Fri Aug 26 11:52:37 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.239256	99.827736	0.000000
1.275425	109.952171	0.005005
1.229512	107.991558	0.010010
1.725116	102.324246	0.015014
1.413682	95.169124	0.020019
1.444713	84.088371	0.025024
0.675581	90.323500	0.030029
0.622443	74.760306	0.035034
0.608977	71.510202	0.040038
0.255458	66.721728	0.045043
0.271870	61.964241	0.050048
-0.231662	66.174401	0.055053
-0.133724	52.552331	0.060058
-0.761438	42.795337	0.065062
-0.975723	36.868425	0.070067
-0.942792	31.409209	0.075072
-1.270219	27.553122	0.080077
-1.578587	23.485268	0.085082
-2.167005	18.448653	0.090086
-2.752277	18.688503	0.095091
-2.553576	14.045011	0.100096
-2.811063	14.221171	0.105101
-3.304874	12.925070	0.110106
-4.015681	15.190215	0.115110
-4.047101	5.017709	0.120115
-4.243115	10.097432	0.125120
-4.507017	15.826781	0.130125
-4.149445	11.446446	0.135130
-4.942216	6.542887	0.140134
-5.207593	12.013047	0.145139
-5.257603	9.898065	0.150144
-5.421813	7.905263	0.155149
-6.014551	7.250966	0.160154
-6.567437	12.338798	0.165158
-7.049408	8.152450	0.170163
-6.930782	6.685068	0.175168
-7.285945	12.495062	0.180173
-6.881219	3.735235	0.185178
-7.448323	1.928546	0.190182
-7.111295	3.290252	0.195187
-7.504344	0.716172	0.200192
-8.407507	12.761602	0.205197
-8.302264	8.721100	0.210202
-8.693974	6.899757	0.215206
-8.798047	15.049715	0.220211
-9.379819	5.333044	0.225216
-9.617200	10.498298	0.230221
-10.009415	6.908558	0.235226
-10.241956	5.821707	0.240230
-10.092937	5.877630	0.245235
-10.206141	6.382490	0.250240
-10.495352	7.927119	0.255245
-10.645354	0.440029	0.260250
-11.167197	3.640660	0.265254
-11.529667	1.169383	0.270259
-11.215917	4.530970	0.275264
-12.278847	8.303049	0.280269
-12.538777	0.972274	0.285274
-12.930771	4.016652	0.290278
-12.893439	10.951899	0.295283
-13.077259	4.080655	0.300288
-12.928048	10.387901	0.305293
-13.089511	-4.579410	0.310298
-13.379644	0.530781	0.315302
-14.165108	3.146058	0.320307
-14.210307	-0.235128	0.325312
-14.606961	10.639984	0.330317
-14.764341	3.568478	0.335322
-14.847757	13.882312	0.340326
-14.986183	4.020687	0.345331
-15.412608	1.635294	0.350336
-15.939972	9.908100	0.355341
-15.883040	-0.945685	0.360346
-15.857098	-2.281581	0.365350
-16.667134	-5.746155	0.370355
-17.126332	1.747270	0.375360
-17.578251	11.172549	0.380365
-17.614403	5.974024	0.385370
-17.823525	12.457280	0.390374
-17.689535	13.651290	0.395379
-17.670343	7.400147	0.400384
-17.974974	8.330267	0.405389
-17.863238	-4.639032	0.410394
-18.148701	-0.288841	0.415398
-18.889796	1.636181	0.420403
-18.709777	11.412306	0.425408
-20.065232	2.043880	0.430413
-20.255395	3.804033	0.435418
-20.484780	3.925200	0.440422
-20.501716	12.542462	0.445427
-20.610130	4.121949	0.450432
-20.416928	11.083546	0.455437
-20.398617	-3.256882	0.460442
-20.585025	0.201559	0.465446
-21.408420	5.293543	0.470451
-21.750897	-5.007688	0.475456
-22.273028	10.607107	0.480461
-22.075586	7.371633	0.485466
-22.179074	9.440982	0.490470
-23.026969	13.227036	0.495475
-23.197724	4.442920	0.500480
-23.353692	14.046739	0.505485
-23.220216	10.052459	0.510490
-23.461131	12.899316	0.515494
-23.999777	9.522194	0.520499
-24.385955	4.621768	0.525504
-24.721702	12.133940	0.530509
-24.674070	6.599679	0.535514
-24.498382	9.182362	0.540518
-24.906085	4.082816	0.545523
-25.593479	2.933911	0.550528
-25.867422	10.604132	0.555533
-26.053662	8.598943	0.560538
-25.999158	1.953176	0.565542
-26.267945	3.595861	0.570547
-26.878799	0.331220	0.575552
-27.493652	-0.711924	0.580557
-27.608248	2.169045	0.585562
-27.572197	7.804235	0.590566
-27.816375	15.476151	0.595571
-27.725335	1.064287	0.600576
-27.856973	10.408061	0.605581
-28.183371	6.298729	0.610586
-28.795199	6.280132	0.615590
-28.630935	8.149611	0.620595
-29.012757	7.190402	0.625600
-30.257126	13.894953	0.630605
-30.026032	2.219977	0.635610
-30.671571	6.686342	0.640614
-30.266714	9.556035	0.645619
-30.407286	8.935737	0.650624
-30.566270	6.597286	0.655629
-30.355582	1.477386	0.660634
-30.675021	4.871122	0.665638
-31.853515	10.670105	0.670643
-31.945706	14.781407	0.675648
-32.375249	10.140824	0.680653
-32.132283	17.113656	0.685658
-31.833871	3.337032	0.690662
-32.642144	5.044732	0.695667
-32.848289	1.967006	0.700672
-33.178574	6.934759	0.705677
-33.051938	7.614241	0.710682
-34.020565	6.088360	0.715686
-34.654041	4.225569	0.720691
-34.770313	7.040363	0.725696
-35.121300	9.097629	0.730701
-34.787173	12.952736	0.735706
-34.848276	6.062386	0.740710
-34.733962	8.901388	0.745715
-34.791488	6.632559	0.750720
-35.585410	12.852539	0.755725
-35.911256	11.520796	0.760730
-36.465288	4.299085	0.765734
-36.719798	13.171627	0.770739
-36.397963	15.696756	0.775744
-37.595792	13.346050	0.780749
-37.850102	15.828010	0.785754
-37.883809	20.948900	0.790758
-38.358534	5.214139	0.795763
-38.175746	12.199502	0.800768
-38.501459	10.396356	0.805773
-38.251562	5.415878	0.810778
-38.140704	5.528361	0.815782
-38.555356	2.182553	0.820787
-39.164114	8.079483	0.825792
-39.596826	7.242089	0.830797
-39.611980	-5.900432	0.835802
-39.575047	2.249709	0.840806
-40.422134	5.216253	0.845811
-40.406088	1.613569	0.850816
-41.479508	5.921936	0.855821
-41.100492	-3.374865	0.860826
-41.303324	2.354461	0.865830
-41.476593	7.408495	0.870835
-41.392279	3.867944	0.875840
-42.125904	8.803589	0.880845
-42.491886	5.121184	0.885850
-42.439341	7.738858	0.890854
-42.799168	7.377316	0.895859
-42.732416	2.349427	0.900864
-43.720402	4.312890	0.905869
-44.370426	3.496677	0.910874
-43.756844	6.140888	0.915878
-43.951913	8.126423	0.920883
-44.121587	-1.711348	0.925888
-44.582270	-4.176823	0.930893
-44.138001	4.166152	0.935898
-44.416125	1.194542	0.940902
-45.209334	6.174262	0.945907
-45.457290	-2.961647	0.950912
-45.576499	0.815349	0.955917
-46.219747	0.055027	0.960922
-46.704188	-4.662422	0.965926
-47.032674	1.250977	0.970931
-46.902573	0.120318	0.975936
-47.218320	7.211772	0.980941
-46.846998	-0.638049	0.985946
-47.011169	-2.206926	0.990950
-47.775658	8.513489	0.995955
-47.980280	-2.609605	1.000960
-48.467612	3.923290	1.005965
-48.488279	-1.081496	1.010970
-48.421281	-0.826147	1.015974
-49.105960	11.606026	1.020979
-49.520167	3.669709	1.025984
-49.785154	10.088897	1.030989
-50.151412	1.635769	1.035994
-49.932492	3.987101	1.040998
-49.816221	6.427180	1.046003
-50.194504	-4.415783	1.051008
-51.332288	3.379441	1.056013
-51.555108	1.256567	1.061018
-51.554994	-0.992763	1.066022
-51.507769	12.473855	1.071027
-51.493830	-4.580290	1.076032
-51.787804	-0.342666	1.081037
-52.256281	5.216058	1.086042
-52.670769	1.389353	1.091046
-53.159791	12.718590	1.096051
-52.590589	4.834794	1.101056
-53.036743	13.066482	1.106061
-53.761697	-1.284764	1.111066
-54.182257	6.822718	1.116070
-54.256010	9.403111	1.121075
-54.598469	3.040607	1.126080
-54.610789	3.393723	1.131085
-54.832905	1.583940	1.136090
-54.614128	1.426529	1.141094
-55.135877	8.426676	1.146099
-55.656633	-4.111960	1.151104
-55.902257	4.379557	1.156109
-56.356724	0.565404	1.161114
-55.903447	11.494834	1.166118
-56.046700	7.603752	1.171123
-56.975438	-0.568815	1.176128
-57.058279	7.024194	1.181133
-57.439748	-1.271545	1.186138
-57.474454	2.644149	1.191142
-57.692624	2.902771	1.196147
-58.047818	-7.200330	1.201152
-58.992996	2.754142	1.206157
-58.814974	2.637877	1.211162
-59.156483	7.879450	1.216166
-59.120514	5.102537	1.221171
-58.566282	-9.270706	1.226176
-59.250214	10.089712	1.231181
-59.189411	-1.571399	1.236186
-59.691852	-5.118663	1.241190
-60.685404	8.582763	1.246195
-60.350611	-11.786206	1.251200
-61.431502	5.655578	1.256205
-61.445417	1.171740	1.261210
-61.722096	-5.064966	1.266214
-61.812963	4.667910	1.271219
-61.792693	0.640641	1.276224
-61.995010	6.774833	1.281229
-62.150714	5.210964	1.286234
-61.982587	1.758602	1.291238
-62.978674	7.813910	1.296243
-62.908396	-0.106092	1.301248
-63.487060	10.411391	1.306253
-63.434283	11.374445	1.311258
-63.397925	7.069433	1.316262
-64.491528	10.042725	1.321267
-64.492130	5.907977	1.326272
-64.954412	7.273916	1.331277
-65.162357	3.263198	1.336282
-64.591501	7.736317	1.341286
-65.090518	15.780091	1.346291
-65.477882	7.213194	1.351296
-66.076436	7.967623	1.356301
-66.281471	9.271364	1.361306
-66.285492	14.115556	1.366310
-66.355489	13.474779	1.371315
-66.465945	8.762371	1.376320
-67.310654	11.813964	1.381325
-67.625853	11.454965	1.386330
-67.767126	13.897180	1.391334
-68.197272	9.769202	1.396339
-67.867883	4.358748	1.401344
-67.889135	12.945042	1.406349
-68.300785	10.038513	1.411354
-69.166421	5.402560	1.416358
-69.592288	15.845637	1.421363
-69.015550	5.423429	1.426368
-69.051208	14.992695	1.431373
-69.662093	10.032349	1.436378
-70.299830	17.142303	1.441382
-70.353348	20.045401	1.446387
-70.989716	14.361383	1.451392
-71.084984	11.389776	1.456397
-70.859362	6.925587	1.461402
-70.903615	15.594554	1.466406
-71.380777	4.045674	1.471411
-71.444342	-4.103414	1.476416
-71.876487	12.054166	1.481421
-72.380033	12.496421	1.486426
-72.883883	11.945340	1.491430
-73.524410	13.525687	1.496435
-73.489120	8.569132	1.501440
-73.938178	8.363848	1.506445
-74.141155	5.782321	1.511450
-73.614569	7.870622	1.516454
-73.657108	20.177509	1.521459
-73.439640	6.647599	1.526464
-74.433809	11.876901	1.531469
-75.024559	7.995385	1.536474
-74.726724	13.222832	1.541478
-75.281307	5.510846	1.546483
-75.829582	2.419955	1.551488
-76.323111	4.790468	1.556493
-76.584215	2.018683	1.561498
-76.655755	7.145458	1.566502
-76.774250	12.852164	1.571507
-76.757037	5.304241	1.576512
-76.726102	6.704114	1.581517
-76.803146	9.139490	1.586522
-77.342320	1.981907	1.591526
-77.899733	0.803276	1.596531
-78.000171	7.858042	1.601536
-78.114889	3.120990	1.606541
-79.020026	3.404318	1.611546
-79.430336	12.959152	1.616550
-79.684716	9.803518	1.621555
-79.368119	7.141093	1.626560
-79.687839	15.862441	1.631565
-79.241760	18.172078	1.636570
-79.421854	2.480034	1.641574
-80.097802	8.267206	1.646579
-80.841195	7.348477	1.651584
-81.440087	8.659759	1.656589
-81.300275	7.647806	1.661594
-81.078620	3.386709	1.666598
-81.582104	8.463683	1.671603
-82.190867	7.046283	1.676608
-82.616850	2.579150	1.681613
-82.577550	1.051356	1.686618
-82.624864	-1.060879	1.691622
-83.249529	-0.849693	1.696627
-82.799290	0.722166	1.701632
-82.761697	4.107766	1.706637
-82.941778	4.774894	1.711642
-83.661513	-2.553883	1.716646
-84.132125	11.284412	1.721651
-84.250559	-0.889773	1.726656
-84.894331	7.578317	1.731661
-85.526528	4.566929	1.736666
-85.554551	1.119799	1.741670
-85.897712	11.578467	1.746675
-85.380923	2.048252	1.751680
-85.419802	3.509612	1.756685
-85.477262	2.639102	1.761690
-86.338632	6.645544	1.766694
-86.788218	-0.579768	1.771699
-86.919089	-3.821066	1.776704
-86.669229	-1.360662	1.781709
-87.144622	2.683755	1.786714
-87.833417	-1.100239	1.791718
-88.020633	0.893563	1.796723
-88.348903	-6.540453	1.801728
-88.320363	4.888519	1.806733
-88.580681	6.678577	1.811738
-89.005240	2.388386	1.816742
-89.484081	0.817885	1.821747
-90.055266	12.482603	1.826752
-90.082569	8.880341	1.831757
-90.023640	3.410762	1.836762
-89.638610	4.157574	1.841766
-90.203307	13.442227	1.846771
-89.921545	5.068532	1.851776
-90.888090	5.630331	1.856781
-91.332695	0.988935	1.861786
-91.237507	12.151280	1.866790
-91.602555	13.856408	1.871795
-91.619480	4.374491	1.876800
-92.437448	12.600796	1.881805
-92.884450	0.025370	1.886810
-92.787125	2.095087	1.891814
-93.163504	8.594889	1.896819
-93.578149	3.227519	1.901824
-93.173628	-2.273722	1.906829
-92.948100	1.101597	1.911834
-93.599513	0.402657	1.916838
-94.633953	8.899938	1.921843
-94.744466	4.551359	1.926848
-94.667445	1.315656	1.931853
-94.474716	8.963829	1.936858
-94.806659	2.903400	1.941862
-95.450611	16.404868	1.946867
-95.831983	2.079221	1.951872
-96.377713	9.105246	1.956877
-96.083324	7.458643	1.961882
-96.215634	4.752223	1.966886
-96.683199	11.380114	1.971891
-96.986383	4.530625	1.976896
-97.532034	12.796784	1.981901
-98.373652	8.979639	1.986906
-98.387103	10.851477	1.991910
-97.714104	11.180144	1.996915
-97.593996	-2.878766	2.006912
-97.958258	4.286308	2.016909
-97.607054	3.031141	2.026906
-96.805744	6.622143	2.036902
-96.589674	5.172612	2.046899
-95.687907	3.423090	2.056896
-95.164055	-2.889246	2.066893
-95.127971	1.584314	2.076890
-94.597164	4.083401	2.086886
-93.635926	0.211772	2.096883
-93.608027	1.233827	2.106880
-93.003340	2.682409	2.116877
-92.676163	7.493937	2.126874
-92.105631	7.604738	2.136870
-91.333982	7.231246	2.146867
-90.984532	2.114940	2.156864
-90.372727	6.597059	2.166861
-89.851157	9.487211	2.176858
-89.636473	8.361000	2.186854
-89.055758	0.126526	2.196851
-88.343452	10.228315	2.206848
-87.870693	5.194174	2.216845
-86.893595	8.894018	2.226842
-86.629571	9.400988	2.236838
-86.494896	7.983137	2.246835
-86.070595	8.034346	2.256832
-85.420694	5.370565	2.266829
-85.288251	6.490380	2.276826
-84.731062	7.398349	2.286822
-84.037738	5.665443	2.296819
-83.048906	15.299709	2.306816
-82.629657	9.716386	2.316813
-82.563825	5.711749	2.326810
-82.309601	11.469105	2.336806
-81.654257	9.840311	2.346803
-80.477239	9.853515	2.356800
-79.975958	11.685650	2.366797
-79.921824	16.717085	2.376794
-79.794373	7.894300	2.386790
-78.715600	14.841034	2.396787
-78.196138	8.934842	2.406784
-78.179348	13.636315	2.416781
-77.170678	11.841638	2.426778
-77.079375	9.302843	2.436774
-76.744360	16.390722	2.446771
-75.585827	10.137946	2.456768
-75.388842	15.077450	2.466765
-74.942510	10.018913	2.476762
-74.112262	19.798247	2.486758
-73.637720	13.626626	2.496755
-73.774193	18.668732	2.506752
-73.251014	16.930640	2.516749
-72.326838	14.629618	2.526746
-71.639488	11.966340	2.536742
-71.392459	12.209871	2.546739
-71.235594	8.552176	2.556736
-70.085182	15.392727	2.566733
-70.041428	16.219085	2.576730
-69.499482	14.905709	2.586726
-69.108955	13.989697	2.596723
-68.703954	16.495704	2.606720
-67.668958	11.019240	2.616717
-67.164647	11.038986	2.626714
-66.972565	11.012315	2.636710
-65.825086	6.836098	2.646707
-65.693628	8.988734	2.656704
-65.824711	7.311330	2.666701
-65.213526	1.086761	2.676698
-64.620368	12.591385	2.686694
-63.146156	9.077025	2.696691
-62.737668	10.204544	2.706688
-63.058543	4.416522	2.716685
-62.861623	6.188345	2.726682
-61.879063	8.975045	2.736678
-61.461134	5.802540	2.746675
-60.532253	9.532066	2.756672
-60.012506	12.907160	2.766669
-59.739669	8.509175	2.776666
-59.841665	11.886043	2.786662
-58.805567	9.554925	2.796659
-58.469979	10.738142	2.806656
-57.791660	12.840477	2.816653
-57.097967	16.245507	2.826650
-57.008726	11.847597	2.836646
-56.485251	12.608767	2.846643
-55.644512	13.358551	2.856640
-55.490513	15.780100	2.866637
-54.745452	15.930249	2.876634
-54.143595	7.423224	2.886630
-53.817270	15.465933	2.896627
-53.664240	14.685097	2.906624
-52.679350	13.762070	2.916621
-52.496496	11.962930	2.926618
-51.286495	6.604933	2.936614
-50.824108	5.455994	2.946611
-50.876680	8.476721	2.956608
-50.721760	8.851798	2.966605
-49.915918	9.559500	2.976602
-49.508498	7.950301	2.986598
-49.033629	4.997004	2.996595
-48.191927	3.028761	3.006592
-47.956464	7.921093	3.016589
-46.823533	15.489769	3.026586
-46.748654	6.491442	3.036582
-46.725307	11.163385	3.046579
-45.630323	7.818941	3.056576
-45.376257	7.883986	3.066573
-44.907138	13.664905	3.076570
-43.967180	9.764911	3.086566
-43.930031	7.304235	3.096563
-43.520688	6.055854	3.106560
-42.549501	4.881547	3.116557
-42.347293	6.304101	3.126554
-42.067269	5.161383	3.136550
-41.060150	4.599180	3.146547
-40.692855	6.851307	3.156544
-40.594421	4.663015	3.166541
-39.621048	-1.497574	3.176538
-39.459067	-0.648444	3.186534
-38.708836	11.367066	3.196531
-38.386300	5.174765	3.206528
-37.712308	7.176408	3.216525
-37.159228	12.184009	3.226522
-36.542125	13.063645	3.236518
-36.257405	5.331399	3.246515
-36.068320	11.789457	3.256512
-35.248710	12.206757	3.266509
-35.160056	10.073837	3.276506
-33.839297	12.598815	3.286502
-33.702579	8.028794	3.296499
-33.350589	3.830720	3.306496
-33.009208	10.347425	3.316493
-32.217172	4.408297	3.326490
-31.763597	6.716679	3.336486
-31.001958	6.699529	3.346483
-30.458932	2.053576	3.356480
-30.499627	7.571761	3.366477
-29.922978	0.430770	3.376474
-29.022332	7.338719	3.386470
-29.012645	7.926470	3.396467
-28.145524	2.140371	3.406464
-27.208379	-1.543780	3.416461
-27.206727	1.607882	3.426458
-27.221671	3.862504	3.436454
-26.618818	4.576471	3.446451
-25.918569	2.813978	3.456448
-25.227167	3.529997	3.466445
-24.932707	0.364045	3.476442
-23.937717	5.372530	3.486438
-23.647000	5.621929	3.496435
-23.228310	3.776567	3.506432
-23.143823	3.342179	3.516429
-22.054002	7.806895	3.526426
-21.750635	9.777549	3.536422
-21.172423	7.280147	3.546419
-20.365392	6.397485	3.556416
-20.129658	10.494687	3.566413
-19.943715	7.190413	3.576410
-19.416276	4.837127	3.586406
-18.848508	7.374810	3.596403
-18.126285	11.250553	3.606400
-17.487626	10.733049	3.616397
-17.166176	8.928168	3.626394
-17.114398	13.240906	3.636390
-16.329049	16.089993	3.646387
-15.749306	9.920997	3.656384
-15.020971	7.812021	3.666381
-14.445878	8.805899	3.676378
-14.612988	10.073721	3.686374
-13.731058	12.749386	3.696371
-13.210861	6.475625	3.706368
-13.043522	13.589615	3.716365
-11.807240	10.844039	3.726362
-11.442175	14.452287	3.736358
-11.641730	10.707538	3.746355
-10.447710	8.668602	3.756352
-10.194424	3.202981	3.766349
-9.973606	15.072851	3.776346
-9.262908	15.263197	3.786342
-8.709067	16.127342	3.796339
-8.326163	15.589472	3.806336
-7.438862	11.225690	3.816333
-7.247777	13.527428	3.826330
-6.788484	13.098037	3.836326
-5.869068	8.843292	3.846323
-5.916698	6.782275	3.856320
-5.417696	17.851757	3.866317
-4.366961	18.141210	3.876314
-4.333419	20.337603	3.886310
-4.282963	27.301909	3.896307
-3.521909	24.383243	3.906304
-3.121224	37.406674	3.916301
-2.366819	47.153493	3.926298
-2.238665	58.895274	3.936294
-1.676178	69.739502	3.946291
-1.022920	78.732335	3.956288
-0.951271	90.913743	3.966285
0.020599	108.748737	3.976282
0.000000	119.719623	3.981286
0.391795	112.866279	3.986291
0.239613	133.064672	3.991296
1.080697	132.424403	3.996301
0.688636	127.626095	4.001306
0.565774	135.440522	4.006310
1.353763	146.552040	4.011315
1.037542	145.544644	4.016320
0.911034	130.884978	4.021325
1.277406	151.110218	4.026330
1.367237	153.276032	4.031334
1.402146	137.009395	4.036339
1.309629	137.242127	4.041344
1.058165	132.643383	4.046349
1.134317	136.896178	4.051354
1.055036	138.284750	4.056358
1.007400	140.199890	4.061363
0.965291	148.833794	4.066368
1.180200	152.043125	4.071373
1.593175	163.225696	4.076378
1.614931	159.773946	4.081382
1.182049	145.171459	4.086387
1.106605	137.599937	4.091392
1.141184	149.404547	4.096397
1.185731	145.984051	4.101402
1.368361	151.647084	4.106406
1.740375	155.663999	4.111411
1.434671	139.190972	4.116416
1.508130	134.269564	4.121421
1.506190	143.302159	4.126426
0.884784	145.116814	4.131430
1.065204	144.921083	4.136435
1.326576	154.570730	4.141440
1.767708	163.192675	4.146445
1.755014	151.973160	4.151450
1.528817	155.944013	4.156454
1.407572	153.457301	4.161459
1.023083	142.080550	4.166464
1.281412	150.961898	4.171469
1.863990	153.376850	4.176474
1.595424	151.928613	4.181478
1.494100	147.717766	4.186483
1.268435	163.261228	4.191488
1.683746	157.138177	4.196493
1.638004	146.483780	4.201498
1.183576	147.133518	4.206502
1.219658	152.506165	4.211507
1.615183	159.613486	4.216512
1.828708	167.733048	4.221517
2.532316	172.011542	4.226522
1.733546	159.563524	4.231526
1.418146	154.772255	4.236531
1.498905	147.027716	4.241536
1.316551	150.903160	4.246541
1.744177	148.416410	4.251546
1.786408	161.406210	4.256550
1.810570	156.568400	4.261555
1.790980	157.213708	4.266560
1.570713	163.673446	4.271565
2.001732	155.902842	4.276570
1.609574	151.721458	4.281574
1.752655	145.254829	4.286579
1.710955	145.577722	4.291584
1.736970	164.444976	4.296589
2.040355	171.019333	4.301594
1.431913	158.468918	4.306598
2.173241	162.257496	4.311603
1.944105	167.181073	4.316608
1.828197	160.871818	4.321613
1.634844	160.617227	4.326618
2.266423	161.186460	4.331622
1.665404	151.346158	4.336627
1.900818	150.382585	4.341632
1.863347	153.381281	4.346637
2.069816	155.484644	4.351642
1.942522	150.531214	4.356646
2.088972	154.244736	4.361651
1.739082	156.757416	4.366656
1.930381	156.648574	4.371661
2.066183	155.959931	4.376666
1.975831	168.138335	4.381670
2.162484	160.190647	4.386675
2.008851	161.230139	4.391680
2.126898	165.856058	4.396685
1.664689	163.007991	4.401690
1.498036	160.964934	4.406694
1.760426	160.012979	4.411699
1.717550	162.686661	4.416704
1.738456	171.854915	4.421709
2.048269	167.073864	4.426714
1.948306	169.563451	4.431718
2.202004	170.365522	4.436723
2.096348	163.039132	4.441728
1.826240	164.675710	4.446733
2.142610	170.336908	4.451738
2.330103	182.124059	4.456742
2.290795	171.664792	4.461747
1.922314	179.020784	4.466752
2.040455	193.523678	4.471757
2.419250	189.978368	4.476762
2.337218	193.654708	4.481766
2.358140	182.876017	4.486771
2.090787	192.921209	4.491776
2.306915	199.262395	4.496781
2.274454	186.030675	4.501786
2.139406	200.013026	4.506790
2.226670	189.967465	4.511795
2.406060	199.971577	4.516800
2.606401	196.128192	4.521805
2.675200	195.171576	4.526810
2.488419	192.907028	4.531814
2.098973	186.513806	4.536819
1.869754	189.033012	4.541824
1.995968	195.100302	4.546829
2.535562	184.762860	4.551834
2.415325	201.030240	4.556838
2.436556	197.771548	4.561843
2.227831	195.494598	4.566848
1.963072	194.140675	4.571853
2.448385	189.569568	4.576858
2.205365	199.775487	4.581862
2.475577	198.815984	4.586867
2.271195	196.418139	4.591872
2.366915	205.438724	4.596877
2.645368	208.983012	4.601882
2.566745	218.476828	4.606886
2.888107	219.081708	4.611891
2.770549	209.646979	4.616896
2.676371	200.781240	4.621901
2.683248	191.966209	4.626906
2.265973	193.685812	4.631910
2.409027	193.913504	4.636915
2.571783	207.204104	4.641920
2.941714	208.753688	4.646925
3.093012	204.272547	4.651930
2.761852	199.303390	4.656934
2.548828	195.986261	4.661939
2.915064	190.364372	4.666944
2.475947	193.580630	4.671949
2.722556	184.361291	4.676954
2.607950	193.863859	4.681958
2.600926	204.071000	4.686963
3.155795	208.799758	4.691968
3.021513	203.046991	4.696973
3.078439	192.000104	4.701978
2.758505	192.204971	4.706982
2.865134	189.258843	4.711987
2.648565	191.959572	4.716992
2.767605	188.818527	4.721997
2.905747	183.880707	4.727002
2.454817	187.807466	4.732006
2.811877	202.678119	4.737011
3.224944	214.756029	4.742016
2.895494	215.145871	4.747021
2.966335	208.177951	4.752026
2.621669	204.950917	4.757030
2.860839	213.180398	4.762035
3.050869	222.249582	4.767040
2.934177	217.079353	4.772045
3.144531	210.985031	4.777050
3.272187	218.453614	4.782054
3.357483	202.922536	4.787059
2.886732	203.229976	4.792064
2.551235	194.942801	4.797069
2.893806	209.667023	4.802074
2.454401	214.528441	4.807078
2.624630	213.945164	4.812083
2.990105	218.624320	4.817088
3.115205	215.786041	4.822093
3.327708	220.384613	4.827098
3.063101	223.649634	4.832102
3.158899	222.663503	4.837107
3.203482	219.600483	4.842112
3.157493	221.860217	4.847117
3.493412	210.485149	4.852122
3.164951	217.891872	4.857126
3.531269	221.530048	4.862131
3.354426	217.805494	4.867136
3.299716	220.588592	4.872141
3.514101	220.783032	4.877146
3.308182	225.525844	4.882150
3.151559	223.550820	4.887155
3.223751	219.448978	4.892160
3.285000	220.103848	4.897165
3.606545	221.202234	4.902170
3.314858	217.163375	4.907174
3.297327	215.188841	4.912179
3.085343	219.214441	4.917184
2.966090	218.309249	4.922189
2.855054	223.027797	4.927194
2.874853	224.774263	4.932198
3.196905	219.931182	4.937203
2.950289	219.767138	4.942208
3.643507	231.769804	4.947213
3.730460	232.411182	4.952218
3.679892	220.058595	4.957222
3.199111	221.579286	4.962227
3.201683	217.947018	4.967232
3.232209	235.073622	4.972237
3.697060	231.388358	4.977242
3.729224	234.746377	4.982246
3.888111	226.866256	4.987251
3.875444	223.729893	4.992256
3.074419	222.206367	4.997261
3.414303	221.318272	5.002266
3.257142	226.414152	5.007270
3.768820	238.508362	5.012275
3.848296	242.969468	5.017280
3.669054	228.836774	5.022285
3.453562	218.888954	5.027290
3.336166	230.331310	5.032294
3.535680	233.925858	5.037299
4.181281	233.018636	5.042304
3.564825	224.060200	5.047309
3.801441	212.343096	5.052314
3.596085	236.520300	5.057318
3.651906	230.469014	5.062323
3.800970	230.028234	5.067328
3.733241	240.646634	5.072333
3.430970	229.506956	5.077338
3.679549	243.119571	5.082342
3.817774	234.590945	5.087347
3.732958	241.905961	5.092352
3.705774	243.817928	5.097357
4.114663	241.125280	5.102362
4.089597	244.799088	5.107366
3.643514	239.455517	5.112371
3.990274	237.882995	5.117376
3.864853	243.957843	5.122381
3.874481	244.203146	5.127386
3.606758	243.204012	5.132390
3.591075	240.960274	5.137395
3.969635	240.246486	5.142400
3.943986	245.514881	5.147405
3.712194	248.679886	5.152410
3.780679	243.211905	5.157414
3.912193	247.462435	5.162419
4.032679	247.212761	5.167424
3.660908	247.650321	5.172429
3.705034	248.927940	5.177434
3.760303	251.905886	5.182438
3.694862	253.235366	5.187443
3.690794	244.681434	5.192448
4.210942	263.607897	5.197453
4.243516	256.721845	5.202458
3.901073	257.395278	5.207462
4.172944	245.413242	5.212467
3.777661	257.110848	5.217472
3.880138	260.113082	5.222477
4.621176	267.071741	5.227482
4.144304	265.266793	5.232486
4.378856	255.751908	5.237491
4.467282	250.236528	5.242496
3.915698	249.449266	5.247501
4.150907	241.832496	5.252506
3.732046	242.435571	5.257510
4.027370	247.578063	5.262515
4.368623	262.160169	5.267520
4.388173	262.691822	5.272525
4.489547	264.045949	5.277530
3.938884	260.987016	5.282534
4.403849	265.856334	5.287539
4.749103	265.799450	5.292544
4.207408	262.577773	5.297549
4.228218	243.456425	5.302554
3.588810	256.416386	5.307558
4.430093	259.047332	5.312563
4.186546	267.946770	5.317568
4.490559	277.127946	5.322573
4.677515	256.370399	5.327578
4.041294	283.085588	5.332582
4.570548	272.022058	5.337587
4.270572	270.853941	5.342592
3.984233	266.181501	5.347597
4.365317	263.635545	5.352602
4.256973	279.458229	5.357606
4.287572	270.740703	5.362611
4.344835	272.728108	5.367616
4.558193	281.616524	5.372621
4.582840	272.381079	5.377626
4.417715	279.056895	5.382630
4.232168	275.605761	5.387635
4.414300	271.135621	5.392640
4.454609	271.265418	5.397645
4.673602	268.456802	5.402650
4.094906	270.707736	5.407654
4.534074	271.063327	5.412659
4.718224	277.975821	5.417664
4.684342	270.584429	5.422669
4.796793	272.914411	5.427674
4.234581	272.821649	5.432678
4.885179	279.699483	5.437683
4.812204	273.611289	5.442688
4.325417	277.929620	5.447693
4.799458	284.781163	5.452698
4.660265	289.273163	5.457702
4.755065	275.509044	5.462707
5.088898	277.519827	5.467712
5.034166	277.778314	5.472717
4.549318	267.723710	5.477722
4.559416	271.740055	5.482726
4.282308	265.952559	5.487731
4.944134	289.352590	5.492736
4.905345	293.914378	5.497741
5.013293	279.980533	5.502746
4.809848	275.491333	5.507750
4.888531	270.616529	5.512755
4.597080	269.314210	5.517760
5.027464	284.027986	5.522765
5.062237	273.601417	5.527770
4.573672	281.260879	5.532774
4.988507	287.454103	5.537779
5.125832	282.010193	5.542784
4.433886	274.116993	5.547789
4.905280	285.619569	5.552794
5.054880	290.104570	5.557798
4.805564	286.767764	5.562803
5.195322	293.860219	5.567808
5.023839	290.976357	5.572813
5.361800	288.373838	5.577818
4.900216	281.903229	5.582822
4.746344	284.916907	5.587827
4.972097	275.441345	5.592832
4.922714	287.486905	5.597837
5.336054	286.818319	5.602842
5.278244	294.730253	5.607846
5.213444	289.425376	5.612851
5.083078	276.050648	5.617856
4.904345	281.241650	5.622861
5.074307	274.343691	5.627866
4.992123	290.741267	5.632870
5.071450	288.220144	5.637875
5.118643	290.645708	5.642880
5.063391	288.730821	5.647885
5.484851	290.455884	5.652890
5.515546	297.180311	5.657894
5.220853	294.008753	5.662899
5.260146	283.964281	5.667904
5.238395	288.716400	5.672909
5.153790	290.042539	5.677914
5.091029	289.865687	5.682918
5.052254	291.833246	5.687923
5.011401	289.387781	5.692928
5.159226	295.711164	5.697933
5.431775	290.084849	5.702938
5.070472	296.993691	5.707942
5.327978	292.970546	5.712947
5.287632	297.222535	5.717952
5.273489	290.827788	5.722957
5.384109	297.675809	5.727962
5.181719	298.998141	5.732966
5.142098	306.296656	5.737971
5.283857	303.550679	5.742976
5.247113	298.241431	5.747981
5.093356	296.098276	5.752986
5.160297	301.216233	5.757990
5.207623	313.227770	5.762995
5.635957	314.695506	5.768000
5.523904	327.228568	5.773005
5.508705	315.022266	5.778010
5.867421	319.310203	5.783014
5.648296	315.554248	5.788019
5.601859	297.936576	5.793024
5.134243	300.957978	5.798029
5.614601	302.673872	5.803034
5.319538	322.942181	5.808038
5.509408	321.201094	5.813043
5.597542	321.196897	5.818048
5.564511	328.592470	5.823053
5.655710	327.597559	5.828058
5.260261	333.195634	5.833062
5.017848	325.260893	5.838067
5.507906	320.211297	5.843072
5.472713	319.511307	5.848077
5.626245	324.270945	5.853082
5.363580	325.143928	5.858086
5.508742	328.012980	5.863091
5.687736	321.898193	5.868096
5.819507	340.840916	5.873101
5.857300	333.583868	5.878106
5.553237	326.022551	5.883110
5.849074	329.073784	5.888115
5.868634	339.007950	5.893120
5.442078	343.857911	5.898125
6.138235	340.364397	5.903130
5.614644	349.326459	5.908134
5.873820	348.175682	5.913139
5.964083	341.770988	5.918144
6.005348	351.556251	5.923149
6.039882	339.680705	5.928154
5.703680	335.360853	5.933158
5.842815	335.079801	5.938163
5.790895	345.774895	5.943168
5.789652	350.843372	5.948173
6.214345	344.177804	5.953178
6.252193	361.866528	5.958182
5.859126	345.780228	5.963187
6.051783	323.689798	5.968192
5.742703	325.734247	5.973197
6.131898	335.882938	5.978202
6.197073	337.894428	5.983206
5.949680	322.785196	5.988211
5.951770	323.329061	5.993216
5.879332	329.443145	5.998221
5.933994	329.137281	6.003226
5.966074	345.513953	6.008230
6.167391	342.723897	6.013235
6.241557	347.312404	6.018240
5.761438	326.509943	6.023245
6.155119	328.758181	6.028250
5.846060	328.616513	6.033254
6.161435	338.852628	6.038259
5.755120	336.840537	6.043264
5.558245	338.696679	6.048269
5.868741	332.561414	6.053274
5.894359	350.726586	6.058278
6.245860	332.825464	6.063283
6.265539	339.523148	6.068288
6.039506	346.796920	6.073293
6.326701	350.858723	6.078298
6.368258	337.359106	6.083302
6.000077	329.965956	6.088307
6.026460	326.254029	6.093312
5.888597	326.373603	6.098317
6.020367	322.189697	6.103322
5.976534	324.420634	6.108326
6.211813	322.878117	6.113331
6.194857	313.329595	6.118336
5.836442	324.524805	6.123341
6.037456	326.195611	6.128346
5.922258	331.310298	6.133350
6.168150	322.464315	6.138355
5.859406	320.835661	6.143360
5.545722	326.949341	6.148365
6.245447	319.959391	6.153370
6.128466	324.786457	6.158374
5.875585	327.078416	6.163379
5.839998	322.452339	6.168384
6.043592	326.245584	6.173389
6.079578	332.880616	6.178394
6.119200	334.601861	6.183398
5.556618	333.740377	6.188403
6.021096	335.737153	6.193408
6.151092	353.734220	6.198413
6.343822	339.635271	6.203418
5.928985	328.326398	6.208422
5.853185	324.247575	6.213427
6.295610	318.740332	6.218432
5.798138	323.218521	6.223437
5.824808	327.928311	6.228442
5.976280	345.804970	6.233446
6.152811	345.685771	6.238451
6.090645	336.182240	6.243456
5.808029	336.694504	6.248461
5.966781	334.442578	6.253466
6.416261	346.306104	6.258470
6.395373	325.561855	6.263475
6.131508	329.260206	6.268480
5.511747	322.187798	6.273485
5.925708	314.498874	6.278490
5.700117	323.031718	6.283494
5.791124	341.696056	6.288499
6.070315	339.064715	6.293504
5.843119	346.737294	6.298509
6.082806	346.658882	6.303514
5.900562	339.597440	6.308518
6.092604	351.073952	6.313523
6.439661	339.706558	6.318528
6.205121	333.583388	6.323533
6.106627	322.209448	6.328538
5.718537	328.293585	6.333542
5.703746	326.622327	6.338547
5.797746	331.375417	6.343552
5.612458	344.321683	6.348557
6.148900	339.451518	6.353562
6.059167	348.032823	6.358566
6.006787	342.729160	6.363571
6.070654	342.216222	6.368576
5.890922	352.402882	6.373581
5.915741	342.183463	6.378586
5.933465	351.934427	6.383590
6.151099	342.210162	6.388595
6.324447	343.103843	6.393600
6.167359	343.552271	6.398605
6.721972	337.464417	6.403610
6.306854	339.566505	6.408614
5.902612	316.490198	6.413619
6.045658	319.736057	6.418624
5.996754	320.117022	6.423629
6.326269	315.990912	6.428634
6.143604	318.765475	6.433638
5.841948	329.303293	6.438643
5.936289	323.524383	6.443648
5.842951	323.254217	6.448653
5.965476	314.860873	6.453658
5.945335	319.391291	6.458662
6.129966	318.919661	6.463667
6.250922	317.948591	6.468672
5.851042	326.837597	6.473677
5.927349	318.793126	6.478682
5.948054	321.298748	6.483686
5.844424	326.835567	6.488691
5.831902	324.907696	6.493696
5.759032	313.896760	6.498701
5.919731	314.175489	6.503706
5.752996	323.638787	6.508710
5.896996	339.112193	6.513715
6.459350	331.890531	6.518720
6.149864	337.098743	6.523725
6.008240	316.898476	6.528730
5.857344	319.740857	6.533734
5.820243	324.568141	6.538739
6.040986	333.252956	6.543744
5.973941	346.142849	6.548749
6.552350	340.218965	6.553754
5.797565	340.421936	6.558758
5.969637	332.517570	6.563763
5.909561	329.113328	6.568768
5.819765	323.685784	6.573773
6.004119	335.976554	6.578778
5.837898	333.917591	6.583782
6.205603	346.356987	6.588787
6.595229	335.514470	6.593792
5.951731	332.226374	6.598797
5.840646	317.336366	6.603802
6.021215	320.921226	6.608806
6.002090	325.131954	6.613811
5.781264	321.993183	6.618816
5.910145	322.302175	6.623821
6.057467	325.778321	6.628826
5.957380	324.227908	6.633830
6.076475	336.187159	6.638835
5.965222	326.131301	6.643840
6.091254	332.780787	6.648845
6.243227	318.817912	6.653850
6.040338	319.422164	6.658854
6.230797	327.855433	6.663859
6.311654	317.348897	6.668864
6.321150	319.998630	6.673869
6.042692	316.906797	6.678874
5.906268	320.357518	6.683878
6.095167	322.700914	6.688883
6.411067	324.391797	6.693888
5.791766	330.103816	6.698893
6.021566	324.528438	6.703898
5.822161	328.659670	6.708902
5.854859	326.452680	6.713907
6.163291	330.014471	6.718912
5.884997	327.450948	6.723917
6.098084	330.461283	6.728922
5.992997	337.197373	6.733926
6.166851	336.009262	6.738931
5.949311	335.935601	6.743936
6.080402	329.682740	6.748941
5.955155	338.620740	6.753946
5.926018	333.946201	6.758950
6.270376	329.045835	6.763955
6.089873	322.784543	6.768960
6.038377	333.058793	6.773965
5.799552	330.368904	6.778970
5.754424	329.834972	6.783974
5.941709	321.485324	6.788979
5.880177	325.705819	6.793984
6.062113	328.695693	6.798989
6.022217	326.692992	6.803994
6.049351	323.192916	6.808998
5.698900	325.955639	6.814003
6.196257	323.872453	6.819008
6.106072	329.932354	6.824013
5.985571	320.169000	6.829018
5.781874	326.031441	6.834022
5.878870	328.433438	6.839027
6.446534	326.652511	6.844032
5.851473	327.786051	6.849037
6.018209	324.128201	6.854042
5.509995	326.750974	6.859046
5.988326	331.023455	6.864051
5.858744	322.931945	6.869056
5.866287	329.916248	6.874061
5.973422	327.460391	6.879066
6.276802	327.849781	6.884070
5.684831	331.156299	6.889075
6.068281	327.951916	6.894080
5.911566	331.510201	6.899085
5.741300	329.404413	6.904090
6.019805	340.563741	6.909094
6.164916	343.322074	6.914099
6.239222	342.706272	6.919104
5.597754	337.285526	6.924109
5.986174	345.343137	6.929114
6.317541	352.935081	6.934118
5.784896	341.669852	6.939123
6.410832	336.203633	6.944128
5.812857	338.027313	6.949133
6.057702	319.067152	6.954138
5.553950	330.968353	6.959142
6.045032	347.216616	6.964147
6.305407	341.740874	6.969152
6.031893	348.034965	6.974157
6.249716	336.646566	6.979162
5.929125	331.944641	6.984166
5.942648	324.827415	6.989171
5.919460	326.242068	6.994176
5.673007	346.730622	6.999181
6.408843	345.046894	7.004186
6.360705	339.824828	7.009190
5.923049	336.675522	7.014195
6.162689	330.054589	7.019200
5.821837	327.538771	7.024205
6.027125	321.517965	7.029210
5.817555	329.703475	7.034214
5.834348	327.397723	7.039219
6.200189	335.427209	7.044224
6.092741	340.246467	7.049229
6.157930	325.098057	7.054234
6.097545	327.666924	7.059238
5.898849	326.097064	7.064243
5.904940	326.134114	7.069248
5.966904	327.285578	7.074253
5.965308	324.065217	7.079258
5.884718	324.640937	7.084262
5.762477	339.130758	7.089267
6.333480	346.090612	7.094272
6.006346	343.550510	7.099277
5.804303	337.539336	7.104282
5.812634	338.022119	7.109286
6.037099	350.613532	7.114291
6.311603	347.720332	7.119296
5.974670	346.788915	7.124301
5.758226	332.744187	7.129306
5.875460	339.214714	7.134310
6.236436	349.478536	7.139315
6.517095	350.551659	7.144320
5.923466	331.260132	7.149325
5.896551	330.492415	7.154330
5.793119	331.565229	7.159334
5.675730	338.920156	7.164339
6.243676	344.497950	7.169344
6.148213	353.402847	7.174349
6.080594	347.310630	7.179354
6.255427	345.875596	7.184358
5.712607	342.113087	7.189363
5.968243	336.476735	7.194368
5.711384	338.800952	7.199373
6.068348	346.167448	7.204378
6.387348	350.866531	7.209382
6.052716	341.263052	7.214387
6.126137	324.427109	7.219392
5.700420	338.306130	7.224397
5.638707	339.676164	7.229402
5.927944	349.289941	7.234406
6.080158	356.900289	7.239411
6.188800	350.359855	7.244416
6.262032	355.960894	7.249421
6.431769	343.516974	7.254426
5.736361	338.898714	7.259430
6.154632	332.012691	7.264435
6.088261	331.776291	7.269440
5.731586	329.427448	7.274445
5.950872	335.885248	7.279450
5.513374	349.127045	7.284454
5.842096	355.795601	7.289459
6.308500	358.867738	7.294464
6.244602	364.392056	7.299469
6.142463	350.671197	7.304474
5.773762	349.887092	7.309478
6.192748	359.132666	7.314483
6.059088	342.278329	7.319488
5.949682	340.520562	7.324493
6.356284	327.634821	7.329498
6.074712	328.200705	7.334502
5.892227	335.113358	7.339507
6.322741	335.865761	7.344512
6.033903	332.117492	7.349517
6.279856	328.289122	7.354522
6.092541	333.725080	7.359526
5.877911	337.254419	7.364531
5.945501	330.366050	7.369536
5.648106	335.809656	7.374541
5.812988	323.866370	7.379546
5.912870	327.992133	7.384550
6.076850	332.845058	7.389555
6.187350	326.228415	7.394560
5.936796	333.933099	7.399565
6.113336	327.157479	7.404570
5.992163	330.086981	7.409574
5.643192	330.533647	7.414579
5.904142	335.257582	7.419584
5.946119	332.482845	7.424589
6.159006	323.256030	7.429594
6.036330	327.694848	7.434598
5.884917	334.140764	7.439603
5.977607	334.445900	7.444608
5.954238	340.292924	7.449613
6.151122	341.015265	7.454618
6.140269	340.890441	7.459622
6.169998	332.628593	7.464627
5.998900	328.545624	7.469632
5.714775	336.144806	7.474637
5.850298	333.450415	7.479642
5.807372	343.289909	7.484646
5.775455	345.458883	7.489651
6.451072	350.279609	7.494656
6.085654	355.351004	7.499661
6.144817	341.760059	7.504666
5.969170	338.636397	7.509670
5.600468	345.350261	7.514675
6.176199	350.563018	7.519680
6.157307	361.161232	7.524685
6.269637	355.809775	7.529690
6.142772	330.292176	7.534694
6.067741	328.529058	7.539699
6.107556	331.790993	7.544704
5.652119	339.151099	7.549709
5.863624	331.617074	7.554714
6.117816	331.653460	7.559718
5.874107	325.452628	7.564723
5.590051	330.989067	7.569728
5.706872	349.421607	7.574733
6.001651	347.736949	7.579738
6.472746	352.991308	7.584742
6.461587	357.760779	7.589747
6.242156	344.121461	7.594752
5.969647	341.980971	7.599757
6.178227	332.587145	7.604762
6.166827	334.841508	7.609766
5.627884	337.029313	7.614771
5.996890	330.590715	7.619776
5.976446	329.730243	7.624781
5.941149	330.308402	7.629786
5.943746	332.193596	7.634790
5.664954	330.626715	7.639795
6.119575	340.559581	7.644800
6.040655	351.714456	7.649805
6.058496	344.742080	7.654810
6.133011	330.857693	7.659814
5.742211	327.372068	7.664819
6.170459	325.587539	7.669824
6.116056	332.040495	7.674829
5.710295	327.851695	7.679834
6.038421	344.707447	7.684838
6.247928	342.884208	7.689843
6.292960	337.211045	7.694848
6.422819	333.638028	7.699853
5.995773	333.040175	7.704858
5.840123	331.254808	7.709862
5.886644	333.098362	7.714867
5.946959	327.482934	7.719872
6.058583	337.035775	7.724877
5.893730	323.675872	7.729882
5.786450	334.370088	7.734886
5.643215	338.166716	7.739891
6.125298	335.149452	7.744896
5.827508	348.663720	7.749901
6.303551	355.157481	7.754906
6.189864	344.187682	7.759910
6.069087	348.468025	7.764915
5.936813	330.341676	7.769920
6.144012	332.919501	7.774925
6.029373	328.565154	7.779930
5.902510	336.237925	7.784934
5.735876	339.930631	7.789939
6.144693	336.105376	7.794944
5.728471	333.993590	7.799949
6.033271	336.037373	7.804954
6.161062	344.309566	7.809958
6.131320	333.563982	7.814963
6.286414	337.984865	7.819968
6.069525	337.892120	7.824973
6.370173	331.109831	7.829978
5.622216	333.719314	7.834982
5.765426	334.282335	7.839987
6.352543	326.575937	7.844992
5.823434	344.643978	7.849997
5.789809	333.740813	7.855002
5.912756	337.565598	7.860006
5.586400	336.898286	7.865011
5.971840	338.065824	7.870016
6.184356	353.139439	7.875021
6.471572	344.309157	7.880026
6.186994	329.686592	7.885030
6.097980	339.185253	7.890035
6.397346	323.829544	7.895040
5.799380	337.627817	7.900045
5.979812	339.985188	7.905050
6.063613	333.442301	7.910054
5.651148	332.383442	7.915059
6.260812	340.400277	7.920064
6.047673	338.377092	7.925069
6.308653	323.767664	7.930074
6.212636	327.999856	7.935078
5.845718	336.712896	7.940083
6.138487	329.409823	7.945088
5.993873	334.892916	7.950093
6.123466	329.282519	7.955098
6.084236	328.516720	7.960102
6.120256	330.801663	7.965107
6.217284	326.287813	7.970112
6.010234	337.785325	7.975117
6.199134	329.846703	7.980122
6.447200	328.151491	7.985139
5.974634	332.983788	7.990157
6.080532	338.871514	7.995174
5.844840	345.027009	8.000192
6.146724	337.034168	8.005210
6.021582	336.125932	8.010227
6.174866	335.035498	8.015245
6.466088	323.162902	8.020262
5.940977	311.966491	8.025280
5.742191	310.530111	8.030298
5.832511	318.521901	8.035315
5.991798	332.555450	8.040333
5.853575	328.544114	8.045350
5.763087	329.249319	8.050368
5.637897	321.174664	8.055386
6.066620	328.438467	8.060403
5.665235	334.884830	8.065421
6.122519	335.653064	8.070438
5.971935	336.926172	8.075456
6.063643	331.036149	8.080474
5.831651	329.791119	8.085491
5.853511	340.983918	8.090509
6.135287	331.337505	8.095526
6.231117	340.915728	8.100544
6.121229	337.269187	8.105562
6.388329	339.032654	8.110579
5.883255	330.913006	8.115597
6.227832	330.670053	8.120614
6.286064	340.036391	8.125632
6.080314	333.943386	8.130650
6.479474	335.610557	8.135667
6.186085	326.855227	8.140685
6.230544	325.961608	8.145702
6.070705	328.656189	8.150720
6.288226	334.520223	8.155738
6.325387	339.891662	8.160755
6.093412	335.620382	8.165773
5.988787	335.119183	8.170790
5.892555	321.678609	8.175808
6.024890	329.162118	8.180826
6.120675	345.237787	8.185843
6.517938	351.768080	8.190861
6.250425	339.963531	8.195878
6.192236	339.085894	8.200896
6.457147	336.684273	8.205914
6.545678	339.068801	8.210931
5.751475	334.594740	8.215949
6.118584	335.853513	8.220966
6.498818	352.516027	8.225984
6.288225	343.719397	8.231002
6.159254	341.284432	8.236019
6.502945	345.162869	8.241037
6.178367	335.983225	8.246054
6.022425	338.147055	8.251072
6.301025	347.030987	8.256090
6.605099	354.951646	8.261107
6.214626	343.630117	8.266125
6.129557	333.280312	8.271142
6.254076	346.785984	8.276160
6.271587	353.432205	8.281178
6.664787	350.786558	8.286195
6.055430	348.514745	8.291213
6.127154	342.861346	8.296230
6.521581	361.257254	8.301248
6.324938	355.106022	8.306266
6.493050	365.588138	8.311283
6.214345	362.283439	8.316301
6.619229	355.495783	8.321318
5.847450	350.601683	8.326336
6.216630	360.534966	8.331354
6.245533	360.420053	8.336371
6.180090	359.736038	8.341389
6.153027	363.037922	8.346406
6.287827	364.951371	8.351424
6.167397	365.086915	8.356442
6.446036	369.622390	8.361459
5.804323	353.881062	8.366477
6.202412	361.749218	8.371494
5.841285	353.682882	8.376512
6.585088	366.495735	8.381530
6.727635	368.508959	8.386547
6.548498	368.786179	8.391565
6.772762	359.457958	8.396582
6.579829	362.760422	8.401600
6.541067	354.000146	8.406618
6.786298	359.986099	8.411635
6.554767	366.576432	8.416653
6.584355	354.836063	8.421670
6.464913	367.521402	8.426688
6.468157	359.978969	8.431706
6.596530	350.823463	8.436723
6.488963	361.332720	8.441741
6.664769	355.145589	8.446758
6.107359	363.048911	8.451776
6.064336	360.032548	8.456794
6.660627	351.725633	8.461811
6.182498	355.078811	8.466829
6.584783	348.790152	8.471846
6.263128	358.969842	8.476864
6.162125	359.556772	8.481882
6.556045	362.947737	8.486899
6.249536	368.896527	8.491917
6.827276	378.680591	8.496934
6.371148	369.433053	8.501952
6.657073	377.766780	8.506970
6.804106	375.295149	8.511987
6.343679	368.449720	8.517005
6.788467	375.414411	8.522022
6.775071	365.908606	8.527040
6.617009	366.756870	8.532058
6.788246	362.230311	8.537075
6.570840	361.077677	8.542093
6.501592	370.138849	8.547110
6.545853	360.242238	8.552128
6.434522	356.917792	8.557146
6.642794	353.512030	8.562163
6.490710	355.009423	8.567181
6.802545	359.798489	8.572199
6.514629	361.029869	8.577216
6.327944	361.235685	8.582234
7.037851	374.555566	8.587251
6.543369	373.231487	8.592269
6.736582	365.126172	8.597287
7.012106	364.998107	8.602304
6.635633	358.997942	8.607322
6.544961	356.222515	8.612339
6.346998	366.168369	8.617357
6.690221	367.992566	8.622375
6.626578	379.302837	8.627392
6.781238	384.220518	8.632410
6.769862	379.217485	8.637427
6.680160	390.310925	8.642445
6.702956	379.338418	8.647463
7.034926	385.727419	8.652480
6.726315	377.081726	8.657498
6.858731	357.063895	8.662515
6.458898	361.682914	8.667533
6.427913	368.128420	8.672551
6.692394	384.105279	8.677568
6.694356	385.108501	8.682586
6.645658	387.889922	8.687603
7.013422	386.986986	8.692621
7.170603	388.997934	8.697639
6.564898	381.342031	8.702656
6.536429	386.174621	8.707674
6.947244	379.913024	8.712691
6.786099	389.064249	8.717709
6.888630	383.317683	8.722727
6.983149	389.320801	8.727744
6.977824	389.091303	8.732762
6.856821	369.011934	8.737779
6.532900	369.198094	8.742797
6.672575	374.821811	8.747815
6.802616	384.331618	8.752832
6.886111	389.314026	8.757850
7.261066	391.332091	8.762867
6.825451	378.865760	8.767885
6.527849	369.991151	8.772903
6.729999	374.772054	8.777920
6.827076	392.321245	8.782938
6.812943	393.686716	8.787955
7.128246	397.951417	8.792973
6.946623	397.216065	8.797991
6.967308	392.602491	8.803008
6.871523	397.918911	8.808026
6.738469	393.395542	8.813043
6.869691	389.222327	8.818061
6.937656	386.387484	8.823079
7.346723	385.547541	8.828096
7.016926	383.601406	8.833114
7.089921	374.978346	8.838131
6.749566	371.932539	8.843149
6.615650	372.979005	8.848167
6.815089	380.830764	8.853184
7.048280	387.828405	8.858202
7.059121	385.598872	8.863219
6.956731	384.687091	8.868237
7.111401	389.371255	8.873255
7.316103	384.561783	8.878272
6.925534	381.119872	8.883290
7.115166	376.331683	8.888307
6.980223	366.614440	8.893325
7.115023	377.502514	8.898343
6.863113	357.134289	8.903360
6.740305	371.423216	8.908378
6.855245	371.831365	8.913395
6.803499	386.049283	8.918413
6.750703	382.927146	8.923431
7.038989	383.548135	8.928448
6.859225	383.156458	8.933466
7.129778	381.220987	8.938483
7.287092	392.578911	8.943501
7.140861	382.582565	8.948519
7.118787	379.537692	8.953536
6.767337	392.271794	8.958554
7.412865	378.630485	8.963571
7.048949	394.080377	8.968589
7.013585	391.340512	8.973607
7.352759	389.517426	8.978624
7.210769	393.679764	8.983642
7.206043	387.981453	8.988659
7.018934	394.160957	8.993677
7.063155	386.905607	8.998695
7.166090	387.186245	9.003712
7.046558	390.650846	9.008730
7.016635	386.000974	9.013747
6.926277	383.881867	9.018765
6.800048	386.429220	9.023783
7.393636	387.163612	9.028800
6.979803	395.000414	9.033818
7.159141	392.858248	9.038835
7.263367	397.818497	9.043853
7.027246	397.779559	9.048871
7.111376	388.249091	9.053888
7.042998	392.153828	9.058906
7.215163	386.412198	9.063923
7.086792	386.621557	9.068941
7.034565	390.479601	9.073959
7.037542	394.152334	9.078976
6.902651	390.740036	9.083994
7.493595	402.958210	9.089011
7.593196	398.158787	9.094029
7.352113	397.148685	9.099047
6.957078	384.265800	9.104064
7.019137	391.321643	9.109082
7.136735	384.704931	9.114099
7.372561	409.929137	9.119117
7.060273	417.608135	9.124135
7.358588	404.367987	9.129152
7.317653	409.780007	9.134170
7.597083	408.890823	9.139187
7.405831	410.110311	9.144205
7.379053	404.939265	9.149223
7.606020	389.138390	9.154240
6.901972	401.081686	9.159258
7.139650	401.025781	9.164275
7.189770	402.693656	9.169293
7.183745	409.419299	9.174311
7.684398	410.395367	9.179328
7.140716	418.605829	9.184346
7.262807	407.062451	9.189363
7.419251	404.781845	9.194381
7.234438	418.758589	9.199399
7.588849	414.443326	9.204416
7.351817	405.332062	9.209434
7.439324	401.222451	9.214451
7.427251	412.139726	9.219469
7.295901	425.142524	9.224487
7.337885	406.981613	9.229504
7.364395	410.369834	9.234522
7.522238	412.554242	9.239539
7.685042	411.437076	9.244557
7.423433	417.729169	9.249575
7.621961	409.036057	9.254592
7.675957	411.069384	9.259610
7.807919	408.407601	9.264627
7.309083	411.514717	9.269645
7.605649	415.230102	9.274663
7.441408	407.502298	9.279680
6.962152	405.415337	9.284698
7.549478	407.353004	9.289715
7.785217	411.819434	9.294733
7.628962	415.674746	9.299751
7.628353	414.557778	9.304768
7.530603	418.889950	9.309786
7.696681	411.653485	9.314803
7.820979	411.716213	9.319821
7.094433	404.782822	9.324839
7.178319	398.089307	9.329856
7.281457	401.809560	9.334874
7.095231	407.076952	9.339891
7.081134	407.517815	9.344909
7.298285	414.552677	9.349927
7.724453	407.282029	9.354944
7.588428	411.689583	9.359962
7.740898	412.445322	9.364979
7.328336	414.320929	9.369997
7.468538	414.191843	9.375015
7.271131	406.787922	9.380032
7.495029	409.943450	9.385050
7.889492	424.214995	9.390067
7.372105	419.565275	9.395085
7.734093	428.508845	9.400103
7.612686	421.837817	9.405120
7.660823	427.258064	9.410138
7.489893	443.375348	9.415155
7.746025	439.949495	9.420173
7.851766	436.969914	9.425191
7.846799	427.052530	9.430208
7.649483	427.796461	9.435226
7.226987	418.783491	9.440243
7.943837	424.203756	9.445261
7.799760	431.045570	9.450279
7.763878	433.828159	9.455296
7.509732	428.610459	9.460314
7.697544	431.948324	9.465331
8.060470	438.376704	9.470349
7.921031	437.009964	9.475367
7.385958	427.572727	9.480384
7.297118	438.864869	9.485402
7.706069	441.035429	9.490419
7.994808	440.753834	9.495437
7.366081	435.985753	9.500455
7.512917	435.404376	9.505472
7.927877	444.355484	9.510490
7.435654	443.207765	9.515507
7.786747	442.326356	9.520525
7.532542	448.977051	9.525543
7.511853	445.723678	9.530560
7.396131	440.714784	9.535578
7.803759	436.347051	9.540595
8.005920	429.786580	9.545613
7.985283	440.313905	9.550631
8.185323	439.064715	9.555648
8.140526	442.801698	9.560666
7.771754	437.201075	9.565683
7.813523	441.899675	9.570701
7.548773	445.500499	9.575719
7.448033	435.948299	9.580736
8.034402	442.152552	9.585754
7.567054	451.493487	9.590771
8.378040	455.557956	9.595789
8.299451	444.635906	9.600807
7.991970	444.194688	9.605824
8.057140	436.696227	9.610842
8.024486	442.848545	9.615859
8.118782	439.687718	9.620877
8.025363	440.055730	9.625895
8.196905	438.555369	9.630912
7.990847	436.703565	9.635930
7.862974	443.391390	9.640947
8.172377	439.805771	9.645965
7.655824	442.032071	9.650983
7.803712	434.006361	9.656000
7.885392	430.658162	9.661018
7.584611	440.313967	9.666035
7.458409	432.125816	9.671053
7.943895	453.398213	9.676071
8.326445	450.271396	9.681088
8.256773	452.917244	9.686106
8.028306	445.685393	9.691123
8.173724	440.465436	9.696141
8.008469	444.375801	9.701159
7.832624	439.347868	9.706176
8.215964	437.842932	9.711194
7.816420	449.783029	9.716211
8.336104	456.278522	9.721229
7.950203	445.846110	9.726247
8.051743	452.334125	9.731264
8.077983	456.476597	9.736282
8.127478	468.794895	9.741299
8.380391	461.983525	9.746317
7.861427	453.436815	9.751335
8.474913	451.978092	9.756352
8.325139	453.976881	9.761370
8.036946	441.446530	9.766387
7.876388	437.457581	9.771405
8.118247	457.240581	9.776423
8.371776	452.615984	9.781440
8.123923	451.045228	9.786458
8.058134	444.217217	9.791475
8.451073	439.324777	9.796493
7.948950	443.233945	9.801511
8.070947	449.182314	9.806528
8.403777	454.283702	9.811546
8.279468	463.454475	9.816563
8.357037	441.412850	9.821581
8.224028	454.740960	9.826599
7.976965	449.881895	9.831616
8.384698	458.124114	9.836634
8.238076	465.995080	9.841651
8.383927	463.753983	9.846669
8.198497	457.174957	9.851687
8.222809	461.541781	9.856704
8.358678	456.834521	9.861722
8.147862	456.595993	9.866739
8.231161	467.097685	9.871757
8.182538	465.243456	9.876775
8.190206	470.001018	9.881792
8.413382	458.580718	9.886810
8.299588	477.270458	9.891827
8.745812	470.050309	9.896845
8.499676	468.463505	9.901863
8.347309	455.997199	9.906880
8.308738	452.620383	9.911898
8.409712	459.815354	9.916915
8.574345	452.266689	9.921933
8.241274	449.172399	9.926951
7.860763	441.629724	9.931968
8.115493	458.100448	9.936986
8.121293	459.759452	9.942003
8.406749	458.780969	9.947021
8.349805	451.352005	9.952039
8.223614	458.093219	9.957056
8.505367	466.231987	9.962074
8.412530	464.368863	9.967091
8.459824	456.948912	9.972109
8.294470	460.843518	9.977127
8.053572	460.530782	9.982144
8.450709	464.116916	9.987162
8.192058	465.129162	9.992179
8.201662	463.026037	9.997197
8.238004	480.288141	10.002215
8.526335	473.133598	10.007232
8.932145	483.941674	10.012250
8.351069	481.700152	10.017267
8.361789	469.460896	10.022285
8.405020	478.927468	10.027303
8.080752	471.685277	10.032320
8.453636	484.044749	10.037338
8.627466	490.572014	10.042355
9.035065	485.197620	10.047373
8.736770	490.520352	10.052391
8.572569	489.116440	10.057408
8.694894	489.924211	10.062426
8.764267	488.547046	10.067443
8.411344	473.035190	10.072461
8.650254	477.996580	10.077479
8.804738	486.259309	10.082496
8.786809	469.369924	10.087514
8.357500	468.209252	10.092531
8.615733	459.516287	10.097549
8.594752	469.024408	10.102567
8.701622	466.136160	10.107584
8.701845	459.723878	10.112602
8.584264	485.773194	10.117619
8.574540	480.028297	10.122637
8.849225	481.370896	10.127655
8.418775	480.566989	10.132672
8.681228	481.166758	10.137690
8.720494	487.453054	10.142707
8.705870	480.187893	10.147725
8.801165	482.934288	10.152743
8.382129	486.218332	10.157760
8.544202	483.362510	10.162778
8.451276	488.940432	10.167795
8.625467	486.625496	10.172813
8.496721	482.028853	10.177831
8.400862	482.365689	10.182848
8.702541	482.694276	10.187866
8.251635	493.111907	10.192883
8.574076	484.598272	10.197901
8.887753	497.033241	10.202919
8.638714	509.795661	10.207936
9.010257	507.749783	10.212954
8.901032	504.910952	10.217971
9.016169	500.014414	10.222989
8.479854	494.124293	10.228007
8.744191	502.275256	10.233024
8.822589	504.210125	10.238042
9.138696	514.988007	10.243059
9.080242	510.579220	10.248077
8.848910	503.521352	10.253095
8.845203	495.569708	10.258112
8.950411	491.091265	10.263130
8.874606	498.954374	10.268147
9.073071	488.680249	10.273165
8.910936	488.058618	10.278183
8.769763	485.672868	10.283200
9.113710	483.281012	10.288218
9.020827	493.043326	10.293235
9.027186	490.167568	10.298253
8.975657	484.937238	10.303271
9.329823	482.401786	10.308288
8.994523	482.908440	10.313306
9.010089	490.883546	10.318323
8.855282	489.490794	10.323341
9.048902	487.838676	10.328359
8.918698	485.943500	10.333376
9.017291	486.792833	10.338394
8.708025	486.285624	10.343411
8.884051	487.138679	10.348429
9.006628	490.647651	10.353447
8.850501	501.934532	10.358464
9.211552	514.251688	10.363482
9.100394	509.510296	10.368499
9.018131	513.199481	10.373517
9.290182	520.238459	10.378535
8.979753	510.094045	10.383552
9.135950	508.738073	10.388570
9.336233	505.936256	10.393587
9.077770	497.172248	10.398605
8.943626	491.834864	10.403623
8.975412	504.752364	10.408640
9.142723	505.733003	10.413658
9.054928	516.854627	10.418675
9.249227	505.514528	10.423693
9.565672	510.492257	10.428711
8.938729	504.281743	10.433728
9.183018	489.942307	10.438746
9.140615	505.979679	10.443763
9.393757	511.317543	10.448781
8.870529	500.824432	10.453799
8.968418	513.548617	10.458816
9.005756	508.739926	10.463834
9.035163	516.375232	10.468851
9.228617	514.628468	10.473869
9.712480	516.727416	10.478887
9.384847	513.648047	10.483904
8.926997	508.045493	10.488922
9.129025	519.270309	10.493939
8.911905	516.896380	10.498957
9.304672	515.768649	10.503975
8.947550	523.391559	10.508992
9.652002	510.258505	10.514010
9.410499	511.151324	10.519027
9.503768	518.164490	10.524045
9.575338	515.382712	10.529063
9.309804	518.838513	10.534080
9.054846	509.900392	10.539098
9.180607	518.789273	10.544115
9.098081	520.869114	10.549133
9.271827	514.533933	10.554151
9.009884	515.934840	10.559168
9.360906	516.482952	10.564186
9.457110	525.953924	10.569203
9.249610	513.313133	10.574221
9.410842	506.159432	10.579239
9.215429	520.611254	10.584256
9.419570	508.171451	10.589274
9.366797	513.762063	10.594291
9.457626	514.331753	10.599309
9.131427	512.871014	10.604327
9.378698	518.200327	10.609344
9.734364	529.328649	10.614362
9.601456	528.781357	10.619379
9.336531	520.125637	10.624397
9.309093	522.253703	10.629415
9.308931	532.418149	10.634432
9.470690	530.619516	10.639450
9.775368	534.138012	10.644467
9.614908	541.272740	10.649485
10.070427	523.586942	10.654503
9.651521	521.481104	10.659520
9.515096	511.091857	10.664538
9.343181	511.017677	10.669555
9.537958	516.023818	10.674573
9.911812	506.583871	10.679591
9.499465	515.285144	10.684608
9.646711	517.518550	10.689626
10.117093	522.869928	10.694643
9.720465	511.880594	10.699661
9.770293	507.511751	10.704679
9.196867	514.745477	10.709696
9.461681	513.827008	10.714714
9.515916	507.267450	10.719731
9.613153	518.732634	10.724749
9.570729	510.673407	10.729767
9.831141	520.696296	10.734784
9.634809	515.624196	10.739802
9.583888	518.790974	10.744819
9.270332	518.104559	10.749837
9.772071	522.475956	10.754855
9.512912	539.241351	10.759872
9.836148	534.697394	10.764890
9.680230	532.105660	10.769907
9.614545	538.099059	10.774925
9.998297	545.818057	10.779943
9.732198	545.275724	10.784960
9.636294	545.700927	10.789978
9.830041	535.465378	10.794995
9.704305	535.740598	10.800013
10.138507	538.901272	10.805031
9.877757	544.107727	10.810048
9.799733	543.163743	10.815066
9.530793	532.924498	10.820083
9.902718	545.498748	10.825101
9.786489	537.441534	10.830119
9.742318	546.120211	10.835136
10.090273	542.550660	10.840154
10.064249	543.987418	10.845171
9.584480	542.913488	10.850189
10.027314	544.403474	10.855207
10.121866	544.363541	10.860224
9.923416	539.253896	10.865242
9.627281	538.331249	10.870259
9.591945	539.592739	10.875277
10.090234	538.902993	10.880295
9.942287	548.140603	10.885312
9.781748	540.907604	10.890330
9.880448	543.678723	10.895347
9.649388	548.037994	10.900365
9.916623	538.860771	10.905383
9.669708	544.809809	10.910400
9.525872	535.144349	10.915418
9.660045	532.337043	10.920435
9.509060	550.000749	10.925453
10.062366	555.055216	10.930471
10.012175	571.715526	10.935488
10.392810	568.368089	10.940506
10.410702	561.009475	10.945523
10.146317	542.085120	10.950541
9.987143	539.383443	10.955559
10.238955	540.546579	10.960576
10.136926	540.404716	10.965594
10.211324	536.454899	10.970611
9.866145	534.072504	10.975629
10.019073	530.924622	10.980647
9.886651	542.864215	10.985664
9.854261	539.514821	10.990682
10.288083	561.379190	10.995699
10.292344	565.903789	11.000717
10.112912	558.430737	11.005735
10.038598	559.038763	11.010752
10.417226	556.928663	11.015770
10.043324	541.072891	11.020787
9.970803	557.105531	11.025805
10.267822	552.019721	11.030823
10.327232	566.725383	11.035840
10.347244	563.885356	11.040858
10.285685	555.216889	11.045875
10.084798	553.058168	11.050893
10.059020	556.138991	11.055911
10.326300	556.914729	11.060928
10.327445	552.502963	11.065946
10.402133	567.625951	11.070963
10.218140	572.053635	11.075981
10.508942	557.186218	11.080999
10.300309	545.741578	11.086016
9.912100	546.322740	11.091034
10.212156	561.224449	11.096051
10.012236	567.387074	11.101069
10.234958	558.159970	11.106087
10.353100	565.838285	11.111104
10.264127	567.354270	11.116122
10.375143	564.932400	11.121139
10.361371	567.926153	11.126157
10.497266	563.597541	11.131175
10.312642	567.365788	11.136192
10.086928	569.360636	11.141210
10.657079	565.081172	11.146227
10.288271	567.874593	11.151245
10.290564	564.371478	11.156263
10.526829	568.004770	11.161280
10.639904	563.389390	11.166298
10.778624	566.870618	11.171315
10.614327	568.859059	11.176333
10.820808	568.833256	11.181351
10.364459	568.124892	11.186368
10.469813	568.269463	11.191386
10.667451	559.866738	11.196403
10.515056	561.764966	11.201421
10.278306	562.975770	11.206439
10.014750	565.036467	11.211456
10.507810	568.184827	11.216474
10.593894	556.883634	11.221491
10.657684	562.828481	11.226509
10.720149	558.605974	11.231527
10.298075	565.181866	11.236544
10.414008	564.889307	11.241562
10.703421	553.228269	11.246579
10.042709	566.272567	11.251597
10.280875	559.482390	11.256615
10.228535	569.759118	11.261632
10.548498	583.512239	11.266650
10.900436	581.377890	11.271667
10.738459	586.206077	11.276685
10.808051	588.236996	11.281703
11.051755	587.675245	11.286720
10.503968	579.723071	11.291738
10.433566	571.011794	11.296755
10.663129	581.853683	11.301773
10.620092	584.419668	11.306791
10.773845	589.662581	11.311808
10.729991	596.211154	11.316826
10.625810	583.923440	11.321843
10.742034	584.331395	11.326861
11.042029	581.413060	11.331879
11.169836	588.348297	11.336896
10.971004	572.465238	11.341914
11.030634	574.554509	11.346931
10.976373	573.079827	11.351949
10.585071	561.474277	11.356967
10.609199	573.900735	11.361984
10.769591	568.214526	11.367002
10.941666	570.137973	11.372019
10.847669	578.922250	11.377037
10.901364	576.859582	11.382055
10.813347	576.248498	11.387072
10.647956	587.902932	11.392090
11.070809	583.005796	11.397107
10.681828	593.672609	11.402125
10.904700	599.955603	11.407143
10.961471	584.692274	11.412160
11.128567	587.815653	11.417178
11.172761	586.597028	11.422195
11.116848	586.075615	11.427213
10.951047	563.516332	11.432231
10.916859	572.095642	11.437248
10.668874	577.618842	11.442266
11.290978	579.661562	11.447283
11.056124	586.050529	11.452301
11.175296	574.368648	11.457319
11.236105	571.108875	11.462336
10.541038	567.625977	11.467354
11.036370	576.485747	11.472371
11.119697	593.343030	11.477389
11.390258	586.064981	11.482407
10.771717	577.991287	11.487424
10.640712	581.968930	11.492442
11.380909	578.745382	11.497459
11.173383	588.582400	11.502477
10.830700	600.217111	11.507495
11.237848	589.774743	11.512512
11.146159	590.953497	11.517530
11.762557	586.253434	11.522547
11.428545	584.604565	11.527565
10.889718	563.857914	11.532583
10.954103	566.476596	11.537600
11.052499	576.906577	11.542618
11.284795	583.995950	11.547635
11.370066	596.109959	11.552653
11.262726	590.566409	11.557671
11.500664	590.643002	11.562688
11.220380	578.947575	11.567706
11.068584	566.187625	11.572723
11.177143	578.935442	11.577741
10.691154	586.452217	11.582759
11.181241	589.140316	11.587776
10.978809	586.013040	11.592794
11.096394	591.602397	11.597811
11.275869	593.679322	11.602829
11.014771	584.839945	11.607847
11.087187	592.973496	11.612864
11.105148	600.430748	11.617882
11.491812	583.746493	11.622899
11.288581	593.750095	11.627917
11.244831	588.556392	11.632935
11.367830	595.495536	11.637952
11.355417	597.264680	11.642970
11.681665	593.111543	11.647987
11.695419	593.816307	11.653005
11.205695	593.204653	11.658023
11.391991	589.543502	11.663040
11.323888	590.119005	11.668058
11.720664	587.390720	11.673075
11.411113	586.804660	11.678093
11.308591	588.288044	11.683111
11.384658	592.536394	11.688128
11.547127	607.263912	11.693146
11.541363	601.502580	11.698163
11.560410	605.292771	11.703181
11.704808	601.903217	11.708199
11.427930	603.688293	11.713216
11.266230	595.142691	11.718234
11.697035	599.764983	11.723251
11.864588	598.984724	11.728269
11.735654	601.381056	11.733287
11.679946	592.758995	11.738304
11.224813	588.973659	11.743322
11.560000	594.497581	11.748339
11.654192	607.784120	11.753357
11.508409	615.894852	11.758375
11.885684	598.978525	11.763392
11.546003	615.930091	11.768410
11.898821	609.904653	11.773427
12.138692	603.126816	11.778445
11.876897	595.679195	11.783463
11.827352	589.470267	11.788480
11.545497	595.014524	11.793498
11.414013	592.684053	11.798515
11.307930	589.112604	11.803533
11.448935	606.181816	11.808551
11.413192	606.761749	11.813568
11.516281	609.301830	11.818586
11.612313	608.012020	11.823603
11.740659	615.152302	11.828621
11.610866	609.867851	11.833639
12.046822	610.169223	11.838656
11.659682	607.966914	11.843674
11.373679	607.708533	11.848691
11.888354	618.900513	11.853709
11.723433	614.233732	11.858727
11.645136	617.679335	11.863744
11.984770	622.000259	11.868762
11.950144	609.878416	11.873779
11.744898	614.514539	11.878797
11.850443	611.288817	11.883815
11.666312	615.987922	11.888832
12.132738	635.243871	11.893850
12.042198	630.063752	11.898867
11.806485	625.565775	11.903885
11.792589	637.136696	11.908903
12.118707	630.253907	11.913920
11.929619	641.877354	11.918938
12.001426	642.683530	11.923955
12.204377	643.096917	11.928973
11.848305	641.347340	11.933991
12.266364	634.933053	11.939008
12.157269	641.444466	11.944026
12.403569	628.644579	11.949043
12.178380	615.700368	11.954061
11.986670	617.188174	11.959079
12.321447	611.784056	11.964096
12.400498	617.543517	11.969114
11.978072	610.502736	11.974131
12.055199	601.096315	11.979149
11.885528	612.764055	11.984167
11.755679	614.854431	11.989184
11.691571	614.914937	11.994202
12.193095	631.691367	11.999219
12.178576	638.954884	12.004237
12.250149	641.938517	12.009255
12.279093	636.187549	12.014272
12.163681	642.302329	12.019290
12.503103	639.999516	12.024307
12.579246	640.038186	12.029325
12.028479	639.319274	12.034343
12.248635	623.266798	12.039360
12.281230	633.713369	12.044378
12.651004	627.956672	12.049395
12.285668	619.739398	12.054413
11.911852	623.997842	12.059431
12.330813	629.451929	12.064448
12.446753	638.762105	12.069466
12.321700	632.968845	12.074483
12.629734	634.912154	12.079501
11.999547	634.101470	12.084519
12.496364	642.348840	12.089536
12.632624	644.129554	12.094554
12.396059	635.352601	12.099571
12.418925	629.154475	12.104589
11.875584	628.753131	12.109607
12.489520	626.205615	12.114624
12.363503	640.498413	12.119642
12.483823	636.348927	12.124659
12.211828	634.772445	12.129677
12.013988	636.557842	12.134695
12.262150	637.977163	12.139712
12.257832	641.073593	12.144730
12.226830	635.590725	12.149747
12.566120	639.533025	12.154765
12.185347	642.965769	12.159783
12.550092	636.585028	12.164800
12.134068	644.939812	12.169818
12.310067	656.960844	12.174835
12.591271	659.586806	12.179853
12.786800	674.631112	12.184871
12.746737	667.615980	12.189888
12.750169	667.388270	12.194906
12.448097	666.154128	12.199923
12.613953	653.388837	12.204941
12.529733	661.417424	12.209959
12.828311	658.133238	12.214976
12.794122	662.868968	12.219994
12.875092	654.108837	12.225011
12.528021	643.752309	12.230029
12.450566	655.339450	12.235047
12.884822	661.608488	12.240064
12.811542	659.291036	12.245082
12.768917	662.099956	12.250099
12.908100	655.044298	12.255117
12.526858	664.324603	12.260135
12.815090	661.013626	12.265152
12.536880	661.186359	12.270170
12.550535	650.341336	12.275187
12.688018	652.879224	12.280205
12.585970	667.083108	12.285223
12.919868	666.431575	12.290240
13.038967	663.869584	12.295258
12.905898	651.892422	12.300275
13.112837	648.603571	12.305293
12.861986	659.425636	12.310311
13.059056	656.434954	12.315328
13.006245	658.680592	12.320346
12.934510	663.100288	12.325363
12.808100	656.603514	12.330381
12.480416	666.004863	12.335399
12.762270	660.709953	12.340416
12.788288	658.673675	12.345434
12.607347	663.829870	12.350451
12.770925	656.688366	12.355469
12.268261	663.153770	12.360487
12.706026	667.102835	12.365504
12.979626	679.171800	12.370522
13.116324	688.406188	12.375539
13.095555	685.313725	12.380557
13.001125	690.049374	12.385575
13.022138	695.035284	12.390592
12.937791	695.411356	12.395610
13.239772	698.355969	12.400627
13.516794	693.112292	12.405645
13.143484	689.945333	12.410663
13.845512	688.526453	12.415680
13.457211	678.384601	12.420698
13.297709	669.071789	12.425715
13.147607	667.873943	12.430733
13.000925	659.837193	12.435751
13.311568	664.468743	12.440768
13.075656	666.774447	12.445786
12.836409	662.718806	12.450803
13.302972	659.916530	12.455821
12.812740	671.208201	12.460839
13.261357	669.478496	12.465856
13.393169	679.300598	12.470874
13.372214	686.833371	12.475891
13.509703	683.593195	12.480909
13.086838	671.872571	12.485927
13.188355	678.840337	12.490944
13.239584	687.478985	12.495962
13.350079	691.444297	12.500979
13.538243	692.169245	12.505997
13.496413	693.172991	12.511015
13.238462	690.638143	12.516032
13.576375	687.511924	12.521050
13.213652	690.941866	12.526067
13.820317	689.272755	12.531085
13.152651	691.424786	12.536103
13.486602	693.872133	12.541120
13.664487	685.888975	12.546138
13.489236	692.480132	12.551155
13.668658	682.063699	12.556173
13.280627	673.944603	12.561191
13.477528	681.547591	12.566208
13.428497	687.768813	12.571226
13.241065	684.755944	12.576243
13.585784	679.766809	12.581261
13.701506	695.710308	12.586279
13.530392	687.402804	12.591296
13.584916	695.005876	12.596314
13.523563	692.759143	12.601331
13.387023	681.101227	12.606349
13.337578	688.363891	12.611367
13.699855	691.624151	12.616384
13.892345	686.901704	12.621402
13.459691	701.166556	12.626419
13.867305	686.170396	12.631437
13.707604	686.867457	12.636455
13.829621	684.879343	12.641472
14.006100	684.621535	12.646490
13.700249	681.541901	12.651507
13.749646	683.377167	12.656525
13.789065	688.505372	12.661543
13.508649	686.680897	12.666560
13.689108	687.220859	12.671578
13.449969	687.434845	12.676595
13.844183	683.002872	12.681613
13.709565	688.006700	12.686631
13.511401	689.154702	12.691648
13.561519	689.547706	12.696666
13.345308	696.243068	12.701683
13.617224	688.822760	12.706701
14.063942	704.566414	12.711719
13.793792	702.074488	12.716736
14.005529	700.299614	12.721754
13.728870	702.280318	12.726771
14.012655	711.283542	12.731789
14.052387	708.311038	12.736807
13.979844	705.800968	12.741824
14.414082	705.704992	12.746842
13.780154	701.041785	12.751859
13.946140	692.505075	12.756877
13.978312	694.185240	12.761895
13.935435	683.610920	12.766912
14.142080	692.234839	12.771930
13.804406	691.277627	12.776947
14.364549	705.753969	12.781965
14.416760	695.126969	12.786983
13.830413	690.364842	12.792000
14.000529	687.665520	12.797018
13.389846	687.571294	12.802035
14.209038	702.616349	12.807053
14.225899	716.760735	12.812071
14.080449	717.578650	12.817088
14.151062	705.607609	12.822106
14.072993	708.169599	12.827123
14.228365	708.470479	12.832141
14.388660	706.189235	12.837159
14.058178	705.372908	12.842176
14.282463	702.643060	12.847194
14.076395	699.730918	12.852211
14.583916	697.474505	12.857229
14.353996	695.484383	12.862247
14.140087	701.630298	12.867264
14.272834	696.554245	12.872282
13.766928	709.710239	12.877299
14.331408	700.344648	12.882317
14.409920	705.687669	12.887335
14.227606	702.689779	12.892352
14.553824	704.586086	12.897370
14.845536	712.691859	12.902387
14.743214	694.972829	12.907405
14.769235	703.400822	12.912423
14.290807	699.193071	12.917440
14.296763	701.609439	12.922458
13.948704	710.528007	12.927475
14.040335	710.352835	12.932493
14.078863	714.272555	12.937511
14.257542	710.685146	12.942528
14.389580	701.257500	12.947546
14.491697	707.240608	12.952563
14.181494	701.542423	12.957581
14.444344	706.061509	12.962599
14.110428	713.182288	12.967616
14.614082	713.747667	12.972634
15.059119	729.867133	12.977651
14.548274	724.698779	12.982669
14.516333	714.895884	12.987687
14.462556	728.259198	12.992704
14.765496	718.180106	12.997722
14.563202	728.227818	13.002739
14.823664	727.698166	13.007757
14.556474	741.498647	13.012775
14.618652	728.241378	13.017792
14.974963	723.357719	13.022810
14.944832	733.861451	13.027827
14.897218	727.421808	13.032845
15.114785	718.902300	13.037863
14.724240	714.311646	13.042880
14.721709	702.298347	13.047898
14.410242	712.798534	13.052915
14.500237	707.350451	13.057933
14.633374	711.747728	13.062951
14.728113	726.293393	13.067968
15.121777	725.316983	13.072986
14.851988	728.293821	13.078003
15.055005	734.564175	13.083021
15.053793	733.797564	13.088039
14.700978	736.418113	13.093056
14.779860	727.349012	13.098074
14.763160	735.982481	13.103091
14.984368	733.641259	13.108109
14.928086	735.991584	13.113127
14.681962	735.218925	13.118144
14.763263	724.729384	13.123162
14.730214	727.609404	13.128179
14.744505	734.931589	13.133197
14.728917	733.438249	13.138215
14.417793	731.501790	13.143232
14.645528	725.505254	13.148250
14.830740	747.515853	13.153267
15.292367	750.536601	13.158285
15.197542	746.875008	13.163303
15.053348	761.628310	13.168320
15.551890	753.197578	13.173338
15.425616	751.765650	13.178355
15.177370	737.291270	13.183373
15.283255	729.543357	13.188391
15.324715	731.660721	13.193408
15.247766	719.374985	13.198426
15.010753	728.364633	13.203443
14.693162	721.203348	13.208461
15.053546	736.373513	13.213479
15.347202	746.574383	13.218496
15.222072	749.689643	13.223514
15.068671	762.137561	13.228531
15.158117	754.370107	13.233549
15.236188	756.750009	13.238567
15.694665	751.118313	13.243584
15.401777	748.809796	13.248602
15.294189	756.147809	13.253619
15.577023	747.618126	13.258637
15.480368	746.547648	13.263655
15.287069	758.042443	13.268672
15.025912	755.719517	13.273690
15.120895	757.172165	13.278707
15.078554	751.934015	13.283725
15.647621	745.152206	13.288743
15.382174	748.630127	13.293760
15.772275	750.510181	13.298778
15.710889	746.193307	13.303795
15.560947	746.380783	13.308813
15.659284	748.602898	13.313831
15.821669	752.825224	13.318848
15.729800	752.009613	13.323866
15.514216	760.008206	13.328883
15.377869	753.086923	13.333901
15.574394	743.715485	13.338919
15.461381	763.184861	13.343936
15.635984	747.884112	13.348954
15.776918	753.564556	13.353971
15.980295	748.221880	13.358989
15.779829	744.141248	13.364007
15.477968	751.660981	13.369024
15.706091	750.230677	13.374042
15.699257	743.191407	13.379059
15.791873	741.261512	13.384077
15.826851	741.174052	13.389095
16.061076	744.416391	13.394112
16.011693	746.854004	13.399130
15.944350	744.409388	13.404147
15.762451	736.949268	13.409165
15.767773	730.163722	13.414183
15.717058	744.025172	13.419200
15.592861	746.767912	13.424218
15.484539	746.175762	13.429235
15.675781	748.011040	13.434253
16.038246	739.582568	13.439271
15.603371	754.005593	13.444288
15.824776	739.309770	13.449306
15.704445	742.866079	13.454323
15.686029	746.602174	13.459341
15.799226	737.688666	13.464359
15.596736	739.793522	13.469376
15.578432	744.160739	13.474394
16.191006	764.867786	13.479411
16.093617	765.264824	13.484429
16.172448	762.279912	13.489447
16.057664	759.656494	13.494464
15.963515	752.504587	13.499482
15.820320	764.834157	13.504499
16.015411	770.294743	13.509517
16.118669	769.082688	13.514535
16.398422	772.059176	13.519552
16.184807	772.486932	13.524570
16.216947	770.386574	13.529587
16.001169	766.810079	13.534605
16.342243	768.480024	13.539623
16.627907	764.547754	13.544640
16.250005	754.104447	13.549658
16.201276	740.921238	13.554675
15.852106	743.295076	13.559693
16.494837	748.979440	13.564711
16.480229	760.692559	13.569728
16.089584	757.578778	13.574746
16.371742	753.820620	13.579763
16.290665	763.464483	13.584781
16.637924	761.523340	13.589799
16.257763	767.774055	13.594816
16.444630	759.136235	13.599834
16.305666	760.865141	13.604851
16.301922	768.796043	13.609869
16.439776	765.256003	13.614887
16.116492	773.536450	13.619904
16.644582	771.384120	13.624922
16.602849	766.212141	13.629939
16.416554	772.240175	13.634957
16.678691	761.529960	13.639975
16.400557	761.967761	13.644992
16.616211	760.908616	13.650010
16.514746	762.407628	13.655027
16.297598	762.211106	13.660045
16.493110	759.353189	13.665063
16.208560	756.175555	13.670080
16.256016	762.107233	13.675098
16.603299	761.829142	13.680115
16.600985	761.558147	13.685133
16.671832	754.033422	13.690151
16.504857	758.379611	13.695168
16.631005	758.173818	13.700186
16.575816	758.763094	13.705203
16.548804	765.593121	13.710221
16.584208	759.314105	13.715239
16.675485	759.208412	13.720256
16.845960	765.622695	13.725274
16.810965	767.695164	13.730291
16.509754	768.357459	13.735309
16.848303	770.166648	13.740327
17.034749	774.975350	13.745344
17.000790	778.821166	13.750362
16.884587	774.762120	13.755379
16.990876	774.540485	13.760397
16.823848	765.746330	13.765415
17.059690	767.038196	13.770432
16.772070	773.201924	13.775450
16.965189	767.441130	13.780467
17.125259	782.491049	13.785485
16.675209	764.027696	13.790503
16.851984	771.087920	13.795520
17.076289	782.849060	13.800538
16.803714	775.371485	13.805555
17.316238	782.565625	13.810573
17.289126	783.185243	13.815591
17.132570	778.652812	13.820608
16.695240	774.271391	13.825626
16.874944	771.841955	13.830643
16.964350	780.818675	13.835661
17.212830	776.273674	13.840679
17.312336	773.597956	13.845696
17.166778	768.647262	13.850714
17.170836	773.149855	13.855731
17.216242	777.841666	13.860749
17.466383	770.617213	13.865767
17.347896	776.678872	13.870784
17.380874	770.125683	13.875802
17.201614	773.404003	13.880819
17.248297	771.269824	13.885837
17.270637	774.456798	13.890855
17.309412	776.176967	13.895872
17.394731	780.938301	13.900890
17.414359	776.302702	13.905907
17.216569	779.899480	13.910925
17.392471	777.385431	13.915943
17.399572	781.142806	13.920960
17.567014	780.592923	13.925978
17.536378	770.531026	13.930995
17.560015	779.880892	13.936013
17.441918	775.976771	13.941031
17.293726	773.945514	13.946048
17.149334	775.419654	13.951066
17.472145	778.373660	13.956083
17.284343	787.841655	13.961101
17.229895	783.318570	13.966119
17.482222	781.335403	13.971136
17.401135	778.179733	13.976154
17.716015	778.837620	13.981171
17.390081	778.528650	13.986189
17.458456	775.734706	13.991207
17.290479	781.655754	13.996224
17.342636	791.859538	14.001242
17.652351	790.883573	14.006259
17.668644	801.250732	14.011277
17.494922	801.785883	14.016295
17.792516	799.416981	14.021312
17.723491	806.531267	14.026330
17.905441	801.961905	14.031347
17.635608	803.310415	14.036365
17.697270	803.262980	14.041383
17.577418	808.422329	14.046400
17.586043	803.791592	14.051418
17.403576	802.589308	14.056435
17.487509	802.005091	14.061453
17.563785	803.277624	14.066471
17.642674	812.994435	14.071488
17.876263	826.912666	14.076506
18.310381	823.869271	14.081523
18.045612	825.343224	14.086541
17.665007	811.754056	14.091559
18.240279	817.357429	14.096576
18.065056	831.787426	14.101594
18.029364	806.629357	14.106611
17.688642	819.658730	14.111629
18.138182	818.881894	14.116647
18.231872	829.760867	14.121664
18.150267	828.280954	14.126682
18.366684	822.923602	14.131699
17.976025	817.906917	14.136717
18.128376	804.389406	14.141735
18.046739	813.654698	14.146752
18.044686	825.466888	14.151770
18.519888	825.064741	14.156787
18.248892	826.388189	14.161805
18.217299	797.303786	14.166823
18.277515	808.692873	14.171840
18.357237	800.295771	14.176858
18.367339	801.468156	14.181875
18.235921	796.007184	14.186893
18.008156	799.523428	14.191911
18.030184	811.451777	14.196928
18.073832	829.700820	14.201946
18.197588	824.667155	14.206963
18.772278	827.165398	14.211981
18.504792	828.305268	14.216999
18.483360	828.886135	14.222016
18.793145	833.328521	14.227034
18.655642	825.511167	14.232051
18.377553	811.539975	14.237069
18.468873	809.853264	14.242087
18.848239	813.776742	14.247104
18.488447	805.984539	14.252122
18.213744	799.981001	14.257139
18.377740	813.162154	14.262157
18.415377	824.207638	14.267175
18.868006	821.315991	14.272192
18.802783	825.523280	14.277210
18.672884	822.791757	14.282227
18.898116	828.004677	14.287245
18.534121	809.603615	14.292263
18.585633	809.775505	14.297280
18.481605	821.953854	14.302298
18.836018	820.453391	14.307315
18.545236	829.091710	14.312333
18.884724	825.611781	14.317351
18.953469	818.021087	14.322368
18.817499	821.876483	14.327386
19.169660	818.258887	14.332403
18.602195	817.574124	14.337421
18.960661	812.668016	14.342439
18.991064	820.237028	14.347456
18.532485	818.822120	14.352474
18.859054	809.566095	14.357491
18.914781	824.165249	14.362509
18.695286	820.538830	14.367527
18.744750	823.311347	14.372544
18.625622	819.331640	14.377562
19.147223	822.478758	14.382579
18.994786	825.301645	14.387597
19.099255	824.023128	14.392615
18.967773	823.816423	14.397632
18.653270	823.070184	14.402650
19.016511	822.073260	14.407667
18.904440	815.088215	14.412685
18.599056	816.612670	14.417703
19.049263	820.061230	14.422720
18.665784	825.675028	14.427738
19.072302	830.623045	14.432755
19.442490	847.350701	14.437773
19.041147	842.547106	14.442791
19.166576	843.354410	14.447808
19.103329	854.933157	14.452826
19.363750	849.584725	14.457843
19.475074	846.771460	14.462861
19.374634	841.091061	14.467879
19.537247	841.873641	14.472896
19.259795	848.414497	14.477914
19.392888	842.012948	14.482931
19.256296	847.537821	14.487949
19.102710	847.959389	14.492967
19.261872	840.689114	14.497984
18.930752	848.181885	14.503002
19.353470	840.173162	14.508019
19.347584	848.969099	14.513037
19.271037	847.627249	14.518055
19.646464	841.273173	14.523072
19.354228	854.096212	14.528090
19.539778	842.757261	14.533107
19.568453	840.111495	14.538125
19.161975	837.672333	14.543143
19.363824	846.287607	14.548160
19.568178	845.832958	14.553178
19.612587	848.675692	14.558195
19.561066	849.832430	14.563213
19.542556	863.581663	14.568231
20.353064	857.595331	14.573248
19.629039	855.991381	14.578266
19.691720	842.371041	14.583283
19.555202	840.271689	14.588301
19.490328	853.823012	14.593319
19.700277	855.210432	14.598336
20.069546	871.641617	14.603354
20.105481	855.541877	14.608371
20.087434	850.634422	14.613389
19.841249	837.579712	14.618407
19.694628	834.964396	14.623424
19.786374	839.052578	14.628442
19.587307	847.547241	14.633459
19.387949	860.043408	14.638477
19.719961	864.255128	14.643495
20.246551	861.276223	14.648512
20.125515	866.451551	14.653530
19.990263	862.461722	14.658547
19.948176	863.976743	14.663565
20.166837	857.126376	14.668583
20.252547	853.632307	14.673600
20.543650	852.078584	14.678618
20.419327	859.980964	14.683635
20.261038	844.170243	14.688653
20.101765	846.350431	14.693671
20.142270	843.971059	14.698688
20.239981	841.895196	14.703706
20.164219	840.051465	14.708723
20.152376	843.243773	14.713741
19.972391	853.736194	14.718759
20.364539	851.967929	14.723776
20.331654	860.929017	14.728794
20.197771	861.675712	14.733811
20.426872	860.863769	14.738829
20.076639	865.989578	14.743847
20.366214	860.655538	14.748864
20.555582	861.762148	14.753882
20.607654	863.164682	14.758899
20.670056	858.434042	14.763917
20.270857	861.087077	14.768935
20.593388	863.116515	14.773952
20.242486	862.315983	14.778970
20.362448	867.438011	14.783987
20.752220	864.442538	14.789005
20.392503	869.737077	14.794023
20.313212	855.081664	14.799040
20.451063	858.604110	14.804058
20.328680	853.870684	14.809075
20.346768	857.657922	14.814093
20.300167	857.305460	14.819111
20.583798	854.888233	14.824128
20.331286	851.708748	14.829146
20.823461	851.979282	14.834163
20.374710	855.466830	14.839181
20.212081	862.863948	14.844199
20.449309	863.742207	14.849216
20.749730	876.450898	14.854234
20.439168	884.909291	14.859251
20.960015	873.338240	14.864269
20.996735	881.947684	14.869287
20.928446	875.836245	14.874304
21.100231	883.058232	14.879322
21.044419	882.328517	14.884339
21.471533	878.781287	14.889357
20.961764	861.598888	14.894375
20.661450	859.171594	14.899392
20.524587	862.462265	14.904410
20.620790	868.316963	14.909427
20.837041	868.210747	14.914445
20.772719	877.665875	14.919463
21.087729	879.996280	14.924480
21.022701	878.687346	14.929498
21.178335	884.457060	14.934515
21.463189	879.382518	14.939533
21.236410	882.201210	14.944551
21.165239	873.950640	14.949568
21.548698	877.816692	14.954586
20.971980	881.949002	14.959603
21.286253	882.338751	14.964621
21.236662	878.139926	14.969639
21.607778	873.793551	14.974656
21.481291	874.274014	14.979674
21.574664	875.534423	14.984691
21.441876	863.623345	14.989709
21.064472	858.573027	14.994727
20.874251	854.285653	14.999744
21.460968	881.453467	15.004762
20.986635	884.405374	15.009779
21.571875	873.512245	15.014797
21.254552	883.098284	15.019815
21.285943	875.447111	15.024832
21.595077	876.500362	15.029850
21.295934	878.992658	15.034867
21.479701	878.913589	15.039885
21.058973	884.246033	15.044903
21.384568	879.079944	15.049920
21.234657	881.334416	15.054938
21.568723	891.058876	15.059955
21.605209	878.771146	15.064973
21.448546	893.034206	15.069991
21.937909	895.088164	15.075008
21.787428	887.799810	15.080026
21.241997	888.105666	15.085043
22.041930	893.030317	15.090061
21.715557	889.950685	15.095079
21.768396	888.752784	15.100096
21.819173	893.386986	15.105114
21.757054	899.717614	15.110131
22.011599	895.231597	15.115149
21.983562	894.923580	15.120167
21.904540	879.302453	15.125184
21.557909	881.278292	15.130202
21.860312	885.967987	15.135219
22.305990	889.944272	15.140237
21.546197	885.947536	15.145255
22.020408	894.381576	15.150272
22.124784	902.904759	15.155290
21.902207	904.580426	15.160307
22.273497	896.898413	15.165325
22.053649	906.788016	15.170343
22.061808	897.319596	15.175360
22.540187	892.508402	15.180378
21.722212	880.969074	15.185395
21.989457	886.544690	15.190413
21.888633	892.739334	15.195431
21.930712	900.669472	15.200448
22.192098	891.903223	15.205466
22.084792	904.009557	15.210483
22.394196	895.980583	15.215501
22.142478	901.463439	15.220519
22.519338	898.662470	15.225536
22.510230	896.600077	15.230554
22.369141	897.657157	15.235571
22.564007	890.122533	15.240589
21.993729	906.150937	15.245607
22.195100	901.414428	15.250624
22.255015	892.471270	15.255642
22.184689	890.434187	15.260659
22.498605	896.453809	15.265677
22.390592	902.712690	15.270695
22.351333	898.357621	15.275712
22.411785	894.536125	15.280730
22.067295	901.201044	15.285747
22.425619	889.970859	15.290765
22.584800	896.980225	15.295783
22.588465	905.900932	15.300800
22.636696	907.509190	15.305818
22.663200	913.049715	15.310835
22.503397	902.187364	15.315853
22.589355	916.785044	15.320871
22.886716	917.035419	15.325888
22.895133	924.996054	15.330906
22.941627	926.661388	15.335923
22.945360	908.101987	15.340941
22.645938	907.943517	15.345959
22.695692	900.096975	15.350976
22.799816	899.938790	15.355994
22.918506	919.571074	15.361011
22.884710	924.369927	15.366029
22.885520	922.978157	15.371047
23.257007	918.537042	15.376064
22.952781	916.451169	15.381082
22.713550	923.020814	15.386099
22.762325	924.180875	15.391117
22.975015	921.803086	15.396135
23.001898	917.614435	15.401152
23.009061	921.034167	15.406170
22.897998	918.649982	15.411187
23.079553	913.171802	15.416205
23.256208	920.910586	15.421223
22.984097	920.605856	15.426240
23.125455	915.408483	15.431258
22.947691	922.949991	15.436275
23.000482	912.660434	15.441293
23.060446	922.847299	15.446311
22.859619	925.671425	15.451328
23.074509	928.291973	15.456346
23.087156	938.047567	15.461363
22.949418	939.025234	15.466381
23.016031	947.450178	15.471399
23.444883	941.930331	15.476416
23.617095	928.434879	15.481434
23.483888	940.002484	15.486451
23.553271	938.401226	15.491469
23.788684	942.063129	15.496487
23.944591	937.466229	15.501504
23.801908	930.173488	15.506522
23.250748	932.525152	15.511539
23.484418	933.050525	15.516557
23.713328	939.250651	15.521575
23.529026	942.561345	15.526592
23.741188	939.530398	15.531610
23.659081	945.460220	15.536627
23.734405	944.580699	15.541645
23.914087	943.703865	15.546663
23.914214	924.239313	15.551680
23.639357	922.372923	15.556698
23.981060	918.968369	15.561715
23.552694	914.998918	15.566733
23.396573	925.396150	15.571751
23.499228	933.944861	15.576768
23.870970	933.909107	15.581786
23.984401	945.687618	15.586803
23.876501	938.045482	15.591821
24.045974	935.794338	15.596839
24.047536	944.008507	15.601856
24.185489	937.079159	15.606874
23.908874	935.951483	15.611891
23.791866	933.707074	15.616909
24.015657	940.318242	15.621927
24.057712	934.839685	15.626944
24.099869	932.788240	15.631962
23.792234	941.788991	15.636979
24.022031	937.458292	15.641997
23.980681	940.487958	15.647015
24.121526	939.737089	15.652032
24.169323	936.447717	15.657050
24.161824	942.915020	15.662067
23.922520	934.886255	15.667085
23.956870	941.186099	15.672103
23.761285	941.639454	15.677120
23.973060	950.067044	15.682138
24.103334	962.767575	15.687155
24.365769	960.025437	15.692173
24.551569	958.450232	15.697191
24.448604	967.854621	15.702208
24.413174	960.968037	15.707226
24.568279	958.400397	15.712243
24.532133	952.091428	15.717261
24.311135	964.064029	15.722279
24.297295	962.917529	15.727296
24.061809	957.507422	15.732314
24.188207	966.424830	15.737331
24.874871	963.556682	15.742349
25.044473	960.623874	15.747367
24.135290	951.601202	15.752384
24.498828	948.963242	15.757402
24.326272	966.166825	15.762419
24.757707	971.082601	15.767437
25.153448	989.706170	15.772455
24.549891	972.939044	15.777472
24.882285	967.219616	15.782490
24.783116	980.353506	15.787507
25.108092	984.556884	15.792525
25.062787	969.861372	15.797543
24.840476	960.744375	15.802560
24.963959	958.828585	15.807578
24.905210	958.418053	15.812595
24.881267	961.454480	15.817613
25.246146	971.092137	15.822631
24.776447	965.611199	15.827648
25.148651	963.375823	15.832666
24.928773	971.823294	15.837683
24.819745	976.690677	15.842701
24.959295	973.617383	15.847719
24.978170	980.531864	15.852736
25.125443	971.625556	15.857754
24.739847	984.652569	15.862771
24.865950	980.060299	15.867789
25.045006	981.720778	15.872807
24.778754	976.526890	15.877824
25.255159	976.957669	15.882842
24.926062	975.257506	15.887859
24.846144	977.876626	15.892877
25.336679	991.278464	15.897895
25.724216	992.344761	15.902912
25.720087	988.867809	15.907930
25.362206	991.754266	15.912947
25.838837	993.229562	15.917965
25.724900	976.509275	15.922983
25.798094	977.116439	15.928000
25.692851	964.371044	15.933018
25.398034	962.043865	15.938035
25.519904	968.055543	15.943053
25.731146	963.664611	15.948071
25.389470	958.495095	15.953088
25.709038	965.397467	15.958106
25.571809	967.489033	15.963123
25.396063	964.793027	15.968141
25.736271	953.915909	15.973159
25.630599	978.774380	15.978176
25.807163	989.476449	15.983194
26.164481	992.021184	15.988211
25.982821	979.148824	15.993229
26.062505	968.271236	15.998247
26.116076	974.154697	16.003264
25.741859	966.557169	16.008282
25.709397	968.689227	16.013299
25.991329	964.984707	16.018317
26.276647	962.627162	16.023335
25.809934	979.368483	16.028352
26.033748	965.644067	16.033370
25.704771	972.461229	16.038387
25.707813	968.954762	16.043405
26.271548	983.367657	16.048423
26.107853	991.178397	16.053440
25.997286	988.011501	16.058458
26.011544	987.924111	16.063475
26.271327	996.473634	16.068493
26.273452	992.878944	16.073511
26.196896	1005.008961	16.078528
26.499502	995.207471	16.083546
26.265729	996.619807	16.088563
26.200511	993.549989	16.093581
26.334485	992.872769	16.098599
26.145990	1005.847020	16.103616
26.491581	988.051648	16.108634
26.248525	1005.253623	16.113651
26.037477	1002.020319	16.118669
26.617608	992.188244	16.123687
26.274634	1002.002398	16.128704
26.333387	996.454952	16.133722
26.300201	996.188759	16.138739
26.134504	993.260814	16.143757
26.785933	995.504143	16.148775
26.492118	1010.612300	16.153792
26.874538	1014.226083	16.158810
26.646451	1011.957934	16.163827
26.339587	1007.871716	16.168845
27.024165	1011.328004	16.173863
27.209769	1017.411825	16.178880
26.566256	1001.073764	16.183898
26.483765	1003.494476	16.188915
26.847132	1015.306701	16.193933
26.926146	1007.906828	16.198951
26.630550	1019.951040	16.203968
26.858876	1018.782611	16.208986
26.973227	1022.955677	16.214003
26.623732	1023.164758	16.219021
27.137023	1017.767438	16.224039
27.101005	1026.369342	16.229056
27.439618	1016.764202	16.234074
27.410804	1026.340111	16.239091
27.044088	1017.835693	16.244109
27.386332	1024.254883	16.249127
26.998541	1002.354444	16.254144
27.190715	1003.845628	16.259162
27.276695	1001.525425	16.264179
26.995858	998.580694	16.269197
27.319554	998.514551	16.274215
27.285465	1010.521197	16.279232
27.128568	1015.414979	16.284250
27.632859	1013.493540	16.289267
27.079021	1017.975762	16.294285
27.399819	1013.024973	16.299303
27.276885	1018.569863	16.304320
27.128729	1020.293913	16.309338
27.134521	1015.562579	16.314355
26.978984	1022.649396	16.319373
27.233008	1006.616548	16.324391
26.982094	1011.117875	16.329408
27.188060	1027.110735	16.334426
27.244271	1034.552746	16.339443
27.425643	1031.583381	16.344461
27.841411	1032.383358	16.349479
27.694349	1040.892107	16.354496
28.097913	1040.251806	16.359514
28.024678	1029.928155	16.364531
27.652612	1036.821476	16.369549
27.886638	1027.671264	16.374567
28.140319	1037.749141	16.379584
27.829027	1031.192653	16.384602
27.878027	1032.333752	16.389619
27.767915	1031.461009	16.394637
27.921077	1023.812903	16.399655
27.893421	1034.704584	16.404672
27.672136	1030.365200	16.409690
28.286058	1037.133409	16.414707
27.811490	1034.111539	16.419725
27.936646	1027.357714	16.424743
27.986519	1031.881642	16.429760
28.089979	1034.980295	16.434778
28.340870	1027.992303	16.439795
27.891327	1030.893038	16.444813
28.014342	1020.731338	16.449831
27.750989	1027.677156	16.454848
27.673108	1023.441676	16.459866
27.784888	1039.594376	16.464883
28.256510	1050.032797	16.469901
28.324314	1046.680331	16.474919
28.364878	1057.217427	16.479936
28.368199	1058.495025	16.484954
28.443001	1053.964371	16.489971
28.577149	1053.369172	16.494989
28.730498	1050.262158	16.500007
28.535892	1052.167010	16.505024
28.495640	1056.417802	16.510042
28.739520	1050.636392	16.515059
28.819586	1055.871981	16.520077
28.915837	1052.666561	16.525095
28.400635	1042.465363	16.530112
28.569057	1044.035986	16.535130
28.400482	1049.423893	16.540147
28.402699	1056.113782	16.545165
28.541114	1053.820122	16.550183
28.314881	1057.452942	16.555200
28.436599	1055.654179	16.560218
28.593439	1050.905629	16.565235
28.518888	1057.313986	16.570253
28.745076	1059.143856	16.575271
28.468091	1061.733711	16.580288
28.819150	1075.311961	16.585306
29.235601	1072.400662	16.590323
28.963162	1075.299075	16.595341
29.053357	1073.524153	16.600359
29.007681	1070.034719	16.605376
28.853440	1076.023152	16.610394
29.072455	1070.621141	16.615411
29.065865	1079.543532	16.620429
29.229088	1075.917432	16.625447
29.323224	1075.233789	16.630464
29.110910	1077.302344	16.635482
29.402811	1064.138444	16.640499
29.278642	1070.014897	16.645517
29.572055	1070.919132	16.650535
29.511826	1065.772035	16.655552
29.424160	1079.611097	16.660570
29.842934	1068.425036	16.665587
29.571252	1071.301241	16.670605
29.479776	1058.790318	16.675623
29.423278	1063.488603	16.680640
29.434153	1066.535405	16.685658
29.704395	1065.499301	16.690675
29.272611	1064.493605	16.695693
29.589235	1064.693647	16.700711
29.488299	1078.578955	16.705728
29.368949	1073.535734	16.710746
29.724461	1067.314065	16.715763
29.395138	1074.595216	16.720781
29.877292	1066.542424	16.725799
30.145829	1072.335645	16.730816
29.771418	1070.879210	16.735834
29.976843	1070.654759	16.740851
29.756503	1073.178993	16.745869
29.843664	1077.258476	16.750887
29.443077	1078.804087	16.755904
29.601313	1081.307249	16.760922
29.798533	1064.806673	16.765939
29.771202	1063.936818	16.770957
29.894663	1060.575683	16.775975
30.029591	1065.685971	16.780992
29.953597	1077.329962	16.786010
30.120919	1077.897228	16.791027
29.993431	1086.778487	16.796045
30.303097	1086.155959	16.801063
30.170992	1093.374854	16.806080
29.695835	1094.726952	16.811098
30.369621	1088.171704	16.816115
30.013143	1090.370002	16.821133
30.145788	1092.141857	16.826151
29.936789	1101.038969	16.831168
29.804744	1095.959849	16.836186
29.816458	1088.355829	16.841203
30.127361	1101.495389	16.846221
30.454271	1115.522392	16.851239
30.590940	1115.870373	16.856256
30.835667	1118.012939	16.861274
31.052967	1104.081150	16.866291
30.452793	1099.737625	16.871309
30.477195	1097.521670	16.876327
30.493108	1098.611121	16.881344
30.372810	1112.764554	16.886362
31.004657	1111.261897	16.891379
30.795014	1102.004001	16.896397
30.507831	1102.124487	16.901415
31.145190	1107.756155	16.906432
30.703752	1112.378689	16.911450
30.678025	1112.575231	16.916467
30.632773	1114.434745	16.921485
30.654406	1107.715943	16.926503
30.783190	1109.305366	16.931520
30.624314	1107.468235	16.936538
30.782916	1109.882983	16.941555
30.970731	1108.348475	16.946573
30.882509	1106.847478	16.951591
30.706694	1103.851664	16.956608
30.898766	1121.576131	16.961626
31.154184	1124.982496	16.966643
31.151065	1123.758579	16.971661
31.171174	1134.188453	16.976679
31.315885	1126.784613	16.981696
31.260468	1126.755407	16.986714
31.515239	1125.260965	16.991731
31.133281	1118.810121	16.996749
31.486278	1122.753552	17.001767
31.800681	1122.060859	17.006784
31.630051	1125.571427	17.011802
31.256190	1115.531215	17.016819
31.404035	1113.397024	17.021837
31.364968	1121.043251	17.026855
31.576811	1127.214542	17.031872
31.391211	1127.338146	17.036890
31.681072	1129.158110	17.041907
31.517559	1120.571512	17.046925
31.711537	1125.085650	17.051943
31.893439	1116.792410	17.056960
31.863948	1117.892086	17.061978
31.968362	1123.786616	17.066995
31.849806	1130.182916	17.072013
31.819570	1124.441004	17.077031
31.973797	1122.788650	17.082048
31.955949	1124.104263	17.087066
31.852222	1119.857006	17.092083
31.988553	1124.727253	17.097101
31.833666	1121.106492	17.102119
31.603927	1115.506096	17.107136
31.639519	1124.664936	17.112154
31.735152	1114.580029	17.117171
31.646398	1120.551969	17.122189
31.465613	1113.394471	17.127207
32.113327	1128.659089	17.132224
31.879160	1148.365498	17.137242
32.316858	1134.165844	17.142259
32.636887	1146.152160	17.147277
32.396653	1140.603883	17.152295
32.476204	1144.738215	17.157312
32.280268	1145.876431	17.162330
32.638208	1144.425885	17.167347
32.318692	1149.815233	17.172365
32.377601	1149.941793	17.177383
32.513247	1154.259896	17.182400
32.419761	1147.902981	17.187418
32.890209	1142.338727	17.192435
32.604870	1142.824995	17.197453
32.289509	1150.160806	17.202471
32.521300	1145.277486	17.207488
32.463573	1157.344715	17.212506
32.536851	1151.592989	17.217523
32.499997	1149.900956	17.222541
32.096471	1143.213622	17.227559
32.746869	1144.141174	17.232576
32.609297	1146.267527	17.237594
32.583623	1151.484895	17.242611
32.870545	1165.379309	17.247629
32.641280	1173.998749	17.252647
32.880111	1169.136417	17.257664
33.164568	1178.991834	17.262682
33.144272	1169.392000	17.267699
33.221058	1163.889031	17.272717
33.259114	1169.402591	17.277735
33.370670	1161.868200	17.282752
33.003468	1167.343872	17.287770
33.566736	1159.234229	17.292787
32.880995	1149.542355	17.297805
32.928681	1160.150985	17.302823
33.200909	1161.989477	17.307840
33.267836	1160.180299	17.312858
33.245089	1160.183876	17.317875
33.380772	1165.284607	17.322893
33.393944	1159.251906	17.327911
33.475918	1162.385484	17.332928
33.196285	1159.790829	17.337946
33.303698	1158.833719	17.342963
33.443883	1160.058458	17.347981
33.298842	1157.894123	17.352999
33.530888	1157.630813	17.358016
33.242695	1163.397136	17.363034
33.232620	1161.129738	17.368051
33.492125	1176.237091	17.373069
34.063337	1180.228611	17.378087
34.273153	1174.436684	17.383104
33.823906	1165.181347	17.388122
33.908333	1159.563581	17.393139
33.608771	1151.960661	17.398157
33.724758	1172.953784	17.403175
34.253548	1180.606298	17.408192
34.120452	1179.973808	17.413210
34.493423	1171.754934	17.418227
34.281538	1159.707651	17.423245
33.780560	1154.357755	17.428263
33.950222	1146.833258	17.433280
33.849608	1155.372699	17.438298
34.125332	1165.175820	17.443315
34.530481	1170.578578	17.448333
34.242149	1170.210098	17.453351
34.270972	1171.543693	17.458368
34.274014	1181.070545	17.463386
34.698610	1172.149361	17.468403
34.380372	1160.876022	17.473421
33.947195	1160.927722	17.478439
34.229206	1166.062475	17.483456
33.977665	1179.491632	17.488474
34.124367	1170.033053	17.493491
34.253367	1170.126611	17.498509
34.254788	1178.195744	17.503527
34.207890	1161.553208	17.508544
34.385676	1191.193021	17.513562
34.739683	1194.195889	17.518579
34.922675	1189.711471	17.523597
34.689365	1199.578086	17.528615
35.181678	1195.588302	17.533632
34.509336	1192.199568	17.538650
34.651251	1189.539275	17.543667
34.556124	1189.238543	17.548685
34.623198	1200.809847	17.553703
35.216964	1194.737231	17.558720
35.044226	1191.775636	17.563738
35.240303	1193.168399	17.568755
35.481338	1190.315950	17.573773
35.155709	1189.334743	17.578791
35.373078	1193.649599	17.583808
34.960822	1175.353501	17.588826
35.299992	1181.539700	17.593843
34.978185	1187.443807	17.598861
34.796282	1193.414496	17.603879
35.054869	1188.141987	17.608896
34.964315	1197.923259	17.613914
34.945094	1185.533539	17.618931
35.503871	1189.195640	17.623949
35.070172	1202.675266	17.628967
35.520841	1191.389489	17.633984
35.159255	1195.239068	17.639002
35.137920	1193.058625	17.644019
35.382446	1200.102159	17.649037
35.636093	1217.318522	17.654055
35.886671	1210.122225	17.659072
35.877006	1213.869679	17.664090
36.068069	1209.055799	17.669107
35.762991	1191.967440	17.674125
35.786853	1193.396483	17.679143
35.809876	1180.264893	17.684160
35.754160	1177.625905	17.689178
35.771433	1187.746986	17.694195
35.896592	1189.330670	17.699213
35.719847	1206.986414	17.704231
36.283838	1201.079376	17.709248
36.139173	1209.695129	17.714266
35.810388	1211.179079	17.719283
36.260431	1198.798338	17.724301
36.194516	1211.002577	17.729319
36.396725	1218.507140	17.734336
36.065854	1204.720580	17.739354
36.037942	1216.975711	17.744371
36.343914	1202.395726	17.749389
36.185767	1214.901504	17.754407
36.814117	1203.979373	17.759424
36.342279	1208.915930	17.764442
36.204616	1205.450259	17.769459
36.505736	1199.719847	17.774477
36.213212	1205.379562	17.779495
36.232893	1207.478283	17.784512
36.490490	1206.756562	17.789530
36.618454	1209.567410	17.794547
36.738195	1203.186744	17.799565
36.513025	1209.372456	17.804583
36.388432	1205.406136	17.809600
36.533211	1213.468744	17.814618
36.139687	1206.842945	17.819635
36.537610	1205.982611	17.824653
36.404802	1229.980973	17.829671
36.907372	1230.268831	17.834688
36.854685	1226.698407	17.839706
36.893121	1229.103477	17.844723
36.955442	1242.064095	17.849741
36.732750	1237.740658	17.854759
36.815508	1226.064020	17.859776
36.863134	1227.820723	17.864794
36.728830	1221.056729	17.869811
36.995333	1227.519344	17.874829
36.778702	1232.223671	17.879847
37.097169	1242.862775	17.884864
37.305587	1249.915107	17.889882
37.327977	1249.801203	17.894899
37.655618	1247.648469	17.899917
37.661730	1240.780555	17.904935
37.899738	1223.478223	17.909952
37.795260	1222.434180	17.914970
37.127465	1214.636103	17.919987
37.308026	1209.675535	17.925005
37.203535	1214.854700	17.930023
37.318751	1225.216172	17.935040
37.512582	1238.367749	17.940058
37.688755	1240.902854	17.945075
37.628953	1234.897268	17.950093
37.689669	1245.513388	17.955111
37.685575	1249.016987	17.960128
37.940497	1251.511430	17.965146
37.729194	1240.429674	17.970163
37.921811	1245.114467	17.975181
37.803110	1234.488509	17.980199
37.826882	1237.167261	17.985216
37.778000	1236.881418	17.990234
37.616882	1236.098656	17.995251
37.969918	1234.434273	18.000269
37.934346	1243.635813	18.005287
37.993855	1239.359956	18.010304
38.128056	1235.466944	18.015322
38.217126	1242.787162	18.020339
38.455800	1246.372882	18.025357
38.234496	1248.029448	18.030375
38.365691	1251.003901	18.035392
38.575666	1261.353796	18.040410
38.346150	1250.375854	18.045427
38.424898	1235.184284	18.050445
38.546221	1254.055982	18.055463
38.584312	1265.057488	18.060480
38.755238	1247.749798	18.065498
38.138170	1240.186807	18.070515
38.563409	1252.642806	18.075533
39.051933	1258.386058	18.080551
38.673574	1264.362111	18.085568
38.860972	1256.626525	18.090586
38.485846	1262.119238	18.095603
38.939179	1263.468797	18.100621
38.683971	1266.061602	18.105639
38.730270	1255.517239	18.110656
38.886583	1251.841687	18.115674
38.714011	1255.377829	18.120691
39.094108	1257.278430	18.125709
38.729577	1256.322211	18.130727
38.761195	1253.776911	18.135744
39.115679	1253.705975	18.140762
38.745524	1253.315519	18.145779
38.828863	1264.193214	18.150797
38.820395	1276.656796	18.155815
38.865917	1288.392459	18.160832
39.172735	1281.316766	18.165850
39.042295	1283.271612	18.170867
39.078631	1277.913760	18.175885
39.207671	1290.538978	18.180903
39.212437	1304.736208	18.185920
39.704445	1306.934971	18.190938
39.463544	1299.925612	18.195955
39.518284	1301.343545	18.200973
39.655549	1304.143492	18.205991
39.831699	1303.096778	18.211008
40.073338	1307.379480	18.216026
39.560817	1305.641571	18.221043
39.893682	1298.391402	18.226061
39.912731	1300.045265	18.231079
39.908374	1302.365490	18.236096
39.836173	1297.870285	18.241114
40.001236	1307.031151	18.246131
40.138533	1295.667867	18.251149
39.957050	1299.079174	18.256167
40.036104	1302.288971	18.261184
39.991415	1292.336263	18.266202
39.894241	1300.824745	18.271219
39.602060	1295.319221	18.276237
39.669010	1296.886731	18.281255
39.987309	1301.675047	18.286272
40.185821	1298.207510	18.291290
39.806310	1297.723835	18.296307
40.028560	1313.651302	18.301325
40.144221	1319.067619	18.306343
40.331112	1327.303603	18.311360
40.383985	1324.979046	18.316378
40.408172	1333.663243	18.321395
40.734613	1330.077951	18.326413
40.455829	1324.693408	18.331431
40.519209	1316.311231	18.336448
40.769691	1313.804430	18.341466
40.703028	1320.666089	18.346483
40.595883	1326.448458	18.351501
40.532413	1322.008692	18.356519
40.940271	1313.689647	18.361536
40.698795	1309.321780	18.366554
40.767464	1314.717010	18.371571
40.743521	1315.613864	18.376589
41.165333	1336.004142	18.381607
41.030442	1340.020428	18.386624
41.348104	1336.688966	18.391642
41.273377	1334.466325	18.396659
41.361479	1322.359602	18.401677
41.287918	1321.651567	18.406695
41.152488	1316.916893	18.411712
41.160009	1318.768212	18.416730
41.027612	1338.092912	18.421747
41.217751	1342.614015	18.426765
41.193889	1343.349912	18.431783
41.496281	1343.851976	18.436800
41.593083	1343.401438	18.441818
41.193901	1344.224172	18.446835
41.599581	1338.127143	18.451853
41.626115	1344.469372	18.456871
41.347323	1345.080858	18.461888
41.394007	1346.588412	18.466906
41.344871	1340.827282	18.471923
41.250975	1342.972105	18.476941
41.493775	1366.088503	18.481959
41.620740	1362.786727	18.486976
41.919077	1357.511136	18.491994
41.553210	1360.711320	18.497011
41.722316	1367.346941	18.502029
41.690305	1362.160651	18.507047
41.932947	1362.946574	18.512064
42.426800	1361.683133	18.517082
42.210524	1367.375209	18.522099
42.369921	1361.594228	18.527117
42.220219	1361.686998	18.532135
42.623679	1363.239991	18.537152
42.645477	1359.825201	18.542170
42.554823	1358.476040	18.547187
42.863648	1347.183847	18.552205
42.864128	1353.930924	18.557223
42.277726	1358.288912	18.562240
42.795251	1362.241495	18.567258
42.601204	1353.384983	18.572275
42.639061	1355.241050	18.577293
42.852805	1352.080400	18.582311
42.578542	1345.767339	18.587328
42.974095	1345.188235	18.592346
42.843205	1353.379035	18.597363
42.750303	1348.833391	18.602381
42.843280	1349.197646	18.607399
42.812159	1346.504311	18.612416
43.312880	1349.455961	18.617434
43.165927	1349.819702	18.622451
42.639637	1346.332459	18.627469
42.766425	1351.289462	18.632487
43.104162	1349.475971	18.637504
42.923371	1350.854840	18.642522
42.974989	1349.972679	18.647539
42.892261	1344.948925	18.652557
42.749058	1344.863958	18.657575
42.945617	1353.426653	18.662592
43.068837	1350.564120	18.667610
43.300511	1356.625106	18.672627
43.241629	1363.517128	18.677645
43.463427	1372.025410	18.682663
43.264795	1360.373560	18.687680
43.500602	1363.297030	18.692698
43.316249	1363.893813	18.697715
43.453390	1364.383736	18.702733
43.605991	1361.728066	18.707751
43.221737	1367.297971	18.712768
43.871179	1375.556636	18.717786
43.769795	1384.127864	18.722803
43.941362	1380.503559	18.727821
43.991147	1387.561710	18.732839
43.625308	1389.628957	18.737856
44.124358	1383.962345	18.742874
44.024882	1388.077270	18.747891
44.230016	1385.687973	18.752909
43.970801	1389.442759	18.757927
43.870181	1394.349973	18.762944
43.871173	1385.545130	18.767962
43.713513	1390.442289	18.772979
44.343080	1391.448838	18.777997
44.195676	1387.798454	18.783015
44.513348	1398.343101	18.788032
44.513637	1398.207390	18.793050
44.255207	1400.605056	18.798067
44.505886	1410.535288	18.803085
44.453106	1411.632298	18.808103
44.351905	1410.010219	18.813120
44.538924	1410.949972	18.818138
44.571217	1414.747740	18.823155
44.415238	1414.358647	18.828173
44.315642	1412.089375	18.833191
44.058834	1418.507304	18.838208
44.649678	1417.484380	18.843226
45.314331	1428.445239	18.848243
45.356482	1425.775198	18.853261
45.648431	1418.973165	18.858279
45.421039	1403.090655	18.863296
45.516500	1396.139341	18.868314
45.373947	1393.681099	18.873331
45.427736	1389.955209	18.878349
45.677263	1399.200803	18.883367
45.425970	1399.713335	18.888384
45.563918	1393.676906	18.893402
45.563824	1394.093523	18.898419
45.294496	1394.141802	18.903437
45.271961	1393.930749	18.908455
45.530548	1394.884605	18.913472
45.395476	1396.265826	18.918490
45.452981	1396.430477	18.923507
45.526885	1399.476991	18.928525
45.489378	1387.762166	18.933543
45.383604	1396.993650	18.938560
45.478232	1402.179737	18.943578
45.509083	1395.614026	18.948595
45.213363	1393.750834	18.953613
45.695972	1409.650474	18.958631
45.733617	1421.545242	18.963648
45.751507	1418.257282	18.968666
46.006760	1419.255840	18.973683
45.799796	1411.657326	18.978701
46.172398	1411.056548	18.983719
46.143089	1413.497437	18.988736
46.057485	1417.641767	18.993754
46.217578	1414.962832	18.998771
45.824688	1417.283604	19.003789
46.241230	1418.752514	19.008807
46.225728	1436.951429	19.013824
46.899830	1440.138033	19.018842
46.457051	1428.353736	19.023859
46.308525	1439.122471	19.028877
46.449744	1432.100903	19.033895
46.450120	1437.560452	19.038912
46.715899	1433.533302	19.043930
46.813032	1434.991982	19.048947
46.713094	1441.950388	19.053965
46.892511	1447.202183	19.058983
46.598511	1452.789621	19.064000
47.007889	1444.448188	19.069018
46.763397	1443.104037	19.074035
46.725750	1443.207764	19.079053
46.986128	1439.942006	19.084071
47.083830	1440.475943	19.089088
47.033521	1437.697217	19.094106
47.148682	1434.722316	19.099123
47.249975	1435.552340	19.104141
46.979453	1439.905348	19.109159
47.005943	1446.550580	19.114176
47.181664	1457.057402	19.119194
47.268303	1459.420285	19.124211
47.441732	1456.777137	19.129229
47.664352	1466.001708	19.134247
47.421744	1464.521562	19.139264
47.567482	1455.088229	19.144282
47.756442	1464.116067	19.149299
47.823441	1460.889882	19.154317
47.822264	1455.354779	19.159335
47.778617	1459.123355	19.164352
47.627542	1465.799395	19.169370
47.937124	1460.701905	19.174387
47.862616	1466.368784	19.179405
47.978455	1456.267914	19.184423
47.648362	1466.310692	19.189440
47.416683	1460.918773	19.194458
47.718020	1469.105447	19.199475
47.735967	1485.358369	19.204493
47.870289	1479.742201	19.209511
48.106834	1487.181571	19.214528
48.051788	1479.351091	19.219546
48.273312	1492.691051	19.224563
47.804710	1490.242533	19.229581
48.558998	1492.242693	19.234599
49.004414	1499.217199	19.239616
48.726200	1489.679440	19.244634
48.541520	1486.221034	19.249651
48.488293	1487.355987	19.254669
48.667239	1471.971888	19.259687
48.479985	1481.995592	19.264704
48.774787	1502.399524	19.269722
49.088964	1499.011770	19.274739
48.816848	1496.933451	19.279757
48.959789	1487.541563	19.284775
49.139616	1487.917545	19.289792
49.065693	1483.012303	19.294810
49.066494	1484.842595	19.299827
48.811066	1489.770782	19.304845
49.472060	1496.541308	19.309863
49.135709	1500.077751	19.314880
49.354966	1495.947376	19.319898
49.449855	1495.058471	19.324915
49.241239	1500.370696	19.329933
49.484720	1499.499681	19.334951
49.278729	1495.287191	19.339968
49.285384	1497.375351	19.344986
49.548864	1489.195470	19.350003
49.499743	1497.288396	19.355021
49.247359	1488.860625	19.360039
49.278123	1491.232212	19.365056
49.645890	1497.966340	19.370074
49.660489	1493.138832	19.375091
49.589445	1499.994931	19.380109
49.618689	1507.756922	19.385127
49.884766	1512.758556	19.390144
49.915434	1519.381074	19.395162
49.876747	1510.023764	19.400179
49.533869	1517.638567	19.405197
50.092595	1503.754295	19.410215
49.859488	1519.374143	19.415232
49.901250	1520.260777	19.420250
49.797247	1521.671885	19.425267
49.820779	1527.184661	19.430285
49.716617	1543.014830	19.435303
50.070584	1534.618865	19.440320
50.284496	1541.392744	19.445338
50.702741	1534.776134	19.450355
50.666416	1547.828073	19.455373
50.696910	1535.998421	19.460391
50.192501	1545.967396	19.465408
50.537734	1552.903872	19.470426
50.820919	1560.869349	19.475443
50.758899	1562.924028	19.480461
50.887554	1566.508007	19.485479
51.030117	1563.642428	19.490496
50.668125	1563.758784	19.495514
51.047480	1562.705664	19.500531
50.965917	1564.103813	19.505549
50.770924	1553.704140	19.510567
51.156640	1566.851332	19.515584
51.024975	1563.760202	19.520602
51.475913	1553.720714	19.525619
51.199911	1561.972072	19.530637
51.419522	1557.993108	19.535655
51.201764	1561.287034	19.540672
51.283227	1578.278087	19.545690
51.313710	1575.016540	19.550707
51.100216	1587.515417	19.555725
51.260185	1579.537805	19.560743
51.717226	1588.274656	19.565760
51.534474	1578.176024	19.570778
51.537383	1575.792941	19.575795
51.710948	1586.132915	19.580813
51.894944	1583.945701	19.585831
52.149435	1584.562529	19.590848
51.911482	1571.837362	19.595866
52.683230	1577.836428	19.600883
51.999016	1579.479888	19.605901
51.952037	1580.509732	19.610919
52.285930	1580.647132	19.615936
52.018022	1580.613138	19.620954
52.402220	1580.133627	19.625971
52.299576	1580.320058	19.630989
52.233778	1587.793921	19.636007
52.644237	1593.337995	19.641024
52.294816	1592.022793	19.646042
52.745195	1595.925922	19.651059
52.441515	1608.678700	19.656077
52.512417	1601.068401	19.661095
52.775473	1596.950119	19.666112
52.558559	1599.407620	19.671130
52.811185	1595.208909	19.676147
52.627320	1599.513749	19.681165
52.594080	1594.431726	19.686183
52.834287	1596.483535	19.691200
52.967196	1599.681845	19.696218
52.954045	1589.036086	19.701235
52.966346	1587.096514	19.706253
53.090856	1589.358842	19.711271
53.024668	1601.885287	19.716288
52.929512	1608.675753	19.721306
53.116696	1613.787530	19.726323
53.417256	1618.632344	19.731341
53.101727	1618.542647	19.736359
53.442451	1615.706169	19.741376
53.128874	1626.667974	19.746394
53.694926	1613.962767	19.751411
53.882957	1617.812072	19.756429
53.616712	1622.139211	19.761447
53.470420	1612.615560	19.766464
53.452344	1623.357784	19.771482
53.978125	1626.883101	19.776499
53.973294	1639.551502	19.781517
54.315880	1636.197169	19.786535
54.441560	1639.112584	19.791552
54.092177	1636.219444	19.796570
54.444373	1628.603208	19.801587
54.000169	1610.447337	19.806605
54.038195	1625.857804	19.811623
54.233150	1628.677224	19.816640
54.166533	1631.591019	19.821658
54.672858	1626.813150	19.826675
54.630917	1641.481831	19.831693
54.672791	1640.651666	19.836711
54.359256	1637.424735	19.841728
54.174621	1637.283100	19.846746
54.281848	1628.389011	19.851763
54.355209	1639.366321	19.856781
54.256543	1629.885741	19.861799
54.555241	1639.527754	19.866816
54.558677	1663.224614	19.871834
55.073282	1660.048626	19.876851
54.872682	1658.290519	19.881869
54.990900	1664.167299	19.886887
55.319260	1665.337529	19.891904
54.733194	1667.451719	19.896922
55.083266	1658.958471	19.901939
54.944363	1665.424404	19.906957
55.072817	1665.997741	19.911975
54.981747	1661.622149	19.916992
54.879531	1676.975598	19.922010
55.240940	1680.207775	19.927027
55.423449	1679.077997	19.932045
55.220718	1677.948237	19.937063
55.445938	1675.581021	19.942080
55.402911	1680.668698	19.947098
55.100114	1674.552471	19.952115
55.587773	1690.659863	19.957133
55.583596	1693.046385	19.962151
55.980252	1699.716130	19.967168
55.908936	1706.471363	19.972186
55.959263	1701.553027	19.977203
56.204543	1698.595694	19.982221
55.763815	1705.742963	19.987239
56.072593	1697.792625	19.992256
55.872668	1695.750380	19.997274
55.696437	1694.395582	20.002291
55.997702	1715.145898	20.007309
56.713835	1716.814347	20.012327
56.511011	1718.004165	20.017344
56.372851	1724.690915	20.022362
56.750034	1715.398139	20.027379
56.490323	1717.332132	20.032397
56.871365	1720.406623	20.037415
56.763416	1705.985350	20.042432
56.760402	1719.934807	20.047450
56.840174	1716.381532	20.052467
56.874700	1712.513404	20.057485
56.837055	1713.462905	20.062503
57.289378	1714.995698	20.067520
57.090875	1715.875568	20.072538
57.094229	1717.730734	20.077555
56.870181	1704.959124	20.082573
56.783272	1712.344804	20.087591
56.971752	1721.069884	20.092608
57.180494	1736.065694	20.097626
57.568612	1735.244735	20.102643
57.406278	1737.289804	20.107661
57.261894	1737.833038	20.112679
57.427687	1723.773083	20.117696
57.521172	1731.042321	20.122714
57.806969	1736.369158	20.127731
58.050834	1739.023187	20.132749
57.685365	1734.314750	20.137767
57.985984	1732.005217	20.142784
57.720473	1733.570878	20.147802
57.654198	1727.250545	20.152819
57.924632	1742.148391	20.157837
58.083664	1753.790946	20.162855
58.451696	1750.628296	20.167872
58.290838	1755.914225	20.172890
58.470565	1755.438142	20.177907
58.460139	1758.144389	20.182925
58.281595	1751.368145	20.187943
58.700256	1733.696358	20.192960
58.558632	1751.795307	20.197978
58.328818	1743.288160	20.202995
58.815078	1754.090799	20.208013
58.344213	1745.861028	20.213031
58.601156	1749.283057	20.218048
58.543096	1747.259745	20.223066
58.341876	1748.228404	20.228083
58.671462	1739.268082	20.233101
58.630484	1752.437663	20.238119
59.338534	1755.120411	20.243136
59.237147	1772.443082	20.248154
59.098374	1768.172723	20.253171
59.421570	1765.370509	20.258189
58.892802	1771.663644	20.263207
59.666029	1765.146320	20.268224
59.604087	1767.895303	20.273242
59.353861	1764.525944	20.278259
59.747806	1768.728240	20.283277
59.362785	1767.219746	20.288295
59.812972	1759.149532	20.293312
59.852812	1764.098096	20.298330
59.785877	1759.737657	20.303347
59.669516	1763.205185	20.308365
59.418510	1767.167060	20.313383
59.824757	1764.926286	20.318400
59.646921	1765.064465	20.323418
59.640220	1759.678454	20.328435
59.423421	1758.471982	20.333453
59.490256	1760.497153	20.338471
59.808675	1778.789598	20.343488
59.992873	1791.169892	20.348506
60.141818	1792.860383	20.353523
60.374855	1795.168958	20.358541
60.307959	1792.440099	20.363559
60.290503	1797.239798	20.368576
60.006596	1797.343997	20.373594
60.286611	1806.761786	20.378611
60.504538	1810.660128	20.383629
60.503831	1817.003611	20.388647
60.562400	1811.629514	20.393664
60.971895	1812.086514	20.398682
60.875162	1805.142874	20.403699
61.155857	1807.008519	20.408717
61.198096	1809.936953	20.413735
61.494513	1814.760375	20.418752
60.918038	1810.261500	20.423770
61.166949	1803.686935	20.428787
61.412678	1807.962810	20.433805
60.848445	1807.185979	20.438823
61.107513	1820.466689	20.443840
61.279133	1830.655625	20.448858
61.470111	1834.394061	20.453875
61.479573	1825.742321	20.458893
61.298422	1832.293789	20.463911
61.653084	1831.096172	20.468928
61.967242	1828.642503	20.473946
61.915497	1830.439985	20.478963
61.850433	1831.737754	20.483981
61.732836	1826.135453	20.488999
61.747212	1828.594845	20.494016
61.942231	1839.423945	20.499034
62.001281	1853.815137	20.504051
62.223144	1856.895499	20.509069
62.068410	1854.843045	20.514087
62.061853	1855.364823	20.519104
62.577306	1860.362444	20.524122
62.164947	1860.101622	20.529139
62.396224	1853.327808	20.534157
62.522860	1868.017766	20.539175
62.474941	1849.982994	20.544192
62.329122	1860.653728	20.549210
62.570809	1862.336098	20.554227
62.839596	1883.107446	20.559245
62.958811	1883.366638	20.564263
62.591122	1888.419713	20.569280
62.530975	1878.601633	20.574298
62.817464	1887.472486	20.579315
63.077422	1873.766993	20.584333
62.658571	1885.417554	20.589351
62.976813	1891.039197	20.594368
63.407974	1902.661573	20.599386
63.225118	1904.927614	20.604403
63.928870	1905.130513	20.609421
63.441398	1910.644070	20.614439
63.704061	1906.273306	20.619456
63.805000	1907.829266	20.624474
63.626626	1905.830981	20.629491
63.682995	1896.954145	20.634509
63.746088	1906.039675	20.639527
63.920592	1897.217032	20.644544
63.831326	1903.968822	20.649562
64.058837	1897.040938	20.654579
64.114727	1890.190271	20.659597
63.786953	1900.239242	20.664615
63.857506	1895.472344	20.669632
64.363650	1898.372749	20.674650
63.934873	1891.408187	20.679667
64.136010	1892.569837	20.684685
64.287957	1903.008038	20.689703
64.269451	1917.171507	20.694720
64.310195	1917.963643	20.699738
64.188214	1927.964809	20.704755
64.356852	1922.756584	20.709773
64.138080	1922.920072	20.714791
64.064502	1931.414648	20.719808
64.484355	1937.026798	20.724826
64.474821	1937.306037	20.729843
65.131186	1942.761440	20.734861
64.902758	1945.782533	20.739879
65.169259	1936.516343	20.744896
65.192737	1943.635616	20.749914
65.355963	1941.347448	20.754931
65.681376	1935.199596	20.759949
65.310979	1934.976423	20.764967
65.527478	1941.525981	20.769984
65.798257	1943.579383	20.775002
65.714273	1936.987169	20.780019
65.816084	1926.544224	20.785037
65.769305	1936.997606	20.790055
65.711770	1936.053512	20.795072
65.987905	1949.189645	20.800090
65.555917	1955.906449	20.805107
65.890029	1958.858895	20.810125
65.943439	1957.824941	20.815143
66.147459	1957.281953	20.820160
65.907074	1952.591854	20.825178
66.244064	1958.548282	20.830195
66.366672	1951.598839	20.835213
66.037307	1967.814753	20.840231
66.082698	1956.749391	20.845248
66.521370	1974.303764	20.850266
66.290067	1986.064051	20.855283
66.560055	1982.648371	20.860301
66.965708	1989.746031	20.865319
66.428811	1977.212290	20.870336
66.535320	1973.187726	20.875354
66.809979	1984.364289	20.880371
66.678049	1978.148767	20.885389
66.841518	1977.085053	20.890407
67.072195	1990.540730	20.895424
67.089950	1983.250980	20.900442
67.284327	2000.287973	20.905459
67.499434	1989.754765	20.910477
67.413853	2001.101039	20.915495
67.087555	1997.929679	20.920512
67.239715	1989.997284	20.925530
67.437794	1986.810558	20.930547
67.328922	1986.401494	20.935565
67.472141	1987.805706	20.940583
67.480017	2000.914212	20.945600
67.810187	2008.979877	20.950618
67.671500	2017.345769	20.955635
67.785643	2016.217147	20.960653
68.021153	2024.281776	20.965671
67.870173	2020.480334	20.970688
67.851542	2017.371526	20.975706
68.080520	2032.089869	20.980723
68.240492	2022.852844	20.985741
67.693848	2015.490003	20.990759
68.320285	2026.974754	20.995776
68.597101	2041.748775	21.000794
68.489993	2044.650006	21.005811
68.782319	2039.728615	21.010829
69.018138	2045.681890	21.015847
68.908888	2040.472713	21.020864
69.143430	2044.494757	21.025882
68.830433	2041.425464	21.030899
68.802869	2036.736923	21.035917
68.984452	2044.109341	21.040935
68.478276	2036.576081	21.045952
69.019753	2034.863352	21.050970
69.092258	2042.009746	21.055987
69.141433	2035.343113	21.061005
69.361887	2045.745484	21.066023
69.447188	2050.803819	21.071040
69.879287	2050.323151	21.076058
69.538914	2061.191560	21.081075
69.741503	2056.041129	21.086093
69.691097	2057.077845	21.091111
69.628227	2057.188658	21.096128
69.834361	2054.777026	21.101146
69.823091	2053.399673	21.106163
69.780330	2057.736304	21.111181
69.570645	2061.297318	21.116199
69.258744	2058.171045	21.121216
69.651847	2068.158369	21.126234
69.725443	2082.310785	21.131251
70.042679	2079.070775	21.136269
70.453093	2087.774105	21.141287
70.485572	2102.321119	21.146304
70.434164	2100.659665	21.151322
70.415457	2110.310324	21.156339
70.231251	2099.877093	21.161357
70.771230	2099.247079	21.166375
70.758564	2092.328110	21.171392
71.140324	2090.390923	21.176410
70.745879	2091.017283	21.181427
70.943214	2095.521678	21.186445
70.963978	2092.899050	21.191463
71.360466	2110.011982	21.196480
71.548555	2108.010269	21.201498
71.600238	2125.817556	21.206515
71.621373	2105.786686	21.211533
71.816965	2090.913882	21.216551
71.372544	2090.203593	21.221568
71.949046	2089.186024	21.226586
71.777419	2092.270884	21.231603
71.952975	2094.392780	21.236621
71.924803	2108.655740	21.241639
71.732989	2102.111813	21.246656
72.073599	2103.201267	21.251674
71.749882	2110.665009	21.256691
72.057601	2107.233964	21.261709
72.200232	2111.529120	21.266727
72.002819	2113.402961	21.271744
72.483390	2108.515361	21.276762
72.267363	2109.154971	21.281779
72.388286	2109.215077	21.286797
72.318237	2104.236474	21.291815
72.424923	2107.981780	21.296832
72.404754	2101.111315	21.301850
72.369980	2129.646488	21.306867
72.828300	2136.783346	21.311885
72.779084	2132.019252	21.316903
72.469922	2143.277344	21.321920
72.806986	2134.795366	21.326938
72.657370	2132.530633	21.331955
72.912855	2143.823896	21.336973
73.342732	2149.084242	21.341991
73.172494	2161.352712	21.347008
73.699660	2143.414307	21.352026
73.528565	2156.541325	21.357043
73.625357	2146.316793	21.362061
73.894092	2160.599843	21.367079
73.767569	2159.587581	21.372096
73.671296	2146.581156	21.377114
73.628891	2153.196350	21.382131
73.735952	2147.647337	21.387149
73.520357	2155.753856	21.392167
73.501957	2155.813563	21.397184
73.783625	2169.659085	21.402202
74.008360	2173.647969	21.407219
74.429482	2182.961933	21.412237
74.417542	2173.306607	21.417255
74.101374	2179.554160	21.422272
74.561824	2180.303054	21.427290
74.146881	2178.745532	21.432307
74.269737	2179.644821	21.437325
74.573869	2189.592414	21.442343
74.475906	2208.385649	21.447360
74.756859	2199.517881	21.452378
74.800280	2209.919507	21.457395
74.935595	2210.472858	21.462413
74.950456	2202.135691	21.467431
74.819421	2196.469091	21.472448
75.269594	2194.268765	21.477466
75.183594	2216.702121	21.482483
75.440770	2210.088250	21.487501
75.366585	2220.429293	21.492519
75.638991	2217.761156	21.497536
75.949692	2214.361186	21.502554
76.070704	2223.223254	21.507571
75.780003	2222.337540	21.512589
75.924605	2216.713230	21.517607
75.743530	2217.745052	21.522624
75.879455	2211.951672	21.527642
75.890847	2217.816863	21.532659
76.048747	2220.427541	21.537677
76.154933	2214.282167	21.542695
76.094942	2220.167941	21.547712
76.495149	2223.454141	21.552730
76.506873	2236.562222	21.557747
76.452810	2244.697283	21.562765
76.857669	2241.244777	21.567783
76.832797	2249.334268	21.572800
76.832508	2240.737497	21.577818
76.457402	2243.263898	21.582835
76.616763	2241.459156	21.587853
76.919461	2239.111364	21.592871
76.641862	2246.208201	21.597888
76.470682	2239.200240	21.602906
77.060593	2257.125842	21.607923
77.007918	2261.842782	21.612941
76.891989	2276.179502	21.617959
77.010125	2265.149963	21.622976
77.535242	2272.058714	21.627994
77.146614	2283.461817	21.633011
77.338435	2293.666808	21.638029
77.559442	2288.879536	21.643047
77.557779	2295.210714	21.648064
78.212565	2285.110677	21.653082
77.969549	2290.778804	21.658099
77.630310	2298.068306	21.663117
78.042403	2290.410905	21.668135
77.843158	2293.159254	21.673152
78.272007	2293.445989	21.678170
78.531261	2307.686449	21.683187
78.457732	2311.160038	21.688205
78.916911	2309.128720	21.693223
78.574391	2309.513460	21.698240
78.685454	2315.410505	21.703258
78.894872	2307.093493	21.708275
78.989271	2306.359268	21.713293
79.286424	2300.149416	21.718311
79.034726	2297.323013	21.723328
79.268412	2294.746104	21.728346
79.006877	2297.702978	21.733363
78.868937	2299.857928	21.738381
79.500452	2291.219573	21.743399
79.107464	2295.522422	21.748416
79.386431	2294.914104	21.753434
79.458182	2294.599993	21.758451
79.135311	2300.346832	21.763469
79.571768	2300.597666	21.768487
79.601455	2311.970375	21.773504
79.590429	2309.033911	21.778522
79.814786	2313.152281	21.783539
79.955958	2317.599201	21.788557
79.963840	2315.953743	21.793575
79.918336	2321.499605	21.798592
79.547547	2320.721034	21.803610
79.868088	2327.358684	21.808627
79.885896	2333.854110	21.813645
80.073094	2336.428684	21.818663
79.892909	2346.142483	21.823680
80.449656	2352.632907	21.828698
80.847105	2362.521884	21.833715
80.921815	2363.343467	21.838733
80.953133	2354.359846	21.843751
80.833346	2357.174733	21.848768
80.643038	2364.482102	21.853786
80.779262	2360.449668	21.858803
80.706407	2381.375778	21.863821
81.171395	2383.765089	21.868839
81.284210	2397.274138	21.873856
81.374194	2394.047363	21.878874
81.144858	2385.382035	21.883891
81.219579	2385.114801	21.888909
81.591771	2388.250750	21.893927
82.059951	2400.502041	21.898944
82.006508	2401.835914	21.903962
82.492008	2403.808599	21.908979
82.132826	2399.253649	21.913997
82.025431	2399.081045	21.919015
82.613446	2403.950751	21.924032
82.349282	2389.717359	21.929050
82.350586	2397.383095	21.934067
82.277236	2396.861187	21.939085
82.575984	2390.676304	21.944103
82.240888	2396.500820	21.949120
82.402476	2399.013114	21.954138
82.416315	2390.155280	21.959155
82.755002	2403.891115	21.964173
83.073792	2405.066042	21.969191
83.252589	2419.319117	21.974208
83.135038	2416.591737	21.979226
82.968316	2414.973455	21.984243
82.901635	2420.131301	21.989261
83.131639	2417.450800	21.994279
82.788774	2421.928924	21.999296
83.013237	2423.276337	22.004314
83.496910	2419.079335	22.009331
83.257760	2428.114352	22.014349
83.462015	2429.490161	22.019367
83.862297	2442.061340	22.024384
83.783573	2445.876612	22.029402
83.561144	2450.957724	22.034419
83.692651	2442.472888	22.039437
84.271449	2436.938707	22.044455
84.044691	2438.283786	22.049472
84.017597	2445.259644	22.054490
84.693403	2455.989015	22.059507
84.515954	2471.761983	22.064525
84.673706	2475.111227	22.069543
84.592902	2462.143193	22.074560
84.816477	2462.278842	22.079578
84.755110	2465.996736	22.084595
84.747534	2470.479477	22.089613
84.900549	2465.567037	22.094631
84.777126	2458.551554	22.099648
84.652116	2466.893435	22.104666
84.882705	2478.004581	22.109683
85.083519	2481.779494	22.114701
85.122859	2477.055173	22.119719
84.950033	2490.419405	22.124736
85.261234	2483.058516	22.129754
85.365712	2498.715025	22.134771
85.490321	2514.712419	22.139789
85.387088	2503.433158	22.144807
86.067843	2502.140544	22.149824
85.643155	2506.988057	22.154842
85.891412	2508.622125	22.159859
86.220326	2525.461936	22.164877
86.488616	2514.386773	22.169895
86.570421	2525.170796	22.174912
86.838429	2517.867114	22.179930
86.656556	2520.044710	22.184947
86.540465	2528.924910	22.189965
86.223567	2514.794309	22.194983
86.667606	2526.626540	22.200000
86.576264	2522.121382	22.205018
86.873414	2517.224359	22.210035
86.651850	2531.041207	22.215053
86.908951	2537.644628	22.220071
87.040739	2542.919942	22.225088
87.328064	2541.218332	22.230106
87.425676	2539.195942	22.235123
87.278015	2540.478217	22.240141
87.385490	2539.246451	22.245159
87.559145	2546.055384	22.250176
87.488180	2566.189255	22.255194
87.713539	2557.636100	22.260211
87.951891	2567.546805	22.265229
88.035135	2561.136623	22.270247
87.995375	2556.686546	22.275264
88.161173	2564.891670	22.280282
88.224808	2556.669830	22.285299
88.321600	2567.186438	22.290317
88.447749	2559.166317	22.295335
88.379225	2553.688700	22.300352
88.425719	2568.849335	22.305370
88.622155	2578.608771	22.310387
88.566879	2588.094956	22.315405
88.565664	2589.897271	22.320423
88.925631	2590.586083	22.325440
88.737741	2592.613136	22.330458
89.018604	2576.915555	22.335475
88.907598	2582.673681	22.340493
89.344519	2594.649086	22.345511
89.213887	2611.450065	22.350528
89.324073	2614.841457	22.355546
89.410380	2614.487203	22.360563
89.467023	2623.242718	22.365581
89.585400	2614.097079	22.370599
89.790371	2614.696407	22.375616
89.682591	2607.163997	22.380634
89.990092	2602.303212	22.385651
89.876398	2608.307935	22.390669
90.219281	2619.449026	22.395687
90.025913	2629.010385	22.400704
90.280392	2641.506568	22.405722
90.439505	2621.201156	22.410739
90.363746	2631.687859	22.415757
90.502455	2632.957116	22.420775
90.826554	2628.242072	22.425792
90.549757	2635.405215	22.430810
90.979766	2635.780144	22.435827
91.259264	2639.700643	22.440845
91.067970	2636.350347	22.445863
91.469079	2644.522028	22.450880
91.228855	2645.641984	22.455898
91.245795	2639.557700	22.460915
91.472789	2648.898976	22.465933
91.135063	2648.200456	22.470951
91.558346	2637.454563	22.475968
91.485227	2646.508023	22.480986
91.826906	2644.460246	22.486003
91.862123	2663.798153	22.491021
91.792600	2661.385174	22.496039
92.116454	2663.575574	22.501056
92.041239	2669.126169	22.506074
92.359438	2657.838006	22.511091
92.361109	2664.768442	22.516109
92.420883	2664.484595	22.521127
92.304865	2663.593753	22.526144
92.378838	2669.531406	22.531162
92.855469	2686.304185	22.536179
92.863471	2685.059492	22.541197
92.751969	2691.379506	22.546215
92.829800	2685.326755	22.551232
92.735632	2691.170664	22.556250
92.923091	2683.633284	22.561267
93.285751	2686.218463	22.566285
93.422623	2703.347136	22.571303
93.503899	2708.355787	22.576320
93.397022	2709.698002	22.581338
93.064072	2711.621410	22.586355
93.359168	2711.278832	22.591373
93.437457	2722.050896	22.596391
93.925694	2729.719864	22.601408
94.013971	2730.987511	22.606426
93.879711	2727.255904	22.611443
94.353849	2740.901476	22.616461
93.785590	2737.934925	22.621479
94.026791	2734.043866	22.626496
94.233460	2737.881044	22.631514
94.306612	2745.677765	22.636531
94.422048	2755.456221	22.641549
94.455197	2748.157451	22.646567
94.778993	2746.412272	22.651584
94.842469	2771.849706	22.656602
95.661650	2767.963334	22.661619
95.075923	2762.525149	22.666637
95.186367	2769.896319	22.671655
95.409160	2776.322119	22.676672
95.299472	2787.773637	22.681690
95.579115	2777.097366	22.686707
95.492230	2771.792968	22.691725
95.935676	2780.365252	22.696743
95.856500	2774.602024	22.701760
95.529780	2763.628816	22.706778
95.493133	2768.122470	22.711795
95.669054	2771.910789	22.716813
95.869693	2786.315403	22.721831
96.148736	2790.520051	22.726848
95.993746	2797.042549	22.731866
96.091920	2790.699393	22.736883
96.294485	2801.467937	22.741901
96.363897	2815.463781	22.746919
96.535763	2811.119559	22.751936
96.576049	2820.748791	22.756954
96.847986	2822.925202	22.761971
96.904828	2816.326519	22.766989
97.049036	2820.498514	22.772007
97.173370	2835.139128	22.777024
97.243777	2842.229359	22.782042
97.423608	2833.070884	22.787059
97.528464	2833.240802	22.792077
97.600101	2831.673741	22.797095
98.153820	2834.705762	22.802112
98.026712	2832.267008	22.807130
97.839401	2830.554055	22.812147
98.207258	2836.013626	22.817165
97.988855	2826.172324	22.822183
97.885561	2833.381122	22.827200
98.072843	2844.799065	22.832218
98.647676	2854.332466	22.837235
98.598003	2850.041663	22.842253
98.493384	2855.410686	22.847271
98.530615	2852.558146	22.852288
98.490553	2859.820230	22.857306
98.770601	2852.618689	22.862323
99.019964	2859.557977	22.867341
99.320172	2873.372754	22.872359
99.583485	2875.493705	22.877376
99.351531	2877.363533	22.882394
99.991742	2868.780359	22.887411
100.218019	2865.472314	22.892429
99.667478	2858.235970	22.897447
99.561513	2841.932453	22.902464
99.552743	2857.777335	22.907482
99.762388	2856.318185	22.912499
100.027343	2857.078610	22.917517
99.405728	2858.848144	22.922535
99.645428	2864.810557	22.927552
100.004177	2883.366120	22.932570
100.166085	2878.215476	22.937587
100.545075	2882.789627	22.942605
100.495329	2881.850583	22.947623
100.517146	2879.050936	22.952640
100.692682	2898.364093	22.957658
100.984553	2902.787697	22.962675
101.233117	2910.260507	22.967693
101.158911	2920.197978	22.972711
101.040027	2913.702365	22.977728
101.327581	2917.782631	22.982746
101.356941	2913.788804	22.987763
101.314194	2915.307258	22.992781
101.265134	2912.139911	22.997799
101.484270	2912.645518	23.002816
101.568173	2932.496888	23.007834
101.482562	2927.630942	23.012851
101.660602	2940.016147	23.017869
101.674638	2938.031973	23.022887
101.746425	2930.610338	23.027904
102.045512	2948.815464	23.032922
102.160307	2959.673514	23.037939
102.215943	2962.754701	23.042957
102.145237	2956.715516	23.047975
102.496365	2941.581086	23.052992
102.768412	2961.078118	23.058010
102.987107	2971.017356	23.063027
103.215248	2971.256451	23.068045
102.942215	2980.044532	23.073063
103.114856	2973.737060	23.078080
103.072825	2977.669819	23.083098
103.325715	2977.138130	23.088115
103.738475	2969.966377	23.093133
103.274244	2973.248436	23.098151
103.332275	2978.380713	23.103168
103.387427	2994.398818	23.108186
103.144865	2989.052315	23.113203
103.566488	2998.562306	23.118221
103.589553	3007.159120	23.123239
104.162422	3014.673009	23.128256
104.350799	3017.073913	23.133274
104.177191	3014.443539	23.138291
104.135025	3022.277271	23.143309
104.330056	3037.872811	23.148327
104.790366	3029.001960	23.153344
105.030866	3034.235244	23.158362
105.328122	3034.312086	23.163379
105.538263	3035.718587	23.168397
105.374634	3031.508605	23.173415
105.427031	3027.605850	23.178432
105.530541	3024.705090	23.183450
105.347689	3033.507561	23.188467
105.304020	3027.890217	23.193485
105.239207	3032.505098	23.198503
105.656034	3046.488062	23.203520
105.790677	3050.140842	23.208538
105.722036	3047.876010	23.213555
105.814591	3050.856780	23.218573
106.094628	3059.085375	23.223591
106.460483	3075.635902	23.228608
106.376026	3075.295601	23.233626
106.323111	3076.414825	23.238643
106.575498	3073.478254	23.243661
106.659104	3080.680145	23.248679
106.720802	3073.136933	23.253696
106.701081	3080.534809	23.258714
107.162520	3088.653115	23.263731
107.456688	3090.210656	23.268749
107.644071	3093.965698	23.273767
107.748954	3091.528663	23.278784
107.521933	3094.625475	23.283802
107.751849	3097.521744	23.288819
107.884282	3086.789306	23.293837
107.591450	3091.351332	23.298855
107.664099	3079.432038	23.303872
107.853428	3088.911966	23.308890
107.728292	3108.590929	23.313907
108.262291	3104.316500	23.318925
108.202365	3115.397527	23.323943
108.526510	3101.245560	23.328960
108.461359	3109.524765	23.333978
108.180870	3118.465568	23.338995
108.620961	3131.242494	23.344013
108.469925	3140.952184	23.349031
108.695885	3143.855389	23.354048
108.797715	3143.037914	23.359066
108.813667	3151.115144	23.364083
108.851988	3150.787287	23.369101
109.193935	3161.303949	23.374119
109.170357	3169.576709	23.379136
109.478216	3166.842947	23.384154
109.085791	3177.802192	23.389171
109.430378	3188.384738	23.394189
109.643327	3187.818231	23.399207
109.949505	3183.102678	23.404224
110.214155	3187.281256	23.409242
110.024328	3185.019494	23.414259
110.418477	3201.420550	23.419277
110.391502	3214.134540	23.424295
110.537017	3202.888702	23.429312
110.725093	3207.615749	23.434330
110.196529	3215.140245	23.439347
110.601881	3211.274025	23.444365
110.886518	3225.492327	23.449383
110.851925	3230.361357	23.454400
111.297340	3233.785890	23.459418
111.218112	3228.754749	23.464435
111.394413	3233.521510	23.469453
111.754744	3248.958940	23.474471
111.787310	3250.311045	23.479488
111.873192	3240.996559	23.484506
111.896627	3251.846917	23.489523
112.242385	3250.050929	23.494541
111.975921	3260.211045	23.499559
112.239725	3251.768353	23.504576
112.250923	3252.041229	23.509594
112.439824	3264.525963	23.514611
112.779834	3271.877379	23.519629
112.472989	3271.748442	23.524647
112.771416	3274.637230	23.529664
113.166940	3274.619871	23.534682
112.621815	3274.859428	23.539699
113.397849	3279.406582	23.544717
113.481050	3294.050819	23.549735
113.021558	3295.501630	23.554752
113.543154	3303.667479	23.559770
113.566695	3301.482947	23.564787
113.885637	3287.069685	23.569805
113.785568	3288.451912	23.574823
113.803135	3280.262162	23.579840
114.286760	3295.765653	23.584858
114.546358	3299.588399	23.589875
114.458294	3305.598832	23.594893
114.610070	3307.058628	23.599911
114.559216	3301.060423	23.604928
114.836789	3305.694658	23.609946
114.710120	3307.270397	23.614963
114.820986	3296.721093	23.619981
114.810676	3295.340338	23.624999
114.911201	3305.045668	23.630016
115.050833	3317.115186	23.635034
115.107215	3314.224873	23.640051
115.170661	3313.877321	23.645069
115.286056	3339.796679	23.650087
115.458552	3344.914396	23.655104
115.440472	3349.455803	23.660122
115.477072	3342.528682	23.665139
115.688651	3347.921213	23.670157
115.595904	3362.015321	23.675175
116.184264	3379.228998	23.680192
116.429084	3365.376386	23.685210
116.123855	3366.064643	23.690227
115.943337	3372.742819	23.695245
116.451868	3385.253622	23.700263
116.649218	3394.527311	23.705280
116.843542	3394.250910	23.710298
117.044166	3398.900306	23.715315
117.489496	3387.563488	23.720333
117.394289	3385.630991	23.725351
117.239092	3384.411658	23.730368
117.756279	3393.512461	23.735386
117.850530	3406.150902	23.740403
117.676880	3401.440561	23.745421
117.998957	3419.456372	23.750439
117.788226	3411.324200	23.755456
118.068334	3409.188083	23.760474
118.023452	3416.463767	23.765491
118.305225	3414.204299	23.770509
118.180994	3410.685607	23.775527
118.238170	3421.385630	23.780544
118.901622	3423.725248	23.785562
118.490844	3432.241471	23.790579
118.860697	3436.567849	23.795597
119.085890	3440.815753	23.800615
118.974023	3455.316901	23.805632
119.239098	3455.250416	23.810650
119.065912	3468.419746	23.815667
119.760156	3449.794390	23.820685
119.917375	3449.994035	23.825703
120.087268	3448.784052	23.830720
120.293899	3443.777781	23.835738
119.859617	3448.210422	23.840755
119.569294	3448.571275	23.845773
120.025057	3464.899856	23.850791
120.372206	3470.397564	23.855808
120.613559	3464.770426	23.860826
120.211590	3477.460925	23.865843
120.196323	3486.209119	23.870861
120.643438	3490.981129	23.875879
120.806060	3497.902608	23.880896
121.052750	3502.336551	23.885914
120.510130	3505.214292	23.890931
121.059929	3520.496210	23.895949
121.240670	3516.402932	23.900967
121.139731	3522.510128	23.905984
121.406981	3532.205403	23.911002
121.515991	3548.887885	23.916019
121.866189	3551.926468	23.921037
122.061697	3542.238108	23.926055
122.224183	3547.512095	23.931072
122.576218	3553.078504	23.936090
122.315765	3565.507161	23.941107
122.449781	3576.422558	23.946125
122.843757	3561.801711	23.951143
122.912762	3570.647293	23.956160
123.232999	3550.681867	23.961178
122.831178	3561.140971	23.966195
122.874827	3560.638687	23.971213
122.809390	3567.128583	23.976231
123.449555	3585.297033	23.981248
123.673570	3591.912307	23.986266
123.372898	3590.731391	23.991283
123.478616	3595.616549	23.996301
123.849739	3599.560868	24.001319
123.921658	3605.571743	24.006336
123.666662	3619.694469	24.011354
123.614420	3620.314942	24.016371
123.923060	3631.667148	24.021389
124.200070	3633.180066	24.026407
124.139549	3636.891757	24.031424
124.364844	3641.591031	24.036442
124.373171	3655.088889	24.041459
124.854616	3655.130746	24.046477
125.272838	3651.663269	24.051495
124.874758	3651.425441	24.056512
125.110505	3655.526567	24.061530
125.331332	3673.438460	24.066547
125.398200	3676.085618	24.071565
125.394070	3676.237794	24.076583
125.445906	3678.385454	24.081600
125.703818	3682.830320	24.086618
125.581760	3693.552097	24.091635
126.113389	3700.744450	24.096653
126.315196	3700.697284	24.101671
126.591300	3705.953628	24.106688
126.913627	3716.874511	24.111706
126.661153	3725.517723	24.116723
126.703390	3721.212402	24.121741
127.105669	3714.584858	24.126759
126.977351	3723.716891	24.131776
127.366117	3717.397604	24.136794
127.280129	3731.857071	24.141811
127.422689	3734.883825	24.146829
127.460425	3746.420312	24.151847
127.114776	3741.774536	24.156864
127.975309	3742.028809	24.161882
128.068586	3747.007475	24.166899
128.492415	3759.699008	24.171917
128.273094	3762.523297	24.176935
128.241660	3772.183143	24.181952
128.440336	3765.363187	24.186970
128.255198	3766.723976	24.191987
128.626473	3772.735643	24.197005
128.704463	3777.937635	24.202023
128.999003	3789.292136	24.207040
128.934987	3796.141704	24.212058
128.779464	3807.313788	24.217075
128.904410	3813.079759	24.222093
129.269372	3812.694722	24.227111
129.344213	3821.416426	24.232128
129.671362	3836.168309	24.237146
129.851880	3843.652104	24.242163
129.702569	3846.885287	24.247181
130.147529	3846.607733	24.252199
130.058180	3859.237202	24.257216
130.534616	3868.896934	24.262234
130.427039	3874.803282	24.267251
130.346124	3864.580193	24.272269
130.230277	3869.926014	24.277287
130.704063	3889.802958	24.282304
131.085300	3892.145547	24.287322
131.181994	3893.285716	24.292339
131.078082	3898.061562	24.297357
131.470384	3903.710186	24.302375
131.489707	3915.738867	24.307392
131.639195	3909.188485	24.312410
132.218627	3915.716981	24.317427
131.993299	3912.163431	24.322445
132.523458	3914.637494	24.327463
132.562255	3930.681071	24.332480
132.803301	3933.610463	24.337498
132.708855	3928.215369	24.342515
132.904288	3927.036098	24.347533
132.914596	3923.108139	24.352551
132.974964	3927.858416	24.357568
133.239066	3926.359139	24.362586
133.504208	3929.404717	24.367603
133.621572	3927.682098	24.372621
133.854885	3909.314252	24.377639
133.684206	3915.946909	24.382656
133.537448	3921.979310	24.387674
133.538311	3920.053892	24.392691
133.800756	3922.724293	24.397709
134.337534	3935.268958	24.402727
133.877085	3948.366580	24.407744
134.279453	3945.438081	24.412762
134.201533	3945.466028	24.417779
134.609511	3957.610978	24.422797
134.661465	3962.946484	24.427815
134.856067	3971.769552	24.432832
134.751873	3974.967328	24.437850
134.788112	3973.898057	24.442867
135.047567	3987.467535	24.447885
135.331897	3990.191352	24.452903
135.080466	4003.565786	24.457920
134.987677	3996.137773	24.462938
135.589688	4006.478722	24.467955
135.429587	4020.596455	24.472973
135.718377	4023.805650	24.477991
135.683842	4045.008636	24.483008
135.887488	4044.509834	24.488026
136.197471	4057.493898	24.493043
136.153238	4068.380533	24.498061
136.908826	4066.132436	24.503079
136.558598	4075.097194	24.508096
137.046196	4088.972106	24.513114
137.321024	4091.040910	24.518131
137.094623	4093.254033	24.523149
137.735023	4086.469342	24.528167
137.809953	4092.025405	24.533184
138.086617	4096.836740	24.538202
138.346617	4106.975335	24.543219
138.188818	4106.864216	24.548237
138.665465	4097.974519	24.553255
138.735525	4104.721265	24.558272
138.915141	4099.277139	24.563290
138.903037	4096.138549	24.568307
138.926911	4095.860269	24.573325
139.299368	4089.287733	24.578343
138.715827	4096.095204	24.583360
139.296476	4090.399266	24.588378
139.658960	4093.300308	24.593395
139.243629	4106.769775	24.598413
139.664487	4112.843275	24.603431
139.609052	4121.550687	24.608448
139.837649	4118.825968	24.613466
139.936004	4120.928563	24.618483
139.718096	4123.894722	24.623501
140.199593	4141.864341	24.628519
140.315320	4141.928422	24.633536
140.248185	4142.825828	24.638554
140.303407	4157.020615	24.643571
140.318485	4166.638710	24.648589
140.875330	4163.670345	24.653607
140.951623	4185.528533	24.658624
141.196385	4187.030738	24.663642
141.696046	4190.699516	24.668659
141.686654	4181.494067	24.673677
141.791932	4184.075350	24.678695
141.638031	4187.492375	24.683712
141.577543	4189.632334	24.688730
141.717568	4202.665057	24.693747
142.068025	4209.535472	24.698765
142.351880	4210.239359	24.703783
142.239244	4223.257777	24.708800
142.690965	4228.114487	24.713818
142.701267	4229.968830	24.718835
142.683825	4229.169876	24.723853
142.965746	4226.474715	24.728871
143.096072	4239.240688	24.733888
143.198731	4249.839432	24.738906
143.476470	4262.137430	24.743923
143.165495	4251.571181	24.748941
143.758042	4250.109120	24.753959
143.939233	4259.265830	24.758976
144.108587	4269.437567	24.763994
144.392774	4270.337096	24.769011
144.166144	4278.979704	24.774029
144.328061	4265.120374	24.779047
144.423362	4278.466278	24.784064
144.327016	4289.257001	24.789082
144.538291	4294.896057	24.794099
145.012755	4309.855805	24.799117
145.436267	4318.984288	24.804135
145.369438	4329.953506	24.809152
145.589997	4331.349019	24.814170
145.975398	4321.362391	24.819187
145.559142	4323.399938	24.824205
146.336435	4324.203760	24.829223
146.149853	4327.136668	24.834240
145.931116	4334.951115	24.839258
146.253962	4346.396251	24.844275
146.260994	4350.517363	24.849293
146.254834	4350.025968	24.854311
146.557525	4356.891251	24.859328
146.529230	4371.812541	24.864346
146.916455	4369.082026	24.869363
147.057461	4378.879478	24.874381
147.148707	4387.084417	24.879399
147.516219	4389.792188	24.884416
147.632038	4390.323394	24.889434
147.935910	4403.595886	24.894451
147.798635	4407.313372	24.899469
147.841148	4409.948649	24.904487
147.600475	4413.959993	24.909504
147.791211	4431.612190	24.914522
148.329251	4430.382702	24.919539
148.889515	4452.689817	24.924557
148.955154	4456.101119	24.929575
148.900867	4470.417361	24.934592
149.499955	4456.764423	24.939610
149.276856	4457.263176	24.944627
149.606246	4476.153215	24.949645
149.988717	4473.110945	24.954663
149.630098	4481.067175	24.959680
149.454716	4477.625678	24.964698
149.886994	4488.267933	24.969715
150.397153	4500.485719	24.974733
150.434901	4510.513951	24.979751
150.490097	4508.305407	24.984768
150.642037	4497.951015	24.989786
150.813394	4506.907375	24.994803
150.942358	4529.894070	24.999821
151.124997	4525.052211	25.004839
151.089076	4528.716066	25.009856
151.296720	4542.486566	25.014874
151.489623	4542.557571	25.019891
151.272995	4552.341357	25.024909
151.736633	4562.265434	25.029927
151.777792	4568.679121	25.034944
151.982442	4576.254154	25.039962
152.360209	4568.519073	25.044979
152.576607	4572.052118	25.049997
152.787308	4558.977218	25.055015
152.765618	4580.137798	25.060032
153.128111	4586.495151	25.065050
153.338672	4597.001546	25.070067
153.226732	4600.064913	25.075085
153.344714	4592.856350	25.080103
153.333539	4593.202169	25.085120
153.264010	4596.097958	25.090138
153.965867	4610.807919	25.095155
153.931885	4611.659154	25.100173
154.000772	4619.267967	25.105191
154.106348	4621.053859	25.110208
154.231605	4630.506697	25.115226
154.676550	4641.276483	25.120243
154.492827	4653.438271	25.125261
154.620143	4644.236554	25.130279
155.074397	4656.485245	25.135296
154.865469	4666.040633	25.140314
154.990340	4668.356955	25.145331
155.070312	4689.069408	25.150349
155.099389	4698.912867	25.155367
155.484838	4699.982881	25.160384
155.551417	4722.471352	25.165402
155.930093	4725.332101	25.170419
156.132408	4717.703183	25.175437
156.020628	4736.049838	25.180455
156.568860	4743.344187	25.185472
156.523302	4740.627339	25.190490
157.008276	4761.349417	25.195507
157.296642	4774.024878	25.200525
157.512876	4772.555082	25.205543
157.672948	4767.966028	25.210560
157.360066	4772.496875	25.215578
157.601458	4762.396700	25.220595
157.930709	4791.217147	25.225613
158.530748	4789.400361	25.230631
158.568432	4788.015177	25.235648
158.499733	4792.028237	25.240666
158.697996	4785.668799	25.245683
159.070285	4786.137992	25.250701
159.160802	4786.619491	25.255719
159.187405	4787.088845	25.260736
159.231862	4798.239874	25.265754
159.332518	4805.379826	25.270771
159.714495	4809.136496	25.275789
159.571025	4816.248176	25.280807
159.884573	4814.056188	25.285824
159.797239	4836.309937	25.290842
160.021366	4826.969955	25.295859
159.946749	4835.333490	25.300877
160.333844	4844.250117	25.305895
160.268542	4858.142262	25.310912
160.433174	4862.396776	25.315930
160.892228	4871.485285	25.320947
160.733880	4880.559447	25.325965
161.066680	4885.403287	25.330983
161.028837	4897.182693	25.336000
160.843652	4915.035928	25.341018
161.628045	4907.966533	25.346035
161.575561	4919.524127	25.351053
161.576188	4929.829823	25.356071
162.089332	4939.134052	25.361088
162.055748	4951.588308	25.366106
162.491910	4955.589088	25.371123
162.152600	4963.574085	25.376141
162.629487	4957.745681	25.381159
163.302587	4972.315219	25.386176
163.127231	4978.630190	25.391194
163.098317	4976.826084	25.396211
163.356418	4987.625166	25.401229
163.453075	4987.588057	25.406247
163.646714	4996.474905	25.411264
163.767909	5002.519607	25.416282
164.024326	4999.799895	25.421299
163.968825	5010.976087	25.426317
164.142887	5026.734434	25.431335
164.688310	5026.226587	25.436352
164.986642	5029.898476	25.441370
165.009902	5027.218216	25.446387
164.844990	5038.938587	25.451405
164.974526	5051.822045	25.456423
165.389430	5048.111776	25.461440
165.589949	5058.206506	25.466458
165.847428	5063.201005	25.471475
165.651368	5075.002003	25.476493
165.761751	5076.165368	25.481511
165.710152	5081.675149	25.486528
165.784647	5104.159704	25.491546
166.339108	5109.957069	25.496563
166.837196	5120.965071	25.501581
166.823035	5129.846460	25.506599
167.257375	5129.816750	25.511616
167.185045	5129.540806	25.516634
167.433739	5137.358578	25.521651
168.132757	5130.270825	25.526669
168.233023	5127.726916	25.531687
168.704826	5118.625994	25.536704
168.465169	5125.257204	25.541722
168.535239	5114.691098	25.546739
168.642031	5121.328341	25.551757
169.004147	5128.711797	25.556775
169.069503	5126.504753	25.561792
169.010976	5139.884711	25.566810
169.222417	5144.390834	25.571827
169.122631	5150.921365	25.576845
169.293381	5152.147936	25.581863
169.728862	5164.598752	25.586880
169.652231	5174.206409	25.591898
169.694921	5179.490055	25.596915
169.815647	5184.771023	25.601933
169.940024	5199.640816	25.606951
170.153161	5205.248302	25.611968
170.127344	5216.915566	25.616986
170.144768	5226.552798	25.622003
170.520249	5238.640541	25.627021
170.716484	5250.686756	25.632039
170.997640	5261.362465	25.637056
170.935658	5278.442473	25.642074
171.533819	5286.237466	25.647091
171.570246	5292.929919	25.652109
171.692935	5304.978151	25.657127
171.692515	5312.673801	25.662144
172.120928	5321.742056	25.667162
172.759079	5323.325154	25.672180
172.911617	5331.691429	25.677197
172.688045	5336.928193	25.682215
173.218614	5344.796865	25.687232
173.101428	5352.558059	25.692250
173.371958	5349.428909	25.697268
173.809737	5358.587263	25.702285
173.824984	5371.722324	25.707303
173.942833	5370.577136	25.712320
174.136406	5384.748187	25.717338
173.809700	5383.520698	25.722356
174.348705	5388.206309	25.727373
174.569858	5406.867962	25.732391
174.893865	5405.614918	25.737408
174.596959	5406.144125	25.742426
175.011466	5413.532167	25.747444
175.240520	5433.070129	25.752461
174.955183	5431.627865	25.757479
175.074174	5436.110576	25.762496
175.404778	5446.680844	25.767514
175.879278	5456.594253	25.772532
175.770075	5459.288024	25.777549
176.227914	5484.781513	25.782567
176.267338	5486.337893	25.787584
176.472323	5492.013025	25.792602
176.750335	5502.152755	25.797620
176.645172	5500.186858	25.802637
176.633052	5507.338332	25.807655
177.060229	5516.975054	25.812672
177.397864	5530.167359	25.817690
177.533567	5540.354519	25.822708
177.719167	5546.105286	25.827725
177.873133	5556.327490	25.832743
177.888295	5560.226653	25.837760
178.022058	5580.281500	25.842778
178.294221	5578.392581	25.847796
178.830605	5591.339342	25.852813
178.765442	5610.714969	25.857831
179.271270	5611.655818	25.862848
179.017390	5608.220013	25.867866
179.527449	5621.439202	25.872884
179.711016	5629.336770	25.877901
179.969404	5636.828123	25.882919
180.141262	5641.416290	25.887936
180.108504	5656.916980	25.892954
180.400452	5662.714358	25.897972
180.667901	5655.292711	25.902989
180.642369	5669.595950	25.908007
181.275997	5684.771956	25.913024
181.105044	5686.736737	25.918042
181.026434	5685.540045	25.923060
181.480540	5695.860801	25.928077
182.063890	5702.556638	25.933095
182.433692	5693.979519	25.938112
182.482096	5692.545249	25.943130
182.403511	5688.731758	25.948148
182.706018	5693.302754	25.953165
182.985239	5701.469552	25.958183
183.324181	5699.668078	25.963200
183.154161	5702.756455	25.968218
183.178013	5708.734477	25.973236
183.493042	5705.367909	25.978253
183.428975	5717.417081	25.983271
183.957109	5720.595630	25.988288
184.379263	5725.987655	25.993306
184.400706	5727.587891	25.998324
184.650204	5713.745388	26.003341
184.633953	5725.736616	26.008359
184.759156	5730.849747	26.013376
185.061730	5740.423916	26.018394
185.086835	5740.262214	26.023412
185.177693	5739.872470	26.028429
185.279519	5758.600411	26.033447
185.181685	5769.976210	26.038464
185.708619	5774.067208	26.043482
185.477300	5777.663881	26.048500
185.745325	5787.278176	26.053517
185.946113	5799.017858	26.058535
186.554728	5817.215566	26.063552
186.888073	5827.046987	26.068570
186.753834	5825.492782	26.073588
187.093513	5819.878019	26.078605
187.275870	5830.635734	26.083623
187.397380	5836.939506	26.088640
187.498566	5851.816599	26.093658
187.115835	5853.760708	26.098676
187.731974	5860.767159	26.103693
187.661307	5871.475907	26.108711
187.526303	5866.105489	26.113728
187.839126	5887.477508	26.118746
188.063066	5899.955451	26.123764
188.503889	5916.351708	26.128781
188.673328	5921.944124	26.133799
188.980719	5933.446332	26.138816
189.286952	5945.125499	26.143834
189.055219	5950.824574	26.148852
189.297597	5958.501636	26.153869
189.761888	5972.012301	26.158887
190.130476	5993.902918	26.163904
189.899130	5997.543831	26.168922
190.178483	6005.682336	26.173940
190.789425	6007.708504	26.178957
190.588043	6024.331107	26.183975
191.000460	6032.976065	26.188992
191.208346	6044.001401	26.194010
191.250855	6050.298606	26.199028
191.469024	6055.084849	26.204045
191.737162	6067.698074	26.209063
191.813641	6074.049975	26.214080
192.091299	6089.647910	26.219098
192.241124	6104.328238	26.224116
192.653198	6107.250298	26.229133
192.798464	6122.925693	26.234151
192.920706	6120.927481	26.239168
193.056505	6132.443903	26.244186
193.152714	6152.151683	26.249204
193.178862	6150.117922	26.254221
193.491322	6161.973030	26.259239
193.929463	6172.852114	26.264256
194.070854	6174.468437	26.269274
194.601126	6202.723196	26.274292
195.008142	6197.811239	26.279309
195.240243	6207.456603	26.284327
195.087263	6210.015250	26.289344
195.326019	6216.828061	26.294362
195.275243	6228.802898	26.299380
195.533651	6233.305137	26.304397
195.669735	6241.687020	26.309415
195.664459	6253.323339	26.314432
195.997535	6245.764970	26.319450
196.395998	6269.299044	26.324468
196.645320	6263.322571	26.329485
196.612723	6267.589181	26.334503
196.833728	6279.758488	26.339520
197.417265	6286.388223	26.344538
197.012065	6291.322086	26.349556
197.623436	6308.784353	26.354573
197.702705	6319.612070	26.359591
198.100943	6322.646803	26.364608
198.345394	6338.177517	26.369626
198.162509	6356.921988	26.374644
198.425326	6347.480506	26.379661
198.417547	6368.397933	26.384679
198.683015	6369.265763	26.389696
199.158704	6379.485691	26.394714
199.273089	6392.142019	26.399732
199.172798	6394.733526	26.404749
199.051591	6401.308876	26.409767
199.385839	6416.008092	26.414784
199.993882	6416.194407	26.419802
200.147980	6449.069536	26.424820
200.650396	6446.042993	26.429837
200.410286	6448.369017	26.434855
200.972553	6460.996699	26.439872
201.409025	6463.274209	26.444890
201.453553	6477.298854	26.449908
201.667690	6471.782356	26.454925
201.710418	6474.439995	26.459943
201.874241	6495.138293	26.464960
202.228794	6491.263513	26.469978
202.057947	6504.526219	26.474996
202.379996	6496.164503	26.480013
202.739276	6512.772866	26.485031
202.448837	6525.299753	26.490048
202.942426	6540.580351	26.495066
202.545870	6551.081383	26.500084
203.317383	6558.354333	26.505101
203.810537	6569.376612	26.510119
203.821944	6574.589772	26.515136
204.322333	6589.964055	26.520154
204.341671	6604.118987	26.525172
204.649375	6600.933331	26.530189
204.506619	6609.971199	26.535207
204.591146	6623.759288	26.540224
204.943617	6630.687132	26.545242
204.944592	6645.217449	26.550260
205.437657	6654.288933	26.555277
205.448633	6656.942072	26.560295
205.801121	6668.115737	26.565312
206.278485	6667.536373	26.570330
206.334108	6694.871420	26.575348
206.392023	6691.746734	26.580365
207.009177	6699.630927	26.585383
206.712898	6712.064149	26.590400
206.957699	6724.350004	26.595418
207.395494	6734.702301	26.600436
207.564317	6743.060377	26.605453
207.470130	6753.321887	26.610471
208.018013	6760.544503	26.615488
208.454635	6765.764122	26.620506
208.430978	6776.526058	26.625524
208.775905	6781.662098	26.630541
208.961580	6797.587477	26.635559
209.420856	6804.334608	26.640576
209.263007	6797.575342	26.645594
209.257208	6815.604538	26.650612
209.987996	6818.417116	26.655629
209.965010	6827.196531	26.660647
210.262776	6834.281338	26.665664
210.510661	6845.540846	26.670682
210.591359	6856.728530	26.675700
211.038848	6861.182546	26.680717
211.177554	6863.061361	26.685735
211.229168	6868.906013	26.690752
211.704808	6878.005575	26.695770
211.237952	6890.714859	26.700788
211.886931	6885.446216	26.705805
211.997267	6909.423727	26.710823
212.271167	6915.918807	26.715840
212.488259	6915.850319	26.720858
212.355657	6937.501262	26.725876
212.813844	6942.165137	26.730893
213.127961	6952.268487	26.735911
212.985742	6971.768040	26.740928
213.727714	6971.703067	26.745946
213.969700	6972.745049	26.750964
214.290353	6980.899658	26.755981
214.525495	6993.708069	26.760999
214.728726	6995.917786	26.766016
214.825450	6984.039537	26.771034
214.654811	6997.293097	26.776052
215.095582	7000.659100	26.781069
215.291300	7014.262862	26.786087
215.023976	7017.944301	26.791104
215.236487	7026.403036	26.796122
215.664927	7041.176482	26.801140
215.901790	7037.926017	26.806157
216.133315	7058.614412	26.811175
216.577666	7067.870467	26.816192
216.546748	7064.497533	26.821210
216.781440	7082.060225	26.826228
216.949814	7086.627201	26.831245
217.490568	7104.742058	26.836263
217.663065	7119.242890	26.841280
217.423561	7109.194194	26.846298
217.789053	7123.058874	26.851316
217.942766	7130.860723	26.856333
218.221483	7146.771921	26.861351
218.431778	7160.310385	26.866368
218.607616	7166.634569	26.871386
218.900452	7186.814785	26.876404
219.044629	7201.714695	26.881421
219.178596	7207.095206	26.886439
219.510916	7228.503641	26.891456
219.763470	7232.590338	26.896474
219.877986	7249.287985	26.901492
220.004822	7267.006546	26.906509
220.225362	7274.816994	26.911527
220.548541	7294.193923	26.916544
220.909868	7295.444637	26.921562
220.810320	7311.711612	26.926580
221.312950	7326.543190	26.931597
221.643366	7345.565479	26.936615
221.731826	7361.983169	26.941632
222.123222	7358.916942	26.946650
222.578999	7367.379000	26.951668
222.550940	7379.029051	26.956685
222.671467	7384.777903	26.961703
222.838594	7402.329322	26.966720
223.250066	7422.200895	26.971738
223.854741	7446.812442	26.976756
223.993205	7445.559740	26.981773
224.578162	7430.271536	26.986791
224.788926	7431.766681	26.991808
224.827398	7435.460576	26.996826
225.148580	7464.194957	27.001844
225.381995	7455.035289	27.006861
225.425434	7463.978295	27.011879
225.704182	7463.811814	27.016896
226.212987	7472.521371	27.021914
225.931617	7479.456671	27.026932
226.014783	7487.433813	27.031949
226.023183	7486.687516	27.036967
226.093722	7508.370643	27.041984
226.591752	7504.201823	27.047002
226.609183	7523.673949	27.052020
226.660134	7543.687019	27.057037
227.520820	7547.748559	27.062055
227.379145	7567.851625	27.067072
227.544880	7576.005364	27.072090
227.827801	7595.085817	27.077108
227.722103	7604.610880	27.082125
227.959468	7617.283634	27.087143
228.065421	7640.852386	27.092160
228.581689	7647.054284	27.097178
228.691079	7659.472340	27.102196
228.940974	7678.952636	27.107213
229.552556	7683.371837	27.112231
229.734373	7699.143912	27.117248
229.769502	7700.757974	27.122266
230.222955	7714.331599	27.127284
230.110633	7725.341507	27.132301
230.349570	7737.228026	27.137319
230.362108	7758.147032	27.142336
230.804115	7761.254117	27.147354
231.101257	7783.767286	27.152372
230.884631	7805.132424	27.157389
231.711358	7794.813174	27.162407
232.034169	7821.596877	27.167424
232.483334	7815.954993	27.172442
232.663696	7827.585508	27.177460
232.734302	7844.861939	27.182477
233.230546	7845.157233	27.187495
233.332427	7862.119431	27.192512
233.605719	7863.904787	27.197530
233.980811	7869.112204	27.202548
234.002372	7893.373161	27.207565
234.488044	7894.285708	27.212583
234.553334	7904.873452	27.217600
234.910970	7903.722346	27.222618
234.942591	7921.551070	27.227636
235.025041	7931.608948	27.232653
235.505284	7942.744561	27.237671
235.608648	7949.257088	27.242688
235.759238	7947.295306	27.247706
236.222997	7967.875959	27.252724
236.396841	7975.867608	27.257741
236.832295	7986.334631	27.262759
236.906494	8002.202645	27.267776
237.248856	8012.573682	27.272794
237.468365	8011.150476	27.277812
237.607244	8031.971198	27.282829
237.775332	8036.506887	27.287847
238.001196	8059.160927	27.292864
238.163991	8058.456866	27.297882
238.415409	8069.142007	27.302900
238.542767	8085.844729	27.307917
238.698167	8093.087939	27.312935
238.622007	8120.306716	27.317952
238.935955	8128.055630	27.322970
239.182345	8150.296177	27.327988
239.369194	8166.718209	27.333005
239.908027	8175.972745	27.338023
239.836145	8201.050531	27.343040
240.194852	8214.459329	27.348058
241.104355	8218.324002	27.353076
241.768439	8237.159516	27.358093
242.252052	8225.333886	27.363111
242.178633	8241.294542	27.368128
242.268076	8236.305209	27.373146
242.609482	8246.468165	27.378164
242.546974	8254.720880	27.383181
242.630280	8256.018103	27.388199
242.537199	8271.091569	27.393216
242.885408	8281.553401	27.398234
243.245100	8295.356731	27.403252
243.305067	8301.197381	27.408269
243.499215	8304.952453	27.413287
243.820882	8320.378114	27.418304
244.378859	8344.199409	27.423322
244.913928	8343.045909	27.428340
244.919038	8354.227330	27.433357
245.375051	8357.622785	27.438375
244.939875	8370.116631	27.443392
245.342364	8377.040509	27.448410
245.933521	8381.564087	27.453428
245.900827	8391.570687	27.458445
246.485197	8407.747938	27.463463
246.715940	8415.317348	27.468480
246.765790	8420.648171	27.473498
247.465303	8421.495883	27.478516
247.127731	8437.895620	27.483533
247.400008	8436.189504	27.488551
247.787923	8454.092712	27.493568
247.801468	8458.671508	27.498586
248.320404	8473.548831	27.503604
248.394033	8491.636758	27.508621
248.512367	8481.913602	27.513639
248.405201	8497.134669	27.518656
248.689355	8513.384009	27.523674
249.219847	8523.760773	27.528692
249.452992	8547.282470	27.533709
249.516824	8557.160478	27.538727
249.825764	8573.036635	27.543744
249.933070	8581.307257	27.548762
250.579509	8605.550792	27.553780
250.517593	8613.472082	27.558797
251.210693	8622.680727	27.563815
251.296005	8639.864058	27.568832
251.774887	8665.140865	27.573850
252.330306	8674.446741	27.578868
252.047750	8685.603693	27.583885
252.399317	8697.511183	27.588903
252.851593	8711.625591	27.593920
253.010738	8716.535376	27.598938
253.067637	8727.020715	27.603956
253.288106	8748.738786	27.608973
253.834235	8748.401229	27.613991
254.222037	8768.909362	27.619008
254.358977	8781.229172	27.624026
254.617405	8781.788822	27.629044
254.442116	8795.931541	27.634061
255.291196	8799.287983	27.639079
255.335664	8825.226177	27.644096
255.500433	8829.588938	27.649114
255.775128	8839.112243	27.654132
255.771121	8865.320080	27.659149
256.199534	8866.645703	27.664167
256.497959	8888.601214	27.669184
256.296175	8902.255629	27.674202
256.982786	8903.525272	27.679220
257.196134	8924.095466	27.684237
257.732787	8935.885895	27.689255
257.727246	8948.695254	27.694272
258.219038	8957.594439	27.699290
258.643210	8952.439145	27.704308
258.849014	8977.405295	27.709325
259.523752	8974.417821	27.714343
259.726341	8985.070053	27.719360
259.587252	8987.336463	27.724378
259.891382	8999.816661	27.729396
259.875936	9007.408857	27.734413
259.956555	9013.666417	27.739431
260.230606	9036.898225	27.744448
260.448230	9049.777096	27.749466
261.128148	9057.403126	27.754484
261.235126	9074.899202	27.759501
261.286914	9088.981535	27.764519
261.121116	9102.311623	27.769536
261.437264	9117.713554	27.774554
261.944165	9127.646016	27.779572
262.022806	9144.063665	27.784589
262.424261	9157.621195	27.789607
262.503617	9175.819400	27.794624
262.718880	9188.720835	27.799642
263.385548	9202.758041	27.804660
263.242046	9227.747340	27.809677
263.745916	9229.206473	27.814695
264.156625	9242.443750	27.819712
264.213191	9253.390387	27.824730
264.633082	9267.090358	27.829748
264.812220	9285.509925	27.834765
265.250874	9304.466872	27.839783
265.546816	9313.879771	27.844800
265.796085	9330.005815	27.849818
266.057138	9334.116916	27.854836
266.315162	9351.772856	27.859853
266.540853	9356.022069	27.864871
266.993024	9378.756153	27.869888
266.924622	9388.301586	27.874906
267.522233	9392.243485	27.879924
267.708625	9403.220514	27.884941
267.987274	9420.488129	27.889959
267.993382	9446.575239	27.894976
268.061411	9457.270792	27.899994
268.686358	9466.657805	27.905012
268.807426	9480.581260	27.910029
269.179282	9485.344474	27.915047
269.834683	9510.623372	27.920064
269.830272	9517.961481	27.925082
270.446870	9535.716475	27.930100
270.651073	9547.227545	27.935117
270.954273	9563.957899	27.940135
271.228427	9567.978610	27.945152
271.677266	9579.429513	27.950170
272.077274	9588.008626	27.955188
271.762543	9597.358880	27.960205
272.225865	9602.950867	27.965223
272.965384	9610.394201	27.970240
272.596410	9624.908687	27.975258
273.096262	9635.309793	27.980276
273.003982	9656.240949	27.985293
273.477927	9661.556620	27.990311
274.235876	9661.883825	27.995328
274.321538	9669.618414	28.000346
274.892428	9673.144621	28.005364
274.796350	9695.254067	28.010381
274.993341	9710.930781	28.015399
275.310462	9707.749445	28.020416
275.283407	9726.362572	28.025434
275.979804	9740.285055	28.030452
275.959171	9746.697545	28.035469
276.127976	9760.777957	28.040487
276.167524	9769.400643	28.045504
276.549062	9793.118671	28.050522
277.111555	9809.388963	28.055540
277.549469	9825.391351	28.060557
277.323634	9838.974424	28.065575
277.841205	9844.551725	28.070592
278.136743	9867.004538	28.075610
278.615458	9875.426296	28.080628
278.545048	9895.823893	28.085645
278.853098	9906.731763	28.090663
279.372586	9922.816255	28.095680
279.469917	9939.733707	28.100698
279.745029	9940.578111	28.105716
279.575073	9974.387705	28.110733
279.854636	9981.091370	28.115751
280.428165	9984.506722	28.120768
280.274397	10001.125490	28.125786
280.611975	10022.507935	28.130804
281.036839	10046.443710	28.135821
281.078650	10046.907675	28.140839
281.506025	10069.033948	28.145856
281.878986	10095.595284	28.150874
282.456784	10100.326596	28.155892
282.535251	10121.389559	28.160909
282.554010	10142.499729	28.165927
283.545367	10150.352416	28.170944
283.201296	10168.500693	28.175962
283.933861	10188.227381	28.180980
283.922571	10199.055688	28.185997
284.182545	10218.852826	28.191015
284.584141	10235.647402	28.196032
284.839973	10263.730110	28.201050
284.927679	10271.452001	28.206068
285.353099	10288.947005	28.211085
285.849591	10309.986147	28.216103
286.241804	10310.256642	28.221120
286.184561	10331.056808	28.226138
286.565991	10346.904257	28.231156
287.480045	10362.649854	28.236173
287.518879	10371.850729	28.241191
288.355273	10382.692411	28.246208
288.462916	10404.240544	28.251226
288.722158	10394.279750	28.256244
288.950226	10404.095284	28.261261
288.925454	10413.435534	28.266279
289.486338	10424.225412	28.271296
289.660011	10436.938433	28.276314
290.113740	10450.466670	28.281332
290.171445	10467.065560	28.286349
290.512304	10476.573094	28.291367
290.951851	10480.602986	28.296384
290.797109	10505.999896	28.301402
291.379001	10510.512817	28.306420
291.730907	10524.457949	28.311437
292.063814	10541.958122	28.316455
292.265080	10547.625927	28.321472
292.061888	10563.810856	28.326490
292.324762	10569.058613	28.331508
292.567094	10595.281056	28.336525
292.940376	10624.883681	28.341543
293.403996	10641.106948	28.346560
293.741060	10659.500133	28.351578
294.061291	10674.978500	28.356596
294.459107	10694.240024	28.361613
294.235216	10715.878020	28.366631
294.825664	10718.059479	28.371648
295.172724	10740.641095	28.376666
295.538584	10756.001915	28.381684
296.071835	10770.967268	28.386701
296.021638	10789.010405	28.391719
296.586448	10802.474243	28.396736
296.889316	10813.964423	28.401754
297.296678	10828.908374	28.406772
297.801658	10841.592194	28.411789
297.819738	10852.940445	28.416807
298.150581	10866.677565	28.421824
298.125869	10875.894896	28.426842
298.360874	10896.249196	28.431860
299.119919	10903.570031	28.436877
299.387485	10914.857376	28.441895
299.860711	10925.165472	28.446912
299.928727	10942.757780	28.451930
300.113100	10954.414895	28.456948
300.503279	10972.718026	28.461965
300.305824	10977.412386	28.466983
301.099078	10985.646752	28.472000
301.264923	11002.485038	28.477018
301.357368	11016.789839	28.482036
301.908020	11031.004370	28.487053
301.900439	11052.384898	28.492071
301.885267	11057.925523	28.497088
302.346978	11082.718888	28.502106
302.306418	11094.107990	28.507124
302.847917	11119.144739	28.512141
303.352549	11141.967539	28.517159
303.631006	11160.796605	28.522176
303.645703	11174.418979	28.527194
304.269189	11188.461259	28.532212
304.453370	11209.284808	28.537229
304.826465	11224.973270	28.542247
305.084593	11239.536623	28.547264
305.525029	11263.035801	28.552282
306.030878	11283.654636	28.557300
306.036074	11298.522644	28.562317
305.912267	11319.365847	28.567335
306.496278	11340.272542	28.572352
306.714171	11359.357524	28.577370
307.189168	11384.989127	28.582388
307.689185	11399.735974	28.587405
307.724921	11420.491300	28.592423
308.348867	11445.408294	28.597440
308.686290	11467.202902	28.602458
309.011676	11483.546307	28.607476
309.369218	11497.627065	28.612493
309.770414	11518.325603	28.617511
310.318347	11524.119716	28.622528
310.743990	11539.576075	28.627546
311.194280	11548.956604	28.632564
311.418522	11566.266257	28.637581
311.741779	11573.399440	28.642599
311.867064	11586.436535	28.647616
312.240085	11596.100669	28.652634
312.438560	11612.741812	28.657652
313.028340	11626.644421	28.662669
312.872452	11648.096082	28.667687
313.364365	11656.829196	28.672704
313.748714	11668.875583	28.677722
313.897862	11691.530208	28.682740
314.362450	11706.993273	28.687757
314.610482	11726.797027	28.692775
315.162517	11737.680617	28.697792
315.041031	11747.879668	28.702810
315.429221	11766.799619	28.707828
316.036526	11779.477621	28.712845
315.649027	11801.350743	28.717863
316.405544	11812.155177	28.722880
316.571759	11835.770392	28.727898
317.138685	11848.334737	28.732916
317.155458	11864.442336	28.737933
316.922034	11887.763022	28.742951
317.883571	11904.051963	28.747968
318.016979	11926.740900	28.752986
318.510338	11950.153761	28.758004
318.641114	11963.559706	28.763021
318.956936	11992.219835	28.768039
319.558415	12005.874610	28.773056
319.553169	12025.793894	28.778074
319.557058	12048.414727	28.783092
320.353325	12069.614431	28.788109
320.533007	12093.477328	28.793127
321.233395	12113.233169	28.798144
321.471082	12122.934434	28.803162
321.790262	12139.753028	28.808180
322.070931	12154.000974	28.813197
321.942971	12167.510499	28.818215
322.594870	12174.062260	28.823232
322.600155	12191.536042	28.828250
323.093725	12209.202224	28.833268
323.634670	12221.988746	28.838285
323.745720	12252.601022	28.843303
324.010372	12274.066867	28.848320
324.256488	12291.310629	28.853338
325.197553	12281.002703	28.858356
326.334851	12289.064097	28.863373
326.296062	12292.837297	28.868391
326.660031	12297.981389	28.873408
326.963674	12317.647644	28.878426
327.123668	12320.344705	28.883444
327.406253	12323.928940	28.888461
327.788418	12340.400035	28.893479
327.872568	12341.154290	28.898496
328.363179	12360.914633	28.903514
328.302936	12368.650950	28.908532
328.786752	12383.603190	28.913549
328.839963	12401.300218	28.918567
328.918859	12411.919986	28.923584
329.266091	12452.259469	28.928602
329.800046	12469.218596	28.933620
330.715830	12487.918198	28.938637
330.507351	12504.111936	28.943655
330.696744	12518.415420	28.948672
330.827769	12547.600930	28.953690
331.222990	12568.787850	28.958708
332.014270	12579.306279	28.963725
332.044449	12602.842589	28.968743
332.529322	12618.694808	28.973760
332.481031	12636.761528	28.978778
332.809064	12654.314960	28.983796
333.379890	12675.013630	28.988813
333.460768	12704.355604	28.993831
333.924110	12720.694399	28.998848
334.249310	12746.486969	29.003866
334.985939	12767.046247	29.008884
335.808421	12783.237610	29.013901
336.067973	12800.602900	29.018919
336.352041	12808.737357	29.023936
337.070528	12818.733590	29.028954
336.595913	12836.721614	29.033972
337.238423	12842.463522	29.038989
337.142234	12853.398155	29.044007
337.170815	12882.056992	29.049024
337.676414	12899.068289	29.054042
337.803361	12925.722469	29.059060
338.764294	12944.930220	29.064077
338.729511	12967.005561	29.069095
339.332952	12982.425956	29.074112
339.358274	13007.334015	29.079130
339.897131	13023.320274	29.084148
340.175065	13039.454533	29.089165
340.524250	13067.801641	29.094183
340.753695	13089.542312	29.099200
341.078574	13102.091499	29.104218
341.142554	13134.850387	29.109236
341.638598	13152.804435	29.114253
341.519422	13183.814059	29.119271
342.549106	13209.361799	29.124288
342.963336	13231.099128	29.129306
343.024711	13253.661932	29.134324
343.357693	13270.128867	29.139341
343.849220	13297.983639	29.144359
344.003972	13310.979447	29.149376
344.661963	13333.961038	29.154394
344.715341	13353.474707	29.159412
345.310961	13369.168214	29.164429
345.296668	13384.928266	29.169447
345.708760	13412.239788	29.174464
346.044949	13431.289510	29.179482
346.383837	13457.781971	29.184500
346.825889	13467.976323	29.189517
346.804858	13498.282763	29.194535
347.366538	13519.170100	29.199552
347.959224	13531.333669	29.204570
348.188576	13545.574869	29.209588
348.915245	13568.615528	29.214605
349.429267	13586.178768	29.219623
349.580720	13590.800509	29.224640
350.108202	13617.184885	29.229658
350.475049	13630.788950	29.234676
350.865354	13647.983085	29.239693
350.910793	13670.965713	29.244711
351.468462	13686.204336	29.249728
351.653004	13708.754823	29.254746
351.875373	13731.836297	29.259764
352.077110	13737.331309	29.264781
352.883604	13763.394554	29.269799
352.834327	13782.567799	29.274816
353.209379	13804.596102	29.279834
353.345904	13830.735321	29.284852
353.793720	13852.332344	29.289869
354.343127	13874.908333	29.294887
354.574940	13898.155912	29.299904
355.148233	13930.960045	29.304922
355.181455	13952.271194	29.309940
355.722099	13973.550739	29.314957
356.362102	13996.636993	29.319975
356.535495	14006.185023	29.324992
357.036534	14021.079039	29.330010
356.919358	14054.278257	29.335028
357.588606	14075.809483	29.340045
358.028120	14094.556410	29.345063
358.466247	14109.018171	29.350080
359.012110	14129.292836	29.355098
359.076898	14164.946106	29.360116
359.494431	14168.809697	29.365133
359.704133	14200.338224	29.370151
359.886828	14224.673889	29.375168
360.783240	14242.604540	29.380186
361.162317	14260.467322	29.385204
361.627067	14283.546471	29.390221
361.791710	14298.834144	29.395239
362.108353	14324.933370	29.400256
362.510880	14347.479103	29.405274
362.846347	14349.201727	29.410292
363.500378	14374.670576	29.415309
364.069754	14386.045659	29.420327
364.248504	14406.936748	29.425344
364.705698	14419.889390	29.430362
365.012670	14442.870133	29.435380
365.361513	14451.876311	29.440397
365.659644	14460.438787	29.445415
365.837326	14476.621460	29.450432
366.258504	14497.408588	29.455450
366.383775	14519.325022	29.460468
366.839764	14540.046774	29.465485
366.973700	14569.888669	29.470503
367.026302	14591.396476	29.475520
367.786720	14608.082258	29.480538
367.904023	14637.588934	29.485556
368.250569	14659.120533	29.490573
368.864942	14661.642976	29.495591
369.124537	14687.574729	29.500608
369.661942	14711.132592	29.505626
369.832143	14732.653831	29.510644
370.590338	14750.811760	29.515661
370.349438	14770.552711	29.520679
370.663688	14792.051592	29.525696
371.406261	14807.429712	29.530714
371.581875	14827.759608	29.535732
371.994467	14856.541658	29.540749
372.466348	14875.044301	29.545767
372.692668	14896.481194	29.550784
373.076344	14918.465235	29.555802
373.542959	14937.445636	29.560820
374.116605	14956.178850	29.565837
374.606302	14969.666850	29.570855
375.108972	15000.870020	29.575872
375.892618	15014.612313	29.580890
375.987732	15028.581817	29.585908
376.155575	15042.416841	29.590925
376.556087	15056.642004	29.595943
376.941747	15079.595475	29.600960
377.258347	15098.128827	29.605978
377.701510	15118.445804	29.610996
377.805793	15142.545356	29.616013
378.366726	15169.394093	29.621031
378.813010	15186.685129	29.626048
379.066508	15201.081721	29.631066
379.462380	15226.525582	29.636084
380.228886	15235.842935	29.641101
380.949098	15265.840986	29.646119
380.980152	15285.934905	29.651136
381.236066	15290.799770	29.656154
381.457961	15319.609049	29.661172
381.651036	15338.427154	29.666189
382.071594	15354.105348	29.671207
382.350086	15385.517750	29.676224
382.799006	15402.906476	29.681242
383.245753	15431.065068	29.686260
383.795301	15442.617575	29.691277
384.171180	15465.045611	29.696295
384.256978	15493.374184	29.701312
384.519377	15504.538755	29.706330
384.884924	15536.932695	29.711348
385.694330	15565.587716	29.716365
385.960384	15595.132723	29.721383
386.081558	15612.212624	29.726400
386.180557	15632.548989	29.731418
386.631243	15668.685055	29.736436
387.150680	15700.455246	29.741453
387.808915	15722.823836	29.746471
388.056988	15751.307548	29.751488
388.714401	15772.330903	29.756506
389.528612	15794.836368	29.761524
389.312581	15817.660162	29.766541
389.928891	15838.064649	29.771559
390.139057	15859.318800	29.776576
390.876764	15871.527623	29.781594
391.271221	15896.426214	29.786612
391.351410	15919.497734	29.791629
391.920697	15944.062815	29.796647
392.145294	15970.920826	29.801664
392.430596	15991.099077	29.806682
392.844332	16011.907967	29.811700
393.400370	16037.078467	29.816717
393.807432	16055.829223	29.821735
394.029527	16075.496281	29.826752
394.402249	16099.997414	29.831770
394.458502	16126.209127	29.836788
394.529648	16154.743092	29.841805
395.093668	16176.375198	29.846823
395.641549	16202.248337	29.851840
396.379995	16227.362265	29.856858
396.641336	16252.237825	29.861876
397.267817	16273.752934	29.866893
397.925166	16277.203781	29.871911
397.896565	16301.454972	29.876928
398.684079	16316.855745	29.881946
398.840496	16343.096379	29.886964
399.434787	16365.646230	29.891981
400.120628	16374.202901	29.896999
400.575755	16395.318443	29.902016
400.961036	16406.287542	29.907034
401.208292	16430.448576	29.912052
401.339375	16446.570690	29.917069
402.107298	16463.721217	29.922087
402.090735	16484.231238	29.927104
402.736228	16504.363431	29.932122
402.745682	16527.639357	29.937140
403.000850	16552.247804	29.942157
403.654505	16575.113976	29.947175
403.831012	16606.136823	29.952192
404.790913	16624.659942	29.957210
405.015106	16657.283080	29.962228
405.156041	16681.318852	29.967245
405.301110	16706.721609	29.972263
405.759857	16734.321210	29.977280
406.335231	16753.008545	29.982298
406.585237	16784.955135	29.987316
406.988703	16811.811744	29.992333
407.842810	16833.029895	29.997351
407.937326	16860.000997	30.002368
408.577805	16887.632536	30.007386
408.951077	16920.299239	30.012404
409.417852	16951.555400	30.017421
410.054637	16975.239559	30.022439
410.471921	16993.954898	30.027456
410.769151	17018.377361	30.032474
410.995908	17043.960514	30.037492
411.401344	17064.541270	30.042509
411.827120	17082.547873	30.047527
412.027270	17119.603738	30.052544
412.716673	17141.893333	30.057562
413.399594	17169.660803	30.062580
414.266146	17195.160346	30.067597
414.429933	17201.123409	30.072615
414.908218	17220.947584	30.077632
415.020242	17226.612339	30.082650
415.328154	17248.951973	30.087668
415.715044	17277.315267	30.092685
416.030819	17290.996228	30.097703
416.556375	17334.239926	30.102720
417.378979	17342.984205	30.107738
417.649158	17362.446108	30.112756
417.648632	17398.191373	30.117773
418.080512	17416.649011	30.122791
418.155745	17452.657375	30.127808
418.932804	17464.946375	30.132826
419.443822	17494.683585	30.137844
419.417848	17526.737541	30.142861
420.017877	17544.363690	30.147879
420.496073	17577.668997	30.152896
420.783904	17607.220027	30.157914
421.443376	17637.629232	30.162932
422.018855	17662.195550	30.167949
422.359453	17665.857052	30.172967
422.862645	17684.932403	30.177984
423.104867	17705.090735	30.183002
423.223084	17720.858999	30.188020
423.700393	17746.533580	30.193037
423.962491	17773.827316	30.198055
424.374599	17803.814138	30.203072
424.815976	17830.069290	30.208090
425.446713	17860.173776	30.213108
425.750336	17887.271691	30.218125
426.388086	17921.127620	30.223143
426.775130	17937.883922	30.228160
426.999592	17971.949577	30.233178
427.833708	17991.586488	30.238196
427.725482	18016.657684	30.243213
428.475926	18043.079799	30.248231
428.923334	18070.780998	30.253248
429.438306	18090.309762	30.258266
429.621304	18121.033964	30.263284
429.839430	18160.072663	30.268301
430.826191	18177.380176	30.273319
430.968648	18210.404023	30.278336
431.712997	18238.122409	30.283354
432.005876	18252.903678	30.288372
432.319556	18280.891326	30.293389
433.149990	18309.866204	30.298407
433.325814	18343.169364	30.303424
433.869008	18368.367029	30.308442
434.148160	18392.197051	30.313460
434.329951	18426.415449	30.318477
435.277996	18453.761293	30.323495
435.321554	18486.339835	30.328512
435.449498	18512.000330	30.333530
435.997050	18536.628965	30.338548
436.434794	18569.778026	30.343565
437.511371	18605.563154	30.348583
437.849217	18637.691818	30.353600
437.862786	18659.169189	30.358618
438.515946	18684.767100	30.363636
438.634542	18721.636571	30.368653
439.746423	18747.428487	30.373671
440.083770	18775.640596	30.378688
440.549210	18809.297474	30.383706
440.876985	18828.180149	30.388724
441.487982	18852.913026	30.393741
441.906537	18880.360856	30.398759
442.183440	18919.846798	30.403776
442.683819	18941.229742	30.408794
442.995060	18960.430999	30.413812
443.397504	18998.697216	30.418829
444.165341	19029.426573	30.423847
444.384192	19057.202671	30.428864
444.772109	19082.564426	30.433882
445.327177	19111.059009	30.438900
445.486644	19135.565611	30.443917
446.243775	19157.104669	30.448935
446.274973	19174.157510	30.453952
446.933377	19209.452902	30.458970
447.639116	19242.150741	30.463988
447.942470	19273.287632	30.469005
448.443883	19291.562499	30.474023
448.654269	19325.146258	30.479040
449.034475	19365.520455	30.484058
449.827779	19386.043301	30.489076
450.010728	19414.552036	30.494093
450.423401	19445.880670	30.499111
451.140878	19481.679097	30.504128
451.569706	19506.396943	30.509146
452.298362	19531.409302	30.514164
452.335763	19555.114125	30.519181
452.753300	19574.583741	30.524199
453.229117	19601.682515	30.529216
453.409772	19641.210175	30.534234
453.717557	19654.511825	30.539252
454.218172	19679.768364	30.544269
454.722458	19706.250023	30.549287
454.916409	19748.094473	30.554304
455.816151	19772.050699	30.559322
456.283891	19803.971532	30.564340
456.694538	19834.669320	30.569357
457.121869	19862.622600	30.574375
457.549799	19890.019853	30.579392
457.584135	19930.777594	30.584410
458.812697	19959.181207	30.589428
459.132855	19989.722744	30.594445
459.380851	20016.630116	30.599463
459.714915	20048.054089	30.604480
460.141581	20090.412704	30.609498
460.548909	20132.692287	30.614516
461.371152	20148.536140	30.619533
462.372616	20169.103224	30.624551
462.665384	20192.769065	30.629568
463.375567	20220.337653	30.634586
463.859139	20238.192881	30.639604
464.166413	20268.395687	30.644621
464.395704	20299.109803	30.649639
465.029219	20323.285059	30.654656
465.347759	20354.516082	30.659674
465.921442	20375.023620	30.664692
466.148129	20415.019532	30.669709
466.627532	20444.222832	30.674727
467.218566	20454.663074	30.679744
467.711731	20503.456664	30.684762
468.599327	20525.703509	30.689780
469.012927	20552.263615	30.694797
469.223656	20576.858818	30.699815
469.239303	20613.886888	30.704832
470.009761	20646.867643	30.709850
470.713649	20674.450488	30.714868
471.165443	20706.432141	30.719885
471.387556	20723.254431	30.724903
472.033532	20759.173743	30.729920
472.043781	20800.575179	30.734938
472.913757	20827.051974	30.739956
473.300620	20875.629267	30.744973
473.698084	20886.731697	30.749991
474.277871	20919.281365	30.755008
474.740520	20951.413365	30.760026
475.247563	20985.983666	30.765044
475.583360	21013.144106	30.770061
476.000184	21039.925510	30.775079
476.375287	21070.491770	30.780096
476.847950	21105.307727	30.785114
477.383496	21138.559657	30.790132
477.799885	21176.714241	30.795149
477.991862	21202.001841	30.800167
478.918551	21235.458412	30.805184
478.800189	21277.752803	30.810202
479.664133	21310.789624	30.815220
480.056962	21351.747242	30.820237
480.649117	21386.797831	30.825255
481.488419	21415.599039	30.830272
482.004811	21444.785434	30.835290
482.483654	21471.336629	30.840308
482.963199	21499.056654	30.845325
483.237420	21521.122112	30.850343
484.028050	21542.784961	30.855360
484.374784	21574.658016	30.860378
484.893718	21597.064568	30.865396
485.317703	21628.199063	30.870413
485.686362	21654.773977	30.875431
486.365442	21684.548292	30.880448
486.702456	21709.314806	30.885466
487.468681	21731.417638	30.890484
487.834001	21761.253552	30.895501
488.284698	21783.948953	30.900519
489.123340	21813.496432	30.905536
488.897027	21841.251004	30.910554
489.298446	21873.634148	30.915572
489.921785	21909.337940	30.920589
490.540228	21933.422752	30.925607
490.838907	21969.556308	30.930624
491.018131	22003.459116	30.935642
491.485207	22041.171504	30.940660
492.089531	22081.510087	30.945677
492.237684	22106.028483	30.950695
492.937974	22157.037036	30.955712
493.663299	22196.529278	30.960730
493.993264	22224.071415	30.965748
494.605943	22260.567332	30.970765
495.789011	22283.642151	30.975783
496.487802	22306.836619	30.980800
496.951432	22343.330618	30.985818
498.007538	22361.003870	30.990836
498.054290	22379.308173	30.995853
499.025120	22402.637327	31.000871
499.478565	22423.961881	31.005888
499.864631	22449.189273	31.010906
500.421808	22471.868891	31.015924
500.801460	22503.074857	31.020941
500.915997	22528.875394	31.025959
501.815705	22547.558885	31.030976
501.870495	22572.920150	31.035994
502.635866	22588.288294	31.041012
503.074165	22634.568208	31.046029
502.820239	22657.336396	31.051047
503.786410	22688.748330	31.056064
504.301169	22726.037563	31.061082
504.601292	22750.975417	31.066100
505.107384	22785.043519	31.071117
505.358258	22825.381776	31.076135
505.943185	22854.704923	31.081152
506.422495	22897.794374	31.086170
506.991233	22930.374363	31.091188
507.284602	22975.041049	31.096205
507.762274	23012.418740	31.101223
508.638470	23054.416766	31.106240
508.565353	23092.505924	31.111258
509.662009	23117.238091	31.116276
510.381689	23149.731754	31.121293
510.902776	23166.263148	31.126311
511.684654	23196.453430	31.131328
512.084216	23233.508793	31.136346
512.578868	23257.298545	31.141364
513.426575	23289.709317	31.146381
513.584435	23322.265448	31.151399
513.859394	23352.155743	31.156416
514.258260	23393.394690	31.161434
514.899658	23415.853752	31.166452
515.377292	23447.564111	31.171469
515.885448	23489.342318	31.176487
516.629361	23521.181955	31.181504
517.031217	23551.741572	31.186522
517.595639	23576.740425	31.191540
517.771812	23600.093599	31.196557
518.104989	23635.220090	31.201575
518.518731	23657.221978	31.206592
518.596172	23694.480005	31.211610
519.388581	23733.446705	31.216628
520.050612	23768.863470	31.221645
520.320889	23807.494536	31.226663
521.117167	23838.524000	31.231680
521.694181	23880.987416	31.236698
522.148803	23907.564611	31.241716
522.970662	23946.350207	31.246733
523.262805	23981.313079	31.251751
524.023211	24012.354718	31.256768
524.601000	24046.217928	31.261786
524.754188	24081.069903	31.266804
525.720997	24113.147517	31.271821
525.931773	24152.989171	31.276839
526.569039	24179.291845	31.281856
526.858572	24225.484878	31.286874
527.532079	24255.996968	31.291892
528.171612	24297.269832	31.296909
528.701055	24334.458690	31.301927
529.468366	24366.087501	31.306944
529.965673	24402.011304	31.311962
530.262131	24436.506672	31.316980
530.693002	24466.715612	31.321997
531.318202	24506.259639	31.327015
532.013099	24537.078478	31.332032
532.627248	24585.882265	31.337050
532.897482	24627.636703	31.342068
533.429822	24662.487542	31.347085
533.890246	24704.509545	31.352103
534.747818	24749.515779	31.357120
535.119219	24793.725715	31.362138
535.405904	24825.505910	31.367156
537.012265	24840.068700	31.372173
537.424770	24876.196142	31.377191
538.263569	24891.946453	31.382208
539.149011	24918.097717	31.387226
539.646117	24943.551129	31.392244
539.945421	24968.744670	31.397261
540.165298	24997.274673	31.402279
540.957379	25023.156230	31.407296
541.836635	25039.639745	31.412314
542.365309	25073.733529	31.417332
543.105251	25079.666174	31.422349
543.034957	25105.448266	31.427367
543.619338	25132.885311	31.432384
543.971984	25163.872150	31.437402
544.184862	25190.773069	31.442420
544.778954	25222.360689	31.447437
545.468157	25265.738565	31.452455
545.812687	25292.397939	31.457472
546.204854	25336.251942	31.462490
546.477247	25372.231461	31.467508
546.793253	25408.387524	31.472525
547.101734	25453.809444	31.477543
547.585434	25497.548435	31.482560
548.017646	25545.081031	31.487578
548.620933	25581.224281	31.492596
549.652468	25625.484958	31.497613
550.369812	25680.525546	31.502631
550.576613	25713.596171	31.507648
550.892066	25759.655991	31.512666
551.536658	25798.257907	31.517684
552.269811	25846.117231	31.522701
552.488814	25887.136531	31.527719
553.722185	25923.232867	31.532736
554.206908	25960.463305	31.537754
554.886394	25990.996070	31.542772
555.486340	26024.656946	31.547789
555.835744	26061.744321	31.552807
556.333206	26087.218089	31.557824
557.141489	26124.322622	31.562842
557.758241	26158.019024	31.567860
558.092627	26184.447325	31.572877
558.685704	26230.793638	31.577895
559.278523	26259.450652	31.582912
559.688527	26300.896094	31.587930
560.353506	26337.347096	31.592948
560.556628	26366.659003	31.597965
561.233598	26415.982016	31.602983
561.763342	26447.189742	31.608000
562.476489	26485.441026	31.613018
563.146833	26525.108405	31.618036
563.768385	26570.882267	31.623053
564.267970	26608.863670	31.628071
564.996962	26636.438258	31.633088
565.447297	26679.944851	31.638106
565.942051	26723.526783	31.643124
566.559073	26753.741786	31.648141
566.770934	26794.726123	31.653159
567.322542	26838.583856	31.658176
567.978842	26873.166429	31.663194
568.437001	26918.821154	31.668212
569.487075	26958.145864	31.673229
570.061928	27011.019183	31.678247
570.364891	27043.135314	31.683264
571.594469	27085.339601	31.688282
571.715474	27128.721462	31.693300
572.692511	27161.396465	31.698317
573.143359	27198.558618	31.703335
573.949010	27240.001276	31.708352
574.008958	27278.880327	31.713370
574.844237	27314.851526	31.718388
575.582495	27346.262029	31.723405
575.999443	27399.173583	31.728423
576.649612	27428.082460	31.733440
577.281873	27460.457683	31.738458
577.764143	27496.718011	31.743476
578.605398	27534.698526	31.748493
579.252307	27577.215758	31.753511
580.016255	27598.630223	31.758528
580.483255	27635.664257	31.763546
581.184445	27673.331858	31.768564
581.676111	27704.319919	31.773581
582.038769	27749.498394	31.778599
582.263664	27774.093947	31.783616
583.245429	27819.062430	31.788634
583.596912	27849.958770	31.793652
584.197163	27883.622695	31.798669
584.619605	27927.085744	31.803687
585.341161	27963.265412	31.808704
585.987080	28000.095284	31.813722
586.155505	28041.221630	31.818740
586.701550	28080.039181	31.823757
587.511535	28132.430065	31.828775
588.173994	28164.264468	31.833792
588.559744	28203.138811	31.838810
589.159417	28252.775395	31.843828
589.963456	28290.510297	31.848845
590.349764	28337.917549	31.853863
591.110855	28376.493611	31.858880
591.555880	28413.608329	31.863898
592.039656	28462.144723	31.868916
592.749511	28498.643194	31.873933
593.592555	28529.110087	31.878951
594.007961	28565.262638	31.883968
594.515243	28607.727913	31.888986
594.540322	28646.077748	31.894004
595.450220	28675.061739	31.899021
595.830460	28723.058653	31.904039
596.242425	28755.602968	31.909056
596.841507	28806.473527	31.914074
597.645029	28857.950780	31.919092
598.599673	28882.756425	31.924109
599.036148	28927.148569	31.929127
599.723067	28977.430693	31.934144
600.688493	29020.975885	31.939162
600.935174	29054.974902	31.944180
601.916393	29093.947867	31.949197
602.230391	29134.314219	31.954215
602.846047	29169.646565	31.959232
603.521802	29203.711772	31.964250
604.066638	29254.263207	31.969268
604.729645	29285.334454	31.974285
605.188111	29322.846946	31.979303
605.700921	29371.033331	31.984320
606.563717	29416.542174	31.989338
606.925805	29470.245113	31.994356
607.461516	29507.139110	31.999373
608.345152	29554.484404	32.004391
608.959413	29587.719139	32.009408
609.930507	29635.025721	32.014426
610.183106	29683.999222	32.019444
611.036767	29721.033738	32.024461
611.687890	29768.207129	32.029479
611.977712	29809.387662	32.034496
612.616193	29846.278913	32.039514
612.926730	29888.461423	32.044532
613.451954	29947.007413	32.049549
614.103615	29993.978966	32.054567
615.024103	30044.189421	32.059584
616.105705	30085.057615	32.064602
616.623563	30127.707709	32.069620
617.182015	30174.251706	32.074637
617.718289	30214.364340	32.079655
617.731825	30250.310616	32.084672
618.612595	30292.341973	32.089690
619.574241	30349.860354	32.094708
620.134665	30391.404482	32.099725
620.629945	30439.159939	32.104743
621.220080	30486.439291	32.109760
622.353951	30521.421482	32.114778
623.181444	30558.183447	32.119796
624.077246	30593.348210	32.124813
624.681037	30626.624183	32.129831
625.296153	30669.614250	32.134848
626.065089	30699.217255	32.139866
626.567949	30737.629363	32.144884
627.104301	30768.425472	32.149901
627.586764	30807.991365	32.154919
628.189084	30835.445969	32.159936
628.916550	30879.645322	32.164954
629.405504	30919.311559	32.169972
629.914924	30952.552179	32.174989
630.859691	30999.796467	32.180007
631.276327	31034.088368	32.185024
632.285448	31074.369281	32.190042
632.245462	31118.562188	32.195060
632.836768	31150.285882	32.200077
633.799010	31196.472221	32.205095
633.983711	31227.216293	32.210112
634.697268	31268.845815	32.215130
635.002488	31308.452901	32.220148
635.894488	31345.547589	32.225165
636.242394	31385.299892	32.230183
636.397316	31430.600993	32.235200
637.269523	31464.860618	32.240218
637.841607	31532.702773	32.245236
638.621353	31561.148490	32.250253
638.952782	31605.145541	32.255271
639.626180	31654.690369	32.260288
640.630983	31701.983810	32.265306
641.690609	31751.734253	32.270324
641.953431	31782.713530	32.275341
642.788423	31832.941649	32.280359
643.138065	31879.964510	32.285376
643.923350	31921.811759	32.290394
644.464824	31965.397576	32.295412
644.974370	32019.046261	32.300429
645.644170	32068.757002	32.305447
645.747781	32123.676595	32.310464
647.092452	32176.095702	32.315482
647.578898	32230.519780	32.320500
648.385500	32281.853391	32.325517
649.170652	32321.223332	32.330535
649.662039	32369.420051	32.335552
650.420548	32410.646595	32.340570
650.936300	32467.133962	32.345588
651.435935	32511.492378	32.350605
652.513049	32564.756990	32.355623
653.250246	32611.120597	32.360640
653.813946	32660.893522	32.365658
654.629773	32709.906622	32.370676
655.281314	32762.555224	32.375693
656.369145	32794.431728	32.380711
656.974585	32833.836937	32.385728
658.158686	32875.105622	32.390746
658.417335	32923.908830	32.395764
659.065097	32967.423302	32.400781
659.722311	33000.397639	32.405799
660.324386	33048.053971	32.410816
661.052084	33083.040507	32.415834
661.155172	33133.240296	32.420852
661.803521	33178.171251	32.425869
662.892361	33227.825848	32.430887
663.360838	33284.404974	32.435904
664.067480	33318.870450	32.440922
664.768782	33368.737441	32.445940
665.234848	33403.784209	32.450957
666.337651	33450.415194	32.455975
666.362423	33501.418323	32.460992
667.419640	33548.777348	32.466010
668.010779	33596.493533	32.471028
668.190481	33649.097700	32.476045
668.887664	33693.086475	32.481063
669.560319	33752.695025	32.486080
670.755631	33803.213202	32.491098
670.935396	33855.482799	32.496116
671.754396	33899.800768	32.501133
672.170226	33955.397306	32.506151
673.085238	34014.349289	32.511168
674.235864	34051.174617	32.516186
674.954597	34091.980756	32.521204
675.522980	34147.313807	32.526221
676.531339	34186.810578	32.531239
676.891073	34224.928964	32.536256
677.721847	34270.832797	32.541274
678.441962	34315.761342	32.546292
678.766769	34364.791533	32.551309
679.307759	34408.907283	32.556327
679.755396	34448.087200	32.561344
680.278682	34488.387129	32.566362
680.845152	34534.503387	32.571380
681.476055	34589.170333	32.576397
682.130739	34634.223548	32.581415
682.812640	34683.799528	32.586432
684.267691	34719.219305	32.591450
685.381439	34756.620639	32.596468
685.600881	34792.808235	32.601485
686.761211	34839.104584	32.606503
687.109618	34884.269239	32.611520
687.874522	34921.156140	32.616538
688.420400	34963.697973	32.621556
688.936570	35008.204519	32.626573
689.764669	35043.273536	32.631591
690.718899	35091.492982	32.636608
691.586863	35127.668714	32.641626
691.919435	35177.293913	32.646644
692.214233	35212.642232	32.651661
693.043488	35265.364291	32.656679
693.616318	35314.275884	32.661696
694.438040	35365.355468	32.666714
695.034539	35419.460878	32.671732
695.415586	35473.555708	32.676749
696.508680	35520.237060	32.681767
696.499272	35573.798590	32.686784
697.447415	35629.759271	32.691802
698.344524	35685.961988	32.696820
698.959972	35740.786069	32.701837
700.208296	35796.068180	32.706855
700.743561	35840.826419	32.711872
701.401434	35887.355034	32.716890
702.076826	35944.946044	32.721908
702.978387	35989.717128	32.726925
703.742401	36035.375956	32.731943
704.909749	36089.944307	32.736960
705.219977	36139.499363	32.741978
705.637511	36190.770316	32.746996
706.316772	36243.012323	32.752013
707.274114	36293.111942	32.757031
707.838317	36344.999056	32.762048
708.818993	36397.972251	32.767066
709.562690	36450.438688	32.772084
709.653813	36504.050142	32.777101
710.406335	36552.380192	32.782119
711.290655	36606.627194	32.787136
711.919351	36657.341585	32.792154
712.642538	36716.330970	32.797172
713.140202	36769.683789	32.802189
714.403013	36828.987840	32.807207
714.546155	36887.701252	32.812224
715.467415	36945.939599	32.817242
716.180539	37001.712848	32.822260
717.002471	37056.647289	32.827277
717.736322	37117.292801	32.832295
718.503071	37174.114131	32.837312
718.849832	37217.760105	32.842330
720.085964	37275.178900	32.847348
720.407846	37332.139457	32.852365
721.436096	37378.866609	32.857383
722.611992	37445.078297	32.862400
723.386986	37494.456655	32.867418
724.191060	37539.714103	32.872436
724.547352	37594.981672	32.877453
725.384313	37633.227918	32.882471
726.014896	37689.483741	32.887488
726.896549	37729.272432	32.892506
727.360879	37765.104473	32.897524
727.765745	37818.657736	32.902541
728.326735	37855.442365	32.907559
729.144205	37911.688650	32.912576
729.783908	37958.736816	32.917594
730.756766	38004.632937	32.922612
731.146878	38062.621867	32.927629
732.069754	38107.071584	32.932647
732.982185	38162.772571	32.937664
733.525613	38201.046555	32.942682
734.175194	38258.388562	32.947700
734.964054	38317.871703	32.952717
735.422573	38364.506313	32.957735
736.432723	38421.008500	32.962752
737.503755	38477.343268	32.967770
738.027638	38519.136795	32.972788
738.423352	38587.610851	32.977805
739.505364	38631.872468	32.982823
739.946885	38698.588092	32.987840
741.106382	38736.931544	32.992858
742.113468	38791.474837	32.997876
742.111223	38844.012675	33.002893
743.223684	38895.611944	33.007911
743.976600	38966.371383	33.012928
744.587281	39018.814233	33.017946
745.192127	39075.210489	33.022964
745.765113	39140.218561	33.027981
746.906694	39197.094403	33.032999
747.616639	39269.334976	33.038016
748.467560	39319.540460	33.043034
749.528673	39377.194491	33.048052
749.905635	39438.831727	33.053069
750.615351	39495.257023	33.058087
751.239854	39552.479899	33.063104
752.020105	39617.318014	33.068122
753.046048	39678.013820	33.073140
753.550614	39742.661239	33.078157
754.623935	39805.550776	33.083175
755.091607	39865.290551	33.088192
756.122350	39922.210852	33.093210
757.002200	39972.109793	33.098228
757.707123	40038.390132	33.103245
758.406986	40104.715729	33.108263
759.048005	40158.984284	33.113280
759.985515	40222.054274	33.118298
761.020595	40270.140009	33.123316
761.640250	40328.339606	33.128333
762.143312	40388.321953	33.133351
762.822690	40440.106162	33.138368
763.645473	40510.480319	33.143386
764.724825	40569.146559	33.148404
764.825099	40627.472076	33.153421
765.768111	40694.609072	33.158439
766.674755	40760.069677	33.163456
767.169807	40822.805533	33.168474
768.114197	40874.555846	33.173492
768.909616	40951.449737	33.178509
769.995821	41000.332321	33.183527
771.002047	41056.266488	33.188544
771.723900	41114.958228	33.193562
772.524312	41170.102555	33.198580
773.231217	41239.187954	33.203597
774.066667	41284.321880	33.208615
774.679121	41348.862410	33.213632
775.124900	41412.170506	33.218650
776.658492	41461.800339	33.223668
776.977461	41525.008337	33.228685
778.141355	41570.243515	33.233703
778.462836	41617.924702	33.238720
779.194221	41665.118439	33.243738
780.415126	41707.676069	33.248756
780.563028	41759.350083	33.253773
781.690423	41815.640484	33.258791
782.532760	41857.801966	33.263808
783.132370	41915.914049	33.268826
784.030710	41961.260946	33.273844
784.649198	42024.524954	33.278861
785.674595	42075.519196	33.283879
786.496937	42118.240864	33.288896
787.006517	42170.688078	33.293914
787.750520	42219.310426	33.298932
788.615667	42275.320272	33.303949
789.375238	42339.151424	33.308967
790.225156	42392.602421	33.313984
790.977169	42450.970486	33.319002
791.927029	42502.103975	33.324020
792.469433	42558.860511	33.329037
793.169130	42611.627047	33.334055
794.193632	42670.509862	33.339072
794.742422	42731.667936	33.344090
795.639221	42784.714123	33.349108
796.697776	42849.094751	33.354125
797.476973	42912.348947	33.359143
798.350625	42971.173825	33.364160
799.053926	43027.931824	33.369178
799.904624	43089.992636	33.374196
800.437137	43158.643178	33.379213
801.123530	43209.762399	33.384231
802.193008	43277.026773	33.389248
802.918696	43337.305113	33.394266
803.734509	43394.520917	33.399284
804.268691	43451.274705	33.404301
805.334556	43515.934446	33.409319
806.529636	43584.097340	33.414336
806.933479	43653.781463	33.419354
807.801136	43717.821161	33.424372
808.214811	43771.495213	33.429389
809.615167	43838.867920	33.434407
810.603558	43894.002473	33.439424
811.431563	43964.228763	33.444442
812.133914	44032.425463	33.449460
812.887375	44087.862728	33.454477
813.678261	44141.820521	33.459495
814.260579	44207.904834	33.464512
815.284387	44275.059171	33.469530
816.270061	44326.248239	33.474548
816.979205	44390.763653	33.479565
818.043618	44455.040517	33.484583
818.826433	44521.967451	33.489600
819.292799	44581.005493	33.494618
820.114127	44643.214389	33.499636
821.097504	44706.770848	33.504653
821.490050	44765.650085	33.509671
822.558314	44833.646798	33.514688
823.685152	44912.583995	33.519706
824.005290	44958.178867	33.524724
824.857658	45033.863641	33.529741
825.594482	45097.149644	33.534759
826.557786	45166.156819	33.539776
827.156849	45240.667220	33.544794
828.465826	45296.925579	33.549812
829.223033	45370.747610	33.554829
829.635059	45436.615377	33.559847
830.776746	45500.744066	33.564864
831.693904	45562.978564	33.569882
832.695489	45627.572221	33.574900
833.272407	45681.623983	33.579917
834.266176	45725.394972	33.584935
836.149220	45760.196918	33.589952
836.625444	45812.695895	33.594970
837.527830	45853.470313	33.599988
838.482502	45911.113779	33.605005
839.120150	45960.026572	33.610023
840.010357	46004.585973	33.615040
840.098098	46056.968872	33.620058
840.803144	46106.693847	33.625076
841.896024	46159.578406	33.630093
842.713526	46219.983103	33.635111
843.304028	46283.832937	33.640128
844.022752	46349.136923	33.645146
844.946962	46399.543256	33.650164
845.810438	46455.994073	33.655181
846.481433	46518.079766	33.660199
847.305274	46587.302808	33.665216
848.011456	46660.985208	33.670234
848.896124	46722.715580	33.675252
850.019050	46797.136953	33.680269
851.056529	46861.804490	33.685287
852.647084	46903.878072	33.690304
853.216555	46966.512192	33.695322
854.533513	47021.116216	33.700340
855.539387	47081.240861	33.705357
856.015384	47129.574058	33.710375
856.628230	47184.009733	33.715392
857.486096	47245.353491	33.720410
858.282099	47314.133944	33.725428
859.052964	47382.557929	33.730445
859.515735	47441.483862	33.735463
860.569722	47509.288475	33.740480
861.148627	47577.135613	33.745498
862.245130	47644.042015	33.750516
863.244595	47697.754490	33.755533
864.139403	47770.677303	33.760551
865.388540	47833.189047	33.765568
865.996692	47895.357900	33.770586
866.648164	47954.578436	33.775604
867.821333	48020.569352	33.780621
868.121637	48084.747812	33.785639
869.251462	48153.757213	33.790656
870.453964	48233.213058	33.795674
871.341607	48285.773949	33.800692
872.258863	48351.217306	33.805709
873.157999	48415.999394	33.810727
874.176694	48478.150221	33.815744
874.780500	48548.640855	33.820762
875.424337	48599.159006	33.825780
876.240872	48676.386286	33.830797
877.461663	48740.815556	33.835815
878.063729	48813.091366	33.840832
878.889643	48873.729600	33.845850
879.852901	48946.386143	33.850868
880.672610	49014.301314	33.855885
881.396116	49092.221433	33.860903
882.748799	49153.455364	33.865920
883.403364	49232.360999	33.870938
884.002935	49298.077962	33.875956
884.779553	49357.358588	33.880973
885.524495	49438.794207	33.885991
886.831461	49500.959892	33.891008
887.327366	49580.030612	33.896026
888.166878	49653.043984	33.901044
889.220739	49729.579895	33.906061
889.973406	49805.473322	33.911079
890.788189	49874.745759	33.916096
891.419590	49950.677523	33.921114
892.404564	50009.649022	33.926132
893.524585	50084.397961	33.931149
894.090061	50148.408076	33.936167
894.949411	50217.003954	33.941184
895.672216	50302.020815	33.946202
896.737799	50358.633353	33.951220
897.511176	50437.379119	33.956237
898.252212	50517.288036	33.961255
899.245867	50586.439871	33.966272
900.024726	50672.702132	33.971290
901.181918	50744.024480	33.976308
902.580420	50809.627734	33.981325
903.324709	50888.651637	33.986343
904.388106	50956.161323	33.991360
905.011683	51027.232273	33.996378
906.307607	51107.031550	34.001396
907.340962	51179.715890	34.006413
908.163489	51244.815282	34.011431
909.548048	51310.934640	34.016448
910.323933	51379.622899	34.021466
911.097098	51446.888145	34.026484
912.051981	51516.884007	34.031501
912.847451	51584.627057	34.036519
914.104155	51653.260265	34.041536
915.025245	51723.907403	34.046554
915.649492	51791.994080	34.051572
916.964458	51848.881501	34.056589
917.440209	51925.502042	34.061607
918.909724	51993.128708	34.066624
919.584305	52058.019301	34.071642
920.663546	52124.504884	34.076660
921.596144	52200.106096	34.081677
922.218101	52276.679727	34.086695
923.135520	52332.427989	34.091712
924.051308	52420.636984	34.096730
925.154559	52485.518991	34.101748
926.348544	52552.253695	34.106765
927.042173	52632.335481	34.111783
927.855561	52695.282650	34.116800
928.586714	52773.308926	34.121818
929.632099	52850.514573	34.126836
931.161877	52919.298847	34.131853
931.749427	52984.901617	34.136871
932.900664	53060.370345	34.141888
933.627341	53136.228119	34.146906
934.579350	53201.901322	34.151924
936.030297	53272.584584	34.156941
936.553754	53335.895001	34.161959
937.315304	53403.427152	34.166976
938.326953	53481.228623	34.171994
939.491007	53550.464013	34.177012
940.191541	53617.696215	34.182029
941.329719	53700.927026	34.187047
942.038210	53761.273643	34.192064
943.041214	53837.097003	34.197082
943.967929	53907.085448	34.202100
945.521756	53967.933807	34.207117
946.359949	54033.380267	34.212135
947.626988	54094.672261	34.217152
948.371334	54162.354820	34.222170
949.194748	54231.626262	34.227188
950.038029	54290.795226	34.232205
950.766957	54366.150384	34.237223
951.480106	54428.845709	34.242240
952.623651	54490.746473	34.247258
953.239732	54574.991885	34.252276
954.389014	54637.461673	34.257293
954.890601	54711.986368	34.262311
955.852657	54775.814584	34.267328
956.708587	54840.659349	34.272346
957.602683	54909.042159	34.277364
958.317806	54983.300326	34.282381
960.020336	55042.812046	34.287399
961.128823	55106.662662	34.292416
961.855686	55171.636008	34.297434
962.407545	55249.995851	34.302452
963.650101	55319.249541	34.307469
964.370326	55396.659724	34.312487
965.187771	55455.683751	34.317504
966.024497	55541.847401	34.322522
966.906819	55620.555718	34.327540
968.324134	55692.877895	34.332557
968.929292	55771.167880	34.337575
969.779779	55840.579051	34.342592
970.862158	55928.420884	34.347610
971.761250	56007.558212	34.352628
973.162619	56089.946432	34.357645
973.859978	56185.253541	34.362663
974.895343	56252.093052	34.367680
975.801161	56337.141329	34.372698
976.946238	56416.026553	34.377716
978.309437	56492.814945	34.382733
978.933899	56575.502982	34.387751
979.922926	56654.774021	34.392768
980.762692	56738.429041	34.397786
981.893129	56822.608695	34.402804
982.838064	56907.216232	34.407821
984.082381	56995.119064	34.412839
985.052592	57074.286835	34.417856
986.139786	57150.101368	34.422874
986.779249	57235.909464	34.427892
988.061874	57318.105230	34.432909
989.367815	57392.766272	34.437927
990.961184	57470.610550	34.442944
991.840232	57533.345203	34.447962
992.578920	57610.557175	34.452980
994.055997	57684.844397	34.457997
994.949124	57757.672146	34.463015
995.435392	57820.544638	34.468032
996.562559	57908.437412	34.473050
997.554712	57982.073200	34.478068
998.364372	58065.117291	34.483085
999.090203	58148.339273	34.488103
1000.849914	58223.489226	34.493120
1001.435133	58300.645024	34.498138
1002.147968	58386.262260	34.503156
1003.873979	58464.449874	34.508173
1004.404592	58540.893414	34.513191
1005.362043	58621.745506	34.518208
1006.341974	58696.727173	34.523226
1007.299975	58779.934182	34.528244
1008.586467	58856.824365	34.533261
1009.355759	58939.960031	34.538279
1010.598935	59025.775470	34.543296
1011.811840	59103.861476	34.548314
1012.232650	59185.216720	34.553332
1013.523186	59256.664299	34.558349
1014.386059	59348.527669	34.563367
1015.872124	59409.476438	34.568384
1017.444079	59482.064477	34.573402
1018.440707	59554.273909	34.578420
1019.292973	59614.568646	34.583437
1020.121128	59702.046108	34.588455
1021.419905	59772.582477	34.593472
1022.195443	59834.313843	34.598490
1022.902236	59899.106905	34.603508
1024.060075	59966.361755	34.608525
1025.030717	60048.520441	34.613543
1025.789882	60115.540270	34.618560
1026.307308	60178.971041	34.623578
1027.471521	60259.720452	34.628596
1028.470323	60324.253984	34.633613
1029.214888	60405.467968	34.638631
1030.139985	60479.121785	34.643648
1030.830866	60565.060277	34.648666
1031.818208	60650.832660	34.653684
1033.232642	60730.753464	34.658701
1034.074668	60824.119466	34.663719
1035.170626	60909.179571	34.668736
1036.028781	60987.915514	34.673754
1037.392893	61081.777245	34.678772
1038.337737	61170.571072	34.683789
1039.349711	61261.709492	34.688807
1040.388418	61348.792941	34.693824
1041.516836	61436.875526	34.698842
1042.890071	61522.451633	34.703860
1043.860539	61612.458422	34.708877
1044.383123	61706.915623	34.713895
1045.426010	61785.264556	34.718912
1046.884740	61877.747315	34.723930
1047.494528	61989.397115	34.728948
1049.019266	62071.463675	34.733965
1049.864247	62167.227097	34.738983
1050.899966	62268.993836	34.744000
1052.308662	62356.384076	34.749018
1053.623744	62447.593646	34.754036
1054.531963	62541.500257	34.759053
1055.761674	62629.932160	34.764071
1056.917058	62714.103019	34.769088
1057.777466	62798.415032	34.774106
1058.873605	62882.962843	34.779124
1060.249057	62974.240922	34.784141
1061.432528	63055.990382	34.789159
1062.231576	63141.490560	34.794176
1063.345155	63233.740921	34.799194
1064.226085	63332.060731	34.804212
1065.523228	63409.052173	34.809229
1066.331793	63506.915486	34.814247
1067.621434	63594.214675	34.819264
1068.875101	63677.867063	34.824282
1069.888844	63767.950918	34.829300
1071.224270	63848.793058	34.834317
1072.493388	63935.533219	34.839335
1073.649667	64006.091245	34.844352
1074.715929	64086.995047	34.849370
1075.829514	64173.798229	34.854388
1077.029550	64243.666408	34.859405
1077.499841	64335.926021	34.864423
1079.042388	64416.801068	34.869440
1080.057791	64506.254258	34.874458
1081.030721	64592.586991	34.879476
1082.119834	64675.135132	34.884493
1083.261482	64756.168640	34.889511
1084.344743	64835.837714	34.894528
1085.337992	64909.076273	34.899546
1086.436173	65005.760823	34.904564
1087.567883	65079.225229	34.909581
1088.021176	65172.883355	34.914599
1089.368419	65259.995796	34.919616
1090.516249	65337.776131	34.924634
1091.648082	65427.372753	34.929652
1092.803857	65513.350979	34.934669
1093.687223	65599.777085	34.939687
1094.719471	65676.753428	34.944704
1095.796914	65757.021441	34.949722
1096.984461	65835.366922	34.954740
1097.864304	65905.245248	34.959757
1098.702446	65986.779468	34.964775
1099.982439	66068.897279	34.969792
1101.335870	66150.250521	34.974810
1102.189097	66230.434647	34.979828
1103.251699	66291.054769	34.984845
1104.693710	66386.076643	34.989863
1105.693649	66463.338983	34.994880
1107.262682	66538.537632	34.999898
1107.906597	66618.875861	35.004916
1109.115196	66707.262133	35.009933
1110.196569	66779.833951	35.014951
1110.766654	66870.776722	35.019968
1112.288844	66958.102044	35.024986
1113.526207	67050.467444	35.030004
1114.866999	67111.742676	35.035021
1116.582852	67195.113217	35.040039
1117.163720	67271.404897	35.045056
1118.922385	67359.435565	35.050074
1119.237688	67441.752298	35.055092
1120.656815	67522.194313	35.060109
1121.869723	67614.590891	35.065127
1122.721933	67693.988353	35.070144
1123.927879	67780.137405	35.075162
1124.557921	67863.843766	35.080180
1125.300794	67954.807825	35.085197
1126.600210	68047.002552	35.090215
1127.845504	68151.198142	35.095232
1129.242026	68246.898860	35.100250
1130.312746	68347.456394	35.105268
1131.285308	68443.648061	35.110285
1132.278491	68533.847065	35.115303
1133.609435	68634.422202	35.120320
1134.736648	68726.475218	35.125338
1136.043736	68831.392103	35.130356
1136.887799	68924.205393	35.135373
1138.228128	69016.821466	35.140391
1139.264565	69116.855468	35.145408
1140.473836	69206.022757	35.150426
1141.482850	69313.223157	35.155444
1143.057856	69408.013945	35.160461
1144.313176	69503.981932	35.165479
1145.601038	69596.342309	35.170496
1146.858516	69679.861931	35.175514
1147.961619	69779.894455	35.180532
1149.417729	69862.446609	35.185549
1150.627084	69941.263520	35.190567
1151.692655	70034.312264	35.195584
1152.967382	70114.360616	35.200602
1154.447404	70205.040572	35.205620
1155.351987	70289.592238	35.210637
1156.551767	70376.029545	35.215655
1157.278661	70472.134025	35.220672
1158.676044	70555.375070	35.225690
1159.378489	70662.141184	35.230708
1160.575220	70743.982977	35.235725
1162.205827	70835.344574	35.240743
1162.952992	70919.321221	35.245760
1163.909779	71007.862779	35.250778
1164.984261	71105.162957	35.255796
1166.461400	71191.053207	35.260813
1167.221077	71297.749687	35.265831
1168.459649	71400.458622	35.270848
1169.662010	71499.095499	35.275866
1170.500276	71586.188335	35.280884
1171.688890	71675.810583	35.285901
1172.683264	71758.472280	35.290919
1173.269649	71852.887595	35.295936
1174.634785	71946.270146	35.300954
1175.822726	72039.009356	35.305972
1176.967321	72136.353109	35.310989
1178.476230	72230.676848	35.316007
1179.081375	72335.324496	35.321024
1180.428968	72425.190526	35.326042
1182.045602	72530.226116	35.331060
1183.003960	72630.868356	35.336077
1184.335487	72718.964726	35.341095
1185.198424	72819.609873	35.346112
1186.719141	72917.100612	35.351130
1187.579991	73023.661685	35.356148
1188.876754	73124.177136	35.361165
1190.456906	73227.093342	35.366183
1191.375191	73328.010452	35.371200
1192.911977	73426.564493	35.376218
1193.846676	73532.508156	35.381236
1195.136433	73631.646042	35.386253
1196.160747	73735.499356	35.391271
1197.687662	73850.002961	35.396288
1198.778088	73943.751981	35.401306
1199.817469	74054.481869	35.406324
1201.205142	74150.895899	35.411341
1202.594886	74256.087641	35.416359
1203.450149	74363.655585	35.421376
1205.117998	74465.106314	35.426394
1206.850329	74567.028714	35.431412
1207.823890	74677.074779	35.436429
1209.100194	74773.217065	35.441447
1210.365963	74871.957969	35.446464
1211.794221	74972.485263	35.451482
1212.892194	75074.090338	35.456500
1213.832358	75174.035696	35.461517
1215.405014	75284.193670	35.466535
1216.544101	75379.713487	35.471552
1217.570560	75467.904437	35.476570
1219.048954	75564.144770	35.481588
1220.449557	75670.670394	35.486605
1221.846027	75770.002266	35.491623
1222.822605	75872.452604	35.496640
1223.728198	75972.849654	35.501658
1225.237908	76062.449373	35.506676
1226.396396	76173.891491	35.511693
1228.161557	76272.027785	35.516711
1228.750379	76373.970357	35.521728
1230.131920	76469.316955	35.526746
1231.857613	76566.485082	35.531764
1233.699721	76647.991270	35.536781
1235.384983	76725.899248	35.541799
1236.449525	76811.656524	35.546816
1237.629970	76888.782162	35.551834
1238.919928	76979.521193	35.556852
1239.541329	77061.522651	35.561869
1241.122447	77150.456146	35.566887
1242.195310	77238.556975	35.571904
1243.324630	77330.284919	35.576922
1244.585392	77417.571686	35.581940
1245.855120	77517.474406	35.586957
1246.484625	77602.237798	35.591975
1247.930217	77705.622809	35.596992
1248.819353	77806.928619	35.602010
1250.140843	77896.246993	35.607028
1250.748021	78001.182430	35.612045
1252.184902	78101.415971	35.617063
1252.954415	78202.057790	35.622080
1254.276299	78300.967146	35.627098
1255.624633	78393.868040	35.632116
1256.829633	78495.659293	35.637133
1258.170618	78586.953124	35.642151
1259.114766	78690.141202	35.647168
1259.979139	78788.616796	35.652186
1261.404410	78885.979300	35.657204
1262.699927	78993.446408	35.662221
1264.120074	79086.477818	35.667239
1265.291030	79188.517634	35.672256
1266.367725	79297.616221	35.677274
1267.515472	79405.247288	35.682292
1268.735116	79519.619981	35.687309
1270.745910	79627.434296	35.692327
1271.765817	79746.957179	35.697344
1273.120473	79845.955663	35.702362
1274.357598	79950.813139	35.707380
1275.493532	80061.527130	35.712397
1277.203112	80171.100750	35.717415
1278.252312	80292.319063	35.722432
1279.496218	80390.563918	35.727450
1280.968875	80497.097119	35.732468
1282.091272	80611.742832	35.737485
1283.729504	80721.773148	35.742503
1285.265790	80827.562895	35.747520
1286.895096	80924.964153	35.752538
1288.563765	81025.818358	35.757556
1289.715481	81130.516201	35.762573
1291.386182	81218.752069	35.767591
1292.622244	81319.953399	35.772608
1293.670415	81417.598863	35.777626
1295.430348	81513.246115	35.782644
1296.775372	81606.044264	35.787661
1297.988368	81705.704884	35.792679
1299.038592	81803.604766	35.797696
1300.335341	81906.547185	35.802714
1302.063994	82007.243551	35.807732
1302.734459	82104.240684	35.812749
1304.101973	82202.916109	35.817767
1305.115015	82308.146725	35.822784
1306.473548	82410.625253	35.827802
1307.904719	82514.524560	35.832820
1308.856722	82628.748918	35.837837
1310.447516	82737.337466	35.842855
1311.731868	82847.165125	35.847872
1313.194341	82944.890771	35.852890
1314.537831	83046.170275	35.857908
1315.410151	83157.228933	35.862925
1316.955602	83264.559530	35.867943
1318.377118	83381.475980	35.872960
1319.590448	83488.922472	35.877978
1320.923528	83594.766919	35.882996
1322.117421	83708.856611	35.888013
1323.249880	83811.616134	35.893031
1324.600343	83928.773963	35.898048
1325.875505	84044.271461	35.903066
1327.486106	84157.411138	35.908084
1328.483112	84274.752109	35.913101
1329.996043	84378.936938	35.918119
1331.356153	84503.140614	35.923136
1332.479502	84620.361969	35.928154
1334.060652	84729.276393	35.933172
1334.826812	84842.905005	35.938189
1336.555399	84964.151653	35.943207
1338.179098	85084.832265	35.948224
1338.982543	85195.770181	35.953242
1340.484894	85311.820300	35.958260
1341.576305	85420.319391	35.963277
1342.957554	85519.625060	35.968295
1344.171767	85635.518588	35.973312
1345.370983	85746.574421	35.978330
1346.831027	85846.236421	35.983348
1347.936422	85962.122854	35.988365
1349.376500	86075.081204	35.993383
1350.739749	86179.093103	35.998400
1351.902349	86292.906477	36.003418
1353.579202	86397.035078	36.008436
1355.072001	86507.896073	36.013453
1356.520793	86624.187886	36.018471
1357.570628	86734.282350	36.023488
1358.965659	86842.397368	36.028506
1360.591007	86939.084836	36.033524
1362.093998	87058.069075	36.038541
1363.245664	87170.658399	36.043559
1364.675683	87291.492399	36.048576
1365.936479	87419.056819	36.053594
1367.555766	87526.695941	36.058612
1368.387147	87646.129260	36.063629
1370.172735	87756.822708	36.068647
1371.384966	87887.792911	36.073664
1372.810840	88004.131802	36.078682
1374.157866	88124.576637	36.083700
1375.529785	88243.877563	36.088717
1376.972423	88367.628715	36.093735
1378.783690	88486.507409	36.098752
1379.864840	88604.790553	36.103770
1381.393241	88720.596736	36.108788
1382.820245	88839.992883	36.113805
1384.372628	88947.470201	36.118823
1385.924041	89078.430921	36.123840
1387.463366	89199.597915	36.128858
1388.683177	89314.770117	36.133876
1390.462568	89434.367272	36.138893
1391.783222	89541.109758	36.143911
1393.236437	89655.575280	36.148928
1394.050042	89780.672216	36.153946
1396.002554	89897.532228	36.158964
1397.678806	90016.983029	36.163981
1398.998425	90126.325799	36.168999
1400.397758	90241.080772	36.174016
1401.192436	90369.668305	36.179034
1402.658071	90483.970320	36.184052
1403.537085	90607.007432	36.189069
1405.383391	90728.183557	36.194087
1406.742532	90859.296094	36.199104
1408.046591	90980.950523	36.204122
1409.521988	91104.239038	36.209140
1410.780810	91236.788297	36.214157
1412.323276	91359.395707	36.219175
1414.162951	91480.233704	36.224192
1415.532169	91608.534331	36.229210
1417.238628	91731.612015	36.234228
1418.488350	91851.909626	36.239245
1419.937984	91972.227296	36.244263
1421.192803	92087.962371	36.249280
1422.480680	92220.663516	36.254298
1424.095239	92336.571684	36.259316
1425.519671	92449.277938	36.264333
1426.807656	92576.226484	36.269351
1428.218278	92697.655774	36.274368
1429.341724	92839.092539	36.279386
1430.816803	92952.591267	36.284404
1432.590139	93090.683370	36.289421
1434.409063	93206.930609	36.294439
1435.885096	93323.763997	36.299456
1436.771118	93440.423496	36.304474
1438.374245	93553.182067	36.309492
1439.526493	93660.383612	36.314509
1440.442870	93771.031783	36.319527
1442.375211	93880.546253	36.324544
1443.433343	93998.258453	36.329562
1445.178419	94108.740831	36.334580
1446.353917	94223.761202	36.339597
1447.697091	94343.496389	36.344615
1449.163733	94465.976007	36.349632
1450.486024	94593.510633	36.354650
1452.049216	94708.459793	36.359668
1453.194141	94843.818337	36.364685
1454.775594	94970.933924	36.369703
1456.229968	95095.674160	36.374720
1457.514350	95231.545059	36.379738
1459.315889	95359.794128	36.384756
1460.852630	95489.479254	36.389773
1462.188113	95617.916008	36.394791
1463.660904	95742.098248	36.399808
1464.929042	95883.006762	36.404826
1466.559159	96018.459689	36.409844
1468.132254	96161.223362	36.414861
1469.836100	96286.601363	36.419879
1471.353379	96417.928569	36.424896
1472.866313	96551.513330	36.429914
1474.073130	96679.150535	36.434932
1475.799432	96811.384885	36.439949
1476.850590	96958.492597	36.444967
1478.781326	97089.606148	36.449984
1480.328538	97228.804017	36.455002
1481.814277	97352.344136	36.460020
1483.505027	97483.496680	36.465037
1484.552799	97622.824728	36.470055
1486.322287	97758.859261	36.475072
1487.796635	97899.250339	36.480090
1489.239270	98041.092107	36.485108
1490.731119	98175.802572	36.490125
1492.435395	98308.046619	36.495143
1493.966233	98437.161700	36.500160
1495.557270	98577.220695	36.505178
1497.471277	98714.187591	36.510196
1498.892441	98845.730002	36.515213
1500.693953	98963.624052	36.520231
1502.006494	99088.998016	36.525248
1503.596681	99226.587977	36.530266
1505.349704	99358.879504	36.535284
1506.674516	99487.333658	36.540301
1508.041828	99627.685622	36.545319
1509.518493	99747.420607	36.550336
1510.962944	99887.685636	36.555354
1512.592296	100014.268962	36.560372
1514.011382	100155.363134	36.565389
1515.712348	100289.479467	36.570407
1517.286157	100415.274330	36.575424
1518.441822	100547.181972	36.580442
1520.223623	100680.754888	36.585460
1521.966520	100821.979058	36.590477
1523.462711	100936.466852	36.595495
1525.491703	101064.931785	36.600512
1527.010784	101204.316142	36.605530
1528.515069	101320.781774	36.610548
1529.560370	101438.003869	36.615565
1531.060019	101568.949311	36.620583
1532.476264	101698.348862	36.625600
1533.318175	101835.254996	36.630618
1535.107897	101968.768578	36.635636
1536.959936	102103.857780	36.640653
1538.506245	102232.896891	36.645671
1539.799172	102351.947422	36.650688
1540.940715	102486.540226	36.655706
1542.174101	102598.095342	36.660724
1543.682242	102725.177178	36.665741
1544.968645	102863.806076	36.670759
1546.932981	102986.811518	36.675776
1548.047875	103122.678922	36.680794
1549.308791	103257.218258	36.685812
1551.053751	103394.421398	36.690829
1552.649411	103529.645104	36.695847
1554.432510	103657.816140	36.700864
1555.491700	103810.862116	36.705882
1557.268916	103955.162709	36.710900
1559.037604	104097.170365	36.715917
1560.305722	104234.248330	36.720935
1561.943191	104378.610545	36.725952
1563.304519	104531.308506	36.730970
1565.450243	104664.904359	36.735988
1567.058941	104807.028690	36.741005
1568.529079	104950.214891	36.746023
1570.552421	105096.105054	36.751040
1571.800843	105254.212597	36.756058
1573.516563	105390.870607	36.761076
1574.972810	105526.618594	36.766093
1576.182241	105680.930361	36.771111
1578.134878	105828.838073	36.776128
1579.915120	105988.616071	36.781146
1581.493028	106135.708553	36.786164
1583.216512	106272.521079	36.791181
1584.611978	106423.586615	36.796199
1586.076870	106585.293121	36.801216
1587.908598	106738.308257	36.806234
1589.443948	106886.222129	36.811252
1590.971916	107037.726247	36.816269
1592.434364	107206.574953	36.821287
1594.347232	107341.308118	36.826304
1595.432063	107505.994579	36.831322
1597.541455	107654.393039	36.836340
1599.556881	107807.257566	36.841357
1600.723172	107957.275042	36.846375
1602.426609	108111.698448	36.851392
1603.973360	108272.804201	36.856410
1605.879208	108425.257390	36.861428
1607.380045	108573.564322	36.866445
1608.973678	108731.456720	36.871463
1610.926166	108890.245040	36.876480
1612.592085	109041.482893	36.881498
1614.548100	109170.459415	36.886516
1616.474359	109321.505798	36.891533
1617.718747	109479.253059	36.896551
1619.437588	109610.931128	36.901568
1620.773244	109763.681836	36.906586
1622.400525	109903.617946	36.911604
1624.314894	110053.616817	36.916621
1626.395098	110183.909280	36.921639
1628.081501	110322.455611	36.926656
1629.810865	110466.879929	36.931674
1631.406800	110605.466820	36.936692
1633.183767	110736.176288	36.941709
1634.424554	110882.390344	36.946727
1636.109659	111018.073605	36.951744
1637.419398	111159.129383	36.956762
1638.855116	111310.209950	36.961780
1640.581230	111455.298264	36.966797
1642.206258	111594.480543	36.971815
1643.747898	111734.145572	36.976832
1645.806611	111886.298350	36.981850
1647.274113	112023.059234	36.986868
1648.982310	112154.583597	36.991885
1649.853387	112294.126913	36.996903
1651.257249	112418.191893	37.001920
1652.947745	112562.351791	37.006938
1654.494216	112691.671259	37.011956
1656.323912	112821.200755	37.016973
1657.241585	112974.055724	37.021991
1658.893768	113115.662004	37.027008
1660.322938	113276.720160	37.032026
1662.145090	113426.189603	37.037044
1663.555585	113577.245626	37.042061
1665.320636	113742.299272	37.047079
1666.525826	113899.374720	37.052096
1668.367402	114076.910270	37.057114
1669.807289	114239.949528	37.062132
1671.821816	114400.452318	37.067149
1672.969170	114575.891563	37.072167
1674.636653	114741.903459	37.077184
1676.271314	114924.459692	37.082202
1678.237239	115104.733080	37.087220
1680.055303	115269.189294	37.092237
1681.893134	115451.031647	37.097255
1683.542803	115632.143196	37.102272
1685.397645	115802.874222	37.107290
1686.739153	115977.186509	37.112308
1689.082646	116157.609222	37.117325
1690.601147	116336.994347	37.122343
1692.184173	116514.061913	37.127360
1694.059298	116688.357910	37.132378
1696.029454	116868.728038	37.137396
1698.252032	117038.215266	37.142413
1699.717813	117208.975265	37.147431
1701.269094	117385.037218	37.152448
1703.239312	117562.848577	37.157466
1704.654382	117732.528051	37.162484
1706.556694	117910.453096	37.167501
1707.834686	118094.437614	37.172519
1709.827264	118275.939899	37.177536
1711.169305	118451.696944	37.182554
1712.860671	118629.239636	37.187572
1714.948352	118806.848321	37.192589
1716.173876	119004.075054	37.197607
1718.033907	119194.379884	37.202624
1719.566235	119375.895647	37.207642
1721.490713	119567.980811	37.212660
1723.085675	119754.029658	37.217677
1724.518028	119945.482979	37.222695
1726.363992	120130.898414	37.227712
1728.503472	120343.579236	37.232730
1729.749614	120529.927141	37.237748
1731.795409	120727.884963	37.242765
1733.383669	120906.392948	37.247783
1735.368781	121098.197251	37.252800
1737.432260	121294.100253	37.257818
1738.623321	121485.979317	37.262836
1740.734153	121675.623124	37.267853
1742.520089	121873.208621	37.272871
1744.245116	122062.457687	37.277888
1745.829089	122248.025504	37.282906
1747.544994	122449.544578	37.287924
1749.561466	122637.127326	37.292941
1751.476453	122807.855028	37.297959
1753.305549	122999.084035	37.302976
1755.360784	123180.396663	37.307994
1756.964523	123373.184829	37.313012
1759.430271	123550.109438	37.318029
1761.177421	123727.755596	37.323047
1762.893089	123896.831804	37.328064
1764.608629	124051.966932	37.333082
1766.080746	124214.549150	37.338100
1767.993814	124365.303468	37.343117
1769.634397	124527.733880	37.348135
1770.893964	124689.513828	37.353152
1772.329939	124859.373430	37.358170
1773.939511	125035.181940	37.363188
1775.542342	125212.857149	37.368205
1776.580199	125393.868772	37.373223
1778.209899	125584.684476	37.378240
1780.311208	125772.700092	37.383258
1781.812042	125975.107734	37.388276
1783.672970	126159.318537	37.393293
1785.267513	126361.497842	37.398311
1786.991240	126562.325940	37.403328
1788.769633	126769.413773	37.408346
1790.702018	126971.251714	37.413364
1792.396338	127170.197027	37.418381
1793.598691	127382.896399	37.423399
1795.751545	127593.216019	37.428416
1797.876778	127802.335734	37.433434
1799.504940	128032.822898	37.438452
1801.577388	128233.325741	37.443469
1803.375436	128446.229659	37.448487
1805.335294	128657.675812	37.453504
1806.998157	128867.621393	37.458522
1808.949846	129079.096320	37.463540
1810.917434	129299.780985	37.468557
1812.570564	129518.079729	37.473575
1814.443620	129725.218293	37.478592
1816.653160	129938.217983	37.483610
1818.101565	130162.413643	37.488628
1819.898822	130381.531801	37.493645
1821.703993	130602.108965	37.498663
1823.495917	130824.630592	37.503680
1825.220144	131045.006944	37.508698
1827.360327	131274.924596	37.513716
1829.648781	131493.426411	37.518733
1831.154314	131716.568202	37.523751
1832.782343	131934.540624	37.528768
1835.074876	132151.915876	37.533786
1836.494319	132377.827851	37.538804
1838.610003	132604.812670	37.543821
1841.005583	132819.815161	37.548839
1842.448744	133035.043072	37.553856
1844.903820	133260.544660	37.558874
1847.003250	133481.407915	37.563892
1848.928133	133679.180408	37.568909
1851.142567	133884.496673	37.573927
1853.055336	134089.327907	37.578944
1855.257257	134289.572424	37.583962
1856.844149	134504.404465	37.588980
1858.333932	134706.005220	37.593997
1860.144217	134917.099262	37.599015
1862.538535	135125.679760	37.604032
1864.336198	135322.413469	37.609050
1865.971704	135532.052963	37.614068
1867.962982	135737.615520	37.619085
1869.568575	135947.185463	37.624103
1871.115363	136163.097601	37.629120
1873.159486	136368.337562	37.634138
1874.512091	136582.276961	37.639156
1876.354993	136791.433178	37.644173
1877.992795	137023.438462	37.649191
1880.102065	137244.344086	37.654208
1882.090832	137454.800374	37.659226
1883.596455	137690.700017	37.664244
1884.858412	137901.880581	37.669261
1886.766593	138115.715278	37.674279
1888.339427	138326.417932	37.679296
1890.325633	138532.679095	37.684314
1892.110929	138751.231207	37.689332
1894.314590	138958.399487	37.694349
1895.884593	139174.030245	37.699367
1897.912950	139385.453584	37.704384
1900.127299	139601.150995	37.709402
1901.975484	139817.502835	37.714420
1903.648952	140036.877835	37.719437
1905.761168	140256.350544	37.724455
1907.375264	140476.752069	37.729472
1909.347604	140697.771468	37.734490
1911.239218	140927.116939	37.739508
1912.972808	141157.148029	37.744525
1914.985595	141381.958864	37.749543
1916.600060	141627.239871	37.754560
1918.813265	141861.197345	37.759578
1920.440841	142092.404280	37.764596
1922.597770	142337.604458	37.769613
1923.888557	142579.260209	37.774631
1925.902157	142814.763593	37.779648
1928.331025	143056.447636	37.784666
1930.407289	143304.799986	37.789684
1932.767351	143543.971537	37.794701
1935.425209	143770.584019	37.799719
1937.457398	144000.226677	37.804736
1939.862891	144223.796444	37.809754
1941.527374	144456.214452	37.814772
1943.439278	144686.627806	37.819789
1945.613150	144914.006171	37.824807
1947.193678	145145.272789	37.829824
1949.321890	145369.982328	37.834842
1951.377017	145599.793741	37.839860
1953.184563	145854.419673	37.844877
1954.752467	146076.973049	37.849895
1956.070772	146323.173731	37.854912
1958.424351	146567.754864	37.859930
1959.941985	146811.959571	37.864948
1962.107699	147064.238468	37.869965
1964.361098	147315.553018	37.874983
1965.913354	147566.140202	37.880000
1968.196262	147818.087217	37.885018
1969.801195	148079.914292	37.890036
1971.693179	148336.938241	37.895053
1973.777759	148603.719589	37.900071
1975.911720	148861.558857	37.905088
1978.040931	149112.545965	37.910106
1979.510259	149371.252726	37.915124
1981.835434	149627.047778	37.920141
1983.962376	149886.593975	37.925159
1985.828182	150149.215728	37.930176
1987.796723	150406.250466	37.935194
1989.938807	150666.293105	37.940212
1991.747311	150936.162758	37.945229
1994.009781	151181.706066	37.950247
1995.963056	151440.956730	37.955264
1998.258987	151690.470162	37.960282
1999.989980	151954.086326	37.965300
2002.333966	152208.595890	37.970317
2004.247762	152462.373876	37.975335
2006.065024	152729.686862	37.980352
2007.938665	152985.288688	37.985370
2009.911643	153244.709763	37.990388
2012.015921	153505.330219	37.995405
2014.115797	153770.484311	38.000423
2015.829284	154019.768789	38.005440
2017.667879	154273.135078	38.010458
2019.508174	154519.253884	38.015476
2021.358436	154764.470913	38.020493
2023.116603	155013.892423	38.025511
2024.993529	155273.198081	38.030528
2027.292990	155530.611158	38.035546
2028.818182	155794.950084	38.040564
2030.462011	156051.286929	38.045581
2032.263585	156307.752684	38.050599
2033.893154	156583.173946	38.055616
2036.160988	156848.366844	38.060634
2038.103549	157130.368554	38.065652
2039.865883	157414.951301	38.070669
2042.343788	157697.507126	38.075687
2044.276843	157981.380487	38.080704
2046.519366	158270.246919	38.085722
2048.934359	158548.843030	38.090740
2050.777134	158831.642677	38.095757
2053.421523	159095.415860	38.100775
2055.225511	159382.045330	38.105792
2057.803389	159666.270557	38.110810
2059.684098	159950.237435	38.115828
2061.883101	160215.544707	38.120845
2064.428072	160497.112858	38.125863
2066.158639	160782.693837	38.130880
2068.431988	161060.523555	38.135898
2070.754338	161355.270072	38.140916
2072.357690	161645.813348	38.145933
2074.613737	161922.989381	38.150951
2076.520010	162209.285816	38.155968
2078.589770	162508.063453	38.160986
2080.539332	162788.185575	38.166004
2082.404565	163093.637690	38.171021
2084.726642	163393.598962	38.176039
2086.981944	163684.659391	38.181056
2088.696079	163977.620876	38.186074
2090.945894	164287.957498	38.191092
2092.738379	164587.105215	38.196109
2095.272102	164882.939460	38.201127
2097.524610	165184.163931	38.206144
2099.413599	165480.888330	38.211162
2101.787198	165780.154078	38.216180
2103.969973	166087.982885	38.221197
2105.914375	166381.122189	38.226215
2108.026946	166690.386648	38.231232
2110.155786	166987.892862	38.236250
2112.730605	167290.549294	38.241268
2114.868055	167594.265459	38.246285
2117.230793	167888.437964	38.251303
2119.299093	168189.323382	38.256320
2121.718769	168479.439192	38.261338
2124.030253	168778.245060	38.266356
2125.898182	169074.873836	38.271373
2127.873009	169368.097081	38.276391
2130.154956	169678.618007	38.281408
2131.950378	169969.205210	38.286426
2134.071557	170260.123791	38.291444
2136.341094	170564.949364	38.296461
2138.362288	170871.490898	38.301479
2140.590748	171178.661707	38.306496
2142.748357	171473.375917	38.311514
2144.793811	171773.873403	38.316532
2146.935969	172076.693387	38.321549
2148.829544	172373.471119	38.326567
2150.554556	172687.316483	38.331584
2153.101885	172996.387797	38.336602
2155.135168	173292.512460	38.341620
2156.917027	173614.174563	38.346637
2159.158741	173916.452994	38.351655
2161.106248	174214.486487	38.356672
2163.281250	174502.543210	38.361690
2165.162173	174792.132410	38.366708
2167.175869	175101.345863	38.371725
2169.091181	175397.839637	38.376743
2170.852105	175704.618617	38.381760
2173.044330	176012.461771	38.386778
2175.293571	176323.408277	38.391796
2177.168425	176631.430129	38.396813
2179.589507	176946.593465	38.401831
2181.560115	177268.418556	38.406848
2183.700657	177589.151767	38.411866
2186.187053	177912.981593	38.416884
2188.006077	178236.535559	38.421901
2190.748043	178560.480452	38.426919
2192.732395	178886.169893	38.431936
2194.715737	179210.895614	38.436954
2196.981329	179544.543906	38.441972
2199.410026	179885.609551	38.446989
2201.962858	180209.640789	38.452007
2203.654348	180551.357066	38.457024
2205.628418	180888.814628	38.462042
2208.327147	181218.947667	38.467060
2211.275817	181531.086628	38.472077
2214.270830	181861.252066	38.477095
2216.489015	182191.234800	38.482112
2218.812825	182516.148011	38.487130
2221.034489	182832.798384	38.492148
2222.957917	183154.804499	38.497165
2225.267356	183485.285524	38.502183
2227.403657	183815.515246	38.507200
2229.685145	184139.348429	38.512218
2232.195438	184478.411734	38.517236
2234.398735	184815.695267	38.522253
2236.820457	185141.872015	38.527271
2238.828204	185496.967542	38.532288
2240.869314	185876.137489	38.537306
2242.967441	186208.743222	38.542324
2245.036843	186557.356052	38.547341
2247.503720	186888.585824	38.552359
2249.202105	187248.485228	38.557376
2251.099915	187596.391640	38.562394
2253.461335	187942.474462	38.567412
2255.584731	188313.868150	38.572429
2258.316888	188657.253996	38.577447
2259.740636	189015.119270	38.582464
2262.283799	189376.570682	38.587482
2264.769056	189731.148866	38.592500
2267.157930	190097.884419	38.597517
2269.571097	190446.354631	38.602535
2271.467318	190810.400515	38.607552
2273.955358	191171.332792	38.612570
2276.827788	191529.945719	38.617588
2278.527947	191892.907849	38.622605
2281.301511	192246.229609	38.627623
2284.005121	192603.805194	38.632640
2285.838638	192966.470375	38.637658
2288.325792	193312.270364	38.642676
2290.169402	193682.937311	38.647693
2293.097845	194034.207997	38.652711
2294.766529	194392.991190	38.657728
2297.071190	194762.929084	38.662746
2300.009266	195117.630355	38.667764
2301.914355	195477.116358	38.672781
2304.271515	195837.777634	38.677799
2306.471901	196201.639435	38.682816
2308.875414	196552.287248	38.687834
2311.048303	196906.401038	38.692852
2312.993699	197256.842495	38.697869
2315.062163	197582.981721	38.702887
2317.253004	197934.631317	38.707904
2319.509144	198278.955898	38.712922
2321.884246	198626.666609	38.717940
2324.044187	198977.586842	38.722957
2326.216772	199312.350309	38.727975
2328.735608	199661.590540	38.732992
2331.034744	200022.245851	38.738010
2333.532524	200377.409626	38.743028
2335.335720	200741.623835	38.748045
2337.901727	201094.924219	38.753063
2340.153499	201458.435160	38.758080
2342.354349	201824.825278	38.763098
2345.168094	202187.031026	38.768116
2346.982492	202564.532894	38.773133
2349.589731	202939.473554	38.778151
2351.829986	203311.169790	38.783168
2353.839687	203697.763172	38.788186
2356.443557	204084.823756	38.793204
2358.529905	204466.986756	38.798221
2360.824259	204848.330668	38.803239
2362.909678	205251.046174	38.808256
2365.191791	205656.551603	38.813274
2367.782299	206045.142343	38.818292
2370.229815	206453.824381	38.823309
2372.993261	206851.306142	38.828327
2374.932849	207254.480114	38.833344
2377.981136	207649.835964	38.838362
2380.668066	208033.639528	38.843380
2382.759127	208448.452105	38.848397
2385.278362	208840.386711	38.853415
2387.958853	209250.256953	38.858432
2389.893147	209642.715743	38.863450
2392.697153	210045.302738	38.868468
2395.267779	210436.368154	38.873485
2398.065555	210837.306123	38.878503
2400.573715	211249.213232	38.883520
2402.842926	211643.401111	38.888538
2405.378487	212049.081272	38.893556
2407.996887	212458.280191	38.898573
2410.257920	212852.572572	38.903591
2413.030971	213255.829450	38.908608
2414.482784	213652.636696	38.913626
2417.365803	214053.667324	38.918644
2419.742853	214464.455967	38.923661
2421.912145	214866.462322	38.928679
2424.753890	215270.244341	38.933696
2427.048618	215678.455958	38.938714
2429.529496	216074.343584	38.943732
2432.154076	216480.955041	38.948749
2434.339459	216882.656074	38.953767
2436.865869	217300.588271	38.958784
2439.279386	217696.487827	38.963802
2442.073953	218110.797039	38.968820
2444.159225	218520.441023	38.973837
2446.939710	218928.884749	38.978855
2449.321475	219332.310016	38.983872
2451.490649	219735.692416	38.988890
2453.794377	220156.430456	38.993908
2456.311253	220558.057160	38.998925
2458.988137	220966.391241	39.003943
2461.874953	221371.161691	39.008960
2464.017704	221774.904934	39.013978
2466.236948	222185.800381	39.018996
2468.788844	222591.283955	39.024013
2471.194362	223009.644902	39.029031
2473.751523	223406.896988	39.034048
2476.212756	223804.392734	39.039066
2478.637290	224188.811166	39.044084
2480.655300	224574.588533	39.049101
2483.009021	224955.791774	39.054119
2485.781195	225341.782110	39.059136
2487.973832	225736.322220	39.064154
2490.600684	226121.446053	39.069172
2492.562493	226522.093661	39.074189
2495.187691	226919.310069	39.079207
2497.494453	227315.178767	39.084224
2499.808029	227710.462057	39.089242
2502.539836	228122.726329	39.094260
2504.636635	228543.599696	39.099277
2506.907133	228961.600660	39.104295
2509.597384	229387.513044	39.109312
2511.811855	229814.693306	39.114330
2514.358800	230238.265085	39.119348
2517.318364	230667.615387	39.124365
2519.607235	231107.180645	39.129383
2522.496782	231540.834661	39.134400
2524.686625	231979.932143	39.139418
2527.668584	232411.996187	39.144436
2529.860027	232848.018951	39.149453
2532.667101	233284.631490	39.154471
2535.485297	233724.620673	39.159488
2538.175901	234160.615526	39.164506
2540.820959	234602.510778	39.169524
2543.372253	235036.367187	39.174541
2546.172470	235476.281352	39.179559
2549.274042	235913.506171	39.184576
2551.163339	236353.967627	39.189594
2553.934727	236798.965600	39.194612
2556.403545	237232.781694	39.199629
2559.110026	237666.636492	39.204647
2561.706458	238111.151994	39.209664
2564.469170	238567.758544	39.214682
2566.991283	239005.222199	39.219700
2569.557129	239450.528123	39.224717
2572.066773	239889.694490	39.229735
2574.653892	240335.021177	39.234752
2576.999610	240796.541296	39.239770
2579.701680	241238.088943	39.244788
2582.341069	241695.116234	39.249805
2584.924130	242148.849056	39.254823
2587.881325	242590.380091	39.259840
2589.768898	243052.424733	39.264858
2592.486985	243511.671903	39.269876
2595.249987	243959.098739	39.274893
2598.020993	244427.836585	39.279911
2600.680333	244881.857085	39.284928
2603.163237	245345.049135	39.289946
2605.863257	245801.855658	39.294964
2608.214423	246259.350521	39.299981
2610.480820	246723.640066	39.304999
2612.895578	247183.968005	39.310016
2615.760156	247668.738370	39.315034
2618.525532	248121.642708	39.320052
2621.271930	248599.595742	39.325069
2623.867643	249068.095849	39.330087
2626.577148	249528.194223	39.335104
2629.322216	249996.058937	39.340122
2632.537653	250448.226793	39.345140
2635.600405	250896.683062	39.350157
2638.284060	251364.655088	39.355175
2641.421305	251801.158277	39.360192
2643.665937	252240.517173	39.365210
2646.335486	252693.627310	39.370228
2648.731835	253136.287676	39.375245
2651.375375	253556.681765	39.380263
2654.119010	253982.241013	39.385280
2656.650563	254402.421485	39.390298
2658.884387	254811.800617	39.395316
2661.402931	255236.476711	39.400333
2663.842023	255665.939324	39.405351
2666.497744	256086.654247	39.410368
2668.498994	256533.505918	39.415386
2671.157564	256972.912881	39.420404
2673.802460	257418.086531	39.425421
2676.299044	257868.031700	39.430439
2678.631600	258322.115744	39.435456
2681.035111	258791.148138	39.440474
2683.602128	259252.025110	39.445492
2686.813487	259715.949740	39.450509
2689.790260	260185.674991	39.455527
2692.769142	260653.874038	39.460544
2694.912505	261117.705399	39.465562
2697.521643	261589.158659	39.470580
2701.080443	262061.300390	39.475597
2703.336524	262536.411464	39.480615
2706.164992	263003.506694	39.485632
2709.065719	263489.917868	39.490650
2711.649098	263971.702723	39.495668
2714.499793	264455.247175	39.500685
2716.833828	264930.742025	39.505703
2719.939297	265422.166980	39.510720
2722.077921	265916.914945	39.515738
2725.000874	266410.497093	39.520756
2728.094520	266895.516239	39.525773
2730.843127	267376.649909	39.530791
2733.733303	267861.543588	39.535808
2736.327328	268366.926719	39.540826
2738.953345	268860.390384	39.545844
2741.920829	269359.030379	39.550861
2744.662796	269871.189202	39.555879
2747.633523	270369.594708	39.560896
2750.592494	270859.541866	39.565914
2753.454634	271354.327002	39.570932
2756.953397	271851.600888	39.575949
2759.440426	272353.245397	39.580967
2762.234527	272838.788198	39.585984
2764.962310	273333.989503	39.591002
2767.583807	273828.645763	39.596020
2770.339382	274330.821133	39.601037
2772.696987	274833.410992	39.606055
2775.569788	275331.828812	39.611072
2778.581244	275845.104297	39.616090
2781.378154	276349.876828	39.621108
2784.396295	276848.237377	39.626125
2786.752062	277349.669217	39.631143
2789.434155	277858.970561	39.636160
2792.172758	278373.211935	39.641178
2794.792938	278879.951308	39.646196
2797.863611	279385.499851	39.651213
2800.413298	279909.435929	39.656231
2804.008879	280404.661801	39.661248
2807.386237	280912.590299	39.666266
2810.159546	281417.765132	39.671284
2813.358613	281901.081895	39.676301
2816.048042	282402.555404	39.681319
2818.894512	282888.231322	39.686336
2821.573853	283397.038324	39.691354
2824.681460	283896.353993	39.696372
2827.626395	284383.020096	39.701389
2830.123941	284873.358268	39.706407
2832.989212	285365.210110	39.711424
2836.009365	285843.017433	39.716442
2838.714014	286312.110000	39.721460
2841.147895	286762.755653	39.726477
2843.311358	287233.246426	39.731495
2846.393584	287690.412334	39.736512
2848.774731	288159.161376	39.741530
2851.917920	288626.366531	39.746548
2855.093030	289100.063626	39.751565
2857.547866	289572.523580	39.756583
2859.814944	290045.999527	39.761600
2863.122185	290535.763514	39.766618
2865.557362	291022.612496	39.771636
2868.602073	291512.181206	39.776653
2871.570060	292004.424000	39.781671
2874.099171	292506.531814	39.786688
2876.613395	293007.266762	39.791706
2879.267968	293515.262635	39.796724
2882.241593	294025.184971	39.801741
2884.904219	294543.250589	39.806759
2887.732012	295057.985386	39.811776
2890.543864	295592.546968	39.816794
2893.443217	296116.959935	39.821812
2896.600968	296648.462129	39.826829
2899.202212	297177.837239	39.831847
2902.178615	297722.737330	39.836864
2905.418376	298257.893064	39.841882
2908.321013	298799.620779	39.846900
2911.491646	299326.678444	39.851917
2914.729363	299880.123221	39.856935
2917.227194	300410.423250	39.861952
2920.284132	300959.620288	39.866970
2923.208332	301502.054281	39.871988
2926.588991	302055.378558	39.877005
2929.847117	302610.163170	39.882023
2932.599078	303148.697861	39.887040
2935.700758	303694.788214	39.892058
2938.184375	304244.548337	39.897076
2941.458057	304786.843517	39.902093
2944.125625	305340.980329	39.907111
2947.088509	305903.086601	39.912128
2950.442336	306461.495934	39.917146
2953.419465	307019.602349	39.922164
2956.561905	307565.543600	39.927181
2959.300771	308134.538731	39.932199
2962.368225	308686.647421	39.937216
2965.454286	309249.356897	39.942234
2968.402531	309806.725700	39.947252
2971.658340	310369.345058	39.952269
2974.294134	310921.977840	39.957287
2977.318791	311489.036461	39.962304
2979.873235	312052.709683	39.967322
2982.717193	312621.305749	39.972340
2985.778833	313196.231533	39.977357
2988.457715	313775.016808	39.982375
2991.571405	314350.148648	39.987392
2994.958747	314926.423553	39.992410
2997.829109	315501.680346	39.997428
3001.159692	316071.097255	40.002445
3004.084191	316643.260296	40.007463
3007.122770	317209.485181	40.012480
3010.168661	317783.746509	40.017498
3012.553615	318362.798085	40.022516
3016.050623	318940.907683	40.027533
3018.958457	319531.256822	40.032551
3021.604683	320104.306527	40.037568
3024.883382	320690.699567	40.042586
3027.976518	321274.322140	40.047604
3031.465521	321859.473784	40.052621
3034.437159	322425.971046	40.057639
3036.875287	322973.081277	40.062656
3039.886497	323509.209557	40.067674
3042.708025	324060.305814	40.072692
3045.676602	324600.308900	40.077709
3048.511256	325154.839364	40.082727
3051.663078	325710.404017	40.087744
3054.330506	326268.903600	40.092762
3056.806332	326839.223471	40.097780
3060.360411	327398.584372	40.102797
3063.259190	327976.332419	40.107815
3065.946541	328552.608089	40.112832
3069.052367	329131.321986	40.117850
3072.046457	329720.091514	40.122868
3075.405840	330304.000392	40.127885
3078.241398	330894.958729	40.132903
3081.420741	331487.630415	40.137920
3084.435476	332080.648399	40.142938
3087.261353	332686.041108	40.147956
3090.518882	333287.577167	40.152973
3093.167212	333907.108137	40.157991
3096.687007	334516.447829	40.163008
3099.935959	335133.734245	40.168026
3102.524497	335760.270519	40.173044
3105.668061	336375.853133	40.178061
3108.703424	337009.147537	40.183079
3111.915359	337643.595675	40.188096
3114.958122	338271.844710	40.193114
3118.123089	338921.445964	40.198132
3121.082766	339552.856174	40.203149
3124.917583	340194.771703	40.208167
3127.695148	340852.894933	40.213184
3131.205791	341482.714109	40.218202
3134.293212	342131.685492	40.223220
3137.378238	342780.340872	40.228237
3140.996770	343425.705642	40.233255
3144.464992	344072.273711	40.238272
3148.184009	344703.625232	40.243290
3150.873037	345349.377527	40.248308
3154.234459	345985.021416	40.253325
3158.029936	346633.163751	40.258343
3161.289059	347266.998954	40.263360
3165.001029	347890.532515	40.268378
3168.132497	348521.143352	40.273396
3171.908547	349140.966672	40.278413
3174.932286	349771.037943	40.283431
3177.979979	350398.456382	40.288448
3181.366301	351018.279527	40.293466
3184.539049	351641.572343	40.298484
3187.926462	352265.529656	40.303501
3191.265955	352899.471749	40.308519
3194.059066	353537.213253	40.313536
3197.368417	354145.680491	40.318554
3200.141989	354769.709729	40.323572
3203.379149	355388.153119	40.328589
3206.910056	356031.535067	40.333607
3209.930388	356654.803929	40.338624
3213.297863	357269.184345	40.343642
3216.443561	357905.109085	40.348660
3219.226293	358530.506501	40.353677
3222.153146	359165.678707	40.358695
3225.381961	359804.187357	40.363712
3228.763569	360437.766678	40.368730
3231.726699	361079.737049	40.373748
3235.400506	361718.972409	40.378765
3238.416241	362358.448581	40.383783
3241.467419	362994.027627	40.388800
3244.926338	363626.462839	40.393818
3247.779166	364263.692871	40.398836
3250.985100	364870.669490	40.403853
3254.187470	365475.327800	40.408871
3257.027906	366085.503928	40.413888
3260.248229	366690.083451	40.418906
3263.139501	367307.372415	40.423924
3266.084103	367920.610545	40.428941
3269.358270	368537.712047	40.433959
3272.349006	369168.350584	40.438976
3275.645578	369808.632559	40.443994
3278.565147	370449.744174	40.449012
3281.936889	371101.514282	40.454029
3285.164741	371739.685160	40.459047
3288.563189	372383.465065	40.464064
3291.585596	373036.536407	40.469082
3294.697556	373693.074727	40.474100
3298.002001	374365.326041	40.479117
3301.246126	375034.073999	40.484135
3304.548277	375718.098338	40.489152
3307.983034	376381.209918	40.494170
3311.300524	377069.555025	40.499188
3314.563472	377755.003083	40.504205
3317.841740	378435.998136	40.509223
3321.117467	379139.571356	40.514240
3324.844343	379831.733035	40.519258
3328.254021	380530.106311	40.524276
3331.295831	381216.942911	40.529293
3334.879447	381922.268079	40.534311
3338.295403	382632.792345	40.539328
3341.890326	383334.024937	40.544346
3345.313945	384027.743211	40.549364
3348.994336	384726.923716	40.554381
3352.966092	385439.765766	40.559399
3356.211574	386161.614905	40.564416
3359.885645	386848.658414	40.569434
3363.258511	387548.062193	40.574452
3366.702617	388245.055111	40.579469
3369.814891	388942.611949	40.584487
3373.262923	389655.466535	40.589504
3376.852072	390364.379374	40.594522
3380.221735	391077.762124	40.599540
3383.431208	391782.186359	40.604557
3386.667373	392488.105180	40.609575
3389.920416	393206.456785	40.614592
3393.397694	393927.638221	40.619610
3396.541716	394646.065250	40.624628
3400.292752	395356.376903	40.629645
3404.156477	396073.585900	40.634663
3407.442585	396795.976403	40.639680
3410.917436	397502.672503	40.644698
3414.028201	398224.742894	40.649716
3417.458215	398946.589551	40.654733
3421.106187	399671.720937	40.659751
3424.704746	400400.178251	40.664768
3427.920024	401115.410731	40.669786
3431.321115	401843.448420	40.674804
3434.279007	402572.847988	40.679821
3437.748996	403302.448319	40.684839
3441.146084	404035.376942	40.689856
3444.868793	404758.919238	40.694874
3448.219532	405496.109585	40.699892
3451.980496	406225.165707	40.704909
3455.224377	406954.582220	40.709927
3458.922449	407682.740395	40.714944
3462.557402	408406.836519	40.719962
3465.979972	409140.151022	40.724980
3469.402173	409871.720914	40.729997
3472.792858	410594.265367	40.735015
3475.915193	411308.420748	40.740020
3479.458084	412000.585663	40.745024
3482.759172	412633.271505	40.750029
3485.951856	413228.271727	40.755034
3489.106792	413763.719165	40.760039
3491.676402	414265.720908	40.765044
3494.395689	414700.388548	40.770048
3496.601352	415100.286571	40.775053
3498.550053	415453.459305	40.780058
3500.652449	415749.550466	40.785063
3502.557141	416019.906518	40.790068
3504.297205	416241.094540	40.795072
3506.014511	416445.042022	40.800077
3507.369761	416592.653577	40.805082
3508.857158	416724.523304	40.810087
3509.777864	416811.652580	40.815092
3511.121826	416865.906213	40.820096
3512.070505	416904.957505	40.825101
3513.013685	416914.902062	40.830106
3513.832134	416903.973503	40.835111
3514.676986	416871.641178	40.840116
3515.294766	416815.561051	40.845120
3515.728831	416754.539749	40.850125
3515.823515	416659.797845	40.855130
3516.547678	416564.501166	40.860135
3516.565558	416460.287395	40.865140
3516.991317	416315.592670	40.870144
3517.008278	416189.673212	40.875149
3517.136717	416050.094121	40.880154
3517.666340	415896.505772	40.885159
3517.669101	415750.148806	40.890164
3517.819085	415578.817053	40.895168
3517.878751	415416.322143	40.900173
3517.480917	415247.912941	40.905178
3517.927408	415067.858859	40.910183
3517.667471	414898.360443	40.915188
3517.638382	414708.437242	40.920192
3517.359105	414520.934928	40.925197
3517.000972	414332.428923	40.930202
3517.408591	414141.164840	40.935207
3516.800238	413976.074980	40.940212
3516.825710	413776.448102	40.945216
3516.936091	413599.730648	40.950221
3516.509222	413407.423395	40.955226
3516.989181	413216.241283	40.960231
3516.111200	413030.543591	40.965236
3516.068202	412842.279827	40.970240
3515.732394	412662.327362	40.975245
3515.714079	412483.997772	40.980250
3515.410118	412297.037892	40.985255
3515.290228	412114.308351	40.990260
3515.160132	411931.933915	40.995264
3515.007231	411767.263537	41.000269
3514.516872	411585.094422	41.005274
3514.924646	411410.950425	41.010279
3514.148398	411235.467586	41.015284
3514.352780	411064.345156	41.020288
3513.905735	410897.583587	41.025293
3514.154148	410733.451651	41.030298
3513.891934	410565.035601	41.035303
3513.494129	410409.675763	41.040308
3513.565875	410238.719699	41.045312
3513.446721	410075.451649	41.050317
3513.093939	409906.791012	41.055322
3512.789225	409756.231079	41.060327
3512.841328	409594.911159	41.065332
3512.810129	409435.378485	41.070336
3512.733568	409282.852168	41.075341
3512.335780	409133.570664	41.080346
3512.419251	408971.429654	41.085351
3511.979112	408821.391702	41.090356
3511.652891	408671.994487	41.095360
3511.876427	408534.939473	41.100365
3511.600647	408387.561675	41.105370
3511.201559	408247.862358	41.110375
3510.897146	408112.408798	41.115380
3510.954536	407973.651334	41.120384
3510.751422	407848.377309	41.125389
3510.602789	407709.193675	41.130394
3510.754492	407564.939985	41.135399
3510.546074	407445.042090	41.140404
3510.453755	407321.422020	41.145408
3510.199835	407192.245820	41.150413
3509.989279	407056.568303	41.155418
3509.874111	406942.893357	41.160423
3509.551806	406822.299575	41.165428
3509.439428	406707.405393	41.170432
3509.471104	406588.683152	41.175437
3509.271534	406467.662490	41.180442
3509.421617	406354.552092	41.185447
3508.745028	406245.780756	41.190452
3508.910536	406143.676349	41.195456
3508.986685	406042.397148	41.200461
3508.815435	405921.419869	41.205466
3508.697845	405814.335201	41.210471
3508.489258	405708.735528	41.215476
3507.997817	405609.876562	41.220480
3508.250504	405511.307258	41.225485
3508.348870	405415.298373	41.230490
3508.142266	405310.964945	41.235495
3507.663498	405212.051525	41.240500
3507.830870	405107.963387	41.245504
3507.601587	405021.085801	41.250509
3507.687890	404928.273190	41.255514
3508.001245	404840.042023	41.260519
3507.414562	404744.187627	41.265524
3507.374165	404652.763534	41.270528
3507.635145	404574.230514	41.275533
3507.419033	404480.194663	41.280538
3506.959464	404387.363303	41.285543
3506.906368	404304.768366	41.290548
3507.072799	404220.870484	41.295552
3506.634196	404129.709206	41.300557
3506.532117	404048.287969	41.305562
3506.646090	403982.105535	41.310567
3506.634962	403909.752090	41.315572
3506.788012	403817.736392	41.320576
3506.366560	403748.084777	41.325581
3506.472502	403681.395315	41.330586
3506.881987	403597.102128	41.335591
3506.315430	403526.406859	41.340596
3506.211620	403451.935264	41.345600
3506.062070	403371.280110	41.350605
3505.818189	403301.396533	41.355610
3505.665523	403227.845154	41.360615
3505.540723	403156.115905	41.365620
3505.795003	403081.384410	41.370624
3505.847960	403020.384355	41.375629
3505.633272	402955.772349	41.380634
3505.716582	402887.257371	41.385639
3505.687513	402816.780719	41.390644
3505.812303	402758.610368	41.395648
3505.693561	402701.797076	41.400653
3505.279016	402627.929321	41.405658
3505.281738	402564.500209	41.410663
3505.321606	402511.366006	41.415668
3505.265190	402449.366587	41.420672
3505.105101	402392.406733	41.425677
3504.655946	402335.440976	41.430682
3504.989944	402274.801152	41.435687
3504.826649	402222.509794	41.440692
3505.028270	402161.535064	41.445696
3504.889883	402114.364721	41.450701
3504.299691	402058.688826	41.455706
3505.170951	402019.632473	41.460711
3504.716515	401958.404085	41.465716
3504.773795	401894.863146	41.470720
3505.085708	401843.511869	41.475725
3504.934251	401793.704181	41.480730
3504.878632	401731.854937	41.485735
3504.554024	401683.038108	41.490740
3504.435594	401626.475834	41.495744
3504.557269	401584.998135	41.500749
3504.546942	401545.925932	41.505754
3504.853938	401491.326937	41.510759
3504.451668	401438.259059	41.515764
3504.337624	401391.235684	41.520768
3504.522981	401348.834230	41.525773
3504.160643	401299.616493	41.530778
3504.197651	401248.712638	41.535783
3504.152833	401206.245249	41.540788
3504.329276	401156.385160	41.545792
3504.366804	401111.418221	41.550797
3503.882769	401068.409971	41.555802
3504.027384	401023.781422	41.560807
3503.891417	400987.468133	41.565812
3504.362676	400943.549798	41.570816
3504.252836	400895.966548	41.575821
3504.076452	400855.904085	41.580826
3504.338009	400803.238916	41.585831
3504.164855	400772.411744	41.590836
3504.244457	400714.801483	41.595840
3504.123803	400678.383832	41.600845
3503.966221	400633.852305	41.605850
3503.813360	400589.472200	41.610855
3504.002215	400548.794149	41.615860
3504.121651	400505.690945	41.620864
3503.888429	400460.714128	41.625869
3503.666480	400422.840156	41.630874
3504.281355	400389.910686	41.635879
3504.196949	400349.883783	41.640884
3504.194063	400306.393261	41.645888
3503.813672	400257.531354	41.650893
3503.720486	400225.473056	41.655898
3504.113805	400183.087858	41.660903
3504.069757	400145.185750	41.665908
3503.773299	400093.265534	41.670912
3503.909987	400053.152967	41.675917
3503.634328	400019.803318	41.680922
3504.077683	399971.523105	41.685927
3503.879640	399943.388389	41.690932
3503.798942	399901.177938	41.695936
3503.833804	399865.902038	41.700941
3503.986953	399810.308049	41.705946
3503.949725	399771.846032	41.710951
3503.692525	399741.690310	41.715956
3503.684102	399698.808505	41.720960
3503.605804	399664.006653	41.725965
3503.350460	399625.781334	41.730970
3503.872002	399593.778756	41.735975
3503.599712	399557.179947	41.740980
3503.681769	399507.737007	41.745984
3503.537213	399476.396168	41.750989
3503.369137	399445.008197	41.755994
3503.667928	399405.072290	41.760999
3503.378947	399369.592284	41.766004
3503.469559	399327.455637	41.771008
3503.548851	399302.727999	41.776013
3503.397088	399266.617482	41.781018
3503.122201	399233.469588	41.786023
3503.517548	399200.978607	41.791028
3503.783622	399168.050943	41.796032
3503.728312	399134.361235	41.801037
3503.649585	399096.056814	41.806042
3503.831317	399056.544533	41.811047
3503.311318	399026.175027	41.816052
3503.434405	398984.489466	41.821056
3503.712121	398950.950675	41.826061
3503.426229	398922.371639	41.831066
3503.613857	398872.809426	41.836071
3503.252868	398834.853008	41.841076
3503.206751	398798.471572	41.846080
3503.584410	398772.580417	41.851085
3503.150417	398742.856927	41.856090
3503.446759	398700.839392	41.861095
3503.626576	398667.772194	41.866100
3503.660708	398644.421182	41.871104
3503.625089	398604.485197	41.876109
3503.194385	398576.029776	41.881114
3503.269008	398541.456217	41.886119
3503.253532	398503.090232	41.891124
3503.133554	398467.937823	41.896128
3503.403289	398433.790511	41.901133
3503.111345	398405.110282	41.906138
3503.284721	398376.205351	41.911143
3503.310005	398343.517009	41.916148
3502.901750	398311.149847	41.921152
3503.264071	398285.412800	41.926157
3503.241937	398258.618997	41.931162
3503.643753	398217.548483	41.936167
3503.384986	398200.992696	41.941172
3503.169696	398155.907144	41.946176
3503.230004	398125.547673	41.951181
3503.247980	398097.884648	41.956186
3503.275355	398053.167160	41.961191
3503.121388	398026.698125	41.966196
3502.962572	397995.103759	41.971200
3503.492395	397967.462438	41.976205
3503.320668	397939.016697	41.981210
3503.452049	397899.053527	41.986215
3503.158800	397866.008064	41.991220
3503.112890	397834.446667	41.996224
3503.107274	397817.343683	42.001229
3502.871782	397778.655481	42.006234
3503.027257	397745.438515	42.011239
3503.130983	397718.929033	42.016244
3503.040211	397691.637730	42.021248
3503.278280	397664.142962	42.026253
3503.127742	397636.048834	42.031258
3503.087415	397593.320408	42.036263
3502.915666	397579.745122	42.041268
3502.784814	397544.542272	42.046272
3502.952661	397517.971833	42.051277
3502.933778	397489.907799	42.056282
3503.156026	397458.304170	42.061287
3503.677774	397436.347952	42.066292
3503.333152	397408.385264	42.071296
3503.324637	397371.792754	42.076301
3503.082836	397347.468308	42.081306
3503.320614	397313.578120	42.086311
3503.446520	397281.075666	42.091316
3502.918434	397243.345700	42.096320
3502.844583	397219.705551	42.101325
3502.711132	397192.318803	42.106330
3502.895230	397163.766002	42.111335
3503.102719	397130.286304	42.116340
3503.122327	397105.464136	42.121344
3503.321022	397077.365754	42.126349
3503.024687	397052.237410	42.131354
3503.409400	397012.233320	42.136359
3502.949253	396992.967244	42.141364
3503.068826	396960.922132	42.146368
3502.838383	396926.089146	42.151373
3502.816762	396899.141454	42.156378
3503.185211	396858.530571	42.161383
3503.119170	396841.943839	42.166388
3503.168639	396818.436367	42.171392
3503.013057	396782.119609	42.176397
3503.133744	396761.798603	42.181402
3503.269357	396716.858721	42.186407
3502.866085	396690.223960	42.191412
3503.170825	396664.544867	42.196416
3503.457113	396632.168834	42.201421
3503.025461	396603.000594	42.206426
3503.172301	396571.356761	42.211431
3503.053576	396539.804968	42.216436
3502.895393	396511.304646	42.221440
3503.215712	396478.009495	42.226445
3502.879670	396452.074593	42.231450
3502.794544	396420.466656	42.236455
3502.949839	396401.561136	42.241460
3503.091530	396366.263368	42.246464
3503.241965	396335.278497	42.251469
3503.265352	396307.257241	42.256474
3503.129677	396276.469086	42.261479
3503.012384	396249.027977	42.266484
3502.726100	396222.983568	42.271488
3502.808531	396190.232601	42.276493
3502.852420	396173.526782	42.281498
3502.907536	396136.110354	42.286503
3502.915880	396125.094817	42.291508
3502.752010	396087.915418	42.296512
3502.870383	396061.757105	42.301517
3502.898398	396045.408967	42.306522
3502.736170	396008.432217	42.311527
3502.946171	395989.111798	42.316532
3502.796255	395957.158027	42.321536
3503.052268	395937.373590	42.326541
3502.728580	395914.633897	42.331546
3502.909405	395883.034619	42.336551
3502.686036	395856.726231	42.341556
3503.211741	395836.442924	42.346560
3502.946152	395795.167528	42.351565
3503.279526	395771.513327	42.356570
3503.314061	395746.484387	42.361575
3503.219384	395722.642958	42.366580
3502.990385	395684.051843	42.371584
3503.225407	395647.824845	42.376589
3502.963785	395619.542584	42.381594
3502.840762	395594.842551	42.386599
3503.045677	395569.127055	42.391604
3502.896163	395535.497636	42.396608
3502.797328	395506.022468	42.401613
3502.556716	395488.040724	42.406618
3502.709979	395458.373992	42.411623
3502.517843	395430.639037	42.416628
3502.850850	395400.741230	42.421632
3503.089772	395379.385475	42.426637
3502.468938	395350.143620	42.431642
3502.605646	395323.067990	42.436647
3502.746896	395306.092620	42.441652
3502.756623	395280.102635	42.446656
3502.916103	395257.185610	42.451661
3502.393237	395230.821619	42.456666
3502.858853	395197.299038	42.461671
3502.296619	395186.016544	42.466676
3502.332801	395162.052675	42.471680
3502.923456	395143.535243	42.476685
3502.606770	395115.514750	42.481690
3502.723416	395087.579069	42.486695
3502.629215	395066.274874	42.491700
3502.519552	395041.013838	42.496704
3502.631102	395014.550886	42.501709
3502.642177	394991.098347	42.506714
3502.729466	394965.197469	42.511719
3502.335827	394945.462548	42.516724
3502.756401	394935.752822	42.521728
3502.988254	394916.326618	42.526733
3502.734648	394875.504605	42.531738
3502.623656	394860.750839	42.536743
3502.537261	394841.272578	42.541748
3502.382292	394818.556346	42.546752
3502.649772	394799.378303	42.551757
3502.401921	394780.178917	42.556762
3502.412491	394753.376071	42.561767
3502.587371	394727.562827	42.566772
3502.643610	394703.595379	42.571776
3502.570572	394673.099971	42.576781
3502.702509	394670.389188	42.581786
3502.546964	394635.744242	42.586791
3502.855626	394619.656018	42.591796
3502.318751	394587.303791	42.596800
3502.838480	394562.401153	42.601805
3502.532837	394541.941561	42.606810
3502.467185	394521.089282	42.611815
3502.225413	394496.711158	42.616820
3502.738268	394476.834789	42.621824
3502.610720	394449.850056	42.626829
3502.549281	394430.164536	42.631834
3502.519848	394404.890346	42.636839
3502.203999	394384.787532	42.641844
3501.961652	394372.896506	42.646848
3502.488574	394355.403603	42.651853
3502.781089	394336.728904	42.656858
3503.050247	394309.834564	42.661863
3502.706104	394303.593801	42.666868
3502.520917	394265.450432	42.671872
3503.041186	394235.978885	42.676877
3502.563941	394217.779205	42.681882
3502.505073	394189.463705	42.686887
3502.844381	394177.482069	42.691892
3502.332309	394145.226909	42.696896
3502.868467	394123.214651	42.701901
3502.341837	394102.636789	42.706906
3502.617178	394071.223463	42.711911
3502.629117	394046.043982	42.716916
3502.479419	394025.864251	42.721920
3502.680566	394000.706040	42.726925
3502.231910	393985.496666	42.731930
3502.589260	393960.974007	42.736935
3502.538550	393947.733147	42.741940
3502.679061	393912.178141	42.746944
3502.552943	393893.669768	42.751949
3502.692882	393881.059107	42.756954
3502.521527	393849.258148	42.761959
3502.574400	393833.767586	42.766964
3502.213328	393797.732083	42.771968
3502.763126	393779.829109	42.776973
3502.446657	393763.583784	42.781978
3502.108762	393740.488903	42.786983
3502.335787	393729.844333	42.791988
3502.095837	393720.135381	42.796993
3501.956559	393691.324188	42.801997
3502.292153	393680.662701	42.807002
3502.373508	393652.680086	42.812007
3501.971966	393641.777954	42.817012
3502.404322	393614.603633	42.822017
3502.532157	393597.426098	42.827021
3502.465301	393581.598669	42.832026
3502.646404	393559.032000	42.837031
3502.613551	393531.879217	42.842036
3502.551482	393514.325073	42.847041
3502.116269	393489.671457	42.852045
3502.267108	393477.058889	42.857050
3502.469490	393447.686613	42.862055
3502.523815	393435.393619	42.867060
3501.879364	393415.899521	42.872065
3502.282566	393399.948063	42.877069
3502.484174	393374.738367	42.882074
3502.318446	393354.357519	42.887079
3502.167408	393337.730824	42.892084
3502.152107	393317.326536	42.897089
3502.764823	393294.793983	42.902093
3502.120337	393288.447404	42.907098
3502.470471	393257.427488	42.912103
3502.400316	393238.605325	42.917108
3502.468592	393215.852842	42.922113
3502.472562	393187.424863	42.927117
3502.306551	393181.562194	42.932122
3502.574403	393150.301129	42.937127
3502.822726	393141.531229	42.942132
3502.577663	393120.248790	42.947137
3502.534265	393097.615100	42.952141
3502.382394	393068.703598	42.957146
3502.648467	393045.361777	42.962151
3502.439006	393029.606942	42.967156
3502.347024	393005.610110	42.972161
3502.145123	392983.457852	42.977165
3502.367181	392969.666375	42.982170
3502.423517	392954.225475	42.987175
3502.440392	392931.379196	42.992180
3502.303297	392907.795399	42.997185
3502.387544	392883.618732	43.002189
3502.131792	392878.480649	43.007194
3502.217508	392855.725114	43.012199
3502.180129	392841.110949	43.017204
3501.883822	392815.064402	43.022209
3502.094524	392792.593943	43.027213
3502.032561	392785.293594	43.032218
3501.994696	392761.186571	43.037223
3502.278957	392748.552864	43.042228
3502.361138	392736.356710	43.047233
3502.063887	392711.325482	43.052237
3502.203498	392709.831628	43.057242
3502.396583	392678.124713	43.062247
3502.307276	392665.346037	43.067252
3502.014252	392649.299372	43.072257
3502.355297	392631.224980	43.077261
3502.458667	392615.015080	43.082266
3502.505534	392588.864124	43.087271
3502.235214	392573.626108	43.092276
3502.167934	392555.158320	43.097281
3502.104348	392541.512579	43.102285
3502.316492	392530.108331	43.107290
3502.315751	392498.025225	43.112295
3502.187681	392488.653722	43.117300
3502.331424	392472.792797	43.122305
3502.234749	392453.821859	43.127309
3502.275372	392440.159845	43.132314
3502.424605	392424.653389	43.137319
3502.179643	392397.938462	43.142324
3502.222057	392373.717033	43.147329
3502.291859	392358.375190	43.152333
3502.171987	392342.199848	43.157338
3502.567783	392322.746053	43.162343
3502.242172	392303.861388	43.167348
3502.196687	392279.298188	43.172353
3502.059993	392263.633063	43.177357
3501.744963	392252.361485	43.182362
3502.038219	392238.304689	43.187367
3502.028100	392218.000202	43.192372
3501.944288	392206.438796	43.197377
3502.663830	392194.346251	43.202381
3502.235153	392178.421914	43.207386
3502.200653	392150.201770	43.212391
3502.125568	392129.907320	43.217396
3501.956524	392117.902246	43.222401
3502.453007	392096.757343	43.227405
3502.196390	392082.887555	43.232410
3502.638491	392070.228936	43.237415
3502.357393	392053.875428	43.242420
3502.229501	392029.324800	43.247425
3502.477351	391998.826855	43.252429
3502.273487	391993.680510	43.257434
3502.216861	391966.986569	43.262439
3502.101364	391943.804602	43.267444
3502.082167	391928.577869	43.272449
3502.407966	391908.728511	43.277453
3502.107516	391899.688200	43.282458
3502.297428	391889.150134	43.287463
3502.567316	391869.512508	43.292468
3502.534006	391843.271697	43.297473
3502.449004	391814.906726	43.302477
3502.026976	391804.869978	43.307482
3502.118559	391780.843374	43.312487
3502.300581	391757.310336	43.317492
3502.188123	391746.362364	43.322497
3502.334417	391722.784086	43.327501
3502.475512	391715.705649	43.332506
3502.205357	391682.698836	43.337511
3502.126510	391669.054982	43.342516
3501.963622	391656.947191	43.347521
3502.462972	391630.064832	43.352525
3502.680584	391624.294390	43.357530
3502.530516	391591.776433	43.362535
3502.490139	391587.518358	43.367540
3502.307452	391560.945124	43.372545
3502.085323	391530.418196	43.377549
3502.261051	391509.881134	43.382554
3502.094170	391494.423279	43.387559
3502.208555	391475.367970	43.392564
3502.522355	391476.029909	43.397569
3502.549006	391438.864469	43.402573
3502.694446	391418.738179	43.407578
3502.550515	391397.489262	43.412583
3502.203475	391376.119631	43.417588
3502.151623	391359.933054	43.422593
3502.160172	391333.685183	43.427597
3501.950237	391324.985943	43.432602
3502.308412	391306.654073	43.437607
3502.396209	391289.328840	43.442612
3502.235690	391274.225226	43.447617
3502.133788	391256.117214	43.452621
3501.933192	391233.100118	43.457626
3501.932083	391213.961043	43.462631
3502.252633	391210.712853	43.467636
3502.219298	391184.522108	43.472641
3502.523330	391175.945906	43.477645
3501.999858	391149.932929	43.482650
3502.236049	391131.416841	43.487655
3502.240615	391123.597966	43.492660
3502.084827	391100.776843	43.497665
3502.388124	391084.077910	43.502669
3502.257181	391059.526784	43.507674
3502.367199	391049.203860	43.512679
3502.315561	391024.741893	43.517684
3502.201172	391012.423165	43.522689
3502.091685	390980.710366	43.527693
3502.106764	390977.154306	43.532698
3501.886033	390949.063292	43.537703
3502.492505	390939.881498	43.542708
3502.175873	390916.120642	43.547713
3502.553783	390894.942389	43.552717
3502.224008	390879.154118	43.557722
3502.251966	390851.582743	43.562727
3502.325347	390843.905375	43.567732
3502.091761	390819.725358	43.572737
3502.351220	390806.992975	43.577741
3502.146304	390791.743668	43.582746
3501.988326	390776.791657	43.587751
3502.161605	390748.943712	43.592756
3502.041743	390734.493427	43.597761
3502.250336	390725.830383	43.602765
3502.225496	390710.553004	43.607770
3502.678398	390673.675455	43.612775
3502.594603	390660.336420	43.617780
3502.287942	390645.407467	43.622785
3502.487143	390625.881384	43.627789
3502.451487	390606.950287	43.632794
3502.259976	390584.946542	43.637799
3502.352606	390564.929308	43.642804
3502.520852	390550.637157	43.647809
3502.627762	390519.499314	43.652813
3502.357300	390506.290781	43.657818
3502.282891	390480.283368	43.662823
3501.970824	390461.344403	43.667828
3501.810413	390452.129458	43.672833
3502.167430	390423.034099	43.677837
3502.082705	390413.299672	43.682842
3501.957766	390394.179229	43.687847
3502.166579	390383.332962	43.692852
3502.287538	390365.951150	43.697857
3502.544706	390349.081205	43.702861
3502.188425	390340.962850	43.707866
3502.266766	390310.286111	43.712871
3502.257850	390289.319841	43.717876
3502.210677	390277.726439	43.722881
3502.048406	390258.281700	43.727885
3501.774867	390245.124274	43.732890
3502.075241	390223.805203	43.737895
3502.429184	390207.833952	43.742900
3502.134977	390193.283556	43.747905
3502.200983	390165.477030	43.752909
3502.001844	390158.730323	43.757914
3502.196332	390147.759258	43.762919
3502.468899	390127.992903	43.767924
3501.961687	390113.932532	43.772929
3502.258056	390089.288558	43.777933
3502.498562	390076.964906	43.782938
3502.163858	390050.109074	43.787943
3501.999162	390032.898404	43.792948
3502.161621	390020.586868	43.797953
3502.293887	390002.390723	43.802957
3502.241400	389999.682739	43.807962
3502.417311	389967.441910	43.812967
3502.083829	389951.222076	43.817972
3502.323351	389929.531446	43.822977
3501.895205	389903.832321	43.827981
3501.589694	389892.710485	43.832986
3501.594420	389881.083435	43.837991
3502.278396	389876.458496	43.842996
3502.187090	389853.727724	43.848001
3502.212736	389842.985879	43.853005
3502.027379	389830.474522	43.858010
3502.187185	389803.414545	43.863015
3501.955979	389792.788804	43.868020
3501.919892	389779.949571	43.873025
3501.981502	389760.063439	43.878029
3501.754483	389750.655515	43.883034
3502.169380	389725.256565	43.888039
3501.994172	389718.607554	43.893044
3501.961037	389708.585584	43.898049
3502.305211	389685.989973	43.903053
3502.163338	389675.451820	43.908058
3502.075668	389651.552574	43.913063
3501.870281	389646.837521	43.918068
3501.950004	389625.603042	43.923073
3501.851916	389600.740726	43.928077
3502.003368	389605.210396	43.933082
3501.929258	389584.710610	43.938087
3502.096549	389564.477865	43.943092
3501.951070	389558.534975	43.948097
3502.211972	389527.219607	43.953101
3502.019475	389522.883306	43.958106
3501.600179	389502.157926	43.963111
3502.098429	389483.574439	43.968116
3502.059215	389476.117251	43.973121
3502.097203	389451.157454	43.978125
3502.388478	389441.059508	43.983130
3501.856414	389424.387905	43.988135
3502.172062	389405.655076	43.993140
3502.107277	389403.126638	43.998145
3502.120378	389379.109906	44.003149
3502.101695	389389.013214	44.008154
3502.623032	389360.881074	44.013159
3502.383018	389340.838457	44.018164
3501.955902	389318.311763	44.023169
3502.297668	389296.173114	44.028173
3502.059103	389281.080423	44.033178
3502.298705	389257.485269	44.038183
3502.299135	389245.731662	44.043188
3501.725895	389229.447120	44.048193
3502.205190	389215.638896	44.053197
3501.823224	389204.833276	44.058202
3501.933391	389178.516528	44.063207
3502.329196	389168.630678	44.068212
3501.899588	389150.216714	44.073217
3502.193626	389136.335731	44.078221
3501.967715	389120.352470	44.083226
3502.156744	389100.242894	44.088231
3502.050878	389089.191172	44.093236
3502.099010	389071.845171	44.098241
3501.941054	389055.978223	44.103245
3502.175330	389046.523634	44.108250
3502.231139	389023.413805	44.113255
3502.306917	388997.863796	44.118260
3501.968339	388977.886995	44.123265
3502.432336	388966.771927	44.128269
3502.164770	388953.003620	44.133274
3502.093285	388934.229135	44.138279
3502.047670	388918.649251	44.143284
3501.975558	388900.255628	44.148289
3502.119356	388882.539204	44.153293
3501.720913	388867.191893	44.158298
3501.909197	388846.828368	44.163303
3502.402941	388837.257166	44.168308
3501.991165	388827.649166	44.173313
3502.003496	388806.043682	44.178317
3501.947292	388783.738031	44.183322
3502.009539	388755.600490	44.188327
3502.299914	388752.534381	44.193332
3502.101724	388748.249602	44.198337
3502.377704	388733.863481	44.203341
3502.287817	388715.269398	44.208346
3501.822713	388691.986459	44.213351
3502.235916	388661.255572	44.218356
3501.981413	388658.858126	44.223361
3502.345623	388637.172353	44.228365
3501.918040	388623.428764	44.233370
3502.144438	388621.007253	44.238375
3502.173498	388592.976238	44.243380
3501.935182	388588.723061	44.248385
3502.018846	388565.710018	44.253389
3502.117041	388550.259843	44.258394
3502.207810	388537.451001	44.263399
3502.190866	388501.151068	44.268404
3501.770596	388498.068581	44.273409
3501.968694	388485.979218	44.278413
3501.663021	388465.590702	44.283418
3502.045969	388457.001282	44.288423
3502.012865	388447.791167	44.293428
3501.981630	388433.097268	44.298433
3502.223141	388411.785804	44.303437
3502.220366	388400.336935	44.308442
3502.298608	388380.320179	44.313447
3502.170394	388359.903961	44.318452
3501.839612	388347.008301	44.323457
3502.057697	388328.949897	44.328461
3501.726808	388310.164536	44.333466
3501.653461	388310.810650	44.338471
3501.956621	388300.481914	44.343476
3502.031977	388280.135500	44.348481
3502.278985	388267.886101	44.353485
3501.931769	388256.465379	44.358490
3501.989082	388231.222098	44.363495
3502.354737	388218.852665	44.368500
3501.878264	388196.510341	44.373505
3502.016321	388177.194944	44.378509
3502.193161	388170.998470	44.383514
3501.883330	388147.589312	44.388519
3501.921723	388136.641653	44.393524
3501.830798	388127.973541	44.398529
3502.271266	388117.699523	44.403533
3502.076386	388105.924998	44.408538
3501.951931	388083.223152	44.413543
3502.490825	388073.162282	44.418548
3501.929142	388049.462194	44.423553
3502.363224	388026.673382	44.428557
3501.720827	388020.528193	44.433562
3501.844214	387991.314025	44.438567
3501.734792	387994.352137	44.443572
3501.697336	387989.483701	44.448577
3502.062167	387961.323566	44.453581
3501.755017	387960.457465	44.458586
3501.911184	387944.160123	44.463591
3502.032215	387923.146248	44.468596
3501.912495	387911.029903	44.473601
3501.979004	387898.783025	44.478605
3501.799104	387882.334842	44.483610
3501.880815	387871.075681	44.488615
3501.720431	387856.579250	44.493620
3501.609639	387844.918452	44.498625
3501.893211	387828.423499	44.503629
3501.734867	387831.646953	44.508634
3501.962807	387817.420105	44.513639
3502.043645	387800.931294	44.518644
3501.998425	387789.793397	44.523649
3501.871365	387759.221637	44.528653
3501.724906	387754.370117	44.533658
3501.642437	387739.252201	44.538663
3501.747088	387732.686045	44.543668
3501.191442	387720.459732	44.548673
3501.618178	387698.407995	44.553677
3501.912185	387698.539990	44.558682
3501.801636	387696.856280	44.563687
3502.095202	387676.069222	44.568692
3501.707459	387661.125700	44.573697
3501.980722	387660.016944	44.578701
3501.852838	387636.325122	44.583706
3501.840200	387619.317604	44.588711
3502.178598	387610.887153	44.593716
3501.729204	387602.401577	44.598721
3501.870393	387581.181180	44.603725
3502.250395	387575.866892	44.608730
3501.862923	387541.197243	44.613735
3501.823791	387534.450310	44.618740
3502.179223	387526.829578	44.623745
3502.107806	387506.175338	44.628749
3501.963336	387499.089363	44.633754
3501.792769	387474.439305	44.638759
3501.719390	387466.428308	44.643764
3501.935691	387458.042193	44.648769
3501.855233	387445.005563	44.653773
3501.964893	387417.087626	44.658778
3501.758667	387418.414517	44.663783
3501.981222	387399.263084	44.668788
3501.703271	387390.573045	44.673793
3502.094061	387373.274094	44.678797
3501.776019	387366.291254	44.683802
3501.837642	387348.992734	44.688807
3501.823837	387342.165645	44.693812
3501.544172	387331.673330	44.698817
3501.930860	387314.730404	44.703821
3501.971993	387313.124615	44.708826
3501.840436	387293.291964	44.713831
3501.924725	387279.493368	44.718836
3501.719513	387270.944294	44.723841
3502.260306	387258.826401	44.728845
3501.810762	387238.433884	44.733850
3502.033216	387224.715309	44.738855
3501.825053	387210.733695	44.743860
3501.890817	387198.232714	44.748865
3502.142457	387194.156933	44.753869
3501.988307	387172.423619	44.758874
3501.509154	387159.804311	44.763879
3501.987928	387152.265824	44.768884
3501.628966	387135.565750	44.773889
3502.161041	387116.467488	44.778893
3501.807330	387108.449225	44.783898
3502.214648	387100.820290	44.788903
3502.149144	387072.700738	44.793908
3502.047983	387066.191823	44.798913
3501.992227	387033.399335	44.803917
3501.728804	387021.812681	44.808922
3502.054570	387010.743648	44.813927
3501.946042	386998.041197	44.818932
3501.650034	386991.461031	44.823937
3501.872088	386987.262882	44.828941
3501.624787	386963.487455	44.833946
3501.728190	386958.546124	44.838951
3502.076813	386940.999558	44.843956
3502.039057	386934.988503	44.848961
3501.774681	386914.846177	44.853965
3501.615563	386904.791910	44.858970
3501.765564	386893.851730	44.863975
3502.398664	386874.128251	44.868980
3501.809218	386875.438639	44.873985
3502.000907	386846.517169	44.878989
3501.968861	386838.677257	44.883994
3501.970821	386832.583832	44.888999
3502.471591	386808.082535	44.894004
3502.164634	386794.623826	44.899009
3502.064777	386759.349802	44.904013
3502.257250	386758.507462	44.909018
3502.080440	386731.521932	44.914023
3502.069462	386723.399434	44.919028
3501.811725	386712.649566	44.924033
3502.071898	386681.914684	44.929037
3502.241630	386672.494635	44.934042
3501.887917	386654.016242	44.939047
3502.045891	386634.975832	44.944052
3502.163192	386631.885623	44.949057
3502.015442	386605.200095	44.954061
3501.895317	386596.510610	44.959066
3502.093803	386582.770027	44.964071
3501.737245	386556.903982	44.969076
3502.059311	386547.130132	44.974081
3501.917359	386538.494799	44.979085
3501.951370	386520.616073	44.984090
3501.630624	386519.041158	44.989095
3501.985030	386501.264892	44.994100
3501.906480	386480.052374	44.999105
3502.151215	386472.346997	45.004109
3501.726275	386450.705975	45.009114
3501.908569	386432.727947	45.014119
3502.099877	386427.239673	45.019124
3501.825085	386413.978864	45.024129
3501.969835	386399.586442	45.029133
3501.678627	386391.253560	45.034138
3501.713676	386375.659542	45.039143
3501.618174	386362.193086	45.044148
3501.712767	386352.200672	45.049153
3501.606916	386346.352405	45.054157
3501.652121	386335.732954	45.059162
3501.524439	386326.460612	45.064167
3502.026975	386308.889658	45.069172
3501.708494	386306.273442	45.074177
3502.088074	386286.106572	45.079181
3501.791396	386271.274995	45.084186
3501.969950	386272.110460	45.089191
3502.330455	386248.239777	45.094196
3501.475895	386240.908503	45.099201
3501.678915	386223.333321	45.104205
3501.743256	386203.215440	45.109210
3501.804377	386193.025062	45.114215
3501.816259	386188.884875	45.119220
3501.868889	386183.468906	45.124225
3502.240396	386159.393317	45.129229
3502.230799	386155.484966	45.134234
3502.403411	386129.840804	45.139239
3502.375408	386122.634762	45.144244
3501.932340	386091.907041	45.149249
3502.034707	386069.853581	45.154253
3501.792523	386058.517068	45.159258
3501.861903	386045.761065	45.164263
3502.042987	386037.176848	45.169268
3501.541244	386025.271376	45.174273
3501.579420	386009.524313	45.179277
3501.407999	386003.153001	45.184282
3501.405365	385996.653866	45.189287
3502.078777	385988.729302	45.194292
3501.920154	385967.224146	45.199297
3502.154414	385947.333511	45.204301
3501.857624	385948.420680	45.209306
3501.468087	385928.347821	45.214311
3501.512423	385908.131263	45.219316
3501.800977	385918.292800	45.224321
3502.108373	385901.234322	45.229325
3502.032477	385874.714566	45.234330
3501.917520	385860.920812	45.239335
3501.938274	385848.629280	45.244340
3502.248096	385831.951216	45.249345
3502.202101	385819.746225	45.254349
3501.860675	385803.728046	45.259354
3502.322175	385791.494847	45.264359
3502.542093	385765.411339	45.269364
3502.155809	385762.373999	45.274369
3502.211488	385733.421645	45.279373
3502.368282	385716.741929	45.284378
3502.048425	385690.716950	45.289383
3502.021730	385680.895482	45.294388
3501.956258	385664.047204	45.299393
3501.975211	385637.918670	45.304397
3502.136450	385628.042547	45.309402
3502.101092	385606.771797	45.314407
3502.092036	385595.678083	45.319412
3501.833225	385587.949238	45.324417
3502.113415	385569.498356	45.329421
3502.157384	385565.708526	45.334426
3501.666832	385547.986910	45.339431
3502.032149	385517.107308	45.344436
3501.733818	385517.788503	45.349441
3501.842727	385503.578876	45.354445
3501.774899	385497.546770	45.359450
3501.813579	385482.535596	45.364455
3501.983449	385467.605558	45.369460
3501.562486	385445.861499	45.374465
3502.070246	385437.023129	45.379469
3501.505118	385435.917795	45.384474
3501.836969	385421.394146	45.389479
3501.653355	385405.401936	45.394484
3501.716783	385394.956983	45.399489
3501.644396	385392.810167	45.404493
3501.723189	385372.562432	45.409498
3501.512211	385349.389185	45.414503
3501.545488	385346.058000	45.419508
3501.409191	385352.274313	45.424513
3501.828147	385338.803426	45.429517
3501.574622	385321.374833	45.434522
3501.750589	385312.562662	45.439527
3501.815769	385301.228759	45.444532
3501.712709	385299.391385	45.449537
3502.025044	385269.839991	45.454541
3501.823813	385269.896729	45.459546
3501.892190	385261.761414	45.464551
3501.926468	385240.733420	45.469556
3501.568318	385232.004336	45.474561
3501.492519	385227.090554	45.479565
3501.636029	385210.818810	45.484570
3501.891248	385196.967092	45.489575
3502.078555	385189.016365	45.494580
3501.692381	385174.426580	45.499585
3501.813407	385147.316846	45.504589
3501.855201	385141.775392	45.509594
3502.024082	385139.286333	45.514599
3502.342373	385116.132072	45.519604
3501.926203	385101.369184	45.524609
3502.120205	385080.900170	45.529613
3501.995551	385074.292838	45.534618
3501.874085	385066.542462	45.539623
3501.739245	385046.302321	45.544628
3501.566002	385034.853062	45.549633
3501.958213	385019.938943	45.554637
3501.844887	385011.603314	45.559642
3501.841047	384999.670659	45.564647
3501.782302	384986.807112	45.569652
3501.881183	384975.213921	45.574657
3502.177204	384953.002409	45.579661
3501.825086	384942.672715	45.584666
3501.903284	384934.078747	45.589671
3502.051831	384914.708445	45.594676
3501.497011	384913.042902	45.599681
3502.059986	384895.791641	45.604685
3502.210249	384880.838920	45.609690
3501.778218	384869.023616	45.614695
3502.032952	384840.445513	45.619700
3501.777647	384838.784136	45.624705
3501.996635	384826.765945	45.629709
3502.034825	384813.607935	45.634714
3502.048372	384788.698099	45.639719
3501.777460	384786.861417	45.644724
3501.576481	384765.488786	45.649729
3501.934848	384750.249704	45.654733
3501.757153	384743.345857	45.659738
3501.750867	384737.177042	45.664743
3501.784415	384711.502310	45.669748
3501.632712	384704.061213	45.674753
3501.947114	384690.428523	45.679757
3501.712026	384677.109846	45.684762
3501.517081	384667.212607	45.689767
3501.629897	384660.009627	45.694772
3501.602036	384665.599866	45.699777
3501.884942	384641.714364	45.704781
3502.061530	384626.427324	45.709786
3501.657930	384619.660158	45.714791
3501.873893	384595.378784	45.719796
3501.570009	384590.601934	45.724801
3501.599424	384581.913878	45.729805
3501.523016	384575.603594	45.734810
3501.658529	384557.885425	45.739815
3502.144919	384542.956373	45.744820
3501.402837	384526.923564	45.749825
3501.488282	384452.389228	45.754829
3501.513845	384373.801498	45.759834
3501.024218	384235.650924	45.764839
3500.768117	384031.548472	45.769844
3500.224176	383802.351947	45.774849
3499.694551	383532.321758	45.779853
3498.972607	383204.857185	45.784858
3498.354884	382848.577606	45.789863
3497.420176	382450.521036	45.794868
3496.237019	382018.368954	45.799873
3495.719364	381537.833340	45.804877
3494.383406	381018.944493	45.809882
3493.143165	380466.459045	45.814887
3492.367130	379885.396574	45.819892
3490.797847	379263.862620	45.824897
3489.790561	378603.878351	45.829901
3488.005558	377908.138349	45.834906
3486.592296	377189.134403	45.839911
3484.970907	376433.036721	45.844916
3483.115942	375636.696763	45.849921
3481.353921	374815.808161	45.854925
3479.963599	373972.586107	45.859930
3477.647948	373094.250419	45.864935
3475.610744	372187.418363	45.869940
3473.534224	371265.117743	45.874945
3471.148107	370300.359505	45.879949
3469.226491	369323.809677	45.884954
3466.884811	368320.005822	45.889959
3464.811044	367290.438860	45.894964
3462.157077	366249.669752	45.899969
3460.067693	365177.370500	45.904973
3457.657141	364078.833882	45.909978
3454.597566	362960.359246	45.914983
3452.439376	361825.388049	45.919988
3449.562877	360672.214082	45.924993
3446.588447	359508.413900	45.929997
3443.706234	358321.554905	45.935002
3440.930552	357123.094899	45.940007
3438.416050	355903.579456	45.945012
3435.492194	354690.485305	45.950017
3432.754496	353446.864506	45.955021
3429.814559	352180.730621	45.960026
3426.841028	350902.579233	45.965031
3423.896494	349617.102631	45.970036
3420.731969	348326.347585	45.975041
3417.698097	347022.810432	45.980045
3414.704332	345714.131590	45.985050
3411.321958	344387.080344	45.990055
3408.337053	343048.728419	45.995060
3404.984332	341698.380524	46.000065
3401.920478	340336.035396	46.005069
3399.117241	338977.208452	46.010074
3395.764765	337611.956430	46.015079
3392.488153	336216.251329	46.020084
3388.759085	334826.286038	46.025089
3385.737918	333431.504647	46.030093
3382.253782	332029.520685	46.035098
3378.864761	330616.966095	46.040103
3375.644440	329205.249614	46.045108
3372.228114	327785.729452	46.050113
3368.610386	326354.412622	46.055117
3365.240523	324930.282070	46.060122
3362.011754	323488.985017	46.065127
3358.517991	322053.301704	46.070132
3354.574419	320604.308611	46.075137
3351.604527	319159.745601	46.080141
3347.533147	317703.602561	46.085146
3343.689552	316253.838947	46.090151
3340.821425	314795.225823	46.095156
3337.029211	313344.089183	46.100161
3333.504471	311880.015502	46.105165
3329.936388	310426.998113	46.110170
3326.016495	308959.079426	46.115175
3322.821324	307486.219758	46.120180
3318.600153	306021.899941	46.125185
3315.444046	304555.717986	46.130189
3311.412061	303100.167327	46.135194
3307.677623	301626.358105	46.140199
3304.279139	300163.705955	46.145204
3300.965850	298693.696695	46.150209
3297.145323	297224.465915	46.155213
3293.254440	295754.164699	46.160218
3289.260076	294281.984358	46.165223
3286.075874	292810.507053	46.170228
3282.274742	291353.727226	46.175233
3278.918672	289871.820544	46.180237
3275.261942	288406.142205	46.185242
3271.167334	286936.807737	46.190247
3267.255913	285469.678190	46.195252
3263.653629	284000.152354	46.200257
3260.072515	282531.127083	46.205261
3256.188882	281070.800613	46.210266
3252.573691	279607.577439	46.215271
3248.834740	278142.130246	46.220276
3245.202491	276681.145521	46.225281
3241.801601	275223.459112	46.230285
3237.752373	273766.968205	46.235290
3233.701745	272304.774500	46.240295
3229.927263	270839.025080	46.245300
3226.225273	269401.733952	46.250305
3222.515893	267941.963086	46.255309
3218.689530	266501.286371	46.260314
3214.611371	265059.431337	46.265319
3211.208613	263612.052719	46.270324
3206.954007	262181.339486	46.275329
3203.463100	260746.058221	46.280333
3199.598827	259310.741038	46.285338
3195.656686	257884.230260	46.290343
3192.205642	256457.652543	46.295348
3188.588372	255037.248291	46.300353
3184.712281	253606.275745	46.305357
3181.124212	252182.655307	46.310362
3177.179889	250769.264070	46.315367
3173.607924	249352.950335	46.320372
3169.541750	247938.179058	46.325377
3165.881997	246534.157472	46.330381
3162.095710	245104.855939	46.335386
3158.123157	243709.700952	46.340391
3154.488007	242311.836230	46.345396
3150.189009	240909.380735	46.350401
3146.790875	239515.640806	46.355405
3142.838357	238137.745685	46.360410
3139.276999	236754.868497	46.365415
3135.697584	235364.755854	46.370420
3131.870990	233980.967955	46.375425
3128.253247	232604.325955	46.380429
3124.490828	231226.557203	46.385434
3120.377831	229844.408870	46.390439
3116.823678	228468.156903	46.395444
3112.802046	227107.283348	46.400449
3109.357197	225736.386500	46.405453
3105.288765	224381.606755	46.410458
3101.377247	223012.515088	46.415463
3097.420254	221653.644845	46.420468
3093.965359	220307.865796	46.425473
3089.904621	218948.914142	46.430477
3086.302187	217612.306856	46.435482
3082.419972	216283.845756	46.440487
3078.971167	214942.204930	46.445492
3074.649445	213610.968568	46.450497
3071.084940	212286.190524	46.455501
3067.326285	210972.323490	46.460506
3063.575876	209641.270354	46.465511
3060.046330	208315.792833	46.470516
3055.924909	207016.417725	46.475521
3052.443076	205707.196668	46.480525
3048.561912	204414.803885	46.485530
3044.847238	203103.624402	46.490535
3041.126777	201799.840872	46.495540
3037.208361	200517.261267	46.500545
3033.378778	199220.722163	46.505549
3029.446425	197942.036638	46.510554
3025.626234	196667.088364	46.515559
3022.133689	195391.056572	46.520564
3018.112299	194106.613561	46.525569
3014.044591	192836.731456	46.530573
3010.479538	191581.859666	46.535578
3006.249721	190326.111365	46.540583
3002.810608	189074.506338	46.545588
2998.780661	187833.345949	46.550593
2995.000241	186589.869255	46.555597
2991.351054	185347.583779	46.560602
2987.401624	184127.691934	46.565607
2983.644135	182903.227457	46.570612
2979.465839	181677.978460	46.575617
2975.904799	180460.084720	46.580621
2972.082346	179253.044143	46.585626
2968.207729	178053.997878	46.590631
2964.622987	176848.354210	46.595636
2960.569933	175663.106175	46.600641
2956.768921	174474.755395	46.605645
2953.060282	173293.104089	46.610650
2948.959125	172113.339481	46.615655
2945.004019	170929.433238	46.620660
2940.947213	169772.637608	46.625665
2937.307281	168614.242472	46.630669
2933.425572	167462.306554	46.635674
2929.512683	166318.146421	46.640679
2925.714036	165174.305798	46.645684
2921.501863	164044.932265	46.650689
2917.529549	162928.039967	46.655693
2913.633585	161810.747696	46.660698
2909.563004	160705.619159	46.665703
2905.513775	159617.956469	46.670708
2901.317963	158531.608519	46.675713
2897.630451	157448.382732	46.680717
2893.593898	156380.261531	46.685722
2889.359155	155330.644438	46.690727
2885.401852	154277.363394	46.695732
2881.386300	153238.211637	46.700737
2877.430678	152209.746953	46.705741
2873.591310	151189.682324	46.710746
2868.945174	150173.020029	46.715751
2864.815859	149186.621075	46.720756
2860.676287	148202.685220	46.725761
2856.580048	147226.994060	46.730765
2853.102117	146275.732755	46.735770
2848.661776	145313.441345	46.740775
2844.448288	144379.915062	46.745780
2839.798265	143456.844149	46.750785
2835.499302	142551.320019	46.755789
2831.107586	141644.707395	46.760794
2826.662176	140706.680915	46.765799
2822.225877	139850.569444	46.770804
2817.911521	139007.953340	46.775809
2813.368944	138198.886414	46.780813
2808.314661	137397.877386	46.785818
2803.917488	136619.908877	46.790823
2799.408773	135853.268045	46.795828
2794.966633	135119.617248	46.800833
2790.928525	134385.991885	46.805837
2786.493475	133670.708169	46.810842
2782.106770	132985.768347	46.815847
2777.845071	132310.742077	46.820852
2773.721092	131645.372583	46.825857
2769.884633	131008.818744	46.830861
2765.930497	130375.867065	46.835866
2761.514982	129739.956455	46.840871
2757.936821	129122.330872	46.845876
2753.918212	128528.505292	46.850881
2749.992192	127921.636128	46.855885
2746.472422	127332.710582	46.860890
2742.424440	126752.092256	46.865895
2738.850022	126184.165664	46.870900
2735.166514	125614.839424	46.875905
2731.691076	125053.310791	46.880909
2728.378306	124489.627931	46.885914
2724.227320	123934.299482	46.890919
2720.927965	123380.525024	46.895924
2717.403953	122825.496003	46.900929
2713.878544	122274.264907	46.905933
2710.193131	121733.176975	46.910938
2706.182829	121200.324431	46.915943
2703.204458	120655.580521	46.920948
2699.756319	120117.924518	46.925953
2696.327646	119584.876528	46.930957
2692.883169	119047.095056	46.935962
2689.161636	118520.033510	46.940967
2685.657492	117982.034772	46.945972
2682.040923	117457.171639	46.950977
2678.450263	116918.832787	46.955981
2675.060803	116390.617648	46.960986
2671.493313	115860.899118	46.965991
2668.147156	115324.465366	46.970996
2664.709731	114805.740654	46.976001
2661.433995	114273.685359	46.981005
2657.847408	113741.012305	46.986010
2654.008781	113215.137837	46.991015
2650.150839	112688.117003	46.996020
2646.621293	112168.528859	47.001025
2643.331254	111641.409595	47.006029
2640.052943	111116.991678	47.011034
2636.257079	110609.609615	47.016039
2632.408324	110087.507940	47.021044
2628.848272	109578.387692	47.026049
2624.943328	109059.602859	47.031053
2621.887566	108544.672803	47.036058
2618.097434	108043.912445	47.041063
2614.407491	107535.172878	47.046068
2610.522672	107042.260147	47.051073
2606.583318	106543.146656	47.056077
2602.962879	106052.063077	47.061082
2599.047503	105571.697866	47.066087
2595.574579	105086.579967	47.071092
2591.677596	104614.424648	47.076097
2587.510109	104145.826436	47.081101
2583.985134	103679.321152	47.086106
2580.288826	103224.988177	47.091111
2576.773561	102761.023790	47.096116
2572.432815	102318.090867	47.101121
2568.501519	101865.173223	47.106125
2564.975367	101428.188486	47.111130
2560.904860	100998.895036	47.116135
2557.555388	100560.242105	47.121140
2553.900354	100143.249502	47.126145
2550.534245	99724.234595	47.131149
2546.960964	99298.877168	47.136154
2543.108088	98879.300834	47.141159
2539.899181	98462.069962	47.146164
2536.085205	98039.588187	47.151169
2532.315532	97626.687654	47.156173
2529.298823	97215.391007	47.161178
2525.780296	96807.545583	47.166183
2522.351584	96387.631178	47.171188
2518.849310	95971.825897	47.176193
2515.512675	95556.254527	47.181197
2512.416315	95148.212512	47.186202
2508.667720	94727.048596	47.191207
2505.217426	94309.275029	47.196212
2501.517728	93895.993517	47.201217
2498.106686	93476.306313	47.206221
2494.904663	93056.363595	47.211226
2491.436920	92645.362810	47.216231
2488.290466	92216.858554	47.221236
2484.622720	91798.873520	47.226241
2481.441837	91370.500932	47.231245
2477.620726	90954.203266	47.236250
2474.070861	90536.776432	47.241255
2470.746842	90097.542493	47.246260
2467.574781	89684.947764	47.251265
2463.859916	89250.983705	47.256269
2460.546754	88814.676523	47.261274
2456.712886	88391.771720	47.266279
2453.635629	87959.582293	47.271284
2450.045662	87528.292101	47.276289
2446.433978	87104.583523	47.281293
2443.441280	86666.644825	47.286298
2439.521487	86237.203603	47.291303
2436.402624	85800.339307	47.296308
2432.511389	85367.400220	47.301313
2429.223018	84935.504421	47.306317
2425.870855	84504.272898	47.311322
2422.307096	84072.775904	47.316327
2418.963252	83632.956131	47.321332
2415.503800	83192.094092	47.326337
2411.789704	82754.720922	47.331341
2408.775482	82312.380557	47.336346
2405.094166	81870.836847	47.341351
2401.546061	81427.018367	47.346356
2398.111134	80980.661625	47.351361
2394.791560	80541.711785	47.356365
2391.412563	80094.712697	47.361370
2387.596881	79650.786231	47.366375
2384.308530	79199.608738	47.371380
2380.728578	78754.377150	47.376385
2377.337969	78304.233559	47.381389
2373.728230	77861.192851	47.386394
2369.729403	77415.844924	47.391399
2366.602365	76967.739692	47.396404
2362.722852	76527.213693	47.401409
2359.339168	76079.036044	47.406413
2356.363929	75631.500711	47.411418
2352.746925	75191.222281	47.416423
2349.049334	74728.930967	47.421428
2345.752458	74280.985583	47.426433
2341.687928	73824.773464	47.431437
2338.879547	73385.579823	47.436442
2334.985128	72934.397701	47.441447
2331.923919	72484.503051	47.446452
2328.340471	72032.653011	47.451457
2324.948628	71585.999536	47.456461
2321.416576	71123.922985	47.461466
2317.940610	70678.504282	47.466471
2314.496459	70209.015178	47.471476
2311.336952	69758.801651	47.476481
2307.666472	69305.012564	47.481485
2304.147974	68835.109150	47.486490
2300.828871	68389.870340	47.491495
2297.412295	67915.257670	47.496500
2293.797296	67458.502640	47.501505
2290.255279	66984.167951	47.506509
2286.748494	66520.957355	47.511514
2283.442688	66058.841052	47.516519
2280.084564	65597.934591	47.521524
2276.285465	65134.433022	47.526529
2272.653764	64665.106420	47.531533
2268.929737	64199.922076	47.536538
2265.441558	63738.854101	47.541543
2262.029460	63267.843942	47.546548
2258.607685	62799.852446	47.551553
2255.231890	62331.431054	47.556557
2251.932067	61871.897845	47.561562
2248.152180	61400.567866	47.566567
2244.371360	60930.389342	47.571572
2241.208467	60470.270792	47.576577
2237.644367	59997.049428	47.581581
2234.268301	59524.734443	47.586586
2230.639799	59060.171415	47.591591
2227.540102	58587.178038	47.596596
2223.998426	58119.008980	47.601601
2220.396342	57650.953580	47.606605
2216.840393	57166.993021	47.611610
2212.826979	56702.021333	47.616615
2209.770971	56221.935915	47.621620
2206.367614	55756.710022	47.626625
2202.696189	55284.670123	47.631629
2199.059617	54801.100004	47.636634
2195.792264	54340.550212	47.641639
2192.521637	53865.012260	47.646644
2188.988186	53392.119539	47.651649
2185.479578	52913.846486	47.656653
2182.500619	52438.196893	47.661658
2178.681568	51959.236779	47.666663
2175.260204	51465.780403	47.671668
2171.686016	50989.720192	47.676673
2167.824720	50518.186466	47.681677
2164.493976	50029.212285	47.686682
2160.887978	49557.867804	47.691687
2157.724059	49069.319408	47.696692
2154.074037	48597.094510	47.701697
2150.518208	48118.902670	47.706701
2147.164912	47625.004416	47.711706
2143.353614	47146.707887	47.716711
2139.965046	46655.645903	47.721716
2136.722151	46173.381058	47.726721
2133.054766	45695.581225	47.731725
2129.694628	45206.911960	47.736730
2126.050493	44727.480278	47.741735
2122.685805	44239.511424	47.746740
2119.143655	43758.543719	47.751745
2115.487503	43275.422786	47.756749
2112.164251	42788.512993	47.761754
2108.777951	42300.989649	47.766759
2105.394085	41801.365747	47.771764
2101.887024	41321.872333	47.776769
2098.187455	40839.268127	47.781773
2094.668856	40342.006435	47.786778
2090.901310	39867.093517	47.791783
2087.705185	39363.140396	47.796788
2084.249454	38888.999211	47.801793
2080.652143	38393.018042	47.806797
2077.082267	37904.632617	47.811802
2073.605843	37416.877697	47.816807
2070.503081	36922.425692	47.821812
2066.812084	36429.560048	47.826817
2063.054612	35939.961761	47.831821
2059.692183	35451.948714	47.836826
2055.887784	34961.289988	47.841831
2052.477362	34472.590681	47.846836
2048.969783	33979.271677	47.851841
2045.759179	33490.171060	47.856845
2041.747440	33005.846096	47.861850
2038.311150	32509.261000	47.866855
2035.120453	32027.885856	47.871860
2031.623751	31542.468915	47.876865
2027.836404	31054.345340	47.881869
2024.340940	30559.805993	47.886874
2020.731352	30073.851631	47.891879
2017.125145	29586.900584	47.896884
2013.579669	29107.993307	47.901889
2010.071696	28618.248967	47.906893
2006.419444	28140.306110	47.911898
2002.659310	27663.683898	47.916903
1998.718948	27180.371598	47.921908
1995.382794	26710.523745	47.926913
1991.462580	26242.165300	47.931917
1987.895595	25775.251695	47.936922
1984.019751	25323.590340	47.941927
1980.282838	24864.593425	47.946932
1975.788505	24425.168743	47.951937
1971.952354	23987.190785	47.956941
1968.368109	23547.326985	47.961946
1964.200300	23122.413315	47.966951
1960.897159	22699.382357	47.971956
1956.959301	22284.631204	47.976961
1953.055223	21878.606444	47.981965
1949.592419	21458.262104	47.986970
1945.587858	21058.015368	47.991975
1942.116794	20649.275371	47.996980
1938.417231	20250.897911	48.001985
1934.744257	19865.224300	48.006989
1931.463838	19464.396979	48.011994
1927.422354	19096.816075	48.016999
1924.074375	18709.410906	48.022004
1920.004660	18326.818987	48.027009
1916.539283	17953.495118	48.032013
1912.906627	17571.065427	48.037018
1909.521936	17207.873602	48.042023
1906.031028	16825.889425	48.047028
1902.389606	16465.724933	48.052033
1899.166206	16099.444723	48.057037
1895.811074	15718.275184	48.062042
1891.912699	15366.942168	48.067047
1888.611527	14982.748703	48.072052
1885.365555	14623.174713	48.077057
1881.728086	14265.412976	48.082061
1878.434383	13887.395395	48.087066
1874.755519	13530.109855	48.092071
1871.365238	13154.395103	48.097076
1867.778617	12794.484507	48.102081
1864.096630	12425.702788	48.107085
1860.729556	12061.026427	48.112090
1857.653787	11705.704451	48.117095
1853.530817	11346.452657	48.122100
1849.941137	10986.852505	48.127105
1846.025351	10631.592972	48.132109
1842.412190	10266.068630	48.137114
1838.587149	9915.939811	48.142119
1834.768276	9565.734314	48.147124
1830.910531	9238.961451	48.152129
1826.631357	8907.990025	48.157133
1823.238353	8590.462054	48.162138
1818.708482	8290.091059	48.167143
1814.988509	7971.959920	48.172148
1811.303212	7671.065589	48.177153
1807.030392	7390.494969	48.182157
1803.639904	7097.156917	48.187162
1799.600418	6816.159971	48.192167
1796.091718	6542.984138	48.197172
1792.624122	6273.730313	48.202177
1788.125187	6010.590676	48.207181
1785.074602	5741.238649	48.212186
1780.781273	5493.337789	48.217191
1777.668092	5234.028607	48.222196
1774.123382	4980.518133	48.227201
1770.607398	4743.579306	48.232205
1766.582967	4485.273882	48.237210
1762.911273	4254.957272	48.242215
1759.509754	4025.857806	48.247220
1756.079440	3786.627133	48.252225
1752.269456	3551.996340	48.257229
1748.947064	3332.231238	48.262234
1744.993615	3099.207636	48.267239
1741.951111	2870.801051	48.272244
1738.416464	2647.296129	48.277249
1734.374877	2428.524135	48.282253
1731.127760	2208.742052	48.287258
1727.763223	1993.198598	48.292263
1724.124716	1772.713914	48.297268
1720.017494	1567.431799	48.302273
1716.686399	1354.510593	48.307277
1713.082274	1137.821935	48.312282
1709.242285	941.123860	48.317287
1705.685036	745.000896	48.322292
1701.549206	549.324488	48.327297
1697.583154	370.211350	48.332301
1693.615761	192.640959	48.337306
1688.498073	57.565759	48.342311
1678.523562	70.279759	48.347316
1669.989275	81.776208	48.352321
1665.075703	100.700642	48.357325
1661.783118	91.187369	48.362330
1659.145439	94.850221	48.367335
1657.006837	99.381343	48.372340
1654.793477	98.425587	48.377345
1651.631790	99.094880	48.382349
1648.969706	93.956950	48.387354
1645.426276	99.076875	48.392359
1642.001300	100.179446	48.397364
1638.616958	85.336970	48.402369
1634.909473	96.768701	48.407373
1632.530162	97.835071	48.412378
1628.897137	110.409972	48.417383
1625.597652	104.194350	48.422388
1622.160678	94.111943	48.427393
1618.862205	91.705265	48.432397
1615.646247	88.887119	48.437402
1611.965786	88.118582	48.442407
1607.974603	94.924848	48.447412
1604.796340	89.598350	48.452417
1601.584703	94.555906	48.457421
1598.205047	78.149847	48.462426
1594.712560	93.227493	48.467431
1591.495732	92.905643	48.472436
1587.905816	88.060827	48.477441
1584.507678	95.255673	48.482445
1581.261084	93.913419	48.487450
1577.788918	87.487409	48.492455
1574.227960	89.098360	48.497460
1570.409951	95.956767	48.502465
1566.829378	97.770085	48.507469
1563.961086	90.661639	48.512474
1560.566133	102.206078	48.517479
1557.008791	98.909570	48.522484
1553.454062	90.943037	48.527489
1549.715228	90.439851	48.532493
1546.047996	84.135957	48.537498
1542.974244	90.119236	48.542503
1539.716396	94.470230	48.547508
1536.027943	82.190252	48.552513
1532.457662	85.770476	48.557517
1529.430188	88.086156	48.562522
1525.533873	92.229646	48.567527
1522.469516	86.942377	48.572532
1518.757625	91.949325	48.577537
1515.073285	89.463514	48.582541
1512.165732	91.548564	48.587546
1508.290091	95.568617	48.592551
1504.720418	90.698515	48.597556
1501.308579	90.071674	48.602561
1497.845703	94.100248	48.607565
1494.415048	91.631901	48.612570
1490.709734	89.247433	48.617575
1487.458770	91.847834	48.622580
1484.280129	88.425956	48.627585
1480.066562	85.832701	48.632589
1477.116189	83.934998	48.637594
1473.198413	95.019815	48.642599
1469.655362	93.363053	48.647604
1466.612030	86.965225	48.652609
1462.971273	93.255056	48.657613
1459.871774	80.304470	48.662618
1455.961977	95.076913	48.667623
1452.701871	92.904723	48.672628
1449.428242	86.387722	48.677633
1445.453703	91.685486	48.682637
1442.078086	83.150106	48.687642
1438.412293	92.496799	48.692647
1434.991589	84.202550	48.697652
1431.717297	84.326249	48.702657
1428.171883	87.972211	48.707661
1424.835763	83.844039	48.712666
1420.723740	96.743416	48.717671
1417.601997	84.270852	48.722676
1414.335655	97.522646	48.727681
1410.613762	91.518337	48.732685
1407.289143	91.706818	48.737690
1404.204586	93.705532	48.742695
1400.147870	85.247696	48.747700
1397.010862	83.233520	48.752705
1393.354138	98.922010	48.757709
1389.927541	90.986180	48.762714
1386.009137	91.143701	48.767719
1382.414479	90.058119	48.772724
1379.351229	89.873734	48.777729
1375.633935	97.947151	48.782733
1372.597783	93.800767	48.787738
1368.787915	88.449226	48.792743
1364.878461	93.081981	48.797748
1362.275122	89.181438	48.802753
1358.036286	95.592839	48.807757
1354.819760	83.138205	48.812762
1351.466849	88.260126	48.817767
1347.758020	92.928093	48.822772
1344.307592	95.812646	48.827777
1340.982972	95.583526	48.832781
1337.697918	92.655946	48.837786
1333.911391	88.499816	48.842791
1330.090509	91.967204	48.847796
1326.902287	88.901170	48.852801
1322.855308	94.238692	48.857805
1319.917756	82.461965	48.862810
1316.358154	97.249500	48.867815
1312.691069	90.420444	48.872820
1309.520572	88.667748	48.877825
1305.665288	90.716832	48.882829
1302.766104	82.034554	48.887834
1298.818546	87.812172	48.892839
1295.497361	82.634512	48.897844
1292.108148	74.370192	48.902849
1288.511823	88.565499	48.907853
1284.847804	86.095537	48.912858
1281.409392	77.003661	48.917863
1278.124896	79.631441	48.922868
1274.161653	80.665968	48.927873
1270.278649	84.753621	48.932877
1267.496382	82.491258	48.937882
1264.208281	88.900209	48.942887
1261.003739	85.200822	48.947892
1256.862964	81.618690	48.952897
1253.269129	87.341254	48.957901
1249.857703	87.419878	48.962906
1246.297208	83.605059	48.967911
1242.753962	81.622496	48.972916
1239.801436	83.588015	48.977921
1235.671801	85.315984	48.982925
1232.128717	78.211387	48.987930
1228.919090	89.578277	48.992935
1225.291488	79.354785	48.997940
1222.080597	75.365334	49.002945
1218.462400	84.505308	49.007949
1215.189092	83.607004	49.012954
1211.750984	86.189098	49.017959
1207.774160	85.096586	49.022964
1204.504542	80.613251	49.027969
1200.507117	82.655996	49.032973
1197.498896	73.573105	49.037978
1193.493839	79.524189	49.042983
1190.288099	83.481120	49.047988
1187.090784	72.412397	49.052993
1183.027575	86.927141	49.057997
1180.072011	73.878284	49.063002
1176.853594	83.364147	49.068007
1173.111120	73.386334	49.073012
1169.622372	76.137661	49.078017
1165.775045	80.529810	49.083021
1162.266244	79.696640	49.088026
1158.586094	70.553835	49.093031
1155.248523	79.495107	49.098036
1151.826312	76.019439	49.103041
1148.450305	78.477979	49.108045
1145.184178	77.983517	49.113050
1141.614947	76.811751	49.118055
1137.498947	78.120002	49.123060
1134.689159	73.387938	49.128065
1131.108430	73.616311	49.133069
1127.416079	79.246649	49.138074
1123.932748	77.915985	49.143079
1120.096893	73.169634	49.148084
1117.029104	62.435102	49.153089
1113.371534	80.430023	49.158093
1109.777092	67.059862	49.163098
1106.468458	77.891676	49.168103
1102.613603	74.771254	49.173108
1099.577224	74.108160	49.178113
1095.972545	78.693493	49.183117
1092.583007	66.158291	49.188122
1088.713175	78.020237	49.193127
1085.380149	72.433175	49.198132
1081.977171	77.230715	49.203137
1078.193977	85.042321	49.208141
1074.860192	76.585917	49.213146
1071.249245	82.966036	49.218151
1067.796627	75.126067	49.223156
1064.501306	76.214835	49.228161
1061.026407	81.732238	49.233165
1057.835519	80.011219	49.238170
1053.738708	80.389535	49.243175
1050.305490	77.842553	49.248180
1046.723983	81.342304	49.253185
1042.999705	88.046944	49.258189
1039.761044	77.386471	49.263194
1036.404982	84.191978	49.268199
1032.935670	77.357500	49.273204
1029.747891	84.089358	49.278209
1025.682834	89.704957	49.283213
1022.325597	85.985078	49.288218
1018.967194	82.989865	49.293223
1015.261237	86.372954	49.298228
1012.178190	82.243410	49.303233
1008.292297	79.817515	49.308237
1004.679745	82.331870	49.313242
1000.958848	84.698580	49.318247
997.726116	78.608711	49.323252
994.500461	84.296124	49.328257
991.049325	81.305860	49.333261
987.615747	79.477097	49.338266
983.876900	81.359395	49.343271
980.272398	79.418038	49.348276
976.709589	84.183521	49.353281
972.840579	91.122663	49.358285
970.270166	80.994080	49.363290
967.056355	79.804975	49.368295
963.050144	82.611560	49.373300
959.327763	77.876044	49.378305
955.724438	94.695132	49.383309
952.185393	82.502753	49.388314
948.727721	86.729865	49.393319
945.151333	78.463105	49.398324
941.759779	82.388866	49.403329
937.828871	85.800650	49.408333
934.624228	84.964454	49.413338
931.513687	79.785696	49.418343
927.811221	83.734547	49.423348
924.794795	78.161499	49.428353
920.824781	92.032170	49.433357
917.274942	82.014928	49.438362
913.827630	87.815943	49.443367
909.910533	78.045694	49.448372
907.033494	79.524936	49.453377
903.325954	75.166761	49.458381
899.718896	76.516038	49.463386
896.182891	74.434319	49.468391
892.707001	83.909648	49.473396
889.226948	79.889377	49.478401
885.442579	94.756183	49.483405
882.517127	76.742050	49.488410
878.785677	87.560597	49.493415
875.011246	80.795788	49.498420
871.967125	76.717152	49.503425
868.090994	80.449438	49.508429
864.954144	83.076414	49.513434
861.435322	75.828904	49.518439
857.616596	77.008660	49.523444
854.455179	77.908929	49.528449
850.491793	80.895518	49.533453
847.273403	66.919564	49.538458
843.583161	80.522055	49.543463
840.018924	75.391792	49.548468
836.681714	74.218748	49.553473
833.566290	76.494386	49.558477
830.105203	74.894548	49.563482
826.211795	75.241231	49.568487
822.511583	79.243523	49.573492
819.278471	69.816068	49.578497
815.616539	76.223120	49.583501
812.439710	77.242849	49.588506
808.634937	80.571737	49.593511
805.269622	77.315046	49.598516
802.114992	74.050869	49.603521
797.952243	74.458465	49.608525
794.829124	75.922241	49.613530
790.765744	72.277522	49.618535
787.366528	77.653450	49.623540
784.290476	76.268921	49.628545
780.765465	78.886727	49.633549
777.280506	72.908924	49.638554
773.877193	75.976009	49.643559
770.390803	78.692205	49.648564
766.771568	73.105457	49.653569
763.175152	84.358555	49.658573
759.664734	72.946362	49.663578
755.907119	77.932006	49.668583
752.376239	78.465868	49.673588
749.110709	74.684301	49.678593
745.737441	76.028838	49.683597
742.562317	70.720964	49.688602
738.802713	71.091121	49.693607
735.149712	76.797617	49.698612
731.997296	67.041251	49.703617
727.874663	76.579297	49.708621
724.473776	75.634473	49.713626
720.733516	78.630633	49.718631
717.113844	84.977334	49.723636
714.061714	77.910295	49.728641
710.529614	77.650270	49.733645
707.111996	77.881775	49.738650
703.972620	85.283141	49.743655
700.388458	81.187358	49.748660
696.869712	75.556505	49.753665
692.494467	77.493612	49.758669
689.321107	82.192165	49.763674
686.115341	78.736652	49.768679
682.670304	78.991410	49.773684
679.086464	74.167939	49.778689
675.393790	89.653201	49.783693
672.432077	75.602524	49.788698
668.952879	78.472631	49.793703
664.880446	82.210187	49.798708
661.411463	71.149062	49.803713
657.473791	79.427653	49.808717
654.185851	71.821548	49.813722
651.144708	77.606804	49.818727
647.693157	77.286793	49.823732
644.154197	69.276854	49.828737
640.801474	82.535749	49.833741
637.496657	71.857186	49.838746
633.545639	74.481214	49.843751
629.895292	76.843308	49.848756
626.496739	66.448255	49.853761
622.634878	81.330278	49.858765
619.938201	74.809020	49.863770
615.980844	72.340530	49.868775
612.667561	76.421808	49.873780
609.122441	65.236513	49.878785
605.212785	66.190016	49.883789
601.904366	67.350471	49.888794
598.705751	63.397166	49.893799
595.084278	77.612194	49.898804
591.650471	72.986839	49.903809
588.387800	71.821206	49.908813
584.412800	72.832339	49.913818
580.755249	75.746037	49.918823
577.311679	71.603082	49.923828
574.198933	72.834317	49.928833
570.599338	77.058244	49.933837
567.355571	72.074287	49.938842
563.503619	69.674816	49.943847
559.715332	70.890998	49.948852
556.792803	62.073292	49.953857
552.775259	69.345620	49.958861
549.209953	60.754527	49.963866
545.943483	70.747740	49.968871
542.186228	72.209022	49.973876
539.119239	60.566509	49.978881
535.391105	67.613455	49.983885
531.966167	61.942722	49.988890
528.266318	67.877983	49.993895
524.881287	65.744344	49.998900
521.466447	76.535756	50.003905
517.925828	66.305208	50.008909
515.116572	68.381356	50.013914
511.064686	66.816591	50.018919
506.913775	71.948903	50.023924
503.779427	71.386546	50.028929
500.404397	75.433154	50.033933
497.087788	72.036055	50.038938
493.326160	74.459779	50.043943
489.908348	78.123918	50.048948
486.369567	69.443286	50.053953
482.190881	74.282541	50.058957
479.229149	67.400785	50.063962
476.353048	74.827609	50.068967
472.752780	83.132780	50.073972
468.830330	72.610515	50.078977
465.609075	76.854645	50.083981
462.088198	70.167503	50.088986
458.532376	67.598566	50.093991
454.438410	76.983475	50.098996
451.287050	69.628222	50.104001
447.604980	79.116684	50.109005
444.335354	70.906671	50.114010
440.788753	74.151116	50.119015
437.162823	69.843590	50.124020
434.172875	72.469880	50.129025
430.162456	74.391357	50.134029
427.247036	68.755211	50.139034
423.675928	70.342549	50.144039
420.395724	66.493719	50.149044
416.376579	67.761677	50.154049
412.369729	70.574754	50.159053
409.220728	65.443198	50.164058
405.545380	69.726388	50.169063
401.972786	68.428700	50.174068
398.946272	64.366377	50.179073
395.453406	72.521955	50.184077
391.998855	65.327807	50.189082
388.248828	66.196380	50.194087
384.920011	62.921419	50.199092
381.100755	64.550558	50.204097
377.758465	67.867602	50.209101
374.487301	61.005567	50.214106
371.065741	63.670583	50.219111
367.144739	60.573237	50.224116
363.895991	72.743460	50.229121
360.087563	68.989528	50.234125
356.797769	66.512066	50.239130
353.554710	70.440069	50.244135
349.549224	74.183058	50.249140
346.376594	69.431666	50.254145
342.467141	65.041752	50.259149
339.006276	66.997904	50.264154
336.128308	60.843432	50.269159
332.475162	63.813417	50.274164
329.001457	62.202962	50.279169
325.119115	70.147103	50.284173
321.640105	62.678377	50.289178
317.932121	63.685942	50.294183
314.566247	67.440085	50.299188
311.388947	62.233861	50.304193
307.800127	69.825432	50.309197
304.354460	65.572122	50.314202
300.852596	69.597368	50.319207
296.976658	66.072251	50.324212
293.787259	67.840617	50.329217
290.133386	73.430232	50.334221
286.747955	66.003888	50.339226
283.123702	67.738718	50.344231
279.824674	66.825553	50.349236
275.910133	66.289780	50.354241
272.778688	74.651682	50.359245
269.376138	65.614541	50.364250
265.891123	67.014494	50.369255
262.352238	64.126587	50.374260
259.128882	68.257168	50.379265
254.924641	73.280758	50.384269
251.342659	64.784068	50.389274
248.269183	65.000018	50.394279
244.944996	74.211316	50.399284
241.640861	56.297458	50.404289
237.583639	68.435367	50.409293
234.083083	69.685889	50.414298
230.517725	61.303673	50.419303
226.777695	67.289508	50.424308
223.942121	69.088215	50.429313
219.938394	78.958952	50.434317
216.735265	61.845594	50.439322
213.502320	73.598922	50.444327
209.477715	70.562024	50.449332
206.324063	70.606969	50.454337
202.516679	74.822156	50.459341
198.858770	67.922291	50.464346
195.748174	62.161553	50.469351
192.258556	67.491492	50.474356
188.907656	58.098329	50.479361
184.911566	68.723988	50.484365
181.827902	71.924860	50.489370
178.278521	66.532985	50.494375
174.642594	69.747075	50.499380
170.933966	66.319316	50.504385
167.111604	60.735835	50.509389
163.870699	63.492967	50.514394
160.543755	72.119422	50.519399
157.462861	67.774546	50.524404
154.291289	59.495549	50.529409
150.141085	64.738520	50.534413
146.562867	56.038798	50.539418
143.037538	57.846827	50.544423
139.216526	72.317546	50.549428
136.005662	60.934796	50.554433
132.229228	58.529972	50.559437
129.198673	61.776361	50.564442
125.529416	60.430493	50.569447
122.089661	67.790069	50.574452
118.587993	63.672058	50.579457
114.813245	73.795043	50.584461
111.542769	66.746294	50.589466
108.479115	60.345533	50.594471
104.710443	67.069808	50.599476
101.181242	62.086082	50.604481
97.465353	72.800998	50.609485
93.864278	72.782745	50.614490
90.380034	72.983576	50.619495
86.659034	68.200551	50.624500
83.370754	60.654724	50.629505
80.267577	68.214993	50.634509
76.779989	61.459475	50.639514
72.843297	63.983273	50.644519
69.243754	66.324869	50.649524
65.846586	65.930035	50.654529
62.353984	65.227367	50.659533
58.756351	69.498496	50.664538
55.843995	64.010628	50.669543
52.291452	67.455352	50.674548
48.897222	61.786255	50.679553
44.798659	74.326073	50.684557
41.453192	70.139464	50.689562
38.145171	59.720961	50.694567
34.176491	63.980261	50.699572
31.359488	60.230216	50.704577
27.113707	69.176901	50.709581
23.771814	69.384051	50.714586
20.547485	62.884940	50.719591
16.757377	74.813605	50.724596
13.752556	64.930010	50.729601
9.904219	65.304596	50.734605
6.611355	63.352833	50.739610
3.098404	68.461805	50.744615