Number of Data Points = 25
        
File	hc(nm)	Pmax(N)	S(N/nm)	A(nm^2)	hmax(nm)	heff(nm)	Er(GPa)	H(GPa)	A	hf(nm)	m	X(mm)	Y(mm)	Drift(nm/s)
3927_Position 120_00000.hld	2810.327397	261226.362342	273.066005	198050825.087989	3520.665340	3527.808769	17.191514	1.318986	0.000000	-1260.464367	5.005294	-129.598000	-52.099000	0.003999
3927_Position 120_00001.hld	2817.688841	273619.603969	287.706063	199074963.053677	3520.866916	3530.967875	18.066562	1.374455	0.000000	-708.394334	4.457613	-129.548000	-52.099000	-0.281618
3927_Position 120_00002.hld	2821.740565	290470.072087	308.662695	199639777.321251	3520.342868	3527.535460	19.355101	1.454971	0.000000	-446.903311	4.223364	-129.498000	-52.099000	-0.301737
3927_Position 120_00003.hld	2831.862428	304515.543131	330.763292	201054283.233319	3518.241879	3522.346114	20.667858	1.514594	0.000000	-464.992464	4.331028	-129.448000	-52.099000	-0.306484
3927_Position 120_00004.hld	2850.683222	312168.327441	350.360934	203697764.438234	3518.774319	3518.926232	21.749905	1.532507	0.000000	-450.620066	4.455205	-129.398000	-52.098500	-0.296591
3927_Position 120_00005.hld	2822.480885	273364.139799	288.027455	199743065.430020	3518.322638	3534.298807	18.056470	1.368579	0.000000	-421.790640	4.168295	-129.598000	-52.049000	-0.317157
3927_Position 120_00006.hld	2822.491216	303401.464840	324.192530	199744506.959681	3519.126328	3524.392331	20.323589	1.518948	0.000000	-489.499633	4.288950	-129.548000	-52.049000	-0.308206
3927_Position 120_00007.hld	2839.559637	310781.070497	342.369115	202133303.699380	3518.911637	3520.362293	21.335876	1.537506	0.000000	-471.777197	4.397904	-129.498000	-52.049000	-0.282236
3927_Position 120_00008.hld	2845.442933	325952.221861	365.144070	202959997.534792	3518.563530	3514.943512	22.708783	1.605992	0.000000	-458.666265	4.451389	-129.448000	-52.049000	-0.259731
3927_Position 120_00009.hld	2869.033618	329693.286785	384.121311	206291856.296594	3517.041985	3512.762457	23.695299	1.598189	0.000000	-431.158357	4.595010	-129.398000	-52.049000	-0.261074
3927_Position 120_00010.hld	2820.579083	319216.793439	341.570679	199477783.587855	3519.004054	3521.495788	21.427334	1.600262	0.000000	-515.639907	4.319845	-129.598000	-51.999000	-0.257785
3927_Position 120_00011.hld	2843.180045	323064.728528	359.214312	202641826.552906	3518.451720	3517.703689	22.357535	1.594265	0.000000	-478.167094	4.442992	-129.548000	-51.999000	-0.251101
3927_Position 120_00012.hld	2849.868244	332240.555923	375.264496	203582937.656282	3517.482260	3513.881013	23.302452	1.631967	0.000000	-465.895110	4.495143	-129.498000	-51.999000	-0.206753
3927_Position 120_00013.hld	2855.666529	353627.148235	406.728159	204400597.376239	3518.308959	3507.749143	25.205655	1.730069	0.000000	-424.535394	4.522760	-129.448000	-51.999000	-0.145232
3927_Position 120_00014.hld	2869.111557	363783.194892	430.103772	206302909.207668	3518.365020	3503.464041	26.531109	1.763345	0.000000	-378.882655	4.590129	-129.398000	-51.999000	-0.139729
3927_Position 120_00015.hld	2897.413127	270359.754620	318.928968	210336138.636253	3515.934515	3533.196753	19.483719	1.285370	0.000000	-377.845262	4.613647	-129.598000	-51.949000	-0.194039
3927_Position 120_00016.hld	2861.620526	341179.764911	394.017345	205241926.550657	3518.349244	3511.045804	24.367845	1.662330	0.000000	-445.337582	4.569098	-129.548000	-51.949000	-0.121376
3927_Position 120_00017.hld	2870.424883	355943.520686	420.028984	206489203.180656	3517.720410	3505.994452	25.897952	1.723788	0.000000	-400.628836	4.609987	-129.498000	-51.949000	-0.088640
3927_Position 120_00018.hld	2889.495476	358188.055820	436.029034	209203854.927512	3517.805853	3505.603627	26.709478	1.712148	0.000000	-383.208155	4.733923	-129.448000	-51.949000	-0.086984
3927_Position 120_00019.hld	2899.721286	375165.092311	469.102026	210666799.862612	3518.860135	3499.534980	28.635455	1.780846	0.000000	-579.372512	5.100218	-129.398000	-51.949000	-0.101330
3927_Position 120_00020.hld	2872.606042	355135.359877	419.166243	206798784.868199	3517.668791	3508.037745	25.825405	1.717299	0.000000	-413.053503	4.628064	-129.598000	-51.899000	-0.127066
3927_Position 120_00021.hld	2881.507431	361015.297765	432.856376	208064611.477634	3517.767807	3507.030094	26.587625	1.735111	0.000000	-400.616184	4.685257	-129.548000	-51.899000	-0.048378
3927_Position 120_00022.hld	2896.821196	368366.713314	455.064102	210251381.971723	3517.599052	3503.933543	27.805965	1.752030	0.000000	-360.764083	4.774278	-129.498000	-51.899000	-0.069106
3927_Position 120_00023.hld	2906.057260	379230.405842	478.514958	211575815.732672	3517.992102	3500.443704	29.147233	1.792409	0.000000	-477.559228	5.019465	-129.448000	-51.899000	-0.047723
3927_Position 120_00024.hld	2921.675780	384575.603594	500.360130	213824975.031216	3517.927408	3498.123993	30.317146	1.798553	0.000000	-680.877593	5.437177	-129.398000	-51.899000	-0.044060