Fri Aug 26 11:34:52 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.338657	106.695839	0.000000
0.753910	102.600747	0.005005
0.524354	92.620405	0.010010
0.396767	95.263012	0.015014
0.320059	87.182381	0.020019
-0.048702	94.285334	0.025024
-0.052814	76.177258	0.030029
-0.333964	75.781352	0.035034
-1.279887	67.668389	0.040038
-0.703668	57.581592	0.045043
-1.236416	60.008875	0.050048
-1.508088	52.869747	0.055053
-1.761590	37.236553	0.060058
-1.991984	41.575057	0.065062
-1.820059	33.607594	0.070067
-2.306685	24.977066	0.075072
-2.474381	18.305801	0.080077
-2.906108	15.120859	0.085082
-3.210170	-0.061519	0.090086
-3.562963	-4.318569	0.095091
-4.214978	2.967650	0.100096
-4.469319	-0.055090	0.105101
-4.233567	9.756698	0.110106
-4.375535	-5.099749	0.115110
-4.777771	-4.926327	0.120115
-5.443525	1.571120	0.125120
-5.384724	-11.703122	0.130125
-5.987742	-7.293958	0.135130
-6.806522	-13.674020	0.140134
-6.345339	-8.772512	0.145139
-6.589669	-6.750799	0.150144
-7.088024	-4.322553	0.155149
-6.634127	-8.841237	0.160154
-7.188589	-11.361682	0.165158
-8.183599	-10.121565	0.170163
-8.383339	-8.600323	0.175168
-7.979032	-2.835775	0.180173
-8.511579	-3.983449	0.185178
-8.690571	-14.183567	0.190182
-8.437709	-13.754650	0.195187
-9.091794	-7.651315	0.200192
-9.528518	-17.089993	0.205197
-9.892151	-16.992182	0.210202
-9.983295	-10.755041	0.215206
-9.354389	-20.027450	0.220211
-10.135328	-14.454840	0.225216
-10.591620	-19.882136	0.230221
-10.949993	-11.664078	0.235226
-11.334371	-16.336971	0.240230
-11.343406	-20.527319	0.245235
-11.986384	-10.486983	0.250240
-12.134096	-11.058681	0.255245
-12.791423	-6.157025	0.260250
-12.798441	-2.387966	0.265254
-12.581649	-11.007777	0.270259
-13.128260	-18.486869	0.275264
-12.830700	-12.579159	0.280269
-12.920683	-10.590969	0.285274
-13.685073	-8.099156	0.290278
-13.623816	-21.579409	0.295283
-14.112072	-5.254860	0.300288
-14.249714	-1.759682	0.305293
-14.914367	0.887439	0.310298
-15.279990	0.703996	0.315302
-15.672178	-15.745921	0.320307
-16.164644	-5.343052	0.325312
-15.653210	-8.032618	0.330317
-15.695647	-4.536445	0.335322
-15.943846	-11.030654	0.340326
-15.643707	-9.862479	0.345331
-16.318050	-4.315954	0.350336
-16.662359	-7.928939	0.355341
-16.752663	-7.221974	0.360346
-17.855148	-2.330098	0.365350
-18.085254	-9.238398	0.370355
-18.402009	-5.196496	0.375360
-18.290219	-7.083546	0.380365
-18.288637	-8.520018	0.385370
-18.671761	-8.387535	0.390374
-18.453475	-13.154262	0.395379
-19.419044	-6.211519	0.400384
-19.907511	-8.925730	0.405389
-19.581669	-17.410662	0.410394
-20.255510	-7.058646	0.415398
-20.053271	-17.432009	0.420403
-20.029502	-14.408038	0.425408
-20.627435	-16.010585	0.430413
-21.143968	-5.850733	0.435418
-21.433887	-5.353125	0.440422
-20.934595	-12.273752	0.445427
-21.152088	-9.060362	0.450432
-22.065048	-14.568412	0.455437
-22.579478	-15.674614	0.460442
-22.834042	-11.778433	0.465446
-22.630515	-19.377482	0.470451
-23.148369	-9.350299	0.475456
-23.212320	-13.794681	0.480461
-23.178091	-13.274779	0.485466
-23.583174	-18.678411	0.490470
-23.977950	-20.065825	0.495475
-24.373515	-14.091325	0.500480
-24.100123	-15.997208	0.505485
-24.584227	-11.780561	0.510490
-25.324052	-20.846188	0.515494
-25.426417	-15.069194	0.520499
-25.559247	-12.188514	0.525504
-25.974408	-22.484727	0.530509
-25.729936	-20.099376	0.535514
-25.770110	-8.488819	0.540518
-25.769056	-18.293038	0.545523
-26.485987	-15.096797	0.550528
-26.672680	-20.354104	0.555533
-27.033914	-17.921899	0.560538
-28.059460	-19.011794	0.565542
-27.946377	-20.712390	0.570547
-28.452524	-16.723257	0.575552
-28.179459	-20.128654	0.580557
-28.380291	-19.379171	0.585562
-28.564793	-10.811712	0.590566
-28.621790	-10.742660	0.595571
-29.114485	-17.375963	0.600576
-29.619755	-11.279981	0.605581
-29.856048	-21.202262	0.610586
-29.879138	-14.415756	0.615590
-29.891403	-16.644145	0.620595
-30.556644	-14.424025	0.625600
-30.911747	-19.955657	0.630605
-30.755663	-13.639956	0.635610
-31.040819	-14.073200	0.640614
-31.201853	-12.172021	0.645619
-32.075488	-8.853307	0.650624
-32.714244	-9.044841	0.655629
-32.820370	-15.444114	0.660634
-32.792448	-7.450709	0.665638
-32.345862	-9.035558	0.670643
-32.587139	-8.555014	0.675648
-33.114486	-15.040558	0.680653
-33.259567	-13.559463	0.685658
-34.056633	-11.518128	0.690662
-34.035173	-17.374136	0.695667
-34.571210	-14.822969	0.700672
-34.564625	-8.490318	0.705677
-34.443747	-18.506174	0.710682
-34.644927	-18.332419	0.715686
-34.928794	-16.190661	0.720691
-35.576946	-6.567118	0.725696
-35.420194	-20.014783	0.730701
-35.820945	-19.253155	0.735706
-36.328944	-15.801553	0.740710
-36.750432	-15.966806	0.745715
-36.982571	-13.836265	0.750720
-37.158809	-15.997996	0.755725
-37.048432	-20.861810	0.760730
-37.248168	-18.217477	0.765734
-37.466901	-19.553209	0.770739
-38.581775	-9.347654	0.775744
-38.513504	-18.450519	0.780749
-38.603385	-13.216451	0.785754
-38.631722	-14.350881	0.790758
-38.741307	-8.041270	0.795763
-38.875028	-6.571434	0.800768
-39.637357	-14.633849	0.805773
-40.334792	-13.705809	0.810778
-40.436168	-6.679329	0.815782
-40.080245	-11.363084	0.820787
-40.448762	-15.086189	0.825792
-40.332153	-15.072641	0.830797
-40.847771	-11.562906	0.835802
-41.741395	-16.577273	0.840806
-42.095013	-17.540839	0.845811
-42.219290	-6.043734	0.850816
-42.034688	-11.811253	0.855821
-41.848978	-14.013521	0.860826
-41.858782	-12.594616	0.865830
-42.496213	-18.797272	0.870835
-43.257983	-15.527613	0.875840
-43.371655	-17.101158	0.880845
-43.244631	-18.860869	0.885850
-43.604575	-18.516867	0.890854
-43.764506	-15.802805	0.895859
-44.439137	-12.268312	0.900864
-44.923011	-16.330947	0.905869
-44.707725	-14.728798	0.910874
-44.870187	-10.590702	0.915878
-44.881669	-16.523836	0.920883
-45.541026	-6.908040	0.925888
-46.154181	-13.025896	0.930893
-46.206727	-10.926480	0.935898
-46.573715	-9.546871	0.940902
-46.096243	-13.433332	0.945907
-46.260055	-14.303069	0.950912
-46.727534	-18.596038	0.955917
-47.363506	-24.685028	0.960922
-47.719420	-16.324993	0.965926
-47.776625	-15.613690	0.970931
-47.786222	-12.682598	0.975936
-48.477673	-9.313159	0.980941
-48.869157	-11.612213	0.985946
-49.184644	-7.864729	0.990950
-49.068415	-13.096437	0.995955
-49.149523	-9.122863	1.000960
-49.499462	-11.206932	1.005965
-49.347813	-11.686040	1.010970
-50.378686	0.259098	1.015974
-50.455162	-12.095601	1.020979
-50.741745	-16.467354	1.025984
-51.025097	-11.883346	1.030989
-50.809631	-12.796318	1.035994
-50.681205	-2.594521	1.040998
-51.192041	-15.874972	1.046003
-51.692263	-9.906323	1.051008
-52.115785	-4.436814	1.056013
-51.962300	-1.739912	1.061018
-52.720249	-6.680495	1.066022
-53.295521	-13.781814	1.071027
-53.226478	-0.454585	1.076032
-53.559989	-12.680681	1.081037
-53.309838	-15.728183	1.086042
-53.683765	-7.295740	1.091046
-53.670616	-5.741208	1.096051
-54.138981	-4.155995	1.101056
-54.578059	-0.756249	1.106061
-54.892779	-7.730464	1.111066
-55.201789	-4.281369	1.116070
-55.005644	-15.814838	1.121075
-55.288707	-10.939820	1.126080
-56.037435	-9.668447	1.131085
-56.184682	-12.600293	1.136090
-56.291939	-7.287591	1.141094
-56.187612	-16.348614	1.146099
-56.831450	-13.280808	1.151104
-56.750741	-11.512177	1.156109
-57.580566	-10.566687	1.161114
-58.373837	-4.134808	1.166118
-57.951708	-15.168807	1.171123
-58.332510	-6.887148	1.176128
-58.155453	-6.373665	1.181133
-57.772834	-5.626442	1.186138
-58.589559	-7.533432	1.191142
-59.147336	-13.612454	1.196147
-59.670944	-9.013183	1.201152
-59.488720	-7.488140	1.206157
-59.652309	-11.777807	1.211162
-59.810353	-18.808048	1.216166
-59.980899	-9.398071	1.221171
-60.522666	-2.736441	1.226176
-60.715625	-6.100917	1.231181
-60.971228	-12.872370	1.236186
-61.532385	-14.964678	1.241190
-62.266843	-11.563234	1.246195
-62.407400	-10.949681	1.251200
-62.182542	-13.113753	1.256205
-61.916408	-8.105953	1.261210
-62.562164	-11.229091	1.266214
-62.543085	-21.535966	1.271219
-62.410056	-19.484428	1.276224
-63.554426	-10.811811	1.281229
-63.673851	-20.341012	1.286234
-64.230816	-6.387993	1.291238
-64.084009	-15.835267	1.296243
-64.093768	-11.720948	1.301248
-64.456461	-9.013279	1.306253
-65.012502	-13.605659	1.311258
-65.732020	-15.005783	1.316262
-65.682383	-17.265955	1.321267
-66.115470	-12.731397	1.326272
-65.982391	-15.282961	1.331277
-65.771826	-12.208984	1.336282
-65.891512	-7.081002	1.341286
-65.950174	-12.010243	1.346291
-66.703520	-8.700767	1.351296
-66.966268	-13.585577	1.356301
-66.740264	-5.632506	1.361306
-67.574880	-5.939072	1.366310
-68.259258	-17.215223	1.371315
-68.538116	-10.860277	1.376320
-68.804941	-17.221871	1.381325
-68.534719	-18.697005	1.386330
-68.625262	-11.466579	1.391334
-68.534152	-17.447320	1.396339
-69.321328	-15.619488	1.401344
-69.926143	-14.066814	1.406349
-69.558984	-15.209041	1.411354
-70.353036	-7.328094	1.416358
-70.172786	-8.298856	1.421363
-69.825238	-9.618358	1.426368
-70.752006	-7.813082	1.431373
-70.866879	-5.238906	1.436378
-71.664046	-9.746290	1.441382
-71.503911	-12.245122	1.446387
-71.648367	-10.884342	1.451392
-72.409305	-6.479064	1.456397
-72.684207	-11.662528	1.461402
-73.112748	-8.267587	1.466406
-73.127663	-12.469675	1.471411
-73.038044	-15.900291	1.476416
-73.132600	-14.556773	1.481421
-73.104440	-12.836906	1.486426
-73.559078	-9.918775	1.491430
-73.962265	-13.332772	1.496435
-74.370837	-9.187994	1.501440
-74.188844	-9.156154	1.506445
-74.776734	-19.368524	1.511450
-75.159802	-8.201276	1.516454
-75.528518	-14.388824	1.521459
-75.626178	-11.760384	1.526464
-75.423572	-7.992330	1.531469
-76.122622	-11.708262	1.536474
-76.896692	-5.197118	1.541478
-77.036116	-17.320555	1.546483
-77.063457	-17.009357	1.551488
-77.378311	-15.932084	1.556493
-77.410565	-13.503647	1.561498
-77.448107	-11.419223	1.566502
-77.093999	-12.394909	1.571507
-77.553009	-11.206608	1.576512
-78.467410	-12.649152	1.581517
-78.501479	-18.366803	1.586522
-78.628449	-13.427507	1.591526
-79.227729	-4.899867	1.596531
-79.495551	-15.446802	1.601536
-79.935465	-8.544779	1.606541
-79.835065	-16.200532	1.611546
-80.167872	-5.117035	1.616550
-80.246817	-11.865374	1.621555
-80.099560	-18.383185	1.626560
-80.972701	-19.031752	1.631565
-81.097879	-11.036660	1.636570
-81.327527	-4.572319	1.641574
-81.536857	-5.985443	1.646579
-81.635912	-8.697010	1.651584
-82.394366	-4.896374	1.656589
-83.235655	-8.634449	1.661594
-83.078597	-10.993602	1.666598
-82.719493	-12.988757	1.671603
-83.054981	-7.880958	1.676608
-83.671589	-8.563140	1.681613
-83.692495	-13.197713	1.686618
-83.408575	-4.643078	1.691622
-83.718341	-10.080532	1.696627
-84.125705	-16.660680	1.701632
-84.835184	-9.944467	1.706637
-84.847754	-13.909646	1.711642
-85.070778	-12.549289	1.716646
-84.859454	-17.457292	1.721651
-85.582402	-16.129824	1.726656
-85.825781	-8.957855	1.731661
-85.798376	-18.576353	1.736666
-86.217409	-13.155002	1.741670
-87.174895	-7.349266	1.746675
-87.252540	-19.475992	1.751680
-87.374717	-12.120423	1.756685
-87.638409	-19.770104	1.761690
-87.932325	-15.573580	1.766694
-87.316281	-14.619102	1.771699
-87.550299	-15.243798	1.776704
-88.482411	-16.708893	1.781709
-88.669749	-19.697767	1.786714
-89.026879	-16.459474	1.791718
-89.436761	-18.622789	1.796723
-89.267556	-11.885207	1.801728
-89.526756	-3.034044	1.806733
-89.226755	-17.022846	1.811738
-90.162571	-9.350775	1.816742
-90.226709	-11.662832	1.821747
-90.576111	-15.312984	1.826752
-90.990095	-12.046856	1.831757
-91.466739	-10.422391	1.836762
-92.001752	-9.810694	1.841766
-91.873954	-19.821295	1.846771
-92.245623	-18.643431	1.851776
-92.528646	-15.451476	1.856781
-92.375511	-17.044416	1.861786
-92.508968	-12.600802	1.866790
-92.562259	-15.838330	1.871795
-92.676842	-20.240024	1.876800
-93.293274	-18.963941	1.881805
-93.643008	-19.687674	1.886810
-93.836157	-5.905195	1.891814
-93.991201	-9.563463	1.896819
-94.652800	-14.503225	1.901824
-95.326170	-4.138630	1.906829
-95.221404	-1.915017	1.911834
-95.324073	-2.737329	1.916838
-95.222802	-11.614384	1.921843
-95.454532	-8.553797	1.926848
-95.558667	-7.192968	1.931853
-95.640552	-15.006994	1.936858
-96.383740	-4.587238	1.941862
-96.475494	-13.215947	1.946867
-96.560069	-11.045109	1.951872
-97.056133	-8.981039	1.956877
-97.346197	-3.038783	1.961882
-97.702394	-6.238641	1.966886
-98.031083	-12.106565	1.971891
-98.003478	-17.096690	1.976896
-98.335498	-5.276189	1.981901
-98.513405	-11.585191	1.986906
-99.450268	-5.260665	1.991910
-99.390904	-6.652351	1.996915
-99.616267	-8.350797	2.006912
-99.054708	-12.777832	2.016909
-98.605928	-8.796097	2.026906
-98.391373	-10.863024	2.036902
-97.804020	-13.494827	2.046899
-97.406349	-11.579971	2.056896
-96.700394	-10.349820	2.066893
-96.049118	-11.122639	2.076890
-95.784573	-7.695073	2.086886
-95.022630	-14.031748	2.096883
-94.498016	-17.322164	2.106880
-94.680364	-11.886391	2.116877
-93.597644	-5.934858	2.126874
-93.107253	-7.332004	2.136870
-92.652668	-7.323455	2.146867
-91.993594	-9.624315	2.156864
-91.457183	-10.122666	2.166861
-91.379173	-10.160019	2.176858
-90.447277	-10.472867	2.186854
-90.295513	-10.208102	2.196851
-89.850562	-12.782888	2.206848
-88.804634	-10.367104	2.216845
-88.626863	-14.522148	2.226842
-88.431555	-16.231297	2.236838
-87.478680	-16.563250	2.246835
-87.313134	-13.199463	2.256832
-86.724622	-11.326991	2.266829
-86.101238	-13.381549	2.276826
-85.988909	-12.486608	2.286822
-85.163459	-17.559759	2.296819
-84.760717	-9.655590	2.306816
-83.782572	-9.896448	2.316813
-83.268035	-7.762210	2.326810
-83.044996	-3.181475	2.336806
-83.367776	-3.964186	2.346803
-82.180937	-8.887707	2.356800
-81.611595	-13.236762	2.366797
-80.831242	-12.116393	2.376794
-80.383331	-6.848438	2.386790
-80.325565	-8.517167	2.396787
-79.875510	-7.963070	2.406784
-79.101270	-9.394907	2.416781
-78.694371	-8.922786	2.426778
-77.768274	-3.624750	2.436774
-77.479595	-6.178374	2.446771
-77.429657	-7.411910	2.456768
-76.575940	-14.060638	2.466765
-76.177408	-6.703822	2.476762
-75.635030	-1.897219	2.486758
-74.680023	-8.507868	2.496755
-74.574760	-12.334854	2.506752
-74.355287	-15.609437	2.516749
-74.128107	-11.786427	2.526746
-73.284039	-10.900884	2.536742
-72.154592	-7.684006	2.546739
-71.969922	-9.739946	2.556736
-72.046430	-11.280067	2.566733
-70.994292	-12.942066	2.576730
-70.769757	-16.470853	2.586726
-70.274854	-9.303266	2.596723
-69.442591	-13.930834	2.606720
-69.390869	-11.008638	2.616717
-68.299368	-12.898504	2.626714
-68.165858	-8.249980	2.636710
-67.852325	-6.455065	2.646707
-66.662674	-9.091951	2.656704
-66.270679	-10.917252	2.666701
-65.960356	-10.629659	2.676698
-65.813180	-1.361599	2.686694
-65.565838	-5.467291	2.696691
-64.710003	-3.598427	2.706688
-63.488678	-11.010788	2.716685
-63.189167	-1.953340	2.726682
-63.177678	-9.899564	2.736678
-63.242848	-4.105077	2.746675
-62.396180	-6.178562	2.756672
-61.289660	-7.795178	2.766669
-60.608341	-9.130188	2.776666
-60.644794	-9.526673	2.786662
-60.721341	-2.206755	2.796659
-59.156408	-6.384551	2.806656
-58.873152	-7.901495	2.816653
-58.995285	-3.536271	2.826650
-57.805188	-7.814090	2.836646
-57.598994	-10.006424	2.846643
-57.360170	-0.486547	2.856640
-56.387619	-6.197136	2.866637
-56.033613	-4.475044	2.876634
-55.587572	-3.711253	2.886630
-54.895128	-2.811604	2.896627
-54.567860	-7.430236	2.906624
-54.169912	-5.246167	2.916621
-53.376050	-12.053464	2.926618
-53.295849	-5.828632	2.936614
-52.953932	-9.293336	2.946611
-51.734157	-9.597155	2.956608
-51.587407	-9.534341	2.966605
-51.218558	-11.321194	2.976602
-50.592479	-12.745801	2.986598
-50.039865	-5.105707	2.996595
-49.326568	-8.992519	3.006592
-48.588984	-8.055551	3.016589
-48.375210	-10.378941	3.026586
-48.642145	-9.111348	3.036582
-47.651919	-6.984651	3.046579
-47.282422	-7.051548	3.056576
-46.284219	-5.426589	3.066573
-45.756945	-6.693266	3.076570
-45.775525	-6.177071	3.086566
-44.784425	-7.484288	3.096563
-44.393490	-1.526405	3.106560
-44.362304	-6.621607	3.116557
-43.587315	-11.411314	3.126554
-42.976996	-5.066287	3.136550
-42.520938	-12.483036	3.146547
-41.480432	-10.500378	3.156544
-41.462489	-11.624399	3.166541
-41.468487	-3.035717	3.176538
-40.778466	-8.981073	3.186534
-39.992367	-6.585017	3.196531
-39.517742	-5.876360	3.206528
-38.514637	-11.829282	3.216525
-38.312703	-8.464822	3.226522
-38.365412	-8.738404	3.236518
-37.818726	-5.684204	3.246515
-36.954224	-3.531595	3.256512
-36.664809	-7.865577	3.266509
-35.733410	-12.334358	3.276506
-35.440278	-5.442617	3.286502
-35.147752	-8.915470	3.296499
-34.233901	-8.297374	3.306496
-34.022855	-7.921465	3.316493
-33.681927	-9.551922	3.326490
-32.743363	-2.161978	3.336486
-32.294709	-5.659141	3.346483
-32.147201	-2.149995	3.356480
-31.980989	-1.307790	3.366477
-30.937983	-2.924020	3.376474
-30.195337	-6.609503	3.386470
-29.645199	-2.478823	3.396467
-29.588018	-7.235962	3.406464
-29.293251	-9.812707	3.416461
-28.645998	-9.910180	3.426458
-28.468756	-12.680862	3.436454
-27.418962	-7.246865	3.446451
-27.108644	-5.321573	3.456448
-26.192199	-4.665867	3.466445
-25.678289	-8.474120	3.476442
-25.464935	-3.689143	3.486438
-24.968206	-9.373163	3.496435
-24.903833	-7.067467	3.506432
-24.099210	-11.994831	3.516429
-23.595127	-7.289965	3.526426
-22.581428	-11.533983	3.536422
-22.304203	-10.100866	3.546419
-22.260729	-6.955646	3.556416
-21.631568	-12.853513	3.566413
-21.075693	-11.783719	3.576410
-19.996466	-14.739185	3.586406
-19.761381	-10.296535	3.596403
-19.534311	-8.697225	3.606400
-19.372862	-11.820229	3.616397
-18.372150	-11.918883	3.626394
-17.929788	-15.418233	3.636390
-17.564986	-10.698017	3.646387
-16.772801	-10.631161	3.656384
-16.778295	-7.126702	3.666381
-15.844224	-6.666969	3.676378
-15.513491	-8.647453	3.686374
-14.975148	-4.004938	3.696371
-14.443100	-5.212172	3.706368
-13.768622	-10.331509	3.716365
-13.560185	-9.625754	3.726362
-13.051074	-17.494240	3.736358
-12.394973	-13.300867	3.746355
-12.122125	-10.162851	3.756352
-11.171560	-12.192325	3.766349
-10.729775	-8.070117	3.776346
-10.747747	-8.992149	3.786342
-9.659457	-14.514857	3.796339
-9.264361	-12.232145	3.806336
-9.013709	-9.730546	3.816333
-8.640237	-20.599890	3.826330
-7.623247	-12.179989	3.836326
-7.367163	-8.313960	3.846323
-7.185466	-4.515541	3.856320
-6.433888	-10.438805	3.866317
-5.931485	-10.000558	3.876314
-5.855535	-9.603615	3.886310
-5.046229	-1.860936	3.896307
-4.791384	4.276526	3.906304
-4.250814	2.595978	3.916301
-3.610475	17.783717	3.926298
-3.372438	29.229698	3.936294
-2.881662	34.278761	3.946291
-2.388152	47.373362	3.956288
-1.961066	57.985331	3.966285
-1.436801	76.919583	3.976282
-0.966881	94.522374	3.986278
-0.568768	113.970469	3.996275
0.000000	121.630850	4.001280
-0.160713	132.263714	4.006285
0.192066	140.870978	4.011290
0.156689	146.735669	4.016294
0.471854	150.245796	4.021299
0.434503	151.488674	4.026304
0.695693	165.273322	4.031309
1.379118	165.913610	4.036314
0.938072	158.645790	4.041318
0.886973	156.325352	4.046323
0.767565	150.535511	4.051328
0.560432	155.901778	4.056333
0.996677	167.871698	4.061338
0.563421	177.370136	4.066342
0.947314	175.374263	4.071347
1.117747	178.533616	4.076352
1.051970	179.866342	4.081357
1.215916	177.363726	4.086362
1.077620	176.360295	4.091366
1.168769	184.075031	4.096371
0.822147	168.532148	4.101376
0.962881	173.255816	4.106381
1.167290	174.008649	4.111386
1.152859	174.181802	4.116390
1.156968	178.186443	4.121395
1.073285	169.705073	4.126400
1.009661	167.801024	4.131405
1.147719	163.739586	4.136410
0.808348	172.252156	4.141414
0.938975	165.914029	4.146419
1.391849	175.043550	4.151424
1.262068	178.002879	4.156429
1.365417	169.457589	4.161434
1.215634	180.718350	4.166438
1.194454	169.541289	4.171443
1.269855	170.839378	4.176448
1.007747	170.054536	4.181453
1.242332	170.005425	4.186458
1.327475	174.737748	4.191462
0.977081	175.950276	4.196467
1.318980	177.403020	4.201472
1.252703	181.877354	4.206477
1.498108	180.966038	4.211482
1.224789	183.539602	4.216486
1.293221	184.636302	4.221491
1.300395	184.654235	4.226496
1.196983	183.499843	4.231501
1.147327	180.008616	4.236506
1.459904	182.272664	4.241510
1.404595	178.089473	4.246515
1.355452	181.283013	4.251520
1.311983	180.625477	4.256525
1.506583	173.793345	4.261530
1.518418	183.554673	4.266534
1.266836	174.355978	4.271539
1.486659	179.839270	4.276544
1.360586	182.238051	4.281549
1.358129	180.096693	4.286554
1.175298	180.982583	4.291558
1.476951	178.746421	4.296563
1.295001	182.799013	4.301568
1.294632	182.906703	4.306573
1.132716	184.162651	4.311578
1.096242	183.437588	4.316582
1.545988	189.400764	4.321587
1.823115	203.230415	4.326592
1.876243	199.378341	4.331597
1.473642	185.903714	4.336602
1.288925	189.491678	4.341606
1.584260	195.823738	4.346611
1.819615	199.374774	4.351616
1.803687	213.895452	4.356621
2.007203	200.155605	4.361626
1.470747	196.490237	4.366630
1.515390	186.473477	4.371635
1.946496	215.151615	4.376640
1.658598	203.399141	4.381645
1.890757	201.562929	4.386650
1.575514	208.727196	4.391654
1.861832	210.387909	4.396659
1.702204	203.851357	4.401664
1.704662	209.659559	4.406669
2.198276	200.291044	4.411674
1.823910	198.890943	4.416678
1.346892	192.663233	4.421683
1.706748	199.545220	4.426688
1.570387	210.952604	4.431693
2.226394	209.885611	4.436698
2.143670	214.264439	4.441702
1.894360	205.233050	4.446707
2.071430	212.684490	4.451712
1.799705	208.854519	4.456717
1.891223	202.123844	4.461722
2.020559	209.937048	4.466726
1.981360	202.451623	4.471731
2.089350	201.118787	4.476736
1.437954	196.205843	4.481741
2.030506	202.093006	4.486746
1.729190	212.247948	4.491750
1.799051	210.702753	4.496755
2.289144	213.945217	4.501760
2.101751	217.742407	4.506765
2.394633	206.703080	4.511770
1.762493	216.185049	4.516774
1.493669	209.981864	4.521779
1.703268	214.707475	4.526784
1.847467	208.003397	4.531789
2.099291	207.322029	4.536794
1.857855	212.317176	4.541798
2.035780	210.131911	4.546803
2.009068	207.877269	4.551808
2.191388	215.539860	4.556813
1.812132	209.353869	4.561818
1.992634	231.791146	4.566822
2.376990	240.013901	4.571827
2.562709	248.375151	4.576832
2.154241	235.065912	4.581837
2.258523	222.300095	4.586842
1.921180	222.896839	4.591846
2.310527	226.493506	4.596851
2.753997	233.017646	4.601856
2.137346	233.366818	4.606861
1.970489	217.726303	4.611866
2.539284	235.787867	4.616870
2.006614	235.041984	4.621875
2.206718	233.697967	4.626880
2.038458	239.928220	4.631885
2.685961	241.520046	4.636890
2.607854	240.735026	4.641894
2.712469	233.515093	4.646899
2.428239	234.986236	4.651904
2.338941	230.665959	4.656909
2.075715	218.833704	4.661914
2.328531	241.446392	4.666918
2.425418	244.111018	4.671923
2.652406	241.693488	4.676928
2.615424	240.699589	4.681933
2.568597	234.977512	4.686938
2.439812	248.794469	4.691942
2.704174	237.177446	4.696947
2.638236	233.473613	4.701952
2.392089	231.610631	4.706957
2.386040	232.582891	4.711962
2.383051	240.717261	4.716966
2.545439	241.334274	4.721971
2.678413	244.869622	4.726976
2.395156	244.825209	4.731981
2.568872	234.136607	4.736986
2.216755	242.217769	4.741990
2.653144	242.339714	4.746995
2.506777	240.556106	4.752000
2.113576	240.623721	4.757005
2.782707	239.874215	4.762010
2.636147	246.401643	4.767014
2.736901	240.691387	4.772019
2.821952	241.753866	4.777024
2.514529	249.983094	4.782029
2.677256	242.852183	4.787034
2.564536	249.602128	4.792038
2.429253	245.570575	4.797043
2.549334	247.260338	4.802048
2.539100	253.390063	4.807053
3.020756	260.658062	4.812058
2.999484	277.511264	4.817062
2.889854	259.659871	4.822067
2.590149	254.809210	4.827072
2.712830	265.008896	4.832077
3.000471	259.313828	4.837082
3.098773	266.647843	4.842086
2.822074	251.555900	4.847091
3.021463	253.571830	4.852096
2.739632	256.456771	4.857101
3.163040	252.126263	4.862106
2.882679	255.498182	4.867110
2.448802	250.592485	4.872115
3.014111	265.987633	4.877120
3.183131	275.832104	4.882125
3.268806	265.365995	4.887130
2.892185	255.405294	4.892134
2.890763	259.977115	4.897139
2.991153	263.992094	4.902144
3.038691	273.032918	4.907149
3.275354	269.474949	4.912154
3.221649	264.013356	4.917158
2.786098	254.742025	4.922163
3.128665	250.367158	4.927168
3.051991	266.637365	4.932173
3.338272	263.878413	4.937178
3.060079	266.984247	4.942182
3.009805	273.936446	4.947187
3.383086	270.255968	4.952192
2.927674	268.147158	4.957197
2.869016	260.810269	4.962202
2.637874	267.278108	4.967206
2.579660	270.618606	4.972211
3.088875	271.393588	4.977216
2.766957	279.909819	4.982221
3.178805	268.282468	4.987226
2.974607	278.482436	4.992230
3.366813	279.364219	4.997235
3.496563	277.354122	5.002240
3.345146	278.598951	5.007245
3.383608	271.091915	5.012250
3.185902	273.663210	5.017254
3.211730	273.431470	5.022259
3.147171	265.899348	5.027264
3.331613	289.240900	5.032269
3.544128	288.780782	5.037274
3.699491	280.743022	5.042278
3.435560	277.601507	5.047283
3.464266	271.184301	5.052288
3.249937	272.514853	5.057293
3.477571	263.238336	5.062298
3.241344	278.375485	5.067302
3.390647	273.888336	5.072307
3.551792	264.568388	5.077312
3.191905	280.044325	5.082317
3.585903	282.055268	5.087322
3.297086	289.272399	5.092326
3.251458	294.860330	5.097331
3.910120	288.708861	5.102336
3.500956	291.135914	5.107341
3.885565	287.934550	5.112346
3.630692	281.672222	5.117350
3.491044	285.297480	5.122355
3.412312	278.906489	5.127360
3.104061	290.932298	5.132365
3.494308	294.876845	5.137370
3.319771	297.593229	5.142374
3.745099	291.566671	5.147379
3.856947	292.802148	5.152384
3.659830	299.549434	5.157389
3.685209	294.644984	5.162394
3.363804	295.492345	5.167398
3.465579	289.883153	5.172403
3.666494	297.416336	5.177408
3.439517	301.978994	5.182413
3.740661	280.846143	5.187418
3.445012	300.440717	5.192422
3.606757	294.632364	5.197427
3.591798	292.863091	5.202432
3.466994	293.790571	5.207437
4.072252	308.765093	5.212442
3.696326	308.978712	5.217446
3.766974	313.570962	5.222451
4.053633	313.700402	5.227456
3.853961	305.850784	5.232461
3.838991	293.818479	5.237466
3.912895	299.182160	5.242470
3.801409	311.174183	5.247475
4.011117	298.980345	5.252480
3.712191	310.776929	5.257485
4.045792	309.557651	5.262490
3.738227	308.855809	5.267494
3.765373	317.339856	5.272499
4.208864	317.188618	5.277504
3.839878	323.443825	5.282509
4.031067	320.655378	5.287514
4.077035	317.199855	5.292518
4.309823	317.325028	5.297523
4.141249	306.613746	5.302528
3.892990	300.616132	5.307533
4.135703	301.239623	5.312538
3.754744	309.375926	5.317542
4.086046	325.607976	5.322547
4.532659	328.854068	5.327552
4.061009	314.447310	5.332557
4.265458	297.347394	5.337562
4.099456	298.844427	5.342566
3.733209	300.477039	5.347571
3.918791	301.618780	5.352576
4.012817	323.718467	5.357581
4.555593	312.643332	5.362586
4.313476	317.065984	5.367590
4.199664	325.356850	5.372595
4.636041	320.157452	5.377600
4.063425	307.825990	5.382605
4.302902	299.284752	5.387610
4.229232	303.975398	5.392614
4.263181	306.137314	5.397619
4.327240	299.274839	5.402624
4.352202	306.772147	5.407629
4.175247	302.756560	5.412634
4.580916	310.346453	5.417638
4.087851	298.926411	5.422643
4.230132	299.274478	5.427648
4.399150	314.693406	5.432653
4.523686	305.977076	5.437658
4.364905	306.954138	5.442662
4.299974	313.231603	5.447667
4.807008	317.521797	5.452672
4.287194	303.903981	5.457677
4.026525	301.090979	5.462682
4.389798	313.360256	5.467686
4.474476	313.669837	5.472691
4.596767	313.726793	5.477696
4.480501	322.211025	5.482701
4.251163	330.852069	5.487706
4.199813	327.962180	5.492710
4.612644	322.728483	5.497715
4.581167	318.649114	5.502720
4.363321	327.225093	5.507725
4.456651	316.014292	5.512730
4.351375	320.940814	5.517734
4.305891	321.742052	5.522739
4.685740	320.781324	5.527744
4.451606	322.304785	5.532749
4.594120	317.473839	5.537754
4.505783	317.225073	5.542758
4.358461	324.417025	5.547763
5.006904	314.505497	5.552768
4.730732	313.564653	5.557773
5.079910	314.611323	5.562778
4.776364	320.435568	5.567782
4.792647	314.659348	5.572787
4.802708	313.828960	5.577792
4.716164	315.351587	5.582797
4.879428	310.362391	5.587802
4.747961	317.118444	5.592806
4.452468	318.189557	5.597811
4.802919	310.906008	5.602816
4.854662	320.107550	5.607821
4.761973	319.995501	5.612826
4.874673	326.596485	5.617830
4.680873	324.136893	5.622835
4.703970	306.660250	5.627840
4.640302	312.554711	5.632845
4.744217	311.877386	5.637850
4.604240	319.587039	5.642854
4.946715	314.547793	5.647859
4.777149	314.172472	5.652864
4.901170	313.555291	5.657869
4.420613	313.747236	5.662874
4.709364	324.044483	5.667878
4.955767	332.285596	5.672883
4.925529	333.653927	5.677888
5.213281	346.593036	5.682893
5.274397	336.621082	5.687898
5.048415	328.693294	5.692902
4.878237	320.975117	5.697907
5.079582	319.510679	5.702912
4.653470	336.765485	5.707917
5.031028	343.173380	5.712922
4.987639	350.064426	5.717926
4.496609	346.996222	5.722931
4.825107	342.063547	5.727936
4.889155	346.789709	5.732941
5.280261	342.381952	5.737946
5.155013	345.052706	5.742950
5.256075	348.368420	5.747955
5.439956	338.991110	5.752960
5.169315	337.483101	5.757965
5.157456	344.720407	5.762970
5.268143	346.351532	5.767974
5.037498	348.178168	5.772979
5.234754	334.970694	5.777984
5.135351	351.712746	5.782989
5.088505	344.956105	5.787994
5.181011	353.815965	5.792998
5.294816	345.569514	5.798003
5.113923	341.073648	5.803008
4.728309	348.021141	5.808013
5.095156	347.359824	5.813018
5.242212	358.723176	5.818022
5.002273	362.215370	5.823027
5.349331	358.934420	5.828032
5.646186	357.739843	5.833037
5.712247	352.658203	5.838042
5.539326	352.137873	5.843046
5.233831	342.365363	5.848051
5.310900	334.545410	5.853056
5.206721	346.273731	5.858061
5.571528	350.981541	5.863066
5.355313	346.010290	5.868070
5.442784	363.014318	5.873075
5.333432	360.668121	5.878080
5.579460	372.231204	5.883085
5.745758	361.603791	5.888090
5.595338	363.851366	5.893094
5.356233	351.964648	5.898099
5.633351	352.544820	5.903104
5.503955	349.799955	5.908109
5.558228	350.085797	5.913114
5.443657	351.324894	5.918118
5.570012	364.248016	5.923123
5.678572	343.999276	5.928128
5.431101	364.696880	5.933133
5.392076	355.148626	5.938138
5.530818	360.862894	5.943142
5.530158	366.908911	5.948147
5.997210	360.771431	5.953152
5.606062	368.074129	5.958157
5.633570	369.623295	5.963162
5.930190	357.545597	5.968166
5.933245	366.229568	5.973171
6.180918	356.510127	5.978176
5.757200	348.837740	5.983181
5.931945	344.451014	5.988186
5.211844	347.113146	5.993190
5.265181	353.125442	5.998195
5.911227	354.227131	6.003200
5.775876	356.538797	6.008205
5.861292	360.299868	6.013210
5.937098	363.575226	6.018214
5.529438	365.344004	6.023219
5.782968	364.045442	6.028224
5.804612	363.827008	6.033229
5.858761	368.858433	6.038234
5.844287	355.193535	6.043238
5.623455	364.383756	6.048243
5.949561	358.881981	6.053248
5.586256	356.553179	6.058253
5.353475	368.649546	6.063258
5.882608	361.733619	6.068262
5.522443	362.549053	6.073267
5.988672	368.126914	6.078272
5.557963	364.369118	6.083277
5.673369	368.770919	6.088282
5.857250	369.248550	6.093286
5.507756	363.931055	6.098291
5.338414	352.827566	6.103296
5.369546	354.195835	6.108301
5.617501	355.264595	6.113306
5.683033	362.163997	6.118310
5.337223	358.048139	6.123315
5.824115	363.426632	6.128320
5.667403	383.613424	6.133325
5.885887	377.432384	6.138330
5.886217	375.287404	6.143334
5.869663	379.491457	6.148339
5.999699	367.487145	6.153344
5.911095	364.773891	6.158349
5.945073	363.449402	6.163354
6.159416	368.765929	6.168358
5.529444	371.315956	6.173363
6.037922	365.440940	6.178368
5.512214	373.887707	6.183373
5.379562	362.876574	6.188378
5.551070	366.678026	6.193382
5.270888	369.898081	6.198387
5.704252	376.727564	6.203392
5.844441	394.969916	6.208397
5.928631	386.832460	6.213402
5.903141	396.912924	6.218406
5.973886	393.602223	6.223411
6.210725	382.201360	6.228416
5.938214	376.289752	6.233421
5.868095	367.666973	6.238426
5.705573	365.414474	6.243430
5.059899	366.597059	6.248435
6.016546	367.485877	6.253440
5.567547	367.533707	6.258445
5.439036	363.877553	6.263450
6.154395	376.085728	6.268454
5.514006	379.121425	6.273459
5.603364	377.354884	6.278464
5.608934	391.505369	6.283469
5.764878	392.161356	6.288474
5.961628	390.463513	6.293478
5.577956	395.452383	6.298483
5.856938	387.376346	6.303488
5.716838	401.328059	6.308493
5.762508	391.829874	6.313498
6.077876	386.383545	6.318502
6.076957	391.021760	6.323507
5.953377	380.714711	6.328512
5.262780	377.706046	6.333517
5.648181	379.354513	6.338522
5.800461	380.270493	6.343526
5.707287	389.051714	6.348531
5.818733	380.596810	6.353536
5.787050	395.351040	6.358541
5.717820	394.589940	6.363546
5.893544	387.817611	6.368550
5.536402	387.942887	6.373555
5.857225	383.153762	6.378560
5.582130	398.907662	6.383565
5.500683	386.164317	6.388570
6.085257	386.611200	6.393574
5.501458	388.711121	6.398579
6.053592	391.061283	6.403584
5.607507	401.131305	6.408589
5.720332	395.273589	6.413594
5.937446	392.689900	6.418598
6.329390	405.676103	6.423603
6.142781	387.118404	6.428608
5.514499	387.146691	6.433613
5.535825	376.424783	6.438618
5.991130	382.643420	6.443622
5.767249	385.506703	6.448627
5.947964	382.033352	6.453632
5.794927	377.947586	6.458637
5.592887	367.118094	6.463642
6.027332	382.068654	6.468646
5.437780	373.612166	6.473651
5.846884	377.550631	6.478656
5.992242	392.739196	6.483661
5.604479	373.564269	6.488666
5.670351	382.782625	6.493670
5.752389	396.728222	6.498675
5.864750	392.227813	6.503680
5.950870	384.298863	6.508685
5.705327	373.292645	6.513690
5.465121	375.819952	6.518694
5.717692	386.720810	6.523699
6.197399	380.764849	6.528704
5.882650	374.717451	6.533709
5.887813	359.265160	6.538714
5.742613	357.497176	6.543718
5.479328	369.765970	6.548723
5.808780	363.997921	6.553728
5.445818	370.837493	6.558733
5.889231	381.559940	6.563738
5.791827	387.450187	6.568742
5.954170	388.589225	6.573747
6.128209	383.259813	6.578752
5.850425	367.759821	6.583757
5.679266	371.427967	6.588762
5.645135	373.084806	6.593766
5.246874	373.836570	6.598771
5.900066	371.782929	6.603776
5.640249	387.610369	6.608781
5.569810	386.482467	6.613786
6.284264	388.718772	6.618790
6.087304	383.152898	6.623795
5.852556	372.192456	6.628800
5.724754	374.828811	6.633805
5.792843	372.973834	6.638810
5.943236	366.952093	6.643814
5.614952	377.481481	6.648819
5.794774	367.440409	6.653824
5.988062	370.738605	6.658829
6.041836	365.810732	6.663834
5.683208	368.906961	6.668838
5.834542	374.499052	6.673843
5.717514	368.012753	6.678848
5.571930	367.013610	6.683853
5.184348	375.540110	6.688858
5.471389	374.691904	6.693862
5.671025	391.855664	6.698867
5.696400	391.459480	6.703872
5.907225	397.383997	6.708877
6.388727	392.981136	6.713882
6.272041	383.666418	6.718886
5.694661	382.781958	6.723891
5.952926	375.012869	6.728896
5.646033	374.889878	6.733901
5.626863	375.329523	6.738906
5.736524	370.443567	6.743910
5.662489	377.364705	6.748915
5.799852	376.625224	6.753920
5.526653	381.302664	6.758925
5.473661	373.983828	6.763930
5.863613	383.882545	6.768934
5.724337	397.685432	6.773939
5.920851	381.893285	6.778944
5.811244	379.629382	6.783949
5.675416	378.824869	6.788954
5.600080	375.065523	6.793958
5.560335	392.450049	6.798963
5.806454	389.479035	6.803968
5.756401	399.844895	6.808973
5.862934	399.502514	6.813978
6.208998	399.926422	6.818982
5.889448	389.558132	6.823987
5.615822	381.808579	6.828992
5.574624	378.107191	6.833997
5.616486	395.931425	6.839002
5.896034	395.078058	6.844006
5.711930	401.285524	6.849011
5.951614	388.906626	6.854016
5.935464	389.946906	6.859021
6.207796	381.248656	6.864026
5.965402	381.723056	6.869030
5.558041	383.320948	6.874035
5.874476	373.170019	6.879040
5.505075	371.038314	6.884045
5.767392	367.802193	6.889050
5.759995	365.902023	6.894054
5.472095	372.992497	6.899059
5.940219	370.708247	6.904064
5.806129	369.856008	6.909069
5.871433	366.928968	6.914074
5.718111	367.696379	6.919078
5.711778	371.379991	6.924083
6.046431	372.134700	6.929088
5.911142	369.824178	6.934093
5.706202	375.291408	6.939098
5.890781	366.660611	6.944102
5.793374	375.768346	6.949107
6.321995	369.023337	6.954112
5.950786	375.003665	6.959117
5.940061	374.831399	6.964122
5.970611	364.513017	6.969126
5.669082	369.299268	6.974131
6.031942	366.547359	6.979136
5.982570	372.553507	6.984141
6.070992	366.234535	6.989146
6.017677	364.702178	6.994150
5.765145	366.174724	6.999155
5.846595	353.877433	7.004160
5.622203	355.835971	7.009165
5.889645	362.270509	7.014170
6.150176	358.753098	7.019174
5.513990	366.663413	7.024179
5.702613	361.081805	7.029184
5.648754	358.496018	7.034189
5.607243	367.629847	7.039194
5.777975	373.842168	7.044198
5.954794	373.447716	7.049203
6.224447	364.537922	7.054208
5.688557	361.217276	7.059213
5.533211	358.963661	7.064218
6.146015	354.575167	7.069222
5.471992	353.974670	7.074227
5.987435	360.300993	7.079232
5.823730	357.415938	7.084237
5.500052	355.732690	7.089242
5.538352	354.976996	7.094246
5.706153	359.550968	7.099251
6.060920	368.275091	7.104256
5.551224	357.977553	7.109261
5.782494	366.711412	7.114266
5.878185	374.770368	7.119270
5.713547	369.038118	7.124275
5.585748	371.456175	7.129280
5.723629	372.035880	7.134285
5.483245	372.133485	7.139290
6.024878	369.780843	7.144294
6.087860	375.139921	7.149299
5.944341	361.656459	7.154304
5.789861	362.382922	7.159309
5.392218	357.613919	7.164314
5.748521	364.977407	7.169318
5.347353	365.115865	7.174323
5.781836	369.063032	7.179328
5.957474	374.031251	7.184333
6.162180	367.988399	7.189338
5.969916	371.666158	7.194342
5.859542	358.297759	7.199347
5.630504	347.270006	7.204352
5.662500	351.197578	7.209357
5.612030	359.184373	7.214362
5.733066	363.037975	7.219366
5.725790	374.390564	7.224371
5.801197	372.464847	7.229376
5.774962	375.895298	7.234381
5.645020	375.529624	7.239386
5.700852	370.769106	7.244390
5.706025	377.788642	7.249395
5.677765	370.488103	7.254400
5.433805	373.452586	7.259405
6.036130	379.740078	7.264410
5.800549	378.157005	7.269414
5.610342	377.291357	7.274419
5.454410	368.928708	7.279424
5.681306	370.557560	7.284429
5.641962	375.356774	7.289434
5.634873	373.269897	7.294438
5.848846	377.824030	7.299443
5.827712	370.623620	7.304448
5.735046	370.894376	7.309453
5.764255	377.394484	7.314458
5.770813	378.858329	7.319462
5.942211	371.956968	7.324467
5.761433	374.940087	7.329472
5.678671	371.039532	7.334477
5.475731	379.790383	7.339482
5.626481	368.985054	7.344486
5.833166	378.905975	7.349491
5.812145	367.194097	7.354496
5.920747	374.067815	7.359501
5.741130	371.087160	7.364506
6.345447	369.107567	7.369510
5.904774	378.850872	7.374515
5.669071	382.010221	7.379520
5.757454	374.482715	7.384525
5.992059	373.547762	7.389530
6.228095	381.103986	7.394534
5.983994	384.134930	7.399539
5.785465	370.141178	7.404544
5.446606	378.897372	7.409549
5.607051	377.834762	7.414554
6.213584	380.847159	7.419558
6.108069	378.111227	7.424563
5.893792	378.903947	7.429568
5.403182	371.564664	7.434573
5.758839	367.152929	7.439578
6.114698	370.906697	7.444582
5.558532	369.579180	7.449587
5.649756	368.365998	7.454592
5.876732	379.903579	7.459597
5.697207	378.454145	7.464602
5.898973	369.295495	7.469606
5.811086	372.858928	7.474611
5.683425	376.071056	7.479616
5.673713	374.300958	7.484621
5.832991	378.357414	7.489626
5.742111	372.914231	7.494630
5.632940	374.060740	7.499635
5.745259	371.357331	7.504640
5.881343	366.321731	7.509645
5.710106	373.359241	7.514650
6.143920	379.932394	7.519654
5.834520	365.114361	7.524659
5.791762	363.890403	7.529664
5.633210	357.337808	7.534669
5.586910	361.913479	7.539674
5.958737	367.360507	7.544678
5.608077	369.515874	7.549683
5.670102	368.864052	7.554688
5.625342	374.856828	7.559693
5.517806	378.091133	7.564698
5.659168	377.493395	7.569702
5.610990	376.611962	7.574707
5.602955	380.700795	7.579712
5.620994	376.553593	7.584717
5.371657	371.638111	7.589722
5.822241	369.945042	7.594726
5.632192	376.049023	7.599731
5.687158	373.876554	7.604736
5.642842	380.052758	7.609741
5.789074	378.498822	7.614746
6.205702	371.888305	7.619750
5.658330	379.965130	7.624755
5.786101	374.418301	7.629760
5.611215	375.043540	7.634765
5.681015	378.977887	7.639770
5.877996	377.460342	7.644774
5.424775	377.170311	7.649779
5.898855	376.039887	7.654784
6.024374	374.998533	7.659789
5.888567	387.003885	7.664794
6.030114	371.685371	7.669798
5.816007	383.706075	7.674803
5.858815	371.791270	7.679808
5.976035	370.425346	7.684813
5.660055	369.838705	7.689818
5.546633	370.492338	7.694822
5.465929	377.256329	7.699827
5.487690	371.235632	7.704832
5.283102	383.068194	7.709837
5.264719	381.289955	7.714842
5.579444	392.551293	7.719846
5.787444	398.985608	7.724851
5.695772	402.622402	7.729856
6.173225	404.386251	7.734861
5.866860	401.922029	7.739866
5.845532	396.180111	7.744870
6.009701	402.023310	7.749875
5.863670	392.706829	7.754880
5.859711	380.501910	7.759885
5.482145	372.208567	7.764890
5.811374	381.025257	7.769894
5.505553	387.327598	7.774899
5.672329	396.308792	7.779904
5.800485	401.559655	7.784909
5.817457	400.402324	7.789914
5.933192	405.433662	7.794918
5.857083	406.647792	7.799923
5.919586	394.116145	7.804928
5.651755	382.702108	7.809933
5.919456	387.548432	7.814938
5.743354	384.608355	7.819942
5.580261	390.780910	7.824947
5.701510	389.066350	7.829952
5.974713	389.121956	7.834957
5.606081	401.945005	7.839962
5.751892	389.878110	7.844966
5.906701	398.373956	7.849971
6.197697	399.473982	7.854976
5.707818	380.817976	7.859981
5.460289	378.711587	7.864986
5.932496	380.685055	7.869990
5.576070	382.591389	7.874995
5.757875	381.652001	7.880000
5.904863	386.510791	7.885005
5.728635	387.035000	7.890010
6.016371	384.585847	7.895014
5.561432	376.807579	7.900019
5.968725	383.726544	7.905024
5.940893	377.068168	7.910029
6.158440	377.047020	7.915034
6.049212	376.595865	7.920038
5.898985	373.743509	7.925043
6.220286	371.640304	7.930048
5.787788	366.104781	7.935053
5.916582	384.646286	7.940058
5.951744	374.314525	7.945062
5.959451	385.474966	7.950067
5.756737	379.422778	7.955072
5.977578	376.667671	7.960077
5.401051	384.790165	7.965082
5.895942	378.455358	7.970086
5.934201	376.067195	7.975091
5.717058	379.805777	7.980096
5.774055	382.356413	7.985101
5.583438	387.881527	7.990106
5.768934	377.630761	7.995110
5.626838	376.510853	8.000115
5.764527	382.279107	8.005133
6.133312	376.522670	8.010150
6.178582	378.516365	8.015168
6.065389	375.018674	8.020186
5.521183	367.148107	8.025203
5.658070	373.289825	8.030221
5.838774	372.561206	8.035238
5.913300	383.348271	8.040256
5.860387	372.532732	8.045274
5.941039	376.193407	8.050291
5.604462	368.852216	8.055309
6.087086	371.939091	8.060326
5.713879	375.468469	8.065344
5.872313	369.710073	8.070362
5.627449	360.555892	8.075379
5.806732	370.361014	8.080397
5.923713	369.522403	8.085414
5.771140	381.329385	8.090432
6.008229	377.654085	8.095450
6.088629	376.051193	8.100467
5.989661	376.366455	8.105485
5.762441	361.194878	8.110502
5.687143	372.074688	8.115520
5.934400	380.966720	8.120538
5.741902	381.388059	8.125555
5.640308	390.804601	8.130573
5.833749	380.199996	8.135590
5.730239	384.899151	8.140608
5.777472	380.615972	8.145626
5.956792	383.724827	8.150643
5.710113	387.600563	8.155661
6.197707	388.228422	8.160678
5.608462	381.336799	8.165696
5.597814	381.284879	8.170714
5.739509	380.802162	8.175731
5.788848	382.135695	8.180749
5.914956	377.360578	8.185766
5.529549	382.854666	8.190784
5.880116	376.567762	8.195802
5.769205	394.360827	8.200819
6.118839	398.273102	8.205837
6.165363	388.786375	8.210854
6.096887	385.379544	8.215872
5.922091	380.310467	8.220890
6.217891	379.292542	8.225907
5.820413	377.091902	8.230925
6.165303	379.382913	8.235942
5.510248	383.820821	8.240960
5.691237	395.342361	8.245978
6.121825	410.842183	8.250995
6.286557	406.376609	8.256013
6.450819	411.185552	8.261030
6.392894	403.128808	8.266048
5.944052	381.440602	8.271066
5.910228	382.657702	8.276083
5.894068	382.732866	8.281101
5.975922	387.194889	8.286118
6.301124	395.317439	8.291136
5.840995	389.153597	8.296154
6.003446	385.190131	8.301171
6.320850	402.285389	8.306189
6.223575	389.387710	8.311206
5.953509	393.244998	8.316224
6.040599	384.670249	8.321242
6.008922	395.054156	8.326259
6.328789	399.318187	8.331277
6.454854	396.979229	8.336294
5.837882	394.475107	8.341312
5.824891	385.007115	8.346330
6.450137	386.383519	8.351347
6.155073	389.383208	8.356365
6.207719	390.514267	8.361382
6.371905	391.842542	8.366400
6.145333	392.894003	8.371418
6.195736	385.691359	8.376435
5.898421	387.211403	8.381453
6.080234	385.548541	8.386470
6.013449	382.179315	8.391488
6.017457	393.838856	8.396506
6.544533	403.744474	8.401523
6.419740	399.305046	8.406541
6.170655	387.052666	8.411558
5.697106	394.267683	8.416576
6.517704	392.735726	8.421594
6.055871	390.191671	8.426611
5.972227	395.114943	8.431629
6.306252	400.547513	8.436646
6.326243	407.376440	8.441664
6.354663	400.552734	8.446682
6.304956	404.476697	8.451699
6.364318	401.576952	8.456717
6.357616	391.495782	8.461734
6.125612	388.881232	8.466752
5.965533	386.214461	8.471770
6.222822	393.845837	8.476787
5.830107	401.348057	8.481805
6.095424	396.342988	8.486822
6.550943	406.423842	8.491840
6.196480	411.348260	8.496858
6.029328	401.033303	8.501875
6.024602	407.938658	8.506893
6.081368	408.308565	8.511910
6.360976	418.520950	8.516928
6.098853	409.697618	8.521946
6.433007	402.053177	8.526963
6.201693	404.468616	8.531981
6.634136	392.331017	8.536998
6.414614	411.971283	8.542016
6.026446	406.960664	8.547034
6.443980	402.847031	8.552051
6.243736	404.443476	8.557069
6.338655	397.947072	8.562087
6.329674	408.021356	8.567104
6.114392	408.499889	8.572122
6.312283	401.176450	8.577139
6.598080	408.626678	8.582157
6.375141	398.351965	8.587175
6.408513	403.843969	8.592192
6.327498	409.278050	8.597210
6.548144	404.945775	8.602227
6.335985	409.860659	8.607245
6.495799	409.463478	8.612263
6.238104	406.739323	8.617280
6.341944	406.543351	8.622298
6.226007	400.843442	8.627315
6.282636	409.818814	8.632333
6.736063	417.034674	8.637351
6.474033	419.773617	8.642368
6.458496	411.337904	8.647386
6.684591	407.645376	8.652403
6.305114	417.515432	8.657421
6.763496	412.470833	8.662439
6.528848	411.724834	8.667456
6.635410	404.803758	8.672474
6.587535	401.646168	8.677491
6.488622	413.817183	8.682509
6.683923	404.408264	8.687527
6.917480	403.100243	8.692544
6.611789	408.550371	8.697562
6.686544	403.066911	8.702579
6.567299	407.828479	8.707597
6.440219	406.251577	8.712615
6.296950	409.278126	8.717632
6.030765	404.516745	8.722650
6.569480	401.829530	8.727667
6.221518	405.932467	8.732685
6.292378	397.981901	8.737703
6.511502	419.128546	8.742720
6.485601	427.147993	8.747738
6.991178	424.929815	8.752755
6.910986	413.547325	8.757773
6.669081	407.873337	8.762791
6.770040	408.952695	8.767808
6.451461	411.548971	8.772826
6.782501	399.878412	8.777843
6.467495	401.524281	8.782861
6.712898	401.735436	8.787879
6.458002	404.523757	8.792896
6.295945	412.005847	8.797914
6.793998	406.033624	8.802931
6.588742	403.339172	8.807949
6.239124	407.120491	8.812967
6.680222	415.704664	8.817984
6.719848	418.090543	8.823002
6.745319	416.521444	8.828019
6.652388	422.711584	8.833037
6.772635	420.042185	8.838055
6.751826	408.476892	8.843072
6.614333	411.275336	8.848090
6.740048	403.865308	8.853107
6.613169	412.143456	8.858125
6.699505	411.915497	8.863143
6.681269	419.775966	8.868160
6.890132	421.703172	8.873178
6.450772	407.328251	8.878195
6.592937	415.734916	8.883213
6.798391	426.189213	8.888231
6.751015	420.323996	8.893248
6.853192	432.643587	8.898266
7.058567	425.520935	8.903283
6.732206	423.170367	8.908301
6.556997	423.412299	8.913319
6.704743	421.937765	8.918336
6.736531	425.684950	8.923354
6.863718	424.093702	8.928371
6.993347	427.017807	8.933389
6.746346	433.244561	8.938407
6.890754	433.960568	8.943424
6.919672	426.568758	8.948442
6.843568	415.554841	8.953459
6.725899	411.180569	8.958477
6.890768	426.955295	8.963495
6.768390	423.238129	8.968512
6.873368	420.981342	8.973530
6.921646	412.901748	8.978547
6.907037	416.069204	8.983565
6.714716	420.835842	8.988583
6.634598	420.630645	8.993600
6.815640	431.407467	8.998618
6.860913	426.130551	9.003635
6.910392	436.587050	9.008653
6.897051	434.014184	9.013671
7.073811	424.298888	9.018688
6.915472	431.395419	9.023706
7.154550	433.788114	9.028723
6.884677	429.563761	9.033741
6.660134	428.907702	9.038759
7.289634	427.121487	9.043776
6.725755	431.027685	9.048794
6.816180	429.031926	9.053811
6.955486	422.859945	9.058829
6.716172	429.735564	9.063847
7.040079	428.700639	9.068864
6.768447	434.618818	9.073882
6.662733	436.033299	9.078899
7.317522	431.958455	9.083917
7.028183	425.856367	9.088935
7.379622	429.156172	9.093952
7.048313	429.861043	9.098970
6.762946	418.381113	9.103987
7.057040	423.554834	9.109005
6.915284	429.964006	9.114023
7.178786	429.657973	9.119040
7.112717	425.070547	9.124058
6.866239	423.840420	9.129075
7.157615	417.143016	9.134093
6.938728	425.258779	9.139111
7.248101	416.968126	9.144128
6.755139	425.827115	9.149146
6.971738	426.168981	9.154163
7.244932	429.556704	9.159181
6.850220	432.076479	9.164199
6.940447	422.144294	9.169216
6.973628	431.650321	9.174234
7.101407	428.875613	9.179251
6.971429	418.778909	9.184269
6.779173	425.978543	9.189287
6.890173	427.703247	9.194304
7.063115	427.117839	9.199322
7.034345	421.003583	9.204339
6.629715	431.395089	9.209357
7.052642	424.828672	9.214375
7.131949	429.470974	9.219392
6.880941	439.011786	9.224410
7.156894	446.709703	9.229427
7.454964	451.624049	9.234445
7.359497	447.927933	9.239463
6.942420	430.649479	9.244480
6.841205	440.586671	9.249498
6.817031	449.211745	9.254515
7.171745	443.182935	9.259533
7.300760	455.028171	9.264551
7.293725	447.323229	9.269568
7.373965	442.410076	9.274586
7.485661	443.169044	9.279603
7.592677	449.656249	9.284621
7.261771	452.333342	9.289639
7.315367	441.094098	9.294656
7.154287	439.998989	9.299674
7.718135	441.536428	9.304691
7.443206	430.758576	9.309709
7.243076	429.133087	9.314727
7.318769	428.613311	9.319744
7.086343	434.320269	9.324762
7.099824	428.101608	9.329779
7.266602	426.810294	9.334797
7.151788	433.606573	9.339815
7.356813	441.072546	9.344832
7.109399	449.407345	9.349850
7.279637	445.256470	9.354867
7.516596	450.391759	9.359885
7.095002	448.769193	9.364903
7.513510	457.240144	9.369920
7.204449	455.754683	9.374938
7.257274	459.946703	9.379955
7.250609	459.834205	9.384973
7.250942	463.245484	9.389991
7.417355	458.625008	9.395008
7.336239	471.525404	9.400026
7.586756	455.313733	9.405043
7.741000	453.664624	9.410061
7.192405	460.758815	9.415079
7.476715	459.862590	9.420096
7.345431	467.974199	9.425114
7.732236	463.575016	9.430131
8.022230	456.653761	9.435149
6.841276	440.071716	9.440167
7.110806	446.726112	9.445184
7.497777	452.888878	9.450202
7.262894	459.877423	9.455219
7.445491	451.947303	9.460237
7.131817	467.380026	9.465255
7.816520	458.178890	9.470272
7.673371	456.475102	9.475290
7.762156	455.410514	9.480307
7.700021	456.199703	9.485325
7.638316	452.498329	9.490343
7.362725	437.274260	9.495360
7.636996	437.654482	9.500378
7.159551	453.295719	9.505395
7.407725	451.171261	9.510413
7.521895	455.741873	9.515431
7.600972	456.786773	9.520448
7.618393	451.021905	9.525466
7.543075	449.332803	9.530483
7.765739	452.504346	9.535501
7.323102	455.362929	9.540519
7.674640	447.782031	9.545536
7.493616	453.670331	9.550554
7.655077	445.494209	9.555571
7.688186	447.881107	9.560589
7.459875	448.560475	9.565607
7.808961	454.432508	9.570624
7.693814	448.858686	9.575642
7.970943	457.837620	9.580659
7.917009	444.361979	9.585677
7.138881	440.888911	9.590695
7.729903	441.494358	9.595712
7.776784	451.376942	9.600730
7.490703	453.286543	9.605747
7.625526	452.877474	9.610765
7.805534	457.175917	9.615783
8.061745	453.721676	9.620800
7.488968	444.009465	9.625818
7.620050	440.612577	9.630835
7.972394	441.034290	9.635853
7.786255	435.357922	9.640871
7.443355	432.751165	9.645888
7.457460	439.599954	9.650906
7.431685	442.239004	9.655923
7.798423	453.400318	9.660941
7.593406	457.490477	9.665959
7.814804	453.580931	9.670976
7.596006	458.096094	9.675994
7.569061	452.606363	9.681011
7.800759	451.383831	9.686029
7.431813	457.067873	9.691047
7.656213	454.842979	9.696064
7.575408	450.242063	9.701082
7.670247	448.605359	9.706099
7.334226	448.692456	9.711117
7.351111	456.604274	9.716135
7.938427	467.614495	9.721152
8.207545	469.327207	9.726170
7.672266	469.016158	9.731187
8.055596	451.909696	9.736205
7.524026	464.908621	9.741223
8.062535	469.905452	9.746240
8.099346	468.091597	9.751258
7.649344	464.100400	9.756275
7.610124	463.715273	9.761293
7.686470	473.000017	9.766311
7.976742	477.915585	9.771328
8.156132	484.520917	9.776346
8.285975	476.763094	9.781363
7.678827	472.121051	9.786381
7.863655	466.781372	9.791399
7.352654	468.981602	9.796416
7.961852	470.840171	9.801434
7.675825	481.402580	9.806451
7.960864	482.039890	9.811469
8.052696	483.641358	9.816487
7.778982	484.106900	9.821504
7.760017	484.236147	9.826522
7.564174	482.584741	9.831539
8.030828	481.940979	9.836557
7.809217	480.116867	9.841575
7.821259	475.280593	9.846592
8.125278	484.965376	9.851610
7.971711	486.791236	9.856627
8.190542	482.033211	9.861645
7.867062	484.384119	9.866663
8.121582	488.371180	9.871680
8.163143	483.255765	9.876698
7.970679	488.732467	9.881715
8.391698	486.202414	9.886733
7.956194	485.689647	9.891751
8.291397	478.944372	9.896768
8.152732	480.237760	9.901786
7.780568	485.518388	9.906803
8.218285	475.443712	9.911821
7.994996	484.882407	9.916839
8.044973	480.242187	9.921856
8.295790	475.397137	9.926874
8.060823	484.900763	9.931891
8.386022	477.652142	9.936909
8.323142	487.839000	9.941927
7.921241	487.851152	9.946944
8.254759	485.116981	9.951962
7.933937	487.921891	9.956979
8.126061	479.740978	9.961997
8.455329	478.244489	9.967015
8.303496	477.242608	9.972032
8.226264	485.790758	9.977050
8.353296	481.305790	9.982067
8.049495	487.459359	9.987085
8.160946	485.719084	9.992103
8.128122	483.654150	9.997120
8.410027	483.509345	10.002138
7.999113	486.378772	10.007155
8.185139	479.069772	10.012173
7.839558	482.891502	10.017191
8.171485	485.474865	10.022208
8.500841	475.682136	10.027226
7.931658	488.052647	10.032243
8.373057	487.709449	10.037261
8.269463	489.155160	10.042279
8.156163	485.657463	10.047296
8.332520	477.602077	10.052314
8.090779	483.988968	10.057331
8.712222	485.933992	10.062349
8.497092	493.796747	10.067367
7.915808	488.061970	10.072384
8.229333	481.727150	10.077402
7.982365	492.157257	10.082419
8.255665	500.890667	10.087437
8.289835	512.693906	10.092455
8.278770	512.619961	10.097472
8.403116	504.105623	10.102490
8.525061	517.274224	10.107507
8.933487	506.172189	10.112525
9.009886	506.163517	10.117543
8.565279	499.710055	10.122560
8.500831	489.956542	10.127578
8.416802	491.799976	10.132595
8.281189	481.647311	10.137613
8.131926	481.916761	10.142631
7.961170	489.914610	10.147648
8.489820	495.616695	10.152666
8.498461	502.283331	10.157683
8.660460	511.835614	10.162701
8.527322	507.842407	10.167719
8.106962	497.980209	10.172736
8.484157	497.205214	10.177754
8.876549	514.112188	10.182771
8.357011	500.904648	10.187789
8.451692	502.363669	10.192807
8.187972	500.359928	10.197824
8.590496	499.139197	10.202842
8.546621	505.072429	10.207859
8.935271	508.738824	10.212877
8.879875	508.015403	10.217895
8.787738	495.094757	10.222912
8.971263	480.824758	10.227930
8.494541	483.903237	10.232947
8.490812	484.755914	10.237965
8.331880	480.643658	10.242983
8.450128	480.265570	10.248000
8.549530	486.384763	10.253018
8.526052	498.531468	10.258035
8.752106	495.993901	10.263053
8.478906	498.633614	10.268071
8.503846	508.172523	10.273088
8.481483	505.055122	10.278106
8.765597	513.313505	10.283123
8.601404	515.664862	10.288141
8.718420	503.863463	10.293159
8.636159	508.155417	10.298176
8.976153	499.522303	10.303194
8.803419	506.775732	10.308211
8.701350	517.565129	10.313229
8.701004	507.164182	10.318247
8.501996	509.489402	10.323264
8.767788	509.523823	10.328282
8.732352	511.400717	10.333299
8.429708	518.444014	10.338317
8.547273	506.184956	10.343335
8.423948	514.402640	10.348352
8.619120	504.400423	10.353370
8.549378	515.276300	10.358387
8.768418	511.168301	10.363405
8.867129	502.004733	10.368423
8.506371	503.272744	10.373440
8.695738	505.521717	10.378458
8.555940	509.936234	10.383475
8.490494	511.577970	10.388493
8.852938	519.366589	10.393511
8.845113	526.916228	10.398528
8.765630	524.584011	10.403546
8.872754	534.274233	10.408563
8.952560	528.307131	10.413581
9.291852	527.916716	10.418599
9.015410	523.150589	10.423616
8.768021	503.441027	10.428634
8.657949	512.073194	10.433651
8.976893	514.772187	10.438669
9.206768	507.800315	10.443687
8.834873	510.827765	10.448704
8.652618	504.005264	10.453722
9.210272	516.443337	10.458739
8.814692	515.135437	10.463757
8.894269	502.147027	10.468775
9.044805	518.173363	10.473792
8.837600	519.584717	10.478810
8.944895	527.867482	10.483827
9.105822	531.872281	10.488845
9.008104	523.701764	10.493863
8.944131	539.919301	10.498880
9.127031	533.951924	10.503898
9.035549	540.659408	10.508915
9.287790	529.550119	10.513933
9.286165	514.870283	10.518951
8.628156	509.169534	10.523968
9.004777	518.732584	10.528986
9.163636	523.454039	10.534003
9.109453	511.758182	10.539021
9.117926	505.515028	10.544039
9.265957	514.157501	10.549056
9.041549	513.012290	10.554074
9.186011	512.554384	10.559091
9.118175	508.936000	10.564109
8.910141	503.458670	10.569127
9.013058	524.342680	10.574144
9.233378	533.273695	10.579162
9.574651	537.897328	10.584179
9.144449	532.542939	10.589197
8.913489	511.382359	10.594215
8.978905	521.375700	10.599232
9.306933	530.693869	10.604250
9.290060	531.766335	10.609267
9.124572	523.032038	10.614285
9.137342	516.311706	10.619303
9.247672	537.967715	10.624320
9.189050	538.141005	10.629338
9.121142	536.801020	10.634355
9.493656	543.896991	10.639373
9.772316	529.094611	10.644391
9.191942	521.106535	10.649408
9.312027	508.935442	10.654426
9.010029	506.779877	10.659443
8.904044	515.357763	10.664461
9.647535	528.117188	10.669479
9.310772	522.842924	10.674496
9.218327	525.921537	10.679514
9.290846	530.681683	10.684531
9.023395	535.283332	10.689549
9.335642	531.078769	10.694567
9.294498	541.593619	10.699584
9.071569	534.285155	10.704602
9.061074	536.489513	10.709619
9.174637	538.431570	10.714637
9.598015	532.470932	10.719655
9.267813	529.032243	10.724672
9.175902	535.957533	10.729690
8.949857	536.163202	10.734707
8.534034	536.240634	10.739725
9.242746	546.761808	10.744743
9.349103	563.116941	10.749760
9.956241	562.056844	10.754778
9.666408	563.985975	10.759795
10.014983	557.639360	10.764813
9.695086	537.221557	10.769831
9.547504	545.449343	10.774848
9.503580	542.079683	10.779866
9.753964	542.163838	10.784883
9.566967	548.242440	10.789901
9.794305	540.147532	10.794919
9.614624	540.996049	10.799936
9.607603	541.382202	10.804954
9.431631	539.939126	10.809971
9.628050	541.975576	10.814989
9.552904	536.950896	10.820007
9.508756	535.951180	10.825024
9.505388	537.365511	10.830042
9.862702	537.256301	10.835059
9.795084	535.976228	10.840077
9.865700	531.083483	10.845095
9.598913	535.849123	10.850112
9.812945	528.299067	10.855130
9.865655	543.191994	10.860147
9.189750	536.742973	10.865165
9.533654	529.907967	10.870183
9.563897	541.232175	10.875200
9.679926	548.071448	10.880218
9.935379	535.241815	10.885235
9.622836	535.369436	10.890253
9.786998	537.606559	10.895271
9.673826	525.945122	10.900288
9.554003	531.644047	10.905306
9.459064	536.291417	10.910323
9.427547	533.535182	10.915341
9.658058	534.477618	10.920359
9.615317	538.996946	10.925376
9.854021	534.024383	10.930394
9.864562	526.209378	10.935411
9.806802	543.887025	10.940429
10.019346	532.903830	10.945447
9.760848	539.681497	10.950464
9.741549	529.154105	10.955482
10.060817	526.081336	10.960499
9.523740	526.793002	10.965517
10.034744	529.976469	10.970535
9.557929	536.226417	10.975552
9.136784	526.648335	10.980570
9.805601	531.710098	10.985587
9.716768	534.188574	10.990605
10.229943	527.901544	10.995623
10.213393	530.466591	11.000640
9.836829	525.734986	11.005658
10.007888	531.057276	11.010675
9.892128	530.980697	11.015693
9.951857	530.554918	11.020711
10.050880	523.543455	11.025728
9.745343	538.933949	11.030746
9.942287	517.911857	11.035763
9.861881	532.595137	11.040781
9.504104	529.820276	11.045799
9.793799	530.980704	11.050816
9.504005	533.686120	11.055834
9.878004	548.282885	11.060851
9.966602	552.936396	11.065869
10.317715	555.614609	11.070887
9.751354	559.126761	11.075904
10.036859	559.265406	11.080922
10.497702	562.349395	11.085939
10.108372	548.534592	11.090957
9.817947	537.333071	11.095975
9.288775	541.893424	11.100992
9.991610	557.764380	11.106010
10.126112	555.862726	11.111027
10.061795	566.570538	11.116045
10.044202	566.519699	11.121063
9.963438	568.883318	11.126080
9.928409	563.322232	11.131098
10.030079	553.154673	11.136115
9.812214	572.252082	11.141133
9.867225	565.023403	11.146151
9.988960	570.492234	11.151168
9.868177	562.514630	11.156186
10.253362	554.953693	11.161203
9.774716	576.616248	11.166221
10.173919	569.008943	11.171239
10.473059	583.759398	11.176256
10.125375	578.530997	11.181274
10.463851	571.015194	11.186291
10.318766	562.924613	11.191309
9.899178	554.501251	11.196327
10.520965	564.745648	11.201344
10.076696	576.838007	11.206362
10.370708	564.024439	11.211379
10.164601	571.784843	11.216397
10.688070	569.484970	11.221415
10.358788	556.724273	11.226432
10.273835	556.355731	11.231450
10.339086	550.867394	11.236467
10.298877	558.015007	11.241485
10.306871	555.293641	11.246503
10.100117	555.373235	11.251520
10.331444	574.343908	11.256538
10.150786	567.956617	11.261555
10.064884	582.946894	11.266573
10.101339	584.411832	11.271591
10.538952	588.016973	11.276608
10.413767	588.841230	11.281626
10.944254	585.754498	11.286643
10.579512	578.102037	11.291661
10.405527	589.991383	11.296679
11.061075	578.440589	11.301696
10.578037	574.056895	11.306714
10.600859	556.208076	11.311731
10.269170	559.371280	11.316749
10.450990	558.983292	11.321767
10.274691	557.767474	11.326784
9.673262	560.262649	11.331802
10.459139	564.962228	11.336819
10.501337	576.521272	11.341837
10.455508	577.815991	11.346855
10.533541	576.677334	11.351872
10.201509	587.578313	11.356890
10.543299	583.905604	11.361907
10.116670	584.435981	11.366925
10.560476	578.219693	11.371943
10.898282	584.866667	11.376960
10.595483	589.650551	11.381978
10.735248	583.633071	11.386995
11.042113	579.729125	11.392013
10.592506	582.838111	11.397031
10.728477	577.998292	11.402048
10.647275	587.007836	11.407066
10.780109	579.255815	11.412083
10.826724	574.502489	11.417101
10.267322	583.106823	11.422119
10.762880	586.204345	11.427136
10.560658	586.194875	11.432154
10.862771	579.186482	11.437171
10.860535	581.326447	11.442189
10.683467	576.305002	11.447207
10.750506	584.975897	11.452224
10.416231	588.183688	11.457242
10.683127	577.681133	11.462259
10.682679	590.774174	11.467277
10.437460	587.659900	11.472295
10.695694	579.525451	11.477312
10.335665	585.097697	11.482330
10.844973	580.565808	11.487347
10.420457	580.928605	11.492365
10.862839	590.380473	11.497383
10.906313	595.542774	11.502400
11.270369	604.602918	11.507418
11.035841	590.360053	11.512435
11.023086	585.546543	11.517453
10.712508	579.605492	11.522471
10.966222	582.434568	11.527488
10.672691	581.287491	11.532506
10.793098	576.595257	11.537523
10.511862	576.926278	11.542541
10.738896	597.645888	11.547559
11.046824	602.085389	11.552576
10.999409	604.415420	11.557594
11.246019	595.812577	11.562611
11.149914	595.739249	11.567629
10.883829	609.997085	11.572647
10.973628	604.984573	11.577664
10.980068	610.070596	11.582682
11.222500	595.081306	11.587699
11.126564	592.319314	11.592717
10.692976	590.099023	11.597735
10.855413	592.582564	11.602752
10.929697	606.632774	11.607770
10.994748	605.177412	11.612787
10.879256	600.932138	11.617805
10.898065	607.347932	11.622823
10.952497	604.695064	11.627840
10.756457	602.362050	11.632858
10.887142	605.102991	11.637875
11.060698	598.168254	11.642893
10.985520	610.941599	11.647911
11.294808	601.978713	11.652928
11.255325	603.827846	11.657946
11.056755	606.982954	11.662963
10.988992	597.233054	11.667981
10.833030	605.339101	11.672999
11.225083	603.918030	11.678016
10.970765	607.460499	11.683034
11.250766	617.969572	11.688051
11.791283	623.032404	11.693069
11.256496	612.102403	11.698087
11.279817	608.425627	11.703104
11.422057	608.996816	11.708122
11.122426	607.014433	11.713139
10.975797	601.369728	11.718157
11.239172	622.695911	11.723175
11.410469	624.982425	11.728192
11.182269	616.671241	11.733210
11.308047	619.611756	11.738227
11.619065	629.412289	11.743245
11.198771	632.652415	11.748263
11.546198	624.333651	11.753280
11.167352	620.315561	11.758298
11.304354	620.679292	11.763315
11.539009	622.526768	11.768333
11.385315	628.660170	11.773351
11.773604	619.385186	11.778368
11.465160	608.744982	11.783386
11.001985	601.170950	11.788403
11.693024	609.877242	11.793421
11.285418	614.235656	11.798439
11.396826	619.636685	11.803456
11.533606	631.341979	11.808474
11.742657	622.861731	11.813491
11.471792	604.796668	11.818509
11.339953	612.731711	11.823527
11.500542	615.493243	11.828544
11.338006	617.304734	11.833562
11.551042	624.996746	11.838579
11.873048	626.496120	11.843597
11.535819	625.993293	11.848615
11.449414	624.681426	11.853632
11.454735	624.314606	11.858650
11.490479	623.782110	11.863667
11.576027	633.895451	11.868685
11.402315	638.400483	11.873703
11.556718	636.012902	11.878720
11.613772	637.944834	11.883738
11.485053	631.947050	11.888755
11.694065	632.305881	11.893773
11.415246	641.687035	11.898791
11.448814	629.696582	11.903808
11.868483	629.240004	11.908826
11.693482	636.534862	11.913843
11.505522	636.845051	11.918861
11.233843	636.862173	11.923879
11.615163	636.821805	11.928896
11.653384	634.114655	11.933914
11.446877	635.835167	11.938931
11.541115	639.891398	11.943949
11.562247	654.483233	11.948967
12.010395	647.707687	11.953984
11.634844	658.037995	11.959002
11.913434	658.338658	11.964019
11.906550	650.971263	11.969037
11.623170	661.997252	11.974055
11.779924	653.840701	11.979072
11.947592	652.700706	11.984090
11.730696	657.035748	11.989107
12.124908	654.932707	11.994125
11.898803	655.678009	11.999143
12.170051	651.217880	12.004160
12.037702	658.891101	12.009178
11.882133	663.645771	12.014195
12.018579	644.182393	12.019213
11.802165	657.170258	12.024231
11.993740	654.795821	12.029248
12.046118	657.747771	12.034266
12.106223	652.083485	12.039283
12.049378	655.323829	12.044301
11.982838	657.016240	12.049319
12.065786	657.372609	12.054336
11.910208	659.580637	12.059354
11.878271	662.791859	12.064371
11.963452	650.562990	12.069389
11.771200	657.317764	12.074407
11.822777	654.179358	12.079424
11.764818	652.597983	12.084442
12.143390	653.997037	12.089459
12.532899	643.992886	12.094477
12.008650	661.768526	12.099495
11.934172	653.909899	12.104512
11.867481	660.178083	12.109530
12.015184	660.294005	12.114547
12.088531	656.562094	12.119565
11.920783	657.897891	12.124583
12.034934	656.958725	12.129600
11.847347	661.434367	12.134618
11.816907	663.360990	12.139635
12.586323	672.793542	12.144653
12.289971	668.951938	12.149671
12.433694	657.584920	12.154688
12.498489	650.872215	12.159706
11.975758	656.851654	12.164723
12.524526	653.320268	12.169741
12.232239	656.303790	12.174759
11.935755	659.136494	12.179776
12.163153	663.105728	12.184794
12.489112	672.941828	12.189811
12.417888	666.906679	12.194829
12.202597	659.057351	12.199847
12.313635	658.361658	12.204864
12.690807	652.947796	12.209882
12.307976	659.246268	12.214899
12.265181	657.463723	12.219917
12.354654	660.154286	12.224935
12.374414	670.009657	12.229952
12.792404	669.711124	12.234970
12.514876	662.833971	12.239987
12.421869	652.289582	12.245005
12.588466	654.362244	12.250023
12.077803	662.271087	12.255040
12.607778	664.063121	12.260058
12.430894	665.081616	12.265075
12.926749	668.876515	12.270093
12.349585	654.876286	12.275111
12.320776	655.890660	12.280128
12.569637	662.232787	12.285146
12.437691	678.713488	12.290163
12.564963	674.395686	12.295181
12.777277	689.730928	12.300199
12.644677	685.298956	12.305216
12.743518	676.946291	12.310234
12.322254	666.951601	12.315251
12.543215	676.958679	12.320269
12.928481	684.415626	12.325287
12.676468	684.199320	12.330304
12.530453	676.468582	12.335322
12.753971	687.772258	12.340339
12.586858	681.426998	12.345357
12.663691	676.280790	12.350375
12.569414	681.309933	12.355392
12.682673	672.967648	12.360410
12.774202	675.178229	12.365427
13.139498	678.990302	12.370445
13.115350	677.731852	12.375463
12.553893	669.923793	12.380480
12.782583	658.275312	12.385498
12.830360	678.334985	12.390515
13.037982	678.271171	12.395533
12.960510	660.800767	12.400551
12.648566	660.792601	12.405568
13.035426	659.078855	12.410586
13.065422	666.411233	12.415603
12.849600	654.708891	12.420621
12.717580	659.371534	12.425639
12.784323	660.516193	12.430656
12.931519	654.809946	12.435674
12.936955	663.828130	12.440691
12.619409	651.305370	12.445709
13.165418	674.875485	12.450727
12.676068	669.643868	12.455744
12.833930	666.750834	12.460762
12.701671	685.352215	12.465779
12.857535	686.883773	12.470797
13.219756	685.732419	12.475815
12.942416	681.682731	12.480832
13.167818	672.767584	12.485850
13.085972	680.070046	12.490867
12.968776	679.230013	12.495885
13.290445	671.366502	12.500903
12.815959	672.942555	12.505920
13.098161	682.902234	12.510938
12.786365	680.031830	12.515955
12.632694	685.262720	12.520973
13.001718	674.993507	12.525991
12.994832	677.459243	12.531008
13.165196	676.912097	12.536026
13.152974	681.717034	12.541043
13.093387	674.414637	12.546061
13.117354	680.343677	12.551079
13.244677	683.189292	12.556096
13.088114	678.606423	12.561114
12.806688	677.814049	12.566131
13.195680	678.463583	12.571149
13.253608	677.365918	12.576167
13.029740	691.156514	12.581184
13.098762	695.434426	12.586202
13.508668	704.468549	12.591219
13.446204	693.092587	12.596237
13.516933	692.889145	12.601255
13.491461	693.211904	12.606272
13.312599	673.611401	12.611290
12.807956	685.290370	12.616307
13.025479	691.063050	12.621325
13.347634	696.970914	12.626343
13.269170	701.142408	12.631360
13.441272	694.554986	12.636378
13.426981	708.839966	12.641395
13.819744	698.529176	12.646413
13.643263	702.371959	12.651431
12.993056	704.114225	12.656448
13.481885	700.598473	12.661466
13.245966	710.499986	12.666483
13.125513	708.480226	12.671501
13.090901	708.065975	12.676519
13.284815	702.939399	12.681536
13.387848	706.716574	12.686554
13.425576	703.072248	12.691571
13.433053	704.374455	12.696589
13.522295	708.169556	12.701607
13.424230	711.586736	12.706624
13.803776	705.916878	12.711642
13.642738	717.760113	12.716659
13.634372	705.025081	12.721677
13.684578	700.356367	12.726695
13.341181	711.114029	12.731712
13.526324	710.709743	12.736730
13.953014	725.064928	12.741747
14.068921	722.967343	12.746765
14.031826	715.124958	12.751783
13.704431	709.047632	12.756800
13.925730	701.502682	12.761818
13.658636	702.386907	12.766835
13.674400	695.662886	12.771853
13.294367	693.156542	12.776871
13.666793	709.631325	12.781888
13.723693	710.162158	12.786906
13.856920	717.440617	12.791923
13.985155	726.581720	12.796941
14.156191	710.590469	12.801959
13.626346	708.779612	12.806976
13.626556	698.122855	12.811994
13.783047	700.963931	12.817011
14.069707	714.403668	12.822029
13.931810	713.724640	12.827047
13.722510	705.855425	12.832064
13.865200	712.154142	12.837082
14.085240	725.503277	12.842099
14.247381	720.463691	12.847117
13.927401	704.899176	12.852135
13.856519	700.530172	12.857152
13.832970	711.108652	12.862170
13.939331	722.332764	12.867187
14.028476	723.543365	12.872205
14.338784	720.456179	12.877223
13.956734	718.562351	12.882240
13.844891	699.323758	12.887258
14.106009	717.908106	12.892275
14.094795	728.816024	12.897293
14.418505	717.727048	12.902311
14.017719	713.775466	12.907328
13.962811	712.288281	12.912346
13.888299	717.528945	12.917363
13.980794	722.084067	12.922381
14.492556	712.448995	12.927399
14.054119	719.911131	12.932416
14.010108	722.483637	12.937434
14.091858	730.366543	12.942451
14.210425	724.869851	12.947469
14.339589	717.837841	12.952487
14.296273	725.216371	12.957504
14.335452	726.362170	12.962522
14.330198	724.709468	12.967539
14.245548	726.723431	12.972557
14.471069	721.418365	12.977575
14.300871	723.376221	12.982592
14.408385	720.115489	12.987610
13.993572	723.705059	12.992627
14.374988	730.323208	12.997645
14.410391	724.918357	13.002663
14.669092	723.978772	13.007680
14.504449	722.947314	13.012698
14.555437	723.551649	13.017715
14.446269	724.174609	13.022733
14.505780	727.175951	13.027751
14.424743	729.441808	13.032768
14.452202	718.985916	13.037786
14.686101	724.276391	13.042803
14.237822	718.943694	13.047821
14.588868	726.901431	13.052839
14.290238	720.343111	13.057856
14.367127	722.136269	13.062874
14.657755	721.444168	13.067891
14.392449	725.373368	13.072909
14.323743	727.978120	13.077927
14.638645	726.386021	13.082944
14.652686	727.810280	13.087962
14.361486	727.972447	13.092979
14.297847	733.047327	13.097997
14.658695	725.461706	13.103015
14.455710	728.251461	13.108032
14.181204	723.658543	13.113050
14.598697	726.496854	13.118067
14.074481	735.007423	13.123085
14.818714	735.850950	13.128103
14.534314	746.343836	13.133120
15.024656	750.067030	13.138138
15.071147	743.211978	13.143155
14.843259	733.628941	13.148173
14.866883	720.800557	13.153191
14.626700	727.259874	13.158208
14.887532	728.468989	13.163226
14.545782	731.441291	13.168243
14.805948	731.419787	13.173261
15.014380	732.517144	13.178279
14.863064	739.230863	13.183296
14.693318	740.712140	13.188314
14.815363	740.866770	13.193331
15.017854	751.495284	13.198349
15.116068	746.323637	13.203367
14.808456	740.205351	13.208384
14.999349	741.980761	13.213402
15.119808	749.794535	13.218419
14.887172	745.646357	13.223437
14.943702	735.381584	13.228455
15.095637	734.730011	13.233472
14.928767	744.134813	13.238490
15.434230	741.547397	13.243507
14.875706	738.756423	13.248525
14.813252	718.172101	13.253543
14.863792	724.586151	13.258560
15.142278	743.480237	13.263578
15.249930	745.284385	13.268595
15.151548	748.906743	13.273613
15.334498	739.644733	13.278631
15.232437	738.445745	13.283648
15.168447	736.745384	13.288666
15.389317	728.992214	13.293683
14.936909	727.428066	13.298701
15.148709	738.455897	13.303719
15.183960	740.407013	13.308736
15.136814	746.470220	13.313754
15.032995	743.873528	13.318771
14.898736	744.036506	13.323789
15.607300	743.790558	13.328807
15.665682	746.274544	13.333824
15.251958	752.382204	13.338842
15.127231	746.942320	13.343859
15.226367	742.916051	13.348877
15.007145	744.846830	13.353895
14.954385	746.540259	13.358912
15.171456	748.734458	13.363930
15.112931	744.650688	13.368947
14.908072	752.041758	13.373965
15.295320	743.581044	13.378983
15.544085	753.968833	13.384000
15.698065	761.193587	13.389018
15.536750	748.375043	13.394035
15.123048	760.850919	13.399053
15.707792	759.529218	13.404071
15.484043	756.837592	13.409088
15.571124	757.477333	13.414106
15.857721	760.364431	13.419123
15.565973	755.209317	13.424141
15.437771	748.813794	13.429159
15.414638	756.637305	13.434176
15.490138	761.636882	13.439194
15.893018	765.288492	13.444211
15.702350	761.389389	13.449229
15.726769	749.321387	13.454247
15.818285	747.502142	13.459264
15.450519	750.582636	13.464282
15.593854	751.746933	13.469299
15.809637	752.461307	13.474317
15.883686	761.216401	13.479335
15.821563	746.593128	13.484352
15.439329	745.917429	13.489370
15.893740	751.419724	13.494387
15.772948	753.922140	13.499405
15.742670	752.102924	13.504423
15.596774	754.814369	13.509440
15.455573	757.323119	13.514458
15.552694	762.455025	13.519475
15.453754	776.380866	13.524493
15.984912	763.217818	13.529511
15.914202	770.042071	13.534528
15.662005	768.904326	13.539546
16.250476	763.337616	13.544563
16.230231	771.580393	13.549581
15.930035	770.715200	13.554599
15.692722	762.029836	13.559616
15.502961	770.848099	13.564634
15.861671	767.112760	13.569651
15.750949	769.774552	13.574669
15.879259	768.725881	13.579687
16.213384	760.958219	13.584704
15.839679	762.666907	13.589722
15.912803	766.436129	13.594739
16.066394	769.312380	13.599757
15.712654	768.483925	13.604775
16.064433	782.030336	13.609792
15.976638	790.760151	13.614810
16.395225	790.136486	13.619827
16.272937	796.697388	13.624845
16.290245	787.527413	13.629863
16.766368	778.456416	13.634880
16.136317	776.405541	13.639898
16.216287	757.294806	13.644915
16.273147	760.258697	13.649933
16.625654	760.386913	13.654951
16.324040	762.781788	13.659968
16.050426	760.886851	13.664986
16.395027	759.091315	13.670003
16.382720	759.364690	13.675021
16.207546	758.022455	13.680039
16.638402	759.571163	13.685056
15.975417	752.236453	13.690074
16.093497	749.425336	13.695091
16.224883	775.344871	13.700109
16.282490	775.746212	13.705127
16.531544	771.671350	13.710144
16.258992	781.966758	13.715162
16.454188	779.411865	13.720179
16.402296	788.129778	13.725197
16.275894	786.038355	13.730215
16.654566	782.340929	13.735232
16.626264	782.124503	13.740250
16.399299	783.725142	13.745267
16.418302	783.343566	13.750285
16.486057	778.407019	13.755303
16.509168	782.843575	13.760320
16.481696	786.098304	13.765338
16.407743	787.441596	13.770355
16.647930	784.860764	13.775373
16.321776	786.549427	13.780391
16.357640	780.437609	13.785408
16.325453	785.214124	13.790426
16.450129	796.776249	13.795443
16.670497	806.698289	13.800461
16.423139	813.827765	13.805479
16.752242	808.841052	13.810496
16.933588	816.680089	13.815514
16.964694	817.306457	13.820531
16.624683	821.067432	13.825549
16.905645	815.141497	13.830567
17.082390	808.676383	13.835584
16.587135	820.789468	13.840602
16.980069	811.860790	13.845619
16.949823	810.404470	13.850637
16.869000	810.530728	13.855655
17.108834	809.512026	13.860672
16.590618	811.779690	13.865690
16.865416	806.429058	13.870707
16.946979	806.567901	13.875725
17.020619	806.102081	13.880743
17.461332	805.247758	13.885760
16.976427	816.103253	13.890778
17.167968	811.456684	13.895795
17.173930	799.337874	13.900813
16.935298	792.647113	13.905831
16.974291	796.301738	13.910848
17.135563	798.776023	13.915866
17.251592	801.992634	13.920883
17.190487	795.375214	13.925901
16.855492	793.161637	13.930919
16.994036	792.373295	13.935936
16.891549	795.870073	13.940954
17.492165	803.628046	13.945971
17.535695	803.551911	13.950989
17.083360	806.105954	13.956007
17.552076	803.091918	13.961024
17.195035	804.371993	13.966042
17.410189	792.671885	13.971059
16.998248	784.950946	13.976077
16.907080	795.082425	13.981095
17.426202	798.520290	13.986112
16.806735	810.980901	13.991130
17.259019	808.565853	13.996147
17.616758	802.934072	14.001165
17.508112	806.567506	14.006183
17.754737	795.815522	14.011200
17.266909	806.532615	14.016218
17.358738	804.943683	14.021235
17.520608	798.316792	14.026253
17.353825	813.524978	14.031271
17.407174	802.358126	14.036288
17.510534	800.142568	14.041306
17.424689	799.414408	14.046323
17.560329	804.862213	14.051341
17.381401	802.053151	14.056359
17.442875	804.123264	14.061376
17.235933	809.479245	14.066394
17.174787	800.592870	14.071411
17.206053	805.173325	14.076429
17.426616	818.550850	14.081447
17.968526	819.365925	14.086464
17.734290	831.659277	14.091482
17.515371	824.002940	14.096499
17.822149	827.985098	14.101517
17.834977	824.142658	14.106535
17.668840	827.374804	14.111552
17.666008	826.646341	14.116570
17.632555	826.904076	14.121587
17.978075	826.055106	14.126605
17.690651	827.201271	14.131623
17.961462	830.684114	14.136640
17.863197	826.590734	14.141658
17.802773	826.303572	14.146675
17.769933	824.907614	14.151693
17.778001	831.012744	14.156711
17.834336	829.899538	14.161728
17.802260	825.691714	14.166746
17.872229	830.430247	14.171763
17.849785	825.337321	14.176781
17.710922	835.132276	14.181799
17.561752	828.575891	14.186816
17.955857	824.358516	14.191834
17.649921	836.035047	14.196851
18.077352	832.475182	14.201869
17.609058	829.335638	14.206887
17.724724	836.910362	14.211904
17.988286	851.259491	14.216922
18.274452	853.518682	14.221939
18.517311	853.291595	14.226957
18.265917	858.660823	14.231975
18.171362	840.949912	14.236992
17.829381	833.902851	14.242010
18.156830	845.477617	14.247027
18.460096	851.786095	14.252045
18.299704	856.989680	14.257063
18.413508	847.135636	14.262080
18.261404	847.086804	14.267098
18.234745	841.663180	14.272115
18.415887	833.884592	14.277133
18.078829	834.085457	14.282151
18.289818	842.254396	14.287168
18.289319	846.902922	14.292186
18.401873	844.465026	14.297203
18.609397	847.171951	14.302221
18.662590	848.495452	14.307239
18.355003	837.618298	14.312256
18.271267	841.645482	14.317274
18.589978	861.082525	14.322291
18.517097	847.887232	14.327309
18.704314	856.593196	14.332327
18.713542	835.164467	14.337344
18.467266	824.097899	14.342362
18.252742	830.941411	14.347379
18.677092	834.185760	14.352397
18.623709	847.593337	14.357415
18.460685	848.445587	14.362432
18.912361	848.962295	14.367450
18.558494	852.649697	14.372467
18.487649	850.341338	14.377485
18.368092	852.720502	14.382503
18.768195	852.109180	14.387520
18.502081	848.455328	14.392538
18.490473	858.867939	14.397555
18.623774	849.765076	14.402573
18.522145	848.553391	14.407591
18.647830	850.193801	14.412608
19.162020	846.623581	14.417626
18.741657	860.012567	14.422643
19.203361	845.604294	14.427661
18.965830	845.038601	14.432679
18.996841	846.283507	14.437696
19.077365	852.989574	14.442714
18.838467	848.536242	14.447731
19.084154	851.413946	14.452749
18.835033	846.892780	14.457767
18.790613	850.708723	14.462784
18.723407	850.094421	14.467802
18.717062	849.555848	14.472819
18.760476	856.763143	14.477837
18.789322	851.867347	14.482855
18.676307	853.768978	14.487872
19.064614	866.921612	14.492890
19.046536	875.318730	14.497907
19.035509	877.090879	14.502925
18.937930	881.880758	14.507943
18.998542	878.198120	14.512960
19.349886	883.653389	14.517978
18.842388	889.043566	14.522995
19.095957	876.371768	14.528013
18.984934	874.931176	14.533031
18.954982	882.714779	14.538048
19.063888	878.598598	14.543066
19.025140	880.898914	14.548083
19.154012	878.944455	14.553101
19.040997	887.895990	14.558119
19.133554	879.298062	14.563136
19.703430	897.481084	14.568154
19.297055	889.942265	14.573171
19.509503	886.434796	14.578189
19.604957	889.777700	14.583207
19.419413	875.624807	14.588224
19.428367	873.332422	14.593242
19.712780	878.889626	14.598259
19.505895	881.348661	14.603277
19.807143	869.688745	14.608295
19.145193	864.749024	14.613312
19.344511	877.031709	14.618330
19.224672	879.546617	14.623347
19.635428	886.478985	14.628365
19.841560	898.596525	14.633383
19.431897	889.726499	14.638400
19.909951	893.262293	14.643418
19.581510	889.898996	14.648435
19.914128	886.442244	14.653453
19.689693	886.606640	14.658471
19.400593	880.204564	14.663488
19.692018	880.711510	14.668506
19.615267	894.485669	14.673523
19.857818	892.740722	14.678541
20.079136	895.426573	14.683559
20.163712	900.440554	14.688576
20.011311	891.369531	14.693594
19.747373	876.521959	14.698611
19.776704	872.579111	14.703629
19.779664	877.148213	14.708647
19.883588	877.867385	14.713664
19.991362	877.939033	14.718682
20.122383	894.549401	14.723699
19.911548	871.788458	14.728717
19.842612	876.558098	14.733735
19.804667	896.268454	14.738752
20.201945	902.167847	14.743770
19.762597	900.529068	14.748787
20.322190	899.110290	14.753805
20.482093	903.686521	14.758823
20.017907	886.550654	14.763840
20.247124	878.568907	14.768858
20.015850	894.333143	14.773875
20.392143	890.279468	14.778893
19.751080	881.382359	14.783911
19.682533	898.408802	14.788928
20.338129	894.302172	14.793946
20.350275	894.814733	14.798963
20.282620	899.158155	14.803981
20.247153	899.596080	14.808999
19.902031	897.541853	14.814016
20.171061	894.549425	14.819034
20.310697	899.914587	14.824051
20.459545	901.172708	14.829069
20.424298	894.974093	14.834087
20.277259	904.666220	14.839104
20.421436	893.043367	14.844122
20.411396	894.550282	14.849139
20.745544	897.010287	14.854157
20.459097	905.382933	14.859175
20.137029	901.879790	14.864192
20.437524	901.129344	14.869210
20.432721	907.548922	14.874227
20.552560	897.378337	14.879245
20.226459	900.231468	14.884263
19.947274	897.501115	14.889280
20.104642	890.265835	14.894298
20.307360	917.332624	14.899315
20.652433	908.411350	14.904333
20.703791	908.491782	14.909351
20.835205	908.720692	14.914368
21.126326	907.062854	14.919386
20.765333	924.141165	14.924403
20.685102	920.089135	14.929421
21.054648	917.993061	14.934439
20.932569	916.011400	14.939456
20.816134	908.724069	14.944474
20.861084	918.203279	14.949491
20.871079	912.761303	14.954509
20.853160	910.154368	14.959527
20.988358	917.132807	14.964544
21.235548	914.872750	14.969562
21.352421	900.593859	14.974579
20.873958	889.358278	14.979597
20.907892	886.039545	14.984615
20.799136	892.882392	14.989632
20.856703	892.299154	14.994650
20.759544	901.589047	14.999667
20.933188	911.376412	15.004685
21.159857	913.619629	15.009703
20.923101	911.715782	15.014720
21.128419	906.445363	15.019738
21.390382	912.249065	15.024755
21.299614	910.679086	15.029773
21.537508	905.646588	15.034791
20.963447	906.969926	15.039808
21.378041	901.319796	15.044826
21.068977	913.044200	15.049843
21.217126	906.084897	15.054861
21.178297	905.554536	15.059879
21.197304	904.526031	15.064896
21.285747	910.994207	15.069914
21.039266	911.657486	15.074931
21.208157	906.165526	15.079949
21.117539	909.852978	15.084967
21.042060	907.406481	15.089984
21.085184	903.016520	15.095002
21.222669	906.488579	15.100019
21.064177	908.955862	15.105037
21.324417	922.904788	15.110055
21.545665	927.872252	15.115072
21.728129	917.455226	15.120090
21.639138	931.777262	15.125107
22.075348	929.907487	15.130125
21.813010	914.419019	15.135143
21.594553	915.017977	15.140160
21.265232	912.980222	15.145178
21.604405	917.358134	15.150195
21.508572	926.774063	15.155213
21.931160	915.395020	15.160231
21.741253	930.903546	15.165248
21.932249	927.995843	15.170266
21.919836	920.360960	15.175283
21.744674	901.677948	15.180301
21.565470	901.551287	15.185319
21.700436	900.659359	15.190336
21.992200	923.786562	15.195354
21.611009	927.623398	15.200371
21.644947	928.571215	15.205389
22.082731	928.253818	15.210407
22.301666	942.120829	15.215424
22.118333	928.242100	15.220442
22.027128	914.083955	15.225459
21.561182	915.418862	15.230477
21.995499	919.043520	15.235495
21.780400	928.096174	15.240512
22.041777	926.954195	15.245530
22.111005	932.535452	15.250547
22.290276	939.406054	15.255565
22.418929	935.756991	15.260583
21.837155	944.595350	15.265600
22.311505	932.687540	15.270618
21.946327	930.993030	15.275635
21.927107	927.783549	15.280653
22.066118	932.691236	15.285671
21.972476	939.433920	15.290688
21.741548	943.177937	15.295706
22.052963	930.850537	15.300723
22.266368	935.052380	15.305741
22.188435	936.658230	15.310759
21.943663	941.808706	15.315776
22.046043	944.976976	15.320794
22.610504	956.271921	15.325811
22.043394	962.277304	15.330829
22.665346	960.088279	15.335847
22.446676	967.948638	15.340864
22.640445	952.875108	15.345882
22.735349	958.174670	15.350899
22.546866	956.089737	15.355917
22.573996	950.140162	15.360935
22.803475	964.074975	15.365952
22.748419	953.903187	15.370970
22.802035	950.111173	15.375987
22.391437	940.748971	15.381005
22.631771	947.717364	15.386023
22.688027	953.603599	15.391040
22.734787	950.702571	15.396058
23.312012	949.293668	15.401075
22.306283	936.357156	15.406093
22.544511	948.605430	15.411111
22.711475	956.371030	15.416128
22.610246	951.362917	15.421146
22.516069	952.766175	15.426163
22.776519	956.042377	15.431181
22.733447	949.466273	15.436199
22.667718	956.794741	15.441216
22.641834	949.392312	15.446234
22.738855	945.757639	15.451251
22.459891	960.955015	15.456269
23.287315	961.511053	15.461287
23.026711	962.637271	15.466304
23.040421	957.245195	15.471322
23.130197	958.058090	15.476339
22.905719	959.582619	15.481357
23.354311	965.862200	15.486375
23.208526	964.278692	15.491392
23.122133	952.890511	15.496410
23.398583	947.246095	15.501427
23.211390	950.699288	15.506445
22.814736	943.575490	15.511463
23.113040	966.234681	15.516480
22.995743	973.489136	15.521498
23.412673	969.586903	15.526515
23.508926	967.915218	15.531533
23.655193	964.298120	15.536551
23.413659	953.139217	15.541568
23.142732	959.098485	15.546586
23.730416	958.142379	15.551603
23.581992	954.785756	15.556621
23.717712	944.483286	15.561639
23.033016	942.270489	15.566656
23.169798	942.451228	15.571674
23.391489	949.741255	15.576691
23.533771	965.845017	15.581709
23.591863	966.991043	15.586727
23.346058	969.929511	15.591744
23.294448	965.898261	15.596762
23.500787	957.096391	15.601779
23.510625	968.424048	15.606797
23.589428	968.960947	15.611815
23.885884	964.973333	15.616832
23.768832	970.028194	15.621850
23.888438	965.885081	15.626867
23.385731	975.560040	15.631885
23.835022	964.202054	15.636903
23.975831	968.295290	15.641920
23.954664	957.868920	15.646938
24.199232	964.707275	15.651955
23.753967	966.979378	15.656973
23.976528	958.427442	15.661991
23.928753	955.061459	15.667008
23.970877	968.697249	15.672026
23.964069	954.339743	15.677043
23.647420	954.729932	15.682061
23.733510	952.444461	15.687079
24.058247	952.154133	15.692096
23.805103	956.308702	15.697114
24.027246	956.072216	15.702131
24.129160	964.662129	15.707149
24.157726	960.328069	15.712167
24.094715	961.363564	15.717184
24.145820	958.749031	15.722202
24.563038	961.325497	15.727219
23.872389	961.183792	15.732237
23.679662	964.593669	15.737255
23.961304	986.816832	15.742272
24.161017	991.266968	15.747290
24.275090	988.787792	15.752307
24.181254	988.865584	15.757325
24.325689	995.321917	15.762343
24.348133	987.419651	15.767360
24.046682	995.662134	15.772378
24.321220	985.511594	15.777395
24.324644	991.929921	15.782413
24.129170	993.566700	15.787431
24.490369	987.451493	15.792448
24.846527	994.196748	15.797466
24.706394	997.333359	15.802483
24.535774	996.271258	15.807501
24.244748	998.620335	15.812519
24.405588	1002.824067	15.817536
24.732782	1005.102137	15.822554
25.389099	999.802497	15.827571
24.739469	994.542090	15.832589
24.952111	982.539296	15.837607
24.951667	980.882666	15.842624
24.527910	986.717418	15.847642
24.335213	972.754906	15.852659
24.863160	984.866581	15.857677
24.664004	977.412224	15.862695
25.177590	995.383208	15.867712
24.829760	995.737228	15.872730
25.112241	978.462929	15.877747
25.072760	983.294282	15.882765
24.737531	966.138260	15.887783
24.936613	980.828886	15.892800
24.898580	993.662993	15.897818
25.475622	993.273421	15.902835
25.004993	988.146090	15.907853
24.910566	983.420926	15.912871
24.993744	982.259352	15.917888
25.114245	1003.251637	15.922906
25.287225	997.067903	15.927923
25.086528	1009.147877	15.932941
25.191798	1002.693821	15.937959
25.118672	998.530216	15.942976
25.382537	999.685231	15.947994
25.211343	999.342730	15.953011
25.541483	1004.066048	15.958029
25.480842	989.890461	15.963047
25.464893	1005.138441	15.968064
25.198427	1003.239210	15.973082
25.788250	1001.863054	15.978099
25.339726	1000.815819	15.983117
25.449896	1001.016481	15.988135
25.563917	993.087331	15.993152
25.497302	997.269672	15.998170
25.527739	996.031103	16.003187
25.506746	995.299150	16.008205
25.455656	990.441007	16.013223
25.856755	991.287481	16.018240
25.363998	996.864740	16.023258
25.385673	996.482744	16.028275
25.527993	996.915081	16.033293
25.517259	998.314818	16.038311
25.401971	998.556894	16.043328
25.297381	998.346032	16.048346
25.922017	997.860689	16.053363
25.482704	997.408458	16.058381
25.310460	1002.370937	16.063399
26.147240	1011.165188	16.068416
25.802087	1015.775902	16.073434
25.888049	1019.732524	16.078451
25.848720	1028.319213	16.083469
25.730085	1023.717726	16.088487
25.802897	1026.836967	16.093504
25.495057	1022.422727	16.098522
26.005115	1020.102795	16.103539
26.260910	1030.136207	16.108557
26.094479	1031.377154	16.113575
26.351984	1019.184317	16.118592
26.070115	1033.343963	16.123610
26.252917	1022.260958	16.128627
26.376016	1020.323162	16.133645
26.083821	1025.219118	16.138663
25.845191	1021.280089	16.143680
26.375742	1026.054259	16.148698
26.192082	1028.418181	16.153715
26.185322	1032.127315	16.158733
26.302807	1023.894659	16.163751
26.321354	1012.247108	16.168768
26.397993	1018.609865	16.173786
26.018247	1017.829627	16.178803
26.216065	1025.221230	16.183821
26.431455	1041.916428	16.188839
26.903216	1041.404395	16.193856
26.494489	1033.837479	16.198874
26.437726	1026.651261	16.203891
26.463123	1030.364855	16.208909
26.238745	1040.870659	16.213927
26.602873	1043.007285	16.218944
26.806638	1037.651865	16.223962
26.797277	1048.698544	16.228979
26.619599	1041.449096	16.233997
26.763540	1046.548549	16.239015
26.910461	1045.686310	16.244032
26.948456	1046.213786	16.249050
26.684238	1044.301577	16.254067
26.861897	1046.710230	16.259085
26.340317	1046.677898	16.264103
26.949856	1044.983094	16.269120
26.678120	1046.994663	16.274138
26.863491	1048.083008	16.279155
27.113619	1037.185169	16.284173
26.838874	1043.504816	16.289191
26.860689	1041.775287	16.294208
26.598352	1045.076098	16.299226
26.785550	1035.885856	16.304243
26.969179	1049.433405	16.309261
26.767247	1053.510597	16.314279
26.850155	1049.471007	16.319296
27.402127	1066.754443	16.324314
27.423394	1070.822134	16.329331
27.586426	1059.963087	16.334349
27.201856	1051.732848	16.339367
27.245396	1048.434680	16.344384
27.187643	1043.867889	16.349402
27.182203	1049.852123	16.354419
27.378925	1065.420488	16.359437
27.220305	1069.629793	16.364455
27.793404	1064.106410	16.369472
27.790520	1073.738315	16.374490
27.443463	1051.380198	16.379507
27.697069	1038.869223	16.384525
27.238538	1047.357089	16.389543
27.464886	1043.847426	16.394560
27.571411	1055.399922	16.399578
27.803291	1055.142984	16.404595
27.653898	1063.974041	16.409613
27.672551	1058.953544	16.414631
27.833378	1047.804518	16.419648
27.689058	1058.455656	16.424666
27.314118	1068.786105	16.429683
27.743282	1065.434205	16.434701
27.509474	1060.822239	16.439719
27.722901	1065.633172	16.444736
27.697334	1060.799438	16.449754
27.494537	1053.784266	16.454771
27.830214	1064.534241	16.459789
27.410169	1058.872001	16.464807
28.038910	1051.045720	16.469824
28.087391	1056.245244	16.474842
28.008975	1054.752223	16.479859
27.979040	1048.612687	16.484877
27.625851	1051.766701	16.489895
28.043323	1067.953941	16.494912
28.352531	1076.726225	16.499930
28.385192	1071.896045	16.504947
28.530771	1064.533143	16.509965
27.797683	1057.783568	16.514983
28.329994	1069.093058	16.520000
28.411021	1071.595654	16.525018
28.323416	1073.950938	16.530035
28.518233	1063.629731	16.535053
28.384978	1055.997826	16.540071
28.401435	1053.445477	16.545088
28.311535	1051.629201	16.550106
28.269037	1052.450072	16.555123
28.326142	1053.009286	16.560141
28.209495	1065.155105	16.565159
28.457560	1065.223846	16.570176
28.340314	1076.003321	16.575194
28.352074	1074.512037	16.580211
28.701910	1069.768173	16.585229
28.260058	1077.587591	16.590247
28.560250	1075.546477	16.595264
28.247456	1079.536795	16.600282
28.387019	1076.084818	16.605299
28.600056	1071.633648	16.610317
28.437760	1078.276622	16.615335
28.355300	1073.761007	16.620352
28.542288	1090.637395	16.625370
28.508022	1094.868371	16.630387
28.893180	1091.065731	16.635405
28.816206	1100.579800	16.640423
29.347265	1097.088955	16.645440
29.311338	1090.325496	16.650458
29.065666	1093.623721	16.655475
29.313057	1091.836976	16.660493
29.299532	1099.245737	16.665511
29.024175	1090.329453	16.670528
28.991370	1072.406727	16.675546
28.898720	1086.133018	16.680563
29.350192	1088.603185	16.685581
29.370122	1094.703403	16.690599
29.043035	1087.960031	16.695616
29.091667	1102.257621	16.700634
29.115638	1094.080518	16.705651
28.832930	1089.823292	16.710669
29.166506	1093.883388	16.715687
29.354107	1094.576918	16.720704
29.318450	1091.117505	16.725722
29.281968	1093.155567	16.730739
29.306205	1088.077389	16.735757
29.297689	1094.229372	16.740775
29.017911	1093.086432	16.745792
29.271146	1093.075474	16.750810
29.448857	1110.985262	16.755827
29.759771	1116.778254	16.760845
29.634173	1117.548951	16.765863
29.857437	1119.786413	16.770880
29.715760	1119.164762	16.775898
29.406644	1119.856735	16.780915
29.995884	1107.706862	16.785933
29.705237	1111.630623	16.790951
29.819999	1112.269223	16.795968
29.750975	1112.933283	16.800986
29.349410	1114.535888	16.806003
29.913565	1112.595683	16.811021
29.956698	1121.011789	16.816039
29.730185	1113.984507	16.821056
29.994772	1109.433784	16.826074
29.813127	1107.335145	16.831091
30.235055	1105.218270	16.836109
29.950869	1107.758798	16.841127
29.852031	1104.586928	16.846144
30.130238	1105.705003	16.851162
29.717279	1112.144022	16.856179
29.750327	1102.053105	16.861197
30.098361	1123.997863	16.866215
30.055840	1131.916075	16.871232
30.318862	1132.206548	16.876250
30.258668	1138.287698	16.881267
30.696791	1129.212972	16.886285
30.644487	1126.993208	16.891303
30.714529	1115.997128	16.896320
30.752082	1107.792657	16.901338
30.610335	1110.090105	16.906355
30.635318	1093.262880	16.911373
30.462624	1098.048733	16.916391
30.339698	1098.604421	16.921408
30.547789	1094.005694	16.926426
30.605898	1103.454552	16.931443
30.988847	1098.311054	16.936461
30.465050	1098.203328	16.941479
30.659296	1094.370453	16.946496
30.807619	1090.282800	16.951514
30.258286	1098.936305	16.956531
30.647431	1098.708529	16.961549
30.607554	1100.056007	16.966567
30.463158	1111.070101	16.971584
30.844001	1116.334659	16.976602
31.188444	1121.532303	16.981619
31.407441	1118.415085	16.986637
30.822350	1111.396297	16.991655
30.769801	1095.136557	16.996672
30.531183	1102.914876	17.001690
30.748166	1110.663289	17.006707
31.093416	1111.897157	17.011725
30.889500	1122.283060	17.016743
30.917361	1116.582622	17.021760
31.148715	1118.241318	17.026778
31.021883	1122.761264	17.031795
30.785061	1117.758437	17.036813
30.876932	1117.166695	17.041831
30.954610	1127.010145	17.046848
31.598871	1136.888462	17.051866
31.333616	1151.354882	17.056883
31.118272	1137.585113	17.061901
31.623276	1137.282494	17.066919
31.493726	1145.526683	17.071936
31.648530	1145.360639	17.076954
31.630258	1140.254351	17.081971
31.943075	1133.487070	17.086989
31.398187	1121.491675	17.092007
31.556225	1117.636030	17.097024
31.440472	1114.100722	17.102042
31.539202	1128.425246	17.107059
31.273067	1130.975590	17.112077
31.868002	1132.448293	17.117095
31.534886	1144.163971	17.122112
31.591230	1138.979794	17.127130
31.821889	1142.030298	17.132147
31.846028	1136.936342	17.137165
31.908472	1136.434387	17.142183
31.821180	1136.665794	17.147200
32.069239	1140.388925	17.152218
31.320314	1138.788855	17.157235
31.822146	1139.916296	17.162253
31.810307	1133.695019	17.167271
31.900565	1148.510024	17.172288
32.102140	1155.452976	17.177306
32.136321	1155.062717	17.182323
32.271118	1161.788853	17.187341
32.530533	1154.767949	17.192359
32.087200	1142.024587	17.197376
32.366947	1144.770806	17.202394
32.249076	1151.668820	17.207411
32.530795	1142.990820	17.212429
32.231255	1140.547618	17.217447
31.950574	1137.997339	17.222464
32.299888	1149.269101	17.227482
32.330724	1163.689431	17.232499
32.401356	1163.053657	17.237517
32.314270	1157.528892	17.242535
32.511787	1162.970328	17.247552
32.480177	1166.588685	17.252570
32.486845	1163.741202	17.257587
32.378888	1171.966263	17.262605
32.454674	1159.312477	17.267623
32.680022	1170.849704	17.272640
32.692436	1157.577785	17.277658
32.730225	1155.315588	17.282675
32.449807	1161.424723	17.287693
32.542818	1161.760601	17.292711
32.180443	1164.464788	17.297728
32.868807	1175.469185	17.302746
32.876374	1183.004083	17.307763
33.035721	1194.482174	17.312781
33.361909	1182.133366	17.317799
33.268165	1189.497849	17.322816
33.218780	1173.319596	17.327834
32.920589	1167.534208	17.332851
33.241735	1178.090856	17.337869
33.282178	1170.731656	17.342887
33.015580	1167.579582	17.347904
33.461896	1179.953407	17.352922
33.057936	1169.876843	17.357939
33.267045	1175.641524	17.362957
33.462856	1180.010266	17.367975
33.217256	1184.223673	17.372992
33.191094	1179.295326	17.378010
33.188490	1186.017617	17.383027
33.236019	1183.933779	17.388045
33.185735	1178.955539	17.393063
33.252428	1180.428441	17.398080
33.424735	1177.312171	17.403098
33.447920	1182.888053	17.408115
33.694020	1186.046613	17.413133
33.494262	1187.043452	17.418151
33.313206	1187.819630	17.423168
33.796407	1184.976844	17.428186
33.361333	1188.831591	17.433203
33.488604	1199.715081	17.438221
33.895229	1204.499127	17.443239
33.988138	1212.519365	17.448256
33.999052	1205.881112	17.453274
33.884833	1199.915592	17.458291
33.943575	1201.478095	17.463309
34.211013	1201.707922	17.468327
33.941106	1205.382324	17.473344
34.199510	1193.122956	17.478362
34.312705	1197.753872	17.483379
34.273034	1195.696233	17.488397
34.499667	1186.932115	17.493415
33.997306	1181.756019	17.498432
34.155744	1180.096724	17.503450
34.123683	1177.990565	17.508467
34.107829	1197.751465	17.513485
34.456264	1192.625936	17.518503
34.292664	1201.440338	17.523520
34.332280	1199.155761	17.528538
34.345240	1205.522188	17.533555
34.538231	1202.497367	17.538573
34.641728	1205.154272	17.543591
34.750301	1213.045839	17.548608
34.558524	1201.926369	17.553626
34.361198	1196.560766	17.558643
34.239276	1200.231061	17.563661
34.263866	1195.944899	17.568679
34.326941	1199.097244	17.573696
34.466193	1194.354576	17.578714
34.509455	1201.659863	17.583731
34.160404	1198.650009	17.588749
34.797934	1198.721229	17.593767
34.209384	1208.428613	17.598784
34.594904	1216.321244	17.603802
35.049819	1218.128178	17.608819
34.800599	1221.669975	17.613837
35.103918	1220.660302	17.618855
34.703942	1230.388830	17.623872
35.094126	1218.269874	17.628890
35.042620	1226.419899	17.633907
34.977847	1219.433665	17.638925
35.478213	1209.194189	17.643943
35.366417	1220.178029	17.648960
35.309167	1219.300234	17.653978
35.302551	1213.532550	17.658995
35.390729	1226.741647	17.664013
35.339604	1216.392373	17.669031
35.307220	1225.618700	17.674048
35.263408	1213.037145	17.679066
35.401257	1211.955406	17.684083
35.272348	1217.204686	17.689101
35.211876	1213.581857	17.694119
35.308134	1214.478961	17.699136
35.341248	1218.573243	17.704154
35.624389	1211.763216	17.709171
35.223796	1212.680873	17.714189
35.834875	1227.193949	17.719207
35.848958	1238.151889	17.724224
35.857590	1230.949095	17.729242
35.681312	1224.302111	17.734259
35.718603	1227.095559	17.739277
36.272991	1230.837287	17.744295
36.338381	1223.376351	17.749312
35.991475	1213.294036	17.754330
35.822136	1204.307539	17.759347
35.606456	1211.927701	17.764365
35.736293	1221.740992	17.769383
35.882146	1227.089507	17.774400
36.369066	1222.592501	17.779418
36.537199	1223.557310	17.784435
36.036869	1224.137047	17.789453
36.418890	1229.205797	17.794471
36.482952	1232.736689	17.799488
36.299389	1228.476616	17.804506
36.147716	1220.913778	17.809523
35.720306	1231.012650	17.814541
36.087695	1220.894857	17.819559
35.988705	1227.849920	17.824576
36.242919	1237.224135	17.829594
36.472045	1226.468305	17.834611
35.798550	1237.665841	17.839629
36.689159	1239.329203	17.844647
36.403120	1247.695634	17.849664
36.730255	1251.201350	17.854682
36.849845	1250.737831	17.859699
36.884765	1251.221610	17.864717
36.812375	1242.586072	17.869735
36.495303	1239.078928	17.874752
36.875622	1243.276947	17.879770
37.363109	1236.368824	17.884787
37.063604	1238.753966	17.889805
36.869386	1229.733461	17.894823
36.774353	1234.541972	17.899840
36.968667	1235.714143	17.904858
37.164885	1231.584287	17.909875
37.068081	1225.616047	17.914893
36.531021	1225.930105	17.919911
36.503548	1242.215182	17.924928
36.699123	1247.063658	17.929946
37.045947	1243.244864	17.934963
36.962318	1249.822005	17.939981
37.114190	1248.050117	17.944999
37.009033	1248.104427	17.950016
37.267903	1262.486177	17.955034
37.860400	1266.521780	17.960051
37.322638	1261.824541	17.965069
37.167953	1250.667708	17.970087
37.489733	1258.901640	17.975104
37.505328	1280.939376	17.980122
37.878865	1270.498706	17.985139
37.865039	1281.287449	17.990157
37.808413	1270.184764	17.995175
37.736330	1251.958704	18.000192
37.265520	1246.919687	18.005210
37.356187	1250.664190	18.010227
37.451653	1264.471782	18.015245
37.788872	1268.114786	18.020263
37.625926	1265.785999	18.025280
37.720617	1273.023349	18.030298
38.015216	1259.331879	18.035315
37.745064	1261.349537	18.040333
37.927544	1261.829277	18.045351
37.800916	1267.213916	18.050368
37.729457	1271.034159	18.055386
37.919889	1280.613987	18.060403
38.039060	1299.795400	18.065421
38.192609	1293.816561	18.070439
38.232043	1295.315807	18.075456
38.027053	1299.074794	18.080474
38.537554	1298.925952	18.085491
38.770062	1282.053616	18.090509
39.185330	1278.123173	18.095527
39.108384	1276.033459	18.100544
38.764481	1266.345120	18.105562
38.879866	1244.590101	18.110579
38.591265	1249.738022	18.115597
38.489349	1245.660892	18.120615
38.322369	1248.407253	18.125632
38.225727	1250.022355	18.130650
38.511777	1248.728192	18.135667
38.818308	1268.230694	18.140685
38.948552	1268.046382	18.145703
38.887428	1268.289496	18.150720
38.654961	1272.721785	18.155738
38.920670	1268.088796	18.160755
39.223984	1282.914923	18.165773
38.821431	1271.922899	18.170791
39.260132	1268.995510	18.175808
39.084305	1275.972023	18.180826
39.186991	1280.042864	18.185843
39.111362	1277.883517	18.190861
38.951909	1270.489127	18.195879
38.855284	1275.487245	18.200896
38.887953	1276.627782	18.205914
39.060936	1270.248294	18.210931
38.897928	1262.270638	18.215949
38.772281	1274.667309	18.220967
39.306106	1274.035154	18.225984
39.261433	1289.672858	18.231002
40.160744	1297.043718	18.236019
39.558741	1286.398319	18.241037
38.892375	1284.170000	18.246055
39.123822	1286.090630	18.251072
39.073372	1297.039719	18.256090
39.386063	1294.823066	18.261107
39.516963	1300.593653	18.266125
39.360160	1294.950311	18.271143
39.585501	1293.267965	18.276160
39.509181	1298.259773	18.281178
39.535670	1307.486444	18.286195
39.852350	1316.740523	18.291213
39.743020	1309.751723	18.296231
39.987346	1307.712971	18.301248
40.268006	1322.545813	18.306266
40.379361	1312.912800	18.311283
40.385225	1317.443693	18.316301
40.367578	1315.571959	18.321319
40.571457	1310.872847	18.326336
40.292050	1296.346068	18.331354
40.188197	1282.034965	18.336371
39.636278	1293.456603	18.341389
40.135470	1311.875118	18.346407
40.511390	1316.553523	18.351424
40.550596	1316.159322	18.356442
40.738964	1312.990035	18.361459
40.435806	1318.184423	18.366477
40.164195	1311.359745	18.371495
40.678366	1314.782704	18.376512
40.643512	1317.833552	18.381530
40.172933	1314.239839	18.386547
40.516998	1319.371329	18.391565
40.870486	1307.368478	18.396583
40.681309	1319.244896	18.401600
40.109666	1311.558059	18.406618
40.197331	1318.531433	18.411635
41.036362	1328.082887	18.416653
40.769310	1337.995906	18.421671
41.256503	1338.746943	18.426688
41.103234	1338.426891	18.431706
41.298890	1336.496698	18.436723
41.277452	1334.941134	18.441741
41.073726	1339.157526	18.446759
41.458775	1330.709501	18.451776
41.083632	1330.067387	18.456794
41.504912	1333.141894	18.461811
41.249767	1338.259385	18.466829
41.185978	1339.556955	18.471847
41.424087	1333.501821	18.476864
41.370203	1337.855829	18.481882
41.135735	1338.589836	18.486899
40.988795	1338.862091	18.491917
41.151144	1334.093699	18.496935
41.570754	1321.916442	18.501952
41.298374	1332.868549	18.506970
41.404674	1324.157813	18.511987
41.236431	1337.116582	18.517005
41.388938	1340.706308	18.522023
41.523636	1348.713790	18.527040
41.776702	1353.559655	18.532058
41.693251	1346.954976	18.537075
41.982020	1347.071031	18.542093
41.560110	1352.555318	18.547111
41.769471	1346.510967	18.552128
41.822296	1357.986814	18.557146
41.984026	1372.409024	18.562163
42.083508	1370.282362	18.567181
41.867907	1378.158203	18.572199
42.020105	1373.817416	18.577216
42.101356	1371.396946	18.582234
41.983623	1373.946309	18.587251
42.376485	1368.040639	18.592269
42.139007	1367.525413	18.597287
42.674625	1369.095736	18.602304
42.553219	1378.563221	18.607322
42.389464	1367.799048	18.612339
42.715031	1366.552372	18.617357
42.590289	1375.212487	18.622375
42.576672	1359.937371	18.627392
42.647386	1368.333521	18.632410
42.585523	1370.053673	18.637427
42.658404	1370.481052	18.642445
42.700528	1372.588959	18.647463
42.847716	1365.446589	18.652480
42.752929	1372.536755	18.657498
42.552324	1363.028025	18.662515
42.698295	1361.525288	18.667533
42.938283	1376.077329	18.672551
42.969177	1382.478897	18.677568
43.265394	1395.485315	18.682586
43.226743	1393.307573	18.687603
43.619015	1393.287592	18.692621
43.060779	1383.986011	18.697639
43.239005	1371.401332	18.702656
42.903324	1385.216185	18.707674
43.205880	1379.987293	18.712691
43.310816	1391.530787	18.717709
43.151031	1389.280387	18.722727
43.473323	1380.911537	18.727744
43.899880	1382.205350	18.732762
43.704246	1383.693866	18.737779
44.027950	1383.400537	18.742797
43.399235	1393.458258	18.747815
43.433956	1376.604003	18.752832
43.334972	1392.729938	18.757850
43.439277	1388.011594	18.762867
43.980709	1390.568785	18.767885
43.404595	1393.940604	18.772903
43.858999	1385.914102	18.777920
43.855481	1392.967975	18.782938
44.051826	1406.548531	18.787955
44.167063	1404.542489	18.792973
43.786705	1403.847535	18.797991
44.072258	1397.794460	18.803008
44.274683	1398.144865	18.808026
44.132819	1404.503911	18.813043
44.376019	1401.947768	18.818061
44.100418	1397.749321	18.823079
44.633804	1394.390602	18.828096
44.331828	1399.559583	18.833114
44.308762	1407.885146	18.838131
44.416740	1402.446699	18.843149
44.285734	1403.114107	18.848167
44.635018	1401.030600	18.853184
44.534530	1406.269199	18.858202
44.240400	1404.295335	18.863219
44.550244	1394.539856	18.868237
44.408392	1411.130075	18.873255
44.427633	1398.311352	18.878272
45.018347	1414.718090	18.883290
44.686879	1426.938628	18.888307
45.200747	1420.947828	18.893325
45.055081	1431.914980	18.898343
44.890949	1430.236456	18.903360
45.060653	1431.279928	18.908378
45.124333	1429.382896	18.913395
45.183906	1428.862445	18.918413
44.887790	1425.942140	18.923431
44.979762	1419.392174	18.928448
45.104236	1419.641107	18.933466
45.054537	1428.232759	18.938483
45.723217	1412.662018	18.943501
45.190632	1423.638913	18.948519
45.302639	1416.341054	18.953536
45.195849	1417.941973	18.958554
45.102449	1426.316364	18.963571
45.352865	1421.300706	18.968589
45.144781	1434.436163	18.973607
45.712430	1434.149034	18.978624
45.761785	1440.601398	18.983642
45.689498	1444.147249	18.988659
45.619617	1440.317553	18.993677
45.657514	1442.116855	18.998695
45.607386	1453.914908	19.003712
45.478333	1448.112562	19.008730
45.446027	1440.938148	19.013747
45.812347	1432.780171	19.018765
45.724948	1445.606510	19.023783
46.221327	1460.065052	19.028800
46.356055	1460.754205	19.033818
46.010713	1466.952448	19.038835
46.674856	1469.225455	19.043853
46.632948	1463.087640	19.048871
46.590319	1450.272202	19.053888
46.409254	1439.715809	19.058906
46.227914	1443.811974	19.063923
46.138065	1441.664288	19.068941
46.295939	1458.889544	19.073959
46.568835	1458.496827	19.078976
46.722426	1458.643396	19.083994
46.151668	1466.460962	19.089011
46.675209	1464.426057	19.094029
46.572002	1465.698215	19.099047
46.887545	1459.511060	19.104064
47.279451	1454.681649	19.109082
46.756464	1471.457498	19.114099
46.911339	1463.695349	19.119117
46.346595	1466.749828	19.124135
46.844395	1466.189549	19.129152
46.807942	1475.000069	19.134170
47.029435	1479.749898	19.139187
47.462152	1470.448621	19.144205
47.915514	1466.019897	19.149223
47.861461	1453.398741	19.154240
47.684700	1449.191205	19.159258
47.611224	1451.052029	19.164275
47.529469	1445.750408	19.169293
47.275437	1447.771888	19.174311
47.279942	1438.565701	19.179328
47.504894	1432.124415	19.184346
47.106820	1455.094625	19.189363
46.951276	1451.836847	19.194381
47.435524	1466.843241	19.199399
47.490699	1471.486418	19.204416
47.993028	1470.209059	19.209434
47.679424	1478.961745	19.214451
47.714769	1471.120372	19.219469
47.554087	1480.486729	19.224487
48.084466	1474.827859	19.229504
47.953969	1473.832066	19.234522
47.367173	1476.747967	19.239539
47.746897	1486.667667	19.244557
48.013045	1491.438949	19.249575
48.150498	1493.945443	19.254592
48.394136	1488.602614	19.259610
47.947897	1495.274172	19.264627
47.862702	1496.638203	19.269645
47.925656	1494.485655	19.274663
48.074776	1491.824225	19.279680
48.630204	1502.745382	19.284698
48.333346	1522.455717	19.289715
48.966516	1506.334995	19.294733
49.071875	1511.910809	19.299751
48.823279	1496.643758	19.304768
49.219607	1491.741064	19.309786
48.703845	1479.952332	19.314803
48.835857	1482.440736	19.319821
48.966074	1488.094724	19.324839
48.604211	1478.172378	19.329856
48.712942	1474.011906	19.334874
48.690262	1487.973767	19.339891
49.311123	1504.808244	19.344909
48.995871	1504.671200	19.349927
49.067285	1501.627387	19.354944
49.296884	1504.062731	19.359962
49.085005	1507.043342	19.364979
49.535053	1500.914127	19.369997
49.201392	1502.332623	19.375015
49.271567	1509.248834	19.380032
49.544789	1500.944373	19.385050
49.303349	1505.772597	19.390067
49.522335	1503.573664	19.395085
49.359691	1501.049136	19.400103
49.139326	1494.500434	19.405120
49.380024	1498.887512	19.410138
49.616165	1530.125207	19.415155
49.752175	1530.176683	19.420173
50.005313	1536.398535	19.425191
50.119888	1528.671035	19.430208
49.884649	1532.207560	19.435226
49.773128	1538.350488	19.440243
49.981919	1536.882138	19.445261
49.923496	1533.000145	19.450279
50.009658	1538.288618	19.455296
50.416896	1532.513201	19.460314
50.130446	1536.105038	19.465331
50.476949	1529.985623	19.470349
50.529266	1529.232766	19.475367
49.833435	1536.277719	19.480384
50.076890	1536.432388	19.485402
49.862266	1539.132562	19.490419
50.462405	1550.829437	19.495437
50.384646	1555.057825	19.500455
50.458366	1560.439762	19.505472
50.741966	1557.242981	19.510490
50.698279	1557.653800	19.515507
50.839372	1562.927416	19.520525
50.819022	1551.500166	19.525543
50.586741	1557.027576	19.530560
50.926434	1559.827644	19.535578
50.658778	1561.945933	19.540595
51.028891	1561.396064	19.545613
51.163391	1562.760610	19.550631
50.758191	1569.406870	19.555648
51.214541	1568.849886	19.560666
51.117164	1579.828546	19.565683
51.123332	1573.708455	19.570701
51.137665	1576.262532	19.575719
51.221475	1581.339942	19.580736
51.606329	1569.903242	19.585754
51.236603	1579.116002	19.590771
51.473815	1580.221556	19.595789
51.464826	1569.152293	19.600807
51.489217	1572.534793	19.605824
51.548733	1573.626987	19.610842
51.542158	1579.100327	19.615859
51.895212	1583.179594	19.620877
51.732561	1585.578188	19.625895
51.801351	1595.265489	19.630912
52.272980	1587.021618	19.635930
52.128498	1599.459317	19.640947
51.727233	1589.041262	19.645965
52.396070	1586.238940	19.650983
52.216580	1587.693400	19.656000
52.576705	1579.769855	19.661018
52.348344	1582.582628	19.666035
52.218982	1575.678895	19.671053
52.552451	1581.743087	19.676071
52.283001	1586.162277	19.681088
52.626499	1577.726917	19.686106
52.657909	1583.954905	19.691123
52.489364	1590.018364	19.696141
52.496403	1579.164354	19.701159
52.547050	1578.547456	19.706176
52.748661	1577.768198	19.711194
52.674206	1583.293134	19.716211
52.575142	1586.745351	19.721229
52.444562	1581.208290	19.726247
52.054044	1584.772157	19.731264
53.027503	1583.951622	19.736282
53.019619	1600.593744	19.741299
53.021739	1597.440781	19.746317
53.448817	1596.664288	19.751335
53.325938	1603.721048	19.756352
53.516655	1601.008944	19.761370
53.533151	1597.314091	19.766387
53.696195	1585.833019	19.771405
53.348020	1572.452828	19.776423
53.519686	1581.341453	19.781440
53.418581	1584.812923	19.786458
53.522918	1587.094208	19.791475
53.655571	1587.026285	19.796493
53.691442	1587.112288	19.801511
54.035091	1600.603785	19.806528
53.684397	1596.107708	19.811546
53.735551	1587.638963	19.816563
53.781618	1595.114392	19.821581
53.978783	1593.183937	19.826599
53.911436	1597.316039	19.831616
54.080349	1587.989502	19.836634
54.220775	1603.150530	19.841651
54.229964	1593.126167	19.846669
54.077894	1592.525052	19.851687
54.017734	1588.053172	19.856704
53.994624	1585.992909	19.861722
54.120474	1579.869961	19.866739
54.008516	1597.781158	19.871757
54.261989	1615.098981	19.876775
54.021112	1623.490114	19.881792
54.228264	1613.980882	19.886810
54.653717	1614.539569	19.891827
54.338423	1624.513908	19.896845
54.724585	1620.303895	19.901863
54.804366	1631.731540	19.906880
54.713131	1642.179097	19.911898
54.846811	1636.638746	19.916915
55.053077	1638.522309	19.921933
54.702163	1628.263652	19.926951
54.535764	1642.857092	19.931968
55.024168	1636.125401	19.936986
55.207006	1632.931672	19.942003
55.045623	1631.934367	19.947021
54.969628	1626.432976	19.952039
55.135898	1634.148486	19.957056
54.966133	1647.991359	19.962074
55.333326	1653.084630	19.967091
55.295851	1652.610841	19.972109
55.467815	1656.633112	19.977127
55.452995	1659.147558	19.982144
55.476970	1653.318163	19.987162
55.978230	1650.586104	19.992179
55.613823	1657.481671	19.997197
55.792551	1652.890529	20.002215
55.662555	1646.823171	20.007232
55.543746	1649.369585	20.012250
55.871544	1666.145700	20.017267
55.784799	1674.664342	20.022285
56.208210	1674.611111	20.027303
56.186080	1670.587734	20.032320
56.751375	1674.861201	20.037338
56.919753	1671.524546	20.042355
56.473182	1664.073707	20.047373
56.618584	1654.327909	20.052391
56.678523	1649.234545	20.057408
56.770446	1638.518764	20.062426
56.579434	1637.791164	20.067443
56.155831	1640.186212	20.072461
56.442385	1640.075392	20.077479
56.471857	1661.720112	20.082496
56.417792	1665.361001	20.087514
56.464974	1658.852635	20.092531
56.545727	1666.843412	20.097549
56.865351	1673.471536	20.102567
56.637320	1664.285657	20.107584
57.130922	1682.004825	20.112602
57.434769	1694.543205	20.117619
56.961022	1681.387615	20.122637
57.293406	1691.134916	20.127655
57.203804	1693.825115	20.132672
57.214855	1688.196541	20.137690
57.437092	1692.766426	20.142707
57.438780	1697.102402	20.147725
57.634392	1685.246958	20.152743
57.158263	1702.287132	20.157760
57.130829	1700.751405	20.162778
57.189876	1697.229791	20.167795
57.325855	1705.903123	20.172813
57.748380	1716.176058	20.177831
57.678967	1727.857372	20.182848
57.586319	1715.693330	20.187866
57.726724	1719.363914	20.192883
57.654562	1721.795776	20.197901
58.000215	1722.104954	20.202919
58.031823	1729.648964	20.207936
58.512976	1742.992925	20.212954
58.536647	1740.123767	20.217971
58.554827	1733.916542	20.222989
58.434600	1718.136997	20.228007
58.490155	1720.744638	20.233024
57.995521	1728.200163	20.238042
58.396915	1734.146532	20.243059
58.258217	1738.640078	20.248077
58.525946	1733.867796	20.253095
58.358230	1736.768984	20.258112
58.974795	1739.604870	20.263130
58.905793	1739.562031	20.268147
58.430270	1736.363486	20.273165
59.267741	1742.140975	20.278183
59.042486	1732.954629	20.283200
58.982847	1726.368194	20.288218
59.538525	1734.076769	20.293235
59.113852	1739.239704	20.298253
58.938203	1737.701803	20.303271
59.097908	1743.594284	20.308288
59.479171	1748.773757	20.313306
59.574967	1746.130059	20.318323
59.541757	1754.649872	20.323341
59.338505	1739.713232	20.328359
59.567059	1741.268280	20.333376
59.823119	1739.748372	20.338394
60.123783	1735.365448	20.343411
59.920205	1740.099475	20.348429
60.029546	1734.089500	20.353447
59.846422	1741.944666	20.358464
60.006863	1744.226704	20.363482
60.010281	1738.050179	20.368499
59.704334	1744.488542	20.373517
60.095382	1742.496326	20.378535
59.935593	1731.037020	20.383552
60.091386	1736.844900	20.388570
60.097840	1738.488177	20.393587
60.090579	1734.648668	20.398605
59.918281	1744.146362	20.403623
59.933926	1753.482253	20.408640
60.361351	1765.079925	20.413658
60.766622	1761.788423	20.418675
60.531484	1767.448890	20.423693
60.493594	1770.793785	20.428711
60.767181	1770.340992	20.433728
60.865104	1771.566078	20.438746
60.469063	1773.745407	20.443763
60.560009	1780.803661	20.448781
60.860712	1788.312111	20.453799
61.183182	1794.605313	20.458816
60.863061	1791.985338	20.463834
61.178483	1789.720861	20.468851
61.315293	1792.890234	20.473869
60.995590	1784.946208	20.478887
61.320323	1797.613956	20.483904
61.550406	1804.237135	20.488922
62.005356	1796.273483	20.493939
61.605887	1800.387911	20.498957
61.911460	1794.312650	20.503975
61.334827	1783.442089	20.508992
61.798078	1795.633822	20.514010
62.268473	1798.243160	20.519027
61.987997	1808.871761	20.524045
62.202960	1808.762619	20.529063
61.976540	1792.283155	20.534080
62.506998	1793.595537	20.539098
62.133279	1785.748286	20.544115
62.053023	1797.740611	20.549133
62.049354	1813.432351	20.554151
62.374301	1811.996389	20.559168
62.078512	1816.063119	20.564186
62.289108	1801.607964	20.569203
62.318627	1809.909747	20.574221
62.479769	1814.429214	20.579239
62.484094	1807.722334	20.584256
62.217529	1817.884858	20.589274
62.727271	1816.391721	20.594291
62.702315	1834.475807	20.599309
62.618279	1833.296029	20.604327
62.791288	1822.845232	20.609344
62.928906	1834.232443	20.614362
63.054464	1824.003634	20.619379
63.005614	1842.429129	20.624397
63.079046	1838.779012	20.629415
63.000994	1835.676360	20.634432
62.758857	1835.878234	20.639450
63.183486	1837.267059	20.644467
63.403201	1853.731966	20.649485
63.690152	1856.909533	20.654503
63.688798	1852.583070	20.659520
63.550424	1856.205566	20.664538
63.954974	1852.017885	20.669555
63.837495	1845.269992	20.674573
63.793535	1849.426913	20.679591
64.238052	1845.239322	20.684608
63.575167	1852.547519	20.689626
64.124437	1849.160997	20.694643
64.042544	1854.592498	20.699661
63.913679	1844.327548	20.704679
64.030519	1848.115440	20.709696
63.619098	1849.839568	20.714714
63.791682	1837.675174	20.719731
64.355902	1858.675126	20.724749
64.089562	1861.544350	20.729767
64.062245	1866.610740	20.734784
64.050840	1874.051051	20.739802
64.218349	1871.396170	20.744819
64.420856	1876.328948	20.749837
64.803682	1889.732511	20.754855
64.965751	1886.844938	20.759872
64.962524	1891.178570	20.764890
65.160744	1887.802514	20.769907
65.059214	1889.977030	20.774925
65.146250	1897.805981	20.779943
65.016025	1903.295516	20.784960
64.752921	1894.989166	20.789978
65.245433	1893.344066	20.794995
64.901246	1892.463573	20.800013
65.180429	1884.678732	20.805031
65.418150	1901.257647	20.810048
65.396140	1915.374378	20.815066
65.704931	1913.562214	20.820083
65.637078	1909.719478	20.825101
65.824856	1912.054088	20.830119
65.882394	1912.837331	20.835136
65.799019	1917.600029	20.840154
65.758016	1915.842325	20.845171
66.010079	1914.209413	20.850189
66.113456	1916.714960	20.855207
66.110040	1913.092572	20.860224
65.929559	1917.359130	20.865242
66.189213	1913.156123	20.870259
65.921851	1916.139128	20.875277
66.169761	1933.073105	20.880295
67.028460	1933.652716	20.885312
66.780801	1938.478868	20.890330
66.472112	1931.142153	20.895347
66.798076	1927.474792	20.900365
67.049671	1929.133570	20.905383
67.075611	1932.626354	20.910400
66.872673	1937.136263	20.915418
67.091899	1941.978090	20.920435
66.930129	1930.193906	20.925453
66.754354	1930.388604	20.930471
66.970243	1933.141733	20.935488
66.789696	1937.966904	20.940506
67.149662	1932.337579	20.945523
67.065198	1931.369308	20.950541
67.557530	1937.364706	20.955559
67.436057	1940.094619	20.960576
67.362395	1948.084315	20.965594
67.269634	1954.303362	20.970611
67.751901	1939.821577	20.975629
67.199916	1950.363142	20.980647
67.718643	1950.162523	20.985664
67.528982	1954.190669	20.990682
67.561151	1946.081329	20.995699
67.579789	1953.280302	21.000717
67.640892	1966.383706	21.005735
68.133437	1961.481684	21.010752
68.113727	1967.364302	21.015770
68.208939	1955.423322	21.020787
68.238352	1964.154398	21.025805
68.333627	1964.698230	21.030823
68.050658	1960.847948	21.035840
68.022607	1959.258644	21.040858
68.435626	1974.914054	21.045875
68.462703	1987.034967	21.050893
68.737927	1985.682475	21.055911
69.191342	1972.057256	21.060928
68.927257	1984.936739	21.065946
68.830662	1982.793193	21.070963
69.077400	1975.789721	21.075981
69.310127	1991.037698	21.080999
69.142590	1977.319798	21.086016
68.910206	1984.504215	21.091034
69.306349	1981.337177	21.096051
69.207062	1976.669312	21.101069
69.092030	1978.056960	21.106087
69.334020	1979.909751	21.111104
69.189424	1989.343299	21.116122
69.509308	2001.478597	21.121139
69.453685	2009.295092	21.126157
69.487333	2011.265533	21.131175
69.778142	2003.112742	21.136192
69.699369	2002.727428	21.141210
69.773761	2001.223159	21.146227
70.260746	2007.667555	21.151245
70.435143	2020.529289	21.156263
70.544833	2005.710968	21.161280
70.148370	2001.212446	21.166298
70.203675	2012.663081	21.171315
70.695220	2011.911249	21.176333
70.582932	2014.863815	21.181351
70.846984	2015.343500	21.186368
70.659922	2010.105445	21.191386
70.850462	2003.719807	21.196403
70.934669	2006.525008	21.201421
70.676112	2012.833008	21.206439
71.018306	2009.847940	21.211456
70.982813	2006.899584	21.216474
70.833924	2009.100424	21.221491
70.668733	2013.127930	21.226509
71.000520	2012.363101	21.231527
70.935234	2010.864799	21.236544
71.052989	2009.199138	21.241562
71.098698	2029.153353	21.246579
71.614693	2028.239917	21.251597
71.537788	2035.444331	21.256615
72.023258	2029.110598	21.261632
71.793230	2036.278890	21.266650
71.755130	2048.804484	21.271667
71.948648	2036.677723	21.276685
71.561418	2039.357506	21.281703
71.953625	2040.012907	21.286720
71.924575	2027.384296	21.291738
71.907149	2029.552047	21.296755
72.058804	2028.695337	21.301773
71.674038	2032.858023	21.306791
72.395564	2046.006991	21.311808
72.158234	2059.870170	21.316826
72.277273	2064.399411	21.321843
72.442980	2057.455863	21.326861
72.169382	2059.856014	21.331879
72.334119	2053.354450	21.336896
72.657617	2056.990286	21.341914
72.634633	2054.885766	21.346931
72.757164	2051.149063	21.351949
72.631805	2065.493451	21.356967
73.103527	2070.630531	21.361984
73.420647	2077.833577	21.367002
73.202860	2078.470338	21.372019
73.266855	2078.741321	21.377037
73.217252	2084.347753	21.382055
73.126741	2070.459992	21.387072
72.908791	2077.194055	21.392090
73.123092	2082.282851	21.397107
72.965761	2069.730989	21.402125
73.121805	2090.021559	21.407143
73.383381	2100.161978	21.412160
73.641046	2103.804917	21.417178
73.462810	2111.687886	21.422195
73.841175	2121.226284	21.427213
73.819992	2122.785533	21.432231
74.023510	2133.196953	21.437248
74.099205	2128.662759	21.442266
73.703569	2128.481416	21.447283
74.410278	2119.553731	21.452301
74.314211	2128.105600	21.457319
74.503381	2116.986210	21.462336
74.596996	2121.497333	21.467354
74.630668	2126.841492	21.472371
74.909400	2139.652353	21.477389
74.783042	2145.731523	21.482407
75.183062	2145.520981	21.487424
75.101835	2140.421052	21.492442
74.784906	2145.049751	21.497459
75.200060	2143.852195	21.502477
74.954580	2139.809835	21.507495
75.196831	2140.513835	21.512512
75.264129	2135.463370	21.517530
75.505423	2144.066868	21.522547
75.622150	2138.689955	21.527565
75.615577	2142.449785	21.532583
75.606426	2136.615922	21.537600
75.616828	2122.671382	21.542618
75.589390	2141.870215	21.547635
75.422448	2131.437451	21.552653
75.536835	2154.038423	21.557671
76.127988	2152.450530	21.562688
76.294473	2157.849764	21.567706
76.052948	2162.353113	21.572723
76.544886	2155.929963	21.577741
76.428357	2159.022074	21.582759
76.299644	2161.046214	21.587776
76.448727	2166.621737	21.592794
76.369489	2163.743286	21.597811
76.677651	2160.444740	21.602829
76.377161	2156.770721	21.607847
76.481328	2164.332020	21.612864
76.753198	2166.076032	21.617882
77.102820	2180.747367	21.622899
77.042406	2175.697838	21.627917
76.955496	2179.612203	21.632935
76.645070	2186.830943	21.637952
77.242946	2182.063949	21.642970
77.034128	2182.708784	21.647987
77.237259	2183.213739	21.653005
77.051580	2188.664656	21.658023
76.998044	2188.029243	21.663040
77.152973	2196.876598	21.668058
77.494139	2213.925716	21.673075
77.406810	2199.226277	21.678093
77.253991	2199.660413	21.683111
77.683083	2205.864573	21.688128
77.909853	2209.752198	21.693146
77.999778	2224.211525	21.698163
78.367991	2223.718741	21.703181
78.163880	2226.275361	21.708199
78.198631	2229.249252	21.713216
78.300742	2225.963840	21.718234
78.149694	2231.403066	21.723251
78.599149	2215.054679	21.728269
78.669999	2218.931866	21.733287
78.416812	2218.538986	21.738304
78.655645	2218.820622	21.743322
78.266844	2214.140963	21.748339
78.634663	2221.064761	21.753357
78.810047	2236.242976	21.758375
79.089194	2238.402449	21.763392
79.626594	2232.982104	21.768410
78.996070	2238.088863	21.773427
79.298208	2228.892737	21.778445
79.431094	2237.371139	21.783463
79.384830	2228.816267	21.788480
79.320953	2220.860619	21.793498
78.967154	2233.596449	21.798515
79.665074	2245.278559	21.803533
79.497764	2246.475541	21.808551
79.405659	2256.929904	21.813568
79.590725	2251.248812	21.818586
79.406100	2259.716696	21.823603
79.923882	2260.403050	21.828621
80.178932	2264.163201	21.833639
79.885223	2282.182279	21.838656
80.231065	2278.347642	21.843674
80.284426	2276.164934	21.848691
80.112558	2267.026808	21.853709
80.824190	2277.368671	21.858727
80.629479	2283.777284	21.863744
81.218705	2278.380416	21.868762
80.896153	2284.401812	21.873779
80.991071	2285.671584	21.878797
81.170794	2286.192811	21.883815
81.221083	2293.787802	21.888832
80.919227	2294.112593	21.893850
81.192601	2298.419039	21.898867
81.320727	2290.985762	21.903885
81.559686	2299.785369	21.908903
81.258317	2296.357624	21.913920
81.425772	2288.069267	21.918938
81.329868	2295.645992	21.923955
81.325237	2290.392076	21.928973
81.670085	2302.015579	21.933991
81.545628	2313.046244	21.939008
81.793361	2317.337751	21.944026
82.041845	2321.411379	21.949043
82.185474	2321.445892	21.954061
82.492772	2323.957619	21.959079
82.352705	2322.818093	21.964096
82.082306	2319.432861	21.969114
82.183925	2312.218309	21.974131
82.060937	2321.595017	21.979149
82.414068	2321.357058	21.984167
82.596142	2323.591619	21.989184
82.935564	2327.048296	21.994202
82.636320	2333.473202	21.999219
82.870687	2329.229851	22.004237
83.134108	2322.883248	22.009255
83.399248	2320.579195	22.014272
83.578211	2317.707858	22.019290
83.428443	2321.433213	22.024307
83.408274	2317.756544	22.029325
83.865065	2319.465468	22.034343
83.617189	2316.985653	22.039360
83.831354	2315.743635	22.044378
83.582503	2328.680956	22.049395
83.451397	2314.748829	22.054413
83.537519	2317.796793	22.059431
83.642462	2329.798512	22.064448
83.745268	2322.564835	22.069466
83.529441	2324.173342	22.074483
84.145667	2335.331714	22.079501
84.050902	2348.535409	22.084519
83.840694	2344.891478	22.089536
83.854182	2345.293413	22.094554
84.377433	2353.875205	22.099571
84.598914	2356.599125	22.104589
84.548007	2362.884385	22.109607
84.436410	2374.698928	22.114624
84.884796	2371.204933	22.119642
84.214014	2375.781479	22.124659
84.423643	2373.353511	22.129677
84.655360	2382.110102	22.134695
84.860684	2388.506965	22.139712
85.065487	2391.242955	22.144730
85.001754	2398.385500	22.149747
85.096068	2399.800551	22.154765
85.744582	2399.614438	22.159783
85.744740	2402.095096	22.164800
86.035853	2407.490782	22.169818
86.076198	2411.464284	22.174835
86.190594	2407.984409	22.179853
86.107818	2404.689878	22.184871
86.089668	2408.943902	22.189888
86.525215	2400.784178	22.194906
86.540484	2411.518578	22.199923
86.700808	2392.706025	22.204941
86.613958	2381.528453	22.209959
86.194974	2386.523419	22.214976
86.260814	2384.821622	22.219994
86.559786	2402.502378	22.225011
86.535707	2405.147766	22.230029
86.866989	2392.194536	22.235047
86.562112	2403.461643	22.240064
86.640888	2400.255576	22.245082
86.527219	2410.868030	22.250099
86.467751	2422.945905	22.255117
86.404873	2428.163167	22.260135
86.527736	2440.026462	22.265152
87.448355	2445.841735	22.270170
87.840190	2448.801095	22.275187
87.671346	2457.111970	22.280205
87.844845	2452.780231	22.285223
87.896061	2455.319223	22.290240
88.070110	2450.526622	22.295258
88.034615	2449.926262	22.300275
88.166029	2452.171883	22.305293
88.435119	2442.835617	22.310311
88.264787	2450.490272	22.315328
88.071344	2447.506471	22.320346
88.160515	2444.888950	22.325363
88.089305	2448.813553	22.330381
88.584836	2458.138217	22.335399
88.371373	2475.529574	22.340416
88.799390	2477.949940	22.345434
88.452190	2476.170421	22.350451
88.292334	2474.200779	22.355469
88.761617	2466.338749	22.360487
88.728117	2469.443234	22.365504
89.129213	2478.896228	22.370522
88.894319	2496.609699	22.375539
88.858877	2493.124733	22.380557
89.304973	2495.087821	22.385575
89.438111	2495.168152	22.390592
89.388090	2496.047068	22.395610
89.134270	2491.333696	22.400627
89.308769	2511.508254	22.405645
89.712740	2512.433260	22.410663
89.978941	2514.225529	22.415680
90.031372	2515.404097	22.420698
90.014027	2513.345986	22.425715
89.884967	2511.557749	22.430733
90.323190	2516.444537	22.435751
90.429084	2538.523418	22.440768
90.554773	2548.161349	22.445786
90.893523	2534.607209	22.450803
91.110393	2540.797188	22.455821
91.139302	2535.367553	22.460839
90.839448	2535.076612	22.465856
90.946971	2528.889917	22.470874
91.276796	2529.551894	22.475891
91.285177	2529.481225	22.480909
91.287258	2527.902959	22.485927
91.026138	2534.577638	22.490944
91.143678	2522.036315	22.495962
91.618623	2524.241084	22.500979
91.113643	2526.137641	22.505997
91.635065	2527.517765	22.511015
91.361503	2546.035779	22.516032
91.697018	2542.376275	22.521050
91.798444	2562.063615	22.526067
91.389647	2555.853150	22.531085
91.919225	2552.037188	22.536103
91.810588	2566.685508	22.541120
92.155108	2568.957929	22.546138
92.560442	2569.308329	22.551155
92.517375	2567.819145	22.556173
92.638150	2566.124559	22.561191
92.708324	2559.179910	22.566208
92.415721	2563.407269	22.571226
92.711168	2576.398890	22.576243
92.454600	2581.662133	22.581261
92.845326	2583.012113	22.586279
92.873691	2580.167338	22.591296
92.769895	2583.210199	22.596314
93.280001	2593.122842	22.601331
93.337308	2603.147017	22.606349
93.554766	2603.892769	22.611367
93.474037	2610.820277	22.616384
93.640370	2613.133071	22.621402
93.892771	2604.058114	22.626419
94.035339	2608.798441	22.631437
93.771553	2604.768294	22.636455
93.955167	2602.874559	22.641472
93.733627	2615.457513	22.646490
94.312435	2624.564157	22.651507
94.080250	2634.283100	22.656525
94.567918	2626.231932	22.661543
94.698439	2633.265425	22.666560
94.532354	2630.703399	22.671578
94.307510	2632.152379	22.676595
94.486422	2633.251298	22.681613
94.897320	2649.415753	22.686631
95.184666	2651.043786	22.691648
95.154347	2653.128406	22.696666
95.244090	2651.722687	22.701683
95.504458	2644.675805	22.706701
95.198761	2648.147772	22.711719
95.216371	2647.362400	22.716736
95.240012	2658.026211	22.721754
95.138185	2651.143023	22.726771
94.983839	2658.877335	22.731789
95.977350	2662.639371	22.736807
95.730619	2673.228512	22.741824
95.984601	2682.161679	22.746842
95.820548	2683.014173	22.751859
95.971831	2678.663746	22.756877
96.047432	2680.321593	22.761895
96.098528	2686.524808	22.766912
95.902414	2697.203920	22.771930
96.433498	2695.745265	22.776947
96.333729	2705.478347	22.781965
96.513682	2714.331530	22.786983
96.630773	2720.224656	22.792000
96.864893	2725.701902	22.797018
96.958501	2721.698142	22.802035
96.856920	2732.277343	22.807053
97.076841	2744.349808	22.812071
97.379518	2742.683694	22.817088
97.764365	2750.255195	22.822106
97.689566	2738.264417	22.827123
97.923323	2745.111454	22.832141
97.752262	2742.663805	22.837159
97.680678	2749.466857	22.842176
98.037754	2736.695571	22.847194
98.264641	2740.182475	22.852211
98.182553	2742.341443	22.857229
98.129978	2739.985809	22.862247
98.192324	2743.570920	22.867264
98.434173	2755.185506	22.872282
98.310126	2756.612490	22.877299
98.881005	2766.853467	22.882317
98.416978	2755.854316	22.887335
98.625560	2761.748992	22.892352
98.642421	2764.384903	22.897370
99.051187	2772.861636	22.902387
98.874464	2779.169786	22.907405
99.038167	2773.072099	22.912423
99.130991	2775.768774	22.917440
99.367733	2784.559496	22.922458
99.554809	2796.488775	22.927475
99.593841	2803.520799	22.932493
99.939951	2808.412541	22.937511
99.886585	2810.630167	22.942528
99.907212	2804.879820	22.947546
99.923839	2802.639646	22.952563
100.124422	2806.793433	22.957581
99.932676	2801.675806	22.962599
100.299945	2810.209514	22.967616
100.377511	2823.544531	22.972634
100.870046	2830.588017	22.977651
100.651297	2832.446353	22.982669
100.553615	2830.306031	22.987687
100.237684	2831.999601	22.992704
100.497794	2832.533577	22.997722
100.891507	2832.860544	23.002739
100.902819	2852.581170	23.007757
100.748736	2860.634291	23.012775
101.150258	2858.384682	23.017792
101.256860	2857.897897	23.022810
101.713875	2860.525259	23.027827
101.207615	2877.328219	23.032845
101.648834	2876.918735	23.037863
102.193544	2880.946371	23.042880
101.869883	2882.060431	23.047898
102.126877	2872.586958	23.052915
101.760892	2876.690103	23.057933
102.147651	2874.897267	23.062951
102.718787	2862.629098	23.067968
102.346892	2874.916880	23.072986
102.205736	2872.290972	23.078003
102.542450	2876.104816	23.083021
102.759178	2887.306796	23.088039
102.750445	2892.607289	23.093056
102.829210	2892.642435	23.098074
102.931341	2889.770346	23.103091
103.005863	2894.445597	23.108109
102.988995	2894.423043	23.113127
103.287530	2892.293615	23.118144
103.324651	2901.440551	23.123162
103.351271	2906.577740	23.128179
103.472609	2912.536547	23.133197
103.461628	2914.848581	23.138215
103.632297	2912.783244	23.143232
103.969199	2921.782523	23.148250
103.702213	2931.819498	23.153267
104.138941	2940.402420	23.158285
103.994649	2937.205738	23.163303
104.074152	2942.180055	23.168320
104.386339	2952.726526	23.173338
104.379293	2950.802473	23.178355
104.429914	2954.540945	23.183373
104.456091	2957.999175	23.188391
104.781937	2954.909191	23.193408
104.732755	2980.181479	23.198426
104.785705	2985.889002	23.203443
105.017705	2982.800999	23.208461
105.178949	2979.919692	23.213479
105.597819	2984.250993	23.218496
105.165518	2998.909027	23.223514
105.743733	2989.603252	23.228531
105.854464	3002.242053	23.233549
105.913255	3002.466519	23.238567
106.150096	2988.416616	23.243584
105.785948	3001.441805	23.248602
106.048500	2989.840191	23.253619
106.335744	3003.250005	23.258637
106.317666	3021.466773	23.263655
106.615258	3013.751169	23.268672
106.680781	3011.629601	23.273690
106.775647	3003.623641	23.278707
106.890366	3010.211576	23.283725
106.979163	3008.998499	23.288743
106.839011	3002.648212	23.293760
107.170851	3012.592000	23.298778
107.271526	3025.462778	23.303795
107.424612	3036.337056	23.308813
107.332825	3030.096006	23.313831
107.478947	3027.321197	23.318848
107.503840	3042.113231	23.323866
107.957429	3035.591589	23.328883
107.843485	3036.253244	23.333901
107.593215	3053.250064	23.338919
108.398353	3052.938567	23.343936
108.454911	3059.983743	23.348954
108.409978	3060.508410	23.353971
108.332929	3056.430150	23.358989
108.477031	3061.972011	23.364007
108.519146	3057.925696	23.369024
108.288693	3060.300324	23.374042
107.989648	3059.406429	23.379059
108.517045	3074.581047	23.384077
108.601523	3077.733548	23.389095
108.892185	3083.031670	23.394112
108.755772	3102.762944	23.399130
109.171706	3110.414974	23.404147
109.356789	3106.895554	23.409165
109.301589	3102.087974	23.414183
109.342226	3105.272554	23.419200
109.507943	3120.389901	23.424218
110.135974	3122.217426	23.429235
110.306901	3128.626222	23.434253
110.293645	3122.019427	23.439271
110.133041	3121.081882	23.444288
110.283070	3130.378630	23.449306
110.404773	3125.139518	23.454323
110.619961	3129.180641	23.459341
110.422874	3138.783928	23.464359
110.655838	3148.531724	23.469376
110.640601	3147.385333	23.474394
110.839893	3145.593253	23.479411
111.242636	3140.086295	23.484429
111.262138	3156.255335	23.489447
111.538124	3156.281869	23.494464
111.796542	3163.652300	23.499482
111.802246	3167.227378	23.504499
111.812089	3159.102029	23.509517
111.893597	3169.694012	23.514535
112.350220	3163.537964	23.519552
112.160265	3164.432386	23.524570
112.105143	3166.520928	23.529587
112.277965	3168.716006	23.534605
111.959535	3155.699265	23.539623
112.281686	3169.861239	23.544640
112.704946	3178.269629	23.549658
112.715700	3193.335417	23.554675
113.091908	3184.042057	23.559693
112.807887	3182.801797	23.564711
112.788182	3184.389313	23.569728
112.864022	3191.352635	23.574746
112.951008	3193.340151	23.579763
112.994379	3193.412370	23.584781
112.794086	3205.361201	23.589799
113.959001	3200.855991	23.594816
113.883197	3215.019993	23.599834
114.157632	3226.064861	23.604851
114.202883	3222.163204	23.609869
114.529554	3215.961091	23.614887
114.696663	3221.035467	23.619904
114.717591	3216.181286	23.624922
114.519452	3215.694596	23.629939
114.942258	3207.703767	23.634957
114.755103	3223.516836	23.639975
114.827277	3217.291223	23.644992
114.699677	3214.899865	23.650010
114.653056	3222.005355	23.655027
114.980969	3224.009019	23.660045
114.884829	3230.528867	23.665063
115.026341	3234.420521	23.670080
114.907633	3243.531926	23.675098
115.414909	3239.769793	23.680115
115.518740	3244.841403	23.685133
115.486604	3256.325383	23.690151
115.897547	3252.183727	23.695168
115.813736	3251.575083	23.700186
115.670535	3264.136825	23.705203
116.162531	3262.504312	23.710221
116.181516	3275.646792	23.715239
116.339352	3276.395543	23.720256
116.261360	3284.885180	23.725274
116.681318	3283.667868	23.730291
116.181109	3279.096801	23.735309
116.638723	3291.501898	23.740327
117.095404	3304.920275	23.745344
116.857475	3300.418833	23.750362
117.031678	3298.576989	23.755379
117.513731	3293.108136	23.760397
117.032487	3312.173724	23.765415
117.318555	3311.933572	23.770432
117.539635	3315.109033	23.775450
117.654685	3328.104036	23.780467
118.045609	3326.168481	23.785485
117.980529	3327.646296	23.790503
118.335417	3335.143806	23.795520
118.434009	3345.565956	23.800538
118.122250	3335.221317	23.805555
118.616656	3341.822851	23.810573
118.391640	3338.001120	23.815591
118.592444	3347.312169	23.820608
118.792494	3360.694795	23.825626
118.998365	3362.436577	23.830643
119.035432	3365.713288	23.835661
118.924370	3365.301408	23.840679
119.590139	3362.477205	23.845696
119.775968	3384.636210	23.850714
119.453094	3389.035751	23.855731
119.818137	3388.843270	23.860749
119.665021	3393.863397	23.865767
119.917019	3389.083660	23.870784
120.048464	3387.674548	23.875802
120.204362	3397.008395	23.880819
120.493741	3402.130065	23.885837
120.370431	3418.728722	23.890855
120.281311	3420.181882	23.895872
120.570960	3410.652544	23.900890
120.513111	3422.039635	23.905907
120.751180	3432.291779	23.910925
120.988452	3444.352546	23.915943
121.251087	3445.880346	23.920960
121.377416	3447.864921	23.925978
120.673073	3446.191406	23.930995
121.119538	3462.316340	23.936013
121.081548	3463.916196	23.941031
121.378265	3471.037765	23.946048
121.851691	3483.484719	23.951066
122.104590	3491.446352	23.956083
122.358710	3485.208100	23.961101
122.022112	3486.261085	23.966119
122.354269	3482.368358	23.971136
122.695930	3496.025719	23.976154
123.004333	3503.726220	23.981171
123.171204	3496.892403	23.986189
122.933433	3495.692263	23.991207
123.368003	3495.425832	23.996224
123.506268	3492.996201	24.001242
123.290577	3496.596345	24.006259
123.861348	3494.377120	24.011277
123.765985	3499.549251	24.016295
123.697517	3489.412827	24.021312
123.621050	3488.219136	24.026330
123.553407	3495.886652	24.031347
124.122409	3511.746369	24.036365
124.392218	3517.107834	24.041383
124.329847	3506.749517	24.046400
124.441572	3514.215524	24.051418
124.358492	3522.826001	24.056435
124.475850	3517.101397	24.061453
124.078407	3522.891837	24.066471
124.623539	3538.389175	24.071488
125.088969	3543.969531	24.076506
124.464216	3552.841103	24.081523
125.305515	3540.000173	24.086541
125.223273	3547.575298	24.091559
125.477686	3565.986908	24.096576
125.411388	3564.977845	24.101594
125.372280	3563.895112	24.106611
126.000708	3560.114051	24.111629
125.733695	3564.157755	24.116647
125.965901	3576.314085	24.121664
126.527990	3582.709486	24.126682
126.136049	3585.611161	24.131699
126.488830	3587.519464	24.136717
126.481130	3592.674817	24.141735
126.161146	3588.277608	24.146752
126.777314	3595.766110	24.151770
126.701846	3604.331254	24.156787
127.124091	3609.063021	24.161805
126.950910	3615.503472	24.166823
127.446984	3620.312122	24.171840
127.527992	3630.421553	24.176858
127.330722	3632.232439	24.181875
127.355967	3636.278000	24.186893
127.742323	3639.670816	24.191911
127.751337	3655.867186	24.196928
127.724714	3647.343299	24.201946
128.029502	3658.229053	24.206963
128.498014	3660.012035	24.211981
128.224939	3678.739446	24.216999
128.354212	3676.983465	24.222016
129.016152	3676.324979	24.227034
128.568443	3682.353700	24.232051
128.966693	3688.474806	24.237069
129.401215	3707.145736	24.242087
129.486366	3711.750108	24.247104
129.377877	3700.407805	24.252122
129.516736	3705.991712	24.257139
129.532471	3709.388587	24.262157
129.975200	3709.938347	24.267175
130.122166	3718.124885	24.272192
130.397293	3720.562914	24.277210
130.483071	3729.046200	24.282227
130.290265	3723.846411	24.287245
130.209701	3722.075752	24.292263
130.437474	3721.516424	24.297280
131.001847	3729.786323	24.302298
130.543841	3748.062851	24.307315
130.824474	3747.615229	24.312333
130.868990	3749.893480	24.317351
131.134719	3746.544442	24.322368
131.163471	3757.047141	24.327386
131.526075	3768.192241	24.332403
131.584200	3760.144322	24.337421
131.423866	3771.885307	24.342439
131.492496	3773.613778	24.347456
131.554849	3789.820902	24.352474
131.523154	3784.599169	24.357491
132.297171	3802.261000	24.362509
132.871174	3797.266898	24.367527
132.825812	3803.128860	24.372544
133.074109	3800.012933	24.377562
133.391982	3802.703130	24.382579
133.593046	3798.057466	24.387597
133.590911	3799.137302	24.392615
133.661226	3790.869691	24.397632
133.520669	3770.322424	24.402650
133.653621	3777.466455	24.407667
134.030137	3778.970242	24.412685
133.874688	3788.419047	24.417703
133.553287	3790.467056	24.422720
133.635270	3790.934108	24.427738
133.510923	3785.859362	24.432755
133.622752	3803.176105	24.437773
133.747840	3814.288775	24.442791
133.794551	3820.089064	24.447808
134.400624	3829.858047	24.452826
134.375228	3845.816915	24.457843
134.498914	3847.120195	24.462861
134.715146	3867.513872	24.467879
135.024993	3872.152740	24.472896
135.284742	3861.103348	24.477914
135.355540	3872.824195	24.482931
135.372780	3878.985749	24.487949
135.678954	3887.122326	24.492967
135.678083	3886.317684	24.497984
135.959740	3885.762586	24.503002
135.836861	3909.605242	24.508019
136.154766	3917.373880	24.513037
136.580940	3905.307484	24.518055
137.201364	3914.401995	24.523072
136.869791	3911.123828	24.528090
136.833552	3915.415744	24.533107
137.148007	3903.575056	24.538125
137.237316	3914.409295	24.543143
137.372159	3928.250684	24.548160
137.786010	3921.381411	24.553178
137.706795	3926.099804	24.558195
137.651669	3925.401451	24.563213
137.835876	3922.405950	24.568231
137.744598	3923.455484	24.573248
137.960453	3940.336379	24.578266
138.058667	3949.395430	24.583283
137.969774	3952.303637	24.588301
138.350404	3954.576928	24.593319
138.152820	3966.828843	24.598336
138.577917	3972.106298	24.603354
138.070481	3985.296535	24.608371
138.669692	3984.442649	24.613389
139.473229	3989.948411	24.618407
138.853895	3990.025966	24.623424
139.887217	4001.003660	24.628442
139.819108	4015.365937	24.633459
139.934980	4019.902480	24.638477
140.376894	4006.949807	24.643495
140.162954	4014.706602	24.648512
140.211979	4012.461234	24.653530
140.274884	4016.024418	24.658547
140.688451	4017.860179	24.663565
140.633886	4017.963431	24.668583
139.840482	4039.041591	24.673600
140.692272	4040.417748	24.678618
140.691703	4043.713067	24.683635
140.992965	4057.415020	24.688653
141.001328	4064.654314	24.693671
141.006435	4062.583061	24.698688
141.370599	4081.549399	24.703706
141.841258	4088.940824	24.708723
142.106112	4092.289517	24.713741
141.910927	4094.390503	24.718759
142.119603	4095.061936	24.723776
142.300393	4092.066939	24.728794
142.017750	4101.239019	24.733811
142.282096	4115.868402	24.738829
142.643106	4123.829265	24.743847
142.925246	4122.541824	24.748864
142.908915	4117.162944	24.753882
142.560652	4123.510894	24.758899
142.664867	4137.253055	24.763917
143.362976	4146.247213	24.768935
143.194583	4152.491419	24.773952
143.620747	4161.644707	24.778970
143.701577	4168.276218	24.783987
143.924576	4169.598779	24.789005
143.992273	4161.656506	24.794023
143.671166	4174.413864	24.799040
143.916682	4192.496087	24.804058
144.013996	4198.231806	24.809075
144.638287	4209.689944	24.814093
144.875528	4208.403175	24.819111
144.637227	4228.094728	24.824128
144.981161	4220.825907	24.829146
145.056299	4228.364188	24.834163
144.999265	4239.817951	24.839181
145.584288	4242.154147	24.844199
145.607935	4251.111330	24.849216
145.704668	4250.313570	24.854234
145.731588	4265.769120	24.859251
146.006816	4263.561099	24.864269
146.328069	4258.252715	24.869287
146.781785	4268.765300	24.874304
146.865249	4277.400708	24.879322
146.904566	4284.098694	24.884339
147.102766	4288.628799	24.889357
147.081205	4272.752739	24.894375
147.104766	4282.098180	24.899392
146.988755	4279.149362	24.904410
146.939543	4296.766251	24.909427
147.577593	4297.831666	24.914445
147.542887	4303.543784	24.919463
147.622529	4309.560047	24.924480
148.087650	4321.431267	24.929498
148.112920	4326.928893	24.934515
148.415394	4320.913239	24.939533
148.614923	4325.566243	24.944551
148.975493	4339.136079	24.949568
149.061438	4341.101790	24.954586
149.241925	4345.568384	24.959603
149.195363	4344.414169	24.964621
149.346714	4334.025259	24.969639
149.115129	4337.706952	24.974656
149.379085	4345.010724	24.979674
149.637646	4356.475395	24.984691
149.649717	4363.998302	24.989709
150.076773	4363.698312	24.994727
150.266405	4375.962813	24.999744
150.461138	4384.012806	25.004762
150.429655	4390.333625	25.009779
150.361032	4393.743762	25.014797
150.693477	4388.944926	25.019815
150.736506	4399.553091	25.024832
150.917342	4406.317468	25.029850
151.050142	4418.492999	25.034867
150.990349	4421.134773	25.039885
151.462445	4419.284314	25.044903
151.408761	4441.996393	25.049920
151.649129	4432.761420	25.054938
151.666189	4437.790061	25.059955
151.953743	4463.974689	25.064973
152.373053	4458.865612	25.069991
152.376912	4465.704910	25.075008
152.645964	4463.680896	25.080026
152.686265	4461.357921	25.085043
152.782404	4475.439327	25.090061
152.744501	4481.982122	25.095079
152.971805	4487.120080	25.100096
153.095017	4481.053373	25.105114
153.495753	4496.419358	25.110131
153.282305	4504.444576	25.115149
153.229107	4502.234000	25.120167
153.373982	4504.802890	25.125184
153.666885	4522.436174	25.130202
153.993452	4530.045910	25.135219
153.770646	4544.385346	25.140237
154.533281	4553.776835	25.145255
154.316970	4564.747424	25.150272
154.763915	4565.744763	25.155290
154.789133	4574.771302	25.160307
154.940701	4585.340583	25.165325
154.957003	4584.400668	25.170343
155.100046	4591.278315	25.175360
155.439682	4606.754909	25.180378
155.992641	4600.365588	25.185395
155.871719	4610.222932	25.190413
156.158511	4609.720674	25.195431
156.186227	4618.027190	25.200448
156.391650	4634.859856	25.205466
156.594945	4623.231702	25.210483
156.679814	4635.266491	25.215501
156.595019	4628.250483	25.220519
156.614077	4648.101277	25.225536
156.601203	4653.980551	25.230554
157.019120	4659.587592	25.235571
156.982391	4672.335744	25.240589
157.341399	4664.685631	25.245607
157.947411	4691.193462	25.250624
158.093201	4704.553969	25.255642
157.978912	4698.363190	25.260659
158.329311	4697.456476	25.265677
158.504123	4709.868705	25.270695
158.748007	4717.355667	25.275712
158.982903	4718.654323	25.280730
159.300599	4719.649699	25.285747
158.919354	4716.846264	25.290765
159.274026	4714.881490	25.295783
159.445899	4728.042256	25.300800
159.756809	4734.698125	25.305818
160.229842	4738.074500	25.310835
160.238271	4745.396122	25.315853
160.494183	4732.039464	25.320871
160.236139	4740.286365	25.325888
160.004274	4742.579363	25.330906
160.914214	4750.792777	25.335923
160.556664	4764.102280	25.340941
161.023821	4755.712473	25.345959
160.925758	4758.335004	25.350976
160.755617	4759.065441	25.355994
161.468395	4770.929964	25.361011
161.444060	4780.485129	25.366029
161.859050	4774.862141	25.371047
162.131352	4789.244631	25.376064
162.067005	4792.007112	25.381082
162.272548	4803.480322	25.386099
162.172138	4808.871405	25.391117
162.313503	4807.353321	25.396135
162.782886	4797.728988	25.401152
162.572397	4825.904469	25.406170
162.812619	4826.826689	25.411187
163.045110	4823.110172	25.416205
163.080779	4823.638122	25.421223
163.215127	4824.182273	25.426240
163.344706	4847.308226	25.431258
163.660103	4844.361591	25.436275
163.661976	4853.890619	25.441293
163.857284	4854.617823	25.446311
164.201466	4871.085055	25.451328
164.058823	4882.246377	25.456346
164.154772	4869.350111	25.461363
164.273033	4884.747778	25.466381
164.706415	4892.391540	25.471399
165.111603	4895.052527	25.476416
164.931900	4899.714219	25.481434
165.275460	4910.373744	25.486451
165.246171	4924.061532	25.491469
165.556023	4914.676614	25.496487
165.714681	4937.170023	25.501504
165.996905	4942.198554	25.506522
166.433795	4947.966867	25.511539
166.247507	4949.331114	25.516557
166.362060	4955.253775	25.521575
166.735522	4959.573689	25.526592
166.784691	4966.677576	25.531610
167.018184	4968.879213	25.536627
166.946283	4979.047925	25.541645
167.104903	4985.797039	25.546663
167.342897	4986.053604	25.551680
167.305626	4998.170779	25.556698
167.771116	5001.488405	25.561715
167.703334	5010.902102	25.566733
167.636362	5024.684214	25.571751
168.464351	5034.564501	25.576768
168.350925	5043.312996	25.581786
168.589917	5040.507640	25.586803
168.922209	5055.752184	25.591821
168.792147	5060.778652	25.596839
168.974949	5060.437770	25.601856
169.213081	5072.398484	25.606874
169.405641	5084.407336	25.611891
169.663638	5092.779224	25.616909
169.813213	5094.741424	25.621927
170.548278	5106.365963	25.626944
170.073141	5121.723645	25.631962
169.921441	5119.982862	25.636979
170.479642	5132.919639	25.641997
170.385549	5135.503728	25.647015
170.627296	5140.879516	25.652032
170.788078	5154.430566	25.657050
171.249173	5160.567643	25.662067
171.075179	5172.191714	25.667085
171.531246	5176.625079	25.672103
171.954248	5181.110939	25.677120
171.788711	5191.644719	25.682138
172.452586	5193.833038	25.687156
172.586106	5209.304360	25.692173
172.771988	5204.951099	25.697191
173.352886	5194.535856	25.702208
172.981784	5203.681228	25.707226
173.476550	5201.937641	25.712244
172.983188	5205.612916	25.717261
173.062520	5206.711717	25.722279
173.414179	5206.335074	25.727296
173.282073	5230.196684	25.732314
173.669002	5227.926966	25.737332
173.803063	5238.897072	25.742349
174.168484	5244.357801	25.747367
174.483378	5245.874465	25.752384
174.563866	5236.323075	25.757402
174.704448	5260.126487	25.762420
174.910886	5273.045531	25.767437
174.931593	5274.633251	25.772455
175.429053	5274.568496	25.777472
174.826087	5273.753367	25.782490
175.324862	5285.601044	25.787508
175.291851	5294.542312	25.792525
175.523437	5299.935512	25.797543
175.706157	5320.515964	25.802560
176.039975	5332.521927	25.807578
176.325647	5327.262964	25.812596
176.721443	5340.203079	25.817613
176.657129	5349.733202	25.822631
177.035486	5339.598775	25.827648
177.343281	5358.957168	25.832666
177.260431	5367.278085	25.837684
177.368109	5379.909555	25.842701
177.234013	5375.454557	25.847719
178.037376	5384.202524	25.852736
177.883543	5407.458541	25.857754
178.140804	5398.078405	25.862772
178.207642	5403.853973	25.867789
178.183403	5409.151304	25.872807
178.688492	5426.777686	25.877824
178.782769	5432.208086	25.882842
179.409836	5430.645898	25.887860
179.372220	5438.530517	25.892877
179.592571	5442.239922	25.897895
179.625109	5447.541051	25.902912
179.619068	5463.488859	25.907930
180.133369	5465.268054	25.912948
180.170790	5480.262150	25.917965
179.984278	5480.123959	25.922983
180.814321	5487.715688	25.928000
180.630890	5503.653270	25.933018
180.871006	5499.272555	25.938036
180.747222	5515.036721	25.943053
180.998306	5519.729355	25.948071
181.620324	5515.661651	25.953088
181.808214	5534.896855	25.958106
181.926131	5534.966948	25.963124
182.243816	5538.626497	25.968141
182.207078	5538.338726	25.973159
182.894946	5540.731685	25.978176
182.764129	5556.231832	25.983194
182.846403	5567.279643	25.988212
183.215348	5565.514576	25.993229
183.229493	5556.276376	25.998247
183.337539	5557.269718	26.003264
183.270152	5576.790921	26.008282
183.557075	5581.455895	26.013300
183.814298	5589.916518	26.018317
183.732937	5605.734131	26.023335
183.874720	5614.105415	26.028352
184.013290	5615.217114	26.033370
184.006142	5633.807283	26.038388
184.660219	5637.499708	26.043405
184.730337	5658.319033	26.048423
185.329298	5660.397568	26.053440
185.106386	5664.400146	26.058458
185.182076	5673.646647	26.063476
185.671257	5682.068042	26.068493
185.586394	5692.696874	26.073511
185.882841	5703.342105	26.078528
186.123238	5705.470156	26.083546
186.244950	5706.082590	26.088564
186.543852	5714.173775	26.093581
186.390470	5732.237568	26.098599
186.992239	5732.775263	26.103616
186.982807	5735.829212	26.108634
187.017926	5747.733595	26.113652
187.331915	5751.103357	26.118669
187.570519	5761.953336	26.123687
187.825768	5772.876487	26.128704
187.961322	5783.660451	26.133722
187.659499	5790.639379	26.138740
188.347284	5793.666861	26.143757
188.337975	5804.817459	26.148775
188.621171	5816.951574	26.153792
188.402974	5826.057668	26.158810
188.434420	5832.047217	26.163828
189.177926	5841.265589	26.168845
189.328981	5857.836387	26.173863
189.843619	5852.361700	26.178880
190.008640	5863.671432	26.183898
190.169445	5872.718543	26.188916
190.682041	5868.554160	26.193933
190.504086	5876.517637	26.198951
191.046988	5875.047431	26.203968
191.164104	5891.913951	26.208986
191.430071	5891.891551	26.214004
191.809635	5885.604539	26.219021
191.652995	5893.280610	26.224039
191.715128	5892.863802	26.229056
191.873052	5902.757347	26.234074
192.067426	5916.531011	26.239092
192.275337	5915.207656	26.244109
192.485068	5924.146163	26.249127
192.576190	5927.560126	26.254144
192.930443	5931.905361	26.259162
192.985075	5937.506228	26.264180
193.456932	5954.522757	26.269197
193.408013	5961.055172	26.274215
194.028202	5964.790821	26.279232
193.705783	5965.889083	26.284250
193.938770	5975.370090	26.289268
194.049812	5988.992639	26.294285
194.129713	5989.826243	26.299303
194.564645	5995.576256	26.304320
194.531268	6005.029303	26.309338
194.554941	6016.301161	26.314356
195.104500	6025.922305	26.319373
195.096223	6038.215586	26.324391
195.787825	6050.131598	26.329408
195.770043	6054.487434	26.334426
195.776167	6065.569499	26.339444
196.439285	6064.307842	26.344461
196.171313	6082.048904	26.349479
196.515400	6079.362763	26.354496
196.887194	6083.073976	26.359514
196.974817	6090.708944	26.364532
197.132396	6095.526768	26.369549
197.541951	6109.055581	26.374567
197.523867	6111.021898	26.379584
198.144501	6129.505364	26.384602
198.210612	6133.327311	26.389620
198.410194	6129.640907	26.394637
198.313160	6138.936632	26.399655
198.341533	6144.873099	26.404672
198.666323	6148.493787	26.409690
198.553779	6153.091679	26.414708
199.231533	6162.143680	26.419725
199.657264	6170.704605	26.424743
199.469929	6176.879848	26.429760
199.773236	6178.767725	26.434778
199.971134	6188.077534	26.439796
200.221334	6188.385881	26.444813
199.822328	6205.970691	26.449831
200.014451	6212.285739	26.454848
200.581978	6225.354425	26.459866
200.596054	6235.718793	26.464884
200.965858	6241.501121	26.469901
201.000834	6257.332754	26.474919
201.294240	6249.941571	26.479936
200.920247	6262.623390	26.484954
201.418946	6274.118178	26.489972
201.984990	6285.671935	26.494989
201.806707	6300.043699	26.500007
202.231026	6303.955120	26.505024
202.601516	6318.639203	26.510042
202.519026	6325.577873	26.515060
203.116383	6327.767221	26.520077
202.963678	6351.725049	26.525095
203.405253	6351.501691	26.530112
203.571007	6357.091700	26.535130
203.754018	6370.517084	26.540148
204.181989	6378.468516	26.545165
204.182767	6377.786618	26.550183
204.351175	6395.608409	26.555200
204.851997	6392.181252	26.560218
204.721658	6409.689705	26.565236
205.286568	6417.755574	26.570253
205.341572	6431.390333	26.575271
205.704015	6435.443998	26.580288
206.125506	6442.676740	26.585306
206.035376	6452.700747	26.590324
205.936826	6449.834087	26.595341
206.044730	6461.831774	26.600359
206.458844	6463.929714	26.605376
206.490444	6488.439859	26.610394
206.650000	6502.153096	26.615412
206.977634	6507.386493	26.620429
207.231797	6521.605873	26.625447
207.624630	6526.699700	26.630464
208.318527	6533.476538	26.635482
208.262984	6544.906263	26.640500
209.042987	6548.661347	26.645517
209.027719	6544.992526	26.650535
209.203619	6548.481795	26.655552
209.279594	6537.288933	26.660570
209.355854	6549.481008	26.665588
209.747846	6558.618735	26.670605
209.757597	6567.367722	26.675623
209.722889	6572.206139	26.680640
209.898505	6565.568684	26.685658
210.102321	6578.678467	26.690676
210.140652	6584.594586	26.695693
210.778591	6586.092639	26.700711
210.694257	6607.833604	26.705728
210.791807	6607.392326	26.710746
210.599193	6616.617942	26.715764
211.402462	6629.044124	26.720781
211.435319	6636.713100	26.725799
211.881186	6660.455028	26.730816
212.039545	6668.016090	26.735834
211.870614	6677.998824	26.740852
212.278537	6688.867188	26.745869
212.378560	6706.794632	26.750887
212.686240	6721.583520	26.755904
212.784087	6726.325579	26.760922
212.830245	6729.850866	26.765940
213.039939	6743.401796	26.770957
213.544889	6753.153386	26.775975
213.564858	6765.209157	26.780992
213.538258	6767.947119	26.786010
213.631791	6787.734983	26.791028
213.891792	6793.932335	26.796045
214.437788	6811.859898	26.801063
214.582445	6823.943647	26.806080
214.942904	6832.641317	26.811098
214.958265	6851.775342	26.816116
215.314437	6859.210983	26.821133
215.837377	6867.431954	26.826151
215.657359	6876.693620	26.831168
216.336497	6873.904694	26.836186
216.821023	6886.876291	26.841204
216.791778	6890.839514	26.846221
217.030893	6903.309521	26.851239
217.235421	6919.715117	26.856256
217.508251	6925.717953	26.861274
217.363167	6926.283576	26.866292
217.876456	6937.135684	26.871309
218.248527	6951.071871	26.876327
218.287975	6954.544581	26.881344
218.469337	6965.520989	26.886362
218.509656	6972.813286	26.891380
218.533680	6969.274005	26.896397
219.051612	6979.614015	26.901415
219.370582	6993.877338	26.906432
219.919360	6999.000685	26.911450
219.648321	7014.470231	26.916468
219.923484	7012.391323	26.921485
220.153934	7022.735077	26.926503
220.271990	7037.332767	26.931520
220.800282	7040.012791	26.936538
220.971321	7060.518105	26.941556
221.328433	7063.527837	26.946573
221.244465	7067.632204	26.951591
221.140890	7076.938892	26.956608
221.588993	7081.497083	26.961626
221.872844	7102.048016	26.966644
221.940206	7127.127989	26.971661
222.199754	7131.472473	26.976679
222.707446	7143.919771	26.981696
223.083517	7138.965057	26.986714
223.149106	7155.398809	26.991732
223.352394	7167.240052	26.996749
223.310935	7168.676618	27.001767
223.582596	7186.448379	27.006784
223.854431	7192.533535	27.011802
224.251644	7202.627292	27.016820
224.402417	7220.676768	27.021837
224.831307	7220.253340	27.026855
224.940679	7235.755395	27.031872
225.204189	7237.318112	27.036890
225.250912	7256.191973	27.041908
225.369762	7255.090740	27.046925
225.616656	7273.630398	27.051943
225.736321	7274.322126	27.056960
225.861921	7291.381183	27.061978
226.527346	7306.035927	27.066996
227.010268	7321.839779	27.072013
227.002241	7319.088320	27.077031
227.151255	7335.310364	27.082048
227.637712	7337.416084	27.087066
227.531938	7354.110301	27.092084
228.015457	7350.543605	27.097101
228.263754	7353.661876	27.102119
228.639024	7362.524806	27.107136
228.993051	7352.055275	27.112154
229.125798	7358.247376	27.117172
228.898514	7354.633499	27.122189
229.296484	7372.218462	27.127207
229.365538	7382.369723	27.132224
229.571239	7379.771235	27.137242
229.911251	7396.907500	27.142260
229.830469	7408.963596	27.147277
230.400240	7410.238725	27.152295
230.334582	7430.550853	27.157312
230.768431	7431.146319	27.162330
230.871803	7448.600436	27.167348
231.141232	7461.444928	27.172365
231.295783	7470.238097	27.177383
231.230561	7482.190798	27.182400
231.472378	7486.727541	27.187418
231.584161	7497.415196	27.192436
232.157456	7507.911045	27.197453
232.702368	7526.401404	27.202471
232.654431	7538.651355	27.207488
232.669658	7543.510666	27.212506
233.154860	7563.986573	27.217524
233.071423	7573.220925	27.222541
233.467738	7590.496979	27.227559
233.689284	7598.361121	27.232576
233.915804	7607.828199	27.237594
234.243873	7629.184163	27.242612
234.254579	7645.866824	27.247629
234.620999	7645.715138	27.252647
234.848221	7671.534938	27.257664
234.863027	7686.648011	27.262682
235.181429	7699.320887	27.267700
235.950494	7722.177290	27.272717
236.462362	7731.265373	27.277735
236.113304	7735.868913	27.282752
236.535127	7746.852549	27.287770
237.087232	7754.835769	27.292788
237.194050	7771.396245	27.297805
237.452770	7771.876927	27.302823
237.631507	7777.872594	27.307840
237.918385	7786.430641	27.312858
238.170241	7804.278693	27.317876
238.236642	7808.189339	27.322893
238.555403	7818.229355	27.327911
239.150375	7829.694352	27.332928
239.207271	7831.652336	27.337946
239.303182	7860.403545	27.342964
239.546624	7859.784834	27.347981
239.916485	7860.257687	27.352999
239.877794	7873.693433	27.358016
240.246082	7884.802295	27.363034
240.576740	7894.158599	27.368052
240.696158	7910.338404	27.373069
240.923577	7912.462423	27.378087
240.993275	7939.516237	27.383104
241.413321	7936.319206	27.388122
241.592554	7958.446924	27.393140
241.580300	7963.932545	27.398157
242.205024	7983.727394	27.403175
241.979624	7991.074092	27.408192
242.163281	8008.418374	27.413210
242.780110	8017.910136	27.418228
242.873810	8030.548769	27.423245
243.161773	8041.016737	27.428263
243.324272	8058.320162	27.433280
243.917264	8071.424092	27.438298
244.146810	8086.415665	27.443316
244.144693	8092.164934	27.448333
244.614905	8094.759449	27.453351
244.917360	8102.775374	27.458368
245.301893	8108.581260	27.463386
245.512392	8112.681055	27.468404
245.530481	8120.804400	27.473421
245.986794	8134.943048	27.478439
245.995814	8147.512864	27.483456
246.150177	8140.019449	27.488474
246.325265	8157.182100	27.493492
245.992432	8168.662319	27.498509
246.123543	8177.295312	27.503527
246.421036	8202.299881	27.508544
246.751726	8222.952115	27.513562
247.480427	8233.572566	27.518580
247.532201	8245.564373	27.523597
248.308821	8253.200313	27.528615
248.180060	8276.910672	27.533632
248.489301	8288.695102	27.538650
248.693451	8305.070425	27.543668
249.258006	8321.598016	27.548685
249.587436	8320.606003	27.553703
249.505887	8345.092042	27.558720
249.858675	8360.067808	27.563738
249.945512	8361.838080	27.568756
250.627781	8374.637880	27.573773
251.902200	8356.693857	27.578791
251.771040	8361.235214	27.583808
251.849826	8353.437776	27.588826
252.531570	8365.375782	27.593844
252.445057	8376.252672	27.598861
252.474991	8381.652924	27.603879
252.561411	8386.826548	27.608896
252.489377	8388.643656	27.613914
253.024519	8399.622670	27.618932
252.923675	8418.410199	27.623949
253.753242	8411.976504	27.628967
253.692200	8427.108307	27.633984
253.878511	8430.823622	27.639002
254.424818	8431.890959	27.644020
254.189484	8452.871508	27.649037
254.647824	8454.871243	27.654055
255.195306	8466.855474	27.659072
255.449491	8475.813564	27.664090
255.481392	8479.849693	27.669108
255.734398	8494.588539	27.674125
255.895839	8493.707911	27.679143
256.071381	8507.840046	27.684160
256.383575	8523.371593	27.689178
256.506454	8522.168633	27.694196
256.355875	8549.282893	27.699213
256.756494	8558.691785	27.704231
257.038126	8578.869025	27.709248
257.532020	8588.718029	27.714266
257.898090	8600.051821	27.719284
257.952405	8608.895867	27.724301
258.269711	8625.762148	27.729319
258.772294	8641.775601	27.734336
258.877130	8649.702562	27.739354
259.148597	8660.265006	27.744372
259.615131	8678.203610	27.749389
260.051309	8680.266804	27.754407
259.969711	8687.512463	27.759424
260.274708	8708.251325	27.764442
260.713711	8708.517698	27.769460
260.580429	8724.778602	27.774477
261.133521	8732.638969	27.779495
261.212540	8753.264680	27.784512
261.370726	8772.596306	27.789530
261.727530	8765.036393	27.794548
261.496583	8792.416089	27.799565
261.984112	8794.266090	27.804583
261.905117	8811.923531	27.809600
262.253860	8826.691938	27.814618
262.623984	8845.554962	27.819636
262.620194	8854.436586	27.824653
262.984751	8875.021136	27.829671
263.547304	8890.930755	27.834688
263.814289	8901.055195	27.839706
264.169775	8918.818737	27.844724
263.998439	8934.804765	27.849741
264.568444	8956.569758	27.854759
264.713128	8974.454571	27.859776
264.720240	8981.001435	27.864794
265.361152	8998.742717	27.869812
265.733430	9012.667809	27.874829
265.661048	9023.299778	27.879847
266.432224	9032.559666	27.884864
267.315553	9050.301142	27.889882
267.250724	9054.384027	27.894900
267.206794	9053.683732	27.899917
267.531797	9074.230462	27.904935
267.983878	9088.812504	27.909952
267.952274	9098.547850	27.914970
268.555078	9104.376899	27.919988
269.013979	9112.599382	27.925005
269.363366	9119.686553	27.930023
269.576073	9126.270917	27.935040
269.591121	9132.564026	27.940058
270.376501	9140.833565	27.945076
270.636761	9146.668599	27.950093
270.512691	9138.289923	27.955111
270.929227	9155.722158	27.960128
271.018421	9178.900908	27.965146
271.583708	9177.622715	27.970164
271.329582	9189.504901	27.975181
271.579367	9210.729656	27.980199
271.736260	9218.329882	27.985216
271.543793	9231.418009	27.990234
272.368455	9245.440177	27.995252
272.182479	9266.941213	28.000269
272.418732	9283.779670	28.005287
273.031988	9298.690390	28.010304
273.537900	9309.620827	28.015322
273.733728	9321.515132	28.020340
273.834167	9326.699466	28.025357
274.360340	9357.450826	28.030375
274.915523	9360.354330	28.035392
274.783597	9383.728779	28.040410
275.147791	9394.387709	28.045428
275.503067	9410.904659	28.050445
275.900932	9410.924873	28.055463
276.061420	9426.105090	28.060480
276.224563	9440.896569	28.065498
276.682008	9448.216464	28.070516
276.843479	9475.981242	28.075533
276.987693	9481.345080	28.080551
277.088020	9491.678909	28.085568
277.571171	9513.278118	28.090586
278.160966	9528.710463	28.095604
277.877672	9540.284847	28.100621
278.475369	9550.613892	28.105639
278.990409	9558.082726	28.110656
279.352135	9577.973907	28.115674
279.588840	9580.235594	28.120692
279.512290	9596.838883	28.125709
279.862786	9609.451246	28.130727
280.199879	9616.133238	28.135744
280.495281	9631.952484	28.140762
280.479172	9629.523978	28.145780
280.870125	9645.101038	28.150797
281.060929	9653.365501	28.155815
281.470752	9670.363565	28.160832
281.959689	9673.564743	28.165850
282.082493	9686.023172	28.170868
282.477748	9709.909521	28.175885
282.569768	9713.753437	28.180903
282.721735	9726.087376	28.185920
282.865911	9746.088381	28.190938
283.251850	9761.647376	28.195956
283.557948	9784.540532	28.200973
283.589272	9801.079849	28.205991
284.190378	9813.615448	28.211008
284.349290	9828.752038	28.216026
284.473264	9841.229332	28.221044
284.614164	9853.659797	28.226061
284.787965	9881.173835	28.231079
285.119430	9892.068630	28.236096
285.360192	9908.695414	28.241114
285.780354	9923.864027	28.246132
286.147575	9946.915204	28.251149
286.347311	9965.357560	28.256167
287.007032	9987.567609	28.261184
287.224512	10013.960513	28.266202
287.747300	10011.116542	28.271220
288.167037	10039.984902	28.276237
288.786476	10054.184874	28.281255
289.382980	10066.756091	28.286272
288.989104	10073.713073	28.291290
289.369084	10082.598684	28.296308
289.450251	10098.527457	28.301325
290.094159	10108.091861	28.306343
290.380797	10115.577536	28.311360
290.593828	10133.759088	28.316378
291.028410	10144.931610	28.321396
291.100116	10152.393930	28.326413
291.457093	10188.679406	28.331431
291.568285	10185.643743	28.336448
291.692579	10210.115983	28.341466
291.855838	10213.146946	28.346484
292.362566	10235.602125	28.351501
292.753520	10254.223383	28.356519
292.890213	10265.881227	28.361536
292.613127	10279.974673	28.366554
293.173495	10297.009864	28.371572
293.713865	10320.874406	28.376589
294.036054	10342.221792	28.381607
294.344365	10349.170592	28.386624
294.370409	10370.497811	28.391642
294.687118	10385.259819	28.396660
295.482768	10402.514225	28.401677
295.572988	10421.097220	28.406695
296.147769	10433.290025	28.411712
296.363562	10444.035811	28.416730
296.757517	10456.244154	28.421748
297.073587	10467.583718	28.426765
297.242044	10480.130292	28.431783
298.331350	10486.155577	28.436800
298.543722	10493.902401	28.441818
298.696360	10501.071253	28.446836
299.056156	10515.056252	28.451853
298.798585	10521.344912	28.456871
299.247207	10530.797855	28.461888
299.443705	10538.837650	28.466906
299.669162	10549.948252	28.471924
300.218545	10567.594780	28.476941
300.227834	10574.928061	28.481959
300.438205	10578.122249	28.486976
300.546986	10593.614581	28.491994
300.793529	10595.938010	28.497012
301.460464	10620.515753	28.502029
301.121590	10635.755757	28.507047
301.656536	10644.623826	28.512064
301.599412	10661.521836	28.517082
302.097195	10679.448043	28.522100
302.639563	10698.513472	28.527117
302.529245	10721.434722	28.532135
302.977721	10731.197219	28.537152
302.967183	10754.431348	28.542170
303.755469	10772.359778	28.547188
304.408782	10779.261343	28.552205
304.627368	10812.257421	28.557223
304.920487	10815.814505	28.562240
305.093202	10835.695411	28.567258
305.265732	10844.818919	28.572276
305.722555	10865.934396	28.577293
306.025045	10885.204707	28.582311
306.364640	10896.607177	28.587328
306.343796	10919.694715	28.592346
307.007936	10937.917333	28.597364
307.482930	10950.091281	28.602381
307.336691	10983.858049	28.607399
307.758205	10988.932868	28.612416
307.978558	11011.768260	28.617434
308.365252	11033.627381	28.622452
308.868157	11049.478678	28.627469
309.012918	11071.132381	28.632487
309.259445	11084.210296	28.637504
309.431851	11101.508704	28.642522
310.124490	11123.746561	28.647540
310.470993	11130.762331	28.652557
311.133500	11143.933401	28.657575
311.894218	11143.448767	28.662592
312.346662	11166.507132	28.667610
312.730241	11154.594200	28.672628
312.966780	11160.051505	28.677645
313.072546	11176.024730	28.682663
313.479749	11170.795718	28.687680
313.799443	11180.509035	28.692698
314.276196	11180.640119	28.697716
315.253834	11178.208262	28.702733
315.237024	11174.608228	28.707751
315.626257	11176.865311	28.712768
315.505909	11179.384863	28.717786
315.618500	11177.431849	28.722804
316.096139	11176.012457	28.727821
316.298899	11194.035609	28.732839
316.402222	11198.421166	28.737856
316.530686	11207.952716	28.742874
316.514818	11223.228163	28.747892
317.087761	11240.079125	28.752909
317.233059	11257.249281	28.757927
317.532448	11266.280622	28.762944
317.956344	11278.405906	28.767962
317.786116	11289.941666	28.772980
318.210444	11307.409441	28.777997
318.270885	11334.213883	28.783015
318.516748	11353.780829	28.788032
319.125266	11381.033635	28.793050
318.912650	11401.584540	28.798068
319.319176	11425.127163	28.803085
319.612705	11452.305966	28.808103
320.196855	11475.227378	28.813120
320.512939	11497.533779	28.818138
320.693777	11517.249953	28.823156
321.050362	11533.462301	28.828173
321.165220	11560.154393	28.833191
321.687851	11576.644056	28.838208
321.733161	11594.332142	28.843226
322.138830	11617.676213	28.848244
322.770616	11637.154956	28.853261
322.773202	11663.460503	28.858279
323.269215	11677.977746	28.863296
323.786385	11709.681673	28.868314
324.105357	11727.936698	28.873332
324.508939	11742.837821	28.878349
324.438383	11755.769800	28.883367
325.112115	11770.559420	28.888384
325.014107	11794.518919	28.893402
325.218229	11819.255550	28.898420
326.048057	11840.323531	28.903437
326.615169	11866.326756	28.908455
326.970590	11882.536431	28.913472
327.307824	11898.521601	28.918490
327.717453	11917.823662	28.923508
328.021062	11936.640183	28.928525
328.013533	11961.987800	28.933543
328.596546	11979.532544	28.938560
329.138251	11997.080576	28.943578
329.217643	12014.883744	28.948596
329.442494	12022.357702	28.953613
329.752395	12047.217102	28.958631
330.138671	12062.509566	28.963648
330.760802	12081.020874	28.968666
330.853595	12103.056464	28.973684
331.367934	12118.420608	28.978701
331.253837	12147.157457	28.983719
331.946362	12164.432710	28.988736
332.360293	12176.007534	28.993754
332.761966	12195.832136	28.998772
333.600390	12204.268468	29.003789
333.561756	12224.622670	29.008807
334.200732	12236.004612	29.013824
334.414021	12248.207520	29.018842
335.071962	12256.766705	29.023860
335.617414	12265.147629	29.028877
335.707222	12285.882929	29.033895
335.382268	12288.788144	29.038912
335.867049	12306.787407	29.043930
336.166011	12328.718538	29.048948
336.597717	12339.220234	29.053965
336.861312	12356.761378	29.058983
337.183182	12372.904073	29.064000
337.477663	12388.391083	29.069018
337.354853	12414.429851	29.074036
338.335110	12423.908352	29.079053
337.938991	12441.997520	29.084071
338.451630	12468.291099	29.089088
339.040508	12476.308533	29.094106
339.476140	12490.529508	29.099124
340.014659	12523.504053	29.104141
339.764683	12530.332172	29.109159
340.288497	12556.330464	29.114176
340.712801	12574.592019	29.119194
340.828606	12598.345578	29.124212
341.656809	12606.319494	29.129229
341.707276	12634.254659	29.134247
341.868552	12656.750742	29.139264
342.808997	12669.273331	29.144282
342.849935	12690.152468	29.149300
343.532271	12700.495353	29.154317
343.586660	12715.663184	29.159335
343.953822	12729.430807	29.164352
344.509190	12740.933437	29.169370
344.534849	12759.623535	29.174388
344.831642	12768.798106	29.179405
345.185462	12782.283645	29.184423
345.320328	12795.320141	29.189440
346.053317	12809.469802	29.194458
346.170277	12838.626454	29.199476
346.573112	12848.052966	29.204493
346.504925	12863.082109	29.209511
346.976663	12877.900895	29.214528
347.381994	12893.468955	29.219546
347.324822	12918.787695	29.224564
348.005909	12948.355625	29.229581
348.346299	12981.437604	29.234599
348.565358	12993.475891	29.239616
349.005902	13005.621807	29.244634
349.471245	13045.230601	29.249652
349.660773	13058.328241	29.254669
350.086369	13081.538401	29.259687
350.218514	13102.378531	29.264704
350.458779	13125.949171	29.269722
350.751934	13156.117810	29.274740
351.434077	13182.742834	29.279757
352.025389	13198.604294	29.284775
352.844479	13217.196584	29.289792
353.580515	13230.449259	29.294810
353.558354	13244.606287	29.299828
353.721845	13263.335425	29.304845
353.919682	13278.872950	29.309863
354.707531	13292.322863	29.314880
354.769775	13309.340457	29.319898
355.096919	13322.704222	29.324916
355.268065	13339.183839	29.329933
355.730889	13361.813815	29.334951
355.804212	13384.716035	29.339968
356.520121	13397.574068	29.344986
356.517536	13427.163922	29.350004
357.120172	13445.881715	29.355021
357.243241	13462.621557	29.360039
357.669044	13496.584825	29.365056
357.992726	13507.463993	29.370074
358.052572	13539.340096	29.375092
358.630106	13566.531424	29.380109
359.184626	13579.601024	29.385127
359.420405	13607.246670	29.390144
360.013692	13622.631334	29.395162
360.024705	13656.492095	29.400180
360.660395	13679.765020	29.405197
361.015864	13705.639526	29.410215
361.433455	13723.934819	29.415232
361.862220	13743.861045	29.420250
361.889243	13770.532047	29.425268
362.675718	13785.940453	29.430285
363.031091	13803.452865	29.435303
363.263622	13828.614033	29.440320
363.853480	13847.883699	29.445338
364.121052	13866.969870	29.450356
364.912107	13885.437709	29.455373
364.992238	13900.725643	29.460391
365.464652	13908.720771	29.465408
365.835917	13917.366401	29.470426
366.063595	13938.751540	29.475444
366.811554	13953.307112	29.480461
367.224671	13963.237859	29.485479
367.488592	13966.086388	29.490496
368.031488	13985.117183	29.495514
367.987242	13992.065382	29.500532
368.501264	14008.909057	29.505549
368.891908	14023.333989	29.510567
369.152262	14027.970504	29.515584
369.064947	14046.559457	29.520602
369.413844	14064.846827	29.525620
369.867172	14075.071383	29.530637
370.177464	14087.298276	29.535655
370.410343	14114.562997	29.540672
370.680155	14131.113210	29.545690
370.738309	14151.827063	29.550708
371.166840	14177.615047	29.555725
371.657360	14199.306942	29.560743
371.715279	14235.691005	29.565760
372.691707	14249.544895	29.570778
372.832792	14277.585224	29.575796
372.837605	14295.162141	29.580813
373.342313	14330.232563	29.585831
373.933617	14357.378672	29.590848
374.074295	14378.098872	29.595866
374.593153	14398.577052	29.600884
375.014440	14432.662708	29.605901
375.413832	14456.807103	29.610919
375.721312	14487.092481	29.615936
376.549843	14504.778209	29.620954
377.069219	14539.218279	29.625972
376.972953	14552.367762	29.630989
377.676481	14575.163833	29.636007
377.640530	14599.985694	29.641024
378.602107	14623.906983	29.646042
378.937091	14645.222526	29.651060
379.384533	14661.483426	29.656077
380.275339	14679.033298	29.661095
380.373720	14694.015852	29.666112
380.989931	14702.863724	29.671130
381.174455	14713.187318	29.676148
381.344331	14728.616694	29.681165
382.243008	14756.776645	29.686183
382.220184	14759.837315	29.691200
382.883416	14780.198689	29.696218
383.035356	14801.103925	29.701236
383.182549	14814.161999	29.706253
383.530953	14837.127363	29.711271
383.560150	14857.319086	29.716288
383.814065	14883.008888	29.721306
384.332014	14912.636868	29.726324
384.683809	14938.245185	29.731341
385.483396	14956.949605	29.736359
385.944133	14992.040727	29.741376
386.025978	15013.339245	29.746394
386.176720	15038.571595	29.751412
387.141848	15057.834601	29.756429
387.497101	15090.238943	29.761447
387.566920	15112.041591	29.766464
388.063304	15119.951389	29.771482
388.552767	15154.337224	29.776500
388.971401	15172.384258	29.781517
389.631716	15181.070737	29.786535
389.503266	15202.057963	29.791552
390.178655	15213.142328	29.796570
390.716979	15240.594817	29.801588
390.709008	15259.336826	29.806605
391.907217	15281.993571	29.811623
392.082284	15308.684737	29.816640
392.546822	15307.731347	29.821658
392.561285	15327.420549	29.826676
392.780323	15348.385421	29.831693
393.119657	15370.686459	29.836711
393.945523	15396.208956	29.841728
394.332619	15400.709223	29.846746
394.013705	15430.515666	29.851764
394.374820	15450.580545	29.856781
394.900148	15473.215944	29.861799
395.155765	15494.036318	29.866816
395.429460	15518.094250	29.871834
395.818820	15542.693213	29.876852
396.119537	15561.523266	29.881869
396.490880	15591.115119	29.886887
397.129260	15620.387518	29.891904
397.438319	15634.314739	29.896922
397.964919	15664.915285	29.901940
398.125876	15696.716095	29.906957
398.615788	15711.417416	29.911975
399.062622	15748.473377	29.916992
399.495932	15767.617769	29.922010
399.909590	15801.874450	29.927028
400.202659	15828.734310	29.932045
401.018052	15850.431204	29.937063
401.210644	15881.270434	29.942080
401.486464	15898.099178	29.947098
402.226817	15920.654258	29.952116
402.171144	15956.222336	29.957133
402.892695	15968.853844	29.962151
403.093147	15998.324491	29.967168
403.746017	16030.778845	29.972186
404.131091	16055.849725	29.977204
404.412120	16084.963703	29.982221
405.172707	16094.051891	29.987239
405.223354	16124.882028	29.992256
405.842403	16145.558099	29.997274
406.262679	16165.965096	30.002292
406.900935	16183.776761	30.007309
407.632879	16203.923669	30.012327
407.835977	16233.248981	30.017344
408.627851	16247.878439	30.022362
409.233996	16266.980633	30.027380
408.692943	16292.660281	30.032397
409.334742	16295.267151	30.037415
409.567933	16335.926460	30.042432
410.463490	16341.904870	30.047450
410.713086	16371.169462	30.052468
410.905616	16394.874760	30.057485
411.532572	16413.692764	30.062503
411.671214	16435.975755	30.067520
412.026953	16456.156229	30.072538
412.539511	16487.303519	30.077556
412.880575	16514.782232	30.082573
413.403910	16543.650730	30.087591
413.773553	16564.078668	30.092608
414.351422	16581.524255	30.097626
414.274196	16608.161757	30.102644
415.051609	16647.912656	30.107661
415.419290	16662.636897	30.112679
416.093662	16680.866633	30.117696
416.517253	16703.898339	30.122714
417.595763	16714.898715	30.127732
417.599704	16730.159717	30.132749
418.683493	16743.461787	30.137767
418.470338	16763.592179	30.142784
418.859071	16776.266561	30.147802
419.667100	16795.508409	30.152820
419.924984	16811.434274	30.157837
420.271672	16821.054697	30.162855
420.121639	16835.919679	30.167872
420.478258	16865.076768	30.172890
421.119156	16887.338944	30.177908
420.934691	16912.821774	30.182925
421.759572	16927.070758	30.187943
422.082808	16949.341399	30.192960
422.054085	16972.330138	30.197978
422.698766	16990.675338	30.202996
422.900523	17020.576904	30.208013
423.374287	17035.796591	30.213031
423.920804	17067.612294	30.218048
424.050943	17093.858117	30.223066
424.493177	17120.753417	30.228084
424.876085	17152.168333	30.233101
425.701064	17170.109774	30.238119
426.305246	17193.246610	30.243136
426.483614	17217.258344	30.248154
426.615453	17246.747905	30.253172
427.004403	17282.362923	30.258189
427.727662	17294.123292	30.263207
428.418634	17319.713578	30.268224
428.844679	17349.883957	30.273242
429.215060	17373.180590	30.278260
429.799608	17411.838656	30.283277
430.284423	17425.550306	30.288295
430.551012	17455.145550	30.293312
431.025956	17469.329391	30.298330
431.621534	17496.217137	30.303348
431.635241	17528.565064	30.308365
432.464160	17555.817704	30.313383
432.512149	17581.059921	30.318400
432.651838	17599.996008	30.323418
433.572828	17628.134612	30.328436
433.834111	17657.430927	30.333453
434.439095	17689.724978	30.338471
434.514558	17726.403527	30.343488
434.948129	17757.612551	30.348506
435.322825	17788.792887	30.353524
435.843480	17816.937235	30.358541
436.291067	17857.809594	30.363559
436.846546	17883.769172	30.368576
437.311801	17913.293127	30.373594
437.623315	17944.072929	30.378612
438.312886	17976.392195	30.383629
438.901180	17997.552005	30.388647
439.382385	18023.668631	30.393664
439.954038	18046.423043	30.398682
440.526724	18074.610206	30.403700
440.725464	18097.309021	30.408717
441.521096	18116.478316	30.413735
442.025996	18141.902826	30.418752
442.212066	18174.098652	30.423770
442.728246	18196.457568	30.428788
442.979724	18210.910487	30.433805
443.400860	18229.980262	30.438823
444.017063	18263.240082	30.443840
444.710935	18293.215465	30.448858
445.367289	18310.214505	30.453876
445.163567	18335.193657	30.458893
445.692526	18355.137522	30.463911
446.245805	18383.839866	30.468928
446.578580	18408.533434	30.473946
447.159221	18423.421709	30.478964
447.257211	18442.687302	30.483981
447.987841	18477.553256	30.488999
448.075520	18502.878939	30.494016
448.530806	18527.983172	30.499034
449.088113	18551.643809	30.504052
449.341896	18589.774519	30.509069
450.014730	18602.330066	30.514087
450.982894	18622.597517	30.519104
451.410897	18655.381911	30.524122
452.300869	18662.003153	30.529140
452.244127	18676.346465	30.534157
453.011759	18688.432450	30.539175
453.104777	18712.936301	30.544192
453.392166	18734.409099	30.549210
454.096745	18753.106753	30.554228
454.320825	18770.773661	30.559245
454.612182	18782.599022	30.564263
455.517525	18805.839371	30.569280
455.167707	18819.299735	30.574298
456.022947	18848.088428	30.579316
456.388188	18884.345003	30.584333
456.627698	18908.636767	30.589351
457.020260	18928.160227	30.594368
457.271959	18951.205583	30.599386
458.074117	18972.238403	30.604404
458.456636	19007.999746	30.609421
458.629002	19038.082741	30.614439
459.045883	19061.449981	30.619456
459.537739	19102.134862	30.624474
459.647658	19138.463247	30.629492
460.075163	19172.069886	30.634509
461.026770	19207.351306	30.639527
461.716860	19231.952389	30.644544
462.157771	19268.956024	30.649562
462.860225	19300.536325	30.654580
463.174710	19333.813364	30.659597
463.714149	19362.456135	30.664615
464.216684	19383.523411	30.669632
464.205234	19414.791749	30.674650
464.977856	19445.053588	30.679668
465.437702	19477.828095	30.684685
465.836516	19509.942475	30.689703
466.763518	19540.091980	30.694720
467.110142	19571.431180	30.699738
467.772340	19595.531643	30.704756
467.959399	19630.301074	30.709773
468.381773	19652.789994	30.714791
469.104955	19675.731219	30.719808
469.473130	19711.098064	30.724826
470.177988	19728.931073	30.729844
470.412256	19752.390751	30.734861
470.577204	19781.269338	30.739879
471.339572	19805.746175	30.744896
471.854711	19851.552791	30.749914
472.068661	19867.674389	30.754932
472.594334	19901.197507	30.759949
472.677718	19924.857783	30.764967
473.458915	19967.596974	30.769984
473.559581	19995.247571	30.775002
474.501321	20021.484730	30.780020
474.866851	20063.663365	30.785037
475.614666	20097.790352	30.790055
475.927494	20123.929699	30.795072
476.157676	20152.792361	30.800090
476.929170	20186.265064	30.805108
477.555269	20222.875236	30.810125
478.232256	20251.744303	30.815143
478.889746	20269.060787	30.820160
478.877918	20298.517325	30.825178
479.243832	20326.878944	30.830196
479.979223	20348.403821	30.835213
480.189858	20376.530645	30.840231
480.936814	20403.209315	30.845248
480.940092	20444.219462	30.850266
481.925740	20465.181108	30.855284
482.762320	20486.766202	30.860301
483.290312	20509.928340	30.865319
484.009541	20524.183799	30.870336
484.187287	20549.125350	30.875354
484.943909	20561.643853	30.880372
484.650188	20579.544645	30.885389
485.104507	20604.834934	30.890407
485.648868	20625.903361	30.895424
485.525354	20656.818360	30.900442
485.845412	20697.236360	30.905460
486.856717	20717.057015	30.910477
487.326293	20750.400778	30.915495
488.301599	20780.544684	30.920512
488.200241	20819.840723	30.925530
488.707388	20835.241428	30.930548
489.436987	20864.355939	30.935565
489.596424	20890.583372	30.940583
490.460592	20913.826335	30.945600
490.739312	20950.397174	30.950618
491.212769	20971.287464	30.955636
491.600309	21010.640457	30.960653
492.189867	21045.457153	30.965671
493.188305	21065.589761	30.970688
493.657307	21092.830743	30.975706
494.073834	21118.348719	30.980724
494.467487	21149.986406	30.985741
495.137115	21182.983846	30.990759
495.438113	21205.859911	30.995776
496.197204	21239.879725	31.000794
496.731799	21265.120460	31.005812
497.180596	21292.946152	31.010829
497.507998	21322.787383	31.015847
498.268669	21342.736149	31.020864
498.615805	21363.532792	31.025882
499.063942	21392.900411	31.030900
499.818894	21431.369342	31.035917
499.935195	21447.918140	31.040935
500.429257	21477.771571	31.045952
500.764189	21511.630425	31.050970
501.070130	21545.203202	31.055988
502.135013	21575.852500	31.061005
502.145012	21608.782747	31.066023
502.923168	21644.569460	31.071040
503.023805	21675.312157	31.076058
503.586295	21715.068981	31.081076
504.629787	21747.611104	31.086093
505.017658	21786.359023	31.091111
505.786386	21812.322233	31.096128
505.960857	21839.787020	31.101146
506.646581	21868.739251	31.106164
507.040468	21891.607972	31.111181
507.256511	21931.476033	31.116199
508.045584	21965.182826	31.121216
508.217069	22004.407159	31.126234
509.138662	22033.796808	31.131252
509.596446	22067.915510	31.136269
510.123672	22091.048041	31.141287
511.280604	22115.940241	31.146304
511.344387	22150.777559	31.151322
511.906161	22181.303928	31.156340
512.437030	22208.303034	31.161357
512.717381	22235.252716	31.166375
513.679509	22259.025430	31.171392
514.125092	22293.146421	31.176410
514.098134	22317.300654	31.181428
514.827200	22351.535582	31.186445
515.181137	22376.572076	31.191463
516.121817	22407.058764	31.196480
516.611291	22440.389657	31.201498
516.956216	22463.961723	31.206516
517.343652	22483.710685	31.211533
517.674200	22519.113721	31.216551
518.149398	22523.804143	31.221568
518.758541	22566.537868	31.226586
518.823373	22584.928071	31.231604
519.829320	22623.530863	31.236621
519.973459	22653.844953	31.241639
520.670551	22689.728328	31.246656
521.326337	22724.032179	31.251674
521.763426	22750.970801	31.256692
522.210483	22772.543227	31.261709
522.666949	22807.649148	31.266727
523.372617	22831.114942	31.271744
523.749756	22872.767011	31.276762
524.052848	22900.548148	31.281780
524.938378	22940.301382	31.286797
525.023741	22969.696229	31.291815
525.593545	23010.168556	31.296832
526.071627	23041.695031	31.301850
526.349532	23084.721559	31.306868
526.939735	23121.469093	31.311885
527.567489	23166.248549	31.316903
528.450375	23208.321786	31.321920
529.033493	23242.328219	31.326938
529.378249	23284.068339	31.331956
530.123816	23319.913715	31.336973
530.372737	23359.002295	31.341991
531.267483	23386.382375	31.347008
531.894026	23423.541867	31.352026
532.519882	23455.437774	31.357044
533.168533	23492.954140	31.362061
533.103565	23530.992408	31.367079
533.864368	23567.891144	31.372096
534.422364	23606.110615	31.377114
535.599506	23629.661936	31.382132
536.118641	23658.838617	31.387149
536.573572	23696.227546	31.392167
536.932142	23725.580980	31.397184
537.815561	23755.535217	31.402202
537.934624	23788.249894	31.407220
538.742158	23817.002761	31.412237
539.077509	23850.164124	31.417255
539.676744	23872.143760	31.422272
540.359498	23913.282815	31.427290
540.982696	23934.481529	31.432308
541.936511	23952.456561	31.437325
542.429001	23981.821121	31.442343
542.625412	24003.617162	31.447360
543.133092	24036.246471	31.452378
543.988022	24065.598966	31.457396
544.518446	24090.458488	31.462413
544.921312	24119.742415	31.467431
545.527456	24144.438554	31.472448
545.761325	24181.319352	31.477466
546.228057	24212.723067	31.482484
547.171336	24232.109192	31.487501
547.217061	24268.381192	31.492519
547.751785	24302.870921	31.497536
548.237194	24333.785332	31.502554
548.177934	24372.399374	31.507572
548.997183	24413.379187	31.512589
549.562648	24458.607284	31.517607
549.932564	24488.889022	31.522624
550.460146	24539.178692	31.527642
550.849693	24580.984070	31.532660
551.487118	24621.796715	31.537677
551.621811	24666.340333	31.542695
552.714354	24710.166187	31.547712
553.303835	24747.883711	31.552730
553.632834	24781.161360	31.557748
554.307830	24807.490662	31.562765
554.959818	24849.843456	31.567783
555.106990	24889.576504	31.572800
555.932479	24922.423205	31.577818
556.636270	24962.322525	31.582836
557.106031	24992.437813	31.587853
557.372351	25032.588643	31.592871
558.483559	25063.153981	31.597888
559.555139	25096.272316	31.602906
559.835990	25125.368166	31.607924
560.481276	25155.020323	31.612941
561.124568	25192.736629	31.617959
561.697157	25226.792325	31.622976
562.219099	25254.144538	31.627994
562.595403	25286.056946	31.633012
563.306754	25319.244369	31.638029
563.862156	25351.470260	31.643047
564.264225	25387.789927	31.648064
564.775688	25418.543968	31.653082
565.468976	25460.013191	31.658100
565.782041	25492.201198	31.663117
566.253560	25533.420711	31.668135
566.804613	25574.362499	31.673152
567.478182	25607.284533	31.678170
568.055145	25649.132480	31.683188
569.064123	25688.416961	31.688205
569.341606	25734.135152	31.693223
569.878737	25761.795361	31.698240
570.632678	25792.575426	31.703258
570.854074	25826.396101	31.708276
571.394932	25858.612431	31.713293
572.357294	25906.088735	31.718311
572.679190	25937.138514	31.723328
573.610367	25974.350125	31.728346
574.146181	26013.670984	31.733364
574.958748	26047.027129	31.738381
575.239098	26081.673277	31.743399
575.898785	26112.632822	31.748416
577.084338	26137.449780	31.753434
577.643658	26165.138690	31.758452
578.536187	26192.902164	31.763469
579.205473	26228.688800	31.768487
579.796107	26260.196514	31.773504
579.901194	26281.061261	31.778522
580.436949	26307.035014	31.783540
581.106061	26328.823197	31.788557
581.615773	26364.028200	31.793575
581.742498	26401.624953	31.798592
582.607545	26432.742620	31.803610
582.992296	26481.277158	31.808628
583.699835	26506.383867	31.813645
584.075058	26552.335179	31.818663
584.446895	26579.984325	31.823680
584.589498	26615.190035	31.828698
585.062973	26659.236604	31.833716
585.489407	26708.428803	31.838733
586.136446	26756.183722	31.843751
586.649873	26800.060056	31.848768
587.731069	26837.199349	31.853786
588.260254	26892.860429	31.858804
589.127027	26930.229196	31.863821
589.909367	26971.447505	31.868839
590.050712	27008.107728	31.873856
590.858288	27047.084927	31.878874
591.342168	27093.500886	31.883892
592.394955	27126.859345	31.888909
592.753462	27157.627213	31.893927
593.171884	27193.302927	31.898944
593.843694	27225.646421	31.903962
594.188468	27256.454498	31.908980
594.841067	27288.219621	31.913997
595.420495	27328.522209	31.919015
595.829324	27369.894280	31.924032
596.554810	27396.282317	31.929050
597.300223	27448.618399	31.934068
598.172320	27474.996357	31.939085
598.224789	27517.315366	31.944103
598.402254	27564.051876	31.949120
598.956333	27610.066229	31.954138
599.599537	27658.727683	31.959156
600.289269	27702.211945	31.964173
601.192525	27753.317049	31.969191
602.103166	27788.803418	31.974208
602.119158	27832.708863	31.979226
603.265206	27871.281014	31.984244
604.687879	27894.381994	31.989261
605.281726	27926.485927	31.994279
605.807603	27965.287531	31.999296
606.462160	27984.216600	32.004314
606.921265	28018.749749	32.009332
607.465971	28050.981617	32.014349
608.018291	28088.780705	32.019367
608.481567	28128.053761	32.024384
609.065684	28165.494092	32.029402
609.610991	28203.610510	32.034420
610.291674	28245.333916	32.039437
611.243968	28277.338359	32.044455
611.459044	28325.612978	32.049472
612.335860	28360.473556	32.054490
612.680535	28408.266794	32.059508
613.287062	28441.425104	32.064525
613.830500	28485.875586	32.069543
614.355406	28528.167394	32.074560
614.831918	28558.792601	32.079578
615.436580	28610.698500	32.084596
616.122489	28662.591883	32.089613
617.269941	28697.025346	32.094631
617.390694	28735.474319	32.099648
618.276445	28773.526164	32.104666
618.486388	28816.866274	32.109684
619.037296	28857.340671	32.114701
620.160830	28912.636645	32.119719
620.409700	28955.724479	32.124736
621.152497	28988.192464	32.129754
621.708882	29043.020853	32.134772
622.478864	29077.077586	32.139789
623.157328	29132.335987	32.144807
623.977440	29176.321406	32.149824
624.585372	29208.886587	32.154842
625.106466	29251.363791	32.159860
625.616595	29302.268505	32.164877
626.186668	29343.252871	32.169895
626.570683	29384.873088	32.174912
627.511965	29423.846672	32.179930
627.696655	29471.199551	32.184948
628.874263	29507.412189	32.189965
629.833210	29547.521027	32.194983
630.112214	29594.246377	32.200000
631.254565	29631.337015	32.205018
632.001392	29663.976113	32.210036
632.278243	29698.508869	32.215053
633.657774	29720.866451	32.220071
634.353760	29757.243001	32.225088
635.320458	29769.684034	32.230106
635.541829	29796.855294	32.235124
636.121292	29811.619560	32.240141
636.750513	29835.769142	32.245159
636.912656	29867.140561	32.250176
637.592350	29898.608448	32.255194
637.972457	29925.369584	32.260212
638.411907	29961.211215	32.265229
639.336880	29993.260530	32.270247
639.599882	30035.147428	32.275264
640.288742	30071.241195	32.280282
640.729261	30113.745371	32.285300
641.469840	30151.240836	32.290317
641.970433	30186.150456	32.295335
642.094147	30234.791458	32.300352
642.892205	30276.532342	32.305370
643.599492	30328.104237	32.310388
643.655079	30377.729644	32.315405
644.580697	30423.976948	32.320423
645.331330	30475.909096	32.325440
645.894926	30524.608729	32.330458
646.367870	30573.038132	32.335476
646.725321	30630.354376	32.340493
647.462529	30688.142651	32.345511
648.081057	30746.619621	32.350528
648.917181	30793.317857	32.355546
649.647252	30852.106471	32.360564
650.509673	30900.893222	32.365581
651.144810	30955.113923	32.370599
652.100436	31015.599948	32.375616
652.737932	31063.612959	32.380634
653.733088	31109.585478	32.385652
654.432244	31152.848032	32.390669
655.217696	31198.037928	32.395687
655.627767	31247.698740	32.400704
656.452316	31298.104298	32.405722
657.258916	31345.181346	32.410740
657.478718	31386.692099	32.415757
658.304145	31432.571650	32.420775
658.868686	31483.106636	32.425792
659.481752	31526.857489	32.430810
660.308553	31585.443484	32.435828
660.633481	31634.536893	32.440845
661.208399	31686.417257	32.445863
661.749061	31741.419638	32.450880
662.530132	31782.786916	32.455898
663.483102	31840.981016	32.460916
663.849762	31893.456943	32.465933
664.865548	31949.100260	32.470951
665.475634	31995.849042	32.475968
666.116887	32039.014992	32.480986
666.962100	32100.071361	32.486004
667.385724	32152.482179	32.491021
668.616164	32195.234326	32.496039
668.839419	32254.952932	32.501056
669.776133	32294.697593	32.506074
671.028205	32331.953026	32.511092
671.863154	32375.418256	32.516109
672.502321	32408.432478	32.521127
672.679821	32452.253086	32.526144
673.751593	32478.998362	32.531162
674.487462	32524.887949	32.536180
674.994410	32574.069035	32.541197
676.079397	32599.497460	32.546215
676.570888	32643.794308	32.551232
677.432462	32675.655358	32.556250
678.077585	32702.157566	32.561268
678.678926	32747.828354	32.566285
679.825990	32771.578340	32.571303
680.011830	32798.518839	32.576320
680.740364	32817.959252	32.581338
681.550752	32853.596421	32.586356
681.643838	32889.794172	32.591373
682.301398	32915.466538	32.596391
682.869606	32953.240472	32.601408
683.298421	32993.198296	32.606426
683.696279	33035.892122	32.611444
684.307017	33086.607152	32.616461
684.766893	33140.355079	32.621479
685.313784	33183.898449	32.626496
685.923477	33237.357778	32.631514
686.981132	33282.408682	32.636532
687.266347	33341.551765	32.641549
687.921840	33384.048143	32.646567
688.597671	33444.199145	32.651584
689.258359	33494.755658	32.656602
689.906108	33547.394298	32.661620
690.732217	33612.997384	32.666637
691.695180	33654.713075	32.671655
692.266450	33723.732230	32.676672
692.988285	33764.385611	32.681690
694.008529	33827.727403	32.686708
694.524139	33884.781422	32.691725
695.713649	33935.123908	32.696743
695.815556	33977.284074	32.701760
696.711528	34028.873716	32.706778
698.309838	34062.790748	32.711796
698.796265	34119.691891	32.716813
700.041092	34156.167746	32.721831
700.414471	34203.502041	32.726848
700.848815	34250.928111	32.731866
701.726405	34297.298995	32.736884
701.986644	34344.682832	32.741901
702.802163	34387.611546	32.746919
703.376067	34434.921469	32.751936
704.208333	34491.118570	32.756954
705.083985	34540.752675	32.761972
705.498410	34585.362781	32.766989
706.262842	34636.354790	32.772007
707.003322	34685.289514	32.777024
707.816422	34738.031848	32.782042
708.108805	34782.478017	32.787060
708.908982	34843.707469	32.792077
709.756999	34888.396138	32.797095
710.331550	34955.256507	32.802112
710.757266	35009.906020	32.807130
711.734904	35059.791021	32.812148
712.183265	35118.268795	32.817165
713.018613	35166.020179	32.822183
713.716528	35227.867316	32.827200
714.431304	35283.876172	32.832218
715.316420	35343.418339	32.837236
716.239652	35398.794393	32.842253
717.132958	35445.190648	32.847271
718.242546	35484.952393	32.852288
718.926936	35528.422309	32.857306
719.742257	35573.395721	32.862324
720.648346	35626.214318	32.867341
721.421553	35661.925273	32.872359
721.884161	35704.393137	32.877376
722.894542	35750.676997	32.882394
723.586614	35782.891620	32.887412
724.158313	35835.598401	32.892429
724.679639	35879.676125	32.897447
725.387112	35923.996847	32.902464
725.833733	35972.936038	32.907482
726.795631	36006.632815	32.912500
727.112052	36063.976649	32.917517
727.702492	36108.176870	32.922535
728.597739	36143.294254	32.927552
728.632241	36189.263087	32.932570
729.362006	36234.067854	32.937588
729.822862	36297.883521	32.942605
730.938989	36346.592893	32.947623
731.567735	36398.065528	32.952640
732.136575	36459.544324	32.957658
733.026875	36509.958505	32.962676
734.024339	36560.533170	32.967693
734.710323	36614.229459	32.972711
735.746622	36662.863460	32.977728
736.615737	36698.200814	32.982746
737.744525	36743.760221	32.987764
738.158797	36800.192924	32.992781
738.826381	36834.524884	32.997799
739.616042	36892.170346	33.002816
740.299730	36948.997801	33.007834
740.997487	36986.916874	33.012852
741.238544	37053.690334	33.017869
742.339144	37103.990985	33.022887
743.029749	37154.298667	33.027904
743.195075	37210.600480	33.032922
744.079612	37280.796534	33.037940
745.070418	37331.721847	33.042957
746.095945	37393.005777	33.047975
746.729843	37444.574986	33.052992
747.266102	37515.110575	33.058010
747.559916	37567.978720	33.063028
748.662679	37623.680408	33.068045
749.649327	37689.618923	33.073063
750.597168	37740.090290	33.078080
751.168010	37807.978274	33.083098
752.371405	37866.017245	33.088116
752.785167	37925.039285	33.093133
753.559871	37973.894054	33.098151
754.549807	38030.948620	33.103168
754.929380	38095.294512	33.108186
755.981042	38144.100232	33.113204
756.847970	38219.607547	33.118221
757.920426	38271.464595	33.123239
758.590798	38314.733701	33.128256
759.051469	38376.924119	33.133274
760.045185	38428.623067	33.138292
760.644144	38484.310565	33.143309
761.421642	38548.450425	33.148327
762.103840	38595.335383	33.153344
762.753040	38648.587199	33.158362
763.832170	38703.681976	33.163380
764.707668	38765.125981	33.168397
765.415253	38820.038592	33.173415
766.186619	38870.097427	33.178432
767.111249	38934.980708	33.183450
767.739682	38979.819650	33.188468
768.360504	39035.593703	33.193485
768.837219	39092.560237	33.198503
770.107162	39154.380292	33.203520
770.255577	39207.875865	33.208538
771.533004	39256.250564	33.213556
772.358342	39317.261281	33.218573
773.348683	39371.132107	33.223591
773.884123	39421.368073	33.228608
774.448006	39470.284353	33.233626
775.492009	39533.342211	33.238644
775.837604	39580.351271	33.243661
776.603216	39628.490280	33.248679
777.206889	39688.157925	33.253696
778.311307	39749.265545	33.258714
779.075332	39799.738738	33.263732
779.886676	39846.328054	33.268749
780.915214	39883.524080	33.273767
781.878765	39923.702590	33.278784
782.751207	39978.984576	33.283802
783.341903	40015.091681	33.288820
783.616704	40068.563381	33.293837
784.883218	40116.201787	33.298855
785.548268	40167.734723	33.303872
785.945286	40225.854987	33.308890
786.659355	40281.478604	33.313908
787.389825	40327.904468	33.318925
788.459851	40379.178815	33.323943
789.286974	40438.699906	33.328960
789.858720	40497.944703	33.333978
791.009012	40551.768272	33.338996
791.645995	40608.416603	33.344013
791.963668	40660.485426	33.349031
793.144258	40719.389403	33.354048
793.615565	40787.302242	33.359066
794.280817	40843.643218	33.364084
795.128159	40901.397943	33.369101
795.865596	40969.143434	33.374119
796.825714	41028.354515	33.379136
797.648282	41091.482992	33.384154
798.607663	41151.757020	33.389172
799.706610	41213.546324	33.394189
800.333184	41279.058540	33.399207
801.165990	41332.041714	33.404224
802.250128	41398.159777	33.409242
803.361823	41443.934176	33.414260
804.304740	41498.146537	33.419277
805.027874	41559.811913	33.424295
806.181681	41599.495890	33.429312
806.752651	41650.098297	33.434330
807.747570	41692.172560	33.439348
808.413242	41747.345759	33.444365
809.105010	41796.677434	33.449383
810.116796	41853.106212	33.454400
810.660253	41890.956725	33.459418
811.272754	41959.369845	33.464436
812.107501	42015.434473	33.469453
812.985021	42079.512272	33.474471
814.013496	42132.644018	33.479488
814.344563	42183.322949	33.484506
815.067383	42235.395700	33.489524
816.015001	42300.064080	33.494541
816.806634	42363.435058	33.499559
817.930989	42415.818892	33.504576
818.550965	42484.352655	33.509594
819.283470	42531.250922	33.514612
820.207684	42592.559010	33.519629
820.759711	42654.956155	33.524647
821.762149	42713.469475	33.529664
822.405643	42783.486850	33.534682
823.336307	42833.213758	33.539700
824.033332	42893.172899	33.544717
825.076927	42950.946753	33.549735
825.824816	43012.618681	33.554752
826.557999	43081.819774	33.559770
827.367468	43144.374304	33.564788
828.406405	43207.209540	33.569805
828.995866	43261.740604	33.574823
830.014116	43324.339044	33.579840
830.520019	43393.209641	33.584858
831.529930	43448.896452	33.589876
832.299287	43519.187521	33.594893
833.213039	43577.944643	33.599911
834.116819	43633.907771	33.604928
834.304515	43690.716225	33.609946
835.120043	43749.375240	33.614964
835.980689	43804.928055	33.619981
836.817856	43874.830188	33.624999
837.725427	43928.396223	33.630016
838.297335	43993.627745	33.635034
838.753934	44059.864147	33.640052
839.844819	44126.659836	33.645069
840.689150	44202.868173	33.650087
841.388660	44268.289374	33.655104
842.446714	44344.123360	33.660122
842.935339	44409.419670	33.665140
844.084836	44479.648284	33.670157
844.799109	44557.630208	33.675175
845.988845	44628.953647	33.680192
846.674081	44701.930878	33.685210
847.598618	44765.439861	33.690228
848.766856	44830.005395	33.695245
849.583411	44906.909943	33.700263
850.987972	44959.408001	33.705280
852.083486	45016.230338	33.710298
852.910409	45079.723785	33.715316
854.009333	45137.045616	33.720333
855.120183	45192.847603	33.725351
856.189976	45241.495566	33.730368
856.906949	45296.574754	33.735386
857.964427	45347.982825	33.740404
858.670904	45403.892566	33.745421
859.465487	45457.865738	33.750439
860.565855	45508.084608	33.755456
860.845663	45569.596126	33.760474
861.571205	45626.458632	33.765492
862.620722	45688.261830	33.770509
862.979653	45753.360862	33.775527
863.764765	45820.304115	33.780544
864.643748	45890.528676	33.785562
865.223421	45958.427882	33.790580
866.241903	46029.972231	33.795597
866.903696	46091.179012	33.800615
867.792253	46163.749817	33.805632
868.354335	46246.676500	33.810650
869.505967	46323.249094	33.815668
870.241509	46385.077785	33.820685
870.959018	46457.220699	33.825703
871.997677	46531.831577	33.830720
873.197707	46607.809294	33.835738
874.248564	46678.224647	33.840756
875.578719	46736.950578	33.845773
877.225886	46781.121770	33.850791
878.523266	46828.599074	33.855808
879.142466	46884.930957	33.860826
879.976729	46936.991047	33.865844
880.920591	46990.084324	33.870861
881.371038	47042.223381	33.875879
882.367869	47104.443549	33.880896
883.258489	47159.297842	33.885914
883.509168	47210.026029	33.890932
884.579247	47260.569843	33.895949
885.345227	47330.759557	33.900967
886.054965	47390.229038	33.905984
886.827541	47454.964943	33.911002
887.641006	47534.523326	33.916020
888.720311	47588.988697	33.921037
889.448098	47656.604263	33.926055
890.307494	47715.589486	33.931072
891.164749	47787.449197	33.936090
891.582591	47845.605159	33.941108
892.908483	47903.227688	33.946125
893.759305	47960.930642	33.951143
894.254767	48022.706295	33.956160
895.285653	48087.789708	33.961178
895.845708	48153.047820	33.966196
896.879263	48216.676116	33.971213
898.048199	48285.610371	33.976231
898.635488	48345.360803	33.981248
899.285007	48407.733514	33.986266
900.165406	48474.176344	33.991284
901.399121	48558.708782	33.996301
902.223562	48628.893412	34.001319
903.317217	48689.173272	34.006336
903.928493	48759.372507	34.011354
904.799560	48832.928893	34.016372
906.005747	48897.873459	34.021389
907.061683	48976.532405	34.026407
907.957861	49031.668734	34.031424
909.300955	49103.634124	34.036442
909.630931	49176.598894	34.041460
910.775787	49244.476920	34.046477
911.768585	49315.504214	34.051495
912.611338	49381.791055	34.056512
913.399770	49453.679394	34.061530
914.348819	49515.198684	34.066548
916.037075	49576.615726	34.071565
916.768769	49662.824752	34.076583
917.682278	49729.335678	34.081600
918.514904	49800.041435	34.086618
919.198902	49858.863381	34.091636
920.671508	49920.574318	34.096653
921.500015	49987.092897	34.101671
922.393569	50050.191334	34.106688
923.217857	50112.282091	34.111706
923.930611	50193.491454	34.116724
925.023650	50254.825815	34.121741
925.660964	50328.056430	34.126759
926.888196	50397.551089	34.131776
927.659355	50480.062065	34.136794
928.492248	50561.057886	34.141812
929.581188	50611.321488	34.146829
930.522104	50696.141503	34.151847
931.084504	50771.523747	34.156864
932.005137	50842.820088	34.161882
933.072666	50918.769552	34.166900
934.244980	50989.558961	34.171917
935.337961	51063.581478	34.176935
936.014703	51145.198415	34.181952
937.103209	51210.585449	34.186970
937.640657	51280.949415	34.191988
938.561590	51349.134263	34.197005
939.672008	51439.865610	34.202023
940.312308	51515.383682	34.207040
941.351041	51597.059756	34.212058
942.414752	51672.594688	34.217076
943.695278	51735.776704	34.222093
944.944743	51822.451038	34.227111
945.460658	51882.677357	34.232128
947.042044	51945.819442	34.237146
947.765806	52022.806796	34.242164
948.768172	52078.528682	34.247181
949.767609	52151.715033	34.252199
950.899013	52210.055714	34.257216
951.862689	52275.768907	34.262234
952.589163	52355.528398	34.267252
953.445852	52401.181297	34.272269
954.873714	52466.594983	34.277287
955.306450	52532.189065	34.282304
956.180783	52581.231164	34.287322
957.176745	52650.711647	34.292340
958.445983	52702.742448	34.297357
958.972106	52761.096471	34.302375
959.907805	52819.285643	34.307392
961.006924	52873.602286	34.312410
961.922276	52938.147922	34.317428
962.650412	53007.791386	34.322445
963.593703	53075.313411	34.327463
964.243677	53143.248300	34.332480
965.177276	53207.836135	34.337498
965.884181	53292.910884	34.342516
966.724499	53364.556517	34.347533
967.820237	53438.598830	34.352551
968.570770	53520.617595	34.357568
969.523030	53599.036320	34.362586
970.650802	53686.780633	34.367604
971.284479	53760.731362	34.372621
972.177570	53850.145423	34.377639
973.501918	53936.898224	34.382656
974.806240	54015.617905	34.387674
975.371803	54095.686810	34.392692
976.593426	54176.191748	34.397709
977.633148	54266.603382	34.402727
978.276840	54348.489796	34.407744
979.431439	54424.348545	34.412762
980.118515	54506.241410	34.417780
981.270337	54595.409200	34.422797
983.058722	54679.390388	34.427815
983.703771	54755.164986	34.432832
984.985533	54837.055026	34.437850
986.059901	54921.837997	34.442868
987.130696	54990.155695	34.447885
988.431851	55069.385654	34.452903
989.206334	55151.349418	34.457920
990.741818	55224.126524	34.462938
991.387924	55302.136609	34.467956
992.169370	55371.487671	34.472973
993.074893	55443.971155	34.477991
993.871740	55528.495737	34.483008
995.048259	55598.507404	34.488026
996.154293	55675.915539	34.493044
997.389931	55753.145542	34.498061
998.356381	55832.689622	34.503079
999.225720	55910.160680	34.508096
1000.830384	55983.486260	34.513114
1001.572006	56059.971451	34.518132
1002.704925	56139.528618	34.523149
1003.734979	56218.640076	34.528167
1004.539695	56293.534050	34.533184
1005.589221	56365.510629	34.538202
1006.393248	56437.500325	34.543220
1007.325110	56524.886966	34.548237
1008.529122	56593.346762	34.553255
1009.153367	56674.826544	34.558272
1010.117143	56749.102291	34.563290
1010.885569	56839.065999	34.568308
1011.977794	56915.499359	34.573325
1013.116763	56996.400143	34.578343
1013.848646	57079.573323	34.583360
1015.412263	57161.781919	34.588378
1016.191737	57243.441998	34.593396
1017.012497	57324.159254	34.598413
1018.558554	57402.877872	34.603431
1019.104894	57489.017964	34.608448
1020.545871	57561.842249	34.613466
1021.204816	57640.592142	34.618484
1022.357194	57713.689654	34.623501
1023.525129	57785.329297	34.628519
1024.268975	57851.535251	34.633536
1025.209023	57933.039772	34.638554
1025.964781	58000.351863	34.643572
1026.976130	58070.731933	34.648589
1027.855907	58157.670614	34.653607
1028.987269	58230.779298	34.658624
1030.415742	58308.569822	34.663642
1031.493050	58395.301397	34.668660
1032.152928	58465.389226	34.673677
1033.572892	58549.504701	34.678695
1034.520584	58624.409017	34.683712
1035.486572	58692.804260	34.688730
1036.252853	58778.680545	34.693748
1037.511825	58856.170098	34.698765
1038.368978	58932.602160	34.703783
1039.200615	59033.868369	34.708800
1040.109285	59115.122264	34.713818
1041.292508	59207.106282	34.718836
1042.323173	59300.032159	34.723853
1043.398377	59383.805450	34.728871
1044.915091	59478.675438	34.733888
1045.991752	59563.860589	34.738906
1046.959469	59647.392012	34.743924
1047.761566	59732.196416	34.748941
1048.916385	59827.377278	34.753959
1050.058493	59920.066646	34.758976
1051.020682	59996.219866	34.763994
1052.561118	60085.018466	34.769012
1053.178245	60172.872415	34.774029
1054.581189	60246.229742	34.779047
1055.378199	60345.569933	34.784064
1056.446117	60423.442358	34.789082
1057.962036	60511.948835	34.794100
1058.663898	60606.969048	34.799117
1060.117729	60686.915364	34.804135
1060.934475	60769.176530	34.809152
1062.111141	60853.483442	34.814170
1063.382811	60950.612734	34.819188
1064.252656	61021.238600	34.824205
1065.597671	61108.780054	34.829223
1066.728289	61193.285199	34.834240
1068.152271	61261.293547	34.839258
1069.190812	61347.358052	34.844276
1070.151767	61431.763829	34.849293
1071.716386	61503.447647	34.854311
1072.621084	61581.361821	34.859328
1073.564337	61656.947129	34.864346
1074.644702	61734.625554	34.869364
1075.428970	61815.793860	34.874381
1076.762835	61884.970031	34.879399
1077.711852	61969.265569	34.884416
1078.740365	62039.825354	34.889434
1079.667331	62128.707865	34.894452
1080.950443	62210.926585	34.899469
1082.508982	62293.229310	34.904487
1083.107281	62373.390250	34.909504
1083.987487	62453.558210	34.914522
1085.031356	62529.143189	34.919540
1086.060552	62620.334750	34.924557
1087.121729	62699.576442	34.929575
1087.840498	62783.783993	34.934592
1088.933496	62872.029292	34.939610
1090.261021	62949.780684	34.944628
1091.167033	63042.866752	34.949645
1092.589408	63125.199771	34.954663
1093.561681	63216.864504	34.959680
1094.632880	63279.584141	34.964698
1095.359112	63361.817400	34.969716
1096.634288	63441.642205	34.974733
1097.789942	63518.137046	34.979751
1098.721575	63597.446083	34.984768
1099.809897	63671.533625	34.989786
1100.595302	63761.387269	34.994804
1101.210831	63834.713259	34.999821
1102.477355	63930.202788	35.004839
1103.635363	64019.682835	35.009856
1105.025056	64114.273942	35.014874
1106.245416	64208.448619	35.019892
1106.805478	64301.631224	35.024909
1107.930734	64389.623653	35.029927
1108.885407	64483.125351	35.034944
1110.161102	64571.550815	35.039962
1111.495559	64684.302933	35.044980
1112.434479	64769.806054	35.049997
1113.730981	64847.182014	35.055015
1114.958030	64947.005516	35.060032
1115.958702	65040.989608	35.065050
1117.289751	65135.283487	35.070068
1118.188948	65244.845464	35.075085
1119.649538	65325.084254	35.080103
1120.801699	65426.472395	35.085120
1122.031627	65515.471762	35.090138
1123.536188	65613.994848	35.095156
1124.212295	65706.012351	35.100173
1125.539443	65792.750048	35.105191
1126.679584	65891.172664	35.110208
1128.071619	65976.691657	35.115226
1129.823489	66056.526564	35.120244
1130.870414	66141.985876	35.125261
1132.576773	66217.466220	35.130279
1133.490944	66293.361333	35.135296
1134.358923	66379.976252	35.140314
1135.749688	66471.587732	35.145332
1136.623932	66551.282235	35.150349
1137.677361	66629.397937	35.155367
1138.575443	66715.597784	35.160384
1139.956723	66799.158532	35.165402
1141.228075	66894.114060	35.170420
1141.640055	66983.632120	35.175437
1143.073797	67074.510981	35.180455
1144.258928	67165.701114	35.185472
1145.220740	67259.914764	35.190490
1146.198776	67350.491989	35.195508
1147.536141	67441.178222	35.200525
1148.848996	67534.907707	35.205543
1149.773757	67628.470010	35.210560
1151.263103	67705.419479	35.215578
1152.978315	67792.363197	35.220596
1154.002147	67873.969676	35.225613
1155.165803	67955.801584	35.230631
1156.409716	68047.802494	35.235648
1157.360943	68131.497865	35.240666
1158.185957	68220.006218	35.245684
1158.986271	68313.641049	35.250701
1160.809325	68392.687082	35.255719
1161.407170	68484.156950	35.260736
1162.687572	68572.051106	35.265754
1165.258337	68639.818657	35.270772
1166.196239	68727.469064	35.275789
1167.281147	68805.295258	35.280807
1168.480225	68886.953664	35.285824
1169.481383	68960.335762	35.290842
1170.451280	69032.190627	35.295860
1171.440008	69122.284894	35.300877
1172.747040	69191.877902	35.305895
1173.750642	69264.715943	35.310912
1174.577361	69340.931315	35.315930
1175.427668	69412.539912	35.320948
1176.318732	69489.923450	35.325965
1177.430274	69575.219545	35.330983
1178.514314	69660.931783	35.336000
1179.413502	69750.902875	35.341018
1180.854770	69844.069906	35.346036
1181.274144	69951.231927	35.351053
1182.549395	70038.517667	35.356071
1183.730753	70135.601448	35.361088
1184.808370	70241.110835	35.366106
1186.467816	70332.700617	35.371124
1187.491410	70431.488086	35.376141
1188.505728	70535.507789	35.381159
1189.882855	70641.865025	35.386176
1190.948946	70744.269112	35.391194
1192.311884	70837.762181	35.396212
1193.616052	70948.627955	35.401229
1194.468747	71045.734625	35.406247
1196.027067	71155.282584	35.411264
1197.126270	71261.191678	35.416282
1198.316453	71361.020579	35.421300
1199.606189	71469.015887	35.426317
1201.035593	71566.870608	35.431335
1202.766030	71676.292637	35.436352
1203.612759	71780.685336	35.441370
1205.153944	71873.483114	35.446388
1206.329194	71974.899813	35.451405
1207.696991	72067.066677	35.456423
1209.330265	72157.647384	35.461440
1209.850099	72259.686473	35.466458
1211.335294	72360.499142	35.471476
1212.369635	72465.156657	35.476493
1213.513460	72556.410192	35.481511
1215.319286	72651.170659	35.486528
1216.292778	72752.431774	35.491546
1217.824305	72853.999050	35.496564
1218.823810	72964.325471	35.501581
1219.787361	73053.252979	35.506599
1221.597172	73159.945703	35.511616
1222.436294	73246.182766	35.516634
1223.758773	73341.058938	35.521652
1224.924918	73448.448305	35.526669
1226.488293	73544.946936	35.531687
1227.624273	73641.309789	35.536704
1228.771471	73742.344993	35.541722
1229.905140	73835.187764	35.546740
1231.197384	73942.901484	35.551757
1232.445419	74032.826611	35.556775
1233.615648	74136.456282	35.561792
1234.769275	74238.898315	35.566810
1236.103127	74337.436810	35.571828
1237.393007	74430.611997	35.576845
1238.881578	74540.590175	35.581863
1240.023926	74626.087858	35.586880
1240.985679	74725.281023	35.591898
1242.294437	74823.343891	35.596916
1243.466187	74927.495718	35.601933
1244.842868	75023.078769	35.606951
1246.174623	75116.921157	35.611968
1247.385571	75230.466705	35.616986
1248.852545	75315.840061	35.622004
1250.297240	75417.835964	35.627021
1250.836974	75509.560984	35.632039
1252.330642	75605.685238	35.637056
1253.544288	75704.880815	35.642074
1255.240648	75791.372666	35.647092
1256.046299	75873.886662	35.652109
1257.286003	75956.713361	35.657127
1258.511926	76038.731767	35.662144
1259.469819	76126.048991	35.667162
1261.017113	76216.137533	35.672180
1261.911201	76306.784067	35.677197
1263.466404	76395.288575	35.682215
1264.530100	76482.248466	35.687232
1265.448142	76582.227978	35.692250
1266.753857	76685.428365	35.697268
1268.250486	76775.019959	35.702285
1269.539583	76877.083596	35.707303
1270.818248	76970.345322	35.712320
1272.158083	77076.784768	35.717338
1273.774786	77172.794104	35.722356
1274.845879	77267.444592	35.727373
1275.577528	77363.921720	35.732391
1276.873292	77463.072949	35.737408
1278.012085	77584.962309	35.742426
1279.327698	77676.282531	35.747444
1280.529647	77794.920033	35.752461
1281.948064	77899.196918	35.757479
1283.554803	78014.440699	35.762496
1284.911810	78128.444365	35.767514
1286.076140	78231.621942	35.772532
1287.623484	78340.973015	35.777549
1288.662350	78445.602425	35.782567
1290.127940	78552.876816	35.787584
1291.233375	78664.210864	35.792602
1292.670522	78768.184100	35.797620
1293.754499	78887.186733	35.802637
1295.404904	78993.597964	35.807655
1297.371895	79096.691859	35.812672
1298.158144	79204.606607	35.817690
1299.698578	79306.893554	35.822708
1300.694708	79418.399684	35.827725
1302.296326	79524.415160	35.832743
1304.295822	79613.836425	35.837760
1305.756755	79719.912555	35.842778
1307.537453	79809.026452	35.847796
1308.415158	79904.488924	35.852813
1309.321097	79995.120481	35.857831
1311.050317	80090.881799	35.862848
1312.206934	80192.598314	35.867866
1313.239493	80284.300639	35.872884
1314.503750	80387.610080	35.877901
1315.752963	80498.219662	35.882919
1316.665795	80601.381890	35.887936
1317.649489	80715.999115	35.892954
1319.147547	80821.604911	35.897972
1320.641994	80934.889279	35.902989
1322.151742	81043.838799	35.908007
1323.579338	81146.732878	35.913024
1324.387797	81257.781486	35.918042
1326.068895	81363.576222	35.923060
1327.435097	81469.699103	35.928077
1329.095044	81571.380308	35.933095
1330.419295	81673.240830	35.938112
1331.593950	81788.174803	35.943130
1332.760314	81882.699560	35.948148
1334.501525	81993.631236	35.953165
1335.552893	82103.467088	35.958183
1336.843438	82197.530129	35.963200
1337.880657	82306.000624	35.968218
1339.417044	82414.444521	35.973236
1340.574167	82528.839435	35.978253
1341.695467	82627.972931	35.983271
1343.279700	82729.860159	35.988288
1344.486253	82834.087171	35.993306
1345.184764	82924.671794	35.998324
1346.878179	83033.309018	36.003341
1347.740846	83136.843124	36.008359
1348.841666	83242.595863	36.013376
1350.533401	83369.720698	36.018394
1351.927284	83472.476472	36.023412
1353.458225	83571.384790	36.028429
1354.795432	83678.230032	36.033447
1355.971825	83780.095819	36.038464
1357.420977	83899.772457	36.043482
1358.769478	84005.172713	36.048500
1359.936836	84122.575409	36.053517
1361.361814	84235.148927	36.058535
1363.247123	84351.477835	36.063552
1364.325261	84466.196938	36.068570
1365.817827	84572.337115	36.073588
1367.343075	84693.183630	36.078605
1369.097768	84804.035492	36.083623
1370.189672	84909.795795	36.088640
1371.789467	85027.515024	36.093658
1372.904344	85145.462267	36.098676
1374.581497	85248.383071	36.103693
1375.896420	85363.512396	36.108711
1377.885836	85455.690765	36.113728
1378.916028	85567.481975	36.118746
1380.026891	85680.198748	36.123764
1381.736534	85794.875542	36.128781
1382.901345	85906.038878	36.133799
1384.451169	86023.199731	36.138816
1386.154082	86130.757474	36.143834
1387.462256	86241.038110	36.148852
1388.842732	86356.085154	36.153869
1389.650488	86466.102397	36.158887
1391.192834	86582.404993	36.163904
1392.647549	86703.980524	36.168922
1393.657131	86818.415517	36.173940
1395.551013	86941.482333	36.178957
1396.472861	87065.702054	36.183975
1398.351342	87178.305163	36.188992
1399.942296	87301.268582	36.194010
1400.981353	87416.664415	36.199028
1402.901008	87526.208459	36.204045
1404.001733	87656.041993	36.209063
1404.919576	87770.710422	36.214080
1406.398021	87890.234276	36.219098
1407.989910	88011.033549	36.224116
1409.562512	88125.233949	36.229133
1411.096101	88247.323190	36.234151
1412.801107	88373.124675	36.239168
1414.300132	88489.061414	36.244186
1415.657542	88601.561003	36.249204
1417.021952	88723.754586	36.254221
1418.160464	88844.906647	36.259239
1419.851208	88962.767017	36.264256
1420.860052	89081.988611	36.269274
1422.547771	89194.755868	36.274292
1423.915191	89321.792522	36.279309
1425.585964	89445.259392	36.284327
1426.515460	89556.637945	36.289344
1427.805615	89685.006182	36.294362
1429.727356	89800.818896	36.299380
1430.927611	89920.901188	36.304397
1432.215072	90052.135584	36.309415
1433.911785	90165.196610	36.314432
1435.267174	90277.715539	36.319450
1436.614162	90394.139627	36.324468
1438.449748	90507.649253	36.329485
1439.241276	90616.974782	36.334503
1440.607991	90715.958238	36.339520
1442.315467	90827.017663	36.344538
1443.378601	90937.784903	36.349556
1444.897729	91047.581743	36.354573
1446.034681	91160.999802	36.359591
1447.499666	91272.783003	36.364608
1449.343607	91396.053545	36.369626
1450.327639	91514.845119	36.374644
1451.680367	91630.335234	36.379661
1453.044328	91756.102687	36.384679
1454.490790	91877.916179	36.389696
1456.301305	92003.589809	36.394714
1457.495383	92120.868197	36.399732
1459.400299	92242.079484	36.404749
1460.788115	92374.068843	36.409767
1462.189660	92498.857609	36.414784
1463.957506	92617.011861	36.419802
1464.907500	92751.935421	36.424820
1466.682322	92875.134023	36.429837
1468.057962	93009.193978	36.434855
1469.593118	93141.151057	36.439872
1471.579725	93276.625372	36.444890
1472.813001	93395.791097	36.449908
1474.111873	93515.973734	36.454925
1475.380521	93651.409358	36.459943
1477.035752	93779.738177	36.464960
1478.795672	93916.175871	36.469978
1480.073404	94057.619794	36.474996
1481.572358	94183.807201	36.480013
1482.804853	94310.264751	36.485031
1484.826881	94451.391835	36.490048
1486.348392	94579.478625	36.495066
1487.814060	94710.756129	36.500084
1489.507557	94833.823153	36.505101
1491.353379	94961.037153	36.510119
1492.955327	95081.660391	36.515136
1494.905717	95202.204516	36.520154
1496.994098	95332.753963	36.525172
1498.209690	95430.774881	36.530189
1499.648441	95547.166344	36.535207
1501.101706	95664.696793	36.540224
1502.594832	95786.505868	36.545242
1503.651267	95902.311704	36.550260
1504.866225	96027.093112	36.555277
1506.418732	96158.540681	36.560295
1507.935724	96289.119693	36.565312
1509.398184	96407.766988	36.570330
1510.796454	96545.857038	36.575348
1512.605070	96669.940162	36.580365
1514.210501	96787.831432	36.585383
1515.617345	96921.764040	36.590400
1517.071580	97036.738909	36.595418
1518.529223	97164.301188	36.600436
1520.583679	97292.582376	36.605453
1522.205700	97416.621432	36.610471
1523.318295	97531.017461	36.615488
1525.160389	97659.878282	36.620506
1526.167871	97785.117285	36.625524
1527.860898	97906.789383	36.630541
1529.261500	98044.796901	36.635559
1530.624814	98161.780244	36.640576
1532.182697	98290.649838	36.645594
1533.811275	98417.708851	36.650612
1535.483027	98540.286738	36.655629
1537.196532	98670.274561	36.660647
1538.762668	98787.482175	36.665664
1540.377108	98884.779894	36.670682
1542.328799	98994.639019	36.675700
1543.740763	99093.769023	36.680717
1545.145318	99192.228602	36.685735
1546.666509	99283.152809	36.690752
1548.157032	99391.069416	36.695770
1549.225121	99500.877650	36.700788
1550.844195	99601.143291	36.705805
1552.086397	99718.569539	36.710823
1553.543676	99845.242538	36.715840
1555.171699	99968.606023	36.720858
1556.653863	100089.926262	36.725876
1558.582245	100198.056333	36.730893
1559.897923	100321.989560	36.735911
1561.027117	100443.264646	36.740928
1563.062460	100581.387145	36.745946
1564.197470	100702.700330	36.750964
1565.857545	100828.914585	36.755981
1567.219536	100955.530704	36.760999
1568.726563	101083.316456	36.766016
1570.226451	101227.559684	36.771034
1571.694074	101372.594604	36.776052
1573.070611	101516.300481	36.781069
1574.654539	101645.902100	36.786087
1576.283214	101795.465245	36.791104
1578.066071	101947.312498	36.796122
1579.048815	102098.473583	36.801140
1580.436834	102246.466113	36.806157
1582.421111	102391.057466	36.811175
1584.064221	102544.197065	36.816192
1586.066422	102689.636394	36.821210
1587.669860	102838.168588	36.826228
1589.104934	102980.071422	36.831245
1590.906471	103125.391763	36.836263
1592.388975	103283.643910	36.841280
1594.467382	103414.722339	36.846298
1595.724484	103574.443652	36.851316
1597.507402	103723.091352	36.856333
1599.030646	103876.230421	36.861351
1600.557029	104018.808150	36.866368
1602.283676	104161.596222	36.871386
1604.014576	104314.007639	36.876404
1605.505854	104452.332527	36.881421
1607.174287	104601.762713	36.886439
1608.987206	104759.133625	36.891456
1610.776331	104898.631205	36.896474
1612.293503	105045.170680	36.901492
1614.142188	105195.741957	36.906509
1615.913684	105341.292186	36.911527
1617.579976	105489.585509	36.916544
1619.642529	105620.598990	36.921562
1620.908526	105768.042913	36.926580
1622.557556	105900.098169	36.931597
1624.157513	106046.299441	36.936615
1625.893010	106180.434483	36.941632
1627.562890	106313.109413	36.946650
1629.757264	106450.889287	36.951668
1631.454396	106590.319420	36.956685
1632.956940	106723.351674	36.961703
1634.379777	106856.371494	36.966720
1636.163243	106986.114971	36.971738
1637.879812	107129.880864	36.976756
1639.347743	107258.545957	36.981773
1640.809770	107395.594066	36.986791
1642.339982	107530.755433	36.991808
1643.917134	107665.580339	36.996826
1645.612209	107806.359867	37.001844
1646.994069	107928.434406	37.006861
1648.352283	108053.429561	37.011879
1649.753619	108183.997874	37.016896
1650.875561	108309.220937	37.021914
1652.556416	108447.963734	37.026932
1654.159792	108581.799059	37.031949
1656.188002	108710.306296	37.036967
1657.398092	108853.689037	37.041984
1659.518887	108982.423808	37.047002
1661.137536	109132.807312	37.052020
1662.687883	109260.782283	37.057037
1664.477040	109391.738619	37.062055
1666.057020	109540.240443	37.067072
1667.833719	109674.623647	37.072090
1669.237450	109823.965696	37.077108
1671.272731	109957.181124	37.082125
1672.837868	110108.325348	37.087143
1674.146915	110259.611532	37.092160
1676.061596	110412.148324	37.097178
1677.570423	110552.283174	37.102196
1679.190491	110700.568092	37.107213
1680.764669	110853.159791	37.112231
1682.454796	111003.628972	37.117248
1684.153417	111169.898710	37.122266
1686.041106	111336.101758	37.127284
1687.415615	111490.705618	37.132301
1689.463324	111652.472016	37.137319
1690.749494	111816.982809	37.142336
1692.871059	111973.793269	37.147354
1694.363315	112138.286152	37.152372
1695.821886	112305.511660	37.157389
1698.038061	112455.993890	37.162407
1699.560534	112631.695258	37.167424
1701.584546	112786.799704	37.172442
1702.937855	112963.340681	37.177460
1704.879885	113116.506250	37.182477
1706.547839	113281.141899	37.187495
1708.509572	113448.002722	37.192512
1710.050434	113604.339984	37.197530
1712.158050	113776.113085	37.202548
1713.602312	113941.623602	37.207565
1716.218611	114098.899001	37.212583
1717.538120	114272.116103	37.217600
1719.221845	114428.713701	37.222618
1720.924853	114591.181098	37.227636
1722.370937	114757.062841	37.232653
1724.304322	114914.549514	37.237671
1725.587439	115080.901990	37.242688
1727.396003	115252.690548	37.247706
1729.179537	115418.953988	37.252724
1731.124283	115576.276855	37.257741
1733.213180	115742.405450	37.262759
1734.709032	115912.419381	37.267776
1736.356171	116068.332095	37.272794
1738.214886	116243.503905	37.277812
1739.741621	116411.333786	37.282829
1741.753405	116572.772569	37.287847
1743.659308	116747.241823	37.292864
1745.569262	116910.194575	37.297882
1746.824347	117069.952219	37.302900
1748.378685	117233.595913	37.307917
1750.393957	117402.039141	37.312935
1752.308284	117571.044241	37.317952
1754.294393	117724.158746	37.322970
1755.870017	117891.924254	37.327988
1757.703806	118054.805055	37.333005
1759.287055	118216.863042	37.338023
1760.915174	118383.214640	37.343040
1762.810205	118530.220191	37.348058
1764.746801	118685.984608	37.353076
1766.039353	118838.336372	37.358093
1767.907479	118987.504203	37.363111
1769.371965	119138.003875	37.368128
1770.748831	119283.076181	37.373146
1772.471306	119445.054325	37.378164
1773.595590	119594.226143	37.383181
1775.558722	119760.531629	37.388199
1777.324634	119940.517149	37.393216
1778.949099	120114.487636	37.398234
1780.638316	120281.028281	37.403252
1782.238015	120463.617115	37.408269
1783.981396	120634.450993	37.413287
1785.497265	120824.322983	37.418304
1787.340308	121006.356429	37.423322
1789.478255	121193.786698	37.428340
1791.052389	121387.977967	37.433357
1793.159898	121567.359760	37.438375
1794.754411	121757.515831	37.443392
1796.461597	121944.471294	37.448410
1798.276092	122142.840413	37.453428
1799.899673	122322.389788	37.458445
1802.096795	122525.889609	37.463463
1803.981602	122717.451296	37.468480
1805.660654	122912.103157	37.473498
1807.597195	123112.843058	37.478516
1808.762353	123319.577506	37.483533
1811.464492	123509.189086	37.488551
1812.716271	123711.814599	37.493568
1815.053042	123909.350158	37.498586
1817.171039	124107.973679	37.503604
1819.084495	124296.455849	37.508621
1821.013056	124494.451101	37.513639
1823.464486	124691.059283	37.518656
1825.332631	124867.626237	37.523674
1827.112530	125065.000444	37.528692
1828.387357	125248.917941	37.533709
1830.796278	125433.674677	37.538727
1832.453974	125639.164605	37.543744
1834.250066	125832.759485	37.548762
1835.904212	126023.408728	37.553780
1837.692767	126221.358114	37.558797
1839.885843	126399.746105	37.563815
1841.951749	126600.432541	37.568832
1843.883196	126791.828791	37.573850
1845.754266	126980.203176	37.578868
1847.464377	127176.469351	37.583885
1849.601526	127361.670408	37.588903
1851.054830	127547.879504	37.593920
1853.018441	127740.708790	37.598938
1855.161076	127932.749882	37.603956
1856.895038	128118.156634	37.608973
1858.826716	128314.139975	37.613991
1860.624182	128505.920254	37.619008
1862.148559	128688.215709	37.624026
1864.916970	128873.198384	37.629044
1866.138248	129078.874874	37.634061
1868.067250	129253.649578	37.639079
1869.993786	129453.673687	37.644096
1871.737722	129639.681938	37.649114
1873.654084	129834.241059	37.654132
1875.202812	130033.628890	37.659149
1877.347468	130222.127574	37.664167
1879.040954	130426.328777	37.669184
1880.405977	130613.948193	37.674202
1882.613933	130810.585285	37.679220
1884.399824	131018.632089	37.684237
1886.383971	131205.599467	37.689255
1887.635883	131389.128933	37.694272
1889.451137	131574.360544	37.699290
1891.350741	131760.074666	37.704308
1892.695950	131951.687124	37.709325
1894.746151	132142.645107	37.714343
1896.601745	132327.594521	37.719360
1898.534396	132522.011035	37.724378
1900.503553	132723.287243	37.729396
1902.177759	132926.335934	37.734413
1903.861415	133124.752732	37.739431
1905.671055	133331.017831	37.744448
1907.311567	133539.835290	37.749466
1909.553030	133743.878024	37.754484
1911.039461	133976.107083	37.759501
1913.208174	134175.557056	37.764519
1915.591706	134384.745047	37.769536
1917.266284	134595.084865	37.774554
1919.422178	134806.074049	37.779572
1921.552545	135032.346016	37.784589
1923.718497	135245.327914	37.789607
1925.168405	135461.924520	37.794624
1927.514404	135666.632324	37.799642
1929.093135	135887.614148	37.804660
1931.078481	136108.076945	37.809677
1933.374408	136323.733885	37.814695
1935.068656	136546.414034	37.819712
1937.052407	136770.623738	37.824730
1939.471054	136983.117655	37.829748
1941.233364	137201.425127	37.834765
1943.148195	137420.737780	37.839783
1944.812663	137644.887243	37.844800
1946.615974	137872.797809	37.849818
1949.209514	138093.568902	37.854836
1950.875340	138341.439272	37.859853
1952.488294	138555.233318	37.864871
1955.184450	138786.321552	37.869888
1956.748373	139021.419619	37.874906
1959.000389	139240.916819	37.879924
1961.028359	139458.774776	37.884941
1963.086107	139684.027667	37.889959
1965.239231	139911.525709	37.894976
1966.930599	140137.523071	37.899994
1969.235426	140354.377580	37.905012
1971.407895	140590.378619	37.910029
1973.267132	140811.416357	37.915047
1975.729142	141029.620080	37.920064
1977.056279	141260.324299	37.925082
1979.389320	141476.684559	37.930100
1981.077605	141699.605872	37.935117
1983.055255	141917.559034	37.940135
1985.261528	142146.709261	37.945152
1987.214157	142376.369618	37.950170
1989.329663	142603.670515	37.955188
1991.198326	142832.115032	37.960205
1993.029651	143054.106508	37.965223
1995.059718	143277.134137	37.970240
1996.974999	143512.618311	37.975258
1999.099642	143742.588269	37.980276
2000.871167	143970.786657	37.985293
2002.765110	144195.959112	37.990311
2004.623263	144433.169921	37.995328
2006.603179	144676.010755	38.000346
2008.856695	144898.008229	38.005364
2010.397970	145137.429301	38.010381
2012.645021	145384.103014	38.015399
2014.491772	145606.319216	38.020416
2016.413642	145849.745877	38.025434
2018.642426	146079.126492	38.030452
2020.494100	146289.020833	38.035469
2022.601020	146503.585137	38.040487
2024.448729	146727.100682	38.045504
2026.138148	146935.614074	38.050522
2029.018821	147140.871347	38.055540
2030.949811	147367.219806	38.060557
2033.199868	147589.800687	38.065575
2035.178017	147799.643414	38.070592
2036.756440	148021.772196	38.075610
2038.915529	148232.972001	38.080628
2040.448545	148464.794242	38.085645
2042.181886	148688.957960	38.090663
2044.237401	148923.899486	38.095680
2046.178049	149166.221815	38.100698
2048.252216	149404.107320	38.105716
2049.944378	149653.768995	38.110733
2051.963197	149893.175764	38.115751
2054.166881	150155.884814	38.120768
2056.007234	150400.348102	38.125786
2058.103546	150656.348909	38.130804
2060.064643	150907.294644	38.135821
2062.171798	151166.748754	38.140839
2064.534643	151426.646656	38.145856
2066.238393	151687.549607	38.150874
2068.521349	151942.778490	38.155892
2070.261563	152205.544174	38.160909
2072.263437	152477.549461	38.165927
2074.685108	152748.322923	38.170944
2076.352176	153024.470374	38.175962
2078.682205	153291.617614	38.180980
2080.876218	153579.478389	38.185997
2082.817577	153850.509644	38.191015
2085.041529	154130.853731	38.196032
2087.017763	154408.673544	38.201050
2088.841446	154689.285782	38.206068
2091.481930	154964.732665	38.211085
2093.762186	155249.300659	38.216103
2096.033867	155518.676244	38.221120
2097.704990	155809.993641	38.226138
2099.825358	156082.315107	38.231156
2101.813260	156369.079458	38.236173
2104.005313	156652.766733	38.241191
2106.482280	156925.645961	38.246208
2108.875863	157212.008525	38.251226
2111.138832	157474.983623	38.256244
2113.390173	157762.995910	38.261261
2115.256052	158043.973124	38.266279
2117.241396	158316.313183	38.271296
2119.540205	158589.887883	38.276314
2122.108259	158863.739293	38.281332
2124.577032	159134.040057	38.286349
2126.613958	159411.416969	38.291367
2129.140573	159662.058921	38.296384
2131.484100	159929.869031	38.301402
2133.616665	160189.791238	38.306420
2136.254809	160458.636888	38.311437
2138.636495	160710.791005	38.316455
2140.317962	160973.122648	38.321472
2142.104341	161240.390326	38.326490
2144.171662	161494.513544	38.331508
2146.216882	161766.961061	38.336525
2148.032886	162039.902464	38.341543
2150.039227	162299.891117	38.346560
2151.978734	162587.301509	38.351578
2154.088993	162859.464247	38.356596
2156.612201	163128.885021	38.361613
2158.294700	163393.803718	38.366631
2160.760589	163655.694180	38.371648
2162.459981	163915.419684	38.376666
2164.608854	164164.170281	38.381684
2166.993015	164422.889788	38.386701
2168.781695	164675.265990	38.391719
2170.998875	164929.277762	38.396736
2172.872301	165182.925019	38.401754
2174.743983	165446.578248	38.406772
2176.686065	165718.118728	38.411789
2178.716581	165986.980274	38.416807
2181.069416	166265.061184	38.421824
2182.688958	166542.254317	38.426842
2185.004325	166831.846460	38.431860
2187.672739	167105.971097	38.436877
2189.418759	167397.825348	38.441895
2191.859480	167667.645352	38.446912
2193.938222	167966.573094	38.451930
2196.176581	168250.990109	38.456948
2198.339728	168552.344998	38.461965
2200.238452	168842.810201	38.466983
2202.593865	169134.424427	38.472000
2204.828561	169438.476387	38.477018
2207.288353	169739.269518	38.482036
2209.474786	170037.097199	38.487053
2211.732221	170350.723133	38.492071
2213.947810	170646.961599	38.497088
2216.607421	170948.147610	38.502106
2218.866567	171249.879668	38.507124
2221.258936	171548.874955	38.512141
2223.749079	171843.856500	38.517159
2226.158080	172131.753888	38.522176
2228.517327	172425.856545	38.527194
2231.075001	172713.479045	38.532212
2233.224208	173016.720885	38.537229
2235.404684	173319.717793	38.542247
2237.686792	173612.719589	38.547264
2239.790093	173907.642294	38.552282
2242.111554	174201.579812	38.557300
2244.309892	174501.048497	38.562317
2246.610827	174801.137245	38.567335
2248.847635	175099.421279	38.572352
2250.876200	175417.408177	38.577370
2253.383100	175716.401649	38.582388
2255.493975	176022.898992	38.587405
2257.170228	176328.042919	38.592423
2259.734476	176637.875128	38.597440
2261.953797	176949.832005	38.602458
2264.262524	177260.709471	38.607476
2266.578539	177571.332986	38.612493
2268.671874	177889.865351	38.617511
2270.918214	178212.844978	38.622528
2273.374425	178528.148623	38.627546
2275.172589	178845.739994	38.632564
2277.850587	179161.595569	38.637581
2279.894197	179482.122550	38.642599
2282.321474	179793.270105	38.647616
2284.332263	180120.306273	38.652634
2286.347032	180452.828921	38.657652
2288.903964	180772.036180	38.662669
2291.370757	181104.262304	38.667687
2293.644522	181433.040158	38.672704
2295.756981	181755.443983	38.677722
2297.880675	182086.558746	38.682740
2300.016703	182415.539314	38.687757
2301.860591	182750.306521	38.692775
2304.005632	183081.675453	38.697792
2306.157705	183430.594808	38.702810
2308.624097	183776.190093	38.707828
2311.044163	184109.856439	38.712845
2313.243643	184438.935677	38.717863
2315.713185	184757.662052	38.722880
2317.854492	185073.468858	38.727898
2319.947790	185383.721750	38.732916
2322.900164	185710.376708	38.737933
2324.719591	186032.256195	38.742951
2326.953707	186353.792764	38.747968
2329.228633	186744.257783	38.752986
2331.547084	187077.136976	38.758004
2334.000600	187405.043300	38.763021
2336.393399	187739.411580	38.768039
2338.950420	188062.833493	38.773056
2341.283659	188399.245068	38.778074
2343.302543	188742.081957	38.783092
2345.818252	189069.602660	38.788109
2348.230173	189412.304264	38.793127
2350.581547	189741.224114	38.798144
2352.712195	190090.397770	38.803162
2355.079831	190434.049169	38.808180
2357.527638	190783.505780	38.813197
2359.591746	191141.786276	38.818215
2362.092063	191488.849190	38.823232
2364.121800	191838.551803	38.828250
2366.632819	192208.882007	38.833268
2369.140645	192569.231381	38.838285
2371.180922	192939.967274	38.843303
2373.645908	193303.068739	38.848320
2376.506805	193677.235228	38.853338
2378.445275	194048.879273	38.858356
2380.430671	194414.090632	38.863373
2383.105669	194808.584772	38.868391
2385.737971	195179.539850	38.873408
2388.441995	195550.306991	38.878426
2390.699390	195920.255614	38.883444
2393.609025	196281.391062	38.888461
2395.847340	196660.209733	38.893479
2398.097831	197022.084722	38.898496
2400.940423	197403.757930	38.903514
2403.223915	197774.164626	38.908532
2406.148260	198148.231987	38.913549
2408.342151	198531.406204	38.918567
2410.567561	198897.455657	38.923584
2413.233805	199271.388186	38.928602
2415.452577	199648.668116	38.933620
2418.578069	200014.097519	38.938637
2420.988843	200397.318846	38.943655
2423.206042	200762.789713	38.948672
2425.825895	201134.676299	38.953690
2428.012925	201499.594655	38.958708
2430.928939	201866.432543	38.963725
2433.352965	202233.855834	38.968743
2435.916532	202610.428465	38.973760
2438.401482	202975.125780	38.978778
2440.773661	203339.561962	38.983796
2443.550543	203706.831790	38.988813
2446.046887	204077.067309	38.993831
2448.489844	204432.121069	38.998848
2451.003537	204788.561632	39.003866
2452.858430	205154.987052	39.008884
2455.909439	205522.624163	39.013901
2458.161940	205890.157589	39.018919
2460.531970	206261.560030	39.023936
2462.728186	206624.073746	39.028954
2464.814810	207002.863053	39.033972
2467.095153	207367.295561	39.038989
2469.497862	207743.242625	39.044007
2471.914302	208122.515988	39.049024
2474.682963	208493.733166	39.054042
2477.000263	208844.215950	39.059060
2479.302723	209182.889051	39.064077
2481.908266	209551.643734	39.069095
2484.195774	209887.017699	39.074112
2486.257945	210243.791381	39.079130
2488.707075	210598.803304	39.084148
2491.288373	210959.180652	39.089165
2493.162420	211334.427939	39.094183
2495.657916	211700.332149	39.099200
2498.293569	212073.378801	39.104218
2500.405815	212453.239316	39.109236
2502.804592	212824.494709	39.114253
2505.489496	213226.927041	39.119271
2507.656340	213606.399400	39.124288
2510.188214	213996.459518	39.129306
2512.254807	214394.315208	39.134324
2515.012911	214792.597205	39.139341
2517.531127	215210.173003	39.144359
2519.953317	215609.498887	39.149376
2522.779259	216008.254261	39.154394
2525.171609	216431.033300	39.159412
2527.876410	216838.471011	39.164429
2530.738502	217256.071561	39.169447
2533.419317	217651.904152	39.174464
2535.775470	218059.041513	39.179482
2538.217142	218472.694692	39.184500
2540.733073	218889.410501	39.189517
2543.491066	219312.998814	39.194535
2545.990835	219731.013320	39.199552
2548.446293	220165.852430	39.204570
2551.092518	220590.678338	39.209588
2553.711038	221010.377177	39.214605
2556.394203	221433.343284	39.219623
2558.830199	221867.551236	39.224640
2562.320579	222288.563004	39.229658
2564.632419	222710.596667	39.234676
2567.829221	223127.538952	39.239693
2570.556357	223547.831570	39.244711
2572.999556	223961.944473	39.249728
2575.604411	224380.147760	39.254746
2578.314611	224803.364727	39.259764
2581.230816	225204.346499	39.264781
2583.672829	225626.309664	39.269799
2586.210338	226040.941597	39.274816
2589.311050	226448.144091	39.279834
2591.807680	226867.609130	39.284852
2594.382208	227279.440775	39.289869
2597.117078	227698.030299	39.294887
2599.380904	228112.171120	39.299904
2602.208518	228516.037075	39.304922
2604.924173	228938.643144	39.309940
2607.339203	229361.499094	39.314957
2610.022904	229771.077569	39.319975
2612.475066	230191.691864	39.324992
2615.257883	230592.871240	39.330010
2617.350427	231020.882874	39.335028
2619.945153	231439.797705	39.340045
2622.173363	231863.367454	39.345063
2624.837675	232292.229310	39.350080
2627.666540	232712.554943	39.355098
2630.085727	233161.472649	39.360116
2632.506159	233584.579426	39.365133
2635.204269	234024.968105	39.370151
2637.293000	234457.601432	39.375168
2640.343367	234882.285733	39.380186
2643.038657	235337.204628	39.385204
2645.628231	235758.479470	39.390221
2648.415150	236194.889218	39.395239
2650.649131	236606.742906	39.400256
2653.384336	237009.855481	39.405274
2655.634226	237421.197718	39.410292
2658.731012	237827.276143	39.415309
2661.857964	238230.300955	39.420327
2664.113500	238633.156040	39.425344
2666.924518	239040.979480	39.430362
2669.129097	239451.437109	39.435380
2671.565034	239879.208753	39.440397
2674.130645	240309.347512	39.445415
2676.616187	240734.214166	39.450432
2679.684110	241163.181088	39.455450
2682.237136	241605.716612	39.460468
2684.834546	242025.406923	39.465485
2687.471667	242465.387543	39.470503
2690.259919	242903.845068	39.475520
2693.481672	243323.664627	39.480538
2696.316718	243770.089850	39.485556
2699.351191	244198.142161	39.490573
2702.000170	244632.147134	39.495591
2704.791974	245068.262861	39.500608
2707.629198	245501.144456	39.505626
2710.493401	245939.076115	39.510644
2713.079970	246376.897618	39.515661
2716.183767	246821.089959	39.520679
2718.638285	247256.262767	39.525696
2721.368618	247693.627089	39.530714
2723.790385	248143.307838	39.535732
2726.452760	248588.479202	39.540749
2728.959827	249039.287565	39.545767
2731.660424	249498.295020	39.550784
2734.434110	249959.398270	39.555802
2737.234046	250414.018613	39.560820
2739.848630	250883.221987	39.565837
2742.458776	251350.976782	39.570855
2745.012003	251823.438437	39.575872
2747.698939	252287.698445	39.580890
2750.481610	252768.580365	39.585908
2753.196333	253250.233388	39.590925
2756.124736	253722.376772	39.595943
2758.684549	254205.447877	39.600960
2761.540136	254684.711908	39.605978
2764.372442	255172.487415	39.610996
2767.001691	255659.937194	39.616013
2770.452730	256149.949882	39.621031
2772.857457	256639.336176	39.626048
2775.805374	257104.276519	39.631066
2778.886378	257594.392252	39.636084
2781.724527	258083.146862	39.641101
2784.581164	258555.818020	39.646119
2787.112056	259058.510870	39.651136
2789.909092	259542.186024	39.656154
2792.623556	260026.380106	39.661172
2795.885300	260514.474913	39.666189
2798.642871	261005.389381	39.671207
2801.562716	261489.139078	39.676224
2804.751424	261966.698082	39.681242
2807.692871	262441.245552	39.686260
2810.871208	262914.611145	39.691277
2813.882618	263377.739194	39.696295
2816.755835	263850.310028	39.701312
2819.741436	264309.755154	39.706330
2822.656607	264781.832743	39.711348
2825.226741	265235.699824	39.716365
2828.118317	265706.583128	39.721383
2830.577047	266183.982979	39.726400
2833.456513	266640.234000	39.731418
2836.553663	267093.883785	39.736436
2838.942063	267533.545508	39.741453
2841.823671	267969.293320	39.746471
2843.866739	268412.992388	39.751488
2846.499241	268859.772469	39.756506
2849.295504	269305.153457	39.761524
2851.857642	269754.937239	39.766541
2855.022491	270202.999581	39.771559
2857.371991	270664.571289	39.776576
2860.089597	271114.095648	39.781594
2862.615543	271589.730918	39.786612
2865.233874	272057.577653	39.791629
2868.054615	272543.016149	39.796647
2870.577263	273021.996659	39.801664
2873.747851	273503.438786	39.806682
2876.533650	273994.842870	39.811700
2879.352985	274491.242042	39.816717
2882.924323	274981.527656	39.821735
2885.693162	275475.033620	39.826752
2888.737857	275967.655616	39.831770
2891.921864	276462.767167	39.836788
2894.615109	276956.809227	39.841805
2897.751446	277445.979467	39.846823
2900.507405	277953.541536	39.851840
2903.658812	278450.931370	39.856858
2906.296775	278964.803292	39.861876
2908.692106	279480.004686	39.866893
2911.718207	279995.815492	39.871911
2914.538188	280517.140117	39.876928
2917.495591	281045.626392	39.881946
2920.636109	281561.027648	39.886964
2923.149136	282086.706022	39.891981
2926.358760	282612.424547	39.896999
2929.355186	283148.253775	39.902016
2932.036041	283676.840087	39.907034
2935.197344	284209.283663	39.912052
2938.207924	284754.392504	39.917069
2941.284219	285280.949858	39.922087
2944.294225	285830.874963	39.927104
2947.314916	286367.335824	39.932122
2950.419697	286910.965406	39.937140
2953.369750	287441.410647	39.942157
2956.669583	287980.354340	39.947175
2959.715191	288528.982082	39.952192
2962.584883	289060.797898	39.957210
2965.691999	289600.265993	39.962228
2968.243415	290149.312336	39.967245
2971.800301	290680.525310	39.972263
2974.671255	291224.942191	39.977280
2977.920036	291753.070942	39.982298
2981.266540	292301.923903	39.987316
2984.179969	292838.042718	39.992333
2987.003762	293366.960024	39.997351
2990.188437	293911.786651	40.002368
2993.726398	294435.683210	40.007386
2996.400150	294962.984845	40.012404
2999.216412	295499.526578	40.017421
3002.374877	296036.441749	40.022439
3005.676224	296567.134917	40.027456
3008.584186	297104.536150	40.032474
3011.633746	297629.597088	40.037492
3014.181369	298173.619824	40.042509
3017.484589	298702.718766	40.047527
3020.145883	299241.737499	40.052544
3023.167006	299773.713554	40.057562
3026.133229	300305.362990	40.062580
3028.674024	300859.972176	40.067597
3032.107862	301393.061434	40.072615
3034.683531	301924.958891	40.077632
3037.868270	302434.822917	40.082650
3040.962395	302944.620000	40.087668
3043.594880	303461.211124	40.092685
3046.555882	303970.968219	40.097703
3049.467062	304482.378101	40.102720
3052.248272	305003.830081	40.107738
3055.162231	305521.143856	40.112756
3057.788511	306055.758344	40.117773
3060.940242	306593.356880	40.122791
3063.907005	307132.069965	40.127808
3066.601851	307676.505425	40.132826
3069.615522	308217.940892	40.137844
3072.609925	308775.440684	40.142861
3075.818469	309330.997144	40.147879
3078.797192	309891.405646	40.152896
3081.407251	310474.759442	40.157914
3084.529330	311027.314859	40.162932
3087.531790	311623.005195	40.167949
3090.790571	312195.805368	40.172967
3094.003760	312771.346785	40.177984
3097.453846	313356.793335	40.183002
3100.742517	313931.801098	40.188020
3104.039925	314512.891463	40.193037
3107.266419	315101.345514	40.198055
3110.418777	315692.316031	40.203072
3113.249278	316278.506987	40.208090
3116.274549	316871.182233	40.213108
3119.361419	317473.610564	40.218125
3122.873814	318060.408023	40.223143
3126.193014	318664.687327	40.228160
3129.337313	319271.548596	40.233178
3132.660524	319861.954920	40.238196
3135.380105	320467.469867	40.243213
3138.822125	321064.489831	40.248231
3142.019638	321677.373837	40.253248
3145.308462	322277.953216	40.258266
3148.515014	322884.271559	40.263284
3151.905577	323492.633209	40.268301
3154.986539	324085.479859	40.273319
3158.183775	324697.736187	40.278336
3161.240942	325310.588796	40.283354
3164.662195	325916.220404	40.288372
3167.755766	326525.090929	40.293389
3171.228384	327131.584433	40.298407
3174.654946	327749.543997	40.303424
3177.705767	328344.363014	40.308442
3180.925762	328958.783963	40.313460
3183.812103	329569.213341	40.318477
3187.238389	330182.974181	40.323495
3190.620779	330798.660300	40.328512
3193.983298	331401.223745	40.333530
3197.517469	332001.975228	40.338548
3200.300608	332614.326153	40.343565
3203.429205	333227.298425	40.348583
3206.794378	333838.042337	40.353600
3209.656193	334460.980288	40.358618
3212.980580	335075.337967	40.363636
3216.064874	335688.733580	40.368653
3219.165335	336302.040420	40.373671
3222.493766	336923.418598	40.378688
3225.381478	337545.438216	40.383706
3228.427133	338162.679410	40.388724
3231.658012	338784.015660	40.393741
3235.043814	339418.810708	40.398759
3238.518677	340036.333460	40.403776
3241.255171	340671.105838	40.408794
3244.802216	341292.197078	40.413812
3247.921344	341903.883866	40.418829
3250.688987	342509.654667	40.423847
3253.935577	343088.178457	40.428864
3257.235538	343689.534444	40.433882
3260.601053	344277.200476	40.438900
3263.784804	344876.601053	40.443917
3266.855487	345471.114313	40.448935
3270.305710	346071.314630	40.453952
3273.242496	346664.458409	40.458970
3276.692774	347265.651812	40.463988
3279.864700	347878.821232	40.469005
3282.847929	348484.528333	40.474023
3285.894802	349104.693201	40.479040
3288.874821	349740.476304	40.484058
3292.123524	350366.493997	40.489076
3295.302874	351007.926521	40.494093
3298.246856	351643.957068	40.499111
3302.085266	352292.817326	40.504128
3304.826068	352942.595899	40.509146
3308.331946	353599.746789	40.514164
3311.746311	354256.670168	40.519181
3314.970122	354916.753240	40.524199
3318.329576	355578.575983	40.529216
3321.751610	356257.030712	40.534234
3325.158318	356915.851685	40.539252
3328.919450	357584.768880	40.544269
3331.982026	358260.219042	40.549287
3335.415917	358922.415099	40.554304
3339.161720	359606.753450	40.559322
3342.492930	360279.861113	40.564340
3345.424159	360963.763260	40.569357
3349.130186	361648.948696	40.574375
3352.809282	362322.944995	40.579392
3356.189350	363013.573874	40.584410
3359.690911	363696.057362	40.589428
3363.590157	364390.045513	40.594445
3366.715714	365059.782293	40.599463
3370.765306	365734.175106	40.604480
3373.965845	366408.937792	40.609498
3377.554961	367078.682564	40.614516
3381.328352	367745.164696	40.619533
3385.103362	368425.948597	40.624551
3388.530387	369085.560626	40.629568
3391.893716	369759.661466	40.634586
3395.702372	370420.525957	40.639604
3398.991121	371082.317296	40.644621
3402.470760	371742.416300	40.649639
3406.020950	372403.274113	40.654656
3409.361146	373070.356294	40.659674
3412.935253	373727.986281	40.664692
3416.330133	374398.118732	40.669709
3419.979256	375059.023998	40.674727
3422.894184	375722.332854	40.679744
3426.310502	376382.127411	40.684762
3430.037193	377045.682781	40.689780
3433.384742	377720.654919	40.694797
3436.731178	378381.449798	40.699815
3440.366136	379047.122900	40.704832
3443.297372	379721.070471	40.709850
3447.124951	380385.286704	40.714868
3450.455693	381054.477272	40.719885
3453.921446	381720.767579	40.724903
3457.807870	382386.874047	40.729920
3460.824215	383062.495129	40.734938
3464.465046	383736.481750	40.739956
3467.866058	384397.951737	40.744973
3471.173180	385066.408953	40.749991
3474.662590	385731.376127	40.755008
3477.988929	386385.806365	40.760013
3481.259496	387002.460664	40.765018
3484.479812	387588.922115	40.770023
3487.453611	388127.833363	40.775028
3490.061229	388607.335270	40.780032
3492.669902	389049.916751	40.785037
3495.183803	389450.999897	40.790042
3497.529951	389794.326215	40.795047
3499.934393	390099.612300	40.800052
3502.206092	390359.959307	40.805056
3503.341636	390593.674569	40.810061
3505.075946	390783.735380	40.815066
3506.863286	390927.943117	40.820071
3508.239270	391046.271770	40.825076
3509.378337	391123.870473	40.830080
3510.520655	391194.107163	40.835085
3511.824154	391218.475763	40.840090
3512.720071	391230.317489	40.845095
3513.359780	391218.186169	40.850100
3514.251303	391174.286076	40.855104
3514.559506	391128.293675	40.860109
3514.949735	391049.949471	40.865114
3515.674031	390964.597845	40.870119
3516.323799	390873.926882	40.875124
3516.748380	390751.306659	40.880128
3516.752154	390635.605054	40.885133
3516.867500	390483.408194	40.890138
3517.067731	390336.756401	40.895143
3517.181227	390193.493399	40.900148
3517.805853	390038.853770	40.905152
3517.116450	389880.838368	40.910157
3516.990201	389691.129756	40.915162
3517.084153	389511.945750	40.920167
3517.134952	389337.082712	40.925172
3516.784804	389159.945345	40.930176
3516.805547	388982.393597	40.935181
3516.940518	388797.054653	40.940186
3516.834449	388628.912981	40.945191
3516.585307	388444.265843	40.950196
3516.828044	388254.463462	40.955200
3516.800215	388074.628006	40.960205
3516.328912	387881.633617	40.965210
3516.188756	387697.065548	40.970215
3515.726158	387514.577291	40.975220
3515.986605	387323.368790	40.980224
3515.771117	387143.809736	40.985229
3515.319185	386949.586548	40.990234
3515.166249	386773.137839	40.995239
3515.019448	386609.711161	41.000244
3514.801585	386428.801799	41.005248
3514.670319	386255.240389	41.010253
3514.480426	386080.315912	41.015258
3514.309239	385901.121955	41.020263
3513.931841	385728.788523	41.025268
3514.094688	385559.213464	41.030272
3512.928575	385391.773682	41.035277
3513.117182	385229.987011	41.040282
3513.125680	385075.184166	41.045287
3513.104417	384919.724872	41.050292
3512.811989	384749.275834	41.055296
3512.481919	384607.014809	41.060301
3512.496720	384450.074404	41.065306
3512.247665	384292.310814	41.070311
3511.909789	384148.220325	41.075316
3512.051111	384002.505609	41.080320
3512.021661	383858.187760	41.085325
3511.971498	383709.073381	41.090330
3511.423336	383564.301383	41.095335
3511.022570	383416.915698	41.100340
3510.803447	383279.530608	41.105344
3510.918780	383145.672983	41.110349
3510.526602	383011.639719	41.115354
3510.466030	382880.728163	41.120359
3510.257172	382753.343139	41.125364
3510.246069	382611.580064	41.130368
3509.746696	382501.810481	41.135373
3509.809894	382376.285698	41.140378
3509.919854	382252.301982	41.145383
3509.421440	382146.720534	41.150388
3509.663694	382019.794954	41.155392
3509.133050	381901.927366	41.160397
3509.478450	381788.493681	41.165402
3509.383365	381680.384444	41.170407
3509.312916	381558.761672	41.175412
3509.139760	381448.936877	41.180416
3508.670468	381338.319714	41.185421
3508.766556	381220.275333	41.190426
3508.338138	381115.999284	41.195431
3508.085108	381010.679770	41.200436
3508.462607	380903.687289	41.205440
3508.227147	380810.324794	41.210445
3507.926413	380696.631398	41.215450
3507.921206	380600.642121	41.220455
3507.516880	380501.387938	41.225460
3507.669435	380414.312243	41.230464
3507.524608	380325.454130	41.235469
3507.316676	380234.599362	41.240474
3507.432962	380140.697251	41.245479
3507.297879	380058.515528	41.250484
3506.922493	379974.644091	41.255488
3506.958926	379879.102807	41.260493
3506.948437	379791.060018	41.265498
3506.957715	379715.813005	41.270503
3506.746141	379629.629418	41.275508
3506.777511	379539.852404	41.280512
3506.525896	379457.001267	41.285517
3506.394470	379379.718166	41.290522
3506.393934	379304.039784	41.295527
3506.101850	379233.231716	41.300532
3506.161479	379154.089743	41.305536
3505.898086	379090.438403	41.310541
3505.742818	379008.510511	41.315546
3506.172225	378934.618062	41.320551
3506.031055	378870.718613	41.325556
3505.958140	378800.256221	41.330560
3506.071632	378729.383694	41.335565
3505.859309	378659.526731	41.340570
3505.815295	378579.230950	41.345575
3505.558563	378508.364652	41.350580
3505.581688	378431.588060	41.355584
3505.126997	378372.028182	41.360589
3505.331474	378312.797335	41.365594
3505.456958	378249.337430	41.370599
3505.160322	378191.123964	41.375604
3505.912508	378127.515453	41.380608
3505.596548	378067.831720	41.385613
3505.282175	377991.893677	41.390618
3505.667051	377941.649787	41.395623
3505.549143	377868.728439	41.400628
3505.632935	377804.054913	41.405632
3505.502979	377743.020867	41.410637
3505.157153	377676.788478	41.415642
3505.304933	377608.853696	41.420647
3505.011368	377551.476463	41.425652
3505.204647	377491.966170	41.430656
3505.172890	377430.763748	41.435661
3505.151710	377371.083381	41.440666
3505.356226	377303.926316	41.445671
3504.771018	377249.870087	41.450676
3505.029504	377184.659930	41.455680
3505.021865	377139.758304	41.460685
3505.032106	377081.774042	41.465690
3504.768303	377019.819464	41.470695
3504.772011	376963.563006	41.475700
3504.956335	376901.030465	41.480704
3504.497488	376853.277826	41.485709
3504.855913	376802.731145	41.490714
3504.747378	376741.589894	41.495719
3504.551904	376685.135268	41.500724
3504.688398	376630.178147	41.505728
3504.346163	376575.955760	41.510733
3504.408161	376531.321661	41.515738
3504.416611	376466.453451	41.520743
3504.201548	376424.757686	41.525748
3504.498411	376370.003663	41.530752
3504.069889	376314.803644	41.535757
3503.977810	376273.952052	41.540762
3504.033635	376225.965820	41.545767
3504.053696	376179.737563	41.550772
3504.290218	376141.882455	41.555776
3504.197194	376094.198535	41.560781
3504.256728	376046.643183	41.565786
3504.015788	375995.654889	41.570791
3503.894263	375960.496704	41.575796
3504.404936	375909.823066	41.580800
3504.084588	375866.771291	41.585805
3504.215972	375815.927910	41.590810
3504.058106	375769.726641	41.595815
3503.702177	375721.092419	41.600820
3504.071945	375676.637606	41.605824
3503.879277	375639.864542	41.610829
3504.034727	375592.344265	41.615834
3503.800134	375543.487650	41.620839
3503.520150	375502.562538	41.625844
3503.745947	375459.120338	41.630848
3503.937344	375423.430178	41.635853
3503.974121	375380.398254	41.640858
3503.846084	375338.204686	41.645863
3503.999943	375300.843854	41.650868
3503.928162	375253.409143	41.655872
3503.866370	375226.114508	41.660877
3503.739387	375166.115539	41.665882
3503.994500	375118.985317	41.670887
3503.986144	375084.240176	41.675892
3504.002513	375022.720013	41.680896
3503.989593	374983.149535	41.685901
3503.651368	374942.715235	41.690906
3503.555319	374892.362711	41.695911
3503.449354	374847.015385	41.700916
3503.630496	374799.565925	41.705920
3503.905175	374784.816775	41.710925
3503.529302	374743.803842	41.715930
3503.725385	374696.123278	41.720935
3503.575443	374659.367639	41.725940
3503.597631	374620.222970	41.730944
3503.637619	374588.212869	41.735949
3503.330213	374541.956583	41.740954
3503.669326	374492.526206	41.745959
3503.698475	374465.623059	41.750964
3503.917392	374418.497260	41.755968
3503.191689	374386.428272	41.760973
3503.600454	374343.336826	41.765978
3503.558185	374297.927876	41.770983
3503.279258	374267.973645	41.775988
3503.616669	374224.562912	41.780992
3503.622049	374189.382690	41.785997
3503.513642	374148.047838	41.791002
3503.502595	374113.454284	41.796007
3503.074719	374076.156901	41.801012
3503.478162	374035.859849	41.806016
3503.363244	374008.419861	41.811021
3503.608047	373959.231802	41.816026
3503.456239	373928.825610	41.821031
3503.537058	373890.153384	41.826036
3504.246725	373846.150712	41.831040
3503.927520	373807.794626	41.836045
3503.542545	373759.694838	41.841050
3503.655026	373719.620405	41.846055
3503.651638	373677.557280	41.851060
3503.720277	373637.083136	41.856064
3503.504875	373603.917786	41.861069
3503.293975	373570.472286	41.866074
3503.745702	373528.668323	41.871079
3503.624366	373481.797071	41.876084
3503.722168	373448.404988	41.881088
3503.240289	373402.250132	41.886093
3503.525653	373361.767259	41.891098
3503.561623	373323.837848	41.896103
3503.176168	373287.167820	41.901108
3503.319180	373245.335264	41.906112
3503.147295	373214.093165	41.911117
3503.172910	373180.305571	41.916122
3502.997503	373139.538455	41.921127
3502.850078	373116.065240	41.926132
3503.126563	373075.024498	41.931136
3503.341293	373044.992114	41.936141
3503.336673	373013.241132	41.941146
3503.386336	372981.938893	41.946151
3502.559960	372951.509584	41.951156
3502.860891	372910.413991	41.956160
3503.163101	372884.203449	41.961165
3502.739682	372860.671358	41.966170
3502.789569	372822.815298	41.971175
3502.411720	372788.378763	41.976180
3502.607719	372760.050894	41.981184
3503.153813	372735.326359	41.986189
3502.828743	372708.705230	41.991194
3503.030399	372667.319904	41.996199
3502.764938	372652.298041	42.001204
3502.886327	372618.825079	42.006208
3503.100430	372578.707774	42.011213
3503.184548	372558.728907	42.016218
3503.198613	372523.621412	42.021223
3502.913092	372490.287821	42.026228
3503.030489	372453.462229	42.031232
3503.046878	372426.787693	42.036237
3502.898742	372389.038061	42.041242
3503.247030	372366.604757	42.046247
3502.994410	372341.597730	42.051252
3503.132075	372299.993195	42.056256
3502.656796	372275.528798	42.061261
3502.653260	372242.481256	42.066266
3503.082610	372207.054715	42.071271
3502.863404	372179.756147	42.076276
3503.469447	372154.615332	42.081280
3503.259344	372121.320366	42.086285
3502.881698	372083.860055	42.091290
3503.282113	372053.975519	42.096295
3502.971092	372014.955207	42.101300
3503.121069	371975.761493	42.106304
3502.788807	371944.339698	42.111309
3502.646603	371920.890058	42.116314
3502.721911	371893.240549	42.121319
3502.886520	371866.644020	42.126324
3502.776676	371832.545629	42.131328
3502.771634	371798.151460	42.136333
3502.692774	371776.215994	42.141338
3502.801775	371753.565408	42.146343
3502.235681	371722.357566	42.151348
3502.746506	371693.166735	42.156352
3502.968293	371663.843033	42.161357
3502.830912	371640.341601	42.166362
3502.292940	371610.450198	42.171367
3502.203347	371583.816748	42.176372
3502.714171	371562.475225	42.181376
3502.884238	371542.406046	42.186381
3502.908286	371510.877509	42.191386
3502.652730	371483.025051	42.196391
3502.667235	371461.862296	42.201396
3502.732471	371417.727429	42.206400
3503.149868	371390.506843	42.211405
3503.004680	371365.177384	42.216410
3502.596933	371322.513129	42.221415
3502.299889	371306.123691	42.226420
3502.707916	371272.350475	42.231424
3502.579197	371260.304136	42.236429
3502.857355	371222.893033	42.241434
3502.997932	371199.881441	42.246439
3502.658875	371174.200931	42.251444
3502.924344	371143.853761	42.256448
3503.175519	371109.825323	42.261453
3503.171725	371081.653853	42.266458
3503.089822	371050.979590	42.271463
3502.564636	371012.956523	42.276468
3502.578028	370989.659711	42.281472
3502.710442	370970.764531	42.286477
3502.504220	370933.199787	42.291482
3502.683775	370902.002012	42.296487
3502.269567	370883.598288	42.301492
3502.679842	370858.410564	42.306496
3502.625297	370833.193534	42.311501
3502.755891	370809.217845	42.316506
3502.825357	370772.321281	42.321511
3503.010428	370744.043871	42.326516
3503.017445	370709.951328	42.331520
3502.972871	370680.490220	42.336525
3503.034021	370655.864713	42.341530
3502.899457	370615.392384	42.346535
3502.645002	370592.314747	42.351540
3502.863407	370558.417758	42.356544
3503.018016	370527.401274	42.361549
3502.666775	370506.904401	42.366554
3502.913496	370469.573397	42.371559
3502.757766	370441.780579	42.376564
3502.666858	370416.035355	42.381568
3502.764080	370397.754957	42.386573
3502.492580	370364.289623	42.391578
3502.488945	370331.443067	42.396583
3502.582784	370311.207041	42.401588
3502.820135	370285.639251	42.406592
3502.745861	370259.764275	42.411597
3502.589221	370237.280819	42.416602
3502.722230	370192.777822	42.421607
3502.773248	370173.589925	42.426612
3502.388874	370144.358960	42.431616
3502.305972	370121.787725	42.436621
3502.316007	370086.017287	42.441626
3502.458443	370070.625708	42.446631
3502.385811	370052.803388	42.451636
3502.452174	370021.241188	42.456640
3502.531309	370005.122703	42.461645
3502.660044	369973.525339	42.466650
3502.861611	369940.163715	42.471655
3503.138337	369922.185331	42.476660
3503.029761	369887.296843	42.481664
3502.783910	369863.582162	42.486669
3502.868102	369819.035362	42.491674
3502.625304	369787.470201	42.496679
3502.650035	369769.403912	42.501684
3502.753783	369731.967158	42.506688
3502.463976	369710.698011	42.511693
3502.554133	369671.662813	42.516698
3503.042873	369656.115501	42.521703
3502.578543	369629.817960	42.526708
3502.720112	369596.973357	42.531712
3502.645576	369567.261701	42.536717
3502.726143	369542.174918	42.541722
3502.795415	369504.794037	42.546727
3502.587093	369483.639063	42.551732
3502.723394	369456.968443	42.556736
3502.677649	369431.596362	42.561741
3502.736318	369408.443623	42.566746
3502.934007	369371.499868	42.571751
3502.818013	369343.598165	42.576756
3502.559677	369323.924330	42.581760
3502.279051	369293.888791	42.586765
3502.299747	369266.448432	42.591770
3502.739120	369240.619617	42.596775
3502.637571	369229.177895	42.601780
3502.742467	369192.934278	42.606784
3502.676970	369167.819082	42.611789
3502.418533	369145.731672	42.616794
3502.690081	369110.198759	42.621799
3502.414116	369086.538922	42.626804
3502.712748	369050.036330	42.631808
3502.718926	369028.085485	42.636813
3502.708626	369004.206403	42.641818
3502.595178	368966.853247	42.646823
3502.518843	368944.229240	42.651828
3502.356227	368913.641425	42.656832
3502.512609	368891.286024	42.661837
3502.378504	368865.596919	42.666842
3502.371536	368838.541530	42.671847
3502.063944	368825.810636	42.676852
3502.442133	368804.614697	42.681856
3502.129148	368774.761479	42.686861
3502.100079	368760.513709	42.691866
3503.071688	368735.922688	42.696871
3502.690990	368715.911798	42.701876
3502.680903	368680.269742	42.706880
3502.568105	368660.801448	42.711885
3502.418737	368629.880997	42.716890
3502.583927	368601.248863	42.721895
3502.290781	368581.427497	42.726900
3502.518559	368554.945039	42.731904
3502.359338	368528.903861	42.736909
3502.408063	368499.476772	42.741914
3502.432425	368482.146480	42.746919
3502.166444	368464.683520	42.751924
3502.066883	368434.441056	42.756928
3502.497194	368415.396191	42.761933
3502.509630	368393.139015	42.766938
3502.681437	368364.353180	42.771943
3502.093396	368347.397566	42.776948
3502.383983	368318.262927	42.781952
3502.534226	368299.464812	42.786957
3502.398364	368273.800851	42.791962
3502.353351	368243.473479	42.796967
3502.616646	368225.318272	42.801972
3502.387737	368195.629204	42.806977
3502.618877	368169.399924	42.811981
3502.201477	368145.176977	42.816986
3502.356925	368115.097739	42.821991
3502.431746	368100.630226	42.826996
3502.574106	368077.539599	42.832001
3502.712566	368057.015557	42.837005
3502.576861	368026.676661	42.842010
3502.392505	367993.347400	42.847015
3502.323524	367982.179574	42.852020
3502.299973	367955.151333	42.857025
3502.172016	367927.631193	42.862029
3502.164378	367918.486278	42.867034
3502.685341	367885.580662	42.872039
3502.447739	367867.172895	42.877044
3502.301802	367834.625059	42.882049
3502.578551	367821.828192	42.887053
3502.136782	367794.890285	42.892058
3502.477676	367766.306191	42.897063
3502.296024	367748.499389	42.902068
3502.561725	367718.555015	42.907073
3502.552370	367691.041597	42.912077
3502.386106	367661.647101	42.917082
3502.375366	367636.903129	42.922087
3501.873325	367619.755855	42.927092
3502.345004	367596.461156	42.932097
3502.425334	367572.719211	42.937101
3502.072443	367546.808900	42.942106
3502.129203	367521.368353	42.947111
3502.027769	367512.314124	42.952116
3502.323191	367485.718525	42.957121
3502.453924	367466.694242	42.962125
3502.487271	367450.581436	42.967130
3502.803332	367429.800650	42.972135
3502.655285	367404.086993	42.977140
3502.584338	367365.454802	42.982145
3502.474299	367340.471962	42.987149
3502.100245	367333.340184	42.992154
3502.296787	367295.199812	42.997159
3502.175031	367284.929157	43.002164
3502.408913	367258.444551	43.007169
3502.073652	367233.903171	43.012173
3502.145175	367213.820856	43.017178
3502.273995	367194.263150	43.022183
3501.875645	367172.932777	43.027188
3502.316726	367150.658747	43.032193
3502.300084	367138.593212	43.037197
3502.127444	367108.868854	43.042202
3502.024293	367086.679464	43.047207
3502.086586	367067.614754	43.052212
3502.139858	367047.408128	43.057217
3502.599683	367023.403420	43.062221
3502.123544	367002.415314	43.067226
3502.396145	366980.472252	43.072231
3502.176216	366964.220739	43.077236
3502.337060	366946.893687	43.082241
3502.427595	366916.696260	43.087245
3502.231020	366899.958345	43.092250
3502.522437	366867.417575	43.097255
3502.054369	366846.860017	43.102260
3502.229108	366827.904685	43.107265
3501.978739	366807.999212	43.112269
3502.110040	366786.967237	43.117274
3502.171187	366764.091449	43.122279
3502.347390	366753.545574	43.127284
3502.093651	366734.275751	43.132289
3502.382264	366708.214044	43.137293
3502.066198	366690.630759	43.142298
3502.067085	366667.052871	43.147303
3502.426267	366643.749503	43.152308
3501.952701	366618.492312	43.157313
3502.313411	366593.003647	43.162317
3501.990465	366582.205090	43.167322
3502.453961	366550.856732	43.172327
3502.244680	366537.728412	43.177332
3502.350848	366523.356856	43.182337
3502.347557	366497.670677	43.187341
3502.226162	366479.701268	43.192346
3502.492863	366439.033524	43.197351
3501.959518	366425.193360	43.202356
3502.116379	366395.772695	43.207361
3502.170877	366385.321847	43.212365
3501.936809	366362.466273	43.217370
3502.510771	366349.139762	43.222375
3502.185816	366323.173186	43.227380
3502.180394	366300.002500	43.232385
3502.113134	366278.416682	43.237389
3502.021668	366261.636633	43.242394
3502.087084	366232.839812	43.247399
3502.430257	366211.901487	43.252404
3502.476301	366200.918330	43.257409
3502.531033	366177.789000	43.262413
3502.100231	366163.805716	43.267418
3502.319226	366121.747533	43.272423
3502.031594	366111.832571	43.277428
3502.159173	366090.394147	43.282433
3501.969856	366075.712643	43.287437
3502.066634	366055.701815	43.292442
3502.305186	366034.703419	43.297447
3502.187610	366016.072528	43.302452
3502.075143	365981.992927	43.307457
3502.467633	365958.353524	43.312461
3501.887349	365937.228401	43.317466
3502.314487	365920.164190	43.322471
3502.168257	365903.900611	43.327476
3501.967500	365886.807049	43.332481
3502.060586	365864.586183	43.337485
3502.031081	365855.571056	43.342490
3502.072162	365820.501873	43.347495
3502.306694	365809.285973	43.352500
3502.194006	365782.625276	43.357505
3502.575647	365767.600689	43.362509
3502.530089	365746.214361	43.367514
3502.011375	365715.322841	43.372519
3502.147520	365695.940839	43.377524
3501.875386	365673.344724	43.382529
3502.163110	365646.443737	43.387533
3501.886588	365636.984228	43.392538
3502.027741	365613.688553	43.397543
3502.131606	365600.434853	43.402548
3501.829323	365581.451305	43.407553
3501.982118	365568.012119	43.412557
3502.099950	365552.113781	43.417562
3502.226383	365526.863902	43.422567
3502.190805	365502.960436	43.427572
3502.021562	365477.781934	43.432577
3502.046920	365456.714664	43.437581
3501.822987	365442.368533	43.442586
3502.451922	365415.896992	43.447591
3501.949483	365411.757478	43.452596
3502.153269	365378.313978	43.457601
3502.106291	365368.488354	43.462605
3501.862270	365348.098132	43.467610
3501.757723	365328.702523	43.472615
3502.119461	365309.005667	43.477620
3501.692362	365285.874382	43.482625
3501.731412	365274.053488	43.487629
3502.027046	365260.109174	43.492634
3502.116741	365242.055334	43.497639
3502.098745	365228.337669	43.502644
3501.922300	365201.864220	43.507649
3502.366792	365182.357669	43.512653
3502.215604	365167.288645	43.517658
3502.348067	365136.955799	43.522663
3501.782526	365124.720757	43.527668
3501.745899	365095.938690	43.532673
3502.226977	365088.724102	43.537677
3502.003747	365073.844101	43.542682
3502.117783	365052.457837	43.547687
3501.933412	365031.372079	43.552692
3501.962500	365015.055313	43.557697
3501.765093	364995.623116	43.562701
3501.725606	364980.409571	43.567706
3502.252517	364955.655868	43.572711
3502.217758	364952.790168	43.577716
3502.150602	364942.332325	43.582721
3502.327655	364913.516827	43.587725
3502.358352	364893.108945	43.592730
3501.843166	364867.373939	43.597735
3502.037811	364859.187519	43.602740
3502.227822	364836.722109	43.607745
3502.277485	364804.546964	43.612749
3501.795316	364795.627358	43.617754
3502.671028	364776.180477	43.622759
3502.477419	364751.767403	43.627764
3502.304916	364726.131400	43.632769
3502.370240	364694.029923	43.637773
3502.369285	364676.752106	43.642778
3502.430545	364639.696471	43.647783
3502.367055	364631.499338	43.652788
3502.698971	364608.655946	43.657793
3502.309017	364574.897378	43.662797
3501.932619	364554.146066	43.667802
3502.541353	364527.956366	43.672807
3502.324411	364510.966152	43.677812
3502.187705	364485.248140	43.682817
3502.642861	364469.703267	43.687821
3502.252632	364442.601762	43.692826
3502.191369	364411.637674	43.697831
3502.237623	364382.791190	43.702836
3502.173453	364366.361529	43.707841
3502.223426	364353.623834	43.712845
3501.567327	364334.135530	43.717850
3501.710643	364312.617124	43.722855
3501.955191	364306.658794	43.727860
3501.772698	364275.713427	43.732865
3501.848693	364257.152927	43.737869
3501.984428	364251.668885	43.742874
3501.908724	364223.425636	43.747879
3501.753365	364221.061408	43.752884
3501.862485	364196.422897	43.757889
3502.082867	364187.342960	43.762893
3502.034557	364172.333643	43.767898
3501.986845	364153.512825	43.772903
3501.882093	364144.991656	43.777908
3501.977921	364116.416700	43.782913
3501.637781	364098.149539	43.787917
3501.691229	364088.053764	43.792922
3502.000967	364070.320692	43.797927
3501.846699	364046.586962	43.802932
3501.802059	364039.936706	43.807937
3502.027951	364018.964243	43.812941
3501.707202	363997.670278	43.817946
3502.119978	363976.185924	43.822951
3501.571752	363958.103514	43.827956
3502.057610	363944.815032	43.832961
3502.400177	363925.958746	43.837965
3502.364742	363910.489921	43.842970
3502.248293	363874.782270	43.847975
3501.838243	363868.138018	43.852980
3502.089348	363843.832853	43.857985
3502.058901	363825.364873	43.862989
3501.935286	363801.372079	43.867994
3502.406987	363783.257896	43.872999
3501.966862	363768.741309	43.878004
3501.837073	363751.864141	43.883009
3501.902277	363726.977975	43.888013
3501.682025	363712.249277	43.893018
3502.119579	363698.764923	43.898023
3502.050621	363684.063487	43.903028
3501.905395	363673.642750	43.908033
3502.249270	363657.403293	43.913037
3501.535046	363640.794875	43.918042
3501.941768	363613.975146	43.923047
3501.824211	363596.181233	43.928052
3501.890340	363579.908725	43.933057
3501.789122	363561.705691	43.938061
3501.508466	363550.924837	43.943066
3502.014244	363532.678149	43.948071
3502.057667	363520.830458	43.953076
3501.936201	363509.110061	43.958081
3502.448907	363485.729468	43.963085
3501.971780	363463.239775	43.968090
3501.806345	363440.040903	43.973095
3501.879002	363429.027155	43.978100
3501.881016	363404.938259	43.983105
3502.088486	363391.159241	43.988109
3501.767726	363369.890233	43.993114
3502.052304	363358.868891	43.998119
3502.188805	363336.156563	44.003124
3502.109064	363319.474640	44.008129
3502.115420	363288.448029	44.013133
3502.064596	363268.000885	44.018138
3502.162535	363249.156826	44.023143
3502.049237	363234.182554	44.028148
3501.912527	363212.833972	44.033153
3502.073037	363190.066976	44.038157
3501.802228	363184.010745	44.043162
3501.963234	363160.252652	44.048167
3502.009109	363146.117512	44.053172
3501.623919	363123.765715	44.058177
3502.081737	363104.636869	44.063181
3501.542520	363095.573159	44.068186
3501.879719	363070.008859	44.073191
3501.972222	363070.756840	44.078196
3502.152889	363046.919365	44.083201
3502.068301	363027.722414	44.088205
3501.585577	363014.685881	44.093210
3501.701119	362994.644635	44.098215
3501.916100	362979.797023	44.103220
3501.888122	362957.262461	44.108225
3502.034040	362948.854401	44.113229
3501.627425	362922.262253	44.118234
3501.802083	362905.210174	44.123239
3501.777629	362900.919688	44.128244
3501.797336	362878.072721	44.133249
3502.121498	362859.396494	44.138253
3501.782616	362843.847277	44.143258
3501.841074	362829.837082	44.148263
3502.003154	362813.523811	44.153268
3501.981591	362788.624948	44.158273
3501.674999	362782.625024	44.163277
3501.591661	362759.184148	44.168282
3501.774264	362748.915354	44.173287
3501.614813	362740.783450	44.178292
3501.805027	362720.527115	44.183297
3501.698337	362711.523033	44.188301
3501.675958	362703.954231	44.193306
3501.680542	362683.447241	44.198311
3501.725829	362669.616894	44.203316
3501.857495	362660.931453	44.208321
3501.964090	362633.496866	44.213325
3501.504952	362620.380257	44.218330
3501.903352	362604.970291	44.223335
3501.803489	362585.800841	44.228340
3501.689736	362583.074257	44.233345
3501.905450	362558.036634	44.238349
3501.687370	362549.430997	44.243354
3501.796357	362539.885087	44.248359
3501.866967	362516.394653	44.253364
3501.623506	362502.736214	44.258369
3501.843205	362476.706884	44.263373
3501.778828	362467.670733	44.268378
3501.642240	362455.672753	44.273383
3501.415335	362433.321215	44.278388
3501.558522	362422.524815	44.283393
3501.582244	362418.684157	44.288397
3501.510821	362414.146802	44.293402
3501.777997	362387.347680	44.298407
3501.880945	362383.774209	44.303412
3502.021691	362366.523812	44.308417
3501.792270	362349.203953	44.313421
3501.661732	362339.059979	44.318426
3501.795899	362316.652165	44.323431
3501.858251	362309.679940	44.328436
3501.950287	362293.046942	44.333441
3502.059040	362266.526474	44.338445
3502.019116	362259.163577	44.343450
3501.965271	362234.294685	44.348455
3502.135789	362220.292175	44.353460
3501.906063	362203.582143	44.358465
3501.738953	362195.070115	44.363469
3501.254952	362161.043900	44.368474
3501.428970	362147.015400	44.373479
3501.705849	362143.541889	44.378484
3501.906128	362133.676710	44.383489
3501.800221	362110.899524	44.388493
3501.535831	362105.960160	44.393498
3502.027494	362081.057074	44.398503
3502.017516	362070.487671	44.403508
3501.896685	362043.545331	44.408513
3501.882231	362021.871935	44.413517
3501.382368	362016.079809	44.418522
3501.740202	361987.614496	44.423527
3501.782867	361978.154960	44.428532
3501.439256	361971.195006	44.433537
3501.593525	361946.954180	44.438541
3502.027610	361935.172122	44.443546
3501.844062	361919.420371	44.448551
3501.845775	361907.273593	44.453556
3502.044518	361892.631257	44.458561
3502.322321	361872.487773	44.463565
3501.960921	361871.451393	44.468570
3502.041033	361825.469937	44.473575
3502.091437	361817.101833	44.478580
3501.626151	361794.481974	44.483585
3501.666242	361783.193160	44.488589
3501.565070	361771.875500	44.493594
3501.714893	361751.294445	44.498599
3501.827225	361741.163297	44.503604
3501.886971	361739.400681	44.508609
3501.765798	361710.526828	44.513613
3501.482891	361703.379485	44.518618
3501.465530	361688.389505	44.523623
3501.712641	361671.198390	44.528628
3501.341163	361665.030456	44.533633
3501.767271	361653.503643	44.538637
3501.480636	361638.987537	44.543642
3501.609379	361622.195984	44.548647
3501.323557	361625.239087	44.553652
3501.727058	361606.600554	44.558657
3501.807762	361582.980757	44.563661
3501.637429	361581.787577	44.568666
3501.785495	361561.232076	44.573671
3501.825757	361542.624616	44.578676
3501.430125	361543.778947	44.583681
3502.000035	361518.482044	44.588685
3501.780176	361496.865643	44.593690
3501.803201	361483.953029	44.598695
3501.677706	361471.571753	44.603700
3501.429861	361455.346942	44.608705
3501.844024	361448.523063	44.613709
3501.888854	361435.607035	44.618714
3502.196731	361418.101378	44.623719
3502.035891	361395.306783	44.628724
3501.920648	361392.072087	44.633729
3501.895501	361360.387666	44.638733
3501.662081	361343.220316	44.643738
3501.745882	361329.103826	44.648743
3501.510679	361309.395558	44.653748
3501.957105	361298.221213	44.658753
3502.106607	361277.411177	44.663757
3502.109793	361264.933556	44.668762
3501.930505	361246.766666	44.673767
3502.176497	361234.429132	44.678772
3501.719864	361216.305382	44.683777
3501.998856	361192.908540	44.688781
3502.050606	361184.463815	44.693786
3501.738440	361157.347157	44.698791
3501.935770	361139.426538	44.703796
3501.884437	361127.846761	44.708801
3501.874170	361110.009254	44.713805
3501.411162	361108.124652	44.718810
3501.869236	361072.781650	44.723815
3501.911655	361062.940684	44.728820
3501.510107	361052.381031	44.733825
3501.634832	361032.286216	44.738829
3501.708263	361024.956200	44.743834
3501.669576	361002.040650	44.748839
3501.572629	360991.865580	44.753844
3501.668374	360975.663278	44.758849
3501.717671	360974.740841	44.763853
3501.573213	360944.472210	44.768858
3501.942020	360936.791264	44.773863
3501.554977	360923.383154	44.778868
3501.623500	360905.812798	44.783873
3501.924382	360892.704219	44.788877
3501.959871	360881.898613	44.793882
3501.826079	360864.308891	44.798887
3501.681901	360850.049767	44.803892
3501.643734	360828.709557	44.808897
3501.681488	360819.479130	44.813901
3501.767983	360816.543337	44.818906
3501.676487	360795.465524	44.823911
3501.948861	360774.839318	44.828916
3501.504494	360760.093208	44.833921
3501.706472	360743.340594	44.838925
3501.497707	360735.292053	44.843930
3501.602348	360715.250977	44.848935
3501.762855	360705.569405	44.853940
3501.454830	360697.205941	44.858945
3501.846701	360676.535660	44.863949
3501.484336	360668.714302	44.868954
3501.729526	360663.212569	44.873959
3501.697937	360644.412436	44.878964
3501.750601	360622.803822	44.883969
3501.690700	360608.302759	44.888973
3501.376489	360604.463631	44.893978
3501.779547	360576.244068	44.898983
3501.879442	360572.670857	44.903988
3501.755235	360561.203852	44.908993
3501.675251	360538.904273	44.913997
3501.768762	360535.891124	44.919002
3501.525555	360513.007027	44.924007
3501.741788	360494.778135	44.929012
3501.230490	360497.907261	44.934017
3501.648531	360472.861827	44.939021
3501.515572	360460.582946	44.944026
3501.667039	360456.772984	44.949031
3501.928138	360455.207672	44.954036
3501.363228	360422.538934	44.959041
3501.750062	360413.686074	44.964045
3501.606788	360411.573785	44.969050
3501.586282	360381.946027	44.974055
3501.499636	360369.482015	44.979060
3501.103523	360368.984646	44.984065
3501.683162	360356.493183	44.989069
3501.938206	360340.875654	44.994074
3501.898471	360324.414547	44.999079
3501.512344	360306.558815	45.004084
3501.645825	360290.756876	45.009089
3501.481176	360281.684844	45.014093
3501.457575	360270.456198	45.019098
3501.411619	360242.890688	45.024103
3501.710640	360254.432398	45.029108
3501.484942	360242.752351	45.034113
3501.623336	360216.250874	45.039117
3501.604362	360204.487817	45.044122
3501.482600	360200.339150	45.049127
3501.737640	360181.239999	45.054132
3501.770845	360178.490326	45.059137
3501.875302	360151.841598	45.064141
3501.583999	360151.022963	45.069146
3501.634121	360134.496944	45.074151
3501.874659	360121.727787	45.079156
3501.875569	360102.464830	45.084161
3501.556424	360085.818358	45.089165
3501.515782	360078.150085	45.094170
3501.574089	360056.591014	45.099175
3501.736806	360045.104576	45.104180
3501.571736	360030.772078	45.109185
3501.753909	360010.896361	45.114189
3501.899941	359999.641218	45.119194
3501.819618	359984.126518	45.124199
3501.596816	359966.651776	45.129204
3501.471939	359957.395567	45.134209
3501.817694	359946.109325	45.139213
3501.435348	359932.903347	45.144218
3501.427010	359916.437132	45.149223
3501.971079	359916.657491	45.154228
3501.584711	359901.901936	45.159233
3501.787705	359883.115651	45.164237
3501.617402	359868.783891	45.169242
3501.896282	359851.713861	45.174247
3501.479887	359842.070960	45.179252
3501.584750	359831.177943	45.184257
3502.007036	359811.595100	45.189261
3501.672921	359810.935595	45.194266
3501.775776	359790.106381	45.199271
3501.840569	359770.401250	45.204276
3501.578103	359765.105418	45.209281
3502.186255	359727.856925	45.214285
3501.533502	359720.004269	45.219290
3501.597344	359710.921923	45.224295
3501.809651	359700.545815	45.229300
3501.758995	359693.717636	45.234305
3502.042271	359670.471430	45.239309
3501.606572	359654.961036	45.244314
3501.687730	359646.130108	45.249319
3501.737740	359619.362319	45.254324
3501.674414	359609.969360	45.259329
3502.080776	359591.710340	45.264333
3501.989658	359571.622730	45.269338
3501.611557	359561.262210	45.274343
3501.415752	359537.760082	45.279348
3501.156459	359527.863914	45.284353
3501.864635	359526.025679	45.289357
3501.777868	359509.444382	45.294362
3501.642736	359487.559224	45.299367
3502.048985	359483.480773	45.304372
3501.894034	359466.350970	45.309377
3501.696882	359445.542791	45.314381
3501.879319	359435.603268	45.319386
3502.112480	359416.659522	45.324391
3502.041233	359403.049114	45.329396
3501.759855	359379.763487	45.334401
3501.626737	359363.443457	45.339405
3501.726747	359343.071821	45.344410
3501.791789	359327.229204	45.349415
3501.884401	359312.932508	45.354420
3501.714211	359284.419750	45.359425
3501.708226	359277.203323	45.364429
3501.772244	359275.617794	45.369434
3501.564270	359255.522746	45.374439
3502.001642	359245.009807	45.379444
3501.581862	359229.928748	45.384449
3501.691095	359201.575738	45.389453
3502.078778	359198.872470	45.394458
3501.812650	359175.609727	45.399463
3501.907720	359168.606272	45.404468
3502.030244	359149.425440	45.409473
3502.027225	359131.916017	45.414477
3501.832626	359113.851882	45.419482
3501.789692	359090.706824	45.424487
3501.637039	359079.446994	45.429492
3501.942644	359069.971044	45.434497
3501.791057	359045.241800	45.439501
3501.644139	359037.335665	45.444506
3501.678684	359010.976367	45.449511
3501.859668	359005.687636	45.454516
3501.566858	358992.187764	45.459521
3501.522378	358973.007396	45.464525
3501.609883	358963.692422	45.469530
3501.545374	358956.662923	45.474535
3501.696447	358934.453279	45.479540
3501.546568	358921.134444	45.484545
3501.544856	358908.859925	45.489549
3501.570943	358895.056248	45.494554
3501.526059	358882.788436	45.499559
3501.868843	358864.360979	45.504564
3502.056295	358865.323015	45.509569
3501.789313	358840.281182	45.514573
3501.889559	358823.797480	45.519578
3501.655796	358795.980332	45.524583
3501.576914	358789.791689	45.529588
3501.625913	358777.255087	45.534593
3501.924776	358743.763951	45.539597
3501.510084	358749.902476	45.544602
3501.397995	358737.746720	45.549607
3501.534282	358718.944686	45.554612
3501.507992	358711.350076	45.559617
3501.825341	358703.676576	45.564621
3501.540305	358685.092568	45.569626
3501.631431	358671.151599	45.574631
3501.845514	358665.069826	45.579636
3501.406992	358635.149620	45.584641
3501.707199	358626.004756	45.589645
3501.853463	358617.773335	45.594650
3501.577923	358602.872832	45.599655
3501.986601	358597.421529	45.604660
3501.850848	358574.163454	45.609665
3502.024337	358556.829546	45.614669
3501.733717	358553.774321	45.619674
3501.829963	358532.208269	45.624679
3501.744510	358513.872654	45.629684
3501.422119	358501.978257	45.634689
3501.905772	358479.132005	45.639693
3501.622079	358473.559694	45.644698
3501.604895	358454.730552	45.649703
3501.851175	358435.707914	45.654708
3501.619216	358437.421413	45.659713
3501.748472	358417.857863	45.664717
3501.224824	358401.216878	45.669722
3501.319435	358397.745891	45.674727
3501.782663	358381.739165	45.679732
3501.501447	358362.493597	45.684737
3501.487975	358358.912354	45.689741
3501.249429	358345.022538	45.694746
3501.345261	358339.111587	45.699751
3501.800340	358316.727117	45.704756
3501.549393	358305.838097	45.709761
3501.746199	358296.810883	45.714765
3501.817378	358287.879458	45.719770
3501.638174	358267.804699	45.724775
3501.913292	358255.639326	45.729780
3501.588546	358247.582759	45.734785
3501.501332	358225.790897	45.739789
3501.545384	358224.894607	45.744794
3501.716804	358203.850328	45.749799
3501.958853	358188.055820	45.754804
3501.315816	358180.836611	45.759809
3501.972804	358148.813961	45.764813
3501.689801	358131.398363	45.769818
3501.566417	358070.321295	45.774823
3501.250627	357965.866007	45.779828
3501.017953	357820.759382	45.784833
3501.047737	357626.891023	45.789837
3500.059232	357394.066194	45.794842
3499.316731	357114.869343	45.799847
3498.746115	356800.620662	45.804852
3497.434419	356445.920517	45.809857
3496.741108	356046.565649	45.814861
3495.990258	355619.281929	45.819866
3494.841010	355155.123706	45.824871
3493.953353	354650.911177	45.829876
3492.575894	354107.776087	45.834881
3491.399338	353532.598981	45.839885
3489.636056	352917.036325	45.844890
3488.577718	352268.536005	45.849895
3486.749807	351590.452176	45.854900
3484.680354	350887.988287	45.859905
3483.589019	350154.699522	45.864909
3481.575757	349397.489150	45.869914
3479.717690	348602.866865	45.874919
3477.990315	347769.257703	45.879924
3475.604453	346924.671052	45.884929
3473.679462	346048.669151	45.889933
3471.231531	345151.343849	45.894938
3469.445534	344227.653014	45.899943
3467.129697	343273.788289	45.904948
3464.457640	342304.391585	45.909953
3462.245334	341320.606224	45.914957
3459.376381	340310.094311	45.919962
3456.748553	339283.012802	45.924967
3454.269619	338245.071130	45.929972
3451.265783	337179.411435	45.934977
3448.631233	336102.397225	45.939981
3445.550364	335007.059246	45.944986
3443.154403	333893.321893	45.949991
3440.659167	332779.439902	45.954996
3437.430441	331636.644570	45.960001
3434.924478	330479.891688	45.965005
3431.899139	329321.099521	45.970010
3429.113704	328131.559606	45.975015
3426.058667	326944.340883	45.980020
3422.489972	325731.525685	45.985025
3419.389932	324524.732196	45.990029
3416.255667	323305.443435	45.995034
3413.130813	322069.199932	46.000039
3409.938278	320823.746691	46.005044
3406.446392	319580.924353	46.010049
3403.395376	318320.289980	46.015053
3399.814094	317064.790669	46.020058
3396.967845	315808.887241	46.025063
3393.926292	314522.725860	46.030068
3390.568395	313245.330862	46.035073
3387.250824	311944.077209	46.040077
3383.377352	310654.019901	46.045082
3380.362272	309351.172518	46.050087
3376.364960	308038.085880	46.055092
3373.030330	306734.939001	46.060097
3369.568341	305418.239213	46.065101
3366.261747	304099.394498	46.070106
3362.621251	302788.814338	46.075111
3359.377024	301467.526934	46.080116
3355.791951	300134.425081	46.085121
3352.016663	298793.277465	46.090125
3348.497029	297467.304255	46.095130
3344.595017	296128.123764	46.100135
3341.210843	294796.442581	46.105140
3337.791245	293467.791493	46.110145
3334.145154	292116.542021	46.115149
3330.617033	290786.551099	46.120154
3326.783233	289446.855213	46.125159
3323.092120	288105.123479	46.130164
3319.296462	286775.752855	46.135169
3315.626943	285437.349526	46.140173
3312.190364	284093.231986	46.145178
3308.543472	282751.718178	46.150183
3305.241137	281418.196270	46.155188
3301.178732	280077.817857	46.160193
3297.453937	278732.321863	46.165197
3293.732128	277392.352368	46.170202
3290.516171	276060.912797	46.175207
3286.533818	274717.960168	46.180212
3282.744732	273391.098753	46.185217
3279.293074	272035.009856	46.190221
3275.336900	270702.964574	46.195226
3271.617739	269362.205416	46.200231
3268.016108	268032.179842	46.205236
3264.152385	266707.396836	46.210241
3260.129575	265368.259194	46.215245
3256.505793	264040.373774	46.220250
3252.777034	262709.228670	46.225255
3249.594494	261388.397773	46.230260
3245.646327	260061.813762	46.235265
3241.952380	258732.959899	46.240269
3238.164878	257409.377794	46.245274
3234.129285	256081.415070	46.250279
3230.612330	254763.112200	46.255284
3226.868639	253460.417886	46.260289
3223.077531	252145.622666	46.265293
3219.408545	250828.836310	46.270298
3215.451498	249517.992558	46.275303
3211.985823	248209.405358	46.280308
3208.012948	246908.808125	46.285313
3204.386008	245601.781342	46.290317
3200.558200	244308.326496	46.295322
3196.473945	242999.444797	46.300327
3193.196596	241708.563717	46.305332
3189.159632	240420.392115	46.310337
3185.266822	239134.025859	46.315341
3181.810371	237849.216273	46.320346
3177.998346	236574.007898	46.325351
3174.079429	235285.542614	46.330356
3170.253282	234008.469070	46.335361
3166.607056	232726.041229	46.340365
3162.883912	231455.720312	46.345370
3158.919789	230197.456016	46.350375
3155.369142	228937.648450	46.355380
3151.414836	227662.722904	46.360385
3148.067565	226396.030520	46.365389
3144.270452	225147.414518	46.370394
3140.201417	223890.971122	46.375399
3136.411931	222621.368388	46.380404
3132.725431	221388.808272	46.385409
3128.923379	220138.592294	46.390413
3125.088330	218910.159527	46.395418
3121.085793	217667.008876	46.400423
3117.531232	216431.483148	46.405428
3113.921120	215195.816734	46.410433
3109.925150	213964.442102	46.415437
3106.421222	212736.051500	46.420442
3102.686121	211513.279265	46.425447
3099.407872	210291.587222	46.430452
3095.137881	209072.907592	46.435457
3091.642243	207868.604858	46.440461
3087.731164	206639.949370	46.445466
3083.898574	205438.106304	46.450471
3080.211230	204237.444795	46.455476
3076.569216	203031.562991	46.460481
3072.479850	201824.332718	46.465485
3068.815937	200633.878529	46.470490
3065.091397	199449.121608	46.475495
3061.541104	198254.490987	46.480500
3057.320835	197075.763463	46.485505
3054.149343	195891.228968	46.490509
3049.794186	194718.170392	46.495514
3046.291696	193549.522500	46.500519
3042.852197	192362.922321	46.505524
3038.629283	191213.915091	46.510529
3035.009906	190048.985810	46.515533
3031.294208	188887.215552	46.520538
3027.409706	187734.396341	46.525543
3023.763242	186579.769955	46.530548
3019.758011	185428.675287	46.535553
3015.961721	184286.116993	46.540557
3011.971099	183148.796729	46.545562
3008.362150	182017.236151	46.550567
3004.700471	180881.699830	46.555572
3000.383724	179771.793019	46.560577
2996.519218	178654.343827	46.565581
2993.018705	177540.544357	46.570586
2989.271886	176434.194423	46.575591
2985.104101	175336.759800	46.580596
2981.684669	174248.262178	46.585601
2977.974489	173147.412772	46.590605
2973.725210	172063.937541	46.595610
2969.639253	170997.535809	46.600615
2966.288761	169910.934714	46.605620
2962.480322	168841.185765	46.610625
2958.829947	167780.707831	46.615629
2954.728939	166720.774240	46.620634
2949.982109	165681.387301	46.625639
2946.220882	164622.286122	46.630644
2942.292916	163602.062386	46.635649
2938.408348	162569.997681	46.640653
2934.461330	161557.802313	46.645658
2930.441885	160562.829743	46.650663
2927.070812	159546.784096	46.655668
2922.661067	158560.699178	46.660673
2918.732519	157570.533566	46.665677
2914.704724	156598.204970	46.670682
2910.533554	155628.523719	46.675687
2906.843471	154662.729029	46.680692
2902.759743	153714.141649	46.685697
2898.958148	152778.710636	46.690701
2894.911171	151843.918859	46.695706
2890.609109	150931.809102	46.700711
2887.031329	150004.776575	46.705716
2882.744600	149107.584092	46.710721
2878.659916	148197.662855	46.715725
2874.792181	147324.282376	46.720730
2870.224695	146456.369851	46.725735
2866.050253	145584.860671	46.730740
2861.904620	144742.844158	46.735745
2857.756992	143909.354465	46.740749
2853.469807	143093.561192	46.745754
2848.935053	142283.800069	46.750759
2844.886787	141497.260620	46.755764
2840.550502	140721.173689	46.760769
2836.253768	139961.785831	46.765773
2831.723048	139226.492741	46.770778
2827.391096	138426.714481	46.775783
2823.147157	137687.482330	46.780788
2818.737155	136985.118748	46.785793
2814.635219	136294.218719	46.790797
2810.564707	135618.857687	46.795802
2806.413034	134963.492427	46.800807
2802.665577	134304.486372	46.805812
2798.772313	133673.105295	46.810817
2794.881096	133040.397191	46.815821
2790.980584	132410.803560	46.820826
2787.090451	131803.186178	46.825831
2782.860455	131187.349093	46.830836
2779.070757	130592.924364	46.835841
2775.192148	129997.504109	46.840845
2771.813989	129423.892830	46.845850
2767.596288	128848.435680	46.850855
2764.072765	128272.191520	46.855860
2760.292998	127710.788024	46.860865
2756.869565	127154.424419	46.865869
2753.554310	126596.397978	46.870874
2749.616982	126043.894237	46.875879
2745.927210	125482.023804	46.880884
2742.606634	124939.372507	46.885889
2739.141040	124385.457026	46.890893
2735.469893	123844.948154	46.895898
2731.206035	123301.753554	46.900903
2728.237632	122768.386570	46.905908
2724.778597	122234.022120	46.910913
2721.409224	121699.383909	46.915917
2717.752517	121163.691300	46.920922
2714.371340	120635.542704	46.925927
2711.029495	120102.677136	46.930932
2707.293395	119563.763438	46.935937
2703.666210	119025.158290	46.940941
2700.557338	118492.227994	46.945946
2696.922257	117967.067791	46.950951
2693.562936	117432.436529	46.955956
2690.200946	116907.604660	46.960961
2686.285217	116362.304752	46.965965
2682.921890	115826.514510	46.970970
2679.384834	115299.634487	46.975975
2675.861143	114770.471163	46.980980
2672.265614	114240.970634	46.985985
2668.564626	113711.519634	46.990989
2665.100736	113189.935336	46.995994
2661.058688	112666.477779	47.000999
2657.304821	112132.951330	47.006004
2653.804219	111621.821303	47.011009
2650.021942	111100.253362	47.016013
2646.432003	110593.551081	47.021018
2642.695431	110089.396199	47.026023
2639.457586	109569.876610	47.031028
2635.411015	109077.391933	47.036033
2631.891642	108571.623239	47.041037
2627.976078	108082.234276	47.046042
2624.164915	107586.479620	47.051047
2620.288973	107100.632577	47.056052
2616.612233	106621.079488	47.061057
2613.004114	106145.056460	47.066061
2609.439001	105683.855657	47.071066
2605.767954	105212.431852	47.076071
2602.010741	104733.795096	47.081076
2598.203839	104280.901006	47.086081
2594.236524	103826.080465	47.091085
2590.770592	103372.065179	47.096090
2586.713266	102934.392799	47.101095
2582.926794	102488.981295	47.106100
2579.457061	102055.995684	47.111105
2575.311884	101613.969336	47.116109
2571.816261	101183.566800	47.121114
2568.067183	100775.045456	47.126119
2564.960140	100346.677982	47.131124
2561.358002	99923.998258	47.136129
2557.747032	99513.475893	47.141133
2554.234829	99082.595473	47.146138
2550.369703	98673.839179	47.151143
2546.888471	98249.408793	47.156148
2543.402783	97841.392088	47.161153
2540.256962	97425.867643	47.166157
2536.684578	97007.085364	47.171162
2532.862271	96590.622363	47.176167
2529.755428	96185.999381	47.181172
2526.078857	95766.423803	47.186177
2522.625745	95366.897740	47.191181
2519.503751	94948.225383	47.196186
2516.043259	94522.914409	47.201191
2512.509739	94115.805076	47.206196
2508.711536	93695.475856	47.211201
2505.581275	93278.174398	47.216205
2502.555300	92857.164661	47.221210
2498.614406	92446.277953	47.226215
2495.600232	92013.600469	47.231220
2491.771601	91604.041873	47.236225
2488.321894	91167.276536	47.241229
2485.058552	90760.881502	47.246234
2481.647172	90339.229769	47.251239
2478.426634	89906.881445	47.256244
2474.322375	89479.746424	47.261249
2470.849174	89058.935540	47.266253
2467.596181	88623.764891	47.271258
2464.230941	88194.602167	47.276263
2461.085712	87763.162694	47.281268
2457.474030	87333.110719	47.286273
2453.755911	86906.588048	47.291277
2450.409514	86467.118927	47.296282
2446.697817	86038.435521	47.301287
2443.524857	85604.059488	47.306292
2439.840975	85178.560441	47.311297
2436.222910	84739.528192	47.316301
2432.853791	84304.922764	47.321306
2429.576497	83878.896941	47.326311
2425.952362	83440.685817	47.331316
2422.487584	83005.225828	47.336321
2419.073901	82573.943697	47.341325
2415.498314	82128.365084	47.346330
2411.968376	81686.584339	47.351335
2408.790702	81244.590580	47.356340
2405.056776	80804.316171	47.361345
2401.726175	80366.627846	47.366349
2398.312314	79924.742499	47.371354
2394.550178	79482.765961	47.376359
2391.128956	79039.384416	47.381364
2387.887145	78602.802358	47.386369
2384.068409	78163.014862	47.391373
2380.784738	77720.217362	47.396378
2377.112262	77263.491995	47.401383
2373.687189	76823.677445	47.406388
2370.262440	76373.799085	47.411393
2366.958652	75928.798663	47.416397
2363.628691	75472.532668	47.421402
2359.873831	75036.887612	47.426407
2356.386923	74578.311862	47.431412
2352.622548	74137.273172	47.436417
2349.281960	73689.331348	47.441421
2346.008350	73233.259767	47.446426
2342.268221	72794.855354	47.451431
2338.784966	72342.196688	47.456436
2335.292914	71894.257948	47.461441
2332.017134	71436.947913	47.466445
2328.667192	70985.040969	47.471450
2324.895009	70540.781250	47.476455
2321.464969	70070.320643	47.481460
2317.947612	69631.159888	47.486465
2314.469269	69176.511056	47.491469
2310.597051	68718.789241	47.496474
2307.076648	68278.756848	47.501479
2304.153612	67813.393828	47.506484
2300.607831	67359.352515	47.511489
2296.767541	66908.113594	47.516493
2293.607091	66447.706345	47.521498
2289.842655	65993.685294	47.526503
2286.365032	65530.836832	47.531508
2282.969455	65085.597310	47.536513
2279.282905	64623.559653	47.541517
2275.993989	64168.481911	47.546522
2272.587672	63715.633032	47.551527
2269.214100	63243.779046	47.556532
2265.651453	62787.525109	47.561537
2262.283944	62331.096869	47.566541
2258.802255	61864.407459	47.571546
2254.841987	61406.990610	47.576551
2251.799743	60937.762640	47.581556
2248.141795	60471.304744	47.586561
2244.701778	60004.117432	47.591565
2241.292487	59538.425512	47.596570
2237.476560	59079.868403	47.601575
2234.127649	58610.218878	47.606580
2230.463883	58156.953996	47.611585
2227.320931	57691.097467	47.616589
2223.927376	57224.026275	47.621594
2220.160950	56761.178150	47.626599
2216.671680	56287.395402	47.631604
2213.099281	55821.889466	47.636609
2209.887699	55353.963599	47.641613
2206.365121	54879.173541	47.646618
2202.768051	54414.022612	47.651623
2199.174359	53938.355272	47.656628
2196.176603	53474.246192	47.661633
2192.706571	52997.538207	47.666637
2189.095141	52525.251861	47.671642
2185.706879	52055.921877	47.676647
2181.923468	51575.307853	47.681652
2178.501357	51101.174949	47.686657
2175.086165	50624.589470	47.691661
2171.381237	50143.789957	47.696666
2168.227585	49685.749667	47.701671
2164.406324	49194.928017	47.706676
2160.519551	48724.855301	47.711681
2157.006310	48260.544003	47.716685
2153.508329	47778.404611	47.721690
2150.218752	47313.938288	47.726695
2146.920325	46837.844813	47.731700
2143.678488	46358.245363	47.736705
2139.902445	45878.891465	47.741709
2136.723553	45396.195145	47.746714
2132.599473	44925.141173	47.751719
2129.479123	44443.388521	47.756724
2125.920040	43968.017958	47.761729
2121.902668	43490.560154	47.766733
2119.074768	43015.292775	47.771738
2115.430730	42542.236142	47.776743
2112.235838	42061.212646	47.781748
2108.560418	41572.392883	47.786753
2105.070973	41090.599500	47.791757
2101.917670	40609.018030	47.796762
2097.809720	40131.051247	47.801767
2094.594423	39643.395011	47.806772
2090.958974	39161.052008	47.811777
2087.434933	38685.910905	47.816781
2083.940382	38196.080055	47.821786
2080.279749	37724.696500	47.826791
2077.023113	37232.023098	47.831796
2073.632937	36763.699563	47.836801
2069.942030	36277.518475	47.841805
2066.521900	35791.445797	47.846810
2062.816276	35313.770687	47.851815
2059.291342	34820.713017	47.856820
2055.992551	34341.678055	47.861825
2052.753577	33854.797612	47.866829
2049.065584	33368.815962	47.871834
2045.468538	32889.797091	47.876839
2042.056148	32396.081523	47.881844
2038.388980	31910.859363	47.886849
2035.026494	31430.557213	47.891853
2031.356260	30935.300280	47.896858
2027.859567	30454.914856	47.901863
2024.327311	29963.126309	47.906868
2020.943364	29483.417704	47.911873
2017.006027	29006.214481	47.916877
2013.631019	28516.254791	47.921882
2009.853478	28046.057639	47.926887
2006.415641	27554.793736	47.931892
2002.919830	27078.783440	47.936897
1999.410783	26599.085986	47.941901
1995.899220	26119.362267	47.946906
1992.931877	25645.210581	47.951911
1989.221331	25154.370469	47.956916
1985.722125	24667.196800	47.961921
1981.992496	24187.122240	47.966925
1978.997045	23703.872293	47.971930
1974.877852	23234.784386	47.976935
1971.631749	22747.295035	47.981940
1968.447157	22276.215448	47.986945
1964.814151	21791.793525	47.991949
1961.250765	21305.852339	47.996954
1957.616815	20826.629604	48.001959
1954.223566	20341.597889	48.006964
1950.219891	19850.225032	48.011969
1946.598674	19381.011858	48.016973
1943.579648	18897.629841	48.021978
1939.806855	18426.423734	48.026983
1936.312227	17934.576557	48.031988
1932.644225	17465.613188	48.036993
1928.697147	16993.047207	48.041997
1925.318063	16520.983873	48.047002
1921.415726	16050.948242	48.052007
1918.305514	15581.652582	48.057012
1914.321600	15114.163521	48.062017
1910.682164	14651.226446	48.067021
1907.311058	14188.955391	48.072026
1903.228325	13729.706421	48.077031
1899.903635	13271.325702	48.082036
1896.575820	12822.774017	48.087041
1892.866074	12363.626741	48.092045
1889.307569	11906.607146	48.097050
1885.466599	11459.367557	48.102055
1882.239015	11011.970343	48.107060
1878.231590	10564.942591	48.112065
1874.374349	10131.675020	48.117069
1870.722181	9691.880743	48.122074
1866.921446	9267.854691	48.127079
1862.746936	8836.097358	48.132084
1858.658155	8421.165880	48.137089
1854.150580	8021.140496	48.142093
1850.399762	7615.128554	48.147098
1845.976005	7236.809697	48.152103
1841.945199	6857.981721	48.157108
1838.209671	6492.350910	48.162113
1834.273921	6142.512761	48.167117
1830.156572	5787.244115	48.172122
1826.320538	5455.341161	48.177127
1821.937140	5130.143435	48.182132
1817.593953	4831.505235	48.187137
1813.207366	4541.612690	48.192141
1809.340498	4240.495570	48.197146
1804.933297	3981.829229	48.202151
1801.160010	3717.372102	48.207156
1797.097088	3456.969927	48.212161
1792.887717	3219.902226	48.217165
1789.095988	2979.826756	48.222170
1785.477659	2763.107609	48.227175
1781.896067	2531.399988	48.232180
1778.475796	2319.945800	48.237185
1774.421379	2117.388903	48.242189
1771.203953	1895.125018	48.247194
1767.453938	1701.694798	48.252199
1764.084462	1499.800808	48.257204
1760.677927	1292.615298	48.262209
1756.777144	1101.183004	48.267213
1753.311736	911.298570	48.272218
1749.797090	717.155831	48.277223
1746.164508	534.283985	48.282228
1742.321466	358.887928	48.287233
1738.579415	179.153074	48.292237
1734.859568	13.488691	48.297242
1724.076004	44.880552	48.302247
1714.944616	75.581893	48.307252
1709.905463	79.558435	48.312257
1706.542435	80.170509	48.317261
1704.287372	70.293301	48.322266
1701.926013	80.781582	48.327271
1700.146522	83.377607	48.332276
1697.614101	74.878648	48.337281
1694.297964	70.247496	48.342285
1691.362239	77.411535	48.347290
1688.020900	79.317354	48.352295
1683.951386	78.688487	48.357300
1680.544310	79.674410	48.362305
1677.278543	83.722951	48.367309
1674.348617	71.992449	48.372314
1670.250479	77.742901	48.377319
1666.642208	68.145915	48.382324
1663.510342	68.778962	48.387329
1660.089021	79.922589	48.392333
1657.624924	70.966922	48.397338
1654.214737	72.563925	48.402343
1651.097084	77.114588	48.407348
1647.257398	70.546486	48.412353
1643.295688	77.939813	48.417357
1639.982384	69.821827	48.422362
1636.940112	74.784693	48.427367
1633.289240	68.193535	48.432372
1629.628644	72.540806	48.437377
1625.878831	79.660712	48.442381
1622.855777	67.767550	48.447386
1619.470030	67.848502	48.452391
1615.980885	63.636589	48.457396
1612.895691	62.297718	48.462401
1608.792073	71.943539	48.467405
1605.900539	69.593778	48.472410
1602.316657	64.865110	48.477415
1599.088117	65.598628	48.482420
1594.905814	66.901365	48.487425
1591.498851	72.329112	48.492429
1588.424840	70.517110	48.497434
1585.340249	73.547217	48.502439
1581.354607	69.861828	48.507444
1577.891105	71.362733	48.512449
1574.346830	78.210209	48.517453
1571.264804	66.168051	48.522458
1567.845805	71.838113	48.527463
1563.957548	57.570818	48.532468
1560.788374	71.604778	48.537473
1557.078670	75.276338	48.542477
1553.775682	62.686456	48.547482
1550.004204	67.541362	48.552487
1546.459752	67.931756	48.557492
1542.981827	65.777673	48.562497
1539.671499	61.844817	48.567501
1536.612870	64.924667	48.572506
1533.196119	68.977731	48.577511
1529.806607	70.470287	48.582516
1525.822735	59.789697	48.587521
1521.861738	66.970946	48.592525
1518.452026	62.183544	48.597530
1515.439255	63.538371	48.602535
1512.044950	61.390259	48.607540
1508.804962	64.545794	48.612545
1504.685441	68.708242	48.617549
1501.386629	63.267678	48.622554
1497.471769	68.037338	48.627559
1494.249192	67.045722	48.632564
1490.869860	69.751556	48.637569
1487.556616	75.493746	48.642573
1484.284703	66.442381	48.647578
1480.805470	70.739287	48.652583
1477.142363	71.290521	48.657588
1473.925074	65.539884	48.662593
1469.916979	71.814160	48.667597
1466.286628	65.074304	48.672602
1462.955877	65.624429	48.677607
1459.448379	71.070993	48.682612
1456.278143	66.284289	48.687617
1452.963668	73.447171	48.692621
1449.458714	71.990155	48.697626
1445.252076	68.506859	48.702631
1441.927398	61.909253	48.707636
1438.453492	66.483736	48.712641
1434.982438	65.473854	48.717645
1431.574730	70.790994	48.722650
1428.195443	63.395147	48.727655
1424.905916	63.426341	48.732660
1421.424574	57.561792	48.737665
1417.566301	65.261721	48.742669
1414.537786	57.925175	48.747674
1410.442403	62.906432	48.752679
1406.934757	63.547370	48.757684
1403.475060	65.054024	48.762689
1400.327996	61.393161	48.767693
1396.760424	63.157047	48.772698
1393.074777	65.205061	48.777703
1389.339754	66.049067	48.782708
1386.362273	70.081223	48.787713
1382.703208	65.070064	48.792717
1379.555928	71.109122	48.797722
1375.608829	65.642932	48.802727
1372.056400	66.888781	48.807732
1369.080942	59.613584	48.812737
1364.926596	67.014757	48.817741
1361.741512	60.351145	48.822746
1358.016166	68.438504	48.827751
1354.324168	72.942538	48.832756
1351.463642	62.343393	48.837761
1347.974482	67.723834	48.842765
1344.518628	62.681051	48.847770
1341.067991	71.908875	48.852775
1337.332972	69.905561	48.857780
1333.713021	61.749939	48.862785
1330.167707	69.635275	48.867789
1326.497119	60.361262	48.872794
1323.647465	63.737621	48.877799
1319.798772	64.599327	48.882804
1316.621775	59.563764	48.887809
1312.822757	63.549793	48.892813
1309.202018	48.785354	48.897818
1305.408790	61.306115	48.902823
1301.977409	64.396544	48.907828
1299.016198	60.864950	48.912833
1295.140818	69.893135	48.917837
1291.830017	72.784466	48.922842
1288.306565	60.826893	48.927847
1284.649785	63.829023	48.932852
1281.621723	57.818013	48.937857
1277.964676	62.025549	48.942861
1274.443886	58.593713	48.947866
1270.632175	64.103455	48.952871
1266.960176	58.512210	48.957876
1263.716201	58.017484	48.962881
1260.090465	60.606667	48.967885
1256.843512	55.509238	48.972890
1253.419698	61.486939	48.977895
1250.006953	57.516280	48.982900
1246.150798	54.968699	48.987905
1242.808244	64.334719	48.992909
1239.471382	63.288153	48.997914
1235.962136	58.364427	49.002919
1232.209490	60.565251	49.007924
1228.597088	60.463226	49.012929
1224.843703	67.001583	49.017933
1221.930254	52.101761	49.022938
1218.517096	59.931725	49.027943
1214.989286	61.828641	49.032948
1211.177882	52.579736	49.037953
1207.313736	62.751427	49.042957
1203.939901	62.685036	49.047962
1200.444692	63.248130	49.052967
1197.503339	61.760363	49.057972
1194.216870	64.429619	49.062977
1190.453048	65.534387	49.067981
1186.915601	63.547796	49.072986
1183.306262	61.521777	49.077991
1179.909697	61.171031	49.082996
1176.497094	50.344653	49.088001
1172.671053	58.463508	49.093005
1169.148777	57.354064	49.098010
1165.517036	58.966610	49.103015
1162.060870	59.909600	49.108020
1159.088548	59.423220	49.113025
1155.336004	53.929951	49.118029
1151.731197	57.759214	49.123034
1148.128606	59.006564	49.128039
1144.712793	59.554141	49.133044
1141.229013	49.649992	49.138049
1137.278571	50.669921	49.143053
1134.321647	49.848960	49.148058
1131.247062	47.458144	49.153063
1127.770804	50.549242	49.158068
1124.127892	55.311397	49.163073
1119.873295	57.387887	49.168077
1116.656791	48.891108	49.173082
1113.432278	53.929815	49.178087
1109.550763	56.479732	49.183092
1106.184061	44.121332	49.188097
1102.730019	51.897552	49.193101
1099.164555	46.555504	49.198106
1095.799023	54.175582	49.203111
1092.306106	53.899954	49.208116
1088.889745	44.943919	49.213121
1085.307646	50.101561	49.218125
1081.845031	54.630015	49.223130
1078.339692	58.576676	49.228135
1074.249559	61.026196	49.233140
1071.489080	53.388561	49.238145
1067.855034	55.374791	49.243149
1064.176352	53.299473	49.248154
1060.370168	62.142891	49.253159
1057.375914	51.238762	49.258164
1053.970994	52.891942	49.263169
1050.173568	63.126017	49.268173
1046.656766	48.462520	49.273178
1043.176146	52.433808	49.278183
1039.802264	59.245287	49.283188
1036.499139	52.995563	49.288193
1032.458652	59.493200	49.293197
1028.818690	56.636757	49.298202
1025.340559	57.969149	49.303207
1021.777140	58.175891	49.308212
1018.930476	50.377679	49.313217
1015.240817	56.975727	49.318221
1011.939323	46.983120	49.323226
1008.670714	44.100514	49.328231
1004.710422	55.384971	49.333236
1001.324206	59.740193	49.338241
997.545407	54.086525	49.343245
994.351710	54.703945	49.348250
990.620473	55.373401	49.353255
987.036626	59.781533	49.358260
983.840920	46.668893	49.363265
980.010725	59.650980	49.368269
976.438177	50.450363	49.373274
973.088748	56.666431	49.378279
969.408894	54.382505	49.383284
966.288844	57.993960	49.388289
962.771358	53.242399	49.393293
959.472394	50.684056	49.398298
955.685819	54.845342	49.403303
952.075695	63.550681	49.408308
948.524632	46.386907	49.413313
944.778437	49.409311	49.418317
941.511561	46.975686	49.423322
938.155444	54.825254	49.428327
934.315935	56.327800	49.433332
931.799912	48.743884	49.438337
927.777251	45.760372	49.443341
924.283892	42.321155	49.448346
920.331746	41.079346	49.453351
917.076327	50.536205	49.458356
913.459658	46.179735	49.463361
910.199729	47.661665	49.468365
907.120383	50.472704	49.473370
903.187631	47.275889	49.478375
899.303513	54.128835	49.483380
895.836429	45.183896	49.488385
892.320418	59.331929	49.493389
889.378490	49.511158	49.498394
885.819053	51.761032	49.503399
882.122528	50.748350	49.508404
878.744276	45.475270	49.513409
874.942122	52.872266	49.518413
871.621407	47.662995	49.523418
868.022363	49.292628	49.528423
864.715088	49.706283	49.533428
861.211687	54.791583	49.538433
857.296132	51.282057	49.543437
853.957288	56.243668	49.548442
850.946861	46.009636	49.553447
847.416748	52.940353	49.558452
843.564681	53.796312	49.563457
839.747483	49.597615	49.568461
836.401223	51.909220	49.573466
832.916861	43.574410	49.578471
829.468599	47.483731	49.583476
826.496090	42.606234	49.588481
822.151138	46.591866	49.593485
818.789939	46.678571	49.598490
815.590843	50.476342	49.603495
811.709218	44.788099	49.608500
808.637715	50.011808	49.613505
805.103424	51.745261	49.618509
801.891394	48.085102	49.623514
798.060635	50.671442	49.628519
794.584979	52.294531	49.633524
791.000985	46.398612	49.638529
787.129838	53.619696	49.643533
784.056475	35.150946	49.648538
780.404158	40.689689	49.653543
776.655493	45.724589	49.658548
773.391331	45.960705	49.663553
769.974249	48.928730	49.668557
766.797961	40.080918	49.673562
763.434509	45.040035	49.678567
759.643605	44.450176	49.683572
756.111367	44.895699	49.688577
752.280445	43.986211	49.693581
748.935915	43.633743	49.698586
745.655790	46.175500	49.703591
741.966329	39.903715	49.708596
738.561489	39.468890	49.713601
735.028294	36.130814	49.718605
731.432970	44.729451	49.723610
727.883006	45.728215	49.728615
724.165556	48.151396	49.733620
720.688962	38.761898	49.738625
717.156797	44.965296	49.743629
713.886714	39.871555	49.748634
710.391179	48.302804	49.753639
706.922993	43.648014	49.758644
703.638897	44.130844	49.763649
700.292699	39.514013	49.768653
696.751821	38.935859	49.773658
693.043898	41.319596	49.778663
689.232348	44.304744	49.783668
685.706462	33.698589	49.788673
682.316222	48.776135	49.793677
679.395720	43.820963	49.798682
675.922593	41.969960	49.803687
671.967479	42.576233	49.808692
668.732950	26.331363	49.813697
664.833166	38.216991	49.818701
660.920923	45.729210	49.823706
657.772094	37.478242	49.828711
653.882561	44.553503	49.833716
650.630163	37.346852	49.838721
647.274873	50.349920	49.843725
643.891958	40.271992	49.848730
640.473403	36.476335	49.853735
636.548863	51.494694	49.858740
633.344014	46.466736	49.863745
630.076025	39.316297	49.868749
626.702509	36.389967	49.873754
623.085862	44.729345	49.878759
619.031760	44.942921	49.883764
615.795246	44.295251	49.888769
612.101093	42.377428	49.893773
608.632854	41.500084	49.898778
605.525151	37.115054	49.903783
602.277679	36.481747	49.908788
598.623409	40.603486	49.913793
594.992381	48.654048	49.918797
591.351683	43.304817	49.923802
587.813704	38.477422	49.928807
584.269523	41.025500	49.933812
580.717988	34.346308	49.938817
577.039486	41.758871	49.943821
573.531896	38.970476	49.948826
570.396375	34.184833	49.953831
566.589986	37.605777	49.958836
563.475550	32.547941	49.963841
559.848989	41.983493	49.968845
556.018571	43.601725	49.973850
552.704725	45.889330	49.978855
549.428082	43.476262	49.983860
546.093641	40.562842	49.988865
542.444176	42.532546	49.993869
538.742559	38.967627	49.998874
535.361229	29.028683	50.003879
531.343864	44.444292	50.008884
528.507324	38.637701	50.013889
524.972749	42.797760	50.018893
521.132814	46.771247	50.023898
517.991316	50.462002	50.028903
514.262285	42.083090	50.033908
511.006570	44.630561	50.038913
506.987433	48.261798	50.043917
503.512956	45.104436	50.048922
500.730596	45.562962	50.053927
496.004610	59.295102	50.058932
493.092639	50.330260	50.063937
489.763759	54.531067	50.068941
486.643937	54.526453	50.073946
482.819059	54.580982	50.078951
479.202839	58.981543	50.083956
475.654712	44.569835	50.088961
471.882489	59.558163	50.093965
468.467655	48.941086	50.098970
465.366046	43.463662	50.103975
461.637588	44.749668	50.108980
458.596715	58.649731	50.113985
454.975110	53.674026	50.118989
451.391483	43.298363	50.123994
447.510577	46.006443	50.128999
444.048283	47.646473	50.134004
440.819949	36.408770	50.139009
437.147411	45.294683	50.144013
433.531504	46.249967	50.149018
430.348708	53.126643	50.154023
427.010046	45.965096	50.159028
423.070743	46.220939	50.164033
419.152410	43.980553	50.169037
416.020561	51.178318	50.174042
412.721890	49.531141	50.179047
409.012151	47.584139	50.184052
406.225828	37.622188	50.189057
402.282673	43.203078	50.194061
398.654542	47.788991	50.199066
395.472389	41.637605	50.204071
391.535923	42.857928	50.209076
388.390005	35.296238	50.214081
384.614980	37.146307	50.219085
380.866737	42.453254	50.224090
377.122574	32.232317	50.229095
373.784824	48.681046	50.234100
370.966097	36.718385	50.239105
367.166771	46.212482	50.244109
363.716829	34.797333	50.249114
360.321902	37.300054	50.254119
356.265677	38.469427	50.259124
352.931737	43.933333	50.264129
349.385511	32.036484	50.269133
345.751514	44.744430	50.274138
342.728744	37.201539	50.279143
339.314523	41.472589	50.284148
335.679663	36.755231	50.289153
332.114319	46.772872	50.294157
328.678643	35.966096	50.299162
325.507312	37.064146	50.304167
321.383994	43.638010	50.309172
317.910247	37.047995	50.314177
314.381878	43.709563	50.319181
310.916607	53.243407	50.324186
307.774994	42.039684	50.329191
304.031257	45.368650	50.334196
300.682191	43.615444	50.339201
296.925141	45.310871	50.344205
293.488955	40.632190	50.349210
290.186577	45.831768	50.354215
286.420423	43.403202	50.359220
283.111664	37.581586	50.364225
279.219638	41.775174	50.369229
276.015036	42.603172	50.374234
272.671909	45.382569	50.379239
269.026614	43.226247	50.384244
265.504512	42.132717	50.389249
261.869814	49.079757	50.394253
258.306096	42.465795	50.399258
255.314802	45.690276	50.404263
251.441800	41.047972	50.409268
248.382429	36.940203	50.414273
244.832765	44.108115	50.419277
241.004346	43.796247	50.424282
237.672075	37.652443	50.429287
233.690462	45.485535	50.434292
230.273268	33.802737	50.439297
227.129808	50.357254	50.444301
223.193143	46.572726	50.449306
219.893763	38.949540	50.454311
216.242198	47.246926	50.459316
213.073479	46.797555	50.464321
209.591062	46.849427	50.469325
206.143777	51.600189	50.474330
202.818853	36.037039	50.479335
198.967843	49.550712	50.484340
195.501738	37.856551	50.489345
191.988856	41.152752	50.494349
188.187584	43.528938	50.499354
184.965333	49.864459	50.504359
181.441511	35.759091	50.509364
178.213102	37.913216	50.514369
173.984262	37.540317	50.519373
170.578101	34.204703	50.524378
167.408646	39.513305	50.529383
163.808076	48.989128	50.534388
160.622808	36.194592	50.539393
156.816152	43.927688	50.544397
153.203767	37.555437	50.549402
149.940042	44.188472	50.554407
146.299569	41.518908	50.559412
142.722752	39.215908	50.564417
139.114630	40.707842	50.569421
135.897095	46.109353	50.574426
132.601987	45.360141	50.579431
129.239266	44.058326	50.584436
125.701029	36.817186	50.589441
121.961090	35.520320	50.594445
118.433154	37.952032	50.599450
114.779786	45.329083	50.604455
111.027150	41.560218	50.609460
108.125427	22.796036	50.614465
104.614016	34.475693	50.619469
100.842564	32.946464	50.624474
97.331162	35.872298	50.629479
93.543413	32.719489	50.634484
90.222310	38.266836	50.639489
86.774173	40.410890	50.644493
83.261893	33.820596	50.649498
80.098610	37.799510	50.654503
76.460620	42.016844	50.659508
72.913475	37.178315	50.664513
69.263251	36.354693	50.669517
65.886980	44.438391	50.674522
62.200277	39.915811	50.679527
58.355850	46.085627	50.684532
55.090182	39.036173	50.689537
51.863515	37.871371	50.694541
48.492812	37.358560	50.699546
45.357256	33.303814	50.704551
41.275431	43.392392	50.709556
37.943827	40.681085	50.714561
34.490110	42.794378	50.719565
30.703406	39.388325	50.724570
27.420099	42.851276	50.729575
23.645255	42.353937	50.734580
19.955691	39.606620	50.739585
16.562872	32.820575	50.744589
13.095569	40.598921	50.749594
9.638736	39.343414	50.754599
5.904805	49.184849	50.759604
2.643792	32.899985	50.764609