Fri Aug 26 11:31:52 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.502815	105.484655	0.000000
1.748313	101.564687	0.005005
1.673387	104.948886	0.010010
1.384919	92.918174	0.015014
1.474809	101.648606	0.020019
1.279735	97.091739	0.025024
1.327675	89.485232	0.030029
1.220265	80.090141	0.035034
0.803165	64.669053	0.040038
0.808227	62.713195	0.045043
0.446620	56.464403	0.050048
0.286223	42.097991	0.055053
-0.540006	42.628486	0.060058
-0.380175	29.272049	0.065062
-1.089693	19.129205	0.070067
-1.469981	19.191648	0.075072
-1.211850	8.847532	0.080077
-1.573673	2.823411	0.085082
-1.741920	0.306106	0.090086
-2.011424	-2.094196	0.095091
-2.312725	-7.722790	0.100096
-2.569454	-15.965162	0.105101
-3.252820	-12.002216	0.110106
-3.973470	-29.413344	0.115110
-3.730402	-22.703079	0.120115
-3.891813	-26.467918	0.125120
-3.572026	-35.910480	0.130125
-4.594408	-24.482349	0.135130
-5.132902	-28.824368	0.140134
-5.201796	-25.507570	0.145139
-5.196037	-24.571961	0.150144
-5.419480	-32.772053	0.155149
-6.262152	-20.081136	0.160154
-6.253554	-21.613607	0.165158
-6.259265	-19.369628	0.170163
-6.706818	-21.182242	0.175168
-6.386181	-20.555076	0.180173
-7.056552	-13.854442	0.185178
-7.396510	-25.035527	0.190182
-8.207671	-14.953188	0.195187
-7.855632	-19.522445	0.200192
-8.018405	-23.767946	0.205197
-8.078614	-9.547430	0.210202
-8.425259	-10.350736	0.215206
-9.433850	-20.029390	0.220211
-9.516126	-21.427494	0.225216
-9.765358	-24.726259	0.230221
-9.964437	-13.325072	0.235226
-9.718740	-18.099227	0.240230
-9.972349	-17.999563	0.245235
-9.949111	-17.756348	0.250240
-9.967105	-26.712904	0.255245
-10.962180	-13.507890	0.260250
-10.791908	-20.563940	0.265254
-11.345247	-25.805286	0.270259
-11.825672	-24.816124	0.275264
-12.335398	-20.048178	0.280269
-12.671316	-17.015658	0.285274
-12.500065	-26.033316	0.290278
-12.771561	-26.560430	0.295283
-13.047258	-13.973605	0.300288
-12.683721	-26.564478	0.305293
-13.066128	-17.934570	0.310298
-13.134178	-21.438709	0.315302
-13.728873	-17.840734	0.320307
-14.498671	-15.689752	0.325312
-14.439971	-26.619706	0.330317
-14.635549	-15.785357	0.335322
-14.507443	-21.610513	0.340326
-15.559307	-26.489511	0.345331
-15.790870	-19.496546	0.350336
-15.859357	-18.482939	0.355341
-15.966055	-12.363595	0.360346
-15.975270	-15.962315	0.365350
-15.932287	-25.656002	0.370355
-16.425670	-22.927985	0.375360
-17.078470	-30.953662	0.380365
-17.805239	-24.671342	0.385370
-17.441288	-25.686522	0.390374
-17.162547	-20.541485	0.395379
-17.530772	-19.269246	0.400384
-17.574211	-22.951217	0.405389
-18.593253	-24.051613	0.410394
-18.508077	-31.398119	0.415398
-18.847422	-24.919866	0.420403
-18.855396	-25.215937	0.425408
-19.387977	-20.529851	0.430413
-20.077315	-19.492343	0.435418
-20.180699	-24.066618	0.440422
-20.264475	-30.592745	0.445427
-20.238327	-17.540410	0.450432
-20.059276	-27.821573	0.455437
-21.026582	-23.577148	0.460442
-21.388647	-22.188814	0.465446
-21.918675	-30.091243	0.470451
-21.945664	-25.550315	0.475456
-21.791868	-31.154849	0.480461
-21.544853	-16.966357	0.485466
-22.149033	-22.187132	0.490470
-22.638860	-20.541633	0.495475
-23.373012	-22.793659	0.500480
-23.163177	-28.691647	0.505485
-23.435446	-24.001801	0.510490
-23.377709	-30.869489	0.515494
-23.877820	-27.922134	0.520499
-24.577806	-14.551103	0.525504
-24.265329	-15.865142	0.530509
-24.558250	-12.269861	0.535514
-24.354352	-20.428930	0.540518
-24.773831	-16.415326	0.545523
-25.480905	-21.411281	0.550528
-25.662268	-21.639228	0.555533
-25.935685	-9.078065	0.560538
-25.899349	-17.046536	0.565542
-26.620755	-19.281566	0.570547
-27.617976	-18.101212	0.575552
-27.389054	-31.987194	0.580557
-27.126627	-18.870413	0.585562
-27.562416	-22.696932	0.590566
-27.565376	-21.459419	0.595571
-28.021946	-14.130873	0.600576
-27.801460	-23.137215	0.605581
-28.014340	-14.505229	0.610586
-28.184635	-18.876104	0.615590
-28.429328	-17.714845	0.620595
-29.311778	-17.349598	0.625600
-29.917070	-19.868451	0.630605
-30.004177	1.904704	0.635610
-30.052414	-23.437970	0.640614
-30.383372	-12.705925	0.645619
-30.556468	-10.397920	0.650624
-30.348869	-23.616224	0.655629
-30.564066	-11.845546	0.660634
-31.059698	-23.173228	0.665638
-31.707646	-20.028854	0.670643
-32.085216	-19.283488	0.675648
-32.044501	-22.307870	0.680653
-31.922254	-25.860618	0.685658
-31.971940	-20.465137	0.690662
-32.553449	-18.283362	0.695667
-32.898851	-12.702635	0.700672
-33.164496	-28.941291	0.705677
-33.467689	-11.414910	0.710682
-33.365461	-25.252698	0.715686
-33.404255	-12.519268	0.720691
-34.356995	-7.720306	0.725696
-34.365408	-15.919083	0.730701
-35.202105	-12.783283	0.735706
-34.873270	-17.298309	0.740710
-35.042952	-13.886726	0.745715
-35.350265	-24.089000	0.750720
-35.876226	-19.916455	0.755725
-36.328517	-12.114029	0.760730
-35.806937	-21.170415	0.765734
-35.734416	-20.567891	0.770739
-36.850826	-6.613182	0.775744
-37.403252	-20.810935	0.780749
-37.633810	-14.703945	0.785754
-37.787917	-23.595016	0.790758
-37.627629	-10.089018	0.795763
-38.381878	-6.292198	0.800768
-37.985655	-23.108457	0.805773
-38.216384	-13.018418	0.810778
-38.429548	-15.788145	0.815782
-38.882064	-17.802458	0.820787
-39.639748	-14.622015	0.825792
-39.591112	-22.997344	0.830797
-39.748234	-19.644663	0.835802
-39.659753	-20.771971	0.840806
-39.659121	-16.222687	0.845811
-40.535577	-17.677465	0.850816
-40.966691	-17.303399	0.855821
-40.733318	-17.209957	0.860826
-40.901082	-24.048863	0.865830
-40.768739	-19.539069	0.870835
-42.210644	-19.200606	0.875840
-42.179077	-19.778070	0.880845
-42.613543	-24.041376	0.885850
-42.758596	-25.980178	0.890854
-42.283829	-28.167340	0.895859
-42.518302	-14.647336	0.900864
-43.177518	-20.153760	0.905869
-43.430313	-16.454000	0.910874
-43.681287	-19.179875	0.915878
-43.848983	-9.662777	0.920883
-44.316940	-9.248174	0.925888
-44.771865	-17.978519	0.930893
-45.199229	-13.951033	0.935898
-45.678785	-15.385354	0.940902
-45.139468	-13.928563	0.945907
-45.612607	-10.210313	0.950912
-45.654261	-19.802241	0.955917
-45.535645	-17.609257	0.960922
-45.307295	-18.827943	0.965926
-46.037562	-19.255154	0.970931
-46.332273	-11.369700	0.975936
-46.472335	-7.225599	0.980941
-47.515874	-11.912913	0.985946
-48.090347	-16.641622	0.990950
-47.364220	-12.170496	0.995955
-48.249947	-17.496126	1.000960
-47.915202	-21.455270	1.005965
-48.363014	-14.846235	1.010970
-48.855316	-22.033230	1.015974
-49.188414	-23.015807	1.020979
-49.539403	-18.620577	1.025984
-49.499751	-24.878031	1.030989
-49.561241	-19.635730	1.035994
-49.757553	-21.180588	1.040998
-49.606383	-21.577365	1.046003
-50.671684	-13.110040	1.051008
-51.040017	-16.203607	1.056013
-50.563555	-25.892020	1.061018
-51.120262	-18.598504	1.066022
-51.862791	-22.291844	1.071027
-52.428034	-9.482773	1.076032
-51.887031	-25.353496	1.081037
-52.254130	-23.629033	1.086042
-52.561557	-22.625679	1.091046
-52.725452	-32.043549	1.096051
-53.083578	-24.281099	1.101056
-52.680864	-24.805624	1.106061
-53.533601	-19.190199	1.111066
-53.664534	-23.870910	1.116070
-54.102189	-26.200735	1.121075
-53.906968	-18.138476	1.126080
-54.098693	-25.638014	1.131085
-54.638404	-21.912565	1.136090
-55.065000	-22.801494	1.141094
-55.437394	-18.826859	1.146099
-55.512495	-7.555703	1.151104
-55.294365	-17.906226	1.156109
-56.041637	-17.862570	1.161114
-56.896824	-23.591570	1.166118
-57.027574	-21.568561	1.171123
-57.564920	-10.994200	1.176128
-56.980415	-17.760417	1.181133
-57.175300	-22.358408	1.186138
-56.975898	-22.022403	1.191142
-57.105502	-18.006480	1.196147
-57.837208	-16.108192	1.201152
-57.908611	-26.147884	1.206157
-58.102377	-19.708115	1.211162
-58.707767	-15.852220	1.216166
-59.595425	-21.490747	1.221171
-59.888330	-21.245763	1.226176
-59.505065	-31.501771	1.231181
-59.772335	-17.650810	1.236186
-59.685636	-13.946964	1.241190
-59.528851	-15.312690	1.246195
-60.251241	-11.043122	1.251200
-60.930700	-19.618287	1.256205
-61.110634	-14.499907	1.261210
-61.451385	-20.688642	1.266214
-61.428597	-19.986630	1.271219
-61.367438	-16.376881	1.276224
-62.094808	-22.900873	1.281229
-62.814779	-21.738377	1.286234
-62.811750	-32.261036	1.291238
-62.856334	-31.918680	1.296243
-62.895906	-24.683539	1.301248
-63.036664	-24.259772	1.306253
-63.375722	-23.121784	1.311258
-63.524311	-24.806944	1.316262
-64.187288	-22.217030	1.321267
-64.546073	-18.446987	1.326272
-64.877302	-26.323422	1.331277
-64.798492	-24.617768	1.336282
-64.588648	-16.706477	1.341286
-64.848896	-26.947710	1.346291
-65.486663	-15.247280	1.351296
-65.736676	-22.832652	1.356301
-65.799287	-23.259416	1.361306
-66.209979	-20.367110	1.366310
-66.790330	-22.004027	1.371315
-67.509648	-23.609815	1.376320
-67.237230	-27.590889	1.381325
-67.300412	-24.091491	1.386330
-67.693286	-24.498470	1.391334
-67.359635	-28.906678	1.396339
-67.854078	-22.293550	1.401344
-67.527563	-24.634793	1.406349
-68.406863	-21.644216	1.411354
-68.474386	-16.097266	1.416358
-68.652491	-15.908120	1.421363
-69.712029	-13.832243	1.426368
-69.776516	-21.636320	1.431373
-70.335205	-21.830827	1.436378
-70.385544	-18.001245	1.441382
-70.408942	-19.560370	1.446387
-70.928687	-14.246718	1.451392
-70.489030	-29.532201	1.456397
-70.465399	-16.814825	1.461402
-71.266995	-9.166813	1.466406
-71.629072	-14.308228	1.471411
-72.041830	-15.607421	1.476416
-71.799701	-16.401161	1.481421
-72.024746	-18.134526	1.486426
-72.109795	-16.178741	1.491430
-72.475565	-19.712451	1.496435
-73.095490	-7.034066	1.501440
-73.153414	-22.931754	1.506445
-73.334004	-21.404003	1.511450
-73.828547	-22.801188	1.516454
-74.225098	-18.503265	1.521459
-74.991515	-11.493459	1.526464
-75.141813	-14.665264	1.531469
-74.724260	-13.167370	1.536474
-74.942553	-14.158332	1.541478
-74.767395	-18.573502	1.546483
-75.236903	-16.617965	1.551488
-75.877692	-18.501726	1.556493
-76.834317	-18.463437	1.561498
-76.872917	-9.526405	1.566502
-76.751684	-11.108050	1.571507
-76.849987	-4.800195	1.576512
-76.472256	-22.360190	1.581517
-76.475017	-10.919974	1.586522
-77.514032	-21.542974	1.591526
-77.453542	-22.707050	1.596531
-78.118001	-19.626542	1.601536
-77.900842	-19.736212	1.606541
-78.599331	-14.961021	1.611546
-79.101311	-19.334032	1.616550
-78.930299	-21.138554	1.621555
-79.595366	-18.114896	1.626560
-79.351312	-28.558029	1.631565
-79.596757	-23.192180	1.636570
-80.414824	-19.455026	1.641574
-80.792307	-20.936874	1.646579
-80.963457	-17.186555	1.651584
-80.822201	-21.675536	1.656589
-81.117268	-21.749743	1.661594
-80.957299	-12.818322	1.666598
-81.226290	-28.863468	1.671603
-81.466024	-28.813417	1.676608
-82.316084	-27.975502	1.681613
-82.210143	-21.459018	1.686618
-82.702162	-18.652122	1.691622
-82.539659	-23.675902	1.696627
-83.047432	-14.409567	1.701632
-83.144103	-22.063105	1.706637
-83.537480	-17.651785	1.711642
-83.943051	-19.357042	1.716646
-83.804302	-27.721087	1.721651
-84.425142	-17.102095	1.726656
-84.691694	-24.634271	1.731661
-85.116809	-23.748629	1.736666
-85.305728	-22.665654	1.741670
-85.119884	-24.387067	1.746675
-85.483197	-16.835773	1.751680
-85.398102	-23.435646	1.756685
-85.788922	-21.881490	1.761690
-86.624812	-13.699813	1.766694
-86.535571	-28.807352	1.771699
-86.798662	-22.489665	1.776704
-86.607298	-23.266010	1.781709
-86.933463	-29.526611	1.786714
-87.798892	-24.447030	1.791718
-87.947445	-27.343867	1.796723
-88.117532	-28.810552	1.801728
-87.991180	-31.759683	1.806733
-88.258319	-23.122420	1.811738
-89.236680	-28.832237	1.816742
-89.579895	-24.637529	1.821747
-89.786710	-11.944380	1.826752
-89.896946	-25.106862	1.831757
-89.926870	-27.525479	1.836762
-89.918093	-24.496013	1.841766
-89.875119	-23.926853	1.846771
-90.385838	-14.508206	1.851776
-90.881633	-14.598614	1.856781
-91.139614	-17.633433	1.861786
-91.521792	-20.174369	1.866790
-91.228488	-26.819314	1.871795
-91.341500	-24.795903	1.876800
-91.935449	-19.100554	1.881805
-92.328668	-16.467223	1.886810
-93.119271	-18.738929	1.891814
-92.415028	-22.008986	1.896819
-93.221941	-22.272406	1.901824
-93.038542	-27.147584	1.906829
-93.635014	-21.318970	1.911834
-94.255659	-27.723539	1.916838
-94.321497	-22.211655	1.921843
-94.550832	-16.917913	1.926848
-94.651807	-27.724924	1.931853
-94.245499	-22.552299	1.936858
-94.877374	-12.807914	1.941862
-95.265280	-20.147197	1.946867
-95.837452	-15.594147	1.951872
-95.672171	-19.881232	1.956877
-95.657434	-16.678693	1.961882
-96.811761	-11.285217	1.966886
-96.348580	-25.356363	1.971891
-96.782480	-16.696296	1.976896
-97.131913	-22.409131	1.981901
-97.066865	-23.497990	1.986906
-97.730824	-22.777632	1.991910
-98.048357	-26.676341	1.996915
-98.349786	-16.657243	2.006912
-97.840199	-16.467195	2.016909
-97.238470	-29.513422	2.026906
-97.205639	-25.669656	2.036902
-96.449173	-28.920143	2.046899
-95.871222	-23.444367	2.056896
-94.871136	-23.929384	2.066893
-94.794665	-29.557461	2.076890
-94.991087	-27.195323	2.086886
-93.891724	-25.380218	2.096883
-93.590515	-27.032996	2.106880
-92.806553	-22.549104	2.116877
-92.284001	-27.147451	2.126874
-92.002470	-27.913380	2.136870
-91.148178	-30.859162	2.146867
-91.066495	-27.187723	2.156864
-90.436555	-25.020771	2.166861
-89.585952	-24.646243	2.176858
-89.369201	-24.135012	2.186854
-88.802204	-23.180987	2.196851
-88.116722	-30.262826	2.206848
-87.835692	-19.834070	2.216845
-87.591383	-21.918298	2.226842
-86.688658	-27.266394	2.236838
-86.468527	-18.823798	2.246835
-85.982936	-21.702671	2.256832
-84.780465	-21.291066	2.266829
-84.659799	-23.020268	2.276826
-84.697045	-22.317439	2.286822
-84.109258	-19.294983	2.296819
-83.700031	-17.983785	2.306816
-82.808317	-20.029436	2.316813
-82.382732	-23.241077	2.326810
-81.316681	-19.824269	2.336806
-80.947361	-17.037050	2.346803
-81.204659	-12.992891	2.356800
-80.754557	-17.643313	2.366797
-79.673553	-23.000162	2.376794
-79.147085	-18.957665	2.386790
-78.867792	-19.498341	2.396787
-78.111523	-14.706037	2.406784
-77.622767	-15.941373	2.416781
-77.680983	-13.173113	2.426778
-77.073295	-20.005267	2.436774
-76.222615	-15.807350	2.446771
-75.540770	-14.240836	2.456768
-75.125115	-19.532103	2.466765
-74.976346	-23.435547	2.476762
-74.359257	-25.900920	2.486758
-73.682928	-23.899575	2.496755
-73.660618	-24.302039	2.506752
-72.547306	-21.950597	2.516749
-72.156732	-21.228853	2.526746
-72.116333	-26.296971	2.536742
-71.008976	-21.128527	2.546739
-70.796183	-27.557083	2.556736
-70.700633	-20.089743	2.566733
-69.757360	-19.232316	2.576730
-69.496890	-22.614644	2.586726
-68.594256	-26.217330	2.596723
-68.117632	-28.008289	2.606720
-68.057545	-22.071757	2.616717
-67.425124	-14.745023	2.626714
-66.881159	-15.510634	2.636710
-66.364057	-17.212866	2.646707
-65.557358	-17.141935	2.656704
-65.377060	-21.167493	2.666701
-64.909995	-14.328179	2.676698
-64.118600	-21.366328	2.686694
-63.726213	-18.877295	2.696691
-63.395446	-21.773242	2.706688
-62.601722	-18.450241	2.716685
-62.459890	-18.858645	2.726682
-61.574129	-15.660843	2.736678
-61.115602	-17.667556	2.746675
-61.001090	-8.882236	2.756672
-60.201159	-14.737000	2.766669
-59.735911	-19.674872	2.776666
-59.409827	-14.264409	2.786662
-58.508826	-10.432273	2.796659
-58.058603	-9.323854	2.806656
-58.129892	-16.116815	2.816653
-57.330495	-21.309446	2.826650
-56.808334	-18.929314	2.836646
-56.144808	-21.427260	2.846643
-55.344417	-22.587577	2.856640
-55.386713	-12.545613	2.866637
-55.093146	-15.195025	2.876634
-54.057800	-18.454091	2.886630
-54.024168	-18.769623	2.896627
-52.863041	-12.234769	2.906624
-52.433232	-4.572386	2.916621
-52.214688	-10.457001	2.926618
-52.173990	-5.394893	2.936614
-51.132253	-7.897878	2.946611
-50.431145	-10.268634	2.956608
-50.492141	-8.066956	2.966605
-50.058982	-15.670198	2.976602
-49.484873	-15.521871	2.986598
-48.600885	-14.233910	2.996595
-48.301245	-12.712419	3.006592
-47.592733	-15.933268	3.016589
-46.971825	-17.819550	3.026586
-46.742258	-14.006411	3.036582
-46.591046	-16.427759	3.046579
-45.425506	-13.482584	3.056576
-44.923508	-14.878367	3.066573
-45.120335	-16.738694	3.076570
-44.443464	-12.184272	3.086566
-43.898684	-12.734606	3.096563
-43.095068	-17.028271	3.106560
-42.568184	-17.797558	3.116557
-42.379005	-12.742732	3.126554
-42.026316	-16.101408	3.136550
-41.003143	-12.668417	3.146547
-40.830431	-14.126966	3.156544
-40.173657	-12.445677	3.166541
-39.199353	-15.242260	3.176538
-39.352211	-15.002919	3.186534
-38.993845	-19.410984	3.196531
-38.116718	-15.023953	3.206528
-37.853703	-21.051700	3.216525
-36.880614	-18.181095	3.226522
-36.495123	-12.722861	3.236518
-36.538518	-12.712799	3.246515
-36.042464	-18.254162	3.256512
-34.905363	-20.052927	3.266509
-34.722139	-19.796225	3.276506
-33.685698	-16.663062	3.286502
-33.203853	-19.503340	3.296499
-33.418234	-15.440522	3.306496
-33.207405	-14.000233	3.316493
-32.225536	-14.061108	3.326490
-31.796054	-20.019744	3.336486
-30.636278	-13.297785	3.346483
-30.256168	-13.990367	3.356480
-30.430139	-17.853067	3.366477
-30.195216	-9.488789	3.376474
-29.447396	-12.500356	3.386470
-28.821158	-15.923798	3.396467
-28.032534	-13.477451	3.406464
-27.555515	-17.359148	3.416461
-27.187958	-12.230728	3.426458
-26.162299	-22.403354	3.436454
-26.178301	-25.292825	3.446451
-25.918570	-20.220476	3.456448
-25.346284	-19.710748	3.466445
-24.897696	-20.537533	3.476442
-24.201452	-20.278347	3.486438
-23.286790	-14.059898	3.496435
-23.199266	-19.439455	3.506432
-22.948841	-14.400500	3.516429
-22.007748	-12.785653	3.526426
-21.745445	-18.848135	3.536422
-21.138844	-16.826427	3.546419
-20.216692	-13.764163	3.556416
-20.027102	-13.562303	3.566413
-19.820517	-14.326066	3.576410
-19.447634	-19.176702	3.586406
-18.594828	-18.932389	3.596403
-18.153791	-19.849861	3.606400
-17.336633	-24.848860	3.616397
-17.023891	-23.060156	3.626394
-16.998541	-14.732939	3.636390
-15.972244	-17.924074	3.646387
-15.512874	-16.896270	3.656384
-15.424501	-11.531152	3.666381
-14.472337	-17.187879	3.676378
-14.260838	-16.403407	3.686374
-13.791239	-20.385315	3.696371
-13.307666	-17.790106	3.706368
-12.782200	-22.635988	3.716365
-11.678936	-18.673790	3.726362
-11.402314	-26.540916	3.736358
-11.059481	-22.726407	3.746355
-11.144339	-20.644555	3.756352
-10.225156	-22.057776	3.766349
-9.675952	-27.186110	3.776346
-8.755461	-26.268115	3.786342
-8.695930	-22.612229	3.796339
-8.245003	-16.457787	3.806336
-7.695118	-21.864986	3.816333
-6.916708	-20.047418	3.826330
-6.449978	-17.183499	3.836326
-6.396937	-16.630939	3.846323
-5.776584	-12.637899	3.856320
-5.696971	-9.685196	3.866317
-4.886967	-1.128527	3.876314
-4.590859	12.738025	3.886310
-4.091152	22.572084	3.896307
-3.596552	30.826262	3.906304
-3.221109	34.642042	3.916301
-2.207627	50.794880	3.926298
-1.929770	66.004254	3.936294
-1.343816	71.915964	3.946291
-1.306966	82.981504	3.956288
-0.295240	105.238841	3.966285
0.000000	108.775764	3.971290
-0.292153	113.759799	3.976294
0.485223	122.326255	3.981299
0.349100	139.731867	3.986304
0.337342	132.008090	3.991309
0.459514	133.570971	3.996314
0.482582	139.939075	4.001318
0.562685	135.257099	4.006323
0.447301	134.101412	4.011328
0.581157	129.860309	4.016333
0.663337	134.732284	4.021338
0.481724	140.951928	4.026342
0.897135	141.175213	4.031347
1.134527	144.042569	4.036352
0.840573	136.562038	4.041357
0.762204	132.480523	4.046362
0.846754	128.971577	4.051366
0.431628	120.102088	4.056371
0.501002	124.242085	4.061376
0.993733	145.023496	4.066381
1.157137	134.374525	4.071386
1.270076	135.771169	4.076390
0.919052	123.775486	4.081395
0.812709	129.809405	4.086400
0.981896	122.373827	4.091405
1.055663	130.363322	4.096410
0.639449	130.092845	4.101414
0.705478	125.074550	4.106419
0.757696	123.260036	4.111424
0.616495	130.473103	4.116429
1.181808	128.173751	4.121434
0.814645	129.180087	4.126438
0.894731	126.674717	4.131443
0.942340	141.789704	4.136448
1.222106	145.580581	4.141453
1.195683	140.842424	4.146458
0.869595	130.592363	4.151462
1.202815	126.854879	4.156467
0.813534	132.258991	4.161472
0.896884	139.930631	4.166477
1.308552	143.144165	4.171482
1.091039	159.265365	4.176486
1.336972	154.260179	4.181491
1.310235	142.653742	4.186496
0.871447	142.124196	4.191501
1.156844	129.513741	4.196506
0.912949	138.429035	4.201510
1.370306	141.290615	4.206515
1.190577	146.310937	4.211520
1.286142	137.263853	4.216525
1.573990	128.961934	4.221530
1.109089	126.898912	4.226534
1.072104	125.506399	4.231539
1.125678	131.904551	4.236544
0.925314	144.998602	4.241549
1.727468	141.928402	4.246554
1.105027	153.379794	4.251558
1.196926	142.884317	4.256563
1.761424	152.926566	4.261568
1.354921	150.367243	4.266573
0.902237	136.935255	4.271578
0.891171	154.599813	4.276582
1.528402	152.823921	4.281587
1.326893	153.212860	4.286592
1.499810	159.307710	4.291597
1.651846	154.690456	4.296602
1.560281	156.653603	4.301606
1.716850	156.249655	4.306611
1.310979	143.215322	4.311616
1.302659	144.678302	4.316621
1.324629	140.606472	4.321626
1.338039	167.789878	4.326630
1.388110	157.421124	4.331635
1.638718	162.342811	4.336640
1.676647	160.407135	4.341645
1.683359	143.800052	4.346650
1.347141	150.809379	4.351654
1.553659	147.316239	4.356659
1.534914	164.061374	4.361664
1.632700	159.354492	4.366669
1.855058	155.238805	4.371674
1.505373	155.340774	4.376678
1.569243	158.494570	4.381683
1.511571	154.786305	4.386688
1.113660	156.031541	4.391693
1.768576	152.512876	4.396698
1.370003	168.788821	4.401702
1.596036	158.177540	4.406707
1.988712	152.472481	4.411712
1.784444	161.593583	4.416717
1.594707	153.432448	4.421722
1.404562	166.433177	4.426726
1.614062	158.902723	4.431731
1.786297	162.934967	4.436736
1.315769	157.775583	4.441741
1.407256	159.669102	4.446746
1.652439	164.303741	4.451750
1.377801	159.740263	4.456755
1.605994	166.870521	4.461760
1.701134	174.736489	4.466765
2.025774	175.524386	4.471770
1.733196	183.710146	4.476774
2.044467	180.608804	4.481779
1.732754	176.516155	4.486784
1.807430	180.547774	4.491789
2.235365	179.073379	4.496794
1.702749	187.783720	4.501798
1.921908	177.429755	4.506803
1.766839	185.388467	4.511808
1.702264	190.773677	4.516813
2.141568	189.050745	4.521818
2.014116	187.397073	4.526822
2.011968	195.578746	4.531827
2.013120	179.383774	4.536832
1.963790	187.047620	4.541837
1.792891	183.189303	4.546842
1.810274	181.222023	4.551846
2.170682	185.652070	4.556851
2.034677	190.823781	4.561856
1.764719	192.321173	4.566861
1.873363	180.247555	4.571866
1.933729	185.913860	4.576870
1.690002	179.713108	4.581875
1.880458	183.926013	4.586880
1.627518	186.085127	4.591885
2.184364	194.515116	4.596890
2.375511	196.491196	4.601894
2.391594	189.629908	4.606899
2.045084	193.660670	4.611904
1.945099	182.264924	4.616909
2.250177	192.407696	4.621914
2.391628	193.110224	4.626918
2.205774	197.957512	4.631923
2.377745	202.518140	4.636928
2.285279	194.076093	4.641933
2.289645	186.017596	4.646938
2.221329	189.672857	4.651942
2.012814	193.792863	4.656947
2.236715	203.726824	4.661952
2.233991	205.135154	4.666957
2.394201	200.877276	4.671962
2.348877	210.808866	4.676966
2.511844	207.676827	4.681971
2.587898	207.668219	4.686976
2.393876	201.649540	4.691981
2.514214	189.963227	4.696986
2.379830	192.534144	4.701990
2.077295	196.858610	4.706995
2.161664	207.418559	4.712000
2.127633	203.333289	4.717005
2.353650	206.249881	4.722010
2.300139	212.851392	4.727014
2.497505	208.173285	4.732019
2.357826	213.623978	4.737024
2.669748	209.437387	4.742029
3.127098	205.038333	4.747034
2.289707	207.737690	4.752038
2.661009	202.589587	4.757043
2.817983	208.016236	4.762048
2.509062	211.832348	4.767053
3.110667	206.569294	4.772058
2.986138	203.994534	4.777062
2.401354	197.736148	4.782067
2.714186	188.088912	4.787072
2.276447	196.591501	4.792077
2.401500	188.969781	4.797082
2.826811	204.741005	4.802086
2.834889	204.464577	4.807091
2.833420	205.720855	4.812096
2.733913	211.358278	4.817101
2.739018	199.680409	4.822106
2.463482	205.905208	4.827110
2.524425	205.490838	4.832115
2.536019	212.319488	4.837120
2.521413	209.006294	4.842125
2.591745	203.307115	4.847130
2.979401	210.858642	4.852134
2.852082	205.724899	4.857139
2.768652	207.908242	4.862144
2.656666	221.371394	4.867149
2.727054	205.064381	4.872154
2.836880	206.265368	4.877158
2.822630	218.517429	4.882163
2.824161	209.061016	4.887168
2.556466	211.383778	4.892173
2.831457	204.811195	4.897178
2.896710	217.408374	4.902182
3.038260	210.847074	4.907187
3.352332	212.000442	4.912192
2.957597	216.737891	4.917197
2.830827	212.863206	4.922202
2.818345	211.941424	4.927206
2.865279	212.130333	4.932211
2.961288	210.549432	4.937216
2.923138	210.631369	4.942221
2.982659	211.346654	4.947226
2.825491	212.152623	4.952230
2.829253	211.297912	4.957235
2.910115	215.167229	4.962240
2.892899	227.783582	4.967245
3.276035	224.886173	4.972250
3.030465	232.004802	4.977254
3.360963	231.576935	4.982259
3.015037	229.723162	4.987264
3.235248	219.837234	4.992269
2.818887	221.351097	4.997274
2.835954	223.873127	5.002278
3.155564	240.078446	5.007283
3.368784	235.394700	5.012288
3.357855	242.075011	5.017293
3.584779	235.041676	5.022298
3.372467	234.758432	5.027302
3.131836	223.862274	5.032307
2.950104	218.107426	5.037312
3.363394	221.940804	5.042317
3.483607	221.643753	5.047322
3.197865	227.288030	5.052326
3.414684	230.826141	5.057331
3.376860	225.972680	5.062336
3.066836	222.781407	5.067341
3.454233	217.573848	5.072346
3.298352	234.865573	5.077350
3.365792	229.381967	5.082355
3.578870	231.193289	5.087360
3.139047	237.007090	5.092365
3.419825	226.785868	5.097370
3.553178	230.836836	5.102374
3.228633	227.559240	5.107379
3.433957	228.169569	5.112384
3.433009	237.164142	5.117389
3.721084	233.553885	5.122394
3.566794	229.458859	5.127398
3.202429	233.641103	5.132403
3.634015	237.294470	5.137408
3.420469	237.552409	5.142413
3.412725	232.295639	5.147418
3.142196	232.575105	5.152422
3.373929	227.916951	5.157427
3.754412	229.256128	5.162432
3.268374	231.116190	5.167437
3.628315	221.493238	5.172442
3.281180	235.122723	5.177446
3.513634	227.310263	5.182451
3.602030	226.391755	5.187456
3.358682	235.920767	5.192461
3.458344	219.539582	5.197466
3.473642	227.098472	5.202470
3.574335	226.646275	5.207475
3.497440	223.899584	5.212480
3.290127	235.893822	5.217485
4.164926	247.975845	5.222490
4.130547	250.796949	5.227494
3.695347	237.722821	5.232499
3.485488	230.178539	5.237504
3.862466	240.455674	5.242509
3.742559	229.920358	5.247514
3.418776	241.610038	5.252518
3.758485	244.607009	5.257523
4.071912	254.549205	5.262528
3.768527	250.929795	5.267533
4.129410	244.777250	5.272538
4.010584	245.358956	5.277542
3.657957	243.199347	5.282547
3.894037	242.485630	5.287552
3.888375	237.348755	5.292557
4.018847	231.311180	5.297562
4.039990	238.103553	5.302566
3.767843	235.621374	5.307571
3.778146	236.249412	5.312576
3.762254	250.928299	5.317581
4.426172	252.128437	5.322586
3.995388	249.069854	5.327590
3.888237	240.867348	5.332595
4.070623	227.598997	5.337600
3.843399	234.221236	5.342605
4.036917	243.239316	5.347610
4.106084	256.364249	5.352614
3.957267	243.890921	5.357619
3.982334	249.689290	5.362624
4.390498	262.065434	5.367629
4.443792	245.678789	5.372634
4.126921	239.258455	5.377638
3.775467	231.540069	5.382643
4.069816	240.656342	5.387648
3.813784	239.781969	5.392653
4.011613	253.244364	5.397658
4.192280	261.407095	5.402662
4.164962	269.165623	5.407667
4.316505	251.830387	5.412672
4.440793	261.805199	5.417677
4.366595	262.016132	5.422682
4.161741	252.598157	5.427686
4.250453	252.549613	5.432691
4.247096	251.582116	5.437696
4.030271	252.827637	5.442701
3.982649	253.648189	5.447706
4.158709	263.314390	5.452710
3.845905	256.899744	5.457715
4.264569	257.056086	5.462720
4.303894	266.680305	5.467725
4.121019	251.001129	5.472730
4.028014	262.053790	5.477734
4.028082	252.524816	5.482739
4.114652	267.681299	5.487744
4.078766	265.377461	5.492749
4.645643	268.750347	5.497754
4.412887	269.944567	5.502758
4.225338	270.467373	5.507763
4.438587	274.936173	5.512768
4.547808	296.410212	5.517773
4.662844	276.910340	5.522778
4.278546	276.619073	5.527782
4.428827	280.012532	5.532787
4.559973	280.982418	5.537792
4.250061	288.487567	5.542797
4.472830	287.839195	5.547802
4.479961	292.669116	5.552806
4.787325	283.468760	5.557811
4.820304	280.939067	5.562816
4.773813	288.064686	5.567821
4.576649	274.618119	5.572826
4.152994	270.365710	5.577830
4.879707	283.483195	5.582835
4.778688	275.653034	5.587840
4.834332	284.980498	5.592845
4.380426	273.548051	5.597850
4.554554	278.725283	5.602854
4.243740	278.609233	5.607859
4.659269	292.534461	5.612864
4.282512	291.726338	5.617869
4.310804	287.004933	5.622874
4.304254	284.927475	5.627878
4.629412	282.975537	5.632883
4.703256	283.103311	5.637888
4.890084	292.653960	5.642893
4.738056	292.171508	5.647898
4.601820	289.019602	5.652902
4.736534	285.850820	5.657907
4.609399	281.419367	5.662912
4.768379	296.757585	5.667917
5.163863	296.373382	5.672922
4.903099	291.254063	5.677926
4.896137	296.212728	5.682931
4.875172	287.626628	5.687936
4.774968	293.371750	5.692941
4.908317	288.649806	5.697946
4.310520	297.057143	5.702950
4.987913	304.079553	5.707955
5.150164	311.378321	5.712960
4.803217	313.061714	5.717965
5.520566	316.854099	5.722970
5.278859	308.103045	5.727974
4.830149	296.771012	5.732979
5.180674	287.779065	5.737984
5.002266	283.725746	5.742989
4.929128	277.106102	5.747994
4.948159	289.406813	5.752998
4.425219	295.027933	5.758003
5.109573	296.054053	5.763008
5.014882	315.190256	5.768013
5.094419	312.716583	5.773018
5.083770	308.342915	5.778022
5.366265	312.256787	5.783027
5.577309	304.001545	5.788032
5.420586	309.695362	5.793037
5.070099	295.326706	5.798042
5.204803	299.889998	5.803046
5.293514	291.274165	5.808051
5.207023	286.728816	5.813056
4.777393	292.496756	5.818061
4.695788	292.958775	5.823066
4.998415	315.506855	5.828070
5.033947	311.942230	5.833075
5.257927	297.734060	5.838080
5.341940	307.297560	5.843085
5.560263	309.759795	5.848090
5.606585	315.029702	5.853094
5.602173	308.247487	5.858099
5.510479	297.400860	5.863104
5.585584	299.936011	5.868109
5.244911	304.060800	5.873114
4.932864	298.484401	5.878118
5.295744	303.980259	5.883123
5.536117	306.464370	5.888128
5.543792	312.347723	5.893133
5.419659	315.189139	5.898138
5.740493	312.677897	5.903142
5.125961	305.930567	5.908147
5.286061	296.541166	5.913152
5.302890	306.393531	5.918157
5.547399	312.170409	5.923162
5.377262	312.779088	5.928166
5.303855	315.264600	5.933171
5.475505	318.116910	5.938176
5.468909	321.272215	5.943181
5.470604	314.912983	5.948186
5.338678	319.419719	5.953190
5.523423	311.288789	5.958195
5.711180	319.624447	5.963200
5.295272	321.720368	5.968205
5.143031	314.167079	5.973210
5.746253	318.964307	5.978214
5.614423	320.493987	5.983219
5.511319	325.398027	5.988224
5.486794	327.787346	5.993229
5.645786	312.690791	5.998234
5.449004	323.538189	6.003238
5.134747	326.235205	6.008243
5.638071	315.789461	6.013248
5.366993	316.518259	6.018253
5.489823	312.060534	6.023258
5.544060	316.705960	6.028262
5.433588	314.072049	6.033267
5.568971	315.993551	6.038272
5.683079	326.409739	6.043277
5.853216	324.576844	6.048282
5.356098	317.959923	6.053286
5.032830	317.475658	6.058291
5.666468	330.196389	6.063296
5.533473	336.838795	6.068301
5.447263	335.586805	6.073306
6.023931	337.164360	6.078310
5.630848	342.015479	6.083315
5.994317	329.626842	6.088320
5.699677	325.003162	6.093325
5.750889	315.352298	6.098330
5.601067	320.307902	6.103334
5.358839	322.452710	6.108339
5.439780	312.243572	6.113344
5.309531	321.318430	6.118349
5.192284	322.811038	6.123354
5.957604	339.899327	6.128358
5.802175	333.365239	6.133363
5.652466	317.105046	6.138368
5.303438	315.023961	6.143373
5.611839	320.028441	6.148378
5.741279	339.405015	6.153382
5.520447	325.743798	6.158387
5.527611	323.869841	6.163392
5.106482	330.196444	6.168397
5.653934	327.020339	6.173402
5.688483	333.345597	6.178406
6.049190	342.761634	6.183411
5.921338	330.550732	6.188416
5.310233	326.798887	6.193421
5.610430	318.868273	6.198426
5.559401	313.864987	6.203430
5.253630	320.581743	6.208435
5.787866	330.344072	6.213440
5.519918	327.810606	6.218445
5.561624	321.106626	6.223450
5.708200	325.702878	6.228454
5.263305	330.084341	6.233459
5.737641	336.704952	6.238464
5.777453	345.569849	6.243469
5.784214	332.721065	6.248474
5.220087	330.755724	6.253478
5.608738	332.043018	6.258483
5.605201	331.651339	6.263488
5.705043	335.473434	6.268493
5.771512	327.648809	6.273498
5.414798	325.303168	6.278502
5.287748	328.195660	6.283507
5.801123	328.919378	6.288512
5.914776	322.039683	6.293517
5.610233	322.871767	6.298522
5.465846	323.811790	6.303526
5.254009	316.792953	6.308531
5.651498	328.677269	6.313536
5.545789	327.440970	6.318541
5.850884	332.205528	6.323546
5.819681	325.032016	6.328550
5.555648	320.451027	6.333555
5.293478	314.714999	6.338560
5.200175	332.360901	6.343565
5.802123	332.640565	6.348570
5.716913	334.526813	6.353574
5.488923	332.825507	6.358579
5.791071	319.494150	6.363584
5.435275	313.598696	6.368589
5.553336	319.964729	6.373594
5.790799	317.346247	6.378598
5.652428	320.604325	6.383603
5.888333	318.318274	6.388608
5.454798	318.828761	6.393613
5.761724	317.145409	6.398618
5.889952	322.453185	6.403622
5.575300	316.516524	6.408627
5.553149	303.447639	6.413632
5.327512	316.317964	6.418637
5.503154	311.614739	6.423642
5.803844	316.835551	6.428646
5.576465	313.697832	6.433651
5.799064	308.892384	6.438656
5.207963	314.824675	6.443661
5.346472	319.703750	6.448666
5.474804	317.950130	6.453670
5.453222	324.518238	6.458675
5.593184	315.353421	6.463680
5.449890	323.104721	6.468685
5.566462	321.738903	6.473690
5.425514	330.793285	6.478694
5.598346	343.705992	6.483699
5.831046	337.975163	6.488704
5.936006	334.988173	6.493709
5.876539	325.443120	6.498714
5.846431	319.933546	6.503718
5.542321	321.613434	6.508723
5.677786	313.733780	6.513728
5.424427	323.574440	6.518733
5.534681	318.995287	6.523738
5.485914	314.178306	6.528742
5.644587	316.213239	6.533747
5.513356	314.829057	6.538752
5.695848	318.059324	6.543757
5.601791	313.224086	6.548762
5.841228	315.439429	6.553766
5.691753	316.702941	6.558771
5.801057	309.096278	6.563776
5.592769	322.821269	6.568781
5.640792	312.481217	6.573786
5.912791	311.470844	6.578790
5.617590	307.970369	6.583795
5.681687	313.670935	6.588800
5.753994	324.799135	6.593805
6.160854	315.589599	6.598810
5.866120	312.437057	6.603814
5.291725	305.734097	6.608819
5.697305	297.581445	6.613824
5.244769	294.757191	6.618829
5.239449	300.500197	6.623834
5.974539	314.435798	6.628838
5.612859	319.022598	6.633843
5.816819	318.940292	6.638848
5.588324	309.465857	6.643853
5.505814	305.312182	6.648858
5.519115	308.296711	6.653862
5.622688	312.368153	6.658867
5.821580	317.924349	6.663872
5.706893	304.657902	6.668877
5.614182	297.130153	6.673882
5.751693	301.648716	6.678886
5.465220	301.895865	6.683891
5.328874	291.894573	6.688896
5.310705	304.704115	6.693901
5.138744	314.528932	6.698906
5.680714	316.105560	6.703910
5.710052	325.785149	6.708915
6.167262	306.472410	6.713920
5.655298	315.837646	6.718925
5.144980	295.998529	6.723930
5.387547	304.161133	6.728934
5.226943	311.832866	6.733939
5.709915	307.822097	6.738944
5.996151	320.318504	6.743949
5.789076	318.980932	6.748954
5.796640	320.590147	6.753958
5.536434	303.429698	6.758963
5.732459	294.800319	6.763968
5.252814	299.500391	6.768973
5.621247	306.526615	6.773978
5.418131	312.050489	6.778982
5.428483	314.510304	6.783987
5.916718	313.251133	6.788992
5.640041	319.609025	6.793997
5.592577	307.904469	6.799002
5.797081	301.807889	6.804006
5.573647	296.562536	6.809011
5.813404	289.998571	6.814016
5.703957	292.166994	6.819021
5.276363	304.572055	6.824026
5.481093	286.883660	6.829030
5.562983	292.983238	6.834035
5.429640	295.610953	6.839040
5.694939	317.639674	6.844045
5.363942	307.766754	6.849050
5.522779	306.473450	6.854054
5.680078	318.322390	6.859059
5.971563	319.036364	6.864064
5.895651	310.680267	6.869069
5.141463	300.522071	6.874074
5.422735	300.025938	6.879078
5.792317	303.470677	6.884083
5.668044	305.306057	6.889088
5.330653	303.295926	6.894093
5.349532	304.979307	6.899098
5.721922	315.443858	6.904102
5.772084	315.815760	6.909107
5.571431	297.352092	6.914112
5.623158	300.805191	6.919117
5.305480	301.136291	6.924122
5.572761	294.783171	6.929126
5.548501	310.991475	6.934131
6.003383	307.687420	6.939136
5.616225	309.899084	6.944141
5.364934	296.970282	6.949146
5.798818	301.176951	6.954150
5.109259	297.124121	6.959155
5.356437	303.346662	6.964160
5.665240	314.830332	6.969165
5.684120	319.936837	6.974170
5.899766	309.975641	6.979174
5.421915	325.011248	6.984179
5.394635	312.348109	6.989184
5.345060	314.288917	6.994189
5.613915	323.206725	6.999194
5.909550	325.900529	7.004198
5.507846	310.726763	7.009203
5.864814	314.553112	7.014208
5.660035	322.117834	7.019213
5.670625	314.248133	7.024218
5.618445	302.977741	7.029222
5.478473	294.233000	7.034227
5.828420	290.682700	7.039232
5.309409	300.007897	7.044237
5.420767	304.786793	7.049242
5.684339	303.281033	7.054246
5.679876	315.022282	7.059251
5.873142	306.984938	7.064256
5.454627	306.369974	7.069261
5.463646	297.358429	7.074266
5.397585	296.286800	7.079270
5.459135	312.010354	7.084275
5.961390	317.623718	7.089280
5.846061	309.068119	7.094285
5.463735	299.902373	7.099290
5.604085	298.314560	7.104294
5.278959	303.689752	7.109299
5.659564	306.718331	7.114304
5.188497	313.755045	7.119309
5.425904	307.605884	7.124314
5.749534	312.781995	7.129318
5.590464	319.529693	7.134323
5.364359	317.698383	7.139328
5.433071	325.093977	7.144333
5.730418	316.224189	7.149338
5.875480	316.565498	7.154342
5.699692	315.409713	7.159347
5.862844	315.340088	7.164352
5.460793	311.568352	7.169357
5.006210	316.479658	7.174362
5.599338	320.047780	7.179366
5.393536	323.018970	7.184371
5.749195	311.042843	7.189376
5.629710	316.367039	7.194381
5.884570	328.216615	7.199386
5.954477	316.731056	7.204390
5.601256	310.183481	7.209395
5.380751	298.009173	7.214400
5.517275	302.360214	7.219405
5.447818	309.796297	7.224410
5.900992	313.547556	7.229414
5.618196	316.293455	7.234419
5.949049	302.312247	7.239424
5.646290	305.573772	7.244429
5.142123	298.704859	7.249434
5.511328	302.045254	7.254438
5.301025	312.733402	7.259443
5.653248	313.627741	7.264448
5.752987	318.724820	7.269453
5.824185	317.935533	7.274458
5.586319	294.434725	7.279462
5.599909	294.701592	7.284467
5.417513	296.909846	7.289472
5.467159	297.028733	7.294477
5.571489	309.224431	7.299482
5.856565	306.263184	7.304486
5.751633	301.543536	7.309491
5.807093	294.533709	7.314496
5.552838	295.671168	7.319501
5.345680	293.643925	7.324506
5.402623	288.595361	7.329510
5.524963	300.538317	7.334515
5.633805	309.063423	7.339520
5.530754	297.155561	7.344525
5.589116	303.189205	7.349530
5.676161	303.476272	7.354534
5.814896	310.259855	7.359539
5.592880	285.687260	7.364544
5.414336	293.257377	7.369549
5.340578	294.300295	7.374554
5.686659	304.050776	7.379558
5.558723	315.140546	7.384563
5.755285	314.648111	7.389568
5.737973	309.892672	7.394573
5.537063	302.865812	7.399578
5.638524	298.737278	7.404582
5.473990	306.558314	7.409587
5.623424	295.370430	7.414592
5.680736	286.155223	7.419597
4.985499	296.672096	7.424602
5.423228	303.469234	7.429606
5.670228	308.976808	7.434611
5.852198	307.252803	7.439616
5.731283	314.152743	7.444621
5.613470	313.778857	7.449626
5.571893	296.296478	7.454630
5.562440	311.591333	7.459635
5.485812	306.168099	7.464640
5.606307	310.448873	7.469645
5.514928	314.607615	7.474650
5.853847	303.342768	7.479654
5.661975	314.436165	7.484659
5.803646	295.855925	7.489664
5.391185	294.914158	7.494669
5.156815	284.769947	7.499674
5.605038	299.278537	7.504678
5.533617	313.640261	7.509683
6.007949	312.345290	7.514688
5.818566	302.611673	7.519693
5.558502	301.016601	7.524698
5.424462	288.332137	7.529702
5.218639	285.134120	7.534707
5.905276	297.663081	7.539712
5.746225	292.591200	7.544717
5.252704	290.345956	7.549722
5.497404	289.102558	7.554726
5.548980	306.994792	7.559731
5.640827	315.240979	7.564736
5.960922	316.349124	7.569741
6.040402	305.849156	7.574746
5.937103	292.511345	7.579750
5.386887	294.849632	7.584755
5.785977	285.755215	7.589760
5.683415	297.502235	7.594765
5.904663	287.688873	7.599770
5.756724	288.664248	7.604774
5.633725	293.735889	7.609779
5.656050	300.091512	7.614784
5.962041	295.997571	7.619789
5.275104	295.266215	7.624794
5.405491	287.260816	7.629798
5.442152	296.214763	7.634803
5.706449	293.259917	7.639808
5.625219	293.184050	7.644813
5.311112	298.794803	7.649818
5.675580	291.904542	7.654822
5.280004	293.389864	7.659827
5.596022	290.873047	7.664832
5.656189	289.440086	7.669837
5.411428	293.651178	7.674842
5.659288	285.659126	7.679846
5.421783	292.279823	7.684851
5.763523	284.368067	7.689856
5.757309	284.403904	7.694861
5.268829	298.207302	7.699866
5.321456	290.865730	7.704870
5.239214	287.888912	7.709875
5.577538	288.949926	7.714880
5.880676	287.561390	7.719885
5.959742	282.601131	7.724890
5.701505	278.851302	7.729894
5.580735	290.816284	7.734899
5.760810	285.814988	7.739904
5.637571	280.228179	7.744909
5.823722	283.207938	7.749914
5.745522	280.284275	7.754918
5.776382	287.777494	7.759923
5.718038	282.838629	7.764928
5.990759	282.742454	7.769933
5.520589	286.912711	7.774938
5.900643	276.479855	7.779942
5.155409	277.326768	7.784947
5.441817	278.126950	7.789952
5.547692	287.873694	7.794957
5.683986	287.757632	7.799962
5.575720	286.281294	7.804966
5.519969	290.722380	7.809971
5.468599	282.115707	7.814976
5.567399	279.025283	7.819981
5.545149	287.573954	7.824986
5.828028	278.083189	7.829990
5.616921	286.094963	7.834995
5.699893	283.389810	7.840000
5.676238	292.391109	7.845005
5.617519	296.127155	7.850010
5.736599	279.037387	7.855014
5.963417	283.358547	7.860019
5.358328	266.289795	7.865024
5.340857	269.348710	7.870029
5.599611	276.622948	7.875034
5.620438	274.623485	7.880038
5.355263	286.035155	7.885043
5.647427	281.962352	7.890048
5.886529	295.342424	7.895053
5.614611	291.325808	7.900058
5.346867	275.533276	7.905062
5.281185	286.556389	7.910067
5.471085	285.251922	7.915072
5.458391	293.321390	7.920077
5.300055	286.177178	7.925082
5.731382	285.002798	7.930086
5.571125	288.125075	7.935091
5.599602	292.673268	7.940096
5.579571	283.716872	7.945101
5.498083	288.013271	7.950106
5.813065	283.497162	7.955110
5.829265	285.826351	7.960115
5.529781	294.747214	7.965120
5.672154	301.536555	7.970125
5.786307	296.146676	7.975142
5.841891	297.602301	7.980160
5.322654	291.207871	7.985178
5.617526	300.751975	7.990195
5.556265	290.426909	7.995213
5.469787	287.594070	8.000230
5.827416	289.125736	8.005248
5.689090	298.551105	8.010266
5.572770	295.369481	8.015283
5.711362	298.301638	8.020301
5.262630	304.717538	8.025318
5.712029	289.986600	8.030336
5.306427	287.266560	8.035354
5.626361	288.772539	8.040371
5.476511	293.261148	8.045389
5.476484	303.390781	8.050406
5.797240	287.446024	8.055424
5.685014	299.363429	8.060442
5.426024	300.161172	8.065459
5.280817	287.031204	8.070477
5.292453	294.770209	8.075494
5.705806	290.818190	8.080512
5.308133	297.021023	8.085530
5.213338	296.082852	8.090547
5.558394	302.463519	8.095565
5.503248	311.740252	8.100582
5.775540	310.258960	8.105600
5.658019	308.838360	8.110618
5.799392	315.392748	8.115635
5.742658	316.095889	8.120653
5.545687	313.346517	8.125670
5.771182	313.595484	8.130688
5.779263	314.345334	8.135706
5.916045	312.563266	8.140723
5.904399	309.826063	8.145741
5.576544	316.967877	8.150758
5.834908	319.199772	8.155776
5.708452	316.423643	8.160794
5.744838	321.662703	8.165811
5.918934	318.959692	8.170829
5.595521	322.342461	8.175846
5.615745	318.461112	8.180864
5.818693	320.862574	8.185882
5.527360	313.710012	8.190899
6.065061	317.428896	8.195917
5.493818	321.045900	8.200934
6.066567	316.194949	8.205952
6.112189	314.928819	8.210970
6.026203	307.479215	8.215987
5.685827	308.469502	8.221005
5.455169	322.462830	8.226022
5.833669	319.639636	8.231040
5.855449	321.192040	8.236058
5.699866	317.704117	8.241075
5.973578	310.820167	8.246093
5.730566	322.814752	8.251110
5.603918	316.362343	8.256128
5.739745	317.773920	8.261146
5.468985	320.747726	8.266163
5.690530	312.230970	8.271181
5.800777	331.901851	8.276198
6.208197	330.844462	8.281216
5.799079	323.189556	8.286234
5.901938	326.231417	8.291251
6.152352	319.584607	8.296269
5.795641	319.062735	8.301286
5.603777	323.403268	8.306304
6.040932	333.591075	8.311322
5.944170	339.147501	8.316339
6.174785	344.324770	8.321357
5.835066	332.891229	8.326374
5.999426	334.705441	8.331392
6.143327	332.145977	8.336410
5.845390	330.081317	8.341427
5.922684	316.743124	8.346445
5.636809	330.505229	8.351462
6.388493	333.108418	8.356480
6.148189	335.200218	8.361498
6.086761	327.772028	8.366515
6.152443	322.917977	8.371533
5.804403	324.707832	8.376550
5.760651	318.460255	8.381568
6.061258	327.858322	8.386586
5.957169	332.901518	8.391603
6.317258	322.466652	8.396621
6.125253	327.943235	8.401638
6.164242	324.560708	8.406656
6.229526	320.501939	8.411674
5.682385	322.912896	8.416691
6.036696	318.263203	8.421709
5.846161	315.247756	8.426726
5.951553	325.613438	8.431744
5.932747	331.429108	8.436762
6.215285	336.588825	8.441779
6.217815	332.416754	8.446797
6.278748	336.632728	8.451814
6.154782	329.943225	8.456832
6.091316	322.531131	8.461850
6.229186	326.479518	8.466867
6.228065	309.101711	8.471885
5.803850	315.617934	8.476902
5.754982	315.543565	8.481920
6.262093	324.256263	8.486938
6.494488	339.547053	8.491955
6.366186	326.786789	8.496973
5.969167	326.766626	8.501990
5.762394	310.080365	8.507008
6.456503	325.715798	8.512026
6.282881	322.199127	8.517043
6.063029	315.433044	8.522061
5.761713	320.128270	8.527078
6.289801	323.845496	8.532096
6.427649	334.461736	8.537114
5.852268	332.891528	8.542131
6.269963	337.348585	8.547149
6.185253	344.865939	8.552166
6.236066	346.890326	8.557184
6.167425	338.933107	8.562202
6.063650	346.551255	8.567219
6.444224	340.010398	8.572237
6.173495	342.921090	8.577255
6.172112	347.430776	8.582272
6.158089	344.962167	8.587290
5.822706	347.715678	8.592307
6.191847	344.597307	8.597325
5.834538	343.135148	8.602343
6.304323	347.454716	8.607360
6.589277	345.646419	8.612378
6.286618	338.924777	8.617395
6.268329	348.833229	8.622413
6.409170	346.839098	8.627431
6.561097	345.960336	8.632448
6.559476	342.827113	8.637466
6.385185	348.553394	8.642483
6.419790	344.966431	8.647501
6.346721	350.351922	8.652519
5.780668	350.209763	8.657536
6.299809	341.271138	8.662554
6.230347	348.202328	8.667571
6.422518	346.307497	8.672589
6.345383	342.520192	8.677607
6.225226	346.799076	8.682624
6.531058	343.185661	8.687642
6.226559	340.569785	8.692659
6.122510	343.823735	8.697677
6.161409	339.339904	8.702695
6.250553	345.028323	8.707712
6.629194	348.977095	8.712730
6.122155	342.965735	8.717747
6.438085	346.286832	8.722765
6.480829	353.553985	8.727783
6.381617	345.850818	8.732800
6.215358	333.377310	8.737818
6.436412	346.142210	8.742835
6.673000	345.568985	8.747853
6.505958	335.515969	8.752871
6.503090	351.969961	8.757888
6.595420	346.373336	8.762906
6.615299	351.728578	8.767923
6.250971	350.415827	8.772941
6.381647	342.474908	8.777959
6.792252	344.449586	8.782976
6.470821	350.703679	8.787994
6.608600	343.083529	8.793011
6.658304	351.170062	8.798029
6.799048	347.875824	8.803047
6.324422	340.701300	8.808064
6.701019	338.910291	8.813082
6.289806	355.951700	8.818099
6.656903	353.720380	8.823117
6.647140	347.003622	8.828135
6.289343	343.951099	8.833152
6.446831	346.905567	8.838170
6.136163	348.083724	8.843187
6.587255	354.324830	8.848205
6.118783	336.552727	8.853223
6.294810	347.506994	8.858240
6.455648	350.596633	8.863258
6.058788	354.101291	8.868275
6.293491	347.258112	8.873293
5.965094	352.916876	8.878311
6.137657	355.843753	8.883328
6.725391	367.172564	8.888346
6.625325	373.783498	8.893363
6.977171	378.553759	8.898381
7.002129	375.886582	8.903399
6.880125	368.903284	8.908416
6.537450	355.261241	8.913434
6.439559	350.685102	8.918451
6.723026	355.270354	8.923469
6.632382	351.153809	8.928487
6.694935	361.317910	8.933504
6.712077	355.269111	8.938522
6.806450	353.064475	8.943539
6.508247	350.889406	8.948557
6.506442	356.670881	8.953575
6.598366	370.260591	8.958592
6.807648	366.618026	8.963610
6.516184	368.910290	8.968627
6.973791	365.115458	8.973645
6.696362	358.778023	8.978663
6.586821	368.315706	8.983680
6.736281	364.679299	8.988698
6.838155	375.032936	8.993715
6.810192	371.600867	8.998733
6.549928	355.503529	9.003751
6.476187	363.514619	9.008768
6.776764	370.198865	9.013786
7.028771	371.690182	9.018803
6.838580	372.256322	9.023821
6.462976	357.388706	9.028839
6.274353	371.056809	9.033856
6.449767	377.681654	9.038874
6.757950	371.716916	9.043891
6.524257	368.279013	9.048909
6.725747	369.323783	9.053927
6.789122	374.637548	9.058944
6.905206	368.535472	9.063962
6.692170	371.209980	9.068979
6.623642	367.938854	9.073997
6.738405	372.383128	9.079015
7.106877	369.324815	9.084032
6.847568	359.649050	9.089050
6.947559	372.486464	9.094067
6.982845	367.536153	9.099085
6.928315	367.248083	9.104103
6.972754	373.047608	9.109120
6.838493	365.794835	9.114138
6.581873	368.472972	9.119155
6.708023	375.566211	9.124173
6.824485	368.280711	9.129191
6.641384	373.680185	9.134208
6.591437	368.926172	9.139226
6.593742	371.614487	9.144243
6.769529	372.581213	9.149261
6.739461	386.177306	9.154279
7.027156	389.998243	9.159296
7.162406	397.052206	9.164314
7.009235	385.747367	9.169331
6.865491	373.106232	9.174349
6.984980	377.925293	9.179367
6.875105	387.702867	9.184384
7.159302	387.197964	9.189402
7.022158	388.702537	9.194419
6.724803	379.490253	9.199437
7.264098	373.618912	9.204455
7.064950	377.143281	9.209472
6.738068	377.847463	9.214490
7.252976	374.816839	9.219507
6.840578	375.427043	9.224525
6.915684	372.875129	9.229543
6.684946	389.588684	9.234560
6.904927	391.466822	9.239578
7.295130	397.076828	9.244595
7.238277	409.124533	9.249613
7.133099	398.825176	9.254631
6.887322	400.753742	9.259648
7.465528	389.912510	9.264666
6.797907	375.415376	9.269683
6.813165	380.610409	9.274701
7.454604	389.431606	9.279719
7.046538	395.904320	9.284736
7.504057	385.665675	9.289754
7.240307	379.102053	9.294771
6.974999	374.372103	9.299789
7.434649	372.047479	9.304807
6.888898	369.750013	9.309824
7.227815	371.966219	9.314842
7.097402	381.800633	9.319859
6.740547	379.426420	9.324877
6.890310	373.047713	9.329895
6.944133	396.826626	9.334912
7.168194	390.758221	9.339930
6.864281	398.293949	9.344947
7.162791	392.021457	9.349965
7.377159	382.694785	9.354983
7.256701	398.255148	9.360000
7.125645	399.761930	9.365018
7.301847	395.625917	9.370035
7.461502	402.578257	9.375053
7.567565	391.523372	9.380071
7.290627	380.569149	9.385088
7.262446	376.505986	9.390106
7.126019	368.887494	9.395123
6.989721	374.469021	9.400141
6.735928	371.065803	9.405159
7.171723	396.795386	9.410176
7.036286	388.690762	9.415194
7.354089	396.603037	9.420211
7.265443	395.326250	9.425229
7.270219	386.663337	9.430247
7.579584	395.643532	9.435264
7.411419	389.330098	9.440282
7.306596	391.994072	9.445299
7.136393	402.361685	9.450317
7.012479	392.361879	9.455335
6.957675	390.483407	9.460352
7.099292	395.485210	9.465370
7.332487	400.204526	9.470387
7.124669	392.227930	9.475405
7.203818	393.768252	9.480423
7.403306	391.556712	9.485440
7.166457	403.828088	9.490458
7.488601	391.947493	9.495475
6.967638	395.619796	9.500493
7.041167	382.976382	9.505511
7.526351	402.863505	9.510528
7.782748	407.541343	9.515546
7.773316	401.657603	9.520563
7.514805	397.005480	9.525581
7.257894	397.272756	9.530599
7.383009	388.916137	9.535616
7.400425	395.565589	9.540634
7.303580	396.587387	9.545651
6.725958	406.333662	9.550669
7.315179	396.746657	9.555687
7.737813	419.104939	9.560704
7.425298	406.881358	9.565722
7.365621	407.061124	9.570739
7.207274	423.624591	9.575757
7.337509	422.761825	9.580775
7.463043	425.746526	9.585792
7.270350	422.557836	9.590810
7.378887	418.517556	9.595827
7.510100	423.177021	9.600845
7.581627	424.150516	9.605863
7.663007	420.373227	9.610880
7.330404	427.604181	9.615898
7.594426	424.934487	9.620915
7.632576	422.375697	9.625933
7.741868	414.475943	9.630951
7.628408	421.382456	9.635968
7.721456	422.254775	9.640986
7.793693	418.605135	9.646003
7.291261	416.405055	9.651021
7.434907	410.939269	9.656039
7.188357	417.402621	9.661056
7.476990	420.204145	9.666074
7.796862	412.015998	9.671091
7.588473	422.698821	9.676109
7.779178	422.243186	9.681127
7.547422	416.637041	9.686144
7.477290	426.187553	9.691162
7.809853	421.885185	9.696179
7.755515	425.484842	9.701197
7.749876	418.212021	9.706215
7.704171	430.182269	9.711232
7.407390	429.647907	9.716250
7.665793	414.930825	9.721267
7.728203	423.883216	9.726285
7.471603	419.256034	9.731303
7.674787	417.984299	9.736320
7.220480	420.585931	9.741338
7.548176	411.061728	9.746355
7.616864	417.927256	9.751373
7.503144	418.945372	9.756391
7.501435	417.910655	9.761408
7.819993	423.673828	9.766426
7.721338	421.477148	9.771443
7.799114	423.841311	9.776461
7.374154	420.518380	9.781479
7.964237	433.352112	9.786496
8.167508	440.026289	9.791514
8.216138	416.080034	9.796531
7.601633	426.949162	9.801549
7.549422	423.943716	9.806567
7.610407	421.005849	9.811584
7.514941	426.107687	9.816602
7.819241	433.252102	9.821619
7.751819	451.483400	9.826637
8.123409	446.894096	9.831655
8.047121	444.829624	9.836672
7.722766	440.048892	9.841690
7.854558	432.013090	9.846707
7.661385	438.755304	9.851725
7.878625	438.213490	9.856743
8.051976	447.044482	9.861760
7.956264	445.371180	9.866778
8.039810	437.263996	9.871795
7.731311	438.798409	9.876813
8.017168	446.299134	9.881831
8.033246	438.959810	9.886848
7.885723	436.013381	9.891866
8.183087	417.935775	9.896883
7.820961	426.099085	9.901901
7.775606	430.748176	9.906919
7.924296	438.052514	9.911936
7.978842	440.088952	9.916954
8.224434	425.358078	9.921971
7.761390	428.554334	9.926989
7.737232	435.459570	9.932007
8.234737	436.262606	9.937024
8.065524	444.007744	9.942042
7.839305	417.926880	9.947059
7.599379	439.769840	9.952077
8.146899	441.593831	9.957095
8.262388	442.664618	9.962112
7.985108	450.552811	9.967130
8.203013	449.322960	9.972147
8.215259	450.075324	9.977165
8.001530	441.954465	9.982183
7.753463	443.119725	9.987200
7.899485	451.487939	9.992218
8.321551	445.931458	9.997235
8.074038	450.258596	10.002253
8.049489	444.913657	10.007271
8.057321	455.562835	10.012288
7.934504	448.494430	10.017306
8.368075	441.932661	10.022323
8.351042	454.242427	10.027341
8.290099	448.619144	10.032359
8.071266	447.716057	10.037376
7.911184	451.941224	10.042394
8.421062	449.148045	10.047411
8.375999	453.639313	10.052429
8.150588	446.236605	10.057447
8.253739	434.383767	10.062464
8.019188	432.015750	10.067482
8.173611	431.916040	10.072499
8.086892	431.270081	10.077517
8.166418	445.303569	10.082535
8.323072	441.382018	10.087552
8.317970	454.611377	10.092570
8.168760	448.200301	10.097587
8.020631	447.106333	10.102605
7.813396	454.412448	10.107623
8.292113	445.363306	10.112640
8.108253	449.289232	10.117658
8.253534	448.458834	10.122675
7.932940	452.604857	10.127693
8.143759	451.874703	10.132711
8.269375	442.517639	10.137728
8.241365	451.572480	10.142746
8.228225	449.472930	10.147763
8.496092	447.234959	10.152781
8.452564	455.919851	10.157799
8.418777	450.036732	10.162816
8.478061	455.628856	10.167834
8.612839	448.031217	10.172851
8.403102	445.173364	10.177869
8.080635	452.210256	10.182887
8.436512	445.931969	10.187904
8.129217	454.244538	10.192922
8.090874	456.191304	10.197939
8.427257	455.788722	10.202957
8.286036	459.891039	10.207975
8.807312	451.611559	10.212992
8.592661	463.279946	10.218010
8.437222	458.857899	10.223027
8.698402	464.226095	10.228045
8.228003	457.988095	10.233063
8.318450	450.179618	10.238080
8.518201	456.415714	10.243098
8.331655	459.944448	10.248115
8.217486	464.421234	10.253133
8.131983	463.055594	10.258151
8.467158	452.249008	10.263168
8.435873	457.811055	10.268186
8.098721	457.686901	10.273203
8.162140	456.932362	10.278221
8.779979	477.710899	10.283239
8.682551	476.905666	10.288256
8.551540	477.039737	10.293274
8.265587	462.322168	10.298291
8.612128	464.890632	10.303309
8.463330	480.300851	10.308327
8.775775	475.859598	10.313344
8.870652	474.358580	10.318362
8.316707	448.918805	10.323379
8.415064	465.666395	10.328397
8.196264	468.969790	10.333415
8.818679	477.393225	10.338432
8.849149	474.598949	10.343450
8.617176	475.190531	10.348467
8.605403	477.622290	10.353485
8.612562	487.694107	10.358503
8.882526	481.476519	10.363520
8.754140	479.776743	10.368538
8.496742	470.119554	10.373555
8.956976	479.025811	10.378573
8.759470	478.835735	10.383591
8.524718	467.682395	10.388608
8.456591	467.667826	10.393626
8.683580	477.326732	10.398643
9.134791	482.488630	10.403661
8.690325	480.143823	10.408679
8.483085	458.616715	10.413696
8.585047	467.301050	10.418714
8.636704	469.988007	10.423731
8.727341	479.529294	10.428749
8.550113	484.290445	10.433767
8.810050	472.277477	10.438784
8.637681	477.359747	10.443802
8.938699	472.913962	10.448819
8.685332	478.693621	10.453837
8.736080	478.499605	10.458855
8.743996	477.870466	10.463872
8.739807	478.379248	10.468890
8.587834	478.775347	10.473907
8.784054	479.470666	10.478925
8.552907	479.052310	10.483943
8.686998	474.537845	10.488960
8.334872	478.082896	10.493978
8.659416	474.867311	10.498995
8.652711	478.270223	10.504013
8.552878	495.307462	10.509031
9.033765	504.141091	10.514048
9.023356	501.280595	10.519066
8.903089	509.620872	10.524083
9.133352	500.768169	10.529101
9.086163	511.861429	10.534119
9.168637	496.496359	10.539136
8.957600	485.768486	10.544154
8.996670	478.378231	10.549171
8.882500	474.738669	10.554189
8.785850	480.497083	10.559207
9.011603	481.304564	10.564224
9.095742	481.837462	10.569242
9.136894	489.726583	10.574259
9.144620	476.231853	10.579277
8.812642	479.429801	10.584295
9.179661	482.916531	10.589312
8.911973	485.934065	10.594330
8.788557	479.421137	10.599347
8.918278	489.417070	10.604365
8.746881	507.509987	10.609383
8.805489	500.782526	10.614400
9.260270	502.008764	10.619418
9.123215	509.102012	10.624435
9.292555	513.137054	10.629453
9.092331	516.033641	10.634471
9.094684	506.235009	10.639488
9.377301	504.622711	10.644506
9.162420	507.991772	10.649523
9.390710	502.443355	10.654541
9.278772	502.457697	10.659559
9.299396	493.290514	10.664576
9.235309	478.573100	10.669594
9.016342	486.269201	10.674611
8.897233	478.193551	10.679629
8.944767	491.689284	10.684647
8.943754	499.733291	10.689664
9.334710	503.629690	10.694682
9.006204	506.505224	10.699699
9.096494	503.070498	10.704717
9.451807	514.587062	10.709735
9.054004	501.808675	10.714752
9.102553	506.651439	10.719770
8.895864	507.523095	10.724787
8.913586	510.142761	10.729805
8.996886	508.081836	10.734823
8.802618	502.056435	10.739840
9.274321	499.562669	10.744858
9.189728	510.690153	10.749875
9.176354	508.202486	10.754893
9.485098	525.053069	10.759911
9.533459	515.105263	10.764928
9.455135	511.983953	10.769946
9.196884	522.188627	10.774963
9.193523	509.718033	10.779981
9.067684	517.453294	10.784999
9.268620	529.012838	10.790016
9.718660	533.954037	10.795034
9.452187	532.616569	10.800051
9.498517	514.767290	10.805069
9.155636	522.678351	10.810087
9.200046	530.030519	10.815104
9.706430	534.448572	10.820122
9.410577	535.681235	10.825139
9.621768	537.201012	10.830157
9.022277	526.363188	10.835175
9.137751	530.457112	10.840192
9.753863	541.664858	10.845210
9.747935	539.882897	10.850227
9.673927	526.419789	10.855245
9.334243	528.577575	10.860263
9.340894	525.777533	10.865280
9.622929	526.184950	10.870298
9.713873	536.609807	10.875315
9.604518	516.503218	10.880333
9.570960	512.939456	10.885351
9.513134	506.208032	10.890368
9.330378	507.069651	10.895386
9.395551	521.607185	10.900403
9.830005	522.899702	10.905421
9.556258	527.136274	10.910439
9.589855	539.450838	10.915456
9.882376	525.510959	10.920474
9.888229	527.299380	10.925491
9.506520	511.384903	10.930509
9.658604	520.238178	10.935527
9.492041	517.553464	10.940544
9.472397	513.719304	10.945562
9.345650	522.628615	10.950579
9.703983	531.954689	10.955597
9.763280	531.753031	10.960615
9.920772	535.770989	10.965632
9.980087	533.612813	10.970650
9.610134	528.794977	10.975667
9.476660	513.343601	10.980685
9.476559	522.766501	10.985703
9.606433	526.902361	10.990720
9.614885	529.902154	10.995738
9.475903	536.361424	11.000755
9.558610	533.350731	11.005773
9.819337	538.346652	11.010791
9.605814	534.511117	11.015808
10.156070	535.359591	11.020826
9.951158	535.666107	11.025843
9.962100	542.872020	11.030861
9.637555	536.115843	11.035879
9.540765	536.598021	11.040896
9.682896	534.805631	11.045914
9.142867	536.647488	11.050931
9.652161	537.808440	11.055949
9.747636	538.102899	11.060967
9.658727	537.349984	11.065984
10.088153	534.386290	11.071002
9.844512	536.734242	11.076019
9.725211	539.936956	11.081037
9.902933	530.413949	11.086055
9.530817	544.025551	11.091072
10.588844	543.068815	11.096090
10.090411	536.062013	11.101107
9.891209	531.571026	11.106125
10.224578	534.422404	11.111143
9.867840	530.949981	11.116160
10.136820	527.345423	11.121178
9.743239	543.077818	11.126195
9.954743	531.794999	11.131213
9.915640	536.755555	11.136231
10.078237	532.274506	11.141248
10.045680	536.962655	11.146266
9.895391	538.475599	11.151283
10.015323	524.253337	11.156301
9.874017	536.642467	11.161319
9.754386	529.396816	11.166336
10.099659	535.146399	11.171354
10.081182	556.753061	11.176371
10.284149	558.911565	11.181389
10.172901	545.365881	11.186407
9.974429	538.987688	11.191424
10.111478	540.096149	11.196442
10.308290	538.755972	11.201459
9.980909	546.857126	11.206477
9.916049	549.066796	11.211495
9.945586	560.744562	11.216512
10.404920	554.364926	11.221530
10.784257	563.987536	11.226547
10.355311	550.677498	11.231565
10.083935	537.778419	11.236583
9.668474	543.009004	11.241600
10.307555	547.163413	11.246618
10.550984	548.943247	11.251635
10.111007	550.217285	11.256653
9.970256	542.697218	11.261671
10.043271	548.388215	11.266688
10.362966	555.729089	11.271706
9.949566	561.322261	11.276723
9.989997	565.311117	11.281741
10.499256	554.366917	11.286759
10.683140	562.647240	11.291776
10.169334	554.765547	11.296794
10.256070	562.284701	11.301811
10.242986	556.439347	11.306829
10.721974	555.194085	11.311847
10.256797	562.644542	11.316864
10.427668	559.134145	11.321882
10.515505	563.169266	11.326899
10.169531	565.511065	11.331917
10.552638	559.260056	11.336935
10.480235	561.814870	11.341952
10.030661	566.476441	11.346970
10.101762	558.689862	11.351987
10.560952	562.641919	11.357005
10.596853	554.753530	11.362023
10.121023	558.942681	11.367040
10.237959	557.334085	11.372058
10.067912	565.249811	11.377075
9.764674	563.305864	11.382093
10.238792	561.329244	11.387111
10.119747	559.533336	11.392128
10.519420	572.491486	11.397146
10.430633	588.372117	11.402163
10.660363	587.212997	11.407181
10.938359	581.173998	11.412199
10.495616	577.939008	11.417216
10.366842	560.776483	11.422234
10.603614	570.954602	11.427251
10.516113	565.250214	11.432269
10.421337	577.086195	11.437287
10.432242	572.616131	11.442304
10.912741	581.806451	11.447322
10.749322	586.079504	11.452339
10.443202	590.538873	11.457357
11.087657	575.619546	11.462375
10.769689	565.103925	11.467392
10.634730	553.903436	11.472410
10.835501	566.008962	11.477427
10.297110	566.279042	11.482445
10.945280	557.601074	11.487463
10.538623	561.028406	11.492480
10.670128	563.826016	11.497498
10.540044	563.597040	11.502515
10.254841	574.506500	11.507533
11.026814	579.722622	11.512551
10.833839	586.490106	11.517568
10.860907	586.441782	11.522586
11.172258	583.341835	11.527603
10.510174	573.340516	11.532621
10.666783	564.385645	11.537639
10.688943	574.366816	11.542656
10.938759	571.276452	11.547674
10.847531	570.460783	11.552691
10.650004	561.977600	11.557709
10.888307	571.445455	11.562727
10.737249	582.400302	11.567744
10.749968	582.635067	11.572762
10.847515	592.673936	11.577779
10.783344	593.504473	11.582797
10.751631	590.095036	11.587815
11.068321	592.554562	11.592832
11.064235	583.883466	11.597850
11.114376	590.458471	11.602867
10.594821	588.731230	11.607885
10.772174	585.289243	11.612903
10.224536	598.284456	11.617920
10.770691	584.907776	11.622938
10.673481	587.725221	11.627955
10.203612	584.049504	11.632973
10.852065	599.588150	11.637991
11.164937	606.264260	11.643008
11.125004	608.826648	11.648026
11.396702	604.274947	11.653043
11.335542	597.802773	11.658061
11.046139	593.609825	11.663079
10.862904	592.647541	11.668096
10.975457	592.970899	11.673114
11.224665	588.747739	11.678131
10.934088	596.088978	11.683149
11.164313	587.744301	11.688167
11.261753	585.179413	11.693184
10.861637	581.505458	11.698202
10.944725	590.552539	11.703219
11.368288	606.154607	11.708237
11.489853	597.000057	11.713255
10.884849	591.622377	11.718272
10.989131	590.328160	11.723290
11.327357	583.897945	11.728307
10.769221	590.539256	11.733325
11.389723	592.336122	11.738343
11.621904	603.581594	11.743360
11.219846	595.029258	11.748378
11.119555	589.907498	11.753395
10.614290	596.988686	11.758413
11.175026	602.736301	11.763431
11.298779	612.064228	11.768448
11.045426	616.528010	11.773466
11.404217	618.106860	11.778483
11.021197	612.928132	11.783501
11.412435	601.314340	11.788519
11.113776	613.068485	11.793536
11.240110	612.749094	11.798554
11.327275	605.736292	11.803571
11.315252	609.307308	11.808589
11.199227	605.529158	11.813607
11.151457	608.597675	11.818624
11.424274	599.886614	11.823642
11.307157	605.127568	11.828659
11.360978	614.169751	11.833677
11.395778	611.049744	11.838695
11.574094	603.120226	11.843712
11.144214	604.064505	11.848730
11.425097	607.208079	11.853747
10.876202	608.827271	11.858765
11.013325	608.080184	11.863783
11.422234	619.235036	11.868800
11.582864	625.953791	11.873818
11.869679	621.936198	11.878835
11.581967	638.927090	11.883853
11.866699	629.459951	11.888871
11.910372	619.276140	11.893888
11.951390	607.136227	11.898906
11.478219	611.555341	11.903923
11.289438	609.505208	11.908941
11.582637	607.458926	11.913959
11.587709	605.040954	11.918976
11.345296	609.203241	11.923994
11.400601	608.440492	11.929011
11.147821	615.605447	11.934029
11.542385	621.268492	11.939047
12.053239	624.874861	11.944064
11.723999	631.559440	11.949082
11.945098	628.009652	11.954099
11.777546	627.726552	11.959117
11.935240	605.706963	11.964135
11.918182	598.410601	11.969152
11.802922	605.494183	11.974170
11.730857	598.184295	11.979187
11.584677	611.132790	11.984205
11.817826	609.547120	11.989223
11.576387	615.605821	11.994240
11.221030	607.014651	11.999258
11.734967	614.281128	12.004275
11.689949	625.090108	12.009293
11.746014	626.012375	12.014311
12.018312	630.946563	12.019328
11.642477	636.603334	12.024346
12.279386	634.434109	12.029363
11.751766	621.912524	12.034381
11.757449	619.768999	12.039399
11.802772	629.569877	12.044416
11.650702	631.225112	12.049434
11.886681	624.192288	12.054451
11.756775	636.210497	12.059469
11.760673	627.168922	12.064487
12.154526	627.420082	12.069504
12.040858	630.249564	12.074522
12.042868	627.333467	12.079539
11.973426	629.733202	12.084557
11.849173	629.591677	12.089575
12.320250	625.801005	12.094592
12.291204	632.224259	12.099610
12.293133	617.720505	12.104627
11.928355	605.962497	12.109645
12.429771	604.092071	12.114663
12.291826	600.569790	12.119680
12.081936	605.272945	12.124698
12.148088	596.489925	12.129715
12.039044	605.882496	12.134733
12.004834	599.775340	12.139751
11.768781	604.889651	12.144768
12.057703	604.134708	12.149786
12.083521	605.090084	12.154803
11.752816	602.099567	12.159821
12.279465	614.283770	12.164839
12.050969	611.545571	12.169856
12.283174	622.743716	12.174874
12.349553	608.381408	12.179891
12.178077	614.662736	12.184909
12.044165	602.433302	12.189927
12.310239	623.446653	12.194944
11.943229	616.368865	12.199962
12.378175	617.115381	12.204979
12.117664	625.423901	12.209997
12.085385	623.573454	12.215015
12.258673	626.768496	12.220032
12.159807	629.904930	12.225050
12.541648	629.397440	12.230067
12.654483	628.303853	12.235085
12.512748	620.824930	12.240103
12.378566	608.279965	12.245120
12.318343	612.751544	12.250138
12.616471	613.241662	12.255155
12.280068	617.800422	12.260173
12.066172	611.500341	12.265191
12.453459	607.792143	12.270208
12.268299	622.428693	12.275226
12.410535	624.063351	12.280243
12.468001	625.815344	12.285261
12.452671	626.385823	12.290279
12.584415	624.648688	12.295296
12.375438	636.925352	12.300314
12.315041	629.995473	12.305331
12.230096	627.935483	12.310349
12.351914	629.813152	12.315367
12.517952	629.348730	12.320384
12.435319	628.219307	12.325402
12.622793	638.083260	12.330419
12.312767	638.384054	12.335437
12.619505	638.106000	12.340455
12.674833	627.257677	12.345472
12.296781	632.005955	12.350490
12.235471	624.123203	12.355507
12.587164	640.755778	12.360525
12.605440	633.936720	12.365543
12.557598	629.027681	12.370560
12.250221	634.074213	12.375578
12.211137	636.645940	12.380595
12.483973	650.545355	12.385613
12.661422	653.966963	12.390631
13.078669	645.034585	12.395648
12.655182	657.969487	12.400666
12.672065	651.586125	12.405683
12.620936	654.320670	12.410701
12.789244	664.913430	12.415719
12.597851	654.412762	12.420736
12.652404	656.436601	12.425754
12.775566	654.984811	12.430771
12.469115	657.538212	12.435789
12.878683	658.194009	12.440807
12.916993	652.754017	12.445824
12.749129	657.150852	12.450842
13.085312	656.095069	12.455859
12.923012	656.843061	12.460877
12.668570	659.208489	12.465895
13.068754	658.764412	12.470912
13.034428	665.709189	12.475930
12.471988	667.702866	12.480947
12.948648	654.671457	12.485965
13.038443	651.161042	12.490983
12.979895	645.016636	12.496000
12.779993	649.610954	12.501018
12.786184	647.947012	12.506035
12.872448	650.215212	12.511053
12.877624	653.572128	12.516071
13.158232	648.084945	12.521088
12.775517	659.593441	12.526106
13.046082	658.595211	12.531123
13.093588	659.544057	12.536141
13.317455	655.801336	12.541159
13.198447	654.570281	12.546176
13.139805	656.305643	12.551194
13.090033	639.875483	12.556211
12.937640	646.018157	12.561229
12.863680	659.589736	12.566247
12.893640	659.739769	12.571264
13.100798	659.291033	12.576282
12.966066	669.852087	12.581299
12.915511	655.413277	12.586317
12.908669	660.801174	12.591335
13.184016	658.571479	12.596352
12.922744	660.922193	12.601370
13.302962	662.169519	12.606387
13.215066	670.709951	12.611405
12.791996	677.043096	12.616423
13.240148	673.599954	12.621440
13.106682	688.679774	12.626458
12.983990	688.190879	12.631475
13.712466	674.668984	12.636493
13.558974	681.300973	12.641511
13.562505	682.177775	12.646528
13.299751	684.074303	12.651546
13.410795	675.880681	12.656563
13.611672	672.185715	12.661581
13.293197	667.375604	12.666599
13.487006	654.741672	12.671616
13.135259	660.075975	12.676634
13.186795	662.579950	12.681651
12.968797	676.445358	12.686669
13.014783	684.709340	12.691687
13.053601	675.046943	12.696704
13.235626	681.494154	12.701722
12.953582	678.174168	12.706739
13.225961	688.716026	12.711757
13.085989	693.518768	12.716775
13.337295	696.856304	12.721792
13.612370	700.726609	12.726810
13.377314	700.211029	12.731827
13.619464	704.982679	12.736845
13.736251	715.214275	12.741863
13.595669	705.425164	12.746880
13.891514	708.777859	12.751898
13.726229	710.580321	12.756915
13.936231	707.436174	12.761933
13.603328	696.017116	12.766951
13.270931	682.303796	12.771968
13.760561	693.758541	12.776986
13.955347	709.295337	12.782003
13.880764	693.560089	12.787021
13.753149	686.681678	12.792039
13.601153	674.297225	12.797056
14.049910	688.235549	12.802074
13.467189	681.645741	12.807091
13.654110	674.456439	12.812109
13.265817	688.787012	12.817127
13.489136	691.481987	12.822144
13.656163	696.520943	12.827162
13.648937	704.597567	12.832179
13.917553	701.516876	12.837197
13.930862	707.195130	12.842215
13.873627	712.098599	12.847232
14.181970	709.469298	12.852250
14.025752	700.187537	12.857267
14.175760	705.936021	12.862285
13.899797	695.151860	12.867303
13.762873	690.225117	12.872320
13.821245	702.772614	12.877338
13.503172	712.967777	12.882355
13.917572	708.665222	12.887373
13.900265	704.003864	12.892391
14.025044	702.097398	12.897408
13.811868	707.814070	12.902426
14.034992	702.354755	12.907443
13.949589	702.491193	12.912461
13.963272	712.975518	12.917479
14.208567	699.494121	12.922496
14.052379	708.954045	12.927514
13.865872	709.402861	12.932531
14.246438	702.480034	12.937549
13.727550	710.298664	12.942567
13.646012	714.243430	12.947584
13.837686	710.152271	12.952602
13.720848	715.475263	12.957619
14.106094	714.787366	12.962637
14.317487	729.371729	12.967655
14.155916	721.182663	12.972672
14.096707	715.079359	12.977690
14.042162	732.336984	12.982707
14.437425	722.726358	12.987725
14.096331	735.377098	12.992743
14.047307	732.405817	12.997760
14.580236	733.537856	13.002778
14.411782	727.363198	13.007795
14.620110	716.030266	13.012813
14.175088	716.481463	13.017831
14.256616	716.260563	13.022848
14.306504	705.397260	13.027866
14.219631	723.855920	13.032883
14.580653	708.377873	13.037901
14.340085	715.465230	13.042919
14.210440	716.492153	13.047936
14.273014	720.420794	13.052954
14.130669	732.958539	13.057971
14.649992	728.828985	13.062989
14.813691	729.415773	13.068007
13.880186	732.600128	13.073024
14.409798	730.324525	13.078042
14.257592	739.723886	13.083059
14.587141	722.458288	13.088077
14.345500	729.981305	13.093095
14.619604	744.555916	13.098112
14.545442	738.234033	13.103130
14.253916	743.404356	13.108147
14.811944	746.684680	13.113165
14.612140	743.386589	13.118183
14.653088	733.739607	13.123200
14.423411	730.152690	13.128218
14.348347	742.941890	13.133235
14.509202	738.959661	13.138253
14.771221	732.411875	13.143271
14.509699	731.840456	13.148288
14.524682	736.092080	13.153306
14.432032	736.409522	13.158323
14.682558	728.490795	13.163341
14.540005	742.511759	13.168359
14.572934	737.792080	13.173376
14.800676	735.916915	13.178394
14.285046	740.421563	13.183411
14.936843	745.028461	13.188429
14.781125	746.494932	13.193447
14.909110	750.356593	13.198464
14.895225	735.217753	13.203482
14.535714	740.477552	13.208499
14.918884	755.268713	13.213517
14.957796	745.420077	13.218535
14.972871	751.839660	13.223552
14.958966	740.800082	13.228570
14.698567	740.332626	13.233587
14.875080	741.996670	13.238605
15.086062	752.276736	13.243623
15.176348	757.614826	13.248640
15.014016	746.885523	13.253658
14.657471	746.852745	13.258675
15.109203	749.291267	13.263693
15.074965	752.212540	13.268711
14.777515	748.506787	13.273728
15.158265	752.329093	13.278746
15.053361	761.342416	13.283763
15.030254	754.820080	13.288781
15.388467	761.628040	13.293799
14.779571	750.551710	13.298816
15.022160	747.825348	13.303834
15.123931	753.906396	13.308851
15.233121	755.192771	13.313869
15.343188	757.501460	13.318887
14.899995	760.700995	13.323904
15.120301	760.878195	13.328922
14.930320	765.710832	13.333939
15.122041	754.904309	13.338957
15.632566	762.821454	13.343975
15.639562	759.118788	13.348992
15.679020	750.955212	13.354010
15.389383	747.431273	13.359027
14.997115	748.126714	13.364045
15.050238	740.194538	13.369063
15.239226	756.862021	13.374080
15.116806	758.604167	13.379098
15.265470	762.983302	13.384115
15.426799	763.822917	13.389133
15.339301	770.712899	13.394151
15.196877	770.160804	13.399168
15.381980	761.911432	13.404186
15.190314	775.665523	13.409203
15.413051	766.924309	13.414221
15.478091	771.477408	13.419239
15.072568	767.917861	13.424256
15.249720	755.699848	13.429274
15.281243	763.618991	13.434291
14.995671	762.221365	13.439309
15.263910	762.889704	13.444327
14.870618	766.914578	13.449344
15.104618	779.658840	13.454362
15.347086	790.849181	13.459379
15.270081	784.016499	13.464397
15.648353	792.796824	13.469415
15.867365	788.515204	13.474432
16.086183	779.067715	13.479450
15.919867	783.783067	13.484467
15.629327	797.445274	13.489485
15.899126	793.714307	13.494503
15.728242	793.037258	13.499520
15.871093	784.472572	13.504538
15.821919	787.569740	13.509555
15.768603	786.984836	13.514573
16.055127	786.763574	13.519591
15.446926	776.643300	13.524608
15.528060	783.832070	13.529626
15.589089	791.708763	13.534643
15.823535	793.733011	13.539661
15.813118	789.818462	13.544679
15.635686	792.837773	13.549696
15.673982	784.008507	13.554714
15.391484	784.579564	13.559731
15.569166	784.334225	13.564749
15.763332	789.791847	13.569767
15.920407	791.664044	13.574784
16.044780	792.922812	13.579802
15.740224	791.887890	13.584819
15.793982	788.452485	13.589837
15.918458	791.642534	13.594855
15.758787	795.672064	13.599872
16.255043	798.160464	13.604890
16.274673	793.546978	13.609907
15.911144	793.376437	13.614925
16.233427	790.006517	13.619943
15.588797	785.016789	13.624960
16.068375	800.133794	13.629978
16.347029	801.340140	13.634995
16.132644	802.632719	13.640013
16.083594	799.071312	13.645031
16.267167	803.069492	13.650048
16.325285	794.975571	13.655066
15.938971	791.021721	13.660083
16.384056	800.350208	13.665101
16.347238	790.699525	13.670119
16.057299	779.870152	13.675136
15.756305	782.394319	13.680154
15.916454	789.655993	13.685171
16.079288	804.364740	13.690189
16.150544	797.556305	13.695207
15.923935	807.273390	13.700224
16.008859	802.397279	13.705242
16.066031	810.508104	13.710259
16.085609	800.870725	13.715277
16.200757	799.429639	13.720295
16.067781	818.223768	13.725312
16.508008	825.732176	13.730330
16.422701	822.255302	13.735347
16.532674	831.377213	13.740365
16.684394	825.799593	13.745383
16.611360	831.535509	13.750400
16.822627	812.622020	13.755418
16.688792	815.401024	13.760435
16.268153	808.524008	13.765453
16.317408	805.335446	13.770471
16.697902	812.240940	13.775488
16.136101	802.466867	13.780506
16.638007	821.215798	13.785523
16.667859	825.641849	13.790541
17.143958	815.463180	13.795559
16.523347	804.944046	13.800576
16.583925	805.174518	13.805594
17.116118	798.606732	13.810611
16.482292	808.961561	13.815629
17.191658	802.492417	13.820647
16.800127	809.183605	13.825664
16.560753	796.572837	13.830682
16.520077	810.660042	13.835699
16.468566	804.328298	13.840717
16.590584	799.828254	13.845735
16.518827	808.991070	13.850752
16.653385	804.836201	13.855770
16.638184	824.590273	13.860787
16.551476	822.849262	13.865805
17.239029	823.256664	13.870823
16.935163	831.306949	13.875840
17.221223	823.044986	13.880858
16.957254	808.774975	13.885875
16.553132	808.815875	13.890893
17.069120	816.495514	13.895911
17.301352	821.028905	13.900928
16.968725	818.445739	13.905946
17.203487	802.965179	13.910963
16.450753	806.080376	13.915981
17.179605	804.221855	13.920999
17.109967	813.207624	13.926016
16.954091	816.482351	13.931034
17.170771	821.781848	13.936051
16.994047	812.913464	13.941069
16.989694	813.750476	13.946087
17.314725	829.885620	13.951104
17.130707	831.545848	13.956122
17.115970	826.656845	13.961139
16.982008	829.262307	13.966157
17.196148	823.188988	13.971175
17.327976	825.989745	13.976192
17.167339	829.814311	13.981210
17.381529	831.548235	13.986227
16.916399	833.103912	13.991245
17.316972	829.336798	13.996263
17.558598	832.603286	14.001280
17.274294	836.352437	14.006298
17.424429	826.041482	14.011315
16.987749	840.562742	14.016333
17.244477	827.937825	14.021351
17.219077	836.683194	14.026368
17.391374	843.365502	14.031386
17.448023	828.168266	14.036403
17.232188	838.126681	14.041421
17.372701	826.763214	14.046439
17.187683	827.432701	14.051456
17.155260	827.362081	14.056474
17.491456	829.714464	14.061491
17.277480	832.963527	14.066509
17.212668	829.092152	14.071527
17.327722	832.539288	14.076544
17.129796	836.375973	14.081562
17.595786	847.058191	14.086579
17.595845	863.426994	14.091597
17.641596	854.855302	14.096615
17.399948	866.872129	14.101632
17.423545	855.394306	14.106650
17.601401	860.573630	14.111667
17.690960	847.924235	14.116685
17.733169	852.846972	14.121703
17.979323	846.203787	14.126720
17.675479	859.334796	14.131738
17.609570	860.219263	14.136755
17.506487	862.169842	14.141773
17.501377	853.195825	14.146791
17.788841	859.648774	14.151808
17.728388	847.698061	14.156826
17.534305	845.986389	14.161843
17.890719	859.393285	14.166861
17.906195	848.986521	14.171879
17.735563	854.425224	14.176896
17.596345	851.518457	14.181914
17.842327	849.918144	14.186931
17.999358	855.299519	14.191949
18.050959	849.343015	14.196967
17.716833	856.167290	14.201984
17.747534	856.544422	14.207002
17.638723	847.517128	14.212019
18.002501	865.426099	14.217037
18.033773	861.243118	14.222055
18.199384	875.957803	14.227072
18.163553	879.286433	14.232090
18.166325	870.999129	14.237107
17.959098	878.696726	14.242125
17.981065	875.177894	14.247143
18.147108	878.560297	14.252160
18.510393	877.800077	14.257178
18.493258	866.382236	14.262195
18.120286	856.461971	14.267213
17.918166	851.381236	14.272231
18.051485	857.397449	14.277248
18.037438	866.724875	14.282266
18.075840	865.160036	14.287283
18.214611	879.074192	14.292301
18.489812	871.381929	14.297319
18.422436	873.705637	14.302336
18.469765	882.275607	14.307354
18.634794	872.303126	14.312371
18.625631	876.135675	14.317389
18.210232	867.317048	14.322407
18.232856	863.766558	14.327424
17.615479	875.829269	14.332442
17.910954	868.821798	14.337459
18.080320	880.512716	14.342477
18.113126	875.613142	14.347495
18.563933	876.499208	14.352512
18.262636	883.040678	14.357530
18.297829	880.416013	14.362547
18.276436	895.462779	14.367565
18.518860	894.569901	14.372583
18.667258	896.067927	14.377600
18.565859	896.358333	14.382618
18.545609	897.368233	14.387635
18.676217	895.347233	14.392653
18.570654	892.214319	14.397671
18.331500	893.687481	14.402688
18.379045	896.697027	14.407706
18.717118	896.581345	14.412723
18.288617	895.805550	14.417741
18.638932	892.144075	14.422759
19.041760	894.340929	14.427776
18.935112	902.139639	14.432794
18.644218	902.399589	14.437811
18.748269	903.926611	14.442829
18.706550	891.897214	14.447847
18.911181	896.513815	14.452864
18.291398	900.564515	14.457882
18.740389	908.074749	14.462899
18.776244	916.520293	14.467917
18.920126	929.613202	14.472935
19.035364	923.507912	14.477952
19.166095	921.026152	14.482970
19.201263	922.298819	14.487987
19.201373	924.892887	14.493005
18.805889	919.611870	14.498023
19.095188	902.099906	14.503040
19.530460	919.959932	14.508058
19.264785	898.839013	14.513075
19.192161	892.213886	14.518093
19.421936	890.770724	14.523111
19.374408	883.949193	14.528128
19.301187	888.132537	14.533146
19.230690	897.124794	14.538163
19.288816	894.357703	14.543181
18.850866	891.753056	14.548199
19.037521	885.317930	14.553216
19.103999	884.648102	14.558234
19.027673	895.256999	14.563251
18.886202	891.511151	14.568269
19.197584	904.398085	14.573287
19.368659	907.760777	14.578304
19.223243	917.673559	14.583322
19.338059	910.063054	14.588339
19.720756	911.291078	14.593357
19.164417	917.708172	14.598375
18.883082	906.968899	14.603392
19.128847	912.216558	14.608410
19.364432	921.372605	14.613427
19.429052	913.094586	14.618445
19.198121	926.321587	14.623463
19.488748	920.255261	14.628480
19.015943	924.974188	14.633498
19.383225	910.668927	14.638515
19.687818	917.693574	14.643533
19.341395	922.610569	14.648551
20.100575	918.232193	14.653568
19.440050	925.135715	14.658586
19.744267	912.828385	14.663603
19.715351	918.137748	14.668621
19.354698	920.750116	14.673639
19.444940	925.109985	14.678656
19.490909	936.400439	14.683674
19.926984	935.991793	14.688691
20.222663	942.471895	14.693709
19.567845	934.113380	14.698727
19.803721	926.452462	14.703744
19.924196	936.794062	14.708762
19.931589	928.878388	14.713779
19.677541	931.720307	14.718797
19.846607	942.092214	14.723815
19.621467	937.324301	14.728832
19.671418	937.875159	14.733850
20.489227	941.443269	14.738867
20.365968	940.370643	14.743885
19.587306	935.067232	14.748903
20.263687	924.298753	14.753920
20.061375	938.184011	14.758938
19.960743	936.085404	14.763955
20.032423	933.770623	14.768973
20.039856	934.536380	14.773991
20.322017	935.578091	14.779008
19.945967	935.437899	14.784026
20.112104	931.369600	14.789043
20.124381	935.268251	14.794061
19.870136	936.365077	14.799079
20.144180	936.546536	14.804096
20.451905	935.387874	14.809114
20.199134	933.107831	14.814131
20.234135	933.219213	14.819149
20.128967	939.764880	14.824167
20.242355	932.874096	14.829184
20.045751	943.034699	14.834202
20.027239	935.867810	14.839219
20.034104	941.401977	14.844237
20.016976	943.430698	14.849255
20.057845	932.660178	14.854272
20.002525	946.976983	14.859290
20.442143	944.185202	14.864307
20.314669	953.678653	14.869325
20.395125	954.111155	14.874343
20.492996	960.521078	14.879360
20.762693	969.826470	14.884378
20.782704	965.733579	14.889395
20.586086	953.914446	14.894413
20.367342	943.619832	14.899431
20.617676	946.995436	14.904448
20.363633	941.064399	14.909466
20.516398	948.573435	14.914483
20.643676	953.214718	14.919501
20.819289	968.868333	14.924519
20.931041	954.138927	14.929536
20.789083	953.716139	14.934554
21.076978	961.024265	14.939571
20.818671	940.760511	14.944589
20.020363	934.791142	14.949607
20.568740	943.090630	14.954624
20.820693	960.108254	14.959642
20.597907	958.536737	14.964659
20.842706	950.123353	14.969677
20.838488	959.234706	14.974695
20.921767	958.934637	14.979712
20.685361	956.828764	14.984730
20.704958	954.203360	14.989747
21.042907	954.343312	14.994765
20.795619	957.335659	14.999783
20.644134	950.328320	15.004800
20.913027	962.309903	15.009818
20.956021	965.023529	15.014835
20.740338	954.160399	15.019853
20.837725	953.419484	15.024871
20.641496	970.308087	15.029888
21.228304	985.714662	15.034906
21.107165	988.734709	15.039923
21.712272	977.159957	15.044941
21.115033	984.391313	15.049959
21.644694	975.860982	15.054976
21.463410	972.686195	15.059994
21.290802	964.763818	15.065011
21.401142	958.201696	15.070029
21.279170	957.545427	15.075047
21.330051	953.031174	15.080064
21.466687	956.904155	15.085082
21.180079	954.354828	15.090099
21.090186	959.620049	15.095117
20.854358	965.116273	15.100135
21.394603	969.387155	15.105152
21.469696	983.109339	15.110170
21.214627	987.775448	15.115187
21.245209	982.409140	15.120205
21.522344	985.386111	15.125223
21.725374	978.897910	15.130240
21.683043	975.568947	15.135258
21.325495	979.013956	15.140275
21.637756	969.425588	15.145293
21.484872	984.657002	15.150311
21.568287	972.762698	15.155328
21.360934	980.277326	15.160346
21.580668	981.827368	15.165363
21.605840	980.659047	15.170381
21.822718	973.180944	15.175399
21.591672	978.726919	15.180416
21.883987	979.760741	15.185434
21.633478	977.868497	15.190451
21.733157	969.127410	15.195469
21.603031	979.650061	15.200487
21.973255	972.075501	15.205504
21.520464	976.065504	15.210522
21.519603	982.736956	15.215539
21.737279	973.235895	15.220557
21.682210	985.555106	15.225575
21.803138	980.891087	15.230592
21.921829	988.607413	15.235610
21.687404	1003.046822	15.240627
22.308733	1000.482356	15.245645
22.060963	1002.297690	15.250663
21.931458	1005.596747	15.255680
22.500257	1000.837745	15.260698
22.108155	987.284962	15.265715
22.537776	975.223146	15.270733
22.007297	974.772488	15.275751
22.246725	977.960452	15.280768
22.096021	971.738765	15.285786
22.034073	973.884918	15.290803
22.050064	973.131431	15.295821
22.037756	988.596576	15.300839
22.155130	995.527329	15.305856
22.132290	994.451688	15.310874
22.257545	1001.646300	15.315891
22.345593	992.664020	15.320909
22.389179	998.467037	15.325927
22.181872	998.622458	15.330944
22.393219	999.643641	15.335962
22.415189	1003.597601	15.340979
22.081576	995.491999	15.345997
22.219447	1001.810504	15.351015
22.085869	1001.717764	15.356032
22.330685	992.846772	15.361050
22.182964	1003.735088	15.366067
22.140614	1000.014810	15.371085
22.167892	1014.504998	15.376103
22.588564	1022.265839	15.381120
23.080070	1015.701153	15.386138
22.696388	1030.599317	15.391155
22.936942	1023.417304	15.396173
22.818700	1018.077313	15.401191
22.242628	1007.964527	15.406208
22.475310	1018.661082	15.411226
22.641110	1021.469204	15.416243
22.846435	1028.553532	15.421261
22.906185	1029.803444	15.426279
22.805156	1034.477139	15.431296
23.150612	1020.465517	15.436314
23.063535	1022.233743	15.441331
22.873747	1025.166656	15.446349
22.972493	1021.496987	15.451367
22.940098	1030.344525	15.456384
23.378514	1021.635878	15.461402
22.597524	1019.681059	15.466419
23.011981	1008.252733	15.471437
22.805453	1023.729213	15.476455
23.113317	1020.162683	15.481472
23.244751	1023.547348	15.486490
22.966784	1028.920765	15.491507
23.100701	1024.775412	15.496525
23.029634	1019.093566	15.501543
22.639525	1017.576497	15.506560
22.897647	1019.483478	15.511578
22.633838	1031.582760	15.516595
22.889723	1022.154618	15.521613
22.827354	1025.998639	15.526631
22.722342	1028.811058	15.531648
23.320327	1037.901273	15.536666
23.530384	1038.512411	15.541683
23.619368	1038.770021	15.546701
23.368232	1024.453658	15.551719
23.281675	1023.043959	15.556736
23.364364	1011.534745	15.561754
23.463565	1012.936301	15.566771
23.289325	1013.616740	15.571789
23.419124	1031.382431	15.576807
23.785869	1042.736615	15.581824
23.497964	1035.296055	15.586842
23.553816	1025.327863	15.591859
23.620946	1014.811976	15.596877
23.364725	1020.705861	15.601895
23.384503	1037.163270	15.606912
23.470627	1038.866662	15.611930
23.705974	1039.322387	15.616947
23.693001	1043.082983	15.621965
23.485278	1048.981949	15.626983
23.435284	1036.622387	15.632000
24.106171	1035.372462	15.637018
23.882945	1039.159482	15.642035
23.870327	1044.987044	15.647053
24.083433	1042.921625	15.652071
24.088056	1045.461360	15.657088
23.667753	1048.562709	15.662106
23.810870	1051.869821	15.667123
23.926497	1039.651726	15.672141
23.975410	1039.287579	15.677159
23.933222	1045.713028	15.682176
24.239873	1037.952681	15.687194
23.729516	1052.586568	15.692211
23.724504	1037.007440	15.697229
23.633468	1037.719105	15.702247
23.564712	1045.575093	15.707264
23.875880	1038.180111	15.712282
23.777939	1044.797274	15.717299
23.592214	1042.380548	15.722317
23.816380	1057.935165	15.727335
24.186891	1062.399752	15.732352
24.479513	1054.496417	15.737370
24.167560	1066.306577	15.742387
24.286367	1065.246747	15.747405
24.541607	1059.889619	15.752423
24.205008	1069.071714	15.757440
24.657325	1068.035696	15.762458
24.691648	1060.317740	15.767475
24.653102	1050.058123	15.772493
24.353087	1041.836817	15.777511
24.099284	1037.979042	15.782528
24.472247	1039.678799	15.787546
24.498537	1053.582202	15.792563
24.641164	1064.065592	15.797581
24.706208	1055.370881	15.802599
24.438694	1052.654467	15.807616
24.437542	1043.670270	15.812634
24.120822	1049.415796	15.817651
24.370418	1058.765389	15.822669
24.616249	1057.912997	15.827687
24.414044	1063.883691	15.832704
24.505437	1057.188785	15.837722
24.446385	1065.292576	15.842739
24.510330	1067.769429	15.847757
24.877206	1056.219095	15.852775
24.697800	1060.819794	15.857792
24.715200	1055.326131	15.862810
24.505370	1058.814428	15.867827
24.637630	1062.470366	15.872845
24.771023	1065.356123	15.877863
24.803180	1078.207763	15.882880
25.059449	1080.623117	15.887898
25.214967	1090.110449	15.892915
25.223424	1070.455101	15.897933
25.159224	1062.146577	15.902951
25.149549	1062.517377	15.907968
24.930510	1053.440869	15.912986
25.036569	1061.853462	15.918003
24.843767	1057.777905	15.923021
25.058197	1052.853160	15.928039
25.147354	1067.721916	15.933056
25.387356	1062.932041	15.938074
25.094353	1062.905147	15.943091
25.217814	1077.323608	15.948109
25.143241	1086.556432	15.953127
25.403704	1077.594602	15.958144
25.187232	1086.032176	15.963162
25.204472	1080.216642	15.968179
25.168581	1089.430822	15.973197
25.337587	1082.840586	15.978215
25.224492	1080.876443	15.983232
25.495949	1078.129758	15.988250
25.645767	1083.206216	15.993267
25.647537	1085.897878	15.998285
25.888021	1074.802706	16.003303
25.589334	1074.817722	16.008320
25.853297	1079.794357	16.013338
25.156582	1070.798525	16.018355
24.845271	1073.415855	16.023373
25.528119	1073.893424	16.028391
25.189445	1080.598574	16.033408
25.393714	1075.697495	16.038426
25.679766	1071.323320	16.043443
25.403345	1073.171523	16.048461
25.384182	1075.210044	16.053479
25.659855	1088.601282	16.058496
25.969163	1091.557482	16.063514
26.120051	1092.572306	16.068531
26.084534	1093.773941	16.073549
25.591724	1082.919166	16.078567
25.701681	1084.606228	16.083584
26.118169	1097.757801	16.088602
26.209464	1097.456481	16.093619
25.926214	1081.125382	16.098637
26.049489	1083.738165	16.103655
26.192805	1095.837218	16.108672
26.055935	1083.308116	16.113690
26.051931	1074.898697	16.118707
26.154282	1082.611297	16.123725
26.128639	1078.380323	16.128743
25.963365	1095.949026	16.133760
26.214274	1100.968725	16.138778
26.631988	1096.930646	16.143795
26.215251	1085.625374	16.148813
26.382475	1075.333705	16.153831
26.168785	1074.786384	16.158848
26.228082	1069.254636	16.163866
26.298633	1083.091212	16.168883
26.424307	1093.940172	16.173901
26.504157	1079.991948	16.178919
26.256818	1083.498712	16.183936
26.243620	1095.186638	16.188954
26.093849	1091.792331	16.193971
25.875587	1100.817164	16.198989
26.306001	1088.256538	16.204007
26.279258	1097.122163	16.209024
26.205347	1095.202411	16.214042
26.448345	1086.773463	16.219059
26.306003	1087.537300	16.224077
26.618266	1099.540624	16.229095
26.372830	1113.770401	16.234112
26.488789	1123.538462	16.239130
26.752927	1115.989826	16.244147
26.710393	1129.941874	16.249165
26.996734	1119.439131	16.254183
26.930119	1121.302010	16.259200
26.629422	1118.496079	16.264218
26.837565	1115.680352	16.269235
26.825431	1117.121342	16.274253
27.001443	1114.253813	16.279271
26.850967	1122.097311	16.284288
26.907413	1121.413257	16.289306
26.834987	1122.718469	16.294323
26.571609	1123.690498	16.299341
26.563820	1116.869002	16.304359
26.742689	1123.029690	16.309376
26.846161	1120.167143	16.314394
27.222061	1142.284306	16.319411
27.119011	1144.159172	16.324429
27.465267	1141.807925	16.329447
27.266262	1136.246946	16.334464
27.139877	1126.461705	16.339482
27.679165	1130.758022	16.344499
27.124650	1130.705573	16.349517
27.155986	1118.705673	16.354535
27.503974	1126.566237	16.359552
27.344682	1124.905925	16.364570
27.372325	1122.216129	16.369587
27.600823	1138.514904	16.374605
27.177322	1133.683149	16.379623
27.627070	1142.285263	16.384640
27.468341	1140.353465	16.389658
27.729988	1132.019422	16.394675
27.587930	1144.178719	16.399693
27.386908	1126.196927	16.404711
27.707176	1131.382560	16.409728
27.731214	1140.817807	16.414746
28.015426	1135.001714	16.419763
27.677485	1129.121545	16.424781
27.498959	1116.573659	16.429799
27.582124	1120.780046	16.434816
27.499366	1120.101886	16.439834
27.981904	1125.514713	16.444851
27.824383	1128.003966	16.449869
27.905252	1129.537773	16.454887
28.046376	1128.932052	16.459904
28.123610	1129.832115	16.464922
28.154235	1130.578490	16.469939
27.716176	1130.075568	16.474957
27.869397	1127.921635	16.479975
28.185610	1129.254699	16.484992
28.244384	1130.750921	16.490010
28.224637	1132.035309	16.495027
28.132248	1123.696432	16.500045
28.200165	1115.241083	16.505063
28.146870	1122.299443	16.510080
28.146670	1120.169398	16.515098
27.805257	1116.533527	16.520115
28.283896	1123.761529	16.525133
27.859610	1116.651434	16.530151
28.255298	1129.108843	16.535168
27.945767	1121.318167	16.540186
28.281262	1127.246189	16.545203
27.943827	1131.038387	16.550221
28.099052	1126.801331	16.555239
28.152453	1128.146913	16.560256
28.231838	1136.068237	16.565274
28.435139	1143.152925	16.570291
28.265765	1159.946009	16.575309
28.374117	1156.726093	16.580327
28.374000	1154.002745	16.585344
28.673282	1155.013402	16.590362
28.977429	1149.071125	16.595379
28.861857	1155.261889	16.600397
28.719698	1154.801258	16.605415
28.861629	1152.582808	16.610432
28.856926	1157.108994	16.615450
28.817603	1147.761462	16.620467
28.773586	1158.696842	16.625485
28.748350	1145.746375	16.630503
28.821351	1146.779640	16.635520
28.489070	1155.430937	16.640538
28.365614	1150.041225	16.645555
28.543698	1148.161127	16.650573
28.520316	1145.176316	16.655591
28.884102	1143.453496	16.660608
28.578793	1152.857978	16.665626
29.097231	1163.822552	16.670643
29.246777	1163.894011	16.675661
29.294901	1164.470406	16.680679
29.187301	1166.683651	16.685696
29.049043	1170.384886	16.690714
29.284912	1173.014866	16.695731
29.325148	1175.694241	16.700749
29.207436	1163.089516	16.705767
29.614403	1166.241961	16.710784
29.086012	1160.293605	16.715802
29.170046	1167.251707	16.720819
29.632382	1164.787711	16.725837
29.128930	1165.156498	16.730855
29.341791	1167.651205	16.735872
29.564875	1168.503315	16.740890
29.523605	1163.261748	16.745907
29.395705	1175.519847	16.750925
29.397289	1168.968269	16.755943
29.607807	1171.236125	16.760960
29.444668	1166.155542	16.765978
29.311950	1181.425009	16.770995
29.379513	1174.105769	16.776013
29.198330	1172.849644	16.781031
29.651489	1177.203564	16.786048
29.482933	1174.837794	16.791066
29.519945	1185.031589	16.796083
29.426955	1192.209765	16.801101
29.780495	1192.394629	16.806119
30.137693	1188.466937	16.811136
29.651304	1199.575358	16.816154
29.753090	1190.474075	16.821171
29.933865	1195.820299	16.826189
30.016983	1188.372400	16.831207
30.146102	1191.053716	16.836224
30.026449	1195.364282	16.841242
30.210787	1192.088348	16.846259
30.220914	1195.160575	16.851277
30.239450	1195.514362	16.856295
30.139636	1190.272435	16.861312
30.016455	1196.937765	16.866330
29.914601	1192.784901	16.871347
30.003230	1197.602678	16.876365
29.753919	1187.524119	16.881383
30.103479	1187.977844	16.886400
30.128539	1197.719074	16.891418
30.303118	1200.715205	16.896435
30.423462	1213.897194	16.901453
30.569761	1210.422053	16.906471
30.287812	1203.015208	16.911488
30.713297	1211.655847	16.916506
30.762375	1207.545751	16.921523
30.149871	1204.441217	16.926541
30.139343	1203.739185	16.931559
30.831788	1201.725348	16.936576
30.771055	1220.881037	16.941594
30.655421	1218.645877	16.946611
30.600915	1213.810297	16.951629
30.480415	1214.898940	16.956647
30.484596	1219.392201	16.961664
30.447041	1218.684909	16.966682
30.685629	1208.615581	16.971699
30.715558	1207.765240	16.976717
30.467772	1210.019251	16.981735
30.830140	1207.719136	16.986752
30.740371	1226.617422	16.991770
30.815568	1226.678366	16.996787
31.350509	1230.287422	17.001805
31.193632	1217.808677	17.006823
31.071915	1213.425372	17.011840
31.081951	1214.755622	17.016858
30.934058	1222.980613	17.021875
31.023337	1224.364796	17.026893
30.999713	1226.350380	17.031911
31.487402	1231.093410	17.036928
31.477362	1237.747452	17.041946
31.405013	1238.468839	17.046963
31.605751	1233.378919	17.051981
31.409405	1215.866522	17.056999
31.497932	1204.012294	17.062016
31.776544	1210.047030	17.067034
31.881145	1203.649812	17.072051
31.728526	1203.806186	17.077069
31.526190	1202.761635	17.082087
31.671291	1194.420463	17.087104
31.356665	1203.005918	17.092122
31.314787	1200.689849	17.097139
31.561193	1201.266931	17.102157
31.630605	1207.772893	17.107175
31.887079	1194.412458	17.112192
31.289082	1198.822747	17.117210
31.406296	1198.179721	17.122227
31.762294	1208.412226	17.127245
31.511943	1217.502074	17.132263
31.943977	1213.477518	17.137280
31.619156	1223.648776	17.142298
31.972292	1229.990650	17.147315
32.073904	1227.434487	17.152333
32.079342	1228.345733	17.157351
31.908662	1222.531009	17.162368
31.971861	1228.854910	17.167386
31.806054	1234.662204	17.172403
32.187204	1223.008554	17.177421
32.320097	1222.419891	17.182439
32.272753	1212.445571	17.187456
32.106247	1225.631205	17.192474
31.453361	1234.695373	17.197491
31.840977	1226.347984	17.202509
31.925679	1230.904451	17.207527
32.297996	1224.951535	17.212544
32.051161	1230.427463	17.217562
32.051066	1243.258998	17.222579
32.601047	1248.203772	17.227597
32.218045	1244.826814	17.232615
32.687900	1241.228707	17.237632
32.430317	1247.047139	17.242650
32.343553	1245.829958	17.247667
32.515278	1237.658188	17.252685
32.705948	1255.698647	17.257703
32.689954	1243.491437	17.262720
32.506869	1246.035180	17.267738
32.642594	1247.472094	17.272755
32.657530	1239.428876	17.277773
32.561029	1247.216689	17.282791
32.702563	1248.362366	17.287808
32.735493	1245.567586	17.292826
32.458240	1246.283007	17.297843
32.595071	1237.816870	17.302861
32.336012	1243.809099	17.307879
32.488191	1260.627952	17.312896
33.107797	1265.211597	17.317914
33.059684	1263.183668	17.322931
33.504920	1261.820539	17.327949
33.170453	1270.768877	17.332967
33.291702	1266.972578	17.337984
33.350547	1265.552844	17.343002
32.783599	1272.170531	17.348019
32.786954	1261.437210	17.353037
33.370392	1270.839079	17.358055
33.258802	1264.787924	17.363072
33.116804	1275.962692	17.368090
32.672568	1266.211083	17.373107
33.443420	1258.463573	17.378125
33.325787	1267.277163	17.383143
33.308233	1261.823592	17.388160
33.691969	1258.677546	17.393178
33.403939	1262.140188	17.398195
33.787388	1259.997730	17.403213
33.356151	1265.694883	17.408231
33.631533	1262.811858	17.413248
33.434011	1259.399707	17.418266
33.374178	1272.265811	17.423283
33.926350	1268.992553	17.428301
33.736680	1285.769980	17.433319
33.932809	1284.347804	17.438336
33.865406	1285.645935	17.443354
33.648866	1291.849310	17.448371
33.905126	1280.631634	17.453389
33.862832	1285.769620	17.458407
33.922831	1282.683442	17.463424
33.834539	1284.095277	17.468442
33.733098	1287.017633	17.473459
33.590429	1278.809588	17.478477
33.808470	1292.320406	17.483495
34.119146	1280.601952	17.488512
34.127583	1283.207399	17.493530
34.091302	1279.950020	17.498547
33.768428	1279.384978	17.503565
33.955796	1285.228819	17.508583
34.540500	1290.610012	17.513600
34.565776	1300.988736	17.518618
33.793101	1302.825865	17.523635
33.929317	1297.301005	17.528653
34.651654	1301.767680	17.533671
34.575099	1307.267612	17.538688
34.363908	1299.780282	17.543706
34.367475	1302.938755	17.548723
34.653291	1304.402798	17.553741
34.897480	1311.560083	17.558759
34.421889	1311.946625	17.563776
34.524509	1304.385187	17.568794
34.262131	1308.676976	17.573811
34.541718	1309.353038	17.578829
34.645702	1306.755469	17.583847
34.897372	1307.498994	17.588864
34.620516	1312.326369	17.593882
34.279738	1318.508072	17.598899
34.658746	1304.311123	17.603917
34.558343	1319.900725	17.608935
35.019832	1322.363055	17.613952
35.103774	1329.295988	17.618970
35.130833	1338.459470	17.623987
35.425244	1337.905615	17.629005
35.328167	1320.134663	17.634023
35.053763	1312.578274	17.639040
35.055050	1310.681504	17.644058
35.071027	1320.641966	17.649075
35.344230	1326.822751	17.654093
35.290983	1328.866607	17.659111
35.094577	1331.977325	17.664128
35.638726	1327.452449	17.669146
35.391062	1333.294611	17.674163
35.212102	1338.053103	17.679181
35.381928	1346.077204	17.684199
35.016385	1339.607970	17.689216
35.478292	1329.270274	17.694234
35.369231	1333.755949	17.699251
35.427692	1328.618726	17.704269
35.383885	1327.167633	17.709287
35.177783	1334.928367	17.714304
35.740019	1329.911525	17.719322
35.583166	1331.479206	17.724339
36.036412	1341.030771	17.729357
35.871718	1339.049387	17.734375
35.329429	1340.778065	17.739392
35.919789	1345.325260	17.744410
35.862336	1353.858123	17.749427
36.144061	1348.979624	17.754445
36.164614	1353.634472	17.759463
36.105983	1349.351765	17.764480
36.419487	1344.591396	17.769498
36.145174	1342.406172	17.774515
36.165319	1326.721888	17.779533
36.186382	1330.571920	17.784551
36.375395	1317.531166	17.789568
36.185133	1317.327328	17.794586
35.917490	1323.384037	17.799603
36.456541	1341.452392	17.804621
36.183914	1340.810097	17.809639
36.165027	1345.499486	17.814656
36.317512	1335.216274	17.819674
36.547824	1344.493281	17.824691
36.483187	1335.342097	17.829709
36.441217	1346.027963	17.834727
36.449295	1345.717505	17.839744
36.579731	1343.851117	17.844762
36.624364	1345.857644	17.849779
36.725001	1351.453078	17.854797
36.229297	1347.399369	17.859815
36.144958	1349.233473	17.864832
36.346574	1341.328402	17.869850
36.690412	1359.660699	17.874867
36.489106	1361.244772	17.879885
37.040762	1367.568410	17.884903
37.016573	1372.605772	17.889920
37.095436	1360.424739	17.894938
36.993240	1364.426513	17.899955
37.036488	1365.357126	17.904973
37.197224	1367.421319	17.909991
36.905081	1362.433349	17.915008
37.203040	1362.481702	17.920026
37.085305	1363.374262	17.925043
37.517615	1363.095583	17.930061
37.501380	1360.557749	17.935079
37.288015	1361.260071	17.940096
37.394573	1351.381633	17.945114
37.044238	1356.154189	17.950131
37.271819	1358.712903	17.955149
37.043673	1357.353624	17.960167
36.741080	1364.719139	17.965184
37.331862	1358.602776	17.970202
36.967929	1360.871734	17.975219
37.112462	1359.656402	17.980237
37.264061	1372.729501	17.985255
37.565441	1386.236882	17.990272
37.989357	1383.090871	17.995290
37.620694	1390.542423	18.000307
37.612516	1392.831734	18.005325
38.181250	1388.082109	18.010343
37.521976	1383.170229	18.015360
37.879507	1390.360392	18.020378
37.844605	1396.737495	18.025395
38.087106	1386.339253	18.030413
37.844535	1384.553026	18.035431
37.714237	1393.905139	18.040448
37.898619	1387.994054	18.045466
37.807058	1380.339740	18.050483
37.972921	1387.319902	18.055501
38.282692	1381.698566	18.060519
38.046857	1387.166517	18.065536
38.208845	1391.856159	18.070554
38.300990	1401.404018	18.075571
38.306214	1402.955938	18.080589
38.603283	1413.336592	18.085607
38.231692	1412.753884	18.090624
38.563069	1404.519312	18.095642
38.330250	1406.733147	18.100659
38.665878	1407.088061	18.105677
38.748268	1403.240979	18.110695
38.891967	1413.099555	18.115712
38.338391	1402.127812	18.120730
38.575877	1403.470000	18.125747
38.412088	1401.169730	18.130765
38.652114	1403.628683	18.135783
38.849577	1411.942003	18.140800
38.656134	1404.420307	18.145818
38.832285	1404.074212	18.150835
38.808848	1409.316596	18.155853
38.957396	1409.691170	18.160871
38.607226	1411.348917	18.165888
38.855347	1404.029873	18.170906
38.999540	1404.780668	18.175923
39.005110	1404.571586	18.180941
38.806076	1400.111910	18.185959
39.177493	1407.953173	18.190976
39.452587	1429.594081	18.195994
39.070153	1422.916006	18.201011
39.012713	1422.019296	18.206029
39.443119	1426.411534	18.211047
39.463791	1430.829697	18.216064
39.562147	1431.161594	18.221082
39.573614	1428.774073	18.226099
39.136264	1424.449326	18.231117
39.717161	1420.597209	18.236135
39.578101	1425.674561	18.241152
39.365605	1422.495085	18.246170
39.746231	1429.441825	18.251187
39.830442	1437.122689	18.256205
39.735402	1432.365945	18.261223
39.734841	1424.975157	18.266240
39.883999	1425.627350	18.271258
39.880223	1421.247721	18.276275
39.679994	1426.012703	18.281293
39.967137	1427.403966	18.286311
39.959871	1427.869073	18.291328
39.816026	1422.217364	18.296346
39.935542	1422.321902	18.301363
39.909655	1422.849869	18.306381
39.954902	1422.132833	18.311399
39.844213	1419.401413	18.316416
40.032232	1422.458605	18.321434
39.910926	1424.506757	18.326451
39.987567	1427.669654	18.331469
39.980561	1421.630564	18.336487
39.893687	1437.293902	18.341504
40.197020	1439.853457	18.346522
40.260852	1440.856609	18.351539
40.305703	1441.786976	18.356557
40.238487	1437.792765	18.361575
40.623448	1440.345922	18.366592
40.697084	1437.554242	18.371610
40.425673	1438.312942	18.376627
40.559975	1438.121686	18.381645
40.742087	1431.412515	18.386663
40.529186	1436.094266	18.391680
40.508548	1437.233646	18.396698
40.679195	1441.275009	18.401715
41.071882	1450.599374	18.406733
40.960120	1458.130877	18.411751
41.039664	1459.336713	18.416768
41.350472	1455.495081	18.421786
40.719098	1443.695974	18.426803
40.895483	1451.646518	18.431821
41.017436	1442.819680	18.436839
41.246055	1454.637450	18.441856
40.965278	1455.325025	18.446874
41.250315	1450.247166	18.451891
41.317419	1448.340133	18.456909
40.848517	1439.589511	18.461927
40.885377	1455.435573	18.466944
41.012663	1446.412241	18.471962
41.205499	1445.179916	18.476979
41.419032	1460.247387	18.481997
42.021104	1461.709541	18.487015
41.556750	1455.397662	18.492032
41.622817	1453.213077	18.497050
41.948280	1451.262663	18.502067
41.561597	1449.012870	18.507085
41.757126	1434.061739	18.512103
41.716858	1441.127665	18.517120
41.694430	1444.779364	18.522138
42.009745	1456.072393	18.527155
42.154985	1467.767453	18.532173
42.073571	1449.432194	18.537191
41.835982	1447.288577	18.542208
42.006203	1457.739500	18.547226
42.167413	1453.734967	18.552243
41.742468	1458.777944	18.557261
42.125200	1461.946839	18.562279
41.997456	1468.108048	18.567296
41.891273	1464.479663	18.572314
42.200398	1466.145220	18.577331
42.061044	1468.174095	18.582349
42.128667	1468.435038	18.587367
42.079679	1472.213955	18.592384
42.065510	1463.193704	18.597402
42.339428	1462.835542	18.602419
42.384677	1471.519730	18.607437
42.580846	1473.240745	18.612455
42.553875	1484.053748	18.617472
42.659117	1496.256832	18.622490
42.827826	1496.915451	18.627507
42.926690	1503.498987	18.632525
42.637187	1475.050079	18.637543
42.704653	1481.395496	18.642560
42.487042	1493.781391	18.647578
43.129143	1488.909861	18.652595
42.709782	1495.173288	18.657613
42.920832	1483.157785	18.662631
43.317495	1483.471640	18.667648
42.962385	1487.730572	18.672666
43.188020	1480.948334	18.677683
42.842295	1486.736385	18.682701
42.993458	1488.082552	18.687719
43.139875	1482.467683	18.692736
43.068977	1484.552175	18.697754
43.388107	1482.665860	18.702771
43.038669	1489.682110	18.707789
43.206225	1486.235165	18.712807
43.290458	1477.209053	18.717824
43.025920	1499.899750	18.722842
43.342182	1505.243908	18.727859
43.647295	1513.228086	18.732877
43.658322	1510.439831	18.737895
43.548210	1508.257424	18.742912
43.441831	1509.507989	18.747930
43.822971	1513.305154	18.752947
43.576352	1522.378796	18.757965
43.259258	1506.374471	18.762983
43.418465	1498.898816	18.768000
43.247152	1525.100102	18.773018
43.870242	1531.119184	18.778035
43.588864	1541.760391	18.783053
44.018437	1541.857682	18.788071
43.808707	1530.999583	18.793088
43.858020	1536.685118	18.798106
43.896638	1528.502382	18.803123
44.077429	1548.801104	18.808141
44.287806	1557.794144	18.813159
45.082073	1551.175814	18.818176
44.356384	1549.556309	18.823194
44.692411	1523.922779	18.828211
44.333365	1525.149568	18.833229
44.391229	1524.203342	18.838247
44.932753	1530.964123	18.843264
44.489999	1536.139284	18.848282
44.839671	1517.405473	18.853299
44.534610	1526.904788	18.858317
44.747596	1534.098580	18.863335
44.778269	1530.480431	18.868352
45.031758	1545.560689	18.873370
45.175017	1530.668110	18.878387
44.789826	1526.489853	18.883405
44.751163	1522.437528	18.888423
45.288569	1526.538573	18.893440
44.951526	1529.270430	18.898458
45.101529	1526.529963	18.903475
44.772030	1535.117892	18.908493
44.983689	1542.188816	18.913511
45.179877	1544.730354	18.918528
45.019017	1552.159086	18.923546
44.998108	1540.378479	18.928563
44.736117	1549.637567	18.933581
45.025579	1547.260397	18.938599
45.123059	1546.143898	18.943616
44.807995	1559.409714	18.948634
45.497565	1565.386898	18.953651
45.221700	1577.819791	18.958669
45.579487	1572.345557	18.963687
45.667158	1569.053046	18.968704
45.441493	1576.599178	18.973722
45.687856	1573.666973	18.978739
45.745375	1579.395426	18.983757
45.685889	1573.825210	18.988775
45.851872	1561.135008	18.993792
45.644972	1571.752013	18.998810
45.940679	1569.708388	19.003827
46.002723	1570.232136	19.008845
46.216585	1571.404443	19.013863
45.973785	1565.140081	19.018880
45.917364	1576.945507	19.023898
46.298384	1586.334878	19.028915
46.578954	1585.079416	19.033933
46.344360	1579.283993	19.038951
46.215447	1582.434740	19.043968
45.988684	1593.032760	19.048986
46.277214	1585.470660	19.054003
46.457029	1593.196668	19.059021
46.214198	1592.338282	19.064039
46.575080	1582.173963	19.069056
46.448976	1581.628768	19.074074
46.577855	1583.316088	19.079091
46.416183	1588.734683	19.084109
46.687018	1578.316138	19.089127
46.804062	1572.690035	19.094144
46.549414	1585.207994	19.099162
47.243523	1592.591992	19.104179
47.101260	1588.678860	19.109197
46.663837	1583.397861	19.114215
47.055569	1583.759824	19.119232
47.182747	1600.390383	19.124250
47.420765	1600.261874	19.129267
47.463715	1600.725479	19.134285
46.915572	1582.472219	19.139303
47.313156	1590.574580	19.144320
47.277397	1590.756945	19.149338
47.778031	1590.634886	19.154355
47.787225	1588.522257	19.159373
47.498820	1575.170632	19.164391
47.696188	1565.956445	19.169408
47.614868	1574.777156	19.174426
47.432271	1568.837940	19.179443
47.221890	1577.864942	19.184461
47.510070	1589.812387	19.189479
47.700267	1592.162358	19.194496
47.938646	1599.434274	19.199514
47.829811	1597.257968	19.204531
47.979376	1603.518061	19.209549
47.866654	1600.139979	19.214567
47.909986	1592.360429	19.219584
48.061812	1594.738465	19.224602
48.036462	1594.830845	19.229619
47.751256	1594.739618	19.234637
47.592313	1594.698161	19.239655
47.967169	1590.780256	19.244672
47.977666	1604.651834	19.249690
47.954113	1604.781805	19.254707
48.080112	1613.728050	19.259725
48.026144	1623.402920	19.264743
48.483727	1617.288273	19.269760
48.397054	1618.437947	19.274778
48.132566	1625.630375	19.279795
48.690796	1618.231402	19.284813
48.642071	1622.335364	19.289831
48.630253	1611.389597	19.294848
48.182374	1616.969529	19.299866
48.237948	1614.622454	19.304883
48.876709	1622.665189	19.309901
48.750052	1635.832297	19.314919
49.073409	1640.253880	19.319936
49.220450	1640.666564	19.324954
49.057853	1637.671788	19.329971
49.194077	1626.810261	19.334989
49.200712	1634.945110	19.340007
49.119042	1631.858838	19.345024
49.165171	1639.425795	19.350042
49.482807	1636.059598	19.355059
49.267888	1634.499418	19.360077
49.052609	1632.377552	19.365095
49.146502	1639.507876	19.370112
49.064082	1635.784235	19.375130
48.922697	1645.712574	19.380147
49.406296	1634.367760	19.385165
49.644476	1652.511679	19.390183
49.669626	1653.959531	19.395200
49.655603	1657.253352	19.400218
49.664305	1659.969268	19.405235
49.979270	1652.330440	19.410253
50.005001	1658.171167	19.415271
49.911009	1662.632487	19.420288
49.879608	1654.097670	19.425306
49.999908	1652.434803	19.430323
49.796733	1657.515891	19.435341
49.603091	1654.857312	19.440359
49.716577	1654.000251	19.445376
49.634937	1654.271813	19.450394
49.721866	1660.585860	19.455411
50.092359	1670.317748	19.460429
50.219043	1681.100635	19.465447
50.416629	1673.593685	19.470464
50.341321	1673.166813	19.475482
50.299546	1667.003663	19.480499
50.295642	1676.768600	19.485517
50.222639	1684.982143	19.490535
50.725149	1693.516349	19.495552
50.916570	1697.270507	19.500570
51.108048	1690.013815	19.505587
51.112110	1678.718388	19.510605
50.770098	1675.770474	19.515623
51.200750	1668.397656	19.520640
51.050140	1673.053990	19.525658
51.017845	1668.656650	19.530675
50.754251	1671.916746	19.535693
51.164758	1685.176986	19.540711
51.154158	1680.981397	19.545728
51.042396	1677.817750	19.550746
51.514682	1686.331411	19.555763
51.815799	1680.537756	19.560781
51.353498	1677.337166	19.565799
51.242926	1669.228087	19.570816
51.615535	1687.767687	19.575834
51.372907	1694.183551	19.580851
51.792888	1688.283022	19.585869
51.635884	1691.195159	19.590887
51.673198	1692.461236	19.595904
51.690799	1680.586175	19.600922
51.777477	1686.976012	19.605939
51.552870	1680.853946	19.610957
51.886821	1689.954048	19.615975
51.846204	1677.627297	19.620992
51.936569	1687.756266	19.626010
51.598514	1689.071318	19.631027
51.719045	1683.315246	19.636045
51.676567	1689.882987	19.641063
51.965378	1684.125961	19.646080
52.190987	1695.581435	19.651098
51.705776	1712.342160	19.656115
52.276442	1710.009551	19.661133
52.492220	1705.011833	19.666151
52.231945	1705.689912	19.671168
52.561205	1716.053108	19.676186
52.384441	1716.386819	19.681203
52.380860	1709.908432	19.686221
52.553288	1703.358460	19.691239
52.307707	1699.862186	19.696256
52.149878	1707.628189	19.701274
52.366543	1721.799126	19.706291
52.712270	1730.641790	19.711309
52.824589	1726.139867	19.716327
52.866095	1730.561172	19.721344
53.114551	1720.471085	19.726362
53.000798	1724.490518	19.731379
53.311241	1722.914808	19.736397
53.139257	1728.858927	19.741415
53.081915	1727.116411	19.746432
53.504856	1717.014938	19.751450
53.602721	1717.274331	19.756467
53.614738	1706.949658	19.761485
53.817192	1715.142419	19.766503
53.636325	1710.215923	19.771520
53.683707	1717.845836	19.776538
53.496107	1713.138143	19.781555
53.618998	1715.271386	19.786573
53.884836	1708.883599	19.791591
53.407123	1705.511830	19.796608
53.411499	1703.848071	19.801626
53.561622	1716.265230	19.806643
53.702679	1716.044517	19.811661
53.743214	1729.674825	19.816679
53.864983	1742.815958	19.821696
54.073530	1727.496473	19.826714
53.981169	1730.401707	19.831731
54.324062	1734.659322	19.836749
54.034391	1728.307523	19.841767
54.086379	1732.922862	19.846784
54.267557	1733.235557	19.851802
54.213872	1729.734647	19.856819
54.417433	1728.020939	19.861837
54.131178	1739.410966	19.866855
54.411648	1752.268614	19.871872
54.816539	1755.405710	19.876890
54.545466	1765.493165	19.881907
54.779237	1755.500021	19.886925
54.917281	1761.092916	19.891943
55.019304	1760.944553	19.896960
55.302227	1760.777493	19.901978
54.898142	1764.002674	19.906995
55.319207	1759.156019	19.912013
55.020553	1759.868479	19.917031
55.149871	1754.278278	19.922048
54.918681	1759.392161	19.927066
55.168100	1760.842974	19.932083
54.875923	1752.235099	19.937101
54.937676	1758.048160	19.942119
55.070183	1758.901778	19.947136
55.241536	1754.933469	19.952154
55.337988	1758.020756	19.957171
54.907337	1756.039706	19.962189
55.326485	1772.549227	19.967207
55.274781	1787.307968	19.972224
55.063966	1782.442920	19.977242
55.613911	1786.097094	19.982259
55.796062	1778.270603	19.987277
55.734851	1786.614904	19.992295
55.621317	1798.741802	19.997312
56.040220	1803.350526	20.002330
56.060881	1810.145172	20.007347
56.374483	1807.603259	20.012365
56.152595	1806.290309	20.017383
56.061813	1805.821661	20.022400
56.067610	1804.305999	20.027418
55.987147	1803.072019	20.032435
56.090439	1799.319430	20.037453
56.880868	1800.474569	20.042471
56.303084	1806.614442	20.047488
56.564696	1798.428422	20.052506
56.490216	1803.180237	20.057523
56.415707	1802.645938	20.062541
56.577800	1806.089096	20.067559
56.292933	1809.781730	20.072576
56.820093	1820.975734	20.077594
56.480021	1828.445107	20.082611
56.734991	1824.567909	20.087629
56.973341	1824.227902	20.092647
56.940920	1832.261620	20.097664
57.293393	1822.073227	20.102682
57.002522	1830.292356	20.107699
56.953027	1818.408714	20.112717
57.069367	1825.743907	20.117735
57.399320	1844.994077	20.122752
57.458036	1843.419678	20.127770
57.679867	1850.476517	20.132787
57.571718	1846.917789	20.137805
57.481409	1844.006400	20.142823
57.918121	1845.058820	20.147840
58.129269	1839.291745	20.152858
57.692470	1818.821244	20.157875
57.678978	1824.683912	20.162893
57.716869	1828.645044	20.167911
57.515150	1844.260346	20.172928
58.192797	1839.985966	20.177946
57.884958	1840.040276	20.182963
58.174475	1841.226069	20.187981
57.937083	1846.766988	20.192999
58.071925	1846.162222	20.198016
58.387533	1836.408762	20.203034
58.132428	1839.980001	20.208051
57.890253	1842.693978	20.213069
58.314704	1844.123859	20.218087
57.914183	1859.653358	20.223104
58.381093	1860.360239	20.228122
58.802607	1866.597019	20.233139
58.611915	1863.789621	20.238157
58.962058	1865.745485	20.243175
58.646988	1869.789984	20.248192
58.731472	1859.419225	20.253210
58.616777	1853.564018	20.258227
58.581956	1862.551206	20.263245
58.991624	1854.869144	20.268263
58.937595	1866.371423	20.273280
59.131678	1862.895028	20.278298
58.940850	1858.863161	20.283315
59.142328	1872.222360	20.288333
59.324315	1873.279726	20.293351
59.196106	1890.818192	20.298368
59.208654	1884.990503	20.303386
59.624561	1890.477058	20.308403
59.632658	1890.987124	20.313421
59.759784	1882.522193	20.318439
59.831363	1883.644088	20.323456
59.774358	1877.164490	20.328474
59.522690	1877.916977	20.333491
59.524678	1873.975011	20.338509
59.945747	1873.414045	20.343527
59.787801	1881.830259	20.348544
59.767974	1871.728206	20.353562
59.922063	1878.574690	20.358579
60.013168	1881.890055	20.363597
59.783260	1880.792950	20.368615
60.335749	1898.619931	20.373632
60.218377	1893.844449	20.378650
60.399006	1898.685963	20.383667
59.999308	1896.106767	20.388685
60.106285	1899.517498	20.393703
60.039098	1912.760761	20.398720
60.503616	1893.686772	20.403738
61.030734	1911.400948	20.408755
60.811929	1910.747095	20.413773
60.635831	1906.741328	20.418791
60.452011	1915.616037	20.423808
60.967245	1921.409040	20.428826
61.334557	1924.510990	20.433843
61.321727	1924.774998	20.438861
61.175762	1924.185546	20.443879
60.782540	1926.175102	20.448896
61.244911	1920.801247	20.453914
61.608238	1913.710219	20.458931
61.356537	1920.720888	20.463949
61.533459	1911.610695	20.468967
61.436723	1918.556209	20.473984
61.495930	1916.429442	20.479002
61.806529	1916.491610	20.484019
61.599642	1916.792143	20.489037
61.680131	1910.139642	20.494055
61.633178	1920.523661	20.499072
61.688232	1907.042570	20.504090
61.789566	1913.408115	20.509107
61.312729	1921.495288	20.514125
61.840111	1924.793230	20.519143
61.951727	1930.683793	20.524160
62.020529	1931.591521	20.529178
61.804044	1937.195487	20.534195
61.651468	1944.484232	20.539213
62.317964	1930.699634	20.544231
62.130134	1943.317897	20.549248
62.054695	1952.974197	20.554266
62.321845	1955.738284	20.559283
62.421622	1965.004380	20.564301
62.468206	1955.643049	20.569319
62.459904	1963.092382	20.574336
62.354615	1956.585558	20.579354
62.839031	1965.255261	20.584371
62.555813	1978.667912	20.589389
63.468546	1982.095223	20.594407
63.405715	1982.988733	20.599424
62.874239	1968.705790	20.604442
63.083094	1965.397495	20.609459
63.158816	1977.469800	20.614477
63.319783	1978.902845	20.619495
63.271143	1983.470797	20.624512
63.163577	1980.233856	20.629530
63.666747	1976.191744	20.634547
63.563354	1968.453810	20.639565
63.831383	1975.020650	20.644583
63.693649	1978.052914	20.649600
63.631466	1985.772587	20.654618
63.748723	1981.878925	20.659635
63.282203	1984.066098	20.664653
64.028542	1970.029189	20.669671
63.598211	1984.035971	20.674688
63.484610	1978.123747	20.679706
63.726846	1979.004475	20.684723
63.804229	1994.380785	20.689741
64.154842	1992.637846	20.694759
64.187552	1997.347776	20.699776
64.291325	2000.332975	20.704794
64.718425	1996.706661	20.709811
64.177711	2005.166748	20.714829
64.270300	1998.464991	20.719847
64.675632	1989.435966	20.724864
64.445569	1994.836929	20.729882
64.771104	1990.254405	20.734899
64.355528	1997.186472	20.739917
64.628799	2000.325169	20.744935
65.186134	2015.112355	20.749952
64.970927	2020.290097	20.754970
65.366356	2007.349251	20.759987
64.953042	2015.953616	20.765005
65.496346	2019.271188	20.770023
65.282931	2015.309078	20.775040
65.243404	2012.121500	20.780058
65.534946	2012.057242	20.785075
65.266314	2015.094113	20.790093
65.271223	2015.569964	20.795111
65.397883	2008.256960	20.800128
65.307184	2008.040768	20.805146
65.709351	2007.697344	20.810163
65.156990	2007.603525	20.815181
65.299937	2014.732674	20.820199
65.485906	2014.675385	20.825216
65.782834	2024.355803	20.830234
65.731427	2015.650351	20.835251
65.399599	2033.952836	20.840269
66.172817	2037.338761	20.845287
66.005611	2049.518369	20.850304
66.008449	2057.553011	20.855322
66.159753	2050.321363	20.860339
66.096724	2057.807660	20.865357
66.592928	2054.034871	20.870375
66.831640	2047.010531	20.875392
66.309723	2050.134182	20.880410
66.748441	2049.138100	20.885427
66.924443	2053.844671	20.890445
66.584085	2045.607089	20.895463
66.544823	2054.926438	20.900480
66.576298	2067.876732	20.905498
67.165850	2066.967623	20.910515
66.861232	2065.465554	20.915533
67.141415	2068.249721	20.920551
67.379947	2072.059743	20.925568
67.152974	2071.060002	20.930586
67.395142	2069.734744	20.935603
67.511477	2071.108470	20.940621
67.730678	2062.291432	20.945639
67.668414	2066.965673	20.950656
67.543967	2067.565811	20.955674
67.735120	2065.478446	20.960691
67.331390	2072.001582	20.965709
67.652871	2066.987305	20.970727
67.735441	2073.062326	20.975744
67.851454	2087.687901	20.980762
67.907793	2090.232356	20.985779
68.127847	2088.901072	20.990797
67.939255	2088.498139	20.995815
68.188856	2094.749142	21.000832
68.197749	2100.292821	21.005850
68.426964	2092.392590	21.010867
68.291892	2099.924836	21.015885
68.196672	2089.727096	21.020903
67.985812	2091.334811	21.025920
68.470006	2095.775649	21.030938
68.978859	2098.773538	21.035955
68.767940	2119.730371	21.040973
68.646055	2127.601418	21.045991
68.889779	2122.526646	21.051008
68.963180	2123.219064	21.056026
68.822473	2121.290664	21.061043
68.979450	2123.232449	21.066061
68.959539	2121.414636	21.071079
68.832059	2120.815987	21.076096
68.685089	2116.881380	21.081114
69.372227	2128.110633	21.086131
69.373496	2140.352438	21.091149
69.443589	2141.035904	21.096167
69.632638	2144.443371	21.101184
69.642747	2149.049558	21.106202
69.666550	2142.724548	21.111219
69.473085	2141.807953	21.116237
69.287885	2144.235380	21.121255
69.598107	2157.899769	21.126272
69.746769	2166.214727	21.131290
69.796609	2156.754950	21.136307
69.695132	2173.816138	21.141325
69.854376	2172.506939	21.146343
70.041440	2172.619902	21.151360
70.034047	2186.371634	21.156378
70.339292	2184.774602	21.161395
70.408758	2190.132144	21.166413
70.400436	2182.234142	21.171431
70.521941	2189.726478	21.176448
70.205089	2185.755186	21.181466
70.773789	2188.317718	21.186483
70.915083	2190.855273	21.191501
70.791468	2189.574332	21.196519
71.035516	2197.107555	21.201536
71.100185	2208.853518	21.206554
71.430209	2203.007855	21.211571
71.370501	2201.499203	21.216589
71.449269	2202.998714	21.221607
71.345758	2206.174019	21.226624
71.232591	2203.231414	21.231642
71.497398	2203.442731	21.236659
71.727704	2201.702723	21.241677
71.517206	2199.797805	21.246695
71.743921	2197.547090	21.251712
71.703423	2205.276106	21.256730
71.725940	2199.172193	21.261747
71.576040	2196.819161	21.266765
71.560554	2189.998454	21.271783
71.757292	2202.607519	21.276800
71.650845	2218.495505	21.281818
72.268965	2219.251447	21.286835
72.150362	2223.120261	21.291853
71.982155	2225.750192	21.296871
71.933758	2215.936430	21.301888
72.039591	2214.597672	21.306906
72.357677	2227.503458	21.311923
72.559258	2233.421141	21.316941
72.334297	2239.285310	21.321959
72.668288	2235.127463	21.326976
72.885119	2237.473374	21.331994
72.834967	2238.863566	21.337011
73.170363	2240.446208	21.342029
72.926181	2234.955037	21.347047
73.208537	2234.478777	21.352064
72.921485	2244.628953	21.357082
72.942542	2241.018470	21.362099
73.158851	2252.529402	21.367117
73.397305	2260.786241	21.372135
73.569965	2261.075025	21.377152
73.617533	2265.135738	21.382170
73.608110	2263.073268	21.387187
73.776911	2261.677363	21.392205
73.590446	2267.481896	21.397223
74.027266	2252.792332	21.402240
73.513192	2263.697426	21.407258
73.665787	2254.322589	21.412275
73.845292	2265.713021	21.417293
74.053688	2279.159814	21.422311
74.249882	2282.392617	21.427328
74.252409	2283.784078	21.432346
74.614619	2280.685392	21.437363
74.750710	2278.458245	21.442381
74.591933	2280.818457	21.447399
75.074906	2284.745109	21.452416
74.837263	2284.122579	21.457434
74.541614	2280.046973	21.462451
74.339315	2282.041557	21.467469
74.376170	2277.608053	21.472487
74.626839	2276.183621	21.477504
74.860634	2285.211255	21.482522
74.835516	2298.296766	21.487539
74.983109	2298.071873	21.492557
75.004333	2314.003186	21.497575
75.118215	2295.927002	21.502592
75.019701	2301.714696	21.507610
75.079879	2317.744095	21.512627
75.497550	2327.680449	21.517645
75.908073	2330.756807	21.522663
76.090820	2327.332584	21.527680
75.624784	2338.965589	21.532698
75.821485	2338.193376	21.537715
76.113573	2334.505960	21.542733
75.903329	2326.740323	21.547751
76.143294	2327.065969	21.552768
76.129617	2329.236330	21.557786
76.149790	2324.401445	21.562803
76.187737	2323.130057	21.567821
76.123861	2338.074194	21.572839
76.255414	2347.704792	21.577856
76.327325	2350.098528	21.582874
76.292404	2346.029653	21.587891
76.637606	2350.454324	21.592909
77.015714	2347.409959	21.597927
76.606052	2346.523858	21.602944
76.631108	2349.234176	21.607962
76.915435	2352.308094	21.612979
77.519178	2359.412977	21.617997
77.390498	2356.071951	21.623015
77.459385	2352.974737	21.628032
77.576852	2349.532269	21.633050
77.542945	2350.487570	21.638067
77.417786	2334.547297	21.643085
77.462763	2335.029542	21.648103
77.619910	2338.997467	21.653120
77.771343	2356.101508	21.658138
77.712541	2362.179702	21.663155
77.980949	2343.022154	21.668173
77.926932	2356.200575	21.673191
77.952328	2352.033940	21.678208
78.011520	2346.741668	21.683226
78.216330	2345.144480	21.688243
78.128179	2347.301190	21.693261
77.790167	2353.353420	21.698279
78.050107	2341.301326	21.703296
78.399442	2345.586489	21.708314
77.890134	2362.111717	21.713331
78.447219	2367.434420	21.718349
78.572333	2371.565140	21.723367
78.712011	2370.719748	21.728384
78.430662	2367.740181	21.733402
78.389685	2386.253377	21.738419
78.850001	2382.511355	21.743437
79.038496	2392.814806	21.748455
79.167692	2391.989981	21.753472
79.469064	2391.542317	21.758490
79.423727	2404.242866	21.763507
79.251273	2396.761667	21.768525
79.326963	2398.867626	21.773543
78.940152	2395.225935	21.778560
79.377793	2408.624509	21.783578
79.118407	2416.854783	21.788595
79.434375	2417.992314	21.793613
79.349405	2432.378046	21.798631
79.696087	2428.297079	21.803648
80.265922	2430.569118	21.808666
80.650254	2438.175282	21.813683
80.628394	2435.338351	21.818701
80.461481	2436.222841	21.823719
80.757132	2427.987051	21.828736
80.870647	2429.673688	21.833754
80.769148	2422.616959	21.838771
81.100854	2407.243001	21.843789
80.587484	2411.148071	21.848807
80.692611	2413.366220	21.853824
80.618610	2424.622643	21.858842
80.811812	2431.712573	21.863859
81.106883	2425.493560	21.868877
80.920240	2422.022683	21.873895
81.273577	2425.366754	21.878912
81.017076	2426.754372	21.883930
81.049248	2425.064127	21.888947
81.375508	2426.569308	21.893965
81.195984	2438.994110	21.898983
81.511721	2447.652439	21.904000
81.515834	2448.223105	21.909018
81.591042	2453.646108	21.914035
81.899493	2446.528699	21.919053
81.691144	2448.211798	21.924071
82.090767	2453.240287	21.929088
82.200337	2445.506861	21.934106
81.964648	2446.941737	21.939123
82.320974	2449.013476	21.944141
82.641063	2467.779829	21.949159
82.390972	2470.021731	21.954176
82.058881	2461.224055	21.959194
82.746425	2469.600430	21.964211
82.794470	2455.829665	21.969229
82.534739	2463.671825	21.974247
82.283532	2466.434642	21.979264
82.594704	2466.061194	21.984282
82.502043	2473.599618	21.989299
82.549553	2475.217636	21.994317
82.986671	2491.816550	21.999335
83.254683	2487.359628	22.004352
83.218855	2487.024426	22.009370
82.954372	2492.828555	22.014387
83.292261	2481.767843	22.019405
83.078824	2485.714598	22.024423
83.299312	2504.281888	22.029440
83.424982	2509.444570	22.034458
83.206679	2518.422782	22.039475
83.725505	2507.109807	22.044493
83.469941	2513.029326	22.049511
83.407256	2521.525688	22.054528
83.628191	2522.741142	22.059546
84.026680	2527.479475	22.064563
84.572763	2524.494140	22.069581
84.487753	2536.819082	22.074599
84.429940	2531.295647	22.079616
84.660566	2539.206671	22.084634
84.468454	2558.636730	22.089651
84.971250	2553.101749	22.094669
84.982038	2558.490630	22.099687
85.231308	2563.738233	22.104704
85.097030	2558.545453	22.109722
84.801446	2559.863421	22.114739
85.069123	2556.293378	22.119757
85.165730	2555.255855	22.124775
85.198674	2554.588029	22.129792
85.259162	2561.241051	22.134810
85.321043	2552.713373	22.139827
85.583504	2549.532335	22.144845
85.501794	2554.828310	22.149863
85.533626	2571.559832	22.154880
85.456583	2580.134202	22.159898
85.169703	2580.286241	22.164915
85.604889	2580.884477	22.169933
86.199800	2594.167180	22.174951
86.096771	2588.029029	22.179968
86.265867	2593.118698	22.184986
86.209049	2601.847731	22.190003
86.472279	2595.636773	22.195021
86.411760	2595.311725	22.200039
86.197743	2600.199094	22.205056
86.511951	2600.390101	22.210074
86.818567	2615.339907	22.215091
86.953888	2615.527206	22.220109
86.806937	2623.923119	22.225127
86.633295	2625.215794	22.230144
87.171042	2620.963014	22.235162
87.030428	2625.233002	22.240179
87.124222	2612.509110	22.245197
87.340366	2628.230461	22.250215
87.242788	2637.691747	22.255232
88.138478	2636.968495	22.260250
87.910034	2638.007752	22.265267
88.126388	2634.502493	22.270285
88.301451	2637.707090	22.275303
87.731860	2617.654009	22.280320
87.764342	2621.117504	22.285338
87.968735	2630.206699	22.290355
87.795673	2638.672961	22.295373
87.918697	2629.258348	22.300391
87.880185	2633.648151	22.305408
88.435409	2635.698414	22.310426
88.189763	2652.971867	22.315443
88.510953	2649.466063	22.320461
88.626066	2648.394092	22.325479
88.233087	2655.127218	22.330496
88.533020	2650.747344	22.335514
88.850008	2662.056658	22.340531
88.761374	2666.665727	22.345549
89.127417	2668.350942	22.350567
89.322305	2668.027157	22.355584
89.635903	2666.671798	22.360602
89.611040	2671.548672	22.365619
89.491066	2666.808104	22.370637
89.759239	2663.970165	22.375655
89.631378	2676.715316	22.380672
89.330989	2670.317509	22.385690
89.436860	2671.699223	22.390707
89.346947	2669.674486	22.395725
89.681101	2684.058285	22.400743
89.986401	2692.674174	22.405760
90.309374	2689.240674	22.410778
90.073449	2699.035980	22.415795
90.123710	2698.362297	22.420813
90.427732	2692.649923	22.425831
90.154411	2692.812477	22.430848
90.736413	2702.874945	22.435866
90.596728	2713.191803	22.440883
90.631654	2712.836113	22.445901
90.904868	2715.309019	22.450919
91.042305	2714.047361	22.455936
91.141284	2704.851064	22.460954
91.358503	2720.354561	22.465971
91.118681	2719.561927	22.470989
91.369744	2717.177959	22.476007
90.764063	2731.670251	22.481024
91.260558	2736.207174	22.486042
91.385214	2734.859135	22.491059
91.621270	2735.560969	22.496077
91.513998	2731.916714	22.501095
91.922899	2751.344933	22.506112
92.044364	2745.907137	22.511130
92.047718	2743.082012	22.516147
91.972334	2750.895596	22.521165
92.517153	2743.428818	22.526183
92.407609	2751.809499	22.531200
92.474841	2746.263373	22.536218
92.251105	2760.528950	22.541235
92.487129	2764.289014	22.546253
92.811970	2774.653514	22.551271
92.696560	2784.079780	22.556288
92.706923	2777.494685	22.561306
92.966475	2781.648753	22.566323
92.787615	2781.610393	22.571341
93.018503	2782.391935	22.576359
93.112370	2794.534556	22.581376
93.501478	2800.549473	22.586394
93.398204	2811.349910	22.591411
93.701790	2803.740770	22.596429
93.627530	2802.038656	22.601447
94.026696	2804.397282	22.606464
94.141103	2793.415360	22.611482
93.611055	2796.193235	22.616499
93.774478	2805.588724	22.621517
94.167975	2815.437588	22.626535
94.354086	2824.769589	22.631552
94.371550	2817.021939	22.636570
94.253626	2822.282603	22.641587
94.369378	2826.992447	22.646605
94.476508	2808.336081	22.651623
94.491602	2817.082427	22.656640
94.440857	2815.584951	22.661658
94.515589	2827.099359	22.666675
94.601318	2836.071422	22.671693
95.134044	2838.911074	22.676711
94.976507	2843.032257	22.681728
94.951558	2835.682556	22.686746
95.119883	2843.827496	22.691763
95.196733	2861.792616	22.696781
95.311815	2861.430756	22.701799
95.373188	2865.893434	22.706816
95.810986	2865.162564	22.711834
95.660981	2863.194502	22.716851
95.649561	2867.902064	22.721869
95.900799	2871.164277	22.726887
96.224067	2890.246185	22.731904
96.285827	2879.187193	22.736922
96.659233	2889.045537	22.741939
96.444395	2889.568248	22.746957
96.646583	2888.337526	22.751975
96.540860	2894.202280	22.756992
96.464969	2883.363549	22.762010
96.721879	2884.475590	22.767027
96.314817	2892.836379	22.772045
96.759318	2895.162711	22.777063
96.341113	2904.008122	22.782080
96.658445	2910.169964	22.787098
97.140881	2915.494987	22.792115
97.512336	2919.641133	22.797133
97.306995	2930.021991	22.802151
97.376223	2928.395364	22.807168
97.621757	2927.041115	22.812186
97.597244	2935.276086	22.817203
97.446613	2935.198613	22.822221
98.013691	2943.521378	22.827239
98.094328	2951.992474	22.832256
98.328755	2952.120161	22.837274
98.627771	2949.820224	22.842291
98.320598	2945.847254	22.847309
98.804722	2948.659774	22.852327
98.700316	2952.315076	22.857344
98.490680	2944.994085	22.862362
99.075478	2956.568030	22.867379
98.543929	2951.206594	22.872397
98.886502	2945.579665	22.877415
98.827354	2954.047276	22.882432
99.030995	2963.809005	22.887450
99.413727	2968.493100	22.892467
99.248068	2976.668007	22.897485
99.468327	2960.461939	22.902503
99.628986	2978.814952	22.907520
99.629358	2968.273594	22.912538
99.894987	2965.849453	22.917555
100.116829	2967.427749	22.922573
99.699996	2976.080460	22.927591
100.046254	2993.653440	22.932608
99.857050	2994.838100	22.937626
100.444262	2998.814961	22.942643
100.266746	2993.082781	22.947661
99.893369	2997.329131	22.952679
100.006190	2998.716100	22.957696
100.522536	3005.920065	22.962714
100.816205	3007.480869	22.967731
100.607546	3017.010146	22.972749
100.706261	3008.564888	22.977767
100.809848	3011.749120	22.982784
100.586526	3017.259802	22.987802
100.794172	3032.269551	22.992819
100.591059	3039.468768	22.997837
101.215647	3032.822666	23.002855
101.298942	3040.040413	23.007872
101.602557	3054.202025	23.012890
101.856368	3057.037797	23.017907
101.492226	3069.523338	23.022925
101.943117	3061.872219	23.027943
101.898382	3055.617524	23.032960
101.743503	3072.580573	23.037978
101.794979	3070.123482	23.042995
101.950730	3077.348900	23.048013
101.934878	3081.728972	23.053031
102.369240	3078.921904	23.058048
102.648634	3093.219875	23.063066
103.155652	3096.865226	23.068083
103.341193	3095.813825	23.073101
103.387539	3096.990224	23.078119
103.020869	3099.565965	23.083136
103.288293	3096.339873	23.088154
103.455853	3092.775844	23.093171
103.138535	3092.831630	23.098189
103.493573	3093.499173	23.103207
103.862912	3092.283443	23.108224
103.592661	3092.252998	23.113242
104.033830	3086.954691	23.118259
103.953713	3089.690964	23.123277
103.981473	3082.512855	23.128295
104.114567	3087.390497	23.133312
104.458549	3098.844223	23.138330
104.380142	3093.030302	23.143347
104.334923	3106.555076	23.148365
104.608471	3104.978681	23.153383
104.669164	3111.234203	23.158400
104.616901	3111.485430	23.163418
104.750259	3106.645338	23.168435
104.466447	3108.299217	23.173453
104.857024	3124.460951	23.178471
104.733982	3134.387256	23.183488
104.997999	3138.834233	23.188506
105.414404	3126.640477	23.193523
105.022487	3132.890728	23.198541
105.458668	3150.828597	23.203559
105.739580	3160.818269	23.208576
105.326115	3161.428723	23.213594
105.672263	3157.439203	23.218611
105.844243	3162.781076	23.223629
106.230966	3171.693820	23.228647
106.287607	3172.802341	23.233664
106.279729	3184.531833	23.238682
106.724170	3181.893612	23.243699
106.348161	3184.107863	23.248717
106.699024	3178.388043	23.253735
106.560899	3184.920724	23.258752
106.414839	3189.579898	23.263770
106.691441	3199.002157	23.268787
106.569083	3208.199329	23.273805
106.695979	3203.461213	23.278823
107.448870	3206.367643	23.283840
107.215829	3234.294821	23.288858
107.545960	3225.153798	23.293875
107.666097	3238.851763	23.298893
107.778094	3226.506497	23.303911
107.822840	3229.602088	23.308928
107.811346	3231.677534	23.313946
107.954144	3228.268828	23.318963
108.237354	3222.982451	23.323981
108.264832	3224.704652	23.328999
108.348260	3231.237573	23.334016
108.226654	3248.975175	23.339034
108.424686	3245.822983	23.344051
108.689700	3248.928469	23.349069
108.741190	3247.942116	23.354087
108.624881	3240.549663	23.359104
108.454481	3245.793372	23.364122
108.981768	3255.956199	23.369139
109.030546	3265.953666	23.374157
109.367870	3262.953373	23.379175
109.594479	3258.865666	23.384192
109.496332	3269.015412	23.389210
109.546776	3265.633703	23.394227
109.203171	3267.369497	23.399245
109.463725	3281.534836	23.404263
109.533845	3286.895761	23.409280
109.173934	3290.250046	23.414298
109.723348	3308.533401	23.419315
109.784047	3317.560101	23.424333
110.093552	3322.959513	23.429351
110.193431	3317.540687	23.434368
110.617232	3338.456929	23.439386
110.990839	3338.780726	23.444403
111.180530	3333.931802	23.449421
111.304492	3325.876986	23.454439
111.524803	3320.496219	23.459456
111.670935	3325.387678	23.464474
111.773265	3324.043071	23.469491
111.938913	3326.883144	23.474509
111.956264	3316.370500	23.479527
112.037175	3298.869706	23.484544
111.718724	3303.300100	23.489562
111.720457	3309.274504	23.494579
111.803858	3316.075734	23.499597
112.052424	3315.535274	23.504615
112.290219	3317.511949	23.509632
111.411183	3317.046052	23.514650
112.036807	3328.276173	23.519667
112.288822	3335.373086	23.524685
112.324625	3340.540532	23.529703
112.123987	3344.690632	23.534720
112.504283	3355.154144	23.539738
112.658182	3363.323660	23.544755
112.820357	3362.850304	23.549773
112.885054	3371.791191	23.554791
113.417622	3378.257394	23.559808
113.531138	3385.540011	23.564826
113.542415	3381.829824	23.569843
113.800388	3386.634451	23.574861
113.873737	3384.685211	23.579879
113.895855	3385.373038	23.584896
113.858467	3386.865485	23.589914
113.854538	3399.033209	23.594931
113.940804	3409.299506	23.599949
114.008226	3405.309142	23.604967
114.460739	3403.023124	23.609984
114.174781	3411.930253	23.615002
114.291079	3431.392141	23.620019
114.364664	3437.948763	23.625037
114.601746	3440.288523	23.630055
115.198196	3438.065308	23.635072
114.926887	3462.350253	23.640090
114.952176	3453.490134	23.645107
115.218571	3448.935387	23.650125
115.103680	3459.861112	23.655143
115.158867	3458.965701	23.660160
115.362349	3481.481879	23.665178
115.823263	3481.637433	23.670195
116.125573	3481.994427	23.675213
115.653078	3489.892251	23.680231
116.059587	3486.420346	23.685248
116.304745	3505.745472	23.690266
116.114539	3508.902941	23.695283
116.835003	3508.977055	23.700301
116.606055	3509.028550	23.705319
117.024289	3516.528898	23.710336
116.935459	3511.455014	23.715354
116.720843	3509.351755	23.720371
117.146757	3513.887242	23.725389
116.914360	3511.218636	23.730407
116.910881	3513.936729	23.735424
117.388937	3524.492431	23.740442
117.290198	3520.426913	23.745459
117.589711	3534.933568	23.750477
117.199861	3536.572433	23.755495
117.753622	3543.215299	23.760512
117.758252	3556.862054	23.765530
118.252239	3555.226050	23.770547
118.455836	3540.537032	23.775565
117.841935	3549.280666	23.780583
117.961356	3552.453060	23.785600
118.611296	3572.169728	23.790618
118.825101	3575.756675	23.795635
118.679156	3578.244463	23.800653
118.940094	3572.216587	23.805671
118.943771	3575.798375	23.810688
119.002800	3596.935833	23.815706
119.020795	3592.403943	23.820723
119.592692	3591.216612	23.825741
119.314021	3590.881324	23.830759
119.905743	3601.990647	23.835776
120.136866	3614.551166	23.840794
120.449353	3622.573016	23.845811
120.494871	3613.870636	23.850829
120.249464	3626.953537	23.855847
120.275185	3616.587757	23.860864
120.227683	3616.715158	23.865882
120.432009	3614.893843	23.870899
120.346235	3612.256050	23.875917
120.456406	3629.443478	23.880935
120.768419	3625.373953	23.885952
120.812317	3641.501755	23.890970
120.768472	3637.522351	23.895987
121.311441	3641.828179	23.901005
120.965007	3670.130337	23.906023
121.355717	3661.724530	23.911040
121.381317	3665.069363	23.916058
121.430516	3671.879208	23.921075
121.694888	3671.816023	23.926093
121.804546	3688.962556	23.931111
122.220551	3682.557004	23.936128
122.541564	3677.166766	23.941146
122.243605	3686.325240	23.946163
122.817340	3682.338047	23.951181
122.791405	3684.005484	23.956199
123.137346	3677.074284	23.961216
123.255968	3689.974305	23.966234
123.130346	3692.853472	23.971251
123.085970	3699.125557	23.976269
123.476440	3698.263152	23.981287
123.447789	3699.804763	23.986304
123.563802	3699.540585	23.991322
123.614942	3709.310682	23.996339
123.664257	3695.153711	24.001357
123.559090	3705.004954	24.006375
123.294347	3705.232459	24.011392
123.684150	3721.738880	24.016410
124.056808	3726.576242	24.021427
124.113100	3716.849516	24.026445
124.017739	3729.536695	24.031463
124.109570	3741.935928	24.036480
124.745365	3744.879618	24.041498
124.562982	3753.111136	24.046515
124.720327	3755.049886	24.051533
124.660846	3755.188621	24.056551
125.093630	3767.184445	24.061568
124.997563	3773.158449	24.066586
124.972518	3772.619544	24.071603
125.432556	3769.656875	24.076621
125.468274	3788.254259	24.081639
125.894949	3792.805480	24.086656
126.318388	3790.789065	24.091674
125.676652	3793.373011	24.096691
125.740879	3792.147927	24.101709
126.187479	3805.375716	24.106727
126.039237	3816.508848	24.111744
126.384127	3815.110660	24.116762
126.420696	3822.812590	24.121779
126.932786	3823.067493	24.126797
126.741832	3834.327224	24.131815
126.630060	3839.429413	24.136832
126.717381	3836.054481	24.141850
127.121804	3846.208367	24.146867
127.750928	3852.467178	24.151885
127.253045	3854.217578	24.156903
127.987118	3860.933490	24.161920
127.620943	3861.142070	24.166938
127.787117	3859.108890	24.171955
128.402220	3871.395179	24.176973
127.828451	3886.603051	24.181991
128.269283	3882.090475	24.187008
128.559180	3881.874972	24.192026
128.382458	3879.418581	24.197043
128.122698	3886.554360	24.202061
128.813881	3906.586913	24.207079
128.907568	3901.812754	24.212096
129.142006	3903.490173	24.217114
129.214432	3908.743610	24.222131
129.369867	3913.441249	24.227149
129.309174	3921.773835	24.232167
129.655941	3933.309722	24.237184
129.670314	3934.740499	24.242202
129.811012	3927.866409	24.247219
130.067572	3934.473630	24.252237
130.304122	3946.894659	24.257255
130.072339	3951.942971	24.262272
130.495234	3949.753030	24.267290
130.285014	3950.581208	24.272307
130.885960	3951.223126	24.277325
130.868858	3956.600986	24.282343
130.944646	3958.978552	24.287360
131.284514	3962.085135	24.292378
131.020194	3973.201717	24.297395
131.246159	3969.385390	24.302413
131.270496	3973.762577	24.307431
131.444825	3979.369454	24.312448
131.717364	3997.418866	24.317466
131.411712	3999.275070	24.322483
131.645265	4001.659642	24.327501
131.803259	4011.504799	24.332519
132.310254	4019.199853	24.337536
132.586453	4016.249985	24.342554
132.597729	4021.096347	24.347571
132.768477	4025.744286	24.352589
132.766257	4023.162862	24.357607
132.688550	4026.400750	24.362624
132.848023	4032.862153	24.367642
133.070738	4041.750364	24.372659
133.292644	4049.262565	24.377677
133.153274	4049.053924	24.382695
133.302447	4048.538387	24.387712
133.417029	4049.221313	24.392730
133.599552	4065.166939	24.397747
133.939788	4062.630037	24.402765
134.001095	4063.614792	24.407783
133.613498	4063.460579	24.412800
134.158760	4069.025514	24.417818
133.980242	4089.818623	24.422835
134.345458	4080.719051	24.427853
134.303355	4098.047416	24.432871
134.283926	4105.726622	24.437888
134.610081	4109.760160	24.442906
134.874729	4122.224280	24.447923
134.847379	4126.505394	24.452941
135.127452	4131.420406	24.457959
135.536755	4145.531704	24.462976
136.068720	4149.697335	24.467994
135.927909	4157.711092	24.473011
136.096063	4160.285777	24.478029
136.296129	4156.542882	24.483047
136.092651	4163.329126	24.488064
136.414606	4158.026976	24.493082
136.417888	4166.248713	24.498099
136.528905	4169.577184	24.503117
136.912395	4178.882314	24.508135
136.857970	4185.790551	24.513152
137.205061	4177.463892	24.518170
137.032671	4183.001718	24.523187
137.468644	4189.959858	24.528205
137.501423	4200.544251	24.533223
137.457174	4207.839138	24.538240
137.566207	4207.225688	24.543258
137.592921	4214.547406	24.548275
137.954637	4223.792823	24.553293
137.984139	4227.676883	24.558311
137.956385	4228.489290	24.563328
138.076686	4240.190042	24.568346
138.263349	4246.581006	24.573363
138.583273	4255.182744	24.578381
138.876170	4262.251564	24.583399
138.865940	4271.201407	24.588416
139.224757	4275.775941	24.593434
138.868271	4277.299204	24.598451
139.239351	4274.662781	24.603469
139.503290	4291.549142	24.608487
139.951695	4302.302454	24.613504
140.353576	4297.073040	24.618522
140.345234	4304.384470	24.623539
140.388883	4303.490814	24.628557
140.245044	4305.369201	24.633575
140.567719	4309.542204	24.638592
140.604145	4293.164715	24.643610
140.296433	4306.380903	24.648627
140.753579	4314.620421	24.653645
140.867794	4326.738813	24.658663
140.806146	4323.718399	24.663680
141.242035	4330.007463	24.668698
141.121547	4347.821721	24.673715
141.534750	4340.478942	24.678733
141.443601	4347.503430	24.683751
141.444949	4356.385228	24.688768
141.549162	4367.129040	24.693786
141.606361	4376.762832	24.698803
142.055634	4373.817524	24.703821
142.448944	4385.526367	24.708839
142.322359	4399.711828	24.713856
143.168166	4396.013539	24.718874
143.064127	4399.100933	24.723891
142.871316	4402.284213	24.728909
142.935703	4394.550675	24.733927
142.815504	4398.101410	24.738944
143.202677	4403.059794	24.743962
143.038773	4405.083350	24.748979
143.173187	4418.495918	24.753997
143.499013	4412.315626	24.759015
143.570986	4441.787980	24.764032
144.011931	4433.702257	24.769050
143.982040	4443.277047	24.774067
143.966351	4452.240454	24.779085
144.490085	4461.157759	24.784103
144.369407	4469.086453	24.789120
144.406032	4471.981515	24.794138
144.584633	4484.673915	24.799155
144.604352	4493.161532	24.804173
145.255443	4488.953802	24.809191
145.241377	4507.499706	24.814208
145.261504	4514.955138	24.819226
145.947288	4521.539938	24.824243
145.377655	4515.117106	24.829261
146.000996	4528.788208	24.834279
145.813035	4541.720788	24.839296
146.242617	4544.611496	24.844314
146.583510	4542.087052	24.849331
146.637271	4531.448090	24.854349
146.821901	4531.662455	24.859367
146.981264	4549.057732	24.864384
147.503128	4557.239940	24.869402
147.345781	4547.640721	24.874419
147.526939	4550.737396	24.879437
147.849507	4544.885829	24.884455
147.563063	4553.386421	24.889472
147.850665	4552.473710	24.894490
147.890307	4554.894860	24.899507
148.153146	4562.460872	24.904525
148.544334	4565.183961	24.909543
147.993710	4577.810047	24.914560
148.286056	4577.246954	24.919578
148.378082	4583.722212	24.924595
148.856148	4590.355159	24.929613
148.811969	4600.497249	24.934631
148.796059	4609.047282	24.939648
148.994019	4607.192141	24.944666
149.221206	4630.264741	24.949683
148.916424	4638.020164	24.954701
149.203536	4638.092319	24.959719
149.344094	4649.487168	24.964736
149.814339	4664.713060	24.969754
149.818346	4671.056858	24.974771
150.111286	4684.918402	24.979789
150.131310	4678.043877	24.984807
150.300637	4694.544483	24.989824
150.469152	4698.132393	24.994842
150.791502	4710.474305	24.999859
150.508411	4714.183032	25.004877
151.359091	4718.554845	25.009895
151.119287	4729.333494	25.014912
151.473912	4738.274108	25.019930
151.856263	4725.544836	25.024947
151.517097	4736.638817	25.029965
151.663609	4738.266877	25.034983
151.824167	4748.576027	25.040000
152.150833	4755.712381	25.045018
152.361718	4750.462073	25.050035
152.501371	4757.043608	25.055053
152.663018	4761.970918	25.060071
152.799167	4778.767156	25.065088
152.665665	4780.691328	25.070106
153.205761	4778.738712	25.075123
153.034201	4784.513322	25.080141
153.324247	4788.565261	25.085159
153.184034	4798.564592	25.090176
153.777594	4798.727919	25.095194
153.640981	4797.679232	25.100211
153.582024	4809.152591	25.105229
154.087381	4810.191353	25.110247
154.288239	4813.240816	25.115264
154.459391	4825.672632	25.120282
154.832378	4827.192842	25.125299
154.740244	4838.955463	25.130317
155.075880	4844.837356	25.135335
154.938282	4852.169130	25.140352
154.996272	4843.341117	25.145370
155.084589	4843.343218	25.150387
155.095366	4865.654393	25.155405
155.815597	4862.212296	25.160423
156.116161	4871.748489	25.165440
156.092693	4884.510507	25.170458
156.465316	4881.848506	25.175475
156.399133	4878.481497	25.180493
156.339294	4883.165558	25.185511
156.316300	4884.715859	25.190528
156.628255	4913.378291	25.195546
157.225176	4899.144591	25.200563
156.955731	4901.197260	25.205581
157.368652	4909.879525	25.210599
157.025701	4931.731353	25.215616
157.466992	4924.084106	25.220634
157.966110	4917.308504	25.225651
157.836390	4939.670051	25.230669
157.849399	4951.530007	25.235687
158.041608	4950.291234	25.240704
158.583874	4961.349127	25.245722
158.677049	4972.164457	25.250739
158.321513	4984.116535	25.255757
159.033937	4987.332584	25.260775
158.980353	4986.561353	25.265792
159.357735	4995.773163	25.270810
159.539265	4999.431706	25.275827
159.304455	5005.333022	25.280845
159.746802	5007.129686	25.285863
159.431901	5013.068726	25.290880
159.692394	5025.357354	25.295898
159.863424	5024.573246	25.300915
159.898585	5048.575866	25.305933
160.170982	5052.027728	25.310951
160.688680	5055.359331	25.315968
160.567681	5061.129314	25.320986
161.132269	5065.189075	25.326003
160.998464	5083.315461	25.331021
161.238107	5082.574328	25.336039
161.160639	5087.662057	25.341056
161.672948	5100.710118	25.346074
161.746001	5110.935248	25.351091
161.683181	5111.955168	25.356109
161.911783	5113.201174	25.361127
162.235163	5129.081617	25.366144
162.260547	5133.724066	25.371162
162.321738	5138.383036	25.376179
162.494150	5144.460889	25.381197
163.111647	5148.550309	25.386215
162.943790	5141.341865	25.391232
163.186697	5149.899205	25.396250
163.057455	5146.923898	25.401267
163.468574	5164.154310	25.406285
163.589661	5167.260444	25.411303
163.764104	5178.685072	25.416320
163.622037	5175.913772	25.421338
163.845748	5181.813200	25.426355
163.661196	5204.571857	25.431373
164.093341	5193.223362	25.436391
164.481619	5208.247832	25.441408
164.633585	5221.437307	25.446426
165.127669	5225.624872	25.451443
164.953427	5239.092415	25.456461
165.377724	5238.956982	25.461479
165.129505	5239.589117	25.466496
165.451531	5246.641163	25.471514
166.036611	5266.622304	25.476531
165.871492	5273.601849	25.481549
165.929181	5267.090548	25.486567
166.415362	5274.688373	25.491584
166.569359	5287.028481	25.496602
166.919114	5295.932252	25.501619
166.522184	5300.410069	25.506637
166.632387	5292.145036	25.511655
167.307154	5315.145668	25.516672
167.246324	5326.083038	25.521690
167.457221	5324.904460	25.526707
167.403051	5336.418441	25.531725
167.795391	5347.607234	25.536743
168.180098	5346.909793	25.541760
168.084943	5356.788781	25.546778
168.487672	5362.811910	25.551795
168.304804	5371.931216	25.556813
168.700010	5374.398126	25.561831
168.941402	5377.662330	25.566848
168.810035	5393.039318	25.571866
169.052937	5396.063395	25.576883
169.359647	5383.515893	25.581901
169.750765	5399.509131	25.586919
170.291487	5415.646387	25.591936
170.379563	5418.069581	25.596954
170.323988	5410.796201	25.601971
170.364209	5419.767164	25.606989
170.488989	5406.941788	25.612007
170.724220	5412.482811	25.617024
170.531717	5416.704715	25.622042
171.087622	5428.139554	25.627059
170.994853	5445.006770	25.632077
171.139397	5437.557023	25.637095
170.795359	5443.358694	25.642112
171.445650	5457.180975	25.647130
171.599718	5452.709505	25.652147
171.472019	5478.707724	25.657165
171.506124	5477.673453	25.662183
171.978167	5488.130234	25.667200
172.131388	5508.447184	25.672218
172.505460	5510.005163	25.677236
172.550391	5520.032883	25.682253
173.054031	5531.876805	25.687271
173.435122	5534.582675	25.692288
173.400389	5536.942935	25.697306
173.474545	5544.756537	25.702324
173.958837	5554.034057	25.707341
174.012979	5555.263064	25.712359
174.271456	5548.319520	25.717376
174.150643	5551.135100	25.722394
174.257661	5542.406438	25.727412
174.188775	5551.918439	25.732429
174.393275	5563.976253	25.737447
174.550283	5569.879880	25.742464
174.692113	5575.347111	25.747482
174.796267	5588.171823	25.752500
175.254755	5592.611227	25.757517
175.311247	5597.908671	25.762535
175.394813	5607.005553	25.767552
175.619168	5621.481394	25.772570
175.921537	5629.180587	25.777588
175.805778	5636.427206	25.782605
176.355333	5636.003963	25.787623
176.704295	5635.624576	25.792640
176.674425	5658.407066	25.797658
176.560786	5664.618012	25.802676
176.972660	5666.501559	25.807693
176.902403	5676.613587	25.812711
177.472540	5682.500279	25.817728
177.607842	5687.772853	25.822746
177.642994	5704.317362	25.827764
177.720021	5712.809252	25.832781
177.749712	5711.409492	25.837799
178.043470	5723.081039	25.842816
178.353018	5736.745094	25.847834
178.542425	5736.232717	25.852852
178.631919	5760.205721	25.857869
179.063445	5771.546504	25.862887
179.148396	5770.605311	25.867904
179.275199	5778.123567	25.872922
179.587405	5788.400229	25.877940
179.766420	5781.730965	25.882957
180.338372	5790.208969	25.887975
180.877627	5794.585342	25.892992
180.871928	5804.308599	25.898010
180.976879	5792.663448	25.903028
181.561460	5795.135655	25.908045
181.115469	5804.655994	25.913063
181.453579	5797.131772	25.918080
181.456989	5800.609873	25.923098
181.389348	5794.152619	25.928116
181.456707	5815.354499	25.933133
181.826410	5824.833081	25.938151
181.921798	5818.416725	25.943168
181.853317	5834.810188	25.948186
182.075593	5835.283863	25.953204
182.278486	5852.070702	25.958221
182.559597	5873.226743	25.963239
183.079169	5877.637768	25.968256
183.168441	5880.461726	25.973274
183.124877	5888.931438	25.978292
183.506754	5902.508598	25.983309
183.295686	5912.614270	25.988327
183.687070	5915.091319	25.993344
183.918930	5928.047906	25.998362
184.234007	5929.176337	26.003380
184.809168	5939.390049	26.008397
184.572327	5950.787654	26.013415
184.975725	5947.202133	26.018432
184.862006	5960.408256	26.023450
184.738452	5957.573979	26.028468
185.179587	5962.767451	26.033485
185.359989	5986.695033	26.038503
185.550498	5985.061877	26.043520
185.802119	5988.012094	26.048538
185.963846	6001.175362	26.053556
186.271434	6001.250651	26.058573
185.887280	6009.391493	26.063591
186.151591	6021.178298	26.068608
186.252986	6027.557914	26.073626
186.672106	6043.001262	26.078644
186.691649	6052.919589	26.083661
186.550462	6070.378899	26.088679
187.270915	6081.274000	26.093696
187.735002	6083.985972	26.098714
187.559477	6087.577216	26.103732
187.997605	6103.503779	26.108749
187.854151	6113.734771	26.113767
188.097524	6118.002614	26.118784
188.295179	6135.443954	26.123802
188.366571	6138.962043	26.128820
188.639622	6156.369568	26.133837
188.851823	6168.454994	26.138855
189.004909	6170.678767	26.143872
189.292616	6182.727193	26.148890
189.062348	6195.080393	26.153908
189.363101	6199.642362	26.158925
189.657829	6218.605962	26.163943
190.112188	6228.595581	26.168960
190.520130	6237.118269	26.173978
191.025771	6242.061873	26.178996
191.362353	6248.749026	26.184013
191.528308	6267.151898	26.189031
191.700519	6259.145092	26.194048
191.444821	6257.129978	26.199066
191.906241	6256.856182	26.204084
192.154725	6260.109972	26.209101
191.955968	6280.432076	26.214119
192.772084	6275.181803	26.219136
192.278170	6278.920511	26.224154
192.334241	6299.824826	26.229172
192.945830	6302.453890	26.234189
192.793012	6304.460145	26.239207
193.203844	6310.848504	26.244224
193.473000	6328.790280	26.249242
193.216884	6331.241929	26.254260
193.854915	6346.430485	26.259277
193.763614	6356.918654	26.264295
194.100689	6351.935499	26.269312
194.205404	6364.088296	26.274330
194.297828	6375.586423	26.279348
194.661009	6387.894709	26.284365
194.712387	6393.808736	26.289383
194.665583	6403.835440	26.294400
194.866047	6415.884977	26.299418
194.881742	6434.784917	26.304436
195.668364	6440.859122	26.309453
195.395896	6456.334733	26.314471
195.933935	6471.785184	26.319488
196.180620	6476.936474	26.324506
196.241441	6488.130234	26.329524
196.708383	6511.695065	26.334541
196.262048	6510.498782	26.339559
196.737150	6520.523212	26.344576
197.134415	6540.377161	26.349594
197.172234	6549.671038	26.354612
197.538281	6555.403544	26.359629
197.524153	6564.661323	26.364647
197.653972	6586.274217	26.369664
198.151877	6594.325341	26.374682
198.480118	6614.723603	26.379700
199.117636	6613.866802	26.384717
199.136035	6634.843657	26.389735
199.342544	6616.635102	26.394752
199.377005	6631.365438	26.399770
199.804114	6644.790899	26.404788
200.244211	6645.716822	26.409805
200.121819	6644.173362	26.414823
200.243173	6645.294120	26.419840
200.313296	6644.090025	26.424858
200.307121	6644.068958	26.429876
200.503660	6651.791376	26.434893
200.652369	6662.788469	26.439911
201.135803	6671.997247	26.444928
201.110146	6677.579274	26.449946
201.136432	6689.413040	26.454964
201.639610	6698.271516	26.459981
201.394374	6720.429099	26.464999
201.897466	6715.773556	26.470016
202.507754	6717.430605	26.475034
202.142689	6734.164626	26.480052
203.040396	6738.618007	26.485069
202.899633	6735.104429	26.490087
203.354960	6750.280729	26.495104
204.126939	6744.863575	26.500122
204.208129	6746.549338	26.505140
204.193849	6728.949576	26.510157
204.374788	6731.951957	26.515175
204.474962	6737.157698	26.520192
204.624566	6740.382775	26.525210
204.548448	6756.850858	26.530228
204.665397	6754.597736	26.535245
204.449993	6763.921677	26.540263
205.078747	6780.845100	26.545280
205.306573	6784.386309	26.550298
205.541466	6800.102052	26.555316
205.829682	6807.974415	26.560333
205.687547	6818.748558	26.565351
205.908553	6828.661194	26.570368
206.268849	6834.593560	26.575386
206.322020	6834.790541	26.580404
206.940892	6847.324499	26.585421
206.774609	6863.620466	26.590439
207.324859	6869.684266	26.595456
207.637365	6879.027091	26.600474
207.489260	6887.624028	26.605492
207.827459	6895.198223	26.610509
208.035051	6914.621218	26.615527
208.228479	6914.038736	26.620544
208.585399	6921.385895	26.625562
208.617266	6937.884680	26.630580
209.074868	6946.614631	26.635597
208.873893	6945.247533	26.640615
209.128460	6963.968773	26.645632
209.619959	6962.437041	26.650650
209.929688	6980.120596	26.655668
210.035157	6980.517785	26.660685
210.346492	6986.650388	26.665703
210.198997	6985.041357	26.670720
210.474420	7004.185560	26.675738
210.700911	7018.109737	26.680756
211.078026	7018.654042	26.685773
210.938047	7033.664404	26.690791
211.470839	7032.321958	26.695808
211.849076	7049.230968	26.700826
211.998684	7052.033087	26.705844
212.594750	7059.099995	26.710861
212.258141	7066.362623	26.715879
212.455076	7076.099203	26.720896
212.667131	7089.599512	26.725914
212.907935	7081.319652	26.730932
213.259321	7091.625675	26.735949
213.810454	7102.806612	26.740967
213.739509	7107.852848	26.745984
213.882176	7111.492614	26.751002
213.771256	7107.945905	26.756020
214.001130	7113.403048	26.761037
214.576117	7116.015834	26.766055
214.501739	7135.413513	26.771072
214.626311	7125.626985	26.776090
214.812189	7146.575195	26.781108
214.916115	7154.981491	26.786125
215.551050	7163.462960	26.791143
215.021746	7174.341785	26.796160
215.547721	7187.512335	26.801178
215.939657	7204.416198	26.806196
216.212237	7210.015092	26.811213
216.033129	7220.293290	26.816231
216.491622	7233.477536	26.821248
216.316633	7240.007938	26.826266
216.534381	7259.028799	26.831284
216.914745	7268.497003	26.836301
217.227166	7284.030622	26.841319
217.332784	7302.529165	26.846336
217.503313	7306.701296	26.851354
217.781427	7327.114471	26.856372
217.853483	7340.450507	26.861389
218.105903	7355.362156	26.866407
218.120372	7363.671985	26.871424
219.107078	7380.417118	26.876442
218.961920	7398.929546	26.881460
219.582378	7412.650627	26.886477
219.727466	7418.515670	26.891495
220.031822	7439.281611	26.896512
220.560162	7443.259163	26.901530
220.747838	7446.292182	26.906548
220.781323	7445.873487	26.911565
221.342357	7459.537561	26.916583
221.338073	7467.926122	26.921600
221.659130	7469.195782	26.926618
221.487598	7479.498200	26.931636
221.610275	7491.260652	26.936653
222.057289	7493.426199	26.941671
222.052704	7511.399126	26.946688
222.516666	7517.097750	26.951706
222.535336	7531.124123	26.956724
222.776017	7539.796581	26.961741
223.183441	7550.993853	26.966759
222.969148	7567.891414	26.971776
223.421204	7576.445744	26.976794
222.994240	7576.805878	26.981812
223.393121	7594.823406	26.986829
224.293190	7609.725981	26.991847
224.243935	7623.358916	26.996864
224.782870	7632.477461	27.001882
224.978353	7651.347506	27.006900
225.229363	7653.912947	27.011917
225.968687	7660.512662	27.016935
226.061576	7669.618589	27.021952
226.508920	7657.240212	27.026970
226.612970	7652.580266	27.031988
226.743062	7658.075205	27.037005
226.996854	7666.632033	27.042023
227.090048	7683.683871	27.047040
227.416891	7683.882450	27.052058
227.396167	7687.506729	27.057076
227.368790	7692.031765	27.062093
227.859354	7700.163445	27.067111
227.872556	7710.367779	27.072128
228.414547	7722.377632	27.077146
228.322917	7730.284274	27.082164
228.509516	7738.267566	27.087181
228.812629	7746.362155	27.092199
228.583037	7754.703845	27.097216
228.964216	7754.249953	27.102234
229.305428	7768.065288	27.107252
229.501616	7790.881530	27.112269
229.829319	7794.716766	27.117287
229.768193	7797.652831	27.122304
229.808950	7808.998897	27.127322
229.911120	7830.346065	27.132340
230.049676	7841.377015	27.137357
230.546249	7856.115312	27.142375
230.768207	7873.807080	27.147392
231.204833	7892.298879	27.152410
231.707226	7903.743608	27.157428
231.572218	7909.851303	27.162445
231.761866	7924.577457	27.167463
232.333881	7941.371884	27.172480
232.488950	7948.255240	27.177498
232.829300	7946.484934	27.182516
233.134459	7974.670214	27.187533
233.040031	7971.483822	27.192551
233.324595	7999.366120	27.197568
234.066815	7993.820648	27.202586
234.299293	8002.245201	27.207604
233.993455	8012.272071	27.212621
234.686726	8015.649504	27.217639
234.629724	8030.654073	27.222656
235.295996	8036.911717	27.227674
235.120089	8044.815830	27.232692
235.281022	8059.013033	27.237709
236.093570	8066.191851	27.242727
235.675624	8085.034723	27.247744
236.145510	8096.705622	27.252762
236.156930	8098.926432	27.257780
236.486292	8119.357765	27.262797
236.788967	8126.641244	27.267815
236.930060	8144.800470	27.272832
237.406740	8149.736477	27.277850
237.622049	8163.417018	27.282868
237.789429	8175.848546	27.287885
238.041958	8188.244726	27.292903
238.022797	8196.440200	27.297920
238.250899	8212.559150	27.302938
238.482071	8228.526100	27.307956
238.635988	8249.490013	27.312973
239.559670	8257.311420	27.317991
239.942191	8265.125530	27.323008
239.655870	8273.318434	27.328026
240.024317	8279.335241	27.333044
240.202358	8296.756436	27.338061
240.263559	8307.007297	27.343079
240.728723	8319.591452	27.348096
240.978926	8335.148275	27.353114
241.170568	8342.269176	27.358132
241.314855	8353.406880	27.363149
241.549616	8376.107346	27.368167
241.922560	8379.768339	27.373184
241.751842	8399.314943	27.378202
242.121611	8406.547046	27.383220
242.760922	8422.074933	27.388237
243.063691	8422.987606	27.393255
242.944945	8440.833988	27.398272
243.025309	8449.765457	27.403290
243.444262	8459.382965	27.408308
243.962095	8472.953496	27.413325
244.317452	8476.503593	27.418343
244.501261	8489.245322	27.423360
244.074481	8491.708039	27.428378
245.002046	8507.219535	27.433396
245.359261	8505.130846	27.438413
245.728285	8501.887993	27.443431
245.798765	8507.060976	27.448448
246.182102	8533.375433	27.453466
246.751147	8528.816511	27.458484
246.334266	8530.725207	27.463501
246.720726	8515.927956	27.468519
246.747467	8544.621542	27.473536
246.894008	8552.541969	27.478554
247.344310	8565.362230	27.483572
247.335238	8575.838861	27.488589
247.669292	8584.573045	27.493607
248.030441	8606.073373	27.498624
247.967637	8610.856716	27.503642
248.338425	8620.352367	27.508660
248.483748	8643.332280	27.513677
248.692583	8654.371719	27.518695
248.762593	8664.337269	27.523712
249.284491	8683.283836	27.528730
249.693878	8684.252537	27.533748
249.822592	8711.361433	27.538765
250.514800	8716.980699	27.543783
250.729385	8725.294714	27.548800
251.040203	8733.881046	27.553818
251.190359	8740.140359	27.558836
251.378785	8743.874352	27.563853
251.787643	8753.825081	27.568871
251.734859	8762.095497	27.573888
251.911908	8772.754789	27.578906
252.378202	8778.642871	27.583924
252.568538	8800.163705	27.588941
252.453141	8801.675051	27.593959
252.503200	8820.527893	27.598976
252.700277	8843.970407	27.603994
253.300756	8864.717111	27.609012
253.334584	8881.804556	27.614029
254.001783	8885.700823	27.619047
254.070126	8916.759507	27.624064
254.016358	8918.652751	27.629082
254.469333	8939.210976	27.634100
254.877330	8955.602495	27.639117
255.429390	8972.018957	27.644135
255.609098	8976.082697	27.649152
255.732950	9003.511649	27.654170
256.296336	9000.702551	27.659188
256.264236	9016.591200	27.664205
256.509323	9023.170486	27.669223
256.623510	9044.046772	27.674240
257.011482	9049.372534	27.679258
257.428764	9069.879632	27.684276
257.560288	9093.518941	27.689293
258.017571	9098.846556	27.694311
258.273439	9116.385850	27.699328
258.532704	9118.574511	27.704346
258.892301	9138.086688	27.709364
258.822147	9150.716869	27.714381
259.235423	9156.783814	27.719399
259.910401	9172.758258	27.724416
259.752131	9182.567041	27.729434
259.977623	9187.700294	27.734452
260.468858	9197.013318	27.739469
260.376200	9218.925986	27.744487
260.516572	9228.937715	27.749504
260.837288	9244.714801	27.754522
261.294980	9252.233481	27.759540
261.333963	9262.867193	27.764557
261.757108	9280.225898	27.769575
261.979811	9285.807934	27.774592
262.567464	9289.053663	27.779610
262.665859	9301.304100	27.784628
262.740395	9313.138353	27.789645
263.123479	9325.909621	27.794663
263.041116	9330.011083	27.799680
263.343705	9354.025055	27.804698
263.656969	9357.547148	27.809716
263.781955	9373.092768	27.814733
263.975376	9384.618095	27.819751
264.440946	9406.775582	27.824768
264.390373	9424.523896	27.829786
265.326874	9423.431000	27.834804
264.895742	9443.919054	27.839821
265.161101	9458.539928	27.844839
265.718377	9471.429410	27.849856
266.215369	9497.497068	27.854874
266.567989	9511.097243	27.859892
266.676275	9519.614441	27.864909
266.706902	9530.489557	27.869927
267.174685	9538.391965	27.874944
267.909733	9559.863607	27.879962
268.350406	9564.445678	27.884980
268.110772	9573.095999	27.889997
268.407370	9589.426493	27.895015
268.587950	9591.987386	27.900032
269.119515	9614.602119	27.905050
269.128648	9617.549634	27.910068
269.263970	9626.978274	27.915085
269.409658	9637.923942	27.920103
270.088160	9665.750581	27.925120
270.001035	9671.238893	27.930138
270.407530	9691.558925	27.935156
270.728953	9703.175026	27.940173
271.270917	9719.337987	27.945191
271.602047	9723.308857	27.950208
271.601585	9748.014602	27.955226
272.385674	9752.732692	27.960244
272.096292	9769.517659	27.965261
272.301650	9779.222785	27.970279
272.968316	9785.600946	27.975296
273.168413	9801.763529	27.980314
273.456130	9815.977073	27.985332
273.337559	9835.791755	27.990349
272.978328	9845.723734	27.995367
274.338190	9860.597602	28.000384
274.044458	9885.863827	28.005402
274.745456	9885.420087	28.010420
274.889240	9905.317132	28.015437
275.057031	9916.351084	28.020455
275.496159	9933.256420	28.025472
275.395875	9945.377191	28.030490
276.281215	9964.347422	28.035508
276.635362	9983.062541	28.040525
276.869060	9994.288346	28.045543
277.109055	9995.488717	28.050560
277.164373	10021.168064	28.055578
277.483992	10021.651959	28.060596
278.093898	10031.834135	28.065613
278.102830	10047.164747	28.070631
278.751123	10052.677599	28.075648
278.930999	10063.510846	28.080666
278.938505	10070.995757	28.085684
279.471403	10088.009772	28.090701
279.420211	10099.927246	28.095719
279.392073	10109.810977	28.100736
279.445352	10123.524509	28.105754
280.010073	10141.506076	28.110772
280.236317	10150.106234	28.115789
280.376332	10170.490379	28.120807
280.757094	10181.560794	28.125824
280.627392	10201.377596	28.130842
281.531692	10211.147786	28.135860
281.653598	10224.105574	28.140877
282.172717	10236.815247	28.145895
282.345309	10246.819352	28.150912
282.506284	10267.648684	28.155930
282.522239	10280.487241	28.160948
282.966596	10299.163374	28.165965
283.383899	10318.677282	28.170983
283.937102	10326.771959	28.176000
284.109359	10344.508560	28.181018
284.078689	10359.027834	28.186036
284.657693	10366.442834	28.191053
284.808414	10383.822885	28.196071
285.472192	10390.716358	28.201088
285.529414	10414.946716	28.206106
286.050567	10426.390093	28.211124
286.043730	10430.255864	28.216141
286.424843	10445.781450	28.221159
286.878290	10458.065780	28.226176
286.659076	10475.039373	28.231194
287.201934	10484.799675	28.236212
287.391438	10493.509906	28.241229
287.744384	10515.951473	28.246247
288.126055	10534.220826	28.251264
288.142566	10555.789701	28.256282
288.441861	10561.871698	28.261300
288.996453	10585.402835	28.266317
289.061020	10606.285443	28.271335
289.812429	10614.033647	28.276352
289.918977	10636.538980	28.281370
290.403268	10637.003570	28.286388
290.189350	10659.208349	28.291405
290.534852	10677.508732	28.296423
291.139299	10698.907304	28.301440
291.011908	10711.948447	28.306458
291.661024	10721.894407	28.311476
292.166317	10742.411754	28.316493
292.133062	10752.470281	28.321511
292.751509	10766.418356	28.326528
292.922933	10784.982754	28.331546
292.909634	10797.279983	28.336564
293.756250	10808.707658	28.341581
293.699383	10836.249542	28.346599
293.965675	10841.812632	28.351616
294.111103	10856.740606	28.356634
294.340818	10866.991905	28.361652
294.744456	10883.717342	28.366669
295.279434	10903.292479	28.371687
295.495799	10913.927935	28.376704
295.759164	10930.700512	28.381722
296.276346	10938.160099	28.386740
296.776354	10951.940462	28.391757
296.835172	10961.861625	28.396775
297.609372	10969.022298	28.401792
297.765302	10989.698505	28.406810
297.853301	10984.051934	28.411828
298.403572	10991.032769	28.416845
298.333887	11003.553621	28.421863
298.464649	11006.741333	28.426880
299.452106	11024.323248	28.431898
299.288766	11020.029309	28.436916
299.653515	11042.232862	28.441933
299.721562	11056.806775	28.446951
299.792890	11069.738292	28.451968
300.375004	11091.143950	28.456986
300.671631	11092.329262	28.462004
300.612894	11110.127813	28.467021
300.862723	11133.871280	28.472039
301.036748	11130.986716	28.477056
300.988912	11148.808867	28.482074
301.332381	11165.221858	28.487092
301.897423	11194.034648	28.492109
302.420322	11211.704853	28.497127
302.904157	11228.980152	28.502144
302.773388	11254.327052	28.507162
303.210763	11263.741071	28.512180
303.682972	11279.237383	28.517197
303.619576	11309.133338	28.522215
304.218365	11332.731161	28.527232
304.424991	11345.534449	28.532250
304.338973	11358.193854	28.537268
305.028525	11375.301487	28.542285
305.138849	11400.115315	28.547303
305.733759	11412.864514	28.552320
306.151893	11433.386719	28.557338
306.276421	11449.265686	28.562356
307.157720	11458.850666	28.567373
307.058271	11470.126070	28.572391
307.530441	11484.005888	28.577408
307.867376	11511.159070	28.582426
308.409408	11522.479884	28.587444
309.098956	11521.437961	28.592461
308.936924	11542.113760	28.597479
309.146934	11552.437970	28.602496
309.618336	11565.939059	28.607514
309.926362	11584.584028	28.612532
310.407803	11598.339342	28.617549
310.616544	11620.621548	28.622567
310.672697	11617.692110	28.627584
311.351211	11630.816826	28.632602
311.448677	11646.475985	28.637620
311.717081	11649.576069	28.642637
311.977282	11669.298990	28.647655
312.416839	11681.238955	28.652672
312.578752	11701.103516	28.657690
312.842764	11709.780612	28.662708
313.320208	11721.061081	28.667725
313.620478	11739.180091	28.672743
314.040211	11748.407646	28.677760
313.916870	11767.659905	28.682778
314.374256	11784.393569	28.687796
314.551262	11790.551844	28.692813
315.292569	11808.008627	28.697831
316.183503	11821.517212	28.702848
316.417056	11838.481545	28.707866
316.468220	11846.604524	28.712884
317.007113	11842.213700	28.717901
317.070752	11864.117768	28.722919
317.354679	11860.155022	28.727936
317.341645	11879.194449	28.732954
317.583948	11895.781713	28.737972
318.229545	11921.507552	28.742989
318.037473	11932.488205	28.748007
318.399320	11946.019256	28.753024
318.533564	11964.524303	28.758042
318.700390	11999.181974	28.763060
319.170500	12013.390902	28.768077
319.222681	12036.386344	28.773095
319.403588	12052.083373	28.778112
320.101817	12078.268566	28.783130
319.958052	12102.409250	28.788148
320.838606	12111.899954	28.793165
321.345611	12140.066442	28.798183
321.604453	12152.688481	28.803200
321.684604	12176.668093	28.808218
321.686230	12194.849826	28.813236
322.416073	12200.407466	28.818253
322.891939	12213.608349	28.823271
324.015203	12211.706290	28.828288
324.413277	12210.798126	28.833306
324.440103	12218.170369	28.838324
324.789084	12226.856581	28.843341
324.675808	12245.223609	28.848359
324.953483	12260.207898	28.853376
325.721650	12260.618868	28.858394
325.967008	12271.332683	28.863412
326.521861	12294.136506	28.868429
326.036046	12305.163107	28.873447
326.424316	12314.885284	28.878464
326.824079	12329.869568	28.883482
327.048703	12348.029363	28.888500
327.459914	12366.229597	28.893517
327.651012	12394.944568	28.898535
327.898577	12410.451529	28.903552
328.317865	12425.556001	28.908570
328.194196	12438.168313	28.913588
328.765322	12456.046912	28.918605
328.964077	12487.214384	28.923623
329.326477	12511.024170	28.928640
330.120995	12532.385779	28.933658
330.067517	12563.617908	28.938676
330.731499	12569.138546	28.943693
331.075283	12596.589060	28.948711
331.400050	12613.280957	28.953728
331.710578	12626.994165	28.958746
331.760388	12650.246505	28.963764
332.590777	12659.808455	28.968781
332.681995	12681.352355	28.973799
332.758119	12695.206312	28.978816
333.545698	12720.630102	28.983834
333.748012	12745.333494	28.988852
334.235660	12756.426691	28.993869
334.846764	12772.069978	28.998887
335.013099	12793.188642	29.003904
335.792975	12794.661977	29.008922
335.890618	12815.772414	29.013940
336.067442	12824.687803	29.018957
336.463528	12837.652082	29.023975
336.455118	12857.288600	29.028992
337.009490	12870.844028	29.034010
337.268156	12897.559835	29.039028
337.617986	12903.312634	29.044045
338.303629	12923.346416	29.049063
338.436826	12946.971391	29.054080
338.816394	12951.677499	29.059098
339.510563	12959.375599	29.064116
339.763963	12972.447445	29.069133
339.726889	12981.140427	29.074151
339.682577	13008.162501	29.079168
340.325877	13019.373723	29.084186
340.855987	13041.456006	29.089204
341.066913	13050.448297	29.094221
341.463570	13070.426176	29.099239
341.499834	13084.820298	29.104256
342.079786	13103.105499	29.109274
342.220066	13126.694861	29.114292
342.612452	13137.241019	29.119309
342.812138	13160.799070	29.124327
342.986507	13184.484247	29.129344
343.939665	13191.516870	29.134362
343.877761	13213.271528	29.139380
344.346706	13239.137199	29.144397
344.743710	13237.888108	29.149415
344.585954	13260.870360	29.154432
345.250123	13272.324797	29.159450
345.343393	13301.549005	29.164468
345.457026	13319.155443	29.169485
346.127281	13329.358451	29.174503
346.424057	13342.802746	29.179520
347.048994	13358.895944	29.184538
347.740195	13386.931414	29.189556
348.131409	13402.625249	29.194573
348.051543	13412.790348	29.199591
348.210359	13439.339310	29.204608
349.257828	13451.921550	29.209626
349.249668	13467.418668	29.214644
349.758418	13483.261641	29.219661
350.065191	13491.061325	29.224679
349.940854	13523.177651	29.229696
350.394876	13535.688126	29.234714
350.699372	13560.029307	29.239732
351.020475	13571.704706	29.244749
351.174806	13593.318768	29.249767
351.640959	13626.947561	29.254784
352.078135	13643.622870	29.259802
351.998309	13666.757694	29.264820
352.506536	13690.937851	29.269837
352.954599	13717.091642	29.274855
353.356331	13738.954726	29.279872
353.975222	13756.056587	29.284890
354.446102	13783.027982	29.289908
354.775587	13803.850792	29.294925
355.226124	13820.571547	29.299943
355.718674	13848.727051	29.304960
356.204173	13861.665483	29.309978
356.642115	13888.815844	29.314996
356.933561	13903.748768	29.320013
357.397196	13915.689566	29.325031
357.097273	13939.392684	29.330048
357.589051	13947.697452	29.335066
357.944814	13972.694357	29.340084
358.295439	13990.204521	29.345101
358.745742	14016.399430	29.350119
358.598961	14037.530335	29.355136
359.457212	14050.249808	29.360154
359.889015	14074.496039	29.365172
360.144294	14093.710670	29.370189
360.602432	14112.593728	29.375207
361.108835	14141.110681	29.380224
361.451001	14149.650417	29.385242
361.459400	14170.984688	29.390260
361.885593	14192.977125	29.395277
362.665146	14217.147294	29.400295
362.781979	14240.577476	29.405312
363.047484	14256.897932	29.410330
363.489881	14282.020711	29.415348
363.686444	14288.754678	29.420365
364.130752	14317.549996	29.425383
364.380100	14340.075421	29.430400
365.218636	14356.960466	29.435418
365.289804	14371.978582	29.440436
365.852276	14402.255704	29.445453
366.360332	14407.589575	29.450471
366.767520	14428.015692	29.455488
367.093835	14448.372313	29.460506
367.452625	14451.727227	29.465524
367.779734	14482.056908	29.470541
368.483427	14483.122224	29.475559
367.684400	14490.854462	29.480576
368.392941	14512.616988	29.485594
368.912365	14532.043585	29.490612
369.328421	14542.236298	29.495629
369.322648	14559.808790	29.500647
369.558093	14579.548083	29.505664
370.245382	14602.517248	29.510682
370.578100	14629.558728	29.515700
370.539976	14651.687145	29.520717
371.107807	14671.062135	29.525735
371.475826	14697.712929	29.530752
371.898735	14709.837422	29.535770
372.758859	14730.704963	29.540788
373.114641	14748.871911	29.545805
373.576732	14762.266212	29.550823
373.805563	14774.695717	29.555840
374.366727	14801.003934	29.560858
374.965069	14815.889799	29.565876
374.896114	14834.391392	29.570893
375.380238	14837.550008	29.575911
375.397296	14871.964661	29.580928
376.210657	14888.137205	29.585946
376.867920	14910.201876	29.590964
376.983141	14921.461706	29.595981
377.216820	14937.901395	29.600999
377.260491	14964.685170	29.606016
378.000617	14981.358707	29.611034
378.133553	15010.061434	29.616052
378.463134	15031.419304	29.621069
379.155710	15059.933919	29.626087
379.366293	15086.824523	29.631104
379.742439	15101.107255	29.636122
379.999343	15126.973775	29.641140
380.221469	15150.259200	29.646157
380.712511	15172.144772	29.651175
381.476836	15197.174428	29.656192
382.105522	15212.854901	29.661210
381.858659	15226.903110	29.666228
382.493090	15258.923187	29.671245
382.840751	15276.886621	29.676263
383.083671	15303.545106	29.681280
383.590396	15326.404297	29.686298
383.963041	15346.849412	29.691316
384.117857	15383.176362	29.696333
384.581304	15395.411836	29.701351
385.085638	15413.856322	29.706368
385.335475	15439.316955	29.711386
386.069097	15462.425226	29.716404
386.504809	15496.747404	29.721421
386.988300	15506.153212	29.726439
387.198743	15535.697385	29.731456
387.485835	15551.942952	29.736474
388.018044	15575.234312	29.741492
388.022182	15597.388827	29.746509
388.408515	15633.718109	29.751527
389.070630	15657.725218	29.756544
389.254180	15678.335933	29.761562
389.874652	15694.441288	29.766580
390.199936	15725.291188	29.771597
390.712104	15738.586792	29.776615
391.116890	15766.493507	29.781632
391.407086	15786.604519	29.786650
392.177251	15792.763346	29.791668
392.220842	15819.286194	29.796685
392.774929	15841.020596	29.801703
392.943350	15858.503998	29.806720
393.338951	15873.962323	29.811738
394.307474	15893.588851	29.816756
394.655620	15912.339223	29.821773
394.849860	15915.435769	29.826791
395.452501	15929.134317	29.831808
395.555638	15937.611006	29.836826
396.267327	15955.429974	29.841844
396.429850	15965.233392	29.846861
396.938894	15984.811531	29.851879
397.327232	16004.108441	29.856896
396.822189	16021.763162	29.861914
397.655301	16030.947411	29.866932
397.861966	16052.016044	29.871949
398.461630	16074.255265	29.876967
398.452036	16103.537688	29.881984
399.192031	16122.783130	29.887002
399.530922	16149.143603	29.892020
400.128681	16187.193899	29.897037
400.300793	16201.373412	29.902055
400.975000	16225.044568	29.907072
400.934649	16249.474459	29.912090
401.601085	16260.646106	29.917108
401.656470	16291.418919	29.922125
402.319073	16309.833316	29.927143
402.641503	16334.873252	29.932160
403.005247	16353.716380	29.937178
403.322815	16384.631711	29.942196
403.638034	16425.382662	29.947213
404.523341	16435.996045	29.952231
404.700696	16466.674350	29.957248
405.065590	16498.425786	29.962266
405.671068	16517.218808	29.967284
406.193343	16544.426152	29.972301
406.692074	16556.423157	29.977319
407.173759	16581.962919	29.982336
407.562104	16604.500961	29.987354
408.278669	16620.579506	29.992372
408.561384	16642.432870	29.997389
408.874425	16666.151323	30.002407
409.419612	16695.079813	30.007424
409.669152	16713.492578	30.012442
409.791101	16724.610292	30.017460
409.938626	16759.510216	30.022477
410.478321	16772.881217	30.027495
411.104438	16798.604081	30.032512
411.549918	16832.134362	30.037530
411.950951	16845.157462	30.042548
412.008390	16875.254981	30.047565
412.560057	16901.520194	30.052583
412.561019	16935.596786	30.057600
413.029203	16962.263570	30.062618
413.969652	16995.420183	30.067636
414.247705	17023.831705	30.072653
414.642001	17049.057211	30.077671
415.078450	17075.188991	30.082688
415.828892	17110.494730	30.087706
416.411850	17106.313792	30.092724
416.714101	17144.358297	30.097741
417.432752	17154.836944	30.102759
417.974197	17175.456720	30.107776
418.104907	17198.825196	30.112794
418.661281	17207.361384	30.117812
418.815707	17230.827278	30.122829
419.108397	17248.393672	30.127847
419.341649	17275.858669	30.132864
419.795595	17309.625354	30.137882
420.466928	17325.266181	30.142900
420.695061	17350.982255	30.147917
421.059556	17369.892593	30.152935
421.502137	17393.424374	30.157952
421.366481	17422.403099	30.162970
422.026117	17439.182917	30.167988
422.557083	17469.011814	30.173005
422.677485	17489.021544	30.178023
423.244347	17507.868927	30.183040
423.471745	17534.419221	30.188058
424.239200	17562.745872	30.193076
424.592093	17597.808015	30.198093
425.150311	17615.327089	30.203111
425.766322	17631.384235	30.208128
425.969852	17658.573290	30.213146
426.404336	17676.054828	30.218164
426.661008	17701.233125	30.223181
426.921510	17720.466380	30.228199
427.858401	17745.033462	30.233216
428.110594	17780.459060	30.238234
428.823150	17801.713017	30.243252
429.350996	17813.197741	30.248269
429.836463	17836.003223	30.253287
430.452335	17857.506031	30.258304
430.574928	17888.776311	30.263322
431.147700	17900.348852	30.268340
431.430368	17927.077440	30.273357
432.010823	17942.129619	30.278375
432.589093	17951.919866	30.283392
433.304288	17980.564814	30.288410
433.981874	17997.926674	30.293428
434.189682	18011.868224	30.298445
434.719073	18023.289660	30.303463
435.013050	18036.832459	30.308480
435.188542	18067.658900	30.313498
435.709311	18076.845384	30.318516
435.903030	18095.843036	30.323533
436.065645	18113.455738	30.328551
436.738456	18136.320852	30.333568
437.273847	18173.655137	30.338586
437.492669	18186.988634	30.343604
437.575117	18219.118539	30.348621
438.171690	18231.951045	30.353639
438.882897	18266.472183	30.358656
439.296003	18300.433322	30.363674
439.417610	18319.341342	30.368692
439.630769	18359.208882	30.373709
440.119953	18381.913352	30.378727
440.704852	18413.611583	30.383744
440.889465	18449.118418	30.388762
441.730299	18472.368405	30.393780
442.533977	18504.411772	30.398797
442.478766	18533.070080	30.403815
442.606593	18553.461961	30.408832
443.387718	18589.507934	30.413850
443.727373	18612.362302	30.418868
444.296151	18635.857000	30.423885
444.524431	18679.538609	30.428903
445.225755	18704.326795	30.433920
445.722105	18732.855308	30.438938
446.468645	18764.863778	30.443956
446.866249	18792.175833	30.448973
447.296528	18813.455898	30.453991
448.019233	18835.758128	30.459008
448.750025	18860.308177	30.464026
448.895190	18880.508176	30.469044
449.382676	18896.377905	30.474061
449.646421	18928.247010	30.479079
449.959308	18947.700763	30.484096
450.074208	18970.830612	30.489114
450.723573	18996.574902	30.494132
451.014772	19028.572566	30.499149
451.655406	19041.594598	30.504167
451.986803	19066.649320	30.509184
452.340493	19092.730378	30.514202
452.767681	19124.713348	30.519220
453.374283	19137.071071	30.524237
453.159748	19171.940106	30.529255
454.058001	19193.956396	30.534272
453.981770	19231.672230	30.539290
454.584316	19270.350155	30.544308
455.040166	19304.337986	30.549325
455.447262	19329.406532	30.554343
456.282060	19352.867002	30.559360
456.591595	19392.538445	30.564378
457.156507	19419.559991	30.569396
457.864600	19452.959168	30.574413
458.154792	19471.361913	30.579431
458.751233	19499.149428	30.584448
459.283235	19527.117594	30.589466
459.653924	19551.566635	30.594484
460.449427	19585.552621	30.599501
460.894199	19613.458678	30.604519
461.645183	19629.205854	30.609536
461.881859	19660.852931	30.614554
462.277183	19680.585204	30.619572
462.645379	19697.181756	30.624589
462.903064	19737.354764	30.629607
463.556396	19762.751970	30.634624
463.920728	19795.434473	30.639642
464.466428	19817.879111	30.644660
464.941376	19839.203888	30.649677
465.301857	19875.096608	30.654695
465.833757	19905.447179	30.659712
466.206735	19930.483903	30.664730
466.640328	19957.002252	30.669748
467.186431	19989.151349	30.674765
467.697394	20019.410587	30.679783
468.377955	20044.993461	30.684800
468.545681	20079.210718	30.689818
469.094111	20110.999530	30.694836
469.493844	20132.652236	30.699853
469.849538	20169.784566	30.704871
470.471775	20201.953750	30.709888
470.603188	20240.056193	30.714906
471.248041	20273.896247	30.719924
471.899180	20299.882071	30.724941
472.497639	20334.860381	30.729959
473.351079	20360.808474	30.734976
473.445173	20394.740798	30.739994
473.783748	20416.226434	30.745012
474.435866	20446.053684	30.750029
474.919207	20483.198327	30.755047
475.220033	20501.802568	30.760064
475.653359	20541.532890	30.765082
475.891405	20575.190392	30.770100
477.042043	20595.949584	30.775117
477.069277	20634.890368	30.780135
477.451522	20660.071902	30.785152
477.789057	20699.286733	30.790170
478.448437	20735.393543	30.795188
479.249202	20756.662282	30.800205
481.130699	20754.764626	30.805223
481.779188	20761.702188	30.810240
482.513787	20790.038670	30.815258
482.568039	20797.435210	30.820276
482.964928	20802.775544	30.825293
483.258051	20818.607601	30.830311
483.740824	20833.159141	30.835328
484.069838	20831.610577	30.840346
484.065860	20855.449849	30.845364
484.884579	20867.200695	30.850381
484.835547	20899.545031	30.855399
485.222475	20904.040302	30.860416
485.566356	20936.588896	30.865434
486.012376	20952.694215	30.870452
486.538805	20977.828439	30.875469
486.445211	21009.769207	30.880487
486.655089	21030.612136	30.885504
487.485642	21062.838763	30.890522
487.956207	21092.189801	30.895540
488.457571	21123.557942	30.900557
488.967975	21155.910382	30.905575
489.611410	21183.718252	30.910592
489.705693	21230.143300	30.915610
490.056107	21249.644053	30.920628
490.794307	21284.122111	30.925645
490.975084	21327.621167	30.930663
491.642481	21364.707235	30.935680
492.281572	21393.084732	30.940698
492.821235	21435.479304	30.945716
493.305229	21461.132543	30.950733
493.921178	21505.177130	30.955751
494.144785	21536.917729	30.960768
494.976874	21564.425077	30.965786
495.071347	21609.618895	30.970804
495.862914	21643.855495	30.975821
496.208016	21681.927468	30.980839
496.736653	21711.700047	30.985856
497.583706	21748.714642	30.990874
497.842186	21786.541244	30.995892
498.688166	21806.862629	31.000909
499.124334	21841.237041	31.005927
499.969022	21886.428435	31.010944
500.299438	21912.763299	31.015962
500.781028	21936.623065	31.020980
501.668568	21968.311549	31.025997
501.832528	21996.846026	31.031015
502.471620	22026.361780	31.036032
502.918063	22064.835743	31.041050
503.290212	22088.895970	31.046068
503.754938	22129.578724	31.051085
503.994156	22161.823388	31.056103
504.332304	22185.560458	31.061120
505.011765	22221.319350	31.066138
505.642630	22251.247433	31.071156
506.392868	22279.552038	31.076173
506.979376	22312.734914	31.081191
507.904176	22352.215461	31.086208
508.013193	22381.403553	31.091226
508.250622	22400.746111	31.096244
509.064874	22433.849505	31.101261
509.912254	22459.826597	31.106279
511.441028	22465.237609	31.111296
511.721632	22483.063353	31.116314
512.060508	22507.299876	31.121332
512.685130	22509.060414	31.126349
512.777127	22532.665616	31.131367
513.285989	22550.885561	31.136384
513.751905	22578.741996	31.141402
513.873480	22604.029787	31.146420
514.853510	22618.372546	31.151437
515.200251	22639.315927	31.156455
515.411786	22675.331732	31.161472
516.202315	22688.895239	31.166490
516.044719	22710.865029	31.171508
516.768926	22738.618291	31.176525
517.111777	22770.348629	31.181543
517.373554	22799.924280	31.186560
517.590205	22825.286016	31.191578
518.315969	22869.430292	31.196596
519.083449	22887.559736	31.201613
519.169985	22921.238514	31.206631
519.940855	22945.661078	31.211648
520.568105	22984.418308	31.216666
520.531693	23020.429107	31.221684
521.209735	23052.290963	31.226701
521.627291	23099.358837	31.231719
522.094602	23124.681934	31.236736
522.698987	23165.054406	31.241754
523.246273	23208.020303	31.246772
523.657477	23248.094431	31.251789
524.143751	23287.771495	31.256807
524.608696	23327.906927	31.261824
525.225743	23363.108890	31.266842
525.925261	23398.967894	31.271860
526.248007	23433.451196	31.276877
526.955638	23467.659794	31.281895
527.372548	23504.479244	31.286912
528.124101	23552.178653	31.291930
528.642305	23587.788185	31.296948
529.591028	23618.199657	31.301965
530.057016	23651.991216	31.306983
530.532635	23692.233146	31.312000
531.384391	23719.076931	31.317018
531.787912	23755.273338	31.322036
532.306181	23785.417164	31.327053
532.783228	23824.313162	31.332071
533.331152	23857.921698	31.337088
534.027409	23894.793171	31.342106
534.295652	23925.412155	31.347124
535.041986	23948.045126	31.352141
535.383577	23980.005083	31.357159
536.239646	24024.403369	31.362176
536.770020	24048.359194	31.367194
537.375278	24084.297301	31.372212
537.873339	24122.110020	31.377229
538.289406	24146.526106	31.382247
538.806379	24185.296528	31.387264
539.566938	24212.294201	31.392282
540.066995	24244.198316	31.397300
540.100234	24272.231913	31.402317
540.615244	24310.870180	31.407335
541.245002	24355.892131	31.412352
542.102791	24384.050295	31.417370
542.710421	24425.132585	31.422388
542.922172	24458.213088	31.427405
543.814359	24485.291750	31.432423
544.269667	24534.303503	31.437440
544.913995	24559.209069	31.442458
544.974799	24596.174445	31.447476
545.453498	24630.332209	31.452493
546.090253	24671.890747	31.457511
546.409978	24715.059626	31.462528
547.588159	24747.364533	31.467546
547.921935	24792.433546	31.472564
548.433274	24834.169933	31.477581
549.263582	24864.007714	31.482599
549.674306	24894.448016	31.487616
550.492404	24928.578732	31.492634
551.537845	24954.743124	31.497652
552.601239	24968.366830	31.502669
552.658469	24985.490207	31.507687
553.600611	25025.447337	31.512704
553.807966	25036.708139	31.517722
554.343531	25052.095070	31.522740
554.872645	25075.243424	31.527757
555.219457	25093.623641	31.532775
555.040730	25126.298389	31.537792
555.720914	25145.985463	31.542810
556.285432	25181.893970	31.547828
556.895047	25213.744661	31.552845
557.249892	25240.920640	31.557863
557.459955	25284.695542	31.562880
558.231422	25304.596068	31.567898
558.542976	25349.366451	31.572916
559.063592	25381.180706	31.577933
559.434283	25424.880351	31.582951
560.028536	25463.691778	31.587968
560.980476	25500.197790	31.592986
561.273872	25538.228319	31.598004
561.574173	25584.302834	31.603021
561.771291	25629.338125	31.608039
562.301395	25687.618413	31.613056
563.375710	25726.658963	31.618074
563.738817	25782.759930	31.623092
564.465652	25815.269543	31.628109
565.011167	25855.169997	31.633127
565.865078	25907.586303	31.638144
566.705834	25939.180969	31.643162
567.668562	25980.748354	31.648180
568.238223	26013.301716	31.653197
569.054271	26054.051547	31.658215
569.233249	26087.601188	31.663232
569.918398	26124.674418	31.668250
570.746955	26155.418139	31.673268
571.154107	26186.455027	31.678285
572.012761	26215.513062	31.683303
572.819243	26244.143187	31.688320
573.624403	26267.066666	31.693338
573.944641	26300.095396	31.698356
574.186045	26327.511701	31.703373
574.716141	26353.309434	31.708391
574.953649	26396.665365	31.713408
575.776866	26428.705929	31.718426
576.215664	26479.184915	31.723444
576.260832	26511.447853	31.728461
577.285706	26543.463527	31.733479
577.350745	26593.413222	31.738496
577.972108	26631.476918	31.743514
578.588593	26672.872113	31.748532
579.316327	26729.841679	31.753549
579.943909	26767.266337	31.758567
580.275701	26818.780361	31.763584
580.931207	26854.791452	31.768602
581.418275	26901.111666	31.773620
582.160245	26949.989881	31.778637
582.756136	26984.386208	31.783655
583.577325	27030.837989	31.788672
584.452990	27067.346079	31.793690
584.883324	27114.010582	31.798708
585.072742	27145.999268	31.803725
586.286488	27188.231609	31.808743
586.346719	27230.447684	31.813760
587.174935	27272.948787	31.818778
587.387332	27315.343598	31.823796
588.380837	27352.358439	31.828813
588.903370	27390.577996	31.833831
589.210509	27429.501107	31.838848
589.721591	27460.410006	31.843866
590.601477	27501.392994	31.848884
591.170781	27550.015123	31.853901
592.301217	27596.723437	31.858919
592.188706	27633.411663	31.863936
592.631713	27653.479416	31.868954
593.424688	27701.586741	31.873972
593.793470	27739.173571	31.878989
594.459225	27780.285263	31.884007
595.494125	27820.947706	31.889024
595.893638	27853.871823	31.894042
596.383281	27894.480248	31.899060
596.907411	27933.408466	31.904077
597.813695	27969.666920	31.909095
598.040858	28006.985551	31.914112
598.992098	28049.778833	31.919130
599.313894	28097.353680	31.924148
599.814999	28124.700386	31.929165
600.244469	28167.164309	31.934183
601.067063	28214.174788	31.939200
601.573578	28251.071146	31.944218
602.138091	28291.984735	31.949236
602.336714	28345.033975	31.954253
603.529838	28385.015578	31.959271
603.660182	28434.681526	31.964288
604.836891	28468.933067	31.969306
605.823452	28529.236277	31.974324
606.227051	28563.248054	31.979341
607.090234	28603.072867	31.984359
607.111503	28638.149271	31.989376
607.896557	28677.790453	31.994394
608.659215	28715.937195	31.999412
609.604110	28770.672762	32.004429
610.256765	28794.589916	32.009447
610.609377	28834.368250	32.014464
611.610869	28874.943192	32.019482
612.712311	28910.660963	32.024500
613.146427	28931.249662	32.029517
613.915629	28947.563951	32.034535
614.440961	28986.974374	32.039552
615.040430	29024.496059	32.044570
615.814359	29051.732009	32.049588
616.209142	29085.847161	32.054605
616.807098	29117.832233	32.059623
617.115073	29159.248917	32.064640
617.496888	29193.157680	32.069658
618.463288	29234.977685	32.074676
618.900137	29280.988772	32.079693
619.581606	29309.712221	32.084711
619.740244	29358.541654	32.089728
620.317669	29397.748810	32.094746
620.984835	29431.512412	32.099764
621.816277	29482.228488	32.104781
622.267113	29520.216685	32.109799
622.904004	29560.103877	32.114816
623.539533	29604.434994	32.119834
623.844697	29646.137542	32.124852
624.269549	29697.094432	32.129869
625.023125	29749.466747	32.134887
626.142308	29791.441094	32.139904
626.553443	29833.405651	32.144922
627.304797	29878.022737	32.149940
627.846000	29922.204877	32.154957
628.829083	29960.774744	32.159975
629.290436	30003.054205	32.164992
629.842644	30038.739349	32.170010
630.665638	30081.569498	32.175028
631.451872	30120.119740	32.180045
632.024271	30156.807004	32.185063
632.734611	30205.476711	32.190080
633.088719	30246.420642	32.195098
633.885647	30279.893630	32.200116
634.153876	30324.555290	32.205133
635.054395	30358.985744	32.210151
635.386869	30393.694320	32.215168
635.883082	30430.804811	32.220186
636.325157	30468.164003	32.225204
636.829805	30512.416313	32.230221
637.742005	30559.519372	32.235239
638.200716	30594.910294	32.240256
638.976635	30650.081746	32.245274
639.736146	30693.277044	32.250292
639.972718	30743.823344	32.255309
640.333371	30785.639668	32.260327
640.966865	30827.944595	32.265344
641.900037	30882.232486	32.270362
642.709576	30929.358693	32.275380
643.236201	30980.707482	32.280397
643.844443	31028.522676	32.285415
644.606672	31071.250558	32.290432
645.166129	31128.972908	32.295450
645.891364	31182.465852	32.300468
646.405443	31234.917157	32.305485
647.026597	31274.076832	32.310503
647.904134	31328.014232	32.315520
648.565196	31381.258499	32.320538
649.381875	31428.308874	32.325556
650.281602	31482.047254	32.330573
651.185478	31510.562153	32.335591
651.838897	31549.534002	32.340608
652.072382	31590.853382	32.345626
653.486407	31637.476200	32.350644
654.020756	31678.799492	32.355661
654.405162	31711.966050	32.360679
655.320462	31751.757250	32.365696
655.780328	31808.504504	32.370714
656.548739	31841.112080	32.375732
657.237747	31890.617214	32.380749
658.122315	31925.014835	32.385767
659.143168	31967.679022	32.390784
659.370414	32009.493298	32.395802
660.617179	32034.668261	32.400820
660.834872	32077.369199	32.405837
661.312928	32105.053523	32.410855
662.158613	32141.366717	32.415872
662.910570	32192.784581	32.420890
663.483891	32216.888756	32.425908
664.055820	32259.642394	32.430925
664.376796	32302.017948	32.435943
665.292800	32350.572184	32.440960
665.606058	32389.737644	32.445978
666.291489	32439.604987	32.450996
667.180272	32494.169531	32.456013
667.702631	32531.254430	32.461031
668.290719	32569.372270	32.466048
668.665988	32622.588348	32.471066
669.609711	32662.269398	32.476084
670.262336	32715.391962	32.481101
670.785804	32752.205239	32.486119
671.577423	32807.980574	32.491136
672.283526	32854.710012	32.496154
672.899327	32899.816222	32.501172
673.612823	32950.849984	32.506189
674.286550	32989.024802	32.511207
675.297547	33035.498556	32.516224
675.793334	33070.672983	32.521242
676.661204	33120.418723	32.526260
677.310105	33166.247391	32.531277
678.024395	33200.717886	32.536295
678.831099	33255.113859	32.541312
678.921859	33290.806897	32.546330
679.633917	33325.467608	32.551348
680.280420	33370.538446	32.556365
680.538155	33411.029464	32.561383
681.384258	33449.254155	32.566400
681.768622	33499.126642	32.571418
682.471585	33550.283628	32.576436
683.037282	33612.051756	32.581453
683.648565	33653.189967	32.586471
684.729459	33691.182563	32.591488
685.000326	33749.804281	32.596506
685.858919	33803.611958	32.601524
686.638570	33855.794598	32.606541
687.043414	33899.677677	32.611559
688.523525	33949.728385	32.616576
688.865764	34000.266139	32.621594
689.785133	34042.760705	32.626612
690.371032	34100.190021	32.631629
691.338687	34139.395978	32.636647
692.528137	34190.643176	32.641664
693.000057	34226.689423	32.646682
693.573250	34266.026569	32.651700
694.272820	34316.553715	32.656717
695.130208	34356.776182	32.661735
695.869357	34408.776831	32.666752
696.020880	34453.326420	32.671770
697.139138	34496.284093	32.676788
697.636391	34552.230024	32.681805
698.538085	34603.358640	32.686823
699.066035	34651.738375	32.691840
699.239240	34697.100705	32.696858
700.040051	34747.815446	32.701876
700.954172	34798.556928	32.706893
701.467108	34857.681464	32.711911
702.346792	34907.410638	32.716928
702.745005	34967.628178	32.721946
703.364826	35025.269705	32.726964
703.994239	35090.105041	32.731981
704.947237	35143.971001	32.736999
705.632588	35197.720697	32.742016
706.277477	35255.422176	32.747034
707.277265	35309.862962	32.752052
707.685482	35373.684035	32.757069
708.208781	35424.127466	32.762087
708.953579	35483.375727	32.767104
709.445123	35550.377345	32.772122
710.315575	35607.924539	32.777140
711.078795	35665.298899	32.782157
711.978393	35724.397281	32.787175
713.108263	35771.554095	32.792192
713.275256	35831.297937	32.797210
714.425085	35882.726135	32.802228
715.219886	35943.662426	32.807245
716.086927	36008.514165	32.812263
716.865516	36051.281289	32.817280
717.199789	36105.208077	32.822298
718.231438	36149.010901	32.827316
719.164061	36198.741194	32.832333
720.233210	36252.914366	32.837351
721.061981	36295.067165	32.842368
721.520210	36345.345874	32.847386
722.283398	36386.794565	32.852404
723.301212	36434.305418	32.857421
723.427311	36483.004814	32.862439
724.615661	36528.282589	32.867456
724.741823	36584.791179	32.872474
725.501498	36630.932611	32.877492
726.082329	36679.213898	32.882509
727.078752	36729.662658	32.887527
728.182294	36751.811536	32.892544
728.616710	36798.712154	32.897562
729.461206	36830.506279	32.902580
729.855719	36880.018423	32.907597
730.335246	36922.916058	32.912615
731.367237	36964.678129	32.917632
731.753741	37012.844990	32.922650
732.350209	37066.777658	32.927668
732.913683	37117.863824	32.932685
733.498326	37180.012492	32.937703
734.416246	37228.204609	32.942720
734.613180	37291.590082	32.947738
735.822520	37339.850905	32.952756
736.549081	37393.549155	32.957773
736.732508	37457.145890	32.962791
737.955999	37522.383062	32.967808
738.638444	37587.767891	32.972826
739.166529	37645.329629	32.977844
740.006993	37705.441812	32.982861
740.420519	37768.017200	32.987879
741.662086	37822.028406	32.992896
742.504807	37894.806612	32.997914
743.057376	37950.177442	33.002932
744.340079	38003.879178	33.007949
745.317918	38054.371902	33.012967
746.471406	38089.224643	33.017984
747.405991	38153.971216	33.023002
748.538614	38182.750444	33.028020
749.613239	38219.658178	33.033037
750.393890	38265.015755	33.038055
751.184225	38296.801525	33.043072
751.857794	38344.003451	33.048090
752.017683	38379.858699	33.053108
752.967269	38413.371488	33.058125
753.584147	38461.581628	33.063143
754.463855	38506.823117	33.068160
755.039090	38552.965792	33.073178
755.682905	38608.014256	33.078196
756.275309	38658.435606	33.083213
756.773193	38711.085080	33.088231
757.442249	38752.768020	33.093248
758.289104	38815.279003	33.098266
759.189147	38863.648322	33.103284
760.023438	38918.914556	33.108301
760.420485	38975.716112	33.113319
760.957073	39038.491048	33.118336
761.548732	39100.087690	33.123354
762.312849	39150.085059	33.128372
763.429024	39202.930382	33.133389
764.330220	39267.489464	33.138407
765.157294	39317.717729	33.143424
766.076629	39384.196794	33.148442
766.830937	39439.906837	33.153460
767.730975	39479.360829	33.158477
767.921012	39540.319291	33.163495
768.849500	39595.167860	33.168512
769.384167	39659.475296	33.173530
770.253667	39712.410858	33.178548
771.150909	39773.361069	33.183565
771.678254	39830.233122	33.188583
772.383361	39892.800908	33.193600
773.461326	39950.972529	33.198618
774.109041	40015.295043	33.203636
775.020043	40063.779178	33.208653
775.633580	40127.614066	33.213671
776.289629	40178.288343	33.218688
776.915967	40225.754700	33.223706
777.670519	40293.293041	33.228724
778.876579	40350.383335	33.233741
779.429391	40402.914541	33.238759
780.529838	40445.374708	33.243776
781.220166	40489.947846	33.248794
781.842765	40548.356385	33.253812
782.630925	40590.764262	33.258829
783.210107	40650.640734	33.263847
783.890764	40701.704504	33.268864
784.836625	40764.439701	33.273882
785.537669	40812.281492	33.278900
786.645676	40873.802793	33.283917
786.863704	40936.740326	33.288935
788.190904	40989.354779	33.293952
789.182558	41036.917824	33.298970
789.874398	41083.250118	33.303988
791.256969	41141.004370	33.309005
791.546131	41191.042433	33.314023
792.276113	41240.910799	33.319040
793.125459	41302.619038	33.324058
793.942986	41367.905729	33.329076
794.871915	41413.335365	33.334093
795.348873	41479.301528	33.339111
796.243303	41522.093119	33.344128
796.766056	41594.516155	33.349146
797.539454	41654.131139	33.354164
798.480247	41700.109760	33.359181
799.267659	41763.890751	33.364199
799.549310	41831.336707	33.369216
800.730700	41896.644230	33.374234
801.488743	41958.254688	33.379252
802.657642	42017.246202	33.384269
803.051027	42099.582808	33.389287
804.095508	42154.280628	33.394304
805.117340	42213.953333	33.399322
805.505688	42277.412130	33.404340
806.347321	42343.083784	33.409357
806.882656	42404.774437	33.414375
808.277456	42479.727373	33.419392
808.919292	42537.391904	33.424410
809.624555	42612.376732	33.429428
810.900729	42661.594073	33.434445
811.577138	42734.230967	33.439463
812.260580	42795.381022	33.444480
813.497996	42855.211655	33.449498
814.306709	42910.416101	33.454516
815.255741	42973.770652	33.459533
816.028168	43035.483089	33.464551
816.585747	43092.649869	33.469568
817.275787	43152.655069	33.474586
817.980186	43219.134997	33.479604
818.852144	43276.620165	33.484621
819.387829	43339.831385	33.489639
820.543745	43407.848154	33.494656
821.347021	43467.551955	33.499674
821.896726	43531.058817	33.504692
823.103957	43598.606454	33.509709
823.652388	43659.950698	33.514727
824.807110	43729.980034	33.519744
825.745110	43790.618833	33.524762
826.227368	43860.310500	33.529780
827.287870	43912.404216	33.534797
828.005572	43978.960259	33.539815
828.992369	44039.876778	33.544832
829.970933	44099.675177	33.549850
830.960405	44164.703038	33.554868
831.611444	44207.550391	33.559885
832.250624	44272.835506	33.564903
833.149380	44323.633380	33.569920
834.006929	44378.751660	33.574938
834.624282	44430.630938	33.579956
835.811946	44482.117941	33.584973
836.459992	44522.404598	33.589991
836.865422	44584.450472	33.595008
838.111228	44631.260634	33.600026
838.903504	44685.649764	33.605044
839.691390	44744.537095	33.610061
840.388853	44806.177578	33.615079
841.497322	44866.780130	33.620096
842.110176	44919.553139	33.625114
842.808634	44986.089891	33.630132
843.821561	45036.530045	33.635149
844.396956	45106.729812	33.640167
845.105817	45170.931372	33.645184
846.282455	45232.156862	33.650202
846.790597	45304.265391	33.655220
847.631532	45364.841361	33.660237
848.553885	45440.693870	33.665255
849.445344	45504.526380	33.670272
850.108594	45569.862153	33.675290
850.525480	45642.106163	33.680308
851.570616	45705.036053	33.685325
852.719273	45787.540783	33.690343
853.464821	45866.414327	33.695360
854.302108	45938.638132	33.700378
855.160657	46012.124018	33.705396
856.241449	46092.205004	33.710413
856.903824	46165.348706	33.715431
858.280332	46238.147424	33.720448
858.531824	46304.302210	33.725466
859.442427	46382.734367	33.730484
860.804495	46447.970242	33.735501
861.604547	46520.049891	33.740519
862.315011	46591.479491	33.745536
863.985386	46650.898691	33.750554
865.136716	46718.768132	33.755572
866.026942	46769.775327	33.760589
867.116462	46817.506367	33.765607
868.265683	46880.619459	33.770624
868.880267	46920.238756	33.775642
869.730904	46989.079423	33.780660
870.571663	47041.632169	33.785677
871.633373	47095.245059	33.790695
872.107368	47151.233289	33.795712
873.246019	47212.799059	33.800730
873.977739	47277.003084	33.805748
874.916025	47328.978291	33.810765
876.078376	47380.950370	33.815783
876.854763	47433.533028	33.820800
877.952873	47483.522593	33.825818
878.788995	47551.861139	33.830836
879.453801	47604.853792	33.835853
880.477561	47651.622594	33.840871
881.188488	47715.831102	33.845888
882.077625	47765.733622	33.850906
882.605474	47833.829998	33.855924
883.632270	47887.867740	33.860941
884.391112	47935.254063	33.865959
884.909272	48012.867289	33.870976
885.833669	48068.692782	33.875994
886.806228	48131.223211	33.881012
887.503833	48190.791571	33.886029
888.080633	48258.027534	33.891047
888.752903	48327.924920	33.896064
889.950984	48406.477514	33.901082
890.687608	48467.014799	33.906100
891.409713	48529.553679	33.911117
892.023427	48595.532247	33.916135
892.765593	48667.754281	33.921152
893.478061	48730.693785	33.926170
894.326246	48802.089942	33.931188
895.571726	48872.203446	33.936205
896.398934	48944.362506	33.941223
897.120781	49019.910289	33.946240
898.162378	49080.136012	33.951258
898.968252	49151.628423	33.956276
900.250860	49218.807966	33.961293
901.385513	49293.862183	33.966311
901.797786	49367.845996	33.971328
902.944392	49439.191367	33.976346
903.609217	49514.642107	33.981364
904.478406	49585.335173	33.986381
905.532136	49655.721351	33.991399
905.992778	49741.599572	33.996416
907.356610	49818.574826	34.001434
908.297318	49894.806365	34.006452
909.297292	49973.148442	34.011469
910.210307	50042.962985	34.016487
911.481540	50116.733257	34.021504
912.126876	50177.131109	34.026522
913.298460	50247.159102	34.031540
914.376467	50321.466267	34.036557
915.467481	50395.961459	34.041575
916.061706	50471.457970	34.046592
917.183959	50539.735619	34.051610
917.976168	50612.107844	34.056628
918.787023	50688.836761	34.061645
920.114660	50759.822723	34.066663
921.259308	50831.444794	34.071680
922.217894	50901.254850	34.076698
923.384334	50967.957757	34.081716
924.359272	51025.693408	34.086733
925.203174	51080.608689	34.091751
926.147488	51155.388587	34.096768
927.026391	51223.180983	34.101786
927.304530	51288.194519	34.106804
927.947321	51361.952716	34.111821
929.642518	51420.115055	34.116839
930.659767	51495.479466	34.121856
931.661937	51552.066951	34.126874
932.823966	51619.120429	34.131892
933.823337	51682.187872	34.136909
934.719863	51752.162016	34.141927
935.744593	51821.635532	34.146944
936.854244	51877.998279	34.151962
937.509694	51945.397309	34.156980
937.999805	51999.553603	34.161997
939.265824	52069.958404	34.167015
939.784149	52143.694170	34.172032
940.852761	52215.629756	34.177050
941.868494	52284.701098	34.182068
942.846962	52351.886509	34.187085
943.417250	52416.180681	34.192103
944.246542	52494.905896	34.197120
945.357579	52559.331426	34.202138
946.537926	52627.277159	34.207156
947.170175	52701.642376	34.212173
948.142901	52771.778574	34.217191
948.989004	52846.123618	34.222208
949.937196	52918.542042	34.227226
950.916356	52994.303234	34.232244
951.921964	53075.148059	34.237261
953.263073	53144.133335	34.242279
953.924896	53225.956049	34.247296
954.776297	53278.591031	34.252314
955.561356	53347.979854	34.257332
955.983571	53422.943236	34.262349
956.806337	53490.358654	34.267367
957.748495	53563.330538	34.272384
958.659211	53636.073412	34.277402
959.745881	53712.902266	34.282420
960.337567	53801.926421	34.287437
961.538702	53873.574386	34.292455
962.675787	53957.394916	34.297472
963.416662	54042.644267	34.302490
964.075719	54118.477907	34.307508
965.377817	54199.957560	34.312525
966.421713	54279.534970	34.317543
967.139250	54365.111855	34.322560
968.574615	54440.768739	34.327578
969.737319	54515.949403	34.332596
970.502784	54595.881303	34.337613
971.770056	54664.218088	34.342631
972.863711	54747.415376	34.347648
974.215585	54822.225849	34.352666
975.009487	54902.008810	34.357684
975.809903	54979.076205	34.362701
976.829933	55050.243356	34.367719
977.679472	55128.714797	34.372736
979.089357	55207.820703	34.377754
980.315311	55283.753366	34.382772
980.794337	55366.751076	34.387789
982.006121	55431.966185	34.392807
982.821458	55505.020781	34.397824
983.579436	55592.304481	34.402842
984.608140	55674.122888	34.407860
985.263336	55759.549984	34.412877
986.588200	55841.746874	34.417895
987.353195	55928.340912	34.422912
988.293141	56009.484483	34.427930
989.869162	56096.630042	34.432948
990.821201	56180.240448	34.437965
991.840652	56250.582250	34.442983
992.552843	56343.615869	34.448000
993.607412	56419.762375	34.453018
994.953906	56506.919851	34.458036
995.759166	56586.928210	34.463053
996.866315	56654.586850	34.468071
997.937252	56746.148568	34.473088
999.087158	56821.091715	34.478106
999.852151	56897.487342	34.483124
1000.764582	56982.245902	34.488141
1002.111321	57058.279350	34.493159
1003.028413	57142.328926	34.498176
1003.997452	57223.858158	34.503194
1004.972091	57298.064291	34.508212
1005.947775	57381.358779	34.513229
1007.087554	57458.185180	34.518247
1008.203138	57542.610314	34.523264
1008.984679	57620.777773	34.528282
1009.840784	57704.452746	34.533300
1010.522661	57784.807091	34.538317
1012.041375	57867.101033	34.543335
1013.333463	57944.354642	34.548352
1013.971279	58038.545650	34.553370
1015.248426	58116.928713	34.558388
1015.945397	58199.782083	34.563405
1017.161184	58272.048628	34.568423
1018.330662	58345.025133	34.573440
1019.008839	58431.553129	34.578458
1020.379774	58512.720374	34.583476
1020.970097	58588.977680	34.588493
1022.005264	58661.292495	34.593511
1022.973067	58736.042114	34.598528
1023.917503	58808.137309	34.603546
1024.888690	58876.139837	34.608564
1025.936480	58954.181567	34.613581
1026.953603	59024.835671	34.618599
1027.570438	59105.672909	34.623616
1028.600584	59190.680426	34.628634
1029.915666	59265.991573	34.633652
1030.745711	59354.727175	34.638669
1031.951985	59435.043359	34.643687
1033.121774	59515.745255	34.648704
1034.256694	59600.472063	34.653722
1035.215824	59675.941162	34.658740
1035.774278	59765.340829	34.663757
1037.348593	59842.088190	34.668775
1038.342704	59919.799586	34.673792
1039.159019	59996.551493	34.678810
1040.527628	60070.635196	34.683828
1042.435435	60151.085072	34.688845
1043.326034	60234.389977	34.693863
1044.408624	60303.183027	34.698880
1045.288670	60381.407364	34.703898
1046.424498	60458.022373	34.708916
1047.150517	60541.012139	34.713933
1048.624300	60617.524405	34.718951
1049.625057	60694.952399	34.723968
1050.396201	60772.783507	34.728986
1051.437570	60852.351472	34.734004
1052.201109	60938.963721	34.739021
1053.686130	61012.411842	34.744039
1054.841232	61092.254055	34.749056
1055.390579	61178.077609	34.754074
1056.694254	61263.258662	34.759092
1057.852925	61353.184707	34.764109
1058.877470	61426.958944	34.769127
1060.029766	61510.328735	34.774144
1060.848354	61587.021977	34.779162
1062.215053	61677.271306	34.784180
1063.232517	61763.106325	34.789197
1064.301702	61846.907975	34.794215
1065.094356	61916.643224	34.799232
1066.334544	62011.205258	34.804250
1067.708690	62096.093373	34.809268
1068.386955	62176.798267	34.814285
1069.484916	62262.831391	34.819303
1070.695645	62354.069661	34.824320
1071.443684	62440.904834	34.829338
1072.935227	62521.376647	34.834356
1073.870385	62609.525293	34.839373
1074.744154	62690.271064	34.844391
1076.276443	62777.814610	34.849408
1077.453554	62859.893719	34.854426
1078.473780	62937.794180	34.859444
1079.986576	63020.555888	34.864461
1080.921780	63095.792341	34.869479
1081.703144	63166.336828	34.874496
1082.552350	63247.297138	34.879514
1083.973690	63320.964625	34.884532
1085.454017	63405.587488	34.889549
1086.369687	63479.555723	34.894567
1087.468773	63560.110990	34.899584
1088.231536	63637.832155	34.904602
1089.303644	63719.082160	34.909620
1090.309211	63807.091156	34.914637
1091.739014	63891.020843	34.919655
1093.117785	63957.574948	34.924672
1093.956760	64034.608114	34.929690
1094.708917	64099.645830	34.934708
1095.691187	64169.851686	34.939725
1096.627329	64242.939039	34.944743
1097.770688	64316.716049	34.949760
1098.736609	64393.008862	34.954778
1099.413968	64465.871259	34.959796
1100.578827	64552.978118	34.964813
1101.422074	64624.112184	34.969831
1102.465367	64712.435033	34.974848
1103.344028	64805.152074	34.979866
1104.416579	64899.440976	34.984884
1105.636705	64988.667904	34.989901
1106.856099	65080.661854	34.994919
1107.967112	65169.406269	34.999936
1108.747311	65273.447346	35.004954
1109.776672	65359.204283	35.009972
1110.901335	65454.202550	35.014989
1111.793442	65549.762847	35.020007
1113.513912	65644.460167	35.025024
1114.565958	65741.199187	35.030042
1115.717662	65837.612842	35.035060
1116.855695	65949.350231	35.040077
1118.087292	66043.732618	35.045095
1119.618566	66129.711610	35.050112
1121.042399	66221.298031	35.055130
1122.682722	66298.099435	35.060148
1123.647398	66381.008217	35.065165
1124.886107	66461.684014	35.070183
1126.028993	66542.336996	35.075200
1127.269015	66622.139388	35.080218
1128.746404	66714.605633	35.085236
1129.989284	66787.006831	35.090253
1130.783103	66867.436603	35.095271
1132.174752	66948.773925	35.100288
1132.831264	67039.507714	35.105306
1133.870735	67121.641177	35.110324
1134.706514	67210.163342	35.115341
1135.573788	67302.321483	35.120359
1137.587955	67385.146159	35.125376
1138.590100	67467.197906	35.130394
1139.673604	67561.476025	35.135412
1140.886722	67648.415086	35.140429
1141.771794	67732.974195	35.145447
1142.949007	67822.547024	35.150464
1143.822225	67920.518840	35.155482
1144.937818	68008.278416	35.160500
1146.040682	68100.447084	35.165517
1147.744085	68178.320723	35.170535
1148.865125	68265.548474	35.175552
1149.993337	68360.797656	35.180570
1150.990932	68446.493972	35.185588
1152.667727	68535.548312	35.190605
1153.381643	68633.699609	35.195623
1154.681093	68711.922676	35.200640
1156.095070	68807.844524	35.205658
1156.859278	68892.698536	35.210676
1157.796302	68980.970450	35.215693
1158.866115	69071.906706	35.220711
1160.260041	69164.578426	35.225728
1161.079386	69250.957351	35.230746
1162.699655	69343.195571	35.235764
1163.969569	69424.737000	35.240781
1164.980258	69524.802066	35.245799
1166.401510	69603.749722	35.250816
1167.627151	69693.498825	35.255834
1168.702162	69775.869533	35.260852
1169.823898	69858.518174	35.265869
1170.650404	69946.994218	35.270887
1172.087900	70013.745016	35.275904
1172.895149	70105.935208	35.280922
1173.550096	70187.625420	35.285940
1175.022600	70272.962597	35.290957
1176.036812	70361.372843	35.295975
1177.220365	70448.154985	35.300992
1178.091552	70535.036694	35.306010
1179.264822	70624.784505	35.311028
1180.695086	70709.996715	35.316045
1181.484238	70814.381845	35.321063
1183.031914	70898.677211	35.326080
1183.611663	70999.283624	35.331098
1184.861465	71089.945644	35.336116
1186.375665	71187.507111	35.341133
1186.978158	71299.826044	35.346151
1188.613279	71377.852930	35.351168
1189.759645	71491.873775	35.356186
1191.512598	71587.081892	35.361204
1192.414863	71684.601148	35.366221
1193.611327	71779.731940	35.371239
1195.320498	71880.026620	35.376256
1196.465580	71981.650670	35.381274
1197.738169	72077.644587	35.386292
1198.893544	72166.881200	35.391309
1200.066091	72268.223447	35.396327
1201.286996	72357.995115	35.401344
1202.471697	72460.856050	35.406362
1203.319312	72563.731859	35.411380
1204.313309	72654.616417	35.416397
1205.613157	72768.859550	35.421415
1207.121551	72875.788013	35.426432
1207.968031	72984.846437	35.431450
1209.432406	73083.106639	35.436468
1211.329238	73176.423592	35.441485
1211.805393	73274.572345	35.446503
1213.983418	73380.436018	35.451520
1214.576818	73475.438809	35.456538
1216.085857	73591.970784	35.461556
1217.259118	73682.210335	35.466573
1218.249667	73786.157914	35.471591
1219.875158	73877.961653	35.476608
1221.080014	73981.167338	35.481626
1222.325441	74076.349438	35.486644
1223.936741	74169.942320	35.491661
1225.116616	74276.724902	35.496679
1226.113505	74370.654782	35.501696
1227.178797	74472.275473	35.506714
1228.309367	74571.923101	35.511732
1230.162701	74668.329993	35.516749
1230.798942	74771.931235	35.521767
1232.128282	74871.853036	35.526784
1233.350264	74969.777937	35.531802
1234.457194	75084.529702	35.536820
1235.209643	75178.500463	35.541837
1236.768455	75283.543413	35.546855
1238.196691	75380.563705	35.551872
1239.915496	75491.637276	35.556890
1240.562256	75588.032614	35.561908
1242.244008	75689.827967	35.566925
1243.077827	75795.289768	35.571943
1244.269724	75890.309305	35.576960
1245.731020	75994.432851	35.581978
1247.000003	76104.324927	35.586996
1248.541170	76191.956912	35.592013
1249.383533	76301.890862	35.597031
1250.796668	76400.487907	35.602048
1252.072023	76501.576878	35.607066
1253.160070	76605.292183	35.612084
1254.391616	76686.082935	35.617101
1255.400376	76783.680258	35.622119
1256.540441	76876.722543	35.627136
1257.555350	76971.507408	35.632154
1258.430563	77070.874664	35.637172
1260.198170	77157.828484	35.642189
1261.217784	77253.994368	35.647207
1262.830575	77355.160670	35.652224
1264.070875	77461.148393	35.657242
1265.036265	77563.442324	35.662260
1266.331298	77664.076515	35.667277
1267.154629	77767.077382	35.672295
1268.773072	77880.266565	35.677312
1270.078385	77980.608959	35.682330
1271.290729	78095.293723	35.687348
1272.972342	78200.493546	35.692365
1274.121721	78303.509022	35.697383
1275.484671	78422.846251	35.702400
1276.727969	78519.995225	35.707418
1277.991005	78626.287958	35.712436
1279.884640	78728.657118	35.717453
1281.637313	78831.251294	35.722471
1282.701187	78932.040136	35.727488
1284.161133	79029.562578	35.732506
1285.357432	79130.496224	35.737524
1286.340263	79214.905681	35.742541
1287.799824	79315.406301	35.747559
1289.226360	79417.027267	35.752576
1290.720583	79511.480270	35.757594
1291.992936	79624.705170	35.762612
1293.099847	79718.256341	35.767629
1294.477866	79822.787499	35.772647
1295.885413	79927.213103	35.777664
1297.048740	80021.111244	35.782682
1298.316900	80129.473999	35.787700
1299.641283	80232.520112	35.792717
1301.035289	80340.876772	35.797735
1302.097475	80439.669656	35.802752
1303.497721	80542.464397	35.807770
1304.903443	80646.373554	35.812788
1306.448639	80744.522224	35.817805
1307.648285	80854.102042	35.822823
1308.659656	80947.912939	35.827840
1310.536797	81052.903142	35.832858
1311.521471	81167.015277	35.837876
1313.048853	81254.437511	35.842893
1313.862111	81357.351956	35.847911
1315.544325	81469.418315	35.852928
1317.259427	81573.814888	35.857946
1318.311455	81679.772067	35.862964
1319.673108	81774.380078	35.867981
1321.054549	81871.164524	35.872999
1322.254616	81977.935989	35.878016
1323.345591	82082.634315	35.883034
1324.764321	82187.497404	35.888052
1326.019393	82289.282223	35.893069
1327.481848	82400.524946	35.898087
1328.675701	82501.737241	35.903104
1329.860410	82606.625644	35.908122
1330.843917	82712.090568	35.913140
1332.956448	82810.969048	35.918157
1334.412740	82924.748827	35.923175
1335.116689	83021.021829	35.928192
1337.139749	83128.556464	35.933210
1338.450371	83229.550463	35.938228
1339.597646	83327.250602	35.943245
1340.802711	83430.289008	35.948263
1342.056772	83534.739256	35.953280
1343.649015	83624.591479	35.958298
1344.216753	83727.020610	35.963316
1345.832070	83811.206085	35.968333
1346.883700	83901.928908	35.973351
1348.237981	83996.203389	35.978368
1349.982497	84086.679575	35.983386
1351.265372	84182.245529	35.988404
1352.493704	84282.787253	35.993421
1353.494815	84383.833520	35.998439
1354.805191	84489.849687	36.003456
1356.335716	84590.611546	36.008474
1357.289705	84695.150758	36.013492
1358.824228	84800.005465	36.018509
1360.105857	84908.941998	36.023527
1361.506569	85032.749007	36.028544
1362.825037	85139.045079	36.033562
1364.241850	85250.914255	36.038580
1365.529066	85359.078676	36.043597
1366.922495	85471.281802	36.048615
1368.289468	85604.574687	36.053632
1370.081195	85705.135068	36.058650
1370.948022	85820.183890	36.063668
1372.283533	85928.241555	36.068685
1373.508450	86058.264041	36.073703
1374.875120	86184.945072	36.078720
1376.298354	86303.089793	36.083738
1377.678452	86422.318808	36.088756
1378.975747	86538.481951	36.093773
1380.699862	86674.195170	36.098791
1382.076132	86802.866885	36.103808
1383.391641	86916.228205	36.108826
1384.914437	87039.796699	36.113844
1386.642407	87168.770104	36.118861
1387.929443	87287.497591	36.123879
1389.121519	87411.968168	36.128896
1390.822349	87538.058169	36.133914
1392.261255	87652.214162	36.138932
1394.025011	87775.165334	36.143949
1395.348267	87889.555682	36.148967
1396.363323	88015.247579	36.153984
1398.228408	88131.442729	36.159002
1399.188817	88254.128098	36.164020
1401.089925	88373.651480	36.169037
1402.778184	88484.210894	36.174055
1403.718037	88608.890545	36.179072
1405.451711	88719.912664	36.184090
1407.225538	88842.765348	36.189108
1408.400508	88947.462846	36.194125
1409.917016	89054.312638	36.199143
1410.924717	89169.048542	36.204160
1412.494185	89297.853189	36.209178
1414.154219	89414.275401	36.214196
1415.619390	89530.487611	36.219213
1417.088682	89644.076292	36.224231
1418.132664	89756.920522	36.229248
1419.333065	89875.456466	36.234266
1420.642604	90003.861065	36.239284
1422.053854	90116.104539	36.244301
1423.398548	90240.525254	36.249319
1425.018330	90370.492663	36.254336
1426.657091	90478.887379	36.259354
1428.100951	90600.898868	36.264372
1429.966782	90722.680419	36.269389
1431.249235	90838.254460	36.274407
1433.057429	90947.093424	36.279424
1434.556914	91047.489427	36.284442
1435.796621	91160.371856	36.289460
1437.120643	91265.206374	36.294477
1438.477504	91362.926103	36.299495
1439.423857	91463.777131	36.304512
1440.855706	91562.651837	36.309530
1442.461828	91664.275348	36.314548
1443.721614	91770.680524	36.319565
1445.247814	91877.222047	36.324583
1446.297897	91994.965941	36.329600
1447.954468	92095.226916	36.334618
1449.192871	92214.767435	36.339636
1450.145987	92318.560683	36.344653
1451.326241	92431.735949	36.349671
1453.059712	92559.096870	36.354688
1454.870318	92668.689455	36.359706
1456.417238	92792.518880	36.364724
1457.590449	92909.955644	36.369741
1459.210475	93024.091301	36.374759
1460.833457	93154.729275	36.379776
1462.317953	93270.471276	36.384794
1463.628956	93398.699967	36.389812
1464.749035	93520.025811	36.394829
1466.568733	93648.252419	36.399847
1467.998198	93776.413554	36.404864
1469.630933	93899.321515	36.409882
1471.000727	94030.192756	36.414900
1472.565673	94159.994827	36.419917
1474.168085	94279.905046	36.424935
1475.293420	94411.513088	36.429952
1477.017086	94542.990537	36.434970
1478.577437	94665.291738	36.439988
1479.735772	94804.577516	36.445005
1481.427276	94926.403026	36.450023
1483.098821	95064.494664	36.455040
1484.611311	95196.071136	36.460058
1486.358490	95328.486248	36.465076
1487.937497	95462.284385	36.470093
1489.405746	95584.679605	36.475111
1490.903066	95707.514430	36.480128
1492.213527	95827.754950	36.485146
1493.834555	95962.005021	36.490164
1495.468510	96094.542422	36.495181
1497.029625	96229.398732	36.500199
1498.325794	96353.763163	36.505216
1499.767964	96480.247604	36.510234
1501.807384	96614.093103	36.515252
1502.681284	96738.626194	36.520269
1504.562544	96860.721283	36.525287
1506.135452	97001.422776	36.530304
1507.320500	97133.704860	36.535322
1508.977181	97261.933735	36.540340
1510.652776	97399.730831	36.545357
1512.383065	97532.817070	36.550375
1513.641191	97657.686958	36.555392
1515.367910	97785.476059	36.560410
1516.493547	97909.657678	36.565428
1517.911352	98042.946818	36.570445
1519.903588	98172.496233	36.575463
1521.276278	98306.921726	36.580480
1523.054048	98445.582163	36.585498
1524.616175	98570.256206	36.590516
1525.680897	98692.777026	36.595533
1527.565677	98821.204891	36.600551
1528.754378	98955.065941	36.605568
1530.714262	99088.820198	36.610586
1532.443544	99207.487160	36.615604
1533.253115	99336.502790	36.620621
1535.485514	99465.398900	36.625639
1536.624300	99601.425540	36.630656
1537.991355	99724.106088	36.635674
1539.036398	99839.623827	36.640692
1540.527179	99962.108542	36.645709
1542.415254	100082.947210	36.650727
1543.839984	100196.315359	36.655744
1545.279896	100310.784487	36.660762
1546.735789	100437.675533	36.665780
1548.058678	100554.078047	36.670797
1549.718690	100683.676650	36.675815
1551.009725	100814.296706	36.680832
1552.836334	100940.257261	36.685850
1554.785805	101058.719281	36.690868
1556.153405	101205.125530	36.695885
1557.709384	101322.825698	36.700903
1559.616481	101452.477658	36.705920
1561.127173	101575.954257	36.710938
1562.537144	101697.152274	36.715956
1563.514175	101828.788805	36.720973
1565.669500	101954.448559	36.725991
1567.031027	102097.221128	36.731008
1568.881606	102241.883330	36.736026
1570.148056	102372.399347	36.741044
1571.855063	102516.083517	36.746061
1573.055099	102649.805919	36.751079
1574.634441	102798.164169	36.756096
1575.926597	102937.654783	36.761114
1577.896736	103077.712427	36.766132
1579.224057	103234.365617	36.771149
1581.057844	103376.664511	36.776167
1582.398888	103523.148624	36.781184
1584.121511	103671.577243	36.786202
1586.035691	103821.624963	36.791220
1587.830996	103962.182677	36.796237
1589.529175	104105.748338	36.801255
1590.985298	104255.691804	36.806272
1592.478969	104398.631247	36.811290
1594.235758	104543.102562	36.816308
1595.546919	104685.780020	36.821325
1597.789212	104837.264707	36.826343
1599.423819	104981.490666	36.831360
1600.994312	105123.001164	36.836378
1602.644645	105254.356308	36.841396
1604.165093	105401.657575	36.846413
1606.203169	105552.048800	36.851431
1607.772896	105684.863634	36.856448
1608.834215	105821.600043	36.861466
1610.957513	105961.062680	36.866484
1612.610662	106112.809640	36.871501
1614.268042	106252.675668	36.876519
1615.694781	106392.831767	36.881536
1617.486684	106538.599517	36.886554
1619.102721	106674.631713	36.891572
1620.849265	106816.388175	36.896589
1622.746177	106948.713235	36.901607
1624.232147	107086.009962	36.906624
1625.993880	107214.717909	36.911642
1627.989320	107347.434944	36.916660
1629.055172	107492.571644	36.921677
1630.604602	107624.560316	36.926695
1632.065365	107766.720245	36.931712
1633.454238	107905.316081	36.936730
1635.718674	108029.776999	36.941748
1636.641243	108177.601783	36.946765
1638.792239	108321.317717	36.951783
1639.975158	108472.032445	36.956800
1641.847260	108608.679170	36.961818
1643.594384	108741.934779	36.966836
1645.209673	108888.957348	36.971853
1646.708587	109024.852230	36.976871
1647.821572	109157.383882	36.981888
1649.569804	109282.500291	36.986906
1651.299109	109407.150902	36.991924
1652.375650	109548.414200	36.996941
1654.021607	109687.687289	37.001959
1655.641089	109839.430567	37.006976
1657.150694	109973.501406	37.011994
1659.134341	110104.594985	37.017012
1659.892143	110256.385413	37.022029
1661.815717	110396.924282	37.027047
1663.298908	110558.063361	37.032064
1664.884019	110712.770520	37.037082
1667.167587	110861.764443	37.042100
1668.326301	111024.186255	37.047117
1670.169003	111168.900329	37.052135
1671.939316	111326.117665	37.057152
1673.537554	111483.590750	37.062170
1675.336244	111637.558538	37.067188
1676.747634	111796.406355	37.072205
1678.858768	111953.510013	37.077223
1681.252995	112113.398370	37.082240
1682.764323	112266.411732	37.087258
1684.418346	112412.923030	37.092276
1686.288924	112572.451072	37.097293
1687.674779	112729.518841	37.102311
1689.903774	112879.151135	37.107328
1691.401699	113034.972627	37.112346
1693.277862	113180.019391	37.117364
1695.082877	113338.952291	37.122381
1696.714461	113490.037117	37.127399
1698.274786	113641.856565	37.132416
1699.737064	113804.877878	37.137434
1701.738592	113962.730288	37.142452
1703.337631	114135.053481	37.147469
1704.544626	114281.971697	37.152487
1706.378678	114450.721344	37.157504
1708.069863	114622.892995	37.162522
1709.806972	114782.134489	37.167540
1711.631470	114944.660630	37.172557
1713.327718	115106.801599	37.177575
1715.310676	115271.904536	37.182592
1716.854861	115435.186728	37.187610
1718.529967	115600.047343	37.192628
1720.226178	115777.043219	37.197645
1721.909073	115942.335380	37.202663
1724.002822	116111.496159	37.207680
1725.566224	116280.461221	37.212698
1727.453637	116453.688987	37.217716
1729.226716	116618.513527	37.222733
1730.895970	116777.190761	37.227751
1732.817192	116943.262037	37.232768
1734.374690	117125.473523	37.237786
1736.323417	117274.114663	37.242804
1738.265616	117444.471993	37.247821
1739.954090	117601.513534	37.252839
1741.909209	117775.853076	37.257856
1743.702032	117939.399298	37.262874
1745.273991	118091.146458	37.267892
1746.888279	118260.873591	37.272909
1748.797219	118424.670212	37.277927
1750.360214	118581.925633	37.282944
1751.809474	118756.703595	37.287962
1753.685902	118916.207461	37.292980
1755.235904	119086.595196	37.297997
1756.779037	119262.553200	37.303015
1758.652081	119428.490713	37.308032
1760.148145	119606.372976	37.313050
1761.993155	119771.961179	37.318068
1763.612124	119932.612921	37.323085
1764.889557	120084.743677	37.328103
1766.558839	120243.993581	37.333120
1768.431166	120404.227323	37.338138
1770.283941	120566.950995	37.343156
1772.124570	120729.423546	37.348173
1773.548792	120903.733180	37.353191
1775.493172	121070.922489	37.358208
1777.000434	121232.282020	37.363226
1778.544846	121403.454681	37.368244
1780.228208	121586.530488	37.373261
1781.643034	121768.976635	37.378279
1783.505814	121952.482902	37.383296
1785.502068	122146.789825	37.388314
1787.326826	122330.519433	37.393332
1789.094705	122516.783153	37.398349
1790.550674	122708.931627	37.403367
1793.022233	122890.736475	37.408384
1794.636817	123086.566282	37.413402
1795.977623	123279.699563	37.418420
1798.138968	123474.862654	37.423437
1799.877453	123661.466175	37.428455
1802.320487	123847.948231	37.433472
1804.153693	124046.159059	37.438490
1806.481063	124231.620667	37.443508
1808.569354	124414.418221	37.448525
1810.228133	124597.600609	37.453543
1812.375524	124767.514192	37.458560
1814.366133	124951.293542	37.463578
1816.361678	125123.515779	37.468596
1818.337522	125302.402133	37.473613
1819.959651	125482.283121	37.478631
1822.169606	125651.505628	37.483648
1823.394827	125830.358902	37.488666
1825.132733	126006.938400	37.493684
1826.957268	126199.642526	37.498701
1828.699120	126396.001501	37.503719
1831.073560	126568.145524	37.508736
1832.388201	126752.456895	37.513754
1834.094343	126946.578511	37.518772
1835.884135	127133.456500	37.523789
1837.793962	127324.439912	37.528807
1839.779863	127514.714583	37.533824
1841.394858	127715.273627	37.538842
1843.065667	127900.422790	37.543860
1845.127815	128100.508116	37.548877
1846.953172	128292.384553	37.553895
1848.705774	128491.340021	37.558912
1850.492276	128697.155022	37.563930
1852.503406	128890.730777	37.568948
1854.164357	129081.126619	37.573965
1856.362690	129278.696958	37.578983
1858.548067	129463.836399	37.584000
1860.480805	129661.652872	37.589018
1862.063242	129850.897148	37.594036
1863.837742	130042.142420	37.599053
1865.506151	130238.962332	37.604071
1867.745466	130432.915654	37.609088
1869.822831	130632.871086	37.614106
1871.519456	130819.957640	37.619124
1873.381013	131016.738392	37.624141
1874.765808	131219.240459	37.629159
1876.791136	131402.624221	37.634176
1879.075023	131606.498072	37.639194
1880.714661	131794.257526	37.644212
1882.882202	131980.679490	37.649229
1884.649451	132173.876716	37.654247
1886.570869	132361.214121	37.659264
1888.073122	132537.388246	37.664282
1890.231252	132712.166773	37.669300
1891.876530	132894.017239	37.674317
1893.444806	133068.102299	37.679335
1895.651622	133247.455993	37.684352
1896.712562	133436.556083	37.689370
1898.385189	133619.052424	37.694388
1900.547064	133806.853455	37.699405
1901.896995	134010.021048	37.704423
1903.704517	134208.461498	37.709440
1905.495049	134408.555055	37.714458
1907.508204	134620.821776	37.719476
1909.237482	134820.952097	37.724493
1911.044617	135036.272877	37.729511
1913.236949	135231.625269	37.734528
1914.849763	135452.485435	37.739546
1917.004938	135673.477994	37.744564
1919.275292	135885.533021	37.749581
1921.318457	136108.841935	37.754599
1923.398148	136314.380855	37.759616
1925.454632	136521.497832	37.764634
1927.450910	136736.873421	37.769652
1929.249760	136935.454143	37.774669
1931.091826	137154.662627	37.779687
1933.529671	137361.774819	37.784704
1935.493796	137579.913077	37.789722
1937.139141	137801.261788	37.794740
1939.383167	138008.622783	37.799757
1940.906745	138235.347720	37.804775
1943.139601	138454.780742	37.809792
1944.854588	138673.787787	37.814810
1946.671859	138899.734217	37.819828
1948.895146	139120.745455	37.824845
1950.437570	139353.957658	37.829863
1952.676768	139564.384708	37.834880
1954.677354	139804.951761	37.839898
1956.567257	140024.369357	37.844916
1958.460277	140252.696319	37.849933
1960.334960	140490.545265	37.854951
1961.894774	140723.266565	37.859968
1964.080233	140955.117486	37.864986
1966.092220	141201.184952	37.870004
1968.315135	141434.187229	37.875021
1970.000293	141673.607147	37.880039
1972.209429	141915.269171	37.885056
1973.903859	142160.388352	37.890074
1976.003918	142386.776862	37.895092
1977.984934	142628.566773	37.900109
1979.740549	142872.715474	37.905127
1981.921065	143119.616753	37.910144
1983.970114	143356.259645	37.915162
1985.642746	143605.044588	37.920180
1987.916208	143851.376635	37.925197
1989.879134	144097.656702	37.930215
1992.006751	144334.038203	37.935232
1994.214127	144578.873822	37.940250
1996.285219	144826.524053	37.945268
1998.308231	145056.845857	37.950285
2000.349189	145300.962075	37.955303
2002.140163	145540.435024	37.960320
2004.357050	145778.142080	37.965338
2006.280110	146012.545253	37.970356
2008.486449	146253.746509	37.975373
2010.743994	146494.902856	37.980391
2012.529439	146735.270735	37.985408
2015.012727	146968.423401	37.990426
2016.702773	147210.572583	37.995444
2018.920121	147425.250449	38.000461
2020.443426	147654.697098	38.005479
2022.535117	147865.613963	38.010496
2024.588958	148093.558405	38.015514
2026.158629	148320.170303	38.020532
2028.237736	148542.134502	38.025549
2029.914834	148773.288331	38.030567
2032.079952	148986.521057	38.035584
2033.696879	149217.622727	38.040602
2035.628025	149456.317668	38.045620
2037.627420	149688.516920	38.050637
2039.373555	149932.028053	38.055655
2041.459105	150185.870458	38.060672
2043.259835	150423.460317	38.065690
2045.427142	150670.184088	38.070708
2048.045967	150911.634454	38.075725
2050.193962	151169.457460	38.080743
2052.168703	151399.890838	38.085760
2054.349619	151650.259949	38.090778
2056.327786	151899.836676	38.095796
2058.470243	152146.901020	38.100813
2060.661576	152395.152067	38.105831
2062.742686	152639.346697	38.110848
2064.740271	152887.833199	38.115866
2066.675767	153146.104716	38.120884
2069.184644	153395.999082	38.125901
2071.241846	153648.033966	38.130919
2073.576492	153907.935158	38.135936
2075.391469	154159.971942	38.140954
2077.177656	154421.255638	38.145972
2079.470219	154681.255776	38.150989
2081.614996	154943.641223	38.156007
2084.170757	155194.310553	38.161024
2086.488630	155428.908881	38.166042
2088.362565	155700.619486	38.171060
2090.597045	155936.261094	38.176077
2092.820692	156202.689507	38.181095
2095.136679	156452.500278	38.186112
2097.303066	156708.733480	38.191130
2099.102985	156962.841347	38.196148
2101.506333	157213.441514	38.201165
2103.506230	157469.361166	38.206183
2105.575466	157712.766719	38.211200
2107.317830	157975.888507	38.216218
2109.597810	158233.278531	38.221236
2111.507445	158486.753760	38.226253
2113.671233	158757.633491	38.231271
2115.650769	159014.794308	38.236288
2117.585804	159281.954225	38.241306
2119.657270	159563.109591	38.246324
2121.900706	159815.700511	38.251341
2123.699107	160097.510188	38.256359
2125.484145	160376.707976	38.261376
2127.731186	160639.940427	38.266394
2129.941726	160927.415362	38.271412
2132.034078	161199.903867	38.276429
2134.272310	161484.368193	38.281447
2136.461286	161756.805976	38.286464
2138.888311	162030.553625	38.291482
2140.564210	162320.530279	38.296500
2143.172271	162588.716785	38.301517
2145.077470	162859.095919	38.306535
2147.666626	163127.630396	38.311552
2150.361603	163401.469133	38.316570
2152.020679	163680.802572	38.321588
2154.325725	163950.489209	38.326605
2156.426162	164215.562005	38.331623
2157.869818	164489.054086	38.336640
2160.464806	164753.620398	38.341658
2162.302805	165013.150874	38.346676
2164.233217	165268.490877	38.351693
2166.254229	165524.566837	38.356711
2167.832881	165784.000988	38.361728
2170.035985	166043.224680	38.366746
2172.297755	166320.837511	38.371764
2174.390779	166576.512632	38.376781
2176.758069	166858.796258	38.381799
2178.803159	167119.699173	38.386816
2181.349357	167385.197481	38.391834
2183.345115	167664.926681	38.396852
2185.670650	167934.156181	38.401869
2187.798381	168213.181398	38.406887
2189.815908	168490.561569	38.411904
2191.759316	168765.846658	38.416922
2193.487286	169066.293766	38.421940
2195.744356	169356.895728	38.426957
2197.712616	169642.668107	38.431975
2199.569005	169955.605612	38.436992
2202.155580	170247.213727	38.442010
2204.523967	170563.438921	38.447028
2206.708718	170860.229015	38.452045
2208.951290	171155.081293	38.457063
2211.028450	171475.279196	38.462080
2213.906296	171785.792636	38.467098
2216.272484	172091.587307	38.472116
2218.682208	172396.805044	38.477133
2220.577976	172700.986595	38.482151
2222.703263	173018.542413	38.487168
2225.018682	173316.756654	38.492186
2226.991764	173627.215215	38.497204
2229.605936	173949.955652	38.502221
2231.673380	174268.871544	38.507239
2233.879236	174582.434038	38.512256
2236.036320	174887.269126	38.517274
2238.515835	175217.222754	38.522292
2240.681861	175539.290200	38.527309
2242.695871	175858.995330	38.532327
2245.105618	176188.620920	38.537344
2247.326264	176502.747287	38.542362
2249.628891	176832.341332	38.547380
2251.665391	177159.997155	38.552397
2254.479331	177488.904696	38.557415
2256.459737	177816.470222	38.562432
2258.735451	178136.143373	38.567450
2260.752281	178469.623246	38.572468
2263.298530	178794.285377	38.577485
2265.215939	179124.837176	38.582503
2267.620473	179466.336892	38.587520
2270.485853	179797.023069	38.592538
2272.511428	180126.672888	38.597556
2275.277235	180445.262322	38.602573
2277.666542	180756.520726	38.607591
2279.851534	181084.371407	38.612608
2282.498849	181408.874982	38.617626
2284.725388	181735.019867	38.622644
2287.125684	182064.313629	38.627661
2289.262650	182387.706352	38.632679
2291.531803	182710.495456	38.637696
2293.838894	183037.013323	38.642714
2296.149879	183364.014274	38.647732
2298.234489	183687.267182	38.652749
2300.651504	184002.062484	38.657767
2302.750775	184322.902355	38.662784
2305.033618	184642.851145	38.667802
2307.749890	184962.022347	38.672820
2309.987508	185285.637687	38.677837
2312.327447	185597.503778	38.682855
2314.291599	185910.826264	38.687872
2316.644920	186205.547719	38.692890
2319.038275	186526.628250	38.697908
2321.334267	186873.860881	38.702925
2323.367807	187173.130541	38.707943
2325.519615	187475.024195	38.712960
2327.743083	187779.803108	38.717978
2329.967802	188073.051246	38.722996
2331.936274	188391.511196	38.728013
2334.064660	188707.585007	38.733031
2336.718834	189035.896845	38.738048
2338.636321	189354.418321	38.743066
2341.213769	189681.067606	38.748084
2343.350704	190013.984020	38.753101
2345.602660	190340.482661	38.758119
2347.774926	190684.571606	38.763136
2350.169348	191024.207342	38.768154
2352.350794	191359.990946	38.773172
2354.757047	191708.516956	38.778189
2357.383687	192050.964354	38.783207
2358.945595	192416.362780	38.788224
2361.714253	192767.248506	38.793242
2363.668398	193127.152258	38.798260
2365.996135	193486.389288	38.803277
2368.781168	193855.335528	38.808295
2370.741236	194226.900517	38.813312
2373.200998	194586.094698	38.818330
2375.879617	194955.721073	38.823348
2378.450777	195315.433337	38.828365
2380.853556	195691.912211	38.833383
2383.415048	196063.312565	38.838400
2386.132050	196426.535874	38.843418
2388.434936	196783.271001	38.848436
2391.044671	197166.961116	38.853453
2393.673224	197522.605965	38.858471
2396.162792	197899.356706	38.863488
2398.693141	198256.898362	38.868506
2401.237863	198627.723784	38.873524
2403.134292	198991.868719	38.878541
2405.567706	199352.704914	38.883559
2408.167710	199729.951108	38.888576
2410.812084	200095.531773	38.893594
2412.889508	200470.346268	38.898612
2415.479737	200845.716884	38.903629
2418.078455	201211.535812	38.908647
2420.618152	201590.345291	38.913664
2422.827246	201962.475458	38.918682
2425.485320	202335.679670	38.923700
2428.098137	202703.430204	38.928717
2430.903891	203067.823754	38.933735
2432.938982	203439.069652	38.938752
2435.826912	203800.200367	38.943770
2438.370916	204160.928063	38.948788
2440.907752	204535.629043	38.953805
2443.168259	204896.275242	38.958823
2445.748820	205253.315911	38.963840
2449.081861	205598.605626	38.968858
2452.026845	205945.201065	38.973876
2453.811629	206294.848174	38.978893
2456.465732	206639.661036	38.983911
2458.723368	206996.907414	38.988928
2461.414472	207339.683404	38.993946
2463.867287	207691.794535	38.998964
2465.893140	208048.494418	39.003981
2468.757593	208400.466378	39.008999
2470.285411	208764.154526	39.014016
2472.924416	209117.991670	39.019034
2475.258528	209460.292888	39.024052
2477.253482	209800.284850	39.029069
2479.980481	210123.295531	39.034087
2482.061816	210481.463736	39.039104
2484.343942	210810.260252	39.044122
2486.316483	211157.624444	39.049140
2488.370541	211509.904655	39.054157
2490.900823	211862.720875	39.059175
2493.065949	212231.420741	39.064192
2494.785436	212606.439688	39.069210
2497.596832	212968.028492	39.074228
2500.169534	213351.806807	39.079245
2502.433855	213717.952628	39.084263
2504.682370	214120.962033	39.089280
2506.937071	214509.922696	39.094298
2509.255350	214911.143884	39.099316
2511.702008	215312.751985	39.104333
2514.075496	215724.863650	39.109351
2516.482005	216141.111418	39.114368
2518.964465	216562.199910	39.119386
2521.790886	216967.180041	39.124404
2524.713338	217389.674258	39.129421
2527.510786	217789.146964	39.134439
2530.290595	218214.890380	39.139456
2532.762500	218629.758360	39.144474
2535.508287	219052.713286	39.149492
2537.651132	219466.159641	39.154509
2540.675297	219889.173432	39.159527
2542.960153	220310.473450	39.164544
2545.905451	220736.421480	39.169562
2548.520295	221158.458134	39.174580
2551.073443	221587.947979	39.179597
2553.964151	222001.253910	39.184615
2556.698828	222434.069201	39.189632
2558.919706	222844.329579	39.194650
2561.772841	223266.355391	39.199668
2564.525086	223694.570210	39.204685
2567.478954	224114.446611	39.209703
2569.919685	224539.839418	39.214720
2572.605984	224947.792262	39.219738
2575.454415	225351.070961	39.224756
2578.437684	225773.102324	39.229773
2581.411002	226174.430899	39.234791
2584.040946	226591.512630	39.239808
2586.906425	226995.677799	39.244826
2589.493819	227401.893121	39.249844
2591.958715	227814.173615	39.254861
2594.654004	228222.963219	39.259879
2597.115248	228634.024706	39.264896
2599.259049	229042.671284	39.269914
2602.129834	229450.544092	39.274932
2604.678077	229869.670132	39.279949
2606.928889	230277.512085	39.284967
2609.458511	230695.040210	39.289984
2612.331839	231105.935001	39.295002
2615.160500	231523.975049	39.300020
2617.817939	231942.447963	39.305037
2620.231344	232344.141166	39.310055
2623.061815	232758.801434	39.315072
2625.772339	233174.394619	39.320090
2628.342501	233586.706828	39.325108
2630.455459	234004.069028	39.330125
2633.258323	234424.016327	39.335143
2635.555228	234839.977376	39.340160
2638.104148	235268.194276	39.345178
2641.023345	235680.907621	39.350196
2643.630659	236109.419429	39.355213
2646.258467	236535.996901	39.360231
2649.360171	236942.558233	39.365248
2651.590782	237335.587491	39.370266
2654.360822	237716.135382	39.375284
2656.562071	238112.572426	39.380301
2658.889041	238502.765551	39.385319
2661.148685	238910.725775	39.390336
2663.801515	239306.811635	39.395354
2666.166400	239712.315679	39.400372
2668.807481	240119.046356	39.405389
2671.482652	240532.172812	39.410407
2674.105172	240958.846855	39.415424
2676.257477	241387.803489	39.420442
2679.199548	241813.130862	39.425460
2681.623169	242237.572886	39.430477
2685.072830	242652.861773	39.435495
2687.870357	243077.320368	39.440512
2690.563126	243512.108175	39.445530
2693.590912	243947.528911	39.450548
2696.219751	244376.050460	39.455565
2698.913904	244819.574171	39.460583
2701.321431	245248.992143	39.465600
2703.762962	245694.509369	39.470618
2706.451117	246134.652657	39.475636
2708.807733	246595.905465	39.480653
2711.227930	247048.764406	39.485671
2714.567212	247516.924058	39.490688
2716.662115	247984.514118	39.495706
2719.403103	248446.744130	39.500724
2722.139523	248919.922122	39.505741
2724.662285	249380.303899	39.510759
2727.854019	249859.809894	39.515776
2730.627004	250341.564292	39.520794
2733.671854	250803.943947	39.525812
2736.283590	251285.136435	39.530829
2739.306188	251760.141658	39.535847
2742.028714	252236.563849	39.540864
2744.599442	252709.883766	39.545882
2747.518758	253191.530547	39.550900
2750.444035	253673.479666	39.555917
2753.128715	254153.991349	39.560935
2755.929275	254629.885722	39.565952
2758.496011	255120.242900	39.570970
2761.459733	255604.516456	39.575988
2764.317937	256096.247289	39.581005
2767.032235	256580.327573	39.586023
2770.183886	257066.039904	39.591040
2772.880783	257556.494976	39.596058
2776.027866	258041.137524	39.601076
2778.923923	258515.682373	39.606093
2781.851549	258995.656251	39.611111
2784.614806	259486.347481	39.616128
2787.352453	259968.531551	39.621146
2790.298881	260437.168187	39.626164
2793.111893	260925.686737	39.631181
2795.822904	261411.983893	39.636199
2798.559959	261888.749914	39.641216
2801.243712	262377.714197	39.646234
2804.157423	262861.077990	39.651252
2807.307934	263344.250414	39.656269
2809.785965	263827.068150	39.661287
2812.661721	264312.056978	39.666304
2815.509311	264799.714906	39.671322
2818.200888	265274.390420	39.676340
2820.646562	265759.795063	39.681357
2823.661714	266246.353333	39.686375
2826.888664	266733.358878	39.691392
2829.336918	267225.105801	39.696410
2832.407111	267707.635373	39.701428
2834.967513	268181.580991	39.706445
2837.680194	268651.894009	39.711463
2840.493398	269098.111496	39.716480
2843.105393	269559.266902	39.721498
2845.880004	270004.800332	39.726516
2848.423457	270477.467152	39.731533
2850.706208	270951.365793	39.736551
2853.667532	271418.222798	39.741568
2856.316790	271885.862459	39.746586
2859.043418	272365.322785	39.751604
2862.422341	272858.291894	39.756621
2864.813863	273349.989623	39.761639
2867.363099	273836.758385	39.766656
2870.090367	274334.341083	39.771674
2873.393237	274825.456708	39.776692
2876.131247	275329.482564	39.781709
2878.707286	275839.270113	39.786727
2881.716429	276344.923692	39.791744
2884.599784	276854.225309	39.796762
2887.524708	277361.130004	39.801780
2890.330446	277883.617552	39.806797
2893.091236	278397.220184	39.811815
2896.153739	278924.105019	39.816832
2899.434686	279450.444344	39.821850
2902.201563	279987.703683	39.826868
2905.069140	280504.043597	39.831885
2908.135086	281035.712818	39.836903
2911.263835	281575.443873	39.841920
2913.898478	282107.781928	39.846938
2916.708900	282649.459130	39.851956
2919.867319	283183.917020	39.856973
2922.260971	283728.368045	39.861991
2925.548529	284265.819517	39.867008
2928.449737	284829.253514	39.872026
2931.389915	285376.425290	39.877044
2934.638209	285925.068319	39.882061
2937.491701	286483.595311	39.887079
2940.692287	287025.507772	39.892096
2943.663451	287593.503971	39.897114
2946.822228	288126.425093	39.902132
2949.958395	288682.985180	39.907149
2952.992361	289230.643947	39.912167
2956.039707	289781.139803	39.917184
2958.946748	290327.793285	39.922202
2962.261824	290875.698873	39.927220
2965.418222	291423.548193	39.932237
2968.001224	291974.833460	39.937255
2971.506645	292515.433293	39.942272
2974.367315	293072.022848	39.947290
2977.422108	293626.545901	39.952308
2980.550244	294164.625373	39.957325
2983.145787	294711.212136	39.962343
2986.410390	295266.347423	39.967360
2989.310700	295823.946094	39.972378
2992.463843	296367.942557	39.977396
2995.551449	296926.847081	39.982413
2998.108241	297467.193868	39.987431
3001.640891	298006.520478	39.992448
3005.346747	298545.789595	39.997466
3008.173395	299082.093078	40.002484
3011.534001	299611.834573	40.007501
3014.161513	300161.309160	40.012519
3017.606346	300694.632068	40.017536
3020.590319	301242.948682	40.022554
3023.611401	301770.081901	40.027572
3026.852764	302288.925241	40.032589
3029.337003	302831.185392	40.037607
3032.825256	303360.667204	40.042624
3035.575219	303884.546913	40.047642
3038.794550	304384.511900	40.052660
3041.237468	304886.496740	40.057677
3044.162953	305391.117731	40.062695
3047.105646	305892.659588	40.067712
3049.596845	306395.510575	40.072730
3052.452915	306914.240722	40.077748
3055.447754	307430.659414	40.082765
3057.582692	307949.287997	40.087783
3060.606880	308475.742998	40.092800
3063.809795	309018.942452	40.097818
3066.782614	309557.196758	40.102836
3069.294158	310097.141341	40.107853
3072.098662	310652.770979	40.112871
3075.328030	311207.693540	40.117888
3078.313975	311766.936939	40.122906
3081.277300	312343.740793	40.127924
3084.451007	312924.362682	40.132941
3087.299427	313495.053568	40.137959
3090.774024	314071.350478	40.142976
3094.030095	314650.770505	40.147994
3096.737065	315228.593632	40.153012
3099.720709	315816.568702	40.158029
3102.770507	316413.839781	40.163047
3106.082638	317001.367617	40.168064
3109.336898	317617.066203	40.173082
3112.266482	318221.539143	40.178100
3115.539445	318814.809768	40.183117
3118.746476	319427.191391	40.188135
3122.270031	320037.840292	40.193152
3125.526111	320652.201729	40.198170
3128.659331	321261.472967	40.203188
3132.121173	321858.732550	40.208205
3134.985976	322472.798788	40.213223
3138.125389	323083.895258	40.218240
3141.624834	323692.262481	40.223258
3144.798610	324308.664276	40.228276
3148.479135	324916.351016	40.233293
3151.448397	325533.020064	40.238311
3155.238535	326129.279194	40.243328
3158.796080	326724.550860	40.248346
3162.298546	327326.774258	40.253364
3165.630085	327919.272489	40.258381
3169.090978	328496.341405	40.263399
3172.781783	329075.725640	40.268416
3176.414998	329655.795325	40.273434
3179.536212	330238.676081	40.278452
3182.662242	330808.558030	40.283469
3185.173931	331400.877673	40.288487
3188.432248	331991.245463	40.293504
3191.715945	332567.444505	40.298522
3194.486301	333153.380031	40.303540
3197.802996	333752.387410	40.308557
3200.948007	334343.979324	40.313575
3203.728158	334921.895099	40.318592
3207.527486	335518.363928	40.323610
3210.233331	336120.878295	40.328628
3213.527214	336707.868886	40.333645
3216.426294	337304.550390	40.338663
3219.805054	337904.419582	40.343680
3222.842677	338501.313561	40.348698
3226.040573	339105.249337	40.353716
3229.826280	339705.532561	40.358733
3232.489733	340306.614417	40.363751
3235.507630	340907.757767	40.368768
3238.871734	341506.351497	40.373786
3241.626585	342121.236179	40.378804
3245.176006	342729.062697	40.383821
3248.357734	343335.693118	40.388839
3251.361184	343907.165357	40.393856
3254.501094	344487.305459	40.398874
3257.272592	345066.757635	40.403892
3260.345862	345643.972096	40.408909
3263.536939	346228.943619	40.413927
3266.881638	346809.139055	40.418944
3270.238330	347397.614710	40.423962
3272.928188	348002.666253	40.428980
3276.519771	348591.642161	40.433997
3279.686387	349190.461425	40.439015
3283.070125	349798.288211	40.444032
3286.713844	350401.549941	40.449050
3289.551842	351013.191735	40.454068
3292.929974	351624.763313	40.459085
3296.196623	352247.395166	40.464103
3299.524623	352865.619196	40.469120
3303.144458	353479.044783	40.474138
3306.259578	354093.982204	40.479156
3309.936438	354716.147121	40.484173
3313.696504	355329.337590	40.489191
3317.158818	355954.173350	40.494208
3320.540757	356564.330946	40.499226
3323.755445	357200.588141	40.504244
3327.348816	357817.456722	40.509261
3330.630138	358447.568515	40.514279
3334.095562	359065.065675	40.519296
3337.558354	359690.560809	40.524314
3340.500983	360324.818288	40.529332
3343.974081	360962.097614	40.534349
3347.575416	361602.917360	40.539367
3350.929564	362245.409343	40.544384
3354.585460	362876.460321	40.549402
3357.843596	363506.089740	40.554420
3360.580026	364152.666369	40.559437
3363.798357	364803.006056	40.564455
3367.087967	365455.195590	40.569472
3370.649025	366113.993424	40.574490
3373.832979	366775.191773	40.579508
3377.179908	367432.193552	40.584525
3380.515769	368114.928535	40.589543
3383.594022	368780.962562	40.594560
3387.226807	369443.853892	40.599578
3391.008824	370119.654824	40.604596
3394.771929	370776.919892	40.609613
3397.927286	371449.188232	40.614631
3401.643874	372109.343066	40.619648
3405.188481	372777.135348	40.624666
3408.268204	373453.218102	40.629684
3412.101446	374116.093793	40.634701
3415.544934	374786.538573	40.639719
3419.091689	375473.164780	40.644736
3422.942811	376133.759156	40.649754
3425.817209	376806.319919	40.654772
3429.411344	377465.528295	40.659789
3432.852747	378132.951716	40.664807
3436.031686	378808.910545	40.669824
3439.693496	379472.289027	40.674842
3442.961819	380149.719526	40.679860
3446.646299	380807.158984	40.684877
3450.433524	381478.395378	40.689895
3453.960191	382144.766719	40.694912
3457.377400	382805.819231	40.699930
3461.243406	383473.851135	40.704948
3464.536833	384144.436736	40.709965
3468.200925	384815.656208	40.714983
3471.409030	385490.145203	40.720000
3475.029888	386148.952449	40.725018
3478.289709	386796.804407	40.730023
3481.659373	387422.141184	40.735028
3484.603894	387993.632096	40.740032
3487.562493	388511.770938	40.745037
3490.501731	388988.497590	40.750042
3493.420604	389431.049424	40.755047
3495.835287	389812.950747	40.760052
3498.245357	390159.663668	40.765056
3500.172100	390447.555101	40.770061
3502.353694	390694.078094	40.775066
3503.862454	390912.806360	40.780071
3505.571264	391089.009145	40.785076
3507.245261	391237.192579	40.790080
3508.706973	391345.149938	40.795085
3510.045155	391418.503065	40.800090
3510.923814	391476.900528	40.805095
3512.329785	391492.317963	40.810100
3513.070871	391490.121274	40.815104
3513.918164	391459.529447	40.820109
3514.523582	391404.251756	40.825114
3514.948694	391349.408134	40.830119
3515.728870	391271.663924	40.835124
3516.090273	391169.819375	40.840128
3516.326085	391054.032857	40.845133
3516.840353	390922.921333	40.850138
3516.857552	390806.558454	40.855143
3516.783640	390657.006667	40.860148
3517.128552	390511.399529	40.865152
3517.425849	390365.088173	40.870157
3517.681087	390191.265498	40.875162
3517.720410	390020.191382	40.880167
3517.499024	389834.179467	40.885172
3517.279558	389646.947362	40.890176
3517.719353	389470.298524	40.895181
3517.701676	389284.149237	40.900186
3517.322501	389099.755658	40.905191
3517.253877	388905.614930	40.910196
3516.915439	388720.856797	40.915200
3516.584549	388527.109335	40.920205
3516.900892	388327.877691	40.925210
3516.670620	388140.458220	40.930215
3516.579651	387952.634861	40.935220
3516.487042	387755.010897	40.940224
3515.979226	387567.147966	40.945229
3515.558853	387377.949866	40.950234
3515.564809	387201.225547	40.955239
3515.833754	387002.600052	40.960244
3515.209526	386818.202395	40.965248
3514.875840	386637.033270	40.970253
3515.225311	386443.925494	40.975258
3514.602479	386270.694559	40.980263
3514.292756	386089.568555	40.985268
3514.212992	385918.586476	40.990272
3514.138882	385751.994696	40.995277
3513.582111	385571.360438	41.000282
3513.532110	385406.260611	41.005287
3513.675851	385232.166995	41.010292
3513.277495	385068.718739	41.015296
3512.726415	384906.359582	41.020301
3513.062360	384741.169997	41.025306
3512.972508	384587.750563	41.030311
3512.528955	384418.770078	41.035316
3512.499029	384263.231959	41.040320
3512.261513	384106.887301	41.045325
3511.733338	383950.180664	41.050330
3511.828507	383807.823629	41.055335
3511.554673	383654.351064	41.060340
3511.469251	383508.643433	41.065344
3511.132531	383359.723961	41.070349
3510.838571	383217.728913	41.075354
3510.840195	383088.916240	41.080359
3510.525499	382947.405376	41.085364
3510.580035	382804.338145	41.090368
3510.206144	382687.033747	41.095373
3510.122010	382543.986655	41.100378
3510.052765	382426.100428	41.105383
3510.018641	382288.554314	41.110388
3509.884148	382172.099073	41.115392
3509.381543	382052.348735	41.120397
3509.681383	381919.243232	41.125402
3509.504575	381801.954948	41.130407
3509.277124	381685.664352	41.135412
3508.967244	381566.795943	41.140416
3508.901064	381448.016038	41.145421
3508.865618	381345.381109	41.150426
3508.505350	381224.385923	41.155431
3508.248281	381119.372195	41.160436
3507.910149	381000.327847	41.165440
3508.008833	380915.471463	41.170445
3508.282491	380804.203148	41.175450
3507.821548	380704.044352	41.180455
3507.622677	380602.980986	41.185460
3507.462029	380502.216015	41.190464
3507.464456	380409.297562	41.195469
3507.548462	380315.426489	41.200474
3507.452136	380222.929057	41.205479
3507.510833	380122.991917	41.210484
3507.410901	380029.859500	41.215488
3507.311926	379943.532439	41.220493
3507.371902	379845.397085	41.225498
3507.092733	379769.763392	41.230503
3507.111494	379670.338651	41.235508
3506.913970	379584.025749	41.240512
3506.317873	379495.184264	41.245517
3506.597185	379403.996853	41.250522
3506.764181	379327.276648	41.255527
3506.604440	379245.629532	41.260532
3506.173083	379169.154353	41.265536
3506.336853	379088.421444	41.270541
3506.354855	379006.212621	41.275546
3505.996555	378927.515940	41.280551
3506.321396	378849.042867	41.285556
3506.134112	378771.030197	41.290560
3505.683610	378704.943631	41.295565
3506.359899	378615.113914	41.300570
3505.904740	378548.748326	41.305575
3505.636100	378469.503014	41.310580
3505.765697	378400.430239	41.315584
3505.544597	378333.367385	41.320589
3505.649496	378262.240983	41.325594
3505.382894	378192.873773	41.330599
3505.361899	378124.128475	41.335604
3505.546373	378059.541484	41.340608
3505.264777	378000.106216	41.345613
3505.338876	377912.094819	41.350618
3505.058906	377852.024047	41.355623
3505.019005	377793.185630	41.360628
3505.153395	377728.478648	41.365632
3504.907837	377678.941894	41.370637
3505.450352	377611.606015	41.375642
3505.386328	377553.050192	41.380647
3505.201191	377496.036923	41.385652
3505.403251	377418.950202	41.390656
3505.183660	377345.382917	41.395661
3505.142849	377278.771910	41.400666
3505.191972	377215.423022	41.405671
3505.077349	377156.036088	41.410676
3505.202736	377091.024196	41.415680
3504.898535	377042.790670	41.420685
3505.178514	376972.065355	41.425690
3504.765511	376917.321315	41.430695
3504.395445	376854.316182	41.435700
3504.452807	376789.314146	41.440704
3504.398344	376736.926747	41.445709
3504.823462	376678.521481	41.450714
3504.396036	376627.334817	41.455719
3504.517334	376575.732492	41.460724
3504.502438	376518.335081	41.465728
3504.459787	376460.637089	41.470733
3504.641713	376402.015086	41.475738
3504.510302	376352.661309	41.480743
3504.083377	376301.346955	41.485748
3504.088435	376248.517572	41.490752
3504.277198	376208.485724	41.495757
3504.143497	376147.143851	41.500762
3504.089556	376104.177990	41.505767
3504.072222	376051.656489	41.510772
3504.133425	375995.541454	41.515776
3503.877032	375956.340464	41.520781
3504.038007	375901.251054	41.525786
3503.941769	375860.907459	41.530791
3503.890191	375813.216593	41.535796
3504.230768	375763.432708	41.540800
3503.851164	375734.333922	41.545805
3504.145274	375678.943955	41.550810
3503.962152	375629.241319	41.555815
3503.849141	375576.225804	41.560820
3504.485177	375535.488384	41.565824
3503.803705	375479.640245	41.570829
3503.898958	375433.906996	41.575834
3503.880330	375386.591240	41.580839
3503.848751	375332.038623	41.585844
3504.097817	375283.893654	41.590848
3503.923243	375245.872673	41.595853
3504.022146	375196.328552	41.600858
3503.914652	375151.464559	41.605863
3503.764031	375096.929994	41.610868
3504.061046	375050.555116	41.615872
3503.972006	375015.873242	41.620877
3504.047717	374963.004961	41.625882
3504.313290	374904.519104	41.630887
3504.054410	374851.982070	41.635892
3503.886043	374800.675440	41.640896
3503.958016	374762.259820	41.645901
3504.048580	374709.337936	41.650906
3503.969768	374660.303093	41.655911
3503.859464	374614.956055	41.660916
3504.093374	374564.856379	41.665920
3503.736755	374517.693310	41.670925
3503.921603	374468.921894	41.675930
3503.526083	374421.078909	41.680935
3503.450426	374387.537160	41.685940
3503.993784	374346.405985	41.690944
3503.981308	374300.738400	41.695949
3504.205274	374249.598285	41.700954
3503.904805	374205.245370	41.705959
3503.869172	374163.162606	41.710964
3503.806605	374105.183308	41.715968
3503.568627	374062.293661	41.720973
3503.837519	374013.736962	41.725978
3503.453646	373968.761630	41.730983
3503.965774	373929.920740	41.735988
3503.954018	373892.405950	41.740992
3503.440930	373846.866311	41.745997
3503.577516	373795.205532	41.751002
3503.933728	373753.391371	41.756007
3503.459148	373709.318755	41.761012
3503.902871	373658.168741	41.766016
3503.825670	373615.507386	41.771021
3503.732918	373574.296237	41.776026
3503.612853	373538.880692	41.781031
3503.643834	373489.140842	41.786036
3503.402928	373442.516737	41.791040
3503.497581	373407.575631	41.796045
3503.651969	373361.296292	41.801050
3503.661754	373322.558119	41.806055
3503.379681	373281.528398	41.811060
3503.395007	373227.345304	41.816064
3503.461118	373193.678430	41.821069
3503.258822	373150.934216	41.826074
3503.207784	373113.500680	41.831079
3503.389334	373069.578949	41.836084
3503.212350	373023.299807	41.841088
3503.066122	372993.120324	41.846093
3503.396818	372950.013442	41.851098
3503.177638	372921.851951	41.856103
3502.923897	372872.993546	41.861108
3503.054814	372839.646376	41.866112
3503.072447	372816.604449	41.871117
3503.117497	372777.097974	41.876122
3503.063156	372743.652508	41.881127
3502.908800	372714.032822	41.886132
3503.203130	372672.150449	41.891136
3502.622653	372645.416592	41.896141
3502.723496	372606.815655	41.901146
3502.684307	372574.459905	41.906151
3502.862457	372546.058388	41.911156
3503.067490	372512.724693	41.916160
3502.929332	372475.126036	41.921165
3503.239520	372445.128950	41.926170
3503.099736	372397.699884	41.931175
3502.987986	372373.560034	41.936180
3502.934285	372337.091137	41.941184
3503.003403	372299.155162	41.946189
3502.754801	372265.307513	41.951194
3503.020382	372229.474648	41.956199
3502.592921	372194.943486	41.961204
3503.059536	372157.301092	41.966208
3503.016673	372128.806530	41.971213
3502.788075	372091.577058	41.976218
3502.526016	372059.356997	41.981223
3502.591505	372029.549955	41.986228
3502.901358	371999.349221	41.991232
3502.846993	371963.337180	41.996237
3503.265431	371934.846842	42.001242
3503.341970	371901.252983	42.006247
3503.060797	371854.937296	42.011252
3503.076090	371820.006536	42.016256
3502.755609	371789.522626	42.021261
3502.971653	371752.477533	42.026266
3503.086551	371724.135825	42.031271
3503.157747	371689.018384	42.036276
3503.014382	371651.368616	42.041280
3502.905872	371615.516967	42.046285
3503.158205	371585.248528	42.051290
3503.116728	371543.518321	42.056295
3503.085219	371523.709121	42.061300
3503.176263	371466.335454	42.066304
3502.909784	371448.188547	42.071309
3503.019471	371405.850346	42.076314
3503.123451	371379.288189	42.081319
3502.961405	371334.528081	42.086324
3503.427711	371296.630545	42.091328
3503.164535	371266.645204	42.096333
3503.170557	371226.710748	42.101338
3503.222038	371190.909865	42.106343
3503.065961	371152.524713	42.111348
3503.295786	371114.079457	42.116352
3502.841939	371078.255453	42.121357
3503.306861	371037.893671	42.126362
3503.206513	371003.157708	42.131367
3502.740905	370972.543067	42.136372
3503.379238	370938.530384	42.141376
3503.364195	370902.358435	42.146381
3503.181790	370859.074128	42.151386
3503.210352	370820.278737	42.156391
3502.785450	370781.503050	42.161396
3502.972733	370734.833169	42.166400
3502.963951	370707.068554	42.171405
3502.924290	370669.553748	42.176410
3503.040162	370638.390992	42.181415
3502.774781	370603.222949	42.186420
3503.007320	370566.326141	42.191424
3502.309185	370549.058738	42.196429
3502.833984	370513.640602	42.201434
3502.740270	370482.205443	42.206439
3502.902117	370450.654269	42.211444
3502.999549	370411.898404	42.216448
3502.902854	370387.297224	42.221453
3502.825718	370357.586806	42.226458
3503.007819	370321.281814	42.231463
3502.648486	370289.151060	42.236468
3502.677619	370251.828221	42.241472
3502.935314	370240.483431	42.246477
3502.403210	370204.213216	42.251482
3502.389810	370168.243297	42.256487
3502.652307	370142.061766	42.261492
3502.969248	370100.299041	42.266496
3502.974783	370070.931112	42.271501
3503.003158	370041.229345	42.276506
3503.203462	370008.630121	42.281511
3502.986116	369963.724006	42.286516
3502.991297	369924.600763	42.291520
3502.797704	369887.998016	42.296525
3502.954980	369855.125864	42.301530
3502.829753	369823.059765	42.306535
3502.725866	369791.041117	42.311540
3502.815204	369751.904539	42.316544
3503.209087	369727.175634	42.321549
3502.946742	369693.784291	42.326554
3502.827659	369656.407516	42.331559
3502.334431	369628.717223	42.336564
3502.734973	369591.538952	42.341568
3502.636247	369563.152092	42.346573
3502.632259	369524.055125	42.351578
3502.514338	369501.793699	42.356583
3502.534156	369479.612440	42.361588
3502.618489	369447.868970	42.366592
3502.830757	369420.119498	42.371597
3502.793264	369385.244732	42.376602
3502.752215	369354.867119	42.381607
3502.759538	369321.052301	42.386612
3502.968721	369278.542987	42.391616
3502.736661	369262.193052	42.396621
3502.844406	369226.355511	42.401626
3503.039220	369193.400535	42.406631
3502.818284	369153.930339	42.411636
3503.095125	369123.477605	42.416640
3502.496701	369094.278861	42.421645
3502.818310	369058.001347	42.426650
3502.572757	369030.271927	42.431655
3502.545009	369005.557194	42.436660
3502.835185	368966.743949	42.441664
3502.457366	368941.067432	42.446669
3502.476237	368913.804852	42.451674
3502.589615	368886.756186	42.456679
3502.700090	368855.922572	42.461684
3502.858763	368822.871169	42.466688
3502.593057	368797.075454	42.471693
3502.712123	368757.780446	42.476698
3502.489257	368727.405049	42.481703
3502.353414	368687.793936	42.486708
3502.673358	368670.544790	42.491712
3502.743012	368650.717827	42.496717
3502.604723	368606.406985	42.501722
3502.659043	368568.417468	42.506727
3502.667144	368539.149174	42.511732
3502.645057	368515.322326	42.516736
3502.680387	368494.382754	42.521741
3502.574088	368467.190035	42.526746
3502.943109	368425.035656	42.531751
3502.482403	368402.064541	42.536756
3502.656887	368371.398281	42.541760
3502.548346	368339.099256	42.546765
3502.941559	368311.345951	42.551770
3502.622452	368266.783256	42.556775
3502.438525	368239.627806	42.561780
3502.269995	368211.326675	42.566784
3502.294319	368184.494447	42.571789
3502.658329	368156.720130	42.576794
3502.553099	368122.159226	42.581799
3502.526641	368107.072331	42.586804
3502.773819	368066.181270	42.591808
3502.491550	368036.017627	42.596813
3502.419660	368019.362587	42.601818
3502.857167	367985.860329	42.606823
3502.413364	367951.758401	42.611828
3502.690929	367914.622483	42.616832
3502.498153	367895.572609	42.621837
3502.502232	367875.221784	42.626842
3502.670046	367836.095764	42.631847
3502.414117	367813.422588	42.636852
3502.466404	367779.497318	42.641856
3502.590848	367757.349248	42.646861
3502.503655	367729.441481	42.651866
3502.752496	367695.688775	42.656871
3502.538000	367666.886133	42.661876
3502.288330	367633.439584	42.666880
3502.348883	367611.758658	42.671885
3502.321302	367576.244978	42.676890
3502.820596	367547.356547	42.681895
3502.917304	367517.895574	42.686900
3502.717499	367485.000034	42.691904
3502.467970	367465.221918	42.696909
3502.484820	367425.432855	42.701914
3502.893971	367402.427201	42.706919
3502.684999	367380.889667	42.711924
3502.656462	367343.800645	42.716928
3502.723358	367315.538212	42.721933
3502.305151	367280.821743	42.726938
3502.628041	367255.060075	42.731943
3501.981395	367227.264283	42.736948
3502.039743	367203.017320	42.741952
3502.127119	367180.010747	42.746957
3502.177523	367143.747603	42.751962
3502.555772	367127.606352	42.756967
3501.946455	367107.121774	42.761972
3501.998187	367077.794383	42.766976
3502.069169	367064.902166	42.771981
3502.195084	367033.708491	42.776986
3501.976511	367013.061414	42.781991
3501.940063	367000.516174	42.786996
3502.063763	366970.262828	42.792001
3502.249729	366959.359814	42.797005
3502.294456	366918.752692	42.802010
3502.750271	366900.083959	42.807015
3502.331691	366873.090764	42.812020
3502.457026	366838.695690	42.817025
3502.286101	366816.059312	42.822029
3502.154313	366792.756243	42.827034
3501.976908	366761.279182	42.832039
3502.414665	366750.819642	42.837044
3502.628989	366724.185146	42.842049
3502.327934	366696.716169	42.847053
3502.437639	366665.677061	42.852058
3502.033098	366635.022829	42.857063
3502.203186	366618.380136	42.862068
3502.293942	366585.997310	42.867073
3501.834066	366563.990064	42.872077
3502.237719	366544.998925	42.877082
3502.019237	366518.939735	42.882087
3502.446877	366498.191731	42.887092
3502.512321	366471.961280	42.892097
3501.860078	366456.234085	42.897101
3502.266488	366429.112095	42.902106
3502.321683	366402.451250	42.907111
3502.075052	366382.112976	42.912116
3502.127600	366357.256427	42.917121
3502.232639	366332.061392	42.922125
3502.206057	366306.759779	42.927130
3502.373246	366284.578519	42.932135
3501.925415	366257.665521	42.937140
3502.263212	366222.144130	42.942145
3502.073014	366211.019887	42.947149
3502.531315	366178.655633	42.952154
3502.242439	366158.222145	42.957159
3502.046072	366133.277100	42.962164
3502.460928	366107.576321	42.967169
3502.276380	366086.897880	42.972173
3502.171798	366056.272578	42.977178
3502.316985	366037.981928	42.982183
3501.936338	366012.735155	42.987188
3502.358442	365987.363442	42.992193
3502.041887	365971.710784	42.997197
3502.127661	365940.572992	43.002202
3502.199341	365912.333849	43.007207
3501.744413	365897.871443	43.012212
3501.947891	365872.000086	43.017217
3502.048090	365848.634748	43.022221
3502.179900	365827.449551	43.027226
3502.195076	365804.961276	43.032231
3502.156754	365783.954969	43.037236
3501.872175	365763.647573	43.042241
3502.096609	365735.105001	43.047245
3502.226112	365714.174159	43.052250
3502.157334	365696.526380	43.057255
3502.358627	365677.642389	43.062260
3502.426638	365643.661345	43.067265
3502.316438	365615.551849	43.072269
3502.176215	365592.554023	43.077274
3502.644968	365557.595827	43.082279
3502.235055	365537.688899	43.087284
3502.216852	365507.837230	43.092289
3502.414834	365488.597916	43.097293
3502.744679	365466.365312	43.102298
3502.517419	365428.212204	43.107303
3502.476219	365403.369427	43.112308
3502.352913	365375.312555	43.117313
3502.358597	365355.239196	43.122317
3502.335444	365333.544179	43.127322
3502.808925	365305.699272	43.132327
3502.327991	365269.999223	43.137332
3502.782744	365238.625404	43.142337
3502.329592	365217.124255	43.147341
3502.427594	365195.537324	43.152346
3502.121987	365162.350704	43.157351
3501.970157	365150.356195	43.162356
3502.068379	365112.634786	43.167361
3502.012773	365089.572579	43.172365
3502.204947	365067.996308	43.177370
3502.424699	365039.225106	43.182375
3502.079090	365027.616421	43.187380
3502.163270	364987.457812	43.192385
3502.223505	364971.644347	43.197389
3501.841293	364948.658261	43.202394
3502.285914	364920.106036	43.207399
3501.851804	364898.017289	43.212404
3502.311733	364871.114199	43.217409
3502.228671	364859.362957	43.222413
3502.317468	364824.793324	43.227418
3501.988931	364805.203545	43.232423
3501.899108	364773.837744	43.237428
3501.914292	364753.076455	43.242433
3501.995305	364737.564537	43.247437
3502.346176	364714.260918	43.252442
3502.317799	364691.676927	43.257447
3502.045531	364676.397813	43.262452
3502.464790	364648.865626	43.267457
3501.962963	364628.794516	43.272461
3501.815265	364600.689878	43.277466
3502.218312	364581.163967	43.282471
3501.891520	364556.339503	43.287476
3502.005469	364538.611771	43.292481
3502.572816	364508.769598	43.297485
3502.067721	364489.130855	43.302490
3502.177882	364465.025997	43.307495
3501.982444	364438.224494	43.312500
3502.369202	364412.907734	43.317505
3502.210006	364388.616048	43.322509
3501.859992	364372.739054	43.327514
3502.306057	364343.042631	43.332519
3502.217325	364319.959563	43.337524
3502.127976	364291.134090	43.342529
3502.179314	364267.825910	43.347533
3501.885385	364249.653291	43.352538
3501.868053	364227.651637	43.357543
3501.819627	364206.798223	43.362548
3502.261649	364173.849870	43.367553
3502.168126	364162.963893	43.372557
3502.030212	364134.476146	43.377562
3502.104460	364117.669075	43.382567
3501.803928	364094.390104	43.387572
3502.060927	364077.452934	43.392577
3502.059153	364053.111064	43.397581
3502.136575	364040.419781	43.402586
3502.229148	364012.251780	43.407591
3501.949625	363994.915273	43.412596
3502.342097	363971.248860	43.417601
3501.993602	363945.360056	43.422605
3502.044470	363922.991828	43.427610
3502.150550	363898.328132	43.432615
3501.965814	363872.794925	43.437620
3501.645251	363849.468057	43.442625
3501.959998	363826.906236	43.447629
3501.870569	363816.553096	43.452634
3502.017981	363788.579625	43.457639
3502.065607	363763.975732	43.462644
3501.815269	363745.821426	43.467649
3502.197635	363727.543244	43.472653
3502.047940	363716.513384	43.477658
3502.174509	363679.649653	43.482663
3502.114160	363665.200965	43.487668
3502.545348	363638.224993	43.492673
3502.219265	363608.495528	43.497677
3502.107986	363587.778506	43.502682
3502.432287	363551.341221	43.507687
3502.086634	363535.463095	43.512692
3502.071519	363504.668741	43.517697
3502.127579	363492.844483	43.522701
3502.175676	363462.065658	43.527706
3502.122403	363443.931321	43.532711
3501.822191	363431.349360	43.537716
3501.932526	363403.406704	43.542721
3502.211648	363389.311615	43.547725
3502.019208	363361.746365	43.552730
3502.022330	363333.718686	43.557735
3501.645485	363325.290442	43.562740
3501.947144	363293.150661	43.567745
3501.993126	363276.195049	43.572749
3501.837204	363266.284034	43.577754
3501.791195	363230.132670	43.582759
3501.500211	363221.767265	43.587764
3501.544061	363198.611867	43.592769
3501.657966	363182.712858	43.597773
3501.688905	363174.043243	43.602778
3502.022288	363149.089449	43.607783
3501.784327	363139.318209	43.612788
3501.957815	363117.616366	43.617793
3501.985204	363098.605317	43.622797
3501.715963	363074.660005	43.627802
3501.963044	363051.396635	43.632807
3501.879516	363027.498616	43.637812
3501.951452	363012.698690	43.642817
3502.200978	362996.753067	43.647821
3501.690937	362974.801741	43.652826
3502.165119	362946.420879	43.657831
3501.987841	362930.389174	43.662836
3502.330369	362900.224618	43.667841
3501.909296	362881.715194	43.672845
3502.027391	362856.565961	43.677850
3502.221386	362832.218031	43.682855
3501.808706	362806.516090	43.687860
3502.236109	362793.210779	43.692865
3501.945432	362776.383502	43.697869
3502.020610	362747.251403	43.702874
3502.095336	362733.848484	43.707879
3502.224886	362709.332609	43.712884
3501.930583	362687.550782	43.717889
3501.913373	362669.664465	43.722893
3501.690919	362646.321380	43.727898
3501.977206	362617.893212	43.732903
3502.272226	362611.240601	43.737908
3502.016004	362579.568021	43.742913
3501.832603	362556.599949	43.747917
3501.678571	362539.420934	43.752922
3502.056153	362518.500037	43.757927
3501.873259	362499.750024	43.762932
3502.205069	362484.045430	43.767937
3502.274095	362458.496924	43.772941
3502.270863	362429.224251	43.777946
3502.217088	362402.500498	43.782951
3502.067735	362382.068077	43.787956
3502.089075	362361.202505	43.792961
3502.230135	362340.699452	43.797965
3501.854474	362322.055557	43.802970
3502.065094	362295.849606	43.807975
3501.741360	362277.121369	43.812980
3502.099579	362253.941725	43.817985
3501.933177	362221.390814	43.822989
3501.826714	362212.843944	43.827994
3502.054699	362186.787661	43.832999
3501.783584	362176.182698	43.838004
3501.510501	362145.096733	43.843009
3501.952173	362133.770971	43.848013
3501.506887	362114.858259	43.853018
3501.861825	362094.753744	43.858023
3501.442024	362076.319852	43.863028
3501.750906	362055.892133	43.868033
3501.789653	362041.198534	43.873037
3501.724561	362021.413442	43.878042
3501.753398	362002.121945	43.883047
3501.861856	361984.037783	43.888052
3501.647050	361969.815594	43.893057
3501.808076	361957.339112	43.898061
3501.841597	361933.040831	43.903066
3501.824375	361917.796833	43.908071
3501.652430	361892.844388	43.913076
3501.943794	361875.189101	43.918081
3501.807348	361858.591416	43.923085
3501.681959	361845.168415	43.928090
3502.041768	361827.527860	43.933095
3501.802313	361807.668115	43.938100
3501.853960	361787.229419	43.943105
3501.781950	361769.071564	43.948109
3501.824874	361756.486319	43.953114
3502.552309	361723.872007	43.958119
3501.925754	361706.486517	43.963124
3501.675785	361678.877835	43.968129
3501.874032	361664.337110	43.973133
3501.673016	361642.590825	43.978138
3501.879303	361622.432890	43.983143
3501.729924	361604.668148	43.988148
3501.480236	361587.833819	43.993153
3501.774058	361563.520144	43.998157
3501.784858	361556.759059	44.003162
3502.343943	361526.864355	44.008167
3501.885191	361524.420065	44.013172
3501.872170	361485.948996	44.018177
3501.695869	361478.429248	44.023181
3501.579801	361453.340683	44.028186
3502.027040	361439.599688	44.033191
3501.596948	361422.564635	44.038196
3502.052647	361388.416721	44.043201
3502.052347	361380.310503	44.048205
3501.479326	361357.884960	44.053210
3501.920789	361334.767887	44.058215
3501.814748	361317.529877	44.063220
3501.740954	361307.300489	44.068225
3502.114432	361275.401476	44.073229
3501.969295	361259.617989	44.078234
3501.831121	361229.907728	44.083239
3502.052413	361220.725100	44.088244
3502.395288	361190.736648	44.093249
3501.947962	361171.544125	44.098253
3501.779555	361154.341138	44.103258
3501.717085	361127.566775	44.108263
3501.628138	361110.148102	44.113268
3501.849545	361098.119282	44.118273
3502.004829	361077.943507	44.123277
3501.589588	361058.237679	44.128282
3501.814378	361026.361540	44.133287
3501.669201	361018.506477	44.138292
3501.685479	360998.174396	44.143297
3502.024294	360983.281112	44.148301
3501.380221	360976.520154	44.153306
3501.633106	360949.493263	44.158311
3501.526510	360948.188492	44.163316
3501.918065	360912.398235	44.168321
3502.009557	360891.622372	44.173325
3501.898672	360877.967972	44.178330
3501.938144	360859.207740	44.183335
3501.488292	360839.837512	44.188340
3501.326597	360829.265869	44.193345
3501.728467	360813.829033	44.198349
3501.585447	360798.172035	44.203354
3501.708392	360779.017580	44.208359
3501.892704	360774.033586	44.213364
3501.667461	360754.526702	44.218369
3501.633171	360734.176899	44.223373
3501.416585	360717.413168	44.228378
3501.461426	360692.273516	44.233383
3501.992157	360687.693022	44.238388
3501.490921	360666.450168	44.243393
3501.771814	360655.784179	44.248397
3501.619424	360632.708155	44.253402
3501.695905	360621.896077	44.258407
3501.484847	360605.410959	44.263412
3501.803724	360585.920944	44.268417
3501.909003	360568.090548	44.273421
3501.584104	360546.464396	44.278426
3501.301031	360534.488442	44.283431
3501.682868	360521.621230	44.288436
3501.501761	360492.323520	44.293441
3501.456697	360488.290021	44.298445
3501.488635	360465.413897	44.303450
3501.555399	360460.956393	44.308455
3501.479355	360460.460045	44.313460
3501.473471	360428.644584	44.318465
3501.811519	360411.794374	44.323469
3501.555428	360407.768290	44.328474
3501.525399	360382.385906	44.333479
3502.031328	360369.855095	44.338484
3502.019678	360353.059270	44.343489
3501.873705	360331.100170	44.348493
3501.856818	360310.823611	44.353498
3501.758163	360284.918160	44.358503
3501.870698	360266.527379	44.363508
3501.529620	360257.203256	44.368513
3501.743422	360231.604914	44.373517
3501.877698	360219.436826	44.378522
3502.046790	360201.291332	44.383527
3501.662659	360177.793593	44.388532
3502.030530	360164.953816	44.393537
3501.735247	360144.263038	44.398541
3501.962085	360133.579865	44.403546
3501.557330	360090.288722	44.408551
3501.309274	360101.585258	44.413556
3501.824050	360074.847198	44.418561
3501.760360	360053.129220	44.423565
3501.343479	360035.837196	44.428570
3501.852524	360017.943645	44.433575
3501.701225	360000.534034	44.438580
3501.604010	359986.572150	44.443585
3501.765831	359962.913049	44.448589
3501.212236	359967.039915	44.453594
3501.578783	359936.792407	44.458599
3501.815496	359926.412579	44.463604
3501.752432	359906.930737	44.468609
3501.530466	359888.718844	44.473613
3501.408322	359886.247450	44.478618
3501.652855	359858.483908	44.483623
3501.611453	359841.895734	44.488628
3501.550007	359834.001920	44.493633
3501.622207	359815.185121	44.498637
3501.393920	359800.023722	44.503642
3501.691996	359786.381428	44.508647
3501.461786	359774.193642	44.513652
3501.598120	359757.908133	44.518657
3502.102738	359741.895677	44.523661
3501.736762	359723.070767	44.528666
3502.028391	359696.163794	44.533671
3501.668745	359689.968199	44.538676
3501.821172	359665.039672	44.543681
3501.866465	359645.972824	44.548685
3501.466253	359636.327340	44.553690
3501.575743	359605.712893	44.558695
3501.670148	359596.549518	44.563700
3501.738498	359585.433377	44.568705
3501.929096	359564.387049	44.573709
3501.729420	359543.452264	44.578714
3502.170199	359525.187848	44.583719
3501.381658	359503.912646	44.588724
3501.591365	359483.015767	44.593729
3501.916560	359470.944738	44.598733
3501.590003	359459.610457	44.603738
3501.804172	359441.127121	44.608743
3501.948734	359417.978548	44.613748
3501.911858	359398.441478	44.618753
3501.826047	359371.262579	44.623757
3501.739351	359360.678751	44.628762
3501.971740	359341.506357	44.633767
3501.492633	359326.587060	44.638772
3501.860495	359300.684412	44.643777
3502.114194	359269.411851	44.648781
3501.661982	359263.484707	44.653786
3501.861750	359228.459300	44.658791
3501.722631	359224.186134	44.663796
3501.640718	359202.292488	44.668801
3501.733681	359186.420040	44.673805
3501.627387	359169.689116	44.678810
3501.697011	359142.943270	44.683815
3501.420914	359138.818474	44.688820
3501.757972	359107.380294	44.693825
3501.581288	359094.523151	44.698829
3501.514404	359083.554939	44.703834
3501.508191	359063.733333	44.708839
3501.546283	359059.940840	44.713844
3501.814092	359040.559437	44.718849
3501.470292	359021.857710	44.723853
3501.798846	359015.275334	44.728858
3501.612648	358994.414315	44.733863
3501.481012	358983.024111	44.738868
3501.184109	358961.214575	44.743873
3501.522868	358945.557890	44.748877
3501.427226	358938.914439	44.753882
3501.675875	358933.437271	44.758887
3501.933640	358910.601077	44.763892
3501.740900	358894.976246	44.768897
3501.843353	358873.206158	44.773901
3501.778732	358866.430795	44.778906
3502.167307	358832.239622	44.783911
3501.828167	358814.680667	44.788916
3501.412571	358792.203306	44.793921
3501.696940	358776.326274	44.798925
3501.871595	358771.470525	44.803930
3501.798908	358742.459223	44.808935
3501.608245	358734.890198	44.813940
3501.576234	358713.471302	44.818945
3501.591547	358695.069288	44.823949
3501.299124	358685.228830	44.828954
3501.847255	358652.817020	44.833959
3501.888196	358649.430657	44.838964
3501.511793	358638.383380	44.843969
3501.617974	358618.747308	44.848973
3501.409511	358608.410894	44.853978
3501.765696	358586.677360	44.858983
3501.707814	358581.247829	44.863988
3501.561327	358555.958286	44.868993
3501.704275	358536.036885	44.873997
3501.232838	358526.707100	44.879002
3501.499282	358500.463761	44.884007
3501.621853	358500.368514	44.889012
3501.611570	358485.197950	44.894017
3501.661650	358455.684403	44.899021
3501.793677	358445.396606	44.904026
3501.953314	358420.872568	44.909031
3502.014007	358418.093046	44.914036
3501.646169	358389.915180	44.919041
3501.673014	358369.376381	44.924045
3501.455716	358359.269986	44.929050
3501.631535	358339.877041	44.934055
3501.772645	358335.839699	44.939060
3501.822796	358310.544768	44.944065
3501.923114	358290.426527	44.949069
3502.053598	358276.250526	44.954074
3501.850663	358252.240232	44.959079
3501.368205	358236.177276	44.964084
3501.531621	358216.303311	44.969089
3501.752751	358217.031400	44.974093
3501.693497	358189.059473	44.979098
3501.629505	358176.667281	44.984103
3501.567926	358150.728831	44.989108
3501.372730	358141.762573	44.994113
3501.402160	358125.645318	44.999117
3501.533158	358103.463611	45.004122
3501.692939	358079.523810	45.009127
3501.736064	358074.383446	45.014132
3501.247865	358061.955562	45.019137
3501.410339	358046.579996	45.024141
3501.430544	358046.297362	45.029146
3501.603107	358018.594179	45.034151
3501.740424	358012.549639	45.039156
3501.667729	357984.427130	45.044161
3502.022042	357965.565293	45.049165
3501.219806	357955.117740	45.054170
3501.613713	357934.674019	45.059175
3501.720265	357920.399921	45.064180
3501.538447	357909.093369	45.069185
3501.817644	357889.607810	45.074189
3501.675996	357879.057435	45.079194
3501.856067	357855.520938	45.084199
3502.029201	357840.626489	45.089204
3501.548958	357821.004918	45.094209
3501.685911	357802.608855	45.099213
3501.245475	357780.109203	45.104218
3501.551295	357771.903557	45.109223
3501.849108	357759.658214	45.114228
3501.550721	357738.203845	45.119233
3501.684584	357717.266737	45.124237
3501.442240	357712.780689	45.129242
3501.431794	357681.369711	45.134247
3501.594233	357683.504760	45.139252
3501.712068	357663.230894	45.144257
3501.849834	357645.825789	45.149261
3501.688999	357626.561027	45.154266
3501.324487	357607.429607	45.159271
3501.600948	357603.879405	45.164276
3501.708902	357587.673405	45.169281
3501.562389	357565.051612	45.174285
3501.626527	357566.719083	45.179290
3501.937674	357542.628238	45.184295
3501.697327	357528.916238	45.189300
3501.462883	357499.039411	45.194305
3501.739596	357486.263529	45.199309
3501.366779	357479.383329	45.204314
3501.469646	357444.574287	45.209319
3501.705955	357438.488815	45.214324
3501.295403	357441.678815	45.219329
3501.932280	357409.658530	45.224333
3501.729112	357404.429304	45.229338
3501.613223	357370.264180	45.234343
3501.714298	357366.944564	45.239348
3501.684263	357348.548801	45.244353
3501.470247	357326.648960	45.249357
3501.503252	357315.588328	45.254362
3501.224624	357301.704278	45.259367
3501.636603	357281.740201	45.264372
3501.510013	357271.593918	45.269377
3501.441118	357249.823930	45.274381
3501.107596	357240.218141	45.279386
3501.848526	357224.193018	45.284391
3501.676200	357221.805461	45.289396
3501.318893	357193.497784	45.294401
3501.978574	357187.371796	45.299405
3501.767215	357157.541878	45.304410
3501.482179	357150.368376	45.309415
3501.256263	357140.059599	45.314420
3501.355698	357117.348376	45.319425
3501.474943	357096.870597	45.324429
3501.714482	357090.428741	45.329434
3501.544451	357065.141637	45.334439
3501.369413	357058.586380	45.339444
3501.608706	357054.381101	45.344449
3501.734542	357022.465356	45.349453
3501.951489	357014.120849	45.354458
3502.200089	356989.556415	45.359463
3501.904856	356979.232955	45.364468
3501.263684	356954.476554	45.369473
3501.694012	356937.050940	45.374477
3501.668051	356917.485178	45.379482
3501.365204	356904.951737	45.384487
3501.504277	356901.499080	45.389492
3501.636064	356886.458115	45.394497
3501.397857	356858.004520	45.399501
3501.381985	356857.498749	45.404506
3501.557016	356839.680745	45.409511
3501.462607	356819.236031	45.414516
3501.751159	356823.765988	45.419521
3501.617115	356787.544391	45.424525
3501.548021	356780.998004	45.429530
3501.356596	356763.618215	45.434535
3501.614955	356733.486054	45.439540
3501.655903	356723.110195	45.444545
3501.635091	356710.685280	45.449549
3501.400647	356694.760835	45.454554
3501.359314	356690.243358	45.459559
3502.042645	356676.056841	45.464564
3501.481518	356656.015049	45.469569
3501.606244	356630.681724	45.474573
3501.365030	356617.833587	45.479578
3501.308562	356601.728905	45.484583
3501.206395	356601.160312	45.489588
3500.891059	356583.088064	45.494593
3501.326474	356567.694708	45.499597
3501.516190	356564.107055	45.504602
3501.609537	356553.570491	45.509607
3501.517579	356533.455612	45.514612
3501.529820	356524.685345	45.519617
3501.660749	356504.383269	45.524621
3501.408929	356485.716518	45.529626
3501.215521	356474.919561	45.534631
3501.487071	356468.980910	45.539636
3501.753333	356453.562989	45.544641
3501.769136	356438.539855	45.549645
3501.480901	356421.200355	45.554650
3501.350937	356399.490106	45.559655
3501.442001	356391.775001	45.564660
3501.457451	356380.945511	45.569665
3501.514702	356357.147414	45.574669
3501.290294	356345.567344	45.579674
3501.236098	356335.384072	45.584679
3501.390003	356322.321833	45.589684
3501.153755	356310.006530	45.594689
3501.531886	356303.670024	45.599693
3501.219180	356294.289444	45.604698
3501.534417	356264.630882	45.609703
3501.722259	356269.151177	45.614708
3501.409602	356262.286759	45.619713
3501.584837	356244.061728	45.624717
3501.776069	356235.695598	45.629722
3501.483746	356213.451333	45.634727
3501.525113	356190.900966	45.639732
3501.468892	356183.894962	45.644737
3501.867212	356155.494169	45.649741
3501.146978	356150.218113	45.654746
3501.662003	356139.539543	45.659751
3501.688537	356112.645281	45.664756
3501.445939	356102.567499	45.669761
3501.642187	356085.914903	45.674765
3501.491862	356073.535304	45.679770
3501.478525	356052.264154	45.684775
3501.353444	356038.228564	45.689780
3501.625762	356026.393165	45.694785
3501.580278	356005.762391	45.699789
3501.458468	355994.776212	45.704794
3501.568729	355978.314853	45.709799
3502.040899	355973.996942	45.714804
3501.366692	355949.041549	45.719809
3501.566094	355943.520686	45.724813
3501.433742	355923.970856	45.729818
3501.389264	355904.814000	45.734823
3501.074358	355879.777223	45.739828
3501.141453	355815.361956	45.744833
3501.372382	355723.242617	45.749837
3500.720047	355580.427469	45.754842
3500.329126	355386.534358	45.759847
3499.985906	355160.022820	45.764852
3499.352810	354882.822313	45.769857
3499.070571	354556.153499	45.774861
3498.005692	354199.051124	45.779866
3497.002764	353796.538657	45.784871
3496.039484	353353.981121	45.789876
3494.930604	352884.369221	45.794881
3493.763872	352370.911546	45.799885
3492.234136	351830.989620	45.804890
3490.568623	351260.957156	45.809895
3489.325337	350647.812195	45.814900
3487.232916	350015.264569	45.819905
3486.182268	349333.402974	45.824909
3484.302228	348648.478583	45.829914
3482.690260	347907.873821	45.834919
3480.773379	347153.724105	45.839924
3478.830618	346373.781821	45.844929
3476.865697	345552.764699	45.849933
3474.454673	344719.008414	45.854938
3472.063299	343852.124655	45.859943
3470.064810	342971.122680	45.864948
3467.909710	342068.611588	45.869953
3465.596457	341130.248981	45.874957
3463.029507	340182.365314	45.879962
3460.504259	339201.722867	45.884967
3458.319924	338218.457618	45.889972
3455.374666	337207.081840	45.894977
3453.003226	336166.648231	45.899981
3450.168203	335131.140326	45.904986
3447.505449	334066.761808	45.909991
3444.570011	332982.964621	45.914996
3441.574525	331895.585110	45.920001
3438.659488	330787.763667	45.925005
3435.873318	329672.488832	45.930010
3433.074511	328551.206755	45.935015
3430.161256	327398.292758	45.940020
3427.111860	326240.584529	45.945025
3424.218255	325063.409571	45.950029
3420.712708	323889.959304	45.955034
3417.511017	322699.892746	45.960039
3414.680168	321503.018510	45.965044
3411.201231	320299.418682	45.970049
3408.580826	319082.803490	45.975053
3404.834898	317860.019798	45.980058
3401.205467	316626.650661	45.985063
3398.283290	315385.555243	45.990068
3394.915649	314148.312006	45.995073
3391.709460	312893.325911	46.000077
3388.190338	311640.365107	46.005082
3384.925211	310375.422640	46.010087
3381.275735	309111.575584	46.015092
3377.778363	307839.096219	46.020097
3374.546269	306563.412801	46.025101
3370.889095	305282.317137	46.030106
3367.660247	303998.679631	46.035111
3363.723260	302719.854541	46.040116
3360.293820	301436.872878	46.045121
3356.699039	300140.549660	46.050125
3353.034163	298857.365624	46.055130
3349.561378	297563.075600	46.060135
3345.971676	296259.687369	46.065140
3342.283874	294978.404713	46.070145
3338.865415	293684.834050	46.075149
3335.446512	292385.329997	46.080154
3332.110081	291089.171167	46.085159
3327.938198	289782.652922	46.090164
3324.284050	288482.798850	46.095169
3320.966319	287167.999394	46.100173
3317.005853	285879.139097	46.105178
3313.563679	284575.713376	46.110183
3309.846694	283271.516727	46.115188
3306.274848	281973.383750	46.120193
3302.306687	280659.682464	46.125197
3298.812505	279364.215505	46.130202
3295.050974	278062.683051	46.135207
3291.230002	276766.103039	46.140212
3287.654853	275466.688487	46.145217
3284.288151	274165.133084	46.150221
3280.665939	272866.092658	46.155226
3276.761391	271572.729388	46.160231
3272.880368	270264.727990	46.165236
3268.951597	268967.053463	46.170241
3265.315322	267687.241978	46.175245
3261.335377	266389.515094	46.180250
3257.701446	265098.389247	46.185255
3254.129486	263809.758697	46.190260
3250.098220	262533.356356	46.195265
3246.766953	261246.109594	46.200269
3242.750097	259969.115831	46.205274
3238.895766	258690.325989	46.210279
3235.313600	257414.230936	46.215284
3231.385413	256149.407703	46.220289
3227.859884	254877.048247	46.225293
3224.282761	253611.383014	46.230298
3220.307312	252343.222159	46.235303
3216.833922	251077.646755	46.240308
3212.986949	249811.482880	46.245313
3208.962282	248542.179255	46.250317
3205.149769	247291.042985	46.255322
3201.518655	246039.462753	46.260327
3197.800574	244779.152776	46.265332
3193.993929	243542.916527	46.270337
3190.195538	242294.702281	46.275341
3186.349615	241058.153626	46.280346
3182.706006	239821.083861	46.285351
3179.072085	238565.669960	46.290356
3175.020291	237345.310077	46.295361
3171.613270	236103.884863	46.300365
3167.867143	234884.488101	46.305370
3164.230398	233658.016118	46.310375
3160.791917	232422.519841	46.315380
3156.872536	231198.480542	46.320385
3153.073394	229972.637706	46.325389
3149.167624	228753.075296	46.330394
3145.780960	227526.859997	46.335399
3141.886484	226311.165388	46.340404
3137.913560	225101.111449	46.345409
3133.927121	223889.557174	46.350413
3130.210071	222676.382567	46.355418
3126.327496	221488.092584	46.360423
3122.632043	220286.021709	46.365428
3118.936878	219099.208612	46.370433
3115.431381	217909.159216	46.375437
3111.554609	216714.305770	46.380442
3107.851611	215521.898909	46.385447
3104.324689	214335.147719	46.390452
3100.414213	213163.843172	46.395457
3096.985314	211969.317063	46.400461
3093.212187	210791.658460	46.405466
3089.558475	209625.930966	46.410471
3085.497087	208445.653565	46.415476
3081.677428	207278.052983	46.420481
3078.184720	206113.616638	46.425485
3074.393407	204954.912579	46.430490
3070.390588	203799.177038	46.435495
3066.990461	202633.626337	46.440500
3062.851193	201491.016987	46.445505
3059.364230	200338.509064	46.450509
3055.586394	199186.767739	46.455514
3051.886726	198047.628880	46.460519
3048.101538	196905.710817	46.465524
3044.062765	195777.032951	46.470529
3040.461944	194640.783793	46.475533
3036.895137	193521.041034	46.480538
3033.018770	192398.631520	46.485543
3029.214600	191277.265136	46.490548
3025.573710	190158.303143	46.495553
3021.789018	189043.550676	46.500557
3017.713713	187946.577974	46.505562
3014.197438	186842.424861	46.510567
3010.242169	185738.835493	46.515572
3006.559579	184641.479719	46.520577
3003.219029	183543.802740	46.525581
2999.127850	182460.336187	46.530586
2995.596205	181372.924641	46.535591
2991.713762	180281.964839	46.540596
2987.564323	179208.603376	46.545601
2983.828778	178137.278522	46.550605
2979.821162	177073.711549	46.555610
2975.909299	176005.789268	46.560615
2972.422228	174957.165159	46.565620
2968.380174	173906.489664	46.570625
2964.561025	172861.483889	46.575629
2960.763419	171824.865251	46.580634
2957.087677	170791.627977	46.585639
2953.563749	169762.722262	46.590644
2949.237189	168743.744931	46.595649
2945.235024	167720.454581	46.600653
2941.339804	166711.253592	46.605658
2937.360504	165711.283429	46.610663
2933.924413	164705.744630	46.615668
2929.538982	163721.154390	46.620673
2925.909402	162736.906756	46.625677
2922.097638	161763.355895	46.630682
2918.364576	160790.787702	46.635687
2914.417669	159821.844345	46.640692
2909.891681	158879.415971	46.645697
2906.093313	157921.501537	46.650701
2902.476487	156984.013933	46.655706
2898.279107	156053.427687	46.660711
2894.527863	155128.679301	46.665716
2890.272844	154212.919981	46.670721
2886.704150	153309.336773	46.675725
2882.598274	152415.523537	46.680730
2878.445882	151522.800884	46.685735
2874.846677	150630.312067	46.690740
2870.322532	149768.777655	46.695745
2866.315787	148897.339876	46.700749
2862.690253	148053.661483	46.705754
2858.495020	147200.617966	46.710759
2854.331207	146377.919297	46.715764
2850.088067	145563.720677	46.720769
2845.879673	144760.179939	46.725773
2841.502083	143964.134689	46.730778
2837.144211	143177.527503	46.735783
2832.747940	142413.179871	46.740788
2828.894238	141663.111877	46.745793
2824.932809	140923.594440	46.750797
2820.605158	140202.453957	46.755802
2816.369794	139478.536432	46.760807
2812.079603	138782.793967	46.765812
2808.016659	138031.556154	46.770817
2803.861135	137319.695099	46.775821
2799.737795	136654.861126	46.780826
2795.826141	135998.629380	46.785831
2791.690602	135352.466739	46.790836
2787.485998	134729.070367	46.795841
2783.911614	134095.547388	46.800845
2779.810315	133484.810172	46.805850
2775.515003	132885.255275	46.810855
2772.266510	132283.205023	46.815860
2767.976228	131698.256522	46.820865
2764.378500	131122.595936	46.825869
2761.023879	130540.354210	46.830874
2756.996285	129974.303512	46.835879
2753.689956	129406.926984	46.840884
2750.005414	128848.228300	46.845889
2745.985432	128278.713881	46.850893
2742.602574	127724.078994	46.855898
2738.410723	127178.989755	46.860903
2735.281986	126627.955027	46.865908
2731.476299	126094.267351	46.870913
2728.263271	125551.374979	46.875917
2724.777498	125015.616630	46.880922
2721.172795	124473.804429	46.885927
2717.756215	123923.245454	46.890932
2714.039842	123404.434469	46.895937
2710.530982	122855.456223	46.900941
2707.083329	122333.565104	46.905946
2703.240579	121795.247550	46.910951
2700.339392	121257.490337	46.915956
2696.573564	120736.674707	46.920961
2692.987962	120207.241227	46.925965
2689.104193	119673.385038	46.930970
2685.721424	119143.209775	46.935975
2682.401844	118614.418157	46.940980
2678.702597	118094.874272	46.945985
2674.937297	117579.073682	46.950989
2671.675543	117052.227800	46.955994
2667.869399	116545.463504	46.960999
2664.672967	116018.456736	46.966004
2661.012365	115494.377984	46.971009
2657.698004	114970.786842	46.976013
2654.128374	114450.828583	46.981018
2650.637213	113938.151227	46.986023
2646.803922	113421.414727	46.991028
2642.919969	112900.243351	46.996033
2639.536083	112382.650753	47.001037
2635.870112	111876.361685	47.006042
2632.068542	111361.887571	47.011047
2628.565732	110850.756321	47.016052
2624.871027	110350.278309	47.021057
2621.442435	109855.906656	47.026061
2617.922359	109359.738191	47.031066
2614.162464	108862.457191	47.036071
2610.542737	108371.429022	47.041076
2606.522930	107884.754312	47.046081
2602.904521	107399.193574	47.051085
2599.370467	106921.254080	47.056090
2595.152838	106443.592905	47.061095
2591.735294	105968.127533	47.066100
2587.836589	105512.561681	47.071105
2584.040663	105042.532649	47.076109
2580.256341	104582.423449	47.081114
2576.549651	104129.922647	47.086119
2572.715032	103686.523746	47.091124
2568.827295	103252.748631	47.096129
2565.095512	102805.316064	47.101133
2561.589975	102372.408198	47.106138
2557.840747	101938.018674	47.111143
2554.207400	101503.705843	47.116148
2550.458316	101098.383544	47.121153
2547.095472	100679.126715	47.126157
2543.449621	100244.629253	47.131162
2539.704341	99831.683494	47.136167
2536.365542	99410.265986	47.141172
2532.590525	99002.406637	47.146177
2529.583198	98585.955902	47.151181
2525.735080	98176.631472	47.156186
2522.074519	97769.329266	47.161191
2518.729210	97359.377923	47.166196
2515.245991	96945.996602	47.171201
2511.946133	96533.875725	47.176205
2508.619915	96113.859783	47.181210
2504.840631	95709.983080	47.186215
2501.461163	95294.777401	47.191220
2497.840411	94886.858266	47.196225
2494.590935	94477.806566	47.201229
2490.803610	94064.536144	47.206234
2487.345465	93655.807375	47.211239
2484.114988	93235.574067	47.216244
2480.550389	92830.939139	47.221249
2477.304829	92414.645911	47.226253
2474.134302	91995.424177	47.231258
2470.486637	91581.644607	47.236263
2466.891872	91172.360488	47.241268
2463.473357	90749.420852	47.246273
2460.107528	90337.024880	47.251277
2456.676171	89908.356019	47.256282
2453.001005	89489.095250	47.261287
2449.823965	89061.161321	47.266292
2446.572782	88641.986274	47.271297
2443.038909	88214.158221	47.276301
2439.366244	87791.719412	47.281306
2435.753474	87372.783834	47.286311
2432.404898	86941.172183	47.291316
2428.597757	86509.282551	47.296321
2425.018997	86083.004396	47.301325
2421.679731	85650.927654	47.306330
2418.121954	85234.542344	47.311335
2414.999531	84796.969315	47.316340
2411.528764	84382.843996	47.321345
2408.076827	83953.731999	47.326349
2404.544755	83522.428595	47.331354
2400.925123	83087.753703	47.336359
2397.570874	82659.179500	47.341364
2394.007484	82231.076207	47.346369
2390.123366	81793.832929	47.351373
2387.064055	81369.258985	47.356378
2383.768929	80936.510090	47.361383
2380.713186	80493.302613	47.366388
2377.000435	80067.173492	47.371393
2373.102806	79630.334445	47.376397
2369.790613	79196.662626	47.381402
2366.089790	78744.502211	47.386407
2362.855470	78307.479222	47.391412
2359.423072	77865.769456	47.396417
2355.843973	77425.004052	47.401421
2352.685866	76976.344349	47.406426
2348.781104	76544.800533	47.411431
2345.425624	76098.433884	47.416436
2341.829551	75663.541462	47.421441
2338.079089	75223.333724	47.426445
2334.754953	74780.971509	47.431450
2331.090452	74341.183904	47.436455
2327.919918	73899.142503	47.441460
2324.296615	73452.632886	47.446465
2321.020499	73016.997106	47.451469
2317.704061	72568.511777	47.456474
2313.351995	72127.280533	47.461479
2309.997867	71676.441750	47.466484
2306.463188	71238.843941	47.471489
2303.233108	70794.959084	47.476493
2299.798033	70347.774398	47.481498
2296.507255	69918.051815	47.486503
2293.173513	69457.808178	47.491508
2289.621055	69019.571129	47.496513
2286.030625	68562.081304	47.501517
2282.462699	68113.451371	47.506522
2278.990851	67665.182489	47.511527
2275.567130	67210.909088	47.516532
2272.431145	66760.578887	47.521537
2269.037851	66319.348109	47.526541
2265.181528	65861.522676	47.531546
2261.778618	65403.393763	47.536551
2258.435547	64947.885190	47.541556
2254.495607	64500.030631	47.546561
2251.327931	64031.043114	47.551565
2247.854191	63583.379902	47.556570
2244.173203	63126.655921	47.561575
2240.532767	62660.883902	47.566580
2236.787056	62211.732791	47.571585
2233.504517	61765.576648	47.576589
2229.976641	61304.255025	47.581594
2226.610894	60862.748168	47.586599
2223.450460	60388.459673	47.591604
2219.421367	59940.612522	47.596609
2215.875659	59472.170095	47.601613
2212.426511	59020.816580	47.606618
2208.641698	58572.157055	47.611623
2205.437007	58111.632302	47.616628
2202.184520	57668.845916	47.621633
2198.563359	57200.808169	47.626637
2195.232764	56734.307874	47.631642
2191.719935	56278.117316	47.636647
2188.426011	55821.241556	47.641652
2184.519424	55355.949124	47.646657
2181.402627	54898.898561	47.651661
2178.181981	54435.281205	47.656666
2174.554788	53971.577615	47.661671
2170.894593	53506.029472	47.666676
2167.365777	53035.096773	47.671681
2163.926456	52573.681719	47.676685
2160.484533	52098.542044	47.681690
2156.667849	51635.180642	47.686695
2153.493151	51166.698210	47.691700
2149.707048	50711.742892	47.696705
2146.134243	50246.455629	47.701709
2142.593625	49782.314507	47.706714
2139.267846	49314.686074	47.711719
2135.781557	48844.764347	47.716724
2132.276963	48385.605990	47.721729
2128.743591	47926.118862	47.726733
2125.321604	47452.245390	47.731738
2121.482507	46980.596775	47.736743
2118.105910	46511.892208	47.741748
2114.419641	46051.788299	47.746753
2111.095521	45597.440288	47.751757
2107.984773	45124.277579	47.756762
2103.989773	44657.350467	47.761767
2101.524900	44185.755934	47.766772
2097.466913	43708.718429	47.771777
2093.865088	43245.475793	47.776781
2090.221734	42763.270382	47.781786
2086.827260	42294.669847	47.786791
2083.736953	41823.001025	47.791796
2080.236592	41359.940724	47.796801
2076.523061	40876.221450	47.801805
2073.022801	40392.454330	47.806810
2069.276897	39929.621065	47.811815
2065.763992	39449.345009	47.816820
2062.002933	38976.428239	47.821825
2058.626188	38505.433699	47.826829
2055.367525	38044.663391	47.831834
2052.105978	37582.419932	47.836839
2048.144379	37096.097675	47.841844
2044.993890	36629.248705	47.846849
2041.301041	36156.212228	47.851853
2037.676047	35678.307321	47.856858
2033.948331	35208.219649	47.861863
2030.839336	34738.927200	47.866868
2027.271170	34271.973176	47.871873
2023.552252	33789.035648	47.876877
2020.144356	33312.519555	47.881882
2016.407327	32838.397959	47.886887
2013.007661	32372.512080	47.891892
2009.298732	31905.220676	47.896897
2006.025807	31437.510653	47.901901
2002.731085	30964.617713	47.906906
1998.860950	30496.939454	47.911911
1995.260493	30029.172774	47.916916
1991.768709	29564.422628	47.921921
1988.542371	29091.561953	47.926925
1985.329506	28623.019162	47.931930
1981.586354	28150.868967	47.936935
1978.223630	27675.983769	47.941940
1974.733936	27197.752077	47.946945
1970.965751	26731.107049	47.951949
1967.580520	26254.471742	47.956954
1963.835244	25796.373163	47.961959
1960.543138	25313.276512	47.966964
1957.028364	24855.163464	47.971969
1953.308518	24378.643621	47.976973
1949.808898	23912.991419	47.981978
1946.227024	23445.443287	47.986983
1942.716468	22970.787023	47.991988
1939.094560	22508.753335	47.996993
1935.804756	22039.678746	48.001997
1932.263482	21568.899708	48.007002
1928.461450	21100.744294	48.012007
1925.024548	20636.464156	48.017012
1921.452462	20169.333957	48.022017
1918.028685	19706.746002	48.027021
1914.509503	19235.715388	48.032026
1910.543474	18784.033005	48.037031
1906.904982	18314.480990	48.042036
1903.565458	17864.698545	48.047041
1899.716054	17415.924226	48.052045
1896.371513	16953.516090	48.057050
1892.508755	16511.854845	48.062055
1889.396467	16048.776799	48.067060
1885.408216	15608.017118	48.072065
1881.865755	15158.414904	48.077069
1878.212951	14714.726429	48.082074
1873.777052	14283.315480	48.087079
1870.272178	13839.409062	48.092084
1866.594803	13408.564780	48.097089
1862.664091	12996.819116	48.102093
1858.564718	12584.013276	48.107098
1854.114546	12189.423726	48.112103
1850.331153	11798.743318	48.117108
1846.153187	11419.576316	48.122113
1842.272415	11045.850381	48.127117
1838.196237	10673.140466	48.132122
1834.360162	10319.289025	48.137127
1830.635857	9963.394697	48.142132
1826.840518	9611.379960	48.147137
1822.889508	9269.984047	48.152141
1818.810492	8932.741812	48.157146
1814.787194	8622.132113	48.162151
1810.906865	8304.564229	48.167156
1806.732320	8015.381443	48.172161
1802.771340	7717.231885	48.177165
1799.268980	7423.538540	48.182170
1795.015262	7149.269779	48.187175
1791.270482	6887.297474	48.192180
1787.877034	6617.374766	48.197185
1784.244842	6356.547691	48.202189
1780.204864	6101.917939	48.207194
1776.609871	5852.121458	48.212199
1773.001858	5604.295684	48.217204
1769.083849	5368.094583	48.222209
1765.347783	5136.368279	48.227213
1762.381817	4890.974464	48.232218
1758.428768	4664.348064	48.237223
1754.863981	4444.831594	48.242228
1751.240991	4226.038839	48.247233
1747.964319	3999.669896	48.252237
1744.607000	3781.303170	48.257242
1741.090891	3561.299365	48.262247
1737.564089	3330.398967	48.267252
1733.870196	3124.426928	48.272257
1730.763456	2904.886352	48.277261
1726.758673	2685.355330	48.282266
1723.314214	2477.810924	48.287271
1719.977557	2276.868255	48.292276
1716.732976	2052.183093	48.297281
1712.632679	1857.049787	48.302285
1709.609384	1639.365810	48.307290
1705.581685	1439.745563	48.312295
1702.291488	1239.376816	48.317300
1698.427243	1041.918675	48.322305
1695.013327	849.891386	48.327309
1691.317131	654.452061	48.332314
1687.255215	475.200717	48.337319
1683.297723	293.328007	48.342324
1678.868396	136.027218	48.347329
1672.739903	31.215330	48.352333
1662.134708	64.063241	48.357338
1655.310998	66.985625	48.362343
1651.127684	65.906251	48.367348
1648.333723	68.261546	48.372353
1645.885255	57.373601	48.377357
1643.876122	64.947069	48.382362
1640.767717	71.422988	48.387367
1638.095427	63.939219	48.392372
1634.874387	64.367856	48.397377
1631.266169	64.888391	48.402381
1627.933970	58.522884	48.407386
1624.779735	59.969325	48.412391
1621.491167	60.696369	48.417396
1618.197222	65.805975	48.422401
1614.134802	70.165172	48.427405
1610.807895	64.567621	48.432410
1607.807684	57.748655	48.437415
1604.690423	64.456902	48.442420
1601.384695	65.601063	48.447425
1597.545700	59.469461	48.452429
1594.331001	58.416503	48.457434
1590.622280	67.054917	48.462439
1587.088188	64.229380	48.467444
1583.689709	61.025239	48.472449
1580.436961	66.985796	48.477453
1577.146808	61.075651	48.482458
1573.238585	64.778111	48.487463
1570.357283	66.476300	48.492468
1566.881475	64.350363	48.497473
1563.079274	63.202191	48.502477
1559.668714	67.684555	48.507482
1556.352677	64.559332	48.512487
1552.847225	65.639672	48.517492
1549.944126	62.288830	48.522497
1545.746950	63.429379	48.527501
1542.175684	51.450734	48.532506
1538.849817	62.076469	48.537511
1535.598857	65.448845	48.542516
1532.161220	59.384495	48.547521
1528.672642	65.097027	48.552525
1525.740579	59.494980	48.557530
1522.041700	67.758548	48.562535
1518.229414	63.407126	48.567540
1515.027940	55.651409	48.572545
1510.947861	62.284894	48.577549
1508.074576	52.288821	48.582554
1504.564388	58.017370	48.587559
1500.912250	52.546388	48.592564
1497.239500	63.396953	48.597569
1493.520028	63.378007	48.602573
1490.811198	53.827730	48.607578
1486.798570	52.544644	48.612583
1483.863067	51.568462	48.617588
1480.515858	61.020623	48.622593
1476.771697	63.084069	48.627597
1473.234456	52.786392	48.632602
1469.449553	51.154658	48.637607
1465.879348	55.253757	48.642612
1462.787177	54.494947	48.647617
1458.904345	57.513267	48.652621
1455.897283	53.311767	48.657626
1452.157381	60.271950	48.662631
1448.453073	61.335795	48.667636
1445.280847	55.521210	48.672641
1441.599784	62.987918	48.677645
1438.478091	49.518822	48.682650
1434.682051	53.327213	48.687655
1431.318457	39.772393	48.692660
1428.079226	51.577348	48.697665
1424.185764	55.603380	48.702669
1420.845492	42.778907	48.707674
1416.998506	52.062087	48.712679
1413.757723	50.598764	48.717684
1411.124140	44.532672	48.722689
1406.661786	55.401732	48.727693
1403.592719	50.779628	48.732698
1399.472127	52.721341	48.737703
1395.934676	44.230184	48.742708
1392.814029	47.756286	48.747713
1389.674251	47.365554	48.752717
1385.938589	45.681875	48.757722
1382.531208	52.296079	48.762727
1379.148504	45.470248	48.767732
1375.759286	45.747917	48.772737
1371.256258	46.774743	48.777741
1368.262469	41.903652	48.782746
1364.969089	47.117578	48.787751
1361.499575	43.266477	48.792756
1358.185485	36.205352	48.797761
1354.303884	40.742058	48.802765
1350.918726	48.390492	48.807770
1347.312037	45.503524	48.812775
1343.850523	62.911177	48.817780
1340.355961	52.518298	48.822785
1336.643583	51.359337	48.827789
1333.680648	56.955259	48.832794
1329.855366	59.325568	48.837799
1326.546093	55.737423	48.842804
1323.329041	53.245380	48.847809
1319.372482	53.788528	48.852813
1315.956557	56.000210	48.857818
1312.012194	54.861542	48.862823
1308.574569	54.580452	48.867828
1305.736539	48.773980	48.872833
1302.207709	53.467750	48.877837
1298.591726	46.751008	48.882842
1295.292126	54.158343	48.887847
1291.538351	49.051220	48.892852
1288.412371	52.647761	48.897857
1284.573933	59.322739	48.902861
1280.905147	56.230312	48.907866
1277.338718	57.225258	48.912871
1273.862458	58.218824	48.917876
1270.568689	55.627999	48.922881
1266.923458	58.527097	48.927885
1263.832437	50.732085	48.932890
1260.075099	53.917547	48.937895
1256.152899	51.149301	48.942900
1253.329047	47.767178	48.947905
1249.225709	55.347075	48.952909
1246.184022	49.863371	48.957914
1242.466680	66.390210	48.962919
1238.996171	54.060592	48.967924
1235.891281	40.804060	48.972929
1231.968541	46.948005	48.977933
1228.628557	45.911423	48.982938
1225.134836	60.223669	48.987943
1221.316504	51.494692	48.992948
1218.038945	47.933263	48.997953
1214.519304	51.524646	49.002957
1211.255860	56.588394	49.007962
1207.561297	58.574543	49.012967
1204.180800	41.105759	49.017972
1200.440230	56.067016	49.022977
1196.593931	53.353401	49.027981
1193.753586	43.681283	49.032986
1190.245649	44.964519	49.037991
1186.702721	48.262142	49.042996
1182.928432	46.413663	49.048001
1179.344736	45.320111	49.053005
1175.776718	42.300599	49.058010
1172.514174	50.262142	49.063015
1168.943463	47.698620	49.068020
1165.867442	46.943653	49.073025
1161.744372	57.462527	49.078029
1158.637437	54.985000	49.083034
1155.007201	48.302137	49.088039
1151.535141	53.717891	49.093044
1147.999320	41.145374	49.098049
1144.609131	47.215921	49.103053
1141.417190	40.354111	49.108058
1137.399181	45.535313	49.113063
1134.163728	50.531433	49.118068
1130.989310	41.699085	49.123073
1127.017179	52.472867	49.128077
1123.403616	48.049448	49.133082
1119.969955	41.943422	49.138087
1116.388024	51.191681	49.143092
1113.245095	42.405054	49.148097
1109.390826	47.756920	49.153101
1106.110327	48.546028	49.158106
1102.245490	49.460894	49.163111
1098.542413	37.578798	49.168116
1095.622568	42.788377	49.173121
1092.335820	53.078997	49.178125
1089.022533	43.758918	49.183130
1085.311680	44.039227	49.188135
1081.167606	47.743636	49.193140
1077.860964	44.025407	49.198145
1074.066169	60.994553	49.203149
1071.212990	53.317570	49.208154
1067.544350	54.673289	49.213159
1063.961023	47.473787	49.218164
1060.792464	39.909176	49.223169
1057.057338	51.879904	49.228173
1053.753418	40.495655	49.233178
1049.828796	48.873464	49.238183
1046.538748	53.049204	49.243188
1043.290756	51.163111	49.248193
1039.824512	56.982920	49.253197
1036.295524	47.598351	49.258202
1032.217403	51.893599	49.263207
1028.722385	52.776217	49.268212
1025.496307	43.379302	49.273217
1021.728095	50.065508	49.278221
1018.777137	49.550511	49.283226
1015.047071	51.241656	49.288231
1011.249878	51.696760	49.293236
1008.002838	48.190720	49.298241
1004.312577	51.185433	49.303245
1000.927616	46.046258	49.308250
997.355577	49.221882	49.313255
993.825962	46.892426	49.318260
990.879106	40.716973	49.323265
986.975174	51.935713	49.328269
983.487341	51.219559	49.333274
980.079090	47.302029	49.338279
975.980261	42.349909	49.343284
972.959697	47.224005	49.348289
969.063722	51.405487	49.353293
965.890055	42.424359	49.358298
962.601381	46.175956	49.363303
959.138831	46.968108	49.368308
955.720861	40.505335	49.373313
951.910253	48.090301	49.378317
948.484551	43.134643	49.383322
945.153836	41.584136	49.388327
941.404552	45.717475	49.393332
937.709038	41.446046	49.398337
934.455637	42.291063	49.403341
930.785800	45.456606	49.408346
927.401887	49.751366	49.413351
923.710550	43.239404	49.418356
920.669490	41.191406	49.423361
916.897406	49.668861	49.428365
913.491743	44.570887	49.433370
909.770060	50.636104	49.438375
906.479508	47.943589	49.443380
902.938965	41.851073	49.448385
899.312246	42.991482	49.453389
896.019330	44.079929	49.458394
892.230093	42.183199	49.463399
888.650984	40.149359	49.468404
885.577692	41.241584	49.473409
881.812273	57.940402	49.478413
878.566606	45.142446	49.483418
875.164990	48.320024	49.488423
870.791245	44.195310	49.493428
867.889628	42.821619	49.498433
864.187552	44.075000	49.503437
861.066396	47.000119	49.508442
857.712237	50.081729	49.513447
853.877479	55.500182	49.518452
850.699815	50.012393	49.523457
846.681424	55.566996	49.528461
843.206552	51.042940	49.533466
840.018291	48.160508	49.538471
836.429167	44.802653	49.543476
832.868971	45.882095	49.548481
829.220187	49.398703	49.553485
826.031439	43.207146	49.558490
822.696001	48.744020	49.563495
818.751953	40.952165	49.568500
815.477425	45.568418	49.573505
811.385738	52.463177	49.578509
807.896270	48.042636	49.583514
804.708555	49.718979	49.588519
801.271498	47.378307	49.593524
797.845584	41.581169	49.598529
794.550274	46.947286	49.603533
791.227835	47.758774	49.608538
787.626654	43.615049	49.613543
783.398578	54.134466	49.618548
780.536433	41.957023	49.623553
776.807610	55.878763	49.628557
773.133573	42.938714	49.633562
769.972750	42.908818	49.638567
766.486226	47.390402	49.643572
763.136112	46.222578	49.648577
759.180680	46.151868	49.653581
755.634409	43.008813	49.658586
752.081387	42.527457	49.663591
748.503512	42.002516	49.668596
745.163604	45.970909	49.673601
741.659566	45.073815	49.678605
738.284298	35.719167	49.683610
734.924153	33.853738	49.688615
731.325708	37.466918	49.693620
727.898260	38.449779	49.698625
724.499308	45.331615	49.703629
720.869376	33.618551	49.708634
717.553216	33.802663	49.713639
714.062151	44.912846	49.718644
710.428622	39.486557	49.723649
706.787633	37.294701	49.728653
702.834853	41.912146	49.733658
699.528063	32.989760	49.738663
695.932655	36.330395	49.743668
692.711776	39.587418	49.748673
689.033570	46.927169	49.753677
685.879156	37.626732	49.758682
682.475847	41.769510	49.763687
678.480975	41.277856	49.768692
675.264899	33.350564	49.773697
671.582897	50.219879	49.778701
668.199002	39.455588	49.783706
664.646151	38.553450	49.788711
661.040759	41.212291	49.793716
657.785444	37.331115	49.798721
654.138431	45.260781	49.803725
650.927960	39.812935	49.808730
647.409691	40.423977	49.813735
643.054162	45.167398	49.818740
640.097819	43.669379	49.823745
636.745364	50.610421	49.828749
633.133633	50.422950	49.833754
629.895445	45.871575	49.838759
626.175256	44.976510	49.843764
622.866664	41.587673	49.848769
619.108902	48.209007	49.853773
615.769359	49.807767	49.858778
612.140456	51.432591	49.863783
608.275041	43.884795	49.868788
604.965788	41.559056	49.873793
601.618114	44.861136	49.878797
598.378114	43.252261	49.883802
594.753843	51.507415	49.888807
591.108819	49.629406	49.893812
587.928855	41.506685	49.898817
583.934385	39.964645	49.903821
580.556609	50.054317	49.908826
577.582783	51.244981	49.913831
573.432509	53.052212	49.918836
569.864928	47.441677	49.923841
566.227796	48.745094	49.928845
562.738469	44.764322	49.933850
559.836627	44.077219	49.938855
556.695455	41.219134	49.943860
553.209418	36.152716	49.948865
549.301278	39.269977	49.953869
545.759641	38.277527	49.958874
542.047278	41.883152	49.963879
538.486795	42.548233	49.968884
535.219747	38.488573	49.973889
531.094465	51.807664	49.978893
527.926137	47.704161	49.983898
524.345059	41.966027	49.988903
521.198083	43.050778	49.993908
517.939895	47.832186	49.998913
514.260468	52.761429	50.003917
510.487884	52.380723	50.008922
507.022440	45.349632	50.013927
503.025949	52.004978	50.018932
500.145885	39.805075	50.023937
496.380495	56.285590	50.028941
493.093578	40.548774	50.033946
489.593006	39.546775	50.038951
485.846370	53.493437	50.043956
482.363117	39.799282	50.048961
478.939925	49.959301	50.053965
475.814136	51.996186	50.058970
472.494769	47.103143	50.063975
468.800950	52.037794	50.068980
465.248152	44.934892	50.073985
461.270876	47.281502	50.078989
458.074879	54.191872	50.083994
454.289822	51.082873	50.088999
450.684502	58.316389	50.094004
447.428339	46.152899	50.099009
444.015846	48.158493	50.104013
440.550883	46.818772	50.109018
437.139076	43.613706	50.114023
433.496312	53.599110	50.119028
430.200166	34.829799	50.124033
426.415632	46.782923	50.129037
422.736669	36.839722	50.134042
419.666764	46.315173	50.139047
415.800675	38.058865	50.144052
412.481873	35.367657	50.149057
408.914196	43.332443	50.154061
405.633283	40.429699	50.159066
402.021881	28.571465	50.164071
398.030404	50.095246	50.169076
394.912114	38.865736	50.174081
391.702758	44.405157	50.179085
388.135978	41.464664	50.184090
384.698724	44.635183	50.189095
380.594141	40.497135	50.194100
377.402098	35.916475	50.199105
373.822961	41.048407	50.204109
370.166705	50.770167	50.209114
367.147699	44.001786	50.214119
363.392591	42.678774	50.219124
360.169399	29.722431	50.224129
356.843758	40.673997	50.229133
352.972103	38.752219	50.234138
349.513225	31.697996	50.239143
345.612884	40.666837	50.244148
342.453877	38.532876	50.249153
339.060265	39.494698	50.254157
335.341810	39.754142	50.259162
331.836145	40.442353	50.264167
328.032286	45.520695	50.269172
324.890643	45.914959	50.274177
321.287455	46.589882	50.279181
317.775125	44.384384	50.284186
314.628381	32.574047	50.289191
310.562177	44.950666	50.294196
307.249828	38.737316	50.299201
304.187798	49.185954	50.304205
300.416757	42.907978	50.309210
296.996218	42.133985	50.314215
292.912765	47.489970	50.319220
289.827044	43.139535	50.324225
286.267292	45.114291	50.329229
282.688071	39.613189	50.334234
279.439396	38.698551	50.339239
275.809275	46.239648	50.344244
272.425022	35.317321	50.349249
268.741777	43.205200	50.354253
265.054046	33.611405	50.359258
262.227526	37.832097	50.364263
258.140230	44.403529	50.369268
255.133046	35.494697	50.374273
251.452365	35.909620	50.379277
247.933838	43.268834	50.384282
244.214062	28.219564	50.389287
240.471143	41.801824	50.394292
237.120506	41.010630	50.399297
233.895006	34.729991	50.404301
230.634623	34.209476	50.409306
227.021531	36.325417	50.414311
223.091787	44.909718	50.419316
220.149626	29.264838	50.424321
216.246922	34.864763	50.429325
212.805167	34.470561	50.434330
209.154308	32.169594	50.439335
205.599989	38.037974	50.444340
202.030663	35.243438	50.449345
198.378063	37.046005	50.454349
194.983690	41.788532	50.459354
191.997270	34.268490	50.464359
188.178656	44.758995	50.469364
185.127138	31.086288	50.474369
181.372713	37.808375	50.479373
177.794391	39.539271	50.484378
174.172142	34.721913	50.489383
170.621259	33.718304	50.494388
167.002304	39.087402	50.499393
163.707133	34.304542	50.504397
160.345902	40.215629	50.509402
156.883580	35.794141	50.514407
153.151789	51.718947	50.519412
149.711928	29.640769	50.524417
146.216946	46.123467	50.529421
142.447187	37.662404	50.534426
139.760089	33.677027	50.539431
135.942294	38.811340	50.544436
132.170201	44.207450	50.549441
128.556517	36.405440	50.554445
124.823392	34.234351	50.559450
121.627460	30.654055	50.564455
117.892129	38.521581	50.569460
114.842621	30.774103	50.574465
111.331506	41.355936	50.579469
107.387271	30.916293	50.584474
104.601620	30.226973	50.589479
100.312962	48.908600	50.594484
97.288343	36.297875	50.599489
93.454033	34.791094	50.604493
89.892134	37.797560	50.609498
86.419678	31.324454	50.614503
82.979677	39.345312	50.619508
79.954440	27.873609	50.624513
76.369989	27.634517	50.629517
72.687481	34.671272	50.634522
69.493469	29.413951	50.639527
65.638731	36.664178	50.644532
61.980033	30.555421	50.649537
58.695931	37.871823	50.654541
55.259622	30.073853	50.659546
51.367788	33.251911	50.664551
47.761138	38.416633	50.669556
44.671861	37.031135	50.674561
41.131489	28.784314	50.679565
37.547726	40.829577	50.684570
34.232594	28.998071	50.689575
30.312925	30.219003	50.694580
26.956032	33.187230	50.699585
23.704303	37.360254	50.704589
20.527887	32.388093	50.709594
17.034938	32.786476	50.714599
12.830172	39.448987	50.719604
9.417360	28.284409	50.724609
5.606671	32.737444	50.729613
2.281888	40.458805	50.734618