Fri Aug 26 11:43:49 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.667448	99.731481	0.000000
1.638696	94.117336	0.005005
1.156589	89.772805	0.010010
1.459962	82.496651	0.015014
1.077950	86.975796	0.020019
1.007980	71.497467	0.025024
0.692253	63.760910	0.030029
0.512333	61.096691	0.035034
0.228757	49.239223	0.040038
-0.367456	51.252425	0.045043
-0.733487	42.406940	0.050048
-0.743337	32.610691	0.055053
-1.405271	36.940425	0.060058
-1.272953	37.049570	0.065062
-1.368616	23.489291	0.070067
-1.758434	20.892560	0.075072
-1.787001	13.623825	0.080077
-2.091353	20.409814	0.085082
-2.419000	5.901773	0.090086
-2.485158	9.142192	0.095091
-3.306043	-3.327586	0.100096
-3.982378	-13.222512	0.105101
-3.844164	-8.634571	0.110106
-3.960500	-4.187323	0.115110
-4.314704	-0.908385	0.120115
-4.245327	-14.544950	0.125120
-4.759764	-19.513984	0.130125
-5.400713	-14.940766	0.135130
-5.193995	-16.731897	0.140134
-5.526376	-18.549819	0.145139
-5.866094	-13.400266	0.150144
-6.335307	-16.297830	0.155149
-6.724375	-11.381029	0.160154
-6.598585	-16.854691	0.165158
-7.238701	-15.432587	0.170163
-6.779609	-15.099083	0.175168
-7.056016	-13.005971	0.180173
-7.889627	-9.193666	0.185178
-7.575603	-16.597983	0.190182
-8.132892	-11.009607	0.195187
-8.269370	-11.244575	0.200192
-8.078234	-10.787096	0.205197
-9.108271	-10.060393	0.210202
-9.429337	-10.510221	0.215206
-9.674752	-8.507352	0.220211
-9.616556	-12.847399	0.225216
-9.640290	-19.930217	0.230221
-10.207707	-8.848187	0.235226
-10.498626	-17.338354	0.240230
-11.109771	-11.732102	0.245235
-10.996034	-9.807298	0.250240
-10.937397	-22.097637	0.255245
-11.393530	-11.086717	0.260250
-11.434260	-11.586520	0.265254
-11.797025	-9.574871	0.270259
-12.146627	-15.471207	0.275264
-12.389626	-8.656819	0.280269
-12.554452	-5.081514	0.285274
-12.588717	-11.871640	0.290278
-13.460649	-8.670278	0.295283
-13.585304	-16.053748	0.300288
-13.587770	-14.278525	0.305293
-13.978573	-9.930908	0.310298
-14.101359	-17.624706	0.315302
-14.083243	-7.333006	0.320307
-14.706126	-6.280567	0.325312
-14.740507	-15.193477	0.330317
-15.256977	-6.403525	0.335322
-15.373455	-9.368665	0.340326
-15.239849	-4.359241	0.345331
-16.182198	-2.700261	0.350336
-16.343373	-12.200850	0.355341
-16.745318	-3.330656	0.360346
-16.769842	-11.185283	0.365350
-16.919196	-10.494463	0.370355
-17.195340	-8.255864	0.375360
-17.226191	-16.947868	0.380365
-17.429434	-16.400512	0.385370
-18.182027	-12.006057	0.390374
-18.261939	-8.655937	0.395379
-18.596570	-3.358482	0.400384
-18.240242	-11.895644	0.405389
-18.999668	-9.461581	0.410394
-19.582287	-14.388363	0.415398
-19.915847	-5.873654	0.420403
-19.985258	-8.105830	0.425408
-19.759780	-15.116724	0.430413
-19.985221	-13.208711	0.435418
-19.914496	-15.418414	0.440422
-20.515088	-9.873915	0.445427
-20.689176	-14.310667	0.450432
-21.244335	-13.120082	0.455437
-22.094066	-7.562101	0.460442
-21.670452	-10.003913	0.465446
-21.647512	-5.935842	0.470451
-21.986913	-8.002599	0.475456
-22.324837	-2.315503	0.480461
-23.150322	-0.272936	0.485466
-23.042101	-13.668783	0.490470
-23.195108	-6.090151	0.495475
-23.083828	-9.116061	0.500480
-23.672643	-10.830784	0.505485
-23.992644	-5.010443	0.510490
-24.166010	-7.245415	0.515494
-24.257703	-3.453714	0.520499
-24.757656	-13.515301	0.525504
-24.839984	-5.327600	0.530509
-25.548421	0.315949	0.535514
-25.940090	-11.543629	0.540518
-25.844710	6.094675	0.545523
-26.107811	-7.664126	0.550528
-25.484633	-7.128388	0.555533
-25.854534	-4.495555	0.560538
-26.658969	-7.264998	0.565542
-27.282878	-6.006763	0.570547
-27.201765	-5.443572	0.575552
-26.932232	-11.505907	0.580557
-27.468966	-1.093015	0.585562
-28.109728	-11.088388	0.590566
-28.327728	-1.987415	0.595571
-28.560606	-11.306003	0.600576
-28.566707	-11.039270	0.605581
-29.082150	-3.587697	0.610586
-29.399440	-12.592595	0.615590
-29.946832	-8.897617	0.620595
-30.120026	-5.257736	0.625600
-30.168809	-11.909564	0.630605
-30.575848	-7.353783	0.635610
-30.419686	-18.359051	0.640614
-30.304067	-11.015228	0.645619
-30.239099	-16.492073	0.650624
-30.662649	-8.890301	0.655629
-31.498523	0.297384	0.660634
-31.693787	-7.160514	0.665638
-31.855673	-7.290289	0.670643
-32.499962	-9.986594	0.675648
-32.828638	-9.267854	0.680653
-33.478267	-3.633463	0.685658
-32.986039	-7.604506	0.690662
-33.322676	-2.740157	0.695667
-33.374405	-4.355013	0.700672
-33.590281	-8.054459	0.705677
-33.521588	-1.073472	0.710682
-33.886140	-6.964318	0.715686
-34.304355	-9.803386	0.720691
-35.037599	-10.144747	0.725696
-34.786738	-5.650272	0.730701
-34.952018	-4.552027	0.735706
-35.236135	-4.944335	0.740710
-36.100451	-7.777219	0.745715
-36.300693	-6.338183	0.750720
-36.057926	-14.563443	0.755725
-36.211118	-1.884995	0.760730
-36.422133	-1.810975	0.765734
-37.390759	-5.839292	0.770739
-37.971646	-8.763760	0.775744
-37.405362	-10.778548	0.780749
-37.841727	-2.352232	0.785754
-37.916083	-4.102765	0.790758
-37.662388	-2.070043	0.795763
-38.449981	-7.167385	0.800768
-38.538759	-21.181098	0.805773
-38.999195	-4.860922	0.810778
-39.033843	-6.592328	0.815782
-39.214076	-11.123033	0.820787
-40.141663	-3.850890	0.825792
-40.547640	-7.799138	0.830797
-41.128462	-0.343712	0.835802
-40.260058	-11.187805	0.840806
-40.364541	-3.426910	0.845811
-40.790738	-11.253795	0.850816
-40.918000	-10.604378	0.855821
-41.173051	-0.811127	0.860826
-41.585836	-8.909011	0.865830
-42.166268	-9.720238	0.870835
-42.437198	-15.268166	0.875840
-42.289913	-10.251384	0.880845
-42.735909	-2.880225	0.885850
-42.973465	-19.509250	0.890854
-43.007004	-12.964750	0.895859
-43.482702	-17.269122	0.900864
-43.277576	-13.175638	0.905869
-44.182684	-5.647578	0.910874
-44.730186	-11.497283	0.915878
-45.069455	-7.322199	0.920883
-45.276213	-8.678807	0.925888
-44.793113	-12.009372	0.930893
-45.030544	-8.542982	0.935898
-45.078214	-10.133160	0.940902
-45.344307	-0.512190	0.945907
-46.162726	-10.369173	0.950912
-46.276609	-10.563367	0.955917
-46.725926	1.218424	0.960922
-46.828883	-8.515847	0.965926
-46.824160	-8.592472	0.970931
-47.268067	-7.305317	0.975936
-47.273940	-14.878116	0.980941
-47.477960	-5.969142	0.985946
-47.962033	-3.669696	0.990950
-48.041146	-12.278258	0.995955
-48.561361	-4.917689	1.000960
-49.240693	-13.420142	1.005965
-49.343216	-1.540493	1.010970
-49.432188	-9.052902	1.015974
-49.150884	-5.534405	1.020979
-49.495861	-7.056147	1.025984
-49.473395	-10.612374	1.030989
-50.342030	-2.428791	1.035994
-50.826120	-7.788514	1.040998
-50.635838	-10.418615	1.046003
-51.070949	-4.760680	1.051008
-51.188107	-9.747278	1.056013
-51.451891	3.195155	1.061018
-52.200013	-10.611505	1.066022
-52.585530	7.085853	1.071027
-52.433371	-7.936621	1.076032
-52.639053	-10.144415	1.081037
-52.601568	-9.055595	1.086042
-52.504967	-5.236267	1.091046
-52.728647	-8.912351	1.096051
-53.599154	-3.164479	1.101056
-53.393066	-10.545664	1.106061
-53.575791	-3.427460	1.111066
-53.921056	-6.069086	1.116070
-54.590775	-3.785026	1.121075
-55.145296	-2.388902	1.126080
-54.945418	-2.812277	1.131085
-55.281611	5.845209	1.136090
-55.066173	-14.992392	1.141094
-56.123640	-1.610023	1.146099
-56.181777	-6.881048	1.151104
-56.264640	-3.271050	1.156109
-56.597445	1.504120	1.161114
-56.735039	-16.551454	1.166118
-56.578786	-9.261413	1.171123
-57.689765	-4.229046	1.176128
-57.854806	-10.207899	1.181133
-58.353807	-1.977468	1.186138
-58.167107	-11.589163	1.191142
-58.119898	-4.582688	1.196147
-58.323164	-2.187762	1.201152
-58.093282	-2.682245	1.206157
-58.888935	2.196627	1.211162
-59.141392	-7.172693	1.216166
-59.327779	0.642083	1.221171
-59.942923	2.354519	1.226176
-60.673246	-5.773015	1.231181
-60.770703	0.696022	1.236186
-60.351880	-6.142504	1.241190
-60.927667	-4.353942	1.246195
-61.206912	-2.317333	1.251200
-60.835009	-8.550625	1.256205
-61.108655	-3.582194	1.261210
-61.770841	-6.788221	1.266214
-62.276325	-2.805548	1.271219
-62.531437	-8.460340	1.276224
-62.253969	-13.150889	1.281229
-63.040378	-6.710621	1.286234
-62.709243	-9.982726	1.291238
-62.842753	-15.539395	1.296243
-63.637583	-14.194438	1.301248
-64.225903	-10.546869	1.306253
-64.057030	-6.995050	1.311258
-63.926490	-17.759052	1.316262
-64.315190	-19.659949	1.321267
-65.027634	-8.064978	1.326272
-65.366908	-10.337390	1.331277
-65.457242	-10.402378	1.336282
-65.370974	-4.341586	1.341286
-65.577569	-5.764655	1.346291
-66.084978	-7.438270	1.351296
-66.399561	-15.845657	1.356301
-66.976594	-9.387372	1.361306
-67.180237	-5.366278	1.366310
-67.094311	-5.686492	1.371315
-67.175173	-12.383942	1.376320
-67.137165	-13.952659	1.381325
-67.381663	-4.110437	1.386330
-67.945288	-13.437631	1.391334
-68.557381	-9.103015	1.396339
-68.954157	-13.134948	1.401344
-68.521199	-15.312468	1.406349
-68.934022	-11.442297	1.411354
-69.599275	-15.736136	1.416358
-70.157896	-20.609704	1.421363
-70.225134	-18.052469	1.426368
-70.309782	-16.213834	1.431373
-70.449232	-4.420185	1.436378
-70.122078	-17.631820	1.441382
-70.336523	-14.368320	1.446387
-70.668407	-9.030168	1.451392
-71.320624	-19.264185	1.456397
-71.603203	-10.099382	1.461402
-71.383536	-16.739222	1.466406
-71.539891	-25.294622	1.471411
-72.559537	-14.265570	1.476416
-72.661043	-12.424309	1.481421
-72.955506	-13.846351	1.486426
-72.754925	-8.967577	1.491430
-73.290278	-12.085787	1.496435
-73.937474	-7.831123	1.501440
-74.004213	-7.127858	1.506445
-74.463450	-10.802064	1.511450
-74.723782	-16.690150	1.516454
-74.609988	-16.239612	1.521459
-75.209005	-8.578885	1.526464
-74.901260	-21.733713	1.531469
-74.818268	-14.909978	1.536474
-75.665691	-16.166833	1.541478
-75.929768	-17.343679	1.546483
-76.294378	-8.507776	1.551488
-76.185722	-12.874659	1.556493
-76.269047	-11.320956	1.561498
-76.434103	-12.741001	1.566502
-76.891105	-14.881191	1.571507
-77.506850	-14.206336	1.576512
-77.718094	-23.430208	1.581517
-78.161723	-7.786511	1.586522
-77.860849	-8.706484	1.591526
-78.165695	-2.512031	1.596531
-78.669660	-11.114550	1.601536
-78.431663	-12.258842	1.606541
-79.228113	-3.156390	1.611546
-78.989165	-18.511892	1.616550
-79.661945	-11.001027	1.621555
-80.436307	-8.710165	1.626560
-80.243787	-13.627924	1.631565
-80.523840	-11.309626	1.636570
-80.584623	-13.093907	1.641574
-80.530989	-16.272185	1.646579
-80.532515	-7.704778	1.651584
-80.994049	-13.605828	1.656589
-82.056391	-7.416816	1.661594
-82.117679	-18.786840	1.666598
-82.240031	-8.742185	1.671603
-82.196639	-16.803525	1.676608
-82.024959	-17.184545	1.681613
-83.018122	-7.956559	1.686618
-83.432552	-15.472070	1.691622
-83.771510	-8.892672	1.696627
-83.745078	-15.891552	1.701632
-83.797335	-11.928831	1.706637
-83.929849	-15.059144	1.711642
-83.989934	-13.847569	1.716646
-84.002912	-12.238383	1.721651
-84.866128	-11.047287	1.726656
-85.014612	-19.161005	1.731661
-85.323594	-11.842820	1.736666
-85.811235	-12.810857	1.741670
-86.400090	-17.376007	1.746675
-86.681974	-13.197207	1.751680
-86.701848	-19.094257	1.756685
-86.845328	-10.027041	1.761690
-86.718059	-15.456639	1.766694
-86.944853	-9.185760	1.771699
-87.309462	-1.808292	1.776704
-86.951373	-7.593359	1.781709
-88.358667	-0.683108	1.786714
-88.013664	-7.377266	1.791718
-87.812066	-6.813853	1.796723
-88.474265	-7.239038	1.801728
-88.454598	-11.946392	1.806733
-89.362151	-4.022498	1.811738
-89.615429	-5.568007	1.816742
-89.553043	-2.923390	1.821747
-89.969026	-4.307530	1.826752
-89.373805	-12.062501	1.831757
-90.203697	-8.975247	1.836762
-90.857507	-5.826826	1.841766
-91.107172	-8.065735	1.846771
-91.397499	-8.605766	1.851776
-91.036075	-10.373531	1.856781
-91.376399	-17.087524	1.861786
-91.947617	-8.197308	1.866790
-92.499545	-11.876064	1.871795
-93.109250	-1.777670	1.876800
-92.872887	-11.890622	1.881805
-93.167404	-6.934762	1.886810
-93.065727	-20.373868	1.891814
-92.719086	-22.012784	1.896819
-92.996142	-19.122336	1.901824
-93.884904	-15.668426	1.906829
-94.299989	-15.404450	1.911834
-94.194381	-14.231328	1.916838
-94.147562	-7.854359	1.921843
-94.662702	0.520947	1.926848
-95.092057	-12.303991	1.931853
-95.596358	-9.760959	1.936858
-95.826623	-13.436015	1.941862
-95.808998	-11.600649	1.946867
-96.162475	-12.326993	1.951872
-96.455879	-15.473381	1.956877
-97.212454	-9.341469	1.961882
-97.229975	-6.779320	1.966886
-97.445656	-13.933486	1.971891
-97.571723	-13.455092	1.976896
-96.949214	-14.083471	1.981901
-97.084026	-12.705242	1.986906
-97.829534	-10.187927	1.991910
-98.194355	-10.371523	1.996915
-98.607436	-12.266345	2.006912
-98.711781	-12.851884	2.016909
-98.318762	-12.456855	2.026906
-97.645207	-16.771510	2.036902
-96.372402	-16.510298	2.046899
-96.098531	-16.882304	2.056896
-96.194418	-15.311964	2.066893
-96.009857	-17.627696	2.076890
-95.036183	-9.745966	2.086886
-94.005884	-18.661799	2.096883
-93.445302	-15.926597	2.106880
-93.419631	-11.970909	2.116877
-93.319127	-7.871655	2.126874
-92.455946	-6.694555	2.136870
-91.901092	-15.105556	2.146867
-91.739473	-9.248248	2.156864
-91.053065	-4.179043	2.166861
-90.127362	-11.539096	2.176858
-89.628164	-8.822845	2.186854
-89.675765	-8.242007	2.196851
-89.091343	-12.010613	2.206848
-88.302767	-11.721521	2.216845
-87.995511	-7.255329	2.226842
-87.286994	-5.439615	2.236838
-86.726833	-7.718798	2.246835
-86.316184	-14.564683	2.256832
-85.892565	-5.662838	2.266829
-85.267949	-8.458888	2.276826
-85.132276	-4.602685	2.286822
-83.933412	-11.469930	2.296819
-83.532947	-6.403719	2.306816
-83.759419	-8.268996	2.316813
-83.146608	-5.336024	2.326810
-82.204686	-6.800366	2.336806
-82.095470	-13.254039	2.346803
-81.144438	-6.670701	2.356800
-81.007859	-0.549741	2.366797
-80.304146	-7.184675	2.376794
-79.381097	-16.850391	2.386790
-79.335849	-9.606522	2.396787
-79.297556	-8.063409	2.406784
-78.559058	-8.811856	2.416781
-77.949276	2.889754	2.426778
-76.978984	-0.390924	2.436774
-76.544262	-3.258774	2.446771
-76.634780	-6.551673	2.456768
-76.138157	-11.580020	2.466765
-75.246026	-7.274582	2.476762
-74.897774	-3.093529	2.486758
-74.004639	-1.426931	2.496755
-73.494800	-4.046726	2.506752
-73.499050	-3.688040	2.516749
-73.319115	-4.745480	2.526746
-72.108969	-9.270392	2.536742
-72.080375	-11.048674	2.546739
-71.132884	-3.606339	2.556736
-70.821765	-7.132829	2.566733
-70.736970	-10.709607	2.576730
-69.428924	-12.516045	2.586726
-69.092249	-11.203116	2.596723
-68.980362	-6.050793	2.606720
-68.569569	-8.715351	2.616717
-68.001142	-5.446029	2.626714
-67.310146	-4.343484	2.636710
-66.643487	-9.436319	2.646707
-66.458206	-16.779285	2.656704
-65.743064	-7.583888	2.666701
-65.289480	-8.468532	2.676698
-65.159151	-10.829671	2.686694
-63.937908	-4.649519	2.696691
-63.519300	-7.597219	2.706688
-63.621377	-1.610154	2.716685
-63.011808	-7.071056	2.726682
-62.291312	-6.413413	2.736678
-62.072593	-10.099739	2.746675
-60.765194	-5.991999	2.756672
-60.421294	-1.737410	2.766669
-60.695048	-2.017816	2.776666
-59.890300	-2.646703	2.786662
-59.408717	-3.662414	2.796659
-58.804673	0.025835	2.806656
-57.892102	1.556364	2.816653
-57.801616	-0.313916	2.826650
-57.695748	-3.368140	2.836646
-56.980535	-1.537629	2.846643
-56.491597	-7.385213	2.856640
-55.666970	-0.579457	2.866637
-55.447411	-4.215232	2.876634
-54.719910	-3.362282	2.886630
-54.030954	-7.302382	2.896627
-53.706591	-4.891515	2.906624
-53.510321	-3.962189	2.916621
-52.953988	-2.030915	2.926618
-52.435868	1.195559	2.936614
-51.721305	-1.421266	2.946611
-51.059913	-4.124844	2.956608
-50.992775	-0.023559	2.966605
-50.272164	-5.615788	2.976602
-49.515959	-6.503202	2.986598
-49.446172	-8.557152	2.996595
-48.707336	-1.174190	3.006592
-48.166771	0.379417	3.016589
-47.811671	1.575441	3.026586
-47.397849	-7.592859	3.036582
-46.815462	-4.034282	3.046579
-46.132544	-6.022144	3.056576
-45.380266	-6.741059	3.066573
-45.126468	-4.658147	3.076570
-44.721295	-3.378056	3.086566
-44.677094	1.154439	3.096563
-43.593869	-4.275678	3.106560
-43.446977	-0.608114	3.116557
-42.812790	1.526442	3.126554
-41.813408	-2.126217	3.136550
-41.949847	4.604273	3.146547
-41.574667	1.248366	3.156544
-40.701100	6.991665	3.166541
-40.411771	0.623978	3.176538
-39.292443	0.643004	3.186534
-38.767777	-3.683317	3.196531
-39.300998	-2.181094	3.206528
-38.716002	-0.251115	3.216525
-37.795787	-0.954998	3.226522
-37.149160	-2.867521	3.236518
-36.077550	-3.417585	3.246515
-36.145400	-6.530289	3.256512
-36.147971	-3.637711	3.266509
-35.293635	-7.619399	3.276506
-34.798925	-5.393439	3.286502
-34.343758	-12.192407	3.296499
-33.210651	-0.426560	3.306496
-33.011656	-2.760380	3.316493
-33.094682	0.680065	3.326490
-32.258663	-0.302136	3.336486
-31.588652	-5.424004	3.346483
-31.489140	-2.382600	3.356480
-30.903961	0.301262	3.366477
-30.306457	-7.299122	3.376474
-29.332485	-6.737962	3.386470
-28.830339	-2.843786	3.396467
-28.704305	2.683295	3.406464
-28.870904	-0.391861	3.416461
-27.794685	-6.210513	3.426458
-27.281517	-7.414868	3.436454
-26.648284	-5.622274	3.446451
-26.259994	-8.124945	3.456448
-25.775975	-5.909990	3.466445
-25.124307	-6.888829	3.476442
-24.284424	-7.380638	3.486438
-23.989719	-8.370420	3.496435
-24.055371	-7.527020	3.506432
-23.150606	2.658860	3.516429
-22.614939	-5.356368	3.526426
-22.380601	-7.173021	3.536422
-21.661369	-6.255429	3.546419
-21.344915	-4.426184	3.556416
-20.613271	-5.810269	3.566413
-20.042354	-10.986396	3.576410
-19.982151	-7.143782	3.586406
-19.143889	-9.494774	3.596403
-18.435024	1.678251	3.606400
-18.484630	-6.632310	3.616397
-17.642622	-5.312531	3.626394
-17.111541	-13.346048	3.636390
-16.493224	-5.237924	3.646387
-16.334897	-9.820807	3.656384
-15.419609	-6.028968	3.666381
-14.918520	-9.166901	3.676378
-15.215316	-10.878683	3.686374
-14.122204	-15.809842	3.696371
-13.764434	-6.964260	3.706368
-12.981154	-1.998827	3.716365
-12.137908	-5.681026	3.726362
-12.206097	-11.562239	3.736358
-11.978487	-8.474259	3.746355
-11.127272	-11.574842	3.756352
-11.065010	-9.699685	3.766349
-10.411145	-8.968312	3.776346
-9.693715	-9.501242	3.786342
-8.951284	-13.718921	3.796339
-8.351093	-15.621045	3.806336
-7.995827	-17.396339	3.816333
-8.156042	-10.763517	3.826330
-7.349094	-5.272765	3.836326
-6.889932	-0.849225	3.846323
-5.688630	-5.930273	3.856320
-5.820682	-0.521394	3.866317
-5.631785	1.530445	3.876314
-4.897062	3.541648	3.886310
-4.246942	12.449424	3.896307
-3.936491	22.053132	3.906304
-3.476180	29.986309	3.916301
-2.706892	39.860699	3.926298
-2.560971	48.748797	3.936294
-1.970366	58.125179	3.946291
-1.776781	69.464004	3.956288
-1.386631	80.712045	3.966285
-0.575962	95.756058	3.976282
-0.029041	118.107882	3.986278
0.000000	121.322096	3.991283
0.487325	133.325131	3.996288
0.889208	130.329878	4.001293
0.857253	137.760015	4.006298
0.549307	143.588019	4.011302
0.906432	135.882707	4.016307
1.228711	146.044884	4.021312
1.394973	148.939101	4.026317
1.358284	140.567459	4.031322
0.730476	141.519435	4.036326
0.711756	146.248906	4.041331
0.838946	144.840291	4.046336
0.954047	161.612001	4.051341
1.654941	158.082983	4.056346
1.382586	158.043171	4.061350
1.538408	154.621166	4.066355
1.502318	153.617612	4.071360
1.005185	152.129036	4.076365
1.141157	149.858534	4.081370
0.894297	160.935051	4.086374
1.281226	157.439099	4.091379
1.166710	167.235874	4.096384
1.111332	167.545082	4.101389
1.525915	160.995044	4.106394
1.352527	175.891337	4.111398
1.711436	165.904725	4.116403
1.776334	160.801148	4.121408
1.410779	164.274866	4.126413
1.625730	165.304430	4.131418
1.335659	164.077835	4.136422
1.044382	150.914901	4.141427
1.472697	164.442542	4.146432
1.452407	166.745728	4.151437
1.698918	159.478396	4.156442
1.337854	170.246842	4.161446
1.811332	167.547313	4.166451
1.377177	167.950296	4.171456
1.491967	160.931257	4.176461
1.632476	151.301352	4.181466
1.275487	161.414279	4.186470
1.752553	157.107048	4.191475
1.835004	157.160685	4.196480
1.287611	154.680214	4.201485
1.481300	156.475532	4.206490
1.417664	168.374554	4.211494
1.408097	175.143177	4.216499
1.663630	175.530525	4.221504
1.880406	166.701801	4.226509
1.735278	165.550713	4.231514
1.871734	169.379693	4.236518
1.523944	158.952638	4.241523
1.622835	166.599690	4.246528
1.533543	172.203839	4.251533
1.489216	166.044781	4.256538
1.694408	166.889208	4.261542
1.919186	166.898540	4.266547
2.199228	167.952770	4.271552
1.756788	172.074359	4.276557
1.860410	162.121169	4.281562
1.534291	162.105546	4.286566
1.699433	162.102017	4.291571
2.101169	163.687778	4.296576
1.612358	166.111367	4.301581
2.402259	166.605335	4.306586
1.871419	152.217394	4.311590
1.624832	152.252661	4.316595
1.722766	147.678604	4.321600
2.024589	164.278880	4.326605
1.855327	160.853706	4.331610
1.711365	162.296646	4.336614
1.726930	160.348603	4.341619
1.908732	164.287578	4.346624
2.214464	162.145664	4.351629
2.397237	158.361967	4.356634
1.608701	156.963052	4.361638
2.044289	160.660038	4.366643
1.837481	173.223579	4.371648
1.933369	168.244885	4.376653
2.164799	167.155387	4.381658
1.932456	174.464883	4.386662
2.042412	173.903649	4.391667
2.335293	163.841900	4.396672
1.963034	165.089438	4.401677
2.249776	169.875758	4.406682
2.114193	174.689869	4.411686
2.083738	178.690369	4.416691
2.080680	175.226660	4.421696
2.122085	171.066348	4.426701
2.089267	169.299839	4.431706
2.180834	181.959296	4.436710
1.957006	179.520190	4.441715
1.946092	177.418083	4.446720
1.873611	176.170264	4.451725
2.173328	175.351700	4.456730
2.023133	178.336321	4.461734
2.042731	179.244446	4.466739
2.205319	172.999387	4.471744
2.039519	172.288104	4.476749
2.270467	169.164439	4.481754
2.257788	172.950203	4.486758
1.965779	168.743730	4.491763
2.078759	169.627824	4.496768
1.826315	167.028664	4.501773
2.635971	183.907384	4.506778
2.760787	181.679744	4.511782
2.083508	178.128024	4.516787
2.352863	177.428080	4.521792
2.585496	184.643039	4.526797
2.262758	179.789631	4.531802
2.184247	185.246576	4.536806
2.731709	188.774293	4.541811
2.437351	175.773168	4.546816
2.152832	177.358213	4.551821
2.454293	195.325281	4.556826
2.836920	189.947605	4.561830
2.944965	187.425189	4.566835
2.495089	182.430228	4.571840
2.432761	174.581404	4.576845
2.542341	171.558891	4.581850
2.541682	183.210841	4.586854
2.351074	171.082558	4.591859
2.481711	168.990051	4.596864
2.231794	169.259948	4.601869
2.253512	173.208031	4.606874
2.670077	192.466936	4.611878
3.069445	190.870410	4.616883
2.563000	191.294140	4.621888
2.516686	188.678702	4.626893
2.504990	180.002600	4.631898
2.772458	186.291507	4.636902
2.493199	194.702948	4.641907
3.222568	188.632222	4.646912
2.920069	185.272080	4.651917
2.568265	175.158843	4.656922
2.353181	184.569499	4.661926
2.343405	179.550308	4.666931
2.189060	198.974036	4.671936
2.182294	200.996717	4.676941
2.756198	191.046219	4.681946
2.591421	187.218555	4.686950
2.592963	183.975585	4.691955
2.524994	189.763077	4.696960
2.512370	198.148823	4.701965
2.943666	203.153085	4.706970
2.962133	210.176778	4.711974
2.999628	202.059305	4.716979
2.885784	203.440614	4.721984
2.915245	203.682831	4.726989
2.924323	194.791522	4.731994
2.762259	204.380590	4.736998
3.053844	201.411990	4.742003
2.902209	193.143638	4.747008
2.531098	203.869377	4.752013
3.170544	213.387440	4.757018
3.071920	214.310809	4.762022
3.183486	217.811489	4.767027
3.108041	205.785472	4.772032
2.724508	205.377000	4.777037
2.929696	201.950464	4.782042
2.975025	213.500364	4.787046
3.424513	211.889705	4.792051
2.960473	205.239174	4.797056
3.210150	203.637481	4.802061
2.990786	188.413259	4.807066
2.876849	199.617797	4.812070
3.197591	206.436241	4.817075
3.294073	219.974462	4.822080
3.225496	204.062377	4.827085
3.157827	194.901449	4.832090
3.010463	203.361959	4.837094
3.089368	200.227161	4.842099
3.210770	210.610472	4.847104
2.998680	217.242968	4.852109
3.391132	220.057689	4.857114
3.090106	223.815594	4.862118
3.530788	214.977294	4.867123
3.603909	210.562105	4.872128
2.769438	205.937057	4.877133
3.199697	210.017688	4.882138
3.747687	223.204046	4.887142
3.744849	207.522161	4.892147
3.379384	199.027678	4.897152
3.178889	197.891536	4.902157
3.276276	193.557991	4.907162
3.146357	193.252398	4.912166
2.675784	194.958160	4.917171
3.156055	200.524258	4.922176
3.521037	213.947905	4.927181
3.906428	218.465784	4.932186
3.556897	218.365223	4.937190
3.403016	213.302021	4.942195
2.981768	209.514284	4.947200
3.286859	215.724578	4.952205
3.285680	218.780915	4.957210
3.055936	215.108890	4.962214
3.479350	209.323070	4.967219
3.744357	216.681694	4.972224
3.048830	214.069258	4.977229
3.289349	206.369416	4.982234
3.576893	216.195365	4.987238
3.742996	217.270502	4.992243
3.729936	217.320028	4.997248
3.681667	210.263083	5.002253
3.593817	203.130048	5.007258
3.589784	218.319540	5.012262
3.384398	213.685127	5.017267
3.422039	217.054951	5.022272
3.687786	226.143997	5.027277
3.537108	212.962290	5.032282
3.635101	218.980209	5.037286
3.397334	211.437088	5.042291
3.592245	218.072653	5.047296
3.572795	221.264710	5.052301
3.775295	208.866392	5.057306
3.629123	223.078296	5.062310
3.591147	220.705158	5.067315
3.601210	230.830576	5.072320
3.962638	238.088777	5.077325
4.144674	225.288683	5.082330
3.679594	220.071456	5.087334
3.664548	221.949900	5.092339
3.656346	219.992895	5.097344
3.901246	227.519167	5.102349
3.657405	222.055526	5.107354
4.015284	238.552233	5.112358
3.917562	232.746307	5.117363
3.822338	235.007387	5.122368
3.890293	233.000560	5.127373
4.180530	241.510011	5.132378
3.907491	229.340739	5.137382
3.700156	224.320658	5.142387
3.714736	226.697514	5.147392
3.819441	240.493893	5.152397
4.098883	227.548920	5.157402
4.215978	234.554103	5.162406
3.995095	235.430071	5.167411
4.190976	231.774029	5.172416
3.643705	226.895457	5.177421
3.996437	239.979354	5.182426
4.112032	239.062907	5.187430
4.306398	241.437083	5.192435
4.313319	236.646225	5.197440
3.677228	230.800738	5.202445
4.110335	231.546409	5.207450
4.440654	246.411790	5.212454
3.978533	233.990387	5.217459
4.014900	227.059460	5.222464
4.012753	239.331761	5.227469
4.309086	247.644117	5.232474
4.172822	241.825207	5.237478
4.198661	246.525622	5.242483
4.167265	244.913905	5.247488
4.128332	246.166496	5.252493
4.194406	232.289817	5.257498
4.257532	244.438066	5.262502
4.194153	244.900378	5.267507
4.441669	237.772060	5.272512
4.251571	239.396193	5.277517
4.416405	237.870980	5.282522
4.023150	229.061277	5.287526
3.969231	243.796660	5.292531
4.218340	244.618434	5.297536
4.032813	254.233328	5.302541
4.345346	246.205887	5.307546
4.050792	243.657564	5.312550
4.274726	243.644882	5.317555
4.458511	240.838589	5.322560
4.406279	240.637956	5.327565
4.500855	250.278838	5.332570
4.198578	247.326764	5.337574
4.288638	252.507553	5.342579
4.243942	245.586077	5.347584
4.089354	242.791339	5.352589
4.237343	239.835599	5.357594
4.083450	250.856570	5.362598
4.271331	259.132034	5.367603
4.321361	261.066787	5.372608
4.656842	264.538941	5.377613
4.652200	259.958680	5.382618
4.585053	262.174263	5.387622
4.875705	263.432487	5.392627
4.854598	261.373086	5.397632
4.172395	252.877273	5.402637
4.575424	258.955278	5.407642
4.468148	262.619752	5.412646
4.414437	273.726376	5.417651
4.730109	264.135575	5.422656
4.618402	278.588925	5.427661
4.664637	269.267858	5.432666
4.654627	267.285821	5.437670
4.504533	273.063980	5.442675
4.643395	260.093416	5.447680
4.406454	272.095418	5.452685
4.727600	272.542154	5.457690
4.800232	274.245603	5.462694
4.488655	266.122341	5.467699
4.711300	263.550435	5.472704
4.643115	268.698920	5.477709
4.928700	267.455455	5.482714
4.778024	272.256125	5.487718
4.844166	266.595514	5.492723
4.858999	262.040693	5.497728
4.677366	270.291440	5.502733
4.382234	271.466866	5.507738
4.656101	276.312166	5.512742
4.395858	270.670734	5.517747
4.883059	272.236871	5.522752
4.538627	281.851211	5.527757
4.881344	280.491284	5.532762
5.101368	293.225730	5.537766
5.055406	290.334981	5.542771
5.113903	284.757810	5.547776
4.833445	283.567674	5.552781
4.828687	280.933097	5.557786
5.190209	287.792679	5.562790
4.965769	293.209105	5.567795
4.979389	296.649121	5.572800
4.616833	299.894613	5.577805
5.026148	296.828575	5.582810
5.253643	297.406949	5.587814
5.007263	294.664459	5.592819
5.296911	292.148554	5.597824
5.057370	290.717934	5.602829
5.044948	293.345772	5.607834
5.196541	292.392081	5.612838
5.243670	294.131140	5.617843
5.173044	290.883569	5.622848
4.954561	292.951879	5.627853
4.747371	293.851028	5.632858
4.733465	296.662592	5.637862
5.248408	292.858786	5.642867
5.170544	283.955658	5.647872
4.913853	287.915478	5.652877
5.011630	292.867291	5.657882
4.958409	289.930216	5.662886
4.784624	290.194589	5.667891
5.244516	294.982457	5.672896
4.870482	298.482831	5.677901
5.139879	307.558696	5.682906
5.123903	308.513494	5.687910
5.613053	313.037388	5.692915
5.691497	311.041574	5.697920
5.350604	299.654761	5.702925
5.262591	294.132036	5.707930
5.247165	291.416862	5.712934
5.294831	299.793270	5.717939
5.461122	297.283916	5.722944
5.308157	304.732963	5.727949
5.635679	309.993854	5.732954
5.488844	301.971473	5.737958
5.472870	294.355820	5.742963
5.414328	286.000166	5.747968
5.272252	292.444622	5.752973
5.257479	292.921514	5.757978
5.513901	308.459665	5.762982
5.311886	315.925845	5.767987
5.731918	306.208044	5.772992
5.199419	319.319098	5.777997
5.984391	314.710794	5.783002
5.494419	307.656144	5.788006
5.384354	304.262854	5.793011
5.763512	307.759853	5.798016
5.612279	312.174649	5.803021
5.538958	311.746348	5.808026
5.808967	302.681483	5.813030
5.744195	308.069890	5.818035
5.711992	296.078206	5.823040
5.186234	294.423235	5.828045
5.416562	301.755657	5.833050
5.630554	312.210032	5.838054
5.629241	306.325797	5.843059
5.838369	307.017761	5.848064
5.371186	315.420553	5.853069
5.582160	318.845665	5.858074
5.872290	315.798180	5.863078
5.342500	313.425675	5.868083
5.534164	314.566440	5.873088
5.569358	322.615775	5.878093
5.831500	316.649390	5.883098
5.745672	314.894283	5.888102
5.588324	317.617454	5.893107
5.678292	316.344332	5.898112
5.434192	317.391595	5.903117
5.321008	314.881460	5.908122
5.656849	325.775607	5.913126
5.758792	329.037367	5.918131
6.376049	336.053300	5.923136
5.778897	347.617899	5.928141
6.455915	334.911499	5.933146
5.960541	326.237868	5.938150
5.861443	328.107263	5.943155
5.730019	316.032940	5.948160
5.742067	330.754960	5.953165
6.369413	328.730628	5.958170
6.010823	335.389142	5.963174
5.664941	326.483431	5.968179
6.222362	331.101103	5.973184
5.925041	332.580589	5.978189
6.374293	331.884267	5.983194
5.953359	321.243881	5.988198
5.689499	319.836027	5.993203
5.770278	330.731925	5.998208
5.732275	337.834062	6.003213
6.117715	337.122366	6.008218
6.165673	345.770827	6.013222
6.097147	342.820308	6.018227
5.865760	348.636459	6.023232
6.027018	340.559764	6.028237
6.225130	334.375555	6.033242
6.213911	338.664156	6.038246
5.807298	340.502339	6.043251
5.967787	339.746574	6.048256
6.110715	337.063684	6.053261
6.397762	337.398674	6.058266
6.201331	341.833169	6.063270
6.086250	342.259243	6.068275
6.193158	334.304906	6.073280
5.572135	344.354643	6.078285
5.932662	338.645011	6.083290
6.286169	346.546722	6.088294
5.989322	346.434792	6.093299
5.812520	343.950377	6.098304
6.151982	339.680345	6.103309
6.110912	341.781149	6.108314
5.788599	348.057538	6.113318
5.906845	352.977708	6.118323
5.867711	340.499864	6.123328
5.945900	348.650082	6.128333
6.432869	341.693245	6.133338
6.093335	340.221243	6.138342
6.129085	343.733752	6.143347
6.180892	339.543308	6.148352
6.293126	340.212395	6.153357
6.124897	334.714801	6.158362
6.221238	338.043872	6.163366
6.300105	340.556265	6.168371
6.194281	324.181643	6.173376
5.570477	319.878099	6.178381
5.926860	320.743285	6.183386
6.370237	334.793886	6.188390
6.192607	341.031927	6.193395
5.865187	328.396500	6.198400
5.845687	339.611732	6.203405
6.112537	325.729028	6.208410
6.254336	339.225484	6.213414
5.964818	329.811131	6.218419
6.463831	329.818894	6.223424
5.912262	323.457188	6.228429
5.917298	309.586787	6.233434
5.866733	322.967651	6.238438
5.788331	332.059716	6.243443
6.360475	338.070289	6.248448
6.146263	342.301913	6.253453
5.684563	329.459605	6.258458
5.984394	338.489619	6.263462
5.916080	338.756553	6.268467
6.480792	337.574026	6.273472
6.120392	339.499925	6.278477
6.366508	334.962859	6.283482
6.136791	325.017186	6.288486
5.878689	318.087780	6.293491
5.972770	320.370015	6.298496
5.629572	325.156382	6.303501
5.783032	335.031747	6.308506
6.447227	343.473532	6.313510
6.305685	347.779262	6.318515
6.274102	334.547284	6.323520
5.954118	331.025324	6.328525
5.897788	316.958831	6.333530
5.908088	324.040788	6.338534
6.364722	330.638809	6.343539
6.188864	324.765926	6.348544
6.268706	324.471963	6.353549
6.365010	315.026020	6.358554
6.186442	325.066968	6.363558
6.032043	323.392138	6.368563
6.052984	319.041993	6.373568
5.686589	318.396736	6.378573
5.470649	316.665051	6.383578
5.620157	322.665494	6.388582
5.809386	327.175978	6.393587
6.310254	333.324196	6.398592
5.728136	337.094253	6.403597
6.183183	341.939835	6.408602
6.162354	341.677364	6.413606
5.678399	337.152729	6.418611
6.539533	341.912938	6.423616
6.304962	341.889388	6.428621
6.362344	331.047976	6.433626
5.942034	326.013569	6.438630
5.851853	332.320248	6.443635
6.126626	329.575704	6.448640
5.864797	331.173049	6.453645
6.064921	335.523654	6.458650
6.182081	335.549742	6.463654
6.137310	336.486879	6.468659
5.995280	315.426132	6.473664
5.634112	330.668161	6.478669
5.934029	333.316976	6.483674
6.324545	340.229011	6.488678
6.014341	334.494099	6.493683
6.177399	332.026371	6.498688
6.255812	332.877891	6.503693
6.261701	328.865439	6.508698
6.003585	313.185243	6.513702
5.513312	318.940453	6.518707
6.097490	321.440605	6.523712
6.154512	341.087840	6.528717
6.252341	336.513751	6.533722
6.187286	328.763358	6.538726
5.791527	328.594064	6.543731
6.236520	316.069333	6.548736
6.087688	324.675659	6.553741
6.186194	319.819899	6.558746
6.055706	317.008743	6.563750
5.674714	323.284769	6.568755
5.908697	312.387398	6.573760
6.127680	339.415632	6.578765
6.208736	336.264657	6.583770
5.863710	331.430495	6.588774
6.058537	335.883164	6.593779
6.124306	342.959655	6.598784
5.982965	331.016578	6.603789
5.878129	340.720194	6.608794
6.092179	340.351552	6.613798
6.068754	342.497064	6.618803
6.447751	338.398044	6.623808
5.847847	331.692690	6.628813
5.963485	322.984039	6.633818
6.213041	329.554191	6.638822
5.931365	329.512665	6.643827
5.872011	322.137868	6.648832
6.237948	328.095124	6.653837
6.086952	330.962838	6.658842
5.789009	331.974193	6.663846
5.768237	334.597010	6.668851
6.446642	338.177135	6.673856
5.931046	344.461470	6.678861
6.102500	344.048842	6.683866
6.504675	335.782781	6.688870
5.931332	325.640677	6.693875
5.911022	315.561168	6.698880
5.637026	327.999240	6.703885
6.122841	332.985559	6.708890
6.215064	329.560769	6.713894
5.923063	341.172764	6.718899
5.926948	346.094919	6.723904
5.906795	338.913325	6.728909
5.983783	346.253821	6.733914
6.268945	342.862262	6.738918
6.296084	341.538810	6.743923
6.023702	341.324997	6.748928
6.003616	344.931620	6.753933
6.423603	338.946979	6.758938
6.111648	323.863604	6.763942
5.624836	334.904824	6.768947
5.896808	329.408296	6.773952
6.282665	342.854100	6.778957
6.108924	340.242661	6.783962
6.051038	342.352410	6.788966
5.468794	339.738135	6.793971
5.754850	345.907148	6.798976
5.713995	354.645371	6.803981
5.841045	343.669719	6.808986
5.831990	348.128825	6.813990
5.994157	338.236024	6.818995
6.150797	346.462611	6.824000
6.090479	341.872015	6.829005
6.303546	331.904854	6.834010
6.097288	336.075127	6.839014
5.843495	344.729442	6.844019
6.183242	348.669176	6.849024
5.904427	348.687315	6.854029
5.808878	352.454383	6.859034
6.038335	353.393116	6.864038
6.438011	355.691050	6.869043
6.197914	343.377368	6.874048
5.839624	358.217182	6.879053
6.075429	352.457362	6.884058
6.372652	348.073685	6.889062
6.323684	354.405592	6.894067
6.290922	345.457447	6.899072
6.153792	343.295880	6.904077
6.189827	344.309020	6.909082
6.181734	348.128908	6.914086
6.505305	338.378653	6.919091
5.827440	322.482233	6.924096
6.015498	332.763490	6.929101
5.897073	331.095713	6.934106
5.960258	337.989110	6.939110
6.258875	350.091275	6.944115
6.440994	343.124955	6.949120
6.022505	331.234520	6.954125
5.870705	326.718282	6.959130
6.154219	324.693701	6.964134
5.790553	331.441587	6.969139
5.930449	326.041552	6.974144
6.248675	338.972709	6.979149
5.885845	331.411045	6.984154
6.009233	330.543999	6.989158
5.964898	336.391133	6.994163
6.043841	335.967598	6.999168
6.016377	349.832095	7.004173
6.170934	349.589773	7.009178
6.369166	341.665506	7.014182
5.865290	327.725634	7.019187
6.070722	322.960791	7.024192
5.976339	333.817526	7.029197
6.280991	326.781515	7.034202
5.888535	327.930970	7.039206
5.926826	328.500839	7.044211
6.112326	329.977917	7.049216
6.256105	346.153724	7.054221
6.327202	335.936587	7.059226
6.298271	326.823343	7.064230
5.881505	328.406846	7.069235
5.975332	324.769838	7.074240
5.758057	324.636029	7.079245
5.901864	310.984462	7.084250
6.022002	316.404191	7.089254
5.893418	333.985948	7.094259
6.018706	334.244884	7.099264
6.146645	337.126117	7.104269
6.206509	335.240759	7.109274
6.317133	324.780196	7.114278
5.849652	326.710111	7.119283
6.328815	320.374583	7.124288
6.271101	323.639053	7.129293
5.755097	324.317370	7.134298
6.127114	324.537892	7.139302
6.109360	318.770106	7.144307
6.467980	322.014046	7.149312
5.817463	314.598419	7.154317
5.783312	316.138167	7.159322
6.032335	324.631930	7.164326
6.097724	326.045451	7.169331
6.005088	319.916008	7.174336
6.040963	318.894912	7.179341
5.892300	313.884652	7.184346
6.048029	319.650012	7.189350
5.869008	323.746440	7.194355
6.208011	323.820244	7.199360
5.962099	327.205764	7.204365
5.829558	327.644046	7.209370
6.013965	331.734511	7.214374
6.323779	339.861317	7.219379
6.243993	330.945811	7.224384
5.822159	327.246723	7.229389
5.798728	319.768259	7.234394
6.104366	329.392140	7.239398
6.063304	336.187874	7.244403
6.186761	334.327416	7.249408
6.327959	331.891565	7.254413
6.054733	322.015943	7.259418
6.183390	322.818511	7.264422
6.000081	322.211185	7.269427
6.192527	313.009698	7.274432
6.033675	312.316309	7.279437
5.984971	318.977187	7.284442
5.937123	310.006099	7.289446
5.829578	321.272992	7.294451
5.776004	320.113967	7.299456
5.986439	321.618798	7.304461
6.315469	336.285142	7.309466
6.302023	329.181600	7.314470
5.862419	325.899724	7.319475
5.910962	316.461216	7.324480
5.775367	320.009890	7.329485
6.023255	326.276585	7.334490
6.386660	341.579813	7.339494
6.242050	332.962296	7.344499
6.035907	327.052999	7.349504
5.924140	314.855396	7.354509
5.870322	320.821057	7.359514
6.147301	314.735306	7.364518
6.313779	319.777668	7.369523
6.248726	319.088657	7.374528
6.073810	320.754725	7.379533
5.890645	327.142317	7.384538
6.119227	322.335906	7.389542
6.047172	314.877670	7.394547
6.105492	309.227754	7.399552
5.900061	318.383882	7.404557
5.712347	310.310915	7.409562
6.042681	311.876170	7.414566
6.158619	329.549563	7.419571
6.025776	317.956342	7.424576
6.137387	323.298309	7.429581
5.948985	316.171393	7.434586
6.041190	315.138363	7.439590
5.977576	319.495228	7.444595
6.112055	324.928545	7.449600
5.932863	313.946810	7.454605
5.975373	325.139724	7.459610
6.326292	323.440000	7.464614
5.853747	325.218846	7.469619
6.194488	319.034582	7.474624
6.130308	318.740897	7.479629
5.882520	323.521900	7.484634
6.183520	309.871169	7.489638
5.579388	326.830947	7.494643
6.164153	326.872814	7.499648
6.486263	348.955961	7.504653
6.517188	336.846855	7.509658
6.248802	319.646512	7.514662
5.799425	330.770484	7.519667
6.049310	319.335968	7.524672
5.969050	325.505061	7.529677
5.910260	320.642155	7.534682
6.081567	313.240939	7.539686
5.767739	322.679697	7.544691
5.886483	313.967402	7.549696
6.036731	322.128535	7.554701
5.663057	334.329036	7.559706
6.116180	334.454673	7.564710
6.332242	334.772241	7.569715
6.593204	329.027495	7.574720
6.446635	326.468773	7.579725
6.220539	322.558880	7.584730
6.045825	314.183336	7.589734
5.721287	324.054025	7.594739
6.014557	314.941240	7.599744
5.626610	322.920418	7.604749
5.862470	327.543863	7.609754
5.921984	317.148209	7.614758
5.646168	320.592167	7.619763
5.989819	334.927209	7.624768
6.264008	327.354947	7.629773
5.772245	342.085817	7.634778
6.546875	335.463839	7.639782
6.265616	339.940015	7.644787
6.079348	315.697144	7.649792
6.259050	325.558926	7.654797
5.924846	309.143947	7.659802
6.100649	316.095730	7.664806
5.688919	321.313538	7.669811
5.933986	318.659041	7.674816
5.950160	321.488071	7.679821
6.009893	342.564877	7.684826
6.338460	333.743975	7.689830
6.221456	337.160046	7.694835
6.141204	321.467968	7.699840
6.012742	312.250007	7.704845
5.918429	316.542049	7.709850
5.854372	318.785631	7.714854
6.039964	333.142117	7.719859
6.317301	320.558066	7.724864
6.076682	320.639860	7.729869
5.832299	317.539558	7.734874
5.986121	313.200361	7.739878
5.872164	334.506677	7.744883
6.333077	333.830685	7.749888
6.487013	327.336987	7.754893
6.095373	317.644317	7.759898
5.928128	315.961997	7.764902
5.858299	323.967574	7.769907
5.817043	311.021853	7.774912
5.722392	313.849155	7.779917
5.761720	330.120303	7.784922
6.466469	341.618235	7.789926
6.249601	341.525491	7.794931
6.371693	323.976450	7.799936
6.372469	323.122168	7.804941
5.628195	320.330647	7.809946
6.108026	310.084687	7.814950
5.785723	318.056806	7.819955
5.940853	319.238060	7.824960
6.185649	334.686296	7.829965
6.147337	332.341669	7.834970
6.099976	319.827155	7.839974
5.704630	321.831258	7.844979
6.378529	329.066156	7.849984
5.982925	335.654504	7.854989
5.828314	318.341536	7.859994
6.270259	328.618063	7.864998
5.587048	333.479517	7.870003
5.873155	331.410240	7.875008
6.033235	341.964773	7.880013
6.105064	350.201403	7.885018
6.529731	330.786115	7.890022
6.299324	345.564879	7.895027
6.086466	326.315295	7.900032
5.944306	321.579262	7.905037
5.806617	318.607879	7.910042
6.135688	316.487622	7.915046
6.103774	329.615655	7.920051
6.220897	336.782222	7.925056
6.065635	329.764035	7.930061
5.765775	324.331231	7.935066
6.279029	318.983797	7.940070
6.022483	327.790390	7.945075
6.125707	315.853536	7.950080
6.273632	325.021089	7.955085
5.817218	320.235910	7.960090
6.197941	314.823692	7.965094
5.836724	322.026766	7.970099
6.052975	310.828442	7.975104
5.877674	318.834620	7.980109
5.935952	323.760955	7.985114
6.240320	324.789262	7.990118
5.951443	331.050690	7.995136
6.469346	336.448267	8.000154
6.325639	319.310365	8.005171
5.972062	316.689481	8.010189
6.175379	314.695062	8.015206
6.234424	317.566995	8.020224
5.956563	317.742831	8.025242
6.181917	316.104723	8.030259
6.245188	323.343388	8.035277
6.354048	316.302048	8.040294
6.366561	323.163629	8.045312
5.972694	319.949448	8.050330
6.323882	318.493708	8.055347
5.989561	319.441997	8.060365
6.134036	313.373358	8.065382
5.745604	323.216321	8.070400
6.010799	314.522336	8.075418
6.152229	320.524447	8.080435
6.011910	324.380421	8.085453
5.865627	321.152937	8.090470
5.772863	323.672987	8.095488
6.077636	323.193252	8.100506
6.176891	318.059406	8.105523
6.286915	320.226008	8.110541
6.177511	315.440214	8.115558
6.025142	320.112215	8.120576
6.330563	318.335416	8.125594
6.339720	315.888416	8.130611
5.885114	316.025503	8.135629
6.194293	323.822295	8.140646
5.941898	338.645758	8.145664
6.500916	344.052714	8.150682
6.647487	332.723303	8.155699
6.254607	325.185754	8.160717
5.903778	323.264991	8.165734
6.017626	316.715152	8.170752
6.131373	337.070225	8.175770
6.437024	339.105390	8.180787
6.321668	341.950835	8.185805
6.385320	326.639308	8.190822
5.956298	326.876547	8.195840
6.254424	334.990628	8.200858
6.546176	340.259324	8.205875
6.617086	336.063954	8.210893
6.354056	314.479417	8.215910
6.173953	322.071537	8.220928
6.061249	314.487214	8.225946
6.450935	315.284910	8.230963
6.344079	319.072560	8.235981
6.229470	321.280448	8.240998
6.389764	316.042431	8.246016
6.121541	322.360775	8.251034
6.431306	310.188661	8.256051
5.931237	323.283523	8.261069
6.250616	332.896373	8.266086
6.438899	345.376020	8.271104
6.826561	339.970059	8.276122
6.373371	331.933840	8.281139
6.447631	318.902189	8.286157
5.922402	323.360861	8.291174
6.485528	323.756033	8.296192
6.490072	320.066433	8.301210
6.408264	318.618152	8.306227
6.161151	320.098787	8.311245
6.492652	312.303300	8.316262
6.093858	325.780005	8.321280
6.261234	333.933376	8.326298
6.828292	342.488400	8.331315
6.150546	339.892739	8.336333
6.509834	339.111042	8.341350
6.432944	344.702209	8.346368
6.227257	339.590591	8.351386
6.721680	345.594552	8.356403
6.535805	336.532154	8.361421
6.244193	324.049743	8.366438
6.269870	330.429622	8.371456
6.309609	336.883049	8.376474
6.742118	341.325144	8.381491
6.407051	345.473362	8.386509
6.376886	341.565112	8.391526
6.468687	335.318484	8.396544
6.552839	342.449770	8.401562
6.540826	340.899107	8.406579
6.333142	338.287061	8.411597
6.431662	341.458947	8.416614
6.783839	343.152373	8.421632
6.398619	342.723265	8.426650
6.608940	334.839345	8.431667
6.479129	342.884365	8.436685
6.664612	338.961474	8.441702
6.453245	336.880148	8.446720
6.308221	338.609962	8.451738
6.823891	339.075636	8.456755
6.014970	337.368198	8.461773
6.683103	347.557882	8.466790
6.945444	350.129939	8.471808
6.757808	345.015509	8.476826
6.101879	327.837436	8.481843
6.004578	335.587073	8.486861
6.402516	343.590949	8.491878
6.466666	350.352987	8.496896
6.485309	355.206643	8.501914
6.867628	359.631313	8.506931
6.441856	358.492189	8.511949
6.576593	346.479839	8.516966
6.597943	344.210808	8.521984
6.915183	351.693950	8.527002
6.762743	350.954058	8.532019
6.781160	352.626870	8.537037
6.895844	353.805038	8.542054
6.866937	355.497841	8.547072
6.643257	352.194044	8.552090
6.574430	337.385946	8.557107
6.517521	341.465609	8.562125
6.468417	348.734404	8.567143
6.691659	347.049287	8.572160
6.576287	349.926292	8.577178
6.662801	349.982284	8.582195
6.479749	357.704259	8.587213
6.986583	359.607123	8.592231
6.776635	350.841940	8.597248
6.393311	342.990487	8.602266
6.437580	350.421460	8.607283
6.686151	347.422812	8.612301
7.003264	353.665810	8.617319
6.826844	352.181767	8.622336
6.578779	351.507254	8.627354
6.887564	344.927054	8.632371
6.868467	344.087511	8.637389
7.036390	343.884688	8.642407
6.864551	341.355419	8.647424
6.573032	351.543050	8.652442
7.096831	341.092124	8.657459
6.693630	337.106263	8.662477
6.867334	344.567571	8.667495
6.902739	333.627832	8.672512
6.495927	333.445070	8.677530
6.823989	338.723890	8.682547
6.669598	344.876204	8.687565
7.219710	346.523034	8.692583
6.641223	332.744138	8.697600
6.465618	325.999535	8.702618
6.742642	336.373177	8.707635
6.699845	344.698124	8.712653
6.629838	344.213628	8.717671
7.083201	345.184437	8.722688
6.963690	358.904845	8.727706
6.939649	351.505507	8.732723
7.071638	357.591148	8.737741
7.165562	349.450803	8.742759
6.775558	338.507872	8.747776
6.541778	332.548610	8.752794
6.950723	330.288657	8.757811
6.745843	340.437548	8.762829
6.815253	346.933693	8.767847
7.046634	343.495933	8.772864
6.894568	352.260752	8.777882
7.034254	343.381178	8.782899
6.995392	335.930508	8.787917
6.804271	337.787414	8.792935
6.961779	333.849945	8.797952
6.841494	349.542736	8.802970
7.100787	343.686571	8.807987
6.678757	344.462335	8.813005
6.668253	339.254060	8.818023
7.090888	344.862121	8.823040
6.722944	350.893061	8.828058
7.128966	342.732528	8.833075
7.029217	342.773341	8.838093
6.821285	348.773055	8.843111
7.325954	348.599848	8.848128
7.028862	345.367440	8.853146
6.926456	338.119156	8.858163
6.522271	344.433432	8.863181
6.721943	352.080037	8.868199
6.476235	350.322776	8.873216
6.489981	351.298920	8.878234
6.741216	345.535522	8.883251
6.852207	355.382790	8.888269
6.690845	353.258964	8.893287
7.102470	365.079036	8.898304
6.920936	376.385586	8.903322
7.444017	370.576699	8.908339
6.752363	369.305412	8.913357
7.009151	375.933331	8.918375
7.267217	360.569416	8.923392
6.970294	373.872513	8.928410
6.987616	370.474388	8.933427
7.127154	367.871389	8.938445
7.332335	377.319017	8.943463
7.451500	370.389654	8.948480
6.756400	361.911429	8.953498
7.165386	355.085263	8.958515
7.163217	354.568114	8.963533
7.182387	366.057992	8.968551
7.214445	354.547591	8.973568
6.858916	359.033495	8.978586
7.059335	362.836426	8.983603
7.304537	367.645344	8.988621
7.406339	366.177939	8.993639
7.309524	358.215603	8.998656
7.022379	356.023003	9.003674
6.712997	347.036630	9.008691
6.882578	366.587824	9.013709
7.118412	364.499979	9.018727
7.448581	360.866964	9.023744
7.279119	378.574422	9.028762
7.387436	378.816358	9.033779
7.254083	378.136606	9.038797
7.227516	374.934652	9.043815
7.435777	373.734678	9.048832
7.445423	377.785053	9.053850
7.092329	363.087462	9.058867
6.989880	354.217182	9.063885
7.285711	370.769805	9.068903
7.484011	365.781462	9.073920
7.138057	363.291921	9.078938
7.440158	370.080032	9.083955
7.370792	356.565814	9.088973
6.992119	352.866449	9.093991
7.226894	350.759837	9.099008
7.289873	377.806494	9.104026
7.355406	362.150679	9.109043
7.138548	360.581418	9.114061
7.115505	368.701340	9.119079
7.436136	366.414110	9.124096
7.216307	378.477666	9.129114
7.335643	373.129250	9.134131
7.728135	367.892933	9.139149
7.496235	369.491117	9.144167
7.637378	364.319180	9.149184
7.371172	351.649767	9.154202
7.172189	341.885701	9.159219
7.414048	352.741328	9.164237
7.177482	359.827886	9.169255
7.215324	355.760730	9.174272
7.388177	378.596443	9.179290
7.433596	374.329298	9.184307
7.231302	371.189416	9.189325
7.198484	383.694048	9.194343
7.229249	363.234451	9.199360
7.512316	369.429110	9.204378
7.230412	378.968354	9.209395
7.512954	363.143058	9.214413
7.444311	373.387514	9.219431
7.469132	362.253756	9.224448
7.325772	368.344403	9.229466
7.701602	365.243892	9.234483
7.694740	367.277228	9.239501
7.149913	372.688809	9.244519
7.243069	369.288344	9.249536
7.282732	367.988395	9.254554
7.351111	367.788448	9.259571
7.608979	355.169973	9.264589
7.266315	369.597284	9.269607
7.223010	367.616013	9.274624
7.168010	365.526116	9.279642
7.154899	374.717410	9.284659
7.259245	374.357237	9.289677
7.404022	386.483945	9.294695
7.791030	387.300994	9.299712
7.709205	397.635875	9.304730
7.709945	392.795043	9.309747
7.725283	373.713695	9.314765
7.525079	376.004341	9.319783
7.483622	364.344442	9.324800
7.554500	375.166747	9.329818
7.300770	369.160088	9.334835
7.420292	379.245870	9.339853
7.367295	387.676561	9.344871
7.621796	388.201834	9.349888
7.739678	394.305461	9.354906
7.773039	398.134410	9.359923
7.956698	406.408349	9.364941
7.791239	393.038446	9.369959
7.650602	377.449430	9.374976
7.584437	372.268744	9.379994
7.260153	375.784163	9.385011
7.581820	385.737494	9.390029
7.676706	391.693230	9.395047
7.959897	384.182931	9.400064
7.874576	391.896016	9.405082
7.891839	381.779538	9.410099
7.778287	370.976572	9.415117
7.323849	369.917646	9.420135
7.415160	373.838547	9.425152
7.561840	386.431992	9.430170
7.740802	396.622132	9.435187
7.850916	394.765286	9.440205
7.947458	395.274129	9.445223
7.830419	391.871675	9.450240
7.971453	390.123618	9.455258
7.605837	390.426721	9.460275
7.708546	377.532602	9.465293
7.864934	392.071568	9.470311
7.594803	378.490767	9.475328
7.942880	385.397951	9.480346
7.529688	382.379261	9.485363
7.746851	385.378057	9.490381
7.712082	398.365816	9.495399
7.843457	399.702326	9.500416
8.027854	398.594423	9.505434
8.023366	400.580059	9.510451
7.674898	388.803852	9.515469
7.998786	391.754476	9.520487
7.647980	378.246193	9.525504
7.638255	380.450380	9.530522
7.397375	396.165145	9.535539
7.985860	394.981705	9.540557
7.977675	409.915520	9.545575
7.843417	398.869620	9.550592
8.185007	397.175539	9.555610
8.050360	399.724211	9.560627
8.008085	394.400951	9.565645
7.968671	403.220835	9.570663
7.790445	402.355575	9.575680
8.042526	397.895309	9.580698
7.963544	410.019003	9.585715
7.977604	389.647179	9.590733
7.790472	394.204698	9.595751
7.723486	390.453641	9.600768
8.109672	390.567111	9.605786
8.151439	399.159769	9.610803
8.118285	396.100840	9.615821
8.179824	398.259223	9.620839
7.727262	389.386635	9.625856
8.019170	376.832268	9.630874
7.715462	379.994208	9.635891
8.027458	386.648248	9.640909
7.721771	394.408266	9.645927
7.802916	398.580051	9.650944
7.988508	396.793500	9.655962
7.773453	399.947952	9.660979
7.960078	397.375485	9.665997
8.211929	403.414078	9.671015
8.114991	399.970624	9.676032
8.420251	405.571735	9.681050
8.000146	395.015289	9.686067
7.834394	395.262029	9.691085
7.592912	399.149548	9.696103
7.723270	395.468744	9.701120
7.769234	392.675194	9.706138
7.645073	406.721395	9.711155
7.974903	405.262662	9.716173
7.910128	413.325989	9.721191
8.402171	417.903994	9.726208
8.497151	403.165007	9.731226
7.829264	408.182370	9.736243
8.065657	402.414953	9.741261
8.104900	405.801197	9.746279
7.821385	406.170409	9.751296
8.166552	416.549266	9.756314
8.184898	422.210832	9.761331
8.182241	419.680455	9.766349
7.929045	421.786863	9.771367
8.408498	427.193611	9.776384
8.470059	419.055118	9.781402
8.425733	428.727803	9.786419
8.009317	410.578286	9.791437
7.899479	417.339039	9.796455
7.854659	426.292313	9.801472
8.472102	425.726025	9.806490
8.212665	436.470415	9.811507
8.443704	422.186731	9.816525
8.370442	432.697015	9.821543
8.098651	427.775535	9.826560
8.378532	430.518433	9.831578
8.553635	432.832699	9.836595
8.566574	418.762847	9.841613
8.276549	415.062290	9.846631
8.046386	412.545246	9.851648
8.233591	416.290288	9.856666
8.268822	426.632205	9.861683
8.691964	426.534805	9.866701
8.365314	419.182554	9.871719
8.226005	409.052571	9.876736
8.385620	404.534121	9.881754
8.144924	415.606923	9.886771
8.486525	420.299865	9.891789
8.192523	430.749847	9.896807
8.096830	439.127253	9.901824
8.394956	425.672524	9.906842
8.397191	423.823005	9.911859
8.562793	423.781481	9.916877
8.393770	426.938237	9.921895
8.125224	426.206953	9.926912
8.377267	416.483069	9.931930
8.430823	428.412580	9.936947
8.480460	422.759436	9.941965
8.499503	428.521876	9.946983
8.511830	432.764342	9.952000
8.597608	422.119648	9.957018
8.171563	424.723159	9.962035
8.417348	423.883395	9.967053
8.561728	421.424794	9.972071
8.386115	428.789054	9.977088
8.865327	424.640539	9.982106
8.555203	424.395387	9.987123
8.423331	418.615879	9.992141
8.719108	421.397324	9.997159
8.160645	430.149720	10.002176
8.876778	415.913583	10.007194
8.517756	428.020934	10.012211
8.517688	434.196585	10.017229
8.612010	425.046337	10.022247
8.542263	425.962905	10.027264
8.321606	422.163187	10.032282
8.378652	426.471268	10.037299
8.479702	424.158262	10.042317
8.583978	424.580699	10.047335
8.238582	425.028970	10.052352
8.519786	423.416868	10.057370
8.212530	427.690157	10.062387
8.203461	421.534939	10.067405
8.527191	426.511519	10.072423
8.742788	431.362931	10.077440
8.655739	429.072899	10.082458
8.809831	436.669836	10.087475
8.376922	431.211736	10.092493
8.700774	424.837433	10.097511
8.517021	426.907785	10.102528
8.802442	429.252209	10.107546
8.652925	428.855825	10.112563
8.772043	432.062388	10.117581
8.866587	437.421776	10.122599
8.413033	434.803817	10.127616
8.394505	428.555401	10.132634
8.481156	447.990214	10.137651
8.592338	454.893286	10.142669
8.513670	462.330823	10.147687
8.868564	460.306478	10.152704
9.133862	455.689513	10.157722
8.946489	456.024822	10.162739
8.924962	454.920578	10.167757
9.065123	441.888043	10.172775
8.856561	436.325586	10.177792
9.008262	435.033434	10.182810
8.818266	438.054609	10.187827
8.586057	426.383346	10.192845
9.121088	431.503744	10.197863
8.781572	427.665730	10.202880
8.790990	423.413644	10.207898
8.735617	426.129849	10.212915
8.574597	425.028391	10.217933
9.001928	424.456991	10.222951
8.399855	438.186325	10.227968
8.876340	441.412985	10.232986
8.922826	457.657390	10.238003
8.970055	461.307476	10.243021
8.669903	456.712281	10.248039
8.813777	461.887279	10.253056
9.191536	448.953439	10.258074
8.989477	448.757730	10.263091
8.807773	454.844910	10.268109
8.905716	445.930761	10.273127
8.917778	461.596733	10.278144
9.089415	456.748210	10.283162
9.075866	453.784044	10.288179
9.281685	459.608928	10.293197
9.319621	439.548895	10.298215
8.827570	435.311771	10.303232
8.794075	424.603599	10.308250
8.872285	429.949749	10.313267
8.861007	444.019427	10.318285
9.214043	443.361769	10.323303
9.255826	449.145920	10.328320
9.164416	432.933838	10.333338
8.885093	435.385126	10.338355
8.692004	432.628789	10.343373
9.301108	429.734932	10.348391
8.954289	440.716980	10.353408
9.177668	439.404200	10.358426
9.230472	444.293585	10.363443
9.114626	441.493664	10.368461
9.117439	430.158173	10.373479
8.596821	434.994832	10.378496
8.857692	443.928920	10.383514
9.010646	450.598279	10.388531
8.697951	455.068071	10.393549
9.161399	442.928741	10.398567
9.081382	450.073008	10.403584
9.042493	447.803876	10.408602
9.115693	455.050516	10.413619
9.029348	456.906898	10.418637
9.098562	446.706560	10.423655
8.846757	459.914339	10.428672
9.062965	446.241986	10.433690
8.838048	455.447366	10.438707
9.186875	460.218086	10.443725
9.338897	447.603402	10.448743
9.042099	456.592768	10.453760
9.125583	450.748163	10.458778
9.124187	471.329589	10.463795
9.202401	475.385090	10.468813
9.584604	466.593922	10.473831
9.093146	478.472629	10.478848
9.357902	465.540593	10.483866
9.313204	468.267764	10.488883
9.378812	472.754396	10.493901
9.590183	456.368925	10.498919
9.224615	455.075261	10.503936
8.950916	452.899489	10.508954
8.979448	464.678293	10.513971
9.089633	479.129855	10.518989
9.374805	473.641986	10.524007
9.536634	480.720210	10.529024
9.531947	475.839176	10.534042
9.425300	476.430148	10.539059
9.253733	480.401469	10.544077
9.567939	477.941664	10.549095
9.231698	486.990832	10.554112
9.461643	477.888865	10.559130
9.828704	472.467138	10.564147
9.451229	468.073318	10.569165
9.371576	453.339389	10.574183
9.491235	468.496334	10.579200
9.353625	466.075321	10.584218
9.462181	468.403108	10.589235
9.191868	484.021551	10.594253
9.422715	482.085941	10.599271
9.337490	483.838015	10.604288
9.357550	470.906206	10.609306
9.438301	478.858546	10.614323
9.491942	481.005546	10.619341
9.477301	476.807684	10.624359
9.144887	485.042097	10.629376
9.414620	480.525416	10.634394
9.320199	479.735462	10.639411
9.249221	476.278484	10.644429
9.599879	470.979226	10.649447
9.469550	482.833267	10.654464
9.324227	483.234610	10.659482
9.381564	487.817202	10.664499
9.303468	480.009680	10.669517
9.706604	484.254423	10.674535
9.832958	496.488210	10.679552
9.722614	493.150962	10.684570
9.562649	482.462447	10.689587
9.631399	475.752321	10.694605
9.615225	464.795287	10.699623
9.347038	464.411068	10.704640
9.688709	487.981150	10.709658
10.150226	492.740644	10.714675
9.770467	483.938721	10.719693
9.753549	472.120304	10.724711
9.894469	478.292954	10.729728
9.762565	473.643157	10.734746
9.565111	469.574742	10.739763
9.570983	472.628540	10.744781
9.792638	470.706985	10.749799
9.651142	471.357028	10.754816
9.643665	477.398155	10.759834
9.725751	478.837015	10.764851
9.463443	482.074573	10.769869
9.960888	477.566619	10.774887
9.894141	471.199468	10.779904
9.791323	481.436685	10.784922
9.707554	483.052839	10.789939
9.951753	483.466115	10.794957
9.679450	468.456070	10.799975
9.510197	481.897153	10.804992
9.589981	491.143469	10.810010
9.626500	502.116361	10.815027
9.646563	507.547324	10.820045
9.819161	503.127808	10.825063
9.932925	505.293851	10.830080
9.825966	500.955730	10.835098
9.984347	499.763514	10.840115
9.787019	509.112942	10.845133
9.881387	500.300304	10.850151
9.870592	509.346147	10.855168
10.139796	510.162611	10.860186
10.129230	502.514970	10.865203
9.848992	507.434137	10.870221
10.031624	504.947479	10.875239
10.317426	514.010259	10.880256
10.109300	508.002764	10.885274
10.052451	496.152680	10.890291
9.940503	490.682456	10.895309
9.993601	493.915089	10.900327
9.942139	496.712742	10.905344
9.864064	505.526073	10.910362
9.948560	492.530569	10.915379
10.088402	505.986659	10.920397
10.189833	505.478621	10.925415
9.908285	500.413480	10.930432
9.949103	503.001116	10.935450
10.296593	499.340130	10.940467
10.121324	506.442448	10.945485
9.945556	498.520743	10.950503
10.189762	506.397156	10.955520
10.222725	497.136509	10.960538
10.331704	497.981074	10.965555
9.906912	488.245774	10.970573
10.188122	488.334566	10.975591
10.558278	487.835179	10.980608
9.648146	483.874566	10.985626
9.915326	481.049716	10.990643
10.044233	495.653003	10.995661
10.147668	501.604290	11.000679
10.129088	505.283565	11.005696
10.095790	504.862773	11.010714
10.040243	500.876393	11.015731
9.733672	497.153149	11.020749
9.925291	496.132475	11.025767
10.242367	502.246150	11.030784
9.898834	501.311953	11.035802
9.894514	496.979942	11.040819
10.021383	499.639382	11.045837
10.420436	507.352837	11.050855
10.133520	510.032524	11.055872
10.213588	527.256330	11.060890
10.639933	513.712147	11.065907
10.654441	513.804595	11.070925
10.522080	510.070003	11.075943
10.651902	504.688359	11.080960
10.241999	509.391040	11.085978
10.976970	498.509530	11.090995
10.501422	498.854995	11.096013
10.614146	498.190572	11.101031
10.394403	488.499082	11.106048
10.407419	494.994595	11.111066
10.141501	491.993980	11.116083
10.198359	496.251616	11.121101
10.169984	491.538361	11.126119
10.019480	495.465382	11.131136
10.213154	497.596893	11.136154
10.450265	489.330054	11.141171
9.964082	494.713607	11.146189
10.035582	499.808370	11.151207
10.302331	500.622060	11.156224
10.364582	516.952423	11.161242
10.608054	511.559393	11.166259
10.351576	526.632945	11.171277
10.439455	519.904047	11.176295
10.838264	518.920537	11.181312
10.550333	521.707677	11.186330
10.810638	514.049415	11.191347
10.332380	509.134813	11.196365
10.592019	519.470246	11.201383
10.846258	518.603915	11.206400
10.188515	503.956796	11.211418
10.570749	512.625882	11.216435
10.605119	518.496413	11.221453
10.851631	520.480850	11.226471
10.750286	512.175183	11.231488
10.268885	501.584037	11.236506
10.730152	512.613875	11.241523
10.659685	508.986405	11.246541
10.776765	516.699588	11.251559
10.609952	509.237210	11.256576
10.377899	518.399555	11.261594
10.620410	516.850272	11.266611
10.654661	513.559931	11.271629
10.249520	527.536371	11.276647
10.703922	519.611211	11.281664
10.364694	519.679843	11.286682
10.483406	514.088497	11.291699
10.900234	522.140002	11.296717
10.682976	524.780445	11.301735
10.724632	520.138327	11.306752
10.567416	522.106731	11.311770
10.888131	513.041105	11.316787
10.614384	522.919967	11.321805
10.615382	531.449612	11.326823
10.337103	521.126618	11.331840
10.600966	528.782239	11.336858
10.928194	521.217691	11.341875
10.710838	524.694400	11.346893
10.666933	536.516087	11.351911
11.017477	541.703109	11.356928
10.643813	546.557941	11.361946
11.151825	542.922444	11.366963
10.920704	536.760736	11.371981
10.829293	529.094115	11.376999
11.051269	527.601675	11.382016
10.474031	536.293932	11.387034
10.901299	540.557021	11.392051
11.259093	542.139143	11.397069
11.353586	545.895492	11.402087
10.847054	533.014069	11.407104
10.859106	529.474729	11.412122
10.520593	527.899149	11.417139
10.798741	539.026938	11.422157
10.933911	544.310608	11.427175
11.295965	551.900461	11.432192
11.384289	556.885328	11.437210
11.429029	534.539423	11.442227
11.377955	529.296385	11.447245
10.989663	528.798326	11.452263
11.032998	518.661933	11.457280
10.720084	526.767102	11.462298
10.691459	524.477428	11.467315
10.842052	527.966274	11.472333
11.087443	543.943114	11.477351
11.486129	546.841094	11.482368
10.869400	542.658069	11.487386
10.704988	523.131198	11.492403
10.882094	542.378469	11.497421
10.919288	546.446684	11.502439
11.555537	555.925116	11.507456
11.196999	545.264324	11.512474
10.971729	544.276999	11.517491
11.140845	547.248591	11.522509
10.873881	546.337182	11.527527
11.177885	546.343534	11.532544
11.320172	547.006198	11.537562
11.614422	549.431311	11.542579
11.599773	537.558851	11.547597
11.411940	552.697474	11.552615
11.297930	536.397302	11.557632
11.123477	537.377513	11.562650
11.062303	538.235950	11.567667
11.299393	542.617008	11.572685
11.529417	555.576277	11.577703
11.238017	549.490219	11.582720
11.533030	547.825466	11.587738
11.054625	538.502410	11.592755
11.404540	537.472866	11.597773
11.337309	546.600096	11.602791
11.385604	538.078623	11.607808
11.042520	551.411130	11.612826
11.130807	549.847988	11.617843
11.219326	549.742729	11.622861
11.279208	550.945220	11.627879
11.073340	541.485060	11.632896
11.351264	543.878002	11.637914
11.357615	544.905799	11.642931
11.136251	539.736606	11.647949
11.371945	546.055462	11.652967
11.647341	552.008393	11.657984
11.474596	554.487282	11.663002
11.439376	540.393275	11.668019
11.612388	540.915462	11.673037
11.076871	547.764630	11.678055
10.963838	547.454077	11.683072
11.422409	552.343429	11.688090
11.621228	562.132958	11.693107
11.614963	562.118193	11.698125
11.741343	561.057182	11.703143
11.469055	549.644532	11.708160
11.291585	547.687285	11.713178
11.668719	568.269846	11.718195
11.547501	568.948292	11.723213
11.623199	579.318710	11.728231
11.928095	573.698356	11.733248
11.572197	570.572888	11.738266
11.502494	563.922154	11.743283
11.898340	562.674027	11.748301
11.575232	557.413378	11.753319
11.286272	553.498040	11.758336
11.764325	567.273886	11.763354
11.799843	568.499106	11.768371
11.940185	571.345800	11.773389
11.667993	564.865442	11.778407
11.540875	547.011556	11.783424
11.436401	559.275014	11.788442
11.785545	568.974872	11.793459
12.058647	567.341930	11.798477
11.520146	577.807976	11.803495
12.168199	570.733075	11.808512
11.834924	555.685115	11.813530
11.614983	559.203257	11.818547
11.683517	556.131624	11.823565
11.831909	570.006134	11.828583
11.984487	572.519577	11.833600
11.777547	576.950844	11.838618
11.526528	578.968572	11.843635
11.688458	575.592072	11.848653
11.840054	579.427897	11.853671
11.673397	576.566441	11.858688
11.782789	581.497544	11.863706
11.926238	575.993841	11.868723
11.693781	576.345639	11.873741
11.676667	579.444057	11.878759
11.921956	580.459900	11.883776
12.029891	578.265717	11.888794
11.944510	578.619861	11.893811
12.135077	569.665984	11.898829
11.878459	576.471740	11.903847
11.640633	569.405386	11.908864
11.584585	564.923628	11.913882
11.554530	582.795768	11.918899
11.924191	586.067489	11.923917
12.162766	589.618385	11.928935
12.329424	591.956076	11.933952
12.135870	579.653869	11.938970
11.643570	586.796113	11.943987
12.127460	586.550404	11.949005
12.234936	597.237764	11.954023
11.976497	606.189675	11.959040
12.381308	609.017287	11.964058
12.135846	601.201058	11.969075
12.357243	582.497642	11.974093
11.763650	587.790654	11.979111
11.815708	593.106212	11.984128
12.149785	591.498487	11.989146
11.829515	608.118855	11.994163
12.201494	597.142329	11.999181
11.911001	600.564171	12.004199
12.284328	603.769054	12.009216
12.336678	602.517604	12.014234
12.231165	601.265487	12.019251
12.501299	599.374238	12.024269
12.254657	606.307835	12.029287
12.493424	609.473712	12.034304
12.514071	603.484212	12.039322
12.027340	610.808628	12.044339
12.443698	605.281359	12.049357
11.987234	610.388931	12.054375
12.006022	612.389900	12.059392
12.285580	611.731054	12.064410
12.133487	606.229177	12.069427
12.245292	608.685860	12.074445
12.238036	610.438430	12.079463
12.070054	604.885381	12.084480
12.147600	596.179452	12.089498
12.417439	603.423937	12.094515
12.656960	604.014662	12.099533
12.228741	604.538946	12.104551
12.266237	608.004393	12.109568
12.592669	604.173102	12.114586
12.245411	615.593966	12.119603
12.511526	600.380063	12.124621
12.501232	607.781771	12.129639
12.456452	608.533521	12.134656
12.380280	609.908672	12.139674
12.533559	617.000904	12.144691
12.829722	618.807215	12.149709
12.217868	610.420047	12.154727
12.513277	616.937906	12.159744
12.720290	620.168687	12.164762
12.561840	623.106089	12.169779
12.851315	617.355585	12.174797
12.487693	612.584046	12.179815
12.467942	606.856444	12.184832
12.634318	612.321460	12.189850
12.587810	611.404125	12.194867
12.742848	622.241878	12.199885
12.727820	618.391168	12.204903
12.454025	613.621422	12.209920
12.881427	619.758983	12.214938
12.720070	620.607777	12.219955
12.670537	603.309777	12.224973
12.575516	613.757286	12.229991
12.664174	628.755098	12.235008
12.932994	616.462924	12.240026
12.658490	629.346171	12.245043
12.784794	623.526399	12.250061
13.049851	626.877527	12.255079
12.892240	614.680149	12.260096
12.798531	600.926548	12.265114
12.600452	605.151323	12.270131
12.596183	615.243889	12.275149
12.858855	625.074002	12.280167
12.826662	622.440902	12.285184
13.139310	621.827394	12.290202
12.984701	623.918476	12.295219
13.182810	606.506179	12.300237
12.718778	607.092841	12.305255
12.559766	607.950736	12.310272
12.768382	609.256301	12.315290
12.794753	625.784846	12.320307
12.912496	624.270758	12.325325
12.997252	633.402770	12.330343
12.689847	624.715738	12.335360
12.928073	629.178689	12.340378
12.946113	630.753759	12.345395
13.174984	619.108407	12.350413
13.227757	628.333754	12.355431
13.351149	628.125240	12.360448
13.062290	627.633786	12.365466
12.796379	625.251661	12.370483
13.189771	622.722705	12.375501
13.022046	623.275856	12.380519
12.847527	634.426849	12.385536
13.272673	620.939573	12.390554
13.069226	628.636440	12.395571
13.000189	627.489091	12.400589
13.176689	631.292648	12.405607
12.952896	638.453064	12.410624
13.324597	618.852084	12.415642
13.530686	627.349843	12.420659
13.566481	632.295575	12.425677
13.360647	629.812580	12.430695
13.037256	612.295289	12.435712
13.162486	623.150306	12.440730
13.054284	628.127923	12.445747
12.929984	627.920105	12.450765
13.335965	630.334144	12.455783
13.301396	631.813269	12.460800
12.996551	626.978928	12.465818
12.869935	633.537255	12.470835
12.963530	631.187515	12.475853
13.164333	629.108250	12.480871
12.513138	628.477558	12.485888
13.021192	627.120442	12.490906
13.213406	651.405105	12.495923
13.278316	648.958846	12.500941
13.445063	654.752010	12.505959
13.585169	664.907329	12.510976
13.825327	646.497560	12.515994
13.509228	643.447930	12.521011
13.180583	636.436713	12.526029
13.439884	644.039448	12.531047
13.354424	650.531416	12.536064
13.594073	654.498709	12.541082
13.844222	651.354603	12.546099
13.452657	646.925064	12.551117
13.214269	637.132257	12.556135
13.212207	650.500101	12.561152
13.366974	641.375043	12.566170
13.613612	659.775359	12.571187
13.433234	658.717925	12.576205
13.793543	661.262151	12.581223
13.725853	664.469441	12.586240
13.964733	652.674191	12.591258
13.374030	644.700264	12.596275
13.447488	657.630337	12.601293
13.946132	659.502954	12.606311
13.548172	664.658234	12.611328
14.033419	650.388435	12.616346
13.709729	644.361018	12.621363
13.678157	634.933629	12.626381
13.405902	632.634539	12.631399
13.554096	643.703735	12.636416
13.766856	639.287400	12.641434
13.701892	657.550044	12.646451
14.140713	659.441441	12.651469
13.918697	638.692693	12.656487
13.400010	638.571525	12.661504
13.680128	632.951855	12.666522
13.666763	646.495018	12.671539
13.636585	654.786589	12.676557
13.705452	650.197002	12.681575
13.327693	663.443476	12.686592
13.657845	648.115425	12.691610
13.652659	655.128207	12.696627
13.825240	658.010919	12.701645
14.051097	666.281566	12.706663
13.814142	665.371790	12.711680
14.019531	657.538986	12.716698
13.505324	650.379937	12.721715
13.574507	658.188997	12.726733
13.733517	666.425871	12.731751
13.791123	672.393818	12.736768
13.914230	678.310543	12.741786
14.327166	673.440170	12.746803
13.430695	673.311552	12.751821
14.288080	669.485940	12.756839
14.017688	677.130136	12.761856
14.407828	675.983873	12.766874
14.557218	666.717633	12.771891
14.120502	672.267100	12.776909
14.332203	657.153137	12.781927
14.022208	661.758254	12.786944
14.103136	657.400308	12.791962
13.908058	662.243144	12.796979
13.831631	657.502614	12.801997
14.096909	649.947657	12.807015
13.906975	665.010966	12.812032
13.906321	660.823506	12.817050
14.183642	668.701146	12.822067
14.318921	682.959626	12.827085
14.146231	677.631341	12.832103
14.167675	678.593682	12.837120
14.040686	675.003380	12.842138
14.280211	672.599356	12.847155
13.928590	688.681901	12.852173
14.040062	678.989229	12.857191
13.725127	675.746915	12.862208
13.958387	678.181541	12.867226
13.956537	681.299691	12.872243
14.177572	685.326691	12.877261
14.172266	682.752509	12.882279
14.163594	691.397342	12.887296
14.439656	697.949800	12.892314
14.431869	692.860914	12.897331
14.346300	701.918497	12.902349
14.444746	694.780803	12.907367
14.185971	697.989449	12.912384
14.359549	704.860813	12.917402
14.590737	696.276075	12.922419
14.526439	703.165541	12.927437
14.717433	697.635463	12.932455
14.509002	701.413764	12.937472
14.418925	690.862559	12.942490
14.773534	692.419945	12.947507
14.636564	687.641498	12.952525
14.534165	679.944966	12.957543
14.331635	689.222718	12.962560
14.684331	691.616660	12.967578
14.307167	691.706978	12.972595
14.490558	697.964607	12.977613
14.473970	697.661125	12.982631
14.796508	703.546808	12.987648
14.727598	700.007417	12.992666
14.708673	703.096672	12.997683
14.505187	703.604902	13.002701
14.899948	698.131459	13.007719
14.646454	703.381019	13.012736
14.701790	701.501113	13.017754
14.721770	697.487151	13.022771
14.602796	706.278548	13.027789
14.669363	694.753087	13.032807
14.888585	699.203235	13.037824
14.579178	701.138553	13.042842
14.592951	695.866435	13.047859
14.595008	706.977358	13.052877
14.532033	702.250500	13.057895
14.296620	704.663430	13.062912
14.833987	704.715497	13.067930
14.945239	699.096853	13.072947
14.561641	711.624773	13.077965
14.458030	698.235543	13.082983
14.661916	717.977435	13.088000
14.604228	718.696487	13.093018
15.475092	718.472575	13.098035
15.212342	722.152043	13.103053
15.075573	720.816425	13.108071
14.981495	711.430284	13.113088
15.068425	711.303182	13.118106
15.376024	709.898378	13.123123
14.949272	706.837563	13.128141
15.022969	699.637451	13.133159
15.069864	703.745215	13.138176
14.768049	705.660416	13.143194
14.771459	702.744060	13.148211
14.778840	723.501130	13.153229
15.143016	724.725681	13.158247
15.226693	725.763539	13.163264
14.960612	731.620961	13.168282
15.180591	728.150191	13.173299
15.166700	731.636285	13.178317
15.215867	725.004852	13.183335
15.333480	725.889108	13.188352
15.046056	725.085013	13.193370
15.066376	719.322736	13.198387
14.784691	725.412951	13.203405
15.253176	718.397509	13.208423
15.296028	723.540976	13.213440
14.922242	726.698108	13.218458
15.198323	727.021223	13.223475
15.235930	732.613619	13.228493
15.373896	721.203253	13.233511
15.316193	729.003698	13.238528
15.206880	731.075117	13.243546
15.516848	728.350860	13.248563
14.926628	727.947348	13.253581
15.162531	720.185502	13.258599
15.075341	728.426025	13.263616
14.820557	732.410359	13.268634
15.128640	743.281159	13.273651
14.963348	743.237507	13.278669
15.481175	752.040228	13.283687
15.414679	754.565716	13.288704
15.342047	756.975399	13.293722
15.579822	754.656841	13.298739
15.579562	752.031372	13.303757
15.613299	742.293966	13.308775
15.633261	747.715550	13.313792
15.412493	748.179137	13.318810
15.674713	745.036291	13.323827
15.934275	758.745322	13.328845
15.797946	744.565914	13.333863
15.950340	735.062493	13.338880
15.861067	743.410641	13.343898
16.150099	740.049034	13.348915
15.552981	744.039334	13.353933
15.814450	724.452245	13.358951
15.594523	717.894269	13.363968
15.544184	716.945967	13.368986
15.673629	731.337933	13.374003
15.903272	747.847566	13.379021
15.698980	733.517807	13.384039
15.917296	731.236994	13.389056
15.452619	721.779165	13.394074
16.051870	743.119426	13.399091
15.992628	741.178463	13.404109
15.984768	736.023307	13.409127
15.753452	724.042450	13.414144
15.578853	720.822457	13.419162
16.046769	723.706533	13.424179
15.643533	727.657176	13.429197
16.009952	733.797961	13.434215
16.071233	730.067885	13.439232
15.976548	726.381028	13.444250
16.005765	719.487624	13.449267
15.516796	724.647625	13.454285
16.101546	730.344174	13.459303
16.133187	730.992516	13.464320
15.954074	727.400852	13.469338
15.769760	730.364388	13.474355
15.781472	737.974155	13.479373
16.020454	740.291139	13.484391
15.985443	728.768849	13.489408
15.816348	740.815283	13.494426
16.011747	746.345247	13.499443
16.058985	751.475417	13.504461
16.132294	746.547453	13.509479
16.367553	739.650363	13.514496
16.155538	745.890679	13.519514
16.344049	741.913581	13.524531
15.851839	747.358106	13.529549
16.214095	732.987474	13.534567
16.385802	734.418712	13.539584
16.220584	740.847394	13.544602
16.192672	742.467497	13.549619
16.414031	736.882189	13.554637
16.216478	736.843559	13.559655
16.174794	733.110580	13.564672
15.839819	738.325501	13.569690
16.217864	732.109904	13.574707
16.169777	734.348510	13.579725
15.513655	732.443678	13.584743
16.196413	744.423753	13.589760
16.221061	751.583402	13.594778
16.075139	747.617349	13.599795
16.216901	766.213979	13.604813
16.396713	757.845488	13.609831
16.530412	760.525994	13.614848
16.154561	769.303769	13.619866
16.537455	758.517943	13.624883
16.762019	762.118391	13.629901
16.736605	760.453017	13.634919
16.600670	764.709178	13.639936
16.099584	768.252200	13.644954
16.521654	762.427357	13.649971
16.366776	755.010354	13.654989
16.500015	760.960243	13.660007
16.529777	758.746652	13.665024
16.572467	764.641215	13.670042
16.761415	753.169243	13.675059
16.481706	757.649753	13.680077
16.437099	757.842923	13.685095
16.358542	755.437921	13.690112
16.370833	763.170681	13.695130
16.545060	750.804782	13.700147
16.579576	759.802674	13.705165
16.842053	771.529478	13.710183
16.770000	780.256803	13.715200
16.874243	782.676819	13.720218
16.924044	770.718431	13.725235
16.592056	758.418720	13.730253
16.775400	775.244847	13.735271
16.711784	780.341793	13.740288
16.410771	784.920297	13.745306
16.909186	777.439438	13.750323
17.073823	777.205565	13.755341
16.765025	784.107884	13.760359
16.817215	777.627435	13.765376
16.854442	785.261651	13.770394
16.734150	783.014617	13.775411
17.021635	784.673979	13.780429
16.988365	778.639167	13.785447
17.049469	784.022800	13.790464
16.870737	780.307993	13.795482
16.694963	784.775483	13.800499
16.762608	786.689972	13.805517
16.887242	783.360264	13.810535
17.171320	774.530576	13.815552
16.383222	790.690638	13.820570
16.928908	779.885765	13.825587
17.044410	790.120724	13.830605
17.175802	807.456727	13.835623
17.490308	798.013237	13.840640
17.120220	797.824751	13.845658
17.255985	786.121204	13.850675
17.086913	783.591440	13.855693
16.970406	790.009400	13.860711
17.543548	798.636279	13.865728
17.260287	790.567083	13.870746
17.484267	781.450112	13.875763
17.084600	780.392099	13.880781
16.910471	777.083663	13.885799
17.698608	791.726561	13.890816
17.503446	791.390922	13.895834
17.762484	786.071123	13.900851
17.361611	783.792038	13.905869
17.271011	778.984257	13.910887
17.838871	770.618456	13.915904
17.514816	778.340477	13.920922
17.178812	778.986103	13.925939
17.135999	775.802384	13.930957
17.150176	777.841959	13.935975
17.385084	775.921464	13.940992
17.243139	803.092189	13.946010
17.972998	805.051894	13.951027
17.585532	793.903165	13.956045
17.438527	785.478251	13.961063
17.642576	779.693659	13.966080
17.515254	775.270281	13.971098
17.464306	776.821393	13.976115
17.753581	785.369391	13.981133
17.847377	787.320833	13.986151
17.538972	777.627210	13.991168
17.740193	779.634507	13.996186
17.836639	783.122367	14.001203
17.827755	777.023801	14.006221
17.425897	777.569230	14.011239
17.529320	776.287726	14.016256
17.595035	795.521057	14.021274
17.545603	800.663137	14.026291
17.936607	801.006228	14.031309
17.886295	801.711512	14.036327
17.814764	792.517472	14.041344
17.946449	797.732334	14.046362
17.672021	801.902773	14.051379
18.544070	799.763157	14.056397
17.894165	788.399680	14.061415
18.032456	776.771483	14.066432
17.684921	778.472911	14.071450
17.468585	781.816972	14.076467
17.576339	784.264842	14.081485
17.982363	799.857151	14.086503
18.116994	797.258010	14.091520
18.188162	806.013540	14.096538
17.955979	795.976690	14.101555
18.006601	791.774904	14.106573
17.770000	797.624602	14.111591
18.078015	797.961680	14.116608
17.870056	801.212924	14.121626
17.898808	796.960895	14.126643
18.018715	802.445828	14.131661
17.921956	804.401695	14.136679
18.117766	798.217604	14.141696
17.849848	807.953709	14.146714
17.989012	809.746616	14.151731
18.137009	806.050359	14.156749
17.994149	805.785470	14.161767
18.031480	801.677267	14.166784
17.974777	814.738170	14.171802
18.148574	823.742810	14.176819
18.534799	815.916494	14.181837
18.348428	823.844309	14.186855
18.357682	831.028477	14.191872
18.204126	833.356098	14.196890
18.441134	836.209873	14.201907
18.615884	821.092057	14.206925
18.212792	834.784403	14.211943
18.330441	820.432850	14.216960
18.462597	821.501034	14.221978
18.604735	817.988719	14.226995
18.450892	819.820935	14.232013
18.201928	826.467808	14.237031
18.507824	825.489282	14.242048
18.735946	822.190790	14.247066
18.456420	826.728091	14.252083
18.666403	819.544579	14.257101
18.768717	818.774471	14.262119
18.860013	820.600077	14.267136
18.738932	811.596774	14.272154
18.201527	799.751883	14.277171
18.686633	807.575144	14.282189
18.908357	828.608225	14.287207
18.689402	817.748816	14.292224
18.691069	812.977151	14.297242
18.311708	825.135273	14.302259
18.963764	828.899543	14.307277
18.794860	823.895663	14.312295
19.004432	820.098301	14.317312
18.754166	811.616870	14.322330
18.478996	810.861355	14.327347
18.684324	815.124353	14.332365
18.429697	824.126271	14.337383
18.390036	819.550383	14.342400
18.995076	824.420161	14.347418
18.173237	827.511376	14.352435
18.767991	827.100085	14.357453
18.589738	828.831964	14.362471
18.539146	835.438488	14.367488
18.534347	841.463543	14.372506
18.649336	845.462910	14.377523
18.892116	849.379267	14.382541
18.904515	860.100522	14.387559
18.881961	848.014496	14.392576
19.050838	844.002564	14.397594
18.767182	851.459557	14.402611
19.003050	846.982770	14.407629
18.939731	858.533145	14.412647
18.895713	851.351298	14.417664
18.996728	853.178551	14.422682
19.108734	862.505247	14.427699
19.295421	848.508987	14.432717
18.928309	861.160674	14.437735
19.367262	872.213145	14.442752
19.724820	876.222088	14.447770
19.033661	866.606944	14.452787
19.082877	845.566423	14.457805
18.855853	855.971512	14.462823
19.033729	868.355319	14.467840
19.451357	874.204164	14.472858
19.454990	874.045850	14.477875
19.836582	875.277168	14.482893
19.405557	874.760505	14.487911
19.320571	873.034970	14.492928
19.461649	871.428867	14.497946
19.612398	876.757546	14.502963
19.352123	859.239651	14.507981
19.421528	860.200846	14.512999
19.311074	863.907123	14.518016
19.416905	861.230407	14.523034
19.838427	872.967229	14.528051
19.637897	863.708032	14.533069
19.667643	861.311399	14.538087
19.331869	848.245375	14.543104
19.693897	847.160281	14.548122
19.403601	868.961076	14.553139
19.786224	866.635730	14.558157
19.977635	869.468209	14.563175
19.503780	862.965493	14.568192
20.025248	860.451276	14.573210
19.730526	853.292684	14.578227
19.648065	840.963533	14.583245
19.422283	850.162940	14.588263
19.520392	862.290926	14.593280
19.484644	860.570348	14.598298
19.531877	860.585122	14.603315
19.787055	858.932855	14.608333
20.125785	868.984784	14.613351
20.189856	867.794605	14.618368
19.913989	863.943430	14.623386
20.111651	870.722748	14.628403
20.382827	861.431134	14.633421
19.908972	854.925265	14.638439
19.480809	858.510598	14.643456
20.074263	861.349905	14.648474
19.758291	871.696270	14.653491
20.089471	877.192511	14.658509
20.278276	872.849275	14.663527
20.327673	872.380885	14.668544
20.261468	865.350807	14.673562
19.888842	853.565429	14.678579
19.979259	858.859316	14.683597
19.886390	861.149090	14.688615
19.661221	866.987564	14.693632
19.786554	862.051469	14.698650
19.886556	870.177707	14.703667
19.733563	859.841321	14.708685
19.857383	872.243014	14.713703
19.864709	877.303697	14.718720
20.642980	884.787865	14.723738
20.470008	890.479367	14.728755
20.408008	872.902187	14.733773
20.253083	873.264008	14.738791
20.026871	870.506449	14.743808
20.343170	878.636884	14.748826
20.302437	893.935925	14.753843
20.258346	885.403424	14.758861
20.499862	889.714453	14.763879
20.563065	887.483017	14.768896
20.312245	882.242573	14.773914
20.550004	881.678586	14.778931
20.647282	889.912553	14.783949
20.844218	889.815658	14.788967
20.569734	887.680979	14.793984
20.476464	876.246557	14.799002
20.618436	896.995498	14.804019
20.610675	896.766375	14.809037
20.924706	897.257150	14.814055
20.711247	880.953212	14.819072
20.299896	862.019824	14.824090
20.533742	878.039786	14.829107
20.949402	880.995138	14.834125
20.576656	881.198375	14.839143
20.883311	887.894459	14.844160
20.842594	874.962352	14.849178
20.546340	875.993102	14.854195
20.755204	880.025198	14.859213
20.974871	887.233430	14.864231
20.806561	890.222903	14.869248
21.003008	874.227527	14.874266
20.832460	878.063081	14.879283
20.677045	878.336618	14.884301
20.901279	884.098816	14.889319
20.908174	881.263936	14.894336
21.282740	880.315740	14.899354
21.043919	881.410130	14.904371
20.705761	874.602267	14.909389
20.790382	876.321624	14.914407
20.570204	891.187866	14.919424
20.779056	887.340109	14.924442
20.660471	887.440659	14.929459
20.973984	881.490672	14.934477
21.215296	888.989018	14.939495
20.921017	889.912167	14.944512
21.187123	886.917010	14.949530
21.119195	889.098766	14.954547
21.212638	885.991641	14.959565
21.304832	886.665273	14.964583
20.944050	882.805224	14.969600
20.808369	879.285660	14.974618
20.689922	893.637460	14.979635
21.262076	907.679780	14.984653
21.396505	903.780493	14.989671
21.328604	909.540847	14.994688
21.700607	906.030594	14.999706
21.524751	913.429804	15.004723
21.584616	909.119257	15.009741
21.734331	908.613158	15.014759
21.331885	897.286819	15.019776
21.572764	886.639789	15.024794
21.291815	879.703099	15.029811
21.105296	885.784864	15.034829
21.671392	897.420298	15.039847
21.377753	896.421508	15.044864
21.699328	899.984789	15.049882
21.637239	902.238219	15.054899
21.791832	897.960262	15.059917
21.728415	904.792865	15.064935
21.527835	905.029255	15.069952
21.772397	892.996281	15.074970
21.657861	895.680744	15.079987
21.375039	902.528572	15.085005
21.735611	905.432547	15.090023
21.180841	904.373430	15.095040
21.489924	902.157357	15.100058
21.866073	905.737388	15.105075
21.713931	898.607070	15.110093
21.620319	904.519745	15.115111
21.824957	899.700677	15.120128
21.774612	901.538877	15.125146
22.054876	908.469447	15.130163
21.701693	906.713084	15.135181
21.713006	903.158006	15.140199
21.685406	897.743950	15.145216
21.957029	904.865208	15.150234
21.703771	899.584113	15.155251
21.855804	931.616426	15.160269
22.207384	925.373325	15.165287
22.036088	923.651755	15.170304
22.106638	926.383143	15.175322
22.069002	927.370475	15.180339
22.139162	927.249138	15.185357
22.549514	922.028814	15.190375
22.298195	910.732584	15.195392
21.967125	906.833191	15.200410
22.047863	909.695530	15.205427
22.212121	915.782649	15.210445
22.425338	914.742811	15.215463
22.063234	910.958699	15.220480
22.245803	917.809812	15.225498
22.265017	920.243085	15.230515
22.242584	920.518009	15.235533
22.580088	920.639064	15.240551
22.354498	936.285652	15.245568
22.342156	925.779008	15.250586
22.693768	924.815450	15.255603
22.397711	925.445393	15.260621
22.341008	910.732759	15.265639
22.360969	912.739891	15.270656
22.170356	921.880211	15.275674
22.337928	922.835592	15.280691
21.966492	924.682763	15.285709
22.731711	913.212482	15.290727
22.650876	926.895749	15.295744
22.621802	921.011711	15.300762
22.463800	925.173518	15.305779
22.328960	925.525902	15.310797
22.499727	914.962353	15.315815
22.510288	927.438523	15.320832
22.669161	926.135752	15.325850
22.694789	928.347126	15.330867
22.328745	923.042561	15.335885
22.755613	943.964944	15.340903
22.917297	947.297515	15.345920
22.565058	941.085097	15.350938
22.813214	944.511499	15.355955
23.092508	951.249737	15.360973
23.246730	940.878093	15.365991
22.703331	952.531677	15.371008
22.686783	949.154494	15.376026
22.925009	946.166824	15.381043
23.082970	942.203906	15.386061
23.351622	945.444084	15.391079
23.231086	953.289124	15.396096
23.273758	947.687390	15.401114
22.900904	927.586626	15.406131
22.956093	935.833479	15.411149
22.702304	934.386679	15.416167
22.728693	947.251709	15.421184
23.185534	949.036194	15.426202
22.793231	947.538376	15.431219
22.665021	954.923873	15.436237
22.942363	950.396423	15.441255
22.893091	952.010404	15.446272
23.155930	961.108545	15.451290
23.391136	969.500951	15.456307
23.247022	972.376219	15.461325
23.671583	957.970460	15.466343
23.499748	971.850962	15.471360
23.260652	954.263405	15.476378
23.429157	952.712984	15.481395
23.386398	971.849789	15.486413
23.660116	967.521710	15.491431
23.280335	963.197552	15.496448
23.516815	962.848352	15.501466
23.591098	961.744937	15.506483
23.697403	963.252647	15.511501
23.573096	950.226205	15.516519
23.380008	946.583025	15.521536
23.689532	957.592585	15.526554
23.993167	959.230514	15.531571
23.355568	960.816178	15.536589
23.592673	954.303718	15.541607
23.379545	951.219068	15.546624
23.704134	968.414697	15.551642
23.867434	968.730130	15.556659
23.740945	967.970393	15.561677
23.661649	960.629897	15.566695
23.848799	966.438919	15.571712
23.959473	972.026326	15.576730
24.173594	964.696947	15.581747
23.880110	965.945018	15.586765
23.928553	965.038126	15.591783
23.248881	963.181115	15.596800
23.691157	969.742508	15.601818
23.677004	965.421381	15.606835
23.638572	965.436870	15.611853
23.502538	963.687716	15.616871
23.622887	970.646364	15.621888
23.870674	981.864363	15.626906
24.099056	983.611839	15.631923
24.096022	994.651152	15.636941
24.307344	1000.825646	15.641959
24.193454	994.522451	15.646976
24.091347	990.290751	15.651994
24.557041	992.320009	15.657011
24.126759	987.303132	15.662029
24.490518	982.348816	15.667047
24.031299	986.071550	15.672064
24.405053	995.092481	15.677082
24.599259	984.869218	15.682099
24.580133	981.520832	15.687117
24.143951	969.290845	15.692135
23.734129	966.511365	15.697152
24.238817	990.530095	15.702170
24.481016	986.008107	15.707187
24.371025	1000.961424	15.712205
24.344637	987.998602	15.717223
24.487299	994.553006	15.722240
24.075397	1004.264299	15.727258
24.443782	994.970104	15.732275
24.219231	996.570355	15.737293
24.747365	991.003474	15.742311
24.608951	983.331352	15.747328
23.924170	994.252753	15.752346
24.485151	991.994293	15.757363
24.641489	1001.105881	15.762381
25.051775	1002.010854	15.767399
24.989521	1005.233138	15.772416
24.932713	1005.895260	15.777434
25.138145	987.105545	15.782451
24.777255	990.497397	15.787469
24.715577	983.595952	15.792487
24.721242	978.306079	15.797504
24.656331	984.492017	15.802522
25.223394	998.487866	15.807539
24.900509	998.288872	15.812557
25.014388	980.804119	15.817575
25.028296	984.664624	15.822592
24.944649	986.451215	15.827610
25.084230	995.537007	15.832627
25.267209	997.301021	15.837645
25.412500	996.890280	15.842663
24.963503	985.078837	15.847680
24.890904	981.861850	15.852698
24.795397	990.062764	15.857715
24.890644	1000.228415	15.862733
25.239111	1004.923601	15.867751
25.497339	1004.236505	15.872768
25.220044	1000.874663	15.877786
25.696127	998.152903	15.882803
25.216514	1001.856726	15.887821
25.356334	999.569166	15.892839
25.407440	981.374676	15.897856
25.408214	983.943370	15.902874
25.280195	981.116857	15.907891
25.365318	999.138737	15.912909
25.379589	990.950542	15.917927
25.346682	1003.414599	15.922944
25.609800	1011.319849	15.927962
25.706713	995.721706	15.932979
25.699989	1003.460687	15.937997
25.486772	995.636108	15.943015
25.632456	992.732265	15.948032
25.603233	992.058367	15.953050
25.487541	989.785345	15.958067
25.808988	999.814794	15.963085
25.614404	996.809298	15.968103
25.744566	992.904344	15.973120
25.646654	996.302588	15.978138
25.669384	995.336584	15.983155
25.490675	999.889789	15.988173
25.729098	1002.282632	15.993191
26.016946	995.550821	15.998208
25.495913	994.502224	16.003226
25.906898	998.070540	16.008243
25.820807	995.344792	16.013261
25.785071	1006.417606	16.018279
25.549073	1005.485572	16.023296
25.634875	1002.925561	16.028314
25.629812	993.667421	16.033331
25.896757	1003.320356	16.038349
26.223242	1011.392463	16.043367
26.397072	1009.023869	16.048384
25.973549	1008.001113	16.053402
26.244081	998.943054	16.058419
26.554027	1000.999719	16.063437
25.879975	999.634125	16.068455
26.122235	997.557830	16.073472
26.037854	1010.424374	16.078490
26.308693	1011.650855	16.083507
25.983354	1015.501071	16.088525
26.289021	1020.988708	16.093543
26.235598	1008.683320	16.098560
26.376342	1019.293171	16.103578
26.526251	1007.726131	16.108595
26.218048	1009.563465	16.113613
26.213164	1002.940344	16.118631
26.752465	1011.156038	16.123648
26.539853	1011.091350	16.128666
26.552325	999.451040	16.133683
26.554183	1005.620279	16.138701
26.803216	1001.535872	16.143719
26.846922	1000.490864	16.148736
26.737166	1007.280229	16.153754
26.568990	1002.516023	16.158771
26.766551	998.616352	16.163789
26.868106	997.663321	16.168807
27.134426	999.382802	16.173824
26.880295	1011.856062	16.178842
26.944945	997.976513	16.183859
26.637214	984.770324	16.188877
26.593934	982.943612	16.193895
27.014286	987.223665	16.198912
27.072699	998.209233	16.203930
26.984569	986.101766	16.208947
26.494612	987.841167	16.213965
26.894121	999.837115	16.218983
27.077087	998.211857	16.224000
26.767662	1008.046051	16.229018
26.882491	1001.054003	16.234035
26.897984	1007.300013	16.239053
27.358440	1002.299078	16.244071
27.517456	1000.507138	16.249088
26.840129	1005.257897	16.254106
26.959960	992.319642	16.259123
27.074670	1003.511039	16.264141
27.225083	1012.087077	16.269159
27.345250	1003.178657	16.274176
27.298182	1000.809744	16.279194
27.250068	1004.165523	16.284211
27.262549	1006.606168	16.289229
27.139276	1003.684240	16.294247
27.252335	995.960336	16.299264
27.181965	1011.781636	16.304282
27.467427	1000.427020	16.309299
27.360039	999.276151	16.314317
27.125482	1006.782367	16.319335
27.147424	999.700642	16.324352
26.854874	1008.471877	16.329370
27.241553	1019.213848	16.334387
27.724727	1027.529805	16.339405
27.277864	1029.385574	16.344423
27.363222	1021.943678	16.349440
27.561905	1035.031251	16.354458
27.591952	1032.675573	16.359475
27.740322	1037.862663	16.364493
27.835288	1031.501691	16.369511
27.929232	1026.116008	16.374528
27.331188	1028.039497	16.379546
27.540237	1031.288971	16.384563
27.845353	1030.831255	16.389581
27.783283	1022.576038	16.394599
27.959143	1029.608116	16.399616
28.064883	1048.914384	16.404634
28.117357	1033.537719	16.409651
28.170653	1025.703188	16.414669
27.823514	1026.577770	16.419687
28.032165	1021.650748	16.424704
27.753270	1036.223301	16.429722
28.287908	1047.576559	16.434739
28.411186	1058.511040	16.439757
28.299141	1047.445499	16.444775
28.332317	1034.347139	16.449792
28.003085	1027.392662	16.454810
28.219613	1026.794107	16.459827
27.982206	1029.743869	16.464845
28.122905	1038.308810	16.469863
28.431976	1039.983770	16.474880
28.466877	1043.089949	16.479898
28.221997	1041.117897	16.484915
28.902921	1034.425856	16.489933
28.538485	1041.475789	16.494951
28.624724	1024.156241	16.499968
28.227852	1029.213628	16.504986
28.410562	1030.665267	16.510003
28.750499	1034.913672	16.515021
28.483513	1048.525031	16.520039
28.552619	1040.262005	16.525056
28.408813	1035.036411	16.530074
28.003838	1039.422887	16.535091
28.329850	1039.047123	16.540109
28.098712	1046.975696	16.545127
28.724367	1041.226361	16.550144
28.464712	1041.885354	16.555162
28.488655	1040.628829	16.560179
29.179438	1052.677292	16.565197
28.775072	1047.722633	16.570215
28.367258	1043.043063	16.575232
28.723447	1062.856298	16.580250
29.235185	1057.421336	16.585267
29.148153	1057.214021	16.590285
29.251994	1063.013956	16.595303
28.743685	1044.190142	16.600320
28.971839	1053.883858	16.605338
29.093850	1066.071378	16.610355
29.306742	1058.647479	16.615373
29.203305	1067.537619	16.620391
29.061717	1057.874674	16.625408
28.960817	1047.163999	16.630426
29.207125	1064.558100	16.635443
28.994802	1057.714795	16.640461
29.185570	1070.399689	16.645479
29.553484	1066.552375	16.650496
29.223978	1066.550068	16.655514
29.502459	1065.957645	16.660531
29.513470	1066.000149	16.665549
29.221047	1061.476175	16.670567
29.363866	1060.248476	16.675584
29.469942	1062.005535	16.680602
29.525830	1072.489776	16.685619
29.518748	1061.287966	16.690637
29.308866	1067.509128	16.695655
29.431078	1062.844858	16.700672
29.605470	1060.425678	16.705690
29.430839	1068.992393	16.710707
29.919300	1062.046288	16.715725
29.870554	1065.168651	16.720743
29.730039	1059.339787	16.725760
29.807331	1064.402253	16.730778
29.501434	1058.412949	16.735795
29.796675	1058.912965	16.740813
29.268307	1056.489595	16.745831
29.542466	1061.123783	16.750848
29.871312	1062.991323	16.755866
29.647416	1072.455634	16.760883
29.991710	1071.199721	16.765901
29.962608	1083.530699	16.770919
30.347897	1077.837712	16.775936
30.340285	1076.668147	16.780954
29.902951	1066.931324	16.785971
30.014216	1053.397920	16.790989
30.114568	1074.080965	16.796007
29.878779	1075.285346	16.801024
30.165233	1082.038298	16.806042
30.135293	1093.479488	16.811059
30.233072	1078.076795	16.816077
30.261757	1084.642666	16.821095
29.912493	1081.213120	16.826112
30.118486	1087.375850	16.831130
29.878709	1079.893035	16.836147
30.275208	1076.773405	16.841165
29.941537	1075.913379	16.846183
30.260280	1081.537852	16.851200
30.399730	1087.048232	16.856218
30.537135	1101.991517	16.861235
30.717537	1097.595886	16.866253
30.751914	1116.279029	16.871271
30.626098	1093.441432	16.876288
30.560499	1090.747192	16.881306
30.251504	1091.164564	16.886323
30.572567	1104.113214	16.891341
30.654110	1103.239032	16.896359
30.759544	1097.308747	16.901376
30.631996	1108.487437	16.906394
30.709221	1103.855407	16.911411
30.923014	1104.888807	16.916429
30.529137	1112.703893	16.921447
30.870082	1106.399269	16.926464
31.004742	1110.168419	16.931482
30.930718	1108.513736	16.936499
31.127149	1093.853055	16.941517
31.375896	1106.588908	16.946535
31.296311	1102.167483	16.951552
31.278274	1105.827864	16.956570
31.164369	1101.042558	16.961587
30.842406	1103.465861	16.966605
31.261120	1107.408532	16.971623
31.197497	1104.606686	16.976640
31.350657	1101.499693	16.981658
30.955392	1098.844157	16.986675
31.252126	1090.807596	16.991693
31.254174	1094.673127	16.996711
31.057308	1095.366527	17.001728
31.006785	1099.265491	17.006746
30.989419	1103.291835	17.011763
30.934956	1099.046379	17.016781
30.830758	1106.466070	17.021799
31.559639	1120.099154	17.026816
31.261855	1129.925290	17.031834
31.590575	1129.271395	17.036851
31.578171	1116.110644	17.041869
31.503461	1122.449633	17.046887
31.386581	1120.195714	17.051904
31.531906	1113.959415	17.056922
31.316284	1117.126703	17.061939
31.675346	1119.027414	17.066957
31.588535	1119.444906	17.071975
31.771274	1117.854386	17.076992
31.788902	1124.958474	17.082010
31.818977	1135.367877	17.087027
32.460335	1130.922560	17.092045
32.244300	1120.172963	17.097063
31.857465	1117.317298	17.102080
32.278512	1115.317293	17.107098
31.927999	1120.787206	17.112115
32.044946	1114.050401	17.117133
31.801694	1113.084778	17.122151
32.040707	1115.808901	17.127168
32.117431	1114.316937	17.132186
32.106756	1123.334672	17.137203
32.194173	1130.793966	17.142221
32.083732	1129.548890	17.147239
31.777231	1135.655732	17.152256
32.258379	1130.528465	17.157274
32.269807	1141.912753	17.162291
32.279870	1136.372842	17.167309
32.122813	1140.124301	17.172327
32.093597	1140.719017	17.177344
32.358549	1141.129079	17.182362
32.221708	1149.955034	17.187379
32.349718	1141.389303	17.192397
32.590185	1143.983817	17.197415
32.150209	1144.005020	17.202432
32.563583	1150.088147	17.207450
32.803572	1156.630613	17.212467
33.086222	1160.531365	17.217485
32.937181	1153.589808	17.222503
32.636734	1162.542227	17.227520
32.622592	1146.446851	17.232538
32.732711	1153.580732	17.237555
33.000523	1167.929417	17.242573
33.105461	1168.547428	17.247591
32.839359	1153.674693	17.252608
32.820213	1146.731849	17.257626
32.983668	1159.998567	17.262643
33.118501	1162.783098	17.267661
32.948804	1152.931975	17.272679
32.857225	1164.379652	17.277696
33.041886	1165.783662	17.282714
32.837589	1170.867910	17.287731
33.153854	1167.356817	17.292749
33.359903	1173.841458	17.297767
33.104244	1171.195732	17.302784
33.489089	1165.761560	17.307802
33.386110	1171.167701	17.312819
33.455686	1171.582937	17.317837
33.482343	1166.182442	17.322855
33.540042	1163.645718	17.327872
33.668890	1158.532270	17.332890
33.469747	1156.512058	17.337907
33.563145	1150.088173	17.342925
33.342891	1140.510014	17.347943
33.189489	1147.631272	17.352960
33.578832	1150.294125	17.357978
33.209775	1152.895179	17.362995
33.385938	1151.214162	17.368013
33.267855	1152.005750	17.373031
33.443473	1155.045859	17.378048
33.676680	1156.779979	17.383066
33.355982	1154.743979	17.388083
33.490280	1164.796349	17.393101
33.810582	1167.741351	17.398119
33.835295	1177.766608	17.403136
33.882909	1174.250005	17.408154
33.970264	1179.699098	17.413171
34.358042	1188.269823	17.418189
34.142263	1190.250574	17.423207
34.116066	1188.010930	17.428224
34.127370	1182.338268	17.433242
34.366959	1181.565705	17.438259
34.304536	1184.052751	17.443277
34.397497	1166.324921	17.448295
33.734516	1167.545328	17.453312
33.998782	1168.050170	17.458330
34.137332	1182.204400	17.463347
34.596529	1185.099378	17.468365
34.588797	1178.830082	17.473383
34.410413	1191.048679	17.478400
34.825489	1188.610942	17.483418
34.394950	1185.130914	17.488435
34.443635	1181.607831	17.493453
34.603970	1184.880697	17.498471
34.279963	1183.476366	17.503488
34.224593	1178.694549	17.508506
34.547833	1174.055755	17.513523
34.477182	1166.294109	17.518541
34.455739	1169.926631	17.523559
34.373705	1170.403341	17.528576
34.509459	1164.938524	17.533594
34.529881	1162.394981	17.538611
34.462813	1167.334786	17.543629
34.593062	1172.881339	17.548647
34.755729	1190.077148	17.553664
34.875486	1193.533058	17.558682
34.962479	1195.435112	17.563699
34.660315	1195.422235	17.568717
34.359253	1194.702292	17.573735
34.519946	1195.122276	17.578752
34.968747	1197.659114	17.583770
35.082931	1198.802703	17.588787
34.876787	1198.389871	17.593805
34.945368	1202.718435	17.598823
35.166981	1214.612839	17.603840
35.330568	1217.790531	17.608858
35.289493	1224.581909	17.613875
35.296965	1219.096023	17.618893
35.353164	1221.911741	17.623911
35.408155	1232.269985	17.628928
35.499249	1225.969507	17.633946
35.578501	1225.193504	17.638963
35.563598	1225.574557	17.643981
35.652300	1229.612818	17.648999
35.556478	1225.616767	17.654016
35.494292	1216.944913	17.659034
35.782182	1217.423988	17.664051
35.747042	1217.044491	17.669069
35.982715	1209.793707	17.674087
35.601039	1210.705232	17.679104
35.525481	1206.560864	17.684122
35.878747	1207.250665	17.689139
35.581675	1212.434576	17.694157
35.832476	1204.196833	17.699175
35.606213	1216.672209	17.704192
35.735888	1210.122734	17.709210
35.881162	1221.940667	17.714227
35.813547	1218.359945	17.719245
35.914218	1208.501410	17.724263
35.822514	1214.215076	17.729280
35.992022	1213.671173	17.734298
35.843646	1209.882122	17.739315
36.014798	1222.715346	17.744333
36.236503	1225.240210	17.749351
36.200548	1230.765321	17.754368
36.272171	1222.173617	17.759386
35.978031	1234.097843	17.764403
36.185309	1233.642732	17.769421
36.339141	1226.849650	17.774439
36.514787	1231.123681	17.779456
36.275793	1232.098199	17.784474
36.440698	1236.916701	17.789491
36.384941	1234.615381	17.794509
36.537544	1230.921475	17.799527
36.509174	1235.590188	17.804544
36.749727	1241.867511	17.809562
36.813763	1231.146824	17.814579
36.739427	1232.032589	17.819597
36.807837	1233.713480	17.824615
36.612676	1231.626368	17.829632
36.558207	1231.022663	17.834650
36.586479	1239.270692	17.839667
36.969736	1250.486704	17.844685
37.241518	1264.598166	17.849703
37.331254	1266.783822	17.854720
37.194407	1254.677445	17.859738
36.811454	1239.551432	17.864755
36.687866	1256.902327	17.869773
37.109390	1248.199328	17.874791
37.413967	1260.175520	17.879808
37.576540	1252.352277	17.884826
37.455223	1251.272988	17.889843
37.105768	1243.927100	17.894861
37.320937	1246.494010	17.899879
37.597475	1255.795296	17.904896
37.200362	1243.562192	17.909914
37.222325	1249.687360	17.914931
37.130658	1250.840911	17.919949
37.047603	1245.021975	17.924967
37.421149	1251.092403	17.929984
37.159357	1258.350502	17.935002
37.600682	1255.129189	17.940019
37.366738	1252.839831	17.945037
37.843523	1247.706898	17.950055
37.671843	1256.124921	17.955072
37.788024	1253.705311	17.960090
37.869258	1257.940400	17.965107
37.463291	1258.502261	17.970125
37.750825	1251.792493	17.975143
37.308332	1263.449503	17.980160
37.677629	1273.957650	17.985178
37.893482	1277.509067	17.990195
37.933050	1281.968399	17.995213
38.061446	1276.271165	18.000231
38.088143	1283.610589	18.005248
37.996823	1280.434332	18.010266
37.895300	1274.593016	18.015283
37.623158	1275.629501	18.020301
37.795654	1277.871701	18.025319
38.523761	1272.810084	18.030336
37.985577	1274.803173	18.035354
38.561181	1269.231972	18.040371
38.256445	1276.916485	18.045389
38.470894	1270.457930	18.050407
38.394135	1288.795641	18.055424
38.300935	1290.448050	18.060442
38.455789	1298.278767	18.065459
38.438817	1294.251489	18.070477
38.390972	1293.858189	18.075495
38.712794	1291.857836	18.080512
38.639027	1286.905285	18.085530
38.750044	1286.269501	18.090547
38.932107	1294.162251	18.095565
38.873349	1289.743849	18.100583
38.628318	1288.686975	18.105600
38.505106	1289.047022	18.110618
38.742836	1289.439236	18.115635
38.477548	1301.548362	18.120653
38.639484	1293.292856	18.125671
38.758186	1297.156048	18.130688
39.191358	1300.206575	18.135706
39.035522	1309.622546	18.140723
39.317986	1307.290647	18.145741
39.297489	1297.495110	18.150759
39.171581	1307.304050	18.155776
39.311277	1306.354532	18.160794
39.651926	1298.323663	18.165811
39.105992	1301.280480	18.170829
39.506852	1297.598401	18.175847
39.298383	1303.961436	18.180864
39.144277	1309.277750	18.185882
39.501748	1306.271454	18.190899
39.224125	1312.496936	18.195917
39.729441	1306.075133	18.200935
39.921668	1312.871246	18.205952
39.642654	1309.698960	18.210970
39.624907	1299.530608	18.215987
39.707119	1297.539158	18.221005
39.467900	1299.810749	18.226023
39.598497	1304.454730	18.231040
39.162192	1307.571204	18.236058
39.497888	1298.976218	18.241075
39.610931	1306.895499	18.246093
39.960673	1302.684891	18.251111
40.139356	1296.616903	18.256128
39.727838	1311.901450	18.261146
40.100736	1321.200391	18.266163
39.979490	1331.513548	18.271181
39.915540	1322.308587	18.276199
40.227676	1328.574795	18.281216
40.230394	1333.453289	18.286234
40.335970	1339.426613	18.291251
39.970958	1323.871701	18.296269
40.218105	1322.526755	18.301287
40.395610	1327.788288	18.306304
40.156946	1331.085434	18.311322
40.565686	1323.397403	18.316339
40.202696	1318.751806	18.321357
39.934834	1315.710327	18.326375
40.547807	1325.360056	18.331392
40.041378	1327.070495	18.336410
40.904877	1331.123846	18.341427
40.747407	1338.678160	18.346445
40.753423	1348.498141	18.351463
41.006746	1354.457935	18.356480
40.718141	1346.963674	18.361498
41.196931	1344.888383	18.366515
40.687903	1322.523567	18.371533
40.861812	1335.192340	18.376551
40.889377	1342.932442	18.381568
40.761458	1342.662062	18.386586
40.952936	1344.121829	18.391603
40.872038	1351.506436	18.396621
41.149251	1344.085028	18.401639
41.323007	1346.377533	18.406656
41.111801	1353.511030	18.411674
41.262789	1344.080087	18.416691
41.150533	1351.794625	18.421709
40.885823	1349.282826	18.426727
41.061872	1356.816778	18.431744
41.029688	1354.584356	18.436762
41.156773	1362.835992	18.441779
41.155470	1377.678028	18.446797
41.536156	1370.767520	18.451815
41.472724	1370.565994	18.456832
41.567399	1373.132748	18.461850
41.742508	1364.815198	18.466867
41.816870	1372.330275	18.471885
41.949684	1368.910822	18.476903
42.011211	1366.414499	18.481920
41.614553	1366.927576	18.486938
42.204920	1366.677905	18.491955
41.768645	1359.680003	18.496973
41.506644	1357.944111	18.501991
41.969331	1360.731277	18.507008
41.725599	1366.468661	18.512026
42.005049	1362.054388	18.517043
41.847317	1366.711718	18.522061
41.940912	1361.398573	18.527079
41.996985	1370.664818	18.532096
41.989414	1376.463266	18.537114
42.359853	1375.948035	18.542131
42.283022	1383.530839	18.547149
42.210432	1384.766635	18.552167
42.222875	1388.996687	18.557184
42.245442	1389.214119	18.562202
42.563576	1386.056144	18.567219
42.420001	1386.116406	18.572237
42.504105	1393.374353	18.577255
42.544832	1392.099411	18.582272
42.559902	1393.637142	18.587290
42.476790	1380.237896	18.592307
42.488251	1387.286244	18.597325
42.265092	1381.145093	18.602343
42.673790	1388.933171	18.607360
42.550242	1410.898016	18.612378
42.586992	1406.038679	18.617395
42.722728	1404.468075	18.622413
42.890780	1410.908226	18.627431
42.748365	1403.091377	18.632448
42.743134	1407.415704	18.637466
43.400738	1408.796592	18.642483
43.245642	1401.770674	18.647501
43.565017	1403.825918	18.652519
43.443736	1401.812491	18.657536
43.127221	1402.701257	18.662554
43.213523	1394.454324	18.667571
43.663699	1398.341669	18.672589
43.338632	1403.514214	18.677607
43.498887	1396.278253	18.682624
43.578186	1399.475412	18.687642
43.475997	1393.889781	18.692659
43.965731	1395.577672	18.697677
43.530491	1398.681373	18.702695
44.140680	1391.488971	18.707712
43.898043	1401.439214	18.712730
43.526434	1390.091980	18.717747
43.767571	1407.824894	18.722765
43.780483	1390.819365	18.727783
43.871213	1393.800148	18.732800
43.627616	1400.544229	18.737818
43.835364	1388.485095	18.742835
44.113635	1388.571196	18.747853
43.951734	1380.198812	18.752871
44.235622	1382.082853	18.757888
43.537796	1388.187592	18.762906
43.851755	1394.664980	18.767923
44.066696	1401.123074	18.772941
44.008347	1419.385469	18.777959
44.084545	1415.750758	18.782976
44.178620	1414.820960	18.787994
43.988915	1420.606755	18.793011
44.179126	1415.205967	18.798029
44.209354	1425.101117	18.803047
44.210909	1411.366771	18.808064
44.378134	1422.240984	18.813082
44.758160	1434.394896	18.818099
44.796273	1440.056864	18.823117
45.081578	1441.672446	18.828135
45.441472	1415.896477	18.833152
45.583362	1414.842469	18.838170
45.444361	1394.423898	18.843187
45.589847	1402.628506	18.848205
45.580717	1396.589726	18.853223
45.664620	1375.196037	18.858240
45.239501	1374.075678	18.863258
44.926950	1377.497945	18.868275
45.192208	1367.932433	18.873293
44.498886	1368.867241	18.878311
44.875488	1361.376703	18.883328
44.836915	1373.630461	18.888346
45.143940	1383.725489	18.893363
45.609196	1385.022714	18.898381
45.433423	1389.010670	18.903399
45.523972	1389.577280	18.908416
45.572653	1395.682559	18.913434
45.589476	1387.733627	18.918451
45.654022	1387.748861	18.923469
45.421381	1388.173286	18.928487
45.554859	1389.200273	18.933504
45.534808	1393.037752	18.938522
45.632632	1395.720785	18.943539
45.613681	1393.300104	18.948557
45.390027	1406.946015	18.953575
45.486269	1397.835994	18.958592
45.364578	1395.999357	18.963610
45.240846	1390.126746	18.968627
45.469513	1397.551537	18.973645
45.354781	1414.058602	18.978663
45.633930	1413.459753	18.983680
45.530186	1419.743408	18.988698
45.452249	1414.791470	18.993715
46.084419	1426.464304	18.998733
45.999566	1436.841284	19.003751
46.183673	1443.010701	19.008768
46.242296	1437.138085	19.013786
46.160452	1442.351668	19.018803
46.369013	1442.559077	19.023821
46.225521	1440.738453	19.028839
46.209156	1440.195080	19.033856
46.368498	1443.550201	19.038874
46.475370	1466.381805	19.043891
46.810080	1461.280400	19.048909
46.485134	1475.172510	19.053927
46.751728	1467.213056	19.058944
46.940267	1467.937983	19.063962
46.987285	1464.979998	19.068979
47.231092	1454.947561	19.073997
47.056212	1462.700299	19.079015
47.521234	1459.989661	19.084032
47.024350	1450.050458	19.089050
46.889649	1439.833962	19.094067
47.150891	1444.501821	19.099085
47.325960	1453.153129	19.104103
47.280105	1455.397790	19.109120
47.120235	1464.751354	19.114138
47.020432	1460.159417	19.119155
47.169327	1453.215538	19.124173
47.058692	1453.620968	19.129191
47.031813	1454.663458	19.134208
47.110568	1455.746307	19.139226
46.669329	1462.073055	19.144243
47.195049	1474.065454	19.149261
47.361691	1478.631284	19.154279
47.557339	1474.327862	19.159296
47.640720	1475.132278	19.164314
47.369526	1485.784454	19.169331
47.739244	1483.953349	19.174349
47.977961	1490.515072	19.179367
47.731365	1485.299037	19.184384
48.205518	1493.815437	19.189402
48.399669	1505.540741	19.194419
48.207207	1489.911480	19.199437
47.901427	1491.107850	19.204455
48.370164	1480.115719	19.209472
48.164905	1477.689320	19.214490
47.854295	1485.980758	19.219507
48.533464	1493.408032	19.224525
48.058789	1509.340059	19.229543
48.228283	1501.581903	19.234560
48.368769	1500.133629	19.239578
48.294996	1510.568888	19.244595
48.801211	1506.668389	19.249613
48.610554	1503.027872	19.254631
48.827852	1511.618985	19.259648
48.783055	1498.500865	19.264666
48.678140	1503.061644	19.269683
48.772241	1502.084500	19.274701
48.941293	1507.603025	19.279719
48.939291	1502.478293	19.284736
49.160558	1495.226480	19.289754
49.202529	1502.576241	19.294771
49.188602	1494.805619	19.299789
49.053898	1502.539496	19.304807
49.165785	1506.157640	19.309824
49.031411	1496.565917	19.314842
49.475641	1510.022713	19.319859
49.150507	1497.787694	19.324877
49.066158	1497.538930	19.329895
49.018382	1504.053743	19.334912
49.116661	1492.797387	19.339930
48.860059	1510.368056	19.344947
48.812790	1494.930782	19.349965
49.161506	1502.633575	19.354983
49.384668	1514.455355	19.360000
49.472763	1518.866165	19.365018
49.249562	1529.671842	19.370035
49.635168	1523.849275	19.375053
49.451621	1527.137875	19.380071
49.825886	1523.059099	19.385088
49.923806	1516.795326	19.390106
50.069523	1520.698542	19.395123
49.988128	1513.686351	19.400141
49.644401	1512.783686	19.405159
49.990663	1526.037994	19.410176
50.160346	1529.871209	19.415194
50.029355	1548.337552	19.420211
50.423889	1536.198744	19.425229
50.447949	1537.492088	19.430247
50.184850	1541.133907	19.435264
50.480440	1540.144326	19.440282
50.697832	1534.237491	19.445299
50.498070	1534.486384	19.450317
50.518182	1534.701043	19.455335
50.285684	1537.605942	19.460352
50.644416	1526.779234	19.465370
50.428436	1536.602324	19.470387
50.958515	1529.854690	19.475405
50.591312	1541.714756	19.480423
50.694809	1535.405926	19.485440
51.017861	1531.414017	19.490458
50.980176	1539.325311	19.495475
50.947244	1529.825075	19.500493
50.639790	1538.419007	19.505511
50.665166	1528.534148	19.510528
51.213462	1541.119531	19.515546
50.526708	1553.660526	19.520563
51.280913	1546.496133	19.525581
51.308711	1567.235229	19.530599
51.271132	1553.996023	19.535616
51.156102	1561.477550	19.540634
51.079795	1559.671700	19.545651
51.121496	1555.597357	19.550669
51.012063	1557.227071	19.555687
51.020944	1569.009666	19.560704
51.689615	1568.182905	19.565722
51.645833	1580.595409	19.570739
51.967762	1569.452508	19.575757
51.559875	1570.374443	19.580775
51.630063	1571.073619	19.585792
51.774240	1574.213371	19.590810
51.568476	1580.696006	19.595827
52.215971	1572.014472	19.600845
52.004813	1574.325911	19.605863
51.758391	1570.889724	19.610880
51.983877	1566.745738	19.615898
52.079206	1580.193792	19.620915
52.260078	1572.121405	19.625933
52.215046	1573.359236	19.630951
52.063246	1568.914224	19.635968
52.658252	1578.680500	19.640986
52.620234	1585.761877	19.646003
52.286713	1568.712285	19.651021
52.365521	1572.256695	19.656039
52.386568	1586.413763	19.661056
52.652895	1581.565971	19.666074
52.627058	1585.865147	19.671091
52.810264	1582.740769	19.676109
52.812378	1587.117645	19.681127
52.912204	1586.016527	19.686144
53.020192	1576.712079	19.691162
52.782181	1579.100284	19.696179
52.865553	1579.712199	19.701197
53.037410	1578.988037	19.706215
52.837352	1584.737627	19.711232
53.221925	1565.398695	19.716250
52.828044	1578.471629	19.721267
52.961761	1577.321053	19.726285
53.464998	1579.186744	19.731303
53.271690	1589.811076	19.736320
53.539040	1598.306074	19.741338
53.050901	1605.031501	19.746355
53.117667	1598.046703	19.751373
53.118599	1597.096683	19.756391
53.155372	1607.577904	19.761408
53.514258	1590.470980	19.766426
53.418615	1611.311399	19.771443
53.934862	1622.841462	19.776461
53.670426	1624.659420	19.781479
53.505398	1630.858014	19.786496
54.058471	1630.913955	19.791514
53.441766	1621.065897	19.796531
53.926986	1625.209772	19.801549
54.069505	1631.884356	19.806567
53.779533	1629.007214	19.811584
54.012511	1629.753632	19.816602
54.241992	1640.059698	19.821619
54.719210	1647.392246	19.826637
54.833510	1643.839921	19.831655
54.620633	1640.183899	19.836672
54.808239	1622.920571	19.841690
54.364565	1631.305378	19.846707
54.424891	1621.175181	19.851725
54.508659	1625.271105	19.856743
54.858692	1640.831846	19.861760
55.366506	1639.323214	19.866778
54.800333	1636.302878	19.871795
54.955436	1623.364985	19.876813
54.938282	1615.212955	19.881831
54.913700	1628.537702	19.886848
55.130299	1635.125012	19.891866
55.074315	1640.744889	19.896883
55.080375	1644.493148	19.901901
55.258178	1634.871682	19.906919
55.364864	1646.336137	19.911936
55.161536	1638.323538	19.916954
55.209409	1637.931107	19.921971
55.164860	1642.687653	19.926989
55.310663	1636.599423	19.932007
55.103314	1643.038145	19.937024
55.301445	1647.245659	19.942042
55.214159	1641.540862	19.947059
55.184040	1661.667381	19.952077
55.755124	1659.044344	19.957095
55.734502	1673.637165	19.962112
55.707573	1664.094897	19.967130
55.434040	1679.187857	19.972147
55.405829	1670.712468	19.977165
55.872185	1668.153073	19.982183
55.752021	1667.736310	19.987200
56.359729	1662.163146	19.992218
55.549572	1672.337602	19.997235
55.945368	1685.688461	20.002253
56.212573	1682.727716	20.007271
56.005311	1686.427145	20.012288
56.554206	1690.580057	20.017306
56.275588	1703.234340	20.022323
56.358304	1697.471499	20.027341
56.428288	1688.538991	20.032359
56.345884	1694.437559	20.037376
56.437304	1687.717137	20.042394
56.648893	1705.394987	20.047411
56.455392	1716.827328	20.052429
56.914143	1707.259912	20.057447
57.023042	1709.385834	20.062464
56.998676	1707.107968	20.067482
56.779758	1712.324036	20.072499
57.162934	1708.613069	20.077517
57.460690	1708.440512	20.082535
57.157021	1709.658659	20.087552
57.536071	1708.432007	20.092570
57.725337	1712.640917	20.097587
57.666288	1719.261708	20.102605
57.501100	1706.755484	20.107623
57.168704	1706.453817	20.112640
57.542677	1704.271726	20.117658
57.412903	1704.269878	20.122675
57.601188	1706.380283	20.127693
57.536474	1695.272255	20.132711
57.538252	1702.883981	20.137728
57.490355	1697.671663	20.142746
57.661796	1694.154613	20.147763
57.364241	1707.499828	20.152781
58.285064	1720.778437	20.157799
58.020283	1727.762630	20.162816
57.772732	1739.601041	20.167834
57.737714	1729.141636	20.172851
57.466557	1723.238218	20.177869
57.997308	1723.518547	20.182887
57.780300	1738.586976	20.187904
58.066301	1742.695624	20.192922
58.252286	1746.415891	20.197939
58.502271	1754.825303	20.202957
58.968299	1734.561457	20.207975
58.608303	1750.993408	20.212992
58.842671	1746.194731	20.218010
58.746140	1748.507280	20.223027
58.810908	1741.462775	20.228045
58.831277	1751.422758	20.233063
58.585571	1751.663028	20.238080
58.595681	1750.519062	20.243098
59.032916	1741.046499	20.248115
59.240593	1736.425553	20.253133
59.275510	1730.537597	20.258151
59.418888	1744.902967	20.263168
59.285457	1727.853627	20.268186
59.511913	1740.590249	20.273203
59.392047	1740.640508	20.278221
59.696668	1734.650597	20.283239
59.752583	1736.765836	20.288256
59.293146	1744.604027	20.293274
59.407542	1739.369583	20.298291
58.915836	1731.404997	20.303309
59.642228	1750.233532	20.308327
59.399544	1758.744899	20.313344
59.811821	1754.748518	20.318362
59.933136	1748.496800	20.323379
59.959310	1753.472745	20.328397
60.159122	1754.113876	20.333415
60.281189	1751.914193	20.338432
60.506269	1743.901119	20.343450
60.724818	1739.975929	20.348467
60.751503	1746.706462	20.353485
60.518683	1721.385260	20.358503
60.263831	1720.468747	20.363520
60.045239	1711.991421	20.368538
60.326578	1724.792072	20.373555
60.333966	1747.680553	20.378573
61.019704	1731.589293	20.383591
60.318592	1731.322940	20.388608
60.657451	1738.055360	20.393626
60.959204	1738.021040	20.398643
61.175966	1740.874959	20.403661
61.056139	1732.085594	20.408679
61.032128	1739.780248	20.413696
60.888453	1745.353849	20.418714
61.146784	1736.010131	20.423731
61.127625	1736.139387	20.428749
61.239988	1734.332547	20.433767
61.032812	1739.559419	20.438784
61.243373	1737.080866	20.443802
61.267853	1737.323251	20.448819
60.760093	1742.868329	20.453837
61.122713	1740.757431	20.458855
61.268506	1761.405797	20.463872
61.049780	1764.090832	20.468890
61.423791	1764.196744	20.473907
61.478497	1768.303538	20.478925
61.644650	1770.455267	20.483943
61.777730	1779.353120	20.488960
62.073022	1780.490640	20.493978
62.161085	1776.857164	20.498995
61.784962	1790.489236	20.504013
62.178917	1777.207923	20.509031
62.349187	1777.749510	20.514048
62.402009	1775.582697	20.519066
62.272135	1779.620400	20.524083
62.420696	1785.975356	20.529101
62.353094	1778.929355	20.534119
62.362418	1781.493677	20.539136
62.121646	1788.310049	20.544154
62.497619	1780.652172	20.549171
62.021318	1783.954840	20.554189
62.475330	1793.935696	20.559207
62.588315	1813.109118	20.564224
62.590237	1815.305358	20.569242
62.791151	1805.844308	20.574259
62.562899	1816.893949	20.579277
62.987476	1809.250583	20.584295
63.038562	1809.914872	20.589312
62.725811	1814.747937	20.594330
63.014354	1819.771416	20.599347
63.229120	1831.537908	20.604365
63.621160	1825.083062	20.609383
63.303838	1830.295551	20.614400
63.289114	1825.399931	20.619418
63.337155	1825.102147	20.624435
63.475883	1830.183668	20.629453
63.314880	1823.827553	20.634471
63.297014	1821.583375	20.639488
63.501908	1832.581367	20.644506
64.011474	1829.753282	20.649523
63.550992	1842.435979	20.654541
64.522010	1850.471236	20.659559
64.309710	1843.501388	20.664576
64.126428	1838.325886	20.669594
64.430674	1826.264057	20.674611
63.865093	1818.374051	20.679629
64.105831	1830.335320	20.684647
64.321607	1831.964920	20.689664
64.373177	1840.635646	20.694682
64.824451	1831.530089	20.699699
64.529177	1838.796792	20.704717
64.763527	1847.297047	20.709735
64.674917	1843.375476	20.714752
64.394932	1829.466884	20.719770
64.955696	1832.153647	20.724787
64.811349	1837.569587	20.729805
65.028481	1836.062014	20.734823
64.883193	1830.325161	20.739840
64.983865	1831.818043	20.744858
64.901478	1824.212576	20.749875
64.781557	1835.264297	20.754893
64.604209	1839.801725	20.759911
65.158372	1849.281011	20.764928
64.952963	1850.322917	20.769946
65.179623	1851.553181	20.774963
65.089624	1854.685261	20.779981
65.074644	1849.231080	20.784999
65.429698	1862.481114	20.790016
65.507981	1874.565539	20.795034
65.392347	1877.471233	20.800051
65.826373	1868.036974	20.805069
65.810883	1869.800417	20.810087
65.582335	1875.879594	20.815104
65.999889	1877.594550	20.820122
66.218252	1880.037976	20.825139
66.433482	1889.172409	20.830157
66.559047	1886.823838	20.835175
66.352664	1870.581009	20.840192
66.070375	1876.018437	20.845210
66.618430	1875.712232	20.850227
66.883429	1895.142950	20.855245
66.694030	1888.093777	20.860263
66.373379	1887.989099	20.865280
66.347622	1901.525678	20.870298
66.970909	1891.787375	20.875315
66.824378	1894.303393	20.880333
66.484053	1891.023780	20.885351
66.948790	1891.327014	20.890368
66.477737	1890.308448	20.895386
66.667114	1889.613105	20.900403
66.931039	1900.292668	20.905421
67.046627	1903.582102	20.910439
67.572052	1912.857607	20.915456
67.520720	1915.365118	20.920474
67.508918	1915.521633	20.925491
67.490604	1909.471486	20.930509
67.466034	1906.530885	20.935527
67.793800	1906.842821	20.940544
67.579835	1904.692283	20.945562
67.666248	1903.081977	20.950579
68.102847	1904.752944	20.955597
67.893099	1907.414511	20.960615
67.812407	1905.176949	20.965632
68.189614	1908.747554	20.970650
68.131754	1899.737012	20.975667
68.137297	1904.094496	20.980685
68.324179	1899.202182	20.985703
68.222846	1897.646355	20.990720
67.883394	1903.727029	20.995738
68.153092	1901.583241	21.000755
68.148259	1905.323783	21.005773
68.173415	1911.268794	21.010791
68.513615	1923.681715	21.015808
68.582310	1932.081566	21.020826
68.913118	1918.620626	21.025843
68.697728	1918.676290	21.030861
68.930603	1918.595887	21.035879
68.751967	1918.863587	21.040896
68.871389	1926.453936	21.045914
68.933419	1916.556843	21.050931
68.770266	1923.253881	21.055949
68.931917	1932.071620	21.060967
68.785481	1942.300686	21.065984
68.813765	1943.697546	21.071002
69.396058	1943.524871	21.076019
69.657253	1943.433747	21.081037
69.706539	1948.769078	21.086055
69.670870	1941.317239	21.091072
69.637997	1945.579726	21.096090
69.541714	1941.829746	21.101107
69.844590	1950.474022	21.106125
69.924972	1965.843492	21.111143
69.879937	1964.515588	21.116160
70.154779	1968.329368	21.121178
70.005971	1959.367672	21.126195
70.148182	1966.253876	21.131213
70.117012	1968.606771	21.136231
70.009388	1961.469095	21.141248
69.849859	1967.966762	21.146266
69.792813	1964.163330	21.151283
70.332053	1981.083515	21.156301
70.389487	1992.132967	21.161319
70.523034	1992.415181	21.166336
70.467881	1995.936350	21.171354
70.691778	1994.374061	21.176371
70.901107	1983.911178	21.181389
70.728887	1995.488712	21.186407
70.703805	2003.401405	21.191424
70.782788	2015.372203	21.196442
70.821274	2005.128419	21.201459
70.893921	2017.377926	21.206477
70.700504	2014.722383	21.211495
71.174748	2024.880107	21.216512
71.382453	2038.822271	21.221530
71.748198	2034.773110	21.226547
72.157689	2037.470833	21.231565
72.074972	2039.494079	21.236583
71.925232	2028.973461	21.241600
71.927853	2040.457528	21.246618
71.833790	2024.998677	21.251635
71.988747	2033.107424	21.256653
71.828539	2036.471381	21.261671
71.988783	2022.680298	21.266688
71.902020	2032.155325	21.271706
72.077837	2032.304721	21.276723
72.180705	2030.268947	21.281741
71.763432	2039.407256	21.286759
72.495458	2038.305515	21.291776
72.495308	2046.997017	21.296794
72.773204	2054.966707	21.301811
72.993735	2052.448688	21.306829
72.436534	2057.875322	21.311847
72.590062	2056.021013	21.316864
72.862982	2050.439893	21.321882
72.747257	2056.722480	21.326899
73.215681	2046.904059	21.331917
73.030833	2057.237005	21.336935
73.631335	2043.749760	21.341952
72.864355	2044.992725	21.346970
72.561803	2046.703046	21.351987
72.952983	2045.638592	21.357005
72.731926	2047.191051	21.362023
73.149337	2061.829605	21.367040
73.241333	2067.436044	21.372058
73.353161	2067.996207	21.377075
73.556474	2081.964337	21.382093
73.450000	2080.002177	21.387111
73.634630	2096.078239	21.392128
73.859140	2098.852111	21.397146
73.773644	2100.661192	21.402163
73.968818	2094.154847	21.407181
73.837453	2098.593658	21.412199
74.301206	2092.995436	21.417216
74.056950	2092.219270	21.422234
74.398296	2101.081701	21.427251
74.849520	2106.225106	21.432269
74.655978	2125.610697	21.437287
74.919292	2118.945404	21.442304
74.804773	2121.317608	21.447322
74.450088	2118.949101	21.452339
74.679407	2104.841073	21.457357
74.501399	2110.252868	21.462375
74.685125	2112.111556	21.467392
74.496945	2116.499254	21.472410
74.905571	2130.126173	21.477427
75.247746	2132.843859	21.482445
75.446307	2140.721793	21.487463
75.502349	2136.821818	21.492480
75.899027	2131.612742	21.497498
75.888943	2129.828083	21.502515
76.010530	2131.172560	21.507533
75.369914	2130.325553	21.512551
75.774476	2121.312334	21.517568
76.005164	2127.335875	21.522586
75.629606	2125.680705	21.527603
75.690523	2126.135183	21.532621
75.605698	2130.661434	21.537639
75.973794	2132.825950	21.542656
75.559205	2125.679193	21.547674
76.106128	2148.206461	21.552691
76.312991	2139.268197	21.557709
76.101160	2153.985860	21.562727
76.588410	2153.117891	21.567744
76.499948	2151.881945	21.572762
76.358633	2149.934670	21.577779
77.036006	2140.001612	21.582797
76.666293	2137.550231	21.587815
76.789072	2133.308492	21.592832
77.121597	2149.563556	21.597850
76.866449	2154.965283	21.602867
77.325573	2157.999296	21.607885
77.498685	2156.302882	21.612903
77.415188	2158.812279	21.617920
77.566053	2157.163512	21.622938
77.367978	2156.973472	21.627955
77.434040	2158.465458	21.632973
77.507386	2161.202913	21.637991
77.845258	2160.355045	21.643008
78.023067	2157.815260	21.648026
77.609516	2159.268305	21.653043
77.784307	2159.130670	21.658061
77.780084	2166.781400	21.663079
77.841954	2152.936102	21.668096
77.873643	2155.433877	21.673114
77.633484	2157.140805	21.678131
77.567872	2154.436938	21.683149
77.839726	2169.379122	21.688167
77.806410	2167.686443	21.693184
78.270623	2171.871590	21.698202
77.990440	2179.688373	21.703219
78.591873	2193.219046	21.708237
78.447789	2199.370392	21.713255
78.846425	2204.572509	21.718272
78.839527	2202.828374	21.723290
79.128962	2192.867319	21.728307
79.483943	2191.571796	21.733325
78.777060	2199.079463	21.738343
79.142396	2189.466372	21.743360
79.458790	2184.140386	21.748378
79.270430	2187.597121	21.753395
79.578392	2182.253513	21.758413
79.376410	2194.574303	21.763431
79.612219	2186.729783	21.768448
79.681243	2188.069824	21.773466
79.451230	2197.472563	21.778483
79.560853	2194.757187	21.783501
79.958966	2212.763123	21.788519
79.875810	2215.657503	21.793536
80.086894	2215.381667	21.798554
79.853168	2218.318426	21.803571
80.222509	2213.309252	21.808589
79.994971	2216.478588	21.813607
80.336631	2219.818093	21.818624
80.459418	2214.282388	21.823642
80.397656	2220.117952	21.828659
80.651819	2224.077026	21.833677
80.792963	2237.815104	21.838695
80.758374	2240.806073	21.843712
81.025440	2239.688345	21.848730
80.699034	2246.770701	21.853747
80.705895	2244.005041	21.858765
80.766205	2248.240468	21.863783
80.558230	2248.184519	21.868800
81.091770	2253.059517	21.873818
80.866714	2263.657632	21.878835
81.312981	2256.736573	21.883853
80.813893	2261.712384	21.888871
80.607600	2267.052886	21.893888
81.558548	2281.640112	21.898906
81.531350	2287.798538	21.903923
81.827681	2288.415194	21.908941
82.049640	2294.386499	21.913959
81.866426	2286.903836	21.918976
82.210947	2292.647764	21.923994
82.056590	2288.354457	21.929011
82.215588	2290.321162	21.934029
82.263617	2288.988211	21.939047
82.579587	2312.517374	21.944064
82.782469	2308.133727	21.949082
82.804139	2308.875202	21.954099
82.906938	2302.929148	21.959117
82.779231	2288.501001	21.964135
82.672078	2297.928848	21.969152
83.177987	2295.890256	21.974170
83.129844	2303.977095	21.979187
83.189522	2298.580585	21.984205
83.253262	2298.949417	21.989223
83.315395	2300.183236	21.994240
83.417221	2290.626899	21.999258
83.462030	2293.384596	22.004275
83.237668	2288.698224	22.009293
83.574008	2292.218462	22.014311
83.763174	2294.328800	22.019328
83.791768	2292.118358	22.024346
83.614227	2293.373713	22.029363
83.881314	2302.481349	22.034381
83.712897	2298.950820	22.039399
83.552607	2301.604744	22.044416
84.084446	2287.032883	22.049434
83.833039	2298.824924	22.054451
83.683621	2309.225087	22.059469
84.013465	2315.053363	22.064487
83.940507	2315.711736	22.069504
84.255301	2301.849035	22.074522
84.052341	2317.613236	22.079539
84.227718	2329.992139	22.084557
84.436305	2325.102642	22.089575
84.421134	2341.825449	22.094592
84.497599	2339.825311	22.099610
84.441111	2360.114520	22.104627
85.016011	2355.802336	22.109645
85.035930	2363.250564	22.114663
85.120652	2367.176087	22.119680
85.066354	2363.422638	22.124698
85.139804	2370.231336	22.129715
85.174981	2377.295319	22.134733
85.634072	2383.640013	22.139751
85.645146	2395.315507	22.144768
85.822683	2385.213968	22.149786
85.986050	2388.278289	22.154803
85.913370	2379.831579	22.159821
86.185871	2381.749062	22.164839
85.894462	2379.938746	22.169856
85.962163	2381.149613	22.174874
85.976226	2398.385504	22.179891
86.274761	2395.678557	22.184909
86.513028	2403.664041	22.189927
86.193998	2406.232236	22.194944
86.427614	2397.662086	22.199962
86.796727	2414.290414	22.204979
86.554544	2404.636088	22.209997
87.027291	2401.412837	22.215015
87.064487	2419.184822	22.220032
87.049781	2432.199342	22.225050
87.348952	2423.947197	22.230067
87.533586	2420.383768	22.235085
87.614490	2427.244979	22.240103
87.516192	2429.217042	22.245120
87.578319	2421.061769	22.250138
87.523632	2428.130295	22.255155
87.450162	2431.092633	22.260173
87.796518	2423.357038	22.265191
87.785233	2431.239368	22.270208
87.840592	2419.310571	22.275226
87.876816	2418.938873	22.280243
88.151164	2429.348872	22.285261
88.193878	2446.129040	22.290279
88.244546	2448.497661	22.295296
88.293836	2446.782626	22.300314
88.191650	2446.912189	22.305331
88.311925	2442.348855	22.310349
88.287493	2442.759821	22.315367
88.083988	2448.279835	22.320384
88.420882	2463.316287	22.325402
88.707821	2462.864525	22.330419
88.934800	2470.353147	22.335437
88.869688	2466.001719	22.340455
88.511187	2466.512038	22.345472
89.093904	2470.738771	22.350490
89.157156	2480.209614	22.355507
89.235803	2478.764578	22.360525
89.338215	2479.155796	22.365543
89.411879	2480.624534	22.370560
89.887930	2478.928264	22.375578
89.997743	2474.776832	22.380595
89.318772	2484.723022	22.385613
89.532752	2484.017514	22.390631
89.577420	2492.402433	22.395648
89.639149	2497.224716	22.400666
89.570988	2505.810258	22.405683
90.014679	2505.151041	22.410701
90.301841	2519.002309	22.415719
90.648528	2532.841164	22.420736
90.632340	2524.458179	22.425754
90.758020	2527.039209	22.430771
90.756900	2530.192284	22.435789
91.215750	2528.924751	22.440807
90.981710	2524.129362	22.445824
91.276013	2528.404168	22.450842
91.086240	2518.848925	22.455859
90.950205	2528.972557	22.460877
91.570355	2525.025699	22.465895
91.336968	2532.387194	22.470912
91.191239	2524.071718	22.475930
91.418690	2527.416440	22.480947
91.263942	2543.978118	22.485965
91.632319	2547.136788	22.490983
91.844366	2549.448736	22.496000
92.041662	2548.991993	22.501018
91.777947	2553.962798	22.506035
91.805400	2559.809830	22.511053
92.241279	2557.687433	22.516071
92.356915	2571.382397	22.521088
92.224071	2569.351701	22.526106
92.163100	2571.248535	22.531123
92.267279	2575.587670	22.536141
92.474873	2567.144576	22.541159
92.434065	2581.286813	22.546176
92.557197	2588.113107	22.551194
92.929452	2586.085825	22.556211
93.055462	2593.779581	22.561229
93.282691	2579.194945	22.566247
93.330697	2587.102829	22.571264
93.168992	2592.998259	22.576282
93.235431	2592.893272	22.581299
93.468383	2616.868136	22.586317
93.612001	2610.505341	22.591335
93.500447	2630.860239	22.596352
93.865412	2618.627467	22.601370
93.849543	2610.459003	22.606387
93.732073	2613.153646	22.611405
93.847461	2614.098309	22.616423
93.789914	2625.386977	22.621440
93.951795	2636.994964	22.626458
94.125340	2641.515833	22.631475
93.938250	2647.317396	22.636493
94.199383	2643.356976	22.641511
94.232387	2653.915142	22.646528
94.462149	2660.339825	22.651546
95.023199	2648.953883	22.656563
95.098239	2647.462055	22.661581
95.176589	2643.195552	22.666599
95.401389	2641.380584	22.671616
95.379251	2640.620307	22.676634
95.611937	2641.840221	22.681651
95.566680	2643.081316	22.686669
95.907400	2627.626841	22.691687
95.643885	2629.836103	22.696704
95.717951	2634.138913	22.701722
96.181823	2624.989967	22.706739
96.036130	2628.989294	22.711757
96.065757	2630.916213	22.716775
96.062098	2636.155844	22.721792
96.171395	2632.613570	22.726810
96.446261	2633.463972	22.731827
96.308922	2638.067960	22.736845
96.445615	2637.222989	22.741863
96.531007	2632.980641	22.746880
96.110760	2630.221455	22.751898
96.312070	2627.943052	22.756915
96.503914	2645.880547	22.761933
96.654876	2651.973487	22.766951
96.685028	2665.672365	22.771968
96.781011	2658.199730	22.776986
96.871357	2663.497321	22.782003
96.890101	2675.862977	22.787021
97.109362	2677.220694	22.792039
97.327762	2682.652999	22.797056
97.482827	2681.398036	22.802074
97.372608	2687.752576	22.807091
97.710773	2695.151393	22.812109
97.681598	2689.232071	22.817127
97.802536	2702.162547	22.822144
97.950867	2708.391626	22.827162
97.854213	2700.652297	22.832179
97.732255	2707.403178	22.837197
98.546459	2727.437312	22.842215
98.166249	2730.722034	22.847232
98.447689	2735.099886	22.852250
98.656035	2730.295531	22.857267
98.477964	2731.513126	22.862285
98.856222	2726.480329	22.867303
98.535422	2734.685559	22.872320
98.638102	2749.724001	22.877338
99.187958	2743.439933	22.882355
99.584185	2741.153261	22.887373
99.719740	2735.965730	22.892391
99.819021	2739.636583	22.897408
99.823820	2740.355455	22.902426
100.336964	2742.746792	22.907443
99.918508	2743.654648	22.912461
100.441579	2733.243475	22.917479
100.174335	2727.298085	22.922496
99.970503	2730.668964	22.927514
100.102762	2733.567761	22.932531
100.028071	2738.749047	22.937549
100.391795	2731.799630	22.942567
100.048342	2734.015039	22.947584
100.198955	2732.050653	22.952602
100.491055	2744.607345	22.957619
100.298508	2757.248970	22.962637
100.358240	2758.593658	22.967655
100.302586	2756.689788	22.972672
100.796190	2774.012339	22.977690
101.094149	2782.547322	22.982707
101.581852	2781.969614	22.987725
101.394603	2791.066178	22.992743
101.370188	2776.908758	22.997760
101.052018	2784.119440	23.002778
101.325800	2779.244919	23.007795
100.820835	2796.937574	23.012813
101.635751	2800.613795	23.017831
101.939377	2804.442211	23.022848
102.105529	2807.951176	23.027866
102.251222	2802.578996	23.032883
101.885982	2802.837887	23.037901
101.992748	2802.442574	23.042919
102.156171	2821.025351	23.047936
101.960539	2831.499288	23.052954
102.388679	2829.513775	23.057971
102.766649	2829.559116	23.062989
102.605733	2822.533544	23.068007
102.598120	2824.781889	23.073024
102.698148	2855.601196	23.078042
103.217481	2847.980512	23.083059
103.018523	2865.745522	23.088077
103.081170	2851.429308	23.093095
103.315613	2853.428514	23.098112
103.065655	2856.074388	23.103130
103.796451	2862.162338	23.108147
103.608410	2868.563774	23.113165
103.548504	2874.093122	23.118183
103.858097	2870.696358	23.123200
103.610146	2867.190723	23.128218
104.285387	2878.599009	23.133235
104.276517	2889.772957	23.138253
104.684383	2879.616344	23.143271
104.394624	2883.852771	23.148288
103.972054	2891.688875	23.153306
104.523836	2882.652355	23.158323
104.410351	2893.179815	23.163341
104.589746	2904.400207	23.168359
105.061754	2916.850107	23.173376
105.181885	2917.513156	23.178394
105.383901	2924.100058	23.183411
105.368104	2919.633534	23.188429
105.682264	2914.373959	23.193447
105.663790	2908.421338	23.198464
105.599712	2912.035603	23.203482
105.389051	2903.404984	23.208499
105.697770	2927.620954	23.213517
105.849030	2933.777066	23.218535
105.685211	2935.330157	23.223552
105.611187	2943.020490	23.228570
105.930433	2942.551063	23.233587
105.951470	2961.231900	23.238605
106.405651	2965.529261	23.243623
106.611603	2962.110743	23.248640
106.325380	2958.415371	23.253658
106.622545	2967.487102	23.258675
106.739350	2976.725787	23.263693
106.951856	2977.724783	23.268711
106.940139	2973.219738	23.273728
106.909045	2981.607213	23.278746
107.166704	2968.387272	23.283763
107.472518	2985.597240	23.288781
107.496692	2998.432532	23.293799
107.470145	3004.351238	23.298816
107.649358	2995.423166	23.303834
107.734856	2991.834030	23.308851
107.816219	2988.390719	23.313869
108.315592	2991.437548	23.318887
108.638650	2984.421775	23.323904
108.607357	2987.222989	23.328922
108.780909	2984.917302	23.333939
108.679990	2989.970188	23.338957
108.895127	2980.370593	23.343975
109.120757	2982.270190	23.348992
108.668304	2989.580764	23.354010
109.055251	2979.818708	23.359027
109.369858	2993.126377	23.364045
108.782507	2991.958577	23.369063
109.218673	2991.477258	23.374080
109.515020	3011.813266	23.379098
109.836813	3005.621425	23.384115
109.974469	3006.931906	23.389133
109.806664	3003.839840	23.394151
109.686999	3001.930130	23.399168
109.366999	2998.454624	23.404186
109.873710	2997.731926	23.409203
109.909337	3004.761369	23.414221
109.967472	3011.443295	23.419239
110.085858	3019.447719	23.424256
110.261775	3022.674313	23.429274
110.518306	3025.184544	23.434291
110.522441	3028.513631	23.439309
110.335734	3029.669468	23.444327
110.535196	3039.453947	23.449344
110.414687	3046.283632	23.454362
110.758584	3048.890728	23.459379
110.765896	3045.439999	23.464397
110.709419	3067.188129	23.469415
111.164861	3076.894901	23.474432
111.328901	3072.886382	23.479450
111.691265	3069.342496	23.484467
112.108080	3074.021279	23.489485
112.098121	3086.944007	23.494503
112.205470	3084.538150	23.499520
111.943563	3091.181563	23.504538
112.112493	3090.006473	23.509555
112.041339	3090.882365	23.514573
112.074670	3097.587121	23.519591
112.605367	3087.594322	23.524608
112.685897	3111.896567	23.529626
112.640119	3119.087066	23.534643
112.625108	3121.595403	23.539661
112.909967	3124.094926	23.544679
113.196089	3107.184099	23.549696
112.796283	3120.748274	23.554714
112.975518	3130.810535	23.559731
113.569618	3131.658601	23.564749
113.212432	3137.780323	23.569767
113.461816	3135.784736	23.574784
113.319153	3144.599954	23.579802
113.566628	3152.404440	23.584819
114.084550	3153.008721	23.589837
113.764845	3153.415177	23.594855
114.361283	3152.586976	23.599872
114.392524	3164.114648	23.604890
114.612118	3171.686774	23.609907
114.774980	3177.093159	23.614925
114.649865	3175.389428	23.619943
114.881516	3172.314044	23.624960
115.094177	3174.518670	23.629978
115.248860	3168.497974	23.634995
115.189630	3172.455554	23.640013
115.340339	3175.452547	23.645031
115.298691	3164.122243	23.650048
115.162232	3185.106560	23.655066
115.758530	3196.748271	23.660083
115.912285	3190.020737	23.665101
115.383645	3198.135446	23.670119
115.599625	3194.557517	23.675136
115.422112	3199.972717	23.680154
115.750015	3220.051556	23.685171
115.927573	3224.496202	23.690189
115.663902	3220.551085	23.695207
116.368294	3237.225818	23.700224
116.560948	3237.767123	23.705242
116.780635	3243.022655	23.710259
117.051838	3238.221003	23.715277
117.121505	3241.719827	23.720295
116.899443	3234.918230	23.725312
117.060709	3242.240663	23.730330
117.224705	3243.032610	23.735347
117.360465	3245.580612	23.740365
117.312102	3256.656784	23.745383
117.507621	3257.882528	23.750400
117.571586	3265.519953	23.755418
117.339076	3263.368980	23.760435
117.565655	3269.803847	23.765453
117.631067	3290.362337	23.770471
118.128002	3285.727522	23.775488
118.181656	3299.025548	23.780506
118.352089	3306.608541	23.785523
118.304565	3313.868826	23.790541
118.170851	3317.815941	23.795559
118.375434	3313.526471	23.800576
118.958610	3325.785759	23.805594
119.104733	3330.692968	23.810611
119.246612	3331.478893	23.815629
119.182185	3337.706599	23.820647
119.444499	3334.017274	23.825664
119.542289	3335.990468	23.830682
119.738553	3350.907533	23.835699
120.004550	3355.029138	23.840717
119.505497	3361.229834	23.845735
120.084024	3351.586090	23.850752
120.209816	3361.249655	23.855770
120.242530	3361.926332	23.860787
120.360808	3358.189992	23.865805
120.422754	3373.715035	23.870823
120.447771	3373.966827	23.875840
120.717264	3378.580255	23.880858
120.690649	3385.701598	23.885875
120.588042	3385.569271	23.890893
120.656879	3398.211680	23.895911
121.169103	3402.342302	23.900928
120.941137	3404.987987	23.905946
120.927971	3410.431318	23.910963
121.281286	3426.302408	23.915981
121.705441	3424.680413	23.920999
121.986043	3427.171173	23.926016
122.039513	3424.167675	23.931034
122.301179	3437.171455	23.936051
122.419523	3446.132398	23.941069
122.755822	3455.643305	23.946087
122.922902	3449.210282	23.951104
123.051599	3443.234570	23.956122
122.809198	3444.181328	23.961139
123.021603	3437.510851	23.966157
122.832564	3438.818573	23.971175
122.889067	3443.641924	23.976192
122.861681	3442.898211	23.981210
122.995384	3443.584417	23.986227
122.723204	3458.347259	23.991245
123.195686	3469.086819	23.996263
123.539521	3456.904113	24.001280
123.744711	3476.206986	24.006298
123.693584	3483.616241	24.011315
124.102011	3490.376367	24.016333
124.262758	3490.837430	24.021351
124.469701	3491.461736	24.026368
124.082180	3490.455316	24.031386
124.366808	3496.657137	24.036403
124.707131	3495.777267	24.041421
124.971395	3512.997367	24.046439
124.734080	3511.462569	24.051456
124.819198	3506.295295	24.056474
124.876374	3514.262126	24.061491
125.313129	3508.617174	24.066509
124.754063	3517.683620	24.071527
125.275102	3522.800787	24.076544
125.406887	3535.660737	24.081562
125.101933	3538.589861	24.086579
125.410923	3542.881562	24.091597
125.857363	3558.479462	24.096615
126.099581	3547.549746	24.101632
126.424013	3559.862104	24.106650
126.339061	3557.757558	24.111667
126.534331	3565.914378	24.116685
126.659260	3576.244152	24.121703
126.912140	3570.069161	24.126720
127.152054	3569.520541	24.131738
126.919405	3566.984497	24.136755
127.010290	3567.383847	24.141773
126.926154	3571.556858	24.146791
127.071246	3574.264421	24.151808
127.227508	3581.991765	24.156826
127.423025	3591.792941	24.161843
127.312691	3588.297300	24.166861
127.742419	3605.693724	24.171879
127.638186	3607.950898	24.176896
128.153520	3615.944286	24.181914
128.012012	3618.579697	24.186931
128.824852	3631.987018	24.191949
128.769474	3636.780497	24.196967
128.954821	3639.778487	24.201984
129.265314	3634.449838	24.207002
129.030710	3637.955080	24.212019
129.443354	3629.463784	24.217037
129.560282	3632.715453	24.222055
129.457511	3630.121304	24.227072
129.869962	3628.217054	24.232090
129.401479	3633.074849	24.237107
129.190123	3627.918980	24.242125
129.469332	3653.737568	24.247143
129.636122	3652.597493	24.252160
129.706247	3663.526062	24.257178
129.825158	3677.347609	24.262195
129.930358	3680.541145	24.267213
129.948423	3687.220092	24.272231
130.234952	3709.729899	24.277248
130.516899	3717.677607	24.282266
130.428636	3721.551453	24.287283
130.515290	3725.072976	24.292301
130.485868	3741.224869	24.297319
130.394711	3744.900329	24.302336
131.092607	3756.722273	24.307354
131.144361	3764.851027	24.312371
131.357442	3767.320785	24.317389
131.645147	3778.932015	24.322407
132.163781	3789.967581	24.327424
132.513633	3784.165636	24.332442
132.357593	3792.131068	24.337459
132.475570	3799.914967	24.342477
132.624458	3794.826056	24.347495
132.305933	3790.886197	24.352512
132.328709	3801.181505	24.357530
132.354121	3814.755746	24.362547
132.458375	3821.983135	24.367565
132.565112	3818.472591	24.372583
132.654155	3840.517777	24.377600
132.967142	3837.694743	24.382618
132.926870	3838.139769	24.387635
133.366312	3841.691607	24.392653
133.856818	3853.201872	24.397671
133.816705	3854.824156	24.402688
134.127298	3854.655900	24.407706
134.182155	3851.450114	24.412723
134.128659	3849.056574	24.417741
134.687177	3867.335887	24.422759
134.885858	3871.038841	24.427776
134.922139	3862.874314	24.432794
134.919125	3865.327230	24.437811
135.405253	3861.659765	24.442829
135.340706	3854.650347	24.447847
135.471170	3857.982012	24.452864
135.758200	3841.887826	24.457882
135.885198	3848.092217	24.462899
136.564661	3847.440436	24.467917
136.348026	3848.335859	24.472935
136.245159	3848.279318	24.477952
136.392464	3849.354797	24.482970
136.238912	3852.124680	24.487987
136.664106	3854.476207	24.493005
136.283646	3852.979448	24.498023
136.262618	3854.693448	24.503040
136.754612	3857.684763	24.508058
136.662112	3867.246868	24.513075
137.034844	3873.416165	24.518093
137.052829	3872.346588	24.523111
136.857395	3874.659026	24.528128
137.303303	3887.527134	24.533146
137.012057	3893.998658	24.538163
137.434667	3899.809853	24.543181
137.694212	3902.777398	24.548199
137.634398	3925.417147	24.553216
137.941914	3917.948932	24.558234
138.202895	3911.419062	24.563251
138.406013	3914.591082	24.568269
138.597421	3928.145877	24.573287
138.704353	3927.245512	24.578304
138.901570	3927.899755	24.583322
138.987664	3926.563913	24.588339
139.244332	3923.105756	24.593357
139.449771	3918.219476	24.598375
139.111760	3938.478545	24.603392
139.518114	3942.183900	24.608410
139.358173	3956.872862	24.613427
139.744422	3948.202462	24.618445
139.809264	3944.269164	24.623463
139.664055	3958.990553	24.628480
140.066279	3974.592542	24.633498
139.935697	3986.780346	24.638515
140.233617	3984.190043	24.643533
140.582718	3990.606092	24.648551
140.619291	3995.113910	24.653568
140.857553	4004.318432	24.658586
140.912905	4009.959590	24.663603
141.265178	4000.202384	24.668621
141.708349	4011.511806	24.673639
142.087172	4016.420849	24.678656
142.203333	4006.899244	24.683674
141.876439	4018.596848	24.688691
142.475190	4010.966469	24.693709
142.349533	4015.224954	24.698727
142.266032	4024.100828	24.703744
142.403083	4014.055181	24.708762
142.445982	4022.371651	24.713779
142.470215	4015.648195	24.718797
142.936111	4005.882764	24.723815
142.444506	4016.305623	24.728832
142.803522	4017.651154	24.733850
142.764193	4043.352610	24.738867
143.099802	4044.698631	24.743885
143.348061	4034.127497	24.748903
143.332226	4042.128024	24.753920
143.281503	4047.864616	24.758938
143.293683	4064.606860	24.763955
143.025859	4071.456711	24.768973
143.562604	4077.755201	24.773991
143.634743	4088.301802	24.779008
143.848677	4106.622383	24.784026
144.140236	4104.793721	24.789043
144.174547	4116.605590	24.794061
144.885042	4121.926999	24.799079
144.700852	4139.359551	24.804096
144.808415	4136.776770	24.809114
145.068427	4134.555322	24.814131
145.351465	4148.916655	24.819149
145.658381	4155.926404	24.824167
145.514282	4162.008982	24.829184
145.894686	4151.799119	24.834202
145.786064	4153.195373	24.839219
146.004909	4170.249576	24.844237
146.266013	4177.604190	24.849255
146.210576	4175.880046	24.854272
146.510335	4177.326348	24.859290
146.531835	4194.452330	24.864307
146.582598	4190.249728	24.869325
146.872728	4206.251284	24.874343
146.806893	4205.014828	24.879360
147.329207	4222.454247	24.884378
147.303486	4234.619579	24.889395
147.338656	4224.835870	24.894413
147.568122	4237.539080	24.899431
147.619947	4247.031570	24.904448
148.004548	4248.104848	24.909466
148.002095	4251.144804	24.914483
148.207111	4257.596007	24.919501
148.906042	4270.472341	24.924519
148.759505	4278.218721	24.929536
148.482510	4278.596455	24.934554
148.693239	4283.029886	24.939571
148.824495	4275.393274	24.944589
149.172665	4283.917998	24.949607
149.506078	4301.863510	24.954624
149.487595	4296.560636	24.959642
149.871380	4301.838275	24.964659
149.933976	4317.152555	24.969677
150.180916	4317.360340	24.974695
150.066684	4321.847530	24.979712
150.223877	4326.043113	24.984730
150.382601	4323.540716	24.989747
150.362740	4346.433592	24.994765
150.541303	4343.801851	24.999783
150.424878	4352.032806	25.004800
150.467316	4344.387899	25.009818
150.962087	4364.773451	25.014835
151.006699	4370.309078	25.019853
151.780439	4376.816970	25.024871
151.579624	4388.791878	25.029888
151.584871	4386.480655	25.034906
151.262527	4393.534809	25.039923
151.402667	4405.971129	25.044941
152.012497	4415.575681	25.049959
152.031568	4418.751194	25.054976
152.386131	4434.383097	25.059994
152.434543	4443.863596	25.065011
152.945059	4456.497952	25.070029
152.957918	4445.376146	25.075047
152.822779	4459.392506	25.080064
153.348939	4460.409038	25.085082
153.713897	4465.945322	25.090099
153.526624	4476.059084	25.095117
153.572733	4472.403191	25.100135
153.633400	4480.035332	25.105152
153.917243	4482.980252	25.110170
154.118959	4499.892239	25.115187
154.048952	4499.085678	25.120205
154.229441	4498.167521	25.125223
154.019836	4511.469551	25.130240
154.378098	4519.071157	25.135258
154.516769	4523.332797	25.140275
154.719600	4540.797014	25.145293
154.952238	4557.650583	25.150311
155.618028	4554.766198	25.155328
155.234171	4550.366043	25.160346
155.613272	4572.303835	25.165363
155.677256	4567.530939	25.170381
156.010748	4560.970609	25.175399
156.516909	4563.309626	25.180416
156.837951	4557.496140	25.185434
156.938513	4559.308062	25.190451
157.114111	4560.480183	25.195469
157.429092	4564.225144	25.200487
157.522652	4561.657108	25.205504
157.450055	4569.019647	25.210522
157.823603	4560.171021	25.215539
157.894227	4555.586477	25.220557
158.078579	4553.578766	25.225575
157.846506	4562.853644	25.230592
157.792061	4557.856148	25.235610
158.031444	4564.860788	25.240627
158.068689	4577.865613	25.245645
158.419069	4581.791292	25.250663
158.235103	4588.700879	25.255680
158.279491	4594.476494	25.260698
158.798246	4607.125455	25.265715
158.857106	4612.816757	25.270733
159.012661	4616.239348	25.275751
159.078587	4639.011920	25.280768
159.133193	4652.995732	25.285786
159.514128	4654.606193	25.290803
159.472870	4668.342961	25.295821
159.871474	4666.683805	25.300839
159.966112	4678.208886	25.305856
159.971459	4688.097081	25.310874
160.335418	4690.739173	25.315891
160.288024	4692.160656	25.320909
160.599117	4704.974585	25.325927
160.724336	4718.404552	25.330944
161.051760	4722.289648	25.335962
161.156250	4730.786238	25.340979
161.602290	4742.225086	25.345997
161.871384	4736.637423	25.351015
162.147949	4737.702301	25.356032
162.405886	4737.112966	25.361050
162.393612	4736.278467	25.366067
161.861257	4739.378911	25.371085
162.128404	4749.658807	25.376103
162.442232	4761.711656	25.381120
162.750908	4763.759492	25.386138
163.168359	4754.351565	25.391155
163.233678	4779.409648	25.396173
163.286219	4790.044933	25.401191
163.646894	4790.503313	25.406208
163.048346	4785.309545	25.411226
163.498708	4790.251852	25.416243
163.578122	4793.746302	25.421261
163.742897	4806.317945	25.426279
164.006220	4812.918090	25.431296
164.025605	4807.129395	25.436314
164.332202	4828.093984	25.441331
164.189373	4843.364937	25.446349
164.714219	4829.328716	25.451367
165.056679	4830.733702	25.456384
164.786719	4845.642524	25.461402
164.966087	4844.206870	25.466419
165.258090	4851.175022	25.471437
165.682371	4859.116856	25.476455
165.932270	4873.332416	25.481472
165.868671	4879.367980	25.486490
166.142194	4871.134498	25.491507
166.049560	4884.143981	25.496525
166.547717	4904.681124	25.501543
166.363686	4897.809849	25.506560
166.479255	4901.046177	25.511578
166.900257	4917.261563	25.516595
166.997959	4926.302209	25.521613
167.196870	4928.970034	25.526631
167.211254	4930.618650	25.531648
167.566905	4942.636700	25.536666
168.190813	4940.440568	25.541683
168.126829	4944.250923	25.546701
167.997455	4947.146622	25.551719
168.008858	4958.391291	25.556736
168.512939	4964.739369	25.561754
168.662735	4967.938816	25.566771
168.593045	4974.824444	25.571789
168.954799	4982.337322	25.576807
169.120058	4993.949459	25.581824
168.772598	4995.162010	25.586842
169.399299	5010.692069	25.591859
169.202227	5020.703497	25.596877
169.663127	5025.764173	25.601895
170.383793	5034.666850	25.606912
170.407564	5039.991288	25.611930
170.870397	5033.921998	25.616947
170.480124	5042.719873	25.621965
170.353042	5051.075905	25.626983
170.479412	5059.439829	25.632000
170.841593	5069.954472	25.637018
170.972839	5067.497286	25.642035
170.987657	5090.085837	25.647053
171.103750	5095.272815	25.652071
171.609607	5107.920978	25.657088
171.588642	5119.120283	25.662106
171.883489	5124.484609	25.667123
172.159870	5134.283503	25.672141
172.666300	5134.031088	25.677159
173.163652	5123.717249	25.682176
172.867493	5133.703131	25.687194
173.235502	5120.170889	25.692212
173.299345	5131.085541	25.697229
173.417209	5144.491717	25.702247
174.062591	5140.221571	25.707264
173.647724	5143.461614	25.712282
173.996415	5143.126438	25.717300
173.663190	5144.715559	25.722317
174.065131	5158.677249	25.727335
174.332207	5164.216361	25.732352
174.357979	5177.510641	25.737370
174.305257	5162.216268	25.742388
174.478508	5176.027344	25.747405
175.223561	5192.208308	25.752423
175.275776	5198.800427	25.757440
174.933067	5204.172500	25.762458
175.178979	5194.529065	25.767476
175.192001	5217.077019	25.772493
175.414598	5224.772644	25.777511
175.474768	5230.634387	25.782528
175.621218	5255.500575	25.787546
176.213164	5246.298809	25.792564
176.404267	5260.328124	25.797581
176.643163	5275.195951	25.802599
177.166487	5272.822894	25.807616
177.153101	5270.362947	25.812634
177.067598	5276.370488	25.817652
177.044439	5296.660964	25.822669
177.531685	5295.035299	25.827687
177.641723	5291.173586	25.832704
177.694501	5311.606924	25.837722
178.027596	5320.456450	25.842740
178.141932	5313.557503	25.847757
178.586256	5338.131221	25.852775
179.118242	5331.486050	25.857792
179.017526	5339.481425	25.862810
179.314462	5335.773681	25.867828
179.057493	5341.978391	25.872845
179.228293	5355.783672	25.877863
180.105738	5350.745036	25.882880
179.738038	5360.543321	25.887898
179.733273	5356.446946	25.892916
180.112370	5360.747107	25.897933
180.251975	5382.849430	25.902951
180.426021	5379.473305	25.907968
180.782520	5394.335546	25.912986
180.731562	5406.508749	25.918004
180.562576	5412.494610	25.923021
180.717919	5414.026629	25.928039
181.194290	5424.334308	25.933056
181.503224	5431.700926	25.938074
181.620159	5435.218069	25.943092
181.548848	5453.887448	25.948109
181.574326	5462.642893	25.953127
181.935926	5472.438171	25.958144
182.165670	5479.754007	25.963162
182.430067	5490.887017	25.968180
182.591513	5506.300546	25.973197
182.283169	5514.542967	25.978215
182.908104	5528.135631	25.983232
182.964260	5530.910997	25.988250
183.123657	5545.933467	25.993268
183.670566	5560.785138	25.998285
183.704159	5566.780546	26.003303
184.183899	5573.145255	26.008320
184.457404	5583.601402	26.013338
184.759457	5575.233743	26.018356
184.958165	5574.284287	26.023373
184.816333	5585.180728	26.028391
185.636284	5590.842227	26.033408
185.155762	5606.889246	26.038426
185.227511	5597.938747	26.043444
185.587559	5601.443324	26.048461
185.573375	5620.889963	26.053479
186.453880	5618.129815	26.058496
186.877155	5606.798199	26.063514
187.054176	5603.042784	26.068532
187.309655	5611.285851	26.073549
186.843537	5599.373014	26.078567
187.240063	5598.777859	26.083584
187.287527	5604.827938	26.088602
187.185765	5596.946116	26.093620
187.375896	5613.797816	26.098637
187.376484	5623.583095	26.103655
187.652545	5626.371587	26.108672
187.975570	5629.525242	26.113690
188.126805	5648.049693	26.118708
188.168100	5649.119690	26.123725
188.161969	5652.460327	26.128743
188.527972	5654.758179	26.133760
189.022418	5669.794876	26.138778
188.992687	5665.168859	26.143796
189.439965	5677.899143	26.148813
189.719237	5689.238292	26.153831
190.115989	5690.982118	26.158848
189.842291	5689.777923	26.163866
190.027183	5691.027586	26.168884
190.243076	5706.821066	26.173901
190.426488	5714.879693	26.178919
190.711954	5710.412926	26.183936
190.730906	5718.108900	26.188954
190.679825	5723.041149	26.193972
191.522449	5724.674526	26.198989
191.427692	5739.342153	26.204007
191.354858	5740.098483	26.209024
191.329987	5756.327220	26.214042
191.751117	5763.632314	26.219060
192.100935	5774.581744	26.224077
191.959027	5788.612807	26.229095
192.368081	5796.124973	26.234112
192.718284	5815.499306	26.239130
192.746767	5816.536585	26.244148
193.335306	5823.020178	26.249165
193.035374	5842.842984	26.254183
193.193667	5839.778575	26.259200
193.400507	5847.385376	26.264218
193.883591	5856.947300	26.269236
193.937775	5863.675087	26.274253
194.163263	5880.174303	26.279271
194.542684	5879.821705	26.284288
194.652256	5896.367391	26.289306
194.979543	5897.222420	26.294324
195.304606	5906.588010	26.299341
195.262933	5914.725961	26.304359
195.963629	5919.717991	26.309376
195.995107	5911.130305	26.314394
195.888038	5918.984875	26.319412
196.130587	5927.454218	26.324429
195.992090	5934.871762	26.329447
196.327559	5935.618194	26.334464
196.542035	5949.341368	26.339482
196.530741	5953.812932	26.344500
196.720544	5961.075206	26.349517
197.397513	5981.030165	26.354535
197.751921	5974.908000	26.359552
197.487603	5990.631286	26.364570
197.770419	6000.464369	26.369588
198.209728	6006.295744	26.374605
198.214486	6018.006126	26.379623
198.501641	6017.453240	26.384640
198.395024	6029.960657	26.389658
198.735218	6028.108451	26.394676
199.030157	6032.516575	26.399693
199.184908	6046.381699	26.404711
199.434768	6049.003877	26.409728
199.659125	6059.439541	26.414746
199.865541	6072.611650	26.419764
199.713051	6071.874680	26.424781
199.953622	6084.094489	26.429799
200.280715	6081.505664	26.434816
200.297519	6096.708621	26.439834
200.388596	6101.713540	26.444852
200.858661	6109.765593	26.449869
200.587036	6134.963230	26.454887
201.243423	6126.827408	26.459904
200.893923	6133.501349	26.464922
201.206594	6158.263975	26.469940
201.588922	6169.230678	26.474957
201.757897	6179.457223	26.479975
201.962681	6188.630188	26.484992
202.435942	6203.983135	26.490010
202.624588	6219.986486	26.495028
202.353880	6221.319745	26.500045
202.350131	6241.276800	26.505063
202.849735	6247.354555	26.510080
203.256375	6269.151219	26.515098
203.703678	6287.030457	26.520116
203.890006	6291.850138	26.525133
204.043687	6295.674237	26.530151
204.499242	6306.036166	26.535168
204.708615	6321.004145	26.540186
204.387594	6319.033887	26.545204
204.912564	6321.007191	26.550221
205.041742	6338.342553	26.555239
204.938049	6341.786893	26.560256
205.706174	6353.337605	26.565274
205.776575	6367.197165	26.570292
206.115316	6362.715631	26.575309
206.114298	6387.476900	26.580327
206.477568	6393.812682	26.585344
206.689825	6393.183059	26.590362
206.645356	6416.530620	26.595380
206.895754	6418.095275	26.600397
207.374523	6423.099900	26.605415
207.540304	6426.252923	26.610432
207.741819	6437.058535	26.615450
207.683975	6449.946920	26.620468
208.219758	6451.053619	26.625485
208.450872	6467.028478	26.630503
208.605629	6461.009839	26.635520
209.138123	6479.819858	26.640538
209.195892	6487.083958	26.645556
209.565108	6490.520990	26.650573
209.497007	6492.918103	26.655591
209.574425	6504.292343	26.660608
209.613086	6510.426167	26.665626
209.851257	6516.566812	26.670644
210.281221	6527.886180	26.675661
210.464458	6536.974288	26.680679
210.837792	6528.973902	26.685696
210.788787	6544.285335	26.690714
210.863647	6556.929008	26.695732
211.199091	6553.713787	26.700749
211.205994	6571.614519	26.705767
211.319385	6582.683319	26.710784
211.704908	6601.415330	26.715802
211.896006	6614.886949	26.720820
212.451757	6611.365940	26.725837
212.414079	6636.098528	26.730855
212.267127	6639.874803	26.735872
212.615499	6642.885793	26.740890
212.797555	6660.970845	26.745908
213.162138	6668.771246	26.750925
213.417803	6680.348287	26.755943
213.822331	6686.314722	26.760960
213.791736	6694.315556	26.765978
213.914813	6707.826244	26.770996
214.240892	6702.396419	26.776013
214.291543	6724.968788	26.781031
214.572719	6733.429336	26.786048
214.785079	6738.598639	26.791066
214.941885	6753.726680	26.796084
215.367990	6760.810429	26.801101
215.288905	6775.119733	26.806119
215.677124	6787.408572	26.811136
215.775773	6800.165509	26.816154
216.133699	6813.592360	26.821172
216.306618	6821.517370	26.826189
216.597744	6828.047628	26.831207
217.080578	6839.939804	26.836224
217.336651	6845.367500	26.841242
217.193269	6858.247391	26.846260
217.651037	6863.391149	26.851277
217.873544	6877.356842	26.856295
217.512475	6878.237012	26.861312
218.203823	6883.271804	26.866330
218.164759	6906.284529	26.871348
218.651785	6910.227325	26.876365
218.793446	6929.562704	26.881383
218.765582	6939.157395	26.886400
218.978989	6944.165597	26.891418
219.154990	6968.385534	26.896436
219.328257	6976.689371	26.901453
219.532476	6997.937569	26.906471
219.724349	7007.308678	26.911488
220.135278	7021.885975	26.916506
220.082325	7031.828712	26.921524
220.635752	7047.760211	26.926541
220.922113	7064.475153	26.931559
221.285019	7071.811937	26.936576
221.435583	7078.048487	26.941594
221.666539	7089.882180	26.946612
222.361282	7096.068739	26.951629
222.390095	7098.807563	26.956647
222.952300	7093.347175	26.961664
222.855782	7103.167304	26.966682
222.939007	7122.186831	26.971700
223.370047	7122.217622	26.976717
223.633830	7144.962520	26.981735
223.773052	7143.305649	26.986752
223.972521	7147.331148	26.991770
224.190397	7152.184027	26.996788
224.393522	7166.433915	27.001805
224.806516	7173.264163	27.006823
225.019253	7170.004803	27.011840
225.242277	7179.532148	27.016858
225.222627	7199.214922	27.021876
225.789881	7193.510643	27.026893
225.948757	7195.749393	27.031911
226.027082	7220.508904	27.036928
226.189968	7216.865850	27.041946
226.181576	7225.368552	27.046964
226.427920	7227.609472	27.051981
226.969662	7240.641827	27.056999
227.039365	7243.724715	27.062016
227.438225	7260.229753	27.067034
227.354163	7270.581539	27.072052
227.698661	7265.997872	27.077069
227.665744	7282.702741	27.082087
227.514016	7288.948545	27.087104
228.275736	7306.009561	27.092122
228.353033	7317.643187	27.097140
228.511440	7322.963113	27.102157
228.844043	7337.256113	27.107175
229.606592	7332.351639	27.112192
229.801823	7332.034008	27.117210
230.179720	7337.010395	27.122228
230.321287	7336.448571	27.127245
230.749164	7348.400144	27.132263
230.684358	7343.548712	27.137280
230.711513	7341.265272	27.142298
230.617466	7350.412738	27.147316
231.251381	7355.990113	27.152333
231.689131	7362.955481	27.157351
231.686565	7367.290287	27.162368
232.067234	7374.643369	27.167386
231.977980	7392.168422	27.172404
232.255110	7390.168058	27.177421
232.641388	7386.518603	27.182439
232.383426	7408.255938	27.187456
233.123774	7415.916079	27.192474
233.200079	7421.839151	27.197492
233.317058	7435.597561	27.202509
233.628214	7433.986504	27.207527
233.675786	7452.462629	27.212544
234.088318	7461.329242	27.217562
234.275396	7466.632119	27.222580
234.149175	7486.016104	27.227597
234.716306	7496.222438	27.232615
235.013817	7506.293968	27.237632
235.252665	7520.769022	27.242650
235.599180	7531.000252	27.247668
235.627281	7550.780145	27.252685
235.559217	7542.175624	27.257703
235.998639	7568.915581	27.262720
236.512038	7568.112760	27.267738
236.598897	7584.155249	27.272756
236.976972	7597.358557	27.277773
237.283735	7597.487622	27.282791
237.409974	7614.546842	27.287808
237.529835	7618.695331	27.292826
237.502182	7631.071583	27.297844
237.932928	7642.877684	27.302861
238.313441	7647.787454	27.307879
238.344425	7665.439266	27.312896
238.667651	7667.721939	27.317914
238.939453	7695.858278	27.322932
239.138346	7695.508502	27.327949
239.459548	7719.593176	27.332967
239.883911	7731.984359	27.337984
240.043728	7740.492680	27.343002
240.143568	7756.669046	27.348020
240.199419	7755.170319	27.353037
240.653206	7770.953801	27.358055
240.558097	7781.361262	27.363072
240.807808	7796.368364	27.368090
240.971712	7812.743163	27.373108
241.439215	7824.625739	27.378125
241.612818	7836.790851	27.383143
241.802033	7852.593495	27.388160
242.058599	7863.732330	27.393178
243.023148	7876.273124	27.398196
242.928739	7882.497577	27.403213
242.989400	7895.763145	27.408231
243.145312	7910.159867	27.413248
243.693340	7923.336950	27.418266
244.083424	7932.440901	27.423284
244.224525	7935.399139	27.428301
244.725137	7947.595494	27.433319
244.689453	7963.840496	27.438336
244.851659	7958.382148	27.443354
245.000510	7981.130190	27.448372
245.278428	7994.488284	27.453389
245.109306	7990.795744	27.458407
245.561503	8009.995518	27.463424
245.500429	8013.711348	27.468442
245.845116	8034.481116	27.473460
245.893802	8044.749530	27.478477
246.331513	8058.063849	27.483495
246.565509	8076.925141	27.488512
246.889264	8085.237622	27.493530
246.965321	8109.420955	27.498548
247.531942	8119.226779	27.503565
247.907067	8129.605424	27.508583
248.108925	8150.293378	27.513600
247.966139	8153.595763	27.518618
248.814077	8176.765583	27.523636
248.318079	8186.020240	27.528653
248.859726	8196.590831	27.533671
249.338764	8215.385702	27.538688
249.913552	8232.400917	27.543706
250.215386	8241.146234	27.548724
250.554107	8255.044370	27.553741
250.248618	8255.647602	27.558759
250.336572	8271.652635	27.563776
250.430741	8283.997731	27.568794
251.205039	8284.429699	27.573812
251.466973	8310.311245	27.578829
251.814286	8323.497765	27.583847
252.134232	8338.162887	27.588864
252.147943	8341.598793	27.593882
252.657154	8357.601457	27.598900
252.525184	8368.567467	27.603917
253.293919	8373.085503	27.608935
253.043265	8398.118808	27.613952
253.442118	8398.066221	27.618970
253.726315	8410.227121	27.623988
253.930634	8421.087137	27.629005
254.373727	8429.021291	27.634023
254.623672	8456.003559	27.639040
254.356693	8464.701787	27.644058
254.646929	8473.559517	27.649076
254.882269	8490.608876	27.654093
255.050918	8508.429485	27.659111
255.357429	8520.672225	27.664128
256.077194	8544.010845	27.669146
256.262682	8552.967005	27.674164
256.450020	8576.619024	27.679181
257.109969	8573.936992	27.684199
257.151147	8595.591268	27.689216
257.294926	8599.414234	27.694234
258.189574	8611.385516	27.699252
258.140934	8625.947240	27.704269
258.573100	8626.025221	27.709287
258.625126	8633.256335	27.714304
258.811074	8632.955915	27.719322
259.381451	8653.075613	27.724340
259.501878	8656.548633	27.729357
259.894180	8663.209022	27.734375
259.938988	8669.689888	27.739392
260.012383	8671.187585	27.744410
260.370673	8679.564414	27.749428
260.356974	8687.342487	27.754445
261.087896	8704.021279	27.759463
261.399980	8711.982267	27.764480
261.460210	8720.989580	27.769498
261.539123	8734.552833	27.774516
261.582046	8745.232956	27.779533
262.081575	8746.642216	27.784551
262.067262	8763.989578	27.789568
262.498773	8770.956454	27.794586
262.847930	8781.993030	27.799604
262.946429	8800.238423	27.804621
263.207220	8808.545248	27.809639
263.592137	8822.717603	27.814656
263.612920	8836.823532	27.819674
263.710597	8836.391624	27.824692
264.035230	8856.268821	27.829709
264.303312	8867.539069	27.834727
264.414686	8889.766827	27.839744
264.298350	8901.321100	27.844762
264.798586	8916.943636	27.849780
264.784415	8932.081145	27.854797
265.272483	8951.080575	27.859815
265.620491	8971.699339	27.864832
266.055477	8989.273733	27.869850
266.326641	9013.636245	27.874868
266.333601	9029.935530	27.879885
266.836095	9034.848783	27.884903
267.565016	9057.934058	27.889920
267.595798	9077.497326	27.894938
268.158889	9083.793462	27.899956
268.405713	9104.222912	27.904973
268.394460	9108.603680	27.909991
268.383749	9123.238819	27.915008
268.934384	9140.334406	27.920026
269.143722	9152.526394	27.925044
269.484568	9173.364342	27.930061
270.012755	9178.677752	27.935079
270.458829	9202.116644	27.940096
270.499226	9209.084592	27.945114
271.185565	9220.245738	27.950132
271.275577	9231.515516	27.955149
271.905286	9237.649789	27.960167
272.492152	9256.529965	27.965184
272.026391	9259.949130	27.970202
272.160228	9252.663652	27.975220
272.453202	9271.927417	27.980237
272.670630	9289.551753	27.985255
272.960917	9302.428976	27.990272
273.522729	9306.821602	27.995290
273.437136	9324.477362	28.000308
273.743908	9337.326785	28.005325
274.062657	9348.898844	28.010343
274.181886	9355.857731	28.015360
274.365109	9372.161447	28.020378
274.905281	9379.200039	28.025396
275.237243	9405.207976	28.030413
275.361563	9413.751010	28.035431
276.232477	9424.160543	28.040448
276.063295	9432.083109	28.045466
276.727835	9437.255391	28.050484
276.590410	9451.184357	28.055501
277.127970	9457.898192	28.060519
277.342821	9471.917562	28.065536
277.393602	9480.794112	28.070554
277.849221	9488.603643	28.075572
278.269423	9497.296399	28.080589
278.329223	9508.031165	28.085607
278.930709	9524.238325	28.090624
278.815955	9529.402512	28.095642
279.463520	9538.381928	28.100660
279.492950	9552.524942	28.105677
279.678901	9555.681679	28.110695
279.945534	9567.969210	28.115712
280.169820	9583.234302	28.120730
280.520516	9598.318708	28.125748
280.707289	9605.396620	28.130765
280.615569	9613.477694	28.135783
281.190813	9628.489279	28.140800
281.690776	9635.979401	28.145818
281.761714	9647.757562	28.150836
282.181009	9664.700434	28.155853
282.259300	9671.612139	28.160871
282.635868	9676.033695	28.165888
283.131303	9691.730251	28.170906
283.555715	9690.316065	28.175924
283.660029	9704.655916	28.180941
283.816958	9705.752350	28.185959
284.435107	9719.687018	28.190976
284.709527	9733.741513	28.195994
285.057259	9733.807390	28.201012
285.007532	9752.240974	28.206029
284.834487	9754.825339	28.211047
285.655302	9770.322914	28.216064
285.569777	9795.960693	28.221082
285.965483	9796.347458	28.226100
285.990123	9814.513787	28.231117
286.282070	9825.392559	28.236135
286.580079	9840.409590	28.241152
287.365612	9863.805944	28.246170
287.672157	9873.946824	28.251188
288.047434	9886.321842	28.256205
287.896066	9895.817319	28.261223
288.068668	9907.077807	28.266240
288.089483	9927.758048	28.271258
288.831426	9935.447417	28.276276
289.353726	9959.058524	28.281293
289.798732	9966.330011	28.286311
290.319251	9981.956605	28.291328
290.131145	9992.831280	28.296346
290.477205	9996.689347	28.301364
290.898361	10009.736126	28.306381
291.072552	10027.449986	28.311399
291.654657	10039.499275	28.316416
291.440891	10056.979932	28.321434
291.988130	10073.300211	28.326452
292.331305	10085.288852	28.331469
292.380773	10104.714528	28.336487
292.721199	10107.869411	28.341504
293.077178	10123.559629	28.346522
293.234343	10130.617093	28.351540
293.028665	10151.601217	28.356557
293.319787	10168.217198	28.361575
294.070365	10188.200007	28.366592
293.997518	10206.874441	28.371610
294.704639	10212.798077	28.376628
294.999290	10250.602541	28.381645
294.999958	10264.728473	28.386663
295.376352	10274.255643	28.391680
295.509936	10297.245709	28.396698
296.056313	10313.815765	28.401716
296.077463	10332.974555	28.406733
296.335870	10348.497026	28.411751
297.110121	10364.801164	28.416768
297.305875	10393.957490	28.421786
297.807855	10396.427380	28.426804
298.014257	10410.919223	28.431821
298.360876	10426.952151	28.436839
298.819921	10435.070973	28.441856
299.241548	10441.007556	28.446874
299.378535	10450.351072	28.451892
300.248252	10469.153718	28.456909
299.958135	10474.152867	28.461927
300.601728	10483.303861	28.466944
300.827799	10497.189648	28.471962
301.132657	10497.056974	28.476980
301.226210	10509.618351	28.481997
301.250313	10526.936119	28.487015
301.593430	10528.590891	28.492032
301.772933	10548.966108	28.497050
302.292064	10556.523083	28.502068
302.317430	10572.814540	28.507085
301.920649	10586.604760	28.512103
302.728414	10594.334676	28.517120
302.609084	10631.942299	28.522138
302.944553	10650.395737	28.527156
303.428682	10666.562178	28.532173
303.708745	10699.340050	28.537191
303.950661	10709.996636	28.542208
304.147282	10732.513283	28.547226
304.571439	10753.952579	28.552244
304.965939	10777.584623	28.557261
305.198193	10801.365097	28.562279
305.822241	10817.336225	28.567296
306.118485	10844.289499	28.572314
305.907090	10858.707807	28.577332
306.726706	10877.644965	28.582349
306.968920	10902.690158	28.587367
307.675559	10925.294981	28.592384
308.137278	10941.588290	28.597402
308.144346	10957.677696	28.602420
308.258896	10968.903660	28.607437
308.449220	10995.036911	28.612455
309.012683	11007.250764	28.617472
309.326460	11028.246568	28.622490
309.645762	11046.109308	28.627508
310.018904	11064.124715	28.632525
310.238174	11093.774199	28.637543
310.906025	11100.695689	28.642560
310.960961	11121.179333	28.647578
311.101829	11143.316782	28.652596
311.851799	11143.477921	28.657613
311.903743	11176.794188	28.662631
312.478756	11186.897146	28.667648
312.650144	11204.053680	28.672666
312.787169	11223.182712	28.677684
312.958219	11232.243455	28.682701
313.363318	11247.124963	28.687719
313.864908	11264.580630	28.692736
313.989895	11286.177627	28.697754
314.398660	11302.931023	28.702772
314.993910	11323.712831	28.707789
315.214826	11341.095437	28.712807
315.604382	11351.126316	28.717824
316.286444	11365.393285	28.722842
316.357833	11394.270568	28.727860
316.750406	11393.135923	28.732877
317.038133	11412.554284	28.737895
317.602725	11415.500828	28.742912
317.481279	11439.567680	28.747930
317.874691	11453.235515	28.752948
318.128165	11459.214392	28.757965
318.363967	11470.797529	28.762983
319.081323	11486.817857	28.768000
319.030885	11499.383371	28.773018
319.319453	11517.125044	28.778036
319.388786	11530.859177	28.783053
319.489184	11572.116204	28.788071
319.729189	11579.574962	28.793088
319.673110	11602.353028	28.798106
320.097130	11621.785120	28.803124
320.557267	11647.940429	28.808141
320.770084	11673.831149	28.813159
321.187414	11694.025338	28.818176
321.806942	11715.078513	28.823194
322.488475	11733.659128	28.828212
323.269471	11725.349916	28.833229
323.607886	11740.554802	28.838247
323.923411	11736.492404	28.843264
324.346784	11743.329050	28.848282
324.271463	11761.582301	28.853300
324.874890	11758.583397	28.858317
324.640098	11779.314953	28.863335
325.416416	11794.928508	28.868352
325.505267	11805.792692	28.873370
325.298037	11828.957690	28.878388
325.926183	11841.146233	28.883405
325.781597	11868.687462	28.888423
326.203099	11883.769012	28.893440
326.553125	11896.089303	28.898458
327.048085	11927.519139	28.903476
327.437394	11943.657242	28.908493
327.679205	11966.569358	28.913511
328.063213	11985.821757	28.918528
328.270212	12000.257902	28.923546
328.287634	12018.108573	28.928564
329.261919	12048.652472	28.933581
329.255457	12063.131371	28.938599
329.261619	12083.604713	28.943616
330.036917	12106.219223	28.948634
329.831570	12138.017366	28.953652
330.481864	12155.583337	28.958669
330.974971	12183.894110	28.963687
331.380913	12201.018198	28.968704
331.941783	12222.409474	28.973722
332.022695	12243.379740	28.978740
332.445135	12257.469931	28.983757
332.901168	12270.923364	28.988775
333.506537	12286.563945	28.993792
334.174256	12297.979305	28.998810
334.347631	12321.047762	29.003828
334.821997	12323.307490	29.008845
334.988455	12347.798022	29.013863
335.324611	12356.435734	29.018880
335.940799	12364.363576	29.023898
335.928458	12384.394889	29.028916
336.367594	12394.854374	29.033933
336.620406	12413.761343	29.038951
336.158220	12425.336900	29.043968
336.814779	12443.041105	29.048986
337.253974	12473.716369	29.054004
337.925652	12490.079389	29.059021
338.047270	12504.753413	29.064039
338.333699	12526.190920	29.069056
338.487860	12542.542980	29.074074
338.995701	12575.238147	29.079092
339.266041	12592.266867	29.084109
339.477794	12604.710199	29.089127
339.630096	12631.202158	29.094144
340.321733	12656.024995	29.099162
340.388490	12673.003381	29.104180
340.897959	12686.189857	29.109197
341.343550	12715.860351	29.114215
341.536979	12728.578185	29.119232
342.179037	12745.792322	29.124250
342.682411	12775.245501	29.129268
343.275082	12770.763960	29.134285
343.431250	12785.464401	29.139303
343.858400	12797.890116	29.144320
344.090061	12812.897762	29.149338
343.826072	12834.200266	29.154356
344.637812	12840.758965	29.159373
344.899157	12858.888237	29.164391
345.296898	12874.927937	29.169408
345.363608	12886.010922	29.174426
345.798512	12906.689980	29.179444
346.074646	12918.356151	29.184461
345.865833	12934.370335	29.189479
346.466973	12953.416243	29.194496
346.633779	12981.943224	29.199514
346.845712	13007.096989	29.204532
347.551965	13027.992878	29.209549
347.944595	13042.710390	29.214567
347.848473	13069.377426	29.219584
348.435236	13092.581414	29.224602
348.633083	13124.084768	29.229620
349.159979	13146.117110	29.234637
349.652815	13170.362114	29.239655
350.182816	13180.627894	29.244672
350.763172	13201.679363	29.249690
350.891101	13222.794975	29.254708
351.361724	13237.118397	29.259725
351.490579	13261.091766	29.264743
351.863924	13280.795567	29.269760
352.336224	13306.963923	29.274778
352.482903	13328.888306	29.279796
352.822059	13341.005976	29.284813
353.400618	13370.590484	29.289831
353.523365	13388.163951	29.294848
354.030600	13406.744939	29.299866
354.254889	13442.943638	29.304884
354.727596	13460.178478	29.309901
355.040685	13484.205553	29.314919
355.303425	13502.354173	29.319936
356.275928	13520.910209	29.324954
356.879213	13547.074295	29.329972
357.163807	13560.899555	29.334989
357.157104	13579.071249	29.340007
358.026596	13589.015977	29.345024
358.269444	13602.017234	29.350042
358.183592	13617.766535	29.355060
358.634398	13630.457540	29.360077
359.150647	13647.303665	29.365095
359.184001	13661.976540	29.370112
359.893205	13682.629536	29.375130
360.069414	13696.654928	29.380148
360.393632	13713.208899	29.385165
360.707380	13736.790923	29.390183
361.182784	13744.384423	29.395200
361.890916	13752.642756	29.400218
362.228940	13773.906278	29.405236
362.673232	13781.239369	29.410253
362.922917	13806.473586	29.415271
363.374239	13815.801420	29.420288
363.941149	13834.720914	29.425306
364.203450	13840.506542	29.430324
364.380061	13852.880378	29.435341
364.604006	13869.889052	29.440359
364.838740	13894.213063	29.445376
364.999976	13899.884967	29.450394
365.426238	13925.098168	29.455412
365.949896	13942.145512	29.460429
366.144653	13968.525366	29.465447
366.159037	13991.393242	29.470464
366.836811	14011.609374	29.475482
367.302183	14029.666952	29.480500
367.392698	14058.646393	29.485517
367.596748	14077.357350	29.490535
367.956097	14095.371495	29.495552
368.723079	14114.607503	29.500570
368.469552	14136.320379	29.505588
369.261273	14150.171333	29.510605
369.685362	14173.544085	29.515623
369.940119	14202.779239	29.520640
370.169848	14214.870294	29.525658
370.431101	14243.741328	29.530676
370.874356	14258.751919	29.535693
371.459646	14285.901975	29.540711
371.255315	14308.952711	29.545728
371.944185	14327.560015	29.550746
372.205501	14351.817313	29.555764
372.776931	14371.595628	29.560781
372.952589	14397.877995	29.565799
373.188086	14426.475408	29.570816
374.081777	14438.251648	29.575834
374.690282	14459.445408	29.580852
375.069126	14472.953487	29.585869
375.313673	14498.012572	29.590887
375.654314	14525.434756	29.595904
376.105444	14531.781757	29.600922
376.136232	14567.005302	29.605940
376.600798	14592.927153	29.610957
377.211565	14602.549519	29.615975
377.655276	14623.955445	29.620992
377.730373	14638.622577	29.626010
378.322463	14670.196606	29.631028
378.491742	14689.554672	29.636045
379.158346	14715.078897	29.641063
379.466586	14731.977320	29.646080
380.077956	14755.394269	29.651098
379.879603	14791.724501	29.656116
380.319485	14804.538003	29.661133
381.109686	14823.025801	29.666151
381.326618	14848.964446	29.671168
381.817120	14865.635652	29.676186
382.254379	14903.607270	29.681204
382.682504	14919.823989	29.686221
383.266360	14934.721641	29.691239
383.331775	14962.765242	29.696256
383.852424	14981.863625	29.701274
383.958006	15009.408370	29.706292
384.257510	15027.101111	29.711309
385.016412	15053.640979	29.716327
385.105977	15069.556820	29.721344
385.824494	15088.690827	29.726362
386.084839	15114.929417	29.731380
386.223522	15139.203654	29.736397
386.789781	15159.135187	29.741415
386.779209	15182.905300	29.746432
387.697863	15200.751308	29.751450
387.748249	15228.248116	29.756468
388.275866	15256.551801	29.761485
388.895388	15274.851855	29.766503
388.995282	15309.927052	29.771520
389.502192	15327.641473	29.776538
389.860341	15347.924581	29.781556
390.072244	15381.589705	29.786573
390.678525	15386.785359	29.791591
390.963193	15415.765062	29.796608
391.719550	15432.894375	29.801626
392.386442	15460.718740	29.806644
392.576608	15481.138680	29.811661
393.112538	15479.788834	29.816679
393.026111	15511.428835	29.821696
393.771471	15514.395268	29.826714
393.891206	15537.832871	29.831732
394.305142	15557.011610	29.836749
394.681704	15573.451673	29.841767
394.841928	15595.540791	29.846784
395.155099	15620.183255	29.851802
395.805009	15641.968797	29.856820
395.922976	15664.664641	29.861837
396.244908	15673.928263	29.866855
396.406644	15707.766001	29.871872
396.841972	15731.262090	29.876890
397.392836	15752.295719	29.881908
397.419526	15782.882644	29.886925
397.826517	15803.550260	29.891943
398.307483	15839.378781	29.896960
398.916168	15860.798314	29.901978
399.359765	15887.461072	29.906996
399.493700	15920.823454	29.912013
400.270864	15945.855214	29.917031
400.311977	15977.564561	29.922048
401.115993	15995.561812	29.927066
401.316093	16027.814987	29.932084
402.138210	16049.649985	29.937101
402.486428	16069.723800	29.942119
402.806783	16089.656690	29.947136
403.420677	16109.891318	29.952154
404.279058	16130.924865	29.957172
404.433023	16156.774023	29.962189
404.915994	16174.284506	29.967207
405.015276	16193.263360	29.972224
405.433070	16208.200496	29.977242
406.041198	16240.197847	29.982260
406.219953	16260.993082	29.987277
406.698316	16281.950148	29.992295
407.187848	16303.477161	29.997312
407.715568	16319.913285	30.002330
408.036294	16349.397286	30.007348
408.516300	16379.064988	30.012365
409.188568	16385.555055	30.017383
409.299872	16418.170132	30.022400
409.509245	16437.890100	30.027418
410.034800	16458.669460	30.032436
410.365310	16483.149258	30.037453
410.928492	16488.190848	30.042471
411.006065	16518.057227	30.047488
411.597227	16532.860241	30.052506
412.027660	16553.588186	30.057524
412.134112	16587.777191	30.062541
413.177641	16609.793133	30.067559
413.234906	16625.475257	30.072576
414.011051	16656.512255	30.077594
414.178132	16674.770386	30.082612
414.101600	16696.022747	30.087629
414.860111	16718.879110	30.092647
415.604584	16739.845784	30.097664
416.304314	16762.534478	30.102682
416.655967	16789.279133	30.107700
416.724821	16802.979254	30.112717
417.226840	16809.859192	30.117735
418.433940	16830.400197	30.122752
418.989513	16837.647662	30.127770
419.535491	16854.457259	30.132788
419.469466	16868.178425	30.137805
419.938906	16873.225237	30.142823
420.035590	16886.501010	30.147840
420.071934	16913.414947	30.152858
420.286778	16930.351965	30.157876
420.806615	16954.278584	30.162893
421.379296	16977.634798	30.167911
421.894299	16992.181555	30.172928
422.100376	17011.457281	30.177946
422.700853	17037.244427	30.182964
422.700244	17048.153963	30.187981
423.279774	17066.171380	30.192999
423.110981	17089.542092	30.198016
423.755160	17110.995401	30.203034
424.122433	17138.426663	30.208052
424.582549	17164.071590	30.213069
425.070793	17190.621821	30.218087
425.075475	17219.208807	30.223104
425.952904	17247.303054	30.228122
426.563907	17273.256280	30.233140
426.631523	17307.209403	30.238157
427.059484	17329.953711	30.243175
427.325153	17352.300069	30.248192
427.763974	17375.592326	30.253210
428.481076	17407.088243	30.258228
428.645127	17425.865560	30.263245
429.057794	17465.077919	30.268263
429.860002	17488.222142	30.273280
430.309172	17508.382819	30.278298
430.717693	17543.262439	30.283316
430.851799	17576.119137	30.288333
431.555753	17599.894712	30.293351
431.959003	17625.839695	30.298368
432.310501	17656.593818	30.303386
432.489749	17677.311542	30.308404
433.086300	17719.796516	30.313421
433.618551	17751.722916	30.318439
434.381239	17780.726530	30.323456
434.834694	17811.395537	30.328474
435.211524	17831.533070	30.333492
435.461878	17864.836477	30.338509
435.858730	17880.043499	30.343527
436.290013	17905.820247	30.348544
436.387387	17939.570854	30.353562
436.769279	17971.855841	30.358580
437.496800	18018.124080	30.363597
437.910093	18041.351625	30.368615
438.646892	18069.500552	30.373632
439.056464	18110.878380	30.378650
439.575506	18132.434435	30.383668
439.748441	18161.081903	30.388685
440.669328	18176.049644	30.393703
441.457218	18202.453543	30.398720
441.681236	18232.565107	30.403738
442.229215	18260.276223	30.408756
442.797644	18284.774970	30.413773
443.018837	18304.482374	30.418791
443.407273	18329.274528	30.423808
443.640721	18355.303782	30.428826
444.406107	18369.360907	30.433844
444.725277	18395.661153	30.438861
444.854997	18412.262108	30.443879
445.486131	18444.540669	30.448896
445.603207	18473.797451	30.453914
446.503511	18503.867327	30.458932
446.510783	18540.336875	30.463949
446.897984	18564.188221	30.468967
447.249193	18598.791222	30.473984
447.453654	18634.844883	30.479002
448.285121	18657.654288	30.484020
448.548399	18697.261975	30.489037
449.275925	18717.491137	30.494055
449.965592	18748.996674	30.499072
450.268633	18781.882817	30.504090
451.128738	18799.899240	30.509108
451.342390	18827.429467	30.514125
451.752449	18851.618756	30.519143
452.194555	18862.889986	30.524160
452.915750	18881.250307	30.529178
453.488216	18895.811668	30.534196
454.207221	18915.777026	30.539213
454.579684	18920.318277	30.544231
455.047646	18926.354564	30.549248
455.116513	18941.986220	30.554266
455.631606	18955.040336	30.559284
456.417344	18981.590940	30.564301
456.571881	18999.534182	30.569319
456.917727	19019.848351	30.574336
457.386722	19042.885216	30.579354
457.875266	19065.799030	30.584372
457.974573	19086.928718	30.589389
458.721306	19124.061312	30.594407
458.980974	19136.447739	30.599424
459.404255	19168.058605	30.604442
459.710098	19193.231146	30.609460
460.022892	19216.279899	30.614477
460.255613	19239.309556	30.619495
460.912257	19271.206461	30.624512
461.302670	19306.038375	30.629530
462.112277	19332.434118	30.634548
461.934747	19364.006164	30.639565
462.408675	19408.680911	30.644583
463.222286	19437.356878	30.649600
463.274365	19474.579331	30.654618
463.666973	19510.384203	30.659636
464.384004	19552.791261	30.664653
464.703735	19577.614660	30.669671
465.675188	19613.961388	30.674688
466.012390	19650.526962	30.679706
466.726671	19678.536423	30.684724
467.176902	19704.464240	30.689741
467.659452	19723.999722	30.694759
467.954010	19762.347458	30.699776
468.139468	19799.410773	30.704794
468.895898	19821.298187	30.709812
469.511333	19865.010587	30.714829
470.209005	19885.365656	30.719847
470.749514	19922.190712	30.724864
471.101717	19951.684781	30.729882
471.343116	19982.870395	30.734900
472.109781	20015.579040	30.739917
472.400240	20043.509695	30.744935
473.110069	20075.121649	30.749952
473.609133	20098.489934	30.754970
474.186652	20114.207611	30.759988
474.793986	20155.312603	30.765005
475.264307	20184.782318	30.770023
475.636150	20205.637024	30.775040
475.952635	20235.490890	30.780058
476.017575	20249.784788	30.785076
476.508373	20275.997678	30.790093
476.852016	20314.711619	30.795111
477.451752	20343.618076	30.800128
477.641605	20378.122998	30.805146
478.571094	20413.947035	30.810164
478.792679	20441.307718	30.815181
479.652900	20468.133070	30.820199
480.408810	20498.222197	30.825216
480.783329	20523.809076	30.830234
481.158637	20553.174094	30.835252
481.800960	20583.236807	30.840269
482.265287	20618.520778	30.845287
482.389356	20637.910803	30.850304
482.824741	20665.339606	30.855322
483.802688	20691.243443	30.860340
484.204847	20711.032519	30.865357
484.754720	20739.492416	30.870375
485.301630	20755.676602	30.875392
485.297772	20784.222768	30.880410
486.034244	20799.265479	30.885428
486.425940	20822.215390	30.890445
487.043718	20848.080733	30.895463
487.805511	20858.538851	30.900480
488.107936	20892.357424	30.905498
488.660855	20902.753310	30.910516
489.084031	20934.070096	30.915533
489.551321	20948.687279	30.920551
489.951172	20976.330551	30.925568
490.208957	20995.567430	30.930586
490.949833	21022.829129	30.935604
491.008854	21051.542806	30.940621
491.435558	21081.595624	30.945639
492.151336	21106.807907	30.950656
492.704091	21137.258194	30.955674
493.044515	21164.696161	30.960692
493.753718	21194.502988	30.965709
493.904680	21223.088873	30.970727
494.823808	21245.742347	30.975744
495.254691	21284.589945	30.980762
495.733592	21306.642280	30.985780
496.538118	21334.930713	30.990797
496.736601	21365.923021	30.995815
497.150711	21392.705362	31.000832
497.223166	21430.749748	31.005850
497.860495	21459.133891	31.010868
498.605672	21502.697065	31.015885
498.852894	21545.655465	31.020903
499.659864	21572.509578	31.025920
500.040561	21598.027394	31.030938
500.433744	21641.835227	31.035956
501.580687	21665.749006	31.040973
501.689080	21705.810237	31.045991
502.140476	21735.575880	31.051008
502.367747	21765.117401	31.056026
503.091455	21803.465505	31.061044
503.406262	21838.269464	31.066061
504.037742	21871.754161	31.071079
504.076268	21910.626164	31.076096
504.303177	21952.034250	31.081114
504.908707	21984.524847	31.086132
505.972537	22024.368480	31.091149
506.428103	22062.518726	31.096167
507.157289	22092.298529	31.101184
507.599395	22126.963127	31.106202
508.130563	22156.988689	31.111220
508.813489	22185.063487	31.116237
509.481241	22229.783995	31.121255
510.348122	22254.708845	31.126272
510.316386	22294.034846	31.131290
510.763259	22315.966925	31.136308
511.284735	22343.334117	31.141325
511.727636	22378.997385	31.146343
512.718199	22412.098528	31.151360
513.402852	22446.605872	31.156378
513.914361	22472.932208	31.161396
514.480627	22495.983271	31.166413
514.557945	22528.386388	31.171431
515.349258	22553.279149	31.176448
515.488252	22585.274677	31.181466
515.573865	22621.651155	31.186484
516.588001	22648.556630	31.191501
517.086389	22672.654746	31.196519
517.970059	22694.272813	31.201536
518.114239	22725.111421	31.206554
518.732348	22741.955954	31.211572
518.984110	22764.752988	31.216589
519.696353	22797.032427	31.221607
519.964039	22831.036661	31.226624
520.264153	22858.230506	31.231642
520.722961	22904.533186	31.236660
521.140167	22927.803842	31.241677
521.653287	22965.302346	31.246695
521.833101	22995.560808	31.251712
522.922622	23039.478178	31.256730
523.138655	23078.697655	31.261748
523.617212	23114.647368	31.266765
524.203692	23161.158253	31.271783
524.298796	23193.129999	31.276800
524.463563	23237.210726	31.281818
525.084554	23276.822518	31.286836
525.770123	23314.515999	31.291853
526.474679	23372.288400	31.296871
527.308670	23418.597062	31.301888
527.586426	23451.975208	31.306906
528.110778	23504.316400	31.311924
529.056662	23549.622176	31.316941
529.498572	23587.783806	31.321959
530.502060	23622.641667	31.326976
531.065433	23651.792448	31.331994
531.746428	23682.827013	31.337012
532.405813	23717.245719	31.342029
532.841506	23754.574512	31.347047
533.492204	23781.525470	31.352064
534.097495	23805.045917	31.357082
535.050947	23842.559677	31.362100
535.907211	23851.039431	31.367117
536.131265	23879.175432	31.372135
536.739488	23907.984691	31.377152
537.389603	23923.706754	31.382170
537.598104	23948.249658	31.387188
538.175270	23978.561503	31.392205
538.340309	24017.841324	31.397223
538.838311	24043.470416	31.402240
539.585458	24084.068934	31.407258
539.915787	24107.449286	31.412276
540.549642	24132.577081	31.417293
540.775789	24182.887448	31.422311
541.756907	24201.553535	31.427328
541.881112	24228.466995	31.432346
542.551097	24282.885565	31.437364
543.533880	24309.166250	31.442381
543.681056	24342.837947	31.447399
544.386515	24366.811095	31.452416
544.827829	24401.524026	31.457434
545.466300	24428.806370	31.462452
545.954121	24448.914462	31.467469
546.521427	24502.641849	31.472487
546.784130	24532.125098	31.477504
547.341822	24571.452311	31.482522
547.606983	24612.089021	31.487540
548.539893	24637.910269	31.492557
549.220795	24672.472623	31.497575
549.767033	24696.376163	31.502592
550.372925	24727.367173	31.507610
550.814365	24763.357240	31.512628
551.971882	24787.089894	31.517645
552.547332	24820.923225	31.522663
553.128685	24842.312645	31.527680
553.374963	24872.317150	31.532698
553.628381	24907.749035	31.537716
554.052995	24933.276945	31.542733
554.605867	24958.721725	31.547751
555.013630	24986.249291	31.552768
555.691718	25026.057898	31.557786
556.006519	25055.059843	31.562804
556.179765	25083.957475	31.567821
556.612188	25133.296507	31.572839
557.136325	25151.743928	31.577856
557.963966	25198.816065	31.582874
558.270937	25237.273597	31.587892
558.854563	25269.577071	31.592909
559.278892	25314.121225	31.597927
559.798804	25350.245481	31.602944
560.517103	25403.503085	31.607962
560.539973	25443.085899	31.612980
561.613681	25481.803718	31.617997
562.189134	25525.547494	31.623015
562.806346	25571.471482	31.628032
563.453058	25611.317734	31.633050
563.980242	25663.986449	31.638068
564.496544	25684.432616	31.643085
565.325906	25742.268280	31.648103
565.763627	25785.768634	31.653120
566.467176	25818.654702	31.658138
567.191313	25861.788324	31.663156
567.921592	25897.786020	31.668173
568.436819	25932.831367	31.673191
568.722496	25972.134155	31.678208
570.097041	26009.592754	31.683226
570.628120	26047.012092	31.688244
571.433083	26068.216335	31.693261
572.107536	26095.703906	31.698279
572.951002	26123.045126	31.703296
573.550019	26146.082677	31.708314
573.905905	26179.320492	31.713332
574.519619	26204.681544	31.718349
574.965363	26233.892323	31.723367
575.385896	26264.465852	31.728384
575.897704	26289.463679	31.733402
576.104245	26322.516422	31.738420
576.986941	26349.207209	31.743437
577.351036	26388.536523	31.748455
578.044262	26427.157398	31.753472
578.701536	26464.197629	31.758490
579.585813	26497.606512	31.763508
580.081667	26517.468951	31.768525
580.309707	26558.526176	31.773543
580.873224	26593.261794	31.778560
581.453548	26623.311710	31.783578
581.809575	26662.939856	31.788596
582.370297	26694.275898	31.793613
582.994611	26745.415506	31.798631
583.355017	26772.434645	31.803648
584.291785	26811.252186	31.808666
584.642388	26855.526823	31.813684
585.284743	26886.882056	31.818701
586.288174	26924.166289	31.823719
586.678286	26968.921673	31.828736
587.520593	26994.854867	31.833754
587.952247	27035.167186	31.838772
588.566322	27067.184399	31.843789
588.901415	27105.641119	31.848807
589.601095	27136.368438	31.853824
590.360874	27176.535155	31.858842
590.559397	27208.516160	31.863860
591.526240	27232.679573	31.868877
592.213663	27271.442012	31.873895
592.705108	27310.260315	31.878912
593.122799	27335.027600	31.883930
593.502253	27372.416117	31.888948
594.099004	27406.332645	31.893965
594.650433	27437.045578	31.898983
595.055649	27470.271517	31.904000
595.824960	27516.062490	31.909018
596.171802	27554.189575	31.914036
596.571479	27599.785466	31.919053
596.954374	27636.093156	31.924071
597.118003	27677.876876	31.929088
598.016008	27729.861215	31.934106
598.608539	27782.746494	31.939124
599.096106	27816.282519	31.944141
599.943231	27870.620009	31.949159
600.431983	27922.365169	31.954176
601.388706	27960.657213	31.959194
601.962054	28014.216048	31.964212
602.553871	28057.412880	31.969229
603.203494	28105.214765	31.974247
603.639365	28151.097000	31.979264
604.465673	28187.109108	31.984282
604.930341	28238.188846	31.989300
605.701141	28283.014273	31.994317
606.654262	28322.135552	31.999335
606.840350	28369.378161	32.004352
607.755787	28406.305907	32.009370
608.094861	28459.586354	32.014388
609.160830	28499.328787	32.019405
610.290002	28535.894823	32.024423
610.626801	28585.592158	32.029440
611.314570	28620.160210	32.034458
611.701937	28653.156995	32.039476
612.252927	28689.781713	32.044493
612.930979	28727.081991	32.049511
613.474807	28771.393927	32.054528
614.396525	28806.109176	32.059546
615.084689	28859.203587	32.064564
615.344734	28893.130766	32.069581
616.143699	28924.787126	32.074599
616.319027	28974.712808	32.079616
616.903688	29015.169571	32.084634
617.535294	29065.890391	32.089652
618.372654	29098.565012	32.094669
618.994532	29151.392386	32.099687
619.723717	29197.913962	32.104704
620.166092	29236.655085	32.109722
620.663042	29279.186620	32.114740
621.047460	29318.120224	32.119757
621.805966	29365.806978	32.124775
622.510677	29429.152771	32.129792
622.816243	29471.069765	32.134810
623.430080	29519.651685	32.139828
624.159148	29571.584846	32.144845
625.154315	29618.742314	32.149863
625.816193	29663.625654	32.154880
626.851768	29702.420695	32.159898
627.385644	29749.359508	32.164916
628.526197	29783.315435	32.169933
628.858458	29817.296112	32.174951
629.210750	29858.580843	32.179968
630.274933	29901.493124	32.184986
630.673996	29942.682248	32.190004
630.914052	29982.771057	32.195021
631.500850	30012.831293	32.200039
632.233144	30068.020567	32.205056
633.046321	30103.545053	32.210074
633.658194	30148.835470	32.215092
634.263170	30186.706043	32.220109
634.760129	30213.221758	32.225127
635.391891	30256.467585	32.230144
635.896313	30286.066958	32.235162
636.634614	30327.134510	32.240180
636.637838	30359.106599	32.245197
637.503889	30404.440185	32.250215
638.259158	30449.949147	32.255232
638.926466	30489.852329	32.260250
639.602829	30534.798530	32.265268
639.909314	30586.294341	32.270285
640.641766	30617.660252	32.275303
641.137055	30669.196413	32.280320
642.136486	30712.720990	32.285338
642.686587	30758.806205	32.290356
643.251862	30795.337639	32.295373
644.411721	30841.669469	32.300391
644.768480	30880.509195	32.305408
645.564829	30912.289139	32.310426
646.056926	30964.022495	32.315444
646.622095	31013.430976	32.320461
647.631007	31056.057166	32.325479
647.851807	31113.699393	32.330496
648.713597	31156.942907	32.335514
649.198535	31205.005228	32.340532
649.507532	31254.511057	32.345549
650.705248	31298.081861	32.350567
651.336789	31336.734274	32.355584
652.164827	31375.495244	32.360602
652.588808	31424.389359	32.365620
653.368988	31469.068572	32.370637
654.246438	31512.765544	32.375655
654.836470	31559.010687	32.380672
655.712059	31601.513361	32.385690
656.470244	31635.550838	32.390708
656.826453	31679.183908	32.395725
657.712434	31717.854319	32.400743
658.017788	31768.461902	32.405760
659.209335	31804.328680	32.410778
659.949718	31840.133000	32.415796
660.137011	31887.440390	32.420813
661.070053	31913.903048	32.425831
661.616194	31963.519052	32.430848
661.922306	32004.050337	32.435866
662.686641	32061.205995	32.440884
663.418463	32098.725278	32.445901
664.127269	32137.695887	32.450919
664.604392	32195.042025	32.455936
665.861160	32230.235605	32.460954
666.360444	32286.352123	32.465972
667.234747	32323.603082	32.470989
667.945615	32357.193941	32.476007
668.502437	32407.997842	32.481024
669.353261	32442.711300	32.486042
669.787000	32479.670779	32.491060
670.042459	32529.788557	32.496077
670.737752	32567.327016	32.501095
671.097937	32621.499991	32.506112
671.909240	32663.894734	32.511130
672.683766	32722.403508	32.516148
673.618410	32763.148200	32.521165
674.150616	32801.053852	32.526183
674.824136	32854.514852	32.531200
675.736724	32898.879399	32.536218
676.379688	32944.866507	32.541236
676.721084	32996.552522	32.546253
677.472178	33032.508957	32.551271
678.181342	33088.879452	32.556288
678.644853	33128.718288	32.561306
679.565327	33176.641502	32.566324
679.876228	33215.157664	32.571341
680.708850	33248.863771	32.576359
681.125278	33294.988068	32.581376
681.767877	33340.887596	32.586394
682.567350	33385.169631	32.591412
683.061752	33428.848073	32.596429
684.150923	33472.560460	32.601447
684.710362	33511.797134	32.606464
685.505217	33567.270479	32.611482
685.710748	33614.819188	32.616500
686.282415	33661.337389	32.621517
687.049570	33715.841823	32.626535
687.858944	33762.234733	32.631552
688.302148	33815.082854	32.636570
689.058731	33862.666464	32.641588
689.923114	33924.686110	32.646605
690.616978	33972.305022	32.651623
691.031710	34026.157027	32.656640
691.600309	34078.202325	32.661658
692.245955	34130.728899	32.666676
693.377536	34197.563310	32.671693
694.068372	34248.907187	32.676711
694.442761	34310.997929	32.681728
695.532368	34362.115624	32.686746
696.384508	34433.034301	32.691764
696.563766	34474.197072	32.696781
697.850342	34522.022116	32.701799
698.209660	34579.968470	32.706816
699.012694	34631.207300	32.711834
699.922900	34692.792150	32.716852
700.270881	34754.768184	32.721869
701.160250	34798.653535	32.726887
702.126015	34862.771893	32.731904
702.812430	34914.661822	32.736922
703.536889	34960.147501	32.741940
704.470204	35022.298750	32.746957
705.284767	35068.756963	32.751975
705.617472	35120.354715	32.756992
706.365804	35169.358835	32.762010
707.419935	35215.242653	32.767028
707.770317	35272.446224	32.772045
708.709186	35325.461236	32.777063
709.323355	35376.099007	32.782080
710.811280	35418.052563	32.787098
711.722322	35457.712337	32.792116
712.402959	35510.508780	32.797133
712.741420	35533.255969	32.802151
713.633993	35580.284857	32.807168
714.804745	35622.427296	32.812186
715.328297	35658.581719	32.817204
715.848116	35692.125468	32.822221
716.356710	35729.256052	32.827239
717.315170	35779.196266	32.832256
717.978828	35824.396099	32.837274
718.599245	35867.528863	32.842292
719.286523	35913.098256	32.847309
719.965824	35962.405812	32.852327
720.526203	36007.912966	32.857344
721.114967	36049.615731	32.862362
721.955130	36095.408310	32.867380
722.338707	36145.457848	32.872397
723.252007	36191.435260	32.877415
723.775586	36234.659721	32.882432
724.521061	36295.098812	32.887450
725.267819	36348.045123	32.892468
725.654196	36392.081637	32.897485
726.772213	36446.140156	32.902503
727.165281	36490.953565	32.907520
727.793120	36546.321636	32.912538
728.613125	36573.952256	32.917556
728.811360	36625.688418	32.922573
729.827680	36679.902470	32.927591
730.430419	36737.456414	32.932608
730.854313	36790.536287	32.937626
731.535033	36832.586691	32.942644
732.079615	36908.044643	32.947661
732.946499	36961.606096	32.952679
733.985901	37018.163316	32.957696
734.751094	37079.777679	32.962714
735.546884	37126.521545	32.967732
736.660693	37180.108341	32.972749
737.389712	37236.467851	32.977767
738.447335	37278.289734	32.982784
739.268027	37324.581206	32.987802
740.422126	37365.395487	32.992820
740.995821	37408.842167	32.997837
741.774584	37457.954328	33.002855
742.682699	37501.627365	33.007872
743.159973	37552.652061	33.012890
743.949145	37583.753989	33.017908
744.009267	37636.405693	33.022925
745.031190	37686.441680	33.027943
746.133908	37733.803053	33.032960
746.405363	37799.973324	33.037978
747.169128	37840.956775	33.042996
747.599043	37906.735949	33.048013
748.285387	37956.103932	33.053031
749.084014	38023.666198	33.058048
749.498557	38087.601859	33.063066
750.639386	38140.282595	33.068084
751.159694	38208.862592	33.073101
751.605893	38261.392492	33.078119
752.862606	38333.456359	33.083136
753.991610	38388.814422	33.088154
754.785646	38452.097674	33.093172
755.442044	38508.655220	33.098189
756.300721	38557.403337	33.103207
757.044292	38616.982949	33.108224
758.278357	38676.511666	33.113242
758.816489	38721.496873	33.118260
759.453473	38772.303571	33.123277
760.015277	38826.353516	33.128295
760.792957	38879.294955	33.133312
761.137262	38942.858342	33.138330
762.084606	38996.621043	33.143348
762.687360	39071.944749	33.148365
763.742891	39131.319126	33.153383
764.849444	39189.243890	33.158400
765.226353	39252.385740	33.163418
765.970058	39310.696154	33.168436
766.954728	39371.353321	33.173453
767.724531	39427.452951	33.178471
768.277130	39484.307465	33.183488
769.072425	39553.133508	33.188506
769.777324	39607.586837	33.193524
770.688530	39667.010449	33.198541
771.330333	39725.635072	33.203559
772.605594	39781.245878	33.208576
773.381440	39835.815217	33.213594
774.300259	39890.773500	33.218612
775.347661	39946.160914	33.223629
775.859672	39997.160696	33.228647
776.745271	40039.653467	33.233664
777.107639	40093.965294	33.238682
778.025585	40144.699860	33.243700
779.119341	40193.857767	33.248717
779.312978	40243.111635	33.253735
780.104432	40294.833837	33.258752
780.897734	40347.156671	33.263770
781.775836	40390.106637	33.268788
782.520692	40427.803051	33.273805
783.061199	40477.401878	33.278823
783.893259	40525.159353	33.283840
784.466104	40589.880949	33.288858
785.183794	40637.745015	33.293876
786.233515	40703.202218	33.298893
786.536562	40762.299775	33.303911
787.446741	40824.585299	33.308928
788.299718	40881.169038	33.313946
788.783866	40946.999610	33.318964
789.793543	41003.141866	33.323981
790.582923	41065.750452	33.328999
791.308298	41129.823794	33.334016
791.694628	41204.695287	33.339034
792.530610	41264.634609	33.344052
793.704860	41335.513343	33.349069
794.611439	41397.990798	33.354087
795.456222	41458.371996	33.359104
796.204612	41528.792716	33.364122
796.918131	41587.879206	33.369140
797.848613	41660.713274	33.374157
798.918556	41721.692604	33.379175
799.723307	41781.524363	33.384192
800.434635	41849.953317	33.389210
801.161005	41905.465262	33.394228
802.199818	41970.396695	33.399245
802.798481	42058.462881	33.404263
803.588842	42106.565516	33.409280
804.227412	42173.172647	33.414298
805.307639	42225.455319	33.419316
806.342674	42289.407954	33.424333
806.996365	42354.109536	33.429351
807.818807	42419.600935	33.434368
808.546077	42486.884610	33.439386
809.824496	42535.829306	33.444404
810.982330	42591.705909	33.449421
811.285216	42654.856480	33.454439
812.726105	42705.610467	33.459456
813.365994	42769.214895	33.464474
814.253607	42815.330584	33.469492
814.987234	42874.885450	33.474509
815.839893	42944.371045	33.479527
816.633954	42991.406130	33.484544
817.315497	43056.896059	33.489562
818.251509	43108.792161	33.494580
818.892968	43168.438067	33.499597
819.343942	43214.540337	33.504615
820.455037	43279.274635	33.509632
821.419031	43337.023884	33.514650
822.229609	43407.921647	33.519668
822.489037	43462.991554	33.524685
823.204218	43534.619306	33.529703
824.116844	43582.503731	33.534720
825.043115	43655.452587	33.539738
826.198457	43719.719553	33.544756
827.011581	43775.058253	33.549773
827.883545	43836.080589	33.554791
828.924118	43894.141957	33.559808
830.060844	43954.927325	33.564826
830.530398	44013.912823	33.569844
831.241837	44066.269922	33.574861
831.855802	44126.928405	33.579879
833.012364	44190.127579	33.584896
833.267491	44253.188943	33.589914
834.254135	44303.100150	33.594932
835.310291	44350.451545	33.599949
835.810478	44406.125173	33.604967
836.641709	44457.085624	33.609984
837.157395	44513.522475	33.615002
838.156857	44572.597753	33.620020
839.123713	44625.662808	33.625037
839.840842	44693.739124	33.630055
840.766652	44750.391053	33.635072
841.835014	44805.154928	33.640090
842.750945	44863.560834	33.645108
843.819691	44917.578521	33.650125
844.704335	44978.930948	33.655143
845.288675	45019.544652	33.660160
846.176595	45083.370132	33.665178
847.313796	45141.698044	33.670196
848.373643	45192.112222	33.675213
848.971594	45238.569025	33.680231
850.060391	45292.464314	33.685248
850.807634	45350.176637	33.690266
851.670156	45413.355478	33.695284
852.518690	45463.322416	33.700301
853.404900	45523.771532	33.705319
853.881390	45581.020545	33.710336
854.919540	45642.717791	33.715354
855.567709	45707.221270	33.720372
856.379861	45766.904509	33.725389
856.804474	45837.806841	33.730407
857.539329	45895.459241	33.735424
858.475486	45960.772598	33.740442
859.294864	46047.226163	33.745460
860.519917	46099.950894	33.750477
861.067112	46170.752960	33.755495
861.981169	46240.391118	33.760512
862.660169	46310.230554	33.765530
863.561332	46378.207440	33.770548
864.891364	46451.058312	33.775565
865.681494	46528.687308	33.780583
866.292424	46588.353448	33.785600
867.384086	46668.048856	33.790618
868.543840	46725.732136	33.795636
869.694490	46794.341999	33.800653
870.283441	46865.803984	33.805671
871.063043	46930.632121	33.810688
872.341210	46997.451461	33.815706
872.715082	47063.905677	33.820724
873.922284	47123.322264	33.825741
874.626794	47197.595079	33.830759
875.698309	47256.311960	33.835776
876.423235	47322.813510	33.840794
877.024557	47396.615929	33.845812
877.940517	47461.747000	33.850829
879.087230	47540.064135	33.855847
880.084772	47610.294521	33.860864
881.047225	47660.583902	33.865882
881.556734	47735.205151	33.870900
882.641191	47798.590217	33.875917
883.833219	47868.310331	33.880935
884.893660	47927.391279	33.885952
885.522855	47990.999584	33.890970
886.336921	48061.709102	33.895988
887.373603	48110.823877	33.901005
887.810365	48176.031597	33.906023
888.650689	48240.600980	33.911040
889.478409	48318.369452	33.916058
890.263801	48382.081066	33.921076
891.427238	48437.402050	33.926093
892.648428	48499.559436	33.931111
893.166504	48554.968512	33.936128
894.413894	48610.245215	33.941146
895.142007	48676.959015	33.946164
896.226291	48724.536688	33.951181
896.761518	48788.155524	33.956199
897.917574	48838.575544	33.961216
898.213633	48899.802515	33.966234
899.218685	48962.943802	33.971252
900.099656	49023.156368	33.976269
900.684615	49094.214763	33.981287
902.021628	49157.064501	33.986304
902.812470	49226.294485	33.991322
903.464736	49288.523606	33.996340
904.401533	49356.453270	34.001357
905.288312	49426.560995	34.006375
906.175008	49498.990870	34.011392
906.870620	49568.129157	34.016410
907.787219	49655.884673	34.021428
908.761944	49726.985591	34.026445
909.858191	49788.140993	34.031463
911.176402	49853.526312	34.036480
912.258778	49926.566093	34.041498
912.979489	49997.922506	34.046516
914.157639	50053.289407	34.051533
914.924532	50139.614888	34.056551
915.733542	50201.379203	34.061568
916.978494	50273.850664	34.066586
918.043588	50345.894808	34.071604
918.445395	50405.179604	34.076621
919.020575	50481.748325	34.081639
919.807616	50552.286274	34.086656
920.944845	50629.482952	34.091674
921.884132	50707.204216	34.096692
923.259723	50788.072001	34.101709
924.099464	50862.715324	34.106727
925.082032	50945.777087	34.111744
926.022461	51009.237774	34.116762
926.616998	51087.494849	34.121780
928.023240	51155.211233	34.126797
928.638566	51234.832250	34.131815
929.829375	51298.564793	34.136832
930.405166	51367.973904	34.141850
931.492279	51447.218504	34.146868
932.717234	51517.393852	34.151885
933.826621	51592.902367	34.156903
934.841484	51661.706188	34.161920
936.206343	51723.445002	34.166938
936.730373	51798.102525	34.171956
937.640689	51857.938305	34.176973
938.631677	51932.030034	34.181991
939.232008	51999.640226	34.187008
940.529344	52069.837620	34.192026
941.171328	52143.452842	34.197044
942.275183	52213.813666	34.202061
942.934075	52277.239397	34.207079
943.858870	52352.399467	34.212096
944.731466	52416.045412	34.217114
945.350404	52507.876105	34.222132
946.514527	52564.655939	34.227149
947.651646	52653.989403	34.232167
948.356993	52725.438883	34.237184
949.726695	52800.442557	34.242202
950.205970	52879.248809	34.247220
951.431767	52950.561014	34.252237
952.331799	53025.954909	34.257255
953.211143	53099.371682	34.262272
954.925454	53178.208166	34.267290
955.263567	53237.529098	34.272308
956.109680	53290.702744	34.277325
957.263857	53358.920397	34.282343
957.880386	53424.311136	34.287360
959.157109	53481.891967	34.292378
959.844479	53554.606022	34.297396
960.492937	53617.986397	34.302413
961.312425	53691.825659	34.307431
962.291533	53777.049562	34.312448
963.402390	53829.790891	34.317466
964.423417	53916.217412	34.322484
965.034710	53989.982445	34.327501
966.092773	54073.201817	34.332519
967.373624	54142.819508	34.337536
968.299858	54217.061456	34.342554
969.258797	54297.183651	34.347572
969.846976	54377.275239	34.352589
970.972362	54458.587068	34.357607
972.099325	54538.905415	34.362624
973.421528	54618.649424	34.367642
974.272282	54692.765402	34.372660
975.408960	54759.274913	34.377677
976.390703	54840.237055	34.382695
977.193573	54910.095952	34.387712
978.310104	54979.146841	34.392730
979.349011	55064.758449	34.397748
980.694903	55135.444758	34.402765
981.889296	55204.262695	34.407783
982.266299	55277.372110	34.412800
983.824746	55349.405549	34.417818
984.638334	55427.522807	34.422836
985.526229	55510.767411	34.427853
986.703837	55579.291617	34.432871
987.393127	55653.954671	34.437888
988.599357	55724.949261	34.442906
989.566257	55806.106871	34.447924
990.144283	55869.706770	34.452941
991.308666	55944.125914	34.457959
992.295684	56039.615269	34.462976
993.573075	56112.644058	34.467994
994.226498	56201.116995	34.473012
995.543892	56267.602614	34.478029
996.224629	56356.002260	34.483047
997.159739	56427.813243	34.488064
998.554531	56505.311968	34.493082
999.263523	56589.189419	34.498100
1000.130454	56674.991819	34.503117
1001.195682	56752.441388	34.508135
1002.008501	56843.847411	34.513152
1003.448002	56916.176254	34.518170
1004.206610	57000.066410	34.523188
1005.414788	57076.399897	34.528205
1006.269204	57167.965233	34.533223
1007.183572	57253.015521	34.538240
1008.423199	57327.047538	34.543258
1009.349512	57414.855932	34.548276
1010.229943	57491.792375	34.553293
1011.151688	57581.456463	34.558311
1012.194620	57662.393365	34.563328
1013.667190	57737.029614	34.568346
1014.385552	57827.194623	34.573364
1015.702320	57906.380891	34.578381
1016.806516	57991.113111	34.583399
1018.080252	58070.926867	34.588416
1018.770740	58139.135516	34.593434
1019.637934	58219.443425	34.598452
1020.973721	58294.596368	34.603469
1021.675486	58355.734238	34.608487
1022.462111	58440.865577	34.613504
1023.667471	58505.463442	34.618522
1024.507642	58588.321118	34.623540
1025.588042	58658.040185	34.628557
1026.555280	58722.156700	34.633575
1027.270904	58804.154738	34.638592
1028.078416	58869.037030	34.643610
1029.055670	58966.837088	34.648628
1030.332824	59045.995291	34.653645
1031.349850	59124.409405	34.658663
1032.399345	59215.642020	34.663680
1033.271402	59287.211861	34.668698
1034.320620	59362.267157	34.673716
1035.412875	59456.070091	34.678733
1036.299707	59535.056459	34.683751
1036.791628	59628.554750	34.688768
1038.184802	59709.019920	34.693786
1039.710169	59803.896088	34.698804
1040.940701	59887.957019	34.703821
1042.112886	59972.748893	34.708839
1042.827025	60057.409814	34.713856
1044.468341	60143.401505	34.718874
1045.211002	60235.470581	34.723892
1046.159227	60324.071002	34.728909
1047.219169	60407.894435	34.733927
1048.262051	60487.619164	34.738944
1049.358183	60561.373268	34.743962
1050.256682	60653.672852	34.748980
1051.531268	60735.248586	34.753997
1052.438609	60826.211864	34.759015
1054.041590	60901.837675	34.764032
1054.941781	60986.074075	34.769050
1055.950053	61074.104512	34.774068
1057.087621	61153.569808	34.779085
1058.346203	61241.042832	34.784103
1059.168799	61324.140430	34.789120
1060.384279	61412.785480	34.794138
1061.297480	61501.136084	34.799156
1062.294443	61581.352598	34.804173
1063.687215	61659.134011	34.809191
1064.669064	61742.967836	34.814208
1066.137782	61827.416137	34.819226
1067.072863	61907.719308	34.824244
1068.226225	61986.665775	34.829261
1069.828682	62064.466472	34.834279
1071.285958	62134.073511	34.839296
1072.612624	62193.401937	34.844314
1074.114452	62253.855329	34.849332
1074.892684	62315.839461	34.854349
1075.820860	62367.507527	34.859367
1076.943623	62449.327813	34.864384
1077.706161	62514.796500	34.869402
1078.656974	62583.515118	34.874420
1079.410510	62646.377496	34.879437
1080.713534	62719.593123	34.884455
1081.600307	62794.405689	34.889472
1082.386317	62870.968672	34.894490
1083.313181	62944.667647	34.899508
1084.591795	63019.065400	34.904525
1085.587911	63094.349288	34.909543
1086.264702	63189.598522	34.914560
1087.322483	63267.456138	34.919578
1088.698819	63357.855648	34.924596
1089.669950	63428.586525	34.929613
1090.846490	63507.426618	34.934631
1091.828207	63591.811149	34.939648
1093.052943	63661.078850	34.944666
1094.136358	63738.016024	34.949684
1094.882889	63816.303638	34.954701
1095.979707	63888.801474	34.959719
1096.735749	63967.847751	34.964736
1098.071121	64037.618386	34.969754
1099.022844	64116.754957	34.974772
1099.748393	64200.953521	34.979789
1100.993961	64273.347022	34.984807
1102.017938	64366.989366	34.989824
1102.993513	64461.196698	34.994842
1103.859353	64551.876251	34.999860
1104.532965	64639.009173	35.004877
1106.010663	64722.446674	35.009895
1106.753588	64814.918930	35.014912
1108.186280	64917.502118	35.019930
1109.243427	65017.504215	35.024948
1110.180184	65117.234228	35.029965
1111.512814	65212.876560	35.034983
1112.659876	65314.423244	35.040000
1113.597616	65408.355126	35.045018
1115.013126	65506.733308	35.050036
1116.107980	65610.036661	35.055053
1117.228390	65704.352727	35.060071
1118.289902	65802.603566	35.065088
1119.437973	65902.215157	35.070106
1120.790974	65994.634766	35.075124
1122.106808	66096.519200	35.080141
1123.335336	66187.388770	35.085159
1123.999193	66298.473364	35.090176
1125.136087	66391.288937	35.095194
1126.804645	66483.104066	35.100212
1127.962067	66580.019769	35.105229
1129.160362	66673.846150	35.110247
1130.153928	66768.027641	35.115264
1131.681034	66861.778210	35.120282
1132.961603	66944.956175	35.125300
1134.004770	67042.689176	35.130317
1135.189635	67128.212578	35.135335
1136.636596	67219.026516	35.140352
1137.957448	67308.518143	35.145370
1139.208358	67392.651903	35.150388
1140.295095	67487.119130	35.155405
1141.729000	67567.590718	35.160423
1142.716303	67660.250593	35.165440
1143.460297	67742.286369	35.170458
1144.636357	67820.614509	35.175476
1145.667467	67914.655098	35.180493
1147.014213	68006.639785	35.185511
1147.639806	68102.453716	35.190528
1149.057065	68195.270210	35.195546
1150.303717	68276.032773	35.200564
1151.120595	68374.394934	35.205581
1152.669010	68463.260003	35.210599
1153.836212	68554.261527	35.215616
1155.062374	68638.244941	35.220634
1156.623471	68725.019463	35.225652
1157.649591	68816.708713	35.230669
1159.139546	68894.516389	35.235687
1160.146258	68989.805751	35.240704
1160.894194	69069.685995	35.245722
1162.648931	69154.823533	35.250740
1163.206924	69244.966211	35.255757
1164.372604	69323.667802	35.260775
1165.689120	69418.783886	35.265792
1166.563504	69509.726721	35.270810
1168.013274	69597.123045	35.275828
1168.750891	69683.091837	35.280845
1169.719509	69766.986042	35.285863
1170.927664	69866.128815	35.290880
1171.615638	69949.535402	35.295898
1173.020001	70041.853989	35.300916
1173.711034	70124.317178	35.305933
1175.773159	70211.746904	35.310951
1176.407059	70297.163981	35.315968
1177.576944	70387.823276	35.320986
1178.559272	70471.470669	35.326004
1179.621819	70568.783454	35.331021
1180.819599	70663.871929	35.336039
1181.911100	70760.902305	35.341056
1183.001736	70849.789843	35.346074
1184.249101	70939.033227	35.351092
1185.338574	71042.739231	35.356109
1186.267479	71145.622102	35.361127
1187.717505	71254.731327	35.366144
1188.806442	71351.384352	35.371162
1190.261220	71457.048847	35.376180
1191.358377	71561.363625	35.381197
1192.648902	71665.851359	35.386215
1193.384522	71769.767301	35.391232
1195.024995	71879.837358	35.396250
1196.274716	71983.015537	35.401268
1197.200987	72085.256582	35.406285
1198.414947	72191.632774	35.411303
1199.741340	72291.975882	35.416320
1200.961867	72405.026521	35.421338
1202.464667	72512.853561	35.426356
1203.655092	72622.946117	35.431373
1205.111549	72716.025961	35.436391
1206.327436	72822.949016	35.441408
1207.615957	72927.784040	35.446426
1208.879355	73030.001602	35.451444
1210.280178	73137.695079	35.456461
1211.704521	73237.494576	35.461479
1212.803183	73338.193749	35.466496
1214.051284	73430.231946	35.471514
1215.112218	73529.025175	35.476532
1216.825721	73636.583348	35.481549
1218.572267	73717.639593	35.486567
1220.269903	73810.989729	35.491584
1221.255534	73897.940667	35.496602
1222.587099	73967.624823	35.501620
1223.729086	74055.324569	35.506637
1225.209675	74137.424117	35.511655
1226.083445	74231.017960	35.516672
1227.457559	74313.704603	35.521690
1229.035199	74394.383883	35.526708
1229.817738	74480.861682	35.531725
1230.846925	74565.933401	35.536743
1232.173863	74653.175667	35.541760
1233.239759	74746.120755	35.546778
1234.573304	74831.791935	35.551796
1235.359897	74938.156988	35.556813
1236.579984	75023.314446	35.561831
1238.156571	75123.451974	35.566848
1239.139330	75222.782974	35.571866
1240.540895	75312.675775	35.576884
1241.396896	75406.263824	35.581901
1242.633985	75503.504258	35.586919
1243.701996	75602.228049	35.591936
1244.593088	75707.794536	35.596954
1245.942286	75811.770096	35.601972
1247.227639	75916.604684	35.606989
1248.663120	76016.615498	35.612007
1249.799806	76117.813230	35.617024
1250.674028	76223.207018	35.622042
1251.889914	76321.264398	35.627060
1253.343969	76427.202089	35.632077
1254.639109	76525.893904	35.637095
1255.757172	76612.376994	35.642112
1256.567031	76711.525040	35.647130
1258.389817	76810.262435	35.652148
1259.431669	76910.743180	35.657165
1260.715547	77003.231424	35.662183
1262.070314	77110.922690	35.667200
1263.209073	77193.515469	35.672218
1264.672399	77280.656334	35.677236
1265.429655	77387.896990	35.682253
1266.690559	77494.590969	35.687271
1268.272131	77585.692075	35.692288
1269.027137	77693.593008	35.697306
1270.541232	77805.290590	35.702324
1271.882413	77913.202494	35.707341
1272.959680	78015.683333	35.712359
1274.583111	78115.634614	35.717376
1275.533513	78236.200641	35.722394
1276.742630	78343.387379	35.727412
1278.261258	78455.606302	35.732429
1279.624486	78571.574335	35.737447
1281.132467	78672.875783	35.742464
1282.209053	78800.911606	35.747482
1283.933046	78891.716187	35.752500
1285.217163	79010.295403	35.757517
1286.632745	79108.965135	35.762535
1288.463390	79211.054461	35.767552
1289.330634	79310.557707	35.772570
1290.658798	79406.493029	35.777588
1292.246620	79522.480781	35.782605
1293.546061	79617.838548	35.787623
1295.061842	79713.226314	35.792640
1296.436190	79818.809477	35.797658
1297.780984	79921.585156	35.802676
1299.142299	80023.167767	35.807693
1299.904577	80130.114275	35.812711
1301.412608	80234.221282	35.817728
1303.008343	80333.703494	35.822746
1305.125167	80399.265833	35.827764
1306.768068	80489.644869	35.832781
1307.806968	80583.234825	35.837799
1309.348138	80671.514536	35.842816
1310.353832	80757.559404	35.847834
1311.945653	80852.977258	35.852852
1313.204709	80936.462055	35.857869
1313.871604	81027.818259	35.862887
1315.312620	81125.084904	35.867904
1316.634599	81219.988560	35.872922
1317.168167	81317.346441	35.877940
1318.641213	81414.697794	35.882957
1319.779424	81521.439085	35.887975
1321.432437	81615.507042	35.892992
1322.623706	81721.125907	35.898010
1324.147781	81826.199249	35.903028
1325.351156	81924.848650	35.908045
1326.564347	82029.692407	35.913063
1328.329429	82129.027954	35.918080
1328.983260	82231.995701	35.923098
1330.552160	82336.569846	35.928116
1331.509496	82449.006278	35.933133
1332.717691	82561.340762	35.938151
1334.468757	82663.011662	35.943168
1335.533917	82767.627801	35.948186
1337.055657	82863.380149	35.953204
1338.236267	82980.193166	35.958221
1339.548648	83083.859736	35.963239
1341.246863	83192.408060	35.968256
1342.236663	83300.256159	35.973274
1343.370035	83397.603879	35.978292
1344.942841	83494.173987	35.983309
1345.803010	83589.423578	35.988327
1347.204479	83676.784176	35.993344
1348.240003	83781.446675	35.998362
1349.349043	83887.948030	36.003380
1350.556239	83996.487156	36.008397
1351.737504	84108.717916	36.013415
1353.536698	84220.751570	36.018432
1354.220655	84330.336386	36.023450
1355.376592	84455.838821	36.028468
1357.312994	84571.463698	36.033485
1358.685148	84698.694804	36.038503
1359.913685	84803.825171	36.043520
1361.168245	84935.662550	36.048538
1362.351306	85044.006665	36.053556
1364.049303	85183.949057	36.058573
1365.219321	85311.531118	36.063591
1367.192474	85426.570840	36.068608
1368.190511	85551.355026	36.073626
1369.493090	85667.729208	36.078644
1371.413106	85791.027754	36.083661
1372.719156	85917.716989	36.088679
1374.314107	86027.711345	36.093696
1375.660538	86153.711061	36.098714
1377.077346	86273.655974	36.103732
1378.504763	86396.932400	36.108749
1380.027681	86518.559823	36.113767
1381.394986	86633.445208	36.118784
1383.116193	86752.698455	36.123802
1384.772814	86863.028520	36.128820
1385.924298	86975.870650	36.133837
1387.520498	87095.208117	36.138855
1389.016790	87210.848698	36.143872
1390.413431	87333.031405	36.148890
1391.590566	87438.965010	36.153908
1393.245144	87550.945379	36.158925
1394.731103	87673.571806	36.163943
1396.461143	87783.577114	36.168960
1397.235140	87891.995523	36.173978
1398.807963	88005.777163	36.178996
1400.575642	88114.599316	36.184013
1401.768524	88238.655022	36.189031
1403.494067	88344.443175	36.194048
1404.964099	88465.085789	36.199066
1406.586029	88559.967032	36.204084
1408.105807	88662.075258	36.209101
1409.532077	88770.040538	36.214119
1410.849229	88872.472504	36.219136
1412.369894	88974.594346	36.224154
1413.788302	89094.905402	36.229172
1415.217657	89194.634363	36.234189
1416.163340	89298.114110	36.239207
1418.170030	89409.970706	36.244224
1419.612540	89517.885494	36.249242
1420.262171	89624.745482	36.254260
1421.914136	89731.690633	36.259277
1422.915167	89848.064980	36.264295
1424.532396	89946.626634	36.269312
1426.098173	90072.368218	36.274330
1427.370518	90192.338924	36.279348
1428.596309	90309.884061	36.284365
1429.575921	90430.002671	36.289383
1431.259678	90549.708001	36.294400
1432.509897	90666.224179	36.299418
1433.856516	90787.947340	36.304436
1435.526379	90905.387674	36.309453
1436.649500	91026.943812	36.314471
1438.091798	91127.817858	36.319488
1439.678460	91245.589317	36.324506
1440.615962	91353.196444	36.329524
1441.998302	91467.299804	36.334541
1443.227833	91584.012868	36.339559
1444.527217	91700.930970	36.344576
1446.139366	91832.401363	36.349594
1446.937552	91951.831865	36.354612
1448.843009	92067.934628	36.359629
1450.200991	92192.564077	36.364647
1451.916989	92307.125643	36.369664
1453.435017	92428.955489	36.374682
1454.786582	92562.180641	36.379700
1456.590530	92677.845262	36.384717
1457.921687	92811.898521	36.389735
1459.034585	92937.811271	36.394752
1460.743654	93063.378257	36.399770
1462.238394	93200.500361	36.404788
1463.506155	93319.368833	36.409805
1464.925759	93456.136212	36.414823
1466.513579	93585.387216	36.419840
1467.888281	93720.312244	36.424858
1469.114408	93859.240911	36.429876
1471.750015	93991.233096	36.434893
1472.920098	94126.926906	36.439911
1474.351394	94257.244453	36.444928
1476.106152	94384.267373	36.449946
1477.323120	94509.333819	36.454964
1479.391932	94639.870636	36.459981
1480.381712	94774.201083	36.464999
1481.464442	94904.753070	36.470016
1484.098878	95027.370130	36.475034
1486.828568	95125.306462	36.480052
1488.782458	95237.040685	36.485069
1490.388926	95339.728366	36.490087
1491.882981	95445.108426	36.495104
1493.070164	95551.157711	36.500122
1494.494592	95658.919671	36.505140
1495.997891	95765.681024	36.510157
1497.185084	95866.166755	36.515175
1498.606110	95986.390620	36.520192
1500.019846	96092.368459	36.525210
1500.939808	96208.107871	36.530228
1502.695622	96326.189419	36.535245
1504.188663	96444.984138	36.540263
1505.278604	96567.847668	36.545280
1506.608364	96686.440548	36.550298
1507.841310	96828.170174	36.555316
1509.523242	96944.731741	36.560333
1511.272712	97076.520039	36.565351
1512.810279	97201.560066	36.570368
1514.080743	97327.757679	36.575386
1515.225730	97458.196557	36.580404
1516.980179	97588.743937	36.585421
1518.379111	97720.728927	36.590439
1519.903185	97852.200605	36.595456
1521.354396	97988.615360	36.600474
1522.869955	98123.816406	36.605492
1524.789201	98256.483241	36.610509
1526.176019	98386.546031	36.615527
1527.358481	98518.834245	36.620544
1529.026153	98653.063107	36.625562
1530.565578	98790.177475	36.630580
1532.195995	98924.476662	36.635597
1533.697955	99053.890406	36.640615
1534.808178	99191.225422	36.645632
1536.490182	99331.375091	36.650650
1537.875237	99467.717733	36.655668
1539.580269	99583.397992	36.660685
1540.936849	99713.863884	36.665703
1542.431948	99828.715648	36.670720
1544.551004	99940.707044	36.675738
1545.649298	100066.714106	36.680756
1547.377644	100180.694115	36.685773
1548.921997	100303.082988	36.690791
1549.785774	100430.902823	36.695808
1551.679197	100549.866074	36.700826
1553.296784	100692.960222	36.705844
1554.808900	100815.318019	36.710861
1556.251375	100961.128277	36.715879
1557.933752	101092.297015	36.720896
1559.276786	101220.400347	36.725914
1560.596409	101355.721555	36.730932
1562.159960	101491.182851	36.735949
1563.679937	101642.752574	36.740967
1565.224541	101780.411317	36.745984
1567.172976	101933.513139	36.751002
1568.610152	102065.991771	36.756020
1570.200062	102202.707054	36.761037
1571.823307	102351.170495	36.766055
1573.765378	102505.505774	36.771072
1575.398703	102629.132018	36.776090
1577.074082	102776.359460	36.781108
1578.750836	102910.959548	36.786125
1581.245770	103030.953929	36.791143
1583.292034	103159.728780	36.796160
1584.846397	103268.713249	36.801178
1586.324819	103399.948324	36.806196
1588.109956	103521.690515	36.811213
1589.862763	103642.652102	36.816231
1591.284077	103780.490542	36.821248
1592.837097	103905.211761	36.826266
1594.272279	104035.606593	36.831284
1595.642149	104161.815357	36.836301
1597.054725	104282.756153	36.841319
1598.563244	104418.605734	36.846336
1600.136020	104558.642659	36.851354
1601.867883	104693.279435	36.856372
1603.417992	104817.104293	36.861389
1604.985936	104957.409903	36.866407
1606.412892	105097.547853	36.871424
1608.129316	105226.559547	36.876442
1609.537742	105374.512040	36.881460
1611.551875	105506.546897	36.886477
1613.096021	105638.148241	36.891495
1614.431037	105782.208650	36.896512
1615.915972	105927.590382	36.901530
1617.526639	106070.112916	36.906548
1619.117778	106213.805627	36.911565
1620.830688	106368.600192	36.916583
1622.384254	106518.994987	36.921600
1623.982941	106665.338528	36.926618
1625.287979	106813.072479	36.931636
1626.894700	106956.753225	36.936653
1628.337549	107104.213388	36.941671
1630.552515	107255.053733	36.946688
1631.809394	107408.719385	36.951706
1633.861225	107563.631466	36.956724
1635.018005	107708.146213	36.961741
1636.752260	107855.868583	36.966759
1638.312811	108003.758109	36.971776
1640.162901	108151.248152	36.976794
1641.787601	108298.431532	36.981812
1643.337312	108445.677933	36.986829
1645.351968	108595.908631	36.991847
1646.983640	108736.131120	36.996864
1648.754944	108855.650161	37.001882
1650.425664	108990.224674	37.006900
1651.768879	109117.559205	37.011917
1653.471495	109249.580913	37.016935
1654.677154	109384.482953	37.021952
1656.273609	109518.170723	37.026970
1657.867557	109660.774156	37.031988
1659.381112	109799.586361	37.037005
1661.071537	109937.598039	37.042023
1662.517178	110079.998005	37.047040
1664.474433	110219.605137	37.052058
1666.282653	110365.158180	37.057076
1667.818726	110507.761388	37.062093
1669.365539	110661.662618	37.067111
1670.863088	110813.276846	37.072128
1673.064750	110953.787280	37.077146
1674.327858	111107.633159	37.082164
1675.913308	111261.074453	37.087181
1677.691945	111415.589647	37.092199
1679.442185	111567.028279	37.097216
1681.334034	111720.576053	37.102234
1683.199828	111887.482506	37.107252
1684.601746	112042.680470	37.112269
1686.412598	112192.400275	37.117287
1688.744471	112339.186169	37.122304
1690.758650	112474.519506	37.127322
1692.495913	112625.000818	37.132340
1693.844448	112772.030310	37.137357
1695.968123	112922.934652	37.142375
1697.487384	113079.387065	37.147392
1699.203913	113218.878585	37.152410
1700.458510	113370.706370	37.157428
1702.051444	113522.114346	37.162445
1703.822216	113668.282788	37.167463
1705.378667	113842.285240	37.172480
1707.144413	114004.169460	37.177498
1708.223954	114161.836426	37.182516
1710.432345	114329.398433	37.187533
1712.485310	114486.750429	37.192551
1714.179722	114649.625195	37.197568
1715.907290	114818.634028	37.202586
1717.588718	114980.383515	37.207604
1719.249262	115138.674518	37.212621
1721.198267	115289.476375	37.217639
1722.696980	115465.879963	37.222656
1724.382597	115616.356346	37.227674
1726.412035	115787.009513	37.232692
1727.795316	115951.244848	37.237709
1729.807401	116120.037818	37.242727
1731.363834	116291.921115	37.247744
1732.970004	116462.643278	37.252762
1734.741270	116623.054230	37.257780
1736.036333	116798.316305	37.262797
1738.078322	116954.462934	37.267815
1739.575231	117136.899464	37.272832
1741.599541	117308.219973	37.277850
1743.485390	117486.640358	37.282868
1744.745790	117649.443678	37.287885
1746.678162	117830.585481	37.292903
1748.354766	117999.946530	37.297920
1750.276163	118169.054612	37.302938
1751.951523	118343.554418	37.307956
1753.573016	118520.625604	37.312973
1755.693085	118693.002982	37.317991
1757.255739	118865.810374	37.323008
1759.128232	119029.437643	37.328026
1760.474982	119213.328232	37.333044
1762.119895	119379.059973	37.338061
1764.443913	119543.392924	37.343079
1765.575206	119708.597180	37.348096
1767.258014	119856.401885	37.353114
1768.889617	120023.432316	37.358132
1770.399857	120189.188525	37.363149
1772.087948	120352.812105	37.368167
1773.569316	120522.468454	37.373184
1775.364603	120705.446509	37.378202
1777.321892	120879.634953	37.383220
1778.503977	121053.361325	37.388237
1780.567702	121238.088697	37.393255
1781.842921	121420.478766	37.398272
1783.892769	121611.045205	37.403290
1785.790463	121801.116163	37.408308
1787.565353	121995.799224	37.413325
1789.450482	122187.789492	37.418343
1790.862046	122386.514233	37.423360
1792.746441	122566.671007	37.428378
1794.864957	122762.864702	37.433396
1796.312315	122967.269911	37.438413
1799.230811	123157.340786	37.443431
1800.688901	123356.304200	37.448448
1802.897352	123537.099994	37.453466
1804.897294	123734.357195	37.458484
1806.551328	123929.195462	37.463501
1808.368561	124108.151859	37.468519
1810.391557	124304.266557	37.473536
1812.051810	124485.469124	37.478554
1813.729988	124667.938332	37.483572
1816.051613	124879.714779	37.488589
1817.726311	125069.645826	37.493607
1819.268587	125259.661808	37.498624
1821.048403	125454.183430	37.503642
1823.092120	125646.216436	37.508660
1824.704131	125846.931660	37.513677
1826.871856	126030.815151	37.518695
1828.374281	126243.753841	37.523712
1830.354183	126441.522193	37.528730
1832.129921	126641.822562	37.533748
1834.049306	126842.101554	37.538765
1835.765282	127035.194362	37.543783
1837.604742	127234.954859	37.548800
1839.501789	127441.203094	37.553818
1842.018676	127637.459999	37.558836
1843.556927	127842.395877	37.563853
1845.227977	128028.471668	37.568871
1847.408908	128237.737290	37.573888
1849.631929	128430.161393	37.578906
1851.384576	128626.541915	37.583924
1853.034385	128825.908216	37.588941
1855.075376	129018.046171	37.593959
1856.791977	129222.352068	37.598976
1858.591120	129413.869722	37.603994
1861.152115	129603.506094	37.609012
1862.467082	129804.565850	37.614029
1865.020865	129974.653282	37.619047
1866.838476	130162.606199	37.624064
1868.993196	130349.733522	37.629082
1871.043262	130533.985113	37.634100
1872.848412	130718.072610	37.639117
1874.661452	130903.669547	37.644135
1876.528981	131091.618789	37.649152
1877.785407	131275.819461	37.654170
1879.964618	131463.823329	37.659188
1881.516262	131655.973238	37.664205
1883.276628	131842.254901	37.669223
1885.006227	132037.474755	37.674240
1886.268044	132225.244064	37.679258
1888.135134	132407.400503	37.684276
1889.747329	132601.968677	37.689293
1891.949838	132780.750084	37.694311
1893.957458	132959.790949	37.699328
1895.277245	133149.090537	37.704346
1896.841411	133335.434500	37.709364
1898.482091	133534.012021	37.714381
1900.511226	133728.837526	37.719399
1902.276594	133931.356350	37.724416
1903.814339	134135.281934	37.729434
1905.784271	134345.079652	37.734452
1907.696132	134562.335888	37.739469
1909.509462	134778.225402	37.744487
1911.570560	134984.865037	37.749504
1913.618157	135194.388190	37.754522
1915.778481	135402.004070	37.759540
1917.139989	135627.256574	37.764557
1919.257886	135835.667798	37.769575
1921.292430	136054.206487	37.774592
1923.214466	136284.653863	37.779610
1925.219485	136491.994372	37.784628
1926.745294	136721.896527	37.789645
1928.979861	136941.842288	37.794663
1931.190820	137170.650268	37.799680
1932.937002	137407.805523	37.804698
1934.986337	137626.400198	37.809716
1936.435785	137866.789173	37.814733
1938.723347	138088.851402	37.819751
1940.868308	138314.820068	37.824768
1942.641969	138550.707895	37.829786
1944.711095	138776.969792	37.834804
1946.956298	139020.083499	37.839821
1948.665273	139249.094077	37.844839
1950.500588	139478.339917	37.849856
1952.837087	139719.387184	37.854874
1954.970921	139951.101582	37.859892
1956.682736	140194.862751	37.864909
1958.953783	140428.004856	37.869927
1961.156600	140658.265230	37.874944
1962.813744	140883.306878	37.879962
1965.266037	141117.490171	37.884980
1966.926169	141353.460406	37.889997
1968.960088	141592.838267	37.895015
1971.226919	141830.391626	37.900032
1972.654604	142064.815130	37.905050
1974.975786	142296.042130	37.910068
1976.722234	142529.606027	37.915085
1978.571536	142771.137867	37.920103
1980.858950	143001.421615	37.925120
1983.101693	143249.024507	37.930138
1984.906004	143476.644317	37.935156
1986.931556	143716.313101	37.940173
1988.795321	143951.997673	37.945191
1990.999573	144197.783712	37.950208
1992.705849	144427.821869	37.955226
1994.915566	144662.339086	37.960244
1996.797737	144911.872075	37.965261
1998.797163	145137.578018	37.970279
2000.945734	145385.320407	37.975296
2002.829601	145621.656991	37.980314
2004.804351	145863.603128	37.985332
2006.894747	146100.925166	37.990349
2009.056301	146334.975334	37.995367
2011.119215	146572.963836	38.000384
2012.589653	146810.563341	38.005402
2014.641260	147049.228501	38.010420
2016.639516	147297.079705	38.015437
2018.973654	147536.286993	38.020455
2021.146559	147755.682000	38.025472
2022.862272	147987.689389	38.030490
2024.913337	148203.487845	38.035508
2026.522444	148432.492940	38.040525
2028.631847	148655.163631	38.045543
2030.270235	148878.340123	38.050560
2031.585245	149113.676899	38.055578
2033.539425	149339.954025	38.060596
2035.390301	149602.778644	38.065613
2037.595517	149845.570526	38.070631
2039.305687	150099.762819	38.075648
2041.182087	150357.421067	38.080666
2043.203631	150610.209138	38.085684
2045.205033	150875.694827	38.090701
2047.098349	151132.021333	38.095719
2049.369127	151396.376011	38.100736
2051.444004	151657.094037	38.105754
2053.445407	151912.823481	38.110772
2055.838578	152192.471361	38.115789
2058.121097	152448.235698	38.120807
2060.301979	152716.913858	38.125824
2062.156254	152988.589105	38.130842
2064.333681	153249.590626	38.135860
2066.455188	153517.558327	38.140877
2068.726462	153785.707099	38.145895
2071.271662	154051.428035	38.150912
2073.292916	154312.788827	38.155930
2075.826452	154579.504187	38.160948
2077.698131	154843.454908	38.165965
2079.501171	155110.857671	38.170983
2081.857312	155373.681805	38.176000
2083.808768	155642.295283	38.181018
2085.936028	155909.994033	38.186036
2087.945164	156184.250064	38.191053
2090.056745	156454.467263	38.196071
2092.243371	156730.538940	38.201088
2094.297680	157001.821221	38.206106
2096.432697	157269.359933	38.211124
2098.454820	157553.281007	38.216141
2100.613050	157829.336830	38.221159
2102.724472	158098.863333	38.226176
2104.327247	158388.528254	38.231194
2106.459967	158673.414927	38.236212
2108.273643	158954.226688	38.241229
2110.568392	159241.655216	38.246247
2113.029532	159531.941012	38.251264
2114.711509	159822.324050	38.256282
2117.387903	160112.820296	38.261300
2119.594480	160400.598036	38.266317
2121.400860	160695.396494	38.271335
2124.042306	160979.529111	38.276352
2126.192074	161265.758128	38.281370
2128.127067	161550.523787	38.286388
2130.014163	161835.234701	38.291405
2132.321470	162118.383395	38.296423
2134.831997	162394.696775	38.301440
2136.843352	162694.081201	38.306458
2139.267694	162973.127388	38.311476
2141.616506	163254.268669	38.316493
2143.858173	163531.187373	38.321511
2146.222119	163800.318230	38.326528
2147.951512	164091.944892	38.331546
2150.291869	164361.703826	38.336564
2152.188700	164639.925086	38.341581
2154.365666	164929.428989	38.346599
2156.364551	165204.932416	38.351616
2158.231356	165492.354037	38.356634
2160.605143	165760.310525	38.361652
2162.370872	166025.328244	38.366669
2164.286542	166288.584234	38.371687
2166.256500	166560.809271	38.376704
2168.100427	166829.385674	38.381722
2170.425387	167098.472305	38.386740
2172.408856	167379.230636	38.391757
2174.483976	167660.344041	38.396775
2176.569136	167937.406721	38.401792
2178.110428	168223.887344	38.406810
2180.884543	168504.362067	38.411828
2182.876258	168792.184247	38.416845
2184.913549	169085.244370	38.421863
2187.616862	169369.694987	38.426880
2189.440991	169680.020655	38.431898
2191.970722	169967.408283	38.436916
2194.097256	170257.602397	38.441933
2196.272177	170559.954137	38.446951
2198.637924	170854.024145	38.451968
2200.696742	171149.311246	38.456986
2203.103799	171443.402552	38.462004
2205.682935	171745.988253	38.467021
2207.676223	172044.590431	38.472039
2210.378579	172344.569053	38.477056
2212.293994	172651.236012	38.482074
2214.514320	172952.218967	38.487092
2216.985361	173256.541680	38.492109
2218.931038	173563.753563	38.497127
2221.128257	173864.438910	38.502144
2223.061788	174176.581855	38.507162
2225.275435	174495.069508	38.512180
2227.454037	174810.237018	38.517197
2229.692732	175128.431252	38.522215
2232.027135	175427.259953	38.527232
2234.850037	175745.708554	38.532250
2236.928041	176063.499740	38.537268
2239.236799	176377.497567	38.542285
2241.174884	176704.684312	38.547303
2243.507935	177018.172860	38.552320
2245.334160	177350.052539	38.557338
2247.791530	177670.863852	38.562356
2250.441118	177986.338500	38.567373
2252.624023	178309.048919	38.572391
2255.206132	178645.514483	38.577408
2256.890503	178974.349507	38.582426
2259.257874	179296.958717	38.587444
2261.687879	179626.619860	38.592461
2263.812336	179960.164817	38.597479
2266.139362	180278.491710	38.602496
2268.344820	180616.115535	38.607514
2270.313823	180948.647061	38.612532
2272.356186	181288.813162	38.617549
2274.453404	181625.213083	38.622567
2277.022243	181959.001025	38.627584
2278.966418	182316.304521	38.632602
2281.229069	182663.044921	38.637620
2283.843486	183007.014222	38.642637
2285.916298	183350.992860	38.647655
2289.445641	183676.052708	38.652672
2291.828761	184011.654685	38.657690
2294.068044	184340.600333	38.662708
2296.292586	184660.608991	38.667725
2298.466815	185005.212655	38.672743
2300.935608	185333.109925	38.677760
2303.333915	185668.029379	38.682778
2305.394133	185985.756526	38.687796
2307.798125	186335.358001	38.692813
2309.635536	186734.348942	38.697831
2311.797722	187053.206474	38.702848
2314.329507	187377.823938	38.707866
2316.160584	187691.045439	38.712884
2318.588608	187999.780819	38.717901
2320.590917	188322.121385	38.722919
2322.699232	188643.481218	38.727936
2324.849461	188964.073475	38.732954
2326.862260	189298.429416	38.737972
2329.075075	189627.980029	38.742989
2330.862857	189967.122787	38.748007
2333.180231	190309.892563	38.753024
2335.320587	190654.799132	38.758042
2337.641331	191009.533979	38.763060
2340.176136	191359.080306	38.768077
2342.085490	191722.517461	38.773095
2344.461833	192075.621223	38.778112
2346.965792	192454.182986	38.783130
2348.940333	192830.516848	38.788148
2351.667606	193183.747005	38.793165
2353.537022	193560.277244	38.798183
2356.271861	193944.776820	38.803200
2358.694203	194320.410432	38.808218
2361.107125	194696.351413	38.813236
2363.880818	195079.908477	38.818253
2366.310475	195462.732754	38.823271
2368.515922	195831.317486	38.828288
2370.908605	196224.640412	38.833306
2373.776789	196605.900981	38.838324
2376.330752	196970.878325	38.843341
2378.508942	197356.591972	38.848359
2380.940929	197742.927603	38.853376
2383.490222	198128.255340	38.858394
2385.797516	198514.561613	38.863412
2388.138259	198903.226051	38.868429
2390.506427	199299.380782	38.873447
2392.837779	199690.080839	38.878464
2395.595144	200069.614889	38.883482
2397.730623	200454.708080	38.888500
2401.038246	200836.800141	38.893517
2403.431474	201230.745820	38.898535
2405.783914	201618.526030	38.903552
2408.711265	201998.444551	38.908570
2411.222403	202374.338905	38.913588
2413.742291	202752.696747	38.918605
2416.081302	203129.533997	38.923623
2418.827012	203499.323045	38.928640
2421.345408	203872.221933	38.933658
2423.550350	204244.001829	38.938676
2426.147408	204605.915994	38.943693
2428.647684	204997.084461	38.948711
2431.011826	205366.428493	38.953728
2433.821018	205735.576934	38.958746
2436.026538	206103.905490	38.963764
2438.907058	206482.824291	38.968781
2441.236038	206860.457845	38.973799
2443.513455	207217.117194	38.978816
2446.109133	207592.729083	38.983834
2448.857143	207955.336912	38.988852
2451.239205	208312.718415	38.993869
2453.104195	208698.429274	38.998887
2455.467136	209072.530201	39.003904
2457.975538	209432.662677	39.008922
2460.597119	209818.740232	39.013940
2463.184476	210188.540160	39.018957
2465.658895	210558.002542	39.023975
2468.433402	210914.920259	39.028992
2471.323799	211284.598338	39.034010
2473.845697	211643.690197	39.039028
2476.269612	211982.043093	39.044045
2478.052447	212327.913976	39.049063
2480.262165	212652.989520	39.054080
2482.935421	212996.487077	39.059098
2484.944529	213343.848098	39.064116
2487.308040	213681.272319	39.069133
2489.381292	214040.208148	39.074151
2491.216687	214391.560259	39.079168
2494.129251	214751.356943	39.084186
2496.127864	215122.550068	39.089204
2498.047631	215491.367872	39.094221
2500.123389	215880.586391	39.099239
2502.638272	216269.203463	39.104256
2505.005111	216655.811621	39.109274
2507.443795	217051.554325	39.114292
2510.074505	217447.165867	39.119309
2511.941909	217863.880140	39.124327
2514.444026	218270.994911	39.129344
2517.154678	218681.761108	39.134362
2519.677846	219103.175633	39.139380
2522.551333	219507.388252	39.144397
2525.154271	219934.303587	39.149415
2527.483293	220353.411976	39.154432
2530.350090	220769.515450	39.159450
2532.627373	221197.015675	39.164468
2534.924121	221619.838735	39.169485
2537.986336	222058.242562	39.174503
2540.465897	222484.340060	39.179520
2543.044996	222919.618490	39.184538
2545.514227	223360.452244	39.189556
2548.051819	223798.379413	39.194573
2551.230840	224229.550986	39.199591
2553.775054	224656.121666	39.204608
2556.577654	225085.421235	39.209626
2559.419730	225516.365961	39.214644
2562.252411	225954.933395	39.219661
2564.618686	226382.725858	39.224679
2567.626461	226812.374580	39.229696
2570.193180	227235.944107	39.234714
2572.806511	227678.915043	39.239732
2575.336081	228101.601064	39.244749
2577.712089	228530.179226	39.249767
2580.446682	228968.075565	39.254784
2583.551859	229397.378323	39.259802
2585.610300	229827.504321	39.264820
2588.728364	230259.777007	39.269837
2591.160142	230696.652804	39.274855
2593.373726	231127.516175	39.279872
2596.435994	231553.014010	39.284890
2598.510156	231991.824624	39.289908
2601.525415	232417.989744	39.294925
2604.551393	232862.646977	39.299943
2607.274918	233288.831476	39.304960
2609.306441	233720.508962	39.309978
2611.854168	234154.646146	39.314996
2614.535975	234589.143139	39.320013
2616.966317	235019.182381	39.325031
2619.946190	235466.486493	39.330048
2622.774746	235898.698430	39.335066
2625.311838	236337.153782	39.340084
2628.149177	236751.961853	39.345101
2631.266601	237183.466914	39.350119
2633.908801	237602.470597	39.355136
2636.390751	238028.535521	39.360154
2638.996855	238450.592217	39.365172
2641.987524	238877.872459	39.370189
2644.578850	239287.203157	39.375207
2647.547369	239714.790530	39.380224
2650.176177	240119.465415	39.385242
2651.976335	240522.871494	39.390260
2654.848452	240913.103633	39.395277
2657.320301	241301.898702	39.400295
2659.622637	241694.580883	39.405312
2662.138453	242087.381662	39.410330
2664.414382	242500.948202	39.415348
2666.813539	242904.587621	39.420365
2669.640987	243318.778226	39.425383
2671.913831	243736.966482	39.430400
2674.547360	244152.811567	39.435418
2677.140831	244583.878513	39.440436
2679.451444	245012.473731	39.445453
2682.120831	245446.042030	39.450471
2684.322054	245898.632808	39.455488
2687.324557	246330.547026	39.460506
2689.974843	246787.816245	39.465524
2692.280710	247238.355476	39.470541
2695.198218	247685.445315	39.475559
2697.635366	248156.842874	39.480576
2700.680160	248606.831970	39.485594
2703.204430	249076.537014	39.490612
2706.209575	249535.827211	39.495629
2709.430308	249992.898037	39.500647
2712.291209	250458.431758	39.505664
2715.396811	250918.972674	39.510682
2718.177426	251376.311395	39.515700
2721.092514	251831.646526	39.520717
2723.633939	252301.390574	39.525735
2726.310972	252763.389927	39.530752
2729.394418	253222.784450	39.535770
2731.689259	253690.301812	39.540788
2734.276908	254156.273422	39.545805
2737.168325	254629.994521	39.550823
2739.813011	255107.689657	39.555840
2742.927978	255579.874084	39.560858
2745.616908	256058.498902	39.565876
2748.228737	256537.159425	39.570893
2750.936710	257015.981071	39.575911
2753.427244	257491.278665	39.580928
2756.052205	257973.361028	39.585946
2758.893480	258466.584248	39.590964
2761.878415	258953.356792	39.595981
2764.792873	259444.253278	39.600999
2767.445369	259936.585572	39.606016
2770.253039	260424.573630	39.611034
2773.233384	260913.955213	39.616052
2776.553349	261396.728644	39.621069
2779.704967	261879.170641	39.626087
2782.445833	262361.598304	39.631104
2785.318244	262834.961069	39.636122
2788.057491	263312.990677	39.641140
2790.659825	263797.110003	39.646157
2793.512399	264274.863731	39.651175
2796.582889	264762.385563	39.656192
2799.441833	265229.313837	39.661210
2802.044837	265717.615130	39.666228
2805.075921	266195.814858	39.671245
2808.166455	266663.564117	39.676263
2810.523344	267147.655187	39.681280
2813.393676	267614.773868	39.686298
2816.266901	268097.865553	39.691316
2818.969801	268583.622763	39.696333
2821.752353	269059.256586	39.701351
2824.347226	269546.244801	39.706368
2827.507416	270020.087914	39.711386
2830.280652	270515.475436	39.716404
2832.977989	270988.496655	39.721421
2835.804053	271456.415841	39.726439
2838.370469	271918.353778	39.731456
2840.731198	272373.870382	39.736474
2843.490225	272827.849599	39.741492
2846.210097	273293.464408	39.746509
2849.093448	273746.048011	39.751527
2851.611192	274207.727373	39.756544
2854.589824	274677.129270	39.761562
2857.132783	275153.554980	39.766580
2859.296400	275642.227247	39.771597
2862.267089	276119.088735	39.776615
2864.681003	276610.179687	39.781632
2867.717513	277103.837324	39.786650
2870.554779	277600.697376	39.791668
2873.345284	278100.989980	39.796685
2876.271249	278613.117970	39.801703
2878.644619	279137.975406	39.806720
2881.766586	279646.739234	39.811738
2884.687086	280162.260656	39.816756
2887.652066	280695.573334	39.821773
2890.733852	281217.360274	39.826791
2893.324878	281741.733933	39.831808
2896.439061	282277.830715	39.836826
2899.104985	282819.072078	39.841844
2902.157504	283345.139870	39.846861
2905.167495	283867.909206	39.851879
2907.932434	284413.439915	39.856896
2911.179982	284945.204295	39.861914
2914.393272	285485.755900	39.866932
2917.737038	286030.853638	39.871949
2920.757857	286561.955120	39.876967
2923.394077	287104.335709	39.881984
2926.649490	287639.988152	39.887002
2929.676924	288191.110070	39.892020
2932.642287	288731.166180	39.897037
2936.362640	289272.268316	39.902055
2939.072058	289818.753837	39.907072
2941.995875	290346.792721	39.912090
2944.702241	290897.814448	39.917108
2947.386863	291444.696029	39.922125
2950.398908	291989.109750	39.927143
2953.819014	292541.554657	39.932160
2956.805360	293086.394281	39.937178
2959.865942	293625.987156	39.942196
2962.944560	294168.644523	39.947213
2966.209588	294710.734771	39.952231
2969.010531	295253.755504	39.957248
2972.170801	295798.238634	39.962266
2975.231339	296336.689699	39.967284
2978.247259	296884.663347	39.972301
2981.068517	297417.784591	39.977319
2984.196541	297962.099959	39.982336
2987.432493	298498.015355	39.987354
2990.418353	299039.702112	39.992372
2993.516700	299580.350608	39.997389
2996.960337	300106.393364	40.002407
3000.266859	300639.560691	40.007424
3003.160438	301163.190982	40.012442
3006.386766	301689.506137	40.017460
3009.310432	302222.565128	40.022477
3012.795282	302749.185039	40.027495
3015.421924	303273.445492	40.032512
3018.335367	303788.187414	40.037530
3021.384260	304308.056335	40.042548
3023.911726	304848.689720	40.047565
3026.950891	305383.856313	40.052583
3029.798738	305913.005660	40.057600
3032.703204	306446.151350	40.062618
3035.696356	306975.571607	40.067636
3038.622216	307479.131107	40.072653
3041.468785	307976.479001	40.077671
3043.810762	308495.526627	40.082688
3046.665586	309002.559167	40.087706
3050.049393	309508.742672	40.092724
3052.159455	310035.348630	40.097741
3055.214573	310559.492053	40.102759
3058.128929	311082.331830	40.107776
3061.093812	311617.899397	40.112794
3064.136505	312161.976808	40.117812
3066.628303	312716.108263	40.122829
3069.975380	313261.749949	40.127847
3072.267654	313817.574501	40.132864
3075.182254	314378.650662	40.137882
3078.650970	314938.237885	40.142900
3081.467639	315516.573359	40.147917
3084.834674	316089.663936	40.152935
3087.840062	316682.218019	40.157952
3090.920892	317263.738438	40.162970
3094.609546	317836.274460	40.167988
3097.532309	318435.543194	40.173005
3100.469091	319026.833177	40.178023
3103.751091	319623.974224	40.183040
3107.028199	320217.123726	40.188058
3110.225353	320808.831083	40.193076
3113.115879	321407.962318	40.198093
3116.520455	322008.679909	40.203111
3119.325502	322606.208901	40.208128
3122.399398	323232.157879	40.213146
3125.491344	323838.607278	40.218164
3128.794634	324456.560040	40.223181
3132.091631	325059.432691	40.228199
3135.676059	325668.392047	40.233216
3138.398306	326280.165985	40.238234
3141.708955	326905.565559	40.243252
3144.696868	327529.711677	40.248269
3148.087913	328152.567500	40.253287
3151.496906	328780.459636	40.258304
3154.665404	329404.091572	40.263322
3158.101393	330015.570341	40.268340
3161.153195	330636.638420	40.273357
3164.591720	331261.517927	40.278375
3167.825071	331881.802070	40.283392
3170.848303	332510.835720	40.288410
3174.317128	333125.837103	40.293428
3177.483851	333744.249454	40.298445
3180.983140	334366.303562	40.303463
3184.262443	334981.228078	40.308480
3187.566746	335601.846051	40.313498
3190.862515	336217.939781	40.318516
3194.085136	336838.017022	40.323533
3197.612785	337445.658022	40.328551
3200.855738	338050.492324	40.333568
3203.692343	338670.852110	40.338586
3207.276576	339280.330526	40.343604
3210.319652	339898.760061	40.348621
3213.859472	340513.068828	40.353639
3216.955086	341119.573629	40.358656
3220.170026	341728.991465	40.363674
3223.342532	342336.528545	40.368692
3226.852732	342952.371773	40.373709
3230.304956	343551.398774	40.378727
3233.639715	344163.113936	40.383744
3236.659684	344760.868429	40.388762
3239.806539	345355.118457	40.393780
3243.036562	345977.722104	40.398797
3246.243958	346573.589721	40.403815
3249.149239	347176.137679	40.408832
3252.209804	347766.174588	40.413850
3255.437130	348332.922375	40.418868
3258.098060	348916.256006	40.423885
3261.098451	349498.360114	40.428903
3264.357716	350077.117344	40.433920
3267.026586	350667.416945	40.438938
3270.174040	351266.708514	40.443956
3273.271601	351861.635762	40.448973
3276.552491	352467.070856	40.453991
3279.728133	353083.286235	40.459008
3282.362367	353705.075625	40.464026
3285.568192	354325.420213	40.469044
3288.930050	354955.286140	40.474061
3292.135800	355582.958156	40.479079
3295.642802	356228.620761	40.484096
3298.836467	356872.873761	40.489114
3302.124323	357510.456986	40.494132
3305.521576	358158.758246	40.499149
3308.968639	358801.410573	40.504167
3312.322003	359458.664718	40.509184
3315.451669	360115.914118	40.514202
3318.908793	360771.830912	40.519220
3322.156582	361437.245719	40.524237
3325.583319	362103.783830	40.529255
3329.215653	362778.993973	40.534272
3332.340688	363434.777262	40.539290
3336.035196	364118.868646	40.544308
3339.250229	364795.643608	40.549325
3342.652722	365464.365211	40.554343
3346.248847	366143.127749	40.559360
3349.120424	366835.342463	40.564378
3353.003991	367509.618598	40.569396
3356.477547	368190.556673	40.574413
3360.079740	368864.667244	40.579431
3363.805133	369541.099234	40.584448
3367.112426	370228.146529	40.589466
3370.471213	370903.589294	40.594484
3374.109805	371585.408056	40.599501
3377.513615	372268.412176	40.604519
3381.161330	372940.948121	40.609536
3384.295392	373634.323196	40.614554
3388.280893	374303.504924	40.619572
3392.066559	374978.731052	40.624589
3395.293839	375654.686001	40.629607
3399.094843	376328.204112	40.634624
3402.298742	376997.263715	40.639642
3405.869754	377663.336295	40.644660
3409.424015	378340.439490	40.649677
3412.737125	379002.693655	40.654695
3416.840563	379665.846821	40.659712
3419.966997	380339.165923	40.664730
3423.580079	380999.144901	40.669748
3427.078956	381668.572506	40.674765
3430.360745	382333.229713	40.679783
3433.933550	382989.821197	40.684800
3437.460412	383654.963487	40.689818
3441.303121	384320.672553	40.694836
3444.839378	384982.081368	40.699853
3448.078698	385645.342584	40.704871
3451.593290	386292.944100	40.709888
3454.720107	386959.708408	40.714906
3458.099253	387617.578203	40.719924
3461.696929	388269.825896	40.724941
3464.894152	388930.905324	40.729959
3468.425232	389581.812305	40.734976
3471.705965	390243.071642	40.739994
3474.820016	390905.605138	40.745012
3478.718805	391548.701761	40.750016
3481.705110	392183.776147	40.755021
3485.057896	392761.718171	40.760026
3487.735334	393284.927545	40.765031
3489.638884	393762.966372	40.770036
3492.537909	394211.094864	40.775040
3494.882565	394607.475148	40.780045
3497.426313	394965.849860	40.785050
3499.896468	395277.025024	40.790055
3502.060331	395548.601661	40.795060
3503.888536	395778.250831	40.800064
3505.265563	395953.708442	40.805069
3507.039694	396108.444865	40.810074
3508.497641	396235.465552	40.815079
3510.160552	396311.849397	40.820084
3511.057042	396369.775399	40.825088
3511.866412	396395.281491	40.830093
3512.714108	396397.332142	40.835098
3513.352544	396392.360216	40.840103
3514.325553	396352.212750	40.845108
3514.988029	396299.170606	40.850112
3515.241007	396237.563422	40.855117
3515.902389	396142.240691	40.860122
3516.022122	396038.423905	40.865127
3516.366426	395930.206586	40.870132
3516.723930	395810.413979	40.875136
3516.833754	395675.837998	40.880141
3517.080172	395537.534652	40.885146
3517.158655	395388.901897	40.890151
3517.765875	395231.861484	40.895156
3517.767807	395071.513366	40.900160
3517.401855	394904.825716	40.905165
3517.722534	394727.878070	40.910170
3517.230731	394553.898133	40.915175
3517.281016	394378.817365	40.920180
3517.435558	394196.663313	40.925184
3517.250225	394027.149610	40.930189
3517.479639	393825.184134	40.935194
3517.182341	393650.253688	40.940199
3517.378497	393454.635568	40.945204
3517.256567	393269.065683	40.950208
3516.773060	393081.113998	40.955213
3516.844211	392873.022831	40.960218
3516.620258	392679.595914	40.965223
3516.433240	392490.781293	40.970228
3516.052249	392300.117085	40.975232
3515.845630	392114.754622	40.980237
3515.980219	391931.520584	40.985242
3515.328280	391753.433417	40.990247
3515.314103	391560.777238	40.995252
3515.353646	391384.508912	41.000256
3514.959200	391209.423734	41.005261
3515.352164	391026.548855	41.010266
3514.884105	390851.320274	41.015271
3514.556441	390673.479407	41.020276
3514.508446	390492.649144	41.025280
3514.099722	390312.990611	41.030285
3513.935607	390150.757416	41.035290
3513.811237	389991.004692	41.040295
3513.532701	389803.859029	41.045300
3513.226175	389652.636473	41.050304
3513.170054	389488.935171	41.055309
3513.158054	389343.376616	41.060314
3512.502154	389181.086665	41.065319
3512.571742	389019.723580	41.070324
3512.567456	388870.073920	41.075328
3512.182017	388719.721085	41.080333
3512.037294	388573.645566	41.085338
3511.807263	388432.507449	41.090343
3511.642517	388282.879232	41.095348
3511.460953	388132.008783	41.100352
3511.160894	388001.871615	41.105357
3511.248794	387857.075827	41.110362
3510.794850	387728.636733	41.115367
3510.435642	387587.742434	41.120372
3510.594142	387460.450642	41.125376
3510.347505	387341.192961	41.130381
3510.469242	387207.203277	41.135386
3510.125107	387084.125998	41.140391
3510.243347	386963.235697	41.145396
3510.108809	386838.652098	41.150400
3509.667962	386717.162138	41.155405
3509.803980	386589.488617	41.160410
3509.678769	386480.261755	41.165415
3509.612009	386360.514447	41.170420
3509.725926	386251.757158	41.175424
3509.221328	386132.203845	41.180429
3509.192802	386017.958342	41.185434
3509.375913	385910.331321	41.190439
3508.797047	385784.973834	41.195444
3508.801303	385688.874999	41.200448
3508.767792	385577.624222	41.205453
3508.817350	385462.424659	41.210458
3508.592112	385365.776357	41.215463
3508.610867	385265.966787	41.220468
3508.532035	385154.670432	41.225472
3508.121397	385058.227541	41.230477
3508.103806	384957.863842	41.235482
3508.059877	384865.704848	41.240487
3507.842674	384757.348152	41.245492
3507.516193	384671.351462	41.250496
3507.428063	384587.374012	41.255501
3507.696709	384486.557673	41.260506
3507.244214	384404.946857	41.265511
3507.290676	384321.226885	41.270516
3507.442545	384230.736306	41.275520
3507.042307	384150.995461	41.280525
3507.197762	384059.437305	41.285530
3506.990145	383972.023270	41.290535
3506.757696	383888.929281	41.295540
3506.779806	383807.699747	41.300544
3506.638292	383724.108643	41.305549
3506.891434	383641.217593	41.310554
3506.709105	383571.242079	41.315559
3506.457765	383487.565731	41.320564
3506.618705	383412.940517	41.325568
3505.944467	383335.347274	41.330573
3505.977169	383259.091114	41.335578
3506.197790	383199.386299	41.340583
3506.167028	383118.391343	41.345588
3506.382484	383051.577279	41.350592
3506.005523	382988.943334	41.355597
3506.437006	382899.902690	41.360602
3506.183850	382839.915281	41.365607
3505.639889	382771.212691	41.370612
3505.837151	382710.266165	41.375616
3505.830482	382643.866497	41.380621
3505.867292	382568.115505	41.385626
3505.371452	382507.809597	41.390631
3505.465686	382441.901558	41.395636
3505.718356	382377.390679	41.400640
3505.475180	382317.502076	41.405645
3505.772201	382243.639483	41.410650
3505.485688	382175.377710	41.415655
3505.314003	382122.485930	41.420660
3505.546938	382058.205864	41.425664
3505.466419	382002.608009	41.430669
3505.763581	381946.773513	41.435674
3505.429645	381883.546161	41.440679
3505.266282	381814.883383	41.445684
3505.125131	381761.960724	41.450688
3504.999533	381705.835993	41.455693
3505.282543	381640.810702	41.460698
3505.133663	381585.908214	41.465703
3505.007840	381525.872559	41.470708
3505.005962	381470.819986	41.475712
3504.676545	381415.996019	41.480717
3504.717820	381366.192961	41.485722
3504.665970	381311.681092	41.490727
3504.956549	381262.905573	41.495732
3505.167338	381219.373477	41.500736
3505.072414	381155.091417	41.505741
3505.025461	381089.912951	41.510746
3505.060403	381040.567346	41.515751
3504.741101	380987.315325	41.520756
3504.896253	380945.188095	41.525760
3504.512543	380880.366238	41.530765
3504.474636	380824.124390	41.535770
3504.466799	380782.733296	41.540775
3504.849323	380730.565062	41.545780
3504.661351	380679.729817	41.550784
3504.360905	380634.981200	41.555789
3504.915384	380574.608950	41.560794
3504.773270	380520.998282	41.565799
3504.507362	380474.314045	41.570804
3504.917639	380419.829985	41.575808
3504.643616	380368.448849	41.580813
3504.162440	380325.911756	41.585818
3504.312017	380271.391773	41.590823
3504.144742	380222.761751	41.595828
3504.545947	380180.315665	41.600832
3504.356652	380139.104161	41.605837
3504.329473	380081.462345	41.610842
3504.581624	380036.296584	41.615847
3504.073145	379993.433069	41.620852
3504.638291	379943.114075	41.625856
3504.269980	379898.070025	41.630861
3504.506024	379850.239982	41.635866
3503.906110	379801.905062	41.640871
3504.090958	379766.653380	41.645876
3504.565832	379715.509963	41.650880
3504.276195	379672.688056	41.655885
3504.524536	379627.293632	41.660890
3504.661910	379584.100391	41.665895
3504.360614	379535.820095	41.670900
3504.322117	379479.016768	41.675904
3504.150975	379433.763475	41.680909
3504.526590	379395.408768	41.685914
3504.053247	379346.799364	41.690919
3504.147684	379303.155226	41.695924
3504.120185	379245.283073	41.700928
3504.115567	379211.406101	41.705933
3504.267663	379160.565796	41.710938
3503.912841	379127.784434	41.715943
3503.825359	379084.371411	41.720948
3504.122466	379040.847677	41.725952
3503.749332	379002.837480	41.730957
3503.965755	378960.240419	41.735962
3503.723197	378922.666913	41.740967
3503.856930	378871.930496	41.745972
3503.863669	378834.521238	41.750976
3503.870298	378806.051340	41.755981
3504.127186	378751.409939	41.760986
3504.209001	378712.084122	41.765991
3504.061878	378664.133791	41.770996
3504.146858	378616.731367	41.776000
3503.901206	378583.602194	41.781005
3504.055563	378530.855615	41.786010
3503.959505	378498.490342	41.791015
3503.912454	378451.819266	41.796020
3504.129288	378417.119532	41.801024
3503.836369	378376.505525	41.806029
3504.087745	378330.270329	41.811034
3504.331359	378298.690038	41.816039
3503.834732	378255.669483	41.821044
3504.216697	378201.997956	41.826048
3504.125004	378165.263386	41.831053
3504.147461	378116.472987	41.836058
3503.824880	378073.272673	41.841063
3503.948230	378033.710821	41.846068
3504.124723	377983.778753	41.851072
3503.922232	377960.242072	41.856077
3504.125757	377905.073907	41.861082
3503.738956	377869.984855	41.866087
3503.840015	377827.048379	41.871092
3503.893404	377786.151009	41.876096
3503.969698	377737.808686	41.881101
3504.237661	377692.407907	41.886106
3504.114203	377663.398296	41.891111
3503.822533	377600.230285	41.896116
3504.076293	377561.434752	41.901120
3503.496310	377528.178513	41.906125
3503.866303	377481.009090	41.911130
3504.035921	377451.801260	41.916135
3503.947128	377407.522200	41.921140
3503.645752	377365.511116	41.926144
3503.659008	377322.917660	41.931149
3503.645933	377290.258637	41.936154
3503.282890	377256.485750	41.941159
3503.596916	377224.461477	41.946164
3503.472955	377186.867069	41.951168
3503.493322	377150.977184	41.956173
3503.407349	377114.138690	41.961178
3503.518296	377087.174583	41.966183
3503.681378	377048.367022	41.971188
3503.913431	376999.795949	41.976192
3503.448315	376969.619662	41.981197
3503.730483	376918.475472	41.986202
3503.824671	376886.662791	41.991207
3503.467783	376860.634784	41.996212
3503.668257	376818.544750	42.001216
3503.432432	376780.586212	42.006221
3503.490212	376737.883308	42.011226
3503.402558	376708.765501	42.016231
3503.540322	376679.612585	42.021236
3503.863226	376635.065002	42.026240
3503.401890	376614.767574	42.031245
3503.061212	376570.272349	42.036250
3503.502379	376539.446588	42.041255
3503.473287	376501.328495	42.046260
3503.650813	376460.663771	42.051264
3503.286179	376437.049391	42.056269
3503.529424	376395.739387	42.061274
3503.208569	376361.298453	42.066279
3503.253349	376319.308063	42.071284
3503.722799	376281.620048	42.076288
3503.481450	376257.325966	42.081293
3503.602735	376220.149216	42.086298
3503.455890	376191.700421	42.091303
3503.216257	376148.280911	42.096308
3503.669061	376118.595793	42.101312
3503.010316	376090.277346	42.106317
3503.567851	376057.782020	42.111322
3503.696057	376022.458019	42.116327
3503.433434	375987.524973	42.121332
3503.719657	375944.836064	42.126336
3503.276217	375909.677067	42.131341
3503.225994	375864.119530	42.136346
3503.130887	375839.446733	42.141351
3503.281672	375800.817083	42.146356
3503.583511	375767.878622	42.151360
3503.567965	375738.418362	42.156365
3503.664902	375701.981257	42.161370
3503.550242	375664.967455	42.166375
3502.902877	375634.818033	42.171380
3503.375331	375595.477662	42.176384
3503.051802	375567.258897	42.181389
3503.257329	375541.218294	42.186394
3503.503123	375501.786063	42.191399
3503.226137	375474.652121	42.196404
3503.441176	375442.666541	42.201408
3503.212380	375415.067855	42.206413
3503.389673	375366.146780	42.211418
3503.314377	375341.089458	42.216423
3503.369161	375299.146728	42.221428
3503.353238	375271.311576	42.226432
3502.881158	375242.861597	42.231437
3503.193160	375214.010181	42.236442
3503.184354	375185.894441	42.241447
3503.635215	375152.246259	42.246452
3503.089200	375112.098496	42.251456
3503.121103	375082.782538	42.256461
3503.392717	375052.743459	42.261466
3503.172257	375011.960698	42.266471
3503.128947	374982.224543	42.271476
3503.014678	374946.174887	42.276480
3503.048862	374921.887531	42.281485
3503.062000	374894.352267	42.286490
3503.061651	374870.248037	42.291495
3502.896661	374838.854279	42.296500
3503.069978	374816.196161	42.301504
3503.052528	374785.312778	42.306509
3503.180768	374754.279689	42.311514
3503.312766	374734.040917	42.316519
3502.987326	374692.207220	42.321524
3503.331423	374668.049211	42.326528
3503.108931	374639.178762	42.331533
3503.245116	374604.461276	42.336538
3503.343475	374575.642431	42.341543
3502.925012	374544.592577	42.346548
3502.876009	374509.675188	42.351552
3502.847439	374478.361387	42.356557
3503.141344	374451.696389	42.361562
3503.676736	374417.272146	42.366567
3503.000393	374390.148467	42.371572
3503.400418	374356.151614	42.376576
3502.842548	374324.894603	42.381581
3502.909277	374292.194147	42.386586
3503.167186	374254.688647	42.391591
3502.771463	374232.220197	42.396596
3503.090539	374202.299800	42.401600
3502.828175	374180.801168	42.406605
3502.980226	374154.462760	42.411610
3503.167801	374120.727278	42.416615
3502.743954	374103.063776	42.421620
3502.863024	374079.905482	42.426624
3503.127150	374055.251369	42.431629
3503.167020	374026.568050	42.436634
3503.069570	373991.759141	42.441639
3503.149726	373972.315290	42.446644
3503.301537	373925.529246	42.451648
3502.897323	373899.988372	42.456653
3502.990827	373869.543900	42.461658
3502.984933	373839.089462	42.466663
3502.521495	373823.006781	42.471668
3503.392920	373778.318367	42.476672
3502.946621	373753.241118	42.481677
3503.212902	373723.404617	42.486682
3503.002402	373700.195685	42.491687
3502.953493	373663.346741	42.496692
3503.151042	373626.230789	42.501696
3502.983969	373612.083135	42.506701
3503.181391	373577.837437	42.511706
3503.390013	373547.349293	42.516711
3502.780631	373521.458979	42.521716
3502.905519	373489.281936	42.526720
3503.107601	373461.411018	42.531725
3503.013291	373434.272023	42.536730
3502.904458	373403.045687	42.541735
3502.868438	373379.656927	42.546740
3502.898925	373340.966317	42.551744
3502.818169	373316.365210	42.556749
3503.081973	373291.481852	42.561754
3503.473675	373262.793789	42.566759
3502.932032	373240.067819	42.571764
3503.046261	373207.409483	42.576768
3503.174903	373174.698063	42.581773
3503.324995	373138.325476	42.586778
3503.360069	373114.874625	42.591783
3502.959362	373084.938013	42.596788
3503.078846	373040.898846	42.601792
3502.713311	373018.221492	42.606797
3502.934136	372994.716232	42.611802
3503.177897	372964.577597	42.616807
3502.703373	372947.124448	42.621812
3503.145001	372905.778297	42.626816
3502.835837	372890.687124	42.631821
3503.107042	372852.745820	42.636826
3503.287082	372825.360320	42.641831
3502.742909	372793.743810	42.646836
3502.899236	372752.746646	42.651840
3502.768010	372731.429687	42.656845
3503.006267	372706.194155	42.661850
3502.774774	372677.018222	42.666855
3502.686793	372653.789343	42.671860
3503.069643	372624.492354	42.676864
3503.064507	372607.346974	42.681869
3502.925612	372575.209915	42.686874
3503.127940	372542.486280	42.691879
3502.773903	372518.612838	42.696884
3503.054589	372479.145433	42.701888
3502.856321	372447.169876	42.706893
3502.953784	372413.166907	42.711898
3503.015326	372400.430969	42.716903
3502.634927	372366.502304	42.721908
3502.595813	372342.325684	42.726912
3502.934015	372332.569507	42.731917
3502.811587	372295.399952	42.736922
3503.029719	372279.896164	42.741927
3502.841848	372249.798518	42.746932
3502.934535	372214.881572	42.751936
3502.228767	372192.561311	42.756941
3502.697424	372164.291974	42.761946
3502.782122	372140.121313	42.766951
3502.415277	372121.812612	42.771956
3502.803833	372089.821532	42.776960
3502.500498	372086.617280	42.781965
3502.823426	372047.244297	42.786970
3503.022692	372025.875366	42.791975
3502.740143	372001.152077	42.796980
3502.958100	371965.072218	42.801985
3502.651791	371946.017310	42.806989
3502.641073	371917.365076	42.811994
3503.076282	371885.366502	42.816999
3502.753248	371868.371744	42.822004
3503.134651	371836.737122	42.827009
3502.807558	371810.420235	42.832013
3502.622240	371783.065160	42.837018
3503.054069	371760.440513	42.842023
3502.913672	371733.052995	42.847028
3502.875723	371700.441967	42.852033
3502.556008	371682.913124	42.857037
3502.751808	371652.780530	42.862042
3502.953347	371632.096816	42.867047
3502.683452	371606.482112	42.872052
3503.116429	371579.818106	42.877057
3502.595870	371551.549666	42.882061
3502.274050	371519.922504	42.887066
3502.533048	371501.160365	42.892071
3502.686494	371485.107339	42.897076
3502.466278	371462.152069	42.902081
3502.515801	371435.090345	42.907085
3502.707298	371419.666433	42.912090
3503.041270	371383.491559	42.917095
3502.484568	371369.962253	42.922100
3502.816587	371335.946872	42.927105
3502.606383	371309.535114	42.932109
3502.643655	371284.304165	42.937114
3502.803015	371268.631141	42.942119
3502.345171	371230.902686	42.947124
3502.641568	371210.584945	42.952129
3502.601946	371190.040045	42.957133
3502.547169	371172.774490	42.962138
3502.796640	371138.187442	42.967143
3502.761428	371128.006293	42.972148
3503.040089	371102.178748	42.977153
3502.671895	371075.232483	42.982157
3502.665698	371050.617765	42.987162
3502.578560	371029.191027	42.992167
3502.612019	371000.251541	42.997172
3503.099708	370977.515956	43.002177
3502.614554	370956.913198	43.007181
3502.856332	370933.352132	43.012186
3502.983010	370908.056124	43.017191
3502.598151	370882.179208	43.022196
3502.906171	370841.231836	43.027201
3502.880424	370823.453480	43.032205
3502.669654	370793.815086	43.037210
3503.141091	370775.679894	43.042215
3502.690263	370751.819997	43.047220
3503.189794	370716.736254	43.052225
3502.943938	370695.359363	43.057229
3502.529266	370669.817136	43.062234
3502.823324	370634.993897	43.067239
3502.656687	370606.898057	43.072244
3502.517086	370582.278284	43.077249
3502.536531	370564.797575	43.082253
3502.413867	370539.438422	43.087258
3502.885878	370526.256699	43.092263
3502.577177	370497.166709	43.097268
3503.018184	370465.775301	43.102273
3502.730709	370450.908062	43.107277
3502.676129	370421.041738	43.112282
3502.510795	370402.548127	43.117287
3502.564885	370375.941938	43.122292
3502.853172	370349.172260	43.127297
3502.638123	370317.628739	43.132301
3502.585405	370293.630289	43.137306
3502.924961	370275.058027	43.142311
3502.484142	370249.494081	43.147316
3502.538957	370221.439607	43.152321
3502.214178	370195.730536	43.157325
3502.016093	370179.960103	43.162330
3502.554772	370152.897234	43.167335
3502.856086	370136.693407	43.172340
3502.934765	370116.713605	43.177345
3502.652796	370083.859223	43.182349
3502.736852	370059.229592	43.187354
3502.838489	370026.467874	43.192359
3502.893206	369999.480169	43.197364
3503.093259	369976.534495	43.202369
3502.582169	369943.283732	43.207373
3502.475141	369921.528989	43.212378
3502.388898	369899.186697	43.217383
3502.248908	369876.217643	43.222388
3502.613752	369857.641171	43.227393
3502.586288	369837.195006	43.232397
3502.198255	369817.668683	43.237402
3502.739743	369796.321013	43.242407
3502.346570	369782.714682	43.247412
3502.422131	369751.531774	43.252417
3502.168275	369743.543522	43.257421
3502.040668	369711.503031	43.262426
3502.368893	369710.359602	43.267431
3502.451751	369687.254099	43.272436
3502.463363	369659.282002	43.277441
3502.180910	369645.709184	43.282445
3502.393763	369620.703465	43.287450
3502.561197	369598.473887	43.292455
3502.495494	369586.493202	43.297460
3502.490124	369560.225755	43.302465
3502.435719	369526.522365	43.307469
3502.375220	369508.494541	43.312474
3502.636790	369494.176473	43.317479
3502.325930	369474.637903	43.322484
3502.579418	369443.350754	43.327489
3502.435032	369434.405406	43.332493
3502.546288	369415.537845	43.337498
3502.559360	369392.493770	43.342503
3502.344209	369369.002501	43.347508
3502.340345	369344.081070	43.352513
3502.514808	369330.462404	43.357517
3502.353263	369310.494009	43.362522
3502.581890	369280.099716	43.367527
3502.275680	369270.442758	43.372532
3502.589867	369231.981765	43.377537
3502.587714	369224.563914	43.382541
3502.713245	369200.689227	43.387546
3502.595212	369175.658391	43.392551
3502.468865	369160.282703	43.397556
3502.824699	369129.207925	43.402561
3502.567123	369110.346746	43.407565
3502.524586	369088.657542	43.412570
3502.661788	369062.367447	43.417575
3502.228916	369038.350873	43.422580
3502.197418	369021.613883	43.427585
3502.552589	369002.327015	43.432589
3502.461865	368970.635617	43.437594
3502.352395	368952.894516	43.442599
3502.153675	368941.010472	43.447604
3502.217018	368915.951182	43.452609
3502.476665	368907.222251	43.457613
3502.196192	368878.354845	43.462618
3502.365948	368864.558852	43.467623
3502.185320	368849.623331	43.472628
3502.530452	368819.896357	43.477633
3502.374596	368804.245610	43.482637
3501.969519	368781.316919	43.487642
3502.408581	368753.810923	43.492647
3502.116087	368745.498132	43.497652
3502.216694	368717.409636	43.502657
3502.020719	368697.420762	43.507661
3502.419254	368696.037705	43.512666
3502.556827	368653.309908	43.517671
3502.385574	368646.654977	43.522676
3502.550647	368613.449862	43.527681
3502.774475	368601.372896	43.532685
3502.222520	368581.845822	43.537690
3502.398420	368554.888695	43.542695
3502.394955	368551.840615	43.547700
3502.667559	368519.812715	43.552705
3502.716377	368511.599176	43.557709
3502.782246	368472.769310	43.562714
3502.514493	368441.130276	43.567719
3502.119819	368429.657595	43.572724
3502.411385	368407.661824	43.577729
3502.486808	368395.938138	43.582733
3502.748938	368375.268015	43.587738
3502.738095	368344.249441	43.592743
3502.419280	368312.719832	43.597748
3502.449670	368288.173232	43.602753
3502.393222	368272.506723	43.607757
3501.898245	368250.633228	43.612762
3502.236175	368227.461440	43.617767
3502.077605	368218.111423	43.622772
3502.323141	368197.494566	43.627777
3502.420607	368177.434258	43.632781
3502.118229	368169.707169	43.637786
3502.502617	368140.811772	43.642791
3502.110176	368121.386588	43.647796
3502.449985	368102.304750	43.652801
3502.625659	368084.518735	43.657805
3502.501895	368062.231647	43.662810
3502.729298	368038.645005	43.667815
3502.498428	368029.153742	43.672820
3502.218316	367997.821009	43.677825
3502.519651	367980.701337	43.682829
3502.273784	367948.016704	43.687834
3502.574763	367931.608426	43.692839
3502.198816	367918.430421	43.697844
3502.445932	367892.909732	43.702849
3502.491514	367872.857284	43.707853
3502.063384	367855.927269	43.712858
3502.275962	367832.342764	43.717863
3502.356693	367820.465579	43.722868
3502.356985	367801.182312	43.727873
3502.487459	367783.987486	43.732877
3502.430975	367763.163252	43.737882
3502.301159	367735.541553	43.742887
3502.510675	367723.314006	43.747892
3502.392200	367693.937473	43.752897
3502.629139	367674.820546	43.757901
3502.707777	367646.200885	43.762906
3502.686707	367621.687127	43.767911
3502.225815	367599.655390	43.772916
3502.382914	367583.269303	43.777921
3502.293572	367567.124806	43.782925
3502.217702	367538.859364	43.787930
3502.559457	367527.220909	43.792935
3502.514792	367500.195486	43.797940
3502.416905	367480.215901	43.802945
3502.219020	367463.173605	43.807949
3502.300400	367444.766706	43.812954
3502.494067	367416.281355	43.817959
3502.182700	367400.374566	43.822964
3502.484908	367375.403787	43.827969
3502.581326	367364.413200	43.832973
3502.450230	367348.071826	43.837978
3502.410535	367322.442822	43.842983
3502.312817	367302.996626	43.847988
3502.284535	367274.596485	43.852993
3502.378270	367257.635720	43.857997
3502.583811	367245.510216	43.863002
3502.668088	367221.310009	43.868007
3502.545427	367209.896134	43.873012
3502.814565	367176.952634	43.878017
3502.534858	367155.273461	43.883021
3502.644568	367140.368086	43.888026
3502.931865	367112.960353	43.893031
3502.402280	367088.804746	43.898036
3502.477177	367058.076318	43.903041
3502.609815	367037.425383	43.908045
3502.354876	367014.167027	43.913050
3502.623913	366976.192757	43.918055
3502.648851	366975.629963	43.923060
3502.405837	366946.830997	43.928065
3502.573396	366913.013760	43.933069
3502.454612	366902.564624	43.938074
3502.299296	366884.092571	43.943079
3502.343290	366867.215538	43.948084
3502.385188	366830.114852	43.953089
3502.597272	366824.085833	43.958093
3502.315212	366801.009373	43.963098
3502.842719	366770.997826	43.968103
3502.277886	366750.201150	43.973108
3502.433115	366726.218150	43.978113
3502.480441	366708.781549	43.983117
3502.260342	366693.444530	43.988122
3502.392517	366661.512632	43.993127
3502.464429	366653.320375	43.998132
3502.563086	366624.772804	44.003137
3502.607139	366609.521671	44.008141
3502.773086	366590.262629	44.013146
3502.384158	366556.836458	44.018151
3502.188792	366548.711170	44.023156
3502.676693	366522.923132	44.028161
3502.323854	366498.409230	44.033165
3502.082703	366470.244680	44.038170
3502.496850	366456.816017	44.043175
3502.108173	366441.200208	44.048180
3502.179811	366412.631225	44.053185
3502.201997	366410.595221	44.058189
3502.234306	366384.827141	44.063194
3502.569986	366368.768278	44.068199
3502.337310	366342.838138	44.073204
3502.403125	366325.042724	44.078209
3502.177368	366303.583182	44.083213
3502.190674	366283.560057	44.088218
3502.396501	366258.654126	44.093223
3502.175312	366254.216862	44.098228
3502.538675	366226.389932	44.103233
3502.393534	366211.981072	44.108237
3502.329226	366179.774327	44.113242
3502.123624	366171.193188	44.118247
3502.380351	366136.039973	44.123252
3502.421196	366117.613128	44.128257
3502.336533	366098.214903	44.133261
3501.778266	366085.216872	44.138266
3502.276205	366069.869417	44.143271
3502.074641	366061.058948	44.148276
3502.021125	366038.657730	44.153281
3502.217386	366013.702262	44.158285
3502.039730	366005.904366	44.163290
3502.509067	365989.341748	44.168295
3502.342897	365975.139303	44.173300
3502.271928	365955.383144	44.178305
3501.898775	365935.750217	44.183309
3502.105021	365929.188357	44.188314
3502.253637	365894.890131	44.193319
3502.117993	365887.644637	44.198324
3502.235646	365868.189368	44.203329
3502.395385	365856.985092	44.208333
3501.986970	365843.353844	44.213338
3502.201615	365814.762019	44.218343
3502.023393	365803.737353	44.223348
3502.245360	365783.173254	44.228353
3501.874846	365773.957054	44.233357
3501.792197	365760.122627	44.238362
3502.150689	365741.163362	44.243367
3502.005325	365722.841466	44.248372
3502.051880	365707.818141	44.253377
3501.954116	365689.336369	44.258381
3502.161867	365686.737869	44.263386
3502.438472	365654.553715	44.268391
3502.278928	365650.640334	44.273396
3502.185000	365629.718755	44.278401
3502.370096	365611.396182	44.283405
3502.319230	365593.288172	44.288410
3502.688277	365566.298193	44.293415
3502.459823	365549.361156	44.298420
3502.376298	365518.096768	44.303425
3502.058158	365495.685494	44.308429
3501.881823	365471.295705	44.313434
3502.309653	365463.632115	44.318439
3502.414277	365441.459910	44.323444
3502.171773	365433.443277	44.328449
3502.042497	365402.998948	44.333453
3502.124387	365394.906416	44.338458
3502.646188	365373.685572	44.343463
3502.221169	365368.847949	44.348468
3502.505003	365338.771209	44.353473
3502.344481	365320.248152	44.358477
3501.896833	365299.635462	44.363482
3501.993172	365282.698545	44.368487
3502.296076	365280.745820	44.373492
3502.485292	365260.288082	44.378497
3502.525569	365229.918821	44.383501
3502.054442	365201.331475	44.388506
3502.394792	365196.857482	44.393511
3502.123753	365171.796152	44.398516
3502.289330	365158.507205	44.403521
3502.109722	365141.536921	44.408525
3502.013820	365126.306788	44.413530
3502.154833	365111.573359	44.418535
3502.080096	365081.043981	44.423540
3501.891533	365071.519750	44.428545
3501.863544	365059.099362	44.433549
3502.061513	365040.317073	44.438554
3502.019615	365026.069418	44.443559
3502.127246	365018.811260	44.448564
3502.109017	364992.973585	44.453569
3502.417798	364972.293772	44.458573
3502.044112	364970.293860	44.463578
3502.402283	364948.488364	44.468583
3502.531052	364925.981698	44.473588
3502.320053	364906.399069	44.478593
3502.076145	364875.031905	44.483597
3502.200351	364869.498923	44.488602
3502.272173	364836.202342	44.493607
3502.241266	364830.490220	44.498612
3501.791347	364803.957292	44.503617
3502.155382	364791.348742	44.508621
3502.014549	364784.891454	44.513626
3502.557426	364762.498083	44.518631
3502.503923	364742.687565	44.523636
3502.307755	364710.880847	44.528641
3502.004726	364708.819104	44.533645
3502.244413	364699.024840	44.538650
3502.294025	364663.063586	44.543655
3502.119646	364659.177788	44.548660
3502.284869	364638.748759	44.553665
3501.956926	364617.634190	44.558669
3501.841663	364602.762522	44.563674
3501.876170	364589.163397	44.568679
3502.151077	364586.528941	44.573684
3502.100436	364564.481868	44.578689
3502.280670	364556.754936	44.583693
3502.264639	364531.755009	44.588698
3502.322538	364501.890431	44.593703
3502.461257	364501.335292	44.598708
3502.103726	364479.234275	44.603713
3502.234613	364454.236829	44.608717
3502.126139	364437.991930	44.613722
3502.294843	364415.834385	44.618727
3502.056362	364401.515381	44.623732
3502.250277	364376.889198	44.628737
3502.138097	364371.545361	44.633741
3501.925004	364348.303766	44.638746
3502.159357	364322.146695	44.643751
3502.041555	364318.455321	44.648756
3502.346549	364291.397907	44.653761
3502.413245	364286.661451	44.658765
3502.132328	364260.432051	44.663770
3502.357020	364241.391000	44.668775
3502.303479	364221.656364	44.673780
3502.260379	364208.069139	44.678785
3502.360565	364179.950894	44.683789
3502.200286	364172.276849	44.688794
3502.228719	364142.924677	44.693799
3502.183569	364135.181888	44.698804
3502.191185	364118.690063	44.703809
3502.469580	364102.105274	44.708813
3502.205792	364083.470456	44.713818
3501.833306	364060.761624	44.718823
3502.062541	364053.560533	44.723828
3501.889736	364018.624068	44.728833
3502.299800	364007.253084	44.733837
3501.457295	364005.580154	44.738842
3502.006249	363978.001709	44.743847
3502.267281	363972.599723	44.748852
3501.764956	363960.201863	44.753857
3502.292998	363943.933870	44.758861
3501.886953	363940.388941	44.763866
3502.389042	363908.015323	44.768871
3501.822391	363903.072447	44.773876
3501.964291	363877.844111	44.778881
3502.151090	363856.115292	44.783885
3502.067678	363849.039031	44.788890
3502.132471	363826.312792	44.793895
3501.976647	363814.089636	44.798900
3501.912165	363804.901419	44.803905
3502.034941	363781.302194	44.808909
3501.914759	363770.166090	44.813914
3502.082183	363748.821352	44.818919
3501.786697	363736.035474	44.823924
3502.131378	363725.513077	44.828929
3502.177550	363716.485481	44.833933
3501.903248	363697.953694	44.838938
3502.018760	363675.803869	44.843943
3502.452414	363660.846306	44.848948
3502.280409	363643.492825	44.853953
3502.501647	363623.511750	44.858957
3502.162043	363617.872839	44.863962
3502.743007	363584.698890	44.868967
3502.352233	363567.176128	44.873972
3502.390576	363537.186564	44.878977
3502.419876	363526.154156	44.883981
3502.174753	363500.706215	44.888986
3502.375746	363475.874899	44.893991
3502.030632	363468.178613	44.898996
3502.152634	363440.894796	44.904001
3502.116512	363436.021743	44.909005
3501.920930	363419.611967	44.914010
3502.202675	363395.454087	44.919015
3502.088641	363391.202990	44.924020
3502.492536	363366.009678	44.929025
3502.200575	363344.431214	44.934029
3501.981222	363337.198114	44.939034
3502.042336	363328.803326	44.944039
3501.965918	363303.379782	44.949044
3501.998008	363291.127168	44.954049
3502.073203	363277.241596	44.959053
3501.970471	363259.978750	44.964058
3502.308123	363240.843245	44.969063
3502.366049	363236.209625	44.974068
3502.144710	363215.509432	44.979073
3502.101887	363197.881485	44.984077
3501.517362	363176.373834	44.989082
3501.909456	363161.701999	44.994087
3501.983338	363149.569874	44.999092
3501.501037	363135.491476	45.004097
3501.654356	363117.070652	45.009101
3501.570174	363123.741269	45.014106
3502.017174	363110.864991	45.019111
3501.855522	363097.219472	45.024116
3501.947345	363079.722963	45.029121
3501.805553	363070.826061	45.034125
3501.855618	363066.219048	45.039130
3501.752499	363040.138767	45.044135
3501.861259	363033.235688	45.049140
3501.830421	363025.642842	45.054145
3501.966943	362996.348942	45.059149
3501.931244	362994.118425	45.064154
3501.914306	362986.625047	45.069159
3502.021268	362962.392371	45.074164
3502.001569	362945.599218	45.079169
3502.164602	362931.293248	45.084173
3502.014148	362926.641186	45.089178
3501.969735	362906.091117	45.094183
3502.381873	362888.824165	45.099188
3502.351551	362884.559969	45.104193
3502.310938	362848.559722	45.109197
3501.738591	362842.804417	45.114202
3501.705986	362827.410780	45.119207
3502.006826	362812.143121	45.124212
3502.021610	362792.651002	45.129217
3502.015075	362777.431157	45.134221
3502.049199	362758.495038	45.139226
3502.114463	362746.160805	45.144231
3501.783955	362732.795499	45.149236
3501.855840	362704.604024	45.154241
3501.603308	362704.440074	45.159245
3501.753105	362700.910140	45.164250
3502.077615	362690.619211	45.169255
3502.139180	362674.346880	45.174260
3502.087649	362659.311850	45.179265
3502.215372	362640.640608	45.184269
3501.787179	362633.439834	45.189274
3502.028742	362613.785255	45.194279
3501.866021	362598.792907	45.199284
3502.016749	362582.938634	45.204289
3502.016240	362573.104812	45.209293
3501.918073	362550.199666	45.214298
3502.144498	362537.281232	45.219303
3501.972451	362521.756672	45.224308
3501.928673	362499.935686	45.229313
3502.046173	362480.783129	45.234317
3501.579583	362475.392457	45.239322
3501.969964	362453.681751	45.244327
3501.755315	362445.761609	45.249332
3501.623712	362438.285937	45.254337
3501.806297	362406.671903	45.259341
3501.598170	362403.146810	45.264346
3501.733729	362393.215522	45.269351
3502.006197	362390.225502	45.274356
3501.860505	362375.179570	45.279361
3501.751545	362361.652567	45.284365
3501.584869	362365.032778	45.289370
3501.835174	362344.461869	45.294375
3502.237422	362332.151259	45.299380
3501.772147	362317.155029	45.304385
3502.242289	362298.099945	45.309389
3501.822093	362287.111612	45.314394
3502.237130	362272.766112	45.319399
3502.450643	362251.667235	45.324404
3501.959287	362240.003861	45.329409
3501.905985	362216.303737	45.334413
3502.133477	362201.250467	45.339418
3502.008484	362186.658617	45.344423
3502.143497	362163.869355	45.349428
3501.558302	362152.423838	45.354433
3501.830380	362148.468234	45.359437
3501.749197	362135.190917	45.364442
3502.090645	362118.925552	45.369447
3502.174371	362111.517934	45.374452
3501.903484	362099.235742	45.379457
3502.157243	362079.604325	45.384461
3501.879147	362069.534011	45.389466
3502.172526	362037.800701	45.394471
3502.028284	362025.956172	45.399476
3501.928199	362020.838729	45.404481
3502.230482	362009.661633	45.409485
3501.984016	362006.955616	45.414490
3501.927804	361977.741528	45.419495
3502.081909	361965.596437	45.424500
3501.866830	361950.688144	45.429505
3502.499468	361928.380313	45.434509
3501.960045	361923.915678	45.439514
3501.928072	361889.818771	45.444519
3501.816389	361883.483367	45.449524
3501.771635	361869.717448	45.454529
3501.971728	361852.787831	45.459533
3501.827467	361836.623307	45.464538
3502.105169	361823.162947	45.469543
3502.119788	361817.951385	45.474548
3502.058476	361800.681246	45.479553
3501.808887	361782.423940	45.484557
3502.025297	361769.481321	45.489562
3501.895268	361750.138113	45.494567
3502.063966	361743.682814	45.499572
3501.955203	361725.403559	45.504577
3502.020728	361716.905984	45.509581
3502.160392	361712.716814	45.514586
3501.922243	361672.451353	45.519591
3501.981685	361665.657279	45.524596
3501.686649	361655.462403	45.529601
3502.005884	361630.433268	45.534605
3502.048990	361629.283080	45.539610
3502.065572	361613.169641	45.544615
3502.175939	361596.075960	45.549620
3501.999561	361583.982142	45.554625
3502.243940	361563.055857	45.559629
3502.128003	361543.430795	45.564634
3502.121257	361529.506336	45.569639
3502.205598	361519.125319	45.574644
3501.949938	361505.163348	45.579649
3502.304022	361470.599303	45.584653
3502.202098	361456.079741	45.589658
3502.215532	361438.416587	45.594663
3502.125397	361422.116358	45.599668
3502.315596	361411.896714	45.604673
3502.359820	361391.941689	45.609677
3502.076830	361385.556602	45.614682
3501.905532	361359.815811	45.619687
3502.062642	361348.635649	45.624692
3502.204380	361329.834348	45.629697
3502.347986	361307.297214	45.634701
3501.931605	361308.734282	45.639706
3502.002377	361267.073380	45.644711
3501.849098	361258.482665	45.649716
3502.013831	361246.005276	45.654721
3502.103127	361228.330193	45.659725
3502.298904	361220.904918	45.664730
3502.023028	361205.522889	45.669735
3501.753123	361183.431188	45.674740
3501.823774	361176.889378	45.679745
3501.924924	361166.022798	45.684749
3501.779133	361143.327280	45.689754
3501.629950	361138.750976	45.694759
3501.702715	361126.237024	45.699764
3501.520915	361114.525039	45.704769
3501.993562	361096.561517	45.709773
3501.889785	361094.468511	45.714778
3501.957629	361074.357128	45.719783
3502.016608	361058.897505	45.724788
3501.653593	361059.106504	45.729793
3501.809023	361045.181996	45.734797
3502.082887	361028.062550	45.739802
3501.970931	361015.297765	45.744807
3501.864499	361001.947638	45.749812
3502.154170	360981.115549	45.754817
3502.127405	360947.067584	45.759821
3502.061262	360894.119093	45.764826
3501.717319	360782.943578	45.769831
3501.285548	360632.061851	45.774836
3500.879214	360446.004527	45.779841
3500.852396	360203.674147	45.784845
3499.845607	359922.002636	45.789850
3498.961314	359612.456590	45.794855
3498.305709	359257.076715	45.799860
3497.396522	358853.471324	45.804865
3496.388953	358424.309248	45.809869
3495.258464	357955.894797	45.814874
3494.210219	357438.968628	45.819879
3493.164954	356897.787021	45.824884
3491.788850	356321.675172	45.829889
3490.202806	355701.640378	45.834893
3488.811212	355056.298614	45.839898
3487.316949	354377.433939	45.844903
3486.098869	353659.749193	45.849908
3483.824249	352920.047612	45.854913
3482.248940	352148.801912	45.859917
3480.115624	351344.553302	45.864922
3478.176528	350516.333784	45.869927
3475.786067	349659.818842	45.874932
3473.659525	348784.657104	45.879937
3471.525317	347882.169576	45.884941
3469.291780	346956.970091	45.889946
3467.244533	346003.597205	45.894951
3464.934901	345041.543056	45.899956
3462.119026	344044.224631	45.904961
3459.509528	343033.496442	45.909965
3456.921735	342009.081187	45.914970
3454.866696	340953.073584	45.919975
3452.068204	339891.708444	45.924980
3449.345740	338803.904365	45.929985
3446.346725	337698.360334	45.934989
3443.363864	336587.643182	45.939994
3440.917742	335459.973251	45.944999
3438.056719	334310.614431	45.950004
3434.951120	333154.569563	45.955009
3432.059208	331969.588736	45.960013
3428.806086	330795.055743	45.965018
3425.751779	329607.382428	45.970023
3422.858887	328402.911011	45.975028
3419.661758	327183.874997	45.980033
3416.608564	325962.083202	45.985037
3413.439671	324730.402562	45.990042
3409.998134	323483.769207	45.995047
3406.889659	322227.379542	46.000052
3403.514672	320983.002069	46.005057
3400.809353	319703.985467	46.010061
3397.074821	318434.759420	46.015066
3393.807601	317149.547580	46.020071
3390.231612	315872.030794	46.025076
3386.543888	314596.810782	46.030081
3383.645978	313286.190851	46.035085
3379.793131	311990.364955	46.040090
3376.228951	310693.338990	46.045095
3373.161753	309375.766494	46.050100
3369.478039	308069.782289	46.055105
3366.231748	306746.466880	46.060109
3362.649151	305433.730507	46.065114
3359.136123	304104.865295	46.070119
3355.233279	302779.513571	46.075124
3351.719861	301463.077825	46.080129
3348.267905	300133.645385	46.085133
3344.628768	298803.242673	46.090138
3341.231957	297483.180874	46.095143
3337.789554	296146.423422	46.100148
3333.685817	294813.581658	46.105153
3330.388582	293476.027932	46.110157
3326.813284	292142.458838	46.115162
3323.158737	290811.622396	46.120167
3319.524784	289468.509990	46.125172
3315.580441	288134.862268	46.130177
3311.935742	286790.066747	46.135181
3308.327130	285463.848360	46.140186
3304.561026	284113.086810	46.145191
3301.064393	282781.860644	46.150196
3297.329016	281457.953739	46.155201
3293.654185	280121.996453	46.160205
3289.758970	278789.766913	46.165210
3286.111379	277455.413474	46.170215
3282.719884	276121.124956	46.175220
3279.210605	274788.284129	46.180225
3275.622607	273451.054771	46.185229
3271.627604	272125.071318	46.190234
3267.850929	270784.978494	46.195239
3264.217637	269448.281089	46.200244
3260.508447	268118.120503	46.205249
3256.407533	266787.875213	46.210253
3252.701328	265465.164515	46.215258
3248.679760	264145.541628	46.220263
3245.176733	262822.587661	46.225268
3241.193988	261511.890249	46.230273
3237.485514	260189.191864	46.235277
3233.806576	258891.175828	46.240282
3230.215833	257581.494484	46.245287
3226.500162	256284.144851	46.250292
3222.322548	254976.667968	46.255297
3219.232908	253665.622494	46.260301
3215.363900	252368.133072	46.265306
3211.566934	251071.258157	46.270311
3207.862613	249772.957708	46.275316
3203.914186	248478.148919	46.280321
3200.736946	247182.854255	46.285325
3196.634948	245889.986808	46.290330
3193.065967	244602.860347	46.295335
3189.045825	243317.273607	46.300340
3185.306245	242035.685560	46.305345
3181.436350	240741.580813	46.310349
3177.368696	239473.249343	46.315354
3174.069503	238205.327732	46.320359
3170.125244	236936.890361	46.325364
3166.646005	235661.194036	46.330369
3163.063359	234382.708289	46.335373
3158.811942	233125.105790	46.340378
3155.157684	231869.215811	46.345383
3151.517319	230602.242300	46.350388
3147.423641	229358.718000	46.355393
3143.948321	228094.440712	46.360397
3140.304655	226854.588075	46.365402
3136.729429	225605.071600	46.370407
3132.990901	224355.988102	46.375412
3128.645779	223122.000807	46.380417
3125.309978	221879.707342	46.385421
3121.292913	220640.017319	46.390426
3117.622555	219410.182689	46.395431
3113.220943	218180.336860	46.400436
3109.800490	216949.628027	46.405441
3106.084789	215734.427940	46.410445
3102.152277	214515.368508	46.415450
3098.796707	213298.923055	46.420455
3095.170846	212094.214212	46.425460
3091.217956	210888.593316	46.430465
3087.705557	209666.966028	46.435469
3083.708371	208469.385577	46.440474
3079.983741	207271.488632	46.445479
3076.248373	206076.095702	46.450484
3072.385371	204889.948830	46.455489
3068.840202	203696.399561	46.460493
3064.656777	202519.893120	46.465498
3060.776698	201328.423560	46.470503
3057.311294	200158.519465	46.475508
3053.389160	198994.093990	46.480513
3049.999044	197816.581155	46.485517
3046.010847	196646.326940	46.490522
3042.312943	195487.140579	46.495527
3038.697283	194328.893618	46.500532
3034.831994	193183.861624	46.505537
3031.148513	192031.121204	46.510541
3027.282428	190885.423123	46.515546
3023.055670	189740.250745	46.520551
3019.497612	188597.226771	46.525556
3015.553490	187469.859035	46.530561
3011.965549	186332.134773	46.535565
3008.077059	185214.739077	46.540570
3004.400400	184092.153687	46.545575
3000.698931	182976.740221	46.550580
2996.723576	181864.896311	46.555585
2992.922082	180758.564051	46.560589
2989.074791	179656.173622	46.565594
2985.137410	178554.141940	46.570599
2981.740128	177472.918927	46.575604
2978.000885	176389.713302	46.580609
2974.141605	175298.940393	46.585613
2969.937074	174233.696709	46.590618
2966.264704	173156.379930	46.595623
2962.559851	172075.506015	46.600628
2958.505855	171021.014426	46.605633
2954.600892	169959.029499	46.610637
2950.759705	168917.468181	46.615642
2947.028316	167879.914617	46.620647
2943.107289	166840.152772	46.625652
2939.224506	165808.407080	46.630657
2935.195317	164773.212132	46.635661
2931.079883	163757.699490	46.640666
2927.265321	162750.874615	46.645671
2923.692612	161740.349316	46.650676
2919.486263	160750.748838	46.655681
2915.421879	159774.696924	46.660685
2911.735458	158795.648807	46.665690
2907.699124	157827.310932	46.670695
2903.804148	156850.235855	46.675700
2899.543812	155900.902101	46.680705
2896.023636	154948.999614	46.685709
2891.630283	154014.900409	46.690714
2887.778429	153088.749858	46.695719
2883.981774	152165.354835	46.700724
2879.954473	151259.318291	46.705729
2875.853097	150343.445872	46.710733
2871.757913	149457.963674	46.715738
2867.644513	148575.209460	46.720743
2863.539266	147707.624250	46.725748
2859.014954	146851.952756	46.730753
2854.825357	145993.571176	46.735757
2850.520300	145178.612223	46.740762
2846.201714	144357.026466	46.745767
2842.249153	143563.021039	46.750772
2837.278924	142780.879869	46.755777
2833.291712	142000.086843	46.760781
2829.059302	141243.289942	46.765786
2824.740922	140506.582793	46.770791
2820.480836	139780.336245	46.775796
2816.065175	139099.583692	46.780801
2811.623872	138302.649203	46.785805
2807.656848	137619.863631	46.790810
2803.625611	136939.706198	46.795815
2799.475104	136280.212582	46.800820
2795.504949	135638.956344	46.805825
2791.592401	135005.142432	46.810829
2787.350771	134373.805772	46.815834
2783.591133	133755.913112	46.820839
2779.701409	133147.310328	46.825844
2775.928661	132553.339626	46.830849
2772.094661	131968.240224	46.835853
2768.393663	131382.212122	46.840858
2764.562938	130790.869568	46.845863
2760.638973	130229.824007	46.850868
2757.154255	129661.594198	46.855873
2753.794693	129098.529560	46.860877
2750.144156	128535.632208	46.865882
2746.522066	127983.727757	46.870887
2743.042805	127423.349953	46.875892
2739.483616	126875.317164	46.880897
2735.712920	126324.895234	46.885901
2732.208024	125777.110321	46.890906
2728.339521	125231.538837	46.895911
2725.145195	124692.483467	46.900916
2721.569982	124154.601090	46.905921
2717.695700	123610.604116	46.910925
2714.650070	123067.159676	46.915930
2710.972825	122536.627924	46.920935
2707.465056	122012.880937	46.925940
2703.987342	121486.465573	46.930945
2700.537853	120950.616601	46.935949
2696.546658	120415.558772	46.940954
2692.877385	119885.417912	46.945959
2689.920527	119361.468356	46.950964
2686.358270	118829.405197	46.955969
2682.770972	118303.279277	46.960973
2679.453286	117776.355731	46.965978
2675.635375	117248.105905	46.970983
2672.567802	116725.621545	46.975988
2668.629899	116199.757660	46.980993
2665.148292	115669.545046	46.985997
2661.686359	115146.127032	46.991002
2657.996966	114636.751387	46.996007
2654.695782	114097.670811	47.001012
2650.768499	113582.561528	47.006017
2647.130791	113050.974359	47.011021
2643.689005	112546.955090	47.016026
2639.632401	112032.269504	47.021031
2636.370935	111521.167414	47.026036
2632.476045	111020.151730	47.031041
2628.749262	110505.106338	47.036045
2625.255473	110012.891328	47.041050
2621.163444	109508.215415	47.046055
2617.650255	109015.152923	47.051060
2613.398943	108524.729475	47.056065
2610.256146	108047.120350	47.061069
2606.258581	107572.002710	47.066074
2602.183175	107104.760121	47.071079
2598.528186	106629.131860	47.076084
2594.911627	106180.060092	47.081089
2591.164447	105726.374685	47.086093
2587.321537	105271.210253	47.091098
2583.449405	104823.874223	47.096103
2579.909619	104369.780730	47.101108
2575.760264	103942.215226	47.106113
2572.649695	103505.532136	47.111117
2568.572325	103071.407629	47.116122
2564.829762	102644.659873	47.121127
2561.540623	102228.371559	47.126132
2558.278451	101815.096723	47.131137
2554.508108	101381.836448	47.136141
2550.904767	100965.689335	47.141146
2546.972333	100541.947292	47.146151
2543.825501	100118.431696	47.151156
2540.050756	99718.837434	47.156161
2536.748942	99297.517388	47.161165
2533.491153	98879.792785	47.166170
2529.722796	98469.994700	47.171175
2526.575128	98054.360778	47.176180
2523.137993	97639.552580	47.181185
2519.650760	97220.957689	47.186189
2515.935988	96797.790538	47.191194
2512.462874	96387.655725	47.196199
2508.880279	95967.160666	47.201204
2505.467236	95563.356005	47.206209
2502.262231	95142.622665	47.211213
2499.016318	94727.480087	47.216218
2495.446803	94306.484408	47.221223
2491.887933	93881.680593	47.226228
2488.339951	93473.832389	47.231233
2484.785824	93048.480236	47.236237
2481.466433	92637.773916	47.241242
2477.946200	92212.542495	47.246247
2474.883438	91784.933243	47.251252
2471.043130	91360.881744	47.256257
2467.850059	90938.260217	47.261261
2464.397387	90519.344349	47.266266
2460.705648	90096.049910	47.271271
2457.590841	89657.742560	47.276276
2453.698279	89227.020784	47.281281
2450.672772	88798.101518	47.286285
2446.796965	88368.837994	47.291290
2443.558523	87941.082338	47.296295
2440.181115	87508.234526	47.301300
2436.431832	87087.799767	47.306305
2433.265410	86642.964242	47.311309
2429.949092	86201.029963	47.316314
2426.102839	85771.164697	47.321319
2422.710028	85331.593088	47.326324
2419.421599	84904.486827	47.331329
2415.787723	84466.490347	47.336333
2412.291691	84032.569522	47.341338
2408.530757	83586.679475	47.346343
2405.632809	83146.429161	47.351348
2401.930448	82718.479935	47.356353
2398.517381	82263.931425	47.361357
2394.635439	81824.782042	47.366362
2390.891007	81390.368653	47.371367
2387.813732	80946.496928	47.376372
2384.257473	80504.891455	47.381377
2381.154735	80060.148648	47.386381
2377.405163	79615.742233	47.391386
2373.822809	79176.003581	47.396391
2370.353843	78726.779484	47.401396
2366.476411	78297.096272	47.406401
2363.479357	77848.752902	47.411405
2359.954445	77403.445452	47.416410
2356.180776	76959.530170	47.421415
2353.436183	76511.944136	47.426420
2349.954689	76069.458381	47.431425
2345.669910	75628.831981	47.436429
2342.496792	75179.645640	47.441434
2338.994634	74730.352915	47.446439
2336.008992	74271.336309	47.451444
2332.024506	73819.251317	47.456449
2328.529939	73367.300919	47.461453
2324.984264	72916.293114	47.466458
2321.596436	72464.760501	47.471463
2318.312110	72008.711835	47.476468
2314.526996	71567.681151	47.481473
2311.325305	71110.403541	47.486477
2307.741071	70647.035413	47.491482
2304.458969	70193.525599	47.496487
2300.734426	69738.499124	47.501492
2297.457875	69285.397874	47.506497
2293.979611	68835.490922	47.511501
2290.472563	68364.425948	47.516506
2286.531955	67910.557118	47.521511
2283.595351	67447.869108	47.526516
2279.824984	66991.736627	47.531521
2276.404885	66535.329283	47.536525
2272.677359	66079.580972	47.541530
2269.145250	65620.014786	47.546535
2266.099325	65157.747228	47.551540
2262.437260	64695.818871	47.556545
2258.642672	64231.793416	47.561549
2255.400567	63772.793379	47.566554
2251.628996	63308.502200	47.571559
2248.399009	62845.436426	47.576564
2244.801956	62390.623293	47.581569
2241.071549	61918.501149	47.586573
2237.861431	61461.112706	47.591578
2234.457519	61002.024090	47.596583
2231.234771	60525.077393	47.601588
2227.268290	60065.662325	47.606593
2223.710455	59597.327350	47.611597
2220.065318	59132.650985	47.616602
2216.403980	58676.698354	47.621607
2213.565901	58205.860568	47.626612
2210.095128	57757.084888	47.631617
2206.557224	57275.961651	47.636621
2203.289666	56807.756066	47.641626
2199.239868	56336.864259	47.646631
2196.596711	55873.833314	47.651636
2192.782492	55393.710926	47.656641
2189.304758	54917.193948	47.661645
2185.737152	54449.931567	47.666650
2182.274363	53971.502637	47.671655
2179.017424	53488.115691	47.676660
2175.328114	53020.868885	47.681665
2171.893251	52545.433634	47.686669
2168.362342	52068.234086	47.691674
2164.355391	51599.758350	47.696679
2161.029750	51110.220953	47.701684
2157.788918	50639.533020	47.706689
2154.167241	50160.826393	47.711693
2150.384602	49688.986232	47.716698
2146.887835	49212.728318	47.721703
2144.017871	48733.350906	47.726708
2140.273193	48258.737134	47.731713
2136.577122	47782.305384	47.736717
2133.481066	47296.967986	47.741722
2129.629571	46817.790032	47.746727
2126.020847	46340.252439	47.751732
2122.521888	45862.371759	47.756737
2119.117557	45397.962947	47.761741
2115.541165	44914.178538	47.766746
2111.887925	44440.943583	47.771751
2109.100889	43960.005840	47.776756
2105.190902	43481.948319	47.781761
2101.743973	43002.953961	47.786765
2098.242488	42506.806957	47.791770
2094.619730	42042.546623	47.796775
2091.030885	41552.585381	47.801780
2087.398911	41064.188906	47.806785
2084.284606	40594.940745	47.811789
2080.767031	40103.073370	47.816794
2076.841631	39634.530072	47.821799
2073.574104	39152.250703	47.826804
2070.158572	38674.829786	47.831809
2066.591092	38191.997206	47.836813
2063.357802	37698.301694	47.841818
2059.899225	37219.068579	47.846823
2056.519522	36724.594128	47.851828
2052.832104	36252.809948	47.856833
2048.864523	35766.816935	47.861837
2045.738344	35280.653377	47.866842
2042.463427	34797.820273	47.871847
2038.900096	34308.628395	47.876852
2035.248139	33828.069307	47.881857
2031.723833	33341.156664	47.886861
2028.280382	32841.084677	47.891866
2024.632867	32364.177531	47.896871
2021.205947	31876.307759	47.901876
2017.690738	31390.345468	47.906881
2014.427177	30901.814011	47.911885
2010.740046	30422.916858	47.916890
2006.955447	29929.267410	47.921895
2003.540166	29443.873963	47.926900
2000.035383	28960.666823	47.931905
1996.461164	28470.669772	47.936909
1992.940846	27984.192935	47.941914
1989.485918	27508.103113	47.946919
1986.035814	27027.252373	47.951924
1982.153771	26536.570369	47.956929
1978.811503	26054.021483	47.961933
1975.179605	25570.768889	47.966938
1971.842317	25093.222256	47.971943
1968.832197	24617.226295	47.976948
1965.047374	24133.968691	47.981953
1961.225136	23647.839678	47.986957
1957.250470	23155.727820	47.991962
1954.093906	22683.741196	47.996967
1950.378893	22208.526896	48.001972
1946.792650	21731.105812	48.006977
1943.280107	21263.858107	48.011981
1939.805027	20782.800286	48.016986
1936.145730	20314.799809	48.021991
1932.862202	19834.090128	48.026996
1928.914974	19364.440620	48.032001
1925.208653	18892.750769	48.037005
1921.604493	18433.983423	48.042010
1917.769914	17976.067123	48.047015
1914.308573	17520.389892	48.052020
1910.390199	17064.310033	48.057025
1906.254517	16627.881926	48.062029
1902.253367	16195.859988	48.067034
1897.831259	15765.322324	48.072039
1893.981555	15353.335872	48.077044
1889.388054	14944.273021	48.082049
1885.111688	14549.730876	48.087053
1882.051345	14149.371948	48.092058
1878.309354	13782.887210	48.097063
1874.421213	13395.394236	48.102068
1870.812809	13024.040402	48.107073
1867.167518	12656.992523	48.112077
1863.636362	12280.142162	48.117082
1859.758760	11915.838965	48.122087
1856.349173	11542.982776	48.127092
1853.094882	11190.806675	48.132097
1848.962262	10841.122740	48.137101
1845.558836	10477.517577	48.142106
1841.766975	10130.949901	48.147111
1838.222846	9782.729430	48.152116
1834.873603	9437.802405	48.157121
1831.149749	9078.841969	48.162125
1828.044623	8741.296613	48.167130
1824.468159	8408.553172	48.172135
1820.909084	8058.455623	48.177140
1817.103692	7723.943373	48.182145
1813.591268	7385.419547	48.187149
1810.079598	7049.408447	48.192154
1806.613255	6730.059450	48.197159
1803.530173	6389.863559	48.202164
1799.776112	6061.003782	48.207169
1796.228359	5726.791627	48.212173
1792.581313	5401.142396	48.217178
1788.611861	5081.697941	48.222183
1785.194263	4749.916996	48.227188
1781.324074	4434.933594	48.232193
1777.473778	4129.585045	48.237197
1773.561773	3822.058342	48.242202
1768.840294	3536.496599	48.247207
1764.956173	3257.381223	48.252212
1760.644165	2992.882665	48.257217
1756.659339	2733.592761	48.262221
1752.877978	2480.615837	48.267226
1748.669512	2244.620984	48.272231
1744.561637	2003.351775	48.277236
1741.017820	1786.028632	48.282241
1736.979835	1567.756749	48.287245
1733.219533	1352.924636	48.292250
1728.939100	1157.153089	48.297255
1725.381837	954.759916	48.302260
1721.717936	760.127515	48.307265
1717.368769	583.520447	48.312269
1714.101064	414.153183	48.317274
1709.875445	256.895537	48.322279
1705.340802	110.488284	48.327284
1698.846238	35.200139	48.332289
1689.327385	76.370306	48.337293
1683.229825	70.678767	48.342298
1678.813441	81.142017	48.347303
1676.349315	74.192114	48.352308
1674.374125	78.106194	48.357313
1671.817948	79.573411	48.362317
1669.460361	78.260462	48.367322
1666.048604	73.308817	48.372327
1663.139936	78.124310	48.377332
1659.548025	76.943365	48.382337
1655.853400	77.034395	48.387341
1652.563039	83.687298	48.392346
1649.581917	79.611412	48.397351
1646.472127	79.019807	48.402356
1642.513128	81.028062	48.407361
1639.000156	82.043096	48.412365
1636.009451	75.501016	48.417370
1632.682804	80.217054	48.422375
1629.707222	75.137416	48.427380
1626.411885	72.281009	48.432385
1622.828682	74.828714	48.437389
1619.633759	78.632087	48.442394
1615.555445	77.631253	48.447399
1611.862139	73.207483	48.452404
1608.874647	62.757744	48.457409
1604.799473	80.944259	48.462413
1602.245388	76.067935	48.467418
1598.701674	84.244048	48.472423
1595.287744	76.916810	48.477428
1591.563666	78.638573	48.482433
1588.364281	81.544152	48.487437
1584.612541	73.215983	48.492442
1581.234195	81.537196	48.497447
1577.775618	77.307846	48.502452
1574.719013	75.698749	48.507457
1570.869824	90.085297	48.512461
1567.748510	67.435016	48.517466
1564.102279	78.072621	48.522471
1560.333053	78.409386	48.527476
1556.996419	79.646913	48.532481
1553.079776	77.225732	48.537485
1549.849491	84.422935	48.542490
1546.387042	76.910271	48.547495
1543.297896	77.001984	48.552500
1539.974090	70.834463	48.557505
1536.426786	73.661320	48.562509
1533.335557	67.859391	48.567514
1529.471903	82.944197	48.572519
1526.102327	83.737609	48.577524
1522.421165	76.806310	48.582529
1518.951528	76.397273	48.587533
1515.668477	69.786822	48.592538
1511.703954	78.389093	48.597543
1508.437419	67.894216	48.602548
1504.498695	79.124667	48.607553
1500.796093	67.084178	48.612557
1498.259369	71.506433	48.617562
1494.615787	82.336614	48.622567
1491.259800	60.551778	48.627572
1488.287552	71.030694	48.632577
1484.179384	74.976217	48.637581
1480.885496	70.876269	48.642586
1477.181179	73.477637	48.647591
1473.402159	66.827333	48.652596
1469.822191	74.721191	48.657601
1466.306641	73.427143	48.662605
1463.403101	74.502357	48.667610
1460.086880	76.904118	48.672615
1456.090843	71.296812	48.677620
1452.745340	66.917006	48.682625
1449.129927	76.961367	48.687629
1445.964930	72.056765	48.692634
1442.309826	72.413744	48.697639
1438.477100	79.983122	48.702644
1435.743282	68.130373	48.707649
1431.751090	73.905446	48.712653
1428.207988	71.217337	48.717658
1424.714420	80.021550	48.722663
1421.335078	78.779071	48.727668
1418.116511	81.364949	48.732673
1414.127779	72.713037	48.737677
1411.254434	72.255491	48.742682
1407.184309	76.543105	48.747687
1403.915345	69.079444	48.752692
1400.345702	76.013100	48.757697
1396.557965	73.682605	48.762701
1393.352971	68.452049	48.767706
1389.899705	69.014894	48.772711
1386.693685	69.494964	48.777716
1383.759946	69.401154	48.782721
1379.444697	76.368608	48.787725
1376.128452	70.766235	48.792730
1372.189165	68.810503	48.797735
1368.544640	63.164319	48.802740
1365.521215	67.867972	48.807745
1361.754189	66.815555	48.812749
1358.805189	67.341042	48.817754
1354.944314	72.678073	48.822759
1351.118649	64.234909	48.827764
1348.053107	61.836305	48.832769
1344.260787	74.502429	48.837773
1341.162807	72.934596	48.842778
1337.392076	66.827180	48.847783
1333.794070	70.291518	48.852788
1330.309057	63.500566	48.857793
1326.741605	65.182154	48.862797
1323.506191	64.350710	48.867802
1320.252967	71.649560	48.872807
1316.463850	69.458494	48.877812
1312.948343	75.959792	48.882817
1309.172224	72.191185	48.887821
1305.950140	62.075401	48.892826
1302.417241	67.510077	48.897831
1299.075347	60.105245	48.902836
1295.848077	68.874333	48.907841
1292.062434	69.270629	48.912845
1288.764470	76.952924	48.917850
1284.727996	69.713149	48.922855
1281.333304	64.164131	48.927860
1277.916013	71.162659	48.932865
1274.242573	73.278358	48.937869
1271.024044	64.493939	48.942874
1267.564965	70.496082	48.947879
1264.106575	70.930026	48.952884
1260.764881	65.252541	48.957889
1257.152562	64.717047	48.962893
1253.564230	62.456774	48.967898
1250.019558	73.002643	48.972903
1246.385087	71.467709	48.977908
1243.217825	70.081510	48.982913
1239.298713	75.607944	48.987917
1235.818741	62.416080	48.992922
1232.581453	69.532121	48.997927
1228.947914	71.929509	49.002932
1225.616285	59.783885	49.007937
1222.157032	65.099537	49.012941
1219.007533	64.286367	49.017946
1215.102414	69.054502	49.022951
1211.536364	63.370820	49.027956
1208.182540	60.422330	49.032961
1204.169320	65.482533	49.037965
1200.826362	66.471143	49.042970
1197.373302	69.729436	49.047975
1194.076915	73.032945	49.052980
1190.626932	61.750455	49.057985
1187.144281	68.525047	49.062989
1183.759084	63.638940	49.067994
1179.712800	62.978019	49.072999
1175.982530	71.157868	49.078004
1172.945225	64.553512	49.083009
1169.101160	70.065105	49.088013
1166.238299	68.508149	49.093018
1162.800752	66.914100	49.098023
1158.981628	65.581922	49.103028
1155.497888	67.010056	49.108033
1151.765101	67.331703	49.113037
1148.294503	66.850090	49.118042
1144.657885	68.102710	49.123047
1141.605911	57.748513	49.128052
1138.353014	60.760523	49.133057
1134.594682	61.114621	49.138061
1131.014706	58.562004	49.143066
1127.510833	65.899874	49.148071
1124.011179	73.537640	49.153076
1120.757903	62.800336	49.158081
1116.771290	74.984188	49.163085
1113.597021	65.838574	49.168090
1110.341324	67.171106	49.173095
1106.500667	69.977223	49.178100
1102.932997	56.735769	49.183105
1099.405721	66.633539	49.188109
1096.257350	61.802329	49.193114
1092.290864	65.713176	49.198119
1089.120660	55.671617	49.203124
1085.833907	64.351893	49.208129
1081.967907	61.071866	49.213133
1079.042857	55.883203	49.218138
1074.896277	63.216715	49.223143
1070.844556	63.597507	49.228148
1067.555422	59.550660	49.233153
1064.284897	70.499937	49.238157
1061.345589	53.864128	49.243162
1057.750193	61.080207	49.248167
1053.889059	63.791441	49.253172
1050.534195	62.579996	49.258177
1046.755479	67.372760	49.263181
1043.402316	56.970555	49.268186
1040.019701	59.512394	49.273191
1036.544152	64.612299	49.278196
1033.415673	59.429997	49.283201
1029.488639	69.586145	49.288205
1026.093562	59.203121	49.293210
1022.478586	62.496123	49.298215
1019.102951	57.380769	49.303220
1015.246083	53.048991	49.308225
1011.609824	60.553000	49.313229
1008.540225	51.615742	49.318234
1004.951658	54.385790	49.323239
1001.303206	56.083181	49.328244
998.119849	57.581629	49.333249
994.527775	62.142868	49.338253
990.865303	62.557990	49.343258
987.268909	60.523628	49.348263
983.691038	64.617596	49.353268
980.439184	65.063712	49.358273
976.650276	64.476648	49.363277
973.284900	62.773314	49.368282
969.770921	66.129692	49.373287
966.397087	63.497553	49.378292
963.100847	64.184693	49.383297
959.830703	68.309854	49.388301
956.184062	58.994200	49.393306
952.262905	72.047367	49.398311
948.472241	61.406404	49.403316
945.097519	61.270550	49.408321
942.021218	75.100184	49.413325
938.464784	67.203634	49.418330
934.838669	64.098255	49.423335
931.085552	72.411384	49.428340
928.087528	69.546747	49.433345
924.553789	60.223015	49.438349
921.545783	58.584279	49.443354
917.674492	71.376590	49.448359
913.517324	73.004488	49.453364
910.131014	66.675957	49.458369
906.728763	65.668054	49.463373
903.363597	62.461949	49.468378
900.039473	64.203777	49.473383
896.441533	66.383688	49.478388
893.059130	56.694729	49.483393
889.402082	64.616425	49.488397
885.910167	55.624705	49.493402
882.240752	61.868414	49.498407
878.792959	59.965956	49.503412
875.421541	56.014202	49.508417
871.880541	64.803664	49.513421
868.252137	67.839349	49.518426
864.784239	66.193116	49.523431
861.249415	63.010263	49.528436
857.982173	62.952599	49.533441
854.116317	67.126208	49.538445
850.511930	62.353365	49.543450
847.406531	69.543803	49.548455
843.668604	65.396010	49.553460
840.577541	59.398011	49.558465
836.955658	59.996653	49.563469
833.474912	66.429291	49.568474
829.900575	65.748735	49.573479
826.121381	75.116271	49.578484
822.606964	58.731387	49.583489
819.456782	67.972531	49.588493
815.905215	63.330673	49.593498
812.347631	63.969927	49.598503
809.043284	68.122570	49.603508
805.171507	57.228519	49.608513
801.676222	63.533710	49.613517
798.449482	67.648964	49.618522
794.991501	60.006031	49.623527
790.987961	69.354707	49.628532
787.944614	59.015053	49.633537
784.231922	71.358746	49.638541
781.134760	64.361983	49.643546
777.204914	70.291911	49.648551
773.323810	67.688145	49.653556
770.108180	58.245325	49.658561
766.812874	57.980074	49.663565
763.310620	65.814408	49.668570
760.010845	66.973506	49.673575
756.321943	65.459765	49.678580
752.848614	61.179053	49.683585
749.221533	68.501323	49.688589
745.770950	56.595780	49.693594
742.265980	56.850375	49.698599
738.741264	59.316289	49.703604
735.250221	53.247700	49.708609
731.462398	61.983843	49.713613
728.024892	56.144196	49.718618
724.723338	57.309902	49.723623
720.780619	61.992186	49.728628
717.957428	55.639305	49.733633
714.571310	64.205352	49.738637
710.763490	55.050879	49.743642
707.309079	57.306540	49.748647
703.380592	64.523875	49.753652
700.259667	52.785321	49.758657
696.654174	55.396687	49.763661
693.159824	54.852391	49.768666
689.892575	53.690626	49.773671
686.076181	52.323290	49.778676
682.721475	53.528912	49.783681
678.478000	63.981100	49.788685
675.272692	68.792199	49.793690
672.170611	58.936262	49.798695
668.360672	61.674369	49.803700
665.047767	58.099506	49.808705
661.522341	71.189149	49.813709
658.272306	56.848015	49.818714
654.980858	71.720345	49.823719
651.177175	67.769477	49.828724
647.735216	63.537680	49.833729
644.113703	70.460469	49.838733
640.891773	58.709173	49.843738
637.358022	59.234011	49.848743
633.783506	58.699038	49.853748
630.425735	52.989361	49.858753
626.785732	65.302756	49.863757
622.873488	62.577317	49.868762
619.605903	59.049188	49.873767
615.917603	59.006481	49.878772
612.897909	52.526025	49.883777
608.721307	63.711269	49.888781
605.570876	58.136992	49.893786
602.431320	56.904741	49.898791
598.705807	63.407134	49.903796
594.964793	55.729211	49.908801
591.473724	56.959235	49.913805
587.663224	67.166862	49.918810
584.385136	52.308112	49.923815
581.192995	57.689789	49.928820
578.105514	52.320848	49.933825
574.281406	54.823895	49.938829
570.220854	49.685531	49.943834
567.214161	53.617852	49.948839
563.280852	53.088126	49.953844
560.188090	50.469237	49.958849
556.692337	55.645087	49.963853
553.230517	50.207880	49.968858
549.540093	59.482512	49.973863
545.996081	57.186967	49.978868
542.426245	49.972778	49.983873
539.192182	61.966721	49.988877
535.941993	52.848861	49.993882
532.430875	56.119414	49.998887
528.330452	48.067202	50.003892
524.774233	48.620861	50.008897
521.163769	57.300931	50.013901
517.780706	57.292975	50.018906
514.713838	58.216531	50.023911
511.065378	61.239557	50.028916
507.665642	54.558861	50.033921
504.001160	58.539808	50.038925
500.379175	58.179918	50.043930
496.897400	62.009040	50.048935
493.107883	67.202158	50.053940
490.162053	60.194543	50.058945
486.402189	63.019786	50.063949
482.923818	63.545512	50.068954
479.854049	56.123773	50.073959
476.186935	70.276322	50.078964
472.715601	53.011660	50.083969
468.832659	62.879402	50.088973
465.430865	58.780584	50.093978
461.835972	58.900522	50.098983
458.124028	64.002475	50.103988
455.032823	53.866489	50.108993
451.108420	59.567813	50.113997
447.904573	62.009115	50.119002
444.728291	47.419284	50.124007
440.973682	55.435285	50.129012
437.827199	57.668346	50.134017
433.816686	59.640462	50.139021
430.370692	58.883035	50.144026
426.936909	52.498712	50.149031
423.271325	58.064835	50.154036
419.936602	49.539112	50.159041
416.511849	63.233159	50.164045
412.858184	58.442755	50.169050
409.590059	58.502338	50.174055
405.933587	62.162519	50.179060
402.603994	52.769155	50.184065
398.886957	57.865577	50.189069
395.581928	57.953053	50.194074
392.061153	49.962485	50.199079
388.620266	66.863837	50.204084
384.787494	62.132958	50.209089
381.201766	60.416555	50.214093
378.164751	59.570155	50.219098
374.334468	50.919115	50.224103
370.190295	46.255705	50.229108
367.279302	49.461319	50.234113
363.706082	52.124644	50.239117
360.738098	59.657531	50.244122
357.055897	47.955818	50.249127
353.298621	59.749653	50.254132
349.889788	54.028993	50.259137
345.867686	60.919257	50.264141
342.815933	46.889016	50.269146
339.551508	42.974475	50.274151
335.990036	59.416880	50.279156
332.689728	48.127104	50.284161
329.003764	63.892889	50.289165
325.680915	57.380585	50.294170
321.670921	54.357215	50.299175
318.134650	54.727467	50.304180
314.636583	53.680779	50.309185
310.971665	62.786947	50.314189
307.910288	52.804532	50.319194
304.453757	58.281174	50.324199
300.732976	60.461295	50.329204
297.738530	59.782278	50.334209
293.687645	56.050292	50.339213
290.247601	57.370483	50.344218
286.914016	57.146052	50.349223
283.091197	58.832712	50.354228
279.761390	52.156992	50.359233
276.271719	56.291077	50.364237
272.731122	58.177401	50.369242
269.496167	57.301722	50.374247
265.959704	56.960187	50.379252
262.137954	56.264448	50.384257
258.853657	62.005337	50.389261
255.185921	59.558262	50.394266
251.750906	49.399920	50.399271
247.973097	57.659987	50.404276
244.662394	58.586735	50.409281
241.189887	52.385642	50.414285
237.855624	60.782294	50.419290
234.659625	56.705259	50.424295
230.532933	61.004962	50.429300
227.536989	44.055497	50.434305
223.816714	49.680770	50.439309
220.135217	51.645983	50.444314
216.885758	53.025094	50.449319
212.892178	59.199106	50.454324
209.914627	49.532684	50.459329
206.129904	53.105289	50.464333
202.716525	49.872001	50.469338
199.288461	55.334729	50.474343
195.566208	58.502154	50.479348
192.387097	52.274374	50.484353
188.300290	53.850291	50.489357
184.707619	63.220457	50.494362
181.646715	59.081270	50.499367
178.038619	63.752644	50.504372
175.276573	50.699198	50.509377
171.675637	56.935466	50.514381
167.410356	56.039885	50.519386
163.791105	52.689963	50.524391
160.351757	56.170839	50.529396
157.864295	47.630316	50.534401
154.193937	55.981224	50.539405
149.991085	55.733967	50.544410
146.672217	57.490876	50.549415
142.897671	47.907426	50.554420
139.524322	54.076627	50.559425
136.298300	54.373292	50.564429
132.402270	60.579581	50.569434
129.308558	51.719009	50.574439
125.504219	59.758598	50.579444
122.464998	56.780270	50.584449
118.437684	59.122032	50.589453
114.940956	54.702708	50.594458
111.824300	56.080138	50.599463
107.820658	58.661816	50.604468
104.626160	58.469538	50.609473
101.188385	60.276603	50.614477
97.566789	50.824368	50.619482
94.493423	47.389469	50.624487
90.451699	55.940567	50.629492
86.992007	49.598309	50.634497
83.355846	50.104366	50.639501
80.076533	52.392946	50.644506
76.439321	52.905494	50.649511
73.347379	62.447636	50.654516
69.999419	50.485153	50.659521
66.043396	51.901526	50.664525
62.447329	58.057956	50.669530
59.358166	56.280111	50.674535
55.313287	52.914222	50.679540
52.208928	49.199426	50.684545
48.587542	51.031921	50.689549
44.974601	49.822832	50.694554
41.600226	40.705436	50.699559
37.787878	52.384474	50.704564
34.512830	59.054056	50.709569
30.954957	63.040604	50.714573
27.601366	52.901272	50.719578
24.038019	52.244431	50.724583
20.298241	53.127286	50.729588
17.248029	49.337629	50.734593
13.747509	54.052379	50.739597
9.702406	52.417051	50.744602
6.524713	51.867842	50.749607
2.820983	50.508385	50.754612