Fri Aug 26 13:32:48 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.873695	100.854293	0.000000
1.506547	108.795289	0.005005
1.349281	107.456231	0.010010
1.640679	100.884226	0.015014
1.634394	107.373864	0.020019
1.577448	101.422389	0.025024
1.358454	91.997142	0.030029
1.150262	82.177924	0.035034
0.888684	74.796710	0.040038
0.181044	66.592800	0.045043
0.128963	60.555163	0.050048
0.264645	49.837728	0.055053
-0.529146	48.123232	0.060058
-0.197060	40.507237	0.065062
-0.539144	40.532019	0.070067
-0.525179	31.374243	0.075072
-0.852029	15.929593	0.080077
-1.328134	15.133712	0.085082
-1.988976	8.472728	0.090086
-2.441003	5.585095	0.095091
-2.811172	0.090533	0.100096
-2.414910	-6.915361	0.105101
-3.381459	-2.225055	0.110106
-2.899076	-13.945524	0.115110
-3.693189	-5.991882	0.120115
-3.896731	-12.246349	0.125120
-4.480064	-12.804078	0.130125
-4.994930	-8.041736	0.135130
-4.751538	-18.026117	0.140134
-5.119028	-19.231198	0.145139
-4.824868	-21.706677	0.150144
-5.418352	-13.739986	0.155149
-6.068037	-9.908908	0.160154
-5.908267	-17.181686	0.165158
-6.462337	-13.912806	0.170163
-6.603287	-10.809483	0.175168
-6.375836	-18.693888	0.180173
-7.207591	-6.336930	0.185178
-7.556724	-9.756254	0.190182
-7.790794	-10.431635	0.195187
-7.963389	-21.585065	0.200192
-7.950829	-23.222627	0.205197
-8.105164	-17.339548	0.210202
-8.108168	-24.052324	0.215206
-9.078579	-23.578550	0.220211
-9.237857	-14.875900	0.225216
-9.484534	-20.326411	0.230221
-9.764830	-10.165462	0.235226
-9.068465	-21.852804	0.240230
-9.973824	-10.724535	0.245235
-10.655864	-9.207367	0.250240
-10.750464	-17.389631	0.255245
-10.803017	-6.840212	0.260250
-10.921316	-27.179807	0.265254
-10.658793	-16.957850	0.270259
-11.610397	-18.723695	0.275264
-11.882632	-21.465316	0.280269
-12.658910	-12.903873	0.285274
-12.359568	-19.341034	0.290278
-12.710022	-15.812802	0.295283
-12.518283	-22.125645	0.300288
-13.021568	-24.201728	0.305293
-13.631684	-20.838705	0.310298
-13.785122	-22.096094	0.315302
-13.763552	-12.833165	0.320307
-13.954537	-14.831327	0.325312
-13.949372	-15.173811	0.330317
-14.613448	-13.352567	0.335322
-14.951998	-22.699028	0.340326
-14.876985	-11.498783	0.345331
-15.010087	-20.864578	0.350336
-15.302011	-16.352077	0.355341
-16.408976	-16.682751	0.360346
-15.839211	-21.143614	0.365350
-16.351085	-18.877850	0.370355
-16.336117	-14.833895	0.375360
-16.447676	-13.943368	0.380365
-17.287467	-5.995270	0.385370
-17.655869	-12.610031	0.390374
-18.095087	-10.406196	0.395379
-18.275683	-14.538269	0.400384
-17.987415	-13.839703	0.405389
-18.573950	-2.337141	0.410394
-18.007173	-16.044858	0.415398
-18.442641	-13.199389	0.420403
-18.980742	-14.162779	0.425408
-19.039159	-20.370237	0.430413
-19.763347	-10.965886	0.435418
-19.842450	-22.500853	0.440422
-20.706808	-6.516455	0.445427
-20.867268	-13.641302	0.450432
-21.107172	-9.257117	0.455437
-20.939324	-12.788568	0.460442
-21.150537	-14.160344	0.465446
-21.068945	-6.482249	0.470451
-21.400040	-9.508925	0.475456
-21.354424	-18.779165	0.480461
-21.760247	-17.371440	0.485466
-21.687886	-17.582022	0.490470
-22.062071	-14.113368	0.495475
-23.205047	-7.892866	0.500480
-23.069120	-12.491821	0.505485
-23.811359	-16.653501	0.510490
-23.494408	-17.427329	0.515494
-23.639765	-13.839284	0.520499
-24.010076	-11.684142	0.525504
-24.104786	-27.560349	0.530509
-24.872803	-11.432775	0.535514
-25.110999	-23.091662	0.540518
-25.149472	-13.060112	0.545523
-25.205185	-8.821660	0.550528
-25.362779	-12.245495	0.555533
-26.158848	-17.332066	0.560538
-26.601647	-17.566839	0.565542
-26.668359	-12.320638	0.570547
-26.567505	-11.684638	0.575552
-26.597084	-20.297787	0.580557
-26.691365	-15.180168	0.585562
-27.271194	-19.607570	0.590566
-27.996957	-15.774139	0.595571
-28.000163	-14.372155	0.600576
-28.275164	-8.963814	0.605581
-28.423119	-18.808170	0.610586
-28.448623	-18.434060	0.615590
-28.321389	-13.366748	0.620595
-28.957673	-11.334703	0.625600
-29.631448	-13.358933	0.630605
-29.998055	-15.804296	0.635610
-29.819930	-17.628982	0.640614
-30.147647	-18.811782	0.645619
-30.563231	-12.625445	0.650624
-30.884400	-26.046211	0.655629
-31.419272	-13.691193	0.660634
-31.494008	-9.101779	0.665638
-31.438111	-17.731401	0.670643
-31.430965	-10.041717	0.675648
-31.464205	-10.261166	0.680653
-31.509132	-15.809525	0.685658
-32.222018	-23.560173	0.690662
-32.642317	-12.861757	0.695667
-32.967806	-15.063595	0.700672
-32.715070	-17.886953	0.705677
-33.505330	-12.683116	0.710682
-33.793044	-13.963890	0.715686
-34.347714	-21.543027	0.720691
-34.239263	-16.615155	0.725696
-34.180687	-18.611046	0.730701
-34.462053	-12.663897	0.735706
-34.547234	-17.598569	0.740710
-35.253978	-14.907009	0.745715
-35.565036	-5.908652	0.750720
-35.273060	-13.319068	0.755725
-35.565097	-14.516915	0.760730
-36.207572	-15.264744	0.765734
-37.023609	-1.530886	0.770739
-37.260579	-12.826150	0.775744
-37.064323	-13.011731	0.780749
-37.317684	-12.304762	0.785754
-37.164353	-18.744498	0.790758
-37.312906	-12.384610	0.795763
-37.320284	-13.133250	0.800768
-38.266037	-16.912078	0.805773
-38.809390	-5.330825	0.810778
-38.610966	-8.999910	0.815782
-38.789957	-11.803504	0.820787
-39.120444	-13.628091	0.825792
-38.877627	-15.478668	0.830797
-39.667686	-4.627767	0.835802
-39.895790	-18.227537	0.840806
-40.234644	-10.597873	0.845811
-40.396400	-14.881568	0.850816
-40.239527	-16.203091	0.855821
-40.937015	-6.704823	0.860826
-41.081397	-20.248026	0.865830
-41.260178	-15.756305	0.870835
-41.524262	-25.076393	0.875840
-41.789173	-24.174645	0.880845
-42.731924	-1.784332	0.885850
-42.604313	-11.197050	0.890854
-43.083018	-9.584994	0.895859
-43.198895	-16.947725	0.900864
-42.791111	-16.748641	0.905869
-43.239344	-12.464893	0.910874
-43.138445	-14.720465	0.915878
-43.842817	-7.283816	0.920883
-44.415643	-14.904420	0.925888
-44.126826	-15.597940	0.930893
-44.652106	-8.644741	0.935898
-45.045938	-13.556666	0.940902
-45.707747	-15.839012	0.945907
-45.977713	-17.024476	0.950912
-45.566155	-15.389689	0.955917
-46.081897	-16.366050	0.960922
-46.016591	-8.267821	0.965926
-46.279153	-12.478876	0.970931
-45.991287	-16.414976	0.975936
-46.254024	-24.561565	0.980941
-47.034499	-5.401285	0.985946
-47.144527	-14.821292	0.990950
-48.081421	-19.512626	0.995955
-48.889859	-10.167921	1.000960
-48.253857	-11.073680	1.005965
-48.297784	-10.475247	1.010970
-48.534948	-10.216872	1.015974
-49.057845	-15.073902	1.020979
-49.110651	-14.065978	1.025984
-49.057960	-10.081677	1.030989
-49.727049	-2.916267	1.035994
-50.093695	-10.132391	1.040998
-50.433203	-9.513246	1.046003
-50.760940	-14.868880	1.051008
-50.671932	-10.270162	1.056013
-51.006330	-7.231628	1.061018
-50.563610	-7.329039	1.066022
-51.554837	-3.343546	1.071027
-51.651663	-2.322439	1.076032
-51.796160	-8.763261	1.081037
-52.197874	-6.021120	1.086042
-52.093326	-12.586134	1.091046
-53.027505	-5.740105	1.096051
-53.608235	-7.778821	1.101056
-53.359289	-14.426427	1.106061
-54.147744	-10.735089	1.111066
-53.669846	-14.593213	1.116070
-53.788342	-9.851460	1.121075
-53.626857	-7.352026	1.126080
-53.658954	-10.706818	1.131085
-54.443503	-9.040816	1.136090
-54.607143	-10.603490	1.141094
-54.732365	-11.042727	1.146099
-56.252045	-8.136010	1.151104
-56.529157	-10.848399	1.156109
-55.981802	-3.923006	1.161114
-56.210215	-16.864690	1.166118
-56.304064	-12.155247	1.171123
-56.714515	-13.337820	1.176128
-56.545940	-15.170510	1.181133
-56.853716	-1.531607	1.186138
-57.030507	-14.269367	1.191142
-57.605053	-17.299262	1.196147
-57.894789	-15.106048	1.201152
-57.763803	-16.296994	1.206157
-58.667352	-6.405989	1.211162
-58.750398	-15.159504	1.216166
-59.100993	-13.750887	1.221171
-59.373778	-14.828348	1.226176
-59.226803	-18.230002	1.231181
-59.801829	-11.933422	1.236186
-60.516322	-18.829638	1.241190
-60.759562	-9.174316	1.246195
-60.503390	-11.874827	1.251200
-60.666475	-7.898058	1.256205
-61.246258	-12.641831	1.261210
-60.933877	-10.181710	1.266214
-61.215889	-2.652640	1.271219
-61.387233	-9.570154	1.276224
-62.106340	-14.080270	1.281229
-62.610310	-5.744715	1.286234
-62.546495	-7.526294	1.291238
-62.791907	-6.371326	1.296243
-62.939614	-4.019897	1.301248
-63.015756	-12.015215	1.306253
-63.176460	-6.798671	1.311258
-63.425768	-9.202188	1.316262
-63.878356	-8.748927	1.321267
-63.897525	-0.045943	1.326272
-64.598625	-15.065305	1.331277
-65.070293	-12.211036	1.336282
-65.488401	-7.036669	1.341286
-65.715202	3.590500	1.346291
-65.677477	4.087639	1.351296
-65.276898	-14.807875	1.356301
-65.789627	-2.215864	1.361306
-65.791902	-7.384901	1.366310
-66.608711	-12.202495	1.371315
-66.863282	-9.638283	1.376320
-66.785617	-8.925909	1.381325
-67.200637	-11.632643	1.386330
-67.324351	-9.288114	1.391334
-67.498116	-6.214482	1.396339
-68.238741	-6.618010	1.401344
-68.120355	-23.527103	1.406349
-68.479962	-9.415084	1.411354
-68.634984	-14.269282	1.416358
-68.488535	-5.497179	1.421363
-69.194043	-11.452031	1.426368
-69.254916	-16.355687	1.431373
-69.985438	-8.468896	1.436378
-69.828474	-11.305815	1.441382
-69.790967	-16.370316	1.446387
-70.660483	-11.897593	1.451392
-71.022135	-17.883836	1.456397
-71.110903	-14.326749	1.461402
-70.968632	-16.474870	1.466406
-71.047369	0.643171	1.471411
-71.659741	-0.963527	1.476416
-72.373937	-9.435283	1.481421
-72.615543	-4.946434	1.486426
-72.657679	-5.990207	1.491430
-72.804904	-4.803072	1.496435
-72.838352	-15.940200	1.501440
-72.959063	-14.241521	1.506445
-73.637557	-1.592063	1.511450
-74.016065	-2.982083	1.516454
-74.187969	-11.968527	1.521459
-74.543334	-12.099858	1.526464
-74.249750	-10.424556	1.531469
-74.524640	-7.249762	1.536474
-74.474012	-9.003979	1.541478
-75.428015	-13.047266	1.546483
-75.569955	-15.144809	1.551488
-75.588526	-8.279995	1.556493
-75.641317	-11.783419	1.561498
-76.322964	-12.939584	1.566502
-76.822625	-17.002993	1.571507
-77.361526	-18.393347	1.576512
-77.371472	-13.573587	1.581517
-77.455640	-10.001398	1.586522
-77.653773	-15.778991	1.591526
-77.509434	-9.651362	1.596531
-77.305269	-9.676829	1.601536
-78.221719	-11.704399	1.606541
-78.713427	-9.606283	1.611546
-78.973591	-11.242509	1.616550
-78.710093	-11.511324	1.621555
-78.506647	-15.241298	1.626560
-79.042202	-16.461336	1.631565
-80.283785	-10.007192	1.636570
-80.223290	-10.728436	1.641574
-80.135929	-17.853898	1.646579
-80.015701	-12.548225	1.651584
-80.655512	-22.179956	1.656589
-81.368226	-16.630704	1.661594
-81.673339	-21.515311	1.666598
-82.027447	-12.355240	1.671603
-81.915020	-9.224932	1.676608
-81.793949	-13.103426	1.681613
-82.148701	-5.009396	1.686618
-82.008375	-11.421798	1.691622
-82.726860	-5.457208	1.696627
-83.235788	-7.440666	1.701632
-83.320321	-14.697547	1.706637
-83.451878	-0.500812	1.711642
-83.572500	-10.102659	1.716646
-84.329574	-11.319844	1.721651
-84.815732	-7.441464	1.726656
-84.686901	-8.426438	1.731661
-84.996335	-11.083175	1.736666
-84.759186	-5.355959	1.741670
-84.789521	-3.228441	1.746675
-84.954536	-8.628393	1.751680
-85.742793	-15.136650	1.756685
-86.285695	-4.618452	1.761690
-86.219353	-11.683699	1.766694
-86.456299	-6.414157	1.771699
-86.741416	-8.233153	1.776704
-87.356923	-12.677143	1.781709
-87.591786	-9.429490	1.786714
-87.503102	-6.146795	1.791718
-87.795165	-9.059328	1.796723
-88.038458	-0.514432	1.801728
-88.008505	-16.603032	1.806733
-88.201644	-9.005549	1.811738
-88.686928	-16.063996	1.816742
-89.080450	-11.349022	1.821747
-89.322598	-10.659617	1.826752
-89.356172	-11.473778	1.831757
-89.848205	-3.744336	1.836762
-89.945587	-9.708455	1.841766
-90.516361	-11.948028	1.846771
-90.983017	-10.423266	1.851776
-90.830236	-21.630512	1.856781
-91.013068	-8.302127	1.861786
-91.003210	-13.966578	1.866790
-91.251579	-21.387765	1.871795
-91.888520	-22.335762	1.876800
-92.178422	-16.494852	1.881805
-92.661836	-18.491771	1.886810
-92.682123	-19.542109	1.891814
-92.709483	-16.725384	1.896819
-92.664769	-9.231371	1.901824
-93.275724	-21.028358	1.906829
-93.853399	-17.154713	1.911834
-93.652992	-15.265596	1.916838
-93.484181	-13.567705	1.921843
-93.794044	-14.054120	1.926848
-94.500193	-12.757815	1.931853
-95.275861	-2.181229	1.936858
-95.195335	-10.210430	1.941862
-95.224621	-7.608531	1.946867
-95.595869	-14.653097	1.951872
-95.380378	-18.954400	1.956877
-96.149444	-10.226409	1.961882
-96.590363	-13.254964	1.966886
-96.990687	-11.177404	1.971891
-97.071987	-16.109514	1.976896
-96.339031	-16.384988	1.981901
-96.737046	-8.220951	1.986906
-97.580104	-20.443690	1.991910
-98.064256	-15.800025	1.996915
-98.429003	-6.900887	2.006912
-97.382554	-11.894556	2.016909
-97.145277	-10.423694	2.026906
-97.109857	-3.168881	2.036902
-96.409728	-9.537255	2.046899
-95.793843	-5.426472	2.056896
-95.603299	-12.542270	2.066893
-94.754080	-8.334775	2.076890
-94.322603	-8.680725	2.086886
-93.841596	-13.101698	2.096883
-93.184207	-16.941936	2.106880
-92.917115	-8.408607	2.116877
-92.489906	-8.142529	2.126874
-92.066825	-9.697229	2.136870
-91.317424	-18.087921	2.146867
-90.520843	-6.551706	2.156864
-90.593439	-6.892029	2.166861
-89.464995	-10.051703	2.176858
-88.930504	-13.353306	2.186854
-88.842847	-13.439823	2.196851
-88.504904	-10.229736	2.206848
-87.794929	-13.070839	2.216845
-87.413212	-11.422901	2.226842
-86.805589	-14.317756	2.236838
-86.028157	-18.693018	2.246835
-85.649755	-14.054269	2.256832
-85.605912	-17.852829	2.266829
-85.078366	-13.031402	2.276826
-84.375084	-12.966693	2.286822
-83.428515	-11.238816	2.296819
-82.786215	-13.990189	2.306816
-82.836713	-8.575097	2.316813
-83.052112	-19.213509	2.326810
-82.009331	-17.563966	2.336806
-80.719327	-16.748005	2.346803
-80.583868	-17.013020	2.356800
-80.383125	-8.260292	2.366797
-80.417419	-8.663597	2.376794
-79.226155	-3.970850	2.386790
-78.735066	-18.403284	2.396787
-78.095210	-17.093302	2.406784
-77.760491	-15.114944	2.416781
-77.425869	-14.872462	2.426778
-76.742561	-12.542914	2.436774
-76.135388	-11.680822	2.446771
-75.888341	-10.398374	2.456768
-75.237347	-13.547062	2.466765
-74.697621	-6.225056	2.476762
-74.250256	-4.805909	2.486758
-73.813412	-9.574788	2.496755
-73.363621	-8.070492	2.506752
-72.782195	-14.664295	2.516749
-72.061531	-9.388278	2.526746
-71.690505	-8.597119	2.536742
-71.441824	-14.214149	2.546739
-70.648660	-12.189966	2.556736
-70.647351	-5.534869	2.566733
-69.555252	-0.956555	2.576730
-69.032023	-4.997646	2.586726
-69.089177	-10.506873	2.596723
-68.264015	-8.126554	2.606720
-67.441997	-4.383639	2.616717
-67.285647	-12.317713	2.626714
-66.779906	-19.324200	2.636710
-66.206583	-13.531085	2.646707
-66.010796	-16.491692	2.656704
-64.986377	-10.524898	2.666701
-64.755181	-10.320164	2.676698
-64.379343	-11.832663	2.686694
-63.646488	-11.791564	2.696691
-63.262543	-13.432033	2.706688
-62.673093	-11.993829	2.716685
-61.983274	-4.137677	2.726682
-62.006716	-9.525446	2.736678
-61.278812	-7.712839	2.746675
-60.320719	-9.933694	2.756672
-60.147615	-4.829003	2.766669
-60.000104	-16.303175	2.776666
-58.871720	-9.975614	2.786662
-58.677309	-15.957981	2.796659
-58.599700	-12.007301	2.806656
-57.803158	-12.983442	2.816653
-57.472824	-8.812359	2.826650
-56.388473	-10.675917	2.836646
-55.819089	-6.592737	2.846643
-55.855897	-13.986738	2.856640
-55.435181	-11.720838	2.866637
-54.747336	-11.875463	2.876634
-54.644777	-15.999934	2.886630
-53.392637	-7.711835	2.896627
-53.018970	-6.984441	2.906624
-53.036989	-7.567670	2.916621
-52.336075	-9.178299	2.926618
-51.692765	-10.095738	2.936614
-50.877244	-9.513164	2.946611
-50.499545	-12.980416	2.956608
-50.108187	-7.947720	2.966605
-49.954552	-12.567969	2.976602
-48.884236	-13.513880	2.986598
-48.652034	-19.999458	2.996595
-48.358728	-22.376555	3.006592
-47.630930	-13.813590	3.016589
-47.448870	-15.875605	3.026586
-46.679647	-17.237118	3.036582
-45.919985	-22.205137	3.046579
-45.746207	-20.569171	3.056576
-45.361258	-14.708713	3.066573
-44.594318	-19.209048	3.076570
-44.422833	-16.844157	3.086566
-43.605157	-21.368230	3.096563
-43.043902	-14.461376	3.106560
-42.922041	-17.717739	3.116557
-42.221426	-15.226165	3.126554
-41.595103	-17.487226	3.136550
-41.307418	-18.038860	3.146547
-40.235640	-13.017074	3.156544
-40.214831	-14.692866	3.166541
-39.738183	-14.200076	3.176538
-39.315443	-13.553179	3.186534
-38.427523	-13.754793	3.196531
-38.425318	-15.326322	3.206528
-37.184162	-11.236866	3.216525
-36.744045	-14.447751	3.226522
-36.837670	-14.594739	3.236518
-36.625710	-9.306036	3.246515
-35.850278	-5.844126	3.256512
-35.145991	-5.282244	3.266509
-34.410130	-11.456619	3.276506
-34.122816	-7.383370	3.286502
-34.131162	-10.584617	3.296499
-33.134048	-11.221367	3.306496
-32.601207	-12.409865	3.316493
-31.734549	-7.131234	3.326490
-31.556295	-11.200972	3.336486
-31.381562	-11.662164	3.346483
-30.850748	-12.004573	3.356480
-29.791595	-12.502101	3.366477
-29.834171	-10.300276	3.376474
-29.398550	-13.710026	3.386470
-28.230001	-18.500965	3.396467
-28.040415	-17.133546	3.406464
-27.770112	-17.194650	3.416461
-26.889790	-11.747093	3.426458
-26.467902	-14.913959	3.436454
-26.328777	-15.787742	3.446451
-25.517186	-19.785032	3.456448
-25.065408	-16.880926	3.466445
-24.796944	-16.045289	3.476442
-24.458126	-15.429672	3.486438
-23.806027	-21.939447	3.496435
-22.967838	-14.765276	3.506432
-22.481484	-16.440695	3.516429
-22.530166	-16.189217	3.526426
-21.263601	-16.595498	3.536422
-20.805015	-19.565345	3.546419
-20.786338	-15.472446	3.556416
-20.297258	-18.513563	3.566413
-19.707361	-21.779444	3.576410
-19.198808	-19.790137	3.586406
-18.250299	-20.653727	3.596403
-17.849888	-21.368627	3.606400
-17.958860	-24.300789	3.616397
-17.366155	-13.220650	3.626394
-16.602332	-22.202779	3.636390
-16.276282	-20.261081	3.646387
-15.183685	-19.059599	3.656384
-15.027335	-16.400924	3.666381
-14.833553	-17.390917	3.676378
-14.058754	-20.207266	3.686374
-13.776903	-13.298087	3.696371
-13.187837	-18.936438	3.706368
-12.231523	-16.690573	3.716365
-12.090778	-24.213584	3.726362
-12.026794	-16.351855	3.736358
-11.052857	-21.454603	3.746355
-10.552099	-14.126527	3.756352
-9.600872	-16.263952	3.766349
-9.308873	-13.334968	3.776346
-9.151607	-11.639411	3.786342
-8.769375	-13.282781	3.796339
-8.255490	-15.035344	3.806336
-7.803966	-14.329574	3.816333
-7.001480	-14.761797	3.826330
-6.554884	-13.846192	3.836326
-6.254412	-2.970792	3.846323
-5.796502	-5.804326	3.856320
-5.477111	-5.521459	3.866317
-4.502842	4.438108	3.876314
-4.214149	10.133006	3.886310
-4.041087	18.427581	3.896307
-3.390595	22.776901	3.906304
-3.152439	35.166682	3.916301
-2.597867	46.240127	3.926298
-1.964363	60.978992	3.936294
-1.631960	71.073379	3.946291
-1.263109	90.430807	3.956288
-0.501991	102.859586	3.966285
0.000000	123.558673	3.971290
-0.315041	127.555969	3.976294
0.339310	133.765593	3.981299
0.418045	140.105967	3.986304
0.667458	136.732625	3.991309
0.723251	141.823761	3.996314
0.408564	139.756258	4.001318
0.533408	142.359492	4.006323
0.798187	142.745356	4.011328
0.915852	134.640700	4.016333
0.617396	146.171269	4.021338
0.606418	148.548886	4.026342
0.661225	144.687000	4.031347
0.853634	147.988378	4.036352
0.572791	140.360206	4.041357
0.572445	151.683018	4.046362
0.675809	140.473865	4.051366
0.627523	142.699106	4.056371
0.870774	155.505716	4.061376
0.925855	157.737011	4.066381
0.965787	170.771435	4.071386
1.182780	151.470897	4.076390
0.921989	152.799107	4.081395
0.947495	150.336960	4.086400
0.838621	139.837877	4.091405
0.964825	144.649139	4.096410
0.599312	139.470175	4.101414
0.915102	143.454675	4.106419
1.187258	153.940980	4.111424
1.331124	146.351081	4.116429
0.985421	149.967189	4.121434
0.782376	147.208441	4.126438
1.078450	133.637666	4.131443
0.858525	140.214360	4.136448
1.089463	141.870959	4.141453
0.846565	158.616100	4.146458
1.173944	157.419873	4.151462
0.766312	165.348216	4.156467
1.184537	175.489097	4.161472
1.212521	164.857962	4.166477
0.994599	169.570954	4.171482
1.342100	175.050105	4.176486
1.499682	170.666024	4.181491
1.183317	161.240082	4.186496
1.114163	148.640460	4.191501
1.129325	162.368415	4.196506
1.184552	156.595604	4.201510
1.385730	163.783769	4.206515
1.026613	155.449625	4.211520
1.329045	166.228608	4.216525
1.498184	168.081487	4.221530
1.160595	152.040456	4.226534
1.309438	159.777755	4.231539
1.395004	165.955728	4.236544
1.553430	147.885488	4.241549
1.287915	150.090770	4.246554
1.024208	151.036631	4.251558
1.149401	157.227414	4.256563
1.158434	174.214910	4.261568
1.467719	175.144324	4.266573
1.665333	169.108902	4.271578
1.490210	163.849668	4.276582
1.234668	160.032935	4.281587
1.066603	168.082163	4.286592
1.436491	170.134735	4.291597
1.311400	168.075673	4.296602
1.431475	165.649418	4.301606
1.626578	161.635974	4.306611
1.730769	168.054651	4.311616
1.795007	156.471939	4.316621
1.510923	160.464423	4.321626
1.531951	153.463107	4.326630
1.178682	153.571886	4.331635
0.984480	161.833983	4.336640
1.345250	163.698153	4.341645
1.680755	170.460456	4.346650
1.373765	167.562870	4.351654
1.790467	170.468671	4.356659
1.432282	173.124971	4.361664
1.701964	158.995152	4.366669
1.572774	166.418247	4.371674
1.504784	163.916872	4.376678
1.811716	159.484232	4.381683
1.665063	157.700604	4.386688
1.713033	161.941936	4.391693
1.454882	171.270660	4.396698
1.277353	173.180678	4.401702
1.152894	172.212984	4.406707
1.198024	174.638815	4.411712
1.672518	178.291737	4.416717
2.023254	197.655756	4.421722
2.068097	198.939547	4.426726
1.871861	176.561789	4.431731
1.417275	167.419949	4.436736
1.783785	177.515100	4.441741
1.907051	195.060620	4.446746
2.257319	188.153558	4.451750
2.110515	176.600528	4.456755
1.638230	170.077799	4.461760
1.678869	167.129252	4.466765
1.712056	170.515533	4.471770
2.037484	175.580516	4.476774
2.058963	171.318863	4.481779
1.775809	171.094031	4.486784
1.939476	168.252875	4.491789
1.940562	190.208589	4.496794
2.078736	180.721357	4.501798
2.214740	171.933639	4.506803
1.779162	177.904863	4.511808
2.220700	167.990764	4.516813
1.888612	176.296482	4.521818
1.860011	174.070540	4.526822
1.599665	167.223756	4.531827
1.809475	193.996884	4.536832
2.268983	195.703320	4.541837
2.485182	201.133321	4.546842
2.392189	185.864078	4.551846
2.181425	173.046048	4.556851
1.907680	175.426616	4.561856
2.127993	170.055194	4.566861
2.161208	172.742300	4.571866
1.965110	176.224392	4.576870
2.161795	174.191158	4.581875
1.986236	183.513356	4.586880
2.475658	178.096868	4.591885
2.042353	180.163767	4.596890
2.143708	175.329707	4.601894
2.111331	179.801847	4.606899
2.294004	192.937447	4.611904
2.404401	186.301844	4.616909
2.418341	188.976136	4.621914
2.138031	175.991766	4.626918
2.213844	169.968980	4.631923
1.955639	179.832377	4.636928
2.733939	183.251342	4.641933
2.428956	193.261231	4.646938
2.043034	195.042351	4.651942
2.217520	185.989214	4.656947
2.414758	204.057886	4.661952
2.774285	196.845666	4.666957
2.286437	188.022198	4.671962
2.361492	185.871862	4.676966
2.534590	173.595164	4.681971
1.928770	180.478722	4.686976
2.348507	177.531258	4.691981
2.153420	197.416846	4.696986
2.199929	201.582487	4.701990
2.365419	191.024838	4.706995
2.129492	199.179556	4.712000
2.329364	189.271436	4.717005
2.366176	201.047226	4.722010
2.297425	198.141014	4.727014
2.192169	192.187540	4.732019
2.075875	200.598872	4.737024
2.671330	213.853712	4.742029
2.474380	225.466602	4.747034
2.848015	231.172650	4.752038
3.042385	217.057674	4.757043
2.762736	213.462977	4.762048
2.876909	211.917137	4.767053
2.780044	206.319847	4.772058
2.411493	205.067461	4.777062
2.668831	196.346259	4.782067
2.346412	198.807174	4.787072
2.485495	199.930763	4.792077
2.676198	198.505884	4.797082
2.379179	201.370958	4.802086
2.549668	207.168737	4.807091
2.641077	222.226265	4.812096
2.752428	219.896272	4.817101
2.621879	232.394150	4.822106
2.774310	227.172481	4.827110
2.828849	222.991088	4.832115
2.600058	227.800699	4.837120
3.070203	225.376877	4.842125
2.793803	230.709581	4.847130
2.795934	240.504004	4.852134
3.216752	225.758992	4.857139
2.691991	228.631056	4.862144
2.992726	224.597988	4.867149
2.962473	229.961968	4.872154
2.793991	221.914480	4.877158
2.735513	228.883676	4.882163
2.536547	221.818512	4.887168
2.710390	221.978096	4.892173
2.940382	228.529064	4.897178
2.859898	230.234159	4.902182
2.745113	223.200179	4.907187
2.759485	225.868081	4.912192
2.872582	223.474542	4.917197
2.992334	227.052996	4.922202
3.141307	228.962804	4.927206
3.100124	225.979531	4.932211
3.020309	225.061829	4.937216
3.292825	225.620492	4.942221
2.986643	226.886175	4.947226
2.851222	228.773825	4.952230
2.862706	228.648647	4.957235
2.712210	230.263404	4.962240
3.148988	224.731715	4.967245
2.600888	227.790907	4.972250
3.135898	237.464397	4.977254
3.215453	245.168229	4.982259
3.376614	249.268576	4.987264
3.491652	246.849421	4.992269
3.203394	243.116856	4.997274
3.086048	243.131957	5.002278
3.307766	245.024113	5.007283
3.111043	251.252395	5.012288
3.312289	246.311016	5.017293
3.272642	251.610028	5.022298
3.038889	256.486856	5.027302
3.361549	248.454633	5.032307
3.462957	260.441863	5.037312
3.391191	249.209290	5.042317
3.282377	242.016188	5.047322
3.048157	250.825547	5.052326
3.602412	250.078034	5.057331
3.165965	247.713108	5.062336
3.595102	252.537344	5.067341
3.455358	253.213978	5.072346
3.281562	252.367854	5.077350
3.388421	252.809944	5.082355
3.140076	266.088634	5.087360
3.275651	258.588562	5.092365
3.499422	256.373935	5.097370
3.199596	262.921988	5.102374
3.142305	251.019621	5.107379
3.300187	262.536162	5.112384
3.399957	257.446068	5.117389
3.478018	259.781363	5.122394
3.700398	250.065853	5.127398
3.774991	257.194672	5.132403
3.254907	252.422546	5.137408
3.330383	255.856043	5.142413
3.207809	251.116937	5.147418
3.194069	248.736815	5.152422
3.443204	251.494717	5.157427
3.567602	263.778920	5.162432
3.353396	279.693984	5.167437
3.605741	275.820296	5.172442
3.877790	283.098713	5.177446
4.065136	278.535968	5.182451
3.516637	263.106630	5.187456
3.759643	257.130548	5.192461
3.471102	257.175466	5.197466
3.645220	272.856061	5.202470
3.937806	282.766634	5.207475
3.801324	277.134362	5.212480
3.722699	255.839157	5.217485
3.545122	259.125396	5.222490
3.544900	270.628593	5.227494
4.234027	269.442475	5.232499
3.752871	273.152461	5.237504
3.879705	262.996249	5.242509
3.910375	254.920902	5.247514
3.560905	253.849035	5.252518
3.696083	256.355767	5.257523
3.493852	284.313130	5.262528
3.854619	277.195595	5.267533
3.834354	274.152111	5.272538
3.816779	287.796676	5.277542
4.110586	275.985158	5.282547
3.638358	279.405860	5.287552
4.063850	276.739052	5.292557
4.089376	279.810179	5.297562
3.695874	275.534020	5.302566
3.858623	281.601942	5.307571
4.168428	277.643378	5.312576
4.259424	266.107048	5.317581
4.183484	275.647897	5.322586
4.004568	282.041092	5.327590
4.151732	283.498780	5.332595
4.131076	284.881360	5.337600
4.132457	281.179619	5.342605
4.310949	279.971766	5.347610
4.310247	275.295935	5.352614
4.072081	261.143867	5.357619
3.996001	259.181565	5.362624
4.079622	269.251212	5.367629
4.043044	264.555660	5.372634
4.281235	282.349122	5.377638
3.947265	275.985149	5.382643
4.242440	283.076471	5.387648
4.297041	276.629853	5.392653
4.016769	285.202795	5.397658
4.041905	283.911253	5.402662
4.432982	278.519538	5.407667
4.217377	277.091475	5.412672
4.386924	277.061907	5.417677
4.463686	283.924650	5.422682
3.997264	277.018162	5.427686
4.551590	279.776006	5.432691
3.914156	285.174429	5.437696
3.733703	279.428782	5.442701
4.546376	280.102659	5.447706
4.130989	277.819869	5.452710
3.985622	276.459963	5.457715
3.819246	285.837731	5.462720
4.094037	282.276916	5.467725
4.210044	287.776326	5.472730
4.107776	279.060454	5.477734
4.290577	289.801192	5.482739
4.572142	303.759855	5.487744
4.777056	294.698761	5.492749
4.270877	294.034097	5.497754
4.499638	278.841226	5.502758
4.283915	277.650459	5.507763
4.314852	286.823504	5.512768
4.486108	293.874014	5.517773
4.466506	301.074463	5.522778
4.278665	309.247054	5.527782
4.668710	298.208297	5.532787
4.488019	309.220773	5.537792
4.514547	301.503547	5.542797
4.596487	300.794770	5.547802
4.680250	304.581320	5.552806
4.472439	294.635377	5.557811
4.266842	311.754497	5.562816
4.253092	296.108996	5.567821
4.514506	298.738447	5.572826
4.850351	309.331984	5.577830
4.590327	300.115490	5.582835
4.279502	299.951911	5.587840
4.777982	305.996042	5.592845
4.750926	310.964087	5.597850
4.409048	321.058884	5.602854
4.600419	302.233563	5.607859
4.610076	310.903742	5.612864
4.920981	303.461772	5.617869
4.729294	305.614450	5.622874
4.904252	298.835879	5.627878
4.760806	302.844462	5.632883
4.677231	309.659413	5.637888
4.833459	310.558881	5.642893
4.632415	302.503772	5.647898
4.471961	309.678699	5.652902
4.998889	307.246026	5.657907
5.327592	316.913717	5.662912
4.838237	310.235409	5.667917
4.702464	303.182519	5.672922
4.786962	311.284235	5.677926
4.837202	313.345464	5.682931
4.932332	313.466686	5.687936
4.953293	310.454740	5.692941
4.979437	320.859227	5.697946
5.077699	320.929341	5.702950
5.024647	313.616799	5.707955
4.787463	315.494993	5.712960
4.961412	325.730939	5.717965
4.861234	321.402772	5.722970
4.941981	330.365608	5.727974
5.616755	328.115553	5.732979
4.657575	324.411502	5.737984
5.252836	319.218935	5.742989
4.879708	320.681705	5.747994
5.065090	323.905117	5.752998
5.366165	323.484918	5.758003
5.089588	320.164962	5.763008
4.911419	314.564479	5.768013
4.818879	320.668998	5.773018
5.044588	329.792757	5.778022
5.232782	328.678301	5.783027
5.389389	326.464632	5.788032
5.570162	322.197124	5.793037
5.249052	331.244673	5.798042
5.246901	329.894102	5.803046
4.829227	310.113249	5.808051
5.051574	324.891055	5.813056
5.326950	322.949955	5.818061
5.371474	329.586784	5.823066
5.347921	320.478992	5.828070
5.521834	318.575836	5.833075
5.646980	324.437659	5.838080
5.119063	317.325599	5.843085
5.379724	308.179890	5.848090
5.365841	311.867751	5.853094
5.069621	310.556639	5.858099
5.348940	328.796153	5.863104
5.471088	314.088079	5.868109
5.527418	320.251675	5.873114
5.407820	328.410486	5.878118
5.593343	323.854341	5.883123
5.134029	320.936154	5.888128
5.192083	316.368220	5.893133
5.448608	325.563108	5.898138
5.443982	316.094874	5.903142
5.418844	314.871268	5.908147
5.409981	330.371599	5.913152
5.640343	326.121679	5.918157
5.451604	319.162449	5.923162
5.277771	320.100652	5.928166
5.636807	323.948749	5.933171
5.539191	332.493274	5.938176
5.047127	322.018944	5.943181
5.441137	323.833665	5.948186
5.301004	326.357962	5.953190
5.393687	322.376248	5.958195
5.039952	324.044803	5.963200
5.266704	326.154480	5.968205
5.745798	335.197663	5.973210
5.366735	348.528403	5.978214
5.660303	345.556265	5.983219
5.765920	354.268471	5.988224
5.855994	351.862681	5.993229
5.863690	344.958276	5.998234
5.334663	333.423527	6.003238
5.606551	329.888464	6.008243
5.634493	347.195879	6.013248
5.627457	347.260243	6.018253
5.644806	356.185506	6.023258
5.832484	342.606139	6.028262
5.749748	335.959423	6.033267
5.689783	325.117263	6.038272
5.528125	320.558228	6.043277
5.406926	330.204227	6.048282
5.725092	338.453069	6.053286
6.006656	335.065193	6.058291
5.499475	335.539615	6.063296
5.686022	326.364308	6.068301
5.413350	328.947206	6.073306
5.494276	330.908748	6.078310
5.865995	340.674157	6.083315
5.229462	332.262902	6.088320
5.887822	339.490685	6.093325
6.203869	341.478895	6.098330
5.830883	339.227460	6.103334
5.625096	330.157527	6.108339
5.555767	335.473840	6.113344
5.462318	322.400159	6.118349
5.979446	326.290080	6.123354
5.837996	327.163132	6.128358
5.919255	320.962279	6.133363
5.489711	322.775512	6.138368
5.615330	323.407670	6.143373
5.749059	321.102652	6.148378
5.579428	326.276394	6.153382
5.646329	315.582163	6.158387
5.714058	326.799576	6.163392
5.595136	329.965966	6.168397
5.947957	322.463680	6.173402
5.342333	337.076184	6.178406
5.500926	317.607391	6.183411
5.347501	328.289772	6.188416
5.266185	327.157167	6.193421
5.484164	333.959977	6.198426
5.599416	323.618875	6.203430
5.613348	330.380688	6.208435
5.709761	330.720005	6.213440
5.724490	314.250656	6.218445
5.677735	325.837063	6.223450
5.589825	326.110168	6.228454
5.844585	313.339776	6.233459
5.694600	317.785970	6.238464
5.578024	324.827524	6.243469
5.799978	320.253053	6.248474
5.434479	321.667180	6.253478
5.641351	316.405372	6.258483
5.418794	323.523537	6.263488
5.470807	317.539207	6.268493
5.654559	325.309107	6.273498
5.447117	328.976488	6.278502
5.556125	320.196065	6.283507
5.352634	321.531185	6.288512
5.763713	328.202689	6.293517
5.569870	328.239191	6.298522
5.045580	330.155760	6.303526
5.725597	336.703139	6.308531
5.628516	342.463530	6.313536
5.936746	344.016366	6.318541
6.091846	341.818748	6.323546
5.746118	340.110389	6.328550
5.703892	333.213762	6.333555
5.169506	326.612060	6.338560
5.481540	330.198562	6.343565
5.840397	335.476681	6.348570
5.936009	329.707018	6.353574
5.849905	322.725479	6.358579
5.668669	332.254279	6.363584
5.653765	325.774173	6.368589
5.786768	331.562011	6.373594
5.719425	330.120351	6.378598
5.490813	318.709677	6.383603
5.437367	328.253379	6.388608
5.532221	326.998435	6.393613
5.756231	322.382515	6.398618
5.337963	321.356156	6.403622
5.532135	320.069929	6.408627
5.505215	327.980197	6.413632
5.484757	327.679661	6.418637
5.810357	337.556650	6.423642
5.472692	336.220352	6.428646
5.487484	342.975709	6.433651
5.473890	347.372202	6.438656
5.401049	347.073494	6.443661
5.660571	345.346827	6.448666
5.589191	356.693483	6.453670
6.024230	353.367128	6.458675
5.583166	358.510375	6.463680
5.855258	352.213362	6.468685
5.978711	346.679800	6.473690
5.251346	335.682122	6.478694
5.737660	333.926473	6.483699
5.738306	340.266423	6.488704
5.832630	341.570994	6.493709
5.734829	324.989444	6.498714
5.413420	325.634255	6.503718
5.528732	328.669265	6.508723
5.623806	322.475752	6.513728
5.165215	325.182507	6.518733
5.720455	329.547377	6.523738
5.934344	355.244455	6.528742
5.906518	343.112817	6.533747
5.359631	336.016357	6.538752
5.789772	331.346195	6.543757
5.804093	323.403074	6.548762
5.215351	326.747015	6.553766
5.755486	329.614643	6.558771
5.563236	334.820383	6.563776
5.435074	326.042082	6.568781
5.800279	328.266241	6.573786
5.855301	333.832107	6.578790
5.743594	328.350983	6.583795
5.614040	330.070054	6.588800
5.481836	330.875229	6.593805
5.693033	325.748784	6.598810
5.640850	326.339023	6.603814
5.821790	329.449235	6.608819
5.700948	330.455118	6.613824
5.846341	324.747307	6.618829
5.651676	323.641841	6.623834
5.496729	328.155248	6.628838
5.944106	332.075012	6.633843
5.537441	334.836958	6.638848
5.289913	333.407534	6.643853
5.439459	315.964919	6.648858
5.379554	331.998373	6.653862
5.474666	324.014199	6.658867
5.556987	339.683836	6.663872
5.916318	347.230259	6.668877
5.739129	332.382117	6.673882
5.484542	337.357122	6.678886
5.511577	330.338983	6.683891
5.630694	334.977397	6.688896
5.564748	345.525947	6.693901
5.624666	340.657166	6.698906
5.990924	348.917507	6.703910
5.388267	337.027230	6.708915
5.264725	338.720056	6.713920
5.762185	344.666285	6.718925
5.514925	346.128442	6.723930
5.355017	351.566429	6.728934
5.499586	350.933319	6.733939
5.551998	354.006599	6.738944
5.726918	355.447317	6.743949
5.848938	350.208202	6.748954
5.357408	358.374316	6.753958
5.698534	347.909448	6.758963
5.801620	353.543766	6.763968
5.786826	355.627780	6.768973
5.946110	351.917259	6.773978
6.101727	351.684219	6.778982
5.907497	337.069677	6.783987
5.907367	335.962395	6.788992
5.349752	324.185334	6.793997
5.795134	329.307613	6.799002
5.262031	325.711227	6.804006
5.625995	324.632678	6.809011
5.274828	326.734260	6.814016
5.359991	323.221944	6.819021
5.325829	331.690151	6.824026
5.316198	348.728176	6.829030
5.601923	350.300336	6.834035
5.244867	348.539956	6.839040
5.587267	354.168651	6.844045
5.727755	351.413331	6.849050
5.561909	361.657911	6.854054
5.670324	354.491053	6.859059
6.020148	355.983631	6.864064
5.961773	343.676417	6.869069
6.094893	342.162418	6.874074
5.603312	355.570793	6.879078
5.882452	343.103463	6.884083
5.481259	331.064766	6.889088
5.588722	327.944439	6.894093
5.837645	331.993176	6.899098
5.522959	332.902691	6.904102
5.797508	329.190047	6.909107
5.693896	332.157904	6.914112
5.465067	330.393381	6.919117
5.594792	325.599154	6.924122
5.283840	329.969175	6.929126
5.977135	337.814768	6.934131
5.713638	341.541499	6.939136
5.521077	333.871026	6.944141
5.575029	340.291259	6.949146
5.470216	331.521975	6.954150
5.976939	342.724831	6.959155
5.426059	345.544033	6.964160
5.934569	337.533454	6.969165
5.948660	335.193279	6.974170
5.642281	336.414707	6.979174
5.353909	335.902788	6.984179
5.523347	328.596727	6.989184
5.763516	329.154103	6.994189
5.756727	329.367121	6.999194
5.719801	324.510259	7.004198
5.632294	327.190875	7.009203
5.674869	331.085082	7.014208
5.375122	323.114931	7.019213
5.741820	331.349887	7.024218
5.322442	328.472935	7.029222
5.856881	326.235240	7.034227
5.338957	333.842313	7.039232
5.564154	322.354654	7.044237
5.707498	330.383943	7.049242
5.706492	332.744213	7.054246
5.841680	336.946699	7.059251
5.524485	339.447947	7.064256
5.458414	339.534156	7.069261
5.544654	330.440902	7.074266
5.504802	330.791944	7.079270
5.621543	336.326055	7.084275
5.822411	349.284934	7.089280
5.802215	354.887828	7.094285
5.721961	334.064174	7.099290
5.578696	333.852360	7.104294
5.599495	324.952792	7.109299
5.179073	328.662825	7.114304
5.450735	343.790467	7.119309
5.878761	355.347263	7.124314
5.703515	352.255130	7.129318
5.880410	346.744885	7.134323
5.681875	328.954662	7.139328
5.292939	336.108227	7.144333
5.745398	330.507626	7.149338
5.477568	328.973798	7.154342
5.724771	336.888845	7.159347
5.414418	344.346548	7.164352
5.593756	352.161439	7.169357
5.968437	355.143415	7.174362
5.280646	338.270904	7.179366
5.992596	337.299523	7.184371
5.816221	329.822681	7.189376
5.572406	336.820776	7.194381
5.794140	333.328322	7.199386
5.418850	328.615887	7.204390
5.715558	323.004738	7.209395
5.772483	329.263156	7.214400
5.922782	328.097654	7.219405
5.691051	325.925465	7.224410
5.696948	332.903662	7.229414
6.185644	326.601406	7.234419
5.726667	327.720045	7.239424
5.607072	332.231113	7.244429
5.590106	323.875255	7.249434
4.604342	330.704133	7.254438
5.319103	327.321576	7.259443
5.442817	333.047586	7.264448
5.789556	343.709049	7.269453
5.914411	336.871827	7.274458
5.559090	335.282019	7.279462
5.613214	322.077795	7.284467
5.640466	329.622131	7.289472
5.388957	322.014624	7.294477
5.550451	332.309460	7.299482
5.520380	344.165360	7.304486
5.412047	335.792084	7.309491
5.695879	341.578588	7.314496
5.477006	350.967727	7.319501
5.909001	350.944753	7.324506
5.727372	358.689299	7.329510
6.013958	353.399251	7.334515
5.340014	339.466827	7.339520
5.725443	341.520163	7.344525
5.652288	336.491771	7.349530
5.447628	341.022413	7.354534
5.875246	336.684831	7.359539
5.750130	336.811871	7.364544
5.728585	334.828415	7.369549
5.779417	333.134242	7.374554
5.470350	330.521685	7.379558
5.587758	320.151776	7.384563
5.522822	335.107195	7.389568
5.146068	327.323036	7.394573
5.797206	331.426206	7.399578
5.519516	342.330420	7.404582
5.576754	350.534473	7.409587
5.946252	348.885595	7.414592
5.997565	338.946739	7.419597
5.707013	334.224273	7.424602
5.586624	329.611354	7.429606
5.710493	325.387506	7.434611
5.532378	330.388566	7.439616
5.262749	326.884033	7.444621
5.432696	332.270657	7.449626
5.722343	335.639186	7.454630
5.882924	337.689565	7.459635
5.636389	338.129734	7.464640
5.519902	338.995736	7.469645
5.778068	330.555909	7.474650
5.496890	328.938739	7.479654
5.579239	330.412850	7.484659
5.572482	329.705227	7.489664
5.626363	331.126824	7.494669
6.139556	330.676762	7.499674
5.712791	325.646482	7.504678
5.923414	326.379298	7.509683
5.854518	329.759358	7.514688
5.709272	332.439474	7.519693
5.511933	329.183108	7.524698
5.348358	328.885872	7.529702
5.293652	316.739455	7.534707
5.465221	316.953177	7.539712
5.139799	326.912540	7.544717
5.878740	345.444335	7.549722
5.825659	339.046097	7.554726
6.007300	327.900567	7.559731
5.391579	329.284052	7.564736
5.621479	325.527741	7.569741
5.364047	319.268893	7.574746
5.619524	340.201274	7.579750
5.940131	334.140318	7.584755
5.453031	332.590010	7.589760
5.510310	322.928639	7.594765
5.842718	327.546497	7.599770
5.693145	322.169345	7.604774
5.987040	326.255371	7.609779
5.668466	328.943491	7.614784
5.649756	338.858270	7.619789
6.091153	324.100481	7.624794
5.673855	328.202327	7.629798
5.695011	324.801214	7.634803
5.852839	322.289967	7.639808
5.908298	332.980957	7.644813
5.924239	333.582735	7.649818
5.527551	329.458917	7.654822
5.787390	330.740881	7.659827
5.271412	333.814070	7.664832
5.483266	331.227973	7.669837
6.246540	337.733917	7.674842
5.874107	332.660374	7.679846
5.558650	328.258158	7.684851
5.757727	335.373954	7.689856
5.785543	320.794455	7.694861
5.595178	308.090208	7.699866
5.503573	314.466657	7.704870
5.736470	315.857217	7.709875
5.632841	318.002513	7.714880
5.462444	317.636739	7.719885
5.480359	311.720994	7.724890
5.085908	335.260208	7.729894
5.414276	328.888003	7.734899
5.759810	323.319871	7.739904
5.558898	331.709639	7.744909
5.795199	327.363883	7.749914
5.871857	332.293640	7.754918
5.797153	331.862347	7.759923
5.750094	332.701720	7.764928
5.451028	334.510459	7.769933
5.827701	332.866792	7.774938
5.452572	334.472241	7.779942
5.686530	330.528639	7.784947
5.790156	326.940682	7.789952
5.726322	332.623127	7.794957
5.867391	319.709084	7.799962
5.562719	317.301485	7.804966
5.424423	314.652850	7.809971
5.701043	326.935542	7.814976
5.360239	332.949008	7.819981
5.749355	314.988211	7.824986
5.871177	330.499833	7.829990
6.032172	322.938829	7.834995
5.535423	317.546131	7.840000
4.979687	308.226981	7.845005
5.382301	319.186608	7.850010
5.881517	327.407257	7.855014
5.863509	324.777857	7.860019
5.845721	330.921360	7.865024
5.624413	323.755231	7.870029
5.448444	305.825479	7.875034
5.507193	317.006319	7.880038
5.657899	326.382196	7.885043
5.758501	327.986340	7.890048
5.581834	336.732997	7.895053
5.551462	321.124863	7.900058
5.515592	329.365550	7.905062
5.572082	329.426349	7.910067
5.509272	325.560591	7.915072
5.802500	328.409715	7.920077
6.006831	316.874688	7.925082
5.206093	321.292491	7.930086
5.546372	323.662897	7.935091
5.704233	327.725811	7.940096
5.727219	337.589807	7.945101
5.521075	325.163246	7.950106
5.500167	327.475995	7.955110
5.737713	330.068038	7.960115
5.543840	324.808512	7.965120
5.812793	324.788777	7.970125
5.543693	322.762893	7.975142
5.575059	325.768472	7.980160
5.907140	323.561468	7.985178
5.722436	329.172525	7.990195
5.558982	328.399594	7.995213
5.762964	328.090133	8.000230
5.684304	332.747460	8.005248
5.647782	327.710445	8.010266
5.902683	327.923201	8.015283
5.529752	323.623337	8.020301
5.780352	316.837582	8.025318
5.561736	324.028576	8.030336
5.672492	320.833608	8.035354
5.488690	326.993604	8.040371
5.234233	332.353606	8.045389
5.688474	323.456583	8.050406
5.741133	332.170535	8.055424
6.020485	327.078028	8.060442
5.735511	331.284665	8.065459
5.364438	326.687881	8.070477
5.392536	318.920656	8.075494
5.922131	328.993004	8.080512
5.711957	328.060099	8.085530
5.840713	325.408252	8.090547
5.747652	330.657922	8.095565
5.735818	327.747113	8.100582
5.314560	333.552784	8.105600
5.309895	327.415806	8.110618
5.694373	337.305637	8.115635
5.457487	336.799744	8.120653
5.628112	327.555579	8.125670
5.645861	344.331294	8.130688
5.556502	338.759734	8.135706
5.995966	352.153229	8.140723
5.937252	353.888495	8.145741
6.105285	339.141304	8.150758
5.710945	339.193228	8.155776
5.362762	331.557163	8.160794
5.609023	337.296772	8.165811
5.667062	359.399244	8.170829
5.913257	352.235486	8.175846
5.891422	357.786482	8.180864
5.990535	358.430572	8.185882
6.259088	359.976037	8.190899
5.993075	362.803873	8.195917
6.237763	348.183587	8.200934
5.851042	342.399562	8.205952
5.577499	334.215417	8.210970
5.858773	334.039081	8.215987
5.439118	342.410032	8.221005
5.921285	342.839855	8.226022
5.995024	353.630097	8.231040
5.481606	359.977116	8.236058
5.975102	350.357639	8.241075
5.783233	361.965526	8.246093
6.384302	353.036160	8.251110
6.046239	351.870715	8.256128
6.205779	357.743747	8.261146
5.927238	339.894674	8.266163
5.796174	332.682370	8.271181
5.909989	332.131341	8.276198
6.178817	335.264043	8.281216
6.153423	336.391394	8.286234
5.916982	333.925786	8.291251
6.017295	330.675642	8.296269
6.042322	327.979987	8.301286
5.832828	330.388787	8.306304
5.715703	334.831209	8.311322
5.959857	333.032347	8.316339
5.914557	334.011328	8.321357
6.029172	344.681597	8.326374
6.076202	354.611355	8.331392
5.859737	351.729246	8.336410
5.838637	347.046411	8.341427
5.943698	350.753693	8.346445
5.960481	357.494662	8.351462
5.852190	346.621427	8.356480
6.225076	350.848712	8.361498
6.239801	347.173257	8.366515
5.767252	357.474231	8.371533
6.196989	353.778338	8.376550
6.231604	352.422331	8.381568
6.008089	358.298203	8.386586
6.404186	358.842407	8.391603
6.143910	365.582337	8.396621
6.053269	341.632565	8.401638
5.875724	345.106152	8.406656
6.046278	344.123434	8.411674
5.978960	354.304512	8.416691
5.810622	358.385704	8.421709
6.259553	360.966534	8.426726
6.180061	357.457216	8.431744
6.023247	354.515330	8.436762
6.297495	355.570784	8.441779
5.737989	364.550468	8.446797
5.907747	352.766139	8.451814
6.005759	362.025280	8.456832
6.056918	368.398003	8.461850
6.297541	354.213823	8.466867
6.053998	358.899984	8.471885
6.250173	360.955308	8.476902
6.354237	357.897068	8.481920
5.862222	362.038123	8.486938
6.261845	353.821739	8.491955
5.815715	358.081875	8.496973
5.950991	361.623517	8.501990
5.929944	356.407369	8.507008
6.033008	363.469404	8.512026
6.293836	352.683854	8.517043
5.864601	356.919270	8.522061
5.923498	353.158045	8.527078
6.497350	363.617976	8.532096
6.270320	365.196423	8.537114
6.143152	356.815918	8.542131
6.089477	368.560074	8.547149
6.527162	367.990175	8.552166
6.360080	359.300320	8.557184
5.862426	360.614805	8.562202
6.352811	367.903699	8.567219
6.132570	363.169819	8.572237
6.541132	371.055247	8.577255
6.368121	359.904917	8.582272
6.319581	359.028891	8.587290
6.241394	355.046026	8.592307
6.119514	355.535185	8.597325
5.685278	367.209211	8.602343
6.584362	380.054666	8.607360
6.296555	383.513870	8.612378
6.292408	385.316379	8.617395
6.199111	382.276240	8.622413
6.570498	379.245800	8.627431
6.341188	383.459561	8.632448
6.112119	387.193628	8.637466
6.472008	379.377874	8.642483
6.476068	382.715900	8.647501
6.504879	383.137419	8.652519
6.162723	392.720715	8.657536
6.509465	391.325576	8.662554
6.699039	380.724663	8.667571
6.266200	374.215700	8.672589
6.408865	377.724639	8.677607
6.333221	378.272869	8.682624
6.151146	382.687547	8.687642
6.471807	377.676952	8.692659
6.662358	378.373075	8.697677
6.304621	375.096414	8.702695
6.296242	377.240389	8.707712
6.104420	379.138387	8.712730
6.485393	376.380994	8.717747
6.326796	382.133163	8.722765
6.358697	372.528741	8.727783
6.332402	376.527865	8.732800
6.456675	384.766814	8.737818
6.685312	382.803115	8.742835
7.044546	385.060260	8.747853
6.927291	384.633565	8.752871
6.543542	370.764323	8.757888
6.429918	365.426894	8.762906
6.392996	363.753838	8.767923
6.308922	362.356353	8.772941
6.320663	357.169812	8.777959
6.742951	369.016578	8.782976
6.267606	366.528205	8.787994
6.586685	373.446164	8.793011
6.521070	391.547647	8.798029
6.384444	386.267439	8.803047
6.661950	382.301767	8.808064
6.635349	392.041049	8.813082
6.786647	378.498730	8.818099
6.647157	371.467593	8.823117
6.352738	365.072774	8.828135
6.408355	374.496304	8.833152
6.589605	379.476074	8.838170
6.488154	376.932641	8.843187
6.751476	379.324633	8.848205
6.730982	384.114921	8.853223
6.837326	377.566186	8.858240
6.452123	366.177506	8.863258
6.132374	365.138589	8.868275
6.738773	376.540151	8.873293
6.637368	377.322753	8.878311
6.884434	381.882044	8.883328
6.503774	393.036532	8.888346
6.772117	379.617992	8.893363
6.362174	384.374246	8.898381
6.409199	383.413915	8.903399
6.785111	383.516318	8.908416
6.541739	384.011772	8.913434
6.832042	377.106209	8.918451
6.537255	389.610561	8.923469
6.768078	392.465182	8.928487
6.939308	382.652879	8.933504
6.995515	385.768203	8.938522
6.756588	374.381988	8.943539
6.492517	370.759403	8.948557
6.378329	378.088785	8.953575
6.751300	369.538890	8.958592
6.848446	378.179670	8.963610
6.895167	374.836881	8.968627
6.933871	383.467829	8.973645
6.827767	385.314613	8.978663
6.642163	375.841879	8.983680
6.885329	383.286029	8.988698
6.890796	372.271997	8.993715
6.765772	357.463127	8.998733
6.448711	368.358403	9.003751
7.063967	371.875807	9.008768
6.541742	373.392923	9.013786
6.842231	383.299013	9.018803
6.976890	386.578838	9.023821
6.521864	386.403538	9.028839
7.023002	388.644901	9.033856
6.958998	389.207097	9.038874
6.809730	369.463416	9.043891
7.123502	367.549576	9.048909
6.618780	370.815345	9.053927
6.751592	359.197702	9.058944
6.683838	366.403091	9.063962
7.138803	374.230806	9.068979
6.602862	365.566820	9.073997
6.459679	378.315788	9.079015
6.919607	388.610445	9.084032
6.831752	393.919281	9.089050
7.154345	387.399987	9.094067
7.004811	392.762604	9.099085
6.980118	389.923211	9.104103
7.309151	386.552243	9.109120
6.652796	379.800382	9.114138
6.543421	370.236892	9.119155
6.982876	384.722263	9.124173
6.845248	390.635263	9.129191
7.192326	394.125002	9.134208
6.797851	401.920890	9.139226
7.222202	390.197877	9.144243
6.953653	381.425983	9.149261
6.858598	376.773589	9.154279
6.981616	373.204337	9.159296
7.006801	381.947837	9.164314
7.054124	377.828666	9.169331
6.765443	385.172597	9.174349
6.528044	382.271654	9.179367
6.975588	383.782941	9.184384
6.918430	391.166562	9.189402
6.754465	397.610657	9.194419
6.769297	386.670894	9.199437
6.525181	398.485744	9.204455
7.036361	392.183225	9.209472
6.647742	390.192560	9.214490
6.718626	391.734092	9.219507
6.814039	391.659273	9.224525
7.067946	401.556847	9.229543
7.188829	413.371679	9.234560
7.231290	411.922933	9.239578
6.820973	406.527549	9.244595
7.147448	407.628521	9.249613
7.119443	411.627919	9.254631
7.319465	403.641395	9.259648
7.120575	398.301453	9.264666
6.915022	388.124955	9.269683
6.883758	402.487980	9.274701
7.011139	407.289962	9.279719
7.078754	406.607277	9.284736
7.417217	414.506794	9.289754
7.244717	412.589768	9.294771
7.242470	409.737410	9.299789
6.981877	420.100089	9.304807
7.195310	412.430193	9.309824
7.382357	412.442087	9.314842
7.551088	402.500781	9.319859
7.046070	390.969801	9.324877
6.933280	393.792720	9.329895
7.232447	407.198634	9.334912
7.087801	411.973547	9.339930
7.104255	415.312805	9.344947
7.382075	412.218036	9.349965
7.227211	413.709515	9.354983
7.632955	403.942734	9.360000
7.346469	404.971893	9.365018
7.059295	396.051421	9.370035
7.182012	387.313275	9.375053
6.723500	389.622006	9.380071
7.043917	398.565687	9.385088
7.491398	403.412499	9.390106
7.360404	415.503222	9.395123
7.472507	414.318173	9.400141
7.186562	411.273312	9.405159
7.490614	409.780682	9.410176
7.323318	404.508399	9.415194
7.142212	411.469537	9.420211
7.212063	406.744125	9.425229
7.193608	408.312190	9.430247
7.456950	406.819587	9.435264
7.181189	405.631815	9.440282
7.270977	404.841541	9.445299
7.416523	410.281291	9.450317
7.102828	411.235795	9.455335
7.215032	405.146863	9.460352
7.189320	407.337720	9.465370
7.189511	413.712083	9.470387
7.609245	408.875393	9.475405
7.172724	409.085355	9.480423
7.289580	403.093523	9.485440
7.347212	411.267125	9.490458
7.446119	403.564574	9.495475
7.469609	408.644650	9.500493
7.439782	422.272203	9.505511
7.169632	410.717266	9.510528
7.738738	408.025246	9.515546
7.396715	413.705003	9.520563
7.450639	405.785404	9.525581
7.190277	407.564694	9.530599
7.318712	402.350504	9.535616
7.424789	411.081423	9.540634
7.306583	406.571473	9.545651
7.421529	406.111780	9.550669
7.364700	407.707910	9.555687
7.555717	406.406439	9.560704
7.432880	401.969791	9.565722
7.280678	411.599258	9.570739
7.106870	408.237152	9.575757
7.287638	419.099127	9.580775
7.710482	423.214516	9.585792
7.802853	425.162939	9.590810
7.575576	434.071997	9.595827
7.760918	433.434093	9.600845
7.638947	433.247960	9.605863
7.884761	426.210458	9.610880
7.766917	419.267445	9.615898
7.644658	416.238122	9.620915
7.476621	411.805353	9.625933
7.700277	414.036277	9.630951
7.353619	414.882310	9.635968
7.258794	406.351586	9.640986
7.425208	411.513546	9.646003
7.950221	420.504275	9.651021
7.627621	419.178635	9.656039
8.008129	411.375434	9.661056
7.532688	403.301583	9.666074
7.143949	405.394335	9.671091
7.826950	413.615730	9.676109
7.560555	423.398675	9.681127
7.748901	423.593395	9.686144
8.177726	419.594688	9.691162
7.729273	418.875593	9.696179
7.499643	411.760650	9.701197
7.642469	407.042809	9.706215
7.249001	406.412979	9.711232
7.601909	417.049346	9.716250
7.814776	424.618146	9.721267
7.799415	422.989062	9.726285
7.769289	431.444567	9.731303
7.772254	432.056294	9.736320
8.001201	424.775278	9.741338
7.594395	418.763992	9.746355
7.935146	421.020864	9.751373
7.748335	432.552274	9.756391
7.640374	426.144180	9.761408
8.145692	427.084771	9.766426
7.806407	417.670654	9.771443
7.829650	411.706018	9.776461
7.384932	418.051828	9.781479
7.429760	419.562707	9.786496
7.810641	419.560201	9.791514
7.473439	422.863010	9.796531
7.930373	427.184520	9.801549
7.645280	433.761090	9.806567
7.712826	434.713039	9.811584
7.988355	432.783057	9.816602
7.636791	428.694423	9.821619
8.068180	428.756633	9.826637
7.767854	427.547439	9.831655
8.147963	432.294301	9.836672
8.002585	424.642397	9.841690
8.042926	434.273455	9.846707
7.992911	436.774197	9.851725
8.008165	438.668360	9.856743
7.659120	432.105306	9.861760
8.085734	431.672822	9.866778
7.753129	434.116582	9.871795
8.100053	430.439878	9.876813
7.764530	424.613142	9.881831
7.955725	433.854657	9.886848
8.065082	423.417680	9.891866
7.561478	426.579148	9.896883
7.492542	430.165222	9.901901
7.568991	441.093943	9.906919
7.809965	432.195359	9.911936
7.768996	433.700664	9.916954
8.253977	452.022581	9.921971
7.925507	446.835337	9.926989
8.107041	441.205789	9.932007
7.997576	434.813705	9.937024
7.975201	432.895393	9.942042
8.180652	445.893071	9.947059
7.986824	442.180643	9.952077
8.197535	439.102629	9.957095
8.073244	440.352677	9.962112
7.986513	436.147073	9.967130
8.170907	449.160654	9.972147
7.993761	437.941495	9.977165
8.039298	442.096699	9.982183
7.956151	450.598336	9.987200
8.053648	446.783747	9.992218
7.900789	453.024171	9.997235
8.194392	447.430818	10.002253
8.312386	452.628731	10.007271
8.100633	445.444722	10.012288
8.664502	448.531507	10.017306
8.143774	441.916288	10.022323
7.977528	434.542170	10.027341
8.407717	440.638166	10.032359
7.823417	447.053054	10.037376
8.206578	442.064266	10.042394
7.847093	450.823512	10.047411
7.982717	454.526057	10.052429
8.087014	447.371731	10.057447
7.998400	457.616141	10.062464
8.289085	451.234329	10.067482
8.245151	459.950760	10.072499
8.275987	454.827486	10.077517
8.323660	454.495025	10.082535
8.432070	455.140826	10.087552
8.383264	448.171275	10.092570
8.271017	456.746870	10.097587
8.335583	451.050328	10.102605
8.464330	450.130916	10.107623
8.307182	455.759813	10.112640
8.757664	449.053335	10.117658
8.461949	454.647004	10.122675
8.154366	455.127211	10.127693
8.677680	452.773658	10.132711
7.998972	446.053652	10.137728
8.357908	445.922026	10.142746
8.324039	454.810448	10.147763
8.593387	453.705051	10.152781
8.409121	448.176634	10.157799
8.146463	456.469549	10.162816
8.292644	447.178637	10.167834
7.964635	447.908165	10.172851
7.889118	447.774756	10.177869
8.136879	447.313317	10.182887
7.935349	451.099912	10.187904
8.460311	458.484441	10.192922
8.137083	458.414846	10.197939
8.343385	455.820330	10.202957
8.330670	454.241322	10.207975
7.972462	461.302634	10.212992
8.508317	466.776301	10.218010
8.841019	481.717009	10.223027
8.525858	467.433089	10.228045
8.766580	472.078593	10.233063
8.531590	463.071071	10.238080
8.509511	441.540343	10.243098
8.207086	448.160640	10.248115
8.293985	461.482885	10.253133
8.629924	461.184434	10.258151
8.248739	476.160550	10.263168
8.808793	474.908909	10.268186
8.807197	474.599897	10.273203
8.430217	472.831461	10.278221
8.900475	475.083955	10.283239
8.485346	460.711468	10.288256
8.404227	463.873433	10.293274
8.476930	471.823820	10.298291
8.417033	472.076125	10.303309
8.881691	469.501340	10.308327
8.708498	476.874662	10.313344
8.886496	474.259305	10.318362
8.588311	465.772837	10.323379
8.296489	460.160182	10.328397
8.833058	464.207382	10.333415
8.806006	470.147372	10.338432
8.886647	453.245759	10.343450
8.665760	455.567991	10.348467
8.660878	449.648744	10.353485
8.768416	446.482655	10.358503
8.544705	452.958162	10.363520
8.464289	454.071998	10.368538
8.926113	464.432673	10.373555
8.418634	464.653683	10.378573
8.773575	462.253764	10.383591
8.530463	470.133407	10.388608
8.927097	477.522146	10.393626
8.798173	480.770448	10.398643
8.794630	478.798709	10.403661
9.090344	472.618068	10.408679
8.604435	469.661133	10.413696
8.408091	467.561630	10.418714
8.540044	480.315168	10.423731
8.640180	484.259919	10.428749
9.007669	474.076198	10.433767
8.446578	479.158953	10.438784
8.824062	473.558844	10.443802
8.871444	483.640090	10.448819
8.883877	486.901097	10.453837
8.865465	474.278179	10.458855
8.824239	473.946937	10.463872
8.904832	480.220447	10.468890
9.252617	479.740278	10.473907
9.016421	478.915553	10.478925
8.987641	481.258368	10.483943
8.672242	486.040952	10.488960
8.754306	480.613063	10.493978
8.888172	479.071188	10.498995
8.787847	481.324162	10.504013
8.834911	473.020611	10.509031
8.830217	484.037728	10.514048
8.736702	479.082123	10.519066
8.907894	483.239863	10.524083
8.754977	488.527300	10.529101
8.902986	470.239316	10.534119
8.864667	478.197525	10.539136
8.806211	469.156203	10.544154
9.019923	472.045058	10.549171
9.005743	471.902099	10.554189
8.737619	465.692489	10.559207
8.657779	480.400795	10.564224
8.846222	481.898787	10.569242
9.230685	490.766273	10.574259
9.120976	496.400419	10.579277
9.297311	487.066924	10.584295
9.189252	488.759396	10.589312
8.868300	473.876798	10.594330
9.322925	481.751947	10.599347
8.998391	477.024807	10.604365
8.976203	474.730939	10.609383
9.083018	487.116029	10.614400
9.063761	483.448992	10.619418
9.122122	483.966894	10.624435
9.127613	490.854831	10.629453
9.052772	493.854885	10.634471
9.470844	494.487187	10.639488
9.390671	481.438399	10.644506
9.360448	480.041987	10.649523
8.869955	485.397761	10.654541
9.208123	473.804871	10.659559
9.016670	474.958087	10.664576
9.020224	485.292299	10.669594
9.118288	481.840515	10.674611
9.221792	492.086589	10.679629
9.334776	488.925956	10.684647
9.591841	495.080482	10.689664
9.460156	484.188716	10.694682
9.065945	472.214418	10.699699
9.217846	474.137800	10.704717
9.347611	480.157513	10.709735
9.340654	474.970693	10.714752
9.242819	469.037511	10.719770
9.621751	467.810915	10.724787
9.118052	475.213605	10.729805
9.056026	480.792987	10.734823
9.235974	480.903813	10.739840
9.468990	482.369619	10.744858
9.430170	477.011042	10.749875
9.255539	482.772051	10.754893
9.189027	481.722100	10.759911
9.104238	486.241572	10.764928
9.499643	492.885774	10.769946
9.441202	495.567709	10.774963
9.549995	501.432912	10.779981
9.219511	507.322332	10.784999
9.341045	506.296747	10.790016
9.274035	501.327543	10.795034
9.717787	495.691864	10.800051
9.528396	508.318738	10.805069
9.871852	501.540545	10.810087
9.381480	485.709216	10.815104
9.060741	479.586684	10.820122
9.470623	499.163671	10.825139
9.350438	496.686251	10.830157
9.373982	502.299652	10.835175
9.147486	498.529185	10.840192
9.173044	499.901067	10.845210
9.457345	499.238287	10.850227
9.249924	506.254050	10.855245
9.759918	497.209411	10.860263
9.370784	501.151452	10.865280
9.069895	497.645021	10.870298
9.746612	496.435172	10.875315
9.179926	503.727766	10.880333
9.246594	498.318046	10.885351
9.288294	511.644211	10.890368
9.420061	518.146441	10.895386
9.550003	519.965955	10.900403
9.641985	531.671762	10.905421
9.684885	523.791695	10.910439
9.852072	520.575283	10.915456
9.508384	529.789678	10.920474
10.060655	521.461092	10.925491
9.847817	524.350099	10.930509
9.809019	510.613224	10.935527
9.838137	508.926717	10.940544
9.555123	502.791993	10.945562
9.511324	495.209446	10.950579
9.273487	502.794806	10.955597
9.514705	517.989618	10.960615
9.699603	515.038681	10.965632
9.754557	528.567912	10.970650
10.124323	519.175883	10.975667
10.074936	518.924801	10.980685
9.960984	518.939381	10.985703
9.622843	506.375688	10.990720
9.754127	505.083510	10.995738
9.883188	502.254872	11.000755
9.970559	499.461127	11.005773
9.572922	501.176597	11.010791
9.973992	504.399187	11.015808
10.033213	511.960389	11.020826
9.924266	491.493961	11.025843
9.778668	505.221649	11.030861
9.587136	497.554811	11.035879
9.782698	503.195076	11.040896
9.542245	519.001345	11.045914
9.911220	516.962135	11.050931
9.968683	524.832871	11.055949
10.327092	531.959354	11.060967
10.042531	515.026184	11.065984
9.532510	508.999382	11.071002
9.900397	506.998210	11.076019
9.790736	513.175127	11.081037
9.677009	515.733135	11.086055
9.815615	526.295641	11.091072
9.312630	529.920914	11.096090
10.069748	520.922990	11.101107
9.546978	530.351453	11.106125
9.876923	523.881455	11.111143
9.860840	532.243307	11.116160
9.505381	525.466631	11.121178
10.085656	532.293494	11.126195
10.190319	545.777131	11.131213
9.996026	531.023081	11.136231
9.730996	529.095204	11.141248
9.937244	550.761446	11.146266
10.464114	552.632766	11.151283
10.369287	546.238363	11.156301
10.407032	540.975139	11.161319
10.378776	528.593546	11.166336
10.114004	535.122810	11.171354
10.365909	524.458461	11.176371
10.005354	525.521249	11.181389
10.148205	522.466408	11.186407
10.072574	529.609977	11.191424
9.904185	531.860932	11.196442
10.246957	526.452395	11.201459
10.094311	529.912673	11.206477
10.156982	527.154326	11.211495
9.981105	524.079685	11.216512
10.401797	527.595857	11.221530
10.063172	530.103680	11.226547
10.227836	523.384873	11.231565
10.262571	529.911683	11.236583
10.107866	525.309560	11.241600
9.813683	528.476308	11.246618
10.574852	537.237832	11.251635
10.142188	540.618639	11.256653
10.306701	538.904737	11.261671
10.319987	533.194063	11.266688
10.094873	535.845153	11.271706
10.668074	535.878972	11.276723
10.549711	536.380211	11.281741
10.266131	532.015893	11.286759
10.425141	526.989402	11.291776
10.216895	525.396651	11.296794
10.379164	524.749715	11.301811
10.267702	522.349825	11.306829
10.082722	531.709917	11.311847
10.551996	537.222374	11.316864
10.425943	540.495485	11.321882
10.448588	534.016527	11.326899
10.389033	542.773299	11.331917
10.580459	544.718935	11.336935
10.284364	528.841541	11.341952
10.320295	544.516443	11.346970
10.453804	538.133826	11.351987
10.738872	537.436213	11.357005
10.316233	545.129256	11.362023
10.556222	538.849975	11.367040
10.274609	548.714250	11.372058
10.750153	539.122712	11.377075
10.524772	542.307152	11.382093
10.327968	538.131284	11.387111
10.738372	535.940461	11.392128
10.419807	546.836079	11.397146
11.002116	534.640274	11.402163
10.470983	531.510496	11.407181
10.101911	530.375111	11.412199
10.335478	522.405401	11.417216
10.498251	539.559489	11.422234
10.529927	536.815433	11.427251
10.574509	548.866288	11.432269
10.392824	547.575500	11.437287
10.417909	545.406800	11.442304
10.364332	548.192123	11.447322
10.511612	537.133819	11.452339
10.690572	551.618862	11.457357
10.299937	550.650928	11.462375
10.609521	545.370623	11.467392
10.396515	549.878518	11.472410
10.382568	549.694498	11.477427
10.511474	559.144584	11.482445
10.630589	573.856703	11.487463
11.113077	577.091876	11.492480
10.868154	574.267808	11.497498
11.045076	572.526725	11.502515
10.779269	562.533070	11.507533
10.684647	563.207331	11.512551
10.685988	550.186825	11.517568
10.378738	559.610149	11.522586
10.688598	566.173027	11.527603
10.962749	578.547906	11.532621
10.801005	572.422676	11.537639
11.124885	578.942353	11.542656
11.296393	577.770134	11.547674
10.824156	568.401883	11.552691
10.707835	558.621631	11.557709
10.937959	556.900668	11.562727
10.893128	552.022666	11.567744
10.718615	554.552276	11.572762
11.133116	561.051526	11.577779
10.874866	565.863101	11.582797
10.955715	568.848394	11.587815
10.965747	555.327936	11.592832
10.874670	586.523301	11.597850
11.111531	567.268369	11.602867
11.070955	558.369379	11.607885
10.791452	557.175868	11.612903
10.750002	566.052904	11.617920
10.826636	568.278336	11.622938
10.879289	571.665635	11.627955
10.593633	577.008477	11.632973
10.527689	583.371109	11.637991
10.867021	571.165774	11.643008
11.165769	578.370988	11.648026
10.949202	569.909631	11.653043
11.213725	567.776229	11.658061
11.085578	572.245672	11.663079
11.325029	571.103899	11.668096
11.082824	577.162625	11.673114
10.952656	567.722181	11.678131
11.198166	562.795816	11.683149
10.789417	567.069115	11.688167
11.000779	559.276407	11.693184
11.039965	570.577067	11.698202
11.085205	569.131031	11.703219
11.336174	569.316003	11.708237
11.171140	575.539431	11.713255
11.161018	564.287876	11.718272
10.997113	580.647147	11.723290
11.276356	585.618029	11.728307
11.382001	580.044433	11.733325
11.139792	579.271129	11.738343
11.139653	569.636877	11.743360
11.216516	581.234622	11.748378
11.938137	590.033886	11.753395
11.966529	571.635039	11.758413
11.416980	573.490927	11.763431
11.535737	565.627432	11.768448
11.248366	567.559259	11.773466
11.179213	566.875772	11.778483
11.225033	562.772571	11.783501
11.073146	576.255152	11.788519
11.218301	568.166648	11.793536
11.386596	575.559423	11.798554
11.346766	576.493386	11.803571
11.381473	569.826352	11.808589
11.019112	570.649592	11.813607
11.374788	564.226064	11.818624
11.408146	574.789208	11.823642
11.510233	572.056273	11.828659
11.432459	570.878688	11.833677
11.293623	571.506186	11.838695
11.584843	579.451001	11.843712
11.502245	580.653543	11.848730
11.606230	582.887342	11.853747
11.191628	572.790621	11.858765
11.590341	593.985156	11.863783
11.767768	589.312371	11.868800
11.408130	585.329095	11.873818
11.320376	569.917823	11.878835
11.709315	579.245385	11.883853
11.649215	599.990676	11.888871
11.493377	599.147122	11.893888
11.612769	597.708473	11.898906
11.536818	598.010614	11.903923
11.952503	585.263228	11.908941
11.603793	588.700397	11.913959
11.532148	576.331838	11.918976
11.521578	580.934448	11.923994
11.668525	591.274797	11.929011
11.509437	587.743115	11.934029
11.472524	596.307047	11.939047
11.650948	584.082577	11.944064
11.777141	584.854997	11.949082
11.669818	588.065243	11.954099
11.908533	588.397283	11.959117
12.042161	598.449388	11.964135
12.031580	586.617246	11.969152
11.976383	589.863556	11.974170
11.197141	567.920409	11.979187
11.519893	572.423785	11.984205
11.696004	585.126344	11.989223
12.055232	592.972217	11.994240
11.844966	589.218138	11.999258
11.639144	590.894284	12.004275
11.781400	587.107409	12.009293
11.608606	600.302940	12.014311
11.630557	585.382638	12.019328
11.965220	582.092804	12.024346
11.850908	588.380920	12.029363
11.930583	585.809257	12.034381
11.573219	597.152741	12.039399
11.829155	585.695654	12.044416
12.038072	588.992356	12.049434
11.893710	584.644217	12.054451
12.062884	590.708323	12.059469
11.748078	588.311683	12.064487
11.536033	590.679891	12.069504
11.557651	593.308352	12.074522
11.099297	598.485593	12.079539
11.983172	607.180711	12.084557
11.923172	611.270339	12.089575
12.007083	615.826691	12.094592
12.082053	617.749444	12.099610
12.012767	626.305809	12.104627
11.982976	614.855321	12.109645
11.846974	629.477824	12.114663
12.060929	616.499903	12.119680
12.323706	621.710035	12.124698
12.144993	622.593043	12.129715
12.251126	619.676442	12.134733
11.750422	614.449695	12.139751
12.042178	621.965273	12.144768
12.213676	622.310935	12.149786
12.066654	625.420075	12.154803
12.461966	616.450035	12.159821
12.174149	621.193648	12.164839
12.547643	619.529249	12.169856
12.359647	613.332356	12.174874
11.973762	614.613679	12.179891
12.307808	609.566223	12.184909
12.192620	619.316266	12.189927
12.249510	621.282858	12.194944
12.348478	614.318635	12.199962
12.281427	616.695828	12.204979
12.750234	609.901234	12.209997
12.692247	617.872035	12.215015
12.517359	615.592456	12.220032
12.619655	612.442933	12.225050
12.218427	603.805191	12.230067
12.780572	595.191023	12.235085
12.112925	593.246933	12.240103
12.033598	601.798537	12.245120
12.440663	594.751640	12.250138
11.914735	611.123125	12.255155
12.099032	615.575489	12.260173
12.042698	609.127734	12.265191
12.236119	612.430010	12.270208
12.663942	608.106383	12.275226
12.441287	617.374560	12.280243
12.441838	615.761915	12.285261
12.392571	613.772034	12.290279
12.106201	610.708271	12.295296
12.403469	599.721247	12.300314
12.380840	620.533308	12.305331
12.501047	616.611010	12.310349
12.223113	621.248947	12.315367
12.655714	631.090426	12.320384
13.044271	629.007130	12.325402
12.834372	617.890784	12.330419
12.483738	607.862975	12.335437
12.633860	611.427602	12.340455
12.288475	616.120219	12.345472
12.454680	614.658501	12.350490
12.648677	633.906346	12.355507
13.026533	622.023169	12.360525
12.590483	626.180817	12.365543
12.847209	610.794767	12.370560
12.621733	615.446625	12.375578
12.255720	618.441543	12.380595
12.768482	622.041225	12.385613
12.702278	636.829585	12.390631
12.766868	642.843723	12.395648
12.957772	645.411122	12.400666
12.703397	641.184235	12.405683
13.058387	627.805665	12.410701
12.814668	616.798722	12.415719
12.316210	617.977656	12.420736
12.911527	619.525915	12.425754
12.890268	641.445431	12.430771
12.926184	635.567105	12.435789
12.952709	636.503363	12.440807
12.958808	630.206820	12.445824
12.791513	620.434470	12.450842
12.460721	621.158127	12.455859
12.558287	639.221833	12.460877
12.896370	645.764568	12.465895
12.798312	646.470924	12.470912
13.056902	637.831417	12.475930
12.455409	635.646657	12.480947
12.999545	631.850848	12.485965
12.898533	635.258928	12.490983
13.001233	640.490833	12.496000
13.112701	631.179985	12.501018
12.734991	640.043142	12.506035
13.212311	635.459347	12.511053
13.252586	638.813873	12.516071
12.880123	632.693030	12.521088
12.900777	638.745564	12.526106
12.987268	641.562740	12.531123
12.635470	646.470950	12.536141
12.847460	637.639890	12.541159
12.985838	639.688467	12.546176
12.970456	641.947169	12.551194
13.073798	640.340609	12.556211
13.144949	637.079170	12.561229
13.052357	647.583074	12.566247
13.356613	663.225770	12.571264
13.464879	644.075981	12.576282
12.863637	645.662225	12.581299
13.120733	644.710197	12.586317
13.438350	653.080108	12.591335
13.241375	645.606549	12.596352
13.170024	639.700744	12.601370
13.118004	659.457117	12.606387
13.463933	657.150090	12.611405
13.351817	665.028358	12.616423
13.265085	652.699962	12.621440
13.788613	658.494333	12.626458
13.435652	646.920578	12.631475
13.291867	634.578989	12.636493
13.523174	634.984764	12.641511
13.216595	639.210616	12.646528
13.374036	634.121225	12.651546
13.159694	640.652143	12.656563
12.984558	642.074217	12.661581
13.702468	645.272748	12.666599
13.189176	653.888788	12.671616
13.798489	660.790072	12.676634
13.458776	660.331736	12.681651
13.344167	644.561677	12.686669
13.425404	650.405974	12.691687
13.405302	665.950856	12.696704
13.770526	662.880304	12.701722
13.342920	664.250173	12.706739
13.646349	659.324231	12.711757
13.391155	661.648675	12.716775
13.227426	657.565455	12.721792
13.506774	652.715845	12.726810
13.561064	668.217590	12.731827
13.454471	656.501332	12.736845
13.832238	662.965315	12.741863
13.631132	659.052011	12.746880
13.855146	659.297982	12.751898
13.855045	668.181254	12.756915
13.888704	666.175300	12.761933
13.645296	667.579604	12.766951
13.600526	659.160882	12.771968
13.584091	653.694629	12.776986
13.275591	668.814219	12.782003
13.571219	660.042707	12.787021
13.804625	657.961474	12.792039
13.476030	663.689711	12.797056
13.803757	656.326951	12.802074
13.376948	661.660239	12.807091
14.104975	659.587200	12.812109
14.345601	658.669292	12.817127
13.952528	664.271873	12.822144
14.088348	656.907435	12.827162
14.062303	656.984065	12.832179
13.498109	665.892048	12.837197
13.915469	648.306687	12.842215
13.238251	662.290830	12.847232
13.586658	664.429782	12.852250
13.534025	656.561374	12.857267
13.610832	655.025212	12.862285
13.982592	654.055331	12.867303
13.700294	660.366472	12.872320
13.683141	647.575983	12.877338
14.000854	654.898192	12.882355
13.520088	663.001108	12.887373
13.870210	678.807083	12.892391
13.819587	690.427905	12.897408
13.874572	683.170713	12.902426
13.769829	687.201054	12.907443
14.209474	691.509543	12.912461
14.295320	682.581340	12.917479
14.342324	686.796331	12.922496
14.415797	675.045714	12.927514
14.009894	674.679731	12.932531
14.388240	686.612444	12.937549
14.221341	676.899960	12.942567
14.432085	688.943973	12.947584
14.116513	669.692894	12.952602
13.843559	672.701734	12.957619
14.135841	672.545771	12.962637
14.153213	673.196288	12.967655
14.088547	682.342074	12.972672
14.399763	668.468534	12.977690
14.589837	672.699114	12.982707
14.285537	687.108036	12.987725
14.235752	683.376286	12.992743
14.301782	681.595656	12.997760
14.544499	679.273139	13.002778
14.512793	679.988100	13.007795
14.207905	669.927888	13.012813
14.260484	657.864966	13.017831
14.207204	669.028613	13.022848
14.556685	674.152680	13.027866
14.561501	678.970663	13.032883
14.026345	667.627226	13.037901
14.306421	667.520499	13.042919
14.213230	680.290300	13.047936
14.234243	679.854693	13.052954
14.155805	679.788007	13.057971
14.260443	679.863224	13.062989
14.571639	674.790906	13.068007
14.203469	677.817727	13.073024
14.268086	679.290834	13.078042
14.519264	677.143719	13.083059
14.344021	685.827058	13.088077
14.217413	678.878998	13.093095
14.220623	684.773323	13.098112
14.221748	689.279470	13.103130
14.608791	700.488184	13.108147
15.180137	707.464823	13.113165
14.842888	687.541782	13.118183
14.554496	682.531259	13.123200
14.666740	678.294617	13.128218
14.341008	677.439643	13.133235
14.536633	694.503562	13.138253
14.888346	698.582754	13.143271
14.624493	702.407507	13.148288
14.645045	703.322608	13.153306
14.891173	704.010090	13.158323
14.702416	704.673767	13.163341
14.419583	700.940430	13.168359
14.628014	699.658317	13.173376
14.921391	703.513071	13.178394
14.737213	703.566986	13.183411
14.576992	713.409296	13.188429
15.166000	700.448656	13.193447
14.888584	710.242941	13.198464
14.671046	700.295340	13.203482
14.860080	702.118295	13.208499
14.749703	710.150940	13.213517
14.761025	701.316379	13.218535
14.890292	700.860761	13.223552
14.623783	700.166972	13.228570
15.067944	700.362890	13.233587
15.029712	703.227896	13.238605
15.122718	693.017361	13.243623
15.011727	698.216284	13.248640
14.359434	702.092048	13.253658
14.728943	699.216475	13.258675
14.706777	712.265565	13.263693
14.948309	690.087599	13.268711
15.171841	705.193810	13.273728
15.296513	707.304487	13.278746
15.176264	703.877184	13.283763
14.908781	696.796421	13.288781
15.204035	701.171572	13.293799
15.181066	698.944066	13.298816
14.894364	697.603348	13.303834
14.805637	711.915612	13.308851
15.131055	716.869875	13.313869
15.651934	717.287370	13.318887
15.599064	721.647303	13.323904
15.350150	713.544351	13.328922
15.596380	711.464272	13.333939
15.109526	697.541402	13.338957
15.462110	691.762072	13.343975
15.045884	700.710149	13.348992
15.504407	694.838586	13.354010
15.767138	703.567349	13.359027
15.090231	705.802828	13.364045
15.412984	689.800536	13.369063
15.361920	698.669668	13.374080
15.297659	695.037996	13.379098
15.392852	704.389270	13.384115
14.761433	697.074846	13.389133
15.201341	696.586640	13.394151
15.501453	716.250383	13.399168
15.375132	720.053726	13.404186
15.620530	711.302632	13.409203
15.753185	706.636787	13.414221
15.572651	698.759873	13.419239
15.701242	693.245782	13.424256
15.196480	690.133960	13.429274
15.254860	694.037923	13.434291
15.469521	705.516469	13.439309
15.485619	714.056426	13.444327
15.617754	715.130873	13.449344
15.390508	728.445427	13.454362
15.789879	720.345675	13.459379
15.531038	724.829193	13.464397
15.719865	725.358345	13.469415
15.893902	718.284568	13.474432
15.571903	720.644666	13.479450
15.530120	710.950552	13.484467
15.614141	717.640164	13.489485
15.943172	713.874673	13.494503
16.211221	717.739686	13.499520
15.657741	698.582420	13.504538
15.634440	701.505059	13.509555
15.481603	710.468934	13.514573
15.745080	708.304122	13.519591
15.857677	715.330100	13.524608
16.048163	728.355560	13.529626
16.104970	712.325229	13.534643
15.575038	714.458934	13.539661
15.731907	714.150491	13.544679
15.753774	722.907297	13.549696
15.376140	725.837773	13.554714
16.006129	720.037332	13.559731
15.884938	727.683519	13.564749
15.969227	723.580603	13.569767
16.186427	720.365836	13.574784
15.933299	721.329860	13.579802
15.937718	718.394366	13.584819
15.892568	726.546247	13.589837
15.914076	727.473824	13.594855
15.898803	714.127592	13.599872
15.919119	718.078511	13.604890
15.978193	708.412875	13.609907
15.915570	717.318528	13.614925
15.979560	710.858314	13.619943
15.925357	710.617446	13.624960
15.850251	718.202807	13.629978
15.768899	721.610998	13.634995
16.125551	738.043993	13.640013
16.522730	741.598582	13.645031
16.094499	733.734972	13.650048
16.185787	744.910870	13.655066
16.250589	735.758707	13.660083
16.028155	744.361062	13.665101
16.307139	739.606156	13.670119
16.395425	744.392227	13.675136
16.220390	746.246624	13.680154
16.482975	738.174473	13.685171
16.454395	740.968557	13.690189
16.481667	731.222655	13.695207
16.151467	726.474240	13.700224
16.712050	730.625058	13.705242
16.439252	730.749574	13.710259
16.267943	721.946593	13.715277
16.310222	713.173476	13.720295
16.332524	719.778028	13.725312
16.475090	740.170047	13.730330
16.740892	735.707518	13.735347
16.502508	734.750582	13.740365
16.253797	719.613540	13.745383
16.093855	724.835872	13.750400
16.390298	741.795780	13.755418
16.462010	743.826348	13.760435
16.376312	736.266000	13.765453
16.357643	745.098554	13.770471
16.418551	749.715325	13.775488
16.583593	750.374410	13.780506
16.572594	754.125092	13.785523
16.747317	750.165875	13.790541
16.592125	748.665827	13.795559
16.729219	740.464895	13.800576
16.700185	745.663695	13.805594
16.801144	737.285359	13.810611
16.533472	750.666182	13.815629
16.927534	747.206130	13.820647
16.512849	744.518915	13.825664
16.687009	748.098761	13.830682
17.036225	744.999130	13.835699
16.406406	741.954105	13.840717
16.715720	742.789536	13.845735
16.678418	742.725912	13.850752
16.612737	757.107205	13.855770
16.821859	740.557689	13.860787
16.685207	748.992061	13.865805
16.558444	748.333315	13.870823
16.938712	751.303578	13.875840
16.767754	763.596413	13.880858
16.980290	770.351240	13.885875
17.148734	768.908095	13.890893
17.255319	764.451415	13.895911
17.043241	746.784082	13.900928
16.923234	755.695534	13.905946
17.131410	737.833394	13.910963
16.801883	749.046412	13.915981
16.730854	761.942206	13.920999
17.525373	768.388676	13.926016
16.990575	779.390684	13.931034
17.083857	770.552795	13.936051
17.045652	774.859966	13.941069
17.022014	774.396595	13.946087
17.510317	769.025286	13.951104
17.296253	769.008117	13.956122
17.296147	765.290705	13.961139
17.119179	755.623925	13.966157
17.156454	766.902918	13.971175
17.270571	764.265908	13.976192
17.373357	774.032589	13.981210
17.341468	759.937851	13.986227
17.328788	759.785190	13.991245
17.326580	755.784093	13.996263
17.383375	755.592213	14.001280
16.986839	752.081689	14.006298
17.140119	748.908425	14.011315
17.175354	755.507821	14.016333
17.274469	767.487219	14.021351
17.304715	760.341141	14.026368
17.018831	772.531960	14.031386
17.549343	768.227019	14.036403
17.553128	765.275837	14.041421
17.391164	764.067167	14.046439
17.315211	761.806878	14.051456
16.856582	772.847514	14.056474
17.269622	768.617666	14.061491
17.538348	770.705922	14.066509
17.339158	772.141218	14.071527
17.971089	782.986819	14.076544
17.850012	774.160213	14.081562
17.462340	767.025554	14.086579
17.469934	762.227692	14.091597
17.544673	772.951763	14.096615
17.837374	775.386570	14.101632
17.599753	773.542759	14.106650
17.690543	772.039123	14.111667
17.793291	769.274498	14.116685
17.668948	776.170138	14.121703
17.860231	773.287590	14.126720
17.799002	776.200368	14.131738
17.655834	768.387030	14.136755
17.922940	770.081075	14.141773
17.736407	781.678937	14.146791
17.884996	772.715675	14.151808
17.877461	778.513877	14.156826
17.821836	786.888316	14.161843
18.251253	777.903417	14.166861
17.786786	772.620490	14.171879
17.787759	763.326776	14.176896
17.740736	777.575797	14.181914
17.906892	779.427567	14.186931
18.005535	785.086168	14.191949
18.251487	790.409419	14.196967
18.332689	771.964274	14.201984
17.727229	778.963224	14.207002
17.943378	773.792072	14.212019
18.166762	778.090072	14.217037
17.776502	781.256045	14.222055
18.203455	780.192360	14.227072
18.364272	789.517683	14.232090
18.123041	782.495912	14.237107
18.188639	776.455133	14.242125
18.067196	777.550131	14.247143
18.380932	780.660142	14.252160
18.085153	773.315519	14.257178
18.140190	772.151954	14.262195
18.269580	773.163719	14.267213
17.845465	789.118740	14.272231
18.538181	791.024224	14.277248
18.554316	785.600195	14.282266
18.265422	789.914844	14.287283
18.219537	786.715780	14.292301
18.104509	786.307662	14.297319
18.157996	780.764214	14.302336
17.998553	793.105768	14.307354
18.289918	793.085643	14.312371
18.494597	782.220216	14.317389
18.063161	790.160879	14.322407
18.311104	792.356512	14.327424
18.344245	787.327455	14.332442
18.497854	780.720722	14.337459
18.527660	782.148767	14.342477
18.224032	790.287274	14.347495
18.167244	773.845398	14.352512
18.410032	784.641138	14.357530
18.507265	801.881421	14.362547
18.740470	806.626011	14.367565
18.515619	816.639381	14.372583
19.142017	803.508748	14.377600
18.734694	802.972575	14.382618
18.276846	791.074239	14.387635
18.410059	795.553536	14.392653
18.494286	806.534918	14.397671
18.831678	804.652068	14.402688
18.922169	813.363521	14.407706
18.668473	818.449002	14.412723
18.915764	809.126381	14.417741
18.241297	819.711515	14.422759
18.329749	804.932149	14.427776
18.921860	805.878183	14.432794
18.618290	807.916697	14.437811
18.986671	813.511219	14.442829
18.777766	806.591701	14.447847
18.684746	802.131376	14.452864
18.840103	806.989069	14.457882
18.882915	809.118815	14.462899
18.676188	797.844076	14.467917
18.750804	814.371546	14.472935
18.998497	807.024341	14.477952
18.958510	819.596616	14.482970
18.959468	819.735312	14.487987
19.282790	821.414298	14.493005
19.288752	813.896449	14.498023
18.844837	808.752319	14.503040
18.862731	815.196651	14.508058
19.198063	826.195752	14.513075
19.454474	824.707349	14.518093
19.139842	821.726842	14.523111
19.197151	802.341826	14.528128
18.901916	809.292488	14.533146
19.128324	827.632962	14.538163
19.333232	818.660908	14.543181
19.310302	832.167784	14.548199
19.438687	828.140027	14.553216
19.310379	816.250325	14.558234
19.185913	816.124534	14.563251
19.511912	821.425865	14.568269
19.248406	822.192700	14.573287
19.225512	818.958493	14.578304
19.283567	814.326325	14.583322
19.177293	819.704426	14.588339
19.423861	813.111609	14.593357
19.281192	828.019328	14.598375
19.513871	828.475386	14.603392
19.766527	826.163926	14.608410
19.729187	824.680235	14.613427
19.659083	829.096524	14.618445
19.578023	830.421917	14.623463
19.641978	823.393639	14.628480
19.605789	826.659122	14.633498
19.305985	835.052667	14.638515
19.642951	828.253272	14.643533
19.239938	833.627086	14.648551
19.710516	833.796803	14.653568
19.860929	831.233025	14.658586
19.651813	832.641470	14.663603
19.602735	824.071865	14.668621
19.679793	827.168242	14.673639
19.660076	834.890191	14.678656
19.552602	826.638938	14.683674
19.690731	824.493628	14.688691
19.656021	823.520754	14.693709
19.504428	831.058112	14.698727
19.459079	833.624454	14.703744
19.456482	822.494637	14.708762
19.541223	840.143989	14.713779
19.544619	842.245163	14.718797
19.315928	850.747561	14.723815
19.656578	847.693427	14.728832
19.907516	854.372881	14.733850
19.831109	857.720369	14.738867
20.169912	849.598432	14.743885
19.893250	863.211106	14.748903
19.927586	853.871127	14.753920
20.409702	851.056890	14.758938
19.886012	853.934390	14.763955
19.958031	856.848525	14.768973
19.808151	858.610657	14.773991
20.101689	852.755264	14.779008
20.104306	841.668803	14.784026
20.074020	874.161675	14.789043
20.470875	868.763550	14.794061
20.623585	876.139942	14.799079
20.135950	860.973710	14.804096
19.797618	858.372417	14.809114
19.993291	869.368044	14.814131
20.433027	869.249081	14.819149
20.333860	873.875028	14.824167
20.397065	889.930986	14.829184
20.804887	878.841373	14.834202
20.098304	876.493068	14.839219
20.344198	869.114560	14.844237
20.358879	873.864790	14.849255
20.211776	883.320152	14.854272
20.357130	882.328707	14.859290
20.383075	884.852398	14.864307
20.569660	879.190369	14.869325
20.498031	885.588706	14.874343
20.636695	880.666266	14.879360
20.717085	878.593054	14.884378
20.322964	881.137967	14.889395
20.748427	884.776542	14.894413
20.424762	884.896355	14.899431
20.528328	885.198952	14.904448
20.878255	877.700104	14.909466
20.907816	889.235989	14.914483
20.885742	884.146075	14.919501
20.864467	883.016475	14.924519
20.329912	877.700249	14.929536
20.372090	875.541470	14.934554
20.737411	885.339919	14.939571
20.581606	873.732163	14.944589
20.755858	882.903968	14.949607
20.798833	881.931619	14.954624
20.970799	874.946462	14.959642
20.921932	882.837068	14.964659
20.716023	879.539829	14.969677
20.998566	892.898207	14.974695
20.787019	885.486775	14.979712
20.853753	875.037235	14.984730
20.627493	885.940778	14.989747
20.979309	883.639118	14.994765
21.042322	882.127175	14.999783
21.077474	881.840836	15.004800
21.303985	873.051579	15.009818
20.814342	877.498487	15.014835
21.083658	879.911705	15.019853
20.819953	868.251326	15.024871
20.911921	883.842065	15.029888
21.280785	880.786687	15.034906
20.864445	886.519189	15.039923
21.341307	889.304027	15.044941
21.388374	897.671997	15.049959
21.281802	898.086205	15.054976
21.275834	891.561080	15.059994
20.904304	893.373504	15.065011
21.125511	898.612281	15.070029
20.982380	903.541719	15.075047
20.615078	905.662748	15.080064
21.049265	898.264379	15.085082
21.300448	911.299458	15.090099
21.371186	902.458702	15.095117
21.373820	902.237384	15.100135
21.302577	903.589656	15.105152
21.554480	900.864902	15.110170
21.309173	920.153053	15.115187
21.523093	912.397662	15.120205
21.722552	914.114877	15.125223
21.871407	907.404698	15.130240
21.508847	904.311722	15.135258
21.670377	908.796105	15.140275
21.685861	906.811889	15.145293
21.695380	902.865737	15.150311
21.858247	908.523844	15.155328
22.081362	907.810618	15.160346
21.769055	913.634226	15.165363
21.908416	909.882446	15.170381
21.603990	914.262658	15.175399
21.433046	903.225272	15.180416
21.798625	894.130336	15.185434
21.809479	895.422489	15.190451
21.269575	892.890444	15.195469
21.754530	909.625507	15.200487
21.704493	897.843481	15.205504
21.619752	905.461979	15.210522
21.852271	924.836682	15.215539
21.972053	929.681013	15.220557
22.054535	919.153258	15.225575
21.948150	928.595993	15.230592
22.592521	914.806088	15.235610
22.268041	908.428376	15.240627
22.264316	888.440557	15.245645
22.104061	893.637741	15.250663
21.947347	897.521591	15.255680
21.881745	896.780735	15.260698
21.751541	906.845690	15.265715
21.999054	909.909231	15.270733
22.484501	919.038915	15.275751
22.121945	911.875040	15.280768
22.424699	905.547991	15.285786
22.370860	901.583302	15.290803
22.163287	893.915633	15.295821
22.141046	894.717489	15.300839
22.041352	901.464176	15.305856
22.768375	903.604167	15.310874
22.212267	900.989439	15.315891
22.268579	906.468481	15.320909
22.570739	913.297769	15.325927
22.324288	920.338705	15.330944
22.731624	906.809768	15.335962
22.154697	897.747969	15.340979
22.412829	908.427789	15.345997
22.703061	904.491578	15.351015
22.695145	912.120207	15.356032
22.933335	902.417111	15.361050
22.354029	886.785458	15.366067
22.537365	888.050755	15.371085
22.531368	881.156418	15.376103
22.391913	892.197925	15.381120
22.355786	905.811051	15.386138
22.453040	910.617860	15.391155
22.576868	903.311991	15.396173
22.655996	908.254162	15.401191
22.966196	912.469253	15.406208
22.836395	905.269142	15.411226
22.773437	915.696009	15.416243
22.804812	911.850591	15.421261
22.537116	901.752899	15.426279
22.736318	913.177183	15.431296
23.066344	911.506902	15.436314
22.850965	913.680016	15.441331
22.665353	908.464082	15.446349
22.872182	905.061552	15.451367
22.920510	908.130859	15.456384
22.763949	904.014910	15.461402
22.770945	909.602614	15.466419
22.846892	910.007340	15.471437
23.256216	899.128914	15.476455
23.073641	910.707309	15.481472
23.029723	901.647725	15.486490
22.975599	915.137430	15.491507
22.830664	918.116911	15.496525
23.240732	917.933141	15.501543
23.102264	936.403119	15.506560
23.373177	934.773598	15.511578
23.321687	928.889850	15.516595
23.395607	931.210423	15.521613
23.219912	920.479872	15.526631
23.006871	921.396641	15.531648
23.441888	928.804839	15.536666
23.349475	937.017822	15.541683
23.275919	937.224924	15.546701
23.398370	934.810649	15.551719
23.103381	935.273128	15.556736
23.185324	940.142288	15.561754
23.334005	933.782414	15.566771
23.070403	936.439554	15.571789
23.467409	932.461467	15.576807
23.485155	943.263941	15.581824
23.190981	932.479247	15.586842
23.291297	936.720710	15.591859
23.228376	939.378164	15.596877
23.277827	944.902466	15.601895
23.791150	956.205288	15.606912
24.054058	960.755950	15.611930
23.765653	964.076506	15.616947
23.824003	958.002081	15.621965
24.117508	943.676658	15.626983
23.556028	948.592351	15.632000
23.298027	943.681161	15.637018
23.532815	948.050010	15.642035
23.657498	956.560554	15.647053
24.054842	952.976877	15.652071
23.561731	964.774066	15.657088
23.412213	960.461351	15.662106
23.718876	960.211631	15.667123
23.531957	966.157742	15.672141
23.866806	951.639687	15.677159
23.559990	956.733478	15.682176
24.092325	974.464751	15.687194
23.759346	969.265432	15.692211
23.737819	978.041743	15.697229
24.489759	973.957893	15.702247
24.073204	973.483110	15.707264
24.037366	971.342779	15.712282
24.273466	977.150449	15.717299
24.102256	997.200304	15.722317
24.337760	980.905228	15.727335
24.086168	990.742983	15.732352
24.557452	987.602214	15.737370
24.637798	979.851812	15.742387
24.737575	978.974753	15.747405
24.441840	961.048838	15.752423
24.279812	963.163159	15.757440
24.300001	963.522920	15.762458
24.339157	955.870458	15.767475
24.180502	954.869538	15.772493
24.685414	974.236598	15.777511
24.399167	972.384557	15.782528
24.398751	977.408559	15.787546
24.697299	974.370425	15.792563
24.787991	978.199994	15.797581
24.664257	967.199398	15.802599
24.298114	957.584052	15.807616
24.338311	967.297470	15.812634
24.673652	970.602962	15.817651
24.271714	983.209617	15.822669
24.617222	983.064299	15.827687
24.400446	988.027318	15.832704
24.321831	988.733816	15.837722
24.462026	984.600045	15.842739
23.995874	982.015480	15.847757
24.648669	981.099654	15.852775
24.747033	1004.421078	15.857792
24.839005	1003.766135	15.862810
25.062012	1008.190480	15.867827
24.979363	1007.133543	15.872845
25.309803	999.300013	15.877863
25.199527	990.660963	15.882880
24.706724	984.312586	15.887898
24.918916	979.164080	15.892915
24.583459	981.267537	15.897933
25.200749	990.455624	15.902951
25.246520	998.637654	15.907968
25.452363	993.152468	15.912986
25.308219	983.218526	15.918003
24.862643	982.435843	15.923021
24.991997	981.178645	15.928039
25.097893	987.726101	15.933056
25.359408	998.487498	15.938074
25.283996	1001.547685	15.943091
25.332610	1002.975975	15.948109
25.450847	1001.941409	15.953127
25.208316	993.013686	15.958144
25.144006	991.395327	15.963162
25.273325	1001.322101	15.968179
25.293435	998.848013	15.973197
25.435095	993.925076	15.978215
25.582215	991.330230	15.983232
25.579918	991.996444	15.988250
25.629279	987.015296	15.993267
25.474943	987.421165	15.998285
25.262928	995.895789	16.003303
25.205553	991.095358	16.008320
25.083277	996.412888	16.013338
24.852837	996.429826	16.018355
25.462743	994.526617	16.023373
25.893324	995.646132	16.028391
25.725367	991.020705	16.033408
25.487106	992.146527	16.038426
25.371742	995.392811	16.043443
25.692447	1013.229655	16.048461
25.625232	1005.666315	16.053479
26.145640	1025.892538	16.058496
26.205737	1023.377508	16.063514
26.083019	1017.182934	16.068531
26.230375	1014.973050	16.073549
26.210413	1000.743723	16.078567
26.005490	1004.436290	16.083584
25.772351	1004.081269	16.088602
26.023481	990.305195	16.093619
25.772806	989.968684	16.098637
25.914422	1003.727777	16.103655
25.920552	1024.084560	16.108672
25.846187	1028.043978	16.113690
26.183237	1019.388915	16.118707
26.080851	1025.533320	16.123725
25.895211	1023.574093	16.128743
26.041686	1020.348193	16.133760
25.989895	1025.108812	16.138778
26.272523	1024.421029	16.143795
25.837734	1027.492993	16.148813
26.186664	1017.946159	16.153831
26.073485	1026.654714	16.158848
26.108016	1020.344139	16.163866
26.359152	1023.227258	16.168883
26.093789	1036.024121	16.173901
26.547806	1033.233166	16.178919
26.816994	1035.917820	16.183936
26.589426	1021.638750	16.188954
26.561502	1012.860637	16.193971
26.333746	1013.277937	16.198989
26.983492	1007.575312	16.204007
26.971735	1007.712834	16.209024
26.418827	1012.778685	16.214042
26.754566	1000.336936	16.219059
26.304464	1004.752473	16.224077
26.878805	1000.039874	16.229095
26.775020	1005.133625	16.234112
26.493655	1009.753262	16.239130
26.770349	1001.274859	16.244147
26.795991	1008.895149	16.249165
26.572126	1009.438073	16.254183
26.932990	1018.555648	16.259200
26.890522	1021.553906	16.264218
26.969358	1023.024828	16.269235
26.759182	1027.604984	16.274253
26.602213	1024.726125	16.279271
27.296717	1026.751276	16.284288
26.772726	1029.979138	16.289306
27.068704	1025.675939	16.294323
26.999410	1029.751331	16.299341
26.844629	1039.378382	16.304359
27.139520	1027.634084	16.309376
27.085715	1038.132180	16.314394
27.353146	1027.875361	16.319411
26.991841	1037.853297	16.324429
27.226613	1027.090332	16.329447
27.667000	1030.404726	16.334464
27.402437	1028.132744	16.339482
27.411085	1028.708894	16.344499
27.356500	1022.172356	16.349517
26.925260	1033.527619	16.354535
27.254788	1024.106877	16.359552
27.079351	1037.643965	16.364570
27.264017	1029.208279	16.369587
27.285779	1028.346519	16.374605
27.048583	1025.413880	16.379623
27.361599	1029.994628	16.384640
27.278214	1057.977065	16.389658
27.672284	1046.422437	16.394675
27.789164	1051.522870	16.399693
27.561407	1057.923487	16.404711
27.758503	1051.130006	16.409728
27.804330	1061.767235	16.414746
27.964694	1045.726793	16.419763
27.958458	1036.957914	16.424781
27.691512	1034.323390	16.429799
27.511446	1019.503604	16.434816
27.127360	1038.709351	16.439834
27.623873	1052.447938	16.444851
27.677837	1052.581539	16.449869
27.523932	1052.763283	16.454887
27.690026	1050.055023	16.459904
27.724484	1055.218782	16.464922
27.874089	1054.068877	16.469939
28.156677	1065.865279	16.474957
28.136747	1056.271713	16.479975
28.248317	1046.133824	16.484992
27.975767	1052.995842	16.490010
28.045836	1052.764023	16.495027
28.082869	1040.810559	16.500045
28.170975	1052.593051	16.505063
28.086161	1048.809874	16.510080
28.155991	1063.590032	16.515098
28.301468	1067.919168	16.520115
28.221020	1069.509567	16.525133
28.538050	1071.195868	16.530151
28.577092	1056.076853	16.535168
27.922335	1062.010631	16.540186
27.758316	1073.870260	16.545203
27.859784	1072.393339	16.550221
28.454742	1075.185065	16.555239
28.464542	1069.821896	16.560256
28.250131	1082.014420	16.565274
28.337849	1076.194155	16.570291
28.609889	1073.393658	16.575309
28.108057	1068.842284	16.580327
28.556505	1077.624365	16.585344
28.219976	1090.836285	16.590362
28.719318	1097.426664	16.595379
29.243515	1096.199500	16.600397
28.902109	1091.591585	16.605415
28.705427	1094.828457	16.610432
28.550552	1084.978180	16.615450
28.483957	1086.004697	16.620467
28.916749	1099.387174	16.625485
29.025714	1094.456676	16.630503
29.180310	1091.664995	16.635520
28.907328	1088.703204	16.640538
28.912565	1092.252616	16.645555
29.141381	1091.267099	16.650573
28.934140	1101.514570	16.655591
29.068851	1093.395897	16.660608
28.834735	1101.182900	16.665626
29.106067	1096.381754	16.670643
28.892615	1101.098137	16.675661
29.054844	1097.358537	16.680679
29.156111	1102.909534	16.685696
29.185258	1102.668307	16.690714
29.180831	1099.257607	16.695731
29.145132	1101.112437	16.700749
29.037880	1100.740970	16.705767
29.063798	1099.689215	16.710784
29.131514	1106.302618	16.715802
29.013695	1100.350246	16.720819
28.863814	1099.319550	16.725837
29.430645	1124.177633	16.730855
29.416661	1109.745319	16.735872
29.326809	1118.816356	16.740890
29.137383	1111.811635	16.745907
29.375122	1111.149772	16.750925
29.304414	1117.194603	16.755943
29.176241	1108.441518	16.760960
29.373300	1116.685254	16.765978
29.287092	1117.184658	16.770995
29.782133	1128.108588	16.776013
29.566056	1133.156744	16.781031
29.532372	1127.989673	16.786048
29.727232	1130.588085	16.791066
29.734650	1135.333204	16.796083
30.022335	1134.802417	16.801101
29.914976	1131.865324	16.806119
30.401353	1131.909510	16.811136
30.037292	1135.418601	16.816154
30.104677	1130.724938	16.821171
30.335187	1130.203054	16.826189
29.737499	1129.488227	16.831207
30.093066	1132.755887	16.836224
29.928429	1136.230773	16.841242
29.895780	1133.269424	16.846259
30.269789	1136.199702	16.851277
30.329282	1129.124661	16.856295
30.100975	1123.795392	16.861312
30.208413	1133.463718	16.866330
30.397256	1131.638675	16.871347
30.279105	1128.059486	16.876365
30.327307	1130.314662	16.881383
30.347985	1131.195052	16.886400
30.496098	1129.827627	16.891418
30.310384	1129.077060	16.896435
30.413382	1124.115926	16.901453
30.455615	1138.521750	16.906471
30.609545	1125.309810	16.911488
30.206659	1128.884903	16.916506
30.553049	1127.426648	16.921523
30.999332	1125.589926	16.926541
30.632824	1132.495005	16.931559
30.472685	1126.331466	16.936576
30.548675	1138.838572	16.941594
30.605371	1130.732029	16.946611
30.786567	1115.777021	16.951629
30.751499	1125.773639	16.956647
30.665509	1123.486465	16.961664
30.581370	1126.898323	16.966682
30.322473	1125.897222	16.971699
30.870321	1125.038754	16.976717
30.881107	1130.742701	16.981735
30.597174	1130.654360	16.986752
30.673100	1146.282539	16.991770
31.160833	1154.518905	16.996787
31.335704	1154.778847	17.001805
31.027371	1157.966843	17.006823
31.023063	1159.447567	17.011840
31.089069	1150.033074	17.016858
31.042479	1155.717560	17.021875
31.006837	1149.550407	17.026893
31.099431	1156.633322	17.031911
31.280046	1153.528314	17.036928
31.091336	1155.135577	17.041946
31.451444	1159.156765	17.046963
31.511503	1158.645639	17.051981
31.005136	1153.956095	17.056999
31.498389	1139.612039	17.062016
31.219779	1149.182690	17.067034
31.194027	1151.446228	17.072051
31.374881	1147.650069	17.077069
31.159332	1162.326419	17.082087
31.385151	1164.134228	17.087104
31.436805	1179.576869	17.092122
31.680634	1171.867201	17.097139
31.747932	1170.982566	17.102157
31.807838	1173.983845	17.107175
31.851418	1170.950662	17.112192
31.742553	1174.656710	17.117210
31.687538	1167.908749	17.122227
31.689116	1165.099855	17.127245
31.772742	1176.226725	17.132263
31.847176	1173.466446	17.137280
31.711204	1168.337380	17.142298
31.582570	1171.402727	17.147315
31.817356	1167.247876	17.152333
31.786114	1172.156812	17.157351
31.788872	1163.351757	17.162368
32.106747	1166.994518	17.167386
31.877700	1182.376725	17.172403
32.163783	1185.270209	17.177421
32.132962	1193.397982	17.182439
32.060517	1185.175821	17.187456
32.017695	1193.368579	17.192474
32.056572	1197.177860	17.197491
32.409926	1193.124462	17.202509
32.179995	1188.473919	17.207527
32.247562	1191.540280	17.212544
32.374390	1187.436946	17.217562
31.730877	1182.181772	17.222579
32.271192	1184.215170	17.227597
32.177356	1188.426962	17.232615
32.445021	1186.908376	17.237632
32.620509	1185.082252	17.242650
32.503186	1178.347143	17.247667
32.532364	1184.240746	17.252685
32.445456	1201.311272	17.257703
32.366146	1211.523108	17.262720
32.941922	1220.433758	17.267738
33.247866	1220.584932	17.272755
32.958786	1203.427749	17.277773
33.050477	1196.076271	17.282791
33.002989	1192.867916	17.287808
32.964570	1196.957474	17.292826
33.027620	1193.668793	17.297843
32.701188	1190.731085	17.302861
32.673895	1185.818621	17.307879
32.545985	1193.204123	17.312896
32.704690	1206.137052	17.317914
33.015397	1213.858213	17.322931
33.155523	1206.884195	17.327949
33.080851	1214.229859	17.332967
33.156495	1211.188522	17.337984
33.531930	1203.373144	17.343002
33.134586	1205.255889	17.348019
32.961233	1199.441518	17.353037
33.105328	1212.313610	17.358055
33.237953	1208.373470	17.363072
33.437791	1201.235524	17.368090
33.552282	1212.190354	17.373107
33.320922	1196.715692	17.378125
33.226925	1208.728610	17.383143
33.410583	1204.455479	17.388160
33.798996	1209.157077	17.393178
33.570865	1210.947206	17.398195
33.648168	1208.221189	17.403213
33.803236	1210.049485	17.408231
33.661716	1212.807578	17.413248
33.724128	1208.016840	17.418266
33.677557	1212.593661	17.423283
33.911593	1213.576535	17.428301
33.639445	1208.291936	17.433319
33.557289	1205.385620	17.438336
33.522854	1202.787453	17.443354
33.334887	1209.314472	17.448371
33.917920	1212.054430	17.453389
34.052498	1216.817641	17.458407
34.423591	1227.735685	17.463424
34.122795	1213.275359	17.468442
34.371511	1202.639504	17.473459
34.484924	1192.239315	17.478477
34.014157	1190.286593	17.483495
34.514134	1194.355440	17.488512
34.331544	1185.424598	17.493530
34.280549	1191.153963	17.498547
34.502191	1188.500149	17.503565
34.211113	1197.990718	17.508583
33.838092	1190.979837	17.513600
34.109191	1184.307326	17.518618
33.994550	1194.221699	17.523635
34.692217	1201.090505	17.528653
34.533910	1218.399380	17.533671
34.235248	1215.700340	17.538688
34.925306	1216.416555	17.543706
34.636111	1209.102283	17.548723
34.739123	1198.132513	17.553741
34.788217	1190.270121	17.558759
34.319842	1188.661007	17.563776
34.412184	1192.405159	17.568794
34.505827	1209.791562	17.573811
35.113710	1213.704759	17.578829
35.002930	1208.628563	17.583847
35.069750	1207.633548	17.588864
34.711694	1196.763967	17.593882
34.872512	1201.412636	17.598899
34.914974	1198.480608	17.603917
35.169010	1205.418487	17.608935
34.723994	1214.797333	17.613952
34.574078	1218.528716	17.618970
34.815649	1220.261495	17.623987
35.041625	1220.481924	17.629005
34.863273	1214.188646	17.634023
34.770706	1225.690116	17.639040
35.058291	1214.903036	17.644058
34.982314	1217.376371	17.649075
35.136352	1214.426969	17.654093
35.221697	1216.991952	17.659111
35.137524	1246.757827	17.664128
35.175353	1233.854216	17.669146
35.484801	1234.484525	17.674163
35.645051	1233.430781	17.679181
35.696596	1226.438990	17.684199
35.572151	1242.492924	17.689216
35.406078	1225.319723	17.694234
35.584664	1242.522521	17.699251
35.819362	1225.088108	17.704269
35.791962	1230.861148	17.709287
35.517923	1226.788660	17.714304
36.142974	1223.090583	17.719322
35.501052	1225.954990	17.724339
35.536116	1233.116320	17.729357
35.637299	1230.295064	17.734375
35.660921	1227.637362	17.739392
35.817992	1224.393997	17.744410
35.677111	1243.397997	17.749427
35.754616	1232.574187	17.754445
35.757008	1246.090057	17.759463
35.917815	1246.702484	17.764480
36.220980	1247.504184	17.769498
36.318950	1250.894024	17.774515
36.450502	1250.813575	17.779533
36.102113	1238.131039	17.784551
35.738742	1229.338775	17.789568
36.208614	1242.330580	17.794586
36.461311	1254.942799	17.799603
36.331930	1253.937304	17.804621
36.226980	1254.297620	17.809639
35.885182	1253.012773	17.814656
36.705653	1243.196743	17.819674
36.337845	1252.039727	17.824691
36.483735	1241.236822	17.829709
36.532137	1253.568425	17.834727
36.510027	1255.171848	17.839744
36.663286	1247.372108	17.844762
36.255273	1253.267531	17.849779
36.481469	1249.205516	17.854797
36.687161	1241.908853	17.859815
36.804593	1244.206913	17.864832
36.560052	1244.399615	17.869850
37.020815	1256.376684	17.874867
36.542976	1265.991040	17.879885
37.040330	1268.479260	17.884903
36.730893	1272.147129	17.889920
37.116842	1265.119036	17.894938
36.902509	1270.296346	17.899955
37.276248	1268.025938	17.904973
37.334592	1263.466191	17.909991
36.917006	1267.987183	17.915008
37.150446	1264.185968	17.920026
37.203675	1263.016342	17.925043
37.238977	1260.726044	17.930061
37.299887	1271.124366	17.935079
37.005457	1268.714992	17.940096
37.209725	1253.368114	17.945114
37.272985	1269.752609	17.950131
37.264249	1267.267196	17.955149
37.000581	1265.957561	17.960167
37.524845	1259.513848	17.965184
37.500465	1255.399327	17.970202
37.156254	1261.287975	17.975219
37.034799	1266.015324	17.980237
37.891385	1278.877519	17.985255
37.371518	1288.331173	17.990272
37.560948	1287.269728	17.995290
37.804837	1283.091342	18.000307
37.597379	1293.326333	18.005325
37.880918	1285.935481	18.010343
37.436044	1297.154178	18.015360
37.944519	1287.238378	18.020378
37.800819	1282.381881	18.025395
37.863882	1285.483673	18.030413
38.036281	1284.715212	18.035431
38.116595	1280.887342	18.040448
37.930453	1278.625208	18.045466
37.924684	1292.647312	18.050483
38.276065	1306.882063	18.055501
38.760562	1302.820846	18.060519
38.411197	1294.859500	18.065536
38.224230	1287.409359	18.070554
38.144253	1288.049808	18.075571
38.178627	1277.996390	18.080589
38.563218	1287.795217	18.085607
38.204451	1301.632447	18.090624
38.281603	1307.976213	18.095642
38.756471	1304.576057	18.100659
38.534241	1314.002319	18.105677
38.449550	1314.239561	18.110695
38.331600	1313.453189	18.115712
38.417862	1307.345897	18.120730
38.059637	1305.779582	18.125747
38.155458	1309.835642	18.130765
38.850022	1309.689625	18.135783
38.872156	1324.332259	18.140800
38.837300	1323.428808	18.145818
38.541872	1327.927639	18.150835
38.752501	1329.355977	18.155853
38.987097	1322.177858	18.160871
38.968133	1323.474684	18.165888
39.049114	1319.381614	18.170906
39.018131	1321.633364	18.175923
38.780285	1327.451824	18.180941
39.116367	1328.261027	18.185959
39.169582	1327.119801	18.190976
39.207479	1327.760834	18.195994
39.298207	1326.616923	18.201011
39.256633	1328.677820	18.206029
39.481441	1326.970235	18.211047
39.242983	1329.522532	18.216064
39.275145	1329.880436	18.221082
39.173995	1320.072156	18.226099
39.451783	1336.798852	18.231117
39.536404	1345.517792	18.236135
39.746163	1352.320611	18.241152
39.516877	1349.995757	18.246170
39.557272	1348.847058	18.251187
39.493684	1356.462455	18.256205
39.715166	1347.515957	18.261223
39.782356	1357.752406	18.266240
39.957531	1350.368931	18.271258
40.093000	1349.511543	18.276275
39.798546	1356.973536	18.281293
39.983648	1349.399168	18.286311
39.637726	1357.203690	18.291328
39.771617	1350.098043	18.296346
39.749872	1344.989011	18.301363
39.808857	1351.117871	18.306381
40.051598	1343.682854	18.311399
39.894238	1350.539674	18.316416
40.019873	1359.946514	18.321434
39.979678	1363.951179	18.326451
40.069285	1374.881582	18.331469
40.319745	1370.389727	18.336487
40.370932	1372.451964	18.341504
39.982840	1368.412980	18.346522
40.125325	1372.761591	18.351539
40.141510	1376.858468	18.356557
40.367058	1372.604021	18.361575
40.579553	1372.015507	18.366592
40.469193	1379.985335	18.371610
40.989038	1396.503986	18.376627
40.872282	1392.470088	18.381645
40.800209	1377.942460	18.386663
40.669757	1376.507933	18.391680
40.900921	1396.075866	18.396698
40.853155	1395.130239	18.401715
40.938824	1400.257722	18.406733
41.444932	1393.384442	18.411751
41.122031	1382.714401	18.416768
40.920618	1374.868839	18.421786
40.894888	1374.307948	18.426803
40.953010	1391.782111	18.431821
41.149837	1394.957770	18.436839
41.043280	1403.015379	18.441856
41.223705	1403.940339	18.446874
41.573640	1404.624311	18.451891
41.362336	1396.038663	18.456909
41.706159	1386.716491	18.461927
41.843523	1397.248150	18.466944
41.303700	1389.524699	18.471962
41.524322	1385.507703	18.476979
41.513814	1392.761399	18.481997
41.782830	1386.429966	18.487015
41.845600	1380.073841	18.492032
41.247750	1378.756267	18.497050
41.498370	1384.422955	18.502067
41.287673	1389.372515	18.507085
41.752095	1392.345564	18.512103
41.767770	1391.693018	18.517120
41.604075	1395.612777	18.522138
41.895534	1398.685340	18.527155
41.831011	1399.405439	18.532173
41.834940	1401.512908	18.537191
41.514107	1387.986526	18.542208
42.041825	1394.323289	18.547226
42.072821	1395.729107	18.552243
41.939777	1405.248829	18.557261
42.220742	1403.661882	18.562279
42.103379	1410.458849	18.567296
42.306288	1417.717198	18.572314
42.205161	1409.142792	18.577331
41.973126	1421.073202	18.582349
42.213386	1408.346232	18.587367
42.567122	1408.054464	18.592384
42.378697	1406.291289	18.597402
42.388602	1405.421890	18.602419
42.419774	1420.369309	18.607437
42.568674	1413.172938	18.612455
42.553435	1414.715345	18.617472
42.601821	1420.454556	18.622490
42.510268	1416.243159	18.627507
42.663682	1408.569557	18.632525
42.419550	1409.639514	18.637543
42.356397	1414.458811	18.642560
42.463284	1431.227983	18.647578
43.284949	1429.979730	18.652595
42.963601	1438.427406	18.657613
42.704370	1440.411749	18.662631
43.526940	1437.784259	18.667648
43.032306	1446.328345	18.672666
43.396315	1434.686628	18.677683
43.439596	1422.851856	18.682701
43.526358	1419.382716	18.687719
43.309838	1426.356075	18.692736
43.190098	1419.952612	18.697754
43.323998	1419.246945	18.702771
43.260484	1421.368072	18.707789
43.261334	1431.769527	18.712807
43.574341	1420.391382	18.717824
43.639824	1417.373682	18.722842
43.463990	1410.944242	18.727859
43.759455	1411.567267	18.732877
43.640229	1412.684049	18.737895
43.732087	1413.345086	18.742912
43.444247	1418.256172	18.747930
43.605971	1415.122502	18.752947
43.510567	1419.681733	18.757965
43.616109	1419.049908	18.762983
43.607157	1423.406331	18.768000
43.906124	1441.818193	18.773018
44.069634	1441.313044	18.778035
43.817717	1440.850483	18.783053
43.564909	1444.948230	18.788071
44.089931	1445.358790	18.793088
43.465962	1444.540742	18.798106
44.207891	1440.543555	18.803123
43.925843	1454.173298	18.808141
43.901622	1459.144336	18.813159
44.300390	1466.690950	18.818176
44.255699	1475.411151	18.823194
44.151773	1465.805196	18.828211
44.138241	1477.824702	18.833229
44.571622	1463.382410	18.838247
44.661708	1468.442953	18.843264
44.491215	1475.055712	18.848282
44.737562	1471.107275	18.853299
44.476746	1472.836246	18.858317
44.334698	1473.214965	18.863335
44.899778	1483.074162	18.868352
44.855866	1491.090499	18.873370
44.836100	1486.722740	18.878387
45.002278	1494.775797	18.883405
45.082139	1488.653661	18.888423
45.308541	1490.824333	18.893440
45.340687	1493.994092	18.898458
45.294346	1470.745966	18.903475
45.108845	1477.234828	18.908493
45.331304	1462.711766	18.913511
45.126679	1458.287588	18.918528
45.289619	1456.573844	18.923546
45.321268	1469.927538	18.928563
45.123502	1475.938623	18.933581
45.355667	1486.676484	18.938599
45.230003	1482.072746	18.943616
45.111302	1482.993789	18.948634
45.117701	1481.654713	18.953651
44.972560	1481.166060	18.958669
45.021200	1477.851168	18.963687
45.579959	1501.208860	18.968704
45.373181	1511.563792	18.973722
45.679065	1502.897568	18.978739
46.011196	1506.500310	18.983757
45.853467	1514.086250	18.988775
46.406311	1509.525190	18.993792
45.881409	1501.215536	18.998810
46.172479	1508.283469	19.003827
46.214463	1500.968007	19.008845
46.246549	1497.845039	19.013863
46.460131	1493.598739	19.018880
46.396960	1486.268096	19.023898
46.705006	1484.822095	19.028915
46.498198	1476.425057	19.033933
46.350600	1466.740694	19.038951
46.647359	1454.311010	19.043968
46.671785	1465.652406	19.048986
46.615048	1457.209922	19.054003
46.762581	1460.235477	19.059021
46.701437	1455.905725	19.064039
46.532205	1452.296553	19.069056
46.549428	1466.716005	19.074074
46.459050	1454.592750	19.079091
46.267500	1468.262062	19.084109
46.629914	1476.066806	19.089127
46.965240	1477.131756	19.094144
46.891194	1482.574466	19.099162
46.900662	1480.013605	19.104179
47.138912	1479.013975	19.109197
46.761432	1486.214391	19.114215
47.029472	1483.985660	19.119232
47.009314	1487.027860	19.124250
46.953701	1485.528023	19.129267
46.942734	1483.014525	19.134285
46.990587	1488.968438	19.139303
47.108069	1483.484236	19.144320
46.885008	1496.476816	19.149338
47.066432	1516.150456	19.154355
47.145200	1522.260515	19.159373
47.133844	1505.135540	19.164391
47.351713	1506.209311	19.169408
47.432967	1514.401833	19.174426
47.800596	1514.773783	19.179443
47.746864	1508.871257	19.184461
47.542725	1511.377211	19.189479
47.816992	1502.895793	19.194496
47.616719	1518.191758	19.199514
48.041952	1526.472742	19.204531
48.118366	1531.948847	19.209549
48.327201	1533.352234	19.214567
48.241555	1515.825400	19.219584
47.902337	1504.848554	19.224602
47.971316	1507.880035	19.229619
48.108531	1512.093800	19.234637
48.023098	1524.919804	19.239655
48.576500	1528.658515	19.244672
48.654245	1522.281073	19.249690
48.332380	1509.941355	19.254707
48.281052	1503.719717	19.259725
48.272533	1502.080001	19.264743
48.687394	1504.817787	19.269760
48.619362	1511.054840	19.274778
48.252767	1506.952516	19.279795
48.785637	1514.992673	19.284813
48.378909	1521.901008	19.289831
48.430912	1512.075089	19.294848
48.493544	1527.374310	19.299866
48.561808	1524.570756	19.304883
48.798634	1521.933464	19.309901
48.742088	1526.145842	19.314919
48.998144	1521.173390	19.319936
49.005614	1527.739525	19.324954
49.178893	1510.270214	19.329971
48.971585	1510.135225	19.334989
49.150404	1519.631699	19.340007
48.666909	1515.702210	19.345024
48.922455	1530.346542	19.350042
49.145849	1541.322490	19.355059
49.029739	1549.880276	19.360077
48.932776	1550.924172	19.365095
49.151103	1544.247120	19.370112
49.114205	1550.630820	19.375130
49.305965	1557.332377	19.380147
49.650537	1566.418057	19.385165
49.509517	1571.145376	19.390183
49.338046	1571.582327	19.395200
49.476518	1580.977817	19.400218
49.539901	1580.242097	19.405235
49.705096	1575.520466	19.410253
49.622790	1568.625120	19.415271
49.692752	1573.325904	19.420288
49.693438	1592.393442	19.425306
49.866027	1603.449922	19.430323
50.440560	1594.221112	19.435341
50.159679	1599.727619	19.440359
50.429191	1593.497023	19.445376
50.526233	1590.849927	19.450394
50.705015	1597.218999	19.455411
50.518868	1585.965802	19.460429
50.479316	1601.075865	19.465447
50.476912	1586.351023	19.470464
50.735007	1586.923068	19.475482
50.618485	1581.342724	19.480499
50.692260	1568.584754	19.485517
50.804933	1580.846616	19.490535
50.629194	1583.190366	19.495552
50.490878	1591.486538	19.500570
50.674993	1585.692124	19.505587
50.973376	1583.707969	19.510605
50.832328	1584.641964	19.515623
51.047259	1583.904739	19.520640
51.001832	1581.696398	19.525658
51.006960	1593.160803	19.530675
50.893844	1583.332150	19.535693
50.939120	1592.092051	19.540711
50.814934	1590.937402	19.545728
51.204350	1588.787592	19.550746
50.938050	1588.428253	19.555763
51.523261	1593.118249	19.560781
51.321769	1606.142265	19.565799
51.357398	1598.499544	19.570816
51.665914	1607.243714	19.575834
51.561110	1598.530931	19.580851
52.085187	1599.809502	19.585869
51.527575	1591.908848	19.590887
51.471694	1587.095400	19.595904
51.334863	1594.129001	19.600922
51.296484	1598.130280	19.605939
51.779141	1597.815282	19.610957
51.706405	1601.701989	19.615975
52.196949	1595.446446	19.620992
51.659042	1596.442230	19.626010
52.042070	1591.468926	19.631027
51.747546	1595.828826	19.636045
51.880462	1600.308373	19.641063
52.533117	1611.832922	19.646080
52.436526	1619.396763	19.651098
52.054525	1613.602118	19.656115
52.032796	1612.945921	19.661133
52.604604	1617.514931	19.666151
52.560276	1622.940434	19.671168
52.568892	1624.223521	19.676186
52.717187	1622.313222	19.681203
52.960797	1617.020785	19.686221
52.740136	1616.010545	19.691239
52.671905	1614.733572	19.696256
53.222180	1610.005627	19.701274
52.789714	1620.490436	19.706291
53.092427	1615.624305	19.711309
52.746055	1619.793464	19.716327
52.713692	1617.106551	19.721344
52.651604	1616.797469	19.726362
52.594668	1619.009116	19.731379
52.779965	1619.191702	19.736397
52.765304	1617.650764	19.741415
52.977806	1630.540912	19.746432
53.137588	1639.431334	19.751450
53.024474	1642.847801	19.756467
53.147685	1644.510686	19.761485
53.211415	1642.654578	19.766503
53.045408	1631.729582	19.771520
53.340771	1652.890978	19.776538
53.299139	1667.673212	19.781555
53.594804	1658.948543	19.786573
52.848903	1664.240288	19.791591
53.271070	1673.762074	19.796608
53.308909	1673.456369	19.801626
54.022902	1688.215649	19.806643
54.464493	1684.116844	19.811661
54.426726	1695.228224	19.816679
54.253437	1689.246421	19.821696
54.590071	1689.645292	19.826714
54.385054	1678.290831	19.831731
54.347878	1658.723931	19.836749
54.150905	1660.351459	19.841767
53.859458	1662.397648	19.846784
54.349573	1669.835450	19.851802
54.558103	1686.399685	19.856819
54.862515	1684.338839	19.861837
54.713351	1697.010784	19.866855
54.901634	1686.948951	19.871872
54.928194	1692.316100	19.876890
54.589436	1679.540228	19.881907
54.883909	1683.249857	19.886925
54.906337	1684.268861	19.891943
54.683257	1688.305229	19.896960
55.068527	1685.487008	19.901978
54.647423	1688.629538	19.906995
54.715793	1677.709049	19.912013
55.042785	1693.333333	19.917031
54.734781	1684.885680	19.922048
55.022609	1684.784055	19.927066
55.091710	1688.219499	19.932083
55.208104	1681.716060	19.937101
55.192120	1689.232667	19.942119
55.030171	1694.341982	19.947136
55.366339	1695.249021	19.952154
55.368630	1698.281450	19.957171
55.327850	1701.951760	19.962189
55.493867	1702.437157	19.967207
55.300017	1711.496284	19.972224
55.570173	1703.564533	19.977242
55.318783	1697.314015	19.982259
55.908394	1704.133568	19.987277
55.929550	1711.758013	19.992295
55.607119	1723.396580	19.997312
55.562451	1723.087941	20.002330
55.743748	1725.076312	20.007347
56.083492	1716.483611	20.012365
55.936361	1724.017495	20.017383
55.882602	1723.293695	20.022400
56.125685	1737.873865	20.027418
56.029435	1749.669742	20.032435
56.592555	1742.995740	20.037453
56.119309	1738.622782	20.042471
56.130580	1744.857038	20.047488
56.117637	1737.527939	20.052506
56.139009	1742.583479	20.057523
56.528322	1746.432994	20.062541
57.013782	1754.004103	20.067559
57.070170	1763.201025	20.072576
57.036514	1758.822738	20.077594
56.976547	1761.751259	20.082611
57.045069	1759.291620	20.087629
57.087770	1766.149010	20.092647
56.829110	1757.548469	20.097664
57.130093	1755.727996	20.102682
57.062465	1761.150856	20.107699
57.475611	1760.303866	20.112717
56.946971	1757.911955	20.117735
57.056605	1755.739412	20.122752
57.686215	1755.676094	20.127770
57.536202	1757.643466	20.132787
57.254250	1759.498834	20.137805
57.437101	1753.467872	20.142823
57.471063	1757.069751	20.147840
57.743791	1765.374591	20.152858
57.582806	1775.820379	20.157875
58.009683	1778.079798	20.162893
57.937616	1789.389085	20.167911
57.908734	1781.661653	20.172928
58.091844	1780.670592	20.177946
57.773098	1777.665316	20.182963
57.933539	1784.390770	20.187981
58.413675	1785.944447	20.192999
58.025732	1790.511448	20.198016
57.998321	1776.421520	20.203034
57.808940	1778.035254	20.208051
58.167904	1784.019725	20.213069
58.510770	1801.680336	20.218087
58.378413	1806.598878	20.223104
58.557962	1805.889244	20.228122
58.672862	1812.637579	20.233139
59.058986	1801.285679	20.238157
59.366279	1793.692099	20.243175
59.214802	1803.072887	20.248192
59.301704	1799.338557	20.253210
59.178043	1785.153152	20.258227
58.749018	1781.675882	20.263245
58.622491	1782.200517	20.268263
58.821064	1794.105159	20.273280
59.467858	1797.305510	20.278298
59.075247	1797.953627	20.283315
59.261179	1790.678752	20.288333
59.398316	1786.513714	20.293351
59.687657	1785.326228	20.298368
59.902805	1784.175541	20.303386
59.697719	1786.413430	20.308403
59.606044	1780.718698	20.313421
59.513751	1779.252951	20.318439
59.814567	1780.124472	20.323456
60.021694	1780.694991	20.328474
59.994848	1786.638543	20.333491
59.741346	1776.263581	20.338509
59.696831	1776.715485	20.343527
59.567053	1771.768322	20.348544
59.475974	1771.937134	20.353562
59.581120	1776.604090	20.358579
59.599472	1784.279497	20.363597
60.090702	1791.442615	20.368615
60.377381	1800.496401	20.373632
60.478062	1800.629046	20.378650
60.282822	1800.700464	20.383667
60.230464	1800.806442	20.388685
60.338619	1800.098457	20.393703
60.221150	1800.460731	20.398720
60.086536	1800.696284	20.403738
60.228388	1818.097867	20.408755
60.369082	1819.003787	20.413773
60.786076	1827.576538	20.418791
60.538488	1837.007023	20.423808
61.034922	1831.201775	20.428826
61.026612	1833.203900	20.433843
60.835452	1831.314872	20.438861
61.061052	1825.296165	20.443879
60.871305	1847.300203	20.448896
61.337490	1850.692791	20.453914
61.457208	1860.634163	20.458931
61.551465	1847.749726	20.463949
61.837974	1852.019224	20.468967
61.726474	1860.106212	20.473984
61.943531	1853.647000	20.479002
61.728649	1846.399792	20.484019
61.683401	1845.538959	20.489037
61.838583	1839.701630	20.494055
61.517998	1844.636865	20.499072
61.729851	1835.331850	20.504090
61.806403	1850.162109	20.509107
61.763694	1852.131721	20.514125
61.796663	1846.392314	20.519143
61.648191	1848.905428	20.524160
61.928264	1843.815535	20.529178
62.091118	1870.732087	20.534195
62.319705	1873.492621	20.539213
62.594592	1869.369235	20.544231
62.499199	1876.024099	20.549248
62.120805	1874.303077	20.554266
62.031229	1870.608832	20.559283
62.253823	1873.382922	20.564301
62.347700	1873.014838	20.569319
62.485290	1885.904211	20.574336
62.858270	1880.335925	20.579354
62.899165	1889.740459	20.584371
62.775747	1902.424320	20.589389
63.016445	1894.430797	20.594407
62.702778	1894.930922	20.599424
62.967705	1896.622260	20.604442
62.899126	1890.904962	20.609459
62.806591	1894.835842	20.614477
62.962724	1893.085246	20.619495
62.662342	1917.249455	20.624512
63.405865	1920.475796	20.629530
63.720234	1916.485112	20.634547
63.402998	1919.419000	20.639565
63.637851	1923.115870	20.644583
63.580368	1926.631032	20.649600
63.705767	1916.875516	20.654618
63.689908	1917.515473	20.659635
63.328010	1923.198800	20.664653
63.665710	1914.230770	20.669671
64.031474	1938.275513	20.674688
64.220038	1919.547369	20.679706
64.069797	1927.731941	20.684723
64.320605	1936.930242	20.689741
64.290809	1941.716084	20.694759
64.429810	1937.465511	20.699776
64.383393	1932.527416	20.704794
64.601383	1938.101527	20.709811
64.487486	1929.604601	20.714829
64.817744	1933.813657	20.719847
64.325583	1938.586277	20.724864
64.830117	1931.135504	20.729882
64.836574	1920.278157	20.734899
64.524622	1930.381453	20.739917
64.512086	1919.886837	20.744935
64.286413	1923.529173	20.749952
64.299222	1934.168908	20.754970
64.310407	1956.179667	20.759987
64.260767	1950.632976	20.765005
65.113537	1955.341375	20.770023
65.112880	1973.033549	20.775040
65.659697	1981.491484	20.780058
65.804325	1973.042651	20.785075
65.732607	1977.876057	20.790093
65.648618	1973.262548	20.795111
65.589326	1972.697396	20.800128
65.917020	1972.419143	20.805146
65.935136	1966.461097	20.810163
65.493757	1984.240835	20.815181
65.890990	1969.510263	20.820199
65.761969	1978.433195	20.825216
65.823622	1981.166085	20.830234
66.212680	1980.436450	20.835251
65.844483	1973.910519	20.840269
66.281134	1975.685586	20.845287
65.844250	1976.350069	20.850304
65.980747	1967.489079	20.855322
66.176878	1978.308589	20.860339
66.188389	1987.910260	20.865357
66.807172	1987.971709	20.870375
66.649545	1976.079485	20.875392
66.381462	1986.939716	20.880410
66.661882	1988.224693	20.885427
66.300730	1995.823573	20.890445
66.889928	1995.201637	20.895463
66.636963	1992.924567	20.900480
67.125474	1998.081025	20.905498
67.286089	2001.054140	20.910515
67.092823	2005.073313	20.915533
67.154172	2002.431714	20.920551
67.167121	2013.005199	20.925568
67.161931	2011.333360	20.930586
67.209607	2001.192253	20.935603
67.170126	2014.017765	20.940621
67.741744	2008.585777	20.945639
67.412981	2003.991434	20.950656
67.484204	2002.121499	20.955674
67.518399	2002.482256	20.960691
67.273988	1999.771492	20.965709
67.348687	1999.715673	20.970727
67.950771	2019.071900	20.975744
67.945013	2027.940950	20.980762
68.366318	2020.443136	20.985779
67.976498	2031.931443	20.990797
68.199994	2029.280373	20.995815
68.317594	2031.496456	21.000832
68.516655	2026.412813	21.005850
68.333902	2028.858702	21.010867
68.364733	2024.189432	21.015885
68.686785	2024.944046	21.020903
68.507684	2020.512597	21.025920
68.775252	2022.067832	21.030938
69.132409	2012.897899	21.035955
68.689683	2029.936250	21.040973
68.537044	2024.314051	21.045991
68.467000	2021.948535	21.051008
68.548436	2031.933834	21.056026
69.311105	2035.179307	21.061043
69.028542	2050.406484	21.066061
69.131913	2034.907380	21.071079
69.371597	2039.644980	21.076096
69.079230	2042.202616	21.081114
69.107823	2047.354951	21.086131
68.859265	2055.072031	21.091149
69.092839	2045.949725	21.096167
69.395091	2060.012841	21.101184
69.485926	2078.776517	21.106202
69.378606	2080.207080	21.111219
69.785027	2083.457533	21.116237
69.836735	2085.560799	21.121255
69.688233	2077.646727	21.126272
69.737909	2090.442633	21.131290
70.296125	2092.804726	21.136307
70.520189	2093.300032	21.141325
70.771522	2079.018138	21.146343
71.278840	2079.074851	21.151360
70.943968	2055.261790	21.156378
71.236109	2045.088908	21.161395
71.257569	2052.536719	21.166413
71.056492	2046.518095	21.171431
71.079223	2048.218753	21.176448
71.115979	2029.990675	21.181466
71.126188	2019.965848	21.186483
70.729633	2022.467115	21.191501
70.955704	2015.315293	21.196519
70.677343	2024.059520	21.201536
70.576187	2035.177825	21.206554
71.131660	2048.374653	21.211571
70.837061	2052.182387	21.216589
71.024969	2051.241059	21.221607
71.313731	2054.238415	21.226624
71.372757	2058.597032	21.231642
71.700291	2053.528095	21.236659
71.599070	2071.188685	21.241677
71.198023	2073.693814	21.246695
71.350857	2070.217417	21.251712
71.547750	2067.551548	21.256730
71.729651	2067.722045	21.261747
71.636029	2069.115760	21.266765
71.488249	2073.007941	21.271783
71.689410	2090.024998	21.276800
71.821682	2095.609349	21.281818
72.223374	2093.577494	21.286835
71.750322	2097.715992	21.291853
71.884188	2093.696565	21.296871
72.031690	2107.727006	21.301888
72.117095	2114.265443	21.306906
72.695825	2122.216681	21.311923
72.501058	2117.898105	21.316941
72.328461	2123.110190	21.321959
72.663164	2110.333301	21.326976
72.884914	2125.510427	21.331994
73.020669	2120.708026	21.337011
73.171806	2127.469774	21.342029
73.004678	2131.576428	21.347047
73.285283	2135.288312	21.352064
73.175636	2151.201897	21.357082
73.560074	2137.508331	21.362099
73.481442	2143.766191	21.367117
73.313542	2147.279651	21.372135
73.504751	2137.172927	21.377152
73.476758	2146.474707	21.382170
73.392328	2144.660550	21.387187
73.485627	2142.683017	21.392205
73.287289	2132.677973	21.397223
73.578223	2154.853714	21.402240
73.380052	2174.871217	21.407258
73.733878	2177.937362	21.412275
73.784102	2171.469296	21.417293
73.591156	2179.752154	21.422311
74.059144	2189.648954	21.427328
74.085902	2194.410278	21.432346
74.723591	2194.336236	21.437363
74.222194	2194.868752	21.442381
74.361975	2188.642368	21.447399
74.737519	2190.818310	21.452416
74.783119	2206.423737	21.457434
75.007569	2183.498614	21.462451
75.005077	2188.185592	21.467469
75.007070	2184.972511	21.472487
75.359641	2178.583606	21.477504
75.206556	2180.040238	21.482522
75.264832	2176.707937	21.487539
75.352621	2187.462387	21.492557
75.295158	2189.005123	21.497575
75.551270	2176.294075	21.502592
75.218460	2186.179846	21.507610
75.473729	2191.615683	21.512627
75.381298	2207.940068	21.517645
75.791085	2208.759930	21.522663
75.565165	2209.448382	21.527680
75.676966	2209.588767	21.532698
75.791493	2211.331956	21.537715
75.686123	2209.495805	21.542733
75.744237	2207.984513	21.547751
76.325439	2216.569757	21.552768
76.025452	2231.995471	21.557786
76.538127	2223.075787	21.562803
76.802084	2222.684372	21.567821
76.493468	2225.863132	21.572839
76.634995	2221.706778	21.577856
76.485504	2226.022157	21.582874
76.549159	2221.978918	21.587891
76.618867	2231.697898	21.592909
76.215622	2226.606983	21.597927
76.657596	2222.271300	21.602944
76.570781	2231.639090	21.607962
76.772286	2241.993996	21.612979
76.625757	2249.575347	21.617997
76.793050	2249.685001	21.623015
77.035880	2239.172530	21.628032
77.262116	2253.724185	21.633050
77.764195	2263.224378	21.638067
77.826499	2257.395062	21.643085
77.817641	2251.513707	21.648103
77.900698	2239.665889	21.653120
77.685668	2250.208735	21.658138
77.791089	2241.093659	21.663155
77.311614	2248.430186	21.668173
77.977501	2258.252029	21.673191
78.493093	2243.509117	21.678208
78.120436	2260.820814	21.683226
78.201474	2248.736607	21.688243
78.143378	2250.260511	21.693261
78.275528	2250.751196	21.698279
78.668705	2246.751326	21.703296
78.625441	2258.160573	21.708314
78.870040	2247.534207	21.713331
78.675481	2249.413889	21.718349
78.378815	2252.417215	21.723367
78.694834	2244.964104	21.728384
78.529247	2258.377499	21.733402
78.761225	2268.077547	21.738419
79.111196	2273.315618	21.743437
78.567840	2272.443949	21.748455
79.633925	2277.359077	21.753472
79.214238	2279.696714	21.758490
79.323612	2275.504326	21.763507
79.563220	2281.274006	21.768525
79.226574	2279.578003	21.773543
79.349423	2277.081431	21.778560
79.172229	2295.751358	21.783578
79.673699	2298.355857	21.788595
79.733817	2300.748189	21.793613
79.583083	2301.557489	21.798631
80.028222	2297.962951	21.803648
79.770596	2304.760004	21.808666
80.190206	2308.399786	21.813683
80.412250	2308.469356	21.818701
80.082154	2322.315533	21.823719
79.919699	2315.782692	21.828736
80.283467	2315.877536	21.833754
80.132352	2321.083178	21.838771
80.091317	2315.421419	21.843789
80.382660	2334.021594	21.848807
80.735264	2341.910302	21.853824
80.797796	2342.254030	21.858842
80.621895	2338.027143	21.863859
80.734325	2339.480321	21.868877
80.975982	2355.266803	21.873895
81.582347	2355.674192	21.878912
81.620160	2353.935662	21.883930
81.568025	2368.335079	21.888947
81.779349	2365.048346	21.893965
81.786203	2357.886335	21.898983
82.047423	2356.996698	21.904000
81.831486	2358.655645	21.909018
81.752900	2356.477618	21.914035
82.182313	2343.297632	21.919053
81.562762	2360.758325	21.924071
82.016797	2357.124517	21.929088
81.770147	2360.350461	21.934106
81.630585	2364.465500	21.939123
81.996276	2356.446000	21.944141
81.758570	2371.928413	21.949159
81.955162	2374.375251	21.954176
82.350552	2383.709072	21.959194
82.316484	2379.930335	21.964211
82.183579	2381.207106	21.969229
82.514313	2402.698420	21.974247
82.711763	2400.654147	21.979264
82.774519	2399.053748	21.984282
82.703270	2411.916051	21.989299
82.814562	2408.808996	21.994317
82.947231	2404.846495	21.999335
82.895426	2403.835167	22.004352
83.166580	2421.775818	22.009370
83.384663	2416.733287	22.014387
83.510194	2421.277311	22.019405
83.498397	2431.962201	22.024423
83.711836	2429.366291	22.029440
83.837132	2425.616385	22.034458
84.125232	2429.336631	22.039475
84.191375	2422.247419	22.044493
83.869171	2426.924273	22.049511
83.932948	2419.223167	22.054528
84.332235	2428.464881	22.059546
84.154337	2420.100769	22.064563
84.031725	2421.953488	22.069581
83.881373	2445.722643	22.074599
84.244245	2440.783804	22.079616
84.233676	2449.868420	22.084634
83.993209	2454.617767	22.089651
84.451215	2464.219610	22.094669
84.520179	2472.013672	22.099687
85.237132	2476.172120	22.104704
85.067693	2475.472612	22.109722
85.005233	2475.245630	22.114739
85.061455	2466.620969	22.119757
85.158988	2465.163482	22.124775
85.159576	2464.547963	22.129792
85.437563	2470.538962	22.134810
85.430168	2472.421087	22.139827
85.682586	2484.655500	22.144845
85.527564	2491.679661	22.149863
86.027431	2483.200529	22.154880
86.258253	2490.098340	22.159898
86.286449	2483.652527	22.164915
86.402599	2477.458126	22.169933
86.269958	2482.263281	22.174951
86.409008	2477.517080	22.179968
86.279716	2477.335219	22.184986
86.203391	2482.816460	22.190003
86.470866	2476.484883	22.195021
86.109105	2485.870364	22.200039
86.221307	2483.511129	22.205056
86.735849	2494.215101	22.210074
86.711038	2495.225726	22.215091
87.123677	2494.236763	22.220109
87.306371	2500.119523	22.225127
87.010500	2501.721497	22.230144
87.336888	2500.922699	22.235162
87.169806	2501.276931	22.240179
87.178892	2497.990101	22.245197
87.359256	2498.911973	22.250215
87.455230	2492.237839	22.255232
87.483507	2498.883147	22.260250
87.714087	2508.836024	22.265267
87.724019	2513.903031	22.270285
87.640563	2521.458896	22.275303
87.803181	2520.676127	22.280320
87.970273	2517.784443	22.285338
88.066708	2517.030915	22.290355
87.933560	2519.428119	22.295373
88.159015	2534.286258	22.300391
88.382538	2535.690595	22.305408
88.518038	2545.532055	22.310426
88.232648	2551.178419	22.315443
88.698089	2535.669851	22.320461
88.453038	2546.583642	22.325479
88.832500	2554.660780	22.330496
89.110478	2544.647623	22.335514
88.833641	2543.876464	22.340531
88.946802	2543.237104	22.345549
89.059561	2538.056293	22.350567
89.201765	2555.228149	22.355584
89.353622	2556.940312	22.360602
89.249030	2565.506258	22.365619
88.972834	2564.734999	22.370637
89.223960	2568.874471	22.375655
89.306281	2575.612386	22.380672
89.830857	2567.975182	22.385690
89.523064	2589.777589	22.390707
89.552256	2587.112506	22.395725
89.725441	2592.775855	22.400743
89.807459	2591.140880	22.405760
90.066063	2591.870682	22.410778
90.700142	2607.460581	22.415795
90.860105	2596.812470	22.420813
91.023004	2590.983163	22.425831
90.643283	2588.167135	22.430848
90.857174	2572.924933	22.435866
90.271085	2589.253936	22.440883
90.971004	2589.040808	22.445901
91.182743	2602.903834	22.450919
91.259058	2598.779639	22.455936
91.146777	2606.898645	22.460954
91.032979	2616.984100	22.465971
91.093761	2604.801813	22.470989
91.275974	2602.674677	22.476007
91.168072	2610.802472	22.481024
91.171893	2622.747457	22.486042
91.230071	2625.821838	22.491059
91.322385	2630.532044	22.496077
91.626305	2639.836056	22.501095
91.678369	2647.440308	22.506112
92.250928	2651.176277	22.511130
92.058577	2658.020109	22.516147
92.213926	2641.849619	22.521165
92.513009	2650.781978	22.526183
92.407060	2644.098196	22.531200
92.471347	2646.499394	22.536218
92.065974	2655.430972	22.541235
92.622696	2658.560294	22.546253
92.673951	2659.230856	22.551271
92.291309	2665.457329	22.556288
92.619215	2668.054189	22.561306
93.084670	2681.186601	22.566323
93.126385	2688.966064	22.571341
93.331530	2685.235232	22.576359
93.345416	2691.589341	22.581376
94.043909	2691.685727	22.586394
93.707366	2689.945484	22.591411
93.790392	2684.586209	22.596429
93.915132	2682.174500	22.601447
93.869399	2680.770861	22.606464
94.298143	2671.763030	22.611482
94.124606	2682.665770	22.616499
94.170799	2670.586704	22.621517
94.133777	2679.767081	22.626535
94.210729	2678.647322	22.631552
94.039101	2672.260956	22.636570
93.769780	2679.962599	22.641587
94.447103	2691.401953	22.646605
94.465537	2702.770316	22.651623
94.348240	2701.463031	22.656640
94.729958	2692.866486	22.661658
94.456658	2709.806513	22.666675
94.693347	2722.523257	22.671693
95.035229	2721.122388	22.676711
95.211819	2721.697694	22.681728
94.935686	2724.631623	22.686746
95.279253	2719.648372	22.691763
95.486286	2718.347400	22.696781
95.495922	2717.165530	22.701799
95.634924	2737.115384	22.706816
95.942260	2733.614805	22.711834
95.903118	2745.967380	22.716851
95.976806	2743.251161	22.721869
96.279863	2738.046976	22.726887
95.965388	2737.486813	22.731904
96.320105	2739.498796	22.736922
96.220614	2751.750309	22.741939
96.432711	2747.592314	22.746957
96.029952	2751.063555	22.751975
96.250946	2757.761013	22.756992
96.247279	2767.791533	22.762010
96.548665	2769.565650	22.767027
96.448164	2776.139585	22.772045
96.714231	2785.266515	22.777063
96.897005	2787.374706	22.782080
97.196199	2774.505037	22.787098
97.492738	2779.347601	22.792115
97.449213	2785.284612	22.797133
97.708115	2778.812242	22.802151
97.522132	2782.530628	22.807168
97.519059	2794.366339	22.812186
97.795799	2805.454689	22.817203
97.712133	2801.235424	22.822221
98.136327	2808.829147	22.827239
98.026187	2809.666867	22.832256
97.921964	2814.063709	22.837274
97.864062	2816.897398	22.842291
98.275797	2826.961115	22.847309
98.528281	2822.850468	22.852327
98.226374	2837.128190	22.857344
98.730952	2829.983181	22.862362
98.685298	2841.888673	22.867379
98.644925	2834.680171	22.872397
99.159204	2846.833034	22.877415
98.642879	2856.353234	22.882432
99.228772	2851.849816	22.887450
99.133215	2850.245621	22.892467
99.262707	2852.661943	22.897485
99.613629	2849.659527	22.902503
99.576116	2872.862522	22.907520
100.030386	2868.632079	22.912538
99.738462	2874.699320	22.917555
99.961190	2873.446390	22.922573
99.823227	2880.966708	22.927591
100.214926	2880.224003	22.932608
100.174155	2877.658140	22.937626
100.200360	2879.901182	22.942643
100.059482	2876.574509	22.947661
100.550072	2884.372541	22.952679
100.514762	2901.244133	22.957696
100.403624	2904.502728	22.962714
100.256937	2902.745529	22.967731
100.373451	2897.551406	22.972749
100.924022	2909.395676	22.977767
100.620785	2926.968629	22.982784
100.891614	2922.520558	22.987802
101.117822	2930.558606	22.992819
101.228022	2925.166624	22.997837
101.630577	2923.456465	23.002855
101.603287	2928.138030	23.007872
101.984252	2938.607423	23.012890
101.992053	2936.608397	23.017907
101.833772	2937.081199	23.022925
102.415544	2933.998642	23.027943
102.371271	2943.353867	23.032960
102.338556	2930.235934	23.037978
102.523271	2942.796810	23.042995
102.417427	2942.305152	23.048013
102.851178	2929.950957	23.053031
102.675638	2934.153787	23.058048
102.838107	2937.328760	23.063066
102.493012	2933.203820	23.068083
102.474094	2933.755918	23.073101
102.810547	2929.556428	23.078119
102.715485	2938.932183	23.083136
103.001957	2950.454648	23.088154
103.218264	2963.976385	23.093171
103.202913	2957.821230	23.098189
103.541951	2956.793205	23.103207
103.156445	2966.993749	23.108224
103.483722	2972.598511	23.113242
103.580094	2983.102771	23.118259
103.685238	2991.244909	23.123277
103.580668	2984.999484	23.128295
103.824353	3001.493187	23.133312
103.589814	3001.179369	23.138330
103.991495	3004.863116	23.143347
103.907524	3011.724925	23.148365
104.282074	3022.419449	23.153383
104.482463	3041.908762	23.158400
104.504040	3039.939141	23.163418
104.624277	3040.346489	23.168435
104.742145	3043.566298	23.173453
105.329330	3048.063854	23.178471
105.222149	3054.518998	23.183488
105.194147	3049.719753	23.188506
105.533578	3056.679776	23.193523
105.671705	3055.089677	23.198541
105.397819	3050.508612	23.203559
105.518732	3060.040170	23.208576
105.766990	3072.098890	23.213594
105.791570	3077.378392	23.218611
105.574495	3082.970100	23.223629
105.922169	3084.348840	23.228647
106.435153	3083.738739	23.233664
106.513761	3073.115637	23.238682
106.397588	3072.966444	23.243699
106.511437	3082.303435	23.248717
107.070691	3097.984315	23.253735
106.986903	3085.022558	23.258752
107.053648	3088.717440	23.263770
107.048092	3084.353390	23.268787
107.109840	3090.558163	23.273805
107.254525	3085.905607	23.278823
107.238398	3090.282489	23.283840
107.150213	3084.829819	23.288858
107.638661	3083.478695	23.293875
107.422640	3109.193650	23.298893
107.647963	3112.605046	23.303911
107.561110	3116.674177	23.308928
107.671521	3106.803573	23.313946
108.170502	3102.992190	23.318963
107.987948	3101.969619	23.323981
108.442972	3124.922669	23.328999
108.110735	3132.050417	23.334016
108.019568	3128.498185	23.339034
108.733789	3121.623409	23.344051
108.561042	3129.209212	23.349069
108.814153	3124.940594	23.354087
108.968212	3129.764407	23.359104
108.697778	3134.518598	23.364122
109.219242	3141.551309	23.369139
109.118793	3164.900193	23.374157
109.023195	3153.745531	23.379175
108.851222	3165.342667	23.384192
108.871664	3163.931845	23.389210
109.037239	3169.672309	23.394227
108.903781	3182.708968	23.399245
109.494231	3192.031779	23.404263
109.872941	3203.836724	23.409280
109.849013	3209.704545	23.414298
110.027341	3202.553374	23.419315
109.987166	3210.765578	23.424333
110.469224	3214.512602	23.429351
110.580055	3225.829037	23.434368
110.442560	3235.817531	23.439386
110.777861	3230.317821	23.444403
110.702860	3232.917527	23.449421
110.885455	3221.725823	23.454439
110.954729	3238.755037	23.459456
110.900092	3253.224988	23.464474
111.134011	3249.928265	23.469491
110.923965	3259.410460	23.474509
111.452753	3261.215501	23.479527
111.358714	3272.813197	23.484544
111.626216	3276.760915	23.489562
111.888241	3272.418283	23.494579
111.729738	3274.175679	23.499597
111.847825	3283.382713	23.504615
112.105936	3292.429080	23.509632
112.099824	3306.923081	23.514650
112.467181	3300.392608	23.519667
112.369162	3304.125812	23.524685
112.751665	3300.872225	23.529703
112.658181	3315.206247	23.534720
112.844200	3322.187103	23.539738
113.181508	3320.805838	23.544755
113.183754	3322.645522	23.549773
113.328425	3321.237438	23.554791
113.061683	3332.278172	23.559808
113.281153	3322.605089	23.564826
113.446297	3339.692064	23.569843
113.582077	3352.216659	23.574861
113.899180	3346.344163	23.579879
114.005576	3351.566821	23.584896
113.785460	3348.681635	23.589914
114.314559	3344.748735	23.594931
114.216803	3350.735406	23.599949
114.547423	3367.436842	23.604967
114.593752	3371.557887	23.609984
114.276960	3374.930645	23.615002
114.526473	3364.189234	23.620019
114.501385	3379.431103	23.625037
114.630419	3390.053606	23.630055
114.700783	3399.773116	23.635072
114.856413	3396.974606	23.640090
115.369651	3392.911606	23.645107
115.526931	3396.434647	23.650125
115.347612	3402.613936	23.655143
115.840949	3412.052980	23.660160
115.927446	3411.745983	23.665178
116.106997	3415.846296	23.670195
116.132104	3408.529528	23.675213
115.963581	3406.797771	23.680231
116.103378	3411.077863	23.685248
116.163814	3407.299977	23.690266
116.759174	3398.938109	23.695283
116.362715	3408.326315	23.700301
116.508529	3414.044685	23.705319
116.645103	3430.757453	23.710336
116.587369	3428.326712	23.715354
117.342205	3421.751649	23.720371
117.216071	3432.104600	23.725389
117.509025	3433.488731	23.730407
117.283948	3429.398644	23.735424
116.942908	3433.788321	23.740442
117.626598	3433.943833	23.745459
117.711646	3449.793537	23.750477
118.129882	3441.594941	23.755495
118.311231	3438.896574	23.760512
118.148533	3438.555782	23.765530
118.389260	3433.635690	23.770547
118.035966	3442.644764	23.775565
118.420902	3439.251903	23.780583
118.578913	3436.617137	23.785600
118.244781	3446.216590	23.790618
118.772880	3453.504043	23.795635
118.704902	3466.215094	23.800653
118.849311	3457.639352	23.805671
118.803471	3455.367720	23.810688
118.957973	3473.434894	23.815706
119.431927	3482.529813	23.820723
119.501229	3487.748817	23.825741
119.361387	3489.591702	23.830759
119.457491	3488.033358	23.835776
119.710342	3504.627094	23.840794
119.994189	3511.832663	23.845811
120.095976	3523.927116	23.850829
120.176756	3517.737865	23.855847
120.445830	3506.163246	23.860864
120.438723	3512.170576	23.865882
120.403009	3522.575781	23.870899
120.487969	3539.886894	23.875917
120.828314	3533.953908	23.880935
121.024318	3527.610998	23.885952
120.680874	3533.374018	23.890970
121.217276	3536.042699	23.895987
121.113480	3553.032876	23.901005
121.200642	3559.098137	23.906023
121.212750	3562.596470	23.911040
120.963734	3567.246441	23.916058
121.427582	3582.664854	23.921075
121.442273	3581.425329	23.926093
121.504291	3590.950558	23.931111
122.016378	3602.267881	23.936128
121.921402	3607.389404	23.941146
122.123733	3594.379577	23.946163
122.159494	3616.006644	23.951181
122.563556	3624.414994	23.956199
122.915061	3632.948311	23.961216
122.948081	3629.266178	23.966234
122.653344	3626.348378	23.971251
122.916376	3643.543493	23.976269
123.259318	3650.815666	23.981287
123.299917	3659.772991	23.986304
123.398240	3648.436332	23.991322
123.455849	3648.818727	23.996339
123.741714	3649.859952	24.001357
123.940252	3669.031454	24.006375
124.635006	3663.358869	24.011392
124.593277	3670.612035	24.016410
124.761143	3655.117275	24.021427
124.672982	3642.758634	24.026445
124.432690	3647.912262	24.031463
124.696509	3637.878609	24.036480
124.568842	3653.212429	24.041498
124.948009	3656.038170	24.046515
124.957557	3656.961449	24.051533
124.982137	3657.756138	24.056551
125.164075	3660.306434	24.061568
124.982885	3668.711238	24.066586
125.199691	3671.877882	24.071603
125.460923	3674.504208	24.076621
125.400488	3680.036995	24.081639
125.678724	3673.889542	24.086656
125.344741	3685.092458	24.091674
125.831542	3684.562165	24.096691
125.968611	3697.307735	24.101709
125.733566	3705.007634	24.106727
125.914252	3715.836911	24.111744
126.123074	3731.124721	24.116762
126.296868	3723.879363	24.121779
126.489968	3740.245901	24.126797
126.845156	3751.691902	24.131815
127.058969	3753.151505	24.136832
126.791817	3754.496616	24.141850
127.122927	3761.284617	24.146867
127.785434	3771.802194	24.151885
127.482504	3779.484288	24.156903
127.907268	3777.088846	24.161920
127.690388	3785.448761	24.166938
127.710120	3787.601393	24.171955
128.189101	3789.038652	24.176973
128.077320	3804.455345	24.181991
128.236846	3794.100126	24.187008
128.139636	3805.181035	24.192026
128.122330	3816.189541	24.197043
128.753872	3825.777723	24.202061
128.299143	3829.127853	24.207079
128.873527	3845.902250	24.212096
129.289769	3851.364031	24.217114
129.416091	3847.329608	24.222131
129.437666	3853.922804	24.227149
129.434539	3860.308380	24.232167
129.676353	3855.381693	24.237184
129.602050	3866.193947	24.242202
130.057217	3879.770715	24.247219
130.294332	3882.318765	24.252237
129.946338	3883.250377	24.257255
130.197018	3863.800382	24.262272
130.324836	3871.743701	24.267290
130.518655	3889.675765	24.272307
130.813421	3890.043336	24.277325
130.855749	3895.759034	24.282343
131.092606	3892.196612	24.287360
130.993501	3904.284722	24.292378
131.216011	3903.754540	24.297395
131.529082	3910.924157	24.302413
131.332320	3919.454595	24.307431
131.030679	3921.338496	24.312448
131.466718	3926.775124	24.317466
131.816938	3933.635965	24.322483
131.939967	3937.047663	24.327501
131.709185	3946.044225	24.332519
132.255215	3940.637743	24.337536
132.184350	3961.038255	24.342554
132.439196	3972.181236	24.347571
132.563404	3973.235023	24.352589
132.611579	3977.949299	24.357607
132.795638	3964.512798	24.362624
132.507252	3982.864063	24.367642
132.929771	3989.473793	24.372659
133.069179	3992.204353	24.377677
132.843792	4007.301184	24.382695
133.203961	4014.583448	24.387712
133.320278	4020.944172	24.392730
133.777037	4022.160814	24.397747
134.267170	4019.928760	24.402765
134.448911	4031.016877	24.407783
134.726519	4028.290810	24.412800
134.947368	4034.086071	24.417818
134.674099	4025.830748	24.422835
135.201761	4025.530806	24.427853
135.421426	4031.982757	24.432871
135.619346	4013.067914	24.437888
135.147846	3996.040610	24.442906
135.348209	4009.874930	24.447923
135.195631	4020.058739	24.452941
135.385555	4028.042958	24.457959
135.536095	4022.840058	24.462976
135.404033	4037.755103	24.467994
135.812847	4028.803359	24.473011
136.246870	4041.288312	24.478029
135.856042	4048.958954	24.483047
135.790581	4044.648187	24.488064
136.251267	4055.986424	24.493082
135.988371	4060.982717	24.498099
136.578448	4065.663147	24.503117
136.515678	4073.721448	24.508135
136.693130	4083.983317	24.513152
136.925804	4091.578998	24.518170
136.900210	4097.778778	24.523187
136.858028	4099.729615	24.528205
137.169018	4120.061387	24.533223
137.459322	4122.317123	24.538240
137.735195	4127.987064	24.543258
137.761068	4148.224381	24.548275
138.139504	4139.949604	24.553293
138.092717	4153.677324	24.558311
138.716091	4139.250656	24.563328
138.877755	4143.028822	24.568346
138.988046	4139.419774	24.573363
138.875193	4137.082739	24.578381
138.937225	4150.654637	24.583399
138.856434	4155.190191	24.588416
139.237265	4147.047602	24.593434
139.200135	4154.505406	24.598451
139.281596	4148.893437	24.603469
139.464941	4168.759066	24.608487
139.518335	4166.247797	24.613504
139.866027	4173.917137	24.618522
139.828814	4179.187644	24.623539
139.968487	4191.664872	24.628557
139.970463	4202.171914	24.633575
140.196771	4204.118838	24.638592
140.270754	4208.330458	24.643610
140.544979	4218.589963	24.648627
140.758843	4235.158878	24.653645
140.571727	4230.368309	24.658663
140.921812	4244.589820	24.663680
141.343675	4251.266031	24.668698
141.429365	4255.589467	24.673715
141.443463	4254.684558	24.678733
141.247716	4274.423102	24.683751
141.467252	4272.807598	24.688768
142.041025	4273.990259	24.693786
142.177817	4282.393184	24.698803
142.192838	4283.277767	24.703821
142.144899	4298.880633	24.708839
142.421809	4301.207917	24.713856
142.838398	4306.890726	24.718874
142.512066	4306.581705	24.723891
142.793269	4304.599932	24.728909
143.037517	4323.708200	24.733927
143.266622	4329.477020	24.738944
143.474184	4326.152643	24.743962
143.564979	4333.953582	24.748979
143.741304	4330.873948	24.753997
143.659030	4337.300422	24.759015
143.826862	4340.086580	24.764032
144.076804	4357.003500	24.769050
144.112458	4350.625297	24.774067
144.352654	4357.310893	24.779085
144.344468	4366.544453	24.784103
144.420392	4375.433506	24.789120
144.848325	4375.758261	24.794138
144.791190	4392.644114	24.799155
144.953591	4389.610828	24.804173
144.921833	4398.084238	24.809191
145.081745	4407.941854	24.814208
144.932596	4414.460832	24.819226
144.991098	4430.605914	24.824243
145.780585	4431.300486	24.829261
145.847165	4430.864007	24.834279
145.815711	4447.711194	24.839296
146.047480	4455.856374	24.844314
146.455213	4463.014629	24.849331
146.544491	4463.161698	24.854349
146.895484	4475.375807	24.859367
146.845439	4476.368376	24.864384
147.220813	4468.049738	24.869402
147.028553	4478.666091	24.874419
147.202766	4483.663885	24.879437
147.454171	4492.746620	24.884455
147.403295	4503.741833	24.889472
147.824777	4489.822932	24.894490
147.726293	4496.589716	24.899507
148.248481	4515.007859	24.904525
148.264753	4509.756284	24.909543
148.367850	4513.275355	24.914560
148.954312	4516.921179	24.919578
148.333683	4523.062241	24.924595
148.727681	4523.695293	24.929613
149.062735	4542.347763	24.934631
148.932636	4545.189807	24.939648
149.111350	4546.108888	24.944666
149.330889	4547.712858	24.949683
149.487685	4561.245059	24.954701
149.470742	4558.264918	24.959719
149.802973	4573.370096	24.964736
149.933616	4566.067993	24.969754
150.314415	4591.180803	24.974771
150.215060	4586.000867	24.979789
150.361213	4600.289129	24.984807
150.191863	4593.308325	24.989824
150.914679	4597.359048	24.994842
150.887912	4617.876533	24.999859
150.825127	4618.470233	25.004877
151.354346	4619.634604	25.009895
151.020677	4622.849243	25.014912
151.103121	4634.956921	25.019930
151.116810	4647.703433	25.024947
151.837821	4647.673238	25.029965
151.906186	4672.541260	25.034983
152.099190	4670.121815	25.040000
152.155086	4667.745812	25.045018
152.359693	4676.766485	25.050035
152.110984	4667.888391	25.055053
152.360087	4678.808598	25.060071
152.763850	4686.021220	25.065088
152.616475	4692.401139	25.070106
152.858435	4706.273706	25.075123
152.926637	4714.573882	25.080141
153.447454	4715.446022	25.085159
153.211165	4724.712121	25.090176
153.031428	4737.858109	25.095194
153.364009	4749.279856	25.100211
153.429421	4759.310197	25.105229
153.900683	4760.704550	25.110247
154.077091	4768.811144	25.115264
154.895404	4775.447922	25.120282
155.029300	4783.460136	25.125299
154.890926	4787.875400	25.130317
155.098666	4791.062592	25.135335
155.272907	4789.176330	25.140352
155.345819	4779.503194	25.145370
155.555363	4789.779407	25.150387
155.774336	4795.739338	25.155405
155.687090	4805.471518	25.160423
156.247435	4804.936060	25.165440
156.121549	4804.690514	25.170458
156.294081	4809.218355	25.175475
156.147714	4812.508028	25.180493
156.362473	4827.110899	25.185511
156.263605	4830.573096	25.190528
156.895269	4834.972645	25.195546
156.544069	4860.824766	25.200563
156.572182	4857.771276	25.205581
157.280456	4864.008570	25.210599
157.646693	4884.057991	25.215616
158.115818	4880.762232	25.220634
158.238161	4891.784371	25.225651
157.854861	4886.231907	25.230669
158.283090	4884.100924	25.235687
157.821322	4899.036444	25.240704
158.439208	4904.482935	25.245722
158.085642	4913.461214	25.250739
158.079756	4922.372742	25.255757
158.701738	4933.743236	25.260775
158.415442	4934.791551	25.265792
158.901174	4951.969022	25.270810
159.118864	4961.786380	25.275827
159.303630	4977.568238	25.280845
159.635079	4987.213233	25.285863
159.528475	4995.663854	25.290880
159.747404	5000.225553	25.295898
159.850516	5015.489874	25.300915
159.683372	5023.328112	25.305933
160.390598	5027.406612	25.310951
160.319899	5047.243315	25.315968
160.519974	5047.167969	25.320986
160.677261	5064.655512	25.326003
161.076742	5060.149013	25.331021
162.175642	5045.063651	25.336039
161.808888	5048.109910	25.341056
162.106187	5047.785849	25.346074
162.138196	5041.859344	25.351091
162.577253	5059.798578	25.356109
162.935038	5058.060475	25.361127
163.068297	5054.955861	25.366144
163.147386	5039.135999	25.371162
163.047267	5036.538034	25.376179
162.814528	5038.038858	25.381197
163.132585	5038.121905	25.386215
163.033875	5052.811639	25.391232
163.359987	5049.617027	25.396250
162.890396	5052.799243	25.401267
163.331240	5061.391928	25.406285
163.581477	5071.785067	25.411303
163.620962	5088.763845	25.416320
163.527619	5078.816570	25.421338
163.691455	5094.759612	25.426355
164.021138	5107.097412	25.431373
164.283211	5114.780484	25.436391
164.433584	5130.277435	25.441408
164.390887	5141.802047	25.446426
164.292425	5151.286796	25.451443
164.970988	5162.680191	25.456461
165.124637	5174.619319	25.461479
164.951244	5182.326026	25.466496
165.175150	5194.910777	25.471514
165.565696	5193.751511	25.476531
165.474373	5206.281184	25.481549
166.208378	5213.524670	25.486567
166.238713	5223.137759	25.491584
166.533201	5231.658616	25.496602
166.455160	5238.798116	25.501619
166.409318	5239.928958	25.506637
166.653291	5245.964058	25.511655
166.876911	5278.586337	25.516672
167.345351	5272.216187	25.521690
167.615465	5280.295796	25.526707
167.527248	5284.261460	25.531725
167.868568	5287.882479	25.536743
167.923887	5287.097362	25.541760
168.020490	5312.823588	25.546778
167.774836	5321.747389	25.551795
167.974404	5330.399861	25.556813
168.647518	5335.392818	25.561831
168.457432	5349.102717	25.566848
168.668552	5360.960420	25.571866
168.937610	5369.658909	25.576883
169.002748	5387.094823	25.581901
169.554180	5393.770225	25.586919
169.568000	5395.564126	25.591936
169.906686	5398.042918	25.596954
170.099553	5416.680547	25.601971
170.002253	5423.194969	25.606989
170.222994	5424.584188	25.612007
170.578984	5436.946525	25.617024
170.687030	5441.714991	25.622042
171.228406	5441.990542	25.627059
171.267026	5444.661257	25.632077
171.592814	5451.554890	25.637095
171.772693	5460.668186	25.642112
171.795612	5461.374831	25.647130
171.857250	5464.850037	25.652147
171.887497	5472.932355	25.657165
172.377911	5474.184896	25.662183
172.067382	5497.992469	25.667200
172.567193	5503.337577	25.672218
172.640161	5495.917819	25.677236
172.795655	5505.249579	25.682253
173.386365	5516.593744	25.687271
173.369801	5516.059705	25.692288
173.852527	5516.227597	25.697306
173.782642	5508.975275	25.702324
173.673176	5510.087630	25.707341
173.902255	5512.346762	25.712359
174.200905	5532.031794	25.717376
174.294913	5526.379568	25.722394
174.561309	5539.134709	25.727412
174.511908	5537.542026	25.732429
174.874206	5531.955351	25.737447
174.684578	5529.125041	25.742464
175.090558	5541.410223	25.747482
175.352877	5553.124349	25.752500
175.063394	5551.726871	25.757517
175.588614	5560.170925	25.762535
175.417927	5576.778842	25.767552
175.549058	5578.374574	25.772570
175.677463	5584.566668	25.777588
175.805563	5596.929873	25.782605
176.396020	5595.752084	25.787623
176.342900	5614.857505	25.792640
176.754652	5622.021909	25.797658
176.837065	5629.082919	25.802676
177.062466	5634.000462	25.807693
177.531646	5636.894576	25.812711
177.817691	5655.492691	25.817728
177.604839	5646.270781	25.822746
177.647816	5648.360041	25.827764
177.751884	5662.374757	25.832781
177.949111	5672.309322	25.837799
178.092062	5687.271287	25.842816
178.099961	5700.909591	25.847834
178.456209	5699.736694	25.852852
178.350321	5722.136434	25.857869
178.817407	5727.515114	25.862887
178.917331	5745.968686	25.867904
179.108334	5752.952863	25.872922
179.434490	5764.272083	25.877940
179.629070	5775.652832	25.882957
180.038610	5772.498769	25.887975
179.801445	5787.942979	25.892992
179.865574	5803.981081	25.898010
180.111069	5807.219393	25.903028
180.160593	5819.314046	25.908045
180.830215	5830.093719	25.913063
180.971171	5844.131241	25.918080
181.322764	5855.490751	25.923098
181.830735	5861.677507	25.928116
182.161898	5850.798810	25.933133
182.545708	5854.836313	25.938151
182.468804	5849.636737	25.943168
182.119721	5860.470862	25.948186
182.526701	5867.793936	25.953204
182.613078	5873.989516	25.958221
183.102049	5879.039703	25.963239
182.860860	5879.424474	25.968256
183.200290	5894.794787	25.973274
183.687054	5904.046767	25.978292
183.504669	5906.392105	25.983309
183.964433	5905.048406	25.988327
183.837308	5928.846926	25.993344
183.798346	5936.744514	25.998362
183.864735	5927.731516	26.003380
183.876554	5947.433244	26.008397
184.116329	5951.856204	26.013415
184.104889	5973.584971	26.018432
184.431739	5989.948502	26.023450
184.866580	6002.734562	26.028468
185.287008	6014.190780	26.033485
185.002142	6002.887058	26.038503
185.305508	6021.517573	26.043520
185.325170	6031.950317	26.048538
186.053486	6046.660454	26.053556
186.008281	6056.989673	26.058573
186.369534	6060.598274	26.063591
186.594757	6071.882895	26.068608
186.636256	6074.363857	26.073626
187.138912	6077.091842	26.078644
186.831509	6083.263571	26.083661
187.297517	6091.480344	26.088679
187.486974	6108.206289	26.093696
187.352733	6100.884835	26.098714
187.933932	6113.802862	26.103732
187.916755	6130.106441	26.108749
188.525983	6126.757083	26.113767
188.661160	6129.261348	26.118784
188.041778	6134.787203	26.123802
188.901820	6151.951729	26.128820
188.634819	6159.452455	26.133837
188.830611	6160.728820	26.138855
188.978585	6169.727486	26.143872
189.381401	6182.625986	26.148890
189.875600	6192.015848	26.153908
189.564523	6202.531748	26.158925
189.979362	6215.131673	26.163943
190.085826	6221.589403	26.168960
190.347821	6240.838975	26.173978
190.469600	6245.116230	26.178996
190.717047	6262.445681	26.184013
190.720614	6264.642160	26.189031
191.243349	6285.202239	26.194048
191.446722	6289.719336	26.199066
191.396115	6295.661755	26.204084
191.567076	6314.092215	26.209101
191.910402	6320.847711	26.214119
192.074859	6331.109719	26.219136
192.131046	6352.774745	26.224154
192.534451	6348.466193	26.229172
192.391810	6370.986090	26.234189
192.773309	6374.983032	26.239207
193.078734	6381.394059	26.244224
192.946735	6399.527694	26.249242
193.333250	6410.607482	26.254260
193.325304	6427.272908	26.259277
193.669584	6436.405291	26.264295
194.209678	6442.372590	26.269312
194.061574	6450.145341	26.274330
194.718612	6462.448880	26.279348
194.808849	6476.551606	26.284365
195.131513	6471.592688	26.289383
195.193547	6489.481547	26.294400
195.372891	6499.280452	26.299418
195.437455	6500.343675	26.304436
195.446409	6518.076678	26.309453
195.729457	6533.525756	26.314471
196.170465	6538.308961	26.319488
196.344027	6547.054449	26.324506
196.648341	6545.858020	26.329524
196.952864	6558.791029	26.334541
197.125347	6576.754323	26.339559
197.110433	6582.328255	26.344576
197.520751	6580.900662	26.349594
197.832335	6578.430939	26.354612
198.096662	6599.028446	26.359629
197.966739	6602.735724	26.364647
197.988057	6605.368266	26.369664
198.211531	6618.042458	26.374682
198.565548	6628.467681	26.379700
198.870492	6628.799006	26.384717
199.181885	6635.057670	26.389735
199.179127	6641.990280	26.394752
199.074090	6654.109548	26.399770
199.578317	6643.493858	26.404788
200.161836	6650.562479	26.409805
200.416837	6654.522356	26.414823
200.290294	6666.228292	26.419840
200.570277	6670.067484	26.424858
200.915597	6662.598537	26.429876
200.764950	6672.455225	26.434893
201.007526	6670.889590	26.439911
201.051355	6686.685402	26.444928
201.010784	6699.719590	26.449946
200.940893	6696.308554	26.454964
201.423948	6711.360462	26.459981
201.622232	6712.598597	26.464999
202.188092	6730.614441	26.470016
202.460436	6745.029951	26.475034
202.448490	6748.731518	26.480052
202.655677	6753.772157	26.485069
203.077835	6760.777554	26.490087
203.186095	6760.022012	26.495104
203.306757	6767.405811	26.500122
203.633330	6781.396215	26.505140
204.039849	6780.537415	26.510157
204.024753	6782.408560	26.515175
204.206330	6774.068542	26.520192
203.974816	6791.416241	26.525210
204.258601	6799.213446	26.530228
204.720813	6818.959635	26.535245
204.911907	6824.318475	26.540263
205.246474	6830.456799	26.545280
205.195368	6850.226118	26.550298
205.343630	6854.824540	26.555316
205.497475	6869.006055	26.560333
205.688905	6884.816940	26.565351
205.962831	6890.090298	26.570368
206.344473	6909.258811	26.575386
206.501666	6911.185222	26.580404
206.699964	6927.380201	26.585421
206.835439	6942.151794	26.590439
207.065636	6946.750111	26.595456
207.191650	6966.110008	26.600474
207.491336	6974.204706	26.605492
207.444694	6982.050276	26.610509
207.604894	6999.356127	26.615527
208.085136	7017.287723	26.620544
208.154399	7021.797469	26.625562
208.576779	7036.726506	26.630580
208.716573	7053.344246	26.635597
208.849831	7056.723372	26.640615
209.390533	7065.197286	26.645632
209.207396	7078.623285	26.650650
209.854483	7093.176449	26.655668
209.887757	7114.684946	26.660685
209.838568	7115.431292	26.665703
210.378994	7119.542556	26.670720
210.417371	7134.910276	26.675738
210.548514	7139.953390	26.680756
210.715048	7153.795371	26.685773
211.466626	7169.029985	26.690791
212.029381	7169.996744	26.695808
212.114181	7190.070422	26.700826
212.189003	7180.042154	26.705844
212.362006	7177.953805	26.710861
212.233759	7178.077941	26.715879
212.705470	7182.288308	26.720896
212.820023	7198.266116	26.725914
212.511000	7207.809967	26.730932
212.572695	7217.188775	26.735949
213.092712	7230.470686	26.740967
213.744377	7247.021537	26.745984
214.086394	7255.406513	26.751002
214.398366	7262.482925	26.756020
214.656250	7257.079297	26.761037
214.365589	7263.479263	26.766055
214.328280	7277.473032	26.771072
214.613769	7277.614833	26.776090
214.819273	7277.705949	26.781108
214.907224	7286.345159	26.786125
215.341825	7302.749914	26.791143
215.487512	7306.310249	26.796160
215.904680	7327.629797	26.801178
215.979873	7326.917263	26.806196
216.375873	7344.366670	26.811213
216.222571	7352.235316	26.816231
216.789459	7352.235444	26.821248
216.675489	7370.436682	26.826266
216.843972	7391.517218	26.831284
216.915541	7399.123581	26.836301
216.725814	7416.515874	26.841319
217.723775	7427.021241	26.846336
217.583585	7441.823527	26.851354
217.880878	7458.161407	26.856372
218.783999	7448.057703	26.861389
218.983983	7448.073914	26.866407
219.701807	7456.217375	26.871424
219.778278	7469.423300	26.876442
219.888977	7463.594251	26.881460
219.969410	7457.539464	26.886477
220.094766	7469.891735	26.891495
220.449040	7482.025277	26.896512
220.635979	7497.651133	26.901530
220.230380	7492.799010	26.906548
220.812779	7501.809620	26.911565
220.814864	7520.876865	26.916583
220.881574	7523.013155	26.921600
221.228272	7535.539365	26.926618
221.525208	7543.830471	26.931636
221.774128	7559.367808	26.936653
221.583216	7583.614057	26.941671
221.920793	7590.209918	26.946688
222.126901	7609.861087	26.951706
222.183107	7613.751102	26.956724
222.463865	7615.462622	26.961741
222.770238	7644.250077	26.966759
223.174812	7654.207107	26.971776
223.510264	7667.625406	26.976794
223.536416	7683.702636	26.981812
224.129291	7679.054901	26.986829
224.089572	7701.929765	26.991847
224.375378	7701.039209	26.996864
224.729410	7718.167186	27.001882
224.954691	7730.286248	27.006900
225.170204	7733.273863	27.011917
225.418971	7761.107608	27.016935
225.494241	7757.680089	27.021952
225.971068	7768.841349	27.026970
225.796851	7790.925933	27.031988
226.430362	7790.385326	27.037005
226.333123	7807.634155	27.042023
226.602193	7812.409740	27.047040
226.678606	7829.802029	27.052058
226.642854	7845.598599	27.057076
226.896520	7855.080436	27.062093
226.940195	7877.191182	27.067111
227.518817	7891.228431	27.072128
227.854143	7905.129937	27.077146
227.757176	7935.739064	27.082164
227.996057	7940.348907	27.087181
228.296046	7962.239903	27.092199
228.625119	7963.830284	27.097216
228.754857	7977.700713	27.102234
228.988294	7989.562962	27.107252
229.376010	7997.107724	27.112269
229.635713	8020.839260	27.117287
230.216661	8029.600956	27.122304
229.805231	8032.518907	27.127322
229.973414	8044.381880	27.132340
230.313393	8060.325341	27.137357
230.595869	8080.448140	27.142375
230.993042	8093.689822	27.147392
231.328636	8109.634009	27.152410
231.834397	8121.580225	27.157428
231.767373	8123.109165	27.162445
231.911841	8149.886359	27.167463
232.520298	8147.291286	27.172480
232.986383	8160.073994	27.177498
232.728929	8173.818588	27.182516
232.995681	8184.532944	27.187533
233.208933	8202.971346	27.192551
233.320990	8205.567891	27.197568
233.407185	8219.236919	27.202586
233.729849	8235.375805	27.207604
233.893691	8249.724151	27.212621
233.854742	8270.200272	27.217639
234.619982	8291.245758	27.222656
235.070903	8307.408937	27.227674
234.862430	8308.341138	27.232692
235.519365	8326.271762	27.237709
236.085460	8340.383917	27.242727
236.317838	8331.918477	27.247744
236.433091	8336.257220	27.252762
236.302790	8356.716090	27.257780
236.669672	8355.677129	27.262797
237.030102	8373.748672	27.267815
237.275357	8387.244680	27.272832
237.311321	8394.184549	27.277850
237.656028	8413.322500	27.282868
237.939087	8412.618604	27.287885
238.371307	8424.049242	27.292903
238.671269	8437.896672	27.297920
238.465836	8445.151963	27.302938
238.198250	8457.749182	27.307956
238.458628	8463.040888	27.312973
238.965057	8480.107964	27.317991
239.605671	8487.061072	27.323008
240.127066	8507.579657	27.328026
240.210732	8514.117514	27.333044
240.598881	8524.263839	27.338061
240.809988	8530.750290	27.343079
241.001684	8545.890109	27.348096
241.357054	8541.575902	27.353114
241.597129	8555.814749	27.358132
241.933229	8562.868965	27.363149
241.974434	8567.888589	27.368167
242.430909	8585.175063	27.373184
242.401218	8579.430661	27.378202
242.146260	8592.865785	27.383220
242.619414	8601.616124	27.388237
242.638970	8627.895700	27.393255
243.070749	8632.099993	27.398272
243.311463	8645.278033	27.403290
243.097578	8654.236386	27.408308
243.391894	8667.620777	27.413325
243.801475	8687.553968	27.418343
243.988860	8699.553285	27.423360
244.201828	8710.670957	27.428378
244.394063	8724.952110	27.433396
244.731919	8749.689000	27.438413
244.942309	8768.744047	27.443431
244.929811	8790.877260	27.448448
245.423670	8795.674933	27.453466
245.459555	8822.034327	27.458484
246.052972	8831.204890	27.463501
246.043993	8846.726636	27.468519
246.156748	8864.632008	27.473536
246.728702	8879.286689	27.478554
246.657751	8889.943531	27.483572
246.810200	8899.072281	27.488589
247.364914	8925.316319	27.493607
247.929611	8942.295824	27.498624
248.278312	8947.280307	27.503642
248.512417	8965.987738	27.508660
248.726676	8974.961674	27.513677
248.836244	8990.256714	27.518695
249.448333	9003.187763	27.523712
249.584457	9004.956662	27.528730
249.872848	9020.798486	27.533748
249.917490	9031.143799	27.538765
250.149239	9046.224121	27.543783
250.454330	9062.903182	27.548800
251.034471	9065.490118	27.553818
251.097578	9088.334903	27.558836
251.433557	9095.878701	27.563853
251.473140	9110.565934	27.568871
252.005961	9117.930709	27.573888
251.955667	9123.858205	27.578906
251.842139	9143.061939	27.583924
252.168942	9154.196883	27.588941
252.420127	9175.986417	27.593959
252.730434	9193.798208	27.598976
253.224942	9204.613456	27.603994
253.551726	9222.852085	27.609012
253.699900	9224.066623	27.614029
253.884654	9243.274537	27.619047
254.104599	9250.088212	27.624064
254.964806	9264.960368	27.629082
254.898747	9284.014784	27.634100
255.329498	9292.257432	27.639117
255.837091	9310.297510	27.644135
256.168594	9309.908074	27.649152
256.552175	9299.300178	27.654170
256.284369	9313.145100	27.659188
256.928531	9319.965371	27.664205
256.957947	9322.679128	27.669223
257.117843	9337.470941	27.674240
257.400847	9347.634090	27.679258
257.467980	9354.086416	27.684276
257.776301	9366.256769	27.689293
258.114260	9373.288906	27.694311
257.816895	9384.833727	27.699328
258.371882	9392.409851	27.704346
258.259764	9420.554859	27.709364
258.599965	9431.665784	27.714381
258.721168	9450.236579	27.719399
259.386741	9460.472832	27.724416
259.734793	9478.140103	27.729434
259.760920	9501.553140	27.734452
259.804359	9516.022245	27.739469
260.682301	9528.858601	27.744487
260.806909	9533.988634	27.749504
261.310444	9546.052941	27.754522
261.028608	9568.472121	27.759540
261.285760	9573.429983	27.764557
261.715380	9588.672532	27.769575
261.789963	9603.979840	27.774592
262.206483	9611.186114	27.779610
262.219692	9631.762966	27.784628
262.592449	9640.687292	27.789645
263.014796	9659.138794	27.794663
263.304855	9672.969749	27.799680
263.385499	9677.014258	27.804698
263.485357	9697.195664	27.809716
263.578835	9710.024828	27.814733
264.472472	9717.396815	27.819751
264.246785	9741.566056	27.824768
264.700003	9749.641234	27.829786
265.072692	9767.270214	27.834804
265.022489	9789.060031	27.839821
265.645285	9798.870587	27.844839
265.919712	9815.728751	27.849856
266.116695	9825.482480	27.854874
266.534530	9844.414776	27.859892
266.622040	9858.482627	27.864909
267.015360	9874.447766	27.869927
267.189937	9884.504957	27.874944
267.465469	9898.729846	27.879962
267.600563	9909.645665	27.884980
268.016391	9933.026990	27.889997
268.372219	9952.935183	27.895015
268.309620	9971.696136	27.900032
268.924125	9976.282742	27.905050
268.719407	10004.297812	27.910068
269.257780	10011.996756	27.915085
269.673981	10036.139065	27.920103
269.435855	10048.151827	27.925120
269.996189	10073.563087	27.930138
270.443253	10089.052760	27.935156
271.428530	10108.376896	27.940173
271.309449	10106.993576	27.945191
271.366699	10119.740259	27.950208
271.599835	10121.399442	27.955226
271.938451	10147.925128	27.960244
272.073534	10156.517297	27.965261
272.780818	10176.945649	27.970279
272.517406	10190.089609	27.975296
273.037627	10199.231205	27.980314
273.289524	10214.091483	27.985332
273.190989	10222.972642	27.990349
273.544092	10241.290266	27.995367
273.696358	10261.956672	28.000384
274.403048	10277.162967	28.005402
274.267109	10299.648717	28.010420
274.650446	10316.351456	28.015437
275.508529	10329.238822	28.020455
275.616429	10341.911466	28.025472
276.058775	10351.668318	28.030490
276.331833	10361.666232	28.035508
276.332715	10376.512044	28.040525
276.912693	10374.233685	28.045543
276.958740	10396.978542	28.050560
277.097622	10415.313901	28.055578
277.510979	10427.629626	28.060596
277.718224	10451.981819	28.065613
277.951218	10461.645026	28.070631
278.053721	10484.472764	28.075648
278.513649	10487.754302	28.080666
278.731895	10513.860372	28.085684
278.774374	10523.411190	28.090701
279.256788	10537.152851	28.095719
278.847339	10562.220048	28.100736
279.305081	10578.437828	28.105754
279.789380	10592.264486	28.110772
279.825187	10611.307558	28.115789
280.689258	10625.962350	28.120807
281.159488	10646.747023	28.125824
281.228389	10646.471067	28.130842
281.621003	10662.197030	28.135860
281.710155	10674.064519	28.140877
282.261061	10684.379296	28.145895
282.841825	10694.477882	28.150912
282.786395	10690.116629	28.155930
283.580608	10710.759370	28.160948
283.599009	10719.887783	28.165965
284.071317	10715.128621	28.170983
284.327773	10732.672418	28.176000
284.437400	10753.885929	28.181018
284.787602	10747.014499	28.186036
284.801782	10763.516202	28.191053
285.034825	10771.171433	28.196071
285.057517	10792.906870	28.201088
285.638624	10802.977046	28.206106
286.097248	10818.961247	28.211124
286.086286	10839.521093	28.216141
286.333174	10847.739384	28.221159
286.275248	10865.704830	28.226176
286.563523	10891.311121	28.231194
287.139452	10909.392635	28.236212
287.160567	10935.779425	28.241229
287.417165	10944.270946	28.246247
287.657308	10971.763534	28.251264
287.795039	10982.145959	28.256282
287.912208	11001.764053	28.261300
287.951039	11030.813130	28.266317
288.616596	11055.843082	28.271335
289.087009	11083.363134	28.276352
289.455172	11100.084725	28.281370
290.259596	11106.782828	28.286388
290.438690	11123.259173	28.291405
291.205228	11138.106375	28.296423
291.497420	11154.609345	28.301440
291.592827	11165.320527	28.306458
292.227706	11172.543935	28.311476
292.437905	11194.446412	28.316493
292.731837	11194.204879	28.321511
292.915158	11205.871753	28.326528
293.131269	11217.877697	28.331546
293.336416	11233.620699	28.336564
293.450404	11255.111960	28.341581
293.684526	11262.773541	28.346599
294.185126	11281.097642	28.351616
294.165734	11296.256778	28.356634
294.534048	11314.194186	28.361652
294.592575	11325.687954	28.366669
295.066591	11340.896611	28.371687
295.360146	11364.103002	28.376704
295.340051	11379.811727	28.381722
295.936608	11400.994369	28.386740
296.110231	11428.425361	28.391757
296.862379	11444.916973	28.396775
296.755457	11453.856858	28.401792
297.107337	11470.641309	28.406810
297.118280	11488.268245	28.411828
297.497194	11507.063044	28.416845
298.009670	11522.417425	28.421863
297.959909	11546.946832	28.426880
298.354225	11572.610171	28.431898
298.868201	11587.323384	28.436916
299.116067	11609.031028	28.441933
299.411682	11623.636174	28.446951
299.938277	11640.513566	28.451968
299.757316	11648.562000	28.456986
300.261466	11670.949746	28.462004
300.230215	11686.496269	28.467021
300.659586	11706.483298	28.472039
301.114843	11741.048119	28.477056
300.847705	11751.936067	28.482074
301.601232	11774.269324	28.487092
301.619449	11794.472022	28.492109
302.202180	11804.820358	28.497127
302.677421	11831.317693	28.502144
302.711336	11853.084188	28.507162
303.040629	11870.333527	28.512180
303.468618	11892.240805	28.517197
303.826153	11913.581231	28.522215
304.366927	11928.666299	28.527232
304.762170	11955.498342	28.532250
305.478898	11962.207252	28.537268
305.595090	11984.873649	28.542285
305.357235	11998.611690	28.547303
305.983123	12009.354441	28.552320
306.047321	12018.716339	28.557338
306.570737	12037.066048	28.562356
306.740192	12052.092192	28.567373
307.327619	12062.070494	28.572391
307.673215	12084.830761	28.577408
308.036432	12095.892330	28.582426
308.612514	12101.600104	28.587444
308.316697	12124.021361	28.592461
308.702446	12147.170160	28.597479
308.953730	12163.781435	28.602496
309.163111	12182.650670	28.607514
309.652905	12193.559969	28.612532
309.602346	12208.124734	28.617549
310.036235	12227.038004	28.622567
310.018094	12257.458812	28.627584
310.217730	12284.047058	28.632602
310.757858	12302.814399	28.637620
310.745680	12331.582923	28.642637
311.312701	12354.574291	28.647655
311.888992	12372.941359	28.652672
312.178680	12406.933217	28.657690
312.611671	12413.954870	28.662708
312.803367	12445.941117	28.667725
313.420698	12458.437994	28.672743
313.552799	12482.043514	28.677760
313.900468	12499.609502	28.682778
314.524081	12521.168128	28.687796
314.388659	12537.429431	28.692813
314.986396	12555.733342	28.697831
315.706129	12570.636338	28.702848
315.931822	12582.155373	28.707866
316.268725	12588.298409	28.712884
316.537622	12608.447166	28.717901
316.754760	12624.877857	28.722919
317.174957	12640.383304	28.727936
317.460152	12657.264460	28.732954
317.878907	12656.394033	28.737972
318.012408	12688.339228	28.742989
318.566770	12702.014442	28.748007
318.434928	12724.382464	28.753024
318.867316	12726.645574	28.758042
319.083811	12746.079508	28.763060
319.322780	12774.291733	28.768077
319.426817	12789.177076	28.773095
319.550406	12807.984509	28.778112
319.973176	12833.127265	28.783130
320.918834	12850.657323	28.788148
320.892902	12872.257478	28.793165
321.197552	12885.558032	28.798183
321.546761	12903.711507	28.803200
321.951663	12920.719521	28.808218
322.284575	12931.227371	28.813236
322.049872	12947.182387	28.818253
322.783154	12966.081368	28.823271
323.255613	12980.053740	28.828288
323.341219	13009.117539	28.833306
323.698493	13023.777331	28.838324
324.002915	13043.965232	28.843341
324.540325	13065.894738	28.848359
324.628111	13076.898715	28.853376
324.745386	13097.425277	28.858394
325.408412	13111.939645	28.863412
325.543091	13146.676955	28.868429
325.744896	13163.397866	28.873447
326.087317	13182.301074	28.878464
325.803027	13201.522919	28.883482
327.050737	13218.655776	28.888500
327.174352	13250.265571	28.893517
327.644779	13275.174132	28.898535
328.117632	13284.529879	28.903552
328.166430	13315.289334	28.908570
328.308907	13328.441766	28.913588
328.775191	13357.787885	28.918605
329.404689	13379.021318	28.923623
329.779272	13393.337653	28.928640
329.590513	13431.697401	28.933658
330.091468	13446.508838	28.938676
330.219588	13472.108843	28.943693
330.291198	13494.063995	28.948711
331.321976	13512.282473	28.953728
331.460307	13533.516757	28.958746
332.394747	13545.128146	28.963764
332.964087	13566.181681	28.968781
333.069656	13588.081129	28.973799
333.324392	13598.497311	28.978816
333.410189	13624.192532	28.983834
334.265155	13634.644763	28.988852
334.242637	13650.058912	28.993869
334.733011	13676.209117	28.998887
335.027489	13691.062365	29.003904
335.095420	13711.603590	29.008922
335.554533	13716.793222	29.013940
335.664500	13739.961650	29.018957
336.026972	13762.042359	29.023975
336.730426	13783.978429	29.028992
336.820594	13809.711117	29.034010
337.456771	13828.986089	29.039028
337.888843	13844.812791	29.044045
337.539470	13854.805259	29.049063
338.205649	13872.095566	29.054080
338.333680	13883.971660	29.059098
338.450972	13908.547604	29.064116
338.848769	13934.058879	29.069133
339.282535	13958.494037	29.074151
339.596930	13991.325925	29.079168
339.950467	13999.181615	29.084186
340.190682	14020.034257	29.089204
340.485746	14047.004877	29.094221
340.925502	14076.593091	29.099239
341.243559	14091.190342	29.104256
341.648921	14112.715292	29.109274
342.320482	14136.396793	29.114292
342.693257	14148.386534	29.119309
343.184118	14169.756128	29.124327
343.957186	14182.463600	29.129344
343.997637	14196.532552	29.134362
344.382099	14207.633110	29.139380
344.807754	14211.706993	29.144397
345.060587	14232.598959	29.149415
345.637289	14242.002175	29.154432
345.803205	14253.689438	29.159450
345.691740	14256.248992	29.164468
346.145879	14279.358181	29.169485
346.262294	14295.853376	29.174503
346.635477	14306.829427	29.179520
346.788681	14337.091107	29.184538
347.135447	14352.520970	29.189556
347.352685	14376.958797	29.194573
347.784940	14401.243175	29.199591
348.448476	14422.178783	29.204608
348.618921	14446.222912	29.209626
348.749852	14478.004149	29.214644
349.425039	14488.702751	29.219661
349.197294	14514.226926	29.224679
349.693843	14532.175859	29.229696
350.015228	14562.626463	29.234714
350.607036	14594.086656	29.239732
350.363829	14611.351837	29.244749
350.919330	14650.131892	29.249767
351.905301	14673.196661	29.254784
352.017143	14698.845069	29.259802
352.044128	14725.075179	29.264820
352.471626	14756.542273	29.269837
352.348419	14781.718929	29.274855
353.195457	14800.279912	29.279872
353.452937	14830.526142	29.284890
353.704709	14854.633920	29.289908
354.410899	14885.148300	29.294925
354.665555	14915.265621	29.299943
355.081269	14939.695378	29.304960
355.449634	14965.910571	29.309978
355.839714	14992.798262	29.314996
356.624907	15020.540342	29.320013
356.803979	15047.255680	29.325031
357.288577	15066.024940	29.330048
357.472699	15090.563583	29.335066
357.472103	15113.940387	29.340084
358.290298	15146.986389	29.345101
358.397956	15154.460802	29.350119
358.697033	15191.235386	29.355136
358.758346	15213.898400	29.360154
359.368629	15241.437486	29.365172
360.017037	15265.092419	29.370189
359.897579	15294.968554	29.375207
361.013073	15315.143141	29.380224
361.204600	15336.870153	29.385242
361.577151	15360.517619	29.390260
361.793139	15382.566170	29.395277
362.326752	15418.088767	29.400295
362.533060	15439.800962	29.405312
363.168810	15464.601388	29.410330
363.446356	15482.578997	29.415348
364.046210	15493.109877	29.420365
364.287889	15520.732017	29.425383
364.594646	15542.166557	29.430400
364.860136	15563.490690	29.435418
365.294574	15568.075135	29.440436
365.792772	15597.372375	29.445453
366.061889	15634.784126	29.450471
366.085247	15649.220009	29.455488
366.821665	15678.464495	29.460506
367.039606	15696.833735	29.465524
367.527107	15718.199276	29.470541
367.509947	15734.024850	29.475559
368.023745	15756.753870	29.480576
368.269020	15770.132017	29.485594
368.643103	15796.524324	29.490612
368.765531	15812.369289	29.495629
369.374698	15845.417462	29.500647
369.709785	15867.160626	29.505664
370.415323	15883.255966	29.510682
370.355183	15908.389546	29.515700
370.813829	15938.025086	29.520717
371.006514	15961.094904	29.525735
371.311865	15981.510023	29.530752
371.711937	16010.321001	29.535770
372.137533	16031.980780	29.540788
372.425442	16061.374635	29.545805
372.690658	16090.977359	29.550823
372.951264	16109.675135	29.555840
373.558620	16157.934645	29.560858
373.993915	16179.902598	29.565876
374.545586	16204.432825	29.570893
375.115420	16242.098989	29.575911
375.544514	16260.631714	29.580928
375.808912	16281.603083	29.585946
376.087626	16299.852897	29.590964
376.311247	16329.579325	29.595981
376.522432	16359.983625	29.600999
376.995884	16384.447301	29.606016
377.499826	16409.597946	29.611034
378.102411	16439.808788	29.616052
378.338008	16456.508381	29.621069
378.341850	16493.922049	29.626087
378.847465	16510.810215	29.631104
379.342675	16545.513385	29.636122
379.552483	16586.814743	29.641140
380.360214	16609.723264	29.646157
380.748268	16629.636644	29.651175
381.062713	16664.440815	29.656192
381.566158	16682.472819	29.661210
381.926626	16715.166407	29.666228
382.603367	16737.558540	29.671245
383.014856	16768.210246	29.676263
383.425004	16783.344790	29.681280
383.648663	16810.017745	29.686298
383.886119	16830.081117	29.691316
384.443730	16854.137484	29.696333
384.364001	16878.400491	29.701351
385.448324	16893.547029	29.706368
385.978806	16928.188548	29.711386
386.249994	16940.748594	29.716404
386.679779	16961.164335	29.721421
387.065292	16986.185725	29.726439
387.348132	16991.719549	29.731456
387.958269	17019.308595	29.736474
388.024424	17041.732972	29.741492
388.097967	17060.514491	29.746509
388.710067	17089.107730	29.751527
389.580439	17103.513913	29.756544
389.836177	17130.283390	29.761562
390.020292	17148.479252	29.766580
390.574882	17158.487472	29.771597
391.082212	17186.143299	29.776615
391.482854	17191.633573	29.781632
392.067344	17212.726686	29.786650
392.260413	17238.716442	29.791668
392.363112	17249.512043	29.796685
392.459778	17283.937473	29.801703
392.826514	17306.065839	29.806720
393.133913	17318.816324	29.811738
393.156594	17349.175730	29.816756
394.001495	17371.523474	29.821773
394.293106	17398.508836	29.826791
394.398740	17417.569975	29.831808
394.693352	17450.976263	29.836826
394.646776	17469.953760	29.841844
395.299684	17495.136331	29.846861
395.936445	17536.126889	29.851879
396.667737	17564.083200	29.856896
397.188576	17594.520208	29.861914
397.333546	17616.929825	29.866932
397.726154	17647.721689	29.871949
397.899594	17669.937420	29.876967
398.273701	17700.258460	29.881984
398.892695	17720.914032	29.887002
399.019519	17757.774044	29.892020
399.818683	17778.925956	29.897037
400.203333	17814.722553	29.902055
400.525304	17833.687251	29.907072
400.927632	17863.681977	29.912090
401.304791	17902.689056	29.917108
401.889494	17927.058410	29.922125
402.258786	17950.324223	29.927143
402.873907	17970.399476	29.932160
403.026954	17992.081785	29.937178
403.362809	18028.688667	29.942196
404.248353	18049.505247	29.947213
404.440271	18080.392218	29.952231
404.956661	18107.994260	29.957248
405.039059	18128.354767	29.962266
405.211950	18164.747219	29.967284
405.586055	18188.890678	29.972301
405.861436	18220.320804	29.977319
406.743488	18248.358873	29.982336
407.281252	18275.629325	29.987354
407.934391	18293.797469	29.992372
408.693965	18306.402404	29.997389
409.342327	18323.642667	30.002407
409.651363	18346.236060	30.007424
410.042623	18362.859374	30.012442
410.151700	18380.834335	30.017460
410.795246	18407.930570	30.022477
410.715640	18429.573779	30.027495
411.278372	18452.329958	30.032512
411.739949	18471.595737	30.037530
411.623702	18508.482386	30.042548
412.393668	18534.169279	30.047565
412.477517	18560.203085	30.052583
413.063584	18597.119549	30.057600
413.247199	18617.648019	30.062618
413.732377	18648.401796	30.067636
414.195358	18672.152973	30.072653
414.769974	18702.216939	30.077671
414.513748	18737.439040	30.082688
415.064911	18753.159661	30.087706
415.326786	18793.854308	30.092724
415.812852	18819.630001	30.097741
417.067646	18846.922298	30.102759
418.014073	18869.461296	30.107776
418.236769	18893.862955	30.112794
418.440333	18920.548269	30.117812
419.293514	18935.343878	30.122829
419.259276	18951.269512	30.127847
419.506227	18979.205351	30.132864
419.989597	18999.472761	30.137882
420.001286	19031.267450	30.142900
420.585827	19056.080485	30.147917
421.058880	19091.631926	30.152935
421.417308	19108.431568	30.157952
421.649195	19137.589284	30.162970
421.858440	19154.848109	30.167988
422.192838	19181.374424	30.173005
422.465136	19209.597260	30.178023
422.389169	19244.084635	30.183040
423.294438	19282.601625	30.188058
423.542637	19311.908687	30.193076
424.047703	19345.130693	30.198093
424.519782	19393.785780	30.203111
424.936267	19421.702180	30.208128
425.173556	19449.918180	30.213146
425.987927	19473.217615	30.218164
426.467706	19507.126151	30.223181
427.167557	19533.096949	30.228199
428.159544	19559.925744	30.233216
428.642171	19580.010660	30.238234
428.680136	19610.014268	30.243252
428.917506	19624.584066	30.248269
429.463630	19656.252349	30.253287
429.901153	19678.953646	30.258304
430.417476	19705.332315	30.263322
431.145220	19738.299201	30.268340
431.285151	19759.063119	30.273357
431.397275	19778.466730	30.278375
431.714496	19817.107915	30.283392
432.703953	19836.836207	30.288410
432.859746	19858.646528	30.293428
433.312682	19888.876584	30.298445
434.249789	19908.373019	30.303463
434.628831	19939.467574	30.308480
435.013827	19968.937547	30.313498
435.229168	19985.387465	30.318516
435.707602	20009.826525	30.323533
436.034362	20046.110091	30.328551
436.385882	20075.496985	30.333568
436.933070	20098.440734	30.338586
437.473945	20135.512468	30.343604
437.772067	20163.966430	30.348621
437.921737	20186.681542	30.353639
438.216810	20223.804344	30.358656
438.567053	20252.970574	30.363674
439.366356	20286.818088	30.368692
439.569279	20326.830130	30.373709
439.886304	20355.609967	30.378727
440.254995	20397.150584	30.383744
440.914740	20432.966037	30.388762
441.287375	20464.694232	30.393780
441.454561	20505.501962	30.398797
442.225124	20542.450256	30.403815
442.070516	20590.270807	30.408832
443.195087	20620.258437	30.413850
443.594659	20659.381279	30.418868
444.063631	20689.294170	30.423885
444.043240	20717.141435	30.428903
444.695932	20765.165277	30.433920
445.507985	20796.484419	30.438938
446.179974	20822.202226	30.443956
446.831772	20863.674486	30.448973
447.428159	20881.455842	30.453991
447.522634	20907.693306	30.459008
447.995788	20940.183762	30.464026
448.315099	20977.487448	30.469044
448.932190	21003.138220	30.474061
448.996363	21027.004900	30.479079
449.556337	21062.792810	30.484096
450.273309	21091.966379	30.489114
450.704727	21130.188007	30.494132
450.813201	21147.281049	30.499149
451.603593	21174.851102	30.504167
451.629418	21214.582928	30.509184
452.266957	21232.345560	30.514202
452.588849	21263.646982	30.519220
452.876834	21292.717039	30.524237
453.316686	21313.442231	30.529255
453.768963	21354.087293	30.534272
454.324447	21389.889135	30.539290
454.385506	21427.271789	30.544308
455.137664	21464.079363	30.549325
455.438206	21487.966669	30.554343
455.847159	21530.659686	30.559360
456.506425	21565.832805	30.564378
456.774040	21601.382880	30.569396
457.173195	21644.185082	30.574413
457.547611	21675.415797	30.579431
458.615667	21699.733582	30.584448
459.074288	21728.360699	30.589466
459.847522	21754.329343	30.594484
459.849357	21794.919070	30.599501
460.599831	21815.861812	30.604519
461.009689	21861.480874	30.609536
461.580665	21886.476535	30.614554
462.349511	21915.030355	30.619572
462.704345	21949.032074	30.624589
462.865552	21971.848549	30.629607
463.398436	22005.348755	30.634624
464.371000	22037.561083	30.639642
464.789557	22064.299352	30.644660
465.106196	22089.227449	30.649677
465.682047	22117.994848	30.654695
466.516507	22144.099804	30.659712
466.595819	22167.908641	30.664730
467.474326	22188.187348	30.669748
467.686013	22216.948397	30.674765
467.738761	22237.760101	30.679783
468.562178	22273.117444	30.684800
468.861000	22289.562616	30.689818
469.776898	22319.054565	30.694836
469.740792	22350.912622	30.699853
470.574069	22370.421361	30.704871
470.693281	22408.049567	30.709888
471.334371	22432.978138	30.714906
471.722560	22459.431009	30.719924
472.038392	22488.568001	30.724941
472.160876	22520.509060	30.729959
472.340459	22559.505639	30.734976
473.240227	22600.513281	30.739994
473.831012	22636.097053	30.745012
473.781193	22671.812211	30.750029
474.462469	22707.009215	30.755047
474.948681	22751.657990	30.760064
475.649218	22782.618529	30.765082
475.895471	22815.747690	30.770100
476.102560	22854.367756	30.775117
476.962413	22894.478628	30.780135
477.033042	22927.736418	30.785152
477.539206	22957.343659	30.790170
478.237450	22989.909874	30.795188
479.001860	23028.974304	30.800205
479.575740	23057.484303	30.805223
479.849981	23092.707446	30.810240
480.923950	23126.017895	30.815258
481.204371	23148.027302	30.820276
481.475070	23178.556181	30.825293
482.258454	23208.619838	30.830311
483.111745	23244.985302	30.835328
483.071734	23268.795080	30.840346
483.134875	23289.612589	30.845364
483.504840	23323.639591	30.850381
484.241886	23338.633554	30.855399
484.735883	23381.045610	30.860416
485.065629	23414.965287	30.865434
485.403821	23442.703697	30.870452
485.761149	23486.375783	30.875469
486.341216	23510.695947	30.880487
486.590226	23553.765777	30.885504
486.862843	23592.686711	30.890522
487.197121	23627.831947	30.895540
487.904350	23678.280916	30.900557
488.364343	23709.665817	30.905575
488.729958	23759.485710	30.910592
489.409116	23797.528588	30.915610
489.746679	23837.684761	30.920628
490.322057	23881.905132	30.925645
490.607538	23918.461331	30.930663
490.969743	23965.255383	30.935680
491.867616	24025.874736	30.940698
492.355967	24061.837206	30.945716
492.945720	24109.247052	30.950733
493.712982	24141.014505	30.955751
494.097595	24181.998188	30.960768
494.347183	24227.148420	30.965786
495.368793	24254.579352	30.970804
495.738294	24300.083919	30.975821
496.326758	24332.524082	30.980839
496.833989	24378.102175	30.985856
497.171872	24412.287695	30.990874
497.825855	24442.038438	30.995892
498.093429	24491.723758	31.000909
498.990434	24521.367273	31.005927
499.319617	24571.889997	31.010944
499.840016	24612.145652	31.015962
500.710870	24636.902198	31.020980
501.017818	24687.978464	31.025997
501.700614	24712.195631	31.031015
501.922167	24748.946567	31.036032
502.649689	24782.920396	31.041050
503.009621	24810.954339	31.046068
503.966557	24843.767694	31.051085
505.068758	24867.388923	31.056103
505.197571	24901.291852	31.061120
505.806718	24924.781363	31.066138
506.833237	24948.515582	31.071156
507.119153	24971.827966	31.076173
507.506156	24993.519482	31.081191
507.865499	25023.607659	31.086208
508.615874	25045.773504	31.091226
509.188477	25067.809060	31.096244
509.415435	25099.339856	31.101261
510.124945	25117.543465	31.106279
510.569506	25155.903515	31.111296
510.739639	25180.668709	31.116314
511.521652	25208.150894	31.121332
511.757847	25234.283539	31.126349
512.204983	25262.361416	31.131367
512.586033	25295.549547	31.136384
513.197345	25325.042825	31.141402
513.714971	25351.852249	31.146420
513.828090	25388.229420	31.151437
514.299151	25423.963206	31.156455
514.656147	25460.485813	31.161472
514.787784	25508.254678	31.166490
515.869359	25538.755727	31.171508
515.965073	25578.017730	31.176525
516.400917	25618.629836	31.181543
516.984122	25652.292663	31.186560
517.357668	25695.581547	31.191578
517.950026	25725.944170	31.196596
518.022314	25767.706490	31.201613
518.881224	25795.948521	31.206631
519.556258	25836.890379	31.211648
519.938993	25880.241428	31.216666
520.575717	25911.242043	31.221684
520.831892	25954.650873	31.226701
521.662072	25991.524208	31.231719
521.975734	26037.174127	31.236736
522.306314	26077.917304	31.241754
523.330797	26114.476224	31.246772
523.824039	26169.325498	31.251789
524.325896	26207.590158	31.256807
525.041074	26241.783258	31.261824
525.264818	26282.568761	31.266842
525.736616	26318.815936	31.271860
526.107466	26369.248214	31.276877
526.428579	26397.012337	31.281895
527.338364	26448.726026	31.286912
527.752268	26498.342967	31.291930
528.641498	26534.177946	31.296948
528.672024	26587.261270	31.301965
529.295600	26632.617808	31.306983
530.193539	26670.764806	31.312000
530.476179	26716.345250	31.317018
531.442523	26754.412236	31.322036
532.037147	26798.977327	31.327053
532.613365	26840.069328	31.332071
533.288661	26863.873135	31.337088
533.662601	26906.229181	31.342106
534.231895	26939.106309	31.347124
534.733088	26988.186294	31.352141
535.284528	27025.705329	31.357159
535.984269	27061.071450	31.362176
536.385475	27113.624435	31.367194
536.917934	27137.254876	31.372212
537.494023	27180.351088	31.377229
537.862509	27216.059779	31.382247
538.665763	27259.360963	31.387264
538.933736	27295.515216	31.392282
539.982744	27330.353419	31.397300
540.374549	27369.794018	31.402317
540.848875	27412.634795	31.407335
541.297552	27445.487282	31.412352
541.403439	27486.508447	31.417370
541.698755	27528.846432	31.422388
542.360890	27585.683114	31.427405
542.974642	27641.137010	31.432423
543.543053	27674.982484	31.437440
543.836564	27726.296070	31.442458
544.669116	27763.772709	31.447476
545.188532	27828.753984	31.452493
545.479517	27871.194482	31.457511
546.063255	27905.903853	31.462528
546.658014	27962.082110	31.467546
547.795731	28005.181129	31.472564
548.159246	28048.944324	31.477581
548.808816	28086.595416	31.482599
549.290925	28130.845964	31.487616
549.792606	28174.745933	31.492634
550.620994	28204.531973	31.497652
550.921810	28252.830860	31.502669
551.422292	28296.137147	31.507687
552.156815	28335.785410	31.512704
552.472471	28383.772590	31.517722
553.117783	28417.752702	31.522740
553.414414	28452.570907	31.527757
553.692825	28495.109471	31.532775
554.634578	28535.022930	31.537792
555.140587	28570.080527	31.542810
555.911732	28617.099818	31.547828
556.381371	28647.106690	31.552845
556.878039	28697.215452	31.557863
557.416015	28730.934687	31.562880
557.976885	28776.950488	31.567898
558.557295	28811.750411	31.572916
559.596196	28858.450464	31.577933
559.425597	28898.228084	31.582951
560.506673	28918.241900	31.587968
561.150269	28957.640057	31.592986
562.124938	28992.878252	31.598004
562.689459	29029.905929	31.603021
563.096727	29070.238643	31.608039
563.693343	29091.092864	31.613056
563.781326	29136.873373	31.618074
564.113145	29181.509882	31.623092
564.610914	29227.315292	31.628109
565.436129	29275.794117	31.633127
565.981316	29309.930361	31.638144
566.711402	29357.924841	31.643162
566.992978	29394.820241	31.648180
567.514650	29441.488371	31.653197
568.028348	29478.815534	31.658215
569.459512	29514.413387	31.663232
570.073246	29556.371000	31.668250
570.628678	29593.192521	31.673268
571.071387	29634.481613	31.678285
571.800417	29674.127008	31.683303
572.238192	29708.786317	31.688320
572.411720	29752.171870	31.693338
573.381396	29794.940537	31.698356
573.811458	29827.243509	31.703373
574.388379	29868.050743	31.708391
575.251229	29909.079030	31.713408
575.328588	29946.329587	31.718426
575.620372	29982.984256	31.723444
576.199667	30029.771174	31.728461
576.760657	30072.660931	31.733479
577.523118	30121.366442	31.738496
578.067154	30172.881047	31.743514
578.630999	30208.570880	31.748532
579.332415	30257.633879	31.753549
579.693966	30321.098962	31.758567
580.556403	30354.643936	31.763584
581.006477	30398.828519	31.768602
581.793909	30443.927825	31.773620
582.509469	30485.087652	31.778637
582.774350	30520.913065	31.783655
583.549118	30571.204355	31.788672
584.182453	30607.490902	31.793690
584.681870	30651.396531	31.798708
585.607981	30704.471232	31.803725
585.941617	30748.769511	31.808743
586.522112	30791.935867	31.813760
586.916544	30837.470172	31.818778
587.804457	30869.216761	31.823796
588.716836	30910.131873	31.828813
589.113976	30954.547134	31.833831
589.825429	30988.116645	31.838848
590.048575	31020.618056	31.843866
590.962896	31069.030348	31.848884
591.458256	31108.866599	31.853901
591.981399	31140.942213	31.858919
592.676663	31178.617159	31.863936
592.797475	31204.434069	31.868954
593.470268	31250.185128	31.873972
594.009325	31289.243706	31.878989
594.192649	31335.804443	31.884007
594.859278	31364.526645	31.889024
595.694261	31410.246488	31.894042
596.054607	31453.897326	31.899060
597.025610	31503.047750	31.904077
597.053772	31551.681303	31.909095
597.671885	31587.207034	31.914112
598.320524	31639.714142	31.919130
598.606123	31691.386554	31.924148
599.863655	31743.729599	31.929165
599.787802	31795.243603	31.934183
600.444371	31840.909991	31.939200
600.845931	31894.758465	31.944218
601.785705	31942.321735	31.949236
602.414440	31996.508087	31.954253
602.568840	32056.774037	31.959271
603.033530	32110.423591	31.964288
603.437230	32157.217374	31.969306
604.083804	32215.826734	31.974324
605.634175	32284.960388	31.979341
605.774802	32351.342490	31.984359
606.396682	32392.685063	31.989376
607.455330	32454.448744	31.994394
607.861274	32501.919388	31.999412
608.649379	32568.624950	32.004429
609.095752	32620.995334	32.009447
609.993248	32670.874338	32.014464
610.647504	32731.102355	32.019482
611.200751	32775.541463	32.024500
611.825820	32824.906917	32.029517
612.394034	32883.151036	32.034535
612.867904	32930.283338	32.039552
613.580379	32993.720932	32.044570
614.201147	33054.062569	32.049588
615.063694	33104.858420	32.054605
615.518741	33153.631560	32.059623
616.149363	33194.708837	32.064640
617.069829	33239.022223	32.069658
617.899090	33296.386023	32.074676
618.834147	33338.762794	32.079693
619.596380	33373.478878	32.084711
620.235745	33420.251451	32.089728
620.529838	33459.080387	32.094746
620.687588	33503.462490	32.099764
622.144487	33543.280161	32.104781
622.490754	33599.329107	32.109799
623.089928	33644.818716	32.114816
623.738743	33683.434792	32.119834
624.476925	33722.985359	32.124852
625.156788	33765.763088	32.129869
625.756920	33817.714233	32.134887
626.299732	33851.384166	32.139904
627.050252	33896.079447	32.144922
627.495701	33938.596874	32.149940
628.094141	33976.152868	32.154957
628.838338	34023.005302	32.159975
629.649605	34063.506123	32.164992
630.021114	34113.053179	32.170010
630.390142	34152.984462	32.175028
631.330780	34194.401102	32.180045
631.693210	34241.958335	32.185063
632.250729	34278.623465	32.190080
632.856934	34321.906939	32.195098
633.707161	34370.071344	32.200116
634.195447	34398.344990	32.205133
635.097075	34442.562698	32.210151
636.086944	34464.037617	32.215168
637.311409	34490.394894	32.220186
637.925385	34516.025322	32.225204
638.289083	34546.493485	32.230221
638.526200	34583.335473	32.235239
639.347193	34616.261535	32.240256
640.049431	34643.345193	32.245274
640.218560	34677.871256	32.250292
640.926674	34714.007903	32.255309
641.603493	34754.202216	32.260327
642.177582	34782.659021	32.265344
642.652216	34823.270615	32.270362
642.984958	34862.494447	32.275380
643.774422	34913.489412	32.280397
644.270191	34962.013834	32.285415
644.994921	35004.616392	32.290432
645.378640	35056.180672	32.295450
646.009071	35104.488458	32.300468
646.705676	35144.174625	32.305485
647.164242	35199.793057	32.310503
648.198045	35246.312291	32.315520
648.590595	35307.675941	32.320538
648.896821	35350.420218	32.325556
650.040807	35399.597137	32.330573
650.044212	35459.390546	32.335591
650.437796	35506.471575	32.340608
651.355470	35573.432071	32.345626
652.092424	35634.743054	32.350644
652.824230	35703.781477	32.355661
653.448432	35759.666444	32.360679
654.242557	35815.367036	32.365696
654.782831	35872.719618	32.370714
655.208630	35930.014302	32.375732
655.959166	35987.992042	32.380749
656.700450	36053.116261	32.385767
657.444747	36119.726097	32.390784
658.286167	36169.862409	32.395802
658.853860	36233.515668	32.400820
659.481391	36278.924346	32.405837
660.306566	36336.265444	32.410855
661.583146	36381.364645	32.415872
662.463468	36436.079706	32.420890
662.984125	36489.826565	32.425908
664.321178	36521.024950	32.430925
664.935899	36562.281989	32.435943
665.386496	36600.479002	32.440960
665.880628	36639.529244	32.445978
666.677485	36688.371163	32.450996
667.228178	36728.177857	32.456013
667.947588	36782.242286	32.461031
668.763019	36810.038258	32.466048
669.681421	36858.570783	32.471066
669.733116	36906.283542	32.476084
670.799447	36945.042929	32.481101
671.168703	36985.112305	32.486119
671.588765	37036.802201	32.491136
672.480052	37083.619550	32.496154
672.664578	37135.023866	32.501172
673.668529	37182.342398	32.506189
674.257669	37245.015239	32.511207
674.948038	37290.308797	32.516224
675.255904	37345.090014	32.521242
676.169535	37400.656011	32.526260
676.567392	37451.313345	32.531277
677.007610	37506.036430	32.536295
677.780601	37549.521849	32.541312
678.393073	37606.305081	32.546330
678.890003	37662.347645	32.551348
679.328143	37707.940611	32.556365
679.964008	37772.207540	32.561383
680.677120	37829.962151	32.566400
681.416623	37885.765187	32.571418
682.089382	37945.100928	32.576436
682.614685	37997.605135	32.581453
683.438719	38056.576167	32.586471
684.250351	38111.622390	32.591488
685.336668	38163.976436	32.596506
685.518362	38222.358652	32.601524
686.566233	38275.699105	32.606541
686.888227	38332.934187	32.611559
687.946998	38400.735281	32.616576
688.905697	38446.286722	32.621594
689.641808	38498.645512	32.626612
690.398178	38557.249035	32.631629
690.846840	38612.523784	32.636647
691.914888	38643.583769	32.641664
693.316135	38679.562342	32.646682
693.859090	38728.998604	32.651700
695.107340	38769.231695	32.656717
695.154438	38819.510523	32.661735
695.877576	38855.613923	32.666752
696.639970	38898.572534	32.671770
697.211819	38940.428940	32.676788
697.918094	38995.044840	32.681805
698.395984	39050.455286	32.686823
698.939127	39101.903339	32.691840
699.538976	39145.039515	32.696858
699.971056	39201.779158	32.701876
700.745721	39258.408705	32.706893
701.470067	39312.516687	32.711911
701.901720	39382.132262	32.716928
702.620929	39435.583668	32.721946
702.979730	39505.059205	32.726964
703.933833	39560.599192	32.731981
704.850218	39625.953648	32.736999
705.281231	39688.285110	32.742016
706.157182	39748.726179	32.747034
706.731525	39816.752588	32.752052
707.693073	39878.249452	32.757069
708.331217	39937.083818	32.762087
709.018384	40003.404729	32.767104
710.252918	40063.550541	32.772122
710.611484	40122.802053	32.777140
711.680180	40169.307598	32.782157
712.219115	40239.332940	32.787175
712.971719	40291.497461	32.792192
713.797995	40346.901259	32.797210
714.134863	40412.025764	32.802228
714.710607	40459.070333	32.807245
715.515844	40523.104064	32.812263
716.124208	40588.787635	32.817280
716.862517	40651.554667	32.822298
717.556067	40722.980454	32.827316
718.345592	40777.923076	32.832333
719.083700	40841.968195	32.837351
719.286990	40906.356054	32.842368
720.220115	40971.844765	32.847386
721.264515	41041.528379	32.852404
721.819147	41092.871849	32.857421
723.007090	41158.207614	32.862439
723.538176	41221.476551	32.867456
724.313840	41270.085503	32.872474
725.353203	41340.877634	32.877492
726.122997	41392.017553	32.882509
726.863473	41441.524115	32.887527
727.547810	41491.336780	32.892544
728.371241	41530.464781	32.897562
729.100624	41587.158043	32.902580
729.854020	41618.783570	32.907597
730.832554	41670.144628	32.912615
731.051499	41721.914981	32.917632
732.010201	41762.540236	32.922650
733.176249	41806.580190	32.927668
734.007394	41849.850169	32.932685
734.818202	41884.249968	32.937703
735.020068	41937.364306	32.942720
736.118599	41981.326578	32.947738
736.577632	42030.460859	32.952756
737.542832	42079.598676	32.957773
738.309240	42123.024740	32.962791
738.621252	42173.383916	32.967808
739.602470	42212.817461	32.972826
740.128925	42270.214499	32.977844
740.569009	42318.865372	32.982861
741.449777	42379.230764	32.987879
741.861809	42444.090304	32.992896
743.022965	42497.606920	32.997914
743.635023	42559.089849	33.002932
744.266185	42616.047729	33.007949
745.032749	42675.520938	33.012967
745.419715	42738.399248	33.017984
746.055265	42795.818624	33.023002
746.696965	42868.189235	33.028020
747.857493	42917.874088	33.033037
748.677208	42988.642482	33.038055
749.309184	43052.375362	33.043072
750.692680	43106.257320	33.048090
751.035427	43169.422040	33.053108
751.699751	43228.760859	33.058125
752.522173	43286.424397	33.063143
752.769920	43350.799852	33.068160
753.980279	43405.379947	33.073178
754.689014	43473.320899	33.078196
755.177050	43534.699353	33.083213
756.091521	43595.379084	33.088231
757.105824	43662.368561	33.093248
757.761653	43737.453297	33.098266
758.549791	43810.531590	33.103284
759.031225	43873.550228	33.108301
759.912679	43948.809288	33.113319
760.535539	44025.917873	33.118336
761.104527	44078.183234	33.123354
761.867990	44162.879671	33.128372
762.639226	44223.026795	33.133389
763.660048	44287.347879	33.138407
764.138272	44356.383745	33.143424
765.036419	44425.341807	33.148442
765.985215	44495.139797	33.153460
767.027586	44563.601435	33.158477
767.643603	44630.845598	33.163495
768.389451	44695.470009	33.168512
769.278560	44758.516249	33.173530
769.920356	44819.703532	33.178548
770.856315	44885.614594	33.183565
771.600364	44951.290054	33.188583
772.558320	45019.570146	33.193600
773.044114	45081.668003	33.198618
774.431055	45146.820152	33.203636
775.234624	45199.051629	33.208653
776.434758	45246.477319	33.213671
777.023929	45305.681573	33.218688
778.450778	45346.006503	33.223706
778.975665	45377.154291	33.228724
779.525875	45428.894395	33.233741
780.494251	45464.831347	33.238759
780.911034	45515.649903	33.243776
781.335955	45564.784682	33.248794
782.003984	45612.211748	33.253812
782.296744	45662.607146	33.258829
783.400175	45714.274444	33.263847
783.976016	45778.726034	33.268864
784.830031	45832.285866	33.273882
785.806180	45893.069801	33.278900
786.076943	45954.855639	33.283917
786.813879	46016.853740	33.288935
787.380200	46094.787977	33.293952
788.293355	46156.271944	33.298970
789.418022	46219.184425	33.303988
790.210870	46293.415099	33.309005
791.098702	46351.070068	33.314023
791.833798	46427.948069	33.319040
792.421372	46487.010196	33.324058
793.263999	46555.698808	33.329076
793.861485	46624.988800	33.334093
794.476521	46683.218467	33.339111
795.329858	46757.542472	33.344128
796.400108	46828.518124	33.349146
796.750890	46901.111593	33.354164
797.700026	46973.131371	33.359181
798.527675	47050.364000	33.364199
799.280407	47133.232459	33.369216
800.555779	47205.600740	33.374234
801.090702	47279.033438	33.379252
801.475900	47350.199610	33.384269
802.682778	47421.813781	33.389287
803.081934	47501.980416	33.394304
804.178004	47583.209201	33.399322
804.961552	47653.422319	33.404340
805.528237	47725.162412	33.409357
806.973298	47799.884858	33.414375
807.852282	47872.392894	33.419392
808.922378	47939.955856	33.424410
809.879329	48009.776159	33.429428
810.592108	48073.498113	33.434445
811.407751	48139.235002	33.439463
812.252168	48210.098313	33.444480
813.261573	48282.346954	33.449498
814.169898	48343.875591	33.454516
814.816880	48400.156160	33.459533
815.962342	48467.727942	33.464551
816.249070	48547.896792	33.469568
817.267357	48611.439841	33.474586
818.300656	48671.583384	33.479604
819.017232	48746.232552	33.484621
819.992195	48795.155879	33.489639
820.285275	48880.234323	33.494656
821.020455	48947.308329	33.499674
821.696414	49009.640456	33.504692
822.443748	49099.204173	33.509709
823.529904	49167.869121	33.514727
824.007667	49249.737878	33.519744
825.064743	49322.925076	33.524762
825.919046	49389.165691	33.529780
826.455080	49467.824833	33.534797
827.668039	49536.616666	33.539815
828.303506	49615.165935	33.544832
829.432219	49687.640875	33.549850
830.401133	49748.341385	33.554868
831.131068	49813.109455	33.559885
832.210012	49863.246294	33.564903
833.380475	49926.959122	33.569920
833.459116	49985.514842	33.574938
835.097223	50029.579763	33.579956
835.787822	50086.775101	33.584973
836.803033	50137.795576	33.589991
837.668730	50187.795493	33.595008
838.082571	50247.767555	33.600026
838.903747	50293.238199	33.605044
839.407602	50363.357677	33.610061
840.448934	50424.421996	33.615079
841.142186	50485.363505	33.620096
841.866378	50557.410655	33.625114
842.666065	50616.273324	33.630132
843.182114	50683.917997	33.635149
843.943957	50754.087084	33.640167
845.139100	50819.671370	33.645184
846.212237	50889.311551	33.650202
846.496999	50958.062318	33.655220
847.335591	51031.023233	33.660237
848.318853	51110.864833	33.665255
849.250745	51191.714407	33.670272
849.713418	51267.411001	33.675290
850.375638	51339.830893	33.680308
851.166464	51425.075382	33.685325
852.169744	51506.136397	33.690343
853.225841	51587.613406	33.695360
853.478287	51678.947273	33.700378
854.766721	51753.839888	33.705396
855.743902	51838.626627	33.710413
856.994784	51915.670599	33.715431
857.757061	52003.117272	33.720448
858.385128	52087.231608	33.725466
859.379132	52163.310321	33.730484
860.308946	52246.283606	33.735501
861.368858	52324.086324	33.740519
862.355920	52400.344065	33.745536
863.212551	52474.293812	33.750554
864.162642	52540.794326	33.755572
864.822385	52629.436246	33.760589
865.729184	52701.392034	33.765607
866.554884	52775.841109	33.770624
867.543830	52859.977992	33.775642
868.507132	52932.729313	33.780660
868.962204	53015.570424	33.785677
869.679663	53090.999166	33.790695
870.903369	53179.220014	33.795712
872.022456	53260.731044	33.800730
873.189538	53340.722541	33.805748
873.666409	53416.056899	33.810765
874.817711	53487.698624	33.815783
875.396235	53562.821467	33.820800
876.275926	53634.569200	33.825818
877.080137	53710.872340	33.830836
878.001802	53809.033098	33.835853
878.910984	53884.510487	33.840871
879.889858	53958.869874	33.845888
880.502545	54044.702202	33.850906
882.026268	54118.692522	33.855924
882.759399	54198.090053	33.860941
883.590637	54271.492566	33.865959
884.515737	54343.956797	33.870976
885.356690	54421.990419	33.875994
886.229403	54495.336549	33.881012
887.044920	54571.014236	33.886029
888.155185	54652.759287	33.891047
888.817257	54735.631194	33.896064
889.223037	54806.380482	33.901082
890.533717	54877.210611	33.906100
891.116878	54954.324233	33.911117
892.250439	55032.466204	33.916135
893.220385	55097.768509	33.921152
893.752313	55169.157387	33.926170
894.721180	55238.782477	33.931188
895.387352	55318.225840	33.936205
896.248455	55378.388268	33.941223
897.045263	55447.344635	33.946240
897.936642	55531.993552	33.951258
899.099463	55602.798244	33.956276
899.614502	55697.264748	33.961293
900.695750	55766.342306	33.966311
901.437636	55861.014630	33.971328
902.311013	55940.915118	33.976346
903.772507	56018.623257	33.981364
904.927072	56092.272202	33.986381
905.842227	56174.964190	33.991399
906.401041	56237.745249	33.996416
907.215675	56328.680576	34.001434
908.403483	56400.300146	34.006452
909.188894	56496.449121	34.011469
910.363336	56555.749360	34.016487
911.198523	56639.967961	34.021504
912.033907	56729.813053	34.026522
912.972727	56803.466137	34.031540
913.592757	56892.877038	34.036557
914.213976	56978.193368	34.041575
915.256621	57061.090089	34.046592
916.043405	57160.994502	34.051610
917.047450	57232.645175	34.056628
918.035941	57324.677434	34.061645
919.021834	57411.609364	34.066663
920.204028	57498.042712	34.071680
920.807793	57601.565945	34.076698
921.850166	57673.914483	34.081716
922.986961	57758.419174	34.086733
924.048268	57846.606737	34.091751
924.694725	57933.916174	34.096768
925.624752	58022.707088	34.101786
926.713185	58112.505312	34.106804
927.527426	58201.403516	34.111821
928.495234	58288.961686	34.116839
929.571132	58375.516001	34.121856
930.472723	58460.673697	34.126874
931.782485	58544.654220	34.131892
932.509431	58643.694348	34.136909
933.847077	58717.462108	34.141927
934.522301	58807.865226	34.146944
935.616922	58888.399342	34.151962
936.476220	58970.584328	34.156980
937.550407	59051.634841	34.161997
938.375381	59139.351242	34.167015
939.903318	59193.830646	34.172032
940.562627	59284.326631	34.177050
941.796623	59355.909848	34.182068
943.167904	59435.984980	34.187085
944.207931	59495.237444	34.192103
945.033905	59562.112388	34.197120
945.632199	59646.682193	34.202138
946.733546	59710.027137	34.207156
947.807487	59795.555128	34.212173
948.631336	59856.405514	34.217191
949.434214	59930.855189	34.222208
950.117168	60007.634053	34.227226
951.062109	60086.182640	34.232244
952.010050	60167.332484	34.237261
952.765824	60241.094182	34.242279
953.721883	60314.185632	34.247296
954.297098	60393.856143	34.252314
955.179334	60465.130261	34.257332
955.769965	60550.489275	34.262349
956.418896	60626.205659	34.267367
957.699899	60702.779680	34.272384
958.087837	60788.481233	34.277402
959.941065	60852.908438	34.282420
960.786239	60939.514133	34.287437
961.428363	61016.853217	34.292455
962.523566	61099.116271	34.297472
963.323386	61191.831897	34.302490
964.588838	61261.801698	34.307508
965.302235	61349.973849	34.312525
966.610819	61442.383350	34.317543
968.099655	61526.979284	34.322560
968.711188	61611.427221	34.327578
969.511443	61699.890947	34.332596
970.459689	61788.781385	34.337613
971.433621	61878.718935	34.342631
972.474227	61957.315601	34.347648
973.169551	62053.772824	34.352666
974.448872	62127.927126	34.357684
975.564815	62222.990213	34.362701
975.984303	62307.533729	34.367719
977.254213	62393.242844	34.372736
977.892246	62498.212160	34.377754
978.891636	62594.016460	34.382772
980.327252	62671.838595	34.387789
981.010656	62763.413484	34.392807
982.205603	62850.908333	34.397824
982.740339	62949.426071	34.402842
984.014613	63048.841940	34.407860
985.342900	63140.343158	34.412877
986.575039	63229.979552	34.417895
987.859252	63303.984689	34.422912
988.762167	63396.945759	34.427930
989.888605	63475.489570	34.432948
990.908807	63552.999307	34.437965
992.082470	63633.353114	34.442983
993.432356	63706.260380	34.448000
994.442678	63795.407907	34.453018
995.485293	63871.104611	34.458036
996.592486	63949.551625	34.463053
997.440453	64026.184370	34.468071
997.930072	64104.183570	34.473088
998.956403	64193.152768	34.478106
999.749754	64268.623590	34.483124
1000.530131	64351.142707	34.488141
1001.507138	64452.003198	34.493159
1002.066196	64535.506980	34.498176
1003.108215	64627.089870	34.503194
1004.088118	64726.482280	34.508212
1005.084402	64824.486088	34.513229
1005.879978	64928.643431	34.518247
1007.314762	65022.717951	34.523264
1008.162271	65124.854812	34.528282
1009.129119	65229.360262	34.533300
1010.121739	65317.990497	34.538317
1011.836633	65407.464590	34.543335
1013.258480	65485.829447	34.548352
1014.458596	65566.406924	34.553370
1015.657525	65645.079209	34.558388
1016.751205	65713.841073	34.563405
1017.344216	65794.842993	34.568423
1018.830798	65875.300893	34.573440
1019.881702	65951.021574	34.578458
1020.791154	66032.513142	34.583476
1021.557513	66102.428627	34.588493
1022.832532	66169.517413	34.593511
1023.790388	66241.885282	34.598528
1024.811628	66309.957287	34.603546
1025.224633	66380.200782	34.608564
1026.498871	66446.752274	34.613581
1026.885403	66527.839330	34.618599
1027.991754	66603.616644	34.623616
1028.481320	66685.327620	34.628634
1029.248122	66783.640667	34.633652
1030.313003	66880.939004	34.638669
1031.173891	66969.424586	34.643687
1032.114684	67061.823480	34.648704
1032.911740	67154.662955	34.653722
1034.141815	67252.063624	34.658740
1035.169798	67355.321042	34.663757
1035.723237	67470.897791	34.668775
1036.827316	67561.639562	34.673792
1038.155266	67674.336144	34.678810
1039.222888	67773.562240	34.683828
1040.545732	67876.737879	34.688845
1041.083550	67990.071699	34.693863
1042.482332	68084.498760	34.698880
1043.462146	68193.085614	34.703898
1044.441910	68305.649224	34.708916
1045.752192	68394.487676	34.713933
1046.741659	68507.867449	34.718951
1047.827975	68605.903494	34.723968
1049.259124	68711.762955	34.728986
1049.980418	68814.459809	34.734004
1051.388132	68922.096686	34.739021
1052.204601	69027.419943	34.744039
1053.564653	69119.108814	34.749056
1054.855253	69220.794216	34.754074
1055.968189	69316.827944	34.759092
1057.132039	69416.336671	34.764109
1058.195943	69520.211400	34.769127
1059.577783	69613.108040	34.774144
1060.485093	69717.755111	34.779162
1061.700239	69815.725042	34.784180
1062.618817	69903.445575	34.789197
1063.310030	70013.547721	34.794215
1064.297370	70107.735966	34.799232
1065.709858	70208.621095	34.804250
1066.650545	70314.050560	34.809268
1067.907566	70412.161864	34.814285
1068.723057	70520.879062	34.819303
1069.945543	70627.057457	34.824320
1071.018442	70728.991624	34.829338
1071.828021	70830.219969	34.834356
1073.220513	70922.644713	34.839373
1074.034014	71030.230860	34.844391
1075.070320	71123.306998	34.849408
1076.312595	71235.120584	34.854426
1077.650509	71329.746270	34.859444
1079.982860	71413.085099	34.864461
1080.726785	71501.712072	34.869479
1082.175509	71578.083965	34.874496
1083.546068	71653.062436	34.879514
1084.573041	71736.542163	34.884532
1086.092186	71810.535416	34.889549
1087.013710	71887.015601	34.894567
1088.589980	71950.817635	34.899584
1089.287335	72032.931120	34.904602
1090.123195	72106.689607	34.909620
1091.320294	72174.946026	34.914637
1091.906198	72268.501625	34.919655
1092.506911	72339.751649	34.924672
1093.432035	72419.842434	34.929690
1094.283616	72514.206128	34.934708
1095.457300	72582.923203	34.939725
1095.927068	72681.817820	34.944743
1096.751221	72765.725011	34.949760
1097.566711	72848.481253	34.954778
1098.371422	72956.671933	34.959796
1099.364597	73045.151312	34.964813
1100.329923	73147.643567	34.969831
1101.603939	73254.343856	34.974848
1102.379275	73364.149321	34.979866
1103.422804	73470.177071	34.984884
1104.756803	73580.327108	34.989901
1106.088366	73696.658964	34.994919
1107.718139	73796.061134	34.999936
1109.410300	73888.930955	35.004954
1109.769618	73992.141433	35.009972
1111.458469	74080.921293	35.014989
1112.425972	74192.942171	35.020007
1113.237071	74291.067675	35.025024
1114.701801	74390.953741	35.030042
1115.507709	74506.788306	35.035060
1116.725667	74604.154981	35.040077
1117.627954	74709.956321	35.045095
1119.241515	74807.591486	35.050112
1120.472590	74904.995214	35.055130
1121.543564	75010.505487	35.060148
1122.594366	75104.353361	35.065165
1124.317228	75213.474280	35.070183
1125.405589	75300.590996	35.075200
1126.302531	75406.851918	35.080218
1127.686400	75509.592095	35.085236
1128.928088	75600.929298	35.090253
1129.866191	75704.436281	35.095271
1131.113658	75805.311452	35.100288
1132.196012	75901.082570	35.105306
1133.087878	76005.953275	35.110324
1134.559939	76094.925558	35.115341
1135.335694	76205.033947	35.120359
1136.361182	76310.543726	35.125376
1137.849944	76411.738284	35.130394
1138.961896	76517.184741	35.135412
1140.191401	76617.559048	35.140429
1140.823750	76719.154073	35.145447
1142.488093	76829.557377	35.150464
1143.848207	76927.163669	35.155482
1144.871604	77024.050006	35.160500
1146.036174	77124.094271	35.165517
1147.404465	77228.186163	35.170535
1148.237871	77334.464542	35.175552
1149.469098	77435.817013	35.180570
1150.346178	77555.808582	35.185588
1151.300481	77651.213109	35.190605
1152.750646	77768.785535	35.195623
1153.513914	77873.924155	35.200640
1154.449483	77970.282804	35.205658
1155.547168	78093.713414	35.210676
1156.847010	78211.007106	35.215693
1157.763067	78323.205115	35.220711
1159.115105	78437.615991	35.225728
1160.059121	78545.516048	35.230746
1161.406986	78664.007683	35.235764
1162.492642	78782.768671	35.240781
1163.977295	78884.429100	35.245799
1164.969116	79012.440930	35.250816
1166.462061	79112.606036	35.255834
1167.415831	79223.864380	35.260852
1168.466110	79331.750977	35.265869
1169.665486	79439.880828	35.270887
1170.818024	79544.091104	35.275904
1172.451737	79643.615461	35.280922
1173.459792	79742.692806	35.285940
1175.044104	79832.698624	35.290957
1175.517651	79924.891976	35.295975
1176.291548	80022.727215	35.300992
1177.713672	80130.115632	35.306010
1178.716388	80224.875421	35.311028
1179.984800	80330.958297	35.316045
1181.320609	80445.037947	35.321063
1182.374309	80554.411051	35.326080
1184.063324	80659.644225	35.331098
1185.204002	80762.809379	35.336116
1186.372217	80867.680980	35.341133
1187.409635	80974.410386	35.346151
1188.232425	81082.073133	35.351168
1189.751378	81188.221628	35.356186
1190.485509	81304.210170	35.361204
1191.743310	81410.602870	35.366221
1193.030379	81524.707186	35.371239
1194.619465	81635.597551	35.376256
1196.112779	81737.647161	35.381274
1196.961694	81857.649080	35.386292
1198.142147	81967.007974	35.391309
1199.371710	82084.823091	35.396327
1200.410499	82201.857522	35.401344
1201.783032	82312.885625	35.406362
1203.688433	82414.062671	35.411380
1205.386307	82512.713040	35.416397
1206.577892	82608.946557	35.421415
1207.906740	82712.811780	35.426432
1209.460673	82807.380469	35.431450
1210.858371	82917.241378	35.436468
1211.865462	82995.437231	35.441485
1213.019252	83094.224999	35.446503
1213.644124	83208.274487	35.451520
1214.932057	83304.178613	35.456538
1215.606968	83414.077927	35.461556
1216.820282	83526.770059	35.466573
1218.059069	83634.555182	35.471591
1219.351779	83751.075011	35.476608
1220.242115	83859.422044	35.481626
1221.414447	83973.275347	35.486644
1223.091060	84084.655847	35.491661
1224.682803	84190.740941	35.496679
1226.019173	84293.153630	35.501696
1227.956519	84395.878611	35.506714
1228.979165	84492.613621	35.511732
1230.399096	84587.551201	35.516749
1231.830853	84684.235851	35.521767
1232.841349	84788.107514	35.526784
1233.968589	84875.729739	35.531802
1235.131185	84975.244900	35.536820
1236.397075	85071.652566	35.541837
1237.490883	85166.820220	35.546855
1238.845160	85274.466832	35.551872
1239.717321	85377.627224	35.556890
1240.967760	85481.337330	35.561908
1241.930983	85592.961441	35.566925
1243.083984	85693.697030	35.571943
1243.979778	85802.113902	35.576960
1245.159934	85918.685395	35.581978
1246.633709	86040.825163	35.586996
1247.729299	86148.895446	35.592013
1248.492807	86252.202586	35.597031
1249.612136	86381.216317	35.602048
1251.180691	86493.687386	35.607066
1252.414560	86613.915455	35.612084
1253.232428	86718.242208	35.617101
1254.513592	86828.224929	35.622119
1255.441874	86950.934963	35.627136
1257.141424	87051.463474	35.632154
1258.522970	87168.528186	35.637172
1258.891397	87291.580235	35.642189
1260.424923	87398.117023	35.647207
1261.599700	87517.052779	35.652224
1263.264229	87629.652685	35.657242
1264.170119	87749.480279	35.662260
1265.330383	87871.245658	35.667277
1266.847351	87986.049550	35.672295
1268.009116	88111.300606	35.677312
1269.347183	88235.891128	35.682330
1270.558110	88366.964983	35.687348
1272.151955	88480.833742	35.692365
1273.559641	88607.797456	35.697383
1274.768348	88739.925148	35.702400
1276.295228	88856.999314	35.707418
1277.609670	88971.306311	35.712436
1278.788602	89099.359588	35.717453
1280.214598	89216.476224	35.722471
1281.389204	89346.330800	35.727488
1282.348249	89471.036215	35.732506
1283.789957	89599.811134	35.737524
1285.297835	89729.222643	35.742541
1286.821764	89852.371645	35.747559
1287.828353	89986.171191	35.752576
1288.820826	90109.061797	35.757594
1290.132417	90241.294213	35.762612
1291.544726	90379.506076	35.767629
1293.304505	90495.764691	35.772647
1294.358329	90633.273115	35.777664
1295.846493	90756.241307	35.782682
1297.126215	90876.580981	35.787700
1298.361555	91000.932935	35.792717
1300.162481	91125.818385	35.797735
1301.273987	91266.375105	35.802752
1302.822847	91395.001661	35.807770
1304.044283	91517.976465	35.812788
1305.231016	91638.080179	35.817805
1306.991293	91756.612238	35.822823
1307.732008	91888.788673	35.827840
1309.355382	92010.929803	35.832858
1310.848379	92131.355357	35.837876
1311.890087	92258.011308	35.842893
1313.888741	92382.313514	35.847911
1315.193500	92503.606349	35.852928
1316.321205	92619.692705	35.857946
1317.606070	92739.494000	35.862964
1318.604439	92869.847506	35.867981
1320.009402	92978.857737	35.872999
1321.096901	93113.875316	35.878016
1322.718604	93235.286502	35.883034
1324.162841	93359.628296	35.888052
1325.251680	93495.458532	35.893069
1326.903477	93614.420313	35.898087
1327.581738	93745.144245	35.903104
1329.349127	93870.096906	35.908122
1330.313010	93992.513400	35.913140
1331.610585	94129.695523	35.918157
1333.071524	94261.225102	35.923175
1333.941331	94394.089413	35.928192
1335.625135	94515.470648	35.933210
1336.960215	94646.146873	35.938228
1338.029977	94786.713635	35.943245
1339.625968	94905.613042	35.948263
1340.884380	95043.350360	35.953280
1342.454124	95154.535503	35.958298
1344.047705	95269.291818	35.963316
1344.806083	95387.537568	35.968333
1346.037469	95496.761195	35.973351
1347.168160	95622.745364	35.978368
1349.102822	95738.046076	35.983386
1350.678887	95841.031539	35.988404
1351.780587	95958.769696	35.993421
1353.330049	96071.102092	35.998439
1354.574740	96197.299004	36.003456
1355.783877	96311.979566	36.008474
1357.212617	96439.416397	36.013492
1358.269177	96554.970887	36.018509
1359.585779	96684.188131	36.023527
1360.715697	96808.009594	36.028544
1362.500991	96949.425443	36.033562
1363.759374	97080.212544	36.038580
1364.840452	97204.055844	36.043597
1366.457415	97336.131880	36.048615
1367.749844	97468.182923	36.053632
1368.998194	97602.320311	36.058650
1370.382123	97739.086548	36.063668
1371.679080	97872.469605	36.068685
1373.294988	98011.508039	36.073703
1374.511062	98155.172905	36.078720
1376.117406	98287.989812	36.083738
1377.150363	98422.126164	36.088756
1378.760930	98570.219071	36.093773
1379.935145	98705.982617	36.098791
1381.490817	98847.683546	36.103808
1382.726730	98987.938992	36.108826
1384.359484	99126.193701	36.113844
1385.423552	99270.952124	36.118861
1387.193241	99412.622246	36.123879
1388.368656	99555.133445	36.128896
1390.428181	99701.805254	36.133914
1392.361201	99826.438917	36.138932
1393.839679	99947.518089	36.143949
1395.514044	100073.777638	36.148967
1397.143664	100203.454879	36.153984
1398.477108	100324.507332	36.159002
1400.023798	100459.079344	36.164020
1400.687252	100581.225890	36.169037
1402.118875	100704.445031	36.174055
1403.852282	100837.620369	36.179072
1405.189945	100970.997306	36.184090
1406.300031	101101.887330	36.189108
1407.706167	101243.444586	36.194125
1409.162786	101362.415254	36.199143
1410.513741	101513.199105	36.204160
1411.752760	101645.478499	36.209178
1413.073037	101782.309884	36.214196
1414.061165	101929.019079	36.219213
1415.816171	102063.134247	36.224231
1416.891761	102209.755018	36.229248
1418.143809	102351.366413	36.234266
1419.754475	102507.718222	36.239284
1420.997192	102645.642940	36.244301
1422.442177	102787.657249	36.249319
1423.814311	102953.544462	36.254336
1425.061133	103099.673439	36.259354
1426.701326	103240.150562	36.264372
1428.365497	103387.382285	36.269389
1429.985089	103532.948009	36.274407
1431.351390	103672.290473	36.279424
1433.070621	103819.287326	36.284442
1434.637514	103963.544541	36.289460
1435.824834	104098.783330	36.294477
1437.452072	104217.560251	36.299495
1438.626785	104345.321395	36.304512
1439.540858	104476.787855	36.309530
1441.220203	104607.679270	36.314548
1442.432028	104742.650590	36.319565
1443.921749	104870.884560	36.324583
1445.214007	105010.814705	36.329600
1446.658607	105138.042376	36.334618
1448.078886	105275.608019	36.339636
1449.463572	105419.785758	36.344653
1450.960993	105556.414942	36.349671
1452.435485	105707.490262	36.354688
1453.666876	105841.372504	36.359706
1455.087749	105983.454884	36.364724
1456.614138	106134.156323	36.369741
1457.517573	106292.677375	36.374759
1459.085181	106444.958751	36.379776
1460.319430	106596.899619	36.384794
1462.120424	106752.734458	36.389812
1463.153037	106920.824372	36.394829
1464.876304	107076.267027	36.399847
1466.012745	107240.868017	36.404864
1467.900357	107409.626106	36.409882
1469.523548	107573.658408	36.414900
1471.290923	107731.874150	36.419917
1472.817447	107885.157405	36.424935
1474.324129	108042.831857	36.429952
1475.573043	108210.869066	36.434970
1477.730425	108360.556432	36.439988
1479.075539	108531.344586	36.445005
1480.719047	108677.334487	36.450023
1482.481476	108824.118060	36.455040
1484.041463	108979.569366	36.460058
1485.719561	109124.947092	36.465076
1487.361213	109282.948570	36.470093
1489.376213	109426.499797	36.475111
1490.847669	109564.873609	36.480128
1492.529256	109705.117418	36.485146
1494.283999	109845.096782	36.490164
1495.947660	109978.179667	36.495181
1497.174292	110119.142686	36.500199
1498.675621	110251.731948	36.505216
1499.991881	110399.555370	36.510234
1501.583069	110531.662495	36.515252
1503.360841	110667.963974	36.520269
1505.103566	110801.595655	36.525287
1506.639063	110940.066376	36.530304
1507.986913	111076.081267	36.535322
1509.336057	111201.342507	36.540340
1510.677082	111342.000938	36.545357
1511.994117	111483.272381	36.550375
1513.972542	111624.251219	36.555392
1515.254946	111762.891367	36.560410
1517.219002	111892.180914	36.565428
1518.489737	112037.405811	36.570445
1519.879326	112159.899489	36.575463
1521.412834	112304.742163	36.580480
1522.560952	112447.121687	36.585498
1524.394567	112588.443929	36.590516
1525.712688	112724.723389	36.595533
1526.888461	112869.573298	36.600551
1528.522049	113013.401369	36.605568
1529.692000	113166.915335	36.610586
1531.248464	113316.412912	36.615604
1532.464000	113455.475852	36.620621
1533.910718	113611.256823	36.625639
1535.656610	113769.274745	36.630656
1537.169473	113916.891903	36.635674
1538.587400	114052.349163	36.640692
1539.673823	114197.700241	36.645709
1540.889497	114331.427135	36.650727
1542.468773	114481.154255	36.655744
1543.708084	114636.147527	36.660762
1545.588785	114790.128464	36.665780
1547.053740	114938.936726	36.670797
1548.434482	115088.595774	36.675815
1549.566693	115243.303896	36.680832
1551.373706	115412.074603	36.685850
1552.929769	115574.797254	36.690868
1554.380792	115731.334908	36.695885
1555.734658	115889.613265	36.700903
1557.496174	116058.153032	36.705920
1558.825639	116234.256662	36.710938
1560.673495	116393.043720	36.715956
1562.239400	116567.260356	36.720973
1563.505572	116746.788115	36.725991
1565.078063	116911.327825	36.731008
1566.570505	117092.940189	36.736026
1568.395756	117264.773252	36.741044
1570.092871	117443.425534	36.746061
1571.845931	117612.341485	36.751079
1573.756452	117778.773021	36.756096
1575.181262	117954.020108	36.761114
1577.192419	118111.431876	36.766132
1578.701566	118291.284370	36.771149
1580.516193	118454.867230	36.776167
1582.209692	118608.652131	36.781184
1583.873374	118780.732895	36.786202
1585.994551	118934.186185	36.791220
1587.516439	119108.091666	36.796237
1589.042764	119279.612592	36.801255
1590.556938	119434.088332	36.806272
1592.165252	119597.251586	36.811290
1594.164659	119752.236576	36.816308
1595.654998	119925.592574	36.821325
1596.820635	120090.742200	36.826343
1598.259944	120256.737869	36.831360
1599.842407	120433.379837	36.836378
1601.370042	120601.189846	36.841396
1603.123954	120779.328889	36.846413
1604.628118	120966.120680	36.851431
1606.431954	121129.805453	36.856448
1607.919359	121303.193469	36.861466
1609.559794	121472.232829	36.866484
1610.632264	121635.551531	36.871501
1611.862562	121821.552839	36.876519
1613.938938	122001.017296	36.881536
1615.550315	122192.935812	36.886554
1617.369628	122368.547574	36.891572
1618.830518	122549.454987	36.896589
1620.113787	122745.994027	36.901607
1621.683445	122934.827400	36.906624
1623.390235	123114.062697	36.911642
1624.985626	123298.035212	36.916660
1626.673458	123484.645511	36.921677
1628.158747	123670.780780	36.926695
1629.959462	123856.677539	36.931712
1631.553199	124051.398712	36.936730
1633.212182	124237.205131	36.941748
1634.602178	124425.236276	36.946765
1636.026426	124624.096889	36.951783
1637.643513	124812.310166	36.956800
1639.651175	125009.940133	36.961818
1641.426392	125202.228268	36.966836
1643.005424	125386.897997	36.971853
1644.318287	125581.061354	36.976871
1646.360067	125746.377393	36.981888
1648.309906	125910.262157	36.986906
1649.835710	126073.909102	36.991924
1651.607850	126247.540774	36.996941
1653.149428	126412.455283	37.001959
1654.969518	126576.464414	37.006976
1656.684237	126758.987887	37.011994
1658.160941	126922.252582	37.017012
1659.992229	127092.415136	37.022029
1661.227999	127264.688300	37.027047
1663.235823	127428.874607	37.032064
1665.135671	127601.261497	37.037082
1666.524821	127773.360667	37.042100
1668.764293	127938.236107	37.047117
1670.416589	128113.936937	37.052135
1671.997065	128275.947487	37.057152
1673.758959	128451.949867	37.062170
1675.353044	128615.253720	37.067188
1677.337532	128786.312871	37.072205
1678.376445	128967.530271	37.077223
1680.052943	129145.870661	37.082240
1681.490563	129339.385222	37.087258
1683.176553	129522.940313	37.092276
1684.542859	129700.899953	37.097293
1686.279772	129894.332413	37.102311
1688.129855	130090.831270	37.107328
1689.406370	130293.231331	37.112346
1690.788600	130489.449588	37.117364
1692.357567	130689.484132	37.122381
1694.086879	130903.007382	37.127399
1695.233527	131108.248257	37.132416
1697.302174	131325.273456	37.137434
1698.664768	131535.875219	37.142452
1700.612577	131761.384450	37.147469
1701.920591	131965.639987	37.152487
1704.108435	132184.592269	37.157504
1705.688583	132411.646650	37.162522
1707.506216	132623.413658	37.167540
1709.614193	132843.117619	37.172557
1710.870073	133062.079788	37.177575
1712.934573	133270.068359	37.182592
1715.136836	133493.212232	37.187610
1716.332619	133709.116299	37.192628
1718.369183	133922.644629	37.197645
1720.157793	134142.252522	37.202663
1722.022355	134357.903399	37.207680
1723.704123	134573.926377	37.212698
1725.875256	134791.016260	37.217716
1727.609084	135006.919031	37.222733
1728.874276	135216.132407	37.227751
1730.734225	135420.914445	37.232768
1732.736147	135635.040076	37.237786
1733.936393	135850.877676	37.242804
1736.571267	136052.407686	37.247821
1737.993630	136270.420689	37.252839
1739.752679	136483.116148	37.257856
1741.294879	136699.995873	37.262874
1743.210841	136907.719921	37.267892
1745.341274	137112.645160	37.272909
1746.867797	137323.883330	37.277927
1748.689274	137528.338228	37.282944
1750.669727	137743.949144	37.287962
1752.543177	137948.473956	37.292980
1754.194685	138161.739605	37.297997
1755.623984	138359.685762	37.303015
1757.309303	138567.922724	37.308032
1758.971839	138782.509283	37.313050
1760.751552	138989.210605	37.318068
1762.256299	139178.265283	37.323085
1763.873701	139382.277864	37.328103
1765.382118	139586.473269	37.333120
1767.440354	139787.918978	37.338138
1768.565074	139994.815493	37.343156
1770.030112	140195.263870	37.348173
1771.241336	140411.209843	37.353191
1773.593921	140615.024483	37.358208
1775.369351	140844.806346	37.363226
1776.648240	141067.838912	37.368244
1778.757447	141288.801577	37.373261
1779.955143	141514.666236	37.378279
1781.647329	141746.711669	37.383296
1783.451686	141984.794411	37.388314
1785.001096	142226.382685	37.393332
1786.701776	142466.984083	37.398349
1788.425670	142720.287031	37.403367
1790.611347	142951.208026	37.408384
1792.276606	143192.440379	37.413402
1794.121018	143451.997902	37.418420
1795.962144	143702.635147	37.423437
1797.852111	143940.181017	37.428455
1799.655550	144176.535782	37.433472
1801.892800	144430.973315	37.438490
1803.204688	144675.098131	37.443508
1805.332837	144934.276548	37.448525
1807.090097	145188.069192	37.453543
1809.528766	145434.167258	37.458560
1811.761002	145669.535801	37.463578
1813.589540	145909.029738	37.468596
1815.440831	146144.903995	37.473613
1817.253122	146388.921122	37.478631
1819.542815	146626.049359	37.483648
1821.710514	146864.314603	37.488666
1823.005600	147090.988991	37.493684
1825.570417	147317.758683	37.498701
1827.791551	147552.414132	37.503719
1829.763292	147772.893790	37.508736
1831.765710	147991.173786	37.513754
1833.207494	148220.153015	37.518772
1835.275074	148438.919751	37.523789
1836.758024	148672.781243	37.528807
1838.483474	148899.751902	37.533824
1840.302598	149137.028271	37.538842
1841.863236	149370.499970	37.543860
1843.731879	149605.029047	37.548877
1845.425051	149849.652054	37.553895
1847.124623	150083.663743	37.558912
1848.965634	150337.747721	37.563930
1850.505744	150581.788611	37.568948
1852.429271	150826.253274	37.573965
1854.199324	151075.210981	37.578983
1856.320979	151316.613306	37.584000
1858.147190	151572.000094	37.589018
1859.818734	151840.296064	37.594036
1861.890587	152090.810805	37.599053
1863.600467	152334.287277	37.604071
1865.717708	152585.165310	37.609088
1867.768902	152833.541393	37.614106
1869.152746	153092.659854	37.619124
1870.925057	153333.541445	37.624141
1872.649915	153592.114081	37.629159
1874.182297	153842.949146	37.634176
1876.217334	154102.681773	37.639194
1877.568972	154371.103155	37.644212
1879.408692	154628.380540	37.649229
1881.105521	154905.192320	37.654247
1883.114641	155164.692625	37.659264
1884.752709	155408.904411	37.664282
1886.516685	155669.346435	37.669300
1888.245901	155911.299249	37.674317
1889.823363	156178.843383	37.679335
1892.011081	156436.975967	37.684352
1893.699760	156693.638614	37.689370
1895.313361	156957.626187	37.694388
1897.354897	157211.303704	37.699405
1899.427133	157481.747317	37.704423
1901.359269	157753.610394	37.709440
1903.244570	158014.297803	37.714458
1904.773799	158280.157821	37.719476
1906.864894	158551.466584	37.724493
1908.923427	158829.675046	37.729511
1910.899621	159105.561696	37.734528
1913.383893	159369.348196	37.739546
1915.315041	159638.300006	37.744564
1917.675659	159904.329715	37.749581
1919.327805	160179.281394	37.754599
1920.891593	160445.792914	37.759616
1923.175367	160718.452374	37.764634
1924.719507	161007.491070	37.769652
1926.945656	161274.626681	37.774669
1929.418354	161553.354230	37.779687
1931.017044	161832.257120	37.784704
1932.727449	162104.465895	37.789722
1934.585351	162388.218726	37.794740
1936.776309	162666.829949	37.799757
1938.530385	162945.053318	37.804775
1940.878550	163232.263020	37.809792
1943.228710	163500.861350	37.814810
1945.560455	163768.790760	37.819828
1947.828130	164040.146487	37.824845
1949.815428	164301.999464	37.829863
1951.756555	164577.229762	37.834880
1953.979084	164850.957335	37.839898
1955.514397	165123.205946	37.844916
1957.206758	165398.719576	37.849933
1958.905909	165676.226612	37.854951
1960.874866	165959.456989	37.859968
1962.967589	166230.506023	37.864986
1964.560002	166532.486654	37.870004
1966.113526	166809.944789	37.875021
1967.793741	167099.154138	37.880039
1969.855143	167402.347949	37.885056
1971.938589	167695.179073	37.890074
1973.488984	168007.952233	37.895092
1975.256786	168307.792904	37.900109
1977.365931	168624.049660	37.905127
1979.275924	168928.022722	37.910144
1981.272136	169224.974882	37.915162
1982.850371	169560.389382	37.920180
1984.723873	169868.371685	37.925197
1986.612542	170190.535730	37.930215
1988.019067	170515.810879	37.935232
1990.615422	170836.445524	37.940250
1992.256698	171171.603645	37.945268
1994.332064	171489.744623	37.950285
1996.534818	171822.621622	37.955303
1998.222230	172159.757791	37.960320
2000.214458	172487.553364	37.965338
2002.162791	172821.998057	37.970356
2003.799750	173159.527421	37.975373
2006.049228	173495.489988	37.980391
2007.873442	173843.798997	37.985408
2010.238075	174176.280063	37.990426
2011.911126	174513.466819	37.995444
2014.065693	174836.472594	38.000461
2016.406304	175155.831777	38.005479
2018.274456	175484.281409	38.010496
2020.518387	175791.531475	38.015514
2022.163503	176106.177358	38.020532
2024.730779	176421.582507	38.025549
2026.861747	176730.326673	38.030567
2028.379270	177047.180111	38.035584
2030.973626	177357.403683	38.040602
2032.761789	177669.912604	38.045620
2035.483210	177972.321828	38.050637
2037.400244	178299.289278	38.055655
2039.851274	178613.933443	38.060672
2041.996499	178903.584675	38.065690
2043.791160	179218.866535	38.070708
2046.117076	179530.790585	38.075725
2048.400522	179841.325489	38.080743
2050.165792	180152.881837	38.085760
2052.054972	180469.347140	38.090778
2054.070339	180790.060744	38.095796
2055.774880	181107.852311	38.100813
2058.013480	181432.292327	38.105831
2059.952726	181752.462413	38.110848
2061.618405	182079.406687	38.115866
2063.811603	182418.334165	38.120884
2065.625934	182755.620145	38.125901
2068.087643	183094.584463	38.130919
2069.744847	183433.878380	38.135936
2071.660146	183791.394910	38.140954
2073.806829	184131.580250	38.145972
2076.207427	184482.826517	38.150989
2078.128877	184830.338779	38.156007
2079.487567	185183.197420	38.161024
2081.927071	185531.088679	38.166042
2083.655409	185954.324032	38.171060
2085.722068	186331.713662	38.176077
2087.981690	186696.501977	38.181095
2089.738906	187067.287824	38.186112
2091.703456	187429.127486	38.191130
2093.870361	187811.866150	38.196148
2095.872930	188182.008117	38.201165
2098.441358	188555.924049	38.206183
2100.416821	188933.718123	38.211200
2102.324811	189316.883376	38.216218
2104.568718	189700.556468	38.221236
2106.597701	190074.713873	38.226253
2108.691907	190457.600022	38.231271
2110.462545	190843.001628	38.236288
2112.823859	191221.937093	38.241306
2115.227950	191612.602125	38.246324
2117.435741	191995.374026	38.251341
2120.056756	192371.021466	38.256359
2122.040168	192748.953755	38.261376
2124.586426	193133.810218	38.266394
2126.533826	193507.813309	38.271412
2128.732040	193886.680853	38.276429
2130.997542	194255.912077	38.281447
2132.987859	194630.648413	38.286464
2135.255029	195005.291936	38.291482
2137.382278	195378.510428	38.296500
2139.548669	195766.837629	38.301517
2141.885211	196145.944176	38.306535
2143.735616	196518.548461	38.311552
2145.834681	196894.747458	38.316570
2147.905235	197278.750175	38.321588
2149.949488	197666.568262	38.326605
2151.997156	198051.491065	38.331623
2154.126309	198439.450408	38.336640
2156.522121	198810.604064	38.341658
2158.645994	199185.458827	38.346676
2160.524443	199544.247874	38.351693
2162.431891	199890.891085	38.356711
2164.098895	200263.787401	38.361728
2166.435490	200628.731129	38.366746
2167.888656	200996.302581	38.371764
2169.825044	201379.879265	38.376781
2172.288622	201756.389158	38.381799
2174.043909	202153.890846	38.386816
2176.503683	202540.284575	38.391834
2179.292982	202930.743074	38.396852
2181.451602	203308.396106	38.401869
2183.374836	203693.504108	38.406887
2185.228544	204103.162669	38.411904
2187.538641	204489.660067	38.416922
2190.035420	204885.401191	38.421940
2191.674099	205285.645943	38.426957
2194.550775	205678.179599	38.431975
2197.493830	206071.186344	38.436992
2199.949740	206471.560292	38.442010
2201.980711	206870.273734	38.447028
2203.938449	207263.766292	38.452045
2206.381519	207650.655438	38.457063
2208.402709	208050.922138	38.462080
2210.722561	208442.709212	38.467098
2213.229373	208844.527511	38.472116
2215.083040	209244.949342	38.477133
2217.332336	209655.242937	38.482151
2219.610967	210058.800757	38.487168
2221.843162	210465.795890	38.492186
2223.699696	210875.796906	38.497204
2225.948429	211294.781126	38.502221
2228.399688	211698.314548	38.507239
2230.167518	212118.975247	38.512256
2232.579596	212537.427787	38.517274
2234.849800	212946.122602	38.522292
2236.903961	213378.807173	38.527309
2239.270564	213801.917328	38.532327
2241.608545	214225.692963	38.537344
2243.787225	214650.764089	38.542362
2246.266529	215080.412407	38.547380
2248.754255	215501.498836	38.552397
2251.600162	215912.393862	38.557415
2253.686616	216342.282527	38.562432
2255.918946	216761.098252	38.567450
2258.202748	217172.590047	38.572468
2260.263808	217592.017476	38.577485
2263.144997	218000.597181	38.582503
2265.444874	218425.958056	38.587520
2267.833046	218838.247894	38.592538
2270.168353	219259.463044	38.597556
2273.351480	219655.193369	38.602573
2275.557980	220060.424593	38.607591
2278.069269	220462.433117	38.612608
2279.971686	220854.502025	38.617626
2282.854234	221257.520151	38.622644
2284.953850	221654.461720	38.627661
2287.331841	222059.946701	38.632679
2289.283703	222454.955467	38.637696
2290.970829	222857.906230	38.642714
2293.263921	223262.083822	38.647732
2295.145276	223681.898300	38.652749
2298.212259	224088.038788	38.657767
2299.584082	224499.828828	38.662784
2301.822554	224919.613363	38.667802
2303.825128	225343.270671	38.672820
2305.895172	225758.762789	38.677837
2307.761966	226176.395083	38.682855
2310.296763	226591.535422	38.687872
2312.072513	226994.117215	38.692890
2314.088001	227398.668579	38.697908
2316.316754	227831.334422	38.702925
2318.694425	228242.180299	38.707943
2320.640328	228660.181011	38.712960
2322.963601	229085.642480	38.717978
2325.387088	229512.739475	38.722996
2327.358918	229945.216045	38.728013
2329.835715	230374.819399	38.733031
2331.789402	230810.804158	38.738048
2334.299671	231253.611961	38.743066
2336.939539	231705.062100	38.748084
2338.902974	232154.584901	38.753101
2341.226773	232590.714233	38.758119
2343.277610	233054.576027	38.763136
2345.273627	233517.379010	38.768154
2348.047457	233982.854976	38.773172
2350.487625	234455.571734	38.778189
2352.923930	234926.561164	38.783207
2355.341212	235388.941170	38.788224
2357.496885	235856.746995	38.793242
2359.804218	236334.944226	38.798260
2362.011255	236815.646047	38.803277
2364.637955	237296.840821	38.808295
2367.014746	237782.544886	38.813312
2369.306326	238264.374770	38.818330
2371.840369	238755.870388	38.823348
2374.262211	239245.121791	38.828365
2376.701537	239723.268359	38.833383
2379.221185	240222.994596	38.838400
2381.498256	240723.341987	38.843418
2383.915458	241211.752480	38.848436
2386.311177	241705.550927	38.853453
2389.075327	242188.621719	38.858471
2391.527762	242690.284442	38.863488
2393.462006	243189.892908	38.868506
2396.238323	243687.794277	38.873524
2398.459599	244185.501510	38.878541
2400.919202	244684.339083	38.883559
2403.357708	245180.435276	38.888576
2406.230997	245693.711201	38.893594
2408.589386	246177.954350	38.898612
2410.820407	246689.371702	38.903629
2414.025229	247188.950940	38.908647
2416.571092	247679.715104	38.913664
2418.945571	248176.626672	38.918682
2421.952791	248671.380821	38.923700
2424.508269	249154.823624	38.928717
2427.060108	249629.603461	38.933735
2429.637927	250115.250120	38.938752
2432.050768	250606.331723	38.943770
2434.675690	251084.042745	38.948788
2436.813098	251575.164305	38.953805
2439.269487	252053.355908	38.958823
2442.064538	252542.898792	38.963840
2443.607499	253022.017010	38.968858
2446.192761	253512.300668	38.973876
2448.361503	254001.631455	38.978893
2450.922542	254491.153558	38.983911
2453.577870	254980.024274	38.988928
2455.959839	255482.855783	38.993946
2458.207792	255968.966869	38.998964
2460.476367	256469.297675	39.003981
2463.255910	256952.858565	39.008999
2465.777635	257454.340107	39.014016
2467.999651	257950.151142	39.019034
2470.424473	258430.866009	39.024052
2472.920591	258919.696165	39.029069
2474.888029	259396.719178	39.034087
2477.366836	259858.826845	39.039104
2479.584570	260332.327350	39.044122
2482.003629	260810.163486	39.049140
2484.503492	261288.366097	39.054157
2486.662695	261764.816333	39.059175
2489.466200	262241.951707	39.064192
2493.185581	262721.304712	39.069210
2496.350565	263179.634706	39.074228
2498.949525	263647.931337	39.079245
2501.123628	264114.844283	39.084263
2503.402938	264583.542176	39.089280
2506.092988	265047.373592	39.094298
2508.731221	265519.668949	39.099316
2510.767304	266022.128380	39.104333
2513.212142	266484.746927	39.109351
2515.785234	266973.224822	39.114368
2518.166524	267461.755563	39.119386
2520.727871	267941.823516	39.124404
2522.864963	268439.124488	39.129421
2525.083932	268932.067025	39.134439
2527.868326	269433.884575	39.139456
2529.921688	269948.131266	39.144474
2532.448403	270457.094865	39.149492
2534.581117	270976.428451	39.154509
2536.877961	271503.581385	39.159527
2539.322141	272029.717784	39.164544
2541.834864	272560.005550	39.169562
2544.507771	273088.715945	39.174580
2546.549968	273630.016592	39.179597
2549.163438	274184.202703	39.184615
2551.839221	274719.505745	39.189632
2554.211939	275278.115737	39.194650
2556.900154	275827.682549	39.199668
2559.544724	276380.604752	39.204685
2562.166343	276934.466398	39.209703
2565.055531	277479.901945	39.214720
2567.905374	278031.358624	39.219738
2571.052397	278576.695652	39.224756
2573.756482	279126.211807	39.229773
2576.497575	279672.823222	39.234791
2579.070281	280212.397114	39.239808
2581.591490	280765.815279	39.244826
2584.194768	281318.023011	39.249844
2586.988278	281864.940365	39.254861
2589.105111	282411.298672	39.259879
2591.964170	282962.412983	39.264896
2594.350601	283518.065901	39.269914
2597.179540	284069.811166	39.274932
2599.798720	284622.727435	39.279949
2601.835636	285181.087876	39.284967
2604.962546	285734.043211	39.289984
2607.809136	286282.009918	39.295002
2610.903692	286830.568405	39.300020
2613.325904	287392.278691	39.305037
2616.230313	287945.301252	39.310055
2619.115044	288469.324650	39.315072
2621.785938	289020.825556	39.320090
2624.271167	289560.772128	39.325108
2627.623296	290095.551768	39.330125
2629.947577	290629.166524	39.335143
2632.734831	291157.956624	39.340160
2635.091123	291707.401123	39.345178
2637.982267	292234.794812	39.350196
2640.447007	292764.179988	39.355213
2643.160891	293295.324486	39.360231
2646.308106	293807.354571	39.365248
2648.799998	294317.324159	39.370266
2651.394668	294804.651496	39.375284
2654.003800	295296.923449	39.380301
2656.333377	295795.505842	39.385319
2659.191157	296292.376900	39.390336
2661.449824	296802.056552	39.395354
2663.681204	297302.240732	39.400372
2666.037434	297811.033029	39.405389
2668.559996	298343.405515	39.410407
2671.035898	298857.374260	39.415424
2673.350877	299394.262672	39.420442
2675.953129	299916.529012	39.425460
2678.288793	300461.578474	39.430477
2680.626461	300998.346174	39.435495
2683.455210	301554.046488	39.440512
2686.118841	302113.320811	39.445530
2688.742753	302676.707964	39.450548
2690.989996	303234.258321	39.455565
2693.700535	303807.418754	39.460583
2696.292531	304381.124442	39.465600
2699.325843	304964.172825	39.470618
2702.114438	305558.294897	39.475636
2704.898412	306127.940542	39.480653
2707.504091	306704.943462	39.485671
2710.346193	307289.391124	39.490688
2712.794540	307883.031193	39.495706
2715.274697	308460.794914	39.500724
2718.154072	309057.628227	39.505741
2720.639477	309670.988680	39.510759
2723.037166	310270.877234	39.515776
2726.057083	310900.687984	39.520794
2728.919257	311508.864760	39.525812
2731.566474	312129.199326	39.530829
2734.390738	312743.153037	39.535847
2736.828564	313368.909936	39.540864
2739.771485	313999.731961	39.545882
2742.469664	314630.304293	39.550900
2744.809582	315257.903588	39.555917
2747.791229	315898.236112	39.560935
2751.029867	316525.804932	39.565952
2753.721254	317158.170499	39.570970
2756.394428	317781.089388	39.575988
2759.471667	318421.370975	39.581005
2762.218435	319058.547918	39.586023
2765.554741	319681.184471	39.591040
2768.213917	320328.989325	39.596058
2771.052529	320969.169111	39.601076
2773.476436	321599.507381	39.606093
2776.084425	322239.805514	39.611111
2779.441007	322882.235817	39.616128
2782.028059	323525.562653	39.621146
2784.728084	324164.142415	39.626164
2787.626017	324811.080225	39.631181
2790.220306	325453.183457	39.636199
2793.347665	326091.514590	39.641216
2796.429048	326742.123127	39.646234
2799.354240	327373.082140	39.651252
2802.835932	328007.242948	39.656269
2806.135458	328631.222769	39.661287
2808.866958	329250.080132	39.666304
2811.998303	329878.480958	39.671322
2814.891265	330492.879151	39.676340
2818.028460	331101.115549	39.681357
2820.556392	331714.637898	39.686375
2823.814129	332321.364884	39.691392
2826.578391	332926.408613	39.696410
2829.303938	333536.978980	39.701428
2832.498351	334127.552919	39.706445
2834.603506	334705.806397	39.711463
2837.352755	335272.687813	39.716480
2840.262897	335861.350734	39.721498
2842.632907	336433.118438	39.726516
2845.101908	337017.747629	39.731533
2847.285737	337606.368850	39.736551
2850.141173	338198.072022	39.741568
2852.531173	338796.052252	39.746586
2854.893295	339410.817879	39.751604
2857.844546	340018.455576	39.756621
2860.562981	340643.340720	39.761639
2862.922499	341271.339591	39.766656
2865.806119	341906.068161	39.771674
2868.795325	342530.979171	39.776692
2871.827091	343166.295861	39.781709
2874.744121	343796.952376	39.786727
2877.833351	344436.395978	39.791744
2880.578871	345089.271179	39.796762
2882.910440	345739.003023	39.801780
2885.807582	346411.533521	39.806797
2888.627365	347080.106746	39.811815
2891.476455	347739.609324	39.816832
2894.492447	348410.711945	39.821850
2897.345484	349093.744088	39.826868
2900.015624	349775.649526	39.831885
2902.850993	350456.019095	39.836903
2906.109298	351140.923333	39.841920
2908.717140	351838.363524	39.846938
2911.721685	352535.549438	39.851956
2914.622076	353232.026520	39.856973
2917.022706	353937.186229	39.861991
2920.296061	354645.439593	39.867008
2923.505817	355354.320766	39.872026
2926.429722	356057.957332	39.877044
2929.661569	356767.132652	39.882061
2932.698386	357466.435542	39.887079
2935.829545	358181.957041	39.892096
2938.826145	358882.932461	39.897114
2942.207332	359598.483368	39.902132
2945.440614	360296.677154	39.907149
2948.331282	361000.687313	39.912167
2951.946758	361712.324289	39.917184
2955.016970	362412.420678	39.922202
2958.000562	363101.868968	39.927220
2961.305366	363792.112947	39.932237
2964.645082	364488.164510	39.937255
2967.611447	365170.724098	39.942272
2970.627543	365861.547175	39.947290
2973.325175	366557.522552	39.952308
2976.871678	367250.130637	39.957325
2979.409151	367932.438431	39.962343
2982.823167	368615.100356	39.967360
2985.891903	369309.658786	39.972378
2988.817200	369988.258643	39.977396
2992.126539	370663.615039	39.982413
2995.007928	371350.373296	39.987431
2998.389038	372030.854515	39.992448
3001.285114	372711.875945	39.997466
3003.748997	373397.964458	40.002484
3006.709036	374074.508433	40.007501
3009.318551	374757.702709	40.012519
3012.478788	375445.531714	40.017536
3015.665813	376133.719123	40.022554
3018.386793	376825.178835	40.027572
3021.422790	377510.035956	40.032589
3024.374630	378205.300047	40.037607
3027.180259	378896.161116	40.042624
3030.088908	379577.286556	40.047642
3032.740946	380246.453309	40.052660
3036.225171	380914.865625	40.057677
3038.516816	381572.200536	40.062695
3041.631070	382241.016405	40.067712
3044.620700	382909.125258	40.072730
3047.123473	383589.854620	40.077748
3050.263931	384271.682381	40.082765
3053.165725	384953.377174	40.087783
3056.072085	385635.584848	40.092800
3059.020365	386333.038002	40.097818
3061.677949	387030.187944	40.102836
3064.715644	387732.222638	40.107853
3067.615061	388439.981908	40.112871
3070.763875	389154.443014	40.117888
3073.540500	389883.070236	40.122906
3076.588519	390612.621213	40.127924
3080.034425	391330.695163	40.132941
3083.462158	392075.689344	40.137959
3086.520268	392800.160620	40.142976
3090.202386	393530.791684	40.147994
3092.504428	394277.311209	40.153012
3095.756602	395020.419408	40.158029
3098.805562	395766.219485	40.163047
3102.086432	396508.618781	40.168064
3105.041496	397262.638743	40.173082
3107.879138	398024.043973	40.178100
3110.866475	398780.592190	40.183117
3113.839501	399550.228864	40.188135
3117.172708	400321.403888	40.193152
3120.240689	401098.516750	40.198170
3122.996715	401878.587711	40.203188
3126.568162	402656.582024	40.208205
3129.587255	403442.328851	40.213223
3132.047486	404227.072759	40.218240
3135.770702	405021.562834	40.223258
3138.781584	405822.309807	40.228276
3142.242604	406617.644742	40.233293
3145.909867	407414.133802	40.238311
3149.099615	408206.721828	40.243328
3152.051600	408991.931059	40.248346
3155.515147	409790.542303	40.253364
3158.718046	410578.894209	40.258381
3162.228437	411382.246835	40.263399
3165.290641	412173.345777	40.268416
3168.746158	412969.413699	40.273434
3172.235438	413770.202340	40.278452
3175.407661	414558.819226	40.283469
3178.840510	415363.250052	40.288487
3181.716202	416154.332885	40.293504
3184.812378	416943.328735	40.298522
3187.816900	417742.829812	40.303540
3191.401501	418536.191644	40.308557
3194.247620	419334.695883	40.313575
3197.644163	420147.294957	40.318592
3200.912653	420945.014347	40.323610
3203.881168	421756.251633	40.328628
3207.196644	422551.474410	40.333645
3210.330942	423355.492925	40.338663
3213.938315	424163.299584	40.343680
3217.079704	424960.326649	40.348698
3220.175164	425768.503116	40.353716
3223.183992	426568.419938	40.358733
3226.491640	427391.311564	40.363751
3229.253474	428206.570289	40.368768
3232.726663	429010.614374	40.373786
3235.703096	429832.294229	40.378804
3239.210973	430635.003344	40.383821
3242.010861	431445.826552	40.388839
3245.421818	432220.989715	40.393856
3248.705401	432994.625756	40.398874
3251.608284	433786.635849	40.403892
3254.734979	434563.973727	40.408909
3258.027978	435340.850196	40.413927
3260.987956	436133.715422	40.418944
3264.201293	436908.469102	40.423962
3267.259088	437707.570251	40.428980
3270.571024	438510.488834	40.433997
3273.938965	439323.216898	40.439015
3276.813770	440129.620983	40.444032
3280.613532	440925.641602	40.449050
3283.183347	441751.978780	40.454068
3286.484903	442571.901641	40.459085
3289.670500	443400.444135	40.464103
3293.016240	444235.693103	40.469120
3296.314520	445070.356063	40.474138
3299.731172	445908.346621	40.479156
3303.063028	446753.483569	40.484173
3306.704442	447601.260267	40.489191
3309.910542	448446.035196	40.494208
3313.865676	449298.733613	40.499226
3316.519845	450151.240674	40.504244
3320.321328	451007.214645	40.509261
3323.604547	451858.229832	40.514279
3326.687672	452729.581801	40.519296
3330.507505	453584.065950	40.524314
3333.565014	454455.589418	40.529332
3336.910038	455324.349594	40.534349
3340.423430	456198.239683	40.539367
3343.535867	457074.167436	40.544384
3347.129523	457948.663950	40.549402
3350.526566	458829.556566	40.554420
3353.823999	459719.352382	40.559437
3357.167748	460599.254431	40.564455
3360.671812	461493.467920	40.569472
3364.434864	462375.988680	40.574490
3367.512845	463274.716271	40.579508
3371.424051	464161.258532	40.584525
3374.330036	465045.034908	40.589543
3378.040594	465942.664265	40.594560
3381.454209	466832.472615	40.599578
3384.877255	467722.686005	40.604596
3388.174407	468622.152291	40.609613
3392.089545	469506.947519	40.614631
3395.619975	470388.073376	40.619648
3399.355229	471276.331885	40.624666
3403.049905	472185.880100	40.629684
3406.149820	473068.189359	40.634701
3409.521363	473954.492751	40.639719
3412.527608	474849.527285	40.644736
3416.332731	475734.455423	40.649754
3419.669556	476640.128420	40.654772
3422.947227	477534.618186	40.659789
3426.773834	478430.081361	40.664807
3430.352546	479316.056121	40.669824
3433.943844	480202.231342	40.674842
3437.241274	481102.968453	40.679860
3440.712240	481996.923943	40.684877
3443.999373	482893.275972	40.689895
3447.291254	483789.827718	40.694912
3450.762134	484683.478072	40.699930
3454.151542	485589.686217	40.704948
3457.425506	486487.646551	40.709965
3461.025635	487395.529470	40.714983
3464.206183	488299.595159	40.720000
3467.924955	489198.435694	40.725018
3471.191501	490094.630982	40.730023
3474.243145	490953.552883	40.735028
3477.787603	491772.609662	40.740032
3480.655712	492538.205133	40.745037
3483.874542	493247.158120	40.750042
3486.629957	493904.197646	40.755047
3488.979754	494515.834169	40.760052
3491.873832	495068.446182	40.765056
3493.849749	495575.595103	40.770061
3496.583546	496034.500718	40.775066
3498.632540	496452.307633	40.780071
3500.832745	496799.813869	40.785076
3503.106535	497111.007532	40.790080
3504.746599	497389.685730	40.795085
3506.520475	497608.423742	40.800090
3507.961757	497802.225320	40.805095
3509.260117	497945.976296	40.810100
3510.811110	498069.598016	40.815104
3512.116767	498154.291420	40.820109
3513.319353	498192.110735	40.825114
3513.824579	498217.268746	40.830119
3514.910644	498214.172288	40.835124
3515.446679	498173.356905	40.840128
3516.297344	498135.874175	40.845133
3517.150539	498060.182364	40.850138
3517.448632	497969.989543	40.855143
3517.778762	497853.241632	40.860148
3518.505183	497732.695988	40.865152
3518.843526	497600.398523	40.870157
3519.017781	497445.512231	40.875162
3519.793775	497289.521146	40.880167
3519.884232	497112.889055	40.885172
3519.737972	496907.973718	40.890176
3519.883972	496728.451157	40.895181
3520.311533	496532.022628	40.900186
3520.323102	496315.969144	40.905191
3519.968321	496096.183481	40.910196
3520.477235	495880.147210	40.915200
3520.748107	495661.166402	40.920205
3520.945327	495424.575352	40.925210
3520.279905	495189.982666	40.930215
3520.403722	494940.522022	40.935220
3520.537629	494700.546853	40.940224
3519.990018	494465.924419	40.945229
3520.406033	494221.909251	40.950234
3520.193039	493982.935769	40.955239
3520.111044	493735.001620	40.960244
3520.097711	493481.498850	40.965248
3520.058498	493254.452654	40.970253
3519.648204	492997.368173	40.975258
3519.864889	492753.259100	40.980263
3519.435864	492496.118453	40.985268
3519.441602	492244.611518	40.990272
3519.298358	491990.043406	40.995277
3519.489091	491750.719061	41.000282
3519.197449	491507.628287	41.005287
3518.820021	491256.366463	41.010292
3518.703480	491005.110357	41.015296
3517.899056	490764.107312	41.020301
3518.246097	490512.316394	41.025306
3518.300366	490271.070876	41.030311
3517.975258	490035.587157	41.035316
3518.048277	489798.724785	41.040320
3517.907885	489563.760521	41.045325
3517.608575	489318.565194	41.050330
3517.587520	489085.746615	41.055335
3517.395069	488848.456220	41.060340
3517.326799	488609.728650	41.065344
3516.719542	488388.859463	41.070349
3516.697348	488144.359720	41.075354
3516.175606	487926.096906	41.080359
3516.620503	487706.316824	41.085364
3515.980534	487485.439675	41.090368
3515.724153	487265.206791	41.095373
3515.787111	487041.486318	41.100378
3515.641804	486830.321849	41.105383
3515.365378	486618.770784	41.110388
3514.776707	486405.244882	41.115392
3514.351249	486209.067282	41.120397
3514.618399	486004.495078	41.125402
3514.261588	485801.027555	41.130407
3513.910155	485608.619407	41.135412
3514.734124	485411.580536	41.140416
3514.184350	485214.500343	41.145421
3513.498981	485015.519075	41.150426
3513.866042	484832.739325	41.155431
3513.712500	484638.924332	41.160436
3513.843661	484440.212759	41.165440
3513.094493	484259.772285	41.170445
3513.119177	484080.320741	41.175450
3513.066054	483895.069309	41.180455
3512.901238	483722.059294	41.185460
3512.772832	483528.580183	41.190464
3512.116374	483367.768073	41.195469
3512.413861	483190.638389	41.200474
3512.381624	483020.328209	41.205479
3512.043430	482850.316403	41.210484
3512.159047	482673.967024	41.215488
3511.555300	482505.458012	41.220493
3511.837599	482331.655638	41.225498
3511.917788	482172.939736	41.230503
3511.698293	482015.936256	41.235508
3511.533686	481841.642190	41.240512
3511.250785	481691.921321	41.245517
3511.331697	481530.015519	41.250522
3511.283544	481374.090582	41.255527
3510.942474	481222.049938	41.260532
3510.871548	481064.559051	41.265536
3510.658198	480917.952854	41.270541
3510.561848	480771.175490	41.275546
3510.543577	480619.179849	41.280551
3510.259095	480466.516717	41.285556
3509.913042	480322.704896	41.290560
3510.176931	480189.206656	41.295565
3509.880949	480045.586650	41.300570
3509.942509	479911.915417	41.305575
3509.420223	479767.216348	41.310580
3509.622801	479633.318678	41.315584
3509.590802	479507.036663	41.320589
3509.491748	479364.794812	41.325594
3509.481171	479237.547135	41.330599
3509.231456	479102.603567	41.335604
3509.682718	478966.033662	41.340608
3509.223060	478838.296757	41.345613
3509.461377	478702.717933	41.350618
3509.060295	478576.485939	41.355623
3508.589042	478458.855417	41.360628
3508.897336	478325.536720	41.365632
3508.528980	478206.271070	41.370637
3508.580927	478079.610857	41.375642
3508.344309	477964.719854	41.380647
3508.047238	477844.227434	41.385652
3508.191522	477730.943307	41.390656
3508.348745	477621.446955	41.395661
3508.173494	477497.243447	41.400666
3508.167242	477384.030825	41.405671
3508.058714	477272.956092	41.410676
3508.168972	477159.673208	41.415680
3507.786040	477052.986316	41.420685
3507.743237	476935.227330	41.425690
3507.675818	476833.544213	41.430695
3507.437221	476717.380947	41.435700
3507.305021	476614.392372	41.440704
3507.153869	476523.132454	41.445709
3507.397437	476411.946409	41.450714
3507.368344	476314.752541	41.455719
3507.719472	476214.415633	41.460724
3507.375722	476109.637092	41.465728
3507.239063	476017.310575	41.470733
3507.393343	475904.972348	41.475738
3507.395690	475814.695447	41.480743
3507.008939	475700.822482	41.485748
3506.975587	475603.422783	41.490752
3506.773084	475504.936763	41.495757
3506.988108	475415.938773	41.500762
3506.899250	475318.748181	41.505767
3506.253431	475223.968915	41.510772
3506.585630	475124.841327	41.515776
3506.636016	475047.543754	41.520781
3506.870178	474950.806170	41.525786
3506.788485	474854.117157	41.530791
3506.534946	474769.586357	41.535796
3506.428489	474676.185893	41.540800
3505.842071	474589.987235	41.545805
3506.444540	474496.475414	41.550810
3506.396686	474414.994364	41.555815
3506.065714	474325.670914	41.560820
3506.367435	474230.788914	41.565824
3506.228859	474155.386896	41.570829
3506.428176	474072.500750	41.575834
3506.083915	473980.093765	41.580839
3505.971490	473901.248913	41.585844
3506.181137	473816.893817	41.590848
3506.078923	473737.692708	41.595853
3506.368014	473648.875675	41.600858
3505.863409	473565.692046	41.605863
3505.822077	473487.744091	41.610868
3505.801829	473401.653213	41.615872
3505.633381	473325.796993	41.620877
3505.403736	473240.597277	41.625882
3505.691586	473170.837032	41.630887
3505.175675	473098.926570	41.635892
3505.315696	473023.829825	41.640896
3505.195789	472952.969318	41.645901
3505.045920	472880.090921	41.650906
3505.289739	472807.656498	41.655911
3505.267682	472740.015441	41.660916
3505.141067	472664.250737	41.665920
3505.300976	472606.085474	41.670925
3505.527699	472532.944693	41.675930
3505.181925	472460.145458	41.680935
3505.000330	472382.669049	41.685940
3505.155419	472314.948103	41.690944
3505.155499	472245.784813	41.695949
3505.272696	472169.221497	41.700954
3504.998261	472095.954510	41.705959
3505.097037	472033.549802	41.710964
3505.227577	471963.454959	41.715968
3505.171753	471896.169568	41.720973
3505.311195	471825.718834	41.725978
3505.477868	471755.769155	41.730983
3504.877330	471687.354238	41.735988
3505.524536	471608.177828	41.740992
3504.994558	471538.234506	41.745997
3505.058567	471472.951135	41.751002
3504.799072	471420.408562	41.756007
3504.905459	471346.269983	41.761012
3504.816455	471268.571637	41.766016
3504.767526	471213.669825	41.771021
3504.755791	471146.323927	41.776026
3504.553936	471073.597239	41.781031
3504.892549	471024.449078	41.786036
3505.138079	470957.315180	41.791040
3504.613137	470891.261585	41.796045
3504.844360	470829.185612	41.801050
3505.089233	470759.876824	41.806055
3504.899493	470690.837627	41.811060
3505.093128	470622.800305	41.816064
3504.682051	470560.216509	41.821069
3504.639868	470490.951256	41.826074
3504.679949	470437.752154	41.831079
3504.671945	470364.688777	41.836084
3504.918369	470303.619731	41.841088
3504.508058	470250.844059	41.846093
3504.449957	470187.243194	41.851098
3504.598216	470121.840210	41.856103
3504.229281	470066.579842	41.861108
3504.654784	470010.285494	41.866112
3504.139102	469943.164779	41.871117
3504.663288	469891.911186	41.876122
3504.533197	469820.482482	41.881127
3504.076931	469771.504837	41.886132
3504.171272	469705.754632	41.891136
3504.333317	469654.657788	41.896141
3504.427128	469596.947230	41.901146
3504.737372	469542.590739	41.906151
3504.035589	469482.121299	41.911156
3504.301999	469423.827046	41.916160
3504.204383	469364.223926	41.921165
3504.163500	469300.212424	41.926170
3504.344961	469251.285696	41.931175
3504.423694	469194.941396	41.936180
3504.301143	469132.863517	41.941184
3503.903305	469083.065652	41.946189
3503.763906	469029.384257	41.951194
3504.409887	468968.349230	41.956199
3504.178666	468917.715848	41.961204
3504.022146	468877.336080	41.966208
3504.178747	468815.314706	41.971213
3504.095239	468758.033361	41.976218
3504.033854	468707.979735	41.981223
3503.917109	468660.463026	41.986228
3504.257999	468610.245368	41.991232
3504.065592	468543.928332	41.996237
3504.235224	468491.613048	42.001242
3504.415459	468432.924158	42.006247
3504.167756	468374.251083	42.011252
3504.036596	468317.177908	42.016256
3504.129088	468257.743501	42.021261
3503.897907	468212.266127	42.026266
3504.270429	468157.237982	42.031271
3503.766136	468116.202487	42.036276
3504.132821	468049.290765	42.041280
3503.926349	468003.252692	42.046285
3503.991029	467947.968332	42.051290
3503.973536	467906.097996	42.056295
3504.016087	467853.193619	42.061300
3503.743444	467791.184641	42.066304
3503.801131	467744.649599	42.071309
3503.698721	467685.041184	42.076314
3503.714776	467644.125837	42.081319
3503.736160	467588.189580	42.086324
3503.813700	467540.335997	42.091328
3503.875878	467500.525714	42.096333
3503.835802	467454.965956	42.101338
3503.646521	467401.590491	42.106343
3503.533035	467364.133571	42.111348
3503.861458	467303.951018	42.116352
3503.800821	467264.614442	42.121357
3503.703653	467205.863242	42.126362
3504.141967	467160.582249	42.131367
3503.682111	467100.471054	42.136372
3504.127955	467042.747403	42.141376
3503.956543	467007.726249	42.146381
3503.832865	466948.775971	42.151386
3503.906246	466900.516604	42.156391
3503.772643	466859.673194	42.161396
3503.945078	466804.368270	42.166400
3503.993575	466753.533039	42.171405
3504.036064	466699.006610	42.176410
3503.764322	466640.432309	42.181415
3503.803606	466603.657962	42.186420
3503.427127	466546.920343	42.191424
3503.471558	466501.597708	42.196429
3503.619089	466455.095662	42.201434
3503.759951	466408.847406	42.206439
3503.309771	466362.539266	42.211444
3503.557639	466312.531462	42.216448
3503.876636	466265.091835	42.221453
3503.500644	466215.231398	42.226458
3503.538051	466177.849488	42.231463
3503.124656	466139.981301	42.236468
3503.638276	466086.289942	42.241472
3503.335903	466053.209088	42.246477
3503.467919	465994.114499	42.251482
3503.833468	465953.899282	42.256487
3503.888478	465895.271524	42.261492
3503.684729	465849.024769	42.266496
3503.850754	465815.263624	42.271501
3504.005191	465754.950839	42.276506
3503.839598	465701.313365	42.281511
3503.942892	465658.659925	42.286516
3503.858081	465601.367931	42.291520
3503.477045	465559.851753	42.296525
3503.347446	465515.362787	42.301530
3503.795288	465467.597383	42.306535
3503.411711	465429.419476	42.311540
3503.399665	465381.017287	42.316544
3502.943583	465330.812625	42.321549
3503.497060	465288.138770	42.326554
3503.539956	465239.778203	42.331559
3503.520728	465205.741184	42.336564
3503.773075	465160.736627	42.341568
3503.645645	465111.036543	42.346573
3503.194672	465061.083179	42.351578
3503.245175	465010.596410	42.356583
3503.518093	464978.536675	42.361588
3503.840309	464925.528937	42.366592
3503.512901	464890.173565	42.371597
3503.433883	464845.725535	42.376602
3503.711930	464795.556776	42.381607
3503.081495	464754.684387	42.386612
3503.188831	464710.055257	42.391616
3503.034285	464675.330087	42.396621
3503.566361	464618.748047	42.401626
3503.472738	464570.356219	42.406631
3503.399429	464538.046035	42.411636
3503.680625	464483.323517	42.416640
3503.534633	464446.320367	42.421645
3503.606646	464396.435392	42.426650
3503.279398	464354.654957	42.431655
3503.089238	464320.491001	42.436660
3503.175191	464278.494332	42.441664
3503.264805	464235.283009	42.446669
3503.218291	464193.003245	42.451674
3503.183625	464153.200085	42.456679
3503.226719	464110.552091	42.461684
3503.059821	464060.399804	42.466688
3502.969770	464033.655387	42.471693
3502.802000	463983.503007	42.476698
3503.308759	463946.144267	42.481703
3503.147968	463906.461319	42.486708
3503.345341	463867.582463	42.491712
3503.496820	463834.123114	42.496717
3503.460158	463780.864126	42.501722
3503.219369	463743.267180	42.506727
3503.196937	463706.040844	42.511732
3503.413368	463648.240073	42.516736
3503.311868	463613.858554	42.521741
3503.210248	463580.589842	42.526746
3503.043806	463533.015724	42.531751
3503.318717	463499.587090	42.536756
3503.476379	463462.483947	42.541760
3503.278009	463414.206277	42.546765
3503.080518	463373.769016	42.551770
3503.376433	463324.503643	42.556775
3503.330634	463288.645825	42.561780
3503.641067	463231.284273	42.566784
3503.489393	463199.540164	42.571789
3503.450556	463154.120305	42.576794
3503.492924	463106.816011	42.581799
3503.231545	463067.652607	42.586804
3503.485835	463010.906077	42.591808
3503.054465	462981.076771	42.596813
3503.152173	462932.144619	42.601818
3503.230453	462882.810658	42.606823
3503.026240	462860.179659	42.611828
3503.177252	462818.928045	42.616832
3503.179301	462788.575673	42.621837
3503.138828	462740.322100	42.626842
3502.847551	462697.267299	42.631847
3502.289800	462660.223143	42.636852
3502.912794	462628.559767	42.641856
3502.676434	462592.578370	42.646861
3502.888746	462561.332888	42.651866
3502.911755	462526.575678	42.656871
3502.861715	462489.603906	42.661876
3503.014243	462455.787561	42.666880
3503.201824	462418.171604	42.671885
3502.917187	462374.052605	42.676890
3503.024524	462332.907784	42.681895
3503.128403	462296.063404	42.686900
3503.073685	462250.997719	42.691904
3502.902331	462222.846622	42.696909
3502.687827	462185.899782	42.701914
3502.681095	462154.788818	42.706919
3502.887996	462123.897497	42.711924
3503.148735	462075.190455	42.716928
3503.103555	462050.307717	42.721933
3502.661270	462015.267745	42.726938
3502.937332	461977.788814	42.731943
3503.084658	461937.800368	42.736948
3503.127185	461898.030494	42.741952
3502.836213	461861.347797	42.746957
3503.083415	461817.903439	42.751962
3503.244202	461779.784346	42.756967
3502.893672	461750.547375	42.761972
3502.897875	461694.948354	42.766976
3502.733924	461672.056558	42.771981
3503.024389	461631.943941	42.776986
3502.900656	461602.772605	42.781991
3502.838054	461570.859824	42.786996
3502.643548	461538.411014	42.792001
3502.720305	461498.230158	42.797005
3502.556330	461468.407176	42.802010
3502.935687	461431.973379	42.807015
3502.723057	461391.280805	42.812020
3502.556174	461360.294495	42.817025
3502.423083	461339.370500	42.822029
3502.857236	461300.651297	42.827034
3502.971713	461256.568481	42.832039
3502.521203	461226.637891	42.837044
3502.774637	461189.919625	42.842049
3502.482672	461168.311862	42.847053
3502.499536	461131.883243	42.852058
3502.752875	461099.718052	42.857063
3502.857968	461070.914933	42.862068
3502.958294	461035.940287	42.867073
3502.917314	461006.147951	42.872077
3502.999282	460962.524764	42.877082
3503.233358	460924.392360	42.882087
3502.960102	460892.409909	42.887092
3502.922470	460849.816895	42.892097
3502.828755	460823.422147	42.897101
3503.046728	460786.961499	42.902106
3502.918365	460738.260606	42.907111
3503.109403	460706.812672	42.912116
3502.897300	460664.195754	42.917121
3502.588981	460630.801663	42.922125
3502.323692	460600.335222	42.927130
3502.906382	460562.906665	42.932135
3502.747339	460537.179355	42.937140
3502.968550	460490.750660	42.942145
3502.725953	460457.649566	42.947149
3502.527390	460424.592150	42.952154
3502.937929	460388.606629	42.957159
3502.916176	460363.110664	42.962164
3502.902089	460315.301478	42.967169
3502.643843	460286.452394	42.972173
3502.711831	460254.213273	42.977178
3502.632608	460223.261859	42.982183
3502.440172	460192.783356	42.987188
3502.578067	460154.208858	42.992193
3502.962125	460132.798158	42.997197
3502.427715	460097.060261	43.002202
3502.826576	460060.873493	43.007207
3502.553544	460024.082873	43.012212
3502.665799	459999.273845	43.017217
3502.515324	459969.496747	43.022221
3502.683982	459937.443746	43.027226
3503.130787	459898.719415	43.032231
3502.748669	459865.487105	43.037236
3502.452542	459828.649065	43.042241
3502.941376	459796.596575	43.047245
3502.647006	459761.478370	43.052250
3502.695009	459726.458603	43.057255
3502.465208	459699.172578	43.062260
3502.711454	459665.487928	43.067265
3502.793078	459638.254536	43.072269
3502.656047	459600.784098	43.077274
3502.605340	459563.401338	43.082279
3502.552949	459541.602454	43.087284
3502.651107	459508.345313	43.092289
3502.401772	459473.017125	43.097293
3502.966682	459443.228987	43.102298
3502.551094	459412.379053	43.107303
3502.343871	459380.940073	43.112308
3502.895739	459346.701274	43.117313
3502.710941	459314.904506	43.122317
3502.554480	459287.505221	43.127322
3502.588241	459245.200704	43.132327
3502.709674	459229.952019	43.137332
3502.576616	459184.536279	43.142337
3502.557752	459161.112578	43.147341
3502.919106	459115.316135	43.152346
3502.810973	459085.480321	43.157351
3502.616590	459055.404889	43.162356
3502.650794	459017.451156	43.167361
3503.212213	458991.154040	43.172365
3502.679304	458953.288416	43.177370
3503.160679	458915.214276	43.182375
3502.897285	458873.106882	43.187380
3502.471495	458836.489291	43.192385
3502.198160	458807.285886	43.197389
3502.520194	458793.017571	43.202394
3502.751579	458751.541268	43.207399
3502.703970	458720.177444	43.212404
3502.767046	458686.418191	43.217409
3502.745486	458651.811860	43.222413
3502.464584	458619.421578	43.227418
3502.515218	458589.610801	43.232423
3502.322518	458561.406416	43.237428
3502.634233	458525.027595	43.242433
3502.523788	458487.601202	43.247437
3502.648308	458466.178226	43.252442
3502.826622	458434.879928	43.257447
3502.594901	458404.454975	43.262452
3502.594172	458372.678428	43.267457
3502.945660	458343.124010	43.272461
3502.869861	458306.197832	43.277466
3502.723623	458258.352909	43.282471
3502.688524	458235.993085	43.287476
3502.913706	458199.070443	43.292481
3502.877035	458168.513523	43.297485
3502.682325	458139.094352	43.302490
3503.009537	458098.765386	43.307495
3502.377172	458068.756393	43.312500
3502.949252	458036.839494	43.317505
3502.827217	458007.762997	43.322509
3502.328038	457974.848864	43.327514
3502.553725	457940.405041	43.332519
3502.364434	457911.490652	43.337524
3502.663502	457882.955630	43.342529
3502.188868	457851.555482	43.347533
3502.347183	457822.738656	43.352538
3502.580905	457788.799297	43.357543
3502.174151	457765.585873	43.362548
3502.350674	457735.248021	43.367553
3502.187367	457711.946040	43.372557
3502.596134	457679.497280	43.377562
3502.850308	457652.638728	43.382567
3502.472054	457631.748378	43.387572
3502.554963	457579.261143	43.392577
3502.402990	457558.588503	43.397581
3502.211096	457524.411245	43.402586
3502.265657	457494.597976	43.407591
3502.348645	457475.103130	43.412596
3502.315104	457447.884214	43.417601
3502.342641	457425.007573	43.422605
3502.144585	457404.898550	43.427610
3502.138397	457366.593270	43.432615
3502.252429	457346.081394	43.437620
3502.488928	457309.205704	43.442625
3502.359876	457281.950788	43.447629
3502.062377	457260.946218	43.452634
3502.618306	457238.644948	43.457639
3502.616509	457211.623135	43.462644
3502.180916	457178.039754	43.467649
3502.165426	457148.742826	43.472653
3502.271826	457130.407829	43.477658
3502.736067	457093.445640	43.482663
3502.585347	457068.521524	43.487668
3502.689745	457024.530678	43.492673
3502.760578	456998.812930	43.497677
3502.427943	456966.073382	43.502682
3502.459517	456933.378306	43.507687
3502.603081	456912.254077	43.512692
3502.538918	456872.995255	43.517697
3502.514870	456834.640980	43.522701
3502.648544	456819.337670	43.527706
3502.870218	456783.323448	43.532711
3502.533770	456752.102225	43.537716
3502.583927	456716.266369	43.542721
3502.655727	456692.977042	43.547725
3502.519870	456650.540779	43.552730
3502.611458	456631.296677	43.557735
3502.599243	456600.682591	43.562740
3502.618234	456555.641148	43.567745
3502.373889	456528.656020	43.572749
3502.494573	456505.308231	43.577754
3502.630883	456470.774201	43.582759
3502.696709	456444.600967	43.587764
3502.525212	456409.760477	43.592769
3502.940067	456381.711037	43.597773
3502.544806	456346.854637	43.602778
3502.526600	456310.775558	43.607783
3502.467341	456282.647920	43.612788
3502.295347	456239.204164	43.617793
3502.874522	456220.136764	43.622797
3502.630900	456186.470991	43.627802
3502.723365	456153.258918	43.632807
3502.627197	456123.922218	43.637812
3502.342087	456094.716083	43.642817
3502.548705	456067.002182	43.647821
3502.686079	456026.849786	43.652826
3502.439195	455996.220552	43.657831
3502.401441	455979.171948	43.662836
3502.411130	455939.646503	43.667841
3502.456739	455910.287382	43.672845
3502.139080	455890.347043	43.677850
3502.582051	455857.535329	43.682855
3502.202860	455830.671320	43.687860
3502.547219	455790.941639	43.692865
3502.705710	455768.750952	43.697869
3502.273698	455736.733066	43.702874
3502.346462	455704.535356	43.707879
3502.486323	455678.602495	43.712884
3502.348680	455651.953662	43.717889
3502.138473	455618.635851	43.722893
3502.330555	455592.947775	43.727898
3502.941427	455563.702544	43.732903
3502.661499	455541.579793	43.737908
3502.287431	455509.704299	43.742913
3502.383928	455480.640188	43.747917
3502.308916	455449.122912	43.752922
3502.285720	455422.152271	43.757927
3502.223587	455405.005685	43.762932
3502.537056	455365.988367	43.767937
3502.529471	455333.093960	43.772941
3502.216283	455310.318180	43.777946
3502.489394	455279.606776	43.782951
3502.558782	455248.927019	43.787956
3502.458607	455218.880903	43.792961
3502.271880	455189.202467	43.797965
3502.348543	455164.037816	43.802970
3502.368505	455129.266202	43.807975
3502.429129	455103.901524	43.812980
3502.704889	455070.507049	43.817985
3502.472574	455053.487821	43.822989
3502.601923	455021.533101	43.827994
3503.032631	454985.330828	43.832999
3502.670861	454950.668873	43.838004
3502.201630	454905.850993	43.843009
3502.380235	454894.031091	43.848013
3502.202708	454862.528715	43.853018
3502.323070	454837.204965	43.858023
3502.413955	454805.407669	43.863028
3502.340404	454773.585292	43.868033
3502.371336	454755.259554	43.873037
3502.372417	454728.587733	43.878042
3502.213407	454702.801161	43.883047
3502.236710	454661.347522	43.888052
3502.236609	454634.422689	43.893057
3501.942868	454618.121146	43.898061
3502.170053	454588.529118	43.903066
3502.088003	454563.236473	43.908071
3502.109470	454545.519320	43.913076
3501.931916	454521.051250	43.918081
3502.044820	454493.197618	43.923085
3501.824052	454472.278979	43.928090
3502.151791	454444.847340	43.933095
3502.063491	454428.564263	43.938100
3501.914476	454404.597703	43.943105
3502.264272	454382.780390	43.948109
3502.032256	454364.292718	43.953114
3502.626791	454329.328891	43.958119
3502.115820	454304.305065	43.963124
3502.306159	454275.123138	43.968129
3502.293535	454247.946605	43.973133
3502.221789	454224.726953	43.978138
3502.432492	454197.566201	43.983143
3502.156034	454168.507349	43.988148
3501.871822	454134.894569	43.993153
3502.196410	454115.510228	43.998157
3501.860547	454090.104564	44.003162
3502.398613	454067.751443	44.008167
3501.952249	454048.740060	44.013172
3502.111809	454025.281701	44.018177
3502.354454	453990.068288	44.023181
3501.938839	453975.860228	44.028186
3502.068801	453947.041442	44.033191
3502.053607	453926.748129	44.038196
3502.393314	453900.680325	44.043201
3502.110405	453881.035972	44.048205
3501.875501	453860.473096	44.053210
3502.278277	453822.551949	44.058215
3502.368499	453806.038065	44.063220
3502.193482	453777.367688	44.068225
3502.143264	453753.840387	44.073229
3502.006090	453731.490691	44.078234
3502.362535	453698.992105	44.083239
3502.591518	453680.634432	44.088244
3502.687976	453642.051978	44.093249
3502.614461	453618.882418	44.098253
3502.393641	453586.726522	44.103258
3502.437354	453561.159803	44.108263
3502.033133	453528.526204	44.113268
3502.243750	453492.810647	44.118273
3502.287195	453473.013827	44.123277
3501.929026	453453.836236	44.128282
3501.953765	453415.618747	44.133287
3502.023859	453408.825537	44.138292
3502.081262	453377.688864	44.143297
3502.215476	453355.195233	44.148301
3502.072258	453334.465634	44.153306
3502.312358	453309.576592	44.158311
3502.205363	453294.915041	44.163316
3501.952245	453260.182239	44.168321
3502.237460	453235.792219	44.173325
3501.949299	453213.566593	44.178330
3502.394468	453186.823339	44.183335
3502.348013	453161.877451	44.188340
3502.355484	453127.660602	44.193345
3502.101566	453099.760629	44.198349
3501.841488	453078.947685	44.203354
3502.458077	453053.088625	44.208359
3502.699954	453029.008756	44.213364
3502.179928	453000.289577	44.218369
3502.542102	452965.055527	44.223373
3502.157394	452941.376736	44.228378
3502.490463	452916.371445	44.233383
3502.283948	452893.120400	44.238388
3501.997347	452859.050026	44.243393
3502.375882	452825.989630	44.248397
3502.201913	452803.948184	44.253402
3502.444299	452786.701051	44.258407
3502.300625	452752.051454	44.263412
3501.994633	452722.741741	44.268417
3502.348693	452694.139127	44.273421
3501.953128	452677.345474	44.278426
3502.103008	452656.670704	44.283431
3502.097774	452633.033683	44.288436
3502.268360	452611.950709	44.293441
3502.146845	452579.220751	44.298445
3501.987505	452561.074199	44.303450
3502.099967	452532.357070	44.308455
3502.173288	452506.024973	44.313460
3502.330549	452480.185943	44.318465
3502.234328	452464.914628	44.323469
3502.119613	452439.522796	44.328474
3502.239329	452405.894493	44.333479
3502.120511	452380.857535	44.338484
3502.140401	452357.570557	44.343489
3502.510073	452323.042710	44.348493
3502.413687	452295.015722	44.353498
3502.624303	452266.282891	44.358503
3502.136422	452247.427882	44.363508
3502.000148	452210.194586	44.368513
3502.139076	452193.975330	44.373517
3501.753416	452169.587010	44.378522
3502.109492	452143.058522	44.383527
3502.014251	452128.444797	44.388532
3501.568278	452102.547236	44.393537
3501.648018	452072.973954	44.398541
3501.619132	452065.233893	44.403546
3502.037828	452039.960958	44.408551
3501.795309	452016.309423	44.413556
3501.687594	452004.835861	44.418561
3501.721033	451981.495665	44.423565
3501.997888	451976.441372	44.428570
3501.727717	451950.516232	44.433575
3501.625699	451935.498456	44.438580
3501.765910	451907.990844	44.443585
3501.834883	451891.225396	44.448589
3501.476799	451872.754738	44.453594
3501.869184	451857.356250	44.458599
3501.824141	451843.544376	44.463604
3501.452964	451812.876604	44.468609
3501.797410	451804.369672	44.473613
3501.721693	451789.094586	44.478618
3501.857167	451763.207288	44.483623
3501.620292	451761.421864	44.488628
3501.631069	451730.188324	44.493633
3501.698057	451715.650253	44.498637
3501.502815	451693.408264	44.503642
3501.983591	451676.578533	44.508647
3501.748666	451652.571000	44.513652
3501.800844	451630.138573	44.518657
3501.878466	451613.523376	44.523661
3501.673135	451590.523540	44.528666
3501.673034	451570.579521	44.533671
3501.659701	451563.140538	44.538676
3501.909938	451545.890984	44.543681
3501.861094	451523.980339	44.548685
3501.478951	451499.539933	44.553690
3501.349066	451495.763669	44.558695
3501.840642	451474.781260	44.563700
3501.617789	451444.950307	44.568705
3501.882206	451429.875083	44.573709
3501.845342	451407.557473	44.578714
3502.010650	451383.942876	44.583719
3501.609858	451371.502114	44.588724
3501.737475	451356.093776	44.593729
3501.914758	451331.211747	44.598733
3501.700339	451315.046678	44.603738
3501.828162	451292.247715	44.608743
3501.770504	451272.261700	44.613748
3501.818172	451254.486564	44.618753
3502.055190	451236.631326	44.623757
3501.835316	451233.122111	44.628762
3502.177766	451195.457859	44.633767
3501.873356	451179.559773	44.638772
3501.535656	451147.367032	44.643777
3501.898210	451137.540831	44.648781
3501.732462	451116.508429	44.653786
3502.139509	451083.997199	44.658791
3501.613410	451074.410491	44.663796
3501.675898	451054.911744	44.668801
3501.862545	451040.961954	44.673805
3501.492215	451025.175231	44.678810
3501.899047	451006.179677	44.683815
3501.835368	450991.256383	44.688820
3501.530115	450968.321915	44.693825
3502.154368	450948.938120	44.698829
3501.701657	450924.305423	44.703834
3501.781229	450903.791429	44.708839
3501.996120	450884.825616	44.713844
3501.764739	450853.729470	44.718849
3502.216669	450832.651237	44.723853
3501.936261	450814.116774	44.728858
3501.811047	450799.253516	44.733863
3501.865137	450786.083480	44.738868
3501.708925	450759.936391	44.743873
3502.073886	450741.807642	44.748877
3502.018779	450727.186524	44.753882
3501.964862	450710.185983	44.758887
3502.069115	450677.822379	44.763892
3501.860611	450655.935516	44.768897
3502.111747	450623.802068	44.773901
3502.140715	450603.295605	44.778906
3501.950902	450575.432324	44.783911
3501.990687	450571.680083	44.788916
3501.542836	450552.158960	44.793921
3501.955873	450528.605931	44.798925
3501.998540	450511.235816	44.803930
3502.147653	450483.370273	44.808935
3501.860469	450460.938568	44.813940
3501.534363	450446.561881	44.818945
3502.128192	450402.529026	44.823949
3501.914127	450400.486800	44.828954
3501.880263	450373.915128	44.833959
3502.142447	450362.433572	44.838964
3501.909849	450340.752565	44.843969
3502.265822	450303.084336	44.848973
3501.927549	450280.761602	44.853978
3502.070136	450255.478495	44.858983
3501.682045	450231.594135	44.863988
3501.764305	450210.066467	44.868993
3501.930135	450191.512542	44.873997
3502.057339	450183.038651	44.879002
3501.754178	450150.686872	44.884007
3502.179921	450142.723363	44.889012
3502.009791	450111.262034	44.894017
3501.896912	450098.775581	44.899021
3501.910821	450078.726474	44.904026
3502.036362	450044.789086	44.909031
3501.861129	450028.768628	44.914036
3501.806404	450009.894471	44.919041
3502.115527	449991.773656	44.924045
3502.011470	449959.896790	44.929050
3502.183665	449933.849265	44.934055
3502.136339	449923.731818	44.939060
3502.009881	449895.655126	44.944065
3501.665847	449878.749567	44.949069
3501.622669	449855.975391	44.954074
3501.772597	449842.182258	44.959079
3501.731209	449829.785742	44.964084
3501.526970	449801.113514	44.969089
3502.106958	449785.633435	44.974093
3501.595240	449769.968854	44.979098
3501.579140	449748.000318	44.984103
3502.118142	449731.615329	44.989108
3501.987770	449716.600104	44.994113
3502.121759	449679.724484	44.999117
3501.671523	449667.593977	45.004122
3502.048307	449645.007306	45.009127
3502.069054	449619.134768	45.014132
3501.775364	449601.866740	45.019137
3501.776696	449573.820285	45.024141
3501.645839	449558.906254	45.029146
3501.711019	449542.746701	45.034151
3502.003892	449527.462956	45.039156
3501.710186	449504.119817	45.044161
3501.835794	449487.495185	45.049165
3501.742535	449469.790839	45.054170
3501.804144	449441.582923	45.059175
3501.457834	449425.740425	45.064180
3501.630560	449409.969022	45.069185
3501.748992	449394.611058	45.074189
3501.662094	449365.059242	45.079194
3501.769865	449351.829176	45.084199
3501.928463	449333.781751	45.089204
3501.523038	449322.757803	45.094209
3502.014500	449300.254107	45.099213
3501.714465	449278.227931	45.104218
3501.844620	449258.615455	45.109223
3502.021859	449234.692424	45.114228
3501.256669	449230.457656	45.119233
3501.987596	449193.133769	45.124237
3501.650990	449177.947683	45.129242
3501.586132	449170.616978	45.134247
3501.475725	449147.953620	45.139252
3501.463890	449141.880308	45.144257
3501.840992	449128.253784	45.149261
3501.618636	449095.685029	45.154266
3501.905122	449084.452012	45.159271
3501.557416	449067.039997	45.164276
3501.973397	449057.659991	45.169281
3501.755599	449038.658313	45.174285
3501.622451	449015.238930	45.179290
3501.580049	448997.019940	45.184295
3501.726471	448977.151494	45.189300
3501.740796	448961.505602	45.194305
3501.691790	448938.174279	45.199309
3501.615208	448923.757544	45.204314
3501.938369	448898.495063	45.209319
3502.024444	448883.293580	45.214324
3502.099868	448864.094209	45.219329
3502.300598	448834.193004	45.224333
3501.932156	448812.885683	45.229338
3501.972682	448782.351169	45.234343
3501.733700	448761.226151	45.239348
3501.635745	448743.319314	45.244353
3502.013229	448736.780265	45.249357
3501.489458	448706.839708	45.254362
3501.983847	448695.928490	45.259367
3501.821055	448682.942548	45.264372
3501.666135	448657.703498	45.269377
3501.825547	448642.389146	45.274381
3501.665648	448613.151226	45.279386
3501.853606	448607.046644	45.284391
3501.736186	448587.066944	45.289396
3501.673552	448570.926412	45.294401
3501.825594	448539.817229	45.299405
3501.647882	448528.757359	45.304410
3501.948585	448506.535503	45.309415
3501.553036	448483.611916	45.314420
3501.411163	448475.027211	45.319425
3501.906163	448455.914000	45.324429
3501.531573	448454.757209	45.329434
3501.801546	448430.312402	45.334439
3501.787165	448397.051858	45.339444
3501.610362	448387.662494	45.344449
3501.724638	448364.912563	45.349453
3501.624261	448349.233363	45.354458
3501.485628	448334.167644	45.359463
3501.506962	448311.482737	45.364468
3501.477458	448303.234865	45.369473
3501.817266	448288.297171	45.374477
3501.823615	448280.752510	45.379482
3502.270601	448257.343127	45.384487
3501.884308	448233.354579	45.389492
3501.631313	448207.978277	45.394497
3501.899784	448177.812304	45.399501
3502.251048	448164.391593	45.404506
3501.726448	448136.981670	45.409511
3501.733967	448127.968521	45.414516
3501.547150	448106.328330	45.419521
3501.883815	448081.973934	45.424525
3501.819111	448070.845569	45.429530
3501.708064	448052.079389	45.434535
3501.787954	448040.523470	45.439540
3501.537582	448004.666205	45.444545
3501.818680	447993.737128	45.449549
3501.610952	447968.555965	45.454554
3501.931358	447953.165350	45.459559
3501.750619	447938.561520	45.464564
3501.762393	447917.548386	45.469569
3501.908045	447897.476358	45.474573
3501.719300	447886.670961	45.479578
3501.803037	447859.570990	45.484583
3501.574502	447835.000437	45.489588
3501.028568	447817.111766	45.494593
3501.745174	447813.658670	45.499597
3501.686333	447800.402769	45.504602
3501.770478	447788.187838	45.509607
3501.738588	447772.497482	45.514612
3501.733965	447747.638817	45.519617
3501.300786	447730.188184	45.524621
3501.594046	447722.851796	45.529626
3501.845708	447700.130283	45.534631
3501.629597	447687.354445	45.539636
3501.629223	447660.976091	45.544641
3501.594268	447643.564668	45.549645
3501.511241	447635.932386	45.554650
3501.682373	447612.008164	45.559655
3501.757393	447604.958842	45.564660
3501.438423	447575.440218	45.569665
3501.916250	447547.924043	45.574669
3501.414488	447542.888417	45.579674
3501.688456	447517.429148	45.584679
3501.741029	447515.142575	45.589684
3501.802039	447496.855355	45.594689
3502.071424	447472.713138	45.599693
3501.548928	447460.288602	45.604698
3501.777662	447435.443828	45.609703
3501.880051	447415.529895	45.614708
3501.549508	447393.455540	45.619713
3501.985401	447387.868910	45.624717
3501.910863	447360.640933	45.629722
3501.795895	447342.735360	45.634727
3502.016565	447324.423121	45.639732
3501.966461	447298.051980	45.644737
3502.070306	447265.631700	45.649741
3501.921813	447257.199343	45.654746
3501.784889	447229.120141	45.659751
3501.910088	447220.290756	45.664756
3501.971967	447197.648782	45.669761
3501.947412	447169.906425	45.674765
3501.761730	447156.467265	45.679770
3501.899274	447140.395575	45.684775
3501.649137	447127.624638	45.689780
3501.732780	447098.093219	45.694785
3501.719651	447078.905741	45.699789
3501.510753	447066.533399	45.704794
3501.689116	447045.594598	45.709799
3502.155518	447032.205771	45.714804
3501.802137	447013.931918	45.719809
3501.833595	446989.319764	45.724813
3501.349691	446976.483833	45.729818
3501.697606	446957.543838	45.734823
3501.843830	446919.749320	45.739828
3501.783422	446860.771833	45.744833
3501.607162	446737.761629	45.749837
3501.269900	446586.927323	45.754842
3500.840726	446379.142989	45.759847
3501.014845	446120.678470	45.764852
3500.632844	445829.890183	45.769857
3499.633019	445476.657543	45.774861
3498.971713	445097.185873	45.779866
3498.545604	444662.574985	45.784871
3498.050293	444204.113231	45.789876
3497.175201	443684.321983	45.794881
3496.570658	443118.946137	45.799885
3495.446211	442522.133115	45.804890
3494.019244	441864.775154	45.809895
3493.228749	441175.842520	45.814900
3492.044640	440455.897316	45.819905
3491.190742	439686.183434	45.824909
3489.725983	438892.523090	45.829914
3488.251697	438041.183874	45.834919
3486.855317	437165.782120	45.839924
3485.420613	436262.381195	45.844929
3483.869677	435304.492290	45.849933
3482.359568	434320.810914	45.854938
3481.025700	433289.980629	45.859943
3479.380776	432229.703850	45.864948
3477.361043	431142.773103	45.869953
3475.561880	430013.381599	45.874957
3473.723341	428851.141492	45.879962
3471.681726	427665.094555	45.884967
3469.380721	426441.408290	45.889972
3467.651359	425195.305957	45.894977
3466.038113	423921.988288	45.899981
3463.625496	422618.196525	45.904986
3461.404675	421275.405748	45.909991
3459.388754	419910.136032	45.914996
3457.072217	418522.563676	45.920001
3454.783344	417099.804318	45.925005
3452.084685	415656.829263	45.930010
3450.162618	414193.095514	45.935015
3447.411140	412698.959155	45.940020
3444.937740	411183.372586	45.945025
3442.252564	409655.387133	45.950029
3439.395748	408107.131618	45.955034
3436.633651	406523.036617	45.960039
3434.511550	404935.736540	45.965044
3431.580424	403322.775851	45.970049
3428.868957	401691.804772	45.975053
3426.144489	400045.089711	45.980058
3423.445224	398375.111167	45.985063
3420.674348	396688.021856	45.990068
3417.552454	394993.304058	45.995073
3414.899152	393265.752875	46.000077
3411.630703	391535.686635	46.005082
3408.672016	389791.361154	46.010087
3405.517126	388025.415110	46.015092
3402.522733	386249.011594	46.020097
3399.651789	384462.993462	46.025101
3395.833791	382667.069646	46.030106
3393.014454	380860.073324	46.035111
3390.170087	379040.486881	46.040116
3386.855598	377200.530639	46.045121
3383.719602	375371.646915	46.050125
3380.376137	373523.697797	46.055130
3376.738866	371653.290465	46.060135
3373.977666	369774.415614	46.065140
3370.658870	367895.908991	46.070145
3367.134151	366013.601531	46.075149
3363.882149	364114.283009	46.080154
3360.632845	362201.881736	46.085159
3357.340688	360284.688540	46.090164
3353.640669	358364.031773	46.095169
3350.262049	356433.572171	46.100173
3346.928526	354505.476804	46.105178
3343.286673	352561.424989	46.110183
3340.109725	350613.370035	46.115188
3336.263917	348660.981061	46.120193
3332.977215	346689.602071	46.125197
3329.380588	344729.037808	46.130202
3325.612311	342769.455897	46.135207
3322.214200	340789.592669	46.140212
3318.603387	338833.555365	46.145217
3315.050512	336851.590804	46.150221
3311.230629	334880.089555	46.155226
3307.724883	332886.155780	46.160231
3304.002918	330903.952844	46.165236
3300.137994	328932.506522	46.170241
3296.842623	326948.841439	46.175245
3292.768246	324958.407888	46.180250
3289.263089	322973.818583	46.185255
3285.749854	320982.038676	46.190260
3281.975296	318993.794154	46.195265
3278.126452	316999.237281	46.200269
3274.124161	315012.070495	46.205274
3271.055699	313026.275077	46.210279
3267.156386	311022.610351	46.215284
3263.324054	309037.657021	46.220289
3259.589425	307038.713223	46.225293
3255.697493	305060.990125	46.230298
3252.053673	303057.676530	46.235303
3248.641485	301066.925720	46.240308
3244.418349	299086.688931	46.245313
3241.003997	297078.868194	46.250317
3237.048114	295092.442787	46.255322
3232.916867	293109.414106	46.260327
3229.383180	291134.398899	46.265332
3225.693079	289148.373834	46.270337
3221.655777	287156.664616	46.275341
3217.639581	285187.422905	46.280346
3213.773235	283225.280854	46.285351
3209.999811	281242.982667	46.290356
3205.966956	279288.550377	46.295361
3202.460769	277313.897530	46.300365
3198.534218	275360.648509	46.305370
3194.703580	273409.120607	46.310375
3191.029942	271455.563263	46.315380
3186.685618	269499.012055	46.320385
3183.336476	267557.823308	46.325389
3178.899226	265614.295346	46.330394
3175.285378	263671.722872	46.335399
3171.204741	261733.822691	46.340404
3167.194928	259815.588721	46.345409
3163.808030	257879.452003	46.350413
3159.920616	255964.984570	46.355418
3155.784429	254037.184294	46.360423
3152.169161	252125.627018	46.365428
3148.065820	250230.090084	46.370433
3144.574856	248317.576885	46.375437
3140.399546	246421.016421	46.380442
3136.106649	244511.747570	46.385447
3132.257193	242613.395265	46.390452
3128.148457	240729.763720	46.395457
3124.731552	238850.315722	46.400461
3120.726662	236979.658218	46.405466
3116.977498	235109.613518	46.410471
3112.719342	233241.040832	46.415476
3108.752533	231390.626748	46.420481
3104.633061	229529.789419	46.425485
3100.804796	227701.274768	46.430490
3096.896463	225868.594075	46.435495
3092.921394	224037.299020	46.440500
3088.924479	222210.746030	46.445505
3084.888308	220398.515625	46.450509
3080.707381	218602.739512	46.455514
3076.714809	216802.100670	46.460519
3073.059640	215012.648140	46.465524
3068.862753	213226.828471	46.470529
3065.121341	211451.873669	46.475533
3060.998633	209683.483647	46.480538
3056.838241	207915.850372	46.485543
3053.040793	206161.341157	46.490548
3049.242723	204429.156468	46.495553
3044.965486	202686.161960	46.500557
3040.909700	200955.578120	46.505562
3036.991479	199246.790704	46.510567
3032.768540	197537.713124	46.515572
3028.397436	195843.296424	46.520577
3024.445243	194145.677782	46.525581
3020.670686	192471.456698	46.530586
3016.655368	190802.185249	46.535591
3012.394118	189136.057166	46.540596
3008.368847	187487.997047	46.545601
3004.397801	185839.571973	46.550605
3000.352906	184216.393999	46.555610
2996.182464	182596.598044	46.560615
2992.080868	180980.256582	46.565620
2988.110710	179388.316255	46.570625
2983.637238	177796.788566	46.575629
2979.471194	176216.063887	46.580634
2975.461865	174657.012384	46.585639
2971.047563	173106.163462	46.590644
2966.351715	171578.519703	46.595649
2962.448847	170058.574087	46.600653
2957.889799	168556.150505	46.605658
2953.595905	167073.332934	46.610663
2949.475194	165604.432702	46.615668
2944.663627	164151.200687	46.620673
2940.805172	162711.344267	46.625677
2936.189386	161292.308084	46.630682
2931.597287	159898.335553	46.635687
2927.339168	158514.066207	46.640692
2922.407724	157159.269409	46.645697
2917.865719	155817.169777	46.650701
2912.270227	154505.859756	46.655706
2907.571371	153220.631032	46.660711
2903.029524	151966.827853	46.665716
2898.111788	150739.046708	46.670721
2893.196399	149529.452180	46.675725
2887.822477	148360.829680	46.680730
2882.751812	147151.122624	46.685735
2877.682311	146026.316793	46.690740
2872.177657	144954.918460	46.695745
2867.303603	143910.992407	46.700749
2862.080854	142902.311167	46.705754
2857.253980	141921.911687	46.710759
2852.461531	140963.321678	46.715764
2847.289433	140050.638402	46.720769
2842.946714	139141.431421	46.725773
2838.478696	138279.640476	46.730778
2833.757057	137422.052435	46.735783
2829.539817	136598.904290	46.740788
2825.126851	135786.716834	46.745793
2821.231548	134998.011240	46.750797
2817.049314	134230.583573	46.755802
2813.242185	133474.458127	46.760807
2809.492182	132727.648546	46.765812
2805.313579	131999.554415	46.770817
2801.620306	131273.444980	46.775821
2797.831197	130561.876673	46.780826
2793.478414	129859.401097	46.785831
2789.963458	129173.393630	46.790836
2786.003739	128490.697362	46.795841
2782.330780	127813.373422	46.800845
2778.905207	127153.231334	46.805850
2775.210789	126492.174977	46.810855
2772.409560	125833.979234	46.815860
2768.190832	125176.523461	46.820865
2764.967080	124524.252606	46.825869
2761.239732	123875.746301	46.830874
2757.770491	123232.488386	46.835879
2754.365709	122590.769731	46.840884
2750.486362	121954.769320	46.845889
2746.833322	121324.174393	46.850893
2743.445621	120699.957909	46.855898
2739.729626	120067.841654	46.860903
2736.585451	119443.340519	46.865908
2732.934291	118816.486861	46.870913
2729.374951	118192.045374	46.875917
2725.696601	117581.633344	46.880922
2722.056014	116962.731003	46.885927
2718.415009	116352.625634	46.890932
2714.632291	115748.986453	46.895937
2710.803157	115134.963108	46.900941
2707.162170	114546.109634	46.905946
2703.034655	113958.472993	46.910951
2699.623671	113371.141213	46.915956
2695.277512	112796.386693	46.920961
2692.114401	112217.363198	46.925965
2688.010736	111656.511492	46.930970
2684.127089	111089.201075	46.935975
2680.560484	110537.615543	46.940980
2676.163016	109991.660221	46.945985
2672.598101	109455.233326	46.950989
2668.965960	108914.439055	46.955994
2664.887459	108373.735365	46.960999
2661.082264	107856.287529	46.966004
2657.272531	107344.594290	46.971009
2653.595945	106833.358321	46.976013
2649.887467	106331.338659	46.981018
2646.461858	105829.905276	46.986023
2642.782693	105324.247567	46.991028
2638.869064	104825.701642	46.996033
2635.745426	104325.946983	47.001037
2632.398430	103841.462738	47.006042
2628.533942	103361.413288	47.011047
2625.324832	102856.685757	47.016052
2622.002347	102373.909675	47.021057
2618.758366	101888.789703	47.026061
2615.036202	101402.480279	47.031066
2611.635514	100909.772956	47.036071
2608.543011	100405.090418	47.041076
2604.931265	99920.603491	47.046081
2601.423471	99426.295817	47.051085
2598.451075	98935.242296	47.056090
2594.692351	98435.168013	47.061095
2591.184833	97930.271166	47.066100
2587.617763	97441.303082	47.071105
2584.087177	96939.399470	47.076109
2581.054266	96448.393787	47.081114
2577.395996	95939.078850	47.086119
2574.459418	95432.709821	47.091124
2570.571770	94938.836331	47.096129
2567.104324	94433.684469	47.101133
2563.967081	93927.078949	47.106138
2560.185929	93424.622858	47.111143
2556.856870	92917.364929	47.116148
2553.398591	92410.008458	47.121153
2549.881492	91898.908448	47.126157
2546.869959	91398.373599	47.131162
2542.860440	90880.315383	47.136167
2539.700886	90373.149856	47.141172
2536.283578	89866.503129	47.146177
2532.399011	89350.675399	47.151181
2529.546749	88826.374003	47.156186
2525.946649	88317.711130	47.161191
2522.728506	87795.085780	47.166196
2519.266910	87274.362472	47.171201
2515.757312	86743.466972	47.176205
2512.556935	86231.220809	47.181210
2508.790729	85699.634714	47.186215
2505.820363	85167.566113	47.191220
2501.920384	84633.492399	47.196225
2498.730611	84099.648365	47.201229
2495.312066	83570.943775	47.206234
2491.679417	83039.322559	47.211239
2488.405024	82506.740950	47.216244
2484.569028	81967.334017	47.221249
2481.039342	81427.597581	47.226253
2477.521235	80902.146510	47.231258
2473.845912	80370.671127	47.236263
2470.497325	79822.694137	47.241268
2466.957019	79296.489279	47.246273
2463.465026	78744.936089	47.251277
2460.094884	78220.058824	47.256282
2456.446215	77686.281203	47.261287
2453.133228	77141.476190	47.266292
2449.464702	76609.513390	47.271297
2446.190241	76062.514192	47.276301
2442.356276	75518.610145	47.281306
2439.178053	74984.545664	47.286311
2435.867916	74440.302485	47.291316
2431.979241	73906.052553	47.296321
2428.706940	73365.330153	47.301325
2425.368564	72815.486450	47.306330
2421.874067	72277.017544	47.311335
2418.304589	71713.430242	47.316340
2414.751592	71180.770188	47.321345
2411.211086	70630.635281	47.326349
2407.828164	70083.350538	47.331354
2404.361114	69533.582846	47.336359
2400.862864	68991.271610	47.341364
2397.403949	68438.504209	47.346369
2393.796229	67884.267395	47.351373
2390.541903	67338.874295	47.356378
2387.089859	66786.198532	47.361383
2383.890204	66228.398511	47.366388
2380.538566	65691.097964	47.371393
2376.841779	65120.533777	47.376397
2373.042859	64560.134519	47.381402
2369.502625	64002.385865	47.386407
2366.414979	63439.711280	47.391412
2362.866679	62882.744115	47.396417
2359.585980	62321.394139	47.401421
2356.136679	61760.927168	47.406426
2352.528159	61189.963130	47.411431
2349.298868	60618.515448	47.416436
2345.291651	60058.351763	47.421441
2341.495687	59491.168756	47.426445
2338.099354	58930.358447	47.431450
2334.602014	58366.201067	47.436455
2331.106998	57805.768448	47.441460
2327.623482	57238.507059	47.446465
2324.301244	56681.309733	47.451469
2320.663336	56117.055638	47.456474
2317.353454	55564.006548	47.461479
2314.143282	54985.913073	47.466484
2310.724007	54419.121094	47.471489
2307.229043	53843.459942	47.476493
2303.603199	53270.059988	47.481498
2300.243175	52703.490410	47.486503
2296.830635	52124.616877	47.491508
2293.483263	51552.497132	47.496513
2289.941680	50977.985832	47.501517
2286.151260	50399.404402	47.506522
2282.669229	49818.322027	47.511527
2279.543956	49238.949462	47.516532
2275.917156	48655.559476	47.521537
2272.463488	48080.117420	47.526541
2269.041677	47496.128988	47.531546
2265.300140	46914.685176	47.536551
2262.268047	46329.397713	47.541556
2258.393484	45749.945288	47.546561
2254.966294	45164.679841	47.551565
2251.733657	44576.532997	47.556570
2247.866377	43991.195537	47.561575
2244.375138	43403.132594	47.566580
2241.001221	42821.477862	47.571585
2237.354526	42234.351576	47.576589
2233.974215	41653.616358	47.581594
2230.060193	41071.090055	47.586599
2227.100673	40485.260486	47.591604
2223.300356	39902.652531	47.596609
2219.756134	39317.953455	47.601613
2216.397203	38733.241314	47.606618
2212.680722	38143.706340	47.611623
2209.854931	37552.235762	47.616628
2205.879586	36965.157071	47.621633
2202.292040	36368.582325	47.626637
2198.389335	35789.474045	47.631642
2194.927119	35210.686980	47.636647
2191.754955	34622.013864	47.641652
2188.102995	34039.599216	47.646657
2184.378761	33452.863796	47.651661
2181.056548	32869.238622	47.656666
2177.635943	32290.195723	47.661671
2173.611053	31703.549779	47.666676
2170.490729	31120.670925	47.671681
2166.603862	30537.667903	47.676685
2163.242703	29960.689653	47.681690
2159.477764	29394.449438	47.686695
2156.395828	28809.348469	47.691700
2152.668076	28230.517712	47.696705
2149.159889	27657.505183	47.701709
2145.666158	27075.204664	47.706714
2141.829976	26511.856109	47.711719
2138.368573	25931.009060	47.716724
2134.590064	25359.155315	47.721729
2130.963953	24785.805207	47.726733
2127.091988	24225.351828	47.731738
2123.540798	23655.754002	47.736743
2120.265998	23096.899185	47.741748
2116.482288	22541.826220	47.746753
2112.678621	21984.820765	47.751757
2108.842990	21439.073594	47.756762
2104.513413	20897.162054	47.761767
2100.537017	20370.887828	47.766772
2096.086357	19855.032473	47.771777
2092.248217	19342.268701	47.776781
2088.745027	18844.718034	47.781786
2084.117077	18357.552273	47.786791
2080.331470	17864.903185	47.791796
2076.342227	17390.034763	47.796801
2072.642308	16918.115898	47.801805
2068.958024	16462.694142	47.806810
2064.947328	16007.403623	47.811815
2061.191119	15558.470840	47.816820
2057.412474	15110.837578	47.821825
2053.697353	14660.979066	47.826829
2049.855870	14227.640068	47.831834
2046.048777	13794.935632	47.836839
2042.301997	13370.754525	47.841844
2038.775649	12953.434491	47.846849
2035.326503	12544.162422	47.851853
2031.596089	12120.570322	47.856858
2028.157314	11731.075132	47.861863
2024.564216	11321.399326	47.866868
2020.734024	10922.497526	47.871873
2017.086364	10540.859548	47.876877
2013.463482	10144.430170	47.881882
2009.546863	9759.994769	47.886887
2005.818710	9399.116478	47.891892
2001.633266	9041.962749	47.896897
1997.274836	8690.802902	47.901901
1993.500524	8343.091111	47.906906
1989.013837	8027.676199	47.911911
1985.226064	7702.447570	47.916916
1981.231249	7394.632658	47.921921
1977.342337	7084.182685	47.926925
1973.556839	6787.748608	47.931930
1969.443299	6507.564811	47.936935
1965.720093	6233.106613	47.941940
1961.822890	5955.869326	47.946945
1958.285872	5678.406131	47.951949
1954.695082	5417.323052	47.956954
1950.685861	5158.609498	47.961959
1947.512377	4910.345496	47.966964
1943.572686	4658.238997	47.971969
1940.274134	4409.406376	47.976973
1936.881399	4168.642125	47.981978
1933.675277	3925.535701	47.986983
1930.315750	3677.421951	47.991988
1926.729418	3446.953064	47.996993
1923.389769	3197.390399	48.001997
1919.667216	2959.721777	48.007002
1916.009971	2711.838508	48.012007
1912.600393	2481.810097	48.017012
1909.182138	2251.083553	48.022017
1905.201732	2027.873493	48.027021
1902.369819	1785.731213	48.032026
1898.618536	1575.175649	48.037031
1894.785305	1347.417196	48.042036
1891.036925	1133.072835	48.047041
1886.787153	909.523171	48.052045
1883.424092	705.121766	48.057050
1879.364550	511.898015	48.062055
1875.305421	320.175918	48.067060
1870.739740	153.891927	48.072065
1863.601038	77.204098	48.077069
1853.718130	90.492246	48.082074
1846.717549	97.235337	48.087079
1842.932362	85.871958	48.092084
1839.862831	79.886233	48.097089
1836.781140	84.038916	48.102093
1834.926851	88.788333	48.107098
1832.119529	89.633370	48.112103
1829.602769	89.727677	48.117108
1826.699881	91.153892	48.122113
1823.564643	90.366873	48.127117
1820.281528	90.099571	48.132122
1816.319616	92.858018	48.137127
1813.410750	86.720740	48.142132
1810.333989	93.036634	48.147137
1806.633023	90.528025	48.152141
1803.592440	97.325500	48.157146
1799.620542	95.615185	48.162151
1796.293440	89.824571	48.167156
1792.571224	88.379112	48.172161
1789.283024	86.720574	48.177165
1786.335272	82.158552	48.182170
1782.161155	93.431924	48.187175
1778.784659	91.448612	48.192180
1775.804222	87.274484	48.197185
1772.865358	95.577871	48.202189
1769.892610	83.543902	48.207194
1766.070747	91.699983	48.212199
1762.506651	81.577185	48.217204
1758.767405	84.709097	48.222209
1755.357476	88.106127	48.227213
1752.176549	82.723035	48.232218
1748.081499	88.517218	48.237223
1745.002234	82.754479	48.242228
1741.619668	72.938789	48.247233
1737.929154	89.575295	48.252237
1735.131145	83.484049	48.257242
1731.594214	86.223813	48.262247
1727.586467	80.732133	48.267252
1724.275939	79.108715	48.272257
1720.748783	77.794255	48.277261
1717.624379	82.301597	48.282266
1713.922707	87.531528	48.287271
1710.750602	81.764261	48.292276
1707.224763	81.734060	48.297281
1703.749437	83.217739	48.302285
1700.398595	77.851610	48.307290
1696.522494	82.520240	48.312295
1693.098261	75.517246	48.317300
1689.683171	78.861298	48.322305
1685.929535	81.849925	48.327309
1682.280814	80.396204	48.332314
1679.236692	82.784028	48.337319
1676.054206	85.016220	48.342324
1672.586394	70.354365	48.347329
1668.818721	78.274222	48.352333
1665.426877	71.788204	48.357338
1661.652487	79.142804	48.362343
1658.815540	78.242936	48.367348
1655.045930	88.807953	48.372353
1651.548192	74.650622	48.377357
1647.782788	77.932143	48.382362
1644.206037	81.636711	48.387367
1641.154062	80.545689	48.392372
1637.861651	85.629669	48.397377
1634.218731	82.909569	48.402381
1630.592797	72.698350	48.407386
1627.219114	80.392375	48.412391
1623.517289	72.309485	48.417396
1620.539593	71.871281	48.422401
1616.489652	80.768364	48.427405
1613.032996	78.196445	48.432410
1609.477014	83.897241	48.437415
1605.866940	75.664033	48.442420
1602.738435	70.241168	48.447425
1599.025885	80.601151	48.452429
1595.593817	76.516322	48.457434
1592.209739	84.547320	48.462439
1588.958870	75.052837	48.467444
1585.927503	84.477911	48.472449
1581.706675	94.442457	48.477453
1578.186898	84.094497	48.482458
1574.700650	81.957450	48.487463
1571.368221	83.251223	48.492468
1567.854665	84.136596	48.497473
1564.307805	83.514905	48.502477
1560.459770	81.203220	48.507482
1557.144640	81.178202	48.512487
1554.122679	77.909055	48.517492
1550.418819	75.226926	48.522497
1546.347831	79.308976	48.527501
1543.551235	80.332693	48.532506
1539.872820	85.435628	48.537511
1536.622749	77.725355	48.542516
1533.191080	77.512837	48.547521
1529.486555	82.097826	48.552525
1526.503430	78.825802	48.557530
1522.490274	76.131705	48.562535
1519.051728	81.080250	48.567540
1515.031288	81.588949	48.572545
1511.480503	75.096054	48.577549
1508.372529	65.155414	48.582554
1505.025491	73.205953	48.587559
1501.341077	81.755088	48.592564
1497.579694	77.297593	48.597569
1494.559828	75.473937	48.602573
1491.005670	66.504399	48.607578
1487.059919	73.714837	48.612583
1484.171281	71.782173	48.617588
1480.530890	79.369020	48.622593
1476.870066	78.739767	48.627597
1473.787022	70.927580	48.632602
1469.836420	75.981135	48.637607
1466.475043	74.251765	48.642612
1462.889930	77.233160	48.647617
1459.299488	81.069583	48.652621
1456.080396	75.676654	48.657626
1452.575400	78.057132	48.662631
1449.054362	69.911334	48.667636
1445.426588	74.228121	48.672641
1441.895040	84.325821	48.677645
1438.748791	80.538204	48.682650
1434.961822	79.485672	48.687655
1431.137627	77.496154	48.692660
1427.976272	76.630980	48.697665
1424.501449	78.750506	48.702669
1421.280776	84.089079	48.707674
1417.537228	84.013700	48.712679
1414.398251	80.240772	48.717684
1410.546452	86.759564	48.722689
1406.712686	84.110325	48.727693
1403.421645	71.081956	48.732698
1399.824649	80.183787	48.737703
1396.444497	70.405749	48.742708
1392.780063	70.507880	48.747713
1389.689848	78.278009	48.752717
1386.176599	71.390158	48.757722
1382.741834	77.227117	48.762727
1379.167795	79.975846	48.767732
1375.754273	74.195584	48.772737
1371.814247	82.588360	48.777741
1368.463162	67.376906	48.782746
1365.136511	75.892503	48.787751
1361.404220	79.086636	48.792756
1358.199198	78.838858	48.797761
1354.376031	76.371472	48.802765
1350.708325	72.016476	48.807770
1347.426836	72.751855	48.812775
1344.074053	75.975501	48.817780
1340.800008	81.448933	48.822785
1336.858699	82.540109	48.827789
1333.510899	80.027208	48.832794
1329.996072	77.369466	48.837799
1326.422196	80.342795	48.842804
1322.965369	64.591004	48.847809
1319.421156	71.463708	48.852813
1316.329022	64.152828	48.857818
1312.256547	74.901021	48.862823
1308.966707	67.696842	48.867828
1305.373922	69.113416	48.872833
1301.728997	67.975518	48.877837
1298.473570	68.194327	48.882842
1295.515527	68.506051	48.887847
1291.758939	73.244686	48.892852
1288.284361	71.748087	48.897857
1284.093414	78.183633	48.902861
1281.191651	67.701581	48.907866
1277.429167	76.566587	48.912871
1273.825327	75.333713	48.917876
1270.640826	77.765559	48.922881
1266.927040	75.442508	48.927885
1263.818879	72.458890	48.932890
1260.392319	77.649186	48.937895
1256.534317	73.924924	48.942900
1252.744891	66.437856	48.947905
1249.146966	74.948224	48.952909
1246.256112	69.086629	48.957914
1242.635638	66.008755	48.962919
1239.091800	74.064625	48.967924
1235.491044	64.574052	48.972929
1231.726183	76.005179	48.977933
1228.549947	63.658157	48.982938
1225.118504	74.199008	48.987943
1221.417259	64.410875	48.992948
1217.898470	68.378525	48.997953
1214.409981	62.739672	49.002957
1211.252243	65.243284	49.007962
1207.657571	60.525774	49.012967
1204.035909	70.254692	49.017972
1200.646681	71.342205	49.022977
1196.490179	74.580235	49.027981
1193.501046	64.171910	49.032986
1189.984807	67.455810	49.037991
1186.498963	66.973356	49.042996
1183.228765	73.271917	49.048001
1179.079444	73.639367	49.053005
1176.066353	60.798738	49.058010
1172.351450	70.206820	49.063015
1168.809100	67.828625	49.068020
1165.962330	67.037895	49.073025
1161.751914	73.498625	49.078029
1158.342742	64.598329	49.083034
1154.856962	74.128932	49.088039
1151.223351	67.835648	49.093044
1148.130377	56.560831	49.098049
1144.620598	60.568211	49.103053
1141.355518	54.967362	49.108058
1137.494904	62.294272	49.113063
1134.095424	58.103201	49.118068
1130.273725	62.431211	49.123073
1126.542317	65.160163	49.128077
1123.463229	61.343154	49.133082
1120.076905	68.801881	49.138087
1116.637140	61.738129	49.143092
1112.903745	61.620077	49.148097
1109.126250	68.399391	49.153101
1106.196650	58.715793	49.158106
1102.810423	61.387853	49.163111
1098.833027	63.323049	49.168116
1095.781347	67.151562	49.173121
1091.657309	72.244795	49.178125
1088.030351	56.215837	49.183130
1084.477283	61.859255	49.188135
1081.293579	61.326620	49.193140
1078.254168	66.567391	49.198145
1074.391881	74.483015	49.203149
1071.153217	66.574899	49.208154
1067.641717	64.207735	49.213159
1064.015029	66.597696	49.218164
1060.674046	56.880069	49.223169
1057.062026	67.233897	49.228173
1053.485074	54.534850	49.233178
1049.518905	62.669117	49.238183
1045.828795	56.005007	49.243188
1042.756424	56.730010	49.248193
1039.257197	59.236171	49.253197
1036.571571	64.595875	49.258202
1032.745635	58.262950	49.263207
1028.925920	65.479101	49.268212
1025.383944	61.791104	49.273217
1021.372774	64.123862	49.278221
1018.114490	64.861987	49.283226
1014.811833	67.451446	49.288231
1011.230356	60.140859	49.293236
1007.723110	59.541538	49.298241
1004.604827	64.535167	49.303245
1000.932103	64.799980	49.308250
997.355710	62.889005	49.313255
993.871172	67.743499	49.318260
990.361508	60.959563	49.323265
986.622256	73.361119	49.328269
983.211356	66.530171	49.333274
980.032637	69.568565	49.338279
976.310456	70.176430	49.343284
973.010959	60.930075	49.348289
969.509456	66.973591	49.353293
966.184266	68.000540	49.358298
962.428667	62.757638	49.363303
958.701356	62.221052	49.368308
955.472438	62.666717	49.373313
951.432135	64.921762	49.378317
948.103920	58.821417	49.383322
944.315392	70.170811	49.388327
940.807226	60.833560	49.393332
937.966350	68.909727	49.398337
934.347155	60.133914	49.403341
931.170558	64.352033	49.408346
927.413685	65.123487	49.413351
923.796084	55.695713	49.418356
920.534207	63.347042	49.423361
916.637348	69.838073	49.428365
913.415648	51.177174	49.433370
909.807545	67.168067	49.438375
906.159693	62.487355	49.443380
902.659103	60.431720	49.448385
899.149750	60.098489	49.453389
895.611267	64.341306	49.458394
892.169850	63.969027	49.463399
888.671630	67.993611	49.468404
885.664279	61.859147	49.473409
881.862338	65.380530	49.478413
878.325301	60.457953	49.483418
874.750812	60.410104	49.488423
871.122115	60.449786	49.493428
867.762051	60.900057	49.498433
864.592609	61.959718	49.503437
860.820287	59.120668	49.508442
857.368304	59.132844	49.513447
853.708670	54.112300	49.518452
850.284204	62.165418	49.523457
846.430006	66.545968	49.528461
843.045346	63.659229	49.533466
839.721205	54.315503	49.538471
835.887071	61.578200	49.543476
833.210120	56.755858	49.548481
829.287557	59.109644	49.553485
825.734207	61.570468	49.558490
822.237257	59.359257	49.563495
818.553026	65.668502	49.568500
815.078855	61.179064	49.573505
811.588577	54.173850	49.578509
808.155307	58.045964	49.583514
804.891956	59.942804	49.588519
801.304405	59.397137	49.593524
797.709178	60.133954	49.598529
794.243849	59.338314	49.603533
790.915461	58.397974	49.608538
787.076571	56.401344	49.613543
783.480348	58.783427	49.618548
780.397261	54.150862	49.623553
776.753681	59.859010	49.628557
773.090247	54.003862	49.633562
769.593464	61.052702	49.638567
765.960588	62.095932	49.643572
762.828716	60.726381	49.648577
759.215823	51.085945	49.653581
755.464755	56.832972	49.658586
752.020471	55.853732	49.663591
748.379856	59.470234	49.668596
745.382748	52.786885	49.673601
741.460317	58.342296	49.678605
738.238271	56.806457	49.683610
734.680471	57.227415	49.688615
731.201019	49.458088	49.693620
727.872117	45.854027	49.698625
723.939885	55.359224	49.703629
720.572830	56.699592	49.708634
717.416590	53.245818	49.713639
713.707564	51.317567	49.718644
710.394641	49.884462	49.723649
706.363031	53.928819	49.728653
702.785521	52.125625	49.733658
699.318380	47.087800	49.738663
696.039694	50.119631	49.743668
692.925361	51.357387	49.748673
688.849881	55.272537	49.753677
685.607037	51.250135	49.758682
682.088463	52.933624	49.763687
678.665093	57.822909	49.768692
675.281083	49.035853	49.773697
671.443152	60.130355	49.778701
668.263307	56.654953	49.783706
664.489075	56.277567	49.788711
660.380217	51.807867	49.793716
657.546283	47.326356	49.798721
654.320156	57.544191	49.803725
650.742082	64.985335	49.808730
647.299457	52.936172	49.813735
643.729526	57.455980	49.818740
639.952962	48.923024	49.823745
636.511421	64.745617	49.828749
633.208096	50.355803	49.833754
629.931533	53.051962	49.838759
625.980575	58.548551	49.843764
622.680185	39.931631	49.848769
618.854023	57.683819	49.853773
615.419120	50.002490	49.858778
611.741971	59.926718	49.863783
608.160830	58.494251	49.868788
605.156464	50.594044	49.873793
601.591794	61.373936	49.878797
597.993254	52.129921	49.883802
594.559465	47.460234	49.888807
590.676875	50.437395	49.893812
587.606215	54.031621	49.898817
584.149124	52.279300	49.903821
580.596596	49.418735	49.908826
576.939995	55.856568	49.913831
573.128430	54.779509	49.918836
570.138325	52.087647	49.923841
566.442149	50.401020	49.928845
562.887198	52.166114	49.933850
559.560186	54.965043	49.938855
556.077142	57.329531	49.943860
552.734555	53.480860	49.948865
549.160772	52.800210	49.953869
545.586793	47.054564	49.958874
541.966336	47.599192	49.963879
538.140308	51.453379	49.968884
534.845081	54.250526	49.973889
531.092378	55.663606	49.978893
527.813430	58.575275	49.983898
524.608471	52.392543	49.988903
521.004664	53.921646	49.993908
517.947893	48.022723	49.998913
513.814404	52.098779	50.003917
510.320032	47.593557	50.008922
507.131561	47.238897	50.013927
503.232141	51.240551	50.018932
500.195046	51.650077	50.023937
496.099415	57.219820	50.028941
492.520063	58.998212	50.033946
489.216448	49.815874	50.038951
485.708989	62.051639	50.043956
482.925966	57.426188	50.048961
478.833124	59.857144	50.053965
475.366523	65.487148	50.058970
471.946871	51.431850	50.063975
468.515813	59.451213	50.068980
465.307951	56.287078	50.073985
461.268975	53.081493	50.078989
457.525940	47.422291	50.083994
454.130407	52.538207	50.088999
450.344461	48.151152	50.094004
447.303098	40.481358	50.099009
443.859370	53.874589	50.104013
440.002707	55.398774	50.109018
436.932715	46.689428	50.114023
433.548854	57.947361	50.119028
430.708085	49.411131	50.124033
426.559322	59.155696	50.129037
422.756069	48.368087	50.134042
419.542259	57.954443	50.139047
415.790551	62.221007	50.144052
412.434981	52.192583	50.149057
408.518621	57.772390	50.154061
404.852648	49.427905	50.159066
401.749463	55.827052	50.164071
398.299099	53.393523	50.169076
395.077426	50.313805	50.174081
391.710303	55.947309	50.179085
387.750492	57.379995	50.184090
384.173597	52.621893	50.189095
380.762052	54.098936	50.194100
377.401913	44.539456	50.199105
373.881874	58.675377	50.204109
370.202808	59.573992	50.209114
367.029052	45.515244	50.214119
363.252315	52.057216	50.219124
359.802480	46.061330	50.224129
356.141704	50.405488	50.229133
352.544843	50.680721	50.234138
349.379273	56.453687	50.239143
345.533662	58.488678	50.244148
342.312986	51.938277	50.249153
338.893707	58.541659	50.254157
335.230865	46.555330	50.259162
331.956727	42.971279	50.264167
328.152977	49.960371	50.269172
324.891425	47.408876	50.274177
320.984510	51.987505	50.279181
317.432215	49.408511	50.284186
314.621455	50.760392	50.289191
310.969622	53.290387	50.294196
307.454768	51.942556	50.299201
303.666033	54.316700	50.304205
300.047530	48.533740	50.309210
296.776931	46.565772	50.314215
292.951340	50.546465	50.319220
289.500259	49.751840	50.324225
285.934548	52.195666	50.329229
282.544810	43.532967	50.334234
279.504118	48.770819	50.339239
275.838352	58.816675	50.344244
272.262042	45.415391	50.349249
268.657715	52.996682	50.354253
264.765288	48.233945	50.359258
261.573419	49.604037	50.364263
258.082699	56.905060	50.369268
255.067877	51.711473	50.374273
251.313810	49.217686	50.379277
247.680724	58.461214	50.384282
244.374980	41.670666	50.389287
240.662559	54.757731	50.394292
237.055841	48.773638	50.399297
233.535173	55.506703	50.404301
230.156134	49.154981	50.409306
227.012672	51.156599	50.414311
222.979029	58.529497	50.419316
219.717423	48.679471	50.424321
215.679449	52.791313	50.429325
212.040098	49.305266	50.434330
209.205967	49.404826	50.439335
205.656007	51.820899	50.444340
202.284557	45.205418	50.449345
199.014435	56.518416	50.454349
195.405195	52.410771	50.459354
191.906873	47.058361	50.464359
188.314553	50.765475	50.469364
184.884215	48.018825	50.474369
181.129372	52.368156	50.479373
177.211026	60.931625	50.484378
173.605290	52.989087	50.489383
170.219024	62.757326	50.494388
167.540735	50.877172	50.499393
163.672705	45.126761	50.504397
160.048764	49.870153	50.509402
156.661515	48.784044	50.514407
152.786759	43.414322	50.519412
149.405014	51.514607	50.524417
146.063384	49.184409	50.529421
143.110386	59.976653	50.534426
139.286227	45.715513	50.539431
135.546922	58.278440	50.544436
132.234100	43.833292	50.549441
128.765966	51.782519	50.554445
124.440915	51.810501	50.559450
121.155308	50.629481	50.564455
117.693038	52.607984	50.569460
114.781342	50.900529	50.574465
111.003146	51.090137	50.579469
107.525906	44.573401	50.584474
104.358789	42.779170	50.589479
100.329600	45.712780	50.594484
97.109853	45.242823	50.599489
93.498959	48.468801	50.604493
89.713595	48.608910	50.609498
86.428562	49.180470	50.614503
83.033334	47.560957	50.619508
79.518745	55.027056	50.624513
76.079835	46.071509	50.629517
72.627120	47.703691	50.634522
68.879904	47.167170	50.639527
65.457362	47.431122	50.644532
62.083184	44.099964	50.649537
58.045678	43.577005	50.654541
55.004046	46.815594	50.659546
51.792623	44.284811	50.664551
48.146721	51.508773	50.669556
44.673122	50.910673	50.674561
40.977555	56.377052	50.679565
37.518474	47.358217	50.684570
33.937077	45.248859	50.689575
30.177729	53.983730	50.694580
27.018559	45.484497	50.699585
23.737221	53.660905	50.704589
19.824703	51.599939	50.709594
16.677611	48.423251	50.714599
12.360496	56.896965	50.719604
9.711090	43.281836	50.724609
6.049435	47.398386	50.729613
2.672112	52.872165	50.734618