643	18.843149
44.775645	1352.870078	18.848167
44.104659	1362.808148	18.853184
44.552332	1357.443091	18.858202
44.759327	1358.815294	18.863219
44.838163	1358.146706	18.868237
44.911560	1355.320390	18.873255
44.300303	1355.851156	18.878272
44.386572	1363.181391	18.883290
44.597711	1380.414066	18.888307
44.836900	1375.097243	18.893325
45.042500	1375.412466	18.898343
44.612995	1380.853785	18.903360
44.953341	1379.011542	18.908378
44.806999	1374.379596	18.913395
44.912065	1379.163326	18.918413
45.498420	1373.603103	18.923431
44.763424	1379.918807	18.928448
44.694733	1374.915008	18.933466
44.467050	1384.231802	18.938483
45.045310	1398.065327	18.943501
45.307711	1398.040346	18.948519
45.168929	1419.316493	18.953536
45.396584	1406.294943	18.958554
45.338684	1399.796755	18.963571
45.332868	1391.917679	18.968589
45.713640	1390.646656	18.973607
45.300606	1406.095670	18.978624
45.337155	1394.476664	18.983642
45.603128	1402.053492	18.988659
45.809140	1416.506723	18.993677
46.027760	1417.283826	18.998695
46.107787	1422.996121	19.003712
46.126632	1423.065866	19.008730
46.133620	1395.776500	19.013747
45.877053	1390.628379	19.018765
46.000430	1389.990724	19.023783
46.194073	1398.623387	19.028800
45.642120	1397.005277	19.033818
46.203015	1410.314493	19.038835
46.163416	1416.364149	19.043853
46.438838	1414.875997	19.048871
46.332548	1423.094620	19.053888
46.528639	1412.728870	19.058906
46.854888	1423.916049	19.063923
46.453931	1427.812895	19.068941
46.360348	1417.242933	19.073959
46.586005	1419.760954	19.078976
46.638805	1414.750852	19.083994
46.810814	1414.724166	19.089011
46.332237	1420.640197	19.094029
46.709755	1404.723518	19.099047
46.464515	1409.830041	19.104064
46.625878	1418.912710	19.109082
46.640784	1418.314034	19.114099
46.659693	1420.179431	19.119117
47.087731	1412.425303	19.124135
46.839759	1415.515684	19.129152
46.668836	1411.316748	19.134170
47.205171	1425.885816	19.139187
46.686551	1434.739846	19.144205
46.789807	1432.461139	19.149223
46.991973	1435.374141	19.154240
47.105843	1441.784922	19.159258
47.315583	1434.039526	19.164275
46.897662	1443.868811	19.169293
46.918230	1444.553673	19.174311
47.095103	1449.758590	19.179328
47.157156	1464.067015	19.184346
47.350969	1459.754475	19.189363
47.473019	1464.977399	19.194381
47.439197	1466.951997	19.199399
47.728968	1466.471471	19.204416
47.769977	1453.415830	19.209434
47.938501	1463.138040	19.214451
47.580462	1461.120500	19.219469
47.833674	1459.178207	19.224487
48.017148	1470.201450	19.229504
48.201049	1476.525600	19.234522
47.978220	1457.533890	19.239539
47.971025	1469.082284	19.244557
48.504221	1478.823465	19.249575
48.340406	1479.426582	19.254592
48.061828	1472.561936	19.259610
48.389863	1474.625364	19.264627
48.459263	1479.581932	19.269645
48.447552	1469.175919	19.274663
48.245605	1463.340769	19.279680
48.699639	1471.131345	19.284698
48.616781	1460.051599	19.289715
48.430435	1468.532018	19.294733
48.504525	1464.323324	19.299751
48.713852	1476.639592	19.304768
48.757578	1486.144558	19.309786
48.782866	1476.748959	19.314803
48.696638	1485.873367	19.319821
48.841513	1487.119550	19.324839
48.816361	1487.779974	19.329856
48.713579	1480.648110	19.334874
48.919246	1481.266285	19.339891
48.812824	1487.395798	19.344909
48.684117	1478.046265	19.349927
48.678760	1479.934381	19.354944
48.803916	1478.520112	19.359962
49.194106	1485.140353	19.364979
49.071138	1508.121450	19.369997
49.161358	1503.279068	19.375015
49.392244	1506.459012	19.380032
49.309033	1504.846806	19.385050
49.435821	1501.024378	19.390067
48.922996	1508.747754	19.395085
49.269404	1495.654000	19.400103
48.978675	1494.496987	19.405120
49.296923	1510.794763	19.410138
49.700400	1506.869294	19.415155
49.449619	1514.715976	19.420173
49.734414	1520.775122	19.425191
49.948243	1515.970296	19.430208
49.744569	1519.782797	19.435226
50.001233	1522.482199	19.440243
49.857155	1520.794261	19.445261
50.056782	1519.175888	19.450279
50.153843	1511.766741	19.455296
50.157221	1522.041721	19.460314
50.191064	1517.548943	19.465331
49.848312	1512.941230	19.470349
49.898592	1538.615724	19.475367
50.268561	1544.222954	19.480384
50.142586	1552.274286	19.485402
50.519649	1542.839661	19.490419
50.508600	1550.128320	19.495437
50.576310	1548.849223	19.500455
50.453705	1543.961070	19.505472
50.550918	1543.513679	19.510490
51.203169	1541.685975	19.515507
50.933672	1538.234511	19.520525
50.696883	1543.737393	19.525543
51.045370	1529.911135	19.530560
50.439279	1541.442366	19.535578
51.212737	1534.410743	19.540595
50.722272	1538.435159	19.545613
50.663142	1539.949797	19.550631
50.754868	1548.125024	19.555648
50.761269	1560.261503	19.560666
50.907494	1559.026986	19.565683
51.245440	1564.143741	19.570701
51.089547	1566.635980	19.575719
51.437783	1563.356581	19.580736
51.375842	1572.628733	19.585754
51.455186	1554.921640	19.590771
51.543223	1556.372340	19.595789
51.449561	1558.135356	19.600807
51.650475	1562.497108	19.605824
51.629389	1558.230626	19.610842
51.743884	1571.303348	19.615859
51.834620	1582.741893	19.620877
52.378884	1577.421694	19.625895
52.124398	1566.384383	19.630912
51.630077	1559.310292	19.635930
52.007077	1550.648855	19.640947
51.875729	1555.766090	19.645965
51.772176	1563.208014	19.650983
52.222761	1572.785381	19.656000
51.791343	1583.087065	19.661018
52.018943	1580.022108	19.666035
52.058223	1586.239424	19.671053
52.222421	1579.618227	19.676071
52.471079	1583.164653	19.681088
52.258873	1584.374919	19.686106
52.733567	1580.356294	19.691123
52.602405	1579.758263	19.696141
52.494865	1580.213764	19.701159
52.674857	1574.489527	19.706176
52.363263	1578.293596	19.711194
52.183946	1572.710510	19.716211
52.555691	1599.136627	19.721229
52.551648	1603.097947	19.726247
52.907928	1591.429032	19.731264
52.796374	1608.459701	19.736282
53.158125	1604.442876	19.741299
53.003220	1604.101009	19.746317
53.065772	1603.308713	19.751335
53.415927	1603.036537	19.756352
53.255598	1602.215825	19.761370
53.460039	1593.328766	19.766387
53.167908	1602.015070	19.771405
52.930731	1598.672173	19.776423
53.217746	1592.820812	19.781440
53.338815	1604.289362	19.786458
53.766025	1609.761468	19.791475
53.456831	1620.088325	19.796493
53.491804	1627.439279	19.801511
53.808139	1617.234573	19.806528
53.773347	1614.734335	19.811546
53.658956	1625.043489	19.816563
53.942517	1616.488089	19.821581
53.727545	1623.013251	19.826599
53.844413	1609.759489	19.831616
53.498712	1615.525506	19.836634
53.903880	1619.776574	19.841651
54.050642	1615.332464	19.846669
54.129443	1631.412007	19.851687
54.487504	1632.640788	19.856704
54.624222	1628.627436	19.861722
54.312132	1619.312692	19.866739
54.502680	1627.955416	19.871757
54.486316	1628.134786	19.876775
54.726195	1635.352853	19.881792
54.648317	1635.466061	19.886810
54.661286	1624.210344	19.891827
54.836153	1626.389158	19.896845
54.135653	1627.325152	19.901863
54.502801	1627.690969	19.906880
54.190586	1632.517644	19.911898
54.753549	1628.920773	19.916915
54.875938	1630.912095	19.921933
54.752574	1639.076670	19.926951
55.050361	1627.716645	19.931968
54.725306	1654.803608	19.936986
55.062201	1655.199382	19.942003
55.456359	1656.473039	19.947021
55.255695	1650.192650	19.952039
55.378319	1656.630549	19.957056
55.578771	1654.870021	19.962074
55.823452	1655.264374	19.967091
55.672715	1647.224709	19.972109
55.132676	1650.572046	19.977127
55.732886	1638.309691	19.982144
55.704679	1649.138781	19.987162
55.652730	1651.674809	19.992179
55.854951	1647.231524	19.997197
55.560582	1650.770990	20.002215
55.948428	1657.189686	20.007232
55.967450	1649.000511	20.012250
55.782817	1651.263703	20.017267
55.886382	1646.665361	20.022285
55.653346	1648.497424	20.027303
55.990958	1653.017799	20.032320
55.838430	1651.763517	20.037338
56.098407	1654.052162	20.042355
56.012011	1657.095337	20.047373
56.432038	1670.104782	20.052391
56.344745	1671.308230	20.057408
56.365842	1667.518001	20.062426
56.218141	1675.629577	20.067443
56.274743	1669.643648	20.072461
56.298745	1675.857063	20.077479
56.305944	1673.362902	20.082496
56.799059	1686.591359	20.087514
57.118523	1688.088090	20.092531
57.270790	1684.608802	20.097549
56.831370	1679.050400	20.102567
57.159478	1672.450987	20.107584
57.164733	1662.730198	20.112602
57.151003	1670.893498	20.117619
57.221234	1663.081359	20.122637
57.100636	1668.061250	20.127655
57.636612	1672.721163	20.132672
57.700373	1667.377917	20.137690
56.956986	1666.660605	20.142707
57.331970	1677.010363	20.147725
57.052634	1684.672214	20.152743
57.555703	1683.552547	20.157760
57.632802	1675.041887	20.162778
57.601584	1688.901102	20.167795
57.381299	1675.696628	20.172813
57.257456	1678.619402	20.177831
57.835201	1684.800255	20.182848
57.520713	1695.017524	20.187866
57.808453	1703.332721	20.192883
58.047976	1704.646237	20.197901
57.887330	1714.495575	20.202919
58.096763	1717.432740	20.207936
58.317755	1717.127022	20.212954
57.730896	1713.229463	20.217971
58.040771	1714.459441	20.222989
57.841430	1710.018700	20.228007
58.567792	1725.003406	20.233024
58.534214	1731.399377	20.238042
58.429297	1734.723166	20.243059
58.729436	1727.433794	20.248077
58.447570	1732.883790	20.253095
58.565528	1731.773586	20.258112
58.658213	1729.919375	20.263130
58.657539	1721.799507	20.268147
59.093317	1716.142700	20.273165
58.799317	1728.335531	20.278183
59.062420	1723.737578	20.283200
59.112615	1723.515258	20.288218
59.018041	1729.447345	20.293235
59.314522	1725.200808	20.298253
59.116333	1722.725995	20.303271
59.131555	1723.632612	20.308288
59.294420	1722.897278	20.313306
59.466937	1722.091011	20.318323
59.279427	1723.903370	20.323341
59.590268	1730.472940	20.328359
59.513379	1731.381275	20.333376
59.546339	1738.060386	20.338394
59.397988	1748.750448	20.343411
59.740502	1740.274175	20.348429
59.522000	1743.161203	20.353447
59.700622	1748.097685	20.358464
59.653058	1745.066074	20.363482
59.472182	1749.212753	20.368499
59.841812	1741.855750	20.373517
60.047426	1757.991404	20.378535
60.495969	1759.938272	20.383552
60.475931	1763.618089	20.388570
60.239481	1764.144159	20.393587
60.584827	1764.112577	20.398605
60.476927	1755.876841	20.403623
60.099500	1759.460818	20.408640
60.446559	1761.344589	20.413658
60.541013	1762.579707	20.418675
60.677910	1759.711882	20.423693
60.591236	1768.647151	20.428711
60.514581	1769.088381	20.433728
60.788966	1768.218914	20.438746
60.237851	1769.112721	20.443763
60.607073	1766.637923	20.448781
60.666663	1788.445371	20.453799
61.028867	1789.534660	20.458816
61.273642	1796.379635	20.463834
61.213290	1789.859595	20.468851
61.098143	1785.001773	20.473869
61.225216	1792.164881	20.478887
61.126981	1791.312402	20.483904
61.356646	1788.414350	20.488922
61.261714	1792.494007	20.493939
61.558084	1791.469634	20.498957
61.464307	1797.300631	20.503975
61.564943	1804.123868	20.508992
61.746516	1809.785762	20.514010
62.022926	1807.861911	20.519027
62.123847	1811.122107	20.524045
61.971416	1810.947114	20.529063
62.180805	1806.288073	20.534080
62.491489	1810.402415	20.539098
62.232615	1805.121984	20.544115
62.154185	1808.470066	20.549133
62.453072	1807.328532	20.554151
62.344482	1810.299447	20.559168
62.653753	1798.435740	20.564186
62.767104	1806.544601	20.569203
62.710056	1797.474085	20.574221
62.346873	1787.949451	20.579239
62.159008	1794.527261	20.584256
62.403647	1803.571914	20.589274
62.395053	1802.102703	20.594291
62.688875	1789.932129	20.599309
62.290951	1798.171084	20.604327
62.306490	1800.368414	20.609344
62.846859	1811.017557	20.614362
62.656217	1822.506376	20.619379
62.540771	1826.368323	20.624397
63.065871	1827.804647	20.629415
63.264042	1813.310433	20.634432
63.302516	1815.160202	20.639450
63.125045	1823.601537	20.644467
63.097739	1824.079267	20.649485
63.149308	1837.780537	20.654503
63.213495	1839.922959	20.659520
63.547078	1836.286019	20.664538
63.197033	1845.148720	20.669555
63.543906	1839.938074	20.674573
63.357621	1837.795916	20.679591
63.740721	1850.533525	20.684608
64.106038	1858.445385	20.689626
64.286091	1866.512330	20.694643
64.205885	1845.841152	20.699661
64.344921	1839.981192	20.704679
64.163570	1836.733703	20.709696
64.386943	1828.045557	20.714714
64.299378	1833.417993	20.719731
64.400095	1842.434580	20.724749
64.784971	1845.852550	20.729767
64.422522	1845.110634	20.734784
64.427799	1840.262450	20.739802
63.950986	1851.966262	20.744819
64.381972	1849.933131	20.749837
64.792367	1851.469369	20.754855
64.776240	1850.960720	20.759872
65.043439	1851.010734	20.764890
64.518058	1849.782930	20.769907
64.808690	1851.265230	20.774925
65.067202	1862.491634	20.779943
65.065321	1876.021369	20.784960
65.457566	1880.306072	20.789978
65.506163	1884.991428	20.794995
65.731019	1879.326383	20.800013
65.662167	1860.950918	20.805031
65.305119	1852.394155	20.810048
65.723715	1863.179058	20.815066
65.517487	1871.426070	20.820083
65.539335	1868.058573	20.825101
65.589291	1873.447481	20.830119
65.486444	1875.186711	20.835136
66.174732	1859.517897	20.840154
65.827008	1871.637138	20.845171
65.761388	1875.649132	20.850189
65.993589	1871.750251	20.855207
65.425616	1874.915780	20.860224
65.914169	1872.949425	20.865242
66.013561	1883.761947	20.870259
66.323200	1892.544053	20.875277
66.230994	1893.306453	20.880295
66.506434	1899.960496	20.885312
66.669343	1892.736605	20.890330
66.318996	1890.222341	20.895347
66.551639	1893.563033	20.900365
66.712541	1894.841465	20.905383
66.770742	1892.929487	20.910400
66.860992	1892.959713	20.915418
66.636027	1890.378589	20.920435
66.683384	1909.085835	20.925453
67.153420	1919.796489	20.930471
66.650831	1919.136351	20.935488
66.876231	1913.026227	20.940506
66.839254	1919.593214	20.945523
67.121717	1913.057626	20.950541
67.306296	1902.889051	20.955559
67.283720	1926.176957	20.960576
67.567074	1934.316214	20.965594
67.837666	1938.701925	20.970611
67.685145	1934.424257	20.975629
67.882187	1924.761832	20.980647
67.904181	1933.926425	20.985664
67.677892	1925.440791	20.990682
68.073454	1933.360599	20.995699
67.933041	1923.245768	21.000717
68.272630	1908.896722	21.005735
68.134730	1922.394019	21.010752
68.470254	1917.456526	21.015770
68.221837	1917.318567	21.020787
68.556938	1924.982689	21.025805
68.872445	1918.618685	21.030823
67.766154	1911.835399	21.035840
68.068102	1912.924609	21.040858
67.977244	1918.468003	21.045875
68.131731	1926.381160	21.050893
68.254027	1932.421564	21.055911
68.289594	1938.163038	21.060928
68.463864	1941.348720	21.065946
68.747742	1950.153801	21.070963
68.843612	1950.700722	21.075981
68.986021	1944.941192	21.080999
68.866315	1955.390224	21.086016
69.178084	1953.511347	21.091034
69.105276	1966.768161	21.096051
68.996282	1979.516204	21.101069
69.294928	1970.756307	21.106087
69.366744	1978.590837	21.111104
69.725134	1972.807138	21.116122
69.698769	1975.888359	21.121139
69.184796	1978.963445	21.126157
69.449342	1968.728732	21.131175
69.358840	1979.971679	21.136192
69.525654	1978.834918	21.141210
69.707609	1985.885414	21.146227
69.782469	1990.197466	21.151245
69.877349	1990.586747	21.156263
69.587733	1990.988552	21.161280
70.086115	2002.086177	21.166298
70.408906	2017.279136	21.171315
70.161983	2014.363728	21.176333
70.460997	2015.342944	21.181351
70.431851	2018.001711	21.186368
70.525851	2019.085434	21.191386
70.873766	2012.883615	21.196403
70.598667	2018.443101	21.201421
70.702894	2003.347954	21.206439
70.677675	2010.121435	21.211456
70.751012	2003.801417	21.216474
70.943345	2012.967934	21.221491
71.160326	2029.263016	21.226509
71.551654	2022.795648	21.231527
71.291166	2029.482685	21.236544
71.586826	2038.456396	21.241562
71.309865	2027.220318	21.246579
71.555253	2025.386484	21.251597
71.834795	2024.705558	21.256615
71.724487	2034.736591	21.261632
71.456897	2029.122922	21.266650
71.508478	2032.119431	21.271667
71.458462	2028.002513	21.276685
71.869905	2017.214706	21.281703
71.786666	2022.264621	21.286720
72.045530	2016.348075	21.291738
71.878425	2025.201317	21.296755
71.802343	2026.623957	21.301773
72.111212	2027.560613	21.306791
72.331796	2046.269435	21.311808
72.614276	2050.404005	21.316826
72.782131	2042.914185	21.321843
72.415298	2041.507042	21.326861
72.634289	2036.044840	21.331879
72.630847	2043.291488	21.336896
72.414068	2045.910043	21.341914
72.645155	2040.622688	21.346931
72.881663	2040.522842	21.351949
72.866916	2038.319237	21.356967
72.516962	2043.120338	21.361984
72.829117	2042.617378	21.367002
72.852199	2034.219103	21.372019
72.651162	2049.809240	21.377037
73.477436	2056.371268	21.382055
73.099548	2062.107724	21.387072
73.107764	2054.374500	21.392090
73.089715	2068.822119	21.397107
73.043824	2065.430416	21.402125
73.361154	2075.738888	21.407143
73.439553	2077.462542	21.412160
73.782110	2087.972230	21.417178
73.561144	2098.749549	21.422195
73.674243	2096.901589	21.427213
73.892093	2086.244871	21.432231
73.904025	2089.673614	21.437248
74.030116	2092.620661	21.442266
74.250238	2106.488407	21.447283
74.116705	2115.304907	21.452301
74.430833	2109.578551	21.457319
74.378984	2122.163157	21.462336
74.303710	2108.074212	21.467354
74.491051	2110.348978	21.472371
74.261143	2116.993415	21.477389
74.773472	2110.907982	21.482407
74.841866	2114.476268	21.487424
75.301747	2121.385712	21.492442
75.276321	2124.940205	21.497459
74.963784	2116.022919	21.502477
75.074809	2107.853925	21.507495
75.270838	2131.865490	21.512512
75.493344	2127.074930	21.517530
75.681231	2125.265818	21.522547
75.514609	2122.246367	21.527565
75.729919	2112.397952	21.532583
76.005785	2112.670690	21.537600
75.837334	2117.156361	21.542618
75.774425	2110.396750	21.547635
76.093908	2122.393344	21.552653
76.161603	2115.177877	21.557671
76.021117	2119.087968	21.562688
75.901938	2125.055576	21.567706
76.312869	2115.738460	21.572723
76.347921	2118.238917	21.577741
76.264039	2110.037149	21.582759
76.334609	2111.604229	21.587776
76.275436	2117.890710	21.592794
76.394235	2113.409803	21.597811
76.217037	2114.229628	21.602829
76.237220	2104.790310	21.607847
76.366629	2111.363022	21.612864
76.520728	2126.263588	21.617882
76.468880	2121.105472	21.622899
76.347349	2137.118827	21.627917
76.502254	2130.530433	21.632935
76.802141	2144.104910	21.637952
76.708442	2158.529664	21.642970
77.135005	2150.437762	21.647987
76.985474	2156.406949	21.653005
77.152328	2154.563238	21.658023
77.052919	2159.461068	21.663040
77.453116	2174.821999	21.668058
77.631274	2177.085579	21.673075
78.093768	2177.714289	21.678093
78.221626	2177.773376	21.683111
78.402209	2165.143629	21.688128
78.206350	2166.518654	21.693146
78.082618	2150.811904	21.698163
78.013060	2156.920126	21.703181
77.744526	2156.384491	21.708199
77.973588	2165.204525	21.713216
78.628793	2176.675493	21.718234
78.790441	2176.483154	21.723251
78.635573	2174.743182	21.728269
78.845964	2179.655902	21.733287
78.660525	2179.211476	21.738304
78.522035	2178.273722	21.743322
78.994649	2173.841860	21.748339
78.624714	2176.689415	21.753357
78.609950	2170.673403	21.758375
78.702811	2165.492744	21.763392
78.697507	2177.745079	21.768410
78.992305	2177.992780	21.773427
79.299807	2193.443902	21.778445
79.202167	2195.870351	21.783463
79.110396	2188.910067	21.788480
79.268920	2202.232030	21.793498
79.377361	2194.959691	21.798515
78.988006	2190.693587	21.803533
79.310729	2201.777658	21.808551
79.460577	2213.002266	21.813568
79.538697	2221.489205	21.818586
79.544394	2222.854945	21.823603
79.705850	2231.382565	21.828621
80.028831	2244.944055	21.833639
80.149383	2242.520534	21.838656
79.888227	2246.884964	21.843674
80.085085	2247.233125	21.848691
80.087812	2246.844612	21.853709
80.072578	2260.364093	21.858727
80.444490	2263.484345	21.863744
80.441925	2270.260709	21.868762
80.817050	2264.177650	21.873779
81.070078	2266.536888	21.878797
80.847456	2260.303886	21.883815
81.025551	2262.700038	21.888832
80.726195	2260.960462	21.893850
81.308844	2274.787675	21.898867
81.539702	2284.513252	21.903885
81.713817	2292.947407	21.908903
81.756893	2287.310536	21.913920
81.816104	2289.586338	21.918938
82.047280	2272.599705	21.923955
81.488923	2266.482093	21.928973
81.700219	2266.600777	21.933991
81.537207	2272.594194	21.939008
81.493549	2279.051894	21.944026
82.093754	2273.375625	21.949043
81.930643	2280.419999	21.954061
81.688159	2279.069219	21.959079
82.189245	2280.976405	21.964096
82.063857	2299.139723	21.969114
82.529144	2302.968163	21.974131
82.521307	2302.761184	21.979149
82.373575	2296.147260	21.984167
82.750240	2288.489122	21.989184
82.413949	2296.491477	21.994202
82.892036	2298.872487	21.999219
82.784384	2290.327179	22.004237
82.813562	2297.524668	22.009255
82.779052	2294.023847	22.014272
82.732198	2294.261623	22.019290
82.961625	2301.509991	22.024307
83.304284	2309.712774	22.029325
82.986054	2313.439131	22.034343
83.137445	2308.331373	22.039360
83.211320	2310.989924	22.044378
83.775426	2317.460317	22.049395
83.717959	2315.200209	22.054413
83.839477	2324.740850	22.059431
84.215639	2323.435766	22.064448
84.108699	2335.479958	22.069466
84.380438	2318.808877	22.074483
84.264923	2312.309859	22.079501
84.251274	2317.740364	22.084519
84.447457	2322.440729	22.089536
84.260965	2331.360260	22.094554
84.673599	2317.176250	22.099571
84.812649	2317.088420	22.104589
84.613282	2325.893182	22.109607
84.837331	2332.359717	22.114624
84.744937	2330.486919	22.119642
84.764388	2320.160770	22.124659
84.778541	2317.867420	22.129677
84.563539	2331.010935	22.134695
84.700551	2320.893713	22.139712
84.418827	2339.450663	22.144730
85.198569	2354.108836	22.149747
85.082947	2353.805021	22.154765
85.114701	2345.806060	22.159783
85.793405	2352.649966	22.164800
85.580527	2370.520847	22.169818
85.839493	2377.477453	22.174835
85.627526	2377.494770	22.179853
85.523332	2376.564290	22.184871
85.473887	2371.724482	22.189888
85.553435	2374.580986	22.194906
85.702181	2384.600286	22.199923
85.900003	2395.858567	22.204941
86.114708	2395.793674	22.209959
86.567484	2397.730487	22.214976
86.162916	2408.044242	22.219994
86.719447	2408.519456	22.225011
86.925786	2413.647480	22.230029
87.122602	2421.576358	22.235047
87.237268	2419.175821	22.240064
87.033302	2409.600817	22.245082
87.071928	2411.583176	22.250099
87.223600	2421.523140	22.255117
87.429311	2415.510591	22.260135
87.210152	2413.663833	22.265152
87.178137	2421.628339	22.270170
87.036784	2416.783893	22.275187
87.358482	2414.556263	22.280205
87.272238	2414.916945	22.285223
87.554918	2421.686828	22.290240
87.448889	2429.552400	22.295258
87.442297	2430.276245	22.300275
87.463394	2435.467832	22.305293
87.563219	2439.665646	22.310311
88.095217	2444.758756	22.315328
88.083837	2459.972561	22.320346
88.272192	2454.688582	22.325363
88.555893	2451.936655	22.330381
88.409923	2461.241286	22.335399
88.515016	2457.895433	22.340416
88.436779	2453.568203	22.345434
88.598867	2455.932157	22.350451
88.829831	2462.470251	22.355469
88.899035	2483.238723	22.360487
88.991795	2479.339329	22.365504
88.884535	2479.621229	22.370522
89.137556	2485.650935	22.375539
89.462689	2481.475505	22.380557
88.897499	2491.546055	22.385575
89.075066	2492.449527	22.390592
89.252709	2485.292537	22.395610
89.068956	2497.913723	22.400627
89.515855	2499.864087	22.405645
89.413006	2498.589385	22.410663
89.920448	2500.650251	22.415680
89.859376	2500.893399	22.420698
89.990747	2514.462835	22.425715
90.563346	2518.520784	22.430733
90.154754	2531.735615	22.435751
90.430477	2521.221117	22.440768
90.491528	2528.584161	22.445786
90.505950	2525.113548	22.450803
90.888372	2534.613679	22.455821
90.628924	2518.861460	22.460839
90.369917	2525.311749	22.465856
90.633683	2525.030920	22.470874
90.488545	2528.607287	22.475891
90.986517	2533.368026	22.480909
90.494782	2539.516860	22.485927
90.960431	2549.928755	22.490944
91.176732	2558.653134	22.495962
91.599540	2569.036994	22.500979
91.658534	2563.631103	22.505997
91.837525	2566.393255	22.511015
92.352205	2562.538613	22.516032
92.314031	2552.682082	22.521050
92.046940	2548.576749	22.526067
92.338337	2539.637811	22.531085
92.222477	2545.573482	22.536103
92.689829	2540.829903	22.541120
92.205099	2538.090298	22.546138
92.429913	2548.388200	22.551155
92.840482	2549.056569	22.556173
92.813705	2550.389517	22.561191
92.807497	2549.702566	22.566208
92.739261	2540.118984	22.571226
92.851320	2549.992599	22.576243
92.774228	2545.936586	22.581261
92.357417	2557.410592	22.586279
92.478846	2557.095115	22.591296
92.828054	2557.151302	22.596314
92.956523	2571.185167	22.601331
93.093563	2564.656204	22.606349
92.875752	2569.932366	22.611367
93.340041	2590.131331	22.616384
93.657022	2592.868847	22.621402
93.382579	2606.242740	22.626419
93.459131	2597.570770	22.631437
93.298423	2603.425073	22.636455
93.694822	2612.771580	22.641472
93.823695	2630.273909	22.646490
94.038863	2624.597513	22.651507
94.479000	2631.330337	22.656525
94.368974	2623.457475	22.661543
94.880559	2626.448741	22.666560
94.625542	2622.770732	22.671578
94.528416	2629.924899	22.676595
94.590591	2637.609728	22.681613
94.546148	2646.702974	22.686631
94.820193	2652.593754	22.691648
95.190275	2646.179968	22.696666
94.912675	2642.991501	22.701683
95.070045	2648.389167	22.706701
94.854912	2655.359730	22.711719
95.435565	2660.227560	22.716736
95.619767	2666.681484	22.721754
95.225095	2666.998666	22.726771
95.869516	2670.445820	22.731789
95.637507	2679.104346	22.736807
95.771654	2677.082623	22.741824
96.105294	2673.230897	22.746842
95.923410	2671.842247	22.751859
96.154786	2675.864989	22.756877
96.179953	2691.089080	22.761895
96.105688	2694.629197	22.766912
96.406338	2698.615910	22.771930
96.449546	2698.707115	22.776947
96.720795	2692.453879	22.781965
96.468778	2693.673572	22.786983
96.674279	2699.855928	22.792000
96.977006	2712.089075	22.797018
96.846363	2713.599165	22.802035
97.141107	2711.659741	22.807053
97.181944	2720.124316	22.812071
97.159499	2721.131530	22.817088
97.288743	2715.664159	22.822106
97.417014	2716.206060	22.827123
97.470513	2725.000051	22.832141
97.674540	2730.497784	22.837159
97.786898	2732.298272	22.842176
97.649075	2731.707550	22.847194
97.472300	2736.772229	22.852211
97.804197	2737.266647	22.857229
97.929298	2753.980670	22.862247
98.032617	2758.897596	22.867264
98.307350	2755.086584	22.872282
98.483515	2756.675153	22.877299
98.702249	2760.336936	22.882317
98.909068	2772.651333	22.887335
99.063746	2767.407223	22.892352
99.026727	2773.621051	22.897370
99.153776	2773.828602	22.902387
99.356349	2769.201934	22.907405
99.472987	2778.689923	22.912423
99.451020	2771.257759	22.917440
99.577520	2767.861175	22.922458
99.205975	2778.766496	22.927475
99.456509	2769.919020	22.932493
99.486185	2769.071826	22.937511
99.478427	2777.682861	22.942528
99.806234	2791.707957	22.947546
99.541052	2798.942008	22.952563
99.804960	2799.898331	22.957581
99.951649	2809.138640	22.962599
99.973652	2811.240406	22.967616
99.854198	2816.444517	22.972634
99.977965	2822.150451	22.977651
100.501876	2823.820594	22.982669
100.661866	2833.178776	22.987687
100.764339	2852.187721	22.992704
101.099169	2844.049825	22.997722
100.774876	2834.190344	23.002739
101.069062	2832.525572	23.007757
101.565710	2839.132901	23.012775
101.227313	2838.030560	23.017792
101.235717	2832.487286	23.022810
101.170342	2843.253451	23.027827
101.436451	2841.949685	23.032845
101.584360	2854.096571	23.037863
101.827276	2853.007872	23.042880
101.910751	2860.850441	23.047898
102.009997	2860.450043	23.052915
101.919411	2863.708687	23.057933
101.794243	2860.673188	23.062951
101.726061	2871.067390	23.067968
102.475199	2868.413364	23.072986
102.195714	2890.350691	23.078003
102.199590	2886.809060	23.083021
102.482701	2885.278563	23.088039
102.352597	2887.198874	23.093056
102.952742	2894.598067	23.098074
102.849761	2913.452856	23.103091
103.358222	2913.332758	23.108109
103.688202	2906.779943	23.113127
103.579580	2905.922715	23.118144
103.788505	2899.073142	23.123162
103.302976	2907.708128	23.128179
103.621595	2907.630211	23.133197
103.717661	2903.332544	23.138215
103.581535	2907.033826	23.143232
103.851143	2910.924425	23.148250
103.857541	2926.066423	23.153267
103.900020	2917.143961	23.158285
104.192691	2923.432753	23.163303
103.876379	2928.598113	23.168320
104.532190	2942.884711	23.173338
104.424554	2946.894019	23.178355
104.486202	2943.027773	23.183373
104.599194	2949.126779	23.188391
104.704850	2951.941438	23.193408
105.255251	2942.125612	23.198426
104.820544	2945.516750	23.203443
104.974447	2961.926654	23.208461
105.573599	2962.777137	23.213479
105.192027	2972.121869	23.218496
105.383466	2964.549093	23.223514
105.220523	2973.787197	23.228531
105.782796	2976.571797	23.233549
106.237681	2979.300527	23.238567
106.313204	2984.666852	23.243584
106.448597	2979.741293	23.248602
106.486636	2977.346300	23.253619
106.831141	2985.577512	23.258637
106.910331	2971.852039	23.263655
106.709664	2958.201709	23.268672
106.600072	2949.018859	23.273690
106.548478	2962.787549	23.278707
106.624382	2970.170555	23.283725
106.972005	2977.511259	23.288743
106.982932	2975.900044	23.293760
106.865192	2977.026259	23.298778
106.928875	2980.421867	23.303795
107.125659	2989.525070	23.308813
107.330375	2998.582857	23.313831
107.303687	3002.727910	23.318848
107.199323	3011.306757	23.323866
107.249161	3008.616406	23.328883
107.473618	3016.670644	23.333901
107.696280	3020.193001	23.338919
107.862679	3038.762960	23.343936
108.164932	3025.902207	23.348954
108.186308	3040.376032	23.353971
108.396230	3046.933396	23.358989
108.375869	3056.594355	23.364007
108.154748	3054.135550	23.369024
109.085901	3060.097744	23.374042
108.864131	3052.093755	23.379059
108.662575	3056.890956	23.384077
108.877293	3046.805413	23.389095
108.725580	3072.908070	23.394112
109.207618	3072.650061	23.399130
109.125251	3083.191775	23.404147
109.218126	3081.006003	23.409165
109.427495	3076.059431	23.414183
109.264622	3083.438630	23.419200
109.469901	3096.293185	23.424218
109.755355	3103.138641	23.429235
109.997290	3110.233897	23.434253
110.119652	3098.026012	23.439271
109.883930	3112.792412	23.444288
110.387557	3111.047665	23.449306
110.480909	3111.329901	23.454323
110.143230	3119.231841	23.459341
110.669283	3117.101711	23.464359
110.793240	3123.508369	23.469376
110.858852	3124.331465	23.474394
110.451800	3126.897739	23.479411
110.827114	3140.647441	23.484429
110.830493	3132.756700	23.489447
111.005998	3144.665932	23.494464
111.519808	3146.075722	23.499482
111.528014	3155.464015	23.504499
111.311828	3169.422608	23.509517
111.620371	3157.886356	23.514535
111.291165	3161.024399	23.519552
111.717887	3177.136377	23.524570
112.167337	3182.428764	23.529587
111.988111	3193.007715	23.534605
112.118458	3191.554631	23.539623
111.564109	3191.353826	23.544640
112.510639	3203.152522	23.549658
112.601536	3210.697412	23.554675
112.561082	3207.099497	23.559693
112.844720	3205.616233	23.564711
112.893257	3215.364391	23.569728
113.258267	3229.210448	23.574746
113.361438	3235.721379	23.579763
113.514879	3234.684463	23.584781
113.520624	3235.529509	23.589799
113.411750	3236.446055	23.594816
113.598473	3228.488853	23.599834
113.898752	3235.625573	23.604851
113.772876	3246.818010	23.609869
114.550321	3247.498723	23.614887
114.597185	3258.455967	23.619904
115.027972	3248.497635	23.624922
114.953468	3232.621309	23.629939
114.756616	3227.356049	23.634957
115.015010	3223.777881	23.639975
114.449116	3227.195808	23.644992
114.617678	3233.971142	23.650010
115.092856	3239.338443	23.655027
115.077967	3250.453636	23.660045
115.300358	3243.633398	23.665063
114.985869	3244.689266	23.670080
115.059511	3243.775238	23.675098
115.471956	3256.181043	23.680115
115.332924	3273.160759	23.685133
116.112580	3266.439963	23.690151
115.564975	3273.677146	23.695168
115.823656	3273.375006	23.700186
115.869754	3272.825066	23.705203
115.705058	3285.977227	23.710221
116.561097	3292.598206	23.715239
115.916217	3292.578770	23.720256
116.035974	3291.360882	23.725274
116.326109	3298.057345	23.730291
116.218429	3313.043841	23.735309
116.516272	3313.944411	23.740327
116.590101	3326.554479	23.745344
116.943863	3337.899540	23.750362
117.065081	3334.188056	23.755379
117.073640	3340.521230	23.760397
117.511746	3336.245955	23.765415
117.463100	3340.479721	23.770432
117.859762	3354.958492	23.775450
118.164779	3352.846968	23.780467
117.998589	3358.080605	23.785485
118.235449	3357.175878	23.790503
118.132743	3360.714241	23.795520
118.126902	3358.436496	23.800538
118.531467	3355.403654	23.805555
118.071819	3367.784350	23.810573
118.947984	3360.041678	23.815591
119.016931	3374.722984	23.820608
119.222006	3377.102461	23.825626
119.487208	3372.106085	23.830643
119.540873	3373.953650	23.835661
120.111790	3367.445218	23.840679
119.582437	3350.768503	23.845696
119.601618	3344.194484	23.850714
119.822443	3347.572008	23.855731
119.684046	3359.640721	23.860749
119.611766	3362.827170	23.865767
119.593331	3363.931636	23.870784
119.782452	3363.375207	23.875802
119.728813	3363.910732	23.880819
119.715315	3380.580637	23.885837
120.164032	3374.763492	23.890855
120.554896	3391.016961	23.895872
120.592987	3397.503365	23.900890
120.782782	3400.731078	23.905907
120.645657	3411.751779	23.910925
120.940672	3406.349918	23.915943
121.014666	3420.771670	23.920960
121.335743	3427.810544	23.925978
121.372153	3434.666496	23.930995
121.232860	3447.455015	23.936013
121.327070	3437.694165	23.941031
121.744978	3443.474435	23.946048
121.975921	3450.991309	23.951066
122.430121	3444.908169	23.956083
122.478442	3455.521283	23.961101
122.558178	3451.191310	23.966119
122.255382	3452.778763	23.971136
122.281030	3448.236279	23.976154
122.174145	3455.427010	23.981171
122.273176	3478.139353	23.986189
122.262294	3478.674537	23.991207
122.552314	3477.281787	23.996224
122.725963	3502.116123	24.001242
122.943565	3503.609934	24.006259
122.906727	3508.596230	24.011277
122.827225	3515.107297	24.016295
123.278947	3523.602965	24.021312
123.412913	3532.457416	24.026330
123.908610	3535.527060	24.031347
123.858410	3547.354920	24.036365
124.130638	3551.194753	24.041383
124.316834	3555.000638	24.046400
124.494505	3543.576046	24.051418
124.658008	3538.680676	24.056435
124.311468	3554.635639	24.061453
124.540766	3549.629024	24.066471
124.857620	3551.015856	24.071488
125.051607	3564.254404	24.076506
125.340654	3569.947468	24.081523
125.520051	3565.333674	24.086541
125.180200	3566.623911	24.091559
125.506556	3562.691070	24.096576
125.711894	3561.352529	24.101594
125.561703	3562.581675	24.106611
125.628878	3564.777494	24.111629
125.534337	3565.874885	24.116647
125.675220	3575.223803	24.121664
125.811134	3591.302525	24.126682
125.992328	3582.667444	24.131699
126.649181	3600.369417	24.136717
126.205479	3604.977217	24.141735
126.525963	3610.226686	24.146752
126.596688	3613.659191	24.151770
126.855987	3623.055979	24.156787
127.117525	3635.883224	24.161805
127.076110	3639.973904	24.166823
127.318615	3635.069365	24.171840
126.908410	3638.526252	24.176858
126.957301	3648.003155	24.181875
127.320868	3663.506785	24.186893
127.584156	3664.712593	24.191911
128.044739	3664.700947	24.196928
128.281221	3687.666744	24.201946
128.408600	3685.115719	24.206963
128.500421	3685.054174	24.211981
128.629197	3678.428252	24.216999
129.090082	3684.233472	24.222016
128.903687	3677.050626	24.227034
128.948818	3677.157318	24.232051
128.923192	3675.324483	24.237069
129.135368	3691.104205	24.242087
129.610243	3692.662132	24.247104
128.630429	3694.752696	24.252122
129.494414	3697.143253	24.257139
129.368886	3708.260172	24.262157
129.280776	3720.652700	24.267175
129.727669	3727.719446	24.272192
129.563908	3738.122716	24.277210
130.127793	3746.165468	24.282227
130.637487	3750.779523	24.287245
130.480393	3741.007136	24.292263
130.819071	3741.096532	24.297280
130.571726	3746.989944	24.302298
130.762405	3746.761509	24.307315
131.158337	3751.854086	24.312333
131.220428	3762.938672	24.317351
131.511919	3765.686651	24.322368
131.439008	3768.200991	24.327386
131.692836	3762.682345	24.332403
131.564664	3769.892297	24.337421
131.318204	3764.394728	24.342439
132.191317	3769.719172	24.347456
131.913511	3784.366424	24.352474
132.348692	3780.022063	24.357491
132.346796	3779.899360	24.362509
132.177978	3787.800551	24.367527
132.157928	3778.663304	24.372544
132.675852	3789.276095	24.377562
133.429400	3782.104677	24.382579
133.469949	3796.509843	24.387597
133.375038	3791.285358	24.392615
133.283048	3781.714280	24.397632
133.282219	3793.569334	24.402650
133.552408	3792.747772	24.407667
133.690524	3789.683749	24.412685
133.745318	3786.929386	24.417703
133.938860	3784.614232	24.422720
133.595999	3794.887607	24.427738
134.064401	3803.213530	24.432755
134.143108	3812.281878	24.437773
133.821824	3818.098450	24.442791
134.348695	3807.834477	24.447808
134.228805	3823.918515	24.452826
134.630894	3832.532525	24.457843
134.975260	3830.026603	24.462861
135.034058	3842.140686	24.467879
135.069774	3845.045280	24.472896
135.026841	3851.954775	24.477914
134.938205	3855.131232	24.482931
135.049715	3862.307061	24.487949
135.330871	3879.749021	24.492967
135.796542	3888.201660	24.497984
135.736059	3890.657269	24.503002
135.900780	3892.752723	24.508019
135.876139	3902.203332	24.513037
136.124756	3914.815006	24.518055
136.272912	3913.052934	24.523072
136.072294	3925.324244	24.528090
136.622390	3930.837903	24.533107
136.890835	3941.637970	24.538125
136.855301	3946.791466	24.543143
136.768980	3942.127415	24.548160
137.194166	3958.650649	24.553178
137.025494	3958.124657	24.558195
137.828709	3981.646472	24.563213
137.913529	3984.051066	24.568231
138.054128	3986.289162	24.573248
138.156682	3989.145498	24.578266
138.609217	3986.038803	24.583283
138.245891	3978.858132	24.588301
138.487147	3984.391486	24.593319
138.625823	3983.634579	24.598336
138.848699	4006.470337	24.603354
138.764668	4011.337868	24.608371
138.887058	4005.309357	24.613389
139.084312	4005.843715	24.618407
139.516798	4011.410429	24.623424
139.583809	4035.539314	24.628442
139.696882	4034.035196	24.633459
139.925371	4037.310656	24.638477
139.979168	4034.629005	24.643495
140.317092	4024.287014	24.648512
140.213312	4032.089810	24.653530
140.220952	4038.338152	24.658547
140.459384	4045.248103	24.663565
140.421182	4049.748693	24.668583
140.684877	4051.459470	24.673600
140.569050	4047.222928	24.678618
140.912375	4063.067776	24.683635
140.914730	4082.453424	24.688653
140.707368	4081.690419	24.693671
141.373478	4080.125444	24.698688
141.740188	4090.897677	24.703706
141.676402	4099.101436	24.708723
142.087050	4090.414607	24.713741
142.059083	4085.135426	24.718759
142.390118	4088.151896	24.723776
142.396866	4092.336182	24.728794
142.220335	4086.139556	24.733811
142.564198	4077.611477	24.738829
142.949091	4100.340066	24.743847
143.277767	4101.661976	24.748864
142.990758	4106.674761	24.753882
143.099554	4113.301917	24.758899
143.187431	4106.817927	24.763917
143.533796	4105.690956	24.768935
143.466408	4106.556898	24.773952
143.459510	4109.812206	24.778970
143.363050	4118.365097	24.783987
143.945547	4124.972163	24.789005
143.720308	4138.790880	24.794023
144.051063	4129.115925	24.799040
143.976909	4142.873247	24.804058
144.049795	4153.542916	24.809075
144.323912	4157.938095	24.814093
144.212091	4165.997860	24.819111
144.696507	4171.853232	24.824128
144.994147	4184.795187	24.829146
145.137712	4190.946669	24.834163
145.163922	4199.824537	24.839181
144.993090	4210.232335	24.844199
145.122368	4216.521771	24.849216
145.278189	4222.321004	24.854234
145.455870	4234.647253	24.859251
146.049510	4245.065459	24.864269
146.547435	4261.757556	24.869287
146.200091	4254.653195	24.874304
146.446419	4263.960803	24.879322
146.594897	4265.847356	24.884339
146.977471	4270.781189	24.889357
146.869081	4273.686194	24.894375
147.348186	4274.568062	24.899392
147.444575	4270.948630	24.904410
147.448981	4275.969748	24.909427
148.124128	4278.187783	24.914445
147.575424	4300.695843	24.919463
147.961879	4294.452526	24.924480
148.052194	4296.565924	24.929498
148.152680	4295.657133	24.934515
148.521838	4287.446963	24.939533
148.469085	4298.811733	24.944551
148.597072	4299.562046	24.949568
148.877602	4310.814964	24.954586
148.709365	4308.758074	24.959603
149.176375	4316.307996	24.964621
148.989348	4327.027703	24.969639
149.109781	4333.479530	24.974656
149.494388	4336.923275	24.979674
149.274759	4346.991553	24.984691
149.711943	4353.258349	24.989709
149.817902	4365.782077	24.994727
149.951205	4364.240063	24.999744
150.575083	4368.520868	25.004762
150.390594	4389.769768	25.009779
150.812450	4385.004390	25.014797
150.705087	4391.835744	25.019815
150.362423	4388.401429	25.024832
151.232961	4399.691954	25.029850
150.911067	4411.802563	25.034867
151.182888	4408.622929	25.039885
151.039401	4412.653924	25.044903
151.420978	4414.040218	25.049920
151.609846	4425.386387	25.054938
151.653473	4425.944676	25.059955
152.036782	4431.995787	25.064973
151.869691	4447.740528	25.069991
152.182609	4455.592258	25.075008
152.537096	4449.798911	25.080026
152.360255	4464.301582	25.085043
152.842082	4474.522697	25.090061
153.105925	4484.951356	25.095079
153.182547	4473.403031	25.100096
153.761684	4464.554069	25.105114
153.401015	4475.092578	25.110131
153.584466	4463.707539	25.115149
153.862336	4462.547022	25.120167
153.698848	4469.585994	25.125184
153.735580	4480.943259	25.130202
153.994877	4492.341633	25.135219
154.156312	4489.920916	25.140237
154.322145	4495.169471	25.145255
154.289756	4512.414663	25.150272
154.688917	4509.650765	25.155290
154.927961	4518.580875	25.160307
155.134267	4525.846369	25.165325
155.163302	4535.279483	25.170343
155.355663	4536.010313	25.175360
155.978260	4529.843780	25.180378
156.188392	4528.605427	25.185395
156.258602	4521.331790	25.190413
156.401222	4531.100731	25.195431
156.461944	4543.871510	25.200448
156.955781	4545.275056	25.205466
156.950014	4546.267149	25.210483
156.980639	4540.546290	25.215501
157.117822	4551.354534	25.220519
156.953411	4543.767060	25.225536
156.815842	4539.375968	25.230554
157.285053	4555.820299	25.235571
157.642364	4558.722285	25.240589
157.155593	4570.211612	25.245607
157.598132	4577.992713	25.250624
157.485569	4579.822093	25.255642
157.818151	4595.192469	25.260659
157.957534	4595.186645	25.265677
158.235407	4609.858522	25.270695
158.345178	4616.050130	25.275712
158.653905	4614.771170	25.280730
158.654149	4630.682557	25.285747
159.322803	4639.337520	25.290765
158.912631	4646.654853	25.295783
158.924514	4646.984518	25.300800
159.341231	4650.183439	25.305818
159.736741	4651.536019	25.310835
159.985920	4657.740657	25.315853
160.244758	4659.382809	25.320871
160.039003	4677.602067	25.325888
160.286331	4677.033382	25.330906
160.298456	4681.371630	25.335923
161.015100	4678.731879	25.340941
161.034612	4683.905422	25.345959
161.340382	4697.531417	25.350976
161.495411	4692.753842	25.355994
161.540631	4705.527148	25.361011
161.721704	4690.572451	25.366029
161.683467	4700.054001	25.371047
161.492536	4697.602894	25.376064
161.945075	4711.704760	25.381082
161.898706	4715.853270	25.386099
162.473661	4714.349783	25.391117
162.582188	4720.254388	25.396135
162.400004	4716.772930	25.401152
162.894448	4731.531131	25.406170
162.616847	4751.242002	25.411187
163.085424	4748.669270	25.416205
163.082944	4741.375299	25.421223
162.925217	4757.191449	25.426240
163.395896	4765.384896	25.431258
163.392574	4770.038054	25.436275
163.986869	4768.354793	25.441293
164.076714	4784.681637	25.446311
163.833272	4804.709201	25.451328
164.103695	4796.662526	25.456346
164.090393	4800.322976	25.461363
164.391074	4806.816350	25.466381
164.745336	4810.924603	25.471399
164.705357	4815.122644	25.476416
164.794348	4822.040377	25.481434
164.903356	4841.097747	25.486451
165.350517	4841.167106	25.491469
165.577475	4849.919346	25.496487
165.347636	4870.535116	25.501504
165.615732	4863.299975	25.506522
165.716692	4885.196271	25.511539
166.154885	4890.377287	25.516557
166.424823	4882.665231	25.521575
166.620469	4898.874700	25.526592
167.301397	4911.050461	25.531610
167.219072	4916.113668	25.536627
167.102976	4911.741238	25.541645
167.379888	4914.248619	25.546663
167.378594	4927.891030	25.551680
167.660095	4930.842757	25.556698
167.751899	4936.626935	25.561715
167.901011	4937.920049	25.566733
168.119359	4950.426684	25.571751
168.173355	4953.136068	25.576768
168.116659	4955.483913	25.581786
168.640641	4968.504823	25.586803
168.821510	4987.330208	25.591821
169.232429	4985.700729	25.596839
168.967074	4990.094877	25.601856
169.005197	4995.256142	25.606874
169.343071	5007.567447	25.611891
169.033342	5005.766083	25.616909
169.694156	5026.110793	25.621927
169.753351	5028.260686	25.626944
170.184142	5036.075379	25.631962
170.262919	5056.368700	25.636979
170.449129	5070.928963	25.641997
170.940383	5059.179983	25.647015
170.937968	5070.145998	25.652032
171.020523	5083.740751	25.657050
171.130553	5079.806544	25.662067
170.889354	5082.713416	25.667085
171.581554	5096.753018	25.672103
171.679144	5104.013575	25.677120
171.868969	5107.497265	25.682138
171.954942	5114.683880	25.687156
172.311185	5141.161811	25.692173
172.697777	5131.108324	25.697191
172.236634	5142.799192	25.702208
172.759614	5140.312631	25.707226
172.971335	5150.260535	25.712244
173.493187	5154.096569	25.717261
173.657183	5143.594790	25.722279
173.962755	5155.090541	25.727296
173.757495	5141.499246	25.732314
173.638230	5155.857776	25.737332
174.009424	5174.252850	25.742349
174.131239	5174.978909	25.747367
174.398282	5179.280745	25.752384
174.158548	5178.181831	25.757402
174.557261	5195.000714	25.762420
174.626755	5206.066093	25.767437
175.047923	5191.234584	25.772455
174.855332	5207.258568	25.777472
175.343570	5216.961443	25.782490
175.224707	5223.886439	25.787508
175.068206	5230.814141	25.792525
175.554560	5240.435253	25.797543
175.483183	5245.837748	25.802560
175.671162	5255.587392	25.807578
176.059505	5269.844887	25.812596
176.093444	5279.526987	25.817613
176.520032	5291.284911	25.822631
176.742418	5297.661235	25.827648
177.239598	5301.892549	25.832666
177.214177	5320.163286	25.837684
177.392636	5323.083773	25.842701
177.685372	5311.292939	25.847719
177.693301	5333.434684	25.852736
178.056442	5341.862935	25.857754
178.255759	5353.747822	25.862772
178.193108	5349.180731	25.867789
178.538651	5362.226550	25.872807
178.409786	5368.408220	25.877824
178.839733	5366.829407	25.882842
179.106163	5380.926049	25.887860
179.474444	5389.344052	25.892877
179.532703	5395.723868	25.897895
180.104003	5383.245688	25.902912
180.538180	5386.258946	25.907930
180.370915	5387.976975	25.912948
180.200537	5386.936693	25.917965
180.841759	5390.088169	25.922983
180.681480	5405.845306	25.928000
180.952878	5400.386559	25.933018
181.299295	5413.192383	25.938036
180.963322	5403.106042	25.943053
181.527671	5413.949304	25.948071
181.273404	5426.712927	25.953088
181.608987	5429.751012	25.958106
181.582810	5425.370771	25.963124
181.933250	5450.233917	25.968141
182.046680	5439.083283	25.973159
182.023829	5452.000286	25.978176
182.562212	5465.382313	25.983194
182.748079	5465.470262	25.988212
182.745499	5460.300363	25.993229
183.185105	5480.910450	25.998247
183.231441	5493.602067	26.003264
183.277189	5494.639853	26.008282
183.464348	5497.278081	26.013300
183.948960	5517.698125	26.018317
183.961541	5511.932421	26.023335
183.927868	5527.246976	26.028352
184.176574	5535.532150	26.033370
184.671199	5534.217872	26.038388
184.454806	5552.704811	26.043405
184.841784	5558.822018	26.048423
185.364773	5561.733095	26.053440
185.168760	5578.594423	26.058458
185.623643	5570.799621	26.063476
185.756269	5588.200067	26.068493
185.825350	5599.029008	26.073511
186.211499	5593.763827	26.078528
186.333937	5599.461377	26.083546
186.358202	5594.921728	26.088564
186.539293	5607.775524	26.093581
187.247775	5605.190577	26.098599
186.866028	5611.569529	26.103616
187.199187	5606.214742	26.108634
187.410213	5610.313913	26.113652
187.188241	5614.291104	26.118669
188.099873	5606.393611	26.123687
187.815431	5628.379215	26.128704
188.231088	5630.401082	26.133722
188.276002	5619.421989	26.138740
188.306010	5635.900959	26.143757
188.663134	5646.138998	26.148775
188.655515	5647.197727	26.153792
188.840748	5648.352694	26.158810
189.202602	5664.956793	26.163828
189.179839	5665.935811	26.168845
189.044765	5678.318047	26.173863
189.210155	5685.154771	26.178880
189.362130	5693.587653	26.183898
190.053232	5709.531315	26.188916
189.910922	5725.263834	26.193933
190.374797	5734.797169	26.198951
190.480511	5742.937402	26.203968
190.873312	5744.063216	26.208986
191.117418	5751.086573	26.214004
191.083994	5771.675939	26.219021
191.328891	5769.418828	26.224039
191.141861	5781.774502	26.229056
191.422523	5796.314329	26.234074
192.010736	5795.847212	26.239092
192.054110	5823.021948	26.244109
192.136059	5817.744090	26.249127
192.433625	5828.632292	26.254144
192.849724	5843.694005	26.259162
193.309756	5839.752492	26.264180
193.319743	5843.239070	26.269197
193.655402	5862.849351	26.274215
193.657996	5866.150845	26.279232
193.921598	5870.759571	26.284250
194.214746	5862.046003	26.289268
194.195017	5877.699594	26.294285
194.451775	5887.445182	26.299303
194.421344	5896.272723	26.304320
194.415952	5903.142430	26.309338
194.697400	5910.772418	26.314356
194.563728	5925.263217	26.319373
194.922652	5936.201907	26.324391
194.859386	5946.966431	26.329408
195.334716	5962.271549	26.334426
196.203111	5974.412529	26.339444
195.965107	5984.983317	26.344461
196.369039	5986.751364	26.349479
196.817166	5991.454501	26.354496
196.350080	6001.656916	26.359514
197.095638	6010.111169	26.364532
197.131513	6016.785098	26.369549
197.316819	6021.017787	26.374567
197.589796	6034.690929	26.379584
197.463431	6053.170672	26.384602
197.956457	6046.783902	26.389620
197.900391	6067.957948	26.394637
198.007219	6073.879041	26.399655
198.325120	6076.623265	26.404672
198.512215	6086.477661	26.409690
198.831750	6103.707450	26.414708
198.795809	6103.021836	26.419725
199.307627	6117.873163	26.424743
199.320983	6117.615490	26.429760
199.191476	6133.608368	26.434778
199.699340	6144.391416	26.439796
199.600409	6150.988525	26.444813
200.089193	6156.733383	26.449831
200.063077	6167.836328	26.454848
200.230768	6183.350518	26.459866
200.386490	6197.354546	26.464884
200.567489	6203.791295	26.469901
200.858967	6209.986724	26.474919
201.241149	6228.542145	26.479936
201.108080	6235.829595	26.484954
201.546598	6243.946648	26.489972
201.807558	6255.573151	26.494989
202.166979	6263.194303	26.500007
202.560299	6269.317077	26.505024
202.373051	6276.313094	26.510042
202.569152	6288.694691	26.515060
202.994410	6301.523590	26.520077
203.298303	6299.364556	26.525095
203.249879	6314.659971	26.530112
203.462902	6326.136149	26.535130
204.024324	6328.211162	26.540148
204.093450	6339.605581	26.545165
204.517011	6356.904644	26.550183
204.514275	6356.965142	26.555200
204.477626	6368.814826	26.560218
205.016164	6373.245139	26.565236
205.198772	6379.467045	26.570253
205.327988	6383.825350	26.575271
206.156674	6386.717379	26.580288
205.787714	6400.168756	26.585306
206.553583	6395.238816	26.590324
206.509044	6398.058457	26.595341
206.412842	6396.624608	26.600359
206.599784	6409.793728	26.605376
206.971157	6420.263581	26.610394
207.266026	6421.833996	26.615412
207.179759	6420.206040	26.620429
207.342228	6426.500545	26.625447
207.869831	6431.216677	26.630464
207.970765	6438.458306	26.635482
208.657003	6443.304422	26.640500
208.736315	6446.309974	26.645517
209.066125	6448.370553	26.650535
209.471644	6442.316098	26.655552
209.594339	6443.253570	26.660570
209.634126	6451.947336	26.665588
209.574132	6451.454856	26.670605
209.783937	6454.623181	26.675623
210.052380	6461.358921	26.680640
210.026404	6473.251206	26.685658
210.359300	6475.775344	26.690676
210.044079	6479.691479	26.695693
210.241928	6493.297744	26.700711
210.589451	6493.733023	26.705728
210.806301	6511.474789	26.710746
210.794755	6520.384922	26.715764
210.842257	6533.111804	26.720781
211.218095	6544.720607	26.725799
211.780590	6550.896055	26.730816
211.480183	6574.372095	26.735834
211.998843	6581.596097	26.740852
212.023098	6609.592571	26.745869
212.210960	6617.082746	26.750887
212.441856	6619.142961	26.755904
212.660855	6640.075970	26.760922
212.819600	6649.123804	26.765940
213.240560	6657.332164	26.770957
213.161413	6670.119897	26.775975
213.636615	6676.147985	26.780992
213.664981	6692.072578	26.786010
214.182575	6698.018311	26.791028
214.245111	6711.693157	26.796045
214.145380	6729.500205	26.801063
214.714065	6737.429905	26.806080
215.044460	6743.048085	26.811098
215.328680	6755.889793	26.816116
215.387580	6765.717163	26.821133
215.606869	6767.896002	26.826151
216.109427	6782.108491	26.831168
215.726206	6784.261180	26.836186
216.054991	6787.969786	26.841204
216.428024	6794.727247	26.846221
216.621752	6805.897368	26.851239
217.341938	6821.193499	26.856256
216.997447	6834.218377	26.861274
217.484814	6840.746552	26.866292
217.642551	6852.888276	26.871309
217.741922	6861.983340	26.876327
218.036724	6870.779657	26.881344
218.062957	6887.976931	26.886362
218.073208	6899.920674	26.891380
218.189282	6911.115576	26.896397
218.267749	6936.780720	26.901415
219.122457	6941.856442	26.906432
219.273612	6966.736899	26.911450
219.699383	6978.401340	26.916468
220.353098	6982.927516	26.921485
220.452663	6986.716045	26.926503
220.726286	6980.344171	26.931520
220.806275	6987.993348	26.936538
220.943423	7005.811137	26.941556
221.372214	7008.235187	26.946573
221.578761	7012.597386	26.951591
221.896740	7009.277534	26.956608
221.853430	7030.807425	26.961626
221.775587	7032.423293	26.966644
222.059361	7033.130527	26.971661
222.237834	7058.136284	26.976679
222.651140	7056.029579	26.981696
222.905201	7076.379933	26.986714
222.889827	7093.587035	26.991732
223.083525	7103.545127	26.996749
223.218937	7119.920634	27.001767
223.471481	7120.847397	27.006784
223.604775	7136.538219	27.011802
223.779685	7153.914632	27.016820
224.319811	7164.049270	27.021837
224.387909	7183.292239	27.026855
224.815109	7183.778269	27.031872
224.846614	7198.563198	27.036890
224.913970	7212.446018	27.041908
225.512496	7225.355924	27.046925
225.570605	7237.412395	27.051943
225.698819	7245.941242	27.056960
226.034587	7256.893801	27.061978
226.306114	7269.914628	27.066996
226.475267	7279.560953	27.072013
226.724566	7292.762040	27.077031
227.140412	7301.849091	27.082048
227.354560	7308.991360	27.087066
227.907366	7314.963383	27.092084
228.034062	7330.380752	27.097101
228.353922	7325.671536	27.102119
228.689484	7334.051339	27.107136
228.900149	7347.735166	27.112154
228.896950	7348.720697	27.117172
229.487280	7342.753979	27.122189
229.462069	7343.698741	27.127207
229.585111	7345.892635	27.132224
229.425732	7352.499586	27.137242
229.894867	7369.246378	27.142260
230.039599	7371.269584	27.147277
229.869557	7379.093596	27.152295
229.818928	7388.306980	27.157312
230.323554	7406.159496	27.162330
230.603436	7422.591702	27.167348
231.226021	7434.693010	27.172365
231.089233	7454.511143	27.177383
231.314782	7451.480250	27.182400
231.587510	7463.613947	27.187418
231.628827	7480.380093	27.192436
232.156260	7481.292489	27.197453
232.578092	7501.535117	27.202471
232.684659	7520.210525	27.207488
232.977134	7525.152963	27.212506
233.285285	7534.253739	27.217524
233.723678	7549.613295	27.222541
233.896942	7547.199806	27.227559
234.266642	7557.058135	27.232576
234.512621	7573.284243	27.237594
234.441074	7573.847934	27.242612
234.857870	7574.654441	27.247629
234.939144	7583.168655	27.252647
234.918211	7596.304699	27.257664
234.979306	7610.738094	27.262682
235.471226	7620.874178	27.267700
235.710428	7635.683948	27.272717
235.545437	7650.723973	27.277735
236.324644	7664.278481	27.282752
236.840729	7672.510372	27.287770
236.865401	7683.852567	27.292788
237.473336	7694.491520	27.297805
237.563178	7699.778088	27.302823
237.985514	7699.141028	27.307840
237.917284	7709.541157	27.312858
238.287907	7722.490054	27.317876
238.362978	7715.176508	27.322893
238.504520	7739.421811	27.327911
239.070340	7744.672172	27.332928
238.802713	7740.796191	27.337946
239.039177	7760.875393	27.342964
239.627635	7777.111500	27.347981
239.312471	7790.656537	27.352999
239.807322	7798.591882	27.358016
240.374373	7807.163162	27.363034
240.355574	7819.238302	27.368052
240.555409	7817.174219	27.373069
241.117784	7837.240647	27.378087
241.311293	7850.397154	27.383104
241.371252	7857.907749	27.388122
241.230475	7867.293255	27.393140
241.854797	7882.624143	27.398157
242.148249	7889.918454	27.403175
242.286867	7891.993181	27.408192
242.438369	7918.358640	27.413210
242.602328	7933.287700	27.418228
243.005876	7942.440123	27.423245
243.324404	7957.345138	27.428263
243.641076	7969.974285	27.433280
243.711296	7977.072927	27.438298
244.246374	7978.378781	27.443316
244.416756	7985.812255	27.448333
244.710496	7996.604480	27.453351
244.818296	8002.346099	27.458368
245.299924	8003.597137	27.463386
245.404150	8013.279212	27.468404
245.580040	8009.700333	27.473421
245.641294	8018.047389	27.478439
245.813441	8028.798581	27.483456
246.198531	8029.957314	27.488474
246.029832	8052.824380	27.493492
246.080871	8068.765578	27.498509
246.615506	8085.944804	27.503527
246.986176	8105.678318	27.508544
246.984499	8107.683360	27.513562
247.394467	8122.627942	27.518580
247.669041	8140.955811	27.523597
247.980786	8145.696527	27.528615
247.529667	8162.435780	27.533632
248.502956	8179.622569	27.538650
248.179505	8214.204293	27.543668
248.468078	8220.795483	27.548685
249.103211	8228.882811	27.553703
249.441147	8252.271078	27.558720
249.826007	8259.680742	27.563738
249.866466	8291.437256	27.568756
250.107371	8295.390315	27.573773
250.623517	8313.844911	27.578791
250.423384	8321.702419	27.583808
250.874577	8328.230446	27.588826
251.403422	8350.812489	27.593844
251.805696	8361.269171	27.598861
252.249854	8381.446152	27.603879
252.456744	8378.130724	27.608896
253.191149	8388.797748	27.613914
252.897397	8404.612964	27.618932
253.607342	8394.889358	27.623949
253.568591	8400.230874	27.628967
253.873018	8417.916650	27.633984
254.157784	8423.580337	27.639002
254.184015	8422.184093	27.644020
254.037548	8439.292895	27.649037
254.275607	8441.248020	27.654055
254.479238	8455.366282	27.659072
254.778239	8468.503650	27.664090
254.701592	8487.382200	27.669108
255.297396	8500.362885	27.674125
255.562300	8510.029677	27.679143
255.927187	8539.226250	27.684160
256.226450	8541.575962	27.689178
256.394723	8560.094435	27.694196
256.883279	8576.643568	27.699213
256.855756	8587.552455	27.704231
257.177108	8599.852971	27.709248
257.585934	8611.135928	27.714266
257.483270	8638.189185	27.719284
257.770628	8642.103515	27.724301
257.989816	8655.922743	27.729319
258.209993	8676.535867	27.734336
258.891170	8685.664381	27.739354
258.713199	8709.938604	27.744372
259.018465	8719.116187	27.749389
259.855942	8736.987633	27.754407
259.727342	8749.803451	27.759424
260.351036	8762.233802	27.764442
260.271858	8774.618891	27.769460
260.530045	8777.622234	27.774477
261.053728	8801.597914	27.779495
260.903265	8806.581245	27.784512
261.363149	8824.445262	27.789530
261.620129	8833.715661	27.794548
261.953888	8840.473681	27.799565
262.300215	8844.344146	27.804583
262.265815	8862.588236	27.809600
262.522944	8869.853863	27.814618
262.866589	8883.369744	27.819636
263.050009	8899.205807	27.824653
263.272126	8907.821833	27.829671
263.321284	8921.118391	27.834688
264.025289	8935.547445	27.839706
264.032650	8952.850613	27.844724
264.308736	8962.212817	27.849741
264.823485	8978.834004	27.854759
264.852074	8987.698039	27.859776
265.050419	8990.590762	27.864794
265.518361	9018.032466	27.869812
265.983032	9029.982614	27.874829
266.349466	9029.597317	27.879847
266.673005	9059.378906	27.884864
266.727052	9065.893255	27.889882
266.664467	9079.103138	27.894900
267.003288	9084.098768	27.899917
267.818490	9098.880025	27.904935
267.857576	9117.987458	27.909952
268.316798	9117.098354	27.914970
268.364637	9137.101077	27.919988
268.436702	9143.524248	27.925005
268.662464	9160.266361	27.930023
268.709347	9172.767849	27.935040
269.419745	9186.002695	27.940058
269.436589	9198.249988	27.945076
270.006071	9216.684556	27.950093
270.319333	9222.745014	27.955111
270.449331	9242.959220	27.960128
270.525443	9248.564087	27.965146
271.172411	9259.232602	27.970164
271.514354	9273.831948	27.975181
271.760986	9276.442524	27.980199
271.921667	9290.918558	27.985216
272.086753	9288.240914	27.990234
272.421131	9324.392446	27.995252
272.847910	9319.947072	28.000269
273.276665	9334.870770	28.005287
273.220844	9352.521967	28.010304
273.405782	9359.780084	28.015322
273.872743	9377.245728	28.020340
273.690040	9398.762195	28.025357
274.314425	9405.623564	28.030375
274.742944	9423.379385	28.035392
275.027785	9423.395121	28.040410
275.272124	9438.944327	28.045428
275.374906	9461.177309	28.050445
276.003323	9464.265200	28.055463
275.859599	9482.703724	28.060480
276.016963	9496.119609	28.065498
276.554857	9503.101826	28.070516
276.477671	9517.694001	28.075533
277.088590	9528.611391	28.080551
277.162300	9545.658519	28.085568
277.432874	9556.029038	28.090586
277.788490	9576.682067	28.095604
278.008518	9598.710683	28.100621
278.428299	9602.295193	28.105639
278.742506	9621.685508	28.110656
279.358836	9630.995080	28.115674
279.599406	9642.112271	28.120692
280.076230	9648.441029	28.125709
280.292414	9670.460858	28.130727
280.299002	9670.270492	28.135744
280.437165	9671.815073	28.140762
280.647970	9687.047668	28.145780
280.998975	9696.610117	28.150797
281.283354	9708.692963	28.155815
281.355478	9722.712690	28.160832
281.697314	9725.365338	28.165850
281.697023	9742.998790	28.170868
282.025419	9761.408290	28.175885
282.702975	9777.951176	28.180903
282.681187	9784.231317	28.185920
282.971444	9805.106313	28.190938
283.084917	9810.673961	28.195956
283.471446	9825.153139	28.200973
284.110434	9831.330422	28.205991
284.863215	9827.102543	28.211008
285.320439	9820.663225	28.216026
285.729191	9838.634060	28.221044
285.901806	9859.650566	28.226061
286.237915	9852.592322	28.231079
286.381310	9858.872030	28.236096
286.300266	9863.841678	28.241114
286.543141	9878.497969	28.246132
286.694736	9881.003450	28.251149
286.922708	9896.151455	28.256167
287.297942	9910.771379	28.261184
287.137468	9919.043307	28.266202
287.529500	9926.600920	28.271220
287.715304	9952.695567	28.276237
287.931678	9967.933841	28.281255
288.225991	9985.420623	28.286272
288.542657	10009.553234	28.291290
288.846894	10029.444383	28.296308
289.518195	10048.062839	28.301325
289.889619	10063.678031	28.306343
289.414304	10078.329471	28.311360
289.517914	10097.854105	28.316378
290.405184	10111.841939	28.321396
290.994811	10129.058710	28.326413
290.980550	10141.251479	28.331431
291.094093	10164.449771	28.336448
291.445683	10177.586480	28.341466
292.093529	10197.556922	28.346484
292.145415	10217.610696	28.351501
292.542284	10232.631645	28.356519
292.376657	10251.630034	28.361536
293.150389	10268.900364	28.366554
293.702212	10289.419447	28.371572
293.537411	10303.126030	28.376589
294.097699	10315.276824	28.381607
294.113199	10341.771099	28.386624
294.534615	10360.343524	28.391642
295.219354	10374.378875	28.396660
295.505214	10389.963459	28.401677
295.396224	10403.314116	28.406695
295.482515	10420.678982	28.411712
295.760563	10438.408684	28.416730
296.810690	10450.919025	28.421748
296.722046	10476.643516	28.426765
297.166659	10486.924314	28.431783
297.357523	10508.911188	28.436800
298.082384	10510.983350	28.441818
298.396307	10517.741915	28.446836
299.075577	10530.973100	28.451853
299.641971	10527.733933	28.456871
299.547359	10522.810589	28.461888
300.176164	10537.906186	28.466906
300.602842	10543.415820	28.471924
300.421620	10561.065585	28.476941
301.233163	10553.923587	28.481959
300.837222	10552.071939	28.486976
301.137779	10547.693287	28.491994
301.104259	10559.459921	28.497012
300.919965	10575.335718	28.502029
301.749793	10584.909329	28.507047
301.849931	10600.052551	28.512064
301.808512	10623.550234	28.517082
302.036791	10634.913055	28.522100
301.913774	10656.409052	28.527117
302.180342	10673.578744	28.532135
302.907626	10693.739428	28.537152
303.008731	10729.844761	28.542170
303.521806	10747.670779	28.547188
303.496188	10769.739026	28.552205
304.292327	10787.438920	28.557223
304.255655	10821.772453	28.562240
304.480772	10834.114696	28.567258
305.176137	10856.929626	28.572276
305.460618	10881.721971	28.577293
305.849746	10893.022018	28.582311
306.430147	10917.660987	28.587328
306.312179	10936.330590	28.592346
306.601161	10956.619788	28.597364
307.242343	10976.112169	28.602381
307.652737	10981.052967	28.607399
308.128101	11000.713276	28.612416
308.158231	11014.642631	28.617434
309.126884	11027.390229	28.622452
308.888865	11043.277943	28.627469
309.415780	11044.155881	28.632487
309.845998	11061.887745	28.637504
309.644859	11079.550571	28.642522
310.415237	11087.835971	28.647540
310.501424	11103.925862	28.652557
311.000201	11114.867964	28.657575
311.059286	11142.149120	28.662592
311.287962	11150.171558	28.667610
312.162971	11153.363435	28.672628
312.238388	11170.879094	28.677645
312.610282	11170.666573	28.682663
312.942752	11191.094501	28.687680
313.288000	11208.224018	28.692698
313.733998	11215.170671	28.697716
313.563644	11239.522785	28.702733
313.998239	11246.164945	28.707751
314.259812	11257.737674	28.712768
314.593165	11277.903484	28.717786
314.793614	11289.318400	28.722804
315.335601	11311.017898	28.727821
315.243791	11330.646868	28.732839
315.660682	11352.160650	28.737856
316.034251	11367.871329	28.742874
316.505476	11372.313343	28.747892
316.574828	11398.753369	28.752909
316.994846	11421.722372	28.757927
317.437074	11434.299602	28.762944
317.735422	11457.290749	28.767962
318.340598	11467.550250	28.772980
318.130352	11488.432428	28.777997
318.464048	11498.510024	28.783015
318.709926	11517.303543	28.788032
319.047358	11541.526473	28.793050
319.909611	11542.052260	28.798068
320.080217	11568.220999	28.803085
320.251121	11571.753071	28.808103
320.919912	11589.410404	28.813120
321.220729	11609.186940	28.818138
321.555565	11612.930317	28.823156
321.805540	11625.891257	28.828173
321.857975	11645.292857	28.833191
322.228542	11659.327571	28.838208
322.331345	11670.874752	28.843226
322.663685	11675.120587	28.848244
322.768520	11698.012695	28.853261
323.082524	11714.320250	28.858279
323.190112	11733.845975	28.863296
323.547182	11748.984859	28.868314
323.950967	11771.495809	28.873332
324.097362	11796.017206	28.878349
324.734673	11821.873662	28.883367
325.062462	11833.303818	28.888384
325.455113	11857.755382	28.893402
326.178352	11872.060585	28.898420
326.322588	11885.496021	28.903437
326.609821	11898.858683	28.908455
327.035789	11914.466935	28.913472
327.037935	11934.078751	28.918490
327.803653	11935.560557	28.923508
328.207056	11953.287969	28.928525
328.887581	11969.361858	28.933543
329.402414	11970.118576	28.938560
329.416970	11988.667551	28.943578
329.938383	11995.312252	28.948596
329.834290	12017.880462	28.953613
330.237422	12028.026476	28.958631
330.416275	12041.788189	28.963648
330.291537	12049.572372	28.968666
330.722002	12066.477846	28.973684
331.225698	12095.724701	28.978701
331.434793	12120.486216	28.983719
331.631735	12132.315846	28.988736
332.396003	12156.425755	28.993754
332.665765	12176.498230	28.998772
333.036443	12196.987618	29.003789
332.915177	12216.230548	29.008807
333.509913	12237.622929	29.013824
333.882389	12259.656214	29.018842
334.452460	12273.455078	29.023860
334.629860	12294.839871	29.028877
334.730508	12307.714011	29.033895
335.174596	12325.858573	29.038912
335.402800	12346.228208	29.043930
335.820055	12369.031445	29.048948
336.187807	12390.677220	29.053965
336.589469	12409.355806	29.058983
337.117075	12425.700196	29.064000
337.371248	12455.775888	29.069018
337.995338	12470.924309	29.074036
338.356514	12485.400027	29.079053
338.307349	12508.326571	29.084071
339.192945	12512.208584	29.089088
339.405210	12526.154914	29.094106
339.784290	12532.436722	29.099124
340.534479	12551.168552	29.104141
340.743544	12551.612917	29.109159
341.027585	12568.835310	29.114176
341.281942	12579.292139	29.119194
341.838449	12575.744709	29.124212
342.260143	12583.917704	29.129229
342.662749	12590.887415	29.134247
343.097863	12597.267885	29.139264
343.141608	12614.373000	29.144282
343.522870	12610.312872	29.149300
343.670769	12620.944185	29.154317
343.942022	12638.493881	29.159335
344.139694	12648.249078	29.164352
344.604794	12655.449074	29.169370
344.544373	12670.063199	29.174388
344.944139	12678.015448	29.179405
345.024932	12692.512872	29.184423
345.511205	12702.747357	29.189440
345.661593	12721.885355	29.194458
345.293637	12739.218882	29.199476
345.617853	12767.282142	29.204493
346.021602	12796.166716	29.209511
346.855406	12817.235182	29.214528
347.850872	12827.693609	29.219546
348.301417	12837.908467	29.224564
348.648931	12847.428869	29.229581
349.002750	12881.152762	29.234599
349.340246	12881.813975	29.239616
349.522928	12905.721717	29.244634
349.502644	12912.192139	29.249652
350.108015	12928.471179	29.254669
350.142836	12965.996354	29.259687
350.392207	12974.891064	29.264704
350.801967	12994.557365	29.269722
351.054525	13021.909022	29.274740
351.251829	13049.323003	29.279757
351.877518	13067.787370	29.284775
352.096713	13086.738189	29.289792
352.297337	13119.715848	29.294810
352.820684	13139.958290	29.299828
353.013987	13162.535253	29.304845
353.029284	13196.943980	29.309863
354.015220	13213.685064	29.314880
354.100784	13250.328179	29.319898
354.519414	13264.258718	29.324916
355.240836	13278.353703	29.329933
355.481256	13312.869697	29.334951
355.996262	13327.764217	29.339968
356.453814	13350.761315	29.344986
356.597502	13369.834698	29.350004
357.372922	13377.836129	29.355021
357.351695	13408.237267	29.360039
357.645256	13424.451595	29.365056
358.251646	13450.090897	29.370074
358.855319	13476.030657	29.375092
359.030581	13482.903463	29.380109
359.523606	13506.460491	29.385127
359.427761	13511.218670	29.390144
359.659416	13542.941709	29.395162
359.622213	13578.966677	29.400180
360.620016	13597.301000	29.405197
360.641023	13623.502200	29.410215
361.368582	13634.148053	29.415232
361.833227	13661.821304	29.420250
362.326826	13681.251056	29.425268
362.504509	13707.475350	29.430285
362.591500	13731.212715	29.435303
363.222529	13740.357847	29.440320
363.553907	13772.785755	29.445338
363.786913	13795.395189	29.450356
364.280358	13817.281986	29.455373
364.449838	13842.149825	29.460391
365.177529	13863.690730	29.465408
365.774041	13880.451981	29.470426
365.749109	13902.637479	29.475444
365.938855	13913.948284	29.480461
366.101077	13941.991139	29.485479
366.962575	13960.293351	29.490496
367.256730	13985.195654	29.495514
367.481661	14007.910812	29.500532
368.094564	14029.791890	29.505549
368.049367	14049.909077	29.510567
368.585539	14050.154130	29.515584
368.652185	14079.911066	29.520602
369.113250	14099.583163	29.525620
369.867249	14118.205431	29.530637
370.037335	14138.661841	29.535655
370.221233	14163.177318	29.540672
370.717345	14178.694420	29.545690
370.987681	14202.012238	29.550708
371.800355	14213.545202	29.555725
371.909559	14256.442610	29.560743
371.888277	14266.829598	29.565760
372.458440	14284.100594	29.570778
372.795612	14317.175927	29.575796
373.317743	14328.192064	29.580813
373.353614	14360.632244	29.585831
373.871972	14387.331833	29.590848
375.003477	14414.776045	29.595866
374.634236	14434.994616	29.600884
375.207217	14450.070479	29.605901
375.167494	14477.002348	29.610919
376.174247	14503.506060	29.615936
376.541028	14521.045790	29.620954
376.798775	14541.517408	29.625972
377.140599	14565.089820	29.630989
377.417282	14586.651232	29.636007
377.855702	14606.488443	29.641024
378.382106	14623.542337	29.646042
379.091001	14640.612050	29.651060
379.582203	14660.643217	29.656077
380.022756	14678.793751	29.661095
380.128943	14690.702275	29.666112
380.777766	14711.899559	29.671130
380.865281	14727.758635	29.676148
381.692172	14739.412874	29.681165
381.333987	14762.327091	29.686183
381.895375	14783.718079	29.691200
382.630144	14810.504581	29.696218
382.732162	14826.045670	29.701236
383.399634	14848.067630	29.706253
383.673163	14879.382144	29.711271
383.748217	14883.343476	29.716288
384.139428	14910.069912	29.721306
384.481773	14933.055286	29.726324
385.096232	14950.440003	29.731341
385.167540	14987.369764	29.736359
385.707079	14996.390792	29.741376
386.034388	15021.197705	29.746394
386.539697	15047.091767	29.751412
387.115341	15065.477451	29.756429
387.539807	15074.090079	29.761447
387.826483	15092.394449	29.766464
388.193271	15112.537049	29.771482
388.522686	15134.851991	29.776500
389.018942	15163.880525	29.781517
389.454555	15183.390325	29.786535
389.859329	15207.206386	29.791552
390.384493	15206.685736	29.796570
391.022622	15242.062351	29.801588
391.236835	15255.015560	29.806605
391.615527	15275.554411	29.811623
392.014639	15294.005697	29.816640
392.571728	15301.151329	29.821658
392.553352	15320.924598	29.826676
393.175843	15338.137876	29.831693
393.127897	15363.957433	29.836711
393.888643	15384.051621	29.841728
393.820281	15383.048573	29.846746
393.964414	15413.067136	29.851764
394.523359	15430.214594	29.856781
394.982233	15465.527942	29.861799
394.944812	15473.508376	29.866816
395.816936	15485.595028	29.871834
395.786173	15517.937013	29.876852
396.002639	15540.740591	29.881869
396.760343	15556.022285	29.886887
397.455074	15579.935792	29.891904
398.149866	15598.805603	29.896922
398.277233	15613.335907	29.901940
398.673708	15629.166583	29.906957
399.006386	15646.065218	29.911975
399.202369	15669.803824	29.916992
400.180704	15687.672629	29.922010
400.535965	15705.869005	29.927028
401.035207	15730.485845	29.932045
401.041085	15746.282679	29.937063
401.725150	15761.155952	29.942080
402.508740	15779.307824	29.947098
402.625530	15797.655110	29.952116
403.079304	15817.304855	29.957133
403.049283	15837.244701	29.962151
403.313656	15864.661777	29.967168
404.033118	15877.056691	29.972186
404.424751	15900.670376	29.977204
404.518657	15923.679830	29.982221
405.022589	15950.715481	29.987239
405.339166	15967.509525	29.992256
406.109637	15987.520721	29.997274
406.207816	16018.046400	30.002292
406.576903	16033.019455	30.007309
407.161300	16063.141046	30.012327
407.647340	16094.929802	30.017344
407.735403	16109.504501	30.022362
408.234754	16141.436545	30.027380
408.634200	16168.924620	30.032397
408.791416	16199.564572	30.037415
409.269933	16228.423778	30.042432
410.082680	16247.847529	30.047450
410.461019	16272.594432	30.052468
410.729765	16291.502831	30.057485
411.552028	16322.522673	30.062503
411.580298	16345.994499	30.067520
412.410863	16367.269560	30.072538
412.750168	16391.302585	30.077556
413.406671	16395.868554	30.082573
413.713552	16426.728763	30.087591
413.801376	16447.566828	30.092608
414.362448	16459.721476	30.097626
414.771202	16495.385635	30.102644
414.945257	16510.130438	30.107661
415.199954	16535.737063	30.112679
415.908376	16560.881443	30.117696
416.153935	16579.073620	30.122714
416.585933	16607.226838	30.127732
416.698455	16632.201934	30.132749
417.298965	16654.997586	30.137767
417.642356	16688.862506	30.142784
418.429603	16711.180657	30.147802
418.946163	16746.010466	30.152820
418.784813	16774.445808	30.157837
419.515311	16794.220873	30.162855
419.776360	16816.987445	30.167872
420.671446	16831.127527	30.172890
421.015365	16864.591552	30.177908
421.315141	16877.355667	30.182925
422.068674	16893.476075	30.187943
421.745138	16920.600854	30.192960
422.464316	16937.986874	30.197978
422.784628	16963.214313	30.202996
423.204745	16987.965111	30.208013
423.818854	17009.299852	30.213031
423.599997	17034.118600	30.218048
424.273217	17045.580247	30.223066
424.784397	17075.999092	30.228084
424.941247	17108.042917	30.233101
425.725728	17129.316525	30.238119
426.024389	17161.455227	30.243136
426.757217	17187.547339	30.248154
426.839065	17219.280859	30.253172
427.301225	17238.336956	30.258189
427.756793	17253.875511	30.263207
427.907755	17286.564887	30.268224
428.573023	17309.250162	30.273242
428.731949	17349.139845	30.278260
428.955856	17377.266575	30.283277
429.636942	17413.291173	30.288295
429.773914	17446.128291	30.293312
430.452513	17479.850820	30.298330
431.130769	17502.060517	30.303348
431.757962	17525.115209	30.308365
432.294840	17549.576915	30.313383
432.734546	17586.157420	30.318400
433.267867	17606.175643	30.323418
433.867376	17624.654831	30.328436
434.182683	17652.009674	30.333453
434.555533	17677.555204	30.338471
434.921120	17708.635748	30.343488
435.437422	17732.725018	30.348506
436.046437	17750.836450	30.353524
436.347012	17767.403983	30.358541
436.876679	17788.326325	30.363559
437.081502	17824.662733	30.368576
437.498971	17850.277351	30.373594
438.160119	17878.273569	30.378612
438.670881	17899.540105	30.383629
439.318065	17921.423469	30.388647
439.363915	17946.578054	30.393664
439.893902	17967.519492	30.398682
440.109189	18000.279028	30.403700
440.495209	18026.063025	30.408717
440.971208	18062.907268	30.413735
441.427113	18089.400641	30.418752
441.655148	18114.015380	30.423770
441.906127	18154.628361	30.428788
442.319671	18190.686587	30.433805
443.441774	18216.343610	30.438823
443.592326	18240.458866	30.443840
444.113828	18273.682900	30.448858
444.333179	18288.475710	30.453876
444.749950	18330.509928	30.458893
445.921408	18345.287223	30.463911
446.821180	18365.293408	30.468928
447.464201	18389.136343	30.473946
447.543155	18408.903948	30.478964
447.797493	18418.403739	30.483981
448.527544	18438.227947	30.488999
448.684054	18461.786619	30.494016
448.957209	18479.483533	30.499034
449.306277	18514.320500	30.504052
449.559473	18537.030309	30.509069
450.220214	18557.787777	30.514087
450.470650	18585.804739	30.519104
451.000009	18596.929614	30.524122
451.724956	18613.280188	30.529140
451.933797	18646.111312	30.534157
452.694825	18659.265976	30.539175
453.008718	18684.373473	30.544192
453.544644	18695.225731	30.549210
454.143735	18706.320861	30.554228
454.088731	18727.170986	30.559245
454.579129	18753.489327	30.564263
454.661776	18779.157300	30.569280
455.569246	18803.768222	30.574298
455.566956	18834.408760	30.579316
456.062464	18855.868250	30.584333
456.479030	18880.378801	30.589351
457.254857	18910.443458	30.594368
457.488659	18938.981560	30.599386
457.702514	18959.872207	30.604404
458.241763	18995.160567	30.609421
459.395294	19003.124471	30.614439
459.615580	19032.359751	30.619456
460.228695	19056.561951	30.624474
460.668838	19081.694531	30.629492
461.077148	19115.240875	30.634509
461.912333	19131.998008	30.639527
462.192942	19159.240347	30.644544
462.574814	19179.277461	30.649562
462.741932	19202.418415	30.654580
462.803081	19228.898990	30.659597
463.584419	19249.707921	30.664615
463.926086	19285.482442	30.669632
464.157588	19316.712795	30.674650
464.712409	19349.377527	30.679668
465.173316	19391.899954	30.684685
465.491040	19418.170265	30.689703
465.957212	19458.303913	30.694720
466.649263	19487.232675	30.699738
467.241399	19521.957796	30.704756
467.407816	19551.006390	30.709773
468.081324	19583.621449	30.714791
468.448762	19630.410822	30.719808
468.913553	19661.327426	30.724826
469.548870	19695.161638	30.729844
469.830184	19728.299197	30.734861
470.454043	19756.354479	30.739879
471.028857	19792.978133	30.744896
471.042895	19826.947202	30.749914
471.935695	19854.069936	30.754932
472.463449	19894.011675	30.759949
472.886408	19913.733572	30.764967
473.447247	19952.621510	30.769984
474.099784	19983.743159	30.775002
475.227017	20007.872825	30.780020
475.580686	20036.179064	30.785037
476.392222	20048.101132	30.790055
476.329270	20070.274379	30.795072
476.799289	20100.628568	30.800090
477.648229	20116.146092	30.805108
477.943110	20147.020419	30.810125
478.397996	20165.240240	30.815143
478.456929	20187.811632	30.820160
478.965955	20211.058504	30.825178
479.590661	20251.832495	30.830196
479.752707	20278.722093	30.835213
480.275557	20301.316165	30.840231
480.642764	20332.552289	30.845248
481.065154	20368.012961	30.850266
481.540842	20386.198160	30.855284
481.806121	20434.951324	30.860301
482.117405	20461.091362	30.865319
482.876843	20496.303936	30.870336
483.076683	20524.293653	30.875354
483.673315	20552.486999	30.880372
483.816494	20587.132273	30.885389
484.648659	20600.491999	30.890407
485.118104	20635.036021	30.895424
485.817487	20672.577016	30.900442
486.402406	20705.150879	30.905460
487.009304	20745.391627	30.910477
487.231255	20767.293855	30.915495
487.438525	20799.282213	30.920512
488.200963	20828.751690	30.925530
489.073924	20854.375175	30.930548
489.238141	20896.435291	30.935565
489.877314	20913.268704	30.940583
490.365699	20942.945291	30.945600
490.636833	20979.801675	30.950618
491.326844	21007.425134	30.955636
491.768106	21045.247120	30.960653
492.188653	21068.382421	30.965671
492.860552	21102.680928	30.970688
492.880135	21126.636912	30.975706
493.628406	21151.496730	30.980724
493.814371	21201.262436	30.985741
494.441149	21230.494587	30.990759
494.883445	21260.267285	30.995776
495.828712	21302.636325	31.000794
496.314478	21330.728002	31.005812
496.570242	21366.854575	31.010829
497.032884	21403.069057	31.015847
497.975030	21428.998443	31.020864
498.383175	21460.470089	31.025882
499.390833	21488.626069	31.030900
499.492463	21520.069707	31.035917
500.634949	21537.773066	31.040935
501.234526	21561.689835	31.045952
501.605936	21586.103399	31.050970
501.972061	21603.093646	31.055988
502.651947	21633.057386	31.061005
502.845890	21653.176841	31.066023
503.406369	21671.331079	31.071040
503.373717	21703.794232	31.076058
504.309381	21723.254901	31.081076
504.827807	21765.546064	31.086093
505.380218	21787.638088	31.091111
505.893338	21816.124266	31.096128
505.949923	21854.551087	31.101146
506.545488	21879.884217	31.106164
506.826478	21914.857895	31.111181
507.232601	21957.482881	31.116199
507.722313	21982.668339	31.121216
508.307342	22021.158545	31.126234
508.608777	22052.736210	31.131252
509.204048	22097.309769	31.136269
509.410505	22129.047670	31.141287
510.119843	22163.784503	31.146304
510.733475	22205.922780	31.151322
511.294515	22240.354266	31.156340
511.559666	22281.314818	31.161357
511.916076	22321.844215	31.166375
512.676400	22354.241857	31.171392
513.231247	22401.286681	31.176410
514.031341	22444.129407	31.181428
514.215001	22476.699167	31.186445
514.989031	22509.979551	31.191463
515.528365	22545.861939	31.196480
515.883751	22585.456862	31.201498
516.633001	22613.256599	31.206516
517.331933	22646.365661	31.211533
517.546010	22667.809958	31.216551
518.139520	22688.759213	31.221568
518.369461	22714.251435	31.226586
519.047621	22747.572420	31.231604
519.567703	22776.779245	31.236621
520.126442	22810.510694	31.241639
520.902523	22845.737525	31.246656
521.003916	22875.755299	31.251674
521.985658	22902.426089	31.256692
522.495539	22927.843412	31.261709
523.190556	22955.544653	31.266727
523.959102	22973.945732	31.271744
523.588651	23012.302264	31.276762
523.972981	23037.530749	31.281780
524.673887	23076.175580	31.286797
525.238935	23108.674368	31.291815
525.993950	23140.871921	31.296832
526.177546	23189.233880	31.301850
526.919674	23210.792447	31.306868
527.305344	23248.993812	31.311885
528.031602	23286.876831	31.316903
528.454293	23325.382210	31.321920
528.974069	23364.681381	31.326938
529.495660	23399.923540	31.331956
530.162477	23440.798682	31.336973
530.448939	23468.545287	31.341991
531.009323	23499.908014	31.347008
531.636755	23551.222264	31.352026
532.596443	23577.764699	31.357044
533.028501	23617.697296	31.362061
533.401155	23648.748253	31.367079
533.719958	23679.308433	31.372096
534.055560	23723.193060	31.377114
534.704582	23759.414438	31.382132
535.638479	23794.504643	31.387149
536.207486	23824.937628	31.392167
537.000531	23861.079899	31.397184
537.345513	23891.573138	31.402202
537.851733	23925.251467	31.407220
538.835099	23957.206263	31.412237
538.874039	23994.098091	31.417255
539.957285	24024.274389	31.422272
540.222672	24055.848218	31.427290
540.772626	24090.777544	31.432308
541.264692	24119.573637	31.437325
541.732988	24150.920132	31.442343
542.255551	24176.792066	31.447360
542.815231	24209.849585	31.452378
543.595348	24235.908995	31.457396
544.460548	24263.642444	31.462413
544.987682	24300.098638	31.467431
545.568936	24324.735684	31.472448
545.936474	24359.213611	31.477466
546.239553	24378.415179	31.482484
547.067375	24411.721979	31.487501
547.465841	24444.343673	31.492519
548.024781	24465.843652	31.497536
548.444768	24501.280520	31.502554
548.861556	24539.473197	31.507572
549.561245	24558.670071	31.512589
549.928754	24606.077888	31.517607
550.633328	24629.223693	31.522624
550.767109	24675.707512	31.527642
551.292415	24712.000438	31.532660
551.718595	24748.991361	31.537677
551.823039	24784.300909	31.542695
552.705006	24826.573599	31.547712
553.073667	24872.762212	31.552730
553.432520	24911.141563	31.557748
554.038538	24948.869518	31.562765
554.482746	24977.674300	31.567783
555.298379	25019.363689	31.572800
555.745988	25051.871292	31.577818
556.399296	25089.099226	31.582836
557.231262	25120.851955	31.587853
557.157945	25166.067322	31.592871
558.189881	25200.936196	31.597888
558.548188	25252.214561	31.602906
559.271954	25291.681681	31.607924
559.883289	25326.527777	31.612941
560.320432	25373.989767	31.617959
561.045231	25406.050336	31.622976
561.695308	25445.921049	31.627994
562.486784	25478.773952	31.633012
563.279519	25513.187674	31.638029
563.751943	25547.746114	31.643047
564.971778	25569.668931	31.648064
565.373868	25607.120207	31.653082
565.628682	25632.915634	31.658100
566.654682	25656.391774	31.663117
567.068471	25682.023481	31.668135
567.894213	25701.890683	31.673152
568.201157	25731.861791	31.678170
568.516880	25765.705591	31.683188
569.654054	25792.507738	31.688205
569.814323	25827.405965	31.693223
570.728446	25851.177821	31.698240
571.210805	25882.189890	31.703258
571.000324	25910.080443	31.708276
571.876630	25941.783333	31.713293
572.537501	25981.356399	31.718311
573.209366	26012.661479	31.723328
574.014871	26049.481992	31.728346
574.200152	26083.435111	31.733364
574.693240	26106.508111	31.738381
575.164759	26146.148897	31.743399
576.038346	26175.830219	31.748416
576.359133	26224.216075	31.753434
576.943921	26257.835538	31.758452
577.777822	26288.686069	31.763469
578.007916	26331.170851	31.768487
578.617298	26360.830376	31.773504
579.130251	26403.555674	31.778522
579.404623	26456.278486	31.783540
580.300399	26487.479928	31.788557
580.755074	26529.121206	31.793575
581.480626	26555.546053	31.798592
582.899022	26583.247161	31.803610
583.516356	26621.892900	31.808628
584.131901	26645.693219	31.813645
584.505095	26676.514944	31.818663
584.651861	26706.512437	31.823680
585.472024	26732.335023	31.828698
586.007913	26774.659372	31.833716
586.633203	26811.345012	31.838733
587.071945	26850.594119	31.843751
587.437271	26886.877959	31.848768
588.150902	26916.623195	31.853786
588.715600	26952.136660	31.858804
589.549411	26997.202276	31.863821
589.920066	27035.052948	31.868839
590.541594	27056.571242	31.873856
591.023658	27089.778313	31.878874
591.308994	27127.680361	31.883892
592.056646	27164.208549	31.888909
592.615801	27205.259817	31.893927
592.834446	27235.531314	31.898944
593.806975	27276.233965	31.903962
594.146667	27303.162276	31.908980
594.886590	27342.953236	31.913997
595.307007	27375.386660	31.919015
595.686009	27421.427820	31.924032
596.788748	27459.563497	31.929050
597.099979	27488.986680	31.934068
597.911315	27536.641999	31.939085
598.161974	27572.982840	31.944103
598.587118	27606.692604	31.949120
599.337503	27647.670757	31.954138
599.897010	27695.991367	31.959156
600.703340	27724.750025	31.964173
601.475182	27783.700263	31.969191
601.581134	27822.699681	31.974208
602.423205	27864.220194	31.979226
602.857137	27912.308051	31.984244
603.408475	27954.057299	31.989261
604.161109	27998.290838	31.994279
605.230800	28043.682327	31.999296
605.579642	28088.573047	32.004314
606.032243	28128.915915	32.009332
607.033895	28168.092584	32.014349
607.188040	28209.733535	32.019367
607.943973	28257.045219	32.024384
608.430195	28304.531732	32.029402
609.087251	28350.493787	32.034420
609.410044	28393.701643	32.039437
610.133627	28435.431385	32.044455
610.898216	28486.888566	32.049472
611.535254	28526.609372	32.054490
611.625266	28584.429230	32.059508
613.150355	28627.677959	32.064525
614.064745	28671.698162	32.069543
614.758230	28706.145416	32.074560
615.589515	28750.494760	32.079578
615.825776	28798.103503	32.084596
616.544232	28816.486148	32.089613
617.274680	28865.332825	32.094631
617.647490	28902.415509	32.099648
618.339883	28939.928886	32.104666
618.861033	28990.489763	32.109684
619.627708	29033.775251	32.114701
619.847030	29075.192914	32.119719
620.644212	29122.632922	32.124736
621.312070	29151.579495	32.129754
621.740012	29198.021583	32.134772
622.671182	29235.574182	32.139789
623.079206	29277.917326	32.144807
623.609020	29318.465435	32.149824
624.455486	29366.827504	32.154842
624.743737	29408.437378	32.159860
625.333889	29462.503098	32.164877
626.039147	29512.069503	32.169895
626.457955	29557.508800	32.174912
627.397493	29600.452529	32.179930
627.526448	29648.996492	32.184948
628.372222	29697.707104	32.189965
629.204803	29744.302351	32.194983
629.655111	29800.280709	32.200000
630.477723	29839.172408	32.205018
630.710766	29894.546420	32.210036
631.616273	29930.998108	32.215053
632.624172	29975.746125	32.220071
633.116171	30026.598544	32.225088
634.012878	30060.738316	32.230106
634.395239	30107.941768	32.235124
635.234808	30132.254910	32.240141
635.575738	30176.367623	32.245159
635.965409	30209.385558	32.250176
637.435179	30220.686614	32.255194
638.198566	30261.054838	32.260212
638.802696	30296.681773	32.265229
639.455094	30326.024326	32.270247
639.544584	30369.272666	32.275264
640.350357	30388.338465	32.280282
640.879507	30433.958480	32.285300
641.587798	30470.290118	32.290317
642.149371	30510.450043	32.295335
642.688754	30557.478373	32.300352
643.280452	30595.490870	32.305370
643.966518	30634.057662	32.310388
644.365402	30680.412805	32.315405
644.964818	30719.290345	32.320423
645.434418	30770.204979	32.325440
646.217194	30817.094871	32.330458
646.404522	30865.114264	32.335476
646.985243	30913.097813	32.340493
648.242040	30968.068807	32.345511
648.412236	31029.562098	32.350528
649.298935	31076.360544	32.355546
649.717204	31127.916191	32.360564
650.644942	31181.402873	32.365581
651.385478	31230.493818	32.370599
651.815608	31285.992599	32.375616
652.649412	31334.209551	32.380634
653.137799	31381.892488	32.385652
653.972005	31431.462406	32.390669
654.882151	31491.874689	32.395687
655.187769	31540.654782	32.400704
656.293404	31588.918513	32.405722
656.362355	31632.318087	32.410740
657.315368	31680.985086	32.415757
658.417949	31732.808684	32.420775
659.240049	31784.341029	32.425792
659.752537	31818.372842	32.430810
660.638882	31872.847608	32.435828
661.417232	31908.993865	32.440845
662.501764	31960.947277	32.445863
662.473879	32008.073533	32.450880
663.049353	32048.430252	32.455898
663.985866	32098.004803	32.460916
664.276070	32144.841627	32.465933
665.194059	32181.952812	32.470951
665.801881	32229.024860	32.475968
666.247535	32276.912480	32.480986
666.622002	32313.027487	32.486004
667.638336	32362.508061	32.491021
668.471738	32405.025306	32.496039
669.228653	32471.027487	32.501056
670.247732	32505.398805	32.506074
670.616427	32553.501341	32.511092
671.124903	32600.336820	32.516109
671.820993	32641.788563	32.521127
672.419443	32698.213196	32.526144
673.241644	32743.236349	32.531162
673.759571	32779.759723	32.536180
674.719748	32823.067294	32.541197
675.390591	32871.515488	32.546215
675.745946	32911.800674	32.551232
676.645827	32968.944073	32.556250
677.124478	33014.786253	32.561268
678.030339	33065.986313	32.566285
678.441826	33099.934793	32.571303
678.942554	33154.163165	32.576320
679.663026	33183.145136	32.581338
680.235159	33228.789893	32.586356
681.134724	33271.172166	32.591373
681.961147	33311.473301	32.596391
682.217120	33359.076829	32.601408
683.250538	33390.210462	32.606426
683.870890	33434.210736	32.611444
684.321078	33481.910753	32.616461
685.206344	33525.484329	32.621479
685.483978	33574.159739	32.626496
686.128994	33615.804711	32.631514
686.816082	33673.014772	32.636532
687.659080	33712.808325	32.641549
688.418600	33767.111798	32.646567
688.834911	33827.481288	32.651584
689.382833	33877.006761	32.656602
690.369735	33920.628560	32.661620
690.651658	33975.537991	32.666637
691.414746	34030.878446	32.671655
692.047831	34081.845274	32.676672
692.821918	34145.005024	32.681690
694.122765	34197.404510	32.686708
694.580086	34250.403293	32.691725
695.938540	34287.753132	32.696743
696.722669	34342.010005	32.701760
697.385498	34386.062566	32.706778
697.909605	34426.014595	32.711796
698.324218	34479.102795	32.716813
699.399026	34511.477175	32.721831
699.942222	34566.442312	32.726848
700.933369	34603.186034	32.731866
701.372439	34659.697662	32.736884
702.247126	34710.653695	32.741901
703.008394	34747.427131	32.746919
703.298759	34800.288904	32.751936
704.556111	34843.326783	32.756954
705.143266	34891.033967	32.761972
706.004485	34946.443749	32.766989
706.901724	34989.866760	32.772007
707.304601	35036.445926	32.777024
708.134621	35080.720495	32.782042
709.036394	35127.746976	32.787060
709.667142	35173.001154	32.792077
709.967297	35208.234902	32.797095
710.347648	35261.924735	32.802112
711.522462	35313.802874	32.807130
712.097421	35358.497092	32.812148
712.966133	35406.490391	32.817165
713.746354	35455.199397	32.822183
714.237137	35501.203180	32.827200
715.460098	35536.824934	32.832218
716.191917	35581.564755	32.837236
716.699258	35638.428772	32.842253
717.517841	35680.139329	32.847271
717.865753	35728.612768	32.852288
718.539145	35770.561081	32.857306
719.178439	35817.231619	32.862324
719.641186	35872.800703	32.867341
720.104353	35922.812065	32.872359
721.137649	35993.423273	32.877376
721.693801	36030.540697	32.882394
722.287483	36094.467820	32.887412
722.922960	36155.233485	32.892429
723.920039	36211.023775	32.897447
724.725016	36270.574669	32.902464
725.726225	36311.903954	32.907482
726.577769	36357.259074	32.912500
726.923657	36405.740696	32.917517
727.633197	36449.663827	32.922535
728.385165	36499.669529	32.927552
729.344050	36545.476246	32.932570
729.991721	36588.764344	32.937588
730.199456	36637.331231	32.942605
730.928307	36682.118097	32.947623
731.601395	36735.279209	32.952640
732.080703	36780.737440	32.957658
733.087221	36838.121334	32.962676
733.493102	36892.323489	32.967693
734.551337	36948.163103	32.972711
735.165823	37008.314800	32.977728
735.900752	37066.506693	32.982746
736.600922	37111.223048	32.987764
737.498029	37173.645514	32.992781
738.541385	37236.127599	32.997799
738.965922	37287.570914	33.002816
739.768470	37337.311453	33.007834
740.958035	37384.936790	33.012852
742.205230	37445.357977	33.017869
743.185958	37484.511184	33.022887
743.774377	37527.791442	33.027904
744.265054	37575.026454	33.032922
744.861804	37620.740096	33.037940
745.316607	37669.163370	33.042957
746.538136	37708.266856	33.047975
746.960305	37766.629487	33.052992
747.618725	37827.149731	33.058010
748.711318	37880.495003	33.063028
749.287917	37941.445654	33.068045
749.913528	37989.526889	33.073063
750.769756	38055.120032	33.078080
751.274228	38106.546547	33.083098
752.179670	38152.870916	33.088116
752.597572	38212.930130	33.093133
753.529073	38260.559649	33.098151
753.987312	38331.110023	33.103168
754.749921	38396.510104	33.108186
755.666114	38456.973025	33.113204
756.614483	38514.010022	33.118221
757.437634	38571.604174	33.123239
758.264281	38641.946450	33.128256
758.860235	38685.695823	33.133274
759.915351	38735.191609	33.138292
760.422471	38801.321975	33.143309
761.307939	38849.288798	33.148327
761.931047	38910.178041	33.153344
762.101534	38977.120198	33.158362
763.303486	39036.288158	33.163380
763.799482	39097.014325	33.168397
764.765312	39154.391787	33.173415
765.592922	39221.586543	33.178432
766.158588	39287.778847	33.183450
767.253313	39344.371562	33.188468
767.861017	39414.016869	33.193485
768.831251	39469.921016	33.198503
769.386760	39531.992459	33.203520
770.045819	39598.689739	33.208538
770.973979	39657.465670	33.213556
771.736152	39728.599372	33.218573
772.621000	39784.561892	33.223591
773.402732	39835.253728	33.228608
774.384945	39899.865298	33.233626
775.485289	39956.041353	33.238644
776.064246	40021.455973	33.243661
776.799839	40076.715214	33.248679
777.679881	40122.175045	33.253696
778.039347	40187.674927	33.258714
779.326304	40227.202851	33.263732
779.859387	40265.115386	33.268749
781.043041	40309.193953	33.273767
781.942222	40356.959615	33.278784
782.628982	40401.596357	33.283802
783.475996	40435.292684	33.288820
784.109616	40486.894488	33.293837
784.770883	40535.551346	33.298855
785.854447	40579.930635	33.303872
786.117591	40637.092551	33.308890
787.282520	40681.585867	33.313908
788.041083	40719.312313	33.318925
788.980320	40764.479683	33.323943
790.134982	40815.381377	33.328960
790.582301	40863.553681	33.333978
791.476874	40901.746244	33.338996
792.185054	40957.891075	33.344013
793.004402	40999.377855	33.349031
793.696909	41047.189855	33.354048
794.273567	41094.147230	33.359066
795.396434	41142.626075	33.364084
795.788402	41191.465458	33.369101
797.063039	41249.224128	33.374119
797.664530	41303.387938	33.379136
798.103077	41353.048933	33.384154
798.996763	41395.233234	33.389172
799.941717	41463.618312	33.394189
800.568753	41517.772352	33.399207
801.631591	41583.831011	33.404224
801.888464	41637.277701	33.409242
802.847666	41691.785235	33.414260
803.503070	41756.592331	33.419277
804.303237	41812.510005	33.424295
805.130485	41879.067924	33.429312
805.799763	41950.900079	33.434330
806.663444	42006.397260	33.439348
807.148945	42064.318875	33.444365
807.750923	42138.603442	33.449383
809.053404	42200.053908	33.454400
809.676501	42279.743287	33.459418
810.393938	42341.114452	33.464436
811.129426	42412.735420	33.469453
811.761063	42480.508343	33.474471
813.320787	42543.330154	33.479488
814.011494	42614.421141	33.484506
814.796203	42677.743469	33.489524
815.680692	42743.630990	33.494541
816.202573	42809.518229	33.499559
817.527889	42868.329537	33.504576
818.237886	42927.477133	33.509594
819.211899	43000.163417	33.514612
819.844500	43057.482855	33.519629
820.663006	43119.776550	33.524647
822.064280	43172.213930	33.529664
822.466805	43244.256282	33.534682
823.400409	43294.382227	33.539700
824.286105	43354.933073	33.544717
824.935436	43423.028717	33.549735
826.069875	43475.767683	33.554752
826.841754	43537.386709	33.559770
827.592725	43600.059127	33.564788
828.380764	43665.420456	33.569805
829.394713	43720.569660	33.574823
830.158138	43779.382314	33.579840
830.931319	43834.999393	33.584858
831.856351	43891.623980	33.589876
832.555720	43947.246506	33.594893
833.295420	44000.750271	33.599911
834.579192	44052.765269	33.604928
834.876107	44110.342098	33.609946
835.663058	44162.061501	33.614964
836.540842	44211.515086	33.619981
837.321359	44263.242052	33.624999
838.026951	44315.474176	33.630016
838.409568	44378.478124	33.635034
839.562346	44432.038808	33.640052
840.843516	44494.922189	33.645069
841.117477	44550.789559	33.650087
842.085332	44612.855470	33.655104
843.197725	44684.570610	33.660122
843.737377	44752.415415	33.665140
844.353547	44800.702878	33.670157
844.841630	44881.561225	33.675175
846.122564	44939.410828	33.680192
846.724153	45012.155359	33.685210
847.440440	45079.549855	33.690228
848.466238	45139.533441	33.695245
849.373891	45215.210322	33.700263
850.810996	45284.397225	33.705280
851.309255	45351.807505	33.710298
851.990825	45419.568991	33.715316
853.012874	45487.100563	33.720333
854.269842	45551.787179	33.725351
855.350379	45610.960153	33.730368
855.992004	45677.520435	33.735386
857.069998	45749.952832	33.740404
857.842628	45815.050866	33.745421
858.819754	45871.197950	33.750439
859.625906	45928.497775	33.755456
860.716740	45994.179373	33.760474
861.239135	46059.298093	33.765492
861.989440	46128.733688	33.770509
863.046763	46192.358866	33.775527
863.782588	46264.156672	33.780544
864.383396	46329.567610	33.785562
865.320795	46390.548824	33.790580
866.384992	46468.792863	33.795597
866.833355	46544.223106	33.800615
868.088940	46606.281392	33.805632
868.771101	46679.853821	33.810650
869.392963	46753.410572	33.815668
870.664103	46825.601290	33.820685
871.401425	46900.475338	33.825703
872.450416	46967.994522	33.830720
872.903060	47040.901664	33.835738
874.139887	47104.501481	33.840756
875.438755	47163.366214	33.845773
876.252162	47232.915589	33.850791
877.044090	47307.655965	33.855808
877.888196	47385.791947	33.860826
878.457372	47439.868205	33.865844
879.402739	47506.089282	33.870861
880.605482	47580.848853	33.875879
881.294935	47642.504673	33.880896
882.603019	47713.945987	33.885914
883.331212	47775.836538	33.890932
884.448263	47838.729546	33.895949
884.839015	47904.981187	33.900967
886.580185	47965.860521	33.905984
887.299367	48032.067736	33.911002
888.000327	48092.653836	33.916020
888.726480	48151.800087	33.921037
889.856858	48208.277090	33.926055
891.040476	48265.182470	33.931072
891.409760	48328.895470	33.936090
892.737716	48385.633176	33.941108
893.650061	48430.035845	33.946125
893.930566	48490.580906	33.951143
895.298322	48532.148213	33.956160
895.658919	48600.374115	33.961178
896.418107	48649.748388	33.966196
897.336704	48716.027779	33.971213
897.837182	48774.103632	33.976231
899.197051	48834.937104	33.981248
899.584511	48893.239632	33.986266
900.421896	48961.411376	33.991284
901.373363	49016.943941	33.996301
902.246457	49089.273430	34.001319
903.315129	49168.437140	34.006336
904.345079	49228.886480	34.011354
904.758752	49304.767844	34.016372
905.814424	49376.899003	34.021389
906.931974	49438.202022	34.026407
907.864186	49506.980656	34.031424
908.811341	49588.385429	34.036442
909.627641	49660.599032	34.041460
910.416059	49731.912466	34.046477
911.020104	49798.882973	34.051495
912.442564	49879.841512	34.056512
913.160579	49957.601030	34.061530
914.041299	50023.377632	34.066548
915.413329	50094.468482	34.071565
916.072695	50177.489223	34.076583
917.292007	50240.619693	34.081600
918.321044	50323.229106	34.086618
919.049250	50395.680180	34.091636
920.229379	50463.796718	34.096653
920.858085	50531.315973	34.101671
922.200431	50597.041340	34.106688
923.013062	50673.276384	34.111706
923.709540	50742.240937	34.116724
924.567495	50818.437770	34.121741
925.440118	50894.506029	34.126759
926.716756	50968.910875	34.131776
927.848021	51039.529627	34.136794
928.072329	51109.100259	34.141812
929.340724	51172.978584	34.146829
930.212516	51255.046366	34.151847
931.328594	51326.883191	34.156864
932.144969	51408.162907	34.161882
933.537659	51480.279842	34.166900
934.464352	51549.198315	34.171917
935.399243	51624.487350	34.176935
936.274358	51695.242889	34.181952
937.026420	51760.487666	34.186970
938.086938	51836.175441	34.191988
939.097081	51898.406556	34.197005
939.821731	51972.122283	34.202023
940.997130	52037.934687	34.207040
941.821282	52114.482733	34.212058
942.598447	52199.131217	34.217076
943.652655	52259.160797	34.222093
944.455103	52342.211331	34.227111
945.511566	52412.782639	34.232128
946.354357	52496.751269	34.237146
947.060186	52574.243073	34.242164
948.389990	52640.950653	34.247181
949.726613	52708.638147	34.252199
950.740686	52773.440014	34.257216
951.431384	52855.889665	34.262234
952.292520	52917.393708	34.267252
953.678125	52980.790520	34.272269
954.434367	53052.416605	34.277287
954.988160	53116.259652	34.282304
956.029746	53178.482968	34.287322
956.817044	53239.550083	34.292340
957.678197	53305.794655	34.297357
958.782990	53375.190710	34.302375
959.242439	53433.639025	34.307392
960.256163	53503.536881	34.312410
960.701823	53572.820976	34.317428
961.742480	53641.689936	34.322445
962.584140	53729.358660	34.327463
963.834891	53810.522192	34.332480
964.785332	53882.063634	34.337498
965.693173	53966.666541	34.342516
966.990913	54026.472918	34.347533
967.706767	54112.846434	34.352551
968.718030	54184.752685	34.357568
970.076672	54264.951788	34.362586
970.851222	54338.319168	34.367604
972.159529	54414.426023	34.372621
972.823812	54490.601733	34.377639
974.063220	54561.518076	34.382656
975.504356	54636.573487	34.387674
975.956824	54706.062362	34.392692
977.599435	54773.322177	34.397709
978.571209	54861.177367	34.402727
979.416594	54923.511789	34.407744
980.568605	55000.087842	34.412762
981.545677	55076.520511	34.417780
982.604885	55133.430514	34.422797
983.316902	55212.569092	34.427815
984.189235	55285.044559	34.432832
985.514358	55350.469598	34.437850
986.608773	55426.777551	34.442868
987.628579	55490.820292	34.447885
988.418201	55565.973745	34.452903
989.245541	55645.159101	34.457920
990.286746	55716.685652	34.462938
991.303611	55785.362070	34.467956
992.576901	55858.340111	34.472973
993.411347	55934.088959	34.477991
994.238877	56012.079422	34.483008
995.252659	56086.965476	34.488026
996.257836	56171.769967	34.493044
997.005375	56243.540003	34.498061
998.257321	56334.369448	34.503079
998.854241	56411.017478	34.508096
1000.085971	56486.465754	34.513114
1000.897236	56572.561259	34.518132
1002.194599	56652.075509	34.523149
1002.916837	56728.964530	34.528167
1003.777857	56815.660723	34.533184
1005.215305	56894.679321	34.538202
1006.062461	56973.043269	34.543220
1007.260311	57047.188536	34.548237
1008.386814	57129.591590	34.553255
1008.942389	57209.957307	34.558272
1010.282478	57282.739449	34.563290
1011.298214	57375.799410	34.568308
1012.594008	57445.278934	34.573325
1013.364210	57515.669561	34.578343
1014.277868	57603.290764	34.583360
1015.474265	57671.856062	34.588378
1016.529614	57752.329342	34.593396
1017.830270	57818.600396	34.598413
1019.076252	57901.019150	34.603431
1019.740804	57976.566741	34.608448
1020.882509	58038.166994	34.613466
1021.625003	58115.930720	34.618484
1022.730370	58163.454751	34.623501
1023.837004	58234.231822	34.628519
1024.523332	58301.916290	34.633536
1025.783767	58365.828020	34.638554
1026.681011	58431.840773	34.643572
1027.305020	58501.750710	34.648589
1028.070620	58568.151421	34.653607
1029.182525	58649.929042	34.658624
1030.324977	58720.461455	34.663642
1031.450238	58803.908438	34.668660
1032.518399	58875.263013	34.673677
1033.274807	58946.343532	34.678695
1034.293358	59025.003952	34.683712
1035.030113	59099.746326	34.688730
1036.285429	59195.086230	34.693748
1037.503897	59271.342821	34.698765
1038.775532	59341.382233	34.703783
1039.701264	59430.881697	34.708800
1040.681608	59511.271246	34.713818
1041.303456	59597.198183	34.718836
1042.556020	59678.792818	34.723853
1043.922219	59773.301231	34.728871
1044.860149	59855.641682	34.733888
1045.975374	59937.853542	34.738906
1046.749113	60024.220401	34.743924
1047.963419	60112.803973	34.748941
1049.269009	60198.854469	34.753959
1050.349843	60285.883370	34.758976
1051.599259	60357.998966	34.763994
1052.548940	60443.124625	34.769012
1053.637184	60521.817019	34.774029
1054.981904	60602.299035	34.779047
1055.771292	60690.526756	34.784064
1056.522941	60773.462649	34.789082
1057.627477	60858.287140	34.794100
1058.737762	60948.383767	34.799117
1059.633023	61023.835301	34.804135
1060.669413	61128.116599	34.809152
1062.075897	61207.628853	34.814170
1062.717988	61298.761788	34.819188
1063.479608	61400.054987	34.824205
1064.857028	61493.909996	34.829223
1065.774259	61579.190243	34.834240
1067.156582	61660.695339	34.839258
1068.155526	61773.353466	34.844276
1069.259077	61850.401934	34.849293
1070.616846	61942.394349	34.854311
1071.100343	62040.967234	34.859328
1072.430299	62126.305403	34.864346
1073.960262	62220.721810	34.869364
1075.271020	62306.683946	34.874381
1076.384767	62396.082689	34.879399
1077.257169	62479.606905	34.884416
1078.201885	62574.926031	34.889434
1079.322115	62655.690265	34.894452
1080.472126	62746.091139	34.899469
1081.602232	62826.037785	34.904487
1082.425022	62913.008538	34.909504
1083.708398	62993.261042	34.914522
1084.656566	63091.626513	34.919540
1085.720969	63182.276526	34.924557
1087.086415	63264.739101	34.929575
1088.067509	63351.433532	34.934592
1089.387993	63424.585242	34.939610
1090.581215	63511.196568	34.944628
1091.368945	63594.452845	34.949645
1092.427694	63674.571593	34.954663
1093.649002	63758.767482	34.959680
1094.847708	63823.722287	34.964698
1095.590862	63895.604179	34.969716
1096.845798	63985.214568	34.974733
1098.053006	64046.098059	34.979751
1098.622465	64133.625289	34.984768
1099.662823	64202.904228	34.989786
1100.741280	64273.785419	34.994804
1101.709661	64356.395714	34.999821
1103.395265	64442.129632	35.004839
1104.169615	64535.064453	35.009856
1105.528912	64610.752225	35.014874
1106.569993	64694.991985	35.019892
1107.476077	64783.209788	35.024909
1108.720262	64866.114364	35.029927
1109.617481	64947.154979	35.034944
1110.665230	65032.717980	35.039962
1111.922305	65123.838855	35.044980
1113.098474	65207.882045	35.049997
1114.159254	65282.035584	35.055015
1115.167668	65382.280973	35.060032
1116.436217	65459.967019	35.065050
1117.736828	65554.349455	35.070068
1119.279051	65646.472452	35.075085
1120.367558	65724.554537	35.080103
1121.355407	65813.560934	35.085120
1122.670929	65895.812032	35.090138
1123.784167	65982.494996	35.095156
1124.931576	66072.199213	35.100173
1126.092886	66153.025327	35.105191
1126.925850	66244.114969	35.110208
1127.993527	66330.420017	35.115226
1129.322285	66421.964944	35.120244
1130.387195	66511.253036	35.125261
1131.978960	66586.594001	35.130279
1132.580658	66669.173986	35.135296
1133.485170	66758.209338	35.140314
1134.935336	66849.445672	35.145332
1135.938434	66943.354100	35.150349
1137.505412	67033.547236	35.155367
1138.519443	67125.390612	35.160384
1139.379598	67207.343295	35.165402
1140.821677	67299.798132	35.170420
1141.591866	67395.352662	35.175437
1142.869176	67487.251333	35.180455
1144.250537	67587.713312	35.185472
1145.068566	67678.747101	35.190490
1146.339555	67759.263669	35.195508
1147.311692	67864.494767	35.200525
1148.485590	67961.261217	35.205543
1149.570534	68060.992410	35.210560
1150.711964	68155.232003	35.215578
1152.137460	68244.058480	35.220596
1153.135848	68333.388632	35.225613
1154.561207	68433.701455	35.230631
1155.510586	68529.510920	35.235648
1156.545433	68619.039006	35.240666
1157.970233	68722.240321	35.245684
1159.088076	68810.021247	35.250701
1160.244851	68899.911240	35.255719
1161.418718	68995.611516	35.260736
1162.353203	69092.476480	35.265754
1163.797759	69177.320473	35.270772
1164.926887	69284.730114	35.275789
1166.352943	69364.910985	35.280807
1167.542445	69453.062862	35.285824
1169.111099	69535.697862	35.290842
1170.223658	69626.869997	35.295860
1171.274907	69712.131559	35.300877
1172.355831	69790.075281	35.305895
1173.337755	69867.838354	35.310912
1174.522401	69951.173991	35.315930
1175.623349	70023.929331	35.320948
1176.323771	70100.236212	35.325965
1177.350956	70182.533307	35.330983
1178.489420	70262.407125	35.336000
1179.226580	70356.407408	35.341018
1180.857021	70441.631872	35.346036
1181.924274	70541.438723	35.351053
1183.162459	70624.856839	35.356071
1184.646591	70720.293565	35.361088
1185.755729	70797.425389	35.366106
1187.038077	70896.186954	35.371124
1188.259761	70996.338784	35.376141
1189.510322	71082.605987	35.381159
1190.660328	71181.249919	35.386176
1192.007567	71272.834562	35.391194
1193.529510	71354.273131	35.396212
1194.219637	71442.275183	35.401229
1195.247832	71536.937316	35.406247
1196.449416	71626.658797	35.411264
1197.599486	71719.238229	35.416282
1199.257180	71816.488369	35.421300
1200.284949	71916.787889	35.426317
1201.299729	72006.527080	35.431335
1202.853085	72106.124922	35.436352
1203.979487	72205.270322	35.441370
1205.285759	72296.421633	35.446388
1206.345141	72406.229729	35.451405
1207.431872	72492.742383	35.456423
1208.857351	72599.226631	35.461440
1210.056691	72682.429368	35.466458
1211.137481	72791.184499	35.471476
1212.434893	72888.114714	35.476493
1213.806574	72991.328535	35.481511
1215.204012	73092.499577	35.486528
1216.429781	73186.566931	35.491546
1217.779074	73276.562350	35.496564
1218.685253	73372.554641	35.501581
1219.961772	73483.853310	35.506599
1221.404166	73582.498721	35.511616
1222.043935	73684.562576	35.516634
1223.409438	73776.191074	35.521652
1224.536247	73882.942294	35.526669
1225.923758	73983.484977	35.531687
1227.336686	74074.068500	35.536704
1228.432253	74183.143689	35.541722
1230.159438	74276.984862	35.546740
1230.744669	74376.805268	35.551757
1232.333364	74468.566069	35.556775
1233.449627	74591.357332	35.561792
1234.794734	74687.818030	35.566810
1236.120145	74779.823544	35.571828
1236.966240	74887.787791	35.576845
1238.489237	74999.231750	35.581863
1239.942703	75092.789062	35.586880
1241.751485	75166.430082	35.591898
1243.507597	75246.096178	35.596916
1244.443587	75343.357584	35.601933
1245.706451	75435.438418	35.606951
1247.146070	75517.662605	35.611968
1248.249775	75611.985510	35.616986
1249.659338	75682.105364	35.622004
1251.133415	75764.286942	35.627021
1251.768934	75854.845492	35.632039
1253.520307	75931.271613	35.637056
1254.254395	76015.241182	35.642074
1255.600695	76086.815981	35.647092
1256.250155	76162.856922	35.652109
1256.927953	76244.163203	35.657127
1258.500945	76340.670364	35.662144
1259.511050	76418.454631	35.667162
1260.537469	76504.052292	35.672180
1261.938725	76606.021393	35.677197
1262.941771	76690.217207	35.682215
1264.063170	76787.188939	35.687232
1265.099736	76890.824638	35.692250
1266.776753	76997.059222	35.697268
1267.726341	77097.897062	35.702285
1269.111222	77197.882130	35.707303
1270.343796	77306.999311	35.712320
1271.535523	77409.219392	35.717338
1272.915015	77502.403864	35.722356
1273.940304	77626.109825	35.727373
1275.275706	77720.619357	35.732391
1276.683006	77836.096052	35.737408
1277.744754	77942.417423	35.742426
1279.197759	78050.401154	35.747444
1280.515890	78172.645191	35.752461
1281.826962	78285.795172	35.757479
1283.387300	78395.549761	35.762496
1284.223200	78499.387483	35.767514
1285.998859	78601.394447	35.772532
1287.119777	78720.251192	35.777549
1288.329823	78831.214861	35.782567
1289.772759	78941.864022	35.787584
1290.788890	79054.391650	35.792602
1292.451124	79170.860424	35.797620
1293.720094	79290.520038	35.802637
1294.762245	79399.231784	35.807655
1296.546297	79507.448420	35.812672
1298.108272	79627.938026	35.817690
1299.559507	79737.195525	35.822708
1300.555937	79860.409275	35.827725
1302.093976	79972.048597	35.832743
1303.446668	80078.408937	35.837760
1304.599159	80188.538194	35.842778
1306.033476	80293.873137	35.847796
1307.229614	80395.039421	35.852813
1308.561074	80513.389673	35.857831
1310.054393	80626.837602	35.862848
1311.414298	80740.395444	35.867866
1312.460510	80842.904289	35.872884
1313.971640	80953.918277	35.877901
1315.242651	81062.904973	35.882919
1316.924887	81170.345764	35.887936
1318.312244	81285.890650	35.892954
1319.613922	81394.265729	35.897972
1320.981793	81496.334148	35.902989
1322.197800	81603.557771	35.908007
1323.606822	81700.806076	35.913024
1324.635151	81819.855192	35.918042
1325.772399	81919.427104	35.923060
1327.275986	82035.843870	35.928077
1328.641339	82142.628201	35.933095
1330.169526	82247.753173	35.938112
1331.132691	82361.239963	35.943130
1332.553789	82469.752640	35.948148
1333.927826	82583.771863	35.953165
1335.740669	82706.566983	35.958183
1336.765142	82801.623664	35.963200
1337.821515	82906.469762	35.968218
1339.217714	83017.978587	35.973236
1340.458033	83128.878598	35.978253
1341.860065	83243.821054	35.983271
1343.377734	83334.482167	35.988288
1344.575599	83433.099698	35.993306
1345.740798	83520.471272	35.998324
1347.135497	83611.000363	36.003341
1348.258569	83720.691894	36.008359
1349.651155	83820.218080	36.013376
1350.723140	83927.979758	36.018394
1352.013449	84035.872579	36.023412
1353.342753	84141.960492	36.028429
1354.550140	84252.211127	36.033447
1355.742260	84359.879710	36.038464
1357.223333	84467.579748	36.043482
1358.699147	84585.392423	36.048500
1360.160957	84707.566585	36.053517
1361.065924	84826.305388	36.058535
1362.401251	84945.003038	36.063552
1364.064181	85067.793656	36.068570
1365.385422	85185.011964	36.073588
1366.994854	85304.251308	36.078605
1368.592602	85413.748726	36.083623
1369.865389	85525.945453	36.088640
1371.196685	85640.351007	36.093658
1372.790232	85763.915676	36.098676
1374.192310	85877.525521	36.103693
1375.676568	85998.941377	36.108711
1377.923364	86086.532566	36.113728
1379.185235	86202.611130	36.118746
1380.458165	86321.121406	36.123764
1382.061499	86418.380894	36.128781
1383.765579	86536.254711	36.133799
1384.947417	86630.425237	36.138816
1386.013244	86748.754070	36.143834
1387.366774	86850.767832	36.148852
1389.006231	86964.129561	36.153869
1389.982712	87078.710061	36.158887
1391.764279	87177.325597	36.163904
1393.015337	87288.531427	36.168922
1394.023287	87402.195904	36.173940
1395.856074	87515.517011	36.178957
1397.059094	87627.301856	36.183975
1398.668059	87740.265830	36.188992
1400.335017	87861.661014	36.194010
1401.383608	87972.026558	36.199028
1402.730883	88087.199584	36.204045
1404.105558	88204.409073	36.209063
1405.619776	88319.747113	36.214080
1406.905914	88439.315743	36.219098
1408.482567	88553.365046	36.224116
1410.221010	88664.538245	36.229133
1411.213562	88772.165530	36.234151
1412.880545	88882.108740	36.239168
1414.003901	89004.505688	36.244186
1415.025884	89126.488041	36.249204
1417.008447	89237.676092	36.254221
1418.184756	89362.258698	36.259239
1420.004514	89479.289911	36.264256
1421.495445	89596.258709	36.269274
1422.400962	89715.790353	36.274292
1423.896410	89824.623173	36.279309
1425.380200	89950.338993	36.284327
1426.889516	90061.185569	36.289344
1428.287988	90183.671285	36.294362
1429.648899	90296.924428	36.299380
1431.443578	90413.963219	36.304397
1432.727813	90530.803101	36.309415
1434.260148	90646.527569	36.314432
1435.871305	90752.291433	36.319450
1437.452058	90848.289018	36.324468
1439.176927	90944.948859	36.329485
1439.957483	91048.523763	36.334503
1441.723235	91135.355713	36.339520
1443.227309	91220.783830	36.344538
1444.086016	91330.823858	36.349556
1446.000800	91422.322766	36.354573
1446.860179	91529.752594	36.359591
1448.215553	91629.805393	36.364608
1449.443511	91742.324245	36.369626
1450.875151	91855.204709	36.374644
1452.110639	91960.017365	36.379661
1453.338130	92067.062281	36.384679
1454.637175	92186.441115	36.389696
1456.287393	92317.324687	36.394714
1457.839142	92437.653771	36.399732
1459.284642	92552.220359	36.404749
1460.490366	92685.240622	36.409767
1461.822650	92808.419053	36.414784
1463.337298	92943.192135	36.419802
1464.893982	93074.004801	36.424820
1466.561300	93197.994531	36.429837
1467.879823	93316.487543	36.434855
1469.806546	93445.723244	36.439872
1471.193332	93574.130947	36.444890
1472.643628	93706.002208	36.449908
1474.482499	93828.041215	36.454925
1476.051517	93949.438262	36.459943
1477.776518	94063.320593	36.464960
1479.068562	94188.424765	36.469978
1480.429358	94325.027730	36.474996
1482.001932	94448.454208	36.480013
1483.617308	94574.574336	36.485031
1485.034520	94692.284108	36.490048
1486.496922	94822.979473	36.495066
1487.891012	94944.775252	36.500084
1489.742552	95071.912706	36.505101
1491.030761	95200.545337	36.510119
1492.854321	95321.692681	36.515136
1494.627152	95441.847027	36.520154
1496.147601	95570.711231	36.525172
1497.919426	95682.602171	36.530189
1499.344582	95803.585244	36.535207
1500.774515	95912.019054	36.540224
1502.178850	96044.541230	36.545242
1503.517203	96169.519432	36.550260
1505.298049	96287.622307	36.555277
1506.628830	96411.423796	36.560295
1507.852030	96537.663635	36.565312
1509.970976	96653.192742	36.570330
1510.772902	96783.099134	36.575348
1512.533047	96912.590722	36.580365
1514.216489	97035.744006	36.585383
1515.787694	97166.343524	36.590400
1517.071691	97283.944373	36.595418
1518.260825	97406.098557	36.600436
1520.038181	97526.716552	36.605453
1521.422465	97656.130257	36.610471
1522.991353	97783.728373	36.615488
1524.706421	97914.879038	36.620506
1526.301652	98048.850427	36.625524
1527.707991	98162.670552	36.630541
1529.519015	98291.500690	36.635559
1530.711714	98420.034611	36.640576
1532.519553	98535.479588	36.645594
1533.815788	98665.012527	36.650612
1535.433991	98789.805427	36.655629
1536.981595	98917.994549	36.660647
1538.053111	99037.447773	36.665664
1539.782030	99157.103371	36.670682
1541.049786	99275.639547	36.675700
1542.732151	99379.913242	36.680717
1543.830259	99505.689962	36.685735
1545.282735	99621.397011	36.690752
1547.144871	99739.652232	36.695770
1548.451401	99875.070720	36.700788
1549.689694	99989.760212	36.705805
1551.290728	100117.286589	36.710823
1552.675816	100250.716750	36.715840
1554.269419	100374.632222	36.720858
1555.872166	100511.300383	36.725876
1557.769891	100635.689302	36.730893
1559.105174	100768.457438	36.735911
1560.484578	100903.894251	36.740928
1562.237498	101044.446029	36.745946
1563.574206	101177.874863	36.750964
1565.390345	101313.524321	36.755981
1567.003243	101454.632137	36.760999
1568.591820	101594.869568	36.766016
1570.045366	101736.814799	36.771034
1571.253009	101882.069871	36.776052
1573.445807	102025.764979	36.781069
1574.883279	102164.177358	36.786087
1576.404228	102305.822967	36.791104
1578.026718	102438.274275	36.796122
1579.443141	102587.835965	36.801140
1581.609599	102724.514411	36.806157
1582.959018	102879.324048	36.811175
1584.351041	103021.322443	36.816192
1586.138598	103170.157048	36.821210
1587.549807	103326.822919	36.826228
1589.625920	103455.670364	36.831245
1591.352487	103610.259898	36.836263
1593.206125	103746.408038	36.841280
1595.327172	103879.003068	36.846298
1596.622090	104018.497755	36.851316
1598.260782	104142.585278	36.856333
1599.869089	104279.217548	36.861351
1601.211264	104417.324535	36.866368
1603.132582	104557.040958	36.871386
1604.364017	104705.119490	36.876404
1606.236480	104837.046986	36.881421
1607.836707	104984.371994	36.886439
1609.706355	105128.029423	36.891456
1611.624497	105249.706522	36.896474
1612.956843	105385.663531	36.901492
1614.929129	105510.718560	36.906509
1616.632371	105644.336579	36.911527
1617.927478	105774.696597	36.916544
1619.737299	105912.813025	36.921562
1621.838727	106052.482273	36.926580
1623.424630	106161.927753	36.931597
1624.965526	106295.484855	36.936615
1626.183573	106433.137600	36.941632
1628.000031	106566.754320	36.946650
1629.384503	106697.370256	36.951668
1631.105160	106835.199999	36.956685
1632.773562	106958.202793	36.961703
1634.077064	107102.159599	36.966720
1635.564643	107232.203611	36.971738
1637.092622	107374.123163	36.976756
1638.674174	107516.656296	36.981773
1640.273264	107654.305380	36.986791
1641.881522	107804.240842	36.991808
1643.978644	107947.405620	36.996826
1645.185949	108080.070590	37.001844
1646.673846	108218.702954	37.006861
1648.268732	108345.069816	37.011879
1649.811880	108470.646316	37.016896
1651.140681	108600.441244	37.021914
1652.633327	108739.582185	37.026932
1654.711862	108871.455199	37.031949
1656.164695	108998.911741	37.036967
1657.524020	109131.531721	37.041984
1659.030243	109263.875727	37.047002
1660.644595	109419.612406	37.052020
1662.015417	109558.179582	37.057037
1664.463808	109701.766139	37.062055
1665.316950	109850.838863	37.067072
1667.209260	109988.654483	37.072090
1668.662215	110135.453907	37.077108
1671.179021	110280.300312	37.082125
1673.363308	110413.126473	37.087143
1674.733597	110565.013078	37.092160
1676.761653	110703.064005	37.097178
1678.255243	110851.064826	37.102196
1679.934619	110992.595148	37.107213
1681.598668	111138.947414	37.112231
1682.742554	111284.709118	37.117248
1684.705753	111426.349180	37.122266
1686.238535	111583.591896	37.127284
1687.982147	111731.709666	37.132301
1690.164692	111884.781739	37.137319
1691.308499	112042.873298	37.142336
1693.015755	112192.241467	37.147354
1694.541184	112353.546944	37.152372
1696.411377	112510.741236	37.157389
1698.529630	112664.993409	37.162407
1699.491973	112826.604252	37.167424
1701.693773	112985.828889	37.172442
1703.441706	113145.416563	37.177460
1705.296483	113308.184262	37.182477
1707.374714	113452.147996	37.187495
1709.236997	113606.012844	37.192512
1710.975692	113754.900684	37.197530
1712.904278	113907.716533	37.202548
1714.453071	114057.104425	37.207565
1716.419734	114199.363665	37.212583
1718.092761	114355.125497	37.217600
1719.891232	114491.108760	37.222618
1721.754104	114643.608179	37.227636
1723.396040	114793.961174	37.232653
1725.212190	114945.987180	37.237671
1726.644510	115089.677447	37.242688
1728.451053	115241.148124	37.247706
1730.333137	115398.505289	37.252724
1731.343387	115553.449514	37.257741
1733.323795	115708.661941	37.262759
1734.911404	115865.255211	37.267776
1736.571262	116021.381302	37.272794
1737.969233	116185.653455	37.277812
1739.417439	116356.399724	37.282829
1741.368646	116516.718808	37.287847
1742.974849	116686.275128	37.292864
1744.655271	116836.769982	37.297882
1746.795929	117016.264624	37.302900
1748.250175	117188.865580	37.307917
1750.329535	117344.437276	37.312935
1751.976010	117514.232082	37.317952
1753.675419	117685.985411	37.322970
1755.523642	117853.784360	37.327988
1757.090486	118024.684682	37.333005
1758.955305	118180.914751	37.338023
1760.648916	118356.629451	37.343040
1762.615479	118508.659303	37.348058
1764.653452	118666.246998	37.353076
1766.207682	118807.763638	37.358093
1767.927061	118946.730936	37.363111
1769.704929	119089.494930	37.368128
1771.406238	119237.066060	37.373146
1772.947336	119385.981874	37.378164
1774.708163	119537.908339	37.383181
1776.742559	119680.913682	37.388199
1778.000554	119842.407624	37.393216
1779.698327	120001.512517	37.398234
1781.669978	120160.144165	37.403252
1783.488568	120326.081315	37.408269
1784.806608	120481.860480	37.413287
1786.287437	120649.754307	37.418304
1787.772932	120829.901726	37.423322
1789.689110	121006.063308	37.428340
1791.390365	121181.701002	37.433357
1793.238431	121362.187700	37.438375
1794.861847	121545.209167	37.443392
1797.140888	121723.791126	37.448410
1799.007695	121897.960178	37.453428
1800.871108	122084.993412	37.458445
1802.830579	122255.914889	37.463463
1804.972942	122436.753998	37.468480
1806.792879	122611.225280	37.473498
1808.596239	122793.006771	37.478516
1810.219898	122985.295353	37.483533
1811.976502	123158.865555	37.488551
1813.568643	123339.629528	37.493568
1815.664753	123529.538427	37.498586
1817.816938	123719.921569	37.503604
1818.965534	123903.649506	37.508621
1820.903296	124089.462817	37.513639
1822.368714	124293.060148	37.518656
1824.558299	124487.297673	37.523674
1826.473140	124684.560136	37.528692
1828.057250	124886.809966	37.533709
1829.568563	125074.647886	37.538727
1831.365494	125280.507520	37.543744
1833.225742	125488.312047	37.548762
1835.267303	125692.854382	37.553780
1836.929505	125885.734471	37.558797
1838.703120	126088.328720	37.563815
1840.708818	126298.284156	37.568832
1843.190076	126505.768873	37.573850
1845.087812	126692.323524	37.578868
1846.696527	126898.309440	37.583885
1848.700117	127087.196471	37.588903
1850.414588	127297.430714	37.593920
1852.135933	127496.538467	37.598938
1854.322821	127686.934843	37.603956
1856.366095	127899.721821	37.608973
1858.541160	128096.605035	37.613991
1860.142900	128299.947404	37.619008
1862.265908	128494.468090	37.624026
1864.130558	128682.863839	37.629044
1865.732394	128878.342852	37.634061
1868.198666	129075.895859	37.639079
1869.980111	129262.556293	37.644096
1871.405344	129463.165900	37.649114
1873.639537	129648.273132	37.654132
1875.508630	129840.517733	37.659149
1877.125276	130034.185464	37.664167
1878.624988	130229.623195	37.669184
1880.411023	130440.521848	37.674202
1882.805889	130633.271851	37.679220
1884.281501	130835.580287	37.684237
1886.414565	131028.220562	37.689255
1887.881573	131221.041494	37.694272
1889.979601	131393.654343	37.699290
1891.763346	131573.967791	37.704308
1893.238314	131759.582992	37.709325
1895.173004	131944.860986	37.714343
1897.226751	132122.482842	37.719360
1898.948740	132317.273749	37.724378
1900.817487	132508.121946	37.729396
1902.574728	132692.453735	37.734413
1904.585738	132896.160359	37.739431
1906.259325	133086.914575	37.744448
1908.168703	133282.086661	37.749466
1910.283966	133475.476521	37.754484
1911.890788	133682.053918	37.759501
1913.751677	133880.674876	37.764519
1915.656902	134079.124871	37.769536
1917.366460	134295.662652	37.774554
1919.150670	134504.906349	37.779572
1921.099185	134722.614480	37.784589
1923.206888	134940.907979	37.789607
1925.112480	135151.760033	37.794624
1926.866006	135370.732522	37.799642
1929.367004	135582.407563	37.804660
1931.037612	135808.475754	37.809677
1933.223359	136024.973163	37.814695
1934.790692	136247.049740	37.819712
1936.570032	136469.386268	37.824730
1938.776066	136691.187957	37.829748
1940.866366	136914.036605	37.834765
1943.201849	137128.231807	37.839783
1945.417657	137352.217827	37.844800
1947.405919	137568.233014	37.849818
1949.602958	137776.336245	37.854836
1951.507055	138001.071882	37.859853
1953.680152	138211.833017	37.864871
1955.762530	138424.525442	37.869888
1957.610449	138637.864460	37.874906
1959.724046	138859.855940	37.879924
1961.700736	139072.555080	37.884941
1963.990596	139288.290208	37.889959
1965.967863	139505.102904	37.894976
1967.644366	139714.425248	37.899994
1969.604770	139926.191685	37.905012
1971.197431	140145.706815	37.910029
1973.374996	140360.931316	37.915047
1975.687329	140578.191715	37.920064
1977.384533	140802.401866	37.925082
1979.354140	141016.253011	37.930100
1981.082125	141245.016457	37.935117
1983.402413	141450.870453	37.940135
1985.344564	141688.245220	37.945152
1987.188989	141906.561662	37.950170
1989.723899	142130.990283	37.955188
1990.871600	142348.871429	37.960205
1992.895301	142571.376433	37.965223
1995.140299	142791.677796	37.970240
1996.767782	143016.670531	37.975258
1999.070356	143240.201248	37.980276
2001.047129	143472.985012	37.985293
2003.005352	143691.101334	37.990311
2005.219337	143919.700149	37.995328
2007.227943	144144.638707	38.000346
2008.902820	144364.858135	38.005364
2011.310411	144596.679006	38.010381
2013.375208	144824.645216	38.015399
2015.237922	145047.084865	38.020416
2017.366167	145264.813536	38.025434
2019.564715	145476.262358	38.030452
2020.694733	145688.436811	38.035469
2022.529388	145889.853815	38.040487
2025.016747	146101.082602	38.045504
2026.477446	146315.607022	38.050522
2028.381924	146535.520945	38.055540
2029.773419	146754.221031	38.060557
2031.364524	146982.626027	38.065575
2033.596416	147208.457283	38.070592
2035.494874	147450.054711	38.075610
2037.865266	147688.723993	38.080628
2040.049849	147929.872960	38.085645
2042.253252	148161.932167	38.090663
2044.745986	148385.811346	38.095680
2046.783190	148616.578390	38.100698
2048.981671	148847.841750	38.105716
2050.892934	149076.663018	38.110733
2053.018146	149310.757623	38.115751
2054.967140	149549.272458	38.120768
2056.711897	149795.118646	38.125786
2059.067394	150018.759528	38.130804
2060.935839	150275.123943	38.135821
2062.775263	150514.853283	38.140839
2065.188646	150758.911620	38.145856
2066.858825	151014.612269	38.150874
2068.944991	151266.695229	38.155892
2071.176194	151519.835724	38.160909
2073.289364	151772.856130	38.165927
2075.199909	152017.429933	38.170944
2077.411822	152282.090007	38.175962
2079.725457	152539.436646	38.180980
2081.715374	152795.565485	38.185997
2083.839724	153048.920023	38.191015
2085.609456	153302.800571	38.196032
2087.509488	153577.721200	38.201050
2090.021858	153832.618322	38.206068
2092.130564	154098.013915	38.211085
2094.025540	154370.654260	38.216103
2096.443596	154621.278998	38.221120
2098.346301	154892.803549	38.226138
2100.510931	155157.979566	38.231156
2102.943968	155418.113466	38.236173
2104.999614	155687.117175	38.241191
2107.317309	155945.227597	38.246208
2109.335105	156209.682309	38.251226
2111.203594	156481.219630	38.256244
2113.558340	156744.431027	38.261261
2115.492329	157025.443547	38.266279
2117.693427	157288.490862	38.271296
2119.588754	157568.724900	38.276314
2121.892380	157840.645055	38.281332
2124.039553	158100.238649	38.286349
2125.947660	158388.738920	38.291367
2128.209232	158660.250394	38.296384
2130.321074	158934.922071	38.301402
2133.141196	159204.889119	38.306420
2135.332607	159462.666260	38.311437
2137.543647	159728.756815	38.316455
2140.040966	159982.679955	38.321472
2141.997413	160256.480369	38.326490
2143.997272	160516.081767	38.331508
2146.070877	160790.247159	38.336525
2148.356638	161042.811051	38.341543
2150.518196	161297.134580	38.346560
2152.340963	161570.212507	38.351578
2154.785335	161831.908416	38.356596
2156.804869	162097.365975	38.361613
2158.769293	162362.909389	38.366631
2160.450779	162611.942574	38.371648
2162.715540	162870.991865	38.376666
2164.553309	163111.712249	38.381684
2166.583713	163356.504344	38.386701
2168.622767	163624.225030	38.391719
2170.831709	163885.356499	38.396736
2173.027181	164138.479848	38.401754
2175.028657	164394.643352	38.406772
2177.126532	164659.845250	38.411789
2178.999929	164932.865957	38.416807
2181.442472	165197.178397	38.421824
2183.173546	165463.684808	38.426842
2185.554693	165728.605620	38.431860
2187.500312	166001.251223	38.436877
2189.728969	166287.781962	38.441895
2192.119376	166580.586232	38.446912
2193.978105	166865.958086	38.451930
2196.120264	167156.670404	38.456948
2198.070112	167447.439263	38.461965
2200.272985	167743.007434	38.466983
2202.407981	168044.732691	38.472000
2204.312779	168333.252193	38.477018
2206.606257	168640.935572	38.482036
2208.733218	168938.133069	38.487053
2210.873659	169260.279434	38.492071
2213.286324	169556.216108	38.497088
2216.005099	169877.907008	38.502106
2218.723084	170176.185763	38.507124
2220.810217	170483.299640	38.512141
2223.116796	170778.584826	38.517159
2225.453339	171068.889153	38.522176
2228.008881	171389.774041	38.527194
2230.135586	171690.563434	38.532212
2232.342726	171998.667990	38.537229
2234.397803	172304.930921	38.542247
2237.281367	172616.640412	38.547264
2239.570409	172934.868729	38.552282
2242.115910	173223.053683	38.557300
2244.428445	173524.240408	38.562317
2246.509375	173834.390923	38.567335
2248.639696	174117.132937	38.572352
2251.218098	174420.161018	38.577370
2253.393345	174719.926129	38.582388
2255.749545	175020.946707	38.587405
2257.904094	175322.444231	38.592423
2260.656340	175621.272144	38.597440
2262.871633	175920.273610	38.602458
2265.575165	176216.812924	38.607476
2267.743612	176505.004936	38.612493
2270.058939	176793.886201	38.617511
2272.706822	177086.069081	38.622528
2274.888221	177379.214467	38.627546
2277.086284	177680.586871	38.632564
2279.428251	177969.595026	38.637581
2281.235469	178268.084294	38.642599
2283.680985	178552.862398	38.647616
2286.011456	178855.081844	38.652634
2287.929914	179161.226855	38.657652
2290.392595	179447.300488	38.662669
2292.253665	179752.872358	38.667687
2294.398085	180057.309091	38.672704
2296.411349	180365.119768	38.677722
2298.622872	180682.450202	38.682740
2300.822740	180973.852374	38.687757
2303.284926	181296.276311	38.692775
2305.566334	181607.173424	38.697792
2307.802031	181913.557840	38.702810
2309.823581	182225.843573	38.707828
2312.394113	182523.796489	38.712845
2314.671823	182830.202771	38.717863
2316.461297	183118.602351	38.722880
2318.816378	183412.197666	38.727898
2320.828663	183713.847778	38.732916
2323.050197	184010.005555	38.737933
2325.097501	184323.005306	38.742951
2327.208661	184629.849606	38.747968
2329.506273	184947.841352	38.752986
2331.431330	185272.394231	38.758004
2333.781109	185577.832768	38.763021
2336.194748	185917.779710	38.768039
2338.234173	186319.912536	38.773056
2341.370137	186632.927846	38.778074
2344.390777	186947.486010	38.783092
2347.104254	187258.892589	38.788109
2349.336271	187572.330778	38.793127
2351.581147	187899.026488	38.798144
2354.262965	188215.571514	38.803162
2356.019674	188536.096801	38.808180
2358.536940	188855.336273	38.813197
2361.024005	189181.413946	38.818215
2363.754450	189514.287298	38.823232
2366.234264	189836.405614	38.828250
2368.224018	190176.355809	38.833268
2370.296372	190499.936423	38.838285
2372.507623	190834.697853	38.843303
2374.892031	191173.116350	38.848320
2377.386157	191518.376862	38.853338
2379.454331	191864.796889	38.858356
2382.132634	192197.381252	38.863373
2384.306355	192552.550027	38.868391
2386.870682	192894.780878	38.873408
2389.420595	193242.984105	38.878426
2391.663763	193606.501957	38.883444
2393.979014	193941.408185	38.888461
2396.490899	194301.838095	38.893479
2398.837447	194652.134312	38.898496
2401.663858	195006.573378	38.903514
2403.491515	195366.071258	38.908532
2406.135618	195724.477796	38.913549
2408.171188	196083.970639	38.918567
2410.453719	196443.629202	38.923584
2413.308469	196805.333371	38.928602
2415.809625	197174.332939	38.933620
2418.308370	197529.616973	38.938637
2421.083967	197887.627580	38.943655
2423.309716	198243.921113	38.948672
2425.476503	198608.734281	38.953690
2427.989410	198974.891575	38.958708
2430.967390	199344.635251	38.963725
2433.301550	199708.459743	38.968743
2435.468842	200068.170521	38.973760
2437.918624	200440.996436	38.978778
2440.241256	200809.016597	38.983796
2443.399182	201165.832237	38.988813
2446.417123	201521.908365	38.993831
2448.900330	201870.574787	38.998848
2451.655956	202213.611009	39.003866
2453.648061	202573.633937	39.008884
2456.483807	202911.045134	39.013901
2458.874702	203271.947316	39.018919
2461.656141	203612.111756	39.023936
2464.196245	203942.153343	39.028954
2466.161676	204300.837528	39.033972
2468.594613	204641.083486	39.038989
2471.031276	204997.307792	39.044007
2473.092629	205358.163657	39.049024
2475.503492	205684.748165	39.054042
2477.610536	206015.775179	39.059060
2480.346757	206347.390690	39.064077
2482.573553	206683.099672	39.069095
2484.958334	207004.101668	39.074112
2487.468480	207336.693815	39.079130
2489.636049	207669.847839	39.084148
2492.171889	208008.736955	39.089165
2494.247401	208345.208703	39.094183
2496.308403	208698.627117	39.099200
2498.727286	209046.122218	39.104218
2501.228229	209422.158308	39.109236
2503.796308	209775.219940	39.114253
2506.278246	210139.193497	39.119271
2508.090020	210515.668701	39.124288
2510.736279	210874.003560	39.129306
2513.136509	211259.609661	39.134324
2515.372052	211646.994763	39.139341
2517.881742	212030.654215	39.144359
2520.540200	212426.764152	39.149376
2523.074454	212820.302769	39.154394
2525.841257	213214.567800	39.159412
2528.403872	213606.070690	39.164429
2531.315135	213997.265745	39.169447
2533.699120	214386.892062	39.174464
2536.755646	214780.351719	39.179482
2539.130010	215180.700756	39.184500
2541.772907	215570.440455	39.189517
2544.331931	215961.768624	39.194535
2546.926508	216366.911309	39.199552
2549.125415	216765.180702	39.204570
2551.662595	217173.559351	39.209588
2554.066389	217576.903740	39.214605
2557.073804	217985.260707	39.219623
2559.122076	218397.577848	39.224640
2562.119760	218811.703655	39.229658
2564.565447	219235.442146	39.234676
2567.175209	219644.548107	39.239693
2569.430539	220069.002685	39.244711
2571.884748	220488.879251	39.249728
2575.060744	220907.881602	39.254746
2577.808547	221322.632117	39.259764
2580.385180	221743.811280	39.264781
2583.458709	222164.532234	39.269799
2586.160108	222577.944080	39.274816
2588.928639	222990.532687	39.279834
2591.547939	223391.636588	39.284852
2593.618205	223809.237068	39.289869
2596.619333	224226.235499	39.294887
2598.966463	224653.141756	39.299904
2601.722532	225062.455600	39.304922
2604.577477	225468.959640	39.309940
2607.084729	225888.473894	39.314957
2610.110558	226290.277001	39.319975
2612.772640	226704.279855	39.324992
2615.496039	227116.977524	39.330010
2618.137026	227521.355423	39.335028
2621.056605	227932.472792	39.340045
2624.128749	228337.367737	39.345063
2626.310462	228745.881510	39.350080
2628.954397	229136.006903	39.355098
2631.472623	229543.756748	39.360116
2634.320547	229945.281951	39.365133
2636.974264	230353.315245	39.370151
2639.315146	230756.494063	39.375168
2642.161594	231156.012043	39.380186
2644.715869	231560.452852	39.385204
2646.971497	231966.286319	39.390221
2649.741560	232350.750958	39.395239
2652.201725	232736.584595	39.400256
2654.978398	233119.244041	39.405274
2657.128040	233493.007819	39.410292
2659.284870	233877.566874	39.415309
2662.261196	234261.363011	39.420327
2664.575714	234652.933801	39.425344
2667.502998	235031.884810	39.430362
2669.722992	235441.099892	39.435380
2672.327461	235843.802186	39.440397
2674.649068	236238.774552	39.445415
2677.281948	236652.369826	39.450432
2679.854851	237049.969645	39.455450
2682.895272	237456.971849	39.460468
2686.021742	237866.119500	39.465485
2688.519107	238275.542386	39.470503
2690.944797	238688.888068	39.475520
2693.972781	239112.453326	39.480538
2696.681437	239527.532114	39.485556
2699.199502	239946.094857	39.490573
2702.629727	240373.863513	39.495591
2704.658385	240800.935107	39.500608
2707.647161	241231.438494	39.505626
2709.969648	241653.255321	39.510644
2712.652047	242094.448958	39.515661
2715.168382	242522.102338	39.520679
2717.745844	242971.414378	39.525696
2720.376555	243415.687463	39.530714
2723.186826	243876.138927	39.535732
2725.482218	244317.007629	39.540749
2728.969725	244774.151071	39.545767
2731.456334	245233.100494	39.550784
2734.375454	245686.774020	39.555802
2736.911065	246144.926318	39.560820
2739.632191	246598.704831	39.565837
2742.665134	247060.715054	39.570855
2745.316303	247528.041924	39.575872
2748.273468	247978.859148	39.580890
2751.471514	248440.281436	39.585908
2754.133061	248908.771709	39.590925
2757.205895	249362.539565	39.595943
2759.846377	249830.852834	39.600960
2762.745567	250280.199886	39.605978
2765.798962	250747.989111	39.610996
2768.391863	251213.765691	39.616013
2771.186374	251662.109161	39.621031
2774.096197	252126.944685	39.626048
2776.562353	252588.139187	39.631066
2779.981290	253036.076696	39.636084
2782.625634	253512.049903	39.641101
2785.697412	253954.120072	39.646119
2788.416695	254420.807062	39.651136
2790.775412	254877.946880	39.656154
2794.271323	255327.618042	39.661172
2797.133128	255793.846473	39.666189
2800.170808	256241.299835	39.671207
2803.020783	256693.226116	39.676224
2805.698101	257142.917028	39.681242
2808.484175	257597.974469	39.686260
2811.367117	258060.508484	39.691277
2814.603201	258510.412468	39.696295
2817.076350	258961.297181	39.701312
2819.851708	259410.380575	39.706330
2822.489657	259861.261729	39.711348
2825.124798	260316.967702	39.716365
2828.163811	260774.793499	39.721383
2830.411339	261229.032241	39.726400
2833.307219	261682.838097	39.731418
2836.446950	262126.774395	39.736436
2838.912450	262557.123313	39.741453
2841.693964	262985.871999	39.746471
2844.173028	263410.906921	39.751488
2846.691937	263853.434311	39.756506
2849.492428	264281.743135	39.761524
2852.466747	264718.862172	39.766541
2855.050266	265151.188938	39.771559
2857.999872	265607.560764	39.776576
2860.322735	266048.864846	39.781594
2863.340697	266506.568165	39.786612
2866.064422	266953.622271	39.791629
2868.723181	267406.678573	39.796647
2871.940233	267872.319812	39.801664
2874.744309	268337.565911	39.806682
2877.679976	268796.414288	39.811700
2880.348817	269274.731624	39.816717
2883.152279	269744.060044	39.821735
2886.019189	270237.478901	39.826752
2889.032328	270712.585909	39.831770
2891.886521	271192.591529	39.836788
2894.702965	271678.797470	39.841805
2897.760287	272162.956874	39.846823
2900.371060	272660.846848	39.851840
2903.399682	273154.884780	39.856858
2906.276357	273656.283258	39.861876
2908.987575	274162.555335	39.866893
2912.074702	274644.816799	39.871911
2915.249265	275150.934626	39.876928
2917.979271	275651.988468	39.881946
2921.047286	276162.357855	39.886964
2924.303625	276673.507395	39.891981
2927.487393	277184.182452	39.896999
2930.491541	277690.742672	39.902016
2933.271902	278191.290308	39.907034
2936.451302	278698.857953	39.912052
2939.143429	279204.288702	39.917069
2942.290279	279720.768390	39.922087
2945.415232	280234.302155	39.927104
2948.632447	280748.198966	39.932122
2951.440189	281254.385210	39.937140
2954.074226	281773.190615	39.942157
2957.329212	282282.982339	39.947175
2960.193351	282806.772602	39.952192
2963.221464	283316.770063	39.957210
2966.362783	283832.104301	39.962228
2969.245335	284354.051937	39.967245
2972.286779	284878.459479	39.972263
2975.679463	285396.333148	39.977280
2978.223556	285916.112457	39.982298
2981.676808	286427.595256	39.987316
2984.352322	286946.736766	39.992333
2987.586931	287455.808063	39.997351
2990.399354	287972.025539	40.002368
2993.305637	288505.389270	40.007386
2996.744890	289015.051423	40.012404
2999.603800	289533.153661	40.017421
3002.932815	290042.240821	40.022439
3006.409972	290561.482668	40.027456
3009.305113	291069.029443	40.032474
3012.806411	291583.612546	40.037492
3015.427007	292080.707455	40.042509
3018.210666	292587.599003	40.047527
3021.027605	293094.836626	40.052544
3024.109394	293612.260889	40.057562
3027.579663	294101.793240	40.062580
3030.589146	294616.503398	40.067597
3033.859641	295117.001310	40.072615
3036.915295	295617.680731	40.077632
3039.442212	296091.906900	40.082650
3042.460677	296560.391055	40.087668
3045.353379	297041.813637	40.092685
3048.128615	297505.681868	40.097703
3050.705211	297985.876272	40.102720
3053.565765	298468.485014	40.107738
3056.650088	298958.467927	40.112756
3059.153324	299455.416905	40.117773
3061.943062	299952.316840	40.122791
3065.214455	300458.175029	40.127808
3067.875597	300961.584843	40.132826
3070.969575	301465.709607	40.137844
3073.667187	301982.279740	40.142861
3076.615416	302508.122487	40.147879
3079.908566	303029.133870	40.152896
3082.634474	303565.764197	40.157914
3086.186266	304093.172664	40.162932
3089.357824	304631.118880	40.167949
3092.560290	305166.389315	40.172967
3095.784234	305696.142445	40.177984
3098.625786	306237.220078	40.183002
3101.958817	306779.941548	40.188020
3104.955038	307331.365336	40.193037
3108.083871	307877.254260	40.198055
3111.314800	308424.821951	40.203072
3114.409986	308984.385277	40.208090
3117.511323	309533.483745	40.213108
3120.727214	310093.218644	40.218125
3124.270400	310653.149950	40.223143
3127.530563	311210.529865	40.228160
3130.463623	311766.659734	40.233178
3134.082576	312330.848976	40.238196
3137.038402	312895.489978	40.243213
3140.076605	313454.375418	40.248231
3143.413667	314022.623584	40.253248
3146.695750	314583.716267	40.258266
3150.127479	315139.144600	40.263284
3152.830676	315708.485707	40.268301
3156.314054	316278.941811	40.273319
3159.585757	316838.663212	40.278336
3162.730293	317408.802392	40.283354
3166.148436	317972.877173	40.288372
3169.303922	318543.913651	40.293389
3172.965305	319115.041622	40.298407
3176.090923	319674.825975	40.303424
3178.872538	320249.628703	40.308442
3182.273877	320818.363967	40.313460
3185.225497	321386.857160	40.318477
3188.717731	321956.425910	40.323495
3192.137686	322523.892123	40.328512
3195.297010	323098.546906	40.333530
3198.848735	323651.995920	40.338548
3202.095133	324222.105053	40.343565
3205.209629	324781.646049	40.348583
3208.097244	325344.234166	40.353600
3211.265463	325918.137962	40.358618
3214.806527	326492.635329	40.363636
3217.707985	327062.580949	40.368653
3220.988802	327635.732431	40.373671
3224.594809	328199.716724	40.378688
3227.505984	328768.773886	40.383706
3230.522599	329333.797870	40.388724
3233.983447	329903.514246	40.393741
3236.818324	330472.558631	40.398759
3240.212474	331049.930391	40.403776
3243.416959	331634.045907	40.408794
3246.583453	332200.425606	40.413812
3250.091495	332773.644010	40.418829
3253.021623	333323.833327	40.423847
3256.277786	333858.895445	40.428864
3259.032545	334408.132280	40.433882
3262.210169	334939.741258	40.438900
3265.504893	335476.194842	40.443917
3268.751839	336037.938331	40.448935
3271.980186	336585.724903	40.453952
3274.848494	337148.144528	40.458970
3278.401198	337694.773326	40.463988
3281.550780	338265.730733	40.469005
3284.863782	338826.254307	40.474023
3287.687203	339395.418363	40.479040
3290.758977	339978.053513	40.484058
3293.589018	340564.571953	40.489076
3296.596291	341159.955428	40.494093
3299.858367	341756.810941	40.499111
3303.175223	342364.147584	40.504128
3306.382232	342976.639118	40.509146
3309.820844	343588.373700	40.514164
3313.105677	344204.483383	40.519181
3316.164706	344836.036061	40.524199
3319.819461	345459.952575	40.529216
3323.552075	346082.121100	40.534234
3326.995513	346716.114942	40.539252
3330.155195	347333.683546	40.544269
3333.318482	347968.483422	40.549287
3337.511523	348594.261288	40.554304
3340.973126	349228.939928	40.559322
3344.136851	349856.274033	40.564340
3347.835306	350498.168540	40.569357
3351.042091	351132.621770	40.574375
3354.881057	351764.099132	40.579392
3358.141324	352398.747408	40.584410
3361.104162	353039.869278	40.589428
3364.921303	353672.808371	40.594445
3368.484225	354312.746420	40.599463
3372.597264	354955.754943	40.604480
3375.601608	355586.475169	40.609498
3379.246372	356223.091269	40.614516
3382.600103	356862.046562	40.619533
3385.770944	357503.501464	40.624551
3389.449818	358134.014342	40.629568
3392.977865	358788.112396	40.634586
3396.229480	359423.126662	40.639604
3399.700895	360062.934937	40.644621
3403.412609	360702.210690	40.649639
3407.046571	361328.456640	40.654656
3410.375950	361972.758204	40.659674
3414.087898	362605.023074	40.664692
3417.615424	363232.386184	40.669709
3420.912897	363859.138157	40.674727
3424.490564	364489.077241	40.679744
3428.067868	365126.834036	40.684762
3431.858508	365755.445489	40.689780
3435.397399	366380.737275	40.694797
3438.595646	367006.550032	40.699815
3441.956910	367630.803314	40.704832
3445.058774	368265.245071	40.709850
3448.544094	368896.420150	40.714868
3452.482867	369516.563822	40.719885
3455.654372	370158.174269	40.724903
3458.836122	370770.705016	40.729920
3462.248289	371412.147991	40.734938
3465.865828	372049.996994	40.739956
3469.399128	372678.165729	40.744973
3472.802480	373312.395800	40.749991
3476.450879	373940.239171	40.755008
3479.474349	374557.176585	40.760013
3483.119659	375133.234676	40.765018
3486.376073	375682.341975	40.770023
3489.305643	376178.025189	40.775028
3492.578528	376623.764075	40.780032
3495.468852	377018.480346	40.785037
3497.683430	377369.460115	40.790042
3500.024447	377674.294524	40.795047
3502.035583	377949.995843	40.800052
3503.855244	378155.197743	40.805056
3505.825262	378325.708500	40.810061
3507.206814	378466.189694	40.815066
3508.968796	378572.300652	40.820071
3510.035287	378658.329475	40.825076
3511.140292	378711.819637	40.830080
3512.104211	378737.015033	40.835085
3513.055638	378740.981238	40.840090
3514.385837	378701.689749	40.845095
3514.765074	378661.327169	40.850100
3515.628324	378582.642520	40.855104
3516.028571	378495.902871	40.860109
3516.437045	378399.688804	40.865114
3516.796955	378269.780780	40.870119
3517.233611	378160.812407	40.875124
3517.884939	378016.711878	40.880128
3518.039421	377861.589439	40.885133
3518.047632	377699.860228	40.890138
3518.280389	377540.812600	40.895143
3518.191509	377364.823234	40.900148
3518.200622	377180.360078	40.905152
3517.812924	377000.224222	40.910157
3518.190682	376826.774679	40.915162
3518.302797	376627.306939	40.920167
3518.349244	376444.052031	40.925172
3518.260408	376242.682449	40.930176
3517.580276	376043.892444	40.935181
3517.295687	375845.928384	40.940186
3517.615548	375644.363754	40.945191
3517.123562	375458.265068	40.950196
3517.227790	375255.384949	40.955200
3516.780186	375064.247582	40.960205
3516.266810	374878.199052	40.965210
3516.497670	374671.484918	40.970215
3516.222984	374490.349582	40.975220
3516.153648	374297.954177	40.980224
3515.611045	374104.081640	40.985229
3515.581785	373917.875035	40.990234
3515.391986	373723.081282	40.995239
3514.900247	373539.992176	41.000244
3514.929681	373355.880909	41.005248
3514.728402	373181.431404	41.010253
3514.635539	372995.101444	41.015258
3514.514882	372813.778674	41.020263
3514.302754	372649.691360	41.025268
3513.793863	372469.519023	41.030272
3513.674274	372304.373783	41.035277
3513.351293	372135.245655	41.040282
3513.421949	371970.729285	41.045287
3513.114115	371798.345242	41.050292
3512.850513	371643.023868	41.055296
3512.543243	371483.466149	41.060301
3512.429641	371322.048365	41.065306
3512.513632	371171.852489	41.070311
3512.191135	371024.437210	41.075316
3511.632406	370861.104577	41.080320
3511.705715	370721.806010	41.085325
3511.187346	370572.818411	41.090330
3511.135422	370431.073733	41.095335
3510.708903	370300.716781	41.100340
3510.790499	370161.414146	41.105344
3510.638416	370029.870052	41.110349
3510.532835	369889.045543	41.115354
3510.890762	369758.716440	41.120359
3510.366258	369628.981334	41.125364
3510.511947	369497.540849	41.130368
3510.059446	369366.827959	41.135373
3509.602805	369231.313587	41.140378
3510.088521	369114.883505	41.145383
3509.801810	368989.224070	41.150388
3509.634128	368869.693617	41.155392
3509.572335	368754.668328	41.160397
3509.057498	368636.130910	41.165402
3509.025660	368514.392959	41.170407
3508.973622	368408.637767	41.175412
3508.967081	368292.992281	41.180416
3508.521092	368184.147251	41.185421
3508.732596	368071.947536	41.190426
3508.794342	367967.113021	41.195431
3508.468433	367861.423827	41.200436
3508.318396	367758.933462	41.205440
3508.189843	367648.360186	41.210445
3507.910743	367551.961267	41.215450
3508.023359	367442.188078	41.220455
3508.091656	367339.077887	41.225460
3507.870598	367240.839618	41.230464
3507.753145	367147.310543	41.235469
3507.574744	367050.970493	41.240474
3507.610854	366957.289870	41.245479
3507.547644	366874.752656	41.250484
3507.113838	366769.457337	41.255488
3507.366510	366677.825487	41.260493
3507.010061	366600.084255	41.265498
3507.074098	366507.236263	41.270503
3506.825720	366432.247157	41.275508
3506.726962	366334.469507	41.280512
3506.538621	366251.035314	41.285517
3506.949937	366178.737722	41.290522
3506.471222	366084.778678	41.295527
3506.193904	366010.987144	41.300532
3506.420773	365933.458242	41.305536
3506.170510	365850.032530	41.310541
3505.998236	365776.325685	41.315546
3505.918791	365696.607918	41.320551
3505.796165	365628.254061	41.325556
3506.034938	365561.800231	41.330560
3506.066445	365494.768706	41.335565
3506.039659	365419.615458	41.340570
3505.982522	365343.247141	41.345575
3505.590341	365269.827316	41.350580
3505.377586	365195.108962	41.355584
3505.803285	365135.027999	41.360589
3505.538823	365059.072327	41.365594
3505.917188	364981.161596	41.370599
3505.530877	364923.035978	41.375604
3505.459053	364859.474654	41.380608
3505.343591	364797.724006	41.385613
3505.281806	364722.803090	41.390618
3505.776510	364660.753934	41.395623
3505.449122	364594.665503	41.400628
3505.418077	364529.775851	41.405632
3505.330445	364462.074453	41.410637
3505.379277	364397.019623	41.415642
3505.434783	364324.721988	41.420647
3505.088284	364266.334778	41.425652
3505.409914	364203.346036	41.430656
3504.951943	364141.164528	41.435661
3505.030305	364079.839576	41.440666
3504.950870	364014.930907	41.445671
3505.299157	363964.032410	41.450676
3505.242058	363903.287179	41.455680
3505.159574	363841.859713	41.460685
3505.103525	363780.758331	41.465690
3505.034289	363713.763818	41.470695
3505.009907	363658.221985	41.475700
3505.222714	363595.731665	41.480704
3505.071487	363537.490491	41.485709
3504.935938	363480.161520	41.490714
3504.804798	363408.780029	41.495719
3504.640467	363359.306989	41.500724
3504.943411	363290.957690	41.505728
3504.799534	363235.459067	41.510733
3504.743213	363184.495138	41.515738
3504.850386	363121.359589	41.520743
3504.701635	363071.248387	41.525748
3504.762503	363015.260105	41.530752
3504.678401	362961.428749	41.535757
3504.003690	362908.908901	41.540762
3504.692260	362848.934833	41.545767
3504.262184	362807.709806	41.550772
3504.604987	362746.849148	41.555776
3504.783754	362692.264902	41.560781
3504.464714	362635.648937	41.565786
3504.533488	362572.569017	41.570791
3504.745595	362524.560648	41.575796
3504.600941	362461.894867	41.580800
3504.592315	362421.061115	41.585805
3504.540905	362375.100967	41.590810
3504.309840	362308.230103	41.595815
3504.391734	362264.256505	41.600820
3504.145531	362212.837649	41.605824
3504.265218	362156.940243	41.610829
3504.159118	362107.862633	41.615834
3504.208655	362064.071653	41.620839
3504.048939	362021.939486	41.625844
3504.206631	361969.390090	41.630848
3504.504080	361916.386862	41.635853
3504.363204	361874.073676	41.640858
3504.413975	361822.582524	41.645863
3504.219621	361772.984459	41.650868
3504.279177	361721.364709	41.655872
3504.429888	361665.334498	41.660877
3504.127856	361616.566098	41.665882
3504.689405	361565.579485	41.670887
3504.192752	361510.132542	41.675892
3504.273443	361458.102464	41.680896
3504.171454	361410.395299	41.685901
3504.352101	361362.517019	41.690906
3504.570555	361308.788069	41.695911
3504.226529	361259.415739	41.700916
3503.814261	361213.103370	41.705920
3504.101224	361158.397840	41.710925
3503.865163	361117.216521	41.715930
3504.140007	361073.668565	41.720935
3504.043282	361024.155717	41.725940
3503.984755	360983.708949	41.730944
3503.858656	360924.925106	41.735949
3503.905097	360885.580005	41.740954
3504.125668	360834.594390	41.745959
3503.940358	360787.839455	41.750964
3503.856662	360746.278147	41.755968
3504.032107	360691.360412	41.760973
3504.110019	360645.758673	41.765978
3503.846976	360599.244252	41.770983
3503.741103	360562.794031	41.775988
3503.812890	360515.490417	41.780992
3503.859797	360479.575395	41.785997
3503.682350	360430.175782	41.791002
3504.006381	360384.179574	41.796007
3503.530854	360344.914993	41.801012
3503.735620	360293.270197	41.806016
3503.888544	360249.384247	41.811021
3503.966156	360200.020806	41.816026
3503.978045	360157.401892	41.821031
3503.842334	360119.583491	41.826036
3503.704234	360058.639743	41.831040
3504.079318	360014.312276	41.836045
3503.710453	359978.867965	41.841050
3503.991307	359939.866349	41.846055
3503.657419	359893.768474	41.851060
3503.123817	359853.800729	41.856064
3503.297921	359808.538543	41.861069
3503.257535	359777.159794	41.866074
3503.138532	359735.577179	41.871079
3503.193973	359703.522701	41.876084
3503.583526	359662.521590	41.881088
3503.549568	359623.517731	41.886093
3503.451063	359585.413329	41.891098
3503.624165	359539.540980	41.896103
3503.336870	359504.032595	41.901108
3503.386868	359470.657227	41.906112
3503.642134	359428.761818	41.911117
3503.092708	359389.050057	41.916122
3503.218721	359352.765604	41.921127
3503.110353	359330.901594	41.926132
3503.367425	359296.731409	41.931136
3504.011183	359248.752305	41.936141
3503.300540	359208.811261	41.941146
3503.542764	359164.223682	41.946151
3503.541312	359123.867205	41.951156
3503.147317	359078.514441	41.956160
3503.701445	359043.230374	41.961165
3503.293494	359005.732502	41.966170
3503.670055	358959.319346	41.971175
3503.412142	358923.475332	41.976180
3503.320736	358880.769050	41.981184
3503.593380	358844.232451	41.986189
3503.477765	358802.851346	41.991194
3503.446486	358768.954168	41.996199
3503.374388	358730.361724	42.001204
3503.386041	358697.804725	42.006208
3503.597287	358655.000202	42.011213
3503.280317	358616.928587	42.016218
3503.663817	358567.972354	42.021223
3503.474979	358536.996642	42.026228
3503.661109	358490.358268	42.031232
3503.926261	358450.493113	42.036237
3503.469401	358403.548038	42.041242
3503.392517	358358.831044	42.046247
3503.268351	358331.936755	42.051252
3503.638717	358288.319118	42.056256
3503.755449	358241.818238	42.061261
3503.343161	358212.122272	42.066266
3503.777232	358165.800624	42.071271
3503.223425	358129.620510	42.076276
3503.000664	358084.519187	42.081280
3503.361581	358052.822075	42.086285
3503.093552	358017.156477	42.091290
3503.329931	357981.641076	42.096295
3502.962312	357954.174391	42.101300
3502.936336	357913.159357	42.106304
3503.095592	357874.046958	42.111309
3502.845087	357850.424983	42.116314
3503.055519	357809.245949	42.121319
3503.172696	357775.807452	42.126324
3503.236459	357737.573840	42.131328
3503.353385	357708.125427	42.136333
3503.170538	357677.376649	42.141338
3503.125513	357632.602813	42.146343
3503.113965	357605.461630	42.151348
3503.143777	357561.006438	42.156352
3503.403800	357524.419406	42.161357
3502.936861	357499.382190	42.166362
3503.315469	357460.209718	42.171367
3503.426052	357420.773923	42.176372
3503.406502	357393.938780	42.181376
3503.072074	357346.312249	42.186381
3503.091147	357306.763474	42.191386
3503.208299	357273.375267	42.196391
3503.119713	357244.212544	42.201396
3503.353437	357197.437733	42.206400
3503.422511	357167.767514	42.211405
3503.120725	357126.362296	42.216410
3503.368416	357090.894943	42.221415
3503.051250	357065.427424	42.226420
3503.170703	357024.820640	42.231424
3503.159904	356984.844042	42.236429
3502.727425	356956.293700	42.241434
3503.032273	356919.876887	42.246439
3503.109125	356888.604019	42.251444
3503.053243	356864.671434	42.256448
3503.215254	356830.513306	42.261453
3503.092691	356797.797278	42.266458
3502.859026	356751.831577	42.271463
3502.840436	356721.335860	42.276468
3502.892359	356693.701106	42.281472
3503.151235	356655.918694	42.286477
3502.703882	356633.571788	42.291482
3502.999341	356594.131590	42.296487
3503.093475	356558.814603	42.301492
3503.222895	356527.050292	42.306496
3502.955620	356482.029806	42.311501
3503.207275	356443.867024	42.316506
3503.258535	356411.453947	42.321511
3503.057251	356384.442884	42.326516
3503.024994	356343.782572	42.331520
3503.243857	356311.902460	42.336525
3503.080078	356288.367461	42.341530
3502.961668	356243.857200	42.346535
3502.916466	356213.390543	42.351540
3502.727455	356177.532617	42.356544
3502.529779	356148.538337	42.361549
3502.534511	356121.977894	42.366554
3502.976932	356087.724485	42.371559
3503.035673	356067.382539	42.376564
3502.989526	356026.596894	42.381568
3503.162756	355991.800698	42.386573
3503.154711	355964.632121	42.391578
3503.069475	355921.793708	42.396583
3502.734924	355894.472549	42.401588
3502.828789	355856.206522	42.406592
3503.008710	355828.957744	42.411597
3502.697412	355807.453228	42.416602
3502.739352	355767.517694	42.421607
3502.781621	355732.157011	42.426612
3502.653863	355704.600175	42.431616
3502.908077	355670.909342	42.436621
3502.498632	355650.360399	42.441626
3502.926606	355611.864167	42.446631
3503.098884	355587.691766	42.451636
3502.934532	355559.200085	42.456640
3503.128362	355525.060994	42.461645
3502.795612	355493.265887	42.466650
3503.014883	355457.953601	42.471655
3503.004316	355426.235373	42.476660
3502.722127	355395.347297	42.481664
3503.097189	355360.646076	42.486669
3502.955230	355323.991933	42.491674
3503.210538	355288.114680	42.496679
3502.934514	355264.952212	42.501684
3502.458539	355223.114071	42.506688
3502.745554	355202.303955	42.511693
3502.869168	355162.964947	42.516698
3502.861059	355138.540685	42.521703
3502.793202	355109.779411	42.526708
3503.053442	355072.757385	42.531712
3503.183238	355044.600718	42.536717
3502.877638	355012.572146	42.541722
3502.962521	354981.804462	42.546727
3502.740247	354949.686608	42.551732
3502.731665	354920.102592	42.556736
3502.824292	354886.054808	42.561741
3502.328887	354852.556001	42.566746
3502.612373	354825.722329	42.571751
3502.480899	354796.004817	42.576756
3502.421178	354773.647094	42.581760
3502.717046	354739.491274	42.586765
3502.640877	354716.017713	42.591770
3502.756701	354692.260085	42.596775
3502.652101	354666.350856	42.601780
3502.656153	354634.172044	42.606784
3503.004672	354606.336792	42.611789
3502.777141	354571.652223	42.616794
3502.510009	354526.349315	42.621799
3502.584611	354499.573289	42.626804
3502.415008	354478.096648	42.631808
3502.715987	354451.158267	42.636813
3502.669552	354437.109740	42.641818
3503.100830	354392.002968	42.646823
3502.734050	354367.227243	42.651828
3502.646819	354344.949751	42.656832
3503.048899	354309.404392	42.661837
3502.852586	354286.406724	42.666842
3502.773040	354250.504148	42.671847
3502.769195	354210.573765	42.676852
3502.483322	354187.056191	42.681856
3502.883639	354144.571903	42.686861
3502.660629	354125.263836	42.691866
3502.782700	354093.371122	42.696871
3503.443418	354067.266056	42.701876
3503.141921	354034.880005	42.706880
3503.381664	353994.377672	42.711885
3502.736200	353971.475087	42.716890
3502.754455	353931.820511	42.721895
3502.946075	353899.484676	42.726900
3502.939933	353867.637104	42.731904
3502.907459	353835.259822	42.736909
3502.776295	353805.795512	42.741914
3502.841878	353763.921999	42.746919
3502.792418	353744.586694	42.751924
3502.581418	353726.547416	42.756928
3502.416012	353688.827468	42.761933
3502.674334	353661.742548	42.766938
3502.669107	353628.064493	42.771943
3502.375379	353602.819277	42.776948
3502.463586	353569.762075	42.781952
3502.483746	353542.866623	42.786957
3502.767563	353524.089358	42.791962
3502.723136	353494.687517	42.796967
3502.752077	353466.799325	42.801972
3502.796168	353440.001736	42.806977
3503.000763	353400.902121	42.811981
3503.301454	353375.411717	42.816986
3502.949672	353334.593901	42.821991
3502.838542	353291.222166	42.826996
3502.759760	353262.511752	42.832001
3502.654467	353236.245606	42.837005
3502.400490	353203.876732	42.842010
3502.515397	353175.847817	42.847015
3502.740440	353157.765781	42.852020
3502.307657	353131.575929	42.857025
3502.570075	353097.169366	42.862029
3502.413883	353080.265026	42.867034
3502.143250	353051.558859	42.872039
3502.385513	353038.278183	42.877044
3502.559158	353015.730397	42.882049
3502.833150	352973.874254	42.887053
3502.787972	352948.589843	42.892058
3502.948680	352926.628636	42.897063
3502.813846	352896.655683	42.902068
3502.468980	352864.681890	42.907073
3502.916484	352831.593432	42.912077
3502.785489	352805.280093	42.917082
3502.749984	352771.987129	42.922087
3502.978627	352727.519587	42.927092
3502.723038	352704.479163	42.932097
3503.308350	352668.725533	42.937101
3502.731003	352634.296638	42.942106
3502.858966	352606.316031	42.947111
3502.716449	352576.013528	42.952116
3502.400128	352548.864575	42.957121
3502.845171	352518.953547	42.962125
3502.640553	352488.152245	42.967130
3502.632111	352460.904470	42.972135
3502.648197	352437.796158	42.977140
3502.373410	352412.165769	42.982145
3502.656809	352368.934744	42.987149
3502.430019	352352.828998	42.992154
3502.714952	352325.713389	42.997159
3502.610315	352291.159728	43.002164
3502.378785	352270.580906	43.007169
3502.431315	352243.475973	43.012173
3502.472843	352222.676695	43.017178
3502.342578	352193.159921	43.022183
3502.746590	352162.466951	43.027188
3502.543936	352132.097130	43.032193
3502.782936	352106.157771	43.037197
3502.805109	352084.827611	43.042202
3502.396847	352040.992036	43.047207
3502.582176	352018.619668	43.052212
3502.653032	351994.104450	43.057217
3502.547619	351961.101139	43.062221
3502.576362	351931.864414	43.067226
3502.313001	351908.672112	43.072231
3502.381032	351886.317905	43.077236
3502.437089	351856.517634	43.082241
3502.665409	351817.056527	43.087245
3502.463289	351808.292914	43.092250
3502.444461	351784.376142	43.097255
3502.708898	351762.499678	43.102260
3502.325919	351739.605483	43.107265
3502.839769	351709.860936	43.112269
3502.435296	351687.224245	43.117274
3502.499680	351649.491560	43.122279
3502.402072	351623.553355	43.127284
3502.265541	351597.849963	43.132289
3502.421994	351562.593980	43.137293
3502.012386	351552.845796	43.142298
3502.070642	351518.647256	43.147303
3502.392846	351505.938164	43.152308
3502.526506	351481.387365	43.157313
3502.536552	351444.196711	43.162317
3502.560798	351427.441363	43.167322
3502.445536	351402.802140	43.172327
3502.707807	351364.326573	43.177332
3502.496928	351346.921434	43.182337
3502.961799	351308.744733	43.187341
3502.159209	351280.068924	43.192346
3502.604063	351254.020589	43.197351
3502.669009	351229.988692	43.202356
3502.201561	351212.089586	43.207361
3502.038078	351181.865297	43.212365
3502.221259	351163.788659	43.217370
3502.311202	351142.955733	43.222375
3502.362317	351117.807422	43.227380
3502.394652	351103.185934	43.232385
3502.166962	351074.928883	43.237389
3502.255666	351052.215003	43.242394
3502.055932	351029.088429	43.247399
3502.220461	351007.328684	43.252404
3502.141576	350986.674451	43.257409
3502.492302	350959.649141	43.262413
3502.196504	350929.826510	43.267418
3502.010243	350913.764580	43.272423
3502.400463	350887.978657	43.277428
3502.457530	350874.471710	43.282433
3502.510209	350843.577961	43.287437
3502.330214	350814.982799	43.292442
3502.226808	350797.153916	43.297447
3502.333399	350770.929051	43.302452
3502.354342	350746.827383	43.307457
3502.258646	350715.321092	43.312461
3502.235765	350688.175753	43.317466
3502.125673	350661.043962	43.322471
3502.243505	350644.604113	43.327476
3502.179124	350623.718608	43.332481
3502.189915	350589.399374	43.337485
3502.380239	350588.429293	43.342490
3502.498214	350552.517270	43.347495
3502.450701	350529.290392	43.352500
3502.030214	350509.909199	43.357505
3502.478204	350494.155094	43.362509
3501.902695	350473.501554	43.367514
3502.412470	350444.925833	43.372519
3502.304376	350428.622715	43.377524
3502.049358	350412.291610	43.382529
3502.301647	350384.188055	43.387533
3502.282048	350353.966028	43.392538
3502.534405	350335.318911	43.397543
3502.182172	350312.851076	43.402548
3502.358190	350284.683043	43.407553
3502.560900	350257.197191	43.412557
3502.222844	350236.023556	43.417562
3502.450026	350203.195489	43.422567
3502.548456	350175.852901	43.427572
3502.347637	350156.640682	43.432577
3502.701022	350119.064617	43.437581
3502.524131	350099.086015	43.442586
3502.532090	350073.918194	43.447591
3502.646940	350041.641285	43.452596
3502.201763	350013.213790	43.457601
3502.694308	349983.343881	43.462605
3502.620027	349959.586923	43.467610
3502.520219	349931.944507	43.472615
3502.845966	349908.659104	43.477620
3502.289029	349888.358198	43.482625
3502.346998	349864.326381	43.487629
3502.311834	349832.098031	43.492634
3502.231049	349810.884085	43.497639
3502.497085	349788.421364	43.502644
3502.225785	349755.822947	43.507649
3502.506497	349737.145657	43.512653
3501.967722	349719.765253	43.517658
3502.363315	349699.799006	43.522663
3502.306457	349671.717527	43.527668
3502.186369	349637.544768	43.532673
3502.619825	349623.826206	43.537677
3502.329567	349608.211978	43.542682
3502.537023	349560.769114	43.547687
3502.592040	349541.770936	43.552692
3502.519660	349515.954236	43.557697
3502.272092	349484.724608	43.562701
3502.279402	349463.471308	43.567706
3502.587390	349438.205470	43.572711
3502.576127	349407.879588	43.577716
3502.362162	349382.694929	43.582721
3502.403143	349356.885885	43.587725
3502.472924	349332.775578	43.592730
3502.416922	349312.574313	43.597735
3502.503702	349284.114251	43.602740
3502.370814	349266.822974	43.607745
3502.412698	349236.590351	43.612749
3502.109334	349223.647242	43.617754
3502.145348	349199.923415	43.622759
3502.306943	349170.078847	43.627764
3502.240389	349153.539836	43.632769
3502.476146	349125.361514	43.637773
3502.732886	349094.459785	43.642778
3501.729378	349061.262814	43.647783
3502.075692	349051.777574	43.652788
3502.174326	349032.746894	43.657793
3502.499362	349008.266146	43.662797
3502.113160	348986.590762	43.667802
3502.068867	348969.133013	43.672807
3502.364970	348936.242115	43.677812
3502.287042	348917.162578	43.682817
3502.611712	348885.563695	43.687821
3502.435515	348868.558589	43.692826
3501.963046	348833.677177	43.697831
3502.536244	348809.055978	43.702836
3502.078182	348789.832147	43.707841
3502.215742	348765.329550	43.712845
3502.303804	348756.977555	43.717850
3502.389716	348720.661771	43.722855
3502.559785	348695.671047	43.727860
3502.108307	348674.615743	43.732865
3502.500423	348648.522707	43.737869
3502.557507	348624.515547	43.742874
3502.520055	348596.862307	43.747879
3502.575365	348574.660352	43.752884
3502.091853	348545.296938	43.757889
3502.391514	348516.625134	43.762893
3502.252936	348491.529753	43.767898
3502.101013	348476.554438	43.772903
3502.411171	348454.795765	43.777908
3502.008062	348432.054918	43.782913
3501.933819	348399.500762	43.787917
3502.174255	348388.125145	43.792922
3501.763019	348372.046136	43.797927
3502.552227	348347.060492	43.802932
3501.966393	348322.644716	43.807937
3502.201265	348294.491247	43.812941
3502.390061	348281.750827	43.817946
3502.423023	348249.306953	43.822951
3502.334208	348218.864939	43.827956
3502.211756	348200.757967	43.832961
3502.220922	348184.511757	43.837965
3502.314276	348160.346084	43.842970
3501.987383	348136.906770	43.847975
3502.458204	348107.750377	43.852980
3502.096272	348092.477076	43.857985
3502.037724	348076.495576	43.862989
3502.316021	348051.309569	43.867994
3502.081505	348033.219944	43.872999
3502.352545	347993.773017	43.878004
3502.105264	347986.388222	43.883009
3502.245716	347957.842402	43.888013
3502.105430	347937.907640	43.893018
3502.093738	347923.266169	43.898023
3502.172493	347892.543555	43.903028
3502.051665	347887.757585	43.908033
3501.789940	347853.452489	43.913037
3502.011286	347841.011907	43.918042
3501.721292	347820.515651	43.923047
3501.677541	347794.998226	43.928052
3501.498729	347786.712940	43.933057
3501.738856	347772.464401	43.938061
3501.896035	347753.195075	43.943066
3502.102803	347747.239509	43.948071
3502.284136	347714.543222	43.953076
3502.109931	347704.019999	43.958081
3502.111413	347681.342792	43.963085
3502.188429	347657.586061	43.968090
3502.186693	347635.239820	43.973095
3502.156218	347607.584673	43.978100
3502.467066	347585.316870	43.983105
3502.078580	347562.979918	43.988109
3502.117923	347546.550742	43.993114
3502.140766	347525.624281	43.998119
3502.243062	347507.990417	44.003124
3502.000387	347474.825996	44.008129
3502.522584	347448.432128	44.013133
3502.382508	347432.437583	44.018138
3502.344370	347406.156300	44.023143
3502.184710	347381.368438	44.028148
3502.238542	347352.530506	44.033153
3502.128097	347334.827963	44.038157
3502.103529	347305.824229	44.043162
3501.792052	347299.517037	44.048167
3501.918806	347276.565832	44.053172
3502.049962	347265.740723	44.058177
3502.112994	347243.790911	44.063181
3502.114853	347222.104834	44.068186
3501.882844	347202.488984	44.073191
3502.115734	347175.682306	44.078196
3501.826071	347163.244723	44.083201
3501.980486	347142.526357	44.088205
3502.082925	347125.477001	44.093210
3501.813355	347103.375468	44.098215
3501.895587	347096.218854	44.103220
3501.831587	347071.085376	44.108225
3501.820494	347050.011360	44.113229
3501.420221	347035.557085	44.118234
3501.796318	347012.719438	44.123239
3501.655511	347002.546722	44.128244
3501.509827	346994.281507	44.133249
3501.792708	346961.670377	44.138253
3501.763705	346965.081704	44.143258
3501.582302	346950.644179	44.148263
3502.317065	346922.920234	44.153268
3502.171615	346909.824532	44.158273
3502.109965	346885.224439	44.163277
3502.021187	346866.043724	44.168282
3502.043334	346849.998233	44.173287
3502.287730	346832.443594	44.178292
3501.952446	346813.580865	44.183297
3502.030762	346781.992906	44.188301
3502.127242	346760.291807	44.193306
3502.088293	346741.738853	44.198311
3502.147558	346717.729984	44.203316
3502.084458	346704.748505	44.208321
3502.271434	346680.821430	44.213325
3502.235352	346660.895117	44.218330
3501.950268	346642.787185	44.223335
3502.272280	346616.500087	44.228340
3501.914508	346607.733886	44.233345
3502.213161	346580.204642	44.238349
3502.577811	346558.461682	44.243354
3502.027231	346544.640751	44.248359
3501.968243	346521.692511	44.253364
3501.800343	346492.456143	44.258369
3501.945757	346481.018396	44.263373
3501.983192	346453.580545	44.268378
3501.816533	346441.047281	44.273383
3502.004284	346418.187694	44.278388
3501.738930	346406.839267	44.283393
3501.861140	346379.896637	44.288397
3502.369972	346359.300604	44.293402
3502.006561	346348.730127	44.298407
3502.333701	346321.780985	44.303412
3502.352614	346305.227264	44.308417
3502.334144	346280.594586	44.313421
3502.752833	346254.546401	44.318426
3502.091872	346226.911958	44.323431
3502.687094	346197.480313	44.328436
3502.269527	346173.138476	44.333441
3502.203193	346150.928420	44.338445
3502.280067	346115.246815	44.343450
3502.056673	346115.027433	44.348455
3501.941625	346076.884109	44.353460
3501.767252	346065.826496	44.358465
3501.728029	346034.739184	44.363469
3502.149306	346020.080356	44.368474
3501.785997	346003.204605	44.373479
3502.278605	345985.407510	44.378484
3501.981558	345976.402879	44.383489
3501.783684	345949.560563	44.388493
3502.007223	345937.093514	44.393498
3501.822369	345916.478038	44.398503
3501.935946	345883.256612	44.403508
3501.813246	345872.623104	44.408513
3501.813421	345849.944868	44.413517
3502.279655	345830.829742	44.418522
3502.204431	345808.086938	44.423527
3502.152337	345780.942138	44.428532
3501.982809	345783.739848	44.433537
3502.143053	345755.722988	44.438541
3502.323227	345739.296441	44.443546
3501.921247	345718.663784	44.448551
3502.050573	345691.439834	44.453556
3501.973391	345666.510755	44.458561
3501.856612	345651.884649	44.463565
3501.983529	345625.118656	44.468570
3502.014949	345614.944146	44.473575
3502.237551	345596.502409	44.478580
3501.973630	345581.416107	44.483585
3502.067910	345558.011151	44.488589
3501.801495	345526.984152	44.493594
3501.808112	345522.813621	44.498599
3502.088454	345496.150775	44.503604
3501.971308	345488.363813	44.508609
3501.737641	345461.602955	44.513613
3501.853795	345448.516827	44.518618
3501.603022	345428.063859	44.523623
3501.751421	345415.887980	44.528628
3501.837361	345400.442062	44.533633
3501.716644	345379.740007	44.538637
3501.542468	345366.546479	44.543642
3501.833049	345358.645191	44.548647
3502.059293	345322.456445	44.553652
3501.514537	345317.049615	44.558657
3501.340899	345294.931971	44.563661
3501.576437	345287.242628	44.568666
3501.728985	345282.464595	44.573671
3501.586168	345258.003073	44.578676
3501.987075	345245.711566	44.583681
3501.663802	345230.736043	44.588685
3501.840201	345210.521566	44.593690
3501.638643	345203.256166	44.598695
3502.228738	345177.968647	44.603700
3501.586908	345174.865116	44.608705
3501.417418	345154.043390	44.613709
3501.671050	345137.198328	44.618714
3501.846920	345116.297412	44.623719
3501.642413	345108.829053	44.628724
3501.972447	345090.039804	44.633729
3501.957123	345066.092222	44.638733
3502.083957	345055.190806	44.643738
3501.938863	345044.001180	44.648743
3501.832890	345025.203469	44.653748
3501.899984	345008.209397	44.658753
3502.402947	344988.884687	44.663757
3501.815789	344968.000718	44.668762
3502.030210	344944.118999	44.673767
3501.922358	344917.744932	44.678772
3501.778586	344912.631587	44.683777
3502.064280	344892.705012	44.688781
3502.224821	344871.069012	44.693786
3502.261739	344854.257534	44.698791
3502.422884	344820.951395	44.703796
3501.886537	344805.703744	44.708801
3501.905337	344786.759361	44.713805
3501.767266	344759.779676	44.718810
3501.995352	344746.065663	44.723815
3502.263642	344726.065425	44.728820
3501.557099	344711.123890	44.733825
3501.828764	344688.733158	44.738829
3501.918905	344671.862458	44.743834
3502.062491	344658.848034	44.748839
3501.833613	344639.077661	44.753844
3501.820533	344632.443860	44.758849
3501.763648	344612.265332	44.763853
3502.222813	344589.845358	44.768858
3502.014119	344572.436336	44.773863
3501.719196	344544.362187	44.778868
3501.933560	344542.396617	44.783873
3501.922971	344498.514625	44.788877
3502.057901	344491.476388	44.793882
3502.118121	344480.381754	44.798887
3502.147992	344461.969396	44.803892
3501.926817	344446.850516	44.808897
3501.970233	344414.426758	44.813901
3501.883726	344395.066317	44.818906
3501.926019	344381.457346	44.823911
3501.827939	344360.827426	44.828916
3501.951083	344336.374708	44.833921
3501.892350	344321.637298	44.838925
3501.890017	344300.483938	44.843930
3502.182193	344287.649653	44.848935
3502.227575	344267.861813	44.853940
3501.807008	344239.934093	44.858945
3501.917227	344224.763545	44.863949
3501.819077	344208.633827	44.868954
3501.723190	344187.978037	44.873959
3501.704379	344170.132457	44.878964
3501.747878	344165.447515	44.883969
3501.559295	344139.212538	44.888973
3501.745365	344122.326641	44.893978
3501.805700	344111.003041	44.898983
3501.842844	344090.250215	44.903988
3501.936645	344092.218896	44.908993
3501.897764	344059.578782	44.913997
3501.882863	344044.376774	44.919002
3501.995972	344024.298574	44.924007
3501.723785	344010.051905	44.929012
3501.774318	344000.890961	44.934017
3501.371293	343984.096666	44.939021
3501.714019	343964.338658	44.944026
3501.668834	343962.616848	44.949031
3501.625780	343943.554498	44.954036
3501.667779	343933.149012	44.959041
3501.482762	343910.244052	44.964045
3501.703193	343890.911841	44.969050
3501.430028	343876.004203	44.974055
3501.747194	343868.123862	44.979060
3501.638104	343845.969812	44.984065
3501.670982	343832.006130	44.989069
3501.747380	343825.180271	44.994074
3501.403191	343810.181955	44.999079
3501.682403	343789.264151	45.004084
3501.697576	343791.524766	45.009089
3501.736701	343765.940564	45.014093
3502.210709	343747.840096	45.019098
3501.656758	343730.306393	45.024103
3502.118399	343699.444126	45.029108
3502.224542	343690.681257	45.034113
3501.818542	343665.013693	45.039117
3501.794797	343644.829440	45.044122
3502.009283	343626.921849	45.049127
3502.274678	343604.861924	45.054132
3502.334910	343596.360433	45.059137
3502.028197	343561.346075	45.064141
3502.251571	343546.589860	45.069146
3501.915353	343539.192507	45.074151
3502.350617	343506.147550	45.079156
3501.992828	343478.234869	45.084161
3501.976189	343461.278490	45.089165
3501.996407	343443.858700	45.094170
3501.893183	343431.772127	45.099175
3502.054448	343402.583596	45.104180
3501.623595	343383.021912	45.109185
3501.722372	343373.293923	45.114189
3501.967356	343346.711190	45.119194
3501.657738	343339.309654	45.124199
3502.063767	343316.769994	45.129204
3501.877736	343308.103346	45.134209
3502.112012	343284.624204	45.139213
3502.050762	343266.199962	45.144218
3502.048008	343251.122845	45.149223
3501.945999	343223.526121	45.154228
3502.046426	343209.627954	45.159233
3501.955962	343188.589332	45.164237
3502.002921	343165.647780	45.169242
3501.726069	343158.113976	45.174247
3501.698924	343140.370865	45.179252
3501.918831	343124.699669	45.184257
3501.856677	343095.876187	45.189261
3501.919079	343088.264149	45.194266
3501.698249	343057.634643	45.199271
3501.998341	343042.917128	45.204276
3501.572290	343036.423563	45.209281
3501.888104	343009.448157	45.214285
3501.916250	342992.738842	45.219290
3501.537785	342975.660546	45.224295
3501.950719	342954.136626	45.229300
3502.210536	342944.103768	45.234305
3501.858138	342922.851482	45.239309
3502.043327	342915.576267	45.244314
3501.903303	342893.375569	45.249319
3501.930690	342872.954073	45.254324
3502.028905	342846.037828	45.259329
3501.903483	342831.259308	45.264333
3501.933006	342806.565814	45.269338
3501.644828	342795.524854	45.274343
3502.046772	342780.282852	45.279348
3501.825282	342763.180024	45.284353
3501.912254	342743.054297	45.289357
3502.167939	342726.462004	45.294362
3502.225787	342709.646225	45.299367
3502.073088	342689.252646	45.304372
3502.203361	342667.111447	45.309377
3501.776093	342649.099805	45.314381
3502.009181	342629.739496	45.319386
3502.051362	342611.120826	45.324391
3501.961846	342577.724400	45.329396
3501.983274	342561.371895	45.334401
3501.642472	342546.575916	45.339405
3502.042171	342527.977847	45.344410
3501.663981	342518.196709	45.349415
3501.887210	342490.650498	45.354420
3501.868580	342475.931488	45.359425
3501.887693	342466.825881	45.364429
3502.209012	342428.839444	45.369434
3501.711946	342430.086514	45.374439
3501.649516	342408.788790	45.379444
3501.560001	342396.318323	45.384449
3501.589312	342387.745069	45.389453
3502.046674	342361.077683	45.394458
3502.095712	342344.441085	45.399463
3502.231931	342318.255894	45.404468
3502.020366	342297.871246	45.409473
3502.219830	342275.998726	45.414477
3502.059805	342258.047003	45.419482
3501.559853	342235.418786	45.424487
3501.635824	342204.157527	45.429492
3501.812817	342205.426847	45.434497
3501.901028	342178.460790	45.439501
3501.923062	342168.744407	45.444506
3501.844038	342156.221369	45.449511
3501.611496	342130.703665	45.454516
3501.656903	342134.409015	45.459521
3501.768041	342103.447316	45.464525
3501.991357	342087.063173	45.469530
3501.745866	342074.362594	45.474535
3501.645014	342053.172340	45.479540
3501.466748	342036.825238	45.484545
3501.749475	342028.059899	45.489549
3501.710534	342005.130951	45.494554
3501.935077	341996.756063	45.499559
3501.770267	341975.296019	45.504564
3501.614823	341966.497142	45.509569
3501.445080	341963.624975	45.514573
3501.751744	341929.657740	45.519578
3502.063744	341916.412665	45.524583
3501.870398	341906.678871	45.529588
3501.866951	341897.347784	45.534593
3501.523972	341879.932877	45.539597
3501.691152	341848.504545	45.544602
3501.762011	341844.908397	45.549607
3501.687559	341831.087750	45.554612
3501.594252	341810.506426	45.559617
3501.702734	341797.064132	45.564621
3501.808249	341782.579784	45.569626
3501.807794	341768.137346	45.574631
3501.915910	341750.194491	45.579636
3502.025148	341733.497382	45.584641
3501.463503	341712.175210	45.589645
3501.308733	341702.028522	45.594650
3501.515910	341693.503702	45.599655
3501.751286	341663.463088	45.604660
3501.645811	341658.495864	45.609665
3501.905581	341655.531407	45.614669
3501.979256	341627.117838	45.619674
3501.895819	341617.316007	45.624679
3501.658943	341597.850270	45.629684
3502.017651	341581.877086	45.634689
3502.189048	341558.584561	45.639693
3502.096957	341543.418900	45.644698
3502.137580	341517.451405	45.649703
3501.992589	341499.954646	45.654708
3501.758196	341476.394657	45.659713
3501.822799	341470.485557	45.664717
3501.847056	341446.732735	45.669722
3501.621288	341427.722868	45.674727
3501.846671	341415.050486	45.679732
3501.673713	341392.447121	45.684737
3501.461768	341381.546416	45.689741
3501.602331	341375.447488	45.694746
3501.518340	341356.288383	45.699751
3501.766249	341336.060522	45.704756
3502.025055	341332.409648	45.709761
3502.015921	341310.035012	45.714765
3501.711918	341301.869344	45.719770
3501.758492	341272.722311	45.724775
3501.675451	341265.615632	45.729780
3501.586494	341254.644894	45.734785
3501.587064	341239.896951	45.739789
3501.761143	341211.238576	45.744794
3501.559502	341213.736518	45.749799
3501.726210	341179.764911	45.754804
3501.983272	341173.495254	45.759809
3501.737697	341161.836887	45.764813
3501.917931	341126.973161	45.769818
3501.445533	341072.784258	45.774823
3501.647583	340961.150891	45.779828
3500.911995	340814.216732	45.784833
3500.348146	340614.187137	45.789837
3500.243217	340381.409881	45.794842
3499.571758	340112.331364	45.799847
3498.632883	339788.621101	45.804852
3497.946386	339440.635002	45.809857
3496.899178	339044.106732	45.814861
3495.809032	338602.672509	45.819866
3494.650991	338146.189072	45.824871
3493.939783	337629.666309	45.829876
3492.301584	337093.266724	45.834881
3490.409657	336526.356343	45.839885
3489.061376	335921.154907	45.844890
3487.508764	335297.384814	45.849895
3485.867479	334623.415058	45.854900
3484.013426	333934.689937	45.859905
3482.058033	333212.396331	45.864909
3480.803826	332460.171698	45.869914
3478.274305	331688.215811	45.874919
3476.536800	330878.172725	45.879924
3474.434037	330048.864261	45.884929
3472.360245	329183.465830	45.889933
3470.071702	328296.867939	45.894938
3467.441417	327409.413163	45.899943
3464.823521	326484.187648	45.904948
3462.661506	325540.910782	45.909953
3459.670782	324582.961249	45.914957
3457.397452	323591.323479	45.919962
3454.292813	322611.188528	45.924967
3451.990904	321600.148344	45.929972
3449.024506	320562.550750	45.934977
3445.550155	319527.983844	45.939981
3443.576238	318474.051679	45.944986
3440.557646	317403.413633	45.949991
3437.371932	316315.830452	45.954996
3434.441731	315223.804854	45.960001
3431.138001	314119.699527	45.965005
3428.244817	313002.679445	45.970010
3425.159841	311882.329103	45.975015
3422.025120	310734.325028	45.980020
3418.747379	309594.433408	45.985025
3415.749805	308446.073725	45.990029
3413.134562	307278.388859	45.995034
3409.478528	306111.882124	46.000039
3406.057494	304923.527212	46.005044
3402.834388	303727.300912	46.010049
3399.428462	302537.769260	46.015053
3396.410330	301331.021931	46.020058
3392.374906	300125.729440	46.025063
3389.220446	298912.154071	46.030068
3385.884507	297705.223769	46.035073
3382.132299	296487.387570	46.040077
3379.464302	295271.215098	46.045082
3375.366345	294038.439967	46.050087
3371.770667	292798.204737	46.055092
3368.666283	291568.940977	46.060097
3365.018852	290336.657184	46.065101
3361.724409	289093.042637	46.070106
3357.723506	287858.729495	46.075111
3354.129254	286607.706129	46.080116
3350.574040	285372.870119	46.085121
3347.220305	284130.801213	46.090125
3343.789889	282874.948921	46.095130
3340.017693	281630.177118	46.100135
3336.014201	280375.949074	46.105140
3332.572785	279130.370837	46.110145
3328.922895	277893.283153	46.115149
3325.251143	276634.741171	46.120154
3321.592951	275392.803649	46.125159
3318.055109	274135.093278	46.130164
3314.262349	272892.553828	46.135169
3310.557722	271643.795461	46.140173
3307.312854	270393.853132	46.145178
3303.770528	269143.990953	46.150183
3299.549731	267886.222214	46.155188
3296.011526	266645.875548	46.160193
3292.287450	265407.223048	46.165197
3288.795923	264147.001988	46.170202
3284.992113	262911.362651	46.175207
3281.260642	261666.225176	46.180212
3277.539954	260415.368167	46.185217
3273.939203	259168.681050	46.190221
3269.976325	257924.380438	46.195226
3266.148934	256691.480834	46.200231
3262.314630	255449.937718	46.205236
3259.000093	254224.575647	46.210241
3254.910532	253000.087728	46.215245
3251.339752	251756.281528	46.220250
3247.452153	250538.414895	46.225255
3243.834090	249315.480261	46.230260
3240.413800	248082.064551	46.235265
3236.177217	246866.034653	46.240269
3232.936308	245635.554720	46.245274
3228.832864	244419.209043	46.250279
3224.824075	243208.801426	46.255284
3221.417608	241988.590423	46.260289
3217.595114	240784.712538	46.265293
3214.068580	239575.944262	46.270298
3210.114908	238377.908853	46.275303
3206.499719	237176.989320	46.280308
3202.673867	235969.196514	46.285313
3199.118383	234776.308190	46.290317
3195.473483	233571.740428	46.295322
3191.439306	232384.982321	46.300327
3187.873558	231187.859572	46.305332
3184.196535	229994.929157	46.310337
3180.008679	228814.862223	46.315341
3176.603049	227612.259752	46.320346
3172.882018	226438.205599	46.325351
3169.114116	225265.788535	46.330356
3165.638124	224083.367811	46.335361
3161.383974	222920.170540	46.340365
3157.990725	221741.456956	46.345370
3153.944555	220577.007101	46.350375
3150.231542	219402.727051	46.355380
3146.486923	218241.341326	46.360385
3142.849390	217085.289878	46.365389
3139.326176	215933.145670	46.370394
3135.560300	214788.657558	46.375399
3131.533173	213625.494191	46.380404
3127.879121	212471.802014	46.385409
3123.593617	211326.209516	46.390413
3120.154049	210164.241232	46.395418
3116.351116	209034.679259	46.400423
3112.605820	207904.018414	46.405428
3108.788609	206766.803619	46.410433
3104.952793	205648.698590	46.415437
3101.265907	204527.902436	46.420442
3097.861944	203407.909213	46.425447
3094.254394	202289.737249	46.430452
3090.191945	201185.268205	46.435457
3086.392711	200071.419146	46.440461
3082.867782	198959.037746	46.445466
3079.116635	197847.667401	46.450471
3074.989893	196751.567415	46.455476
3071.684492	195650.433163	46.460481
3068.058417	194571.309474	46.465485
3064.262563	193457.791306	46.470490
3060.300388	192371.709806	46.475495
3056.229885	191289.321819	46.480500
3052.852970	190205.817184	46.485505
3049.250220	189133.053164	46.490509
3044.843907	188059.049422	46.495514
3041.740205	186991.550757	46.500519
3037.776935	185914.800409	46.505524
3034.075674	184855.285094	46.510529
3030.158335	183801.849519	46.515533
3026.287667	182735.279019	46.520538
3022.304236	181690.865413	46.525543
3018.594551	180641.914079	46.530548
3015.023974	179595.855972	46.535553
3010.827107	178571.779666	46.540557
3007.447046	177541.630306	46.545562
3003.474907	176512.909614	46.550567
2999.476905	175495.217680	46.555572
2995.517607	174478.576371	46.560577
2991.942049	173468.673566	46.565581
2988.078655	172463.207774	46.570586
2984.164031	171473.408253	46.575591
2980.289053	170474.933887	46.580596
2976.678234	169490.969120	46.585601
2972.773929	168510.614882	46.590605
2968.899069	167519.373304	46.595610
2965.275393	166558.121809	46.600615
2961.110195	165587.892285	46.605620
2957.539360	164633.456853	46.610625
2953.249404	163685.294852	46.615629
2949.514169	162731.306994	46.620634
2945.633707	161796.651679	46.625639
2941.467334	160854.048659	46.630644
2937.297815	159927.497266	46.635649
2933.628913	159012.807576	46.640653
2930.112386	158104.777019	46.645658
2925.982282	157199.044698	46.650663
2922.123032	156301.251129	46.655668
2917.955790	155404.091920	46.660673
2913.601890	154537.048663	46.665677
2909.951389	153660.440605	46.670682
2906.079385	152794.939701	46.675687
2901.841224	151944.742252	46.680692
2898.149323	151106.218838	46.685697
2894.458094	150273.460186	46.690701
2890.058947	149442.415219	46.695706
2886.021074	148625.273846	46.700711
2882.038421	147805.655124	46.705716
2877.923622	147009.738065	46.710721
2873.401846	146237.004588	46.715725
2869.802698	145459.252982	46.720730
2865.558654	144693.790795	46.725735
2861.203018	143945.726025	46.730740
2856.986067	143206.430408	46.735745
2852.984253	142486.376103	46.740749
2848.845612	141761.175205	46.745754
2844.459316	141060.439797	46.750759
2840.387930	140364.487673	46.755764
2836.427057	139692.753067	46.760769
2832.045066	139024.834033	46.765773
2828.583702	138367.671803	46.770778
2824.612863	137719.847341	46.775783
2820.509490	137084.393183	46.780788
2816.379245	136429.003748	46.785793
2812.385877	135745.945006	46.790797
2808.841103	135131.218739	46.795802
2804.868548	134527.635207	46.800807
2800.778187	133931.316640	46.805812
2797.423545	133339.916482	46.810817
2793.640301	132768.283147	46.815821
2790.086301	132177.934620	46.820826
2785.972280	131595.695300	46.825831
2782.391866	131021.979868	46.830836
2778.968635	130459.823175	46.835841
2774.341466	129900.952245	46.840845
2771.262192	129341.822351	46.845850
2767.737519	128791.838441	46.850855
2763.726633	128240.589113	46.855860
2760.312050	127691.352993	46.860865
2756.662827	127160.680064	46.865869
2753.291333	126621.944915	46.870874
2749.509283	126092.260371	46.875879
2745.892181	125552.483677	46.880884
2742.610654	125017.482326	46.885889
2738.950789	124484.454717	46.890893
2735.360483	123956.637888	46.895898
2731.928461	123422.469731	46.900903
2728.527860	122901.149075	46.905908
2724.987228	122362.102938	46.910913
2721.230761	121837.099951	46.915917
2717.853257	121312.528297	46.920922
2713.899112	120794.946250	46.925927
2710.377998	120268.656042	46.930932
2707.162708	119739.642136	46.935937
2703.394500	119229.275428	46.940941
2700.359241	118705.181933	46.945946
2696.582426	118194.932157	46.950951
2692.780780	117679.784633	46.955956
2689.545300	117150.072368	46.960961
2685.610691	116639.753793	46.965965
2682.093626	116119.446196	46.970970
2678.574493	115612.090711	46.975975
2675.051782	115101.602041	46.980980
2671.811143	114592.373523	46.985985
2667.863019	114087.242013	46.990989
2664.347493	113578.413728	46.995994
2661.346645	113078.806958	47.000999
2657.492247	112562.912731	47.006004
2654.421771	112051.709951	47.011009
2650.478644	111558.145006	47.016013
2646.796333	111046.670414	47.021018
2642.938012	110544.422693	47.026023
2638.915868	110049.619675	47.031028
2635.537079	109546.205483	47.036033
2631.341212	109057.113720	47.041037
2627.840631	108570.971774	47.046042
2624.074457	108091.806524	47.051047
2620.135145	107623.112045	47.056052
2616.653728	107144.195335	47.061057
2612.609358	106687.136581	47.066061
2609.161332	106222.440072	47.071066
2605.408448	105761.699964	47.076071
2601.489308	105304.640315	47.081076
2597.944178	104857.481941	47.086081
2593.635446	104423.032801	47.091085
2590.036961	103975.246204	47.096090
2586.407769	103542.139156	47.101095
2582.628506	103109.874616	47.106100
2579.399635	102683.135573	47.111105
2575.686578	102275.390982	47.116109
2571.896396	101841.517780	47.121114
2568.040424	101432.191661	47.126119
2564.370165	101019.562526	47.131124
2560.945336	100597.863549	47.136129
2557.262440	100202.100349	47.141133
2553.722034	99781.840786	47.146138
2550.279674	99389.075047	47.151143
2547.111883	98984.451582	47.156148
2543.826188	98567.993805	47.161153
2540.275301	98167.456434	47.166157
2536.556771	97747.429217	47.171162
2533.169446	97357.577555	47.176167
2529.490042	96947.645656	47.181172
2526.252979	96533.011657	47.186177
2522.460139	96131.127101	47.191181
2519.413427	95719.969012	47.196186
2515.853315	95308.413333	47.201191
2512.205391	94915.569960	47.206196
2508.917835	94497.527035	47.211201
2505.318204	94088.179412	47.216205
2502.200448	93668.698047	47.221210
2498.145199	93266.827910	47.226215
2494.978406	92853.693475	47.231220
2491.785074	92440.390865	47.236225
2487.868261	92047.066917	47.241229
2484.916499	91631.031204	47.246234
2481.263971	91209.964222	47.251239
2477.770874	90789.843972	47.256244
2474.370052	90373.107716	47.261249
2470.524048	89958.581102	47.266253
2467.283764	89542.847886	47.271258
2463.983119	89126.507300	47.276263
2460.699832	88709.394831	47.281268
2456.888813	88278.356711	47.286273
2453.493931	87870.001815	47.291277
2449.922174	87452.088080	47.296282
2446.590965	87032.859711	47.301287
2443.430659	86607.601614	47.306292
2439.702108	86175.806600	47.311297
2435.972025	85759.796532	47.316301
2432.570305	85330.300764	47.321306
2429.048542	84903.815401	47.326311
2425.530219	84486.621991	47.331316
2422.063455	84056.634503	47.336321
2418.483875	83633.429029	47.341325
2415.075226	83218.853850	47.346330
2411.676551	82795.289696	47.351335
2408.180951	82363.210913	47.356340
2404.900829	81933.023236	47.361345
2401.445416	81509.703106	47.366349
2398.153843	81082.273854	47.371354
2394.624022	80647.597443	47.376359
2391.097701	80213.854456	47.381364
2387.624557	79777.074345	47.386369
2383.826279	79346.880050	47.391373
2380.098291	78903.282086	47.396378
2377.054254	78468.373670	47.401383
2373.479472	78042.902265	47.406388
2370.130587	77608.385110	47.411393
2366.416755	77172.560044	47.416397
2363.017548	76735.765887	47.421402
2359.550796	76299.370247	47.426407
2356.214749	75862.212019	47.431412
2352.764376	75421.484765	47.436417
2349.278852	74987.030813	47.441421
2345.608236	74543.177454	47.446426
2342.400086	74103.856376	47.451431
2338.873903	73667.880905	47.456436
2335.341954	73221.031102	47.461441
2331.432423	72779.644224	47.466445
2327.796358	72341.498173	47.471450
2324.478911	71897.735572	47.476455
2321.093960	71450.410301	47.481460
2317.469059	71009.402379	47.486465
2313.979021	70577.909943	47.491469
2310.523449	70134.820824	47.496474
2307.402517	69686.513345	47.501479
2303.861443	69255.190439	47.506484
2300.469554	68789.115071	47.511489
2296.902223	68354.231002	47.516493
2293.349866	67907.735455	47.521498
2289.810899	67457.125938	47.526503
2286.108239	67022.037951	47.531508
2282.829667	66570.032476	47.536513
2278.868771	66127.376638	47.541517
2275.564207	65674.312092	47.546522
2272.162330	65234.003173	47.551527
2268.578814	64786.196280	47.556532
2264.959181	64335.369153	47.561537
2261.468676	63893.758289	47.566541
2258.377742	63443.417107	47.571546
2254.629266	62990.279653	47.576551
2251.290638	62539.910848	47.581556
2247.877617	62094.175592	47.586561
2244.064255	61644.721972	47.591565
2241.123585	61192.062861	47.596570
2237.355850	60742.605911	47.601575
2233.732862	60287.994505	47.606580
2230.127703	59836.853563	47.611585
2226.756792	59388.679656	47.616589
2223.204243	58930.922448	47.621594
2219.983342	58479.277313	47.626599
2216.369097	58026.045703	47.631604
2212.996597	57571.147931	47.636609
2208.821567	57114.397656	47.641613
2205.479986	56665.508295	47.646618
2201.737752	56213.688611	47.651623
2198.620275	55765.142941	47.656628
2195.315440	55307.232223	47.661633
2192.193014	54870.968256	47.666637
2188.527959	54412.147499	47.671642
2185.155961	53945.994211	47.676647
2181.416215	53496.941251	47.681652
2178.311480	53033.124467	47.686657
2174.591718	52575.991142	47.691661
2171.107016	52107.950719	47.696666
2167.605734	51647.217403	47.701671
2164.199631	51190.703157	47.706676
2160.536936	50720.466464	47.711681
2157.063883	50262.566391	47.716685
2153.847293	49791.600479	47.721690
2149.969730	49332.329308	47.726695
2146.114222	48868.947420	47.731700
2142.794763	48404.045369	47.736705
2139.153496	47950.682923	47.741709
2135.745265	47489.073451	47.746714
2132.418920	47027.923619	47.751719
2128.743330	46567.839607	47.756724
2125.404596	46104.008799	47.761729
2121.756581	45646.634681	47.766733
2118.348456	45185.452846	47.771738
2115.409770	44722.875706	47.776743
2111.433547	44270.286306	47.781748
2107.997377	43794.139868	47.786753
2104.615719	43331.184973	47.791757
2100.944245	42872.190994	47.796762
2097.601833	42402.432714	47.801767
2093.539009	41940.247078	47.806772
2090.566913	41472.987349	47.811777
2087.188939	41008.495495	47.816781
2083.380024	40540.231918	47.821786
2079.982872	40072.801958	47.826791
2076.334230	39615.432335	47.831796
2072.821187	39138.504873	47.836801
2069.121386	38677.251206	47.841805
2065.878417	38224.019516	47.846810
2062.626345	37754.480536	47.851815
2058.721119	37282.904378	47.856820
2055.601605	36808.198784	47.861825
2051.947753	36345.327133	47.866829
2048.067544	35878.266252	47.871834
2044.905084	35417.969009	47.876839
2040.976638	34945.535369	47.881844
2037.624051	34478.822539	47.886849
2034.130846	34027.310015	47.891853
2030.370994	33557.435641	47.896858
2026.655839	33086.170411	47.901863
2023.389010	32633.682868	47.906868
2020.214680	32175.904855	47.911873
2016.787334	31715.362273	47.916877
2013.182237	31248.684641	47.921882
2009.870291	30787.815103	47.926887
2006.219658	30315.981450	47.931892
2002.836798	29844.009173	47.936897
1999.305050	29377.863007	47.941901
1995.900190	28921.156099	47.946906
1992.558839	28444.431433	47.951911
1988.968767	27975.474668	47.956916
1985.487061	27511.454322	47.961921
1981.610669	27048.621189	47.966925
1978.251373	26581.048319	47.971930
1974.864834	26103.187985	47.976935
1971.357147	25649.263359	47.981940
1968.024539	25166.329045	47.986945
1963.843485	24700.517935	47.991949
1960.440919	24233.177334	47.996954
1957.097541	23762.664420	48.001959
1953.393368	23305.256620	48.006964
1950.061627	22831.190815	48.011969
1946.922399	22371.068516	48.016973
1943.129940	21906.795260	48.021978
1939.276567	21436.030397	48.026983
1935.684814	20978.563780	48.031988
1932.401709	20504.330812	48.036993
1928.578524	20043.710470	48.041997
1924.878760	19585.114973	48.047002
1921.500534	19122.008479	48.052007
1917.749608	18675.191660	48.057012
1914.493663	18211.726753	48.062017
1910.701782	17757.571458	48.067021
1907.008943	17304.006727	48.072026
1903.833016	16848.693913	48.077031
1899.927765	16404.176435	48.082036
1896.370628	15939.555792	48.087041
1892.912886	15498.140209	48.092045
1889.317879	15048.121744	48.097050
1885.916707	14599.350186	48.102055
1881.863497	14164.358814	48.107060
1878.138381	13718.982843	48.112065
1874.731062	13280.320882	48.117069
1871.210716	12833.034259	48.122074
1867.443789	12403.389096	48.127079
1863.624696	11981.799695	48.132084
1859.683919	11556.835561	48.137089
1854.977334	11161.969132	48.142093
1850.984269	10758.494135	48.147098
1846.985031	10364.506261	48.152103
1842.823501	9987.429979	48.157108
1838.718681	9612.555590	48.162113
1834.766528	9258.508469	48.167117
1830.964373	8898.617552	48.172122
1827.411407	8557.565622	48.177127
1822.927608	8218.044840	48.182132
1819.038584	7880.624789	48.187137
1814.922560	7555.551783	48.192141
1810.891520	7256.082090	48.197146
1806.746709	6958.670017	48.202151
1802.313630	6687.256278	48.207156
1798.513798	6402.683669	48.212161
1794.362786	6141.114661	48.217165
1790.348220	5876.983728	48.222170
1786.920182	5648.070443	48.227175
1782.927343	5398.279057	48.232180
1779.528026	5171.832537	48.237185
1775.739513	4935.534858	48.242189
1772.344832	4710.441463	48.247194
1768.508514	4477.973584	48.252199
1764.865326	4260.038197	48.257204
1761.740800	4045.616301	48.262209
1757.986858	3832.921390	48.267213
1754.630352	3626.742596	48.272218
1751.289769	3413.896519	48.277223
1746.954309	3196.524705	48.282228
1743.578595	2986.356609	48.287233
1740.570929	2788.676486	48.292237
1737.070288	2591.774539	48.297242
1733.775708	2389.074507	48.302247
1730.241874	2197.440801	48.307252
1726.363676	1990.754447	48.312257
1723.121127	1794.539320	48.317261
1719.457530	1591.029318	48.322266
1715.737768	1400.173455	48.327271
1712.226731	1210.691918	48.332276
1708.688778	1023.320556	48.337281
1705.117066	837.487714	48.342285
1701.661544	660.060771	48.347290
1697.773200	470.908423	48.352295
1693.658289	307.754995	48.357300
1689.524064	137.171352	48.362305
1683.723742	42.815129	48.367309
1673.153820	93.678002	48.372314
1666.784657	83.026982	48.377319
1661.795453	84.379400	48.382324
1659.087492	78.562150	48.387329
1656.581415	87.617671	48.392333
1653.700799	90.318667	48.397338
1651.817696	84.619802	48.402343
1648.630440	96.875448	48.407348
1646.006513	90.494631	48.412353
1642.713295	91.111693	48.417357
1638.476889	96.741328	48.422362
1635.299735	90.066975	48.427367
1631.593824	99.236482	48.432372
1628.439773	94.510537	48.437377
1625.608682	90.942861	48.442381
1622.251089	95.711229	48.447386
1619.103536	89.937090	48.452391
1615.410835	93.134636	48.457396
1612.181912	92.675525	48.462401
1608.480808	89.607089	48.467405
1604.675353	97.153292	48.472410
1601.545256	90.686751	48.477415
1598.202368	92.308113	48.482420
1594.585569	88.252137	48.487425
1591.033671	88.817717	48.492429
1587.577023	90.301764	48.497434
1584.205845	81.594887	48.502439
1581.050686	91.763820	48.507444
1577.430228	81.811281	48.512449
1573.903302	89.589373	48.517453
1570.428949	92.515661	48.522458
1567.160303	77.924168	48.527463
1563.896118	89.056014	48.532468
1560.376047	86.611129	48.537473
1557.370219	87.259395	48.542477
1553.198046	90.550555	48.547482
1549.777942	79.364634	48.552487
1545.712330	83.547188	48.557492
1542.894780	91.872921	48.562497
1539.671123	87.043929	48.567501
1536.150457	90.072338	48.572506
1532.584326	82.702421	48.577511
1529.220690	91.369408	48.582516
1525.654492	84.372818	48.587521
1521.968734	77.470770	48.592525
1518.570650	89.335287	48.597530
1515.226879	80.744378	48.602535
1511.343016	92.728799	48.607540
1508.407238	79.891980	48.612545
1504.767932	83.868983	48.617549
1501.038469	88.296609	48.622554
1497.863508	79.761684	48.627559
1494.497252	81.858081	48.632564
1490.806108	76.057843	48.637569
1487.364443	82.025685	48.642573
1483.625576	78.273459	48.647578
1480.256306	82.116685	48.652583
1476.648488	83.674889	48.657588
1473.458759	79.539805	48.662593
1470.150755	80.298385	48.667597
1466.089601	84.761821	48.672602
1462.928353	77.506065	48.677607
1458.999274	87.823927	48.682612
1456.168328	80.871095	48.687617
1452.609863	85.983940	48.692621
1449.030838	86.167784	48.697626
1445.698695	79.466967	48.702631
1441.735570	82.159297	48.707636
1438.409504	89.001313	48.712641
1435.294372	89.612819	48.717645
1431.386850	84.630862	48.722650
1428.122531	87.834509	48.727655
1424.690125	83.000062	48.732660
1420.920076	78.319408	48.737665
1417.612256	79.549354	48.742669
1414.036862	85.345030	48.747674
1410.449844	74.390758	48.752679
1407.090360	83.939769	48.757684
1403.909829	80.404363	48.762689
1400.353587	82.460737	48.767693
1395.976150	85.495963	48.772698
1393.174504	79.070080	48.777703
1389.593805	77.349649	48.782708
1386.060929	81.920686	48.787713
1382.501932	82.341861	48.792717
1379.303984	82.055118	48.797722
1375.761366	81.015282	48.802727
1372.080874	85.811774	48.807732
1368.700482	93.146295	48.812737
1365.230055	84.397956	48.817741
1361.352233	84.811812	48.822746
1358.485990	77.408917	48.827751
1354.682713	80.386415	48.832756
1351.224062	85.657733	48.837761
1347.850941	85.610226	48.842765
1343.713833	88.557432	48.847770
1340.194798	87.738551	48.852775
1337.227977	83.261909	48.857780
1333.840020	77.987131	48.862785
1330.706043	78.512996	48.867789
1327.283452	84.069762	48.872794
1323.688513	76.922661	48.877799
1319.595663	82.036434	48.882804
1315.988264	72.050281	48.887809
1312.651572	77.938518	48.892813
1308.968832	77.869607	48.897818
1305.430476	75.927464	48.902823
1301.923863	77.463603	48.907828
1298.930472	83.260442	48.912833
1295.673220	77.436990	48.917837
1291.794588	86.867497	48.922842
1288.470035	80.912153	48.927847
1284.578966	91.777751	48.932852
1280.894847	84.274383	48.937857
1277.665983	85.634418	48.942861
1274.006061	88.194149	48.947866
1271.095086	88.213919	48.952871
1267.207671	85.538352	48.957876
1263.639821	84.977009	48.962881
1259.588240	84.987661	48.967885
1256.685526	90.887446	48.972890
1253.426939	81.331051	48.977895
1249.754730	76.575084	48.982900
1246.308778	81.575517	48.987905
1242.775757	76.323333	48.992909
1239.020677	80.783437	48.997914
1235.810553	75.740417	49.002919
1232.483101	83.025570	49.007924
1228.970746	90.807734	49.012929
1225.638000	73.559308	49.017933
1221.687196	84.747405	49.022938
1218.316707	81.586433	49.027943
1214.855741	88.373526	49.032948
1211.079648	79.432356	49.037953
1207.802610	80.230431	49.042957
1204.286272	83.473321	49.047962
1200.707819	67.114185	49.052967
1197.244901	78.406668	49.057972
1193.940341	78.671202	49.062977
1190.582546	73.888451	49.067981
1186.336262	73.189116	49.072986
1183.375844	71.185503	49.077991
1179.521787	74.117138	49.082996
1175.923298	76.300327	49.088001
1172.727994	75.079906	49.093005
1168.909931	80.119282	49.098010
1165.757978	63.522932	49.103015
1162.726929	79.281752	49.108020
1159.403579	76.888554	49.113025
1155.667795	79.029842	49.118029
1151.609505	79.981166	49.123034
1147.978611	75.149184	49.128039
1144.447303	77.666761	49.133044
1140.904245	76.231560	49.138049
1138.041816	81.229753	49.143053
1134.514255	77.033407	49.148058
1130.871267	68.137977	49.153063
1127.254460	73.794583	49.158068
1123.586680	74.678798	49.163073
1120.521696	78.145660	49.168077
1116.656523	75.121813	49.173082
1113.140675	76.681554	49.178087
1110.008586	76.818012	49.183092
1106.371411	73.122777	49.188097
1102.540199	74.231745	49.193101
1099.020328	81.746167	49.198106
1095.716145	78.011754	49.203111
1091.997954	79.637794	49.208116
1088.792984	81.459187	49.213121
1085.654768	73.500734	49.218125
1081.587801	81.271155	49.223130
1078.345807	80.371217	49.228135
1074.368023	87.963248	49.233140
1071.266219	85.162259	49.238145
1067.689523	75.190357	49.243149
1063.992315	78.094425	49.248154
1060.762039	73.276025	49.253159
1057.218139	77.763381	49.258164
1053.161837	79.138341	49.263169
1050.092052	71.957000	49.268173
1046.573862	78.373363	49.273178
1043.219330	78.873476	49.278183
1039.701940	67.566770	49.283188
1036.141804	75.555685	49.288193
1033.131451	74.056559	49.293197
1029.211411	77.330666	49.298202
1025.993499	73.019701	49.303207
1022.300500	76.362869	49.308212
1018.897240	80.394911	49.313217
1015.580967	75.488666	49.318221
1011.523358	72.548573	49.323226
1007.861889	79.243500	49.328231
1004.362732	83.091160	49.333236
1000.971417	82.787100	49.338241
997.710336	75.303357	49.343245
994.469131	73.811697	49.348250
990.922067	75.344672	49.353255
987.222682	78.543308	49.358260
983.434485	73.080956	49.363265
980.279626	74.584518	49.368269
976.707044	76.855440	49.373274
973.386944	65.935644	49.378279
969.640791	79.799999	49.383284
966.091667	72.126988	49.388289
962.592694	66.733513	49.393293
958.823581	80.000343	49.398298
955.494849	74.884080	49.403303
951.863050	74.652261	49.408308
948.185532	70.858929	49.413313
945.051736	73.963201	49.418317
941.920240	78.592008	49.423322
938.528280	76.098790	49.428327
934.615438	72.123797	49.433332
930.686762	75.867483	49.438337
927.297016	68.036796	49.443341
924.432906	71.725497	49.448346
920.922061	60.977772	49.453351
917.133711	74.260248	49.458356
913.712348	71.594445	49.463361
910.267184	74.038524	49.468365
906.060354	75.569807	49.473370
903.129223	79.635930	49.478375
899.981008	77.272450	49.483380
896.383294	69.417195	49.488385
892.547332	71.700651	49.493389
888.814104	75.651193	49.498394
885.438921	66.369283	49.503399
881.711593	69.546969	49.508404
878.538783	70.575619	49.513409
875.225397	68.000578	49.518413
871.831998	75.818017	49.523418
868.426132	73.833162	49.528423
864.690637	76.768518	49.533428
860.840536	79.721715	49.538433
858.014777	62.827899	49.543437
853.987264	75.799601	49.548442
850.123495	68.210393	49.553447
846.801926	75.203587	49.558452
843.565900	65.241980	49.563457
840.353544	67.849136	49.568461
836.759540	74.520916	49.573466
833.363650	67.121464	49.578471
829.572909	67.430082	49.583476
825.991140	74.973132	49.588481
822.611299	68.536105	49.593485
818.882532	74.577147	49.598490
815.833627	69.622987	49.603495
812.076046	76.548018	49.608500
808.461479	67.297060	49.613505
804.759136	70.486682	49.618509
801.045375	79.445464	49.623514
798.243460	66.034319	49.628519
794.874358	63.154760	49.633524
790.958446	70.322730	49.638529
787.850600	72.923114	49.643533
783.868595	71.910622	49.648538
780.533876	65.052137	49.653543
776.967074	62.060991	49.658548
773.251524	71.766675	49.663553
769.938334	69.299184	49.668557
766.242268	72.769400	49.673562
762.545240	70.991232	49.678567
759.667337	73.891172	49.683572
756.423910	67.170336	49.688577
752.961052	64.438252	49.693581
748.814642	70.901808	49.698586
745.505134	72.423138	49.703591
742.003422	63.926564	49.708596
738.069050	67.747083	49.713601
734.968629	61.886656	49.718605
731.299790	75.846539	49.723610
728.167894	75.100342	49.728615
724.341160	71.010743	49.733620
720.671755	68.007103	49.738625
717.708853	64.548643	49.743629
714.004979	65.805509	49.748634
710.885958	60.495297	49.753639
707.300069	64.868995	49.758644
703.420068	57.415222	49.763649
699.988257	62.372360	49.768653
696.013272	60.311614	49.773658
692.392268	64.950201	49.778663
689.105482	63.111345	49.783668
685.853666	69.252151	49.788673
682.691912	56.153312	49.793677
678.954165	62.632347	49.798682
675.628235	61.938508	49.803687
672.476151	63.571377	49.808692
668.116293	64.218541	49.813697
665.003471	60.641062	49.818701
661.228042	62.130530	49.823706
657.763433	58.712218	49.828711
654.489754	62.977208	49.833716
651.196658	59.117755	49.838721
647.529231	58.745994	49.843725
643.590868	65.496701	49.848730
640.309262	62.660490	49.853735
636.931780	59.573457	49.858740
633.323234	58.009319	49.863745
629.817851	52.670685	49.868749
625.943104	62.470756	49.873754
622.734787	62.555859	49.878759
619.206162	67.335091	49.883764
615.621093	64.160157	49.888769
612.232929	52.127940	49.893773
608.555117	69.464849	49.898778
605.088658	66.872548	49.903783
602.021706	65.935927	49.908788
598.520412	68.575431	49.913793
595.471583	62.963252	49.918797
591.331327	58.359354	49.923802
587.727290	54.820394	49.928807
584.418201	60.046329	49.933812
580.850733	62.895446	49.938817
577.789053	61.407530	49.943821
573.760184	56.254800	49.948826
570.386062	59.902700	49.953831
566.720736	68.221216	49.958836
563.046104	63.497381	49.963841
559.860617	59.067549	49.968845
555.890773	67.847912	49.973850
552.964250	59.094161	49.978855
549.548393	56.712286	49.983860
545.487158	67.620205	49.988865
542.416670	61.438783	49.993869
538.594754	63.093688	49.998874
535.566163	52.802473	50.003879
531.869293	59.357410	50.008884
528.118224	61.048741	50.013889
524.835187	54.837140	50.018893
521.340948	60.506344	50.023898
518.146319	63.904850	50.028903
514.622150	55.797789	50.033908
510.937058	57.194122	50.038913
507.432590	57.189305	50.043917
503.692280	67.287986	50.048922
500.055295	54.699760	50.053927
496.592826	58.054545	50.058932
492.721359	60.745359	50.063937
489.620525	50.130054	50.068941
485.875842	60.422397	50.073946
482.888194	55.338537	50.078951
479.360117	58.893357	50.083956
475.606193	61.005907	50.088961
472.656099	56.276860	50.093965
468.367016	56.713726	50.098970
465.171188	58.011751	50.103975
461.425150	61.214538	50.108980
458.150296	57.621188	50.113985
455.106228	55.228903	50.118989
450.939727	58.592058	50.123994
447.603445	48.538585	50.128999
444.252557	49.348238	50.134004
440.692782	56.938502	50.139009
437.363559	54.584284	50.144013
433.909223	71.155596	50.149018
430.262377	63.716199	50.154023
426.573713	63.414211	50.159028
423.344518	66.697888	50.164033
419.978354	63.688217	50.169037
416.065486	62.491018	50.174042
412.549997	61.956435	50.179047
409.258021	63.339035	50.184052
405.674696	66.718973	50.189057
402.159422	62.694837	50.194061
398.499380	69.743914	50.199066
394.705567	60.948048	50.204071
391.810647	55.201216	50.209076
387.967944	72.336011	50.214081
384.993210	60.733009	50.219085
381.030652	66.965503	50.224090
377.501706	59.412854	50.229095
374.104922	56.347849	50.234100
370.413936	57.450897	50.239105
367.451600	59.573097	50.244109
363.682909	63.548193	50.249114
360.078155	58.459187	50.254119
356.489619	62.697293	50.259124
352.770318	69.812545	50.264129
349.244827	61.310264	50.269133
345.816188	70.158243	50.274138
342.811781	60.401121	50.279143
339.533129	61.310270	50.284148
335.903704	66.978392	50.289153
332.181652	61.287574	50.294157
328.487246	67.816838	50.299162
325.062812	62.763038	50.304167
321.424783	56.787069	50.309172
317.631160	59.418332	50.314177
314.414253	55.683110	50.319181
311.141307	64.589104	50.324186
307.585677	66.389239	50.329191
304.377296	67.388688	50.334196
300.496357	59.969946	50.339201
296.998366	58.217810	50.344205
292.985205	55.761292	50.349210
290.060932	67.134441	50.354215
286.816000	56.867466	50.359220
282.518703	59.178527	50.364225
279.625570	55.560578	50.369229
276.610430	58.380685	50.374234
272.976044	62.594302	50.379239
269.488010	62.083937	50.384244
265.357446	60.069632	50.389249
262.184406	60.845292	50.394253
258.341189	63.104645	50.399258
254.705243	60.829844	50.404263
251.286607	53.006957	50.409268
247.565547	51.583778	50.414273
244.512502	58.725018	50.419277
240.999115	54.830329	50.424282
237.880774	63.667965	50.429287
234.301292	65.465495	50.434292
230.407343	65.002514	50.439297
226.845958	55.113841	50.444301
223.172377	61.744271	50.449306
220.027288	60.750264	50.454311
216.442108	68.385632	50.459316
212.994729	59.792128	50.464321
209.465356	55.137492	50.469325
205.690495	59.575460	50.474330
202.222052	56.828514	50.479335
199.338860	54.385909	50.484340
195.609867	57.105199	50.489345
192.372115	55.375836	50.494349
188.140214	69.372768	50.499354
184.562978	55.655384	50.504359
181.584437	54.486761	50.509364
178.054423	62.123032	50.514369
174.545214	61.938671	50.519373
170.861082	63.360208	50.524378
167.152035	67.803754	50.529383
164.218659	58.304522	50.534388
160.326225	62.137561	50.539393
156.842029	52.657655	50.544397
153.207107	59.013161	50.549402
149.738773	56.649009	50.554407
146.810110	57.975076	50.559412
142.668596	71.957940	50.564417
139.660753	56.095541	50.569421
135.960366	64.353108	50.574426
132.387217	55.333131	50.579431
128.727625	55.368337	50.584436
125.080115	56.024902	50.589441
122.078987	47.643512	50.594445
118.508462	56.608498	50.599450
115.030176	50.968358	50.604455
111.590024	59.410028	50.609460
107.495539	66.571059	50.614465
104.285478	56.140513	50.619469
100.665772	59.333167	50.624474
97.573856	54.139058	50.629479
94.064884	58.554623	50.634484
90.206267	57.374343	50.639489
86.942908	61.330903	50.644493
83.290894	63.367529	50.649498
80.009334	67.532562	50.654503
76.229268	70.522405	50.659508
72.612882	66.846253	50.664513
69.535094	68.581512	50.669517
65.731932	66.965507	50.674522
62.335758	65.488611	50.679527
58.922330	58.360955	50.684532
55.283226	66.064840	50.689537
51.625880	58.114649	50.694541
48.434195	66.362622	50.699546
44.890164	61.707133	50.704551
41.253216	61.131406	50.709556
37.696053	66.509905	50.714561
34.679793	58.564304	50.719565
30.942305	69.225706	50.724570
27.495626	69.094904	50.729575
23.704370	71.681548	50.734580
19.959899	72.745518	50.739585
16.884547	62.515470	50.744589
13.123909	60.193688	50.749594
9.685952	67.676440	50.754599
6.197088	58.434566	50.759604
2.576780	66.958079	50.764609