Fri Aug 26 11:40:51 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.481147	96.379459	0.000000
1.283862	100.504049	0.005005
0.687106	94.003998	0.010010
1.090939	90.964220	0.015014
0.772970	91.659212	0.020019
1.082007	76.890707	0.025024
0.986610	88.838966	0.030029
0.601727	79.224532	0.035034
0.232209	64.798960	0.040038
-0.143089	75.639220	0.045043
0.040235	51.649278	0.050048
-0.561494	52.964234	0.055053
-0.160534	51.380189	0.060058
-0.595886	42.263999	0.065062
-1.193316	40.338709	0.070067
-1.458172	23.052756	0.075072
-2.075208	26.505553	0.080077
-2.154608	17.599701	0.085082
-2.632797	20.923315	0.090086
-3.016354	10.600056	0.095091
-3.234257	5.211600	0.100096
-3.457425	2.642769	0.105101
-3.371768	4.575171	0.110106
-3.280922	2.555377	0.115110
-3.664866	-0.779331	0.120115
-4.222506	-3.239139	0.125120
-4.482913	-0.287947	0.130125
-4.697279	-5.680114	0.135130
-5.325857	-1.608615	0.140134
-5.503348	2.775451	0.145139
-5.581786	-6.124211	0.150144
-5.676633	-0.838721	0.155149
-6.208227	-5.264041	0.160154
-6.528360	-10.924466	0.165158
-6.874954	-3.711088	0.170163
-6.877229	-8.810421	0.175168
-6.838179	-11.110040	0.180173
-7.206300	-7.313205	0.185178
-7.749052	-3.764416	0.190182
-8.127522	-3.252990	0.195187
-8.353841	-11.927151	0.200192
-8.656612	-3.262159	0.205197
-8.711945	2.665726	0.210202
-8.526550	-13.703237	0.215206
-9.657536	1.512894	0.220211
-9.681972	-15.804125	0.225216
-10.036044	-4.116200	0.230221
-9.909209	1.761176	0.235226
-10.001254	-1.764507	0.240230
-10.045127	-7.189546	0.245235
-10.548891	-7.930395	0.250240
-10.877370	-5.664605	0.255245
-10.789613	-10.293918	0.260250
-11.104104	-5.379178	0.265254
-11.748868	3.051173	0.270259
-12.032765	-3.747479	0.275264
-12.248005	0.120464	0.280269
-12.467042	-1.908027	0.285274
-12.160935	-2.721189	0.290278
-13.249313	-1.580395	0.295283
-13.176469	-8.722480	0.300288
-13.881388	6.101462	0.305293
-13.807383	-2.720699	0.310298
-13.766987	-8.573295	0.315302
-14.173522	-2.660331	0.320307
-13.832072	-4.994379	0.325312
-14.807325	-1.368759	0.330317
-15.234758	-8.907498	0.335322
-15.373429	-2.909694	0.340326
-15.335098	8.859507	0.345331
-15.361203	-2.974673	0.350336
-16.179109	10.411590	0.355341
-16.903481	2.703952	0.360346
-16.875524	4.382755	0.365350
-17.248068	3.143765	0.370355
-16.794355	4.129878	0.375360
-17.004575	5.035873	0.380365
-17.146082	-1.920986	0.385370
-17.064678	-0.275814	0.390374
-18.160521	3.216727	0.395379
-18.368414	-4.596632	0.400384
-18.573542	3.689341	0.405389
-18.654668	-1.748880	0.410394
-18.408856	-2.558982	0.415398
-19.541379	-4.926117	0.420403
-19.755992	-5.291222	0.425408
-19.994055	2.053950	0.430413
-20.052410	-0.958141	0.435418
-19.659454	-0.320060	0.440422
-20.540926	-0.888209	0.445427
-21.145483	-7.279442	0.450432
-21.967374	-1.507444	0.455437
-21.227411	1.936539	0.460442
-21.129609	-3.089795	0.465446
-21.489403	-3.473423	0.470451
-21.361699	0.651161	0.475456
-21.852965	-4.466947	0.480461
-22.579156	-8.710112	0.485466
-22.484094	-3.118846	0.490470
-23.085525	-2.901723	0.495475
-23.086453	-0.629987	0.500480
-23.839615	-4.669644	0.505485
-24.132002	-6.016022	0.510490
-24.249391	-2.096879	0.515494
-24.381832	1.732863	0.520499
-24.567075	0.670349	0.525504
-24.730697	-7.017029	0.530509
-24.592415	-4.567659	0.535514
-24.862657	-3.519446	0.540518
-25.965270	4.608882	0.545523
-25.818321	-1.497579	0.550528
-26.295511	5.941772	0.555533
-25.666587	7.653551	0.560538
-25.885883	3.176443	0.565542
-26.890528	7.891769	0.570547
-27.097176	-0.465931	0.575552
-27.379161	1.805275	0.580557
-27.495194	-10.258497	0.585562
-27.269812	-2.564720	0.590566
-28.169411	3.640142	0.595571
-28.316186	-1.759385	0.600576
-28.713085	-0.710434	0.605581
-28.794143	1.004324	0.610586
-28.945194	-10.832541	0.615590
-29.238591	2.275905	0.620595
-29.416573	-2.378471	0.625600
-29.903231	6.242391	0.630605
-30.270080	-7.405278	0.635610
-30.046149	-3.026769	0.640614
-30.677398	8.694828	0.645619
-30.605499	7.924458	0.650624
-30.864096	4.329797	0.655629
-31.272286	3.988505	0.660634
-31.427783	-0.451081	0.665638
-31.700925	-0.433763	0.670643
-31.556540	-2.278401	0.675648
-32.313205	0.541257	0.680653
-32.991197	3.835868	0.685658
-33.364033	2.815215	0.690662
-33.773342	0.012786	0.695667
-33.061390	7.567535	0.700672
-33.343655	5.276815	0.705677
-33.445174	5.517339	0.710682
-33.039102	-2.144849	0.715686
-34.239503	1.870154	0.720691
-34.452116	1.390847	0.725696
-34.598721	11.936041	0.730701
-35.105498	5.358744	0.735706
-35.731281	-1.741004	0.740710
-36.066044	5.043442	0.745715
-36.264144	-6.042643	0.750720
-36.053754	9.344278	0.755725
-36.345017	-6.418981	0.760730
-36.400993	-3.471146	0.765734
-36.591302	2.838407	0.770739
-36.075532	-7.536279	0.775744
-37.228877	0.903655	0.780749
-37.762876	1.464606	0.785754
-37.707598	1.598462	0.790758
-37.939107	2.090171	0.795763
-37.835445	-9.106169	0.800768
-38.896290	4.067985	0.805773
-39.062762	3.606803	0.810778
-39.006150	-0.641189	0.815782
-39.280317	2.517782	0.820787
-39.292846	4.864089	0.825792
-39.794907	4.085012	0.830797
-40.340073	7.937888	0.835802
-40.482116	-0.483652	0.840806
-40.821554	-1.677177	0.845811
-40.674371	-0.137156	0.850816
-40.877251	0.489295	0.855821
-40.835948	-8.043043	0.860826
-41.011949	-6.145830	0.865830
-42.151458	5.300572	0.870835
-42.361794	-4.853499	0.875840
-42.098306	-9.813881	0.880845
-42.056366	-1.205726	0.885850
-42.644148	-1.183710	0.890854
-43.315598	7.086288	0.895859
-43.451654	1.685091	0.900864
-43.529302	-1.267050	0.905869
-43.785582	2.316228	0.910874
-43.610214	-10.121932	0.915878
-44.618654	-1.056014	0.920883
-44.662759	-16.921018	0.925888
-44.986344	-10.837482	0.930893
-45.282439	-0.420876	0.935898
-45.217195	-2.664464	0.940902
-45.438842	5.529171	0.945907
-45.332348	-5.344920	0.950912
-45.954768	-4.757547	0.955917
-46.443440	-13.865402	0.960922
-46.170421	-13.917303	0.965926
-46.731715	1.029797	0.970931
-46.954024	-16.215280	0.975936
-47.495113	-10.841334	0.980941
-47.825897	-9.619186	0.985946
-48.018031	-3.492842	0.990950
-48.510640	-1.717170	0.995955
-48.088396	-4.316888	1.000960
-48.332471	-3.506859	1.005965
-48.932852	-5.868265	1.010970
-49.520014	-0.620015	1.015974
-49.766469	2.170823	1.020979
-49.937413	-7.742614	1.025984
-50.018261	-8.356327	1.030989
-50.078663	-1.902493	1.035994
-49.768152	-3.507250	1.040998
-50.080054	2.995235	1.046003
-50.631172	2.109905	1.051008
-51.161279	-10.819502	1.056013
-51.590051	-4.811333	1.061018
-51.258541	-6.881250	1.066022
-51.651722	4.597639	1.071027
-51.725054	-6.764126	1.076032
-52.092096	4.682221	1.081037
-52.223285	4.332600	1.086042
-52.414067	-3.796621	1.091046
-53.463138	0.979403	1.096051
-53.609020	-2.098151	1.101056
-53.834965	3.147641	1.106061
-53.970763	2.599429	1.111066
-54.156039	-1.765919	1.116070
-54.342575	2.170317	1.121075
-54.096558	-5.776985	1.126080
-54.606551	-3.245660	1.131085
-55.423359	8.919263	1.136090
-55.300336	1.377072	1.141094
-55.692061	8.034351	1.146099
-55.800988	-5.147293	1.151104
-55.906152	-1.230053	1.156109
-56.267677	3.052957	1.161114
-56.606343	-2.626728	1.166118
-57.005094	8.024157	1.171123
-56.816524	-0.224240	1.176128
-57.243572	-3.419361	1.181133
-57.232437	-1.506994	1.186138
-57.678448	-4.243599	1.191142
-58.261594	-4.402632	1.196147
-58.013268	-14.409817	1.201152
-58.184229	-5.433171	1.206157
-58.876837	-1.411812	1.211162
-58.818438	-1.964952	1.216166
-59.606807	-1.250504	1.221171
-59.852590	-3.417192	1.226176
-59.951863	-2.284872	1.231181
-59.882814	6.692375	1.236186
-59.885444	-6.474182	1.241190
-60.727253	0.072845	1.246195
-60.890168	-2.540165	1.251200
-61.138611	0.829928	1.256205
-61.078468	-4.924504	1.261210
-61.528716	-11.156267	1.266214
-62.229472	-2.163567	1.271219
-62.540972	-10.447988	1.276224
-62.674648	-1.632164	1.281229
-63.100457	-2.676203	1.286234
-62.619094	-7.322509	1.291238
-62.999428	-0.508825	1.296243
-62.972392	-10.168358	1.301248
-63.261672	-1.015105	1.306253
-64.419157	-2.808896	1.311258
-64.170997	-8.858347	1.316262
-64.370866	-4.891563	1.321267
-64.023480	-6.536862	1.326272
-64.365724	-3.854493	1.331277
-65.394101	-6.506750	1.336282
-65.297286	-7.141798	1.341286
-65.993409	1.176328	1.346291
-65.870058	-9.390347	1.351296
-65.764080	-10.476058	1.356301
-65.994206	-7.330273	1.361306
-66.739453	-3.844865	1.366310
-67.220227	1.975257	1.371315
-66.969428	-3.473515	1.376320
-67.099304	2.136955	1.381325
-67.425370	2.981896	1.386330
-68.095099	-2.934132	1.391334
-68.655630	-1.695194	1.396339
-68.658552	-3.036023	1.401344
-68.769757	3.128340	1.406349
-68.400703	-3.866881	1.411354
-68.419207	-9.476194	1.416358
-69.177373	1.132574	1.421363
-69.638947	-6.173064	1.426368
-69.940860	-9.843230	1.431373
-70.330279	6.070492	1.436378
-69.885689	-5.349767	1.441382
-70.511809	0.227240	1.446387
-71.163636	-4.540010	1.451392
-71.708491	-2.522094	1.456397
-71.880520	4.654613	1.461402
-71.768595	-8.972686	1.466406
-71.584653	0.568777	1.471411
-71.462565	-3.091480	1.476416
-71.944234	-9.267733	1.481421
-72.859696	0.289889	1.486426
-73.038820	-5.101434	1.491430
-73.358674	3.357417	1.496435
-72.718688	-7.517481	1.501440
-73.360005	-7.170765	1.506445
-74.185871	3.467527	1.511450
-74.630113	-7.007611	1.516454
-74.518779	-2.649536	1.521459
-74.589262	-8.772756	1.526464
-74.708067	-3.031139	1.531469
-74.805823	-3.847856	1.536474
-75.289611	-14.117523	1.541478
-76.118939	-5.421170	1.546483
-76.024147	-5.768012	1.551488
-76.304436	-4.604344	1.556493
-76.749166	-4.459073	1.561498
-76.549575	-2.139468	1.566502
-76.637877	-9.019186	1.571507
-76.561448	-0.255056	1.576512
-77.443580	-7.219976	1.581517
-77.603408	-5.059536	1.586522
-77.650392	-11.293977	1.591526
-78.008465	-7.198162	1.596531
-78.305967	-7.781306	1.601536
-78.971401	-4.763889	1.606541
-79.347738	-4.059812	1.611546
-79.538887	-9.578970	1.616550
-79.726530	-6.591654	1.621555
-79.469880	0.951724	1.626560
-79.530010	-8.317764	1.631565
-79.479873	-4.990998	1.636570
-80.370201	-3.561510	1.641574
-80.908356	-7.827621	1.646579
-81.058053	-6.763378	1.651584
-81.388105	-7.104181	1.656589
-81.071150	-12.493650	1.661594
-81.262949	-11.252015	1.666598
-82.090593	-1.268322	1.671603
-82.133337	-1.853168	1.676608
-82.275213	-2.621889	1.681613
-82.488438	-4.338082	1.686618
-82.637057	-14.204370	1.691622
-83.593685	-1.527322	1.696627
-83.558922	-4.702601	1.701632
-83.796861	-10.828219	1.706637
-83.942900	-3.911817	1.711642
-83.602408	-7.359315	1.716646
-84.542220	-7.004087	1.721651
-85.126910	-10.120879	1.726656
-85.431297	-2.585058	1.731661
-85.640128	7.254835	1.736666
-85.334352	-3.191555	1.741670
-85.420202	-2.013870	1.746675
-85.693042	-3.303181	1.751680
-85.824594	10.393811	1.756685
-85.890727	-0.032638	1.761690
-86.224537	-4.292603	1.766694
-86.807610	1.249229	1.771699
-86.634761	-4.728387	1.776704
-87.840509	-4.224189	1.781709
-88.178974	-1.093171	1.786714
-87.943559	-8.687655	1.791718
-88.394920	-1.220696	1.796723
-88.363495	-1.038835	1.801728
-88.744728	1.039023	1.806733
-88.542297	9.318483	1.811738
-88.714304	-2.891590	1.816742
-89.496765	-7.537262	1.821747
-89.635680	-8.973971	1.826752
-89.484989	-12.812679	1.831757
-90.187985	-3.307123	1.836762
-90.691048	-10.590479	1.841766
-91.366564	2.188329	1.846771
-91.250490	-5.523611	1.851776
-91.380421	-8.227173	1.856781
-91.100103	-8.340320	1.861786
-91.360561	-10.830576	1.866790
-91.780694	-11.752117	1.871795
-91.877161	-5.495143	1.876800
-92.510591	-3.884200	1.881805
-92.709090	-4.204358	1.886810
-92.705194	-15.755301	1.891814
-92.947468	-2.803517	1.896819
-93.081168	-10.811910	1.901824
-93.470538	-12.991040	1.906829
-94.299026	-13.415581	1.911834
-94.248769	-13.761816	1.916838
-94.466038	-3.401779	1.921843
-94.689210	-8.422423	1.926848
-95.223253	-6.488446	1.931853
-95.515821	-9.179339	1.936858
-95.583281	-13.411172	1.941862
-95.868337	-6.080836	1.946867
-95.608780	-9.319587	1.951872
-95.822103	6.743878	1.956877
-96.219708	1.566900	1.961882
-96.600002	-6.336664	1.966886
-97.147358	0.186660	1.971891
-97.443602	-7.027662	1.976896
-97.158763	-8.603113	1.981901
-97.806148	0.510986	1.986906
-97.201740	-9.475714	1.991910
-98.127178	-3.269996	1.996915
-98.430148	-11.869410	2.006912
-98.581087	-8.053990	2.016909
-97.918234	-2.569199	2.026906
-97.347605	-4.995602	2.036902
-96.375764	-5.016846	2.046899
-96.006662	-2.508291	2.056896
-96.149586	-2.080375	2.066893
-95.421215	1.845217	2.076890
-94.862688	-6.157601	2.086886
-94.023650	-3.753892	2.096883
-93.781221	-2.524366	2.106880
-93.282082	-5.338767	2.116877
-92.375737	-6.252604	2.126874
-92.254134	-3.749860	2.136870
-91.785367	-7.329280	2.146867
-90.792286	-6.048743	2.156864
-90.528018	-5.405472	2.166861
-90.588298	-6.944888	2.176858
-89.726366	-9.030189	2.186854
-89.561281	-1.000265	2.196851
-88.573550	-0.783238	2.206848
-87.985003	1.840032	2.216845
-87.915944	-7.059056	2.226842
-86.938952	-9.998542	2.236838
-86.564444	-2.191287	2.246835
-86.382548	-7.734355	2.256832
-85.338048	-1.738801	2.266829
-85.112102	-1.925832	2.276826
-85.052139	0.402784	2.286822
-83.831696	1.236121	2.296819
-83.473930	-2.259495	2.306816
-83.452724	-4.084020	2.316813
-82.284673	2.738071	2.326810
-81.999130	-2.171760	2.336806
-82.173318	-2.470713	2.346803
-81.200267	0.494985	2.356800
-80.789294	1.416346	2.366797
-80.255392	-1.406636	2.376794
-79.497721	5.558545	2.386790
-79.476685	-2.785058	2.396787
-78.432823	-4.762475	2.406784
-78.364146	4.685749	2.416781
-77.691581	3.855827	2.426778
-76.818872	1.553444	2.436774
-76.683871	-0.748114	2.446771
-76.310093	-5.481622	2.456768
-75.641165	-0.415909	2.466765
-75.269262	-4.930554	2.476762
-74.405398	-5.277095	2.486758
-73.787708	2.384598	2.496755
-73.504257	0.398869	2.506752
-73.411065	3.371688	2.516749
-72.572287	0.159126	2.526746
-72.167617	5.256483	2.536742
-71.986583	1.034473	2.546739
-71.034565	0.509486	2.556736
-70.758730	-2.849834	2.566733
-69.863199	-4.965708	2.576730
-69.464309	-1.159870	2.586726
-69.123107	-3.949680	2.596723
-68.723220	1.937175	2.606720
-67.988125	6.558615	2.616717
-67.963893	3.400021	2.626714
-67.033582	1.848915	2.636710
-66.157651	-1.119184	2.646707
-66.363581	-0.130281	2.656704
-65.527100	2.064761	2.666701
-64.995455	1.697090	2.676698
-64.979624	5.587914	2.686694
-64.219008	-1.575258	2.696691
-63.594303	-3.268842	2.706688
-63.297225	0.856947	2.716685
-62.596778	1.283425	2.726682
-62.403758	-0.631205	2.736678
-61.014920	0.590882	2.746675
-60.680590	-1.931773	2.756672
-60.149725	3.788977	2.766669
-60.529052	3.949601	2.776666
-60.355120	0.770867	2.786662
-59.308221	-5.679800	2.796659
-58.539389	-6.721106	2.806656
-58.269729	1.447756	2.816653
-57.235909	-3.046411	2.826650
-56.715499	-3.301464	2.836646
-56.541949	-2.067547	2.846643
-56.233650	9.437215	2.856640
-55.891213	0.685617	2.866637
-55.011636	-4.221675	2.876634
-54.710850	5.161903	2.886630
-53.772591	7.889110	2.896627
-53.581283	7.913372	2.906624
-53.333366	1.913376	2.916621
-52.561957	5.414136	2.926618
-52.363599	2.918986	2.936614
-51.047415	7.240885	2.946611
-50.755309	5.912687	2.956608
-50.682648	6.341881	2.966605
-50.485515	3.083508	2.976602
-49.309285	10.566380	2.986598
-49.002796	8.992031	2.996595
-48.415262	3.594868	3.006592
-48.277037	10.320726	3.016589
-47.585112	10.751699	3.026586
-47.432758	10.658486	3.036582
-46.718796	12.042671	3.046579
-45.994078	18.506161	3.056576
-45.056608	15.819906	3.066573
-44.893746	14.438974	3.076570
-44.797823	12.941756	3.086566
-44.500117	14.153176	3.096563
-43.607890	5.705599	3.106560
-42.710441	7.618729	3.116557
-42.012982	10.741379	3.126554
-42.236646	6.519023	3.136550
-41.874651	10.156387	3.146547
-41.224729	5.021931	3.156544
-40.677391	9.742297	3.166541
-39.843924	5.003734	3.176538
-39.086923	3.767873	3.186534
-39.309970	7.952474	3.196531
-38.794956	8.296956	3.206528
-37.889273	9.651290	3.216525
-37.830703	7.184240	3.226522
-36.854759	6.744225	3.236518
-36.223978	4.761434	3.246515
-35.816054	7.900655	3.256512
-35.979036	2.579166	3.266509
-34.922867	5.512922	3.276506
-34.893188	8.942276	3.286502
-34.183659	4.707667	3.296499
-33.296680	8.995028	3.306496
-33.131812	8.123783	3.316493
-32.296908	10.011807	3.326490
-32.285948	8.857258	3.336486
-31.754176	9.598260	3.346483
-30.507635	8.764500	3.356480
-30.380872	6.492732	3.366477
-30.211093	5.883640	3.376474
-29.615263	9.094970	3.386470
-28.965794	6.450391	3.396467
-28.410969	12.347973	3.406464
-27.767921	1.968890	3.416461
-27.396796	2.624035	3.426458
-27.427422	8.311839	3.436454
-26.403163	10.620194	3.446451
-25.545825	10.366533	3.456448
-25.412471	9.284791	3.466445
-25.372360	6.649560	3.476442
-24.697520	11.609826	3.486438
-24.206438	7.792518	3.496435
-23.090810	12.655646	3.506432
-22.821294	9.205443	3.516429
-22.772650	11.589675	3.526426
-22.216427	10.223522	3.536422
-21.507944	11.174588	3.546419
-21.021560	9.908004	3.556416
-19.964315	8.495520	3.566413
-19.642136	6.725499	3.576410
-19.875755	9.495789	3.586406
-19.040731	7.183435	3.596403
-18.189498	4.624646	3.606400
-17.927206	10.919390	3.616397
-18.033139	2.969336	3.626394
-17.017226	5.130108	3.636390
-16.424664	7.885800	3.646387
-15.647732	10.714153	3.656384
-15.105616	9.514917	3.666381
-15.101143	5.253872	3.676378
-14.904393	6.908649	3.686374
-14.158144	3.143476	3.696371
-13.598952	1.678664	3.706368
-12.936935	8.997689	3.716365
-12.530114	1.360594	3.726362
-12.267802	7.845396	3.736358
-11.105451	8.174617	3.746355
-10.867778	11.619103	3.756352
-10.525659	9.668586	3.766349
-9.470703	4.588272	3.776346
-9.390555	9.371877	3.786342
-9.393989	5.270448	3.796339
-8.755754	8.503686	3.806336
-8.113718	5.853928	3.816333
-6.905383	10.119767	3.826330
-6.802274	3.077969	3.836326
-6.302755	6.494358	3.846323
-6.288839	11.652560	3.856320
-5.357056	7.434029	3.866317
-5.135673	12.379371	3.876314
-4.987128	10.538185	3.886310
-4.254263	22.252447	3.896307
-3.642926	31.280425	3.906304
-3.200313	31.870590	3.916301
-2.521318	39.830027	3.926298
-2.211814	52.101219	3.936294
-2.061575	59.956097	3.946291
-1.542825	70.826275	3.956288
-0.629520	80.234903	3.966285
-0.130506	100.132967	3.976282
0.000000	103.800738	3.981286
0.212166	102.439067	3.986291
0.712957	117.505634	3.991296
0.411893	119.090147	3.996301
1.217357	124.915686	4.001306
0.708125	127.772767	4.006310
1.090274	115.413049	4.011315
0.980219	124.981378	4.016320
0.725620	115.659842	4.021325
0.697439	106.473896	4.026330
0.854700	121.973593	4.031334
0.546142	117.127549	4.036339
0.768598	129.883699	4.041344
0.826646	121.500545	4.046349
1.258721	111.875951	4.051354
0.855512	113.859170	4.056358
1.125081	123.197554	4.061363
0.734973	116.538775	4.066368
0.580907	117.967527	4.071373
0.869492	117.543055	4.076378
0.688921	125.078638	4.081382
0.897452	121.351112	4.086387
0.878477	109.170907	4.091392
0.879164	118.279078	4.096397
1.190699	123.998028	4.101402
1.010987	119.748836	4.106406
0.772161	117.005261	4.111411
0.988226	121.125607	4.116416
0.984068	125.786428	4.121421
0.999415	114.141863	4.126426
1.102651	129.536086	4.131430
1.373391	117.472115	4.136435
1.000521	119.814432	4.141440
0.965874	131.911444	4.146445
1.369040	130.203667	4.151450
1.211213	128.659162	4.156454
1.466303	129.903991	4.161459
1.201287	124.282396	4.166464
0.933433	128.408488	4.171469
1.099488	119.467532	4.176474
1.384083	136.446991	4.181478
1.606188	133.843614	4.186483
1.233188	129.377749	4.191488
1.045273	126.328861	4.196493
1.477701	116.425807	4.201498
0.864912	127.217657	4.206502
1.617565	129.229716	4.211507
1.570263	140.936410	4.216512
1.296091	132.209519	4.221517
1.294193	120.358833	4.226522
0.918051	128.601891	4.231526
1.621232	128.255232	4.236531
2.152521	135.876132	4.241536
1.469969	126.418747	4.246541
1.277842	119.368483	4.251546
1.247007	123.628509	4.256550
1.052840	121.517040	4.261555
1.532560	136.539449	4.266560
1.714800	131.639131	4.271565
1.709338	120.918427	4.276570
1.177848	118.172964	4.281574
1.602085	120.157063	4.286579
1.319849	123.703280	4.291584
1.758848	132.999471	4.296589
1.738911	128.098995	4.301594
1.445266	133.260458	4.306598
1.376390	123.650581	4.311603
1.295812	136.801920	4.316608
1.934733	141.827679	4.321613
2.075361	144.979039	4.326618
1.625743	129.262455	4.331622
1.537119	124.666896	4.336627
1.450510	132.959787	4.341632
1.276368	131.705715	4.346637
1.856153	132.713335	4.351642
1.658328	142.200429	4.356646
1.775097	137.810162	4.361651
2.003667	153.333584	4.366656
1.703275	138.362529	4.371661
1.738403	132.131067	4.376666
1.404317	129.721852	4.381670
1.680664	135.142572	4.386675
1.860289	145.323852	4.391680
1.827205	152.795356	4.396685
2.282307	148.308117	4.401690
1.960802	146.007670	4.406694
1.660809	140.306096	4.411699
1.806880	123.145885	4.416704
1.708702	129.305104	4.421709
1.577167	130.644930	4.426714
1.854694	142.487707	4.431718
2.327108	140.000376	4.436723
2.028061	147.396231	4.441728
2.202373	133.509173	4.446733
2.010731	125.702715	4.451738
1.371988	134.856670	4.456742
1.759828	129.535210	4.461747
2.294190	145.574147	4.466752
2.039294	134.275356	4.471757
1.934342	125.496811	4.476762
1.550951	131.102505	4.481766
2.120614	136.294064	4.486771
2.372587	140.990938	4.491776
2.055275	136.301272	4.496781
2.019053	131.843080	4.501786
1.845658	133.806339	4.506790
2.163001	143.118313	4.511795
1.884855	141.481812	4.516800
2.079909	148.433753	4.521805
2.148142	148.166971	4.526810
1.791457	147.048885	4.531814
2.471115	139.783787	4.536819
2.503956	140.696236	4.541824
2.041201	136.902386	4.546829
2.390609	132.630918	4.551834
2.243562	128.585441	4.556838
1.882384	125.101635	4.561843
2.260423	133.815713	4.566848
2.177529	133.180168	4.571853
2.403323	135.837390	4.576858
2.448569	150.702837	4.581862
2.428199	134.033589	4.586867
2.025307	129.164266	4.591872
1.728784	134.727962	4.596877
2.537340	144.232368	4.601882
2.033255	143.855384	4.606886
2.650311	142.930529	4.611891
2.441756	148.603916	4.616896
2.214807	148.658332	4.621901
2.302927	140.529908	4.626906
2.287606	149.526695	4.631910
2.336902	144.087104	4.636915
2.497087	147.317675	4.641920
2.347104	140.362079	4.646925
2.607755	140.982801	4.651930
2.420756	143.808696	4.656934
2.295087	136.200764	4.661939
2.380405	148.453111	4.666944
2.267963	139.020847	4.671949
2.382513	143.568280	4.676954
2.206034	144.630375	4.681958
2.112780	144.581720	4.686963
2.204738	145.054706	4.691968
2.176662	148.292444	4.696973
2.676106	142.719493	4.701978
2.315028	146.315953	4.706982
2.497988	154.753539	4.711987
3.015494	162.531616	4.716992
2.688994	155.869246	4.721997
2.407975	150.553845	4.727002
2.386223	154.208203	4.732006
2.666854	156.632270	4.737011
2.576715	158.063727	4.742016
2.649667	164.208967	4.747021
3.194917	163.402856	4.752026
2.451530	156.099895	4.757030
2.609701	143.654810	4.762035
2.771993	154.022287	4.767040
2.888477	165.839534	4.772045
2.650679	149.685003	4.777050
2.358488	155.146794	4.782054
2.578964	156.017374	4.787059
2.997104	159.707645	4.792064
2.857422	170.058874	4.797069
2.962627	168.024171	4.802074
2.790679	168.803995	4.807078
2.913254	156.231570	4.812083
2.448059	163.526754	4.817088
2.444373	161.891810	4.822093
2.906198	159.165686	4.827098
2.760772	157.875505	4.832102
2.854243	157.677558	4.837107
2.789234	164.533959	4.842112
3.019372	158.503073	4.847117
3.032856	162.363912	4.852122
2.960629	161.381865	4.857126
2.922128	162.552188	4.862131
2.802173	157.009234	4.867136
2.617341	170.920293	4.872141
3.011570	167.388465	4.877146
2.946402	168.781235	4.882150
2.940924	158.092147	4.887155
3.005713	159.787376	4.892160
3.183578	169.851889	4.897165
3.156270	163.415007	4.902170
3.303969	163.132689	4.907174
3.331721	153.877900	4.912179
2.803864	158.420957	4.917184
2.940258	162.759356	4.922189
2.912947	160.397283	4.927194
2.645983	163.808255	4.932198
2.836206	153.224738	4.937203
3.054001	167.810241	4.942208
3.463021	168.967834	4.947213
3.351377	163.290710	4.952218
2.730064	168.202651	4.957222
3.320899	167.465370	4.962227
3.132664	170.405353	4.967232
2.920830	177.281455	4.972237
3.447657	178.199249	4.977242
3.183730	195.665955	4.982246
3.485909	184.552474	4.987251
3.547905	182.840864	4.992256
2.873915	173.597250	4.997261
3.492387	174.984817	5.002266
3.523801	173.610155	5.007270
3.036403	170.696471	5.012275
3.248612	174.181532	5.017280
3.535219	190.572288	5.022285
3.509689	179.721799	5.027290
3.254354	176.578998	5.032294
3.330727	180.379431	5.037299
3.745535	180.884407	5.042304
3.531533	183.527856	5.047309
2.977224	172.440169	5.052314
3.052382	183.596329	5.057318
3.751204	181.915278	5.062323
3.783507	190.759142	5.067328
3.390758	192.585721	5.072333
4.013432	187.926854	5.077338
3.276640	171.068567	5.082342
3.279801	166.876311	5.087347
3.154411	162.776834	5.092352
3.554863	171.860755	5.097357
3.600108	174.093688	5.102362
3.739366	185.983332	5.107366
3.927056	183.679527	5.112371
3.442661	171.116175	5.117376
3.561494	178.665275	5.122381
3.610787	180.941871	5.127386
3.870448	186.115274	5.132390
3.593700	169.042997	5.137395
3.502950	167.196987	5.142400
3.378501	172.139134	5.147405
3.787699	169.728078	5.152410
3.684704	182.092024	5.157414
3.884447	179.884417	5.162419
3.892869	175.020641	5.167424
3.726520	173.809644	5.172429
3.835119	161.777215	5.177434
3.611790	176.007475	5.182438
3.753330	172.195458	5.187443
3.922849	183.960170	5.192448
3.828211	187.319006	5.197453
3.882798	178.151773	5.202458
3.574433	177.836061	5.207462
3.892310	183.088983	5.212467
3.771573	182.962351	5.217472
3.936761	187.324746	5.222477
3.793469	183.477983	5.227482
3.548836	189.770753	5.232486
3.628604	191.065030	5.237491
3.989996	185.747672	5.242496
3.767991	192.403906	5.247501
4.033503	182.877971	5.252506
3.872960	192.327651	5.257510
3.876659	184.275624	5.262515
4.056145	189.597549	5.267520
3.840792	187.017984	5.272525
4.099636	195.111588	5.277530
3.638106	197.214626	5.282534
3.804552	194.350993	5.287539
3.662750	196.518142	5.292544
3.678148	197.192870	5.297549
3.786841	183.043913	5.302554
3.631444	201.477629	5.307558
3.918079	206.248216	5.312563
4.335553	217.272007	5.317568
3.851076	214.721684	5.322573
4.274911	213.880692	5.327578
4.348854	215.688394	5.332582
4.250180	216.839617	5.337587
4.436142	215.852167	5.342592
4.050757	212.372113	5.347597
4.276185	208.053494	5.352602
3.807200	214.355895	5.357606
4.269630	210.857731	5.362611
4.033681	217.772404	5.367616
4.011838	225.463646	5.372621
3.739095	227.578421	5.377626
3.806795	229.450369	5.382630
3.688621	221.414137	5.387635
3.751541	228.133588	5.392640
3.960382	238.784925	5.397645
4.846385	230.699906	5.402650
4.550695	240.585095	5.407654
4.383002	226.425354	5.412659
4.449629	232.372291	5.417664
4.273228	226.847594	5.422669
4.176744	214.195343	5.427674
3.987824	220.647124	5.432678
4.510125	223.982677	5.437683
4.794300	235.387893	5.442688
4.428467	226.855556	5.447693
4.509842	224.508189	5.452698
4.182701	227.261006	5.457702
4.368479	234.350463	5.462707
4.548876	229.285894	5.467712
4.278174	234.386867	5.472717
4.629747	231.788627	5.477722
4.759915	239.585918	5.482726
4.528335	229.836805	5.487731
4.388674	228.150261	5.492736
4.098456	238.657842	5.497741
4.343553	236.550732	5.502746
4.418635	248.289061	5.507750
4.506886	236.901978	5.512755
4.395918	234.799687	5.517760
4.606975	237.592093	5.522765
4.687568	238.737552	5.527770
4.706298	238.744226	5.532774
4.379145	236.808469	5.537779
4.551794	242.099838	5.542784
4.531698	234.946816	5.547789
4.662068	231.845190	5.552794
4.416007	230.925005	5.557798
4.470608	230.081390	5.562803
4.579859	230.238482	5.567808
4.561083	232.010002	5.572813
4.718726	231.118708	5.577818
4.703810	247.015472	5.582822
4.769767	238.238735	5.587827
5.095234	243.949227	5.592832
4.772077	243.015735	5.597837
5.088624	231.871514	5.602842
4.675705	238.051300	5.607846
4.847691	235.458875	5.612851
5.009251	230.375093	5.617856
4.685079	239.182737	5.622861
5.157956	237.280601	5.627866
5.022860	232.031040	5.632870
4.841539	237.845745	5.637875
4.669626	238.337672	5.642880
4.612534	237.068532	5.647885
4.824966	228.332267	5.652890
4.842269	237.618242	5.657894
4.948864	251.224567	5.662899
5.493064	249.747915	5.667904
5.001402	249.141208	5.672909
5.087023	228.450145	5.677914
4.554756	238.163364	5.682918
4.649130	229.951669	5.687923
4.780299	247.097488	5.692928
4.803479	263.048446	5.697933
4.987326	257.723909	5.702938
4.830770	264.553473	5.707942
4.999664	258.937041	5.712947
5.390287	252.561604	5.717952
5.006861	252.441072	5.722957
5.273755	258.144869	5.727962
5.107268	259.778043	5.732966
5.335083	262.896867	5.737971
5.357481	260.922502	5.742976
5.270767	271.993191	5.747981
5.555854	254.162654	5.752986
5.333656	258.844803	5.757990
5.385007	255.078448	5.762995
5.126113	249.623534	5.768000
5.326811	266.711092	5.773005
4.868567	253.884187	5.778010
5.301217	257.904406	5.783014
5.556365	251.119802	5.788019
5.275990	249.005921	5.793024
5.380131	256.171372	5.798029
5.628226	250.213587	5.803034
5.088332	245.621821	5.808038
5.140560	242.886693	5.813043
5.168928	249.317308	5.818048
4.989493	263.996375	5.823053
5.154477	259.560607	5.828058
5.148858	266.929808	5.833062
5.413735	258.463768	5.838067
5.320341	259.762865	5.843072
5.741813	263.439983	5.848077
5.506809	254.539258	5.853082
5.407194	256.500533	5.858086
5.504705	256.150099	5.863091
5.242738	253.416433	5.868096
5.303455	253.834176	5.873101
5.299394	253.161043	5.878106
5.093250	259.147295	5.883110
5.108012	253.384023	5.888115
5.359015	258.315192	5.893120
5.206892	262.704864	5.898125
5.766088	259.935092	5.903130
5.472936	276.520595	5.908134
5.824415	279.898573	5.913139
5.523088	277.066630	5.918144
5.744539	278.351508	5.923149
5.575983	268.700126	5.928154
5.246229	261.683889	5.933158
5.725234	270.230457	5.938163
5.549509	274.490932	5.943168
5.751669	277.303712	5.948173
5.849595	275.266967	5.953178
6.113367	274.580605	5.958182
5.666088	269.161344	5.963187
5.350129	262.611184	5.968192
5.467509	278.636072	5.973197
5.627534	274.052379	5.978202
6.049935	284.654674	5.983206
6.034964	269.177171	5.988211
5.868777	284.344563	5.993216
5.795048	276.513353	5.998221
5.887974	262.629374	6.003226
5.501512	257.871349	6.008230
5.638093	267.834780	6.013235
5.905407	269.916094	6.018240
5.561056	277.100762	6.023245
5.721289	278.312916	6.028250
6.132628	282.551590	6.033254
5.712366	271.287949	6.038259
5.715721	268.206094	6.043264
5.433361	260.850290	6.048269
5.873162	277.558953	6.053274
5.885130	281.024593	6.058278
5.549647	280.108836	6.063283
5.502209	277.522095	6.068288
5.681530	300.956213	6.073293
5.802883	284.619092	6.078298
5.433900	284.097685	6.083302
5.641528	282.613323	6.088307
5.339193	285.011117	6.093312
5.702015	284.334642	6.098317
5.887785	281.806502	6.103322
5.566154	283.172773	6.108326
5.839624	277.653946	6.113331
5.844607	289.305142	6.118336
5.763467	291.798209	6.123341
5.862890	285.268787	6.128346
5.927528	287.482897	6.133350
6.023415	292.308515	6.138355
6.314728	289.656376	6.143360
5.771686	296.925770	6.148365
6.070721	280.114908	6.153370
6.163462	264.247323	6.158374
5.736799	269.211241	6.163379
5.692747	261.780369	6.168384
5.675039	270.410602	6.173389
5.582375	265.537230	6.178394
5.416793	268.144679	6.183398
5.786546	264.958321	6.188403
5.918583	261.951342	6.193408
5.669104	259.513117	6.198413
5.738353	253.361720	6.203418
5.661176	266.775212	6.208422
5.670014	266.220290	6.213427
5.755759	265.843214	6.218432
5.729266	279.407009	6.223437
5.777448	271.484055	6.228442
5.876970	279.320936	6.233446
5.699509	278.054716	6.238451
5.985629	266.513422	6.243456
5.653672	260.902205	6.248461
5.722950	261.119303	6.253466
5.451200	267.027189	6.258470
5.692502	277.439382	6.263475
5.849555	278.585594	6.268480
5.690146	289.193058	6.273485
6.179304	278.936240	6.278490
5.814674	275.918004	6.283494
5.576443	268.330705	6.288499
5.633005	259.925571	6.293504
5.851763	272.163555	6.298509
5.946421	256.960052	6.303514
5.766066	268.978606	6.308518
5.484271	268.633446	6.313523
5.882772	270.918957	6.318528
5.665054	273.493396	6.323533
5.649345	269.345181	6.328538
5.581924	276.097599	6.333542
5.809534	275.986331	6.338547
5.955217	276.314917	6.343552
5.723709	274.342118	6.348557
5.686183	264.138838	6.353562
5.868067	277.306363	6.358566
5.820431	276.829834	6.363571
5.524416	268.299261	6.368576
5.890102	280.530193	6.373581
5.930866	264.740301	6.378586
5.562264	263.883485	6.383590
5.767572	267.255746	6.388595
5.942517	268.813614	6.393600
5.318131	275.143395	6.398605
5.998220	269.608717	6.403610
5.848429	275.329941	6.408614
5.456013	267.057982	6.413619
5.758746	265.552487	6.418624
5.732469	276.329037	6.423629
5.837334	278.834269	6.428634
5.859983	278.498654	6.433638
5.866929	277.659294	6.438643
5.723463	267.516798	6.443648
5.194620	271.022347	6.448653
5.913558	270.031004	6.453658
5.728793	285.944757	6.458662
5.885294	288.837413	6.463667
6.216354	275.014422	6.468672
5.952677	268.630123	6.473677
5.523867	263.109914	6.478682
5.568335	258.547380	6.483686
5.479419	260.314006	6.488691
5.666900	270.639664	6.493696
5.819757	272.466722	6.498701
5.995386	281.009911	6.503706
5.902321	275.225456	6.508710
5.715470	267.468810	6.513715
5.572669	259.423740	6.518720
5.430101	273.401063	6.523725
5.443439	276.268551	6.528730
5.650013	271.753540	6.533734
5.924519	290.506384	6.538739
6.229977	282.480095	6.543744
6.025445	288.238319	6.548749
5.786399	265.791295	6.553754
5.359845	260.473211	6.558758
5.624772	265.399051	6.563763
5.930118	267.449133	6.568768
6.154797	277.699403	6.573773
6.094705	268.935949	6.578778
5.405810	257.359810	6.583782
5.430450	262.038329	6.588787
5.864427	264.906761	6.593792
5.601870	271.059984	6.598797
5.964055	271.873706	6.603802
5.805583	269.683897	6.608806
5.715265	264.832306	6.613811
5.790697	257.022173	6.618816
5.483571	257.437078	6.623821
5.711192	267.155384	6.628826
5.916975	278.357703	6.633830
5.661338	272.171463	6.638835
5.830454	269.538352	6.643840
5.786955	281.991178	6.648845
5.929638	265.615953	6.653850
5.696547	260.169673	6.658854
5.472459	261.349917	6.663859
5.775704	262.033613	6.668864
5.774335	273.325128	6.673869
5.889359	270.504290	6.678874
5.653985	271.123154	6.683878
5.802604	277.573022	6.688883
5.931877	268.526989	6.693888
5.580045	273.754498	6.698893
5.832871	268.830498	6.703898
5.609049	269.691167	6.708902
5.861042	279.497433	6.713907
6.116489	274.902046	6.718912
5.627653	278.705082	6.723917
5.727137	265.841951	6.728922
5.829406	264.971932	6.733926
5.475148	264.128701	6.738931
5.849847	256.404847	6.743936
5.406435	270.881416	6.748941
6.052439	274.618489	6.753946
6.046946	279.380796	6.758950
5.747051	265.330190	6.763955
5.654277	272.671836	6.768960
5.454811	262.088818	6.773965
5.854986	263.168702	6.778970
5.679015	270.061402	6.783974
6.022059	271.248256	6.788979
6.083200	264.392615	6.793984
5.880029	266.787621	6.798989
5.840124	256.844138	6.803994
5.697360	258.578019	6.808998
5.933268	262.859820	6.814003
5.931721	262.300188	6.819008
5.660914	263.323194	6.824013
6.202364	260.065812	6.829018
6.043993	266.455908	6.834022
6.114347	264.733498	6.839027
6.042495	261.071743	6.844032
5.923082	268.360588	6.849037
6.012288	261.918185	6.854042
5.870056	248.023376	6.859046
5.811310	239.781734	6.864051
5.565478	234.119152	6.869056
5.498631	236.723879	6.874061
5.701495	237.486477	6.879066
6.058628	249.475115	6.884070
5.697476	244.855519	6.889075
5.559749	249.366330	6.894080
4.999728	256.543441	6.899085
5.553175	258.845953	6.904090
5.848891	263.235499	6.909094
5.389384	261.070415	6.914099
5.657081	252.961435	6.919104
5.411347	260.595804	6.924109
5.557343	253.015126	6.929114
5.544972	261.894455	6.934118
5.256093	260.939806	6.939123
5.496689	262.911387	6.944128
5.814123	272.697968	6.949133
6.365383	278.306879	6.954138
6.206607	272.656040	6.959142
6.004658	256.970382	6.964147
6.159043	258.528287	6.969152
5.708335	263.821807	6.974157
5.747512	255.061886	6.979162
5.703355	260.048502	6.984166
5.684342	265.720888	6.989171
5.410532	256.902132	6.994176
5.452063	256.070043	6.999181
5.726385	252.272136	7.004186
5.721795	262.295507	7.009190
5.542437	261.399735	7.014195
5.837698	257.060740	7.019200
5.646107	260.282829	7.024205
5.531058	255.204142	7.029210
5.743649	258.572104	7.034214
5.592221	258.143373	7.039219
5.654486	265.533641	7.044224
6.229580	269.522194	7.049229
5.856069	261.775629	7.054234
5.729851	256.761955	7.059238
5.617622	258.892870	7.064243
5.949682	262.985698	7.069248
5.546958	262.694167	7.074253
5.840396	253.005663	7.079258
5.613041	266.287516	7.084262
5.254163	261.620106	7.089267
5.640820	268.102510	7.094272
5.660234	272.310455	7.099277
6.005091	278.865808	7.104282
5.687824	281.357674	7.109286
5.843910	282.937462	7.114291
5.843779	282.115022	7.119296
5.863525	274.737485	7.124301
5.825294	265.515057	7.129306
5.592051	270.442533	7.134310
5.403399	264.359760	7.139315
5.944918	275.528786	7.144320
5.996119	283.199189	7.149325
5.931689	270.690599	7.154330
5.878294	267.380303	7.159334
5.834584	259.050891	7.164339
5.634973	260.110267	7.169344
5.602274	261.883958	7.174349
5.712807	256.263959	7.179354
5.881780	260.986443	7.184358
5.532851	260.620099	7.189363
5.341343	257.467346	7.194368
5.437298	278.646052	7.199373
6.043871	277.931626	7.204378
5.973191	279.850435	7.209382
5.892209	285.668515	7.214387
5.801932	266.169033	7.219392
5.359479	272.517942	7.224397
5.714519	267.916542	7.229402
5.352145	277.521074	7.234406
5.530235	284.782588	7.239411
6.326391	274.354589	7.244416
6.071349	281.756304	7.249421
6.201386	270.112762	7.254426
5.908117	267.225783	7.259430
5.284167	260.049712	7.264435
5.810511	266.013667	7.269440
5.313863	270.023556	7.274445
6.266239	270.558730	7.279450
5.941301	268.043670	7.284454
5.734830	264.829972	7.289459
5.935340	261.948370	7.294464
5.263373	259.781565	7.299469
5.487047	259.186866	7.304474
5.713907	271.499517	7.309478
5.962814	277.196630	7.314483
6.026142	268.110246	7.319488
5.633172	264.587071	7.324493
5.516161	254.437299	7.329498
5.970758	271.535949	7.334502
5.938913	272.246509	7.339507
5.815051	262.733701	7.344512
5.129377	265.706858	7.349517
5.516573	274.751767	7.354522
5.993195	282.710267	7.359526
6.002985	281.108014	7.364531
5.798077	268.558024	7.369536
5.625643	263.665436	7.374541
5.691657	269.552371	7.379546
5.741498	277.159710	7.384550
5.715739	272.551160	7.389555
6.113313	271.549743	7.394560
5.890050	262.941408	7.399565
5.719601	262.430218	7.404570
5.671662	265.557177	7.409574
5.902038	255.631722	7.414579
5.614456	256.151150	7.419584
5.395785	266.843756	7.424589
5.720774	270.298622	7.429594
6.184896	277.344759	7.434598
5.906331	274.607347	7.439603
5.757803	267.521763	7.444608
5.826742	261.990494	7.449613
5.928112	258.633957	7.454618
5.847500	260.712494	7.459622
5.547534	260.727660	7.464627
5.620204	254.161287	7.469632
5.650662	265.194746	7.474637
5.395244	266.281793	7.479642
5.755369	271.642056	7.484646
5.916683	281.829429	7.489651
5.985703	266.069938	7.494656
5.985607	262.820945	7.499661
5.857880	258.895813	7.504666
6.077536	261.414807	7.509670
5.880584	268.718889	7.514675
6.146790	260.809450	7.519680
5.614451	259.310589	7.524685
5.901292	257.889824	7.529690
5.840207	256.254317	7.534694
5.666989	264.709447	7.539699
5.806579	262.229627	7.544704
5.451301	272.421498	7.549709
5.825982	263.663118	7.554714
5.809852	263.782785	7.559718
5.405413	267.993448	7.564723
5.879789	268.236057	7.569728
5.575242	265.847534	7.574733
5.943286	263.082213	7.579738
6.012905	264.115489	7.584742
5.860218	268.347066	7.589747
6.050218	265.495573	7.594752
5.738334	259.147256	7.599757
5.758231	255.749622	7.604762
5.651835	260.350468	7.609766
5.801098	264.013023	7.614771
5.871110	253.122303	7.619776
5.957614	252.083900	7.624781
5.707061	259.930986	7.629786
5.758493	261.571358	7.634790
5.689108	267.969745	7.639795
5.867083	260.896602	7.644800
5.889375	263.632984	7.649805
6.141775	257.418268	7.654810
5.746720	247.571214	7.659814
5.470697	248.104660	7.664819
5.947148	248.910081	7.669824
5.767317	269.733091	7.674829
5.675100	261.825674	7.679834
5.579153	266.731772	7.684838
5.808122	266.686730	7.689843
5.821991	256.712729	7.694848
5.617871	267.216412	7.699853
5.850083	254.686957	7.704858
5.786178	271.970739	7.709862
5.710496	271.685234	7.714867
5.832104	269.616329	7.719872
5.745548	268.377084	7.724877
5.626966	265.010500	7.729882
5.905484	268.456782	7.734886
5.841008	271.459769	7.739891
5.624774	264.213889	7.744896
5.774238	272.400488	7.749901
5.987233	264.679662	7.754906
5.751004	257.800721	7.759910
5.565405	258.035357	7.764915
5.659277	250.614653	7.769920
5.635765	257.145096	7.774925
6.061264	258.550060	7.779930
5.480082	253.863482	7.784934
5.486215	268.140344	7.789939
6.034664	257.953398	7.794944
5.508861	269.513221	7.799949
5.872807	258.023089	7.804954
5.808721	261.532203	7.809958
5.712994	267.067841	7.814963
6.060631	264.422754	7.819968
5.678723	274.973105	7.824973
5.894116	266.954518	7.829978
5.619029	257.047652	7.834982
5.745268	252.570462	7.839987
5.724740	264.057939	7.844992
5.534419	265.811880	7.849997
6.050423	261.188584	7.855002
6.020515	259.522913	7.860006
5.827588	256.421001	7.865011
5.921475	243.615704	7.870016
5.336428	244.301666	7.875021
5.459710	246.595223	7.880026
5.867242	253.520450	7.885030
5.729730	258.243197	7.890035
5.754516	259.631459	7.895040
5.668521	266.051413	7.900045
5.867879	257.763250	7.905050
5.729495	258.661236	7.910054
5.682846	261.563372	7.915059
6.025903	255.442107	7.920064
5.710494	253.574121	7.925069
5.546847	254.238764	7.930074
5.647957	255.042515	7.935078
5.730995	258.152243	7.940083
5.724702	262.800778	7.945088
5.476070	266.164624	7.950093
5.413090	264.890071	7.955098
5.927583	263.930560	7.960102
5.829330	259.099188	7.965107
5.955232	265.147637	7.970112
5.913568	262.794112	7.975117
5.678283	264.735384	7.980122
5.664137	264.452857	7.985139
5.812364	264.723350	7.990157
5.508025	267.115457	7.995174
5.444113	266.330292	8.000192
5.359100	265.873440	8.005210
5.770361	265.601237	8.010227
5.555678	270.052626	8.015245
6.004681	260.948286	8.020262
5.575511	258.358177	8.025280
5.715957	261.372111	8.030298
5.602150	269.796494	8.035315
5.834773	263.632166	8.040333
5.951203	268.533744	8.045350
5.807429	270.026747	8.050368
5.863608	262.125901	8.055386
5.780262	265.171524	8.060403
5.667885	259.414342	8.065421
5.769495	263.835418	8.070438
5.779389	266.257490	8.075456
5.747638	257.972729	8.080474
6.061428	256.532345	8.085491
5.292552	263.843805	8.090509
5.861685	270.833342	8.095526
5.852915	276.189891	8.100544
5.851902	269.235165	8.105562
6.138066	279.679986	8.110579
6.041254	276.331268	8.115597
5.927016	269.810713	8.120614
5.624990	268.005489	8.125632
5.883163	259.874391	8.130650
6.049415	271.732659	8.135667
5.723928	264.509737	8.140685
5.948012	264.743175	8.145702
5.817144	264.990854	8.150720
6.097392	275.089475	8.155738
5.926170	265.466354	8.160755
5.503164	274.049326	8.165773
5.945393	269.947692	8.170790
6.188000	285.258949	8.175808
6.357194	274.784449	8.180826
5.974486	265.576085	8.185843
5.707125	264.084182	8.190861
5.876323	267.058929	8.195878
5.810427	281.348462	8.200896
5.876402	285.260725	8.205914
6.130554	284.744755	8.210931
6.170433	287.439857	8.215949
6.306030	282.849506	8.220966
5.866452	273.943465	8.225984
5.822970	269.680782	8.231002
6.170464	280.302236	8.236019
6.060985	287.119742	8.241037
5.980221	266.415778	8.246054
6.043118	276.696555	8.251072
5.787459	274.445480	8.256090
6.102912	279.505411	8.261107
6.191737	287.705760	8.266125
5.941202	284.605024	8.271142
6.049850	284.562963	8.276160
6.094699	285.010488	8.281178
6.237891	285.095584	8.286195
6.234574	276.768519	8.291213
5.731199	271.981029	8.296230
5.969068	278.394177	8.301248
5.988993	279.981606	8.306266
6.273043	282.051745	8.311283
5.980763	290.661706	8.316301
6.168332	283.598723	8.321318
5.916536	292.205537	8.326336
5.705941	288.909244	8.331354
6.002809	275.596896	8.336371
6.010228	281.045594	8.341389
5.886921	285.612141	8.346406
6.087996	281.017907	8.351424
6.090159	280.531704	8.356442
6.008774	292.687303	8.361459
5.932569	294.908202	8.366477
5.936125	284.800293	8.371494
6.305517	285.806323	8.376512
6.331104	285.467943	8.381530
6.189774	280.150738	8.386547
5.781687	286.023872	8.391565
6.219116	283.191541	8.396582
6.194087	295.644463	8.401600
6.062555	296.791598	8.406618
6.247067	292.853154	8.411635
5.967579	291.902748	8.416653
6.320292	288.026473	8.421670
5.935090	282.523188	8.426688
5.897450	288.581628	8.431706
6.260204	299.232273	8.436723
6.397833	314.503100	8.441741
6.587540	299.960946	8.446758
6.402794	291.321315	8.451776
5.941688	284.242570	8.456794
6.107116	276.813829	8.461811
6.222062	297.714642	8.466829
6.440364	299.684573	8.471846
6.402702	286.345411	8.476864
6.204045	286.729870	8.481882
6.376936	282.534476	8.486899
6.074229	285.936130	8.491917
6.402518	283.483689	8.496934
6.433812	282.626898	8.501952
5.945399	283.375189	8.506970
6.220865	294.067822	8.511987
6.394425	305.836618	8.517005
6.538360	302.942689	8.522022
6.344675	290.606060	8.527040
6.236765	285.312050	8.532058
6.304425	292.048333	8.537075
6.507891	304.036520	8.542093
6.302203	289.003703	8.547110
6.613345	288.800733	8.552128
6.227520	289.028152	8.557146
6.292978	281.157409	8.562163
6.248954	297.204385	8.567181
6.681110	303.211773	8.572199
6.273631	293.126833	8.577216
6.308494	290.688520	8.582234
6.738243	289.971650	8.587251
6.393978	294.241261	8.592269
6.460810	290.456831	8.597287
6.331855	280.255954	8.602304
6.064027	280.764785	8.607322
6.438396	288.052880	8.612339
6.593744	300.357808	8.617357
6.351919	295.217181	8.622375
6.343493	298.389993	8.627392
6.520159	306.298979	8.632410
6.523351	296.916913	8.637427
6.524933	298.873252	8.642445
6.451417	292.299014	8.647463
6.566417	283.827300	8.652480
6.377130	284.484839	8.657498
6.461828	285.557284	8.662515
6.380784	300.448759	8.667533
6.687058	300.795625	8.672551
6.338836	292.257181	8.677568
6.366749	296.882232	8.682586
6.748430	304.715119	8.687603
6.777543	299.888892	8.692621
6.373469	296.452319	8.697639
6.506581	294.266936	8.702656
6.190031	282.627901	8.707674
6.866460	297.205789	8.712691
6.549789	303.323456	8.717709
6.410118	297.677802	8.722727
6.592853	298.148039	8.727744
6.432832	292.612846	8.732762
6.725939	295.795511	8.737779
6.566022	297.101692	8.742797
6.454678	298.889431	8.747815
6.823743	293.287639	8.752832
6.681327	295.910145	8.757850
6.331502	297.413142	8.762867
6.325752	311.683868	8.767885
6.843801	306.125144	8.772903
6.974778	310.989757	8.777920
6.536283	311.449426	8.782938
6.799105	295.520040	8.787955
6.534506	297.473643	8.792973
6.807818	293.461416	8.797991
6.670178	288.667467	8.803008
6.322848	289.024584	8.808026
6.711602	283.138880	8.813043
6.490571	302.208104	8.818061
6.698373	298.474303	8.823079
6.793789	309.302269	8.828096
6.711721	296.973502	8.833114
6.953360	287.734186	8.838131
6.396546	296.890236	8.843149
6.723362	292.472070	8.848167
6.590697	287.554278	8.853184
6.738398	307.247711	8.858202
6.914095	297.655760	8.863219
6.613572	295.405356	8.868237
6.477344	286.291142	8.873255
6.821996	301.744306	8.878272
6.751119	310.613278	8.883290
7.048916	300.999159	8.888307
6.862171	296.358012	8.893325
6.993421	286.148174	8.898343
6.948661	283.586567	8.903360
6.902303	289.561163	8.908378
6.935926	287.252424	8.913395
6.872424	290.771461	8.918413
6.758922	292.177706	8.923431
6.720525	291.202385	8.928448
6.648388	284.861451	8.933466
6.723807	278.857285	8.938483
6.306566	286.587349	8.943501
6.540590	290.227310	8.948519
7.090970	297.128263	8.953536
6.675463	301.390034	8.958554
6.617930	293.825597	8.963571
6.974010	298.812940	8.968589
6.723464	305.986914	8.973607
6.951730	304.266369	8.978624
6.579593	314.715882	8.983642
6.797916	305.962997	8.988659
6.958442	308.554116	8.993677
7.291398	315.782402	8.998695
6.939699	299.027248	9.003712
6.795129	299.759872	9.008730
6.807984	308.439091	9.013747
6.691751	305.263795	9.018765
6.602945	310.471880	9.023783
6.675993	312.199355	9.028800
6.723707	315.675836	9.033818
6.812175	309.208907	9.038835
6.833567	314.699619	9.043853
6.327397	319.770728	9.048871
6.653632	312.881792	9.053888
6.964944	319.176229	9.058906
6.746992	307.092661	9.063923
6.867645	318.503651	9.068941
6.440738	319.075118	9.073959
7.006005	325.468865	9.078976
6.940456	335.646605	9.083994
7.160168	335.653519	9.089011
6.972072	333.073199	9.094029
6.946737	343.572868	9.099047
7.605531	340.658728	9.104064
7.244390	325.268252	9.109082
7.366108	328.569121	9.114099
7.122659	320.052218	9.119117
7.095382	321.833183	9.124135
7.102203	319.291940	9.129152
6.916229	316.954275	9.134170
6.804886	312.758950	9.139187
6.956502	311.593107	9.144205
7.127993	309.770955	9.149223
7.108179	307.521023	9.154240
6.625811	314.122058	9.159258
6.905577	311.727658	9.164275
7.152773	320.641780	9.169293
7.196867	326.444524	9.174311
7.287251	302.473041	9.179328
6.712324	313.462181	9.184346
7.334316	324.971833	9.189363
7.024993	319.598725	9.194381
7.244990	325.658088	9.199399
7.548419	311.189732	9.204416
7.266285	307.835150	9.209434
6.960705	309.501663	9.214451
7.029342	306.594212	9.219469
6.789435	311.503949	9.224487
7.113952	323.861444	9.229504
7.183128	322.011042	9.234522
7.141978	334.662150	9.239539
7.340728	334.934245	9.244557
7.081977	337.366598	9.249575
7.465954	325.870915	9.254592
7.136069	319.535387	9.259610
7.347502	325.845378	9.264627
6.960177	319.884845	9.269645
6.846548	327.952642	9.274663
7.316047	316.314268	9.279680
7.448021	334.779487	9.284698
7.445133	325.167991	9.289715
7.561434	328.192008	9.294733
7.218055	316.800111	9.299751
7.174561	308.715958	9.304768
6.813992	325.298211	9.309786
7.116630	328.646646	9.314803
7.458819	339.840130	9.319821
7.355234	331.023751	9.324839
7.260070	327.583254	9.329856
7.134911	346.959472	9.334874
7.538709	333.207578	9.339891
7.437690	333.144515	9.344909
7.224113	337.516858	9.349927
7.137142	337.984909	9.354944
7.679456	337.951061	9.359962
7.460039	336.486399	9.364979
7.334168	335.710877	9.369997
7.365769	334.667854	9.375015
7.595593	331.328227	9.380032
7.190315	325.809121	9.385050
7.290703	332.676015	9.390067
7.518072	337.235310	9.395085
7.468672	329.855773	9.400103
7.573045	319.779482	9.405120
7.485047	317.814704	9.410138
7.150319	321.805141	9.415155
7.078247	317.471164	9.420173
7.376911	333.467973	9.425191
7.461722	331.750828	9.430208
7.193344	334.639090	9.435226
7.026052	337.877667	9.440243
7.321758	333.085659	9.445261
7.250801	345.533145	9.450279
7.353731	349.452291	9.455296
7.581550	336.235850	9.460314
7.541717	334.929409	9.465331
7.638165	335.788601	9.470349
7.349992	341.308586	9.475367
7.441619	333.651484	9.480384
7.510897	340.785142	9.485402
7.439746	340.802631	9.490419
7.214902	333.314716	9.495437
7.144688	343.635191	9.500455
7.289553	337.386677	9.505472
7.240379	337.672127	9.510490
7.428198	353.610478	9.515507
7.853228	347.384607	9.520525
7.365808	351.480871	9.525543
7.829966	347.110732	9.530560
7.690779	341.562814	9.535578
7.303309	334.822858	9.540595
7.357542	339.147193	9.545613
7.567560	358.114652	9.550631
7.875306	354.239053	9.555648
7.661105	350.886509	9.560666
7.595477	353.317197	9.565683
7.736092	349.587535	9.570701
7.185343	341.055355	9.575719
7.428280	345.883613	9.580736
7.824277	351.577929	9.585754
7.682137	365.182005	9.590771
7.597936	361.178092	9.595789
7.581356	357.371923	9.600807
7.450692	348.452459	9.605824
7.579192	354.210514	9.610842
7.495562	358.890816	9.615859
7.871628	352.536875	9.620877
7.963061	354.668569	9.625895
7.670734	347.986374	9.630912
7.939231	361.725318	9.635930
7.442872	355.286316	9.640947
8.011076	361.367211	9.645965
7.864802	365.934198	9.650983
7.794759	359.248947	9.656000
7.987822	353.592493	9.661018
7.879871	345.603562	9.666035
7.832546	335.781241	9.671053
7.638535	338.194047	9.676071
7.517977	342.173233	9.681088
8.017474	348.946438	9.686106
7.479001	349.614167	9.691123
7.682787	344.514594	9.696141
7.765535	358.462326	9.701159
7.787562	360.974036	9.706176
7.818641	353.070747	9.711194
7.904255	356.159503	9.716211
7.981511	353.316971	9.721229
8.065343	361.038475	9.726247
7.911130	356.060906	9.731264
7.939443	355.400225	9.736282
7.752390	347.313162	9.741299
8.192697	341.725508	9.746317
7.680214	335.487828	9.751335
7.470975	342.936236	9.756352
7.904479	345.181917	9.761370
7.426939	359.213730	9.766387
7.793842	357.727202	9.771405
7.815382	360.570329	9.776423
7.948086	360.272071	9.781440
8.221371	356.531218	9.786458
7.900566	356.814782	9.791475
8.046585	355.094417	9.796493
8.207850	360.481319	9.801511
8.238701	354.742829	9.806528
7.618534	351.740655	9.811546
7.560709	356.082441	9.816563
8.103562	357.108802	9.821581
7.960315	365.020290	9.826599
8.142178	363.392167	9.831616
8.122789	349.396896	9.836634
7.779893	362.672486	9.841651
7.957732	352.856122	9.846669
7.726876	358.673284	9.851687
7.703469	355.919004	9.856704
8.135987	352.661417	9.861722
7.807545	357.752199	9.866739
8.299961	359.032553	9.871757
7.963214	361.079444	9.876775
8.246107	354.998771	9.881792
7.971616	345.757738	9.886810
7.818857	360.089259	9.891827
8.161540	359.830887	9.896845
8.221361	357.678998	9.901863
8.071878	364.818325	9.906880
8.257255	359.794193	9.911898
8.005166	367.700538	9.916915
8.309700	357.006113	9.921933
8.100432	358.313671	9.926951
8.069745	355.166070	9.931968
8.157833	341.769420	9.936986
8.022117	357.906463	9.942003
8.246377	358.218765	9.947021
8.163263	368.061606	9.952039
7.914502	358.630378	9.957056
8.114123	355.667813	9.962074
7.693492	372.735962	9.967091
8.227397	364.312590	9.972109
8.241264	363.064055	9.977127
8.020900	365.840710	9.982144
8.278248	362.783955	9.987162
8.121845	369.236433	9.992179
8.018634	357.961743	9.997197
7.960800	365.314007	10.002215
8.302116	379.751645	10.007232
8.381871	382.380595	10.012250
8.615106	387.175662	10.017267
8.380507	377.619149	10.022285
8.695784	365.307360	10.027303
8.129797	362.252570	10.032320
8.089890	363.656828	10.037338
8.229459	360.309159	10.042355
8.253064	360.520166	10.047373
8.237573	363.937073	10.052391
8.175707	358.414979	10.057408
8.454426	358.974408	10.062426
8.249241	371.556413	10.067443
8.491944	361.900349	10.072461
8.424650	360.825388	10.077479
8.418509	367.973955	10.082496
8.628790	351.809715	10.087514
8.478540	360.697381	10.092531
8.490526	361.711728	10.097549
8.337733	365.430865	10.102567
8.206584	364.529938	10.107584
8.358253	355.355085	10.112602
8.246192	368.187662	10.117619
8.299502	373.932185	10.122637
8.363506	360.851679	10.127655
8.144536	374.511903	10.132672
8.666075	374.588582	10.137690
8.319829	382.386524	10.142707
8.821023	378.076880	10.147725
8.529982	371.385009	10.152743
8.453322	368.960894	10.157760
8.434620	365.126653	10.162778
8.298170	369.057828	10.167795
8.370910	370.977851	10.172813
8.389365	378.283531	10.177831
8.560816	391.283410	10.182848
8.751143	385.545325	10.187866
8.907904	391.182233	10.192883
8.446065	369.748571	10.197901
8.607050	364.160221	10.202919
8.332185	357.159741	10.207936
8.615019	369.785676	10.212954
8.840192	377.245352	10.217971
8.517432	361.356590	10.222989
8.560671	372.072804	10.228007
8.306235	364.592640	10.233024
8.256036	374.190531	10.238042
8.701638	383.007525	10.243059
8.959791	371.720741	10.248077
8.842000	385.545092	10.253095
8.410728	379.884857	10.258112
8.593135	372.469210	10.263130
8.842878	381.846846	10.268147
9.004371	370.543556	10.273165
8.702049	366.545201	10.278183
8.317615	369.536741	10.283200
8.353007	369.458750	10.288218
8.627722	379.308997	10.293235
8.682401	378.041483	10.298253
9.071198	387.460584	10.303271
8.780520	387.089397	10.308288
8.948714	372.424308	10.313306
8.425187	371.395134	10.318323
8.824781	373.532497	10.323341
9.060563	375.370333	10.328359
8.740450	376.616259	10.333376
9.106726	360.579194	10.338394
8.428298	367.491626	10.343411
8.467079	365.333544	10.348429
8.701085	374.568466	10.353447
8.871401	386.634450	10.358464
9.283927	381.281471	10.363482
8.725444	373.469966	10.368499
8.363044	377.471035	10.373517
8.758295	371.202458	10.378535
8.912317	386.376125	10.383552
8.953333	379.963893	10.388570
8.552748	382.358378	10.393587
8.609033	387.493405	10.398605
8.808856	386.048666	10.403623
8.476938	394.885743	10.408640
8.510047	394.031820	10.413658
8.902955	395.867285	10.418675
8.949978	385.130889	10.423693
9.003296	388.723271	10.428711
8.821799	396.867934	10.433728
9.134048	394.458998	10.438746
9.297412	398.854714	10.443763
9.071431	397.482582	10.448781
8.898301	392.097715	10.453799
8.897699	405.045501	10.458816
9.357401	396.346504	10.463834
9.184355	394.852527	10.468851
9.024617	392.592814	10.473869
9.156247	398.075855	10.478887
8.825269	397.338576	10.483904
9.220645	397.658949	10.488922
8.861032	394.161789	10.493939
8.598720	391.536213	10.498957
8.965416	387.048702	10.503975
8.875927	391.269201	10.508992
8.813404	394.964822	10.514010
9.155550	395.997191	10.519027
9.209504	390.412874	10.524045
8.886935	392.725790	10.529063
8.965874	392.287587	10.534080
9.317265	389.358189	10.539098
9.265522	391.575292	10.544115
8.943081	397.690734	10.549133
9.265269	396.340546	10.554151
9.069979	388.062252	10.559168
9.448253	384.560654	10.564186
9.153520	383.969203	10.569203
9.071173	386.935801	10.574221
9.401059	397.749405	10.579239
8.667910	391.902649	10.584256
8.753340	395.360651	10.589274
9.164050	391.929737	10.594291
9.208642	389.044950	10.599309
9.473640	398.249814	10.604327
9.231936	392.007823	10.609344
9.235593	395.153525	10.614362
9.039405	393.158250	10.619379
8.909315	388.429367	10.624397
9.197948	393.089585	10.629415
9.114399	401.237933	10.634432
9.085470	397.137048	10.639450
9.292827	391.307952	10.644467
8.920895	393.862071	10.649485
9.312098	385.438818	10.654503
8.924738	389.794052	10.659520
8.901021	397.699566	10.664538
8.977774	409.111137	10.669555
9.195091	420.320958	10.674573
9.343438	410.528088	10.679591
8.846298	422.521301	10.684608
9.288214	414.787536	10.689626
9.375445	418.914258	10.694643
9.425575	418.414272	10.699661
9.595196	417.346599	10.704679
9.544614	418.096150	10.709696
9.664127	418.118665	10.714714
9.541753	410.131950	10.719731
9.410912	419.079736	10.724749
9.793763	402.367900	10.729767
9.647826	407.326145	10.734784
9.470463	405.921198	10.739802
9.345212	400.270110	10.744819
9.283259	407.313781	10.749837
9.497581	408.918289	10.754855
8.880572	419.459634	10.759872
9.146372	405.694457	10.764890
9.567027	409.721930	10.769907
9.323960	419.662283	10.774925
9.388588	414.947255	10.779943
9.732656	425.168562	10.784960
9.666178	410.924968	10.789978
9.385154	408.763027	10.794995
9.233254	412.617727	10.800013
9.300541	412.197116	10.805031
9.182748	416.627145	10.810048
9.307743	419.356349	10.815066
9.156862	414.122637	10.820083
9.189941	429.353039	10.825101
9.778433	434.174853	10.830119
9.540823	444.739189	10.835136
9.750667	448.676423	10.840154
9.748330	437.108279	10.845171
9.861973	433.275507	10.850189
9.974376	419.531047	10.855207
9.581482	417.863026	10.860224
9.682454	415.445959	10.865242
9.515942	411.991309	10.870259
9.323427	417.603716	10.875277
9.941130	422.755477	10.880295
9.632445	435.965838	10.885312
9.671151	429.471901	10.890330
10.157559	410.307775	10.895347
9.443657	417.661228	10.900365
9.472841	417.180281	10.905383
9.734596	431.589325	10.910400
10.178445	428.752817	10.915418
10.014905	423.413782	10.920435
9.668294	423.177528	10.925453
9.590977	419.289288	10.930471
9.804728	413.490746	10.935488
9.938559	423.971992	10.940506
9.834829	413.306386	10.945523
9.434256	417.168248	10.950541
9.862696	414.599216	10.955559
9.681885	419.660718	10.960576
9.670382	426.210572	10.965594
9.599415	428.850373	10.970611
9.640183	434.896655	10.975629
9.829189	435.435343	10.980647
9.540214	441.697061	10.985664
10.012077	438.376531	10.990682
10.075366	442.106219	10.995699
9.985732	440.633964	11.000717
9.930856	435.019243	11.005735
10.042535	450.922201	11.010752
10.105126	451.991787	11.015770
10.210987	437.872810	11.020787
10.108594	442.051151	11.025805
9.830176	432.539298	11.030823
10.174443	426.341754	11.035840
9.725541	427.522533	11.040858
9.717169	429.732888	11.045875
9.728566	444.745783	11.050893
10.375659	437.690083	11.055911
10.206250	437.467263	11.060928
10.089591	440.909403	11.065946
9.519211	423.986218	11.070963
9.952103	440.498685	11.075981
10.115394	436.282660	11.080999
10.110345	437.186060	11.086016
10.068375	442.929662	11.091034
10.351682	439.445995	11.096051
10.181955	445.840619	11.101069
10.110665	430.966628	11.106087
10.362990	444.370499	11.111104
9.903285	430.197581	11.116122
10.307206	427.316799	11.121139
9.632024	432.856044	11.126157
9.847516	427.634710	11.131175
10.019203	438.457191	11.136192
10.109284	431.330437	11.141210
10.149937	441.879847	11.146227
10.211989	442.318387	11.151245
10.204050	436.399727	11.156263
10.217458	434.144607	11.161280
10.220502	438.303375	11.166298
10.172947	438.553863	11.171315
10.109788	440.958933	11.176333
9.984013	437.636784	11.181351
10.341386	442.829084	11.186368
9.924522	437.185521	11.191386
10.319309	438.260186	11.196403
9.916841	442.280131	11.201421
10.051353	434.736223	11.206439
10.145388	437.646966	11.211456
10.041257	444.018754	11.216474
10.177259	438.194441	11.221491
10.118089	445.225070	11.226509
10.250718	450.206223	11.231527
10.648343	466.755762	11.236544
10.621683	458.116681	11.241562
10.807045	443.085961	11.246579
10.481981	435.856592	11.251597
10.279974	433.319447	11.256615
10.223851	425.069958	11.261632
10.192973	431.275709	11.266650
10.590439	430.838403	11.271667
10.612559	440.854238	11.276685
10.365479	432.968976	11.281703
9.944921	432.365558	11.286720
10.187638	440.630375	11.291738
10.870901	446.264217	11.296755
10.578567	445.356826	11.301773
10.499807	442.857291	11.306791
10.463660	436.741061	11.311808
10.085301	438.046551	11.316826
10.357371	440.800194	11.321843
10.842466	458.017725	11.326861
10.457202	457.749621	11.331879
10.723920	449.418300	11.336896
10.340934	452.497986	11.341914
10.807520	437.729582	11.346931
10.289108	441.628730	11.351949
10.538186	447.854012	11.356967
10.855688	458.871543	11.361984
10.220022	453.738544	11.367002
10.649131	457.095713	11.372019
10.450198	467.423678	11.377037
10.763715	463.338884	11.382055
10.734342	467.174519	11.387072
10.552856	464.826669	11.392090
10.673596	460.046090	11.397107
10.894864	471.261640	11.402125
10.634847	456.136159	11.407143
11.008604	440.523869	11.412160
10.606405	441.012602	11.417178
10.433389	439.029492	11.422195
10.344465	448.100148	11.427213
10.513461	454.905917	11.432231
11.160219	457.285660	11.437248
10.806410	469.944520	11.442266
10.877713	461.066134	11.447283
10.727338	445.418687	11.452301
10.403971	456.586488	11.457319
10.814820	462.925437	11.462336
10.842310	459.210209	11.467354
10.961459	459.535724	11.472371
10.726345	466.170898	11.477389
10.809137	457.388550	11.482407
11.044353	465.275868	11.487424
10.719719	468.081397	11.492442
11.147214	459.074974	11.497459
10.371086	457.353014	11.502477
10.430252	457.580575	11.507495
10.829638	457.149280	11.512512
10.700731	467.141309	11.517530
11.233610	458.651784	11.522547
10.816600	464.406451	11.527565
10.732748	460.768516	11.532583
11.292000	463.196596	11.537600
10.880564	464.210606	11.542618
10.706524	463.205904	11.547635
10.773863	461.403109	11.552653
10.661859	460.234122	11.557671
10.651459	460.305265	11.562688
10.459645	462.802948	11.567706
11.188064	454.822597	11.572723
10.908434	458.627769	11.577741
11.033819	463.572187	11.582759
10.786307	461.035811	11.587776
10.614079	476.061544	11.592794
11.168826	482.157199	11.597811
11.158881	483.881835	11.602829
11.175002	487.950220	11.607847
11.486111	480.779566	11.612864
11.163945	476.724318	11.617882
11.046831	464.839527	11.622899
11.065734	460.567086	11.627917
11.013202	464.788160	11.632935
11.421125	473.563731	11.637952
11.188714	477.569829	11.642970
11.084182	462.738855	11.647987
11.094028	462.481814	11.653005
10.870381	462.418909	11.658023
11.355886	472.195364	11.663040
11.168572	483.212617	11.668058
11.186017	487.410178	11.673075
11.073342	486.301251	11.678093
11.041691	488.284875	11.683111
11.656550	487.810564	11.688128
11.009690	487.968179	11.693146
11.056362	485.625826	11.698163
11.110345	485.112616	11.703181
11.108333	488.915594	11.708199
11.597106	483.399242	11.713216
11.467726	492.413106	11.718234
11.472006	480.856526	11.723251
11.147156	479.177904	11.728269
11.325828	491.842233	11.733287
11.183003	486.301147	11.738304
11.081311	488.649110	11.743322
11.176486	488.855286	11.748339
11.476057	479.335465	11.753357
11.186873	488.576170	11.758375
11.354309	491.238819	11.763392
11.188013	492.265154	11.768410
11.243229	493.982801	11.773427
11.507544	493.664049	11.778445
11.105756	490.122945	11.783463
11.094349	486.868183	11.788480
11.215405	490.001935	11.793498
11.513417	500.050584	11.798515
11.343374	498.956899	11.803533
11.840187	508.551742	11.808551
11.416070	499.248722	11.813568
11.309768	497.785369	11.818586
11.725241	504.707409	11.823603
11.718131	502.897267	11.828621
11.431901	501.528196	11.833639
11.509236	503.873532	11.838656
11.420395	504.872029	11.843674
11.786404	507.964490	11.848691
11.876417	506.530528	11.853709
11.487121	498.727337	11.858727
11.399128	494.184366	11.863744
11.851034	507.926424	11.868762
11.735824	500.137360	11.873779
11.423179	494.771027	11.878797
11.604582	508.810810	11.883815
11.832236	516.229135	11.888832
11.574630	511.232908	11.893850
11.751891	519.242877	11.898867
11.671531	524.001605	11.903885
11.485392	519.208833	11.908903
11.773377	513.849960	11.913920
11.629528	516.766197	11.918938
11.654143	517.519823	11.923955
11.698338	518.636457	11.928973
11.636388	513.707591	11.933991
11.714499	516.210591	11.939008
11.850768	525.877357	11.944026
11.862706	515.026431	11.949043
11.603429	513.586894	11.954061
11.758427	528.309270	11.959079
12.076476	519.436617	11.964096
11.841228	510.741629	11.969114
11.963402	522.108333	11.974131
11.968579	513.669386	11.979149
11.647154	522.018921	11.984167
12.149620	518.813527	11.989184
11.628181	522.350262	11.994202
11.794241	519.648505	11.999219
11.877490	514.652853	12.004237
11.440334	514.765195	12.009255
12.035271	517.392845	12.014272
12.033531	521.293613	12.019290
11.787435	518.700207	12.024307
11.677314	525.729334	12.029325
11.556982	519.638805	12.034343
11.706445	518.725737	12.039360
11.770111	533.026856	12.044378
12.391437	535.432659	12.049395
12.380558	538.811014	12.054413
12.225137	531.116556	12.059431
12.224604	520.425351	12.064448
11.938747	525.146649	12.069466
11.932365	520.385848	12.074483
12.050405	508.615886	12.079501
11.975244	523.699127	12.084519
12.062778	530.214665	12.089536
11.786926	527.316635	12.094554
12.115652	542.166601	12.099571
12.143343	532.496587	12.104589
12.053395	536.562564	12.109607
12.343247	529.180615	12.114624
12.516744	536.175054	12.119642
12.267770	534.636085	12.124659
12.304676	524.481824	12.129677
11.573339	522.680302	12.134695
12.086273	524.175215	12.139712
11.984092	534.977283	12.144730
11.879676	535.081998	12.149747
12.033616	537.178736	12.154765
12.148808	539.865306	12.159783
12.325506	530.415078	12.164800
12.243189	539.942323	12.169818
12.206170	531.083924	12.174835
12.403445	528.547711	12.179853
12.005253	537.679187	12.184871
12.380940	525.048627	12.189888
12.277523	528.709619	12.194906
12.373799	538.890681	12.199923
12.511323	524.684658	12.204941
12.099797	532.069970	12.209959
12.593678	531.510357	12.214976
12.513693	523.343430	12.219994
12.292632	529.641939	12.225011
12.457357	528.328880	12.230029
12.307981	535.676534	12.235047
12.269773	533.467305	12.240064
12.706167	549.824701	12.245082
12.818923	539.863739	12.250099
12.677385	530.892230	12.255117
12.295132	535.063676	12.260135
12.481809	534.709677	12.265152
12.224966	523.701787	12.270170
12.623804	549.156496	12.275187
12.681770	538.752805	12.280205
12.547237	551.450163	12.285223
12.664073	545.505728	12.290240
12.365844	540.146605	12.295258
12.676453	553.847584	12.300275
12.477620	556.065519	12.305293
12.371657	568.878357	12.310311
12.751158	565.711033	12.315328
12.845099	567.318521	12.320346
12.778550	566.887188	12.325363
13.184617	556.309373	12.330381
12.321400	541.391340	12.335399
12.640449	548.464103	12.340416
12.573750	551.538741	12.345434
12.684150	558.467277	12.350451
12.896709	555.060872	12.355469
12.642567	556.807757	12.360487
12.723024	558.250092	12.365504
12.800156	562.924351	12.370522
12.861420	555.110942	12.375539
12.855685	557.816343	12.380557
12.783742	562.617949	12.385575
12.417674	562.403656	12.390592
12.793069	558.905628	12.395610
12.488569	560.104956	12.400627
13.050459	550.001480	12.405645
12.858141	567.176272	12.410663
13.007012	563.391634	12.415680
12.804068	565.073746	12.420698
12.595105	559.994195	12.425715
12.942263	547.169255	12.430733
12.871194	562.614793	12.435751
12.622962	567.068323	12.440768
12.886203	563.133340	12.445786
12.462381	562.637718	12.450803
12.835772	560.796728	12.455821
12.762540	562.622739	12.460839
13.062380	566.883644	12.465856
13.272003	566.144235	12.470874
13.166512	562.629565	12.475891
13.273348	551.050660	12.480909
13.046526	565.024664	12.485927
12.663221	560.401429	12.490944
13.400901	557.629600	12.495962
12.864206	550.654032	12.500979
12.648935	563.531219	12.505997
12.989830	567.934049	12.511015
13.195625	573.995707	12.516032
13.180179	582.234517	12.521050
13.253086	584.037777	12.526067
13.660138	577.044642	12.531085
13.224178	572.622097	12.536103
12.789424	567.710238	12.541120
13.330441	569.017753	12.546138
13.357723	574.693813	12.551155
13.395915	563.889260	12.556173
13.154593	559.862430	12.561191
12.831532	561.866188	12.566208
13.253722	563.905386	12.571226
13.041178	582.437124	12.576243
13.841778	569.831889	12.581261
13.317948	581.346547	12.586279
13.559608	574.429655	12.591296
13.400586	563.466467	12.596314
13.176376	558.543919	12.601331
13.055143	555.962623	12.606349
13.389456	573.743362	12.611367
13.138279	592.631405	12.616384
13.239934	580.945995	12.621402
13.458084	582.594103	12.626419
13.448801	588.121232	12.631437
13.613843	589.594580	12.636455
13.205063	593.192681	12.641472
13.859022	590.588511	12.646490
13.363162	584.190370	12.651507
13.136748	580.470471	12.656525
13.369645	588.301403	12.661543
13.426595	584.632053	12.666560
13.520181	581.821655	12.671578
13.322990	583.319844	12.676595
13.766315	581.117684	12.681613
13.668848	592.105237	12.686631
13.531540	586.850427	12.691648
13.773133	586.049238	12.696666
13.993823	594.582633	12.701683
13.600252	582.074960	12.706701
13.768400	592.503627	12.711719
13.771477	591.471341	12.716736
13.879889	581.653038	12.721754
13.693612	583.540832	12.726771
13.779397	588.428336	12.731789
13.552170	592.102306	12.736807
13.335110	594.670208	12.741824
13.810880	582.910770	12.746842
13.746777	593.823704	12.751859
13.450698	586.510869	12.756877
13.375499	577.955024	12.761895
13.699818	578.980712	12.766912
13.815247	582.475103	12.771930
13.717621	588.438848	12.776947
13.662135	574.852946	12.781965
13.905985	587.911122	12.786983
13.471094	589.894427	12.792000
13.860363	588.988197	12.797018
13.371661	582.800373	12.802035
13.811203	586.884904	12.807053
13.742206	587.075619	12.812071
13.938973	586.199362	12.817088
13.958006	582.523294	12.822106
13.963582	591.872787	12.827123
13.933852	579.545142	12.832141
13.911717	583.004150	12.837159
13.489194	583.963090	12.842176
14.226318	597.263194	12.847194
13.970579	612.027501	12.852211
13.830661	599.814824	12.857229
13.663417	596.322383	12.862247
14.088014	606.370318	12.867264
14.115760	602.572973	12.872282
13.996493	606.952788	12.877299
14.019586	593.020136	12.882317
14.328271	605.872579	12.887335
14.173009	603.839350	12.892352
14.172681	595.514827	12.897370
13.979514	605.841974	12.902387
14.053845	599.882049	12.907405
13.867073	603.186820	12.912423
13.946063	606.068377	12.917440
14.026572	602.707768	12.922458
14.231569	609.940319	12.927475
14.126132	608.666162	12.932493
14.319345	605.499436	12.937511
14.165339	614.198472	12.942528
14.118525	610.614698	12.947546
13.833611	610.024866	12.952563
13.903387	602.279536	12.957581
14.012193	611.117526	12.962599
14.540988	602.480252	12.967616
14.435756	606.349817	12.972634
14.443585	611.407249	12.977651
14.548234	601.213995	12.982669
14.605539	598.756367	12.987687
14.285313	598.074208	12.992704
14.664608	596.396390	12.997722
14.358063	597.835871	13.002739
14.193051	605.047137	13.007757
14.413649	601.159809	13.012775
13.812150	609.919049	13.017792
14.247116	605.638596	13.022810
14.360697	625.006347	13.027827
14.657874	626.055198	13.032845
14.552594	629.593430	13.037863
14.634155	637.160779	13.042880
14.870429	622.431237	13.047898
14.584525	615.060004	13.052915
14.313240	616.907390	13.057933
14.233500	610.384494	13.062951
14.193339	617.421698	13.067968
14.308823	621.875415	13.072986
14.811203	628.897577	13.078003
14.469623	620.291672	13.083021
14.820636	630.313208	13.088039
14.470553	637.004214	13.093056
14.380814	631.252854	13.098074
14.540967	638.019046	13.103091
14.499117	632.411702	13.108109
14.784254	631.048332	13.113127
14.510084	628.623375	13.118144
15.070608	622.972737	13.123162
14.624397	626.866995	13.128179
14.467856	629.741048	13.133197
14.812824	629.207773	13.138215
14.370953	629.977231	13.143232
14.652174	627.472114	13.148250
14.979191	632.079084	13.153267
14.729282	623.430503	13.158285
14.673542	622.104428	13.163303
14.495909	638.532261	13.168320
14.950923	636.031641	13.173338
15.169190	634.886956	13.178355
14.563797	641.387350	13.183373
14.957607	636.744082	13.188391
15.000943	643.638914	13.193408
15.056549	638.811626	13.198426
15.109804	635.483656	13.203443
14.892536	631.841213	13.208461
14.827294	617.471033	13.213479
14.837981	631.127254	13.218496
15.094539	644.196116	13.223514
14.966689	645.232251	13.228531
14.898164	649.178158	13.233549
15.486392	647.941159	13.238567
14.919667	657.859456	13.243584
15.095144	649.573804	13.248602
15.356808	655.421673	13.253619
14.830277	636.440261	13.258637
15.435646	645.784756	13.263655
15.089329	643.232181	13.268672
15.212957	645.071730	13.273690
15.063516	648.058284	13.278707
14.937312	653.493189	13.283725
15.164961	648.538130	13.288743
15.263807	651.659591	13.293760
15.085779	652.428995	13.298778
15.066367	653.858486	13.303795
15.266671	660.653149	13.308813
15.215742	653.548260	13.313831
15.012468	656.312832	13.318848
14.873129	647.214695	13.323866
15.271587	646.521619	13.328883
15.167083	658.333942	13.333901
15.374699	654.136210	13.338919
15.327382	658.394386	13.343936
15.223961	650.309942	13.348954
15.173862	652.867635	13.353971
15.054322	666.979644	13.358989
15.424634	651.437132	13.364007
15.014596	672.713603	13.369024
15.624311	675.503072	13.374042
15.462981	675.989020	13.379059
15.614730	686.959919	13.384077
15.753558	671.005323	13.389095
15.344549	674.410978	13.394112
15.942220	667.751034	13.399130
15.785000	667.065582	13.404147
15.702996	668.059868	13.409165
15.591008	646.344191	13.414183
15.402264	659.359324	13.419200
15.356233	645.235430	13.424218
15.275305	651.556343	13.429235
15.499574	668.316090	13.434253
15.707659	675.358846	13.439271
15.924454	677.158647	13.444288
15.562469	667.697548	13.449306
15.474059	670.822921	13.454323
15.652838	680.931260	13.459341
15.760901	667.969896	13.464359
15.755540	678.684395	13.469376
15.852240	675.630509	13.474394
15.919730	671.176890	13.479411
15.894587	672.105521	13.484429
15.826245	665.643944	13.489447
15.578580	659.342828	13.494464
15.608575	670.701889	13.499482
15.904081	669.968039	13.504499
15.694652	671.796332	13.509517
16.270137	679.599210	13.514535
15.714297	674.579946	13.519552
15.342575	666.436286	13.524570
15.650423	675.625155	13.529587
15.703418	676.235519	13.534605
16.002184	673.039723	13.539623
16.122529	677.173972	13.544640
15.894090	665.107572	13.549658
16.289142	668.239719	13.554675
15.746902	675.329873	13.559693
15.880425	662.295124	13.564711
15.542174	674.585647	13.569728
15.622058	673.544554	13.574746
15.530219	673.700959	13.579763
15.753637	688.958750	13.584781
16.478511	687.252364	13.589799
16.509081	696.607488	13.594816
16.324930	685.477730	13.599834
15.968382	679.029464	13.604851
16.088289	665.880072	13.609869
15.914839	677.359172	13.614887
16.335288	689.730387	13.619904
16.264634	683.408014	13.624922
16.311587	692.896280	13.629939
16.172223	696.449298	13.634957
16.256315	687.205904	13.639975
16.130718	703.603606	13.644992
16.227145	701.950886	13.650010
16.419816	696.666757	13.655027
16.208071	698.425989	13.660045
16.453521	693.976213	13.665063
16.573329	693.844054	13.670080
16.277747	702.618823	13.675098
16.758189	692.852984	13.680115
16.071693	689.570754	13.685133
16.247516	683.374101	13.690151
16.334163	692.521684	13.695168
16.243964	706.487149	13.700186
16.537150	697.362668	13.705203
16.324688	706.537893	13.710221
16.457517	700.871774	13.715239
16.172670	704.841907	13.720256
16.265784	704.259483	13.725274
16.603873	698.690790	13.730291
16.147908	715.250389	13.735309
15.919967	696.203490	13.740327
16.188905	706.733292	13.745344
16.378211	722.280436	13.750362
16.861141	722.707100	13.755379
16.716408	732.512401	13.760397
16.922662	725.272770	13.765415
16.774097	717.103809	13.770432
16.725237	710.134271	13.775450
16.749956	710.253594	13.780467
16.399459	706.227950	13.785485
16.790474	704.406292	13.790503
17.009771	713.167171	13.795520
16.657973	704.266180	13.800538
16.829852	695.488778	13.805555
16.563596	705.644332	13.810573
16.584604	703.145006	13.815591
16.582950	721.615653	13.820608
16.664912	734.364637	13.825626
17.078237	724.028583	13.830643
16.872459	724.104901	13.835661
16.949835	727.867168	13.840679
17.160256	728.746503	13.845696
16.910638	729.337714	13.850714
17.324048	722.037430	13.855731
16.877602	718.913473	13.860749
16.862165	704.062115	13.865767
17.071596	705.209836	13.870784
16.710099	724.680065	13.875802
16.975329	708.873007	13.880819
16.893536	723.544053	13.885837
17.129921	723.980703	13.890855
16.888317	721.364477	13.895872
16.993061	716.750417	13.900890
17.195067	724.630399	13.905907
16.930395	727.985190	13.910925
17.231018	728.557000	13.915943
16.804698	727.269681	13.920960
16.962357	724.288344	13.925978
17.024278	713.454760	13.930995
16.994489	720.042282	13.936013
17.013080	720.241451	13.941031
17.205360	730.268824	13.946048
17.044818	725.330005	13.951066
17.514466	722.842872	13.956083
17.392663	723.745531	13.961101
17.507306	724.545107	13.966119
17.399144	721.665116	13.971136
17.291178	723.736384	13.976154
17.507030	713.752963	13.981171
17.362481	728.957630	13.986189
17.346423	716.201742	13.991207
16.708254	726.500417	13.996224
17.254230	728.592942	14.001242
17.147492	719.022649	14.006259
17.052982	742.036200	14.011277
17.229871	746.313136	14.016295
17.724200	746.592864	14.021312
17.668343	757.460435	14.026330
17.967092	745.974596	14.031347
17.812998	756.980534	14.036365
17.849167	736.977316	14.041383
17.747598	728.390792	14.046400
17.558841	725.188844	14.051418
17.569607	726.509505	14.056435
17.608801	732.931662	14.061453
17.334551	728.521769	14.066471
17.458154	721.869345	14.071488
16.933499	736.082352	14.076506
17.638495	744.231156	14.081523
17.629649	752.090332	14.086541
17.811305	747.688344	14.091559
17.598523	749.381472	14.096576
17.567692	753.567678	14.101594
17.587920	757.114795	14.106611
17.794685	755.691036	14.111629
17.732872	750.484381	14.116647
17.805817	753.281699	14.121664
17.550823	758.430585	14.126682
17.667239	753.331875	14.131699
17.755527	747.448621	14.136717
17.805178	757.097442	14.141735
17.882561	754.223269	14.146752
17.769671	760.587066	14.151770
17.799018	758.288399	14.156787
17.948392	760.767715	14.161805
17.747551	762.291733	14.166823
18.005103	765.262275	14.171840
18.081902	775.733674	14.176858
18.196112	766.930504	14.181875
17.611800	764.793650	14.186893
18.043971	778.725177	14.191911
18.223750	768.463327	14.196928
17.581307	768.503494	14.201946
18.268827	776.784418	14.206963
17.898088	776.706545	14.211981
18.071446	772.236417	14.216999
18.176355	768.149321	14.222016
18.060980	772.645331	14.227034
17.874603	772.374656	14.232051
18.298311	773.750944	14.237069
18.072197	766.641729	14.242087
18.148198	768.242561	14.247104
18.210830	769.447856	14.252122
17.989209	770.230363	14.257139
18.222714	773.012152	14.262157
18.341417	775.518336	14.267175
18.508195	768.827615	14.272192
18.346737	777.256501	14.277210
18.085720	760.480481	14.282227
18.504644	770.355828	14.287245
18.390077	771.314166	14.292263
18.360543	766.067768	14.297280
18.148626	772.011500	14.302298
18.260658	788.501666	14.307315
18.468367	792.669675	14.312333
18.722739	793.242378	14.317351
18.857225	793.881082	14.322368
19.099097	785.058026	14.327386
18.672580	768.345635	14.332403
18.686376	775.570155	14.337421
18.632125	767.203455	14.342439
18.684194	766.889344	14.347456
18.480959	761.878269	14.352474
18.757541	761.399818	14.357491
18.645253	773.181872	14.362509
18.611726	776.349210	14.367527
18.628361	764.863103	14.372544
18.111734	772.201764	14.377562
18.406077	775.510551	14.382579
18.954474	790.291811	14.387597
18.514084	807.095215	14.392615
18.673219	794.113185	14.397632
18.707800	802.069760	14.402650
18.676276	801.872802	14.407667
18.805255	799.422921	14.412685
18.679149	801.026822	14.417703
18.891997	800.473090	14.422720
18.683473	801.124175	14.427738
18.747456	796.636357	14.432755
18.734002	798.756034	14.437773
18.409798	801.103969	14.442791
18.613593	796.862618	14.447808
18.638466	815.688983	14.452826
19.148085	816.588008	14.457843
19.110195	818.014079	14.462861
18.884437	824.931943	14.467879
18.987596	823.063576	14.472896
19.002756	828.201976	14.477914
19.475785	817.250674	14.482931
19.633257	813.152229	14.487949
19.144141	810.754402	14.492967
19.322526	789.397272	14.497984
18.945343	797.503159	14.503002
19.114847	784.292310	14.508019
19.149774	785.789089	14.513037
18.598004	792.909174	14.518055
18.757092	798.608964	14.523072
18.787475	818.592620	14.528090
19.552152	812.932227	14.533107
19.361589	810.134477	14.538125
18.898603	821.068630	14.543143
19.404725	812.725112	14.548160
19.229354	812.872433	14.553178
19.702745	802.908822	14.558195
19.484125	807.086410	14.563213
19.136262	814.875324	14.568231
19.354416	804.777888	14.573248
19.311213	814.693654	14.578266
19.141209	806.029387	14.583283
19.305541	804.874155	14.588301
19.384165	814.900337	14.593319
19.888054	821.067143	14.598336
19.212017	817.568672	14.603354
19.296675	825.356519	14.608371
20.014720	833.487554	14.613389
19.895372	832.256571	14.618407
19.697517	815.199274	14.623424
19.394197	817.862686	14.628442
19.424315	827.053852	14.633459
19.510357	833.784322	14.638477
19.697393	837.639989	14.643495
20.155170	825.791677	14.648512
20.088716	834.565550	14.653530
19.808750	817.438986	14.658547
19.737195	810.564458	14.663565
19.865668	813.403631	14.668583
19.676936	824.888361	14.673600
19.832968	809.783006	14.678618
19.837415	817.545469	14.683635
19.806061	817.007667	14.688653
19.751370	809.947482	14.693671
19.853740	825.467227	14.698688
19.919245	829.259766	14.703706
19.911369	839.450904	14.708723
20.237602	833.464304	14.713741
20.212376	829.858191	14.718759
20.070928	817.490972	14.723776
20.071765	812.605895	14.728794
19.439722	816.402898	14.733811
19.986249	820.827422	14.738829
20.098707	839.886322	14.743847
20.346159	825.460978	14.748864
20.256605	837.065970	14.753882
20.450859	835.887143	14.758899
20.120866	826.518805	14.763917
19.896892	827.304837	14.768935
20.320509	828.015286	14.773952
20.562826	830.057275	14.778970
20.077803	827.374794	14.783987
20.159570	817.443748	14.789005
20.078772	823.073601	14.794023
20.187075	826.941524	14.799040
20.462922	835.201367	14.804058
19.926719	843.439328	14.809075
20.363813	832.793406	14.814093
20.331101	842.877963	14.819111
19.997154	839.067456	14.824128
20.019933	842.428005	14.829146
20.228450	850.111374	14.834163
20.390448	833.755404	14.839181
20.104388	836.722237	14.844199
20.194463	836.452699	14.849216
20.136236	836.465020	14.854234
20.353581	848.284160	14.859251
20.824410	849.432217	14.864269
20.880962	858.739201	14.869287
20.816073	846.009757	14.874304
20.678406	840.180587	14.879322
20.655045	831.348313	14.884339
20.997768	828.704208	14.889357
20.343005	834.991457	14.894375
20.657500	834.109481	14.899392
20.631441	833.876959	14.904410
20.241950	830.488502	14.909427
20.984402	845.788689	14.914445
20.725705	855.554997	14.919463
21.016077	858.482577	14.924480
20.998233	842.675294	14.929498
20.726165	836.027629	14.934515
20.642556	838.091963	14.939533
20.898770	850.154355	14.944551
21.111193	855.795367	14.949568
20.918583	850.252452	14.954586
20.891750	848.577885	14.959603
20.995338	849.271894	14.964621
20.984568	849.226334	14.969639
20.918764	846.017844	14.974656
21.203611	850.808157	14.979674
21.085309	862.225143	14.984691
21.304748	842.938022	14.989709
21.101159	836.065107	14.994727
21.091009	831.361611	14.999744
21.195260	837.779988	15.004762
21.136596	845.716387	15.009779
21.063954	836.740309	15.014797
20.690576	847.057784	15.019815
21.050360	849.387591	15.024832
21.359427	854.663271	15.029850
21.280615	853.968759	15.034867
21.301083	853.618543	15.039885
21.234512	859.208323	15.044903
21.457701	856.993069	15.049920
21.614879	851.559789	15.054938
21.439315	854.225406	15.059955
21.857605	834.620163	15.064973
20.953274	840.750617	15.069991
20.873392	837.496985	15.075008
21.211164	838.773052	15.080026
21.238546	857.068909	15.085043
21.140174	862.379627	15.090061
21.469199	858.077740	15.095079
21.562046	857.179781	15.100096
21.718845	850.796689	15.105114
21.054870	860.550363	15.110131
21.334258	849.979476	15.115149
21.151007	859.046093	15.120167
21.321322	851.269223	15.125184
21.299867	857.426319	15.130202
21.342706	877.067284	15.135219
21.826268	869.632944	15.140237
21.700785	878.744224	15.145255
21.880912	871.641143	15.150272
21.788719	872.498174	15.155290
21.754244	880.339307	15.160307
21.768127	870.939495	15.165325
22.085952	872.587890	15.170343
21.955177	876.048091	15.175360
22.217338	867.673104	15.180378
21.817170	859.779931	15.185395
21.960784	851.353983	15.190413
21.565583	858.736887	15.195431
21.858751	865.902168	15.200448
21.896663	871.683962	15.205466
22.032537	872.114175	15.210483
22.202192	873.776172	15.215501
21.908884	878.628108	15.220519
22.155292	868.857587	15.225536
22.197246	859.292469	15.230554
22.001611	859.370364	15.235571
21.919553	851.493935	15.240589
21.952663	869.015762	15.245607
21.929948	865.727978	15.250624
22.482745	868.737774	15.255642
22.002655	875.193496	15.260659
22.175070	867.062851	15.265677
22.345769	883.515569	15.270695
22.359573	868.934069	15.275712
22.531573	867.402108	15.280730
22.187327	869.229322	15.285747
22.174236	864.425292	15.290765
22.429711	874.124180	15.295783
21.841822	863.732496	15.300800
21.954051	865.091017	15.305818
22.122583	869.000064	15.310835
22.079014	868.536744	15.315853
22.144475	876.049898	15.320871
22.288743	871.016245	15.325888
22.256160	876.354592	15.330906
22.502211	882.681481	15.335923
22.662235	885.020304	15.340941
22.529680	887.979024	15.345959
22.299618	894.310620	15.350976
22.976667	885.325087	15.355994
22.331108	896.906236	15.361011
22.674896	892.352740	15.366029
23.082095	898.137005	15.371047
22.926938	891.606813	15.376064
22.529374	872.734454	15.381082
22.492471	885.429472	15.386099
22.555435	890.674054	15.391117
22.580593	887.568156	15.396135
22.317555	892.125056	15.401152
22.135271	893.488409	15.406170
22.259020	897.230869	15.411187
22.616945	899.226465	15.416205
22.923424	903.060394	15.421223
22.896303	912.642359	15.426240
23.122723	911.660486	15.431258
23.190716	908.983406	15.436275
22.927659	900.759605	15.441293
22.846075	899.197698	15.446311
22.933846	906.530671	15.451328
23.095499	909.030186	15.456346
22.895895	911.062096	15.461363
23.018525	911.702650	15.466381
23.408490	910.938305	15.471399
23.140741	922.138762	15.476416
23.382638	910.071547	15.481434
23.084807	916.486284	15.486451
23.264894	908.824630	15.491469
23.408358	900.698477	15.496487
22.826271	907.539312	15.501504
23.426777	897.817782	15.506522
23.257036	915.753081	15.511539
23.365760	916.004490	15.516557
23.786285	907.961426	15.521575
22.921243	901.084176	15.526592
23.450912	900.575784	15.531610
23.351657	912.778769	15.536627
23.104392	913.562119	15.541645
23.392777	908.291427	15.546663
23.171707	923.984689	15.551680
23.308890	916.885121	15.556698
23.504592	920.294498	15.561715
23.375736	920.128472	15.566733
23.789391	909.372546	15.571751
23.462853	918.079659	15.576768
23.794210	912.325759	15.581786
23.449652	917.763184	15.586803
23.692211	924.668131	15.591821
23.682972	909.597890	15.596839
23.437335	919.516831	15.601856
24.054650	911.004479	15.606874
23.678384	912.985002	15.611891
23.825302	905.644086	15.616909
23.911187	906.706918	15.621927
22.922558	904.942258	15.626944
23.363478	910.585581	15.631962
23.132881	913.499611	15.636979
23.846222	925.086947	15.641997
24.156228	928.065129	15.647015
24.188665	933.901443	15.652032
24.525301	932.334376	15.657050
23.973940	922.369307	15.662067
23.605106	913.117421	15.667085
23.881091	917.479952	15.672103
23.925424	939.263496	15.677120
23.927051	930.446216	15.682138
23.984233	941.274209	15.687155
24.030541	935.820298	15.692173
24.323838	932.691578	15.697191
24.093741	941.655080	15.702208
24.345399	944.036447	15.707226
24.298983	939.439553	15.712243
24.276469	944.293526	15.717261
24.472470	940.056511	15.722279
24.346070	936.257849	15.727296
24.304096	942.859973	15.732314
24.410791	937.983626	15.737331
24.225341	936.914403	15.742349
24.148140	929.791404	15.747367
24.239467	942.832564	15.752384
24.486126	933.636313	15.757402
24.565397	933.614603	15.762419
24.026066	939.113916	15.767437
24.761292	931.078647	15.772455
24.634278	939.189828	15.777472
24.770436	942.046760	15.782490
24.467574	932.456396	15.787507
24.368916	936.413370	15.792525
24.455308	935.822518	15.797543
24.461161	930.305481	15.802560
24.402427	933.678738	15.807578
24.576347	936.002782	15.812595
24.533807	939.676470	15.817613
24.476821	939.552901	15.822631
24.528539	939.301956	15.827648
24.955063	946.184580	15.832666
24.805114	954.229913	15.837683
24.743948	948.366706	15.842701
25.011152	956.407050	15.847719
24.916816	955.137451	15.852736
25.060533	940.526197	15.857754
24.937680	931.769323	15.862771
24.644474	934.699415	15.867789
25.146122	934.693992	15.872807
25.130247	952.763158	15.877824
24.996712	951.909909	15.882842
24.934156	946.261509	15.887859
24.855122	949.855677	15.892877
25.078564	945.005331	15.897895
25.086249	951.634439	15.902912
24.903519	946.405529	15.907930
25.113885	951.254802	15.912947
25.090092	952.899590	15.917965
25.513356	955.194281	15.922983
25.061885	967.852921	15.928000
25.136554	955.243679	15.933018
25.268444	947.195045	15.938035
24.950317	952.536848	15.943053
25.280025	948.802867	15.948071
24.933032	960.599497	15.953088
25.281795	952.513938	15.958106
25.055414	957.459614	15.963123
24.529605	962.404575	15.968141
25.504054	973.304363	15.973159
25.342503	977.848639	15.978176
25.594326	982.041383	15.983194
25.649799	983.894734	15.988211
25.667328	981.518985	15.993229
25.656692	976.077082	15.998247
25.450260	987.700370	16.003264
25.560078	978.288721	16.008282
25.533454	973.417342	16.013299
25.618384	975.111475	16.018317
26.139046	977.248997	16.023335
25.558554	975.114678	16.028352
25.745170	975.975641	16.033370
25.825961	975.906358	16.038387
25.738436	983.875714	16.043405
25.866429	977.639070	16.048423
25.748032	978.556990	16.053440
25.655356	974.181880	16.058458
25.732825	971.569586	16.063475
25.552153	971.837652	16.068493
25.584735	971.403497	16.073511
25.836122	990.996339	16.078528
26.172040	987.879908	16.083546
26.222411	993.741852	16.088563
26.286337	996.423850	16.093581
26.097305	980.510556	16.098599
26.124975	985.839555	16.103616
26.299415	978.794120	16.108634
26.087361	967.261439	16.113651
26.257762	972.139030	16.118669
26.189143	967.933742	16.123687
26.038367	980.409877	16.128704
26.429031	990.864093	16.133722
26.552257	992.239846	16.138739
26.109395	989.812702	16.143757
26.583222	988.836485	16.148775
26.208106	982.097515	16.153792
26.495430	982.377920	16.158810
26.443184	981.745538	16.163827
26.275212	984.387902	16.168845
26.472347	989.210843	16.173863
26.570863	996.422262	16.178880
26.736539	986.822034	16.183898
26.761863	983.810766	16.188915
26.171401	978.967214	16.193933
26.644887	987.647628	16.198951
26.956726	983.124329	16.203968
26.426174	984.724947	16.208986
26.824438	971.863343	16.214003
26.448309	984.668051	16.219021
27.023830	981.993990	16.224039
26.698504	983.565809	16.229056
26.777721	989.423260	16.234074
27.038722	983.169061	16.239091
26.372180	990.540619	16.244109
26.423101	986.117903	16.249127
26.527889	992.962277	16.254144
26.748510	985.212229	16.259162
26.814398	982.901532	16.264179
26.709655	996.676990	16.269197
27.055748	989.450193	16.274215
26.638459	995.694213	16.279232
26.671415	991.949622	16.284250
26.995478	987.973519	16.289267
27.005554	1003.495166	16.294285
27.059170	1006.500657	16.299303
27.500866	1008.688346	16.304320
27.386251	999.475728	16.309338
27.696204	997.016578	16.314355
27.260632	978.295188	16.319373
27.154100	987.315212	16.324391
27.307451	985.700940	16.329408
27.302021	976.897359	16.334426
27.265308	970.411812	16.339443
27.272943	978.208563	16.344461
27.478441	983.614013	16.349479
27.532657	987.127482	16.354496
27.276761	981.234624	16.359514
27.380105	985.627208	16.364531
27.180175	994.497678	16.369549
27.588084	998.883871	16.374567
27.481302	1001.138020	16.379584
27.584882	1006.556190	16.384602
27.799252	999.558178	16.389619
27.617556	1002.511944	16.394637
27.635808	1003.604246	16.399655
27.535385	994.209543	16.404672
27.597684	1008.265109	16.409690
27.769289	1002.832693	16.414707
27.625490	997.720781	16.419725
27.565800	1004.284661	16.424743
27.564926	1000.898779	16.429760
27.960067	1010.096322	16.434778
27.978424	1001.790789	16.439795
27.531263	1008.594876	16.444813
27.795710	1004.637518	16.449831
27.836744	1004.391392	16.454848
27.604563	992.943877	16.459866
28.171694	1013.251274	16.464883
28.556944	1009.546502	16.469901
28.624616	1005.591379	16.474919
28.143624	1000.361555	16.479936
27.973107	990.785266	16.484954
28.396184	992.183760	16.489971
28.355498	996.207459	16.494989
28.295464	995.128173	16.500007
28.340622	1004.793606	16.505024
28.106375	1000.468934	16.510042
28.240966	987.449559	16.515059
28.029523	996.697357	16.520077
28.425108	994.325859	16.525095
28.461021	995.349140	16.530112
28.287327	993.407097	16.535130
28.679798	991.496823	16.540147
28.308329	996.897437	16.545165
28.433856	997.733199	16.550183
28.612904	999.422148	16.555200
28.295841	998.991939	16.560218
28.429464	990.687400	16.565235
28.385133	993.026497	16.570253
28.540535	1002.267674	16.575271
28.932845	1011.576109	16.580288
28.889137	1009.250915	16.585306
28.623764	994.962082	16.590323
28.487243	1002.424688	16.595341
28.723548	1007.108995	16.600359
29.191579	1004.707282	16.605376
28.684389	1006.149632	16.610394
28.471113	1003.251247	16.615411
28.522914	1008.178871	16.620429
28.600069	1019.442451	16.625447
28.816591	1019.680234	16.630464
28.737302	1021.216906	16.635482
28.858932	1018.095965	16.640499
28.671083	1026.090427	16.645517
28.832834	1017.506945	16.650535
28.607767	1020.458000	16.655552
28.648555	1032.882256	16.660570
29.411012	1033.233851	16.665587
29.086686	1044.335897	16.670605
29.391599	1045.339389	16.675623
29.372507	1038.863697	16.680640
29.250436	1050.543317	16.685658
29.116849	1044.019178	16.690675
28.915929	1046.108112	16.695693
29.340926	1048.585580	16.700711
29.442455	1035.031685	16.705728
29.316415	1043.966413	16.710746
29.524763	1041.538856	16.715763
29.251893	1042.240993	16.720781
29.078815	1045.474286	16.725799
29.373237	1042.036109	16.730816
29.414743	1033.796384	16.735834
29.714934	1032.493755	16.740851
29.311391	1039.865409	16.745869
29.251675	1033.875718	16.750887
29.866957	1037.371268	16.755904
29.569475	1041.788404	16.760922
29.755115	1035.637437	16.765939
29.788130	1051.430105	16.770957
29.971303	1051.707793	16.775975
29.979087	1037.628857	16.780992
29.877180	1035.259073	16.786010
30.087247	1033.241497	16.791027
29.873422	1032.078857	16.796045
29.526840	1030.431967	16.801063
30.097701	1034.960053	16.806080
29.869800	1034.175139	16.811098
29.957401	1037.153254	16.816115
29.849765	1052.437655	16.821133
30.280970	1064.510817	16.826151
30.485534	1053.629571	16.831168
29.994108	1047.678689	16.836186
30.015765	1029.996882	16.841203
30.363951	1041.028932	16.846221
30.310775	1049.093954	16.851239
30.163249	1040.962551	16.856256
30.211237	1044.969299	16.861274
30.332030	1051.429358	16.866291
30.618914	1046.405007	16.871309
30.183242	1035.560340	16.876327
30.152945	1041.024611	16.881344
30.193487	1049.027705	16.886362
30.315740	1049.791397	16.891379
30.203754	1052.409275	16.896397
30.607653	1054.571298	16.901415
30.944890	1056.737388	16.906432
30.523906	1053.691456	16.911450
30.462168	1047.686296	16.916467
30.444946	1058.620618	16.921485
30.621649	1057.526559	16.926503
30.692697	1049.171776	16.931520
30.592306	1057.442965	16.936538
30.928967	1052.000615	16.941555
30.549725	1054.565431	16.946573
30.740380	1053.768998	16.951591
30.659710	1054.860926	16.956608
30.539413	1055.940089	16.961626
30.865660	1043.550387	16.966643
30.779037	1050.992622	16.971661
30.962089	1055.789372	16.976679
31.052792	1050.429498	16.981696
30.734851	1054.524779	16.986714
31.067965	1056.177123	16.991731
30.855452	1058.372003	16.996749
31.147278	1071.666059	17.001767
31.273498	1061.933079	17.006784
31.517590	1073.912306	17.011802
31.308624	1052.772957	17.016819
30.979394	1060.003664	17.021837
31.107697	1057.213031	17.026855
31.840424	1062.561665	17.031872
31.238152	1060.367611	17.036890
31.023080	1052.511803	17.041907
31.254129	1061.731765	17.046925
31.066860	1081.380381	17.051943
31.684674	1074.909651	17.056960
31.143122	1089.510572	17.061978
31.363584	1079.097045	17.066995
31.252268	1075.674696	17.072013
31.220490	1088.586809	17.077031
31.436563	1077.978308	17.082048
31.151373	1084.940240	17.087066
31.508379	1084.105281	17.092083
31.393463	1088.736997	17.097101
31.366934	1099.698039	17.102119
31.791128	1102.724743	17.107136
31.580193	1113.297944	17.112154
31.601713	1098.027097	17.117171
31.744318	1101.886584	17.122189
31.830540	1104.849146	17.127207
31.731776	1100.036301	17.132224
31.933745	1098.408138	17.137242
31.659248	1099.366147	17.142259
31.675987	1095.579878	17.147277
31.861409	1095.850906	17.152295
32.104900	1099.631570	17.157312
32.356321	1117.678221	17.162330
32.329203	1105.245665	17.167347
32.290504	1087.986603	17.172365
32.117016	1097.806048	17.177383
32.308136	1096.936958	17.182400
32.095620	1096.143334	17.187418
32.283829	1088.918989	17.192435
32.241245	1087.120622	17.197453
32.338035	1098.431688	17.202471
32.497386	1109.609945	17.207488
32.345512	1106.752475	17.212506
32.437555	1105.763112	17.217523
32.655238	1110.311492	17.222541
32.628661	1095.729781	17.227559
32.932535	1089.206941	17.232576
32.680223	1088.738247	17.237594
32.360191	1087.822510	17.242611
32.432882	1080.669802	17.247629
32.371984	1089.007439	17.252647
32.484063	1092.600282	17.257664
32.847791	1103.112406	17.262682
32.855092	1102.817882	17.267699
32.992373	1103.440383	17.272717
32.769516	1104.526051	17.277735
33.018302	1094.941226	17.282752
32.954472	1104.014620	17.287770
32.834686	1109.625387	17.292787
33.018799	1100.337804	17.297805
33.001000	1104.733500	17.302823
32.707709	1100.973410	17.307840
32.841804	1095.575208	17.312858
32.614672	1106.706341	17.317875
32.845581	1102.536436	17.322893
32.544001	1108.942358	17.327911
33.118996	1093.897762	17.332928
32.925976	1099.617757	17.337946
33.318730	1127.927055	17.342963
33.409801	1118.628702	17.347981
33.369590	1120.418071	17.352999
33.080525	1116.748837	17.358016
33.192199	1118.590297	17.363034
33.031161	1119.745234	17.368051
33.488734	1126.954451	17.373069
33.512853	1130.201238	17.378087
33.568244	1119.191701	17.383104
33.610000	1124.767854	17.388122
33.367366	1126.519313	17.393139
33.840610	1130.807005	17.398157
33.382608	1131.490632	17.403175
33.843090	1129.465615	17.408192
33.652524	1130.918637	17.413210
33.835360	1126.964491	17.418227
33.755946	1119.131713	17.423245
33.666899	1120.950776	17.428263
33.829602	1110.255892	17.433280
34.174151	1119.603379	17.438298
33.652774	1122.685790	17.443315
33.989235	1117.013080	17.448333
33.701633	1121.315090	17.453351
34.390435	1118.812717	17.458368
34.250121	1122.959252	17.463386
34.061710	1115.187627	17.468403
34.173265	1113.422062	17.473421
34.012207	1121.024236	17.478439
34.110929	1115.868219	17.483456
34.123401	1113.351229	17.488474
33.540493	1121.129536	17.493491
34.024807	1124.642339	17.498509
34.301824	1131.242203	17.503527
34.483540	1131.024664	17.508544
34.510440	1133.838678	17.513562
34.858242	1136.467032	17.518579
34.668325	1115.255215	17.523597
34.511642	1117.952645	17.528615
34.577425	1103.037815	17.533632
34.667824	1100.852673	17.538650
34.131023	1105.509054	17.543667
34.774224	1111.313449	17.548685
34.610692	1129.418408	17.553703
34.730316	1128.181755	17.558720
34.648417	1124.249894	17.563738
34.562982	1139.994811	17.568755
34.872512	1137.336895	17.573773
34.582967	1136.119767	17.578791
35.079566	1130.239085	17.583808
35.081527	1130.582858	17.588826
34.705748	1136.246113	17.593843
35.202979	1132.946754	17.598861
34.741711	1127.123691	17.603879
35.180214	1133.168245	17.608896
34.963297	1132.410019	17.613914
34.885110	1131.522897	17.618931
35.083195	1130.403414	17.623949
34.802362	1130.137972	17.628967
35.091452	1135.669309	17.633984
35.054644	1135.779279	17.639002
34.806525	1129.695814	17.644019
35.060766	1129.504852	17.649037
35.047607	1134.663530	17.654055
35.164543	1140.938031	17.659072
35.539035	1148.519950	17.664090
35.601267	1158.656175	17.669107
36.001043	1145.156744	17.674125
35.488433	1138.814658	17.679143
35.298223	1122.885640	17.684160
35.610449	1131.932056	17.689178
35.587150	1141.772323	17.694195
35.821043	1143.607379	17.699213
35.884094	1143.985822	17.704231
35.343769	1131.967663	17.709248
35.585965	1134.928036	17.714266
35.624076	1150.145648	17.719283
36.057832	1154.792940	17.724301
36.029286	1154.829041	17.729319
35.841417	1151.525893	17.734336
35.873378	1149.772718	17.739354
35.735518	1148.153279	17.744371
35.981113	1144.959367	17.749389
35.948602	1151.645300	17.754407
36.465954	1155.115096	17.759424
35.989296	1145.450691	17.764442
35.508249	1148.627812	17.769459
36.005245	1143.024773	17.774477
35.814542	1150.943997	17.779495
36.133281	1157.647828	17.784512
35.833217	1146.485336	17.789530
35.901342	1164.276554	17.794547
36.208578	1168.561699	17.799565
36.529912	1171.572872	17.804583
36.407468	1181.640034	17.809600
36.342986	1174.707460	17.814618
36.119707	1184.534705	17.819635
36.078852	1185.686713	17.824653
36.034229	1184.333619	17.829671
36.410568	1196.131393	17.834688
36.838067	1198.337096	17.839706
36.593119	1207.915265	17.844723
36.886633	1192.425265	17.849741
36.942942	1192.615411	17.854759
37.131104	1193.611844	17.859776
36.641648	1183.902073	17.864794
36.389096	1184.970278	17.869811
36.940122	1193.739706	17.874829
36.848047	1200.116197	17.879847
36.650561	1201.942685	17.884864
36.462979	1199.987002	17.889882
36.747077	1199.270687	17.894899
37.016674	1185.037263	17.899917
36.835313	1192.860378	17.904935
36.979996	1195.349953	17.909952
36.918206	1191.153016	17.914970
37.223883	1213.514738	17.919987
37.192305	1214.488580	17.925005
37.651721	1214.186778	17.930023
37.508688	1210.090847	17.935040
37.722261	1199.154462	17.940058
37.186750	1193.093631	17.945075
37.606533	1187.019765	17.950093
37.403387	1197.601270	17.955111
37.261892	1187.439693	17.960128
37.152740	1202.115393	17.965146
37.767632	1212.638969	17.970163
37.894878	1205.348330	17.975181
37.735806	1215.809375	17.980199
37.642365	1207.398078	17.985216
37.924723	1214.009765	17.990234
37.908193	1221.851410	17.995251
38.027407	1199.430033	18.000269
37.638353	1199.582224	18.005287
37.854348	1196.408691	18.010304
38.037237	1203.679640	18.015322
37.929803	1218.124714	18.020339
38.364498	1215.775500	18.025357
38.363316	1205.525795	18.030375
37.987602	1198.013668	18.035392
37.998306	1183.435548	18.040410
37.942652	1185.981559	18.045427
37.774807	1197.539016	18.050445
38.029479	1212.943869	18.055463
37.893067	1218.254303	18.060480
38.312023	1217.043623	18.065498
38.103629	1219.102183	18.070515
38.442923	1210.771830	18.075533
38.178530	1206.887299	18.080551
38.355289	1213.171446	18.085568
38.136859	1205.177239	18.090586
37.865375	1214.620689	18.095603
38.332758	1223.598813	18.100621
38.596782	1230.131310	18.105639
38.476201	1232.409728	18.110656
38.590502	1233.704839	18.115674
38.348877	1249.237487	18.120691
38.362400	1232.225774	18.125709
38.561960	1242.479520	18.130727
38.450830	1240.171104	18.135744
39.097238	1236.599192	18.140762
39.230499	1249.331092	18.145779
39.345993	1237.983922	18.150797
39.473931	1241.918306	18.155815
38.922380	1233.742423	18.160832
39.170663	1226.246738	18.165850
39.019322	1228.511010	18.170867
39.167593	1227.673831	18.175885
39.303798	1220.842535	18.180903
39.130865	1225.906195	18.185920
39.143480	1221.180117	18.190938
39.099451	1229.748722	18.195955
39.332429	1225.300757	18.200973
39.400478	1227.010165	18.205991
39.020596	1234.453955	18.211008
39.411722	1242.326812	18.216026
39.281303	1252.101768	18.221043
39.256695	1247.681278	18.226061
39.422970	1249.296501	18.231079
39.520703	1253.601663	18.236096
39.697454	1250.503657	18.241114
39.721411	1252.153661	18.246131
39.649003	1242.268473	18.251149
39.394272	1249.610733	18.256167
39.266507	1254.503267	18.261184
39.535134	1245.637949	18.266202
39.655137	1248.560562	18.271219
39.937504	1262.212837	18.276237
40.453953	1264.092276	18.281255
40.044433	1262.647666	18.286272
39.976448	1248.618229	18.291290
39.820546	1249.532535	18.296307
40.051195	1260.428388	18.301325
40.391978	1255.749037	18.306343
40.025801	1273.809954	18.311360
40.458833	1261.122609	18.316378
40.439408	1266.206561	18.321395
40.025545	1258.918097	18.326413
40.163808	1262.715180	18.331431
39.969545	1262.789706	18.336448
40.193902	1253.366390	18.341466
40.226928	1265.507995	18.346483
40.014295	1261.085219	18.351501
40.532648	1255.096969	18.356519
40.284910	1263.406974	18.361536
40.730202	1258.036010	18.366554
40.573510	1265.656501	18.371571
40.608778	1278.870737	18.376589
40.583031	1286.130023	18.381607
40.719453	1287.412226	18.386624
40.735233	1290.887559	18.391642
40.832949	1287.107576	18.396659
41.123008	1294.567004	18.401677
41.485174	1283.020454	18.406695
41.100101	1299.982966	18.411712
41.055096	1294.691484	18.416730
40.953442	1299.923948	18.421747
41.201197	1294.558483	18.426765
41.497509	1295.067868	18.431783
40.930137	1298.009148	18.436800
41.282990	1292.056120	18.441818
41.310003	1287.166837	18.446835
41.145214	1295.596486	18.451853
41.534746	1291.496514	18.456871
41.268318	1295.732152	18.461888
41.342214	1285.322389	18.466906
41.442993	1282.681174	18.471923
41.265118	1282.882536	18.476941
41.353390	1286.879911	18.481959
41.211438	1289.805446	18.486976
40.978977	1282.087943	18.491994
41.395210	1293.601861	18.497011
41.343843	1308.937681	18.502029
41.441716	1312.750530	18.507047
41.515681	1313.954097	18.512064
42.152426	1309.001434	18.517082
41.915215	1307.151297	18.522099
41.680962	1313.060816	18.527117
41.953394	1307.700972	18.532135
41.849838	1302.418604	18.537152
41.699783	1309.157612	18.542170
42.000686	1307.750711	18.547187
42.155137	1322.120381	18.552205
42.541078	1329.694283	18.557223
42.174151	1318.693572	18.562240
42.440472	1306.540235	18.567258
42.581438	1308.140469	18.572275
42.068116	1302.331765	18.577293
42.676444	1310.843021	18.582311
41.857423	1301.496922	18.587328
42.556676	1310.202304	18.592346
42.693186	1317.294329	18.597363
42.552935	1301.644552	18.602381
42.834057	1303.907772	18.607399
42.432305	1305.078108	18.612416
42.650561	1304.870657	18.617434
42.528309	1310.058994	18.622451
42.462843	1322.825043	18.627469
43.024840	1319.089532	18.632487
42.814561	1329.397671	18.637504
42.897096	1316.452433	18.642522
42.733736	1319.242451	18.647539
42.667193	1321.771242	18.652557
43.172290	1323.507288	18.657575
42.856562	1322.281599	18.662592
42.875850	1318.526445	18.667610
42.694003	1326.883025	18.672627
42.401095	1323.820260	18.677645
42.845622	1333.022905	18.682663
42.682226	1351.484674	18.687680
43.228363	1339.941002	18.692698
43.542115	1340.832682	18.697715
43.199843	1345.045426	18.702733
43.741829	1342.875152	18.707751
43.379705	1344.058255	18.712768
43.194879	1345.766021	18.717786
43.566073	1341.384870	18.722803
43.180192	1355.680904	18.727821
43.509420	1354.039216	18.732839
43.822606	1366.105712	18.737856
43.808484	1364.855152	18.742874
43.898149	1366.283497	18.747891
43.956615	1368.145890	18.752909
43.859486	1369.666435	18.757927
44.004897	1366.222994	18.762944
44.100635	1373.668528	18.767962
44.288241	1361.688357	18.772979
43.999589	1352.887661	18.777997
44.169540	1358.055763	18.783015
44.140517	1360.114814	18.788032
44.105713	1353.647765	18.793050
44.465530	1353.863242	18.798067
44.229426	1356.844472	18.803085
44.024626	1363.027134	18.808103
43.775940	1369.592172	18.813120
44.275424	1357.345694	18.818138
44.359454	1363.634865	18.823155
44.358287	1358.910896	18.828173
44.032054	1350.273843	18.833191
44.337907	1356.282322	18.838208
44.308201	1357.142271	18.843226
44.863842	1358.649544	18.848243
44.919748	1379.308356	18.853261
45.178329	1368.967620	18.858279
44.422251	1364.477951	18.863296
44.791823	1377.021671	18.868314
44.828274	1375.479213	18.873331
44.535118	1386.368335	18.878349
44.915354	1380.789713	18.883367
44.923726	1385.190870	18.888384
45.027544	1382.886840	18.893402
44.950110	1377.922275	18.898419
44.931776	1381.892088	18.903437
45.424335	1374.740162	18.908455
45.173292	1385.588013	18.913472
45.382752	1375.630463	18.918490
45.558974	1377.446121	18.923507
44.930367	1376.982356	18.928525
45.479548	1372.185321	18.933543
45.165526	1382.497020	18.938560
45.433418	1375.970211	18.943578
45.552279	1367.939194	18.948595
45.603561	1370.708424	18.953613
45.705806	1369.414500	18.958631
45.454601	1376.311293	18.963648
45.211486	1383.055350	18.968666
45.631475	1389.210172	18.973683
45.265567	1404.150077	18.978701
45.813074	1402.916214	18.983719
46.014919	1405.838733	18.988736
46.054459	1397.050034	18.993754
46.000090	1390.611264	18.998771
46.056477	1396.204159	19.003789
45.843685	1395.505239	19.008807
45.858261	1394.979204	19.013824
46.285174	1396.904155	19.018842
46.442011	1389.201733	19.023859
45.992265	1388.697497	19.028877
46.034503	1393.102852	19.033895
46.174563	1386.905212	19.038912
46.019082	1405.129118	19.043930
46.457038	1401.848406	19.048947
46.447640	1410.809339	19.053965
46.708616	1412.135276	19.058983
46.993548	1412.772670	19.064000
46.911951	1409.935768	19.069018
47.269309	1403.325591	19.074035
46.737965	1398.494809	19.079053
47.087375	1390.260629	19.084071
46.811252	1387.375122	19.089088
46.828968	1392.320783	19.094106
46.786094	1385.113362	19.099123
46.592761	1396.349866	19.104141
47.031055	1406.071074	19.109159
47.254988	1416.314814	19.114176
47.208569	1433.505594	19.119194
47.273170	1418.612775	19.124211
47.541504	1416.122179	19.129229
47.186549	1408.934935	19.134247
47.328121	1406.337844	19.139264
47.161742	1415.373714	19.144282
47.169565	1415.104350	19.149299
47.523899	1415.614173	19.154317
47.267131	1406.710656	19.159335
47.212163	1419.844371	19.164352
47.205586	1406.496374	19.169370
47.451789	1403.396996	19.174387
47.218743	1405.809711	19.179405
47.453684	1407.499464	19.184423
47.450449	1433.406208	19.189440
47.125590	1429.916052	19.194458
47.551247	1425.813581	19.199475
47.502285	1433.559382	19.204493
47.451781	1436.697922	19.209511
47.769531	1444.563359	19.214528
47.650712	1455.059304	19.219546
48.091593	1454.056635	19.224563
48.034723	1460.951606	19.229581
48.162745	1451.694664	19.234599
48.251426	1444.198491	19.239616
48.218918	1454.933463	19.244634
48.462043	1449.230999	19.249651
48.353524	1458.570309	19.254669
48.808624	1449.218262	19.259687
48.521885	1448.758073	19.264704
48.347920	1454.159632	19.269722
48.627946	1446.450628	19.274739
48.590690	1455.999750	19.279757
48.249408	1451.805241	19.284775
48.412899	1444.259550	19.289792
48.681635	1453.148798	19.294810
48.946938	1445.186466	19.299827
48.631656	1449.672745	19.304845
48.617918	1446.800025	19.309863
48.873298	1458.683079	19.314880
48.927379	1466.327644	19.319898
49.082354	1461.071249	19.324915
48.871229	1473.058504	19.329933
49.305108	1466.619429	19.334951
49.434201	1467.615606	19.339968
49.157987	1469.394417	19.344986
49.515360	1467.038275	19.350003
48.934328	1468.192353	19.355021
49.014124	1470.559524	19.360039
49.693221	1463.646766	19.365056
49.382147	1462.066890	19.370074
49.463014	1458.873323	19.375091
49.270821	1469.746776	19.380109
49.599489	1464.116196	19.385127
49.388814	1458.534877	19.390144
49.169253	1464.741962	19.395162
49.973372	1481.292275	19.400179
49.826124	1494.367829	19.405197
50.287290	1490.199853	19.410215
50.479538	1480.699365	19.415232
49.864447	1467.701687	19.420250
49.810090	1465.510636	19.425267
49.894608	1475.315365	19.430285
50.178764	1489.693378	19.435303
49.984686	1486.599419	19.440320
50.044857	1497.449376	19.445338
50.178030	1485.584895	19.450355
50.020542	1487.089600	19.455373
50.076046	1492.742624	19.460391
50.250166	1485.738065	19.465408
49.906409	1489.906893	19.470426
50.385694	1492.233959	19.475443
50.344493	1502.620016	19.480461
50.634693	1504.484214	19.485479
50.478069	1504.473984	19.490496
50.890262	1502.525873	19.495514
50.862256	1495.069937	19.500531
50.840838	1505.847395	19.505549
50.499814	1508.819739	19.510567
50.925486	1501.709736	19.515584
50.946644	1514.301487	19.520602
51.211124	1504.786584	19.525619
51.148824	1505.661082	19.530637
51.238389	1504.302850	19.535655
51.370506	1492.631035	19.540672
50.973204	1498.540754	19.545690
50.994355	1494.267715	19.550707
51.129238	1496.506392	19.555725
51.296785	1498.588503	19.560743
51.626727	1497.041366	19.565760
51.308851	1502.648384	19.570778
51.691786	1508.152602	19.575795
51.953076	1508.222474	19.580813
51.975945	1512.264797	19.585831
51.851505	1497.672747	19.590848
51.568744	1504.631307	19.595866
51.723664	1494.148847	19.600883
51.491056	1500.802949	19.605901
51.650381	1517.194908	19.610919
51.990883	1512.048470	19.615936
51.806171	1511.373576	19.620954
51.775554	1512.984764	19.625971
51.783220	1518.799880	19.630989
51.842722	1520.516959	19.636007
51.785042	1515.142178	19.641024
52.070585	1512.863486	19.646042
52.376343	1510.326024	19.651059
52.313598	1511.661344	19.656077
52.039000	1513.190597	19.661095
52.513771	1521.994151	19.666112
52.260233	1535.891023	19.671130
52.432397	1533.655228	19.676147
52.423221	1537.042974	19.681165
52.274504	1547.499446	19.686183
52.579614	1537.498511	19.691200
52.512187	1546.061444	19.696218
52.699392	1531.480805	19.701235
52.664976	1528.081110	19.706253
52.374477	1548.803520	19.711271
52.934900	1550.625650	19.716288
53.108378	1560.722693	19.721306
52.910284	1552.191825	19.726323
53.400532	1557.183883	19.731341
53.147829	1565.561073	19.736359
53.349465	1556.737590	19.741376
53.073640	1561.785806	19.746394
53.428859	1551.571932	19.751411
53.396021	1557.409146	19.756429
53.252673	1557.980681	19.761447
53.238787	1547.710667	19.766464
53.525021	1553.027981	19.771482
53.446373	1543.645376	19.776499
53.142588	1554.185956	19.781517
53.253985	1572.415819	19.786535
53.710978	1575.967682	19.791552
53.721330	1574.915271	19.796570
54.126904	1567.202448	19.801587
54.085957	1567.035351	19.806605
53.715227	1575.563469	19.811623
54.199590	1562.839516	19.816640
54.163379	1573.287954	19.821658
54.013006	1574.659013	19.826675
54.055900	1564.506382	19.831693
54.174943	1566.378299	19.836711
54.664401	1563.338852	19.841728
54.647679	1570.921901	19.846746
54.645138	1573.005256	19.851763
54.687317	1563.641699	19.856781
54.324289	1568.088104	19.861799
54.735198	1574.279118	19.866816
54.620479	1570.797242	19.871834
54.218585	1570.708434	19.876851
54.296226	1564.782386	19.881869
54.413818	1573.401733	19.886887
54.931832	1586.118151	19.891904
54.830952	1589.147795	19.896922
54.968348	1587.220368	19.901939
54.945602	1581.849595	19.906957
55.185999	1594.227385	19.911975
55.185734	1592.185689	19.916992
55.145844	1594.391628	19.922010
55.033047	1589.416732	19.927027
54.879202	1581.061999	19.932045
54.884594	1586.511413	19.937063
55.264190	1587.809428	19.942080
55.210565	1587.142524	19.947098
55.169477	1588.326153	19.952115
55.868284	1598.448725	19.957133
55.741843	1601.741130	19.962151
55.833189	1597.681203	19.967168
55.967230	1585.371545	19.972186
55.584273	1581.805197	19.977203
55.569500	1575.230805	19.982221
55.647076	1597.855746	19.987239
55.869263	1593.235798	19.992256
55.690064	1601.399587	19.997274
55.706277	1605.506084	20.002291
55.974613	1604.959468	20.007309
55.647861	1600.525973	20.012327
55.946253	1601.833475	20.017344
56.285499	1597.933770	20.022362
56.166792	1623.581054	20.027379
56.750110	1623.225241	20.032397
56.376183	1624.886735	20.037415
56.635163	1616.770673	20.042432
56.591440	1621.299923	20.047450
56.460297	1624.593065	20.052467
56.625654	1618.246237	20.057485
56.828586	1627.991588	20.062503
56.841083	1620.298916	20.067520
56.792029	1621.385955	20.072538
56.886091	1623.861381	20.077555
56.712265	1624.911042	20.082573
56.577200	1631.133433	20.087591
56.987625	1622.918049	20.092608
57.029876	1623.883574	20.097626
57.027661	1625.528220	20.102643
57.036549	1620.565927	20.107661
56.944217	1631.925712	20.112679
57.408182	1644.202456	20.117696
57.099680	1645.572893	20.122714
56.823262	1649.018049	20.127731
57.330885	1646.417580	20.132749
57.135626	1650.800014	20.137767
57.735091	1645.294476	20.142784
57.804857	1646.574461	20.147802
57.518752	1651.870460	20.152819
57.793736	1649.997345	20.157837
57.793261	1658.846559	20.162855
58.039388	1667.464874	20.167872
58.309969	1664.143901	20.172890
57.987944	1670.976093	20.177907
58.325719	1667.887660	20.182925
58.281396	1674.471485	20.187943
58.419689	1662.208450	20.192960
57.849280	1651.466435	20.197978
58.234092	1663.711334	20.202995
58.502936	1656.600440	20.208013
58.085244	1663.302354	20.213031
57.908410	1662.029769	20.218048
57.705781	1670.039444	20.223066
57.974583	1671.345247	20.228083
58.347731	1675.292043	20.233101
58.415647	1687.538960	20.238119
58.357552	1687.049477	20.243136
58.653574	1686.908811	20.248154
58.852597	1692.937192	20.253171
58.834906	1680.445961	20.258189
58.949775	1698.577581	20.263207
59.208507	1702.289728	20.268224
59.184108	1702.574498	20.273242
58.961473	1707.428277	20.278259
59.068929	1698.076578	20.283277
59.500193	1714.650446	20.288295
59.310924	1693.371567	20.293312
59.078165	1696.036745	20.298330
58.976137	1710.544493	20.303347
59.627683	1710.724023	20.308365
59.371007	1698.399378	20.313383
59.182998	1700.028776	20.318400
59.399839	1696.921296	20.323418
59.472367	1711.054721	20.328435
59.827167	1722.215557	20.333453
59.866557	1724.630080	20.338471
59.748068	1718.210642	20.343488
60.031521	1726.545458	20.348506
60.173632	1719.684649	20.353523
60.246648	1719.594484	20.358541
60.246595	1717.555896	20.363559
60.336619	1714.862642	20.368576
60.293004	1710.198839	20.373594
60.270107	1714.103163	20.378611
60.680205	1713.610213	20.383629
60.554843	1718.584553	20.388647
60.621155	1713.098886	20.393664
60.608402	1714.237086	20.398682
60.317678	1718.505009	20.403699
60.963712	1708.990553	20.408717
60.588774	1723.768025	20.413735
60.915732	1717.108817	20.418752
60.681731	1713.494003	20.423770
60.555713	1723.839743	20.428787
60.838406	1724.509057	20.433805
60.826334	1740.312512	20.438823
61.037656	1736.704099	20.443840
61.341953	1741.819838	20.448858
60.957914	1740.181867	20.453875
61.449186	1731.199592	20.458893
61.439825	1732.820113	20.463911
61.432059	1732.531081	20.468928
61.540123	1734.145944	20.473946
61.283903	1730.518806	20.478963
61.409344	1735.201632	20.483981
61.426242	1733.453900	20.488999
61.666651	1759.285312	20.494016
61.573215	1758.744524	20.499034
61.689559	1752.133874	20.504051
62.052427	1751.654588	20.509069
62.033554	1752.213061	20.514087
62.322030	1755.421959	20.519104
62.740632	1754.810917	20.524122
62.041424	1750.555296	20.529139
62.467092	1741.365474	20.534157
62.584802	1757.025658	20.539175
62.155659	1749.430094	20.544192
62.881531	1744.365604	20.549210
62.708905	1744.285281	20.554227
62.820342	1744.498409	20.559245
62.648043	1751.029602	20.564263
62.574599	1750.037567	20.569280
62.756168	1745.464930	20.574298
62.827676	1750.102506	20.579315
62.623340	1746.558808	20.584333
62.750536	1737.475420	20.589351
62.622090	1741.778044	20.594368
62.810690	1736.607854	20.599386
62.565778	1748.398577	20.604403
63.009237	1753.846111	20.609421
63.259786	1757.695247	20.614439
63.324857	1758.325859	20.619456
63.456427	1767.848862	20.624474
63.461133	1767.617849	20.629491
63.917955	1759.593999	20.634509
63.902680	1765.349650	20.639527
63.632102	1765.429748	20.644544
63.715139	1759.190363	20.649562
63.741171	1766.738436	20.654579
63.643916	1756.310863	20.659597
63.981503	1761.525568	20.664615
63.953912	1770.117121	20.669632
63.655671	1760.560303	20.674650
63.842900	1767.963355	20.679667
64.014606	1757.263527	20.684685
64.106245	1766.515029	20.689703
63.727501	1767.953217	20.694720
63.946710	1767.382687	20.699738
64.042542	1773.591268	20.704755
63.747854	1781.075670	20.709773
64.022794	1779.950493	20.714791
64.112350	1789.950277	20.719808
64.231770	1789.370035	20.724826
64.503670	1808.215795	20.729843
64.365347	1803.636143	20.734861
64.699415	1814.607755	20.739879
64.711502	1807.950198	20.744896
64.885035	1803.640737	20.749914
65.191665	1801.538611	20.754931
65.108479	1807.633062	20.759949
65.330926	1797.812114	20.764967
65.407391	1795.742669	20.769984
65.526886	1791.596262	20.775002
65.437131	1803.776286	20.780019
65.535674	1803.281348	20.785037
65.420237	1801.863490	20.790055
65.240199	1805.918536	20.795072
65.311072	1800.501562	20.800090
65.430432	1815.643975	20.805107
65.632156	1825.260230	20.810125
65.793950	1821.350234	20.815143
65.767107	1821.392384	20.820160
66.019382	1833.762180	20.825178
65.648476	1821.439455	20.830195
65.897144	1821.362968	20.835213
65.917857	1819.037105	20.840231
65.954936	1822.657552	20.845248
65.923995	1837.946465	20.850266
66.239564	1850.022387	20.855283
66.317854	1851.143264	20.860301
66.554308	1848.783808	20.865319
66.544328	1839.888988	20.870336
66.448488	1845.859186	20.875354
66.377461	1844.516464	20.880371
66.348456	1845.035490	20.885389
66.364653	1839.775344	20.890407
66.570712	1866.792566	20.895424
66.538982	1871.907009	20.900442
67.180282	1874.038484	20.905459
67.086610	1871.613656	20.910477
67.394029	1870.290908	20.915495
66.999079	1869.506717	20.920512
67.263287	1876.178283	20.925530
66.918603	1869.106022	20.930547
66.938284	1869.270320	20.935565
67.352461	1871.759058	20.940583
67.482503	1889.686532	20.945600
67.960742	1888.210950	20.950618
67.771277	1888.464618	20.955635
67.704636	1889.674336	20.960653
67.903448	1880.330409	20.965671
67.687905	1881.238252	20.970688
68.075984	1876.305216	20.975706
68.065415	1876.493159	20.980723
67.774931	1876.197647	20.985741
68.016280	1874.951459	20.990759
67.698929	1885.011493	20.995776
68.227197	1876.651410	21.000794
68.302073	1879.899899	21.005811
68.170135	1882.416859	21.010829
68.182218	1871.707100	21.015847
68.413870	1879.384158	21.020864
68.517963	1880.188585	21.025882
68.313689	1889.113826	21.030899
68.392229	1899.992727	21.035917
68.589485	1903.165360	21.040935
68.712611	1906.933379	21.045952
68.699385	1901.750381	21.050970
69.002137	1901.431936	21.055987
68.719598	1896.357145	21.061005
68.830969	1903.759440	21.066023
69.106173	1930.330478	21.071040
69.602266	1926.491491	21.076058
69.355668	1916.207002	21.081075
69.342637	1926.876107	21.086093
69.606351	1924.711219	21.091111
69.495276	1926.104589	21.096128
69.634030	1922.551621	21.101146
69.526871	1930.000575	21.106163
69.510086	1924.884400	21.111181
69.939585	1922.599023	21.116199
69.904492	1929.736946	21.121216
69.772991	1921.119790	21.126234
69.423248	1925.864026	21.131251
69.623498	1930.528944	21.136269
70.110742	1940.760393	21.141287
69.855459	1954.253904	21.146304
70.012344	1950.767538	21.151322
69.773577	1958.158096	21.156339
69.649798	1962.090804	21.161357
70.394377	1970.316069	21.166375
70.116882	1978.656285	21.171392
70.494224	1969.136188	21.176410
70.538330	1970.028857	21.181427
70.762251	1989.541865	21.186445
71.439624	1988.366644	21.191463
71.506217	1978.907547	21.196480
71.429993	1959.318102	21.201498
71.559407	1965.259581	21.206515
71.311092	1962.890376	21.211533
71.365863	1954.850139	21.216551
71.147281	1959.690731	21.221568
71.255175	1943.705098	21.226586
71.687479	1952.698522	21.231603
71.593750	1963.632687	21.236621
71.683237	1952.405881	21.241639
71.361057	1954.374939	21.246656
71.671841	1960.865711	21.251674
71.966637	1969.416633	21.256691
71.521193	1983.267988	21.261709
72.393677	1976.113479	21.266727
72.138483	1983.225729	21.271744
72.045308	1972.964658	21.276762
72.222984	1978.759767	21.281779
72.077993	1970.621232	21.286797
71.911663	1972.250434	21.291815
71.739640	1980.138714	21.296832
71.726727	1976.252729	21.301850
72.407803	1983.064567	21.306867
72.626486	1986.344336	21.311885
72.477939	1999.635064	21.316903
72.553121	1996.505405	21.321920
72.858063	2000.794266	21.326938
72.914523	1997.282499	21.331955
72.822194	1993.661350	21.336973
72.919865	1986.157238	21.341991
72.884223	1986.484791	21.347008
72.614718	1988.455119	21.352026
72.905238	1995.302521	21.357043
73.063507	2009.782609	21.362061
73.099204	2017.237761	21.367079
73.245678	2023.252345	21.372096
73.304447	2005.292382	21.377114
73.152172	2015.781241	21.382131
73.280725	2017.462370	21.387149
73.968694	2026.100433	21.392167
73.783394	2034.893399	21.397184
73.938632	2028.936181	21.402202
74.036627	2032.111668	21.407219
73.902713	2034.726791	21.412237
74.182550	2028.324123	21.417255
74.110345	2037.238343	21.422272
74.298247	2034.340446	21.427290
74.335141	2031.709067	21.432307
74.344874	2026.768621	21.437325
74.348345	2021.529339	21.442343
74.568408	2027.822813	21.447360
74.687567	2023.717432	21.452378
74.375235	2026.496038	21.457395
74.365844	2020.053193	21.462413
74.974456	2032.263502	21.467431
75.188651	2043.670502	21.472448
75.215750	2050.158135	21.477466
75.458336	2057.142418	21.482483
75.039244	2056.526085	21.487501
75.033795	2054.595602	21.492519
74.990947	2050.742665	21.497536
75.333132	2049.793203	21.502554
75.460707	2049.372636	21.507571
74.848569	2046.974855	21.512589
75.131349	2047.511619	21.517607
75.557961	2067.479169	21.522624
75.499782	2074.841659	21.527642
75.750426	2070.838877	21.532659
75.624710	2077.356625	21.537677
75.993783	2071.145184	21.542695
75.867812	2072.190575	21.547712
76.088500	2068.476493	21.552730
75.947180	2079.061517	21.557747
76.300143	2088.401892	21.562765
76.433577	2094.216550	21.567783
76.195069	2099.148649	21.572800
76.248920	2100.216540	21.577818
76.555241	2098.338501	21.582835
76.601551	2103.163137	21.587853
76.900506	2091.228259	21.592871
76.764574	2095.311218	21.597888
76.372180	2089.164676	21.602906
76.656208	2088.918573	21.607923
77.163262	2103.375993	21.612941
77.367314	2113.061472	21.617959
77.264073	2112.881977	21.622976
76.997840	2115.987949	21.627994
77.349837	2108.671417	21.633011
77.172026	2113.379465	21.638029
77.207934	2112.720693	21.643047
77.100552	2113.343453	21.648064
77.284128	2113.974563	21.653082
77.307528	2118.244168	21.658099
77.485070	2126.882852	21.663117
77.559928	2128.891102	21.668135
78.004029	2139.110448	21.673152
77.982420	2136.374548	21.678170
78.316629	2131.298344	21.683187
78.280581	2136.924799	21.688205
77.948545	2133.366190	21.693223
78.217698	2129.322642	21.698240
78.350888	2132.849289	21.703258
78.542231	2137.610327	21.708275
78.573586	2155.887964	21.713293
78.758981	2154.593661	21.718311
78.729564	2157.429230	21.723328
78.812699	2154.639148	21.728346
78.799340	2155.064224	21.733363
78.887213	2162.246213	21.738381
78.888097	2154.485688	21.743399
79.080363	2159.325487	21.748416
78.927209	2161.091517	21.753434
79.007700	2153.971880	21.758451
79.238331	2165.215446	21.763469
79.274429	2171.442934	21.768487
79.014689	2180.364331	21.773504
79.445789	2183.465891	21.778522
79.918972	2172.501116	21.783539
79.748170	2185.839630	21.788557
79.923151	2174.387925	21.793575
79.815384	2176.418302	21.798592
80.211124	2177.155244	21.803610
79.742088	2172.970985	21.808627
79.540585	2180.393705	21.813645
80.103647	2186.712731	21.818663
80.398315	2197.681246	21.823680
80.224068	2198.248144	21.828698
80.736548	2197.597224	21.833715
80.750601	2192.564537	21.838733
80.537491	2195.201482	21.843751
80.421345	2192.404550	21.848768
80.758135	2192.008214	21.853786
80.822062	2183.824430	21.858803
80.890103	2195.838135	21.863821
81.170130	2191.212184	21.868839
81.353596	2202.756621	21.873856
80.897135	2202.054578	21.878874
81.132248	2204.337702	21.883891
81.252679	2215.434347	21.888909
81.640584	2210.475999	21.893927
81.747653	2205.555065	21.898944
81.302102	2204.403177	21.903962
81.526810	2199.072590	21.908979
81.560641	2200.219347	21.913997
81.418206	2196.142031	21.919015
81.957173	2208.562130	21.924032
81.859058	2226.762162	21.929050
82.248382	2230.507739	21.934067
82.086474	2239.732687	21.939085
82.197948	2230.275937	21.944103
82.567779	2224.711298	21.949120
82.302167	2224.209926	21.954138
82.235074	2222.680360	21.959155
82.201881	2231.358218	21.964173
82.472156	2230.852310	21.969191
82.700259	2243.740576	21.974208
82.571213	2254.771940	21.979226
82.856472	2245.458547	21.984243
82.520258	2248.957310	21.989261
82.706851	2248.480210	21.994279
83.129937	2242.194026	21.999296
82.939948	2248.380998	22.004314
82.892394	2257.569214	22.009331
82.774711	2262.971721	22.014349
83.351855	2264.011800	22.019367
83.271746	2271.418813	22.024384
83.078339	2267.983768	22.029402
83.530874	2272.473790	22.034419
83.331577	2288.938073	22.039437
83.586423	2297.069316	22.044455
84.145222	2287.574450	22.049472
84.159422	2303.405872	22.054490
84.367967	2291.298735	22.059507
84.343364	2293.054232	22.064525
84.611446	2295.016637	22.069543
84.457345	2287.554755	22.074560
84.247511	2286.624952	22.079578
84.057377	2285.190281	22.084595
84.448956	2298.753761	22.089613
84.677754	2303.632095	22.094631
85.140761	2311.121831	22.099648
84.905518	2310.782995	22.104666
84.892074	2312.019175	22.109683
84.960553	2321.022092	22.114701
85.207127	2310.651123	22.119719
85.383771	2310.415425	22.124736
85.196331	2314.276066	22.129754
85.005894	2317.505979	22.134771
85.309577	2312.813195	22.139789
85.302185	2322.888334	22.144807
85.933699	2329.329305	22.149824
85.429608	2336.029140	22.154842
86.040111	2333.201106	22.159859
85.953640	2332.810703	22.164877
85.520827	2333.944910	22.169895
85.925015	2330.846025	22.174912
85.732731	2346.318291	22.179930
86.143082	2348.634114	22.184947
86.340291	2352.150838	22.189965
86.179624	2351.831949	22.194983
86.774469	2349.549180	22.200000
86.266636	2355.820391	22.205018
86.526598	2346.245782	22.210035
86.534966	2361.560582	22.215053
86.523771	2360.221129	22.220071
86.695392	2371.316212	22.225088
86.709241	2385.500335	22.230106
87.171898	2372.113275	22.235123
87.820001	2371.248719	22.240141
87.773545	2370.331347	22.245159
87.858550	2359.108140	22.250176
87.356622	2367.240468	22.255194
87.839378	2365.593723	22.260211
87.829239	2366.415958	22.265229
87.605158	2367.470330	22.270247
87.902222	2365.764128	22.275264
87.672077	2372.320333	22.280282
88.104940	2359.755323	22.285299
88.175318	2360.047439	22.290317
87.932411	2363.276062	22.295335
88.019133	2371.057952	22.300352
88.459940	2389.622393	22.305370
88.435585	2386.605999	22.310387
88.491669	2386.846690	22.315405
88.309059	2382.538887	22.320423
89.040674	2374.093262	22.325440
88.582461	2389.468106	22.330458
88.502722	2388.862045	22.335475
88.667599	2381.391489	22.340493
89.012158	2378.093583	22.345511
89.165592	2395.004849	22.350528
88.856676	2403.299659	22.355546
89.264838	2404.877328	22.360563
89.458544	2414.337350	22.365581
89.140437	2410.877507	22.370599
89.214395	2406.147877	22.375616
89.177979	2409.085567	22.380634
89.442040	2418.035989	22.385651
89.595052	2418.908569	22.390669
89.459239	2427.649839	22.395687
90.173541	2428.621234	22.400704
89.941050	2433.880711	22.405722
89.988688	2416.392313	22.410739
90.035656	2425.890968	22.415757
89.882857	2448.085766	22.420775
90.232285	2454.504425	22.425792
90.128121	2457.010830	22.430810
90.355862	2447.772563	22.435827
90.755538	2455.641474	22.440845
90.662327	2465.950975	22.445863
90.513024	2471.749812	22.450880
90.934428	2474.420561	22.455898
91.055990	2468.307483	22.460915
91.526209	2462.686113	22.465933
91.183239	2471.330261	22.470951
91.381795	2467.247133	22.475968
91.155968	2468.153450	22.480986
91.363666	2477.204202	22.486003
91.537344	2487.825636	22.491021
91.324758	2499.223630	22.496039
91.602476	2494.544309	22.501056
92.148051	2489.103715	22.506074
92.187781	2487.005194	22.511091
92.296683	2488.900880	22.516109
91.917731	2487.224174	22.521127
92.203005	2496.073497	22.526144
91.888820	2509.339895	22.531162
92.270715	2514.093457	22.536179
92.447723	2502.028961	22.541197
92.537802	2506.521822	22.546215
92.747828	2509.850377	22.551232
92.692983	2510.105184	22.556250
92.755090	2529.934330	22.561267
93.367069	2529.116420	22.566285
93.223621	2530.682145	22.571303
93.458308	2544.320736	22.576320
93.420811	2533.817129	22.581338
93.601293	2531.904986	22.586355
93.920969	2524.959415	22.591373
93.578045	2531.580578	22.596391
93.810238	2527.552164	22.601408
94.017127	2526.257645	22.606426
93.753314	2525.547686	22.611443
94.074110	2518.712405	22.616461
94.059901	2523.186791	22.621479
94.188609	2516.892692	22.626496
94.166772	2523.798398	22.631514
94.002690	2523.457946	22.636531
94.420508	2535.666746	22.641549
94.424432	2553.030657	22.646567
94.416245	2556.147025	22.651584
94.166875	2549.416283	22.656602
94.227199	2549.943514	22.661619
94.291233	2550.318678	22.666637
94.693441	2574.298742	22.671655
94.405064	2573.769343	22.676672
94.432774	2578.186720	22.681690
94.412590	2592.044922	22.686707
94.922936	2600.013438	22.691725
94.818008	2605.966368	22.696743
94.881426	2606.291132	22.701760
95.786458	2615.681541	22.706778
95.831113	2620.617035	22.711795
95.888439	2613.036886	22.716813
96.067874	2632.245076	22.721831
96.012897	2626.563403	22.726848
96.046492	2628.401396	22.731866
96.181129	2626.493224	22.736883
96.399498	2615.924485	22.741901
96.226367	2624.914675	22.746919
96.397060	2620.785354	22.751936
96.737026	2630.762401	22.756954
96.768063	2639.853364	22.761971
96.962258	2638.305174	22.766989
97.133722	2644.817887	22.772007
97.000844	2632.719494	22.777024
96.759892	2647.830340	22.782042
97.009737	2642.274786	22.787059
97.651252	2632.426009	22.792077
96.747038	2632.907740	22.797095
96.859413	2640.048234	22.802112
97.717567	2654.729168	22.807130
97.260733	2667.730692	22.812147
97.690583	2655.462613	22.817165
97.190219	2671.743731	22.822183
97.529163	2669.661724	22.827200
98.006993	2671.720913	22.832218
97.569683	2684.359620	22.837235
98.409954	2685.014750	22.842253
98.095356	2686.689193	22.847271
98.553523	2690.458867	22.852288
98.399251	2691.865333	22.857306
98.802032	2705.739827	22.862323
99.106319	2713.560582	22.867341
99.008134	2712.862701	22.872359
98.762584	2709.382035	22.877376
98.974297	2711.059751	22.882394
99.045911	2707.390839	22.887411
99.244690	2704.374368	22.892429
99.084601	2707.795300	22.897447
99.361664	2705.517780	22.902464
99.714617	2721.164276	22.907482
99.645958	2722.327023	22.912499
99.715317	2718.680553	22.917517
99.733635	2725.210827	22.922535
100.044565	2724.023182	22.927552
100.310580	2722.899338	22.932570
100.203071	2726.955923	22.937587
100.208606	2726.137743	22.942605
100.308258	2728.590360	22.947623
100.421888	2723.605141	22.952640
100.446994	2720.192796	22.957658
100.583676	2738.353635	22.962675
101.039095	2736.518594	22.967693
100.714245	2745.223173	22.972711
100.598098	2746.036681	22.977728
100.986470	2738.512243	22.982746
100.694723	2748.338381	22.987763
101.038645	2734.603436	22.992781
100.848676	2755.033855	22.997799
101.202164	2762.348313	23.002816
101.237153	2765.461151	23.007834
101.020750	2768.654158	23.012851
101.281516	2770.762935	23.017869
101.346077	2784.835327	23.022887
101.590460	2788.934976	23.027904
101.795694	2790.752575	23.032922
101.619850	2789.984724	23.037939
101.888071	2792.575220	23.042957
102.287247	2800.210812	23.047975
102.275312	2812.530896	23.052992
102.196228	2812.742140	23.058010
102.126170	2808.792283	23.063027
102.171308	2811.483792	23.068045
103.037556	2824.560324	23.073063
103.446199	2826.090616	23.078080
103.515817	2812.739174	23.083098
103.288938	2815.078527	23.088115
103.668823	2810.645171	23.093133
103.582961	2813.297111	23.098151
103.655599	2807.797500	23.103168
103.893920	2822.956961	23.108186
103.805388	2813.420581	23.113203
104.124183	2814.043289	23.118221
104.032060	2811.261455	23.123239
103.813703	2810.235113	23.128256
104.346997	2804.202997	23.133274
103.991464	2814.417829	23.138291
104.506920	2807.514258	23.143309
103.967380	2806.998707	23.148327
103.916545	2803.288876	23.153344
104.153945	2824.138869	23.158362
104.357010	2822.819676	23.163379
104.286487	2829.632085	23.168397
104.502822	2842.169135	23.173415
104.947442	2849.980725	23.178432
105.097202	2854.603250	23.183450
104.878062	2865.825756	23.188467
104.909917	2867.727166	23.193485
105.392505	2872.916467	23.198503
105.455762	2882.759996	23.203520
106.086673	2884.770128	23.208538
105.595073	2892.885303	23.213555
105.751897	2888.082680	23.218573
105.791941	2883.651720	23.223591
105.974688	2890.910756	23.228608
106.021811	2880.870340	23.233626
106.024051	2897.543665	23.238643
106.278876	2907.486781	23.243661
106.420853	2913.997871	23.248679
106.236843	2900.057792	23.253696
106.833385	2908.827296	23.258714
106.938451	2910.291241	23.263731
106.799826	2909.457624	23.268749
106.798299	2917.206150	23.273767
107.189405	2921.125181	23.278784
107.117865	2914.792686	23.283802
107.150061	2920.714902	23.288819
107.290746	2919.765208	23.293837
107.898629	2927.018035	23.298855
107.468135	2922.988558	23.303872
107.767277	2935.569590	23.308890
108.118876	2943.695533	23.313907
107.997116	2933.069099	23.318925
107.947243	2942.182281	23.323943
108.270384	2939.897558	23.328960
108.598484	2941.374122	23.333978
108.421402	2937.939561	23.338995
108.384447	2935.963390	23.344013
108.810322	2942.168334	23.349031
108.748981	2938.094003	23.354048
108.730429	2935.647866	23.359066
108.897945	2947.940103	23.364083
109.216423	2958.618175	23.369101
109.220167	2963.093032	23.374119
108.859025	2968.047617	23.379136
109.454400	2961.854290	23.384154
109.400506	2963.191496	23.389171
109.236615	2958.167362	23.394189
109.434917	2953.560253	23.399207
109.809240	2973.316031	23.404224
110.129308	2976.113096	23.409242
110.150498	2980.108671	23.414259
109.943452	2968.201495	23.419277
110.074745	2980.269000	23.424295
109.886624	2989.719340	23.429312
110.131695	2981.989873	23.434330
110.028386	2995.589904	23.439347
110.295862	3000.547621	23.444365
110.435774	3003.713599	23.449383
110.298188	3013.623186	23.454400
110.686243	3024.511392	23.459418
110.836596	3028.811946	23.464435
111.035796	3026.688533	23.469453
111.113164	3033.323345	23.474471
110.995941	3048.459450	23.479488
111.371385	3054.435576	23.484506
111.810203	3053.363712	23.489523
111.759651	3057.632430	23.494541
112.024121	3052.790910	23.499559
111.807486	3069.889831	23.504576
112.571837	3077.162543	23.509594
112.428411	3072.883190	23.514611
112.559617	3074.870150	23.519629
112.740544	3067.614582	23.524647
112.398183	3069.621618	23.529664
112.683571	3064.625344	23.534682
112.468982	3069.295182	23.539699
112.512083	3066.233454	23.544717
112.671172	3081.279225	23.549735
112.744388	3086.172528	23.554752
113.235441	3086.654806	23.559770
112.848705	3091.484008	23.564787
113.383652	3104.214657	23.569805
113.840105	3103.364129	23.574823
113.805560	3111.954251	23.579840
114.066607	3112.254568	23.584858
113.599874	3108.640986	23.589875
113.550902	3118.300126	23.594893
114.265596	3123.797380	23.599911
114.020589	3139.922386	23.604928
114.178473	3122.327766	23.609946
114.348145	3128.607381	23.614963
114.367120	3133.613294	23.619981
114.634104	3138.713152	23.624999
114.768984	3157.079843	23.630016
115.008026	3152.015014	23.635034
115.009464	3154.047435	23.640051
114.876172	3149.589743	23.645069
115.062413	3166.338822	23.650087
115.111574	3171.677752	23.655104
115.241637	3172.746466	23.660122
115.736439	3180.708195	23.665139
115.453741	3185.429696	23.670157
115.701729	3188.124397	23.675175
116.016313	3204.904028	23.680192
116.157115	3205.229381	23.685210
116.414041	3211.640622	23.690227
116.740086	3204.857919	23.695245
116.537841	3195.945018	23.700263
116.248021	3198.878104	23.705280
116.498475	3201.345181	23.710298
116.788329	3194.697517	23.715315
116.832266	3196.379308	23.720333
117.191512	3203.352189	23.725351
116.822956	3213.272597	23.730368
117.047555	3216.154000	23.735386
116.964446	3213.500102	23.740403
116.994098	3220.237096	23.745421
117.104534	3234.485754	23.750439
117.563891	3247.509171	23.755456
117.735593	3246.744000	23.760474
117.857939	3248.287342	23.765491
117.755523	3253.252221	23.770509
118.165559	3260.182498	23.775527
117.957204	3269.472015	23.780544
118.595532	3270.840340	23.785562
118.589978	3267.404260	23.790579
118.451217	3271.743573	23.795597
118.570582	3271.554656	23.800615
118.760317	3288.590515	23.805632
118.936097	3288.433844	23.810650
119.073510	3294.686978	23.815667
119.047354	3289.919049	23.820685
119.601775	3290.454591	23.825703
119.021660	3306.663481	23.830720
119.742478	3315.559020	23.835738
119.652699	3314.272761	23.840755
119.193796	3322.332539	23.845773
119.959891	3309.929605	23.850791
119.920407	3331.391404	23.855808
120.072688	3333.987406	23.860826
120.421917	3341.129176	23.865843
120.007486	3346.811765	23.870861
120.578187	3337.879450	23.875879
120.709942	3358.443520	23.880896
120.818403	3358.688694	23.885914
120.885647	3358.646762	23.890931
121.084808	3360.683141	23.895949
121.069262	3353.505390	23.900967
121.071368	3365.104061	23.905984
121.444169	3374.268433	23.911002
121.723228	3374.689041	23.916019
121.775497	3380.014924	23.921037
121.651216	3381.252653	23.926055
121.542743	3379.517968	23.931072
121.888256	3390.463518	23.936090
121.973066	3404.025100	23.941107
122.008944	3403.656654	23.946125
122.625314	3400.871731	23.951143
122.099594	3404.892583	23.956160
121.879250	3408.865890	23.961178
122.888816	3415.295740	23.966195
122.850739	3427.314166	23.971213
123.192038	3423.391657	23.976231
123.001005	3433.297171	23.981248
123.535326	3431.089975	23.986266
123.831887	3438.410418	23.991283
123.495660	3448.632070	23.996301
123.617529	3442.158811	24.001319
123.740234	3448.335384	24.006336
123.936845	3445.858834	24.011354
124.187757	3441.019322	24.016371
123.857206	3449.718814	24.021389
124.212596	3439.207163	24.026407
124.320806	3444.022523	24.031424
124.011706	3461.549670	24.036442
124.286776	3464.398005	24.041459
124.313177	3468.664308	24.046477
124.814615	3467.033496	24.051495
124.667849	3483.096170	24.056512
124.822226	3493.907420	24.061530
124.934621	3487.359871	24.066547
124.891973	3485.646489	24.071565
125.601575	3492.650152	24.076583
125.264106	3508.982411	24.081600
125.722398	3512.632305	24.086618
126.046584	3506.607265	24.091635
125.971696	3503.750048	24.096653
126.147516	3502.457142	24.101671
126.399063	3499.987812	24.106688
126.749879	3499.062184	24.111706
126.728095	3489.395118	24.116723
126.537626	3497.738268	24.121741
126.840079	3504.827420	24.126759
127.295563	3522.437582	24.131776
127.173657	3519.559277	24.136794
126.969102	3518.022597	24.141811
127.250755	3518.831016	24.146829
127.345587	3528.385925	24.151847
127.467134	3519.570793	24.156864
127.129913	3519.367744	24.161882
127.289032	3533.738464	24.166899
127.794805	3541.837518	24.171917
128.188073	3538.525508	24.176935
127.758667	3545.479281	24.181952
128.042534	3563.024672	24.186970
128.194089	3568.581336	24.191987
128.099678	3570.994847	24.197005
128.258889	3567.867613	24.202023
128.528443	3598.219975	24.207040
128.963758	3595.469525	24.212058
129.119448	3598.102909	24.217075
128.709920	3603.775346	24.222093
128.765780	3612.610440	24.227111
129.368399	3626.255693	24.232128
129.556922	3622.009745	24.237146
129.839599	3619.065277	24.242163
129.694292	3615.316331	24.247181
129.748120	3623.514192	24.252199
129.677384	3640.780310	24.257216
129.697606	3642.440585	24.262234
130.020871	3654.731151	24.267251
130.044523	3656.586579	24.272269
130.353676	3659.691605	24.277287
130.333921	3664.564822	24.282304
130.427638	3682.338776	24.287322
130.859002	3690.705137	24.292339
131.055259	3692.584194	24.297357
131.254636	3694.636358	24.302375
131.494928	3701.650047	24.307392
131.419877	3710.016356	24.312410
131.904331	3707.333989	24.317427
131.704813	3716.234143	24.322445
132.019462	3720.752314	24.327463
131.914702	3716.069102	24.332480
131.780240	3717.775561	24.337498
132.413578	3724.724909	24.342515
131.939926	3733.576222	24.347533
132.179424	3737.478007	24.352551
132.623931	3743.721360	24.357568
132.915319	3755.429899	24.362586
133.446245	3756.006990	24.367603
133.135344	3760.647813	24.372621
133.280045	3759.826857	24.377639
133.397785	3750.936455	24.382656
133.406250	3757.512825	24.387674
133.891623	3741.671979	24.392691
133.443107	3745.349480	24.397709
133.388608	3751.304404	24.402727
133.459070	3759.155708	24.407744
133.991337	3768.598452	24.412762
134.211019	3772.159301	24.417779
133.985356	3788.026218	24.422797
134.462328	3786.212970	24.427815
134.448844	3788.588659	24.432832
134.524049	3795.078902	24.437850
134.653618	3796.734792	24.442867
134.680748	3811.729125	24.447885
134.983404	3821.431739	24.452903
135.109501	3834.734717	24.457920
134.939072	3822.862306	24.462938
135.490516	3827.735010	24.467955
135.783684	3839.740014	24.472973
135.899535	3840.189201	24.477991
135.887612	3837.091722	24.483008
135.676986	3843.402390	24.488026
136.020489	3856.494786	24.493043
136.255336	3864.790824	24.498061
136.276266	3860.974913	24.503079
136.664991	3879.182882	24.508096
136.640519	3880.234667	24.513114
137.110602	3877.033731	24.518131
137.157457	3880.583634	24.523149
137.016333	3887.053934	24.528167
137.687129	3899.075934	24.533184
137.437800	3910.534195	24.538202
137.636370	3904.380236	24.543219
137.537052	3909.755126	24.548237
137.969538	3915.268159	24.553255
137.969829	3917.244032	24.558272
138.173944	3929.502836	24.563290
138.276906	3920.459996	24.568307
138.354400	3926.864710	24.573325
138.337063	3934.594041	24.578343
138.517122	3944.088557	24.583360
138.930274	3956.848244	24.588378
139.129038	3954.585916	24.593395
139.147205	3960.570627	24.598413
139.291789	3957.855919	24.603431
139.526621	3959.990970	24.608448
139.595703	3970.822098	24.613466
140.020648	3972.185828	24.618483
139.835463	3984.044464	24.623501
139.613482	3980.563037	24.628519
139.782984	3989.794094	24.633536
140.033608	3999.893127	24.638554
140.254652	4001.815702	24.643571
140.767163	4002.278887	24.648589
140.734638	4011.311001	24.653607
140.864500	4021.154251	24.658624
140.697829	4026.981542	24.663642
140.801374	4033.448520	24.668659
141.253257	4041.654036	24.673677
141.066668	4045.628539	24.678695
141.777035	4059.345723	24.683712
141.434897	4056.741498	24.688730
141.545628	4048.836802	24.693747
141.925124	4065.856477	24.698765
142.008193	4072.446596	24.703783
142.097187	4069.964623	24.708800
142.237676	4076.084986	24.713818
142.789489	4069.358343	24.718835
142.691654	4073.473692	24.723853
142.791744	4089.845663	24.728871
143.176483	4087.620647	24.733888
143.493475	4097.324334	24.738906
143.141271	4087.695766	24.743923
143.319353	4086.828566	24.748941
143.283190	4093.516164	24.753959
143.427695	4084.337365	24.758976
143.649931	4101.413121	24.763994
144.030825	4114.149534	24.769011
144.343929	4105.765112	24.774029
143.855597	4122.967299	24.779047
144.377455	4110.955351	24.784064
144.326716	4128.622828	24.789082
144.929523	4136.647075	24.794099
144.388553	4140.471613	24.799117
144.612469	4139.439460	24.804135
144.980428	4146.622824	24.809152
145.064494	4164.474507	24.814170
145.373149	4149.598241	24.819187
145.471790	4158.183907	24.824205
145.633567	4159.572842	24.829223
146.009876	4164.384530	24.834240
145.399181	4182.590591	24.839258
145.926555	4175.589959	24.844275
146.162034	4174.735913	24.849293
146.150915	4198.249080	24.854311
146.817058	4197.621520	24.859328
146.741393	4206.136500	24.864346
146.952346	4203.240982	24.869363
146.570302	4216.080469	24.874381
146.668111	4233.598667	24.879399
147.057495	4230.009382	24.884416
147.065714	4240.929056	24.889434
147.164936	4247.923890	24.894451
147.407993	4255.221433	24.899469
147.388451	4269.497459	24.904487
147.906481	4277.348745	24.909504
148.317128	4281.905769	24.914522
148.701347	4280.955965	24.919539
148.645627	4284.638701	24.924557
148.527208	4298.062155	24.929575
149.217672	4297.124641	24.934592
148.955561	4308.676677	24.939610
149.361305	4308.932395	24.944627
149.430242	4302.744826	24.949645
149.214654	4307.620299	24.954663
149.286075	4311.002332	24.959680
149.417604	4320.943333	24.964698
149.537763	4321.985252	24.969715
149.856504	4326.502938	24.974733
149.819123	4343.960227	24.979751
150.071977	4352.834452	24.984768
150.179671	4354.648460	24.989786
150.185916	4368.447098	24.994803
150.452727	4374.636273	24.999821
150.628336	4383.431005	25.004839
150.676040	4385.077601	25.009856
151.164481	4397.393459	25.014874
151.579257	4406.532885	25.019891
151.436202	4408.935142	25.024909
151.374428	4408.477719	25.029927
151.768046	4416.534661	25.034944
151.782162	4425.922700	25.039962
152.008647	4422.333488	25.044979
152.138927	4415.321993	25.049997
152.112206	4433.481573	25.055015
152.654115	4436.998699	25.060032
152.652046	4439.420042	25.065050
153.083847	4433.115964	25.070067
153.372197	4435.144892	25.075085
152.969067	4445.020854	25.080103
152.646350	4451.421780	25.085120
153.113601	4455.673338	25.090138
153.682399	4458.867490	25.095155
153.621013	4464.473366	25.100173
153.601681	4469.349890	25.105191
154.189901	4485.014950	25.110208
154.159320	4484.596858	25.115226
154.322851	4493.396682	25.120243
154.234026	4500.644992	25.125261
154.036219	4515.270914	25.130279
154.264153	4513.278580	25.135296
154.138927	4523.846750	25.140314
154.807084	4531.434891	25.145331
154.990816	4543.447932	25.150349
154.989742	4552.642707	25.155367
155.730273	4555.096799	25.160384
155.581333	4565.627653	25.165402
155.437813	4567.458699	25.170419
156.391193	4580.147345	25.175437
156.024261	4581.110452	25.180455
156.702860	4577.233030	25.185472
156.571969	4582.666693	25.190490
156.483699	4585.167760	25.195507
156.625597	4603.459078	25.200525
156.867570	4604.182192	25.205543
156.736086	4602.248963	25.210560
157.191825	4615.861021	25.215578
157.301752	4630.107705	25.220595
157.337776	4632.024434	25.225613
157.639494	4639.827491	25.230631
158.199390	4645.674428	25.235648
158.616567	4651.540431	25.240666
158.223245	4645.197454	25.245683
158.434384	4645.805428	25.250701
158.874385	4649.852954	25.255719
159.192491	4662.299673	25.260736
159.442991	4672.913594	25.265754
159.701033	4669.941230	25.270771
159.603690	4667.923768	25.275789
159.582143	4673.166833	25.280807
159.685575	4660.212780	25.285824
159.959197	4669.481633	25.290842
159.634034	4666.855737	25.295859
159.971674	4668.457218	25.300877
159.952050	4688.456126	25.305895
160.206155	4689.938046	25.310912
160.245559	4695.146377	25.315930
160.523280	4704.771283	25.320947
160.563516	4709.382929	25.325965
160.892783	4715.975985	25.330983
160.778162	4723.499851	25.336000
161.199437	4735.719080	25.341018
161.232750	4738.570539	25.346035
161.435154	4748.743783	25.351053
161.559751	4778.981815	25.356071
161.670335	4766.689418	25.361088
162.018403	4771.818151	25.366106
162.190313	4787.178990	25.371123
163.058812	4776.204755	25.376141
162.998962	4779.588376	25.381159
163.243502	4770.702984	25.386176
163.520453	4771.827836	25.391194
163.524366	4771.906236	25.396211
163.607106	4759.716029	25.401229
163.643963	4774.936907	25.406247
163.730287	4761.991757	25.411264
163.533597	4773.297173	25.416282
163.730411	4781.612180	25.421299
164.036803	4770.252002	25.426317
163.905370	4787.235117	25.431335
164.056212	4792.568165	25.436352
164.428900	4794.432496	25.441370
164.272766	4807.152004	25.446387
164.871605	4806.560156	25.451405
164.905618	4826.187878	25.456423
164.860874	4825.014443	25.461440
165.382747	4836.820369	25.466458
164.928428	4852.168287	25.471475
164.974857	4845.895657	25.476493
165.244475	4868.747328	25.481511
165.174642	4878.410655	25.486528
165.710175	4894.541957	25.491546
165.615449	4904.174452	25.496563
166.240971	4917.577232	25.501581
166.367072	4918.728736	25.506599
166.404125	4941.468354	25.511616
166.720522	4945.812957	25.516634
166.863026	4949.865835	25.521651
167.008178	4958.671902	25.526669
167.282438	4973.101596	25.531687
167.989687	4956.477071	25.536704
168.273187	4951.786750	25.541722
168.266254	4944.692251	25.546739
169.214852	4948.685912	25.551757
168.996753	4944.641847	25.556775
169.299798	4939.563400	25.561792
169.538875	4938.200573	25.566810
169.134045	4941.786286	25.571827
169.292956	4938.472635	25.576845
169.445163	4956.690107	25.581863
169.662845	4961.555114	25.586880
169.837835	4964.996900	25.591898
169.687665	4972.835735	25.596915
169.989010	4959.187802	25.601933
169.953629	4977.772239	25.606951
170.345530	4986.561999	25.611968
170.529184	4991.277646	25.616986
170.838898	4992.965573	25.622003
170.925232	4991.127804	25.627021
170.682899	5002.191108	25.632039
171.008853	5001.761685	25.637056
171.356108	5012.183981	25.642074
171.144450	5011.715157	25.647091
171.505037	5021.131630	25.652109
171.863547	5035.772365	25.657127
171.979697	5050.633920	25.662144
171.661492	5043.243790	25.667162
171.747681	5062.649004	25.672180
172.121288	5066.766934	25.677197
172.251623	5081.695748	25.682215
172.563975	5096.286902	25.687232
172.802318	5088.062022	25.692250
172.872217	5103.697841	25.697268
173.227559	5115.914967	25.702285
173.462850	5119.139068	25.707303
173.575987	5124.632750	25.712320
174.058310	5137.543484	25.717338
173.740757	5134.616469	25.722356
174.252250	5129.600211	25.727373
174.711412	5127.470803	25.732391
174.767800	5128.652113	25.737408
174.872818	5133.279033	25.742426
175.092107	5146.274915	25.747444
175.145054	5147.068516	25.752461
175.447657	5145.888329	25.757479
175.400675	5151.751004	25.762496
175.642777	5152.477278	25.767514
175.571527	5151.071212	25.772532
175.964187	5165.208012	25.777549
175.994508	5167.633879	25.782567
175.503232	5179.446257	25.787584
176.109584	5187.419920	25.792602
176.271765	5197.249309	25.797620
176.262667	5195.337995	25.802637
176.532912	5214.831507	25.807655
176.905356	5226.638859	25.812672
176.915632	5240.077693	25.817690
177.000831	5255.480837	25.822708
176.989862	5252.821720	25.827725
177.718079	5253.131413	25.832743
177.871741	5258.833469	25.837760
178.220159	5266.313877	25.842778
178.441850	5282.424945	25.847796
178.661740	5284.603515	25.852813
178.820293	5284.373757	25.857831
178.400067	5287.494772	25.862848
179.371992	5302.453722	25.867866
179.373424	5311.127668	25.872884
179.329804	5311.121932	25.877901
179.466918	5320.841657	25.882919
179.607619	5330.014753	25.887936
180.149501	5339.516800	25.892954
180.085440	5337.841298	25.897972
180.264286	5340.218812	25.902989
180.499546	5350.579826	25.908007
180.839375	5357.499750	25.913024
181.006133	5359.251003	25.918042
180.812656	5380.559284	25.923060
181.310408	5385.743801	25.928077
181.625842	5382.440422	25.933095
181.470522	5376.827166	25.938112
181.570045	5386.679039	25.943130
181.900632	5403.748624	25.948148
181.890687	5418.286051	25.953165
182.116503	5424.873378	25.958183
182.020663	5440.781500	25.963200
182.402387	5453.723904	25.968218
182.513297	5455.985749	25.973236
183.100742	5467.605115	25.978253
183.345432	5479.426208	25.983271
183.294096	5495.491589	25.988288
183.626567	5495.755579	25.993306
183.613091	5505.593544	25.998324
183.985428	5516.362601	26.003341
184.002026	5521.432675	26.008359
184.188646	5534.998942	26.013376
184.360423	5532.705900	26.018394
184.363381	5545.385373	26.023412
184.657578	5561.687418	26.028429
184.929565	5566.600951	26.033447
184.854529	5572.332399	26.038464
185.020714	5581.864657	26.043482
185.477875	5598.330756	26.048500
185.568127	5605.561096	26.053517
185.950257	5623.052153	26.058535
186.115646	5629.475352	26.063552
186.545004	5633.127031	26.068570
187.013197	5642.931114	26.073588
186.847729	5634.510020	26.078605
187.277299	5641.163556	26.083623
186.721370	5641.736318	26.088640
187.104568	5639.561862	26.093658
187.190927	5655.006199	26.098676
187.678992	5663.560357	26.103693
187.936174	5662.384053	26.108711
187.388425	5676.743421	26.113728
187.792567	5679.085904	26.118746
187.969879	5694.809675	26.123764
188.290334	5712.708149	26.128781
188.762913	5716.100590	26.133799
188.671537	5727.778460	26.138816
188.849219	5738.060275	26.143834
188.957278	5746.673636	26.148852
189.433569	5760.823132	26.153869
189.739645	5760.867119	26.158887
189.586829	5773.754085	26.163904
189.888256	5780.531790	26.168922
190.215238	5792.223481	26.173940
190.457031	5792.965613	26.178957
190.913940	5799.697023	26.183975
191.231097	5814.578412	26.188992
191.162456	5819.702876	26.194010
191.099515	5830.533574	26.199028
191.317212	5844.398267	26.204045
191.837388	5847.770696	26.209063
191.794267	5852.319852	26.214080
191.860761	5845.058896	26.219098
191.847743	5866.809982	26.224116
192.053235	5870.660707	26.229133
192.683413	5878.346872	26.234151
192.387410	5893.200681	26.239168
193.256981	5895.110877	26.244186
193.675376	5912.808061	26.249204
193.514251	5915.576338	26.254221
193.997566	5918.695678	26.259239
193.918353	5929.563690	26.264256
194.023999	5919.487226	26.269274
194.227591	5942.536768	26.274292
194.412321	5949.212754	26.279309
194.663625	5946.979881	26.284327
194.481150	5960.155690	26.289344
194.739630	5966.665526	26.294362
195.092228	5972.478882	26.299380
195.174991	5985.499777	26.304397
195.226421	5984.847918	26.309415
195.000775	5994.340385	26.314432
195.701137	6014.146584	26.319450
195.893270	6019.489347	26.324468
196.243469	6032.456012	26.329485
196.125375	6027.209241	26.334503
196.596048	6054.769200	26.339520
197.056105	6055.663603	26.344538
197.264520	6068.860706	26.349556
197.266884	6069.043522	26.354573
197.663685	6086.965201	26.359591
197.656663	6086.246680	26.364608
198.087003	6087.344580	26.369626
197.982589	6096.647766	26.374644
198.147256	6110.524074	26.379661
198.391213	6114.441465	26.384679
198.559014	6132.102117	26.389696
199.007689	6132.458509	26.394714
199.425010	6143.135705	26.399732
199.004777	6144.896350	26.404749
199.492119	6150.467819	26.409767
199.217539	6173.134384	26.414784
199.271443	6169.461218	26.419802
199.946175	6185.385755	26.424820
200.371035	6193.820582	26.429837
200.146474	6187.015170	26.434855
200.268365	6215.450404	26.439872
199.978069	6223.785090	26.444890
200.620249	6241.735008	26.449908
200.407411	6248.693967	26.454925
200.739153	6259.457158	26.459943
200.799741	6275.777274	26.464960
201.541331	6287.802474	26.469978
201.565025	6301.138987	26.474996
201.583734	6319.100819	26.480013
202.337269	6325.634723	26.485031
202.381711	6350.723519	26.490048
203.141687	6348.872280	26.495066
203.240760	6352.591311	26.500084
203.474150	6352.207839	26.505101
203.753244	6361.138940	26.510119
203.802227	6364.957316	26.515136
204.093574	6366.919708	26.520154
204.030515	6368.356447	26.525172
204.301746	6397.292723	26.530189
204.479381	6396.791663	26.535207
204.042979	6399.647064	26.540224
204.624211	6418.695704	26.545242
205.175490	6421.738261	26.550260
205.147054	6435.831126	26.555277
205.598748	6441.730218	26.560295
205.611297	6449.771635	26.565312
205.847212	6453.968141	26.570330
205.980954	6463.414367	26.575348
206.256289	6477.946103	26.580365
206.370727	6481.091404	26.585383
206.639080	6494.620408	26.590400
206.748927	6499.464737	26.595418
207.079445	6513.340784	26.600436
207.057506	6526.842402	26.605453
207.759087	6543.018766	26.610471
207.995303	6538.063926	26.615488
208.146133	6540.922624	26.620506
208.511083	6547.103577	26.625524
208.215134	6565.862782	26.630541
209.170241	6560.445616	26.635559
208.999563	6568.821813	26.640576
209.591507	6574.604413	26.645594
209.685164	6581.891430	26.650612
209.581305	6593.922192	26.655629
209.735433	6592.114745	26.660647
209.808391	6607.865021	26.665664
210.109338	6618.020813	26.670682
210.281901	6613.773499	26.675700
210.572155	6635.692942	26.680717
211.063502	6644.433300	26.685735
210.768059	6643.567100	26.690752
211.027315	6656.696735	26.695770
211.273343	6660.355069	26.700788
211.540515	6664.070090	26.705805
211.849032	6684.752463	26.710823
211.641703	6689.864038	26.715840
212.140693	6712.196175	26.720858
212.248624	6713.820979	26.725876
212.427398	6739.927964	26.730893
212.662934	6735.702385	26.735911
212.769120	6750.655266	26.740928
213.025984	6760.874823	26.745946
213.293859	6773.239265	26.750964
213.392080	6781.239078	26.755981
213.862951	6792.451280	26.760999
213.597142	6805.236606	26.766016
214.039269	6804.006183	26.771034
214.443431	6829.090138	26.776052
214.631084	6832.738655	26.781069
214.651662	6839.907725	26.786087
214.814059	6849.371787	26.791104
214.900814	6846.728791	26.796122
215.334386	6860.260754	26.801140
215.278291	6877.701286	26.806157
215.681255	6892.570196	26.811175
216.038894	6902.493189	26.816192
216.185424	6912.041831	26.821210
216.636045	6923.348813	26.826228
216.460342	6932.136339	26.831245
216.606605	6948.636280	26.836263
217.528583	6953.742574	26.841280
217.211601	6964.711355	26.846298
217.674869	6968.907308	26.851316
217.570582	6985.421035	26.856333
218.104838	6996.494066	26.861351
218.281201	7010.325042	26.866368
218.515155	7032.376839	26.871386
218.608752	7033.590362	26.876404
218.602853	7047.304529	26.881421
218.832335	7063.756892	26.886439
219.111682	7078.430537	26.891456
219.242517	7081.093554	26.896474
219.540925	7094.217408	26.901492
219.987236	7109.881576	26.906509
220.304352	7114.251845	26.911527
221.082501	7143.353455	26.916544
221.147442	7141.569310	26.921562
221.477797	7140.211054	26.926580
221.116877	7141.302781	26.931597
221.351624	7160.920702	26.936615
221.828943	7167.617875	26.941632
221.788399	7178.546901	26.946650
222.384715	7185.077183	26.951668
222.258373	7192.016719	26.956685
222.476445	7213.973346	26.961703
222.789226	7218.252766	26.966720
222.935712	7236.669129	26.971738
223.548850	7231.162954	26.976756
223.560243	7237.241345	26.981773
223.668536	7240.293029	26.986791
224.315113	7250.467970	26.991808
224.201687	7253.816193	26.996826
224.671333	7269.884099	27.001844
224.885954	7277.790242	27.006861
224.786737	7277.742652	27.011879
225.145275	7291.463399	27.016896
225.563549	7297.784678	27.021914
225.653011	7304.065602	27.026932
225.743776	7311.378615	27.031949
226.011415	7328.103077	27.036967
226.298144	7334.236496	27.041984
226.593085	7343.623355	27.047002
226.664857	7343.154537	27.052020
226.803873	7358.765742	27.057037
227.033855	7371.458487	27.062055
227.194143	7383.022465	27.067072
227.136093	7402.443152	27.072090
227.651381	7406.804735	27.077108
227.756251	7424.406981	27.082125
228.024159	7438.246125	27.087143
228.391458	7446.860966	27.092160
228.247482	7458.904853	27.097178
228.493095	7454.027226	27.102196
228.620292	7482.798229	27.107213
228.899619	7486.634645	27.112231
229.466600	7502.043597	27.117248
229.801235	7517.390872	27.122266
230.039912	7522.325905	27.127284
230.011193	7543.611050	27.132301
230.048478	7560.358961	27.137319
230.431518	7556.751079	27.142336
230.179153	7574.469066	27.147354
230.926164	7588.716738	27.152372
231.173495	7587.469240	27.157389
231.508327	7608.416895	27.162407
232.094507	7611.324789	27.167424
232.009960	7629.196645	27.172442
232.618973	7632.426148	27.177460
232.667018	7643.483718	27.182477
232.690709	7657.904037	27.187495
232.962024	7659.809709	27.192512
232.868797	7679.854918	27.197530
233.716940	7679.865033	27.202548
233.785332	7697.924658	27.207565
233.667854	7693.109811	27.212583
234.103682	7713.767212	27.217600
234.434115	7723.631748	27.222618
234.937111	7739.142412	27.227636
235.113913	7746.353810	27.232653
235.247302	7742.860527	27.237671
235.854662	7745.780929	27.242688
236.345900	7757.009495	27.247706
236.641730	7759.517490	27.252724
236.820437	7761.424962	27.257741
236.633727	7751.124671	27.262759
236.889467	7755.529904	27.267776
237.089989	7773.695310	27.272794
237.306624	7777.175343	27.277812
237.618971	7783.226001	27.282829
237.493028	7797.262482	27.287847
238.047936	7804.787554	27.292864
237.711284	7813.319592	27.297882
238.428799	7822.239976	27.302900
238.376898	7840.690988	27.307917
238.201793	7856.158947	27.312935
238.676391	7862.607401	27.317952
239.022113	7885.971897	27.322970
239.235930	7901.294106	27.327988
239.196087	7913.811406	27.333005
239.554030	7930.487632	27.338023
240.145943	7931.390018	27.343040
240.377695	7958.115565	27.348058
240.634082	7962.735422	27.353076
241.375292	7970.487271	27.358093
241.091259	7976.438267	27.363111
241.500929	7987.632320	27.368128
241.475859	7996.482139	27.373146
241.984440	8009.845427	27.378164
241.848954	8025.206336	27.383181
241.936714	8041.968925	27.388199
242.531870	8050.517006	27.393216
242.912986	8064.708364	27.398234
243.113712	8070.931187	27.403252
243.374091	8076.342853	27.408269
243.156588	8095.104029	27.413287
243.839893	8098.691417	27.418304
243.889486	8127.191381	27.423322
244.274554	8135.197639	27.428340
244.734385	8132.281700	27.433357
244.439233	8153.615344	27.438375
244.695340	8152.603217	27.443392
245.107746	8170.960173	27.448410
245.150422	8172.869925	27.453428
245.728855	8186.007790	27.458445
245.695281	8204.380544	27.463463
245.890787	8200.725968	27.468480
246.120807	8231.357392	27.473498
246.735090	8225.206717	27.478516
247.365591	8238.175506	27.483533
247.615763	8240.056118	27.488551
247.914067	8241.288363	27.493568
247.660825	8250.663165	27.498586
248.018943	8253.546686	27.503604
248.524581	8267.911392	27.508621
248.438224	8274.630432	27.513639
248.399709	8284.915768	27.518656
248.683838	8297.600724	27.523674
249.021535	8315.663226	27.528692
249.500056	8319.882374	27.533709
249.519871	8335.857082	27.538727
250.153652	8344.850743	27.543744
250.152000	8367.183914	27.548762
250.265117	8375.377839	27.553780
250.564930	8386.860743	27.558797
250.909529	8398.399822	27.563815
250.899741	8403.421131	27.568832
250.976394	8431.068109	27.573850
251.273859	8443.400658	27.578868
251.761590	8459.372079	27.583885
251.823007	8463.586744	27.588903
252.167658	8479.731997	27.593920
252.044364	8505.348662	27.598938
252.617472	8505.436331	27.603956
253.202202	8530.197736	27.608973
253.563653	8543.549591	27.613991
253.827547	8549.661716	27.619008
253.898495	8556.637347	27.624026
254.178827	8574.579593	27.629044
254.663744	8575.874364	27.634061
254.946174	8585.131210	27.639079
255.112523	8599.596354	27.644096
255.162242	8608.387467	27.649114
255.543073	8629.404894	27.654132
255.525885	8643.665023	27.659149
256.171768	8662.718563	27.664167
256.621567	8667.946216	27.669184
256.899439	8678.624504	27.674202
256.751787	8696.052598	27.679220
257.085998	8691.811212	27.684237
257.016036	8709.798656	27.689255
257.446230	8722.795815	27.694272
257.728755	8741.924949	27.699290
257.935706	8754.978987	27.704308
258.343164	8765.536125	27.709325
258.627623	8773.100545	27.714343
259.274738	8787.573072	27.719360
259.195917	8800.816860	27.724378
259.300135	8808.851350	27.729396
259.734936	8822.911808	27.734413
259.875758	8836.244553	27.739431
260.289805	8846.039847	27.744448
260.326092	8854.530086	27.749466
260.543226	8869.044362	27.754484
260.685759	8874.035771	27.759501
260.971866	8906.762223	27.764519
261.112914	8908.306296	27.769536
261.532285	8932.487818	27.774554
261.435247	8940.449513	27.779572
262.267682	8941.753350	27.784589
262.463231	8962.648460	27.789607
262.756013	8965.343367	27.794624
263.124509	8987.745946	27.799642
263.182177	8987.061440	27.804660
263.485974	8992.971758	27.809677
263.721589	9008.607208	27.814695
264.289172	9012.970509	27.819712
264.322565	9021.047689	27.824730
264.557653	9035.385659	27.829748
264.859338	9039.534634	27.834765
265.245148	9054.698425	27.839783
265.796224	9066.414149	27.844800
265.606273	9072.590791	27.849818
265.949393	9079.012788	27.854836
265.964245	9082.672870	27.859853
266.076403	9105.424901	27.864871
266.508829	9116.139368	27.869888
266.821870	9133.092032	27.874906
266.933978	9142.896606	27.879924
267.552413	9148.470688	27.884941
267.776137	9164.155478	27.889959
268.437383	9186.582178	27.894976
268.393615	9191.962595	27.899994
268.976760	9202.880963	27.905012
268.932980	9209.783144	27.910029
268.800063	9228.955361	27.915047
269.783438	9230.504081	27.920064
270.001740	9246.556017	27.925082
269.920778	9257.653583	27.930100
270.335992	9263.874989	27.935117
270.480331	9281.100314	27.940135
270.756535	9294.942719	27.945152
270.977389	9300.329327	27.950170
271.124289	9310.081216	27.955188
271.625966	9316.447038	27.960205
271.868109	9337.445819	27.965223
272.004987	9348.632655	27.970240
272.049011	9366.041008	27.975258
272.054788	9378.223846	27.980276
272.580752	9392.497864	27.985293
272.954837	9420.661997	27.990311
273.002450	9433.460329	27.995328
273.601343	9453.557568	28.000346
273.978327	9460.094399	28.005364
274.547957	9459.355428	28.010381
275.039165	9479.832541	28.015399
275.470199	9486.525142	28.020416
275.748623	9488.669849	28.025434
275.846313	9504.001997	28.030452
276.307792	9504.574324	28.035469
276.155521	9513.883527	28.040487
276.601691	9519.405610	28.045504
276.672198	9527.493020	28.050522
276.524515	9543.883186	28.055540
277.128842	9562.975699	28.060557
277.290296	9567.373947	28.065575
277.524605	9592.503899	28.070592
277.651992	9602.783081	28.075610
278.258397	9616.656408	28.080628
278.415363	9623.830585	28.085645
278.387567	9647.110229	28.090663
278.798483	9665.386816	28.095680
279.290359	9672.142630	28.100698
279.318031	9687.602648	28.105716
280.069541	9694.741121	28.110733
279.825590	9719.251107	28.115751
280.208722	9730.633472	28.120768
280.490807	9750.284666	28.125786
280.501484	9777.486122	28.130804
280.924512	9774.970320	28.135821
281.118867	9793.587005	28.140839
281.393629	9801.787968	28.145856
281.745098	9814.034093	28.150874
282.217197	9835.540689	28.155892
283.277636	9830.504010	28.160909
283.235491	9842.688300	28.165927
283.537479	9859.769642	28.170944
284.086201	9855.548272	28.175962
283.991300	9852.582671	28.180980
284.631083	9872.052014	28.185997
284.379249	9890.921384	28.191015
284.802075	9896.958696	28.196032
284.968604	9912.829833	28.201050
285.086383	9922.652881	28.206068
285.460676	9937.613965	28.211085
285.685412	9956.238712	28.216103
285.672962	9970.647517	28.221120
286.319189	9980.663009	28.226138
286.251098	10007.725513	28.231156
286.620496	10012.157797	28.236173
286.955211	10031.829511	28.241191
286.830184	10045.040334	28.246208
287.465027	10061.359645	28.251226
287.781464	10087.424677	28.256244
288.355780	10098.790133	28.261261
288.549830	10116.106371	28.266279
288.980999	10130.506223	28.271296
289.089653	10146.604425	28.276314
289.530855	10165.760844	28.281332
289.892978	10169.777530	28.286349
289.670785	10189.472967	28.291367
290.122756	10202.710893	28.296384
290.499723	10224.539013	28.301402
290.304711	10241.003465	28.306420
290.847930	10253.816766	28.311437
291.262656	10282.288457	28.316455
291.605465	10294.346806	28.321472
291.792243	10314.660693	28.326490
292.234216	10335.067481	28.331508
292.771157	10344.617109	28.336525
292.878668	10367.071458	28.341543
293.184888	10386.416460	28.346560
293.941004	10384.025535	28.351578
293.811989	10411.622234	28.356596
294.609660	10412.988430	28.361613
294.725576	10429.332022	28.366631
294.646304	10443.451644	28.371648
295.587857	10453.601386	28.376666
295.672600	10468.961604	28.381684
295.698506	10477.902550	28.386701
296.050176	10493.650637	28.391719
296.333925	10513.232916	28.396736
296.364677	10519.757721	28.401754
296.689434	10545.260082	28.406772
296.980613	10563.035224	28.411789
297.100506	10572.498341	28.416807
297.501534	10581.750353	28.421824
298.106358	10604.048629	28.426842
298.231465	10618.916445	28.431860
298.252782	10629.121143	28.436877
298.726943	10654.505671	28.441895
299.058201	10668.511032	28.446912
299.563422	10689.119909	28.451930
299.255783	10704.453001	28.456948
299.876924	10716.809294	28.461965
300.267632	10737.511831	28.466983
300.135456	10740.825711	28.472000
300.616564	10767.090235	28.477018
301.010387	10780.069244	28.482036
301.553970	10790.505308	28.487053
301.583399	10807.380515	28.492071
301.763344	10834.320352	28.497088
302.007208	10847.464839	28.502106
302.262005	10877.897857	28.507124
302.429881	10883.403684	28.512141
302.838231	10900.286290	28.517159
303.418931	10919.731199	28.522176
304.061795	10933.814545	28.527194
304.315373	10957.490906	28.532212
304.712756	10970.854705	28.537229
305.029871	10988.348357	28.542247
304.962026	11010.628703	28.547264
305.609293	11012.491984	28.552282
306.236162	11012.792332	28.557300
306.400051	11034.837708	28.562317
306.552640	11039.900757	28.567335
306.931485	11059.752979	28.572352
307.105495	11067.120823	28.577370
307.002863	11081.304556	28.582388
307.553885	11089.308362	28.587405
308.029637	11116.050993	28.592423
308.282269	11129.434284	28.597440
308.768962	11146.068104	28.602458
308.591461	11159.568901	28.607476
309.088011	11181.736323	28.612493
309.476943	11207.744272	28.617511
309.600736	11217.980700	28.622528
310.457613	11231.162637	28.627546
310.595804	11249.836883	28.632564
310.649640	11256.844610	28.637581
311.192146	11269.276664	28.642599
311.657093	11289.403059	28.647616
312.158993	11303.028687	28.652634
312.323063	11321.086415	28.657652
312.710057	11331.723984	28.662669
312.913693	11345.541325	28.667687
313.055118	11366.523342	28.672704
313.243315	11369.067536	28.677722
313.623472	11384.824572	28.682740
313.955762	11401.526863	28.687757
314.508139	11420.768306	28.692775
314.355429	11437.100922	28.697792
315.025482	11449.519554	28.702810
315.179418	11464.740359	28.707828
315.068700	11481.180148	28.712845
315.434233	11499.017229	28.717863
315.463964	11528.987450	28.722880
315.976416	11545.279756	28.727898
316.461646	11574.295017	28.732916
316.682713	11587.279380	28.737933
317.240948	11608.089420	28.742951
317.125386	11626.939324	28.747968
317.555887	11655.218040	28.752986
318.020744	11677.056280	28.758004
318.494054	11695.255680	28.763021
318.868861	11707.183659	28.768039
319.476526	11734.639200	28.773056
319.918737	11742.931782	28.778074
320.305240	11765.925376	28.783092
320.364173	11771.517894	28.788109
320.738748	11786.272018	28.793127
320.810854	11799.112366	28.798144
321.477836	11817.076488	28.803162
321.526424	11825.812460	28.808180
321.594605	11855.493031	28.813197
322.132283	11857.957623	28.818215
322.108215	11887.254746	28.823232
322.620600	11897.298428	28.828250
323.080110	11920.653445	28.833268
323.289633	11930.636937	28.838285
323.672040	11930.808008	28.843303
323.550016	11954.443062	28.848320
323.727695	11973.762355	28.853338
324.229654	11998.247611	28.858356
324.554004	12018.886116	28.863373
324.942267	12035.596047	28.868391
325.147776	12055.965748	28.873408
325.903874	12074.620401	28.878426
326.745278	12085.516051	28.883444
326.975273	12099.715079	28.888461
327.546331	12106.708911	28.893479
327.474078	12123.241160	28.898496
327.685697	12130.110973	28.903514
328.099345	12152.557696	28.908532
328.281812	12174.936234	28.913549
328.754630	12192.460452	28.918567
329.217495	12200.791073	28.923584
329.533086	12217.992448	28.928602
329.980646	12236.606882	28.933620
330.185691	12248.927927	28.938637
330.510273	12262.275565	28.943655
330.520277	12274.143865	28.948672
331.145633	12295.395770	28.953690
331.520772	12311.845902	28.958708
331.886357	12323.011546	28.963725
332.289694	12337.850042	28.968743
332.329326	12357.229114	28.973760
332.686883	12374.610404	28.978778
333.054044	12385.409546	28.983796
333.276220	12412.907149	28.988813
333.377963	12417.631139	28.993831
333.809692	12445.456146	28.998848
333.968056	12469.187133	29.003866
334.297611	12482.872030	29.008884
334.638594	12514.576324	29.013901
335.000748	12528.549848	29.018919
335.491575	12560.594031	29.023936
335.750730	12578.341338	29.028954
336.044427	12604.899711	29.033972
336.403074	12629.316527	29.038989
336.822504	12643.874878	29.044007
336.877932	12668.901032	29.049024
337.575786	12685.797019	29.054042
338.108929	12700.205084	29.059060
338.197165	12727.452431	29.064077
338.823597	12728.842313	29.069095
339.250613	12764.193487	29.074112
339.470177	12764.187823	29.079130
339.869433	12790.647922	29.084148
340.302205	12799.510844	29.089165
340.638221	12814.849654	29.094183
340.868272	12834.107995	29.099200
341.176924	12839.118814	29.104218
341.616094	12866.438040	29.109236
341.881434	12884.456242	29.114253
342.305562	12899.917189	29.119271
342.802574	12926.693829	29.124288
342.929557	12934.874969	29.129306
343.162862	12946.560511	29.134324
343.304214	12969.022181	29.139341
343.890173	12971.994130	29.144359
343.827752	12998.169564	29.149376
344.026981	13015.089791	29.154394
344.183941	13036.724922	29.159412
344.486163	13054.608075	29.164429
345.077633	13069.035763	29.169447
345.641737	13102.458903	29.174464
345.615601	13122.407936	29.179482
346.609268	13146.758140	29.184500
346.213594	13169.799435	29.189517
347.055557	13185.321880	29.194535
347.785009	13204.799689	29.199552
347.800610	13226.450729	29.204570
348.174094	13241.784053	29.209588
348.250346	13261.549926	29.214605
348.694380	13278.533330	29.219623
348.983901	13304.711237	29.224640
349.194006	13321.506890	29.229658
349.826439	13349.917770	29.234676
349.553496	13371.888633	29.239693
350.687534	13392.901534	29.244711
350.387372	13425.648222	29.249728
350.616655	13451.390450	29.254746
351.018607	13473.790044	29.259764
351.439720	13500.029840	29.264781
352.017334	13522.095828	29.269799
352.662290	13554.373494	29.274816
353.260637	13572.220510	29.279834
353.714624	13583.016296	29.284852
354.031570	13608.293508	29.289869
354.799344	13625.874196	29.294887
354.982913	13641.395308	29.299904
354.958794	13652.170830	29.304922
355.619404	13669.424029	29.309940
355.826090	13689.650047	29.314957
356.418422	13695.576942	29.319975
356.854442	13718.994692	29.324992
356.965872	13738.613480	29.330010
357.594038	13748.643288	29.335028
357.502016	13767.024288	29.340045
358.072923	13790.556919	29.345063
358.218496	13813.587365	29.350080
358.588083	13826.913316	29.355098
359.129197	13835.772492	29.360116
359.262861	13861.861749	29.365133
360.116463	13874.127099	29.370151
360.019750	13895.682703	29.375168
359.955998	13915.736323	29.380186
360.764211	13928.896164	29.385204
360.943075	13953.623742	29.390221
361.552353	13986.261393	29.395239
361.739384	14001.504359	29.400256
362.261597	14030.419751	29.405274
362.513978	14055.796036	29.410292
362.445153	14077.006441	29.415309
362.935603	14098.180328	29.420327
363.306009	14121.870905	29.425344
363.495067	14146.120289	29.430362
364.271404	14160.993735	29.435380
364.495060	14187.107325	29.440397
364.896866	14196.162049	29.445415
365.599160	14226.218169	29.450432
366.159302	14238.583130	29.455450
366.791394	14248.742072	29.460468
366.734337	14273.809967	29.465485
367.258611	14288.571169	29.470503
367.641605	14312.572670	29.475520
367.741888	14325.817736	29.480538
368.284471	14333.716875	29.485556
368.148062	14354.180183	29.490573
368.582137	14371.055588	29.495591
368.729185	14393.723334	29.500608
369.200588	14418.990213	29.505626
369.295189	14430.973017	29.510644
369.559739	14454.292050	29.515661
370.424567	14482.084211	29.520679
370.836913	14505.184497	29.525696
370.994861	14531.311948	29.530714
371.509116	14547.300243	29.535732
371.930325	14571.517186	29.540749
372.322391	14590.022577	29.545767
372.891996	14616.250277	29.550784
372.871800	14634.586194	29.555802
373.590780	14638.823045	29.560820
373.739709	14662.444560	29.565837
374.379292	14676.294374	29.570855
374.523607	14702.297859	29.575872
374.784594	14720.129002	29.580890
375.384814	14742.290795	29.585908
375.561117	14768.317813	29.590925
376.237561	14782.945177	29.595943
376.753690	14812.121673	29.600960
377.332910	14827.067387	29.605978
377.451387	14839.252009	29.610996
377.611490	14870.928407	29.616013
378.488578	14884.119247	29.621031
378.363155	14897.150357	29.626048
378.402331	14930.522646	29.631066
378.978668	14945.892092	29.636084
379.507094	14965.260898	29.641101
379.372860	15003.189084	29.646119
380.028529	15022.364440	29.651136
380.360131	15056.092508	29.656154
381.036197	15068.942111	29.661172
381.498125	15098.238020	29.666189
381.773975	15120.397064	29.671207
382.457288	15137.812293	29.676224
382.353595	15162.604382	29.681242
382.826995	15174.743438	29.686260
383.395879	15208.472733	29.691277
383.588625	15224.960114	29.696295
384.181989	15243.340057	29.701312
384.418771	15267.011808	29.706330
385.081893	15285.440937	29.711348
385.210799	15307.604126	29.716365
385.745256	15341.487452	29.721383
386.205105	15365.762555	29.726400
386.347794	15388.615340	29.731418
387.452767	15399.061319	29.736436
388.123299	15427.311473	29.741453
388.341445	15430.041050	29.746471
389.135121	15450.897633	29.751488
389.053339	15454.337133	29.756506
389.439867	15465.153972	29.761524
389.447247	15486.774125	29.766541
389.962288	15506.215046	29.771559
390.213100	15524.746495	29.776576
390.472334	15548.910944	29.781594
390.886666	15562.136402	29.786612
391.187345	15583.470977	29.791629
391.046741	15608.439935	29.796647
391.722285	15634.181967	29.801664
391.835284	15656.057478	29.806682
392.981510	15676.752043	29.811700
393.505740	15696.457022	29.816717
393.809626	15715.454132	29.821735
394.324827	15737.810343	29.826752
394.513384	15752.211217	29.831770
395.105610	15767.796775	29.836788
394.921351	15783.525338	29.841805
395.232332	15798.611483	29.846823
395.591736	15825.170452	29.851840
395.909327	15864.287001	29.856858
396.196916	15877.140781	29.861876
396.635280	15902.051570	29.866893
397.053579	15925.351625	29.871911
397.435079	15954.178150	29.876928
397.779183	15992.722339	29.881946
398.290220	16014.223619	29.886964
399.019877	16030.691275	29.891981
398.794401	16061.845386	29.896999
399.613956	16085.190550	29.902016
399.929003	16109.501776	29.907034
400.231196	16126.339262	29.912052
400.839836	16162.009585	29.917069
401.212020	16181.012317	29.922087
401.639593	16200.555997	29.927104
401.668854	16234.077388	29.932122
402.425996	16261.108802	29.937140
402.972114	16283.331345	29.942157
403.234986	16312.457972	29.947175
403.778353	16329.270723	29.952192
404.350314	16360.825462	29.957210
404.572384	16379.722268	29.962228
404.765735	16402.325181	29.967245
405.398495	16425.535606	29.972263
406.063520	16439.237460	29.977280
406.538216	16473.953278	29.982298
407.350092	16485.964674	29.987316
407.911053	16505.503692	29.992333
407.617922	16521.878329	29.997351
408.669871	16538.002517	30.002368
408.639709	16557.213546	30.007386
409.257397	16567.565481	30.012404
409.396073	16591.415223	30.017421
409.413433	16619.626698	30.022439
409.851215	16629.921398	30.027456
410.053651	16656.629135	30.032474
410.859659	16686.189753	30.037492
411.511012	16711.861202	30.042509
411.529306	16747.409748	30.047527
412.116964	16762.819958	30.052544
412.385757	16798.755990	30.057562
412.336681	16817.044799	30.062580
413.286663	16841.482356	30.067597
413.695058	16867.539266	30.072615
414.467781	16888.770223	30.077632
414.905743	16905.366165	30.082650
415.527100	16932.612333	30.087668
415.900920	16949.900528	30.092685
416.126650	16964.287049	30.097703
416.576607	16985.375695	30.102720
417.100121	17001.936293	30.107738
417.196483	17020.723803	30.112756
417.495513	17051.008240	30.117773
417.655796	17086.465820	30.122791
418.341009	17106.336699	30.127808
418.418586	17134.650101	30.132826
418.732405	17160.409441	30.137844
419.507082	17192.973136	30.142861
419.700327	17229.307071	30.147879
420.206351	17247.039253	30.152896
420.432079	17291.627767	30.157914
420.872354	17316.258988	30.162932
421.240629	17344.015760	30.167949
421.682325	17363.880596	30.172967
421.844835	17394.891181	30.177984
422.308830	17416.834079	30.183002
422.820677	17453.548397	30.188020
423.318891	17472.359068	30.193037
423.401407	17497.649500	30.198055
424.020809	17526.078114	30.203072
424.653296	17561.741008	30.208090
424.816712	17591.159849	30.213108
425.805592	17608.795083	30.218125
425.994869	17637.022344	30.223143
426.239920	17665.462064	30.228160
426.421358	17700.374203	30.233178
426.967115	17734.806435	30.238196
427.120367	17765.288411	30.243213
427.357154	17797.842111	30.248231
428.328770	17827.122856	30.253248
428.994476	17862.749549	30.258266
429.543089	17886.347557	30.263284
430.066843	17908.066925	30.268301
430.456877	17931.095854	30.273319
431.116600	17953.868039	30.278336
431.375272	17983.342138	30.283354
431.930689	18009.188186	30.288372
432.376252	18031.861141	30.293389
432.862853	18062.601237	30.298407
433.600875	18077.382634	30.303424
434.081385	18101.894883	30.308442
434.544272	18120.762224	30.313460
434.991470	18138.892900	30.318477
435.243218	18159.315625	30.323495
435.594185	18170.360635	30.328512
435.935868	18192.696181	30.333530
436.232880	18222.796409	30.338548
436.873799	18245.319172	30.343565
436.970461	18273.163786	30.348583
437.596899	18298.531681	30.353600
437.992308	18331.825987	30.358618
438.089959	18351.483230	30.363636
439.168934	18371.922697	30.368653
439.443736	18403.631283	30.373671
440.229975	18421.166146	30.378688
440.282171	18445.663384	30.383706
440.861597	18477.931141	30.388724
441.646875	18487.765265	30.393741
442.055814	18517.140974	30.398759
442.797702	18531.757864	30.403776
443.005947	18546.066161	30.408794
443.753729	18567.315490	30.413812
444.166021	18586.355417	30.418829
443.887419	18607.606641	30.423847
444.465122	18626.854603	30.428864
444.933358	18653.277341	30.433882
445.445852	18675.334152	30.438900
445.987039	18702.958561	30.443917
445.934518	18724.699069	30.448935
446.733862	18745.839486	30.453952
447.231407	18779.175519	30.458970
447.603703	18796.642497	30.463988
447.719329	18813.978875	30.469005
447.955431	18848.385487	30.474023
448.379731	18876.830670	30.479040
448.366769	18912.381742	30.484058
449.109767	18949.021851	30.489076
449.376888	18978.780440	30.494093
449.836755	19005.047020	30.499111
450.894317	19026.690860	30.504128
452.098011	19038.949267	30.509146
452.346899	19064.067378	30.514164
452.603631	19077.566181	30.519181
452.751774	19110.603390	30.524199
453.100412	19119.305462	30.529216
453.666223	19147.192011	30.534234
453.628293	19174.863024	30.539252
454.250585	19206.063954	30.544269
454.691066	19230.230073	30.549287
455.512022	19264.540055	30.554304
455.789742	19281.895839	30.559322
455.896690	19314.030059	30.564340
456.822975	19330.413076	30.569357
456.889777	19366.179997	30.574375
456.885949	19396.524730	30.579392
457.348028	19418.407021	30.584410
457.858968	19462.697101	30.589428
458.323652	19493.720861	30.594445
458.596458	19527.124752	30.599463
459.368965	19568.000661	30.604480
459.631711	19601.399929	30.609498
460.327819	19644.113734	30.614516
460.661371	19676.807149	30.619533
460.993914	19708.306704	30.624551
461.813833	19748.385882	30.629568
462.250172	19788.152104	30.634586
462.964057	19818.031959	30.639604
464.083100	19843.849570	30.644621
464.441433	19867.037363	30.649639
464.492124	19895.415840	30.654656
465.036385	19918.720061	30.659674
465.318971	19957.423885	30.664692
465.999857	19984.156495	30.669709
466.347377	20027.051766	30.674727
466.776008	20045.850499	30.679744
467.475411	20079.460595	30.684762
467.598979	20111.561950	30.689780
468.209019	20144.446869	30.694797
468.908801	20182.662887	30.699815
469.221374	20208.947704	30.704832
469.666937	20237.581104	30.709850
469.948041	20272.627660	30.714868
470.244438	20303.426185	30.719885
470.557414	20341.759594	30.724903
471.569775	20372.446768	30.729920
472.156766	20410.339616	30.734938
472.661139	20441.080708	30.739956
473.202614	20465.933943	30.744973
473.961095	20499.434476	30.749991
474.021393	20521.241555	30.755008
474.517311	20553.266713	30.760026
474.887407	20582.310407	30.765044
475.363099	20603.825459	30.770061
476.265092	20632.148292	30.775079
477.305957	20642.512358	30.780096
478.234849	20649.823248	30.785114
478.510509	20679.507284	30.790132
479.007309	20684.307651	30.795149
478.865831	20711.548370	30.800167
479.657190	20737.588771	30.805184
480.189778	20748.347931	30.810202
480.496305	20781.622354	30.815220
480.709895	20796.032562	30.820237
481.406386	20825.720805	30.825255
481.623276	20853.878934	30.830272
482.418350	20872.514006	30.835290
482.273677	20902.497590	30.840308
482.945531	20914.865260	30.845325
483.089221	20951.078021	30.850343
483.307225	20977.441775	30.855360
483.574517	21003.102884	30.860378
484.060933	21049.257943	30.865396
484.513159	21065.280266	30.870413
484.977145	21107.471081	30.875431
485.830921	21134.020393	30.880448
486.547402	21157.602559	30.885466
486.512085	21178.111047	30.890484
487.530699	21207.174755	30.895501
487.836859	21239.066300	30.900519
488.364275	21272.850544	30.905536
488.700879	21292.258725	30.910554
488.713675	21329.838368	30.915572
489.482795	21361.247345	30.920589
489.949346	21407.330517	30.925607
490.251057	21442.774014	30.930624
490.738085	21474.890519	30.935642
491.315192	21502.260564	30.940660
492.041699	21533.891278	30.945677
492.321270	21574.001452	30.950695
492.890755	21608.272560	30.955712
493.881824	21637.878264	30.960730
494.158608	21674.570793	30.965748
494.645993	21706.637074	30.970765
495.335406	21736.662677	30.975783
495.544574	21775.160370	30.980800
496.185787	21800.713761	30.985818
496.587561	21837.595647	30.990836
497.238530	21873.415207	30.995853
497.685044	21915.275592	31.000871
497.991764	21948.223395	31.005888
498.963038	21977.207154	31.010906
499.343852	22018.326078	31.015924
499.707672	22044.813889	31.020941
500.396020	22077.007452	31.025959
500.932793	22116.137217	31.030976
501.732455	22145.893538	31.035994
502.225556	22175.350103	31.041012
502.611091	22204.684448	31.046029
502.910608	22229.994615	31.051047
503.430383	22263.724882	31.056064
503.583044	22291.882428	31.061082
503.644934	22323.807437	31.066100
504.430416	22363.954193	31.071117
504.971449	22394.161866	31.076135
505.703948	22443.472824	31.081152
506.203479	22477.010726	31.086170
506.355200	22516.264415	31.091188
506.954748	22548.112403	31.096205
507.761923	22588.812290	31.101223
508.838761	22616.036580	31.106240
509.481144	22637.843847	31.111258
510.085775	22664.686765	31.116276
510.490735	22695.901812	31.121293
511.484416	22719.398467	31.126311
511.993992	22740.803163	31.131328
512.662760	22742.847545	31.136346
513.619123	22757.895495	31.141364
514.230322	22753.851189	31.146381
515.334661	22776.483965	31.151399
515.441658	22792.744686	31.156416
516.079355	22787.552541	31.161434
516.048511	22807.676576	31.166452
516.221448	22814.366667	31.171469
517.072575	22827.004623	31.176487
517.325439	22842.850910	31.181504
517.382842	22863.409901	31.186522
517.889083	22886.161189	31.191540
518.293194	22893.617813	31.196557
518.424548	22922.860099	31.201575
518.686053	22952.056891	31.206592
519.412926	22971.387014	31.211610
519.393114	22991.294677	31.216628
519.594143	23033.916002	31.221645
520.463977	23069.362439	31.226663
520.485717	23102.343892	31.231680
521.233673	23140.355956	31.236698
521.435850	23183.685144	31.241716
522.076320	23214.971769	31.246733
522.341802	23264.287968	31.251751
523.119640	23315.812002	31.256768
523.669041	23342.885603	31.261786
523.898782	23389.357809	31.266804
524.527747	23434.674783	31.271821
525.142955	23470.452252	31.276839
525.690427	23523.459747	31.281856
526.043891	23571.619262	31.286874
526.907795	23611.061244	31.291892
527.041384	23651.697562	31.296909
527.959095	23693.854862	31.301927
528.633768	23745.250730	31.306944
529.581736	23780.035405	31.311962
529.601870	23815.375327	31.316980
530.400180	23857.077625	31.321997
531.133502	23891.876953	31.327015
531.543532	23937.892669	31.332032
532.210721	23970.010457	31.337050
532.689054	24009.241527	31.342068
533.134612	24047.403510	31.347085
533.777343	24077.035506	31.352103
534.500207	24125.922439	31.357120
535.065906	24162.884242	31.362138
535.567635	24192.399335	31.367156
535.804265	24228.553067	31.372173
536.648862	24265.781287	31.377191
536.986349	24311.878672	31.382208
537.678424	24344.391305	31.387226
538.029376	24382.840388	31.392244
538.587061	24424.284325	31.397261
539.505711	24463.605727	31.402279
539.681144	24503.908660	31.407296
540.485283	24534.040715	31.412314
540.777002	24579.141060	31.417332
541.339421	24615.845117	31.422349
541.832836	24645.956200	31.427367
542.317534	24693.718830	31.432384
543.314213	24724.838627	31.437402
543.551621	24765.669591	31.442420
544.407935	24801.386639	31.447437
544.875783	24842.371469	31.452455
545.398653	24883.859696	31.457472
545.789015	24915.503904	31.462490
546.517666	24949.269409	31.467508
546.888164	24993.865503	31.472525
547.483362	25025.465358	31.477543
548.120168	25067.473388	31.482560
548.722201	25113.904290	31.487578
549.107657	25147.875226	31.492596
549.965581	25187.706753	31.497613
550.159888	25215.564930	31.502631
550.855537	25254.954203	31.507648
551.405675	25281.360445	31.512666
552.459261	25309.097623	31.517684
553.195345	25341.333285	31.522701
553.523884	25359.969389	31.527719
554.008076	25396.592262	31.532736
554.566999	25399.450306	31.537754
555.237251	25432.675908	31.542772
555.367204	25461.776779	31.547789
556.024958	25482.725302	31.552807
556.779827	25529.266086	31.557824
557.178126	25557.510081	31.562842
557.606404	25583.859857	31.567860
557.534297	25617.940738	31.572877
558.363251	25644.443088	31.577895
558.872178	25683.900191	31.582912
559.500612	25722.163294	31.587930
560.072934	25756.529593	31.592948
560.734981	25790.565995	31.597965
561.363677	25817.175587	31.602983
561.788870	25860.855045	31.608000
562.300909	25894.535788	31.613018
562.665082	25935.134523	31.618036
562.894581	25973.839398	31.623053
563.707941	26019.152486	31.628071
564.188695	26067.633142	31.633088
564.733197	26109.676684	31.638106
565.529755	26153.684477	31.643124
566.540011	26187.465107	31.648141
566.982471	26229.632222	31.653159
567.523254	26264.560452	31.658176
568.179204	26302.485419	31.663194
568.906795	26318.620797	31.668212
569.656271	26358.269293	31.673229
570.180707	26395.052038	31.678247
570.680053	26426.738541	31.683264
571.198954	26456.172137	31.688282
571.618182	26504.328463	31.693300
572.192176	26543.783442	31.698317
573.078585	26574.424000	31.703335
573.927775	26610.518261	31.708352
574.738810	26648.577738	31.713370
575.152609	26671.183410	31.718388
575.300742	26710.022444	31.723405
576.049619	26749.419000	31.728423
576.545218	26785.631820	31.733440
576.978606	26819.636038	31.738458
577.512831	26852.524917	31.743476
578.053196	26894.134651	31.748493
578.668704	26928.167580	31.753511
579.282042	26974.044844	31.758528
579.770510	27011.251440	31.763546
580.483449	27043.923205	31.768564
580.785373	27090.601312	31.773581
581.403606	27130.985937	31.778599
581.891461	27169.001903	31.783616
582.514133	27222.374035	31.788634
582.922351	27249.961555	31.793652
583.365961	27302.123008	31.798669
584.290953	27340.557904	31.803687
584.971100	27383.777509	31.808704
585.507457	27411.376902	31.813722
585.770082	27446.672811	31.818740
586.682218	27498.843998	31.823757
587.382473	27540.221598	31.828775
588.290641	27575.916543	31.833792
588.615986	27613.920720	31.838810
589.241170	27645.172401	31.843828
589.412371	27697.042298	31.848845
590.329325	27732.755113	31.853863
590.975920	27781.624886	31.858880
591.544091	27803.917053	31.863898
592.246204	27845.686852	31.868916
592.689372	27882.276379	31.873933
593.358655	27905.500980	31.878951
594.083024	27932.344964	31.883968
594.637207	27959.917047	31.888986
595.866938	27977.429288	31.894004
596.290689	27999.940087	31.899021
597.087395	28022.708876	31.904039
597.489617	28049.495717	31.909056
597.537405	28090.628386	31.914074
598.456562	28109.585918	31.919092
598.799240	28145.534231	31.924109
599.483732	28172.669164	31.929127
599.729014	28214.618288	31.934144
600.265955	28249.278758	31.939162
600.743639	28281.805847	31.944180
601.031848	28324.051899	31.949197
602.079012	28358.974438	31.954215
602.718266	28402.891521	31.959232
603.180941	28442.949021	31.964250
603.860515	28480.381384	31.969268
604.098392	28537.154154	31.974285
605.110571	28573.289747	31.979303
605.368475	28623.656837	31.984320
605.807765	28678.350753	31.989338
606.228390	28711.873435	31.994356
606.951284	28771.769617	31.999373
607.739754	28811.315711	32.004391
608.218210	28859.910853	32.009408
608.550730	28917.068151	32.014426
609.495569	28960.420562	32.019444
610.465032	29005.753953	32.024461
611.557836	29047.225208	32.029479
611.923887	29087.482316	32.034496
612.483089	29129.340204	32.039514
613.744652	29149.212488	32.044532
614.504202	29185.363211	32.049549
615.526235	29217.547897	32.054567
616.315277	29247.019337	32.059584
616.504647	29270.750026	32.064602
617.079527	29294.781017	32.069620
617.742286	29334.442507	32.074637
618.344162	29367.925408	32.079655
618.957738	29399.017245	32.084672
619.745953	29426.314687	32.089690
620.309912	29456.561014	32.094708
620.448347	29501.158909	32.099725
621.393096	29540.309152	32.104743
621.631585	29567.186684	32.109760
621.814424	29606.563119	32.114778
622.522010	29647.261194	32.119796
623.200348	29689.234421	32.124813
623.848758	29733.848247	32.129831
624.688812	29780.101083	32.134848
625.141496	29816.888547	32.139866
625.605362	29851.676890	32.144884
625.861235	29900.593598	32.149901
626.610604	29943.915313	32.154919
627.210493	29987.860892	32.159936
627.735156	30038.019261	32.164954
628.426815	30084.896388	32.169972
628.879213	30135.350694	32.174989
630.005938	30166.850539	32.180007
630.474007	30218.547872	32.185024
630.798966	30271.835260	32.190042
631.888959	30304.807544	32.195060
632.406952	30355.258499	32.200077
633.350176	30396.509248	32.205095
634.233791	30424.526428	32.210112
634.899975	30454.031373	32.215130
635.807423	30479.194049	32.220148
636.409484	30507.280457	32.225165
636.923480	30539.173356	32.230183
637.150158	30566.351132	32.235200
637.502572	30606.335206	32.240218
638.465261	30648.146022	32.245236
638.752548	30688.285783	32.250253
639.361744	30717.338523	32.255271
640.123701	30755.527097	32.260288
640.617007	30807.601258	32.265306
641.224216	30841.926468	32.270324
641.862402	30876.891691	32.275341
642.863083	30931.927748	32.280359
642.964946	30962.254549	32.285376
643.437791	31012.612999	32.290394
644.270932	31051.005966	32.295412
644.473720	31110.547438	32.300429
645.202140	31158.192498	32.305447
646.484376	31213.248689	32.310464
646.642945	31256.203671	32.315482
647.661696	31302.375217	32.320500
647.981863	31355.236287	32.325517
648.934233	31396.999656	32.330535
649.365438	31448.143193	32.335552
649.654245	31500.282540	32.340570
650.709370	31537.187901	32.345588
651.227324	31589.538341	32.350605
652.152967	31653.065216	32.355623
653.115264	31693.879402	32.360640
653.720973	31746.507371	32.365658
654.045970	31783.299254	32.370676
654.996713	31836.739802	32.375693
655.605649	31891.927901	32.380711
656.173721	31930.028716	32.385728
656.851771	31990.832601	32.390746
657.532241	32029.010927	32.395764
658.151677	32086.796126	32.400781
658.627317	32140.431528	32.405799
659.286914	32186.711530	32.410816
659.791969	32244.116702	32.415834
660.532658	32292.426244	32.420852
661.324138	32350.627918	32.425869
661.882770	32395.425837	32.430887
662.505096	32448.318512	32.435904
663.601136	32501.289302	32.440922
664.103941	32545.211176	32.445940
664.530080	32598.412935	32.450957
665.326955	32659.364645	32.455975
666.155918	32709.311426	32.460992
666.399412	32756.308625	32.466010
667.233185	32810.149200	32.471028
668.558919	32864.261036	32.476045
669.533511	32916.885117	32.481063
669.896067	32948.931740	32.486080
670.624557	33000.709267	32.491098
671.391967	33037.466104	32.496116
672.089417	33089.811342	32.501133
672.660428	33136.284261	32.506151
673.509825	33174.798746	32.511168
674.422563	33234.988101	32.516186
674.831917	33259.637427	32.521204
675.308834	33302.230968	32.526221
676.162505	33355.804326	32.531239
676.828988	33391.654473	32.536256
677.156106	33442.509328	32.541274
677.885541	33487.953148	32.546292
678.497130	33515.264525	32.551309
679.165246	33562.443998	32.556327
679.791309	33605.406913	32.561344
679.739923	33647.710390	32.566362
680.575460	33695.142276	32.571380
681.296215	33738.463732	32.576397
681.853487	33795.751241	32.581415
682.485454	33849.221285	32.586432
683.040595	33896.842689	32.591450
683.778011	33949.310300	32.596468
684.808217	34001.277259	32.601485
685.278241	34055.778284	32.606503
685.860676	34101.783716	32.611520
686.745396	34158.958018	32.616538
687.444800	34207.512342	32.621556
688.321979	34252.555480	32.626573
688.932655	34311.347127	32.631591
689.791141	34353.915017	32.636608
690.534417	34411.010866	32.641626
691.581733	34460.776099	32.646644
692.140323	34503.055888	32.651661
692.614009	34556.489147	32.656679
693.606817	34593.302144	32.661696
694.211694	34648.289509	32.666714
694.706846	34692.678619	32.671732
695.366725	34740.582787	32.676749
696.074259	34802.098376	32.681767
697.452026	34838.959359	32.686784
697.780171	34889.766975	32.691802
698.348050	34940.733393	32.696820
699.149307	34996.000901	32.701837
699.687062	35049.336920	32.706855
700.413042	35089.859434	32.711872
700.840222	35146.298349	32.716890
701.482758	35207.920078	32.721908
702.057612	35256.110527	32.726925
703.070118	35319.451658	32.731943
703.759428	35372.018821	32.736960
704.399224	35436.784028	32.741978
705.051402	35494.371195	32.746996
706.131820	35545.638649	32.752013
706.486444	35608.273745	32.757031
707.503478	35655.960000	32.762048
708.233814	35702.628761	32.767066
708.849284	35759.469950	32.772084
709.940035	35810.698502	32.777101
710.432772	35869.221997	32.782119
711.076986	35915.120600	32.787136
712.083090	35974.424378	32.792154
712.847922	36014.746608	32.797172
713.468211	36075.919078	32.802189
714.177972	36124.115793	32.807207
714.913640	36171.967145	32.812224
715.340073	36221.175596	32.817242
716.075236	36277.120648	32.822260
717.355353	36320.448856	32.827277
717.591668	36381.087617	32.832295
718.339823	36433.155058	32.837312
718.799438	36488.707273	32.842330
719.540262	36540.219690	32.847348
720.409849	36585.098262	32.852365
720.920738	36650.260298	32.857383
721.821001	36701.773579	32.862400
722.785029	36749.065865	32.867418
723.615221	36799.211851	32.872436
724.800304	36854.512979	32.877453
725.148602	36900.282727	32.882471
725.906927	36943.434184	32.887488
726.769004	36991.381519	32.892506
727.287402	37034.058331	32.897524
728.194301	37066.570265	32.902541
728.921751	37109.309532	32.907559
729.580173	37147.076925	32.912576
730.371207	37196.686145	32.917594
730.869114	37231.898792	32.922612
731.604370	37267.624674	32.927629
732.062216	37319.277874	32.932647
732.858172	37367.641039	32.937664
733.593436	37415.160114	32.942682
733.910236	37469.491424	32.947700
734.489212	37521.221106	32.952717
734.956752	37583.951931	32.957735
736.416336	37623.941418	32.962752
737.830976	37658.841331	32.967770
738.791689	37707.995335	32.972788
740.023736	37748.905753	32.977805
740.141291	37784.210136	32.982823
740.724717	37821.073500	32.987840
741.741743	37860.139545	32.992858
741.770651	37924.337129	32.997876
742.570998	37962.071222	33.002893
743.032065	38021.705837	33.007911
743.797282	38070.948019	33.012928
744.390564	38125.010304	33.017946
744.681574	38187.852583	33.022964
745.729974	38243.564321	33.027981
746.497574	38313.155891	33.032999
747.445895	38358.873294	33.038016
748.034491	38421.258896	33.043034
748.509870	38485.325417	33.048052
749.608436	38542.402348	33.053069
750.455188	38610.496503	33.058087
751.362991	38661.798328	33.063104
752.300331	38710.654732	33.068122
753.158811	38774.833218	33.073140
753.593601	38824.881086	33.078157
754.469049	38882.373075	33.083175
755.357022	38938.415129	33.088192
755.846018	38986.867671	33.093210
756.605623	39050.657649	33.098228
757.641820	39092.948087	33.103245
758.279563	39154.474449	33.108263
759.110087	39214.782095	33.113280
759.602939	39269.697635	33.118298
760.255379	39336.806192	33.123316
761.456814	39400.616959	33.128333
762.407910	39456.378605	33.133351
763.305999	39507.279224	33.138368
764.173479	39552.701875	33.143386
764.740356	39612.090433	33.148404
765.285286	39664.545176	33.153421
766.081645	39711.313588	33.158439
766.724180	39777.900165	33.163456
767.645027	39826.009108	33.168474
768.615850	39881.844668	33.173492
769.365121	39928.658825	33.178509
770.254655	39985.797412	33.183527
770.777687	40037.465959	33.188544
771.627042	40087.034824	33.193562
772.406510	40147.264480	33.198580
773.162940	40191.801412	33.203597
773.782680	40263.060230	33.208615
774.408169	40317.249474	33.213632
774.970758	40367.047020	33.218650
775.726565	40423.790183	33.223668
776.777595	40486.173000	33.228685
777.129530	40537.312839	33.233703
777.871503	40586.994426	33.238720
778.580882	40644.599164	33.243738
779.581069	40701.450468	33.248756
780.394116	40754.220265	33.253773
780.967836	40813.750179	33.258791
781.632137	40864.367838	33.263808
782.342663	40921.637942	33.268826
783.263413	40976.744166	33.273844
784.008635	41028.127504	33.278861
784.768014	41093.030288	33.283879
785.338490	41151.998760	33.288896
786.612275	41207.430075	33.293914
787.350112	41258.593751	33.298932
788.556567	41307.780941	33.303949
789.782454	41361.234228	33.308967
790.111700	41416.186986	33.313984
791.223597	41459.962837	33.319002
792.021425	41527.397049	33.324020
792.527288	41577.275760	33.329037
793.061492	41630.325091	33.334055
793.739925	41687.728692	33.339072
794.891179	41746.576738	33.344090
795.329762	41805.112134	33.349108
796.142261	41870.483303	33.354125
797.024367	41928.576835	33.359143
797.768159	41986.363171	33.364160
798.582185	42047.414900	33.369178
799.384723	42119.650618	33.374196
800.340269	42175.051707	33.379213
801.141198	42237.649230	33.384231
801.931013	42295.454515	33.389248
802.891995	42353.094163	33.394266
803.261419	42418.055254	33.399284
804.319931	42480.157988	33.404301
805.332613	42534.178612	33.409319
805.811346	42603.424098	33.414336
806.635881	42672.274431	33.419354
807.696819	42734.927769	33.424372
808.426780	42792.142815	33.429389
808.962755	42856.117892	33.434407
809.775431	42922.542095	33.439424
810.437083	42992.822916	33.444442
811.307849	43069.440635	33.449460
812.519587	43130.250036	33.454477
813.115132	43201.041484	33.459495
813.856549	43274.005229	33.464512
814.641590	43327.734335	33.469530
815.670412	43398.288193	33.474548
816.283140	43461.550995	33.479565
817.075162	43527.297126	33.484583
817.476491	43600.378140	33.489600
818.628886	43661.957256	33.494618
819.240519	43743.519621	33.499636
820.297868	43810.705376	33.504653
821.196652	43887.378495	33.509671
821.412346	43955.435752	33.514688
822.711131	44020.358088	33.519706
823.688771	44089.094125	33.524724
824.778748	44160.159561	33.529741
825.489312	44226.268336	33.534759
826.478346	44288.981551	33.539776
827.666606	44358.754613	33.544794
827.978961	44419.309067	33.549812
828.859502	44474.183625	33.554829
830.072301	44541.252515	33.559847
830.578033	44607.697929	33.564864
831.742586	44669.151443	33.569882
832.604155	44734.542429	33.574900
833.121679	44785.141347	33.579917
833.921457	44839.384184	33.584935
834.419356	44901.777076	33.589952
836.022513	44952.466723	33.594970
836.346016	45009.206776	33.599988
837.539669	45048.580807	33.605005
838.796800	45101.766309	33.610023
839.280030	45157.476115	33.615040
840.242757	45196.993891	33.620058
841.066736	45254.390425	33.625076
841.323233	45313.418888	33.630093
842.048109	45377.637502	33.635111
842.496157	45437.212104	33.640128
843.783929	45511.578346	33.645146
844.254870	45570.434940	33.650164
845.283932	45639.977446	33.655181
846.216920	45699.553167	33.660199
846.909862	45765.024027	33.665216
847.427252	45833.995236	33.670234
848.233207	45912.486285	33.675252
849.240063	45980.135576	33.680269
850.430264	46053.184066	33.685287
851.180005	46133.835412	33.690304
852.020174	46199.721105	33.695322
852.913455	46263.675663	33.700340
853.831046	46338.671603	33.705357
855.234062	46404.153987	33.710375
856.209082	46451.864108	33.715392
857.460377	46519.546560	33.720410
858.077736	46589.921537	33.725428
859.004391	46650.702701	33.730445
860.058577	46703.208769	33.735463
860.762844	46756.003491	33.740480
861.516418	46819.633449	33.745498
862.442896	46892.820613	33.750516
863.205243	46945.353696	33.755533
863.909265	47010.680962	33.760551
864.623795	47082.465717	33.765568
865.801342	47144.107463	33.770586
866.357376	47218.302264	33.775604
867.388762	47276.576320	33.780621
868.333231	47348.604478	33.785639
869.372706	47409.604194	33.790656
870.986692	47451.675238	33.795674
871.728321	47524.254279	33.800692
872.116389	47583.331478	33.805709
873.346901	47633.990313	33.810727
873.962649	47701.256495	33.815744
875.284286	47749.098870	33.820762
875.923953	47809.744368	33.825780
876.739446	47869.837576	33.830797
877.889768	47929.853516	33.835815
878.003000	47986.228922	33.840832
878.979334	48044.855151	33.845850
879.942321	48109.152040	33.850868
880.395446	48178.077156	33.855885
881.479160	48241.299119	33.860903
882.544187	48314.867882	33.865920
883.396322	48371.698603	33.870938
884.081502	48438.380455	33.875956
884.851840	48507.301476	33.880973
885.924198	48573.113663	33.885991
886.834630	48633.137174	33.891008
887.953032	48696.595413	33.896026
889.030948	48753.043981	33.901044
889.710616	48824.352534	33.906061
890.712943	48882.622590	33.911079
891.522279	48942.283058	33.916096
892.141154	48995.260784	33.921114
893.174943	49047.294643	33.926132
893.720874	49114.392402	33.931149
894.605768	49158.604643	33.936167
895.168815	49233.975370	33.941184
896.132889	49294.979237	33.946202
896.925242	49356.028979	33.951220
897.660565	49422.541409	33.956237
898.333503	49494.068210	33.961255
898.988868	49561.251473	33.966272
899.963434	49625.778605	33.971290
900.886436	49712.312286	33.976308
901.994029	49782.532271	33.981325
903.260304	49857.782931	33.986343
903.907793	49929.593435	33.991360
904.839908	50007.813295	33.996378
905.841281	50070.300245	34.001396
906.323587	50150.109069	34.006413
907.663805	50223.059065	34.011431
908.209094	50297.967859	34.016448
909.412037	50371.180120	34.021466
910.269098	50450.602647	34.026484
910.608841	50536.951838	34.031501
911.877396	50609.047410	34.036519
912.793866	50700.179279	34.041536
914.286991	50780.364416	34.046554
914.830713	50854.155364	34.051572
915.655450	50941.607421	34.056589
916.969627	51013.969227	34.061607
917.970268	51096.940159	34.066624
918.902563	51170.222399	34.071642
920.039841	51249.116861	34.076660
920.848800	51316.224395	34.081677
921.982395	51375.891331	34.086695
922.954559	51452.762154	34.091712
924.069641	51523.720254	34.096730
925.356995	51586.736259	34.101748
926.012417	51665.162998	34.106765
927.404906	51723.151746	34.111783
928.206164	51788.983721	34.116800
928.921486	51851.956618	34.121818
929.933108	51925.545273	34.126836
930.596893	52001.447204	34.131853
931.980035	52051.579543	34.136871
932.728146	52135.302182	34.141888
933.336417	52189.586044	34.146906
934.833623	52267.947061	34.151924
935.498598	52332.915940	34.156941
936.759946	52388.421063	34.161959
937.379119	52457.421743	34.166976
938.398983	52518.912684	34.171994
939.318866	52591.461021	34.177012
940.187573	52670.193314	34.182029
941.277165	52725.358975	34.187047
942.171075	52797.070420	34.192064
943.205028	52863.495655	34.197082
944.303083	52926.671320	34.202100
945.038611	52997.876509	34.207117
945.688051	53056.205721	34.212135
946.540968	53119.350462	34.217152
947.679041	53193.125929	34.222170
948.211570	53265.888526	34.227188
949.380052	53334.255774	34.232205
950.917584	53409.937694	34.237223
951.758136	53477.249037	34.242240
952.743222	53543.183912	34.247258
953.632626	53610.279214	34.252276
954.224970	53674.655656	34.257293
955.379678	53719.549681	34.262311
955.733324	53779.989640	34.267328
956.512257	53852.070254	34.272346
957.054423	53918.492775	34.277364
957.906349	53992.739277	34.282381
959.361390	54072.948034	34.287399
960.082343	54147.658375	34.292416
960.773469	54222.772262	34.297434
961.699157	54303.254046	34.302452
962.409153	54378.428774	34.307469
963.393604	54461.635687	34.312487
964.443851	54546.807029	34.317504
965.243979	54625.094611	34.322522
966.386844	54714.422397	34.327540
966.965227	54799.073252	34.332557
967.965451	54878.267101	34.337575
969.127280	54968.776275	34.342592
970.311168	55049.106504	34.347610
971.628223	55130.219971	34.352628
972.807661	55214.329445	34.357645
973.781311	55293.054197	34.362663
974.773591	55374.035534	34.367680
975.988484	55453.406729	34.372698
977.178926	55528.447046	34.377716
977.818316	55606.243969	34.382733
979.054557	55688.479402	34.387751
979.972794	55769.017967	34.392768
981.102673	55842.840984	34.397786
981.942837	55919.360970	34.402804
983.011391	56003.344949	34.407821
983.721039	56076.373427	34.412839
984.695266	56160.929557	34.417856
985.404519	56246.356278	34.422874
986.787354	56319.375642	34.427892
987.753617	56413.021787	34.432909
989.034115	56487.184093	34.437927
990.371660	56564.514742	34.442944
991.127367	56644.258841	34.447962
992.540179	56720.970727	34.452980
993.497482	56799.956164	34.457997
994.368965	56874.936462	34.463015
995.494797	56941.137369	34.468032
996.705900	57014.185595	34.473050
998.020875	57086.085018	34.478068
998.898393	57154.192167	34.483085
1000.016174	57213.787789	34.488103
1001.486183	57275.879263	34.493120
1002.213192	57345.250841	34.498138
1003.157847	57405.392857	34.503156
1003.980391	57488.148248	34.508173
1004.668061	57547.742035	34.513191
1005.833239	57620.843564	34.518208
1007.061628	57689.517856	34.523226
1007.795218	57765.528713	34.528244
1008.407608	57841.704244	34.533261
1009.446050	57903.320227	34.538279
1010.194003	57993.145832	34.543296
1011.082495	58077.215757	34.548314
1012.025577	58153.910417	34.553332
1013.087006	58234.447657	34.558349
1013.995805	58312.724108	34.563367
1014.827921	58399.196344	34.568384
1015.675599	58485.476592	34.573402
1016.766313	58562.466031	34.578420
1017.918961	58659.921100	34.583437
1018.857405	58736.080349	34.588455
1019.845941	58826.751373	34.593472
1020.502083	58910.860370	34.598490
1021.607870	58996.418703	34.603508
1022.692305	59072.720849	34.608525
1023.646993	59147.796550	34.613543
1024.687268	59231.258236	34.618560
1025.638705	59320.588728	34.623578
1026.667931	59389.229240	34.628596
1027.809239	59477.271200	34.633613
1028.538094	59545.737380	34.638631
1029.963011	59635.742206	34.643648
1031.036913	59722.896764	34.648666
1031.972390	59801.256158	34.653684
1033.008816	59887.784188	34.658701
1033.847657	59966.564248	34.663719
1035.709385	60057.192564	34.668736
1036.493037	60129.531894	34.673754
1037.965763	60206.517726	34.678772
1038.753041	60288.376721	34.683789
1039.593042	60372.189981	34.688807
1041.075729	60446.915331	34.693824
1041.945208	60529.787750	34.698842
1042.946823	60606.145579	34.703860
1043.630427	60690.053901	34.708877
1044.828853	60771.894825	34.713895
1046.239534	60847.658033	34.718912
1047.407629	60931.339852	34.723930
1048.841430	61008.157038	34.728948
1049.648665	61094.016077	34.733965
1051.072882	61171.563201	34.738983
1051.809926	61242.735723	34.744000
1052.661141	61329.158430	34.749018
1053.770947	61400.184766	34.754036
1054.568570	61492.420939	34.759053
1055.431319	61575.133361	34.764071
1056.844010	61662.932068	34.769088
1057.702949	61750.279234	34.774106
1058.559807	61843.083532	34.779124
1059.568864	61929.224246	34.784141
1060.560005	62023.711110	34.789159
1061.795487	62109.848861	34.794176
1062.788218	62202.038329	34.799194
1064.102157	62293.690721	34.804212
1064.999796	62386.193197	34.809229
1065.792404	62473.091141	34.814247
1067.035965	62563.761647	34.819264
1067.752751	62666.554629	34.824282
1069.202751	62750.812787	34.829300
1069.733029	62853.711540	34.834317
1071.094248	62958.741305	34.839335
1072.462841	63045.178110	34.844352
1073.490041	63137.289731	34.849370
1074.883860	63227.015040	34.854388
1076.006751	63309.945989	34.859405
1077.053606	63405.322042	34.864423
1077.915594	63481.602895	34.869440
1079.112425	63585.977210	34.874458
1080.572934	63674.744181	34.879476
1082.004311	63747.461766	34.884493
1083.045372	63824.418484	34.889511
1084.532303	63905.515867	34.894528
1085.333654	63988.847310	34.899546
1086.470346	64062.346033	34.904564
1087.530107	64136.755898	34.909581
1088.869020	64214.471447	34.914599
1090.106231	64298.381804	34.919616
1091.100033	64373.264779	34.924634
1092.055789	64443.899664	34.929652
1093.068796	64526.370630	34.934669
1093.966116	64606.903672	34.939687
1094.973384	64670.795262	34.944704
1095.746326	64755.602418	34.949722
1096.769295	64822.916908	34.954740
1097.800118	64897.738711	34.959757
1098.731605	64981.312764	34.964775
1099.736539	65057.658476	34.969792
1100.499951	65142.658348	34.974810
1101.247273	65218.164654	34.979828
1102.296225	65311.350825	34.984845
1103.650820	65404.749335	34.989863
1104.805211	65497.647553	34.994880
1105.600933	65588.974876	34.999898
1107.134705	65670.425217	35.004916
1108.370028	65761.792367	35.009933
1108.855410	65859.316415	35.014951
1109.993586	65953.769947	35.019968
1111.109615	66052.994606	35.024986
1112.299841	66150.808925	35.030004
1113.905559	66249.628914	35.035021
1114.318031	66350.331783	35.040039
1115.753482	66442.917486	35.045056
1116.813258	66550.718980	35.050074
1118.302840	66648.963468	35.055092
1119.188587	66752.886521	35.060109
1120.251378	66843.094146	35.065127
1121.081651	66938.510983	35.070144
1121.787595	67055.252555	35.075162
1123.405573	67153.352380	35.080180
1124.722954	67264.757351	35.085197
1126.317585	67367.914105	35.090215
1127.582970	67472.471129	35.095232
1128.545973	67570.674511	35.100250
1129.852846	67667.925670	35.105268
1131.008882	67766.884868	35.110285
1132.347836	67868.772816	35.115303
1133.653749	67963.271018	35.120320
1134.442968	68063.985327	35.125338
1135.452654	68165.165913	35.130356
1136.739965	68250.493530	35.135373
1137.848635	68356.591826	35.140391
1139.330569	68454.996419	35.145408
1140.577419	68550.810313	35.150426
1141.357767	68648.698012	35.155444
1142.842357	68743.133284	35.160461
1143.478322	68846.134959	35.165479
1144.812405	68951.928357	35.170496
1146.225055	69053.189016	35.175514
1147.195880	69146.686310	35.180532
1148.516575	69238.046288	35.185549
1149.681506	69338.358849	35.190567
1151.412835	69421.708996	35.195584
1152.381627	69525.775998	35.200602
1153.539993	69613.477366	35.205620
1154.981090	69708.695447	35.210637
1156.304919	69800.772446	35.215655
1157.749476	69870.630785	35.220672
1158.403157	69973.551877	35.225690
1159.434148	70062.471355	35.230708
1160.609227	70143.054632	35.235725
1161.499907	70249.124983	35.240743
1163.043385	70326.688043	35.245760
1164.174505	70429.036382	35.250778
1165.490540	70517.488792	35.255796
1166.761059	70588.667926	35.260813
1167.491522	70680.802413	35.265831
1168.713376	70765.515300	35.270848
1169.704403	70870.426421	35.275866
1170.822078	70954.611561	35.280884
1172.029645	71040.859988	35.285901
1172.640587	71113.726307	35.290919
1173.842750	71189.742980	35.295936
1174.405523	71292.328817	35.300954
1175.747742	71374.124705	35.305972
1177.111467	71468.379745	35.310989
1178.106625	71555.663458	35.316007
1179.362162	71655.255281	35.321024
1181.120650	71757.479510	35.326042
1181.493494	71839.313753	35.331060
1182.816485	71943.759557	35.336077
1183.850324	72042.728772	35.341095
1185.109647	72136.546518	35.346112
1186.209594	72244.764471	35.351130
1187.334705	72337.058661	35.356148
1188.638543	72438.191100	35.361165
1189.798295	72548.503440	35.366183
1190.785459	72657.069942	35.371200
1192.308566	72761.234529	35.376218
1193.275374	72865.828088	35.381236
1194.769499	72967.376230	35.386253
1195.662778	73080.189395	35.391271
1196.712218	73192.814079	35.396288
1198.321335	73300.893775	35.401306
1199.357494	73418.613123	35.406324
1200.890597	73522.272518	35.411341
1201.686652	73616.775590	35.416359
1203.230797	73732.352715	35.421376
1204.240526	73851.395354	35.426394
1205.345361	73962.532754	35.431412
1206.756342	74071.913036	35.436429
1208.342401	74178.986604	35.441447
1209.628779	74279.647470	35.446464
1211.042278	74379.326292	35.451482
1212.586105	74489.244926	35.456500
1214.119682	74582.281326	35.461517
1215.447099	74692.095149	35.466535
1216.616963	74784.238884	35.471552
1217.891210	74885.195248	35.476570
1219.409001	74971.192877	35.481588
1221.048177	75060.819869	35.486605
1222.027845	75153.323810	35.491623
1223.157736	75248.528024	35.496640
1224.428408	75343.824664	35.501658
1225.166712	75437.507158	35.506676
1226.269602	75522.253789	35.511693
1227.202101	75623.582795	35.516711
1228.182292	75725.854777	35.521728
1229.847996	75831.377189	35.526746
1231.055606	75934.209911	35.531764
1232.562467	76032.816316	35.536781
1233.760209	76135.207992	35.541799
1234.968698	76228.161357	35.546816
1236.196882	76329.041639	35.551834
1237.670927	76422.410357	35.556852
1239.584839	76521.043857	35.561869
1240.612164	76609.162493	35.566887
1241.893667	76692.922282	35.571904
1243.203602	76783.480300	35.576922
1244.259917	76873.862750	35.581940
1245.643781	76966.246652	35.586957
1246.716885	77060.490695	35.591975
1247.936385	77144.058846	35.596992
1249.270782	77231.358984	35.602010
1250.421254	77329.594884	35.607028
1251.821244	77407.447972	35.612045
1252.487488	77503.124988	35.617063
1253.367971	77600.808505	35.622080
1254.342720	77682.845600	35.627098
1255.464661	77780.150145	35.632116
1256.628992	77866.224668	35.637133
1257.913467	77967.051594	35.642151
1259.088825	78062.068595	35.647168
1260.376467	78160.463484	35.652186
1262.582629	78227.260909	35.657204
1264.017632	78307.948765	35.662221
1265.340643	78392.872785	35.667239
1266.682266	78477.578811	35.672256
1267.786407	78569.340264	35.677274
1268.627924	78653.921986	35.682292
1270.149610	78741.970562	35.687309
1271.149088	78841.388207	35.692327
1272.236045	78931.443315	35.697344
1273.586105	79022.597925	35.702362
1274.649951	79128.366145	35.707380
1275.804165	79230.180790	35.712397
1276.885442	79321.758282	35.717415
1278.232469	79436.250262	35.722432
1279.881165	79542.258420	35.727450
1280.454782	79653.501814	35.732468
1281.883253	79765.157352	35.737485
1283.254413	79865.863723	35.742503
1284.701712	79976.896412	35.747520
1285.821802	80087.296353	35.752538
1287.033394	80208.261090	35.757556
1288.384059	80315.623501	35.762573
1289.742330	80431.878838	35.767591
1291.070039	80546.479761	35.772608
1292.854059	80659.502498	35.777626
1293.384404	80774.785914	35.782644
1294.772358	80886.376247	35.787661
1296.250574	81002.425255	35.792679
1297.063850	81113.637180	35.797696
1298.755856	81241.322417	35.802714
1299.623335	81358.570206	35.807732
1300.992742	81478.096898	35.812749
1302.400941	81604.370966	35.817767
1303.891620	81730.886157	35.822784
1305.571152	81842.346228	35.827802
1306.970881	81960.679302	35.832820
1308.268101	82075.848702	35.837837
1309.590541	82201.251911	35.842855
1310.786173	82317.882480	35.847872
1312.608666	82419.287997	35.852890
1313.538970	82544.373669	35.857908
1315.210543	82658.587608	35.862925
1316.261469	82789.813254	35.867943
1317.815760	82895.151961	35.872960
1319.431226	83009.376050	35.877978
1320.583117	83118.541286	35.882996
1321.949039	83213.938979	35.888013
1323.322532	83337.666797	35.893031
1324.371514	83451.790785	35.898048
1325.829751	83565.674143	35.903066
1327.033841	83683.233961	35.908084
1328.623530	83782.057792	35.913101
1330.065085	83899.682907	35.918119
1331.401057	84016.399981	35.923136
1332.949891	84109.238068	35.928154
1334.100785	84222.715743	35.933172
1335.328732	84330.099875	35.938189
1336.732030	84430.982299	35.943207
1338.050603	84547.311451	35.948224
1340.078374	84654.293547	35.953242
1340.870127	84766.346773	35.958260
1342.036320	84867.394349	35.963277
1343.173606	84972.919683	35.968295
1344.545095	85074.290823	35.973312
1346.238408	85157.619124	35.978330
1347.200635	85254.480299	35.983348
1348.463849	85351.307623	35.988365
1349.683737	85458.646546	35.993383
1350.830645	85560.079696	35.998400
1352.806682	85653.337799	36.003418
1353.847227	85757.994068	36.008436
1355.246807	85857.120742	36.013453
1356.869334	85948.825543	36.018471
1358.078491	86057.511546	36.023488
1359.262361	86158.269447	36.028506
1360.592441	86275.566831	36.033524
1361.779281	86378.593267	36.038541
1363.704372	86482.746996	36.043559
1364.556506	86596.445252	36.048576
1365.742208	86706.531237	36.053594
1366.963063	86819.476021	36.058612
1368.337200	86933.537861	36.063629
1369.541718	87056.813767	36.068647
1371.009355	87177.121989	36.073664
1372.507933	87293.231416	36.078682
1373.544630	87426.457280	36.083700
1374.946512	87553.544234	36.088717
1376.222904	87686.353805	36.093735
1377.826979	87812.307920	36.098752
1379.686592	87939.730819	36.103770
1380.307307	88064.140970	36.108788
1381.972862	88181.672588	36.113805
1383.292368	88315.276660	36.118823
1384.811501	88445.124514	36.123840
1386.514199	88567.632233	36.128858
1387.455948	88700.701233	36.133876
1389.437517	88815.068698	36.138893
1391.217491	88936.742191	36.143911
1392.700570	89059.210096	36.148928
1394.792554	89155.984406	36.153946
1396.409404	89272.628172	36.158964
1397.839542	89380.557071	36.163981
1399.469533	89494.208830	36.168999
1400.252570	89607.853447	36.174016
1402.282108	89711.761587	36.179034
1403.246175	89827.039049	36.184052
1404.265474	89928.266386	36.189069
1405.942850	90046.678027	36.194087
1407.282236	90161.518165	36.199104
1408.940450	90273.546318	36.204122
1409.885744	90379.095661	36.209140
1411.332194	90505.389930	36.214157
1412.630147	90616.233438	36.219175
1413.888770	90744.205510	36.224192
1415.518343	90863.705084	36.229210
1416.566818	90979.024543	36.234228
1417.750898	91097.745250	36.239245
1419.573266	91219.522855	36.244263
1420.515852	91348.674660	36.249280
1422.319426	91470.215402	36.254298
1423.716208	91597.472536	36.259316
1424.954956	91716.275889	36.264333
1426.567457	91831.802325	36.269351
1427.880679	91965.258957	36.274368
1429.520308	92086.409451	36.279386
1430.959181	92204.917417	36.284404
1432.330881	92330.812726	36.289421
1433.753159	92445.103682	36.294439
1435.115544	92567.287847	36.299456
1436.505188	92684.905470	36.304474
1438.038004	92801.588702	36.309492
1439.281019	92916.352938	36.314509
1441.032054	93012.470310	36.319527
1442.029005	93121.354602	36.324544
1443.711782	93224.466971	36.329562
1444.864913	93343.442110	36.334580
1446.398721	93447.516346	36.339597
1447.711319	93569.585528	36.344615
1448.690319	93690.338238	36.349632
1450.357219	93803.797697	36.354650
1452.216217	93911.916882	36.359668
1453.431966	94026.296604	36.364685
1454.919877	94142.231442	36.369703
1456.516373	94272.624746	36.374720
1458.037838	94388.225736	36.379738
1459.503503	94507.397568	36.384756
1460.698006	94632.075085	36.389773
1462.438993	94756.427216	36.394791
1463.495817	94883.129868	36.399808
1465.082856	95010.194150	36.404826
1466.527509	95140.931638	36.409844
1467.777399	95283.222006	36.414861
1469.039379	95409.958256	36.419879
1470.969292	95547.961067	36.424896
1472.405946	95680.578060	36.429914
1473.826190	95819.345887	36.434932
1474.944133	95961.279621	36.439949
1476.594487	96097.528421	36.444967
1477.781049	96234.433093	36.449984
1479.398619	96373.869845	36.455002
1481.282760	96522.683985	36.460020
1482.398084	96671.669199	36.465037
1484.174194	96798.077539	36.470055
1485.943092	96942.817229	36.475072
1487.753708	97079.501697	36.480090
1489.268553	97212.290475	36.485108
1490.684185	97352.358787	36.490125
1492.466521	97488.859287	36.495143
1493.944986	97618.701843	36.500160
1494.980331	97748.246283	36.505178
1496.725030	97893.361721	36.510196
1498.270157	98028.164784	36.515213
1500.152466	98156.476204	36.520231
1501.303875	98292.507922	36.525248
1502.853366	98424.256905	36.530266
1504.589318	98562.467935	36.535284
1505.792148	98693.460672	36.540301
1507.855771	98837.795526	36.545319
1509.174214	98964.106276	36.550336
1511.092511	99090.843918	36.555354
1512.242914	99232.901386	36.560372
1513.626486	99370.689033	36.565389
1515.391709	99501.369358	36.570407
1516.967585	99627.946911	36.575424
1518.294160	99764.819683	36.580442
1519.812059	99892.852513	36.585460
1521.337660	100033.067619	36.590477
1522.952331	100163.545876	36.595495
1524.487330	100303.101468	36.600512
1525.890619	100437.378948	36.605530
1527.482229	100556.351173	36.610548
1529.001442	100697.837920	36.615565
1530.665468	100822.758348	36.620583
1531.880437	100956.509473	36.625600
1533.883511	101094.170026	36.630618
1535.261766	101217.501016	36.635636
1536.852423	101358.776677	36.640653
1538.446979	101493.142858	36.645671
1539.625390	101605.793551	36.650688
1541.549315	101718.442701	36.655706
1542.691076	101833.800309	36.660724
1543.728535	101961.814659	36.665741
1545.204745	102077.159105	36.670759
1546.611889	102201.021798	36.675776
1547.879912	102321.901860	36.680794
1549.659950	102457.181324	36.685812
1551.281216	102591.750711	36.690829
1552.858471	102725.642864	36.695847
1554.036393	102870.894245	36.700864
1555.947425	102998.421669	36.705882
1557.628199	103117.021666	36.710900
1559.035342	103261.313552	36.715917
1560.898026	103390.878599	36.720935
1562.161269	103532.709042	36.725952
1563.542764	103677.108161	36.730970
1565.602159	103812.197552	36.735988
1567.016982	103955.033194	36.741005
1568.692073	104078.734436	36.746023
1569.757468	104242.482575	36.751040
1571.292623	104382.917668	36.756058
1573.265249	104528.458342	36.761076
1574.551967	104676.921185	36.766093
1575.968617	104817.528698	36.771111
1577.365544	104975.206189	36.776128
1578.926799	105129.473458	36.781146
1580.727005	105290.906147	36.786164
1582.622881	105446.695036	36.791181
1584.115275	105599.200051	36.796199
1585.687774	105751.769365	36.801216
1586.979828	105915.579140	36.806234
1589.110648	106075.036818	36.811252
1590.430995	106220.648298	36.816269
1592.518012	106375.600216	36.821287
1594.322854	106525.867168	36.826304
1595.692442	106665.690872	36.831322
1597.704600	106824.435105	36.836340
1599.090212	106976.202133	36.841357
1601.071507	107128.675969	36.846375
1602.469636	107269.676955	36.851392
1603.725982	107425.003857	36.856410
1605.525275	107580.551282	36.861428
1607.103156	107732.621427	36.866445
1609.069296	107880.675539	36.871463
1610.597607	108031.562766	36.876480
1612.012492	108180.553555	36.881498
1613.594746	108338.636246	36.886516
1615.241388	108502.390546	36.891533
1617.171584	108643.225587	36.896551
1619.176246	108785.964397	36.901568
1620.905434	108924.321088	36.906586
1622.809031	109072.364683	36.911604
1624.544460	109218.127166	36.916621
1626.112631	109347.278937	36.921639
1628.331882	109483.279017	36.926656
1629.714109	109614.692569	36.931674
1631.078973	109740.783276	36.936692
1632.403999	109885.382364	36.941709
1634.639657	110025.338507	36.946727
1636.531435	110159.375885	36.951744
1637.855342	110295.518479	36.956762
1638.853054	110428.250375	36.961780
1640.702370	110580.075154	36.966797
1642.624252	110713.919743	36.971815
1644.095133	110844.905620	36.976832
1645.553000	110982.120625	36.981850
1647.229546	111113.772972	36.986868
1648.431834	111249.836729	36.991885
1650.096923	111376.875739	36.996903
1651.318580	111504.402716	37.001920
1652.061271	111648.313407	37.006938
1653.704309	111782.459074	37.011956
1655.307776	111932.856835	37.016973
1657.136509	112073.594617	37.021991
1658.535016	112223.289954	37.027008
1659.795662	112388.441365	37.032026
1661.605340	112534.624507	37.037044
1663.226128	112695.333291	37.042061
1664.543806	112847.757791	37.047079
1666.371575	113009.133284	37.052096
1667.883711	113170.888365	37.057114
1669.775963	113334.373220	37.062132
1671.732728	113508.501984	37.067149
1673.354147	113669.849140	37.072167
1675.722633	113828.683747	37.077184
1677.024124	113984.780813	37.082202
1678.675435	114146.341042	37.087220
1680.419229	114317.767397	37.092237
1682.010427	114482.382316	37.097255
1683.864830	114645.130692	37.102272
1685.292899	114817.128530	37.107290
1687.187665	114986.708201	37.112308
1689.137794	115152.056614	37.117325
1690.636586	115321.902393	37.122343
1692.639886	115497.352457	37.127360
1693.942148	115669.386554	37.132378
1695.777707	115826.093245	37.137396
1697.794655	116012.717537	37.142413
1699.080220	116168.648821	37.147431
1701.366918	116339.543522	37.152448
1703.462952	116512.510720	37.157466
1705.399060	116669.598520	37.162484
1706.893245	116830.814498	37.167501
1708.982970	116994.107378	37.172519
1710.708142	117155.491747	37.177536
1712.330362	117319.784722	37.182554
1713.974658	117482.197785	37.187572
1715.615504	117653.693703	37.192589
1717.186662	117816.309853	37.197607
1719.174757	117983.072880	37.202624
1720.758583	118156.190824	37.207642
1722.345041	118323.208126	37.212660
1724.075870	118498.955728	37.217677
1725.657158	118663.438518	37.222695
1727.184423	118828.222167	37.227712
1728.753941	119007.244391	37.232730
1730.884343	119175.880486	37.237748
1731.777888	119350.252908	37.242765
1733.634505	119541.448025	37.247783
1735.676451	119712.941579	37.252800
1737.042233	119905.978058	37.257818
1739.219924	120075.498685	37.262836
1741.076736	120253.518002	37.267853
1742.469962	120433.563746	37.272871
1744.293005	120606.757064	37.277888
1746.037115	120796.441080	37.282906
1748.013634	120975.320353	37.287924
1749.758368	121165.120243	37.292941
1751.137968	121340.643790	37.297959
1753.161106	121524.262545	37.302976
1754.340998	121712.085345	37.307994
1756.426171	121891.560812	37.313012
1758.120869	122077.250238	37.318029
1759.866132	122264.454916	37.323047
1761.789108	122448.956209	37.328064
1763.213691	122620.926592	37.333082
1765.037597	122785.033988	37.338100
1766.418291	122951.266108	37.343117
1768.091853	123132.841002	37.348135
1769.743213	123295.899098	37.353152
1771.544234	123480.462253	37.358170
1773.274889	123654.444585	37.363188
1775.156759	123839.935575	37.368205
1777.159477	124004.540313	37.373223
1778.606183	124191.572232	37.378240
1780.415245	124382.646214	37.383258
1782.301226	124558.764937	37.388276
1784.061795	124742.109676	37.393293
1785.648456	124922.298084	37.398311
1787.840642	125113.962913	37.403328
1789.187821	125308.754137	37.408346
1790.889161	125497.706193	37.413364
1792.899050	125702.634071	37.418381
1794.594975	125890.408963	37.423399
1796.735738	126084.217719	37.428416
1798.186136	126284.871436	37.433434
1800.316264	126481.487479	37.438452
1802.045252	126680.463198	37.443469
1804.020971	126880.226125	37.448487
1805.866017	127073.565436	37.453504
1807.689680	127276.500296	37.458522
1809.604808	127482.847404	37.463540
1811.249301	127672.871376	37.468557
1812.804311	127876.282352	37.473575
1814.998199	128074.659585	37.478592
1816.932935	128285.498894	37.483610
1818.654221	128485.093490	37.488628
1820.500535	128683.946401	37.493645
1822.278387	128891.666726	37.498663
1824.404942	129092.089261	37.503680
1826.208952	129297.599903	37.508698
1827.917538	129504.217534	37.513716
1829.713067	129713.385551	37.518733
1831.757837	129922.274746	37.523751
1833.512894	130119.296232	37.528768
1835.616171	130332.885510	37.533786
1837.610281	130530.645657	37.538804
1839.912259	130732.101753	37.543821
1841.948828	130908.439766	37.548839
1844.478479	131092.898256	37.553856
1846.132576	131285.461952	37.558874
1848.349781	131468.600367	37.563892
1849.624996	131658.953517	37.568909
1851.454173	131862.924648	37.573927
1853.365721	132046.696751	37.578944
1855.234070	132243.570791	37.583962
1856.870934	132431.536384	37.588980
1858.189448	132629.449380	37.593997
1859.827434	132838.517568	37.599015
1862.106196	133034.747633	37.604032
1863.873399	133239.965659	37.609050
1865.702248	133439.693508	37.614068
1867.522639	133639.119049	37.619085
1869.052384	133850.429443	37.624103
1870.633654	134045.858975	37.629120
1872.310207	134253.506722	37.634138
1874.240093	134472.637669	37.639156
1876.340413	134679.244395	37.644173
1877.884117	134903.766992	37.649191
1879.670925	135120.119080	37.654208
1881.290320	135336.980461	37.659226
1883.270358	135547.454771	37.664244
1885.202854	135757.277615	37.669261
1887.388425	135950.235810	37.674279
1889.315125	136151.026485	37.679296
1890.617886	136349.415309	37.684314
1892.867104	136548.089144	37.689332
1894.562672	136734.502948	37.694349
1896.357065	136948.083559	37.699367
1898.445639	137148.904200	37.704384
1899.787873	137361.668826	37.709402
1901.716524	137564.851111	37.714420
1903.376102	137778.964166	37.719437
1905.040275	138005.919813	37.724455
1907.341779	138216.864001	37.729472
1908.605586	138448.541391	37.734490
1910.590607	138667.747414	37.739508
1912.526690	138899.436627	37.744525
1914.145228	139135.414983	37.749543
1916.061185	139359.101995	37.754560
1918.011171	139596.325502	37.759578
1919.886780	139847.280245	37.764596
1922.228545	140081.196436	37.769613
1924.324336	140317.779031	37.774631
1926.075181	140555.165240	37.779648
1927.609826	140802.523167	37.784666
1929.606519	141046.257021	37.789684
1932.066688	141277.495573	37.794701
1933.881337	141530.689569	37.799719
1935.870010	141775.925904	37.804736
1938.261042	142013.549651	37.809754
1940.282001	142263.783727	37.814772
1942.385035	142504.411741	37.819789
1944.538118	142749.855845	37.824807
1946.276421	142985.948742	37.829824
1948.447447	143226.671255	37.834842
1950.383519	143468.231075	37.839860
1952.750078	143710.715018	37.844877
1954.260634	143944.119264	37.849895
1956.423580	144184.784240	37.854912
1958.449148	144427.489744	37.859930
1960.449817	144666.951203	37.864948
1962.807512	144906.269398	37.869965
1964.648648	145145.504132	37.874983
1967.074992	145379.267528	37.880000
1968.752029	145614.874738	37.885018
1971.047763	145855.742813	37.890036
1972.753743	146091.373112	37.895053
1974.283984	146331.055280	37.900071
1976.558523	146566.104285	37.905088
1978.564428	146807.999261	37.910106
1980.013639	147054.881274	37.915124
1982.283904	147294.300450	37.920141
1984.110019	147551.013586	37.925159
1986.099992	147781.771576	37.930176
1988.211774	148036.145291	37.935194
1990.406374	148279.033167	37.940212
1993.036900	148521.219687	37.945229
1994.870788	148784.182494	37.950247
1996.904106	149024.306494	37.955264
1998.353835	149249.290905	37.960282
2000.417215	149494.984547	37.965300
2002.776605	149737.955022	37.970317
2004.998106	149981.773113	37.975335
2007.607146	150206.035327	37.980352
2009.380369	150427.432962	37.985370
2011.612547	150661.707192	37.990388
2013.520709	150895.207798	37.995405
2015.231760	151126.226800	38.000423
2016.979218	151350.945183	38.005440
2019.233600	151590.208468	38.010458
2020.602511	151806.216450	38.015476
2022.653818	152016.102328	38.020493
2024.289308	152245.576499	38.025511
2025.775660	152469.845042	38.030528
2027.591327	152694.774087	38.035546
2029.504119	152932.293841	38.040564
2031.562637	153164.219336	38.045581
2033.367809	153408.955264	38.050599
2035.522373	153647.049728	38.055616
2037.400106	153898.288480	38.060634
2039.747031	154137.319817	38.065652
2041.662459	154377.155573	38.070669
2043.237887	154639.437743	38.075687
2045.543635	154889.294067	38.080704
2047.482157	155147.828040	38.085722
2049.422643	155409.384117	38.090740
2051.775805	155653.079629	38.095757
2053.514187	155914.339387	38.100775
2055.859072	156178.146381	38.105792
2058.415656	156438.760675	38.110810
2060.253728	156703.715256	38.115828
2062.407570	156966.755769	38.120845
2064.120000	157237.800351	38.125863
2065.782652	157494.432649	38.130880
2067.674702	157782.424678	38.135898
2069.563685	158051.972883	38.140916
2072.378582	158333.971592	38.145933
2074.215178	158603.885881	38.150951
2076.254966	158879.431751	38.155968
2078.359061	159169.352440	38.160986
2080.557350	159461.379943	38.166004
2082.611155	159740.558340	38.171021
2084.512418	160034.653337	38.176039
2086.394643	160317.631553	38.181056
2089.050743	160599.868542	38.186074
2090.915331	160912.165942	38.191092
2092.988704	161195.626207	38.196109
2095.430876	161474.015589	38.201127
2097.496036	161785.232366	38.206144
2099.628300	162069.398337	38.211162
2101.506509	162357.261495	38.216180
2103.700758	162647.984104	38.221197
2105.762326	162944.543391	38.226215
2107.851003	163243.080385	38.231232
2110.467734	163540.305055	38.236250
2112.105946	163832.833468	38.241268
2114.316982	164130.834935	38.246285
2116.306795	164430.763907	38.251303
2118.537572	164726.098785	38.256320
2121.089698	165027.136381	38.261338
2122.982630	165318.819141	38.266356
2125.140396	165611.744286	38.271373
2127.404282	165917.096713	38.276391
2129.988136	166211.507105	38.281408
2131.854318	166506.766859	38.286426
2133.966049	166802.548320	38.291444
2136.407008	167095.664295	38.296461
2138.493006	167380.812419	38.301479
2140.560284	167684.870132	38.306496
2143.048227	167978.795104	38.311514
2144.766840	168272.244281	38.316532
2147.297772	168558.927752	38.321549
2149.032781	168860.274307	38.326567
2151.560363	169143.837192	38.331584
2153.618744	169434.876625	38.336602
2155.758899	169723.123829	38.341620
2158.518933	170001.206830	38.346637
2160.775401	170277.274216	38.351655
2162.775281	170538.196617	38.356672
2164.848175	170797.864240	38.361690
2166.864431	171068.461335	38.366708
2168.813729	171323.959900	38.371725
2170.866655	171599.936923	38.376743
2173.042062	171860.849345	38.381760
2174.981619	172134.230284	38.386778
2176.388789	172411.275786	38.391796
2178.671255	172685.900497	38.396813
2180.676422	172972.492485	38.401831
2183.117821	173257.303453	38.406848
2185.176531	173535.851525	38.411866
2187.274876	173836.717224	38.416884
2189.512643	174122.363010	38.421901
2191.859972	174416.652770	38.426919
2193.678933	174703.902287	38.431936
2195.872316	175005.011604	38.436954
2198.243050	175307.961068	38.441972
2200.173760	175613.824530	38.446989
2202.304208	175921.258030	38.452007
2204.135185	176235.672520	38.457024
2206.441494	176545.392070	38.462042
2208.719609	176861.859973	38.467060
2211.456677	177169.267213	38.472077
2213.801214	177480.495401	38.477095
2216.087286	177798.946560	38.482112
2218.128125	178103.595712	38.487130
2220.277823	178437.334083	38.492148
2222.378523	178756.325604	38.497165
2224.845437	179077.623255	38.502183
2226.502135	179402.222856	38.507200
2229.357710	179717.316205	38.512218
2231.918264	180038.653598	38.517236
2234.539168	180347.842680	38.522253
2237.008904	180661.221586	38.527271
2239.160591	180983.210147	38.532288
2241.679029	181299.148864	38.537306
2243.625453	181622.035155	38.542324
2245.868566	181931.186831	38.547341
2248.115689	182250.523582	38.552359
2250.358315	182572.427350	38.557376
2253.159563	182886.676571	38.562394
2255.069311	183207.948552	38.567412
2257.358645	183537.747241	38.572429
2259.600307	183850.562807	38.577447
2262.192832	184163.248582	38.582464
2264.599295	184482.872779	38.587482
2266.509521	184813.369754	38.592500
2268.711381	185128.633878	38.597517
2270.853603	185456.023607	38.602535
2272.930448	185812.201759	38.607552
2275.405218	186185.692281	38.612570
2277.552246	186510.976520	38.617588
2279.773723	186839.577510	38.622605
2281.565522	187175.536042	38.627623
2283.871329	187510.221874	38.632640
2286.462927	187845.321476	38.637658
2288.828461	188165.725492	38.642676
2291.426209	188487.796102	38.647693
2293.809813	188811.094782	38.652711
2295.914314	189143.175414	38.657728
2298.832398	189463.751233	38.662746
2301.276031	189791.259822	38.667764
2302.901376	190115.975692	38.672781
2305.368018	190446.860807	38.677799
2307.388635	190771.872623	38.682816
2309.764849	191098.684232	38.687834
2312.073741	191423.576798	38.692852
2314.299493	191737.535589	38.697869
2316.191836	192046.898793	38.702887
2318.373446	192347.200557	38.707904
2320.695922	192651.189638	38.712922
2322.987854	192976.114428	38.717940
2325.087113	193273.942003	38.722957
2327.195519	193595.467863	38.727975
2329.076493	193921.779909	38.732992
2331.462724	194251.595696	38.738010
2333.953314	194577.281115	38.743028
2336.578204	194910.312771	38.748045
2339.214665	195240.600142	38.753063
2341.316885	195567.897922	38.758080
2343.737361	195902.614954	38.763098
2345.514919	196236.747026	38.768116
2348.060402	196581.454402	38.773133
2350.587007	196930.255210	38.778151
2352.946720	197276.034667	38.783168
2355.523056	197615.888075	38.788186
2357.388762	197965.099086	38.793204
2359.728350	198314.542003	38.798221
2361.880883	198662.770167	38.803239
2364.595489	199018.252804	38.808256
2367.211844	199365.749960	38.813274
2369.224336	199723.934499	38.818292
2371.798234	200078.196785	38.823309
2374.388036	200439.646179	38.828327
2376.457709	200810.347508	38.833344
2379.092510	201175.347846	38.838362
2381.676053	201539.137659	38.843380
2384.075245	201910.984082	38.848397
2386.039960	202273.398447	38.853415
2388.686501	202642.007262	38.858432
2391.300614	203014.127439	38.863450
2393.358211	203384.709237	38.868468
2395.677701	203752.329739	38.873485
2398.046173	204129.316921	38.878503
2400.530880	204498.386537	38.883520
2402.642707	204887.887884	38.888538
2405.189718	205271.327230	38.893556
2407.382769	205653.780888	38.898573
2409.912613	206033.185317	38.903591
2412.339025	206433.513148	38.908608
2414.734058	206823.558422	38.913626
2417.140323	207202.450734	38.918644
2419.248580	207598.613355	38.923661
2422.253461	207992.528684	38.928679
2424.678866	208380.057071	38.933696
2427.185931	208766.557266	38.938714
2429.646376	209163.734699	38.943732
2432.536027	209537.957636	38.948749
2435.189689	209923.496928	38.953767
2437.760396	210311.056575	38.958784
2440.619297	210684.727102	38.963802
2443.377624	211051.529474	38.968820
2445.964921	211423.871500	38.973837
2448.769722	211787.009511	38.978855
2451.245768	212164.806160	38.983872
2453.566688	212530.586149	38.988890
2456.267358	212894.097366	38.993908
2458.608786	213253.600333	38.998925
2461.032106	213615.961566	39.003943
2463.299650	213977.102656	39.008960
2465.822290	214339.118960	39.013978
2468.161339	214707.515133	39.018996
2470.618836	215065.376098	39.024013
2472.719803	215426.290529	39.029031
2475.010729	215785.524486	39.034048
2477.603960	216144.279852	39.039066
2479.853008	216492.622711	39.044084
2482.002321	216841.870504	39.049101
2484.652553	217172.063926	39.054119
2486.665570	217531.342576	39.059136
2489.008003	217891.332341	39.064154
2491.243102	218243.184405	39.069172
2493.182146	218614.669207	39.074189
2495.627771	218978.327214	39.079207
2497.930209	219364.871297	39.084224
2500.135212	219744.673322	39.089242
2502.302845	220127.428243	39.094260
2504.456420	220529.695837	39.099277
2506.920529	220921.601283	39.104295
2509.727682	221326.866860	39.109312
2512.070690	221726.107881	39.114330
2514.933358	222128.265870	39.119348
2517.290537	222539.114652	39.124365
2520.337233	222943.860905	39.129383
2522.282700	223365.443728	39.134400
2524.975789	223773.369936	39.139418
2527.437657	224184.152066	39.144436
2530.187415	224619.556839	39.149453
2532.679940	225024.135724	39.154471
2535.166424	225461.207424	39.159488
2538.124083	225876.231272	39.164506
2541.262024	226291.785955	39.169524
2543.590196	226717.602872	39.174541
2546.343055	227127.806355	39.179559
2549.047785	227546.908708	39.184576
2551.870085	227972.496138	39.189594
2554.426240	228382.425172	39.194612
2557.196475	228793.692607	39.199629
2560.255241	229209.792599	39.204647
2562.753909	229622.372237	39.209664
2565.691111	230029.828068	39.214682
2568.459194	230450.926611	39.219700
2570.933163	230870.698907	39.224717
2573.395952	231273.934719	39.229735
2575.882226	231683.949527	39.234752
2578.483497	232091.761457	39.239770
2581.653070	232507.740981	39.244788
2583.899762	232918.300380	39.249805
2586.522742	233325.345996	39.254823
2589.063069	233741.041499	39.259840
2591.539297	234147.321803	39.264858
2594.340631	234564.169994	39.269876
2596.629067	234979.878247	39.274893
2599.449338	235396.240061	39.279911
2601.982112	235811.807886	39.284928
2604.268052	236232.697685	39.289946
2607.072188	236648.654279	39.294964
2609.501180	237077.142016	39.299981
2612.098046	237494.704947	39.304999
2614.483277	237921.648858	39.310016
2617.299223	238348.931660	39.315034
2619.753673	238777.006864	39.320052
2622.217994	239208.788870	39.325069
2624.987514	239634.756175	39.330087
2627.551958	240056.969665	39.335104
2630.159339	240488.651333	39.340122
2632.751832	240914.669694	39.345140
2635.471239	241353.699556	39.350157
2638.348134	241787.039240	39.355175
2640.950091	242220.344767	39.360192
2643.436808	242649.475945	39.365210
2645.913511	243071.850678	39.370228
2648.605992	243494.089467	39.375245
2651.247613	243910.721319	39.380263
2653.318635	244320.048916	39.385280
2655.891719	244725.766609	39.390298
2658.718774	245122.552987	39.395316
2661.122789	245554.714480	39.400333
2663.769889	245953.813549	39.405351
2666.018463	246383.406398	39.410368
2668.841383	246800.029752	39.415386
2671.999843	247220.486608	39.420404
2674.066526	247653.686741	39.425421
2677.110127	248073.600718	39.430439
2680.184300	248499.173737	39.435456
2682.762543	248917.837255	39.440474
2685.401691	249339.513189	39.445492
2687.974823	249767.675966	39.450509
2691.143577	250184.644192	39.455527
2693.908132	250629.515086	39.460544
2696.886858	251059.389600	39.465562
2699.550783	251486.492334	39.470580
2702.393552	251917.274781	39.475597
2705.313354	252340.499685	39.480615
2707.640977	252771.563146	39.485632
2710.025595	253213.463069	39.490650
2712.883507	253657.599585	39.495668
2715.568807	254101.329792	39.500685
2718.070652	254550.726327	39.505703
2720.519370	254994.668397	39.510720
2723.428082	255450.171307	39.515738
2726.198048	255913.771915	39.520756
2728.900870	256369.634022	39.525773
2731.661152	256830.235643	39.530791
2734.625267	257288.797253	39.535808
2736.740920	257749.394350	39.540826
2740.310070	258202.575159	39.545844
2742.724210	258671.199934	39.550861
2745.938245	259132.027466	39.555879
2749.051375	259604.121418	39.560896
2751.600609	260067.106313	39.565914
2754.769956	260518.816751	39.570932
2757.390007	260987.654513	39.575949
2760.387419	261423.767049	39.580967
2763.344617	261890.135665	39.585984
2766.040859	262350.700979	39.591002
2768.779969	262803.612369	39.596020
2771.824992	263266.202400	39.601037
2774.657548	263720.467052	39.606055
2777.941992	264175.040459	39.611072
2780.468897	264627.139071	39.616090
2783.386543	265071.834533	39.621108
2785.934342	265524.764194	39.626125
2788.658534	265980.356715	39.631143
2791.584656	266436.957129	39.636160
2794.588723	266897.251574	39.641178
2797.027515	267349.199471	39.646196
2799.964441	267812.192373	39.651213
2803.001956	268258.734582	39.656231
2805.815287	268714.249839	39.661248
2808.676492	269167.723605	39.666266
2811.579299	269612.629539	39.671284
2814.338570	270070.762659	39.676301
2817.009334	270533.478899	39.681319
2819.916139	270986.250933	39.686336
2822.156586	271447.175449	39.691354
2824.947516	271889.116180	39.696372
2827.817264	272359.030355	39.701389
2830.768350	272820.675251	39.706407
2833.475404	273284.108071	39.711424
2835.931908	273734.599532	39.716442
2838.339842	274173.058068	39.721460
2840.960000	274612.827328	39.726477
2843.524954	275063.371014	39.731495
2846.149142	275497.827090	39.736512
2848.336954	275959.751384	39.741530
2851.222461	276421.412108	39.746548
2853.666700	276889.970383	39.751565
2856.171151	277353.488164	39.756583
2858.943483	277828.440404	39.761600
2861.619334	278315.213712	39.766618
2864.413837	278802.346440	39.771636
2867.056226	279298.972177	39.776653
2870.250093	279798.302320	39.781671
2873.085520	280294.028081	39.786688
2875.802137	280797.666809	39.791706
2878.804281	281307.860267	39.796724
2881.468670	281817.264734	39.801741
2884.748018	282325.630358	39.806759
2887.550106	282844.249669	39.811776
2890.239843	283365.650632	39.816794
2893.303512	283886.811817	39.821812
2896.313442	284416.687449	39.826829
2899.038296	284942.692854	39.831847
2902.231764	285467.326281	39.836864
2905.248690	286000.845264	39.841882
2908.221657	286526.977628	39.846900
2911.668585	287056.714023	39.851917
2914.708064	287582.726167	39.856935
2917.790925	288114.008918	39.861952
2920.532010	288648.082865	39.866970
2923.987458	289169.904054	39.871988
2926.736639	289704.450459	39.877005
2929.885196	290233.978956	39.882023
2933.256024	290754.505413	39.887040
2936.351326	291281.468913	39.892058
2939.421715	291802.845907	39.897076
2942.225908	292333.654362	39.902093
2945.246075	292873.260382	39.907111
2948.642491	293379.593058	39.912128
2952.051877	293900.010754	39.917146
2955.369294	294402.360929	39.922164
2958.662269	294917.278352	39.927181
2961.377570	295422.582563	39.932199
2964.941582	295930.898558	39.937216
2967.813707	296435.052494	39.942234
2970.724553	296934.727648	39.947252
2973.574705	297437.022874	39.952269
2976.753456	297937.231499	39.957287
2980.135484	298441.364550	39.962304
2983.263160	298943.298557	39.967322
2986.473076	299434.425662	39.972340
2989.626810	299919.159622	39.977357
2992.563676	300411.716811	39.982375
2996.018890	300893.247280	39.987392
2999.101920	301390.418621	39.992410
3001.713791	301869.482235	39.997428
3005.101931	302358.803602	40.002445
3007.362988	302852.433729	40.007463
3010.426150	303334.180981	40.012480
3013.098363	303829.108802	40.017498
3015.792510	304316.692274	40.022516
3019.109886	304817.881928	40.027533
3021.927230	305310.031505	40.032551
3025.130464	305805.416257	40.037568
3027.622991	306293.926198	40.042586
3031.068144	306793.375875	40.047604
3033.576062	307301.596823	40.052621
3036.584289	307796.865465	40.057639
3039.454533	308261.843380	40.062656
3041.567498	308746.149495	40.067674
3044.847902	309217.171808	40.072692
3047.381278	309711.302134	40.077709
3049.823814	310184.095331	40.082727
3053.158066	310677.025136	40.087744
3055.674027	311189.722466	40.092762
3058.411719	311697.328932	40.097780
3061.209278	312212.001926	40.102797
3064.189833	312736.590033	40.107815
3066.953941	313248.033557	40.112832
3070.614080	313780.702042	40.117850
3074.004896	314303.584344	40.122868
3077.097936	314835.364483	40.127885
3080.086847	315371.519866	40.132903
3082.812312	315902.558016	40.137920
3085.489258	316437.835706	40.142938
3088.598101	317003.493733	40.147956
3091.976632	317560.271110	40.152973
3094.671072	318117.249472	40.157991
3097.930616	318674.361265	40.163008
3100.865037	319240.297010	40.168026
3103.980083	319799.269480	40.173044
3107.129886	320382.590592	40.178061
3110.112427	320967.173256	40.183079
3113.471431	321542.071999	40.188096
3116.739264	322123.194103	40.193114
3119.895905	322700.214790	40.198132
3123.321955	323288.096698	40.203149
3126.786994	323872.792492	40.208167
3129.622198	324456.613861	40.213184
3132.953123	325043.217039	40.218202
3136.031008	325629.825838	40.223220
3139.470431	326215.862488	40.228237
3142.219723	326814.735006	40.233255
3145.671940	327397.986945	40.238272
3148.598646	327995.621782	40.243290
3151.733817	328601.029567	40.248308
3155.390424	329183.969847	40.253325
3158.247525	329791.736777	40.258343
3161.640610	330398.319956	40.263360
3164.856201	330985.741807	40.268378
3168.309427	331592.119386	40.273396
3171.682808	332190.711579	40.278413
3174.742077	332785.436537	40.283431
3178.408230	333376.227175	40.288448
3181.286384	333979.941915	40.293466
3184.886613	334574.300904	40.298484
3188.204061	335164.635750	40.303501
3191.729066	335754.244038	40.308519
3194.722103	336344.864263	40.313536
3197.875796	336943.440212	40.318554
3201.309670	337523.725134	40.323572
3204.913355	338112.801369	40.328589
3207.825818	338697.359255	40.333607
3211.051995	339279.956541	40.338624
3214.427866	339875.101438	40.343642
3217.195054	340459.526392	40.348660
3221.052021	341042.098194	40.353677
3223.811055	341627.392837	40.358695
3227.186848	342203.172463	40.363712
3230.403852	342798.698598	40.368730
3233.851570	343384.617495	40.373748
3237.631537	343962.891922	40.378765
3240.342666	344548.931037	40.383783
3243.926163	345125.136924	40.388800
3246.861696	345707.342642	40.393818
3249.349912	346277.308881	40.398836
3252.868351	346831.940776	40.403853
3256.127239	347368.903924	40.408871
3259.590893	347926.493138	40.413888
3262.683271	348472.643933	40.418906
3265.440808	349023.072436	40.423924
3269.177946	349570.093694	40.428941
3271.830229	350122.700852	40.433959
3275.124006	350675.680607	40.438976
3278.176022	351246.589340	40.443994
3281.368532	351812.040246	40.449012
3284.544061	352388.969369	40.454029
3287.801650	352959.156599	40.459047
3290.656077	353538.117953	40.464064
3293.789201	354125.442566	40.469082
3296.805011	354724.183131	40.474100
3300.498795	355324.378646	40.479117
3303.569721	355924.330037	40.484135
3307.494924	356519.903360	40.489152
3310.627992	357124.410499	40.494170
3314.100461	357727.179920	40.499188
3317.538071	358324.188640	40.504205
3320.694533	358934.385603	40.509223
3324.292731	359540.699361	40.514240
3327.661378	360157.809618	40.519258
3330.872185	360774.374202	40.524276
3334.427117	361382.432087	40.529293
3337.907022	361998.143919	40.534311
3341.294868	362624.274519	40.539328
3344.673721	363238.962571	40.544346
3347.576842	363876.978395	40.549364
3351.393117	364493.168956	40.554381
3354.381030	365136.517194	40.559399
3358.068706	365768.540675	40.564416
3361.177733	366399.347962	40.569434
3364.559966	367038.411150	40.574452
3367.822663	367672.410442	40.579469
3371.246655	368322.943547	40.584487
3374.869430	368966.335575	40.589504
3378.077822	369607.598272	40.594522
3381.558900	370254.733340	40.599540
3385.464586	370898.620110	40.604557
3388.927921	371544.131851	40.609575
3392.234294	372183.774778	40.614592
3396.108227	372835.096259	40.619610
3399.466343	373471.483588	40.624628
3403.194905	374106.075712	40.629645
3406.016929	374753.360380	40.634663
3409.816569	375408.635238	40.639680
3413.376159	376047.717963	40.644698
3416.567556	376702.549469	40.649716
3419.923990	377350.854199	40.654733
3423.345700	377992.192104	40.659751
3426.577964	378624.754062	40.664768
3430.310773	379274.523995	40.669786
3434.209950	379936.030589	40.674804
3437.695693	380560.249154	40.679821
3441.280097	381211.615448	40.684839
3444.851681	381856.584751	40.689856
3448.410577	382496.626454	40.694874
3451.633387	383134.171923	40.699892
3455.202339	383779.574929	40.704909
3458.597732	384416.555231	40.709927
3462.196891	385057.464002	40.714944
3465.420762	385700.314375	40.719962
3469.187169	386343.545182	40.724980
3472.603153	386979.850245	40.729997
3475.733384	387612.917065	40.735015
3478.875149	388232.588007	40.740020
3482.111944	388825.568183	40.745024
3485.288916	389386.583144	40.750029
3488.528660	389888.428580	40.755034
3491.003077	390348.853808	40.760039
3493.470614	390766.423131	40.765044
3496.279067	391132.682568	40.770048
3498.436331	391461.115079	40.775053
3500.744065	391737.179823	40.780058
3502.823488	391978.096337	40.785063
3504.523213	392180.538705	40.790068
3506.162614	392351.920639	40.795072
3507.495169	392478.625454	40.800077
3509.200702	392572.731543	40.805082
3510.723568	392633.665814	40.810087
3511.614050	392666.118049	40.815092
3512.768057	392675.583787	40.820096
3513.221270	392668.660181	40.825101
3513.913409	392629.514796	40.830106
3514.630267	392578.435850	40.835111
3515.261484	392494.576174	40.840116
3515.827932	392400.725613	40.845120
3516.278971	392310.953855	40.850125
3516.570065	392185.264845	40.855130
3516.954029	392056.971691	40.860135
3517.175035	391934.541294	40.865140
3517.128369	391777.986339	40.870144
3517.150099	391632.892959	40.875149
3517.357572	391463.401761	40.880154
3517.012505	391307.144063	40.885159
3517.597769	391141.653222	40.890164
3517.668791	390959.894048	40.895168
3517.187703	390775.681033	40.900173
3517.488666	390584.034261	40.905178
3517.334788	390399.462900	40.910183
3517.298971	390207.256378	40.915188
3516.943624	390019.235819	40.920192
3516.932689	389836.567258	40.925197
3516.396200	389644.561195	40.930202
3516.730993	389451.529569	40.935207
3516.319327	389269.756908	40.940212
3516.197084	389075.118021	40.945216
3515.979952	388884.503373	40.950221
3516.282269	388700.609947	40.955226
3516.108117	388517.347810	40.960231
3515.765299	388326.951546	40.965236
3515.637215	388135.276462	40.970240
3515.097360	387944.781013	40.975245
3515.244033	387766.947041	40.980250
3514.994299	387582.242741	40.985255
3514.705358	387400.081939	40.990260
3514.809614	387228.597642	40.995264
3514.271406	387060.106374	41.000269
3514.373298	386880.267450	41.005274
3513.942409	386705.562414	41.010279
3513.878360	386539.304209	41.015284
3513.490437	386361.518106	41.020288
3513.295024	386193.754753	41.025293
3513.237278	386035.819773	41.030298
3512.936860	385867.029648	41.035303
3512.925380	385707.257407	41.040308
3512.687488	385545.970637	41.045312
3512.108928	385389.305981	41.050317
3512.409017	385229.913877	41.055322
3512.208018	385087.279910	41.060327
3511.928827	384932.723998	41.065332
3511.769939	384775.634801	41.070336
3511.622031	384634.081816	41.075341
3511.518096	384483.939223	41.080346
3510.987566	384348.080882	41.085351
3510.922266	384211.362311	41.090356
3510.931023	384067.801337	41.095360
3510.686156	383940.529284	41.100365
3510.876101	383798.233549	41.105370
3510.300682	383658.849170	41.110375
3510.228367	383529.186838	41.115380
3510.005719	383400.207427	41.120384
3509.845789	383281.831330	41.125389
3509.639996	383147.922050	41.130394
3509.420743	383033.083503	41.135399
3509.358050	382913.827261	41.140404
3509.432049	382792.390866	41.145408
3508.973699	382687.465535	41.150413
3509.056059	382565.874422	41.155418
3509.040890	382455.343647	41.160423
3508.798074	382351.881572	41.165428
3508.800553	382228.726969	41.170432
3508.610305	382127.388806	41.175437
3508.580319	382015.969717	41.180442
3508.191275	381907.602401	41.185447
3508.101235	381807.288510	41.190452
3508.142091	381705.049372	41.195456
3507.887030	381604.277906	41.200461
3507.682023	381502.812640	41.205466
3507.563392	381411.719481	41.210471
3507.549528	381320.381159	41.215476
3507.612584	381218.212839	41.220480
3507.306306	381120.469324	41.225485
3507.219905	381024.214860	41.230490
3507.410616	380951.888817	41.235495
3507.068854	380859.711122	41.240500
3507.543472	380769.818506	41.245504
3507.009520	380673.099120	41.250509
3507.138426	380587.475116	41.255514
3507.198040	380501.785432	41.260519
3506.917457	380410.206102	41.265524
3507.155167	380318.875929	41.270528
3506.674780	380246.703162	41.275533
3506.937464	380163.850370	41.280538
3506.877208	380078.965197	41.285543
3506.534984	379993.818890	41.290548
3506.624752	379901.011991	41.295552
3506.527883	379831.800407	41.300557
3506.535964	379750.636611	41.305562
3506.438252	379669.158891	41.310567
3506.259474	379590.233061	41.315572
3506.439882	379506.248220	41.320576
3505.899228	379437.764939	41.325581
3506.207323	379349.544092	41.330586
3506.040697	379276.837329	41.335591
3505.821077	379203.732284	41.340596
3505.784455	379133.493670	41.345600
3505.704788	379072.607208	41.350605
3506.093077	378994.911938	41.355610
3505.919005	378923.145010	41.360615
3505.864049	378861.670113	41.365620
3506.002673	378780.152880	41.370624
3505.852088	378706.756365	41.375629
3505.672429	378633.084813	41.380634
3505.962838	378570.641237	41.385639
3505.691394	378489.567868	41.390644
3505.728744	378426.604614	41.395648
3505.720305	378352.321525	41.400653
3505.366746	378284.618836	41.405658
3505.274427	378216.773738	41.410663
3505.505620	378148.065431	41.415668
3505.722805	378081.213088	41.420672
3505.424218	378027.393185	41.425677
3505.374165	377958.728157	41.430682
3505.278926	377896.723967	41.435687
3505.143168	377825.938596	41.440692
3505.380847	377761.698149	41.445696
3505.139590	377700.478136	41.450701
3505.150190	377637.821949	41.455706
3505.130292	377575.119566	41.460711
3505.124653	377514.421200	41.465716
3505.463645	377442.011705	41.470720
3504.983486	377385.094894	41.475725
3505.081243	377322.525996	41.480730
3505.354516	377267.320307	41.485735
3505.126383	377201.652552	41.490740
3504.903623	377135.704427	41.495744
3505.068873	377082.902543	41.500749
3504.911472	377012.677139	41.505754
3504.876272	376954.420287	41.510759
3504.562702	376893.946220	41.515764
3504.613744	376832.373965	41.520768
3504.708623	376786.897041	41.525773
3504.718758	376723.426057	41.530778
3504.717972	376676.566944	41.535783
3504.408683	376625.844452	41.540788
3504.800194	376561.754983	41.545792
3504.632884	376515.708846	41.550797
3504.603467	376451.989396	41.555802
3504.307590	376400.604038	41.560807
3504.204394	376347.537706	41.565812
3504.340320	376293.214936	41.570816
3504.231909	376246.219432	41.575821
3504.551868	376194.433069	41.580826
3504.581333	376152.470246	41.585831
3504.460709	376107.228899	41.590836
3504.507591	376039.153446	41.595840
3504.113806	375994.360796	41.600845
3504.349050	375941.088608	41.605850
3504.625778	375886.819308	41.610855
3504.068281	375843.321823	41.615860
3504.255413	375788.609089	41.620864
3504.471130	375738.641395	41.625869
3504.272799	375674.413021	41.630874
3504.462743	375635.878685	41.635879
3504.171151	375587.259606	41.640884
3504.059181	375530.814963	41.645888
3503.982572	375485.616527	41.650893
3504.022448	375432.424540	41.655898
3503.967019	375385.851085	41.660903
3503.796045	375342.775233	41.665908
3503.824156	375291.311952	41.670912
3503.958368	375253.496929	41.675917
3504.122971	375207.219120	41.680922
3504.043513	375164.230341	41.685927
3503.797012	375123.096253	41.690932
3503.716611	375062.810401	41.695936
3503.633043	375021.066613	41.700941
3503.962572	374975.423135	41.705946
3504.113590	374941.491206	41.710951
3503.896609	374897.126425	41.715956
3504.166461	374837.420563	41.720960
3504.075350	374795.068010	41.725965
3503.892307	374746.481335	41.730970
3503.868916	374705.591295	41.735975
3503.784117	374655.846176	41.740980
3504.125377	374606.796666	41.745984
3503.964771	374564.784769	41.750989
3504.088654	374517.978727	41.755994
3504.132925	374463.844364	41.760999
3504.100759	374409.112184	41.766004
3503.849518	374363.507259	41.771008
3503.986274	374329.322787	41.776013
3503.967418	374276.747291	41.781018
3503.850437	374233.813686	41.786023
3503.714571	374192.025969	41.791028
3503.838585	374151.061361	41.796032
3503.622350	374106.949184	41.801037
3503.887262	374054.506907	41.806042
3503.954600	374023.126909	41.811047
3503.958113	373976.389473	41.816052
3504.035298	373923.569749	41.821056
3503.728901	373899.334536	41.826061
3503.887663	373835.960686	41.831066
3503.600550	373792.341645	41.836071
3503.608440	373754.290198	41.841076
3504.062599	373700.928770	41.846080
3503.461157	373667.721974	41.851085
3503.854694	373622.244088	41.856090
3503.583709	373582.991156	41.861095
3503.723793	373542.150144	41.866100
3504.112751	373493.624642	41.871104
3503.663747	373451.147896	41.876109
3503.636589	373413.431645	41.881114
3503.644599	373360.316791	41.886119
3503.522450	373317.255551	41.891124
3503.506718	373276.743206	41.896128
3503.451218	373244.263782	41.901133
3503.559485	373195.552823	41.906138
3503.611414	373162.726369	41.911143
3503.285173	373131.965429	41.916148
3503.242306	373083.811219	41.921152
3503.138903	373050.348367	41.926157
3502.951857	373024.595126	41.931162
3503.482340	372988.620421	41.936167
3503.643582	372947.318009	41.941172
3503.455937	372898.347756	41.946176
3503.329364	372873.728034	41.951181
3503.543451	372820.910294	41.956186
3503.689102	372777.654129	41.961191
3503.474909	372746.900726	41.966196
3503.711166	372701.191780	41.971200
3503.388845	372666.949674	41.976205
3503.349251	372619.225976	41.981210
3503.656953	372586.714661	41.986215
3503.324062	372546.580823	41.991220
3503.466645	372502.486445	41.996224
3503.040710	372472.299126	42.001229
3503.129583	372438.831014	42.006234
3503.527133	372398.405482	42.011239
3503.443038	372358.588285	42.016244
3503.348238	372308.789674	42.021248
3503.158340	372279.149662	42.026253
3503.327778	372238.022733	42.031258
3503.760502	372202.240036	42.036263
3503.759419	372162.079411	42.041268
3503.286767	372116.327403	42.046272
3503.279828	372080.028714	42.051277
3503.377690	372038.175960	42.056282
3503.499262	371995.989223	42.061287
3503.138213	371961.599857	42.066292
3503.658719	371917.674362	42.071296
3503.180414	371896.309214	42.076301
3503.177803	371853.100083	42.081306
3503.180114	371820.101942	42.086311
3503.251894	371776.347662	42.091316
3503.400577	371731.387423	42.096320
3503.468169	371704.729642	42.101325
3503.117391	371659.389762	42.106330
3503.120795	371626.823067	42.111335
3502.993720	371593.616167	42.116340
3502.998076	371556.527553	42.121344
3503.019933	371523.678436	42.126349
3503.352581	371486.614852	42.131354
3503.175528	371450.468829	42.136359
3503.159780	371416.964963	42.141364
3503.573611	371372.750376	42.146368
3503.111992	371335.454548	42.151373
3503.362295	371295.660001	42.156378
3503.546409	371263.547420	42.161383
3503.308426	371229.798479	42.166388
3503.245196	371181.390109	42.171392
3503.396379	371154.972826	42.176397
3503.289345	371113.074359	42.181402
3503.671374	371087.992862	42.186407
3503.114703	371035.012237	42.191412
3503.473848	370992.914030	42.196416
3503.477725	370968.119901	42.201421
3503.480956	370926.305609	42.206426
3503.304583	370876.593344	42.211431
3503.257001	370844.846581	42.216436
3503.494287	370802.309790	42.221440
3503.182028	370766.260132	42.226445
3502.799929	370727.757154	42.231450
3503.236766	370691.590831	42.236455
3503.042567	370671.425308	42.241460
3503.192279	370632.255159	42.246464
3502.851483	370598.343630	42.251469
3503.003870	370558.182220	42.256474
3503.294544	370531.818854	42.261479
3502.648957	370496.227179	42.266484
3503.277951	370464.654144	42.271488
3503.087822	370434.605748	42.276493
3502.656414	370396.186198	42.281498
3503.169797	370362.141463	42.286503
3503.080708	370336.675338	42.291508
3503.281299	370296.023378	42.296512
3503.151918	370265.685906	42.301517
3503.108037	370227.409053	42.306522
3503.150320	370196.435097	42.311527
3502.935177	370159.734447	42.316532
3503.176256	370116.586331	42.321536
3502.980785	370087.630772	42.326541
3502.815625	370054.732824	42.331546
3503.184568	370026.172050	42.336551
3502.936371	369998.901279	42.341556
3503.002116	369955.881818	42.346560
3502.800011	369928.857849	42.351565
3502.693305	369893.283169	42.356570
3503.073396	369846.785047	42.361575
3502.976500	369824.723854	42.366580
3502.799284	369791.522623	42.371584
3502.803841	369755.778030	42.376589
3502.929972	369720.166900	42.381594
3502.971320	369681.469573	42.386599
3502.641561	369664.728622	42.391604
3503.009437	369627.834937	42.396608
3503.208855	369596.505611	42.401613
3502.931277	369563.472157	42.406618
3502.993711	369522.713560	42.411623
3502.754490	369494.932812	42.416628
3502.914941	369459.570060	42.421632
3503.044568	369430.918902	42.426637
3502.728941	369400.736505	42.431642
3502.883971	369379.702760	42.436647
3502.815276	369343.969046	42.441652
3502.628137	369314.046015	42.446656
3502.601696	369288.848648	42.451661
3502.667707	369255.761368	42.456666
3502.806225	369222.408716	42.461671
3502.626701	369199.928011	42.466676
3503.137559	369169.184872	42.471680
3502.468969	369133.391813	42.476685
3502.627809	369112.585923	42.481690
3502.798122	369082.784858	42.486695
3502.880125	369055.207742	42.491700
3502.957233	369014.750992	42.496704
3502.854658	368982.248538	42.501709
3502.687797	368950.137127	42.506714
3503.363648	368915.531864	42.511719
3503.180175	368887.868872	42.516724
3503.064352	368841.751134	42.521728
3502.973900	368818.138435	42.526733
3503.036974	368779.588928	42.531738
3502.866717	368753.397254	42.536743
3502.685286	368723.396495	42.541748
3502.756286	368701.257490	42.546752
3502.640538	368668.070782	42.551757
3502.612499	368630.373628	42.556762
3503.004330	368606.609488	42.561767
3502.866369	368581.225604	42.566772
3503.083372	368545.243183	42.571776
3502.904367	368510.389372	42.576781
3502.554325	368475.790784	42.581786
3502.808758	368444.299194	42.586791
3502.594703	368425.481653	42.591796
3502.733888	368383.820282	42.596800
3502.955042	368355.230015	42.601805
3502.810698	368327.789040	42.606810
3502.705106	368296.963048	42.611815
3502.891412	368272.671687	42.616820
3503.123528	368235.238396	42.621824
3503.076203	368200.363715	42.626829
3502.855135	368173.772922	42.631834
3502.991893	368136.964081	42.636839
3502.997132	368123.396634	42.641844
3502.738442	368081.364836	42.646848
3502.996054	368052.235069	42.651853
3502.670875	368014.126032	42.656858
3502.500409	367983.995759	42.661863
3502.520694	367965.624162	42.666868
3502.910409	367933.882304	42.671872
3502.685892	367904.598757	42.676877
3502.813294	367871.678158	42.681882
3502.900317	367848.011632	42.686887
3502.661340	367817.129661	42.691892
3503.027923	367769.741033	42.696896
3502.761537	367749.203569	42.701901
3502.544440	367705.081437	42.706906
3502.793461	367679.179220	42.711911
3502.711853	367657.063153	42.716916
3503.091900	367625.474896	42.721920
3502.827654	367593.681989	42.726925
3502.855284	367550.156694	42.731930
3503.073968	367516.916607	42.736935
3502.487411	367493.202168	42.741940
3502.778773	367466.327725	42.746944
3502.371317	367439.307938	42.751949
3502.614472	367412.059849	42.756954
3502.898486	367382.442570	42.761959
3502.217147	367359.073053	42.766964
3502.756766	367319.634411	42.771968
3502.735716	367292.376509	42.776973
3502.566201	367265.573598	42.781978
3502.552290	367229.269764	42.786983
3502.503787	367205.471358	42.791988
3502.656489	367180.371287	42.796993
3502.427766	367145.548956	42.801997
3502.791832	367132.839844	42.807002
3502.746035	367103.629295	42.812007
3502.669145	367070.333060	42.817012
3503.077089	367037.012154	42.822017
3502.948489	367008.602005	42.827021
3502.611488	366975.828868	42.832026
3502.652262	366934.790471	42.837031
3502.813295	366916.574149	42.842036
3502.569921	366883.151163	42.847041
3502.613164	366862.463253	42.852045
3502.628120	366823.359647	42.857050
3502.754537	366804.615093	42.862055
3502.573881	366780.913122	42.867060
3502.604341	366752.655819	42.872065
3502.700547	366726.319197	42.877069
3502.451252	366685.554248	42.882074
3502.676983	366656.529657	42.887079
3502.278510	366638.578076	42.892084
3502.660430	366607.598185	42.897089
3502.331111	366588.238415	42.902093
3502.691307	366551.875511	42.907098
3503.006726	366532.694855	42.912103
3502.786105	366502.596239	42.917108
3502.519978	366465.847953	42.922113
3502.136857	366434.631224	42.927117
3502.397029	366409.971092	42.932122
3502.362588	366387.694266	42.937127
3502.039039	366368.130191	42.942132
3502.481486	366336.429183	42.947137
3502.185360	366315.209320	42.952141
3502.221419	366296.681758	42.957146
3502.417173	366255.237167	42.962151
3502.299146	366241.433939	42.967156
3502.468933	366219.658761	42.972161
3502.386353	366195.128005	42.977165
3501.929857	366170.274301	42.982170
3502.329927	366145.719212	42.987175
3502.588473	366124.311266	42.992180
3502.796772	366091.782567	42.997185
3502.464721	366077.885527	43.002189
3502.319334	366049.045116	43.007194
3502.497202	366027.675060	43.012199
3502.507588	366001.198687	43.017204
3502.792915	365972.443622	43.022209
3502.727370	365943.489051	43.027213
3502.394481	365912.086086	43.032218
3502.890055	365882.256494	43.037223
3502.386426	365856.622212	43.042228
3502.404340	365824.681814	43.047233
3502.664158	365790.264577	43.052237
3502.539269	365776.233523	43.057242
3502.433352	365749.546347	43.062247
3502.282775	365718.877042	43.067252
3502.694248	365686.341682	43.072257
3502.519437	365670.133255	43.077261
3502.702536	365634.813083	43.082266
3502.649077	365609.591284	43.087271
3502.602200	365585.156089	43.092276
3502.345244	365550.996842	43.097281
3502.332475	365542.055263	43.102285
3502.327948	365515.758625	43.107290
3502.612787	365484.487745	43.112295
3501.976879	365467.055140	43.117300
3502.604758	365428.972235	43.122305
3502.222931	365410.864851	43.127309
3502.458719	365385.267539	43.132314
3502.677880	365355.429605	43.137319
3502.372717	365337.462696	43.142324
3502.408555	365301.936362	43.147329
3502.441923	365280.943961	43.152333
3502.231517	365254.831575	43.157338
3502.541419	365218.779732	43.162343
3502.150524	365203.112839	43.167348
3502.378206	365174.543816	43.172353
3502.271941	365155.529505	43.177357
3502.413420	365135.434881	43.182362
3502.540586	365098.623662	43.187367
3502.471459	365076.833991	43.192372
3502.127636	365051.606075	43.197377
3502.538855	365036.144585	43.202381
3502.487235	365003.756753	43.207386
3502.452810	364968.367989	43.212391
3502.519817	364955.958240	43.217396
3502.587601	364934.147157	43.222401
3502.346398	364914.696331	43.227405
3502.304704	364885.127187	43.232410
3502.055791	364856.682836	43.237415
3502.250340	364845.549038	43.242420
3502.238362	364821.946262	43.247425
3502.529217	364788.234460	43.252429
3502.226888	364764.600593	43.257434
3502.319146	364733.079381	43.262439
3502.210605	364723.847548	43.267444
3502.343552	364697.274692	43.272449
3502.251774	364671.956409	43.277453
3502.172880	364656.621804	43.282458
3502.535085	364627.573954	43.287463
3502.133538	364604.438167	43.292468
3502.429346	364573.901467	43.297473
3502.266411	364554.870175	43.302477
3502.129202	364530.600608	43.307482
3502.271298	364499.681206	43.312487
3502.117284	364493.327599	43.317492
3502.825910	364462.040499	43.322497
3502.734344	364435.426115	43.327501
3502.282149	364402.845862	43.332506
3502.289724	364378.502821	43.337511
3502.363827	364361.492658	43.342516
3502.024751	364333.747876	43.347521
3502.247403	364310.006540	43.352525
3502.313348	364276.176693	43.357530
3502.379829	364269.178903	43.362535
3502.269332	364244.676260	43.367540
3502.362862	364221.945908	43.372545
3502.401721	364201.307608	43.377549
3502.466708	364171.136729	43.382554
3502.335010	364137.591571	43.387559
3502.129723	364130.890133	43.392564
3502.463448	364096.891363	43.397569
3502.130897	364082.256575	43.402573
3502.568869	364048.165298	43.407578
3502.491267	364029.374480	43.412583
3502.318123	364004.601882	43.417588
3502.674864	363972.530507	43.422593
3502.360314	363946.306112	43.427597
3502.415239	363919.693875	43.432602
3502.354729	363892.006966	43.437607
3502.430194	363880.992973	43.442612
3502.383072	363839.608161	43.447617
3502.334812	363817.941355	43.452621
3502.475931	363797.693414	43.457626
3502.634580	363763.314948	43.462631
3502.239316	363739.821766	43.467636
3502.361834	363723.642222	43.472641
3502.577370	363697.563805	43.477645
3502.463422	363664.269443	43.482650
3502.030020	363646.423090	43.487655
3502.247148	363634.599257	43.492660
3502.426339	363607.967402	43.497665
3502.307767	363578.688415	43.502669
3502.155247	363557.139280	43.507674
3501.999845	363533.506969	43.512679
3502.190894	363514.546968	43.517684
3502.292884	363485.360615	43.522689
3502.214820	363471.854778	43.527693
3502.067903	363441.716127	43.532698
3502.214920	363421.009631	43.537703
3502.399293	363403.194047	43.542708
3502.088119	363374.580078	43.547713
3502.181619	363356.270406	43.552717
3501.993089	363331.753737	43.557722
3502.399507	363310.193675	43.562727
3502.061280	363293.831492	43.567732
3502.344180	363264.693000	43.572737
3502.336597	363240.148097	43.577741
3502.075474	363219.555792	43.582746
3502.342072	363192.503399	43.587751
3502.338060	363174.767812	43.592756
3502.250898	363148.939297	43.597761
3502.388054	363117.434780	43.602765
3502.317128	363100.116126	43.607770
3502.674528	363069.339592	43.612775
3501.959781	363049.148091	43.617780
3502.446508	363025.669553	43.622785
3502.218506	363004.233404	43.627789
3502.350689	362984.418272	43.632794
3502.686397	362963.021424	43.637799
3502.446021	362941.917490	43.642804
3502.530630	362911.742271	43.647809
3502.167105	362898.890444	43.652813
3502.317427	362863.724506	43.657818
3502.715186	362838.557164	43.662823
3502.334753	362810.690332	43.667828
3502.194539	362788.071481	43.672833
3502.126962	362771.031629	43.677837
3501.848961	362741.471696	43.682842
3502.328066	362720.154001	43.687847
3502.014968	362704.981879	43.692852
3502.456035	362680.392108	43.697857
3502.723674	362653.872685	43.702861
3502.046381	362626.788783	43.707866
3502.703419	362596.651221	43.712871
3502.255942	362579.924484	43.717876
3502.330831	362552.621822	43.722881
3502.391670	362526.388574	43.727885
3502.126639	362497.919042	43.732890
3502.139761	362472.074332	43.737895
3502.169348	362454.282266	43.742900
3502.302501	362433.399363	43.747905
3502.146324	362413.933654	43.752909
3502.162853	362392.611475	43.757914
3502.268314	362365.202241	43.762919
3502.024479	362352.763536	43.767924
3502.139274	362324.997060	43.772929
3502.133213	362310.488464	43.777933
3501.927084	362293.266611	43.782938
3502.226618	362270.096128	43.787943
3502.086782	362234.517202	43.792948
3502.455806	362221.474854	43.797953
3502.361489	362198.619714	43.802957
3501.991177	362179.288818	43.807962
3502.210321	362148.609081	43.812967
3502.187441	362135.475214	43.817972
3501.859540	362105.439603	43.822977
3502.071219	362096.665340	43.827981
3502.186684	362066.687752	43.832986
3502.076544	362041.471718	43.837991
3502.184567	362027.250165	43.842996
3502.293268	361995.977589	43.848001
3502.215277	361981.454614	43.853005
3502.500186	361957.015604	43.858010
3502.128784	361929.400652	43.863015
3501.820151	361903.554697	43.868020
3502.043169	361886.926522	43.873025
3501.966565	361861.781351	43.878029
3501.854855	361851.913830	43.883034
3502.064721	361833.686759	43.888039
3501.940500	361816.578942	43.893044
3501.907166	361797.322417	43.898049
3502.131691	361779.423379	43.903053
3502.158904	361758.531078	43.908058
3501.999871	361736.930814	43.913063
3502.179633	361723.104535	43.918068
3502.076272	361696.540349	43.923073
3502.173401	361672.714791	43.928077
3502.157457	361656.174497	43.933082
3502.324306	361634.167687	43.938087
3501.902658	361617.233096	43.943092
3502.014308	361591.397704	43.948097
3502.212538	361566.793983	43.953101
3502.128604	361551.077380	43.958106
3502.401587	361532.179603	43.963111
3501.805381	361510.342266	43.968116
3502.283134	361479.519954	43.973121
3501.839781	361469.373564	43.978125
3501.750804	361458.511322	43.983130
3502.156459	361435.857325	43.988135
3501.924893	361419.807863	43.993140
3502.010535	361393.671408	43.998145
3502.412170	361366.850463	44.003149
3502.102234	361353.201865	44.008154
3502.105734	361331.779310	44.013159
3501.846793	361313.802757	44.018164
3501.837734	361288.722830	44.023169
3501.986283	361266.693186	44.028173
3501.782534	361250.817188	44.033178
3502.034320	361232.456170	44.038183
3501.744394	361211.053778	44.043188
3501.996899	361195.614989	44.048193
3502.140864	361172.289983	44.053197
3502.371464	361153.576447	44.058202
3502.083686	361122.644188	44.063207
3502.186684	361108.880397	44.068212
3501.985727	361083.931808	44.073217
3502.181724	361067.281972	44.078221
3501.965848	361046.884419	44.083226
3501.996819	361017.605056	44.088231
3501.992740	361001.748679	44.093236
3501.953678	360983.483592	44.098241
3502.183448	360965.557842	44.103245
3501.709119	360951.096043	44.108250
3501.944277	360933.728501	44.113255
3501.940918	360918.176914	44.118260
3501.826843	360890.368488	44.123265
3501.531510	360875.421380	44.128269
3501.602342	360866.694088	44.133274
3501.756543	360843.824654	44.138279
3501.761759	360830.304661	44.143284
3502.277669	360814.723039	44.148289
3502.000453	360799.290243	44.153293
3502.045250	360781.596465	44.158298
3502.242002	360759.076116	44.163303
3501.884857	360741.317801	44.168308
3502.103999	360715.871526	44.173313
3502.317331	360687.224183	44.178317
3501.976857	360677.976358	44.183322
3502.280030	360659.734056	44.188327
3502.242910	360645.432785	44.193332
3502.198364	360608.490247	44.198337
3502.449837	360591.628217	44.203341
3502.454997	360568.629293	44.208346
3502.446239	360528.123350	44.213351
3502.355817	360509.688081	44.218356
3502.542957	360482.848905	44.223361
3502.041925	360467.730304	44.228365
3502.012789	360440.950158	44.233370
3502.115937	360420.782074	44.238375
3502.135391	360402.329642	44.243380
3502.190564	360384.811905	44.248385
3502.337580	360352.769281	44.253389
3502.046633	360346.486920	44.258394
3502.435820	360314.914823	44.263399
3502.156862	360291.629536	44.268404
3502.162870	360263.446069	44.273409
3502.423609	360248.107166	44.278413
3502.229958	360227.731013	44.283418
3502.070173	360201.530064	44.288423
3502.316642	360186.828669	44.293428
3501.910124	360160.564429	44.298433
3501.910597	360139.090672	44.303437
3501.921870	360115.201005	44.308442
3501.928895	360096.318303	44.313447
3502.027438	360089.721150	44.318452
3502.326163	360052.470387	44.323457
3502.602006	360039.187469	44.328461
3502.122561	360019.262254	44.333466
3502.471828	359988.178873	44.338471
3502.155772	359964.975347	44.343476
3501.899702	359932.537571	44.348481
3502.162190	359929.396445	44.353485
3501.809785	359902.157868	44.358490
3501.838344	359883.805355	44.363495
3501.739764	359867.734372	44.368500
3501.817927	359852.194963	44.373505
3501.779922	359829.202194	44.378509
3501.767036	359817.006042	44.383514
3502.061837	359793.707327	44.388519
3501.618318	359780.409172	44.393524
3501.867809	359764.893884	44.398529
3502.195267	359748.654889	44.403533
3501.865087	359730.154802	44.408538
3502.300590	359706.224211	44.413543
3501.802373	359697.686786	44.418548
3502.092877	359674.261583	44.423553
3501.824566	359654.099967	44.428557
3502.068565	359643.464801	44.433562
3502.455248	359616.898765	44.438567
3502.200961	359598.335962	44.443572
3502.180212	359568.732873	44.448577
3502.120901	359544.752087	44.453581
3501.669438	359527.287281	44.458586
3502.267724	359510.878948	44.463591
3501.518875	359490.893655	44.468596
3501.647572	359477.175949	44.473601
3501.711857	359452.769245	44.478605
3501.632653	359436.313819	44.483610
3502.075482	359427.375745	44.488615
3501.888377	359402.626920	44.493620
3502.136278	359381.571566	44.498625
3502.202688	359359.019635	44.503629
3501.828431	359348.455161	44.508634
3501.931476	359319.772862	44.513639
3501.863530	359308.703267	44.518644
3502.097597	359288.285338	44.523649
3501.900564	359268.569817	44.528653
3501.671469	359251.070248	44.533658
3502.190512	359228.346131	44.538663
3501.944346	359216.211453	44.543668
3501.814716	359188.124336	44.548673
3502.030485	359176.400617	44.553677
3502.053765	359159.014204	44.558682
3502.172488	359137.343444	44.563687
3501.982441	359114.119658	44.568692
3502.175708	359095.080285	44.573697
3502.126399	359076.383611	44.578701
3502.092769	359059.463444	44.583706
3501.895388	359042.187543	44.588711
3502.056570	359042.848729	44.593716
3501.972875	359011.831728	44.598721
3502.093751	358992.828969	44.603725
3502.158933	358970.988527	44.608730
3502.565635	358941.877414	44.613735
3502.189114	358918.402946	44.618740
3501.982316	358894.673324	44.623745
3502.114479	358873.152768	44.628749
3502.025099	358855.250024	44.633754
3501.915616	358824.363914	44.638759
3501.894922	358820.809292	44.643764
3501.874805	358789.070582	44.648769
3502.066989	358782.661886	44.653773
3502.132699	358761.507387	44.658778
3502.204563	358745.485531	44.663783
3502.139904	358718.251945	44.668788
3502.143248	358696.268445	44.673793
3502.244730	358670.711699	44.678797
3502.060377	358647.435844	44.683802
3502.244065	358628.372258	44.688807
3501.872424	358606.472460	44.693812
3502.288742	358582.543975	44.698817
3502.471951	358565.310237	44.703821
3502.156393	358549.831433	44.708826
3502.270013	358508.719234	44.713831
3501.968906	358495.728738	44.718836
3501.661725	358472.217723	44.723841
3502.097001	358452.225381	44.728845
3502.039837	358429.183710	44.733850
3502.157859	358411.527987	44.738855
3502.214623	358396.931494	44.743860
3501.929457	358378.220268	44.748865
3502.169334	358349.668253	44.753869
3501.869168	358334.796887	44.758874
3501.835052	358317.978042	44.763879
3502.124699	358298.008262	44.768884
3502.073702	358277.456119	44.773889
3501.837926	358251.519462	44.778893
3501.742263	358239.208490	44.783898
3501.617160	358219.506513	44.788903
3501.858880	358198.603795	44.793908
3502.150790	358185.444644	44.798913
3501.922443	358174.297940	44.803917
3501.812724	358153.475294	44.808922
3501.937476	358126.719996	44.813927
3501.994276	358117.282496	44.818932
3502.072351	358087.967569	44.823937
3502.222244	358073.712233	44.828941
3501.948492	358060.946026	44.833946
3502.175258	358036.817884	44.838951
3501.621953	358017.258655	44.843956
3501.643710	357997.686170	44.848961
3502.061629	357981.889625	44.853965
3502.181503	357970.993635	44.858970
3502.461367	357942.689166	44.863975
3502.240330	357931.744553	44.868980
3502.053008	357889.992163	44.873985
3502.005420	357877.444832	44.878989
3501.742969	357848.182667	44.883994
3501.512762	357839.882574	44.888999
3501.617787	357829.039674	44.894004
3501.892652	357809.859733	44.899009
3502.135631	357795.157733	44.904013
3502.124803	357772.743728	44.909018
3502.150241	357747.553855	44.914023
3501.723696	357732.574789	44.919028
3501.688063	357720.533830	44.924033
3502.211166	357705.381560	44.929037
3502.163086	357694.689512	44.934042
3502.050531	357673.434930	44.939047
3501.856359	357659.334603	44.944052
3501.740309	357636.352331	44.949057
3502.149861	357611.127988	44.954061
3502.058608	357601.332146	44.959066
3502.117095	357573.697160	44.964071
3501.855888	357558.514377	44.969076
3502.269021	357522.640555	44.974081
3501.815794	357508.707545	44.979085
3501.549889	357492.458033	44.984090
3501.515775	357470.403241	44.989095
3501.918355	357457.379048	44.994100
3501.734746	357439.591802	44.999105
3501.921189	357420.247474	45.004109
3501.790516	357413.431265	45.009114
3501.778319	357385.908770	45.014119
3501.885767	357380.682062	45.019124
3501.892532	357357.960037	45.024129
3502.101434	357333.808710	45.029133
3502.070432	357319.479515	45.034138
3502.009480	357297.911664	45.039143
3501.357164	357275.825858	45.044148
3501.624461	357253.469857	45.049153
3501.661892	357240.044922	45.054157
3501.126150	357249.887814	45.059162
3501.605104	357224.499866	45.064167
3501.347748	357212.950685	45.069172
3501.271265	357202.389963	45.074177
3501.593920	357185.286245	45.079181
3501.792528	357170.387531	45.084186
3502.063035	357154.689749	45.089191
3501.892777	357139.848421	45.094196
3501.656913	357125.423939	45.099201
3501.841463	357109.866587	45.104205
3501.508915	357096.982054	45.109210
3502.144771	357080.414092	45.114215
3501.737123	357064.262657	45.119220
3501.631836	357058.992753	45.124225
3501.929478	357043.087370	45.129229
3501.545101	357025.737773	45.134234
3501.766313	357010.098420	45.139239
3501.766890	356997.136591	45.144244
3501.667521	356967.822798	45.149249
3501.910721	356950.934639	45.154253
3501.410115	356946.310787	45.159258
3501.420186	356914.362125	45.164263
3501.301261	356904.977016	45.169268
3501.265785	356902.212351	45.174273
3501.452533	356893.592966	45.179277
3501.131873	356877.859960	45.184282
3501.567844	356861.704219	45.189287
3501.274877	356858.598387	45.194292
3501.404517	356857.815848	45.199297
3501.256825	356833.592545	45.204301
3501.244286	356826.808654	45.209306
3501.847350	356813.041360	45.214311
3501.544915	356814.918439	45.219316
3501.574365	356794.784854	45.224321
3501.855392	356777.229911	45.229325
3501.735601	356774.808757	45.234330
3501.653600	356746.508675	45.239335
3501.469673	356745.927421	45.244340
3501.783363	356737.161161	45.249345
3501.626508	356708.593121	45.254349
3501.618753	356701.833874	45.259354
3501.647638	356684.572271	45.264359
3501.598720	356664.222056	45.269364
3501.443531	356643.659625	45.274369
3501.803607	356649.373046	45.279373
3501.440704	356622.209436	45.284378
3501.942296	356609.093234	45.289383
3501.871108	356601.022220	45.294388
3501.848735	356572.051892	45.299393
3501.856317	356559.902094	45.304397
3501.597854	356544.464229	45.309402
3501.537611	356517.990486	45.314407
3501.638386	356517.390340	45.319412
3501.785902	356496.551965	45.324417
3501.998204	356481.294969	45.329421
3501.513888	356463.274383	45.334426
3501.689152	356441.872505	45.339431
3501.743134	356441.559213	45.344436
3501.603171	356430.652285	45.349441
3501.656718	356405.050293	45.354445
3501.392768	356392.739357	45.359450
3501.659491	356385.479843	45.364455
3501.917021	356378.298006	45.369460
3501.755032	356357.380621	45.374465
3501.556968	356341.475770	45.379469
3501.744949	356330.390694	45.384474
3502.049364	356312.272699	45.389479
3501.884490	356299.742981	45.394484
3502.107561	356283.874231	45.399489
3502.317681	356251.182112	45.404493
3502.147136	356235.171260	45.409498
3501.947164	356211.743504	45.414503
3501.884513	356194.445042	45.419508
3501.841589	356175.186464	45.424513
3501.920870	356160.026260	45.429517
3501.666874	356142.630464	45.434522
3502.186334	356116.447412	45.439527
3502.020847	356101.655677	45.444532
3501.677076	356082.443858	45.449537
3501.967262	356068.369099	45.454541
3501.941717	356043.999093	45.459546
3502.189298	356028.812636	45.464551
3502.107808	356002.977166	45.469556
3501.903827	355994.545416	45.474561
3502.447378	355969.883465	45.479565
3502.148302	355945.860942	45.484570
3502.027381	355920.412784	45.489575
3501.951825	355910.613966	45.494580
3501.795499	355894.066985	45.499585
3501.968644	355869.055934	45.504589
3501.908712	355857.653441	45.509594
3502.180295	355830.212492	45.514599
3501.832136	355807.569982	45.519604
3501.772916	355794.744040	45.524609
3502.424714	355775.936269	45.529613
3502.097695	355751.994195	45.534618
3501.927389	355729.400201	45.539623
3502.235298	355709.527582	45.544628
3501.602281	355695.062573	45.549633
3501.640393	355670.682370	45.554637
3501.230122	355660.655978	45.559642
3501.616993	355653.758846	45.564647
3501.537500	355632.650223	45.569652
3501.975326	355612.782742	45.574657
3502.133797	355604.040320	45.579661
3502.093495	355591.745098	45.584666
3501.832141	355577.730529	45.589671
3501.502957	355562.481098	45.594676
3501.451101	355544.519766	45.599681
3501.905049	355528.157208	45.604685
3501.527615	355514.364006	45.609690
3501.810252	355492.716022	45.614695
3501.897610	355485.814628	45.619700
3501.592516	355469.468489	45.624705
3501.528869	355447.188111	45.629709
3501.311602	355435.682864	45.634714
3501.728960	355407.049695	45.639719
3501.748178	355398.659302	45.644724
3501.678527	355390.130235	45.649729
3501.713504	355361.556528	45.654733
3501.919149	355363.100462	45.659738
3501.866566	355343.105791	45.664743
3501.789504	355329.342017	45.669748
3501.620116	355311.017589	45.674753
3501.572224	355299.079268	45.679757
3501.573071	355269.011199	45.684762
3501.576840	355267.104453	45.689767
3501.653333	355247.928390	45.694772
3501.650813	355242.032183	45.699777
3501.977729	355228.612169	45.704781
3501.835430	355208.428040	45.709786
3501.702169	355196.325046	45.714791
3501.775814	355174.124777	45.719796
3501.600571	355157.046597	45.724801
3501.838432	355142.115392	45.729805
3501.804515	355135.359877	45.734810
3501.771972	355114.523186	45.739815
3501.882696	355099.255908	45.744820
3501.790701	355072.633382	45.749825
3501.981476	354995.793713	45.754829
3501.379879	354898.438497	45.759834
3501.037835	354738.007977	45.764839
3501.089588	354546.836621	45.769844
3500.226594	354314.833393	45.774849
3499.628263	354026.105681	45.779853
3499.131104	353712.043248	45.784858
3498.150155	353341.039742	45.789863
3497.139773	352944.338264	45.794868
3496.116099	352503.608271	45.799873
3495.145982	352033.377447	45.804877
3493.921259	351529.167762	45.809882
3492.923188	350972.752752	45.814887
3491.631317	350391.004139	45.819892
3490.038623	349783.159074	45.824897
3488.829749	349130.500994	45.829901
3486.390151	348455.319555	45.834906
3484.930237	347737.210980	45.839911
3483.224224	346996.930759	45.844916
3481.320613	346231.647927	45.849921
3479.235170	345429.027589	45.854925
3477.216725	344621.496286	45.859930
3475.608509	343766.870086	45.864935
3472.924387	342902.855288	45.869940
3470.526933	342005.236266	45.874945
3468.820728	341078.219497	45.879949
3466.145093	340148.633857	45.884954
3463.552160	339169.678880	45.889959
3460.779439	338202.549993	45.894964
3458.570878	337206.469475	45.899969
3455.973772	336176.827844	45.904973
3453.399685	335153.537276	45.909978
3450.486384	334093.953792	45.914983
3447.808207	333024.486647	45.919988
3444.960938	331947.232925	45.924993
3442.217499	330835.011025	45.929997
3438.993153	329733.718414	45.935002
3436.318527	328593.035965	45.940007
3433.438068	327460.543387	45.945012
3430.146879	326304.145976	45.950017
3427.329131	325141.460401	45.955021
3424.058190	323972.707033	45.960026
3421.240483	322790.112772	45.965031
3418.062352	321595.482544	45.970036
3414.679976	320385.026149	45.975041
3411.590719	319169.783391	45.980045
3408.494813	317954.889481	45.985050
3405.094044	316735.429855	45.990055
3402.098791	315498.139501	45.995060
3398.462321	314250.126709	46.000065
3395.267858	312993.207249	46.005069
3391.664337	311742.348373	46.010074
3388.350767	310479.044298	46.015079
3385.161523	309216.451158	46.020084
3381.846075	307943.233223	46.025089
3378.290604	306659.611479	46.030093
3374.448774	305377.248646	46.035098
3371.250978	304099.207250	46.040103
3367.650466	302816.387011	46.045108
3364.145398	301528.430611	46.050113
3360.754830	300245.134181	46.055117
3357.349665	298935.415846	46.060122
3353.575852	297634.759938	46.065127
3349.712800	296336.760754	46.070132
3346.195317	295036.082345	46.075137
3342.708017	293733.563252	46.080141
3339.213979	292431.602433	46.085146
3335.396314	291130.631616	46.090151
3331.633171	289831.432614	46.095156
3328.162481	288526.815689	46.100161
3324.682487	287209.598142	46.105165
3321.109015	285914.848279	46.110170
3317.283931	284604.303285	46.115175
3313.795712	283301.395128	46.120180
3309.790463	281987.417833	46.125185
3306.447658	280682.326412	46.130189
3302.498732	279379.750584	46.135194
3298.885043	278067.119781	46.140199
3295.130150	276774.017455	46.145204
3291.419685	275471.492088	46.150209
3287.774580	274169.063217	46.155213
3283.860575	272875.058604	46.160218
3280.326123	271559.816251	46.165223
3276.942417	270271.572657	46.170228
3273.061719	268963.730691	46.175233
3269.476423	267663.565608	46.180237
3265.321775	266375.363450	46.185242
3261.636873	265076.198461	46.190247
3258.059084	263778.070078	46.195252
3254.293680	262483.494834	46.200257
3250.814372	261206.430973	46.205261
3246.727988	259925.449365	46.210266
3243.104381	258632.540472	46.215271
3239.617871	257346.854602	46.220276
3235.601243	256061.009259	46.225281
3231.739589	254789.312355	46.230285
3227.785693	253522.049523	46.235290
3224.247425	252247.376643	46.240295
3220.340350	250973.896648	46.245300
3216.627475	249713.568486	46.250305
3213.209800	248456.775993	46.255309
3209.333457	247180.690702	46.260314
3205.626045	245916.031105	46.265319
3202.271769	244646.953650	46.270324
3198.063943	243405.812752	46.275329
3194.430652	242133.580959	46.280333
3190.521686	240894.901947	46.285338
3187.107934	239633.982625	46.290343
3183.124819	238390.745297	46.295348
3179.334226	237141.309821	46.300353
3175.944434	235893.004663	46.305357
3171.596783	234662.138035	46.310362
3167.866012	233422.410819	46.315367
3164.015958	232192.504831	46.320372
3160.700091	230965.849777	46.325377
3156.791570	229747.027619	46.330381
3152.887647	228522.676517	46.335386
3149.431061	227297.669006	46.340391
3145.477230	226079.487618	46.345396
3141.723198	224863.974747	46.350401
3138.034808	223642.670514	46.355405
3134.120650	222442.286801	46.360410
3130.784146	221238.987310	46.365415
3126.745858	220027.877784	46.370420
3122.842639	218833.125817	46.375425
3119.194903	217631.434455	46.380429
3115.351644	216434.589997	46.385434
3111.562584	215233.945539	46.390439
3107.615181	214049.960462	46.395444
3104.075803	212861.942817	46.400449
3100.308505	211681.809381	46.405453
3096.563357	210508.884842	46.410458
3092.849223	209327.174075	46.415463
3089.383887	208161.373245	46.420468
3085.572015	206997.975250	46.425473
3081.837814	205827.313055	46.430477
3077.987523	204671.497806	46.435482
3074.180685	203507.252942	46.440487
3070.422553	202349.298322	46.445492
3066.438793	201196.479937	46.450497
3062.987316	200044.961933	46.455501
3059.065555	198901.598442	46.460506
3055.399322	197764.086576	46.465511
3051.814555	196619.516702	46.470516
3047.844211	195492.944392	46.475521
3044.462247	194351.927103	46.480525
3041.031984	193224.144077	46.485530
3036.916464	192090.085969	46.490535
3033.096923	190972.264731	46.495540
3029.118584	189853.867688	46.500545
3025.242987	188735.440189	46.505549
3021.575494	187624.554615	46.510554
3017.620439	186514.056350	46.515559
3014.326815	185419.382005	46.520564
3010.273989	184318.649958	46.525569
3006.503816	183215.492660	46.530573
3002.676592	182137.030699	46.535578
2998.936082	181050.546875	46.540583
2995.077136	179962.821280	46.545588
2991.231736	178890.791577	46.550593
2987.358092	177814.552786	46.555597
2983.070600	176752.255831	46.560602
2979.359501	175699.990847	46.565607
2975.627243	174653.687861	46.570612
2971.667187	173604.900700	46.575617
2968.138244	172566.193683	46.580621
2964.278778	171535.686600	46.585626
2960.360948	170499.487037	46.590631
2956.673328	169473.424404	46.595636
2952.493040	168460.818845	46.600641
2948.942762	167448.193289	46.605645
2944.808513	166448.211375	46.610650
2940.747568	165445.266762	46.615655
2937.136678	164453.506402	46.620660
2933.258757	163461.305961	46.625665
2929.173663	162486.335987	46.630669
2925.409421	161518.369466	46.635674
2921.568180	160556.780905	46.640679
2917.802636	159596.964493	46.645684
2913.748554	158649.362699	46.650689
2909.728818	157695.839403	46.655693
2906.090684	156753.789931	46.660698
2901.924117	155817.870258	46.665703
2898.252341	154903.447652	46.670708
2894.185004	153998.035136	46.675713
2890.388827	153081.548414	46.680717
2886.364318	152184.710381	46.685722
2881.891817	151292.308829	46.690727
2878.112177	150415.415691	46.695732
2873.575011	149551.940049	46.700737
2869.726177	148679.081775	46.705741
2865.503510	147841.429992	46.710746
2861.365081	147008.435813	46.715751
2857.084899	146189.741448	46.720756
2852.943380	145390.252530	46.725761
2848.777338	144598.287350	46.730765
2844.474096	143812.399942	46.735770
2840.345163	143053.485155	46.740775
2835.963329	142286.147446	46.745780
2831.870634	141552.455848	46.750785
2827.843082	140818.994257	46.755789
2823.261367	140103.595131	46.760794
2818.833341	139403.386725	46.765799
2815.171766	138709.201791	46.770804
2810.658876	138037.487684	46.775809
2807.050937	137365.807860	46.780813
2802.353908	136649.219963	46.785818
2798.513242	136008.065797	46.790823
2794.922419	135373.866076	46.795828
2790.858438	134748.755820	46.800833
2786.504872	134142.667040	46.805837
2783.094245	133542.062591	46.810842
2778.827048	132945.148797	46.815847
2775.042554	132362.008385	46.820852
2771.308236	131787.250949	46.825857
2767.775759	131216.349511	46.830861
2763.770513	130643.455782	46.835866
2760.464946	130088.065681	46.840871
2756.889857	129520.284517	46.845876
2753.265469	128966.116246	46.850881
2749.635920	128413.724127	46.855885
2746.165008	127872.507861	46.860890
2742.922337	127322.232326	46.865895
2739.113441	126778.055718	46.870900
2735.513392	126230.610443	46.875905
2731.811753	125681.522130	46.880909
2728.467096	125145.524143	46.885914
2724.654329	124602.725354	46.890919
2721.029950	124064.546792	46.895924
2717.215025	123545.469763	46.900929
2714.485701	123004.647990	46.905933
2710.873595	122475.315345	46.910938
2707.249844	121939.887114	46.915943
2703.916214	121413.107140	46.920948
2700.337341	120888.051142	46.925953
2696.799615	120350.304071	46.930957
2693.291171	119825.327836	46.935962
2689.689482	119289.869163	46.940967
2686.082261	118758.666226	46.945972
2681.800856	118237.965012	46.950977
2678.546643	117716.488015	46.955981
2675.273728	117193.457064	46.960986
2671.688123	116674.271435	46.965991
2668.671484	116158.119864	46.970996
2664.589123	115639.483754	46.976001
2661.256012	115116.656673	46.981005
2657.313401	114606.202108	46.986010
2653.860086	114079.225203	46.991015
2650.154573	113568.010788	46.996020
2646.343341	113060.901463	47.001025
2642.840874	112541.481681	47.006029
2639.601078	112041.138219	47.011034
2635.971667	111537.137134	47.016039
2632.311198	111036.364663	47.021044
2628.312484	110532.549734	47.026049
2624.914121	110028.674001	47.031053
2620.942064	109541.295143	47.036058
2617.277470	109051.955524	47.041063
2613.459450	108567.553918	47.046068
2609.678542	108093.272800	47.051073
2606.187870	107612.380532	47.056077
2602.288872	107146.737358	47.061082
2598.625725	106682.996098	47.066087
2594.533211	106208.064914	47.071092
2591.047742	105755.508118	47.076097
2587.597135	105297.142608	47.081101
2583.774449	104847.993674	47.086106
2579.676608	104397.800372	47.091111
2576.298861	103960.314144	47.096116
2571.932688	103522.517160	47.101121
2568.513823	103091.607740	47.106125
2564.905102	102667.393983	47.111130
2561.320964	102244.478349	47.116135
2557.611699	101819.439542	47.121140
2553.672234	101401.992054	47.126145
2550.697745	100974.117145	47.131149
2546.979308	100564.793247	47.136154
2543.138218	100151.464560	47.141159
2539.996113	99726.402955	47.146164
2536.301475	99316.747997	47.151169
2533.121707	98908.238244	47.156173
2529.425630	98500.424099	47.161178
2525.842151	98086.624367	47.166183
2522.533289	97671.605353	47.171188
2518.817173	97265.233571	47.176193
2515.892410	96857.422168	47.181197
2512.236883	96438.139671	47.186202
2508.479763	96030.023738	47.191207
2505.204869	95620.973933	47.196212
2501.579248	95206.913606	47.201217
2498.372179	94789.972533	47.206221
2495.410785	94381.017329	47.211226
2491.795277	93965.752080	47.216231
2488.393228	93540.077385	47.221236
2484.717616	93119.076542	47.226241
2481.492197	92698.634070	47.231245
2477.941387	92279.404344	47.236250
2474.456972	91852.419069	47.241255
2471.046798	91426.266876	47.246260
2467.405317	90999.686564	47.251265
2463.918132	90579.060109	47.256269
2460.751656	90162.430096	47.261274
2457.569047	89727.436011	47.266279
2454.062856	89300.083791	47.271284
2450.020158	88869.149379	47.276289
2446.889404	88434.877629	47.281293
2443.241268	88010.818596	47.286298
2439.680821	87582.368890	47.291303
2436.214942	87145.728992	47.296308
2432.498774	86715.054789	47.301313
2429.585697	86282.203888	47.306317
2425.677389	85852.347298	47.311322
2422.070324	85411.563052	47.316327
2419.017589	84983.034456	47.321332
2414.991542	84556.696249	47.326337
2411.771991	84125.157573	47.331341
2407.990948	83695.122818	47.336346
2404.689817	83262.669830	47.341351
2401.240968	82821.862657	47.346356
2397.976771	82393.812257	47.351361
2394.657037	81945.161221	47.356365
2391.376529	81513.112797	47.361370
2387.697132	81081.310916	47.366375
2383.980273	80641.341650	47.371380
2380.399731	80194.613624	47.376385
2377.015998	79748.001848	47.381389
2373.564490	79314.388276	47.386394
2369.944182	78863.928335	47.391399
2366.825628	78429.590981	47.396404
2363.047407	77983.564430	47.401409
2359.736188	77541.219024	47.406413
2356.411699	77097.358834	47.411418
2352.668221	76653.342477	47.416423
2349.356521	76205.824582	47.421428
2345.752822	75765.115602	47.426433
2342.008190	75313.425539	47.431437
2338.397462	74864.084222	47.436442
2335.007515	74422.309930	47.441447
2332.224788	73981.857967	47.446452
2328.225673	73533.056576	47.451457
2324.762836	73076.217564	47.456461
2321.093290	72635.532245	47.461466
2317.707850	72177.134842	47.466471
2314.720943	71733.882271	47.471476
2311.154003	71282.512300	47.476481
2307.595933	70813.969608	47.481485
2303.564460	70368.960020	47.486490
2300.735743	69918.736642	47.491495
2297.384108	69471.027449	47.496500
2293.790695	69006.534847	47.501505
2290.257838	68536.321651	47.506509
2286.735934	68091.563876	47.511514
2283.011074	67630.404729	47.516519
2279.691462	67168.245021	47.521524
2275.936532	66706.415323	47.526529
2272.704997	66250.320418	47.531533
2269.153251	65790.087984	47.536538
2265.125636	65331.201062	47.541543
2262.086339	64861.416768	47.546548
2258.570729	64407.728684	47.551553
2255.082914	63951.435934	47.556557
2251.482200	63486.702570	47.561562
2247.748007	63028.281756	47.566567
2244.346154	62565.946322	47.571572
2240.570593	62109.103794	47.576577
2237.373234	61643.498073	47.581581
2234.253692	61186.538780	47.586586
2230.560391	60728.020963	47.591591
2227.158636	60262.219355	47.596596
2223.205254	59803.499143	47.601601
2220.156404	59336.441884	47.606605
2216.255327	58876.925092	47.611610
2212.559567	58412.340468	47.616615
2209.335267	57953.072189	47.621620
2205.636730	57488.683435	47.626625
2202.447163	57028.621545	47.631629
2198.453456	56571.034898	47.636634
2195.322654	56108.024820	47.641639
2191.901387	55651.787931	47.646644
2188.532067	55190.089060	47.651649
2184.814287	54718.238895	47.656653
2181.484018	54258.379299	47.661658
2178.260087	53789.928461	47.666663
2174.679050	53326.046794	47.671668
2171.087426	52863.990309	47.676673
2168.034284	52388.188283	47.681677
2164.188922	51921.603370	47.686682
2160.550614	51453.726886	47.691687
2157.248847	50984.932072	47.696692
2153.661774	50507.951244	47.701697
2150.507362	50036.526622	47.706701
2146.969855	49570.651641	47.711706
2143.166837	49089.090744	47.716711
2140.115681	48613.708634	47.721716
2136.378934	48149.688584	47.726721
2132.582512	47672.685179	47.731725
2129.314589	47194.785042	47.736730
2125.402679	46727.383774	47.741735
2122.675977	46260.866860	47.746740
2118.810569	45774.337687	47.751745
2115.350793	45298.803376	47.756749
2111.758054	44821.790534	47.761754
2108.230112	44353.414988	47.766759
2104.926094	43872.813552	47.771764
2100.947392	43400.634590	47.776769
2097.654348	42919.988670	47.781773
2094.087850	42453.079656	47.786778
2090.798058	41976.131568	47.791783
2087.364983	41493.693347	47.796788
2083.395978	41022.781241	47.801793
2080.124727	40532.939527	47.806797
2076.696233	40067.708349	47.811802
2073.184975	39590.675562	47.816807
2070.033781	39115.144194	47.821812
2066.353363	38635.204308	47.826817
2063.059768	38158.200920	47.831821
2059.346806	37673.513672	47.836826
2055.722835	37194.059924	47.841831
2052.568812	36714.835380	47.846836
2048.784894	36238.325025	47.851841
2045.465239	35752.187449	47.856845
2041.625423	35283.472516	47.861850
2038.272842	34800.265088	47.866855
2035.104719	34315.658176	47.871860
2031.250455	33829.964874	47.876865
2027.462986	33342.389911	47.881869
2023.735707	32868.729222	47.886874
2020.385619	32392.871956	47.891879
2017.299590	31915.178142	47.896884
2014.094673	31442.146682	47.901889
2010.563273	30958.028961	47.906893
2006.818923	30469.868038	47.911898
2002.723230	29993.148792	47.916903
1999.458083	29515.183300	47.921908
1995.804755	29041.851981	47.926913
1992.144293	28566.061319	47.931917
1988.333082	28089.069525	47.936922
1985.121190	27613.262921	47.941927
1981.780440	27134.851538	47.946932
1977.903994	26669.790283	47.951937
1974.565556	26196.102200	47.956941
1971.139792	25725.448398	47.961946
1967.274715	25249.773611	47.966951
1963.959393	24777.825925	47.971956
1960.316754	24321.291284	47.976961
1956.873296	23850.652482	47.981965
1953.461431	23384.004720	47.986970
1949.821151	22915.382544	47.991975
1946.442661	22433.718704	47.996980
1942.400418	21975.602252	48.001985
1938.946927	21507.104651	48.006989
1935.556784	21058.663326	48.011994
1931.396556	20586.135844	48.016999
1928.288383	20132.388912	48.022004
1924.751401	19679.599654	48.027009
1921.068819	19224.487328	48.032013
1917.534548	18763.092117	48.037018
1913.653013	18316.519198	48.042023
1909.988937	17868.516677	48.047028
1906.192090	17423.268506	48.052033
1902.424726	16983.643527	48.057037
1898.889255	16548.279939	48.062042
1894.623155	16126.544802	48.067047
1890.945413	15697.109055	48.072052
1886.576946	15288.909701	48.077057
1882.697214	14887.149625	48.082061
1878.626434	14484.547543	48.087066
1874.686195	14098.628554	48.092071
1871.297485	13714.531189	48.097076
1867.222554	13348.825631	48.102081
1863.473751	12970.928725	48.107085
1859.788196	12612.385608	48.112090
1855.440565	12242.204053	48.117095
1851.974941	11881.199777	48.122100
1848.335490	11536.814490	48.127105
1844.386393	11202.297154	48.132109
1841.060658	10860.645378	48.137114
1837.120459	10526.787666	48.142119
1833.414857	10207.634613	48.147124
1829.412472	9896.013066	48.152129
1825.508162	9579.041522	48.157133
1821.420542	9272.660185	48.162138
1817.060369	8983.339540	48.167143
1813.167616	8687.411361	48.172148
1809.416185	8419.344579	48.177153
1805.743972	8140.811840	48.182157
1801.934111	7882.703544	48.187162
1798.479227	7612.820392	48.192167
1794.655993	7351.486976	48.197172
1790.986353	7106.404264	48.202177
1787.161879	6864.270114	48.207181
1783.382629	6620.435766	48.212186
1779.797569	6388.996299	48.217191
1776.608772	6158.627908	48.222196
1772.488989	5932.901228	48.227201
1769.395497	5701.447762	48.232205
1765.733326	5470.902220	48.237210
1762.190247	5254.246348	48.242215
1759.000251	5027.288059	48.247220
1755.070626	4808.738789	48.252225
1751.836700	4594.685048	48.257229
1748.225949	4378.629256	48.262234
1744.646732	4153.650636	48.267239
1741.331114	3938.269322	48.272244
1737.437780	3728.647827	48.277249
1734.483245	3511.620569	48.282253
1730.625916	3310.197049	48.287258
1727.218880	3110.487162	48.292263
1723.832018	2891.718381	48.297268
1719.931353	2690.542691	48.302273
1716.628515	2473.771995	48.307277
1712.873298	2273.179527	48.312282
1709.565349	2067.302167	48.317287
1706.284992	1865.972733	48.322292
1702.616254	1672.103400	48.327297
1699.012237	1475.505101	48.332301
1695.525953	1268.212438	48.337306
1691.432726	1075.731834	48.342311
1688.028868	881.833021	48.347316
1683.812919	698.819665	48.352321
1680.585087	508.206869	48.357325
1676.462314	338.723688	48.362330
1672.343125	173.044357	48.367335
1668.481134	24.853382	48.372340
1656.753221	69.837960	48.377345
1649.116327	85.238022	48.382349
1644.660471	80.926667	48.387354
1641.280610	78.605486	48.392359
1638.746304	70.891471	48.397364
1636.079047	74.340696	48.402369
1634.219680	74.231566	48.407373
1631.195020	75.714815	48.412378
1627.548118	76.738101	48.417383
1625.313150	65.772674	48.422388
1621.227459	77.016561	48.427393
1618.045731	73.892603	48.432397
1614.536120	82.781623	48.437402
1610.974668	74.993364	48.442407
1608.233847	71.699545	48.447412
1604.081804	72.965968	48.452417
1600.562391	78.616886	48.457421
1597.528483	72.382154	48.462426
1594.376355	81.604668	48.467431
1590.457178	73.650632	48.472436
1587.097348	69.317394	48.477441
1584.269166	66.518058	48.482445
1581.184357	66.716720	48.487450
1577.303960	83.601166	48.492455
1573.968409	75.606914	48.497460
1569.920940	79.362711	48.502465
1566.695653	85.075419	48.507469
1563.074672	74.534525	48.512474
1559.342406	74.723233	48.517479
1556.781384	72.818771	48.522484
1553.013387	76.056517	48.527489
1549.556980	85.225154	48.532493
1546.219166	71.005104	48.537498
1542.486439	80.498316	48.542503
1539.220324	71.170838	48.547508
1535.688519	78.791506	48.552513
1532.648827	74.819726	48.557517
1528.925183	72.251516	48.562522
1525.060642	77.956155	48.567527
1522.105714	68.792214	48.572532
1517.991502	73.842863	48.577537
1514.634991	68.265786	48.582541
1511.463086	64.770161	48.587546
1507.633541	74.079127	48.592551
1504.657484	67.971445	48.597556
1501.232317	68.507821	48.602561
1497.646011	70.344248	48.607565
1493.920193	71.670889	48.612570
1490.507541	74.726783	48.617575
1487.105664	70.586760	48.622580
1483.803929	72.125799	48.627585
1480.212648	79.344447	48.632589
1477.300821	69.424009	48.637594
1473.278829	70.056446	48.642599
1470.179835	67.875064	48.647604
1466.428466	73.837332	48.652609
1462.413926	69.919219	48.657613
1459.459851	63.880887	48.662618
1455.498847	73.982257	48.667623
1452.172535	68.308741	48.672628
1448.854961	71.156854	48.677633
1445.503426	69.546282	48.682637
1441.490312	69.639513	48.687642
1438.317326	73.164298	48.692647
1434.898114	67.033854	48.697652
1431.536966	78.206099	48.702657
1427.911630	67.789298	48.707661
1424.630885	72.403347	48.712666
1421.179814	66.600561	48.717671
1417.839586	63.131147	48.722676
1414.109137	66.707900	48.727681
1410.315663	64.894043	48.732685
1406.877042	70.915200	48.737690
1402.887018	65.170994	48.742695
1399.825338	72.028806	48.747700
1396.317656	63.387513	48.752705
1393.156513	67.062314	48.757709
1389.437860	64.341489	48.762714
1385.725045	75.097079	48.767719
1382.481002	65.032220	48.772724
1379.225264	78.893013	48.777729
1375.458520	80.127961	48.782733
1372.590595	77.268394	48.787738
1368.776877	74.359890	48.792743
1365.439978	74.145401	48.797748
1361.541981	75.309033	48.802753
1357.984239	74.521489	48.807757
1354.592108	65.662905	48.812762
1350.788440	61.009650	48.817767
1347.623399	63.112706	48.822772
1344.192856	67.598219	48.827777
1340.237075	73.019682	48.832781
1337.415484	70.772991	48.837786
1333.730121	80.268326	48.842791
1330.057854	75.347849	48.847796
1326.542006	75.961631	48.852801
1323.142881	76.104837	48.857805
1319.639080	72.268596	48.862810
1315.561363	78.031739	48.867815
1313.027443	71.589512	48.872820
1309.537234	72.825715	48.877825
1305.467071	63.886019	48.882829
1302.535047	66.161613	48.887834
1298.497835	73.522441	48.892839
1294.914975	72.577466	48.897844
1291.679290	68.101560	48.902849
1288.210183	73.137234	48.907853
1285.041561	63.658591	48.912858
1281.124273	71.136791	48.917863
1277.610249	66.780140	48.922868
1274.224578	80.025255	48.927873
1270.422361	79.794619	48.932877
1267.207609	76.913119	48.937882
1263.992404	70.298539	48.942887
1260.263380	68.908093	48.947892
1256.178729	73.251822	48.952897
1253.024029	74.002382	48.957901
1250.006412	71.817849	48.962906
1246.064322	82.409820	48.967911
1243.040060	71.307884	48.972916
1239.499823	72.855595	48.977921
1235.855302	72.325177	48.982925
1232.346294	73.301727	48.987930
1228.312076	69.279148	48.992935
1225.530131	74.470452	48.997940
1221.469204	73.280367	49.002945
1218.016346	73.219980	49.007949
1214.839962	72.414222	49.012954
1211.033991	63.822556	49.017959
1207.719237	69.330907	49.022964
1204.174894	73.862616	49.027969
1200.597101	72.157579	49.032973
1197.509770	66.171662	49.037978
1193.625061	71.347960	49.042983
1190.358552	72.723357	49.047988
1186.503896	67.625655	49.052993
1183.077483	76.628279	49.057997
1179.954117	67.838620	49.063002
1176.203431	64.613457	49.068007
1172.945823	65.126948	49.073012
1169.263317	68.424181	49.078017
1165.285967	67.369788	49.083021
1162.111477	66.158789	49.088026
1158.813445	74.726987	49.093031
1155.454257	69.998247	49.098036
1151.681502	68.738006	49.103041
1148.047317	73.109701	49.108045
1144.803663	64.718415	49.113050
1141.267848	65.173976	49.118055
1137.700245	68.155940	49.123060
1133.951344	64.225004	49.128065
1130.646594	66.473208	49.133069
1127.269227	59.839603	49.138074
1123.842548	60.616692	49.143079
1120.282986	61.487230	49.148084
1116.447221	65.659354	49.153089
1113.117618	70.803034	49.158093
1109.950117	56.828659	49.163098
1106.140565	66.688167	49.168103
1102.797474	57.799854	49.173108
1099.279547	57.553461	49.178113
1095.684624	65.405423	49.183117
1092.364797	64.175927	49.188122
1088.085401	67.689462	49.193127
1084.922276	61.690052	49.198132
1081.800052	58.835303	49.203137
1078.180598	70.291356	49.208141
1074.821669	62.139485	49.213146
1071.435738	66.330176	49.218151
1067.935685	67.178802	49.223156
1063.937748	71.252791	49.228161
1060.366665	67.142330	49.233165
1056.990561	61.207714	49.238170
1053.540685	66.420737	49.243175
1050.092698	60.652331	49.248180
1046.869898	61.948173	49.253185
1043.324702	63.942753	49.258189
1040.010890	65.335017	49.263194
1036.269149	61.928153	49.268199
1032.813956	57.818642	49.273204
1029.170727	63.906466	49.278209
1025.391691	74.783099	49.283213
1022.222190	57.680173	49.288218
1018.447242	61.074064	49.293223
1015.182263	54.315421	49.298228
1011.819595	63.504270	49.303233
1007.822905	68.182333	49.308237
1004.544701	58.945423	49.313242
1001.010496	68.439380	49.318247
997.748382	66.422646	49.323252
994.389391	71.425379	49.328257
990.679005	64.271007	49.333261
987.221532	67.587011	49.338266
983.578070	67.619594	49.343271
980.025706	66.818604	49.348276
976.794137	62.509778	49.353281
973.047781	66.392758	49.358285
969.578396	67.885174	49.363290
965.706308	73.844119	49.368295
962.390585	67.852661	49.373300
958.843447	66.823075	49.378305
955.716460	80.869459	49.383309
952.346968	63.092176	49.388314
949.100606	69.035974	49.393319
945.729178	70.418234	49.398324
941.835869	74.121618	49.403329
937.770548	74.678607	49.408333
934.719477	68.816796	49.413338
930.721555	69.572097	49.418343
927.487269	64.978970	49.423348
924.020032	71.504469	49.428353
920.488582	70.586338	49.433357
916.969361	66.423534	49.438362
913.658042	65.724233	49.443367
910.408096	65.894880	49.448372
906.756963	74.603471	49.453377
902.802589	67.271964	49.458381
899.434175	56.014874	49.463386
895.724345	71.075771	49.468391
892.763520	66.731138	49.473396
889.382928	72.426923	49.478401
885.238271	68.140025	49.483405
881.969251	65.219569	49.488410
878.544141	72.545250	49.493415
874.996351	63.325018	49.498420
871.591930	66.082294	49.503425
868.188890	76.090503	49.508429
864.923251	66.535292	49.513434
861.099649	67.348886	49.518439
857.152032	59.934084	49.523444
853.883321	71.085613	49.528449
850.576293	70.787437	49.533453
847.232399	56.141408	49.538458
843.644287	66.523262	49.543463
839.933849	71.969847	49.548468
836.311236	68.595087	49.553473
832.913724	69.184174	49.558477
829.659788	60.829348	49.563482
825.862140	64.214137	49.568487
822.461467	66.964506	49.573492
819.162177	66.431018	49.578497
815.217793	58.519025	49.583501
812.302745	51.044737	49.588506
808.778507	59.240040	49.593511
805.336093	66.919584	49.598516
801.494767	72.358074	49.603521
797.796348	74.480933	49.608525
794.447357	57.833102	49.613530
790.731165	69.532004	49.618535
787.667010	66.399340	49.623540
783.785738	57.158278	49.628545
780.233193	61.267362	49.633549
777.067331	51.801046	49.638554
773.651670	65.775297	49.643559
770.134832	60.327696	49.648564
766.581001	58.685425	49.653569
762.939491	62.460356	49.658573
759.395257	62.306682	49.663578
755.704515	69.566155	49.668583
752.334260	55.379822	49.673588
749.051641	62.537797	49.678593
745.361064	57.598125	49.683597
742.039342	56.125364	49.688602
738.523977	60.681069	49.693607
734.816403	64.548543	49.698612
731.168059	61.661848	49.703617
727.855539	60.320531	49.708621
724.645263	54.515178	49.713626
720.876977	58.230755	49.718631
717.532334	68.815154	49.723636
714.059420	60.488110	49.728641
710.423642	57.526699	49.733645
707.299593	58.237741	49.738650
703.301136	59.331668	49.743655
700.402591	60.194263	49.748660
696.417978	68.486552	49.753665
692.510362	59.850706	49.758669
689.719800	61.278607	49.763674
685.888997	54.456247	49.768679
682.183190	59.127021	49.773684
678.778002	65.744112	49.778689
675.012768	70.262793	49.783693
671.659971	59.164667	49.788698
668.130779	61.428870	49.793703
664.890796	70.348706	49.798708
661.493880	64.455358	49.803713
657.492017	63.904714	49.808717
654.330735	58.885825	49.813722
650.682912	69.324439	49.818727
647.650525	62.441064	49.823732
643.794663	61.389980	49.828737
640.322150	57.653375	49.833741
636.830451	57.175171	49.838746
633.141854	64.937340	49.843751
630.098933	58.606089	49.848756
626.685507	60.507435	49.853761
622.730441	59.519253	49.858765
619.427424	55.060258	49.863770
616.067915	60.787577	49.868775
612.133752	58.809078	49.873780
608.816138	60.053286	49.878785
605.175527	56.678204	49.883789
602.041555	52.645301	49.888794
598.054415	62.662186	49.893799
594.672155	70.367180	49.898804
591.217044	56.333297	49.903809
588.022560	68.726087	49.908813
584.691485	68.276667	49.913818
580.753272	75.656935	49.918823
577.182100	70.198841	49.923828
573.739401	62.028468	49.928833
570.145163	64.081352	49.933837
566.884110	64.022820	49.938842
563.582790	63.204949	49.943847
560.121119	68.328100	49.948852
556.459340	65.924401	49.953857
552.630887	67.112103	49.958861
549.457289	61.753472	49.963866
545.516054	63.059970	49.968871
542.406607	60.633563	49.973876
538.947888	60.169220	49.978881
535.313527	67.290220	49.983885
531.785956	57.032396	49.988890
528.221312	69.292992	49.993895
524.405382	60.712510	49.998900
520.730101	68.181558	50.003905
517.758849	72.314067	50.008909
514.451862	57.428262	50.013914
510.731429	70.757121	50.018919
507.043132	66.763071	50.023924
503.658155	66.720675	50.028929
500.057267	67.464845	50.033933
496.973432	65.072420	50.038938
493.151934	58.754834	50.043943
489.690906	61.429213	50.048948
486.394897	64.400597	50.053953
482.796753	62.439408	50.058957
479.370395	55.395942	50.063962
475.537880	61.282327	50.068967
472.243352	60.694359	50.073972
468.565950	55.471120	50.078977
464.913107	68.463599	50.083981
461.630372	72.125763	50.088986
458.088574	68.510699	50.093991
454.766367	59.255438	50.098996
451.303590	66.786318	50.104001
447.589441	66.940703	50.109005
444.173824	57.469041	50.114010
440.777604	71.358016	50.119015
437.073400	62.111608	50.124020
433.089956	68.008841	50.129025
429.710451	63.232762	50.134029
426.939032	54.451732	50.139034
423.485842	56.030270	50.144039
419.421908	48.757056	50.149044
416.447049	52.023287	50.154049
412.420183	64.052130	50.159053
409.206792	59.133139	50.164058
405.640056	60.299099	50.169063
402.080542	57.667541	50.174068
398.756926	56.789890	50.179073
395.109791	61.404105	50.184077
391.693260	53.027225	50.189082
387.874193	57.563805	50.194087
384.821033	60.029169	50.199092
381.239501	59.707351	50.204097
377.648650	66.353367	50.209101
374.274114	59.785892	50.214106
370.691460	58.878973	50.219111
366.923026	58.671673	50.224116
363.462173	61.826915	50.229121
359.907025	62.734820	50.234125
356.532653	57.315733	50.239130
353.174170	68.509721	50.244135
349.790191	63.443295	50.249140
346.443826	64.151024	50.254145
342.669733	57.107938	50.259149
338.762971	55.527004	50.264154
334.886131	67.203476	50.269159
332.010430	56.660719	50.274164
329.032357	58.301338	50.279169
324.878715	56.122946	50.284173
321.632443	54.432860	50.289178
318.005916	63.197759	50.294183
314.654470	62.723074	50.299188
311.264557	56.281389	50.304193
307.402389	54.294896	50.309197
304.065040	61.812585	50.314202
300.361480	61.639486	50.319207
296.777955	59.410304	50.324212
293.485351	52.874382	50.329217
289.814489	65.138865	50.334221
286.653743	57.006913	50.339226
283.067928	50.855154	50.344231
278.992415	55.029886	50.349236
275.693763	56.907077	50.354241
272.500931	69.226849	50.359245
269.151918	56.451486	50.364250
265.739998	60.231852	50.369255
262.197170	59.812279	50.374260
258.450035	53.388257	50.379265
254.752737	64.094009	50.384269
251.528736	57.310139	50.389274
247.690836	65.997224	50.394279
244.257175	55.047823	50.399284
241.316154	58.830806	50.404289
237.346281	63.406701	50.409293
234.131709	60.003316	50.414298
230.217306	63.286131	50.419303
227.083629	63.644396	50.424308
223.622607	60.336328	50.429313
220.104709	64.987387	50.434317
216.735061	52.417726	50.439322
212.841263	56.361702	50.444327
209.728307	59.364724	50.449332
205.985772	54.566115	50.454337
202.162145	69.530841	50.459341
198.791484	53.183934	50.464346
195.289639	60.290655	50.469351
192.057555	58.582560	50.474356
188.416941	55.141113	50.479361
184.787501	61.856426	50.484365
181.535513	55.292056	50.489370
177.824460	52.076707	50.494375
174.400362	56.428436	50.499380
171.483873	58.717524	50.504385
167.268782	63.382224	50.509389
163.787786	47.296113	50.514394
160.115863	55.669466	50.519399
156.330477	58.982822	50.524404
152.830542	57.164580	50.529409
149.800532	59.531454	50.534413
146.819211	52.273238	50.539418
143.490229	53.955856	50.544423
139.755855	57.055634	50.549428
136.431272	57.684071	50.554433
132.019979	55.099754	50.559437
129.040254	53.988273	50.564442
125.272134	54.420019	50.569447
121.521359	56.098709	50.574452
118.491623	47.759742	50.579457
114.718088	63.292451	50.584461
111.467111	50.432268	50.589466
108.041108	45.312325	50.594471
104.237477	51.377740	50.599476
100.959745	55.099267	50.604481
97.172384	67.046550	50.609485
93.635363	54.347958	50.614490
90.371654	55.454126	50.619495
86.562036	59.837415	50.624500
83.193505	59.786188	50.629505
79.835999	59.872447	50.634509
76.497819	58.272633	50.639514
72.596076	63.208089	50.644519
69.487939	55.963304	50.649524
66.036510	51.347183	50.654529
62.399108	63.391336	50.659533
58.923177	63.046797	50.664538
54.773370	61.184223	50.669543
51.801023	55.639327	50.674548
48.648182	57.718462	50.679553
44.452177	62.155587	50.684557
41.586599	57.388146	50.689562
37.462607	57.982878	50.694567
33.993761	52.942381	50.699572
30.909131	55.412681	50.704577
26.911158	58.676898	50.709581
23.618330	56.462611	50.714586
20.330619	62.548948	50.719591
16.894463	58.287950	50.724596
13.314708	58.206347	50.729601
9.323913	60.697518	50.734605
6.276699	63.019632	50.739610
2.301106	56.175667	50.744615