Fri Aug 26 13:30:07 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.821297	96.007221	0.000000
0.654991	96.767065	0.005005
0.273235	86.674327	0.010010
0.379917	88.185744	0.015014
0.442449	79.020386	0.020019
-0.128595	81.377616	0.025024
-0.360858	75.655919	0.030029
-0.605780	72.331077	0.035034
-1.009156	61.779827	0.040038
-1.138167	50.078590	0.045043
-1.083382	47.409418	0.050048
-1.423461	45.231982	0.055053
-1.869013	33.984986	0.060058
-2.371516	35.739937	0.065062
-2.668327	23.511206	0.070067
-2.950854	22.776922	0.075072
-2.936022	17.747574	0.080077
-2.853066	20.221261	0.085082
-3.699976	14.756628	0.090086
-3.512751	2.354477	0.095091
-3.645430	6.778899	0.100096
-4.214996	8.987199	0.105101
-4.466501	5.128740	0.110106
-5.075324	0.379988	0.115110
-5.041055	-1.105946	0.120115
-5.996125	3.253537	0.125120
-6.317497	0.098794	0.130125
-6.555913	0.487061	0.135130
-6.719824	3.109910	0.140134
-6.883689	-2.499029	0.145139
-6.845157	9.339609	0.150144
-6.749125	3.437112	0.155149
-6.333569	-4.615785	0.160154
-6.845055	7.200924	0.165158
-7.406770	7.437055	0.170163
-8.155883	15.076802	0.175168
-8.755795	13.094843	0.180173
-9.143177	3.793939	0.185178
-9.503707	8.272819	0.190182
-9.302639	-6.548499	0.195187
-9.402599	3.138280	0.200192
-9.511231	1.892886	0.205197
-9.425265	-0.591315	0.210202
-9.663882	6.633601	0.215206
-9.689124	1.417515	0.220211
-10.684193	-2.008809	0.225216
-10.874332	0.807941	0.230221
-10.935811	-8.198862	0.235226
-11.291670	-0.844968	0.240230
-11.699101	-8.168636	0.245235
-11.981887	-3.429791	0.250240
-12.041350	-3.613531	0.255245
-12.061435	-7.574454	0.260250
-12.583711	-0.068104	0.265254
-12.714440	-1.889002	0.270259
-13.587857	4.833658	0.275264
-13.635695	-3.175563	0.280269
-13.567777	1.299881	0.285274
-14.121240	6.280181	0.290278
-13.695202	4.866122	0.295283
-14.062584	3.572433	0.300288
-14.371636	4.509517	0.305293
-14.817486	-2.010936	0.310298
-15.154210	10.145546	0.315302
-15.086084	2.206849	0.320307
-15.352913	5.032376	0.325312
-15.870220	6.473266	0.330317
-16.427301	6.278422	0.335322
-16.968446	7.204187	0.340326
-16.933913	4.971593	0.345331
-17.187361	15.742094	0.350336
-16.872936	7.685956	0.355341
-16.852958	3.073411	0.360346
-17.285310	9.199074	0.365350
-17.744623	-1.226373	0.370355
-18.200214	3.824106	0.375360
-18.478509	-1.257670	0.380365
-18.670557	-1.677022	0.385370
-18.942556	9.782873	0.390374
-18.545029	3.463289	0.395379
-19.272320	9.530473	0.400384
-19.798156	5.986800	0.405389
-19.970577	-0.266188	0.410394
-19.960506	12.364626	0.415398
-19.861099	3.769350	0.420403
-20.801620	4.883842	0.425408
-21.419441	6.881363	0.430413
-21.105437	8.651548	0.435418
-21.671171	1.801761	0.440422
-21.273439	8.127199	0.445427
-21.866186	10.104999	0.450432
-22.051607	6.720288	0.455437
-21.927841	1.885947	0.460442
-22.635528	9.898878	0.465446
-22.861632	2.626066	0.470451
-22.955790	3.292418	0.475456
-23.270011	2.816161	0.480461
-23.616536	0.756789	0.485466
-24.338096	7.825952	0.490470
-24.086153	-2.314780	0.495475
-24.144211	1.984132	0.500480
-24.787399	2.685348	0.505485
-24.536648	1.140400	0.510490
-24.783658	4.408913	0.515494
-25.656310	3.927857	0.520499
-26.527133	6.651279	0.525504
-26.040655	10.254828	0.530509
-26.135978	6.400526	0.535514
-26.084942	9.072163	0.540518
-26.179143	6.616013	0.545523
-26.125119	5.667985	0.550528
-26.742178	9.604697	0.555533
-26.872771	3.889341	0.560538
-27.801338	9.440553	0.565542
-28.294489	1.193793	0.570547
-28.647253	9.917063	0.575552
-28.897243	2.663788	0.580557
-28.403699	4.333254	0.585562
-28.625647	7.825648	0.590566
-29.112237	-1.757187	0.595571
-28.757541	-2.141447	0.600576
-29.420869	4.599121	0.605581
-29.780458	-3.652614	0.610586
-30.292328	14.409172	0.615590
-30.140350	6.264438	0.620595
-30.493364	7.996111	0.625600
-31.001326	7.967619	0.630605
-31.227948	5.177760	0.635610
-31.528782	5.585237	0.640614
-31.261484	3.272112	0.645619
-31.699345	4.415905	0.650624
-32.373520	9.522564	0.655629
-32.543418	4.670673	0.660634
-33.103704	12.268364	0.665638
-33.072471	-1.577422	0.670643
-33.242301	6.930710	0.675648
-33.431054	10.231281	0.680653
-33.243249	0.255553	0.685658
-33.514040	6.770496	0.690662
-33.909950	3.703285	0.695667
-34.226820	11.557295	0.700672
-34.827463	16.127343	0.705677
-34.769220	8.664729	0.710682
-35.107259	14.737745	0.715686
-35.146426	1.393282	0.720691
-35.786453	0.559644	0.725696
-35.977876	9.204011	0.730701
-35.723080	1.897452	0.735706
-36.091884	10.813037	0.740710
-36.385941	9.463641	0.745715
-37.229364	3.963671	0.750720
-37.470160	7.474818	0.755725
-37.467838	-6.167154	0.760730
-37.544953	13.332829	0.765734
-37.749570	-0.036490	0.770739
-38.296791	-1.191451	0.775744
-38.963653	-2.523929	0.780749
-38.909099	1.672031	0.785754
-39.180478	4.881066	0.790758
-39.226838	-0.929657	0.795763
-38.984170	3.373050	0.800768
-39.293881	-1.786088	0.805773
-39.068436	-0.093862	0.810778
-40.189621	1.842832	0.815782
-40.678761	7.914062	0.820787
-40.569350	5.207920	0.825792
-40.878602	1.918418	0.830797
-40.776781	-2.529704	0.835802
-41.617211	1.872039	0.840806
-41.827745	1.202475	0.845811
-42.298844	5.255660	0.850816
-42.306998	12.995167	0.855821
-41.947094	6.428350	0.860826
-42.425562	7.872684	0.865830
-43.028328	-1.252316	0.870835
-43.674400	8.342329	0.875840
-43.590897	3.258003	0.880845
-43.431378	-1.142158	0.885850
-43.709181	4.646240	0.890854
-43.853208	-3.091748	0.895859
-44.489659	4.400743	0.900864
-45.137422	11.603945	0.905869
-44.908610	5.478303	0.910874
-45.283475	10.487742	0.915878
-45.337106	6.585821	0.920883
-45.525621	8.791737	0.925888
-45.657032	4.525455	0.930893
-46.019759	6.894531	0.935898
-46.726681	10.127090	0.940902
-46.790908	6.856382	0.945907
-46.912997	6.650757	0.950912
-47.213649	7.599187	0.955917
-46.873909	7.932237	0.960922
-47.415142	10.275325	0.965926
-47.867525	7.125162	0.970931
-48.195300	3.208981	0.975936
-48.458171	9.988436	0.980941
-48.310255	11.224516	0.985946
-49.577733	18.211008	0.990950
-49.568913	4.637618	0.995955
-49.797486	5.366026	1.000960
-49.763055	8.037084	1.005965
-50.027531	10.536391	1.010970
-50.115995	11.407493	1.015974
-49.956545	7.991232	1.020979
-50.001994	8.931564	1.025984
-50.765489	5.399587	1.030989
-50.622867	13.150418	1.035994
-51.756190	9.084421	1.040998
-52.483420	5.856834	1.046003
-52.184908	6.382957	1.051008
-52.075241	9.361828	1.056013
-52.356282	10.727969	1.061018
-52.950374	9.589797	1.066022
-52.489217	8.872597	1.071027
-52.896514	18.164324	1.076032
-53.401493	16.569367	1.081037
-53.495339	7.861817	1.086042
-54.162122	12.258671	1.091046
-54.010629	15.110813	1.096051
-54.007248	14.771760	1.101056
-54.489550	16.874728	1.106061
-55.119555	8.548039	1.111066
-55.595233	18.612848	1.116070
-55.841671	10.751601	1.121075
-55.854888	6.770625	1.126080
-55.912552	7.086459	1.131085
-55.414369	8.119311	1.136090
-56.602129	14.678954	1.141094
-56.851279	18.026894	1.146099
-57.240758	12.260099	1.151104
-57.242353	23.586152	1.156109
-56.751445	7.251772	1.161114
-57.283201	11.472584	1.166118
-57.716813	7.449499	1.171123
-58.319926	9.609240	1.176128
-58.625001	10.659596	1.181133
-58.399398	7.707581	1.186138
-59.221043	9.819093	1.191142
-59.599083	4.743356	1.196147
-59.930699	6.835516	1.201152
-60.176999	13.058756	1.206157
-60.242287	0.784509	1.211162
-60.142732	8.557860	1.216166
-60.051119	6.942780	1.221171
-60.438039	7.850860	1.226176
-60.449078	4.442164	1.231181
-61.356554	4.542312	1.236186
-61.566379	8.709836	1.241190
-61.518548	7.705827	1.246195
-61.608722	0.228363	1.251200
-61.848772	5.093428	1.256205
-62.528467	-6.604279	1.261210
-62.362965	2.269237	1.266214
-62.816496	1.270526	1.271219
-62.827328	0.873578	1.276224
-64.173768	10.922105	1.281229
-63.734299	4.055011	1.286234
-64.080645	1.998776	1.291238
-64.486820	4.811199	1.296243
-64.355182	-4.469270	1.301248
-64.335132	-1.096812	1.306253
-64.388689	-6.634339	1.311258
-65.133833	1.219909	1.316262
-65.279593	4.260694	1.321267
-65.435838	-6.847822	1.326272
-66.057914	6.302171	1.331277
-66.751428	-0.856735	1.336282
-67.349023	7.458579	1.341286
-66.844520	4.143613	1.346291
-66.699955	-0.798363	1.351296
-67.144577	2.678081	1.356301
-67.029766	-3.363370	1.361306
-67.543835	11.585735	1.366310
-68.057585	9.191746	1.371315
-68.589790	1.523688	1.376320
-68.792340	3.576770	1.381325
-68.731827	-3.519208	1.386330
-69.216452	8.230041	1.391334
-69.076066	-1.849028	1.396339
-68.907238	12.139571	1.401344
-69.637774	10.943553	1.406349
-70.112091	3.794808	1.411354
-70.332125	7.195157	1.416358
-70.398775	2.577121	1.421363
-70.502547	-0.396373	1.426368
-70.823426	9.384910	1.431373
-71.517022	1.567981	1.436378
-72.096681	7.662795	1.441382
-72.057657	-5.497687	1.446387
-71.902190	-0.127916	1.451392
-72.138232	0.813618	1.456397
-71.638298	-8.163538	1.461402
-72.952331	7.650408	1.466406
-73.439664	7.277032	1.471411
-73.575571	7.329812	1.476416
-73.437168	8.918536	1.481421
-73.645008	-1.995294	1.486426
-74.000082	1.448225	1.491430
-73.823395	7.849204	1.496435
-73.797935	7.038496	1.501440
-74.472706	10.633030	1.506445
-74.406629	1.185603	1.511450
-75.059034	7.810579	1.516454
-75.613433	4.951538	1.521459
-75.928720	0.995450	1.526464
-76.282405	15.375441	1.531469
-75.881719	2.500316	1.536474
-76.234190	4.386923	1.541478
-76.856292	10.807873	1.546483
-77.452217	9.204933	1.551488
-77.815081	11.112140	1.556493
-77.526513	-2.817997	1.561498
-77.876070	5.452369	1.566502
-77.917701	-1.871306	1.571507
-77.337848	-9.677705	1.576512
-78.170338	7.219153	1.581517
-79.050437	-0.366264	1.586522
-79.175411	17.015206	1.591526
-79.064339	10.942697	1.596531
-79.122926	4.124678	1.601536
-79.767510	1.349279	1.606541
-79.990270	2.728490	1.611546
-80.338542	-0.127844	1.616550
-80.797594	1.221722	1.621555
-80.445576	4.074275	1.626560
-80.827732	6.459031	1.631565
-81.391254	-8.100867	1.636570
-81.778117	-1.868403	1.641574
-82.027937	-0.969014	1.646579
-82.235858	-5.492289	1.651584
-82.250705	2.143852	1.656589
-81.671128	-0.853784	1.661594
-82.602245	0.904627	1.666598
-83.477085	-0.455576	1.671603
-83.389652	-10.649775	1.676608
-83.733239	7.759104	1.681613
-83.465984	-3.605170	1.686618
-83.932096	2.241018	1.691622
-84.192181	4.616258	1.696627
-84.487133	0.492496	1.701632
-85.009730	-1.030115	1.706637
-84.554454	-3.416797	1.711642
-85.093069	11.463364	1.716646
-85.226728	-0.458561	1.721651
-85.723992	-3.608060	1.726656
-86.246502	12.259812	1.731661
-86.292514	2.567256	1.736666
-86.343052	4.280306	1.741670
-86.602844	3.934776	1.746675
-87.029547	0.359854	1.751680
-87.920095	6.259473	1.756685
-87.658660	3.953589	1.761690
-88.013582	4.575124	1.766694
-88.219217	-6.433955	1.771699
-88.164508	2.134118	1.776704
-88.376376	3.163634	1.781709
-88.263107	-16.949409	1.786714
-88.789404	0.083257	1.791718
-89.389086	2.429118	1.796723
-89.366823	-5.268321	1.801728
-89.856858	0.059591	1.806733
-89.740157	0.490640	1.811738
-90.542872	0.985751	1.816742
-90.948588	3.633593	1.821747
-90.960055	1.512563	1.826752
-91.017226	10.284715	1.831757
-91.010674	0.818084	1.836762
-90.715252	-3.302689	1.841766
-91.545165	0.632362	1.846771
-91.963457	0.814528	1.851776
-92.618176	-0.877329	1.856781
-92.388265	-7.813025	1.861786
-92.718313	2.820698	1.866790
-93.715126	2.033122	1.871795
-93.541132	-8.487755	1.876800
-94.083240	-2.632900	1.881805
-93.633348	-8.641103	1.886810
-94.041669	-2.481225	1.891814
-94.089252	3.176416	1.896819
-93.895654	0.982330	1.901824
-94.521512	6.249137	1.906829
-95.315978	-9.072036	1.911834
-95.407282	-0.338867	1.916838
-95.546850	2.998335	1.921843
-95.452683	-1.186012	1.926848
-95.846095	5.139219	1.931853
-96.404939	-1.771742	1.936858
-96.968364	1.982617	1.941862
-97.209068	-1.820572	1.946867
-97.102452	-4.355441	1.951872
-97.559106	7.266068	1.956877
-97.531557	-7.363713	1.961882
-97.589891	-2.900253	1.966886
-97.658464	3.627491	1.971891
-97.886750	-2.097958	1.976896
-98.294139	1.999088	1.981901
-98.329765	-5.335010	1.986906
-99.112387	-4.270409	1.991910
-99.576077	-13.255706	1.996915
-99.928418	-6.154578	2.006912
-99.181921	-11.019197	2.016909
-98.980065	0.983367	2.026906
-98.306641	3.127537	2.036902
-97.662646	4.531883	2.046899
-97.650507	5.122316	2.056896
-96.709545	0.911635	2.066893
-96.453994	-0.990786	2.076890
-95.847899	0.970638	2.086886
-94.788044	2.554147	2.096883
-94.901195	2.445023	2.106880
-94.728713	7.381896	2.116877
-93.922049	2.935543	2.126874
-93.304956	9.073431	2.136870
-92.549567	8.990628	2.146867
-91.822322	13.315290	2.156864
-91.926333	7.141793	2.166861
-91.751394	7.386943	2.176858
-90.694037	2.648142	2.186854
-90.482221	7.398332	2.196851
-89.696675	11.989505	2.206848
-89.031545	9.560829	2.216845
-89.191876	7.748502	2.226842
-88.048700	9.147983	2.236838
-88.013115	6.370684	2.246835
-87.273738	-0.669029	2.256832
-86.618533	10.550228	2.266829
-86.312376	6.520745	2.276826
-85.775573	6.905949	2.286822
-84.880989	4.656950	2.296819
-85.075935	8.387126	2.306816
-84.452076	4.266997	2.316813
-83.431405	2.654078	2.326810
-83.113808	8.559843	2.336806
-83.303141	8.136309	2.346803
-82.180998	13.074203	2.356800
-81.669771	7.384600	2.366797
-81.353085	5.684895	2.376794
-80.483088	9.553357	2.386790
-80.356995	8.019537	2.396787
-79.836051	15.068855	2.406784
-79.467448	4.957194	2.416781
-78.702849	10.577959	2.426778
-77.659715	10.843148	2.436774
-77.483252	5.278524	2.446771
-77.196245	9.773097	2.456768
-76.953092	9.560982	2.466765
-76.437596	4.580276	2.476762
-75.921019	-4.059271	2.486758
-75.323850	12.883527	2.496755
-74.972522	5.391065	2.506752
-74.397842	2.346104	2.516749
-73.631753	5.242427	2.526746
-73.289388	10.963779	2.536742
-73.070312	10.454482	2.546739
-72.410090	9.166938	2.556736
-71.262444	7.185803	2.566733
-71.000652	3.375463	2.576730
-70.681232	14.254213	2.586726
-70.652846	17.091175	2.596723
-69.628039	20.004237	2.606720
-69.304059	14.692231	2.616717
-68.906269	8.431099	2.626714
-67.964583	7.559046	2.636710
-67.782588	11.962269	2.646707
-67.287899	8.546471	2.656704
-66.509675	9.530791	2.666701
-66.395237	9.668156	2.676698
-65.773102	6.761519	2.686694
-65.212302	9.873532	2.696691
-65.222977	9.133922	2.706688
-64.428692	7.391532	2.716685
-63.474426	9.279742	2.726682
-63.000630	8.857493	2.736678
-62.543151	6.549845	2.746675
-62.218979	7.953305	2.756672
-61.789558	13.515391	2.766669
-61.191927	9.465866	2.776666
-60.844871	8.208075	2.786662
-60.175000	11.509006	2.796659
-59.341946	9.684555	2.806656
-59.487988	3.476422	2.816653
-58.606906	5.746646	2.826650
-57.904092	7.724690	2.836646
-57.988245	8.117881	2.846643
-57.405615	6.430619	2.856640
-56.419904	3.828490	2.866637
-56.494110	2.769333	2.876634
-55.776838	13.161669	2.886630
-55.025660	12.575860	2.896627
-54.702162	4.416181	2.906624
-54.180683	3.029867	2.916621
-53.401548	10.447616	2.926618
-53.452276	7.465185	2.936614
-52.737066	9.564839	2.946611
-52.109628	4.075713	2.956608
-51.872974	0.839470	2.966605
-50.873993	6.496600	2.976602
-50.775886	5.645022	2.986598
-50.459159	1.392156	2.996595
-49.238462	-2.098666	3.006592
-49.154805	4.505570	3.016589
-48.986330	7.463265	3.026586
-47.707291	3.969694	3.036582
-47.673333	4.034062	3.046579
-47.597974	8.577428	3.056576
-46.502785	5.223350	3.066573
-46.150564	5.700648	3.076570
-45.958343	8.350548	3.086566
-45.035668	13.772482	3.096563
-44.696595	5.379136	3.106560
-44.164425	3.468490	3.116557
-43.331488	4.374603	3.126554
-43.109526	7.599559	3.136550
-43.168549	9.832432	3.146547
-41.837722	9.001157	3.156544
-41.463165	3.640098	3.166541
-41.503120	-2.882314	3.176538
-40.734117	8.819723	3.186534
-40.301702	7.846405	3.196531
-39.468015	4.929004	3.206528
-38.806161	2.323449	3.216525
-38.892993	5.485615	3.226522
-38.303315	1.399318	3.236518
-37.226666	-3.158759	3.246515
-37.335756	3.339277	3.256512
-36.913569	1.176501	3.266509
-35.832712	0.871970	3.276506
-35.609408	-0.930400	3.286502
-35.179344	-5.327619	3.296499
-34.221495	-4.307912	3.306496
-34.089262	-0.258058	3.316493
-34.029099	-0.482862	3.326490
-33.268420	2.404802	3.336486
-33.035224	0.984182	3.346483
-31.820975	0.744410	3.356480
-31.366016	-0.450988	3.366477
-31.371263	1.247674	3.376474
-30.447448	-0.831651	3.386470
-30.132214	3.972129	3.396467
-29.910347	2.698986	3.406464
-28.990936	-9.218483	3.416461
-28.752160	0.732017	3.426458
-28.361890	-0.830264	3.436454
-27.464000	2.213428	3.446451
-27.118545	1.278991	3.456448
-26.599486	2.737637	3.466445
-26.125109	5.197893	3.476442
-25.835349	0.480407	3.486438
-24.882798	5.970546	3.496435
-24.410984	6.917047	3.506432
-24.017607	11.170156	3.516429
-24.058947	2.047285	3.526426
-23.417366	4.063373	3.536422
-22.336468	4.043928	3.546419
-21.570194	4.627814	3.556416
-21.545387	0.268350	3.566413
-21.460573	6.299056	3.576410
-20.586744	5.624463	3.586406
-20.256486	6.152696	3.596403
-19.694626	3.122402	3.606400
-18.692319	4.179536	3.616397
-18.636573	4.861378	3.626394
-18.280685	3.469170	3.636390
-17.917062	4.837981	3.646387
-17.097936	3.782279	3.656384
-16.337754	5.225557	3.666381
-15.883265	8.689900	3.676378
-15.553920	3.982088	3.686374
-15.539783	6.805430	3.696371
-14.665462	9.060872	3.706368
-14.088948	4.640848	3.716365
-12.846966	6.658487	3.726362
-13.221158	4.952312	3.736358
-12.682659	5.359428	3.746355
-12.271763	4.652379	3.756352
-11.557258	2.035459	3.766349
-11.016208	1.852987	3.776346
-10.884266	1.582163	3.786342
-9.922481	0.551766	3.796339
-9.403405	3.356676	3.806336
-9.318356	-5.655995	3.816333
-8.438529	-1.484962	3.826330
-7.944067	3.151535	3.836326
-7.695296	9.682552	3.846323
-6.972967	-2.112375	3.856320
-6.575691	2.136958	3.866317
-6.248455	3.821867	3.876314
-5.632091	6.196664	3.886310
-5.224545	11.147627	3.896307
-4.500467	10.030700	3.906304
-4.216195	13.138256	3.916301
-3.826412	28.307788	3.926298
-3.314911	31.924811	3.936294
-2.769864	37.095118	3.946291
-2.595367	43.963984	3.956288
-1.977466	56.586042	3.966285
-1.388067	68.731057	3.976282
-1.289588	86.277420	3.986278
-0.428391	92.602246	3.996275
-0.001890	106.641594	4.006272
0.000000	119.659196	4.011277
0.044602	137.571196	4.016282
0.560672	142.112937	4.021286
0.867241	141.258455	4.026291
0.172732	152.312841	4.031296
1.176917	160.540184	4.036301
1.149962	167.744865	4.041306
1.219796	167.971250	4.046310
1.647777	170.666479	4.051315
1.394188	176.957350	4.056320
1.570320	167.470548	4.061325
1.291078	164.223796	4.066330
1.236303	172.223727	4.071334
1.741365	169.009881	4.076339
1.184386	160.152903	4.081344
1.437722	155.649513	4.086349
1.569915	161.627221	4.091354
1.127242	154.033733	4.096358
1.142581	156.774224	4.101363
1.399644	166.668089	4.106368
1.735281	169.380859	4.111373
1.732579	170.498037	4.116378
1.073996	152.327234	4.121382
1.280876	161.039372	4.126387
1.303171	173.434289	4.131392
1.497432	165.393625	4.136397
1.402798	172.558226	4.141402
1.662788	171.673031	4.146406
1.511217	172.737460	4.151411
1.209190	174.571939	4.156416
1.448240	174.003207	4.161421
1.103889	170.076912	4.166426
1.719107	172.141892	4.171430
1.652910	167.849596	4.176435
1.868470	179.983479	4.181440
1.735205	162.648339	4.186445
1.722619	169.180087	4.191450
1.637143	167.883620	4.196454
1.952255	173.940417	4.201459
1.606881	162.633451	4.206464
1.434412	152.365725	4.211469
1.431698	155.219755	4.216474
1.861416	161.726926	4.221478
1.928873	167.777988	4.226483
1.405916	164.787475	4.231488
1.589339	165.141704	4.236493
1.697975	173.457868	4.241498
1.718131	166.779378	4.246502
1.759627	176.978888	4.251507
1.748530	179.676043	4.256512
1.931133	170.529908	4.261517
1.699005	169.246784	4.266522
2.022809	172.059470	4.271526
1.865312	171.909973	4.276531
1.549320	173.177166	4.281536
1.510070	161.911121	4.286541
1.543024	176.553745	4.291546
1.523661	170.074391	4.296550
1.539224	170.438936	4.301555
1.770824	177.701439	4.306560
1.500641	179.474015	4.311565
1.822447	180.926636	4.316570
2.375551	178.467752	4.321574
2.281973	171.307109	4.326579
1.554294	179.063808	4.331584
1.873624	172.829104	4.336589
1.973061	171.908796	4.341594
2.066020	179.015720	4.346598
2.108148	174.668593	4.351603
2.135381	175.474235	4.356608
2.142695	175.840065	4.361613
1.945383	183.548990	4.366618
1.689293	179.846226	4.371622
2.030631	171.371383	4.376627
1.898255	174.751790	4.381632
1.985732	172.900063	4.386637
1.874217	180.832904	4.391642
2.165238	182.157445	4.396646
2.341954	169.146225	4.401651
2.216980	183.645770	4.406656
2.095947	174.195741	4.411661
2.144904	168.828851	4.416666
2.200485	179.567156	4.421670
2.087233	170.406975	4.426675
1.968425	182.643538	4.431680
1.786071	181.004660	4.436685
2.099780	192.655047	4.441690
2.329763	195.010958	4.446694
2.638988	200.204998	4.451699
2.422710	202.355151	4.456704
2.147278	182.273914	4.461709
2.276872	181.668441	4.466714
2.320524	192.911635	4.471718
2.555925	187.860551	4.476723
1.993537	186.173277	4.481728
2.608529	189.124122	4.486733
2.267255	189.753028	4.491738
2.222813	192.297194	4.496742
2.446253	194.242846	4.501747
2.359113	201.415783	4.506752
2.497786	193.364779	4.511757
2.123550	189.218512	4.516762
2.472817	195.523092	4.521766
2.848036	195.344436	4.526771
1.866140	196.503344	4.531776
2.327181	195.640627	4.536781
2.695312	197.639680	4.541786
2.596555	199.338112	4.546790
2.901889	197.746684	4.551795
2.303313	194.951432	4.556800
2.373654	189.451496	4.561805
2.550908	202.787226	4.566810
2.265753	205.365708	4.571814
2.465611	203.486990	4.576819
2.534148	204.165982	4.581824
2.534644	199.100850	4.586829
2.424770	209.751042	4.591834
2.452511	207.184131	4.596838
2.822115	203.238415	4.601843
2.342286	209.320919	4.606848
2.720320	199.442006	4.611853
2.521680	205.521857	4.616858
2.373071	201.947883	4.621862
2.694286	200.300200	4.626867
2.613882	209.212112	4.631872
2.626200	204.069209	4.636877
2.741764	202.175142	4.641882
2.477284	204.108180	4.646886
2.671734	204.261381	4.651891
2.653341	214.694857	4.656896
2.552715	206.848780	4.661901
2.748739	199.997366	4.666906
2.419365	210.460277	4.671910
3.065236	215.285540	4.676915
2.944584	226.494226	4.681920
2.903921	214.839235	4.686925
2.602338	209.995134	4.691930
2.875602	215.985697	4.696934
3.142547	225.188376	4.701939
2.995609	210.345131	4.706944
3.175302	202.736977	4.711949
2.830707	205.505043	4.716954
2.688102	196.564548	4.721958
2.952748	201.578873	4.726963
2.716153	203.444296	4.731968
2.891945	196.567560	4.736973
2.863845	208.631835	4.741978
3.250389	220.726470	4.746982
3.132614	209.257490	4.751987
2.637791	207.834935	4.756992
2.836919	224.555569	4.761997
3.000277	227.121168	4.767002
2.997522	228.130793	4.772006
3.149639	215.474537	4.777011
3.039636	225.523660	4.782016
3.178942	232.917612	4.787021
3.045592	227.961894	4.792026
2.828121	228.856256	4.797030
3.462878	236.201542	4.802035
3.299192	230.216024	4.807040
3.186172	228.303761	4.812045
3.049833	231.896763	4.817050
3.022964	237.643004	4.822054
3.230000	229.549703	4.827059
2.951823	235.951988	4.832064
2.950211	236.603940	4.837069
3.246176	224.614963	4.842074
3.230835	231.087052	4.847078
3.303330	233.919894	4.852083
3.171648	239.552744	4.857088
3.068670	234.481566	4.862093
3.092478	224.569208	4.867098
3.112303	232.263329	4.872102
3.375333	230.871469	4.877107
3.295234	232.532199	4.882112
3.025010	226.455705	4.887117
3.129499	214.575639	4.892122
3.092636	235.382529	4.897126
2.956678	228.143042	4.902131
3.365327	243.587747	4.907136
3.841839	245.854662	4.912141
3.380417	238.042600	4.917146
3.238346	233.173657	4.922150
3.108496	227.002543	4.927155
3.418778	248.508354	4.932160
3.654556	242.492273	4.937165
3.670075	246.586805	4.942170
3.353067	249.882080	4.947174
3.719952	243.238160	4.952179
3.362691	245.840529	4.957184
3.490057	250.765513	4.962189
3.317490	247.331299	4.967194
3.661129	254.826320	4.972198
4.056049	247.387113	4.977203
3.394601	240.713481	4.982208
3.457576	241.589489	4.987213
3.385421	249.427649	4.992218
3.780571	255.237900	4.997222
3.707783	253.844541	5.002227
3.509194	242.252085	5.007232
3.658432	252.491809	5.012237
4.085124	250.922609	5.017242
3.473643	247.148617	5.022246
3.650286	233.643828	5.027251
3.267453	251.828132	5.032256
3.619991	256.737042	5.037261
3.825192	258.315390	5.042266
3.556257	256.943080	5.047270
3.732910	251.559447	5.052275
3.637344	256.088882	5.057280
3.815470	255.042426	5.062285
3.784209	260.789359	5.067290
3.205695	258.139666	5.072294
3.635395	252.694489	5.077299
3.198222	251.016186	5.082304
3.393832	249.065360	5.087309
3.376302	261.843017	5.092314
3.766429	263.987345	5.097318
4.510572	268.949179	5.102323
4.316927	282.175041	5.107328
4.010170	266.464473	5.112333
4.155819	256.033265	5.117338
3.558252	256.566039	5.122342
3.821397	241.877213	5.127347
3.438137	254.275219	5.132352
3.953189	268.156340	5.137357
4.152446	279.479763	5.142362
4.151255	276.075806	5.147366
4.161308	271.607102	5.152371
3.994470	260.354531	5.157376
3.952009	262.793997	5.162381
4.223571	266.405753	5.167386
4.180481	258.746842	5.172390
3.841557	247.385035	5.177395
3.935513	256.785503	5.182400
4.026979	262.168486	5.187405
4.457835	268.767266	5.192410
3.909670	265.831279	5.197414
3.625039	261.572970	5.202419
4.036726	276.087109	5.207424
3.886690	273.437138	5.212429
3.805531	278.502162	5.217434
3.678237	278.572584	5.222438
3.882817	277.964924	5.227443
3.920910	266.689933	5.232448
3.780235	281.739320	5.237453
4.487487	290.427399	5.242458
4.410865	286.845363	5.247462
4.188683	279.375676	5.252467
4.163625	282.571720	5.257472
4.317793	284.452238	5.262477
4.451486	277.151766	5.267482
4.413079	281.764054	5.272486
4.464378	280.500067	5.277491
4.211916	277.245962	5.282496
4.539874	276.900660	5.287501
4.353224	274.208935	5.292506
4.420581	273.606822	5.297510
4.491453	263.190416	5.302515
4.194754	279.852262	5.307520
4.637675	276.891676	5.312525
4.856842	277.104303	5.317530
4.338764	278.478896	5.322534
4.777812	270.624694	5.327539
4.190559	280.520369	5.332544
4.377152	272.825692	5.337549
4.430121	273.361582	5.342554
4.531277	285.930956	5.347558
4.631567	275.380251	5.352563
4.424306	279.202599	5.357568
4.472333	284.481623	5.362573
4.388340	280.002250	5.367578
4.543461	270.550301	5.372582
4.937169	276.250055	5.377587
4.528170	276.706014	5.382592
4.440684	277.928146	5.387597
4.355125	276.150805	5.392602
4.649293	280.616402	5.397606
4.582115	279.785305	5.402611
4.512742	292.340106	5.407616
4.669742	279.989922	5.412621
4.535063	274.047328	5.417626
4.266625	283.890203	5.422630
4.896611	287.933365	5.427635
4.653555	279.147671	5.432640
4.639048	279.880724	5.437645
5.093849	278.655151	5.442650
4.493106	282.750730	5.447654
4.685211	287.384077	5.452659
4.809085	287.510303	5.457664
4.500089	286.131573	5.462669
4.799848	291.412534	5.467674
4.871328	297.561088	5.472678
5.326158	289.853114	5.477683
4.903500	278.418904	5.482688
4.565163	272.735804	5.487693
4.985353	284.600623	5.492698
4.901239	289.789494	5.497702
5.015924	271.874651	5.502707
4.585283	279.835077	5.507712
4.772047	280.796215	5.512717
4.586811	287.057501	5.517722
4.977019	304.257813	5.522726
5.029430	295.840550	5.527731
5.043300	302.377719	5.532736
5.007435	300.836242	5.537741
5.276571	296.877675	5.542746
4.566482	300.066486	5.547750
5.049697	287.004295	5.552755
5.075103	296.178180	5.557760
4.903291	303.228304	5.562765
5.212985	303.208542	5.567770
4.916958	304.384052	5.572774
4.968118	299.326822	5.577779
5.001197	300.011339	5.582784
5.348338	291.725357	5.587789
5.308439	298.036783	5.592794
5.340753	297.250303	5.597798
5.377614	281.587460	5.602803
4.761164	280.886173	5.607808
4.700391	291.240873	5.612813
5.321575	294.893111	5.617818
4.685006	305.081209	5.622822
5.050609	295.435128	5.627827
4.910879	303.236378	5.632832
5.027028	310.671931	5.637837
4.974546	300.799881	5.642842
4.893309	299.164231	5.647846
5.074995	292.501672	5.652851
5.035463	309.860646	5.657856
4.863721	305.201943	5.662861
5.604568	321.692795	5.667866
5.292986	322.699890	5.672870
5.651415	319.046948	5.677875
5.473956	310.181424	5.682880
5.239163	300.081501	5.687885
5.601385	300.626188	5.692890
5.288486	309.194706	5.697894
5.185559	302.519510	5.702899
5.526800	297.037473	5.707904
5.259879	305.342570	5.712909
5.113400	300.933031	5.717914
5.387106	317.186569	5.722918
5.632267	317.474242	5.727923
5.476249	312.003184	5.732928
5.110405	312.056964	5.737933
5.746746	321.176870	5.742938
5.498454	329.931487	5.747942
5.527585	322.014537	5.752947
5.256407	326.194852	5.757952
5.412133	324.319829	5.762957
5.581367	327.564722	5.767962
5.751906	323.485462	5.772966
5.737565	325.601025	5.777971
5.251886	327.514732	5.782976
5.538159	325.704803	5.787981
5.656462	327.119520	5.792986
5.664964	327.039087	5.797990
5.643701	328.428079	5.802995
5.711250	330.657440	5.808000
5.669370	325.076861	5.813005
5.753716	323.061093	5.818010
5.590984	331.232925	5.823014
5.927697	331.594927	5.828019
6.152173	322.907258	5.833024
5.562596	316.874127	5.838029
5.403897	293.841846	5.843034
5.486232	324.985036	5.848038
6.101190	320.956802	5.853043
5.923013	321.883016	5.858048
5.564171	316.500482	5.863053
5.728704	320.363026	5.868058
5.490435	322.782367	5.873062
6.068225	319.177528	5.878067
5.810949	316.547412	5.883072
5.568023	320.141208	5.888077
5.611868	317.075074	5.893082
5.736755	326.315742	5.898086
6.062568	328.125249	5.903091
5.459155	331.553715	5.908096
5.704456	337.134229	5.913101
5.633626	319.824014	5.918106
5.639204	311.236870	5.923110
5.505819	317.059831	5.928115
5.551077	318.666250	5.933120
5.922529	327.318047	5.938125
5.865529	327.339560	5.943130
5.930396	345.859208	5.948134
5.898949	332.266522	5.953139
6.076376	342.479764	5.958144
5.863371	343.003284	5.963149
6.257192	337.769307	5.968154
5.998787	335.898651	5.973158
6.272220	349.915529	5.978163
5.984092	350.716497	5.983168
6.271478	347.539674	5.988173
6.529790	345.095030	5.993178
6.363643	346.383196	5.998182
6.178812	329.764590	6.003187
5.906108	328.639629	6.008192
5.916040	332.339588	6.013197
6.360452	336.474929	6.018202
6.169509	333.151124	6.023206
5.957347	327.704621	6.028211
5.977462	333.962424	6.033216
5.959755	346.237141	6.038221
6.347857	345.157988	6.043226
6.120666	349.843979	6.048230
6.126071	342.889314	6.053235
6.565483	345.668210	6.058240
6.160255	343.073780	6.063245
5.978369	335.347863	6.068250
5.869675	345.776494	6.073254
6.146176	339.731895	6.078259
6.595908	339.655529	6.083264
6.047648	337.754073	6.088269
6.387036	337.694887	6.093274
6.335850	329.515197	6.098278
6.084648	330.376852	6.103283
6.403546	327.378621	6.108288
6.111639	326.737532	6.113293
6.286045	326.068131	6.118298
5.942485	334.252299	6.123302
5.987439	328.110879	6.128307
5.820024	331.936526	6.133312
5.913893	344.940502	6.138317
6.263871	336.340851	6.143322
5.908419	349.243949	6.148326
6.325420	342.854776	6.153331
6.335004	352.179847	6.158336
6.357945	344.431527	6.163341
6.459826	337.126491	6.168346
6.077734	340.106056	6.173350
5.942437	328.756784	6.178355
5.985093	330.211753	6.183360
5.759463	328.990879	6.188365
6.609509	342.190326	6.193370
6.176119	344.927946	6.198374
6.206281	336.020592	6.203379
6.110363	342.964003	6.208384
6.188546	336.779443	6.213389
6.338449	335.196385	6.218394
6.273671	336.633280	6.223398
6.297601	325.192782	6.228403
6.245356	333.271483	6.233408
6.004881	333.460765	6.238413
6.167303	326.336129	6.243418
6.357017	331.899986	6.248422
6.339780	322.879798	6.253427
6.289326	324.592867	6.258432
5.864707	333.143990	6.263437
5.900575	332.318991	6.268442
6.005922	339.079208	6.273446
6.157782	332.509861	6.278451
6.282231	329.987986	6.283456
6.143175	334.511557	6.288461
6.074935	335.803462	6.293466
5.998227	343.531643	6.298470
6.038812	339.915529	6.303475
6.126760	343.337594	6.308480
5.890638	339.106514	6.313485
6.112408	334.117621	6.318490
5.869044	336.015748	6.323494
6.229229	351.778136	6.328499
6.295460	351.071793	6.333504
6.153137	347.990348	6.338509
6.154833	327.669649	6.343514
6.048926	335.095495	6.348518
6.350595	333.346441	6.353523
6.169101	333.836582	6.358528
6.285960	334.068302	6.363533
6.271077	331.909799	6.368538
6.093315	333.933751	6.373542
6.023430	325.016669	6.378547
6.166496	327.680353	6.383552
6.204991	329.101169	6.388557
6.016193	331.987364	6.393562
5.920945	337.804394	6.398566
6.112476	332.019794	6.403571
6.088988	335.503499	6.408576
6.120040	338.741436	6.413581
6.469580	341.945604	6.418586
6.426516	337.016926	6.423590
6.288947	332.352896	6.428595
6.201903	338.902626	6.433600
6.234049	333.525649	6.438605
6.297650	326.938409	6.443610
6.319291	325.647400	6.448614
6.287576	333.371735	6.453619
6.041425	331.844014	6.458624
6.133979	329.482125	6.463629
6.446717	330.233831	6.468634
6.271861	335.443171	6.473638
6.132933	328.140831	6.478643
6.343345	332.584682	6.483648
6.027927	336.547265	6.488653
6.297918	324.669831	6.493658
5.977173	321.932539	6.498662
6.215484	324.995837	6.503667
6.176357	330.190371	6.508672
6.119638	330.721194	6.513677
6.131944	332.674425	6.518682
5.932889	338.934716	6.523686
6.577582	332.854939	6.528691
6.451042	321.558091	6.533696
6.263929	329.641971	6.538701
6.221663	327.190344	6.543706
6.342397	334.242387	6.548710
6.270786	322.778801	6.553715
6.033378	312.334435	6.558720
5.719801	318.400583	6.563725
6.248535	325.069565	6.568730
6.037219	328.642623	6.573734
6.053549	325.973069	6.578739
5.883776	322.089161	6.583744
5.499591	339.112690	6.588749
6.145193	325.857512	6.593754
6.180211	329.303633	6.598758
6.423476	316.032013	6.603763
6.587556	318.445656	6.608768
6.097721	334.024004	6.613773
6.236110	319.477922	6.618778
6.030800	332.462033	6.623782
6.226389	330.773788	6.628787
6.366216	326.848002	6.633792
6.163128	329.818677	6.638797
6.311179	322.512786	6.643802
6.125352	322.883381	6.648806
6.230854	329.333528	6.653811
5.920674	333.744539	6.658816
5.921406	339.777576	6.663821
6.259818	325.387005	6.668826
6.041433	333.456773	6.673830
6.285619	331.628086	6.678835
6.456513	323.198691	6.683840
6.396691	334.863038	6.688845
6.625095	323.033207	6.693850
5.907118	325.277306	6.698854
5.689601	314.472345	6.703859
5.851291	314.380716	6.708864
5.942006	339.049714	6.713869
6.091830	330.769126	6.718874
5.981953	342.707021	6.723878
6.243793	330.634703	6.728883
6.166809	338.059210	6.733888
6.109140	333.632671	6.738893
6.223090	332.184922	6.743898
5.626594	340.633097	6.748902
5.892986	334.023772	6.753907
5.825793	329.579735	6.758912
5.847185	330.069924	6.763917
6.064828	326.264897	6.768922
6.131252	333.315904	6.773926
5.674440	334.054551	6.778931
6.180415	336.965448	6.783936
6.189033	346.505798	6.788941
6.474804	344.417539	6.793946
6.016443	337.326279	6.798950
6.012798	336.902894	6.803955
6.302212	329.027672	6.808960
5.997735	331.245355	6.813965
6.271147	339.093026	6.818970
6.000373	336.034745	6.823974
6.322029	335.661951	6.828979
6.557205	335.141273	6.833984
6.302945	336.547560	6.838989
6.578770	328.642816	6.843994
6.382771	340.787105	6.848998
6.010511	328.601547	6.854003
6.211771	335.495522	6.859008
6.393991	334.195329	6.864013
6.120054	324.180579	6.869018
6.220133	333.763629	6.874022
6.396209	324.181841	6.879027
6.291321	325.713564	6.884032
6.174300	336.513638	6.889037
6.538074	317.462165	6.894042
6.519377	329.145415	6.899046
6.453849	316.228750	6.904051
6.346623	311.294251	6.909056
5.921820	302.002179	6.914061
5.769424	309.425760	6.919066
5.991056	309.210906	6.924070
5.907845	322.663208	6.929075
6.310983	320.863557	6.934080
5.944070	329.905556	6.939085
6.058611	320.849033	6.944090
6.299578	331.669296	6.949094
5.897227	331.890108	6.954099
6.180651	334.924238	6.959104
5.513556	327.103031	6.964109
6.418359	332.337256	6.969114
6.152016	331.771279	6.974118
6.193272	331.954660	6.979123
6.465888	332.611375	6.984128
5.962061	333.752803	6.989133
5.960540	326.938425	6.994138
5.821851	329.443502	6.999142
5.850221	332.903313	7.004147
6.155650	326.632756	7.009152
6.223473	330.241445	7.014157
5.992442	328.467766	7.019162
6.152030	332.796145	7.024166
5.832840	323.092157	7.029171
5.876260	324.945631	7.034176
5.925238	330.895224	7.039181
5.997671	328.283373	7.044186
5.995512	336.670647	7.049190
5.922080	333.777791	7.054195
6.223484	341.984929	7.059200
6.292608	354.347372	7.064205
6.074094	345.535677	7.069210
6.283331	344.832379	7.074214
6.102668	347.514833	7.079219
6.112387	338.787827	7.084224
6.184005	355.373416	7.089229
6.274108	352.344366	7.094234
6.038828	346.642034	7.099238
6.137213	344.829719	7.104243
6.151873	342.932365	7.109248
6.201881	347.464467	7.114253
6.191041	340.433240	7.119258
6.039400	340.561235	7.124262
6.313875	341.995930	7.129267
6.274992	333.206893	7.134272
6.004688	343.350642	7.139277
6.436168	333.071035	7.144282
6.078494	333.920795	7.149286
6.161394	336.511592	7.154291
6.232968	329.619395	7.159296
6.010264	344.184906	7.164301
6.175380	333.386796	7.169306
5.959878	329.048106	7.174310
6.223457	329.351894	7.179315
6.183606	333.853692	7.184320
6.087374	343.138287	7.189325
6.181701	327.162741	7.194330
5.928412	342.052546	7.199334
6.446585	343.278458	7.204339
6.145177	337.858502	7.209344
6.340909	335.885501	7.214349
6.474537	338.787934	7.219354
6.120663	337.821140	7.224358
6.166211	338.418298	7.229363
6.343378	336.938560	7.234368
6.355069	344.191079	7.239373
6.150610	335.120942	7.244378
6.080745	337.305261	7.249382
5.843619	334.868154	7.254387
6.335957	330.346491	7.259392
6.127511	333.963395	7.264397
6.415242	339.951747	7.269402
6.330816	336.124148	7.274406
6.250763	341.116253	7.279411
6.505578	338.381093	7.284416
6.068687	341.695051	7.289421
6.151468	336.170987	7.294426
6.306263	331.230487	7.299430
6.149796	336.297761	7.304435
6.170416	326.977453	7.309440
6.129632	338.056718	7.314445
6.413366	333.187890	7.319450
6.575748	334.712801	7.324454
5.957528	315.263740	7.329459
5.988390	316.309264	7.334464
6.107493	334.121280	7.339469
6.310833	324.215714	7.344474
6.407148	338.326598	7.349478
5.967099	326.319272	7.354483
5.898663	315.149420	7.359488
5.980561	342.240020	7.364493
6.284195	329.705623	7.369498
6.353937	333.975226	7.374502
5.922527	341.325206	7.379507
6.210963	335.620429	7.384512
6.018862	337.826944	7.389517
6.213186	340.811674	7.394522
6.195212	339.694507	7.399526
5.756310	337.605185	7.404531
6.084043	337.503522	7.409536
5.894401	339.504014	7.414541
6.119025	335.020868	7.419546
5.896326	335.865431	7.424550
6.139961	336.207124	7.429555
6.271075	330.425605	7.434560
5.918904	336.978650	7.439565
6.522627	327.358751	7.444570
6.377208	337.109736	7.449574
6.156797	348.802259	7.454579
6.236888	329.589301	7.459584
6.308428	342.046269	7.464589
6.238468	336.495368	7.469594
6.535840	336.271884	7.474598
6.321465	333.964110	7.479603
6.230140	312.439889	7.484608
5.702802	313.043986	7.489613
5.933423	327.415518	7.494618
6.251037	329.770458	7.499622
6.229851	338.717506	7.504627
5.811505	336.223194	7.509632
5.986642	334.304019	7.514637
6.421266	334.448301	7.519642
6.846095	331.259573	7.524646
6.117545	321.442154	7.529651
6.331551	310.342223	7.534656
6.026859	306.349613	7.539661
6.059925	312.842668	7.544666
5.911066	317.690458	7.549670
5.803429	324.721107	7.554675
6.306829	325.712041	7.559680
6.441394	343.021795	7.564685
6.108808	322.832241	7.569690
6.056820	310.900544	7.574694
5.794729	327.971491	7.579699
6.476621	335.119658	7.584704
6.125331	335.838711	7.589709
6.192116	328.026625	7.594714
6.100509	315.851162	7.599718
6.278539	319.929900	7.604723
5.955086	317.253140	7.609728
5.895053	325.696875	7.614733
6.169947	322.436583	7.619738
6.179038	329.961578	7.624742
6.253374	335.970498	7.629747
6.275319	330.000336	7.634752
6.160681	340.319160	7.639757
6.157166	324.852386	7.644762
6.084492	316.799432	7.649766
5.748472	332.616416	7.654771
6.277043	329.756379	7.659776
6.205203	343.602388	7.664781
6.245335	329.109561	7.669786
6.095165	333.793047	7.674790
6.205182	335.712083	7.679795
6.427964	332.985075	7.684800
5.984571	333.664686	7.689805
6.153072	322.951476	7.694810
6.274305	327.504121	7.699814
5.946166	324.344045	7.704819
6.153697	325.978982	7.709824
5.992917	333.887925	7.714829
6.354528	338.229143	7.719834
6.108583	339.074162	7.724838
6.257791	328.598065	7.729843
6.218439	333.599649	7.734848
6.023618	332.462562	7.739853
6.345337	330.678750	7.744858
5.765441	318.993753	7.749862
5.772007	319.998768	7.754867
5.870625	330.575443	7.759872
5.789385	336.228943	7.764877
6.239016	329.711310	7.769882
6.277231	334.049097	7.774886
5.988020	334.230148	7.779891
6.052593	334.482664	7.784896
5.708281	347.172058	7.789901
6.321545	336.465520	7.794906
6.577562	332.398259	7.799910
6.397802	337.772875	7.804915
6.340770	339.572389	7.809920
6.088902	336.194796	7.814925
6.252697	336.393899	7.819930
6.361348	335.475313	7.824934
6.346285	338.818504	7.829939
6.533251	331.667899	7.834944
6.181398	328.799411	7.839949
5.860912	316.333723	7.844954
6.045249	322.151509	7.849958
6.221920	334.519338	7.854963
6.310774	326.915784	7.859968
5.993428	328.736846	7.864973
6.345453	329.539381	7.869978
5.936619	320.874387	7.874982
5.982366	331.358056	7.879987
6.641669	329.695687	7.884992
6.146331	322.002761	7.889997
6.162563	307.317524	7.895002
6.051987	311.441194	7.900006
5.763416	314.412521	7.905011
6.315885	324.817291	7.910016
6.118978	334.278905	7.915021
6.426292	320.810651	7.920026
5.896032	315.904050	7.925030
5.620902	325.846065	7.930035
6.123702	332.319775	7.935040
6.215934	330.603330	7.940045
5.973146	332.419111	7.945050
6.421473	334.722062	7.950054
6.297663	333.605556	7.955059
6.228330	335.153890	7.960064
6.444865	339.565152	7.965069
6.223819	333.889080	7.970074
6.117948	311.677440	7.975078
6.173932	306.186030	7.980083
6.100886	311.518714	7.985088
5.778171	316.792197	7.990093
5.909338	322.899831	7.995098
6.085975	337.263958	8.000102
5.856744	331.247483	8.005107
6.248946	337.393572	8.010112
6.011022	338.570804	8.015130
6.620671	328.999527	8.020147
6.454786	329.110540	8.025165
6.326115	328.732948	8.030182
5.960227	317.915623	8.035200
5.919364	333.819997	8.040218
6.436595	340.265282	8.045235
6.020296	339.020497	8.050253
5.768583	341.969157	8.055270
6.153454	333.619390	8.060288
6.321270	339.043009	8.065306
6.259309	341.368869	8.070323
6.206787	336.356429	8.075341
5.815210	337.383001	8.080358
6.293180	329.820269	8.085376
6.087564	341.010555	8.090394
6.269791	332.998435	8.095411
6.383093	341.882795	8.100429
6.284810	342.273600	8.105446
6.345204	333.459986	8.110464
6.067824	344.787672	8.115482
6.354309	344.092992	8.120499
6.605601	339.844245	8.125517
6.127183	347.867738	8.130534
6.137017	335.890591	8.135552
6.401563	342.955853	8.140570
6.223293	333.860680	8.145587
5.748534	334.568862	8.150605
5.732093	338.812564	8.155622
6.146340	332.187507	8.160640
5.913839	338.168887	8.165658
5.954664	344.344384	8.170675
6.605465	345.855565	8.175693
6.202243	341.320581	8.180710
6.175696	349.321055	8.185728
6.487546	352.816254	8.190746
6.418995	349.302074	8.195763
6.618557	343.161693	8.200781
6.413652	347.160202	8.205798
6.270554	334.607296	8.210816
6.314892	334.824425	8.215834
6.513599	337.232769	8.220851
6.559640	345.584836	8.225869
6.079607	343.589467	8.230886
6.525430	334.289834	8.235904
6.226428	332.875316	8.240922
5.985451	331.874618	8.245939
6.257694	344.489427	8.250957
6.330296	355.920411	8.255974
6.722607	347.225515	8.260992
6.568198	350.455657	8.266010
6.093688	341.902036	8.271027
6.473708	342.615980	8.276045
6.672283	347.637203	8.281062
6.629524	342.973517	8.286080
6.206164	348.583851	8.291098
6.253277	332.138845	8.296115
6.697712	334.164967	8.301133
6.147769	335.437088	8.306150
6.787637	348.344936	8.311168
6.543405	331.415147	8.316186
6.426367	335.122277	8.321203
6.682259	325.735462	8.326221
6.199496	332.831871	8.331238
6.360640	322.749793	8.336256
6.549408	329.864717	8.341274
6.463646	336.198768	8.346291
6.404168	336.122810	8.351309
6.622932	347.780326	8.356326
6.464271	337.716476	8.361344
6.380560	338.881296	8.366362
6.457911	346.584741	8.371379
6.715047	345.392885	8.376397
6.570542	351.893870	8.381414
6.785999	337.256068	8.386432
6.469996	342.489945	8.391450
6.232964	337.231693	8.396467
6.931299	339.625359	8.401485
6.638100	339.210271	8.406502
6.640760	337.092415	8.411520
6.264620	337.801021	8.416538
6.332280	342.662755	8.421555
6.657988	338.528647	8.426573
6.262792	351.064352	8.431590
6.492568	347.964446	8.436608
6.835879	344.524989	8.441626
6.590852	353.332610	8.446643
6.796677	346.632707	8.451661
6.463302	355.409905	8.456678
6.800864	348.938784	8.461696
6.617454	350.762875	8.466714
6.502477	358.041860	8.471731
6.785988	350.900694	8.476749
6.764061	349.020182	8.481766
6.682232	347.701231	8.486784
6.816632	344.736089	8.491802
6.082672	340.075884	8.496819
6.286990	346.434199	8.501837
6.560233	352.560890	8.506854
6.480070	354.536155	8.511872
6.851446	353.948171	8.516890
6.685143	355.106917	8.521907
6.709151	352.392478	8.526925
6.598384	360.226199	8.531942
6.349387	355.392659	8.536960
6.503992	350.480503	8.541978
6.514836	361.485630	8.546995
6.744965	350.414550	8.552013
6.615933	357.809326	8.557030
6.454317	356.007363	8.562048
6.624946	352.597947	8.567066
6.601680	358.953832	8.572083
6.882879	360.708742	8.577101
6.607333	359.180123	8.582119
6.646390	355.002285	8.587136
6.865381	351.888279	8.592154
6.643127	353.828865	8.597171
6.780528	342.724894	8.602189
7.172797	357.195466	8.607207
6.857019	353.640887	8.612224
6.958118	353.170719	8.617242
6.504150	356.526392	8.622259
6.781728	350.140345	8.627277
6.781523	360.377218	8.632295
6.807499	347.100586	8.637312
6.860236	356.164787	8.642330
6.706705	358.492283	8.647347
7.004764	357.088939	8.652365
6.781909	354.460270	8.657383
6.886742	352.717802	8.662400
7.074293	357.778613	8.667418
6.772592	360.476298	8.672435
6.788900	352.433201	8.677453
6.760764	358.483748	8.682471
6.839079	351.652226	8.687488
6.943875	348.701159	8.692506
6.895659	362.429321	8.697523
6.888199	352.771086	8.702541
6.826740	350.032087	8.707559
6.624958	354.623369	8.712576
7.082642	354.085059	8.717594
6.548705	350.696984	8.722611
6.878600	358.705078	8.727629
6.821959	371.333244	8.732647
6.721547	375.766745	8.737664
7.265758	372.065643	8.742682
7.044255	374.425813	8.747699
6.895564	357.885044	8.752717
6.952183	358.756632	8.757735
6.704841	353.815544	8.762752
7.091196	360.880783	8.767770
7.023893	367.906210	8.772787
7.116309	373.262688	8.777805
7.120028	373.514542	8.782823
6.907097	366.851429	8.787840
7.183130	355.861557	8.792858
6.718655	359.502873	8.797875
6.854876	348.408549	8.802893
7.109230	365.390390	8.807911
7.110867	376.217088	8.812928
7.125861	354.560804	8.817946
6.725080	362.452302	8.822963
7.005439	369.736007	8.827981
6.979286	377.162108	8.832999
6.932514	386.292307	8.838016
7.354607	375.519510	8.843034
6.968189	375.412409	8.848051
7.147994	376.091259	8.853069
7.045382	370.180942	8.858087
6.950650	373.726826	8.863104
7.171488	372.048342	8.868122
7.271911	380.407737	8.873139
7.062187	367.117297	8.878157
6.889410	365.411740	8.883175
6.895843	372.630804	8.888192
7.289935	377.684708	8.893210
7.179149	385.770893	8.898227
7.344888	377.398422	8.903245
7.190478	369.517590	8.908263
6.913304	364.404428	8.913280
7.039874	372.611433	8.918298
7.057914	380.336750	8.923315
7.043012	382.784669	8.928333
7.304994	395.836589	8.933351
7.198794	382.356460	8.938368
7.364112	375.896369	8.943386
7.264300	373.358986	8.948403
6.797490	369.490267	8.953421
7.059954	372.816444	8.958439
7.127755	384.661581	8.963456
7.051589	380.779372	8.968474
7.212546	385.389920	8.973491
7.591417	379.003870	8.978509
7.311055	393.727512	8.983527
7.271339	387.252006	8.988544
7.271304	384.326722	8.993562
7.431760	392.717799	8.998579
7.214925	381.040986	9.003597
7.131973	380.473248	9.008615
7.151100	388.160531	9.013632
7.262276	385.912172	9.018650
7.161803	390.468755	9.023667
7.207537	391.954233	9.028685
7.125995	389.420315	9.033703
7.127619	386.810336	9.038720
7.161005	384.359505	9.043738
7.230883	384.143492	9.048755
7.148315	391.354332	9.053773
7.429853	383.033253	9.058791
7.269088	386.365370	9.063808
7.289381	382.105245	9.068826
7.496512	398.438098	9.073843
7.548228	383.686905	9.078861
7.641208	374.451653	9.083879
7.346144	382.894714	9.088896
7.392122	383.465020	9.093914
7.638614	385.828062	9.098931
7.447985	380.931782	9.103949
7.134067	383.274786	9.108967
7.261519	386.940705	9.113984
7.217938	387.338772	9.119002
7.281743	391.150295	9.124019
7.017734	388.556428	9.129037
7.366553	382.436974	9.134055
7.240762	380.358046	9.139072
7.118117	382.030676	9.144090
6.988181	392.944138	9.149107
6.975091	388.348400	9.154125
7.145852	390.234111	9.159143
7.213191	405.566310	9.164160
7.431002	398.403798	9.169178
7.328542	409.925186	9.174195
7.291487	408.810687	9.179213
7.556495	408.119348	9.184231
7.412422	420.593913	9.189248
7.807423	407.591122	9.194266
7.935553	420.158998	9.199283
7.284693	409.348119	9.204301
7.355950	405.947853	9.209319
7.530682	422.970547	9.214336
7.426063	406.542785	9.219354
7.480723	407.487261	9.224371
7.525268	414.984416	9.229389
7.998125	414.664637	9.234407
7.442016	405.823904	9.239424
7.860720	405.891234	9.244442
7.370770	394.020262	9.249459
7.504905	393.295654	9.254477
7.593310	394.064470	9.259495
6.951317	399.500589	9.264512
8.189074	401.800811	9.269530
8.002381	392.451312	9.274547
7.499143	393.905504	9.279565
7.270305	390.208001	9.284583
7.368738	388.229854	9.289600
7.435470	399.008563	9.294618
7.789815	401.285391	9.299635
7.792809	404.696151	9.304653
7.694185	397.005426	9.309671
7.736579	392.779724	9.314688
7.574659	394.146062	9.319706
7.774942	389.772709	9.324723
7.452152	393.616022	9.329741
7.661410	391.166208	9.334759
8.057120	403.244311	9.339776
7.600266	387.152261	9.344794
7.571388	379.087786	9.349811
7.310463	386.566222	9.354829
7.889797	393.184883	9.359847
7.608826	409.341292	9.364864
7.783636	413.173403	9.369882
7.695850	412.227740	9.374899
7.709986	418.786096	9.379917
7.782963	408.954369	9.384935
7.711948	412.076868	9.389952
7.700305	410.784852	9.394970
7.841187	410.456804	9.399987
7.756375	423.010502	9.405005
7.521539	411.434296	9.410023
7.766434	413.144373	9.415040
7.718055	409.888959	9.420058
7.478878	420.671131	9.425075
7.566471	421.995468	9.430093
8.054089	422.926180	9.435111
7.760630	414.480028	9.440128
7.848430	413.680586	9.445146
7.827340	412.904411	9.450163
7.502031	414.094229	9.455181
7.589039	410.391724	9.460199
7.746832	411.074002	9.465216
7.536823	413.097890	9.470234
7.813384	409.602546	9.475251
7.580500	410.361429	9.480269
7.423029	412.020551	9.485287
7.637789	409.677169	9.490304
7.654651	411.851917	9.495322
7.726804	418.413862	9.500339
7.640591	433.340826	9.505357
8.119928	437.371669	9.510375
8.146630	442.517505	9.515392
7.995281	435.563926	9.520410
8.004850	431.381193	9.525427
7.733592	430.675523	9.530445
7.900846	423.763857	9.535463
7.905697	433.719133	9.540480
7.408004	436.904912	9.545498
8.071821	432.481468	9.550515
7.924680	438.910314	9.555533
7.908655	432.491060	9.560551
8.173862	431.616662	9.565568
8.075208	430.183566	9.570586
8.147238	436.562509	9.575603
8.117307	432.953942	9.580621
8.214009	418.839466	9.585639
8.010300	428.562137	9.590656
7.773874	422.944023	9.595674
8.000797	425.123935	9.600691
7.918808	436.519082	9.605709
7.992488	432.547263	9.610727
7.976222	424.474493	9.615744
8.065933	433.529821	9.620762
8.538556	419.789138	9.625779
8.254530	429.019413	9.630797
8.080180	416.139973	9.635815
7.849685	402.076454	9.640832
7.761351	406.927782	9.645850
8.062092	414.268289	9.650867
8.264690	436.250478	9.655885
8.477609	437.378587	9.660903
8.356395	422.938293	9.665920
8.155680	408.081222	9.670938
8.120007	403.561576	9.675955
8.138872	402.798113	9.680973
8.043882	405.148057	9.685991
8.119678	406.774015	9.691008
8.106898	406.902213	9.696026
8.191378	404.623296	9.701043
7.883617	418.369821	9.706061
8.122741	411.749911	9.711079
8.062543	417.600354	9.716096
8.170231	424.040010	9.721114
8.246654	418.856001	9.726131
8.019005	434.145795	9.731149
8.230095	430.597528	9.736167
8.365657	430.011544	9.741184
8.260537	443.218480	9.746202
8.182004	420.989727	9.751219
8.123583	430.339503	9.756237
8.273811	431.407948	9.761255
8.579147	433.405248	9.766272
7.979844	437.862793	9.771290
8.093261	427.074912	9.776307
8.244896	435.372713	9.781325
8.115861	424.821388	9.786343
8.076647	429.308486	9.791360
7.659806	438.114499	9.796378
8.466879	430.330080	9.801395
8.238083	431.246110	9.806413
8.151966	435.724735	9.811431
8.491401	427.650228	9.816448
8.212079	437.514058	9.821466
8.398963	431.517624	9.826483
8.330537	435.658997	9.831501
8.139388	432.870752	9.836519
8.341623	433.997369	9.841536
8.371992	439.502376	9.846554
8.447352	427.041618	9.851571
8.344641	431.156771	9.856589
8.286261	431.875863	9.861607
8.534352	428.479617	9.866624
8.220242	440.390565	9.871642
8.597903	427.879583	9.876659
8.660732	430.223893	9.881677
8.339456	431.678158	9.886695
8.241935	431.611278	9.891712
8.247238	434.251708	9.896730
8.481232	423.789020	9.901747
8.250852	432.360882	9.906765
8.455419	431.385477	9.911783
8.537237	426.096490	9.916800
8.065217	433.923375	9.921818
8.350013	425.712217	9.926835
8.468853	431.645237	9.931853
8.636226	431.335153	9.936871
8.865288	431.163779	9.941888
8.257767	430.687180	9.946906
8.427887	430.651209	9.951923
8.312983	434.149755	9.956941
8.595422	433.430456	9.961959
8.818647	429.760385	9.966976
8.318425	436.932134	9.971994
8.450887	429.511513	9.977011
8.700465	433.612840	9.982029
8.410680	428.072455	9.987047
8.638962	429.034078	9.992064
8.390157	428.937107	9.997082
8.475938	427.689879	10.002099
8.600338	441.309179	10.007117
8.614691	446.576853	10.012135
8.854358	445.924170	10.017152
8.190240	447.520174	10.022170
8.421496	442.958957	10.027187
8.891271	454.792046	10.032205
8.486192	449.260139	10.037223
8.869577	447.739367	10.042240
8.681767	456.222566	10.047258
9.106881	441.340608	10.052275
8.411808	436.245156	10.057293
8.463906	447.871885	10.062311
8.797837	446.743802	10.067328
8.972845	447.619051	10.072346
8.763266	436.171434	10.077363
8.775274	440.360241	10.082381
8.436206	437.863256	10.087399
8.906277	441.198146	10.092416
8.695823	439.406934	10.097434
8.751011	434.166269	10.102451
8.830915	429.287812	10.107469
8.383130	420.909863	10.112487
8.895976	438.062956	10.117504
8.660326	447.131081	10.122522
8.804102	451.274130	10.127539
8.765560	449.500330	10.132557
9.079203	454.544692	10.137575
9.047038	439.162761	10.142592
8.997110	438.362673	10.147610
8.813801	432.073600	10.152627
8.727493	431.377002	10.157645
8.522750	425.217495	10.162663
8.670234	439.467483	10.167680
9.048570	445.483175	10.172698
8.977301	440.139127	10.177715
8.661002	431.210554	10.182733
8.528559	439.227556	10.187751
8.816995	439.551841	10.192768
8.702817	452.283692	10.197786
8.591107	454.737226	10.202803
9.288075	454.325752	10.207821
8.811532	447.047278	10.212839
8.804526	445.669335	10.217856
8.818452	464.613648	10.222874
8.841663	449.816348	10.227891
8.701118	451.599063	10.232909
8.757582	450.861301	10.237927
9.348032	444.660026	10.242944
8.903758	448.490708	10.247962
8.828359	454.611760	10.252979
8.756465	447.740475	10.257997
8.839663	445.887763	10.263015
9.164015	438.705492	10.268032
8.969799	448.246824	10.273050
8.993607	448.495552	10.278067
9.248478	449.490904	10.283085
8.775932	449.176316	10.288103
9.013002	445.384172	10.293120
8.793979	454.960926	10.298138
8.952022	456.428924	10.303155
8.879648	443.464163	10.308173
8.429736	450.880536	10.313191
9.064460	460.627310	10.318208
8.839377	470.785656	10.323226
9.316765	472.522654	10.328243
9.949407	479.174072	10.333261
9.497101	467.653778	10.338279
9.582228	451.900141	10.343296
9.637989	459.619620	10.348314
9.202646	458.409347	10.353331
9.368885	452.674884	10.358349
9.073284	456.842164	10.363367
9.533397	449.323186	10.368384
9.539447	453.033266	10.373402
9.351940	441.247710	10.378419
9.367640	433.778998	10.383437
8.817470	435.278369	10.388455
8.982920	429.837510	10.393472
9.372549	444.895514	10.398490
8.995831	445.253937	10.403507
9.184419	437.559500	10.408525
9.027920	450.948001	10.413543
9.204142	442.128922	10.418560
8.880584	450.923573	10.423578
9.033689	445.598235	10.428595
9.230152	449.509030	10.433613
8.895240	445.323126	10.438631
9.350320	456.416928	10.443648
9.313555	452.796798	10.448666
9.114119	450.552612	10.453683
9.148997	449.177615	10.458701
8.850241	462.007635	10.463719
9.116716	445.777667	10.468736
8.874595	450.050223	10.473754
9.315534	462.926014	10.478771
9.566802	472.836634	10.483789
9.060203	476.945257	10.488807
9.411210	468.168376	10.493824
9.728407	474.654322	10.498842
9.304615	465.729845	10.503859
9.341445	453.824149	10.508877
9.248233	460.951472	10.513895
9.623249	464.421080	10.518912
9.004791	465.511384	10.523930
9.169881	475.750988	10.528947
9.760879	468.243181	10.533965
9.569553	478.626637	10.538983
9.461049	467.614520	10.544000
9.889148	476.898038	10.549018
9.458574	469.353634	10.554035
9.324053	459.942331	10.559053
9.090140	462.970287	10.564071
9.707724	467.468738	10.569088
9.852302	475.351111	10.574106
9.091431	460.164665	10.579123
9.597506	454.749656	10.584141
9.537108	468.265213	10.589159
9.613619	463.119044	10.594176
9.643068	462.344464	10.599194
9.659936	459.593253	10.604211
9.535764	451.493092	10.609229
9.256328	453.890694	10.614247
9.723753	465.724156	10.619264
9.347375	464.760309	10.624282
9.384780	467.733400	10.629299
9.531681	476.312810	10.634317
9.616847	487.836593	10.639335
9.648821	485.430147	10.644352
9.714670	485.369387	10.649370
9.394150	479.111128	10.654387
9.619016	474.724459	10.659405
9.761707	481.038771	10.664423
9.780269	475.753306	10.669440
9.901964	479.398051	10.674458
9.889575	483.442352	10.679475
10.020222	471.534661	10.684493
9.477667	462.499294	10.689511
9.611713	465.801304	10.694528
9.572839	458.066537	10.699546
9.100780	461.693276	10.704563
9.688351	468.730385	10.709581
9.575855	480.875044	10.714599
9.530010	483.876878	10.719616
9.812106	480.642577	10.724634
9.408217	484.908771	10.729651
9.722837	482.660280	10.734669
9.644633	485.200116	10.739687
9.870802	475.218275	10.744704
9.761874	476.592147	10.749722
9.671853	482.466189	10.754739
9.781884	481.230959	10.759757
9.564464	477.982918	10.764775
9.876099	469.524575	10.769792
9.570108	473.740812	10.774810
9.297329	475.004502	10.779827
9.920016	483.828559	10.784845
9.775887	485.084842	10.789863
9.928088	493.963222	10.794880
9.973901	488.455770	10.799898
9.535420	491.597628	10.804915
10.008533	486.929320	10.809933
9.639993	496.999569	10.814951
9.970564	491.056480	10.819968
10.062211	497.312476	10.824986
10.118589	502.087652	10.830003
10.239245	493.065771	10.835021
9.808407	483.056837	10.840039
9.758578	481.631913	10.845056
10.273895	492.568043	10.850074
9.601439	496.295414	10.855091
10.198869	494.305833	10.860109
10.114752	496.063989	10.865127
9.706926	489.822475	10.870144
10.577032	484.852528	10.875162
10.066472	476.361256	10.880179
10.228833	470.049907	10.885197
9.826907	476.584705	10.890215
9.786937	474.246264	10.895232
10.039571	462.407944	10.900250
9.997055	468.154670	10.905267
10.055138	480.847098	10.910285
9.947449	484.660096	10.915303
10.319384	484.889335	10.920320
9.913023	481.487682	10.925338
10.188988	489.662015	10.930355
10.499418	483.188759	10.935373
9.997058	473.042651	10.940391
9.982491	474.392364	10.945408
10.384501	477.728391	10.950426
9.910792	475.246052	10.955443
10.243829	482.537381	10.960461
10.226063	481.738595	10.965479
10.186117	484.695331	10.970496
10.220619	469.968836	10.975514
10.133714	487.133308	10.980531
10.267894	490.810824	10.985549
10.092210	479.739735	10.990567
10.080472	486.330544	10.995584
10.365449	485.456221	11.000602
10.337926	495.621690	11.005619
10.404993	486.071694	11.010637
10.340970	478.842582	11.015655
10.112721	472.677251	11.020672
10.195279	480.654486	11.025690
10.473761	490.207446	11.030707
10.870006	484.560232	11.035725
10.294968	471.888297	11.040743
10.057545	471.249938	11.045760
9.887637	468.287976	11.050778
10.247810	485.202966	11.055795
10.432594	485.975714	11.060813
10.540639	484.008682	11.065831
10.465545	481.612596	11.070848
10.261141	470.710078	11.075866
10.399130	481.086442	11.080883
10.815101	477.231724	11.085901
10.253079	470.796485	11.090919
10.191044	469.849965	11.095936
10.446457	473.824167	11.100954
10.246932	473.252486	11.105971
10.546966	478.166436	11.110989
10.627541	472.801893	11.116007
10.031936	475.835674	11.121024
10.664910	469.861287	11.126042
10.372888	496.783416	11.131059
10.499189	489.720318	11.136077
10.430638	490.693448	11.141095
10.591775	501.788865	11.146112
10.751802	491.811002	11.151130
10.767530	476.165974	11.156147
10.473956	474.993585	11.161165
10.320555	480.473570	11.166183
9.872004	478.110385	11.171200
10.553943	480.841122	11.176218
10.266036	488.850795	11.181235
10.300549	492.051547	11.186253
10.582219	497.151390	11.191271
10.411876	494.845867	11.196288
10.650769	490.188780	11.201306
10.463777	500.666244	11.206323
10.582198	497.823480	11.211341
10.816639	493.523674	11.216359
10.415075	498.903454	11.221376
10.647830	486.007914	11.226394
10.636401	495.186314	11.231411
10.498537	489.682214	11.236429
10.544780	493.572228	11.241447
10.440637	496.273887	11.246464
10.684520	495.743616	11.251482
10.737440	492.690155	11.256499
10.706629	493.830970	11.261517
10.914567	492.103993	11.266535
10.695435	487.578177	11.271552
11.035989	490.308422	11.276570
10.999084	493.381445	11.281587
11.155612	489.974198	11.286605
11.263731	494.274280	11.291623
10.998462	496.325716	11.296640
11.264517	495.473272	11.301658
10.965259	495.623985	11.306675
11.094459	482.763504	11.311693
10.848799	479.362077	11.316711
10.687913	470.535512	11.321728
10.889474	472.801426	11.326746
10.845891	474.269260	11.331763
10.676016	488.549766	11.336781
10.750590	498.819255	11.341799
10.896373	500.020934	11.346816
11.026380	482.767658	11.351834
10.819238	491.231793	11.356851
10.942745	494.030544	11.361869
10.824993	487.835382	11.366887
10.504444	488.898237	11.371904
10.896233	482.759436	11.376922
10.798683	492.150048	11.381939
10.695213	483.036841	11.386957
10.605374	488.544801	11.391975
11.000163	485.810480	11.396992
10.885367	480.542621	11.402010
10.545705	492.902529	11.407027
10.530717	492.958492	11.412045
11.010425	505.235015	11.417063
11.270851	520.130171	11.422080
11.100977	510.686478	11.427098
10.980219	510.077287	11.432115
11.262874	509.790276	11.437133
10.893955	505.653833	11.442151
10.871019	495.534049	11.447168
11.049702	506.585713	11.452186
11.372631	510.161266	11.457203
11.208740	514.396411	11.462221
11.039294	506.022421	11.467239
10.410632	506.782972	11.472256
11.090185	507.664871	11.477274
10.976869	507.770856	11.482291
10.984672	514.387034	11.487309
11.008247	510.400909	11.492327
11.253755	519.870661	11.497344
11.340376	520.791232	11.502362
11.025435	518.328347	11.507379
11.002103	516.479592	11.512397
11.379311	513.221009	11.517415
11.352895	519.675268	11.522432
11.414391	507.592135	11.527450
11.240436	515.928045	11.532467
11.077809	509.301225	11.537485
11.406178	512.468851	11.542503
11.200657	511.491023	11.547520
11.237798	513.924546	11.552538
11.493452	514.642082	11.557555
11.360121	520.371408	11.562573
11.348306	516.431815	11.567591
11.420645	517.282030	11.572608
11.587164	515.050282	11.577626
11.068691	522.379534	11.582643
11.128675	524.219394	11.587661
11.654276	510.748090	11.592679
11.472039	522.610160	11.597696
11.819762	513.571848	11.602714
11.542756	513.024853	11.607731
11.406833	516.031249	11.612749
11.540786	507.556374	11.617767
11.307042	518.789019	11.622784
11.529166	516.043709	11.627802
11.576254	515.679771	11.632819
11.486856	523.298807	11.637837
11.673526	511.966163	11.642855
11.247243	505.875833	11.647872
11.492095	515.803255	11.652890
11.445092	517.060196	11.657907
11.476474	522.249505	11.662925
11.597718	510.128668	11.667943
11.289292	518.356133	11.672960
11.561089	515.423216	11.677978
11.807271	519.058055	11.682995
11.679445	517.623182	11.688013
11.666322	515.230065	11.693031
11.505058	521.048942	11.698048
11.348437	515.232190	11.703066
11.805759	512.450261	11.708083
11.564768	503.983274	11.713101
11.809093	512.187788	11.718119
11.493536	522.281359	11.723136
11.195458	513.444576	11.728154
11.314765	517.380022	11.733171
11.330660	520.204999	11.738189
11.683667	519.831299	11.743207
11.472125	527.690251	11.748224
11.556673	521.858036	11.753242
11.581635	516.382223	11.758259
11.750129	524.305073	11.763277
11.880410	526.165545	11.768295
11.787273	517.754423	11.773312
11.599877	516.215221	11.778330
11.665674	519.250169	11.783347
11.545405	533.261067	11.788365
11.816107	539.785833	11.793383
11.894692	539.041467	11.798400
12.045999	537.316991	11.803418
11.834611	525.206909	11.808435
11.646150	524.942759	11.813453
11.835404	529.599429	11.818471
12.107017	537.935400	11.823488
11.760853	524.401010	11.828506
11.750184	521.587807	11.833523
11.650918	550.010499	11.838541
11.995418	547.205107	11.843559
12.020595	538.945960	11.848576
11.951441	539.199696	11.853594
12.041252	545.282434	11.858611
12.143269	541.056881	11.863629
12.178077	524.222311	11.868647
11.927665	528.612936	11.873664
11.559810	517.858908	11.878682
12.083580	532.627870	11.883699
11.729292	546.028304	11.888717
11.924621	542.596072	11.893735
12.067532	550.396691	11.898752
12.042507	549.797839	11.903770
12.387476	543.704175	11.908787
11.848045	546.571439	11.913805
12.000490	541.501784	11.918823
12.269527	533.621218	11.923840
11.871555	538.435588	11.928858
12.180807	531.116781	11.933875
12.034350	532.966694	11.938893
11.926711	530.477842	11.943911
11.843274	536.003754	11.948928
11.911004	537.738272	11.953946
12.388781	528.241067	11.958963
11.836167	546.361690	11.963981
12.312160	535.091277	11.968999
11.987076	528.120532	11.974016
12.326689	533.167185	11.979034
11.984303	537.935032	11.984051
12.081954	528.765242	11.989069
12.166180	533.621294	11.994087
12.401441	536.876002	11.999104
12.249532	535.309184	12.004122
12.271154	540.787183	12.009139
12.100542	527.689340	12.014157
12.055568	536.854049	12.019175
12.141769	536.051696	12.024192
11.861515	537.297620	12.029210
12.248772	548.992148	12.034227
12.474043	561.753274	12.039245
12.539235	555.100434	12.044263
12.131211	553.519844	12.049280
12.424748	560.536501	12.054298
12.614518	553.476118	12.059315
12.443780	554.947978	12.064333
12.323301	546.512699	12.069351
12.563921	533.278244	12.074368
12.300908	535.089502	12.079386
12.343789	534.590526	12.084403
12.350444	553.974703	12.089421
12.503375	562.464858	12.094439
12.648209	565.995570	12.099456
12.486448	558.488166	12.104474
12.403155	547.270112	12.109491
12.047335	557.108051	12.114509
12.278743	547.980539	12.119527
12.470717	557.455490	12.124544
12.371724	568.875460	12.129562
12.636663	554.018347	12.134579
12.612035	568.651826	12.139597
12.451588	567.064245	12.144615
12.682687	568.599769	12.149632
12.725873	572.619658	12.154650
12.818251	560.746267	12.159667
12.426349	569.232894	12.164685
12.706903	565.673784	12.169703
12.952935	558.926518	12.174720
13.084582	555.706160	12.179738
12.799421	542.402089	12.184755
12.348442	549.796579	12.189773
12.350890	551.307744	12.194791
12.715706	553.819637	12.199808
12.674059	564.451226	12.204826
12.822814	555.863575	12.209843
12.792283	564.779908	12.214861
12.536695	560.073565	12.219879
13.004417	564.705823	12.224896
12.832574	563.473451	12.229914
12.831324	568.746746	12.234931
12.875442	573.041033	12.239949
12.904955	565.942484	12.244967
12.581217	563.544075	12.249984
12.642619	566.608116	12.255002
12.326159	564.401070	12.260019
12.589530	563.792028	12.265037
12.555847	552.727185	12.270055
12.781875	557.349736	12.275072
12.568207	561.766204	12.280090
12.940544	551.584846	12.285107
12.741214	561.089167	12.290125
12.459769	555.954525	12.295143
12.783100	567.280339	12.300160
13.083408	574.860811	12.305178
13.078931	576.972633	12.310195
13.088065	583.064789	12.315213
12.856685	572.040181	12.320231
12.982649	567.577374	12.325248
13.225003	575.024865	12.330266
12.940545	564.374584	12.335283
12.839989	562.465268	12.340301
13.096660	582.738315	12.345319
13.271436	585.794175	12.350336
12.757150	578.114442	12.355354
13.256675	577.484409	12.360371
12.939856	578.770741	12.365389
13.059863	587.291279	12.370407
13.110217	576.121823	12.375424
13.212849	586.267079	12.380442
13.170046	584.680113	12.385459
13.433771	588.066092	12.390477
13.140624	577.268840	12.395495
13.201525	565.734847	12.400512
13.013869	563.002840	12.405530
13.340358	564.596092	12.410547
12.914664	572.280132	12.415565
13.026432	580.394868	12.420583
13.440001	568.960591	12.425600
13.304290	582.437469	12.430618
13.667618	580.875630	12.435635
13.423688	577.641164	12.440653
12.921581	570.821035	12.445671
13.448189	570.306702	12.450688
13.133296	573.937394	12.455706
13.073194	577.455837	12.460723
13.733962	580.666392	12.465741
13.263764	579.480472	12.470759
13.571676	572.922372	12.475776
13.387633	566.169483	12.480794
13.060271	558.195580	12.485811
13.411169	563.114257	12.490829
13.578968	566.019728	12.495847
13.225119	558.021547	12.500864
13.121027	572.159339	12.505882
13.836166	572.410880	12.510899
13.559289	583.353648	12.515917
13.614081	572.925085	12.520935
13.423805	557.482466	12.525952
13.312071	560.832227	12.530970
13.372825	572.672276	12.535987
13.440901	574.782268	12.541005
13.430597	582.565732	12.546023
13.542120	577.922142	12.551040
13.550775	586.040313	12.556058
13.668821	573.907307	12.561075
13.834683	584.746431	12.566093
13.882353	582.365929	12.571111
13.275408	559.761702	12.576128
13.249876	573.852552	12.581146
13.480348	578.991946	12.586163
13.841360	577.361043	12.591181
13.531682	581.887135	12.596199
13.851961	575.387067	12.601216
13.641145	584.138984	12.606234
13.832627	580.925085	12.611251
13.627541	583.986440	12.616269
13.679769	590.226517	12.621287
13.852747	582.774279	12.626304
13.814349	579.428920	12.631322
13.774488	581.360067	12.636339
14.018138	584.080169	12.641357
13.794625	586.383879	12.646375
13.602214	577.132999	12.651392
13.790722	577.302439	12.656410
13.628917	581.420516	12.661427
13.786930	585.094341	12.666445
13.468339	584.793648	12.671463
13.865292	577.956607	12.676480
13.663912	573.607878	12.681498
13.730595	577.863941	12.686515
13.743959	575.495093	12.691533
13.546582	580.663234	12.696551
13.556852	579.566601	12.701568
13.348604	583.183847	12.706586
13.805980	593.125558	12.711603
14.093168	596.391126	12.716621
13.881378	607.090255	12.721639
14.157508	604.475372	12.726656
14.413947	604.485920	12.731674
13.884553	589.190742	12.736691
13.885224	585.709917	12.741709
14.019324	581.217439	12.746727
14.101804	596.620027	12.751744
14.152065	601.023813	12.756762
13.926060	591.216447	12.761779
14.095013	603.355237	12.766797
14.001496	598.693075	12.771815
14.414397	599.070565	12.776832
14.314167	607.833677	12.781850
13.892198	596.308575	12.786867
14.201126	588.576403	12.791885
14.017436	593.297467	12.796903
14.305184	593.517725	12.801920
14.428604	590.513228	12.806938
14.340343	592.647563	12.811955
13.991625	583.787074	12.816973
14.136826	584.020059	12.821991
14.438958	587.744026	12.827008
14.273257	575.932896	12.832026
14.249577	580.976168	12.837043
14.230076	570.395079	12.842061
14.038562	578.796865	12.847079
14.340073	587.393280	12.852096
14.106099	605.704183	12.857114
14.557590	596.005916	12.862131
14.681769	597.251989	12.867149
14.143085	596.688931	12.872167
14.402423	579.147193	12.877184
14.421028	592.795704	12.882202
14.056131	594.922620	12.887219
14.326043	596.837095	12.892237
14.164514	597.625900	12.897255
14.336008	592.714204	12.902272
14.192944	604.444002	12.907290
14.224034	601.457035	12.912307
14.583933	592.864893	12.917325
14.566874	592.574054	12.922343
14.594642	592.383530	12.927360
14.596997	598.782847	12.932378
14.509984	597.568821	12.937395
14.837331	597.236983	12.942413
14.662559	595.446511	12.947431
14.475585	597.331140	12.952448
14.279755	598.548145	12.957466
14.525869	604.249976	12.962483
15.044197	595.513251	12.967501
14.480598	604.815545	12.972519
14.468568	603.015512	12.977536
14.334879	593.641877	12.982554
14.240000	601.747773	12.987571
14.782751	598.444467	12.992589
14.778735	601.345138	12.997607
14.789417	590.876097	13.002624
14.570725	595.719372	13.007642
14.573292	598.275049	13.012659
14.905210	591.151495	13.017677
14.564536	585.006785	13.022695
14.604319	590.065424	13.027712
14.517248	597.513723	13.032730
14.885477	604.534547	13.037747
14.809554	602.722372	13.042765
15.000368	622.431386	13.047783
14.867656	605.973102	13.052800
14.853266	597.565459	13.057818
14.563892	608.282980	13.062835
15.091521	613.641195	13.067853
15.018390	614.365746	13.072871
14.937988	601.638796	13.077888
15.011985	603.022065	13.082906
15.019041	610.064411	13.087923
14.778265	595.601568	13.092941
14.846666	593.432423	13.097959
15.083335	608.407089	13.102976
14.999254	615.432070	13.107994
14.885223	616.749945	13.113011
14.929775	617.184786	13.118029
14.993402	624.136283	13.123047
14.822299	619.066490	13.128064
14.764185	621.814647	13.133082
14.915893	632.542400	13.138099
14.829399	625.588115	13.143117
14.875533	618.370197	13.148135
14.771826	616.991519	13.153152
15.283241	618.877862	13.158170
14.946396	626.229368	13.163187
14.647291	617.086594	13.168205
15.252638	617.244781	13.173223
15.351733	624.850291	13.178240
15.437612	619.992941	13.183258
15.195253	623.015928	13.188275
15.160496	613.882488	13.193293
15.388188	618.391192	13.198311
15.213876	615.038587	13.203328
15.553866	619.340466	13.208346
15.280133	628.051710	13.213363
15.400887	624.394397	13.218381
15.600275	628.023921	13.223399
15.172236	622.864748	13.228416
15.244398	615.737449	13.233434
15.267666	623.692422	13.238451
15.148154	623.363888	13.243469
15.185751	615.270023	13.248487
15.155732	617.818153	13.253504
15.460290	623.744411	13.258522
15.476892	640.971808	13.263539
15.850579	633.873292	13.268557
15.301492	618.849387	13.273575
15.214400	618.004586	13.278592
15.743335	624.173609	13.283610
15.447523	628.744889	13.288627
15.411990	626.506719	13.293645
15.255589	635.414284	13.298663
15.475289	645.222623	13.303680
15.720993	650.678390	13.308698
15.888083	645.388683	13.313715
15.795057	636.964865	13.318733
15.858042	631.950136	13.323751
15.534935	628.279883	13.328768
15.476275	617.158931	13.333786
15.465580	623.800120	13.338803
15.790555	627.574185	13.343821
15.730896	640.250347	13.348839
15.547885	638.054071	13.353856
15.760676	640.949393	13.358874
16.063019	643.827618	13.363891
15.889939	631.386464	13.368909
15.674239	622.120252	13.373927
15.426239	623.600991	13.378944
15.531489	624.666984	13.383962
15.542505	634.687682	13.388979
15.870362	634.620841	13.393997
15.945239	635.527468	13.399015
15.974374	644.999419	13.404032
15.639844	641.949454	13.409050
15.715916	644.099233	13.414067
15.748693	641.585348	13.419085
15.582366	638.076868	13.424103
15.731940	631.275167	13.429120
16.079542	635.957702	13.434138
15.783284	645.691745	13.439155
16.103279	646.818975	13.444173
16.034511	632.834230	13.449191
15.868327	637.372707	13.454208
15.998390	636.683436	13.459226
15.645159	646.031890	13.464243
15.736121	645.541203	13.469261
16.236765	637.132246	13.474279
15.895276	648.425926	13.479296
16.194069	639.171116	13.484314
16.066280	641.718694	13.489331
15.892050	640.764388	13.494349
16.019721	639.302348	13.499367
16.173433	649.231412	13.504384
16.023363	648.895013	13.509402
15.893786	661.001431	13.514419
16.412417	658.932585	13.519437
16.746945	656.213933	13.524455
15.994837	650.799107	13.529472
15.918810	642.356860	13.534490
16.133600	654.078310	13.539507
16.160744	653.212566	13.544525
16.586609	661.650807	13.549543
16.384882	672.521971	13.554560
16.295986	654.554713	13.559578
16.259181	649.732235	13.564595
16.667258	656.989863	13.569613
16.525288	636.607323	13.574631
16.342710	635.679563	13.579648
16.005586	617.514315	13.584666
16.378829	632.035409	13.589683
16.294910	655.403641	13.594701
16.472249	658.683168	13.599719
16.596875	660.105894	13.604736
16.717694	652.475562	13.609754
16.142375	648.235526	13.614771
16.375567	655.851728	13.619789
16.906149	657.451081	13.624807
16.606666	660.170555	13.629824
16.267067	641.611207	13.634842
16.716150	643.576683	13.639859
16.600077	662.866483	13.644877
16.855041	652.798012	13.649895
16.327212	651.242377	13.654912
16.692775	652.274154	13.659930
16.647513	654.319754	13.664947
16.307462	650.342877	13.669965
16.734481	648.139980	13.674983
16.516045	658.234284	13.680000
16.906839	662.446216	13.685018
17.044287	661.093101	13.690035
17.117808	651.889136	13.695053
16.718528	642.843993	13.700071
16.563373	639.428443	13.705088
16.515862	635.929864	13.710106
16.628802	647.474671	13.715123
16.891438	655.613288	13.720141
16.999816	662.179150	13.725159
16.732477	665.789834	13.730176
16.922151	662.137562	13.735194
16.831677	663.568533	13.740211
17.038079	660.011483	13.745229
17.234795	654.029222	13.750247
16.406104	638.717487	13.755264
16.954310	646.316196	13.760282
16.440311	667.962136	13.765299
16.774735	659.039426	13.770317
17.250693	649.785427	13.775335
16.985239	666.296245	13.780352
16.603339	660.318867	13.785370
17.002472	665.375224	13.790387
17.027339	664.364672	13.795405
17.151715	661.801810	13.800423
16.865778	665.850874	13.805440
17.131683	664.887998	13.810458
16.913091	659.478462	13.815475
16.693443	661.525969	13.820493
17.226079	658.378855	13.825511
16.803207	659.546011	13.830528
16.994771	660.876267	13.835546
17.157715	665.805303	13.840563
16.588887	678.926827	13.845581
17.044094	676.126269	13.850599
17.244231	689.374219	13.855616
17.504163	685.398590	13.860634
17.202935	685.196174	13.865651
17.554278	685.179323	13.870669
17.597543	679.855238	13.875687
17.413972	673.859600	13.880704
17.591712	662.660789	13.885722
17.250734	659.892680	13.890739
17.191344	665.190835	13.895757
17.462199	651.976830	13.900775
17.168187	662.344825	13.905792
17.057103	662.895413	13.910810
17.421893	677.443106	13.915827
17.495413	682.988806	13.920845
17.688019	673.258223	13.925863
17.675236	678.946742	13.930880
17.735991	667.065580	13.935898
17.316743	662.693948	13.940915
17.301500	666.035017	13.945933
17.453497	674.266604	13.950951
17.523727	681.261274	13.955968
17.175851	676.689185	13.960986
17.356558	685.840924	13.966003
17.594565	690.455333	13.971021
17.483944	680.674132	13.976039
17.706108	681.071854	13.981056
17.437991	675.124091	13.986074
17.219358	676.849561	13.991091
17.225514	681.203432	13.996109
17.374098	671.470238	14.001127
17.565914	690.888850	14.006144
17.607449	694.580832	14.011162
18.124840	694.361410	14.016179
18.103962	695.936176	14.021197
17.876568	688.681924	14.026215
17.640715	683.388674	14.031232
17.716890	676.569982	14.036250
18.103490	682.764343	14.041267
17.840880	677.768738	14.046285
17.783961	670.216563	14.051303
17.749476	677.423188	14.056320
17.844035	694.957223	14.061338
18.297994	680.553396	14.066355
18.087306	691.605841	14.071373
18.017254	680.827437	14.076391
17.917312	678.113313	14.081408
17.769919	670.925504	14.086426
17.858282	674.566012	14.091443
17.848258	694.183304	14.096461
18.284484	691.524549	14.101479
18.345244	692.244036	14.106496
18.221006	691.531243	14.111514
18.051383	682.428233	14.116531
17.886448	675.489297	14.121549
18.016731	687.186058	14.126567
18.449404	686.717904	14.131584
18.239113	681.802512	14.136602
18.108395	671.396463	14.141619
17.965916	671.478587	14.146637
18.431059	675.738905	14.151655
18.064183	678.816000	14.156672
18.035093	696.173636	14.161690
18.275893	684.516886	14.166707
17.992391	696.088736	14.171725
18.302151	690.978767	14.176743
18.269067	686.619585	14.181760
18.187702	695.048456	14.186778
18.616100	683.898965	14.191795
17.874771	692.386408	14.196813
18.250627	695.278440	14.201831
18.380127	694.649213	14.206848
18.202294	694.487543	14.211866
18.292319	697.796450	14.216883
18.167940	700.999888	14.221901
18.529363	698.778797	14.226919
18.564299	701.992144	14.231936
18.385808	691.391557	14.236954
18.706943	681.057157	14.241971
18.612577	689.841486	14.246989
18.443154	680.552260	14.252007
18.456778	687.281202	14.257024
18.419715	688.101123	14.262042
18.769540	684.288217	14.267059
18.773613	680.412383	14.272077
18.619008	690.212755	14.277095
18.553756	686.931516	14.282112
18.652217	683.413356	14.287130
18.784402	682.758466	14.292147
18.563101	690.243482	14.297165
18.500680	688.779477	14.302183
18.639953	693.182051	14.307200
18.368863	708.352617	14.312218
19.172042	705.242266	14.317235
18.625776	705.712294	14.322253
19.291751	716.928053	14.327271
19.071802	687.727970	14.332288
18.820568	684.769167	14.337306
18.856748	681.434268	14.342323
18.659150	682.547416	14.347341
18.718711	693.144391	14.352359
19.006877	697.672101	14.357376
18.890925	709.451394	14.362394
19.151925	702.490311	14.367411
18.786101	707.520620	14.372429
19.091467	701.584541	14.377447
19.134835	707.595673	14.382464
19.206458	711.380801	14.387482
19.148430	696.428692	14.392499
19.009724	695.159594	14.397517
19.168408	700.064057	14.402535
19.130223	692.442686	14.407552
19.064757	691.512467	14.412570
19.107535	691.010347	14.417587
19.132083	701.963059	14.422605
19.307831	705.649926	14.427623
19.399455	707.472256	14.432640
19.040655	698.240907	14.437658
19.139324	694.735336	14.442675
18.928917	708.855078	14.447693
19.201509	700.080825	14.452711
19.195996	700.419325	14.457728
19.128287	708.675669	14.462746
19.353310	705.494393	14.467763
19.263010	703.583465	14.472781
19.291925	707.725523	14.477799
19.293105	707.286681	14.482816
18.959392	711.993266	14.487834
19.273419	700.063182	14.492851
19.087125	707.845701	14.497869
19.277066	699.816437	14.502887
19.430295	703.235421	14.507904
19.217109	713.937987	14.512922
19.814714	713.579847	14.517939
19.679916	712.401655	14.522957
19.512949	707.387995	14.527975
19.520202	696.297755	14.532992
19.590349	707.735660	14.538010
19.525749	699.730248	14.543027
19.365229	702.125146	14.548045
19.622405	719.482415	14.553063
19.773681	725.098069	14.558080
19.429696	729.831503	14.563098
19.763849	731.505625	14.568115
19.755075	723.191720	14.573133
19.489426	722.986920	14.578151
19.982062	723.989449	14.583168
19.718216	724.879393	14.588186
20.159746	729.572575	14.593203
20.048211	723.114439	14.598221
19.707621	716.994915	14.603239
20.005440	698.374133	14.608256
19.675352	713.140494	14.613274
20.028099	716.522105	14.618291
20.025720	707.172144	14.623309
19.606812	714.504906	14.628327
19.802053	720.239942	14.633344
19.706016	724.458261	14.638362
19.800768	724.512917	14.643379
20.181970	726.978104	14.648397
19.661488	727.381004	14.653415
19.979718	729.272193	14.658432
19.716088	732.295353	14.663450
19.834378	725.451152	14.668467
19.855082	732.339949	14.673485
20.169959	730.252328	14.678503
20.099040	728.900093	14.683520
19.684983	731.444919	14.688538
20.034876	723.012057	14.693555
20.243381	731.925970	14.698573
19.973723	736.105054	14.703591
20.595475	735.758934	14.708608
20.009194	739.315152	14.713626
20.516172	740.271270	14.718643
20.196516	732.034164	14.723661
20.616820	740.927729	14.728679
20.542388	728.221847	14.733696
20.475378	734.439516	14.738714
20.075568	723.876524	14.743731
20.490766	728.447577	14.748749
20.346380	737.681515	14.753767
20.342315	731.490656	14.758784
20.146129	727.425093	14.763802
20.024217	736.803849	14.768819
20.546200	753.485627	14.773837
20.770041	762.930481	14.778855
20.654983	743.001206	14.783872
20.555727	740.192294	14.788890
20.463426	743.778897	14.793907
20.750872	755.735246	14.798925
20.622661	755.272369	14.803943
20.616158	750.751248	14.808960
20.684619	757.440121	14.813978
20.628435	750.982825	14.818995
20.739000	750.826743	14.824013
20.224833	742.443198	14.829031
20.960943	745.471647	14.834048
20.521749	760.674742	14.839066
20.653563	746.018071	14.844083
20.525355	743.197888	14.849101
20.301492	753.880051	14.854119
20.328791	745.655189	14.859136
20.345936	748.120259	14.864154
20.533316	745.856834	14.869171
20.806824	748.932062	14.874189
20.516347	774.017753	14.879207
21.330249	767.005274	14.884224
20.981545	771.982444	14.889242
21.157865	755.722050	14.894259
21.007595	749.367762	14.899277
20.785807	750.342675	14.904295
21.426184	740.962048	14.909312
21.112354	750.348602	14.914330
20.868295	742.222794	14.919347
20.908334	745.703589	14.924365
20.686305	746.306166	14.929383
20.974696	750.603489	14.934400
21.163235	762.051396	14.939418
21.288161	771.003587	14.944435
21.472151	770.391119	14.949453
21.236711	769.818709	14.954471
21.200514	750.527221	14.959488
21.067619	752.592788	14.964506
21.328270	769.416251	14.969523
21.468477	770.457876	14.974541
21.118819	767.511227	14.979559
21.276519	763.273797	14.984576
21.267393	765.922834	14.989594
21.588964	768.189034	14.994611
21.409586	762.776517	14.999629
21.366282	757.484822	15.004647
21.460640	757.473270	15.009664
21.348707	752.236441	15.014682
21.327525	764.250316	15.019699
21.177294	765.084704	15.024717
21.314042	770.693168	15.029735
21.635126	772.653342	15.034752
21.626346	775.463267	15.039770
21.560817	764.185507	15.044787
21.523285	771.714527	15.049805
21.207113	778.090920	15.054823
21.354119	766.817937	15.059840
21.561782	765.021550	15.064858
21.395800	778.550626	15.069875
21.435696	766.502237	15.074893
21.079049	770.054266	15.079911
21.765276	778.395223	15.084928
21.525208	783.658429	15.089946
21.761773	793.303283	15.094963
21.780236	791.637335	15.099981
21.650471	803.469332	15.104999
22.064735	785.982162	15.110016
21.795035	788.529766	15.115034
21.934263	796.018651	15.120051
21.969422	786.179982	15.125069
21.898889	789.182555	15.130087
22.173753	789.979161	15.135104
21.731669	798.132893	15.140122
22.017885	790.113845	15.145139
21.795608	783.089124	15.150157
21.978890	794.152874	15.155175
22.073070	790.225119	15.160192
22.371698	787.089172	15.165210
22.116733	794.361729	15.170227
21.965202	792.665445	15.175245
21.910105	787.236726	15.180263
21.943838	787.515470	15.185280
22.005298	786.622287	15.190298
22.046167	783.315040	15.195315
22.237989	787.557981	15.200333
21.765345	796.136180	15.205351
22.079494	795.083737	15.210368
22.392686	788.893954	15.215386
22.335876	784.541598	15.220403
22.586701	784.903304	15.225421
22.763444	794.087272	15.230439
22.525322	789.898840	15.235456
22.554205	799.449805	15.240474
22.162874	802.480237	15.245491
22.626775	785.950985	15.250509
22.412904	787.117165	15.255527
22.591408	787.862504	15.260544
22.729638	790.296104	15.265562
22.530748	787.786710	15.270579
22.244498	785.180469	15.275597
22.308260	780.752539	15.280615
22.491048	789.171884	15.285632
22.586027	781.936827	15.290650
22.510559	783.696820	15.295667
22.931128	782.454245	15.300685
22.532687	787.735799	15.305703
22.293282	782.051764	15.310720
22.680171	778.709579	15.315738
22.550542	784.286939	15.320755
22.870231	774.508114	15.325773
22.530315	780.922918	15.330791
22.645073	783.925043	15.335808
22.616799	778.066130	15.340826
22.648557	788.490771	15.345843
22.877383	783.270305	15.350861
22.489758	784.870623	15.355879
22.340993	783.839763	15.360896
22.751044	788.670401	15.365914
22.822026	814.469864	15.370931
22.985297	804.649106	15.375949
23.009337	808.713054	15.380967
23.031179	806.273430	15.385984
23.307016	807.262383	15.391002
23.045753	811.739970	15.396019
22.935195	806.742745	15.401037
23.433461	802.272405	15.406055
23.328545	805.867296	15.411072
23.326864	802.172207	15.416090
23.050547	796.793707	15.421107
22.940874	778.059566	15.426125
23.184879	801.679882	15.431143
23.236900	802.567987	15.436160
23.430872	793.537694	15.441178
23.023754	812.964486	15.446195
23.137818	804.959611	15.451213
23.190390	803.250482	15.456231
23.411113	803.550605	15.461248
23.207755	798.649879	15.466266
23.040865	800.954267	15.471283
23.379365	802.495180	15.476301
23.106969	798.892732	15.481319
23.119255	803.169941	15.486336
23.020820	804.273969	15.491354
22.990944	813.584789	15.496371
23.258008	816.093005	15.501389
23.577582	822.575553	15.506407
23.692744	829.471770	15.511424
23.679251	826.961908	15.516442
23.510259	822.570206	15.521459
23.920210	820.126955	15.526477
23.556889	824.194415	15.531495
23.470545	827.189989	15.536512
23.811324	824.602878	15.541530
23.633428	836.309851	15.546547
23.914188	824.889777	15.551565
23.853551	830.967635	15.556583
23.746799	823.700856	15.561600
23.957787	816.116373	15.566618
23.729254	812.835287	15.571635
23.873812	812.232112	15.576653
23.776413	808.700243	15.581671
23.886286	810.573389	15.586688
23.837162	821.622850	15.591706
23.498391	828.308884	15.596723
24.042542	822.259851	15.601741
24.146778	826.645822	15.606759
23.979249	831.295007	15.611776
23.995822	826.997486	15.616794
23.681693	830.135820	15.621811
23.923816	829.523765	15.626829
23.528668	829.926088	15.631847
23.841011	826.292552	15.636864
24.187094	823.357487	15.641882
23.995648	819.420549	15.646899
24.135323	827.515275	15.651917
24.273893	830.554724	15.656935
24.021022	822.733200	15.661952
24.082944	828.612100	15.666970
24.119548	838.537413	15.671987
24.571720	836.712418	15.677005
24.594307	833.638376	15.682023
24.350247	831.704037	15.687040
24.218174	822.503593	15.692058
23.944210	830.369241	15.697075
24.124350	842.591657	15.702093
24.321878	850.387060	15.707111
24.478779	841.769602	15.712128
24.495943	840.564585	15.717146
25.134010	843.308524	15.722163
24.852057	848.127003	15.727181
24.441223	832.664836	15.732199
24.349481	842.180957	15.737216
24.910942	839.770918	15.742234
24.559469	838.519158	15.747251
24.953233	837.678373	15.752269
25.127960	819.054539	15.757287
24.984301	822.554483	15.762304
24.603624	812.174646	15.767322
24.527854	815.818648	15.772339
24.301143	815.304835	15.777357
24.995734	823.398366	15.782375
24.915416	829.299412	15.787392
24.479597	830.894615	15.792410
25.088930	847.294646	15.797427
24.975887	843.418077	15.802445
25.071357	840.758707	15.807463
24.945955	827.192869	15.812480
24.756498	823.763690	15.817498
24.878778	834.164796	15.822515
24.837336	852.931957	15.827533
25.100912	847.459915	15.832551
24.773570	848.593274	15.837568
25.046200	841.683974	15.842586
24.904941	841.664926	15.847603
24.977135	844.525370	15.852621
24.752404	845.178863	15.857639
24.544829	846.571278	15.862656
25.260575	838.643117	15.867674
25.035233	849.066798	15.872691
25.177294	841.704470	15.877709
25.182624	839.163273	15.882727
25.051711	846.877271	15.887744
25.352403	850.737214	15.892762
25.608391	865.570238	15.897779
25.484585	861.420793	15.902797
25.099967	849.302747	15.907815
25.430535	859.235951	15.912832
25.627233	868.909143	15.917850
25.505517	853.739606	15.922867
25.383558	865.343217	15.927885
25.473510	858.547557	15.932903
25.256928	861.708577	15.937920
25.227747	855.953919	15.942938
25.099028	860.773790	15.947955
25.156457	863.885837	15.952973
25.289199	853.362924	15.957991
25.201432	859.202026	15.963008
25.774574	868.699847	15.968026
25.950389	867.350210	15.973043
25.727551	871.695601	15.978061
25.856289	867.257533	15.983079
25.828978	877.637776	15.988096
25.752996	868.668409	15.993114
25.764613	876.420188	15.998131
25.594246	872.852331	16.003149
25.950078	879.704785	16.008167
26.142064	882.773796	16.013184
26.103933	871.195064	16.018202
25.818561	875.155727	16.023219
26.018544	880.609217	16.028237
26.090528	867.861505	16.033255
25.857125	870.895762	16.038272
26.338799	874.405648	16.043290
25.866136	882.788237	16.048307
25.325638	893.270479	16.053325
25.865967	884.829981	16.058343
26.322158	895.920731	16.063360
26.723752	887.549168	16.068378
26.603382	881.013457	16.073395
26.274565	882.528890	16.078413
26.088768	878.190283	16.083431
26.176760	878.091361	16.088448
26.055262	880.439183	16.093466
25.996627	887.214164	16.098483
25.887330	885.460804	16.103501
26.222111	880.987496	16.108519
26.090618	881.096313	16.113536
25.966013	888.373857	16.118554
26.301635	898.246337	16.123571
26.537841	912.896292	16.128589
26.867627	908.370108	16.133607
26.629455	910.682453	16.138624
26.665069	909.764886	16.143642
26.973069	908.631345	16.148659
26.643688	898.663182	16.153677
26.573286	885.372752	16.158695
26.215632	883.225726	16.163712
26.569628	893.751733	16.168730
26.420982	900.382946	16.173747
26.594795	903.467413	16.178765
26.929500	900.429968	16.183783
26.552519	903.808468	16.188800
26.508082	898.213958	16.193818
26.602676	909.064376	16.198835
26.667111	909.278384	16.203853
26.876270	899.800715	16.208871
26.827211	905.589625	16.213888
27.258510	910.473791	16.218906
26.992849	908.350308	16.223923
26.936109	904.922540	16.228941
27.020581	902.249094	16.233959
26.942373	906.922261	16.238976
27.000748	904.293903	16.243994
27.157533	898.904743	16.249011
26.753676	915.213283	16.254029
27.062629	912.388123	16.259047
26.849530	920.761873	16.264064
27.450209	917.083426	16.269082
27.723286	915.485119	16.274099
27.228341	909.225463	16.279117
27.380932	903.032244	16.284135
26.971501	908.476486	16.289152
27.097297	903.085838	16.294170
27.697071	904.639728	16.299187
27.544453	916.434334	16.304205
27.495088	899.539932	16.309223
27.371418	900.029373	16.314240
27.194874	900.691144	16.319258
27.418207	904.115030	16.324275
27.535972	919.490315	16.329293
27.441970	912.578111	16.334311
27.726809	914.812181	16.339328
27.493569	917.944248	16.344346
27.682011	926.179745	16.349363
27.644971	922.676324	16.354381
27.983747	922.399505	16.359399
28.105275	922.768721	16.364416
27.656425	909.376253	16.369434
27.712280	906.233904	16.374451
27.691530	921.229979	16.379469
28.171215	907.140691	16.384487
27.546278	908.459240	16.389504
27.861483	925.189153	16.394522
28.074957	922.473529	16.399539
27.960479	924.028176	16.404557
28.043155	918.107763	16.409575
27.626044	919.886249	16.414592
28.145078	923.273567	16.419610
27.742683	919.558794	16.424627
27.830040	924.152540	16.429645
27.599295	925.286642	16.434663
27.507443	921.555076	16.439680
27.732839	917.647887	16.444698
27.979258	916.362992	16.449715
27.756912	939.169340	16.454733
27.934192	932.113908	16.459751
28.241719	942.404187	16.464768
28.279293	942.909548	16.469786
28.569684	938.742933	16.474803
28.608536	938.616949	16.479821
28.818072	933.519360	16.484839
28.838052	930.530911	16.489856
28.500352	924.369840	16.494874
28.274789	915.139724	16.499891
28.461740	918.663949	16.504909
28.212133	913.066665	16.509927
28.509892	922.377022	16.514944
28.586241	925.691257	16.519962
29.001950	928.851672	16.524979
28.842584	928.709214	16.529997
28.458716	914.650233	16.535015
28.452699	918.346510	16.540032
28.668310	931.232480	16.545050
28.621442	923.448263	16.550067
28.586700	939.071365	16.555085
28.780357	932.177482	16.560103
28.798438	931.704446	16.565120
28.790969	939.159429	16.570138
29.002804	927.327153	16.575155
28.978971	933.528701	16.580173
28.960323	921.236864	16.585191
29.178949	933.652163	16.590208
29.027979	929.327054	16.595226
28.996887	914.140200	16.600243
28.764837	923.652964	16.605261
29.106991	931.798262	16.610279
28.977842	929.139138	16.615296
28.854905	939.916149	16.620314
28.719765	932.357106	16.625331
28.891028	940.330203	16.630349
29.063670	930.798244	16.635367
28.955163	931.310571	16.640384
28.915438	936.381687	16.645402
28.924393	935.780687	16.650419
29.133976	938.070658	16.655437
29.143453	944.333294	16.660455
29.335176	951.779359	16.665472
29.335478	959.081666	16.670490
29.717062	957.829370	16.675507
29.372936	955.755966	16.680525
29.135599	947.629018	16.685543
29.293326	945.275512	16.690560
29.171308	958.914642	16.695578
29.498009	952.233560	16.700595
29.845922	947.581471	16.705613
29.701190	955.569061	16.710631
29.631419	950.846306	16.715648
29.712492	954.973990	16.720666
29.790552	948.883875	16.725683
29.660959	954.805258	16.730701
29.301521	953.649402	16.735719
29.951360	950.619687	16.740736
29.118661	958.386195	16.745754
29.918185	951.350637	16.750771
29.547504	955.154190	16.755789
29.576770	961.590472	16.760807
29.964506	966.844347	16.765824
29.883508	960.422395	16.770842
30.115069	964.495093	16.775859
30.352903	975.471570	16.780877
30.280275	964.920608	16.785895
30.046589	961.671854	16.790912
30.310355	974.641874	16.795930
30.401196	955.172598	16.800947
30.214578	950.329183	16.805965
30.269766	947.666601	16.810983
30.186199	937.407686	16.816000
30.252266	951.030149	16.821018
30.029618	943.017677	16.826035
30.152569	947.167241	16.831053
30.321159	962.840755	16.836071
30.662462	958.375881	16.841088
30.473385	976.402470	16.846106
30.198197	965.753660	16.851123
30.283059	970.208954	16.856141
30.645297	971.960776	16.861159
30.672192	960.485469	16.866176
30.607016	970.723342	16.871194
30.350201	964.789499	16.876211
30.361043	975.586728	16.881229
30.595262	962.589632	16.886247
30.740750	967.190117	16.891264
30.391346	969.898475	16.896282
30.537008	967.739346	16.901299
30.296739	972.740712	16.906317
30.638916	975.931519	16.911335
30.837694	967.989119	16.916352
30.390765	977.885655	16.921370
30.740092	970.408953	16.926387
30.409741	970.062747	16.931405
30.503930	978.092042	16.936423
30.868449	972.717852	16.941440
30.560180	982.920999	16.946458
31.044956	974.479641	16.951475
31.444347	976.945187	16.956493
31.076230	973.477525	16.961511
31.239538	973.856016	16.966528
31.247249	978.307545	16.971546
31.460393	977.542212	16.976563
31.426011	978.551073	16.981581
31.284083	977.509669	16.986599
31.334804	980.790036	16.991616
31.330966	975.640451	16.996634
31.301990	971.394166	17.001651
31.003135	981.147731	17.006669
31.126254	988.383591	17.011687
31.471546	981.926818	17.016704
31.522769	978.646324	17.021722
31.415671	976.977817	17.026739
31.629679	973.842390	17.031757
31.269458	979.159073	17.036775
31.312247	970.732885	17.041792
31.043616	976.246742	17.046810
31.585225	966.562646	17.051827
31.512535	973.017962	17.056845
31.595955	970.742293	17.061863
31.878141	969.745309	17.066880
31.576777	979.385657	17.071898
31.970413	974.982056	17.076915
31.791830	970.096360	17.081933
31.715048	978.111250	17.086951
32.355083	976.967033	17.091968
31.814179	975.615371	17.096986
31.619428	966.730717	17.102003
32.053110	975.634940	17.107021
31.822990	983.844116	17.112039
32.111459	993.149646	17.117056
32.021752	997.733110	17.122074
32.117275	990.703007	17.127091
32.306624	994.996875	17.132109
32.174477	1004.099660	17.137127
32.057069	992.274422	17.142144
31.957308	1005.638728	17.147162
31.982331	998.976198	17.152179
32.269271	1003.005570	17.157197
31.982167	996.732457	17.162215
32.314370	993.588090	17.167232
32.096700	998.270372	17.172250
32.415081	999.688205	17.177267
32.510421	998.792892	17.182285
31.695499	1000.478691	17.187303
32.195650	999.763343	17.192320
32.252907	1020.105807	17.197338
32.614144	1018.525323	17.202355
32.639632	1030.380635	17.207373
32.658655	1022.040171	17.212391
32.827449	1018.716119	17.217408
32.473851	1021.469319	17.222426
32.801393	1018.887397	17.227443
33.010471	1015.355106	17.232461
32.729934	1021.593496	17.237479
32.917316	1016.145889	17.242496
33.146230	1024.236278	17.247514
32.885415	1013.045569	17.252531
33.163737	1012.727669	17.257549
32.692170	1009.052048	17.262567
33.108911	1005.891362	17.267584
33.354852	1016.263855	17.272602
32.982233	999.564851	17.277619
32.804402	982.485249	17.282637
32.795083	1000.266129	17.287655
32.776974	1011.689568	17.292672
32.769755	1012.018873	17.297690
33.097357	1011.238873	17.302707
33.323832	1006.469979	17.307725
33.129860	1017.611540	17.312743
32.822056	1008.924344	17.317760
33.031773	1011.381558	17.322778
32.825559	1010.460613	17.327795
33.118560	1016.477163	17.332813
33.365829	1034.877679	17.337831
33.322923	1038.403003	17.342848
33.618110	1038.978710	17.347866
33.661687	1049.281745	17.352883
33.733219	1035.947013	17.357901
33.926839	1041.319494	17.362919
33.890243	1028.803163	17.367936
33.568167	1012.538083	17.372954
33.633241	1012.546869	17.377971
33.737787	1022.947692	17.382989
33.649799	1030.503611	17.388007
33.638532	1030.808300	17.393024
33.942421	1033.216141	17.398042
33.762485	1032.101759	17.403059
34.101047	1028.000205	17.408077
33.688715	1032.163703	17.413095
34.008946	1030.100460	17.418112
33.883121	1035.535298	17.423130
33.988562	1037.308174	17.428147
34.010216	1029.475374	17.433165
33.797090	1037.246435	17.438183
33.845562	1029.210647	17.443200
33.845144	1033.250053	17.448218
33.861001	1031.881128	17.453235
34.109179	1029.658693	17.458253
33.729334	1044.079631	17.463271
34.005011	1049.054337	17.468288
34.190094	1062.311222	17.473306
34.378462	1059.596331	17.478323
34.477674	1051.599969	17.483341
34.468696	1049.461750	17.488359
34.447204	1050.979840	17.493376
34.600703	1054.525080	17.498394
34.388005	1054.813795	17.503411
34.728220	1052.539159	17.508429
34.367440	1058.749031	17.513447
34.485266	1050.715058	17.518464
34.543040	1054.208931	17.523482
34.473156	1054.623731	17.528499
34.940444	1049.975119	17.533517
34.586309	1059.778359	17.538535
35.131312	1049.737089	17.543552
34.822152	1049.526435	17.548570
34.703671	1047.963833	17.553587
34.712521	1049.496134	17.558605
34.820667	1051.846093	17.563623
34.799949	1047.327110	17.568640
34.534927	1052.452271	17.573658
34.702621	1051.331099	17.578675
34.906700	1049.254382	17.583693
34.926825	1060.936983	17.588711
34.922077	1063.803129	17.593728
35.456046	1063.221367	17.598746
35.036578	1079.728145	17.603763
35.266648	1075.895932	17.608781
34.804175	1078.814412	17.613799
35.436379	1074.332619	17.618816
35.249065	1067.450662	17.623834
34.981529	1077.817931	17.628851
35.108025	1074.030247	17.633869
35.073842	1079.769561	17.638887
34.988104	1073.420889	17.643904
35.037984	1071.544899	17.648922
35.049359	1076.150514	17.653939
35.766961	1086.175062	17.658957
35.663412	1095.999266	17.663975
35.725993	1096.507050	17.668992
36.000718	1093.772397	17.674010
35.768643	1093.272034	17.679027
35.839846	1087.649992	17.684045
36.174916	1081.563998	17.689063
35.655855	1068.990214	17.694080
35.736416	1069.444706	17.699098
35.209648	1074.424437	17.704115
35.676715	1090.310365	17.709133
35.880957	1094.961695	17.714151
35.813113	1100.059326	17.719168
35.776865	1087.915279	17.724186
35.827380	1098.662225	17.729203
36.137804	1089.077172	17.734221
36.088588	1096.671263	17.739239
36.260142	1083.772196	17.744256
36.672975	1078.185328	17.749274
36.185374	1091.386025	17.754291
36.413020	1085.777495	17.759309
36.256874	1080.891431	17.764327
36.548175	1081.341514	17.769344
36.531869	1078.898324	17.774362
35.877485	1083.913705	17.779379
36.125205	1081.972198	17.784397
36.441891	1088.076603	17.789415
36.498109	1082.501076	17.794432
36.369332	1092.767856	17.799450
36.236474	1088.111690	17.804467
36.799513	1101.852549	17.809485
36.906871	1111.978435	17.814503
36.935958	1095.478727	17.819520
36.923245	1086.489932	17.824538
36.594935	1082.896131	17.829555
36.635789	1082.829794	17.834573
36.436580	1087.553405	17.839591
36.482612	1102.993664	17.844608
37.100885	1100.095070	17.849626
36.997731	1105.491686	17.854643
37.124844	1101.542956	17.859661
37.110266	1105.048104	17.864679
37.002217	1109.334655	17.869696
37.343729	1105.330453	17.874714
37.054083	1117.806081	17.879731
37.220462	1104.358702	17.884749
37.433649	1108.008267	17.889767
36.982081	1104.282175	17.894784
37.040709	1109.704096	17.899802
37.412211	1111.975191	17.904819
37.190208	1106.288342	17.909837
37.092975	1107.111339	17.914855
37.040038	1105.049385	17.919872
37.156096	1102.049104	17.924890
36.971329	1106.742069	17.929907
37.019378	1097.630202	17.934925
37.021741	1115.128515	17.939943
37.247532	1130.758558	17.944960
37.932693	1121.900929	17.949978
37.941442	1127.482098	17.954995
37.857819	1126.090785	17.960013
37.333260	1124.932224	17.965031
37.667412	1127.098684	17.970048
37.724803	1116.401158	17.975066
37.719242	1127.519765	17.980083
38.027448	1123.445006	17.985101
37.803046	1124.691741	17.990119
37.705699	1123.605518	17.995136
37.767239	1115.510853	18.000154
38.067763	1125.518310	18.005171
37.861551	1119.664899	18.010189
37.924223	1115.076111	18.015207
37.888671	1125.905901	18.020224
38.281784	1120.438853	18.025242
38.404705	1129.574572	18.030259
38.116695	1131.080517	18.035277
38.314651	1125.867912	18.040295
38.528502	1139.732594	18.045312
38.419078	1123.901357	18.050330
38.254258	1124.390899	18.055347
38.520037	1128.442529	18.060365
38.863304	1132.046600	18.065383
38.153536	1125.558385	18.070400
38.776642	1130.318076	18.075418
38.795178	1125.089226	18.080435
38.568700	1118.090272	18.085453
38.636011	1115.122825	18.090471
38.518879	1123.043078	18.095488
38.846050	1127.419660	18.100506
38.653204	1139.719288	18.105523
38.762350	1143.063170	18.110541
38.940878	1142.082316	18.115559
38.837056	1142.830602	18.120576
38.596303	1136.597559	18.125594
38.788453	1138.508422	18.130611
38.451961	1139.728429	18.135629
38.746497	1122.600393	18.140647
38.670184	1138.649860	18.145664
39.039900	1135.736311	18.150682
39.023353	1154.080197	18.155699
39.247285	1147.784268	18.160717
39.390736	1160.318726	18.165735
39.246200	1167.261820	18.170752
39.579592	1162.192218	18.175770
39.411900	1150.469377	18.180787
39.214720	1146.214525	18.185805
39.578618	1154.085144	18.190823
39.548870	1149.671681	18.195840
39.496460	1150.187903	18.200858
39.731749	1158.154286	18.205875
39.752665	1146.455730	18.210893
39.750500	1135.180492	18.215911
39.452677	1136.432348	18.220928
39.290570	1132.989382	18.225946
39.698213	1147.840055	18.230963
39.479998	1158.082929	18.235981
39.455169	1152.595738	18.240999
39.724469	1160.935519	18.246016
39.918382	1161.246134	18.251034
39.797368	1163.675968	18.256051
39.814391	1160.833106	18.261069
39.895513	1156.320330	18.266087
39.375515	1159.279337	18.271104
39.873345	1157.049575	18.276122
40.008635	1162.396460	18.281139
40.091889	1175.208541	18.286157
40.191121	1182.138934	18.291175
40.162378	1182.982829	18.296192
40.540075	1172.449992	18.301210
39.988811	1178.519151	18.306227
39.887678	1180.939580	18.311245
40.132442	1185.562535	18.316263
40.160273	1184.826045	18.321280
40.551670	1176.389663	18.326298
40.277227	1184.523782	18.331315
40.433669	1183.688374	18.336333
40.519752	1170.752059	18.341351
40.234749	1178.420765	18.346368
40.653321	1180.179616	18.351386
40.422104	1204.029090	18.356403
40.565093	1203.381966	18.361421
41.226562	1192.132755	18.366439
40.911738	1204.082193	18.371456
41.248663	1203.922422	18.376474
41.022483	1189.482069	18.381491
40.748099	1187.025397	18.386509
40.981995	1183.249370	18.391527
41.015312	1200.395812	18.396544
40.734907	1195.232420	18.401562
41.099542	1203.131348	18.406579
41.237193	1205.467266	18.411597
41.279498	1195.661971	18.416615
41.090818	1206.891188	18.421632
41.023944	1205.128035	18.426650
41.032324	1200.547679	18.431667
41.494068	1206.591670	18.436685
41.399369	1199.562699	18.441703
41.118221	1210.632748	18.446720
41.581613	1200.556763	18.451738
41.288277	1200.308930	18.456755
41.109470	1202.264933	18.461773
41.529298	1201.088717	18.466791
41.259576	1204.482131	18.471808
41.403994	1216.580980	18.476826
41.610133	1217.451422	18.481843
41.531671	1217.062837	18.486861
41.832192	1220.676738	18.491879
41.837427	1221.745716	18.496896
41.948919	1214.204957	18.501914
41.755377	1218.697348	18.506931
41.888300	1222.798087	18.511949
42.018903	1214.437006	18.516967
41.765910	1233.530993	18.521984
41.972389	1218.117543	18.527002
42.425478	1224.162888	18.532019
42.109887	1219.689771	18.537037
41.900681	1219.176376	18.542055
42.173129	1224.221062	18.547072
42.163535	1220.321992	18.552090
42.504642	1221.635320	18.557107
42.390941	1225.465191	18.562125
42.630869	1219.245641	18.567143
42.537640	1221.033689	18.572160
42.676288	1203.850951	18.577178
42.562409	1213.809371	18.582195
42.296664	1209.457883	18.587213
42.792510	1219.974622	18.592231
42.616857	1224.167586	18.597248
42.378358	1220.682849	18.602266
42.594999	1230.261616	18.607283
42.757644	1234.550233	18.612301
43.145766	1232.246025	18.617319
42.824723	1234.612339	18.622336
43.180918	1239.094883	18.627354
43.311398	1229.913309	18.632371
43.361777	1214.221211	18.637389
43.039060	1206.470351	18.642407
42.839532	1204.125098	18.647424
42.916420	1204.236185	18.652442
43.175259	1209.784754	18.657459
43.204881	1218.505859	18.662477
43.348553	1216.283894	18.667495
43.350470	1219.928506	18.672512
43.025103	1223.248537	18.677530
43.261906	1219.434180	18.682547
43.238169	1237.836076	18.687565
43.328484	1230.759352	18.692583
43.384662	1234.458635	18.697600
43.419234	1235.418905	18.702618
43.520927	1231.019671	18.707635
43.572721	1232.800920	18.712653
43.733602	1225.871000	18.717671
43.361003	1230.037825	18.722688
43.276142	1236.675011	18.727706
43.408996	1235.571876	18.732723
43.458762	1240.553406	18.737741
44.060677	1248.828819	18.742759
43.809060	1256.400843	18.747776
43.485553	1254.504073	18.752794
43.948313	1254.466721	18.757811
43.753744	1256.734451	18.762829
43.770553	1255.816638	18.767847
43.826356	1258.771218	18.772864
44.005162	1255.533926	18.777882
44.211193	1262.182635	18.782899
44.110208	1277.128386	18.787917
44.406861	1273.311011	18.792935
44.482053	1277.455465	18.797952
44.507381	1279.376538	18.802970
44.739313	1272.912063	18.807987
44.842887	1273.514455	18.813005
44.716861	1257.534205	18.818023
44.689690	1254.590913	18.823040
44.000019	1251.255310	18.828058
43.706123	1253.828836	18.833075
44.079881	1265.080974	18.838093
44.510067	1265.004513	18.843111
44.639366	1261.393076	18.848128
44.756264	1272.325450	18.853146
44.783991	1283.981768	18.858163
44.478495	1289.877001	18.863181
44.956128	1287.243270	18.868199
44.903545	1287.674317	18.873216
44.834184	1294.088206	18.878234
44.863306	1290.558632	18.883251
44.862438	1286.733928	18.888269
44.912059	1287.518290	18.893287
44.846241	1292.189628	18.898304
45.095345	1303.107749	18.903322
45.612055	1305.466714	18.908339
45.527090	1309.531970	18.913357
45.515061	1310.717250	18.918375
45.572698	1302.951310	18.923392
45.363592	1304.580683	18.928410
45.766408	1293.630454	18.933427
45.721924	1301.160780	18.938445
45.500513	1297.477708	18.943463
45.678700	1296.550547	18.948480
45.915022	1297.978025	18.953498
46.025755	1290.036566	18.958515
45.588845	1282.388659	18.963533
45.956931	1281.908457	18.968551
45.842617	1277.770060	18.973568
45.536810	1281.289027	18.978586
46.166777	1291.396764	18.983603
46.060826	1304.945294	18.988621
46.434191	1302.457183	18.993639
46.081027	1305.576431	18.998656
46.078814	1306.365708	19.003674
46.263219	1301.338198	19.008691
45.938938	1311.667101	19.013709
46.009382	1299.875526	19.018727
46.130557	1297.767506	19.023744
45.983899	1301.889702	19.028762
46.327337	1301.331286	19.033779
46.359124	1301.449397	19.038797
46.339843	1302.604247	19.043815
46.307663	1313.739738	19.048832
46.437636	1327.592380	19.053850
46.552386	1328.716897	19.058867
46.567199	1331.147697	19.063885
46.984630	1327.737539	19.068903
46.928618	1336.522527	19.073920
46.890934	1343.916112	19.078938
46.931208	1341.167432	19.083955
47.096078	1332.892478	19.088973
47.008734	1333.805464	19.093991
47.144882	1335.523096	19.099008
46.487200	1343.641216	19.104026
47.015004	1331.301886	19.109043
47.232036	1340.107481	19.114061
46.805022	1336.601579	19.119079
46.845007	1333.360639	19.124096
46.581878	1333.385811	19.129114
47.231642	1343.234875	19.134131
47.200424	1352.659795	19.139149
47.156237	1344.846574	19.144167
47.142213	1350.235699	19.149184
47.252422	1346.548322	19.154202
47.770563	1344.776123	19.159219
47.613147	1348.183637	19.164237
47.704438	1344.928396	19.169255
47.863254	1344.272491	19.174272
47.661224	1347.349280	19.179290
47.899492	1331.211260	19.184307
47.934903	1342.891667	19.189325
47.662555	1339.762471	19.194343
47.772687	1345.634036	19.199360
47.828813	1368.037815	19.204378
48.252395	1363.657860	19.209395
48.387377	1365.785932	19.214413
48.311094	1367.019089	19.219431
48.787918	1352.128322	19.224448
48.420127	1343.453457	19.229466
48.203461	1330.699862	19.234483
48.255792	1327.564299	19.239501
47.798727	1341.618803	19.244519
48.154958	1345.192498	19.249536
48.490174	1360.231350	19.254554
48.550887	1367.477082	19.259571
48.641671	1359.892149	19.264589
48.262394	1352.815906	19.269607
48.384333	1354.737724	19.274624
48.530929	1357.577199	19.279642
48.444112	1364.274698	19.284659
48.710731	1355.775608	19.289677
48.723381	1359.541654	19.294695
48.912839	1369.635970	19.299712
48.970001	1382.057786	19.304730
49.173467	1371.618231	19.309747
49.713729	1378.836641	19.314765
48.642544	1361.532847	19.319783
49.243353	1361.581299	19.324800
49.201678	1373.109625	19.329818
49.172384	1365.862122	19.334835
49.406542	1377.612593	19.339853
49.257121	1381.697367	19.344871
49.474626	1385.074918	19.349888
49.643388	1379.705838	19.354906
49.541233	1386.298436	19.359923
49.480115	1388.195110	19.364941
49.450171	1389.086538	19.369959
49.546930	1380.026902	19.374976
49.469052	1392.570737	19.379994
49.513195	1385.718892	19.385011
49.584056	1388.270361	19.390029
49.160912	1385.136233	19.395047
49.326157	1375.472644	19.400064
49.098752	1389.538766	19.405082
49.728904	1397.377507	19.410099
49.916418	1404.950650	19.415117
50.014380	1398.614286	19.420135
50.350862	1399.158330	19.425152
50.403739	1385.526438	19.430170
50.564621	1383.522680	19.435187
50.837417	1381.056528	19.440205
50.966730	1385.119996	19.445223
51.056879	1373.252722	19.450240
50.932678	1364.300079	19.455258
50.737890	1357.160397	19.460275
50.682949	1352.043906	19.465293
50.277649	1356.821765	19.470311
50.829433	1348.909442	19.475328
50.711216	1340.173630	19.480346
50.949061	1338.997338	19.485363
50.944699	1343.870560	19.490381
50.547963	1346.693641	19.495399
51.086497	1344.337599	19.500416
50.934152	1350.420446	19.505434
50.858842	1347.995873	19.510451
50.780425	1346.868820	19.515469
50.668446	1348.956445	19.520487
50.734352	1358.640802	19.525504
50.901674	1368.337776	19.530522
51.035233	1369.254240	19.535539
51.070685	1367.601371	19.540557
51.058215	1378.430876	19.545575
51.490021	1368.306066	19.550592
51.179165	1390.243146	19.555610
51.257434	1371.567481	19.560627
51.565780	1372.387304	19.565645
51.302384	1386.825102	19.570663
51.688964	1388.279686	19.575680
51.735810	1399.320876	19.580698
51.604590	1394.361416	19.585715
51.729971	1396.885463	19.590733
51.783960	1396.634043	19.595751
51.933505	1400.634405	19.600768
51.673034	1396.395659	19.605786
51.779254	1399.197246	19.610803
51.821870	1387.918031	19.615821
51.651780	1407.261229	19.620839
51.668382	1398.848383	19.625856
51.734373	1400.883059	19.630874
52.124101	1409.081130	19.635891
52.294332	1420.232510	19.640909
52.360200	1422.084170	19.645927
52.854176	1402.195033	19.650944
53.038660	1407.070429	19.655962
52.715168	1388.223767	19.660979
52.878744	1378.699292	19.665997
52.510918	1376.916707	19.671015
52.571147	1370.169660	19.676032
52.442676	1373.604231	19.681050
52.412857	1376.382813	19.686067
52.696596	1386.235241	19.691085
52.615264	1392.004087	19.696103
52.826106	1387.982298	19.701120
52.822156	1403.787207	19.706138
52.549585	1396.173624	19.711155
53.317427	1394.343608	19.716173
52.975785	1397.476856	19.721191
53.195659	1404.461136	19.726208
53.065578	1400.000116	19.731226
53.051606	1406.992403	19.736243
53.065317	1396.882179	19.741261
52.945169	1405.472060	19.746279
53.375536	1408.065389	19.751296
53.527014	1418.462293	19.756314
53.019314	1423.041517	19.761331
53.311077	1422.617376	19.766349
53.539174	1419.782636	19.771367
53.812017	1422.359467	19.776384
54.333661	1414.044707	19.781402
53.923471	1422.600858	19.786419
53.917899	1415.573704	19.791437
53.837191	1421.803212	19.796455
53.864342	1415.591476	19.801472
53.605136	1421.858243	19.806490
53.950036	1424.389142	19.811507
54.001983	1413.045343	19.816525
53.927393	1422.003680	19.821543
54.377886	1427.525633	19.826560
54.310169	1435.776004	19.831578
54.345152	1436.985531	19.836595
54.582912	1446.248701	19.841613
54.497624	1446.249340	19.846631
54.311500	1436.949694	19.851648
54.851922	1436.824511	19.856666
54.564827	1438.800556	19.861683
54.638581	1440.701483	19.866701
54.360876	1443.351411	19.871719
54.487094	1439.074541	19.876736
54.847002	1447.289896	19.881754
54.684471	1445.096641	19.886771
55.079390	1445.918768	19.891789
54.772434	1441.662002	19.896807
54.942355	1438.687993	19.901824
54.929784	1440.955813	19.906842
54.709907	1449.144672	19.911859
54.748456	1452.840434	19.916877
54.712819	1456.352085	19.921895
54.927894	1465.243254	19.926912
55.323317	1458.005327	19.931930
55.290973	1464.549214	19.936947
55.243984	1455.710738	19.941965
55.192126	1451.906560	19.946983
55.488786	1460.078120	19.952000
56.029623	1472.809705	19.957018
55.484373	1465.692986	19.962035
55.833531	1465.698568	19.967053
55.584052	1468.536610	19.972071
55.956317	1475.983190	19.977088
55.926351	1471.143644	19.982106
55.638742	1474.574608	19.987123
56.084376	1470.585672	19.992141
56.183892	1478.248288	19.997159
56.135867	1483.879434	20.002176
56.256178	1481.373893	20.007194
56.124472	1487.425170	20.012211
56.343207	1475.960688	20.017229
56.089297	1479.108693	20.022247
56.346971	1480.182565	20.027264
56.458691	1480.111505	20.032282
56.120763	1480.293491	20.037299
56.148108	1478.610316	20.042317
56.553211	1477.026118	20.047335
56.171335	1477.038220	20.052352
56.377722	1484.712602	20.057370
56.616161	1503.736677	20.062387
56.706301	1501.936425	20.067405
56.967014	1511.896650	20.072423
56.986994	1503.997629	20.077440
57.071039	1497.287852	20.082458
56.787950	1502.147709	20.087475
57.271206	1501.154105	20.092493
56.836724	1499.713247	20.097511
56.899990	1500.788986	20.102528
57.115319	1498.489557	20.107546
56.857120	1505.725037	20.112563
57.110451	1516.128230	20.117581
57.424548	1524.915648	20.122599
57.447722	1526.231163	20.127616
57.740091	1521.189938	20.132634
57.492369	1519.868325	20.137651
57.575381	1516.721640	20.142669
57.454029	1527.498759	20.147687
57.373742	1527.113607	20.152704
57.504722	1522.296327	20.157722
57.648725	1531.618321	20.162739
57.782924	1534.043184	20.167757
57.870343	1541.534139	20.172775
57.777884	1544.117371	20.177792
58.167551	1543.700075	20.182810
57.992570	1541.606578	20.187827
58.215057	1536.535203	20.192845
58.340614	1543.420613	20.197863
58.214647	1539.700539	20.202880
58.356650	1529.084267	20.207898
58.559168	1543.645313	20.212915
58.034774	1529.857034	20.217933
58.505295	1544.720341	20.222951
58.736044	1556.045423	20.227968
58.623898	1554.396583	20.232986
58.551592	1564.124660	20.238003
58.741470	1557.796020	20.243021
58.748365	1558.325111	20.248039
58.895648	1553.394830	20.253056
58.951450	1558.710029	20.258074
58.772071	1554.723710	20.263091
58.875570	1560.621626	20.268109
59.030293	1558.981729	20.273127
59.164011	1577.545655	20.278144
59.448907	1579.760867	20.283162
59.186734	1586.602517	20.288179
59.380139	1577.922214	20.293197
59.113029	1579.248214	20.298215
59.428596	1578.047182	20.303232
59.530035	1578.021904	20.308250
59.569613	1575.172309	20.313267
59.701924	1581.589616	20.318285
59.628118	1584.485534	20.323303
59.528761	1574.143501	20.328320
59.647048	1569.277691	20.333338
59.245670	1583.913859	20.338355
59.796149	1594.696873	20.343373
59.439407	1601.928799	20.348391
59.722486	1595.165906	20.353408
59.687560	1595.758315	20.358426
59.781007	1608.509160	20.363443
59.970536	1610.789717	20.368461
60.761500	1616.003097	20.373479
60.631854	1615.363692	20.378496
60.891955	1605.183430	20.383514
60.580743	1601.722562	20.388531
60.661145	1590.973831	20.393549
60.355736	1586.382269	20.398567
60.507317	1606.631823	20.403584
60.924831	1604.184135	20.408602
61.011737	1616.980186	20.413619
61.012394	1614.594243	20.418637
61.198381	1616.692313	20.423655
60.603798	1619.716656	20.428672
60.771746	1617.920058	20.433690
60.911383	1616.954700	20.438707
60.948001	1615.964356	20.443725
61.044490	1615.580082	20.448743
60.957225	1611.191239	20.453760
61.196539	1606.246615	20.458778
61.206822	1626.079526	20.463795
61.554870	1633.457358	20.468813
61.386617	1637.138017	20.473831
61.173885	1640.642563	20.478848
61.504447	1634.683318	20.483866
61.277352	1634.633450	20.488883
61.388091	1634.392126	20.493901
61.365005	1647.429390	20.498919
61.629638	1659.181614	20.503936
62.451200	1651.735249	20.508954
62.284894	1648.529526	20.513971
62.425594	1648.431862	20.518989
62.586280	1646.841523	20.524007
62.612880	1651.567995	20.529024
62.338851	1629.740559	20.534042
62.337496	1635.225628	20.539059
61.844992	1628.390970	20.544077
62.242399	1642.864949	20.549095
62.763424	1645.665109	20.554112
62.685823	1639.690514	20.559130
62.566651	1648.239333	20.564147
62.492174	1642.642953	20.569165
62.720110	1644.639820	20.574183
62.656906	1644.072122	20.579200
62.845354	1642.534265	20.584218
62.288248	1646.906640	20.589235
62.551313	1653.461409	20.594253
62.971679	1662.847742	20.599271
63.128502	1674.967063	20.604288
63.126389	1669.144810	20.609306
63.251157	1675.474962	20.614323
63.457583	1671.116119	20.619341
63.429314	1665.446265	20.624359
63.552369	1669.220434	20.629376
63.796160	1663.236819	20.634394
63.211746	1663.220492	20.639411
63.197031	1666.356536	20.644429
63.304549	1660.801244	20.649447
63.129645	1676.285867	20.654464
63.368703	1684.684253	20.659482
63.335727	1689.284309	20.664499
63.688943	1686.761412	20.669517
63.703188	1689.690976	20.674535
63.264113	1691.422461	20.679552
63.959273	1701.015345	20.684570
64.372583	1705.280828	20.689587
64.340825	1707.444369	20.694605
64.613641	1712.246135	20.699623
64.528100	1706.758757	20.704640
64.629311	1701.848232	20.709658
64.749346	1705.250487	20.714675
64.729034	1709.318390	20.719693
65.224881	1702.635942	20.724711
64.817493	1702.547871	20.729728
64.498254	1698.883102	20.734746
64.896212	1700.294916	20.739763
64.752497	1706.625853	20.744781
65.223097	1705.760444	20.749799
64.927798	1701.243019	20.754816
64.967463	1708.056657	20.759834
64.937273	1702.380778	20.764851
64.793762	1699.752177	20.769869
65.118098	1696.637317	20.774887
64.952202	1699.020561	20.779904
65.299215	1706.770976	20.784922
65.203275	1722.508438	20.789939
65.353932	1727.726867	20.794957
65.324279	1723.755069	20.799975
65.373533	1735.973231	20.804992
65.666527	1722.224802	20.810010
65.489802	1730.874141	20.815027
65.619235	1727.663385	20.820045
65.731759	1737.324910	20.825063
65.720214	1751.648050	20.830080
66.312394	1750.889944	20.835098
66.190670	1751.287584	20.840115
66.107594	1750.700885	20.845133
66.091959	1746.909940	20.850151
65.905145	1744.953964	20.855168
66.269069	1745.392759	20.860186
66.569908	1755.930710	20.865203
66.156968	1748.985785	20.870221
66.325223	1761.548363	20.875239
66.751985	1769.062322	20.880256
66.865137	1773.406113	20.885274
67.162685	1773.000000	20.890291
67.148132	1771.960809	20.895309
67.091300	1765.913508	20.900327
66.787592	1769.870911	20.905344
66.980272	1768.856261	20.910362
67.148261	1765.920369	20.915379
67.207389	1767.369162	20.920397
67.402256	1773.309729	20.925415
67.037531	1768.904084	20.930432
67.119863	1772.470016	20.935450
67.364763	1766.842808	20.940467
67.492558	1767.125858	20.945485
67.480842	1756.994142	20.950503
67.523966	1767.578537	20.955520
67.587770	1765.233236	20.960538
67.637805	1773.111971	20.965555
67.892130	1784.976339	20.970573
68.088581	1789.461804	20.975591
67.963719	1794.849384	20.980608
68.062047	1793.571705	20.985626
67.836130	1795.853851	20.990643
68.185304	1792.454233	20.995661
68.370459	1786.397653	21.000679
67.932960	1794.787815	21.005696
67.634937	1791.432156	21.010714
67.998794	1795.648555	21.015731
68.011631	1795.409849	21.020749
68.463068	1803.601651	21.025767
68.760288	1814.544154	21.030784
68.611364	1815.681352	21.035802
68.571798	1818.496235	21.040819
68.830453	1821.488756	21.045837
68.743926	1809.418318	21.050855
68.481518	1823.973083	21.055872
68.230759	1832.116431	21.060890
68.873172	1833.730043	21.065907
69.031223	1850.674650	21.070925
69.375787	1843.031064	21.075943
69.355580	1837.268380	21.080960
69.452464	1837.597271	21.085978
69.544763	1834.913000	21.090995
69.312444	1839.307439	21.096013
69.430346	1835.650323	21.101031
69.778534	1835.510887	21.106048
69.558003	1831.934867	21.111066
69.703077	1844.905067	21.116083
69.560976	1842.443487	21.121101
69.934806	1841.040857	21.126119
69.716615	1851.596557	21.131136
69.936079	1855.377847	21.136154
69.987491	1848.960206	21.141171
70.318941	1859.424023	21.146189
70.295824	1862.902246	21.151207
70.043631	1854.029247	21.156224
70.116859	1856.138590	21.161242
70.136835	1858.082650	21.166259
70.420275	1878.633884	21.171277
70.894818	1874.400510	21.176295
70.676217	1884.489221	21.181312
70.705862	1883.342153	21.186330
70.752447	1879.737158	21.191347
71.068387	1879.328179	21.196365
71.031523	1872.889558	21.201383
70.862374	1881.124367	21.206400
70.935241	1879.894829	21.211418
71.190713	1872.160958	21.216435
71.277870	1876.126958	21.221453
71.084975	1877.343591	21.226471
71.316412	1895.233051	21.231488
71.310637	1898.869532	21.236506
71.765607	1893.171707	21.241523
71.908205	1901.051866	21.246541
71.531169	1894.527340	21.251559
72.015460	1908.855461	21.256576
71.805098	1899.685584	21.261594
71.695682	1894.697342	21.266611
71.772442	1897.655078	21.271629
71.783264	1893.964127	21.276647
71.784135	1896.065805	21.281664
72.026956	1908.077218	21.286682
72.269714	1913.802086	21.291699
72.120970	1924.836182	21.296717
72.190015	1916.714737	21.301735
72.237237	1918.891255	21.306752
72.240783	1921.630012	21.311770
72.146506	1913.726507	21.316787
72.388719	1924.175853	21.321805
73.124455	1930.496181	21.326823
73.199972	1937.222270	21.331840
72.812834	1936.790207	21.336858
72.792798	1935.174328	21.341875
72.884820	1939.458332	21.346893
73.012284	1942.976244	21.351911
73.085442	1941.595172	21.356928
72.718880	1934.428351	21.361946
73.222049	1936.230916	21.366963
73.483127	1947.431600	21.371981
73.040714	1942.324772	21.376999
72.842282	1943.280331	21.382016
73.027360	1953.634445	21.387034
73.532150	1948.563184	21.392051
73.618974	1964.528032	21.397069
73.569468	1958.788805	21.402087
73.898056	1957.033437	21.407104
73.802348	1964.603576	21.412122
74.252559	1970.999933	21.417139
74.271252	1978.716374	21.422157
74.342508	1982.848981	21.427175
74.352064	1982.759111	21.432192
74.293651	1990.130944	21.437210
74.639278	1985.725105	21.442227
74.384360	1980.579606	21.447245
74.367365	1981.005128	21.452263
74.755531	1978.312642	21.457280
74.397637	1988.861770	21.462298
74.766554	1979.349188	21.467315
74.473164	1986.587184	21.472333
74.686067	1984.477427	21.477351
74.518617	1990.376643	21.482368
74.784098	2006.670332	21.487386
75.189065	2006.720877	21.492403
74.842260	2018.177201	21.497421
74.937258	2013.305429	21.502439
75.593377	2006.152931	21.507456
75.442272	2011.853942	21.512474
75.370610	2016.008808	21.517491
75.377190	2025.507097	21.522509
75.627397	2023.823888	21.527527
75.313665	2029.203073	21.532544
75.273944	2034.675303	21.537562
75.927311	2030.890596	21.542579
75.851969	2031.931141	21.547597
75.454842	2036.928823	21.552615
76.020246	2048.097968	21.557632
75.690979	2048.846676	21.562650
76.018696	2050.764935	21.567667
76.037695	2048.890495	21.572685
76.221374	2052.002030	21.577703
76.157066	2053.204966	21.582720
76.724794	2064.648326	21.587738
76.993319	2062.675072	21.592755
77.191925	2065.433977	21.597773
76.849674	2068.415951	21.602791
76.968356	2065.989480	21.607808
76.763101	2074.384640	21.612826
76.973285	2065.531069	21.617843
77.109507	2070.991697	21.622861
77.151086	2065.645370	21.627879
77.453918	2066.459773	21.632896
77.191865	2074.721759	21.637914
77.160492	2065.422939	21.642931
76.932606	2071.836541	21.647949
77.348983	2084.348092	21.652967
77.873870	2076.729984	21.657984
77.542050	2083.005130	21.663002
77.919336	2080.708815	21.668019
77.804427	2073.445951	21.673037
78.016859	2086.393216	21.678055
78.115748	2080.583507	21.683072
78.066568	2076.112877	21.688090
78.285346	2071.026150	21.693107
78.296409	2078.396670	21.698125
77.967416	2079.871201	21.703143
78.314835	2069.329928	21.708160
78.518033	2072.100743	21.713178
78.144108	2077.287334	21.718195
78.696415	2088.799386	21.723213
78.993291	2085.925430	21.728231
79.428913	2086.037478	21.733248
78.920990	2090.070928	21.738266
78.853108	2092.647256	21.743283
79.051741	2088.087545	21.748301
79.165538	2093.296041	21.753319
79.609594	2082.099060	21.758336
79.307766	2090.165266	21.763354
79.604453	2075.699593	21.768371
79.450786	2076.686060	21.773389
79.470628	2074.625286	21.778407
79.963685	2078.730115	21.783424
79.880560	2075.022195	21.788442
80.021187	2077.663891	21.793459
79.954285	2071.652770	21.798477
79.636159	2084.524841	21.803495
79.534322	2076.982218	21.808512
79.485205	2078.798198	21.813530
80.150208	2073.575721	21.818547
79.917568	2076.663712	21.823565
79.697308	2090.265350	21.828583
80.011252	2092.378271	21.833600
79.853851	2112.376690	21.838618
80.286426	2116.235314	21.843635
80.628855	2128.294486	21.848653
80.884244	2126.951303	21.853671
81.014640	2125.043731	21.858688
80.805190	2127.070879	21.863706
81.187243	2127.652036	21.868723
81.265336	2126.882434	21.873741
81.333281	2120.752468	21.878759
81.535538	2120.708337	21.883776
81.361915	2125.475576	21.888794
81.050078	2125.549358	21.893811
81.369724	2122.037507	21.898829
81.120719	2119.797668	21.903847
81.207882	2125.685691	21.908864
81.293284	2126.117366	21.913882
81.304989	2138.619373	21.918899
81.456259	2141.568704	21.923917
81.516299	2150.822040	21.928935
81.341518	2148.927264	21.933952
81.767497	2163.419310	21.938970
81.805909	2171.675588	21.943987
81.911374	2161.484371	21.949005
82.323493	2168.852450	21.954023
82.241817	2167.160936	21.959040
82.492560	2156.729343	21.964058
82.631281	2163.612942	21.969075
83.063176	2170.981099	21.974093
82.936580	2168.914709	21.979111
82.991267	2154.243643	21.984128
83.008397	2153.972703	21.989146
83.109758	2152.842856	21.994163
82.754171	2152.333287	21.999181
82.768996	2166.933533	22.004199
83.343466	2170.063144	22.009216
83.055520	2175.794980	22.014234
83.154970	2174.854786	22.019251
83.427906	2174.124278	22.024269
83.368817	2181.774019	22.029287
82.871465	2173.409267	22.034304
83.407193	2192.239461	22.039322
83.897039	2196.587826	22.044339
84.214359	2199.874249	22.049357
83.900186	2200.121972	22.054375
83.965487	2190.732292	22.059392
84.019595	2199.879274	22.064410
84.057930	2203.161794	22.069427
84.128301	2196.245592	22.074445
84.179471	2197.373752	22.079463
84.113627	2190.526098	22.084480
83.994866	2192.242475	22.089498
84.184008	2215.655449	22.094515
84.386678	2218.852423	22.099533
84.422682	2223.804812	22.104551
84.326797	2215.469057	22.109568
84.736786	2235.660156	22.114586
84.668061	2240.774030	22.119603
84.788454	2236.002390	22.124621
84.782051	2250.088431	22.129639
84.976290	2251.976999	22.134656
85.182735	2264.088994	22.139674
85.178171	2265.090129	22.144691
85.702553	2263.869166	22.149709
85.544585	2265.323396	22.154727
85.654187	2263.535818	22.159744
85.879686	2262.339297	22.164762
85.692570	2268.431025	22.169779
85.852841	2265.142785	22.174797
85.705832	2283.375592	22.179815
86.102298	2288.073051	22.184832
86.293822	2291.975555	22.189850
85.968564	2301.771821	22.194867
86.319821	2287.644638	22.199885
86.341696	2301.186645	22.204903
86.303763	2293.245797	22.209920
87.040109	2299.739742	22.214938
86.560741	2302.847249	22.219955
86.781178	2313.486416	22.224973
86.890164	2317.849924	22.229991
86.788288	2324.272401	22.235008
87.015180	2315.589684	22.240026
87.070771	2321.132373	22.245043
87.232871	2311.623412	22.250061
87.132844	2321.618164	22.255079
87.387220	2314.193559	22.260096
87.406430	2331.141302	22.265114
87.587161	2341.881347	22.270131
88.015771	2331.683906	22.275149
87.288056	2343.190274	22.280167
87.596869	2337.420386	22.285184
87.730817	2342.527981	22.290202
87.506191	2346.886630	22.295219
88.043566	2348.554517	22.300237
88.276534	2358.292305	22.305255
88.487216	2352.316772	22.310272
88.453068	2356.901402	22.315290
88.461244	2351.449731	22.320307
88.449761	2354.957798	22.325325
88.621330	2353.236307	22.330343
88.550728	2352.268928	22.335360
88.722982	2349.177634	22.340378
88.669006	2352.155799	22.345395
89.051038	2359.225667	22.350413
89.048114	2371.483948	22.355431
88.930126	2371.647476	22.360448
89.466100	2366.078911	22.365466
88.918798	2380.189304	22.370483
89.249041	2375.391268	22.375501
89.185868	2382.653544	22.380519
89.342207	2369.276209	22.385536
89.752973	2371.045866	22.390554
89.520106	2385.467091	22.395571
89.970828	2392.412662	22.400589
89.942417	2400.916149	22.405607
89.832808	2396.934558	22.410624
89.993925	2388.968988	22.415642
90.015296	2398.600879	22.420659
89.858579	2391.988216	22.425677
89.865228	2409.900565	22.430695
90.126106	2415.348202	22.435712
90.772029	2418.428861	22.440730
90.459560	2424.868381	22.445747
90.663059	2415.731639	22.450765
90.987509	2413.973716	22.455783
90.748020	2420.471304	22.460800
90.800329	2407.138542	22.465818
90.662536	2431.943996	22.470835
90.790589	2435.805918	22.475853
91.103325	2441.655769	22.480871
91.198389	2438.806866	22.485888
91.530701	2432.657725	22.490906
91.439829	2450.847246	22.495923
91.774347	2459.742408	22.500941
91.693587	2457.495268	22.505959
91.670549	2454.396490	22.510976
92.195484	2462.368858	22.515994
92.027543	2460.883264	22.521011
92.223145	2456.639532	22.526029
92.384796	2457.658984	22.531047
92.174940	2466.885071	22.536064
92.235193	2456.694414	22.541082
92.392096	2464.642027	22.546099
92.682523	2475.137841	22.551117
92.752662	2483.228367	22.556135
92.838731	2479.557140	22.561152
92.811467	2479.349916	22.566170
92.576300	2484.682289	22.571187
92.996831	2486.390473	22.576205
93.059287	2485.689567	22.581223
92.734920	2481.280617	22.586240
93.358610	2491.431046	22.591258
93.315024	2500.779596	22.596275
93.215066	2508.492647	22.601293
93.572034	2499.218352	22.606311
93.684165	2505.209917	22.611328
93.622040	2503.531108	22.616346
93.505813	2509.574008	22.621363
94.050425	2520.106018	22.626381
93.923775	2526.898522	22.631399
93.812846	2531.750787	22.636416
93.855289	2525.324832	22.641434
94.169321	2523.675825	22.646451
94.288272	2529.925129	22.651469
94.420293	2542.531771	22.656487
94.782756	2544.933857	22.661504
95.176203	2550.149443	22.666522
94.987132	2549.228902	22.671539
95.011283	2544.538441	22.676557
95.200246	2545.455809	22.681575
95.213640	2540.044296	22.686592
95.253887	2536.301292	22.691610
94.887764	2543.989522	22.696627
95.257083	2542.303501	22.701645
95.274687	2539.375117	22.706663
95.040918	2532.496669	22.711680
95.734193	2539.253045	22.716698
95.869093	2553.800196	22.721715
95.901718	2557.175194	22.726733
95.853521	2556.504137	22.731751
95.729733	2558.637925	22.736768
96.008767	2557.720248	22.741786
96.027456	2552.408900	22.746803
95.939644	2548.654271	22.751821
96.147385	2547.081774	22.756839
96.078910	2564.302183	22.761856
96.440573	2568.951483	22.766874
96.473107	2576.145284	22.771891
96.578391	2572.957074	22.776909
96.604680	2576.819090	22.781927
96.654639	2589.782547	22.786944
97.074730	2587.899256	22.791962
97.089665	2597.364986	22.796979
97.123086	2601.929691	22.801997
97.338620	2600.592678	22.807015
97.113476	2604.680052	22.812032
97.508093	2608.636218	22.817050
97.278835	2619.882106	22.822067
97.909830	2633.411586	22.827085
97.827134	2615.788550	22.832103
97.893876	2625.760662	22.837120
98.017264	2629.983140	22.842138
97.649380	2624.078658	22.847155
98.172130	2637.309391	22.852173
98.421465	2644.485246	22.857191
98.265550	2652.503738	22.862208
98.338063	2634.256872	22.867226
98.608113	2641.909217	22.872243
98.826260	2645.185915	22.877261
98.740988	2645.754636	22.882279
98.796876	2644.937973	22.887296
98.642079	2660.126804	22.892314
99.111232	2671.731080	22.897331
98.845830	2666.107297	22.902349
99.005084	2670.008596	22.907367
98.986062	2678.971534	22.912384
99.064736	2683.040028	22.917402
99.056222	2689.375510	22.922419
99.638751	2695.514824	22.927437
99.768671	2691.590556	22.932455
99.748263	2703.113272	22.937472
100.169475	2715.678166	22.942490
100.248546	2715.533285	22.947507
99.977993	2724.270299	22.952525
100.528318	2713.151063	22.957543
100.591037	2715.135902	22.962560
101.158530	2710.092540	22.967578
100.936724	2713.696543	22.972595
100.638839	2708.036776	22.977613
100.750123	2707.605991	22.982631
100.665868	2715.761688	22.987648
100.907395	2709.055344	22.992666
100.773221	2710.575338	22.997683
101.119358	2723.846257	23.002701
101.418491	2722.515156	23.007719
101.314902	2734.274922	23.012736
101.395859	2730.998946	23.017754
101.839882	2734.723369	23.022771
101.437413	2734.902787	23.027789
101.486220	2726.228663	23.032807
101.599709	2745.548091	23.037824
101.681976	2753.337025	23.042842
101.967689	2752.336242	23.047859
102.275480	2754.857331	23.052877
102.835712	2746.387616	23.057895
102.614113	2739.096907	23.062912
102.898948	2748.192467	23.067930
102.914979	2741.783170	23.072947
102.981076	2745.351824	23.077965
102.984263	2736.410221	23.082983
102.834708	2740.252309	23.088000
103.108566	2735.169443	23.093018
103.189476	2733.487279	23.098035
102.889781	2741.490324	23.103053
102.919526	2733.952185	23.108071
103.324882	2754.510694	23.113088
103.341762	2750.465146	23.118106
103.574304	2759.171190	23.123123
103.281975	2759.923642	23.128141
103.805999	2757.809541	23.133159
103.458038	2767.199306	23.138176
103.635663	2775.415252	23.143194
103.958926	2781.421379	23.148211
103.974953	2787.421689	23.153229
104.416423	2779.800492	23.158247
104.322271	2800.692464	23.163264
104.860383	2802.477055	23.168282
104.911296	2802.633227	23.173299
104.625716	2812.975903	23.178317
105.010433	2804.050610	23.183335
104.886997	2799.054830	23.188352
104.786707	2799.079896	23.193370
105.051321	2806.076697	23.198387
105.083651	2813.680913	23.203405
105.242376	2817.793783	23.208423
105.717554	2829.141583	23.213440
105.462554	2827.710541	23.218458
105.500786	2826.076042	23.223475
105.551875	2824.385889	23.228493
105.725875	2826.599587	23.233511
105.702105	2845.486020	23.238528
106.147298	2845.179985	23.243546
106.418343	2847.870924	23.248563
106.210522	2839.527058	23.253581
107.250643	2835.580978	23.258599
106.950783	2841.336973	23.263616
106.504211	2842.466923	23.268634
106.837707	2844.693665	23.273651
106.710645	2839.035664	23.278669
106.750299	2854.443714	23.283687
106.792356	2856.277138	23.288704
106.816691	2866.615778	23.293722
107.058633	2867.433388	23.298739
106.889023	2868.618057	23.303757
107.538878	2879.771422	23.308775
107.405689	2887.010086	23.313792
107.620944	2890.315684	23.318810
107.866243	2882.712362	23.323827
107.775943	2890.124246	23.328845
107.907414	2897.861398	23.333863
107.883680	2906.840964	23.338880
108.325939	2913.055846	23.343898
108.519755	2910.065250	23.348915
108.385121	2912.708897	23.353933
108.630006	2914.274043	23.358951
108.395608	2907.124125	23.363968
108.489617	2916.236856	23.368986
108.799280	2917.814009	23.374003
108.815269	2926.885239	23.379021
109.147448	2936.671018	23.384039
109.309057	2933.313015	23.389056
109.339790	2928.290040	23.394074
109.238642	2930.455064	23.399091
109.017001	2943.331663	23.404109
109.587441	2947.197409	23.409127
109.932135	2955.475797	23.414144
109.666646	2962.612001	23.419162
109.818213	2956.033191	23.424179
109.606965	2958.811860	23.429197
110.058422	2957.542242	23.434215
110.204187	2974.540323	23.439232
110.152633	2984.423745	23.444250
110.477312	2984.625665	23.449267
110.098357	2975.800249	23.454285
110.617117	2981.684479	23.459303
110.954564	2992.914959	23.464320
110.728121	2996.361936	23.469338
110.760108	3004.868929	23.474355
111.051807	3008.386731	23.479373
111.428876	3001.097390	23.484391
111.045775	3006.759090	23.489408
111.429077	3017.581622	23.494426
111.669867	3013.658959	23.499443
111.275067	3030.318337	23.504461
111.250698	3015.763026	23.509479
111.756213	3029.757353	23.514496
112.088297	3047.869004	23.519514
112.319290	3043.231424	23.524531
112.440732	3051.576175	23.529549
112.524810	3047.842021	23.534567
112.478767	3046.700351	23.539584
112.227616	3046.534289	23.544602
112.503755	3049.959838	23.549619
112.452821	3064.586833	23.554637
113.051414	3063.483666	23.559655
113.193649	3067.876899	23.564672
113.155571	3071.547052	23.569690
113.178671	3063.189222	23.574707
112.936886	3078.070025	23.579725
113.446652	3091.053784	23.584743
113.717972	3075.896912	23.589760
113.651541	3080.038585	23.594778
113.897818	3078.191774	23.599795
114.066584	3082.123243	23.604813
114.595072	3094.659078	23.609831
114.533128	3087.046696	23.614848
114.064199	3091.588741	23.619866
114.666141	3100.474147	23.624883
114.743427	3107.118342	23.629901
114.789713	3102.635749	23.634919
114.781100	3101.257851	23.639936
114.492738	3098.746278	23.644954
114.573625	3108.236727	23.649971
114.781551	3113.175219	23.654989
115.102841	3136.209024	23.660007
115.152757	3126.177403	23.665024
114.915113	3138.759958	23.670042
115.488419	3140.135122	23.675059
115.676503	3151.619353	23.680077
115.889018	3158.072082	23.685095
116.272611	3159.779772	23.690112
115.927141	3157.299175	23.695130
116.288027	3145.404356	23.700147
116.374617	3143.705489	23.705165
116.206485	3147.477965	23.710183
116.793520	3148.986706	23.715200
116.615504	3157.343412	23.720218
117.256377	3151.676216	23.725235
117.163589	3155.929318	23.730253
117.127197	3146.387697	23.735271
117.439945	3149.094282	23.740288
116.880674	3149.137153	23.745306
117.410490	3150.266600	23.750323
117.618411	3150.732879	23.755341
117.962743	3155.274567	23.760359
117.878947	3143.893996	23.765376
117.698660	3154.012170	23.770394
117.979751	3144.556834	23.775411
118.104561	3145.531563	23.780429
118.353419	3142.169406	23.785447
118.144535	3141.270855	23.790464
118.132970	3152.852449	23.795482
118.114660	3161.029642	23.800499
118.141122	3166.690749	23.805517
118.039022	3180.372654	23.810535
118.386643	3185.608186	23.815552
118.557872	3195.311857	23.820570
118.907854	3195.613993	23.825587
118.686160	3203.014902	23.830605
118.889969	3211.706703	23.835623
119.151605	3215.933044	23.840640
119.425496	3219.169607	23.845658
119.405595	3221.549258	23.850675
119.536250	3230.722722	23.855693
119.324534	3245.321242	23.860711
119.547885	3244.011371	23.865728
119.639423	3257.435946	23.870746
119.811991	3265.962206	23.875763
120.312515	3267.102532	23.880781
120.359946	3274.445789	23.885799
120.663118	3260.606227	23.890816
120.832955	3279.942706	23.895834
120.759291	3290.846018	23.900851
121.110867	3296.948907	23.905869
121.324624	3302.429401	23.910887
121.320146	3293.848515	23.915904
121.449879	3299.736608	23.920922
121.605637	3296.767655	23.925939
121.623296	3296.941633	23.930957
121.541773	3297.478229	23.935975
121.636020	3302.279821	23.940992
121.669677	3318.140531	23.946010
122.247754	3319.423439	23.951027
122.103051	3322.299112	23.956045
121.914803	3316.899823	23.961063
122.203306	3329.836144	23.966080
122.394608	3346.016355	23.971098
122.458842	3350.118810	23.976115
122.570012	3356.783071	23.981133
122.216532	3361.319833	23.986151
122.937275	3369.577739	23.991168
122.763142	3378.710358	23.996186
123.039600	3377.679421	24.001203
123.386255	3385.935609	24.006221
123.216556	3395.607251	24.011239
123.538130	3385.814089	24.016256
123.375284	3396.961749	24.021274
123.579494	3414.484538	24.026291
123.538359	3420.629674	24.031309
123.989374	3426.082736	24.036327
124.045062	3416.700225	24.041344
124.430015	3433.680438	24.046362
124.409773	3434.390555	24.051379
124.702752	3442.446819	24.056397
124.838790	3444.281452	24.061415
124.851258	3442.650909	24.066432
124.953803	3449.676350	24.071450
124.892126	3449.862682	24.076467
125.076784	3448.972280	24.081485
125.099440	3462.672850	24.086503
125.326577	3463.641135	24.091520
125.119710	3475.799361	24.096538
125.393619	3467.257111	24.101555
125.504395	3478.134976	24.106573
125.627967	3488.439586	24.111591
125.769059	3475.464639	24.116608
125.784016	3498.578163	24.121626
126.165947	3508.138732	24.126643
126.284629	3517.746604	24.131661
126.379405	3516.576667	24.136679
126.886810	3512.116865	24.141696
126.591919	3519.848074	24.146714
126.730066	3524.952197	24.151731
127.073698	3529.430966	24.156749
126.953690	3527.600107	24.161767
127.325689	3530.515303	24.166784
127.473028	3544.606828	24.171802
127.518886	3559.162343	24.176819
127.951115	3548.963653	24.181837
128.398582	3551.055961	24.186855
128.462484	3540.857809	24.191872
127.992974	3542.430082	24.196890
128.331136	3540.319580	24.201907
128.501576	3526.601478	24.206925
128.390199	3540.651219	24.211943
128.828284	3546.327264	24.216960
128.983309	3555.102575	24.221978
128.644138	3564.141048	24.226995
128.993859	3566.927158	24.232013
129.238287	3569.672850	24.237031
128.968173	3559.274196	24.242048
129.196488	3576.711329	24.247066
129.237655	3588.247119	24.252083
129.239009	3586.820289	24.257101
129.522197	3595.013863	24.262119
129.698012	3600.913818	24.267136
129.995089	3615.117802	24.272154
130.384243	3611.746340	24.277171
130.600101	3613.044634	24.282189
130.468610	3613.860452	24.287207
130.668609	3614.801408	24.292224
130.998366	3628.441667	24.297242
130.689605	3634.174049	24.302259
130.862452	3627.193999	24.307277
130.731241	3637.500488	24.312295
131.637531	3629.910721	24.317312
131.385519	3630.988332	24.322330
131.718453	3642.765946	24.327347
132.276201	3646.706415	24.332365
131.693069	3652.472052	24.337383
132.253529	3634.735258	24.342400
132.378393	3639.472206	24.347418
132.285334	3635.058518	24.352435
132.326946	3641.001474	24.357453
132.348809	3643.674518	24.362471
132.630210	3638.773285	24.367488
132.900786	3643.332893	24.372506
132.976734	3645.827082	24.377523
132.729558	3655.403614	24.382541
132.910209	3659.547982	24.387559
132.950656	3653.923613	24.392576
133.085414	3667.739447	24.397594
132.948553	3678.438209	24.402611
133.332419	3682.446789	24.407629
133.541562	3685.207461	24.412647
133.389683	3694.077966	24.417664
133.321169	3703.440490	24.422682
133.572650	3716.041982	24.427699
133.906923	3711.463901	24.432717
134.105928	3719.961011	24.437735
134.169166	3733.974247	24.442752
134.439329	3745.780639	24.447770
134.409395	3739.356050	24.452787
135.437782	3738.656209	24.457805
135.534704	3744.536931	24.462823
136.090698	3732.762850	24.467840
136.163004	3728.642172	24.472858
136.104605	3727.609694	24.477875
136.017817	3712.574322	24.482893
135.880084	3715.603628	24.487911
136.041831	3710.945096	24.492928
136.320363	3715.427735	24.497946
136.268686	3716.988625	24.502963
136.529365	3709.063783	24.507981
136.620862	3716.813824	24.512999
136.404716	3725.053637	24.518016
136.484166	3740.645623	24.523034
136.338842	3744.742919	24.528051
136.558382	3743.821822	24.533069
136.749707	3757.420608	24.538087
136.832745	3761.987350	24.543104
136.666481	3771.396692	24.548122
137.052025	3775.272469	24.553139
137.465875	3781.772983	24.558157
137.512268	3792.484313	24.563175
137.473374	3800.983781	24.568192
137.910430	3805.552230	24.573210
137.960588	3811.727473	24.578227
138.333699	3811.391617	24.583245
138.938359	3831.677300	24.588263
139.212750	3831.618782	24.593280
139.312297	3832.682701	24.598298
139.137126	3832.956144	24.603315
139.520304	3827.246798	24.608333
139.292939	3832.256416	24.613351
139.166180	3814.828439	24.618368
139.451980	3823.817083	24.623386
139.499404	3837.599301	24.628403
139.483649	3825.481769	24.633421
139.947329	3835.620002	24.638439
139.767663	3837.825765	24.643456
140.287573	3843.498634	24.648474
140.029643	3848.904390	24.653491
140.373057	3836.544713	24.658509
140.035546	3859.546296	24.663527
140.112948	3873.462749	24.668544
140.757769	3878.020964	24.673562
140.913213	3889.182498	24.678579
141.345256	3888.824841	24.683597
141.434549	3887.516859	24.688615
141.742614	3884.486222	24.693632
141.915349	3883.095812	24.698650
141.551978	3885.958275	24.703667
141.755842	3879.620330	24.708685
141.908285	3902.132217	24.713703
141.825176	3907.747491	24.718720
142.265226	3905.920929	24.723738
142.222258	3913.158582	24.728755
142.470576	3905.377611	24.733773
142.475982	3920.653030	24.738791
142.515311	3927.959939	24.743808
142.740728	3934.332032	24.748826
142.555031	3937.261530	24.753843
142.742563	3952.041493	24.758861
143.269786	3954.866311	24.763879
143.459481	3952.277031	24.768896
143.328503	3956.968676	24.773914
143.453734	3962.696718	24.778931
143.559704	3977.435745	24.783949
143.982166	3988.337986	24.788967
143.966249	3989.801799	24.793984
144.137078	3991.157632	24.799002
144.425291	4011.802100	24.804019
144.532185	4009.939022	24.809037
144.150190	4014.966451	24.814055
144.426051	4016.047119	24.819072
144.904489	4026.419883	24.824090
144.768510	4040.041433	24.829107
144.938579	4045.484768	24.834125
145.289696	4057.300855	24.839143
145.285016	4062.809277	24.844160
145.734277	4062.679346	24.849178
145.573029	4083.640063	24.854195
145.983818	4075.555971	24.859213
146.163735	4074.991374	24.864231
146.129731	4088.464520	24.869248
146.468595	4099.982695	24.874266
146.715021	4106.263202	24.879283
146.911577	4104.929036	24.884301
146.978530	4110.880826	24.889319
146.613628	4116.786228	24.894336
147.262562	4119.790969	24.899354
147.099125	4134.647819	24.904371
147.091564	4142.710157	24.909389
147.494868	4148.959942	24.914407
147.713405	4158.199104	24.919424
147.842847	4151.875807	24.924442
148.058510	4155.314141	24.929459
148.479799	4171.149970	24.934477
148.858499	4174.648144	24.939495
148.828875	4170.805209	24.944512
149.039890	4162.370268	24.949530
148.997365	4163.371106	24.954547
148.998868	4178.113936	24.959565
149.218456	4175.415813	24.964583
149.520389	4181.252135	24.969600
149.561950	4177.682182	24.974618
149.808515	4187.115842	24.979635
150.038508	4189.699750	24.984653
149.930692	4190.401437	24.989671
149.952255	4188.333840	24.994688
150.061248	4194.894592	24.999706
149.859824	4204.028721	25.004723
150.324198	4207.911258	25.009741
150.715770	4213.900919	25.014759
150.351603	4230.297814	25.019776
150.982144	4229.268517	25.024794
150.954557	4239.101550	25.029811
151.051630	4252.608068	25.034829
151.597532	4255.761439	25.039847
151.399896	4254.321349	25.044864
151.594161	4255.439986	25.049882
151.759057	4276.801503	25.054899
151.954900	4279.898908	25.059917
151.995127	4287.338388	25.064935
152.012870	4287.992123	25.069952
152.506731	4291.721741	25.074970
152.799222	4302.767504	25.079987
152.635770	4308.878328	25.085005
153.075261	4303.942835	25.090023
152.868620	4309.602716	25.095040
153.023849	4292.985739	25.100058
152.957793	4317.309172	25.105075
152.842078	4318.195160	25.110093
153.472669	4321.357452	25.115111
153.382988	4343.314196	25.120128
154.168590	4353.402602	25.125146
153.715936	4351.077402	25.130163
153.670839	4357.005686	25.135181
154.203290	4371.034743	25.140199
154.154214	4385.350042	25.145216
154.386161	4382.328018	25.150234
154.485752	4413.901150	25.155251
154.437752	4412.803886	25.160269
154.942738	4426.805699	25.165287
155.315147	4444.407462	25.170304
155.348155	4429.930455	25.175322
155.494498	4442.851833	25.180339
155.559246	4461.132782	25.185357
156.023957	4459.879939	25.190375
156.210755	4462.467454	25.195392
156.387961	4455.584254	25.200410
156.075075	4467.775434	25.205427
156.393129	4483.523450	25.210445
156.828783	4486.280545	25.215463
156.810043	4485.260786	25.220480
156.988556	4500.998979	25.225498
157.084850	4503.240767	25.230515
157.182268	4511.574153	25.235533
157.624928	4508.235230	25.240551
157.873543	4516.153690	25.245568
158.399826	4522.441274	25.250586
158.225388	4525.703687	25.255603
158.499279	4520.500376	25.260621
158.828768	4536.698018	25.265639
158.666911	4529.128989	25.270656
158.720932	4522.242848	25.275674
158.735253	4527.603261	25.280691
158.274234	4539.634483	25.285709
159.155914	4541.533053	25.290727
158.787273	4550.592386	25.295744
159.464160	4565.142002	25.300762
159.303373	4565.056545	25.305779
159.431155	4572.760272	25.310797
159.403018	4578.345100	25.315815
159.473738	4591.956978	25.320832
159.824224	4602.523596	25.325850
160.461033	4606.770764	25.330867
160.722108	4606.887920	25.335885
161.076678	4607.151494	25.340903
161.359021	4622.049813	25.345920
161.730073	4628.276379	25.350938
161.740833	4633.489029	25.355955
161.718670	4631.829049	25.360973
161.682054	4623.145218	25.365991
161.661984	4633.554912	25.371008
161.865970	4632.790857	25.376026
161.741168	4634.729350	25.381043
161.898458	4649.293646	25.386061
162.179546	4648.312421	25.391079
162.167822	4665.128294	25.396096
162.520086	4669.795389	25.401114
162.722400	4676.225000	25.406131
162.385766	4680.500642	25.411149
162.848469	4690.352279	25.416167
162.776710	4707.041813	25.421184
163.369188	4706.081545	25.426202
163.048089	4718.207887	25.431219
163.178771	4736.586166	25.436237
163.553521	4730.505396	25.441255
163.742760	4751.323939	25.446272
163.844195	4747.567794	25.451290
164.562683	4751.884347	25.456307
164.341142	4765.503981	25.461325
165.181871	4776.003844	25.466343
164.939470	4794.983169	25.471360
164.921749	4783.155693	25.476378
165.212171	4778.060209	25.481395
164.969415	4787.911257	25.486413
165.396725	4796.486960	25.491431
165.078326	4811.548406	25.496448
165.410887	4813.071662	25.501466
165.564640	4835.786518	25.506483
166.015387	4836.843165	25.511501
166.149969	4849.564654	25.516519
166.308636	4859.672042	25.521536
166.633450	4864.930555	25.526554
166.686937	4865.960673	25.531571
166.885818	4891.244213	25.536589
166.646583	4890.413425	25.541607
166.993129	4901.615273	25.546624
167.184019	4913.579967	25.551642
167.779453	4910.157214	25.556659
167.772321	4932.117600	25.561677
168.245908	4938.836496	25.566695
168.139838	4946.078073	25.571712
168.345140	4940.342415	25.576730
168.290795	4941.663936	25.581747
168.334046	4963.594421	25.586765
168.914395	4965.966072	25.591783
168.998988	4972.799203	25.596800
169.041128	4976.207894	25.601818
169.558922	4976.862713	25.606835
169.503665	4976.798701	25.611853
170.072989	4984.758973	25.616871
170.133953	4992.653198	25.621888
170.195730	5000.417885	25.626906
170.258859	4988.584000	25.631923
170.256465	5002.993525	25.636941
170.864378	5016.124374	25.641959
170.800410	5022.999591	25.646976
170.874804	5027.561687	25.651994
171.006821	5018.472639	25.657011
171.359331	5034.657673	25.662029
171.632661	5047.509209	25.667047
171.456928	5037.940937	25.672064
171.602638	5044.669886	25.677082
171.879824	5060.718317	25.682100
171.921025	5070.282262	25.687117
172.284017	5074.919384	25.692135
172.596419	5079.141417	25.697152
173.056521	5077.778776	25.702170
173.625440	5080.152222	25.707188
173.173604	5080.803340	25.712205
173.594810	5076.173507	25.717223
173.570624	5083.904267	25.722240
173.985537	5085.657773	25.727258
174.017234	5079.368311	25.732276
174.055548	5095.349800	25.737293
174.145457	5092.198263	25.742311
174.108931	5115.839529	25.747328
174.448694	5104.701112	25.752346
174.606211	5096.804354	25.757364
174.494606	5123.664284	25.762381
174.843046	5126.614976	25.767399
175.048576	5135.623084	25.772416
174.957324	5137.818394	25.777434
175.209881	5148.381639	25.782452
175.301936	5157.622065	25.787469
175.392803	5163.248518	25.792487
175.215313	5177.505522	25.797504
175.098027	5192.627509	25.802522
175.296252	5196.141356	25.807540
175.441801	5223.731579	25.812557
175.929080	5236.471027	25.817575
176.342456	5244.944949	25.822592
176.413949	5262.158763	25.827610
176.775674	5262.714788	25.832628
176.462127	5284.076224	25.837645
176.901872	5286.229916	25.842663
177.139416	5309.071205	25.847680
177.332452	5312.699516	25.852698
177.827936	5331.712876	25.857716
177.911410	5344.215400	25.862733
178.094194	5347.602264	25.867751
178.246126	5358.582174	25.872768
178.476766	5367.214020	25.877786
179.166560	5361.226035	25.882804
179.339786	5377.956956	25.887821
179.441441	5383.401877	25.892839
179.356868	5394.052474	25.897856
179.506485	5398.113693	25.902874
179.756605	5408.213461	25.907892
179.845159	5416.974773	25.912909
180.448518	5417.887749	25.917927
180.290604	5423.568798	25.922944
180.610089	5443.383023	25.927962
180.931300	5445.201658	25.932980
180.933884	5443.667169	25.937997
180.927905	5445.356823	25.943015
181.612970	5457.399607	25.948032
181.622307	5466.956095	25.953050
182.056390	5457.570434	25.958068
181.983874	5459.077900	25.963085
182.234514	5459.802740	25.968103
182.446323	5470.173656	25.973120
182.508697	5483.598110	25.978138
182.593654	5482.871491	25.983156
182.672179	5485.599116	25.988173
183.012461	5491.420423	25.993191
183.197120	5504.971055	25.998208
183.065797	5507.731354	26.003226
183.112149	5514.914705	26.008244
183.344516	5522.886641	26.013261
183.416935	5533.118310	26.018279
183.901987	5545.435347	26.023296
184.021721	5560.287153	26.028314
183.917502	5558.248453	26.033332
184.531504	5574.689974	26.038349
184.514954	5585.541581	26.043367
184.938196	5586.299529	26.048384
185.169454	5606.547488	26.053402
185.053434	5616.559175	26.058420
185.186637	5616.238548	26.063437
185.598555	5632.162342	26.068455
185.899058	5637.768931	26.073472
186.033544	5645.790882	26.078490
185.991232	5649.560069	26.083508
186.260049	5662.924106	26.088525
186.282598	5665.950876	26.093543
186.694902	5669.128456	26.098560
186.653627	5686.650631	26.103578
187.036361	5690.789258	26.108596
186.967031	5685.919986	26.113613
187.092318	5713.413096	26.118631
187.709606	5714.746900	26.123648
187.692830	5723.483723	26.128666
188.054049	5725.738079	26.133684
188.316634	5745.583588	26.138701
188.369646	5744.154859	26.143719
188.541467	5757.297324	26.148736
188.600537	5759.153647	26.153754
188.591822	5772.302133	26.158772
188.924469	5780.795188	26.163789
189.021681	5791.285139	26.168807
189.120015	5794.612634	26.173824
188.732817	5805.806170	26.178842
189.175046	5822.940698	26.183860
190.028115	5837.003049	26.188877
189.607887	5840.455478	26.193895
190.594993	5854.039268	26.198912
190.317124	5869.455127	26.203930
190.655198	5867.742107	26.208948
190.809192	5877.184747	26.213965
191.175804	5880.000156	26.218983
191.576975	5886.001507	26.224000
191.814485	5916.220535	26.229018
192.390293	5899.369313	26.234036
193.143148	5880.943809	26.239053
193.556308	5874.525237	26.244071
194.064132	5877.287096	26.249088
193.888640	5866.765056	26.254106
194.029885	5855.720221	26.259124
193.910796	5853.677490	26.264141
193.763548	5846.774834	26.269159
194.282815	5840.554403	26.274176
194.034282	5846.271787	26.279194
193.994402	5843.888439	26.284212
194.272427	5844.422793	26.289229
193.953634	5862.316630	26.294247
194.262562	5873.774307	26.299264
194.221671	5878.973259	26.304282
194.309815	5894.344781	26.309300
194.993486	5906.492251	26.314317
194.963491	5922.201007	26.319335
195.189803	5922.203635	26.324352
195.349369	5935.269221	26.329370
195.248009	5944.612761	26.334388
195.478712	5958.295454	26.339405
195.530573	5977.997254	26.344423
196.093818	5980.946210	26.349440
196.125068	6003.151285	26.354458
196.177010	6011.994343	26.359476
196.506466	6027.966046	26.364493
196.456757	6045.881300	26.369511
196.771585	6048.755305	26.374528
196.893928	6069.314302	26.379546
197.552484	6078.233407	26.384564
198.049048	6101.183726	26.389581
197.887409	6102.522035	26.394599
198.342932	6111.507489	26.399616
198.406112	6133.600426	26.404634
198.418031	6140.991410	26.409652
198.790215	6146.596466	26.414669
198.989589	6158.131355	26.419687
199.221196	6152.902598	26.424704
199.253779	6165.811347	26.429722
199.448911	6178.129758	26.434740
199.671569	6174.114541	26.439757
199.710201	6195.248597	26.444775
200.011719	6197.158762	26.449792
200.270771	6202.926655	26.454810
200.530566	6217.479406	26.459828
200.766313	6227.291455	26.464845
200.709111	6230.242349	26.469863
201.031858	6241.679167	26.474880
201.274367	6262.781559	26.479898
201.529026	6257.874320	26.484916
201.775464	6259.354291	26.489933
201.523288	6278.756517	26.494951
201.807562	6277.938859	26.499968
201.873962	6299.797902	26.504986
202.086277	6294.013378	26.510004
202.616879	6319.502947	26.515021
202.922034	6328.909661	26.520039
203.049118	6343.631538	26.525056
203.077420	6347.992801	26.530074
203.280095	6356.784148	26.535092
203.807381	6369.874869	26.540109
203.565997	6378.596468	26.545127
203.609917	6400.493855	26.550144
204.045257	6410.940990	26.555162
204.333136	6426.237670	26.560180
205.038841	6421.986204	26.565197
205.625267	6407.724507	26.570215
206.263628	6406.608651	26.575232
206.189819	6410.897439	26.580250
206.293070	6411.039181	26.585268
206.732877	6422.833534	26.590285
206.449774	6442.894184	26.595303
206.754252	6436.981626	26.600320
206.653847	6433.278656	26.605338
207.035532	6436.388536	26.610356
206.886216	6442.371604	26.615373
206.889589	6462.362421	26.620391
207.147827	6456.943187	26.625408
207.366534	6490.370142	26.630426
207.474261	6487.124046	26.635444
208.011851	6504.231743	26.640461
208.125071	6524.442279	26.645479
208.427690	6519.256027	26.650496
208.259314	6532.553029	26.655514
208.783351	6537.408522	26.660532
208.830197	6545.757028	26.665549
208.565825	6567.282769	26.670567
209.350917	6564.947665	26.675584
209.413734	6586.918095	26.680602
209.360837	6594.732883	26.685620
209.559892	6606.927860	26.690637
209.865534	6629.072035	26.695655
210.594241	6621.215118	26.700672
210.734721	6637.182053	26.705690
210.734490	6647.697137	26.710708
211.178951	6661.754296	26.715725
211.244818	6674.632968	26.720743
211.624642	6666.508362	26.725760
212.011365	6688.441112	26.730778
212.350029	6689.048127	26.735796
212.090730	6695.070498	26.740813
212.218898	6712.560963	26.745831
212.249885	6714.762684	26.750848
212.176551	6727.293726	26.755866
212.424271	6742.925226	26.760884
212.713510	6756.170086	26.765901
212.626029	6777.100319	26.770919
213.167297	6793.727888	26.775936
213.275715	6807.291358	26.780954
213.669482	6828.620239	26.785972
213.973223	6831.477154	26.790989
214.257599	6851.030051	26.796007
214.389593	6861.512045	26.801024
214.698269	6864.769107	26.806042
215.169564	6884.438150	26.811060
215.041416	6888.934386	26.816077
215.012382	6892.660723	26.821095
215.670998	6911.000041	26.826112
215.679213	6921.308777	26.831130
215.900348	6934.924242	26.836148
216.012341	6935.351895	26.841165
216.364173	6954.562939	26.846183
216.564636	6967.165163	26.851200
216.574097	6979.045816	26.856218
216.708352	6989.502277	26.861236
217.700116	6995.339441	26.866253
217.417438	7011.738770	26.871271
217.575583	7013.778675	26.876288
218.268926	7033.495385	26.881306
218.229838	7047.915392	26.886324
218.381265	7047.563493	26.891341
218.759309	7069.981042	26.896359
219.154591	7077.394795	26.901376
218.998944	7076.554046	26.906394
219.286488	7087.005639	26.911412
219.701525	7087.641817	26.916429
220.147235	7099.246281	26.921447
220.295667	7102.531490	26.926464
220.917577	7105.963961	26.931482
220.859632	7119.162119	26.936500
221.263364	7110.752639	26.941517
221.349945	7125.853954	26.946535
221.559579	7127.185043	26.951552
221.940155	7127.223637	26.956570
221.887915	7138.637321	26.961588
221.965903	7153.168613	26.966605
222.023012	7166.882395	26.971623
222.394085	7167.531734	26.976640
222.117999	7182.070822	26.981658
222.604536	7198.678870	26.986676
222.884541	7207.531195	26.991693
223.103631	7211.563061	26.996711
223.242680	7228.057924	27.001728
223.752583	7244.362477	27.006746
223.683112	7256.220873	27.011764
223.880188	7258.071648	27.016781
223.918094	7271.254991	27.021799
224.386520	7294.997244	27.026816
224.611072	7302.014652	27.031834
224.704682	7325.739534	27.036852
225.177524	7328.885886	27.041869
225.275191	7348.133756	27.046887
225.545996	7362.130099	27.051904
225.529961	7361.892658	27.056922
225.700638	7381.242842	27.061940
226.127573	7382.716903	27.066957
226.550897	7402.965364	27.071975
226.424191	7407.344698	27.076992
227.059978	7423.711890	27.082010
226.966325	7438.791014	27.087028
227.172508	7449.176558	27.092045
227.550611	7462.313388	27.097063
227.585394	7471.690177	27.102080
228.293626	7478.818606	27.107098
228.846831	7496.265744	27.112116
229.013093	7500.492155	27.117133
229.087630	7505.455772	27.122151
229.133392	7506.569323	27.127168
229.540474	7503.904661	27.132186
229.414982	7524.892173	27.137204
229.901226	7522.653991	27.142221
230.202218	7529.135544	27.147239
230.283030	7539.736386	27.152256
230.957491	7541.042491	27.157274
230.955401	7539.227591	27.162292
231.598099	7537.312307	27.167309
231.637573	7544.368094	27.172327
231.375651	7542.107486	27.177344
232.429702	7547.616289	27.182362
232.036026	7561.962472	27.187380
232.309551	7562.194520	27.192397
232.390091	7565.212576	27.197415
232.337638	7575.120729	27.202432
232.426577	7596.213842	27.207450
232.652669	7619.211333	27.212468
232.678925	7615.049596	27.217485
233.130934	7637.652052	27.222503
233.403598	7655.442924	27.227520
233.955244	7662.772590	27.232538
233.829033	7676.849925	27.237556
233.856021	7679.140778	27.242573
234.222219	7694.290578	27.247591
234.749901	7698.205057	27.252608
235.714578	7704.703308	27.257626
236.040852	7709.848773	27.262644
235.958240	7718.884076	27.267661
236.008694	7724.950109	27.272679
236.356724	7739.645023	27.277696
236.602528	7741.630322	27.282714
236.452765	7743.541458	27.287732
236.685773	7760.419943	27.292749
236.708268	7761.641309	27.297767
236.821798	7779.984283	27.302784
236.976621	7800.041372	27.307802
237.246854	7808.156788	27.312820
237.578274	7828.262180	27.317837
238.029919	7833.858544	27.322855
238.240158	7861.830978	27.327872
238.661022	7867.372163	27.332890
238.605332	7880.542103	27.337908
238.795026	7902.964738	27.342925
239.555021	7907.853317	27.347943
239.690027	7919.194137	27.352960
240.061874	7927.776799	27.357978
240.220003	7935.237294	27.362996
240.435235	7951.304227	27.368013
240.563152	7962.488329	27.373031
240.380751	7979.175974	27.378048
240.752841	7989.201358	27.383066
241.054646	7999.439734	27.388084
241.158017	8013.074334	27.393101
241.527210	8024.618688	27.398119
241.669111	8046.351250	27.403136
241.782239	8051.170100	27.408154
242.178847	8073.999549	27.413172
242.482142	8096.455245	27.418189
243.135625	8090.806679	27.423207
243.553771	8106.725349	27.428224
243.726924	8115.383231	27.433242
243.597579	8130.578971	27.438260
243.895800	8132.590880	27.443277
244.400604	8139.094587	27.448295
244.801021	8152.177926	27.453312
244.716896	8158.239797	27.458330
244.913237	8173.372240	27.463348
244.985895	8186.386666	27.468365
245.551496	8194.333145	27.473383
245.482411	8201.339788	27.478400
245.898625	8195.885979	27.483418
246.260175	8212.893245	27.488436
246.227382	8214.928284	27.493453
246.613248	8231.230928	27.498471
246.713923	8243.631730	27.503488
246.700217	8254.351880	27.508506
246.497364	8274.913466	27.513524
246.930148	8281.472635	27.518541
247.563256	8295.634274	27.523559
247.440157	8321.657757	27.528576
248.065280	8333.178245	27.533594
248.325901	8353.058457	27.538612
248.063983	8368.076140	27.543629
248.774185	8389.818497	27.548647
248.987249	8405.106378	27.553664
249.456555	8413.948756	27.558682
249.566615	8427.481596	27.563700
249.457898	8435.864652	27.568717
250.059046	8447.846715	27.573735
250.297972	8459.342168	27.578752
250.815975	8474.361639	27.583770
251.197095	8484.341688	27.588788
251.577240	8490.284032	27.593805
252.143545	8500.711974	27.598823
252.339598	8516.435111	27.603840
252.429351	8511.316170	27.608858
252.496985	8514.699453	27.613876
252.757272	8534.406274	27.618893
253.152438	8543.048735	27.623911
253.123727	8553.181025	27.628928
253.392014	8554.319979	27.633946
253.386221	8565.689430	27.638964
253.390375	8592.899480	27.643981
253.903008	8605.836233	27.648999
254.227021	8614.281438	27.654016
254.475042	8619.796090	27.659034
255.092377	8635.384286	27.664052
254.992616	8638.045426	27.669069
255.690358	8656.730838	27.674087
255.655794	8665.942234	27.679104
255.932624	8673.327721	27.684122
255.871631	8689.390946	27.689140
255.976627	8703.859273	27.694157
256.316866	8709.602691	27.699175
256.501730	8738.941110	27.704192
256.962559	8748.084893	27.709210
257.619184	8765.567650	27.714228
257.471945	8775.235479	27.719245
257.747841	8787.704081	27.724263
258.239709	8814.377590	27.729280
258.131566	8812.187596	27.734298
258.360365	8839.464061	27.739316
258.854391	8853.265775	27.744333
259.132602	8864.316526	27.749351
259.555070	8877.014938	27.754368
259.555848	8902.846311	27.759386
260.209740	8906.981343	27.764404
260.334737	8920.610090	27.769421
260.059201	8942.929621	27.774439
260.890976	8954.430955	27.779456
261.018201	8963.604683	27.784474
261.505505	8976.526697	27.789492
261.414701	8992.509583	27.794509
262.104064	8995.474132	27.799527
262.165703	9009.570593	27.804544
262.251445	9020.398831	27.809562
262.646444	9021.713831	27.814580
262.423732	9043.444345	27.819597
262.615179	9044.222751	27.824615
262.771279	9062.411985	27.829632
263.346622	9077.729265	27.834650
263.717180	9086.202169	27.839668
264.035585	9106.970827	27.844685
264.025398	9127.127662	27.849703
263.992660	9141.886133	27.854720
264.611486	9159.905552	27.859738
264.819553	9173.881469	27.864756
265.170383	9193.571740	27.869773
265.411571	9213.635862	27.874791
265.658462	9214.591916	27.879808
265.927427	9236.239795	27.884826
266.147315	9255.679001	27.889844
266.563150	9270.547697	27.894861
266.480298	9290.094058	27.899879
267.091194	9303.019159	27.904896
267.474094	9321.703746	27.909914
267.829135	9329.342523	27.914932
267.851320	9352.806456	27.919949
268.544128	9368.828687	27.924967
268.638355	9383.450767	27.929984
268.714268	9393.185206	27.935002
269.346329	9405.523002	27.940020
268.859881	9428.504235	27.945037
269.328089	9437.931361	27.950055
269.747988	9469.722225	27.955072
270.048509	9483.693454	27.960090
270.915549	9499.009871	27.965108
270.878827	9502.261192	27.970125
271.346934	9509.118394	27.975143
271.214026	9531.618488	27.980160
271.170952	9550.997912	27.985178
272.156564	9552.805088	27.990196
272.129298	9582.512535	27.995213
272.427060	9591.950489	28.000231
272.628383	9608.519873	28.005248
273.021495	9614.722613	28.010266
273.063871	9626.265179	28.015284
273.505197	9652.669929	28.020301
273.838129	9659.396684	28.025319
274.158125	9674.877345	28.030336
274.452961	9684.824119	28.035354
274.879523	9700.746013	28.040372
274.837143	9725.155014	28.045389
275.380880	9717.088803	28.050407
275.675261	9742.073691	28.055424
275.561896	9762.720869	28.060442
276.203514	9761.553807	28.065460
276.454298	9788.136805	28.070477
276.418466	9800.518859	28.075495
276.906997	9817.274196	28.080512
277.113052	9835.090168	28.085530
277.445297	9842.562214	28.090548
277.594366	9870.559840	28.095565
278.036496	9870.980368	28.100583
277.788577	9887.664143	28.105600
278.266423	9905.466285	28.110618
278.600151	9919.821018	28.115636
278.717533	9941.215478	28.120653
278.969137	9949.685197	28.125671
279.174337	9964.723007	28.130688
279.782877	9986.508333	28.135706
280.260420	9985.022656	28.140724
280.283722	10004.758466	28.145741
280.887343	10012.207275	28.150759
281.107339	10025.048504	28.155776
281.288497	10041.090985	28.160794
281.334471	10043.303400	28.165812
281.626582	10068.781622	28.170829
281.910054	10070.663435	28.175847
282.143129	10102.291874	28.180864
282.189461	10119.624656	28.185882
282.336017	10136.818716	28.190900
282.721018	10153.719925	28.195917
282.996940	10162.359609	28.200935
283.640676	10189.964970	28.205952
283.991395	10203.527944	28.210970
284.270631	10209.180293	28.215988
284.098833	10242.889542	28.221005
284.734531	10255.760932	28.226023
285.150824	10273.863485	28.231040
285.259934	10297.899187	28.236058
285.402319	10306.963869	28.241076
285.774145	10335.887350	28.246093
285.815755	10345.545537	28.251111
286.629066	10361.887707	28.256128
286.578444	10383.943460	28.261146
287.492908	10383.535856	28.266164
287.654294	10411.314519	28.271181
288.198879	10405.906389	28.276199
288.518912	10422.218057	28.281216
288.169485	10442.002886	28.286234
288.580733	10453.302251	28.291252
288.943487	10471.492267	28.296269
289.464966	10477.845812	28.301287
289.570954	10501.497061	28.306304
289.912151	10518.932706	28.311322
289.985002	10525.605546	28.316340
290.414208	10550.649465	28.321357
290.789089	10565.351920	28.326375
291.057214	10580.620394	28.331392
291.180210	10594.013875	28.336410
292.012986	10589.877463	28.341428
292.739417	10590.841027	28.346445
293.193012	10593.015306	28.351463
293.915803	10605.118761	28.356480
293.984782	10613.547752	28.361498
294.199335	10599.852237	28.366516
294.297285	10603.202765	28.371533
294.585442	10604.528200	28.376551
294.919407	10588.502882	28.381568
295.008577	10606.631429	28.386586
295.013827	10607.899872	28.391604
295.280555	10616.345440	28.396621
295.466606	10638.039435	28.401639
295.328879	10655.808678	28.406656
295.615675	10672.915094	28.411674
295.636787	10687.189636	28.416692
296.187187	10697.804429	28.421709
296.050134	10714.866360	28.426727
296.648786	10735.779498	28.431744
296.434630	10769.000575	28.436762
297.202793	10781.346519	28.441780
297.379954	10798.994253	28.446797
298.151825	10820.625675	28.451815
298.303393	10838.738418	28.456832
298.358535	10864.999779	28.461850
298.929288	10885.008083	28.466868
298.651188	10894.369008	28.471885
298.748427	10915.840344	28.476903
299.144926	10941.275091	28.481920
299.407985	10968.410419	28.486938
300.024441	10989.478944	28.491956
300.414424	11014.895861	28.496973
300.540669	11027.581873	28.501991
301.384076	11043.146376	28.507008
301.273564	11061.053853	28.512026
301.769925	11075.763058	28.517044
302.129343	11090.187318	28.522061
302.226928	11102.410535	28.527079
302.704830	11116.800582	28.532096
302.802140	11138.347942	28.537114
302.730564	11150.297563	28.542132
303.607910	11173.769584	28.547149
303.939426	11192.637715	28.552167
304.109169	11208.869272	28.557184
304.500536	11230.465683	28.562202
304.889540	11235.384500	28.567220
305.249080	11244.441091	28.572237
304.929399	11271.667583	28.577255
305.697524	11287.581866	28.582272
305.855810	11309.394634	28.587290
306.008957	11329.285293	28.592308
306.340645	11343.751956	28.597325
306.300957	11371.114981	28.602343
306.796858	11394.261445	28.607360
307.288672	11432.220612	28.612378
307.337311	11447.950235	28.617396
308.040672	11474.623057	28.622413
308.521469	11498.021447	28.627431
308.948095	11520.392620	28.632448
308.713328	11533.810897	28.637466
309.102694	11551.723116	28.642484
309.776782	11568.249058	28.647501
310.061220	11589.044720	28.652519
310.765436	11602.897856	28.657536
310.680768	11618.550491	28.662554
310.787126	11635.711140	28.667572
310.905991	11660.391221	28.672589
311.385095	11683.123856	28.677607
312.401190	11710.856641	28.682624
312.562944	11720.181074	28.687642
313.041422	11735.398799	28.692660
313.444248	11741.603898	28.697677
313.252850	11754.961902	28.702695
313.650387	11769.393383	28.707712
314.014061	11795.686955	28.712730
314.389805	11803.405627	28.717748
314.705908	11827.669993	28.722765
314.783771	11839.751512	28.727783
315.436271	11852.403518	28.732800
315.729490	11876.633619	28.737818
315.948360	11885.816623	28.742836
316.120479	11904.381895	28.747853
316.124608	11926.516197	28.752871
316.883033	11940.089587	28.757888
316.988628	11967.986607	28.762906
317.250344	11971.747639	28.767924
317.860528	12002.054370	28.772941
318.135615	12021.671011	28.777959
318.642847	12028.639890	28.782976
318.591890	12053.280615	28.787994
318.941725	12065.960941	28.793012
318.957242	12080.730009	28.798029
319.774286	12112.583542	28.803047
320.228608	12129.699944	28.808064
319.934440	12145.451944	28.813082
320.495261	12154.632366	28.818100
321.096642	12166.389451	28.823117
320.752520	12196.639818	28.828135
321.620711	12205.841882	28.833152
321.842556	12219.148510	28.838170
322.232384	12224.847409	28.843188
322.682264	12243.796060	28.848205
322.522319	12266.578370	28.853223
323.392124	12275.780217	28.858240
323.430874	12297.170667	28.863258
323.932432	12302.886929	28.868276
324.413955	12317.211027	28.873293
324.350509	12341.781447	28.878311
324.785343	12353.375117	28.883328
325.162443	12363.777855	28.888346
325.308525	12373.856586	28.893364
325.694868	12385.255732	28.898381
325.979900	12401.915609	28.903399
326.705919	12409.100029	28.908416
326.877553	12432.724550	28.913434
327.475593	12443.070831	28.918452
327.889471	12461.055889	28.923469
327.788938	12475.675976	28.928487
328.528898	12486.458056	28.933504
328.352938	12501.232003	28.938522
328.296139	12512.507594	28.943540
329.049288	12532.236648	28.948557
329.265834	12557.657398	28.953575
329.419173	12572.496970	28.958592
329.877755	12593.342420	28.963610
330.196785	12615.659023	28.968628
330.349728	12637.710997	28.973645
330.733551	12658.666048	28.978663
330.907831	12672.081450	28.983680
331.290294	12702.393188	28.988698
331.528289	12736.084168	28.993716
332.071957	12749.028451	28.998733
332.294245	12774.319131	29.003751
332.645200	12791.875371	29.008768
332.759645	12821.142751	29.013786
332.957571	12843.355324	29.018804
333.708851	12872.425748	29.023821
334.096997	12900.589625	29.028839
334.217244	12908.837988	29.033856
334.590191	12937.430588	29.038874
334.921123	12974.063223	29.043892
335.002433	12990.827968	29.048909
335.935860	13018.038732	29.053927
336.010759	13029.644646	29.058944
336.841415	13056.044118	29.063962
337.110754	13072.015470	29.068980
337.652382	13089.286519	29.073997
337.602974	13118.099879	29.079015
338.365044	13139.542884	29.084032
338.566774	13142.170355	29.089050
338.781588	13168.511127	29.094068
339.448819	13183.337491	29.099085
339.538486	13208.226248	29.104103
340.161400	13215.787026	29.109120
340.267900	13234.196459	29.114138
340.294197	13251.816303	29.119156
340.425015	13263.975753	29.124173
340.544125	13290.562117	29.129191
340.834851	13313.648155	29.134208
341.226476	13332.957496	29.139226
341.895942	13364.952968	29.144244
342.349140	13385.926449	29.149261
342.661507	13411.336589	29.154279
343.012937	13432.903856	29.159296
343.136236	13448.974052	29.164314
343.759821	13477.695818	29.169332
344.018217	13494.594493	29.174349
344.172146	13514.913655	29.179367
344.423225	13531.248239	29.184384
344.703072	13548.917307	29.189402
345.101633	13572.353189	29.194420
345.355201	13592.489554	29.199437
345.575089	13614.478561	29.204455
345.664013	13641.288014	29.209472
346.510930	13662.866827	29.214490
346.610270	13692.178960	29.219508
347.486595	13716.393280	29.224525
347.529567	13740.911056	29.229543
347.882606	13765.276381	29.234560
348.033799	13781.440412	29.239578
348.108931	13808.646991	29.244596
348.898715	13826.555882	29.249613
348.973478	13864.562778	29.254631
349.535800	13891.895738	29.259648
350.601805	13911.852276	29.264666
350.472893	13928.401100	29.269684
351.464551	13941.421726	29.274701
351.681168	13958.835752	29.279719
351.926627	13978.294826	29.284736
352.304035	13991.831126	29.289754
352.783164	14012.586522	29.294772
353.074301	14021.831951	29.299789
353.135489	14050.171604	29.304807
353.563157	14072.804605	29.309824
353.660525	14091.083657	29.314842
353.724683	14109.630011	29.319860
354.563119	14132.830733	29.324877
355.024056	14153.159629	29.329895
355.274564	14176.016129	29.334912
355.783751	14192.765854	29.339930
356.187453	14222.451437	29.344948
356.527056	14230.688333	29.349965
357.012853	14250.334490	29.354983
357.199169	14270.557839	29.360000
357.653189	14290.818483	29.365018
358.000494	14309.346215	29.370036
358.458706	14313.733997	29.375053
358.721183	14346.918749	29.380071
358.955181	14368.337989	29.385088
359.041614	14385.156857	29.390106
359.233319	14403.383627	29.395124
359.629666	14426.814595	29.400141
360.132044	14468.337351	29.405159
360.189323	14488.442066	29.410176
360.848103	14507.477319	29.415194
361.280423	14524.697222	29.420212
361.524323	14548.799477	29.425229
362.048086	14577.320546	29.430247
362.180301	14596.352597	29.435264
363.066142	14615.169440	29.440282
363.332337	14645.000257	29.445300
363.950626	14661.540768	29.450317
364.324135	14680.140577	29.455335
364.720242	14694.865067	29.460352
365.302048	14707.305780	29.465370
365.150497	14720.725990	29.470388
365.747683	14740.519535	29.475405
366.334270	14768.453179	29.480423
366.305404	14774.154874	29.485440
366.646768	14796.034755	29.490458
367.285351	14820.824381	29.495476
367.397550	14837.503838	29.500493
367.484826	14855.428330	29.505511
367.948219	14874.121712	29.510528
368.444480	14890.027689	29.515546
368.426622	14917.177694	29.520564
369.150625	14926.580403	29.525581
369.377273	14944.527495	29.530599
369.290124	14963.382469	29.535616
370.135752	14980.901628	29.540634
370.329174	15015.629995	29.545652
370.285205	15036.550061	29.550669
371.270250	15043.950980	29.555687
371.889958	15059.632601	29.560704
372.232572	15084.386536	29.565722
372.249595	15109.216457	29.570740
372.673390	15120.630375	29.575757
373.374993	15142.533526	29.580775
373.226264	15163.144749	29.585792
373.564577	15182.802199	29.590810
373.598002	15213.156502	29.595828
374.371755	15239.147845	29.600845
374.867456	15261.345317	29.605863
375.140608	15282.863711	29.610880
375.391506	15310.136661	29.615898
375.588675	15339.309774	29.620916
375.962860	15361.099924	29.625933
376.352933	15395.438332	29.630951
376.948414	15421.495576	29.635968
377.631581	15441.977589	29.640986
377.574509	15466.620542	29.646004
377.855359	15484.739723	29.651021
378.611229	15510.560519	29.656039
379.051341	15540.327763	29.661056
379.559686	15562.315173	29.666074
380.055720	15583.233884	29.671092
380.530571	15603.483210	29.676109
380.576384	15625.763778	29.681127
380.880834	15649.368471	29.686144
381.857802	15667.464725	29.691162
382.140534	15695.323862	29.696180
382.655980	15700.129423	29.701197
382.675374	15723.004811	29.706215
383.053182	15754.493866	29.711232
383.543298	15765.853631	29.716250
384.333949	15782.327227	29.721268
384.599797	15801.993439	29.726285
385.292960	15821.169938	29.731303
385.649328	15837.521695	29.736320
386.168293	15845.156563	29.741338
386.042268	15876.013642	29.746356
386.338557	15876.558098	29.751373
386.724250	15896.360506	29.756391
387.093374	15922.109420	29.761408
387.871688	15932.022135	29.766426
387.810155	15951.663669	29.771444
387.959473	15980.210392	29.776461
388.322833	15999.075209	29.781479
388.329260	16029.687675	29.786496
388.758793	16056.889664	29.791514
389.669387	16085.122212	29.796532
389.737237	16108.088425	29.801549
390.593003	16120.076833	29.806567
391.033169	16157.715580	29.811584
391.522106	16162.269561	29.816602
391.803505	16189.611659	29.821620
391.936167	16210.578152	29.826637
392.639171	16233.679351	29.831655
392.961794	16250.955794	29.836672
393.308960	16273.749229	29.841690
393.671284	16282.930985	29.846708
394.560868	16304.837791	29.851725
394.759054	16310.820432	29.856743
394.642170	16337.946811	29.861760
395.248032	16350.425916	29.866778
395.440416	16368.013310	29.871796
396.093209	16388.779006	29.876813
396.460751	16400.812014	29.881831
396.250528	16429.386954	29.886848
396.704007	16444.495504	29.891866
397.485782	16460.200425	29.896884
397.587849	16489.045834	29.901901
398.146098	16505.331991	29.906919
397.724079	16540.999071	29.911936
398.242084	16565.610760	29.916954
398.770959	16603.388175	29.921972
398.933760	16628.330023	29.926989
399.540353	16658.218376	29.932007
400.160041	16695.969202	29.937024
400.755151	16708.147006	29.942042
400.804086	16745.396159	29.947060
402.162256	16751.223619	29.952077
403.298947	16748.611492	29.957095
404.382974	16759.257179	29.962112
404.908104	16761.089419	29.967130
405.011441	16765.346673	29.972148
405.413700	16769.870076	29.977165
405.701919	16769.695693	29.982183
405.915400	16783.231074	29.987200
405.861321	16793.520184	29.992218
406.150230	16806.102624	29.997236
406.542960	16819.622758	30.002253
406.953803	16831.396621	30.007271
407.112184	16860.265405	30.012288
407.268214	16877.776806	30.017306
407.496803	16901.145335	30.022324
407.360985	16921.797496	30.027341
407.892817	16957.995921	30.032359
408.023612	16982.292569	30.037376
408.749736	17012.598734	30.042394
409.040569	17050.679400	30.047412
409.130346	17085.487667	30.052429
409.631254	17118.229509	30.057447
410.280203	17152.135954	30.062464
410.418721	17193.326464	30.067482
411.098030	17220.911301	30.072500
411.211673	17258.315615	30.077517
411.938705	17279.977213	30.082535
411.874839	17315.621553	30.087552
412.627802	17354.597383	30.092570
413.015581	17390.683231	30.097588
413.351179	17419.342067	30.102605
413.921711	17448.848764	30.107623
414.250708	17496.494759	30.112640
415.028275	17516.051478	30.117658
415.474131	17555.492455	30.122676
415.463601	17590.683641	30.127693
416.051828	17611.583898	30.132711
416.519311	17652.749444	30.137728
417.158863	17674.444057	30.142746
417.942784	17703.589431	30.147764
418.078455	17727.143990	30.152781
418.614959	17741.855289	30.157799
419.134017	17768.117139	30.162816
419.689081	17788.119392	30.167834
420.350208	17806.949105	30.172852
420.705346	17829.964246	30.177869
421.339454	17849.512052	30.182887
421.709457	17873.428294	30.187904
421.831392	17894.477257	30.192922
422.373738	17908.019085	30.197940
422.570992	17930.060802	30.202957
422.991094	17947.159346	30.207975
423.336314	17981.667295	30.212992
423.583317	17989.879171	30.218010
424.112452	18003.941139	30.223028
424.182472	18036.944299	30.228045
424.583258	18055.631584	30.233063
425.424737	18082.803896	30.238080
425.649356	18098.524250	30.243098
426.286868	18125.861040	30.248116
426.629251	18153.420698	30.253133
427.017148	18175.622535	30.258151
427.486547	18202.518123	30.263168
427.567132	18225.317467	30.268186
428.177274	18248.937778	30.273204
428.088764	18283.103159	30.278221
429.040217	18312.242325	30.283239
429.420073	18345.823196	30.288256
429.384041	18367.339481	30.293274
430.141163	18405.852460	30.298292
430.436248	18433.356706	30.303309
431.129938	18465.739159	30.308327
431.260494	18504.040323	30.313344
431.733244	18531.965588	30.318362
431.947536	18569.855847	30.323380
432.498609	18600.270729	30.328397
432.794562	18636.543770	30.333415
433.290983	18676.247652	30.338432
433.785384	18710.784216	30.343450
434.355984	18740.280240	30.348468
434.733286	18785.846588	30.353485
435.511914	18805.593978	30.358503
435.943204	18842.781329	30.363520
436.308332	18872.865487	30.368538
436.864261	18900.449821	30.373556
436.783831	18931.298364	30.378573
437.264018	18966.437765	30.383591
438.150310	18997.698181	30.388608
438.496863	19031.740289	30.393626
439.462973	19042.809937	30.398644
440.106257	19071.120075	30.403661
440.788086	19084.457804	30.408679
440.958790	19103.952670	30.413696
441.288680	19130.422713	30.418714
442.421803	19153.191959	30.423732
443.003715	19174.467631	30.428749
443.061751	19174.698650	30.433767
443.710480	19192.571363	30.438784
443.997968	19210.683542	30.443802
444.479741	19238.191454	30.448820
444.758340	19256.734661	30.453837
444.931794	19269.020797	30.458855
445.337111	19300.369214	30.463872
445.589480	19314.614213	30.468890
446.329617	19344.602815	30.473908
446.314194	19379.516869	30.478925
446.644540	19408.950229	30.483943
446.919025	19445.152308	30.488960
447.140575	19467.703726	30.493978
447.745773	19510.766057	30.498996
447.689283	19544.492742	30.504013
448.073144	19568.857480	30.509031
448.976942	19603.761506	30.514048
449.815988	19655.083009	30.519066
450.369859	19678.082042	30.524084
450.521973	19712.496773	30.529101
450.933668	19748.248443	30.534119
451.455987	19773.312115	30.539136
451.494252	19799.165093	30.544154
451.929156	19824.918450	30.549172
452.933260	19856.098729	30.554189
453.485662	19874.985290	30.559207
454.041639	19899.576362	30.564224
454.265732	19932.482937	30.569242
454.582878	19952.360199	30.574260
455.079941	19982.545573	30.579277
455.303155	20012.072337	30.584295
455.903297	20035.096178	30.589312
456.089964	20070.030548	30.594330
456.610743	20100.559900	30.599348
456.993270	20134.269801	30.604365
457.349188	20169.576033	30.609383
457.679741	20204.848368	30.614400
458.274968	20234.077470	30.619418
459.172650	20266.317443	30.624436
459.504277	20308.659645	30.629453
459.991338	20336.383097	30.634471
460.590795	20369.162473	30.639488
460.697341	20410.333191	30.644506
461.222482	20441.588971	30.649524
461.721146	20476.747173	30.654541
461.946815	20516.162099	30.659559
462.534648	20541.140741	30.664576
463.094493	20579.044291	30.669594
463.569312	20608.564376	30.674612
463.603829	20651.774928	30.679629
464.569053	20687.151509	30.684647
465.024698	20715.183659	30.689664
465.358054	20757.943561	30.694682
465.651183	20794.189463	30.699700
466.200138	20837.610974	30.704717
467.068332	20869.995534	30.709735
467.874392	20905.195105	30.714752
468.028869	20943.055056	30.719770
468.865323	20969.316049	30.724788
469.276704	21004.065464	30.729805
469.724783	21032.472022	30.734823
470.328851	21058.876722	30.739840
470.826147	21087.610566	30.744858
471.130087	21117.031653	30.749876
471.459226	21147.257603	30.754893
471.654720	21175.710009	30.759911
472.619430	21207.271360	30.764928
472.712781	21237.572065	30.769946
473.560983	21256.445504	30.774964
474.246971	21305.198337	30.779981
474.881216	21330.619363	30.784999
475.485140	21359.488646	30.790016
475.685366	21382.342552	30.795034
475.890960	21412.885107	30.800052
476.457047	21444.812179	30.805069
477.139188	21464.217142	30.810087
477.834620	21488.965417	30.815104
477.951933	21514.195465	30.820122
479.121929	21533.928927	30.825140
479.647430	21562.854946	30.830157
479.633978	21583.758368	30.835175
479.841308	21604.197788	30.840192
480.140217	21636.855475	30.845210
480.730997	21659.914278	30.850228
481.028064	21688.117830	30.855245
480.973400	21722.890521	30.860263
481.775586	21757.176046	30.865280
482.404644	21801.591856	30.870298
482.816193	21825.569664	30.875316
483.553319	21862.519274	30.880333
483.935428	21876.828082	30.885351
484.150853	21904.438075	30.890368
484.651115	21939.737656	30.895386
485.126067	21972.317945	30.900404
485.627021	21998.739962	30.905421
485.837956	22021.409704	30.910439
486.805550	22063.416578	30.915456
486.892769	22099.785401	30.920474
487.450675	22127.361345	30.925492
487.729592	22153.540117	30.930509
488.455939	22191.092289	30.935527
489.096569	22215.622541	30.940544
489.269656	22257.222749	30.945562
489.688657	22289.035078	30.950580
489.887673	22334.909141	30.955597
490.346529	22372.926651	30.960615
490.927463	22406.527422	30.965632
491.318554	22462.033156	30.970650
491.983097	22486.534748	30.975668
492.514063	22531.814180	30.980685
492.907788	22571.346069	30.985703
493.954929	22615.016201	30.990720
494.516792	22662.572194	30.995738
495.123801	22680.043872	31.000756
495.748688	22703.970580	31.005773
496.495501	22743.075036	31.010791
498.111514	22732.504851	31.015808
498.803966	22751.157544	31.020826
499.392760	22763.735063	31.025844
500.167119	22781.414575	31.030861
500.108473	22800.790848	31.035879
500.571992	22806.607809	31.040896
500.819916	22825.822643	31.045914
501.152183	22838.541246	31.050932
501.943810	22849.981450	31.055949
502.216558	22877.615473	31.060967
502.802712	22895.280154	31.065984
502.865995	22924.261171	31.071002
503.484778	22943.734328	31.076020
504.316304	22973.309851	31.081037
504.110006	22995.097833	31.086055
504.789966	23014.138171	31.091072
504.971922	23053.457555	31.096090
505.432060	23081.700899	31.101108
505.898953	23114.006293	31.106125
506.382341	23137.108820	31.111143
506.602742	23174.318257	31.116160
506.969026	23208.370856	31.121178
507.290236	23241.084593	31.126196
508.049790	23282.437681	31.131213
508.227888	23323.053588	31.136231
508.870856	23362.112244	31.141248
509.693847	23403.879083	31.146266
509.979310	23444.674413	31.151284
510.522243	23479.622554	31.156301
510.822434	23530.816897	31.161319
511.544397	23562.103860	31.166336
511.868076	23604.467014	31.171354
511.964842	23639.124706	31.176372
513.073079	23686.806629	31.181389
513.646692	23724.050575	31.186407
513.870654	23753.943015	31.191424
513.952915	23803.042441	31.196442
514.933609	23851.711443	31.201460
515.664117	23886.296183	31.206477
515.722957	23930.603327	31.211495
516.720332	23958.568389	31.216512
516.910584	24001.035307	31.221530
517.739931	24036.375863	31.226548
518.077687	24074.175357	31.231565
518.677203	24109.141072	31.236583
519.570537	24130.089270	31.241600
520.076134	24168.412587	31.246618
520.751599	24197.628757	31.251636
520.933312	24223.755882	31.256653
521.581614	24254.164385	31.261671
522.244586	24290.807788	31.266688
521.782360	24329.433744	31.271706
522.730825	24363.144916	31.276724
523.541142	24393.313553	31.281741
523.847170	24440.806202	31.286759
524.079177	24475.633873	31.291776
524.692882	24528.759927	31.296794
525.507375	24566.663079	31.301812
526.235942	24594.500260	31.306829
526.742877	24632.969607	31.311847
527.680420	24663.289471	31.316864
527.811615	24701.109669	31.321882
528.220646	24728.396436	31.326900
529.203168	24767.771517	31.331917
529.895258	24802.806190	31.336935
530.475441	24827.014153	31.341952
530.803869	24860.803732	31.346970
531.284565	24898.633090	31.351988
532.253237	24923.956116	31.357005
532.245748	24961.217003	31.362023
532.788382	24994.537416	31.367040
533.165298	25035.290163	31.372058
533.591705	25067.921005	31.377076
534.098974	25102.763792	31.382093
534.649572	25151.452365	31.387111
535.055599	25178.348400	31.392128
535.694482	25228.123020	31.397146
536.202723	25254.605112	31.402164
537.223631	25283.295125	31.407181
537.873280	25322.268107	31.412199
538.097483	25353.881838	31.417216
538.876833	25387.185013	31.422234
539.285234	25432.281574	31.427252
539.622115	25458.196564	31.432269
540.122934	25503.828709	31.437287
540.750289	25537.263229	31.442304
541.399003	25579.845396	31.447322
541.571813	25622.533338	31.452340
542.339081	25658.385687	31.457357
542.818706	25699.060595	31.462375
543.173380	25743.192979	31.467392
543.881533	25784.135831	31.472410
543.897732	25826.741151	31.477428
545.018233	25861.205401	31.482445
545.481811	25905.270628	31.487463
546.336517	25937.937327	31.492480
547.258798	25973.475396	31.497498
547.384572	26017.239546	31.502516
548.470099	26038.968770	31.507533
548.546015	26080.010648	31.512551
549.192630	26116.773697	31.517568
549.827858	26149.095714	31.522586
550.450427	26177.381350	31.527604
550.996849	26214.589927	31.532621
551.380562	26241.610938	31.537639
551.745116	26284.447390	31.542656
552.467120	26322.829618	31.547674
552.810532	26359.520233	31.552692
553.067820	26395.725045	31.557709
553.586021	26440.313816	31.562727
553.860855	26468.003036	31.567744
554.256683	26509.811263	31.572762
554.734688	26554.646703	31.577780
555.497423	26602.458884	31.582797
556.042704	26636.622170	31.587815
556.620598	26680.146734	31.592832
556.799788	26725.964438	31.597850
557.365302	26772.392032	31.602868
557.969085	26802.722851	31.607885
558.537192	26857.688664	31.612903
559.151555	26906.302034	31.617920
559.854109	26953.637766	31.622938
560.418204	26997.563329	31.627956
561.272575	27029.966406	31.632973
561.585694	27089.769537	31.637991
562.086721	27127.606240	31.643008
562.715470	27167.831124	31.648026
563.422541	27215.590219	31.653044
564.207119	27248.080354	31.658061
565.209327	27287.899726	31.663079
565.722114	27330.955488	31.668096
566.317149	27363.405792	31.673114
566.789392	27405.039646	31.678132
567.416830	27435.917597	31.683149
567.892008	27479.188098	31.688167
568.738101	27520.068757	31.693184
569.395941	27559.171197	31.698202
569.806117	27599.355119	31.703220
570.550272	27625.512868	31.708237
571.008637	27674.133405	31.713255
571.686557	27694.524755	31.718272
572.543560	27723.907405	31.723290
573.336728	27756.226369	31.728308
574.072304	27789.281194	31.733325
574.739830	27818.048798	31.738343
575.076549	27851.064689	31.743360
575.314092	27871.094985	31.748378
575.788636	27910.959805	31.753396
576.454158	27929.817460	31.758413
577.159814	27979.651677	31.763431
577.580689	28014.335970	31.768448
578.238536	28046.625899	31.773466
578.875530	28086.118147	31.778484
579.144697	28117.931456	31.783501
579.904507	28161.721625	31.788519
580.252318	28192.720105	31.793536
580.861215	28234.618809	31.798554
581.072231	28273.210694	31.803572
581.508194	28311.388401	31.808589
582.698627	28346.832018	31.813607
582.699280	28382.391387	31.818624
583.373020	28430.303903	31.823642
584.011219	28477.495195	31.828660
584.285416	28518.340482	31.833677
584.847680	28560.506262	31.838695
585.707422	28624.615326	31.843712
586.386181	28666.156407	31.848730
586.665923	28726.355106	31.853748
587.190650	28752.295638	31.858765
587.944436	28801.770415	31.863783
588.662279	28844.898592	31.868800
589.342166	28877.344425	31.873818
590.130943	28915.158623	31.878836
590.829364	28949.131303	31.883853
591.498407	28994.277389	31.888871
591.922159	29037.205245	31.893888
592.600484	29080.087239	31.898906
592.789909	29113.444143	31.903924
593.460514	29153.337758	31.908941
594.236769	29177.217016	31.913959
594.398934	29226.513127	31.918976
595.146986	29245.928031	31.923994
595.653194	29290.733512	31.929012
596.150174	29316.912952	31.934029
596.915262	29357.146224	31.939047
597.393898	29403.087679	31.944064
597.964778	29439.034182	31.949082
598.555909	29496.860583	31.954100
599.253724	29534.039033	31.959117
600.039162	29572.183654	31.964135
600.299926	29621.079787	31.969152
601.538278	29642.169645	31.974170
602.183772	29681.758472	31.979188
603.074619	29713.616548	31.984205
603.551673	29749.034596	31.989223
604.129812	29793.438078	31.994240
604.642236	29823.288266	31.999258
605.178478	29860.170088	32.004276
605.431083	29899.890030	32.009293
606.324510	29936.052676	32.014311
606.504268	29983.198709	32.019328
606.895623	30025.179197	32.024346
607.864396	30069.086309	32.029364
608.039488	30107.345904	32.034381
609.046991	30164.913416	32.039399
609.369896	30209.818971	32.044416
610.038303	30254.228359	32.049434
610.374024	30303.733919	32.054452
611.233274	30352.987427	32.059469
612.056055	30402.942061	32.064487
612.389930	30451.215630	32.069504
612.811291	30492.806806	32.074522
613.736766	30554.983705	32.079540
614.466494	30591.906253	32.084557
615.720856	30631.756117	32.089575
616.166057	30673.919183	32.094592
616.674382	30710.320138	32.099610
617.487834	30753.469052	32.104628
618.178404	30795.202248	32.109645
618.946863	30833.377141	32.114663
619.093895	30886.187917	32.119680
620.115635	30925.050505	32.124698
620.595814	30969.313740	32.129716
620.804007	31013.859621	32.134733
621.617971	31057.736051	32.139751
621.843167	31112.014441	32.144768
622.323392	31155.980962	32.149786
622.973809	31213.309884	32.154804
623.466845	31271.965685	32.159821
624.415785	31312.831595	32.164839
624.893724	31369.315437	32.169856
625.627244	31409.247886	32.174874
625.781486	31467.590335	32.179892
626.594057	31517.941191	32.184909
627.479621	31564.886137	32.189927
628.158569	31615.359177	32.194944
629.177692	31655.266605	32.199962
629.693789	31694.847835	32.204980
630.556612	31743.566770	32.209997
631.188548	31786.461626	32.215015
631.934379	31844.700399	32.220032
632.338672	31882.997137	32.225050
632.897517	31932.724727	32.230068
633.438612	31976.361108	32.235085
633.631476	32005.929153	32.240103
634.014320	32067.834737	32.245120
634.842070	32106.767676	32.250138
635.322283	32159.188455	32.255156
635.698407	32209.242272	32.260173
636.351557	32259.486990	32.265191
636.789508	32315.606648	32.270208
637.381534	32358.818665	32.275226
638.028744	32413.022118	32.280244
638.898194	32473.007190	32.285261
639.326387	32525.500207	32.290279
639.635163	32579.693559	32.295296
640.646083	32634.201313	32.300314
641.312972	32695.811672	32.305332
642.293815	32755.603204	32.310349
642.833836	32807.232386	32.315367
643.743014	32859.208833	32.320384
644.359299	32914.625895	32.325402
644.987331	32964.136553	32.330420
645.850799	33009.994504	32.335437
646.763534	33055.528786	32.340455
647.419369	33107.772883	32.345472
647.661733	33164.020100	32.350490
648.604396	33205.680969	32.355508
649.536513	33256.219730	32.360525
650.002203	33304.315038	32.365543
650.429971	33364.143836	32.370560
651.037386	33408.398778	32.375578
651.475611	33455.468206	32.380596
651.938741	33513.837838	32.385613
652.857682	33568.678460	32.390631
653.276674	33625.487381	32.395648
654.241786	33672.911506	32.400666
654.914544	33729.744427	32.405684
655.379558	33796.586306	32.410701
656.380226	33845.611131	32.415719
656.756338	33904.785678	32.420736
657.714453	33957.876278	32.425754
658.378803	34012.466869	32.430772
658.995065	34067.172567	32.435789
659.980761	34114.872670	32.440807
660.698168	34157.929799	32.445824
661.794079	34193.006200	32.450842
662.597530	34238.756063	32.455860
663.312314	34283.647341	32.460877
663.889411	34327.725595	32.465895
664.248731	34371.192958	32.470912
664.785175	34418.742404	32.475930
665.760517	34465.553456	32.480948
666.605254	34514.540895	32.485965
667.443705	34548.229099	32.490983
667.974556	34593.472117	32.496000
668.660666	34629.706829	32.501018
669.633544	34659.827380	32.506036
669.730761	34699.991632	32.511053
670.596516	34734.213296	32.516071
671.107548	34787.160626	32.521088
671.964821	34827.851700	32.526106
672.181592	34877.026254	32.531124
672.690528	34926.882536	32.536141
673.424776	34974.313928	32.541159
673.998036	35031.918245	32.546176
674.293137	35082.914637	32.551194
675.688478	35136.262603	32.556212
676.167659	35186.889168	32.561229
676.830475	35225.379390	32.566247
677.465621	35282.329847	32.571264
677.638799	35325.847122	32.576282
678.447636	35375.114026	32.581300
678.989178	35430.991950	32.586317
679.644922	35473.568197	32.591335
679.928197	35528.721534	32.596352
680.556968	35587.292425	32.601370
681.124486	35645.702299	32.606388
681.825354	35705.273936	32.611405
682.467570	35756.053521	32.616423
683.316786	35807.174051	32.621440
683.720071	35870.877023	32.626458
685.079113	35915.684129	32.631476
685.713728	35969.462443	32.636493
687.027929	36006.613403	32.641511
687.796230	36054.895507	32.646528
688.319101	36106.137112	32.651546
689.314413	36150.571380	32.656564
689.576227	36199.564950	32.661581
690.630426	36253.202791	32.666599
690.951442	36297.679105	32.671616
691.691372	36348.046549	32.676634
692.324856	36398.557144	32.681652
692.894264	36452.403738	32.686669
693.874676	36490.442147	32.691687
694.520065	36551.472770	32.696704
694.700553	36604.640497	32.701722
695.590909	36659.164804	32.706740
696.214026	36720.572441	32.711757
697.645384	36754.759914	32.716775
698.914177	36793.025866	32.721792
699.552819	36831.554384	32.726810
700.424534	36870.217414	32.731828
701.141408	36920.444372	32.736845
701.554518	36957.073340	32.741863
702.322833	36997.725526	32.746880
702.855313	37047.633713	32.751898
703.727446	37081.200569	32.756916
704.185676	37141.705576	32.761933
705.282081	37176.084982	32.766951
705.912259	37217.644343	32.771968
706.564411	37268.881269	32.776986
707.242653	37295.181608	32.782004
707.937149	37343.459157	32.787021
708.477133	37391.261327	32.792039
708.960577	37431.604581	32.797056
709.313345	37493.075496	32.802074
710.095496	37544.084175	32.807092
710.778720	37599.484136	32.812109
711.100954	37654.466183	32.817127
711.516240	37726.039107	32.822144
712.086672	37778.813912	32.827162
713.179006	37845.880749	32.832180
713.716961	37912.357487	32.837197
714.390950	37966.520440	32.842215
715.091694	38033.029121	32.847232
715.961344	38099.562304	32.852250
717.801411	38128.073093	32.857268
718.711632	38172.904235	32.862285
719.511918	38218.182586	32.867303
720.506407	38258.801962	32.872320
721.474774	38305.559337	32.877338
721.824838	38349.535837	32.882356
722.519795	38389.063844	32.887373
723.276535	38413.570089	32.892391
723.913596	38467.012841	32.897408
723.969126	38511.250523	32.902426
724.865494	38557.893183	32.907444
725.346050	38608.603544	32.912461
725.803333	38657.597611	32.917479
726.550812	38719.314128	32.922496
726.896520	38777.172670	32.927514
727.629375	38816.878952	32.932532
728.018298	38886.126392	32.937549
728.920548	38934.343562	32.942567
729.540229	38990.408350	32.947584
730.264968	39035.213252	32.952602
731.486380	39087.807726	32.957620
732.300258	39143.551787	32.962637
732.802442	39190.301446	32.967655
733.303915	39247.270638	32.972672
733.883068	39307.408786	32.977690
734.844949	39358.052307	32.982708
735.565889	39426.585789	32.987725
736.232059	39486.249245	32.992743
736.957923	39543.873594	32.997760
737.307683	39603.536037	33.002778
738.283325	39661.229323	33.007796
738.693826	39733.062617	33.012813
739.072146	39802.112273	33.017831
739.991295	39870.698519	33.022848
740.478285	39951.096001	33.027866
741.615865	40020.679537	33.032884
742.276627	40091.203922	33.037901
742.957086	40164.172898	33.042919
743.984378	40224.174266	33.047936
745.085703	40298.520079	33.052954
745.109668	40361.713602	33.057972
745.973685	40442.155397	33.062989
746.712825	40513.851575	33.068007
747.664689	40582.732215	33.073024
748.857578	40662.782123	33.078042
749.455926	40721.529869	33.083060
750.064165	40785.601282	33.088077
751.112741	40863.182623	33.093095
752.226136	40925.917275	33.098112
753.229511	40974.856869	33.103130
754.368372	41022.940667	33.108148
755.478934	41085.157622	33.113165
756.128791	41140.692023	33.118183
757.323966	41185.598897	33.123200
757.854736	41239.463472	33.128218
758.507261	41275.948665	33.133236
759.098020	41342.427717	33.138253
759.725113	41383.015290	33.143271
760.492424	41440.960764	33.148288
761.129915	41503.239904	33.153306
762.021153	41560.072265	33.158324
762.983874	41618.980740	33.163341
763.586414	41663.645652	33.168359
764.433118	41726.322929	33.173376
764.864623	41791.240672	33.178394
765.608901	41829.641503	33.183412
766.351040	41892.493647	33.188429
766.848646	41962.960938	33.193447
767.367312	42025.639539	33.198464
767.988311	42091.774629	33.203482
768.879406	42160.543213	33.208500
769.654146	42222.587994	33.213517
770.472886	42297.908014	33.218535
771.297390	42363.854126	33.223552
771.716181	42426.770785	33.228570
772.831030	42487.485769	33.233588
773.318314	42556.748539	33.238605
774.233560	42624.471225	33.243623
774.776306	42686.667276	33.248640
775.582517	42755.337088	33.253658
776.507090	42828.030285	33.258676
777.451252	42891.593849	33.263693
777.955653	42953.682775	33.268711
779.191106	43003.280193	33.273728
780.022015	43053.490968	33.278746
780.520273	43109.857220	33.283764
781.476400	43164.122026	33.288781
781.804640	43218.510006	33.293799
782.758025	43281.276310	33.298816
783.652330	43350.206238	33.303834
784.325460	43399.733959	33.308852
785.091440	43466.982791	33.313869
785.750627	43533.679195	33.318887
786.680377	43584.963706	33.323904
787.466020	43652.817252	33.328922
788.129442	43717.925949	33.333940
788.721259	43786.347712	33.338957
789.218864	43851.362436	33.343975
790.538457	43925.092007	33.348992
791.110240	43989.393493	33.354010
791.653763	44062.580182	33.359028
792.469178	44129.298336	33.364045
793.536197	44203.093450	33.369063
794.289406	44272.358150	33.374080
795.267930	44347.634987	33.379098
796.055555	44421.467993	33.384116
797.020225	44484.128420	33.389133
798.168478	44553.446358	33.394151
799.117999	44611.662771	33.399168
799.818004	44672.359782	33.404186
800.481225	44734.100053	33.409204
802.229528	44783.185178	33.414221
803.306335	44837.517530	33.419239
804.089338	44877.745693	33.424256
804.741957	44950.418610	33.429274
805.290948	45001.164746	33.434292
806.054213	45060.284245	33.439309
806.809887	45113.990431	33.444327
807.842615	45171.980289	33.449344
808.339445	45236.505790	33.454362
809.187817	45290.678715	33.459380
809.824772	45353.512789	33.464397
810.303065	45412.203160	33.469415
811.300437	45470.983675	33.474432
811.474179	45546.908543	33.479450
812.211498	45616.338035	33.484468
813.249202	45688.472658	33.489485
813.538310	45768.017587	33.494503
814.620765	45841.657582	33.499520
815.462948	45918.137529	33.504538
816.098363	45997.831789	33.509556
816.902935	46067.138346	33.514573
817.534843	46154.715650	33.519591
818.808247	46226.366181	33.524608
819.462958	46308.696416	33.529626
820.231040	46388.346106	33.534644
821.131335	46452.957798	33.539661
822.061675	46532.171556	33.544679
823.289924	46600.192902	33.549696
824.040881	46681.503694	33.554714
825.203693	46732.765494	33.559732
826.833842	46782.107473	33.564749
827.280705	46855.242436	33.569767
828.320821	46907.270204	33.574784
828.747675	46971.925455	33.579802
829.650742	47029.788479	33.584820
830.694529	47090.381592	33.589837
831.124601	47161.489489	33.594855
831.957768	47214.087899	33.599872
832.979900	47278.955019	33.604890
833.137065	47343.438226	33.609908
834.222325	47396.674718	33.614925
834.742432	47463.727130	33.619943
835.637327	47526.400601	33.624960
836.824598	47589.844817	33.629978
837.565194	47639.618154	33.634996
838.362260	47693.646704	33.640013
839.027654	47761.619994	33.645031
839.833060	47830.748382	33.650048
840.480244	47888.792617	33.655066
841.069839	47962.857889	33.660084
842.014583	48022.051821	33.665101
842.324907	48091.030322	33.670119
843.366966	48162.090380	33.675136
844.623207	48235.793389	33.680154
845.439646	48312.095667	33.685172
846.336567	48378.548055	33.690189
847.054294	48451.810498	33.695207
849.324489	48499.860902	33.700224
850.461027	48548.176450	33.705242
851.296264	48609.685477	33.710260
851.795899	48665.407532	33.715277
852.363514	48726.838330	33.720295
853.316421	48786.134208	33.725312
854.204922	48854.904819	33.730330
854.693248	48921.238925	33.735348
855.272972	48980.795852	33.740365
856.132467	49052.646306	33.745383
857.234640	49120.834041	33.750400
858.132423	49188.250309	33.755418
858.628668	49254.223531	33.760436
859.578640	49324.605619	33.765453
860.622993	49393.416859	33.770471
861.124664	49457.567727	33.775488
862.373916	49531.320305	33.780506
862.814428	49609.608779	33.785524
863.569021	49675.815052	33.790541
864.238085	49764.969560	33.795559
864.893264	49840.682023	33.800576
866.032845	49915.730935	33.805594
866.774580	50002.527786	33.810612
867.806250	50082.617593	33.815629
868.449900	50166.817318	33.820647
869.946364	50242.128090	33.825664
870.592262	50318.413000	33.830682
871.542045	50397.023484	33.835700
872.682892	50467.904512	33.840717
873.597346	50544.205310	33.845735
874.276279	50622.282964	33.850752
875.051189	50701.617686	33.855770
875.942804	50780.687757	33.860788
876.906833	50854.476333	33.865805
877.407215	50933.316780	33.870823
878.376329	51003.821253	33.875840
879.517166	51092.407620	33.880858
880.377157	51170.364037	33.885876
881.208415	51247.401414	33.890893
882.168346	51335.023496	33.895911
882.857514	51407.293792	33.900928
884.245901	51479.151760	33.905946
884.433818	51557.802538	33.910964
885.429965	51632.708535	33.915981
886.085095	51715.115158	33.920999
887.441231	51790.123811	33.926016
888.602607	51861.360256	33.931034
889.123952	51954.589428	33.936052
889.900428	52023.190803	33.941069
890.666534	52107.815133	33.946087
891.454166	52178.161609	33.951104
892.343608	52258.730354	33.956122
893.316833	52330.187352	33.961140
894.407121	52401.974362	33.966157
895.328381	52481.197486	33.971175
896.068268	52543.162145	33.976192
897.246326	52600.464924	33.981210
897.845813	52683.029175	33.986228
898.885159	52749.832695	33.991245
900.017485	52811.895172	33.996263
901.019042	52876.578845	34.001280
902.408594	52939.506479	34.006298
903.790727	53007.415347	34.011316
904.294570	53064.026925	34.016333
904.890239	53143.537108	34.021351
905.514504	53219.107239	34.026368
906.897203	53289.794730	34.031386
907.408676	53356.928941	34.036404
908.427717	53423.224997	34.041421
909.190834	53492.940146	34.046439
909.824974	53572.838125	34.051456
910.549424	53644.749185	34.056474
911.227515	53731.658486	34.061492
912.343304	53810.197734	34.066509
912.997092	53909.653431	34.071527
913.725899	53994.347354	34.076544
914.849044	54073.234375	34.081562
915.904219	54158.814631	34.086580
917.039858	54231.207691	34.091597
918.187733	54310.060018	34.096615
919.030511	54398.325666	34.101632
919.987963	54466.393464	34.106650
920.859740	54563.242453	34.111668
921.696308	54636.037687	34.116685
922.622148	54721.405980	34.121703
923.549510	54816.621017	34.126720
925.244312	54895.105398	34.131738
926.048719	54977.721761	34.136756
927.217389	55052.890302	34.141773
927.841051	55125.954334	34.146791
928.723745	55203.192918	34.151808
929.978435	55269.982748	34.156826
930.923849	55350.211672	34.161844
931.900388	55421.886408	34.166861
932.736625	55495.874074	34.171879
933.627113	55567.879067	34.176896
934.819704	55647.266814	34.181914
935.042103	55730.514315	34.186932
935.954354	55803.681069	34.191949
936.779351	55892.455009	34.196967
937.746872	55973.638202	34.201984
938.669133	56058.163851	34.207002
939.679538	56151.093054	34.212020
940.330190	56228.244524	34.217037
941.519936	56311.261206	34.222055
942.609365	56394.781098	34.227072
943.653486	56463.701839	34.232090
944.202269	56550.913757	34.237108
944.907514	56637.025763	34.242125
946.214819	56738.821827	34.247143
947.269630	56822.911861	34.252160
948.310940	56897.935192	34.257178
949.090780	56985.220318	34.262196
950.279435	57070.961187	34.267213
951.142907	57153.784766	34.272231
952.056316	57232.955447	34.277248
953.325350	57310.026811	34.282266
955.251274	57365.351413	34.287284
956.241239	57409.999438	34.292301
957.729003	57471.037857	34.297319
958.413350	57519.587961	34.302336
959.396390	57565.661361	34.307354
960.128989	57619.520456	34.312372
960.841534	57668.819617	34.317389
961.954226	57731.809442	34.322407
962.074291	57794.719772	34.327424
963.260088	57864.862981	34.332442
963.645872	57943.149799	34.337460
964.694385	58014.257838	34.342477
965.393205	58088.464801	34.347495
965.845690	58165.659690	34.352512
966.832772	58250.119702	34.357530
967.704203	58340.806889	34.362548
968.218749	58421.898011	34.367565
969.167158	58506.839629	34.372583
969.803210	58615.121620	34.377600
971.261619	58704.155489	34.382618
971.744796	58808.057000	34.387636
972.772313	58899.342253	34.392653
974.007500	59001.431290	34.397671
974.573686	59105.574328	34.402688
975.886010	59196.031530	34.407706
977.156835	59301.205008	34.412724
978.071777	59404.200057	34.417741
979.080626	59504.111150	34.422759
980.222485	59599.628293	34.427776
981.204454	59689.315929	34.432794
982.405187	59794.698669	34.437812
983.464665	59899.508876	34.442829
984.570946	59993.634277	34.447847
985.149609	60079.765622	34.452864
986.217096	60178.898149	34.457882
987.285767	60278.682847	34.462900
988.242092	60378.491770	34.467917
989.429995	60475.258453	34.472935
990.608588	60570.469860	34.477952
991.737747	60660.600227	34.482970
992.691310	60761.252998	34.487988
993.819456	60862.024593	34.493005
994.838858	60946.159800	34.498023
995.624916	61044.605388	34.503040
996.966558	61134.723414	34.508058
997.616741	61238.571309	34.513076
998.728641	61325.927991	34.518093
1000.446050	61401.796864	34.523111
1002.263555	61474.706967	34.528128
1003.337000	61553.100916	34.533146
1004.214832	61630.044348	34.538164
1005.052510	61700.518678	34.543181
1006.118130	61787.719627	34.548199
1006.858620	61855.380008	34.553216
1007.822992	61938.438414	34.558234
1008.663361	62026.764042	34.563252
1009.217430	62110.678156	34.568269
1010.387770	62188.704560	34.573287
1011.582939	62286.692638	34.578304
1012.240629	62373.484394	34.583322
1013.550870	62462.624666	34.588340
1014.588458	62540.248722	34.593357
1015.360159	62622.896306	34.598375
1016.227043	62714.974098	34.603392
1017.447831	62800.040162	34.608410
1018.537270	62887.867985	34.613428
1018.863355	62985.683926	34.618445
1020.415636	63063.045925	34.623463
1021.749731	63148.848860	34.628480
1022.949013	63214.694362	34.633498
1024.019710	63291.948457	34.638516
1024.543075	63358.304698	34.643533
1026.096423	63425.032549	34.648551
1027.216885	63493.454889	34.653568
1028.177844	63562.497310	34.658586
1028.941931	63631.266704	34.663604
1029.799138	63710.600081	34.668621
1031.110852	63771.688004	34.673639
1031.682451	63859.783454	34.678656
1032.853135	63943.848346	34.683674
1033.745244	64020.448798	34.688692
1034.342822	64101.292528	34.693709
1035.783360	64183.246111	34.698727
1036.426515	64275.218898	34.703744
1037.134554	64350.443608	34.708762
1038.516948	64450.322938	34.713780
1039.471134	64542.052038	34.718797
1040.581801	64625.925983	34.723815
1041.242080	64723.221907	34.728832
1042.406499	64821.655246	34.733850
1043.230523	64919.350605	34.738868
1043.928818	65011.539087	34.743885
1045.703255	65099.223755	34.748903
1046.690548	65210.759431	34.753920
1047.873892	65304.500525	34.758938
1048.809010	65400.084925	34.763956
1049.623359	65506.444797	34.768973
1051.080214	65595.535457	34.773991
1052.054679	65703.992121	34.779008
1053.012790	65793.597954	34.784026
1054.039612	65899.211001	34.789044
1055.533920	66005.859663	34.794061
1056.056195	66099.504017	34.799079
1057.202405	66204.460312	34.804096
1058.621206	66295.427052	34.809114
1059.890790	66398.199688	34.814132
1060.896814	66496.493278	34.819149
1062.023483	66592.457568	34.824167
1062.710914	66697.063122	34.829184
1063.963631	66791.508034	34.834202
1065.276363	66884.557398	34.839220
1066.049008	66986.801963	34.844237
1066.983997	67081.968532	34.849255
1068.246039	67184.897478	34.854272
1069.304289	67281.976681	34.859290
1070.737736	67382.087591	34.864308
1071.766374	67482.977361	34.869325
1073.036263	67579.733507	34.874343
1073.770824	67664.087617	34.879360
1074.969680	67768.839565	34.884378
1075.869201	67868.845547	34.889396
1077.311610	67964.455611	34.894413
1078.458514	68051.095829	34.899431
1079.393322	68158.784015	34.904448
1080.233292	68248.993063	34.909466
1081.793749	68340.673197	34.914484
1082.598575	68443.165512	34.919501
1083.491563	68533.962488	34.924519
1084.540689	68630.123794	34.929536
1085.498931	68739.577324	34.934554
1086.950418	68835.233542	34.939572
1087.722919	68938.809268	34.944589
1088.979071	69037.896831	34.949607
1089.897855	69131.750180	34.954624
1091.094246	69237.774877	34.959642
1092.278886	69332.929936	34.964660
1093.217560	69431.739170	34.969677
1094.957867	69509.952772	34.974695
1095.940867	69588.911357	34.979712
1096.788283	69673.406457	34.984730
1097.901090	69749.818860	34.989748
1098.840164	69846.166460	34.994765
1100.179380	69917.256862	34.999783
1101.146188	70000.284404	35.004800
1102.262872	70092.635061	35.009818
1102.865860	70178.588245	35.014836
1104.056495	70278.235320	35.019853
1105.295623	70372.473889	35.024871
1106.074889	70471.704494	35.029888
1107.153757	70561.510829	35.034906
1108.384901	70659.721980	35.039924
1109.615493	70762.923411	35.044941
1110.562347	70866.182080	35.049959
1111.513166	70967.110250	35.054976
1112.141734	71083.210595	35.059994
1114.073942	71173.031854	35.065012
1115.017655	71272.733831	35.070029
1115.959051	71365.901502	35.075047
1117.106768	71482.340748	35.080064
1117.825592	71593.793965	35.085082
1119.556783	71700.150732	35.090100
1120.557865	71802.961382	35.095117
1122.173492	71902.763810	35.100135
1123.296775	72000.654828	35.105152
1124.498364	72105.740506	35.110170
1125.917062	72203.522971	35.115188
1126.686959	72304.041166	35.120205
1127.836086	72407.907685	35.125223
1129.028940	72506.017730	35.130240
1129.979255	72601.265512	35.135258
1131.231376	72704.686545	35.140276
1132.068199	72818.431693	35.145293
1133.659638	72922.953326	35.150311
1135.188074	73030.550259	35.155328
1136.061738	73128.686969	35.160346
1137.124365	73218.219943	35.165364
1138.455378	73325.608157	35.170381
1139.899609	73424.987057	35.175399
1141.010176	73527.458072	35.180416
1141.801068	73631.689138	35.185434
1143.080577	73726.066442	35.190452
1143.893070	73823.227297	35.195469
1145.109004	73920.959012	35.200487
1146.339620	74028.467022	35.205504
1146.947503	74141.898825	35.210522
1148.617458	74245.716809	35.215540
1149.291854	74355.985286	35.220557
1150.295387	74467.545614	35.225575
1151.602138	74577.640578	35.230592
1152.761729	74681.527031	35.235610
1154.282294	74803.458066	35.240628
1154.922785	74904.614231	35.245645
1155.993687	75018.231008	35.250663
1157.542531	75133.534533	35.255680
1158.584193	75247.612830	35.260698
1159.938717	75353.004210	35.265716
1160.816843	75455.784802	35.270733
1162.461333	75566.920600	35.275751
1163.653063	75673.744593	35.280768
1164.927118	75780.188856	35.285786
1166.213481	75880.095467	35.290804
1167.186857	75998.405675	35.295821
1168.307239	76094.044794	35.300839
1169.728769	76203.596537	35.305856
1170.690765	76299.983064	35.310874
1171.853576	76389.498385	35.315892
1172.739997	76484.402602	35.320909
1173.781076	76586.060081	35.325927
1175.061195	76675.355411	35.330944
1175.860261	76779.445412	35.335962
1177.423411	76872.915578	35.340980
1178.803342	76968.618726	35.345997
1180.014344	77065.057886	35.351015
1181.108650	77168.710731	35.356032
1181.962109	77268.563171	35.361050
1184.223903	77348.270542	35.366068
1185.691927	77436.893077	35.371085
1186.969381	77533.830264	35.376103
1188.034579	77608.049504	35.381120
1188.528594	77697.495887	35.386138
1190.022563	77786.761580	35.391156
1190.766547	77880.730082	35.396173
1191.642192	77989.195878	35.401191
1192.807804	78088.850716	35.406208
1194.118824	78207.346003	35.411226
1195.183192	78294.057935	35.416244
1196.247516	78414.847438	35.421261
1196.986339	78532.090368	35.426279
1198.526342	78648.550343	35.431296
1199.319613	78766.583897	35.436314
1200.575829	78882.531630	35.441332
1201.599004	78996.653867	35.446349
1202.670624	79118.408121	35.451367
1203.884362	79235.491444	35.456384
1205.056343	79375.461220	35.461402
1206.524118	79493.722280	35.466420
1207.819341	79623.361857	35.471437
1209.008290	79740.628539	35.476455
1210.294986	79867.572142	35.481472
1211.205289	79995.081667	35.486490
1212.572228	80118.986071	35.491508
1214.371621	80235.627734	35.496525
1215.934065	80339.321014	35.501543
1217.514603	80456.314395	35.506560
1218.636070	80578.776774	35.511578
1220.076629	80687.595987	35.516596
1221.775980	80796.717412	35.521613
1222.740964	80902.722903	35.526631
1224.438706	81003.496332	35.531648
1225.768844	81105.708306	35.536666
1226.590862	81203.907521	35.541684
1228.083877	81315.039518	35.546701
1229.464077	81412.671144	35.551719
1230.472247	81514.111206	35.556736
1231.322996	81625.863857	35.561754
1232.420275	81725.897158	35.566772
1233.627779	81836.480189	35.571789
1234.771551	81941.625582	35.576807
1236.118867	82061.677381	35.581824
1237.210567	82171.633594	35.586842
1238.821707	82273.806085	35.591860
1240.017820	82384.887170	35.596877
1240.902137	82494.978283	35.601895
1242.768207	82589.358199	35.606912
1243.757578	82713.484892	35.611930
1244.863106	82807.058998	35.616948
1246.347562	82913.662733	35.621965
1247.694746	83020.807715	35.626983
1249.087219	83120.419907	35.632000
1250.322528	83219.486747	35.637018
1251.731548	83333.794691	35.642036
1252.549654	83443.063551	35.647053
1253.589590	83539.729197	35.652071
1254.775310	83633.927073	35.657088
1255.876415	83737.337251	35.662106
1256.758432	83840.997305	35.667124
1257.558518	83936.447242	35.672141
1258.867838	84044.197495	35.677159
1259.755989	84163.151291	35.682176
1261.188921	84273.227255	35.687194
1262.440092	84394.076809	35.692212
1263.423524	84517.388688	35.697229
1264.613976	84627.199655	35.702247
1265.936706	84755.553467	35.707264
1267.060718	84876.095399	35.712282
1268.452535	84994.087273	35.717300
1269.647693	85115.202004	35.722317
1271.106465	85252.051881	35.727335
1272.701862	85363.487904	35.732352
1273.732156	85480.955167	35.737370
1275.027750	85604.337160	35.742388
1276.636790	85735.881981	35.747405
1277.740680	85855.493456	35.752423
1279.373640	85980.117034	35.757440
1280.768217	86097.504759	35.762458
1282.302257	86219.952581	35.767476
1283.598822	86332.047093	35.772493
1283.982597	86460.934789	35.777511
1285.704051	86591.110118	35.782528
1287.091249	86711.732787	35.787546
1288.338725	86830.426229	35.792564
1289.908254	86964.631201	35.797581
1290.845712	87084.666474	35.802599
1292.542041	87206.269507	35.807616
1293.610726	87334.953082	35.812634
1294.915464	87462.269903	35.817652
1296.500963	87586.160089	35.822669
1297.688755	87724.090244	35.827687
1299.353327	87844.788469	35.832704
1300.490789	87971.107076	35.837722
1301.520144	88089.041214	35.842740
1302.657720	88216.450689	35.847757
1303.584528	88353.613379	35.852775
1305.415850	88483.437869	35.857792
1306.849661	88613.540239	35.862810
1308.187488	88738.551010	35.867828
1309.442479	88868.745701	35.872845
1310.907892	89002.836796	35.877863
1312.312068	89124.303147	35.882880
1313.376541	89262.500478	35.887898
1315.069414	89390.132733	35.892916
1316.613299	89511.528233	35.897933
1317.718779	89643.929367	35.902951
1319.083271	89757.940021	35.907968
1320.525361	89889.339367	35.912986
1321.629339	90020.918651	35.918004
1323.499254	90144.483811	35.923021
1324.322142	90266.349465	35.928039
1325.760288	90391.516331	35.933056
1327.011429	90507.271080	35.938074
1328.507852	90638.576551	35.943092
1329.850421	90760.008467	35.948109
1331.135314	90892.235126	35.953127
1332.777317	91007.449371	35.958144
1333.785074	91132.787713	35.963162
1334.854620	91266.253542	35.968180
1336.040904	91384.024228	35.973197
1337.624726	91516.270472	35.978215
1338.938420	91647.380661	35.983232
1340.378287	91776.646723	35.988250
1341.391103	91904.864489	35.993268
1343.190871	92012.022657	35.998285
1344.346844	92128.977149	36.003303
1345.532679	92237.866644	36.008320
1346.773612	92354.073675	36.013338
1347.824186	92464.087696	36.018356
1349.290794	92583.479754	36.023373
1350.440891	92700.209223	36.028391
1352.040234	92829.632394	36.033408
1352.953675	92954.435281	36.038426
1354.392432	93083.124053	36.043444
1355.746495	93203.030366	36.048461
1356.936376	93343.571715	36.053479
1358.741732	93464.815701	36.058496
1359.578933	93597.973051	36.063514
1360.840355	93733.650616	36.068532
1362.346581	93854.930031	36.073549
1363.620515	94003.928150	36.078567
1365.314700	94147.918326	36.083584
1366.842233	94279.171330	36.088602
1367.863081	94399.362335	36.093620
1370.359353	94521.149385	36.098637
1371.672375	94648.900983	36.103655
1373.047285	94771.700125	36.108672
1374.528644	94904.167124	36.113690
1375.704418	95033.133152	36.118708
1377.261884	95151.608437	36.123725
1378.401489	95297.414151	36.128743
1379.672703	95420.219328	36.133760
1381.319067	95552.523984	36.138778
1382.302720	95687.860424	36.143796
1383.979580	95816.472847	36.148813
1385.060900	95948.499540	36.153831
1386.663434	96093.222867	36.158848
1388.056700	96234.202032	36.163866
1389.640503	96362.628376	36.168884
1390.861933	96497.335547	36.173901
1392.069438	96637.952489	36.178919
1393.478930	96772.821712	36.183936
1395.038697	96916.262540	36.188954
1396.077793	97057.528702	36.193972
1397.876472	97193.302544	36.198989
1398.992156	97335.977773	36.204007
1400.926546	97466.445653	36.209024
1401.931812	97608.708305	36.214042
1403.196985	97751.235379	36.219060
1404.980219	97886.608960	36.224077
1406.297429	98026.276955	36.229095
1407.997385	98169.828425	36.234112
1409.215888	98313.214624	36.239130
1410.340649	98443.901284	36.244148
1412.042485	98585.489444	36.249165
1413.034961	98740.537374	36.254183
1414.845789	98882.908533	36.259200
1416.088404	99025.089875	36.264218
1417.254485	99165.356852	36.269236
1419.209015	99301.128131	36.274253
1420.882154	99457.645554	36.279271
1422.152683	99588.859326	36.284288
1423.747017	99732.535681	36.289306
1424.628087	99873.281141	36.294324
1426.287293	100003.079636	36.299341
1427.633276	100148.368495	36.304359
1429.015091	100293.918658	36.309376
1430.754093	100437.727770	36.314394
1432.154382	100573.501944	36.319412
1433.643034	100712.128080	36.324429
1434.888018	100845.087774	36.329447
1436.410988	100974.543723	36.334464
1437.776691	101109.818417	36.339482
1439.207547	101239.251725	36.344500
1440.855008	101349.736425	36.349517
1441.880835	101475.430348	36.354535
1443.652830	101602.149637	36.359552
1444.886025	101719.203874	36.364570
1446.602396	101850.864540	36.369588
1447.859999	101967.370710	36.374605
1449.683205	102098.572010	36.379623
1451.048612	102217.407754	36.384640
1452.742846	102336.180070	36.389658
1453.984344	102468.183373	36.394676
1455.693580	102590.592952	36.399693
1456.791751	102728.083982	36.404711
1458.346394	102848.806997	36.409728
1460.021144	102972.656031	36.414746
1461.504713	103093.467076	36.419764
1463.279199	103206.093620	36.424781
1464.970669	103328.026917	36.429799
1466.459871	103454.011292	36.434816
1467.833865	103573.142199	36.439834
1468.831163	103699.774614	36.444852
1470.264086	103843.202568	36.449869
1471.769080	103974.296035	36.454887
1473.077805	104114.650840	36.459904
1474.305314	104252.508435	36.464922
1475.203473	104395.311976	36.469940
1476.645901	104537.055123	36.474957
1478.036323	104682.052830	36.479975
1479.042125	104833.564753	36.484992
1480.504934	104988.442312	36.490010
1481.791383	105157.967315	36.495028
1483.923744	105315.404832	36.500045
1485.247382	105479.942665	36.505063
1486.451825	105642.128781	36.510080
1488.258888	105800.329249	36.515098
1489.998990	105967.581468	36.520116
1491.435925	106119.247621	36.525133
1492.630685	106276.759478	36.530151
1494.634200	106432.409051	36.535168
1496.226271	106591.318707	36.540186
1497.572314	106751.281793	36.545204
1499.215157	106909.918755	36.550221
1500.732401	107069.958130	36.555239
1501.778354	107220.244520	36.560256
1503.455980	107379.601016	36.565274
1504.592793	107551.938225	36.570292
1506.349831	107718.790638	36.575309
1508.176066	107880.383424	36.580327
1509.802692	108042.350409	36.585344
1511.559015	108199.098975	36.590362
1513.022083	108358.277837	36.595380
1514.748360	108519.610208	36.600397
1516.117214	108679.451923	36.605415
1517.830127	108837.414803	36.610432
1519.492941	108983.174627	36.615450
1520.842067	109147.650049	36.620468
1522.392699	109291.665993	36.625485
1523.994184	109444.284968	36.630503
1525.316459	109608.677980	36.635520
1527.163981	109747.881550	36.640538
1528.524468	109917.748278	36.645556
1530.196596	110070.485805	36.650573
1531.605450	110217.761330	36.655591
1533.149881	110369.619670	36.660608
1534.622580	110528.401149	36.665626
1535.925738	110675.175108	36.670644
1538.433553	110807.990157	36.675661
1540.287378	110931.396396	36.680679
1541.851415	111061.417193	36.685696
1543.697309	111180.501143	36.690714
1545.047470	111305.344007	36.695732
1546.011792	111431.553574	36.700749
1547.448934	111561.266235	36.705767
1548.872866	111695.445398	36.710784
1550.572976	111829.632809	36.715802
1551.642170	111969.334068	36.720820
1552.969644	112098.304847	36.725837
1554.329157	112243.782978	36.730855
1555.496792	112400.781446	36.735872
1557.299305	112546.572320	36.740890
1558.648728	112696.784265	36.745908
1560.216073	112851.947005	36.750925
1561.683022	113010.157087	36.755943
1562.950557	113185.469228	36.760960
1564.551700	113338.168445	36.765978
1565.904879	113511.566493	36.770996
1567.638030	113675.204168	36.776013
1569.270683	113841.229850	36.781031
1570.736051	114010.503699	36.786048
1572.442918	114179.829528	36.791066
1574.213743	114349.247653	36.796084
1575.682948	114509.632678	36.801101
1578.011583	114669.618305	36.806119
1579.699717	114826.127764	36.811136
1581.283601	114985.621915	36.816154
1583.118107	115144.621167	36.821172
1585.232075	115293.722922	36.826189
1586.987655	115446.039143	36.831207
1588.072361	115613.312330	36.836224
1590.015124	115767.084671	36.841242
1591.395170	115925.473144	36.846260
1593.076776	116090.106263	36.851277
1594.898216	116235.388963	36.856295
1596.014463	116394.835170	36.861312
1597.163432	116540.134946	36.866330
1598.759991	116712.926829	36.871348
1600.418143	116891.848766	36.876365
1602.265175	117057.627316	36.881383
1603.807045	117220.080246	36.886400
1605.558799	117376.083257	36.891418
1607.547666	117545.748481	36.896436
1609.166285	117706.923202	36.901453
1610.524665	117863.674395	36.906471
1612.262733	118037.693396	36.911488
1613.728236	118194.441977	36.916506
1615.394640	118361.865273	36.921524
1616.835414	118522.005703	36.926541
1618.512080	118693.525834	36.931559
1619.695304	118862.396436	36.936576
1621.349315	119035.316901	36.941594
1623.328069	119207.439235	36.946612
1624.502029	119378.089374	36.951629
1626.556464	119547.613851	36.956647
1627.604600	119731.603816	36.961664
1629.709967	119892.433015	36.966682
1631.302667	120077.380017	36.971700
1632.925826	120243.676703	36.976717
1634.415184	120416.400718	36.981735
1635.950965	120583.372077	36.986752
1637.976677	120758.005655	36.991770
1639.983265	120912.309119	36.996788
1641.294264	121082.805965	37.001805
1643.520217	121239.841911	37.006823
1644.891107	121420.783359	37.011840
1646.467631	121570.234577	37.016858
1647.791986	121725.751063	37.021876
1648.964197	121886.847968	37.026893
1650.960542	122035.144700	37.031911
1652.738051	122191.378996	37.036928
1654.085969	122346.412243	37.041946
1655.232089	122500.285082	37.046964
1656.504423	122676.769734	37.051981
1658.372341	122829.034634	37.056999
1659.483862	123014.222715	37.062016
1660.871984	123199.305185	37.067034
1662.592878	123384.463585	37.072052
1664.226301	123568.279089	37.077069
1665.964441	123747.030196	37.082087
1667.544322	123944.010950	37.087104
1669.126686	124122.686501	37.092122
1670.519132	124308.750278	37.097140
1672.069471	124513.591062	37.102157
1673.915000	124714.390824	37.107175
1675.648032	124904.400482	37.112192
1677.809951	125098.911327	37.117210
1680.240418	125292.264921	37.122228
1681.750588	125485.775363	37.127245
1684.038130	125667.164396	37.132263
1685.646214	125855.903963	37.137280
1687.374568	126029.186189	37.142298
1689.490185	126213.090978	37.147316
1691.311576	126390.508773	37.152333
1692.998010	126559.778117	37.157351
1694.455245	126748.557981	37.162368
1695.986569	126930.171828	37.167386
1697.425957	127116.317307	37.172404
1698.909637	127307.036712	37.177421
1700.606221	127502.278486	37.182439
1702.353209	127698.502927	37.187456
1704.133297	127886.336976	37.192474
1705.865723	128091.484572	37.197492
1707.227962	128294.533969	37.202509
1708.929694	128490.845322	37.207527
1710.390806	128700.580190	37.212544
1711.786664	128900.277842	37.217562
1713.830079	129107.107514	37.222580
1715.280157	129317.430808	37.227597
1716.861410	129539.242384	37.232615
1718.269184	129756.603380	37.237632
1720.076634	129973.243527	37.242650
1721.741490	130188.346376	37.247668
1723.371142	130411.360325	37.252685
1725.308710	130625.306408	37.257703
1727.399578	130850.509322	37.262720
1729.254238	131057.428640	37.267738
1731.399300	131280.849056	37.272756
1732.634506	131498.575681	37.277773
1734.991272	131702.311355	37.282791
1736.476462	131924.251780	37.287808
1737.952842	132145.725245	37.292826
1740.030004	132360.241894	37.297844
1741.673926	132576.172011	37.302861
1743.541175	132783.643240	37.307879
1745.351686	133000.260087	37.312896
1747.193201	133203.638892	37.317914
1749.166814	133424.483158	37.322932
1750.755132	133631.456197	37.327949
1752.588070	133844.330521	37.332967
1754.117402	134050.299597	37.337984
1756.070265	134248.095458	37.343002
1757.761879	134468.557407	37.348020
1759.506600	134688.504620	37.353037
1761.569249	134885.943625	37.358055
1762.856982	135083.136122	37.363072
1764.531893	135279.761657	37.368090
1766.331277	135472.460369	37.373108
1767.948101	135667.142485	37.378125
1769.687649	135849.319942	37.383143
1771.669457	136047.779102	37.388160
1774.174516	136231.526660	37.393178
1776.112307	136431.415580	37.398196
1777.927115	136602.975860	37.403213
1779.237391	136792.406253	37.408231
1781.541720	136973.637425	37.413248
1783.890382	137149.075871	37.418266
1785.613908	137332.962198	37.423284
1787.411453	137523.271516	37.428301
1789.070936	137700.291359	37.433319
1790.817460	137896.942443	37.438336
1792.184060	138081.750229	37.443354
1793.910749	138271.972141	37.448372
1795.331778	138475.655895	37.453389
1796.864395	138681.366296	37.458407
1798.766974	138885.712927	37.463424
1800.258455	139100.847756	37.468442
1801.440184	139312.148523	37.473460
1803.000867	139528.264389	37.478477
1804.460936	139758.838692	37.483495
1806.457850	139992.097109	37.488512
1807.930426	140223.598142	37.493530
1809.433964	140447.557216	37.498548
1811.218104	140710.434270	37.503565
1813.006564	140950.468621	37.508583
1814.979919	141200.399668	37.513600
1816.509412	141443.751039	37.518618
1818.605987	141686.330065	37.523636
1820.670535	141927.430439	37.528653
1822.455861	142171.329446	37.533671
1824.449739	142423.129220	37.538688
1826.547441	142670.967152	37.543706
1829.049382	142893.462298	37.548724
1831.165347	143131.197424	37.553741
1833.060167	143367.724356	37.558759
1835.044981	143606.383281	37.563776
1836.555612	143839.900923	37.568794
1838.585339	144067.767249	37.573812
1840.313181	144309.617076	37.578829
1842.171496	144548.147914	37.583847
1843.981175	144795.533651	37.588864
1845.433755	145033.114599	37.593882
1847.205434	145283.212018	37.598900
1848.963580	145534.950050	37.603917
1850.813070	145775.772638	37.608935
1852.485190	146023.579253	37.613952
1854.045460	146275.478672	37.618970
1856.268940	146533.495312	37.623988
1858.197804	146788.754102	37.629005
1859.998758	147034.920945	37.634023
1861.903125	147291.785278	37.639040
1863.493472	147554.462151	37.644058
1865.639825	147798.662300	37.649076
1867.607911	148052.486956	37.654093
1869.815416	148294.014456	37.659111
1871.605214	148555.383362	37.664128
1873.792150	148796.281736	37.669146
1876.003630	149035.184611	37.674164
1877.761859	149283.856491	37.679181
1879.405585	149517.303097	37.684199
1881.493437	149768.819939	37.689216
1882.900072	150007.827057	37.694234
1884.884916	150258.283317	37.699252
1886.910282	150489.885032	37.704269
1888.281851	150723.582335	37.709287
1890.039381	150964.392297	37.714304
1891.922220	151204.079501	37.719322
1893.835144	151428.518278	37.724340
1895.237182	151679.071804	37.729357
1896.879980	151918.139435	37.734375
1898.662156	152168.521786	37.739392
1900.470082	152415.347044	37.744410
1902.085339	152662.114532	37.749428
1904.116849	152918.922564	37.754445
1906.096347	153177.504313	37.759463
1907.789256	153449.054229	37.764480
1909.157342	153713.775894	37.769498
1911.444881	153977.936799	37.774516
1913.469465	154264.341775	37.779533
1914.777596	154538.990691	37.784551
1917.017198	154806.793430	37.789568
1918.410987	155095.357206	37.794586
1920.955620	155372.610409	37.799604
1923.022116	155647.920954	37.804621
1924.767947	155923.155769	37.809639
1927.051510	156201.697624	37.814656
1928.638898	156484.386022	37.819674
1931.050631	156767.848804	37.824692
1932.898187	157059.944270	37.829709
1934.917635	157336.374511	37.834727
1936.957092	157624.202850	37.839744
1938.585451	157907.577189	37.844762
1940.750583	158204.452889	37.849780
1942.831803	158493.497616	37.854797
1944.822686	158784.106580	37.859815
1946.501862	159067.440375	37.864832
1948.390225	159366.307196	37.869850
1950.469784	159652.374326	37.874868
1952.161261	159963.017773	37.879885
1954.367857	160254.564984	37.884903
1956.665500	160554.465667	37.889920
1958.528751	160851.959782	37.894938
1960.575708	161143.015480	37.899956
1962.296972	161437.017806	37.904973
1964.326795	161732.204955	37.909991
1966.802031	162035.525578	37.915008
1968.611484	162331.587720	37.920026
1971.178213	162621.287030	37.925044
1973.128779	162904.202375	37.930061
1974.813716	163201.582875	37.935079
1977.288000	163485.930067	37.940096
1979.082688	163785.390989	37.945114
1981.122254	164075.280395	37.950132
1983.069799	164364.880690	37.955149
1985.298992	164646.084310	37.960167
1987.582217	164928.524945	37.965184
1989.451195	165211.742238	37.970202
1991.832572	165483.657388	37.975220
1993.788656	165778.429903	37.980237
1995.930257	166054.142807	37.985255
1997.834926	166332.217166	37.990272
1999.586255	166627.685444	37.995290
2001.568022	166899.757319	38.000308
2003.863700	167184.465399	38.005325
2005.608072	167471.507770	38.010343
2007.525764	167756.124656	38.015360
2008.893447	168035.698773	38.020378
2010.977449	168322.018837	38.025396
2013.049515	168605.053411	38.030413
2014.756268	168913.527255	38.035431
2017.169042	169194.555805	38.040448
2018.705894	169480.140366	38.045466
2020.206874	169743.346573	38.050484
2022.170231	170026.771884	38.055501
2023.743971	170314.245866	38.060519
2025.929142	170597.664262	38.065536
2027.739394	170897.623245	38.070554
2029.498079	171191.052311	38.075572
2031.149810	171494.136537	38.080589
2032.827535	171800.976401	38.085607
2035.067886	172117.215021	38.090624
2036.999168	172433.579246	38.095642
2038.797258	172745.559428	38.100660
2040.708094	173064.024556	38.105677
2043.042503	173384.977328	38.110695
2044.904805	173702.119371	38.115712
2046.754261	174039.378116	38.120730
2048.770656	174362.860482	38.125748
2050.953305	174701.593954	38.130765
2052.600514	175036.145661	38.135783
2054.798485	175372.403478	38.140800
2057.293244	175725.924059	38.145818
2059.036893	176075.918695	38.150836
2061.230824	176414.797282	38.155853
2062.825838	176765.376711	38.160871
2065.324613	177105.467817	38.165888
2067.664413	177456.873923	38.170906
2069.567865	177804.539871	38.175924
2071.999028	178160.810892	38.180941
2074.150853	178512.936351	38.185959
2076.220777	178851.793255	38.190976
2078.484091	179206.545501	38.195994
2080.144341	179556.135778	38.201012
2082.960252	179916.925675	38.206029
2084.783553	180272.284045	38.211047
2086.914012	180626.402333	38.216064
2089.317418	180982.485961	38.221082
2091.173260	181323.874617	38.226100
2094.156084	181668.721070	38.231117
2095.898342	182023.514756	38.236135
2098.138330	182364.923677	38.241152
2100.350463	182712.840141	38.246170
2102.427536	183072.563758	38.251188
2104.944704	183423.178383	38.256205
2107.034215	183771.092400	38.261223
2108.829922	184125.961829	38.266240
2111.002812	184478.310168	38.271258
2113.103032	184835.192073	38.276276
2115.072075	185183.993415	38.281293
2117.234256	185525.070008	38.286311
2119.042112	185951.772533	38.291328
2121.312942	186321.510515	38.296346
2123.277297	186678.572465	38.301364
2125.343914	187040.725005	38.306381
2127.088750	187410.421722	38.311399
2129.382936	187772.973152	38.316416
2131.494427	188140.151583	38.321434
2133.519984	188515.040758	38.326452
2135.716950	188878.601621	38.331469
2137.521132	189252.968976	38.336487
2139.487138	189617.889006	38.341504
2141.793918	190003.534455	38.346522
2144.044689	190370.749407	38.351540
2146.644099	190744.718542	38.356557
2148.523769	191121.315529	38.361575
2150.655565	191492.413398	38.366592
2152.453703	191861.887923	38.371610
2154.744347	192243.834821	38.376628
2156.809727	192603.135202	38.381645
2158.792991	192978.045459	38.386663
2160.826826	193335.701839	38.391680
2162.990171	193691.535623	38.396698
2165.020834	194043.961929	38.401716
2167.651682	194387.202240	38.406733
2169.421903	194753.641576	38.411751
2172.205464	195110.119390	38.416768
2174.258795	195466.254586	38.421786
2177.068619	195799.742063	38.426804
2179.663759	196146.015245	38.431821
2181.830200	196509.070147	38.436839
2183.669089	196855.589813	38.441856
2185.879994	197207.615373	38.446874
2187.546413	197568.058268	38.451892
2189.873234	197929.974191	38.456909
2191.665564	198296.292487	38.461927
2193.546993	198670.319970	38.466944
2195.633427	199046.755059	38.471962
2197.899977	199426.109673	38.476980
2200.148497	199800.946475	38.481997
2202.492917	200179.427146	38.487015
2205.026198	200554.602457	38.492032
2207.431228	200929.569984	38.497050
2209.637897	201316.584490	38.502068
2211.803249	201695.071165	38.507085
2213.773175	202076.688189	38.512103
2216.556988	202456.909281	38.517120
2219.060894	202828.537935	38.522138
2221.369376	203206.751629	38.527156
2224.098477	203580.328200	38.532173
2226.166425	203957.259961	38.537191
2228.284852	204329.256518	38.542208
2230.501456	204706.852524	38.547226
2232.839232	205091.619391	38.552244
2235.187270	205468.891592	38.557261
2237.067445	205865.797510	38.562279
2239.307628	206238.388410	38.567296
2241.488103	206631.006788	38.572314
2243.469028	207026.298861	38.577332
2245.470169	207417.955878	38.582349
2247.794619	207807.276997	38.587367
2249.985332	208199.083705	38.592384
2252.418193	208599.998534	38.597402
2254.622814	208996.097553	38.602420
2256.861595	209387.492306	38.607437
2259.254703	209793.724585	38.612455
2261.426860	210190.922914	38.617472
2263.516091	210588.846051	38.622490
2266.060008	210995.463196	38.627508
2268.475244	211388.383114	38.632525
2270.594841	211806.168788	38.637543
2272.849908	212216.846402	38.642560
2274.793309	212628.208176	38.647578
2276.838732	213041.840945	38.652596
2278.757323	213455.773432	38.657613
2280.950152	213885.185392	38.662631
2282.964190	214300.755311	38.667648
2285.189036	214730.239551	38.672666
2287.164651	215175.615017	38.677684
2289.490409	215601.883687	38.682701
2291.931808	216034.358750	38.687719
2293.753770	216467.159300	38.692736
2296.107681	216918.600134	38.697754
2298.517563	217358.067483	38.702772
2300.980743	217800.422987	38.707789
2303.186153	218240.253201	38.712807
2305.574918	218674.999861	38.717824
2308.052201	219100.155790	38.722842
2311.360453	219504.402253	38.727860
2313.997564	219893.790473	38.732877
2316.205051	220296.049393	38.737895
2318.235464	220694.804935	38.742912
2320.732168	221088.381905	38.747930
2322.823459	221485.731141	38.752948
2325.463668	221883.960476	38.757965
2327.515275	222291.147586	38.762983
2330.023596	222686.831938	38.768000
2331.718019	223091.305866	38.773018
2334.031985	223505.108404	38.778036
2336.353717	223919.875191	38.783053
2338.416250	224341.363675	38.788071
2340.883809	224762.636772	38.793088
2343.145925	225189.530793	38.798106
2345.322829	225614.736033	38.803124
2348.057811	226023.062327	38.808141
2350.748533	226453.801919	38.813159
2353.097995	226873.670834	38.818176
2355.146760	227307.507947	38.823194
2357.541545	227746.295752	38.828212
2360.539846	228174.319834	38.833229
2363.047744	228586.898244	38.838247
2365.318763	229024.231565	38.843264
2367.825771	229449.105431	38.848282
2370.073738	229884.638347	38.853300
2372.810296	230319.536153	38.858317
2374.630792	230755.643286	38.863335
2376.867942	231194.810046	38.868352
2379.463163	231631.786897	38.873370
2381.328557	232074.719975	38.878388
2383.585956	232519.420837	38.883405
2385.968977	232969.081004	38.888423
2388.615721	233419.233262	38.893440
2391.326212	233866.148931	38.898458
2393.665373	234326.281210	38.903476
2396.190825	234779.956886	38.908493
2398.492040	235235.623107	38.913511
2400.764215	235692.309526	38.918528
2403.218845	236143.733875	38.923546
2405.557976	236608.563461	38.928564
2408.695557	237046.924573	38.933581
2411.605478	237485.041150	38.938599
2414.299117	237945.571458	38.943616
2416.784467	238384.819923	38.948634
2419.005557	238833.787688	38.953652
2421.341872	239281.288882	38.958669
2423.395276	239732.516957	38.963687
2425.618080	240195.098734	38.968704
2428.083211	240637.446328	38.973722
2430.613500	241090.198464	38.978740
2433.113832	241553.598500	38.983757
2435.278966	242005.821623	38.988775
2437.437719	242465.665908	38.993792
2439.887610	242931.459183	38.998810
2441.915737	243409.866345	39.003828
2444.408156	243872.094711	39.008845
2446.762961	244342.574139	39.013863
2448.774117	244826.950677	39.018880
2451.511099	245292.364199	39.023898
2454.018614	245778.769774	39.028916
2455.862356	246259.231628	39.033933
2458.763859	246744.684479	39.038951
2460.864899	247227.466403	39.043968
2463.906410	247693.208007	39.048986
2466.562214	248179.889382	39.054004
2469.248614	248654.803352	39.059021
2471.316201	249134.613425	39.064039
2473.252154	249598.972641	39.069056
2476.039430	250048.083760	39.074074
2478.150980	250509.390302	39.079092
2480.505171	250972.029518	39.084109
2483.099533	251427.974701	39.089127
2485.323092	251887.939003	39.094144
2487.796364	252342.909722	39.099162
2490.469308	252818.525135	39.104180
2492.723063	253297.938353	39.109197
2495.192124	253774.522338	39.114215
2497.515988	254252.372047	39.119232
2500.120876	254729.312787	39.124250
2502.248591	255223.802365	39.129268
2504.615702	255717.516294	39.134285
2506.874910	256213.226534	39.139303
2509.174511	256714.796330	39.144320
2511.807958	257219.817620	39.149338
2513.754170	257737.288768	39.154356
2516.673694	258240.940703	39.159373
2518.966322	258761.909895	39.164391
2521.615054	259291.203696	39.169408
2524.110667	259812.467070	39.174426
2526.827830	260340.145415	39.179444
2529.588609	260852.549043	39.184461
2532.275930	261382.919790	39.189479
2534.804261	261910.925230	39.194496
2537.802245	262431.539936	39.199514
2540.545901	262954.274584	39.204532
2543.106204	263488.719153	39.209549
2545.919647	264014.943033	39.214567
2548.747536	264555.665173	39.219584
2551.332785	265071.632558	39.224602
2553.839830	265600.309163	39.229620
2556.349566	266132.335309	39.234637
2558.845020	266654.023522	39.239655
2561.059884	267191.296754	39.244672
2564.597036	267712.791908	39.249690
2567.035063	268230.899530	39.254708
2570.606402	268749.208977	39.259725
2573.176853	269264.217200	39.264743
2575.768122	269780.971837	39.269760
2578.535368	270287.130660	39.274778
2580.890498	270800.767000	39.279796
2583.313458	271321.729816	39.284813
2585.849362	271848.157906	39.289831
2588.048688	272381.670332	39.294848
2590.761268	272893.588188	39.299866
2593.220321	273429.263358	39.304884
2596.024014	273957.491050	39.309901
2598.817565	274481.831331	39.314919
2600.988908	275017.922210	39.319936
2603.743534	275554.426791	39.324954
2606.302258	276074.780929	39.329972
2608.843287	276604.607244	39.334989
2611.716488	277136.384659	39.340007
2614.063274	277673.649744	39.345024
2616.519166	278205.027807	39.350042
2619.032627	278753.027296	39.355060
2621.912043	279280.497381	39.360077
2624.532956	279817.349441	39.365095
2626.993542	280344.826535	39.370112
2629.577482	280876.927954	39.375130
2632.362890	281418.593337	39.380148
2635.166385	281958.829831	39.385165
2637.822942	282496.698134	39.390183
2640.899460	283036.071495	39.395200
2643.761294	283556.073354	39.400218
2646.179175	284077.638702	39.405236
2649.270982	284562.452620	39.410253
2651.820671	285067.509743	39.415271
2654.100784	285559.807028	39.420288
2656.502024	286065.540133	39.425306
2659.329018	286558.659236	39.430324
2661.592533	287062.679607	39.435341
2663.679083	287568.856663	39.440359
2666.593851	288087.698571	39.445376
2668.661845	288607.709217	39.450394
2671.593104	289115.393361	39.455412
2674.288264	289642.991780	39.460429
2676.639600	290156.344073	39.465447
2678.706051	290696.143251	39.470464
2681.513917	291247.273688	39.475482
2683.802794	291791.269093	39.480500
2686.676390	292349.768195	39.485517
2689.242124	292905.263308	39.490535
2691.361445	293471.359638	39.495552
2694.411441	294034.386019	39.500570
2696.624574	294614.929095	39.505588
2698.655750	295195.418645	39.510605
2701.216409	295777.013355	39.515623
2703.978040	296392.718749	39.520640
2706.774716	296974.823296	39.525658
2710.024923	297585.209908	39.530676
2712.554548	298189.329756	39.535693
2715.422061	298786.053542	39.540711
2718.646604	299390.001564	39.545728
2721.595710	299981.495453	39.550746
2724.751745	300580.516041	39.555764
2727.574341	301180.775113	39.560781
2730.522574	301768.238720	39.565799
2733.323807	302361.125986	39.570816
2736.108376	302961.421862	39.575834
2739.255024	303558.912965	39.580852
2741.662555	304160.116968	39.585869
2744.967924	304755.056586	39.590887
2747.615407	305349.863277	39.595904
2750.274482	305949.306576	39.600922
2753.387703	306533.517968	39.605940
2756.138027	307138.771313	39.610957
2759.293329	307727.455203	39.615975
2762.055301	308320.863815	39.620992
2765.224601	308905.165687	39.626010
2768.158988	309495.538169	39.631028
2770.452993	310083.541099	39.636045
2773.650706	310683.274919	39.641063
2776.339014	311274.450841	39.646080
2778.940215	311859.566910	39.651098
2781.662804	312442.169550	39.656116
2784.315590	313039.598058	39.661133
2787.631407	313625.596199	39.666151
2790.264476	314214.941816	39.671168
2793.089855	314815.163177	39.676186
2795.765406	315420.298178	39.681204
2798.335362	316009.503649	39.686221
2801.447933	316601.865456	39.691239
2803.689196	317205.166150	39.696256
2806.698824	317796.335401	39.701274
2809.717761	318385.465121	39.706292
2812.242371	318996.386738	39.711309
2815.400291	319594.792019	39.716327
2817.827924	320194.292392	39.721344
2820.300112	320794.944817	39.726362
2823.771905	321401.599589	39.731380
2826.450112	322004.943552	39.736397
2829.488806	322593.378441	39.741415
2832.224574	323188.449666	39.746432
2835.058719	323767.257565	39.751450
2837.646730	324325.821915	39.756468
2839.945364	324909.848132	39.761485
2843.343031	325462.536660	39.766503
2845.622913	326035.639260	39.771520
2848.580395	326602.386691	39.776538
2851.653840	327193.186354	39.781556
2854.128604	327771.409958	39.786573
2856.996609	328330.890606	39.791591
2860.056618	328934.098651	39.796608
2862.635562	329516.720596	39.801626
2865.165392	330108.297276	39.806644
2867.947101	330716.671445	39.811661
2870.787618	331310.743884	39.816679
2873.456364	331911.861172	39.821696
2875.954006	332523.878873	39.826714
2879.030781	333150.586381	39.831732
2880.937437	333780.509782	39.836749
2883.889903	334418.301419	39.841767
2887.008247	335054.103137	39.846784
2890.523895	335684.023234	39.851802
2893.347472	336322.233601	39.856820
2896.495402	336965.125838	39.861837
2899.340194	337596.664953	39.866855
2902.330177	338230.301178	39.871872
2904.998853	338878.484762	39.876890
2908.376998	339523.806975	39.881908
2911.071735	340177.314860	39.886925
2913.879796	340822.042878	39.891943
2916.902615	341484.200537	39.896960
2920.016551	342141.233787	39.901978
2923.177303	342793.251186	39.906996
2925.886382	343454.101605	39.912013
2929.017192	344113.276060	39.917031
2932.326894	344763.610080	39.922048
2935.100928	345429.332337	39.927066
2938.298721	346074.612219	39.932084
2941.254137	346743.095352	39.937101
2944.105618	347399.992700	39.942119
2946.974033	348071.708763	39.947136
2950.097487	348740.252657	39.952154
2953.474942	349397.307677	39.957172
2956.084258	350056.396188	39.962189
2959.187876	350725.004301	39.967207
2962.413999	351393.452854	39.972224
2965.180459	352057.902415	39.977242
2968.401436	352720.365995	39.982260
2971.082380	353392.863863	39.987277
2974.203193	354054.504078	39.992295
2977.379568	354723.169834	39.997312
2980.040399	355388.428434	40.002330
2983.503855	356053.395930	40.007348
2986.175623	356735.153322	40.012365
2988.976499	357401.817595	40.017383
2992.294053	358084.636271	40.022400
2994.746002	358765.343757	40.027418
2998.099057	359431.193680	40.032436
3001.546595	360099.168915	40.037453
3004.661565	360772.681573	40.042471
3008.002875	361438.945426	40.047488
3011.146749	362109.559422	40.052506
3014.593045	362750.127190	40.057524
3017.750114	363404.995528	40.062541
3021.008974	364048.250980	40.067559
3024.107379	364694.786725	40.072576
3026.918392	365350.172478	40.077594
3029.964397	365996.662206	40.082612
3032.563753	366635.376206	40.087629
3035.430583	367254.926653	40.092647
3038.324700	367867.744032	40.097664
3040.852616	368493.301022	40.102682
3044.035411	369121.073669	40.107700
3046.850788	369741.439718	40.112717
3050.114910	370348.292554	40.117735
3053.196586	370970.237146	40.122752
3055.915248	371608.922164	40.127770
3058.556894	372238.483051	40.132788
3061.289141	372877.947604	40.137805
3064.209514	373528.516036	40.142823
3067.116633	374184.847669	40.147840
3069.602561	374856.987505	40.152858
3073.082675	375518.948963	40.157876
3075.565641	376204.128514	40.162893
3078.294871	376883.147077	40.167911
3081.541629	377568.401077	40.172928
3084.769333	378259.745464	40.177946
3088.099206	378936.186601	40.182964
3091.203924	379637.520096	40.187981
3094.087551	380335.627140	40.192999
3097.068384	381040.032800	40.198016
3100.035708	381755.920718	40.203034
3103.624138	382471.641640	40.208052
3106.480609	383191.458366	40.213069
3109.481229	383904.470432	40.218087
3112.773780	384625.192244	40.223104
3115.687525	385353.220930	40.228122
3118.602804	386088.699180	40.233140
3121.572826	386838.126094	40.238157
3125.045910	387569.979771	40.243175
3128.172997	388325.136812	40.248192
3131.148372	389068.520266	40.253210
3134.848829	389807.236289	40.258228
3137.781705	390547.239715	40.263245
3141.337160	391287.832948	40.268263
3144.738214	392034.200362	40.273280
3147.704101	392797.980368	40.278298
3151.180055	393542.467025	40.283316
3154.517744	394286.496581	40.288333
3158.108352	395041.703636	40.293351
3161.794682	395768.064409	40.298368
3164.770947	396519.472607	40.303386
3168.040275	397248.688176	40.308404
3171.310309	397987.904641	40.313421
3174.481261	398727.315796	40.318439
3178.001652	399462.144018	40.323456
3181.210867	400189.556535	40.328474
3184.872111	400921.836438	40.333492
3188.340794	401654.477435	40.338509
3191.132157	402375.154363	40.343527
3194.732709	403108.437100	40.348544
3197.347593	403855.565236	40.353562
3200.614865	404584.854084	40.358580
3203.898322	405311.434730	40.363597
3206.783436	406043.215774	40.368615
3209.767555	406781.283121	40.373632
3212.590728	407532.862074	40.378650
3216.267999	408263.890589	40.383668
3219.252720	409011.498148	40.388685
3222.446781	409750.699242	40.393703
3226.010767	410491.437008	40.398720
3229.070073	411238.805506	40.403738
3232.241213	411983.348429	40.408756
3235.778770	412729.528913	40.413773
3239.063890	413474.913532	40.418791
3242.428046	414210.092060	40.423808
3245.765466	414922.384940	40.428826
3249.380401	415618.626420	40.433844
3252.524491	416320.634206	40.438861
3255.933800	417011.196888	40.443879
3259.270280	417698.915937	40.448896
3261.970271	418397.686847	40.453914
3265.109056	419086.402840	40.458932
3267.974566	419788.085596	40.463949
3270.960830	420497.817485	40.468967
3274.043826	421202.807016	40.473984
3276.992820	421923.823646	40.479002
3279.881036	422656.100925	40.484020
3282.833585	423391.932198	40.489037
3285.878548	424136.014988	40.494055
3288.768845	424882.673305	40.499072
3292.076614	425653.356055	40.504090
3295.482876	426419.292253	40.509108
3298.710088	427193.113850	40.514125
3301.318329	427972.259493	40.519143
3304.747713	428749.679881	40.524160
3307.914841	429550.110785	40.529178
3311.382233	430345.660630	40.534196
3314.620403	431146.824639	40.539213
3317.632068	431969.017316	40.544231
3320.505556	432783.363088	40.549248
3323.895737	433620.791927	40.554266
3327.647095	434447.212484	40.559284
3330.784970	435280.010049	40.564301
3333.980615	436120.847845	40.569319
3337.407899	436961.966466	40.574336
3340.835108	437814.669543	40.579354
3344.261622	438661.069322	40.584372
3347.889989	439514.321623	40.589389
3351.299305	440380.603925	40.594407
3354.435845	441235.168364	40.599424
3358.220816	442097.372457	40.604442
3361.709856	442958.521925	40.609460
3365.723975	443812.326542	40.614477
3369.039971	444672.867638	40.619495
3372.801797	445523.702781	40.624512
3376.213544	446393.896307	40.629530
3379.610399	447254.000720	40.634548
3383.362479	448101.283181	40.639565
3386.524783	448975.028120	40.644583
3390.031243	449828.529614	40.649600
3393.357604	450704.033514	40.654618
3396.486800	451559.985525	40.659636
3400.501250	452425.098996	40.664653
3404.222857	453276.786767	40.669671
3408.047267	454130.033021	40.674688
3411.364801	454996.896154	40.679706
3414.912577	455851.364016	40.684724
3418.839728	456694.424559	40.689741
3422.369633	457545.783756	40.694759
3425.738773	458383.902883	40.699776
3429.155029	459229.695741	40.704794
3432.846978	460075.757458	40.709812
3436.735580	460916.650085	40.714829
3439.998512	461757.195053	40.719847
3443.371325	462593.846639	40.724864
3447.016527	463427.841372	40.729882
3450.918229	464268.364489	40.734900
3454.585016	465088.197363	40.739917
3457.685373	465926.542522	40.744935
3461.030197	466746.748006	40.749952
3464.256925	467581.408822	40.754970
3467.901741	468410.918577	40.759988
3471.309731	469235.682428	40.765005
3474.482712	470069.934033	40.770010
3477.910322	470839.485597	40.775015
3481.103318	471579.409281	40.780020
3483.992833	472271.266029	40.785024
3486.813339	472912.800914	40.790029
3489.590990	473502.296902	40.795034
3492.142545	474044.186194	40.800039
3494.793815	474532.407255	40.805044
3496.924052	474983.591246	40.810048
3499.325164	475362.436358	40.815053
3501.476981	475707.747934	40.820058
3503.268502	475998.973017	40.825063
3505.003340	476264.878312	40.830068
3506.481446	476487.653868	40.835072
3508.306985	476663.820997	40.840077
3509.539125	476804.495669	40.845082
3510.628588	476908.597812	40.850087
3511.939032	476998.260062	40.855092
3512.548784	477041.885030	40.860096
3513.821999	477061.196523	40.865101
3514.700486	477059.442425	40.870106
3515.506042	477024.695009	40.875111
3516.334050	476979.077212	40.880116
3517.287890	476906.904360	40.885120
3518.009225	476808.535119	40.890125
3518.336631	476697.944335	40.895130
3519.118115	476571.764939	40.900135
3519.448760	476421.544720	40.905140
3519.455511	476269.098945	40.910144
3519.988979	476098.878632	40.915149
3520.145833	475928.917308	40.920154
3520.639567	475730.848060	40.925159
3520.436139	475538.950605	40.930164
3520.378346	475335.856984	40.935168
3520.926261	475121.040240	40.940173
3520.771682	474909.969541	40.945178
3520.823451	474686.681296	40.950183
3520.823820	474453.641572	40.955188
3520.723034	474235.324852	40.960192
3520.671583	474001.225082	40.965197
3520.935578	473761.815285	40.970202
3520.927809	473524.112531	40.975207
3520.759464	473289.970127	40.980212
3520.800257	473042.394557	40.985216
3520.827824	472800.327927	40.990221
3519.890929	472548.498571	40.995226
3520.261412	472305.511751	41.000231
3520.346555	472060.846719	41.005236
3519.671955	471806.184350	41.010240
3519.959853	471562.592615	41.015245
3519.990562	471320.351862	41.020250
3519.417283	471068.089162	41.025255
3519.804614	470828.920481	41.030260
3519.515990	470575.341843	41.035264
3519.448391	470326.427355	41.040269
3518.830327	470089.578618	41.045274
3519.450465	469841.105982	41.050279
3518.653962	469606.907479	41.055284
3518.518098	469363.652485	41.060288
3518.124987	469123.619707	41.065293
3518.116894	468889.187198	41.070298
3518.132993	468649.994100	41.075303
3518.056244	468421.128258	41.080308
3517.275921	468185.996846	41.085312
3517.260192	467955.496825	41.090317
3517.026809	467731.045544	41.095322
3517.139745	467512.808352	41.100327
3517.058890	467286.051562	41.105332
3516.763916	467071.361622	41.110336
3516.598112	466840.009749	41.115341
3516.459833	466631.257575	41.120346
3516.279755	466402.278899	41.125351
3515.911989	466195.327152	41.130356
3515.597855	465987.555263	41.135360
3515.723493	465774.452260	41.140365
3515.600453	465577.975008	41.145370
3515.519234	465362.420614	41.150375
3515.347563	465158.510882	41.155380
3515.225286	464963.998941	41.160384
3515.013552	464755.588906	41.165389
3514.782155	464556.840437	41.170394
3514.606380	464359.396106	41.175399
3515.008334	464170.357465	41.180404
3514.188801	463970.934873	41.185408
3514.605976	463768.029522	41.190413
3514.227381	463586.238147	41.195418
3513.827526	463398.984943	41.200423
3513.741098	463209.556300	41.205428
3513.782507	463025.316023	41.210432
3513.446300	462841.638375	41.215437
3512.990893	462668.651197	41.220442
3512.891797	462497.579733	41.225447
3513.161936	462327.005562	41.230452
3512.628753	462147.296945	41.235456
3513.011992	461973.868667	41.240461
3512.643330	461804.501634	41.245466
3512.157027	461637.478379	41.250471
3512.393987	461473.932886	41.255476
3511.991763	461304.515524	41.260480
3512.321462	461147.428159	41.265485
3511.807514	460985.967927	41.270490
3511.660762	460823.841919	41.275495
3511.625588	460672.372171	41.280500
3510.875889	460521.771177	41.285504
3511.177467	460368.576754	41.290509
3511.373382	460227.793054	41.295514
3510.784083	460071.344783	41.300519
3510.829133	459923.448181	41.305524
3510.683425	459788.026551	41.310528
3510.739250	459636.027547	41.315533
3510.458336	459504.925406	41.320538
3510.295032	459355.842034	41.325543
3510.390122	459232.623041	41.330548
3510.361385	459086.602841	41.335552
3510.482428	458942.885618	41.340557
3509.981085	458812.065503	41.345562
3509.749201	458678.874913	41.350567
3509.834436	458558.789786	41.355572
3509.721782	458426.185889	41.360576
3509.484639	458296.535155	41.365581
3509.606394	458173.203264	41.370586
3509.311381	458050.238954	41.375591
3509.586123	457921.922587	41.380596
3509.008727	457798.393220	41.385600
3509.345288	457673.809915	41.390605
3508.867123	457553.350080	41.395610
3508.972326	457440.439627	41.400615
3509.061392	457313.564534	41.405620
3508.649895	457207.210152	41.410624
3508.960258	457082.677295	41.415629
3508.452510	456976.893124	41.420634
3508.740267	456867.037387	41.425639
3508.652943	456751.824632	41.430644
3508.500732	456641.631103	41.435648
3508.692623	456528.954279	41.440653
3508.540122	456417.595460	41.445658
3508.864551	456304.188084	41.450663
3508.273979	456192.187515	41.455668
3508.205345	456084.963237	41.460672
3508.387882	455970.057579	41.465677
3508.063931	455864.845350	41.470682
3507.834824	455755.771561	41.475687
3507.388429	455652.044724	41.480692
3507.305408	455560.507883	41.485696
3507.249241	455463.247644	41.490701
3507.241676	455376.961369	41.495706
3507.320411	455272.492659	41.500711
3507.706923	455189.332500	41.505716
3507.246293	455086.161233	41.510720
3507.499659	454997.099580	41.515725
3507.054378	454901.617510	41.520730
3507.196442	454803.968504	41.525735
3507.815381	454726.185283	41.530740
3507.132276	454623.906301	41.535744
3507.499153	454521.564555	41.540749
3507.384305	454439.592316	41.545754
3506.864681	454347.104873	41.550759
3507.105151	454259.408009	41.555764
3506.817850	454161.164303	41.560768
3507.229069	454066.101154	41.565773
3506.804485	453986.806852	41.570778
3506.714264	453888.733411	41.575783
3506.659636	453812.822433	41.580788
3506.634713	453731.592108	41.585792
3506.585482	453645.759359	41.590797
3506.297378	453556.977150	41.595802
3506.300303	453480.245967	41.600807
3506.259352	453400.535037	41.605812
3506.359701	453314.778636	41.610816
3506.339284	453239.366018	41.615821
3506.621270	453161.982655	41.620826
3506.169088	453080.309679	41.625831
3506.287557	452994.953832	41.630836
3506.341394	452925.450329	41.635840
3506.237868	452843.519545	41.640845
3505.940585	452759.138346	41.645850
3505.997344	452685.533544	41.650855
3505.801378	452613.131945	41.655860
3505.822518	452539.228381	41.660864
3506.140414	452463.304270	41.665869
3505.832639	452405.142576	41.670874
3505.948758	452332.336949	41.675879
3505.777597	452254.817681	41.680884
3505.527729	452180.296771	41.685888
3505.558865	452108.212100	41.690893
3505.513614	452040.593421	41.695898
3505.663841	451971.982319	41.700903
3505.843907	451906.504657	41.705908
3505.586093	451833.046520	41.710912
3506.068527	451768.280580	41.715917
3505.436484	451699.992638	41.720922
3505.650376	451631.420938	41.725927
3505.943667	451555.851128	41.730932
3505.926546	451485.188796	41.735936
3505.685467	451412.283139	41.740941
3505.389162	451342.524225	41.745946
3505.519808	451265.966097	41.750951
3505.406426	451194.153326	41.755956
3505.117310	451139.679898	41.760960
3505.350226	451072.317990	41.765965
3505.168703	451013.777765	41.770970
3505.236531	450952.060030	41.775975
3505.515657	450883.880284	41.780980
3505.253103	450826.010132	41.785984
3505.292392	450752.450698	41.790989
3505.285302	450688.769464	41.795994
3505.463657	450624.097327	41.800999
3505.188642	450567.595078	41.806004
3505.093064	450498.560974	41.811008
3505.355382	450437.823654	41.816013
3505.440093	450372.000860	41.821018
3505.077828	450311.157813	41.826023
3505.290336	450257.565481	41.831028
3505.265794	450189.531599	41.836032
3505.380119	450123.804533	41.841037
3505.110181	450055.403341	41.846042
3505.036038	449994.970002	41.851047
3505.093608	449930.212915	41.856052
3504.867317	449880.079556	41.861056
3504.961286	449824.530035	41.866061
3504.819952	449762.385140	41.871066
3504.874625	449701.677648	41.876071
3505.264766	449641.778372	41.881076
3505.050829	449578.277267	41.886080
3505.112117	449513.062476	41.891085
3505.271058	449461.045493	41.896090
3505.255772	449395.437190	41.901095
3504.773482	449336.482670	41.906100
3505.064793	449278.825102	41.911104
3505.229971	449208.226693	41.916109
3505.050375	449149.325711	41.921114
3504.934177	449092.743489	41.926119
3505.075059	449045.436379	41.931124
3504.706887	448983.324098	41.936128
3504.981069	448919.795345	41.941133
3504.777023	448865.301784	41.946138
3504.766456	448810.322307	41.951143
3504.933602	448749.745993	41.956148
3504.894518	448689.859727	41.961152
3505.043506	448630.703413	41.966157
3505.042504	448574.911687	41.971162
3504.905407	448516.508309	41.976167
3504.927846	448466.180432	41.981172
3504.684435	448407.540104	41.986176
3504.245233	448352.271538	41.991181
3504.617993	448294.851304	41.996186
3504.373000	448241.121666	42.001191
3504.758105	448176.459211	42.006196
3504.359871	448130.853733	42.011200
3504.256184	448079.784972	42.016205
3504.615057	448029.201012	42.021210
3504.821306	447979.400104	42.026215
3504.813739	447920.164575	42.031220
3504.686241	447873.098687	42.036224
3504.522387	447808.014047	42.041229
3504.341903	447761.361154	42.046234
3503.846598	447719.718901	42.051239
3504.446582	447662.362570	42.056244
3503.973345	447616.716841	42.061248
3504.391192	447563.337725	42.066253
3504.343886	447512.916797	42.071258
3504.223066	447462.962847	42.076263
3504.534383	447415.017392	42.081268
3504.341648	447366.694565	42.086272
3504.498269	447316.697041	42.091277
3504.195476	447260.796347	42.096282
3504.194241	447219.430484	42.101287
3504.350251	447166.293478	42.106292
3503.801092	447121.569693	42.111296
3504.183657	447075.941328	42.116301
3504.288311	447025.191610	42.121306
3504.036505	446984.218632	42.126311
3504.244887	446942.363831	42.131316
3503.958014	446887.775958	42.136320
3504.185737	446833.411640	42.141325
3504.261418	446801.349285	42.146330
3504.494415	446745.161102	42.151335
3504.407833	446692.161732	42.156340
3503.949517	446648.080878	42.161344
3504.305284	446589.746515	42.166349
3504.149034	446544.352570	42.171354
3503.735710	446505.378359	42.176359
3504.017632	446463.004680	42.181364
3504.069818	446413.375370	42.186368
3503.843914	446373.814740	42.191373
3504.130927	446329.110793	42.196378
3503.944829	446275.366188	42.201383
3504.304758	446236.625516	42.206388
3503.792495	446194.881145	42.211392
3503.879463	446139.372074	42.216397
3504.042624	446107.699968	42.221402
3504.079014	446055.641677	42.226407
3503.848061	446013.093593	42.231412
3503.857782	445963.773482	42.236416
3503.983456	445917.220137	42.241421
3503.864909	445888.021982	42.246426
3503.840343	445841.846271	42.251431
3503.944887	445808.764976	42.256436
3504.206055	445763.405410	42.261440
3504.274299	445716.556678	42.266445
3503.795998	445668.830792	42.271450
3503.728260	445620.888984	42.276455
3503.879838	445580.103267	42.281460
3503.709697	445540.684069	42.286464
3503.940892	445495.075322	42.291469
3504.125379	445452.157470	42.296474
3503.938836	445415.880023	42.301479
3504.268920	445353.950522	42.306484
3504.212144	445318.108420	42.311488
3504.260746	445261.691200	42.316493
3504.152759	445219.223413	42.321498
3504.103980	445174.366360	42.326503
3504.222066	445121.178686	42.331508
3503.873075	445066.949513	42.336512
3503.804259	445026.399415	42.341517
3503.969311	444985.711560	42.346522
3503.592146	444946.829681	42.351527
3503.944470	444906.720165	42.356532
3504.168043	444868.504209	42.361536
3503.926628	444818.966916	42.366541
3503.646808	444774.701863	42.371546
3503.916832	444733.440093	42.376551
3504.010029	444688.154653	42.381556
3504.068498	444645.153253	42.386560
3504.277821	444597.925247	42.391565
3503.880002	444551.500547	42.396570
3503.864973	444522.891783	42.401575
3504.221966	444478.678840	42.406580
3504.048999	444430.952865	42.411584
3503.926164	444385.902859	42.416589
3503.941994	444347.920711	42.421594
3503.688375	444292.256507	42.426599
3504.117183	444254.463102	42.431604
3503.756923	444218.412887	42.436608
3503.913384	444166.988888	42.441613
3503.976191	444131.885472	42.446618
3503.834221	444076.253883	42.451623
3504.216295	444029.858430	42.456628
3503.597371	443988.581407	42.461632
3503.954684	443938.492814	42.466637
3504.029612	443900.956318	42.471642
3503.440785	443855.319201	42.476647
3503.688179	443818.312751	42.481652
3503.212237	443777.215569	42.486656
3503.622681	443744.741304	42.491661
3503.363071	443706.294288	42.496666
3503.639574	443666.902861	42.501671
3503.461730	443626.316013	42.506676
3503.467922	443593.651182	42.511680
3503.098628	443560.842157	42.516685
3503.574186	443522.888059	42.521690
3503.462041	443491.355584	42.526695
3503.578554	443448.291726	42.531700
3503.525558	443417.104415	42.536704
3503.630281	443372.320382	42.541709
3503.496173	443341.094923	42.546714
3503.312458	443297.419083	42.551719
3503.594806	443253.316118	42.556724
3503.319879	443214.971750	42.561728
3503.425744	443183.607397	42.566733
3503.403894	443147.705006	42.571738
3503.369939	443128.162107	42.576743
3503.714608	443086.783767	42.581748
3503.238127	443049.381997	42.586752
3503.393694	443002.360861	42.591757
3503.734267	442970.048045	42.596762
3503.415649	442940.572499	42.601767
3503.685397	442896.369360	42.606772
3503.864322	442861.954481	42.611776
3503.433088	442825.659379	42.616781
3503.719478	442787.429357	42.621786
3503.629394	442743.180561	42.626791
3503.925880	442706.569409	42.631796
3503.648480	442670.553930	42.636800
3503.448180	442621.662731	42.641805
3503.631955	442587.145300	42.646810
3503.575235	442547.702067	42.651815
3503.563601	442504.453387	42.656820
3503.251054	442473.304880	42.661824
3503.029683	442435.153148	42.666829
3503.237844	442405.949294	42.671834
3503.308376	442374.589076	42.676839
3503.380252	442337.049896	42.681844
3503.332413	442309.506370	42.686848
3503.592216	442266.873287	42.691853
3503.305496	442225.945804	42.696858
3503.193980	442192.283920	42.701863
3503.339645	442157.214524	42.706868
3503.223826	442128.668398	42.711872
3503.414164	442093.237411	42.716877
3503.212686	442067.641975	42.721882
3503.030659	442026.697764	42.726887
3503.269214	441983.814111	42.731892
3503.178708	441964.835897	42.736896
3503.614165	441927.695131	42.741901
3503.442054	441892.218871	42.746906
3503.345046	441860.073519	42.751911
3503.573084	441821.648013	42.756916
3503.462281	441798.773009	42.761920
3503.306731	441749.366092	42.766925
3503.600189	441712.702816	42.771930
3503.458267	441675.296869	42.776935
3503.470539	441630.472390	42.781940
3503.037383	441598.024367	42.786945
3503.385213	441565.150873	42.791949
3503.628503	441539.840032	42.796954
3503.414115	441498.190637	42.801959
3503.532678	441446.663723	42.806964
3503.380083	441428.859520	42.811969
3503.374081	441379.580298	42.816973
3503.550232	441344.605930	42.821978
3503.621632	441312.382782	42.826983
3503.619469	441261.532568	42.831988
3503.086093	441234.113661	42.836993
3503.416967	441202.001891	42.841997
3503.448580	441171.709323	42.847002
3502.996284	441135.667450	42.852007
3503.242075	441096.629914	42.857012
3503.287819	441065.119412	42.862017
3503.186307	441038.494040	42.867021
3503.535064	441009.873913	42.872026
3503.196357	440964.747916	42.877031
3503.370203	440934.382184	42.882036
3503.133372	440901.851753	42.887041
3503.539482	440865.827729	42.892045
3503.371472	440833.489067	42.897050
3503.512200	440792.593229	42.902055
3503.417427	440756.849536	42.907060
3503.088929	440722.712280	42.912065
3503.559269	440679.485678	42.917069
3503.221073	440653.403086	42.922074
3503.272311	440622.245534	42.927079
3503.524792	440582.040944	42.932084
3503.463533	440546.443586	42.937089
3503.222186	440509.861183	42.942093
3503.146866	440474.468476	42.947098
3503.476086	440448.281742	42.952103
3503.262474	440411.188329	42.957108
3503.382145	440383.615904	42.962113
3503.146291	440339.536057	42.967117
3503.588132	440313.179658	42.972122
3503.166573	440272.370188	42.977127
3503.210108	440236.553333	42.982132
3503.108571	440202.126558	42.987137
3503.559096	440169.741153	42.992141
3503.526760	440134.746326	42.997146
3503.458390	440090.690485	43.002151
3503.286599	440052.830091	43.007156
3503.164095	440021.951838	43.012161
3503.458262	439983.866842	43.017165
3502.951020	439961.760408	43.022170
3502.983783	439934.403456	43.027175
3503.122405	439893.354038	43.032180
3503.044650	439861.962043	43.037185
3503.222715	439837.114927	43.042189
3503.451998	439808.410264	43.047194
3502.990604	439769.631979	43.052199
3503.440276	439736.334228	43.057204
3503.621933	439703.432689	43.062209
3503.544459	439660.137042	43.067213
3503.224143	439633.189163	43.072218
3503.061061	439592.743217	43.077223
3503.500646	439555.191905	43.082228
3503.368597	439524.213018	43.087233
3503.138793	439490.716653	43.092237
3503.232795	439457.777674	43.097242
3502.976824	439425.146363	43.102247
3503.315406	439390.700273	43.107252
3503.054868	439354.118612	43.112257
3503.328780	439330.370285	43.117261
3503.490318	439293.216294	43.122266
3503.015219	439261.783826	43.127271
3503.393024	439225.659770	43.132276
3503.177928	439196.770062	43.137281
3503.312468	439163.013805	43.142285
3503.393398	439128.303409	43.147290
3503.055446	439099.989862	43.152295
3503.045038	439063.014138	43.157300
3502.974848	439034.810788	43.162305
3502.727788	439007.040151	43.167309
3502.972265	438974.988690	43.172314
3502.834417	438947.758168	43.177319
3502.875972	438915.029023	43.182324
3502.951051	438884.168818	43.187329
3502.964860	438850.228174	43.192333
3503.491534	438824.312392	43.197338
3503.227976	438800.748349	43.202343
3503.311814	438759.350413	43.207348
3502.830040	438727.310238	43.212353
3502.890601	438693.210073	43.217357
3503.653122	438660.570918	43.222362
3503.021022	438638.684982	43.227367
3502.957328	438599.234547	43.232372
3503.200273	438571.994884	43.237377
3503.310663	438545.535639	43.242381
3503.051057	438514.068394	43.247386
3502.894286	438481.065431	43.252391
3503.124824	438448.103451	43.257396
3503.336023	438432.012749	43.262401
3502.828489	438384.323413	43.267405
3502.846536	438354.990894	43.272410
3503.059857	438325.931879	43.277415
3503.421101	438295.887338	43.282420
3503.148614	438268.372856	43.287425
3503.570725	438230.872300	43.292429
3502.963237	438209.488599	43.297434
3503.089985	438180.848084	43.302439
3503.163070	438131.294791	43.307444
3503.048600	438104.414015	43.312449
3502.939405	438067.856976	43.317453
3502.887493	438032.759997	43.322458
3503.282516	438008.433949	43.327463
3503.076411	437972.904943	43.332468
3503.315266	437952.098445	43.337473
3503.278258	437912.490462	43.342477
3503.429276	437875.436648	43.347482
3503.192956	437849.739587	43.352487
3503.358451	437813.392600	43.357492
3502.733553	437793.682828	43.362497
3502.826124	437757.499055	43.367501
3502.522259	437726.442652	43.372506
3502.844754	437711.955062	43.377511
3503.349637	437677.277359	43.382516
3503.012923	437645.618045	43.387521
3503.417980	437605.586028	43.392525
3503.277844	437585.547316	43.397530
3503.276860	437545.426385	43.402535
3503.489419	437505.677405	43.407540
3503.056917	437478.034705	43.412545
3503.080794	437457.109147	43.417549
3502.959316	437413.713906	43.422554
3502.749899	437385.681749	43.427559
3502.810581	437358.316739	43.432564
3502.877719	437329.380270	43.437569
3502.822601	437302.438468	43.442573
3503.364615	437272.009575	43.447578
3503.145722	437242.864191	43.452583
3503.548084	437198.627064	43.457588
3503.222264	437173.094994	43.462593
3502.942915	437135.752102	43.467597
3503.266557	437111.993271	43.472602
3503.339270	437084.119405	43.477607
3503.063850	437043.280237	43.482612
3502.915723	437009.564148	43.487617
3502.966105	436984.479878	43.492621
3502.870415	436948.830463	43.497626
3502.694749	436930.063080	43.502631
3502.910685	436896.644756	43.507636
3502.726254	436867.493437	43.512641
3502.516691	436848.477950	43.517645
3502.920194	436814.169078	43.522650
3502.856943	436791.280613	43.527655
3502.939535	436751.499630	43.532660
3502.860780	436731.703770	43.537665
3502.878551	436702.926017	43.542669
3502.896234	436672.577765	43.547674
3502.607548	436643.442328	43.552679
3502.672553	436617.899359	43.557684
3502.707752	436590.030611	43.562689
3502.811141	436567.977176	43.567693
3503.071468	436550.458749	43.572698
3502.813673	436512.756663	43.577703
3503.007977	436491.195599	43.582708
3502.671715	436473.465974	43.587713
3502.977050	436440.083605	43.592717
3502.937138	436411.517033	43.597722
3502.800837	436389.044743	43.602727
3503.044995	436355.013151	43.607732
3503.207383	436330.113240	43.612737
3502.901544	436303.006401	43.617741
3502.950751	436270.676819	43.622746
3502.838696	436239.841457	43.627751
3503.286980	436202.332854	43.632756
3502.893706	436177.367228	43.637761
3503.024001	436141.630483	43.642765
3503.439853	436120.135851	43.647770
3502.784429	436085.585166	43.652775
3502.891346	436049.497255	43.657780
3502.923230	436024.769242	43.662785
3502.867962	435990.276979	43.667789
3502.950395	435973.494979	43.672794
3502.850234	435940.681463	43.677799
3503.089450	435904.319382	43.682804
3502.674181	435882.345870	43.687809
3502.679203	435850.275767	43.692813
3502.995426	435822.159525	43.697818
3502.957992	435795.618152	43.702823
3502.853983	435767.009934	43.707828
3502.398978	435754.719026	43.712833
3502.779282	435724.059533	43.717837
3502.999879	435697.021907	43.722842
3502.554322	435673.684972	43.727847
3502.794309	435645.377683	43.732852
3502.704821	435624.366440	43.737857
3502.954782	435598.793335	43.742861
3503.127767	435565.784686	43.747866
3503.257337	435548.944317	43.752871
3502.973278	435500.959689	43.757876
3502.857717	435467.539803	43.762881
3502.560062	435451.981754	43.767885
3502.990227	435421.921984	43.772890
3502.503836	435400.870933	43.777895
3502.693932	435363.299546	43.782900
3502.562134	435346.651664	43.787905
3502.653831	435321.812113	43.792909
3502.897403	435292.439808	43.797914
3502.351727	435269.573937	43.802919
3502.112043	435242.759291	43.807924
3502.782399	435223.453275	43.812929
3502.845803	435200.239221	43.817933
3502.904372	435175.353972	43.822938
3502.642590	435143.881518	43.827943
3502.820024	435120.294974	43.832948
3502.982116	435101.219921	43.837953
3503.096037	435072.931410	43.842957
3503.091579	435046.738527	43.847962
3502.787005	435020.592309	43.852967
3502.810341	434983.299457	43.857972
3502.568480	434965.199095	43.862977
3502.789220	434940.490967	43.867981
3502.851871	434911.804880	43.872986
3502.844057	434890.577467	43.877991
3503.066515	434853.709364	43.882996
3502.851722	434831.196803	43.888001
3502.426332	434803.295812	43.893005
3502.639966	434770.988791	43.898010
3502.684931	434753.248920	43.903015
3502.976254	434715.609857	43.908020
3502.674732	434692.958635	43.913025
3502.914142	434658.823458	43.918029
3502.636783	434634.952434	43.923034
3502.524650	434615.615582	43.928039
3502.524565	434583.290840	43.933044
3502.466638	434561.969534	43.938049
3502.685387	434542.986446	43.943053
3502.878140	434511.442230	43.948058
3502.913759	434488.839638	43.953063
3502.589236	434460.719791	43.958068
3502.716980	434443.169418	43.963073
3502.717622	434412.009598	43.968077
3502.523323	434392.127980	43.973082
3502.583514	434384.062657	43.978087
3502.717823	434349.892625	43.983092
3502.632020	434331.108722	43.988097
3502.470147	434297.846017	43.993101
3502.870091	434268.903824	43.998106
3502.738161	434259.500348	44.003111
3502.529985	434220.266053	44.008116
3502.631343	434193.548880	44.013121
3502.596811	434175.162182	44.018125
3502.749465	434148.791633	44.023130
3502.612881	434133.866126	44.028135
3502.716089	434103.449854	44.033140
3502.550066	434079.358150	44.038145
3502.625645	434057.964847	44.043149
3503.050460	434029.879770	44.048154
3502.548534	433998.898826	44.053159
3502.559636	433978.224810	44.058164
3502.515973	433948.439159	44.063169
3502.091031	433930.112980	44.068173
3502.800103	433902.287490	44.073178
3502.613082	433880.934855	44.078183
3502.771599	433852.434952	44.083188
3502.745797	433834.907923	44.088193
3502.504557	433809.459560	44.093197
3502.547744	433786.550965	44.098202
3502.210896	433764.765506	44.103207
3502.709122	433740.772689	44.108212
3502.670942	433721.828781	44.113217
3502.614954	433702.735621	44.118221
3502.514496	433679.241235	44.123226
3502.642374	433646.591010	44.128231
3502.653925	433631.996742	44.133236
3502.693035	433601.538991	44.138241
3502.676003	433575.194069	44.143245
3502.657104	433557.817722	44.148250
3502.627461	433537.504257	44.153255
3502.915288	433506.855648	44.158260
3502.741122	433477.241588	44.163265
3502.557039	433445.652945	44.168269
3502.871316	433422.296385	44.173274
3502.836793	433401.274174	44.178279
3502.951807	433375.161779	44.183284
3502.731993	433349.608141	44.188289
3502.715615	433333.295250	44.193293
3503.044355	433292.354120	44.198298
3502.897332	433266.029008	44.203303
3502.926349	433233.950838	44.208308
3502.961884	433214.133586	44.213313
3502.826856	433185.627717	44.218317
3502.813389	433146.918318	44.223322
3502.884359	433126.892786	44.228327
3502.706978	433088.006099	44.233332
3503.116788	433068.991842	44.238337
3503.052972	433045.490989	44.243341
3502.649916	433014.797108	44.248346
3502.785262	432994.254723	44.253351
3502.746925	432962.541276	44.258356
3502.580911	432943.667173	44.263361
3502.686818	432913.958003	44.268365
3502.834552	432876.489736	44.273370
3502.733293	432864.192608	44.278375
3502.641011	432839.175828	44.283380
3502.536538	432809.752588	44.288385
3502.455196	432782.048501	44.293389
3502.826782	432764.458670	44.298394
3502.777440	432737.306916	44.303399
3502.705708	432707.827758	44.308404
3502.798896	432691.345267	44.313409
3502.589689	432655.046875	44.318413
3502.969317	432630.969810	44.323418
3502.980382	432608.622208	44.328423
3503.168898	432560.252737	44.333428
3502.893576	432537.544251	44.338433
3502.673542	432517.664720	44.343437
3502.986845	432482.298121	44.348442
3502.771872	432459.276125	44.353447
3502.944499	432438.321985	44.358452
3503.097758	432402.017390	44.363457
3502.915832	432370.477340	44.368461
3502.850425	432351.029622	44.373466
3502.551108	432331.820969	44.378471
3502.850731	432295.898775	44.383476
3502.752786	432276.101343	44.388481
3502.592477	432242.328164	44.393485
3502.599015	432222.058371	44.398490
3502.612962	432200.925981	44.403495
3502.831012	432172.870410	44.408500
3503.058720	432154.288980	44.413505
3502.823849	432121.337949	44.418509
3502.907545	432088.945357	44.423514
3502.335756	432062.482032	44.428519
3502.731903	432037.641582	44.433524
3502.793946	432018.021683	44.438529
3502.699323	431995.943190	44.443533
3502.934747	431960.182388	44.448538
3502.683683	431943.043422	44.453543
3502.716655	431907.415373	44.458548
3502.775138	431876.597208	44.463553
3502.436161	431854.708599	44.468557
3502.824018	431825.511304	44.473562
3502.709896	431811.898019	44.478567
3502.508012	431781.018874	44.483572
3502.637950	431757.334303	44.488577
3502.283914	431723.691722	44.493581
3502.694188	431713.341198	44.498586
3502.532669	431695.073268	44.503591
3503.110327	431673.599223	44.508596
3502.582157	431630.558337	44.513601
3502.659256	431613.976097	44.518605
3502.941690	431578.409980	44.523610
3502.692525	431553.111927	44.528615
3502.566937	431531.899182	44.533620
3502.465086	431498.977079	44.538625
3502.373245	431482.674387	44.543629
3502.371629	431455.158711	44.548634
3502.336551	431439.607259	44.553639
3502.423891	431411.266896	44.558644
3502.420443	431394.392961	44.563649
3502.116266	431369.204580	44.568653
3502.212608	431340.305299	44.573658
3502.364788	431340.180253	44.578663
3502.609626	431316.122551	44.583668
3502.154709	431292.325734	44.588673
3502.263865	431277.055754	44.593677
3502.481955	431259.387114	44.598682
3502.516343	431236.628924	44.603687
3502.466619	431213.731773	44.608692
3502.513297	431190.819593	44.613697
3501.896311	431170.138997	44.618701
3502.241887	431158.328685	44.623706
3502.285340	431136.633137	44.628711
3502.336791	431125.983418	44.633716
3502.619370	431109.318104	44.638721
3502.319863	431080.023966	44.643725
3502.669962	431048.703051	44.648730
3502.230249	431031.136568	44.653735
3502.345388	431012.622253	44.658740
3502.395877	430991.685576	44.663745
3502.459164	430973.939419	44.668749
3502.261239	430948.227213	44.673754
3502.114134	430936.898837	44.678759
3502.120636	430914.955419	44.683764
3502.183702	430902.884864	44.688769
3501.972276	430876.262509	44.693773
3502.538873	430862.948041	44.698778
3502.434728	430848.572404	44.703783
3502.221632	430821.798208	44.708788
3502.385652	430815.438225	44.713793
3502.092539	430790.804813	44.718797
3502.386694	430766.688091	44.723802
3502.140698	430759.479731	44.728807
3502.450077	430740.681556	44.733812
3502.693395	430719.663908	44.738817
3502.641842	430699.553612	44.743821
3502.295419	430672.495906	44.748826
3502.280800	430650.048720	44.753831
3502.386580	430628.444266	44.758836
3502.507912	430607.141424	44.763841
3502.209814	430585.498419	44.768845
3502.249978	430559.039190	44.773850
3502.624162	430546.717299	44.778855
3502.598489	430521.079083	44.783860
3502.543385	430499.347495	44.788865
3502.072382	430479.809010	44.793869
3502.513711	430466.665799	44.798874
3502.054108	430440.030797	44.803879
3502.459489	430422.889706	44.808884
3502.632181	430400.058352	44.813889
3502.256780	430383.849552	44.818893
3502.459570	430348.800377	44.823898
3502.548275	430345.644598	44.828903
3502.416897	430317.691437	44.833908
3502.618423	430301.747530	44.838913
3502.311726	430275.493927	44.843917
3502.135911	430248.307736	44.848922
3502.394078	430234.230010	44.853927
3502.391603	430225.007155	44.858932
3502.661824	430206.011857	44.863937
3502.298352	430185.138742	44.868941
3502.596520	430150.378437	44.873946
3502.342331	430137.748657	44.878951
3502.137765	430116.597356	44.883956
3502.035382	430092.592196	44.888961
3502.189905	430081.672489	44.893965
3502.576458	430065.547567	44.898970
3502.820549	430049.090059	44.903975
3502.442359	430021.884371	44.908980
3502.595625	429986.436841	44.913985
3502.440580	429969.179856	44.918989
3502.786795	429940.391676	44.923994
3502.399479	429922.714695	44.928999
3502.739491	429894.991649	44.934004
3502.635723	429871.138470	44.939009
3502.572242	429843.478141	44.944013
3502.414962	429817.606102	44.949018
3502.463661	429797.631323	44.954023
3502.686512	429773.929914	44.959028
3502.850992	429750.947056	44.964033
3502.328807	429732.581395	44.969037
3502.413726	429698.613658	44.974042
3502.175729	429702.451556	44.979047
3502.427113	429670.535681	44.984052
3502.400791	429655.792316	44.989057
3502.174960	429627.447449	44.994061
3502.234300	429606.254535	44.999066
3502.194953	429593.134867	45.004071
3502.353197	429561.689418	45.009076
3502.648874	429551.102205	45.014081
3502.326416	429544.158693	45.019085
3502.883809	429523.952443	45.024090
3502.544755	429493.496491	45.029095
3502.497820	429465.022196	45.034100
3502.679997	429440.667891	45.039105
3502.494490	429426.759992	45.044109
3502.572115	429391.677924	45.049114
3502.369379	429379.951879	45.054119
3502.552057	429353.722258	45.059124
3502.564913	429326.049328	45.064129
3502.521165	429314.754618	45.069133
3502.571803	429284.795178	45.074138
3502.188628	429268.434634	45.079143
3502.276627	429250.987164	45.084148
3502.438494	429224.507214	45.089153
3502.294824	429200.203321	45.094157
3502.455179	429174.128976	45.099162
3502.524645	429171.938920	45.104167
3502.565732	429141.017835	45.109172
3502.509854	429122.579045	45.114177
3502.442576	429099.023338	45.119181
3502.357499	429072.682974	45.124186
3502.247256	429051.313137	45.129191
3502.337654	429031.685859	45.134196
3502.685388	429012.069197	45.139201
3502.376482	428989.361843	45.144205
3502.519609	428965.469156	45.149210
3502.284199	428956.281958	45.154215
3502.019232	428926.827214	45.159220
3502.346198	428913.852816	45.164225
3502.149890	428891.888036	45.169229
3502.242254	428866.584076	45.174234
3502.435949	428841.872483	45.179239
3502.476771	428821.948629	45.184244
3502.436958	428808.017625	45.189249
3502.238549	428794.618098	45.194253
3502.439160	428763.925006	45.199258
3502.205277	428752.558202	45.204263
3502.150128	428731.787619	45.209268
3502.566719	428718.393700	45.214273
3502.188117	428706.846667	45.219277
3502.166956	428684.398274	45.224282
3502.292318	428655.034430	45.229287
3502.235688	428647.694469	45.234292
3502.293835	428624.524132	45.239297
3502.060339	428617.617131	45.244301
3502.222612	428590.325377	45.249306
3502.399150	428571.140372	45.254311
3502.376985	428548.083806	45.259316
3502.583921	428515.210050	45.264321
3502.365631	428506.678839	45.269325
3502.373345	428481.438244	45.274330
3501.982381	428466.700059	45.279335
3502.491363	428443.864809	45.284340
3502.460898	428431.300490	45.289345
3502.146597	428407.174226	45.294349
3502.262483	428388.910755	45.299354
3502.138681	428378.084106	45.304359
3502.115398	428348.540216	45.309364
3502.254308	428335.696070	45.314369
3502.104743	428320.565439	45.319373
3501.842539	428297.799347	45.324378
3502.195046	428294.804920	45.329383
3502.458783	428268.713305	45.334388
3502.399099	428244.800632	45.339393
3501.801281	428239.876113	45.344397
3502.122868	428207.997653	45.349402
3502.138848	428191.523426	45.354407
3502.170432	428179.608162	45.359412
3502.377707	428160.012521	45.364417
3502.072896	428151.798715	45.369421
3502.419994	428124.730975	45.374426
3502.242552	428124.353111	45.379431
3502.290391	428093.885493	45.384436
3502.085637	428079.219409	45.389441
3501.941775	428069.257317	45.394445
3502.231724	428041.336754	45.399450
3502.169885	428033.946695	45.404455
3502.073207	428015.107769	45.409460
3502.189318	427987.670326	45.414465
3502.128063	427983.473171	45.419469
3502.497749	427961.824753	45.424474
3502.575518	427945.644804	45.429479
3502.482372	427917.124805	45.434484
3502.758136	427894.021123	45.439489
3502.348840	427877.562132	45.444493
3502.433901	427853.778517	45.449498
3502.467991	427828.127528	45.454503
3502.625132	427804.991519	45.459508
3502.651442	427782.686775	45.464513
3502.693823	427765.751939	45.469517
3502.628518	427737.379402	45.474522
3502.537335	427711.038189	45.479527
3502.175211	427691.834797	45.484532
3502.494753	427669.281562	45.489537
3502.299499	427655.678044	45.494541
3502.271838	427623.548899	45.499546
3502.279951	427604.490545	45.504551
3502.472548	427584.592523	45.509556
3502.140185	427560.822833	45.514561
3502.346593	427554.303163	45.519565
3502.600423	427527.958705	45.524570
3502.478888	427514.343619	45.529575
3502.349431	427485.169764	45.534580
3502.296632	427466.678281	45.539585
3502.121667	427451.753680	45.544589
3502.329708	427431.498315	45.549594
3502.431879	427427.579718	45.554599
3502.295184	427402.410917	45.559604
3502.621887	427392.578000	45.564609
3502.415342	427362.300907	45.569613
3502.324278	427338.341350	45.574618
3502.290300	427313.612614	45.579623
3502.077486	427298.491051	45.584628
3502.097055	427273.095034	45.589633
3501.892004	427264.257124	45.594637
3502.126321	427252.512499	45.599642
3502.081345	427237.567511	45.604647
3502.390595	427214.660576	45.609652
3502.165103	427203.088844	45.614657
3501.929680	427179.100876	45.619661
3502.211071	427165.676277	45.624666
3502.266788	427151.729253	45.629671
3502.197303	427136.078415	45.634676
3502.271124	427112.092930	45.639681
3502.310035	427094.245737	45.644685
3502.415436	427073.397763	45.649690
3502.326950	427039.047004	45.654695
3502.057401	427027.482027	45.659700
3502.088283	427009.990805	45.664705
3501.829403	427005.874884	45.669709
3501.981334	426978.329116	45.674714
3502.228550	426981.787916	45.679719
3502.207876	426954.877200	45.684724
3502.267853	426941.132109	45.689729
3501.885475	426916.203672	45.694733
3502.179446	426903.790650	45.699738
3501.969698	426894.750565	45.704743
3502.079345	426875.878461	45.709748
3502.491854	426854.070129	45.714753
3502.024658	426839.139862	45.719757
3502.096106	426817.283193	45.724762
3501.984113	426807.264828	45.729767
3502.229697	426800.029217	45.734772
3502.204193	426767.949054	45.739777
3502.278684	426760.942797	45.744781
3502.353012	426735.943068	45.749786
3502.503509	426729.583890	45.754791
3502.306583	426702.750949	45.759796
3502.369776	426686.065394	45.764801
3501.978904	426669.399797	45.769805
3502.361311	426634.518896	45.774810
3502.096795	426611.143011	45.779815
3501.829174	426550.361058	45.784820
3502.172491	426434.894366	45.789825
3501.317787	426290.367034	45.794829
3501.288873	426080.171233	45.799834
3500.848925	425827.560530	45.804839
3500.777565	425540.877072	45.809844
3500.480848	425196.336966	45.814849
3499.730654	424820.129202	45.819853
3498.911092	424382.030647	45.824858
3498.364610	423916.810140	45.829863
3497.457614	423405.858280	45.834868
3496.710789	422848.482297	45.839873
3495.699461	422252.247705	45.844877
3494.582762	421607.696462	45.849882
3493.458994	420936.305755	45.854887
3492.432544	420222.947597	45.859892
3491.220836	419465.785686	45.864897
3490.345805	418670.311784	45.869901
3488.908722	417826.621356	45.874906
3487.225753	416957.479033	45.879911
3485.759381	416056.420145	45.884916
3484.561856	415095.691937	45.889921
3482.891716	414115.518909	45.894925
3481.182338	413095.239241	45.899930
3479.369652	412041.755613	45.904935
3477.949411	410960.515261	45.909940
3476.200950	409837.981059	45.914945
3474.071670	408684.301076	45.919949
3472.216380	407496.426456	45.924954
3470.134081	406285.541030	45.929959
3468.100046	405041.857059	45.934964
3466.229519	403766.011291	45.939969
3463.961737	402471.888280	45.944973
3461.601332	401138.073895	45.949978
3459.551300	399789.721491	45.954983
3456.503860	398415.562683	45.959988
3454.526110	397008.267669	45.964993
3452.053535	395591.271232	45.969997
3449.813772	394138.672389	45.975002
3447.342219	392663.990320	45.980007
3444.751536	391165.173561	45.985012
3442.307784	389654.260521	45.990017
3439.828093	388112.415863	45.995021
3437.405707	386552.847639	46.000026
3434.386095	384969.637922	46.005031
3431.752989	383370.425417	46.010036
3429.208457	381737.174564	46.015041
3426.059943	380104.321591	46.020045
3423.492005	378450.959871	46.025050
3420.699533	376775.053170	46.030055
3417.539846	375090.818988	46.035060
3414.645611	373394.602348	46.040065
3411.956242	371675.894961	46.045069
3408.478481	369935.940868	46.050074
3405.307706	368197.711685	46.055079
3402.317148	366454.902339	46.060084
3399.392433	364678.183823	46.065089
3396.086314	362898.952047	46.070093
3392.719701	361112.710918	46.075098
3389.962113	359314.248301	46.080103
3386.759327	357504.896626	46.085108
3383.794069	355677.432577	46.090113
3380.262507	353841.612986	46.095117
3377.167507	351988.868030	46.100122
3374.008350	350135.569076	46.105127
3370.117229	348276.686222	46.110132
3367.233918	346401.118863	46.115137
3363.649447	344524.641139	46.120141
3360.150201	342639.148223	46.125146
3356.842573	340751.489283	46.130151
3353.146310	338841.132824	46.135156
3349.951471	336940.896465	46.140161
3346.333310	335030.709062	46.145165
3342.782125	333111.384655	46.150170
3339.192673	331210.383757	46.155175
3335.252638	329283.018016	46.160180
3332.409565	327345.034440	46.165185
3328.973871	325429.867575	46.170189
3325.273856	323489.263775	46.175194
3322.027340	321539.442369	46.180199
3318.224922	319589.643671	46.185204
3314.569568	317636.096351	46.190209
3310.952678	315701.667273	46.195213
3307.286693	313734.034020	46.200218
3303.736883	311772.126395	46.205223
3299.863828	309822.555259	46.210228
3296.329303	307860.078245	46.215233
3292.449134	305906.841050	46.220237
3288.483997	303934.683712	46.225242
3284.774127	301974.094211	46.230247
3281.013706	300025.937742	46.235252
3277.617230	298061.009503	46.240257
3273.500559	296111.346309	46.245261
3270.055347	294156.269539	46.250266
3266.244851	292202.763866	46.255271
3262.186434	290245.263567	46.260276
3258.906698	288276.889728	46.265281
3254.952323	286323.403431	46.270285
3251.316468	284353.313989	46.275290
3247.922034	282399.705221	46.280295
3243.571542	280442.042413	46.285300
3239.758215	278492.137487	46.290305
3235.891941	276542.064462	46.295309
3231.926108	274599.700049	46.300314
3228.408241	272648.283625	46.305319
3224.454834	270711.965297	46.310324
3220.714320	268764.648870	46.315329
3216.874378	266839.588902	46.320333
3213.099896	264906.613065	46.325338
3209.224875	262978.964725	46.330343
3205.318283	261044.997594	46.335348
3201.264092	259116.445358	46.340353
3197.387591	257196.748257	46.345357
3193.525817	255280.025591	46.350362
3189.670310	253372.749071	46.355367
3185.675804	251458.058743	46.360372
3181.810691	249558.223649	46.365377
3177.813199	247653.422003	46.370381
3174.200247	245768.635240	46.375386
3169.860639	243880.658827	46.380391
3166.198011	241985.048167	46.385396
3162.566606	240109.895045	46.390401
3158.196909	238234.895443	46.395405
3154.113420	236346.673280	46.400410
3150.138392	234480.302773	46.405415
3145.886119	232622.780263	46.410420
3142.635361	230767.388353	46.415425
3138.259193	228937.840185	46.420429
3134.237787	227096.314719	46.425434
3130.698343	225268.670227	46.430439
3126.565979	223440.558117	46.435444
3122.465309	221616.314293	46.440449
3118.606905	219810.017259	46.445453
3114.638995	218004.455174	46.450458
3110.830924	216204.095532	46.455463
3106.696644	214420.960140	46.460468
3102.686706	212623.500934	46.465473
3098.593613	210864.624198	46.470477
3094.765183	209082.312301	46.475482
3090.859786	207327.938305	46.480487
3086.699179	205566.359607	46.485492
3083.015319	203817.532264	46.490497
3078.844083	202080.257502	46.495501
3074.451180	200344.460901	46.500506
3070.691014	198621.801852	46.505511
3066.282229	196907.794736	46.510516
3062.547678	195200.451996	46.515521
3058.461785	193502.455309	46.520525
3054.341360	191818.925702	46.525530
3050.390032	190141.122995	46.530535
3045.929144	188480.281796	46.535540
3042.181211	186825.950103	46.540545
3037.735948	185189.144892	46.545549
3033.514298	183556.049182	46.550554
3029.650992	181930.360497	46.555559
3025.316628	180323.030194	46.560564
3020.908901	178720.857958	46.565569
3016.807660	177138.425883	46.570573
3012.623386	175568.296127	46.575578
3008.511092	174005.798237	46.580583
3003.923056	172469.412937	46.585588
2999.820514	170927.878238	46.590593
2995.364280	169420.660350	46.595597
2991.138002	167914.800074	46.600602
2987.012745	166439.365905	46.605607
2982.159580	164972.592203	46.610612
2978.026442	163512.510061	46.615617
2973.414624	162091.521437	46.620621
2968.627023	160677.935693	46.625626
2964.008296	159285.203425	46.630631
2959.364633	157914.766788	46.635636
2955.036368	156561.710205	46.640641
2949.937143	155242.797875	46.645645
2945.086669	153939.772299	46.650650
2940.191421	152670.915263	46.655655
2934.645501	151434.932124	46.660660
2929.782168	150217.615472	46.665665
2924.786795	149042.913128	46.670669
2919.459474	147895.023796	46.675674
2914.648104	146783.306862	46.680679
2909.069450	145710.899404	46.685684
2904.203248	144559.856787	46.690689
2899.285144	143547.667239	46.695693
2894.258906	142559.868422	46.700698
2889.516921	141589.820001	46.705703
2884.574539	140666.974523	46.710708
2880.204818	139744.019546	46.715713
2875.591288	138853.359950	46.720717
2871.250419	137975.715423	46.725722
2866.825720	137140.758352	46.730727
2862.303211	136311.263987	46.735732
2858.133375	135510.303079	46.740737
2854.031165	134724.662678	46.745741
2849.684162	133948.106353	46.750746
2846.006595	133187.984244	46.755751
2841.771723	132450.910594	46.760756
2837.871477	131707.093489	46.765761
2834.433142	130994.827784	46.770765
2830.092579	130293.233991	46.775770
2826.920147	129583.100127	46.780775
2822.780816	128900.043944	46.785780
2819.288116	128210.169517	46.790785
2815.790169	127537.007992	46.795789
2812.177500	126858.774822	46.800794
2808.762794	126182.786013	46.805799
2805.209994	125524.140242	46.810804
2801.081950	124858.586692	46.815809
2797.298539	124195.674085	46.820813
2794.075844	123552.462046	46.825818
2790.548455	122900.913909	46.830823
2787.024926	122266.112558	46.835828
2783.530759	121608.348865	46.840833
2779.937487	120977.750609	46.845837
2776.001148	120349.594098	46.850842
2772.832614	119700.472456	46.855847
2768.993862	119076.416411	46.860852
2765.938352	118446.513517	46.865857
2761.772007	117826.293074	46.870861
2758.310949	117205.795058	46.875866
2754.826983	116577.376132	46.880871
2750.837890	115968.908378	46.885876
2747.182125	115356.838402	46.890881
2743.293951	114751.019832	46.895885
2739.595315	114154.616391	46.900890
2736.149937	113556.581222	46.905895
2732.022638	112974.262961	46.910900
2728.162108	112388.492397	46.915905
2724.086601	111814.995990	46.920909
2719.993614	111240.151116	46.925914
2716.327338	110691.134593	46.930919
2712.521120	110144.182568	46.935924
2708.757658	109593.520061	46.940929
2704.837119	109053.150283	46.945933
2701.430095	108520.400396	46.950938
2697.698918	107991.599285	46.955943
2693.587200	107463.170601	46.960948
2690.455893	106937.864590	46.965953
2686.389117	106416.271669	46.970957
2682.762016	105912.669530	46.975962
2679.524876	105401.374312	46.980967
2675.707117	104892.007683	46.985972
2672.285764	104391.574149	46.990977
2668.863884	103883.635764	46.995981
2664.880010	103371.712292	47.000986
2661.828473	102871.930420	47.005991
2658.242565	102369.379336	47.010996
2654.704305	101865.455765	47.016001
2651.172153	101388.523151	47.021005
2647.698449	100886.002760	47.026010
2644.375947	100388.601444	47.031015
2640.450110	99891.009329	47.036020
2637.774956	99394.691862	47.041025
2634.047041	98900.947967	47.046029
2630.768568	98391.509402	47.051034
2627.400269	97889.921708	47.056039
2623.901537	97397.525291	47.061044
2620.749639	96890.556611	47.066049
2617.186765	96379.961893	47.071053
2613.636315	95872.436225	47.076058
2610.506236	95363.849446	47.081063
2606.492419	94854.353753	47.086068
2603.383970	94334.000340	47.091073
2599.952629	93830.123854	47.096077
2596.248882	93323.388071	47.101082
2592.901599	92812.259415	47.106087
2589.640275	92303.819764	47.111092
2586.377250	91782.402809	47.116097
2582.804321	91275.858603	47.121101
2579.278753	90754.589170	47.126106
2576.027777	90225.929345	47.131111
2572.248334	89717.016720	47.136116
2568.878039	89182.460381	47.141121
2565.712495	88662.111607	47.146125
2562.096299	88130.915835	47.151130
2558.718959	87606.476791	47.156135
2555.458694	87090.172485	47.161140
2552.042436	86551.808804	47.166145
2548.437935	86028.996007	47.171149
2544.574673	85489.209768	47.176154
2541.482250	84961.877488	47.181159
2537.955328	84439.665706	47.186164
2534.577282	83896.251446	47.191169
2531.299721	83368.088031	47.196173
2527.831931	82824.327054	47.201178
2524.495399	82282.867903	47.206183
2520.715152	81751.167214	47.211188
2517.334014	81200.247264	47.216193
2513.811546	80660.931339	47.221197
2510.448958	80123.493447	47.226202
2506.923857	79575.384128	47.231207
2503.523143	79024.205356	47.236212
2500.284730	78475.247634	47.241217
2496.476749	77936.651427	47.246221
2492.859411	77387.863295	47.251226
2489.667806	76831.996879	47.256231
2485.892696	76286.659027	47.261236
2482.624893	75722.483491	47.266241
2478.840568	75174.604196	47.271245
2475.227327	74627.852325	47.276250
2472.111995	74079.256305	47.281255
2468.152655	73529.596547	47.286260
2464.933161	72969.636437	47.291265
2461.261664	72421.084938	47.296269
2457.837714	71868.608149	47.301274
2454.536859	71312.543155	47.306279
2451.125641	70763.046082	47.311284
2447.521280	70213.495387	47.316289
2443.993046	69655.831384	47.321293
2440.379886	69104.204231	47.326298
2436.840447	68537.126415	47.331303
2433.368545	67990.382660	47.336308
2429.933081	67435.081833	47.341313
2426.685626	66873.403545	47.346317
2422.683144	66317.847087	47.351322
2419.751784	65755.249291	47.356327
2416.218207	65198.057569	47.361332
2412.852572	64630.373129	47.366337
2409.455711	64074.524201	47.371341
2405.766359	63519.215473	47.376346
2402.703329	62943.836286	47.381351
2398.615835	62387.618326	47.386356
2395.508394	61814.144417	47.391361
2391.875252	61250.608476	47.396365
2388.223751	60673.203282	47.401370
2384.630841	60106.241458	47.406375
2381.263001	59549.328366	47.411380
2377.761683	58975.493486	47.416385
2374.333695	58409.922459	47.421389
2371.107315	57841.458881	47.426394
2367.845833	57271.339063	47.431399
2364.127858	56693.867540	47.436404
2360.759380	56112.542338	47.441409
2357.203017	55549.000136	47.446413
2353.483539	54968.893159	47.451418
2350.105803	54404.309838	47.456423
2346.333585	53832.429469	47.461428
2343.347756	53246.420327	47.466433
2339.861118	52671.554766	47.471437
2336.103641	52094.024040	47.476442
2332.614416	51506.836379	47.481447
2328.898054	50928.865109	47.486452
2325.654460	50348.760464	47.491457
2322.062838	49774.306473	47.496461
2318.703413	49192.904242	47.501466
2315.409948	48608.442952	47.506471
2311.752809	48033.224599	47.511476
2308.101043	47451.740947	47.516481
2305.083005	46872.907093	47.521485
2301.355716	46286.270808	47.526490
2297.967405	45700.129766	47.531495
2294.272883	45115.427839	47.536500
2290.857756	44528.573268	47.541505
2287.650816	43939.368085	47.546509
2283.930864	43360.004881	47.551514
2280.296986	42758.595417	47.556519
2276.891239	42168.675607	47.561524
2273.462870	41594.227556	47.566529
2269.967179	40996.376522	47.571533
2266.194308	40416.103544	47.576538
2263.193908	39827.236193	47.581543
2259.525725	39238.501398	47.586548
2256.112121	38634.311656	47.591553
2252.834116	38045.478872	47.596557
2248.831985	37458.626038	47.601562
2245.502544	36852.038832	47.606567
2241.838747	36259.143802	47.611572
2238.198546	35669.900191	47.616577
2235.178745	35079.612862	47.621581
2231.510510	34483.015479	47.626586
2227.709512	33887.799375	47.631591
2224.258384	33300.506576	47.636596
2220.810936	32698.189247	47.641601
2217.452442	32113.919569	47.646605
2213.625768	31518.223384	47.651610
2210.343634	30924.031249	47.656615
2206.677271	30341.589462	47.661620
2203.303988	29738.471781	47.666625
2199.826635	29149.113999	47.671629
2196.011983	28559.572153	47.676634
2192.621872	27961.052834	47.681639
2189.223930	27373.127901	47.686644
2185.720479	26778.462859	47.691649
2182.180133	26195.783606	47.696653
2178.545010	25597.479773	47.701658
2175.052509	25001.686797	47.706663
2171.149572	24419.964297	47.711668
2167.928164	23832.349409	47.716673
2164.459183	23246.234757	47.721677
2160.631713	22651.330460	47.726682
2157.515263	22061.635576	47.731687
2153.578177	21475.335634	47.736692
2149.911858	20883.404984	47.741697
2146.916949	20308.255771	47.746701
2143.529100	19725.254302	47.751706
2139.939472	19126.295886	47.756711
2136.311448	18548.839364	47.761716
2132.887321	17946.553604	47.766721
2129.220031	17362.602290	47.771725
2125.449171	16795.404148	47.776730
2121.823565	16207.196928	47.781735
2117.962810	15629.996754	47.786740
2114.775873	15050.261559	47.791745
2110.932544	14481.810028	47.796749
2107.339452	13911.424184	47.801754
2103.750289	13345.015487	47.806759
2100.117229	12771.285665	47.811764
2095.878908	12204.125671	47.816769
2091.727618	11642.344555	47.821773
2087.240031	11106.941949	47.826778
2081.348262	10634.833645	47.831783
2074.341678	10208.160979	47.836788
2068.816243	9772.581750	47.841793
2063.673423	9368.625320	47.846797
2058.712657	9001.258654	47.851802
2053.975279	8650.981876	47.856807
2049.701987	8324.650241	47.861812
2045.527373	8005.462104	47.866817
2041.442968	7710.341857	47.871821
2037.396456	7428.772909	47.876826
2033.890845	7151.994930	47.881831
2030.347174	6893.029568	47.886836
2027.036296	6630.430031	47.891841
2023.599455	6368.834950	47.896845
2019.874826	6121.150046	47.901850
2016.712660	5875.697536	47.906855
2013.507504	5633.663371	47.911860
2010.185647	5386.669446	47.916865
2006.916130	5141.572642	47.921869
2003.121088	4902.484966	47.926874
1999.740432	4657.025914	47.931879
1996.422918	4419.556959	47.936884
1993.012800	4179.159447	47.941889
1989.791271	3943.817773	47.946893
1986.214852	3717.324938	47.951898
1983.023755	3475.867941	47.956903
1979.347089	3251.494483	47.961908
1975.967482	3012.547477	47.966913
1972.822255	2783.100837	47.971917
1969.445977	2545.510617	47.976922
1965.940407	2304.406198	47.981927
1962.718787	2086.146442	47.986932
1958.902714	1848.855371	47.991937
1955.611607	1620.528382	47.996941
1951.977467	1406.881410	48.001946
1948.276984	1176.352097	48.006951
1943.993269	955.525168	48.011956
1940.140375	750.633367	48.016961
1936.471593	544.971780	48.021965
1932.198543	363.024019	48.026970
1927.964842	184.757736	48.031975
1921.545791	72.103571	48.036980
1910.162627	115.604452	48.041985
1903.285819	115.431375	48.046989
1898.745447	115.691920	48.051994
1896.027184	112.672848	48.056999
1893.777195	107.900967	48.062004
1891.708805	111.532105	48.067009
1889.794598	110.045676	48.072013
1886.628379	121.244427	48.077018
1883.329398	104.379604	48.082023
1879.985803	107.212641	48.087028
1876.109056	104.702900	48.092033
1872.741501	106.815178	48.097037
1869.423461	104.721512	48.102042
1866.671965	110.113584	48.107047
1863.155576	105.731791	48.112052
1859.487844	110.937438	48.117057
1856.649811	105.001092	48.122061
1853.079764	111.833499	48.127066
1849.763992	107.126260	48.132071
1846.657670	113.908642	48.137076
1843.489640	108.412792	48.142081
1839.885686	101.779418	48.147085
1836.381278	105.039277	48.152090
1832.589145	108.321771	48.157095
1828.700256	106.775691	48.162100
1825.466376	103.805239	48.167105
1822.343827	104.848020	48.172109
1818.524006	110.400037	48.177114
1815.569261	111.138296	48.182119
1812.094994	102.928200	48.187124
1808.649673	106.552181	48.192129
1804.887747	94.527140	48.197133
1801.534413	102.923487	48.202138
1798.186146	98.695869	48.207143
1795.271984	98.396446	48.212148
1791.531054	109.282844	48.217153
1788.049865	105.341665	48.222157
1784.377220	108.747932	48.227162
1780.961548	98.086343	48.232167
1777.432668	98.667193	48.237172
1773.912351	98.667754	48.242177
1770.824379	100.404335	48.247181
1766.956953	103.628949	48.252186
1763.837576	98.786754	48.257191
1760.103050	107.501855	48.262196
1756.874404	109.595685	48.267201
1753.152714	106.289881	48.272205
1749.971198	111.160435	48.277210
1746.668276	100.895747	48.282215
1742.793423	110.363505	48.287220
1739.311287	104.331272	48.292225
1735.954051	105.353639	48.297229
1732.174907	106.194903	48.302234
1728.950909	109.800261	48.307239
1725.833128	102.474314	48.312244
1722.182864	103.077225	48.317249
1719.211572	107.231700	48.322253
1714.906446	109.603805	48.327258
1711.597976	105.499714	48.332263
1708.006905	107.061506	48.337268
1704.349152	109.006994	48.342273
1701.007743	96.789975	48.347277
1697.491691	104.249884	48.352282
1694.579275	105.873727	48.357287
1691.214093	100.898957	48.362292
1687.414453	106.770536	48.367297
1683.835454	99.715694	48.372301
1680.031452	106.802813	48.377306
1676.058722	100.625487	48.382311
1673.229145	106.551725	48.387316
1669.703033	107.850314	48.392321
1666.392921	100.699842	48.397325
1663.116889	111.906183	48.402330
1659.856016	101.540054	48.407335
1655.701142	98.371287	48.412340
1651.798385	108.286306	48.417345
1648.697288	99.727096	48.422349
1645.193287	107.321170	48.427354
1642.232329	102.520770	48.432359
1638.753550	104.821214	48.437364
1635.189971	103.170742	48.442369
1632.113683	101.653231	48.447373
1627.963432	107.199739	48.452378
1624.034742	104.365924	48.457383
1620.618630	105.489210	48.462388
1617.211559	112.400661	48.467393
1614.219861	95.152730	48.472397
1610.543811	97.699011	48.477402
1607.216182	100.697255	48.482407
1603.325862	95.342332	48.487412
1599.690422	90.915833	48.492417
1596.419513	88.805370	48.497421
1592.962988	91.333302	48.502426
1589.841195	91.812844	48.507431
1585.898887	98.662067	48.512436
1582.089880	95.173728	48.517441
1578.589315	96.860646	48.522445
1575.172893	97.085495	48.527450
1571.860757	95.718591	48.532455
1568.754181	104.408723	48.537460
1565.388454	105.055945	48.542465
1561.651921	93.409810	48.547469
1557.955732	103.561592	48.552474
1554.380104	107.209033	48.557479
1551.131371	104.503509	48.562484
1547.473854	105.050618	48.567489
1544.308108	91.610415	48.572493
1540.516019	105.915238	48.577498
1537.425676	103.808312	48.582503
1533.672594	94.325562	48.587508
1529.926839	105.301293	48.592513
1526.427678	98.180267	48.597517
1522.814670	96.942454	48.602522
1519.609536	93.524646	48.607527
1516.500122	103.420588	48.612532
1512.523953	107.399288	48.617537
1509.313266	99.436113	48.622541
1505.211890	101.112148	48.627546
1502.189816	96.931872	48.632551
1498.808037	95.164536	48.637556
1495.113833	92.376499	48.642561
1491.860555	94.157810	48.647565
1488.107054	100.563207	48.652570
1484.560580	94.952308	48.657575
1481.035519	95.418697	48.662580
1477.424454	106.569614	48.667585
1474.141654	103.205026	48.672589
1470.183227	104.419062	48.677594
1467.100609	107.540529	48.682599
1463.474613	102.856316	48.687604
1460.181583	110.471343	48.692609
1457.011927	95.029145	48.697613
1453.372134	100.600613	48.702618
1449.972882	92.227047	48.707623
1446.585051	99.537293	48.712628
1442.520436	88.464260	48.717633
1439.019010	94.896860	48.722637
1435.540237	104.049877	48.727642
1431.739782	94.210695	48.732647
1428.731142	86.908940	48.737652
1425.296413	95.068026	48.742657
1421.650890	88.194424	48.747661
1417.937109	101.446198	48.752666
1414.363006	95.266982	48.757671
1410.946642	93.068449	48.762676
1407.465111	100.491355	48.767681
1404.241151	90.866165	48.772685
1401.136173	101.856052	48.777690
1397.347880	95.725995	48.782695
1393.715324	94.117923	48.787700
1390.004227	96.112867	48.792705
1386.387038	92.079017	48.797709
1383.182219	95.751008	48.802714
1380.005793	90.199586	48.807719
1376.149500	100.044100	48.812724
1372.591873	99.911303	48.817729
1368.996854	94.867951	48.822733
1365.484372	94.864167	48.827738
1361.908434	100.229552	48.832743
1358.457098	86.897117	48.837748
1355.331497	95.223220	48.842753
1352.034607	90.307471	48.847757
1347.924006	94.297615	48.852762
1344.343768	90.327622	48.857767
1341.306266	92.423364	48.862772
1337.650605	97.608174	48.867777
1334.596804	82.461187	48.872781
1330.862124	94.947432	48.877786
1326.927976	92.832666	48.882791
1323.305902	93.042093	48.887796
1319.857666	98.542624	48.892801
1316.584255	95.265179	48.897805
1313.465115	100.575285	48.902810
1309.605623	87.413955	48.907815
1306.064006	94.675376	48.912820
1302.747627	99.709304	48.917825
1299.133437	95.361794	48.922829
1295.427411	97.985531	48.927834
1291.978066	90.258855	48.932839
1288.784901	89.977592	48.937844
1285.245492	101.740600	48.942849
1281.595150	85.360889	48.947853
1277.768197	85.092857	48.952858
1274.178537	93.810725	48.957863
1271.223965	91.265090	48.962868
1267.943200	92.617271	48.967873
1264.516353	84.380911	48.972877
1260.669311	99.494690	48.977882
1257.049034	94.588161	48.982887
1253.486893	93.842324	48.987892
1249.810839	102.434442	48.992897
1246.479674	88.425278	48.997901
1242.852151	101.103652	49.002906
1239.679151	93.080875	49.007911
1236.171085	95.604203	49.012916
1232.821638	93.600915	49.017921
1229.274276	91.742327	49.022925
1225.746126	92.111147	49.027930
1222.288469	87.426081	49.032935
1218.458591	84.466216	49.037940
1215.003889	97.829516	49.042945
1211.788029	86.725660	49.047949
1208.031130	99.006564	49.052954
1204.473329	90.872851	49.057959
1201.057749	92.856613	49.062964
1197.465593	95.911878	49.067969
1194.290684	84.937691	49.072973
1190.324662	100.563524	49.077978
1187.221083	94.576855	49.082983
1183.640739	87.430562	49.087988
1179.692162	100.048179	49.092993
1176.504795	87.823113	49.097997
1172.932865	94.833000	49.103002
1169.688223	88.320975	49.108007
1166.184795	85.284994	49.113012
1162.300983	94.045489	49.118017
1159.030260	93.061318	49.123021
1155.260690	81.781078	49.128026
1151.809743	92.372404	49.133031
1148.279476	94.933995	49.138036
1145.113440	89.738486	49.143041
1142.185687	78.691041	49.148045
1137.917793	85.556162	49.153050
1134.538952	89.568460	49.158055
1131.281337	89.983763	49.163060
1127.495319	92.812950	49.168065
1123.601754	81.627947	49.173069
1120.405472	94.175917	49.178074
1117.031481	90.366837	49.183079
1113.845426	91.286684	49.188084
1109.797155	87.120665	49.193089
1106.685104	84.178792	49.198093
1103.309138	89.519390	49.203098
1099.505771	88.887049	49.208103
1096.404711	83.668779	49.213108
1092.397748	88.497007	49.218113
1088.984652	86.282187	49.223117
1085.222787	86.339397	49.228122
1081.868436	84.064816	49.233127
1078.535248	90.844560	49.238132
1074.877119	87.598559	49.243137
1071.742431	84.049624	49.248141
1068.224775	88.744743	49.253146
1064.531501	84.650021	49.258151
1061.078794	81.612487	49.263156
1057.114600	84.586471	49.268161
1053.941316	85.551790	49.273165
1050.568528	85.871136	49.278170
1046.739904	86.913156	49.283175
1043.389445	90.199723	49.288180
1039.541723	98.268089	49.293185
1036.560655	83.204758	49.298189
1033.165478	85.811768	49.303194
1029.584618	89.475877	49.308199
1025.946082	89.741682	49.313204
1022.052146	92.701570	49.318209
1018.899704	87.975352	49.323213
1015.357794	92.202863	49.328218
1012.202189	87.553066	49.333223
1008.537325	84.684602	49.338228
1005.131355	81.829621	49.343233
1001.539791	85.074630	49.348237
997.767184	79.739452	49.353242
994.348940	83.710436	49.358247
991.250147	85.815745	49.363252
987.362014	79.808870	49.368257
984.025201	81.033763	49.373261
980.341981	84.903630	49.378266
976.886062	79.557123	49.383271
973.325245	87.340389	49.388276
969.465773	89.725455	49.393281
966.439042	84.109666	49.398285
962.938884	81.604703	49.403290
959.725341	79.086762	49.408295
956.110481	84.477210	49.413300
952.307927	79.608598	49.418305
949.386245	80.120321	49.423309
945.612672	81.694771	49.428314
941.541896	78.509861	49.433319
938.364121	76.179341	49.438324
934.624436	78.416053	49.443329
931.369689	78.277287	49.448333
927.600694	83.859404	49.453338
924.564794	84.933061	49.458343
921.228933	78.596627	49.463348
917.389691	82.133290	49.468353
914.089340	67.005809	49.473357
910.291758	73.592095	49.478362
906.571475	67.774241	49.483367
903.245430	69.525798	49.488372
899.555869	76.133236	49.493377
896.249091	71.867651	49.498381
892.790746	79.011723	49.503386
889.432825	73.093171	49.508391
885.990437	73.954867	49.513396
881.733720	81.817988	49.518401
878.982271	70.170531	49.523405
875.062868	82.002173	49.528410
871.652394	66.442603	49.533415
868.688516	71.500771	49.538420
864.420317	77.242855	49.543425
861.421473	65.083435	49.548429
857.448151	79.574627	49.553434
854.223073	74.685741	49.558439
851.132779	74.458111	49.563444
847.045752	88.261510	49.568449
844.332639	80.078636	49.573453
840.138600	80.978251	49.578458
836.864505	80.874144	49.583463
833.653910	81.677618	49.588468
829.766508	82.921797	49.593473
826.311603	80.324389	49.598477
822.805773	82.885369	49.603482
819.162113	81.984601	49.608487
815.833922	79.323179	49.613492
812.136217	83.935615	49.618497
808.765177	74.703590	49.623501
805.445002	83.895201	49.628506
801.762515	76.097347	49.633511
798.326729	76.246198	49.638516
794.886847	71.368615	49.643521
791.361050	73.670120	49.648525
787.202594	78.338463	49.653530
783.856849	71.848573	49.658535
780.483781	78.818029	49.663540
776.954955	73.922657	49.668545
774.069642	78.237794	49.673549
770.312484	85.871305	49.678554
766.907938	81.839250	49.683559
763.296011	76.513901	49.688564
759.617046	80.224942	49.693569
756.329365	77.898899	49.698573
752.613141	73.586345	49.703578
748.917501	77.923224	49.708583
745.906333	76.265964	49.713588
742.211365	81.444277	49.718593
738.906564	78.880462	49.723597
735.293266	80.543879	49.728602
731.518099	78.138706	49.733607
727.565702	75.527011	49.738612
724.284436	75.838474	49.743617
721.181611	70.737595	49.748621
718.036927	79.781669	49.753626
714.637949	87.264516	49.758631
710.788893	80.115851	49.763636
707.207069	83.283442	49.768641
703.387877	75.177867	49.773645
700.058225	73.946668	49.778650
696.523082	67.131948	49.783655
693.270248	82.343029	49.788660
689.891858	77.019303	49.793665
686.206951	75.985773	49.798669
682.420089	75.192735	49.803674
679.198977	76.225646	49.808679
675.905319	71.107027	49.813684
672.192343	76.000254	49.818689
668.577847	73.462514	49.823693
665.190441	71.749942	49.828698
661.686393	67.837798	49.833703
658.281416	74.419932	49.838708
654.578923	75.129161	49.843713
651.090566	71.594215	49.848717
647.300426	70.317652	49.853722
643.490523	73.463808	49.858727
640.416180	73.040734	49.863732
637.060461	71.468761	49.868737
634.153568	60.038541	49.873741
630.323731	73.254583	49.878746
626.542110	80.670452	49.883751
623.305906	71.151728	49.888756
619.584492	78.131129	49.893761
616.292330	76.523955	49.898765
612.397378	77.528898	49.903770
608.815551	72.660788	49.908775
605.613788	65.547422	49.913780
601.795528	71.972439	49.918785
598.567724	72.038319	49.923789
595.311948	67.556041	49.928794
591.749224	66.791398	49.933799
588.453291	70.003076	49.938804
584.443597	76.397788	49.943809
580.865496	64.018565	49.948813
577.288823	75.344456	49.953818
573.972226	75.458962	49.958823
570.855243	69.018918	49.963828
566.992033	76.232362	49.968833
563.247865	70.253777	49.973837
560.329558	78.677337	49.978842
556.554915	73.529213	49.983847
553.203425	71.295387	49.988852
549.467756	73.980757	49.993857
545.948840	82.649676	49.998861
542.480545	82.794128	50.003866
538.720493	77.937955	50.008871
535.626725	79.675537	50.013876
531.856705	81.268466	50.018881
528.431292	70.045528	50.023885
525.182611	82.908523	50.028890
521.731888	82.797150	50.033895
518.217579	78.301346	50.038900
514.452934	77.330872	50.043905
511.092860	70.931845	50.048909
507.199572	79.431261	50.053914
503.739498	73.522351	50.058919
500.706215	76.104709	50.063924
496.595910	73.368944	50.068929
493.389952	75.294833	50.073933
490.422292	77.319662	50.078938
486.359417	73.152866	50.083943
483.302782	75.295949	50.088948
479.318653	74.577942	50.093953
475.786453	73.235940	50.098957
472.685557	81.333599	50.103962
468.859989	72.741863	50.108967
465.636391	65.970433	50.113972
462.045162	83.107080	50.118977
458.457141	78.284250	50.123981
454.836529	76.500447	50.128986
450.920359	81.029871	50.133991
447.956877	72.762663	50.138996
444.366151	75.798792	50.144001
441.027658	73.948926	50.149005
437.467253	82.086487	50.154010
433.479833	76.073030	50.159015
430.447900	68.895291	50.164020
427.036143	80.714357	50.169025
423.777170	75.432195	50.174029
419.937693	78.965785	50.179034
416.151942	81.042054	50.184039
412.859571	75.505673	50.189044
409.359395	85.079653	50.194049
406.034819	77.631108	50.199053
402.067684	77.840584	50.204058
398.503922	86.810715	50.209063
395.781061	73.966200	50.214068
391.938801	78.155104	50.219073
388.248149	71.652544	50.224077
384.549436	75.401497	50.229082
381.058000	69.582912	50.234087
377.707372	66.260681	50.239092
374.161263	79.663510	50.244097
370.950161	75.493841	50.249101
368.053716	78.105527	50.254106
363.807901	75.292808	50.259111
360.307333	66.802358	50.264116
356.562897	70.121847	50.269121
353.105249	72.203990	50.274125
349.873046	70.150934	50.279130
346.208779	73.853401	50.284135
343.175105	71.367654	50.289140
339.659437	85.449100	50.294145
336.080220	76.743111	50.299149
332.406937	76.033680	50.304154
328.590025	78.159102	50.309159
324.815006	73.472975	50.314164
321.494422	77.662925	50.319169
318.558685	71.058670	50.324173
314.960904	74.292059	50.329178
311.284800	80.663337	50.334183
307.994840	77.281051	50.339188
304.341984	77.546015	50.344193
300.903942	79.175872	50.349197
297.240718	78.771755	50.354202
293.642340	82.486117	50.359207
290.208021	77.047785	50.364212
286.446455	85.137584	50.369217
283.266542	74.477574	50.374221
280.284421	70.398818	50.379226
276.308154	75.541876	50.384231
272.737003	73.203089	50.389236
269.093082	89.961977	50.394241
265.771342	77.125307	50.399245
262.186061	77.047572	50.404250
258.895854	80.539959	50.409255
255.378490	70.805663	50.414260
251.738390	76.497482	50.419265
248.448094	76.016331	50.424269
244.305973	79.967206	50.429274
240.883241	75.839997	50.434279
237.859436	69.344378	50.439284
233.761214	82.257384	50.444289
230.352291	68.042294	50.449293
227.272826	83.112489	50.454298
223.706909	80.260381	50.459303
220.323542	77.702547	50.464308
216.540741	74.346387	50.469313
212.949053	76.034977	50.474317
209.695327	76.221996	50.479322
206.061537	84.516527	50.484327
202.415005	77.684441	50.489332
199.323794	80.029082	50.494337
196.105271	83.826680	50.499341
192.568141	77.948806	50.504346
188.705251	79.094345	50.509351
185.087390	74.545123	50.514356
181.077794	76.694237	50.519361
177.741430	73.398288	50.524365
174.721857	75.421740	50.529370
171.243370	72.476940	50.534375
167.941064	76.879188	50.539380
164.170754	82.537507	50.544385
160.573114	81.563233	50.549389
157.361769	82.370064	50.554394
153.581374	77.735423	50.559399
149.887222	79.360883	50.564404
146.467324	88.555397	50.569409
143.062637	79.670421	50.574413
139.564600	74.298984	50.579418
135.864434	74.982612	50.584423
132.644845	69.517208	50.589428
129.331097	79.043194	50.594433
125.922785	81.228411	50.599437
122.334837	79.015646	50.604442
118.340808	74.714822	50.609447
115.124725	71.396994	50.614452
111.348308	80.397085	50.619457
108.095062	71.896654	50.624461
104.508845	78.032500	50.629466
100.998812	73.403233	50.634471
97.818277	72.231156	50.639476
93.855348	75.334767	50.644481
90.463252	74.847342	50.649485
86.646688	67.371063	50.654490
83.443562	77.778304	50.659495
80.522647	79.612405	50.664500
76.836845	88.554104	50.669505
73.134616	75.194611	50.674509
69.743782	74.843029	50.679514
66.174540	77.600621	50.684519
62.441977	77.530028	50.689524
58.649581	81.119605	50.694529
55.408045	70.912154	50.699533
51.613509	78.630629	50.704538
48.455842	75.784591	50.709543
45.000732	74.139596	50.714548
41.514212	71.797163	50.719553
38.215277	67.897482	50.724557
34.690744	73.903511	50.729562
30.520403	83.458471	50.734567
27.458001	72.258222	50.739572
24.013094	85.031560	50.744577
20.500725	78.156478	50.749581
16.876877	78.397986	50.754586
13.630489	74.164270	50.759591
10.223415	76.039271	50.764596
6.758215	87.379474	50.769601
3.122195	78.634948	50.774605