Fri Aug 26 11:49:48 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
-0.244363	103.256626	0.000000
-0.026091	108.952065	0.005005
0.305763	108.473339	0.010010
-0.090141	104.172332	0.015014
-0.295952	95.925123	0.020019
-0.526327	91.835621	0.025024
-0.647807	92.015918	0.030029
-0.243119	79.488147	0.035034
-0.638786	76.642390	0.040038
-1.114010	66.959715	0.045043
-1.164069	57.489249	0.050048
-1.569804	50.159010	0.055053
-1.912317	35.017378	0.060058
-2.115756	33.163557	0.065062
-2.245672	35.442665	0.070067
-2.912532	14.606371	0.075072
-3.347014	14.028672	0.080077
-3.286933	9.976221	0.085082
-3.845496	15.166179	0.090086
-4.242058	12.627446	0.095091
-4.271169	9.227938	0.100096
-4.432015	11.701677	0.105101
-4.688580	0.687900	0.110106
-5.212025	6.527261	0.115110
-5.339636	3.984618	0.120115
-5.510264	-8.023261	0.125120
-5.624123	3.045095	0.130125
-6.026983	2.617492	0.135130
-7.116063	1.641859	0.140134
-7.185744	-1.555186	0.145139
-7.170660	-10.260666	0.150144
-7.371010	2.061302	0.155149
-7.340603	3.179697	0.160154
-7.438326	1.034183	0.165158
-7.542695	2.331744	0.170163
-8.079156	4.240727	0.175168
-8.734345	7.854417	0.180173
-8.626300	-1.555216	0.185178
-8.938343	4.399921	0.190182
-9.033277	7.170270	0.195187
-8.908914	4.525123	0.200192
-9.576826	8.751376	0.205197
-9.825777	9.720285	0.210202
-10.167505	4.385848	0.215206
-10.503958	1.780813	0.220211
-11.100750	13.022439	0.225216
-11.283100	9.479116	0.230221
-11.210736	2.482569	0.235226
-11.395184	-2.645408	0.240230
-11.672971	-4.598376	0.245235
-11.359770	-4.213685	0.250240
-11.787354	1.152021	0.255245
-12.349220	0.148084	0.260250
-13.166417	7.482129	0.265254
-12.854222	-5.755655	0.270259
-12.653762	-0.437116	0.275264
-13.764940	3.459533	0.280269
-14.065946	-2.365278	0.285274
-14.766286	7.655483	0.290278
-14.545182	3.157199	0.295283
-14.648060	0.196269	0.300288
-14.523010	-1.474583	0.305293
-14.397112	4.792004	0.310298
-14.941449	9.429271	0.315302
-15.483924	4.992929	0.320307
-15.704390	4.891255	0.325312
-15.917700	6.534797	0.330317
-16.034725	6.818801	0.335322
-16.052920	6.002288	0.340326
-16.732708	3.839837	0.345331
-17.335309	3.829298	0.350336
-17.688492	3.874834	0.355341
-17.453758	0.586102	0.360346
-17.511730	3.312732	0.365350
-17.723538	11.593358	0.370355
-18.063998	6.106869	0.375360
-18.734614	4.458663	0.380365
-18.615630	9.131853	0.385370
-19.015888	0.130381	0.390374
-19.124773	10.900584	0.395379
-19.037769	0.953245	0.400384
-19.787799	6.761448	0.405389
-20.196896	1.953176	0.410394
-20.450983	-2.195884	0.415398
-20.155766	9.504782	0.420403
-20.237166	-8.784159	0.425408
-21.172356	2.718948	0.430413
-21.552572	-2.033711	0.435418
-21.790628	-1.414500	0.440422
-21.985269	-6.047360	0.445427
-21.835828	3.012216	0.450432
-22.012917	1.600370	0.455437
-22.072676	2.549312	0.460442
-22.966671	6.405820	0.465446
-23.455329	-3.916942	0.470451
-23.495686	-4.941968	0.475456
-23.458569	-4.403564	0.480461
-23.677538	-1.057104	0.485466
-23.729110	0.861801	0.490470
-23.945245	0.680362	0.495475
-24.476383	-0.685850	0.500480
-24.732013	7.898979	0.505485
-25.189602	2.247237	0.510490
-25.199573	7.465669	0.515494
-25.400850	-5.084748	0.520499
-25.768215	-0.196637	0.525504
-26.421549	13.103830	0.530509
-26.521295	8.816846	0.535514
-26.676400	14.617841	0.540518
-26.625981	7.820855	0.545523
-26.540011	7.642997	0.550528
-26.985438	9.151843	0.555533
-27.454747	9.395787	0.560538
-27.879824	5.963022	0.565542
-27.835831	4.095989	0.570547
-27.377747	7.131398	0.575552
-28.393194	10.503797	0.580557
-28.970069	13.709839	0.585562
-29.354590	6.249772	0.590566
-29.442433	11.132329	0.595571
-29.359046	-0.367793	0.600576
-29.628280	10.386247	0.605581
-30.066191	0.729438	0.610586
-30.480076	5.327411	0.615590
-30.619518	3.789485	0.620595
-30.596325	-1.225293	0.625600
-30.912102	4.344460	0.630605
-30.967627	6.039363	0.635610
-31.552918	3.612272	0.640614
-31.627188	4.901983	0.645619
-31.780112	2.281028	0.650624
-32.224431	19.259904	0.655629
-32.034079	8.034178	0.660634
-32.869672	14.111960	0.665638
-33.039828	-0.287708	0.670643
-33.074797	6.753708	0.675648
-33.320754	14.641032	0.680653
-33.841240	6.474497	0.685658
-34.684929	12.275139	0.690662
-34.742031	5.776459	0.695667
-34.890678	15.695508	0.700672
-34.632906	13.605371	0.705677
-35.074604	7.799300	0.710682
-35.141819	7.290965	0.715686
-35.195765	10.219442	0.720691
-35.485289	9.008592	0.725696
-36.385120	5.716182	0.730701
-36.379926	9.935707	0.735706
-36.450089	15.109730	0.740710
-36.490342	11.098210	0.745715
-36.278151	7.461823	0.750720
-37.287591	2.126951	0.755725
-37.201845	1.531528	0.760730
-37.535922	9.470534	0.765734
-38.049047	-2.155001	0.770739
-38.871753	6.995829	0.775744
-39.369480	6.437470	0.780749
-38.883959	0.784416	0.785754
-39.068307	6.858871	0.790758
-39.146653	7.741107	0.795763
-39.323447	6.629761	0.800768
-39.482944	16.417627	0.805773
-39.881354	4.555935	0.810778
-40.333166	8.191741	0.815782
-40.806406	19.575477	0.820787
-40.711698	3.407220	0.825792
-41.204607	8.422444	0.830797
-40.992285	-0.516222	0.835802
-41.030293	10.894654	0.840806
-41.867665	5.729135	0.845811
-42.655080	-0.969033	0.850816
-42.749778	11.532633	0.855821
-42.794273	0.378278	0.860826
-42.627028	10.191194	0.865830
-42.719620	1.461348	0.870835
-42.725315	2.411363	0.875840
-43.605416	13.782516	0.880845
-43.747460	1.624657	0.885850
-43.712967	-1.908134	0.890854
-43.887722	9.179195	0.895859
-44.487503	0.167664	0.900864
-45.205463	5.939237	0.905869
-45.033358	1.211310	0.910874
-45.296148	7.041723	0.915878
-45.327753	2.329695	0.920883
-45.421352	-5.561627	0.925888
-46.652814	8.502703	0.930893
-46.617878	5.153334	0.935898
-46.809299	14.576023	0.940902
-46.915995	5.585789	0.945907
-46.521361	4.730309	0.950912
-47.042294	11.338044	0.955917
-47.217364	5.936533	0.960922
-47.850576	7.610653	0.965926
-48.384562	11.110563	0.970931
-48.537864	-1.966161	0.975936
-48.369716	14.914185	0.980941
-48.266142	8.624597	0.985946
-49.017107	10.750470	0.990950
-49.635940	7.977438	0.995955
-49.684109	-0.534705	1.000960
-50.003420	11.097132	1.005965
-50.029941	5.530129	1.010970
-49.948772	15.255213	1.015974
-50.273477	9.737799	1.020979
-50.763643	12.528558	1.025984
-51.225955	4.352968	1.030989
-51.056152	5.288313	1.035994
-51.353303	-2.669389	1.040998
-51.903750	8.618798	1.046003
-52.378550	3.162719	1.051008
-52.682149	21.271250	1.056013
-52.545963	5.839989	1.061018
-52.540625	3.349412	1.066022
-52.651174	5.922881	1.071027
-53.197232	5.764339	1.076032
-53.794356	7.445495	1.081037
-54.229740	1.091135	1.086042
-54.093934	6.005303	1.091046
-54.232222	11.183604	1.096051
-54.098943	-1.216429	1.101056
-54.676150	9.016105	1.106061
-55.277775	4.832574	1.111066
-55.816325	6.476138	1.116070
-55.966992	12.225822	1.121075
-55.872176	-1.281825	1.126080
-55.876395	5.065128	1.131085
-55.684884	1.428799	1.136090
-56.310480	9.656794	1.141094
-56.583064	8.883053	1.146099
-56.769022	12.857103	1.151104
-57.259779	14.078788	1.156109
-57.676464	9.088206	1.161114
-58.054980	6.540340	1.166118
-58.346093	2.691263	1.171123
-58.277789	-4.355265	1.176128
-58.736923	-4.720323	1.181133
-58.579716	-2.795962	1.186138
-58.439787	-2.814548	1.191142
-59.479752	-2.200188	1.196147
-59.526278	2.277313	1.201152
-59.709966	2.682424	1.206157
-59.723723	3.700131	1.211162
-60.639906	-0.374312	1.216166
-61.029381	4.662769	1.221171
-61.225851	4.519396	1.226176
-61.758326	7.746997	1.231181
-61.655555	3.583502	1.236186
-61.586100	3.866944	1.241190
-61.661332	5.925569	1.246195
-61.447146	6.056766	1.251200
-61.993398	6.230437	1.256205
-62.579353	0.399376	1.261210
-63.392949	9.308351	1.266214
-63.335850	10.004989	1.271219
-63.201183	-0.367367	1.276224
-63.150414	8.065353	1.281229
-63.324941	-2.031079	1.286234
-64.174454	3.368685	1.291238
-64.633244	11.229035	1.296243
-64.426600	7.065185	1.301248
-64.523438	4.280479	1.306253
-65.020665	7.458301	1.311258
-65.548547	1.735252	1.316262
-66.010991	7.062095	1.321267
-65.926894	-3.852858	1.326272
-65.977745	10.239615	1.331277
-65.829351	-7.575754	1.336282
-66.348187	3.612597	1.341286
-67.024436	5.650910	1.346291
-67.260313	-1.291313	1.351296
-67.000069	8.924720	1.356301
-67.075665	-5.837662	1.361306
-67.829885	7.978360	1.366310
-68.805893	6.327087	1.371315
-68.765897	-2.227253	1.376320
-68.807750	5.859232	1.381325
-68.544400	-5.659412	1.386330
-68.569779	0.943924	1.391334
-68.957002	-2.127749	1.396339
-69.685120	-6.038490	1.401344
-70.353025	7.805219	1.406349
-70.162526	4.880866	1.411354
-70.460145	0.488658	1.416358
-70.710557	-3.705263	1.421363
-70.292095	0.984567	1.426368
-70.352089	1.256527	1.431373
-71.127484	-9.230381	1.436378
-71.904205	-8.391263	1.441382
-72.218937	0.256543	1.446387
-72.171760	-1.683748	1.451392
-72.919586	-0.830146	1.456397
-72.618142	3.817795	1.461402
-73.251692	-3.081491	1.466406
-73.261957	-2.516728	1.471411
-73.399103	-4.197374	1.476416
-73.741163	-2.321823	1.481421
-73.360335	-6.715263	1.486426
-73.297695	-3.298760	1.491430
-74.416240	-5.794675	1.496435
-74.616386	-2.305620	1.501440
-74.533677	-4.352679	1.506445
-75.010569	-5.189517	1.511450
-75.641156	-3.335479	1.516454
-76.310929	1.976190	1.521459
-75.808052	-1.117018	1.526464
-76.409693	2.247896	1.531469
-76.104322	-1.396669	1.536474
-75.993659	7.001415	1.541478
-76.801667	3.030348	1.546483
-77.169488	4.318310	1.551488
-77.778527	1.404555	1.556493
-77.740132	-2.666660	1.561498
-77.948354	2.427618	1.566502
-77.941965	6.286299	1.571507
-77.840478	1.464968	1.576512
-78.846241	15.332814	1.581517
-79.209314	1.352316	1.586522
-79.380760	8.775634	1.591526
-79.472541	11.624582	1.596531
-79.088491	-3.301113	1.601536
-79.500404	-1.471631	1.606541
-80.621924	6.871540	1.611546
-80.387443	8.537106	1.616550
-80.726127	15.673266	1.621555
-80.533026	-2.965285	1.626560
-80.938953	-3.683463	1.631565
-81.258115	1.010487	1.636570
-81.892237	7.727588	1.641574
-82.260296	5.658968	1.646579
-82.271531	4.847699	1.651584
-82.391985	7.897257	1.656589
-82.381218	6.747217	1.661594
-82.383326	4.055326	1.666598
-83.264829	6.824761	1.671603
-83.431979	0.204020	1.676608
-83.737181	7.486817	1.681613
-84.025806	10.192414	1.686618
-83.632754	12.988019	1.691622
-84.464397	2.626918	1.696627
-85.012137	-1.261290	1.701632
-85.275260	9.624667	1.706637
-85.275175	2.440068	1.711642
-85.643624	11.545479	1.716646
-85.433021	-1.970701	1.721651
-85.693017	2.663420	1.726656
-85.612541	4.001800	1.731661
-86.468521	10.655373	1.736666
-86.534308	14.069729	1.741670
-86.912494	7.978536	1.746675
-86.681389	7.284553	1.751680
-87.542486	8.234882	1.756685
-87.664112	10.639241	1.761690
-88.245802	9.385301	1.766694
-88.663248	-0.046907	1.771699
-88.103937	-6.163846	1.776704
-88.496097	7.352200	1.781709
-88.458613	1.139343	1.786714
-89.054634	-4.193456	1.791718
-89.743581	4.673963	1.796723
-89.501920	5.870192	1.801728
-89.491474	-0.525109	1.806733
-90.122791	6.950828	1.811738
-90.838786	1.643035	1.816742
-91.419908	9.440175	1.821747
-90.825107	-1.108222	1.826752
-91.263144	6.894422	1.831757
-90.965022	9.138515	1.836762
-90.934635	11.126914	1.841766
-91.750009	1.146081	1.846771
-92.237395	-1.840396	1.851776
-92.465638	11.435004	1.856781
-92.784373	-6.304465	1.861786
-92.651531	2.450817	1.866790
-93.381416	3.861589	1.871795
-93.697513	0.434005	1.876800
-94.077766	7.817070	1.881805
-94.118166	3.267759	1.886810
-94.064461	2.708961	1.891814
-94.056684	8.607972	1.896819
-94.238789	2.916506	1.901824
-94.897264	12.623874	1.906829
-95.795293	9.391297	1.911834
-95.927602	1.066258	1.916838
-96.050290	11.275476	1.921843
-95.549586	4.933549	1.926848
-96.008726	5.938348	1.931853
-95.777704	5.174778	1.936858
-96.215992	-2.776763	1.941862
-97.094967	0.735732	1.946867
-97.299001	-2.291699	1.951872
-97.162990	4.612362	1.956877
-97.285213	-2.587990	1.961882
-97.829109	0.568624	1.966886
-98.249219	4.212146	1.971891
-98.287967	-4.494439	1.976896
-98.669134	-1.043636	1.981901
-99.014426	4.068820	1.986906
-99.243074	0.298602	1.991910
-100.045711	3.546121	1.996915
-100.042790	1.820209	2.006912
-98.934992	-0.408032	2.016909
-98.561814	6.487014	2.026906
-98.806286	2.103060	2.036902
-98.157896	7.608988	2.046899
-97.524172	7.627595	2.056896
-96.963138	6.127526	2.066893
-96.295275	-1.905110	2.076890
-95.957787	-1.732677	2.086886
-95.640547	1.217803	2.096883
-94.997487	0.797815	2.106880
-94.579889	1.588145	2.116877
-93.691008	-4.638476	2.126874
-93.338724	-3.084068	2.136870
-93.231233	-0.233973	2.146867
-92.468332	3.667113	2.156864
-92.209423	0.066394	2.166861
-91.308018	5.780006	2.176858
-90.870043	5.265243	2.186854
-90.749283	-0.632714	2.196851
-89.398666	1.840099	2.206848
-88.986785	2.517282	2.216845
-89.259853	8.154012	2.226842
-88.616652	0.207575	2.236838
-87.997016	4.463575	2.246835
-87.687394	-0.469135	2.256832
-86.639885	5.617691	2.266829
-86.296720	3.470492	2.276826
-86.085667	5.157760	2.286822
-85.339609	-1.667491	2.296819
-85.104582	6.294402	2.306816
-84.274421	4.758766	2.316813
-83.714784	0.556877	2.326810
-83.695591	4.595933	2.336806
-82.716030	-0.827544	2.346803
-82.167946	1.047992	2.356800
-81.906365	6.490607	2.366797
-81.571492	3.049114	2.376794
-80.714058	2.611588	2.386790
-80.572318	0.736495	2.396787
-80.046086	5.716601	2.406784
-79.298464	0.310230	2.416781
-79.006435	8.732068	2.426778
-78.478249	10.883125	2.436774
-77.867731	14.687569	2.446771
-77.465742	9.157619	2.456768
-76.894480	0.392447	2.466765
-76.541529	5.070094	2.476762
-75.451914	8.296278	2.486758
-75.172085	6.301486	2.496755
-75.020298	7.703387	2.506752
-74.563693	4.616728	2.516749
-74.029463	7.992739	2.526746
-73.630806	5.713360	2.536742
-72.705732	7.989515	2.546739
-72.294399	12.943166	2.556736
-71.865804	11.235644	2.566733
-70.955700	7.460674	2.576730
-70.803098	9.489652	2.586726
-70.490203	12.428140	2.596723
-70.168504	11.583035	2.606720
-69.416703	17.614543	2.616717
-68.929206	11.497927	2.626714
-68.214076	11.149078	2.636710
-67.989251	13.303022	2.646707
-67.337200	10.841642	2.656704
-66.428953	9.002420	2.666701
-66.213164	9.513739	2.676698
-66.455842	5.959438	2.686694
-65.471355	11.650616	2.696691
-64.854289	14.766652	2.706688
-63.792819	11.829725	2.716685
-63.873090	8.177280	2.726682
-63.778650	12.834994	2.736678
-62.773943	11.550937	2.746675
-62.229661	7.642865	2.756672
-61.932929	6.817486	2.766669
-61.217549	10.950881	2.776666
-60.724926	8.878609	2.786662
-60.523819	9.401717	2.796659
-60.012080	5.432190	2.806656
-59.214849	11.244387	2.816653
-58.959066	10.662961	2.826650
-58.528804	10.719584	2.836646
-58.051950	7.832503	2.846643
-57.133942	5.313876	2.856640
-56.486233	5.285959	2.866637
-56.288028	2.084316	2.876634
-56.162360	9.882682	2.886630
-55.231907	9.608010	2.896627
-55.038150	10.053070	2.906624
-54.017710	9.976623	2.916621
-53.544409	0.821237	2.926618
-53.562970	11.461305	2.936614
-52.997848	8.579486	2.946611
-52.460403	3.288198	2.956608
-51.830512	0.880954	2.966605
-50.966149	6.467295	2.976602
-50.828395	5.105988	2.986598
-50.685007	4.909514	2.996595
-49.978105	6.576598	3.006592
-49.331127	0.770929	3.016589
-48.717735	-1.842814	3.026586
-48.155505	-10.378502	3.036582
-47.979553	-6.034415	3.046579
-47.279798	-4.949073	3.056576
-46.234599	-2.051748	3.066573
-46.174084	-1.766501	3.076570
-46.432503	7.783213	3.086566
-45.406578	2.830837	3.096563
-44.677887	5.546201	3.106560
-44.169878	2.369179	3.116557
-43.390054	1.969078	3.126554
-43.223578	-1.734455	3.136550
-43.174246	-1.802247	3.146547
-42.349947	-2.076229	3.156544
-41.773171	2.883338	3.166541
-41.454076	0.163368	3.176538
-40.740917	2.675251	3.186534
-40.369593	2.360927	3.196531
-39.628680	-0.465900	3.206528
-38.786419	0.882346	3.216525
-38.847910	3.486332	3.226522
-38.756318	10.542431	3.236518
-37.804871	10.144119	3.246515
-37.397612	2.494165	3.256512
-36.294629	10.301918	3.266509
-36.162721	10.256113	3.276506
-35.901199	-0.884118	3.286502
-35.736800	-0.957155	3.296499
-35.024848	0.582435	3.306496
-33.799473	-1.952370	3.316493
-33.520998	-1.545842	3.326490
-33.170456	0.395298	3.336486
-33.148884	6.223731	3.346483
-32.346849	-1.741103	3.356480
-31.660240	-6.621640	3.366477
-31.578090	-2.326300	3.376474
-30.691401	-3.693345	3.386470
-30.113190	-7.533840	3.396467
-29.704982	0.850903	3.406464
-28.870113	0.134967	3.416461
-28.650195	-5.062533	3.426458
-28.556719	3.596121	3.436454
-28.062895	-5.533949	3.446451
-27.046006	-4.545499	3.456448
-26.905390	2.015140	3.466445
-26.073438	-0.132137	3.476442
-26.074182	0.381218	3.486438
-25.406154	5.374095	3.496435
-24.385548	-4.686935	3.506432
-24.382418	-2.488972	3.516429
-23.821591	-1.752618	3.526426
-22.831040	0.719244	3.536422
-22.700141	7.854750	3.546419
-22.637233	2.833743	3.556416
-21.864857	1.319776	3.566413
-21.302510	3.319802	3.576410
-20.164931	-2.888524	3.586406
-19.780995	4.131559	3.596403
-20.162519	1.913467	3.606400
-19.596993	-2.650456	3.616397
-18.570850	-2.715119	3.626394
-18.313438	-4.408657	3.636390
-17.930337	3.431987	3.646387
-17.093079	5.329024	3.656384
-16.540722	2.895839	3.666381
-16.206499	0.230531	3.676378
-15.623753	-2.302416	3.686374
-15.291270	-1.055356	3.696371
-14.603001	-3.237280	3.706368
-13.820586	-2.681140	3.716365
-13.728803	-4.773361	3.726362
-13.685716	-9.379479	3.736358
-12.690844	-2.581227	3.746355
-12.301899	-0.617557	3.756352
-11.805474	-9.507286	3.766349
-11.035890	-6.421333	3.776346
-10.900326	-5.596593	3.786342
-9.959623	-8.134589	3.796339
-9.297303	-10.480360	3.806336
-9.371636	-7.294688	3.816333
-8.967512	-7.373373	3.826330
-8.332100	-3.278210	3.836326
-8.252197	-9.049436	3.846323
-6.757380	0.030906	3.856320
-6.631274	-6.593287	3.866317
-6.348464	-10.596856	3.876314
-5.617171	2.650672	3.886310
-5.330365	4.379998	3.896307
-4.773147	11.588509	3.906304
-4.405221	15.956565	3.916301
-4.521629	17.099295	3.926298
-3.709934	36.362452	3.936294
-3.075554	45.345544	3.946291
-2.346095	61.856132	3.956288
-1.928596	65.288345	3.966285
-1.863357	82.634109	3.976282
-1.430802	96.263998	3.986278
-0.568569	116.967017	3.996275
0.000000	119.781595	4.001280
-0.363781	135.821094	4.006285
0.049668	132.324183	4.011290
0.122070	141.104770	4.016294
0.467223	152.358009	4.021299
0.702810	150.404184	4.026304
0.278060	149.192232	4.031309
0.710338	141.658715	4.036314
0.338538	153.817662	4.041318
-0.052415	155.890662	4.046323
0.233588	149.037958	4.051328
-0.110848	163.217398	4.056333
0.814864	172.472566	4.061338
0.913155	171.017830	4.066342
0.863519	179.545361	4.071347
1.222117	174.617512	4.076352
1.056979	169.176438	4.081357
0.722534	158.873860	4.086362
0.621956	162.002606	4.091366
0.575151	159.301831	4.096371
0.628622	152.197437	4.101376
0.628819	163.842904	4.106381
0.842759	159.146384	4.111386
0.467792	166.076291	4.116390
0.547237	178.117542	4.121395
0.700062	177.018137	4.126400
0.843082	184.180604	4.131405
0.843160	174.224555	4.136410
1.036781	180.186439	4.141414
0.820982	179.919527	4.146419
1.478070	183.591518	4.151424
0.939863	181.232998	4.156429
0.949170	165.024103	4.161434
0.946183	166.979752	4.166438
0.701529	167.033700	4.171443
0.691394	162.514432	4.176448
0.464820	175.017768	4.181453
1.179817	174.435095	4.186458
1.166042	183.406286	4.191462
0.935420	189.443717	4.196467
1.159184	191.867089	4.201472
1.282017	189.725177	4.206477
1.193752	179.362111	4.211482
0.661092	171.906054	4.216486
0.746267	174.414275	4.221491
0.923292	178.448904	4.226496
0.825011	179.340580	4.231501
1.267783	186.582925	4.236506
1.042357	183.084238	4.241510
0.928371	193.972404	4.246515
1.183590	181.452014	4.251520
1.241875	186.131539	4.256525
1.546516	179.054465	4.261530
1.263875	176.921903	4.266534
1.312078	186.563634	4.271539
1.285129	186.760851	4.276544
1.282659	188.539257	4.281549
1.562313	185.822450	4.286554
1.007790	177.550403	4.291558
1.185920	183.445099	4.296563
1.338439	186.385751	4.301568
1.180735	195.414157	4.306573
1.575405	191.793612	4.311578
1.051108	190.736358	4.316582
1.139175	187.888033	4.321587
1.735443	189.430852	4.326592
1.153871	184.291887	4.331597
1.445555	184.496440	4.336602
1.487926	182.246836	4.341606
1.186850	181.009299	4.346611
1.291764	178.515847	4.351616
1.121984	187.925770	4.356621
0.834728	184.531620	4.361626
1.176950	181.093245	4.366630
0.780622	187.488661	4.371635
0.831249	181.574240	4.376640
1.344708	192.412168	4.381645
1.584207	196.557293	4.386650
1.526384	201.973053	4.391654
1.468321	200.586950	4.396659
1.683587	201.591156	4.401664
1.361976	192.172389	4.406669
1.546252	197.553618	4.411674
1.636194	209.371799	4.416678
1.381420	207.823338	4.421683
1.754995	207.205240	4.426688
1.666426	205.801740	4.431693
1.335667	191.338335	4.436698
1.643072	194.577568	4.441702
1.763823	197.241600	4.446707
1.695991	193.123604	4.451712
1.523236	208.696839	4.456717
1.392245	212.478883	4.461722
1.443074	205.947505	4.466726
1.265217	199.603591	4.471731
1.504997	204.473156	4.476736
1.103323	210.208204	4.481741
1.193214	202.642550	4.486746
1.632199	206.111229	4.491750
1.380872	203.236651	4.496755
2.040029	216.051352	4.501760
1.832978	224.410429	4.506765
1.713933	208.155041	4.511770
1.513116	209.401197	4.516774
2.055441	222.683335	4.521779
2.239419	222.452252	4.526784
1.894836	215.719849	4.531789
2.059377	216.886975	4.536794
1.778915	207.825615	4.541798
1.545737	209.124265	4.546803
1.902325	205.436882	4.551808
1.819923	212.685078	4.556813
2.221909	208.566693	4.561818
1.837374	217.497553	4.566822
1.997840	215.036573	4.571827
2.088943	213.826556	4.576832
1.810242	220.086614	4.581837
1.625491	220.466585	4.586842
1.819030	228.307723	4.591846
2.370921	237.235159	4.596851
2.464428	220.725208	4.601856
2.140854	220.367511	4.606861
2.286874	210.183079	4.611866
2.002354	209.452315	4.616870
1.765581	207.018385	4.621875
2.115288	214.310032	4.626880
1.975724	217.890937	4.631885
2.307512	214.337124	4.636890
2.052667	208.647421	4.641894
2.046731	212.001880	4.646899
2.376133	208.938809	4.651904
2.003229	218.162081	4.656909
1.709120	207.486207	4.661914
1.635920	212.603816	4.666918
2.050653	224.963046	4.671923
2.558743	228.345040	4.676928
2.205106	242.073569	4.681933
2.397833	241.047039	4.686938
2.342388	232.497950	4.691942
2.271769	235.451206	4.696947
2.287826	219.661979	4.701952
1.922055	213.761760	4.706957
1.926684	226.608776	4.711962
2.265986	231.583073	4.716966
2.147846	243.924045	4.721971
2.471478	240.409461	4.726976
2.194410	244.473678	4.731981
2.516723	239.956412	4.736986
2.576009	241.136763	4.741990
2.393264	236.217254	4.746995
2.575175	228.985267	4.752000
2.338659	237.386902	4.757005
2.265145	242.061652	4.762010
2.500181	240.572965	4.767014
2.619883	245.337853	4.772019
2.652105	247.325994	4.777024
2.706388	243.951421	4.782029
2.432104	239.663082	4.787034
2.470537	235.867044	4.792038
2.696143	230.969377	4.797043
2.648568	222.953729	4.802048
2.013509	221.568878	4.807053
2.447477	223.725414	4.812058
2.504228	231.904219	4.817062
2.875573	231.466797	4.822067
2.882424	231.519550	4.827072
2.192733	222.477608	4.832077
2.318448	226.134267	4.837082
2.521942	241.478112	4.842086
2.639027	242.908886	4.847091
2.802329	241.845809	4.852096
2.476986	246.524970	4.857101
2.873100	241.733627	4.862106
2.659151	240.976055	4.867110
2.695160	247.168140	4.872115
2.696745	232.912378	4.877120
2.316796	235.451899	4.882125
2.637593	234.823035	4.887130
2.835912	237.816674	4.892134
2.726855	245.268345	4.897139
2.863515	245.452744	4.902144
2.642472	250.103012	4.907149
2.678080	249.173709	4.912154
2.715238	249.642513	4.917158
2.531120	246.396805	4.922163
2.754321	245.881210	4.927168
2.611092	243.514967	4.932173
2.584046	242.408762	4.937178
2.371498	241.204893	4.942182
2.419250	240.827344	4.947187
2.915855	252.620202	4.952192
2.745762	268.648646	4.957197
2.772779	264.345026	4.962202
2.912359	266.183579	4.967206
2.830568	273.064716	4.972211
3.015985	267.173571	4.977216
2.813854	277.256116	4.982221
3.023972	264.575015	4.987226
2.969071	256.864206	4.992230
2.756310	267.005347	4.997235
3.045692	259.614249	5.002240
2.797527	263.474657	5.007245
3.045880	262.335064	5.012250
2.996183	259.634723	5.017254
2.625890	268.772195	5.022259
3.008525	266.099451	5.027264
2.770515	259.499132	5.032269
3.061661	264.854251	5.037274
3.025405	259.469011	5.042278
3.058140	263.000953	5.047283
2.882256	252.708433	5.052288
2.455415	268.302298	5.057293
3.344196	280.777581	5.062298
3.251485	280.374446	5.067302
3.347232	283.368244	5.072307
3.370420	275.373192	5.077312
3.310418	293.067599	5.082317
3.561023	279.930939	5.087322
3.214144	268.791855	5.092326
2.835499	263.368176	5.097331
3.538189	272.427172	5.102336
3.247687	274.446581	5.107341
3.251706	268.172400	5.112346
2.972804	276.757819	5.117350
3.256099	284.752683	5.122355
3.156710	284.644811	5.127360
3.386749	285.659377	5.132365
3.766186	285.530736	5.137370
3.230269	291.213946	5.142374
3.318269	286.359835	5.147379
3.817631	280.650755	5.152384
3.297433	285.088186	5.157389
3.606063	271.110448	5.162394
3.308521	261.940991	5.167398
2.920084	266.465469	5.172403
3.341298	277.216573	5.177408
3.218699	278.773251	5.182413
3.444342	274.017933	5.187418
3.271102	281.992130	5.192422
3.626078	292.883268	5.197427
3.883362	279.024247	5.202432
3.517021	287.319571	5.207437
3.495241	286.174580	5.212442
3.416876	290.701405	5.217446
3.384709	284.632165	5.222451
3.647237	284.695729	5.227456
3.419667	294.902465	5.232461
3.386125	281.734116	5.237466
3.662174	298.012655	5.242470
3.405040	297.752177	5.247475
3.947803	286.186671	5.252480
3.654498	291.028530	5.257485
3.865511	291.549359	5.262490
3.693866	297.403642	5.267494
3.690198	292.155685	5.272499
3.685644	279.470033	5.277504
3.249184	286.887277	5.282509
3.267353	285.932215	5.287514
3.304641	286.353544	5.292518
3.175362	285.424603	5.297523
3.630197	300.887550	5.302528
3.825375	307.595866	5.307533
3.906154	314.616220	5.312538
4.109657	313.455133	5.317542
3.997624	319.575383	5.322547
3.695398	309.922585	5.327552
3.676637	315.588558	5.332557
3.824113	309.988039	5.337562
3.759852	310.289141	5.342566
3.698365	316.392029	5.347571
3.668383	310.021888	5.352576
3.685743	312.183190	5.357581
4.055180	319.424353	5.362586
3.898416	321.641239	5.367590
3.678661	320.071497	5.372595
4.083669	316.556884	5.377600
3.834808	329.301075	5.382605
4.143904	320.815406	5.387610
4.602199	320.367608	5.392614
4.192505	319.004606	5.397619
3.984595	320.084198	5.402624
4.092621	319.292310	5.407629
4.172449	317.508248	5.412634
4.313108	314.408109	5.417638
4.063843	323.033228	5.422643
3.944554	319.040271	5.427648
4.354061	315.521793	5.432653
3.945220	308.600047	5.437658
3.757333	300.255040	5.442662
3.901148	312.469854	5.447667
4.070082	317.062585	5.452672
4.112121	316.761853	5.457677
3.897434	313.622129	5.462682
4.256582	313.389081	5.467686
3.922753	314.048524	5.472691
4.111265	312.462672	5.477696
4.023442	323.055783	5.482701
4.041889	307.196506	5.487706
4.176101	310.779094	5.492710
4.041938	321.759063	5.497715
4.149943	309.660130	5.502720
4.349531	319.540950	5.507725
4.336634	319.473394	5.512730
4.248359	317.051129	5.517734
4.172493	317.863394	5.522739
4.428877	308.161587	5.527744
4.415059	316.145779	5.532749
4.252566	321.255175	5.537754
4.531097	313.941673	5.542758
4.350030	315.940884	5.547763
4.151249	308.397984	5.552768
4.185883	316.485361	5.557773
4.267720	315.605804	5.562778
4.611576	323.901299	5.567782
4.478401	332.688678	5.572787
4.563276	322.738326	5.577792
4.458190	323.529830	5.582797
4.030532	327.044883	5.587802
4.952138	329.131836	5.592806
4.211656	324.223212	5.597811
4.690706	326.163937	5.602816
4.527646	327.268183	5.607821
4.541280	329.600907	5.612826
4.713842	335.502848	5.617830
4.252939	327.772966	5.622835
4.555320	332.506272	5.627840
4.715523	343.639735	5.632845
4.526089	337.958787	5.637850
4.686534	341.970725	5.642854
4.914726	346.038553	5.647859
4.828549	331.710956	5.652864
4.348199	334.822933	5.657869
4.100447	330.144470	5.662874
4.623339	343.334814	5.667878
4.762517	341.269431	5.672883
4.748298	341.062878	5.677888
4.940854	338.884782	5.682893
4.776250	342.004546	5.687898
4.811287	336.222212	5.692902
4.476766	339.336795	5.697907
4.937664	342.036473	5.702912
4.405702	344.941356	5.707917
4.460576	342.955537	5.712922
4.365174	341.296830	5.717926
4.289180	346.218763	5.722931
4.415041	343.592314	5.727936
4.173842	342.725087	5.732941
4.671666	360.867375	5.737946
5.368067	365.387484	5.742950
5.315230	364.895882	5.747955
4.930042	347.495416	5.752960
4.657395	347.635978	5.757965
4.838818	354.232560	5.762970
5.158981	359.377549	5.767974
5.045115	356.529000	5.772979
5.080568	344.346428	5.777984
4.800881	342.077347	5.782989
4.820877	342.820904	5.787994
4.871857	353.335475	5.792998
4.901547	366.384331	5.798003
4.854814	363.965083	5.803008
4.982564	371.266043	5.808013
5.157202	370.017699	5.813018
4.999964	376.179807	5.818022
4.623242	373.327889	5.823027
5.311443	369.405346	5.828032
5.159279	371.200750	5.833037
5.161717	368.302454	5.838042
5.257377	373.185013	5.843046
4.874520	364.614072	5.848051
4.767228	361.251978	5.853056
4.691564	374.722197	5.858061
4.959022	370.067909	5.863066
5.047074	367.039226	5.868070
4.963076	378.334116	5.873075
5.293889	369.889335	5.878080
5.022076	373.927453	5.883085
5.448171	376.211782	5.888090
5.332471	370.392796	5.893094
5.030893	373.144756	5.898099
5.323559	367.543759	5.903104
4.853130	373.080760	5.908109
5.032012	381.762631	5.913114
5.289110	381.770094	5.918118
5.212112	387.628652	5.923123
5.335406	392.921360	5.928128
5.537038	388.865766	5.933133
5.353234	393.339432	5.938138
5.660936	386.790139	5.943142
5.324108	392.587915	5.948147
5.629498	381.454769	5.953152
4.968016	380.643486	5.958157
5.217413	394.553483	5.963162
5.542353	396.783963	5.968166
5.487143	399.326728	5.973171
5.703906	395.205503	5.978176
5.536777	386.670564	5.983181
5.478396	395.126795	5.988186
5.905678	392.896328	5.993190
5.487837	386.836481	5.998195
5.512253	376.813255	6.003200
5.369036	377.202581	6.008205
5.225069	379.521885	6.013210
5.453378	381.001790	6.018214
5.711891	391.885863	6.023219
5.455280	386.291288	6.028224
5.707530	389.570781	6.033229
5.518327	381.928284	6.038234
5.440110	369.453350	6.043238
5.235743	373.294308	6.048243
5.606787	385.891404	6.053248
5.411903	387.256869	6.058253
5.772768	392.588517	6.063258
5.602087	380.450670	6.068262
5.218871	378.378034	6.073267
5.260192	378.014139	6.078272
5.458635	383.978504	6.083277
5.293140	377.531363	6.088282
5.524797	399.511581	6.093286
5.470728	395.916570	6.098291
5.675967	389.145952	6.103296
5.339339	392.615207	6.108301
5.181733	395.873094	6.113306
5.572878	384.327967	6.118310
5.370046	397.947716	6.123315
5.465627	389.498421	6.128320
5.285813	387.704159	6.133325
5.663180	397.506723	6.138330
5.935535	389.700612	6.143334
5.378136	392.508225	6.148339
5.619558	388.319887	6.153344
5.516474	395.599851	6.158349
5.280167	395.652499	6.163354
5.620484	391.113409	6.168358
5.606266	396.256688	6.173363
5.654357	387.280122	6.178368
5.292186	390.013046	6.183373
5.406466	387.850295	6.188378
5.691322	381.168522	6.193382
5.501492	383.773373	6.198387
5.705129	388.556869	6.203392
5.581740	388.908307	6.208397
5.662580	395.593330	6.213402
5.875913	390.836734	6.218406
5.663480	403.312718	6.223411
5.623389	377.759392	6.228416
5.289749	374.182605	6.233421
5.322532	372.051527	6.238426
5.298580	377.604434	6.243430
5.552888	385.977175	6.248435
5.634195	396.009329	6.253440
5.588853	384.598600	6.258445
5.388998	387.337888	6.263450
5.849552	385.162353	6.268454
5.188772	388.087299	6.273459
5.559407	372.378770	6.278464
5.454952	389.466435	6.283469
5.222935	386.721697	6.288474
5.491324	388.559190	6.293478
5.164462	386.844769	6.298483
5.381704	391.613492	6.303488
5.409050	398.430230	6.308493
5.056099	392.575411	6.313498
5.584566	390.980914	6.318502
5.484303	390.477714	6.323507
5.521253	384.081307	6.328512
5.530990	386.284932	6.333517
5.367396	395.092897	6.338522
5.610851	396.475535	6.343526
5.411111	394.061123	6.348531
5.691929	391.170099	6.353536
5.527996	399.585819	6.358541
5.581723	393.471531	6.363546
5.588324	389.740527	6.368550
5.405074	396.102842	6.373555
5.692314	393.432278	6.378560
5.773813	396.229000	6.383565
5.882797	399.306177	6.388570
5.839161	385.766005	6.393574
5.487072	389.319923	6.398579
5.477288	380.456773	6.403584
5.705254	393.117279	6.408589
5.544144	397.600068	6.413594
6.178052	385.991833	6.418598
5.357243	392.469231	6.423603
5.649086	379.307095	6.428608
5.593986	374.775792	6.433613
5.552285	369.786830	6.438618
5.470993	368.815612	6.443622
5.187692	371.846296	6.448627
5.219808	365.697418	6.453632
5.358776	374.973948	6.458637
5.007735	380.074754	6.463642
5.408682	388.968822	6.468646
5.315742	398.661118	6.473651
5.644807	387.075036	6.478656
5.294693	387.107438	6.483661
5.499879	384.724894	6.488666
5.577051	387.395740	6.493670
5.575931	389.044244	6.498675
5.999621	389.288357	6.503680
5.886770	394.045201	6.508685
5.646123	390.140725	6.513690
5.659978	370.618531	6.518694
5.203377	367.984692	6.523699
5.684939	370.690648	6.528704
5.540917	367.122304	6.533709
5.487359	374.710918	6.538714
5.657246	371.403741	6.543718
5.235317	373.092453	6.548723
5.308179	367.465568	6.553728
5.341714	383.104912	6.558733
5.707181	400.217497	6.563738
5.768823	385.765603	6.568742
5.722521	386.981386	6.573747
5.484958	380.336660	6.578752
5.512491	380.354556	6.583757
5.583125	377.901214	6.588762
5.557835	370.283821	6.593766
5.241074	372.136489	6.598771
5.639110	365.440263	6.603776
5.378474	369.609516	6.608781
5.461245	367.078357	6.613786
5.284691	372.683495	6.618790
5.629961	379.010971	6.623795
5.935326	382.490997	6.628800
5.642476	380.420110	6.633805
5.568902	377.074909	6.638810
5.500629	367.626096	6.643814
5.371104	374.894349	6.648819
5.268356	376.577658	6.653824
5.516905	369.056832	6.658829
5.399021	371.245525	6.663834
5.762777	365.440474	6.668838
4.980861	372.512914	6.673843
5.502911	376.898823	6.678848
5.518305	384.277392	6.683853
5.228163	386.856734	6.688858
5.873080	379.995516	6.693862
5.708954	396.719161	6.698867
5.609087	381.504653	6.703872
5.616630	373.534139	6.708877
5.261754	372.814321	6.713882
5.494885	371.503087	6.718886
5.358008	367.993741	6.723891
5.655679	374.866455	6.728896
5.413013	377.144179	6.733901
5.444981	380.926196	6.738906
5.781436	377.045763	6.743910
5.456869	377.808169	6.748915
5.713364	371.526278	6.753920
5.818628	368.551861	6.758925
5.334500	363.154066	6.763930
5.837157	372.921292	6.768934
5.334534	365.754701	6.773939
5.869558	367.107758	6.778944
5.677411	364.711151	6.783949
5.588675	376.699629	6.788954
5.843652	365.533215	6.793958
5.640930	360.942643	6.798963
5.641666	361.448758	6.803968
5.753117	367.084983	6.808973
5.369215	360.387120	6.813978
5.738328	365.711148	6.818982
5.448460	365.601295	6.823987
5.713326	369.131916	6.828992
5.534784	368.005000	6.833997
5.652949	371.991890	6.839002
5.349918	365.657915	6.844006
5.541953	369.876909	6.849011
5.806962	370.550682	6.854016
5.292024	360.817082	6.859021
5.573245	368.470627	6.864026
5.586259	367.759968	6.869030
5.338395	372.939618	6.874035
5.469975	360.375079	6.879040
5.220220	357.557178	6.884045
5.151632	370.795342	6.889050
5.483938	358.079331	6.894054
5.479968	365.426107	6.899059
5.515524	367.815533	6.904064
5.694179	363.674938	6.909069
5.495180	369.413282	6.914074
5.480433	370.475457	6.919078
5.337502	368.153442	6.924083
5.313757	374.576335	6.929088
5.463071	376.011593	6.934093
5.374784	370.185175	6.939098
5.514512	371.090423	6.944102
5.404753	380.586014	6.949107
5.813608	370.667448	6.954112
5.603512	374.189764	6.959117
5.150410	376.550871	6.964122
5.330398	379.806813	6.969126
5.251159	378.585341	6.974131
5.348233	374.644105	6.979136
5.527145	377.055503	6.984141
5.297842	371.880618	6.989146
5.076182	367.052552	6.994150
5.279169	377.204954	6.999155
5.535536	391.094881	7.004160
5.456676	390.398526	7.009165
5.510323	394.721329	7.014170
6.013494	394.684152	7.019174
5.279757	390.195233	7.024179
5.458579	377.582198	7.029184
5.551581	382.642341	7.034189
5.579812	385.333462	7.039194
5.563046	382.510919	7.044198
5.322259	384.241029	7.049203
5.523283	388.256150	7.054208
5.859215	399.340142	7.059213
5.327202	381.570202	7.064218
5.367014	383.370517	7.069222
5.252397	387.804937	7.074227
5.893274	378.530439	7.079232
5.670278	371.661989	7.084237
5.399078	377.471687	7.089242
5.508873	370.788701	7.094246
5.318497	377.911408	7.099251
5.253496	385.046235	7.104256
5.564207	388.326117	7.109261
5.492727	392.570326	7.114266
5.788949	386.924477	7.119270
5.711225	401.303022	7.124275
5.643045	382.245999	7.129280
5.565643	374.779084	7.134285
5.027902	380.886543	7.139290
5.485301	383.735467	7.144294
5.320006	392.948650	7.149299
5.380699	388.747323	7.154304
5.530305	394.950247	7.159309
5.662344	395.815565	7.164314
5.876951	395.576547	7.169318
5.502657	386.795457	7.174323
5.534974	379.599355	7.179328
5.573201	373.648836	7.184333
5.226759	368.479535	7.189338
5.471569	377.217576	7.194342
5.556070	388.571659	7.199347
5.740253	387.293354	7.204352
5.379827	378.399379	7.209357
5.534967	381.459876	7.214362
5.429073	372.516784	7.219366
5.641442	386.176280	7.224371
5.591714	376.468314	7.229376
5.446227	377.971618	7.234381
5.347602	376.120424	7.239386
5.568550	370.052873	7.244390
5.489215	380.584586	7.249395
5.476900	387.062650	7.254400
5.976607	382.388017	7.259405
5.486573	379.806837	7.264410
5.327564	371.950838	7.269414
5.529956	370.660209	7.274419
5.506349	375.523374	7.279424
5.523706	366.554767	7.284429
5.401628	365.782885	7.289434
5.574231	366.037618	7.294438
5.286659	376.323345	7.299443
5.574796	377.211813	7.304448
5.382936	387.732577	7.309453
5.485772	395.179793	7.314458
5.665620	384.369908	7.319462
5.135347	393.959452	7.324467
5.453470	389.480766	7.329472
5.530065	396.944723	7.334477
5.648272	396.350560	7.339482
5.725636	389.859275	7.344486
5.583550	396.338566	7.349491
5.688167	390.801641	7.354496
5.353607	376.645557	7.359501
5.194878	378.508421	7.364506
5.596285	375.133559	7.369510
5.256168	389.223922	7.374515
5.503708	383.933662	7.379520
5.786146	385.512707	7.384525
5.599396	395.450557	7.389530
5.656294	388.987769	7.394534
5.611314	383.062856	7.399539
5.370174	372.008482	7.404544
5.144192	373.897636	7.409549
5.388888	386.716881	7.414554
5.615167	393.113507	7.419558
5.555891	395.650578	7.424563
5.752490	389.026835	7.429568
5.587487	384.806866	7.434573
5.288592	381.550529	7.439578
5.754542	380.146098	7.444582
5.273951	382.236244	7.449587
5.487282	382.408707	7.454592
5.986181	389.841710	7.459597
5.541407	382.612323	7.464602
5.679582	369.920202	7.469606
5.564996	376.006068	7.474611
5.379421	367.318989	7.479616
5.605393	371.760486	7.484621
5.394366	369.648387	7.489626
5.474460	368.617241	7.494630
5.354507	374.729252	7.499635
5.468853	363.869468	7.504640
5.480197	373.352527	7.509645
5.388743	370.434048	7.514650
5.544601	376.553735	7.519654
5.471058	382.785071	7.524659
5.424564	387.809988	7.529664
5.766447	381.423052	7.534669
5.459678	384.065092	7.539674
5.610821	377.128897	7.544678
5.498133	383.916813	7.549683
5.509978	373.123601	7.554688
5.666734	369.097145	7.559693
5.611507	368.460384	7.564698
5.573813	373.230831	7.569702
5.485894	374.807428	7.574707
5.463169	376.835775	7.579712
5.162694	374.383267	7.584717
5.158464	383.963668	7.589722
5.444948	389.227803	7.594726
5.519890	394.860230	7.599731
5.874303	394.893670	7.604736
5.812246	391.214484	7.609741
5.237013	380.224777	7.614746
5.518998	370.930232	7.619750
5.470399	383.377531	7.624755
5.125374	377.945419	7.629760
5.932037	386.365035	7.634765
5.564968	385.830610	7.639770
5.429094	381.384647	7.644774
5.596543	372.459106	7.649779
5.589143	370.821496	7.654784
5.402567	376.339613	7.659789
5.374979	374.176807	7.664794
5.846666	380.785152	7.669798
5.689445	383.913265	7.674803
5.570702	377.541102	7.679808
5.671379	366.395547	7.684813
5.228587	367.837573	7.689818
5.471675	375.307236	7.694822
5.003627	380.366149	7.699827
5.295198	382.307598	7.704832
6.006732	399.821875	7.709837
5.262249	376.352378	7.714842
5.403737	382.088333	7.719846
5.445675	397.194877	7.724851
5.602569	402.099548	7.729856
5.796154	397.864873	7.734861
5.632693	390.775177	7.739866
5.431151	371.191608	7.744870
5.320456	382.129996	7.749875
5.613280	368.717782	7.754880
5.656721	367.543648	7.759885
5.275625	372.579529	7.764890
5.456632	373.155652	7.769894
5.279751	380.057963	7.774899
5.776726	387.912039	7.779904
5.900021	373.931439	7.784909
5.442363	379.406343	7.789914
5.802279	379.141538	7.794918
5.314615	377.604012	7.799923
5.186061	374.150315	7.804928
5.285141	366.839421	7.809933
5.098938	391.529546	7.814938
5.809139	389.438525	7.819942
5.785373	396.975055	7.824947
5.752246	394.110765	7.829952
5.762595	375.389530	7.834957
5.236449	376.936283	7.839962
5.487842	367.583229	7.844966
5.568907	376.172760	7.849971
5.446076	379.690982	7.854976
5.588332	370.614343	7.859981
5.117753	377.736385	7.864986
5.173825	376.351479	7.869990
5.550612	390.311241	7.874995
5.655005	395.287358	7.880000
5.716628	393.509287	7.885005
5.803113	401.326042	7.890010
5.707498	383.386915	7.895014
5.527324	386.809664	7.900019
5.296264	374.655912	7.905024
5.364111	370.494604	7.910029
5.608153	377.983101	7.915034
5.508276	371.354906	7.920038
4.988962	381.939304	7.925043
5.365640	391.403456	7.930048
5.905863	398.633879	7.935053
5.637332	400.390457	7.940058
5.656435	385.790164	7.945062
5.514405	382.734027	7.950067
5.469264	382.911933	7.955072
5.633085	369.893121	7.960077
5.510044	376.185944	7.965082
5.514752	381.168087	7.970086
5.345275	378.400958	7.975091
5.297873	368.110512	7.980096
5.482273	379.461690	7.985101
5.367429	400.410706	7.990106
5.721791	397.119094	7.995110
5.489821	409.269099	8.000115
5.224861	403.100782	8.005133
5.669479	385.385260	8.010150
5.577751	397.804395	8.015168
5.579174	404.620393	8.020186
5.455814	396.573821	8.025203
5.677671	399.540329	8.030221
6.068875	389.545505	8.035238
5.395802	393.295101	8.040256
5.344570	375.555811	8.045274
5.095090	380.094628	8.050291
5.567279	391.179481	8.055309
5.565967	393.429693	8.060326
5.700977	406.047048	8.065344
5.944129	397.182901	8.070362
5.595643	386.135660	8.075379
5.199771	383.142677	8.080397
5.849794	395.051866	8.085414
5.784769	383.326209	8.090432
5.689249	369.579391	8.095450
5.710971	370.402822	8.100467
5.244028	377.335913	8.105485
5.652431	377.155604	8.110502
5.462047	389.523825	8.115520
5.621298	392.749375	8.120538
5.823982	400.098895	8.125555
5.594994	388.856331	8.130573
5.444345	386.046061	8.135590
5.649243	392.174002	8.140608
5.751412	387.172224	8.145626
5.830203	399.877218	8.150643
5.543200	386.759771	8.155661
5.703590	390.698318	8.160678
5.374747	393.977773	8.165696
5.552850	385.130072	8.170714
6.154217	394.604373	8.175731
5.663982	392.585394	8.180749
5.629419	380.810818	8.185766
5.521528	396.504863	8.190784
5.710801	393.297702	8.195802
5.793615	391.123233	8.200819
5.986371	397.609654	8.205837
5.714622	384.742284	8.210854
5.257504	383.560706	8.215872
5.699865	391.292605	8.220890
5.766473	402.945516	8.225907
5.665105	400.468380	8.230925
6.113197	395.030907	8.235942
5.775492	401.722990	8.240960
5.913920	394.904227	8.245978
5.826850	401.850761	8.250995
5.826348	396.498911	8.256013
5.889196	382.351904	8.261030
5.295408	381.106403	8.266048
5.334695	387.380041	8.271066
5.440218	390.623423	8.276083
5.456632	400.993491	8.281101
5.881533	397.295231	8.286118
5.412602	397.522906	8.291136
5.500452	400.014843	8.296154
5.725278	404.091675	8.301171
6.046223	403.681999	8.306189
6.116555	394.216789	8.311206
5.852848	402.430991	8.316224
5.930828	395.826756	8.321242
6.094859	401.453005	8.326259
5.895574	402.358183	8.331277
5.886499	400.482027	8.336294
6.158268	405.296281	8.341312
5.874447	397.776439	8.346330
5.975501	402.481580	8.351347
5.968169	400.109717	8.356365
6.059072	399.697991	8.361382
5.723560	407.771905	8.366400
5.889622	391.608144	8.371418
5.913059	400.534991	8.376435
5.615823	402.970127	8.381453
5.941457	399.590264	8.386470
5.542734	403.366570	8.391488
5.576084	392.679574	8.396506
5.656208	399.514874	8.401523
5.553819	400.360786	8.406541
5.664931	402.678697	8.411558
5.690104	415.395207	8.416576
5.768188	416.058394	8.421594
5.775305	422.381233	8.426611
5.854899	427.499955	8.431629
6.197387	416.897350	8.436646
6.165159	431.210097	8.441664
6.000080	426.928380	8.446682
6.034102	430.062987	8.451699
6.100694	429.361570	8.456717
6.466978	423.286764	8.461734
6.038717	404.968707	8.466752
5.583008	398.617968	8.471770
6.328507	402.629511	8.476787
6.084815	401.357900	8.481805
5.987276	401.259520	8.486822
5.837399	405.022327	8.491840
5.843319	407.116788	8.496858
6.138934	411.444519	8.501875
5.841075	425.164334	8.506893
6.058019	419.374699	8.511910
5.946147	421.459101	8.516928
6.097431	417.762415	8.521946
6.093352	413.370432	8.526963
5.859407	417.594432	8.531981
6.103457	410.352140	8.536998
6.041264	423.505114	8.542016
6.105769	420.569826	8.547034
6.170915	414.428305	8.552051
5.933532	424.673809	8.557069
5.957815	419.520055	8.562087
6.280694	422.505550	8.567104
6.094317	421.518488	8.572122
6.328839	426.281746	8.577139
6.028143	429.228639	8.582157
6.502924	416.980279	8.587175
6.380299	419.848954	8.592192
6.108716	411.774963	8.597210
6.139798	398.576426	8.602227
6.206690	401.759556	8.607245
5.950399	394.926514	8.612263
6.005824	413.782342	8.617280
6.272551	421.203947	8.622298
6.608522	410.608672	8.627315
6.018920	409.958933	8.632333
6.001842	404.224673	8.637351
6.042527	410.693752	8.642368
6.601158	416.144964	8.647386
6.468262	407.945245	8.652403
5.743477	411.308440	8.657421
6.143947	410.122717	8.662439
6.349343	425.720676	8.667456
6.247784	423.836827	8.672474
6.372899	408.828081	8.677491
6.067968	412.129062	8.682509
6.029193	416.253250	8.687527
6.287383	429.217497	8.692544
6.232318	427.474725	8.697562
6.497370	417.742511	8.702579
6.344627	421.467900	8.707597
6.338584	410.111720	8.712615
6.261280	411.622723	8.717632
6.047774	407.007742	8.722650
6.399947	412.494254	8.727667
6.404358	418.460925	8.732685
6.216446	416.486386	8.737703
6.302642	422.071115	8.742720
6.312653	422.391469	8.747738
6.384449	416.621278	8.752755
6.216543	412.440986	8.757773
6.256070	411.614403	8.762791
6.475234	417.191049	8.767808
6.343772	425.772816	8.772826
6.611709	412.622594	8.777843
6.253553	412.369142	8.782861
6.281486	409.953920	8.787879
6.273472	408.519388	8.792896
6.155260	421.573790	8.797914
6.654301	425.311302	8.802931
6.425547	421.714809	8.807949
6.432397	422.805633	8.812967
6.310761	411.735679	8.817984
6.464512	421.689921	8.823002
6.407857	408.173694	8.828019
6.328325	413.714799	8.833037
6.435269	416.891696	8.838055
6.539313	428.860670	8.843072
6.313758	424.847134	8.848090
6.716475	412.976051	8.853107
6.340890	408.067586	8.858125
6.331149	409.445000	8.863143
6.673290	410.859140	8.868160
6.302429	411.238795	8.873178
6.390279	404.118649	8.878195
6.454123	409.126216	8.883213
6.494629	416.381080	8.888231
6.635488	416.236116	8.893248
6.169544	430.136731	8.898266
6.743080	425.004750	8.903283
6.504684	429.371450	8.908301
6.519117	416.150247	8.913319
6.316162	413.288159	8.918336
6.572912	419.947652	8.923354
6.637658	423.150054	8.928371
6.439037	422.941187	8.933389
6.183657	421.122312	8.938407
6.230506	423.806819	8.943424
6.273015	425.561087	8.948442
6.493005	423.718688	8.953459
6.326084	425.470852	8.958477
6.638092	427.770111	8.963495
6.954561	417.947845	8.968512
6.895431	423.479465	8.973530
6.663614	418.532834	8.978547
6.572525	429.459272	8.983565
6.524044	429.712997	8.988583
6.536933	429.190346	8.993600
6.356521	425.671529	8.998618
6.628932	427.494138	9.003635
6.077868	435.847766	9.008653
6.167607	425.161438	9.013671
6.611905	421.548512	9.018688
6.518086	431.525527	9.023706
6.953595	428.829104	9.028723
6.489215	427.427757	9.033741
6.406824	426.083696	9.038759
6.527928	416.960845	9.043776
6.575049	432.558207	9.048794
6.640790	438.685741	9.053811
6.566247	450.265990	9.058829
6.816627	458.987127	9.063847
6.848688	446.605716	9.068864
6.452557	437.718013	9.073882
6.899291	443.757828	9.078899
6.346269	448.123028	9.083917
6.921004	452.767054	9.088935
6.854588	450.016239	9.093952
6.714010	457.819996	9.098970
7.077804	447.116231	9.103987
6.784566	442.620947	9.109005
6.705498	435.911767	9.114023
6.731242	429.757442	9.119040
6.760437	439.983539	9.124058
6.644904	426.747851	9.129075
6.605069	433.418814	9.134093
6.910791	438.253036	9.139111
7.154187	437.019187	9.144128
6.468717	441.632214	9.149146
6.843624	437.963819	9.154163
6.950707	425.270956	9.159181
6.856687	438.425740	9.164199
6.993171	431.651444	9.169216
6.619273	432.552254	9.174234
6.722692	420.778256	9.179251
7.004287	427.945098	9.184269
6.371479	437.021473	9.189287
6.618498	443.919163	9.194304
6.863835	452.259249	9.199322
6.993750	451.787801	9.204339
7.351850	453.540271	9.209357
6.744422	446.458937	9.214375
7.159911	449.202811	9.219392
7.163719	451.890868	9.224410
6.432086	430.495926	9.229427
6.565339	442.785394	9.234445
6.830874	446.827497	9.239463
7.078628	442.216425	9.244480
6.974569	461.352743	9.249498
7.175543	458.030146	9.254515
7.278726	452.709470	9.259533
6.803486	443.976086	9.264551
6.894674	441.500520	9.269568
6.556969	443.279276	9.274586
6.952432	441.857657	9.279603
7.285843	448.132858	9.284621
7.225993	458.095132	9.289639
7.001742	442.503311	9.294656
6.366725	434.425937	9.299674
7.170143	450.123301	9.304691
7.013747	456.026664	9.309709
7.108992	460.603343	9.314727
7.312058	460.357179	9.319744
6.763230	446.933332	9.324762
7.317850	454.004028	9.329779
7.039787	442.011716	9.334797
6.995444	434.205276	9.339815
6.932649	423.571099	9.344832
6.826706	439.640400	9.349850
7.055839	451.340618	9.354867
7.142718	455.988022	9.359885
6.879865	453.305659	9.364903
6.869627	446.065077	9.369920
6.605008	456.955436	9.374938
6.888408	456.024611	9.379955
6.913801	458.264362	9.384973
7.245052	466.294447	9.389991
7.656405	448.476750	9.395008
7.415566	463.494155	9.400026
7.395611	459.669495	9.405043
7.546565	457.276136	9.410061
6.787788	439.331380	9.415079
7.059220	447.386548	9.420096
7.010887	461.869076	9.425114
7.340376	462.530990	9.430131
7.428254	469.879480	9.435149
7.097617	471.190102	9.440167
7.438383	455.065351	9.445184
6.888680	444.671066	9.450202
7.291223	450.238105	9.455219
7.214095	451.824820	9.460237
7.124714	459.974039	9.465255
7.435913	453.642724	9.470272
7.213612	446.110127	9.475290
7.172461	437.684682	9.480307
7.246799	441.996381	9.485325
7.198340	448.615046	9.490343
7.374701	445.176369	9.495360
7.081241	440.482314	9.500378
7.232550	458.098870	9.505395
7.036472	451.306921	9.510413
7.292559	448.401757	9.515431
7.135980	448.476664	9.520448
7.114404	451.310677	9.525466
7.146705	456.607177	9.530483
7.346091	448.983678	9.535501
7.123883	449.595796	9.540519
7.427878	453.827562	9.545536
7.278315	448.628287	9.550554
7.030618	451.519596	9.555571
6.622878	452.605548	9.560589
6.831764	450.117967	9.565607
7.165607	445.701764	9.570624
7.145889	465.752715	9.575642
7.147911	464.322928	9.580659
7.657982	470.996644	9.585677
7.555093	475.616798	9.590695
7.604267	471.945466	9.595712
7.505161	464.087582	9.600730
7.235601	453.671763	9.605747
7.272659	457.998738	9.610765
7.388453	469.322158	9.615783
7.535460	466.493932	9.620800
7.432490	468.927230	9.625818
7.409716	475.437770	9.630835
7.674974	476.832330	9.635853
7.162692	466.567898	9.640871
7.401315	460.569757	9.645888
7.472982	467.018254	9.650906
7.291414	473.925884	9.655923
7.600270	472.281072	9.660941
7.601901	486.159423	9.665959
7.729637	477.657172	9.670976
7.446323	471.468905	9.675994
7.131240	477.340180	9.681011
7.463903	473.362790	9.686029
7.602770	487.241863	9.691047
7.706095	483.562098	9.696064
7.795577	482.790846	9.701082
7.970943	467.673245	9.706099
7.950700	461.645984	9.711117
7.634273	456.106630	9.716135
7.650715	451.042446	9.721152
7.565605	454.280808	9.726170
7.166679	450.127010	9.731187
7.369363	437.829487	9.736205
7.000980	445.211137	9.741223
7.714042	459.000788	9.746240
7.632848	465.514109	9.751258
7.542199	471.498753	9.756275
7.290791	463.014518	9.761293
7.621653	475.456269	9.766311
7.636905	470.849834	9.771328
7.841987	481.525073	9.776346
7.786796	478.324403	9.781363
7.939958	468.312951	9.786381
7.183957	462.968263	9.791399
7.366443	463.514216	9.796416
7.442695	472.540169	9.801434
7.572439	479.673872	9.806451
7.683132	476.851298	9.811469
7.477773	485.201614	9.816487
7.631601	482.189296	9.821504
7.736645	475.924783	9.826522
7.867146	484.320631	9.831539
8.108603	479.278207	9.836557
7.685686	472.480544	9.841575
7.943195	478.480409	9.846592
8.121847	477.509090	9.851610
7.569964	488.131785	9.856627
7.992127	481.376104	9.861645
7.747153	487.362693	9.866663
8.031390	478.993858	9.871680
7.646111	462.281589	9.876698
7.631251	472.830129	9.881715
7.361240	477.413191	9.886733
7.441353	486.195564	9.891751
8.149239	483.425168	9.896768
8.084455	481.469320	9.901786
7.855826	481.678515	9.906803
7.869011	474.156576	9.911821
7.893547	490.710513	9.916839
7.719571	469.831428	9.921856
7.793905	476.500409	9.926874
7.742223	481.447092	9.931891
7.715233	476.739940	9.936909
7.980614	476.392560	9.941927
8.032357	472.922789	9.946944
7.949171	476.157700	9.951962
7.869186	480.679620	9.956979
8.069540	478.171275	9.961997
8.085855	488.311046	9.967015
7.985634	480.547998	9.972032
7.937317	487.734673	9.977050
7.732688	485.655437	9.982067
8.085048	489.491536	9.987085
7.760211	480.053095	9.992103
7.800043	474.773833	9.997120
8.072615	477.347469	10.002138
7.813252	484.983548	10.007155
7.987610	484.057077	10.012173
7.806828	485.120316	10.017191
7.739778	485.345377	10.022208
7.924773	485.146206	10.027226
8.017781	493.342779	10.032243
8.152996	489.534976	10.037261
8.208312	487.462602	10.042279
8.095458	480.613505	10.047296
8.151053	481.400111	10.052314
7.933267	490.254114	10.057331
7.925337	486.941947	10.062349
7.601518	484.439477	10.067367
7.818312	477.030996	10.072384
7.669135	477.682235	10.077402
7.767798	480.977192	10.082419
7.634336	480.527816	10.087437
8.123278	505.324611	10.092455
8.005535	502.487110	10.097472
8.263048	507.196319	10.102490
8.443160	511.210713	10.107507
8.275406	503.944141	10.112525
7.948981	503.234488	10.117543
8.002967	504.037124	10.122560
8.068242	500.842939	10.127578
7.798136	511.169323	10.132595
8.177219	504.492921	10.137613
7.927262	503.998570	10.142631
8.089198	504.206913	10.147648
8.459827	501.624718	10.152666
8.258093	510.413118	10.157683
8.210808	506.352872	10.162701
8.221077	506.799414	10.167719
8.146499	500.294629	10.172736
7.968116	499.334719	10.177754
7.840447	506.950303	10.182771
8.156548	502.565250	10.187789
8.056317	502.722897	10.192807
8.267230	507.931645	10.197824
8.147514	495.797882	10.202842
8.270171	508.988408	10.207859
8.491778	501.781129	10.212877
8.259669	499.766127	10.217895
7.964696	495.533020	10.222912
8.281986	501.372113	10.227930
8.171998	500.325818	10.232947
8.098280	501.498615	10.237965
8.556208	508.013214	10.242983
8.172258	510.427153	10.248000
8.613562	517.509207	10.253018
8.557235	520.424378	10.258035
8.476492	498.694493	10.263053
8.561026	492.654064	10.268071
8.119467	496.651643	10.273088
8.548884	493.119910	10.278106
8.395165	504.987064	10.283123
8.307118	505.556206	10.288141
8.516313	508.647775	10.293159
8.271781	507.126989	10.298176
8.623133	500.379170	10.303194
8.331220	500.490926	10.308211
8.278707	500.265621	10.313229
8.339844	507.697182	10.318247
8.107594	506.177640	10.323264
8.613644	513.208588	10.328282
8.556457	532.154655	10.333299
8.370635	530.694152	10.338317
8.554300	526.960845	10.343335
8.690310	530.748591	10.348352
8.781992	514.044058	10.353370
8.387676	513.266084	10.358387
8.599153	507.095437	10.363405
8.500450	500.566006	10.368423
8.278965	501.010764	10.373440
8.400920	508.344497	10.378458
8.309999	529.826654	10.383475
8.806865	524.040737	10.388493
8.951696	525.993669	10.393511
8.515367	521.451219	10.398528
8.606520	505.163325	10.403546
8.531831	517.463130	10.408563
8.677896	518.655355	10.413581
8.560874	512.879820	10.418599
8.512247	529.230599	10.423616
8.884544	528.655142	10.428634
8.513763	520.322003	10.433651
8.579606	514.710491	10.438669
8.940413	509.346532	10.443687
8.459348	515.672832	10.448704
8.586152	519.503032	10.453722
8.664720	520.696299	10.458739
8.948773	516.543440	10.463757
8.913780	511.821746	10.468775
8.713107	505.671091	10.473792
8.679877	498.705453	10.478810
8.478067	498.888383	10.483827
8.424975	506.227281	10.488845
8.873840	513.996090	10.493863
8.696803	525.295713	10.498880
9.024981	521.536751	10.503898
8.724129	517.310865	10.508915
8.779042	519.034810	10.513933
8.836996	509.978546	10.518951
8.657825	511.874630	10.523968
9.027320	515.834294	10.528986
8.749905	516.641194	10.534003
8.857845	505.226182	10.539021
8.575704	505.232280	10.544039
8.708675	519.156475	10.549056
9.123271	519.849320	10.554074
8.967326	517.371198	10.559091
8.869731	510.122101	10.564109
8.587529	508.966926	10.569127
8.931378	523.849169	10.574144
8.950837	520.012047	10.579162
8.994161	528.680254	10.584179
9.073422	519.516531	10.589197
8.626297	498.118234	10.594215
8.613532	520.282454	10.599232
9.139464	521.087347	10.604250
8.674628	518.663629	10.609267
8.896734	527.546986	10.614285
9.138985	526.259663	10.619303
8.908335	532.644806	10.624320
9.215735	526.654868	10.629338
9.231769	530.095237	10.634355
9.047425	523.967279	10.639373
8.934622	515.947410	10.644391
8.817426	512.655406	10.649408
9.066910	513.989312	10.654426
8.873854	528.062101	10.659443
9.125262	528.751953	10.664461
9.057384	528.497483	10.669479
8.855293	533.940948	10.674496
8.696699	529.500414	10.679514
8.979795	519.998855	10.684531
9.147100	527.628479	10.689549
9.593171	526.034880	10.694567
8.997524	534.464919	10.699584
9.046689	529.316726	10.704602
9.521763	527.175837	10.709619
9.315696	523.055106	10.714637
8.821805	511.030082	10.719655
8.888585	528.322212	10.724672
9.127978	521.216294	10.729690
9.042585	525.445590	10.734707
8.766978	532.033384	10.739725
9.214676	531.029639	10.744743
9.146156	533.766838	10.749760
9.198174	528.466729	10.754778
9.158146	531.249982	10.759795
8.826002	535.142176	10.764813
9.130205	531.699356	10.769831
9.188042	535.480340	10.774848
9.046656	530.371282	10.779866
8.937440	530.344144	10.784883
9.082041	528.270487	10.789901
9.187709	535.284890	10.794919
9.008568	537.335600	10.799936
9.116335	534.169505	10.804954
9.118282	532.036011	10.809971
8.805690	535.697952	10.814989
9.319381	546.460875	10.820007
9.321001	556.729200	10.825024
9.347330	558.164123	10.830042
9.555626	561.987956	10.835059
9.272770	554.237533	10.840077
9.543097	554.255438	10.845095
9.348626	553.215983	10.850112
9.051001	538.904080	10.855130
9.586388	554.122583	10.860147
9.268412	561.288160	10.865165
9.189063	559.839477	10.870183
9.145437	565.334015	10.875200
9.597986	559.542364	10.880218
9.600459	558.279749	10.885235
9.143036	561.961090	10.890253
9.193640	553.294096	10.895271
9.280424	560.696441	10.900288
9.415002	560.940601	10.905306
9.396296	554.401851	10.910323
9.260672	563.189450	10.915341
9.416667	559.902238	10.920359
9.494773	556.892230	10.925376
9.421083	562.066414	10.930394
9.416024	563.051808	10.935411
9.449454	565.236674	10.940429
9.270788	555.870104	10.945447
9.220296	569.542049	10.950464
9.284569	557.887661	10.955482
9.471294	549.530819	10.960499
9.694715	563.049664	10.965517
9.562686	559.516974	10.970535
9.381807	559.488372	10.975552
9.328888	560.074136	10.980570
9.801528	562.802819	10.985587
9.628321	571.353287	10.990605
9.625652	566.916868	10.995623
9.246056	566.385897	11.000640
9.368347	578.175413	11.005658
9.768147	581.335144	11.010675
9.691654	582.931238	11.015693
9.797294	575.476909	11.020711
9.736920	574.953038	11.025728
9.750478	577.150468	11.030746
10.223061	575.937728	11.035763
9.186960	569.648892	11.040781
9.677279	559.446046	11.045799
9.594920	582.599437	11.050816
9.806281	578.158092	11.055834
10.131647	579.600104	11.060851
9.683762	566.977767	11.065869
9.601132	557.138672	11.070887
9.617523	569.263393	11.075904
9.996470	571.624828	11.080922
10.026757	557.454351	11.085939
9.720512	561.020640	11.090957
9.727828	553.916129	11.095975
9.471987	563.691237	11.100992
10.128968	575.596309	11.106010
10.094617	556.560385	11.111027
9.772559	565.481150	11.116045
9.622348	554.526004	11.121063
9.644227	555.033853	11.126080
10.001384	565.944230	11.131098
9.898455	559.749937	11.136115
9.647406	559.085348	11.141133
10.070056	573.791269	11.146151
9.786118	573.968052	11.151168
10.131391	575.113487	11.156186
9.955311	561.640983	11.161203
9.686216	563.532140	11.166221
9.988073	568.417490	11.171239
9.899862	572.088684	11.176256
9.979900	573.972817	11.181274
10.009693	576.382304	11.186291
9.814625	585.292774	11.191309
10.229079	579.226194	11.196327
10.094629	581.389866	11.201344
10.119920	573.367404	11.206362
10.094335	559.868315	11.211379
9.707771	561.951322	11.216397
10.114004	564.207527	11.221415
10.061396	560.324815	11.226432
9.809120	564.463345	11.231450
10.165574	562.470303	11.236467
10.262476	577.618248	11.241485
10.496003	573.703606	11.246503
10.217283	567.716553	11.251520
9.612032	561.815055	11.256538
9.955515	554.150141	11.261555
9.514760	566.999260	11.266573
9.864593	569.062284	11.271591
9.873755	569.799322	11.276608
9.909158	584.486653	11.281626
10.215780	579.841136	11.286643
9.926544	585.702110	11.291661
10.068234	579.627507	11.296679
10.268534	585.560579	11.301696
10.104400	588.994299	11.306714
10.207350	584.358402	11.311731
9.944703	583.818689	11.316749
9.993359	583.959467	11.321767
9.755476	585.372415	11.326784
10.275651	600.258825	11.331802
10.663334	596.471649	11.336819
10.040116	594.889901	11.341837
9.907076	597.438347	11.346855
10.258372	604.051632	11.351872
10.217301	611.271941	11.356890
10.752446	599.853468	11.361907
10.423466	609.800927	11.366925
10.129306	594.535425	11.371943
10.383715	591.362267	11.376960
10.008753	599.076351	11.381978
10.378708	606.819619	11.386995
10.909534	606.389884	11.392013
10.764182	600.880652	11.397031
10.540100	577.465768	11.402048
10.460690	585.534600	11.407066
10.384232	577.660517	11.412083
10.372361	581.376628	11.417101
10.129207	583.288993	11.422119
10.075831	586.497193	11.427136
9.988758	595.794780	11.432154
10.669520	595.815052	11.437171
10.577495	601.986139	11.442189
10.569672	600.169726	11.447207
10.518168	587.457258	11.452224
10.454060	589.912924	11.457242
10.468812	576.694708	11.462259
10.557877	584.450143	11.467277
10.522110	583.411221	11.472295
10.522843	577.724623	11.477312
10.527729	584.877808	11.482330
10.966714	582.297582	11.487347
10.468762	580.522769	11.492365
10.600192	579.161182	11.497383
10.558602	575.671211	11.502400
10.199552	580.823561	11.507418
10.524663	579.999840	11.512435
10.756352	590.440638	11.517453
10.717207	591.459741	11.522471
10.678041	577.139122	11.527488
10.375069	578.644252	11.532506
10.393308	589.424383	11.537523
10.770623	599.110396	11.542541
10.739544	597.240801	11.547559
10.946467	599.540665	11.552576
10.698859	597.973016	11.557594
10.835694	587.083606	11.562611
10.536494	586.170904	11.567629
10.772445	592.786364	11.572647
10.645852	579.662733	11.577664
10.877002	591.182855	11.582682
10.726528	592.500147	11.587699
10.812884	592.429937	11.592717
10.528025	589.962410	11.597735
10.771542	591.272005	11.602752
10.596428	598.080851	11.607770
10.867651	602.933113	11.612787
10.778207	605.010889	11.617805
10.468529	611.168532	11.622823
10.858303	599.996746	11.627840
10.253831	604.922237	11.632858
10.868452	600.307652	11.637875
10.951388	611.563698	11.642893
10.801349	606.455965	11.647911
10.983899	607.734030	11.652928
10.877045	599.561724	11.657946
10.989387	600.920145	11.662963
11.032610	605.946756	11.667981
10.970576	594.857940	11.672999
11.053388	598.884348	11.678016
10.805561	598.821990	11.683034
10.905974	601.182617	11.688051
10.658108	594.575394	11.693069
10.557231	606.276604	11.698087
10.878676	597.191894	11.703104
10.869899	600.273236	11.708122
10.939954	596.920506	11.713139
10.966594	604.994926	11.718157
10.739691	606.658620	11.723175
11.013136	615.183747	11.728192
11.414947	631.631740	11.733210
11.202622	617.167642	11.738227
11.034751	607.780430	11.743245
10.602926	607.465864	11.748263
10.978613	615.495409	11.753280
11.041074	623.059351	11.758298
11.235833	627.260832	11.763315
11.294556	624.783984	11.768333
11.338735	620.636891	11.773351
10.911234	613.593746	11.778368
11.215045	622.051034	11.783386
11.320698	613.930839	11.788403
11.578614	608.447176	11.793421
10.874489	601.421859	11.798439
11.266366	598.006399	11.803456
11.089507	614.500293	11.808474
11.373562	609.709965	11.813491
10.711623	608.667553	11.818509
10.964697	617.779654	11.823527
11.279377	615.392338	11.828544
11.291802	633.100116	11.833562
11.039248	635.654553	11.838579
11.208640	631.421694	11.843597
11.143855	631.602225	11.848615
11.383085	630.167048	11.853632
11.305699	627.351644	11.858650
11.178858	632.452076	11.863667
11.296441	632.086681	11.868685
11.361036	631.537040	11.873703
11.522539	630.694610	11.878720
11.363595	634.853337	11.883738
11.534069	631.447097	11.888755
11.489251	628.860143	11.893773
11.090473	631.440502	11.898791
11.196011	628.038062	11.903808
11.139398	636.223284	11.908826
11.180354	634.891558	11.913843
11.442234	634.080835	11.918861
11.668143	629.810775	11.923879
11.832963	631.946792	11.928896
11.700713	634.195331	11.933914
11.421153	631.805864	11.938931
11.629495	625.077109	11.943949
10.900890	632.836802	11.948967
11.509856	628.854226	11.953984
11.156054	630.556615	11.959002
11.506153	631.237417	11.964019
11.673555	632.909146	11.969037
11.706639	632.367567	11.974055
11.694997	623.662894	11.979072
11.192020	633.643769	11.984090
11.284956	631.947358	11.989107
11.812645	637.368745	11.994125
11.981390	645.540973	11.999143
11.656223	631.621432	12.004160
11.876959	627.446849	12.009178
11.958932	627.598218	12.014195
11.655859	622.466972	12.019213
11.699992	625.032017	12.024231
11.515354	619.487872	12.029248
11.137576	635.179969	12.034266
11.118344	631.828511	12.039283
11.443609	640.525456	12.044301
11.714340	644.229137	12.049319
11.644555	644.154836	12.054336
11.647190	652.179367	12.059354
11.596224	647.147712	12.064371
11.914341	641.733558	12.069389
12.108835	655.225419	12.074407
12.124002	654.632982	12.079424
12.351459	650.473125	12.084442
12.232960	635.044544	12.089459
12.073527	626.937214	12.094477
11.849932	619.631954	12.099495
11.947344	614.324751	12.104512
11.648271	620.203047	12.109530
11.387392	620.183745	12.114547
11.840538	628.160212	12.119565
11.847672	637.225411	12.124583
12.120030	646.006332	12.129600
12.113933	641.377931	12.134618
11.949204	636.386081	12.139635
11.813321	639.490377	12.144653
11.591610	642.090504	12.149671
12.129675	635.733270	12.154688
11.927942	641.949853	12.159706
11.809751	648.118720	12.164723
12.244122	644.519917	12.169741
12.219470	642.396862	12.174759
12.097781	639.970192	12.179776
12.078734	636.249489	12.184794
12.022943	638.306251	12.189811
12.435630	638.557602	12.194829
12.151822	624.798878	12.199847
12.057209	626.533492	12.204864
11.996518	622.582601	12.209882
11.971019	636.465292	12.214899
12.317854	637.484260	12.219917
12.233319	642.985191	12.224935
12.325171	627.864679	12.229952
11.739048	624.279606	12.234970
12.339057	638.645555	12.239987
12.635253	643.967292	12.245005
11.925353	634.601344	12.250023
11.830707	625.294236	12.255040
11.955336	634.975432	12.260058
12.330839	642.951372	12.265075
12.105366	639.401659	12.270093
12.291832	649.511875	12.275111
12.579294	653.077258	12.280128
12.191405	648.401006	12.285146
12.154797	652.887815	12.290163
12.385375	643.340721	12.295181
12.049220	646.056493	12.300199
12.479421	637.554409	12.305216
12.461577	652.149105	12.310234
12.521105	640.586916	12.315251
12.422050	642.233863	12.320269
12.420614	647.292685	12.325287
12.329127	641.494198	12.330304
12.157238	648.684399	12.335322
12.072695	651.212680	12.340339
12.323959	651.129416	12.345357
12.088561	653.760077	12.350375
11.945496	646.451734	12.355392
12.269942	645.681761	12.360410
11.875294	650.467302	12.365427
12.222313	654.534634	12.370445
12.596247	651.765718	12.375463
12.739952	661.103144	12.380480
12.740363	666.953761	12.385498
12.723509	661.197294	12.390515
12.758195	656.811838	12.395533
12.689415	644.688978	12.400551
12.799617	642.425010	12.405568
12.238887	637.393834	12.410586
11.752982	645.052631	12.415603
12.499529	649.152427	12.420621
12.646949	658.962626	12.425639
12.533614	662.041325	12.430656
12.707112	665.621299	12.435674
12.531620	673.181287	12.440691
12.507053	663.626571	12.445709
12.608015	663.181716	12.450727
12.418552	664.722826	12.455744
12.500794	663.271065	12.460762
12.491986	661.713565	12.465779
12.783078	658.446324	12.470797
12.366397	660.729685	12.475815
12.886171	662.977692	12.480832
12.968358	654.798017	12.485850
12.556513	664.070469	12.490867
13.113472	662.437503	12.495885
12.948083	664.959440	12.500903
12.619718	664.909620	12.505920
12.776227	655.260447	12.510938
12.781792	661.697217	12.515955
12.922530	662.656760	12.520973
12.677902	666.229254	12.525991
12.781925	662.012876	12.531008
13.091877	657.767593	12.536026
12.905852	664.606565	12.541043
13.202693	662.446075	12.546061
13.140176	666.630819	12.551079
12.918997	658.337437	12.556096
12.738466	661.237256	12.561114
12.561738	662.299875	12.566131
13.003323	671.190155	12.571149
12.780724	670.647359	12.576167
12.778035	658.776121	12.581184
13.015455	656.479722	12.586202
12.615633	664.346022	12.591219
13.148994	666.976908	12.596237
12.858817	676.205177	12.601255
13.073514	685.818731	12.606272
13.611285	682.620372	12.611290
13.094527	688.112877	12.616307
13.652698	675.728285	12.621325
13.155422	665.537137	12.626343
13.248819	672.319984	12.631360
13.282521	667.341410	12.636378
13.035013	653.176240	12.641395
13.179449	656.779671	12.646413
13.002909	652.124159	12.651431
12.901020	656.662156	12.656448
13.114646	647.912932	12.661466
12.919837	665.056583	12.666483
13.274276	663.259496	12.671501
13.400012	677.989642	12.676519
13.372817	681.594556	12.681536
13.274382	674.736827	12.686554
13.182274	678.509631	12.691571
13.663139	669.718787	12.696589
13.459517	675.866252	12.701607
12.759446	668.196517	12.706624
13.103320	666.167553	12.711642
13.204221	677.168388	12.716659
13.056673	688.649709	12.721677
13.264094	674.366356	12.726695
13.014182	684.020690	12.731712
13.156531	672.574968	12.736730
13.194034	679.003616	12.741747
13.565090	679.002684	12.746765
13.503579	679.895891	12.751783
13.243908	682.366240	12.756800
13.404395	678.219959	12.761818
13.115412	682.496770	12.766835
13.491828	669.001277	12.771853
13.272924	677.514732	12.776871
13.661340	681.032846	12.781888
13.680379	675.472750	12.786906
13.485907	681.262199	12.791923
13.470554	675.922045	12.796941
13.340445	685.418876	12.801959
13.744361	701.298581	12.806976
13.610193	689.649757	12.811994
13.822824	691.008348	12.817011
13.755632	681.902056	12.822029
13.756313	685.931804	12.827047
13.690496	691.376189	12.832064
13.651440	689.652989	12.837082
13.445974	682.398526	12.842099
13.562128	676.775974	12.847117
13.682901	684.772660	12.852135
13.583104	682.134299	12.857152
13.581093	689.626260	12.862170
13.841497	697.541253	12.867187
13.855871	703.875684	12.872205
14.130997	697.941206	12.877223
13.999034	696.835207	12.882240
13.842225	682.621179	12.887258
13.629259	691.648094	12.892275
13.656412	682.037980	12.897293
13.698745	692.691351	12.902311
13.639841	686.660566	12.907328
13.758917	686.941854	12.912346
13.890294	698.294550	12.917363
13.853934	704.207706	12.922381
14.164040	704.143683	12.927399
13.857263	696.371676	12.932416
14.116573	694.513661	12.937434
13.876533	692.966914	12.942451
13.727734	681.743236	12.947469
14.161603	699.877751	12.952487
13.828773	698.074061	12.957504
14.324918	704.011602	12.962522
13.710661	692.172446	12.967539
13.690329	700.421474	12.972557
14.172193	702.451334	12.977575
13.711501	709.232106	12.982592
14.196666	708.506531	12.987610
13.871353	716.231870	12.992627
14.113583	708.803554	12.997645
14.224222	713.999574	13.002663
14.097324	705.540016	13.007680
14.225659	708.666300	13.012698
14.247513	705.166425	13.017715
14.298299	701.905035	13.022733
14.315866	697.367606	13.027751
14.413179	706.573428	13.032768
14.060196	710.042886	13.037786
14.267186	716.489338	13.042803
14.156271	707.250990	13.047821
14.218664	707.689422	13.052839
14.157892	718.851149	13.057856
13.970505	710.896451	13.062874
13.885495	706.239296	13.067891
14.117991	706.531327	13.072909
14.297197	705.105490	13.077927
14.078365	712.407164	13.082944
14.118932	698.395914	13.087962
14.497140	704.815704	13.092979
14.049329	707.832883	13.097997
14.090946	708.170411	13.103015
13.970109	707.027967	13.108032
14.380655	722.464861	13.113050
14.654394	731.053112	13.118067
14.175385	719.142390	13.123085
14.420288	721.534183	13.128103
14.225855	734.720599	13.133120
14.764594	731.941789	13.138138
14.548859	727.068305	13.143155
14.464525	729.602875	13.148173
14.868888	729.211762	13.153191
14.598626	721.888480	13.158208
14.618225	701.966716	13.163226
14.743503	704.159390	13.168243
14.814073	704.476632	13.173261
14.834288	700.197557	13.178279
14.761596	702.518880	13.183296
14.829863	704.452195	13.188314
14.872000	697.342206	13.193331
14.369913	699.544198	13.198349
14.753686	697.824589	13.203367
15.152873	705.437120	13.208384
14.853940	704.619040	13.213402
14.375852	710.301184	13.218419
14.356977	703.459458	13.223437
14.886191	699.012775	13.228455
14.458547	706.337490	13.233472
14.272510	704.867538	13.238490
14.724583	703.897816	13.243507
14.492278	706.957178	13.248525
14.447108	707.421824	13.253543
14.648201	730.149435	13.258560
14.678697	719.831904	13.263578
14.437413	726.326065	13.268595
14.874724	730.101655	13.273613
14.910406	735.688036	13.278631
14.527625	732.320581	13.283648
14.743980	723.883309	13.288666
14.825102	731.722092	13.293683
14.932776	728.963063	13.298701
15.221212	727.810542	13.303719
14.705944	737.575645	13.308736
15.020678	727.829216	13.313754
15.282062	721.612856	13.318771
15.037231	731.780804	13.323789
14.830179	730.260474	13.328807
14.835790	726.352884	13.333824
14.743272	725.603647	13.338842
15.013045	725.249267	13.343859
14.706194	734.499097	13.348877
15.387684	728.182614	13.353895
15.142798	735.469419	13.358912
15.108047	733.679274	13.363930
15.189435	732.013053	13.368947
14.875982	734.813664	13.373965
14.997572	733.273723	13.378983
14.975523	737.480585	13.384000
15.442675	742.453853	13.389018
15.358166	745.764755	13.394035
15.076005	739.383717	13.399053
14.991675	739.131806	13.404071
15.004733	753.866936	13.409088
15.302475	752.687719	13.414106
15.103082	752.721956	13.419123
15.158817	752.378811	13.424141
15.394816	759.123710	13.429159
15.724467	764.616994	13.434176
15.383967	757.856881	13.439194
15.467345	756.269241	13.444211
15.347658	751.330304	13.449229
15.632758	747.666362	13.454247
15.062435	745.997471	13.459264
15.405755	750.425151	13.464282
15.923140	746.144394	13.469299
15.328002	744.334204	13.474317
15.463844	738.642298	13.479335
15.390449	738.521223	13.484352
15.369796	746.984910	13.489370
15.492043	747.120543	13.494387
15.115689	752.045270	13.499405
15.541081	745.484640	13.504423
15.667847	754.954137	13.509440
15.623297	756.955515	13.514458
15.845258	755.677646	13.519475
15.568118	748.652060	13.524493
15.847642	749.732006	13.529511
15.438295	748.868001	13.534528
15.738193	744.873563	13.539546
16.024983	740.180600	13.544563
15.459081	736.289409	13.549581
15.787329	737.538487	13.554599
15.465568	734.098418	13.559616
15.596738	739.673088	13.564634
15.700661	740.572098	13.569651
15.576470	749.979683	13.574669
15.553216	747.196856	13.579687
15.534476	757.386419	13.584704
15.923730	749.196760	13.589722
16.209163	742.304485	13.594739
15.583394	743.440178	13.599757
16.023452	750.270063	13.604775
15.844498	743.816152	13.609792
15.846289	740.928444	13.614810
16.182546	746.240819	13.619827
15.565851	751.228211	13.624845
15.913514	743.982275	13.629863
16.011393	751.843704	13.634880
15.749658	748.182854	13.639898
16.054176	747.337086	13.644915
15.758518	758.122013	13.649933
15.904888	749.316940	13.654951
16.197066	752.218912	13.659968
15.932345	755.384311	13.664986
16.223171	753.941091	13.670003
15.690031	749.460991	13.675021
15.604605	747.555662	13.680039
15.845902	760.582740	13.685056
16.023837	750.807106	13.690074
16.123611	741.633764	13.695091
15.968832	750.913572	13.700109
16.088129	748.834362	13.705127
16.270011	748.039245	13.710144
16.139423	757.211152	13.715162
16.176991	758.385573	13.720179
15.983105	764.279096	13.725197
15.912306	760.247699	13.730215
16.403215	766.416443	13.735232
16.098188	771.585682	13.740250
16.480959	763.759932	13.745267
15.958725	781.469054	13.750285
16.122231	777.697809	13.755303
16.194419	772.217768	13.760320
15.900173	765.652415	13.765338
16.135833	762.396942	13.770355
16.330125	766.901476	13.775373
16.220325	774.867832	13.780391
16.323479	771.752905	13.785408
16.403061	777.332464	13.790426
16.483404	772.845200	13.795443
16.500650	769.377587	13.800461
16.422508	776.187182	13.805479
16.388935	760.720023	13.810496
16.447132	775.104171	13.815514
16.411763	774.977175	13.820531
16.341266	777.604270	13.825549
16.622217	771.776154	13.830567
16.353715	771.180543	13.835584
16.392675	782.386741	13.840602
17.010653	783.271986	13.845619
16.642493	782.054439	13.850637
16.666282	765.716837	13.855655
16.772894	762.733912	13.860672
16.739100	763.726947	13.865690
16.891477	762.134874	13.870707
16.645262	763.104179	13.875725
16.329312	762.992468	13.880743
16.243501	765.274817	13.885760
16.677086	775.015280	13.890778
16.905297	780.893581	13.895795
16.802681	784.103171	13.900813
16.658562	787.653729	13.905831
17.157669	786.187546	13.910848
16.600888	785.406452	13.915866
16.929958	783.095767	13.920883
16.817996	783.851672	13.925901
17.050667	785.721531	13.930919
17.045739	783.453382	13.935936
16.930959	788.350015	13.940954
17.079919	778.638836	13.945971
17.066809	767.529673	13.950989
16.721276	764.847512	13.956007
16.809051	768.993103	13.961024
16.944311	780.701842	13.966042
17.153813	776.790896	13.971059
17.137640	788.895591	13.976077
16.869316	791.360990	13.981095
17.194448	786.886102	13.986112
17.266074	786.802406	13.991130
17.046857	776.283888	13.996147
16.972881	782.452228	14.001165
17.021022	777.644939	14.006183
17.177247	783.951002	14.011200
16.974413	788.088196	14.016218
17.107925	788.338837	14.021235
16.944482	791.447450	14.026253
16.846619	790.064745	14.031271
17.241964	783.155341	14.036288
17.006304	787.363916	14.041306
17.089163	788.313543	14.046323
17.307426	790.804165	14.051341
17.253065	788.928708	14.056359
17.269414	788.108871	14.061376
17.386366	781.750881	14.066394
17.638427	786.495727	14.071411
17.306808	787.172227	14.076429
17.469184	780.321186	14.081447
17.471761	780.986676	14.086464
17.234624	794.558470	14.091482
17.500185	789.177700	14.096499
17.783611	782.888462	14.101517
17.586844	788.346953	14.106535
17.397606	786.009673	14.111552
17.481727	783.579340	14.116570
17.508952	787.923705	14.121587
17.331076	782.728739	14.126605
17.386819	786.857231	14.131623
17.657911	784.514549	14.136640
17.403613	787.122926	14.141658
17.028634	793.773623	14.146675
17.421093	790.288611	14.151693
17.146373	792.941193	14.156711
17.927207	805.196355	14.161728
17.810737	820.519736	14.166746
17.667832	816.300743	14.171763
17.705025	797.076702	14.176781
17.591356	793.342298	14.181799
17.750624	787.795047	14.186816
17.881860	800.716217	14.191834
17.955560	797.340792	14.196851
17.646748	788.928452	14.201869
17.692689	784.891497	14.206887
18.268406	780.163006	14.211904
17.575424	788.185455	14.216922
17.605825	790.449714	14.221939
17.772346	785.990053	14.226957
17.989670	803.391552	14.231975
18.260530	799.590965	14.236992
17.678539	795.181573	14.242010
17.519215	796.673822	14.247027
18.025406	813.298230	14.252045
17.759673	809.937782	14.257063
17.875614	805.388165	14.262080
17.983845	813.266944	14.267098
17.868026	808.276897	14.272115
18.111129	805.307428	14.277133
18.091250	809.444543	14.282151
18.208508	801.619093	14.287168
17.904136	809.959731	14.292186
18.166499	803.074179	14.297203
18.085758	806.750569	14.302221
17.718525	805.384557	14.307239
17.974648	803.075760	14.312256
17.795047	808.591544	14.317274
18.218450	813.284474	14.322291
17.951038	817.554803	14.327309
17.732351	820.498457	14.332327
18.331904	823.425166	14.337344
18.481643	834.800336	14.342362
18.561061	820.416878	14.347379
18.260828	813.855595	14.352397
18.047228	814.529499	14.357415
18.524318	817.371135	14.362432
18.556433	826.034920	14.367450
18.470332	812.021213	14.372467
18.788473	807.648390	14.377485
18.258079	811.120244	14.382503
18.335509	788.750013	14.387520
18.173355	804.228811	14.392538
18.563879	812.947237	14.397555
18.815114	823.621808	14.402573
18.649703	814.855779	14.407591
18.557688	799.852107	14.412608
18.000763	805.761144	14.417626
18.231262	813.472568	14.422643
18.681529	818.483199	14.427661
18.379329	829.313367	14.432679
18.911300	821.511698	14.437696
18.701809	823.576633	14.442714
18.838579	817.101939	14.447731
18.821417	816.019083	14.452749
18.541809	832.929953	14.457767
18.985892	813.781394	14.462784
18.845440	815.122388	14.467802
18.899141	810.304757	14.472819
18.913283	799.159774	14.477837
18.616068	792.329794	14.482855
18.634442	791.093088	14.487872
18.386507	800.624104	14.492890
18.729298	807.191453	14.497907
19.108254	810.423896	14.502925
18.797970	822.041091	14.507943
18.870072	813.102387	14.512960
19.220320	821.205413	14.517978
19.613624	798.735498	14.522995
19.131197	791.284278	14.528013
18.973068	799.352841	14.533031
19.058972	786.524166	14.538048
18.767649	789.696869	14.543066
18.594635	789.941588	14.548083
18.732146	798.005144	14.553101
18.495755	808.799807	14.558119
18.916147	816.955024	14.563136
19.048756	815.170370	14.568154
18.755268	817.545020	14.573171
18.955405	810.580794	14.578189
18.818191	809.715439	14.583207
19.219035	811.041580	14.588224
19.064598	816.212632	14.593242
18.747182	818.168141	14.598259
18.856911	820.704067	14.603277
19.253690	843.830533	14.608295
19.170113	829.040112	14.613312
19.179341	843.103745	14.618330
19.441461	845.893651	14.623347
19.629595	846.915251	14.628365
19.380222	847.784069	14.633383
19.463642	834.583372	14.638400
19.405142	848.673332	14.643418
19.507094	838.994685	14.648435
19.684065	827.095362	14.653453
19.515343	826.872367	14.658471
19.586195	818.725940	14.663488
19.187987	823.553106	14.668506
19.133710	820.866613	14.673523
19.397598	828.023751	14.678541
19.585322	838.623015	14.683559
19.369895	836.965128	14.688576
19.451083	832.714397	14.693594
19.434554	840.404336	14.698611
20.026952	835.007377	14.703629
19.774931	844.804133	14.708647
20.142150	833.919728	14.713664
19.664768	823.425598	14.718682
19.578786	823.057181	14.723699
19.730528	826.798361	14.728717
19.790893	832.576584	14.733735
19.759841	832.571988	14.738752
19.475918	831.622181	14.743770
19.697020	842.326700	14.748787
19.528902	838.758550	14.753805
19.459097	840.214774	14.758823
19.588010	838.345489	14.763840
19.776414	829.215105	14.768858
19.408119	845.773732	14.773875
19.615616	841.178294	14.778893
19.470847	843.460365	14.783911
19.708112	850.675304	14.788928
19.501060	854.055798	14.793946
19.917631	859.390416	14.798963
20.274710	854.475046	14.803981
20.287189	861.182204	14.808999
20.429023	856.757927	14.814016
20.338282	851.593555	14.819034
20.239761	836.357342	14.824051
20.450895	829.830042	14.829069
20.163664	831.436879	14.834087
20.138322	830.478369	14.839104
20.289394	825.733934	14.844122
20.035898	823.100548	14.849139
20.600000	828.800340	14.854157
20.112063	834.499834	14.859175
20.234886	824.092130	14.864192
20.092443	828.772182	14.869210
19.966247	835.560880	14.874227
20.411209	826.838663	14.879245
19.687644	837.481984	14.884263
20.087579	840.629118	14.889280
20.352031	849.436617	14.894298
20.174597	845.488073	14.899315
20.448822	840.733927	14.904333
20.500927	846.156843	14.909351
20.393608	844.030857	14.914368
20.382207	848.513790	14.919386
20.110574	855.880547	14.924403
20.356001	843.781211	14.929421
20.496651	854.753877	14.934439
20.398873	853.197589	14.939456
20.532553	854.827254	14.944474
20.334608	859.645340	14.949491
20.344797	858.116422	14.954509
20.244367	850.757177	14.959527
20.117889	849.779698	14.964544
20.192474	854.889857	14.969562
20.751689	873.140729	14.974579
20.871396	869.606652	14.979597
20.758312	878.368808	14.984615
21.031151	881.087625	14.989632
21.076353	865.712248	14.994650
20.911482	860.988593	14.999667
21.189236	850.244336	15.004685
20.916677	851.769998	15.009703
20.889792	844.926310	15.014720
20.871911	839.725351	15.019738
20.657669	857.699011	15.024755
21.086556	848.871992	15.029773
20.710691	860.272211	15.034791
20.758404	853.334856	15.039808
20.919827	853.521193	15.044826
20.854309	846.402660	15.049843
20.560985	857.203062	15.054861
20.844349	868.349171	15.059879
20.706479	872.851801	15.064896
21.173802	874.735627	15.069914
20.826867	876.979754	15.074931
21.127588	877.977515	15.079949
20.915597	877.562445	15.084967
21.114338	880.441118	15.089984
21.116253	871.749991	15.095002
20.929369	888.195208	15.100019
21.390172	878.555340	15.105037
21.136042	881.886366	15.110055
21.165296	880.890950	15.115072
21.340350	877.742720	15.120090
21.198154	878.935671	15.125107
21.020754	876.839526	15.130125
21.254414	885.714952	15.135143
21.381019	876.288060	15.140160
21.252402	876.383859	15.145178
21.028281	876.945798	15.150195
21.380898	882.239888	15.155213
21.814570	884.782189	15.160231
21.338760	879.037150	15.165248
21.469327	874.504173	15.170266
21.394181	881.086129	15.175283
21.479090	883.493388	15.180301
21.375966	881.092195	15.185319
21.417836	894.383945	15.190336
21.855667	893.094547	15.195354
21.756878	902.744404	15.200371
21.771622	884.628270	15.205389
21.948632	886.326929	15.210407
21.426798	879.923198	15.215424
21.510079	874.264677	15.220442
21.430078	881.156650	15.225459
21.646528	883.865313	15.230477
21.867077	890.126685	15.235495
21.440551	904.797842	15.240512
21.859623	901.933499	15.245530
21.764003	902.254530	15.250547
22.088251	897.214876	15.255565
21.864278	903.245670	15.260583
21.932089	906.097396	15.265600
22.099254	896.083524	15.270618
22.251257	903.365407	15.275635
22.168341	891.736872	15.280653
21.856570	879.402381	15.285671
21.612583	879.105900	15.290688
21.828519	885.194424	15.295706
21.651853	898.719013	15.300723
21.879676	892.993802	15.305741
22.279055	895.980090	15.310759
22.013163	888.656058	15.315776
22.317508	893.730455	15.320794
22.170248	907.613382	15.325811
22.260786	898.334101	15.330829
22.235252	897.972050	15.335847
22.232963	897.262405	15.340864
22.149671	888.521422	15.345882
21.977407	901.357379	15.350899
22.262310	891.271532	15.355917
22.154070	898.461391	15.360935
22.141070	904.219502	15.365952
21.986862	898.462253	15.370970
22.052553	895.940103	15.375987
22.100593	887.279656	15.381005
21.932018	892.525513	15.386023
22.215454	913.785748	15.391040
22.509900	913.238180	15.396058
22.406664	921.954644	15.401075
22.651675	918.385269	15.406093
22.971021	925.287664	15.411111
22.922509	916.197278	15.416128
22.521560	901.071212	15.421146
22.168369	903.218488	15.426163
22.642651	910.630073	15.431181
22.836783	906.497436	15.436199
22.455425	898.970476	15.441216
22.783951	894.990481	15.446234
22.775043	906.235767	15.451251
22.623265	901.598424	15.456269
22.835422	914.604906	15.461287
22.653948	913.178406	15.466304
22.788268	905.839391	15.471322
22.687736	920.043248	15.476339
23.053586	908.489994	15.481357
23.008805	911.375030	15.486375
22.670060	903.854056	15.491392
22.792954	901.638572	15.496410
22.578777	908.583004	15.501427
22.872421	916.691731	15.506445
23.078613	909.158492	15.511463
22.785446	921.988043	15.516480
23.002539	917.646705	15.521498
22.605180	912.003047	15.526515
23.041315	917.741726	15.531533
22.823798	916.838377	15.536551
23.015140	921.703164	15.541568
23.153717	919.097080	15.546586
23.224926	907.889496	15.551603
23.147274	913.288456	15.556621
23.247362	911.398406	15.561639
22.975363	916.070250	15.566656
22.991634	906.436464	15.571674
23.222620	913.614537	15.576691
23.201004	916.738958	15.581709
23.178307	917.111750	15.586727
23.026982	910.072822	15.591744
22.931672	910.198149	15.596762
23.006137	920.250220	15.601779
23.245421	921.727753	15.606797
23.668662	931.040733	15.611815
23.556119	935.085010	15.616832
23.373007	922.193983	15.621850
23.717389	931.790635	15.626867
23.647977	933.524510	15.631885
23.641307	929.186451	15.636903
23.786071	937.917957	15.641920
23.811236	920.750040	15.646938
23.824641	908.945555	15.651955
23.485284	907.344826	15.656973
23.629477	898.205511	15.661991
23.355120	905.670539	15.667008
23.916215	915.268154	15.672026
23.632931	922.854497	15.677043
23.529751	926.758462	15.682061
23.670487	923.678682	15.687079
23.767565	932.509126	15.692096
23.647856	935.506815	15.697114
23.505856	930.110565	15.702131
23.691489	926.313754	15.707149
23.939142	924.940358	15.712167
23.791206	935.686612	15.717184
23.946679	928.767163	15.722202
24.169686	924.563755	15.727219
24.239181	930.457350	15.732237
23.819901	932.119469	15.737255
23.503017	935.132079	15.742272
24.085407	924.144691	15.747290
24.255494	926.876357	15.752307
24.439831	932.294491	15.757325
24.315994	926.030743	15.762343
24.149161	931.421503	15.767360
24.106687	932.254956	15.772378
24.070594	932.503604	15.777395
23.783003	933.539319	15.782413
24.085363	929.771669	15.787431
23.930687	931.354721	15.792448
24.204050	928.547774	15.797466
23.954171	929.991018	15.802483
23.959384	931.792168	15.807501
24.315534	942.848098	15.812519
24.059746	954.614681	15.817536
24.098152	960.096569	15.822554
24.135643	953.949701	15.827571
24.727779	944.620701	15.832589
24.694417	940.902164	15.837607
24.576202	948.387080	15.842624
24.657537	947.049044	15.847642
24.841669	945.830700	15.852659
24.736884	949.526641	15.857677
24.829773	960.967547	15.862695
24.413278	957.914560	15.867712
24.500876	949.389933	15.872730
24.660545	939.847409	15.877747
24.739919	947.560331	15.882765
24.745127	939.758576	15.887783
24.803689	942.737978	15.892800
24.708523	937.236606	15.897818
25.030523	942.043186	15.902835
24.967573	945.164581	15.907853
24.893870	935.614214	15.912871
24.749794	929.666033	15.917888
24.881761	939.213712	15.922906
24.917891	944.547629	15.927923
24.667945	938.432897	15.932941
25.031181	944.934000	15.937959
25.187311	942.255754	15.942976
25.241755	941.082847	15.947994
24.804073	927.423584	15.953011
24.680131	942.517864	15.958029
25.045678	936.919515	15.963047
24.812941	947.653735	15.968064
24.638076	941.549401	15.973082
24.905061	948.081270	15.978099
24.739093	949.176942	15.983117
25.180695	941.427161	15.988135
25.108623	950.829892	15.993152
24.895494	948.837129	15.998170
25.338197	962.170661	16.003187
25.367259	970.535198	16.008205
25.342039	959.503538	16.013223
25.499593	959.106667	16.018240
25.129012	961.417601	16.023258
25.419265	958.156748	16.028275
25.490617	973.368968	16.033293
25.586837	959.778028	16.038311
25.384509	960.320797	16.043328
25.607558	960.308197	16.048346
25.634279	961.178214	16.053363
25.542968	960.567631	16.058381
25.683520	953.158200	16.063399
25.231633	957.226915	16.068416
25.615937	955.131667	16.073434
25.883834	952.152001	16.078451
25.636752	955.687066	16.083469
25.589712	956.252993	16.088487
25.629693	960.081028	16.093504
25.786776	954.218492	16.098522
25.542922	950.229774	16.103539
25.643077	958.034137	16.108557
25.536691	953.396024	16.113575
25.482547	957.702607	16.118592
25.354463	967.622143	16.123610
25.452380	951.919754	16.128627
25.512641	972.649931	16.133645
25.911767	972.953892	16.138663
25.840566	971.002144	16.143680
26.372638	976.069510	16.148698
26.205498	972.242410	16.153715
26.251518	965.702898	16.158733
26.056511	967.623586	16.163751
26.305766	972.236378	16.168768
26.089692	974.207682	16.173786
26.638140	970.023020	16.178803
25.952337	964.055033	16.183821
26.216490	961.729187	16.188839
26.351746	977.303838	16.193856
26.267197	955.905340	16.198874
26.330562	951.417519	16.203891
26.119465	954.757636	16.208909
26.045823	964.308940	16.213927
26.448012	978.781703	16.218944
26.522113	981.020247	16.223962
26.723130	967.823232	16.228979
26.426928	965.991721	16.233997
26.467659	957.853075	16.239015
26.451989	958.909569	16.244032
26.144955	966.780489	16.249050
26.164698	976.692793	16.254067
26.222284	978.634113	16.259085
26.672294	972.233667	16.264103
26.617899	977.042056	16.269120
26.694492	976.859758	16.274138
26.949276	975.116026	16.279155
26.610989	973.073321	16.284173
26.736914	981.249215	16.289191
26.907917	979.591109	16.294208
26.739309	985.108391	16.299226
26.898155	981.060124	16.304243
26.534965	980.974700	16.309261
26.625035	977.549356	16.314279
26.767938	973.771810	16.319296
26.762251	983.060084	16.324314
26.917203	978.043610	16.329331
26.824147	981.134985	16.334349
26.507719	983.866671	16.339367
26.745753	974.608567	16.344384
26.711500	996.596849	16.349402
27.243164	991.591146	16.354419
27.090329	995.468144	16.359437
27.004634	995.585663	16.364455
26.930424	1004.351295	16.369472
27.117727	1002.990445	16.374490
27.374713	987.657727	16.379507
27.434710	996.314099	16.384525
27.119152	997.944296	16.389543
27.388638	992.433468	16.394560
27.308271	994.926434	16.399578
27.635754	998.387829	16.404595
27.319682	998.695849	16.409613
27.149226	998.296399	16.414631
27.258390	991.289464	16.419648
27.155743	996.260003	16.424666
27.425824	982.509435	16.429683
27.268880	999.729562	16.434701
27.235530	990.860835	16.439719
27.517417	994.512361	16.444736
27.107841	999.398148	16.449754
27.581296	1003.575261	16.454771
27.732721	1024.196632	16.459789
27.982102	1022.153940	16.464807
27.857452	1009.181165	16.469824
27.511552	1008.689113	16.474842
27.845089	1004.102410	16.479859
27.770406	1016.162722	16.484877
27.714880	1017.465262	16.489895
27.762170	1014.794484	16.494912
27.936616	1016.932205	16.499930
27.905744	1015.709462	16.504947
28.287214	1013.097105	16.509965
28.184178	1001.541058	16.514983
27.658983	997.551953	16.520000
27.842036	1010.247462	16.525018
28.069145	1003.187445	16.530035
28.118386	1003.022028	16.535053
28.425002	1003.788509	16.540071
28.052338	994.019575	16.545088
28.013402	990.339764	16.550106
28.356803	992.302856	16.555123
28.225356	997.407266	16.560141
27.893956	993.548932	16.565159
27.794084	991.260825	16.570176
28.132744	1009.113840	16.575194
28.283757	1010.908076	16.580211
28.075682	1013.752282	16.585229
27.756114	1012.293627	16.590247
28.137947	1001.050244	16.595264
28.184110	1013.022312	16.600282
28.546761	1008.102878	16.605299
28.422715	1008.658706	16.610317
28.267513	1012.782225	16.615335
28.339109	1019.177286	16.620352
28.598035	1029.661439	16.625370
28.854096	1027.718690	16.630387
28.623418	1016.381318	16.635405
28.747245	1018.930857	16.640423
28.620600	1016.353430	16.645440
28.495120	1017.000998	16.650458
28.756415	1019.970938	16.655475
28.748485	1029.474176	16.660493
29.057122	1029.404070	16.665511
28.882259	1015.170496	16.670528
28.558090	1018.638682	16.675546
28.946838	1026.038387	16.680563
28.941786	1030.640296	16.685581
28.740791	1032.142208	16.690599
28.906082	1027.597474	16.695616
28.559990	1037.740336	16.700634
28.816341	1028.381524	16.705651
28.922199	1030.125989	16.710669
29.146025	1032.199220	16.715687
28.942325	1034.837624	16.720704
28.934712	1032.598262	16.725722
29.182433	1030.031973	16.730739
29.309047	1033.843380	16.735757
29.207267	1039.640604	16.740775
29.038557	1031.045392	16.745792
28.983833	1037.580046	16.750810
29.235040	1032.100453	16.755827
29.444190	1032.765348	16.760845
29.110967	1036.821917	16.765863
29.052855	1036.032597	16.770880
29.370364	1044.068240	16.775898
29.460580	1048.898314	16.780915
29.981231	1042.647788	16.785933
29.537376	1042.167831	16.790951
29.453288	1021.980990	16.795968
29.188014	1028.778792	16.800986
29.627820	1039.809136	16.806003
29.571316	1045.630869	16.811021
29.453414	1041.802399	16.816039
29.557911	1045.841311	16.821056
29.958184	1041.304168	16.826074
29.833688	1042.118839	16.831091
30.246179	1041.344608	16.836109
29.728065	1039.418254	16.841127
30.192334	1041.258393	16.846144
29.727092	1042.962392	16.851162
30.215367	1039.730653	16.856179
29.787863	1025.343905	16.861197
29.731817	1023.841064	16.866215
30.178725	1036.050550	16.871232
30.028344	1038.005322	16.876250
29.613899	1031.042025	16.881267
29.506783	1033.412931	16.886285
29.973671	1040.055719	16.891303
30.027376	1034.808844	16.896320
29.860927	1050.528362	16.901338
30.285953	1038.997368	16.906355
30.317665	1038.216153	16.911373
29.730056	1041.551793	16.916391
30.606832	1035.914842	16.921408
30.257139	1049.835708	16.926426
30.215477	1043.915725	16.931443
30.207591	1040.085904	16.936461
30.102650	1034.901599	16.941479
30.341347	1035.006481	16.946496
29.931079	1046.819267	16.951514
30.481505	1045.963601	16.956531
30.734718	1053.993481	16.961549
29.751938	1054.487354	16.966567
30.352911	1060.844190	16.971584
30.806632	1059.429232	16.976602
30.718637	1067.136707	16.981619
30.699358	1063.662100	16.986637
30.588664	1061.224193	16.991655
30.954173	1058.715299	16.996672
30.972266	1063.383040	17.001690
30.411858	1063.580782	17.006707
30.941597	1061.377672	17.011725
30.665877	1065.778739	17.016743
30.717655	1057.123939	17.021760
31.128743	1069.200172	17.026778
30.936877	1066.538220	17.031795
31.159808	1066.774943	17.036813
31.149399	1061.582223	17.041831
31.285448	1060.838410	17.046848
31.101475	1057.556702	17.051866
30.719778	1061.355740	17.056883
30.679918	1054.611819	17.061901
30.576729	1067.711693	17.066919
31.158535	1061.991273	17.071936
30.694191	1061.681760	17.076954
30.787716	1066.517636	17.081971
31.171200	1073.987607	17.086989
31.043092	1081.382602	17.092007
31.302299	1084.049925	17.097024
31.303656	1091.427923	17.102042
31.255919	1081.636752	17.107059
31.551663	1078.734779	17.112077
31.527479	1084.857603	17.117095
31.821254	1081.195398	17.122112
31.839143	1082.211961	17.127130
31.932182	1079.688682	17.132147
32.082438	1068.904185	17.137165
31.634795	1063.599662	17.142183
31.757641	1059.355013	17.147200
31.560602	1050.161453	17.152218
31.481413	1047.945857	17.157235
31.819712	1074.224862	17.162253
31.667167	1077.514861	17.167271
31.935231	1067.810227	17.172288
31.747708	1065.431617	17.177306
32.072353	1073.945838	17.182323
32.221471	1070.350339	17.187341
31.542266	1066.312614	17.192359
31.851443	1060.685134	17.197376
31.878545	1070.192407	17.202394
32.324841	1073.168265	17.207411
32.354383	1063.270400	17.212429
31.679049	1072.852327	17.217447
32.046354	1069.532121	17.222464
31.928922	1068.818306	17.227482
31.957657	1079.546608	17.232499
32.034754	1076.864869	17.237517
32.038074	1076.043891	17.242535
31.940930	1080.685398	17.247552
31.907510	1085.411658	17.252570
31.906791	1077.288878	17.257587
32.401068	1072.102784	17.262605
31.860778	1079.053876	17.267623
32.408735	1091.052009	17.272640
32.121634	1096.209083	17.277658
32.196079	1106.734628	17.282675
32.647244	1100.614819	17.287693
32.251843	1101.695731	17.292711
32.423512	1096.790228	17.297728
32.496961	1104.822873	17.302746
32.452866	1103.984031	17.307763
32.730247	1097.862879	17.312781
32.605580	1098.589218	17.317799
32.518407	1097.599294	17.322816
32.836722	1102.539035	17.327834
32.462442	1101.325573	17.332851
32.524703	1098.835485	17.337869
32.393194	1126.061861	17.342887
32.720574	1115.861976	17.347904
32.427612	1117.570716	17.352922
32.612283	1135.798124	17.357939
33.191597	1122.043483	17.362957
33.224422	1120.318516	17.367975
33.162333	1125.986513	17.372992
32.923573	1123.325542	17.378010
33.258653	1117.596183	17.383027
33.785871	1120.663591	17.388045
33.395995	1116.457732	17.393063
33.499170	1117.590405	17.398080
33.414919	1122.719059	17.403098
33.138274	1125.330964	17.408115
33.375602	1116.006626	17.413133
33.197970	1126.315812	17.418151
33.491212	1120.091198	17.423168
33.676262	1118.336219	17.428186
33.426188	1119.290364	17.433203
33.145000	1116.677025	17.438221
33.188592	1114.353942	17.443239
33.543565	1113.484524	17.448256
33.690084	1111.031809	17.453274
33.360786	1115.980866	17.458291
33.384978	1117.637070	17.463309
33.634060	1129.025364	17.468327
33.965785	1139.192137	17.473344
34.020601	1130.016127	17.478362
33.727607	1131.358804	17.483379
33.724935	1126.713964	17.488397
33.794225	1136.656512	17.493415
33.810635	1147.468824	17.498432
34.039699	1142.923598	17.503450
34.299145	1141.273797	17.508467
34.112468	1132.072270	17.513485
33.733607	1123.351944	17.518503
33.820676	1130.208534	17.523520
34.208674	1139.984699	17.528538
34.221441	1136.934273	17.533555
34.371899	1131.088489	17.538573
34.374345	1135.007612	17.543591
34.049580	1142.423783	17.548608
34.157706	1136.007082	17.553626
34.230878	1140.322289	17.558643
34.222662	1134.801006	17.563661
34.005336	1143.532185	17.568679
34.049800	1134.979471	17.573696
34.275047	1131.018661	17.578714
34.130565	1135.055333	17.583731
34.174812	1128.860016	17.588749
34.297281	1135.625891	17.593767
34.174129	1147.845316	17.598784
34.604742	1148.873362	17.603802
34.396531	1159.667005	17.608819
34.707627	1152.988324	17.613837
35.055556	1154.679334	17.618855
35.083152	1160.421740	17.623872
35.372738	1154.039895	17.628890
34.853474	1150.968161	17.633907
34.782770	1135.837813	17.638925
34.734008	1133.008405	17.643943
35.071877	1137.941955	17.648960
35.073237	1134.845969	17.653978
34.603063	1145.749818	17.658995
34.692390	1138.903702	17.664013
34.758935	1150.920026	17.669031
34.835307	1149.690044	17.674048
35.343491	1150.030677	17.679066
34.827437	1151.859360	17.684083
34.726190	1146.759653	17.689101
35.082681	1156.960450	17.694119
34.843764	1155.037950	17.699136
35.406958	1159.863841	17.704154
35.086275	1167.232051	17.709171
35.701347	1174.691254	17.714189
35.991090	1158.169873	17.719207
35.909301	1145.767831	17.724224
35.865294	1143.897036	17.729242
35.885644	1145.332937	17.734259
36.056927	1140.780929	17.739277
35.621077	1144.556858	17.744295
35.920763	1145.961891	17.749312
35.966133	1132.179923	17.754330
35.732850	1137.571624	17.759347
35.818849	1131.615956	17.764365
35.733775	1130.698287	17.769383
35.313278	1140.726561	17.774400
35.528569	1138.095879	17.779418
35.633917	1152.188972	17.784435
35.900392	1148.663547	17.789453
35.803164	1148.341054	17.794471
35.577949	1150.414786	17.799488
35.934367	1136.410818	17.804506
35.791557	1138.597949	17.809523
35.768631	1143.698127	17.814541
35.913848	1143.423093	17.819559
35.801467	1151.831827	17.824576
35.994314	1157.343378	17.829594
35.809331	1164.191846	17.834611
36.141285	1162.372965	17.839629
36.134796	1165.362533	17.844647
36.009865	1153.794016	17.849664
36.064055	1162.533423	17.854682
36.338643	1173.119363	17.859699
36.584335	1175.485849	17.864717
36.325598	1179.231054	17.869735
36.583127	1183.132563	17.874752
36.560224	1175.795826	17.879770
36.555563	1189.442177	17.884787
36.775988	1183.594949	17.889805
36.642126	1188.819708	17.894823
36.567407	1182.999498	17.899840
36.809286	1182.737816	17.904858
36.779795	1190.928537	17.909875
36.625760	1178.603993	17.914893
36.660057	1184.405323	17.919911
36.784535	1187.371347	17.924928
36.912720	1178.650944	17.929946
36.727140	1184.981965	17.934963
36.810739	1181.690132	17.939981
36.700375	1181.148780	17.944999
36.715475	1185.394144	17.950016
36.665776	1182.728975	17.955034
36.479236	1189.271584	17.960051
36.932277	1204.415107	17.965069
37.389281	1207.360920	17.970087
37.160236	1215.809938	17.975104
37.463345	1202.256029	17.980122
37.412572	1210.282817	17.985139
37.461406	1210.723372	17.990157
37.860939	1211.544823	17.995175
37.577039	1201.951301	18.000192
37.299926	1185.619136	18.005210
37.217307	1183.422991	18.010227
37.360772	1200.754329	18.015245
37.644055	1203.780837	18.020263
37.467650	1206.074192	18.025280
38.150659	1204.358438	18.030298
38.005924	1200.777106	18.035315
37.532092	1203.173573	18.040333
37.652625	1205.057781	18.045351
37.431603	1208.569904	18.050368
37.705243	1205.459915	18.055386
37.965610	1207.959820	18.060403
37.803140	1202.036502	18.065421
38.102985	1198.430133	18.070439
37.759307	1200.935722	18.075456
37.866055	1203.046136	18.080474
37.761863	1202.762596	18.085491
37.841273	1201.655213	18.090509
37.911643	1203.458869	18.095527
37.951867	1209.155144	18.100544
38.472953	1219.387154	18.105562
38.268746	1230.069765	18.110579
38.299744	1234.135942	18.115597
38.393678	1222.994049	18.120615
38.379632	1221.229033	18.125632
38.687829	1218.012677	18.130650
38.176301	1218.461583	18.135667
38.172360	1217.423981	18.140685
38.533866	1212.053392	18.145703
38.402159	1220.869108	18.150720
38.679646	1224.808544	18.155738
38.565896	1228.900412	18.160755
38.584180	1218.234201	18.165773
38.862365	1220.564077	18.170791
38.832079	1215.816217	18.175808
39.114201	1220.102067	18.180826
38.842031	1218.875854	18.185843
38.835841	1221.480378	18.190861
39.194082	1214.737530	18.195879
39.124291	1219.141286	18.200896
39.432430	1217.322952	18.205914
39.145772	1207.900268	18.210931
39.164181	1195.274309	18.215949
39.108860	1184.411297	18.220967
38.741476	1189.675571	18.225984
39.000903	1199.613796	18.231002
39.118983	1209.182717	18.236019
38.891030	1213.734173	18.241037
39.435655	1214.277416	18.246055
39.059325	1219.060256	18.251072
39.068912	1214.678571	18.256090
39.477087	1213.176019	18.261107
39.195044	1216.527232	18.266125
39.272701	1203.330314	18.271143
39.054938	1222.324208	18.276160
38.919260	1217.718988	18.281178
39.132919	1223.486093	18.286195
39.370897	1228.255342	18.291213
39.727740	1227.944201	18.296231
39.245734	1224.248120	18.301248
39.626262	1222.282816	18.306266
39.672617	1222.982532	18.311283
39.663543	1232.208347	18.316301
39.510307	1227.255566	18.321319
39.673037	1248.787460	18.326336
40.006737	1242.635399	18.331354
39.845616	1254.946015	18.336371
39.963536	1250.310770	18.341389
40.306829	1241.209708	18.346407
40.092146	1246.563832	18.351424
40.190156	1249.915838	18.356442
40.518810	1251.934904	18.361459
40.229919	1254.450905	18.366477
40.249293	1248.868487	18.371495
40.316081	1255.273850	18.376512
40.358242	1248.980987	18.381530
40.255726	1249.830114	18.386547
40.338215	1246.197616	18.391565
40.692831	1247.565703	18.396583
40.214095	1247.151130	18.401600
40.620858	1242.710755	18.406618
40.660111	1248.214690	18.411635
40.667037	1243.814478	18.416653
40.401481	1242.388419	18.421671
40.278196	1247.602081	18.426688
40.212865	1242.657700	18.431706
40.501990	1251.953861	18.436723
40.383038	1263.670941	18.441741
40.978158	1260.009119	18.446759
40.889312	1270.263539	18.451776
40.692833	1269.757682	18.456794
40.907121	1263.163461	18.461811
41.101354	1272.108335	18.466829
41.335713	1270.235211	18.471847
40.808926	1273.204819	18.476864
40.716355	1277.877223	18.481882
40.962810	1271.464182	18.486899
40.856267	1274.598733	18.491917
41.118885	1272.393006	18.496935
40.941862	1293.005867	18.501952
41.057447	1290.690487	18.506970
41.271702	1296.340759	18.511987
41.395137	1293.279388	18.517005
41.462552	1286.682779	18.522023
41.320485	1294.209423	18.527040
41.549874	1283.904779	18.532058
41.857493	1279.075890	18.537075
41.443460	1287.900882	18.542093
41.853799	1280.585010	18.547111
41.756146	1283.885436	18.552128
41.349162	1289.720792	18.557146
41.330405	1277.081628	18.562163
41.735466	1299.121806	18.567181
41.670695	1300.321664	18.572199
41.635859	1310.012277	18.577216
42.188644	1304.293144	18.582234
41.966887	1308.408158	18.587251
42.131206	1307.540013	18.592269
42.279662	1304.215968	18.597287
42.204471	1303.609176	18.602304
41.822324	1311.255257	18.607322
42.168792	1297.946989	18.612339
41.867443	1301.234951	18.617357
42.332512	1296.832822	18.622375
42.016135	1294.499490	18.627392
42.143100	1304.461553	18.632410
42.275340	1298.533344	18.637427
42.331674	1304.271322	18.642445
42.513503	1301.497503	18.647463
42.630192	1314.493896	18.652480
42.731636	1309.485661	18.657498
42.690106	1301.160850	18.662515
42.822051	1300.521807	18.667533
42.834078	1295.748403	18.672551
42.669402	1297.219436	18.677568
42.629495	1298.251321	18.682586
42.940395	1303.100754	18.687603
43.020144	1318.409792	18.692621
42.969246	1316.644193	18.697639
43.138330	1316.501140	18.702656
43.373842	1312.327252	18.707674
43.453886	1298.845869	18.712691
43.152022	1295.254269	18.717709
43.531435	1288.056817	18.722727
43.584556	1285.694359	18.727744
42.762210	1284.361298	18.732762
42.973513	1286.944592	18.737779
42.997828	1295.407850	18.742797
43.217704	1304.560187	18.747815
43.306761	1317.276863	18.752832
43.477615	1315.943796	18.757850
43.349317	1317.295558	18.762867
43.287803	1319.668869	18.767885
43.503615	1316.867666	18.772903
43.535474	1316.010676	18.777920
43.434710	1318.693055	18.782938
43.549500	1309.425564	18.787955
43.166134	1322.496664	18.792973
43.944561	1336.788065	18.797991
44.141527	1334.933380	18.803008
43.734491	1332.102917	18.808026
43.942414	1321.154654	18.813043
43.715901	1341.614330	18.818061
44.001367	1334.952195	18.823079
44.076782	1340.557826	18.828096
44.066648	1340.366937	18.833114
44.500100	1329.992625	18.838131
43.866207	1347.404112	18.843149
44.305842	1337.054080	18.848167
44.262200	1338.291677	18.853184
44.402846	1336.278502	18.858202
44.463165	1327.638020	18.863219
44.346236	1336.372598	18.868237
44.402840	1324.053026	18.873255
44.398066	1323.611994	18.878272
44.130944	1333.638588	18.883290
44.273709	1338.495273	18.888307
44.477880	1345.305312	18.893325
44.597214	1338.059971	18.898343
44.362475	1343.565570	18.903360
44.892973	1359.789075	18.908378
45.425528	1346.265605	18.913395
45.473344	1335.074018	18.918413
45.376438	1324.271043	18.923431
45.278943	1328.530817	18.928448
44.867392	1320.626526	18.933466
45.074367	1316.062605	18.938483
45.172969	1333.404213	18.943501
45.441306	1323.402751	18.948519
45.118064	1315.560452	18.953536
45.113255	1323.094140	18.958554
45.717510	1314.438404	18.963571
45.635396	1323.827117	18.968589
45.314070	1325.824315	18.973607
45.469139	1324.234930	18.978624
45.217382	1321.045777	18.983642
45.478475	1323.611857	18.988659
45.301254	1323.462762	18.993677
45.133519	1328.484553	18.998695
44.978336	1327.628282	19.003712
44.781904	1330.439167	19.008730
45.421308	1329.247744	19.013747
45.438235	1346.078217	19.018765
45.565297	1350.082127	19.023783
45.736919	1356.404932	19.028800
45.748765	1346.225641	19.033818
46.080927	1343.810262	19.038835
45.397097	1349.351070	19.043853
45.748286	1358.019086	19.048871
45.983356	1363.921759	19.053888
45.692976	1376.236805	19.058906
45.854464	1366.081542	19.063923
45.952189	1378.983105	19.068941
45.982108	1372.392302	19.073959
46.355152	1365.981608	19.078976
46.153333	1370.803590	19.083994
46.627637	1364.831568	19.089011
46.415653	1374.814886	19.094029
46.164895	1370.053974	19.099047
46.409949	1377.353123	19.104064
46.464367	1382.652766	19.109082
46.674592	1378.640591	19.114099
46.538264	1395.406609	19.119117
46.538489	1392.872491	19.124135
46.839199	1383.077396	19.129152
46.618363	1381.707478	19.134170
46.818311	1388.849552	19.139187
46.824445	1388.384729	19.144205
46.827525	1391.890398	19.149223
46.961648	1384.765813	19.154240
46.752436	1376.385023	19.159258
46.798168	1384.529408	19.164275
46.569781	1391.640342	19.169293
46.853236	1398.409655	19.174311
47.240669	1402.104793	19.179328
47.097744	1405.358641	19.184346
47.206850	1403.404019	19.189363
47.161292	1411.679394	19.194381
47.116631	1402.136878	19.199399
47.150574	1406.085870	19.204416
47.371507	1415.055062	19.209434
47.844102	1423.404404	19.214451
47.775748	1425.996546	19.219469
47.770113	1421.080691	19.224487
47.916680	1423.680396	19.229504
47.800537	1420.583721	19.234522
47.942925	1408.253891	19.239539
47.987413	1406.280926	19.244557
47.698300	1410.715721	19.249575
48.084992	1406.496183	19.254592
47.912114	1417.098288	19.259610
48.266648	1419.299538	19.264627
48.266661	1402.662093	19.269645
47.909270	1398.372213	19.274663
47.854590	1405.449796	19.279680
48.059648	1409.851832	19.284698
48.545509	1426.281165	19.289715
48.254369	1432.202674	19.294733
48.310504	1421.678771	19.299751
48.446176	1425.987472	19.304768
48.421597	1426.912837	19.309786
48.582071	1433.745492	19.314803
48.479448	1425.613173	19.319821
48.426368	1424.576897	19.324839
48.469753	1433.355990	19.329856
48.381925	1433.448597	19.334874
48.809590	1424.198605	19.339891
48.524319	1429.705786	19.344909
48.209817	1433.213572	19.349927
48.945822	1440.310075	19.354944
48.988208	1447.028576	19.359962
49.080483	1445.837124	19.364979
49.156654	1438.611086	19.369997
49.200955	1446.414892	19.375015
49.285239	1442.617972	19.380032
48.871512	1437.551054	19.385050
49.245322	1433.036868	19.390067
49.341273	1440.731644	19.395085
49.107595	1447.736126	19.400103
49.655300	1445.381850	19.405120
49.527275	1452.802232	19.410138
49.269858	1440.626147	19.415155
49.487838	1449.097195	19.420173
49.376441	1440.354005	19.425191
49.742675	1442.446138	19.430208
49.583736	1445.677240	19.435226
49.703282	1439.511118	19.440243
49.979124	1443.567624	19.445261
49.491687	1449.188339	19.450279
49.449042	1452.489698	19.455296
49.481025	1454.804289	19.460314
49.595245	1461.852441	19.465331
49.808744	1468.178233	19.470349
49.986969	1471.984855	19.475367
50.267786	1466.522611	19.480384
49.989316	1470.599154	19.485402
50.012490	1471.731682	19.490419
49.891654	1468.831391	19.495437
49.698985	1477.565206	19.500455
50.692010	1478.041800	19.505472
50.734898	1479.057649	19.510490
50.451656	1469.391295	19.515507
50.391044	1469.315562	19.520525
50.529613	1486.846759	19.525543
50.625255	1483.196386	19.530560
51.037913	1487.304185	19.535578
50.621297	1485.873222	19.540595
51.044672	1486.709911	19.545613
50.991075	1487.986938	19.550631
50.853780	1485.101829	19.555648
50.924870	1490.174845	19.560666
51.045325	1484.327304	19.565683
50.937272	1487.266466	19.570701
50.948574	1481.805153	19.575719
51.044619	1480.553151	19.580736
50.956814	1486.152682	19.585754
50.913300	1485.209589	19.590771
50.820951	1471.268918	19.595789
50.962473	1481.399229	19.600807
51.147358	1475.519570	19.605824
51.202778	1503.601051	19.610842
51.452956	1504.512043	19.615859
51.679385	1503.782543	19.620877
51.361910	1505.321564	19.625895
51.598403	1503.479642	19.630912
51.668759	1503.610738	19.635930
51.619467	1502.046844	19.640947
51.782717	1501.838425	19.645965
51.613779	1512.029714	19.650983
51.841766	1501.135022	19.656000
51.672343	1503.111744	19.661018
51.591336	1504.301521	19.666035
51.722582	1503.791969	19.671053
51.826263	1527.861219	19.676071
52.396596	1522.783076	19.681088
52.496504	1521.069717	19.686106
52.442742	1517.335300	19.691123
52.496214	1511.712776	19.696141
52.294500	1523.360860	19.701159
52.847991	1516.505448	19.706176
52.432454	1516.112586	19.711194
52.169580	1505.868678	19.716211
52.169365	1509.128728	19.721229
52.230719	1524.062106	19.726247
52.457851	1517.014506	19.731264
52.122469	1521.462844	19.736282
52.303756	1512.954918	19.741299
52.860572	1529.572118	19.746317
52.704865	1541.288790	19.751335
52.960280	1534.934221	19.756352
52.840239	1539.200711	19.761370
52.925151	1533.510169	19.766387
53.012839	1532.735996	19.771405
53.293765	1537.744796	19.776423
53.395239	1533.970427	19.781440
53.219221	1530.119342	19.786458
53.646444	1541.644268	19.791475
53.364773	1534.808425	19.796493
53.451874	1537.559418	19.801511
53.422140	1524.009749	19.806528
53.420305	1521.535894	19.811546
53.345169	1532.561511	19.816563
53.517590	1527.472736	19.821581
53.691832	1530.920224	19.826599
53.748844	1529.327153	19.831616
53.676038	1528.426488	19.836634
53.546988	1527.209529	19.841651
53.980794	1537.319611	19.846669
54.039635	1542.110523	19.851687
54.114421	1541.931657	19.856704
54.299944	1538.201007	19.861722
53.955355	1550.161690	19.866739
54.315868	1548.972649	19.871757
54.226420	1553.155484	19.876775
54.617724	1551.276830	19.881792
54.458954	1546.469991	19.886810
54.090531	1538.584133	19.891827
54.217399	1546.406687	19.896845
54.075475	1538.460318	19.901863
54.306946	1542.608964	19.906880
54.381087	1545.002210	19.911898
54.196878	1535.951569	19.916915
54.567466	1544.525136	19.921933
55.051536	1558.587989	19.926951
55.088013	1550.635930	19.931968
54.989483	1541.360505	19.936986
54.961387	1538.209074	19.942003
54.964061	1527.358914	19.947021
54.453379	1546.111577	19.952039
54.888512	1547.164191	19.957056
55.225648	1552.353595	19.962074
55.041094	1558.946524	19.967091
55.442109	1557.946839	19.972109
55.210276	1556.332464	19.977127
55.653118	1547.951059	19.982144
55.600873	1547.589997	19.987162
55.795580	1552.842602	19.992179
55.714909	1555.278888	19.997197
55.403233	1553.112049	20.002215
55.488120	1547.260558	20.007232
55.311510	1557.194289	20.012250
54.992520	1558.118160	20.017267
55.358231	1556.366569	20.022285
55.164610	1568.060760	20.027303
55.875842	1572.627028	20.032320
55.958122	1575.192583	20.037338
55.927074	1581.578581	20.042355
55.882423	1585.685019	20.047373
56.194146	1590.212506	20.052391
56.162804	1577.101711	20.057408
56.213068	1585.160274	20.062426
55.933055	1592.733768	20.067443
56.423376	1584.048304	20.072461
56.267573	1579.714370	20.077479
55.806799	1587.950332	20.082496
56.417257	1590.458901	20.087514
56.151948	1602.167431	20.092531
56.454041	1600.318442	20.097549
56.538322	1603.369691	20.102567
56.464233	1607.597484	20.107584
56.503436	1606.799298	20.112602
56.803869	1617.886416	20.117619
57.014515	1624.379969	20.122637
56.875899	1646.562030	20.127655
57.245951	1639.766690	20.132672
57.453722	1623.166122	20.137690
57.149928	1637.490561	20.142707
57.487119	1630.826575	20.147725
57.208081	1627.259755	20.152743
57.422540	1618.008145	20.157760
57.575787	1626.277914	20.162778
57.415318	1628.070216	20.167795
57.786593	1618.402863	20.172813
57.700023	1615.544550	20.177831
57.206485	1612.386676	20.182848
57.482429	1616.903962	20.187866
57.796048	1623.842237	20.192883
57.606734	1625.850472	20.197901
57.716197	1623.621210	20.202919
57.546084	1621.624829	20.207936
57.769747	1617.683093	20.212954
57.703075	1628.653802	20.217971
57.740195	1618.561941	20.222989
57.794764	1633.395480	20.228007
57.744745	1643.962811	20.233024
58.161455	1645.128755	20.238042
57.902068	1643.064218	20.243059
57.936894	1641.834359	20.248077
58.235615	1646.307080	20.253095
58.152451	1659.710389	20.258112
58.751908	1655.391393	20.263130
58.651965	1661.971186	20.268147
58.734617	1665.505546	20.273165
58.609113	1668.299129	20.278183
58.734008	1669.390585	20.283200
59.032876	1656.266190	20.288218
58.886169	1675.186386	20.293235
59.197331	1666.957973	20.298253
59.113599	1659.917691	20.303271
58.977678	1661.324315	20.308288
59.120887	1651.212761	20.313306
59.184527	1658.802208	20.318323
59.411750	1653.297757	20.323341
59.250874	1659.104383	20.328359
59.426834	1659.982757	20.333376
59.363291	1662.343806	20.338394
59.485865	1657.183857	20.343411
59.362176	1649.294561	20.348429
59.635718	1658.407166	20.353447
59.057660	1662.116980	20.358464
59.472563	1658.782944	20.363482
58.973490	1663.910067	20.368499
59.277309	1672.292116	20.373517
59.414516	1678.244846	20.378535
59.652674	1680.997589	20.383552
60.071150	1677.997516	20.388570
59.701808	1684.745496	20.393587
59.871753	1676.075154	20.398605
59.948330	1694.111677	20.403623
60.198874	1710.978707	20.408640
60.430476	1708.897680	20.413658
60.121959	1704.454946	20.418675
60.222534	1717.867562	20.423693
60.330733	1701.077293	20.428711
60.090302	1710.664431	20.433728
60.490735	1708.071114	20.438746
60.443732	1710.470620	20.443763
60.309436	1708.837890	20.448781
60.520264	1716.256118	20.453799
60.627287	1734.079653	20.458816
61.038393	1727.022263	20.463834
60.835600	1726.283840	20.468851
60.608542	1724.719200	20.473869
60.560067	1717.670250	20.478887
61.064040	1724.433757	20.483904
61.373932	1728.797459	20.488922
61.491925	1749.465902	20.493939
61.773230	1739.212875	20.498957
61.715016	1722.584198	20.503975
61.769040	1719.921734	20.508992
61.589322	1709.992972	20.514010
61.600168	1720.402547	20.519027
61.969558	1717.085054	20.524045
61.998029	1714.464440	20.529063
61.355868	1711.547443	20.534080
61.797698	1712.270814	20.539098
62.081318	1716.190470	20.544115
61.879405	1707.066757	20.549133
62.016559	1708.642312	20.554151
62.093763	1710.684802	20.559168
62.177979	1717.718792	20.564186
62.474418	1729.119033	20.569203
62.469391	1730.678855	20.574221
62.274917	1716.504579	20.579239
61.837299	1727.327971	20.584256
62.249585	1720.907886	20.589274
62.226867	1733.490779	20.594291
62.188883	1725.114724	20.599309
62.642275	1728.357840	20.604327
62.495145	1739.997567	20.609344
62.248639	1732.884766	20.614362
62.311597	1735.002062	20.619379
62.651790	1747.137133	20.624397
63.007489	1749.413985	20.629415
62.768004	1750.906169	20.634432
62.947200	1744.036361	20.639450
63.072312	1755.810440	20.644467
62.955097	1754.411737	20.649485
62.985666	1747.382027	20.654503
62.764931	1758.591402	20.659520
63.148986	1774.879115	20.664538
63.241672	1776.082893	20.669555
63.022351	1783.183103	20.674573
63.519864	1782.370359	20.679591
63.171502	1781.118098	20.684608
63.418931	1780.934441	20.689626
63.381049	1791.370579	20.694643
63.375256	1798.093558	20.699661
64.042944	1801.565261	20.704679
63.925737	1804.209246	20.709696
64.427061	1800.905912	20.714714
64.058439	1794.661033	20.719731
64.108917	1798.023700	20.724749
64.508228	1798.545406	20.729767
64.357465	1794.800786	20.734784
64.646617	1789.160416	20.739802
64.435699	1797.187154	20.744819
64.460351	1791.521692	20.749837
64.669814	1793.773979	20.754855
64.583221	1796.722474	20.759872
65.107813	1775.089291	20.764890
64.969529	1783.991518	20.769907
64.824630	1787.106883	20.774925
65.026023	1779.005966	20.779943
65.032718	1799.852746	20.784960
65.224694	1795.202674	20.789978
64.862788	1794.539516	20.794995
64.942816	1791.361739	20.800013
64.798016	1786.801974	20.805031
64.932200	1792.398597	20.810048
65.080574	1779.445869	20.815066
65.299590	1786.310572	20.820083
64.686929	1790.391881	20.825101
65.000030	1777.451379	20.830119
65.134517	1804.877224	20.835136
64.623377	1807.188056	20.840154
64.940948	1812.869746	20.845171
65.171972	1827.552893	20.850189
65.398792	1822.654385	20.855207
65.410699	1823.463633	20.860224
65.691506	1841.995542	20.865242
65.930707	1847.806213	20.870259
65.814539	1857.127923	20.875277
66.053464	1847.679875	20.880295
65.992125	1852.467490	20.885312
66.402202	1852.832883	20.890330
66.535735	1848.624254	20.895347
66.416415	1857.627709	20.900365
66.630311	1858.067829	20.905383
66.314698	1851.347605	20.910400
66.524741	1856.503235	20.915418
66.589541	1852.589338	20.920435
66.418386	1868.045213	20.925453
66.715990	1874.351743	20.930471
67.057895	1879.019776	20.935488
67.030091	1870.793552	20.940506
67.168345	1868.253655	20.945523
67.288685	1866.502367	20.950541
67.212589	1867.259044	20.955559
66.948860	1871.077756	20.960576
67.316003	1871.206829	20.965594
67.112555	1871.550976	20.970611
66.886053	1876.979714	20.975629
67.148256	1872.044124	20.980647
67.139454	1878.587716	20.985664
67.411812	1887.956251	20.990682
67.611618	1884.958631	20.995699
67.555325	1889.480374	21.000717
67.966933	1892.345006	21.005735
67.812094	1899.312142	21.010752
68.138534	1893.675402	21.015770
68.578272	1893.913097	21.020787
68.423124	1902.350935	21.025805
68.247725	1886.336816	21.030823
68.000109	1895.530684	21.035840
67.880270	1886.340451	21.040858
68.278724	1891.583526	21.045875
68.009108	1901.191089	21.050893
68.369324	1896.375937	21.055911
68.558787	1898.041198	21.060928
68.250906	1900.206783	21.065946
68.553486	1904.473834	21.070963
68.665101	1908.634914	21.075981
68.376972	1909.541374	21.080999
68.451778	1919.376199	21.086016
68.617387	1911.059880	21.091034
68.798115	1915.879254	21.096051
68.533652	1922.014528	21.101069
68.864943	1932.320684	21.106087
68.968513	1942.103704	21.111104
69.218742	1943.813158	21.116122
69.364835	1929.872876	21.121139
69.189650	1941.845316	21.126157
69.341231	1931.672339	21.131175
69.188352	1944.332453	21.136192
69.977193	1944.847166	21.141210
70.071099	1957.292135	21.146227
69.787299	1957.229057	21.151245
69.885550	1948.380391	21.156263
69.638416	1959.382555	21.161280
69.793177	1958.449594	21.166298
70.425040	1967.165729	21.171315
70.208704	1965.501565	21.176333
70.322587	1963.208455	21.181351
70.115079	1960.555115	21.186368
70.086798	1964.820044	21.191386
70.139330	1961.299366	21.196403
70.085533	1965.315794	21.201421
70.308415	1960.187480	21.206439
70.105919	1976.995905	21.211456
70.109538	1980.066088	21.216474
70.597184	1981.927937	21.221491
70.577468	1986.156822	21.226509
70.645424	1979.566184	21.231527
71.180107	1994.407326	21.236544
71.066193	2004.770216	21.241562
70.946022	1998.805332	21.246579
71.410240	2012.701215	21.251597
71.497242	1996.863902	21.256615
71.770960	2001.813994	21.261632
71.692663	1994.362463	21.266650
71.608857	1993.867445	21.271667
71.827615	1995.493438	21.276685
72.029307	1986.382486	21.281703
71.561508	1977.612468	21.286720
71.826680	1977.006310	21.291738
71.914494	1984.544792	21.296755
71.858098	1990.767619	21.301773
71.921647	1990.000340	21.306791
72.070144	1985.356989	21.311808
72.229750	1991.830219	21.316826
71.962637	1976.975898	21.321843
71.789287	1982.923430	21.326861
71.885263	1985.250218	21.331879
71.928138	1979.035885	21.336896
72.261257	1990.825072	21.341914
72.600578	1995.764948	21.346931
72.429992	2014.133778	21.351949
72.592629	2009.415632	21.356967
72.355805	2012.614779	21.361984
72.088069	2015.244360	21.367002
72.542061	2012.633193	21.372019
72.585929	2023.877279	21.377037
72.580595	2031.392413	21.382055
73.167374	2035.211288	21.387072
72.788108	2033.768153	21.392090
72.898583	2034.019244	21.397107
73.255479	2034.153070	21.402125
73.367060	2041.807801	21.407143
73.345399	2045.225929	21.412160
73.554520	2049.463383	21.417178
73.896929	2047.377689	21.422195
73.994911	2061.292760	21.427213
74.101204	2054.096499	21.432231
74.200992	2049.227175	21.437248
73.823744	2055.282220	21.442266
74.289891	2055.077132	21.447283
73.871350	2059.743685	21.452301
74.487256	2051.470806	21.457319
73.958097	2052.162325	21.462336
73.939133	2049.971942	21.467354
74.527962	2040.084290	21.472371
74.409954	2041.327202	21.477389
74.265323	2040.687012	21.482407
74.380050	2045.254755	21.487424
74.267130	2046.149722	21.492442
74.925039	2056.222053	21.497459
74.960270	2065.084781	21.502477
75.035615	2071.710020	21.507495
75.079885	2070.399763	21.512512
74.945957	2073.567120	21.517530
75.061910	2069.061363	21.522547
74.925320	2070.073631	21.527565
74.781781	2073.229861	21.532583
75.226461	2065.539079	21.537600
75.322790	2069.298617	21.542618
75.374846	2068.656207	21.547635
75.319355	2088.449455	21.552653
75.592648	2091.057932	21.557671
75.961320	2093.291781	21.562688
75.573992	2091.720502	21.567706
75.363358	2094.880870	21.572723
75.482712	2104.298589	21.577741
76.218679	2106.768757	21.582759
76.316562	2100.157636	21.587776
75.765259	2112.220309	21.592794
76.481485	2109.943857	21.597811
76.078157	2120.285599	21.602829
76.218086	2114.409574	21.607847
76.486652	2108.952198	21.612864
76.246074	2113.237592	21.617882
76.173738	2116.935034	21.622899
76.415790	2118.352275	21.627917
76.493553	2137.664063	21.632935
77.063654	2129.991598	21.637952
77.424221	2134.552648	21.642970
77.032417	2125.903274	21.647987
77.132993	2135.273438	21.653005
77.225238	2129.038741	21.658023
77.459725	2131.486001	21.663040
77.515623	2130.426405	21.668058
77.605072	2124.015413	21.673075
77.010663	2120.787942	21.678093
77.280470	2122.465962	21.683111
77.500585	2118.186983	21.688128
77.431334	2126.826156	21.693146
77.414185	2119.936279	21.698163
77.349759	2129.606696	21.703181
77.392992	2136.142280	21.708199
78.125457	2145.202619	21.713216
77.916213	2148.356468	21.718234
77.792189	2149.445682	21.723251
77.779965	2147.020697	21.728269
78.073900	2150.231911	21.733287
78.427482	2169.194663	21.738304
78.727998	2174.629803	21.743322
78.581728	2168.713109	21.748339
78.745904	2173.109076	21.753357
78.631367	2174.881657	21.758375
79.042066	2167.006765	21.763392
79.111056	2170.745334	21.768410
78.831965	2170.425889	21.773427
78.843205	2175.347465	21.778445
78.728514	2171.445664	21.783463
78.706342	2168.832868	21.788480
78.794807	2173.152256	21.793498
79.115840	2185.846057	21.798515
79.115963	2193.985289	21.803533
79.005791	2194.507432	21.808551
79.363897	2183.910819	21.813568
79.468271	2209.618821	21.818586
79.620176	2205.224203	21.823603
79.796009	2215.368525	21.828621
79.640092	2217.633571	21.833639
79.922488	2207.815629	21.838656
79.526759	2210.638744	21.843674
79.980874	2211.448592	21.848691
80.130307	2218.409506	21.853709
80.417061	2229.792640	21.858727
80.637773	2221.120442	21.863744
80.719026	2229.395388	21.868762
80.761978	2226.024481	21.873779
80.593964	2224.917686	21.878797
80.848289	2227.226163	21.883815
81.042500	2221.556257	21.888832
81.075176	2226.771170	21.893850
80.882515	2228.802084	21.898867
80.821171	2219.488957	21.903885
80.705385	2228.671939	21.908903
81.067952	2227.750792	21.913920
81.111633	2223.347772	21.918938
81.140338	2222.399707	21.923955
81.469012	2236.487290	21.928973
81.483828	2249.856851	21.933991
81.594418	2244.973169	21.939008
81.463593	2251.112995	21.944026
81.691316	2247.653352	21.949043
82.077149	2244.863407	21.954061
81.645061	2254.367060	21.959079
82.243413	2243.644639	21.964096
82.161601	2248.126263	21.969114
81.980524	2243.442635	21.974131
81.841055	2258.963345	21.979149
81.960678	2261.655735	21.984167
82.273378	2267.521375	21.989184
82.054159	2274.801654	21.994202
82.550887	2269.460193	21.999219
82.501450	2265.819625	22.004237
82.651580	2274.380530	22.009255
82.557658	2267.183796	22.014272
82.625780	2282.492315	22.019290
82.846785	2291.616580	22.024307
83.117094	2299.145717	22.029325
82.837050	2303.282657	22.034343
83.034277	2293.935546	22.039360
82.893232	2303.633766	22.044378
82.800820	2300.896180	22.049395
83.074548	2307.995576	22.054413
83.251776	2321.980567	22.059431
83.358777	2315.301671	22.064448
83.704694	2320.126996	22.069466
83.757029	2311.237960	22.074483
83.931696	2310.472303	22.079501
83.807228	2314.793318	22.084519
84.228535	2310.082160	22.089536
83.743350	2333.887554	22.094554
84.229522	2335.348861	22.099571
84.786943	2335.561929	22.104589
84.267232	2334.607720	22.109607
84.486998	2340.232219	22.114624
84.581877	2335.575033	22.119642
84.663137	2335.934824	22.124659
84.709770	2326.910961	22.129677
84.472828	2325.612908	22.134695
84.684385	2321.799143	22.139712
84.327014	2330.581108	22.144730
84.858369	2347.881573	22.149747
84.901479	2360.221115	22.154765
85.157626	2366.165025	22.159783
85.131756	2355.987875	22.164800
85.224809	2363.958072	22.169818
85.537708	2369.224077	22.174835
85.663044	2379.086003	22.179853
85.204185	2381.215187	22.184871
85.773600	2375.821351	22.189888
85.826025	2384.277592	22.194906
85.819806	2382.662730	22.199923
86.148558	2373.746407	22.204941
86.096526	2381.489877	22.209959
86.315704	2373.120820	22.214976
86.193610	2373.973047	22.219994
86.520933	2380.950513	22.225011
86.942056	2378.757846	22.230029
86.476277	2389.377725	22.235047
86.805447	2386.678635	22.240064
86.633994	2389.662531	22.245082
86.756932	2395.131699	22.250099
86.838066	2388.693503	22.255117
86.838545	2402.958556	22.260135
87.020513	2394.863542	22.265152
87.057639	2389.896578	22.270170
87.264564	2382.959089	22.275187
87.435431	2386.808081	22.280205
87.011670	2392.453889	22.285223
87.390890	2395.004890	22.290240
87.557888	2407.448260	22.295258
87.298838	2408.261849	22.300275
87.716623	2407.193233	22.305293
87.633035	2411.163903	22.310311
87.817598	2404.930518	22.315328
87.703043	2401.814488	22.320346
87.839920	2422.572294	22.325363
88.146774	2420.492093	22.330381
88.256806	2431.688262	22.335399
88.385401	2430.977114	22.340416
88.130966	2428.757070	22.345434
88.138173	2437.258249	22.350451
88.287714	2441.236813	22.355469
87.937391	2436.551080	22.360487
88.285845	2437.812917	22.365504
88.696836	2444.780537	22.370522
88.839230	2445.531625	22.375539
89.063820	2442.372253	22.380557
88.702376	2448.813157	22.385575
89.035774	2452.624234	22.390592
89.166927	2462.822993	22.395610
89.384975	2474.245384	22.400627
89.589247	2466.847499	22.405645
89.300194	2475.735670	22.410663
89.515364	2474.323032	22.415680
89.873787	2471.679339	22.420698
89.836351	2467.964273	22.425715
89.935079	2471.215406	22.430733
89.533228	2482.393467	22.435751
89.652713	2492.209027	22.440768
90.327419	2494.439465	22.445786
90.203081	2498.918304	22.450803
90.465783	2492.833680	22.455821
90.469085	2491.624451	22.460839
90.502857	2493.367660	22.465856
90.557557	2497.701852	22.470874
90.446968	2507.591113	22.475891
90.802410	2512.623304	22.480909
90.576240	2517.973282	22.485927
90.941364	2520.737950	22.490944
90.833628	2511.671751	22.495962
90.923908	2521.775915	22.500979
91.502561	2533.413617	22.505997
91.499375	2531.716213	22.511015
91.703293	2531.656098	22.516032
91.927378	2528.872356	22.521050
91.688808	2528.035320	22.526067
92.201394	2518.380199	22.531085
92.004495	2529.078226	22.536103
92.063006	2522.586696	22.541120
92.363286	2526.829008	22.546138
92.055771	2528.612732	22.551155
92.034632	2515.382887	22.556173
91.825985	2524.362713	22.561191
92.182533	2522.271607	22.566208
92.531891	2534.563589	22.571226
92.567037	2550.868462	22.576243
92.492606	2545.495917	22.581261
92.619897	2541.840402	22.586279
92.711774	2541.914503	22.591296
92.839350	2543.886125	22.596314
92.470339	2553.907171	22.601331
93.064288	2559.751211	22.606349
93.144930	2564.131877	22.611367
93.298925	2565.408220	22.616384
93.458212	2559.519567	22.621402
93.302068	2572.474142	22.626419
93.672666	2567.720316	22.631437
93.383517	2568.667995	22.636455
93.389158	2586.927916	22.641472
93.954675	2584.892638	22.646490
93.668782	2599.413887	22.651507
94.164374	2593.412898	22.656525
94.078120	2590.743741	22.661543
93.958448	2598.280069	22.666560
94.365704	2601.416913	22.671578
94.211402	2620.086806	22.676595
94.520363	2611.034581	22.681613
94.181859	2625.639787	22.686631
94.255409	2614.500201	22.691648
94.479863	2608.206883	22.696666
94.345937	2620.744594	22.701683
94.817404	2629.018935	22.706701
94.959579	2634.706104	22.711719
95.130740	2635.418005	22.716736
95.075709	2642.101627	22.721754
94.686854	2645.217250	22.726771
95.600255	2645.993483	22.731789
95.554814	2657.646377	22.736807
95.619433	2672.277226	22.741824
95.772087	2665.341766	22.746842
95.703916	2664.755925	22.751859
96.097156	2659.815499	22.756877
96.072673	2661.179602	22.761895
95.982216	2667.767755	22.766912
95.891993	2663.846257	22.771930
95.955561	2666.689458	22.776947
96.477525	2675.271563	22.781965
96.744935	2682.438369	22.786983
96.254774	2683.010220	22.792000
96.655580	2678.968084	22.797018
96.739727	2682.111063	22.802035
96.531884	2680.925227	22.807053
97.089964	2687.371387	22.812071
96.711343	2702.705635	22.817088
97.079196	2704.949159	22.822106
97.162645	2712.908382	22.827123
97.260020	2705.836334	22.832141
97.425252	2708.367045	22.837159
97.799988	2717.148832	22.842176
98.096521	2720.568044	22.847194
97.839461	2723.786247	22.852211
98.217198	2725.071951	22.857229
98.063457	2721.245542	22.862247
97.738077	2725.616873	22.867264
97.885475	2722.785076	22.872282
98.303549	2728.451411	22.877299
98.221728	2724.604336	22.882317
98.298538	2729.386457	22.887335
98.604866	2739.715903	22.892352
98.849600	2751.427829	22.897370
98.022707	2747.595758	22.902387
98.755694	2746.585355	22.907405
98.880030	2742.008691	22.912423
98.968660	2746.874190	22.917440
99.036147	2758.335984	22.922458
98.559837	2775.001579	22.927475
98.889795	2772.905117	22.932493
99.136624	2771.664266	22.937511
99.683714	2788.779657	22.942528
99.740221	2782.241005	22.947546
99.780490	2790.225921	22.952563
100.026094	2792.933495	22.957581
99.820266	2791.984042	22.962599
99.996940	2790.012438	22.967616
100.258695	2787.771946	22.972634
100.244050	2796.169391	22.977651
100.168856	2791.888890	22.982669
100.359211	2802.305861	22.987687
100.422143	2820.528696	22.992704
100.726272	2806.200181	22.997722
100.652361	2809.610808	23.002739
100.733943	2808.698665	23.007757
100.579783	2816.818015	23.012775
100.668690	2821.557248	23.017792
101.182208	2824.832235	23.022810
101.145747	2836.685835	23.027827
101.168776	2831.070794	23.032845
101.530848	2835.063697	23.037863
101.445536	2833.707282	23.042880
101.615600	2832.563593	23.047898
101.619834	2834.406116	23.052915
101.593836	2846.491643	23.057933
101.845133	2853.844078	23.062951
101.559552	2862.163806	23.067968
101.808049	2852.679023	23.072986
102.168224	2852.774475	23.078003
102.244943	2857.528240	23.083021
102.553194	2872.146568	23.088039
102.221921	2876.108563	23.093056
102.546293	2878.358878	23.098074
102.882366	2883.921255	23.103091
102.742940	2878.811216	23.108109
102.848545	2876.654991	23.113127
102.736217	2896.420107	23.118144
102.964755	2897.151490	23.123162
102.930818	2900.966202	23.128179
103.313688	2896.279813	23.133197
103.308231	2900.834926	23.138215
103.477151	2910.958626	23.143232
103.667964	2910.420826	23.148250
103.649373	2919.017776	23.153267
104.064416	2920.726914	23.158285
103.968493	2926.912034	23.163303
103.967608	2913.347354	23.168320
104.279299	2911.260032	23.173338
104.558181	2905.551480	23.178355
104.649743	2904.770334	23.183373
104.960217	2909.822263	23.188391
104.955301	2915.431427	23.193408
104.902462	2903.408700	23.198426
105.067325	2911.390053	23.203443
105.165083	2923.008199	23.208461
105.597906	2925.494123	23.213479
105.204139	2928.130834	23.218496
105.371031	2926.072367	23.223514
105.770850	2930.453926	23.228531
105.533380	2928.022875	23.233549
105.863662	2922.953313	23.238567
105.698620	2916.711060	23.243584
106.079998	2909.250702	23.248602
105.849270	2922.400194	23.253619
105.831421	2922.459820	23.258637
105.844635	2922.154816	23.263655
105.986664	2941.400655	23.268672
106.582942	2942.245214	23.273690
106.256775	2946.237990	23.278707
106.572747	2949.701561	23.283725
106.977395	2945.071735	23.288743
106.402945	2950.466598	23.293760
106.850905	2946.619050	23.298778
106.584150	2968.560743	23.303795
106.711363	2957.172727	23.308813
107.009024	2962.210885	23.313831
106.828791	2971.177041	23.318848
107.424758	2975.427077	23.323866
107.711734	2995.426806	23.328883
107.569431	2992.857842	23.333901
107.726340	2994.954348	23.338919
107.623381	2996.403284	23.343936
107.777161	2990.654216	23.348954
107.984266	2995.794854	23.353971
107.717536	2999.731046	23.358989
107.969293	3009.387426	23.364007
107.927067	3029.990766	23.369024
108.036272	3019.359824	23.374042
108.228323	3016.782985	23.379059
108.497310	3037.713456	23.384077
108.791622	3038.343078	23.389095
108.831727	3038.112788	23.394112
108.952497	3052.223915	23.399130
109.239251	3047.239997	23.404147
109.163894	3043.063613	23.409165
109.519394	3041.638551	23.414183
109.135588	3036.733788	23.419200
109.717619	3051.773586	23.424218
109.532477	3055.804395	23.429235
109.698005	3060.115155	23.434253
109.684763	3056.090058	23.439271
109.517418	3068.554381	23.444288
109.761552	3065.249834	23.449306
110.250485	3079.275257	23.454323
110.319628	3085.725095	23.459341
110.149117	3092.123876	23.464359
110.122196	3091.307514	23.469376
110.343798	3083.916146	23.474394
110.496801	3093.616352	23.479411
110.698219	3102.229634	23.484429
110.846883	3093.893314	23.489447
110.704863	3110.201029	23.494464
110.909829	3112.148041	23.499482
111.253201	3118.100713	23.504499
111.188646	3122.668240	23.509517
111.834447	3131.783606	23.514535
111.667297	3134.022110	23.519552
111.586223	3124.181356	23.524570
111.504781	3135.379371	23.529587
111.797399	3138.979173	23.534605
112.340063	3134.245751	23.539623
112.183318	3145.165133	23.544640
112.077121	3149.025865	23.549658
112.093617	3152.416169	23.554675
112.073808	3160.028712	23.559693
112.217752	3164.768936	23.564711
112.129168	3175.930214	23.569728
112.740763	3182.939481	23.574746
113.155001	3187.366201	23.579763
113.420966	3189.777144	23.584781
113.391569	3189.636576	23.589799
113.327807	3186.632434	23.594816
113.811216	3187.147405	23.599834
113.754153	3183.567805	23.604851
113.763691	3185.059207	23.609869
113.794113	3182.397045	23.614887
114.062480	3186.846475	23.619904
113.908483	3198.040045	23.624922
114.366773	3203.914888	23.629939
113.978299	3205.547163	23.634957
114.418744	3203.941588	23.639975
114.019458	3220.147431	23.644992
114.666660	3213.655525	23.650010
114.746158	3216.496333	23.655027
114.540516	3230.102940	23.660045
114.933643	3226.749916	23.665063
114.960201	3234.380521	23.670080
114.930606	3231.431019	23.675098
114.845993	3244.479093	23.680115
114.832914	3254.233650	23.685133
115.098294	3253.759977	23.690151
115.016245	3260.397537	23.695168
115.554740	3271.073036	23.700186
115.928532	3282.244452	23.705203
116.030310	3286.047584	23.710221
116.096989	3285.033584	23.715239
115.850526	3281.540263	23.720256
116.073383	3279.132179	23.725274
116.455709	3292.685165	23.730291
116.312685	3304.369451	23.735309
116.787497	3298.156847	23.740327
116.748586	3298.876233	23.745344
116.677697	3309.267894	23.750362
117.170446	3308.219119	23.755379
117.096267	3310.228550	23.760397
117.114815	3300.754084	23.765415
117.284592	3310.259271	23.770432
117.325100	3316.918800	23.775450
117.778540	3317.552063	23.780467
117.717520	3327.011131	23.785485
117.730379	3310.534035	23.790503
117.808689	3319.172900	23.795520
117.504364	3326.249078	23.800538
118.089886	3343.974468	23.805555
117.841088	3353.481723	23.810573
118.414376	3340.326000	23.815591
118.257493	3350.869944	23.820608
118.218324	3349.114942	23.825626
118.746350	3362.793636	23.830643
118.950384	3379.230774	23.835661
119.033664	3372.586741	23.840679
118.990051	3378.650250	23.845696
118.723026	3375.239016	23.850714
119.248123	3392.427844	23.855731
119.336612	3399.730104	23.860749
119.402012	3394.865771	23.865767
119.190984	3389.526865	23.870784
119.581487	3404.691464	23.875802
119.831414	3411.627728	23.880819
119.437816	3418.784121	23.885837
120.402206	3427.676448	23.890855
120.729264	3431.027921	23.895872
120.660698	3442.754359	23.900890
120.794311	3438.034047	23.905907
120.637917	3441.400824	23.910925
120.981667	3431.888283	23.915943
120.754272	3432.135187	23.920960
121.204331	3438.904587	23.925978
121.254582	3438.050946	23.930995
121.225512	3456.061504	23.936013
121.434717	3460.665398	23.941031
121.649188	3463.501011	23.946048
121.139867	3464.647135	23.951066
121.369342	3457.778315	23.956083
121.871280	3472.357509	23.961101
121.922320	3480.823951	23.966119
121.840549	3476.001446	23.971136
121.926175	3479.630388	23.976154
122.432889	3488.505629	23.981171
122.332138	3503.689984	23.986189
122.234879	3502.912961	23.991207
122.326840	3505.199542	23.996224
122.776862	3510.125760	24.001242
123.526107	3515.901752	24.006259
123.641389	3525.832154	24.011277
123.845666	3515.078807	24.016295
124.252210	3513.996099	24.021312
123.590216	3506.293949	24.026330
123.983960	3504.095944	24.031347
123.587567	3509.772555	24.036365
123.836293	3510.358794	24.041383
124.160574	3514.360890	24.046400
123.983752	3520.318938	24.051418
124.283576	3509.118321	24.056435
123.929469	3504.170931	24.061453
123.900433	3509.077050	24.066471
124.182594	3519.521175	24.071488
123.964219	3537.201482	24.076506
124.193578	3535.701336	24.081523
124.579904	3559.880807	24.086541
124.562525	3563.058685	24.091559
124.937905	3565.746171	24.096576
124.937688	3579.055937	24.101594
125.382183	3585.217112	24.106611
125.355097	3585.366551	24.111629
125.609817	3589.357401	24.116647
125.690341	3595.499498	24.121664
125.581913	3601.882481	24.126682
125.979076	3600.119489	24.131699
126.410464	3608.990737	24.136717
126.266026	3608.953294	24.141735
126.306243	3615.559323	24.146752
126.613543	3616.130133	24.151770
127.032601	3627.007501	24.156787
127.167567	3627.497831	24.161805
127.292141	3626.970323	24.166823
127.089386	3623.236570	24.171840
127.375139	3633.345644	24.176858
127.644089	3619.782608	24.181875
127.558033	3627.585566	24.186893
127.661587	3625.713630	24.191911
127.571077	3631.737182	24.196928
127.594278	3652.498326	24.201946
127.880354	3647.432289	24.206963
127.840140	3653.318613	24.211981
128.327214	3657.904545	24.216999
128.367526	3666.672585	24.222016
128.326194	3674.367602	24.227034
128.276823	3667.791457	24.232051
128.472158	3681.342287	24.237069
128.878083	3685.151806	24.242087
129.080346	3694.039832	24.247104
128.887683	3694.054084	24.252122
129.622865	3687.608281	24.257139
129.471270	3699.101627	24.262157
129.716185	3690.226114	24.267175
129.872658	3691.950336	24.272192
129.786473	3711.336685	24.277210
130.083060	3698.504687	24.282227
130.393955	3711.775582	24.287245
130.136541	3698.300749	24.292263
130.408711	3702.670810	24.297280
130.183599	3707.948382	24.302298
130.671158	3717.991366	24.307315
130.528177	3728.498648	24.312333
130.527939	3734.369306	24.317351
130.798848	3735.706437	24.322368
130.864595	3749.817209	24.327386
131.065269	3753.551387	24.332403
130.978406	3761.897401	24.337421
131.257635	3759.205885	24.342439
131.346015	3766.524092	24.347456
131.650253	3788.624068	24.352474
132.142622	3784.564276	24.357491
131.632270	3788.784755	24.362509
131.768638	3789.896650	24.367527
132.399404	3801.009442	24.372544
132.204830	3813.390144	24.377562
132.502319	3809.234438	24.382579
132.947419	3813.795383	24.387597
132.717867	3811.274604	24.392615
133.196355	3819.166500	24.397632
132.971439	3820.839645	24.402650
133.153588	3824.437848	24.407667
133.377616	3829.986402	24.412685
133.265842	3836.426801	24.417703
133.730796	3828.214492	24.422720
133.691976	3837.509404	24.427738
133.393519	3834.295506	24.432755
133.760223	3843.896565	24.437773
133.877890	3852.917777	24.442791
134.106756	3862.044775	24.447808
133.805271	3869.373222	24.452826
134.423430	3871.303331	24.457843
134.610444	3885.692017	24.462861
134.574053	3887.563066	24.467879
134.677100	3881.155645	24.472896
134.440905	3905.596627	24.477914
134.771856	3912.754033	24.482931
135.114487	3907.451867	24.487949
134.872779	3928.598605	24.492967
135.264846	3927.663316	24.497984
135.337507	3935.217602	24.503002
135.698347	3945.012160	24.508019
135.982655	3954.619793	24.513037
136.150453	3951.443752	24.518055
136.229175	3947.303137	24.523072
136.454342	3963.620736	24.528090
136.653064	3971.483663	24.533107
136.870643	3967.283549	24.538125
137.159764	3977.313386	24.543143
137.215465	3975.827617	24.548160
137.092849	3972.314878	24.553178
137.168289	3976.021256	24.558195
136.887398	3983.832609	24.563213
136.949469	3999.102500	24.568231
137.452610	3998.749607	24.573248
137.370840	4017.207651	24.578266
137.710104	4016.940241	24.583283
137.614182	4027.367775	24.588301
137.844929	4035.093180	24.593319
138.618282	4039.154885	24.598336
138.481919	4044.109421	24.603354
138.535467	4037.097333	24.608371
138.632893	4048.561599	24.613389
138.946820	4065.200037	24.618407
139.143758	4061.460777	24.623424
138.889962	4073.001836	24.628442
139.289045	4069.594075	24.633459
139.353856	4077.032860	24.638477
139.508425	4096.473670	24.643495
139.793777	4100.371489	24.648512
140.059064	4099.727372	24.653530
139.742453	4099.454761	24.658547
139.746105	4106.524325	24.663565
140.113719	4123.094488	24.668583
140.214253	4117.441729	24.673600
140.398259	4132.301368	24.678618
140.633815	4147.730596	24.683635
140.938113	4150.075733	24.688653
140.743581	4151.024540	24.693671
141.001026	4157.303411	24.698688
140.901874	4169.057177	24.703706
141.282519	4170.042687	24.708723
141.817892	4177.922729	24.713741
141.529257	4185.176708	24.718759
141.945757	4198.671399	24.723776
142.223191	4195.756001	24.728794
142.074367	4193.137379	24.733811
142.509699	4197.185465	24.738829
142.396755	4200.826530	24.743847
142.798521	4192.494486	24.748864
142.547039	4199.824750	24.753882
142.697697	4204.434794	24.758899
142.966373	4207.281025	24.763917
142.931810	4218.103124	24.768935
142.771962	4215.943880	24.773952
142.874165	4231.109873	24.778970
143.109149	4237.000886	24.783987
143.081791	4243.889109	24.789005
143.459298	4264.412727	24.794023
143.572772	4267.725016	24.799040
143.797120	4269.665981	24.804058
143.773779	4276.641968	24.809075
144.097194	4302.325171	24.814093
144.372627	4301.493244	24.819111
144.852758	4291.195188	24.824128
145.072264	4314.151738	24.829146
145.166139	4319.045253	24.834163
145.544554	4310.401158	24.839181
145.133861	4318.722095	24.844199
145.698896	4307.486006	24.849216
145.627737	4308.563961	24.854234
145.574949	4305.605269	24.859251
146.240076	4316.062828	24.864269
146.032920	4324.935999	24.869287
146.342349	4321.526369	24.874304
146.425976	4325.540864	24.879322
146.513587	4330.350136	24.884339
146.759009	4323.923548	24.889357
146.535208	4342.359849	24.894375
147.061066	4342.366392	24.899392
146.867285	4356.123502	24.904410
146.920003	4359.110696	24.909427
147.185150	4362.614019	24.914445
147.159276	4378.074677	24.919463
147.898324	4380.497349	24.924480
147.639376	4388.425400	24.929498
147.392317	4388.820569	24.934515
147.971936	4397.164114	24.939533
147.865037	4407.091716	24.944551
148.164766	4403.421604	24.949568
148.008926	4428.507300	24.954586
148.180160	4433.016353	24.959603
148.807870	4431.968600	24.964621
148.571631	4447.272688	24.969639
148.783808	4449.199786	24.974656
149.226729	4470.594077	24.979674
149.489289	4473.504430	24.984691
149.739395	4471.612746	24.989709
149.694523	4481.890557	24.994727
150.105781	4478.332477	24.999744
150.108269	4481.744150	25.004762
150.610193	4485.816654	25.009779
150.700560	4483.836211	25.014797
150.883799	4493.412522	25.019815
151.025277	4479.843438	25.024832
151.019353	4489.392384	25.029850
150.814568	4489.664187	25.034867
151.035186	4476.212195	25.039885
151.085481	4491.102416	25.044903
151.297793	4493.408261	25.049920
151.383832	4496.450261	25.054938
151.558125	4509.168553	25.059955
151.902944	4510.453203	25.064973
151.976715	4524.351854	25.069991
152.295430	4526.972556	25.075008
152.655444	4528.437912	25.080026
152.705838	4531.374993	25.085043
152.809321	4524.111901	25.090061
152.629493	4533.252367	25.095079
152.869652	4536.298785	25.100096
152.844395	4535.134899	25.105114
152.830450	4542.554573	25.110131
153.277078	4553.986887	25.115149
153.439556	4557.421011	25.120167
153.799478	4552.876652	25.125184
153.696774	4554.833848	25.130202
153.821449	4566.751874	25.135219
153.936955	4564.518155	25.140237
153.759388	4573.194302	25.145255
153.903440	4579.705608	25.150272
154.000773	4592.653730	25.155290
154.293519	4598.052943	25.160307
154.660427	4607.329270	25.165325
155.059637	4617.626398	25.170343
154.833654	4623.519865	25.175360
155.042862	4632.041131	25.180378
154.909112	4642.433875	25.185395
155.386228	4638.647720	25.190413
155.565546	4655.219280	25.195431
156.039474	4663.367926	25.200448
156.388411	4660.709615	25.205466
156.318661	4667.513064	25.210483
156.474407	4658.976068	25.215501
156.328598	4687.501026	25.220519
156.716057	4688.816927	25.225536
156.706222	4694.215932	25.230554
156.870058	4705.199972	25.235571
157.319952	4706.698695	25.240589
157.362097	4721.861824	25.245607
157.419214	4716.272454	25.250624
157.427358	4724.405266	25.255642
157.511013	4735.427060	25.260659
157.567480	4745.888097	25.265677
157.566568	4751.825474	25.270695
157.794378	4764.406201	25.275712
158.349161	4764.127323	25.280730
158.425837	4788.681760	25.285747
158.675479	4791.802499	25.290765
159.046959	4789.172224	25.295783
158.828819	4793.691486	25.300800
159.320838	4807.146467	25.305818
159.376630	4819.173234	25.310835
160.149886	4813.772197	25.315853
160.095511	4809.276494	25.320871
160.137284	4816.419311	25.325888
160.657949	4823.894749	25.330906
160.468488	4834.542477	25.335923
160.643427	4834.442680	25.340941
160.622298	4833.997795	25.345959
160.796750	4826.108032	25.350976
160.892297	4829.382182	25.355994
160.577038	4841.087961	25.361011
160.648553	4853.519481	25.366029
161.140107	4861.930612	25.371047
161.115462	4868.730270	25.376064
161.180246	4874.316565	25.381082
161.371590	4897.631760	25.386099
161.988363	4902.084189	25.391117
161.743761	4918.905064	25.396135
161.907876	4921.429949	25.401152
162.275244	4942.855500	25.406170
162.223905	4938.700188	25.411187
162.783618	4936.924389	25.416205
162.229470	4954.607851	25.421223
163.011082	4968.431360	25.426240
163.217826	4954.536116	25.431258
162.976577	4974.481396	25.436275
163.546227	4976.779016	25.441293
163.459890	4979.983662	25.446311
163.550704	4986.740136	25.451328
163.640764	5005.481766	25.456346
164.175520	5013.867303	25.461363
164.254295	5014.347483	25.466381
164.507278	5030.469170	25.471399
164.912359	5042.107119	25.476416
164.731466	5033.474006	25.481434
164.942047	5041.193512	25.486451
165.329319	5049.119090	25.491469
165.661236	5058.300091	25.496487
165.471160	5058.197150	25.501504
165.759549	5056.312072	25.506522
165.740827	5068.154904	25.511539
166.064697	5073.978692	25.516557
166.078284	5086.618247	25.521575
166.032155	5082.515750	25.526592
166.532791	5098.870398	25.531610
166.707211	5109.654178	25.536627
166.796031	5112.279194	25.541645
167.241528	5111.076700	25.546663
167.411260	5127.602837	25.551680
167.537779	5126.232207	25.556698
167.484327	5138.269880	25.561715
167.778226	5134.991932	25.566733
167.723193	5149.978004	25.571751
167.640228	5160.757697	25.576768
168.133887	5159.648709	25.581786
168.078938	5180.452180	25.586803
168.280368	5179.546511	25.591821
168.475610	5200.210045	25.596839
168.653341	5203.521971	25.601856
169.092426	5212.585358	25.606874
169.360657	5217.038470	25.611891
169.421896	5221.381768	25.616909
169.395246	5233.901431	25.621927
169.618661	5243.970609	25.626944
169.927726	5244.572766	25.631962
169.976337	5254.505028	25.636979
170.068607	5253.868871	25.641997
170.154165	5267.510580	25.647015
170.449226	5288.638461	25.652032
170.610935	5284.446744	25.657050
170.838166	5299.714113	25.662067
171.046224	5309.716276	25.667085
171.478667	5313.477824	25.672103
171.486057	5315.850401	25.677120
171.665258	5325.632954	25.682138
171.737798	5335.596257	25.687156
171.840411	5342.922355	25.692173
172.142181	5351.066550	25.697191
172.052974	5354.442159	25.702208
172.700822	5357.744051	25.707226
172.740213	5360.465181	25.712244
172.679180	5360.297956	25.717261
173.169073	5376.155798	25.722279
172.943355	5385.752060	25.727296
173.195460	5383.771590	25.732314
173.686207	5400.914022	25.737332
173.843586	5412.016288	25.742349
174.091550	5403.568751	25.747367
173.975076	5414.019220	25.752384
174.048835	5413.635304	25.757402
174.406483	5433.598323	25.762420
174.437794	5439.224725	25.767437
174.546492	5433.314608	25.772455
174.765528	5440.609994	25.777472
175.070596	5458.201206	25.782490
175.370657	5455.664027	25.787508
175.407776	5455.232153	25.792525
175.569797	5459.831279	25.797543
175.552439	5479.420289	25.802560
175.468706	5474.840609	25.807578
175.829361	5484.945373	25.812596
176.430390	5502.809360	25.817613
176.201397	5516.168792	25.822631
176.130565	5515.075069	25.827648
176.623806	5523.183218	25.832666
176.868586	5534.581292	25.837684
176.869213	5540.433461	25.842701
177.479894	5546.269565	25.847719
177.392480	5557.599424	25.852736
177.561462	5561.749262	25.857754
177.813253	5576.870996	25.862772
177.929424	5583.169202	25.867789
178.390782	5581.298177	25.872807
178.360194	5597.628658	25.877824
178.524161	5601.334212	25.882842
178.752052	5608.672479	25.887860
178.946935	5617.890881	25.892877
179.504638	5619.808503	25.897895
178.994606	5634.464929	25.902912
179.454765	5634.996227	25.907930
179.468235	5645.947430	25.912948
179.760691	5652.862152	25.917965
179.934611	5651.414659	25.922983
180.348578	5663.521952	25.928000
180.720055	5660.339156	25.933018
180.770756	5665.457559	25.938036
180.832512	5678.610859	25.943053
181.056045	5684.624077	25.948071
181.312180	5694.060254	25.953088
181.378008	5694.151053	25.958106
181.546950	5691.975164	25.963124
181.499864	5711.370188	25.968141
182.292340	5710.041034	25.973159
182.408922	5722.365121	25.978176
182.425329	5711.835433	25.983194
182.429790	5731.613867	25.988212
182.773127	5739.609720	25.993229
183.083723	5735.053809	25.998247
182.807459	5746.946649	26.003264
183.037104	5753.353510	26.008282
183.305728	5770.742365	26.013300
183.202236	5770.395508	26.018317
183.522500	5784.774427	26.023335
183.669457	5790.439751	26.028352
183.926627	5792.681961	26.033370
184.281432	5805.114218	26.038388
184.273345	5813.856110	26.043405
184.666757	5816.635828	26.048423
184.671617	5834.119471	26.053440
184.823924	5839.563016	26.058458
184.671078	5844.492198	26.063476
185.008787	5855.415142	26.068493
185.327460	5868.064559	26.073511
185.940473	5887.038182	26.078528
186.096718	5890.378832	26.083546
186.112440	5895.332289	26.088564
186.215395	5894.719699	26.093581
186.414835	5902.109863	26.098599
186.646092	5921.335510	26.103616
186.849776	5928.362014	26.108634
187.219452	5921.754533	26.113652
186.994387	5921.672816	26.118669
187.229674	5945.882147	26.123687
187.237451	5949.621560	26.128704
187.391897	5944.805813	26.133722
187.766257	5964.962524	26.138740
187.721868	5978.533456	26.143757
188.214969	5982.494037	26.148775
188.336167	5999.277896	26.153792
188.318754	5993.532437	26.158810
188.790111	6015.328171	26.163828
188.677970	6024.575641	26.168845
189.211782	6029.006545	26.173863
188.846492	6051.952171	26.178880
189.548569	6038.847057	26.183898
189.819602	6055.285663	26.188916
190.132390	6062.191064	26.193933
190.279010	6067.256766	26.198951
190.424262	6079.122076	26.203968
190.504111	6087.525274	26.208986
190.516185	6095.070952	26.214004
190.943066	6100.424478	26.219021
191.056899	6115.265100	26.224039
191.169086	6122.918312	26.229056
191.641120	6126.484469	26.234074
191.935995	6135.867495	26.239092
191.859123	6149.194236	26.244109
192.323609	6144.339637	26.249127
192.314101	6149.937890	26.254144
192.377326	6161.443539	26.259162
192.632968	6156.716151	26.264180
193.074379	6180.271843	26.269197
193.002943	6184.219349	26.274215
193.435013	6185.834614	26.279232
193.610063	6198.617105	26.284250
193.577757	6208.332049	26.289268
193.967766	6212.182466	26.294285
194.320009	6215.236972	26.299303
194.245178	6230.037614	26.304320
194.549655	6234.122318	26.309338
194.777012	6232.947403	26.314356
195.085174	6245.058930	26.319373
195.088108	6251.643314	26.324391
195.400518	6250.341516	26.329408
195.649954	6257.607244	26.334426
195.597197	6275.295992	26.339444
195.672239	6292.677604	26.344461
196.116981	6284.994507	26.349479
196.125394	6299.223514	26.354496
196.712446	6311.389522	26.359514
196.702457	6316.665920	26.364532
196.619459	6333.901716	26.369549
196.881299	6334.536517	26.374567
197.105387	6347.601892	26.379584
197.217542	6352.549930	26.384602
197.835204	6358.025350	26.389620
197.530174	6362.621659	26.394637
197.878558	6378.325633	26.399655
197.771655	6390.558698	26.404672
197.998692	6398.582418	26.409690
198.610388	6415.568083	26.414708
198.729683	6419.921569	26.419725
199.227527	6428.136736	26.424743
199.281333	6437.532196	26.429760
199.427160	6434.791613	26.434778
199.638301	6439.547488	26.439796
199.639389	6456.666137	26.444813
199.486940	6464.629013	26.449831
199.710881	6466.661825	26.454848
199.975340	6486.015480	26.459866
200.372254	6495.325984	26.464884
200.673920	6512.322127	26.469901
200.919503	6517.899719	26.474919
200.869024	6525.044941	26.479936
200.934280	6536.130667	26.484954
201.549163	6536.925167	26.489972
201.609742	6552.232159	26.494989
202.257881	6558.577307	26.500007
202.074957	6570.396170	26.505024
202.196904	6577.574546	26.510042
202.714629	6583.037183	26.515060
203.060520	6594.552761	26.520077
203.232546	6585.175800	26.525095
203.146162	6599.984853	26.530112
203.133100	6615.896828	26.535130
203.764836	6618.920516	26.540148
203.450325	6626.211056	26.545165
204.254751	6637.942535	26.550183
204.388128	6650.700263	26.555200
204.394502	6648.694782	26.560218
204.499744	6651.225919	26.565236
204.611556	6658.579525	26.570253
205.165087	6665.141470	26.575271
205.741301	6674.667220	26.580288
205.965880	6695.324725	26.585306
205.920216	6693.905025	26.590324
206.097405	6692.384337	26.595341
206.012891	6704.730925	26.600359
206.256562	6698.752035	26.605376
206.003827	6709.918941	26.610394
206.428301	6716.308437	26.615412
206.728620	6740.723356	26.620429
207.451835	6744.272627	26.625447
207.388532	6759.314972	26.630464
207.490267	6770.145777	26.635482
207.782919	6772.265785	26.640500
207.909025	6794.226690	26.645517
208.251593	6802.999693	26.650535
208.175879	6806.512366	26.655552
208.521897	6821.857220	26.660570
208.759844	6818.350928	26.665588
209.034551	6838.189503	26.670605
209.083497	6844.268167	26.675623
209.477302	6854.703148	26.680640
209.130062	6875.257319	26.685658
209.990979	6869.422190	26.690676
209.714574	6886.650736	26.695693
210.453589	6895.403100	26.700711
210.371498	6899.267186	26.705728
210.481749	6921.508507	26.710746
211.005537	6935.417855	26.715764
210.694512	6933.146080	26.720781
211.259568	6948.554798	26.725799
211.046471	6942.656413	26.730816
211.404984	6967.662364	26.735834
211.445641	6973.212021	26.740852
211.531577	6993.623121	26.745869
211.669270	7001.181183	26.750887
211.830239	7026.123265	26.755904
212.221672	7045.804992	26.760922
212.928869	7058.126419	26.765940
212.818081	7066.995386	26.770957
213.028470	7078.630227	26.775975
213.293951	7088.065672	26.780992
213.479066	7111.974991	26.786010
214.024086	7114.444038	26.791028
213.892691	7122.186101	26.796045
213.890412	7134.921091	26.801063
214.356514	7140.414032	26.806080
214.470321	7163.674746	26.811098
214.867174	7160.980207	26.816116
215.266032	7186.567345	26.821133
215.434719	7181.537550	26.826151
215.941213	7197.776371	26.831168
215.825098	7213.231384	26.836186
216.523002	7218.934493	26.841204
216.533202	7219.112881	26.846221
216.702511	7230.804724	26.851239
217.021331	7226.591261	26.856256
217.028462	7242.317539	26.861274
217.274401	7239.741190	26.866292
217.210034	7251.346310	26.871309
217.200412	7264.013082	26.876327
218.214738	7269.190261	26.881344
218.072214	7275.021075	26.886362
218.641275	7280.542225	26.891380
218.648195	7303.747150	26.896397
218.765446	7307.081504	26.901415
219.157081	7310.777217	26.906432
219.034051	7333.857197	26.911450
219.592442	7336.987132	26.916468
219.283197	7357.213926	26.921485
219.289520	7349.964840	26.926503
220.289171	7368.478891	26.931520
219.845903	7378.334201	26.936538
220.615321	7385.592031	26.941556
220.896726	7404.473647	26.946573
220.854596	7409.022971	26.951591
221.010022	7409.570203	26.956608
221.304533	7428.541352	26.961626
221.977758	7430.611659	26.966644
221.915010	7449.452195	26.971661
222.557590	7453.582399	26.976679
222.629919	7458.877879	26.981696
222.258052	7470.688854	26.986714
222.736869	7472.606334	26.991732
222.903065	7496.307589	26.996749
223.196754	7503.244922	27.001767
223.627472	7508.557228	27.006784
223.362772	7531.204920	27.011802
223.818418	7537.769794	27.016820
223.921443	7546.040621	27.021837
224.242833	7556.597770	27.026855
224.312246	7567.513000	27.031872
224.571380	7593.738053	27.036890
224.828333	7589.682514	27.041908
225.359645	7618.990555	27.046925
225.272567	7627.256290	27.051943
225.461193	7634.544661	27.056960
225.689881	7650.028438	27.061978
226.198210	7664.149104	27.066996
226.282221	7681.151806	27.072013
226.617321	7689.317115	27.077031
226.898607	7697.121446	27.082048
226.838255	7704.325489	27.087066
227.082643	7719.418579	27.092084
227.372971	7731.805363	27.097101
227.635735	7746.504157	27.102119
227.830137	7758.069309	27.107136
228.319162	7765.045782	27.112154
228.709981	7774.907194	27.117172
228.778741	7770.877758	27.122189
228.615839	7784.730502	27.127207
229.206355	7784.613347	27.132224
229.120526	7805.775028	27.137242
229.555443	7812.125399	27.142260
229.792923	7809.607114	27.147277
230.019406	7829.296421	27.152295
230.427404	7826.830510	27.157312
230.362037	7841.924572	27.162330
230.661491	7848.687507	27.167348
230.950287	7857.734572	27.172365
230.901481	7866.651099	27.177383
231.773780	7873.107029	27.182400
231.246412	7890.293504	27.187418
231.569631	7889.305606	27.192436
231.529842	7910.340275	27.197453
231.845226	7930.369428	27.202471
232.534686	7937.040107	27.207488
232.353659	7955.915361	27.212506
232.807018	7960.895950	27.217524
233.109597	7978.739377	27.222541
233.228650	7987.468824	27.227559
233.634028	8006.082357	27.232576
233.560723	8020.154944	27.237594
233.777984	8023.012940	27.242612
234.357184	8039.787345	27.247629
234.425201	8062.696430	27.252647
234.833524	8061.954146	27.257664
235.033730	8076.896560	27.262682
235.268314	8084.462084	27.267700
235.415802	8112.028032	27.272717
235.421434	8120.917265	27.277735
236.005131	8130.846707	27.282752
235.847757	8147.960032	27.287770
236.307649	8159.566184	27.292788
237.063950	8165.393094	27.297805
236.846748	8186.035818	27.302823
237.030958	8193.839689	27.307840
237.737410	8198.856708	27.312858
237.946228	8204.708884	27.317876
238.252393	8209.409386	27.322893
238.362406	8216.123025	27.327911
238.800506	8228.768111	27.332928
239.015667	8230.493103	27.337946
239.212745	8237.373144	27.342964
240.021928	8248.877618	27.347981
239.802245	8261.432558	27.352999
240.347032	8258.317048	27.358016
240.397726	8261.557757	27.363034
240.380009	8260.686061	27.368052
240.804069	8274.261525	27.373069
240.883645	8288.815638	27.378087
241.084508	8280.216265	27.383104
241.388498	8302.107078	27.388122
241.324169	8311.695525	27.393140
241.830365	8311.133730	27.398157
241.903915	8329.612988	27.403175
242.059625	8339.893308	27.408192
242.314230	8358.331778	27.413210
242.462482	8360.644935	27.418228
242.701874	8373.583091	27.423245
242.599390	8395.963498	27.428263
243.117031	8403.314604	27.433280
242.936765	8424.068653	27.438298
243.427732	8435.793267	27.443316
243.626204	8445.669201	27.448333
244.133491	8468.387277	27.453351
244.179832	8475.417157	27.458368
244.215646	8488.958513	27.463386
244.828606	8506.072207	27.468404
245.082325	8508.754123	27.473421
245.584124	8524.063519	27.478439
245.359157	8530.062260	27.483456
245.774478	8560.068627	27.488474
246.130914	8560.063685	27.493492
246.309115	8571.991776	27.498509
246.418129	8588.413680	27.503527
246.728112	8588.712734	27.508544
246.751736	8612.734387	27.513562
246.878844	8617.349215	27.518580
247.458641	8626.805973	27.523597
247.542625	8650.088993	27.528615
247.795435	8655.451431	27.533632
248.211035	8679.349003	27.538650
248.425762	8687.950232	27.543668
248.713387	8703.671972	27.548685
248.910764	8712.541109	27.553703
249.338866	8724.272537	27.558720
249.624781	8733.794046	27.563738
249.843695	8747.925876	27.568756
250.320049	8760.682186	27.573773
250.519912	8774.207682	27.578791
250.333446	8788.314257	27.583808
250.878704	8800.785199	27.588826
250.999748	8819.244924	27.593844
251.158854	8832.372699	27.598861
251.469763	8851.368019	27.603879
251.661207	8853.500872	27.608896
251.775009	8869.764425	27.613914
252.301386	8878.942332	27.618932
252.700033	8883.297111	27.623949
253.026912	8905.005121	27.628967
253.713401	8907.720747	27.633984
253.727506	8920.839588	27.639002
253.962766	8933.516739	27.644020
253.995079	8950.642317	27.649037
254.205617	8955.657825	27.654055
254.619916	8968.711238	27.659072
254.769796	8976.984885	27.664090
254.819814	8982.442133	27.669108
255.540239	9001.992650	27.674125
255.166896	9024.542271	27.679143
255.869851	9036.047993	27.684160
255.947052	9048.307830	27.689178
255.731343	9050.952410	27.694196
256.393284	9064.286208	27.699213
256.271764	9082.806060	27.704231
257.001893	9101.354354	27.709248
257.318024	9119.335690	27.714266
257.341423	9138.035093	27.719284
257.524699	9148.390500	27.724301
257.783056	9168.350948	27.729319
258.374923	9174.484771	27.734336
258.983416	9184.796098	27.739354
259.138511	9202.966759	27.744372
259.164115	9203.568987	27.749389
259.147447	9221.769565	27.754407
259.453385	9231.913334	27.759424
259.835149	9252.312450	27.764442
260.371598	9257.005783	27.769460
260.953705	9258.932633	27.774477
260.792464	9277.752481	27.779495
261.369817	9280.848231	27.784512
261.847143	9291.079009	27.789530
261.738540	9304.504530	27.794548
262.175167	9299.672393	27.799565
262.135734	9298.810343	27.804583
262.198180	9310.213895	27.809600
262.621419	9318.899772	27.814618
262.963499	9325.211451	27.819636
263.294996	9337.507662	27.824653
263.340884	9347.164729	27.829671
263.492193	9336.766666	27.834688
263.976512	9355.050395	27.839706
264.208289	9369.799509	27.844724
264.544771	9390.521548	27.849741
264.682741	9396.751369	27.854759
264.852669	9390.824136	27.859776
265.381163	9404.826184	27.864794
265.348028	9422.593829	27.869812
265.789146	9422.698836	27.874829
265.786834	9439.779741	27.879847
265.909915	9448.411379	27.884864
266.446235	9461.951299	27.889882
266.366162	9474.778945	27.894900
266.396412	9489.404825	27.899917
266.841394	9515.796266	27.904935
267.174923	9525.538091	27.909952
267.492717	9543.649027	27.914970
267.557586	9560.264942	27.919988
268.036006	9579.673787	27.925005
268.567057	9594.995305	27.930023
268.343328	9614.721879	27.935040
268.816193	9619.365217	27.940058
269.178044	9647.758851	27.945076
269.481658	9650.818351	27.950093
269.771048	9667.996128	27.955111
269.821065	9691.857207	27.960128
270.429274	9704.309489	27.965146
270.608686	9719.638497	27.970164
270.674178	9736.933285	27.975181
271.349904	9751.250500	27.980199
271.563918	9771.171142	27.985216
272.131564	9769.362093	27.990234
272.216516	9782.817814	27.995252
272.632656	9787.779439	28.000269
272.555376	9801.004691	28.005287
272.934849	9827.539380	28.010304
273.254831	9837.659194	28.015322
273.293293	9852.975527	28.020340
274.071437	9858.193382	28.025357
274.374884	9881.494298	28.030375
274.628311	9887.621063	28.035392
274.953119	9897.721215	28.040410
274.888807	9909.179600	28.045428
275.148784	9928.730167	28.050445
275.278643	9941.999045	28.055463
275.817905	9958.052079	28.060480
276.091684	9964.759801	28.065498
275.890510	9989.197110	28.070516
276.307184	9994.603888	28.075533
276.542215	10020.842453	28.080551
276.683662	10034.466369	28.085568
277.464243	10041.897175	28.090586
277.337200	10060.314669	28.095604
277.590721	10072.891880	28.100621
277.971284	10106.890702	28.105639
278.103670	10118.318593	28.110656
278.558360	10130.911884	28.115674
278.584313	10143.442481	28.120692
279.150885	10164.145349	28.125709
279.657804	10187.579152	28.130727
279.540950	10194.815059	28.135744
280.117827	10207.960859	28.140762
280.227606	10223.749466	28.145780
280.475677	10231.834732	28.150797
280.766764	10239.449175	28.155815
281.055902	10259.519669	28.160832
281.780311	10270.021942	28.165850
281.835125	10282.800729	28.170868
281.908233	10290.007098	28.175885
282.254019	10298.389759	28.180903
282.583013	10314.690538	28.185920
283.296531	10312.119907	28.190938
283.568232	10324.075616	28.195956
283.898929	10327.989815	28.200973
283.971376	10347.001692	28.205991
284.015453	10355.586061	28.211008
284.457945	10363.726365	28.216026
284.268214	10384.512493	28.221044
284.861333	10392.585156	28.226061
285.342698	10411.328207	28.231079
285.388446	10420.850087	28.236096
285.595376	10445.344438	28.241114
285.860040	10460.900746	28.246132
286.266757	10473.643821	28.251149
286.567171	10479.949752	28.256167
286.339785	10509.086859	28.261184
286.527385	10519.407628	28.266202
287.077438	10541.325927	28.271220
287.449942	10558.968356	28.276237
287.785960	10579.849664	28.281255
288.018336	10589.181547	28.286272
288.443621	10606.297988	28.291290
288.574788	10631.088545	28.296308
289.200379	10644.836451	28.301325
289.883575	10656.542022	28.306343
289.750638	10672.826623	28.311360
290.329472	10683.834882	28.316378
290.585881	10700.510403	28.321396
291.060270	10702.432078	28.326413
291.565149	10710.117625	28.331431
291.809905	10724.433226	28.336448
292.182485	10733.386564	28.341466
292.180340	10739.225026	28.346484
292.662598	10735.042165	28.351501
292.782443	10751.464296	28.356519
292.813972	10768.891627	28.361536
293.171961	10782.002447	28.366554
293.437444	10805.139929	28.371572
293.646599	10819.855827	28.376589
293.746064	10827.623484	28.381607
293.957762	10855.224559	28.386624
294.300654	10859.386412	28.391642
294.607367	10882.640711	28.396660
295.108091	10901.864333	28.401677
295.206721	10909.805815	28.406695
295.286981	10934.165813	28.411712
295.755611	10946.558567	28.416730
295.663437	10967.734310	28.421748
295.828376	10984.247507	28.426765
296.820971	11008.920242	28.431783
296.932748	11029.716981	28.436800
297.230366	11041.435462	28.441818
297.937577	11061.858520	28.446836
297.834689	11079.003948	28.451853
298.279237	11100.424660	28.456871
298.092234	11114.444668	28.461888
298.870438	11130.657281	28.466906
298.712104	11151.944573	28.471924
299.188208	11172.937351	28.476941
300.095345	11186.935474	28.481959
299.801734	11198.957652	28.486976
300.256746	11214.863856	28.491994
300.101646	11229.680991	28.497012
300.675956	11236.108729	28.502029
301.080845	11251.075512	28.507047
301.146155	11284.377230	28.512064
301.782625	11304.903137	28.517082
301.815463	11313.726511	28.522100
301.866016	11340.387186	28.527117
302.280517	11351.111986	28.532135
302.372496	11373.219409	28.537152
303.462019	11394.075887	28.542170
303.654367	11418.040160	28.547188
304.067211	11423.741604	28.552205
304.176541	11432.114226	28.557223
304.567461	11463.483671	28.562240
304.967445	11467.526257	28.567258
305.116219	11491.999459	28.572276
305.243340	11502.443859	28.577293
305.626734	11519.987617	28.582311
305.892440	11545.497311	28.587328
306.546652	11552.822098	28.592346
306.965371	11572.460190	28.597364
307.293423	11595.866775	28.602381
307.169110	11604.935782	28.607399
307.572017	11632.025126	28.612416
307.965342	11636.561369	28.617434
308.247600	11653.148461	28.622452
308.595933	11675.791011	28.627469
308.857102	11692.412998	28.632487
308.823177	11716.242368	28.637504
309.336182	11733.229356	28.642522
309.587172	11749.672995	28.647540
310.307874	11771.019908	28.652557
310.724648	11774.883122	28.657575
310.719647	11800.125862	28.662592
311.524986	11809.024974	28.667610
311.559268	11835.928865	28.672628
311.766291	11839.761596	28.677645
312.135626	11859.777118	28.682663
312.192735	11882.531566	28.687680
313.011821	11892.619003	28.692698
313.512648	11913.447725	28.697716
313.565190	11928.864611	28.702733
313.799948	11938.417832	28.707751
313.732946	11951.380920	28.712768
314.297120	11973.886024	28.717786
314.723423	11979.673958	28.722804
315.015936	12001.659330	28.727821
315.619036	12012.857215	28.732839
315.913583	12036.980038	28.737856
315.986297	12046.072263	28.742874
316.458855	12066.330864	28.747892
316.668747	12073.207176	28.752909
316.714431	12096.352054	28.757927
316.749725	12111.607576	28.762944
317.127422	12120.481843	28.767962
317.319732	12145.406980	28.772980
317.660729	12180.615650	28.777997
318.051796	12199.554543	28.783015
318.106128	12216.313398	28.788032
318.540766	12234.973982	28.793050
319.027370	12262.670113	28.798068
319.556230	12275.603811	28.803085
320.254544	12288.315360	28.808103
320.555991	12306.999910	28.813120
321.229895	12308.846487	28.818138
321.509222	12319.997074	28.823156
321.928495	12336.026631	28.828173
322.126257	12328.878424	28.833191
322.151321	12337.851901	28.838208
322.583485	12346.929362	28.843226
323.203528	12361.945639	28.848244
322.749642	12373.731429	28.853261
323.370816	12386.701356	28.858279
323.454142	12396.824670	28.863296
324.086967	12406.180376	28.868314
324.254042	12419.757833	28.873332
324.448475	12434.676228	28.878349
325.100232	12448.323504	28.883367
325.237148	12467.662214	28.888384
325.236734	12477.527045	28.893402
325.772803	12494.264831	28.898420
325.657698	12518.057332	28.903437
326.437710	12535.161366	28.908455
326.215138	12549.446914	28.913472
326.484976	12566.538828	28.918490
327.222771	12592.128019	28.923508
327.227420	12626.742551	28.928525
327.889841	12638.765222	28.933543
328.121599	12662.058661	28.938560
328.388975	12684.936075	28.943578
328.790760	12710.511425	28.948596
328.995783	12726.937814	28.953613
329.498075	12741.499063	28.958631
329.349595	12765.496011	28.963648
329.972258	12788.583491	28.968666
330.582732	12804.814200	28.973684
330.879074	12831.814500	28.978701
331.502385	12849.978971	28.983719
331.826622	12864.628033	28.988736
331.933015	12880.192046	28.993754
332.503693	12898.358442	28.998772
332.488338	12918.848654	29.003789
333.279217	12932.676723	29.008807
333.155710	12954.222728	29.013824
333.594270	12967.676211	29.018842
334.093856	12982.967522	29.023860
334.440605	13015.293778	29.028877
334.773847	13038.477148	29.033895
335.329554	13049.585140	29.038912
335.889137	13055.940014	29.043930
336.254806	13066.910238	29.048948
336.229461	13079.564465	29.053965
336.741651	13085.708837	29.058983
337.098023	13102.437247	29.064000
337.391046	13123.047037	29.069018
338.136695	13140.504335	29.074036
338.094634	13150.214951	29.079053
338.746957	13154.480722	29.084071
338.767739	13181.009695	29.089088
338.721556	13194.043026	29.094106
339.041715	13205.105678	29.099124
339.165615	13237.874372	29.104141
339.710671	13249.126243	29.109159
340.025511	13273.399069	29.114176
340.547561	13293.010242	29.119194
341.227261	13303.306458	29.124212
341.269216	13323.867134	29.129229
341.861078	13341.661190	29.134247
341.982906	13352.044285	29.139264
342.083610	13369.583256	29.144282
342.649583	13379.246697	29.149300
343.051593	13400.370345	29.154317
343.503003	13407.642175	29.159335
343.867258	13429.172784	29.164352
344.115213	13425.676337	29.169370
344.657557	13437.459268	29.174388
344.553196	13458.573394	29.179405
344.883676	13465.276706	29.184423
344.892239	13481.368023	29.189440
345.484960	13494.898936	29.194458
346.221186	13514.789628	29.199476
346.138468	13542.260486	29.204493
346.665849	13567.719551	29.209511
346.640811	13582.325653	29.214528
346.986703	13611.706735	29.219546
347.430677	13623.814574	29.224564
347.529418	13649.564693	29.229581
348.068675	13662.194569	29.234599
348.346631	13689.862123	29.239616
348.738868	13715.576114	29.244634
349.516956	13726.021458	29.249652
349.584933	13753.816534	29.254669
350.109879	13769.401381	29.259687
350.476672	13795.296286	29.264704
350.748399	13810.607954	29.269722
351.246970	13822.243202	29.274740
351.298852	13845.209256	29.279757
351.497653	13868.354574	29.284775
351.997271	13883.248708	29.289792
352.130573	13911.782282	29.294810
352.875154	13931.921593	29.299828
353.077532	13958.186536	29.304845
353.563449	13973.101822	29.309863
353.899892	14003.217632	29.314880
354.463610	14016.393426	29.319898
354.818014	14037.768363	29.324916
355.199874	14054.733656	29.329933
355.618024	14067.812144	29.334951
355.676683	14090.493221	29.339968
356.230324	14116.343686	29.344986
356.577928	14127.573138	29.350004
356.952750	14150.704029	29.355021
357.180643	14165.536475	29.360039
357.496879	14180.869934	29.365056
357.852350	14198.625809	29.370074
358.597186	14214.233635	29.375092
359.317373	14226.289385	29.380109
359.536609	14249.454093	29.385127
359.847435	14253.789073	29.390144
360.162793	14280.302147	29.395162
360.576245	14291.243538	29.400180
360.678130	14311.792798	29.405197
360.931925	14328.970914	29.410215
361.390782	14333.848154	29.415232
361.327717	14358.809654	29.420250
361.833308	14381.712039	29.425268
362.041457	14406.514531	29.430285
362.590199	14436.421127	29.435303
363.117780	14449.378628	29.440320
363.074075	14479.914396	29.445338
363.547503	14501.883989	29.450356
363.519709	14521.998903	29.455373
364.244424	14546.007434	29.460391
364.707271	14569.241981	29.465408
365.086627	14595.322349	29.470426
365.326777	14628.249042	29.475444
365.810434	14638.974429	29.480461
366.230488	14661.988370	29.485479
366.952133	14678.247598	29.490496
367.103012	14709.956674	29.495514
367.009542	14717.399108	29.500532
367.958906	14742.617205	29.505549
368.270783	14764.564881	29.510567
368.537622	14772.156519	29.515584
368.429992	14775.388266	29.520602
369.124842	14797.746917	29.525620
369.551117	14821.388546	29.530637
369.565146	14837.038024	29.535655
370.233459	14854.054180	29.540672
370.442343	14879.330892	29.545690
370.893412	14902.185547	29.550708
370.883755	14922.405437	29.555725
371.166419	14950.358327	29.560743
372.122198	14970.920636	29.565760
372.140015	14996.543064	29.570778
372.466872	15010.590175	29.575796
373.269629	15035.240912	29.580813
373.161652	15058.208053	29.585831
373.792115	15088.886176	29.590848
373.752917	15114.258669	29.595866
374.142850	15135.701948	29.600884
374.828019	15163.980944	29.605901
375.036797	15190.979289	29.610919
376.098076	15204.536385	29.615936
376.017214	15235.976071	29.620954
376.495292	15253.420133	29.625972
376.727563	15280.092812	29.630989
377.235632	15303.902323	29.636007
377.678056	15327.598915	29.641024
378.217787	15351.653054	29.646042
378.415725	15372.302199	29.651060
378.860086	15393.629916	29.656077
379.343070	15424.817905	29.661095
379.553476	15437.869675	29.666112
379.907608	15467.590274	29.671130
380.042121	15503.162564	29.676148
380.842924	15526.222495	29.681165
380.985797	15547.644694	29.686183
381.590899	15573.239630	29.691200
382.006969	15594.448805	29.696218
382.460990	15610.384141	29.701236
382.534718	15640.401322	29.706253
382.910820	15666.215212	29.711271
383.647836	15684.607891	29.716288
383.737516	15718.251549	29.721306
384.154534	15728.583670	29.726324
384.766180	15750.100504	29.731341
385.241553	15774.711578	29.736359
385.876293	15795.849034	29.741376
386.099444	15819.596165	29.746394
386.564008	15825.167725	29.751412
386.978756	15845.404635	29.756429
387.445587	15868.276944	29.761447
387.502117	15878.118883	29.766464
387.710869	15904.341302	29.771482
388.259257	15931.259398	29.776500
388.686331	15948.895218	29.781517
389.127765	15970.347210	29.786535
389.455251	15984.480216	29.791552
390.075675	16006.239163	29.796570
391.020727	16031.112228	29.801588
391.236101	16036.823711	29.806605
391.766401	16059.699002	29.811623
392.027265	16065.823468	29.816640
392.026750	16082.957483	29.821658
392.463930	16100.945603	29.826676
392.785806	16119.674948	29.831693
393.072234	16138.027672	29.836711
393.657739	16147.032557	29.841728
393.813904	16161.369232	29.846746
394.199536	16176.943005	29.851764
394.602668	16186.200542	29.856781
395.157505	16214.172919	29.861799
395.481909	16216.724929	29.866816
395.698240	16242.150728	29.871834
395.949658	16267.391071	29.876852
396.317975	16297.057059	29.881869
396.632195	16310.778627	29.886887
397.261624	16324.849086	29.891904
397.333975	16352.713594	29.896922
397.623086	16379.840080	29.901940
397.715284	16399.044469	29.906957
398.443357	16428.591486	29.911975
398.813664	16450.648865	29.916992
399.101124	16480.226655	29.922010
399.530974	16502.208498	29.927028
400.162301	16533.905812	29.932045
400.448880	16566.749657	29.937063
400.781226	16584.685068	29.942080
401.258425	16606.154313	29.947098
401.712677	16624.718257	29.952116
401.808005	16657.146694	29.957133
402.379591	16690.404351	29.962151
402.850496	16719.546515	29.967168
403.295914	16751.292081	29.972186
403.670832	16784.482607	29.977204
403.972652	16807.830226	29.982221
404.182739	16839.985272	29.987239
404.937625	16862.403326	29.992256
405.318014	16891.935699	29.997274
406.004758	16918.151417	30.002292
406.279045	16940.707552	30.007309
406.226112	16978.127876	30.012327
406.998408	16994.854971	30.017344
407.340073	17025.641175	30.022362
408.196641	17052.563405	30.027380
409.102351	17072.396695	30.032397
409.217663	17090.549559	30.037415
409.665389	17106.793496	30.042432
410.007852	17136.208967	30.047450
410.505044	17153.057991	30.052468
410.867831	17168.370812	30.057485
410.914705	17189.620280	30.062503
411.679325	17214.030248	30.067520
411.866872	17245.690436	30.072538
412.548685	17273.682492	30.077556
412.833088	17289.724597	30.082573
412.971534	17324.547922	30.087591
413.539032	17334.800631	30.092608
413.829734	17363.507522	30.097626
414.046900	17391.373098	30.102644
414.909905	17409.763618	30.107661
415.514736	17453.247937	30.112679
415.630320	17465.728359	30.117696
416.109213	17488.168002	30.122714
416.440204	17520.858109	30.127732
416.982325	17537.574133	30.132749
417.552570	17565.261809	30.137767
417.846482	17576.643788	30.142784
418.109709	17599.091866	30.147802
418.210047	17623.018275	30.152820
419.099090	17648.666537	30.157837
419.338579	17672.356560	30.162855
419.516166	17693.984215	30.167872
420.180451	17718.985307	30.172890
420.425751	17749.680278	30.177908
420.763456	17772.811855	30.182925
420.910619	17796.851216	30.187943
421.645966	17815.454673	30.192960
422.226194	17842.041997	30.197978
422.445244	17865.091082	30.202996
422.904238	17892.897624	30.208013
423.005698	17915.870317	30.213031
423.877159	17935.198135	30.218048
423.989072	17965.522545	30.223066
424.402794	17999.110268	30.228084
425.378103	18014.979085	30.233101
425.150813	18037.617748	30.238119
425.532494	18058.013752	30.243136
426.068057	18089.611669	30.248154
426.606044	18116.793457	30.253172
427.243622	18133.820480	30.258189
427.413578	18168.798354	30.263207
427.762627	18195.599041	30.268224
428.245605	18225.986120	30.273242
428.634758	18253.500821	30.278260
429.456232	18277.378946	30.283277
429.594356	18314.585751	30.288295
429.965237	18329.626588	30.293312
430.390982	18370.023224	30.298330
430.745622	18400.209447	30.303348
431.488857	18409.538302	30.308365
431.886583	18454.172138	30.313383
432.076898	18476.057701	30.318400
432.666754	18512.783928	30.323418
432.745549	18541.920399	30.328436
433.752554	18564.057965	30.333453
433.858953	18590.865387	30.338471
434.297472	18630.350861	30.343488
434.732542	18654.472814	30.348506
435.230970	18697.025714	30.353524
435.875718	18719.895828	30.358541
435.915999	18754.774914	30.363559
436.287609	18784.441057	30.368576
437.521383	18816.354738	30.373594
437.353645	18847.242100	30.378612
438.192694	18869.444070	30.383629
438.890991	18901.055882	30.388647
439.102184	18929.155193	30.393664
439.797002	18957.457228	30.398682
440.217974	18989.889422	30.403700
440.773248	18993.069212	30.408717
441.217818	19018.131462	30.413735
442.210478	19032.014689	30.418752
442.673600	19039.675385	30.423770
442.750164	19059.582948	30.428788
443.315091	19075.156424	30.433805
443.639784	19110.693127	30.438823
444.247395	19117.977573	30.443840
444.522000	19133.589976	30.448858
444.949530	19177.336366	30.453876
445.370070	19192.243789	30.458893
445.501350	19211.909237	30.463911
445.537834	19232.549748	30.468928
445.899695	19266.122470	30.473946
446.334042	19296.240820	30.478964
446.809758	19329.903328	30.483981
447.422351	19359.570740	30.488999
448.100333	19385.209944	30.494016
448.933298	19408.544353	30.499034
449.070833	19427.905793	30.504052
449.848388	19449.454640	30.509069
450.291034	19473.696469	30.514087
450.472845	19485.652986	30.519104
450.586184	19512.302654	30.524122
450.924646	19531.677142	30.529140
451.622336	19549.397327	30.534157
451.488442	19581.512551	30.539175
452.374195	19595.431781	30.544192
452.645069	19627.521974	30.549210
452.965878	19656.944645	30.554228
453.449402	19676.309330	30.559245
453.979837	19713.830489	30.564263
454.308335	19737.085882	30.569280
454.609322	19768.906270	30.574298
455.025511	19797.057053	30.579316
455.878794	19826.062239	30.584333
456.221609	19857.516141	30.589351
456.542847	19890.376025	30.594368
456.932168	19920.672933	30.599386
457.278508	19953.004628	30.604404
458.123065	19988.348278	30.609421
458.444283	20020.399690	30.614439
458.855216	20047.945132	30.619456
459.188073	20072.350111	30.624474
459.522754	20113.876503	30.629492
460.512700	20137.661197	30.634509
460.919993	20174.210491	30.639527
461.011588	20209.678080	30.644544
461.781199	20233.295016	30.649562
461.873047	20273.608588	30.654580
462.668964	20301.789435	30.659597
463.304506	20339.194345	30.664615
463.340610	20370.880045	30.669632
464.214750	20403.427267	30.674650
464.959046	20444.941139	30.679668
465.465999	20465.901432	30.684685
465.816931	20495.503902	30.689703
466.011803	20516.910873	30.694720
466.835548	20540.001669	30.699738
467.289846	20575.710407	30.704756
467.864654	20596.723458	30.709773
468.484713	20634.295614	30.714791
468.815025	20651.619091	30.719808
469.293622	20681.991736	30.724826
469.400128	20714.197755	30.729844
470.370348	20738.997158	30.734861
470.906730	20771.787120	30.739879
471.065773	20792.062699	30.744896
471.762169	20815.091510	30.749914
472.485834	20845.255665	30.754932
472.381086	20870.014084	30.759949
473.160798	20897.718130	30.764967
473.485307	20927.950870	30.769984
473.729354	20944.384530	30.775002
474.111919	20983.125291	30.780020
474.704188	21006.088401	30.785037
475.350741	21035.898395	30.790055
475.909817	21065.298730	30.795072
476.593247	21102.091089	30.800090
476.579334	21127.612840	30.805108
477.552487	21149.189981	30.810125
478.099718	21175.742775	30.815143
478.686864	21199.553561	30.820160
478.867651	21214.897910	30.825178
479.005178	21253.165568	30.830196
479.704135	21278.841906	30.835213
480.149922	21309.365952	30.840231
480.307943	21343.049793	30.845248
480.824861	21374.997134	30.850266
481.272069	21405.040911	30.855284
481.971860	21432.063135	30.860301
482.353590	21454.737309	30.865319
482.452969	21487.508041	30.870336
483.207989	21513.289690	30.875354
483.470232	21553.099163	30.880372
483.782222	21576.927969	30.885389
484.396086	21604.513511	30.890407
484.887395	21637.381439	30.895424
485.515224	21660.598836	30.900442
485.922424	21697.018294	30.905460
486.425443	21729.385394	30.910477
486.726582	21763.363598	30.915495
487.054751	21800.029335	30.920512
487.472647	21835.619661	30.925530
488.244170	21875.761205	30.930548
488.819416	21906.948425	30.935565
489.002843	21929.881485	30.940583
489.658100	21967.867738	30.945600
490.596335	22008.236342	30.950618
491.023829	22038.353659	30.955636
491.377249	22066.934499	30.960653
491.792041	22103.827422	30.965671
492.208470	22142.160803	30.970688
493.122517	22163.261730	30.975706
493.659459	22192.066927	30.980724
494.357935	22222.881619	30.985741
494.835882	22245.693373	30.990759
495.542616	22281.416460	30.995776
495.790852	22303.019265	31.000794
496.334404	22333.396987	31.005812
496.539738	22365.426034	31.010829
497.255455	22393.262210	31.015847
497.634277	22424.386047	31.020864
498.152204	22456.126468	31.025882
498.713839	22489.111242	31.030900
499.794464	22506.060480	31.035917
500.274782	22533.364813	31.040935
500.393830	22558.728703	31.045952
501.142582	22586.054508	31.050970
501.283422	22613.879390	31.055988
501.652517	22638.774779	31.061005
502.207811	22675.255133	31.066023
502.599977	22705.840239	31.071040
503.002662	22734.660809	31.076058
503.324638	22779.916583	31.081076
504.199395	22818.243111	31.086093
504.887330	22843.234455	31.091111
505.142666	22878.719272	31.096128
505.603913	22900.934092	31.101146
506.040306	22939.663999	31.106164
506.450602	22972.982765	31.111181
507.313605	23001.864760	31.116199
507.253465	23039.313599	31.121216
508.075104	23086.255258	31.126234
508.792982	23121.207221	31.131252
509.373167	23154.424018	31.136269
509.635870	23177.971758	31.141287
509.815469	23226.378591	31.146304
510.219726	23251.016518	31.151322
510.887754	23289.312952	31.156340
512.062770	23328.143476	31.161357
512.342481	23359.018814	31.166375
512.440925	23402.048603	31.171392
513.088559	23422.250821	31.176410
513.930009	23446.113199	31.181428
514.019085	23485.820819	31.186445
514.631037	23512.290854	31.191463
515.364616	23562.154111	31.196480
516.165090	23590.244178	31.201498
516.906409	23625.066998	31.206516
516.992515	23646.089875	31.211533
517.772611	23673.184815	31.216551
517.767965	23697.090746	31.221568
518.478595	23721.770029	31.226586
518.718037	23761.454791	31.231604
519.085408	23782.800535	31.236621
519.808948	23815.294696	31.241639
520.208156	23863.997489	31.246656
520.568753	23896.327114	31.251674
521.538944	23932.422911	31.256692
521.777791	23954.243829	31.261709
522.761770	23978.198405	31.266727
523.092760	24017.919979	31.271744
523.511055	24043.668884	31.276762
523.956151	24079.644480	31.281780
524.507963	24117.012717	31.286797
525.098405	24143.733393	31.291815
525.572845	24178.642965	31.296832
526.081266	24221.199947	31.301850
526.684676	24251.982042	31.306868
527.185670	24289.478580	31.311885
527.763501	24317.452673	31.316903
528.522524	24358.511176	31.321920
528.980974	24385.151615	31.326938
529.195865	24414.206075	31.331956
529.887435	24451.818595	31.336973
530.720010	24483.942991	31.341991
530.814591	24530.868540	31.347008
531.382460	24566.149727	31.352026
531.879717	24604.936594	31.357044
532.158732	24646.045137	31.362061
532.815022	24677.559028	31.367079
533.064772	24717.869708	31.372096
533.929346	24759.493992	31.377114
534.819748	24808.798802	31.382132
535.457622	24838.609560	31.387149
536.012306	24870.303879	31.392167
536.523514	24898.775758	31.397184
537.452546	24931.037526	31.402202
538.197457	24960.560065	31.407220
538.347154	24995.148768	31.412237
539.038460	25025.216906	31.417255
539.266240	25065.361079	31.422272
539.557487	25091.883140	31.427290
540.268840	25134.132414	31.432308
540.367360	25166.763996	31.437325
541.373987	25214.162161	31.442343
542.042105	25257.214693	31.447360
542.397269	25283.575387	31.452378
543.304589	25311.979869	31.457396
543.690428	25347.037986	31.462413
544.497293	25374.371220	31.467431
544.951058	25401.677304	31.472448
545.813911	25432.288117	31.477466
546.074487	25454.195764	31.482484
546.335671	25491.169438	31.487501
547.132982	25517.069788	31.492519
547.191357	25556.097452	31.497536
548.133624	25589.198741	31.502554
548.816328	25629.475452	31.507572
549.417831	25667.218034	31.512589
549.865545	25695.726209	31.517607
550.167836	25735.752687	31.522624
550.366697	25763.718282	31.527642
551.236085	25793.089956	31.532660
551.620537	25835.669669	31.537677
552.767002	25864.423213	31.542695
552.927187	25898.626332	31.547712
553.219950	25928.587235	31.552730
553.997838	25958.687534	31.557748
554.424084	25991.168319	31.562765
555.346141	26012.063542	31.567783
555.573747	26053.669599	31.572800
555.916024	26076.936614	31.577818
556.469868	26107.861998	31.582836
556.587762	26139.683199	31.587853
557.426869	26184.044595	31.592871
557.762679	26223.681311	31.597888
558.252490	26263.578528	31.602906
559.094775	26305.241091	31.607924
559.415808	26353.228991	31.612941
560.379674	26379.458443	31.617959
561.053887	26412.173062	31.622976
561.617508	26460.635369	31.627994
562.043285	26483.163057	31.633012
562.436714	26519.403873	31.638029
563.372684	26552.185411	31.643047
563.698037	26598.618500	31.648064
564.191304	26631.633405	31.653082
564.865681	26671.546937	31.658100
565.276544	26720.273809	31.663117
566.134964	26758.010041	31.668135
566.648656	26800.103986	31.673152
567.220596	26836.462943	31.678170
568.246455	26878.894447	31.683188
568.415468	26919.892039	31.688205
569.228217	26951.309301	31.693223
569.909417	26986.608698	31.698240
570.842336	27011.213195	31.703258
571.476895	27040.187158	31.708276
571.840457	27079.644269	31.713293
572.476027	27105.533925	31.718311
572.981265	27147.004210	31.723328
573.567462	27169.027356	31.728346
574.125585	27206.924939	31.733364
574.196815	27244.474936	31.738381
575.303225	27278.204435	31.743399
575.832708	27312.763272	31.748416
576.214197	27352.161241	31.753434
576.587114	27385.139230	31.758452
576.935032	27422.911934	31.763469
577.472111	27467.354770	31.768487
578.079422	27504.809153	31.773504
578.591049	27544.673900	31.778522
579.351538	27591.787324	31.783540
579.634945	27630.689156	31.788557
580.665838	27670.473315	31.793575
581.347569	27715.722142	31.798592
581.741494	27756.623209	31.803610
582.495354	27795.812381	31.808628
583.218833	27829.994278	31.813645
583.912890	27858.536683	31.818663
584.601199	27899.866241	31.823680
585.017393	27930.310208	31.828698
585.738134	27961.844490	31.833716
585.842887	27994.492309	31.838733
586.746747	28033.664911	31.843751
587.834908	28066.545302	31.848768
588.429649	28110.139945	31.853786
589.059638	28132.947383	31.858804
589.323652	28164.173851	31.863821
589.715651	28195.677507	31.868839
590.490398	28233.650734	31.873856
591.256454	28273.799652	31.878874
591.982715	28294.986868	31.883892
592.226524	28326.779259	31.888909
592.763919	28355.466841	31.893927
593.585653	28379.837491	31.898944
593.760711	28410.939132	31.903962
594.508512	28435.131740	31.908980
594.448412	28471.819563	31.913997
594.977282	28503.858602	31.919015
595.798696	28548.815753	31.924032
596.506573	28570.593936	31.929050
596.904130	28609.012142	31.934068
597.499674	28644.416247	31.939085
598.057108	28684.908165	31.944103
598.545809	28730.454768	31.949120
598.964516	28778.863003	31.954138
599.507496	28808.846098	31.959156
600.065468	28867.131093	31.964173
600.794482	28911.376544	31.969191
601.120251	28953.257696	31.974208
601.728769	29012.666652	31.979226
602.613119	29048.589048	31.984244
603.359755	29097.680199	31.989261
604.416824	29140.655163	31.994279
604.949682	29168.630344	31.999296
605.355122	29218.103582	32.004314
606.070161	29251.985781	32.009332
606.851043	29293.038278	32.014349
607.376971	29332.531367	32.019367
608.014516	29386.854913	32.024384
608.405855	29424.472866	32.029402
609.266275	29460.962272	32.034420
610.002629	29505.814674	32.039437
610.768594	29539.664138	32.044455
611.150335	29572.707502	32.049472
611.845503	29614.235416	32.054490
612.597080	29649.876133	32.059508
613.336899	29691.681696	32.064525
613.953056	29726.250098	32.069543
614.687569	29760.465119	32.074560
615.027450	29800.316765	32.079578
615.741289	29834.958637	32.084596
616.306130	29875.748847	32.089613
616.920431	29910.191427	32.094631
617.668270	29943.064617	32.099648
618.170229	29985.343961	32.104666
618.706469	30020.133894	32.109684
619.417558	30068.019256	32.114701
620.059975	30111.180910	32.119719
620.954492	30143.228807	32.124736
620.771479	30185.084219	32.129754
621.510747	30235.772168	32.134772
621.957443	30273.951963	32.139789
622.283834	30321.309935	32.144807
623.334343	30353.618329	32.149824
623.810544	30416.585490	32.154842
624.620037	30466.567744	32.159860
624.906243	30515.873033	32.164877
625.536603	30553.828797	32.169895
626.113758	30601.552935	32.174912
626.749288	30656.177249	32.179930
627.198333	30704.901368	32.184948
627.975107	30761.634249	32.189965
628.335000	30803.298935	32.194983
629.301498	30849.186745	32.200000
630.248429	30908.504253	32.205018
631.047724	30957.509475	32.210036
631.735755	31004.673647	32.215053
632.409981	31039.165680	32.220071
633.216391	31071.816629	32.225088
633.989413	31104.599256	32.230106
634.631676	31132.313546	32.235124
635.269316	31175.705744	32.240141
635.443669	31213.657853	32.245159
636.350575	31239.934050	32.250176
636.489000	31283.309367	32.255194
637.273158	31312.278745	32.260212
637.847121	31364.316391	32.265229
638.774795	31397.941453	32.270247
639.165727	31439.292836	32.275264
639.381651	31487.979232	32.280282
640.092028	31524.805415	32.285300
640.753262	31566.051757	32.290317
641.107205	31611.739506	32.295335
641.793183	31668.014892	32.300352
642.161926	31717.967642	32.305370
643.104895	31775.910146	32.310388
643.837215	31826.957094	32.315405
644.453050	31863.659520	32.320423
645.299402	31918.115272	32.325440
645.457768	31960.629154	32.330458
646.144027	32017.019232	32.335476
647.199238	32067.624562	32.340493
647.946765	32122.153129	32.345511
648.830753	32163.094148	32.350528
649.406654	32211.972751	32.355546
650.218705	32257.919338	32.360564
650.776327	32305.429183	32.365581
651.167788	32355.632800	32.370599
651.758547	32401.601511	32.375616
652.495003	32458.161982	32.380634
653.327870	32496.582887	32.385652
654.094624	32557.715922	32.390669
654.766165	32603.527101	32.395687
655.777524	32642.913023	32.400704
656.160449	32676.561744	32.405722
657.161447	32723.396620	32.410740
657.874202	32779.607628	32.415757
658.458053	32821.216215	32.420775
659.119672	32856.895437	32.425792
659.400837	32904.607733	32.430810
659.819265	32959.215012	32.435828
660.644349	32998.048983	32.440845
661.426684	33052.087773	32.445863
662.291799	33086.749477	32.450880
662.638479	33147.475484	32.455898
663.305025	33182.547580	32.460916
664.227048	33239.087605	32.465933
664.918894	33289.803050	32.470951
665.682756	33334.096807	32.475968
666.105941	33387.149229	32.480986
666.530070	33437.457837	32.486004
667.210291	33480.146461	32.491021
667.707786	33531.626114	32.496039
668.650620	33581.525570	32.501056
669.368287	33639.362922	32.506074
669.943559	33679.981972	32.511092
670.824842	33724.612319	32.516109
671.994378	33759.265684	32.521127
672.839628	33804.818534	32.526144
673.146348	33850.550150	32.531162
674.081205	33891.594124	32.536180
674.706076	33921.786844	32.541197
675.511215	33970.418919	32.546215
675.959468	34004.249275	32.551232
676.771838	34044.433818	32.556250
677.239405	34092.157736	32.561268
677.869889	34132.579399	32.566285
678.320223	34178.978508	32.571303
679.477277	34207.179446	32.576320
680.003048	34242.686187	32.581338
680.659188	34280.474037	32.586356
681.462478	34306.062138	32.591373
681.601390	34352.611268	32.596391
682.388440	34390.536997	32.601408
682.776403	34427.083410	32.606426
683.430022	34480.007887	32.611444
684.077375	34515.673191	32.616461
684.641234	34568.921664	32.621479
685.720388	34602.300712	32.626496
686.215590	34655.680220	32.631514
686.640876	34696.052717	32.636532
687.661925	34741.270430	32.641549
687.925865	34789.653558	32.646567
688.743888	34836.856743	32.651584
689.438407	34895.700119	32.656602
690.199676	34944.309665	32.661620
691.078915	34999.223548	32.666637
691.549962	35043.705593	32.671655
692.162887	35090.403852	32.676672
692.913854	35143.561423	32.681690
693.755662	35197.261380	32.686708
694.671452	35247.061518	32.691725
694.867962	35301.703108	32.696743
695.683993	35351.664444	32.701760
696.847624	35401.224038	32.706778
697.618683	35450.680469	32.711796
698.108222	35504.088294	32.716813
698.673132	35562.182328	32.721831
699.327328	35604.847703	32.726848
700.069509	35664.703768	32.731866
700.786976	35716.540209	32.736884
701.565175	35758.396239	32.741901
702.267582	35822.141150	32.746919
702.792230	35876.745787	32.751936
703.379298	35929.355467	32.756954
704.255357	35988.609902	32.761972
704.929434	36042.363406	32.766989
705.256350	36102.696339	32.772007
706.405136	36153.764862	32.777024
707.143650	36210.720812	32.782042
707.903607	36261.458100	32.787060
708.800085	36324.510397	32.792077
709.514710	36383.386393	32.797095
710.183482	36428.276853	32.802112
711.099983	36478.320050	32.807130
711.206158	36542.798565	32.812148
711.937483	36593.376703	32.817165
712.463847	36644.176561	32.822183
713.424555	36701.232020	32.827200
714.611564	36760.642542	32.832218
714.812561	36816.861785	32.837236
716.143798	36857.546313	32.842253
716.988090	36922.568680	32.847271
717.900397	36963.913004	32.852288
718.572827	37000.906459	32.857306
719.069490	37059.476803	32.862324
719.914525	37100.528351	32.867341
720.504613	37155.783698	32.872359
721.576545	37194.586975	32.877376
721.791215	37248.775466	32.882394
722.621542	37303.829393	32.887412
723.769394	37345.403368	32.892429
724.587869	37392.662759	32.897447
725.653939	37438.732867	32.902464
725.925070	37474.777884	32.907482
726.324882	37526.832591	32.912500
727.076999	37558.458740	32.917517
727.666934	37594.340509	32.922535
728.079676	37644.129727	32.927552
729.186059	37685.729791	32.932570
729.739914	37727.959759	32.937588
730.448973	37777.760071	32.942605
731.192754	37824.804401	32.947623
731.831706	37860.881337	32.952640
732.562831	37910.735434	32.957658
732.771108	37966.159808	32.962676
733.775519	38015.996901	32.967693
734.422737	38062.361202	32.972711
735.210602	38123.759996	32.977728
735.622210	38180.139739	32.982746
736.288543	38236.530565	32.987764
737.151814	38300.232544	32.992781
737.917604	38361.420452	32.997799
738.642244	38420.433297	33.002816
739.608233	38469.341532	33.007834
740.285802	38536.525815	33.012852
741.153570	38585.481222	33.017869
741.836241	38645.260055	33.022887
742.674312	38696.585390	33.027904
743.646067	38751.159391	33.032922
743.886467	38810.982237	33.037940
744.891220	38868.403395	33.042957
745.232997	38940.333421	33.047975
745.985624	39003.257912	33.052992
746.686710	39056.692275	33.058010
747.168528	39114.657130	33.063028
748.222278	39177.048320	33.068045
749.085414	39240.917522	33.073063
750.217337	39309.740924	33.078080
750.975250	39374.354146	33.083098
751.260297	39436.897368	33.088116
752.596906	39505.095083	33.093133
753.650292	39555.838765	33.098151
754.141789	39612.924422	33.103168
755.172451	39668.389575	33.108186
755.456504	39728.859534	33.113204
756.462804	39777.094119	33.118221
757.086076	39845.562052	33.123239
757.957223	39901.640767	33.128256
759.089140	39950.855383	33.133274
760.195074	39999.296295	33.138292
761.054325	40060.752731	33.143309
761.731874	40111.195749	33.148327
762.166744	40152.696425	33.153344
762.724132	40206.503824	33.158362
763.543113	40264.887258	33.163380
764.357542	40301.718833	33.168397
765.297473	40373.630072	33.173415
765.874227	40423.678435	33.178432
767.056387	40468.364612	33.183450
767.678020	40521.954093	33.188468
768.878009	40567.889893	33.193485
769.560686	40622.715994	33.198503
770.160506	40660.972921	33.203520
771.044063	40696.858417	33.208538
771.949562	40757.708821	33.213556
772.367547	40793.995814	33.218573
773.285062	40849.057873	33.223591
773.867915	40896.608272	33.228608
774.343709	40952.612112	33.233626
775.116748	41008.620418	33.238644
775.733913	41064.982000	33.243661
776.584261	41121.655270	33.248679
777.346424	41170.481179	33.253696
778.534209	41222.719372	33.258714
779.033234	41270.675750	33.263732
779.712630	41305.974238	33.268749
780.478812	41349.790963	33.273767
781.330502	41400.608303	33.278784
781.671134	41452.238957	33.283802
782.471189	41507.036360	33.288820
783.149885	41555.983641	33.293837
784.145705	41613.894123	33.298855
784.514847	41668.354240	33.303872
785.747107	41711.732314	33.308890
786.202220	41777.203032	33.313908
787.172159	41840.152508	33.318925
788.121150	41897.609336	33.323943
788.958245	41954.950915	33.328960
789.662439	42002.067406	33.333978
790.393645	42076.451737	33.338996
790.932524	42118.547129	33.344013
791.851961	42178.311477	33.349031
792.561662	42239.101616	33.354048
793.710475	42286.041984	33.359066
794.466205	42347.445082	33.364084
795.525621	42388.745266	33.369101
796.508941	42451.839885	33.374119
797.041518	42503.999716	33.379136
797.573269	42569.827705	33.384154
798.390908	42624.770637	33.389172
799.298243	42688.864437	33.394189
799.948371	42753.890269	33.399207
800.465116	42820.790246	33.404224
801.497510	42875.662424	33.409242
802.198818	42946.449163	33.414260
803.116559	43006.500647	33.419277
803.914107	43072.073713	33.424295
804.759739	43137.152466	33.429312
806.110663	43201.507605	33.434330
806.571481	43262.965489	33.439348
807.222732	43318.505302	33.444365
808.265203	43388.905126	33.449383
809.206748	43452.888298	33.454400
809.889009	43506.488288	33.459418
810.401451	43564.460181	33.464436
811.541769	43633.757638	33.469453
812.506446	43692.696789	33.474471
813.317012	43760.414090	33.479488
814.169036	43821.376192	33.484506
814.921917	43877.919942	33.489524
815.832196	43937.146520	33.494541
816.703618	43989.579698	33.499559
817.328805	44054.632215	33.504576
818.630414	44098.959318	33.509594
819.293158	44162.058129	33.514612
820.275091	44225.392070	33.519629
820.901803	44283.341731	33.524647
821.724062	44341.691224	33.529664
822.680815	44403.068744	33.534682
823.277233	44460.485930	33.539700
824.052245	44518.748362	33.544717
824.645068	44581.220386	33.549735
825.301207	44649.634931	33.554752
826.341358	44695.060269	33.559770
826.506169	44772.862687	33.564788
827.603170	44833.315025	33.569805
828.663378	44906.228112	33.574823
829.096793	44970.693264	33.579840
830.196303	45025.085912	33.584858
830.720010	45101.404043	33.589876
831.875830	45163.758433	33.594893
833.311330	45225.829089	33.599911
833.522836	45283.409521	33.604928
834.313294	45334.036706	33.609946
835.025741	45400.388971	33.614964
836.178821	45457.336208	33.619981
836.573605	45510.498708	33.624999
837.223708	45574.767406	33.630016
838.325221	45636.834265	33.635034
839.092449	45715.083870	33.640052
839.999129	45763.296494	33.645069
840.956608	45824.266643	33.650087
841.279044	45899.859741	33.655104
842.445609	45952.871522	33.660122
842.849723	46033.740701	33.665140
844.063685	46090.237267	33.670157
845.484912	46156.152497	33.675175
846.368503	46225.074153	33.680192
847.716439	46273.693627	33.685210
848.183704	46336.417831	33.690228
849.209550	46387.320725	33.695245
850.254008	46443.920480	33.700263
850.987315	46501.074888	33.705280
852.261243	46559.176413	33.710298
852.996980	46612.345383	33.715316
853.682219	46666.104328	33.720333
854.354853	46723.192833	33.725351
855.421653	46788.804512	33.730368
856.541034	46832.513840	33.735386
856.818291	46898.969910	33.740404
858.177548	46946.981783	33.745421
859.206200	47008.260370	33.750439
859.548486	47079.837291	33.755456
860.565390	47134.159355	33.760474
860.877813	47192.519733	33.765492
862.213569	47257.123013	33.770509
862.750637	47319.351974	33.775527
863.189650	47391.882727	33.780544
863.999697	47448.856786	33.785562
865.008481	47520.325024	33.790580
865.997265	47598.331598	33.795597
866.591901	47669.466224	33.800615
867.540821	47743.108063	33.805632
868.596556	47821.990664	33.810650
869.276780	47888.469154	33.815668
870.263531	47952.565708	33.820685
871.186715	48024.074167	33.825703
872.165200	48099.572509	33.830720
873.127852	48169.841642	33.835738
874.109319	48232.959221	33.840756
874.553177	48308.301076	33.845773
875.521360	48379.120394	33.850791
876.325502	48450.585463	33.855808
877.397111	48514.986719	33.860826
878.371690	48585.059159	33.865844
879.086571	48654.824280	33.870861
879.874111	48723.477486	33.875879
881.081038	48807.825091	33.880896
882.246219	48867.531120	33.885914
883.033393	48939.088936	33.890932
883.690134	49001.999806	33.895949
885.362138	49053.643235	33.900967
885.910996	49123.758294	33.905984
887.308979	49179.715158	33.911002
888.308981	49243.250214	33.916020
888.628418	49309.997799	33.921037
889.925714	49357.069097	33.926055
890.551044	49432.209268	33.931072
891.435170	49467.014294	33.936090
892.265981	49521.763301	33.941108
893.218528	49581.118366	33.946125
894.354290	49624.703997	33.951143
894.545379	49676.060565	33.956160
895.493345	49725.717724	33.961178
896.370241	49789.621438	33.966196
896.930624	49853.922576	33.971213
897.930670	49917.902381	33.976231
898.567031	49982.622281	33.981248
899.415517	50038.995784	33.986266
900.332658	50104.425223	33.991284
900.852646	50171.852715	33.996301
901.720368	50253.727678	34.001319
902.567625	50328.469276	34.006336
903.692605	50392.443610	34.011354
904.811182	50469.667908	34.016372
905.022424	50538.258091	34.021389
906.577736	50606.904992	34.026407
907.573056	50680.011283	34.031424
908.490471	50744.974298	34.036442
909.735345	50822.477494	34.041460
910.649038	50891.471879	34.046477
911.749282	50956.084346	34.051495
912.581320	51030.020714	34.056512
913.450143	51091.347813	34.061530
914.294931	51168.129878	34.066548
915.224023	51241.140695	34.071565
916.189735	51304.876612	34.076583
917.060123	51377.700853	34.081600
917.589873	51439.866241	34.086618
918.743202	51516.860854	34.091636
919.572641	51596.917952	34.096653
920.532320	51662.035152	34.101671
921.714202	51742.487133	34.106688
922.777731	51813.694510	34.111706
923.605542	51884.166854	34.116724
924.292665	51951.421667	34.121741
925.471816	52025.364130	34.126759
926.410796	52105.323674	34.131776
926.907219	52184.403260	34.136794
928.262893	52252.611569	34.141812
928.822921	52328.119352	34.146829
929.564272	52401.574338	34.151847
931.003634	52484.456557	34.156864
931.800170	52565.180182	34.161882
932.766218	52627.559249	34.166900
933.847118	52706.650868	34.171917
935.037817	52776.506270	34.176935
935.985033	52851.683390	34.181952
936.872828	52920.789088	34.186970
938.223082	52981.521044	34.191988
939.370859	53048.840204	34.197005
940.579531	53114.587125	34.202023
941.077518	53183.747952	34.207040
941.906124	53242.062321	34.212058
943.297413	53307.085302	34.217076
944.179021	53377.901821	34.222093
945.163080	53444.741382	34.227111
945.820039	53502.937580	34.232128
946.884789	53560.387036	34.237146
947.470706	53634.034619	34.242164
948.142335	53705.410029	34.247181
949.638590	53772.246730	34.252199
950.008199	53836.329160	34.257216
951.381251	53907.893414	34.262234
951.990928	53973.976454	34.267252
952.979091	54053.726192	34.272269
953.900146	54112.718090	34.277287
954.888532	54180.021018	34.282304
955.719537	54241.387613	34.287322
956.396630	54295.026446	34.292340
957.079005	54364.294939	34.297357
958.306684	54436.478274	34.302375
958.780680	54516.366569	34.307392
959.814273	54589.479178	34.312410
960.810701	54661.800451	34.317428
961.369921	54731.399274	34.322445
962.563661	54807.544143	34.327463
963.600248	54881.150790	34.332480
964.491115	54964.127165	34.337498
965.755143	55036.699031	34.342516
966.394459	55117.019259	34.347533
967.258640	55193.286283	34.352551
968.310607	55271.821503	34.357568
969.191320	55352.826385	34.362586
970.459870	55438.314941	34.367604
971.308504	55516.515580	34.372621
972.264620	55601.743269	34.377639
973.438661	55680.501322	34.382656
974.679164	55768.900190	34.387674
975.727756	55847.830210	34.392692
976.390037	55923.080482	34.397709
977.259188	56005.817073	34.402727
978.432058	56086.120814	34.407744
979.391866	56173.913042	34.412762
980.303924	56249.441894	34.417780
981.559267	56332.727052	34.422797
982.487747	56405.918588	34.427815
983.710112	56497.221498	34.432832
984.445401	56568.215920	34.437850
985.990139	56645.153767	34.442868
986.792915	56737.921554	34.447885
987.969118	56818.119656	34.452903
988.912413	56883.646253	34.457920
990.054445	56963.508411	34.462938
991.244103	57033.155075	34.467956
992.373457	57113.494366	34.472973
993.409552	57176.823881	34.477991
994.271541	57239.262982	34.483008
995.118469	57314.223088	34.488026
996.274230	57388.173364	34.493044
997.034540	57472.780018	34.498061
998.439763	57551.546241	34.503079
999.235082	57627.990003	34.508096
1000.263956	57707.555809	34.513114
1001.451209	57773.122813	34.518132
1002.100119	57856.836786	34.523149
1002.929659	57927.997781	34.528167
1003.655312	58016.269922	34.533184
1004.806114	58092.083881	34.538202
1005.866066	58172.684356	34.543220
1006.519871	58252.652120	34.548237
1007.728723	58343.812272	34.553255
1008.702162	58422.686538	34.558272
1009.974866	58502.552464	34.563290
1011.111135	58582.174065	34.568308
1011.790740	58662.544240	34.573325
1013.178610	58741.880364	34.578343
1014.368283	58828.969303	34.583360
1014.844157	58904.542766	34.588378
1015.888876	58985.230607	34.593396
1016.835728	59066.256748	34.598413
1018.087326	59144.210294	34.603431
1019.192363	59220.256448	34.608448
1019.748748	59314.351051	34.613466
1020.852129	59382.562186	34.618484
1022.016011	59460.346851	34.623501
1022.759473	59533.766592	34.628519
1024.014487	59602.821878	34.633536
1025.072122	59683.978415	34.638554
1026.138975	59736.834569	34.643572
1026.835400	59824.048168	34.648589
1027.989953	59893.936429	34.653607
1029.010724	59972.415941	34.658624
1029.863557	60052.206753	34.663642
1030.961752	60131.339333	34.668660
1031.931417	60208.124896	34.673677
1032.931855	60295.102971	34.678695
1033.799583	60370.911160	34.683712
1035.282758	60457.536166	34.688730
1036.612358	60526.196352	34.693748
1037.282733	60607.175717	34.698765
1038.028230	60695.549463	34.703783
1039.363265	60770.558230	34.708800
1040.243685	60863.563963	34.713818
1041.291082	60933.598478	34.718836
1042.052318	61033.478594	34.723853
1043.423877	61120.971524	34.728871
1044.506201	61204.946064	34.733888
1045.301258	61302.068510	34.738906
1046.624415	61376.884757	34.743924
1047.501928	61475.773765	34.748941
1048.577238	61546.761509	34.753959
1050.150858	61646.454364	34.758976
1050.737194	61731.957480	34.763994
1051.942592	61818.573567	34.769012
1053.138422	61907.590542	34.774029
1054.186459	61991.092020	34.779047
1055.242478	62063.369264	34.784064
1056.145745	62166.675449	34.789082
1057.339082	62247.844682	34.794100
1058.493600	62336.648081	34.799117
1059.652824	62430.660818	34.804135
1061.119113	62514.953540	34.809152
1061.844970	62589.106819	34.814170
1063.513239	62674.128273	34.819188
1064.416955	62760.724993	34.824205
1065.210323	62841.211460	34.829223
1066.638220	62919.896562	34.834240
1067.519680	63012.372164	34.839258
1068.725373	63081.432263	34.844276
1069.836550	63167.706915	34.849293
1070.604482	63248.420226	34.854311
1071.952542	63332.639179	34.859328
1072.554778	63425.147120	34.864346
1074.055058	63503.949416	34.869364
1075.094414	63580.994198	34.874381
1076.259300	63673.339515	34.879399
1077.487942	63748.595469	34.884416
1078.285544	63838.339745	34.889434
1079.074537	63922.109618	34.894452
1080.016802	64002.215822	34.899469
1081.067980	64097.353210	34.904487
1081.858373	64186.511110	34.909504
1083.001675	64279.577392	34.914522
1084.080505	64364.126619	34.919540
1085.062653	64458.605073	34.924557
1086.305226	64550.365445	34.929575
1087.462608	64639.816026	34.934592
1088.592842	64738.893939	34.939610
1090.121080	64813.163179	34.944628
1091.503937	64908.840787	34.949645
1092.519247	64997.650022	34.954663
1093.521021	65065.854707	34.959680
1094.411272	65153.037933	34.964698
1095.712436	65229.996395	34.969716
1096.377856	65304.135493	34.974733
1097.678799	65378.125240	34.979751
1098.672940	65444.464511	34.984768
1099.177108	65533.070306	34.989786
1100.744609	65612.767783	34.994804
1101.664301	65684.532282	34.999821
1102.378229	65776.847915	35.004839
1103.874142	65859.703844	35.009856
1104.770417	65939.665112	35.014874
1105.795348	66030.002279	35.019892
1106.846969	66128.414137	35.024909
1107.970844	66212.088868	35.029927
1109.351286	66291.804943	35.034944
1110.342207	66384.902732	35.039962
1111.511688	66471.078373	35.044980
1112.826212	66568.817897	35.049997
1113.466585	66659.660356	35.055015
1114.491180	66744.320981	35.060032
1115.880535	66843.689718	35.065050
1117.268401	66934.885326	35.070068
1118.634793	67020.063486	35.075085
1119.512191	67116.435942	35.080103
1120.861360	67197.850210	35.085120
1121.805140	67300.272176	35.090138
1123.061076	67394.155494	35.095156
1124.214415	67486.991441	35.100173
1125.361163	67570.679748	35.105191
1126.230035	67667.410176	35.110208
1127.545656	67767.889347	35.115226
1128.865704	67858.244058	35.120244
1130.197676	67946.254546	35.125261
1131.115053	68039.268523	35.130279
1132.435936	68131.441239	35.135296
1133.388076	68220.271588	35.140314
1134.699943	68305.582826	35.145332
1135.999465	68396.265546	35.150349
1136.863711	68484.300033	35.155367
1138.222671	68579.469665	35.160384
1139.559235	68676.479347	35.165402
1140.561451	68760.630931	35.170420
1141.780087	68855.880415	35.175437
1142.286201	68948.575459	35.180455
1143.722767	69039.023832	35.185472
1144.770108	69136.973059	35.190490
1145.938627	69226.792635	35.195508
1146.895529	69316.981055	35.200525
1148.308298	69418.135407	35.205543
1150.339544	69498.583337	35.210560
1151.871942	69584.010122	35.215578
1152.858689	69663.133130	35.220596
1154.351371	69745.945183	35.225613
1155.091988	69828.273020	35.230631
1156.656758	69902.323470	35.235648
1157.505623	69988.218913	35.240666
1158.617352	70064.132323	35.245684
1159.715467	70148.805397	35.250701
1160.302440	70235.464285	35.255719
1161.919719	70314.180860	35.260736
1162.935090	70408.796494	35.265754
1163.923396	70490.074725	35.270772
1164.970357	70571.818998	35.275789
1166.041349	70671.271080	35.280807
1166.869216	70754.981366	35.285824
1168.299358	70848.337237	35.290842
1169.260145	70949.466595	35.295860
1170.226838	71033.637422	35.300877
1171.131937	71123.669206	35.305895
1172.583103	71203.839109	35.310912
1173.864759	71287.797088	35.315930
1174.725626	71377.355369	35.320948
1175.912010	71459.327683	35.325965
1176.743366	71547.751300	35.330983
1178.027685	71639.764885	35.336000
1179.110942	71735.039667	35.341018
1179.787575	71829.909481	35.346036
1181.165764	71914.753662	35.351053
1182.261925	72021.223424	35.356071
1183.699280	72123.169692	35.361088
1185.046619	72224.636423	35.366106
1185.833385	72319.364207	35.371124
1187.393803	72418.531431	35.376141
1188.466261	72532.504832	35.381159
1189.489907	72627.196850	35.386176
1190.619876	72724.608403	35.391194
1191.732761	72832.560700	35.396212
1193.591186	72939.333483	35.401229
1194.685111	73038.385664	35.406247
1195.914638	73136.201204	35.411264
1196.925612	73249.870625	35.416282
1198.308009	73361.367533	35.421300
1199.201004	73456.108185	35.426317
1200.788778	73563.976880	35.431335
1201.995665	73663.305128	35.436352
1203.308009	73770.115595	35.441370
1204.751926	73879.033906	35.446388
1205.843776	73973.770783	35.451405
1207.100914	74087.443468	35.456423
1207.924939	74177.054972	35.461440
1209.319637	74282.170073	35.466458
1210.327000	74391.601748	35.471476
1211.915599	74493.280270	35.476493
1213.413243	74600.204550	35.481511
1215.174735	74700.932306	35.486528
1216.252424	74810.785409	35.491546
1217.312747	74903.364523	35.496564
1218.942237	74996.894022	35.501581
1219.933680	75090.548496	35.506599
1221.582086	75183.265039	35.511616
1222.727912	75274.286793	35.516634
1223.864693	75377.394336	35.521652
1224.771664	75469.365935	35.526669
1226.097320	75563.198037	35.531687
1227.408507	75655.892700	35.536704
1228.984128	75755.437328	35.541722
1230.178732	75853.040249	35.546740
1231.830384	75948.469658	35.551757
1232.694845	76039.119782	35.556775
1233.728782	76133.493292	35.561792
1234.927160	76229.196921	35.566810
1235.891483	76323.949279	35.571828
1237.564671	76412.093342	35.576845
1238.464974	76517.104133	35.581863
1239.672040	76611.832383	35.586880
1241.340328	76699.952811	35.591898
1242.399193	76803.901309	35.596916
1243.603282	76895.603501	35.601933
1244.950425	76995.745628	35.606951
1245.965435	77093.279635	35.611968
1247.304726	77173.041559	35.616986
1248.203298	77285.909496	35.622004
1249.763432	77377.215868	35.627021
1250.953625	77483.046671	35.632039
1252.029199	77573.466376	35.637056
1253.341117	77675.808011	35.642074
1254.375986	77765.537958	35.647092
1255.621932	77850.218857	35.652109
1256.366355	77943.807635	35.657127
1257.297547	78039.255193	35.662144
1258.366666	78131.907315	35.667162
1259.725958	78226.883515	35.672180
1261.040343	78331.710163	35.677197
1262.024304	78439.058936	35.682215
1263.471226	78547.602890	35.687232
1264.778395	78653.153978	35.692250
1265.911058	78762.001059	35.697268
1267.179295	78863.315126	35.702285
1268.395322	78979.193703	35.707303
1269.852924	79086.255916	35.712320
1271.065028	79193.673469	35.717338
1271.875846	79307.690883	35.722356
1273.947993	79413.467865	35.727373
1275.034835	79525.910313	35.732391
1276.525035	79640.988872	35.737408
1278.213422	79749.766019	35.742426
1279.665276	79846.975772	35.747444
1280.945070	79957.616306	35.752461
1282.572802	80059.195525	35.757479
1283.601626	80154.457844	35.762496
1285.233271	80263.309183	35.767514
1286.047228	80371.604094	35.772532
1287.607689	80469.761972	35.777549
1288.989993	80567.301801	35.782567
1290.198082	80666.224691	35.787584
1291.492065	80768.846649	35.792602
1292.993423	80876.060995	35.797620
1294.432854	80985.439178	35.802637
1295.654065	81091.304329	35.807655
1296.861845	81194.372028	35.812672
1298.053390	81295.086111	35.817690
1299.263135	81403.716174	35.822708
1300.587787	81498.455595	35.827725
1301.846993	81608.839824	35.832743
1303.389547	81709.095332	35.837760
1304.747025	81811.787250	35.842778
1305.954350	81930.935590	35.847796
1307.789116	82025.331325	35.852813
1308.722890	82140.646172	35.857831
1310.055030	82248.500260	35.862848
1311.619474	82339.949030	35.867866
1312.769085	82445.577033	35.872884
1314.252758	82543.336021	35.877901
1315.299519	82658.990160	35.882919
1316.490399	82762.991155	35.887936
1318.182510	82860.731469	35.892954
1319.130586	82969.484321	35.897972
1320.705364	83077.835959	35.902989
1322.047781	83182.511773	35.908007
1323.369355	83288.027462	35.913024
1324.631562	83392.716536	35.918042
1325.832593	83508.793595	35.923060
1327.212900	83608.308202	35.928077
1328.712023	83718.409919	35.933095
1330.257134	83816.999995	35.938112
1331.624519	83911.449432	35.943130
1332.448815	84021.416615	35.948148
1334.062687	84127.941590	35.953165
1335.571436	84228.363334	35.958183
1336.445164	84341.022930	35.963200
1338.164399	84433.480692	35.968218
1339.415812	84549.630168	35.973236
1340.669904	84647.964307	35.978253
1342.296348	84752.715717	35.983271
1343.383977	84848.897040	35.988288
1344.774054	84944.613464	35.993306
1345.588803	85035.934171	35.998324
1346.915012	85125.198856	36.003341
1348.574937	85217.300914	36.008359
1349.709766	85316.808987	36.013376
1350.726548	85414.954607	36.018394
1351.978516	85525.000368	36.023412
1353.174473	85624.474647	36.028429
1354.498078	85728.947292	36.033447
1355.656274	85842.455493	36.038464
1357.160868	85937.764575	36.043482
1358.307090	86058.472921	36.048500
1359.589085	86170.949413	36.053517
1361.395586	86287.627734	36.058535
1362.554996	86398.793663	36.063552
1364.155971	86506.241814	36.068570
1365.276972	86624.130630	36.073588
1366.713198	86734.570478	36.078605
1368.390281	86855.516306	36.083623
1369.531788	86975.468879	36.088640
1370.914517	87090.569025	36.093658
1372.210057	87208.395022	36.098676
1373.549734	87329.179905	36.103693
1374.768050	87455.635977	36.108711
1376.696522	87574.340693	36.113728
1378.302570	87699.850412	36.118746
1379.527124	87833.251565	36.123764
1380.565827	87939.081740	36.128781
1382.596439	88051.981205	36.133799
1383.715043	88179.190918	36.138816
1385.384661	88290.411353	36.143834
1386.556965	88414.813092	36.148852
1388.265584	88526.395854	36.153869
1389.451326	88652.355240	36.158887
1390.660643	88777.221635	36.163904
1392.273824	88886.552190	36.168922
1393.508595	89007.879883	36.173940
1394.830402	89132.007915	36.178957
1396.247483	89251.496003	36.183975
1397.671544	89378.992835	36.188992
1399.336847	89499.520494	36.194010
1400.588455	89628.578682	36.199028
1402.049939	89744.982275	36.204045
1403.235475	89863.786494	36.209063
1404.550513	89997.284711	36.214080
1406.432570	90116.044891	36.219098
1407.888966	90231.956918	36.224116
1409.619664	90356.571372	36.229133
1410.813683	90474.426194	36.234151
1412.348295	90608.691397	36.239168
1413.905324	90723.968665	36.244186
1415.119668	90841.251455	36.249204
1416.607777	90964.017823	36.254221
1418.230721	91080.084643	36.259239
1419.836520	91196.471424	36.264256
1421.422914	91311.670336	36.269274
1422.770601	91420.582573	36.274292
1424.472253	91524.370537	36.279309
1426.412027	91621.911550	36.284327
1427.629852	91733.253184	36.289344
1429.234686	91827.196877	36.294362
1430.597905	91943.028619	36.299380
1431.985669	92046.803866	36.304397
1433.397130	92157.432519	36.309415
1434.244415	92265.373730	36.314432
1435.576443	92363.607421	36.319450
1437.198384	92464.356520	36.324468
1438.496773	92567.501070	36.329485
1440.144656	92653.430428	36.334503
1440.899868	92754.911091	36.339520
1442.557066	92858.406363	36.344538
1443.298427	92965.656775	36.349556
1444.684919	93073.022620	36.354573
1446.150544	93163.747428	36.359591
1447.055211	93293.052756	36.364608
1448.908007	93408.332243	36.369626
1450.094627	93520.395064	36.374644
1451.724513	93633.910280	36.379661
1453.221169	93752.643344	36.384679
1454.361973	93881.496132	36.389696
1456.154517	94006.369481	36.394714
1457.814894	94125.293979	36.399732
1458.950228	94250.080485	36.404749
1460.126048	94370.095353	36.409767
1461.665422	94503.388374	36.414784
1462.917107	94623.658599	36.419802
1464.511614	94753.483785	36.424820
1466.305257	94880.654730	36.429837
1467.922816	95013.506822	36.434855
1469.211582	95146.220528	36.439872
1470.550499	95276.366548	36.444890
1472.020355	95407.671558	36.449908
1473.417937	95536.326500	36.454925
1475.068964	95669.518431	36.459943
1476.532584	95805.186512	36.464960
1478.264880	95949.382174	36.469978
1479.995452	96077.683304	36.474996
1481.255776	96211.914402	36.480013
1482.898185	96332.776897	36.485031
1484.532823	96480.400030	36.490048
1486.059441	96609.039309	36.495066
1487.785887	96745.735349	36.500084
1489.072539	96867.022883	36.505101
1490.647920	96995.935033	36.510119
1491.894238	97133.353974	36.515136
1493.399381	97259.425983	36.520154
1495.250036	97401.416904	36.525172
1496.699228	97536.980635	36.530189
1498.179090	97659.014406	36.535207
1499.329331	97799.683695	36.540224
1501.040641	97939.771896	36.545242
1502.983428	98070.722882	36.550260
1504.560101	98199.005911	36.555277
1505.982851	98335.071564	36.560295
1507.443771	98465.858322	36.565312
1508.784821	98598.312262	36.570330
1510.519634	98732.036537	36.575348
1511.635715	98866.694352	36.580365
1513.505104	98996.545004	36.585383
1515.242040	99135.582293	36.590400
1516.109820	99264.423642	36.595418
1518.075035	99397.759884	36.600436
1519.341749	99527.047282	36.605453
1521.189210	99663.445482	36.610471
1522.740499	99801.893371	36.615488
1524.165596	99933.110055	36.620506
1526.039502	100061.493746	36.625524
1527.474877	100189.857462	36.630541
1528.804988	100316.919613	36.635559
1530.457064	100451.132999	36.640576
1532.025064	100579.135326	36.645594
1533.394504	100701.666965	36.650612
1535.133752	100843.335545	36.655629
1536.900380	100974.199034	36.660647
1538.091350	101095.897853	36.665664
1539.537398	101212.575033	36.670682
1541.277228	101324.338595	36.675700
1542.526824	101441.237340	36.680717
1544.098254	101553.966069	36.685735
1545.444431	101671.091487	36.690752
1546.862455	101792.250447	36.695770
1548.833088	101908.062428	36.700788
1549.816277	102026.031658	36.705805
1551.292822	102149.933996	36.710823
1552.807496	102280.284101	36.715840
1554.103756	102410.377118	36.720858
1555.761206	102540.744071	36.725876
1557.197811	102680.451868	36.730893
1558.854819	102810.033895	36.735911
1560.329796	102941.090114	36.740928
1561.864080	103086.198154	36.745946
1563.456600	103215.208595	36.750964
1564.699078	103362.569346	36.755981
1566.782002	103497.501574	36.760999
1568.296843	103639.394670	36.766016
1569.568430	103779.424407	36.771034
1571.301296	103921.170663	36.776052
1572.528336	104059.889911	36.781069
1574.568360	104207.142955	36.786087
1576.292500	104343.605226	36.791104
1578.453297	104476.804960	36.796122
1580.473114	104606.451648	36.801140
1582.008999	104747.395252	36.806157
1583.703671	104874.012538	36.811175
1585.305464	105006.806898	36.816192
1587.233835	105140.311715	36.821210
1588.888963	105260.394070	36.826228
1590.309877	105411.742785	36.831245
1591.996634	105537.108537	36.836263
1593.371237	105660.951077	36.841280
1595.024090	105789.569009	36.846298
1596.868041	105924.979337	36.851316
1597.888014	106063.358705	36.856333
1599.668313	106198.196766	36.861351
1601.186593	106338.477740	36.866368
1602.276729	106482.173412	36.871386
1603.806539	106627.005850	36.876404
1605.447171	106771.631456	36.881421
1607.187884	106912.552216	36.886439
1608.946965	107058.124284	36.891456
1610.680040	107209.216873	36.896474
1612.260321	107338.105565	36.901492
1613.745577	107497.682994	36.906509
1615.284468	107642.632448	36.911527
1617.289814	107781.753042	36.916544
1618.538858	107927.040457	36.921562
1620.330407	108065.612178	36.926580
1621.731280	108214.440377	36.931597
1623.443249	108369.637157	36.936615
1625.387798	108508.605304	36.941632
1626.891286	108657.343358	36.946650
1628.598481	108792.456627	36.951668
1630.187587	108943.629960	36.956685
1631.651220	109093.314463	36.961703
1633.459848	109227.272365	36.966720
1634.819614	109373.639174	36.971738
1636.851050	109515.704658	36.976756
1637.931904	109678.385843	36.981773
1639.796347	109819.311899	36.986791
1641.176939	109969.355477	36.991808
1642.529725	110118.161269	36.996826
1644.644718	110264.325496	37.001844
1646.553726	110407.593012	37.006861
1648.682662	110527.683442	37.011879
1650.152427	110652.036368	37.016896
1651.585463	110773.605537	37.021914
1653.397620	110896.574487	37.026932
1654.380815	111025.113255	37.031949
1655.979221	111155.535061	37.036967
1657.809950	111290.993832	37.041984
1658.891623	111424.274325	37.047002
1660.859626	111560.575114	37.052020
1662.257170	111706.755527	37.057037
1664.052132	111850.097371	37.062055
1665.898919	111984.617837	37.067072
1667.180464	112134.495799	37.072090
1668.769543	112291.542562	37.077108
1670.461098	112446.189846	37.082125
1672.137455	112589.033156	37.087143
1673.639149	112751.155682	37.092160
1675.208802	112901.917811	37.097178
1676.763556	113051.478079	37.102196
1678.054015	113219.875255	37.107213
1679.835530	113377.049004	37.112231
1681.674265	113557.283828	37.117248
1683.004448	113731.194054	37.122266
1685.049249	113888.925128	37.127284
1687.013901	114058.324656	37.132301
1688.650872	114223.780942	37.137319
1690.486500	114392.301642	37.142336
1692.215224	114556.603718	37.147354
1694.287887	114723.452981	37.152372
1696.171109	114899.032943	37.157389
1697.570363	115059.127112	37.162407
1699.513992	115221.699217	37.167424
1701.128327	115390.411156	37.172442
1702.769594	115557.864049	37.177460
1704.519948	115718.350355	37.182477
1706.325623	115897.092582	37.187495
1707.838828	116058.720718	37.192512
1709.333489	116229.446396	37.197530
1711.186669	116399.901443	37.202548
1713.064129	116576.137148	37.207565
1714.494582	116746.494695	37.212583
1716.739521	116924.425182	37.217600
1718.203997	117091.011988	37.222618
1719.902947	117261.494986	37.227636
1721.446878	117442.061098	37.232653
1723.573258	117614.610050	37.237671
1725.417844	117787.013395	37.242688
1726.995036	117968.388631	37.247706
1728.704288	118138.252497	37.252724
1730.093713	118320.648002	37.257741
1731.886134	118488.027111	37.262759
1733.950228	118671.156453	37.267776
1735.595480	118848.022442	37.272794
1737.278377	119005.666721	37.277812
1739.031732	119192.259010	37.282829
1740.228274	119373.915855	37.287847
1742.585610	119548.365713	37.292864
1743.928984	119751.514336	37.297882
1745.982571	119925.746816	37.302900
1747.380725	120103.443527	37.307917
1749.264731	120278.084540	37.312935
1751.162099	120463.975640	37.317952
1753.065687	120647.380446	37.322970
1754.981403	120828.551698	37.327988
1755.675475	121006.171878	37.333005
1757.950246	121189.648334	37.338023
1759.420828	121370.536220	37.343040
1761.709427	121551.881148	37.348058
1763.688931	121727.655498	37.353076
1764.764426	121879.697756	37.358093
1766.825018	122054.598364	37.363111
1768.245735	122212.918138	37.368128
1769.682754	122392.547451	37.373146
1771.499390	122558.811478	37.378164
1772.955088	122732.172830	37.383181
1774.702669	122916.754284	37.388199
1776.555505	123089.611404	37.393216
1778.318565	123269.599908	37.398234
1780.545741	123449.212540	37.403252
1782.568226	123630.392822	37.408269
1784.475269	123807.951063	37.413287
1786.124244	123986.019639	37.418304
1787.938533	124166.346752	37.423322
1790.169778	124337.615407	37.428340
1791.856634	124514.614820	37.433357
1793.383652	124697.856087	37.438375
1795.423851	124866.733689	37.443392
1796.854348	125064.999394	37.448410
1798.733731	125244.268262	37.453428
1800.456051	125437.162135	37.458445
1802.257207	125622.902210	37.463463
1803.996713	125812.103449	37.468480
1805.681393	125998.015606	37.473498
1807.554009	126198.755353	37.478516
1809.362731	126397.958261	37.483533
1810.984735	126599.360628	37.488551
1813.027919	126789.813184	37.493568
1814.810774	126986.092335	37.498586
1816.392336	127189.990514	37.503604
1818.050492	127384.755860	37.508621
1820.016839	127586.731132	37.513639
1822.215602	127790.079482	37.518656
1823.513707	128001.270101	37.523674
1825.677638	128210.538142	37.528692
1827.745496	128409.317130	37.533709
1829.630027	128625.913234	37.538727
1831.791454	128819.630056	37.543744
1833.566256	129019.434486	37.548762
1835.592590	129228.120040	37.553780
1837.468028	129426.832306	37.558797
1839.194137	129634.856098	37.563815
1840.974634	129825.135051	37.568832
1843.047697	130038.854357	37.573850
1844.560494	130235.419192	37.578868
1846.707930	130438.052471	37.583885
1848.152854	130638.448781	37.588903
1850.031168	130837.700102	37.593920
1851.685812	131058.201590	37.598938
1853.633580	131260.514578	37.603956
1855.492770	131472.675644	37.608973
1857.268918	131684.038631	37.613991
1859.484465	131884.879104	37.619008
1861.322879	132101.182878	37.624026
1863.570825	132297.706180	37.629044
1865.732859	132503.493645	37.634061
1867.455904	132713.423428	37.639079
1869.628411	132907.842238	37.644096
1871.126359	133106.071987	37.649114
1872.665666	133306.148746	37.654132
1874.516191	133510.999714	37.659149
1876.094756	133728.811196	37.664167
1878.315911	133928.365931	37.669184
1880.055531	134141.611757	37.674202
1881.605823	134344.026279	37.679220
1883.379764	134561.595735	37.684237
1885.377741	134779.321722	37.689255
1887.073024	134975.257776	37.694272
1888.651104	135168.801971	37.699290
1890.692736	135366.195851	37.704308
1892.691997	135558.648344	37.709325
1894.335401	135760.547208	37.714343
1896.121483	135954.937982	37.719360
1897.659183	136166.410281	37.724378
1899.205988	136374.798580	37.729396
1901.248360	136581.296086	37.734413
1902.738166	136803.653828	37.739431
1904.850635	137017.578568	37.744448
1906.542497	137244.437252	37.749466
1908.793308	137460.893186	37.754484
1910.875367	137691.335344	37.759501
1912.105868	137914.309869	37.764519
1914.376985	138135.156551	37.769536
1916.610159	138376.289025	37.774554
1918.570074	138599.660927	37.779572
1920.418013	138831.731465	37.784589
1922.174259	139068.601677	37.789607
1924.414644	139287.301247	37.794624
1926.117739	139537.786192	37.799642
1927.754049	139766.112531	37.804660
1930.079879	140003.901354	37.809677
1931.734194	140248.496540	37.814695
1933.940543	140474.224826	37.819712
1935.821661	140722.657814	37.824730
1937.568752	140962.597404	37.829748
1939.755737	141203.891113	37.834765
1941.967426	141456.667507	37.839783
1944.073833	141688.343747	37.844800
1946.285666	141931.439356	37.849818
1948.046606	142172.791525	37.854836
1950.164020	142407.185392	37.859853
1951.716867	142647.087426	37.864871
1953.786242	142895.654577	37.869888
1955.818684	143145.205974	37.874906
1957.947348	143399.997928	37.879924
1959.990680	143637.353625	37.884941
1961.936967	143872.923358	37.889959
1963.829460	144106.509992	37.894976
1965.957198	144356.001897	37.899994
1967.795427	144607.570790	37.905012
1970.094786	144850.096050	37.910029
1971.825448	145099.374236	37.915047
1973.662871	145344.905603	37.920064
1975.887289	145598.488135	37.925082
1977.923234	145852.304342	37.930100
1979.864804	146095.957399	37.935117
1981.621255	146340.021197	37.940135
1984.229104	146587.824795	37.945152
1986.040552	146841.528546	37.950170
1988.030065	147089.595796	37.955188
1990.161434	147329.785531	37.960205
1991.733461	147583.365184	37.965223
1994.105375	147831.135311	37.970240
1996.537329	148079.734985	37.975258
1997.841093	148340.353710	37.980276
2000.170810	148582.028772	37.985293
2002.215603	148837.241751	37.990311
2003.641889	149069.578117	37.995328
2005.750528	149314.578392	38.000346
2007.620737	149581.537701	38.005364
2010.146009	149819.100825	38.010381
2012.061028	150069.478475	38.015399
2014.424616	150317.147301	38.020416
2016.270142	150561.128005	38.025434
2018.384487	150799.317915	38.030452
2020.738290	151023.115442	38.035469
2022.431489	151248.984177	38.040487
2024.005068	151466.342473	38.045504
2026.095245	151690.450329	38.050522
2027.728008	151928.072750	38.055540
2029.799355	152145.457814	38.060557
2030.752680	152392.124267	38.065575
2032.832291	152633.196317	38.070592
2034.880441	152883.705774	38.075610
2036.928943	153134.419401	38.080628
2038.726029	153388.956056	38.085645
2040.604054	153653.902987	38.090663
2042.982767	153907.869098	38.095680
2044.710621	154174.923659	38.100698
2046.483414	154447.545196	38.105716
2048.385630	154703.988213	38.110733
2050.617820	154983.954209	38.115751
2052.753021	155261.512053	38.120768
2054.384674	155536.369538	38.125786
2056.346424	155818.971324	38.130804
2058.938999	156083.412069	38.135821
2060.827427	156382.797402	38.140839
2063.051718	156665.476677	38.145856
2064.768056	156950.762600	38.150874
2066.817655	157244.414635	38.155892
2069.043763	157531.375890	38.160909
2071.265174	157826.489348	38.165927
2073.249772	158119.889220	38.170944
2075.633992	158418.509437	38.175962
2077.471941	158711.249482	38.180980
2080.345640	158984.431643	38.185997
2082.463579	159273.880880	38.191015
2085.307317	159561.365029	38.196032
2087.090652	159841.322223	38.201050
2089.028135	160143.790903	38.206068
2091.270353	160422.384387	38.211085
2093.378873	160705.443331	38.216103
2095.542907	160999.298790	38.221120
2097.700035	161286.720048	38.226138
2099.816667	161571.838315	38.231156
2102.322504	161856.783033	38.236173
2104.292199	162133.585632	38.241191
2106.519931	162417.763611	38.246208
2108.412350	162702.807567	38.251226
2109.852974	163001.406141	38.256244
2111.918379	163294.246456	38.261261
2114.232512	163601.446663	38.266279
2116.591340	163892.301505	38.271296
2118.519163	164181.891619	38.276314
2120.594238	164489.272836	38.281332
2122.887586	164774.771267	38.286349
2125.017319	165069.678949	38.291367
2127.423006	165362.970634	38.296384
2129.542266	165662.085040	38.301402
2131.677645	165957.947964	38.306420
2133.218989	166246.388284	38.311437
2135.658565	166555.474322	38.316455
2137.870404	166842.390785	38.321472
2140.139920	167144.014920	38.326490
2142.329074	167448.763575	38.331508
2144.639543	167736.404796	38.336525
2146.531935	168036.974167	38.341543
2148.591546	168334.877841	38.346560
2150.811144	168638.115983	38.351578
2152.784652	168936.835489	38.356596
2155.141780	169234.658533	38.361613
2156.950197	169540.541993	38.366631
2158.877588	169835.298209	38.371648
2161.006514	170115.371668	38.376666
2163.056146	170402.886439	38.381684
2164.929598	170678.646648	38.386701
2166.577005	170971.521016	38.391719
2168.743139	171268.505955	38.396736
2170.695777	171560.103485	38.401754
2172.774581	171862.932509	38.406772
2174.819615	172172.434224	38.411789
2177.006163	172471.553924	38.416807
2179.060735	172779.786863	38.421824
2181.275954	173095.970204	38.426842
2183.347032	173412.761369	38.431860
2185.920272	173727.151974	38.436877
2188.319552	174049.519784	38.441895
2190.448362	174362.902785	38.446912
2192.716231	174679.046241	38.451930
2194.891967	174996.322717	38.456948
2197.485945	175313.624246	38.461965
2199.551197	175632.926725	38.466983
2201.667426	175950.990804	38.472000
2203.898080	176272.708100	38.477018
2205.985522	176607.401183	38.482036
2208.357455	176920.603874	38.487053
2210.809259	177238.747678	38.492071
2212.974473	177564.099199	38.497088
2215.272719	177891.336042	38.502106
2217.392971	178228.074940	38.507124
2219.710907	178554.930309	38.512141
2221.890181	178884.779974	38.517159
2224.171304	179219.694508	38.522176
2226.441088	179547.957964	38.527194
2228.528675	179887.629089	38.532212
2230.691200	180226.553321	38.537229
2233.095304	180560.310904	38.542247
2235.069728	180910.822956	38.547264
2237.339812	181245.670637	38.552282
2239.576072	181607.167311	38.557300
2241.947891	181947.386097	38.562317
2244.047320	182288.359670	38.567335
2245.914588	182642.526928	38.572352
2248.498398	182996.279221	38.577370
2250.935091	183352.620971	38.582388
2253.453878	183692.213614	38.587405
2255.618803	184036.866054	38.592423
2258.033950	184387.652667	38.597440
2260.339190	184741.353104	38.602458
2262.623340	185088.454364	38.607476
2264.967652	185440.195486	38.612493
2267.644738	185782.539175	38.617511
2269.445704	186190.702680	38.622528
2271.786534	186554.335018	38.627546
2274.057871	186907.032315	38.632564
2276.529143	187256.270757	38.637581
2279.013020	187605.863986	38.642599
2281.312785	187959.804951	38.647616
2283.705980	188299.407104	38.652634
2285.749053	188655.066676	38.657652
2287.380693	188996.364304	38.662669
2289.890248	189351.953529	38.667687
2292.127173	189708.653116	38.672704
2294.341915	190072.164514	38.677722
2296.619723	190434.524247	38.682740
2298.908093	190784.462745	38.687757
2301.215199	191141.511478	38.692775
2303.256158	191509.575699	38.697792
2305.908437	191859.841774	38.702810
2308.156771	192222.643419	38.707828
2310.761792	192575.052574	38.712845
2313.029677	192911.842966	38.717863
2314.966225	193233.927982	38.722880
2317.310724	193569.768403	38.727898
2319.558242	193910.704995	38.732916
2321.506855	194241.655624	38.737933
2323.646003	194584.998566	38.742951
2326.084629	194926.492325	38.747968
2328.259239	195278.569550	38.752986
2330.349492	195644.199701	38.758004
2332.833085	195988.889741	38.763021
2335.129243	196350.095322	38.768039
2337.239232	196712.296075	38.773056
2339.226043	197061.917781	38.778074
2341.533166	197443.725111	38.783092
2343.963462	197801.484325	38.788109
2346.593320	198172.244442	38.793127
2349.002714	198557.239395	38.798144
2351.517209	198925.809395	38.803162
2353.340822	199305.512237	38.808180
2355.668131	199674.976843	38.813197
2357.990193	200065.806246	38.818215
2359.840993	200452.671023	38.823232
2362.808485	200840.048805	38.828250
2365.345722	201235.724782	38.833268
2367.727424	201634.220160	38.838285
2370.160446	202019.651697	38.843303
2372.635761	202432.994745	38.848320
2374.998923	202813.409254	38.853338
2377.532918	203210.716060	38.858356
2379.609064	203615.639556	38.863373
2382.328686	204010.709201	38.868391
2384.161657	204415.570681	38.873408
2386.613639	204827.093812	38.878426
2389.217309	205237.171656	38.883444
2391.578617	205645.941717	38.888461
2394.079096	206051.490186	38.893479
2396.020174	206452.299955	38.898496
2398.696795	206863.360432	38.903514
2401.189913	207282.096565	38.908532
2403.851363	207703.322204	38.913549
2406.259571	208109.930445	38.918567
2408.702718	208529.337162	38.923584
2411.432758	208949.843123	38.928602
2413.700667	209363.461246	38.933620
2416.201089	209768.864016	38.938637
2418.628344	210182.255467	38.943655
2420.975002	210605.948485	38.948672
2423.386991	211021.020250	38.953690
2426.203918	211440.348211	38.958708
2428.541601	211864.019162	38.963725
2431.122160	212261.817548	38.968743
2433.647251	212687.569007	38.973760
2436.288938	213096.053867	38.978778
2438.978212	213503.744332	38.983796
2441.511590	213911.408756	38.988813
2444.190552	214313.919466	38.993831
2446.959807	214731.023717	38.998848
2449.325649	215128.757364	39.003866
2451.934597	215530.924656	39.008884
2454.073861	215931.590418	39.013901
2456.816110	216322.534686	39.018919
2459.348989	216725.629525	39.023936
2461.281753	217124.143811	39.028954
2463.710877	217525.477234	39.033972
2466.362992	217931.272774	39.038989
2468.908432	218329.845119	39.044007
2470.834126	218734.915997	39.049024
2473.430692	219126.977549	39.054042
2475.651794	219523.695905	39.059060
2477.772321	219908.744323	39.064077
2480.285504	220280.420155	39.069095
2482.589583	220668.844559	39.074112
2484.985364	221044.400447	39.079130
2487.721973	221434.993460	39.084148
2489.697617	221824.511072	39.089165
2492.533912	222215.774797	39.094183
2494.305201	222628.569219	39.099200
2496.758822	223022.890444	39.104218
2499.204589	223435.148281	39.109236
2501.213347	223848.261754	39.114253
2504.327626	224266.360299	39.119271
2506.539929	224679.264420	39.124288
2509.445620	225093.229273	39.129306
2512.098918	225504.032521	39.134324
2514.452440	225929.388177	39.139341
2517.233968	226355.210708	39.144359
2519.630317	226772.506577	39.149376
2521.930776	227195.126785	39.154394
2524.751609	227619.164795	39.159412
2527.242967	228057.835946	39.164429
2529.663123	228497.458025	39.169447
2531.796139	228939.284012	39.174464
2534.571456	229371.127716	39.179482
2537.161756	229805.210206	39.184500
2539.339022	230257.393659	39.189517
2542.202802	230700.375415	39.194535
2544.524029	231155.609894	39.199552
2547.222090	231606.009510	39.204570
2549.994061	232048.039429	39.209588
2552.550365	232499.044811	39.214605
2555.278397	232946.873049	39.219623
2557.952502	233407.411292	39.224640
2560.444060	233857.841397	39.229658
2563.271388	234312.918569	39.234676
2565.820057	234772.204910	39.239693
2568.189221	235228.698902	39.244711
2570.855158	235684.739771	39.249728
2573.464675	236148.943531	39.254746
2576.255844	236608.342576	39.259764
2578.661646	237071.484576	39.264781
2581.258533	237528.270735	39.269799
2584.214999	237998.438867	39.274816
2586.809136	238453.090318	39.279834
2589.487601	238902.799716	39.284852
2591.783037	239366.235177	39.289869
2594.559870	239827.156277	39.294887
2597.269376	240293.802905	39.299904
2600.026463	240763.210332	39.304922
2602.638539	241217.067258	39.309940
2604.847919	241691.029299	39.314957
2607.561256	242144.259181	39.319975
2610.285956	242609.476799	39.324992
2612.971710	243070.406455	39.330010
2616.162173	243536.007056	39.335028
2618.605850	243999.792302	39.340045
2621.448177	244445.707033	39.345063
2624.369799	244897.654428	39.350080
2626.901469	245363.201310	39.355098
2629.485583	245818.323824	39.360116
2632.049513	246277.512915	39.365133
2634.975761	246728.337870	39.370151
2637.288230	247177.047269	39.375168
2639.610106	247626.922675	39.380186
2642.575746	248089.271089	39.385204
2645.162974	248561.990643	39.390221
2647.484238	249002.032010	39.395239
2649.928772	249436.362966	39.400256
2652.382457	249868.913247	39.405274
2654.965326	250302.128185	39.410292
2657.386899	250741.006384	39.415309
2660.020645	251178.275460	39.420327
2662.519448	251611.804849	39.425344
2664.824990	252053.415553	39.430362
2667.921337	252493.352424	39.435380
2670.619731	252948.006813	39.440397
2673.450913	253398.752699	39.445415
2676.013644	253846.846415	39.450432
2678.646476	254294.267405	39.455450
2681.139057	254739.879918	39.460468
2683.891379	255208.337289	39.465485
2686.786825	255660.031328	39.470503
2689.527079	256120.740073	39.475520
2691.795414	256581.139667	39.480538
2694.709155	257051.064237	39.485556
2697.400513	257525.771711	39.490573
2700.214338	257992.990518	39.495591
2702.850032	258472.630915	39.500608
2705.658195	258940.075701	39.505626
2708.584183	259424.061571	39.510644
2711.569969	259903.768927	39.515661
2713.910083	260390.966358	39.520679
2716.655012	260872.586921	39.525696
2719.319270	261365.749733	39.530714
2722.096538	261842.636795	39.535732
2724.896024	262329.754582	39.540749
2727.613363	262815.765439	39.545767
2730.318036	263315.923785	39.550784
2732.944610	263799.074241	39.555802
2735.525188	264285.912615	39.560820
2738.290522	264792.353736	39.565837
2741.086310	265301.226001	39.570855
2743.889240	265802.830499	39.575872
2746.416098	266312.501585	39.580890
2748.749725	266817.907756	39.585908
2751.977381	267326.423278	39.590925
2754.587456	267848.391955	39.595943
2757.573273	268362.451225	39.600960
2760.220889	268884.891032	39.605978
2762.930230	269400.943407	39.610996
2765.775654	269924.819767	39.616013
2768.590783	270437.446598	39.621031
2771.513923	270965.520998	39.626048
2774.193220	271489.134883	39.631066
2777.203213	272010.078300	39.636084
2779.749294	272529.897167	39.641101
2782.370736	273054.196517	39.646119
2785.370684	273582.497310	39.651136
2788.098448	274111.853071	39.656154
2791.519288	274636.653240	39.661172
2793.874717	275161.158776	39.666189
2797.056965	275677.989595	39.671207
2800.065608	276204.113790	39.676224
2802.873485	276732.297497	39.681242
2806.008342	277248.008253	39.686260
2808.061812	277772.670862	39.691277
2810.688479	278300.339029	39.696295
2813.877236	278830.735034	39.701312
2816.216473	279360.472336	39.706330
2818.941755	279887.047690	39.711348
2822.477027	280412.096608	39.716365
2825.460984	280937.278422	39.721383
2828.362217	281458.101534	39.726400
2830.785855	281979.782495	39.731418
2833.896337	282486.243322	39.736436
2836.353845	282998.414265	39.741453
2838.885470	283501.123520	39.746471
2842.445231	283983.151183	39.751488
2844.891668	284471.747930	39.756506
2848.050145	284960.712912	39.761524
2850.566726	285456.554268	39.766541
2853.352585	285947.957160	39.771559
2855.985386	286436.917223	39.776576
2858.270823	286952.234423	39.781594
2861.181989	287465.495066	39.786612
2863.879514	287988.230839	39.791629
2866.741033	288496.920601	39.796647
2869.575169	289017.113091	39.801664
2872.246316	289552.967914	39.806682
2875.307904	290071.897685	39.811700
2878.048415	290616.594334	39.816717
2880.776592	291146.155248	39.821735
2884.021597	291678.322653	39.826752
2887.008584	292221.113440	39.831770
2889.673934	292753.463338	39.836788
2892.761635	293306.588022	39.841805
2895.712644	293850.512448	39.846823
2898.289669	294393.271443	39.851840
2901.279922	294963.813200	39.856858
2904.222137	295509.120239	39.861876
2907.117312	296074.892872	39.866893
2909.818417	296635.180886	39.871911
2912.913312	297193.675768	39.876928
2915.816039	297763.695874	39.881946
2918.628063	298332.226488	39.886964
2921.543327	298919.852085	39.891981
2924.382575	299487.884375	39.896999
2927.363241	300063.708023	39.902016
2930.563914	300645.406503	39.907034
2933.157692	301225.035372	39.912052
2935.808168	301808.431748	39.917069
2939.115118	302406.849613	39.922087
2942.441657	302993.961115	39.927104
2945.165257	303587.506251	39.932122
2948.214677	304170.484566	39.937140
2951.062923	304767.322342	39.942157
2954.509174	305354.845611	39.947175
2958.176603	305924.304972	39.952192
2960.850778	306522.621691	39.957210
2963.811926	307105.707295	39.962228
2967.253858	307698.001582	39.967245
2970.571278	308266.194373	39.972263
2974.200199	308834.357543	39.977280
2977.515445	309414.949559	39.982298
2980.574893	309965.928183	39.987316
2983.379192	310535.418204	39.992333
2986.045072	311107.689610	39.997351
2989.054822	311663.783592	40.002368
2993.112704	312221.484620	40.007386
2996.793312	312770.430691	40.012404
3000.122675	313313.181434	40.017421
3003.565351	313848.928713	40.022439
3006.406244	314374.560788	40.027456
3009.220216	314922.017365	40.032474
3011.913032	315449.842797	40.037492
3015.062463	315989.442964	40.042509
3017.882124	316521.449067	40.047527
3020.869645	317051.011817	40.052544
3023.830743	317596.205206	40.057562
3027.131113	318131.086548	40.062580
3029.421810	318663.631552	40.067597
3032.454769	319215.493371	40.072615
3035.204161	319728.033100	40.077632
3037.625370	320263.558101	40.082650
3040.226697	320779.077459	40.087668
3043.337983	321288.319577	40.092685
3045.639842	321816.307169	40.097703
3048.736181	322348.681338	40.102720
3051.450185	322886.487750	40.107738
3053.784534	323430.410855	40.112756
3056.665779	323975.814966	40.117773
3059.514949	324530.782831	40.122791
3062.219903	325091.347841	40.127808
3065.310782	325669.910798	40.132826
3067.972908	326248.608389	40.137844
3070.739289	326824.566656	40.142861
3074.135711	327427.642830	40.147879
3077.441241	328014.739946	40.152896
3080.011451	328614.450871	40.157914
3083.005512	329217.993877	40.162932
3086.142463	329823.154481	40.167949
3089.168357	330435.274418	40.172967
3092.319464	331044.447732	40.177984
3095.207710	331679.478283	40.183002
3098.843945	332291.651461	40.188020
3101.962068	332917.645164	40.193037
3105.335313	333536.967804	40.198055
3108.345031	334168.183540	40.203072
3111.457118	334807.439506	40.208090
3114.577984	335435.318867	40.213108
3117.813586	336071.692841	40.218125
3120.611579	336706.601993	40.223143
3124.556974	337350.808285	40.228160
3127.658018	337995.337517	40.233178
3130.763296	338632.372107	40.238196
3134.156664	339263.719791	40.243213
3137.165439	339910.790939	40.248231
3140.579963	340548.681833	40.253248
3144.133375	341189.354903	40.258266
3147.263010	341832.060537	40.263284
3150.764574	342471.627742	40.268301
3153.447956	343108.419350	40.273319
3157.003218	343751.961748	40.278336
3160.025838	344400.748544	40.283354
3163.026857	345045.950691	40.288372
3166.420289	345692.246108	40.293389
3169.576898	346342.547423	40.298407
3173.144012	346976.897941	40.303424
3176.373715	347621.913967	40.308442
3179.805611	348267.317149	40.313460
3183.283440	348906.082470	40.318477
3186.124901	349553.327469	40.323495
3189.371808	350192.179867	40.328512
3192.751914	350831.354034	40.333530
3195.629566	351476.856514	40.338548
3199.046448	352120.867713	40.343565
3202.212692	352766.045961	40.348583
3205.446188	353406.231468	40.353600
3208.836532	354052.439065	40.358618
3212.105844	354688.967692	40.363636
3215.479572	355333.909421	40.368653
3218.614331	355980.953899	40.373671
3221.848994	356608.956263	40.378688
3224.996007	357255.161145	40.383706
3228.463306	357888.881262	40.388724
3231.819208	358519.690492	40.393741
3234.777559	359157.899745	40.398759
3238.573532	359796.522952	40.403776
3241.456098	360435.376241	40.408794
3244.585912	361060.185884	40.413812
3248.079897	361691.642732	40.418829
3251.316161	362295.752514	40.423847
3254.082792	362882.814804	40.428864
3256.872850	363491.734684	40.433882
3259.701094	364097.341259	40.438900
3263.497921	364702.252402	40.443917
3266.966466	365312.321515	40.448935
3269.714623	365915.951445	40.453952
3272.924261	366521.068233	40.458970
3275.844473	367145.654662	40.463988
3279.185592	367762.559597	40.469005
3282.059419	368393.233352	40.474023
3285.326394	369021.373957	40.479040
3288.974125	369663.986400	40.484058
3291.749148	370310.115461	40.489076
3295.041189	370951.892338	40.494093
3298.108989	371595.665749	40.499111
3301.196300	372257.866857	40.504128
3304.410185	372914.661059	40.509146
3307.815825	373584.280560	40.514164
3311.419132	374236.675481	40.519181
3314.930862	374918.558950	40.524199
3318.082932	375583.887346	40.529216
3321.617654	376253.927927	40.534234
3324.429589	376941.062807	40.539252
3328.323536	377615.902855	40.544269
3331.242778	378298.933035	40.549287
3334.745146	378981.171006	40.554304
3338.096324	379680.006365	40.559322
3341.789245	380374.210670	40.564340
3345.217766	381058.534085	40.569357
3348.538781	381760.712844	40.574375
3351.835988	382451.529532	40.579392
3355.422894	383147.981300	40.584410
3358.686661	383854.645735	40.589428
3362.284453	384547.841457	40.594445
3365.919853	385259.828975	40.599463
3369.624857	385965.733232	40.604480
3373.321865	386663.439542	40.609498
3376.575224	387357.650377	40.614516
3380.088593	388054.359089	40.619533
3383.549723	388753.107543	40.624551
3387.122260	389445.615455	40.629568
3390.569733	390141.516354	40.634586
3393.944963	390828.167310	40.639604
3397.269284	391515.921011	40.644621
3400.598692	392220.566939	40.649639
3404.425307	392919.342796	40.654656
3408.059819	393613.014490	40.659674
3411.456220	394323.158512	40.664692
3414.765573	395003.220940	40.669709
3417.963976	395711.430753	40.674727
3421.166759	396397.950514	40.679744
3424.803379	397095.014276	40.684762
3427.659277	397807.821793	40.689780
3431.376030	398503.110279	40.694797
3434.699867	399227.951301	40.699815
3438.005347	399925.286370	40.704832
3441.345012	400636.970685	40.709850
3444.619431	401354.059230	40.714868
3448.745930	402071.347192	40.719885
3451.761506	402786.406807	40.724903
3455.151153	403496.881439	40.729920
3458.995637	404212.577183	40.734938
3462.012243	404929.391344	40.739956
3465.635139	405637.232244	40.744973
3469.230954	406364.588683	40.749991
3472.411173	407069.315817	40.755008
3476.375400	407776.479148	40.760013
3479.409806	408447.629160	40.765018
3482.745739	409059.004660	40.770023
3485.793257	409643.979322	40.775028
3488.553575	410170.445567	40.780032
3491.722511	410649.661632	40.785037
3494.592478	411081.689969	40.790042
3497.220736	411458.358064	40.795047
3499.712692	411785.079636	40.800052
3501.314625	412071.256239	40.805056
3503.511894	412312.549943	40.810061
3505.365274	412513.571788	40.815066
3507.279254	412664.927463	40.820071
3508.463777	412793.723875	40.825076
3509.876444	412893.523194	40.830080
3511.371762	412952.733729	40.835085
3512.055469	412979.255028	40.840090
3513.272171	412983.579750	40.845095
3513.916962	412971.966165	40.850100
3514.502825	412926.481189	40.855104
3514.925746	412868.544463	40.860109
3515.379358	412804.161403	40.865114
3515.928805	412713.794649	40.870119
3516.063575	412609.544005	40.875124
3516.753081	412489.331038	40.880128
3517.252253	412357.379811	40.885133
3517.225380	412221.502677	40.890138
3517.277876	412073.388482	40.895143
3517.342862	411915.989248	40.900148
3517.571383	411748.063938	40.905152
3517.856491	411589.917983	40.910157
3517.940550	411403.092976	40.915162
3517.751026	411224.526135	40.920167
3517.790508	411042.270083	40.925172
3517.852291	410852.907646	40.930176
3517.992102	410663.582154	40.935181
3517.679779	410463.774552	40.940186
3517.625254	410271.584582	40.945191
3517.669192	410069.080216	40.950196
3517.349744	409869.572672	40.955200
3516.780290	409669.544226	40.960205
3516.637876	409478.730633	40.965210
3516.671388	409277.894619	40.970215
3516.178882	409090.530916	40.975220
3516.300148	408899.924930	40.980224
3516.528505	408700.930319	40.985229
3516.037208	408518.127209	40.990234
3516.005981	408307.247989	40.995239
3515.599888	408118.848015	41.000244
3515.599123	407929.013632	41.005248
3515.566767	407740.450832	41.010253
3515.309378	407545.021921	41.015258
3515.143359	407355.208363	41.020263
3515.045296	407167.259727	41.025268
3514.392806	406993.803994	41.030272
3514.069763	406803.249183	41.035277
3514.009033	406621.733311	41.040282
3514.217555	406447.581286	41.045287
3513.849033	406279.098526	41.050292
3513.403193	406112.655938	41.055296
3513.166607	405934.053770	41.060301
3512.878751	405764.692096	41.065306
3512.790633	405592.609043	41.070311
3512.707111	405430.519083	41.075316
3512.432444	405275.763830	41.080320
3512.255644	405124.087265	41.085325
3511.626432	404972.987459	41.090330
3511.798725	404809.381841	41.095335
3511.178772	404662.439039	41.100340
3511.296573	404519.744006	41.105344
3511.191660	404370.791095	41.110349
3510.838822	404234.611361	41.115354
3511.142437	404080.417562	41.120359
3510.858592	403948.386029	41.125364
3510.339310	403805.024546	41.130368
3510.498163	403669.167722	41.135373
3510.593352	403532.457400	41.140378
3510.012761	403400.976279	41.145383
3510.038737	403271.023737	41.150388
3509.830940	403142.984279	41.155392
3509.860597	403024.852591	41.160397
3509.538827	402898.047305	41.165402
3509.612924	402768.642585	41.170407
3509.350432	402642.740027	41.175412
3509.050498	402521.967661	41.180416
3509.121066	402403.978634	41.185421
3508.809587	402287.114068	41.190426
3508.793820	402168.274623	41.195431
3508.842991	402058.203198	41.200436
3508.431905	401947.847658	41.205440
3508.681690	401836.779813	41.210445
3508.376555	401730.770783	41.215450
3508.484038	401618.303173	41.220455
3508.239700	401509.289701	41.225460
3507.743331	401397.726907	41.230464
3507.773782	401283.239826	41.235469
3507.419460	401191.901523	41.240474
3507.718048	401093.965735	41.245479
3507.391494	400991.559628	41.250484
3507.448699	400901.171068	41.255488
3507.191918	400800.478645	41.260493
3506.815124	400707.873255	41.265498
3507.017877	400616.750476	41.270503
3506.771518	400531.837676	41.275508
3506.590356	400451.684703	41.280512
3506.845795	400361.567678	41.285517
3506.085896	400277.444330	41.290522
3506.442972	400195.938016	41.295527
3506.398634	400123.780841	41.300532
3506.406077	400027.408309	41.305536
3506.432991	399946.155492	41.310541
3506.192427	399865.350007	41.315546
3505.822304	399782.077693	41.320551
3505.984195	399709.024405	41.325556
3506.263398	399635.901884	41.330560
3506.142738	399555.076663	41.335565
3505.359591	399477.348493	41.340570
3505.756343	399405.424953	41.345575
3505.564028	399339.733622	41.350580
3505.574461	399260.054233	41.355584
3505.672314	399187.770534	41.360589
3505.550518	399129.274198	41.365594
3505.901720	399052.535358	41.370599
3505.547418	398977.733083	41.375604
3505.217642	398908.813875	41.380608
3505.427458	398838.440214	41.385613
3505.220518	398771.480783	41.390618
3504.908285	398692.763198	41.395623
3505.351547	398632.452140	41.400628
3505.446978	398577.219479	41.405632
3505.262687	398500.714418	41.410637
3505.284477	398439.301156	41.415642
3504.995880	398387.426692	41.420647
3505.156761	398317.262092	41.425652
3504.820969	398249.915205	41.430656
3505.052981	398186.590729	41.435661
3504.882225	398132.718013	41.440666
3504.873161	398061.513289	41.445671
3504.571889	398003.600357	41.450676
3504.497708	397942.302238	41.455680
3504.892184	397886.260123	41.460685
3504.794739	397839.227015	41.465690
3504.658724	397773.421030	41.470695
3504.480764	397720.005272	41.475700
3504.317341	397655.827340	41.480704
3504.731193	397602.014699	41.485709
3504.312168	397547.671741	41.490714
3504.302397	397483.114151	41.495719
3504.189450	397433.950974	41.500724
3504.402761	397379.255457	41.505728
3504.374229	397326.932152	41.510733
3504.071390	397282.619883	41.515738
3504.167212	397228.348336	41.520743
3504.085238	397177.403392	41.525748
3504.096546	397131.722331	41.530752
3504.294108	397071.902312	41.535757
3504.159627	397029.187529	41.540762
3504.162274	396970.311176	41.545767
3503.991671	396925.723884	41.550772
3503.899108	396875.033715	41.555776
3504.161303	396825.455609	41.560781
3503.926918	396771.538934	41.565786
3504.039214	396723.557367	41.570791
3504.145573	396683.088490	41.575796
3503.716092	396639.200770	41.580800
3504.082029	396584.428913	41.585805
3503.721577	396533.272140	41.590810
3503.745355	396483.578153	41.595815
3503.673715	396441.613877	41.600820
3503.811182	396400.835141	41.605824
3503.867017	396350.679080	41.610829
3503.675605	396313.707356	41.615834
3503.903659	396258.296369	41.620839
3503.812533	396212.578722	41.625844
3503.138161	396161.469997	41.630848
3503.811038	396115.379490	41.635853
3503.738942	396089.149341	41.640858
3503.774068	396036.813286	41.645863
3503.625481	395998.768508	41.650868
3503.633926	395954.456075	41.655872
3503.681469	395907.802631	41.660877
3503.705893	395863.792087	41.665882
3503.615612	395822.489469	41.670887
3503.515323	395780.274697	41.675892
3503.491580	395726.221358	41.680896
3503.593541	395683.213573	41.685901
3503.639739	395648.843256	41.690906
3503.495024	395590.849308	41.695911
3503.465701	395558.419423	41.700916
3503.413838	395517.008781	41.705920
3503.462821	395480.556698	41.710925
3503.592089	395436.122985	41.715930
3503.470300	395392.438876	41.720935
3503.441379	395343.512093	41.725940
3503.535925	395304.870029	41.730944
3503.423811	395267.122961	41.735949
3502.904843	395221.723787	41.740954
3503.499572	395185.440124	41.745959
3503.901613	395134.313972	41.750964
3503.331348	395098.211464	41.755968
3503.188228	395060.570414	41.760973
3503.020836	395026.130922	41.765978
3503.268166	394978.378629	41.770983
3503.015676	394933.648074	41.775988
3502.995345	394904.159957	41.780992
3503.013196	394873.295351	41.785997
3503.124296	394841.654798	41.791002
3503.705182	394801.667249	41.796007
3503.723100	394768.924385	41.801012
3503.070050	394718.773691	41.806016
3503.354470	394671.827177	41.811021
3503.415415	394632.377097	41.816026
3502.953370	394589.099793	41.821031
3503.475023	394551.608299	41.826036
3503.132967	394520.342403	41.831040
3502.970940	394486.510426	41.836045
3503.129668	394450.293502	41.841050
3503.452791	394403.543485	41.846055
3503.246140	394360.429070	41.851060
3503.167737	394329.375701	41.856064
3503.356759	394284.016862	41.861069
3503.013892	394259.603475	41.866074
3502.817554	394216.791764	41.871079
3502.618350	394184.944830	41.876084
3502.906044	394146.270845	41.881088
3503.237733	394109.417360	41.886093
3502.985684	394065.548062	41.891098
3502.893023	394029.877239	41.896103
3503.010199	394002.650885	41.901108
3503.116893	393971.974344	41.906112
3502.996981	393923.667967	41.911117
3502.721375	393892.035582	41.916122
3502.827079	393863.338765	41.921127
3503.110415	393829.893418	41.926132
3502.991592	393798.591846	41.931136
3503.048619	393750.409875	41.936141
3503.117172	393728.876127	41.941146
3503.240989	393686.622799	41.946151
3503.235279	393652.308467	41.951156
3503.244579	393619.362332	41.956160
3503.132683	393578.566841	41.961165
3503.255937	393536.567151	41.966170
3503.177887	393494.344901	41.971175
3502.978018	393472.548119	41.976180
3502.911898	393421.288135	41.981184
3503.352552	393382.741416	41.986189
3503.121891	393358.005079	41.991194
3502.970024	393309.956263	41.996199
3503.022892	393280.556295	42.001204
3502.805943	393244.091445	42.006208
3502.840012	393199.972999	42.011213
3502.858303	393179.563374	42.016218
3503.269110	393142.289999	42.021223
3502.721983	393106.130137	42.026228
3502.816465	393074.591381	42.031232
3503.251272	393045.994674	42.036237
3503.120142	393010.531388	42.041242
3502.750794	392963.226417	42.046247
3502.945034	392930.098276	42.051252
3502.745949	392911.092873	42.056256
3502.976912	392867.298530	42.061261
3502.966614	392833.440627	42.066266
3503.053968	392787.384109	42.071271
3503.262148	392756.893293	42.076276
3502.543643	392724.313019	42.081280
3502.926155	392680.850106	42.086285
3502.610641	392658.410652	42.091290
3502.909717	392618.767937	42.096295
3502.942591	392596.223448	42.101300
3503.079430	392557.570404	42.106304
3503.250373	392512.617178	42.111309
3502.818099	392482.174916	42.116314
3502.939835	392444.082455	42.121319
3503.042643	392410.714010	42.126324
3502.709933	392380.814542	42.131328
3502.817738	392341.810319	42.136333
3502.641269	392316.810663	42.141338
3502.638557	392281.732450	42.146343
3502.304832	392253.863588	42.151348
3502.564696	392219.404373	42.156352
3503.027985	392188.771618	42.161357
3502.892126	392161.024155	42.166362
3502.663444	392121.868882	42.171367
3502.592683	392090.354564	42.176372
3502.595569	392061.519322	42.181376
3503.083251	392026.567494	42.186381
3502.769175	391994.278665	42.191386
3502.251103	391961.920006	42.196391
3502.702533	391939.309777	42.201396
3502.696770	391909.460384	42.206400
3502.656890	391878.093285	42.211405
3502.475083	391852.434026	42.216410
3502.421394	391819.038359	42.221415
3502.562320	391787.033815	42.226420
3501.923912	391759.059501	42.231424
3502.259720	391730.527424	42.236429
3502.124659	391708.160546	42.241434
3502.267444	391678.541587	42.246439
3502.636535	391658.431464	42.251444
3502.336315	391632.435034	42.256448
3502.475738	391597.333721	42.261453
3502.586253	391576.451504	42.266458
3502.193236	391538.996165	42.271463
3502.827675	391520.063037	42.276468
3502.598229	391486.795801	42.281472
3502.864692	391453.959017	42.286477
3502.819218	391432.034847	42.291482
3502.913277	391397.854112	42.296487
3502.778117	391351.271073	42.301492
3502.584809	391323.328531	42.306496
3502.902962	391277.791688	42.311501
3502.839499	391258.713125	42.316506
3502.373266	391227.310004	42.321511
3502.625278	391197.216561	42.326516
3502.253876	391163.615604	42.331520
3502.502489	391130.730399	42.336525
3502.622799	391109.440119	42.341530
3502.889082	391081.324248	42.346535
3502.323117	391051.459449	42.351540
3502.042378	391023.124028	42.356544
3502.390359	390987.684782	42.361549
3502.484845	390971.830557	42.366554
3502.319339	390938.857234	42.371559
3502.022673	390915.347117	42.376564
3501.899233	390898.511397	42.381568
3502.627803	390861.337402	42.386573
3502.381778	390830.711794	42.391578
3502.585017	390811.845222	42.396583
3502.287774	390785.999736	42.401588
3502.287677	390760.514129	42.406592
3502.410682	390729.475592	42.411597
3502.610385	390706.344949	42.416602
3502.325785	390675.268235	42.421607
3502.293217	390649.330650	42.426612
3502.158473	390638.537962	42.431616
3502.224046	390595.932967	42.436621
3502.514814	390576.392603	42.441626
3502.160100	390546.037397	42.446631
3502.310736	390512.049701	42.451636
3502.273418	390499.972572	42.456640
3502.482287	390463.741919	42.461645
3502.304013	390444.096748	42.466650
3501.797624	390411.048840	42.471655
3502.264693	390390.287823	42.476660
3502.053617	390363.006950	42.481664
3502.262353	390338.376869	42.486669
3502.258953	390326.472068	42.491674
3502.394949	390295.608655	42.496679
3502.426033	390276.641541	42.501684
3502.248943	390247.654482	42.506688
3502.353615	390217.532001	42.511693
3502.036039	390192.247518	42.516698
3502.133976	390161.643707	42.521703
3502.028122	390130.563875	42.526708
3502.208541	390115.482655	42.531712
3501.678730	390088.301848	42.536717
3502.000644	390076.219380	42.541722
3502.090968	390053.866692	42.546727
3502.107503	390030.865459	42.551732
3501.932604	390011.447882	42.556736
3501.873557	389998.358492	42.561741
3502.224325	389971.294375	42.566746
3501.997292	389948.026348	42.571751
3502.225076	389924.535214	42.576756
3502.147636	389902.893891	42.581760
3502.232269	389873.611815	42.586765
3502.097960	389854.974735	42.591770
3502.067452	389820.557344	42.596775
3502.226574	389798.371416	42.601780
3501.668992	389779.647834	42.606784
3502.126067	389760.563264	42.611789
3502.227266	389740.874044	42.616794
3502.066791	389713.533809	42.621799
3502.294118	389688.341713	42.626804
3502.387803	389666.242004	42.631808
3502.306269	389641.453317	42.636813
3501.868885	389618.623878	42.641818
3502.149631	389590.351747	42.646823
3502.315687	389569.992279	42.651828
3501.846950	389549.706191	42.656832
3502.045740	389510.962559	42.661837
3501.923929	389506.564488	42.666842
3501.871758	389476.237043	42.671847
3501.994935	389458.803484	42.676852
3502.076560	389432.923008	42.681856
3502.146925	389406.891945	42.686861
3502.247238	389384.613255	42.691866
3502.203591	389366.012470	42.696871
3502.446698	389342.391473	42.701876
3502.324003	389317.964265	42.706880
3502.236327	389290.637621	42.711885
3501.875081	389266.374413	42.716890
3501.740015	389247.508522	42.721895
3502.182385	389231.675203	42.726900
3501.885606	389205.777218	42.731904
3502.129830	389174.692481	42.736909
3502.072549	389160.688486	42.741914
3501.795830	389133.035685	42.746919
3502.126106	389111.203296	42.751924
3502.229045	389090.650171	42.756928
3502.368342	389055.799121	42.761933
3502.278549	389028.345589	42.766938
3502.270393	388998.924604	42.771943
3502.297715	388981.378697	42.776948
3502.244872	388957.625686	42.781952
3502.328549	388926.768711	42.786957
3502.150811	388908.670784	42.791962
3502.309577	388884.580142	42.796967
3502.484195	388858.430737	42.801972
3502.308454	388834.595189	42.806977
3501.874870	388805.037088	42.811981
3502.002242	388785.317651	42.816986
3502.173594	388767.444547	42.821991
3502.442805	388740.442554	42.826996
3502.181978	388718.498715	42.832001
3502.468204	388683.624281	42.837005
3501.798513	388658.063003	42.842010
3501.928231	388645.857432	42.847015
3502.029213	388621.369347	42.852020
3502.162078	388597.637867	42.857025
3502.032645	388571.865499	42.862029
3501.935653	388545.732645	42.867034
3502.363119	388531.805183	42.872039
3502.259450	388496.356499	42.877044
3502.345466	388476.516322	42.882049
3502.267241	388444.236914	42.887053
3502.107130	388430.121577	42.892058
3502.236648	388388.670621	42.897063
3502.669197	388368.065609	42.902068
3502.087226	388346.679147	42.907073
3502.317847	388306.177011	42.912077
3502.540740	388288.980983	42.917082
3502.190305	388264.892821	42.922087
3501.990089	388239.435764	42.927092
3502.398889	388228.836698	42.932097
3502.186168	388200.487460	42.937101
3501.938162	388172.956058	42.942106
3502.122989	388162.137948	42.947111
3502.395722	388136.810284	42.952116
3502.103792	388113.423703	42.957121
3502.235005	388082.532900	42.962125
3502.081482	388055.240534	42.967130
3501.950400	388037.997869	42.972135
3502.335262	388002.904041	42.977140
3501.878875	387984.950352	42.982145
3502.213112	387957.810461	42.987149
3501.991093	387931.493325	42.992154
3502.197502	387913.258736	42.997159
3502.038655	387890.511300	43.002164
3501.751110	387861.843290	43.007169
3502.200780	387841.869859	43.012173
3501.891618	387816.327776	43.017178
3502.009821	387801.864129	43.022183
3502.057071	387776.723512	43.027188
3501.550982	387758.777395	43.032193
3502.193981	387729.685170	43.037197
3502.228613	387709.725444	43.042202
3501.798809	387689.177906	43.047207
3502.349359	387674.088387	43.052212
3502.143183	387643.985777	43.057217
3501.893188	387613.458365	43.062221
3501.920905	387600.354212	43.067226
3502.196860	387578.173516	43.072231
3502.014020	387547.610186	43.077236
3501.832169	387535.122521	43.082241
3502.120091	387513.422267	43.087245
3501.729040	387495.584996	43.092250
3501.704890	387475.481907	43.097255
3501.832380	387456.396092	43.102260
3501.978312	387435.301779	43.107265
3501.747380	387413.732953	43.112269
3501.657764	387398.133586	43.117274
3501.970685	387375.261494	43.122279
3501.931754	387355.947625	43.127284
3501.983268	387344.946807	43.132289
3502.343033	387306.860174	43.137293
3502.193720	387290.330685	43.142298
3502.100573	387266.099974	43.147303
3502.203738	387234.628575	43.152308
3502.130283	387211.994174	43.157313
3502.174004	387193.911318	43.162317
3502.447571	387168.658712	43.167322
3502.004332	387146.208733	43.172327
3501.917490	387111.110901	43.177332
3501.915369	387093.162046	43.182337
3502.012271	387068.114545	43.187341
3502.193040	387040.997546	43.192346
3501.724911	387016.012532	43.197351
3501.960037	387003.992863	43.202356
3502.073190	386982.192408	43.207361
3502.071046	386959.927503	43.212365
3502.021232	386938.837846	43.217370
3501.642985	386909.345056	43.222375
3501.975113	386901.245393	43.227380
3501.782053	386885.890298	43.232385
3501.807462	386859.965133	43.237389
3501.848494	386835.053035	43.242394
3501.880346	386818.038058	43.247399
3501.815284	386791.695302	43.252404
3501.877063	386781.962051	43.257409
3501.949863	386755.420087	43.262413
3502.007037	386742.691727	43.267418
3501.759931	386717.722799	43.272423
3501.736915	386696.222557	43.277428
3501.712406	386678.581550	43.282433
3502.023931	386661.116734	43.287437
3501.531935	386642.888352	43.292442
3501.651022	386617.938506	43.297447
3501.484182	386604.204013	43.302452
3501.718378	386580.962626	43.307457
3501.765579	386563.767371	43.312461
3501.581002	386544.526321	43.317466
3501.505445	386529.584326	43.322471
3501.651107	386516.004264	43.327476
3501.666316	386501.759006	43.332481
3502.087738	386474.629339	43.337485
3501.710961	386446.557535	43.342490
3501.666456	386435.774371	43.347495
3501.705792	386420.357440	43.352500
3502.025292	386407.867364	43.357505
3502.327135	386380.121490	43.362509
3501.789944	386363.347089	43.367514
3501.813850	386339.554266	43.372519
3502.113349	386319.983830	43.377524
3501.845396	386298.343644	43.382529
3501.692176	386272.191786	43.387533
3501.783033	386271.441412	43.392538
3501.797204	386254.911193	43.397543
3502.485918	386225.937067	43.402548
3502.261732	386196.978023	43.407553
3502.115785	386178.949344	43.412557
3501.879867	386152.530954	43.417562
3501.699311	386129.607582	43.422567
3501.513803	386108.741458	43.427572
3501.429980	386099.868434	43.432577
3501.621399	386079.349854	43.437581
3501.570661	386073.188284	43.442586
3501.961007	386037.583091	43.447591
3502.172813	386019.016237	43.452596
3501.638735	386003.866005	43.457601
3501.863416	385980.473215	43.462605
3501.837802	385959.810588	43.467610
3501.617074	385950.095589	43.472615
3502.240945	385909.553795	43.477620
3501.636455	385912.288361	43.482625
3501.771799	385876.621067	43.487629
3501.706249	385865.206208	43.492634
3501.911117	385849.179221	43.497639
3501.888165	385824.936202	43.502644
3501.644003	385814.133065	43.507649
3501.521283	385794.120143	43.512653
3501.751726	385779.257034	43.517658
3501.122597	385747.567678	43.522663
3501.783936	385734.973299	43.527668
3501.564533	385720.865667	43.532673
3501.468877	385699.909057	43.537677
3501.457288	385693.919028	43.542682
3501.792842	385673.733140	43.547687
3501.758272	385659.647491	43.552692
3501.505408	385647.068384	43.557697
3501.494444	385630.236997	43.562701
3501.839185	385621.322505	43.567706
3501.645140	385603.580184	43.572711
3501.862803	385579.401046	43.577716
3501.946212	385566.515677	43.582721
3501.650480	385541.146923	43.587725
3501.768158	385519.014441	43.592730
3501.482155	385510.807409	43.597735
3501.771323	385479.634946	43.602740
3501.711382	385471.824345	43.607745
3501.705141	385445.547203	43.612749
3501.732465	385435.844186	43.617754
3501.618477	385410.573968	43.622759
3501.578608	385398.367826	43.627764
3501.498200	385387.894478	43.632769
3501.661390	385366.287963	43.637773
3501.888904	385352.923048	43.642778
3501.589088	385336.593429	43.647783
3502.137430	385316.323367	43.652788
3502.021393	385296.892975	43.657793
3502.046578	385272.286483	43.662797
3501.682454	385243.322736	43.667802
3501.380519	385233.848607	43.672807
3501.950640	385197.046335	43.677812
3501.977986	385189.044336	43.682817
3501.931199	385168.003513	43.687821
3501.893069	385149.703427	43.692826
3501.550865	385134.446646	43.697831
3501.945704	385109.909424	43.702836
3501.844626	385086.718844	43.707841
3501.899509	385064.621129	43.712845
3501.772091	385048.772296	43.717850
3501.767308	385029.172048	43.722855
3502.072825	385008.025490	43.727860
3501.408546	385009.144496	43.732865
3501.639221	384984.226460	43.737869
3501.721978	384963.927010	43.742874
3501.871077	384942.601618	43.747879
3501.536640	384924.017409	43.752884
3501.682185	384920.262460	43.757889
3501.779422	384895.415882	43.762893
3501.808367	384876.368850	43.767898
3501.474819	384858.622327	43.772903
3501.426764	384842.735626	43.777908
3501.518935	384828.020430	43.782913
3501.386250	384802.650958	43.787917
3501.606947	384805.536521	43.792922
3501.353595	384782.597871	43.797927
3501.289819	384766.764349	43.802932
3501.261167	384751.306205	43.807937
3501.494530	384733.217475	43.812941
3501.471084	384720.424477	43.817946
3501.755954	384714.413475	43.822951
3501.697257	384696.268606	43.827956
3501.616498	384684.754022	43.832961
3501.840122	384670.449915	43.837965
3501.932305	384645.248416	43.842970
3501.460948	384627.599349	43.847975
3501.701167	384595.798665	43.852980
3501.332036	384596.033876	43.857985
3501.504983	384571.479886	43.862989
3501.568853	384561.923193	43.867994
3501.673859	384549.440196	43.872999
3501.539770	384527.752279	43.878004
3501.741078	384515.355842	43.883009
3501.519652	384499.191220	43.888013
3501.770911	384477.570249	43.893018
3501.801701	384458.319494	43.898023
3501.894508	384444.949676	43.903028
3501.631983	384418.559015	43.908033
3501.580347	384399.371824	43.913037
3501.468807	384389.258379	43.918042
3501.786883	384374.380816	43.923047
3501.560110	384355.830219	43.928052
3502.005427	384334.966039	43.933057
3502.060979	384315.889058	43.938061
3501.743411	384290.598629	43.943066
3501.597317	384276.351835	43.948071
3502.107527	384244.280185	43.953076
3501.679326	384240.589028	43.958081
3501.774997	384212.771316	43.963085
3501.893983	384193.252730	43.968090
3501.544305	384175.508243	43.973095
3501.962844	384159.370774	43.978100
3501.464811	384133.168811	43.983105
3501.650258	384115.874218	43.988109
3501.622114	384102.015226	43.993114
3501.895313	384085.341728	43.998119
3501.977609	384065.092419	44.003124
3501.783134	384045.597108	44.008129
3501.743286	384032.476237	44.013133
3501.700918	384002.597721	44.018138
3501.598700	383999.998395	44.023143
3501.540489	383968.675020	44.028148
3501.482881	383965.789448	44.033153
3501.764938	383940.989357	44.038157
3501.658456	383924.247882	44.043162
3501.621847	383907.267005	44.048167
3501.623599	383884.186288	44.053172
3501.700275	383878.664528	44.058177
3501.806816	383855.262786	44.063181
3501.872997	383835.853710	44.068186
3501.449973	383820.938805	44.073191
3501.694265	383806.275525	44.078196
3501.681702	383787.411880	44.083201
3501.598882	383766.070818	44.088205
3501.975198	383745.445418	44.093210
3501.595400	383746.088554	44.098215
3501.823497	383721.093519	44.103220
3501.498362	383703.090972	44.108225
3501.732259	383694.396191	44.113229
3501.931064	383666.079404	44.118234
3502.040438	383642.245375	44.123239
3501.720847	383620.128513	44.128244
3501.755852	383595.061838	44.133249
3501.844668	383586.186466	44.138253
3501.672115	383568.185472	44.143258
3501.349045	383545.180389	44.148263
3501.750703	383527.927929	44.153268
3501.826054	383524.183700	44.158273
3501.663422	383492.444340	44.163277
3501.685836	383482.969870	44.168282
3501.189778	383464.155835	44.173287
3501.435006	383446.749923	44.178292
3501.366231	383433.937946	44.183297
3501.528359	383415.326151	44.188301
3501.418437	383408.081311	44.193306
3501.016405	383411.343245	44.198311
3501.517644	383385.873723	44.203316
3501.746923	383366.362739	44.208321
3501.573723	383357.502670	44.213325
3501.613830	383339.671557	44.218330
3501.702459	383326.809641	44.223335
3502.147964	383295.102361	44.228340
3501.651652	383284.642089	44.233345
3501.748310	383253.979319	44.238349
3501.675154	383244.697376	44.243354
3501.312355	383226.167130	44.248359
3501.269527	383201.569235	44.253364
3501.306762	383206.921137	44.258369
3501.581916	383188.951777	44.263373
3501.945816	383165.255442	44.268378
3501.747011	383151.803372	44.273383
3501.781416	383124.451070	44.278388
3501.611108	383114.168524	44.283393
3501.593987	383099.190036	44.288397
3501.971662	383091.539137	44.293402
3501.403492	383068.724119	44.298407
3501.756746	383044.521493	44.303412
3501.845874	383026.301656	44.308417
3501.699697	383005.249133	44.313421
3501.601893	382987.718549	44.318426
3501.373764	382977.114851	44.323431
3501.679454	382962.593890	44.328436
3501.448086	382948.004141	44.333441
3501.631658	382927.484258	44.338445
3501.755275	382913.524835	44.343450
3501.429070	382894.176111	44.348455
3501.418916	382877.469750	44.353460
3501.385778	382864.880473	44.358465
3501.584537	382847.989231	44.363469
3501.792605	382833.407213	44.368474
3501.114962	382822.898793	44.373479
3501.431775	382799.209451	44.378484
3501.386608	382786.266517	44.383489
3501.839757	382762.809848	44.388493
3501.444202	382755.736233	44.393498
3501.169706	382745.444362	44.398503
3501.475954	382729.805926	44.403508
3501.206738	382729.009914	44.408513
3501.161798	382702.532848	44.413517
3501.289224	382678.339628	44.418522
3501.223511	382682.945891	44.423527
3501.635323	382668.052760	44.428532
3501.418102	382651.327691	44.433537
3501.560200	382643.129296	44.438541
3501.545331	382619.288265	44.443546
3501.107142	382610.291428	44.448551
3501.449759	382600.385922	44.453556
3501.607143	382586.903523	44.458561
3501.562088	382560.654860	44.463565
3501.428488	382549.325290	44.468570
3501.227200	382541.713538	44.473575
3501.977776	382517.169275	44.478580
3501.636210	382511.102889	44.483585
3501.601556	382484.979494	44.488589
3501.666498	382481.998508	44.493594
3501.557918	382460.736551	44.498599
3501.481744	382445.284417	44.503604
3501.367213	382442.026644	44.508609
3501.551339	382414.294798	44.513613
3501.723529	382407.818338	44.518618
3501.561614	382385.980592	44.523623
3501.491087	382363.595362	44.528628
3501.488315	382348.690384	44.533633
3501.567534	382336.337292	44.538637
3501.834147	382328.474918	44.543642
3501.270144	382305.176117	44.548647
3501.627199	382289.935793	44.553652
3501.727206	382275.243314	44.558657
3501.683934	382256.764220	44.563661
3501.538698	382249.524550	44.568666
3501.521005	382222.611078	44.573671
3501.559437	382213.362185	44.578676
3501.427211	382194.922283	44.583681
3501.387529	382171.008522	44.588685
3501.819723	382167.665638	44.593690
3501.710520	382145.032310	44.598695
3501.716502	382126.570852	44.603700
3501.805799	382111.499054	44.608705
3501.448560	382094.059022	44.613709
3501.357889	382079.700818	44.618714
3501.437633	382067.169766	44.623719
3501.600671	382051.096137	44.628724
3501.364804	382034.170428	44.633729
3501.767498	382016.586695	44.638733
3501.393281	382004.329399	44.643738
3501.520949	381984.883973	44.648743
3501.432805	381962.856640	44.653748
3501.455512	381963.259431	44.658753
3500.985531	381935.019430	44.663757
3501.280075	381933.196123	44.668762
3501.275662	381920.703489	44.673767
3501.829968	381904.187988	44.678772
3501.278059	381883.730944	44.683777
3501.671132	381870.567000	44.688781
3501.929406	381854.097533	44.693786
3501.305518	381845.941905	44.698791
3501.608045	381829.897219	44.703796
3501.672225	381815.362414	44.708801
3501.090311	381802.604086	44.713805
3501.374670	381779.299762	44.718810
3501.409830	381774.850527	44.723815
3501.656352	381757.468674	44.728820
3501.366267	381732.146066	44.733825
3501.129834	381719.841800	44.738829
3501.590726	381711.415752	44.743834
3501.288848	381697.471101	44.748839
3501.600425	381678.149187	44.753844
3501.399599	381673.101826	44.758849
3501.128884	381651.762864	44.763853
3501.208590	381641.923301	44.768858
3501.052878	381634.710483	44.773863
3501.525071	381619.375671	44.778868
3501.109508	381606.108887	44.783873
3500.921922	381586.788402	44.788877
3501.158557	381587.437236	44.793882
3501.255499	381585.847801	44.798887
3501.444188	381565.554587	44.803892
3501.201363	381554.698659	44.808897
3501.297455	381546.964159	44.813901
3501.446325	381533.939620	44.818906
3500.952802	381516.164899	44.823911
3501.233407	381509.087297	44.828916
3501.158886	381506.026328	44.833921
3501.460355	381499.072444	44.838925
3501.793990	381477.486935	44.843930
3501.565806	381460.889772	44.848935
3501.732421	381436.790874	44.853940
3501.568819	381439.254143	44.858945
3501.352838	381411.329556	44.863949
3501.501849	381395.410067	44.868954
3501.233411	381386.081665	44.873959
3501.532789	381368.488181	44.878964
3501.365462	381364.451289	44.883969
3501.429447	381354.664850	44.888973
3501.482372	381332.995936	44.893978
3501.236038	381320.439087	44.898983
3501.433583	381309.463743	44.903988
3501.162504	381279.262163	44.908993
3501.292712	381267.814801	44.913997
3501.548153	381264.854819	44.919002
3501.161306	381244.727097	44.924007
3501.360327	381231.669210	44.929012
3500.923152	381222.392402	44.934017
3501.078284	381228.234240	44.939021
3501.522683	381203.964932	44.944026
3501.539328	381189.462569	44.949031
3501.194958	381175.930550	44.954036
3501.071665	381166.655665	44.959041
3500.872727	381151.729741	44.964045
3501.224372	381155.154002	44.969050
3501.095861	381151.085643	44.974055
3501.076556	381143.089649	44.979060
3501.361187	381130.577052	44.984065
3501.582634	381114.519151	44.989069
3501.513022	381100.766581	44.994074
3501.179323	381085.074382	44.999079
3501.486971	381067.504802	45.004084
3501.407637	381066.222099	45.009089
3501.298253	381040.464397	45.014093
3501.616027	381027.057808	45.019098
3501.302917	381025.989239	45.024103
3501.387977	380999.337847	45.029108
3501.669945	380990.406138	45.034113
3501.164710	380976.873655	45.039117
3501.305801	380954.124162	45.044122
3501.188819	380947.920885	45.049127
3501.153493	380936.219804	45.054132
3501.215849	380928.820492	45.059137
3501.248693	380915.051881	45.064141
3501.615191	380903.592984	45.069146
3501.394310	380893.317428	45.074151
3501.528950	380867.775524	45.079156
3501.353928	380855.588264	45.084161
3501.365007	380846.114597	45.089165
3501.819755	380824.687462	45.094170
3501.768053	380820.454734	45.099175
3501.199312	380787.454769	45.104180
3501.524739	380784.026749	45.109185
3501.603205	380761.845506	45.114189
3501.733002	380747.731596	45.119194
3501.261541	380741.634219	45.124199
3501.235642	380706.721301	45.129204
3501.202081	380704.568054	45.134209
3501.556533	380691.917413	45.139213
3501.408668	380679.471903	45.144218
3501.316762	380677.175368	45.149223
3501.220534	380661.725297	45.154228
3501.308837	380645.154549	45.159233
3501.270951	380623.753122	45.164237
3501.680907	380609.951062	45.169242
3501.035164	380597.557595	45.174247
3501.293995	380582.585505	45.179252
3501.375428	380577.138488	45.184257
3501.473568	380574.025147	45.189261
3501.510230	380546.517419	45.194266
3501.664460	380538.468843	45.199271
3501.205160	380530.718891	45.204276
3501.248582	380514.104255	45.209281
3501.416539	380509.989662	45.214285
3501.222850	380503.747427	45.219290
3501.154356	380490.375278	45.224295
3501.214557	380464.616016	45.229300
3501.491822	380458.986133	45.234305
3501.451506	380452.034370	45.239309
3501.560668	380429.492547	45.244314
3501.230030	380423.373182	45.249319
3501.245232	380407.397731	45.254324
3501.376206	380384.827081	45.259329
3501.290518	380384.916636	45.264333
3501.276844	380379.611350	45.269338
3501.193166	380355.626590	45.274343
3501.211318	380342.469434	45.279348
3500.980669	380335.166340	45.284353
3500.948641	380339.539223	45.289357
3501.028300	380304.507765	45.294362
3501.063967	380304.273701	45.299367
3501.493196	380287.675070	45.304372
3501.191261	380293.029561	45.309377
3500.952725	380272.725644	45.314381
3501.470657	380260.074751	45.319386
3500.964636	380261.194710	45.324391
3501.249732	380252.109897	45.329396
3501.316354	380233.561482	45.334401
3501.336762	380215.020245	45.339405
3501.303244	380216.269837	45.344410
3501.202161	380201.810642	45.349415
3501.495367	380188.712186	45.354420
3501.656052	380179.088024	45.359425
3501.299716	380149.380908	45.364429
3501.669275	380139.648045	45.369434
3501.159169	380136.730882	45.374439
3501.078150	380113.532724	45.379444
3501.114761	380093.973091	45.384449
3501.223598	380088.648682	45.389453
3501.227900	380085.753044	45.394458
3501.278564	380081.682030	45.399463
3501.519410	380057.341761	45.404468
3501.372829	380052.793541	45.409473
3501.290527	380037.391725	45.414477
3501.305230	380013.696083	45.419482
3501.092003	380010.783497	45.424487
3501.280247	380004.456315	45.429492
3501.259457	379991.584386	45.434497
3501.465987	379974.842449	45.439501
3501.489130	379970.013854	45.444506
3501.084270	379950.167284	45.449511
3501.068415	379929.168181	45.454516
3501.205578	379931.711763	45.459521
3500.996990	379930.855436	45.464525
3501.378145	379909.261245	45.469530
3501.098438	379907.654136	45.474535
3501.256180	379881.244249	45.479540
3501.232110	379884.523985	45.484545
3501.213779	379865.861556	45.489549
3500.993314	379856.499749	45.494554
3501.298253	379856.553914	45.499559
3501.506912	379852.991574	45.504564
3501.554237	379832.058748	45.509569
3501.114571	379826.895826	45.514573
3501.327192	379807.562541	45.519578
3500.849811	379791.510998	45.524583
3501.218606	379775.454746	45.529588
3501.139357	379767.899378	45.534593
3500.821617	379769.117034	45.539597
3501.185283	379755.474102	45.544602
3501.013169	379745.317482	45.549607
3501.246027	379734.335986	45.554612
3501.256679	379726.588851	45.559617
3500.998957	379726.349647	45.564621
3501.242748	379706.579720	45.569626
3501.283660	379698.472335	45.574631
3501.523706	379683.578845	45.579636
3501.331999	379675.990160	45.584641
3501.071982	379660.285641	45.589645
3501.203866	379645.485146	45.594650
3501.214514	379642.105963	45.599655
3501.486665	379624.033040	45.604660
3501.441185	379612.586902	45.609665
3501.011936	379600.540202	45.614669
3501.416203	379590.268435	45.619674
3501.185583	379568.083493	45.624679
3501.189492	379579.053683	45.629684
3501.261028	379568.986057	45.634689
3501.418496	379554.460878	45.639693
3501.364593	379527.601063	45.644698
3501.289064	379525.682808	45.649703
3501.359335	379508.555454	45.654708
3501.284166	379498.942351	45.659713
3501.174902	379494.743762	45.664717
3501.526322	379475.947334	45.669722
3501.100281	379464.458770	45.674727
3501.253050	379446.251931	45.679732
3501.018032	379447.685287	45.684737
3501.384106	379433.584698	45.689741
3501.541527	379414.793019	45.694746
3501.695824	379404.864824	45.699751
3501.607703	379371.458150	45.704756
3501.489431	379366.092750	45.709761
3501.340882	379357.633811	45.714765
3501.346983	379331.958047	45.719770
3501.554830	379327.405339	45.724775
3501.852341	379297.849472	45.729780
3501.594301	379290.397976	45.734785
3501.213386	379279.334033	45.739789
3501.758276	379254.615570	45.744794
3501.398623	379246.367215	45.749799
3501.318781	379230.405842	45.754804
3501.062295	379207.640524	45.759809
3501.216401	379213.787718	45.764813
3501.424498	379186.937577	45.769818
3501.346485	379125.466808	45.774823
3500.851024	379022.640322	45.779828
3500.821073	378877.253608	45.784833
3500.141587	378681.251137	45.789837
3500.069087	378456.175543	45.794842
3499.038475	378172.504817	45.799847
3498.361460	377849.512423	45.804852
3497.970073	377491.474261	45.809857
3496.737944	377104.304081	45.814861
3496.221405	376650.448715	45.819866
3495.008349	376191.157216	45.824871
3494.133777	375674.809977	45.829876
3492.937510	375114.841248	45.834881
3491.453335	374530.877358	45.839885
3490.013148	373912.146105	45.844890
3488.588880	373263.348787	45.849895
3487.108945	372573.343071	45.854900
3485.285587	371853.576461	45.859905
3483.735759	371111.622491	45.864909
3482.206244	370331.692277	45.869914
3479.942008	369530.464079	45.874919
3478.494079	368691.181356	45.879924
3476.499872	367825.993814	45.884929
3474.333296	366935.095135	45.889933
3472.269313	366006.447861	45.894938
3469.842665	365076.150312	45.899943
3467.713536	364100.954659	45.904948
3465.784361	363113.828953	45.909953
3463.379428	362098.461811	45.914957
3461.055275	361059.338150	45.919962
3458.287714	360010.133247	45.924967
3455.963929	358926.844735	45.929972
3453.861836	357828.234497	45.934977
3450.969807	356706.579805	45.939981
3448.378866	355556.396654	45.944986
3445.227547	354405.267227	45.949991
3442.600160	353240.135923	45.954996
3439.838699	352061.714065	45.960001
3436.901559	350847.764311	45.965005
3434.253431	349632.885396	45.970010
3431.400046	348410.265170	45.975015
3428.314235	347173.246593	45.980020
3425.406723	345919.654419	45.985025
3422.267867	344646.906837	45.990029
3419.489171	343366.860369	45.995034
3416.080959	342083.152223	46.000039
3413.033590	340777.701767	46.005044
3410.017289	339466.883742	46.010049
3406.311267	338153.505830	46.015053
3403.271026	336820.242551	46.020058
3399.993371	335492.232097	46.025063
3397.240260	334154.860542	46.030068
3393.725470	332798.586653	46.035073
3390.004400	331437.642078	46.040077
3387.025496	330076.457680	46.045082
3383.278284	328698.405015	46.050087
3379.883571	327333.502184	46.055092
3376.777895	325955.280306	46.060097
3372.982305	324570.784887	46.065101
3370.098955	323184.701885	46.070106
3366.366449	321785.883194	46.075111
3363.148510	320382.689677	46.080116
3359.458784	318977.921052	46.085121
3355.648238	317562.312929	46.090125
3352.504506	316151.415670	46.095130
3348.707710	314748.718144	46.100135
3345.420462	313322.845068	46.105140
3341.851905	311908.295589	46.110145
3337.521496	310493.135357	46.115149
3334.471594	309076.512791	46.120154
3330.790652	307655.519473	46.125159
3326.807728	306225.421920	46.130164
3323.343530	304807.699084	46.135169
3319.705379	303384.390777	46.140173
3316.138737	301961.083722	46.145178
3312.590612	300540.102976	46.150183
3309.020658	299108.067789	46.155188
3305.277446	297685.643944	46.160193
3301.567949	296254.321358	46.165197
3298.006928	294828.438412	46.170202
3294.275721	293408.656719	46.175207
3290.299930	291978.315697	46.180212
3287.191334	290556.436139	46.185217
3283.006278	289129.575253	46.190221
3279.569029	287700.835324	46.195226
3275.999548	286281.555273	46.200231
3272.303938	284854.322049	46.205236
3268.627432	283422.142854	46.210241
3265.015533	281997.638802	46.215245
3261.267826	280572.364162	46.220250
3257.413402	279149.981340	46.225255
3253.526688	277720.091671	46.230260
3250.015707	276292.969180	46.235265
3245.817887	274884.871791	46.240269
3242.254660	273455.492902	46.245274
3238.195554	272053.335723	46.250279
3234.667020	270637.629351	46.255284
3231.202838	269233.553102	46.260289
3227.033236	267817.012123	46.265293
3223.533513	266414.707911	46.270298
3219.469560	265009.263447	46.275303
3216.070094	263606.141218	46.280308
3212.534036	262206.485253	46.285313
3208.292167	260817.056829	46.290317
3204.853979	259424.838370	46.295322
3200.785688	258031.632442	46.300327
3197.225336	256627.279863	46.305332
3193.345830	255250.338409	46.310337
3189.718283	253864.074227	46.315341
3186.094651	252476.242753	46.320346
3182.121004	251105.337836	46.325351
3178.456238	249722.658256	46.330356
3174.529304	248344.872565	46.335361
3170.672689	246970.248909	46.340365
3167.375545	245599.603251	46.345370
3163.385171	244243.063766	46.350375
3159.750816	242860.483044	46.355380
3156.027340	241504.879134	46.360385
3151.858338	240151.960733	46.365389
3148.705366	238780.082002	46.370394
3144.615988	237427.546366	46.375399
3140.863149	236072.202524	46.380404
3137.033220	234738.947520	46.385409
3133.090947	233386.910063	46.390413
3129.662854	232026.537250	46.395418
3125.328546	230686.244855	46.400423
3121.967131	229352.955704	46.405428
3118.172639	228027.169358	46.410433
3113.945236	226693.808693	46.415437
3110.544502	225366.558910	46.420442
3106.769696	224059.360731	46.425447
3103.015364	222725.315715	46.430452
3099.246245	221400.137547	46.435457
3095.184989	220087.817613	46.440461
3091.619742	218771.118644	46.445466
3087.397057	217472.327686	46.450471
3084.060943	216164.004212	46.455476
3080.752282	214879.213571	46.460481
3076.104876	213587.478983	46.465485
3072.844649	212293.139468	46.470490
3068.733354	211010.016671	46.475495
3064.969539	209724.553606	46.480500
3061.472152	208431.797154	46.485505
3057.308854	207167.140744	46.490509
3053.538390	205889.416420	46.495514
3049.749507	204631.313021	46.500519
3046.393162	203367.649520	46.505524
3042.098147	202115.830352	46.510529
3038.240891	200857.585352	46.515533
3034.649229	199611.914811	46.520538
3031.000734	198371.356397	46.525543
3026.936929	197131.025733	46.530548
3023.538928	195883.802747	46.535553
3019.336654	194661.622099	46.540557
3015.586165	193433.550851	46.545562
3012.075501	192207.771588	46.550567
3008.228926	190990.460493	46.555572
3004.509573	189768.456652	46.560577
3000.805992	188564.645354	46.565581
2996.898419	187342.035292	46.570586
2992.942854	186146.031361	46.575591
2989.533589	184942.775481	46.580596
2985.718054	183738.349581	46.585601
2981.405212	182560.981582	46.590605
2977.997983	181363.702626	46.595610
2973.788356	180183.751373	46.600615
2970.062771	179012.295656	46.605620
2966.200918	177839.680149	46.610625
2962.317728	176681.227999	46.615629
2959.032700	175517.683041	46.620634
2954.612391	174367.100021	46.625639
2950.599181	173214.509863	46.630644
2947.241677	172085.118015	46.635649
2942.950819	170957.033871	46.640653
2939.421746	169823.374515	46.645658
2935.324994	168697.777023	46.650663
2931.575907	167571.583056	46.655668
2927.494238	166459.664549	46.660673
2922.728985	165373.035321	46.665677
2919.205078	164282.055398	46.670682
2915.531908	163201.184825	46.675687
2911.425631	162123.607073	46.680692
2907.865465	161052.606466	46.685697
2903.624390	159998.161591	46.690701
2900.009974	158946.475369	46.695706
2895.896223	157904.583210	46.700711
2891.855611	156870.435825	46.705716
2888.332007	155827.953552	46.710721
2884.223114	154806.452753	46.715725
2880.337765	153789.084144	46.720730
2876.037066	152794.412952	46.725735
2871.934526	151793.811030	46.730740
2867.907713	150814.874756	46.735745
2863.471769	149837.572279	46.740749
2859.672425	148869.834311	46.745754
2855.175285	147919.757763	46.750759
2851.274596	146985.638954	46.755764
2847.290411	146062.289587	46.760769
2842.697529	145152.272267	46.765773
2838.563332	144259.123103	46.770778
2833.927567	143377.977562	46.775783
2829.602854	142507.449072	46.780788
2825.226948	141670.012426	46.785793
2820.861198	140799.444509	46.790797
2816.545972	139934.024643	46.795802
2811.778705	139142.394245	46.800807
2807.707844	138357.678964	46.805812
2803.432939	137596.405165	46.810817
2798.351352	136852.953316	46.815821
2794.378733	136132.075185	46.820826
2789.740897	135409.327407	46.825831
2785.466439	134719.216482	46.830836
2781.633856	134034.123284	46.835841
2777.184900	133365.928591	46.840845
2773.219288	132701.434237	46.845850
2768.830815	132075.089269	46.850855
2764.577015	131446.239121	46.855860
2761.079024	130838.002183	46.860865
2756.630721	130241.560838	46.865869
2753.424412	129642.555899	46.870874
2749.365209	129054.224275	46.875879
2745.693094	128479.565277	46.880884
2742.308801	127896.487162	46.885889
2738.282464	127339.299411	46.890893
2735.253171	126758.573299	46.895898
2731.256997	126208.226379	46.900903
2727.075696	125654.036411	46.905908
2723.977978	125101.987463	46.910913
2719.828454	124555.769494	46.915917
2716.911514	124014.912351	46.920922
2713.476687	123467.962058	46.925927
2709.806372	122924.108262	46.930932
2706.288216	122382.578351	46.935937
2702.848422	121855.503715	46.940941
2699.295000	121317.046237	46.945946
2696.078470	120779.548445	46.950951
2692.504099	120252.859804	46.955956
2689.415166	119711.312945	46.960961
2685.080629	119184.159540	46.965965
2682.057720	118641.905398	46.970970
2678.411888	118107.614708	46.975975
2675.404358	117575.622900	46.980980
2671.597778	117044.487784	46.985985
2667.661501	116511.600165	46.990989
2664.453543	115975.415183	46.995994
2660.715240	115451.400269	47.000999
2657.085306	114924.336965	47.006004
2653.922674	114388.142580	47.011009
2650.261298	113859.993274	47.016013
2646.478076	113335.240033	47.021018
2642.871635	112814.688154	47.026023
2639.465072	112294.659420	47.031028
2635.963124	111772.834934	47.036033
2632.181307	111259.732642	47.041037
2628.808166	110736.606469	47.046042
2624.229105	110222.613444	47.051047
2620.723843	109719.267324	47.056052
2617.032344	109208.825232	47.061057
2613.541960	108723.289826	47.066061
2610.695687	108224.108926	47.071066
2606.466217	107731.239917	47.076071
2602.375438	107249.289238	47.081076
2598.966019	106748.590147	47.086081
2594.974503	106277.138192	47.091085
2591.629573	105793.515670	47.096090
2587.502607	105319.059919	47.101095
2583.960641	104851.002783	47.106100
2580.098096	104393.400107	47.111105
2576.318324	103938.307660	47.116109
2572.381411	103472.695579	47.121114
2568.572753	103027.089937	47.126119
2564.739983	102590.378943	47.131124
2561.125638	102153.398238	47.136129
2557.311295	101715.704548	47.141133
2553.834113	101281.879032	47.146138
2550.326946	100863.468703	47.151143
2546.331097	100427.866881	47.156148
2543.134874	100006.419646	47.161153
2539.591233	99591.946052	47.166157
2536.264590	99161.760466	47.171162
2532.401546	98736.137820	47.176167
2528.724973	98325.069267	47.181172
2525.302949	97910.357040	47.186177
2521.995049	97493.497380	47.191181
2518.692369	97075.854458	47.196186
2515.367951	96663.202190	47.201191
2511.588670	96246.114657	47.206196
2508.154201	95824.378650	47.211201
2504.812410	95411.275366	47.216205
2501.367802	94986.642128	47.221210
2498.042636	94573.051788	47.226215
2494.476870	94151.587644	47.231220
2491.135668	93729.547897	47.236225
2487.323767	93311.869509	47.241229
2484.076804	92880.703031	47.246234
2480.773255	92471.318201	47.251239
2477.309203	92054.352578	47.256244
2474.367485	91617.959463	47.261249
2470.455572	91191.532868	47.266253
2467.253255	90759.678022	47.271258
2463.612903	90335.038270	47.276263
2459.928498	89902.381372	47.281268
2456.733412	89465.525290	47.286273
2452.817933	89055.189469	47.291277
2449.683086	88610.827704	47.296282
2446.141816	88190.306897	47.301287
2442.756076	87753.251630	47.306292
2439.557905	87320.112101	47.311297
2435.839104	86884.341249	47.316301
2432.602368	86445.325817	47.321306
2428.924198	86016.142412	47.326311
2425.510138	85570.879274	47.331316
2421.881993	85126.888561	47.336321
2418.569595	84702.685664	47.341325
2415.721964	84256.401904	47.346330
2411.810113	83812.310500	47.351335
2408.290955	83367.186765	47.356340
2404.689462	82928.205495	47.361345
2401.202002	82481.070971	47.366349
2397.989154	82038.816558	47.371354
2393.961676	81590.471831	47.376359
2390.686392	81143.300082	47.381364
2387.315659	80697.725327	47.386369
2383.542321	80258.647280	47.391373
2380.508455	79809.681085	47.396378
2376.912671	79359.907817	47.401383
2373.307307	78913.394767	47.406388
2370.163910	78457.583664	47.411393
2366.567538	78009.813786	47.416397
2362.719382	77561.709392	47.421402
2359.162097	77104.956451	47.426407
2355.950923	76660.361826	47.431412
2352.570970	76202.402644	47.436417
2348.850298	75760.784855	47.441421
2345.610152	75303.416000	47.446426
2342.376670	74836.301062	47.451431
2338.720285	74388.714551	47.456436
2335.225904	73918.430720	47.461441
2331.480418	73475.127384	47.466445
2328.173594	73007.420898	47.471450
2325.050483	72550.258700	47.476455
2321.222875	72094.813948	47.481460
2317.723886	71630.932913	47.486465
2314.068847	71177.280214	47.491469
2310.393849	70707.792624	47.496474
2306.870360	70259.087198	47.501479
2303.609111	69795.125524	47.506484
2300.385978	69329.566467	47.511489
2296.524937	68873.535556	47.516493
2293.039749	68416.768632	47.521498
2289.669057	67958.157472	47.526503
2286.410889	67498.165889	47.531508
2283.009697	67025.414430	47.536513
2279.228201	66564.797466	47.541517
2276.104415	66096.767978	47.546522
2272.557840	65630.545719	47.551527
2269.021714	65163.486261	47.556532
2265.259863	64691.869003	47.561537
2261.250750	64223.269417	47.566541
2258.019622	63755.242970	47.571546
2254.921014	63293.018195	47.576551
2251.155959	62817.977820	47.581556
2248.333605	62353.138122	47.586561
2244.346762	61886.203704	47.591565
2241.044356	61413.625041	47.596570
2237.348447	60951.581323	47.601575
2234.023043	60468.077465	47.606580
2230.647633	59986.824658	47.611585
2226.766116	59519.176398	47.616589
2223.763710	59047.059945	47.621594
2220.093541	58576.230499	47.626599
2216.675829	58109.063895	47.631604
2213.061832	57626.207156	47.636609
2209.335873	57149.151534	47.641613
2206.008554	56674.816092	47.646618
2202.580933	56191.610240	47.651623
2198.782050	55716.187081	47.656628
2195.759570	55243.996173	47.661633
2192.196662	54770.198458	47.666637
2188.706031	54275.824424	47.671642
2184.851432	53800.683116	47.676647
2181.494901	53320.703176	47.681652
2178.177495	52852.659861	47.686657
2174.616617	52377.209855	47.691661
2171.235638	51887.614231	47.696666
2167.658099	51415.009381	47.701671
2164.160302	50931.567241	47.706676
2160.863092	50443.670051	47.711681
2157.331868	49962.397415	47.716685
2153.807444	49480.645381	47.721690
2150.402838	48991.013333	47.726695
2146.796437	48514.165696	47.731700
2143.480032	48015.496112	47.736705
2139.870929	47533.931506	47.741709
2136.527047	47047.610825	47.746714
2132.809602	46560.927468	47.751719
2128.977166	46075.376023	47.756724
2125.847346	45588.146578	47.761729
2122.355760	45104.687604	47.766733
2118.880451	44613.049503	47.771738
2115.487837	44130.160618	47.776743
2111.976977	43632.835997	47.781748
2108.384547	43140.798418	47.786753
2104.691618	42647.766509	47.791757
2101.323684	42164.085946	47.796762
2097.714950	41670.878903	47.801767
2094.556943	41181.366456	47.806772
2090.783691	40682.906473	47.811777
2087.113825	40197.686784	47.816781
2083.791224	39705.348186	47.821786
2080.439162	39223.581555	47.826791
2076.942346	38732.832789	47.831796
2073.727180	38235.020519	47.836801
2069.649803	37744.131013	47.841805
2066.183885	37240.896989	47.846810
2062.917525	36743.292082	47.851815
2059.008944	36252.385137	47.856820
2055.750095	35759.055614	47.861825
2051.846994	35276.962586	47.866829
2048.628609	34790.799557	47.871834
2045.246422	34296.578789	47.876839
2041.801901	33802.100412	47.881844
2038.278046	33311.518719	47.886849
2034.767216	32817.954857	47.891853
2031.129911	32321.335708	47.896858
2027.935101	31831.586801	47.901863
2023.930584	31337.608746	47.906868
2020.486628	30851.458154	47.911873
2017.255058	30355.133378	47.916877
2013.882525	29855.743543	47.921882
2010.185251	29374.762297	47.926887
2006.803516	28868.946666	47.931892
2003.222330	28378.002685	47.936897
1999.632794	27885.297531	47.941901
1996.160170	27395.969782	47.946906
1992.510454	26901.910096	47.951911
1989.205654	26406.395793	47.956916
1986.059130	25918.446893	47.961921
1981.801218	25417.896939	47.966925
1978.454143	24923.838515	47.971930
1974.537147	24435.608302	47.976935
1971.119836	23958.582940	47.981940
1967.839749	23465.025225	47.986945
1963.873201	22973.411078	47.991949
1960.629956	22482.120961	47.996954
1957.012024	22002.462334	48.001959
1953.337052	21525.009668	48.006964
1949.696111	21027.216869	48.011969
1946.168698	20549.891546	48.016973
1942.814782	20074.717111	48.021978
1939.001764	19588.927480	48.026983
1935.240673	19117.937761	48.031988
1932.323477	18638.518242	48.036993
1928.619989	18170.221637	48.041997
1924.958898	17695.114985	48.047002
1921.642711	17207.530971	48.052007
1917.742811	16739.416706	48.057012
1914.433851	16264.018121	48.062017
1910.319675	15798.841568	48.067021
1907.065790	15327.282600	48.072026
1903.493905	14856.228013	48.077031
1899.617974	14404.501621	48.082036
1896.102812	13932.707467	48.087041
1892.284646	13483.362183	48.092045
1888.491476	13030.446151	48.097050
1884.663774	12584.489060	48.102055
1880.605536	12146.239583	48.107060
1876.995394	11708.627017	48.112065
1873.025897	11293.825691	48.117069
1868.600923	10870.183845	48.122074
1864.264326	10452.859336	48.127079
1860.566472	10049.942413	48.132084
1856.935890	9649.229983	48.137089
1853.120537	9254.654463	48.142093
1849.250423	8869.901730	48.147098
1845.638404	8492.586606	48.152103
1841.510005	8126.323460	48.157108
1838.314861	7761.890984	48.162113
1834.310553	7401.921336	48.167117
1831.180269	7035.954938	48.172122
1827.374592	6672.778406	48.177127
1823.905104	6329.352528	48.182132
1820.529669	5967.373102	48.187137
1816.581065	5617.329083	48.192141
1813.157531	5263.643539	48.197146
1809.552005	4928.752646	48.202151
1805.558043	4577.397054	48.207156
1802.415112	4236.393242	48.212161
1798.289012	3905.877376	48.217165
1795.231979	3570.068633	48.222170
1791.771740	3235.256006	48.227175
1788.236366	2909.529881	48.232180
1784.257697	2579.910798	48.237185
1780.420849	2264.112234	48.242189
1776.779405	1944.400212	48.247194
1772.746328	1641.109438	48.252199
1768.409750	1353.019916	48.257204
1763.970514	1076.435892	48.262209
1758.941773	830.611769	48.267213
1754.498604	589.977109	48.272218
1750.240426	368.840422	48.277223
1745.022483	165.126588	48.282228
1737.309389	66.160926	48.287233
1726.044478	94.489332	48.292237
1718.832117	97.054554	48.297242
1714.773608	98.423404	48.302247
1712.209450	99.208500	48.307252
1710.376215	95.248173	48.312257
1707.823303	103.026470	48.317261
1705.854279	99.017675	48.322266
1703.268239	87.201984	48.327271
1699.871979	100.701802	48.332276
1696.961306	95.570922	48.337281
1693.332089	102.219618	48.342285
1690.256871	92.482687	48.347290
1687.245880	91.303070	48.352295
1683.282893	94.207269	48.357300
1679.874432	88.277525	48.362305
1676.790528	87.245296	48.367309
1673.867554	95.707600	48.372314
1670.338228	89.961181	48.377319
1666.733089	92.148471	48.382324
1663.150050	83.945891	48.387329
1659.793562	94.364397	48.392333
1656.614151	92.337814	48.397338
1653.199000	96.782892	48.402343
1650.134488	96.200057	48.407348
1646.492261	89.923892	48.412353
1643.149502	99.334207	48.417357
1639.561134	99.158768	48.422362
1636.529264	88.969019	48.427367
1632.865398	88.020734	48.432372
1629.357596	79.496409	48.437377
1625.765710	84.677662	48.442381
1622.537690	91.972582	48.447386
1619.073701	92.030883	48.452391
1615.382000	86.062976	48.457396
1612.512219	91.346973	48.462401
1608.575210	87.913407	48.467405
1604.796977	82.256359	48.472410
1601.650655	86.124931	48.477415
1598.080740	94.096315	48.482420
1595.144489	89.466132	48.487425
1591.673083	97.510769	48.492429
1588.029569	89.836458	48.497434
1584.597602	93.496395	48.502439
1581.365229	87.045721	48.507444
1577.635651	79.188662	48.512449
1573.903947	88.672164	48.517453
1570.457211	88.670837	48.522458
1566.921220	79.518170	48.527463
1563.274557	98.017634	48.532468
1559.911787	91.448054	48.537473
1556.479208	98.566012	48.542477
1553.289569	88.682403	48.547482
1550.489026	84.986541	48.552487
1546.616895	89.708390	48.557492
1542.765557	80.614300	48.562497
1539.451065	80.456355	48.567501
1535.916087	82.003159	48.572506
1532.276154	85.983363	48.577511
1529.037036	86.471736	48.582516
1525.976735	79.013544	48.587521
1522.227708	84.883638	48.592525
1518.122151	83.232171	48.597530
1514.699471	90.940198	48.602535
1511.230352	94.972912	48.607540
1508.097607	73.694318	48.612545
1504.548646	87.028066	48.617549
1500.867436	76.717956	48.622554
1497.989976	91.067139	48.627559
1494.416796	81.556447	48.632564
1490.680962	84.203847	48.637569
1486.781150	89.157795	48.642573
1483.751925	86.399187	48.647578
1480.262251	80.814302	48.652583
1476.437011	91.492424	48.657588
1473.227058	91.511198	48.662593
1469.779091	83.123115	48.667597
1465.880794	92.749608	48.672602
1462.797024	89.249695	48.677607
1459.343865	91.166578	48.682612
1456.077511	80.269894	48.687617
1452.204283	80.404562	48.692621
1448.836738	77.980187	48.697626
1445.168565	81.572494	48.702631
1441.997221	88.187893	48.707636
1438.518867	76.919258	48.712641
1434.751068	83.852115	48.717645
1431.004059	87.304837	48.722650
1427.958760	87.721923	48.727655
1424.301331	92.578039	48.732660
1420.892293	88.651041	48.737665
1417.500410	87.625645	48.742669
1413.545705	79.208881	48.747674
1410.426108	88.559149	48.752679
1406.809500	71.924272	48.757684
1403.377078	81.709197	48.762689
1399.471338	85.034771	48.767693
1396.195351	94.896592	48.772698
1392.835532	82.321889	48.777703
1389.073993	92.654747	48.782708
1386.171565	85.039126	48.787713
1382.443492	85.616271	48.792717
1378.956196	89.525274	48.797722
1375.462485	76.196314	48.802727
1371.990969	81.991584	48.807732
1368.575362	73.551031	48.812737
1364.541072	80.016014	48.817741
1361.058944	79.808249	48.822746
1357.921297	79.429810	48.827751
1354.497879	79.753899	48.832756
1351.161462	73.502952	48.837761
1347.247198	81.651321	48.842765
1343.622820	87.982904	48.847770
1340.927625	83.732841	48.852775
1336.545357	87.872896	48.857780
1333.676545	82.223032	48.862785
1329.981879	86.898291	48.867789
1325.857651	83.765984	48.872794
1323.267219	78.711858	48.877799
1319.592265	73.658866	48.882804
1315.899063	79.368423	48.887809
1312.347641	87.491955	48.892813
1309.072456	75.704515	48.897818
1305.677302	75.467400	48.902823
1301.623672	83.017381	48.907828
1298.513342	74.247755	48.912833
1294.795413	83.188125	48.917837
1291.109599	77.611654	48.922842
1288.025945	74.437607	48.927847
1284.463773	74.862393	48.932852
1281.251617	73.274375	48.937857
1277.185196	80.658672	48.942861
1273.711281	74.783471	48.947866
1270.478417	74.435680	48.952871
1267.012812	84.067589	48.957876
1263.991688	79.842958	48.962881
1260.506661	82.422865	48.967885
1256.798110	76.157090	48.972890
1253.294932	69.166505	48.977895
1249.207280	76.604725	48.982900
1245.802509	75.628810	48.987905
1241.930175	72.077668	48.992909
1238.622467	75.901778	48.997914
1235.410714	73.671474	49.002919
1231.544832	80.024833	49.007924
1228.759420	73.454027	49.012929
1225.470190	73.934408	49.017933
1221.639167	85.502428	49.022938
1218.506277	79.067963	49.027943
1214.264185	81.784696	49.032948
1210.930737	68.187229	49.037953
1206.945918	81.952638	49.042957
1203.977999	75.239403	49.047962
1200.740757	70.798491	49.052967
1196.910754	73.938289	49.057972
1193.793329	61.038018	49.062977
1189.920174	69.743126	49.067981
1186.044947	64.642238	49.072986
1182.631602	73.038500	49.077991
1179.305663	73.043720	49.082996
1176.224887	67.528114	49.088001
1172.720961	69.142881	49.093005
1169.091996	74.092653	49.098010
1165.511856	68.550376	49.103015
1161.944396	76.976956	49.108020
1158.690614	76.379337	49.113025
1154.802111	78.784779	49.118029
1151.225877	75.415345	49.123034
1148.169427	63.894449	49.128039
1144.355792	74.203774	49.133044
1141.009895	61.544717	49.138049
1137.510059	74.295016	49.143053
1133.821360	78.940885	49.148058
1130.694258	67.108292	49.153063
1126.779228	78.423635	49.158068
1123.387400	65.173792	49.163073
1120.230267	71.087811	49.168077
1116.412037	70.970354	49.173082
1112.762064	66.558899	49.178087
1109.347780	75.869615	49.183092
1105.911590	67.087474	49.188097
1102.281424	78.140183	49.193101
1098.878572	73.554224	49.198106
1095.865644	60.995205	49.203111
1091.748130	64.768209	49.208116
1088.570817	72.846166	49.213121
1085.015727	77.347858	49.218125
1081.215710	79.179562	49.223130
1078.027328	78.290204	49.228135
1074.184338	78.486647	49.233140
1070.686538	76.569801	49.238145
1067.348514	82.056413	49.243149
1063.909670	76.577574	49.248154
1060.759280	71.303768	49.253159
1057.181343	82.870358	49.258164
1053.307167	70.024632	49.263169
1049.752374	77.765890	49.268173
1046.386587	81.349125	49.273178
1043.017818	84.980279	49.278183
1038.951434	92.424699	49.283188
1035.861214	82.120760	49.288193
1032.352026	79.348334	49.293197
1028.814065	70.098004	49.298202
1025.545760	68.847779	49.303207
1021.685168	75.263601	49.308212
1018.262351	80.197115	49.313217
1014.855503	74.403264	49.318221
1011.178924	79.550282	49.323226
1007.985316	69.388997	49.328231
1004.651702	76.754150	49.333236
1000.998288	64.354956	49.338241
997.332808	69.765994	49.343245
994.053152	70.725788	49.348250
990.317542	71.592045	49.353255
986.615479	77.815518	49.358260
983.342360	75.522032	49.363265
979.637707	69.537269	49.368269
976.248126	74.861071	49.373274
973.163211	72.244068	49.378279
969.230034	80.376418	49.383284
965.756499	68.892005	49.388289
962.599922	69.617513	49.393293
958.453391	68.905790	49.398298
955.600309	73.133703	49.403303
951.987885	82.117774	49.408308
948.635937	74.224195	49.413313
945.055359	70.978851	49.418317
941.194519	76.695545	49.423322
937.361054	81.601241	49.428327
933.918718	84.136568	49.433332
931.166735	76.206545	49.438337
927.734134	77.560304	49.443341
923.997724	79.496017	49.448346
920.178933	69.485850	49.453351
916.705339	77.904156	49.458356
913.242452	70.192366	49.463361
909.827152	75.855526	49.468365
906.639244	73.033107	49.473370
902.981552	75.367846	49.478375
898.639821	74.721317	49.483380
895.559453	72.296601	49.488385
892.236149	73.981354	49.493389
889.063452	71.415991	49.498394
885.522821	74.741723	49.503399
881.447411	74.813022	49.508404
878.283522	68.313839	49.513409
874.889624	69.797616	49.518413
870.968670	74.998503	49.523418
867.478999	73.839701	49.528423
864.407534	76.083190	49.533428
861.213474	70.243587	49.538433
857.366474	76.265010	49.543437
853.470005	74.479853	49.548442
849.879233	72.466780	49.553447
846.749208	76.668211	49.558452
843.748527	80.140844	49.563457
840.241992	66.997503	49.568461
835.868476	80.190686	49.573466
832.627894	74.769606	49.578471
829.137798	77.957766	49.583476
825.812977	75.004813	49.588481
822.147408	70.048516	49.593485
818.538670	71.125992	49.598490
815.039043	74.733242	49.603495
811.655815	73.814135	49.608500
808.462028	73.858934	49.613505
805.117595	70.614816	49.618509
800.937045	70.110886	49.623514
797.905370	62.993203	49.628519
793.872885	72.621618	49.633524
790.623690	65.803544	49.638529
787.458159	68.283139	49.643533
783.849471	67.728156	49.648538
780.092375	59.688881	49.653543
776.377257	70.602961	49.658548
773.192477	65.812269	49.663553
769.879325	61.607860	49.668557
766.485813	75.490023	49.673562
763.361166	68.987914	49.678567
759.224757	77.199367	49.683572
756.105575	72.464901	49.688577
752.286339	74.540073	49.693581
748.757415	71.372138	49.698586
745.153573	70.490547	49.703591
741.381348	64.519511	49.708596
738.536869	65.724791	49.713601
734.411277	64.946568	49.718605
730.538256	68.390493	49.723610
727.778368	63.865852	49.728615
723.701311	71.783336	49.733620
720.645172	63.521061	49.738625
717.150961	67.497625	49.743629
713.041527	72.262806	49.748634
710.193712	65.268372	49.753639
706.740231	66.166672	49.758644
703.474129	69.598377	49.763649
699.605085	67.590681	49.768653
695.921985	64.769451	49.773658
692.774648	57.315462	49.778663
688.739982	75.805663	49.783668
685.559487	66.132772	49.788673
682.303215	74.026889	49.793677
679.094158	66.892546	49.798682
675.386637	64.900838	49.803687
671.669691	66.213469	49.808692
667.852066	67.690467	49.813697
664.463332	71.005228	49.818701
660.977797	75.303142	49.823706
657.610013	65.959961	49.828711
654.052304	73.258779	49.833716
650.544345	66.699306	49.838721
646.869043	63.437119	49.843725
644.067500	63.354438	49.848730
640.126068	64.300233	49.853735
636.363187	69.441732	49.858740
632.990028	68.255334	49.863745
629.320413	76.833880	49.868749
626.031330	68.854649	49.873754
622.781893	58.816030	49.878759
619.205070	68.009697	49.883764
615.728039	63.992170	49.888769
612.014971	69.040497	49.893773
608.557368	70.888552	49.898778
604.725570	58.267296	49.903783
601.484079	66.336277	49.908788
598.284660	63.828897	49.913793
594.541598	58.214009	49.918797
590.974582	69.010130	49.923802
587.540876	67.190939	49.928807
583.871997	69.764729	49.933812
580.840042	67.525502	49.938817
577.462101	73.515055	49.943821
573.168961	66.657060	49.948826
569.839824	59.490815	49.953831
566.200099	67.988780	49.958836
562.920211	71.871885	49.963841
559.761484	61.610354	49.968845
555.999570	66.179086	49.973850
552.678734	61.033134	49.978855
549.025216	76.708446	49.983860
545.524823	70.796364	49.988865
542.198419	70.485363	49.993869
538.542220	81.390286	49.998874
535.080853	70.593755	50.003879
531.311356	73.455291	50.008884
527.515456	67.642999	50.013889
524.560470	68.878158	50.018893
520.769155	73.698237	50.023898
517.519287	62.647332	50.028903
514.035673	71.111508	50.033908
510.775311	63.023429	50.038913
507.001194	67.258717	50.043917
503.598126	72.587817	50.048922
500.274903	64.550654	50.053927
496.106308	64.889610	50.058932
493.081117	62.146319	50.063937
489.293542	59.202186	50.068941
485.805874	66.259162	50.073946
482.628286	58.218315	50.078951
479.048563	64.153866	50.083956
475.360882	68.040353	50.088961
471.873242	62.445833	50.093965
468.231911	68.137884	50.098970
465.039971	55.458181	50.103975
461.318188	60.893844	50.108980
457.680969	60.257929	50.113985
454.597759	65.277815	50.118989
450.700396	64.691890	50.123994
447.499044	57.246356	50.128999
443.910438	56.052397	50.134004
440.849688	62.732874	50.139009
436.871421	62.896680	50.144013
433.372520	64.890384	50.149018
429.811352	56.770063	50.154023
426.053662	67.118161	50.159028
422.775589	59.412498	50.164033
419.597745	62.308484	50.169037
415.736125	59.878913	50.174042
412.429959	51.408860	50.179047
408.898943	62.718221	50.184052
404.939200	61.259353	50.189057
402.068159	68.049501	50.194061
398.065469	66.502410	50.199066
394.665318	57.781241	50.204071
391.388995	67.159086	50.209076
388.301936	60.088061	50.214081
384.345799	58.691909	50.219085
380.684531	62.685022	50.224090
377.316258	61.618117	50.229095
373.671263	65.083530	50.234100
370.250176	68.621649	50.239105
367.160130	63.908020	50.244109
363.471786	59.626050	50.249114
359.864496	57.707371	50.254119
356.094598	62.562095	50.259124
352.860503	62.793551	50.264129
349.300032	63.309931	50.269133
345.436606	66.211420	50.274138
342.249570	66.422897	50.279143
339.190075	63.922243	50.284148
335.246508	66.200316	50.289153
331.917806	63.716265	50.294157
328.251612	64.094087	50.299162
324.761235	59.597811	50.304167
320.957425	67.792316	50.309172
317.687033	66.931638	50.314177
314.421679	61.470215	50.319181
310.679757	70.262510	50.324186
306.962422	61.767903	50.329191
303.520412	74.116917	50.334196
300.152761	71.268785	50.339201
297.030782	67.673747	50.344205
293.376324	63.911680	50.349210
289.582373	60.266242	50.354215
285.994858	68.085401	50.359220
282.750102	67.100517	50.364225
279.703448	63.098298	50.369229
275.782572	63.588542	50.374234
272.496808	59.832353	50.379239
268.707542	69.508355	50.384244
265.154808	68.577748	50.389249
261.801838	70.295662	50.394253
258.185205	60.187741	50.399258
254.926074	58.439495	50.404263
250.812854	61.895562	50.409268
247.609037	60.404452	50.414273
244.152404	59.724636	50.419277
240.565474	64.626814	50.424282
237.266038	51.464046	50.429287
233.644226	58.206575	50.434292
229.990752	61.521468	50.439297
226.738868	59.522168	50.444301
223.293057	67.104142	50.449306
219.771423	58.594906	50.454311
215.757017	63.142874	50.459316
212.833674	54.942280	50.464321
209.389835	61.647613	50.469325
205.392403	60.545813	50.474330
202.192695	51.701736	50.479335
198.697671	59.338825	50.484340
195.323972	50.376310	50.489345
191.745381	56.704001	50.494349
187.928767	52.008615	50.499354
184.586951	58.321590	50.504359
181.028870	62.393569	50.509364
177.908760	59.769503	50.514369
174.520597	58.604488	50.519373
170.687168	62.504209	50.524378
167.085741	57.765832	50.529383
163.315822	66.530858	50.534388
159.916926	66.126793	50.539393
156.631373	64.610458	50.544397
153.006646	73.352883	50.549402
149.665541	64.239768	50.554407
146.034287	63.153732	50.559412
142.698833	57.981657	50.564417
139.365941	57.443936	50.569421
135.515182	68.046980	50.574426
132.294270	57.864826	50.579431
128.254191	63.191897	50.584436
124.938728	58.079985	50.589441
121.494501	48.989267	50.594445
117.951823	61.869627	50.599450
114.689694	52.222227	50.604455
111.061457	67.422215	50.609460
107.627991	62.376132	50.614465
104.106032	56.824990	50.619469
100.456182	56.732080	50.624474
97.282675	55.539984	50.629479
93.790817	58.937295	50.634484
90.140335	56.430618	50.639489
86.567301	48.271095	50.644493
82.474304	60.243750	50.649498
79.289225	54.298489	50.654503
75.977932	60.106865	50.659508
72.078152	60.112981	50.664513
69.245176	59.557546	50.669517
65.235736	69.236206	50.674522
62.149968	62.095440	50.679527
58.483657	60.537165	50.684532
55.301988	52.424277	50.689537
51.700192	58.752432	50.694541
47.979875	51.444723	50.699546
44.252295	50.025701	50.704551
40.783629	56.731748	50.709556
37.716636	55.665441	50.714561
33.835840	54.814423	50.719565
30.402810	66.440730	50.724570
26.981663	61.921075	50.729575
23.297945	65.256521	50.734580
19.930229	63.132923	50.739585
16.614379	54.408203	50.744589
12.982422	59.124433	50.749594
9.692839	57.210128	50.754599
5.736589	60.217860	50.759604
2.479592	53.768137	50.764609