Fri Aug 26 11:37:52 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.438945	104.082541	0.000000
0.837848	119.465502	0.005005
0.720020	116.680922	0.010010
0.745288	104.212246	0.015014
0.184529	102.081909	0.020019
0.468202	98.829871	0.025024
0.105810	103.268040	0.030029
0.042174	89.766046	0.035034
0.140369	82.869885	0.040038
-0.381766	81.669978	0.045043
-0.728335	63.460246	0.050048
-0.910210	66.475130	0.055053
-1.499638	66.649236	0.060058
-1.370772	51.737946	0.065062
-1.913734	52.148419	0.070067
-2.260492	40.962043	0.075072
-2.049973	38.157990	0.080077
-2.794936	30.924906	0.085082
-2.930823	19.930331	0.090086
-3.218212	24.511822	0.095091
-3.145502	16.322560	0.100096
-3.563351	14.748930	0.105101
-4.813655	7.303481	0.110106
-4.165578	15.633763	0.115110
-4.527560	10.916265	0.120115
-4.640121	4.673023	0.125120
-5.204938	11.974145	0.130125
-6.000534	11.582422	0.135130
-5.898445	5.672742	0.140134
-6.456502	14.453397	0.145139
-6.100735	5.995451	0.150144
-6.070176	17.424175	0.155149
-6.673102	12.927682	0.160154
-7.108626	5.810940	0.165158
-7.516214	11.575362	0.170163
-7.817201	10.385319	0.175168
-7.677035	7.775716	0.180173
-8.075477	18.167124	0.185178
-8.034126	18.505602	0.190182
-8.985903	12.671421	0.195187
-8.761181	12.285347	0.200192
-8.876771	13.818808	0.205197
-9.224320	14.948637	0.210202
-9.158994	3.533617	0.215206
-9.857749	6.742858	0.220211
-10.405227	7.024324	0.225216
-10.376961	2.907268	0.230221
-10.450157	16.671095	0.235226
-10.519470	7.036020	0.240230
-10.742103	19.412132	0.245235
-11.631007	7.791352	0.250240
-11.295612	12.642856	0.255245
-12.216419	9.151277	0.260250
-11.591127	1.322061	0.265254
-12.125169	15.432876	0.270259
-12.452405	3.148865	0.275264
-13.175793	9.174419	0.280269
-13.457367	19.718468	0.285274
-13.331993	13.919051	0.290278
-13.468169	12.725494	0.295283
-13.478125	0.028267	0.300288
-13.628609	7.318659	0.305293
-14.538128	12.541156	0.310298
-14.577095	9.250787	0.315302
-14.864053	8.722926	0.320307
-14.823319	10.507283	0.325312
-14.862375	6.109654	0.330317
-15.226590	18.321154	0.335322
-16.122050	7.005105	0.340326
-16.707328	15.249016	0.345331
-16.438170	9.281686	0.350336
-16.245450	16.344645	0.355341
-16.614521	17.069716	0.360346
-16.921898	4.488394	0.365350
-17.202411	5.427459	0.370355
-17.380096	13.370634	0.375360
-17.464587	15.465545	0.380365
-17.939858	7.367935	0.385370
-18.223166	6.618051	0.390374
-18.840128	8.640847	0.395379
-19.074039	6.968979	0.400384
-18.786447	1.391073	0.405389
-18.978968	7.314989	0.410394
-19.585132	-6.684569	0.415398
-20.189800	10.591385	0.420403
-19.967334	4.624999	0.425408
-20.123773	1.564886	0.430413
-20.589908	4.120999	0.435418
-20.173758	0.339007	0.440422
-21.274464	5.727306	0.445427
-21.898367	4.090850	0.450432
-21.695970	0.354794	0.455437
-21.762937	10.020731	0.460442
-21.847798	3.222703	0.465446
-22.271707	9.995703	0.470451
-22.473513	9.226801	0.475456
-22.706698	10.395770	0.480461
-23.140440	13.067059	0.485466
-23.346103	8.448606	0.490470
-23.955688	11.596510	0.495475
-23.694967	5.352095	0.500480
-23.643572	5.726972	0.505485
-24.459099	11.728909	0.510490
-24.380991	7.933112	0.515494
-24.801072	10.488382	0.520499
-24.934553	10.986954	0.525504
-24.984252	7.964002	0.530509
-26.343283	12.456086	0.535514
-26.155144	5.318170	0.540518
-26.280531	9.333450	0.545523
-26.624526	8.131123	0.550528
-26.511574	6.386268	0.555533
-26.647849	18.258567	0.560538
-26.397774	0.531791	0.565542
-27.093848	13.282156	0.570547
-27.980574	15.448191	0.575552
-27.788478	11.742209	0.580557
-27.500839	13.111651	0.585562
-27.980206	8.760432	0.590566
-28.836279	5.521359	0.595571
-28.950834	5.865129	0.600576
-29.382725	-1.562211	0.605581
-29.320328	8.501183	0.610586
-29.138639	3.335221	0.615590
-30.295229	10.737971	0.620595
-30.354077	10.810485	0.625600
-30.336801	13.250206	0.630605
-30.569142	15.105554	0.635610
-30.725173	0.324087	0.640614
-31.016185	6.241192	0.645619
-31.083490	4.597167	0.650624
-31.502633	14.298957	0.655629
-31.995599	9.968836	0.660634
-31.859793	4.053908	0.665638
-32.264237	3.420957	0.670643
-32.346137	3.557170	0.675648
-32.790716	5.034289	0.680653
-33.562796	8.805421	0.685658
-33.574780	5.735470	0.690662
-33.950035	7.546633	0.695667
-33.847151	5.800181	0.700672
-33.623781	-2.431509	0.705677
-34.129113	-0.435585	0.710682
-34.687982	-6.783333	0.715686
-35.288403	16.869861	0.720691
-35.204136	10.811100	0.725696
-35.086536	7.255918	0.730701
-35.382494	10.013317	0.735706
-35.313082	6.256838	0.740710
-36.316044	10.342319	0.745715
-36.666629	9.292872	0.750720
-36.360355	2.060637	0.755725
-36.574450	8.981296	0.760730
-37.395833	-0.818240	0.765734
-37.925084	13.491134	0.770739
-38.430829	13.554138	0.775744
-37.719240	17.331540	0.780749
-38.190723	12.039492	0.785754
-37.701456	9.916516	0.790758
-38.149849	11.337284	0.795763
-38.281802	6.871865	0.800768
-39.025072	7.459053	0.805773
-39.133229	2.300256	0.810778
-39.370379	-0.766271	0.815782
-40.538732	8.017655	0.820787
-40.480621	8.442105	0.825792
-40.372402	8.653117	0.830797
-40.924853	3.209168	0.835802
-40.946489	-7.322302	0.840806
-41.253626	9.461251	0.845811
-41.261996	2.803170	0.850816
-40.877261	0.734435	0.855821
-41.683568	10.926758	0.860826
-41.817896	14.215794	0.865830
-42.225594	8.353851	0.870835
-42.557273	11.698922	0.875840
-43.510434	8.762857	0.880845
-43.287605	13.581267	0.885850
-43.558907	11.807657	0.890854
-44.035996	14.330677	0.895859
-43.877506	6.713341	0.900864
-44.237663	4.279711	0.905869
-44.295025	12.738805	0.910874
-44.331251	9.546083	0.915878
-44.633658	10.884012	0.920883
-44.819240	13.472372	0.925888
-45.509851	7.078696	0.930893
-45.622163	11.522195	0.935898
-45.547736	4.364022	0.940902
-46.193302	15.379176	0.945907
-46.916162	12.037106	0.950912
-47.235285	5.702645	0.955917
-47.298895	10.815581	0.960922
-47.418199	9.758597	0.965926
-47.492826	8.637712	0.970931
-47.359702	5.067459	0.975936
-47.121201	8.083317	0.980941
-47.493812	7.230283	0.985946
-48.425258	6.309240	0.990950
-48.865838	11.423923	0.995955
-48.669144	14.753164	1.000960
-48.567210	11.466167	1.005965
-49.847747	11.760533	1.010970
-49.857131	8.418105	1.015974
-50.182704	11.138988	1.020979
-50.387641	4.059112	1.025984
-50.397360	11.878060	1.030989
-50.614135	14.768659	1.035994
-50.357422	9.401196	1.040998
-51.070003	17.225181	1.046003
-51.270887	7.177176	1.051008
-51.823016	8.648896	1.056013
-51.922061	5.620974	1.061018
-51.348055	2.893205	1.066022
-52.417352	12.629785	1.071027
-52.740431	7.589869	1.076032
-53.009372	0.905924	1.081037
-53.259570	1.058849	1.086042
-53.084631	3.996020	1.091046
-53.659644	6.493158	1.096051
-54.492219	1.883736	1.101056
-54.284127	-2.606152	1.106061
-54.616072	13.516901	1.111066
-54.814907	12.013573	1.116070
-54.756157	6.869916	1.121075
-54.953402	13.104605	1.126080
-54.901096	6.503513	1.131085
-55.570495	15.785539	1.136090
-56.141646	2.223437	1.141094
-56.146908	15.473661	1.146099
-56.520085	20.071670	1.151104
-55.939981	11.755959	1.156109
-56.987644	4.826276	1.161114
-57.303613	16.628477	1.166118
-57.733327	10.115088	1.171123
-58.074906	11.474934	1.176128
-57.681461	17.611328	1.181133
-58.174900	15.862814	1.186138
-58.266992	6.857691	1.191142
-58.809780	6.603772	1.196147
-59.048798	8.820814	1.201152
-58.835406	6.569957	1.206157
-59.275360	12.836108	1.211162
-59.025227	6.903379	1.216166
-59.679561	9.634322	1.221171
-60.290310	8.919602	1.226176
-60.284186	6.463743	1.231181
-60.895426	14.657912	1.236186
-60.584307	2.369426	1.241190
-61.328391	7.540854	1.246195
-61.763422	0.547424	1.251200
-61.705006	6.558813	1.256205
-62.083170	9.588430	1.261210
-62.130901	11.427689	1.266214
-61.660458	8.076988	1.271219
-62.983848	10.538794	1.276224
-63.306074	-4.308534	1.281229
-63.626103	3.644143	1.286234
-63.353677	3.427805	1.291238
-63.375942	7.006263	1.296243
-63.788008	2.052969	1.301248
-63.392921	-2.396434	1.306253
-64.109634	4.365205	1.311258
-64.154357	9.396108	1.316262
-64.832844	3.304257	1.321267
-65.447794	7.383105	1.326272
-65.661578	7.966944	1.331277
-65.935662	8.180534	1.336282
-66.081699	6.444367	1.341286
-66.239317	9.243499	1.346291
-66.335177	5.857591	1.351296
-66.499534	7.360680	1.356301
-67.567222	4.413976	1.361306
-67.579154	0.388600	1.366310
-67.844818	4.321319	1.371315
-67.910964	8.735483	1.376320
-67.696352	-1.114625	1.381325
-67.728075	18.169616	1.386330
-67.965715	11.445994	1.391334
-68.558955	8.738618	1.396339
-68.762547	8.640687	1.401344
-68.752939	8.639270	1.406349
-69.286690	3.856776	1.411354
-69.931826	-0.174409	1.416358
-70.806833	16.419163	1.421363
-70.843403	4.077248	1.426368
-70.217405	4.302550	1.431373
-70.451709	5.683657	1.436378
-70.629335	-2.020541	1.441382
-70.780570	2.577706	1.446387
-71.514272	1.410749	1.451392
-71.771175	0.678900	1.456397
-72.290414	-0.031085	1.461402
-71.920866	2.992839	1.466406
-72.166695	-2.116046	1.471411
-72.331355	-0.103565	1.476416
-73.007557	1.495036	1.481421
-73.716232	5.528368	1.486426
-73.370549	2.323639	1.491430
-74.133772	7.978921	1.496435
-73.955919	6.334688	1.501440
-73.688809	3.341503	1.506445
-74.459995	3.515437	1.511450
-74.699739	-1.233741	1.516454
-75.134860	8.714131	1.521459
-75.000269	1.208084	1.526464
-74.919381	0.591314	1.531469
-76.025510	0.007507	1.536474
-76.327345	-0.552836	1.541478
-76.484693	2.043780	1.546483
-76.636894	7.727307	1.551488
-76.486315	4.318846	1.556493
-76.765749	-0.471606	1.561498
-76.609500	-0.021310	1.566502
-77.598582	2.002480	1.571507
-78.362164	3.592540	1.576512
-77.789384	-1.124966	1.581517
-78.357292	5.724232	1.586522
-78.184628	-4.818506	1.591526
-78.348378	-5.685077	1.596531
-78.918817	3.337933	1.601536
-79.510550	1.753417	1.606541
-79.689383	2.793704	1.611546
-79.798063	4.936670	1.616550
-79.721078	6.446473	1.621555
-80.168108	-2.474906	1.626560
-80.459555	-1.749267	1.631565
-81.317896	2.696495	1.636570
-80.599950	-2.492850	1.641574
-81.259655	-3.962383	1.646579
-81.464968	-5.834846	1.651584
-81.413103	-9.534807	1.656589
-81.645134	1.352676	1.661594
-82.115055	-8.666082	1.666598
-82.209861	8.014804	1.671603
-82.847630	0.790360	1.676608
-82.633250	-11.090762	1.681613
-83.796800	6.063398	1.686618
-83.803387	-4.261612	1.691622
-84.088380	0.480842	1.696627
-84.496873	-6.497734	1.701632
-84.096191	-11.840150	1.706637
-84.706038	-1.143770	1.711642
-84.245274	-0.769360	1.716646
-84.634695	8.380487	1.721651
-84.952380	-0.273141	1.726656
-85.256624	4.010420	1.731661
-85.807447	6.706265	1.736666
-85.795336	-11.897731	1.741670
-86.122847	7.666659	1.746675
-86.745291	-0.423844	1.751680
-86.870603	-5.042147	1.756685
-87.067909	3.309021	1.761690
-86.978840	-0.944044	1.766694
-87.286462	-0.171595	1.771699
-87.943816	3.869564	1.776704
-87.947226	-1.783247	1.781709
-88.517606	4.076116	1.786714
-88.467404	-0.582170	1.791718
-88.698138	-4.367840	1.796723
-88.780486	-5.319848	1.801728
-88.903434	6.423816	1.806733
-89.530677	2.168391	1.811738
-89.929878	-2.818541	1.816742
-89.808254	6.492171	1.821747
-90.215688	7.267506	1.826752
-90.050721	5.460771	1.831757
-91.546411	6.965513	1.836762
-91.676502	-1.147868	1.841766
-91.205864	8.668467	1.846771
-91.249580	5.166877	1.851776
-91.401856	-4.923485	1.856781
-91.749822	0.445683	1.861786
-91.672322	-8.503580	1.866790
-92.202252	0.396066	1.871795
-93.212362	0.002947	1.876800
-93.154568	0.709010	1.881805
-93.063297	1.574369	1.886810
-93.148510	-0.066867	1.891814
-93.676585	3.954163	1.896819
-94.390326	-2.492849	1.901824
-94.357622	-3.519717	1.906829
-94.509215	0.977349	1.911834
-94.704424	1.295713	1.916838
-94.449175	5.375107	1.921843
-95.454806	4.503581	1.926848
-95.757106	0.545562	1.931853
-96.219471	7.489054	1.936858
-96.027340	-4.663843	1.941862
-95.776744	-1.770090	1.946867
-96.551971	-0.399671	1.951872
-96.513389	2.871930	1.956877
-97.043991	4.258043	1.961882
-97.642554	-0.893993	1.966886
-97.457307	0.396480	1.971891
-97.789533	5.133635	1.976896
-97.434272	-4.149932	1.981901
-98.233620	-0.333429	1.986906
-98.880648	-3.168463	1.991910
-99.165876	5.835449	1.996915
-99.089506	0.904424	2.006912
-98.866907	2.922586	2.016909
-98.005173	2.018822	2.026906
-98.053364	-2.135859	2.036902
-97.666037	3.626203	2.046899
-96.956679	10.617873	2.056896
-95.914237	4.022144	2.066893
-95.258913	2.488472	2.076890
-95.412339	-0.294054	2.086886
-94.994275	3.594286	2.096883
-94.096058	3.495771	2.106880
-93.701049	4.413241	2.116877
-93.654445	3.044036	2.126874
-92.770318	8.738251	2.136870
-92.359074	-0.622790	2.146867
-91.310661	9.186015	2.156864
-90.797148	2.571275	2.166861
-91.351515	3.737930	2.176858
-90.272684	3.630299	2.186854
-89.592249	6.251893	2.196851
-89.393660	6.474546	2.206848
-88.777630	4.798110	2.216845
-88.531866	2.523613	2.226842
-87.848245	8.325072	2.236838
-86.727031	5.160357	2.246835
-86.829646	3.738361	2.256832
-86.709803	11.411011	2.266829
-85.861307	9.118692	2.276826
-85.390582	7.296993	2.286822
-84.390442	3.653802	2.296819
-84.175133	0.886720	2.306816
-83.796444	8.443042	2.316813
-82.835459	9.706364	2.326810
-82.559820	6.112624	2.336806
-81.934068	4.970014	2.346803
-81.895249	2.135381	2.356800
-81.616575	7.369520	2.366797
-80.753017	4.260761	2.376794
-80.378425	7.911959	2.386790
-79.599594	4.917758	2.396787
-79.550141	5.252327	2.406784
-78.364176	8.482599	2.416781
-78.137669	6.698925	2.426778
-78.089557	-1.322663	2.436774
-76.751430	2.647330	2.446771
-76.389609	-1.048522	2.456768
-76.651705	0.503431	2.466765
-75.975606	1.925147	2.476762
-75.347600	0.820199	2.486758
-75.177980	4.132691	2.496755
-73.645225	1.648307	2.506752
-73.777019	3.477736	2.516749
-73.066865	10.662514	2.526746
-72.556682	10.269635	2.536742
-72.202434	7.157814	2.546739
-71.895765	4.560233	2.556736
-70.852348	6.685004	2.566733
-70.871463	7.388197	2.576730
-70.661579	5.854191	2.586726
-69.628474	9.108264	2.596723
-69.114054	4.869149	2.606720
-68.264155	9.038702	2.616717
-67.927513	7.282227	2.626714
-67.828397	4.659943	2.636710
-67.571974	5.988618	2.646707
-66.748635	1.121718	2.656704
-66.266879	8.630317	2.666701
-65.411200	7.911223	2.676698
-65.182155	12.551231	2.686694
-65.060721	3.884685	2.696691
-64.583014	0.205633	2.706688
-63.624472	-2.775368	2.716685
-62.643295	1.291383	2.726682
-62.835733	2.731126	2.736678
-62.536975	0.869681	2.746675
-61.556991	-4.670984	2.756672
-61.125630	-2.894394	2.766669
-60.848586	2.875339	2.776666
-60.097126	3.113276	2.786662
-59.691563	2.682836	2.796659
-59.278453	-0.621874	2.806656
-58.387735	-1.682198	2.816653
-58.269954	-0.034174	2.826650
-58.011594	4.737478	2.836646
-57.165721	1.834205	2.846643
-56.511223	2.432517	2.856640
-56.239098	4.332100	2.866637
-55.381652	0.809325	2.876634
-55.122523	5.979987	2.886630
-54.850288	5.091985	2.896627
-54.094520	5.981796	2.906624
-53.839502	6.084794	2.916621
-53.088303	5.185571	2.926618
-52.543642	-0.917686	2.936614
-52.732951	8.608683	2.946611
-51.556347	6.132236	2.956608
-51.056104	7.831581	2.966605
-50.464841	3.729383	2.976602
-49.732401	3.713699	2.986598
-49.928777	0.139601	2.996595
-49.408989	-0.365642	3.006592
-48.239099	0.120748	3.016589
-47.906538	3.167127	3.026586
-47.875222	2.592225	3.036582
-47.270447	7.933977	3.046579
-46.246435	2.826764	3.056576
-46.266815	5.519464	3.066573
-45.664664	11.830940	3.076570
-45.095340	6.186324	3.086566
-44.868124	4.671793	3.096563
-44.080392	9.034752	3.106560
-43.652337	5.708708	3.116557
-43.172629	3.495985	3.126554
-42.408514	-1.925543	3.136550
-41.877160	-1.292218	3.146547
-41.779447	-4.728379	3.156544
-41.311843	1.838451	3.166541
-40.913020	5.102588	3.176538
-40.235047	0.885524	3.186534
-39.145156	9.892788	3.196531
-38.990439	1.373109	3.206528
-38.951208	7.271735	3.216525
-38.059251	-0.580311	3.226522
-37.611120	3.569437	3.236518
-37.339035	1.743822	3.246515
-36.421560	0.761692	3.256512
-36.202215	-0.856147	3.266509
-35.624813	1.198637	3.276506
-34.959015	4.858347	3.286502
-34.611030	2.403215	3.296499
-34.096989	7.043197	3.306496
-33.542204	3.314131	3.316493
-33.402559	-0.784272	3.326490
-32.865673	-0.874042	3.336486
-32.055138	-0.848033	3.346483
-31.417726	-4.504435	3.356480
-30.590526	5.516209	3.366477
-30.104381	6.574708	3.376474
-30.346452	7.081374	3.386470
-30.046788	2.866193	3.396467
-29.102817	5.570299	3.406464
-28.934553	5.351029	3.416461
-27.634357	6.213093	3.426458
-27.255542	3.664465	3.436454
-27.222922	3.276253	3.446451
-26.833696	-2.939014	3.456448
-25.908761	2.489101	3.466445
-25.968275	3.464671	3.476442
-24.684618	-1.150795	3.486438
-24.299212	8.859446	3.496435
-24.099878	3.975664	3.506432
-23.944699	1.202105	3.516429
-23.072990	-0.751715	3.526426
-22.892797	1.985781	3.536422
-21.725921	1.747240	3.546419
-21.342164	-0.798989	3.556416
-21.391936	0.418976	3.566413
-20.440288	5.437468	3.576410
-19.868799	2.903189	3.586406
-19.737474	6.243820	3.596403
-19.147929	1.695245	3.606400
-18.589694	-1.556036	3.616397
-18.388955	0.196277	3.626394
-17.638754	6.288305	3.636390
-17.265172	3.094283	3.646387
-16.345505	0.708525	3.656384
-15.924794	2.759197	3.666381
-15.809646	2.864966	3.676378
-14.780679	-0.453271	3.686374
-14.381748	-0.724294	3.696371
-14.236901	-2.118298	3.706368
-13.501368	-9.331454	3.716365
-12.993485	-1.054007	3.726362
-12.733437	5.180859	3.736358
-12.263799	-1.398543	3.746355
-11.424953	1.578514	3.756352
-11.223615	-4.927436	3.766349
-10.617332	2.561777	3.776346
-10.310373	-0.314606	3.786342
-8.763780	-0.916366	3.796339
-8.896468	7.866286	3.806336
-8.547636	-4.766770	3.816333
-8.362862	-1.513654	3.826330
-7.182280	-0.895884	3.836326
-6.745859	-2.775595	3.846323
-6.876159	0.155958	3.856320
-6.295818	5.301952	3.866317
-5.960248	9.766992	3.876314
-4.881546	14.309559	3.886310
-4.831601	15.949141	3.896307
-4.435477	25.621949	3.906304
-3.683130	33.107440	3.916301
-3.565765	43.374839	3.926298
-3.092580	50.333616	3.936294
-2.193401	62.468617	3.946291
-1.606144	72.681878	3.956288
-1.402362	83.182927	3.966285
-1.379907	96.056318	3.976282
-0.365220	113.089653	3.986278
0.000000	120.449758	3.991283
-0.118902	131.379822	3.996288
0.393104	130.879416	4.001293
0.122346	146.097752	4.006298
0.348295	148.204454	4.011302
0.348658	144.423895	4.016307
0.263183	145.686930	4.021312
0.754827	142.430977	4.026317
0.733029	147.417224	4.031322
0.846316	166.239310	4.036326
0.869464	150.085257	4.041331
0.652180	152.166059	4.046336
0.821347	163.747299	4.051341
1.381943	160.736864	4.056346
0.796120	160.113165	4.061350
1.346250	148.907298	4.066355
0.773672	153.492096	4.071360
0.866688	147.745128	4.076365
0.451841	145.503485	4.081370
0.462087	153.869868	4.086374
1.447184	156.440488	4.091379
1.070619	152.810360	4.096384
0.962461	145.465426	4.101389
0.823285	146.825405	4.106394
1.053851	150.623950	4.111398
1.164646	142.944379	4.116403
0.993101	148.428491	4.121408
1.425213	142.799566	4.126413
1.197850	156.897545	4.131418
1.127795	153.877737	4.136422
1.182412	152.534244	4.141427
1.104868	159.566576	4.146432
0.930558	154.731237	4.151437
0.739369	157.738095	4.156442
0.437997	156.864469	4.161446
0.920723	153.242917	4.166451
1.037859	161.152911	4.171456
1.230317	168.345683	4.176461
1.120638	159.972787	4.181466
1.250076	168.766697	4.186470
1.383455	164.965423	4.191475
0.705947	159.018889	4.196480
1.032578	164.735481	4.201485
1.239608	165.487916	4.206490
1.086422	178.587298	4.211494
1.379911	170.271845	4.216499
1.815859	176.249824	4.221504
1.358879	167.029351	4.226509
1.631352	151.912125	4.231514
0.887016	151.752856	4.236518
1.098011	147.360551	4.241523
1.116657	164.628191	4.246528
1.649801	166.405499	4.251533
1.286026	160.970086	4.256538
1.095458	172.800325	4.261542
1.144044	170.881982	4.266547
0.741986	173.690727	4.271552
1.370412	167.170710	4.276557
1.548488	172.287192	4.281562
1.369014	173.495264	4.286566
1.430224	170.746073	4.291571
1.555211	183.302288	4.296576
1.282782	176.156920	4.301581
1.449930	172.071984	4.306586
1.127243	179.987192	4.311590
1.732580	179.595637	4.316595
1.612627	178.918384	4.321600
1.529814	182.781546	4.326605
1.553303	183.508776	4.331610
1.247538	186.492351	4.336614
1.840764	184.622082	4.341619
1.146121	180.386592	4.346624
1.193330	180.151536	4.351629
1.968722	177.629662	4.356634
1.400404	177.547388	4.361638
1.908218	170.229922	4.366643
1.647843	182.026744	4.371648
1.758055	178.940901	4.376653
1.653532	177.818332	4.381658
1.424514	185.158989	4.386662
2.089990	176.295246	4.391667
1.821029	176.134726	4.396672
1.868359	178.443244	4.401677
1.953896	180.157370	4.406682
2.180088	184.140096	4.411686
2.196852	166.190056	4.416691
1.847793	171.372792	4.421696
1.506956	162.681554	4.426701
1.945320	168.111840	4.431706
1.580438	162.319104	4.436710
1.727463	165.925021	4.441715
1.701888	178.251580	4.446720
1.744981	181.323203	4.451725
2.197627	180.249922	4.456730
2.134547	174.416520	4.461734
1.729723	166.048447	4.466739
1.590001	164.643465	4.471744
1.448387	176.016843	4.476749
1.710447	175.729354	4.481754
1.956293	178.098710	4.486758
2.235076	186.344206	4.491763
2.006164	180.406911	4.496768
2.038560	184.312246	4.501773
1.824618	184.418399	4.506778
1.787867	185.041116	4.511782
2.025917	173.659203	4.516787
1.912884	186.986451	4.521792
1.996072	183.117060	4.526797
1.869661	179.292958	4.531802
2.204416	186.542674	4.536806
2.243941	178.757127	4.541811
1.938343	180.763100	4.546816
1.833802	183.958947	4.551821
1.893196	176.274709	4.556826
1.517547	186.662667	4.561830
2.099899	169.915342	4.566835
2.094950	178.901018	4.571840
1.746880	173.966180	4.576845
1.735040	185.809728	4.581850
2.169123	189.307682	4.586854
2.340379	192.644083	4.591859
1.918940	193.301386	4.596864
2.313557	190.914723	4.601869
2.662044	201.759406	4.606874
2.372142	193.360771	4.611878
2.360429	184.602461	4.616883
1.965832	177.409676	4.621888
1.979802	179.612659	4.626893
2.296824	185.488938	4.631898
2.397317	193.702087	4.636902
2.756774	186.246366	4.641907
2.116825	183.562050	4.646912
1.932079	180.107690	4.651917
2.204806	190.828123	4.656922
2.392845	194.652281	4.661926
2.741389	198.100281	4.666931
2.525065	204.467721	4.671936
1.968596	180.254255	4.676941
2.121477	195.280127	4.681946
1.976171	201.402397	4.686950
2.536654	192.627758	4.691955
1.980716	207.833602	4.696960
2.256503	198.299712	4.701965
2.280072	206.148366	4.706970
2.352525	202.119295	4.711974
2.654745	200.974524	4.716979
2.613009	208.355632	4.721984
2.662634	213.356086	4.726989
2.601804	201.308862	4.731994
2.388163	210.020170	4.736998
2.614069	197.441098	4.742003
2.377084	203.365676	4.747008
1.967924	201.309797	4.752013
2.452107	202.705600	4.757018
2.110604	210.766116	4.762022
2.767535	211.072028	4.767027
2.748856	224.384613	4.772032
2.788798	216.409164	4.777037
2.445132	204.377502	4.782042
2.628654	219.379642	4.787046
2.816531	214.747316	4.792051
2.663547	215.448241	4.797056
2.752218	216.892970	4.802061
2.422870	211.993171	4.807066
2.600662	217.036945	4.812070
2.741332	218.789946	4.817075
2.883062	220.349797	4.822080
3.230691	225.629716	4.827085
3.066216	207.973602	4.832090
2.634417	206.430599	4.837094
2.729471	203.676134	4.842099
2.575378	205.737612	4.847104
2.869569	212.512776	4.852109
2.706422	215.119818	4.857114
2.737688	224.283372	4.862118
2.967760	222.219710	4.867123
2.666280	221.554901	4.872128
2.942193	220.765393	4.877133
3.321741	228.602923	4.882138
2.629419	218.643964	4.887142
2.958978	217.653119	4.892147
2.641471	230.623103	4.897152
2.779608	225.663169	4.902157
2.967013	227.544933	4.907162
2.646745	231.043289	4.912166
2.839332	229.200593	4.917171
2.491155	232.829842	4.922176
2.946210	221.588113	4.927181
2.909883	228.218595	4.932186
2.871569	232.609502	4.937190
3.114001	227.244196	4.942195
2.803263	229.032680	4.947200
2.770719	232.378674	4.952205
3.073820	241.468276	4.957210
3.492204	253.453688	4.962214
3.624500	229.762490	4.967219
3.162712	226.294308	4.972224
3.085049	222.424644	4.977229
3.314198	222.850942	4.982234
3.216957	227.510444	4.987238
3.899281	225.657936	4.992243
3.286860	231.308791	4.997248
3.225495	223.330130	5.002253
3.318065	215.691328	5.007258
3.113752	228.020442	5.012262
3.038485	218.503235	5.017267
3.472479	231.824438	5.022272
3.330373	220.833870	5.027277
3.325181	220.451952	5.032282
3.362046	228.697170	5.037286
3.713368	220.167050	5.042291
3.389017	226.902485	5.047296
3.553927	217.445958	5.052301
3.312836	215.730896	5.057306
3.276984	222.051261	5.062310
3.552833	224.817739	5.067315
3.195541	229.755007	5.072320
3.642555	229.030605	5.077325
3.007917	207.151416	5.082330
3.305429	221.635949	5.087334
3.455709	222.805337	5.092339
3.445789	225.882058	5.097344
3.661428	219.274435	5.102349
3.322527	223.838687	5.107354
2.936475	223.114281	5.112358
2.679850	224.837393	5.117363
2.972327	224.333201	5.122368
3.241275	220.767066	5.127373
3.734825	226.780385	5.132378
3.643045	225.443862	5.137382
3.580071	217.468618	5.142387
3.306343	225.768520	5.147392
3.679567	225.694671	5.152397
3.527673	225.927202	5.157402
3.712141	224.474904	5.162406
3.622102	222.438937	5.167411
3.330861	228.068257	5.172416
3.598267	230.586120	5.177421
3.850111	236.599111	5.182426
3.801411	237.774172	5.187430
3.746255	225.944341	5.192435
3.419242	233.078818	5.197440
3.780931	242.795199	5.202445
4.027281	234.952116	5.207450
3.600305	237.037103	5.212454
4.189541	224.312860	5.217459
3.784856	224.651187	5.222464
3.638595	224.541164	5.227469
3.620111	228.039988	5.232474
3.032651	243.314044	5.237478
3.447889	242.528152	5.242483
3.780749	248.218492	5.247488
3.491934	244.710721	5.252493
3.791457	243.180398	5.257498
3.502051	254.349051	5.262502
3.760025	243.818186	5.267507
3.780777	253.233323	5.272512
4.017765	254.474633	5.277517
3.980767	243.597397	5.282522
3.800049	250.073202	5.287526
4.142665	251.674544	5.292531
4.044251	256.963809	5.297536
4.189453	252.012259	5.302541
4.272153	254.261497	5.307546
4.202865	255.060121	5.312550
4.133282	246.168425	5.317555
4.145006	255.433111	5.322560
4.033949	250.027925	5.327565
4.213502	248.339114	5.332570
4.155732	247.734432	5.337574
4.377661	241.613030	5.342579
4.096356	246.642873	5.347584
3.882334	246.261832	5.352589
3.997034	250.053128	5.357594
4.198278	251.031090	5.362598
4.195049	256.789579	5.367603
4.204681	248.391738	5.372608
3.979409	249.306395	5.377613
4.411200	253.329890	5.382618
3.928805	255.945516	5.387622
4.250411	249.663062	5.392627
3.962687	253.823893	5.397632
4.076894	254.530675	5.402637
4.104233	258.054007	5.407642
4.114787	252.952581	5.412646
4.364311	246.472547	5.417651
4.023622	254.612049	5.422656
4.118668	248.447126	5.427661
4.451237	257.506839	5.432666
4.212157	257.550469	5.437670
4.172667	249.514608	5.442675
4.083791	244.510922	5.447680
3.988588	253.659381	5.452685
4.027986	251.698168	5.457690
3.945466	258.399127	5.462694
4.277615	246.236904	5.467699
4.128791	267.102518	5.472704
4.404673	273.232000	5.477709
5.069398	271.031058	5.482714
4.314055	268.655754	5.487718
4.350892	261.322998	5.492723
4.120090	265.800829	5.497728
4.449645	273.389904	5.502733
4.838245	275.338422	5.507738
4.698088	268.374898	5.512742
4.384400	259.135231	5.517747
4.055117	261.170210	5.522752
4.465530	272.394428	5.527757
4.672812	264.725090	5.532762
4.329530	275.693342	5.537766
4.732645	277.098609	5.542771
4.751217	275.238711	5.547776
4.158329	273.303176	5.552781
4.780645	271.099346	5.557786
4.574909	279.847421	5.562790
4.790195	278.017005	5.567795
5.196556	285.568818	5.572800
4.552203	273.685162	5.577805
4.361790	262.496450	5.582810
4.464394	266.704077	5.587814
4.506268	271.572880	5.592819
4.741114	282.454287	5.597824
4.694466	279.095462	5.602829
4.696223	283.021407	5.607834
4.591878	279.826587	5.612838
5.002154	278.905427	5.617843
4.819189	286.874857	5.622848
4.493342	274.109560	5.627853
5.260682	286.432960	5.632858
4.835501	291.134047	5.637862
4.874441	280.665736	5.642867
4.713794	275.698524	5.647872
4.446923	271.136987	5.652877
4.458978	275.887050	5.657882
4.796981	284.787746	5.662886
5.226787	272.436298	5.667891
4.992400	283.011121	5.672896
5.030739	279.955433	5.677901
4.887008	279.924107	5.682906
4.466382	283.441263	5.687910
4.767469	277.288541	5.692915
5.008536	278.513399	5.697920
5.179037	272.441121	5.702925
4.989660	277.383895	5.707930
5.055255	286.858506	5.712934
5.254798	271.749369	5.717939
5.194752	272.056184	5.722944
4.876329	271.643942	5.727949
4.820219	272.000762	5.732954
4.771349	278.870493	5.737958
5.069776	276.324793	5.742963
5.040898	274.908871	5.747968
5.354892	274.641768	5.752973
5.406365	276.804124	5.757978
4.972000	283.809805	5.762982
5.133229	275.932502	5.767987
5.198081	281.965131	5.772992
4.918867	282.597129	5.777997
4.970102	278.811785	5.783002
5.060846	281.037628	5.788006
4.875489	274.299434	5.793011
5.308957	284.181829	5.798016
4.998876	270.727558	5.803021
5.107182	283.450953	5.808026
5.054762	286.496337	5.813030
5.152983	277.410822	5.818035
4.994370	280.368337	5.823040
4.841483	286.656328	5.828045
4.778380	283.009005	5.833050
5.235846	301.012033	5.838054
5.604258	304.570854	5.843059
5.305201	313.618208	5.848064
5.369247	309.267725	5.853069
5.636868	302.152115	5.858074
5.310436	310.688048	5.863078
5.606878	301.619114	5.868083
5.384632	286.411124	5.873088
5.072288	275.339462	5.878093
5.354682	292.436451	5.883098
5.619548	299.826806	5.888102
5.438813	311.902375	5.893107
5.635044	313.485386	5.898112
4.991766	298.808003	5.903117
4.990933	308.340423	5.908122
5.249963	305.126985	5.913126
5.328236	299.524630	5.918131
5.584316	303.923501	5.923136
5.314285	305.895477	5.928141
5.647105	296.036285	5.933146
5.444903	303.496199	5.938150
5.458955	300.181703	5.943155
5.472278	298.537750	5.948160
5.335356	301.381162	5.953165
5.741865	294.073091	5.958170
5.282613	312.725051	5.963174
5.567296	304.898116	5.968179
5.913659	307.792831	5.973184
5.557501	308.525393	5.978189
5.467691	306.672875	5.983194
5.467939	290.057197	5.988198
5.511740	300.066708	5.993203
5.426079	314.547702	5.998208
5.794683	315.581866	6.003213
5.618730	322.164520	6.008218
5.640839	323.724024	6.013222
6.441125	312.789148	6.018227
5.601865	310.958406	6.023232
5.622169	307.775809	6.028237
5.815911	301.272804	6.033242
5.442266	309.351025	6.038246
5.807185	300.192338	6.043251
5.699260	303.512117	6.048256
5.435145	308.643702	6.053261
5.693855	303.500461	6.058266
5.714134	311.504695	6.063270
6.035010	305.187535	6.068275
5.906500	298.915034	6.073280
5.936755	303.890057	6.078285
6.002372	301.753917	6.083290
5.528588	306.203152	6.088294
5.719926	304.079075	6.093299
5.635795	298.150835	6.098304
5.211928	293.370131	6.103309
5.691138	295.301380	6.108314
5.629988	307.453237	6.113318
5.944872	307.122721	6.118323
5.587153	301.980545	6.123328
5.371839	305.465739	6.128333
6.007200	297.742391	6.133338
5.787101	300.301367	6.138342
6.139478	308.946742	6.143347
5.848519	303.079176	6.148352
5.660380	300.191622	6.153357
5.988779	293.177282	6.158362
5.625391	305.584999	6.163366
5.954244	301.092050	6.168371
6.073548	304.028444	6.173376
5.439911	304.763081	6.178381
5.829304	299.561530	6.183386
5.297330	288.024192	6.188390
5.874650	302.354496	6.193395
5.896053	310.896383	6.198400
5.397000	301.628608	6.203405
5.684633	290.473014	6.208410
5.542568	308.740233	6.213414
5.618460	307.472509	6.218419
5.638851	309.899131	6.223424
5.367141	310.729275	6.228429
5.574545	310.314254	6.233434
5.605674	305.187464	6.238438
5.460299	290.451548	6.243443
5.430955	303.462138	6.248448
5.430890	305.676814	6.253453
5.689616	296.645392	6.258458
5.591210	300.419260	6.263462
5.572509	300.925278	6.268467
5.669649	306.424552	6.273472
5.556173	303.069800	6.278477
5.757759	300.583466	6.283482
5.564770	306.966291	6.288486
5.860031	305.613793	6.293491
5.619232	304.594690	6.298496
5.564929	306.264163	6.303501
5.945324	298.067995	6.308506
5.563931	311.146058	6.313510
5.625995	301.335347	6.318515
5.492746	298.973911	6.323520
5.881770	310.144536	6.328525
5.837318	299.610106	6.333530
5.580318	302.291883	6.338534
5.717738	301.767539	6.343539
5.923356	310.065613	6.348544
5.786965	298.137653	6.353549
6.072725	300.579903	6.358554
5.635622	311.344490	6.363558
5.545972	299.532636	6.368563
5.693811	302.587971	6.373568
5.660102	294.769484	6.378573
5.780718	295.298103	6.383578
5.678635	302.141326	6.388582
5.590075	299.931117	6.393587
5.814156	298.077184	6.398592
5.567206	307.002529	6.403597
5.793602	304.157998	6.408602
5.685626	302.441184	6.413606
5.827755	303.422025	6.418611
5.787610	305.905527	6.423616
5.873217	309.198339	6.428621
5.837348	296.489115	6.433626
5.888287	306.146348	6.438630
5.671709	309.587447	6.443635
5.835718	310.931871	6.448640
5.584864	302.606197	6.453645
5.769877	295.354758	6.458650
5.208735	297.175909	6.463654
5.543941	301.176489	6.468659
5.539505	305.065439	6.473664
5.687817	307.816986	6.478669
5.519955	302.929983	6.483674
5.397809	309.418836	6.488678
5.484161	303.508342	6.493683
5.571834	305.022835	6.498688
5.780538	306.505830	6.503693
5.405895	305.656259	6.508698
5.490823	303.023576	6.513702
5.465383	301.584971	6.518707
5.397799	300.045363	6.523712
5.717074	303.997805	6.528717
5.376174	305.057015	6.533722
5.243833	312.661077	6.538726
6.059504	315.928805	6.543731
5.809930	312.968558	6.548736
5.408217	312.496517	6.553741
5.299240	306.141881	6.558746
5.681656	324.960197	6.563750
5.724000	332.957841	6.568755
5.821185	328.086510	6.573760
5.250120	327.049225	6.578765
5.897835	333.598553	6.583770
5.638144	339.520384	6.588774
5.744300	339.409023	6.593779
5.832414	338.114085	6.598784
5.719368	331.972041	6.603789
6.143586	327.802753	6.608794
5.811985	319.258693	6.613798
6.075271	310.318301	6.618803
5.882886	301.999343	6.623808
5.807070	301.289904	6.628813
5.660135	295.883962	6.633818
5.745007	307.285435	6.638822
5.894802	308.141699	6.643827
5.654334	313.098765	6.648832
5.590038	309.910358	6.653837
5.672197	300.178775	6.658842
5.666645	309.939716	6.663846
5.734867	314.159035	6.668851
5.596693	310.510740	6.673856
5.689963	304.472621	6.678861
5.733996	304.807524	6.683866
5.528181	303.216672	6.688870
5.872582	307.892853	6.693875
5.923305	299.346223	6.698880
5.328886	306.677383	6.703885
6.007164	306.720550	6.708890
5.540196	312.102016	6.713894
5.542937	298.209884	6.718899
5.672552	301.514825	6.723904
5.577186	298.995633	6.728909
5.754478	303.973073	6.733914
5.321002	316.695425	6.738918
5.736017	307.797848	6.743923
5.888670	307.220513	6.748928
5.274884	305.737472	6.753933
5.580213	302.453553	6.758938
5.832861	308.792304	6.763942
5.600705	302.267026	6.768947
5.362545	308.391135	6.773952
5.661871	308.547086	6.778957
5.864023	304.285831	6.783962
5.710509	312.896080	6.788966
5.769801	296.207930	6.793971
6.081093	308.200562	6.798976
5.666083	299.410075	6.803981
5.717114	303.100567	6.808986
5.892049	309.365999	6.813990
5.753580	312.301400	6.818995
5.787488	310.828245	6.824000
5.505889	310.445069	6.829005
5.632427	305.553356	6.834010
5.467673	300.874673	6.839014
5.388449	303.981180	6.844019
5.598842	308.940812	6.849024
5.362692	307.405302	6.854029
5.886761	309.364369	6.859034
5.567012	305.390011	6.864038
5.191236	303.809804	6.869043
5.507628	306.886352	6.874048
5.511762	306.699129	6.879053
5.610078	312.631648	6.884058
5.994790	322.145176	6.889062
6.243314	321.954703	6.894067
5.722875	308.121875	6.899072
5.969377	312.402019	6.904077
5.597860	304.228007	6.909082
5.467158	309.408422	6.914086
5.720382	296.173306	6.919091
5.562167	300.693627	6.924096
5.225393	311.066113	6.929101
5.839219	302.074311	6.934106
5.518144	310.175984	6.939110
5.663043	302.405614	6.944115
5.815490	307.595726	6.949120
5.519294	315.418286	6.954125
5.764654	313.842607	6.959130
5.632477	306.336834	6.964134
5.838583	308.089147	6.969139
6.085667	309.920500	6.974144
5.707716	310.545726	6.979149
5.833432	315.009188	6.984154
5.412737	320.373960	6.989158
5.798473	314.132118	6.994163
5.414014	306.570713	6.999168
5.600825	309.215029	7.004173
5.741797	303.729458	7.009178
5.689386	314.896051	7.014182
5.797582	316.059343	7.019187
5.816643	309.365237	7.024192
5.700016	309.744136	7.029197
5.617851	305.881481	7.034202
5.403599	306.171177	7.039206
5.183861	302.867771	7.044211
5.647520	311.913429	7.049216
5.178443	330.940254	7.054221
5.676243	328.034480	7.059226
5.827225	332.085896	7.064230
5.968108	339.628447	7.069235
5.606749	337.697984	7.074240
5.672559	338.817258	7.079245
5.647272	332.788098	7.084250
5.665168	340.419399	7.089254
5.615692	333.293037	7.094259
6.027110	338.015738	7.099264
5.731563	326.118867	7.104269
5.689910	306.773099	7.109274
5.098963	312.945809	7.114278
5.885466	320.574489	7.119283
5.935427	337.540034	7.124288
5.805331	320.305555	7.129293
5.724541	309.836886	7.134298
5.321152	314.218216	7.139302
5.456181	309.265070	7.144307
5.632939	324.948546	7.149312
5.563435	323.608548	7.154317
6.046266	327.083121	7.159322
6.204396	324.334636	7.164326
6.019011	313.581698	7.169331
5.458748	311.501877	7.174336
5.393919	311.306409	7.179341
4.991239	307.417728	7.184346
5.267790	322.063792	7.189350
5.425466	330.932477	7.194355
5.714531	335.332548	7.199360
5.535834	329.409530	7.204365
5.916038	330.805715	7.209370
5.468462	338.955569	7.214374
6.095710	340.177251	7.219379
6.167921	341.773247	7.224384
5.719627	335.509395	7.229389
5.944152	326.556048	7.234394
5.563492	329.171663	7.239398
5.657280	310.102191	7.244403
5.455724	325.053646	7.249408
5.244720	336.839721	7.254413
5.851856	326.877692	7.259418
5.550365	336.722689	7.264422
5.828599	331.082863	7.269427
5.675869	344.337317	7.274432
5.518968	345.586178	7.279437
5.820379	344.140972	7.284442
5.840623	342.363062	7.289446
5.793663	343.484075	7.294451
6.076436	343.547693	7.299456
5.413221	330.616587	7.304461
5.339862	324.990377	7.309466
5.667509	340.042944	7.314470
5.677845	327.880152	7.319475
5.709864	334.468395	7.324480
5.673856	339.172175	7.329485
5.890050	326.961513	7.334490
5.282657	337.322366	7.339494
5.441539	331.356279	7.344499
5.394965	328.279003	7.349504
5.601513	342.641759	7.354509
5.613719	326.312082	7.359514
5.862298	340.358249	7.364518
5.420139	334.248464	7.369523
6.012369	336.108337	7.374528
5.745328	339.380132	7.379533
6.039521	334.168083	7.384538
5.828268	335.311512	7.389542
5.751311	336.668146	7.394547
6.137636	334.605453	7.399552
5.969705	328.139767	7.404557
5.677328	310.974855	7.409562
5.478984	318.000748	7.414566
5.495271	319.640250	7.419571
5.188674	312.496983	7.424576
5.818058	328.720584	7.429581
5.746937	326.757588	7.434586
5.880565	342.384522	7.439590
5.509912	330.556288	7.444595
5.546829	324.561738	7.449600
5.420976	336.109931	7.454605
6.037876	331.467725	7.459610
5.259858	338.881267	7.464614
5.715803	332.941693	7.469619
5.677749	324.816990	7.474624
5.884353	341.853062	7.479629
6.047165	330.811787	7.484634
5.865554	324.291286	7.489638
5.431258	314.877383	7.494643
5.673757	326.520076	7.499648
5.525710	335.119994	7.504653
5.661859	333.710011	7.509658
6.115842	329.982170	7.514662
5.666061	323.051014	7.519667
5.478815	314.737577	7.524672
5.482057	313.550765	7.529677
5.865856	331.315361	7.534682
5.450876	327.178659	7.539686
5.737574	330.101649	7.544691
5.832530	330.972780	7.549696
5.694152	324.945412	7.554701
5.768426	311.921640	7.559706
5.607791	311.212752	7.564710
5.575979	321.234048	7.569715
5.543301	315.209208	7.574720
5.672553	327.594021	7.579725
5.853939	326.740134	7.584730
5.817323	325.164064	7.589734
5.773981	319.691367	7.594739
5.623948	305.917927	7.599744
5.430651	317.416499	7.604749
4.636797	318.596853	7.609754
5.545588	333.527296	7.614758
5.737819	337.970917	7.619763
5.860039	343.858596	7.624768
6.178764	343.555955	7.629773
5.717986	335.914673	7.634778
5.741128	334.553921	7.639782
5.794032	328.499934	7.644787
6.271250	330.776340	7.649792
5.766593	323.505720	7.654797
5.324789	311.546211	7.659802
5.308193	323.048912	7.664806
5.518725	334.797827	7.669811
5.816089	332.451597	7.674816
5.497141	341.441953	7.679821
5.765837	333.674440	7.684826
5.682269	339.685906	7.689830
5.480129	338.240009	7.694835
6.063906	329.591388	7.699840
5.659802	340.540676	7.704845
5.859076	333.897595	7.709850
5.862977	337.389792	7.714854
5.615947	329.126784	7.719859
5.295358	321.694632	7.724864
5.291455	324.090238	7.729869
5.276621	332.925673	7.734874
5.685668	338.531415	7.739878
5.856108	337.508392	7.744883
6.036092	328.321538	7.749888
5.553820	342.892778	7.754893
5.889391	334.814302	7.759898
5.749301	337.139366	7.764902
5.971695	333.517183	7.769907
6.144774	328.501160	7.774912
5.971230	319.983111	7.779917
5.709388	312.643053	7.784922
5.787449	314.962623	7.789926
5.565204	314.532241	7.794931
5.432764	309.266405	7.799936
5.304798	308.334135	7.804941
5.321955	304.376924	7.809946
5.487611	324.488138	7.814950
5.663512	331.604462	7.819955
5.979781	333.643340	7.824960
5.526603	335.862130	7.829965
5.848434	338.985292	7.834970
5.622346	337.887968	7.839974
5.501785	333.923719	7.844979
5.914490	331.145087	7.849984
5.721534	338.106875	7.854989
5.660017	335.569753	7.859994
5.900618	344.583720	7.864998
5.553660	332.701177	7.870003
5.373271	329.306219	7.875008
5.235231	333.956282	7.880013
5.393262	335.045379	7.885018
5.219929	342.814021	7.890022
5.431778	343.790336	7.895027
5.703419	342.982506	7.900032
5.414142	335.039280	7.905037
5.984785	333.381317	7.910042
5.366823	338.536367	7.915046
5.268626	339.750777	7.920051
5.880943	342.986898	7.925056
5.455513	340.686766	7.930061
5.486205	325.939226	7.935066
5.421279	345.001215	7.940070
5.536454	344.844159	7.945075
6.006592	356.568487	7.950080
5.847138	353.711258	7.955085
6.110614	338.823062	7.960090
5.954515	344.678146	7.965094
6.105786	343.009548	7.970099
6.102585	333.506368	7.975104
5.864404	339.029388	7.980109
5.760132	338.685039	7.985114
5.765745	337.684515	7.990118
5.933447	341.415314	7.995136
5.816104	333.995843	8.000154
5.929388	346.013858	8.005171
5.952907	321.995938	8.010189
5.710790	315.662504	8.015206
5.563880	317.171756	8.020224
6.074719	323.050123	8.025242
6.011156	322.154433	8.030259
5.794690	310.023277	8.035277
5.722978	311.965764	8.040294
5.702648	311.129613	8.045312
5.640569	301.069760	8.050330
5.473372	314.100200	8.055347
5.615697	306.274259	8.060365
5.818921	316.586836	8.065382
5.581120	312.515316	8.070400
5.373522	311.490583	8.075418
5.198382	320.965875	8.080435
5.571863	330.235840	8.085453
5.849683	335.134378	8.090470
5.831846	345.973669	8.095488
5.659964	329.490254	8.100506
5.918517	337.459064	8.105523
5.938668	337.269824	8.110541
6.179003	340.015749	8.115558
5.620638	335.299895	8.120576
5.663436	328.272037	8.125594
5.826272	342.021085	8.130611
5.834158	331.966100	8.135629
5.926148	334.656231	8.140646
5.335755	340.800730	8.145664
5.724266	341.803767	8.150682
5.298235	348.443358	8.155699
5.822468	340.349668	8.160717
5.593665	339.432371	8.165734
5.520919	343.871126	8.170752
5.873766	341.642039	8.175770
5.593649	342.515662	8.180787
5.794632	341.499892	8.185805
5.933737	348.234519	8.190822
5.499406	356.304906	8.195840
6.096916	350.992538	8.200858
5.890891	365.834083	8.205875
6.189337	353.622727	8.210893
5.770645	346.865519	8.215910
5.603905	341.460718	8.220928
6.417528	349.791210	8.225946
5.755830	354.122861	8.230963
5.693165	336.476940	8.235981
6.072822	340.659075	8.240998
5.893850	347.115040	8.246016
6.104062	354.346655	8.251034
6.131149	344.771485	8.256051
5.990844	338.838734	8.261069
6.199845	344.221335	8.266086
5.931116	341.331673	8.271104
6.088561	338.517661	8.276122
5.694467	341.315031	8.281139
6.050974	340.738924	8.286157
5.978843	336.682627	8.291174
5.906206	346.672119	8.296192
6.239193	342.502255	8.301210
6.169545	344.804166	8.306227
6.185067	335.713613	8.311245
6.022521	344.994464	8.316262
6.172101	342.102785	8.321280
6.058051	329.378190	8.326298
6.389164	341.775674	8.331315
6.233064	341.796902	8.336333
5.724866	337.584449	8.341350
5.771639	343.115377	8.346368
6.058342	338.794938	8.351386
6.099499	347.867359	8.356403
5.537798	341.277578	8.361421
6.086865	335.218562	8.366438
5.766782	345.095109	8.371456
6.301780	328.719375	8.376474
6.174997	339.111747	8.381491
5.934333	339.272366	8.386509
5.800476	332.407703	8.391526
5.831549	334.302633	8.396544
5.912599	346.480292	8.401562
6.523020	358.932126	8.406579
6.046817	350.760680	8.411597
5.901325	343.238297	8.416614
6.266601	351.827934	8.421632
5.725216	347.548066	8.426650
5.860408	365.526828	8.431667
6.168214	361.941516	8.436685
6.433206	358.741547	8.441702
6.061390	352.658655	8.446720
6.385910	350.683272	8.451738
6.174361	359.482637	8.456755
6.356952	364.702107	8.461773
6.636441	363.913941	8.466790
6.222404	342.930415	8.471808
5.971165	339.671977	8.476826
5.610675	349.179298	8.481843
6.463371	355.847003	8.486861
6.326166	355.249941	8.491878
6.330791	362.825976	8.496896
6.087955	355.366079	8.501914
5.919436	360.996800	8.506931
6.196967	355.579625	8.511949
6.040792	358.955303	8.516966
5.864024	367.411603	8.521984
6.127820	359.554104	8.527002
6.349701	365.452229	8.532019
6.181032	366.254856	8.537037
6.114489	356.366072	8.542054
6.022824	358.904930	8.547072
6.141271	360.167754	8.552090
6.175514	352.945569	8.557107
6.196081	357.265663	8.562125
6.264769	360.413837	8.567143
6.245392	351.473869	8.572160
6.623547	353.321072	8.577178
6.145056	364.894780	8.582195
6.249570	367.747059	8.587213
6.307594	357.826257	8.592231
6.356983	362.826637	8.597248
6.548567	365.226726	8.602266
6.539812	367.089992	8.607283
6.121784	355.798030	8.612301
6.523749	355.104398	8.617319
6.387097	365.791796	8.622336
6.482138	353.621577	8.627354
6.619867	354.562680	8.632371
6.407335	366.180181	8.637389
6.304544	361.702641	8.642407
6.553982	361.626016	8.647424
6.737516	357.267990	8.652442
6.420364	354.231240	8.657459
6.554954	369.783418	8.662477
6.666815	369.904929	8.667495
6.316692	367.009002	8.672512
6.639988	360.858904	8.677530
5.533773	357.364371	8.682547
5.944448	361.039935	8.687565
6.103561	349.762254	8.692583
6.066096	365.890297	8.697600
6.097605	362.426895	8.702618
6.177688	365.216709	8.707635
5.966937	368.787068	8.712653
6.616055	369.859978	8.717671
6.293685	383.028231	8.722688
6.484877	386.425565	8.727706
6.632399	397.690397	8.732723
6.513570	388.330417	8.737741
6.872177	380.565439	8.742759
6.337006	365.347163	8.747776
6.530572	361.861685	8.752794
6.788056	369.407820	8.757811
6.349106	362.571714	8.762829
6.281788	360.852986	8.767847
6.293606	376.048765	8.772864
6.731593	382.572777	8.777882
6.639535	387.178643	8.782899
6.562717	374.123188	8.787917
6.393579	366.251045	8.792935
6.875476	377.034638	8.797952
6.413851	372.392070	8.802970
6.501642	367.029678	8.807987
6.468771	377.814527	8.813005
6.798455	381.322835	8.818023
6.389402	377.287429	8.823040
6.619512	378.479224	8.828058
6.807028	378.121921	8.833075
6.726119	376.026632	8.838093
6.716204	365.254915	8.843111
6.364291	362.520205	8.848128
6.357880	366.317511	8.853146
6.764415	373.789951	8.858163
6.669754	383.603022	8.863181
6.684267	375.462453	8.868199
6.381772	372.593822	8.873216
6.716923	383.539114	8.878234
6.541512	382.872264	8.883251
6.698375	395.322160	8.888269
6.907033	399.041809	8.893287
6.388908	386.692494	8.898304
6.793269	388.043341	8.903322
6.962548	391.472489	8.908339
6.684852	381.307314	8.913357
6.636530	378.771473	8.918375
6.168008	377.456020	8.923392
6.097073	392.371222	8.928410
6.642316	401.226337	8.933427
6.292646	398.065261	8.938445
6.592248	382.048004	8.943463
6.511303	398.397430	8.948480
6.983972	397.942083	8.953498
6.988270	398.266524	8.958515
6.659719	401.577535	8.963533
6.902932	391.732017	8.968551
6.788047	400.118740	8.973568
6.654358	396.977683	8.978586
6.968162	390.797496	8.983603
6.640499	393.401503	8.988621
6.755017	389.489693	8.993639
6.654358	390.789790	8.998656
6.406789	395.571341	9.003674
6.835550	395.337415	9.008691
6.887031	405.553755	9.013709
6.968977	390.731654	9.018727
6.649318	396.553168	9.023744
6.959779	400.907029	9.028762
6.879658	404.072068	9.033779
6.774261	407.796436	9.038797
7.395897	386.926148	9.043815
6.633950	389.219095	9.048832
7.141424	390.721137	9.053850
6.498788	394.525994	9.058867
6.463448	404.907322	9.063885
6.855859	399.822523	9.068903
6.543785	396.456788	9.073920
6.713328	392.520632	9.078938
6.739930	398.872029	9.083955
6.938838	407.989343	9.088973
7.328268	402.460062	9.093991
6.691112	397.437739	9.099008
6.797923	399.541779	9.104026
6.968672	399.603631	9.109043
7.084859	395.773606	9.114061
6.956303	393.688890	9.119079
6.902111	401.397169	9.124096
6.604574	392.670893	9.129114
7.093447	399.328993	9.134131
6.808527	418.351466	9.139149
7.150092	410.917315	9.144167
7.043260	411.530444	9.149184
7.084096	408.854492	9.154202
7.201341	388.381454	9.159219
6.820417	393.887475	9.164237
6.820910	390.501476	9.169255
6.887340	396.455371	9.174272
6.772768	410.840925	9.179290
7.500187	408.282124	9.184307
6.980380	405.917513	9.189325
7.180578	400.064263	9.194343
7.266537	395.162872	9.199360
7.108520	392.820824	9.204378
7.245298	389.896419	9.209395
6.858310	395.782062	9.214413
7.119820	390.575643	9.219431
7.165297	396.349773	9.224448
7.117707	389.998648	9.229466
7.188589	387.690386	9.234483
7.049686	389.422448	9.239501
6.891347	388.790807	9.244519
6.840154	396.056828	9.249536
6.829448	397.762620	9.254554
7.283037	412.820223	9.259571
6.829237	414.957904	9.264589
7.189045	417.824088	9.269607
7.741561	416.627356	9.274624
7.360485	410.473306	9.279642
6.930757	398.649834	9.284659
7.038505	404.433206	9.289677
6.776678	389.876058	9.294695
7.405722	399.267207	9.299712
6.956119	411.170944	9.304730
7.056487	412.061066	9.309747
6.804067	422.056502	9.314765
6.995363	421.190551	9.319783
7.678579	416.243498	9.324800
7.029307	423.700474	9.329818
7.178126	412.717830	9.334835
7.379313	426.038116	9.339853
7.172106	418.673626	9.344871
7.316316	420.326899	9.349888
7.137178	422.838362	9.354906
7.560298	418.935299	9.359923
7.733850	414.247470	9.364941
7.413056	407.168899	9.369959
7.062908	400.688162	9.374976
6.870464	400.330060	9.379994
7.519190	409.882243	9.385011
7.207239	418.018805	9.390029
7.069535	415.001439	9.395047
7.280362	415.236923	9.400064
7.299025	419.734045	9.405082
7.549642	419.865509	9.410099
7.588464	421.857066	9.415117
7.079003	416.319420	9.420135
7.184533	406.457463	9.425152
7.270885	414.014484	9.430170
7.737472	410.129901	9.435187
7.670834	420.083788	9.440205
7.713655	403.396471	9.445223
7.119414	390.307962	9.450240
7.123576	397.527497	9.455258
7.148071	394.847780	9.460275
7.266951	400.373810	9.465293
7.890408	405.988530	9.470311
7.907620	397.790729	9.475328
7.185324	400.465648	9.480346
6.927200	399.436153	9.485363
7.155659	399.444841	9.490381
7.490039	410.440760	9.495399
7.459903	418.318862	9.500416
7.294587	429.291613	9.505434
7.639501	422.424952	9.510451
7.693509	418.614070	9.515469
7.668923	419.025056	9.520487
7.551109	400.368385	9.525504
7.325042	393.549611	9.530522
7.054102	391.020029	9.535539
7.195714	414.747416	9.540557
7.585432	419.963054	9.545575
7.734018	427.393633	9.550592
7.364987	426.204689	9.555610
7.148946	418.775305	9.560627
7.475819	424.701282	9.565645
7.607539	427.407330	9.570663
7.361665	419.184213	9.575680
7.014342	427.562960	9.580698
7.689340	418.969260	9.585715
7.289419	424.014368	9.590733
7.351592	429.511369	9.595751
7.436894	412.890009	9.600768
7.246522	427.615565	9.605786
7.484575	418.692284	9.610803
7.416746	416.500284	9.615821
7.428384	423.936405	9.620839
7.749053	432.659253	9.625856
7.453661	449.764757	9.630874
7.883425	440.477118	9.635891
7.777439	440.679882	9.640909
7.521835	436.106201	9.645927
7.548391	424.388387	9.650944
7.220247	442.051221	9.655962
7.839747	444.043885	9.660979
7.876071	441.204537	9.665997
8.249001	447.312689	9.671015
7.850526	436.005009	9.676032
7.127239	426.773833	9.681050
7.617682	429.654392	9.686067
7.795924	424.773336	9.691085
7.529667	428.046252	9.696103
8.017196	438.466105	9.701120
7.712379	437.033645	9.706138
7.916090	425.651147	9.711155
7.914651	427.623728	9.716173
7.126522	428.652187	9.721191
7.773005	425.601082	9.726208
7.693638	438.154058	9.731226
7.940035	434.120724	9.736243
7.724261	424.018464	9.741261
7.621659	429.203465	9.746279
7.928194	433.292870	9.751296
7.739402	441.012657	9.756314
7.428150	451.809337	9.761331
8.050839	441.014815	9.766349
8.037019	430.789594	9.771367
7.958527	430.909186	9.776384
7.687561	423.942764	9.781402
7.614658	422.499442	9.786419
8.202494	429.924745	9.791437
7.709575	430.181441	9.796455
7.822489	426.061601	9.801472
7.976617	434.371744	9.806490
7.773919	427.173797	9.811507
7.687998	432.110062	9.816525
7.749637	434.401010	9.821543
8.314531	428.961161	9.826560
7.804645	433.240793	9.831578
8.203395	439.411192	9.836595
7.918223	429.237686	9.841613
7.684576	427.964551	9.846631
7.912224	425.322622	9.851648
7.771200	433.217995	9.856666
8.072455	439.321527	9.861683
8.109834	436.295831	9.866701
7.950717	435.724267	9.871719
7.870522	435.405489	9.876736
7.785986	436.504273	9.881754
7.427980	438.901583	9.886771
7.978466	446.250661	9.891789
7.655229	452.388315	9.896807
8.035569	447.308538	9.901824
7.554399	447.995730	9.906842
8.149874	437.366386	9.911859
8.017933	435.853363	9.916877
7.962097	439.156631	9.921895
7.848450	435.239313	9.926912
8.040668	440.861229	9.931930
7.735071	432.016274	9.936947
7.663098	447.512324	9.941965
7.813385	446.412927	9.946983
8.308174	440.605312	9.952000
8.015956	440.250121	9.957018
8.089196	448.396149	9.962035
7.868322	440.162818	9.967053
8.475693	463.426453	9.972071
8.101233	454.718435	9.977088
8.059724	447.315511	9.982106
7.984810	452.669769	9.987123
8.154493	453.798397	9.992141
7.895347	473.612140	9.997159
8.269788	469.006624	10.002176
8.302754	471.816413	10.007194
8.501024	470.677988	10.012211
8.318762	453.798462	10.017229
7.715101	454.419522	10.022247
8.397974	462.126673	10.027264
8.316111	460.227173	10.032282
8.426189	447.253013	10.037299
8.431423	451.048524	10.042317
7.659419	451.869355	10.047335
8.249261	439.259139	10.052352
8.044417	449.171448	10.057370
8.046499	452.860157	10.062387
8.606265	464.941274	10.067405
8.052738	459.293716	10.072423
8.075032	459.091518	10.077440
8.228320	478.269880	10.082458
8.441007	478.205287	10.087475
8.486936	460.857902	10.092493
7.785374	466.925083	10.097511
8.258254	468.400962	10.102528
8.351073	473.281008	10.107546
8.473941	470.191506	10.112563
8.881183	471.557690	10.117581
8.111864	464.227053	10.122599
7.973669	460.695384	10.127616
8.333539	471.987160	10.132634
8.608806	473.241355	10.137651
8.451130	469.999882	10.142669
8.269012	475.907299	10.147687
8.787154	469.969812	10.152704
8.487927	459.489224	10.157722
8.194061	453.671857	10.162739
8.374113	442.394013	10.167757
7.840980	444.458847	10.172775
8.625326	457.521111	10.177792
8.508442	466.485661	10.182810
8.424980	472.699594	10.187827
9.294501	465.183219	10.192845
8.441839	461.311532	10.197863
8.619326	445.979073	10.202880
8.340210	447.193355	10.207898
8.071719	450.018521	10.212915
8.589109	446.438429	10.217933
8.151757	453.916068	10.222951
7.971304	456.494008	10.227968
8.159665	477.522431	10.232986
8.317814	473.089438	10.238003
8.445301	475.502677	10.243021
8.282824	476.310656	10.248039
8.727551	476.411898	10.253056
8.844455	480.123759	10.258074
8.748429	480.700496	10.263091
8.952604	471.384851	10.268109
8.403893	479.391054	10.273127
8.702945	471.316588	10.278144
8.644208	479.994394	10.283162
8.424835	482.218654	10.288179
8.607950	470.583726	10.293197
8.405911	474.029679	10.298215
8.394382	472.254920	10.303232
8.791227	472.836965	10.308250
8.667537	473.834555	10.313267
8.735529	474.530915	10.318285
8.411819	475.417643	10.323303
8.899965	476.701806	10.328320
8.615346	474.821250	10.333338
8.395925	478.850551	10.338355
8.717637	470.961896	10.343373
8.877565	472.372897	10.348391
8.688849	466.264614	10.353408
8.657310	474.811957	10.358426
8.567722	481.740024	10.363443
8.612188	480.351003	10.368461
8.554739	472.354132	10.373479
8.390510	474.314197	10.378496
8.744753	478.487698	10.383514
8.303827	473.886060	10.388531
8.490815	476.936944	10.393549
8.598084	481.972525	10.398567
8.739411	469.738218	10.403584
9.231727	474.650734	10.408602
8.621500	472.587356	10.413619
8.535936	472.537644	10.418637
8.840742	474.531974	10.423655
8.849291	482.378835	10.428672
8.782462	479.681768	10.433690
8.825830	478.993473	10.438707
9.192445	479.147900	10.443725
8.830595	474.486615	10.448743
8.572312	470.995731	10.453760
9.043150	469.082757	10.458778
9.184163	479.910019	10.463795
8.727381	476.894988	10.468813
8.882105	468.846149	10.473831
8.974047	470.993536	10.478848
8.816582	478.866243	10.483866
8.710994	479.340332	10.488883
8.837270	473.280828	10.493901
8.917929	486.029818	10.498919
9.077066	481.546178	10.503936
8.994345	479.012523	10.508954
8.872798	480.852340	10.513971
8.615745	477.250815	10.518989
9.047618	489.175145	10.524007
8.831204	501.503361	10.529024
9.306588	499.687501	10.534042
8.913291	494.895413	10.539059
9.056639	484.601511	10.544077
8.820622	499.602463	10.549095
8.799503	501.196283	10.554112
9.163529	495.633060	10.559130
8.728546	499.440320	10.564147
9.158454	493.929954	10.569165
8.922367	503.515813	10.574183
8.916346	495.851735	10.579200
9.225457	493.083510	10.584218
9.143350	499.363509	10.589235
9.168636	510.057337	10.594253
9.295506	498.109271	10.599271
8.786008	504.171806	10.604288
9.396537	493.991344	10.609306
8.852928	493.287147	10.614323
9.038713	492.336848	10.619341
9.253910	504.133984	10.624359
9.112809	499.788601	10.629376
9.588122	492.346214	10.634394
9.386040	500.150142	10.639411
9.217470	502.246579	10.644429
9.462727	502.205317	10.649447
9.048130	489.167656	10.654464
9.254165	483.395518	10.659482
8.972164	494.651552	10.664499
9.235329	492.976026	10.669517
9.096271	497.365187	10.674535
9.539348	496.283314	10.679552
9.519269	491.098619	10.684570
8.856369	489.052907	10.689587
9.139604	490.608805	10.694605
9.328539	501.305549	10.699623
9.127293	496.114347	10.704640
9.436210	499.076826	10.709658
8.985864	493.441593	10.714675
9.059205	500.104470	10.719693
9.331028	498.206700	10.724711
9.153988	496.946836	10.729728
9.861109	496.761083	10.734746
9.445190	499.394625	10.739763
9.429303	493.729616	10.744781
9.375812	495.975385	10.749799
9.481264	500.373811	10.754816
9.353710	497.989138	10.759834
9.073797	502.078353	10.764851
9.245449	495.424824	10.769869
9.286704	498.747699	10.774887
9.584233	497.780002	10.779904
9.572090	494.881922	10.784922
9.624578	500.522457	10.789939
9.582468	496.884308	10.794957
9.452093	499.072623	10.799975
9.157103	497.209458	10.804992
9.268427	494.563541	10.810010
9.067490	504.563630	10.815027
9.411522	503.525579	10.820045
9.569440	506.394811	10.825063
9.463972	502.567718	10.830080
9.329157	493.983307	10.835098
9.710585	498.909939	10.840115
9.481547	501.874130	10.845133
9.446852	499.642249	10.850151
9.112719	508.126273	10.855168
9.821849	497.725339	10.860186
9.366066	501.895582	10.865203
9.747403	502.091897	10.870221
9.311386	503.049758	10.875239
9.116318	510.499165	10.880256
9.033284	492.569096	10.885274
9.473149	511.797544	10.890291
9.819955	515.041293	10.895309
9.873089	511.697565	10.900327
9.352665	505.000315	10.905344
9.426504	501.479805	10.910362
9.754064	520.567965	10.915379
9.648663	517.674934	10.920397
9.661340	517.265959	10.925415
9.592155	521.628468	10.930432
9.695230	517.535384	10.935450
9.619168	536.721116	10.940467
9.537959	524.754939	10.945485
9.643779	531.406459	10.950503
9.778615	532.370112	10.955520
10.382813	531.439869	10.960538
10.032163	522.321029	10.965555
9.599522	512.893083	10.970573
9.098113	506.836626	10.975591
9.578965	518.226354	10.980608
9.825741	513.867911	10.985626
9.591238	525.410045	10.990643
9.456962	519.378470	10.995661
9.802498	532.212478	11.000679
9.511744	521.235095	11.005696
9.753325	523.633732	11.010714
9.709006	518.430713	11.015731
9.773905	531.936393	11.020749
9.844696	526.393571	11.025767
9.852468	530.239194	11.030784
10.220922	515.612212	11.035802
9.996097	525.316245	11.040819
9.466508	532.246569	11.045837
9.784460	528.249409	11.050855
9.809744	526.128101	11.055872
10.016856	524.827357	11.060890
9.962316	519.127335	11.065907
10.035714	526.531793	11.070925
10.074867	522.950410	11.075943
9.906671	525.791528	11.080960
10.146090	524.397396	11.085978
9.660603	524.308969	11.090995
10.017125	511.750807	11.096013
10.286179	520.093588	11.101031
10.049838	522.494055	11.106048
9.830096	523.528693	11.111066
9.632166	524.096051	11.116083
10.118344	522.486782	11.121101
9.699621	518.979846	11.126119
9.684128	520.216201	11.131136
9.980466	520.564599	11.136154
10.343497	514.859521	11.141171
9.760235	524.022940	11.146189
9.792628	532.251102	11.151207
9.509302	539.745819	11.156224
10.289614	538.245381	11.161242
10.610129	535.746761	11.166259
10.416732	533.230330	11.171277
10.445104	532.408674	11.176295
10.159249	526.372296	11.181312
10.299518	515.188958	11.186330
10.215327	529.696104	11.191347
10.140127	514.043183	11.196365
10.275500	507.950694	11.201383
9.814578	509.792863	11.206400
9.920566	518.672248	11.211418
10.380559	524.997236	11.216435
10.317197	524.764194	11.221453
10.501139	532.416520	11.226471
10.343611	522.040059	11.231488
9.956533	519.762059	11.236506
9.908608	520.489091	11.241523
10.117467	530.434858	11.246541
10.642577	527.661398	11.251559
10.157363	526.383244	11.256576
10.205889	520.720820	11.261594
10.544960	524.480148	11.266611
10.163880	532.851578	11.271629
10.050210	520.003716	11.276647
10.400194	536.974109	11.281664
10.151179	535.880075	11.286682
10.370881	543.369054	11.291699
10.386485	539.668263	11.296717
10.736925	534.365909	11.301735
10.594999	540.428029	11.306752
10.438872	528.530315	11.311770
10.141470	525.080224	11.316787
10.469329	527.976646	11.321805
10.034596	534.052796	11.326823
10.012453	544.318547	11.331840
10.341428	531.950844	11.336858
10.173036	535.612467	11.341875
10.437341	538.070681	11.346893
10.820577	539.172377	11.351911
10.621547	539.373850	11.356928
10.458806	535.792342	11.361946
9.924124	531.542942	11.366963
10.127392	545.405768	11.371981
10.816540	530.324917	11.376999
10.435815	534.139515	11.382016
10.349836	536.627022	11.387034
10.792200	540.180930	11.392051
10.903698	538.898228	11.397069
10.476232	530.226826	11.402087
10.462686	539.105899	11.407104
10.563472	535.959866	11.412122
10.600990	536.288605	11.417139
10.424401	538.824932	11.422157
10.356989	535.582016	11.427175
10.428097	543.507523	11.432192
10.673774	535.365602	11.437210
10.743246	530.113306	11.442227
10.529880	533.349605	11.447245
10.576057	520.205468	11.452263
10.375606	530.300166	11.457280
10.616253	528.161105	11.462298
10.375283	531.057734	11.467315
10.140000	554.200233	11.472333
10.600088	550.935142	11.477351
10.645934	557.895799	11.482368
10.378709	560.320014	11.487386
10.926565	550.086165	11.492403
10.435597	558.178083	11.497421
10.755403	552.397676	11.502439
10.274054	563.470205	11.507456
11.059093	557.008317	11.512474
10.962589	555.120553	11.517491
10.619310	556.253318	11.522509
11.386489	553.893426	11.527527
10.918054	564.560020	11.532544
10.968396	565.947067	11.537562
10.734043	555.181778	11.542579
10.733658	564.446962	11.547597
10.982685	564.133725	11.552615
11.071228	558.768003	11.557632
11.254325	559.992375	11.562650
10.544120	564.738710	11.567667
11.061068	566.756823	11.572685
11.040749	551.366712	11.577703
10.854288	565.741493	11.582720
10.919041	570.780564	11.587738
11.030669	563.681938	11.592755
10.929570	566.070822	11.597773
11.299266	561.781587	11.602791
11.116691	558.982613	11.607808
10.787539	563.480278	11.612826
11.071803	560.633864	11.617843
11.011715	562.612436	11.622861
11.314243	565.326624	11.627879
11.001193	567.316181	11.632896
11.031008	560.833028	11.637914
10.803345	561.897302	11.642931
10.764551	561.026145	11.647949
10.896550	552.497990	11.652967
10.939934	564.381875	11.657984
10.961199	567.733120	11.663002
10.989390	567.062964	11.668019
10.991247	576.542390	11.673037
10.949968	567.182864	11.678055
11.079808	565.534402	11.683072
11.070218	566.075594	11.688090
11.181361	557.598018	11.693107
10.673916	564.458638	11.698125
10.540096	558.367021	11.703143
10.932626	572.714775	11.708160
11.016183	585.012123	11.713178
11.262346	577.182519	11.718195
11.248854	584.673111	11.723213
11.598170	573.715954	11.728231
11.538024	577.733101	11.733248
11.526195	581.256752	11.738266
11.868211	570.799330	11.743283
11.151984	567.928814	11.748301
11.477891	565.120095	11.753319
11.178139	557.605860	11.758336
10.534087	557.378027	11.763354
11.258692	566.457753	11.768371
11.277673	575.874555	11.773389
11.756097	578.457221	11.778407
11.117372	579.323576	11.783424
11.445332	583.302388	11.788442
11.588168	581.727636	11.793459
11.034434	580.965054	11.798477
11.154044	572.858522	11.803495
11.381030	577.105507	11.808512
11.454173	583.736890	11.813530
11.388324	579.505997	11.818547
11.662458	584.102234	11.823565
11.597778	585.008595	11.828583
11.467836	580.775058	11.833600
11.517506	587.138708	11.838618
11.500281	569.835761	11.843635
11.034374	575.017412	11.848653
11.427476	576.900181	11.853671
11.394983	589.704730	11.858688
11.710431	586.449530	11.863706
11.436065	580.076843	11.868723
11.902887	584.501074	11.873741
11.839307	579.149564	11.878759
11.709477	578.750153	11.883776
11.664855	573.297867	11.888794
11.581630	562.370194	11.893811
11.408588	563.151420	11.898829
11.499540	556.172777	11.903847
11.881601	568.174339	11.908864
11.710389	567.431092	11.913882
11.808252	559.021853	11.918899
11.095000	559.603177	11.923917
11.353054	570.506942	11.928935
11.552320	574.859224	11.933952
11.687048	578.606199	11.938970
11.774973	577.466014	11.943987
11.440440	580.973640	11.949005
11.701141	586.584940	11.954023
11.726680	583.526351	11.959040
11.630767	584.087295	11.964058
11.640595	582.113548	11.969075
11.521017	576.379454	11.974093
11.832279	586.195704	11.979111
11.863102	584.534256	11.984128
11.845525	589.725000	11.989146
11.412096	582.935283	11.994163
11.379751	596.938970	11.999181
11.598237	588.274261	12.004199
11.647673	583.141829	12.009216
11.728939	603.013164	12.014234
12.208955	593.228491	12.019251
11.451921	593.561023	12.024269
12.165914	603.361915	12.029287
11.836740	602.987229	12.034304
11.650309	602.558762	12.039322
11.720851	597.303124	12.044339
12.101987	606.455281	12.049357
12.271527	606.381629	12.054375
12.222048	600.172728	12.059392
12.014317	582.309319	12.064410
11.896505	580.734126	12.069427
11.714753	590.816480	12.074445
12.089228	595.772622	12.079463
12.036350	606.832114	12.084480
11.882920	605.776840	12.089498
12.026387	609.989501	12.094515
12.292010	607.467861	12.099533
12.277200	597.725516	12.104551
11.968081	594.842101	12.109568
12.062325	581.706213	12.114586
12.045394	581.333403	12.119603
11.935313	584.380068	12.124621
11.863731	598.023807	12.129639
12.258859	599.060542	12.134656
11.522031	596.584532	12.139674
12.267966	610.227223	12.144691
11.814556	603.658351	12.149709
12.083139	615.298933	12.154727
11.993037	606.802177	12.159744
11.932411	613.700540	12.164762
12.488734	605.128384	12.169779
12.292533	608.642879	12.174797
12.254988	608.904413	12.179815
12.145984	615.778753	12.184832
12.034904	608.430774	12.189850
12.277636	603.407090	12.194867
11.744491	612.950900	12.199885
12.091870	613.774172	12.204903
12.180359	613.429128	12.209920
11.731425	615.427224	12.214938
12.422059	623.877978	12.219955
12.158365	629.062873	12.224973
12.335323	636.798378	12.229991
12.313234	638.622726	12.235008
12.671018	640.643539	12.240026
12.548584	635.493672	12.245043
12.624859	638.000110	12.250061
12.680756	629.559503	12.255079
12.328287	614.243142	12.260096
12.457380	605.971024	12.265114
12.492914	608.133521	12.270131
12.811409	616.304554	12.275149
12.492572	615.764163	12.280167
12.808571	602.650536	12.285184
12.200484	611.454962	12.290202
12.361376	613.080411	12.295219
12.621318	614.444295	12.300237
12.227548	609.516555	12.305255
12.387240	608.627115	12.310272
12.140442	614.203835	12.315290
12.666534	613.323617	12.320307
12.689449	625.554699	12.325325
12.650684	628.684938	12.330343
12.769579	616.454023	12.335360
12.242584	617.754245	12.340378
12.490566	620.177145	12.345395
12.382239	634.669199	12.350413
12.224500	641.377574	12.355431
12.768595	636.325895	12.360448
12.349214	646.726134	12.365466
12.602196	634.234498	12.370483
12.539986	643.875408	12.375501
12.593631	645.066295	12.380519
12.816225	635.880235	12.385536
12.798157	645.687836	12.390554
12.786634	637.702674	12.395571
12.788963	636.626302	12.400589
12.724649	639.792078	12.405607
13.055369	627.360924	12.410624
12.616072	640.418188	12.415642
12.350435	634.318667	12.420659
12.746442	638.943278	12.425677
11.931765	634.702735	12.430695
12.885827	651.058497	12.435712
13.038606	656.304784	12.440730
12.988428	642.948349	12.445747
12.674262	642.893205	12.450765
12.850584	640.792548	12.455783
12.904852	636.252617	12.460800
12.784585	641.935872	12.465818
13.061524	644.130213	12.470835
12.696260	649.703299	12.475853
12.797317	659.902599	12.480871
13.012866	659.039173	12.485888
13.025999	666.049144	12.490906
13.472111	658.917337	12.495923
12.890057	647.912649	12.500941
12.845197	640.371316	12.505959
12.976131	647.646951	12.510976
13.029383	664.152445	12.515994
13.238698	651.828535	12.521011
13.196946	645.548991	12.526029
13.265263	647.949376	12.531047
13.111643	636.161649	12.536064
12.740788	630.908456	12.541082
12.941814	635.803256	12.546099
13.323732	645.747389	12.551117
12.749942	652.612061	12.556135
13.417513	659.980867	12.561152
13.253234	665.238653	12.566170
13.179334	658.519157	12.571187
13.357360	655.361077	12.576205
12.954859	646.101930	12.581223
13.135444	651.072498	12.586240
13.560229	659.886540	12.591258
13.321174	645.701164	12.596275
12.902194	648.035414	12.601293
12.896086	650.371651	12.606311
13.212458	648.050379	12.611328
13.202094	656.976351	12.616346
13.291757	662.617461	12.621363
13.294275	653.257382	12.626381
13.168907	653.545213	12.631399
13.451346	664.183317	12.636416
13.509044	666.455976	12.641434
12.913562	665.002482	12.646451
13.564520	659.233595	12.651469
12.681205	656.597355	12.656487
13.221304	662.105219	12.661504
13.080830	662.909780	12.666522
13.546231	665.055847	12.671539
13.492569	660.804103	12.676557
13.175402	662.261000	12.681575
13.522748	661.446478	12.686592
13.390715	661.391378	12.691610
13.351158	664.395519	12.696627
13.404216	662.702200	12.701645
13.441328	663.204567	12.706663
13.616168	665.777711	12.711680
13.398378	675.720562	12.716698
13.947790	688.242084	12.721715
13.775581	666.415823	12.726733
13.097421	663.883334	12.731751
13.936687	667.350226	12.736768
13.437876	671.457783	12.741786
13.365766	666.072862	12.746803
13.808102	668.415017	12.751821
13.325251	685.041868	12.756839
13.694689	681.917095	12.761856
13.739472	687.161272	12.766874
13.632523	685.650648	12.771891
13.694642	682.497987	12.776909
13.595444	685.142201	12.781927
13.948470	672.540291	12.786944
13.897090	684.663065	12.791962
13.356655	678.013044	12.796979
13.842757	675.504402	12.801997
13.643010	676.920929	12.807015
13.471063	682.558597	12.812032
13.554549	688.803414	12.817050
13.573330	692.852478	12.822067
13.909565	683.494071	12.827085
13.920494	690.214072	12.832103
13.828717	682.288720	12.837120
14.399213	675.718187	12.842138
14.056039	686.886040	12.847155
13.974273	673.465076	12.852173
14.015340	681.439501	12.857191
13.911000	684.324348	12.862208
14.070961	681.405754	12.867226
13.753109	685.513540	12.872243
14.294472	684.438444	12.877261
13.807300	686.202669	12.882279
13.532971	682.742643	12.887296
14.186928	689.356215	12.892314
13.649181	688.865683	12.897331
14.040755	685.696439	12.902349
14.110783	691.511023	12.907367
13.778440	685.929936	12.912384
14.119253	682.585566	12.917402
14.267067	691.142957	12.922419
14.280471	685.220871	12.927437
14.166871	692.310543	12.932455
14.571417	679.650115	12.937472
14.135627	683.123036	12.942490
13.917306	686.861888	12.947507
14.214351	681.536247	12.952525
14.124449	691.225674	12.957543
14.373311	684.414892	12.962560
14.290831	695.924000	12.967578
14.241870	692.097535	12.972595
14.235284	685.134027	12.977613
14.051345	685.058607	12.982631
14.092749	684.452659	12.987648
13.909469	683.913249	12.992666
13.731343	688.235958	12.997683
14.281657	680.583008	13.002701
14.206747	681.437320	13.007719
14.088125	687.035130	13.012736
14.569391	685.871564	13.017754
14.139763	694.540952	13.022771
14.302542	686.626456	13.027789
14.264810	688.544760	13.032807
14.162177	685.023288	13.037824
14.231623	690.506614	13.042842
14.038487	693.654588	13.047859
14.541357	704.832732	13.052877
14.544651	719.556777	13.057895
14.673646	714.049015	13.062912
14.451938	708.324468	13.067930
14.303990	710.401940	13.072947
14.752444	708.631277	13.077965
14.185736	710.512025	13.082983
14.051082	713.347950	13.088000
14.434217	715.948629	13.093018
14.327369	711.670441	13.098035
14.702120	709.033970	13.103053
15.107645	718.561072	13.108071
15.112764	714.252827	13.113088
14.973671	705.457549	13.118106
14.524197	702.753754	13.123123
14.817876	686.427888	13.128141
14.568021	694.693758	13.133159
14.431151	690.211974	13.138176
14.542477	693.549222	13.143194
14.497229	700.028673	13.148211
14.554553	704.545093	13.153229
14.704602	710.770087	13.158247
14.695115	705.122948	13.163264
15.092466	703.861997	13.168282
14.827497	706.677187	13.173299
15.095849	705.325871	13.178317
14.354578	690.776855	13.183335
14.535795	695.980858	13.188352
14.611705	700.500694	13.193370
14.466428	707.065148	13.198387
14.835483	702.788602	13.203405
14.551980	707.418047	13.208423
14.692830	704.051159	13.213440
14.992107	703.663827	13.218458
15.021524	712.504740	13.223475
14.895446	706.307729	13.228493
14.352734	702.283592	13.233511
14.839172	704.237046	13.238528
14.862119	699.099238	13.243546
14.646197	715.984348	13.248563
14.945543	721.226769	13.253581
15.466336	738.224407	13.258599
14.963038	723.310120	13.263616
15.411823	701.011601	13.268634
14.832697	711.058066	13.273651
14.942892	696.360696	13.278669
14.972045	714.703447	13.283687
14.839914	722.749037	13.288704
15.147546	722.745399	13.293722
14.796428	727.363286	13.298739
15.110250	730.574341	13.303757
15.010775	735.907263	13.308775
14.887868	736.614421	13.313792
15.085121	731.966999	13.318810
15.216149	735.212827	13.323827
15.141359	738.604306	13.328845
15.232827	726.964546	13.333863
15.177543	732.792342	13.338880
15.274773	729.924530	13.343898
15.039300	730.791221	13.348915
15.218833	733.167990	13.353933
15.291536	741.752879	13.358951
15.537708	740.537553	13.363968
15.274706	730.016452	13.368986
15.231256	740.591736	13.374003
15.458475	730.492910	13.379021
15.487894	730.999632	13.384039
15.292993	724.642922	13.389056
15.402450	722.959750	13.394074
15.092805	727.741588	13.399091
15.365937	729.437932	13.404109
15.705675	730.600059	13.409127
15.246540	740.378558	13.414144
15.617126	726.205492	13.419162
15.120322	728.640229	13.424179
15.603438	729.764255	13.429197
15.548587	727.033727	13.434215
15.361519	724.667757	13.439232
15.481325	718.523973	13.444250
15.402653	734.592496	13.449267
15.726758	745.656493	13.454285
15.718684	725.432946	13.459303
15.186070	731.546492	13.464320
15.223431	733.472042	13.469338
15.603874	744.025510	13.474355
15.538480	747.213563	13.479373
16.043822	750.035053	13.484391
16.029112	748.424858	13.489408
15.983614	744.935503	13.494426
15.633741	742.146769	13.499443
15.497922	735.774544	13.504461
15.906975	747.222934	13.509479
16.028218	749.741321	13.514496
16.132961	730.140811	13.519514
15.942588	733.954215	13.524531
15.586680	728.282113	13.529549
15.401460	724.568371	13.534567
15.660887	741.284825	13.539584
15.662815	740.795470	13.544602
15.514978	751.194516	13.549619
15.850845	749.630720	13.554637
16.094014	753.569125	13.559655
15.951748	756.030713	13.564672
16.182109	753.965808	13.569690
15.623676	748.047531	13.574707
15.910168	745.885528	13.579725
15.938430	754.045010	13.584743
15.876021	762.373242	13.589760
15.968224	754.390812	13.594778
16.080478	756.727569	13.599795
16.076500	755.017876	13.604813
16.057990	751.820954	13.609831
15.966132	761.573838	13.614848
16.305911	756.459265	13.619866
16.137358	758.937569	13.624883
15.972470	758.572013	13.629901
16.500261	755.596137	13.634919
15.876044	757.754079	13.639936
16.269475	751.946366	13.644954
16.149449	756.932210	13.649971
16.342677	752.859748	13.654989
16.536283	754.227660	13.660007
16.103347	758.179817	13.665024
15.965083	753.919133	13.670042
16.268023	761.594054	13.675059
15.994834	757.982362	13.680077
16.109429	749.870219	13.685095
16.021538	760.875299	13.690112
16.239413	762.204721	13.695130
15.982107	761.866177	13.700147
16.031091	762.552884	13.705165
16.136537	755.433055	13.710183
15.951922	773.370507	13.715200
16.377889	775.560595	13.720218
16.219555	775.118281	13.725235
16.523106	776.443832	13.730253
16.588479	775.546979	13.735271
16.746901	784.468825	13.740288
16.895177	775.227994	13.745306
16.517915	768.031842	13.750323
16.234761	763.841050	13.755341
16.746261	761.615611	13.760359
16.580949	764.232263	13.765376
16.568712	755.325693	13.770394
16.671819	749.891376	13.775411
16.595851	755.640352	13.780429
16.791476	753.397825	13.785447
16.850670	755.884849	13.790464
16.911703	754.480605	13.795482
16.506126	749.220159	13.800499
16.165126	750.690242	13.805517
16.649764	750.270893	13.810535
16.909534	760.107880	13.815552
16.604478	760.833931	13.820570
16.752281	764.503173	13.825587
16.111180	762.397231	13.830605
16.648834	766.403394	13.835623
16.817495	780.912400	13.840640
16.522428	774.908928	13.845658
16.669148	786.937814	13.850675
16.706447	782.365775	13.855693
16.900010	769.078590	13.860711
16.571985	779.849679	13.865728
16.665100	777.522126	13.870746
17.001382	773.209643	13.875763
16.793873	777.751536	13.880781
17.165123	788.962849	13.885799
16.937700	779.919362	13.890816
16.740906	773.928992	13.895834
16.924847	779.243045	13.900851
16.985324	781.089264	13.905869
17.382640	777.130183	13.910887
16.665008	787.927225	13.915904
16.819557	780.452612	13.920922
17.183304	777.401291	13.925939
16.580608	783.087122	13.930957
16.903763	776.611865	13.935975
16.966509	780.329066	13.940992
17.202760	785.073261	13.946010
17.333582	787.025290	13.951027
16.980580	787.926060	13.956045
17.034484	783.259920	13.961063
17.491200	793.394455	13.966080
17.420726	785.588814	13.971098
17.429890	787.080116	13.976115
17.164001	775.275064	13.981133
17.346585	774.331560	13.986151
17.041556	777.140376	13.991168
17.297117	760.571076	13.996186
16.970187	771.288342	14.001203
17.349381	786.054898	14.006221
17.484729	796.687582	14.011239
17.280384	793.617413	14.016256
17.454842	797.604394	14.021274
17.520681	791.289112	14.026291
17.026468	791.309335	14.031309
17.387513	795.582836	14.036327
17.133697	798.090200	14.041344
17.201432	797.596909	14.046362
17.110092	801.827240	14.051379
17.249511	801.966554	14.056397
17.506374	802.450488	14.061415
17.632654	800.666863	14.066432
17.727964	801.213820	14.071450
17.234133	798.333885	14.076467
17.233676	790.435291	14.081485
17.454525	787.314701	14.086503
17.624355	805.256957	14.091520
17.648036	796.300594	14.096538
17.983413	791.237188	14.101555
17.501366	798.330621	14.106573
17.931184	787.483872	14.111591
17.319969	791.189247	14.116608
17.128335	796.028466	14.121626
17.998451	801.071594	14.126643
17.748766	812.619433	14.131661
17.371292	800.718132	14.136679
17.740053	809.433677	14.141696
17.934558	818.192137	14.146714
18.040147	819.333923	14.151731
17.925926	824.243146	14.156749
17.858917	803.312339	14.161767
17.996548	796.559856	14.166784
17.596880	792.084250	14.171802
17.819910	800.838260	14.176819
17.669819	815.529462	14.181837
17.936803	809.018759	14.186855
18.145261	817.219640	14.191872
18.236825	815.646541	14.196890
17.889196	814.984397	14.201907
17.954101	815.665472	14.206925
18.284114	812.998082	14.211943
17.767551	809.856605	14.216960
17.564711	812.109888	14.221978
18.171680	815.726584	14.226995
17.748337	821.851549	14.232013
17.962772	812.329007	14.237031
17.944552	812.824214	14.242048
18.103880	816.946095	14.247066
18.308279	815.320715	14.252083
18.189065	819.533300	14.257101
18.406274	819.420668	14.262119
18.098324	818.237965	14.267136
18.116356	819.513301	14.272154
18.049271	818.816945	14.277171
18.267582	821.840922	14.282189
18.334371	820.035000	14.287207
18.128008	820.786712	14.292224
18.311855	829.070323	14.297242
18.296222	809.008800	14.302259
18.306671	819.465289	14.307277
18.315871	815.329950	14.312295
18.397415	820.334919	14.317312
18.370170	820.291905	14.322330
18.536507	817.233444	14.327347
18.435188	820.269317	14.332365
18.399308	819.549168	14.337383
18.363842	818.213590	14.342400
18.165831	826.190591	14.347418
17.890241	822.462498	14.352435
18.431690	836.194004	14.357453
18.860665	834.943899	14.362471
18.783499	842.229924	14.367488
18.754664	832.120416	14.372506
18.855027	837.946103	14.377523
18.158805	832.405846	14.382541
18.680522	833.044199	14.387559
18.961435	830.084659	14.392576
18.461199	823.554552	14.397594
18.693598	828.744314	14.402611
18.859739	841.461315	14.407629
19.137309	823.395875	14.412647
18.603032	819.143186	14.417664
18.348943	814.073723	14.422682
18.877285	818.554705	14.427699
18.952226	822.879069	14.432717
19.217483	826.662577	14.437735
18.798349	820.306032	14.442752
18.572594	808.990156	14.447770
19.413865	810.203586	14.452787
18.558786	817.061625	14.457805
18.705177	806.464114	14.462823
18.828862	819.058325	14.467840
19.088474	823.877786	14.472858
19.515228	818.951619	14.477875
19.159200	814.573351	14.482893
19.040183	800.444899	14.487911
18.719285	799.305237	14.492928
18.671597	794.639133	14.497946
19.005484	808.156789	14.502963
19.200289	814.822962	14.507981
19.566649	812.534911	14.512999
19.016842	810.711386	14.518016
18.782964	800.898899	14.523034
18.829151	792.226204	14.528051
18.962810	813.929397	14.533069
19.240129	821.791364	14.538087
19.267861	821.613562	14.543104
18.880884	823.797688	14.548122
19.235256	822.836902	14.553139
19.345707	821.734219	14.558157
19.279462	821.921332	14.563175
18.994508	822.388643	14.568192
18.845988	820.903414	14.573210
19.559521	825.055771	14.578227
19.106717	826.641094	14.583245
19.342903	822.120128	14.588263
19.535472	819.799175	14.593280
19.334879	830.373734	14.598298
19.238637	823.894333	14.603315
19.266240	828.674180	14.608333
19.514697	822.257873	14.613351
19.531287	824.066750	14.618368
19.264376	827.118939	14.623386
19.524698	823.253759	14.628403
19.336508	825.047184	14.633421
19.225933	834.626302	14.638439
19.568976	843.721399	14.643456
19.427126	847.268503	14.648474
19.679943	845.594557	14.653491
20.005067	849.933622	14.658509
19.546505	849.998786	14.663527
19.547840	841.935793	14.668544
19.508752	841.863065	14.673562
19.767032	834.605803	14.678579
19.751268	846.211915	14.683597
19.918177	853.762892	14.688615
20.168528	843.133395	14.693632
19.787233	836.300751	14.698650
19.910908	847.635852	14.703667
19.602952	840.264782	14.708685
19.955446	842.851316	14.713703
19.953230	844.240257	14.718720
19.763527	848.416488	14.723738
19.833046	844.997566	14.728755
19.959393	846.928208	14.733773
20.134195	842.754455	14.738791
19.927048	841.010117	14.743808
20.118220	843.407179	14.748826
19.722072	836.368570	14.753843
19.838325	842.037154	14.758861
19.874596	846.358077	14.763879
19.918539	838.329476	14.768896
19.877200	843.397765	14.773914
20.035789	836.610447	14.778931
19.755076	838.636023	14.783949
19.847993	837.561314	14.788967
19.969180	841.266273	14.793984
19.664712	847.218108	14.799002
19.644161	856.647525	14.804019
20.210727	875.490577	14.809037
20.021060	880.023407	14.814055
20.259031	873.858017	14.819072
20.504777	876.925068	14.824090
20.476898	877.295552	14.829107
20.486128	879.935536	14.834125
20.146897	881.272813	14.839143
20.326018	874.870438	14.844160
20.303930	884.596747	14.849178
19.960080	861.840784	14.854195
20.671073	861.679673	14.859213
20.521578	874.534201	14.864231
20.629023	860.856424	14.869248
20.410651	873.655405	14.874266
20.766019	866.436660	14.879283
20.286701	868.698284	14.884301
20.547362	875.054433	14.889319
20.586192	875.540759	14.894336
20.307684	868.881442	14.899354
20.744456	871.915595	14.904371
20.569708	870.109406	14.909389
20.563071	873.932101	14.914407
20.656047	866.971955	14.919424
20.427034	869.860465	14.924442
20.597076	870.506238	14.929459
20.744919	870.682109	14.934477
20.724459	865.399537	14.939495
21.091541	862.101535	14.944512
20.337813	875.839071	14.949530
20.408466	867.803143	14.954547
20.814963	870.920902	14.959565
20.756998	877.194120	14.964583
21.097202	864.837061	14.969600
20.393240	871.769420	14.974618
20.900226	876.029685	14.979635
21.386554	875.244006	14.984653
20.934740	879.969126	14.989671
21.628596	859.393148	14.994688
20.959096	866.834522	14.999706
20.978335	866.762179	15.004723
21.064314	866.745716	15.009741
20.651218	870.953579	15.014759
20.813861	871.654151	15.019776
20.959877	871.211785	15.024794
21.053258	866.006159	15.029811
20.804541	871.766290	15.034829
21.238087	885.312669	15.039847
21.083596	890.209244	15.044864
21.371101	896.507574	15.049882
20.873579	889.238580	15.054899
21.526849	891.506899	15.059917
21.389585	887.375412	15.064935
21.256560	877.755459	15.069952
21.237037	895.597903	15.074970
21.378339	882.792130	15.079987
21.475877	887.005697	15.085005
21.693363	893.396976	15.090023
21.236233	872.217566	15.095040
21.133961	879.504360	15.100058
21.542780	885.461913	15.105075
21.338957	879.415798	15.110093
21.477445	877.579773	15.115111
21.738928	888.704100	15.120128
21.504339	876.461773	15.125146
21.252788	881.692186	15.130163
21.587673	882.324918	15.135181
21.420856	881.962815	15.140199
21.562923	887.494854	15.145216
21.349284	893.176949	15.150234
21.673343	884.483036	15.155251
21.773049	891.624781	15.160269
21.646651	893.749410	15.165287
21.876858	890.725173	15.170304
21.713940	893.672822	15.175322
21.892583	887.800679	15.180339
21.897717	885.174394	15.185357
21.451778	891.179827	15.190375
21.687101	880.697811	15.195392
21.672121	896.292672	15.200410
21.750935	894.582698	15.205427
22.028491	880.398749	15.210445
21.921830	894.540470	15.215463
21.739612	881.393758	15.220480
21.876471	892.001018	15.225498
21.651051	887.700224	15.230515
21.772085	881.458366	15.235533
21.852121	872.818230	15.240551
21.648912	882.850442	15.245568
21.941344	884.849902	15.250586
21.998012	880.000274	15.255603
21.839307	883.710951	15.260621
21.933248	883.368208	15.265639
21.953072	878.495916	15.270656
21.736338	887.160651	15.275674
22.128226	901.770697	15.280691
22.399283	902.082015	15.285709
22.429394	915.946844	15.290727
22.665852	901.917596	15.295744
22.387486	894.541897	15.300762
22.204283	888.704001	15.305779
22.028636	881.429076	15.310797
21.942096	884.601512	15.315815
22.168341	889.927946	15.320832
22.700701	893.871848	15.325850
22.547041	897.960430	15.330867
22.250546	883.682823	15.335885
22.252909	903.049239	15.340903
22.644180	899.665416	15.345920
22.590029	904.719938	15.350938
22.187534	887.931092	15.355955
22.395758	891.909681	15.360973
22.184040	911.479847	15.365991
22.235981	901.556534	15.371008
22.616967	911.264281	15.376026
22.237411	907.568136	15.381043
22.128710	903.567894	15.386061
22.055320	916.760889	15.391079
22.223889	903.903520	15.396096
22.405455	909.066507	15.401114
22.725457	928.358249	15.406131
23.174653	913.819353	15.411149
23.128079	922.094704	15.416167
22.615914	906.926027	15.421184
22.746860	908.849649	15.426202
22.769941	920.323532	15.431219
22.870664	911.973640	15.436237
22.770827	917.593844	15.441255
23.284171	906.159675	15.446272
23.353721	902.040165	15.451290
22.698627	896.682827	15.456307
22.976483	893.865760	15.461325
22.839122	894.199643	15.466343
22.824154	887.975801	15.471360
22.780737	893.782868	15.476378
23.071886	910.743845	15.481395
23.625130	913.094011	15.486413
23.031103	912.299817	15.491431
23.267341	901.060271	15.496448
23.126322	892.684912	15.501466
22.839074	888.116040	15.506483
23.121762	898.069453	15.511501
23.063292	917.315971	15.516519
23.006631	915.425121	15.521536
23.090574	923.115275	15.526554
23.290284	915.280133	15.531571
23.724171	919.182569	15.536589
23.359254	924.875604	15.541607
23.517356	916.500997	15.546624
23.527684	900.922780	15.551642
22.833100	900.403013	15.556659
23.488142	909.181330	15.561677
23.156157	922.723853	15.566695
23.487854	919.696432	15.571712
22.924217	922.435083	15.576730
23.283779	924.143235	15.581747
23.385483	918.958388	15.586765
23.221986	930.969401	15.591783
23.446953	921.760734	15.596800
23.258858	918.441866	15.601818
23.001648	930.499026	15.606835
23.757158	931.277705	15.611853
23.536114	941.508382	15.616871
23.677590	946.731269	15.621888
23.770700	938.865378	15.626906
23.838538	946.289811	15.631923
23.966152	949.750801	15.636941
23.582516	929.209962	15.641959
23.834294	931.976289	15.646976
23.654876	935.658645	15.651994
23.458846	940.943546	15.657011
23.977278	935.788483	15.662029
24.336679	955.342358	15.667047
23.835540	940.976650	15.672064
23.902338	943.216369	15.677082
24.089660	945.629824	15.682099
24.194034	941.517506	15.687117
24.235224	935.789822	15.692135
23.909625	922.668559	15.697152
23.681659	927.302036	15.702170
23.718458	936.552157	15.707187
24.062223	936.738549	15.712205
24.111531	943.619924	15.717223
24.043802	946.344483	15.722240
24.024715	942.589050	15.727258
23.897388	942.937150	15.732275
24.139050	940.081531	15.737293
23.827277	934.989457	15.742311
23.925224	942.235636	15.747328
24.135364	934.692345	15.752346
24.199957	944.121175	15.757363
24.562428	934.887937	15.762381
23.800332	945.464783	15.767399
24.428241	948.904681	15.772416
24.787003	955.636897	15.777434
24.385789	950.590302	15.782451
24.373017	943.179541	15.787469
24.353424	952.615172	15.792487
24.447019	960.445847	15.797504
24.696654	964.720957	15.802522
24.402982	953.980440	15.807539
24.854399	950.817611	15.812557
24.212746	956.597923	15.817575
24.642129	961.179554	15.822592
24.921586	959.226900	15.827610
24.637845	970.713874	15.832627
24.772806	960.124363	15.837645
24.568919	975.139647	15.842663
24.873146	968.301202	15.847680
24.931188	970.106796	15.852698
24.658870	959.173607	15.857715
24.729979	951.724537	15.862733
24.788780	962.694279	15.867751
24.650257	960.434326	15.872768
24.916835	963.513927	15.877786
25.212434	973.506397	15.882803
24.980622	960.828086	15.887821
24.936847	957.736044	15.892839
24.607990	945.786051	15.897856
24.796788	948.880915	15.902874
24.411242	966.130337	15.907891
24.759721	958.174185	15.912909
24.461675	961.306982	15.917927
24.351490	966.471230	15.922944
25.123609	971.431838	15.927962
24.631368	980.502424	15.932979
25.235405	974.857505	15.937997
25.041841	979.267892	15.943015
25.087853	983.126594	15.948032
25.545620	988.846192	15.953050
25.814689	987.160235	15.958067
25.743553	990.074676	15.963085
25.396756	962.083662	15.968103
25.241587	968.757047	15.973120
25.278235	963.140512	15.978138
25.240344	985.883617	15.983155
25.684142	978.733109	15.988173
25.544588	971.484084	15.993191
24.792699	971.039508	15.998208
25.441160	975.044245	16.003226
25.473808	982.556222	16.008243
25.558938	972.703439	16.013261
25.260214	984.669271	16.018279
25.400874	985.758272	16.023296
25.791586	983.718868	16.028314
25.480052	977.929325	16.033331
25.611104	976.226989	16.038349
25.526333	987.821847	16.043367
25.395420	993.203921	16.048384
26.064852	981.338311	16.053402
25.254393	986.497987	16.058419
25.965172	976.976972	16.063437
25.723701	975.282145	16.068455
25.203930	981.936564	16.073472
26.540056	987.879160	16.078490
26.154624	988.226422	16.083507
26.255454	987.570186	16.088525
26.230588	976.784647	16.093543
25.828336	977.229201	16.098560
26.165320	973.465659	16.103578
26.079919	972.860509	16.108595
26.211104	980.079438	16.113613
26.128744	974.459339	16.118631
25.893745	975.846664	16.123648
25.800939	976.590170	16.128666
25.421733	986.280620	16.133683
25.723875	985.110212	16.138701
25.909609	993.267376	16.143719
26.092561	1001.219854	16.148736
26.449777	996.307621	16.153754
26.238344	1006.754587	16.158771
25.736790	1006.457222	16.163789
26.267895	1000.110451	16.168807
25.842649	999.536122	16.173824
26.373870	986.549647	16.178842
26.364076	997.754149	16.183859
26.241087	993.696152	16.188877
26.565594	987.113314	16.193895
26.632073	994.051994	16.198912
26.464049	988.615638	16.203930
26.904842	997.096004	16.208947
26.308378	995.387019	16.213965
26.216132	999.068438	16.218983
26.618989	993.682049	16.224000
27.171736	994.908858	16.229018
26.321760	1004.738886	16.234035
26.322345	1005.868632	16.239053
26.823947	1011.098584	16.244071
26.774667	1024.783358	16.249088
27.022895	1014.999830	16.254106
26.643150	1005.465557	16.259123
27.039907	1002.879265	16.264141
27.189652	989.005458	16.269159
26.423868	993.902565	16.274176
26.703001	986.619904	16.279194
26.849299	1011.903141	16.284211
27.049566	1016.208040	16.289229
27.129344	1016.848938	16.294247
27.191802	1017.300033	16.299264
27.329794	996.807287	16.304282
27.212434	991.530296	16.309299
27.016128	990.096673	16.314317
26.869485	986.768183	16.319335
27.034135	986.670044	16.324352
27.462091	989.418417	16.329370
27.093659	992.726278	16.334387
26.844024	996.460603	16.339405
27.577994	996.974400	16.344423
27.382645	995.550095	16.349440
27.403565	992.545802	16.354458
27.244456	993.422705	16.359475
27.187449	991.364646	16.364493
27.695393	992.677325	16.369511
27.571007	994.830055	16.374528
27.492979	974.774903	16.379546
26.954238	987.096836	16.384563
27.165838	1002.280979	16.389581
27.374042	1009.087148	16.394599
27.009953	1013.110691	16.399616
27.485045	1015.599270	16.404634
27.350273	1018.012391	16.409651
27.476392	1016.563279	16.414669
27.515450	1008.904584	16.419687
26.956883	1012.803775	16.424704
27.521355	1018.999067	16.429722
27.170451	1027.845703	16.434739
27.875687	1030.705543	16.439757
27.683645	1027.579770	16.444775
27.660690	1033.696116	16.449792
27.846199	1036.965075	16.454810
27.903473	1033.472285	16.459827
27.934691	1030.595768	16.464845
28.087288	1027.043958	16.469863
27.684440	1040.209446	16.474880
27.784381	1033.428028	16.479898
27.908033	1032.427416	16.484915
27.959615	1034.975625	16.489933
27.994983	1030.851939	16.494951
27.543341	1032.850502	16.499968
28.122853	1032.473180	16.504986
27.984375	1032.254983	16.510003
28.112983	1054.246428	16.515021
28.539634	1046.148681	16.520039
28.288276	1039.223144	16.525056
27.985924	1029.165576	16.530074
28.088111	1030.926434	16.535091
27.988117	1038.777818	16.540109
28.493820	1042.653321	16.545127
28.651750	1056.211185	16.550144
28.395420	1047.692762	16.555162
28.492456	1043.303857	16.560179
28.890778	1031.183783	16.565197
28.578446	1032.750408	16.570215
28.522623	1029.606582	16.575232
28.734857	1023.656582	16.580250
28.893526	1017.150045	16.585267
28.653323	1023.382262	16.590285
28.852686	1022.234165	16.595303
28.275016	1015.189033	16.600320
28.622646	1020.695420	16.605338
28.317524	1027.499469	16.610355
28.382280	1024.639822	16.615373
28.798890	1018.250912	16.620391
28.500628	1031.845071	16.625408
28.683673	1039.403082	16.630426
29.034038	1045.638030	16.635443
29.001448	1049.231278	16.640461
29.242102	1036.226892	16.645479
28.898555	1029.924773	16.650496
28.898913	1024.029851	16.655514
28.718124	1024.035988	16.660531
28.860513	1039.619096	16.665549
29.109317	1042.149222	16.670567
28.885489	1044.475228	16.675584
29.092645	1041.845868	16.680602
29.299362	1042.441757	16.685619
29.236846	1041.788861	16.690637
29.220338	1043.129551	16.695655
28.949371	1045.936260	16.700672
28.794220	1046.585335	16.705690
29.134635	1046.655487	16.710707
28.680090	1045.053787	16.715725
29.278115	1041.842870	16.720743
29.208638	1045.710099	16.725760
29.427196	1045.060778	16.730778
29.161017	1045.768164	16.735795
28.951556	1051.623225	16.740813
29.385430	1064.125134	16.745831
29.373164	1075.358471	16.750848
29.860319	1063.773647	16.755866
29.845769	1064.403988	16.760883
29.717094	1063.168109	16.765901
29.566158	1045.771910	16.770919
29.824100	1053.744294	16.775936
29.339300	1057.524713	16.780954
29.817607	1051.242948	16.785971
29.795023	1074.353006	16.790989
29.755225	1063.516092	16.796007
29.577955	1065.456161	16.801024
29.861296	1068.356449	16.806042
29.814515	1069.348409	16.811059
29.817765	1067.498707	16.816077
30.090851	1057.790180	16.821095
30.173701	1063.612356	16.826112
29.971478	1058.408518	16.831130
30.228066	1059.476318	16.836147
29.968061	1064.285230	16.841165
30.017679	1051.960662	16.846183
30.168754	1052.950217	16.851200
29.928297	1063.748868	16.856218
30.066594	1061.663549	16.861235
29.973970	1068.021124	16.866253
29.982922	1074.637438	16.871271
29.936684	1070.270833	16.876288
29.884579	1063.323732	16.881306
29.959460	1059.872376	16.886323
29.823591	1062.979941	16.891341
30.062959	1061.522660	16.896359
29.660804	1073.722403	16.901376
29.923121	1087.046290	16.906394
30.427661	1083.856233	16.911411
30.399583	1088.253505	16.916429
30.239541	1085.009132	16.921447
30.469864	1085.617127	16.926464
30.380436	1081.522327	16.931482
30.645726	1085.485764	16.936499
30.657190	1086.007915	16.941517
30.646087	1075.472635	16.946535
30.469048	1082.291476	16.951552
30.446232	1089.196760	16.956570
31.271261	1073.639867	16.961587
30.424514	1086.379048	16.966605
30.271008	1081.599957	16.971623
30.720453	1090.527139	16.976640
30.721542	1103.468838	16.981658
31.297186	1104.221882	16.986675
31.023207	1110.055449	16.991693
31.035530	1085.571188	16.996711
30.782170	1086.702608	17.001728
31.254048	1094.143090	17.006746
31.096361	1086.612823	17.011763
31.037073	1089.544370	17.016781
30.992543	1093.726457	17.021799
31.287330	1095.318481	17.026816
31.138135	1098.368167	17.031834
31.258305	1089.806883	17.036851
31.142410	1095.271855	17.041869
31.328212	1100.311163	17.046887
31.285053	1096.196534	17.051904
31.411609	1103.280535	17.056922
31.528288	1104.477418	17.061939
31.234715	1093.515897	17.066957
31.654213	1088.414064	17.071975
31.083510	1085.151579	17.076992
31.355467	1086.251702	17.082010
31.893046	1090.491478	17.087027
31.646231	1098.189024	17.092045
31.508865	1089.333327	17.097063
31.832414	1081.904858	17.102080
31.293146	1087.991159	17.107098
31.459246	1090.770851	17.112115
31.582555	1093.879093	17.117133
31.940610	1090.727620	17.122151
31.777805	1091.936459	17.127168
31.763628	1094.173026	17.132186
31.738809	1095.256241	17.137203
31.427052	1094.594812	17.142221
31.925614	1093.538980	17.147239
31.618021	1094.379047	17.152256
31.750641	1093.821998	17.157274
32.047498	1095.549397	17.162291
31.832964	1098.726020	17.167309
31.973733	1091.698386	17.172327
32.070092	1093.154048	17.177344
31.568729	1098.852603	17.182362
32.004836	1091.302466	17.187379
31.690049	1098.837028	17.192397
31.986773	1103.180578	17.197415
31.734164	1106.442025	17.202432
31.957130	1121.981102	17.207450
32.361467	1117.503307	17.212467
32.401527	1118.740522	17.217485
32.647209	1109.361278	17.222503
32.224489	1116.313057	17.227520
32.366980	1122.296378	17.232538
32.832922	1118.111945	17.237555
32.677502	1120.361039	17.242573
33.011312	1122.543430	17.247591
32.633980	1111.793753	17.252608
32.642655	1124.519695	17.257626
32.692976	1111.642716	17.262643
32.544778	1104.578018	17.267661
32.311343	1109.231328	17.272679
32.583299	1105.421079	17.277696
32.263162	1118.741003	17.282714
32.959354	1114.940440	17.287731
32.766682	1122.465467	17.292749
32.628039	1115.093167	17.297767
32.683125	1119.180856	17.302784
32.460878	1116.842401	17.307802
32.607951	1114.089842	17.312819
32.069733	1115.720046	17.317837
32.586657	1125.592937	17.322855
33.032232	1136.287975	17.327872
33.013410	1139.266877	17.332890
32.970498	1136.367172	17.337907
32.635008	1129.322157	17.342925
32.841860	1134.998819	17.347943
33.006569	1135.222560	17.352960
32.813455	1141.920852	17.357978
33.331117	1138.996982	17.362995
33.374985	1143.301016	17.368013
33.500112	1151.537117	17.373031
33.662143	1146.645766	17.378048
33.174581	1144.178203	17.383066
33.355054	1131.249389	17.388083
33.136969	1143.874952	17.393101
33.637129	1148.606557	17.398119
33.696336	1150.222641	17.403136
33.364680	1143.413706	17.408154
33.532934	1148.512565	17.413171
33.591906	1157.437459	17.418189
34.004273	1162.760244	17.423207
33.644235	1149.682044	17.428224
33.651494	1149.002502	17.433242
33.755307	1154.139797	17.438259
34.238486	1158.435395	17.443277
33.890622	1151.777302	17.448295
33.853128	1135.262749	17.453312
33.256293	1132.114776	17.458330
33.412508	1141.848179	17.463347
34.062368	1154.225006	17.468365
33.946162	1149.411688	17.473383
34.233706	1150.540945	17.478400
34.189673	1150.096605	17.483418
34.517569	1139.966093	17.488435
34.468161	1139.159676	17.493453
34.182970	1138.774973	17.498471
34.486442	1131.340142	17.503488
34.086180	1116.444194	17.508506
33.847168	1122.846671	17.513523
34.080721	1138.371491	17.518541
34.301435	1143.676773	17.523559
34.113972	1146.978576	17.528576
34.612860	1143.789388	17.533594
34.619607	1140.285510	17.538611
34.595792	1145.985466	17.543629
34.210680	1139.036535	17.548647
34.432055	1144.729874	17.553664
34.269727	1140.494934	17.558682
34.073380	1142.759870	17.563699
34.545534	1145.390934	17.568717
34.527085	1145.485403	17.573735
34.559043	1134.507887	17.578752
34.535283	1143.089054	17.583770
34.300740	1136.918246	17.588787
34.688704	1139.556106	17.593805
34.384571	1150.774974	17.598823
34.537281	1151.492884	17.603840
34.446168	1158.885350	17.608858
34.585249	1164.853438	17.613875
34.611907	1160.204064	17.618893
34.468464	1162.214616	17.623911
34.635313	1164.142143	17.628928
34.766680	1184.899412	17.633946
35.135939	1186.060131	17.638963
35.115275	1181.396029	17.643981
35.073053	1191.217158	17.648999
35.588847	1181.571761	17.654016
35.163752	1196.893069	17.659034
35.422412	1183.787943	17.664051
35.447155	1179.334521	17.669069
35.714810	1182.641209	17.674087
35.679324	1172.579879	17.679104
35.113267	1167.265400	17.684122
35.105792	1156.309789	17.689139
35.220688	1180.736629	17.694157
35.621781	1178.487305	17.699175
35.278121	1185.209052	17.704192
35.447642	1186.069512	17.709210
35.494625	1181.366476	17.714227
35.446042	1179.764672	17.719245
35.436804	1183.231235	17.724263
35.311385	1177.826057	17.729280
35.390201	1181.891131	17.734298
35.138333	1185.370225	17.739315
35.871476	1196.361351	17.744333
35.723445	1200.496462	17.749351
36.640105	1199.369218	17.754368
35.944599	1196.113520	17.759386
36.036640	1193.388452	17.764403
36.399719	1203.922808	17.769421
36.140392	1190.478605	17.774439
36.027167	1181.196229	17.779456
36.018385	1176.700690	17.784474
36.048052	1182.057819	17.789491
36.397344	1196.236086	17.794509
36.129877	1206.979069	17.799527
36.757255	1196.177053	17.804544
36.030515	1181.669549	17.809562
36.050059	1180.991249	17.814579
36.202792	1192.565041	17.819597
36.009929	1201.320886	17.824615
36.328203	1187.578474	17.829632
36.515189	1192.611313	17.834650
36.283673	1194.698696	17.839667
36.122850	1189.800796	17.844685
36.428143	1194.755256	17.849703
36.710581	1190.719297	17.854720
36.669658	1193.240906	17.859738
36.493713	1192.946489	17.864755
36.728783	1199.246779	17.869773
36.386173	1200.660343	17.874791
36.520822	1205.240590	17.879808
36.750417	1221.848533	17.884826
36.961768	1222.809779	17.889843
37.152905	1223.815197	17.894861
36.954798	1230.877215	17.899879
36.988057	1221.786604	17.904896
37.256594	1227.819764	17.909914
36.703366	1211.369658	17.914931
37.337733	1218.857478	17.919949
36.726972	1225.592424	17.924967
36.969049	1215.954911	17.929984
36.800745	1224.309314	17.935002
36.747749	1226.832807	17.940019
37.021949	1221.324372	17.945037
36.899085	1227.046087	17.950055
37.428202	1219.822240	17.955072
36.965784	1223.031167	17.960090
37.392760	1226.502405	17.965107
37.776684	1228.471881	17.970125
37.711932	1224.376362	17.975143
37.314230	1218.877866	17.980160
37.291822	1223.258509	17.985178
37.686637	1225.668099	17.990195
37.750462	1232.367446	17.995213
37.394861	1230.699830	18.000231
38.037934	1236.592629	18.005248
37.833665	1234.181931	18.010266
37.863569	1226.887483	18.015283
37.727775	1220.433030	18.020301
37.977971	1228.962117	18.025319
38.124536	1215.053916	18.030336
38.022462	1220.220130	18.035354
37.773724	1211.447983	18.040371
38.006177	1218.925795	18.045389
37.995943	1231.007821	18.050407
38.238688	1227.732268	18.055424
38.184162	1233.739990	18.060442
38.007545	1238.419200	18.065459
38.169554	1236.143978	18.070477
37.958590	1239.004490	18.075495
38.306712	1234.589068	18.080512
38.210891	1242.417801	18.085530
38.336776	1236.537979	18.090547
38.509324	1236.047292	18.095565
38.625939	1237.809080	18.100583
38.178050	1231.185465	18.105600
38.081479	1234.103905	18.110618
38.368117	1235.990699	18.115635
38.591108	1231.837755	18.120653
38.483055	1234.429781	18.125671
38.316952	1232.609585	18.130688
38.525821	1232.129023	18.135706
38.238440	1231.198707	18.140723
38.228646	1245.606490	18.145741
38.304020	1253.995551	18.150759
38.768484	1237.409062	18.155776
38.599784	1254.672337	18.160794
38.780465	1256.080171	18.165811
38.726272	1256.293814	18.170829
39.074611	1257.217954	18.175847
39.239695	1249.220799	18.180864
38.935166	1252.670236	18.185882
39.335573	1255.867907	18.190899
39.410548	1244.968832	18.195917
39.024059	1252.293717	18.200935
39.288307	1249.175757	18.205952
39.225549	1248.999416	18.210970
39.475461	1253.186190	18.215987
39.587332	1247.343260	18.221005
39.500130	1243.917104	18.226023
39.535431	1249.544774	18.231040
39.385452	1253.295194	18.236058
39.272397	1245.805248	18.241075
39.195387	1245.287144	18.246093
39.285533	1261.310924	18.251111
39.440449	1269.592934	18.256128
39.513966	1271.225736	18.261146
39.248516	1274.078958	18.266163
40.198798	1265.145350	18.271181
39.803892	1267.078300	18.276199
39.999009	1270.172237	18.281216
39.949664	1269.236416	18.286234
39.851872	1270.536130	18.291251
39.929513	1258.368002	18.296269
39.587525	1271.773492	18.301287
39.849086	1262.492681	18.306304
39.890107	1270.571519	18.311322
39.487088	1271.423295	18.316339
40.175978	1271.808422	18.321357
39.558789	1266.167359	18.326375
39.817642	1272.344052	18.331392
40.300308	1280.474053	18.336410
40.630326	1297.959522	18.341427
40.381039	1280.878207	18.346445
40.083058	1274.004018	18.351463
39.996758	1282.020634	18.356480
40.465893	1294.349959	18.361498
40.342173	1300.923897	18.366515
40.538611	1294.111578	18.371533
40.681731	1294.149334	18.376551
40.532076	1295.753769	18.381568
40.347097	1293.434734	18.386586
40.240850	1295.190201	18.391603
40.849024	1290.772145	18.396621
40.377769	1290.056647	18.401639
40.626680	1289.623497	18.406656
40.811749	1286.959670	18.411674
40.444879	1285.170727	18.416691
40.980214	1297.795860	18.421709
41.056055	1305.679944	18.426727
41.219813	1305.468335	18.431744
41.181032	1304.770708	18.436762
41.077858	1301.877203	18.441779
41.311466	1303.633405	18.446797
41.329099	1301.648896	18.451815
40.998844	1294.363159	18.456832
41.220501	1300.362617	18.461850
40.908009	1314.602990	18.466867
41.236290	1301.802518	18.471885
41.430330	1313.250037	18.476903
41.458787	1308.849653	18.481920
41.800123	1299.856203	18.486938
41.600020	1315.388735	18.491955
41.584677	1310.124169	18.496973
41.134317	1318.042849	18.501991
41.450826	1310.410254	18.507008
41.672796	1316.214009	18.512026
41.273115	1317.219902	18.517043
41.555089	1307.929577	18.522061
41.983216	1305.486680	18.527079
41.993828	1302.373487	18.532096
41.549010	1307.968631	18.537114
41.328953	1306.570238	18.542131
41.506633	1316.335108	18.547149
41.712900	1334.098656	18.552167
41.862838	1332.254491	18.557184
42.357438	1324.218621	18.562202
42.255696	1328.715785	18.567219
42.400310	1326.834579	18.572237
42.336360	1317.929467	18.577255
42.425766	1328.812620	18.582272
42.528675	1324.870855	18.587290
42.012025	1321.773478	18.592307
42.053322	1319.898892	18.597325
42.170238	1321.490228	18.602343
42.345152	1325.250039	18.607360
42.456315	1314.629309	18.612378
42.377663	1323.373743	18.617395
42.374051	1321.357826	18.622413
42.331068	1325.006396	18.627431
42.219260	1324.421124	18.632448
42.367425	1323.558691	18.637466
42.538971	1334.053517	18.642483
42.510734	1341.543567	18.647501
43.119720	1345.557692	18.652519
42.634812	1349.701107	18.657536
43.207657	1346.295242	18.662554
43.031944	1351.078483	18.667571
43.146630	1351.789698	18.672589
43.043195	1337.876143	18.677607
43.079448	1349.509198	18.682624
42.700680	1341.375771	18.687642
42.916263	1349.272832	18.692659
42.817440	1349.212558	18.697677
42.735589	1342.560313	18.702695
42.785762	1347.292605	18.707712
43.259995	1349.225943	18.712730
42.627124	1358.902440	18.717747
43.540178	1362.275935	18.722765
43.714428	1365.231126	18.727783
43.702119	1376.120676	18.732800
43.870019	1360.151450	18.737818
43.669877	1367.210683	18.742835
43.894751	1365.714609	18.747853
43.791280	1354.436150	18.752871
43.826057	1351.499067	18.757888
43.640248	1337.156525	18.762906
43.422384	1349.744329	18.767923
43.717196	1349.187267	18.772941
44.219047	1362.130083	18.777959
44.006746	1356.539562	18.782976
43.752690	1371.209539	18.787994
43.796755	1369.356607	18.793011
43.735025	1369.470439	18.798029
44.044207	1367.740332	18.803047
43.798403	1363.127015	18.808064
43.767463	1360.209630	18.813082
44.122480	1372.582023	18.818099
44.312343	1373.799088	18.823117
44.298980	1375.473829	18.828135
44.268940	1390.415058	18.833152
44.670718	1379.995196	18.838170
44.583605	1389.848671	18.843187
44.462745	1394.115297	18.848205
44.428458	1395.114797	18.853223
44.229501	1393.391218	18.858240
44.525067	1385.345285	18.863258
44.262091	1384.947650	18.868275
44.361024	1386.822659	18.873293
44.535722	1394.224331	18.878311
44.461935	1388.536493	18.883328
44.615882	1390.216744	18.888346
44.342699	1399.761523	18.893363
44.979305	1390.002529	18.898381
45.228309	1397.301114	18.903399
45.247224	1409.848939	18.908416
45.477172	1406.329192	18.913434
45.386714	1401.716924	18.918451
45.143585	1391.110285	18.923469
45.126394	1389.115409	18.928487
45.208933	1394.290800	18.933504
45.586943	1393.588238	18.938522
45.309808	1381.973881	18.943539
45.460971	1377.898359	18.948557
45.532334	1376.792260	18.953575
45.384394	1380.302548	18.958592
45.307574	1382.602553	18.963610
45.359854	1386.542418	18.968627
45.900737	1390.664987	18.973645
45.824466	1394.858399	18.978663
45.681079	1388.619662	18.983680
45.652329	1388.160312	18.988698
45.789670	1395.488905	18.993715
45.514143	1390.274292	18.998733
46.025897	1388.121322	19.003751
45.652437	1403.336938	19.008768
46.105173	1390.583297	19.013786
45.935974	1400.070861	19.018803
46.158058	1398.818217	19.023821
46.066842	1395.935457	19.028839
45.897454	1405.372559	19.033856
46.366508	1394.601385	19.038874
45.698267	1401.705110	19.043891
45.809289	1403.975872	19.048909
46.228594	1400.817966	19.053927
45.845688	1411.206658	19.058944
46.435971	1412.689587	19.063962
46.513755	1423.956461	19.068979
46.167788	1414.527162	19.073997
46.210712	1416.451921	19.079015
46.316587	1413.847742	19.084032
46.317282	1416.037853	19.089050
46.601272	1417.262356	19.094067
46.663385	1423.545474	19.099085
47.093297	1425.675070	19.104103
46.920270	1423.584532	19.109120
47.116056	1418.302840	19.114138
46.816143	1411.425744	19.119155
46.834913	1416.144008	19.124173
47.252515	1424.517736	19.129191
46.865769	1440.871549	19.134208
46.316734	1429.226911	19.139226
46.786025	1442.556710	19.144243
46.778127	1444.199049	19.149261
47.346563	1433.608039	19.154279
46.851671	1445.730956	19.159296
47.335914	1441.982259	19.164314
47.383015	1447.305195	19.169331
47.360422	1460.175101	19.174349
47.635655	1451.775695	19.179367
47.947957	1456.426178	19.184384
48.194787	1445.430795	19.189402
48.029809	1433.865215	19.194419
47.714206	1424.390157	19.199437
48.507803	1430.815010	19.204455
47.763531	1429.274161	19.209472
47.830363	1425.265407	19.214490
47.891633	1432.807832	19.219507
47.826181	1431.603109	19.224525
47.703101	1428.980927	19.229543
47.817879	1432.933162	19.234560
47.445385	1428.046061	19.239578
47.901605	1443.164092	19.244595
47.626553	1448.104838	19.249613
48.197400	1439.107143	19.254631
47.991213	1457.607222	19.259648
48.254921	1451.106264	19.264666
48.283527	1450.682164	19.269683
48.052413	1448.733212	19.274701
48.254421	1451.523149	19.279719
48.007620	1449.535612	19.284736
48.433923	1452.906014	19.289754
48.340718	1473.442963	19.294771
48.611027	1470.623826	19.299789
48.551260	1469.159437	19.304807
48.630271	1477.974075	19.309824
48.740372	1469.912798	19.314842
48.648648	1475.307850	19.319859
48.887331	1477.189513	19.324877
48.913126	1475.976892	19.329895
48.607900	1474.165709	19.334912
48.880087	1465.025151	19.339930
49.094398	1476.974552	19.344947
49.213989	1483.908310	19.349965
49.119408	1474.717553	19.354983
49.058000	1476.535484	19.360000
48.830918	1469.296728	19.365018
49.077319	1483.522803	19.370035
49.336292	1504.872810	19.375053
49.318823	1500.227062	19.380071
49.184347	1504.581042	19.385088
49.439720	1491.889616	19.390106
49.435866	1495.058753	19.395123
49.403990	1505.124600	19.400141
49.482330	1482.374693	19.405159
49.366996	1497.594382	19.410176
49.410767	1494.621161	19.415194
49.568739	1498.516192	19.420211
49.313160	1522.840235	19.425229
49.770824	1512.856568	19.430247
49.925113	1518.134434	19.435264
49.779474	1507.206430	19.440282
50.108573	1510.749769	19.445299
49.956566	1511.060696	19.450317
50.168891	1504.119590	19.455335
50.048022	1508.398868	19.460352
50.272008	1508.266242	19.465370
49.981389	1507.579415	19.470387
50.607963	1513.004656	19.475405
50.136249	1516.151965	19.480423
50.544629	1521.614336	19.485440
50.495727	1520.214525	19.490458
50.948454	1527.374146	19.495475
50.828556	1534.411484	19.500493
50.733562	1520.060966	19.505511
50.597977	1512.101039	19.510528
50.413084	1527.539869	19.515546
50.734645	1520.304035	19.520563
50.955756	1524.214488	19.525581
50.672803	1524.220751	19.530599
50.741050	1530.632341	19.535616
51.183433	1534.334774	19.540634
51.118902	1522.952314	19.545651
50.597674	1529.818603	19.550669
50.971108	1532.092707	19.555687
51.022911	1522.244810	19.560704
50.784978	1532.216520	19.565722
51.031864	1539.067364	19.570739
51.353087	1554.733534	19.575757
51.258856	1549.326543	19.580775
51.389090	1548.653085	19.585792
51.841679	1546.051712	19.590810
51.878391	1548.435049	19.595827
51.761114	1553.007272	19.600845
51.971587	1551.055828	19.605863
51.664448	1539.812117	19.610880
51.567576	1546.097940	19.615898
51.842495	1539.835048	19.620915
52.099160	1540.593594	19.625933
52.137575	1541.281978	19.630951
51.231995	1546.494492	19.635968
52.054887	1545.217724	19.640986
52.319843	1541.575733	19.646003
51.702462	1544.572155	19.651021
51.762325	1539.974318	19.656039
51.935773	1542.623547	19.661056
52.131749	1545.947776	19.666074
52.099313	1545.593139	19.671091
51.676670	1546.536346	19.676109
52.160009	1553.807978	19.681127
52.305245	1564.587907	19.686144
52.203332	1563.433034	19.691162
52.364537	1561.722793	19.696179
52.202634	1574.769108	19.701197
52.142643	1567.980829	19.706215
52.668934	1584.230488	19.711232
53.233765	1579.815955	19.716250
53.458481	1581.008673	19.721267
52.768216	1580.185247	19.726285
53.160021	1574.147145	19.731303
53.304297	1564.196463	19.736320
52.965997	1560.992380	19.741338
53.359357	1567.870923	19.746355
53.241912	1564.657700	19.751373
52.890659	1566.202027	19.756391
53.113914	1576.300776	19.761408
53.465351	1587.105419	19.766426
53.176716	1577.525094	19.771443
53.387054	1583.542189	19.776461
53.492812	1584.169596	19.781479
53.446747	1589.917341	19.786496
53.775715	1584.760034	19.791514
53.605215	1573.542366	19.796531
53.763522	1583.613361	19.801549
54.013358	1576.663230	19.806567
53.793574	1575.760241	19.811584
53.663856	1580.422772	19.816602
53.643569	1575.641741	19.821619
53.360640	1582.644520	19.826637
53.545091	1577.607547	19.831655
54.343883	1598.053098	19.836672
54.204027	1605.469118	19.841690
53.900832	1604.064710	19.846707
54.287490	1604.051926	19.851725
54.130690	1604.325731	19.856743
54.268154	1605.011319	19.861760
54.350324	1611.786849	19.866778
54.636588	1603.571850	19.871795
54.572193	1608.580829	19.876813
54.499422	1603.205194	19.881831
54.434451	1604.237886	19.886848
54.627789	1596.602256	19.891866
54.638859	1606.036614	19.896883
54.444331	1601.633005	19.901901
54.734575	1602.979627	19.906919
54.883269	1598.727711	19.911936
54.721647	1600.097347	19.916954
54.835692	1601.461934	19.921971
54.860509	1619.304512	19.926989
54.944753	1622.573566	19.932007
55.033423	1622.335774	19.937024
54.538474	1628.121861	19.942042
54.983416	1620.955141	19.947059
55.091029	1625.568109	19.952077
55.257305	1620.985241	19.957095
55.216021	1624.434788	19.962112
55.277414	1622.547574	19.967130
55.303561	1634.952418	19.972147
55.462580	1643.174002	19.977165
55.374511	1644.245007	19.982183
55.601954	1642.338249	19.987200
55.449204	1644.555434	19.992218
55.649629	1636.423213	19.997235
55.639312	1643.970562	20.002253
55.860069	1644.539040	20.007271
55.832357	1658.669075	20.012288
55.831170	1639.194513	20.017306
56.160262	1642.343397	20.022323
56.067821	1652.371419	20.027341
56.321907	1653.812038	20.032359
56.633860	1664.316757	20.037376
56.128685	1650.159388	20.042394
56.447570	1645.729482	20.047411
56.385730	1646.910014	20.052429
56.358633	1654.895489	20.057447
56.375840	1665.518683	20.062464
56.365954	1668.357425	20.067482
56.427976	1668.846474	20.072499
56.484361	1666.290991	20.077517
56.308865	1666.558240	20.082535
56.701335	1660.914489	20.087552
56.746922	1664.568273	20.092570
56.505132	1661.513250	20.097587
56.763549	1676.087909	20.102605
57.277341	1688.511544	20.107623
57.378107	1682.673356	20.112640
56.768648	1684.967965	20.117658
57.174475	1676.544965	20.122675
57.399635	1684.339696	20.127693
57.232364	1680.976416	20.132711
57.534510	1679.042244	20.137728
57.542750	1681.957062	20.142746
57.604012	1678.409875	20.147763
57.268533	1679.806586	20.152781
57.920543	1682.703226	20.157799
57.850478	1683.664130	20.162816
57.848224	1685.128883	20.167834
57.974883	1682.426754	20.172851
57.839469	1675.183109	20.177869
57.865745	1675.362138	20.182887
58.210506	1678.808396	20.187904
57.963683	1687.310943	20.192922
58.011912	1673.928945	20.197939
57.756396	1673.533297	20.202957
58.216857	1680.218397	20.207975
57.897233	1674.477223	20.212992
58.166925	1679.756105	20.218010
58.690491	1691.657501	20.223027
57.961319	1682.701141	20.228045
58.281973	1699.317444	20.233063
58.185093	1693.431129	20.238080
58.132338	1707.640843	20.243098
58.305746	1709.100339	20.248115
58.372321	1704.116398	20.253133
58.387989	1707.348807	20.258151
58.663244	1716.035176	20.263168
58.681330	1724.045205	20.268186
58.686256	1725.467817	20.273203
58.517663	1731.370387	20.278221
58.814449	1729.478071	20.283239
59.133673	1731.217830	20.288256
59.093182	1732.224627	20.293274
59.162473	1728.862377	20.298291
59.578652	1730.091568	20.303309
59.036573	1724.549119	20.308327
59.558403	1721.763367	20.313344
59.124532	1720.126825	20.318362
59.056608	1739.243156	20.323379
59.431477	1747.229205	20.328397
59.288293	1751.035477	20.333415
59.680754	1744.353417	20.338432
59.828812	1745.015270	20.343450
59.865763	1740.727069	20.348467
59.947878	1745.694340	20.353485
59.720666	1742.750645	20.358503
59.692778	1742.272217	20.363520
59.879961	1749.949810	20.368538
60.024629	1737.515293	20.373555
60.032846	1729.151018	20.378573
59.890764	1735.027371	20.383591
60.427298	1748.141799	20.388608
60.272887	1762.433657	20.393626
60.434573	1762.124533	20.398643
60.572787	1756.829615	20.403661
60.271166	1757.813951	20.408679
60.790889	1758.181248	20.413696
60.651398	1762.933712	20.418714
60.530464	1758.354500	20.423731
60.864980	1759.861502	20.428749
60.481568	1768.426380	20.433767
60.744546	1752.306297	20.438784
60.469598	1756.360308	20.443802
61.001873	1762.396770	20.448819
61.151673	1772.185167	20.453837
61.427400	1780.148796	20.458855
61.343665	1777.245875	20.463872
60.955120	1782.826092	20.468890
61.319594	1779.553577	20.473907
61.441413	1770.934904	20.478925
61.165991	1782.559962	20.483943
60.938856	1772.619652	20.488960
61.099970	1779.225161	20.493978
61.151197	1782.502541	20.498995
61.833861	1796.563110	20.504013
61.730160	1801.111191	20.509031
62.254645	1799.012998	20.514048
61.397275	1800.670859	20.519066
61.788101	1801.541076	20.524083
62.002385	1800.964980	20.529101
61.590573	1804.778372	20.534119
61.988124	1799.894356	20.539136
61.644943	1800.863074	20.544154
62.134685	1800.509185	20.549171
62.516127	1796.855319	20.554189
62.186338	1805.872625	20.559207
62.407238	1815.359634	20.564224
62.233747	1824.854402	20.569242
62.636291	1817.252380	20.574259
62.489391	1812.885486	20.579277
62.455183	1825.473433	20.584295
62.440158	1818.715930	20.589312
62.283423	1820.555049	20.594330
62.391005	1822.034272	20.599347
63.093016	1832.244824	20.604365
62.393726	1842.559945	20.609383
63.238773	1848.572987	20.614400
63.138724	1846.669857	20.619418
62.780984	1847.047536	20.624435
63.066823	1847.615356	20.629453
62.858747	1844.858018	20.634471
63.229539	1837.718536	20.639488
63.150504	1845.503893	20.644506
63.401920	1837.770753	20.649523
63.464864	1842.188754	20.654541
63.587499	1857.586300	20.659559
63.508963	1859.672033	20.664576
64.013284	1872.267689	20.669594
63.875278	1860.369418	20.674611
64.051482	1851.758018	20.679629
64.185157	1861.103993	20.684647
64.004414	1843.427624	20.689664
63.759196	1856.184150	20.694682
64.154731	1867.092554	20.699699
63.641588	1861.564492	20.704717
63.894024	1866.966041	20.709735
63.953986	1864.100694	20.714752
64.072595	1868.528970	20.719770
63.739392	1864.067990	20.724787
64.444986	1878.446955	20.729805
64.252909	1878.095076	20.734823
64.260851	1877.118744	20.739840
64.480209	1887.344513	20.744858
64.299630	1887.290654	20.749875
64.718945	1884.407225	20.754893
65.014556	1911.167547	20.759911
65.035867	1906.534591	20.764928
65.131518	1907.513888	20.769946
65.499980	1902.694336	20.774963
65.405250	1888.867361	20.779981
65.219290	1888.460878	20.784999
65.321705	1880.829816	20.790016
65.427300	1875.599903	20.795034
65.271512	1886.228072	20.800051
65.370510	1880.942379	20.805069
65.491851	1899.783254	20.810087
65.806640	1899.090517	20.815104
65.992686	1904.350930	20.820122
65.887507	1902.448593	20.825139
65.930702	1900.633612	20.830157
65.820204	1910.222763	20.835175
65.980706	1902.459567	20.840192
65.898255	1907.244216	20.845210
65.917414	1911.189353	20.850227
66.070602	1891.769378	20.855245
66.238473	1901.965301	20.860263
66.087656	1897.734699	20.865280
65.954131	1896.316474	20.870298
66.125772	1907.521702	20.875315
66.116202	1907.378100	20.880333
65.688504	1920.933124	20.885351
66.498272	1928.718996	20.890368
66.246592	1925.542387	20.895386
66.324693	1926.148865	20.900403
66.842959	1921.984504	20.905421
66.702739	1926.689787	20.910439
66.729006	1940.354033	20.915456
66.689752	1942.730315	20.920474
66.684889	1946.420415	20.925491
67.219302	1941.805397	20.930509
67.287642	1940.564029	20.935527
67.562237	1941.834216	20.940544
67.311049	1937.884329	20.945562
67.424541	1933.959718	20.950579
67.331151	1932.197558	20.955597
67.524388	1941.458560	20.960615
67.528614	1940.220863	20.965632
67.872320	1939.615144	20.970650
67.873144	1941.975718	20.975667
67.728107	1937.507514	20.980685
67.467336	1948.022672	20.985703
67.546593	1927.298153	20.990720
67.850998	1940.754988	20.995738
68.011815	1951.599000	21.000755
68.406252	1958.310264	21.005773
68.070649	1961.625813	21.010791
67.970403	1966.309102	21.015808
68.178047	1965.349012	21.020826
68.111078	1970.797166	21.025843
68.028398	1965.138932	21.030861
68.071490	1959.044537	21.035879
68.291627	1964.728865	21.040896
68.331989	1967.297889	21.045914
68.192693	1977.421754	21.050931
68.505655	1985.733141	21.055949
68.846733	1995.302524	21.060967
68.933000	1985.777222	21.065984
69.238838	1982.908290	21.071002
69.131407	1983.581527	21.076019
68.805233	1983.635545	21.081037
68.805706	1984.989441	21.086055
69.030358	2002.160636	21.091072
69.587424	2006.962511	21.096090
69.351385	2002.842987	21.101107
69.942880	2006.960978	21.106125
69.859669	2003.218462	21.111143
69.810412	2003.800588	21.116160
69.765392	1995.696951	21.121178
69.653446	2004.970786	21.126195
69.565815	1988.911389	21.131213
69.732011	1997.548601	21.136231
69.459258	1993.340118	21.141248
69.875381	1990.665461	21.146266
70.157118	1997.962353	21.151283
69.900531	1989.629717	21.156301
70.187650	1998.983433	21.161319
70.175867	2010.529720	21.166336
70.213613	2006.579015	21.171354
70.307962	2011.452934	21.176371
70.753764	2010.758731	21.181389
70.692261	2016.171332	21.186407
70.466827	2014.133066	21.191424
70.658016	2020.872843	21.196442
70.485000	2018.715957	21.201459
70.565236	2009.500862	21.206477
70.763855	2007.576462	21.211495
70.306692	2023.408418	21.216512
71.153384	2029.834692	21.221530
70.596868	2036.858152	21.226547
70.930478	2036.579063	21.231565
70.882167	2040.184425	21.236583
70.993979	2046.248577	21.241600
70.921696	2058.476528	21.246618
71.149231	2061.978984	21.251635
71.411196	2064.371504	21.256653
71.772797	2064.747647	21.261671
71.381533	2062.684699	21.266688
72.029378	2056.912698	21.271706
71.869770	2074.528813	21.276723
72.096160	2064.082210	21.281741
72.140600	2072.817314	21.286759
72.574307	2071.531676	21.291776
72.460094	2057.126912	21.296794
72.118564	2066.297662	21.301811
71.822377	2051.249020	21.306829
72.290071	2070.465357	21.311847
72.539594	2074.876458	21.316864
72.700096	2076.312747	21.321882
72.625923	2078.640833	21.326899
72.781868	2070.815155	21.331917
72.777044	2070.793894	21.336935
72.626111	2069.135358	21.341952
72.689516	2074.774692	21.346970
72.697904	2075.685532	21.351987
72.746979	2076.861447	21.357005
72.995676	2078.650093	21.362023
72.583123	2078.556608	21.367040
73.131581	2072.383492	21.372058
72.571553	2081.717662	21.377075
73.056149	2091.709739	21.382093
72.671147	2098.703363	21.387111
73.019882	2097.462512	21.392128
73.162650	2113.425214	21.397146
73.186402	2119.083360	21.402163
73.588805	2115.441946	21.407181
74.087694	2118.012189	21.412199
73.955498	2121.832608	21.417216
74.020877	2112.840689	21.422234
74.186952	2113.607053	21.427251
74.581298	2106.848823	21.432269
74.557719	2116.342496	21.437287
73.942196	2118.044785	21.442304
74.504724	2110.455602	21.447322
74.454230	2113.723633	21.452339
74.390100	2110.710302	21.457357
74.327263	2109.599805	21.462375
74.363269	2114.899420	21.467392
74.899089	2119.480562	21.472410
74.612374	2128.863725	21.477427
74.826097	2139.270405	21.482445
75.123801	2140.720053	21.487463
75.089157	2140.283693	21.492480
75.485544	2133.080146	21.497498
74.973482	2138.793318	21.502515
75.264974	2134.714711	21.507533
75.270383	2127.265913	21.512551
75.333701	2130.516227	21.517568
75.261038	2128.968581	21.522586
75.217563	2129.739168	21.527603
75.690759	2129.419410	21.532621
75.281668	2130.082812	21.537639
75.620217	2139.390723	21.542656
75.871247	2148.491349	21.547674
75.704833	2144.234713	21.552691
75.390127	2148.686340	21.557709
75.833016	2158.116878	21.562727
75.537871	2154.650335	21.567744
76.272130	2158.165439	21.572762
76.337183	2168.847759	21.577779
76.244148	2173.419521	21.582797
76.260929	2173.786234	21.587815
76.146625	2183.496050	21.592832
76.480539	2177.712925	21.597850
76.330317	2187.876480	21.602867
75.952394	2183.264584	21.607885
76.650456	2192.283008	21.612903
76.462200	2201.360531	21.617920
76.570707	2195.662990	21.622938
76.756379	2201.693603	21.627955
76.601352	2207.575281	21.632973
77.239385	2213.339799	21.637991
77.534422	2225.902014	21.643008
77.700416	2218.715368	21.648026
77.577762	2218.620929	21.653043
77.724744	2202.654207	21.658061
77.682695	2191.381436	21.663079
77.419313	2198.756970	21.668096
77.628139	2203.575246	21.673114
77.339209	2215.029109	21.678131
77.769468	2220.235813	21.683149
78.079662	2214.238608	21.688167
77.983727	2223.112411	21.693184
77.996031	2218.114685	21.698202
78.086263	2223.109229	21.703219
78.158242	2226.137295	21.708237
78.170027	2215.979649	21.713255
78.225741	2222.901549	21.718272
78.318938	2229.445211	21.723290
77.950162	2235.167664	21.728307
78.575287	2246.027931	21.733325
78.659172	2236.786903	21.738343
78.562966	2247.270303	21.743360
78.643825	2233.182182	21.748378
78.783164	2236.562698	21.753395
79.116434	2257.510699	21.758413
79.274323	2257.773389	21.763431
78.905279	2260.396730	21.768448
79.751806	2259.962037	21.773466
79.545095	2264.696696	21.778483
79.310341	2268.668821	21.783501
79.176448	2254.077603	21.788519
79.314323	2265.089487	21.793536
79.685066	2258.325407	21.798554
79.831685	2260.827435	21.803571
79.313935	2258.443312	21.808589
79.623417	2250.884000	21.813607
79.430223	2270.689468	21.818624
79.798096	2273.939730	21.823642
79.727005	2284.204635	21.828659
79.639682	2281.409493	21.833677
80.371174	2287.711780	21.838695
80.211126	2297.857992	21.843712
80.829686	2292.582808	21.848730
80.973515	2300.879648	21.853747
81.031964	2294.637573	21.858765
81.107862	2294.319706	21.863783
80.915239	2296.095030	21.868800
81.018235	2282.401077	21.873818
81.522166	2287.321761	21.878835
81.249551	2279.597432	21.883853
81.565733	2265.056059	21.888871
81.291666	2264.511798	21.893888
81.225825	2258.503692	21.898906
81.366103	2263.430492	21.903923
81.587452	2274.842818	21.908941
81.514984	2281.020952	21.913959
81.365839	2291.159151	21.918976
81.975697	2279.144164	21.923994
81.863400	2289.535415	21.929011
81.708907	2288.142514	21.934029
81.726126	2280.581354	21.939047
81.487040	2281.458146	21.944064
81.532697	2283.275270	21.949082
81.547666	2303.083080	21.954099
81.771378	2309.341349	21.959117
81.742419	2306.082655	21.964135
82.216708	2323.272099	21.969152
82.073397	2333.283174	21.974170
82.679286	2335.622184	21.979187
82.675061	2340.388456	21.984205
82.723501	2335.571274	21.989223
82.555598	2341.975738	21.994240
82.744331	2341.040666	21.999258
82.792825	2334.620235	22.004275
82.222694	2333.541367	22.009293
83.123959	2340.353757	22.014311
83.055652	2354.023576	22.019328
83.409214	2360.690860	22.024346
83.159504	2362.506639	22.029363
82.893576	2363.845233	22.034381
83.294809	2355.103877	22.039399
83.361832	2361.850490	22.044416
83.539664	2373.528445	22.049434
83.924321	2377.637699	22.054451
83.581100	2378.609609	22.059469
84.120067	2374.811173	22.064487
83.958533	2377.023504	22.069504
84.122120	2373.807407	22.074522
84.429187	2372.803413	22.079539
83.949074	2382.320967	22.084557
84.268063	2371.793493	22.089575
84.193246	2388.863353	22.094592
84.422851	2386.978273	22.099610
84.381369	2388.887874	22.104627
84.741202	2393.490175	22.109645
84.700334	2386.263081	22.114663
85.063008	2387.964582	22.119680
84.731700	2392.248431	22.124698
84.576681	2394.040002	22.129715
84.938419	2406.803411	22.134733
85.314540	2409.181360	22.139751
85.303730	2414.292681	22.144768
84.838595	2411.376450	22.149786
85.137286	2411.311089	22.154803
85.048197	2419.095104	22.159821
85.502825	2430.528017	22.164839
85.644544	2432.790976	22.169856
86.143672	2434.733185	22.174874
86.199273	2432.695299	22.179891
86.107419	2438.314737	22.184909
86.465156	2429.163524	22.189927
86.384686	2429.968288	22.194944
86.523174	2426.727686	22.199962
86.389966	2422.724606	22.204979
86.414310	2425.280410	22.209997
86.860735	2421.704669	22.215015
86.694041	2431.668944	22.220032
86.748818	2425.080235	22.225050
86.733097	2428.257697	22.230067
86.595113	2422.907749	22.235085
86.721356	2417.440920	22.240103
86.908369	2431.282498	22.245120
87.255184	2444.830947	22.250138
87.336487	2446.317469	22.255155
87.335793	2450.647693	22.260173
87.832282	2435.860345	22.265191
87.559858	2446.330269	22.270208
87.321207	2438.840439	22.275226
87.278591	2430.408007	22.280243
87.320921	2439.951555	22.285261
87.252859	2449.281906	22.290279
87.841671	2463.578537	22.295296
87.960666	2468.120518	22.300314
88.268829	2462.587480	22.305331
88.062201	2454.527732	22.310349
88.346847	2463.326621	22.315367
88.269812	2479.273374	22.320384
88.345984	2467.940995	22.325402
88.116903	2466.742741	22.330419
88.724483	2468.301972	22.335437
88.577492	2486.733934	22.340455
88.482863	2484.009330	22.345472
88.660135	2487.627000	22.350490
88.737243	2488.527161	22.355507
88.443802	2491.870958	22.360525
89.104877	2486.683779	22.365543
89.148532	2504.691576	22.370560
89.114262	2522.739927	22.375578
89.347131	2514.122544	22.380595
89.426647	2520.040396	22.385613
89.904458	2502.652188	22.390631
89.554139	2505.402045	22.395648
89.622826	2504.551930	22.400666
89.823008	2505.953673	22.405683
89.622099	2502.696466	22.410701
89.897636	2500.649578	22.415719
90.067797	2522.339699	22.420736
90.262461	2533.923614	22.425754
90.200514	2528.243038	22.430771
90.200005	2534.337467	22.435789
90.375641	2532.681695	22.440807
90.255443	2532.577404	22.445824
90.334446	2531.826675	22.450842
90.708731	2532.768938	22.455859
90.362752	2550.130495	22.460877
90.853182	2550.470813	22.465895
90.960497	2553.370348	22.470912
90.833029	2548.353263	22.475930
90.827865	2553.072398	22.480947
91.071704	2562.275347	22.485965
91.504729	2563.934352	22.490983
91.375540	2569.840530	22.496000
91.548545	2577.081999	22.501018
91.701501	2573.125856	22.506035
91.445512	2576.362845	22.511053
91.939086	2572.558812	22.516071
92.052628	2568.561466	22.521088
92.010995	2576.114084	22.526106
91.822661	2563.945449	22.531123
91.933929	2576.893155	22.536141
92.583688	2573.203670	22.541159
92.559717	2591.597650	22.546176
92.308784	2589.850485	22.551194
92.699375	2581.912308	22.556211
92.177869	2591.032445	22.561229
92.378015	2591.657816	22.566247
92.535117	2595.013543	22.571264
92.959900	2613.804770	22.576282
93.296151	2607.039617	22.581299
93.015370	2616.254841	22.586317
93.120963	2602.509743	22.591335
93.504487	2601.228726	22.596352
93.106913	2613.406709	22.601370
93.289075	2599.987386	22.606387
93.047779	2612.734371	22.611405
93.505678	2623.646154	22.616423
93.807426	2630.959126	22.621440
93.959334	2628.461222	22.626458
93.880803	2624.954550	22.631475
93.736709	2632.239100	22.636493
94.209899	2625.825032	22.641511
94.629768	2627.735418	22.646528
94.629563	2633.223875	22.651546
94.691638	2613.754183	22.656563
94.388701	2622.392150	22.661581
94.611951	2632.598803	22.666599
95.118872	2634.817553	22.671616
95.053957	2643.831912	22.676634
95.223416	2641.287089	22.681651
95.066144	2631.966631	22.686669
94.881085	2632.263785	22.691687
95.470047	2640.324209	22.696704
95.037821	2650.197393	22.701722
95.191256	2639.089578	22.706739
95.301257	2640.256045	22.711757
95.375349	2640.140439	22.716775
95.368503	2642.881025	22.721792
95.664107	2634.487363	22.726810
95.266433	2638.308197	22.731827
95.453855	2657.546710	22.736845
95.830798	2657.895231	22.741863
95.812471	2663.717903	22.746880
95.741914	2667.560402	22.751898
96.159539	2674.391412	22.756915
96.015247	2684.207161	22.761933
96.174003	2682.550848	22.766951
96.525990	2686.646324	22.771968
96.311273	2687.692924	22.776986
96.713252	2691.622815	22.782003
96.813645	2712.434024	22.787021
96.545610	2709.398686	22.792039
96.887426	2704.554665	22.797056
96.620491	2710.646450	22.802074
97.146476	2712.152130	22.807091
97.460198	2720.536331	22.812109
97.532930	2719.297383	22.817127
98.052116	2717.947896	22.822144
97.986526	2722.540773	22.827162
98.486756	2715.074655	22.832179
98.439726	2720.807133	22.837197
98.300838	2711.262847	22.842215
98.520150	2720.163559	22.847232
98.254497	2717.702250	22.852250
98.465672	2709.747766	22.857267
98.294642	2701.644492	22.862285
98.452311	2705.587176	22.867303
98.390762	2711.716417	22.872320
98.390583	2712.448727	22.877338
98.334352	2712.003090	22.882355
98.352854	2714.275800	22.887373
98.871164	2740.759676	22.892391
99.075417	2734.466343	22.897408
99.188722	2744.204145	22.902426
98.951711	2742.382209	22.907443
98.907150	2746.596248	22.912461
99.015070	2757.486857	22.917479
99.345986	2759.490008	22.922496
99.243079	2766.897599	22.927514
99.149464	2769.187772	22.932531
99.952261	2776.665811	22.937549
99.267100	2788.165949	22.942567
100.004046	2791.620798	22.947584
99.756440	2790.466436	22.952602
100.173358	2784.622853	22.957619
100.236512	2797.625549	22.962637
100.476553	2815.303256	22.967655
100.656583	2812.359099	22.972672
100.750477	2809.194805	22.977690
100.914137	2812.701042	22.982707
101.034992	2817.599459	22.987725
100.915775	2810.816774	22.992743
100.866982	2808.318532	22.997760
101.176038	2814.503726	23.002778
101.528388	2810.197725	23.007795
101.385628	2812.025301	23.012813
101.091109	2810.218623	23.017831
101.564871	2828.986670	23.022848
101.550632	2830.052562	23.027866
101.948141	2829.905538	23.032883
101.686894	2829.737991	23.037901
101.503052	2832.506162	23.042919
101.956109	2832.410455	23.047936
101.820048	2831.525926	23.052954
102.137798	2824.602613	23.057971
102.215600	2844.858868	23.062989
102.420894	2850.599443	23.068007
102.574615	2850.686052	23.073024
102.476296	2859.816183	23.078042
102.510848	2852.861205	23.083059
102.616545	2853.024724	23.088077
102.154709	2854.112964	23.093095
102.774135	2863.065071	23.098112
103.240871	2873.877793	23.103130
103.256567	2875.563930	23.108147
103.290127	2873.371622	23.113165
103.224967	2872.185693	23.118183
103.560949	2878.606579	23.123200
103.586756	2890.636773	23.128218
103.829592	2888.197267	23.133235
103.658343	2885.440346	23.138253
103.554981	2894.823766	23.143271
103.892425	2882.289008	23.148288
104.054361	2903.570581	23.153306
104.312644	2910.423335	23.158323
104.782383	2915.879740	23.163341
104.723222	2914.235242	23.168359
104.944811	2911.758011	23.173376
105.055269	2918.220336	23.178394
105.061105	2894.952856	23.183411
104.974896	2908.502798	23.188429
105.274374	2910.132131	23.193447
105.260017	2909.938768	23.198464
104.924885	2911.540663	23.203482
104.890635	2905.603168	23.208499
105.235678	2911.221009	23.213517
105.134598	2931.429467	23.218535
105.419886	2932.795901	23.223552
105.699979	2936.217757	23.228570
105.690891	2934.035237	23.233587
105.896640	2944.431003	23.238605
105.837858	2947.372243	23.243623
106.071306	2943.621257	23.248640
106.104247	2952.715218	23.253658
105.902636	2952.964457	23.258675
106.593281	2966.134692	23.263693
106.647092	2979.230501	23.268711
106.966170	2975.226314	23.273728
106.838829	2987.674929	23.278746
106.507394	2973.113882	23.283763
106.826389	2971.410502	23.288781
106.801357	2981.236250	23.293799
107.411229	2990.088914	23.298816
107.206274	3014.123048	23.303834
107.519279	2998.966137	23.308851
107.419653	2996.384257	23.313869
107.230926	3002.498681	23.318887
107.665917	3004.147954	23.323904
107.688946	3015.323361	23.328922
107.490162	3020.817604	23.333939
108.066161	3027.308483	23.338957
107.891050	3035.686881	23.343975
108.006787	3028.387805	23.348992
108.330785	3041.264851	23.354010
108.299579	3038.643908	23.359027
108.777989	3041.526775	23.364045
108.929951	3036.166218	23.369063
108.822172	3040.910925	23.374080
108.998910	3039.864065	23.379098
108.744273	3044.839942	23.384115
108.971674	3035.235299	23.389133
108.973839	3062.488041	23.394151
109.369225	3055.075980	23.399168
109.525028	3062.339261	23.404186
109.602169	3055.497507	23.409203
109.800689	3049.577377	23.414221
109.626385	3052.277819	23.419239
110.062629	3050.149039	23.424256
110.089937	3060.676806	23.429274
110.115855	3078.258708	23.434291
110.201826	3080.047543	23.439309
109.991858	3073.275732	23.444327
110.267501	3082.619178	23.449344
109.920674	3077.882274	23.454362
110.275196	3092.133827	23.459379
110.475752	3096.038359	23.464397
110.575622	3106.368644	23.469415
110.955879	3103.996085	23.474432
110.918795	3122.534675	23.479450
111.062311	3117.610954	23.484467
111.591829	3128.376182	23.489485
111.639620	3122.305909	23.494503
111.346070	3128.575565	23.499520
111.396252	3132.686572	23.504538
111.523619	3148.946114	23.509555
111.590766	3149.052515	23.514573
112.090625	3143.041254	23.519591
112.574051	3139.544827	23.524608
112.503298	3143.980810	23.529626
112.399619	3144.369454	23.534643
112.890778	3132.034676	23.539661
112.405011	3147.588021	23.544679
112.750917	3150.226421	23.549696
112.817864	3162.064181	23.554714
112.756635	3160.489416	23.559731
113.137758	3168.150049	23.564749
113.020554	3173.357054	23.569767
113.127786	3168.966041	23.574784
113.216069	3183.663103	23.579802
113.506917	3196.592765	23.584819
113.693428	3196.529088	23.589837
113.649426	3200.900953	23.594855
113.664271	3191.038956	23.599872
113.948335	3197.231330	23.604890
114.065571	3209.171756	23.609907
114.429490	3220.464648	23.614925
114.298251	3218.897622	23.619943
114.418806	3208.810852	23.624960
114.542849	3214.406387	23.629978
114.209494	3224.179274	23.634995
114.497060	3215.246895	23.640013
114.444460	3246.646139	23.645031
115.017709	3237.517775	23.650048
115.404639	3227.588359	23.655066
114.911580	3227.573676	23.660083
115.055189	3236.577960	23.665101
115.485824	3248.684235	23.670119
115.767177	3253.037019	23.675136
115.949512	3260.687611	23.680154
115.966667	3256.679871	23.685171
115.898486	3252.335085	23.690189
115.977370	3248.210427	23.695207
116.289071	3256.210145	23.700224
116.248257	3246.508279	23.705242
115.835827	3257.524391	23.710259
116.669092	3263.419820	23.715277
116.317547	3285.624482	23.720295
116.578501	3279.899707	23.725312
116.476350	3276.800571	23.730330
116.645781	3277.127760	23.735347
117.080831	3278.489841	23.740365
116.780017	3296.492095	23.745383
117.357982	3304.024299	23.750400
117.568558	3304.575482	23.755418
117.622281	3300.325327	23.760435
118.026992	3294.391952	23.765453
117.680382	3306.934893	23.770471
117.819926	3298.420038	23.775488
117.965760	3292.930956	23.780506
118.206389	3304.132631	23.785523
118.115809	3318.933398	23.790541
117.830944	3321.493285	23.795559
118.205976	3321.690624	23.800576
118.442569	3317.453023	23.805594
118.254626	3340.361353	23.810611
118.706040	3346.196326	23.815629
118.814803	3351.147270	23.820647
118.968097	3341.001675	23.825664
118.969984	3349.573593	23.830682
118.788371	3363.668965	23.835699
119.434478	3361.264451	23.840717
119.352530	3360.936423	23.845735
119.358468	3358.413803	23.850752
119.880511	3369.426521	23.855770
120.001886	3380.365912	23.860787
120.011698	3382.706339	23.865805
120.028759	3384.660586	23.870823
120.211895	3381.097245	23.875840
120.224157	3387.518216	23.880858
120.303270	3384.649646	23.885875
120.620742	3384.114248	23.890893
120.870535	3398.372881	23.895911
121.072271	3396.305822	23.900928
121.471489	3406.501301	23.905946
121.006416	3398.367744	23.910963
121.644277	3397.293257	23.915981
121.339774	3404.489471	23.920999
121.273412	3397.998171	23.926016
121.408349	3404.901880	23.931034
121.425632	3418.382437	23.936051
121.920851	3424.482047	23.941069
122.080700	3421.963861	23.946087
121.584714	3421.356272	23.951104
122.022151	3433.142839	23.956122
121.771968	3440.078116	23.961139
121.908664	3443.465585	23.966157
122.408727	3450.353495	23.971175
122.797077	3460.913657	23.976192
123.137223	3465.061656	23.981210
123.233822	3477.459963	23.986227
122.746283	3465.081650	23.991245
122.766305	3468.594599	23.996263
123.168767	3463.759871	24.001280
123.339611	3473.031464	24.006298
123.470241	3485.130953	24.011315
123.748001	3477.667597	24.016333
123.621119	3487.039206	24.021351
124.019988	3479.560150	24.026368
124.525213	3491.954815	24.031386
124.364623	3485.370843	24.036403
124.435354	3484.305744	24.041421
124.416966	3474.641293	24.046439
124.104989	3482.880243	24.051456
124.658400	3499.376764	24.056474
124.208147	3506.264311	24.061491
124.973014	3503.664542	24.066509
125.321532	3507.536659	24.071527
124.791596	3514.313523	24.076544
124.974524	3513.742257	24.081562
125.218136	3525.410722	24.086579
125.486802	3522.458963	24.091597
125.326232	3536.996217	24.096615
125.635084	3533.410117	24.101632
125.887521	3541.113039	24.106650
125.880186	3562.144001	24.111667
125.967981	3558.374535	24.116685
126.176177	3564.774533	24.121703
125.696862	3544.270829	24.126720
126.273412	3551.481427	24.131738
126.230326	3579.240675	24.136755
126.410840	3568.749844	24.141773
126.559600	3594.831711	24.146791
126.816625	3598.705468	24.151808
126.989598	3596.242026	24.156826
126.907665	3599.297443	24.161843
127.157420	3604.030821	24.166861
127.412620	3616.470811	24.171879
127.094154	3617.158026	24.176896
127.690225	3625.738565	24.181914
128.022643	3635.739421	24.186931
128.141187	3631.614813	24.191949
128.218384	3637.287210	24.196967
128.034805	3640.759298	24.201984
128.681414	3634.207409	24.207002
128.732303	3643.327331	24.212019
128.820667	3636.714012	24.217037
129.160209	3639.312445	24.222055
129.039367	3660.326475	24.227072
129.128192	3658.349559	24.232090
128.862089	3665.467305	24.237107
129.352699	3662.866027	24.242125
129.862093	3657.118234	24.247143
129.794979	3659.606391	24.252160
129.871184	3658.925488	24.257178
130.018710	3667.386509	24.262195
129.735703	3678.168104	24.267213
129.854514	3684.200158	24.272231
129.815783	3687.428769	24.277248
130.328296	3688.914540	24.282266
129.954481	3702.377294	24.287283
130.241517	3707.805576	24.292301
130.853804	3713.262127	24.297319
130.708687	3719.117505	24.302336
130.714097	3722.569654	24.307354
130.497290	3726.435147	24.312371
130.948994	3737.948259	24.317389
131.071567	3744.582588	24.322407
131.073823	3753.700668	24.327424
131.578946	3745.172872	24.332442
131.852786	3762.246565	24.337459
132.190837	3760.568552	24.342477
132.325902	3769.157810	24.347495
132.570877	3772.560045	24.352512
132.417552	3765.757059	24.357530
132.866141	3758.282772	24.362547
132.718853	3755.651391	24.367565
132.832548	3757.167698	24.372583
132.949671	3762.732919	24.377600
132.525834	3765.491254	24.382618
133.060750	3779.478549	24.387635
132.842430	3784.013413	24.392653
132.757841	3793.444878	24.397671
133.012841	3800.743513	24.402688
133.189197	3815.683034	24.407706
133.335589	3824.920741	24.412723
133.768965	3825.216316	24.417741
133.705775	3830.115257	24.422759
134.057741	3847.432522	24.427776
134.253529	3848.951837	24.432794
134.423666	3846.188960	24.437811
134.465957	3838.089835	24.442829
134.749060	3843.487209	24.447847
134.605786	3865.104656	24.452864
134.951817	3873.130867	24.457882
134.894938	3871.609020	24.462899
135.043065	3866.261439	24.467917
135.841441	3863.858404	24.472935
135.432235	3875.183702	24.477952
135.749471	3885.433249	24.482970
135.844300	3881.927745	24.487987
136.043382	3875.792634	24.493005
136.410325	3873.854456	24.498023
136.584209	3884.552415	24.503040
136.182154	3889.267411	24.508058
136.343457	3886.218684	24.513075
136.385157	3893.411691	24.518093
136.737176	3902.295485	24.523111
137.040808	3896.999435	24.528128
136.806445	3904.323802	24.533146
136.514205	3905.332039	24.538163
137.306551	3910.511273	24.543181
137.390023	3917.751442	24.548199
137.452747	3920.522422	24.553216
137.747128	3925.179499	24.558234
137.952933	3941.733702	24.563251
138.167220	3942.817736	24.568269
138.571223	3939.882715	24.573287
138.123352	3947.073058	24.578304
138.569393	3943.225643	24.583322
138.875425	3946.817250	24.588339
138.503031	3942.014658	24.593357
138.625429	3953.711742	24.598375
138.773978	3965.057571	24.603392
139.245576	3967.392460	24.608410
139.131601	3970.386647	24.613427
139.340800	3966.898040	24.618445
139.924545	3978.188747	24.623463
139.155121	3982.623243	24.628480
139.646363	3988.430132	24.633498
139.727928	3992.432293	24.638515
139.757571	4010.699436	24.643533
140.418464	4014.567217	24.648551
140.566301	4029.905891	24.653568
140.861307	4020.280731	24.658586
140.218633	4014.500722	24.663603
140.521759	4018.351611	24.668621
140.746469	4033.018656	24.673639
140.556025	4036.087885	24.678656
140.754907	4039.983415	24.683674
141.158734	4052.375316	24.688691
141.331140	4062.404478	24.693709
141.426289	4069.169448	24.698727
141.795719	4079.594044	24.703744
141.556972	4086.268971	24.708762
141.800157	4089.854610	24.713779
141.868547	4092.627891	24.718797
142.303545	4083.732099	24.723815
142.442568	4096.177883	24.728832
142.636525	4109.713514	24.733850
142.808130	4102.531558	24.738867
142.562358	4104.226955	24.743885
142.733820	4100.109783	24.748903
142.558576	4115.107450	24.753920
143.150570	4126.592656	24.758938
143.738761	4126.876759	24.763955
143.088744	4126.141621	24.768973
143.837007	4124.832122	24.773991
143.748682	4144.077281	24.779008
144.324412	4142.990333	24.784026
144.534503	4146.495916	24.789043
144.225507	4153.197587	24.794061
144.643259	4146.094073	24.799079
144.427850	4158.036417	24.804096
144.544635	4147.829771	24.809114
145.014162	4167.164855	24.814131
144.862063	4170.288106	24.819149
145.013444	4167.000997	24.824167
145.375037	4169.596076	24.829184
145.452028	4177.405494	24.834202
145.570907	4189.734539	24.839219
145.506505	4192.348600	24.844237
145.984246	4187.561930	24.849255
145.803370	4202.699423	24.854272
146.202480	4202.956152	24.859290
146.156997	4214.550133	24.864307
146.450125	4217.465197	24.869325
146.504618	4209.553385	24.874343
146.749112	4220.369959	24.879360
146.904397	4235.786555	24.884378
146.690158	4241.750709	24.889395
146.806659	4241.306547	24.894413
147.599372	4253.107780	24.899431
147.404227	4265.993935	24.904448
147.430869	4259.693006	24.909466
147.431944	4257.489806	24.914483
147.943870	4273.071851	24.919501
148.472024	4286.558739	24.924519
148.154611	4289.344771	24.929536
148.239924	4281.579633	24.934554
148.794212	4283.421929	24.939571
148.388770	4299.992718	24.944589
149.112921	4301.836977	24.949607
149.035520	4295.381792	24.954624
149.529183	4299.818560	24.959642
149.792756	4300.494090	24.964659
149.435203	4309.365462	24.969677
149.875756	4307.781913	24.974695
149.746663	4324.963061	24.979712
149.834647	4328.961140	24.984730
150.045593	4328.631681	24.989747
149.659590	4334.325913	24.994765
150.392811	4343.696621	24.999783
150.668038	4355.913061	25.004800
150.336677	4353.234498	25.009818
150.663461	4354.701898	25.014835
150.842995	4376.146601	25.019853
150.910321	4374.213986	25.024871
150.893848	4384.657808	25.029888
151.014146	4391.377950	25.034906
151.062863	4400.366026	25.039923
151.339803	4405.098539	25.044941
151.740300	4407.946416	25.049959
151.792081	4423.849583	25.054976
152.177780	4421.018338	25.059994
152.055382	4424.380047	25.065011
151.999378	4425.158995	25.070029
152.589646	4430.748605	25.075047
152.344710	4443.573199	25.080064
152.840498	4442.069417	25.085082
152.797133	4444.721271	25.090099
153.125116	4452.778959	25.095117
153.157648	4460.140906	25.100135
153.090525	4466.479930	25.105152
153.046916	4473.897925	25.110170
153.424581	4482.222494	25.115187
153.232445	4496.348794	25.120205
153.633992	4502.665365	25.125223
154.044782	4511.878041	25.130240
154.497156	4519.597599	25.135258
154.838764	4510.460475	25.140275
154.521185	4528.949488	25.145293
154.918825	4532.823649	25.150311
154.766851	4538.033303	25.155328
154.912922	4538.967020	25.160346
155.562482	4545.295494	25.165363
155.379680	4562.769302	25.170381
155.590666	4564.725048	25.175399
155.744918	4555.497128	25.180416
155.711928	4572.250062	25.185434
156.231555	4582.736787	25.190451
156.381891	4589.253475	25.195469
156.289333	4589.160648	25.200487
156.192456	4593.001340	25.205504
156.684070	4608.416393	25.210522
156.747758	4604.783031	25.215539
156.977220	4617.252970	25.220557
157.627530	4616.110196	25.225575
157.982821	4613.611920	25.230592
158.048455	4622.764761	25.235610
158.696403	4605.398548	25.240627
158.446907	4614.714078	25.245645
158.386439	4611.374650	25.250663
158.933019	4622.491635	25.255680
158.607859	4608.878357	25.260698
158.991187	4605.687626	25.265715
158.913482	4616.081143	25.270733
159.342766	4610.351837	25.275751
159.230446	4609.583464	25.280768
158.987020	4609.321586	25.285786
159.557356	4607.995568	25.290803
158.964580	4618.605002	25.295821
159.543786	4620.705435	25.300839
159.430614	4641.952983	25.305856
159.661042	4650.360524	25.310874
159.717632	4647.454228	25.315891
159.446350	4659.714927	25.320909
160.215105	4679.982455	25.325927
160.465451	4687.042289	25.330944
160.192762	4692.706364	25.335962
160.748375	4709.714989	25.340979
160.601835	4721.151426	25.345997
160.596083	4717.850805	25.351015
160.910187	4744.069565	25.356032
160.854229	4752.234509	25.361050
161.601655	4755.517671	25.366067
162.114148	4769.401911	25.371085
162.528182	4759.760985	25.376103
162.611237	4761.017009	25.381120
162.992654	4761.020833	25.386138
163.002912	4766.110602	25.391155
163.014160	4760.881918	25.396173
163.033570	4754.509345	25.401191
162.987723	4751.858868	25.406208
163.276918	4770.174747	25.411226
163.515049	4763.613454	25.416243
163.221009	4779.899042	25.421261
163.255568	4787.273432	25.426279
163.578578	4787.993386	25.431296
163.695598	4797.438174	25.436314
164.058324	4805.108684	25.441331
163.876133	4813.006075	25.446349
163.899635	4817.907568	25.451367
164.341854	4825.032276	25.456384
164.296674	4834.944235	25.461402
164.565621	4831.111581	25.466419
165.010182	4845.741901	25.471437
165.015746	4850.169576	25.476455
165.389149	4855.736267	25.481472
165.762631	4860.289736	25.486490
165.695102	4865.508431	25.491507
166.062256	4872.455459	25.496525
165.924053	4869.134399	25.501543
166.287170	4887.151653	25.506560
166.333343	4896.317132	25.511578
166.631159	4900.607781	25.516595
166.496864	4900.161617	25.521613
166.583053	4918.244112	25.526631
166.990357	4925.932985	25.531648
166.908085	4930.273348	25.536666
167.419902	4928.217813	25.541683
167.730696	4950.816955	25.546701
167.602787	4945.294239	25.551719
167.787691	4951.972966	25.556736
168.062448	4965.610290	25.561754
168.656316	4964.741425	25.566771
168.838990	4966.259721	25.571789
169.049056	4967.303442	25.576807
168.989928	4961.277607	25.581824
168.523196	4977.179920	25.586842
169.079518	4982.557193	25.591859
169.128437	4992.432493	25.596877
169.282965	4990.587243	25.601895
169.207454	5004.496924	25.606912
169.369193	5016.668351	25.611930
170.182843	5028.264821	25.616947
170.635294	5034.412675	25.621965
170.325526	5033.807595	25.626983
170.418480	5028.528235	25.632000
170.060341	5039.780021	25.637018
170.551340	5049.441327	25.642035
170.729159	5071.578385	25.647053
170.943423	5076.418683	25.652071
171.228258	5078.890117	25.657088
171.488570	5091.491308	25.662106
171.757082	5091.755760	25.667123
171.961120	5105.290567	25.672141
171.917754	5103.447707	25.677159
172.160471	5115.104714	25.682176
172.074548	5114.341679	25.687194
172.640220	5131.188155	25.692212
172.663189	5129.246584	25.697229
172.473156	5131.428964	25.702247
173.345583	5132.413763	25.707264
173.570458	5155.809342	25.712282
173.387399	5158.798697	25.717300
173.669217	5164.957379	25.722317
173.784423	5157.730127	25.727335
173.628213	5162.186220	25.732352
173.828846	5173.126983	25.737370
173.956856	5175.998468	25.742388
173.936050	5183.346917	25.747405
174.680532	5195.187844	25.752423
174.553422	5202.597042	25.757440
174.444381	5204.659500	25.762458
175.133953	5217.913626	25.767476
174.728118	5225.322037	25.772493
175.293124	5226.626162	25.777511
175.228050	5235.266216	25.782528
175.864104	5249.930180	25.787546
175.846927	5254.295207	25.792564
176.232862	5258.360738	25.797581
176.385991	5268.519830	25.802599
176.535048	5266.293468	25.807616
176.758983	5270.409476	25.812634
176.675842	5276.265175	25.817652
176.849454	5290.148915	25.822669
177.051916	5294.445035	25.827687
176.830637	5299.239568	25.832704
177.443433	5321.725867	25.837722
177.771215	5320.005123	25.842740
178.340226	5311.820179	25.847757
178.172183	5312.777589	25.852775
178.738247	5326.739143	25.857792
178.872199	5341.257241	25.862810
178.929577	5330.371061	25.867828
179.216215	5339.524577	25.872845
178.869257	5342.921417	25.877863
178.906209	5343.165107	25.882880
179.255104	5358.454664	25.887898
179.191822	5360.516329	25.892916
179.511032	5364.399725	25.897933
179.895727	5386.782731	25.902951
180.005960	5378.388255	25.907968
179.963712	5395.474824	25.912986
180.228690	5411.598185	25.918004
180.647667	5413.108138	25.923021
180.568113	5427.182911	25.928039
181.087441	5424.933605	25.933056
181.095873	5440.519290	25.938074
181.160572	5444.502302	25.943092
181.400982	5453.741986	25.948109
181.475924	5465.251730	25.953127
181.512743	5467.045299	25.958144
182.059122	5485.328174	25.963162
182.345266	5493.339179	25.968180
182.593892	5489.143394	25.973197
182.675842	5499.468368	25.978215
183.037564	5507.082515	25.983232
182.842223	5512.589600	25.988250
183.236625	5515.359691	25.993268
183.329371	5518.849089	25.998285
183.578888	5538.961681	26.003303
183.864842	5538.162826	26.008320
183.846220	5545.845675	26.013338
184.191990	5551.366380	26.018356
184.372501	5548.472213	26.023373
184.481892	5553.313184	26.028391
184.573854	5563.289415	26.033408
185.054108	5571.636394	26.038426
184.820778	5588.538248	26.043444
184.951630	5577.829874	26.048461
185.149947	5595.778794	26.053479
185.893192	5601.414398	26.058496
185.728849	5615.060599	26.063514
185.606565	5613.873912	26.068532
186.225817	5621.154454	26.073549
186.603005	5630.994775	26.078567
186.451225	5618.445915	26.083584
186.696390	5632.729128	26.088602
186.515217	5649.240975	26.093620
187.129258	5647.917552	26.098637
186.897274	5656.990988	26.103655
187.327770	5656.873538	26.108672
187.456615	5675.417317	26.113690
187.457678	5679.438697	26.118708
187.764629	5681.780509	26.123725
187.456768	5696.550757	26.128743
187.921577	5700.518881	26.133760
188.164185	5721.844875	26.138778
188.337171	5730.372341	26.143796
188.700455	5731.035561	26.148813
189.043512	5748.630657	26.153831
189.365630	5745.660750	26.158848
189.694208	5746.881774	26.163866
189.819816	5765.056829	26.168884
190.124441	5766.710879	26.173901
190.093233	5768.770752	26.178919
190.767635	5771.206884	26.183936
190.207238	5772.465303	26.188954
190.620163	5785.478825	26.193972
190.748882	5787.599029	26.198989
190.947082	5796.599246	26.204007
191.021733	5803.352272	26.209024
191.057471	5818.002835	26.214042
191.456094	5824.342422	26.219060
191.616458	5830.532865	26.224077
191.447686	5848.324538	26.229095
191.994969	5851.598030	26.234112
191.905844	5870.264328	26.239130
192.042946	5880.211609	26.244148
192.453588	5886.681923	26.249165
192.687023	5899.205788	26.254183
193.161185	5918.068532	26.259200
193.227273	5922.060902	26.264218
193.309044	5919.709203	26.269236
193.348516	5929.460218	26.274253
193.840488	5943.070771	26.279271
193.717309	5945.801559	26.284288
194.024311	5965.596325	26.289306
194.452124	5973.872739	26.294324
194.868204	5977.387644	26.299341
194.848117	5992.918266	26.304359
194.992569	5998.006427	26.309376
195.194748	5996.276766	26.314394
195.283901	6018.084708	26.319412
195.848142	6022.321519	26.324429
195.886047	6027.082204	26.329447
196.325785	6038.889058	26.334464
196.309371	6044.292687	26.339482
196.708686	6051.834921	26.344500
196.716617	6043.831706	26.349517
196.467747	6056.288720	26.354535
196.892952	6070.859911	26.359552
197.048977	6074.405853	26.364570
197.474723	6095.811097	26.369588
197.486539	6101.639651	26.374605
197.367343	6107.946316	26.379623
197.721821	6118.557502	26.384640
198.045788	6116.196481	26.389658
198.057067	6138.067196	26.394676
198.485801	6149.440218	26.399693
198.782461	6155.716879	26.404711
199.023871	6164.925203	26.409728
199.271317	6172.541638	26.414746
198.999509	6176.548791	26.419764
199.745023	6182.673507	26.424781
199.701293	6199.508527	26.429799
199.717317	6203.335137	26.434816
200.040710	6208.332365	26.439834
200.383468	6220.792081	26.444852
200.736434	6217.757319	26.449869
200.832366	6218.954621	26.454887
200.818108	6225.175542	26.459904
201.332287	6241.033562	26.464922
200.878437	6254.112920	26.469940
201.370471	6247.110669	26.474957
201.519069	6268.082608	26.479975
201.809100	6277.147682	26.484992
201.967477	6284.124601	26.490010
202.380332	6303.104616	26.495028
202.685997	6292.883145	26.500045
202.510294	6299.066093	26.505063
202.751940	6322.997196	26.510080
203.207312	6324.741470	26.515098
203.617024	6324.778775	26.520116
203.858356	6334.583810	26.525133
203.973927	6332.220482	26.530151
204.217557	6324.385632	26.535168
204.430466	6323.029915	26.540186
204.468642	6338.157175	26.545204
204.922170	6351.938168	26.550221
204.836184	6356.831868	26.555239
205.098098	6356.058819	26.560256
205.674993	6366.913311	26.565274
205.289344	6378.732091	26.570292
205.958961	6370.313204	26.575309
205.824048	6388.797758	26.580327
205.940972	6396.990186	26.585344
206.275393	6402.834901	26.590362
206.442894	6422.153124	26.595380
206.525841	6418.958340	26.600397
207.038933	6437.234729	26.605415
207.209325	6447.991565	26.610432
207.222204	6454.047348	26.615450
207.220508	6461.235502	26.620468
207.406037	6471.447042	26.625485
207.733807	6485.465528	26.630503
207.948672	6496.247036	26.635520
208.208728	6506.469090	26.640538
208.345294	6526.066873	26.645556
208.700147	6524.846878	26.650573
208.960469	6536.464175	26.655591
209.023970	6536.018741	26.660608
209.493213	6555.605799	26.665626
209.712173	6560.338435	26.670644
209.894938	6565.389222	26.675661
210.156075	6590.564546	26.680679
209.937245	6594.020585	26.685696
210.261084	6597.089091	26.690714
210.313282	6618.824585	26.695732
210.589123	6615.448213	26.700749
210.765856	6628.713768	26.705767
211.192489	6634.720978	26.710784
211.436293	6650.081647	26.715802
211.546186	6656.516985	26.720820
211.474715	6666.380368	26.725837
211.996868	6685.381644	26.730855
212.512661	6688.878009	26.735872
213.134993	6693.595230	26.740890
213.028646	6715.677511	26.745908
212.786055	6715.746926	26.750925
213.050624	6721.021777	26.755943
213.544441	6724.628899	26.760960
213.599358	6725.100254	26.765978
213.633345	6731.288582	26.770996
213.731720	6738.732745	26.776013
213.908553	6748.598552	26.781031
214.129739	6755.733181	26.786048
214.369165	6764.459133	26.791066
214.427458	6789.189641	26.796084
215.124343	6793.885812	26.801101
214.721252	6809.966054	26.806119
215.286760	6817.132333	26.811136
215.876213	6819.401901	26.816154
216.268746	6829.897090	26.821172
216.346557	6827.571145	26.826189
215.997088	6836.281486	26.831207
216.227559	6850.302774	26.836224
216.387448	6855.562393	26.841242
216.888894	6871.306144	26.846260
216.953752	6878.417807	26.851277
217.243309	6900.672274	26.856295
217.215236	6917.625474	26.861312
217.831141	6929.241327	26.866330
217.735020	6941.987682	26.871348
218.494036	6941.146687	26.876365
218.724112	6960.455737	26.881383
218.921374	6967.969831	26.886400
219.016975	6963.002023	26.891418
219.186019	6973.270076	26.896436
219.613407	6969.677481	26.901453
219.868602	6971.260420	26.906471
219.844947	6990.287011	26.911488
220.644559	6987.621382	26.916506
220.210333	7009.698240	26.921524
221.118546	7016.760734	26.926541
220.952685	7026.111820	26.931559
221.163782	7023.926097	26.936576
221.320504	7014.996447	26.941594
221.542439	7035.408566	26.946612
221.814315	7047.693631	26.951629
221.796078	7047.327203	26.956647
222.024975	7060.019882	26.961664
222.692717	7073.651269	26.966682
223.044514	7077.526804	26.971700
222.659196	7078.347664	26.976717
222.807951	7104.175710	26.981735
222.565953	7111.161613	26.986752
223.137759	7112.837328	26.991770
223.047915	7130.134964	26.996788
223.411138	7143.671756	27.001805
223.967106	7161.200342	27.006823
223.957435	7175.997963	27.011840
224.363366	7181.547681	27.016858
224.331934	7210.352405	27.021876
224.594989	7216.760938	27.026893
224.882649	7230.641026	27.031911
225.451159	7244.483714	27.036928
225.494702	7252.309129	27.041946
225.642217	7271.211500	27.046964
226.238376	7286.868256	27.051981
226.403164	7287.480362	27.056999
226.323594	7303.049767	27.062016
227.173144	7312.211344	27.067034
226.754976	7320.538002	27.072052
226.750166	7332.244435	27.077069
227.208603	7345.940180	27.082087
227.191199	7364.868324	27.087104
228.071543	7365.706813	27.092122
228.360371	7374.052857	27.097140
228.530285	7383.238201	27.102157
228.736990	7400.120569	27.107175
228.876381	7396.133926	27.112192
229.417849	7406.334770	27.117210
229.264272	7417.199437	27.122228
229.337169	7424.710983	27.127245
229.783550	7426.169491	27.132263
229.726993	7444.478752	27.137280
230.474084	7442.771455	27.142298
230.496768	7450.183495	27.147316
230.386063	7461.284593	27.152333
230.539733	7462.750793	27.157351
230.878613	7480.512366	27.162368
231.330804	7480.839812	27.167386
231.363163	7505.262791	27.172404
231.639558	7517.951550	27.177421
232.080896	7520.095894	27.182439
232.474094	7534.035547	27.187456
232.738564	7535.926466	27.192474
232.793828	7545.767433	27.197492
232.638217	7553.636610	27.202509
233.131947	7560.729121	27.207527
233.381518	7569.532801	27.212544
233.136923	7581.257783	27.217562
233.597600	7589.864448	27.222580
233.681807	7616.255721	27.227597
234.049759	7621.871467	27.232615
234.219265	7647.927501	27.237632
234.752063	7659.670406	27.242650
234.826359	7666.099013	27.247668
235.199870	7687.766807	27.252685
235.725922	7698.677363	27.257703
235.366665	7710.423435	27.262720
236.186467	7713.496996	27.267738
236.646382	7732.196516	27.272756
236.299057	7739.754672	27.277773
237.049650	7752.271902	27.282791
237.312296	7753.759042	27.287808
237.189466	7761.083370	27.292826
237.216433	7775.758963	27.297844
237.427712	7789.929175	27.302861
237.991535	7796.751998	27.307879
238.374360	7801.942455	27.312896
238.957234	7811.739305	27.317914
238.778126	7823.810980	27.322932
238.723793	7833.388196	27.327949
239.407975	7835.860975	27.332967
239.456863	7850.972030	27.337984
239.669885	7852.678419	27.343002
240.124304	7867.413814	27.348020
239.870704	7879.165643	27.353037
240.573540	7890.326601	27.358055
240.856843	7897.783485	27.363072
240.790654	7902.194657	27.368090
240.935413	7912.302855	27.373108
241.066682	7930.993761	27.378125
241.403848	7939.600878	27.383143
241.765745	7947.733762	27.388160
241.970256	7956.626724	27.393178
242.265524	7971.172307	27.398196
242.415338	7980.370551	27.403213
242.592461	7994.413647	27.408231
242.403248	8004.229781	27.413248
243.273355	8027.610664	27.418266
243.687522	8035.593385	27.423284
243.605028	8057.853511	27.428301
243.952091	8062.506610	27.433319
243.994441	8075.295331	27.438336
244.554676	8084.413944	27.443354
244.547201	8083.910070	27.448372
244.971951	8097.898908	27.453389
244.936925	8103.940594	27.458407
245.350765	8116.008540	27.463424
245.491466	8132.955527	27.468442
245.890237	8142.007754	27.473460
245.924933	8152.351052	27.478477
246.013443	8152.823528	27.483495
246.293804	8165.322697	27.488512
246.607928	8177.680867	27.493530
247.204864	8193.628722	27.498548
246.844631	8214.129629	27.503565
247.329842	8212.665086	27.508583
248.107254	8234.308527	27.513600
247.853722	8234.351234	27.518618
248.575573	8251.394116	27.523636
248.188469	8273.866090	27.528653
248.999767	8263.896294	27.533671
248.803705	8291.888575	27.538688
249.291366	8304.573399	27.543706
249.597835	8316.421417	27.548724
249.584154	8327.687881	27.553741
250.283355	8338.704457	27.558759
250.322762	8338.985690	27.563776
250.855767	8354.470084	27.568794
250.994926	8358.893594	27.573812
251.022136	8367.097713	27.578829
251.120774	8375.555905	27.583847
251.342353	8393.544988	27.588864
251.740295	8411.980186	27.593882
251.864788	8415.790370	27.598900
251.762448	8431.743118	27.603917
252.925127	8435.233822	27.608935
253.046994	8460.553361	27.613952
253.351051	8467.824136	27.618970
253.196113	8473.673090	27.623988
253.732426	8487.692211	27.629005
254.684498	8481.586712	27.634023
254.805958	8491.465234	27.639040
254.648829	8508.537860	27.644058
255.339534	8510.274126	27.649076
254.960833	8511.633870	27.654093
255.657276	8525.211359	27.659111
255.486037	8533.282280	27.664128
255.656424	8534.512342	27.669146
256.283880	8553.224498	27.674164
256.122806	8563.424867	27.679181
256.559928	8574.971732	27.684199
256.551741	8581.451385	27.689216
256.340573	8599.425958	27.694234
256.982114	8619.282005	27.699252
257.072282	8643.186046	27.704269
257.714979	8654.530473	27.709287
257.848765	8667.999927	27.714304
258.254083	8679.412898	27.719322
258.400677	8698.499989	27.724340
258.364645	8711.468679	27.729357
259.071645	8724.280656	27.734375
258.979535	8743.086090	27.739392
259.501507	8760.147933	27.744410
259.477489	8770.267093	27.749428
260.094225	8790.124029	27.754445
260.059132	8789.877004	27.759463
260.183347	8808.156317	27.764480
260.707473	8816.854708	27.769498
261.201710	8835.701548	27.774516
261.305391	8850.984846	27.779533
261.561539	8859.759707	27.784551
262.013771	8865.498470	27.789568
262.184259	8883.224472	27.794586
262.588811	8885.920890	27.799604
262.679526	8888.842966	27.804621
262.972073	8903.121354	27.809639
262.934553	8910.934837	27.814656
263.156128	8917.836620	27.819674
263.629874	8931.256495	27.824692
263.267951	8941.598841	27.829709
263.926360	8960.925390	27.834727
264.315394	8978.620616	27.839744
264.898740	8991.054232	27.844762
265.155926	8998.190443	27.849780
264.803823	9013.061792	27.854797
265.587686	9024.302386	27.859815
265.766625	9042.674439	27.864832
265.836564	9062.765184	27.869850
266.287543	9073.596689	27.874868
266.279056	9077.468756	27.879885
267.001662	9089.078841	27.884903
266.724957	9103.755409	27.889920
266.953895	9126.318779	27.894938
267.801528	9132.406498	27.899956
267.426769	9152.146671	27.904973
268.177761	9156.626662	27.909991
268.258392	9163.891454	27.915008
268.782778	9183.024414	27.920026
269.694311	9189.474750	27.925044
269.598685	9202.251003	27.930061
269.623103	9209.628751	27.935079
270.322519	9213.090705	27.940096
270.527887	9232.525957	27.945114
270.726988	9231.765731	27.950132
270.642386	9243.460542	27.955149
271.281330	9253.416765	27.960167
271.532216	9258.410332	27.965184
271.618013	9267.110878	27.970202
271.975835	9284.151405	27.975220
272.026070	9289.741355	27.980237
272.728514	9307.703822	27.985255
273.244498	9314.784079	27.990272
272.725293	9319.174558	27.995290
273.328166	9335.608687	28.000308
273.713507	9348.534322	28.005325
274.123981	9360.616238	28.010343
274.506902	9370.255620	28.015360
273.972687	9374.493746	28.020378
274.506201	9394.228530	28.025396
274.729151	9404.397988	28.030413
275.272340	9413.346271	28.035431
275.385307	9422.907735	28.040448
275.794807	9449.996086	28.045466
275.933055	9452.213107	28.050484
275.999048	9471.645051	28.055501
276.215842	9478.083677	28.060519
276.551178	9502.458971	28.065536
276.622548	9510.710394	28.070554
277.066871	9528.489099	28.075572
277.639742	9544.836525	28.080589
277.840052	9555.151667	28.085607
278.299920	9561.100994	28.090624
278.596985	9585.646531	28.095642
278.841708	9591.859842	28.100660
279.090380	9608.573522	28.105677
279.136087	9620.870259	28.110695
279.247665	9625.942445	28.115712
279.376504	9641.847613	28.120730
280.365129	9643.979625	28.125748
280.323448	9666.099567	28.130765
280.544742	9678.523711	28.135783
280.891869	9693.454078	28.140800
280.661966	9701.563055	28.145818
280.869274	9719.925049	28.150836
281.341987	9736.783928	28.155853
281.551006	9747.659814	28.160871
282.201233	9767.645193	28.165888
282.142941	9786.616912	28.170906
282.716955	9796.002600	28.175924
282.650377	9815.925977	28.180941
282.773596	9835.589346	28.185959
283.554865	9849.385088	28.190976
283.606641	9873.293535	28.195994
283.953148	9882.200049	28.201012
284.188457	9895.487254	28.206029
284.486023	9911.991529	28.211047
285.040346	9926.113131	28.216064
285.145326	9943.531459	28.221082
285.892560	9949.464590	28.226100
285.930066	9967.468074	28.231117
286.313816	9969.508015	28.236135
286.922048	9984.511629	28.241152
286.858550	9995.704772	28.246170
287.275638	10014.514309	28.251188
287.705107	10019.259267	28.256205
288.169452	10035.131483	28.261223
288.529617	10038.990559	28.266240
288.421500	10043.355093	28.271258
288.798726	10060.377527	28.276276
289.052674	10064.212100	28.281293
289.257921	10073.664813	28.286311
289.745518	10086.900248	28.291328
289.817540	10093.001692	28.296346
290.259917	10104.037211	28.301364
290.437986	10107.725740	28.306381
290.502804	10134.439355	28.311399
290.642717	10139.980870	28.316416
290.919164	10161.300428	28.321434
291.087186	10174.813007	28.326452
291.640132	10195.151828	28.331469
292.238220	10204.161411	28.336487
292.320204	10217.299062	28.341504
292.361765	10249.876497	28.346522
292.785090	10254.309895	28.351540
293.229312	10274.293162	28.356557
293.103308	10287.681102	28.361575
293.436630	10301.382738	28.366592
293.839770	10331.643355	28.371610
293.721882	10347.840128	28.376628
295.311368	10357.080637	28.381645
295.734686	10364.750366	28.386663
296.004422	10370.407505	28.391680
296.243748	10382.538835	28.396698
296.436363	10380.895510	28.401716
296.492084	10394.141568	28.406733
296.954399	10405.129959	28.411751
297.301299	10414.371350	28.416768
297.540780	10424.055715	28.421786
297.308987	10424.991734	28.426804
297.556582	10427.434967	28.431821
297.618015	10456.217655	28.436839
298.197772	10462.344368	28.441856
298.237912	10489.422276	28.446874
298.584537	10494.938030	28.451892
299.156182	10515.365855	28.456909
299.525875	10538.512090	28.461927
299.989640	10550.681209	28.466944
299.962332	10563.520380	28.471962
300.169281	10573.869785	28.476980
300.642414	10585.064987	28.481997
300.499604	10605.951456	28.487015
300.926124	10621.792174	28.492032
300.981301	10638.483228	28.497050
301.201128	10662.663323	28.502068
301.605987	10677.108723	28.507085
301.889497	10695.889226	28.512103
302.360148	10711.202174	28.517120
302.507477	10736.593474	28.522138
302.851354	10758.960959	28.527156
303.560131	10765.986500	28.532173
304.007892	10784.293165	28.537191
304.409334	10794.883954	28.542208
304.949788	10803.482861	28.547226
305.006251	10803.268916	28.552244
305.290333	10824.979569	28.557261
305.433209	10831.894318	28.562279
306.134901	10842.195266	28.567296
306.266617	10860.516478	28.572314
306.558949	10876.217273	28.577332
306.939325	10877.171677	28.582349
306.779745	10890.505283	28.587367
307.318872	10899.843287	28.592384
307.435865	10932.208092	28.597402
308.000460	10935.978696	28.602420
308.644070	10959.966901	28.607437
308.325178	10965.816901	28.612455
309.126501	10971.599856	28.617472
309.211377	10997.800075	28.622490
309.443784	11013.103000	28.627508
309.958550	11030.310145	28.632525
309.952156	11043.045350	28.637543
310.302505	11055.920788	28.642560
310.626858	11076.280375	28.647578
310.716397	11087.377725	28.652596
310.795573	11115.779768	28.657613
311.240072	11139.360310	28.662631
311.396558	11151.587133	28.667648
311.550229	11177.577970	28.672666
311.960733	11202.388997	28.677684
312.740108	11225.993294	28.682701
312.874442	11241.014868	28.687719
313.595434	11258.136440	28.692736
313.927883	11282.858685	28.697754
314.210823	11294.257588	28.702772
314.509797	11312.319546	28.707789
314.570024	11331.545930	28.712807
315.107277	11334.619900	28.717824
315.305001	11363.025965	28.722842
315.826817	11376.651685	28.727860
316.248162	11392.853823	28.732877
316.481700	11409.764087	28.737895
316.700532	11426.771382	28.742912
317.158976	11445.389630	28.747930
317.251663	11467.102408	28.752948
317.637084	11474.058574	28.757965
317.417614	11502.084585	28.762983
318.190848	11514.262990	28.768000
319.161755	11519.066133	28.773018
319.838489	11537.015818	28.778036
320.126561	11536.456366	28.783053
319.724220	11551.883813	28.788071
320.484612	11563.015937	28.793088
320.378175	11570.831791	28.798106
320.997768	11579.384005	28.803124
322.330391	11569.318670	28.808141
321.814751	11568.666469	28.813159
322.700792	11564.123792	28.818176
322.399112	11566.747417	28.823194
322.569414	11573.190851	28.828212
323.041684	11591.147160	28.833229
323.328131	11602.406772	28.838247
323.218356	11608.123372	28.843264
323.736266	11622.113001	28.848282
323.330845	11624.639111	28.853300
323.686736	11643.172481	28.858317
324.103884	11667.588393	28.863335
324.342043	11686.620088	28.868352
324.613633	11705.343469	28.873370
324.710318	11721.637486	28.878388
325.127983	11738.604637	28.883405
325.345497	11759.767844	28.888423
326.274518	11782.077033	28.893440
326.206060	11796.745396	28.898458
326.496034	11823.217969	28.903476
327.075527	11837.109759	28.908493
327.546030	11862.689095	28.913511
327.937101	11874.008366	28.918528
328.231670	11896.432253	28.923546
328.372143	11919.742192	28.928564
328.615130	11937.260884	28.933581
328.726627	11963.524618	28.938599
329.104408	11979.171988	28.943616
329.478610	12003.478191	28.948634
329.846934	12021.350051	28.953652
330.333237	12041.881250	28.958669
330.674910	12067.048324	28.963687
331.497332	12073.194630	28.968704
331.653624	12095.046643	28.973722
332.198067	12114.012142	28.978740
332.901432	12122.879962	28.983757
333.084728	12129.675223	28.988775
333.343552	12149.345177	28.993792
333.703599	12152.756325	28.998810
333.612031	12166.986501	29.003828
334.277949	12179.065216	29.008845
333.725151	12197.876382	29.013863
334.622041	12207.487744	29.018880
334.837920	12224.666738	29.023898
335.318050	12248.366281	29.028916
335.633513	12263.695191	29.033933
336.172999	12285.964580	29.038951
336.351584	12302.830524	29.043968
336.847080	12324.696307	29.048986
336.879189	12342.178738	29.054004
337.104752	12351.765224	29.059021
337.253371	12385.333856	29.064039
337.457458	12399.565544	29.069056
337.834675	12420.657268	29.074074
338.174859	12453.324668	29.079092
338.876337	12474.571221	29.084109
338.988471	12498.931496	29.089127
339.387282	12513.009804	29.094144
340.202516	12538.530078	29.099162
340.169713	12550.152577	29.104180
340.904017	12568.681631	29.109197
340.846554	12596.450376	29.114215
341.401139	12609.525604	29.119232
341.533926	12628.325196	29.124250
341.951199	12657.924247	29.129268
342.437028	12668.335601	29.134285
342.357753	12680.445395	29.139303
342.991411	12711.090796	29.144320
342.962189	12715.977329	29.149338
343.600430	12737.676113	29.154356
344.039278	12755.168233	29.159373
344.232362	12768.520895	29.164391
344.747043	12790.368445	29.169408
344.731147	12812.904916	29.174426
345.315306	12825.710436	29.179444
345.693307	12845.479402	29.184461
345.819977	12864.962265	29.189479
346.185331	12891.194088	29.194496
346.811292	12901.091139	29.199514
346.425445	12928.150467	29.204532
347.119892	12940.405228	29.209549
347.300983	12966.192171	29.214567
347.944071	12988.929409	29.219584
348.513261	13005.795171	29.224602
348.355752	13035.465352	29.229620
349.297321	13055.165748	29.234637
349.338173	13073.999044	29.239655
349.588164	13095.329220	29.244672
350.005955	13117.081709	29.249690
350.594262	13140.244492	29.254708
350.867222	13154.377609	29.259725
351.346393	13167.878643	29.264743
351.481045	13190.240550	29.269760
352.209996	13200.301723	29.274778
352.337188	13232.021542	29.279796
352.839058	13249.144315	29.284813
353.317783	13272.535897	29.289831
353.527904	13291.002008	29.294848
353.986614	13307.768399	29.299866
353.866422	13331.073297	29.304884
354.169781	13342.634476	29.309901
354.912031	13372.136687	29.314919
355.430217	13393.027554	29.319936
356.101494	13399.036781	29.324954
355.662078	13429.818832	29.329972
356.451495	13454.248583	29.334989
356.775130	13473.211936	29.340007
357.438101	13489.207742	29.345024
357.642303	13504.324457	29.350042
357.771586	13537.004463	29.355060
358.113942	13541.002833	29.360077
358.239524	13561.396059	29.365095
358.495434	13585.681668	29.370112
358.879651	13603.347293	29.375130
359.556274	13635.503307	29.380148
359.764812	13655.650034	29.385165
359.980321	13672.344084	29.390183
360.338765	13698.754950	29.395200
360.765637	13711.595035	29.400218
360.891191	13740.824354	29.405236
361.181048	13772.990287	29.410253
361.806716	13801.339723	29.415271
361.853144	13820.371844	29.420288
362.475634	13849.302909	29.425306
363.304523	13870.831210	29.430324
364.115572	13886.308501	29.435341
364.424397	13898.102859	29.440359
365.030481	13912.557321	29.445376
365.406212	13913.402084	29.450394
365.415163	13942.536180	29.455412
365.804164	13951.090643	29.460429
366.092224	13969.958978	29.465447
366.550496	13976.961577	29.470464
367.123834	13985.645257	29.475482
367.108726	13998.683823	29.480500
367.154096	14018.553172	29.485517
367.679975	14036.967696	29.490535
367.918708	14058.174392	29.495552
368.479303	14074.802442	29.500570
368.629874	14089.324797	29.505588
368.749646	14102.945613	29.510605
369.007901	14126.208360	29.515623
369.060722	14152.152683	29.520640
369.476374	14169.706571	29.525658
369.517765	14200.958195	29.530676
370.377200	14217.751433	29.535693
370.346247	14239.578234	29.540711
370.819755	14280.558894	29.545728
371.606166	14301.923767	29.550746
371.541654	14329.222445	29.555764
371.916165	14351.368373	29.560781
372.537490	14381.626809	29.565799
372.452104	14414.066996	29.570816
373.828196	14445.360718	29.575834
373.980056	14472.726975	29.580852
374.239160	14485.745291	29.585869
374.640841	14517.137144	29.590887
374.949428	14536.504978	29.595904
375.619231	14559.729450	29.600922
375.900524	14582.316499	29.605940
376.331130	14601.245380	29.610957
376.687429	14626.230419	29.615975
376.679806	14649.342556	29.620992
377.240175	14678.031911	29.626010
377.514658	14701.829711	29.631028
378.254857	14726.199291	29.636045
378.662939	14750.159523	29.641063
378.950856	14778.130342	29.646080
379.282207	14792.227168	29.651098
379.973545	14816.294976	29.656116
380.355448	14845.741893	29.661133
380.410619	14863.782047	29.666151
380.527902	14895.026153	29.671168
381.169599	14914.993089	29.676186
381.682049	14946.431568	29.681204
382.211768	14968.595108	29.686221
382.914408	14979.498238	29.691239
383.224999	15005.589925	29.696256
383.237182	15019.487115	29.701274
383.932575	15043.823022	29.706292
384.875222	15059.369217	29.711309
385.510432	15064.939295	29.716327
385.296874	15084.420558	29.721344
386.330287	15090.342371	29.726362
386.153159	15107.177763	29.731380
386.666300	15128.911403	29.736397
386.708126	15147.102337	29.741415
386.750065	15172.345473	29.746432
387.199048	15189.891957	29.751450
387.312030	15217.546415	29.756468
387.833418	15232.855149	29.761485
388.265008	15256.079659	29.766503
388.400313	15286.611009	29.771520
389.042351	15315.797081	29.776538
389.405844	15343.141116	29.781556
390.007639	15369.333243	29.786573
390.726911	15388.988571	29.791591
390.462762	15413.736465	29.796608
391.219423	15422.625975	29.801626
391.643081	15449.528120	29.806644
391.619288	15467.947493	29.811661
391.623307	15495.177164	29.816679
392.467182	15521.672902	29.821696
393.026597	15543.159785	29.826714
393.578266	15570.297988	29.831732
393.651371	15590.369944	29.836749
394.537248	15602.024992	29.841767
394.268349	15630.055323	29.846784
394.809708	15652.985302	29.851802
395.054415	15665.100249	29.856820
395.083691	15697.477391	29.861837
395.666833	15710.060791	29.866855
395.746900	15742.970166	29.871872
396.108670	15766.294600	29.876890
396.839166	15809.790427	29.881908
397.296603	15837.237399	29.886925
397.898959	15855.509133	29.891943
398.176075	15895.080504	29.896960
398.643563	15907.571499	29.901978
399.095429	15935.894329	29.906996
399.389841	15958.859963	29.912013
400.001475	15986.204186	29.917031
400.409822	16001.167931	29.922048
400.958964	16011.564956	29.927066
401.919675	16041.678446	29.932084
401.757711	16067.974644	29.937101
402.794077	16086.583297	29.942119
402.613446	16108.252352	29.947136
402.834535	16130.370541	29.952154
403.210429	16159.728829	29.957172
403.838408	16174.317417	29.962189
404.202200	16202.834379	29.967207
404.502888	16218.832042	29.972224
404.737651	16236.087529	29.977242
405.388822	16283.086758	29.982260
405.892049	16304.204242	29.987277
406.070958	16325.912320	29.992295
406.201668	16353.887812	29.997312
406.928126	16372.355489	30.002330
407.243880	16399.121009	30.007348
407.832178	16435.938323	30.012365
408.367612	16456.239257	30.017383
408.752023	16477.362796	30.022400
409.060623	16500.029981	30.027418
408.992260	16521.735716	30.032436
409.393144	16554.018552	30.037453
409.822523	16587.332963	30.042471
410.360944	16620.084050	30.047488
410.764969	16646.946718	30.052506
411.464550	16669.749057	30.057524
412.036715	16703.319381	30.062541
412.394921	16734.048901	30.067559
412.863574	16759.265597	30.072576
412.981488	16780.942625	30.077594
413.983746	16801.092288	30.082612
414.394352	16818.020871	30.087629
415.245340	16833.705968	30.092647
415.267335	16863.313094	30.097664
415.840844	16879.445708	30.102682
416.091849	16891.863663	30.107700
416.466413	16923.721667	30.112717
416.714258	16948.028606	30.117735
416.845316	16965.689386	30.122752
417.035488	16996.151746	30.127770
418.203814	17007.931086	30.132788
418.072986	17039.801635	30.137805
418.612185	17070.831998	30.142823
418.785864	17098.741873	30.147840
419.694772	17131.587764	30.152858
419.865550	17146.033493	30.157876
420.354590	17179.544945	30.162893
420.689400	17205.500044	30.167911
420.852012	17226.857923	30.172928
421.285747	17242.093476	30.177946
421.492702	17274.328749	30.182964
422.384361	17302.515642	30.187981
422.716584	17320.590782	30.192999
423.265075	17341.626557	30.198016
423.359430	17365.259883	30.203034
423.803490	17385.121196	30.208052
423.851826	17404.655635	30.213069
424.204067	17434.515445	30.218087
425.035879	17462.307596	30.223104
425.514117	17496.039220	30.228122
425.823801	17527.301881	30.233140
425.957076	17563.023525	30.238157
426.576810	17582.478664	30.243175
427.176476	17611.027324	30.248192
427.382800	17641.753511	30.253210
427.829121	17667.818216	30.258228
428.373593	17704.417364	30.263245
428.628552	17726.949050	30.268263
429.427560	17755.081542	30.273280
429.692409	17781.174651	30.278298
430.277725	17805.897608	30.283316
430.676487	17838.021838	30.288333
431.029386	17859.098104	30.293351
431.680510	17899.313427	30.298368
432.311339	17926.379468	30.303386
433.311952	17939.319442	30.308404
434.015078	17959.696935	30.313421
433.918892	17979.219709	30.318439
434.081932	18002.315629	30.323456
434.696400	18003.022342	30.328474
435.590158	18023.926146	30.333492
435.441235	18056.849857	30.338509
436.050492	18075.694349	30.343527
436.419382	18097.355895	30.348544
436.752192	18127.368258	30.353562
437.123040	18146.186761	30.358580
437.423167	18173.904779	30.363597
437.700979	18198.505543	30.368615
438.594039	18229.826978	30.373632
438.506757	18248.881154	30.378650
439.721521	18273.614113	30.383668
439.438117	18301.625313	30.388685
440.336738	18332.548055	30.393703
440.235460	18362.034526	30.398720
440.634248	18385.372168	30.403738
441.697383	18411.253407	30.408756
441.950658	18445.113314	30.413773
442.169052	18466.293309	30.418791
442.841530	18495.571082	30.423808
443.490146	18522.470936	30.428826
443.770607	18544.361542	30.433844
444.393820	18573.893484	30.438861
444.800482	18601.627115	30.443879
445.153993	18616.607752	30.448896
445.236974	18653.590098	30.453914
446.088588	18674.084214	30.458932
446.106732	18699.199852	30.463949
446.599879	18727.634078	30.468967
447.104114	18764.089876	30.473984
447.518874	18786.774809	30.479002
448.023327	18821.941905	30.484020
448.604980	18855.820900	30.489037
448.745088	18878.769813	30.494055
449.028334	18915.020230	30.499072
449.453538	18948.519418	30.504090
449.830501	18986.208423	30.509108
450.255202	19014.078823	30.514125
451.097050	19037.019759	30.519143
451.238844	19063.879231	30.524160
451.901050	19092.995248	30.529178
451.993470	19109.608955	30.534196
452.340482	19150.461760	30.539213
453.219899	19177.730923	30.544231
453.968006	19216.436598	30.549248
453.988696	19235.177999	30.554266
454.706591	19257.007628	30.559284
454.846293	19289.345172	30.564301
455.574064	19313.915207	30.569319
456.118911	19339.221335	30.574336
456.539833	19361.615366	30.579354
457.121273	19395.331075	30.584372
457.179444	19422.627349	30.589389
457.691673	19452.575924	30.594407
458.018356	19495.776503	30.599424
458.332821	19522.514961	30.604442
459.374664	19548.780105	30.609460
459.535644	19585.252974	30.614477
460.114010	19616.783588	30.619495
460.661377	19652.280349	30.624512
460.680685	19685.566011	30.629530
461.746214	19705.175011	30.634548
462.064518	19741.592091	30.639565
462.752568	19763.426936	30.644583
463.152608	19787.568434	30.649600
463.803261	19817.388617	30.654618
463.857596	19848.078778	30.659636
464.622888	19881.412906	30.664653
465.283068	19908.249701	30.669671
465.824717	19934.441607	30.674688
465.919289	19966.894704	30.679706
466.586484	19988.707777	30.684724
467.148115	20018.415767	30.689741
467.437726	20050.560651	30.694759
468.819537	20047.395133	30.699776
469.190563	20054.849486	30.704794
469.886869	20065.576442	30.709812
470.574530	20101.096406	30.714829
470.763288	20107.517736	30.719847
471.509263	20130.285352	30.724864
471.556891	20138.200750	30.729882
471.889804	20166.851565	30.734900
472.148679	20173.318864	30.739917
472.623991	20194.302794	30.744935
472.869979	20215.196087	30.749952
472.885530	20257.499090	30.754970
473.336163	20284.154214	30.759988
474.092219	20313.762889	30.765005
474.122280	20348.463244	30.770023
474.886299	20369.863634	30.775040
474.767506	20405.863510	30.780058
475.875226	20438.267071	30.785076
476.138392	20481.782988	30.790093
476.497821	20504.750215	30.795111
477.163412	20542.479431	30.800128
477.545164	20574.989918	30.805146
478.136530	20606.975014	30.810164
478.466727	20646.007631	30.815181
478.711439	20676.751589	30.820199
479.706426	20710.215646	30.825216
479.917307	20742.443423	30.830234
480.869021	20765.874750	30.835252
481.499157	20793.804167	30.840269
482.153041	20818.147513	30.845287
482.189544	20829.900065	30.850304
482.781508	20857.292150	30.855322
483.324313	20887.269758	30.860340
483.937052	20905.674181	30.865357
484.599006	20925.031331	30.870375
484.664354	20949.561236	30.875392
485.213671	20975.519569	30.880410
485.827803	20993.936496	30.885428
486.343137	21017.404468	30.890445
486.571109	21040.525472	30.895463
486.756244	21066.648031	30.900480
487.009047	21105.004919	30.905498
487.655481	21125.653612	30.910516
487.820200	21157.055242	30.915533
488.796049	21192.266955	30.920551
489.622489	21219.382949	30.925568
489.381699	21252.623308	30.930586
490.087081	21279.404404	30.935604
490.077112	21311.496901	30.940621
490.433501	21348.094272	30.945639
490.946037	21391.105825	30.950656
491.225421	21430.286916	30.955674
491.771201	21473.426159	30.960692
493.044287	21519.927400	30.965709
493.416302	21550.772959	30.970727
494.026405	21578.156909	30.975744
494.063187	21617.628877	30.980762
495.080021	21645.259206	30.985780
495.245276	21694.239561	30.990797
496.249617	21720.096450	30.995815
497.032848	21752.944451	31.000832
497.319157	21785.364387	31.005850
497.902930	21811.027810	31.010868
498.141268	21842.791865	31.015885
498.574575	21882.588063	31.020903
499.059157	21904.659169	31.025920
499.568949	21952.777756	31.030938
500.277611	21973.076453	31.035956
500.816029	22010.215387	31.040973
501.414932	22043.983489	31.045991
502.106634	22065.870886	31.051008
502.053557	22104.713321	31.056026
503.046728	22132.632357	31.061044
503.502875	22171.755811	31.066061
503.816320	22203.900509	31.071079
504.268625	22226.292932	31.076096
504.861039	22266.633813	31.081114
505.427388	22297.848363	31.086132
505.541052	22331.363927	31.091149
506.065173	22365.213726	31.096167
506.895287	22399.913201	31.101184
506.848233	22442.559218	31.106202
507.398879	22472.417965	31.111220
508.030802	22510.446861	31.116237
508.573205	22552.944482	31.121255
509.437510	22590.400262	31.126272
509.864892	22626.894172	31.131290
510.151730	22655.081878	31.136308
510.736256	22680.607303	31.141325
510.848934	22724.884582	31.146343
511.966781	22762.307537	31.151360
512.431037	22807.749799	31.156378
512.911619	22844.317973	31.161396
513.282747	22877.446844	31.166413
513.411511	22909.261264	31.171431
514.238617	22940.404640	31.176448
514.719717	22983.013829	31.181466
515.303385	23016.495296	31.186484
516.128082	23054.615287	31.191501
516.322388	23092.018348	31.196519
517.493034	23117.952287	31.201536
517.662220	23135.549519	31.206554
517.721099	23162.547562	31.211572
518.451231	23190.167822	31.216589
519.214385	23219.230022	31.221607
519.778385	23248.803509	31.226624
520.443496	23274.525682	31.231642
521.146380	23282.757388	31.236660
521.498087	23310.417771	31.241677
522.616250	23345.623817	31.246695
522.593759	23365.488018	31.251712
523.054968	23396.512142	31.256730
523.436210	23425.735203	31.261748
523.708974	23449.553466	31.266765
524.449677	23484.357231	31.271783
525.202793	23505.478379	31.276800
525.661603	23544.098606	31.281818
525.957928	23567.287755	31.286836
526.644516	23592.943807	31.291853
527.096712	23627.874885	31.296871
527.699427	23656.545643	31.301888
528.131791	23689.799038	31.306906
528.544792	23730.076044	31.311924
528.961516	23760.766429	31.316941
529.150723	23799.827228	31.321959
529.806569	23831.933900	31.326976
530.367656	23874.254507	31.331994
530.703871	23911.940338	31.337012
531.035154	23952.634943	31.342029
531.953962	24001.048704	31.347047
532.645984	24031.519712	31.352064
532.889792	24076.430466	31.357082
534.066058	24108.039498	31.362100
534.734907	24134.311977	31.367117
534.762736	24175.218577	31.372135
535.284504	24197.659288	31.377152
536.145171	24247.352872	31.382170
536.114104	24276.868864	31.387188
537.103371	24315.313218	31.392205
537.569998	24358.926059	31.397223
537.769356	24389.272092	31.402240
538.801710	24427.469819	31.407258
539.653617	24460.438011	31.412276
540.237042	24493.277430	31.417293
541.343485	24510.154907	31.422311
542.064271	24533.942637	31.427328
542.330117	24560.512234	31.432346
543.130828	24582.568707	31.437364
543.565346	24602.590493	31.442381
544.125916	24651.383892	31.447399
544.191240	24661.225767	31.452416
544.703571	24699.163722	31.457434
545.129588	24720.981667	31.462452
545.971647	24750.564656	31.467469
546.539373	24783.988387	31.472487
546.883913	24802.514031	31.477504
546.695397	24850.407097	31.482522
547.308480	24886.320130	31.487540
547.871914	24921.482618	31.492557
548.376908	24960.831459	31.497575
548.493807	25000.575730	31.502592
549.377625	25043.297260	31.507610
549.792062	25086.370013	31.512628
550.337343	25115.216119	31.517645
550.803992	25159.494257	31.522663
551.391330	25194.862049	31.527680
551.916644	25244.155309	31.532698
552.025686	25281.619984	31.537716
553.241868	25315.480820	31.542733
553.942819	25361.890560	31.547751
554.765605	25386.390185	31.552768
554.967584	25424.175599	31.557786
555.654619	25455.363679	31.562804
556.870769	25481.407378	31.567821
556.645593	25511.972874	31.572839
557.480051	25539.504317	31.577856
558.269348	25574.019779	31.582874
558.543176	25600.956055	31.587892
559.282395	25620.577521	31.592909
559.619992	25658.822563	31.597927
560.429308	25682.029103	31.602944
560.727995	25728.887818	31.607962
561.273118	25754.259006	31.612980
561.626642	25786.580199	31.617997
562.144060	25833.727415	31.623015
562.319379	25870.854242	31.628032
563.132047	25918.018890	31.633050
563.790229	25964.335563	31.638068
564.491723	25999.023420	31.643085
565.191617	26040.132550	31.648103
565.289602	26083.231425	31.653120
566.067164	26118.356356	31.658138
566.807282	26162.594132	31.663156
567.136604	26196.417563	31.668173
567.608488	26252.167909	31.673191
568.475550	26284.871311	31.678208
568.994733	26338.383599	31.683226
569.467694	26379.775228	31.688244
570.114603	26404.113878	31.693261
570.726687	26444.965746	31.698279
571.562739	26495.363934	31.703296
571.975838	26531.999923	31.708314
572.754672	26574.064814	31.713332
573.746059	26601.156163	31.718349
574.251765	26645.867574	31.723367
574.699278	26672.399042	31.728384
575.125980	26712.698867	31.733402
575.599467	26756.928895	31.738420
576.577224	26790.311093	31.743437
577.113203	26831.491596	31.748455
577.585890	26865.116867	31.753472
577.871017	26909.370230	31.758490
578.543659	26941.656236	31.763508
579.286899	26970.107619	31.768525
579.103739	27017.733232	31.773543
580.237464	27059.358358	31.778560
580.933263	27104.704808	31.783578
580.861487	27143.844338	31.788596
581.653914	27171.226554	31.793613
582.741369	27214.350771	31.798631
583.176651	27260.243742	31.803648
583.421570	27295.143950	31.808666
583.876232	27345.565710	31.813684
584.988854	27383.383676	31.818701
585.261722	27437.607165	31.823719
586.076992	27475.699123	31.828736
586.764569	27510.960572	31.833754
586.962759	27558.325837	31.838772
587.816679	27591.349418	31.843789
588.198381	27635.778943	31.848807
588.696560	27673.124271	31.853824
589.501480	27717.159431	31.858842
589.845619	27765.362029	31.863860
590.714041	27795.337259	31.868877
591.347056	27847.609659	31.873895
592.256678	27886.920182	31.878912
592.466185	27921.308704	31.883930
592.497127	27961.590456	31.888948
593.362908	27988.943399	31.893965
594.123950	28045.127700	31.898983
594.560730	28079.721287	31.904000
594.966590	28115.508000	31.909018
595.400669	28154.223097	31.914036
595.931069	28192.525081	31.919053
596.494490	28234.652238	31.924071
596.664615	28270.880435	31.929088
597.716271	28327.273096	31.934106
598.700217	28376.154967	31.939124
599.140959	28425.134160	31.944141
599.584458	28474.814628	31.949159
600.159898	28522.287742	31.954176
600.759603	28571.596494	31.959194
601.264980	28621.185517	31.964212
602.230206	28666.613604	31.969229
602.977691	28714.408019	31.974247
603.268810	28754.688758	31.979264
604.338887	28807.104164	31.984282
605.028261	28851.981460	31.989300
605.710646	28890.267415	31.994317
606.196249	28935.284068	31.999335
606.752574	28975.808391	32.004352
607.333486	29013.453015	32.009370
607.984048	29063.109000	32.014388
608.483630	29110.399346	32.019405
609.070928	29153.712995	32.024423
609.566428	29198.886708	32.029440
610.422398	29243.018353	32.034458
610.521303	29291.408110	32.039476
611.487116	29331.041358	32.044493
612.118099	29389.879090	32.049511
612.719039	29426.295104	32.054528
613.250932	29475.641877	32.059546
613.843389	29531.173853	32.064564
614.802827	29577.376020	32.069581
615.274525	29631.820902	32.074599
615.660350	29677.764938	32.079616
616.505105	29715.237039	32.084634
617.660335	29763.172701	32.089652
618.476080	29795.883430	32.094669
618.719195	29835.990458	32.099687
619.442685	29877.040470	32.104704
620.364396	29911.308826	32.109722
620.790840	29960.483549	32.114740
621.538380	29987.958719	32.119757
622.188327	30038.729673	32.124775
622.474677	30080.467610	32.129792
623.207499	30112.528037	32.134810
623.824890	30158.550880	32.139828
624.474560	30198.961952	32.144845
625.200122	30247.275370	32.149863
625.099461	30292.291449	32.154880
626.040431	30333.321160	32.159898
626.525755	30376.646944	32.164916
627.321530	30419.153303	32.169933
628.088151	30475.179056	32.174951
628.312454	30516.067848	32.179968
628.659456	30565.338559	32.184986
629.319527	30619.491238	32.190004
630.386524	30668.934569	32.195021
630.911905	30706.976543	32.200039
631.556285	30751.371937	32.205056
632.928933	30798.277404	32.210074
633.194694	30852.504721	32.215092
633.668875	30881.072982	32.220109
634.270195	30917.510543	32.225127
634.984110	30952.969792	32.230144
635.652208	30994.542688	32.235162
636.471764	31019.359368	32.240180
637.217936	31060.199604	32.245197
637.896802	31091.827459	32.250215
638.456486	31134.827189	32.255232
639.408354	31156.981083	32.260250
640.006998	31199.665133	32.265268
640.323056	31225.129372	32.270285
640.913088	31266.607503	32.275303
641.129434	31305.868159	32.280320
641.611489	31333.519207	32.285338
641.826708	31383.608891	32.290356
642.907586	31436.086221	32.295373
643.386329	31482.373819	32.300391
644.174733	31533.335508	32.305408
645.105286	31575.456619	32.310426
645.229203	31617.380987	32.315444
645.841660	31665.272821	32.320461
646.499418	31719.245416	32.325479
646.579601	31781.115263	32.330496
647.595712	31832.206602	32.335514
648.585931	31878.074092	32.340532
649.247555	31945.341107	32.345549
649.639785	31976.907468	32.350567
650.228564	32046.032079	32.355584
650.946115	32104.566957	32.360602
651.577606	32158.803974	32.365620
652.143749	32218.766169	32.370637
652.936038	32270.607788	32.375655
653.831918	32321.067905	32.380672
655.092674	32369.568482	32.385690
655.548820	32423.384637	32.390708
656.554045	32461.405709	32.395725
656.977820	32512.015645	32.400743
657.741559	32561.833123	32.405760
658.403312	32596.323419	32.410778
659.419057	32645.918534	32.415796
659.978170	32685.261196	32.420813
660.716561	32714.625345	32.425831
661.273921	32772.915199	32.430848
662.568183	32794.379034	32.435866
663.458458	32825.698460	32.440884
664.471184	32858.876489	32.445901
665.408351	32883.683419	32.450919
665.604082	32916.426069	32.455936
666.200699	32940.609631	32.460954
667.018705	32971.580174	32.465972
667.197429	33000.823226	32.470989
667.625613	33037.948951	32.476007
668.223055	33082.792861	32.481024
668.766673	33116.088581	32.486042
669.161113	33178.046415	32.491060
669.661066	33215.926252	32.496077
670.581680	33267.674512	32.501095
670.532768	33313.131622	32.506112
671.163951	33368.977646	32.511130
672.037523	33425.209667	32.516148
672.334652	33472.990372	32.521165
673.112727	33531.564090	32.526183
673.717217	33585.929142	32.531200
674.332460	33644.092294	32.536218
675.105807	33698.418707	32.541236
675.516986	33756.727737	32.546253
676.344944	33817.184832	32.551271
677.153892	33868.932995	32.556288
677.728334	33922.532283	32.561306
677.962692	33986.104314	32.566324
678.587161	34030.345429	32.571341
679.715060	34078.611449	32.576359
680.064776	34132.088197	32.581376
680.855350	34186.312035	32.586394
681.377445	34233.142708	32.591412
682.001114	34304.305156	32.596429
682.930334	34347.968419	32.601447
683.372632	34415.258558	32.606464
684.390697	34471.635274	32.611482
684.930469	34523.439598	32.616500
685.437384	34583.714945	32.621517
685.920042	34632.259712	32.626535
686.427170	34707.551277	32.631552
688.743663	34739.770633	32.636570
690.198513	34774.052541	32.641588
690.890550	34815.958102	32.646605
691.414426	34853.280787	32.651623
691.692727	34904.690495	32.656640
692.369677	34940.332993	32.661658
693.523854	34979.947716	32.666676
694.068227	35030.323666	32.671693
694.778307	35064.475406	32.676711
695.275102	35104.306504	32.681728
695.499801	35148.865107	32.686746
696.115834	35201.734074	32.691764
697.289737	35248.686831	32.696781
698.417285	35276.008676	32.701799
698.889016	35323.962405	32.706816
699.373566	35372.224059	32.711834
700.378054	35422.693709	32.716852
700.868429	35479.041458	32.721869
701.562942	35496.991159	32.726887
702.277224	35546.810781	32.731904
702.347286	35601.112484	32.736922
703.097399	35653.038583	32.741940
703.900073	35706.632170	32.746957
704.646179	35767.442712	32.751975
705.019633	35822.001247	32.756992
705.935811	35867.104972	32.762010
706.541058	35924.890280	32.767028
706.924902	35985.264656	32.772045
707.820262	36043.504633	32.777063
708.670905	36105.842660	32.782080
708.901695	36158.837216	32.787098
709.994230	36216.869932	32.792116
710.618687	36274.431897	32.797133
711.151869	36329.921641	32.802151
711.928693	36394.756942	32.807168
712.837669	36457.333517	32.812186
713.283467	36514.127241	32.817204
714.234446	36575.698586	32.822221
715.023332	36628.658017	32.827239
715.789859	36689.031727	32.832256
716.700040	36737.015241	32.837274
717.171129	36794.494995	32.842292
718.027005	36857.605833	32.847309
718.497868	36921.548217	32.852327
719.319202	36983.419142	32.857344
719.916252	37038.173622	32.862362
720.788356	37094.586370	32.867380
721.777645	37155.742418	32.872397
722.542221	37208.707076	32.877415
723.024026	37264.302099	32.882432
724.098010	37326.577316	32.887450
724.760041	37374.923384	32.892468
725.272783	37426.340636	32.897485
726.018157	37474.851009	32.902503
726.967005	37533.953031	32.907520
727.573033	37584.097796	32.912538
728.363467	37627.213999	32.917556
728.721214	37681.545773	32.922573
729.240245	37727.056726	32.927591
729.885735	37791.151583	32.932608
730.554083	37838.055974	32.937626
731.490298	37900.809597	32.942644
731.957577	37958.697774	32.947661
732.714063	38009.914074	32.952679
733.297469	38065.666095	32.957696
733.919153	38134.723308	32.962714
734.916969	38186.471579	32.967732
735.511845	38246.104934	32.972749
736.369499	38310.977731	32.977767
737.269932	38372.865652	32.982784
737.966129	38430.181959	32.987802
739.279781	38480.180722	32.992820
739.063691	38549.432919	32.997837
739.963132	38607.970142	33.002855
740.688902	38686.156937	33.007872
741.537063	38740.680642	33.012890
742.746911	38802.957971	33.017908
743.631685	38868.561778	33.022925
744.156501	38916.742968	33.027943
744.794672	38971.774228	33.032960
745.666453	39037.216153	33.037978
746.355219	39093.586814	33.042996
746.976994	39157.189853	33.048013
748.160433	39218.523921	33.053031
748.766075	39283.951110	33.058048
749.532930	39347.595363	33.063066
750.351534	39401.904006	33.068084
751.073981	39467.730945	33.073101
752.728120	39514.909238	33.078119
752.980089	39566.846495	33.083136
753.777303	39627.931977	33.088154
754.906447	39674.401848	33.093172
755.276078	39738.317778	33.098189
755.995718	39785.559922	33.103207
756.394195	39844.981634	33.108224
757.223328	39910.679480	33.113242
757.907027	39975.767759	33.118260
758.677531	40034.980301	33.123277
759.533693	40093.186787	33.128295
760.213973	40144.110139	33.133312
761.244903	40207.772730	33.138330
762.268984	40268.628653	33.143348
762.501416	40336.501320	33.148365
763.499222	40382.999482	33.153383
763.908850	40450.610926	33.158400
764.917412	40516.364889	33.163418
765.687920	40572.410464	33.168436
766.283479	40625.087295	33.173453
767.471380	40688.897616	33.178471
768.805385	40741.719073	33.183488
769.081407	40796.216859	33.188506
770.022585	40849.649943	33.193524
770.516585	40907.276231	33.198541
771.423307	40959.494352	33.203559
772.170369	41012.078968	33.208576
772.695246	41080.034913	33.213594
773.841487	41129.003371	33.218612
774.350661	41191.908919	33.223629
775.015735	41251.261347	33.228647
775.942766	41312.027782	33.233664
776.815335	41363.746232	33.238682
777.649893	41416.419393	33.243700
778.582095	41474.592440	33.248717
779.637841	41513.709641	33.253735
780.098480	41559.813275	33.258752
779.978414	41604.685575	33.263770
781.000178	41656.223380	33.268788
781.967317	41709.553337	33.273805
782.440066	41769.632813	33.278823
783.269021	41821.333837	33.283840
783.711928	41882.113972	33.288858
784.788265	41949.822336	33.293876
785.081980	42021.542397	33.298893
786.040184	42081.199302	33.303911
786.622716	42143.545918	33.308928
787.270458	42211.479925	33.313946
788.420845	42270.139747	33.318964
788.857860	42334.147660	33.323981
789.696677	42404.582416	33.328999
790.582859	42471.038063	33.334016
791.508188	42527.855148	33.339034
793.232415	42583.801690	33.344052
793.924572	42645.974547	33.349069
795.335663	42697.100005	33.354087
796.665387	42741.072182	33.359104
797.851032	42791.543544	33.364122
798.543815	42824.394717	33.369140
799.421795	42877.089929	33.374157
799.994054	42915.658734	33.379175
800.480012	42956.492711	33.384192
801.145603	43003.630059	33.389210
802.277970	43031.991986	33.394228
803.454410	43076.488367	33.399245
804.405254	43120.374809	33.404263
804.763388	43166.301697	33.409280
805.360636	43207.700714	33.414298
806.237064	43264.849891	33.419316
806.991672	43311.632490	33.424333
807.437106	43358.463317	33.429351
807.812230	43415.045764	33.434368
808.629169	43468.049169	33.439386
809.315837	43528.871806	33.444404
810.053721	43591.533567	33.449421
810.641735	43654.010107	33.454439
811.620761	43718.412049	33.459456
811.936924	43793.815611	33.464474
812.964417	43855.269207	33.469492
813.504859	43921.511062	33.474509
814.086341	43988.493101	33.479527
815.055790	44052.347211	33.484544
815.746134	44127.320470	33.489562
816.558610	44202.192741	33.494580
817.368138	44288.976261	33.499597
818.538915	44357.860151	33.504615
819.409262	44435.450413	33.509632
820.105639	44499.247111	33.514650
821.073481	44568.953916	33.519668
821.440992	44640.392669	33.524685
822.309981	44708.711061	33.529703
823.231551	44779.583281	33.534720
824.093365	44858.833612	33.539738
825.373441	44935.779895	33.544756
826.013709	45005.849009	33.549773
826.630268	45064.978880	33.554791
827.586785	45139.382770	33.559808
828.416304	45220.612983	33.564826
829.505229	45281.687752	33.569844
830.301087	45353.871785	33.574861
831.425658	45418.344553	33.579879
832.380377	45477.081293	33.584896
832.720432	45546.831949	33.589914
833.581943	45599.314794	33.594932
834.588366	45661.092942	33.599949
835.170311	45722.133972	33.604967
835.999365	45776.039242	33.609984
836.500279	45846.803210	33.615002
837.785675	45904.268729	33.620020
838.284738	45975.741877	33.625037
838.702432	46046.019691	33.630055
840.033244	46115.250993	33.635072
840.476041	46184.684000	33.640090
841.069978	46253.537019	33.645108
842.005680	46331.952380	33.650125
842.874287	46410.669450	33.655143
843.594464	46482.837269	33.660160
844.546520	46564.622612	33.665178
845.450208	46637.148243	33.670196
846.389103	46715.659334	33.675213
846.829847	46785.796699	33.680231
848.583531	46863.884151	33.685248
849.331063	46947.480335	33.690266
850.173358	47015.373420	33.695284
850.971339	47084.349042	33.700301
851.479538	47165.092265	33.705319
852.675569	47227.673927	33.710336
853.360059	47309.921148	33.715354
854.272559	47382.504740	33.720372
855.587815	47453.026793	33.725389
855.939205	47520.801702	33.730407
857.153347	47595.287495	33.735424
857.684712	47679.090842	33.740442
858.880085	47752.510937	33.745460
860.118574	47832.421666	33.750477
861.045153	47912.109198	33.755495
861.867114	47966.697732	33.760512
862.514353	48041.538946	33.765530
863.015748	48115.352930	33.770548
864.144614	48187.513186	33.775565
864.937014	48268.203447	33.780583
866.374709	48328.776694	33.785600
867.314752	48403.061078	33.790618
868.455601	48477.061388	33.795636
869.793105	48531.615315	33.800653
870.423796	48593.681413	33.805671
871.439765	48647.925060	33.810688
871.994004	48714.824201	33.815706
872.836881	48772.745505	33.820724
873.440767	48842.085670	33.825741
874.271888	48912.801504	33.830759
875.541040	48979.235845	33.835776
876.292552	49051.660036	33.840794
876.856923	49111.631098	33.845812
877.681414	49177.179909	33.850829
878.743180	49249.366632	33.855847
879.809314	49307.678430	33.860864
879.879820	49382.734034	33.865882
880.839478	49459.131934	33.870900
882.054208	49525.899003	33.875917
882.410333	49609.205281	33.880935
883.815179	49676.936503	33.885952
884.205182	49758.599407	33.890970
885.464360	49830.092915	33.895988
886.313044	49902.707133	33.901005
887.283517	49980.724769	33.906023
888.305649	50052.015446	33.911040
888.810187	50129.562003	33.916058
889.856661	50201.551645	33.921076
890.594285	50273.538975	33.926093
890.973214	50344.753529	33.931111
892.535892	50403.022458	33.936128
893.264208	50485.059190	33.941146
894.105935	50541.181945	33.946164
895.422034	50598.989918	33.951181
895.832302	50660.779578	33.956199
897.496692	50720.039484	33.961216
898.126521	50789.172706	33.966234
898.436295	50857.925710	33.971252
899.433646	50918.371900	33.976269
900.831168	50988.556740	33.981287
901.429135	51058.758693	33.986304
901.985850	51127.328535	33.991322
903.154087	51201.497892	33.996340
903.749630	51269.264879	34.001357
904.774061	51346.443547	34.006375
905.936929	51421.082662	34.011392
906.481343	51488.522905	34.016410
907.442985	51566.382775	34.021428
908.886062	51637.878582	34.026445
909.706946	51723.379017	34.031463
910.362977	51791.707581	34.036480
911.112285	51864.533268	34.041498
912.301660	51939.043379	34.046516
913.477707	52014.036691	34.051533
914.272899	52094.720978	34.056551
915.161832	52163.950849	34.061568
916.327111	52236.902778	34.066586
916.672095	52305.281271	34.071604
917.886530	52377.827356	34.076621
918.416592	52462.451959	34.081639
919.838193	52539.288031	34.086656
920.637615	52621.871766	34.091674
921.600921	52697.836886	34.096692
922.240742	52770.764713	34.101709
923.244034	52854.791881	34.106727
923.734736	52937.880382	34.111744
924.693289	53021.668334	34.116762
926.293079	53115.753258	34.121780
927.244712	53187.646721	34.126797
927.949072	53267.640497	34.131815
928.882973	53344.960119	34.136832
929.983541	53428.145263	34.141850
930.544098	53513.249840	34.146868
931.931926	53591.695583	34.151885
933.046309	53666.178594	34.156903
934.120497	53745.496300	34.161920
934.931008	53807.744579	34.166938
935.636636	53889.986699	34.171956
936.617110	53962.257727	34.176973
937.638331	54047.507685	34.181991
938.651392	54124.184755	34.187008
939.570952	54206.679443	34.192026
940.257252	54284.673508	34.197044
941.499057	54370.200375	34.202061
941.994204	54451.800117	34.207079
943.105997	54518.274852	34.212096
944.455490	54604.443932	34.217114
945.553456	54677.989813	34.222132
946.344528	54751.735571	34.227149
947.497419	54832.677366	34.232167
948.334109	54892.494407	34.237184
949.742179	54971.511145	34.242202
950.244829	55049.745160	34.247220
951.161678	55109.866688	34.252237
952.073427	55182.342006	34.257255
953.715288	55251.153708	34.262272
954.664421	55322.744000	34.267290
955.200764	55383.431721	34.272308
956.224087	55436.342165	34.277325
957.101126	55503.140993	34.282343
957.689795	55557.954600	34.287360
958.747980	55625.763434	34.292378
959.412964	55685.128248	34.297396
960.445677	55757.092878	34.302413
961.361581	55831.227591	34.307431
962.222733	55898.498312	34.312448
962.871195	55975.902639	34.317466
964.239399	56053.277452	34.322484
965.667436	56115.359748	34.327501
966.592911	56182.855419	34.332519
967.516840	56248.301059	34.337536
968.164533	56322.985343	34.342554
969.071589	56399.002799	34.347572
970.336451	56477.875980	34.352589
970.594833	56550.469836	34.357607
971.741026	56635.659034	34.362624
973.031014	56715.851787	34.367642
973.402335	56794.479052	34.372660
974.628975	56863.537269	34.377677
975.418320	56952.580395	34.382695
976.290180	57040.655360	34.387712
977.342875	57123.519198	34.392730
978.778315	57208.785664	34.397748
980.674756	57246.469945	34.402765
982.088300	57316.310471	34.407783
983.326888	57380.052071	34.412800
984.305388	57443.030557	34.417818
984.936188	57506.525342	34.422836
985.724356	57569.236327	34.427853
987.025008	57650.196355	34.432871
987.595877	57728.346267	34.437888
988.005683	57800.072256	34.442906
989.244997	57870.169360	34.447924
990.126120	57942.423664	34.452941
991.577008	58010.304728	34.457959
992.580825	58083.293514	34.462976
993.659187	58156.239273	34.467994
994.479957	58236.712687	34.473012
995.103322	58296.679072	34.478029
996.086731	58380.026388	34.483047
996.797980	58463.954337	34.488064
997.884587	58536.779710	34.493082
998.835985	58619.753085	34.498100
1000.089770	58707.439261	34.503117
1000.533175	58796.638005	34.508135
1001.046437	58878.414617	34.513152
1002.256584	58965.355336	34.518170
1003.455823	59059.526155	34.523188
1004.902373	59146.595289	34.528205
1005.821754	59229.677010	34.533223
1007.046761	59310.154368	34.538240
1008.078012	59400.175262	34.543258
1008.759210	59488.029346	34.548276
1009.767922	59564.300492	34.553293
1011.130926	59649.751439	34.558311
1011.863543	59736.161624	34.563328
1012.863679	59819.739154	34.568346
1013.448535	59903.584159	34.573364
1014.153167	59991.860494	34.578381
1015.492465	60090.425219	34.583399
1016.485228	60180.625892	34.588416
1017.758107	60262.149667	34.593434
1018.660309	60355.232408	34.598452
1019.843142	60447.632523	34.603469
1021.068653	60521.701839	34.608487
1022.066300	60600.047765	34.613504
1023.280294	60672.695144	34.618522
1024.505744	60750.797212	34.623540
1025.398371	60812.835709	34.628557
1026.418323	60891.293032	34.633575
1027.267707	60965.093090	34.638592
1028.184864	61039.528464	34.643610
1029.243050	61104.694190	34.648628
1030.273081	61182.365975	34.653645
1030.908297	61260.112122	34.658663
1031.753094	61347.422047	34.663680
1033.057698	61428.849824	34.668698
1033.936592	61514.142114	34.673716
1035.415167	61596.056092	34.678733
1036.554892	61675.218897	34.683751
1037.077428	61762.282948	34.688768
1038.120071	61843.170512	34.693786
1039.222980	61935.854539	34.698804
1040.315461	62021.912929	34.703821
1041.342974	62125.364233	34.708839
1042.420624	62207.602189	34.713856
1043.115474	62288.171871	34.718874
1044.243399	62375.992095	34.723892
1044.929159	62461.437997	34.728909
1046.175150	62558.887726	34.733927
1047.386662	62667.313539	34.738944
1048.514857	62757.654517	34.743962
1049.603275	62856.244073	34.748980
1050.356485	62946.030068	34.753997
1051.633689	63040.843418	34.759015
1052.734049	63145.661333	34.764032
1054.121126	63233.431596	34.769050
1054.898043	63330.830766	34.774068
1056.160567	63417.260024	34.779085
1057.363130	63505.908251	34.784103
1058.886461	63604.800248	34.789120
1060.356280	63675.403556	34.794138
1061.311655	63762.666808	34.799156
1062.650030	63844.850618	34.804173
1063.562232	63932.982143	34.809191
1064.245195	64014.287291	34.814208
1065.553390	64101.015682	34.819226
1066.519082	64175.003462	34.824244
1068.112643	64247.874491	34.829261
1069.155623	64326.718967	34.834279
1069.982133	64422.164829	34.839296
1071.440744	64497.311323	34.844314
1072.257602	64576.419688	34.849332
1073.123008	64655.546069	34.854349
1074.191458	64736.356737	34.859367
1075.080836	64818.259113	34.864384
1076.197254	64907.995631	34.869402
1077.112104	64998.700811	34.874420
1078.350003	65091.280617	34.879437
1079.563599	65173.614832	34.884455
1080.836982	65256.706051	34.889472
1082.004659	65327.354724	34.894490
1082.451336	65406.985484	34.899508
1083.776673	65494.918910	34.904525
1084.750010	65580.875186	34.909543
1085.378714	65677.610143	34.914560
1086.834211	65764.808846	34.919578
1087.956730	65854.085620	34.924596
1088.872375	65942.027398	34.929613
1089.873050	66020.630528	34.934631
1091.154870	66121.792262	34.939648
1091.942629	66214.155027	34.944666
1092.864781	66307.598834	34.949684
1094.058954	66387.287270	34.954701
1094.857331	66470.469084	34.959719
1096.021851	66554.911076	34.964736
1096.970201	66638.544940	34.969754
1097.831157	66737.115512	34.974772
1099.066196	66828.385223	34.979789
1100.318909	66922.140723	34.984807
1100.907068	67007.680615	34.989824
1102.162818	67103.120449	34.994842
1103.206266	67191.724121	34.999860
1104.264163	67294.843797	35.004877
1105.342855	67388.184901	35.009895
1106.288595	67498.192474	35.014912
1107.621709	67587.670497	35.019930
1108.856218	67685.287518	35.024948
1109.785573	67792.000186	35.029965
1111.388048	67886.451912	35.034983
1112.352207	67985.036567	35.040000
1113.879110	68075.961396	35.045018
1115.137731	68173.139644	35.050036
1115.938201	68273.808673	35.055053
1117.122849	68357.367066	35.060071
1118.270080	68465.061693	35.065088
1119.417874	68559.181443	35.070106
1121.324907	68647.231507	35.075124
1122.888139	68725.381838	35.080141
1123.896901	68810.096138	35.085159
1124.937413	68909.970479	35.090176
1126.103928	68983.060903	35.095194
1127.102487	69066.295984	35.100212
1128.370347	69161.076756	35.105229
1129.366593	69248.960388	35.110247
1130.066360	69330.241948	35.115264
1131.302259	69427.523451	35.120282
1132.526019	69526.320550	35.125300
1133.614069	69622.764653	35.130317
1134.629600	69711.248394	35.135335
1135.617511	69805.125301	35.140352
1136.933220	69900.173613	35.145370
1137.741077	70003.020135	35.150388
1139.042422	70095.449914	35.155405
1141.154640	70189.165872	35.160423
1141.806255	70295.919472	35.165440
1142.997643	70380.939763	35.170458
1143.923502	70476.076194	35.175476
1144.949899	70574.319110	35.180493
1146.309768	70662.416887	35.185511
1147.238259	70755.761904	35.190528
1148.694606	70844.795121	35.195546
1150.175862	70938.194061	35.200564
1151.197402	71039.339686	35.205581
1152.438248	71123.569492	35.210599
1153.174459	71217.250042	35.215616
1154.520753	71316.281833	35.220634
1155.665853	71389.154401	35.225652
1156.618768	71488.767334	35.230669
1158.233116	71577.031225	35.235687
1159.512671	71670.337528	35.240704
1160.682403	71754.618430	35.245722
1162.117505	71847.229905	35.250740
1162.877268	71931.283892	35.255757
1164.015887	72024.955351	35.260775
1165.049287	72118.871496	35.265792
1165.918082	72217.018458	35.270810
1167.420189	72303.377146	35.275828
1168.469052	72404.232479	35.280845
1169.624414	72500.170119	35.285863
1170.609129	72594.361509	35.290880
1171.815112	72678.500409	35.295898
1173.268687	72758.839384	35.300916
1173.464851	72840.843528	35.305933
1174.769823	72919.204965	35.310951
1175.339416	73018.288069	35.315968
1176.728641	73113.456927	35.320986
1177.644439	73200.682420	35.326004
1178.985166	73304.750849	35.331021
1180.470629	73394.079485	35.336039
1181.306675	73490.374398	35.341056
1182.347956	73601.824132	35.346074
1183.758229	73691.114808	35.351092
1184.765802	73803.799233	35.356109
1186.008645	73906.833979	35.361127
1187.002852	74017.900136	35.366144
1188.334725	74120.035222	35.371162
1189.413266	74233.141065	35.376180
1191.132053	74347.832344	35.381197
1192.501744	74440.171752	35.386215
1192.967948	74549.232365	35.391232
1194.565388	74647.426895	35.396250
1195.851649	74754.904065	35.401268
1197.197766	74872.961550	35.406285
1198.641906	74964.822520	35.411303
1199.362106	75076.277721	35.416320
1200.865028	75180.885556	35.421338
1201.877392	75283.746151	35.426356
1203.145493	75404.427458	35.431373
1204.321579	75505.781407	35.436391
1205.764233	75617.063063	35.441408
1207.051160	75721.643289	35.446426
1208.470185	75824.328650	35.451444
1209.816317	75923.618324	35.456461
1211.801713	76030.041747	35.461479
1212.806299	76125.787885	35.466496
1213.980218	76219.557266	35.471514
1215.353451	76308.583755	35.476532
1216.474315	76410.887073	35.481549
1218.015657	76499.558677	35.486567
1219.271850	76594.393269	35.491584
1220.297059	76691.544271	35.496602
1221.209195	76787.383143	35.501620
1222.591421	76885.188643	35.506637
1223.420123	76984.942775	35.511655
1225.145578	77090.790123	35.516672
1226.074952	77184.448895	35.521690
1227.316894	77286.394641	35.526708
1228.536526	77387.824867	35.531725
1230.117079	77485.563653	35.536743
1230.999448	77597.599377	35.541760
1232.509802	77693.867706	35.546778
1233.845722	77788.554706	35.551796
1234.635528	77887.507450	35.556813
1235.570403	78001.652199	35.561831
1236.620398	78105.746434	35.566848
1238.354412	78206.326885	35.571866
1239.858204	78308.957770	35.576884
1240.737135	78418.071053	35.581901
1242.160335	78522.374811	35.586919
1243.042393	78627.409276	35.591936
1244.220631	78724.531023	35.596954
1245.896966	78827.504371	35.601972
1247.114928	78942.837800	35.606989
1247.972602	79037.768242	35.612007
1249.431333	79141.650758	35.617024
1250.692393	79245.665783	35.622042
1252.689351	79340.141226	35.627060
1254.090584	79435.659866	35.632077
1255.167874	79520.638251	35.637095
1256.907881	79587.207468	35.642112
1257.936385	79659.259134	35.647130
1258.980269	79734.108392	35.652148
1259.634686	79832.240392	35.657165
1260.912611	79921.584856	35.662183
1262.390987	80007.021728	35.667200
1262.970642	80106.749947	35.672218
1264.242277	80204.850539	35.677236
1265.631406	80299.373193	35.682253
1266.833149	80388.477638	35.687271
1268.453206	80490.427077	35.692288
1269.733953	80590.161925	35.697306
1270.611176	80681.902329	35.702324
1272.057042	80792.938467	35.707341
1273.263674	80894.713021	35.712359
1274.419513	80984.966755	35.717376
1275.132434	81091.797922	35.722394
1276.673666	81200.565686	35.727412
1277.748710	81321.265073	35.732429
1279.234287	81440.304718	35.737447
1280.413858	81549.408860	35.742464
1281.674477	81653.002189	35.747482
1283.289610	81764.623979	35.752500
1283.817251	81876.035389	35.757517
1285.239064	81994.947944	35.762535
1287.080031	82110.919705	35.767552
1288.676212	82229.565384	35.772570
1289.865289	82336.555229	35.777588
1290.875148	82451.846880	35.782605
1292.541137	82558.269204	35.787623
1293.962070	82671.761973	35.792640
1295.524655	82777.707086	35.797658
1296.937613	82882.674940	35.802676
1297.918403	82996.389562	35.807693
1299.218150	83111.866846	35.812711
1300.436129	83218.399398	35.817728
1301.900477	83339.388926	35.822746
1303.497327	83438.881949	35.827764
1304.474100	83555.108180	35.832781
1305.738925	83660.076626	35.837799
1307.414946	83772.076982	35.842816
1308.623427	83882.655417	35.847834
1310.123519	83989.501724	35.852852
1311.336603	84100.802517	35.857869
1312.595109	84203.873339	35.862887
1314.154641	84313.220419	35.867904
1315.372101	84428.728521	35.872922
1317.383409	84528.122823	35.877940
1319.203846	84625.975982	35.882957
1320.568656	84722.189807	35.887975
1322.233724	84809.892963	35.892992
1322.929542	84903.119789	35.898010
1324.154850	84994.870680	35.903028
1325.102797	85104.430012	35.908045
1326.672137	85194.797519	35.913063
1327.736069	85312.056358	35.918080
1328.664386	85414.017166	35.923098
1330.165095	85512.632705	35.928116
1331.302499	85627.119034	35.933133
1332.425318	85741.101229	35.938151
1334.088596	85839.907997	35.943168
1335.169907	85957.344152	35.948186
1336.298985	86066.169335	35.953204
1337.613250	86179.819341	35.958221
1338.905235	86288.138479	35.963239
1340.567732	86407.120643	35.968256
1341.648814	86505.728851	35.973274
1343.031023	86616.087998	35.978292
1344.314780	86713.398181	35.983309
1345.350195	86810.443218	35.988327
1346.778748	86909.062070	35.993344
1347.546673	87035.966631	35.998362
1349.099803	87129.003822	36.003380
1350.259083	87242.998907	36.008397
1351.441185	87353.100532	36.013415
1353.310871	87463.260289	36.018432
1354.410148	87582.423623	36.023450
1355.497355	87695.189807	36.028468
1357.154357	87813.405553	36.033485
1358.361761	87929.360034	36.038503
1359.751444	88050.406272	36.043520
1361.316271	88175.759744	36.048538
1362.496969	88281.493059	36.053556
1363.650400	88405.200747	36.058573
1365.228509	88533.316304	36.063591
1366.680089	88649.438378	36.068608
1367.797523	88780.211942	36.073626
1369.161231	88900.847515	36.078644
1370.256482	89025.238516	36.083661
1372.095100	89153.151464	36.088679
1373.179331	89286.707805	36.093696
1374.936997	89413.050353	36.098714
1376.484942	89538.855792	36.103732
1378.093065	89661.382727	36.108749
1379.622320	89784.594121	36.113767
1381.218385	89899.874848	36.118784
1382.727032	90023.901529	36.123802
1383.997119	90137.903218	36.128820
1385.577841	90261.995710	36.133837
1386.909188	90390.373139	36.138855
1388.258670	90500.143594	36.143872
1389.683962	90623.146509	36.148890
1391.611588	90740.837546	36.153908
1393.158743	90853.430089	36.158925
1394.514930	90970.970173	36.163943
1396.111936	91073.860407	36.168960
1397.424861	91190.596964	36.173978
1399.071936	91299.703011	36.178996
1400.085637	91397.742348	36.184013
1401.793183	91511.199563	36.189031
1403.547882	91626.791767	36.194048
1404.964811	91739.205112	36.199066
1405.911041	91845.279062	36.204084
1407.445094	91957.624293	36.209101
1408.522484	92062.664661	36.214119
1410.174536	92169.326966	36.219136
1411.183994	92295.341847	36.224154
1412.507043	92411.409812	36.229172
1413.909123	92536.008432	36.234189
1415.391372	92653.953697	36.239207
1417.274530	92769.416200	36.244224
1418.386025	92886.849725	36.249242
1419.782238	92997.014895	36.254260
1421.183524	93119.866942	36.259277
1422.816018	93231.428412	36.264295
1424.061853	93343.253267	36.269312
1425.857621	93464.929929	36.274330
1426.568033	93574.088547	36.279348
1428.618042	93694.839316	36.284365
1429.716792	93808.197068	36.289383
1431.224054	93927.588295	36.294400
1432.315136	94048.565761	36.299418
1433.404272	94161.393963	36.304436
1435.026100	94285.889461	36.309453
1436.561929	94409.359487	36.314471
1438.040255	94516.994990	36.319488
1439.191384	94632.033421	36.324506
1440.840735	94727.842414	36.329524
1442.261936	94833.561273	36.334541
1443.740576	94944.531822	36.339559
1444.803080	95052.639523	36.344576
1445.824762	95168.790182	36.349594
1447.228877	95280.343928	36.354612
1448.583730	95406.495280	36.359629
1449.810672	95522.437856	36.364647
1451.431156	95657.649952	36.369664
1452.265896	95788.282252	36.374682
1454.038631	95923.408425	36.379700
1455.102831	96056.655365	36.384717
1456.789466	96185.800423	36.389735
1458.786677	96320.234232	36.394752
1460.544318	96448.215816	36.399770
1462.208921	96564.258930	36.404788
1464.475006	96691.908854	36.409805
1465.149539	96815.864747	36.414823
1466.904627	96946.485392	36.419840
1468.492226	97071.986109	36.424858
1469.957573	97194.020383	36.429876
1471.642986	97315.970173	36.434893
1472.471572	97456.941571	36.439911
1474.282857	97584.665907	36.444928
1475.559606	97714.996574	36.449946
1477.351390	97843.460225	36.454964
1478.664905	97977.373705	36.459981
1480.143404	98103.402565	36.464999
1481.873583	98232.878837	36.470016
1483.075005	98367.572010	36.475034
1484.550571	98500.828638	36.480052
1486.173093	98626.101901	36.485069
1487.219817	98760.656016	36.490087
1489.565289	98901.068130	36.495104
1491.149211	99026.551805	36.500122
1492.140042	99161.851575	36.505140
1494.158960	99281.601909	36.510157
1495.261540	99415.199303	36.515175
1496.912500	99549.662690	36.520192
1498.082362	99687.383510	36.525210
1499.716766	99823.574726	36.530228
1501.069047	99956.488964	36.535245
1503.003001	100095.208210	36.540263
1504.697371	100230.834010	36.545280
1506.046912	100366.285855	36.550298
1507.838960	100493.074004	36.555316
1508.976048	100622.411371	36.560333
1510.696389	100755.296965	36.565351
1512.497432	100888.728363	36.570368
1514.038343	101011.475405	36.575386
1516.168520	101120.185600	36.580404
1518.308677	101230.517371	36.585421
1520.025297	101343.019970	36.590439
1521.951848	101445.677559	36.595456
1522.970434	101571.018242	36.600474
1524.556364	101684.429821	36.605492
1526.031635	101796.527819	36.610509
1527.572860	101908.527190	36.615527
1528.655546	102015.121349	36.620544
1530.065861	102127.560224	36.625562
1531.282382	102245.595399	36.630580
1532.718191	102375.565176	36.635597
1533.976182	102500.276275	36.640615
1535.675953	102607.993435	36.645632
1536.690677	102750.252201	36.650650
1537.758991	102856.838649	36.655668
1539.442966	102980.280808	36.660685
1540.921145	103104.021710	36.665703
1542.131034	103217.370327	36.670720
1543.574300	103341.637376	36.675738
1544.634411	103460.829648	36.680756
1546.763911	103581.478786	36.685773
1547.793813	103712.455234	36.690791
1549.458803	103846.046626	36.695808
1550.951060	103981.846214	36.700826
1552.309110	104115.587894	36.705844
1553.539987	104246.116756	36.710861
1555.057263	104404.736402	36.715879
1556.721393	104547.928802	36.720896
1558.414990	104689.506973	36.725914
1559.462277	104830.210036	36.730932
1561.324910	104969.747084	36.735949
1562.476661	105138.037996	36.740967
1564.083768	105285.134980	36.745984
1566.130867	105428.005264	36.751002
1567.745583	105587.946682	36.756020
1569.534106	105738.884666	36.761037
1571.432407	105897.312582	36.766055
1572.873647	106042.447983	36.771072
1574.365601	106186.117943	36.776090
1576.400030	106328.702376	36.781108
1577.913136	106482.247860	36.786125
1579.255139	106627.794287	36.791143
1581.619457	106763.786370	36.796160
1583.969909	106896.978874	36.801178
1585.751617	107033.848876	36.806196
1587.061516	107172.631477	36.811213
1589.025808	107311.870716	36.816231
1590.436962	107442.916437	36.821248
1592.166250	107573.165008	36.826266
1593.630994	107714.258871	36.831284
1595.278925	107842.707844	36.836301
1596.799111	107975.932332	36.841319
1598.333829	108118.031393	36.846336
1599.930780	108245.551452	36.851354
1601.092413	108380.342289	36.856372
1602.863227	108517.777849	36.861389
1604.111354	108661.432745	36.866407
1605.880798	108808.557696	36.871424
1607.759589	108954.169923	36.876442
1609.119158	109091.722491	36.881460
1611.172780	109243.192617	36.886477
1612.791379	109378.905322	36.891495
1613.722789	109530.082166	36.896512
1615.411276	109672.125621	36.901530
1616.893051	109819.160129	36.906548
1618.734497	109965.999783	36.911565
1620.372293	110114.292042	36.916583
1622.180092	110256.966043	36.921600
1623.899633	110402.976858	36.926618
1625.169737	110555.094550	36.931636
1627.215399	110705.164618	36.936653
1628.486801	110849.991579	36.941671
1630.012633	110991.418936	36.946688
1631.723002	111140.832878	36.951706
1633.069852	111295.554217	36.956724
1634.682328	111448.624317	36.961741
1636.500756	111594.447126	36.966759
1638.219180	111746.829891	36.971776
1639.719344	111892.779550	36.976794
1641.207783	112056.600397	36.981812
1643.391066	112202.394275	36.986829
1644.849219	112350.571684	36.991847
1646.205656	112498.803584	36.996864
1647.946240	112631.174429	37.001882
1649.203380	112773.348201	37.006900
1651.096745	112911.352534	37.011917
1652.469543	113051.087108	37.016935
1654.199793	113190.449534	37.021952
1655.280961	113330.839333	37.026970
1656.979035	113485.908637	37.031988
1658.837906	113628.410650	37.037005
1660.560412	113787.688016	37.042023
1662.110151	113929.655935	37.047040
1663.390600	114072.807755	37.052058
1664.900521	114231.967967	37.057076
1666.818839	114377.697748	37.062093
1668.267783	114545.518421	37.067111
1669.791441	114694.088416	37.072128
1671.876938	114858.970509	37.077146
1673.708950	115024.882065	37.082164
1675.229845	115192.859390	37.087181
1676.671951	115351.210639	37.092199
1678.440124	115526.798874	37.097216
1679.921618	115688.316218	37.102234
1681.268894	115863.996934	37.107252
1683.489931	116036.054595	37.112269
1685.350912	116211.492129	37.117287
1686.827658	116384.770703	37.122304
1688.809680	116551.807291	37.127322
1690.196199	116736.199563	37.132340
1691.971458	116903.472847	37.137357
1694.114548	117081.242407	37.142375
1695.758245	117248.778706	37.147392
1697.895666	117418.572719	37.152410
1699.668998	117591.138503	37.157428
1700.979326	117742.721948	37.162445
1702.937044	117923.746058	37.167463
1704.700974	118104.864620	37.172480
1706.681919	118267.101811	37.177498
1708.331471	118441.682152	37.182516
1710.077706	118620.789175	37.187533
1711.394750	118795.727320	37.192551
1713.278374	118969.106715	37.197568
1715.378670	119116.551812	37.202586
1716.815055	119299.896085	37.207604
1719.111820	119462.723457	37.212621
1720.684764	119636.839205	37.217639
1722.086460	119808.166432	37.222656
1723.914231	119965.424320	37.227674
1725.527396	120151.003016	37.232692
1727.298610	120326.169232	37.237709
1729.651365	120486.341138	37.242727
1730.781051	120659.046392	37.247744
1732.497722	120824.836599	37.252762
1734.116394	121003.429177	37.257780
1736.093117	121172.135986	37.262797
1737.933708	121334.636363	37.267815
1739.683924	121521.418072	37.272832
1741.371780	121684.641363	37.277850
1743.592647	121860.163143	37.282868
1745.248123	122020.957320	37.287885
1746.937682	122188.203678	37.292903
1748.484321	122362.361151	37.297920
1750.436777	122532.041707	37.302938
1751.951764	122707.474178	37.307956
1753.745048	122870.470347	37.312973
1755.408884	123041.453886	37.317991
1756.941030	123225.765905	37.323008
1758.757563	123391.082077	37.328026
1760.648611	123560.040839	37.333044
1762.479580	123721.131783	37.338061
1764.465135	123878.799510	37.343079
1765.470019	124030.315595	37.348096
1767.368572	124192.159080	37.353114
1768.891595	124359.123386	37.358132
1770.376714	124521.286269	37.363149
1772.155253	124683.074302	37.368167
1773.636991	124846.444206	37.373184
1775.412872	124999.378984	37.378202
1776.859947	125190.297454	37.383220
1778.353168	125360.962264	37.388237
1780.138366	125548.823143	37.393255
1782.392413	125730.903025	37.398272
1784.173824	125914.769961	37.403290
1785.425418	126100.052276	37.408308
1787.447157	126296.227552	37.413325
1789.176659	126478.785705	37.418343
1790.384306	126673.541721	37.423360
1792.324897	126858.758303	37.428378
1793.790529	127068.890497	37.433396
1795.561344	127275.893345	37.438413
1797.756106	127480.306540	37.443431
1799.810417	127687.508383	37.448448
1801.922919	127884.032349	37.453466
1803.736464	128082.494162	37.458484
1805.718581	128278.520114	37.463501
1807.702521	128465.767104	37.468519
1809.459508	128678.691378	37.473536
1811.283013	128869.022796	37.478554
1813.171215	129073.618407	37.483572
1815.361940	129273.143670	37.488589
1817.400232	129466.184872	37.493607
1818.996089	129658.230056	37.498624
1820.809300	129847.336800	37.503642
1823.423161	130038.819266	37.508660
1825.068012	130243.826369	37.513677
1826.602395	130427.396456	37.518695
1828.295618	130628.020565	37.523712
1830.446646	130821.456403	37.528730
1832.249744	131024.539431	37.533748
1833.782965	131224.785223	37.538765
1835.873951	131428.434385	37.543783
1837.975757	131633.351651	37.548800
1839.320616	131821.766042	37.553818
1840.991195	132022.615888	37.558836
1843.531425	132207.914911	37.563853
1845.488136	132402.530047	37.568871
1846.960813	132595.965224	37.573888
1848.963116	132796.525937	37.578906
1850.612868	133004.692174	37.583924
1852.744412	133207.404412	37.588941
1854.659355	133409.389973	37.593959
1856.507161	133601.172425	37.598976
1858.230670	133798.278998	37.603994
1860.275022	133994.790894	37.609012
1861.710644	134201.739913	37.614029
1863.469807	134394.935391	37.619047
1865.292603	134616.202754	37.624064
1866.941506	134820.748599	37.629082
1868.823007	135028.647199	37.634100
1870.557800	135239.653088	37.639117
1872.607186	135449.659309	37.644135
1874.133331	135666.016501	37.649152
1876.283623	135866.707642	37.654170
1878.245627	136085.067387	37.659188
1879.663377	136301.292216	37.664205
1881.462787	136508.817040	37.669223
1882.889876	136729.280784	37.674240
1885.268522	136939.001560	37.679258
1887.078505	137141.451719	37.684276
1888.549318	137353.079564	37.689293
1890.153101	137552.924139	37.694311
1891.811083	137763.915628	37.699328
1893.921690	137969.304785	37.704346
1895.540703	138187.969050	37.709364
1897.119390	138408.353791	37.714381
1899.177448	138621.444243	37.719399
1900.990094	138838.254039	37.724416
1903.042139	139051.372770	37.729434
1905.275221	139270.530295	37.734452
1907.583580	139488.052752	37.739469
1909.671843	139703.097750	37.744487
1911.524207	139921.365771	37.749504
1913.555789	140131.193030	37.754522
1915.116372	140353.569448	37.759540
1917.026351	140584.014595	37.764557
1918.934013	140794.105187	37.769575
1920.555866	141032.554464	37.774592
1922.592323	141253.109669	37.779610
1924.941731	141485.191342	37.784628
1926.559858	141720.408411	37.789645
1928.945821	141950.253010	37.794663
1930.727585	142179.773925	37.799680
1932.819945	142401.810534	37.804698
1934.712760	142631.988932	37.809716
1936.982538	142863.086976	37.814733
1939.298543	143077.743571	37.819751
1940.989987	143309.428690	37.824768
1943.445445	143528.824841	37.829786
1945.559301	143751.308414	37.834804
1947.709017	143961.679607	37.839821
1949.773086	144185.860861	37.844839
1951.867537	144405.862819	37.849856
1953.424650	144629.350770	37.854874
1954.683703	144839.128157	37.859892
1956.526790	145072.955498	37.864909
1958.778995	145309.944008	37.869927
1960.176925	145546.761975	37.874944
1962.470807	145778.605929	37.879962
1964.385347	146027.657046	37.884980
1966.217869	146263.814186	37.889997
1968.699612	146501.216754	37.895015
1971.260972	146724.913033	37.900032
1974.134948	146923.430767	37.905050
1976.214428	147149.742361	37.910068
1977.831623	147371.747992	37.915085
1979.761357	147583.818462	37.920103
1981.552753	147809.720841	37.925120
1982.672937	148040.348777	37.930138
1984.550892	148268.016634	37.935156
1986.211662	148517.411169	37.940173
1988.488516	148755.884045	37.945191
1990.453497	149011.643437	37.950208
1992.349990	149242.968163	37.955226
1994.837547	149476.765887	37.960244
1996.438276	149724.690374	37.965261
1998.398997	149952.441442	37.970279
2000.040549	150203.395438	37.975296
2002.306343	150454.824646	37.980314
2004.153121	150695.594433	37.985332
2005.928521	150949.209341	37.990349
2007.642099	151188.783488	37.995367
2009.186840	151440.545270	38.000384
2011.389681	151704.556555	38.005402
2013.742516	151960.916940	38.010420
2015.615986	152218.901745	38.015437
2017.523621	152463.858732	38.020455
2019.015618	152707.726358	38.025472
2021.116120	152943.071681	38.030490
2023.076740	153179.315641	38.035508
2024.544405	153431.352346	38.040525
2026.913775	153674.402169	38.045543
2028.654766	153926.462021	38.050560
2030.282596	154169.997509	38.055578
2032.728164	154428.753951	38.060596
2034.668967	154686.308015	38.065613
2037.315712	154921.932005	38.070631
2040.089360	155165.052221	38.075648
2042.017375	155406.020094	38.080666
2044.199843	155658.437784	38.085684
2045.946194	155913.920333	38.090701
2047.872072	156159.283943	38.095719
2049.493304	156415.486358	38.100736
2051.630047	156681.371811	38.105754
2054.015768	156939.031661	38.110772
2055.779050	157212.226280	38.115789
2057.889990	157454.722871	38.120807
2059.967255	157726.614207	38.125824
2061.850881	158000.631571	38.130842
2064.069951	158267.539593	38.135860
2066.214275	158537.164465	38.140877
2069.053481	158775.249449	38.145895
2071.137337	159035.935944	38.150912
2073.337549	159303.638562	38.155930
2075.604195	159563.334029	38.160948
2077.315637	159829.629672	38.165965
2079.421209	160090.685434	38.170983
2081.302900	160366.376821	38.176000
2083.359268	160637.827360	38.181018
2085.437667	160911.903617	38.186036
2087.353589	161183.606900	38.191053
2089.536802	161458.481743	38.196071
2091.594217	161748.751793	38.201088
2093.096480	162023.823933	38.206106
2094.815841	162309.591391	38.211124
2096.820866	162608.874804	38.216141
2099.387654	162907.665912	38.221159
2101.654509	163194.786726	38.226176
2103.060114	163495.322857	38.231194
2105.492795	163790.812544	38.236212
2107.812888	164082.182151	38.241229
2110.187294	164378.153302	38.246247
2112.015386	164670.097221	38.251264
2114.027003	164971.256750	38.256282
2116.800518	165265.265289	38.261300
2118.509727	165567.896550	38.266317
2121.016489	165863.358513	38.271335
2123.432535	166151.979768	38.276352
2125.300403	166438.935432	38.281370
2127.629759	166733.438441	38.286388
2129.346103	167030.640929	38.291405
2131.700068	167317.499207	38.296423
2133.909445	167617.547720	38.301440
2135.896410	167923.561553	38.306458
2138.255294	168220.618321	38.311476
2140.286685	168510.883658	38.316493
2142.520676	168799.061739	38.321511
2144.968677	169098.635010	38.326528
2146.509584	169388.459669	38.331546
2148.571122	169691.625342	38.336564
2150.164535	169997.036357	38.341581
2152.832398	170293.444150	38.346599
2154.994556	170609.803116	38.351616
2157.242128	170917.833380	38.356634
2159.173103	171204.988873	38.361652
2161.516909	171499.521929	38.366669
2163.394724	171774.701490	38.371687
2165.512259	172053.095320	38.376704
2167.324991	172337.543571	38.381722
2169.874260	172611.085264	38.386740
2171.678542	172904.311009	38.391757
2173.601489	173199.614530	38.396775
2176.021528	173499.755858	38.401792
2178.111984	173774.693651	38.406810
2180.594617	174057.355173	38.411828
2182.597351	174353.145859	38.416845
2184.836963	174647.948438	38.421863
2186.930382	174953.885626	38.426880
2188.965787	175267.870888	38.431898
2191.402924	175550.633681	38.436916
2193.258954	175860.915918	38.441933
2195.646228	176165.300881	38.446951
2197.475187	176488.326015	38.451968
2199.679512	176800.906780	38.456986
2201.579706	177112.050345	38.462004
2204.053979	177445.327927	38.467021
2205.914585	177761.407041	38.472039
2208.249149	178086.835858	38.477056
2210.074314	178418.999232	38.482074
2212.692131	178764.907400	38.487092
2214.421527	179092.059624	38.492109
2216.743225	179434.359332	38.497127
2219.112862	179773.325842	38.502144
2221.168678	180119.809381	38.507162
2223.452062	180452.899669	38.512180
2225.915683	180799.855727	38.517197
2228.154599	181147.229055	38.522215
2230.833002	181493.062227	38.527232
2232.720417	181829.546321	38.532250
2235.135438	182170.648188	38.537268
2237.778612	182523.602176	38.542285
2240.611224	182843.103785	38.547303
2244.158623	183168.997229	38.552320
2246.302810	183497.497625	38.557338
2248.761231	183815.689204	38.562356
2250.475690	184139.686913	38.567373
2253.242280	184448.104906	38.572391
2256.056269	184754.306790	38.577408
2258.314970	185078.400681	38.582426
2260.431018	185390.021514	38.587444
2262.435976	185706.867411	38.592461
2264.654540	186016.721684	38.597479
2267.210382	186404.246097	38.602496
2268.702954	186734.026935	38.607514
2270.673546	187057.105176	38.612532
2272.674441	187390.949080	38.617549
2274.524543	187715.165664	38.622567
2277.483014	188055.110920	38.627584
2279.127162	188397.065174	38.632602
2281.375158	188729.731794	38.637620
2283.410305	189076.148487	38.642637
2286.101185	189421.524413	38.647655
2288.803543	189759.584407	38.652672
2290.650722	190094.730488	38.657690
2293.092306	190430.470853	38.662708
2295.544926	190771.874740	38.667725
2297.620079	191110.798339	38.672743
2300.242188	191447.123156	38.677760
2302.413140	191782.630123	38.682778
2304.960074	192112.923204	38.687796
2307.269538	192446.505426	38.692813
2309.502295	192786.984085	38.697831
2312.111762	193106.551032	38.702848
2314.166711	193427.449738	38.707866
2316.532329	193728.513623	38.712884
2318.805777	194045.772970	38.717901
2320.366466	194352.602606	38.722919
2322.331543	194669.225652	38.727936
2324.459123	195003.350958	38.732954
2326.645464	195318.163053	38.737972
2328.580583	195662.836064	38.742989
2330.751552	196008.489303	38.748007
2333.114061	196351.649674	38.753024
2334.905586	196703.866470	38.758042
2337.154936	197056.800349	38.763060
2339.290029	197414.731599	38.768077
2341.614185	197782.058330	38.773095
2343.860802	198148.407391	38.778112
2346.369339	198523.759632	38.783130
2348.333243	198897.343243	38.788148
2351.023645	199277.114386	38.793165
2353.277097	199666.785029	38.798183
2355.694866	200038.827472	38.803200
2357.774622	200435.207787	38.808218
2359.863561	200813.704541	38.813236
2362.780733	201207.797246	38.818253
2365.203002	201596.608032	38.823271
2368.282546	201972.768680	38.828288
2371.052812	202372.450088	38.833306
2373.973995	202745.893614	38.838324
2376.306335	203119.353362	38.843341
2378.502648	203505.409315	38.848359
2381.025040	203875.183081	38.853376
2383.507492	204260.891258	38.858394
2385.923920	204632.080155	38.863412
2388.499724	205020.671251	38.868429
2390.641089	205389.745172	38.873447
2393.464772	205780.153590	38.878464
2395.800530	206161.112608	38.883482
2397.973262	206538.998540	38.888500
2400.680985	206925.794545	38.893517
2403.091981	207306.566100	38.898535
2405.622308	207685.795560	38.903552
2408.082384	208083.174416	38.908570
2410.520191	208456.805475	38.913588
2413.315348	208830.457727	38.918605
2415.168412	209224.274924	38.923623
2417.880717	209605.003364	38.928640
2420.102415	209991.905528	38.933658
2422.990153	210368.009811	38.938676
2426.000852	210746.610432	38.943693
2428.622642	211126.110420	38.948711
2431.177277	211492.030531	38.953728
2433.094567	211881.929580	38.958746
2435.559416	212245.400484	38.963764
2438.476905	212610.935285	38.968781
2440.728402	212988.056584	38.973799
2443.113351	213363.557137	38.978816
2444.707797	213746.497391	38.983834
2447.528280	214120.711647	38.988852
2450.026483	214509.151724	38.993869
2452.263008	214893.136485	38.998887
2454.567955	215276.196459	39.003904
2456.618141	215670.804371	39.008922
2458.767325	216058.716067	39.013940
2460.747056	216449.804569	39.018957
2463.473421	216854.368288	39.023975
2465.597418	217265.986770	39.028992
2467.892582	217676.740644	39.034010
2469.988498	218071.927864	39.039028
2472.615476	218476.914864	39.044045
2474.839797	218880.669224	39.049063
2477.426880	219251.774123	39.054080
2479.688106	219639.823602	39.059098
2482.212976	220039.416503	39.064116
2484.105244	220428.514608	39.069133
2486.580681	220837.515124	39.074151
2488.628841	221238.630879	39.079168
2491.521702	221646.423644	39.084186
2493.610991	222067.094471	39.089204
2496.226771	222471.780585	39.094221
2498.618772	222892.175973	39.099239
2501.528720	223313.278412	39.104256
2503.775728	223734.687363	39.109274
2506.517024	224153.072610	39.114292
2509.207358	224568.722220	39.119309
2511.642349	224996.097506	39.124327
2514.748988	225425.019574	39.129344
2517.336988	225859.458851	39.134362
2519.303180	226278.041123	39.139380
2522.279214	226702.232953	39.144397
2525.101085	227146.136910	39.149415
2527.838432	227566.123307	39.154432
2530.252292	227992.536398	39.159450
2532.342288	228429.567891	39.164468
2534.864342	228854.414286	39.169485
2537.837437	229307.058612	39.174503
2541.014920	229731.955138	39.179520
2543.227620	230147.195675	39.184538
2545.912349	230583.778170	39.189556
2548.889547	231019.044729	39.194573
2551.670022	231443.519560	39.199591
2554.790032	231859.151525	39.204608
2557.914420	232282.581575	39.209626
2561.031835	232689.753899	39.214644
2563.820519	233087.780878	39.219661
2565.833663	233510.443048	39.224679
2568.658585	233908.870255	39.229696
2571.413380	234316.021593	39.234714
2573.369828	234741.409776	39.239732
2576.062267	235148.722521	39.244749
2578.424205	235566.806729	39.249767
2580.627733	235983.975234	39.254784
2583.298674	236407.650140	39.259802
2586.179380	236818.869517	39.264820
2589.146989	237230.430568	39.269837
2591.410803	237651.118975	39.274855
2594.125564	238069.729807	39.279872
2596.622736	238494.064384	39.284890
2599.281077	238913.953102	39.289908
2602.069316	239332.195215	39.294925
2604.279545	239765.108310	39.299943
2606.598311	240190.586066	39.304960
2609.329279	240617.065983	39.309978
2611.983270	241037.358797	39.314996
2614.912343	241460.986790	39.320013
2617.242286	241904.217070	39.325031
2619.427688	242330.855342	39.330048
2621.639990	242773.035459	39.335066
2623.880291	243213.838639	39.340084
2626.603455	243650.374336	39.345101
2628.989487	244113.380855	39.350119
2632.009032	244554.949298	39.355136
2634.684715	245011.329480	39.360154
2636.942864	245463.531378	39.365172
2639.728706	245908.486570	39.370189
2641.842593	246358.295683	39.375207
2644.307341	246813.256740	39.380224
2646.995089	247267.521562	39.385242
2649.445977	247700.966616	39.390260
2651.873217	248127.200018	39.395277
2654.772466	248569.286341	39.400295
2657.209818	249005.753313	39.405312
2659.529669	249446.860721	39.410330
2661.900380	249885.063229	39.415348
2665.081914	250342.444126	39.420365
2667.692995	250792.977752	39.425383
2670.209811	251247.589142	39.430400
2672.566277	251693.765328	39.435418
2675.122570	252156.191807	39.440436
2677.918816	252615.277325	39.445453
2680.345176	253098.601531	39.450471
2683.092384	253558.022041	39.455488
2686.025548	254032.018120	39.460506
2688.414021	254515.089561	39.465524
2691.178109	254992.106166	39.470541
2693.299300	255489.161273	39.475559
2696.491885	255974.896695	39.480576
2698.938017	256478.959191	39.485594
2701.829776	256973.018607	39.490612
2704.461408	257462.341256	39.495629
2707.425309	257965.657041	39.500647
2710.014300	258458.106834	39.505664
2712.795276	258959.186451	39.510682
2715.920356	259468.821283	39.515700
2718.942118	259968.563867	39.520717
2721.928781	260475.345729	39.525735
2724.186264	260978.708252	39.530752
2727.298818	261479.116112	39.535770
2729.906529	261995.348376	39.540788
2732.867939	262489.730103	39.545805
2735.640331	262995.670566	39.550823
2738.687062	263504.182177	39.555840
2741.259714	264006.796278	39.560858
2744.183128	264517.735254	39.565876
2747.034581	265010.624029	39.570893
2749.750472	265523.393754	39.575911
2752.563116	266032.539198	39.580928
2755.741017	266535.808888	39.585946
2758.552126	267046.473395	39.590964
2760.878631	267554.848605	39.595981
2764.367979	268055.217457	39.600999
2767.198448	268559.496019	39.606016
2770.540287	269052.618683	39.611034
2772.996257	269551.997588	39.616052
2775.887209	270056.055564	39.621069
2778.701358	270550.852511	39.626087
2781.621431	271048.855807	39.631104
2784.190283	271545.539542	39.636122
2787.047892	272045.553443	39.641140
2790.070543	272534.567186	39.646157
2793.250323	273037.090439	39.651175
2795.673610	273527.029980	39.656192
2798.891192	274019.154226	39.661210
2801.492977	274518.939672	39.666228
2804.723065	275009.659368	39.671245
2807.095873	275508.966584	39.676263
2809.694671	275997.619954	39.681280
2812.925875	276488.990946	39.686298
2815.127301	276986.233288	39.691316
2817.908097	277485.642599	39.696333
2821.117791	277973.503174	39.701351
2824.038214	278461.735866	39.706368
2826.425735	278956.397247	39.711386
2829.981917	279452.981379	39.716404
2832.896451	279941.129400	39.721421
2835.185205	280423.733989	39.726439
2838.145286	280882.512360	39.731456
2841.332883	281329.418634	39.736474
2843.369849	281796.435835	39.741492
2846.035947	282248.623499	39.746509
2849.232089	282715.124280	39.751527
2851.627117	283191.091642	39.756544
2854.379003	283658.366425	39.761562
2856.304635	284135.035338	39.766580
2859.102650	284615.983693	39.771597
2862.079033	285107.083627	39.776615
2864.500176	285599.663078	39.781632
2867.377521	286093.031339	39.786650
2869.704397	286607.786083	39.791668
2872.420686	287119.911648	39.796685
2875.072085	287643.088992	39.801703
2878.124515	288165.590375	39.806720
2880.896943	288685.363451	39.811738
2883.786354	289224.487967	39.816756
2886.412126	289765.426392	39.821773
2889.517526	290308.113759	39.826791
2892.099492	290847.500929	39.831808
2895.481285	291396.128182	39.836826
2898.666805	291948.869015	39.841844
2901.811245	292485.006036	39.846861
2904.335163	293035.021733	39.851879
2907.427605	293586.010348	39.856896
2910.286682	294139.797704	39.861914
2913.395274	294700.320057	39.866932
2916.457855	295244.544446	39.871949
2919.397650	295808.053070	39.876967
2922.363659	296371.272892	39.881984
2925.668895	296919.709171	39.887002
2928.571661	297484.705135	39.892020
2931.721014	298049.327076	39.897037
2934.708770	298608.484790	39.902055
2937.651750	299169.674883	39.907072
2940.822024	299734.403528	39.912090
2943.494686	300307.251466	39.917108
2946.673464	300852.571735	39.922125
2949.509148	301416.192709	39.927143
2952.674104	301982.422094	39.932160
2955.911516	302540.916930	39.937178
2958.615486	303109.719284	39.942196
2961.997876	303671.708223	39.947213
2965.483419	304230.527340	39.952231
2967.930165	304791.761345	39.957248
2971.722928	305348.032898	39.962266
2974.871441	305905.388653	39.967284
2977.740682	306457.425763	39.972301
2980.942349	307000.647766	39.977319
2983.222979	307556.140461	39.982336
2986.193348	308117.027761	39.987354
2989.102212	308669.998859	39.992372
2992.592508	309227.264433	39.997389
2995.046170	309793.619500	40.002407
2997.940775	310360.635420	40.007424
3001.048088	310920.580870	40.012442
3004.203204	311496.096451	40.017460
3007.242572	312053.298010	40.022477
3010.616929	312614.019548	40.027495
3013.454563	313174.843294	40.032512
3016.325547	313723.726470	40.037530
3019.531894	314291.890354	40.042548
3022.626246	314844.633944	40.047565
3025.379697	315409.301356	40.052583
3028.511960	315975.806224	40.057600
3031.641643	316526.747358	40.062618
3034.450907	317101.561738	40.067636
3037.135304	317626.774371	40.072653
3040.340945	318158.878517	40.077671
3043.178162	318684.130954	40.082688
3045.872536	319213.941813	40.087706
3048.714271	319755.498087	40.092724
3051.202214	320292.128888	40.097741
3054.594803	320827.521068	40.102759
3057.283491	321380.322341	40.107776
3060.459992	321947.961263	40.112794
3063.488468	322499.274088	40.117812
3066.693478	323051.770215	40.122829
3069.014094	323605.843020	40.127847
3072.108378	324182.066466	40.132864
3074.969181	324767.021396	40.137882
3077.693065	325346.381821	40.142900
3080.479103	325936.939217	40.147917
3083.616050	326526.317041	40.152935
3086.468487	327137.043197	40.157952
3090.046668	327740.060968	40.162970
3092.927986	328356.599563	40.167988
3096.622335	328948.036975	40.173005
3099.100024	329560.306566	40.178023
3102.860919	330165.618439	40.183040
3106.417700	330767.781451	40.188058
3109.484304	331384.116815	40.193076
3112.360143	331995.728004	40.198093
3115.764775	332610.824132	40.203111
3118.822212	333237.988905	40.208128
3122.094455	333850.675590	40.213146
3125.151690	334470.640849	40.218164
3128.606957	335094.338957	40.223181
3132.188936	335706.997820	40.228199
3135.268265	336329.998052	40.233216
3138.706195	336944.459800	40.238234
3141.813912	337562.133285	40.243252
3144.890058	338184.874177	40.248269
3148.439001	338804.309511	40.253287
3151.494690	339433.449255	40.258304
3154.832044	340042.978842	40.263322
3158.069232	340656.698499	40.268340
3161.598791	341269.372886	40.273357
3165.625129	341873.437610	40.278375
3168.497068	342496.337829	40.283392
3171.453130	343091.772882	40.288410
3174.589488	343699.292166	40.293428
3178.035165	344313.599941	40.298445
3181.423070	344923.721316	40.303463
3184.421058	345541.677843	40.308480
3187.234997	346146.541135	40.313498
3190.986689	346755.533285	40.318516
3193.817627	347367.421727	40.323533
3197.409369	347968.251425	40.328551
3200.797346	348570.243063	40.333568
3204.110938	349182.149835	40.338586
3207.191569	349791.038745	40.343604
3210.079179	350404.738641	40.348621
3213.511735	351009.239629	40.353639
3216.708794	351617.518533	40.358656
3220.066884	352228.727396	40.363674
3223.283291	352842.837038	40.368692
3226.021312	353451.304820	40.373709
3229.270007	354066.197220	40.378727
3232.013054	354676.085888	40.383744
3234.835426	355302.023563	40.388762
3238.328475	355930.658404	40.393780
3241.370644	356549.844158	40.398797
3244.765806	357179.888685	40.403815
3247.739788	357806.208788	40.408832
3250.495672	358394.449934	40.413850
3254.037568	358973.761398	40.418868
3256.564975	359575.171490	40.423885
3260.468376	360176.304861	40.428903
3263.990608	360775.331062	40.433920
3266.997840	361370.522056	40.438938
3270.307699	361973.993114	40.443956
3273.236884	362568.209253	40.448973
3276.424319	363176.059841	40.453991
3279.068675	363792.701083	40.459008
3282.304077	364423.861119	40.464026
3285.247389	365050.161666	40.469044
3287.829063	365689.886272	40.474061
3291.551384	366332.941921	40.479079
3294.380602	366981.773528	40.484096
3297.213172	367637.026731	40.489114
3300.756977	368307.257460	40.494132
3304.042648	368978.551549	40.499149
3307.851134	369643.717540	40.504167
3310.435754	370325.123312	40.509184
3314.180742	371003.696792	40.514202
3317.988596	371696.610601	40.519220
3320.747312	372369.932695	40.524237
3324.142422	373053.375399	40.529255
3328.009750	373745.949983	40.534272
3331.168463	374428.761899	40.539290
3334.738249	375120.461271	40.544308
3338.566737	375814.661528	40.549325
3341.904178	376506.311040	40.554343
3345.238856	377199.260526	40.559360
3348.613852	377893.401767	40.564378
3351.919274	378596.427118	40.569396
3355.119543	379283.871790	40.574413
3359.313202	379975.272816	40.579431
3362.810211	380671.905960	40.584448
3366.686125	381366.283341	40.589466
3370.254850	382060.588720	40.594484
3373.282334	382751.717842	40.599501
3376.749140	383446.685769	40.604519
3380.078533	384148.848910	40.609536
3383.630298	384844.550882	40.614554
3387.545539	385554.156530	40.619572
3390.719594	386245.700393	40.624589
3394.514629	386934.317821	40.629607
3397.905227	387631.209177	40.634624
3401.528974	388319.258176	40.639642
3405.449762	389010.685654	40.644660
3408.604103	389698.794886	40.649677
3412.458609	390363.962895	40.654695
3415.718135	391055.841216	40.659712
3419.473778	391737.292922	40.664730
3422.619795	392416.440616	40.669748
3426.198614	393100.514760	40.674765
3429.870053	393775.137524	40.679783
3432.990192	394465.522843	40.684800
3436.094399	395139.183029	40.689818
3440.018086	395818.417715	40.694836
3442.997925	396509.727821	40.699853
3446.613509	397188.009419	40.704871
3449.803412	397869.881459	40.709888
3453.424772	398552.527189	40.714906
3457.043481	399236.267113	40.719924
3460.447045	399932.979054	40.724941
3464.004425	400610.057074	40.729959
3467.247346	401296.072721	40.734976
3470.789420	401996.193582	40.739994
3474.069948	402680.289388	40.745012
3477.347912	403351.111577	40.750016
3480.696895	403987.689313	40.755021
3483.399178	404589.695454	40.760026
3486.706879	405150.342014	40.765031
3490.019756	405661.506170	40.770036
3492.438077	406122.722443	40.775040
3495.215938	406533.798735	40.780045
3497.629177	406893.683605	40.785050
3500.053674	407210.184578	40.790055
3501.975496	407484.702496	40.795060
3503.942980	407723.748668	40.800064
3505.948490	407910.330537	40.805069
3507.299090	408066.320715	40.810074
3509.040392	408181.360331	40.815079
3510.473158	408255.913943	40.820084
3511.464607	408313.947240	40.825088
3512.398673	408330.644353	40.830093
3513.259577	408333.199158	40.835098
3514.276508	408317.619048	40.840103
3515.293187	408270.281886	40.845108
3515.689423	408201.835894	40.850112
3516.360360	408129.085581	40.855117
3516.658917	408025.751623	40.860122
3517.264566	407911.766618	40.865127
3517.767979	407773.750302	40.870132
3517.760486	407642.357016	40.875136
3518.055646	407486.513789	40.880141
3518.323890	407325.194568	40.885146
3518.452268	407154.053798	40.890151
3518.556275	406978.450994	40.895156
3518.507308	406807.030767	40.900160
3518.731199	406604.466856	40.905165
3518.860135	406422.615534	40.910170
3518.734252	406231.467185	40.915175
3518.624456	406017.737505	40.920180
3518.176310	405821.359343	40.925184
3518.006226	405615.702207	40.930189
3518.033237	405414.426615	40.935194
3518.057335	405210.257665	40.940199
3518.308096	405003.666932	40.945204
3517.716038	404797.712847	40.950208
3517.169141	404588.654809	40.955213
3517.166164	404386.309225	40.960218
3517.091051	404184.328239	40.965223
3517.073978	403979.647211	40.970228
3516.772318	403785.968539	40.975232
3516.222903	403583.700843	40.980237
3516.014938	403386.655304	40.985242
3515.949299	403184.917685	40.990247
3515.911354	402994.946139	40.995252
3515.656749	402801.353271	41.000256
3515.411065	402606.488805	41.005261
3514.904034	402417.143634	41.010266
3514.876528	402244.670692	41.015271
3514.573561	402053.616224	41.020276
3514.336920	401883.405859	41.025280
3514.385309	401694.323513	41.030285
3514.155150	401512.894766	41.035290
3513.815573	401339.245715	41.040295
3513.719730	401156.930591	41.045300
3513.580405	400997.913439	41.050304
3513.025514	400831.043356	41.055309
3512.667097	400663.684771	41.060314
3512.184030	400495.329424	41.065319
3512.168969	400340.703463	41.070324
3511.962662	400194.428946	41.075328
3511.715735	400045.673150	41.080333
3511.739720	399895.808520	41.085338
3511.900251	399750.184610	41.090343
3511.782881	399598.716090	41.095348
3511.353170	399457.089913	41.100352
3511.331042	399308.751181	41.105357
3510.803898	399151.811759	41.110362
3510.877966	399022.132417	41.115367
3510.505285	398871.104917	41.120372
3509.729620	398736.785618	41.125376
3509.990305	398606.262912	41.130381
3510.059592	398488.761764	41.135386
3509.673259	398369.402345	41.140391
3509.675576	398243.688535	41.145396
3509.273473	398125.345379	41.150400
3509.174037	397996.448660	41.155405
3508.925179	397891.682283	41.160410
3509.039763	397768.181606	41.165415
3509.020360	397648.406157	41.170420
3508.747828	397543.895687	41.175424
3508.618154	397430.125258	41.180429
3508.446884	397328.034277	41.185434
3508.015732	397220.704812	41.190439
3508.131481	397113.188245	41.195444
3508.193061	397021.565970	41.200448
3508.505652	396911.936899	41.205453
3507.938988	396810.514279	41.210458
3507.569411	396714.339154	41.215463
3507.924095	396613.838190	41.220468
3507.364817	396521.193964	41.225472
3507.460904	396420.732424	41.230477
3507.490570	396328.401849	41.235482
3507.065273	396235.532633	41.240487
3507.448424	396153.094698	41.245492
3506.953056	396057.342544	41.250496
3507.114609	395961.995353	41.255501
3506.863983	395870.366465	41.260506
3506.547564	395789.102042	41.265511
3507.405155	395698.772017	41.270516
3506.689836	395624.319909	41.275520
3506.712661	395528.231202	41.280525
3506.495577	395448.878977	41.285530
3506.732655	395369.049747	41.290535
3506.555779	395286.899004	41.295540
3505.841763	395201.126160	41.300544
3506.151336	395121.944691	41.305549
3505.898380	395059.398027	41.310554
3506.003257	394995.425013	41.315559
3506.014745	394918.522673	41.320564
3505.548670	394845.298342	41.325568
3505.780051	394769.884098	41.330573
3505.860993	394700.584234	41.335578
3505.305851	394631.078591	41.340583
3505.411171	394563.601904	41.345588
3505.794934	394509.583980	41.350592
3505.692136	394440.616521	41.355597
3505.470196	394373.596311	41.360602
3505.367185	394303.308713	41.365607
3505.404993	394231.323882	41.370612
3505.020001	394176.460378	41.375616
3504.766928	394101.068665	41.380621
3505.102104	394046.549650	41.385626
3504.734537	393988.231230	41.390631
3505.342114	393930.471587	41.395636
3504.794780	393876.749420	41.400640
3504.535842	393802.626730	41.405645
3505.133658	393752.177897	41.410650
3504.636719	393696.213956	41.415655
3504.709851	393629.450333	41.420660
3504.784478	393583.245070	41.425664
3504.914467	393533.579254	41.430669
3504.292302	393473.420996	41.435674
3504.250889	393423.832390	41.440679
3504.677567	393355.490114	41.445684
3504.096284	393318.219150	41.450688
3504.466679	393263.895942	41.455693
3504.314454	393204.831438	41.460698
3504.476735	393169.068958	41.465703
3504.436756	393113.997062	41.470708
3504.360025	393060.047557	41.475712
3504.364200	393006.491450	41.480717
3504.482276	392954.491176	41.485722
3504.691216	392903.898038	41.490727
3504.398017	392845.971401	41.495732
3504.299925	392798.116309	41.500736
3504.466301	392750.676845	41.505741
3503.952938	392707.505731	41.510746
3504.266797	392652.885370	41.515751
3504.440166	392594.073299	41.520756
3504.387462	392553.114627	41.525760
3504.515232	392486.085533	41.530765
3504.509667	392433.697269	41.535770
3504.725037	392391.173665	41.540775
3504.155231	392336.182454	41.545780
3504.398002	392294.669718	41.550784
3504.171920	392243.787547	41.555789
3503.833284	392188.658500	41.560794
3503.826586	392140.280239	41.565799
3503.977937	392094.110970	41.570804
3504.228294	392051.378268	41.575808
3504.028246	391990.287631	41.580813
3504.104401	391951.490822	41.585818
3503.672813	391902.619784	41.590823
3503.676623	391867.235414	41.595828
3503.951464	391826.986041	41.600832
3503.953449	391776.067405	41.605837
3503.925225	391736.728070	41.610842
3503.484343	391681.156890	41.615847
3503.708986	391631.421697	41.620852
3504.054988	391606.695421	41.625856
3504.207637	391553.569917	41.630861
3504.184475	391520.676807	41.635866
3503.621728	391470.759215	41.640871
3503.954673	391406.741239	41.645876
3503.742110	391365.450082	41.650880
3503.935896	391320.744994	41.655885
3503.635963	391278.908849	41.660890
3503.637432	391242.102458	41.665895
3503.556637	391195.409179	41.670900
3503.510088	391158.711670	41.675904
3503.447852	391119.376636	41.680909
3503.693882	391078.318238	41.685914
3503.134863	391029.668356	41.690919
3503.258058	390990.101189	41.695924
3503.623503	390960.497529	41.700928
3503.601985	390927.806440	41.705933
3503.632814	390888.964234	41.710938
3503.461344	390847.462738	41.715943
3503.369168	390806.964197	41.720948
3502.729748	390770.866048	41.725952
3503.341910	390727.465519	41.730957
3503.623606	390688.330117	41.735962
3503.139292	390655.964524	41.740967
3503.297580	390616.848212	41.745972
3503.672130	390596.939492	41.750976
3503.304839	390550.289569	41.755981
3502.919225	390501.916271	41.760986
3503.085782	390476.785249	41.765991
3503.387916	390431.655534	41.770996
3503.197155	390406.935427	41.776000
3503.177990	390373.024778	41.781005
3503.383500	390345.856799	41.786010
3502.951504	390303.912622	41.791015
3503.414514	390274.521418	41.796020
3503.032111	390231.934785	41.801024
3503.219104	390195.580268	41.806029
3503.169577	390163.095600	41.811034
3503.098668	390128.024968	41.816039
3503.410725	390079.618429	41.821044
3503.018365	390065.667132	41.826048
3503.042089	390021.849235	41.831053
3503.524962	389989.357645	41.836058
3502.904295	389953.255378	41.841063
3503.111867	389913.241808	41.846068
3503.430405	389875.419405	41.851072
3503.436783	389830.537697	41.856077
3503.331191	389802.046737	41.861082
3502.690466	389765.947317	41.866087
3503.078701	389729.129251	41.871092
3503.004177	389703.908033	41.876096
3503.051853	389668.869067	41.881101
3503.157689	389637.857262	41.886106
3503.232165	389601.544767	41.891111
3503.016647	389563.551141	41.896116
3503.001990	389538.066584	41.901120
3503.130092	389494.789990	41.906125
3503.072253	389474.566872	41.911130
3502.582414	389441.921306	41.916135
3502.643504	389396.624129	41.921140
3502.888986	389363.635565	41.926144
3502.943029	389336.794676	41.931149
3503.169851	389308.860676	41.936154
3502.984605	389273.984326	41.941159
3503.145232	389238.038677	41.946164
3503.098610	389209.334774	41.951168
3502.956852	389173.816873	41.956173
3503.572539	389142.547410	41.961178
3502.884614	389105.794341	41.966183
3503.048225	389069.111795	41.971188
3502.838729	389046.982602	41.976192
3502.671377	389005.096583	41.981197
3503.079625	388969.238943	41.986202
3503.023034	388942.160984	41.991207
3502.921552	388909.809688	41.996212
3502.799123	388879.238634	42.001216
3503.125088	388849.232419	42.006221
3503.137325	388813.563109	42.011226
3502.988430	388779.238903	42.016231
3503.093900	388739.366262	42.021236
3503.095683	388713.269033	42.026240
3502.930332	388678.718773	42.031245
3502.819963	388644.083750	42.036250
3503.191731	388609.678289	42.041255
3502.809525	388579.781950	42.046260
3502.611263	388550.009269	42.051264
3502.758382	388518.405757	42.056269
3502.695511	388487.317225	42.061274
3502.605055	388459.076234	42.066279
3502.555912	388431.057261	42.071284
3502.561099	388406.000027	42.076288
3502.875978	388385.083360	42.081293
3503.033395	388348.578424	42.086298
3502.547309	388314.534528	42.091303
3502.783140	388287.765767	42.096308
3502.896249	388269.241361	42.101312
3502.783991	388228.792505	42.106317
3502.732423	388193.411491	42.111322
3502.712055	388164.524591	42.116327
3502.600970	388140.043694	42.121332
3502.598600	388114.403447	42.126336
3502.935429	388084.470784	42.131341
3502.925714	388059.567843	42.136346
3502.537705	388030.814159	42.141351
3502.723869	387995.243550	42.146356
3502.796785	387982.107220	42.151360
3502.873539	387944.725703	42.156365
3503.116739	387906.708939	42.161370
3502.985174	387875.224143	42.166375
3502.777422	387835.652672	42.171380
3502.904587	387816.922647	42.176384
3502.705516	387781.792489	42.181389
3503.001273	387748.540096	42.186394
3502.403515	387726.800183	42.191399
3502.695225	387694.665387	42.196404
3502.738358	387666.098065	42.201408
3502.950078	387636.971342	42.206413
3503.021851	387608.678759	42.211418
3502.852809	387571.918843	42.216423
3502.923963	387535.273821	42.221428
3502.701063	387507.687052	42.226432
3502.576772	387479.094795	42.231437
3502.794524	387445.752590	42.236442
3502.595412	387412.449822	42.241447
3503.005082	387393.802458	42.246452
3502.859480	387365.975016	42.251456
3502.978914	387330.439236	42.256461
3502.827182	387285.222124	42.261466
3502.281650	387258.446916	42.266471
3502.524955	387235.915617	42.271476
3502.403182	387217.985515	42.276480
3502.639660	387187.305766	42.281485
3502.485785	387156.839051	42.286490
3502.846988	387135.711033	42.291495
3502.751172	387102.493331	42.296500
3502.714516	387080.894034	42.301504
3502.640767	387051.506401	42.306509
3502.668004	387011.998616	42.311514
3502.337978	386987.626827	42.316519
3502.940371	386965.496391	42.321524
3502.697081	386933.342324	42.326528
3502.539128	386897.950650	42.331533
3502.711702	386878.222725	42.336538
3502.497444	386849.923022	42.341543
3502.961246	386818.064985	42.346548
3502.786010	386796.309291	42.351552
3502.556039	386760.192374	42.356557
3502.614047	386741.116875	42.361562
3502.652773	386710.898920	42.366567
3502.608048	386671.427188	42.371572
3502.659235	386650.296229	42.376576
3502.036821	386616.829784	42.381581
3502.439293	386595.136348	42.386586
3502.330632	386575.401174	42.391591
3502.721029	386552.567103	42.396596
3502.423213	386529.180006	42.401600
3502.595912	386501.352854	42.406605
3502.651113	386459.986495	42.411610
3502.638197	386448.462197	42.416615
3502.597452	386414.981135	42.421620
3502.337633	386390.597844	42.426624
3502.087560	386363.293322	42.431629
3502.244231	386338.743615	42.436634
3502.390376	386327.397620	42.441639
3502.335569	386280.183308	42.446644
3501.916172	386267.122694	42.451648
3501.781587	386241.678834	42.456653
3502.104005	386223.120351	42.461658
3502.225230	386204.059998	42.466663
3502.496475	386175.353934	42.471668
3502.534499	386170.955834	42.476672
3502.691313	386139.144714	42.481677
3502.518127	386119.393835	42.486682
3502.311021	386092.488557	42.491687
3502.721348	386059.444609	42.496692
3502.169740	386037.848385	42.501696
3502.386927	386014.355282	42.506701
3502.351011	385986.915473	42.511706
3502.385094	385964.237875	42.516711
3502.436703	385930.056297	42.521716
3502.203176	385910.644703	42.526720
3502.369773	385878.450897	42.531725
3502.686558	385861.568707	42.536730
3502.502447	385829.657915	42.541735
3502.694465	385805.051413	42.546740
3502.369497	385768.820917	42.551744
3502.271383	385749.794355	42.556749
3502.375464	385724.033554	42.561754
3501.973773	385717.418768	42.566759
3502.546610	385682.013230	42.571764
3502.547533	385665.484732	42.576768
3502.562169	385629.378915	42.581773
3501.904539	385598.328588	42.586778
3502.429112	385582.708736	42.591783
3502.745791	385547.723714	42.596788
3502.133163	385531.315995	42.601792
3502.207799	385506.016565	42.606797
3502.525725	385481.618662	42.611802
3502.802556	385461.797243	42.616807
3502.509095	385427.084726	42.621812
3502.025066	385405.502836	42.626816
3502.273891	385384.136950	42.631821
3501.980416	385359.046995	42.636826
3502.152842	385343.100950	42.641831
3502.559274	385310.869105	42.646836
3502.236190	385291.801039	42.651840
3502.140201	385272.012098	42.656845
3502.619529	385251.828938	42.661850
3502.298269	385228.241170	42.666855
3502.654045	385194.417506	42.671860
3502.520031	385177.427284	42.676864
3502.757495	385143.901252	42.681869
3502.611096	385122.901328	42.686874
3502.405539	385092.897187	42.691879
3502.349482	385054.287957	42.696884
3502.529816	385034.735122	42.701888
3502.435832	385003.088557	42.706893
3502.239349	384976.739023	42.711898
3501.867067	384954.910851	42.716903
3501.915094	384922.658117	42.721908
3502.006898	384921.450578	42.726912
3502.197031	384891.892427	42.731917
3502.502355	384878.743711	42.736922
3501.944942	384857.426676	42.741927
3502.016121	384838.169966	42.746932
3502.368616	384824.861541	42.751936
3501.889184	384794.087183	42.756941
3501.937416	384769.273544	42.761946
3502.085855	384757.697981	42.766951
3502.224890	384735.282249	42.771956
3502.115230	384710.569293	42.776960
3502.510504	384688.443720	42.781965
3502.103214	384667.737921	42.786970
3501.811039	384660.978865	42.791975
3502.264737	384622.289657	42.796980
3502.359553	384605.466568	42.801985
3502.282312	384592.656531	42.806989
3502.051756	384559.456465	42.811994
3501.863395	384538.665713	42.816999
3501.959136	384509.528056	42.822004
3501.953964	384502.571954	42.827009
3502.005767	384488.929289	42.832013
3502.324276	384463.362361	42.837018
3502.278130	384444.174394	42.842023
3502.408780	384409.749962	42.847028
3502.309282	384390.874944	42.852033
3502.187074	384367.712435	42.857037
3502.299200	384342.431408	42.862042
3502.277231	384321.106774	42.867047
3502.484835	384304.570624	42.872052
3501.998176	384289.996018	42.877057
3501.985600	384259.478445	42.882061
3502.421811	384234.832430	42.887066
3502.051494	384210.819712	42.892071
3502.342554	384197.418959	42.897076
3502.261159	384177.220646	42.902081
3502.178896	384155.270487	42.907085
3502.345396	384124.140898	42.912090
3501.908931	384108.593525	42.917095
3502.085301	384078.655715	42.922100
3501.985012	384063.106784	42.927105
3502.125888	384037.008474	42.932109
3502.194044	384015.948862	42.937114
3501.950207	384001.463259	42.942119
3502.307545	383969.745185	42.947124
3501.850846	383942.343265	42.952129
3502.120658	383929.580454	42.957133
3501.968388	383908.986703	42.962138
3501.950237	383901.829329	42.967143
3502.333209	383869.421583	42.972148
3502.014920	383852.103680	42.977153
3501.803828	383825.323583	42.982157
3501.930214	383809.891572	42.987162
3502.079830	383795.090716	42.992167
3502.067974	383762.261843	42.997172
3502.079339	383753.627146	43.002177
3502.009679	383733.502831	43.007181
3502.160585	383707.402626	43.012186
3502.124489	383689.913744	43.017191
3502.059724	383668.722184	43.022196
3502.472275	383649.538417	43.027201
3502.473621	383630.418625	43.032205
3502.333857	383604.871374	43.037210
3502.153596	383587.938075	43.042215
3502.677403	383558.148725	43.047220
3502.442315	383531.397448	43.052225
3502.089898	383503.851874	43.057229
3502.377833	383483.620935	43.062234
3502.102403	383458.196216	43.067239
3502.175640	383434.824711	43.072244
3502.129037	383416.550141	43.077249
3501.989333	383395.243059	43.082253
3502.003939	383375.765533	43.087258
3501.948614	383352.261609	43.092263
3502.100029	383335.606622	43.097268
3501.830842	383316.884178	43.102273
3501.950936	383294.851011	43.107277
3502.359142	383273.890226	43.112282
3502.375127	383248.166034	43.117287
3502.420598	383214.921276	43.122292
3502.087772	383198.773215	43.127297
3502.313947	383179.973586	43.132301
3502.352464	383158.892493	43.137306
3502.106273	383132.548798	43.142311
3502.484805	383107.275886	43.147316
3502.351218	383083.326843	43.152321
3502.474739	383071.881359	43.157325
3502.395528	383047.314415	43.162330
3502.001437	383021.145973	43.167335
3502.556381	382985.764894	43.172340
3502.479288	382966.555247	43.177345
3502.254360	382935.180429	43.182349
3502.335581	382910.664567	43.187354
3501.985918	382889.821404	43.192359
3501.906124	382871.653182	43.197364
3502.284217	382850.747524	43.202369
3501.924639	382837.523489	43.207373
3502.132774	382809.458278	43.212378
3502.057387	382790.324412	43.217383
3502.310886	382770.072881	43.222388
3502.075283	382750.456074	43.227393
3501.962557	382732.749938	43.232397
3502.108558	382698.143084	43.237402
3501.815288	382687.473270	43.242407
3502.316466	382659.336904	43.247412
3502.317275	382637.804193	43.252417
3502.213492	382608.314549	43.257421
3502.125190	382594.083267	43.262426
3501.859328	382583.536107	43.267431
3502.307587	382557.464645	43.272436
3502.137676	382532.911327	43.277441
3502.064080	382512.812066	43.282445
3502.282976	382482.408723	43.287450
3502.179692	382470.236493	43.292455
3501.929420	382448.564949	43.297460
3502.024002	382420.872482	43.302465
3501.973408	382409.707725	43.307469
3502.453892	382374.997606	43.312474
3502.106465	382357.530876	43.317479
3502.075458	382331.609946	43.322484
3501.924038	382324.142768	43.327489
3501.507383	382294.269779	43.332493
3502.086677	382288.669510	43.337498
3502.059731	382266.836098	43.342503
3502.036781	382249.217232	43.347508
3502.076018	382223.209084	43.352513
3501.858326	382212.247993	43.357517
3502.071447	382181.184986	43.362522
3501.616472	382169.524412	43.367527
3501.689119	382138.610177	43.372532
3502.026122	382133.606219	43.377537
3501.808306	382113.300555	43.382541
3501.919942	382100.332922	43.387546
3502.087241	382085.045873	43.392551
3501.831390	382057.966194	43.397556
3502.264722	382039.946076	43.402561
3502.302800	382023.231703	43.407565
3502.352024	381999.050067	43.412570
3502.198324	381974.341340	43.417575
3501.938023	381947.439988	43.422580
3502.270783	381932.609568	43.427585
3501.961344	381912.419577	43.432589
3501.806139	381896.827100	43.437594
3501.548202	381878.279614	43.442599
3501.530696	381854.133620	43.447604
3502.081247	381837.999601	43.452609
3501.715400	381817.259666	43.457613
3502.039726	381803.598567	43.462618
3501.839413	381792.761560	43.467623
3501.917579	381775.228211	43.472628
3501.822921	381754.522204	43.477633
3501.540540	381738.644705	43.482637
3501.690179	381708.098875	43.487642
3501.653701	381700.969137	43.492647
3501.611904	381684.419336	43.497652
3501.868426	381668.584900	43.502657
3501.464635	381656.586018	43.507661
3501.520004	381645.404443	43.512666
3501.510150	381632.988742	43.517671
3501.679316	381619.199332	43.522676
3502.128388	381601.963655	43.527681
3501.691076	381590.731757	43.532685
3502.100962	381575.127333	43.537690
3502.021400	381541.671347	43.542695
3502.134726	381530.556884	43.547700
3501.966269	381506.586418	43.552705
3502.207604	381487.986354	43.557709
3502.162602	381463.895064	43.562714
3501.990382	381443.962683	43.567719
3502.175604	381417.245390	43.572724
3502.133701	381394.804130	43.577729
3501.340708	381388.579229	43.582733
3501.572937	381372.494459	43.587738
3501.715816	381351.979710	43.592743
3501.899833	381335.521516	43.597748
3501.409521	381315.181452	43.602753
3501.859487	381304.877890	43.607757
3501.720424	381288.393761	43.612762
3501.829291	381267.884240	43.617767
3501.702618	381264.120378	43.622772
3501.787717	381237.951748	43.627777
3501.993791	381226.213275	43.632781
3502.030341	381211.682477	43.637786
3501.678497	381197.821559	43.642791
3501.820301	381177.713141	43.647796
3501.797808	381151.332623	43.652801
3501.864621	381148.655961	43.657805
3501.934297	381121.067564	43.662810
3501.874928	381114.372922	43.667815
3501.960782	381098.031429	43.672820
3501.662643	381075.299649	43.677825
3501.589545	381062.055522	43.682829
3502.064622	381033.794496	43.687834
3501.482096	381023.473735	43.692839
3501.821072	380992.719849	43.697844
3501.655391	380992.847286	43.702849
3501.452593	380982.619782	43.707853
3501.773002	380957.607769	43.712858
3501.887078	380958.072581	43.717863
3502.073084	380934.148006	43.722868
3502.324881	380914.682512	43.727873
3501.811741	380892.034818	43.732877
3501.561861	380873.942455	43.737882
3501.713945	380855.076497	43.742887
3501.810818	380834.136803	43.747892
3501.678514	380830.297573	43.752897
3501.564648	380797.430036	43.757901
3501.876440	380798.371966	43.762906
3501.813361	380778.168153	43.767911
3501.933223	380755.726566	43.772916
3501.671303	380743.400455	43.777921
3501.647283	380721.819237	43.782925
3501.754531	380718.501384	43.787930
3501.659468	380698.607217	43.792935
3502.180899	380681.410464	43.797940
3501.961493	380673.877209	43.802945
3501.690314	380651.293231	43.807949
3501.966712	380634.947193	43.812954
3501.613749	380610.242788	43.817959
3501.591080	380594.679697	43.822964
3501.614846	380588.276716	43.827969
3501.309888	380568.719843	43.832973
3501.545563	380557.078042	43.837978
3501.832642	380545.529815	43.842983
3502.137074	380528.925405	43.847988
3502.299984	380515.441121	43.852993
3501.723862	380490.568174	43.857997
3501.723257	380465.758013	43.863002
3501.621884	380466.332544	43.868007
3501.950455	380445.051752	43.873012
3501.881009	380423.629724	43.878017
3501.721508	380410.525685	43.883021
3501.902057	380380.075074	43.888026
3501.900920	380366.794003	43.893031
3502.084586	380351.909707	43.898036
3501.904286	380336.802700	43.903041
3501.933778	380321.561460	43.908045
3501.872016	380290.005697	43.913050
3501.716952	380284.595463	43.918055
3501.928080	380254.901787	43.923060
3501.812142	380243.619298	43.928065
3501.959500	380218.506538	43.933069
3502.067953	380204.928990	43.938074
3501.907930	380179.787841	43.943079
3502.164875	380163.977827	43.948084
3501.912612	380143.675991	43.953089
3501.990430	380128.579488	43.958093
3502.272691	380107.483393	43.963098
3502.131276	380092.217826	43.968103
3501.875189	380063.866378	43.973108
3502.176835	380044.113140	43.978113
3502.300693	380023.270181	43.983117
3502.035865	380003.681248	43.988122
3502.117295	379982.235382	43.993127
3501.911545	379953.495058	43.998132
3501.869695	379941.413669	44.003137
3501.322051	379930.223620	44.008141
3501.521706	379904.289784	44.013146
3501.285469	379892.924285	44.018151
3501.717474	379892.374634	44.023156
3501.362866	379861.371827	44.028161
3501.879881	379856.491796	44.033165
3501.693717	379840.902912	44.038170
3501.233788	379827.819937	44.043175
3501.876670	379812.762297	44.048180
3501.920033	379809.022556	44.053185
3502.180621	379775.460596	44.058189
3502.019130	379761.975617	44.063194
3501.941743	379747.715690	44.068199
3501.942828	379716.911314	44.073204
3501.614231	379701.903204	44.078209
3501.403302	379688.756018	44.083213
3502.047525	379664.911356	44.088218
3501.701135	379656.711899	44.093223
3501.474512	379639.199156	44.098228
3501.673566	379616.210976	44.103233
3501.291276	379612.664420	44.108237
3501.518713	379600.058460	44.113242
3501.604355	379590.242643	44.118247
3501.265924	379570.487075	44.123252
3501.520129	379561.025945	44.128257
3501.253038	379545.093945	44.133261
3501.838368	379526.540546	44.138266
3501.598512	379527.644553	44.143271
3501.773229	379518.449731	44.148276
3501.545225	379494.105762	44.153281
3501.526562	379484.483904	44.158285
3501.730852	379457.126768	44.163290
3501.532480	379452.002451	44.168295
3501.424743	379439.143827	44.173300
3501.173743	379409.343345	44.178305
3501.229002	379409.715757	44.183309
3501.148919	379402.592179	44.188314
3501.517244	379398.598649	44.193319
3501.440733	379385.201835	44.198324
3501.786390	379364.628587	44.203329
3501.673146	379355.808660	44.208333
3502.031322	379332.871659	44.213338
3501.843427	379317.257339	44.218343
3501.827405	379304.968474	44.223348
3501.632826	379294.002563	44.228353
3501.764813	379280.446274	44.233357
3501.875277	379263.718880	44.238362
3501.277479	379250.809446	44.243367
3501.121672	379247.760904	44.248372
3501.882058	379233.141772	44.253377
3501.212503	379219.862555	44.258381
3501.459192	379200.142635	44.263386
3501.424780	379190.624704	44.268391
3501.516544	379165.951320	44.273396
3501.381908	379167.648464	44.278401
3501.617469	379161.466135	44.283405
3501.357062	379130.422414	44.288410
3501.536435	379124.121841	44.293415
3501.494683	379118.820713	44.298420
3501.891561	379103.064477	44.303425
3501.460858	379096.935020	44.308429
3501.974434	379076.259231	44.313434
3501.604303	379064.965002	44.318439
3501.574670	379044.145157	44.323444
3501.871519	379034.854974	44.328449
3501.711549	379022.689963	44.333453
3501.421258	379004.323249	44.338458
3501.503450	378981.352703	44.343463
3501.649577	378969.165430	44.348468
3502.078691	378964.806833	44.353473
3501.667117	378939.602064	44.358477
3501.871535	378925.069278	44.363482
3501.624046	378912.663876	44.368487
3501.971629	378895.213661	44.373492
3501.488446	378873.702382	44.378497
3501.624624	378862.227695	44.383501
3502.008083	378848.022549	44.388506
3501.895151	378832.472466	44.393511
3501.701109	378808.224164	44.398516
3501.772082	378785.890095	44.403521
3501.538974	378776.987044	44.408525
3501.959205	378763.360240	44.413530
3502.108478	378746.626482	44.418535
3501.616975	378723.440234	44.423540
3501.691767	378708.292599	44.428545
3501.094421	378705.820625	44.433549
3501.523778	378686.148087	44.438554
3501.555202	378672.276987	44.443559
3501.638507	378654.055063	44.448564
3502.058777	378653.431027	44.453569
3501.812290	378631.171625	44.458573
3501.857156	378627.914011	44.463578
3501.642056	378598.691143	44.468583
3501.269170	378582.444875	44.473588
3501.491551	378574.715290	44.478593
3501.222713	378565.766935	44.483597
3501.621940	378540.080068	44.488602
3501.096606	378540.085707	44.493607
3501.294725	378532.918604	44.498612
3501.456093	378532.106287	44.503617
3501.446443	378508.819473	44.508621
3501.579276	378495.313444	44.513626
3501.833744	378489.686736	44.518631
3501.957864	378459.598246	44.523636
3501.167743	378452.000787	44.528641
3501.204552	378443.055621	44.533645
3501.564835	378421.133360	44.538650
3501.709354	378413.034900	44.543655
3501.482101	378405.502217	44.548660
3501.359082	378383.096413	44.553665
3501.650786	378363.165697	44.558669
3501.639351	378378.329223	44.563674
3501.792654	378354.407403	44.568679
3501.397779	378339.408833	44.573684
3501.802294	378322.330331	44.578689
3501.768327	378306.691463	44.583693
3501.933949	378294.754812	44.588698
3501.616183	378267.680862	44.593703
3501.791051	378247.717448	44.598708
3501.805993	378225.823370	44.603713
3501.454842	378211.452838	44.608717
3501.735189	378200.285587	44.613722
3501.539878	378183.808269	44.618727
3501.900390	378169.276178	44.623732
3501.747948	378154.265175	44.628737
3501.247392	378143.955920	44.633741
3501.776377	378129.956318	44.638746
3501.441022	378122.364187	44.643751
3501.894641	378094.281140	44.648756
3501.913979	378087.141738	44.653761
3501.913816	378063.192744	44.658765
3502.099645	378044.852863	44.663770
3501.961939	378024.785542	44.668775
3501.895365	378008.084909	44.673780
3502.224347	377997.316353	44.678785
3501.820937	377981.074467	44.683789
3501.813149	377958.421802	44.688794
3501.910646	377938.851150	44.693799
3501.835791	377923.015244	44.698804
3501.978815	377908.313680	44.703809
3501.934772	377893.641218	44.708813
3502.048241	377864.798162	44.713818
3501.626031	377861.740122	44.718823
3501.736464	377838.967371	44.723828
3501.840476	377814.214639	44.728833
3501.374373	377802.147500	44.733837
3501.541112	377780.127847	44.738842
3501.405812	377774.434656	44.743847
3501.571489	377763.259670	44.748852
3501.603104	377746.391211	44.753857
3501.751910	377728.844182	44.758861
3502.035449	377717.396866	44.763866
3501.586267	377711.600124	44.768871
3501.588572	377686.202776	44.773876
3501.855232	377669.272295	44.778881
3501.603823	377657.730418	44.783885
3501.688568	377640.117108	44.788890
3501.481408	377629.025481	44.793895
3501.836645	377613.706599	44.798900
3501.386680	377586.804912	44.803905
3501.429535	377581.464915	44.808909
3501.808034	377557.989885	44.813914
3501.504117	377543.332273	44.818919
3501.450795	377537.626275	44.823924
3501.733360	377523.766292	44.828929
3501.527114	377508.229956	44.833933
3501.998553	377486.365824	44.838938
3501.939346	377486.324322	44.843943
3501.579207	377456.792607	44.848948
3501.871433	377443.667601	44.853953
3501.464828	377432.073584	44.858957
3501.903443	377406.963639	44.863962
3501.103813	377410.542189	44.868967
3501.390999	377382.204924	44.873972
3501.634611	377372.998642	44.878977
3501.553979	377371.335042	44.883981
3501.696871	377353.407727	44.888986
3501.467998	377344.757510	44.893991
3501.199283	377329.459368	44.898996
3501.579239	377317.895288	44.904001
3501.483264	377307.675136	44.909005
3501.488932	377298.226484	44.914010
3501.382513	377292.325517	44.919015
3501.702725	377261.595625	44.924020
3501.652011	377251.546191	44.929025
3501.645715	377252.944111	44.934029
3501.810905	377223.558969	44.939034
3501.554679	377215.547905	44.944039
3501.661687	377187.416256	44.949044
3501.876651	377168.360110	44.954049
3501.747232	377171.834397	44.959053
3501.864659	377142.050237	44.964058
3501.477948	377136.015069	44.969063
3501.330493	377110.157926	44.974068
3501.273217	377098.407814	44.979073
3501.389680	377091.481612	44.984077
3501.426616	377087.513910	44.989082
3501.637173	377077.271368	44.994087
3501.720830	377054.857686	44.999092
3501.851703	377052.246836	45.004097
3501.261568	377031.868208	45.009101
3501.333752	377018.447065	45.014106
3501.421304	377016.147726	45.019111
3501.588840	376999.511624	45.024116
3501.836016	376974.456462	45.029121
3501.424916	376971.853749	45.034125
3501.728287	376943.411913	45.039130
3501.666333	376929.681428	45.044135
3501.855024	376914.337269	45.049140
3501.689725	376898.006875	45.054145
3501.225592	376892.466258	45.059149
3501.515082	376876.090478	45.064154
3501.656535	376860.169488	45.069159
3501.464100	376851.894410	45.074164
3501.746063	376843.596303	45.079169
3501.440487	376820.049294	45.084173
3501.576114	376800.954438	45.089178
3501.941978	376800.135647	45.094183
3501.800475	376771.966041	45.099188
3501.687655	376765.786576	45.104193
3501.463240	376740.372818	45.109197
3501.718596	376732.967746	45.114202
3501.747349	376723.566096	45.119207
3501.514157	376705.239708	45.124212
3501.741953	376695.400706	45.129217
3501.227848	376688.648719	45.134221
3501.394354	376660.989823	45.139226
3501.645442	376659.503140	45.144231
3501.589957	376646.787427	45.149236
3501.988714	376622.038525	45.154241
3501.745502	376602.824694	45.159245
3501.901569	376593.428585	45.164250
3501.510155	376585.463767	45.169255
3501.277019	376562.667204	45.174260
3501.619254	376542.828867	45.179265
3501.545539	376526.458597	45.184269
3501.659860	376532.536448	45.189274
3501.616783	376510.700794	45.194279
3501.559896	376484.219399	45.199284
3501.514491	376489.712557	45.204289
3501.293903	376473.212722	45.209293
3501.487517	376452.381516	45.214298
3501.302901	376458.988468	45.219303
3501.166531	376454.565076	45.224308
3501.473890	376425.995082	45.229313
3501.550613	376409.601332	45.234317
3501.294629	376403.723443	45.239322
3501.581249	376400.935905	45.244327
3501.261745	376385.187958	45.249332
3501.738212	376368.960563	45.254337
3501.174927	376365.517929	45.259341
3501.756181	376350.747319	45.264346
3501.402704	376327.080342	45.269351
3501.378403	376323.503032	45.274356
3501.283313	376305.408866	45.279361
3501.354524	376297.422770	45.284365
3501.373506	376277.913922	45.289370
3501.517562	376275.097759	45.294375
3501.318316	376261.261305	45.299380
3501.387740	376247.256045	45.304385
3500.851245	376240.812209	45.309389
3501.423646	376225.433346	45.314394
3501.366358	376226.788458	45.319399
3501.274083	376204.807822	45.324404
3501.899895	376195.973438	45.329409
3501.682110	376188.692642	45.334413
3501.396272	376164.913402	45.339418
3501.289256	376160.206009	45.344423
3501.531598	376153.539362	45.349428
3501.582056	376139.968772	45.354433
3501.498689	376127.206355	45.359437
3501.914794	376107.000623	45.364442
3501.674606	376092.205308	45.369447
3501.319702	376075.751529	45.374452
3501.849032	376072.392818	45.379457
3501.198542	376061.979097	45.384461
3501.541395	376042.648269	45.389466
3502.119817	376033.541823	45.394471
3501.622718	376005.858528	45.399476
3502.108274	376004.589311	45.404481
3501.821572	375985.153219	45.409485
3501.679393	375957.465443	45.414490
3501.423922	375943.586778	45.419495
3501.326347	375926.102314	45.424500
3501.629084	375925.090131	45.429505
3501.145897	375922.777918	45.434509
3501.442308	375895.174220	45.439514
3501.551426	375886.369343	45.444519
3501.006244	375889.451314	45.449524
3501.260748	375873.283562	45.454529
3501.155723	375863.724638	45.459533
3501.138597	375845.795824	45.464538
3500.987537	375850.695982	45.469543
3501.705663	375834.252870	45.474548
3501.625552	375826.315581	45.479553
3501.570410	375810.297571	45.484557
3501.639953	375799.543113	45.489562
3501.507833	375783.130684	45.494567
3501.414627	375756.908216	45.499572
3501.518343	375755.419019	45.504577
3501.246188	375752.235788	45.509581
3501.639161	375730.331649	45.514586
3501.371362	375718.435903	45.519591
3501.267289	375717.436220	45.524596
3501.220131	375697.657858	45.529601
3501.425890	375682.183349	45.534605
3501.844074	375672.644536	45.539610
3501.606672	375663.614121	45.544615
3501.224272	375647.215157	45.549620
3501.968253	375633.130008	45.554625
3501.587119	375615.943459	45.559629
3501.615406	375605.728723	45.564634
3501.477444	375598.384548	45.569639
3501.254410	375582.417928	45.574644
3501.604671	375562.222037	45.579649
3501.407809	375553.210676	45.584653
3501.733647	375547.851640	45.589658
3501.438339	375536.036292	45.594663
3501.500537	375518.171114	45.599668
3501.729873	375508.737828	45.604673
3501.693862	375497.186903	45.609677
3502.060224	375480.544326	45.614682
3501.623030	375457.753186	45.619687
3501.309933	375435.298303	45.624692
3501.384483	375436.328149	45.629697
3501.739406	375419.890508	45.634701
3502.032113	375400.567027	45.639706
3501.426807	375393.092326	45.644711
3501.236126	375368.230810	45.649716
3501.382634	375357.895988	45.654721
3501.637417	375356.865848	45.659725
3501.914079	375334.750896	45.664730
3501.682227	375330.316778	45.669735
3501.606260	375314.962098	45.674740
3501.191691	375292.268895	45.679745
3500.994787	375282.470070	45.684749
3501.261347	375274.453274	45.689754
3501.383021	375263.207903	45.694759
3501.233189	375259.548390	45.699764
3501.236943	375239.101388	45.704769
3500.896845	375244.488260	45.709773
3501.290660	375232.235352	45.714778
3501.394109	375233.895693	45.719783
3501.408311	375215.225004	45.724788
3501.966628	375199.238169	45.729793
3501.647599	375188.645533	45.734797
3501.433939	375161.780849	45.739802
3501.699631	375165.092311	45.744807
3501.329264	375156.895200	45.749812
3501.572833	375131.203909	45.754817
3501.508682	375103.553917	45.759821
3501.447157	375046.236814	45.764826
3500.858898	374944.501389	45.769831
3500.677085	374799.878317	45.774836
3500.846689	374613.416879	45.779841
3500.073114	374382.650656	45.784845
3499.671782	374101.531728	45.789850
3498.809117	373788.222793	45.794855
3497.692296	373416.425814	45.799860
3497.381120	373021.281534	45.804865
3496.399995	372579.547298	45.809869
3495.141933	372108.331675	45.814874
3494.277439	371591.194884	45.819879
3493.231397	371038.664639	45.824884
3492.075744	370442.903318	45.829889
3490.210439	369822.470563	45.834893
3488.817079	369167.654073	45.839898
3486.990090	368487.230342	45.844903
3485.357279	367773.376432	45.849908
3484.066298	367026.371836	45.854913
3481.688675	366257.132932	45.859917
3480.454137	365442.646933	45.864922
3478.139724	364619.463879	45.869927
3476.335142	363760.198243	45.874932
3474.189067	362859.414609	45.879937
3472.185286	361960.080741	45.884941
3470.616343	361015.926975	45.889946
3467.816003	360056.738318	45.894951
3465.194255	359061.302438	45.899956
3463.095021	358050.580317	45.904961
3460.501015	357025.974362	45.909965
3457.914814	355975.383378	45.914970
3455.245218	354913.815292	45.919975
3452.490129	353826.298447	45.924980
3450.166559	352711.885794	45.929985
3447.110741	351605.301364	45.934989
3444.676988	350454.248761	45.939994
3441.689130	349313.079920	45.944999
3438.897880	348145.808443	45.950004
3436.082224	346962.940759	45.955009
3433.317044	345772.498012	45.960013
3430.267857	344558.285246	45.965018
3427.142566	343338.625577	45.970023
3424.157100	342111.400271	45.975028
3421.393882	340858.186451	45.980033
3418.071566	339609.312704	45.985037
3414.639033	338331.727958	45.990042
3411.967169	337078.316692	45.995047
3408.594913	335783.289535	46.000052
3405.368615	334482.370395	46.005057
3402.367591	333186.864597	46.010061
3398.802063	331883.110925	46.015066
3395.410154	330564.330284	46.020071
3391.644238	329245.944658	46.025076
3388.982757	327905.467595	46.030081
3385.056721	326576.461943	46.035085
3381.964682	325239.803984	46.040090
3378.651140	323902.704439	46.045095
3375.167599	322560.652979	46.050100
3371.485467	321197.651977	46.055105
3368.071411	319849.398173	46.060109
3365.230141	318479.819875	46.065114
3361.265248	317112.053036	46.070119
3358.014761	315736.856181	46.075124
3354.243389	314355.337517	46.080129
3350.285999	312986.172801	46.085133
3347.452975	311596.410696	46.090138
3344.018833	310220.544596	46.095143
3340.378393	308833.983435	46.100148
3336.894203	307443.516128	46.105153
3332.511632	306056.941823	46.110157
3329.181920	304665.406755	46.115162
3325.620474	303273.997568	46.120167
3322.201981	301879.984267	46.125172
3318.097500	300482.503695	46.130177
3314.600437	299096.117326	46.135181
3311.018489	297698.459435	46.140186
3307.762374	296319.195714	46.145191
3303.681796	294919.944075	46.150196
3300.601599	293524.525452	46.155201
3296.430842	292129.167861	46.160205
3292.796974	290721.196213	46.165210
3289.201566	289331.413897	46.170215
3285.342410	287947.548592	46.175220
3281.678018	286546.261760	46.180225
3277.977397	285157.502183	46.185229
3274.270281	283756.648196	46.190234
3270.611302	282372.918289	46.195239
3267.060221	280980.845236	46.200244
3263.453151	279586.819740	46.205249
3259.533543	278199.691616	46.210253
3255.915923	276796.629623	46.215258
3252.626118	275415.643448	46.220263
3248.339850	274025.622909	46.225268
3244.809413	272628.969058	46.230273
3240.895293	271256.160105	46.235277
3236.963268	269868.844502	46.240282
3233.190399	268491.694179	46.245287
3229.443989	267107.084495	46.250292
3225.488218	265735.602008	46.255297
3222.112045	264377.125113	46.260301
3218.088052	262991.815351	46.265306
3214.467281	261629.165669	46.270311
3211.197358	260270.239439	46.275316
3207.255481	258905.825209	46.280321
3203.377535	257544.339986	46.285325
3199.290915	256183.356682	46.290330
3195.825863	254831.379857	46.295335
3191.953401	253470.794765	46.300340
3188.659787	252119.275138	46.305345
3184.452519	250771.374913	46.310349
3180.785434	249417.572963	46.315354
3177.361780	248076.761903	46.320359
3173.221209	246731.850425	46.325364
3169.834288	245394.503692	46.330369
3165.474251	244051.060139	46.335373
3162.231182	242710.108856	46.340378
3158.372819	241381.266918	46.345383
3154.253547	240048.689510	46.350388
3150.344280	238721.065057	46.355393
3146.721531	237404.622110	46.360397
3143.259913	236083.768536	46.365402
3139.752355	234777.485876	46.370407
3135.304138	233462.304384	46.375412
3131.923143	232140.841017	46.380417
3128.192086	230838.200052	46.385421
3124.755688	229528.634496	46.390426
3120.989759	228222.098525	46.395431
3116.538060	226921.857232	46.400436
3113.192963	225617.291802	46.405441
3109.303512	224328.601969	46.410445
3105.293592	223038.250513	46.415450
3101.505873	221747.483560	46.420455
3097.860308	220462.350242	46.425460
3094.430444	219171.480463	46.430465
3090.224551	217905.744577	46.435469
3087.202670	216625.845148	46.440474
3083.072238	215353.991732	46.445479
3079.588516	214077.508385	46.450484
3075.626559	212792.750439	46.455489
3071.625154	211539.228180	46.460493
3067.986285	210279.466177	46.465498
3063.545084	209031.550417	46.470503
3060.328326	207781.387582	46.475508
3056.814542	206527.737810	46.480513
3052.708810	205292.397007	46.485517
3048.769393	204044.762589	46.490522
3045.010023	202812.159679	46.495527
3041.381192	201584.842181	46.500532
3037.725979	200356.519023	46.505537
3033.496455	199139.194438	46.510541
3030.286008	197919.377997	46.515546
3026.525659	196703.502704	46.520551
3022.659295	195489.335197	46.525556
3019.018499	194273.029839	46.530561
3015.269754	193069.256362	46.535565
3011.550250	191863.707351	46.540570
3008.054479	190667.481326	46.545575
3003.692209	189470.154654	46.550580
3000.053992	188270.410763	46.555585
2996.124229	187090.358512	46.560589
2992.276971	185903.762331	46.565594
2988.642268	184718.369078	46.570599
2984.656343	183552.040387	46.575604
2980.939496	182385.174620	46.580609
2976.923383	181220.457844	46.585613
2973.606177	180065.119177	46.590618
2969.846174	178913.760075	46.595623
2965.752925	177762.111575	46.600628
2962.451787	176609.005940	46.605633
2958.092842	175470.873872	46.610637
2954.337626	174324.554540	46.615642
2950.085650	173198.099111	46.620647
2946.295951	172087.195119	46.625652
2942.523159	170965.255206	46.630657
2938.219989	169866.137177	46.635661
2934.658426	168760.288230	46.640666
2930.627297	167666.074885	46.645671
2926.473983	166578.211218	46.650676
2922.835439	165496.419924	46.655681
2918.898143	164428.961241	46.660685
2914.897393	163367.753779	46.665690
2911.158105	162306.268282	46.670695
2906.984192	161263.158149	46.675700
2903.381068	160216.552603	46.680705
2899.104826	159183.764325	46.685709
2895.252035	158157.876725	46.690714
2891.384287	157142.954280	46.695719
2887.281158	156139.158261	46.700724
2883.700982	155123.983969	46.705729
2879.159830	154133.513828	46.710733
2875.177869	153147.835350	46.715738
2871.219328	152181.552366	46.720743
2867.044726	151216.490630	46.725748
2863.499248	150271.823588	46.730753
2859.027156	149330.256835	46.735757
2855.040144	148390.361841	46.740762
2851.036189	147467.155968	46.745767
2846.524933	146559.353288	46.750772
2842.804151	145655.897193	46.755777
2838.320576	144777.439140	46.760781
2834.194830	143905.659054	46.765786
2829.528073	143057.708440	46.770791
2825.269804	142215.027338	46.775796
2820.980440	141386.946689	46.780801
2816.714266	140590.888260	46.785805
2812.412320	139784.899246	46.790810
2807.824953	139019.083347	46.795815
2803.460283	138227.749201	46.800820
2799.416387	137424.966622	46.805825
2795.022856	136700.442818	46.810829
2790.471508	135984.211609	46.815834
2786.227477	135293.845413	46.820839
2782.034413	134599.907109	46.825844
2778.322927	133920.317968	46.830849
2774.217947	133279.040391	46.835853
2770.383473	132619.882476	46.840858
2766.098645	131979.885814	46.845863
2761.899267	131354.208727	46.850868
2757.931594	130727.423422	46.855873
2754.408440	130122.088089	46.860877
2750.155191	129524.761439	46.865882
2746.541454	128938.460912	46.870887
2742.761442	128348.709227	46.875892
2739.371622	127778.671345	46.880897
2735.732194	127210.295490	46.885901
2731.763826	126632.044939	46.890906
2728.648503	126078.815319	46.895911
2724.995995	125513.568429	46.900916
2721.202314	124945.947546	46.905921
2717.614142	124400.827147	46.910925
2713.932837	123841.496821	46.915930
2710.449303	123301.882140	46.920935
2706.625414	122756.184968	46.925940
2703.231517	122209.512736	46.930945
2699.311401	121673.333028	46.935949
2696.150620	121133.087376	46.940954
2692.478975	120599.567153	46.945959
2688.849791	120063.758600	46.950964
2685.862237	119520.405531	46.955969
2682.417416	118989.504732	46.960973
2678.604162	118462.750689	46.965978
2675.358045	117925.437391	46.970983
2671.640873	117399.560637	46.975988
2668.066924	116859.147243	46.980993
2664.612980	116340.200078	46.985997
2660.586312	115802.542793	46.991002
2657.102822	115270.899516	46.996007
2653.550479	114752.943596	47.001012
2650.440128	114225.389864	47.006017
2646.636846	113695.612048	47.011021
2643.338372	113173.837283	47.016026
2639.267019	112657.873749	47.021031
2636.074308	112147.070079	47.026036
2632.556628	111614.404960	47.031041
2629.200817	111118.389875	47.036045
2625.564053	110597.582582	47.041050
2622.054709	110070.342744	47.046055
2618.027637	109564.817001	47.051060
2614.664668	109050.651886	47.056065
2610.860134	108558.671165	47.061069
2607.137375	108049.115437	47.066074
2603.351147	107539.920350	47.071079
2599.241445	107042.478689	47.076084
2595.767366	106559.386591	47.081089
2591.552695	106079.963292	47.086093
2588.219780	105594.727275	47.091098
2584.359036	105117.283731	47.096103
2580.382609	104658.296855	47.101108
2577.134262	104186.135554	47.106113
2573.156161	103717.780765	47.111117
2569.294298	103266.180450	47.116122
2565.691068	102811.647940	47.121127
2561.774143	102368.940683	47.126132
2558.135968	101919.497511	47.131137
2554.265364	101489.454665	47.136141
2550.304388	101052.440894	47.141146
2546.762518	100628.624404	47.146151
2543.268545	100212.838679	47.151156
2540.373279	99779.845057	47.156161
2536.742117	99359.706796	47.161165
2533.029838	98934.045338	47.166170
2529.149243	98511.542215	47.171175
2525.398395	98095.201121	47.176180
2521.884070	97675.346421	47.181185
2518.639976	97260.017676	47.186189
2514.759449	96853.142988	47.191194
2511.723861	96434.882389	47.196199
2507.818197	96027.806252	47.201204
2504.715300	95615.120583	47.206209
2501.371400	95210.865117	47.211213
2497.796797	94790.994836	47.216218
2494.830540	94378.622006	47.221223
2490.933347	93966.132698	47.226228
2488.184021	93543.012210	47.231233
2484.002043	93117.858645	47.236237
2480.319184	92702.188909	47.241242
2476.950419	92281.723639	47.246247
2473.821103	91863.031251	47.251252
2470.588614	91444.780013	47.256257
2467.119635	91016.914653	47.261261
2463.770356	90600.014747	47.266266
2460.570788	90175.245119	47.271271
2456.391939	89744.598728	47.276276
2453.100663	89308.776355	47.281281
2449.542284	88888.184761	47.286285
2446.192845	88457.478760	47.291290
2442.822170	88038.140547	47.296295
2439.008180	87608.789723	47.301300
2435.752078	87177.808402	47.306305
2432.028851	86751.937052	47.311309
2428.273763	86319.686671	47.316314
2425.411404	85889.018823	47.321319
2422.169078	85466.508827	47.326324
2418.574950	85028.815405	47.331329
2415.148727	84592.779353	47.336333
2411.375050	84161.084982	47.341338
2408.246336	83723.415236	47.346343
2404.851888	83289.236024	47.351348
2401.300413	82849.701945	47.356353
2397.618499	82419.289935	47.361357
2394.437107	81973.843313	47.366362
2390.544659	81534.700287	47.371367
2387.170537	81093.019296	47.376372
2383.814880	80645.309100	47.381377
2380.062155	80205.898417	47.386381
2376.718772	79762.938117	47.391386
2373.378578	79321.521212	47.396391
2369.809657	78881.213813	47.401396
2366.152889	78442.908411	47.406401
2362.456723	78012.452302	47.411405
2359.017782	77560.537594	47.416410
2356.057881	77121.611440	47.421415
2352.060578	76683.526887	47.426420
2348.680514	76235.600020	47.431425
2345.633236	75785.812746	47.436429
2341.737789	75345.130595	47.441434
2338.345154	74901.913796	47.446439
2335.205481	74456.087086	47.451444
2331.460085	74008.279495	47.456449
2328.110260	73551.757570	47.461453
2324.588892	73104.298549	47.466458
2321.172157	72641.859928	47.471463
2317.345958	72198.031766	47.476468
2314.367236	71749.101761	47.481473
2310.890803	71296.358807	47.486477
2307.650677	70833.518125	47.491482
2303.757147	70374.964577	47.496487
2300.085752	69921.234632	47.501492
2297.044159	69460.799774	47.506497
2293.135736	69001.269765	47.511501
2290.165956	68537.831158	47.516506
2286.364304	68085.163002	47.521511
2282.860813	67627.346490	47.526516
2279.406545	67165.671142	47.531521
2275.625885	66700.049655	47.536525
2272.614316	66242.327406	47.541530
2269.028935	65778.964766	47.546535
2265.340908	65319.130217	47.551540
2261.859248	64849.199163	47.556545
2258.412621	64393.380660	47.561549
2254.852962	63926.773052	47.566554
2251.063438	63456.040141	47.571559
2247.721346	63000.795596	47.576564
2244.529811	62532.214728	47.581569
2240.495971	62072.703099	47.586573
2237.180989	61611.704659	47.591578
2233.928641	61144.682634	47.596583
2229.931754	60678.864166	47.601588
2226.948808	60202.635493	47.606593
2223.522584	59744.119889	47.611597
2219.854979	59284.216363	47.616602
2216.520041	58807.555720	47.621607
2212.730702	58351.864141	47.626612
2209.490001	57876.266846	47.631617
2206.018502	57419.287049	47.636621
2202.540608	56948.370601	47.641626
2199.531882	56471.749787	47.646631
2195.642132	56004.913274	47.651636
2192.673951	55526.687105	47.656641
2188.204134	55050.049288	47.661645
2185.216837	54571.750166	47.666650
2181.477643	54100.188445	47.671655
2178.061398	53628.585901	47.676660
2174.783471	53156.768286	47.681665
2171.082186	52686.891152	47.686669
2167.585420	52209.556776	47.691674
2163.797267	51732.258494	47.696679
2160.443000	51260.332508	47.701684
2157.150154	50783.902793	47.706689
2153.180086	50314.483373	47.711693
2149.656212	49838.781505	47.716698
2146.605589	49359.787263	47.721703
2143.509606	48889.347530	47.726708
2139.829840	48412.748090	47.731713
2135.813220	47928.060850	47.736717
2132.330581	47454.977247	47.741722
2129.361961	46974.916760	47.746727
2125.421820	46497.916027	47.751732
2122.080793	46022.550835	47.756737
2118.611395	45546.448299	47.761741
2115.471115	45071.167128	47.766746
2111.733059	44583.680000	47.771751
2108.190540	44105.285804	47.776756
2105.072957	43610.075590	47.781761
2101.388519	43127.894356	47.786765
2097.609143	42645.262827	47.791770
2095.176454	42160.675832	47.796775
2090.844471	41682.697832	47.801780
2087.531633	41184.674685	47.806785
2083.864833	40702.112693	47.811789
2080.287957	40214.722358	47.816794
2077.098513	39726.540831	47.821799
2073.112563	39242.089063	47.826804
2069.887388	38753.770152	47.831809
2066.330724	38274.541736	47.836813
2062.631550	37790.914742	47.841818
2059.459172	37302.544431	47.846823
2055.572793	36803.215162	47.851828
2052.359026	36322.994366	47.856833
2048.739967	35833.769909	47.861837
2045.426357	35350.499459	47.866842
2041.876636	34846.212997	47.871847
2038.273279	34370.572167	47.876852
2034.702415	33884.180587	47.881857
2031.436414	33394.482220	47.886861
2027.867137	32902.586080	47.891866
2024.165076	32413.726400	47.896871
2020.888443	31924.032397	47.901876
2017.841272	31432.051621	47.906881
2014.047585	30942.080944	47.911885
2009.852664	30443.850562	47.916890
2006.449444	29968.564065	47.921895
2003.421892	29480.232565	47.926900
1999.858767	28983.612168	47.931905
1996.080856	28497.442324	47.936909
1992.576999	28009.340378	47.941914
1988.997114	27516.807354	47.946919
1985.726662	27024.668967	47.951924
1982.136975	26533.403232	47.956929
1978.621171	26047.232128	47.961933
1975.369515	25554.214158	47.966938
1971.753109	25070.502577	47.971943
1967.855544	24586.428248	47.976948
1964.629380	24097.750263	47.981953
1960.902454	23608.389247	47.986957
1957.309351	23117.574994	47.991962
1953.833347	22634.515002	47.996967
1949.893896	22143.696352	48.001972
1946.720302	21665.142331	48.006977
1943.215877	21190.015033	48.011981
1939.514720	20704.053667	48.016986
1936.225439	20213.283209	48.021991
1932.684890	19732.084244	48.026996
1929.354371	19240.128445	48.032001
1926.092990	18757.940934	48.037005
1922.124758	18277.864125	48.042010
1918.775387	17791.128758	48.047015
1914.984807	17315.896362	48.052020
1911.726351	16827.505425	48.057025
1907.864615	16353.023451	48.062029
1904.018206	15870.967254	48.067034
1900.886192	15388.697993	48.072039
1897.366962	14919.419430	48.077044
1893.688375	14436.005422	48.082049
1890.110647	13958.160294	48.087053
1886.492358	13488.495462	48.092058
1882.748999	13020.470017	48.097063
1879.120592	12547.980733	48.102068
1875.497710	12085.338475	48.107073
1871.931405	11624.702658	48.112077
1868.252739	11151.113408	48.117082
1864.660000	10684.391963	48.122087
1860.627764	10227.734425	48.127092
1857.754179	9772.721495	48.132097
1853.869892	9318.361265	48.137101
1849.664890	8864.853363	48.142106
1846.373218	8418.427791	48.147111
1842.527237	7987.367599	48.152116
1838.662287	7537.339878	48.157121
1834.674769	7126.391134	48.162125
1830.835588	6696.914044	48.167130
1826.733060	6284.606324	48.172135
1822.317559	5894.949530	48.177140
1818.234642	5498.692118	48.182145
1813.710517	5131.290734	48.187149
1809.867753	4777.268439	48.192154
1805.736064	4413.817265	48.197159
1800.998374	4075.612038	48.202164
1796.910059	3746.390574	48.207169
1792.919916	3438.408049	48.212173
1788.576858	3127.587260	48.217178
1783.904935	2843.240820	48.222183
1779.413802	2584.351579	48.227188
1775.669323	2325.995336	48.232193
1771.546730	2082.395534	48.237197
1767.416933	1842.138198	48.242202
1763.711845	1622.579982	48.247207
1759.719122	1410.150121	48.252212
1756.191514	1192.872907	48.257217
1752.289823	1000.492888	48.262221
1748.488256	805.501858	48.267226
1744.779743	612.953587	48.272231
1741.297402	446.118920	48.277236
1737.155648	268.644400	48.282241
1732.365405	118.825311	48.287245
1724.899410	63.164107	48.292250
1715.810124	87.183492	48.297255
1709.825298	97.302450	48.302260
1706.483105	93.361887	48.307265
1703.869185	94.556561	48.312269
1701.450594	88.801814	48.317274
1699.005585	88.850247	48.322279
1696.068003	99.032760	48.327284
1693.584873	90.342650	48.332289
1690.402428	86.253843	48.337293
1686.812302	89.353147	48.342298
1684.251359	87.473948	48.347303
1679.976004	87.528855	48.352308
1676.840107	81.477638	48.357313
1673.278959	91.023220	48.362317
1669.449822	94.988616	48.367322
1666.846089	90.569298	48.372327
1663.443137	104.142969	48.377332
1659.878134	98.101588	48.382337
1656.880486	95.195719	48.387341
1653.112650	89.037219	48.392346
1650.353729	90.899859	48.397351
1646.586263	95.899680	48.402356
1643.572705	95.830966	48.407361
1639.572375	90.850749	48.412365
1636.457870	103.711983	48.417370
1633.354278	91.815544	48.422375
1629.328282	91.059702	48.427380
1625.860691	84.424213	48.432385
1622.703916	88.522240	48.437389
1619.290437	87.031998	48.442394
1615.802435	80.962827	48.447399
1612.494013	90.260271	48.452404
1608.920877	91.885815	48.457409
1605.455653	88.976799	48.462413
1601.619975	83.062981	48.467418
1598.273042	80.451926	48.472423
1594.768306	74.882066	48.477428
1591.593199	79.894091	48.482433
1588.136578	86.702623	48.487437
1584.491937	90.990479	48.492442
1581.201380	80.243107	48.497447
1577.484282	80.729983	48.502452
1574.528925	85.018121	48.507457
1571.330122	79.327881	48.512461
1567.391502	84.126556	48.517466
1563.953651	86.588409	48.522471
1560.144008	81.100810	48.527476
1556.998043	79.841016	48.532481
1553.538009	82.549927	48.537485
1549.861433	83.723348	48.542490
1546.196050	75.163495	48.547495
1542.720391	85.309527	48.552500
1539.088922	84.723240	48.557505
1536.200614	87.678519	48.562509
1532.815030	91.116150	48.567514
1529.326043	80.456619	48.572519
1525.722714	78.021519	48.577524
1522.136816	83.584695	48.582529
1518.756607	77.166574	48.587533
1515.030816	86.509996	48.592538
1512.009786	80.206810	48.597543
1508.191873	80.237993	48.602548
1505.010583	85.617974	48.607553
1501.573864	80.135614	48.612557
1497.921233	80.169546	48.617562
1494.347753	89.059000	48.622567
1490.593781	79.260119	48.627572
1487.095284	72.227677	48.632577
1483.752103	75.775766	48.637581
1479.867814	79.281529	48.642586
1476.986501	73.367884	48.647591
1473.504808	81.097792	48.652596
1470.050478	79.098243	48.657601
1466.684136	76.012507	48.662605
1462.595031	83.299129	48.667610
1458.980813	70.466669	48.672615
1455.828880	82.957230	48.677620
1452.220078	67.301914	48.682625
1449.275869	67.140168	48.687629
1445.241026	74.902387	48.692634
1441.829216	72.095810	48.697639
1438.123655	74.842944	48.702644
1434.998504	62.886644	48.707649
1431.818764	70.461985	48.712653
1428.005728	75.813749	48.717658
1424.635759	75.759401	48.722663
1421.024381	81.892849	48.727668
1417.519118	76.107965	48.732673
1413.814377	78.959376	48.737677
1410.403078	79.632784	48.742682
1407.015058	83.906017	48.747687
1403.564763	89.460749	48.752692
1400.181949	83.979503	48.757697
1396.789975	81.834217	48.762701
1393.401574	73.516012	48.767706
1389.940534	80.746008	48.772711
1385.877914	77.819276	48.777716
1382.365208	80.795820	48.782721
1379.153841	83.383784	48.787725
1375.115861	89.406470	48.792730
1371.872138	91.369895	48.797735
1368.509039	84.177190	48.802740
1364.731415	78.868132	48.807745
1361.839742	79.245534	48.812749
1358.029521	90.639521	48.817754
1354.795878	79.889661	48.822759
1351.192127	88.768012	48.827764
1347.560009	81.190086	48.832769
1344.448678	87.935391	48.837773
1340.524516	88.938565	48.842778
1337.078616	78.465351	48.847783
1333.280290	82.954310	48.852788
1330.050411	82.713654	48.857793
1326.753499	85.545886	48.862797
1322.824068	93.459387	48.867802
1319.400885	79.550033	48.872807
1316.300532	87.625545	48.877812
1312.714832	83.754573	48.882817
1309.439452	79.012742	48.887821
1305.724301	82.470048	48.892826
1302.166315	80.894769	48.897831
1298.295012	92.076806	48.902836
1295.251046	86.757963	48.907841
1291.527853	84.398495	48.912845
1287.878581	92.565777	48.917850
1284.760873	92.766401	48.922855
1280.582399	91.638873	48.927860
1277.653891	84.008385	48.932865
1274.442664	84.881614	48.937869
1270.219715	85.181508	48.942874
1267.105271	75.947503	48.947879
1263.498132	88.673430	48.952884
1260.030715	84.192445	48.957889
1256.646506	79.385304	48.962893
1253.366512	90.424684	48.967898
1250.162509	86.241214	48.972903
1246.481881	84.033310	48.977908
1242.783954	80.780919	48.982913
1238.813331	89.409500	48.987917
1235.614681	89.205121	48.992922
1232.417859	90.617102	48.997927
1228.726149	90.530598	49.002932
1225.042568	81.217510	49.007937
1221.392433	86.607208	49.012941
1217.759354	92.930706	49.017946
1214.708456	78.469892	49.022951
1211.163016	81.720459	49.027956
1207.901493	85.306477	49.032961
1204.265733	83.683205	49.037965
1200.677678	81.163512	49.042970
1197.289674	72.573202	49.047975
1193.661491	90.225102	49.052980
1189.855176	81.155747	49.057985
1186.559792	70.839469	49.062989
1183.135036	86.669055	49.067994
1179.897014	80.785663	49.072999
1175.878719	72.600343	49.078004
1172.578241	76.375918	49.083009
1168.779281	81.833076	49.088013
1165.835134	80.282486	49.093018
1162.671306	72.638031	49.098023
1158.976414	78.018880	49.103028
1155.043075	71.813463	49.108033
1151.606513	82.592478	49.113037
1147.967025	78.391389	49.118042
1144.792447	77.727701	49.123047
1140.921359	81.136528	49.128052
1137.366728	79.079867	49.133057
1133.811470	80.126879	49.138061
1130.672357	83.943779	49.143066
1127.372466	76.823534	49.148071
1123.652392	67.516154	49.153076
1120.301763	64.310962	49.158081
1116.782401	75.156644	49.163085
1112.765561	78.641943	49.168090
1109.493752	77.117053	49.173095
1105.822120	71.956052	49.178100
1102.483770	69.770821	49.183105
1099.065878	73.431803	49.188109
1095.332453	80.242312	49.193114
1092.343721	71.801839	49.198119
1088.673751	76.865608	49.203124
1085.176877	78.298998	49.208129
1081.944419	71.759875	49.213133
1077.940015	75.455208	49.218138
1074.672957	76.327655	49.223143
1070.742445	75.949317	49.228148
1067.367582	76.031806	49.233153
1064.326351	79.102663	49.238157
1060.954902	81.614330	49.243162
1057.953333	74.893741	49.248167
1053.224164	77.325690	49.253172
1049.673758	73.363846	49.258177
1046.195948	69.463468	49.263181
1042.892004	77.532710	49.268186
1039.509887	74.971492	49.273191
1035.650185	79.470027	49.278196
1032.914232	73.650873	49.283201
1029.224468	77.844552	49.288205
1025.716705	76.859426	49.293210
1022.481099	69.922179	49.298215
1018.736414	78.847784	49.303220
1014.923415	80.729013	49.308225
1011.246018	70.753801	49.313229
1007.757097	75.770412	49.318234
1004.500227	75.344170	49.323239
1000.909739	71.470829	49.328244
997.855079	76.290132	49.333249
994.256880	78.606152	49.338253
990.365270	80.208562	49.343258
987.080395	76.948859	49.348263
983.765714	73.997510	49.353268
980.035105	77.741980	49.358273
976.781654	76.546435	49.363277
972.836831	77.204862	49.368282
969.689803	67.444489	49.373287
966.162611	75.118222	49.378292
962.141161	73.621458	49.383297
958.921098	70.800914	49.388301
955.115467	84.329674	49.393306
952.430880	78.274749	49.398311
948.444272	76.516305	49.403316
944.827437	77.421066	49.408321
941.816876	73.229675	49.413325
937.822836	81.162741	49.418330
934.867189	77.108331	49.423335
930.710649	80.207280	49.428340
927.533908	76.541621	49.433345
923.838551	77.730683	49.438349
920.255237	80.484146	49.443354
917.062800	76.697547	49.448359
913.355417	85.111165	49.453364
909.892510	75.080437	49.458369
906.801359	77.339683	49.463373
903.426678	81.294505	49.468378
899.706265	63.774315	49.473383
896.084020	72.101910	49.478388
891.788634	73.947514	49.483393
888.882930	68.619867	49.488397
885.114600	73.037754	49.493402
882.332984	70.588720	49.498407
878.778489	92.924039	49.503412
875.162598	77.257307	49.508417
871.370908	76.851059	49.513421
867.599815	81.864150	49.518426
863.881337	69.990830	49.523431
860.791180	76.422815	49.528436
857.347179	79.028050	49.533441
854.299441	76.544516	49.538445
850.878066	80.585703	49.543450
847.331340	73.446985	49.548455
843.366199	79.850665	49.553460
839.661236	74.979627	49.558465
836.377728	67.929650	49.563469
832.921262	82.327850	49.568474
829.502275	72.866094	49.573479
825.728045	77.136212	49.578484
822.556867	69.138629	49.583489
818.907682	76.081570	49.588493
815.167571	79.188473	49.593498
811.834759	74.990318	49.598503
808.615909	72.239206	49.603508
804.866353	73.762578	49.608513
801.780839	70.161828	49.613517
797.852056	71.042401	49.618522
794.462116	69.425211	49.623527
790.788864	68.978392	49.628532
787.449793	71.450242	49.633537
783.785515	75.462809	49.638541
779.909837	80.944594	49.643546
776.995258	72.559069	49.648551
773.649395	64.136285	49.653556
769.915990	71.449834	49.658561
766.575510	66.692911	49.663565
762.681355	74.537672	49.668570
759.326114	71.165573	49.673575
755.477897	78.367286	49.678580
752.131378	61.235015	49.683585
749.430352	69.248373	49.688589
745.058329	63.010088	49.693594
741.801228	69.917306	49.698599
738.775089	64.766614	49.703604
734.921171	68.906779	49.708609
731.700109	68.778708	49.713613
727.624044	71.194453	49.718618
724.208310	67.676757	49.723623
720.223629	72.723108	49.728628
717.079849	68.770782	49.733633
713.927974	64.557132	49.738637
710.375915	70.624441	49.743642
707.092070	58.860671	49.748647
702.956214	63.652152	49.753652
699.436893	80.727110	49.758657
696.346285	69.967776	49.763661
692.876182	68.799665	49.768666
689.441954	71.877945	49.773671
685.449251	76.099830	49.778676
682.091416	70.219354	49.783681
678.648162	68.512405	49.788685
674.894743	74.519317	49.793690
672.325767	73.925919	49.798695
668.318730	68.823533	49.803700
664.854316	71.232653	49.808705
661.722326	77.487668	49.813709
657.642904	74.247300	49.818714
653.926012	67.309112	49.823719
650.837871	72.383578	49.828724
647.535557	76.551776	49.833729
644.038001	70.120433	49.838733
640.036272	73.603429	49.843738
637.059283	65.455433	49.848743
633.394760	71.448508	49.853748
629.568690	58.813737	49.858753
625.851600	67.943864	49.863757
622.620515	69.937024	49.868762
619.220368	68.533412	49.873767
615.586479	73.651712	49.878772
612.103576	68.056467	49.883777
608.923006	60.136318	49.888781
604.804309	65.877403	49.893786
601.530976	66.690766	49.898791
598.667625	67.035357	49.903796
594.658495	76.422918	49.908801
591.217091	62.042035	49.913805
588.017752	70.854290	49.918810
584.345227	69.758833	49.923815
580.832539	68.129144	49.928820
576.873960	78.318737	49.933825
574.062809	72.289901	49.938829
570.153552	70.244235	49.943834
567.016718	67.932794	49.948839
563.153813	68.404521	49.953844
559.055786	71.023018	49.958849
556.153197	70.965608	49.963853
552.547305	70.533644	49.968858
549.803231	70.872326	49.973863
546.330476	70.726513	49.978868
541.945404	63.734185	49.983873
538.302411	67.582114	49.988877
535.007755	66.010235	49.993882
531.914287	66.143891	49.998887
528.025055	60.305043	50.003892
523.976437	66.721743	50.008897
520.787581	61.052267	50.013901
517.350802	60.419980	50.018906
514.132597	70.070382	50.023911
510.951018	66.702923	50.028916
507.383205	62.854606	50.033921
504.006426	68.954752	50.038925
499.913867	69.981082	50.043930
496.686154	69.373196	50.048935
493.417680	67.082259	50.053940
489.737910	70.062746	50.058945
486.085195	64.376906	50.063949
482.404784	63.118182	50.068954
478.798602	70.275907	50.073959
475.331317	67.288280	50.078964
471.949486	72.145896	50.083969
468.893803	61.393832	50.088973
464.995954	66.493127	50.093978
461.862310	65.247359	50.098983
458.201755	62.330952	50.103988
454.754667	69.701186	50.108993
451.102527	65.461057	50.113997
447.536853	70.037255	50.119002
444.128551	63.326309	50.124007
440.584917	63.789477	50.129012
436.947663	65.298575	50.134017
433.798849	61.163585	50.139021
429.872449	64.448221	50.144026
426.288478	65.610513	50.149031
423.310418	67.820560	50.154036
419.715354	62.005538	50.159041
416.439956	59.611290	50.164045
412.158595	62.011582	50.169050
409.042359	66.280540	50.174055
405.646149	65.274967	50.179060
401.557745	68.980287	50.184065
398.354209	57.178776	50.189069
395.008748	68.579516	50.194074
391.656930	63.406818	50.199079
387.619664	65.857695	50.204084
384.409171	64.566956	50.209089
380.950386	60.597286	50.214093
377.635632	68.263290	50.219098
374.228980	64.345614	50.224103
370.838171	65.984027	50.229108
367.225276	65.581653	50.234113
363.301399	60.491693	50.239117
359.800657	66.301110	50.244122
356.318825	62.955110	50.249127
352.522480	64.583896	50.254132
349.676969	71.942738	50.259137
346.544804	59.861215	50.264141
342.091180	63.996712	50.269146
338.903375	58.096158	50.274151
335.378295	65.187484	50.279156
331.575551	69.275434	50.284161
328.672447	68.000120	50.289165
325.008709	67.871415	50.294170
321.076411	63.311105	50.299175
317.861591	59.357248	50.304180
313.983605	68.740226	50.309185
311.032777	64.973053	50.314189
307.525598	66.446098	50.319194
303.957933	59.453116	50.324199
300.745116	61.070154	50.329204
297.001158	64.990772	50.334209
293.660931	59.537886	50.339213
289.574908	67.906083	50.344218
286.299226	63.173954	50.349223
283.050743	59.706219	50.354228
279.013581	64.960096	50.359233
275.831707	60.210201	50.364237
272.212972	70.732867	50.369242
269.016278	56.383575	50.374247
265.704438	61.179691	50.379252
261.923946	58.883085	50.384257
258.522861	56.043372	50.389261
254.739548	69.318733	50.394266
251.614207	64.246837	50.399271
248.303578	68.716912	50.404276
244.440299	69.479800	50.409281
240.778751	67.512681	50.414285
237.077148	59.591467	50.419290
233.919591	60.981617	50.424295
230.487741	62.759310	50.429300
226.694539	67.532300	50.434305
223.607681	56.946491	50.439309
219.832205	62.131161	50.444314
216.302392	62.000603	50.449319
212.811065	64.360181	50.454324
209.148888	61.849016	50.459329
205.971797	57.550792	50.464333
202.239574	59.675801	50.469338
198.674298	59.291348	50.474343
195.445553	56.383686	50.479348
191.395974	55.179320	50.484353
188.343212	54.496784	50.489357
184.723708	58.464475	50.494362
181.438352	61.412064	50.499367
178.195667	65.950658	50.504372
174.181054	64.993943	50.509377
170.577418	60.695697	50.514381
167.194367	62.731547	50.519386
163.986467	60.127519	50.524391
159.862932	52.322634	50.529396
156.616334	59.196615	50.534401
153.133490	64.968463	50.539405
149.670170	57.753630	50.544410
146.615224	57.400459	50.549415
142.657982	62.831728	50.554420
139.631218	63.135374	50.559425
136.016524	61.240070	50.564429
132.321568	71.480391	50.569434
129.008917	61.793432	50.574439
125.371413	62.410459	50.579444
121.498205	66.306930	50.584449
118.457480	63.695863	50.589453
114.486260	67.591776	50.594458
111.053522	66.822881	50.599463
107.656779	62.119122	50.604468
103.966626	53.338808	50.609473
101.233902	57.785355	50.614477
97.453861	58.032285	50.619482
93.687164	56.809204	50.624487
90.346742	58.999773	50.629492
86.553676	64.082795	50.634497
83.061428	59.270529	50.639501
79.504384	54.547445	50.644506
76.287762	49.173431	50.649511
72.794157	56.019437	50.654516
69.255290	66.959934	50.659521
65.781998	49.502765	50.664525
61.676757	57.956227	50.669530
58.134309	53.328947	50.674535
55.022064	52.655690	50.679540
51.498373	61.319157	50.684545
48.512734	55.510563	50.689549
45.148315	63.563957	50.694554
41.275294	55.536604	50.699559
37.755591	50.516659	50.704564
34.098191	60.751133	50.709569
30.904710	53.032421	50.714573
26.891653	58.326865	50.719578
23.463624	61.556106	50.724583
20.251243	66.074179	50.729588
16.533813	66.162681	50.734593
13.049614	55.088309	50.739597
8.963485	60.770608	50.744602
6.109173	65.432242	50.749607
2.957629	64.300053	50.754612