Fri Aug 26 13:35:30 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.285739	105.933912	0.000000
1.079483	104.137469	0.005005
1.370912	96.151355	0.010010
1.152405	110.285829	0.015014
1.022633	101.852780	0.020019
1.385506	99.452049	0.025024
0.515703	95.345050	0.030029
0.777384	85.579271	0.035034
0.457957	81.522620	0.040038
-0.051093	59.930907	0.045043
-0.209315	52.910135	0.050048
-0.327108	51.371997	0.055053
-0.406347	54.567001	0.060058
-0.629507	47.376013	0.065062
-0.876402	29.593679	0.070067
-1.269904	28.864072	0.075072
-2.264255	23.428769	0.080077
-2.195331	12.671186	0.085082
-2.431000	17.434395	0.090086
-2.697752	1.021874	0.095091
-3.297510	0.393982	0.100096
-3.443139	0.328111	0.105101
-3.405076	-9.121235	0.110106
-3.808656	-8.966617	0.115110
-4.341186	-6.283157	0.120115
-4.645095	-12.006275	0.125120
-5.040670	-4.503776	0.130125
-5.113344	-3.293405	0.135130
-4.967851	-1.794311	0.140134
-4.857946	-6.246806	0.145139
-5.797440	-5.028019	0.150144
-6.247950	-1.196274	0.155149
-6.328295	-15.065765	0.160154
-6.620712	-3.488745	0.165158
-6.571501	-0.101787	0.170163
-6.731213	-1.990885	0.175168
-7.719406	-9.189281	0.180173
-7.435519	-6.186862	0.185178
-7.579581	-7.667123	0.190182
-7.771811	-12.645192	0.195187
-8.151630	-4.506091	0.200192
-8.892102	-5.175347	0.205197
-8.913705	-9.483983	0.210202
-9.221064	-1.650381	0.215206
-9.238489	-9.389051	0.220211
-9.117795	-2.216859	0.225216
-9.237711	-6.997389	0.230221
-9.916941	-6.100689	0.235226
-10.242725	0.024256	0.240230
-10.178538	-5.762503	0.245235
-10.778373	-5.545692	0.250240
-11.573577	-7.917953	0.255245
-11.597802	-9.552908	0.260250
-11.932883	-12.892117	0.265254
-11.586034	-6.432157	0.270259
-11.735326	-7.943239	0.275264
-11.989213	5.427896	0.280269
-12.028246	-9.007995	0.285274
-12.780023	-4.177090	0.290278
-13.406244	-11.371734	0.295283
-13.171747	-4.726608	0.300288
-13.568772	1.428411	0.305293
-13.672529	-11.241582	0.310298
-13.734092	-7.182505	0.315302
-14.640608	-7.563326	0.320307
-14.777821	-5.377998	0.325312
-15.106375	-0.337750	0.330317
-14.885553	-9.407442	0.335322
-15.250853	-1.571146	0.340326
-15.207586	-4.937628	0.345331
-15.640452	-3.788231	0.350336
-16.362126	3.420208	0.355341
-16.204712	-2.017249	0.360346
-16.765287	-5.087241	0.365350
-16.588330	-9.765301	0.370355
-16.339603	-14.878462	0.375360
-17.435817	-7.308003	0.380365
-17.551299	-9.805077	0.385370
-18.004476	-4.868809	0.390374
-17.905484	-1.862911	0.395379
-17.669339	1.045705	0.400384
-18.536107	-3.387597	0.405389
-18.381695	-6.679638	0.410394
-19.100634	-2.777628	0.415398
-19.053883	-3.689670	0.420403
-19.733580	-2.647369	0.425408
-20.598719	-3.891978	0.430413
-20.224655	-9.477055	0.435418
-20.566381	-5.494576	0.440422
-20.423718	-7.142860	0.445427
-20.349384	-11.808105	0.450432
-20.820928	-0.544868	0.455437
-20.804346	-10.098432	0.460442
-21.846163	-14.014112	0.465446
-21.913894	-9.609240	0.470451
-22.191387	-15.409232	0.475456
-22.413662	-11.252371	0.480461
-22.061861	-9.592418	0.485466
-22.437995	-8.980182	0.490470
-22.979530	-13.464119	0.495475
-22.862813	-9.496074	0.500480
-23.571666	-12.666360	0.505485
-24.157157	-3.350001	0.510490
-24.740212	-1.259765	0.515494
-24.286513	-13.605276	0.520499
-24.663362	-5.985476	0.525504
-25.085219	-0.462483	0.530509
-24.974726	-1.827359	0.535514
-25.050702	-4.068002	0.540518
-25.147807	1.891628	0.545523
-25.800032	1.158015	0.550528
-26.475204	-1.444899	0.555533
-26.498257	-10.989127	0.560538
-27.066850	-0.106234	0.565542
-26.929461	-4.284607	0.570547
-26.951745	-7.011319	0.575552
-27.025171	-0.425813	0.580557
-26.874169	-10.835505	0.585562
-27.799677	-7.597332	0.590566
-27.998323	-7.199385	0.595571
-27.824744	-5.141538	0.600576
-28.908438	-5.127790	0.605581
-28.815569	-11.738393	0.610586
-29.490324	-7.871736	0.615590
-29.552057	-3.034378	0.620595
-29.565468	-5.727671	0.625600
-29.563654	-2.026462	0.630605
-29.539165	-9.186383	0.635610
-30.505042	-14.081959	0.640614
-30.882564	0.263837	0.645619
-31.077320	-0.044312	0.650624
-31.245615	-3.789127	0.655629
-31.507224	-11.341084	0.660634
-31.408395	-1.811745	0.665638
-31.863387	2.536371	0.670643
-31.771438	-4.377800	0.675648
-32.246064	-5.746483	0.680653
-32.346417	-6.993112	0.685658
-32.337730	-4.400246	0.690662
-32.510418	-12.639902	0.695667
-33.369940	-6.580550	0.700672
-33.678268	-5.728944	0.705677
-33.609574	-11.117783	0.710682
-33.956356	2.593666	0.715686
-34.821462	-11.441529	0.720691
-35.226557	-9.622602	0.725696
-34.989565	-3.522011	0.730701
-35.110538	-5.512047	0.735706
-35.197795	0.037939	0.740710
-35.624065	2.866201	0.745715
-35.587123	-0.711260	0.750720
-35.902941	3.988496	0.755725
-36.430857	-2.379928	0.760730
-36.833510	-2.867671	0.765734
-36.991510	0.867912	0.770739
-36.815497	-3.885929	0.775744
-37.420911	6.158009	0.780749
-37.180132	-3.035010	0.785754
-38.099716	0.879260	0.790758
-38.325236	-3.217300	0.795763
-38.317376	-7.109759	0.800768
-38.453336	-0.327862	0.805773
-38.464303	-11.120444	0.810778
-38.792715	1.211962	0.815782
-39.441609	-3.517843	0.820787
-39.366127	-4.709595	0.825792
-39.985139	6.200133	0.830797
-39.779796	-4.740022	0.835802
-40.406456	-0.811252	0.840806
-40.785906	0.506992	0.845811
-41.005092	0.670865	0.850816
-41.290153	-2.790024	0.855821
-41.060851	-8.314597	0.860826
-41.025284	-6.788898	0.865830
-41.861285	0.712576	0.870835
-42.451948	-6.076331	0.875840
-43.252631	3.200772	0.880845
-42.888044	-5.151013	0.885850
-43.237819	3.442139	0.890854
-43.021230	-2.580311	0.895859
-42.789999	-7.469294	0.900864
-43.307486	1.757388	0.905869
-43.380641	-1.397986	0.910874
-44.229861	1.075364	0.915878
-44.540378	-5.440797	0.920883
-44.602398	-10.299939	0.925888
-44.912355	-6.154734	0.930893
-44.439994	-7.724643	0.935898
-45.226665	3.745842	0.940902
-45.994506	-7.871661	0.945907
-45.971141	-4.648353	0.950912
-46.009706	2.058270	0.955917
-46.217502	-1.911340	0.960922
-47.120073	0.620936	0.965926
-47.326868	2.791789	0.970931
-47.636144	0.229979	0.975936
-47.405484	2.683885	0.980941
-47.432008	8.869800	0.985946
-47.684995	9.608391	0.990950
-47.869793	6.125562	0.995955
-47.670632	0.893570	1.000960
-48.825699	8.292870	1.005965
-48.784617	-0.571674	1.010970
-49.558301	8.308937	1.015974
-49.423663	3.817791	1.020979
-49.382136	0.916634	1.025984
-49.611990	8.728680	1.030989
-50.207229	-0.641045	1.035994
-50.704311	-0.272558	1.040998
-50.666487	0.376462	1.046003
-50.759427	-4.968230	1.051008
-51.326815	1.077276	1.056013
-50.892245	-1.622495	1.061018
-51.435797	6.659156	1.066022
-52.144937	0.205058	1.071027
-52.010421	-5.545194	1.076032
-52.459519	-0.036942	1.081037
-52.540827	-7.439809	1.086042
-52.659119	-0.847318	1.091046
-53.120330	-4.094126	1.096051
-53.521605	-0.842665	1.101056
-53.920506	-6.835719	1.106061
-53.195232	-8.153952	1.111066
-53.807985	-1.535093	1.116070
-54.505272	7.947368	1.121075
-54.810151	-0.815855	1.126080
-55.106101	7.477863	1.131085
-54.965831	-1.003506	1.136090
-55.233724	-1.059831	1.141094
-55.510388	-0.067627	1.146099
-56.309929	-8.386846	1.151104
-56.411735	0.578968	1.156109
-56.280745	-6.692444	1.161114
-56.626627	5.516138	1.166118
-56.618013	0.756723	1.171123
-56.877846	3.217398	1.176128
-57.660375	15.715427	1.181133
-57.652186	2.809709	1.186138
-58.148063	2.308008	1.191142
-58.504958	-7.146277	1.196147
-58.577589	-3.411333	1.201152
-58.920164	0.906625	1.206157
-58.377342	-5.008437	1.211162
-58.896192	9.811769	1.216166
-59.265836	-0.485226	1.221171
-59.333654	-13.872625	1.226176
-60.336794	-3.482041	1.231181
-59.759783	-6.675370	1.236186
-60.390845	-1.091333	1.241190
-60.934679	-1.832331	1.246195
-60.981116	1.990282	1.251200
-61.190531	3.218779	1.256205
-61.071209	8.568931	1.261210
-61.313774	4.563606	1.266214
-61.819172	0.634005	1.271219
-62.211793	-6.745698	1.276224
-62.512195	4.690201	1.281229
-62.511327	3.642939	1.286234
-62.460487	8.026189	1.291238
-63.120999	9.343904	1.296243
-63.498033	-3.074739	1.301248
-63.866959	1.487758	1.306253
-63.764385	0.709387	1.311258
-64.261964	5.997407	1.316262
-64.291368	1.671003	1.321267
-64.336938	-3.949973	1.326272
-65.200343	5.232495	1.331277
-65.270929	-5.826041	1.336282
-65.193886	5.690291	1.341286
-64.936792	0.208843	1.346291
-65.803611	-1.551174	1.351296
-66.634997	4.219073	1.356301
-66.601443	0.765521	1.361306
-66.772065	-2.975766	1.366310
-66.689672	8.118970	1.371315
-66.526558	9.833611	1.376320
-67.562813	1.288663	1.381325
-67.513457	10.993382	1.386330
-68.041596	9.316667	1.391334
-68.088579	6.309073	1.396339
-68.244428	7.722212	1.401344
-69.046597	3.051072	1.406349
-69.190747	-2.228701	1.411354
-69.544104	1.844171	1.416358
-69.484418	11.876300	1.421363
-69.482132	9.278635	1.426368
-69.816274	9.188334	1.431373
-69.681532	-2.604501	1.436378
-70.630014	0.520196	1.441382
-70.929615	2.670698	1.446387
-71.249234	-3.970590	1.451392
-71.380373	12.918377	1.456397
-71.296637	5.473991	1.461402
-71.172764	9.633906	1.466406
-71.748238	8.628926	1.471411
-72.035114	9.319011	1.476416
-72.668914	12.533914	1.481421
-72.734521	6.729400	1.486426
-73.119918	9.146353	1.491430
-73.089160	14.494477	1.496435
-73.238474	9.699541	1.501440
-74.045374	8.749575	1.506445
-74.334325	1.603655	1.511450
-74.505046	8.141038	1.516454
-75.089331	10.215649	1.521459
-74.479292	-0.227554	1.526464
-74.387217	12.697423	1.531469
-74.505432	9.096664	1.536474
-75.037445	6.854262	1.541478
-75.708425	7.566189	1.546483
-75.794185	1.805941	1.551488
-75.948224	14.601566	1.556493
-76.349328	3.259142	1.561498
-76.876965	11.762934	1.566502
-77.045216	9.081094	1.571507
-76.879432	0.725462	1.576512
-77.301624	12.287892	1.581517
-77.601919	11.135666	1.586522
-78.092041	5.438377	1.591526
-78.397392	10.117522	1.596531
-78.455819	9.016219	1.601536
-78.443342	8.735913	1.606541
-78.429371	0.327992	1.611546
-79.246710	1.885252	1.616550
-79.992150	10.416629	1.621555
-79.693206	3.647391	1.626560
-80.261800	6.921740	1.631565
-79.913755	7.313659	1.636570
-80.050838	7.404640	1.641574
-80.309071	4.803247	1.646579
-80.867197	4.491566	1.651584
-81.090201	12.596764	1.656589
-81.428853	2.510072	1.661594
-81.475573	4.978692	1.666598
-82.582580	6.182436	1.671603
-82.642803	1.395777	1.676608
-82.713377	2.960147	1.681613
-82.912234	-2.102308	1.686618
-82.643729	-3.681604	1.691622
-82.978220	-5.382140	1.696627
-82.941929	-9.174624	1.701632
-84.292372	1.785709	1.706637
-84.269646	7.777299	1.711642
-84.528636	0.917770	1.716646
-84.596412	7.167050	1.721651
-84.120632	1.132717	1.726656
-84.770769	7.548599	1.731661
-84.732407	-5.311190	1.736666
-85.169784	1.533454	1.741670
-86.004651	4.153261	1.746675
-85.744311	-2.948472	1.751680
-86.016828	2.260213	1.756685
-86.455195	-5.185130	1.761690
-87.111611	3.313400	1.766694
-87.614211	0.775365	1.771699
-87.264616	-8.595936	1.776704
-87.724412	2.624342	1.781709
-87.727529	3.336682	1.786714
-87.622738	3.238149	1.791718
-87.816703	-2.176231	1.796723
-88.205248	-6.250568	1.801728
-88.637839	2.175148	1.806733
-88.900624	-0.938045	1.811738
-88.991595	3.951320	1.816742
-89.688985	-1.523877	1.821747
-89.959154	-9.137770	1.826752
-90.666770	4.775383	1.831757
-90.359072	-1.334015	1.836762
-90.411631	0.613514	1.841766
-90.574267	2.571855	1.846771
-90.227302	-6.049255	1.851776
-91.296950	-1.298566	1.856781
-91.703800	1.485544	1.861786
-92.097913	-4.929017	1.866790
-92.078649	-0.797108	1.871795
-91.880617	-4.288922	1.876800
-91.994448	4.349746	1.881805
-92.530309	-3.589764	1.886810
-93.448989	-0.096398	1.891814
-93.436003	0.316053	1.896819
-93.409365	-0.662457	1.901824
-93.574632	9.132621	1.906829
-93.578139	-2.436213	1.911834
-94.509539	-1.759666	1.916838
-94.816970	-3.790270	1.921843
-94.729309	-1.329920	1.926848
-94.851331	6.563406	1.931853
-94.884048	-3.760733	1.936858
-95.153266	0.014310	1.941862
-95.869119	4.314460	1.946867
-96.257278	4.425552	1.951872
-96.668680	9.054772	1.956877
-96.770364	0.471878	1.961882
-96.673791	-0.118903	1.966886
-96.616099	4.674550	1.971891
-96.396043	-13.325957	1.976896
-97.443105	-1.644100	1.981901
-97.699739	-3.970504	1.986906
-97.856024	-1.639844	1.991910
-98.257966	-3.503877	1.996915
-98.745291	1.301481	2.006912
-98.435778	-1.207929	2.016909
-98.106192	-1.620288	2.026906
-97.325247	-0.794670	2.036902
-96.853327	0.794960	2.046899
-95.802883	-0.689446	2.056896
-95.487613	-7.197371	2.066893
-95.421565	-4.980698	2.076890
-94.971407	-10.673355	2.086886
-94.540422	-4.819983	2.096883
-93.620755	-3.097335	2.106880
-92.789312	4.192004	2.116877
-92.927944	-1.912643	2.126874
-92.620979	-9.597653	2.136870
-91.338921	-3.832445	2.146867
-91.298620	-2.007724	2.156864
-91.124656	-2.275481	2.166861
-89.915236	-3.879670	2.176858
-90.056016	1.597079	2.186854
-88.928844	-2.531621	2.196851
-88.657796	-6.127893	2.206848
-88.421630	-13.719518	2.216845
-87.716219	-3.908088	2.226842
-87.333505	-7.404542	2.236838
-86.804032	-7.011755	2.246835
-85.939138	0.335729	2.256832
-85.755446	-6.082021	2.266829
-85.488064	-0.836711	2.276826
-84.872181	-6.216230	2.286822
-84.114399	-8.703572	2.296819
-83.667044	-6.806019	2.306816
-82.898075	-6.998531	2.316813
-82.645892	-9.514852	2.326810
-82.633546	-6.241314	2.336806
-81.804337	-7.038730	2.346803
-81.313718	-0.741661	2.356800
-80.144392	-5.234873	2.366797
-79.795112	-4.874215	2.376794
-79.856837	1.584879	2.386790
-80.027821	-2.233997	2.396787
-78.870687	-7.843502	2.406784
-77.735195	-10.041208	2.416781
-77.231396	-8.424864	2.426778
-76.973688	-2.034513	2.436774
-77.002197	-3.252728	2.446771
-76.612476	-1.634460	2.456768
-75.794216	-2.354146	2.466765
-75.120886	2.663239	2.476762
-74.296510	10.739270	2.486758
-73.938200	8.713252	2.496755
-74.195773	4.153947	2.506752
-73.267161	2.333730	2.516749
-72.897464	2.627855	2.526746
-71.853741	2.839208	2.536742
-71.272810	-2.243443	2.546739
-71.265656	0.048922	2.556736
-71.191191	-0.184337	2.566733
-70.235137	-4.318070	2.576730
-69.806151	1.785865	2.586726
-68.951103	3.889195	2.596723
-68.342838	0.126380	2.606720
-68.229042	2.079037	2.616717
-67.857072	0.633748	2.626714
-67.040413	0.617538	2.636710
-66.828957	1.110524	2.646707
-66.329909	-1.653302	2.656704
-66.042803	4.086266	2.666701
-65.038594	5.339606	2.676698
-64.232751	10.681641	2.686694
-64.029265	2.673793	2.696691
-64.240009	1.572647	2.706688
-63.194889	0.155592	2.716685
-62.917429	-2.681434	2.726682
-61.972397	1.799489	2.736678
-61.500647	4.760757	2.746675
-61.286666	0.216727	2.756672
-60.471697	1.490028	2.766669
-60.010006	0.775176	2.776666
-60.090784	-3.136937	2.786662
-59.029421	1.820033	2.796659
-58.425914	-4.587059	2.806656
-58.024459	1.945633	2.816653
-57.607989	-4.821963	2.826650
-57.124587	-5.625722	2.836646
-57.049820	-5.165304	2.846643
-55.817746	-1.894782	2.856640
-55.268272	-7.875325	2.866637
-55.500652	-4.110703	2.876634
-54.851077	-6.340453	2.886630
-54.015726	-3.312259	2.896627
-53.848326	3.611656	2.906624
-53.088556	2.755363	2.916621
-52.757763	-1.417228	2.926618
-52.186104	-3.495469	2.936614
-51.704354	-0.969732	2.946611
-51.319740	-2.759099	2.956608
-50.256897	-8.170198	2.966605
-50.008257	-1.585204	2.976602
-49.959744	3.564312	2.986598
-48.726443	2.327025	2.996595
-48.272165	-3.451805	3.006592
-48.074907	-4.119149	3.016589
-48.030633	-4.217832	3.026586
-47.483591	-7.432606	3.036582
-46.739161	2.280894	3.046579
-45.744429	-1.114455	3.056576
-45.305807	-5.379860	3.066573
-45.031117	2.737408	3.076570
-44.839921	-5.316039	3.086566
-43.808446	-3.037446	3.096563
-43.514087	-5.515987	3.106560
-43.306952	-4.265251	3.116557
-42.386061	-12.432307	3.126554
-42.046614	-7.068342	3.136550
-41.936791	-10.221377	3.146547
-41.226127	-3.280682	3.156544
-40.574696	-5.479044	3.166541
-40.309268	-5.849737	3.176538
-39.479499	-2.253657	3.186534
-39.269529	-7.091656	3.196531
-38.436214	-6.933069	3.206528
-37.739059	-8.337125	3.216525
-37.931958	-4.863741	3.226522
-37.296350	-2.203575	3.236518
-36.605953	-0.163303	3.246515
-36.403567	1.807239	3.256512
-35.476335	-4.178272	3.266509
-35.160734	-6.432047	3.276506
-34.393968	-6.548190	3.286502
-34.105790	-1.353630	3.296499
-33.549460	-2.691412	3.306496
-32.863000	-0.900774	3.316493
-32.344239	-7.095107	3.326490
-31.891819	-3.503628	3.336486
-31.835979	-1.203004	3.346483
-31.316364	3.125588	3.356480
-30.677868	-0.375848	3.366477
-29.956550	-3.291486	3.376474
-29.165792	-2.445219	3.386470
-29.011754	7.867039	3.396467
-28.867279	4.705439	3.406464
-28.017274	2.460320	3.416461
-27.358326	8.053302	3.426458
-27.402173	5.750957	3.436454
-26.579146	-0.652304	3.446451
-26.183689	3.426367	3.456448
-25.189256	7.275568	3.466445
-24.602648	6.778844	3.476442
-24.627188	2.968841	3.486438
-24.491829	1.528715	3.496435
-23.594475	6.723461	3.506432
-23.225481	-0.179292	3.516429
-22.689292	-0.639657	3.526426
-21.713502	4.067723	3.536422
-21.768295	0.918142	3.546419
-21.006179	-1.158075	3.556416
-20.199689	0.471329	3.566413
-19.925912	-3.027171	3.576410
-19.944844	3.396755	3.586406
-19.178370	7.417660	3.596403
-18.641603	8.398504	3.606400
-17.822953	7.393666	3.616397
-17.552050	6.432931	3.626394
-17.361984	3.267400	3.636390
-16.579098	5.375633	3.646387
-16.130509	6.405051	3.656384
-15.392731	4.142561	3.666381
-14.744447	4.551697	3.676378
-14.870228	-2.274021	3.686374
-14.112317	-0.389973	3.696371
-13.313133	5.184343	3.706368
-12.709088	3.563542	3.716365
-12.658832	5.459572	3.726362
-11.906412	6.115412	3.736358
-11.664698	1.126754	3.746355
-11.268552	5.819850	3.756352
-9.917475	4.415346	3.766349
-9.788299	0.131598	3.776346
-10.024411	3.956990	3.786342
-9.134891	9.083268	3.796339
-8.545616	6.568311	3.806336
-8.265916	1.982369	3.816333
-7.438864	6.354960	3.826330
-7.132845	3.405784	3.836326
-6.144220	5.339439	3.846323
-5.763873	5.400666	3.856320
-5.561409	1.273394	3.866317
-5.348134	2.982491	3.876314
-4.923685	5.368271	3.886310
-4.403255	17.007771	3.896307
-3.852929	23.989282	3.906304
-2.947488	40.447101	3.916301
-2.429267	47.721881	3.926298
-2.532538	51.418898	3.936294
-2.017147	61.994866	3.946291
-1.083036	76.047138	3.956288
-0.991652	79.143667	3.966285
-0.277386	89.267383	3.976282
-0.074085	101.713397	3.986278
0.000000	116.388484	3.991283
0.886320	119.683094	3.996288
1.093877	121.539519	4.001293
0.910671	131.919578	4.006298
0.903723	139.004137	4.011302
0.958693	144.161877	4.016307
1.097560	138.138824	4.021312
1.110438	135.137704	4.026317
0.786259	151.085623	4.031322
1.192628	130.892001	4.036326
1.384899	144.896110	4.041331
1.412294	139.643364	4.046336
1.410024	138.444726	4.051341
1.089581	143.274950	4.056346
1.344939	141.871689	4.061350
1.556976	151.051303	4.066355
1.393310	145.059532	4.071360
1.750684	151.729878	4.076365
1.031886	152.414453	4.081370
1.698774	150.874353	4.086374
1.815620	139.188605	4.091379
1.287244	139.960587	4.096384
1.348870	137.802902	4.101389
0.896528	136.481356	4.106394
1.440840	156.204346	4.111398
1.242627	158.889560	4.116403
1.643778	161.133452	4.121408
1.873162	160.686498	4.126413
1.576465	156.803456	4.131418
1.856485	155.140098	4.136422
1.484155	159.405781	4.141427
1.748927	161.455777	4.146432
1.607043	154.106563	4.151437
1.563798	151.943059	4.156442
1.603649	137.203709	4.161446
1.593213	150.195373	4.166451
1.382424	155.321730	4.171456
1.669544	149.525520	4.176461
0.919511	154.618780	4.181466
1.283370	151.746503	4.186470
1.486790	153.736451	4.191475
1.812360	158.668571	4.196480
1.800344	148.894753	4.201485
1.655217	155.744575	4.206490
2.108807	164.092506	4.211494
2.022935	161.483233	4.216499
1.864056	165.415136	4.221504
1.919521	159.297496	4.226509
1.804144	165.351773	4.231514
2.045502	151.884468	4.236518
1.457662	154.601872	4.241523
1.739244	152.599759	4.246528
1.996481	163.936288	4.251533
1.495384	165.210211	4.256538
1.894072	155.881793	4.261542
1.728382	162.937295	4.266547
2.138824	152.385874	4.271552
1.960568	168.288944	4.276557
1.907597	162.653245	4.281562
1.723698	158.132562	4.286566
1.966228	172.745782	4.291571
2.015063	160.820679	4.296576
1.959704	159.532232	4.301581
1.855826	158.656288	4.306586
1.850245	161.937917	4.311590
1.879366	161.373450	4.316595
2.113904	165.190317	4.321600
2.056122	161.678189	4.326605
1.763016	165.393715	4.331610
2.109094	167.234906	4.336614
1.929185	164.804785	4.341619
1.835189	170.517222	4.346624
1.949218	157.395595	4.351629
1.571174	165.803409	4.356634
2.015861	172.460168	4.361638
2.334175	177.551607	4.366643
2.381650	182.058810	4.371648
2.586434	185.608238	4.376653
2.304022	170.292629	4.381658
2.197472	164.905710	4.386662
2.062179	161.513215	4.391667
1.826702	163.524043	4.396672
2.062741	163.265873	4.401677
2.100147	181.697947	4.406682
2.545985	177.699291	4.411686
2.615762	191.165702	4.416691
2.512466	175.841182	4.421696
2.163928	158.229564	4.426701
2.052154	157.933801	4.431706
2.265327	164.629767	4.436710
2.185024	171.023425	4.441715
2.263415	176.686879	4.446720
2.631268	182.754507	4.451725
2.420868	182.388680	4.456730
2.417862	173.448655	4.461734
2.302372	172.656774	4.466739
2.562221	177.058145	4.471744
2.583308	161.280849	4.476749
1.892820	165.115192	4.481754
2.423485	166.288582	4.486758
2.495732	181.883750	4.491763
2.464773	181.929735	4.496768
2.525998	182.290389	4.501773
2.257566	189.577027	4.506778
2.462230	184.581398	4.511782
2.198538	176.817716	4.516787
2.306787	187.041700	4.521792
2.682254	183.452621	4.526797
2.316892	186.847217	4.531802
2.729690	186.583671	4.536806
2.376011	193.608344	4.541811
2.486077	184.770927	4.546816
2.603119	185.334856	4.551821
2.254041	190.014531	4.556826
2.507225	191.462074	4.561830
2.364506	198.207137	4.566835
2.432097	185.836182	4.571840
2.559857	186.173822	4.576845
2.363704	194.806424	4.581850
2.907308	197.528001	4.586854
3.036129	195.318720	4.591859
2.771508	191.338929	4.596864
2.796028	193.122623	4.601869
2.926676	188.328338	4.606874
3.122848	185.535946	4.611878
2.810060	181.263109	4.616883
2.608442	182.186692	4.621888
2.771052	182.028537	4.626893
2.726509	188.030666	4.631898
2.755611	183.005426	4.636902
2.604090	194.073432	4.641907
2.547053	200.425514	4.646912
2.773262	187.691349	4.651917
2.663355	191.802289	4.656922
2.926297	197.516107	4.661926
2.886301	207.924532	4.666931
2.903676	204.071672	4.671936
3.089131	201.072144	4.676941
3.030568	201.479922	4.681946
2.786728	183.576738	4.686950
2.917120	193.006360	4.691955
2.844847	195.551752	4.696960
3.306509	192.901516	4.701965
2.732696	196.910685	4.706970
3.128740	198.876973	4.711974
3.092506	206.687436	4.716979
2.635301	193.657885	4.721984
2.942589	198.308133	4.726989
3.111955	215.061932	4.731994
3.449380	209.359107	4.736998
3.066215	206.150726	4.742003
2.965653	197.355588	4.747008
3.265190	201.010486	4.752013
3.021415	204.401972	4.757018
3.143452	199.476150	4.762022
2.803263	199.658864	4.767027
2.786142	207.165802	4.772032
3.098224	199.657305	4.777037
3.107164	210.532663	4.782042
3.340717	206.892910	4.787046
3.400566	213.862697	4.792051
3.201144	211.891176	4.797056
3.341587	203.577355	4.802061
3.438779	208.706394	4.807066
3.449867	208.214335	4.812070
3.311996	212.547928	4.817075
3.643821	208.832764	4.822080
3.140765	199.233445	4.827085
2.929355	196.599422	4.832090
3.416098	202.493526	4.837094
3.238514	205.052152	4.842099
3.333496	206.888150	4.847104
3.718363	203.142584	4.852109
3.319365	206.102669	4.857114
3.511445	199.710651	4.862118
3.249772	193.262736	4.867123
3.244732	192.890244	4.872128
3.253975	197.590060	4.877133
3.242106	215.159831	4.882138
3.782176	200.744333	4.887142
3.582933	207.412780	4.892147
3.434548	202.136765	4.897152
3.819891	201.083412	4.902157
3.289474	194.354644	4.907162
3.192706	191.256694	4.912166
3.562096	204.752395	4.917171
3.753551	204.324000	4.922176
3.716721	206.256449	4.927181
3.390066	207.221647	4.932186
3.224503	190.236389	4.937190
3.567559	211.838361	4.942195
3.476500	212.102506	4.947200
3.762369	206.246363	4.952205
3.401448	211.253745	4.957210
3.658608	207.107293	4.962214
3.522608	210.054904	4.967219
3.674545	207.677511	4.972224
3.648522	206.849553	4.977229
3.471739	215.090016	4.982234
3.463645	214.183338	4.987238
3.671973	216.431950	4.992243
3.499137	214.636619	4.997248
3.851059	212.079395	5.002253
3.795905	213.378799	5.007258
3.672409	216.172608	5.012262
3.653563	209.987429	5.017267
3.614916	215.340095	5.022272
3.766854	212.317311	5.027277
3.478910	217.917596	5.032282
3.549713	213.904558	5.037286
3.766972	212.646426	5.042291
3.638671	211.337695	5.047296
3.631898	222.573002	5.052301
3.691314	242.833483	5.057306
4.250927	227.687273	5.062310
4.113150	223.260630	5.067315
3.384903	230.397419	5.072320
4.096871	229.770925	5.077325
3.684007	235.608958	5.082330
3.876263	235.079200	5.087334
4.019921	241.118482	5.092339
4.089674	240.278774	5.097344
4.252683	236.324140	5.102349
3.938991	235.142346	5.107354
4.337258	234.596331	5.112358
3.963069	222.430173	5.117363
3.712672	214.639096	5.122368
3.972759	225.209611	5.127373
3.825395	237.172318	5.132378
4.017437	231.286483	5.137382
4.306304	238.287059	5.142387
4.498782	236.887255	5.147392
4.488770	219.890405	5.152397
3.797882	213.154978	5.157402
3.839411	210.272768	5.162406
3.822382	217.381073	5.167411
3.965630	227.881198	5.172416
4.576698	222.091473	5.177421
4.249009	230.478823	5.182426
4.393756	228.339822	5.187430
4.068793	224.420038	5.192435
4.293574	233.828659	5.197440
4.312210	220.383324	5.202445
3.729960	222.191892	5.207450
4.114863	226.731989	5.212454
4.307558	232.823743	5.217459
4.111845	239.074047	5.222464
3.851235	238.424977	5.227469
3.825270	236.837725	5.232474
4.498111	230.696703	5.237478
4.202762	235.678064	5.242483
4.181254	241.461494	5.247488
4.235223	233.838150	5.252493
4.195277	237.716751	5.257498
4.222567	233.745284	5.262502
4.157518	232.768381	5.267507
4.186510	245.532519	5.272512
4.488678	243.286750	5.277517
4.393320	258.363928	5.282522
4.662809	256.771801	5.287526
4.488973	243.049539	5.292531
4.324844	235.836629	5.297536
4.601749	238.694647	5.302541
4.548052	242.009091	5.307546
4.386934	237.130509	5.312550
4.441139	239.747961	5.317555
4.682163	256.949376	5.322560
4.890538	244.752610	5.327565
4.440481	244.199473	5.332570
4.215467	238.777195	5.337574
4.598621	244.889918	5.342579
4.710755	247.773592	5.347584
4.585653	237.707291	5.352589
4.650221	244.024637	5.357594
4.886835	239.837084	5.362598
4.737470	233.947458	5.367603
4.421439	231.658741	5.372608
4.497852	226.926672	5.377613
4.421903	246.034507	5.382618
4.575221	242.394585	5.387622
4.945040	252.467152	5.392627
4.759875	251.974011	5.397632
4.933403	252.693659	5.402637
4.882410	251.885406	5.407642
5.219469	249.706969	5.412646
4.979051	235.881187	5.417651
4.296116	240.230050	5.422656
4.352445	229.600843	5.427661
4.793110	247.315318	5.432666
4.940867	253.727280	5.437670
4.992950	264.232131	5.442675
4.714291	251.472125	5.447680
5.250683	241.850146	5.452685
4.493959	236.728947	5.457690
4.489008	240.035801	5.462694
4.656911	247.934718	5.467699
4.757991	255.787097	5.472704
5.114499	253.488575	5.477709
4.831882	259.356956	5.482714
4.743202	259.791570	5.487718
4.741675	253.464477	5.492723
4.414040	261.741104	5.497728
4.887339	258.750533	5.502733
4.743861	255.656680	5.507738
4.919159	253.051022	5.512742
4.899810	255.800149	5.517747
4.769009	253.919177	5.522752
4.575906	254.518743	5.527757
5.047813	272.952862	5.532762
5.201390	280.151686	5.537766
4.885720	285.708853	5.542771
5.013512	278.488439	5.547776
5.400963	273.223886	5.552781
5.379339	289.093185	5.557786
5.530348	282.147559	5.562790
5.357402	269.639995	5.567795
4.873337	265.327367	5.572800
5.152308	257.415885	5.577805
4.632943	267.142860	5.582810
5.282371	268.196529	5.587814
5.445816	278.797942	5.592819
5.221125	279.367625	5.597824
5.547190	271.325422	5.602829
5.094325	274.458417	5.607834
5.101621	263.340125	5.612838
4.929643	270.323883	5.617843
5.346923	270.534192	5.622848
5.518930	282.010615	5.627853
5.377844	289.128772	5.632858
5.253551	280.014592	5.637862
5.283767	275.333994	5.642867
5.456845	287.667613	5.647872
5.296626	284.845276	5.652877
5.403825	279.602209	5.657882
5.479781	282.855346	5.662886
5.261338	282.927358	5.667891
5.296767	281.317889	5.672896
5.427524	284.236634	5.677901
5.446418	286.131942	5.682906
5.350506	277.889686	5.687910
5.519868	279.872295	5.692915
5.175202	280.859284	5.697920
5.436553	280.976814	5.702925
5.350126	287.187973	5.707930
5.514685	277.136660	5.712934
5.470209	282.790805	5.717939
5.287635	283.970851	5.722944
5.586584	278.954188	5.727949
5.334209	290.540983	5.732954
5.310447	279.405371	5.737958
5.657885	276.181298	5.742963
5.223702	285.442614	5.747968
5.443482	287.287663	5.752973
5.514588	289.956274	5.757978
5.433792	279.762830	5.762982
5.669380	274.417520	5.767987
5.476680	283.422941	5.772992
5.726713	284.965893	5.777997
5.730680	286.506029	5.783002
5.587816	287.752657	5.788006
5.934415	289.419777	5.793011
5.793984	292.871118	5.798016
6.086136	283.024559	5.803021
5.647004	290.182794	5.808026
5.593272	276.425988	5.813030
5.630329	276.274726	5.818035
5.436073	284.106662	5.823040
5.479294	292.195851	5.828045
6.098629	303.520384	5.833050
6.013359	304.416367	5.838054
6.166678	302.064056	5.843059
5.737408	288.213854	5.848064
5.960608	280.861527	5.853069
5.471475	279.612135	5.858074
5.916544	297.522123	5.863078
5.815594	297.642280	5.868083
5.913344	300.585149	5.873088
6.299285	298.772411	5.878093
5.812642	292.754948	5.883098
5.508331	292.517633	5.888102
5.807559	300.228451	5.893107
5.621284	307.524491	5.898112
6.154675	309.263768	5.903117
5.937540	307.576563	5.908122
6.241012	306.156308	5.913126
6.187542	304.943485	5.918131
5.815468	310.395549	5.923136
6.022439	311.505454	5.928141
5.769190	305.344083	5.933146
6.027963	309.334374	5.938150
6.093577	310.346068	5.943155
5.862677	310.261835	5.948160
5.987385	308.568862	5.953165
5.654638	310.139279	5.958170
5.848209	298.628138	5.963174
6.049795	300.868320	5.968179
6.058662	312.104412	5.973184
6.262037	309.266588	5.978189
5.754162	319.789054	5.983194
6.080125	320.307804	5.988198
6.222304	324.806625	5.993203
6.285178	336.012178	5.998208
6.422174	316.385461	6.003213
6.192272	315.804372	6.008218
6.041984	321.187107	6.013222
6.476821	324.210372	6.018227
6.275285	316.604627	6.023232
5.883498	311.132364	6.028237
6.158933	317.793384	6.033242
6.239312	323.127551	6.038246
6.195088	327.206150	6.043251
6.255223	334.890935	6.048256
6.389258	319.684361	6.053261
6.411570	321.171024	6.058266
6.234999	309.271426	6.063270
6.525927	304.015564	6.068275
6.233574	311.356595	6.073280
6.373856	310.866564	6.078285
6.305771	309.317501	6.083290
6.122487	315.986668	6.088294
6.085583	310.351584	6.093299
5.792239	308.533878	6.098304
6.325940	301.727974	6.103309
6.064227	309.494496	6.108314
5.977187	310.074385	6.113318
6.112224	310.648172	6.118323
5.549508	313.871042	6.123328
6.414737	311.834986	6.128333
6.043785	325.110695	6.133338
6.357856	324.561969	6.138342
6.422090	326.190799	6.143347
6.384087	322.112422	6.148352
6.423559	310.916326	6.153357
6.310731	305.226628	6.158362
6.358387	302.944550	6.163366
5.886397	308.972143	6.168371
6.120887	301.966057	6.173376
6.309360	300.437159	6.178381
6.140257	311.954056	6.183386
6.158021	305.823254	6.188390
5.852792	304.421843	6.193395
6.119057	313.140689	6.198400
6.355513	321.057439	6.203405
6.144231	322.874696	6.208410
6.501217	325.410218	6.213414
6.002696	315.509579	6.218419
6.059395	319.354168	6.223424
5.926115	312.788144	6.228429
6.495303	329.280487	6.233434
6.434086	324.920991	6.238438
5.922641	305.945728	6.243443
6.180236	322.363194	6.248448
6.167177	319.603358	6.253453
6.144969	334.283240	6.258458
6.072304	333.753598	6.263462
6.565592	327.858793	6.268467
6.023360	325.462916	6.273472
6.138357	324.979985	6.278477
6.073684	328.818163	6.283482
6.036486	335.556340	6.288486
6.460084	335.990288	6.293491
6.458554	341.881370	6.298496
6.326349	331.237165	6.303501
5.833549	331.320256	6.308506
6.005723	334.963375	6.313510
6.025179	325.450310	6.318515
6.059899	332.544276	6.323520
6.239686	337.888280	6.328525
6.212057	345.842994	6.333530
6.322385	342.700118	6.338534
6.423092	338.014856	6.343539
6.447398	335.299820	6.348544
6.364329	333.294351	6.353549
6.175157	319.172629	6.358554
6.216910	314.129563	6.363558
6.039039	309.114366	6.368563
6.064509	316.282531	6.373568
6.336544	325.459221	6.378573
6.207618	333.110168	6.383578
6.167791	330.322861	6.388582
6.635132	323.830995	6.393587
6.237769	320.938008	6.398592
6.084510	314.479497	6.403597
6.155573	312.304503	6.408602
5.981521	318.937433	6.413606
6.126066	307.348500	6.418611
5.803583	316.244434	6.423616
6.155047	321.039693	6.428621
6.479304	326.899028	6.433626
6.575351	323.179423	6.438630
6.774860	312.863225	6.443635
6.228744	312.236459	6.448640
6.098343	305.053070	6.453645
6.202709	306.333972	6.458650
6.140684	301.664565	6.463654
6.005876	304.153271	6.468659
6.011388	306.243650	6.473664
6.258164	301.235105	6.478669
6.008086	313.153744	6.483674
5.752056	312.981676	6.488678
6.351249	313.600252	6.493683
6.458444	334.078020	6.498688
6.512204	321.731271	6.503693
6.140906	312.130358	6.508698
6.111301	312.252061	6.513702
6.122537	314.037836	6.518707
5.981830	309.042162	6.523712
6.535318	308.728237	6.528717
6.252318	311.929702	6.533722
6.075937	312.934782	6.538726
6.208117	304.438706	6.543731
5.856568	311.475748	6.548736
6.534523	314.831310	6.553741
6.465737	303.756476	6.558746
5.865394	311.743398	6.563750
6.334548	306.124436	6.568755
6.246117	309.485428	6.573760
5.960808	308.738963	6.578765
6.138623	306.455602	6.583770
6.483814	315.013467	6.588774
6.388670	308.662966	6.593779
6.033577	312.717198	6.598784
6.020655	298.542741	6.603789
6.076960	313.030051	6.608794
6.352590	309.658967	6.613798
6.193559	301.031066	6.618803
6.078232	307.408080	6.623808
5.873967	308.689579	6.628813
6.362057	316.832899	6.633818
5.749581	322.733676	6.638822
6.352272	326.853919	6.643827
6.167698	324.532068	6.648832
6.030509	331.140280	6.653837
5.971173	342.089623	6.658842
6.049966	331.741591	6.663846
6.752555	328.465377	6.668851
6.317851	335.765307	6.673856
6.769867	331.857402	6.678861
6.237824	315.723172	6.683866
6.448126	319.815923	6.688870
6.499927	302.388599	6.693875
5.918917	307.060123	6.698880
6.008063	309.001443	6.703885
5.976350	301.125660	6.708890
5.910771	305.707442	6.713894
6.651872	305.538309	6.718899
6.426332	312.302637	6.723904
6.227839	303.968775	6.728909
6.235647	308.108869	6.733914
6.392622	303.585695	6.738918
6.459330	291.483719	6.743923
6.443917	303.286723	6.748928
6.378697	296.007769	6.753933
6.243566	302.356228	6.758938
5.949937	309.463344	6.763942
6.534280	306.787664	6.768947
6.276172	306.698176	6.773952
6.419269	303.578678	6.778957
6.299113	303.758771	6.783962
6.379182	307.998344	6.788966
6.396005	288.323930	6.793971
6.249380	308.233759	6.798976
6.682778	301.924352	6.803981
6.450691	284.503281	6.808986
6.151242	282.895332	6.813990
6.528816	277.249509	6.818995
6.057222	292.125872	6.824000
6.231535	280.351991	6.829005
6.338326	282.996063	6.834010
6.052746	276.362018	6.839014
6.145651	280.210453	6.844019
5.981706	282.055136	6.849024
5.970004	282.794135	6.854029
6.258815	284.770802	6.859034
6.092566	288.865227	6.864038
6.372022	283.415009	6.869043
5.829838	280.281991	6.874048
6.108153	301.963754	6.879053
6.086820	312.752141	6.884058
6.335258	319.844464	6.889062
6.930399	308.859241	6.894067
6.293818	300.188637	6.899072
6.304568	287.519583	6.904077
6.144125	293.713796	6.909082
6.111259	291.573968	6.914086
6.463231	279.712317	6.919091
5.736530	288.025780	6.924096
5.934538	281.351241	6.929101
6.321188	283.050089	6.934106
5.801793	291.116145	6.939110
5.997361	299.820683	6.944115
6.185243	311.471820	6.949120
6.018138	314.920991	6.954125
6.310669	315.457601	6.959130
5.946154	316.074366	6.964134
6.373071	304.941334	6.969139
5.850593	308.461653	6.974144
6.205652	311.636539	6.979149
6.394394	302.283787	6.984154
6.018830	315.999961	6.989158
6.626784	309.381805	6.994163
6.284622	321.210386	6.999168
6.203972	315.439746	7.004173
6.329572	315.603721	7.009178
5.797964	314.886113	7.014182
6.265443	312.829729	7.019187
6.075385	309.480533	7.024192
6.355500	309.781799	7.029197
6.233139	314.157293	7.034202
5.955237	315.092760	7.039206
6.180090	314.292175	7.044211
6.190063	313.458607	7.049216
6.401120	312.827845	7.054221
6.336066	312.714627	7.059226
6.303656	315.446814	7.064230
6.299991	317.896121	7.069235
6.429337	310.352755	7.074240
6.210321	300.642719	7.079245
5.959503	299.688408	7.084250
5.940457	305.686607	7.089254
6.113805	304.840258	7.094259
5.792587	320.847979	7.099264
6.334261	309.023210	7.104269
6.492902	315.094984	7.109274
5.963222	312.450387	7.114278
6.568001	311.967127	7.119283
6.178670	319.149257	7.124288
6.110109	304.625961	7.129293
6.563658	311.148518	7.134298
6.302784	307.807184	7.139302
6.380886	294.127912	7.144307
5.854450	298.493551	7.149312
6.286986	294.762690	7.154317
5.856542	298.471153	7.159322
6.416388	306.008521	7.164326
6.801193	302.398983	7.169331
6.430855	306.518861	7.174336
6.074837	296.140474	7.179341
6.244396	290.659909	7.184346
5.755208	290.375450	7.189350
6.302855	287.601084	7.194355
5.929885	287.130855	7.199360
5.722698	290.399604	7.204365
6.125403	297.480554	7.209370
6.054458	296.510893	7.214374
6.526041	308.529137	7.219379
6.366737	306.874056	7.224384
6.643149	300.655529	7.229389
6.488622	290.732982	7.234394
6.467831	288.439417	7.239398
6.195460	285.596577	7.244403
6.054230	289.573214	7.249408
5.964197	287.999097	7.254413
6.080230	282.014351	7.259418
5.695327	298.769107	7.264422
6.430321	303.314825	7.269427
6.179311	301.243761	7.274432
6.136777	289.301161	7.279437
6.206551	299.774805	7.284442
6.149248	298.088025	7.289446
6.264398	304.369044	7.294451
6.282076	308.267161	7.299456
6.343207	286.105516	7.304461
6.375712	286.916724	7.309466
6.190337	284.699404	7.314470
5.778727	282.235740	7.319475
5.968227	298.790334	7.324480
6.249469	298.123335	7.329485
6.449576	309.750422	7.334490
5.977906	310.852097	7.339494
6.061860	304.964084	7.344499
6.118925	305.932817	7.349504
6.204691	303.708080	7.354509
6.122809	316.255418	7.359514
5.982803	313.284399	7.364518
6.131945	299.787048	7.369523
6.155079	309.486528	7.374528
6.058243	309.305493	7.379533
6.226123	308.681453	7.384538
6.048706	317.757278	7.389542
5.989387	303.605859	7.394547
5.955052	310.615657	7.399552
6.015798	327.149196	7.404557
6.394166	308.772531	7.409562
6.126664	321.045058	7.414566
6.217626	301.786185	7.419571
6.127692	312.654854	7.424576
6.392749	310.933701	7.429581
6.017703	309.685526	7.434586
6.002163	309.317831	7.439590
5.988302	305.374901	7.444595
6.031067	306.877361	7.449600
5.988108	305.640755	7.454605
6.036774	305.838855	7.459610
6.040779	307.945288	7.464614
6.682363	313.125636	7.469619
6.335040	321.778672	7.474624
6.385040	310.312023	7.479629
6.093233	306.703428	7.484634
6.076567	305.159014	7.489638
6.393199	304.628871	7.494643
5.882540	307.435519	7.499648
5.794720	314.719397	7.504653
6.042738	314.294848	7.509658
6.106370	333.197550	7.514662
6.329308	335.583105	7.519667
6.505411	333.727106	7.524672
6.488925	322.394185	7.529677
6.129875	320.865114	7.534682
6.148548	319.558801	7.539686
6.124192	308.540320	7.544691
5.998298	310.125986	7.549696
6.089323	309.381038	7.554701
6.375494	314.281372	7.559706
6.092130	311.785082	7.564710
6.162557	314.953666	7.569715
6.032718	322.288380	7.574720
6.515856	320.840151	7.579725
6.355420	315.448922	7.584730
6.152002	312.465630	7.589734
6.471194	305.101511	7.594739
6.341206	309.092221	7.599744
6.323813	300.429613	7.604749
6.432356	304.285109	7.609754
6.069240	317.958218	7.614758
6.425052	307.200081	7.619763
6.072932	310.665403	7.624768
6.384263	303.596732	7.629773
6.375123	309.068217	7.634778
5.958998	313.704580	7.639782
6.581303	301.095321	7.644787
6.321299	309.083035	7.649792
6.385815	316.577309	7.654797
6.315454	314.652120	7.659802
6.237053	306.739312	7.664806
6.403347	309.503834	7.669811
6.333329	315.462517	7.674816
6.295330	313.946733	7.679821
6.471009	308.224769	7.684826
5.991705	313.237958	7.689830
6.363665	302.537419	7.694835
6.300823	309.785769	7.699840
6.164893	296.734594	7.704845
6.168571	299.065698	7.709850
5.930082	304.519108	7.714854
6.091500	307.607086	7.719859
6.214584	308.518085	7.724864
6.400027	318.619396	7.729869
6.508635	312.060004	7.734874
6.387395	297.696772	7.739878
6.015852	285.587105	7.744883
5.983024	285.728292	7.749888
6.145725	302.533830	7.754893
6.214496	310.087549	7.759898
5.986382	306.573438	7.764902
6.321908	306.179556	7.769907
6.005007	315.694704	7.774912
5.930091	310.239543	7.779917
6.242389	313.449560	7.784922
6.279914	313.219132	7.789926
6.442908	308.441924	7.794931
6.302668	311.295301	7.799936
6.113103	310.815498	7.804941
6.165192	303.739736	7.809946
6.446413	315.755986	7.814950
6.288782	295.757556	7.819955
6.308742	303.875681	7.824960
6.094473	291.956654	7.829965
6.445980	287.880913	7.834970
6.103408	289.604715	7.839974
6.219896	285.495965	7.844979
6.081350	283.891437	7.849984
6.084076	282.555973	7.854989
5.926919	288.819273	7.859994
6.183543	302.465480	7.864998
6.274645	298.993418	7.870003
6.164340	313.323174	7.875008
6.282064	311.457285	7.880013
6.425406	312.346148	7.885018
6.551796	305.575185	7.890022
6.382447	289.729351	7.895027
6.401257	280.222738	7.900032
5.978120	289.241895	7.905037
6.029201	283.754470	7.910042
6.159718	285.224283	7.915046
6.238577	275.815888	7.920051
5.992246	284.098849	7.925056
6.297345	286.066653	7.930061
6.386792	279.263488	7.935066
6.164342	284.562537	7.940070
6.317889	277.252693	7.945075
5.832634	283.886608	7.950080
5.775595	280.814093	7.955085
6.028140	287.832999	7.960090
6.025293	300.643262	7.965094
6.248347	299.583534	7.970099
6.079807	307.190018	7.975104
6.312683	305.768100	7.980109
6.362702	299.404492	7.985114
6.270421	309.397182	7.990118
6.608342	305.137823	7.995136
5.765094	299.342894	8.000154
5.994905	304.791619	8.005171
6.208168	306.367819	8.010189
6.016861	315.258631	8.015206
6.095312	310.563509	8.020224
5.938580	317.407250	8.025242
6.040194	309.982063	8.030259
6.056698	311.427961	8.035277
5.886103	312.874590	8.040294
5.843450	311.464393	8.045312
6.088989	308.964815	8.050330
5.850745	310.860607	8.055347
6.366505	321.206523	8.060365
6.218917	326.430009	8.065382
6.434660	326.251296	8.070400
6.402179	329.714957	8.075418
6.301401	322.100382	8.080435
6.048336	315.383629	8.085453
6.034438	325.275557	8.090470
6.550233	324.867101	8.095488
6.158495	333.918509	8.100506
6.422464	336.449283	8.105523
6.371564	331.442954	8.110541
6.568294	339.585435	8.115558
6.362402	330.415721	8.120576
6.296457	320.025084	8.125594
6.569003	322.712302	8.130611
6.431973	310.666569	8.135629
6.279734	318.355318	8.140646
6.608441	313.005884	8.145664
6.528817	312.664889	8.150682
6.179364	313.653399	8.155699
6.314714	307.570411	8.160717
6.228777	312.800072	8.165734
6.076266	310.775856	8.170752
6.373800	315.201086	8.175770
6.091121	330.953835	8.180787
6.367078	328.099244	8.185805
6.498172	327.750685	8.190822
6.584226	325.373760	8.195840
6.385919	328.175312	8.200858
6.433021	336.811277	8.205875
6.381665	336.352277	8.210893
6.601940	347.198624	8.215910
6.456089	330.569122	8.220928
6.546504	329.513725	8.225946
6.427834	333.748156	8.230963
6.364247	317.787473	8.235981
6.219877	326.405910	8.240998
6.780084	334.838915	8.246016
6.681901	332.932462	8.251034
6.273844	319.486800	8.256051
6.587918	316.263379	8.261069
6.429211	313.593223	8.266086
6.444584	315.165523	8.271104
6.160860	320.186154	8.276122
6.453112	332.185711	8.281139
6.624659	337.053416	8.286157
6.404471	338.738129	8.291174
6.539210	330.884921	8.296192
6.770772	337.535678	8.301210
6.206255	342.735726	8.306227
6.608225	336.182051	8.311245
6.536288	343.760484	8.316262
6.873161	334.048695	8.321280
6.769385	336.702993	8.326298
6.409623	330.741264	8.331315
6.260490	315.122088	8.336333
6.526595	333.253938	8.341350
6.748374	329.552607	8.346368
6.723311	329.717483	8.351386
6.178448	324.674462	8.356403
6.982776	328.695760	8.361421
6.487481	334.572954	8.366438
6.575249	328.128159	8.371456
6.553370	328.336718	8.376474
6.192052	343.653624	8.381491
6.572595	336.784567	8.386509
6.218100	341.447014	8.391526
6.134026	340.601811	8.396544
6.642252	336.739121	8.401562
6.415263	342.836461	8.406579
6.229907	338.327564	8.411597
6.119274	344.012334	8.416614
6.506285	338.098425	8.421632
6.844502	338.307720	8.426650
6.707552	342.557621	8.431667
7.147460	348.819357	8.436685
6.764374	341.633716	8.441702
6.873961	340.916141	8.446720
6.931015	336.700843	8.451738
6.563087	337.240976	8.456755
6.889994	332.715436	8.461773
6.860504	338.744156	8.466790
6.409075	341.518853	8.471808
6.999295	338.009449	8.476826
6.599820	341.590208	8.481843
6.682844	337.793721	8.486861
6.552473	334.229264	8.491878
6.456233	346.816307	8.496896
6.958927	329.442082	8.501914
7.037140	344.671621	8.506931
7.185735	332.186949	8.511949
7.150407	343.054157	8.516966
6.733579	339.026243	8.521984
6.952761	341.374653	8.527002
6.594194	343.705725	8.532019
6.838561	338.426217	8.537037
6.896861	341.976725	8.542054
7.236643	329.654781	8.547072
6.958500	326.290048	8.552090
6.514946	315.450151	8.557107
6.668059	322.778953	8.562125
6.887221	340.340640	8.567143
6.513675	334.163317	8.572160
6.752620	328.827855	8.577178
6.695224	340.660962	8.582195
6.932075	337.802991	8.587213
7.149497	326.361587	8.592231
7.085475	328.365947	8.597248
7.266344	329.764166	8.602266
6.518312	326.295879	8.607283
6.688530	313.091526	8.612301
6.988688	325.522168	8.617319
6.940910	336.284018	8.622336
6.970303	326.698997	8.627354
6.383908	322.653309	8.632371
6.601595	326.494561	8.637389
7.125951	327.773032	8.642407
6.919035	331.762440	8.647424
7.001320	341.197614	8.652442
6.737226	336.877692	8.657459
6.861992	332.942170	8.662477
6.637727	329.957190	8.667495
6.699858	334.182404	8.672512
6.930796	330.113594	8.677530
7.018677	336.051460	8.682547
6.836995	328.894423	8.687565
7.072808	335.380425	8.692583
6.805064	341.563000	8.697600
6.889873	331.846278	8.702618
6.733505	334.969487	8.707635
6.898317	337.708193	8.712653
6.912844	331.353691	8.717671
6.806074	332.730426	8.722688
7.275675	327.690393	8.727706
6.884721	328.761100	8.732723
7.007429	332.576118	8.737741
7.329837	333.630426	8.742759
6.728608	336.172839	8.747776
6.815128	327.733883	8.752794
6.832390	327.879547	8.757811
6.498900	331.560477	8.762829
6.997478	330.753937	8.767847
6.752155	330.990975	8.772864
6.951759	340.439438	8.777882
7.310664	355.265543	8.782899
7.481258	353.279372	8.787917
7.204205	346.023574	8.792935
6.829112	336.315343	8.797952
6.775941	336.920072	8.802970
7.143493	335.947750	8.807987
7.273402	348.868793	8.813005
7.008309	332.866891	8.818023
7.052367	346.738520	8.823040
7.299057	338.520759	8.828058
7.185834	340.409712	8.833075
6.921556	329.188463	8.838093
7.252105	332.339996	8.843111
7.132832	339.916330	8.848128
7.255141	332.989656	8.853146
6.995873	339.745235	8.858163
7.411010	341.267918	8.863181
6.959177	333.733241	8.868199
6.734765	333.181272	8.873216
7.350072	348.955161	8.878234
7.311445	355.947778	8.883251
7.172230	349.339511	8.888269
7.139307	344.709055	8.893287
7.258525	349.521798	8.898304
7.155064	342.355732	8.903322
7.318063	348.720539	8.908339
7.099203	340.909759	8.913357
7.226966	347.863843	8.918375
7.083122	361.414464	8.923392
7.445621	352.598030	8.928410
7.366076	351.881501	8.933427
7.212733	341.687486	8.938445
7.161681	347.672233	8.943463
7.294416	348.528868	8.948480
7.162157	348.312825	8.953498
7.038918	361.898106	8.958515
7.416706	362.038128	8.963533
7.449826	358.889999	8.968551
7.010446	350.384598	8.973568
7.383890	362.848034	8.978586
7.667400	368.398866	8.983603
6.903273	348.391259	8.988621
7.422914	350.124877	8.993639
7.480594	358.976944	8.998656
7.073007	349.930136	9.003674
6.988356	355.793891	9.008691
7.500386	361.851909	9.013709
7.145337	355.864192	9.018727
6.944308	369.663551	9.023744
7.548977	355.211318	9.028762
7.509542	361.683383	9.033779
7.627929	363.668814	9.038797
7.224015	356.464320	9.043815
7.174131	364.812458	9.048832
7.610761	365.451375	9.053850
7.163995	375.991363	9.058867
7.258122	369.009106	9.063885
7.353534	363.945275	9.068903
7.223170	368.913642	9.073920
7.573248	361.645397	9.078938
7.231223	370.641749	9.083955
7.748044	376.522311	9.088973
7.337826	364.828328	9.093991
7.472200	370.743189	9.099008
7.523492	371.000313	9.104026
7.316839	362.067373	9.109043
7.565013	376.314321	9.114061
7.684987	365.724306	9.119079
7.941323	368.776953	9.124096
7.763734	358.135448	9.129114
7.775732	360.686522	9.134131
6.886167	341.730345	9.139149
7.195466	362.165420	9.144167
7.378425	353.828194	9.149184
7.687636	362.044686	9.154202
7.629832	368.708952	9.159219
7.298828	367.630808	9.164237
7.798606	366.779902	9.169255
7.720054	364.504335	9.174272
7.214436	358.754643	9.179290
7.528131	365.910147	9.184307
7.558736	365.441541	9.189325
7.551018	358.273184	9.194343
7.402635	365.298671	9.199360
7.519196	364.311780	9.204378
7.751756	366.405660	9.209395
7.433519	357.957129	9.214413
7.432788	365.877916	9.219431
7.118377	364.311222	9.224448
7.463616	366.507472	9.229466
7.539151	360.806144	9.234483
7.845814	374.119384	9.239501
7.618875	364.299712	9.244519
7.340780	373.447049	9.249536
7.518002	361.409155	9.254554
7.396048	361.311421	9.259571
7.235158	367.922313	9.264589
7.540174	357.600122	9.269607
7.608293	368.656355	9.274624
8.081795	370.990418	9.279642
7.954050	373.285556	9.284659
7.530864	378.763394	9.289677
7.608889	368.511251	9.294695
7.549413	377.450992	9.299712
7.716456	368.463021	9.304730
7.290371	370.552159	9.309747
7.785220	382.977773	9.314765
8.122870	382.615987	9.319783
7.747606	374.315175	9.324800
7.407040	378.041395	9.329818
7.517553	370.557996	9.334835
7.201898	384.514061	9.339853
7.661894	379.024252	9.344871
7.895832	389.903210	9.349888
7.896508	389.025875	9.354906
8.415863	392.192200	9.359923
7.728624	388.941641	9.364941
7.425160	378.729954	9.369959
7.526801	390.913854	9.374976
7.812711	393.800963	9.379994
8.056706	388.840217	9.385011
7.970712	395.038692	9.390029
7.857945	395.586434	9.395047
7.591625	398.278672	9.400064
7.637490	390.155268	9.405082
8.216140	392.056418	9.410099
8.254767	394.776912	9.415117
7.967894	372.325087	9.420135
7.824761	368.850968	9.425152
7.327764	366.375479	9.430170
7.713096	371.089993	9.435187
7.650420	384.293497	9.440205
7.997156	387.770705	9.445223
8.035821	396.827713	9.450240
8.027039	392.427002	9.455258
7.901234	394.046535	9.460275
8.045114	392.490531	9.465293
8.016130	393.659510	9.470311
7.756458	385.406964	9.475328
7.599828	394.181969	9.480346
8.020657	388.597275	9.485363
7.575495	386.953112	9.490381
7.886579	388.217459	9.495399
7.954559	390.788222	9.500416
7.719849	390.099006	9.505434
8.029044	390.656785	9.510451
7.618919	395.444666	9.515469
8.007322	396.797956	9.520487
7.699701	386.564823	9.525504
7.941978	396.577842	9.530522
7.932755	390.924413	9.535539
7.865857	394.832078	9.540557
7.796256	387.692278	9.545575
7.867113	396.264616	9.550592
7.717851	394.362953	9.555610
8.285360	392.687346	9.560627
8.146390	408.455657	9.565645
8.360793	403.695164	9.570663
8.053424	400.650531	9.575680
8.198670	393.795997	9.580698
8.032708	388.110171	9.585715
7.891703	395.339637	9.590733
8.102167	380.503815	9.595751
7.938875	385.505713	9.600768
7.959824	392.167193	9.605786
8.393569	389.603589	9.610803
7.777918	401.107111	9.615821
8.356110	402.427696	9.620839
8.140180	391.318795	9.625856
7.772689	397.605278	9.630874
8.240520	406.794275	9.635891
8.059441	421.723443	9.640909
8.362576	416.235956	9.645927
8.432590	409.610869	9.650944
8.091867	407.451852	9.655962
8.136450	391.849782	9.660979
8.038687	404.916760	9.665997
8.249737	401.090859	9.671015
8.121563	404.884997	9.676032
8.218966	425.331046	9.681050
8.477255	406.742008	9.686067
8.131677	413.438474	9.691085
8.160150	403.127757	9.696103
8.464755	398.119704	9.701120
8.027031	405.960232	9.706138
8.312724	399.667622	9.711155
8.035921	416.271555	9.716173
8.498268	407.366968	9.721191
8.381281	397.760521	9.726208
8.002736	398.157149	9.731226
8.434511	389.916859	9.736243
8.391855	406.676821	9.741261
8.055625	404.507638	9.746279
8.234957	396.372918	9.751296
8.310542	405.531472	9.756314
8.661285	405.486367	9.761331
8.462899	397.328409	9.766349
8.186430	398.090977	9.771367
8.515502	400.782028	9.776384
8.185579	383.647833	9.781402
8.377377	394.391351	9.786419
8.241474	388.637732	9.791437
8.459534	393.447721	9.796455
8.753361	394.822047	9.801472
7.984894	394.171756	9.806490
8.373918	390.438062	9.811507
8.587596	400.376645	9.816525
8.511703	397.059300	9.821543
8.318245	382.677664	9.826560
8.115159	387.127211	9.831578
8.375901	395.900346	9.836595
8.521725	408.408721	9.841613
8.647947	406.479944	9.846631
8.527795	392.945220	9.851648
8.131070	391.233558	9.856666
8.467276	397.609283	9.861683
8.185609	411.332871	9.866701
8.421865	410.522992	9.871719
8.932222	417.155617	9.876736
8.959654	411.919329	9.881754
8.912661	399.313592	9.886771
8.890772	390.140443	9.891789
8.134714	390.955591	9.896807
8.340429	381.986837	9.901824
8.133245	387.364779	9.906842
8.296430	384.811744	9.911859
8.479896	402.388517	9.916877
8.607058	412.043948	9.921895
8.588667	415.107820	9.926912
8.537413	412.518744	9.931930
8.679972	405.484753	9.936947
8.507420	411.693555	9.941965
8.783380	414.396033	9.946983
8.624586	409.119318	9.952000
8.480908	408.015161	9.957018
8.295165	406.201224	9.962035
8.634619	414.627615	9.967053
8.660272	419.148848	9.972071
8.745848	414.310585	9.977088
8.554741	412.964518	9.982106
8.890653	416.080518	9.987123
8.807265	414.929107	9.992141
8.643569	417.318206	9.997159
8.663409	411.666556	10.002176
8.610853	407.193767	10.007194
9.003734	413.058926	10.012211
8.648019	402.413572	10.017229
8.260805	396.424538	10.022247
8.591816	400.368076	10.027264
8.388404	404.612561	10.032282
8.482438	408.075472	10.037299
8.731392	409.226425	10.042317
8.543723	408.697133	10.047335
8.807943	404.105599	10.052352
8.738662	414.918180	10.057370
9.140366	408.907290	10.062387
8.876843	414.764202	10.067405
8.716485	413.040981	10.072423
9.075780	409.570674	10.077440
8.875792	406.752306	10.082458
8.925774	414.759888	10.087475
9.033928	406.652023	10.092493
8.457559	418.446071	10.097511
8.477628	410.626460	10.102528
8.788332	413.938879	10.107546
8.808498	418.318962	10.112563
8.828847	411.221949	10.117581
8.735802	415.493433	10.122599
8.844406	409.692271	10.127616
8.408018	418.062743	10.132634
8.598920	405.596678	10.137651
8.836903	411.378662	10.142669
8.805465	412.112547	10.147687
9.059547	409.633714	10.152704
8.791795	417.536141	10.157722
8.836464	413.089236	10.162739
8.620203	413.754072	10.167757
8.585438	410.244138	10.172775
8.852118	409.066624	10.177792
8.992136	427.417007	10.182810
8.907365	425.612592	10.187827
8.831104	432.860394	10.192845
8.789075	437.679333	10.197863
8.849152	434.258764	10.202880
9.128707	444.733042	10.207898
9.378519	438.824682	10.212915
9.157371	428.319299	10.217933
9.318491	423.059038	10.222951
9.230024	416.250351	10.227968
8.995798	413.948526	10.232986
9.147635	417.209945	10.238003
8.954312	403.626649	10.243021
8.596598	417.494619	10.248039
8.964371	403.050830	10.253056
8.976122	411.654468	10.258074
9.239572	425.700272	10.263091
9.071739	426.531129	10.268109
8.953994	425.706942	10.273127
9.224907	416.065335	10.278144
8.844596	421.915188	10.283162
8.752368	432.245383	10.288179
9.100059	436.381981	10.293197
8.880908	441.970076	10.298215
9.168597	436.390318	10.303232
9.326117	432.986134	10.308250
9.161241	436.666079	10.313267
9.321000	438.402092	10.318285
9.215592	433.205415	10.323303
8.991561	431.883406	10.328320
9.156164	430.769117	10.333338
9.406051	435.186018	10.338355
9.107761	434.068065	10.343373
9.280980	440.298777	10.348391
9.362301	421.317576	10.353408
9.224653	426.318649	10.358426
8.976574	425.650447	10.363443
9.581003	432.634485	10.368461
9.416791	436.907587	10.373479
9.593567	427.050269	10.378496
9.271358	419.700490	10.383514
9.188352	419.495712	10.388531
9.096118	412.955842	10.393549
8.974251	426.357931	10.398567
9.392395	426.576873	10.403584
9.278282	430.883196	10.408602
9.344794	431.475606	10.413619
9.395951	420.678534	10.418637
9.551037	432.614313	10.423655
9.348538	427.978681	10.428672
9.225692	427.098486	10.433690
9.105366	429.512391	10.438707
9.342108	428.588832	10.443725
9.325833	432.763164	10.448743
9.344704	437.383283	10.453760
9.346493	424.451212	10.458778
9.332889	430.335486	10.463795
9.696832	426.119721	10.468813
9.427506	427.979341	10.473831
9.453363	421.193876	10.478848
9.428454	429.812697	10.483866
9.164158	432.514092	10.488883
9.508812	429.475228	10.493901
9.225871	428.433776	10.498919
9.753288	424.031621	10.503936
9.799005	426.678436	10.508954
9.437115	438.211896	10.513971
9.441941	433.521893	10.518989
9.598167	436.340843	10.524007
9.324399	435.973271	10.529024
9.348810	445.114568	10.534042
9.087895	433.574010	10.539059
9.403660	430.183056	10.544077
9.257703	438.767082	10.549095
9.098931	433.443021	10.554112
9.341864	434.456064	10.559130
9.425825	429.643294	10.564147
9.276872	430.326051	10.569165
9.591135	435.285167	10.574183
9.523986	425.803481	10.579200
9.133357	441.175525	10.584218
9.683392	451.588760	10.589235
9.712797	453.307203	10.594253
9.882465	464.716895	10.599271
9.782957	456.694987	10.604288
9.829397	439.088749	10.609306
9.346985	435.642196	10.614323
9.685524	443.765802	10.619341
9.829113	447.495546	10.624359
9.966880	429.957145	10.629376
9.765854	435.839046	10.634394
9.077932	444.415943	10.639411
9.597751	440.677653	10.644429
9.676667	447.235458	10.649447
9.960525	456.585663	10.654464
9.995743	448.388155	10.659482
9.718803	443.890335	10.664499
9.475325	437.651701	10.669517
9.437549	442.728742	10.674535
9.622356	451.213941	10.679552
10.146445	455.607088	10.684570
9.822272	457.099729	10.689587
9.863778	457.910617	10.694605
9.885936	452.539446	10.699623
9.754140	436.646078	10.704640
9.801892	442.489247	10.709658
9.755359	441.783353	10.714675
9.633303	445.519745	10.719693
9.487269	452.974068	10.724711
9.990030	450.014721	10.729728
9.666410	456.385907	10.734746
10.059463	452.080401	10.739763
9.633243	446.094267	10.744781
9.874235	455.050378	10.749799
10.042826	452.373422	10.754816
9.823885	456.257438	10.759834
9.739396	457.094254	10.764851
9.794095	451.607569	10.769869
9.865945	459.261489	10.774887
10.208838	456.115603	10.779904
10.140992	459.139848	10.784922
9.936444	457.959963	10.789939
9.963545	452.105209	10.794957
9.869353	458.241869	10.799975
9.996630	456.341323	10.804992
9.825938	447.289137	10.810010
9.585820	462.539940	10.815027
10.309464	453.783986	10.820045
9.914476	451.156910	10.825063
10.265419	453.708871	10.830080
10.308018	458.530418	10.835098
10.237082	459.614420	10.840115
10.118581	457.950947	10.845133
9.999190	455.501855	10.850151
9.786149	454.424273	10.855168
10.057028	454.470494	10.860186
10.142608	465.653450	10.865203
10.168561	460.597251	10.870221
10.164582	455.353219	10.875239
9.862930	455.829390	10.880256
10.039320	456.360514	10.885274
9.621307	467.085418	10.890291
9.661539	456.981112	10.895309
10.131438	455.203938	10.900327
9.871435	450.599342	10.905344
10.147740	447.274487	10.910362
10.019630	459.910751	10.915379
10.200566	452.634092	10.920397
10.184909	448.092434	10.925415
9.906859	459.278356	10.930432
10.293395	450.697961	10.935450
9.757639	461.185586	10.940467
10.157329	471.388723	10.945485
10.287321	478.377224	10.950503
10.116901	485.021199	10.955520
10.367414	476.859581	10.960538
9.918749	480.072504	10.965555
10.453960	478.465030	10.970573
10.353417	473.583149	10.975591
10.475130	470.629480	10.980608
10.349127	477.771441	10.985626
10.501893	485.586335	10.990643
10.648270	473.483744	10.995661
10.256895	454.011244	11.000679
9.871234	465.854521	11.005696
10.200139	466.106291	11.010714
10.572443	477.014250	11.015731
10.314285	480.472053	11.020749
10.212903	480.472096	11.025767
10.317578	479.966709	11.030784
10.448495	478.908153	11.035802
10.314034	483.302860	11.040819
10.548238	476.772099	11.045837
10.384170	475.415506	11.050855
10.011016	475.921744	11.055872
10.263546	480.180461	11.060890
10.267191	480.419761	11.065907
10.705838	487.082511	11.070925
10.343202	489.417391	11.075943
9.822948	491.981930	11.080960
10.066310	474.827813	11.085978
10.188081	487.358922	11.090995
10.118721	483.368389	11.096013
10.158709	493.198375	11.101031
10.539931	500.374975	11.106048
10.531627	497.583550	11.111066
10.524155	508.301360	11.116083
10.480054	498.885472	11.121101
10.673894	500.635119	11.126119
10.640751	505.421137	11.131136
10.750916	499.704905	11.136154
10.979651	507.744655	11.141171
10.881019	491.988079	11.146189
10.815675	479.536613	11.151207
10.410111	490.792898	11.156224
10.671432	477.684687	11.161242
10.578253	481.369256	11.166259
10.640477	477.074229	11.171277
10.385661	479.190359	11.176295
10.006831	498.741855	11.181312
10.922613	491.890385	11.186330
10.786534	497.812685	11.191347
10.480503	499.135254	11.196365
10.713706	499.951010	11.201383
10.547857	504.505236	11.206400
11.014643	496.776974	11.211418
10.753069	503.005979	11.216435
10.819539	500.477453	11.221453
11.019197	497.644181	11.226471
10.699221	509.546685	11.231488
10.986072	491.969233	11.236506
10.872162	485.824012	11.241523
10.746814	472.207991	11.246541
10.978316	480.483972	11.251559
10.187949	485.788649	11.256576
10.860065	490.976072	11.261594
10.518798	493.102508	11.266611
10.678594	500.749064	11.271629
11.092390	494.285005	11.276647
10.662775	501.281752	11.281664
11.131647	488.314779	11.286682
10.898708	500.746498	11.291699
10.707037	497.958377	11.296717
11.244473	500.026894	11.301735
11.189366	506.211132	11.306752
11.283113	491.873050	11.311770
11.092402	482.464218	11.316787
10.983522	481.859544	11.321805
10.803506	479.697586	11.326823
10.604314	480.413413	11.331840
10.731609	477.196954	11.336858
10.816760	482.826041	11.341875
10.844724	500.676419	11.346893
11.005924	501.030037	11.351911
10.897026	501.315260	11.356928
11.422816	499.535690	11.361946
11.431036	499.812145	11.366963
11.014544	490.820297	11.371981
10.794881	484.606339	11.376999
10.921500	492.570468	11.382016
10.994681	488.374713	11.387034
11.036302	500.069439	11.392051
10.971787	497.501350	11.397069
11.185929	506.733054	11.402087
11.100656	500.586525	11.407104
11.101523	496.764928	11.412122
10.962162	499.418480	11.417139
10.954941	495.317289	11.422157
11.120268	494.253374	11.427175
11.231188	496.858491	11.432192
11.371424	498.749021	11.437210
11.418016	498.363125	11.442227
11.019386	501.946940	11.447245
11.336769	501.310610	11.452263
10.998730	497.620670	11.457280
11.039761	493.183778	11.462298
11.357835	502.279383	11.467315
11.346549	497.970551	11.472333
11.345019	491.034695	11.477351
10.983158	502.075910	11.482368
11.445236	498.851503	11.487386
11.140414	488.993398	11.492403
10.964347	503.511618	11.497421
11.356489	493.980476	11.502439
11.177644	501.231655	11.507456
11.214871	500.982911	11.512474
11.496905	500.948503	11.517491
11.105452	505.777685	11.522509
11.207465	497.560288	11.527527
11.037455	499.322405	11.532544
11.268673	499.406358	11.537562
11.285961	496.295382	11.542579
10.935100	493.030297	11.547597
11.343731	498.605868	11.552615
11.245159	495.976813	11.557632
11.008657	497.582034	11.562650
11.284529	501.322750	11.567667
11.360451	510.664335	11.572685
11.551424	510.028752	11.577703
11.581123	519.494297	11.582720
11.506681	520.537825	11.587738
11.778882	511.533410	11.592755
11.500571	509.560313	11.597773
11.452616	504.859575	11.602791
11.066711	498.807189	11.607808
11.307438	504.235343	11.612826
11.570253	510.155498	11.617843
11.694060	522.036250	11.622861
12.036495	519.171278	11.627879
11.385603	511.159457	11.632896
11.634834	508.558295	11.637914
11.621387	505.152316	11.642931
11.392855	507.059239	11.647949
11.753170	510.105188	11.652967
11.297945	506.771147	11.657984
11.840245	511.937765	11.663002
11.786404	513.025420	11.668019
11.758958	519.666082	11.673037
11.689233	496.956239	11.678055
11.467521	503.387311	11.683072
11.093101	498.727937	11.688090
11.364328	513.040830	11.693107
11.472657	517.621796	11.698125
11.947581	522.262445	11.703143
11.686052	525.190630	11.708160
11.694935	521.364624	11.713178
12.287098	519.558940	11.718195
11.721882	528.687947	11.723213
12.225583	520.013540	11.728231
11.879751	522.289006	11.733248
11.747742	504.467502	11.738266
11.644089	503.025764	11.743283
11.687518	514.095399	11.748301
11.868771	515.802828	11.753319
12.013188	513.820715	11.758336
12.028475	514.922853	11.763354
11.562496	505.739896	11.768371
11.312817	502.922937	11.773389
11.941529	509.227915	11.778407
12.332815	513.379834	11.783424
12.248953	510.609637	11.788442
12.006317	495.200511	11.793459
11.500813	492.619036	11.798477
11.456052	492.430392	11.803495
11.692750	509.765465	11.808512
11.672246	515.985342	11.813530
11.798816	508.022880	11.818547
12.070789	517.640043	11.823565
11.693845	518.452971	11.828583
11.910019	514.645182	11.833600
11.554486	516.448809	11.838618
12.296584	517.175866	11.843635
12.061644	517.789968	11.848653
11.866553	516.712743	11.853671
11.786971	524.402891	11.858688
11.732929	526.961117	11.863706
11.837353	516.272453	11.868723
11.597807	517.123946	11.873741
12.281302	529.697009	11.878759
12.173491	534.646132	11.883776
12.158777	532.919157	11.888794
12.169241	520.802982	11.893811
12.272806	521.234998	11.898829
11.667389	521.222003	11.903847
11.994031	524.939042	11.908864
12.228707	542.684698	11.913882
12.230514	544.675678	11.918899
12.228839	542.517501	11.923917
12.241653	539.590243	11.928935
12.514831	539.105954	11.933952
12.090403	538.073902	11.938970
12.127997	521.705981	11.943987
12.164278	538.308616	11.949005
12.368745	538.469314	11.954023
12.132140	540.276516	11.959040
12.616815	545.505762	11.964058
12.347271	530.271202	11.969075
12.203226	530.965822	11.974093
12.261802	525.418553	11.979111
12.408871	529.671613	11.984128
12.403354	518.955886	11.989146
12.373641	513.889405	11.994163
12.019422	521.183675	11.999181
12.015625	534.595863	12.004199
12.256049	532.939613	12.009216
12.397194	547.544174	12.014234
12.368451	542.247170	12.019251
12.634885	551.404487	12.024269
12.226000	538.305910	12.029287
12.583933	541.418504	12.034304
12.539321	549.478742	12.039322
12.508598	537.028157	12.044339
12.578584	543.284445	12.049357
12.285758	542.127766	12.054375
12.161081	547.470821	12.059392
12.414461	548.968216	12.064410
12.720009	551.918562	12.069427
12.204173	548.625507	12.074445
12.262187	549.332847	12.079463
12.183725	542.386861	12.084480
11.905836	555.169583	12.089498
12.244789	545.804478	12.094515
12.558628	554.825034	12.099533
12.395054	547.560952	12.104551
12.509474	554.280519	12.109568
12.811865	561.620891	12.114586
12.501333	549.501028	12.119603
12.579193	560.953477	12.124621
12.662672	560.738554	12.129639
12.874486	549.626069	12.134656
12.445342	553.321937	12.139674
12.780640	543.575567	12.144691
13.000619	543.702293	12.149709
12.856705	545.201588	12.154727
12.833625	545.034812	12.159744
12.838480	541.783759	12.164762
13.129918	540.684429	12.169779
12.796624	542.885366	12.174797
12.806191	552.010096	12.179815
12.675004	546.220979	12.184832
12.521354	546.462679	12.189850
12.592657	542.604860	12.194867
12.499387	542.407989	12.199885
12.463079	547.323893	12.204903
12.592362	543.766301	12.209920
12.796917	565.123594	12.214938
13.235744	566.522693	12.219955
12.853112	560.968371	12.224973
12.576581	549.875117	12.229991
13.013268	553.628675	12.235008
13.223024	552.617797	12.240026
12.855191	548.026809	12.245043
12.866236	547.141541	12.250061
12.688125	549.715930	12.255079
12.903836	544.488158	12.260096
12.808093	559.707098	12.265114
13.267887	563.198296	12.270131
13.087318	566.839686	12.275149
13.132150	547.535843	12.280167
12.987057	541.562708	12.285184
12.747099	549.221035	12.290202
12.790829	555.841161	12.295219
13.172967	554.143910	12.300237
13.077515	561.943838	12.305255
13.098719	566.601495	12.310272
13.094259	570.439519	12.315290
12.916600	560.997058	12.320307
12.815800	567.096916	12.325325
12.929490	571.430919	12.330343
12.857910	568.886009	12.335360
13.035203	568.684881	12.340378
13.163324	568.734394	12.345395
13.216663	578.578126	12.350413
13.195195	572.194431	12.355431
13.271176	575.436133	12.360448
13.145162	569.987015	12.365466
13.140490	565.487796	12.370483
13.298279	560.483623	12.375501
13.345374	568.283449	12.380519
13.191337	565.451590	12.385536
12.977311	571.253512	12.390554
12.991121	569.541026	12.395571
13.120859	565.500542	12.400589
13.148634	567.702066	12.405607
13.292072	572.167132	12.410624
12.766890	571.961772	12.415642
12.835534	573.421663	12.420659
13.261492	587.521185	12.425677
13.309270	591.818120	12.430695
13.690190	589.994828	12.435712
13.671111	593.150353	12.440730
12.999326	586.523935	12.445747
13.201210	592.280043	12.450765
13.380655	598.033334	12.455783
13.475401	598.154313	12.460800
13.446250	600.724452	12.465818
13.465198	597.285010	12.470835
13.126397	590.622525	12.475853
13.697430	594.752789	12.480871
13.864556	590.738034	12.485888
13.315242	588.144432	12.490906
13.457349	590.356559	12.495923
13.721490	587.645772	12.500941
13.620962	587.857112	12.505959
13.759154	585.503592	12.510976
13.002922	579.149091	12.515994
13.289438	582.979682	12.521011
13.462329	583.249433	12.526029
13.692639	596.694644	12.531047
13.679772	590.205465	12.536064
13.668832	594.823955	12.541082
13.486623	591.273828	12.546099
13.510575	588.082907	12.551117
13.569097	590.339605	12.556135
14.129823	592.647494	12.561152
13.932610	597.519039	12.566170
13.966711	593.480816	12.571187
13.910629	586.225228	12.576205
13.264257	577.710921	12.581223
13.578471	584.490908	12.586240
13.597351	590.161903	12.591258
13.513570	589.578562	12.596275
13.585111	588.450353	12.601293
13.458277	595.968015	12.606311
13.837681	589.484031	12.611328
13.687504	596.241656	12.616346
13.714916	597.458670	12.621363
13.753819	586.379395	12.626381
13.544943	600.473632	12.631399
13.957687	586.294081	12.636416
13.478327	593.604709	12.641434
13.668444	593.190154	12.646451
13.825766	597.028240	12.651469
13.594196	607.995588	12.656487
13.708579	608.167157	12.661504
13.804934	622.381138	12.666522
14.085075	611.179084	12.671539
14.332081	613.674671	12.676557
14.096380	622.004526	12.681575
13.955353	621.575258	12.686592
13.802025	618.607586	12.691610
13.508552	617.031297	12.696627
14.108069	619.121720	12.701645
13.597785	620.532903	12.706663
13.865698	614.766828	12.711680
13.901636	613.464287	12.716698
14.031279	623.507594	12.721715
14.442409	616.832475	12.726733
13.909469	613.971242	12.731751
14.236978	611.045466	12.736768
13.752142	622.683391	12.741786
14.085260	617.727640	12.746803
14.168517	622.874247	12.751821
14.132324	626.278585	12.756839
14.287106	621.735591	12.761856
14.287187	628.460367	12.766874
14.270273	625.149574	12.771891
14.223887	619.874228	12.776909
14.337462	617.814859	12.781927
14.444870	616.974541	12.786944
14.301188	612.878791	12.791962
14.250694	615.821469	12.796979
14.305234	613.004462	12.801997
14.020356	624.371424	12.807015
13.971527	621.845054	12.812032
14.128807	621.066396	12.817050
14.174092	624.366533	12.822067
14.349128	612.224672	12.827085
14.157017	619.929226	12.832103
14.064806	610.347208	12.837120
14.647985	628.445771	12.842138
14.236439	633.697821	12.847155
14.571226	630.322802	12.852173
14.380899	627.405068	12.857191
14.536568	637.116140	12.862208
14.703718	626.215681	12.867226
14.138369	616.148769	12.872243
14.704805	626.701560	12.877261
14.386742	626.432395	12.882279
14.519806	627.923284	12.887296
14.461704	622.144853	12.892314
14.015575	627.531669	12.897331
14.693719	634.794633	12.902349
14.645001	641.022102	12.907367
14.629835	644.902833	12.912384
14.477849	641.600445	12.917402
14.406531	649.002194	12.922419
14.846510	635.922853	12.927437
14.178312	642.628610	12.932455
14.417847	645.961621	12.937472
14.531825	642.668314	12.942490
14.623131	647.747406	12.947507
14.750575	637.184468	12.952525
14.810216	647.462741	12.957543
14.963602	641.436790	12.962560
14.780343	639.556172	12.967578
14.572667	644.621855	12.972595
14.580804	643.569784	12.977613
14.450037	645.060728	12.982631
14.748801	639.999871	12.987648
14.863258	644.725077	12.992666
14.625389	635.162567	12.997683
14.890896	639.340411	13.002701
14.856669	645.010225	13.007719
14.698453	643.482300	13.012736
14.843911	641.556814	13.017754
14.538883	652.188501	13.022771
14.822950	645.747741	13.027789
14.749596	645.039704	13.032807
14.367434	639.608356	13.037824
14.965072	656.789549	13.042842
14.793048	659.795336	13.047859
15.338348	664.964687	13.052877
15.092570	675.281062	13.057895
15.266551	678.075196	13.062912
15.199443	657.823021	13.067930
14.839699	655.853119	13.072947
15.042462	650.450614	13.077965
14.788845	648.448411	13.082983
15.274674	659.717489	13.088000
15.066087	648.866049	13.093018
14.631257	651.101742	13.098035
15.177576	659.148916	13.103053
15.476847	671.456867	13.108071
15.221972	661.496219	13.113088
15.178634	648.842400	13.118106
14.860577	648.131438	13.123123
15.413402	648.509287	13.128141
15.391291	650.677565	13.133159
14.963004	647.093160	13.138176
14.908725	651.832017	13.143194
14.966452	659.100073	13.148211
15.138094	656.741335	13.153229
15.336820	666.893827	13.158247
15.643570	660.610470	13.163264
15.367505	664.604407	13.168282
15.401223	651.929121	13.173299
15.103991	643.120591	13.178317
15.139496	657.003261	13.183335
15.598930	664.644259	13.188352
15.240892	658.833623	13.193370
15.287066	676.170121	13.198387
15.635138	669.949752	13.203405
15.425363	665.106916	13.208423
14.719521	650.072721	13.213440
15.164783	659.126514	13.218458
14.975580	670.630082	13.223475
15.372398	667.576745	13.228493
15.230951	675.465932	13.233511
15.297739	669.955208	13.238528
15.668904	656.018753	13.243546
15.443598	663.217273	13.248563
15.436840	668.232747	13.253581
15.788457	667.105105	13.258599
15.484281	673.252443	13.263616
15.868590	671.283454	13.268634
15.613488	673.103017	13.273651
15.805154	668.311281	13.278669
15.347073	670.670512	13.283687
15.626755	667.657503	13.288704
15.635492	670.534166	13.293722
15.834271	668.186980	13.298739
15.786409	667.787385	13.303757
15.815355	662.730663	13.308775
15.581112	667.071525	13.313792
15.669822	664.520579	13.318810
15.589832	669.604258	13.323827
15.603287	665.610257	13.328845
15.884377	665.339320	13.333863
15.424682	662.589747	13.338880
15.772286	668.847035	13.343898
15.457436	662.575255	13.348915
15.609436	657.612979	13.353933
15.549625	659.310620	13.358951
15.580639	680.253274	13.363968
16.061439	682.778740	13.368986
16.075825	686.538118	13.374003
15.969823	676.538504	13.379021
15.868065	671.088735	13.384039
15.804363	667.318178	13.389056
15.729107	671.268228	13.394074
16.011938	679.056645	13.399091
16.005884	677.107410	13.404109
16.016633	679.166438	13.409127
15.652146	681.337535	13.414144
16.239111	679.478998	13.419162
16.096847	683.871814	13.424179
15.957238	673.552398	13.429197
16.117396	681.552413	13.434215
16.043513	679.765211	13.439232
16.148199	676.037860	13.444250
16.432375	685.410226	13.449267
16.257561	676.683601	13.454285
15.982397	658.357232	13.459303
16.116779	658.497286	13.464320
16.082484	658.745650	13.469338
16.414799	664.809665	13.474355
16.248535	660.565946	13.479373
16.179601	647.811976	13.484391
15.990169	656.137798	13.489408
16.301208	650.254548	13.494426
16.043871	652.055523	13.499443
15.971110	657.213809	13.504461
16.081004	673.631547	13.509479
15.986035	676.401285	13.514496
16.397008	680.307191	13.519514
16.158841	679.031543	13.524531
16.173262	675.883114	13.529549
16.252288	676.243218	13.534567
16.118696	674.619942	13.539584
16.425527	668.175629	13.544602
16.235388	673.427932	13.549619
16.216078	676.192202	13.554637
16.285680	675.525019	13.559655
16.463976	676.103188	13.564672
16.309742	670.453313	13.569690
16.024421	683.341422	13.574707
16.020519	683.073833	13.579725
16.526247	685.753203	13.584743
16.151354	698.904569	13.589760
16.493914	696.658065	13.594778
16.624803	701.648961	13.599795
16.557242	696.834465	13.604813
16.697831	694.177611	13.609831
16.739751	710.833176	13.614848
16.861328	702.603171	13.619866
16.715854	708.072583	13.624883
16.481180	708.143870	13.629901
16.679419	704.099001	13.634919
16.484114	707.073708	13.639936
16.567990	703.933394	13.644954
16.924827	704.124017	13.649971
16.577736	709.113598	13.654989
16.676946	701.805383	13.660007
16.709620	706.177278	13.665024
16.709637	695.719349	13.670042
16.551648	704.848156	13.675059
16.466008	709.689737	13.680077
16.868795	704.536929	13.685095
16.890339	708.301509	13.690112
16.796179	702.399282	13.695130
16.734148	699.988562	13.700147
16.794304	710.519246	13.705165
16.875084	697.754552	13.710183
16.631582	709.070946	13.715200
16.781619	700.129636	13.720218
16.771323	704.527155	13.725235
16.838964	709.704620	13.730253
16.696248	704.529451	13.735271
16.968644	716.734324	13.740288
17.136991	717.976740	13.745306
17.152166	718.236337	13.750323
16.918109	717.928845	13.755341
16.916412	715.385656	13.760359
17.275384	730.117393	13.765376
17.178417	719.355825	13.770394
17.106668	698.552079	13.775411
17.081647	706.539914	13.780429
16.879364	698.679059	13.785447
17.112652	715.367947	13.790464
17.255234	718.984301	13.795482
17.430009	724.255539	13.800499
17.118693	720.741266	13.805517
17.205870	702.875970	13.810535
17.076201	704.303634	13.815552
17.459197	718.861214	13.820570
17.277767	709.898926	13.825587
17.018467	706.433360	13.830605
17.436542	721.998458	13.835623
17.106376	710.875586	13.840640
17.263673	726.951489	13.845658
17.388498	724.622121	13.850675
17.501041	721.638282	13.855693
17.585939	713.461318	13.860711
17.019016	715.288410	13.865728
17.459530	730.001140	13.870746
17.793906	723.612477	13.875763
17.115114	712.591219	13.880781
17.663879	707.425149	13.885799
17.426592	719.131887	13.890816
17.478267	723.330421	13.895834
17.526578	714.594283	13.900851
17.206751	722.971996	13.905869
17.502943	721.139793	13.910887
17.522346	722.774615	13.915904
17.462890	728.678750	13.920922
17.798904	729.484820	13.925939
17.581803	721.550526	13.930957
17.842583	720.872510	13.935975
17.436009	723.646592	13.940992
17.825852	722.370989	13.946010
17.640952	719.067400	13.951027
17.453190	724.477131	13.956045
17.664877	722.178420	13.961063
17.554640	722.141974	13.966080
17.461264	723.220018	13.971098
17.895624	726.093536	13.976115
17.531550	727.005452	13.981133
17.618448	707.562346	13.986151
17.667377	714.260614	13.991168
17.820708	719.248021	13.996186
17.799917	724.331965	14.001203
17.469483	726.352604	14.006221
17.457003	719.304760	14.011239
17.539065	722.996807	14.016256
17.823351	733.864981	14.021274
17.797711	737.106756	14.026291
17.903316	749.921425	14.031309
18.222612	745.696758	14.036327
18.054767	740.979911	14.041344
17.908987	737.869037	14.046362
17.986818	737.415158	14.051379
18.051351	751.375430	14.056397
18.462587	737.025587	14.061415
18.138253	730.903576	14.066432
17.850035	729.919731	14.071450
17.961044	721.454685	14.076467
17.735340	732.007799	14.081485
18.312313	735.187307	14.086503
18.240786	748.559711	14.091520
18.521755	738.708088	14.096538
18.313079	733.584204	14.101555
17.898230	733.244902	14.106573
18.107435	724.155517	14.111591
18.079784	732.273155	14.116608
18.387792	740.152351	14.121626
18.174638	743.770449	14.126643
18.098790	745.697805	14.131661
18.719063	741.782872	14.136679
18.468759	734.854098	14.141696
18.348242	731.654087	14.146714
18.633329	720.618447	14.151731
18.239197	729.922883	14.156749
18.120592	715.633461	14.161767
18.298664	723.501323	14.166784
17.982146	717.564286	14.171802
18.434032	724.285023	14.176819
17.965107	741.480885	14.181837
18.330389	741.670193	14.186855
18.439330	743.540377	14.191872
18.181805	737.376406	14.196890
18.324199	744.577668	14.201907
18.272415	752.020597	14.206925
18.260692	742.173519	14.211943
18.549044	738.073588	14.216960
18.600762	747.955535	14.221978
18.748230	753.985246	14.226995
18.552221	742.547985	14.232013
18.496808	742.503003	14.237031
18.676738	736.182562	14.242048
18.712434	744.770010	14.247066
18.599908	738.839074	14.252083
18.349207	741.039798	14.257101
18.238717	737.020899	14.262119
18.837106	757.638629	14.267136
18.697841	761.586043	14.272154
19.020777	760.342945	14.277171
18.838002	766.891122	14.282189
18.833103	768.829524	14.287207
19.157233	756.648573	14.292224
19.140336	766.127816	14.297242
19.090786	751.149138	14.302259
18.447519	743.227539	14.307277
18.732767	735.076174	14.312295
19.133981	745.689473	14.317312
18.783714	751.894506	14.322330
18.939185	746.833838	14.327347
18.663129	753.794152	14.332365
18.952717	754.061516	14.337383
19.152690	769.635368	14.342400
18.944915	771.043642	14.347418
19.125203	765.505750	14.352435
19.147136	773.192823	14.357453
19.211731	767.581427	14.362471
19.169873	771.201263	14.367488
18.852490	757.801108	14.372506
19.068557	765.338035	14.377523
19.170558	768.692482	14.382541
19.064417	769.652601	14.387559
19.366145	763.594044	14.392576
18.842260	762.044150	14.397594
19.106954	761.662159	14.402611
18.924937	774.174500	14.407629
18.730620	766.833066	14.412647
18.882762	771.423054	14.417664
18.972646	770.374026	14.422682
19.336428	763.308606	14.427699
18.922469	760.116409	14.432717
19.140884	778.344499	14.437735
19.532313	778.179454	14.442752
19.282268	788.042136	14.447770
19.663667	792.337668	14.452787
19.648410	794.902516	14.457805
19.550948	790.045314	14.462823
19.536942	772.369265	14.467840
19.341113	777.881252	14.472858
19.380109	768.114623	14.477875
19.502671	778.648254	14.482893
19.521440	775.994576	14.487911
19.535537	782.685671	14.492928
19.518028	782.060448	14.497946
19.700422	788.125757	14.502963
19.686111	780.036790	14.507981
19.650628	780.307431	14.512999
19.558640	766.212634	14.518016
19.330608	783.983238	14.523034
19.679149	781.543294	14.528051
19.746526	792.167574	14.533069
19.803538	793.600893	14.538087
20.057887	793.394076	14.543104
19.677625	793.759422	14.548122
19.879967	775.317562	14.553139
19.576368	777.091039	14.558157
19.637223	785.157053	14.563175
19.975422	779.465187	14.568192
19.751007	788.077375	14.573210
20.058010	788.995259	14.578227
19.969171	793.180974	14.583245
20.027108	793.405513	14.588263
19.941688	767.027680	14.593280
19.565269	779.156895	14.598298
19.737614	775.400055	14.603315
19.589615	786.127290	14.608333
19.613834	799.289170	14.613351
19.927897	788.438319	14.618368
19.763106	789.577978	14.623386
19.833117	787.455947	14.628403
19.839068	787.142642	14.633421
19.801097	792.390221	14.638439
20.285991	789.313684	14.643456
19.633392	804.963506	14.648474
20.546788	798.273234	14.653491
19.969301	806.249302	14.658509
20.208873	809.736968	14.663527
20.686614	802.161499	14.668544
20.224287	800.163372	14.673562
20.255761	792.404932	14.678579
19.925279	799.856561	14.683597
20.482586	806.261124	14.688615
20.305310	787.916224	14.693632
20.261420	789.185377	14.698650
20.174887	784.484261	14.703667
20.516856	802.671049	14.708685
20.376623	802.140670	14.713703
20.457500	801.153001	14.718720
20.222914	794.628843	14.723738
20.489475	810.391173	14.728755
20.713961	814.345078	14.733773
20.325146	806.380678	14.738791
20.703836	803.487926	14.743808
20.509032	803.527761	14.748826
20.575951	796.262403	14.753843
20.502669	792.199830	14.758861
20.200892	793.534381	14.763879
20.818595	805.243753	14.768896
20.647441	819.108234	14.773914
20.628271	816.675045	14.778931
20.791194	817.444955	14.783949
20.604241	816.745131	14.788967
20.911770	808.492436	14.793984
20.963096	806.764619	14.799002
20.636508	800.870147	14.804019
20.447494	795.314007	14.809037
20.532202	811.884112	14.814055
21.073414	812.225906	14.819072
20.625900	812.447093	14.824090
20.561408	811.321115	14.829107
20.884386	815.770911	14.834125
20.729613	820.383452	14.839143
20.891482	815.993936	14.844160
20.714654	819.407584	14.849178
20.826717	813.754071	14.854195
20.929729	809.316917	14.859213
20.902614	820.637560	14.864231
20.769552	807.688338	14.869248
20.683721	814.189881	14.874266
20.821123	816.633136	14.879283
20.570751	816.246134	14.884301
20.585293	812.002630	14.889319
20.758019	817.744416	14.894336
20.820729	832.146835	14.899354
21.199310	842.296670	14.904371
21.420931	829.752944	14.909389
21.269911	832.843849	14.914407
21.248471	833.882299	14.919424
21.092559	837.138064	14.924442
21.466164	834.372328	14.929459
21.404373	834.684934	14.934477
21.005354	831.310523	14.939495
21.592979	840.774577	14.944512
21.450240	833.286233	14.949530
21.072056	817.948423	14.954547
21.137905	821.371623	14.959565
21.374960	844.002255	14.964583
21.289291	844.836117	14.969600
21.156096	842.411211	14.974618
21.370963	833.118923	14.979635
21.387867	835.476803	14.984653
21.456595	835.920562	14.989671
21.551573	833.021488	14.994688
21.397308	840.250043	14.999706
21.275619	846.230176	15.004723
21.574751	835.324818	15.009741
21.213315	841.418015	15.014759
21.239937	839.088144	15.019776
21.379765	844.585759	15.024794
21.419309	844.409230	15.029811
21.613986	837.026137	15.034829
21.609443	844.237694	15.039847
21.700588	839.385826	15.044864
21.523555	837.223359	15.049882
21.585769	842.146095	15.054899
21.985175	849.973240	15.059917
21.809350	858.218145	15.064935
21.839170	846.928688	15.069952
21.909223	850.064069	15.074970
21.655925	857.664647	15.079987
22.015465	847.980607	15.085005
21.662770	860.314460	15.090023
22.126751	855.685397	15.095040
22.000947	863.269283	15.100058
21.977750	856.920467	15.105075
21.895199	843.183891	15.110093
21.891471	854.535627	15.115111
22.115576	848.782610	15.120128
22.155747	852.481206	15.125146
21.955822	849.082104	15.130163
22.131222	852.898497	15.135181
22.133914	850.768005	15.140199
21.937128	844.083313	15.145216
22.134768	852.361584	15.150234
21.803363	866.140602	15.155251
22.485877	857.879992	15.160269
22.303448	866.722360	15.165287
22.313698	850.544581	15.170304
22.520937	844.327145	15.175322
21.774316	837.276795	15.180339
21.957109	841.265599	15.185357
22.369099	849.362176	15.190375
22.489397	840.491696	15.195392
22.365914	851.126793	15.200410
22.406142	855.352386	15.205427
22.704781	845.008816	15.210445
22.243883	848.908499	15.215463
22.375299	837.249790	15.220480
22.299653	834.494042	15.225498
22.440435	851.124880	15.230515
22.617143	847.408369	15.235533
22.246068	855.891950	15.240551
22.351918	843.217920	15.245568
22.758772	841.068683	15.250586
22.731404	848.192280	15.255603
22.850914	849.019442	15.260621
22.746095	842.415103	15.265639
22.332123	847.355177	15.270656
22.441514	849.824889	15.275674
22.229002	853.007420	15.280691
22.666950	845.734766	15.285709
22.039944	852.285868	15.290727
22.475781	849.876504	15.295744
22.574371	853.004287	15.300762
22.604378	847.751692	15.305779
22.668593	847.176858	15.310797
22.922910	853.025869	15.315815
22.817062	845.487597	15.320832
22.678633	848.825846	15.325850
22.726729	868.948733	15.330867
23.104840	874.917329	15.335885
23.019907	876.202346	15.340903
22.985202	883.680540	15.345920
23.281300	873.504603	15.350938
22.742508	872.253658	15.355955
23.009913	859.835322	15.360973
22.735230	866.388378	15.365991
23.037594	871.251641	15.371008
22.908489	877.741011	15.376026
23.079180	879.222908	15.381043
22.965627	869.997513	15.386061
22.644715	870.053826	15.391079
22.805243	870.915627	15.396096
23.153933	869.684290	15.401114
22.702986	876.119630	15.406131
23.168073	870.994943	15.411149
22.987712	873.348829	15.416167
23.444112	894.146611	15.421184
23.397149	893.440766	15.426202
23.389817	895.543659	15.431219
23.498966	897.429605	15.436237
23.268999	891.277067	15.441255
23.484119	888.750588	15.446272
23.775597	895.082965	15.451290
23.218910	890.079490	15.456307
23.531416	883.422783	15.461325
23.518250	888.859028	15.466343
23.518388	884.141235	15.471360
23.402062	889.224322	15.476378
23.485026	891.546679	15.481395
23.441619	890.139709	15.486413
23.198494	904.533001	15.491431
23.041734	899.650288	15.496448
23.744142	898.202935	15.501466
23.791218	900.275266	15.506483
23.805356	897.480284	15.511501
23.924242	894.640591	15.516519
23.730153	895.169452	15.521536
23.716936	899.210877	15.526554
23.726772	896.684801	15.531571
23.799106	892.268182	15.536589
23.730340	891.354298	15.541607
23.889658	895.277343	15.546624
23.995793	893.790287	15.551642
23.639076	901.122969	15.556659
23.453668	897.753156	15.561677
23.433475	894.158808	15.566695
23.339589	891.977078	15.571712
24.071255	894.851670	15.576730
24.022575	914.677259	15.581747
24.256984	907.341597	15.586765
24.171165	911.252321	15.591783
24.222117	906.428783	15.596800
24.316080	896.584099	15.601818
24.141727	899.315740	15.606835
23.934006	888.422995	15.611853
24.117863	889.647229	15.616871
24.233928	884.542166	15.621888
24.239124	884.030167	15.626906
23.941553	882.069494	15.631923
24.376870	898.446240	15.636941
24.215034	911.195370	15.641959
24.044476	908.687911	15.646976
24.468417	911.484189	15.651994
24.688707	916.571677	15.657011
24.526336	908.376319	15.662029
24.448108	898.173445	15.667047
24.546414	898.237069	15.672064
24.292538	892.239729	15.677082
24.298725	901.071682	15.682099
24.584651	910.390247	15.687117
24.808941	911.753351	15.692135
24.157083	900.885568	15.697152
24.414332	898.096914	15.702170
24.504099	909.468841	15.707187
24.275876	903.458036	15.712205
24.909487	907.531295	15.717223
24.610828	918.215796	15.722240
24.725858	904.710337	15.727258
24.839027	915.015143	15.732275
24.513777	908.568174	15.737293
24.511807	914.264609	15.742311
24.330505	925.123341	15.747328
24.905931	908.567187	15.752346
24.996660	899.635010	15.757363
24.445687	910.980470	15.762381
24.736425	912.172286	15.767399
24.797387	906.990592	15.772416
24.630947	904.154297	15.777434
25.041778	907.952981	15.782451
24.509061	910.999189	15.787469
24.775335	925.212203	15.792487
24.581687	939.174951	15.797504
24.759051	932.870619	15.802522
24.900522	940.857882	15.807539
24.799149	940.826366	15.812557
24.861999	944.906450	15.817575
24.988578	939.506252	15.822592
25.451418	940.595537	15.827610
24.829647	939.650989	15.832627
25.224052	936.550647	15.837645
25.148160	935.139264	15.842663
25.064739	932.331064	15.847680
25.248985	933.208110	15.852698
25.546565	946.150817	15.857715
25.558342	933.971042	15.862733
25.180000	931.543267	15.867751
25.198395	930.707327	15.872768
25.443588	923.821250	15.877786
25.316007	936.877482	15.882803
25.300637	939.240401	15.887821
25.597784	945.783348	15.892839
25.529414	946.639767	15.897856
25.724420	943.523133	15.902874
25.413713	941.327819	15.907891
25.553923	947.137824	15.912909
25.931128	947.448353	15.917927
25.843351	933.472685	15.922944
25.903453	929.584969	15.927962
25.501274	935.290074	15.932979
25.603261	927.353343	15.937997
25.712765	923.830313	15.943015
25.246141	930.618399	15.948032
25.374836	938.724412	15.953050
25.584444	952.356148	15.958067
25.568945	952.838270	15.963085
25.752242	951.339196	15.968103
25.641236	950.908401	15.973120
25.943404	947.838197	15.978138
25.883553	959.441729	15.983155
25.644342	958.305076	15.988173
25.805191	954.682529	15.993191
26.092971	955.167924	15.998208
25.674484	950.742504	16.003226
25.679721	953.354676	16.008243
25.825984	957.743660	16.013261
26.018295	966.429905	16.018279
26.323288	973.953075	16.023296
26.397876	969.520307	16.028314
26.483172	967.821899	16.033331
25.795018	952.806783	16.038349
26.582907	957.597631	16.043367
25.967530	957.324259	16.048384
26.214831	960.327923	16.053402
26.358129	970.650161	16.058419
26.239828	972.199151	16.063437
26.637995	964.998913	16.068455
26.397573	968.848515	16.073472
26.471436	962.872705	16.078490
26.726439	961.160498	16.083507
26.062870	946.987297	16.088525
26.649455	944.456621	16.093543
26.369556	949.035030	16.098560
26.124172	955.542532	16.103578
26.479568	966.131539	16.108595
26.147937	965.387964	16.113613
26.273423	966.662316	16.118631
26.389123	974.473729	16.123648
26.871664	975.708269	16.128666
26.648472	976.087032	16.133683
26.250826	975.287464	16.138701
26.736262	966.883923	16.143719
26.807198	987.066501	16.148736
26.790563	969.090872	16.153754
27.467976	967.432814	16.158771
26.960798	971.538541	16.163789
26.907050	963.881655	16.168807
27.140438	965.221257	16.173824
27.061837	961.531850	16.178842
27.222220	963.545523	16.183859
27.094316	971.476913	16.188877
27.241219	964.543009	16.193895
27.251991	972.541168	16.198912
27.022763	950.795990	16.203930
27.147689	948.062643	16.208947
26.739702	957.684928	16.213965
27.193245	952.584106	16.218983
26.946804	971.462270	16.224000
26.930061	970.799053	16.229018
27.155803	975.462840	16.234035
27.026778	968.748616	16.239053
27.821872	972.392814	16.244071
26.843864	971.547909	16.249088
26.649748	971.694931	16.254106
27.043626	959.824868	16.259123
26.623759	968.199336	16.264141
27.324036	967.620138	16.269159
27.089740	977.597235	16.274176
27.341977	981.206037	16.279194
27.365006	985.850897	16.284211
27.519692	994.770226	16.289229
27.363689	990.931922	16.294247
27.235426	998.083910	16.299264
27.227786	995.244967	16.304282
27.567177	994.460030	16.309299
27.389912	985.484331	16.314317
27.617109	992.366383	16.319335
27.656982	1007.138565	16.324352
27.682231	995.373209	16.329370
27.572770	995.910986	16.334387
27.294083	998.277041	16.339405
27.275395	993.382273	16.344423
27.312475	1008.609319	16.349440
27.573793	1015.858446	16.354458
27.825126	1017.643373	16.359475
27.482181	1021.354318	16.364493
27.845948	1016.702948	16.369511
27.977872	1021.135206	16.374528
27.801175	1023.204524	16.379546
28.013350	1016.317240	16.384563
27.755304	1013.735028	16.389581
28.037287	1015.988546	16.394599
28.195225	1015.626327	16.399616
28.117523	1018.901506	16.404634
28.061594	1010.478093	16.409651
28.171391	1021.547177	16.414669
28.325037	1014.167243	16.419687
28.223339	1014.994141	16.424704
28.263129	1008.985752	16.429722
28.387181	1004.368553	16.434739
28.586372	1007.209305	16.439757
28.451334	1003.755891	16.444775
28.399721	1010.211153	16.449792
28.512991	1016.258901	16.454810
28.426049	1012.365659	16.459827
28.208874	1017.164688	16.464845
28.261349	1009.510179	16.469863
28.358695	1019.407263	16.474880
28.199314	1009.071796	16.479898
28.349726	1011.579323	16.484915
28.344684	1009.743501	16.489933
28.466836	1014.268795	16.494951
28.734052	1019.983312	16.499968
28.929762	1022.518502	16.504986
28.958156	1010.875719	16.510003
28.860405	1011.288600	16.515021
29.176234	1009.118802	16.520039
28.834454	1012.633907	16.525056
28.800102	1019.831242	16.530074
28.879341	1014.217489	16.535091
28.741537	1016.725711	16.540109
28.934014	1008.841125	16.545127
29.056735	1012.444852	16.550144
28.870557	1009.965058	16.555162
29.219111	1009.027217	16.560179
29.026608	1001.884215	16.565197
28.758640	1015.508307	16.570215
28.705535	1007.207530	16.575232
29.002040	1009.913214	16.580250
28.868894	1004.600770	16.585267
28.716841	1006.540019	16.590285
29.025508	1003.090104	16.595303
28.893486	1000.873272	16.600320
28.918237	1013.615515	16.605338
29.182703	1026.967373	16.610355
28.889919	1022.897898	16.615373
28.966211	1021.683716	16.620391
29.224594	1030.104089	16.625408
29.305801	1027.611063	16.630426
29.400193	1031.661010	16.635443
29.280991	1031.588089	16.640461
29.246692	1026.496930	16.645479
29.499671	1030.550587	16.650496
29.306981	1028.696642	16.655514
29.805530	1025.927202	16.660531
29.599399	1032.147759	16.665549
29.249943	1024.508486	16.670567
29.382258	1032.008075	16.675584
29.388212	1038.100940	16.680602
29.355850	1027.852982	16.685619
29.280437	1044.290446	16.690637
29.457838	1049.460388	16.695655
29.694815	1055.810776	16.700672
29.461687	1059.170120	16.705690
29.799148	1048.577396	16.710707
29.879315	1056.924544	16.715725
29.615150	1053.964588	16.720743
29.977073	1057.070341	16.725760
30.155203	1055.868703	16.730778
30.036208	1052.176100	16.735795
29.989245	1053.388947	16.740813
29.843908	1049.160812	16.745831
30.197764	1054.722997	16.750848
29.743563	1056.731385	16.755866
30.054264	1051.141542	16.760883
29.883831	1053.717964	16.765901
29.802723	1052.689230	16.770919
29.808530	1060.145412	16.775936
29.378793	1063.456475	16.780954
30.063055	1065.858801	16.785971
30.216017	1069.896482	16.790989
30.503832	1072.035492	16.796007
30.335921	1074.052955	16.801024
30.417823	1082.993128	16.806042
30.332512	1075.195944	16.811059
30.696590	1075.063558	16.816077
30.583551	1067.365367	16.821095
30.096493	1075.242270	16.826112
30.377941	1076.009517	16.831130
30.574703	1074.306367	16.836147
30.243540	1076.030516	16.841165
30.601429	1069.253067	16.846183
30.409958	1063.034517	16.851200
30.118618	1063.982461	16.856218
30.267041	1069.403070	16.861235
30.288700	1065.887377	16.866253
30.636222	1084.972981	16.871271
30.705767	1091.055963	16.876288
30.491954	1096.820153	16.881306
30.693013	1090.799251	16.886323
31.022697	1089.349955	16.891341
31.260760	1092.891560	16.896359
31.193789	1092.870467	16.901376
30.316119	1082.605766	16.906394
30.939530	1086.813198	16.911411
30.818976	1089.015791	16.916429
31.018557	1085.522885	16.921447
31.302785	1087.356346	16.926464
31.017586	1097.391928	16.931482
31.226439	1088.393929	16.936499
30.931660	1084.675040	16.941517
31.083286	1088.391045	16.946535
30.999645	1081.742295	16.951552
31.242183	1091.294926	16.956570
31.360606	1081.910228	16.961587
31.562405	1081.676877	16.966605
31.633113	1080.731801	16.971623
31.602176	1087.082888	16.976640
31.616521	1087.080691	16.981658
31.438866	1075.457324	16.986675
31.618475	1063.819366	16.991693
31.141410	1064.957170	16.996711
31.373920	1072.337035	17.001728
31.574678	1084.016836	17.006746
31.978079	1080.905602	17.011763
31.624940	1087.250050	17.016781
31.642278	1078.913027	17.021799
31.728019	1081.029852	17.026816
31.560102	1085.196389	17.031834
31.852664	1074.424450	17.036851
31.724426	1070.834266	17.041869
31.433189	1077.128049	17.046887
31.762280	1083.281070	17.051904
32.159791	1088.530361	17.056922
32.277683	1082.345688	17.061939
31.985116	1075.268728	17.066957
31.745958	1064.607983	17.071975
31.672596	1073.733269	17.076992
31.826935	1091.690795	17.082010
31.948181	1073.453754	17.087027
32.278468	1074.437456	17.092045
31.924559	1083.177244	17.097063
32.183557	1066.865866	17.102080
31.810186	1082.254709	17.107098
31.782080	1081.018908	17.112115
32.107986	1080.718898	17.117133
31.874811	1087.802051	17.122151
32.546062	1076.488319	17.127168
31.920388	1092.497113	17.132186
31.588206	1089.415198	17.137203
32.358704	1093.555550	17.142221
32.198082	1106.001677	17.147239
32.319797	1100.933542	17.152256
32.314571	1102.670063	17.157274
32.145761	1097.508309	17.162291
32.406750	1103.075501	17.167309
32.105161	1110.835181	17.172327
32.368690	1099.569137	17.177344
32.296455	1107.936882	17.182362
32.521862	1103.023014	17.187379
32.819642	1104.475675	17.192397
32.491899	1120.725282	17.197415
33.243334	1121.321527	17.202432
32.662563	1115.059431	17.207450
32.497371	1108.215087	17.212467
32.935095	1114.903465	17.217485
33.155152	1126.674962	17.222503
33.378681	1103.290689	17.227520
33.112682	1111.896884	17.232538
32.476526	1102.269903	17.237555
32.748184	1105.096233	17.242573
32.309650	1106.751897	17.247591
32.836743	1123.856167	17.252608
32.822720	1124.164497	17.257626
32.881593	1116.540503	17.262643
33.113039	1130.541356	17.267661
32.861497	1128.614514	17.272679
33.346892	1120.539107	17.277696
33.257569	1132.734314	17.282714
33.258926	1125.365422	17.287731
33.530917	1120.046669	17.292749
33.530267	1119.898486	17.297767
33.421380	1115.863473	17.302784
33.674661	1119.323820	17.307802
33.632330	1126.020673	17.312819
33.418524	1118.511716	17.317837
33.256848	1114.895172	17.322855
33.763820	1119.026067	17.327872
33.370842	1114.419912	17.332890
33.716494	1123.577813	17.337907
34.088779	1115.166574	17.342925
33.954041	1120.296774	17.347943
33.944377	1122.573624	17.352960
34.106512	1124.943644	17.357978
33.818896	1115.865141	17.362995
34.060320	1112.690759	17.368013
33.938573	1110.863629	17.373031
33.889972	1100.176350	17.378048
33.867440	1105.746661	17.383066
33.594115	1111.264505	17.388083
33.734004	1114.947630	17.393101
33.790663	1117.738009	17.398119
34.156675	1119.520872	17.403136
34.105300	1123.786037	17.408154
33.971299	1122.954880	17.413171
34.257460	1116.015014	17.418189
33.743803	1124.492519	17.423207
33.889937	1122.099823	17.428224
33.793899	1119.082121	17.433242
33.770302	1112.461880	17.438259
33.999105	1128.331356	17.443277
33.948055	1145.412053	17.448295
34.508422	1135.519866	17.453312
34.379215	1143.053908	17.458330
34.311570	1139.889772	17.463347
34.119431	1133.504045	17.468365
34.399025	1137.989080	17.473383
34.307246	1127.308507	17.478400
34.313998	1133.088860	17.483418
34.127958	1141.862499	17.488435
34.375502	1141.839774	17.493453
34.023135	1148.982534	17.498471
34.335178	1143.499749	17.503488
34.636057	1151.370771	17.508506
34.430217	1149.301112	17.513523
34.839838	1145.516719	17.518541
34.969370	1149.185685	17.523559
34.548164	1145.884094	17.528576
34.890544	1156.248027	17.533594
35.009296	1150.697506	17.538611
34.954079	1142.128754	17.543629
34.721567	1145.740480	17.548647
34.730965	1150.930298	17.553664
35.131953	1161.206214	17.558682
35.045954	1172.735062	17.563699
35.279055	1173.172173	17.568717
35.071464	1174.605695	17.573735
35.451623	1173.107510	17.578752
35.521320	1156.446830	17.583770
35.193279	1151.698012	17.588787
35.512251	1143.260347	17.593805
35.249642	1149.142603	17.598823
35.242767	1138.575035	17.603840
35.169420	1130.996868	17.608858
35.254260	1148.173173	17.613875
35.534889	1155.293120	17.618893
35.235191	1167.170814	17.623911
35.380985	1165.459812	17.628928
35.660836	1164.731474	17.633946
35.733076	1166.496965	17.638963
35.699325	1167.360628	17.643981
35.665269	1166.056321	17.648999
35.639611	1159.496343	17.654016
35.741346	1162.973981	17.659034
35.616680	1168.263571	17.664051
35.727336	1169.716971	17.669069
35.601256	1171.636415	17.674087
35.376028	1168.799763	17.679104
35.528883	1166.434417	17.684122
35.507177	1179.114584	17.689139
35.851478	1183.715786	17.694157
35.848832	1185.849541	17.699175
35.799512	1189.852472	17.704192
35.801071	1185.500448	17.709210
35.891985	1196.512622	17.714227
36.115275	1189.642476	17.719245
36.265095	1183.727349	17.724263
36.274252	1188.759426	17.729280
36.288416	1183.562847	17.734298
36.295402	1193.578237	17.739315
36.446064	1192.393490	17.744333
36.524920	1191.614395	17.749351
36.247635	1192.859956	17.754368
36.134330	1187.396047	17.759386
35.944287	1191.562898	17.764403
36.480524	1200.659609	17.769421
36.653882	1214.357150	17.774439
36.740057	1225.231224	17.779456
36.937119	1212.681586	17.784474
36.684662	1217.277880	17.789491
36.698957	1211.178718	17.794509
36.862698	1220.383928	17.799527
36.822772	1215.643882	17.804544
36.917440	1212.523890	17.809562
36.876893	1207.313732	17.814579
37.040027	1211.536052	17.819597
36.678529	1204.229934	17.824615
36.932157	1209.785683	17.829632
36.729698	1216.980869	17.834650
36.806936	1218.796079	17.839667
36.901499	1218.024005	17.844685
37.119232	1214.575584	17.849703
37.335810	1217.924901	17.854720
37.223568	1218.030775	17.859738
37.001181	1223.187275	17.864755
37.395642	1221.519602	17.869773
37.065374	1223.783265	17.874791
37.154692	1219.606916	17.879808
37.112228	1216.094866	17.884826
37.155674	1219.449048	17.889843
37.172425	1209.079730	17.894861
37.101495	1214.834334	17.899879
37.199702	1220.026124	17.904896
37.439201	1231.397035	17.909914
37.486183	1233.450485	17.914931
37.663979	1227.373199	17.919949
37.563779	1245.073866	17.924967
37.388872	1241.194270	17.929984
37.732018	1237.852550	17.935002
37.829054	1239.188156	17.940019
37.814779	1232.304489	17.945037
37.850330	1239.907593	17.950055
38.142479	1237.889776	17.955072
38.142161	1225.749554	17.960090
37.708082	1236.852959	17.965107
37.505617	1233.157534	17.970125
37.678891	1237.832716	17.975143
37.479944	1232.019211	17.980160
37.792194	1234.470015	17.985178
37.432714	1245.994153	17.990195
38.119427	1245.477020	17.995213
37.966024	1252.238551	18.000231
38.342934	1251.050132	18.005248
38.474371	1257.966131	18.010266
38.339702	1258.678254	18.015283
38.319479	1250.653109	18.020301
38.452898	1254.034315	18.025319
38.299514	1264.816325	18.030336
38.731804	1259.955409	18.035354
38.458386	1263.507256	18.040371
38.613426	1263.615697	18.045389
38.526072	1252.628248	18.050407
38.178401	1256.564038	18.055424
38.499742	1253.232022	18.060442
38.083723	1264.976413	18.065459
38.459818	1258.366471	18.070477
38.510936	1255.994862	18.075495
38.588062	1261.243594	18.080512
38.758031	1266.547300	18.085530
38.760834	1281.723112	18.090547
39.125610	1273.385551	18.095565
39.079146	1277.444862	18.100583
39.115469	1287.137001	18.105600
39.415979	1279.730936	18.110618
39.030142	1274.069592	18.115635
38.939376	1260.930418	18.120653
38.840740	1265.881470	18.125671
38.947897	1279.677730	18.130688
39.162344	1273.187625	18.135706
39.078617	1270.764425	18.140723
38.956011	1284.328220	18.145741
39.354505	1277.809457	18.150759
39.170758	1277.071245	18.155776
39.214735	1280.860856	18.160794
39.190619	1275.919518	18.165811
39.243145	1269.022280	18.170829
39.405800	1279.979154	18.175847
39.309613	1284.948765	18.180864
39.898040	1289.928551	18.185882
39.931058	1295.973110	18.190899
39.745736	1284.063623	18.195917
39.889197	1280.399536	18.200935
39.433645	1281.218424	18.205952
39.738917	1275.402140	18.210970
40.102129	1289.007063	18.215987
40.010567	1292.420148	18.221005
39.532286	1276.497925	18.226023
39.753295	1284.671774	18.231040
40.225908	1291.294826	18.236058
40.176526	1298.838596	18.241075
39.790666	1300.060043	18.246093
40.026948	1301.200405	18.251111
39.734173	1301.567917	18.256128
40.252635	1288.737811	18.261146
40.143904	1292.503863	18.266163
40.130457	1301.919738	18.271181
40.121333	1297.130694	18.276199
40.097975	1299.008912	18.281216
40.296862	1294.998522	18.286234
40.188552	1298.991728	18.291251
40.100204	1301.533314	18.296269
40.246510	1291.967440	18.301287
40.086745	1307.600930	18.306304
40.288927	1308.115441	18.311322
40.537890	1315.101527	18.316339
40.314980	1316.382811	18.321357
40.560398	1317.206172	18.326375
40.645627	1320.143613	18.331392
40.624165	1313.526121	18.336410
40.933843	1314.292139	18.341427
40.819536	1308.689493	18.346445
40.833428	1311.518120	18.351463
40.681022	1309.654717	18.356480
40.742142	1310.579355	18.361498
41.185187	1306.022865	18.366515
40.808850	1309.354060	18.371533
41.244662	1312.423109	18.376551
40.898638	1315.831636	18.381568
40.841707	1310.472520	18.386586
41.082340	1321.508798	18.391603
41.317934	1335.357688	18.396621
41.519003	1334.894074	18.401639
41.799545	1343.276432	18.406656
41.777193	1317.919911	18.411674
41.477678	1309.319688	18.416691
41.057224	1307.264490	18.421709
41.388549	1302.141572	18.426727
41.441563	1325.050779	18.431744
41.737624	1317.998840	18.436762
41.899388	1323.900287	18.441779
41.804514	1317.477260	18.446797
41.920345	1307.518492	18.451815
41.648927	1298.939145	18.456832
41.625178	1301.170873	18.461850
41.662290	1303.942235	18.466867
41.971099	1310.937936	18.471885
41.604931	1295.638867	18.476903
41.828445	1315.479327	18.481920
41.885130	1317.367175	18.486938
42.166214	1318.039815	18.491955
41.796364	1322.502936	18.496973
41.968079	1315.770159	18.501991
41.672091	1323.626889	18.507008
42.088545	1322.451244	18.512026
42.224243	1317.431363	18.517043
41.924018	1324.998420	18.522061
42.437926	1319.578827	18.527079
42.177072	1318.937824	18.532096
42.081764	1316.803600	18.537114
42.199780	1329.619910	18.542131
42.547891	1337.953875	18.547149
42.476928	1338.640303	18.552167
42.315266	1346.308872	18.557184
42.256621	1338.605250	18.562202
42.390977	1351.658874	18.567219
42.548747	1344.603209	18.572237
42.663987	1337.323796	18.577255
42.642635	1340.318860	18.582272
42.521811	1336.632794	18.587290
42.548967	1340.081054	18.592307
42.599464	1350.711451	18.597325
42.994057	1342.176712	18.602343
42.910885	1349.113537	18.607360
42.756919	1354.000645	18.612378
43.037507	1354.171591	18.617395
42.785110	1372.953277	18.622413
43.464638	1352.003395	18.627431
42.882472	1367.491263	18.632448
42.950432	1357.943864	18.637466
43.280306	1346.752541	18.642483
43.117797	1353.335647	18.647501
43.635400	1346.943481	18.652519
43.543843	1355.901331	18.657536
43.761436	1347.832804	18.662554
43.504086	1353.004252	18.667571
43.534821	1355.707187	18.672589
43.557962	1343.244495	18.677607
43.574496	1354.899508	18.682624
43.350952	1353.593132	18.687642
43.681275	1358.177621	18.692659
43.550515	1365.598389	18.697677
43.344969	1353.518435	18.702695
43.259609	1357.990919	18.707712
43.413551	1361.372105	18.712730
43.558129	1366.594588	18.717747
43.914551	1378.831016	18.722765
44.093493	1376.673019	18.727783
43.939156	1379.306942	18.732800
44.225565	1372.329069	18.737818
44.432423	1382.310290	18.742835
44.417351	1376.805781	18.747853
44.564475	1373.731242	18.752871
44.308118	1378.413392	18.757888
44.253947	1381.852231	18.762906
44.125445	1374.497142	18.767923
44.456737	1377.146973	18.772941
44.624231	1374.801411	18.777959
44.444171	1374.801080	18.782976
44.466594	1377.028785	18.787994
44.751164	1367.958896	18.793011
44.508537	1371.471256	18.798029
44.550410	1367.501076	18.803047
44.607256	1369.067012	18.808064
44.524114	1366.965601	18.813082
44.646528	1370.774576	18.818099
44.422703	1371.096641	18.823117
44.447219	1366.144550	18.828135
44.614978	1364.123996	18.833152
44.347620	1362.590910	18.838170
44.596210	1382.304464	18.843187
44.702180	1398.054450	18.848205
44.702065	1384.866357	18.853223
44.831779	1394.168472	18.858240
44.482367	1393.014234	18.863258
45.148469	1394.437977	18.868275
45.316356	1419.522711	18.873293
45.634212	1411.214483	18.878311
45.714211	1407.086878	18.883328
45.206360	1398.762046	18.888346
45.329998	1403.331390	18.893363
45.432055	1414.297782	18.898381
45.634304	1410.201636	18.903399
45.655043	1414.727043	18.908416
45.883749	1415.644529	18.913434
45.773954	1399.942534	18.918451
45.426428	1395.225086	18.923469
45.436521	1399.455501	18.928487
45.850985	1405.910924	18.933504
45.866172	1409.998536	18.938522
45.808109	1407.754359	18.943539
45.755072	1414.695986	18.948557
45.796729	1409.662319	18.953575
45.737651	1413.723624	18.958592
46.015078	1412.531750	18.963610
46.103122	1406.209599	18.968627
45.796268	1412.913031	18.973645
45.680380	1410.895609	18.978663
46.160142	1407.737715	18.983680
45.945109	1411.419357	18.988698
45.992012	1411.926490	18.993715
45.970430	1424.572099	18.998733
46.168066	1434.191866	19.003751
46.247648	1439.664331	19.008768
46.579737	1437.520353	19.013786
46.826437	1433.231088	19.018803
46.309450	1439.323459	19.023821
46.156873	1428.601678	19.028839
46.504198	1435.531471	19.033856
46.515015	1436.602804	19.038874
46.369707	1434.855048	19.043891
46.446933	1446.749982	19.048909
46.841047	1453.296954	19.053927
46.939335	1448.503770	19.058944
46.898034	1452.492888	19.063962
47.407865	1451.406839	19.068979
47.430054	1444.268102	19.073997
47.397148	1447.072478	19.079015
47.301161	1448.214089	19.084032
47.241367	1440.453798	19.089050
46.999190	1429.805927	19.094067
47.515332	1444.741007	19.099085
47.038092	1438.453208	19.104103
47.448680	1436.208645	19.109120
47.547827	1441.883194	19.114138
47.324885	1436.370005	19.119155
47.922707	1449.329450	19.124173
47.408912	1437.704533	19.129191
47.524568	1439.002541	19.134208
47.477690	1441.960571	19.139226
47.737148	1434.601859	19.144243
47.830641	1441.325021	19.149261
47.927940	1444.282695	19.154279
47.806752	1437.683839	19.159296
47.456944	1446.287465	19.164314
47.634202	1441.090665	19.169331
47.693489	1435.852273	19.174349
47.912239	1437.875848	19.179367
47.833760	1432.002495	19.184384
47.837910	1448.118674	19.189402
48.212839	1454.779088	19.194419
48.383358	1465.412958	19.199437
48.269204	1460.349887	19.204455
48.526242	1456.551315	19.209472
48.308952	1466.879490	19.214490
48.357118	1468.279527	19.219507
48.572275	1464.452761	19.224525
48.721545	1460.939213	19.229543
48.748994	1460.382706	19.234560
48.504663	1460.452343	19.239578
48.509906	1461.130066	19.244595
48.795356	1461.426489	19.249613
48.679901	1457.256720	19.254631
48.775844	1459.933739	19.259648
48.648239	1464.030972	19.264666
48.734500	1454.651086	19.269683
48.523463	1452.471747	19.274701
48.946751	1454.545530	19.279719
48.788559	1454.409249	19.284736
48.720734	1462.710202	19.289754
48.575930	1453.965899	19.294771
48.776095	1457.892177	19.299789
48.582474	1478.166996	19.304807
48.824873	1480.347841	19.309824
48.867654	1493.160204	19.314842
48.880718	1488.456017	19.319859
48.826979	1496.372937	19.324877
48.784364	1507.049483	19.329895
49.323956	1505.662149	19.334912
49.185275	1498.138179	19.339930
49.403584	1498.053733	19.344947
49.790196	1501.875252	19.349965
49.557994	1504.189953	19.354983
49.532338	1508.523790	19.360000
49.758759	1504.827806	19.365018
49.709251	1506.634377	19.370035
50.115930	1510.080385	19.375053
50.232225	1517.371232	19.380071
50.537850	1500.196967	19.385088
50.130215	1501.320831	19.390106
50.329770	1500.270464	19.395123
50.268801	1494.217638	19.400141
50.221672	1504.730783	19.405159
50.357588	1496.507646	19.410176
50.362282	1497.213859	19.415194
50.312534	1496.079230	19.420211
50.315178	1499.389325	19.425229
50.572740	1502.669198	19.430247
50.326063	1498.235825	19.435264
50.548203	1497.974056	19.440282
50.494180	1496.410899	19.445299
50.346565	1495.424052	19.450317
50.515133	1506.329652	19.455335
50.679646	1511.451243	19.460352
51.068839	1521.019142	19.465370
51.034963	1513.362081	19.470387
51.053893	1510.392686	19.475405
50.619207	1508.115615	19.480423
51.048938	1511.848371	19.485440
51.149784	1509.210208	19.490458
51.003337	1514.651616	19.495475
50.980622	1516.308848	19.500493
50.829468	1514.918604	19.505511
50.971414	1522.208615	19.510528
51.055863	1516.669633	19.515546
51.093080	1516.884784	19.520563
51.367093	1516.548666	19.525581
50.945961	1515.165742	19.530599
51.251150	1519.384954	19.535616
51.648288	1543.844029	19.540634
51.700847	1545.653648	19.545651
52.032110	1542.402086	19.550669
51.903134	1539.190622	19.555687
51.939746	1526.507952	19.560704
51.705263	1517.989021	19.565722
51.294134	1514.979284	19.570739
51.653441	1525.965654	19.575757
51.749707	1530.138500	19.580775
51.554478	1527.972470	19.585792
51.598371	1532.790950	19.590810
51.700796	1534.050000	19.595827
52.053099	1535.746676	19.600845
51.940390	1546.812860	19.605863
52.234404	1553.719442	19.610880
52.157783	1563.577642	19.615898
51.848909	1560.195366	19.620915
52.571435	1558.482896	19.625933
52.009715	1555.468196	19.630951
52.691630	1551.183726	19.635968
52.522462	1567.008257	19.640986
52.291720	1563.402374	19.646003
52.510053	1560.285158	19.651021
52.229456	1563.620428	19.656039
52.455908	1560.722856	19.661056
52.799096	1571.673894	19.666074
53.053194	1581.035638	19.671091
52.827804	1574.206799	19.676109
52.937586	1578.068279	19.681127
53.274579	1579.391798	19.686144
53.091096	1578.101258	19.691162
52.802415	1582.851610	19.696179
52.799341	1583.063567	19.701197
52.888884	1577.810956	19.706215
53.087420	1567.047048	19.711232
53.027392	1578.348050	19.716250
52.855206	1586.741049	19.721267
53.212207	1583.532810	19.726285
53.095592	1599.204018	19.731303
53.207144	1604.655778	19.736320
53.374710	1599.829675	19.741338
53.459189	1604.064336	19.746355
53.974567	1595.551697	19.751373
53.620521	1585.034761	19.756391
54.247190	1587.367232	19.761408
54.257602	1587.965259	19.766426
54.138831	1588.709634	19.771443
54.274688	1576.547970	19.776461
54.132856	1582.799733	19.781479
54.291481	1575.977377	19.786496
54.280633	1584.468334	19.791514
54.178228	1583.048404	19.796531
54.551811	1582.592639	19.801549
54.282670	1586.951781	19.806567
54.216235	1584.986600	19.811584
54.256205	1584.399738	19.816602
54.011840	1589.439842	19.821619
54.478204	1580.628724	19.826637
54.118871	1578.545042	19.831655
54.624178	1584.194270	19.836672
54.689806	1585.730455	19.841690
54.693780	1583.602831	19.846707
54.795749	1574.233060	19.851725
54.564396	1581.464449	19.856743
54.491227	1577.149211	19.861760
54.771806	1598.322337	19.866778
54.836191	1600.635056	19.871795
55.094751	1604.069430	19.876813
54.925268	1605.342416	19.881831
55.024214	1603.944784	19.886848
54.821916	1605.863518	19.891866
54.870665	1606.102121	19.896883
55.458644	1607.585384	19.901901
54.851877	1610.214041	19.906919
55.196918	1606.565841	19.911936
55.220993	1615.537376	19.916954
55.085505	1627.695926	19.921971
55.361945	1617.390082	19.926989
55.162762	1643.005660	19.932007
55.553775	1629.283111	19.937024
55.672727	1629.558122	19.942042
55.595087	1629.267285	19.947059
55.800642	1625.849085	19.952077
55.407631	1635.109634	19.957095
55.663912	1646.096339	19.962112
56.065117	1646.409457	19.967130
55.842992	1651.427181	19.972147
56.194413	1646.992170	19.977165
56.242165	1648.370195	19.982183
55.961870	1650.449402	19.987200
56.007187	1651.139828	19.992218
56.324431	1660.763187	19.997235
56.295445	1641.188779	20.002253
56.121135	1643.775357	20.007271
56.260306	1649.143934	20.012288
56.573694	1651.304280	20.017306
56.230455	1648.874096	20.022323
56.565758	1665.775215	20.027341
56.590399	1674.898174	20.032359
56.500765	1685.556901	20.037376
56.510004	1673.111922	20.042394
56.938160	1677.027999	20.047411
56.959066	1673.528083	20.052429
56.752292	1676.911842	20.057447
56.888841	1672.775371	20.062464
57.134594	1671.903998	20.067482
56.885739	1678.648993	20.072499
56.894137	1682.422137	20.077517
57.415277	1686.131231	20.082535
57.084985	1697.136709	20.087552
57.913621	1683.967688	20.092570
58.343200	1666.660354	20.097587
58.496369	1645.959340	20.102605
58.482401	1647.009297	20.107623
58.544078	1639.564527	20.112640
58.323440	1625.356533	20.117658
58.096935	1615.614997	20.122675
58.155452	1604.014475	20.127693
58.372200	1605.148431	20.132711
58.266880	1601.431493	20.137728
58.551959	1609.125294	20.142746
58.419659	1601.224740	20.147763
58.220393	1595.789868	20.152781
58.026537	1585.733991	20.157799
58.053741	1580.967617	20.162816
58.477322	1583.994437	20.167834
58.129450	1582.060451	20.172851
58.273330	1603.235932	20.177869
58.433667	1606.035493	20.182887
58.422342	1611.632620	20.187904
58.401261	1606.813796	20.192922
58.363720	1608.836268	20.197939
58.291874	1607.645111	20.202957
58.120268	1607.813880	20.207975
58.144476	1606.046026	20.212992
58.762861	1619.204369	20.218010
58.454916	1637.029290	20.223027
58.567326	1631.151398	20.228045
58.624293	1633.768239	20.233063
58.433129	1633.719143	20.238080
58.813693	1640.908934	20.243098
58.750340	1662.918339	20.248115
59.176490	1665.512419	20.253133
59.150406	1663.645090	20.258151
58.859676	1666.918840	20.263168
59.232849	1662.600361	20.268186
59.257563	1664.310184	20.273203
59.408389	1665.183003	20.278221
59.540169	1678.284606	20.283239
59.296849	1681.219610	20.288256
59.907054	1689.156322	20.293274
59.646136	1690.948489	20.298291
59.639504	1679.676804	20.303309
59.673039	1689.824041	20.308327
59.713154	1695.362692	20.313344
60.067048	1687.705145	20.318362
59.716513	1681.258674	20.323379
59.929652	1688.117938	20.328397
59.891072	1680.887581	20.333415
59.363532	1689.632606	20.338432
60.084968	1695.500689	20.343450
60.188517	1711.835165	20.348467
60.559059	1707.652787	20.353485
60.454534	1717.947771	20.358503
60.029215	1712.071521	20.363520
60.428491	1713.694629	20.368538
60.227160	1716.020331	20.373555
60.824898	1716.189240	20.378573
60.585620	1718.735450	20.383591
60.320899	1721.503377	20.388608
60.636498	1723.530841	20.393626
60.719632	1730.034814	20.398643
60.588610	1731.544823	20.403661
60.870447	1738.248241	20.408679
60.683312	1736.977193	20.413696
60.771975	1735.843090	20.418714
60.996866	1746.137295	20.423731
61.271548	1752.188566	20.428749
61.435004	1751.320534	20.433767
61.228747	1753.448187	20.438784
61.347215	1753.843200	20.443802
61.472596	1751.311636	20.448819
61.244215	1746.812235	20.453837
61.676253	1748.329257	20.458855
61.437305	1752.349214	20.463872
61.688048	1746.639100	20.468890
62.052863	1764.390961	20.473907
62.023798	1764.638527	20.478925
61.977431	1757.803835	20.483943
61.895863	1763.440349	20.488960
62.334206	1769.453521	20.493978
62.372567	1769.734771	20.498995
62.473193	1758.357972	20.504013
62.548143	1751.946217	20.509031
62.196783	1746.497108	20.514048
62.666329	1747.181450	20.519066
62.502922	1740.349209	20.524083
62.173096	1749.978684	20.529101
62.516085	1752.598349	20.534119
62.275025	1764.473621	20.539136
62.952386	1755.904127	20.544154
62.911684	1758.261631	20.549171
62.805852	1755.990134	20.554189
62.842086	1750.906721	20.559207
62.810197	1768.344801	20.564224
62.848088	1758.025523	20.569242
62.873780	1755.427427	20.574259
62.932387	1763.102906	20.579277
62.680224	1749.300518	20.584295
62.710016	1776.341809	20.589312
63.231379	1776.431091	20.594330
63.243580	1777.729452	20.599347
63.097672	1773.308723	20.604365
63.416790	1777.497425	20.609383
63.190761	1782.825070	20.614400
63.381395	1777.840690	20.619418
63.778252	1787.735751	20.624435
63.633439	1798.226407	20.629453
63.924292	1797.168120	20.634471
63.943860	1810.880597	20.639488
64.103494	1804.193701	20.644506
63.751536	1797.157258	20.649523
63.886174	1805.616201	20.654541
64.119760	1799.810908	20.659559
64.075395	1800.941348	20.664576
64.258672	1786.730300	20.669594
64.180328	1794.253541	20.674611
64.070245	1794.712542	20.679629
64.228938	1794.823574	20.684647
64.340800	1800.095460	20.689664
64.380806	1790.675261	20.694682
64.140444	1803.503527	20.699699
64.234579	1818.791812	20.704717
64.715217	1823.166822	20.709735
64.450399	1824.621929	20.714752
64.721495	1816.693188	20.719770
64.642448	1820.492600	20.724787
64.867250	1814.726541	20.729805
65.257682	1826.361520	20.734823
65.227362	1834.035095	20.739840
65.415301	1831.023553	20.744858
65.690144	1838.261443	20.749875
65.501880	1824.916120	20.754893
65.240306	1817.957117	20.759911
65.431748	1824.400079	20.764928
65.300097	1829.514222	20.769946
65.257369	1837.205510	20.774963
65.281054	1841.187753	20.779981
65.641795	1840.380522	20.784999
65.273284	1844.853030	20.790016
65.480529	1834.226466	20.795034
65.715611	1847.662413	20.800051
66.164341	1865.199333	20.805069
65.882381	1864.378553	20.810087
65.869594	1871.617057	20.815104
66.060761	1855.094608	20.820122
66.190062	1858.198851	20.825139
66.180643	1866.610822	20.830157
65.992417	1860.028559	20.835175
65.923237	1867.181164	20.840192
66.446463	1871.899860	20.845210
66.420009	1879.534982	20.850227
66.431102	1888.395063	20.855245
66.766832	1883.956126	20.860263
66.478611	1887.317890	20.865280
66.590936	1885.255414	20.870298
66.695602	1877.986894	20.875315
66.452265	1890.345457	20.880333
66.986356	1895.141365	20.885351
67.065681	1905.635058	20.890368
67.255606	1905.495068	20.895386
67.719940	1901.664128	20.900403
67.329810	1900.412050	20.905421
67.939148	1893.885484	20.910439
67.818623	1887.646131	20.915456
67.366586	1878.523407	20.920474
67.783869	1883.713051	20.925491
67.789978	1884.368564	20.930509
68.015062	1884.030590	20.935527
67.847603	1884.653165	20.940544
68.147597	1877.938076	20.945562
68.293004	1872.348466	20.950579
67.991488	1859.970676	20.955597
68.089195	1860.848619	20.960615
68.023026	1863.045995	20.965632
68.045484	1872.904719	20.970650
68.246789	1864.115795	20.975667
67.592271	1868.746451	20.980685
68.127916	1863.812475	20.985703
67.994176	1884.002690	20.990720
68.158836	1879.669286	20.995738
68.143436	1882.726633	21.000755
68.148988	1885.566117	21.005773
68.560540	1901.792850	21.010791
68.635036	1908.048916	21.015808
68.736861	1912.451369	21.020826
68.988216	1917.720507	21.025843
68.593198	1913.840318	21.030861
68.890094	1916.104254	21.035879
68.916463	1910.659402	21.040896
68.839772	1923.424401	21.045914
69.094292	1918.944448	21.050931
68.850446	1935.093367	21.055949
69.175681	1936.260948	21.060967
69.438387	1933.367140	21.065984
69.377488	1935.071383	21.071002
69.564397	1932.416602	21.076019
69.319286	1945.965257	21.081037
69.087332	1943.886947	21.086055
69.438808	1949.011114	21.091072
69.383494	1959.213365	21.096090
70.131058	1969.123354	21.101107
69.652598	1958.963250	21.106125
69.625721	1963.382597	21.111143
69.956501	1958.379503	21.116160
69.742344	1973.296183	21.121178
70.109349	1981.141498	21.126195
69.823083	1985.929451	21.131213
70.117584	1990.847898	21.136231
70.318441	1995.572635	21.141248
70.320319	1995.285191	21.146266
70.424741	2002.619112	21.151283
70.610900	2012.155769	21.156301
70.755071	2007.759249	21.161319
71.070950	2009.474267	21.166336
70.651301	2014.658550	21.171354
71.361789	2012.149465	21.176371
71.009171	2015.385575	21.181389
70.841931	2003.592716	21.186407
71.325626	2003.384896	21.191424
71.239863	2007.141210	21.196442
71.600075	2003.351708	21.201459
71.052180	2006.138518	21.206477
71.389926	2009.229270	21.211495
71.331609	2009.828545	21.216512
71.499932	2005.014839	21.221530
71.406699	2014.948460	21.226547
72.027993	2024.086003	21.231565
72.130226	2022.331208	21.236583
72.262926	2020.997719	21.241600
71.700808	2032.771671	21.246618
72.177403	2018.764090	21.251635
72.255340	2018.354346	21.256653
72.159736	2018.277746	21.261671
72.341105	2020.723791	21.266688
72.025398	2034.147799	21.271706
72.364456	2025.211112	21.276723
72.604600	2024.908662	21.281741
72.130706	2023.773762	21.286759
72.502880	2018.511732	21.291776
72.279530	2026.155481	21.296794
72.807503	2022.270425	21.301811
72.563168	2021.857205	21.306829
73.224565	2034.598890	21.311847
73.520551	2024.801029	21.316864
72.985328	2024.038608	21.321882
72.952907	2012.609776	21.326899
72.874173	2017.270748	21.331917
73.231862	2024.521063	21.336935
73.292955	2029.153957	21.341952
73.288269	2039.856475	21.346970
73.679192	2027.244523	21.351987
73.518784	2029.787964	21.357005
73.131352	2032.735996	21.362023
73.642875	2024.343680	21.367040
73.596551	2026.395970	21.372058
73.810803	2024.434378	21.377075
73.990942	2031.908007	21.382093
73.789809	2031.030452	21.387111
73.883389	2024.991254	21.392128
73.645442	2031.040379	21.397146
73.858314	2042.314965	21.402163
74.057558	2052.625965	21.407181
73.898662	2049.365417	21.412199
74.184251	2051.811019	21.417216
73.775175	2050.372524	21.422234
74.269375	2064.869711	21.427251
74.369587	2078.490940	21.432269
74.667104	2080.811607	21.437287
74.747695	2076.166183	21.442304
74.637818	2079.194090	21.447322
74.577163	2073.563914	21.452339
74.963579	2086.859710	21.457357
74.917493	2098.909983	21.462375
75.245300	2094.314431	21.467392
75.694504	2107.098672	21.472410
75.518444	2100.110465	21.477427
75.544019	2100.958624	21.482445
75.302076	2097.679438	21.487463
75.755616	2099.868514	21.492480
75.412042	2099.322415	21.497498
75.641982	2106.393829	21.502515
75.638969	2097.504052	21.507533
75.823667	2099.069082	21.512551
75.694987	2099.938102	21.517568
75.492974	2095.043170	21.522586
75.977347	2103.122740	21.527603
75.948036	2109.843183	21.532621
75.935441	2124.605525	21.537639
76.395330	2119.872631	21.542656
76.315649	2114.668301	21.547674
76.812317	2112.485997	21.552691
76.560682	2113.623479	21.557709
76.461794	2114.980188	21.562727
76.888194	2108.601954	21.567744
76.811344	2115.692733	21.572762
76.495763	2111.320430	21.577779
76.716326	2107.218118	21.582797
76.548439	2106.543675	21.587815
77.007319	2106.396525	21.592832
77.006206	2128.766057	21.597850
77.315831	2120.562929	21.602867
77.196099	2132.605755	21.607885
77.456339	2139.154889	21.612903
77.756922	2124.666522	21.617920
77.505642	2137.490416	21.622938
77.137973	2127.193040	21.627955
77.528713	2140.614441	21.632973
77.170826	2128.497716	21.637991
77.375538	2132.155180	21.643008
77.434819	2139.559304	21.648026
77.592205	2145.086148	21.653043
77.989199	2153.700078	21.658061
77.528776	2155.741112	21.663079
77.941502	2159.186307	21.668096
77.676038	2158.047349	21.673114
78.241867	2160.787022	21.678131
78.531593	2168.442471	21.683149
78.648401	2166.404513	21.688167
79.265461	2168.665973	21.693184
79.000298	2151.744062	21.698202
78.562486	2147.895731	21.703219
78.854764	2139.969862	21.708237
78.422068	2145.345570	21.713255
78.843807	2151.718079	21.718272
79.120295	2164.257841	21.723290
78.990817	2165.007062	21.728307
78.956566	2169.421296	21.733325
79.008581	2167.200912	21.738343
79.311496	2164.086203	21.743360
79.114485	2168.421631	21.748378
79.359733	2163.485448	21.753395
79.028795	2172.073859	21.758413
79.318222	2178.618464	21.763431
79.677327	2182.419166	21.768448
79.498326	2191.353177	21.773466
79.510941	2182.205293	21.778483
79.802160	2184.097745	21.783501
79.875366	2197.432921	21.788519
80.404582	2209.917587	21.793536
80.179738	2215.399817	21.798554
80.446256	2216.882687	21.803571
80.548202	2212.290710	21.808589
80.433160	2222.006925	21.813607
80.670246	2205.177187	21.818624
80.516420	2210.578928	21.823642
80.404589	2212.161732	21.828659
80.686031	2207.743791	21.833677
80.395025	2217.490555	21.838695
80.975240	2206.865664	21.843712
80.742716	2215.094774	21.848730
80.848774	2230.283720	21.853747
81.334693	2229.741020	21.858765
81.297406	2225.473689	21.863783
80.991435	2221.749990	21.868800
80.910157	2225.934863	21.873818
81.065928	2235.126058	21.878835
81.448580	2231.389822	21.883853
81.497227	2249.162988	21.888871
81.721497	2251.340440	21.893888
81.905329	2258.071937	21.898906
81.714091	2256.842517	21.903923
82.175354	2254.305929	21.908941
81.633496	2255.646404	21.913959
82.128182	2255.531550	21.918976
81.955531	2258.174765	21.923994
81.779045	2256.302387	21.929011
82.353470	2267.530292	21.934029
82.029029	2276.796275	21.939047
82.345259	2270.791761	21.944064
82.321650	2273.377057	21.949082
82.547426	2278.744964	21.954099
82.618857	2270.405274	21.959117
82.686587	2294.266536	21.964135
83.148553	2296.315463	21.969152
83.220552	2298.172627	21.974170
83.157494	2299.053531	21.979187
83.482093	2292.990899	21.984205
83.110736	2300.948158	21.989223
83.405518	2296.796376	21.994240
83.620545	2296.299007	21.999258
83.414220	2286.755943	22.004275
83.776010	2281.568042	22.009293
83.717155	2290.290882	22.014311
83.793237	2282.483821	22.019328
83.634269	2287.261503	22.024346
83.763866	2283.384764	22.029363
83.605239	2284.914897	22.034381
83.499849	2284.088698	22.039399
83.945376	2297.425944	22.044416
84.315448	2305.605459	22.049434
84.512975	2314.455660	22.054451
84.494461	2318.820141	22.059469
84.332828	2319.520723	22.064487
84.501192	2314.646965	22.069504
84.432909	2319.135965	22.074522
84.565920	2313.563929	22.079539
84.560599	2312.280311	22.084557
84.467766	2339.786539	22.089575
84.590687	2342.636226	22.094592
84.683757	2346.178565	22.099610
85.013733	2344.331473	22.104627
84.965882	2342.164488	22.109645
85.063903	2355.903040	22.114663
85.370087	2349.903220	22.119680
85.509935	2354.602836	22.124698
85.741756	2356.438279	22.129715
86.234549	2352.435547	22.134733
86.081295	2359.677182	22.139751
85.952742	2351.939823	22.144768
85.930923	2351.583475	22.149786
86.012748	2348.541028	22.154803
86.175341	2347.944517	22.159821
85.540501	2353.074033	22.164839
86.244767	2348.154701	22.169856
85.832206	2353.634639	22.174874
85.867219	2370.456942	22.179891
86.063132	2365.648312	22.184909
86.111632	2370.463146	22.189927
86.425253	2385.509448	22.194944
86.481018	2389.691958	22.199962
86.469591	2401.689699	22.204979
86.616212	2390.065482	22.209997
86.686278	2404.982453	22.215015
87.136254	2406.872304	22.220032
87.408284	2415.310145	22.225050
87.644912	2421.007785	22.230067
87.742436	2414.791106	22.235085
87.789306	2410.466445	22.240103
87.871645	2411.741308	22.245120
87.936673	2411.936361	22.250138
87.190236	2411.058474	22.255155
87.724228	2411.679159	22.260173
87.626830	2414.105541	22.265191
87.614841	2411.835128	22.270208
87.787717	2407.992652	22.275226
87.746171	2428.061822	22.280243
88.172135	2441.206550	22.285261
88.008706	2439.291092	22.290279
88.254498	2436.283066	22.295296
88.406373	2421.423112	22.300314
88.407609	2434.605558	22.305331
88.698956	2444.394329	22.310349
88.681257	2455.679826	22.315367
88.585397	2458.664586	22.320384
88.793717	2452.351745	22.325402
88.710543	2458.399008	22.330419
89.178121	2447.327580	22.335437
89.165696	2448.494116	22.340455
89.137454	2454.996757	22.345472
89.476827	2448.054404	22.350490
89.254711	2465.592214	22.355507
89.839942	2472.785193	22.360525
90.219399	2474.190538	22.365543
89.981162	2469.449475	22.370560
89.834712	2447.683269	22.375578
90.000115	2452.590384	22.380595
89.754115	2463.804128	22.385613
90.041934	2472.955951	22.390631
89.830022	2474.358687	22.395648
89.977028	2474.796613	22.400666
89.961049	2471.526361	22.405683
89.838133	2471.536067	22.410701
90.499304	2487.844398	22.415719
90.585264	2489.150263	22.420736
91.087815	2487.247884	22.425754
90.721312	2492.525021	22.430771
91.068438	2485.262690	22.435789
91.061851	2476.676258	22.440807
90.697079	2485.973876	22.445824
90.928624	2481.106015	22.450842
91.089484	2488.260925	22.455859
91.210656	2498.035192	22.460877
91.375486	2506.442426	22.465895
91.411523	2505.827742	22.470912
91.586460	2502.145882	22.475930
91.434565	2507.730460	22.480947
91.686936	2503.758814	22.485965
91.757097	2510.366084	22.490983
91.789836	2524.897621	22.496000
92.250373	2530.917064	22.501018
92.290012	2537.421791	22.506035
92.209010	2538.908299	22.511053
92.632663	2531.466767	22.516071
92.437270	2537.455783	22.521088
92.475049	2535.707817	22.526106
92.481538	2539.667645	22.531123
92.670706	2536.176080	22.536141
92.597126	2536.929236	22.541159
92.470702	2557.848111	22.546176
92.901030	2557.156257	22.551194
92.939462	2555.812158	22.556211
93.203307	2555.622783	22.561229
93.103778	2560.807878	22.566247
92.848072	2561.706164	22.571264
93.469190	2574.116813	22.576282
93.210981	2584.938030	22.581299
93.605086	2587.420464	22.586317
93.778136	2584.524731	22.591335
93.431878	2586.500697	22.596352
94.052734	2590.459565	22.601370
94.235149	2605.179317	22.606387
93.975716	2607.327973	22.611405
94.718813	2608.408450	22.616423
94.401366	2609.417344	22.621440
94.779944	2608.537872	22.626458
94.556357	2602.279598	22.631475
94.150877	2603.608333	22.636493
94.458214	2601.105130	22.641511
94.303410	2611.648313	22.646528
94.580326	2600.073107	22.651546
94.752913	2618.843585	22.656563
94.926150	2615.360796	22.661581
94.814460	2619.638864	22.666599
95.165789	2632.849006	22.671616
95.336230	2627.046966	22.676634
95.095634	2635.350113	22.681651
94.958270	2623.839392	22.686669
95.602058	2632.402506	22.691687
95.363712	2636.630864	22.696704
95.616114	2639.021751	22.701722
95.471010	2652.826788	22.706739
95.799683	2646.141664	22.711757
96.074650	2649.586311	22.716775
95.663002	2664.313390	22.721792
96.139684	2664.147686	22.726810
96.263743	2679.700311	22.731827
96.359366	2671.735393	22.736845
96.883183	2661.112703	22.741863
96.924377	2674.986589	22.746880
96.980432	2660.848309	22.751898
97.156131	2662.067627	22.756915
96.705851	2657.627790	22.761933
97.188568	2668.914412	22.766951
97.035960	2662.020171	22.771968
97.473045	2656.599516	22.776986
97.488528	2664.379933	22.782003
97.138031	2659.640517	22.787021
97.132824	2677.586607	22.792039
97.199079	2680.678718	22.797056
97.550830	2680.011718	22.802074
97.647777	2680.302797	22.807091
97.993451	2686.447482	22.812109
97.832639	2693.819826	22.817127
97.747936	2703.986048	22.822144
98.046788	2699.221267	22.827162
98.201589	2709.097719	22.832179
98.088065	2701.859681	22.837197
98.405864	2697.259222	22.842215
98.308080	2716.696794	22.847232
98.614445	2724.703369	22.852250
98.586221	2727.532465	22.857267
98.615844	2732.476577	22.862285
99.216948	2724.230948	22.867303
98.601345	2728.003629	22.872320
98.620121	2738.179007	22.877338
99.182618	2745.782768	22.882355
98.783590	2744.879178	22.887373
99.322361	2737.075628	22.892391
99.381090	2745.600488	22.897408
99.601084	2762.359641	22.902426
99.984397	2764.215725	22.907443
99.769071	2759.382648	22.912461
100.222535	2759.918047	22.917479
100.211228	2755.211010	22.922496
100.163984	2752.248555	22.927514
100.119215	2761.228227	22.932531
100.368741	2761.473460	22.937549
100.479883	2760.105401	22.942567
100.540301	2778.508471	22.947584
100.995439	2783.181204	22.952602
100.776672	2777.957306	22.957619
100.954548	2779.532927	22.962637
100.911312	2774.114430	22.967655
101.045106	2784.316113	22.972672
101.114667	2779.943645	22.977690
101.112241	2775.863275	22.982707
101.006576	2783.264942	22.987725
101.566134	2790.345274	22.992743
101.493254	2803.804640	22.997760
101.809379	2796.790027	23.002778
101.498440	2803.576670	23.007795
101.655032	2809.021785	23.012813
102.104540	2808.282752	23.017831
101.647912	2807.962530	23.022848
101.570069	2803.549885	23.027866
101.662190	2820.341626	23.032883
102.060631	2825.947925	23.037901
102.629091	2821.431495	23.042919
102.336380	2831.314567	23.047936
102.755145	2819.796037	23.052954
102.857254	2810.409818	23.057971
102.849153	2834.785421	23.062989
103.087391	2839.652898	23.068007
103.031314	2850.079855	23.073024
103.346575	2845.867950	23.078042
103.727893	2841.895091	23.083059
103.663583	2848.261468	23.088077
103.814694	2824.046707	23.093095
103.587190	2846.127307	23.098112
103.633857	2841.146111	23.103130
103.866160	2830.303599	23.108147
103.690724	2841.897944	23.113165
103.882929	2829.575167	23.118183
103.975243	2828.020670	23.123200
104.009744	2842.668965	23.128218
104.162965	2853.148552	23.133235
104.094431	2856.201713	23.138253
104.245582	2856.496980	23.143271
104.257228	2853.351756	23.148288
104.594008	2863.622874	23.153306
104.661497	2873.446733	23.158323
104.562913	2873.951311	23.163341
104.754219	2876.257059	23.168359
104.910454	2889.690286	23.173376
104.685856	2887.355076	23.178394
105.394430	2899.190554	23.183411
105.145933	2908.303013	23.188429
105.258350	2902.251120	23.193447
105.552401	2909.035136	23.198464
105.751966	2923.903972	23.203482
105.796835	2932.355332	23.208499
105.643022	2940.686137	23.213517
106.082176	2937.152417	23.218535
106.041218	2935.514510	23.223552
106.090907	2928.553953	23.228570
106.341636	2949.073706	23.233587
106.282788	2955.631792	23.238605
106.319895	2953.950167	23.243623
106.435029	2962.778801	23.248640
106.957887	2941.087688	23.253658
107.305962	2925.783323	23.258675
107.255983	2933.419400	23.263693
107.663518	2925.992839	23.268711
107.718196	2927.871702	23.273728
107.606093	2935.097693	23.278746
107.634341	2937.665543	23.283763
107.641085	2931.708995	23.288781
107.835810	2932.953773	23.293799
108.087664	2939.895863	23.298816
107.991827	2946.235622	23.303834
107.983330	2939.757533	23.308851
108.415519	2958.077656	23.313869
108.433710	2955.953968	23.318887
108.629733	2955.033469	23.323904
108.869624	2956.182846	23.328922
109.099716	2943.573200	23.333939
108.901216	2943.982873	23.338957
108.906017	2949.183396	23.343975
109.380650	2945.483191	23.348992
109.080237	2944.236003	23.354010
109.009804	2935.902311	23.359027
108.890620	2937.618879	23.364045
109.075399	2949.564345	23.369063
108.889260	2941.075080	23.374080
108.691436	2942.485127	23.379098
109.034071	2947.263790	23.384115
109.112582	2976.312893	23.389133
109.539768	2963.590488	23.394151
109.405386	2975.389986	23.399168
109.636211	2985.904909	23.404186
109.710048	2987.954381	23.409203
109.972044	2985.095234	23.414221
110.135531	2997.075608	23.419239
110.141251	3012.198781	23.424256
110.541826	3011.647256	23.429274
110.579539	3008.327516	23.434291
110.323752	3006.988162	23.439309
110.507306	3022.670690	23.444327
111.281645	3031.314666	23.449344
111.058352	3038.327615	23.454362
111.182170	3031.718428	23.459379
111.401619	3025.861289	23.464397
111.271950	3033.790709	23.469415
111.665025	3028.572474	23.474432
111.610282	3029.698295	23.479450
111.995795	3041.530512	23.484467
112.406704	3052.393013	23.489485
112.456438	3057.106844	23.494503
112.174060	3053.776966	23.499520
112.397166	3060.067108	23.504538
112.489333	3057.745680	23.509555
112.730537	3057.989057	23.514573
112.580226	3044.122469	23.519591
112.916787	3062.343968	23.524608
112.499010	3057.185690	23.529626
112.897954	3049.429025	23.534643
112.763618	3060.275426	23.539661
112.963739	3070.198676	23.544679
113.332704	3070.015023	23.549696
113.173047	3071.204523	23.554714
113.068343	3072.180319	23.559731
113.006006	3077.801627	23.564749
113.181911	3094.675263	23.569767
113.136085	3085.662261	23.574784
113.204271	3100.513825	23.579802
114.049409	3109.774884	23.584819
113.970492	3119.902566	23.589837
113.782131	3116.917836	23.594855
114.233064	3122.793795	23.599872
114.369056	3132.894338	23.604890
114.443862	3144.983301	23.609907
114.608755	3135.558733	23.614925
114.883157	3138.905723	23.619943
114.862373	3143.529559	23.624960
114.816212	3157.423731	23.629978
115.117356	3157.323228	23.634995
115.036410	3166.804247	23.640013
115.394231	3165.394596	23.645031
115.583102	3162.755110	23.650048
115.725384	3167.978478	23.655066
115.887451	3175.111382	23.660083
116.049518	3182.032827	23.665101
116.140159	3183.622066	23.670119
116.438877	3187.309298	23.675136
116.072034	3193.382036	23.680154
116.459925	3186.791645	23.685171
116.230944	3192.123321	23.690189
116.308302	3190.129263	23.695207
116.374119	3189.194307	23.700224
115.740575	3197.517861	23.705242
116.419737	3208.389191	23.710259
116.792931	3212.377290	23.715277
116.978091	3219.086849	23.720295
116.991133	3228.546956	23.725312
116.980279	3231.913126	23.730330
117.223760	3240.444174	23.735347
116.935785	3241.451669	23.740365
117.439333	3250.526117	23.745383
117.641338	3258.400841	23.750400
117.760611	3265.594097	23.755418
117.914269	3260.255264	23.760435
118.138102	3263.606995	23.765453
118.390449	3276.646810	23.770471
118.282277	3289.256718	23.775488
118.099602	3281.947151	23.780506
118.511928	3279.525351	23.785523
118.800397	3277.842435	23.790541
118.869188	3287.852531	23.795559
119.032713	3288.868637	23.800576
118.900138	3294.261081	23.805594
119.359455	3293.015519	23.810611
119.441953	3302.982459	23.815629
119.675025	3304.110828	23.820647
119.669214	3299.743657	23.825664
119.548877	3297.338506	23.830682
119.737920	3296.286518	23.835699
119.419566	3309.292120	23.840717
119.804022	3321.345617	23.845735
120.200681	3324.818791	23.850752
120.272485	3330.087897	23.855770
120.260783	3321.463984	23.860787
120.525035	3337.642364	23.865805
120.883412	3342.626988	23.870823
121.079003	3340.671317	23.875840
120.864399	3339.050940	23.880858
120.600033	3341.585501	23.885875
121.129022	3335.932561	23.890893
121.180849	3359.772467	23.895911
121.597009	3365.306742	23.900928
121.463977	3375.670237	23.905946
121.377665	3362.093275	23.910963
121.259580	3362.023325	23.915981
121.596394	3374.425140	23.920999
122.070831	3374.600648	23.926016
122.358026	3378.043533	23.931034
122.126576	3386.803245	23.936051
122.073975	3384.920928	23.941069
122.321469	3387.363179	23.946087
123.174120	3389.594434	23.951104
123.334854	3401.332482	23.956122
123.353362	3393.230911	23.961139
123.376812	3374.605921	23.966157
123.386463	3375.453463	23.971175
123.609168	3362.469091	23.976192
123.604128	3375.163999	23.981210
123.500719	3375.890273	23.986227
123.894299	3381.686875	23.991245
123.690945	3386.856810	23.996263
124.152504	3379.011351	24.001280
123.981442	3377.759774	24.006298
124.159817	3378.167590	24.011315
124.045867	3384.365139	24.016333
123.787663	3394.025372	24.021351
124.321419	3394.040148	24.026368
124.235816	3411.115761	24.031386
124.462543	3399.926596	24.036403
124.814040	3405.856004	24.041421
124.425875	3408.779121	24.046439
124.900406	3422.040100	24.051456
124.655355	3426.348591	24.056474
124.831012	3429.625793	24.061491
125.303120	3439.822518	24.066509
125.105773	3447.087235	24.071527
125.628970	3454.113526	24.076544
125.547349	3459.804235	24.081562
125.391444	3462.877414	24.086579
125.536828	3472.601100	24.091597
125.743915	3487.223049	24.096615
126.222569	3480.482706	24.101632
125.956192	3486.596711	24.106650
126.191085	3503.559389	24.111667
126.822647	3505.992359	24.116685
126.390040	3510.544691	24.121703
126.572053	3515.869285	24.126720
126.711115	3518.779771	24.131738
127.090021	3525.497154	24.136755
127.386487	3531.368892	24.141773
127.148058	3540.603194	24.146791
127.412273	3537.844613	24.151808
127.619021	3552.722320	24.156826
127.754396	3567.712150	24.161843
127.719365	3562.977032	24.166861
127.601991	3567.464519	24.171879
128.062918	3573.092887	24.176896
128.350501	3580.480999	24.181914
128.317422	3590.232534	24.186931
128.816555	3585.957112	24.191949
128.463955	3593.435432	24.196967
128.923903	3581.351358	24.201984
128.979516	3589.498359	24.207002
128.907129	3607.509491	24.212019
129.284403	3598.468234	24.217037
129.025350	3612.380121	24.222055
129.243925	3609.379295	24.227072
129.504276	3612.643344	24.232090
129.878480	3620.008518	24.237107
130.292670	3632.300623	24.242125
130.052068	3628.979913	24.247143
129.804929	3628.254625	24.252160
129.847418	3628.648886	24.257178
129.954984	3644.302756	24.262195
130.552212	3643.790034	24.267213
130.343041	3655.661588	24.272231
130.531318	3658.517091	24.277248
130.689314	3658.208470	24.282266
130.560887	3674.748130	24.287283
130.814493	3673.540883	24.292301
130.988339	3681.950421	24.297319
131.774309	3683.538760	24.302336
131.780102	3685.472656	24.307354
132.153627	3692.493938	24.312371
132.252686	3677.477047	24.317389
132.319633	3686.480819	24.322407
132.299865	3682.226195	24.327424
132.812172	3679.637278	24.332442
132.680798	3686.885507	24.337459
132.986930	3675.794277	24.342477
132.899542	3679.967814	24.347495
132.827548	3676.876498	24.352512
132.867824	3672.716684	24.357530
132.853543	3671.387021	24.362547
133.151564	3673.524760	24.367565
132.811083	3690.110075	24.372583
133.254514	3683.065831	24.377600
133.381139	3683.488024	24.382618
133.543313	3690.867301	24.387635
133.348292	3692.608372	24.392653
133.319189	3708.091047	24.397671
133.758190	3713.546125	24.402688
133.843827	3721.953634	24.407706
133.960684	3734.427819	24.412723
134.416018	3737.156537	24.417741
134.285298	3752.077482	24.422759
134.313877	3754.203524	24.427776
134.628995	3754.656341	24.432794
134.343746	3767.268902	24.437811
134.813888	3782.086853	24.442829
134.850294	3784.596741	24.447847
134.893913	3792.998201	24.452864
135.120312	3798.956685	24.457882
135.180162	3804.407696	24.462899
135.489977	3817.180145	24.467917
135.781786	3826.619257	24.472935
136.290375	3826.139268	24.477952
136.434365	3819.207873	24.482970
136.261555	3825.279019	24.487987
136.342476	3814.677266	24.493005
137.100654	3824.204736	24.498023
137.411425	3824.595107	24.503040
137.854058	3823.872887	24.508058
137.548759	3817.765785	24.513075
137.900656	3797.280696	24.518093
137.751250	3802.947348	24.523111
137.635821	3794.980074	24.528128
137.621503	3788.805585	24.533146
137.688158	3803.957810	24.538163
138.038206	3811.550916	24.543181
138.235503	3822.683861	24.548199
138.334177	3826.834776	24.553216
138.415307	3819.666980	24.558234
138.025535	3822.754537	24.563251
138.219536	3822.730682	24.568269
138.391266	3839.021762	24.573287
138.370719	3848.512674	24.578304
138.763851	3849.066972	24.583322
138.460781	3856.461938	24.588339
138.828090	3866.318566	24.593357
138.741264	3877.274843	24.598375
138.856056	3892.602710	24.603392
139.333990	3900.198037	24.608410
139.293660	3902.634670	24.613427
139.569988	3914.819026	24.618445
139.788567	3923.597308	24.623463
139.817229	3922.137847	24.628480
140.638709	3924.206743	24.633498
140.247956	3940.796958	24.638515
140.507838	3946.952279	24.643533
140.726278	3948.954097	24.648551
141.149131	3944.608406	24.653568
141.376515	3944.762417	24.658586
141.376963	3945.412575	24.663603
141.642689	3953.141963	24.668621
141.790714	3951.408259	24.673639
142.016997	3960.822924	24.678656
141.714249	3953.449716	24.683674
142.041339	3959.711359	24.688691
141.782837	3962.434469	24.693709
141.957686	3960.731306	24.698727
142.188050	3969.684526	24.703744
142.397996	3982.475798	24.708762
142.434241	3993.223607	24.713779
142.538802	3990.950631	24.718797
142.594748	3992.665282	24.723815
142.478707	3996.180535	24.728832
143.142621	4005.659653	24.733850
142.938794	4013.872488	24.738867
142.824418	4022.185027	24.743885
143.240681	4020.763056	24.748903
143.081921	4031.443405	24.753920
143.473274	4028.516611	24.758938
143.626828	4046.736038	24.763955
143.691760	4053.363626	24.768973
143.879720	4069.068475	24.773991
143.938269	4074.560802	24.779008
144.482818	4075.129409	24.784026
144.093552	4086.164462	24.789043
144.260921	4089.373637	24.794061
144.681106	4100.216392	24.799079
144.729048	4100.619283	24.804096
144.905818	4107.911238	24.809114
145.010812	4126.801128	24.814131
145.083834	4134.143965	24.819149
145.538283	4132.709729	24.824167
145.638038	4151.815088	24.829184
146.055542	4159.044333	24.834202
146.211460	4162.703499	24.839219
146.227379	4157.218563	24.844237
146.446949	4154.406870	24.849255
146.517190	4171.162245	24.854272
147.027601	4170.517838	24.859290
146.907492	4180.879783	24.864307
146.815561	4183.005700	24.869325
147.057771	4172.555380	24.874343
146.960779	4185.015826	24.879360
147.581784	4184.963367	24.884378
147.459437	4197.875964	24.889395
147.537011	4195.474599	24.894413
147.829998	4209.865976	24.899431
148.114707	4216.219527	24.904448
148.563559	4224.924229	24.909466
148.388983	4224.882007	24.914483
148.281868	4212.248225	24.919501
148.946325	4219.827273	24.924519
149.152044	4239.591678	24.929536
149.141047	4240.887516	24.934554
148.820380	4240.457718	24.939571
149.253889	4248.413617	24.944589
149.088370	4236.672680	24.949607
149.180304	4253.885576	24.954624
149.629321	4261.624436	24.959642
149.892659	4267.952927	24.964659
149.539082	4274.525814	24.969677
150.102613	4277.584967	24.974695
149.957601	4288.345390	24.979712
150.405878	4284.522767	24.984730
150.778858	4292.494421	24.989747
150.790463	4308.255342	24.994765
150.832487	4311.941739	24.999783
150.689981	4322.180998	25.004800
151.054163	4311.178188	25.009818
151.125954	4329.328566	25.014835
151.076858	4332.183257	25.019853
151.201903	4335.146559	25.024871
151.333787	4352.877280	25.029888
151.831946	4358.796796	25.034906
151.586627	4362.288058	25.039923
151.845716	4374.980423	25.044941
152.359388	4383.883428	25.049959
152.123152	4391.877380	25.054976
152.635360	4382.107705	25.059994
152.516860	4402.292058	25.065011
152.689104	4401.753950	25.070029
153.172694	4402.385718	25.075047
153.381685	4397.650266	25.080064
153.219146	4407.744344	25.085082
153.447565	4414.624370	25.090099
153.639944	4418.091687	25.095117
153.961749	4425.553727	25.100135
154.006447	4432.875845	25.105152
154.218952	4422.609918	25.110170
154.645453	4436.478829	25.115187
154.678044	4437.859430	25.120205
154.650441	4438.788575	25.125223
154.936568	4441.045044	25.130240
154.893876	4447.771598	25.135258
155.278751	4439.883964	25.140275
154.695979	4450.349658	25.145293
155.340607	4453.787604	25.150311
155.269545	4462.289294	25.155328
155.730466	4467.207766	25.160346
156.001570	4485.182076	25.165363
156.191169	4483.520758	25.170381
156.177855	4481.963627	25.175399
156.287192	4494.963463	25.180416
156.470162	4488.593889	25.185434
157.152471	4498.168250	25.190451
156.858026	4509.002572	25.195469
156.914018	4512.772057	25.200487
156.983262	4522.334564	25.205504
157.560381	4508.097930	25.210522
157.544638	4516.319586	25.215539
157.595381	4537.004852	25.220557
157.795137	4529.575266	25.225575
157.958482	4533.798341	25.230592
158.051745	4529.756335	25.235610
158.258878	4539.654052	25.240627
158.424077	4551.720416	25.245645
158.589248	4551.224439	25.250663
158.664808	4554.785722	25.255680
158.615335	4550.690181	25.260698
158.627132	4566.284009	25.265715
159.038539	4574.215085	25.270733
159.216412	4578.473785	25.275751
159.398646	4595.824454	25.280768
159.268577	4607.696941	25.285786
159.625851	4610.115955	25.290803
160.016217	4615.219054	25.295821
160.232839	4627.318495	25.300839
160.013759	4630.070287	25.305856
160.438194	4621.362069	25.310874
160.881534	4628.745300	25.315891
160.812215	4641.028150	25.320909
161.499324	4654.509453	25.325927
161.052828	4651.391054	25.330944
161.175920	4657.419565	25.335962
161.513099	4655.334393	25.340979
161.375595	4668.814679	25.345997
161.865617	4674.805007	25.351015
161.702327	4683.393757	25.356032
161.687958	4678.172203	25.361050
162.018612	4692.131987	25.366067
161.865306	4692.515721	25.371085
162.395820	4698.158862	25.376103
162.586041	4723.497247	25.381120
162.805665	4725.533688	25.386138
163.001492	4722.978118	25.391155
162.787686	4731.644196	25.396173
163.369981	4739.173128	25.401191
163.428988	4747.184398	25.406208
163.635266	4745.971825	25.411226
163.600742	4749.190455	25.416243
163.614024	4758.392500	25.421261
164.126020	4766.645737	25.426279
164.094257	4762.847249	25.431296
164.095208	4767.622781	25.436314
164.719584	4784.466053	25.441331
164.735704	4799.756393	25.446349
164.797795	4796.252615	25.451367
164.831016	4796.803008	25.456384
164.998219	4810.220177	25.461402
165.616119	4813.927493	25.466419
165.261553	4819.642185	25.471437
165.597482	4823.920525	25.476455
165.676361	4835.820602	25.481472
165.783131	4839.635909	25.486490
165.901957	4840.939986	25.491507
166.379181	4855.012802	25.496525
166.757409	4854.262697	25.501543
166.640512	4871.865369	25.506560
166.831061	4879.660519	25.511578
166.964451	4884.134540	25.516595
167.184831	4890.873961	25.521613
167.277264	4894.060225	25.526631
167.378583	4904.716378	25.531648
167.545135	4910.668765	25.536666
167.922769	4910.256488	25.541683
167.965083	4927.272581	25.546701
168.290194	4928.172089	25.551719
168.124384	4940.934160	25.556736
167.919605	4951.211877	25.561754
168.612746	4952.893700	25.566771
168.739151	4962.144521	25.571789
168.795215	4978.183181	25.576807
169.011689	4993.164724	25.581824
169.095401	4995.831551	25.586842
169.218953	5010.145782	25.591859
169.487724	5019.352372	25.596877
170.201853	5028.050882	25.601895
170.100443	5039.486756	25.606912
170.442757	5038.499188	25.611930
170.560469	5037.546588	25.616947
170.850580	5049.420231	25.621965
171.204706	5054.541723	25.626983
171.649500	5061.205233	25.632000
171.381301	5055.865266	25.637018
171.880829	5049.954400	25.642035
171.683681	5059.508162	25.647053
172.403518	5041.192845	25.652071
172.714407	5040.819365	25.657088
172.419990	5046.417444	25.662106
172.772742	5040.175909	25.667123
172.917340	5039.140212	25.672141
172.878543	5035.929863	25.677159
172.736301	5036.198249	25.682176
173.006755	5052.743351	25.687194
172.827341	5051.638153	25.692212
173.335474	5057.827802	25.697229
173.854285	5049.723353	25.702247
173.963446	5047.695732	25.707264
173.945241	5072.603056	25.712282
174.293068	5080.067629	25.717300
174.161189	5080.141858	25.722317
174.311214	5078.521369	25.727335
174.378400	5081.089774	25.732352
174.586838	5090.981277	25.737370
174.715335	5101.402892	25.742388
174.863159	5104.826775	25.747405
175.007861	5104.870569	25.752423
175.071399	5102.758508	25.757440
174.957973	5118.542755	25.762458
175.231161	5126.631323	25.767476
175.245401	5120.871743	25.772493
175.696232	5138.581986	25.777511
175.836307	5143.174977	25.782528
175.827766	5165.009675	25.787546
176.293228	5161.588224	25.792564
176.056560	5180.870149	25.797581
176.543703	5192.694272	25.802599
176.881118	5207.303636	25.807616
176.791911	5208.229786	25.812634
177.148689	5220.904379	25.817652
177.184991	5227.704149	25.822669
177.115178	5233.049518	25.827687
177.559230	5253.630176	25.832704
177.892308	5255.099786	25.837722
178.183259	5260.824592	25.842740
178.593209	5272.184155	25.847757
178.644826	5279.369809	25.852775
179.094797	5272.292371	25.857792
179.171255	5292.254813	25.862810
179.254621	5293.267733	25.867828
179.139040	5297.101972	25.872845
179.224457	5302.568393	25.877863
179.842363	5305.928596	25.882880
179.846469	5318.298324	25.887898
179.850893	5316.343797	25.892916
180.185437	5329.006145	25.897933
180.409497	5337.825296	25.902951
180.849761	5346.320391	25.907968
180.250418	5351.912377	25.912986
180.932249	5366.250448	25.918004
181.013175	5371.717590	25.923021
180.788723	5373.614914	25.928039
181.787188	5387.199803	25.933056
181.524723	5385.548812	25.938074
181.866218	5387.096034	25.943092
181.959493	5413.425839	25.948109
181.818386	5423.817014	25.953127
181.928152	5427.006987	25.958144
182.231658	5443.354751	25.963162
182.515484	5445.804254	25.968180
182.747226	5459.372838	25.973197
183.262185	5468.222519	25.978215
183.754814	5466.545499	25.983232
183.553987	5479.367060	25.988250
183.983608	5487.131564	25.993268
184.135518	5497.158350	25.998285
184.306582	5492.191780	26.003303
184.464758	5492.255574	26.008320
184.526417	5505.456106	26.013338
184.774379	5515.467948	26.018356
184.898196	5522.216325	26.023373
184.970790	5512.050479	26.028391
185.361153	5506.569969	26.033408
185.591581	5527.480912	26.038426
185.794885	5537.184065	26.043444
185.804604	5529.130256	26.048461
185.939510	5544.933027	26.053479
186.355520	5532.226350	26.058496
185.956132	5551.998012	26.063514
186.204499	5554.999132	26.068532
186.436803	5572.159861	26.073549
186.468749	5581.258407	26.078567
186.960516	5590.092819	26.083584
186.795933	5593.524397	26.088602
187.112133	5596.265596	26.093620
187.440701	5610.210631	26.098637
187.731693	5626.150156	26.103655
187.875516	5619.202319	26.108672
187.708071	5636.911454	26.113690
188.006649	5651.798687	26.118708
188.739352	5648.089328	26.123725
188.695874	5666.640933	26.128743
188.818933	5675.766376	26.133760
189.277400	5666.717767	26.138778
189.239643	5653.292512	26.143796
189.387522	5672.246779	26.148813
189.399447	5684.167306	26.153831
189.732892	5685.157096	26.158848
189.561216	5698.062656	26.163866
189.867547	5703.226496	26.168884
190.418337	5703.554291	26.173901
190.676676	5719.994564	26.178919
190.731253	5723.407829	26.183936
190.983248	5735.423589	26.188954
190.827269	5732.976312	26.193972
191.305280	5745.600832	26.198989
191.024418	5755.048041	26.204007
191.354756	5765.467021	26.209024
191.436833	5785.539610	26.214042
191.699838	5798.213424	26.219060
192.281371	5801.026981	26.224077
192.447618	5802.929810	26.229095
192.678193	5811.798682	26.234112
192.791571	5830.663788	26.239130
192.900481	5825.523721	26.244148
193.639201	5829.711181	26.249165
193.686682	5846.247529	26.254183
193.818248	5852.483453	26.259200
193.640431	5847.716307	26.264218
193.895748	5848.819281	26.269236
194.313741	5862.128737	26.274253
193.917304	5870.833259	26.279271
194.288968	5875.617655	26.284288
194.534747	5886.599118	26.289306
194.582773	5881.724200	26.294324
195.411334	5903.047507	26.299341
195.252007	5915.417832	26.304359
195.659943	5924.249676	26.309376
196.139691	5938.345039	26.314394
196.446942	5936.554792	26.319412
196.602226	5937.714382	26.324429
196.380068	5944.185335	26.329447
196.801692	5944.896256	26.334464
196.725195	5961.672973	26.339482
196.839658	5954.843217	26.344500
197.297591	5965.510760	26.349517
197.468136	5982.144865	26.354535
197.904885	5974.216929	26.359552
197.819548	5977.866674	26.364570
197.925627	5972.616526	26.369588
198.162023	5995.528372	26.374605
198.080471	6006.153665	26.379623
198.642258	6009.137631	26.384640
198.893623	6024.360809	26.389658
199.013897	6045.059062	26.394676
199.328654	6040.672888	26.399693
198.885176	6048.456770	26.404711
199.248291	6052.604904	26.409728
199.483716	6064.197316	26.414746
199.418811	6074.687479	26.419764
200.240538	6082.981483	26.424781
200.038871	6091.460075	26.429799
200.330723	6106.146703	26.434816
200.386015	6107.492329	26.439834
200.365949	6117.937656	26.444852
200.933149	6127.009962	26.449869
200.605446	6149.460569	26.454887
201.041715	6157.483171	26.459904
201.440756	6155.034656	26.464922
201.590554	6177.016374	26.469940
201.889820	6187.790823	26.474957
201.717423	6189.282387	26.479975
202.226618	6208.906990	26.484992
202.327204	6218.070927	26.490010
202.608264	6235.739225	26.495028
203.034445	6239.129455	26.500045
203.029047	6258.531188	26.505063
203.433889	6266.309354	26.510080
203.583978	6271.238835	26.515098
203.737739	6276.527606	26.520116
204.290873	6287.865513	26.525133
204.482330	6300.980123	26.530151
204.706494	6294.676109	26.535168
204.306872	6303.501285	26.540186
204.441842	6310.005154	26.545204
204.976891	6322.005643	26.550221
204.957298	6339.632463	26.555239
205.260953	6344.421258	26.560256
205.430417	6363.016177	26.565274
205.786427	6377.121675	26.570292
205.812903	6383.475156	26.575309
206.447210	6402.341824	26.580327
206.530094	6404.983734	26.585344
206.749271	6422.137836	26.590362
206.844889	6436.321800	26.595380
207.078612	6436.790520	26.600397
207.237255	6468.260243	26.605415
207.132373	6463.500520	26.610432
207.643199	6475.612210	26.615450
207.461746	6484.296178	26.620468
208.022527	6504.964251	26.625485
208.398219	6528.063421	26.630503
208.362784	6524.533458	26.635520
208.717405	6538.004797	26.640538
209.144969	6542.294533	26.645556
209.478857	6550.383756	26.650573
209.289302	6564.782680	26.655591
210.189811	6566.422907	26.660608
209.984611	6567.828064	26.665626
210.107356	6588.520235	26.670644
210.195547	6589.324132	26.675661
210.477437	6591.448951	26.680679
210.714482	6602.612139	26.685696
210.969180	6607.992620	26.690714
211.118219	6623.806753	26.695732
211.563394	6629.681602	26.700749
211.646825	6639.151467	26.705767
211.895549	6648.137877	26.710784
211.850709	6657.425691	26.715802
212.255601	6664.073909	26.720820
212.541336	6665.146945	26.725837
212.879446	6685.341655	26.730855
212.954362	6694.298326	26.735872
213.680414	6677.126308	26.740890
214.808180	6661.586930	26.745908
214.963413	6652.824958	26.750925
215.156123	6654.256560	26.755943
215.113835	6650.522452	26.760960
215.185749	6643.449682	26.765978
214.821195	6640.930583	26.770996
215.009464	6645.895259	26.776013
215.101010	6645.555900	26.781031
215.416995	6643.259148	26.786048
215.417393	6638.018949	26.791066
215.232621	6642.413512	26.796084
215.805401	6650.042585	26.801101
215.533546	6665.792857	26.806119
215.556784	6666.644751	26.811136
215.819884	6667.857051	26.816154
216.057571	6685.879779	26.821172
216.276292	6697.762458	26.826189
216.155600	6719.262922	26.831207
216.218468	6733.919414	26.836224
216.577726	6748.416131	26.841242
217.013452	6767.651866	26.846260
217.201143	6781.266175	26.851277
217.526693	6800.282341	26.856295
217.803537	6816.158819	26.861312
218.016048	6822.922279	26.866330
218.102472	6847.591606	26.871348
218.230223	6853.790586	26.876365
218.612814	6872.760065	26.881383
218.766967	6892.693222	26.886400
219.046260	6902.176925	26.891418
218.987696	6919.441028	26.896436
219.458300	6934.185725	26.901453
219.960177	6953.780701	26.906471
219.973874	6962.377691	26.911488
220.272703	6966.169857	26.916506
220.616996	6981.515107	26.921524
221.016380	6989.588015	26.926541
221.540061	7001.098263	26.931559
221.460856	7005.940526	26.936576
221.998885	7012.719670	26.941594
221.846052	7021.901367	26.946612
221.963523	7035.829850	26.951629
222.195182	7041.532882	26.956647
222.633180	7064.168451	26.961664
223.087059	7074.941450	26.966682
223.037440	7076.451852	26.971700
223.329850	7091.808429	26.976717
223.319502	7098.859233	26.981735
223.658095	7107.216300	26.986752
224.174216	7113.749505	26.991770
224.184197	7129.137457	26.996788
224.723890	7138.808032	27.001805
224.713475	7145.565281	27.006823
224.664796	7156.107202	27.011840
225.017147	7158.988225	27.016858
225.678457	7170.833874	27.021876
225.559513	7173.851411	27.026893
225.869830	7179.715866	27.031911
226.260206	7195.985385	27.036928
226.594587	7189.670219	27.041946
226.338402	7210.422087	27.046964
226.516460	7213.153472	27.051981
227.018382	7213.012229	27.056999
226.945132	7239.105418	27.062016
227.262891	7236.723083	27.067034
227.596918	7261.928962	27.072052
227.595905	7269.136220	27.077069
227.851846	7274.002139	27.082087
228.196436	7284.716513	27.087104
228.691667	7290.050277	27.092122
228.608810	7300.480799	27.097140
228.881102	7305.382064	27.102157
229.086412	7318.870912	27.107175
229.339185	7325.369429	27.112192
229.779641	7334.777756	27.117210
230.392570	7322.746319	27.122228
230.471929	7324.116700	27.127245
230.926496	7326.489368	27.132263
230.908068	7327.234134	27.137280
231.264512	7325.805447	27.142298
231.152608	7342.977234	27.147316
231.477963	7342.320501	27.152333
231.604001	7346.401667	27.157351
231.558116	7352.848829	27.162368
232.403266	7359.507681	27.167386
232.167352	7375.221396	27.172404
232.101783	7367.333184	27.177421
232.486494	7388.111748	27.182439
232.357854	7401.952551	27.187456
233.292670	7404.092617	27.192474
233.120223	7420.819314	27.197492
233.358803	7430.038139	27.202509
233.641296	7457.130646	27.207527
233.541883	7454.238681	27.212544
234.237310	7459.102522	27.217562
234.158736	7477.222620	27.222580
234.144152	7494.669829	27.227597
234.416975	7501.092678	27.232615
234.537827	7525.391358	27.237632
235.285017	7524.732083	27.242650
235.283110	7542.928702	27.247668
235.567809	7553.204280	27.252685
236.039137	7564.659897	27.257703
236.113292	7577.512722	27.262720
236.728694	7584.753568	27.267738
236.962912	7599.283054	27.272756
236.870378	7608.092613	27.277773
237.337682	7614.763031	27.282791
237.159372	7625.877861	27.287808
237.608922	7644.736696	27.292826
237.809907	7656.837428	27.297844
237.910700	7674.828774	27.302861
238.322290	7678.246803	27.307879
238.386445	7688.421045	27.312896
238.897909	7703.920819	27.317914
239.280497	7714.639000	27.322932
239.527737	7730.947063	27.327949
239.852632	7725.674975	27.332967
240.055390	7739.158216	27.337984
240.658309	7739.294842	27.343002
241.083745	7750.552521	27.348020
240.692877	7758.407853	27.353037
241.286634	7755.477376	27.358055
241.080487	7778.179385	27.363072
241.333449	7774.490633	27.368090
241.834697	7790.112033	27.373108
241.778966	7802.552737	27.378125
242.241122	7816.762784	27.383143
242.264195	7830.147789	27.388160
242.147605	7829.506178	27.393178
242.591505	7851.343095	27.398196
242.562970	7860.745786	27.403213
242.983819	7872.199984	27.408231
243.233370	7892.454010	27.413248
243.644747	7913.225859	27.418266
244.005422	7928.417819	27.423284
243.794527	7938.357210	27.428301
244.173505	7945.401393	27.433319
244.238317	7966.034684	27.438336
244.400078	7978.713145	27.443354
244.887955	7988.354355	27.448372
245.064387	8001.005291	27.453389
245.433071	8010.668227	27.458407
246.000890	8019.842405	27.463424
246.254613	8042.675190	27.468442
246.360970	8055.539120	27.473460
246.611002	8065.855109	27.478477
246.789476	8066.720784	27.483495
246.958751	8081.279704	27.488512
246.764068	8093.025602	27.493530
246.849601	8100.248124	27.498548
247.453806	8122.249825	27.503565
248.152276	8127.978387	27.508583
248.335402	8145.007122	27.513600
248.486396	8146.060185	27.518618
248.864831	8167.475162	27.523636
249.079169	8180.925354	27.528653
249.526939	8187.782129	27.533671
249.579513	8207.432612	27.538688
249.737287	8212.257239	27.543706
250.396806	8213.950932	27.548724
250.364107	8225.472805	27.553741
250.630362	8236.092593	27.558759
251.144697	8254.263212	27.563776
251.286529	8258.449460	27.568794
251.533134	8271.566366	27.573812
251.941947	8282.738563	27.578829
251.974806	8280.621443	27.583847
252.022209	8297.560953	27.588864
252.150763	8300.060274	27.593882
252.708687	8324.999135	27.598900
252.341088	8331.635634	27.603917
252.813044	8347.483061	27.608935
253.077437	8360.976104	27.613952
253.432005	8385.207961	27.618970
253.527290	8395.403004	27.623988
253.951060	8418.181367	27.629005
254.212037	8425.458785	27.634023
254.352027	8452.379207	27.639040
254.752555	8467.508581	27.644058
254.797789	8480.016105	27.649076
255.346284	8500.505236	27.654093
255.564606	8507.072677	27.659111
256.018329	8525.590804	27.664128
255.810753	8532.290859	27.669146
256.225804	8550.906587	27.674164
256.246778	8564.857565	27.679181
256.569530	8579.121476	27.684199
256.925073	8602.488432	27.689216
257.134959	8617.799149	27.694234
257.736475	8632.193340	27.699252
257.558027	8654.459594	27.704269
258.119534	8660.067580	27.709287
258.628408	8669.727979	27.714304
258.846692	8687.935646	27.719322
259.249655	8692.864295	27.724340
259.652283	8707.238996	27.729357
260.064381	8708.024131	27.734375
260.378237	8717.411837	27.739392
260.236898	8722.589403	27.744410
260.791148	8728.605804	27.749428
260.921848	8733.886247	27.754445
261.694869	8733.986932	27.759463
261.314793	8731.087948	27.764480
261.331084	8756.973603	27.769498
261.667246	8760.270982	27.774516
262.178809	8769.280654	27.779533
262.581964	8788.820347	27.784551
262.728666	8780.503846	27.789568
262.487939	8790.363096	27.794586
262.527427	8804.949107	27.799604
263.037122	8817.485577	27.804621
263.295910	8829.593867	27.809639
263.689374	8838.773501	27.814656
263.605555	8851.740207	27.819674
264.131306	8864.911946	27.824692
264.160352	8877.485402	27.829709
264.141451	8887.089171	27.834727
264.648756	8906.552788	27.839744
264.963495	8918.469313	27.844762
265.435522	8937.019733	27.849780
265.318223	8955.314637	27.854797
265.673445	8962.236625	27.859815
266.179384	8979.092744	27.864832
266.362890	8998.606870	27.869850
266.698280	9010.744395	27.874868
266.861567	9028.541061	27.879885
267.546440	9050.477641	27.884903
267.785411	9064.139328	27.889920
267.863825	9069.570078	27.894938
268.263210	9072.920814	27.899956
268.635665	9087.117394	27.904973
268.623322	9092.590695	27.909991
269.186300	9096.607382	27.915008
269.427744	9114.742406	27.920026
269.672814	9120.706043	27.925044
269.585405	9134.642753	27.930061
270.061235	9152.886553	27.935079
270.236606	9156.152207	27.940096
270.592885	9167.825638	27.945114
270.992566	9187.928270	27.950132
270.965206	9200.324454	27.955149
271.525117	9223.755094	27.960167
271.975334	9218.763005	27.965184
272.195893	9238.230572	27.970202
272.286460	9255.738846	27.975220
272.790732	9254.564834	27.980237
272.894071	9278.417071	27.985255
273.041022	9289.949524	27.990272
273.138967	9312.606072	27.995290
273.734632	9318.044769	28.000308
274.016332	9338.929973	28.005325
273.944416	9338.353968	28.010343
274.219241	9364.216008	28.015360
273.819503	9380.689399	28.020378
274.333136	9401.248102	28.025396
275.103671	9423.550654	28.030413
275.278026	9450.899716	28.035431
275.675680	9457.527978	28.040448
276.078589	9482.110513	28.045466
276.499729	9484.573916	28.050484
276.728017	9509.565698	28.055501
276.814948	9512.523147	28.060519
277.431896	9538.123789	28.065536
277.820503	9538.887362	28.070554
278.200785	9551.592870	28.075572
278.149637	9570.686332	28.080589
278.281317	9574.246171	28.085607
278.978176	9576.575102	28.090624
279.200334	9589.649391	28.095642
279.374762	9603.807739	28.100660
279.547009	9614.193535	28.105677
279.798097	9632.545415	28.110695
280.555260	9628.345257	28.115712
280.645529	9638.541766	28.120730
281.067822	9644.067539	28.125748
281.520585	9656.070398	28.130765
281.619180	9642.980928	28.135783
281.758174	9646.684875	28.140800
281.672673	9660.432248	28.145818
282.043348	9663.904380	28.150836
282.236369	9671.698030	28.155853
282.189231	9687.049647	28.160871
282.961314	9704.821642	28.165888
282.949178	9721.437055	28.170906
282.963733	9731.326519	28.175924
283.281136	9747.391804	28.180941
283.663605	9759.383572	28.185959
283.951609	9773.256000	28.190976
283.889662	9799.606781	28.195994
284.347058	9809.847260	28.201012
284.849495	9825.246036	28.206029
284.946923	9844.670264	28.211047
285.184164	9856.059564	28.216064
285.393923	9880.038084	28.221082
285.936012	9899.178446	28.226100
286.087848	9917.012478	28.231117
286.317954	9942.459209	28.236135
286.788528	9952.896626	28.241152
287.147336	9977.767684	28.246170
287.584932	9982.893356	28.251188
288.226948	10000.164929	28.256205
288.092274	10000.747933	28.261223
288.663309	10006.743198	28.266240
289.010253	10024.101776	28.271258
289.291396	10037.372424	28.276276
289.403301	10049.678032	28.281293
289.338435	10055.109277	28.286311
289.681644	10073.093631	28.291328
289.975663	10095.284898	28.296346
290.199803	10112.129091	28.301364
290.624431	10127.795975	28.306381
290.807189	10148.643820	28.311399
291.340911	10161.221666	28.316416
291.908031	10181.700289	28.321434
291.867849	10197.903725	28.326452
292.397211	10203.798193	28.331469
292.386555	10224.729909	28.336487
292.888590	10237.337999	28.341504
293.347868	10250.066418	28.346522
293.425321	10269.854137	28.351540
293.795516	10275.615540	28.356557
293.529591	10295.128380	28.361575
293.952582	10314.085642	28.366592
294.401819	10334.058664	28.371610
294.634544	10349.152556	28.376628
294.977259	10362.792734	28.381645
295.162048	10395.638538	28.386663
295.491471	10400.976925	28.391680
296.125183	10426.563555	28.396698
296.202507	10444.899086	28.401716
296.664951	10451.097687	28.406733
297.344413	10465.882163	28.411751
297.716877	10477.822278	28.416768
297.775442	10498.149936	28.421786
297.973199	10500.784022	28.426804
298.493546	10516.824693	28.431821
298.625428	10534.135137	28.436839
298.906266	10541.410298	28.441856
299.048120	10558.896027	28.446874
299.403483	10567.375195	28.451892
299.946677	10568.976717	28.456909
300.011920	10595.855053	28.461927
300.661313	10597.601072	28.466944
300.946743	10615.389715	28.471962
301.098989	10621.939778	28.476980
301.464654	10627.588329	28.481997
301.512413	10639.778018	28.487015
302.027449	10644.411891	28.492032
302.053628	10649.677579	28.497050
302.752989	10667.297634	28.502068
303.269592	10670.516747	28.507085
302.931457	10678.601902	28.512103
303.003904	10695.356572	28.517120
303.412681	10716.242485	28.522138
303.575232	10725.730545	28.527156
304.281658	10741.859265	28.532173
304.006592	10760.789889	28.537191
304.011976	10774.684963	28.542208
304.372215	10802.325972	28.547226
304.876489	10829.998276	28.552244
305.345673	10846.517655	28.557261
305.338518	10870.505962	28.562279
305.592734	10874.324829	28.567296
306.204272	10897.879002	28.572314
306.405198	10913.887650	28.577332
307.101102	10937.810792	28.582349
307.038115	10958.735691	28.587367
307.297658	10971.811447	28.592384
307.713484	11000.451330	28.597402
308.291901	11021.124883	28.602420
308.778034	11032.018320	28.607437
308.866640	11053.058653	28.612455
309.080511	11067.155139	28.617472
309.555311	11087.661764	28.622490
309.794693	11105.104404	28.627508
310.228698	11113.666303	28.632525
310.535703	11143.772636	28.637543
310.578774	11159.777653	28.642560
310.979377	11178.423530	28.647578
311.067369	11201.765947	28.652596
311.718736	11214.837708	28.657613
311.649560	11235.722832	28.662631
312.031883	11255.615693	28.667648
312.482965	11284.187371	28.672666
312.687238	11304.003805	28.677684
313.264702	11321.905533	28.682701
313.278207	11349.525552	28.687719
313.850680	11371.633940	28.692736
314.183059	11383.969255	28.697754
314.421135	11413.240532	28.702772
314.944133	11428.779526	28.707789
314.922955	11443.784373	28.712807
315.446824	11462.076642	28.717824
316.178206	11476.759113	28.722842
316.134544	11493.920953	28.727860
316.594911	11510.578068	28.732877
316.846768	11531.132519	28.737895
317.227331	11551.139641	28.742912
317.451873	11557.186196	28.747930
317.451127	11579.702986	28.752948
318.196227	11595.220171	28.757965
318.461571	11615.775772	28.762983
319.289755	11636.379547	28.768000
319.238321	11648.105382	28.773018
319.234938	11665.621073	28.778036
319.687372	11681.250202	28.783053
319.742212	11697.269634	28.788071
320.617042	11717.708357	28.793088
320.830722	11737.779550	28.798106
321.003308	11753.559666	28.803124
321.616398	11771.756251	28.808141
321.766370	11781.392056	28.813159
321.698507	11789.798735	28.818176
322.185350	11803.622774	28.823194
322.236166	11818.057814	28.828212
322.751992	11830.431174	28.833229
322.785614	11852.497716	28.838247
322.938040	11878.846471	28.843264
323.265176	11900.415834	28.848282
323.132340	11924.030351	28.853300
323.969859	11946.556012	28.858317
324.295716	11963.193423	28.863335
324.856451	11983.586607	28.868352
325.353941	12002.676080	28.873370
325.359902	12019.701212	28.878388
326.439102	12040.102155	28.883405
326.569981	12061.815934	28.888423
326.608138	12073.957527	28.893440
326.940796	12094.556854	28.898458
327.327575	12120.370552	28.903476
327.647061	12125.145761	28.908493
328.048296	12149.451043	28.913511
328.524491	12170.047052	28.918528
328.788396	12175.099328	28.923546
328.850429	12205.210771	28.928564
329.631317	12202.117862	28.933581
330.385658	12228.790213	28.938599
330.418834	12229.489248	28.943616
330.951592	12237.370018	28.948634
330.505554	12253.303702	28.953652
331.007217	12272.853823	28.958669
331.453815	12293.789291	28.963687
331.812972	12315.139423	28.968704
332.098173	12328.559480	28.973722
332.058995	12350.233755	28.978740
332.458697	12363.923362	28.983757
332.670224	12393.465550	28.988775
333.344941	12417.144425	28.993792
333.473665	12437.396952	28.998810
333.689922	12450.632051	29.003828
334.326550	12473.214883	29.008845
334.631835	12502.562655	29.013863
334.900552	12528.834219	29.018880
335.085181	12535.326230	29.023898
335.389274	12570.484522	29.028916
335.856948	12579.689189	29.033933
336.455297	12600.064558	29.038951
336.779195	12620.236372	29.043968
337.260643	12638.934272	29.048986
337.278126	12660.530612	29.054004
337.398083	12678.842744	29.059021
337.953345	12699.771221	29.064039
337.945085	12722.331598	29.069056
338.492006	12747.101268	29.074074
338.969928	12770.290195	29.079092
339.602695	12790.783565	29.084109
339.906540	12807.185159	29.089127
340.275239	12829.181734	29.094144
340.883386	12843.903413	29.099162
340.830561	12858.188023	29.104180
341.428663	12879.946845	29.109197
341.699009	12892.277021	29.114215
341.957845	12913.071890	29.119232
342.384000	12924.850479	29.124250
342.591464	12946.057580	29.129268
343.038335	12956.440373	29.134285
343.464824	12975.905038	29.139303
343.798289	13003.300836	29.144320
344.177309	13000.601936	29.149338
344.509366	13023.750728	29.154356
344.951184	13030.332340	29.159373
345.178385	13036.265279	29.164391
345.482931	13042.934581	29.169408
345.650070	13057.665086	29.174426
346.017258	13080.135862	29.179444
346.098812	13088.560911	29.184461
346.616738	13102.857901	29.189479
346.883919	13120.677026	29.194496
347.170831	13130.936401	29.199514
347.754183	13153.117827	29.204532
348.194119	13158.768215	29.209549
348.360660	13181.766131	29.214567
348.891674	13200.087405	29.219584
349.463145	13209.004648	29.224602
349.705145	13232.234031	29.229620
349.510530	13241.927388	29.234637
349.912341	13257.897288	29.239655
350.126501	13283.714193	29.244672
350.737723	13302.840966	29.249690
350.864345	13324.967384	29.254708
351.077641	13349.088740	29.259725
351.386435	13369.333180	29.264743
351.825306	13407.961501	29.269760
352.113613	13427.861827	29.274778
352.309237	13457.572367	29.279796
352.812256	13479.024579	29.284813
353.280968	13504.221104	29.289831
353.460278	13525.455344	29.294848
354.110219	13551.520561	29.299866
354.412649	13572.940951	29.304884
354.747679	13595.748927	29.309901
355.407989	13618.212605	29.314919
355.303993	13654.330139	29.319936
355.890772	13657.933591	29.324954
356.859276	13694.755819	29.329972
356.830231	13705.149959	29.334989
357.190764	13715.710826	29.340007
357.724651	13752.101874	29.345024
357.884878	13764.408712	29.350042
358.392847	13784.767854	29.355060
358.544331	13809.423638	29.360077
358.890895	13828.232141	29.365095
359.500612	13847.429175	29.370112
359.761016	13863.854241	29.375130
360.191942	13880.944367	29.380148
360.238979	13902.960691	29.385165
360.965831	13919.985833	29.390183
360.880702	13947.697648	29.395200
361.256106	13966.429164	29.400218
362.027784	13991.658122	29.405236
362.120204	14017.545508	29.410253
362.596400	14036.172979	29.415271
362.979607	14061.143551	29.420288
363.105889	14081.612963	29.425306
363.588577	14094.327722	29.430324
363.980447	14116.536933	29.435341
364.391995	14131.078640	29.440359
364.830575	14161.358795	29.445376
364.773352	14182.501118	29.450394
365.043757	14210.625350	29.455412
365.846059	14229.663312	29.460429
365.989808	14248.175373	29.465447
366.042111	14279.791693	29.470464
366.611618	14303.874598	29.475482
366.990744	14329.531451	29.480500
367.355817	14356.103199	29.485517
368.057012	14368.613591	29.490535
368.016868	14383.431085	29.495552
369.032605	14413.700742	29.500570
369.485966	14418.509380	29.505588
369.873548	14432.189745	29.510605
370.457201	14447.273351	29.515623
370.086209	14461.100256	29.520640
370.511767	14475.911639	29.525658
371.015056	14502.275749	29.530676
371.592493	14517.594075	29.535693
372.418608	14519.038217	29.540711
372.223510	14535.645311	29.545728
372.319073	14550.119685	29.550746
372.977407	14578.588302	29.555764
373.212591	14592.816749	29.560781
373.545654	14619.198048	29.565799
373.964127	14639.417297	29.570816
374.251193	14659.300161	29.575834
374.543628	14674.868260	29.580852
375.169129	14701.570485	29.585869
375.497729	14713.330640	29.590887
375.796893	14732.788513	29.595904
375.628542	14754.994102	29.600922
376.532031	14780.730995	29.605940
376.451823	14805.869435	29.610957
377.551120	14834.411901	29.615975
377.419282	14860.458514	29.620992
377.896810	14876.285351	29.626010
378.190807	14910.369483	29.631028
378.372798	14936.354710	29.636045
378.981442	14949.258872	29.641063
379.492502	14981.326030	29.646080
379.573867	15000.006441	29.651098
380.303413	15030.637452	29.656116
380.599066	15054.350227	29.661133
380.923889	15068.331371	29.666151
381.251915	15108.666866	29.671168
381.612708	15133.149664	29.676186
382.069987	15155.877320	29.681204
382.171081	15186.495885	29.686221
382.218169	15207.995769	29.691239
382.937970	15241.006744	29.696256
383.063624	15271.969022	29.701274
383.594542	15292.177776	29.706292
384.218478	15323.997389	29.711309
384.793757	15341.786427	29.716327
385.301696	15381.412318	29.721344
385.913902	15403.298175	29.726362
386.409021	15424.671706	29.731380
386.176244	15449.800006	29.736397
386.676195	15470.932812	29.741415
387.029413	15501.165225	29.746432
387.592596	15521.107066	29.751450
388.051087	15549.365064	29.756468
388.499819	15578.512089	29.761485
388.816771	15603.337089	29.766503
388.751324	15627.852138	29.771520
389.192061	15654.792909	29.776538
389.460439	15681.905831	29.781556
390.116589	15720.429228	29.786573
390.576080	15743.274096	29.791591
390.888813	15769.691735	29.796608
391.388742	15805.883555	29.801626
391.744129	15825.156927	29.806644
392.349142	15853.335715	29.811661
392.984371	15882.757365	29.816679
393.165166	15907.095472	29.821696
393.529762	15930.656479	29.826714
393.670290	15947.733666	29.831732
394.154221	15970.751867	29.836749
394.780624	15991.284435	29.841767
395.088952	16008.111313	29.846784
395.200839	16026.153155	29.851802
395.967915	16057.651668	29.856820
395.751633	16078.893493	29.861837
396.502326	16095.408389	29.866855
397.057401	16121.346621	29.871872
397.248855	16143.434639	29.876890
397.235369	16167.026372	29.881908
397.623718	16202.844680	29.886925
398.034932	16224.200585	29.891943
398.466115	16264.083447	29.896960
398.980583	16286.013959	29.901978
400.022127	16301.198303	29.906996
400.675442	16313.344748	29.912013
401.058461	16329.857078	29.917031
401.495306	16352.646192	29.922048
401.803102	16367.989037	29.927066
402.155079	16380.416157	29.932084
402.328998	16393.471095	29.937101
402.520217	16420.751836	29.942119
403.005003	16453.886771	29.947136
403.237427	16469.427776	29.952154
403.922171	16492.409025	29.957172
404.235007	16524.020082	29.962189
404.493406	16551.647448	29.967207
405.091676	16574.977049	29.972224
406.036225	16590.192517	29.977242
406.388032	16605.759265	29.982260
406.569169	16631.582690	29.987277
407.176781	16648.663588	29.992295
407.802189	16666.559760	29.997312
407.658211	16696.075543	30.002330
407.837475	16715.582528	30.007348
408.485254	16746.352200	30.012365
409.129739	16760.370096	30.017383
409.289893	16786.190679	30.022400
409.178430	16811.279763	30.027418
410.241359	16830.706148	30.032436
410.542920	16861.330922	30.037453
410.279874	16887.192256	30.042471
410.831594	16915.851515	30.047488
411.212953	16939.581710	30.052506
411.726587	16975.672535	30.057524
412.325931	17010.606717	30.062541
412.591712	17035.915310	30.067559
413.544361	17053.637719	30.072576
413.953284	17088.639589	30.077594
414.249745	17105.920942	30.082612
414.485708	17138.827324	30.087629
414.748926	17164.986122	30.092647
415.193743	17191.170378	30.097664
415.698519	17212.876046	30.102682
416.348340	17239.401157	30.107700
416.957791	17264.643914	30.112717
417.232357	17278.179673	30.117735
418.265058	17291.332098	30.122752
418.234295	17320.136336	30.127770
418.819453	17336.794942	30.132788
419.125464	17347.198911	30.137805
419.712132	17361.700028	30.142823
420.108453	17374.600986	30.147840
420.574617	17396.884568	30.152858
421.099319	17416.888072	30.157876
421.418670	17433.600777	30.162893
421.861749	17448.515973	30.167911
421.862737	17457.081836	30.172928
422.012113	17488.846268	30.177946
422.765011	17497.948912	30.182964
423.189518	17520.245439	30.187981
423.396820	17541.318700	30.192999
423.857513	17555.068886	30.198016
424.043282	17572.307878	30.203034
424.501971	17603.348411	30.208052
424.416017	17628.377733	30.213069
424.938086	17666.521615	30.218087
425.554974	17696.008915	30.223104
425.436388	17726.760487	30.228122
425.880910	17754.442727	30.233140
426.025761	17798.691149	30.238157
426.384862	17826.734238	30.243175
427.053623	17862.145584	30.248192
427.583617	17894.091482	30.253210
428.177730	17932.521583	30.258228
428.387762	17965.496585	30.263245
429.009325	18002.576976	30.268263
429.580337	18032.817371	30.273280
430.110780	18063.879060	30.278298
430.447088	18103.897375	30.283316
431.057281	18131.819691	30.288333
431.563935	18170.415497	30.293351
432.343097	18190.465474	30.298368
432.417138	18221.276285	30.303386
432.594989	18250.510596	30.308404
433.301805	18282.037932	30.313421
433.498966	18308.426512	30.318439
434.256319	18327.772481	30.323456
434.572148	18369.140133	30.328474
435.586141	18391.409070	30.333492
435.974058	18419.688594	30.338509
436.543953	18438.924875	30.343527
437.575140	18451.032802	30.348544
437.904152	18478.253939	30.353562
438.203924	18494.342026	30.358580
438.598078	18513.371996	30.363597
438.844482	18540.669254	30.368615
439.454981	18551.326550	30.373632
439.593101	18582.930276	30.378650
439.892150	18597.900372	30.383668
439.971463	18619.885495	30.388685
440.544848	18648.660831	30.393703
441.103220	18677.691246	30.398720
441.112200	18708.828834	30.403738
441.902856	18737.241966	30.408756
442.054476	18771.194012	30.413773
442.206068	18809.271472	30.418791
443.744027	18819.980374	30.423808
444.045041	18851.811880	30.428826
444.421214	18878.552420	30.433844
444.726506	18901.829370	30.438861
445.241160	18925.572843	30.443879
445.395348	18945.183905	30.448896
445.874993	18979.186329	30.453914
446.381624	19011.485176	30.458932
446.753876	19043.508070	30.463949
447.301725	19061.061599	30.468967
447.917008	19087.695709	30.473984
448.104293	19125.085927	30.479002
448.355460	19143.740765	30.484020
449.265071	19185.352552	30.489037
449.578494	19214.232374	30.494055
449.818585	19241.120952	30.499072
450.166801	19276.673234	30.504090
450.842875	19299.772902	30.509108
451.318841	19330.238604	30.514125
451.356749	19351.289662	30.519143
451.901258	19372.982096	30.524160
452.194662	19413.205638	30.529178
453.014912	19430.293807	30.534196
453.350201	19461.937761	30.539213
453.013546	19492.884019	30.544231
453.605133	19523.464697	30.549248
454.089985	19561.662327	30.554266
454.231512	19602.326877	30.559284
454.569190	19650.403352	30.564301
454.978464	19679.319484	30.569319
455.794640	19717.219443	30.574336
456.597266	19766.588474	30.579354
456.780584	19798.433533	30.584372
457.409552	19832.679551	30.589389
457.985127	19859.965323	30.594407
458.661841	19891.266199	30.599424
458.996234	19936.077543	30.604442
459.707382	19956.999173	30.609460
460.529886	19978.857496	30.614477
460.728235	20015.780173	30.619495
461.076848	20041.585230	30.624512
461.897464	20070.014603	30.629530
462.076759	20097.280266	30.634548
462.938673	20128.167296	30.639565
463.204737	20149.417460	30.644583
463.840757	20181.811829	30.649600
464.086751	20215.568477	30.654618
464.453978	20247.215050	30.659636
465.043215	20275.927146	30.664653
465.277786	20303.614117	30.669671
465.625625	20334.840543	30.674688
465.926682	20370.086258	30.679706
466.334628	20396.994523	30.684724
467.063066	20429.665546	30.689741
467.656006	20477.337869	30.694759
468.220893	20500.999627	30.699776
468.469330	20526.239655	30.704794
469.463602	20565.396110	30.709812
469.755881	20596.359925	30.714829
470.160961	20624.090303	30.719847
470.667434	20644.627540	30.724864
471.397624	20680.040777	30.729882
472.049733	20707.732817	30.734900
472.675091	20732.592208	30.739917
472.556031	20761.882827	30.744935
472.760984	20783.484374	30.749952
473.948093	20813.418365	30.754970
474.384806	20841.099899	30.759988
475.397795	20866.878434	30.765005
475.688410	20868.412779	30.770023
476.580280	20881.504291	30.775040
477.368772	20904.904272	30.780058
477.459630	20920.546704	30.785076
477.912964	20933.213699	30.790093
478.614368	20949.127562	30.795111
478.464708	20969.558784	30.800128
478.771519	20996.123478	30.805146
479.256156	21020.746095	30.810164
479.698977	21037.306837	30.815181
480.021135	21077.958969	30.820199
480.083410	21095.924795	30.825216
480.421475	21124.260232	30.830234
481.233181	21162.966116	30.835252
481.724235	21188.264001	30.840269
482.276679	21219.542124	30.845287
482.537899	21249.892611	30.850304
483.180466	21281.750725	30.855322
483.540293	21315.207220	30.860340
484.023670	21329.304059	30.865357
484.206341	21349.860853	30.870375
484.944751	21384.579066	30.875392
485.251233	21418.037722	30.880410
485.422188	21449.817887	30.885428
485.758671	21478.337314	30.890445
486.354876	21513.387494	30.895463
486.719792	21546.104335	30.900480
487.348674	21581.794029	30.905498
487.485822	21618.204820	30.910516
488.603623	21657.104127	30.915533
488.411558	21696.769771	30.920551
489.169796	21721.217985	30.925568
489.860835	21762.445952	30.930586
490.099345	21798.601194	30.935604
490.972425	21834.626122	30.940621
491.536865	21876.461657	30.945639
491.673020	21908.007875	30.950656
492.300728	21943.938512	30.955674
492.783933	21981.136467	30.960692
493.601019	22013.903745	30.965709
494.056619	22048.041618	30.970727
494.382672	22078.383289	30.975744
494.987949	22119.770682	30.980762
495.540944	22148.099408	30.985780
496.427422	22186.087982	30.990797
496.811229	22214.272538	30.995815
497.166751	22244.180210	31.000832
497.916104	22274.898589	31.005850
498.004672	22313.997336	31.010868
498.745838	22340.098148	31.015885
499.172224	22380.837841	31.020903
499.650389	22418.296470	31.025920
500.498710	22437.720824	31.030938
500.680585	22471.472369	31.035956
501.606031	22504.425794	31.040973
502.190621	22536.452932	31.045991
502.372667	22564.081755	31.051008
503.010992	22590.205228	31.056026
503.212431	22623.189418	31.061044
504.118992	22657.510891	31.066061
504.220048	22686.852244	31.071079
505.046729	22724.743745	31.076096
505.424874	22756.575902	31.081114
505.928255	22789.058409	31.086132
506.506552	22816.986070	31.091149
506.884271	22842.177347	31.096167
507.310298	22887.101206	31.101184
508.105540	22917.402717	31.106202
508.221917	22951.247422	31.111220
509.083099	22982.309669	31.116237
509.640614	23019.251574	31.121255
509.942999	23055.203284	31.126272
510.517450	23086.777931	31.131290
510.387264	23126.708518	31.136308
510.874147	23151.289215	31.141325
511.621600	23196.846181	31.146343
511.894735	23239.450311	31.151360
512.650869	23264.652723	31.156378
512.987179	23308.403537	31.161396
513.928379	23350.467893	31.166413
514.146051	23387.223267	31.171431
514.861162	23424.849121	31.176448
515.656573	23460.661622	31.181466
515.638638	23500.006771	31.186484
516.023897	23530.726911	31.191501
516.855275	23577.541816	31.196519
517.210939	23609.600009	31.201536
517.938144	23640.848443	31.206554
518.383246	23681.101323	31.211572
519.273025	23694.706890	31.216589
519.802796	23719.913525	31.221607
520.077544	23748.174114	31.226624
520.752522	23766.040662	31.231642
521.092853	23801.994135	31.236660
522.010138	23830.255919	31.241677
522.738822	23850.654480	31.246695
523.157703	23876.301960	31.251712
524.192831	23899.471211	31.256730
524.457841	23912.719210	31.261748
524.710489	23939.978764	31.266765
525.397948	23968.061671	31.271783
525.654301	23996.268603	31.276800
526.545921	24018.259686	31.281818
526.561140	24048.298886	31.286836
527.114249	24074.873609	31.291853
527.357658	24110.760578	31.296871
527.790783	24145.012988	31.301888
528.203620	24178.699883	31.306906
528.836281	24226.185496	31.311924
529.413160	24256.876927	31.316941
529.620165	24289.932528	31.321959
530.126195	24335.251639	31.326976
530.682523	24368.265627	31.331994
531.405864	24412.059723	31.337012
531.791645	24460.658614	31.342029
532.522134	24496.167120	31.347047
532.743449	24547.755605	31.352064
533.578332	24575.923848	31.357082
533.942229	24617.297153	31.362100
534.330928	24665.643312	31.367117
535.100652	24709.064313	31.372135
535.525567	24739.628478	31.377152
536.325032	24784.011886	31.382170
536.442105	24827.433634	31.387188
537.012556	24872.529073	31.392205
538.162837	24906.209823	31.397223
538.623125	24956.909029	31.402240
539.224516	24998.214552	31.407258
540.038890	25027.170246	31.412276
540.311077	25057.398459	31.417293
541.201169	25100.586708	31.422311
541.415425	25134.811692	31.427328
541.941134	25168.482683	31.432346
542.361616	25217.160162	31.437364
542.905804	25243.453448	31.442381
543.590261	25277.889860	31.447399
544.239058	25325.356612	31.452416
544.886765	25359.362831	31.457434
545.228865	25399.584652	31.462452
545.903335	25431.292797	31.467469
546.528938	25467.084781	31.472487
546.670545	25513.746183	31.477504
547.320304	25546.880285	31.482522
547.770216	25583.445551	31.487540
548.212586	25629.738096	31.492557
548.742418	25658.201823	31.497575
549.296338	25712.218856	31.502592
549.746931	25749.359414	31.507610
550.236437	25793.117097	31.512628
550.758676	25829.064853	31.517645
551.588960	25877.522142	31.522663
551.772156	25913.883058	31.527680
552.793160	25960.901541	31.532698
553.075130	25998.391120	31.537716
553.439623	26035.008424	31.542733
554.381723	26073.324394	31.547751
554.588915	26104.562837	31.552768
555.543784	26142.213365	31.557786
556.065049	26184.639781	31.562804
556.756186	26208.168623	31.567821
557.215889	26244.272214	31.572839
557.627613	26281.388205	31.577856
558.267034	26316.414841	31.582874
558.860508	26344.534676	31.587892
559.405380	26383.703068	31.592909
560.181866	26424.952668	31.597927
560.212078	26464.454135	31.602944
561.020364	26495.264650	31.607962
561.333045	26546.161481	31.612980
561.835689	26589.425888	31.617997
562.589690	26614.797184	31.623015
562.717683	26670.924460	31.628032
563.254945	26709.475305	31.633050
564.103600	26754.095572	31.638068
564.660394	26797.528957	31.643085
565.231098	26842.723575	31.648103
565.815020	26892.991285	31.653120
566.322724	26932.804860	31.658138
567.028474	26976.695770	31.663156
567.608452	27019.860578	31.668173
568.669788	27057.976574	31.673191
569.292494	27101.646838	31.678208
569.696394	27134.960870	31.683226
570.410748	27175.602298	31.688244
570.840934	27217.008549	31.693261
571.413972	27253.285906	31.698279
571.738917	27301.768403	31.703296
572.515158	27330.752314	31.708314
572.976586	27376.989017	31.713332
573.845686	27410.389090	31.718349
574.490821	27439.456769	31.723367
574.725174	27493.585198	31.728384
575.485303	27529.954011	31.733402
575.717404	27573.584974	31.738420
576.505667	27613.925041	31.743437
577.187162	27658.175143	31.748455
577.731116	27702.073852	31.753472
578.342269	27729.257449	31.758490
579.435862	27776.717609	31.763508
580.051015	27815.416444	31.768525
580.434897	27839.513293	31.773543
580.981307	27885.807451	31.778560
581.361140	27932.367822	31.783578
582.253834	27958.098440	31.788596
582.957017	27992.669302	31.793613
583.308438	28031.327439	31.798631
583.791868	28080.558219	31.803648
584.292678	28113.252006	31.808666
585.055727	28156.934296	31.813684
585.190429	28197.750175	31.818701
585.868002	28234.474410	31.823719
586.408552	28280.302659	31.828736
587.214577	28321.007957	31.833754
587.544859	28369.593298	31.838772
587.645480	28400.548483	31.843789
588.207243	28450.905668	31.848807
588.889228	28505.624445	31.853824
589.355040	28557.109257	31.858842
590.336375	28601.346337	31.863860
590.537257	28656.867289	31.868877
591.468032	28701.915182	31.873895
592.145752	28752.109684	31.878912
592.825681	28780.314252	31.883930
593.885016	28817.789158	31.888948
594.089977	28860.655975	31.893965
595.200460	28881.809262	31.898983
595.627266	28921.519233	31.904000
596.204207	28950.359502	31.909018
596.640172	28983.760061	31.914036
597.205107	29017.108995	31.919053
597.634651	29058.854094	31.924071
598.239586	29097.531672	31.929088
598.341561	29142.728524	31.934106
599.004502	29178.799374	31.939124
599.372439	29235.509487	31.944141
599.884750	29278.727546	31.949159
600.264298	29327.010414	31.954176
601.064981	29383.666211	31.959194
601.968809	29434.478240	31.964212
602.413957	29479.552881	31.969229
603.136909	29522.327804	31.974247
603.864797	29576.890600	31.979264
604.096909	29620.576503	31.984282
604.832794	29682.091386	31.989300
605.591174	29725.847291	31.994317
606.568382	29766.933366	31.999335
607.068840	29819.319862	32.004352
607.817197	29868.134444	32.009370
608.979855	29903.224870	32.014388
609.300140	29948.945763	32.019405
609.998526	29987.098467	32.024423
610.706532	30031.526578	32.029440
611.332510	30067.648995	32.034458
611.680416	30103.157369	32.039476
612.304253	30154.716412	32.044493
612.522843	30195.453679	32.049511
613.194805	30249.603454	32.054528
613.705587	30300.030012	32.059546
614.937651	30348.814684	32.064564
615.198224	30399.065515	32.069581
616.100913	30437.073469	32.074599
616.429133	30477.667804	32.079616
616.775673	30524.289821	32.084634
617.678210	30565.186839	32.089652
618.176797	30622.449351	32.094669
618.421433	30672.855040	32.099687
619.396707	30723.090221	32.104704
620.266080	30753.802854	32.109722
621.266588	30801.398314	32.114740
621.358261	30855.222808	32.119757
622.353418	30892.306936	32.124775
622.916848	30940.615536	32.129792
623.316928	30987.167050	32.134810
624.138202	31040.575022	32.139828
624.881806	31086.384251	32.144845
625.819964	31123.654668	32.149863
626.060883	31163.505371	32.154880
626.683664	31215.990161	32.159898
627.711904	31256.002944	32.164916
628.019584	31295.053325	32.169933
628.658000	31338.793405	32.174951
629.240503	31390.804476	32.179968
629.644206	31427.779351	32.184986
629.957183	31475.540289	32.190004
630.684732	31528.635393	32.195021
630.949857	31577.548213	32.200039
631.711609	31621.636340	32.205056
632.136323	31675.992705	32.210074
633.291982	31736.961609	32.215092
633.800631	31784.047993	32.220109
634.450342	31825.821319	32.225127
635.412898	31863.278921	32.230144
635.736801	31888.350751	32.235162
636.604331	31937.695340	32.240180
636.942377	31982.513968	32.245197
637.611657	32026.339198	32.250215
638.564208	32073.761724	32.255232
639.016293	32120.579521	32.260250
639.795465	32152.408256	32.265268
640.181065	32196.688918	32.270285
640.403144	32242.739935	32.275303
641.527171	32297.602274	32.280320
642.014084	32344.680668	32.285338
642.295856	32386.923318	32.290356
643.166888	32441.117378	32.295373
644.039028	32493.534972	32.300391
644.662218	32540.175354	32.305408
644.936393	32588.829948	32.310426
646.041083	32638.891584	32.315444
646.426731	32696.613615	32.320461
646.843555	32746.447530	32.325479
647.604167	32797.878069	32.330496
647.872821	32859.728014	32.335514
648.762149	32912.763538	32.340532
649.291564	32967.296635	32.345549
650.045577	33017.578143	32.350567
650.595002	33085.062196	32.355584
651.319078	33141.620099	32.360602
652.230780	33193.900532	32.365620
652.488064	33264.566376	32.370637
653.570325	33312.186482	32.375655
654.461973	33362.997416	32.380672
654.694621	33419.253245	32.385690
655.818511	33472.847956	32.390708
656.384162	33538.794669	32.395725
657.068584	33584.213997	32.400743
658.036983	33636.594189	32.405760
658.630979	33693.041067	32.410778
659.062912	33732.658316	32.415796
659.919764	33783.633744	32.420813
660.511148	33835.453546	32.425831
661.446856	33880.341265	32.430848
662.499607	33928.972607	32.435866
663.504842	33963.063898	32.440884
663.719079	34010.491962	32.445901
664.837123	34054.656218	32.450919
665.316696	34089.518676	32.455936
665.568289	34144.799865	32.460954
666.684680	34185.000553	32.465972
667.264690	34228.730500	32.470989
667.842290	34277.069921	32.476007
668.309467	34321.513086	32.481024
668.756144	34371.788788	32.486042
669.654923	34413.844641	32.491060
669.862815	34463.468590	32.496077
670.771797	34511.933992	32.501095
671.165570	34559.518696	32.506112
671.975820	34618.027127	32.511130
672.969688	34663.160366	32.516148
673.506405	34713.524026	32.521165
673.939414	34765.212712	32.526183
674.799176	34815.652779	32.531200
675.152170	34869.750416	32.536218
675.964197	34920.451066	32.541236
676.522889	34975.136564	32.546253
677.195434	35032.877262	32.551271
677.765835	35083.451530	32.556288
678.320021	35133.434117	32.561306
679.147823	35181.136013	32.566324
679.608062	35225.575842	32.571341
679.958664	35282.545394	32.576359
681.025169	35328.111336	32.581376
681.262232	35387.836569	32.586394
681.980164	35437.193727	32.591412
682.985564	35494.112498	32.596429
683.651990	35544.407366	32.601447
684.815244	35588.681615	32.606464
685.590969	35627.142426	32.611482
686.679854	35666.831760	32.616500
687.537395	35704.887963	32.621517
688.304131	35751.266543	32.626535
689.206889	35782.550441	32.631552
689.507110	35823.646373	32.636570
690.026761	35861.053623	32.641588
690.731211	35909.775375	32.646605
691.501843	35946.030882	32.651623
692.160792	35990.536227	32.656640
692.351023	36045.509474	32.661658
693.520383	36090.118936	32.666676
693.982516	36127.839110	32.671693
694.495982	36180.644209	32.676711
695.216666	36237.040235	32.681728
695.896292	36290.407776	32.686746
696.178011	36347.511048	32.691764
696.910316	36398.480571	32.696781
697.389314	36457.393421	32.701799
698.305250	36515.169824	32.706816
698.740280	36579.881762	32.711834
699.235110	36643.389526	32.716852
699.981975	36707.515846	32.721869
700.609075	36771.382787	32.726887
701.493858	36828.867704	32.731904
702.563581	36906.848935	32.736922
702.480826	36957.010847	32.741940
703.270005	37024.906468	32.746957
703.870317	37095.183939	32.751975
705.360500	37155.066838	32.756992
705.900770	37232.189516	32.762010
706.653459	37294.375457	32.767028
707.362107	37350.485433	32.772045
708.209936	37422.742578	32.777063
709.202941	37472.561184	32.782080
710.122826	37533.925055	32.787098
711.040341	37589.098906	32.792116
711.590426	37639.119639	32.797133
712.269511	37693.047230	32.802151
713.316248	37750.844558	32.807168
713.583708	37806.708240	32.812186
714.260111	37859.580657	32.817204
714.861526	37920.002432	32.822221
715.436040	37982.749279	32.827239
716.185115	38041.731954	32.832256
716.834616	38100.806173	32.837274
717.491206	38153.214458	32.842292
718.420514	38222.628681	32.847309
718.861857	38283.607575	32.852327
719.948245	38336.828377	32.857344
720.806716	38401.859321	32.862362
721.289559	38457.931465	32.867380
721.922577	38514.612739	32.872397
722.495519	38580.548685	32.877415
723.486804	38644.257016	32.882432
724.081366	38695.923764	32.887450
725.000745	38747.078443	32.892468
725.730262	38803.637953	32.897485
726.402081	38869.413946	32.902503
727.256948	38914.685349	32.907520
728.164904	38964.906409	32.912538
728.766058	39016.288330	32.917556
729.041619	39061.789345	32.922573
729.805959	39119.096793	32.927591
730.825549	39159.524330	32.932608
731.504512	39212.336436	32.937626
732.059117	39268.026409	32.942644
733.007909	39320.929578	32.947661
733.395740	39390.109338	32.952679
734.130359	39441.035146	32.957696
734.752053	39503.292137	32.962714
735.321107	39569.149498	32.967732
735.899459	39621.990915	32.972749
736.239781	39698.242909	32.977767
737.167955	39767.327111	32.982784
738.127512	39832.005135	32.987802
738.916531	39891.517870	32.992820
740.079335	39957.328251	32.997837
740.229586	40027.369154	33.002855
741.339384	40080.571645	33.007872
742.118298	40148.307970	33.012890
742.341581	40219.672511	33.017908
743.756876	40286.848543	33.022925
744.277863	40344.203442	33.027943
745.429376	40409.922091	33.032960
746.302662	40470.662837	33.037978
746.698581	40529.302533	33.042996
747.751547	40602.278333	33.048013
748.134770	40668.724490	33.053031
749.363114	40721.783614	33.058048
750.327791	40783.428026	33.063066
751.074390	40848.717740	33.068084
752.001073	40891.540915	33.073101
752.733490	40961.177982	33.078119
753.684125	41002.884563	33.083136
754.592805	41066.290339	33.088154
755.392180	41119.606942	33.093172
756.159176	41168.172765	33.098189
757.080310	41217.423038	33.103207
758.197499	41250.465017	33.108224
759.217260	41302.014868	33.113242
759.938605	41351.802499	33.118260
760.709141	41391.608903	33.123277
761.137349	41438.514137	33.128295
761.992650	41472.722979	33.133312
762.668526	41519.064900	33.138330
763.082326	41578.058803	33.143348
763.638017	41624.046509	33.148365
764.112358	41688.982673	33.153383
764.563779	41738.395783	33.158400
765.545102	41798.661717	33.163418
766.149887	41867.486697	33.168436
767.033390	41924.295998	33.173453
767.770216	41980.944865	33.178471
768.576562	42052.616758	33.183488
769.300980	42111.778783	33.188506
769.846947	42166.952569	33.193524
770.597910	42234.402461	33.198541
771.265198	42312.573352	33.203559
771.953869	42372.873772	33.208576
772.993387	42431.405730	33.213594
773.687056	42492.452023	33.218612
774.150260	42546.241867	33.223629
774.519512	42628.299427	33.228647
775.794874	42691.520008	33.233664
776.478714	42763.662354	33.238682
777.182182	42836.035901	33.243700
777.866321	42890.424682	33.248717
778.724556	42962.692329	33.253735
779.743977	43006.991564	33.258752
780.615682	43062.205437	33.263770
781.449069	43121.536638	33.268788
782.411129	43168.577512	33.273805
782.945099	43236.665126	33.278823
783.898060	43283.037211	33.283840
784.900722	43336.447732	33.288858
785.313997	43413.333814	33.293876
786.283925	43457.553109	33.298893
787.117246	43522.217423	33.303911
787.126480	43590.058905	33.308928
788.144784	43649.988926	33.313946
788.467944	43719.141835	33.318964
789.284988	43779.900503	33.323981
790.064081	43853.480040	33.328999
790.894892	43933.497143	33.334016
791.981714	44013.082519	33.339034
792.074447	44085.599504	33.344052
793.525369	44155.020983	33.349069
794.670566	44229.904710	33.354087
795.287005	44296.217990	33.359104
795.888871	44362.495784	33.364122
796.567374	44443.746571	33.369140
797.355452	44510.577751	33.374157
798.416879	44587.809782	33.379175
799.198978	44661.891234	33.384192
800.328675	44724.925243	33.389210
801.326750	44796.272569	33.394228
802.298977	44854.087667	33.399245
802.785109	44924.401815	33.404263
804.244119	44988.973004	33.409280
805.034396	45047.607615	33.414298
805.636621	45123.534025	33.419316
806.364486	45177.383939	33.424333
807.248109	45231.760062	33.429351
808.301209	45293.567793	33.434368
809.415003	45346.453482	33.439386
810.054944	45410.501857	33.444404
811.128480	45461.085236	33.449421
811.858616	45517.301402	33.454439
812.655380	45581.483996	33.459456
813.501131	45642.129420	33.464474
813.836579	45711.697770	33.469492
814.837266	45767.663701	33.474509
815.356939	45831.485300	33.479527
816.292501	45901.397297	33.484544
817.017801	45967.755530	33.489562
817.775455	46028.219614	33.494580
818.307555	46085.233453	33.499597
818.964355	46177.007410	33.504615
819.743701	46246.040205	33.509632
820.613154	46317.722376	33.514650
821.183152	46404.551293	33.519668
821.817777	46479.313289	33.524685
822.920674	46548.574987	33.529703
823.211763	46626.199662	33.534720
824.497499	46695.091748	33.539738
825.554010	46777.316972	33.544756
826.289485	46841.000302	33.549773
827.113344	46921.086117	33.554791
827.934389	47003.374124	33.559808
829.369685	47069.403673	33.564826
829.704746	47140.235389	33.569844
831.070672	47207.237708	33.574861
831.896240	47276.222183	33.579879
832.657648	47343.894689	33.584896
833.447513	47400.163202	33.589914
834.102219	47462.323598	33.594932
835.218616	47521.900792	33.599949
836.131425	47570.122636	33.604967
836.803230	47632.445320	33.609984
837.614209	47688.160881	33.615002
838.098994	47749.342643	33.620020
838.978578	47807.375885	33.625037
839.761768	47878.336268	33.630055
840.232689	47944.075653	33.635072
840.857586	48018.679773	33.640090
841.662693	48090.896352	33.645108
842.658798	48168.777176	33.650125
843.367866	48228.742283	33.655143
844.111804	48320.289956	33.660160
845.241001	48382.720642	33.665178
846.170480	48465.958704	33.670196
847.013849	48529.528765	33.675213
847.988629	48606.756455	33.680231
848.569738	48692.143647	33.685248
849.680971	48754.495905	33.690266
850.411783	48841.435664	33.695284
851.165727	48921.185140	33.700301
852.131628	48996.036732	33.705319
852.914558	49077.503081	33.710336
853.830322	49146.605732	33.715354
854.925675	49238.203616	33.720372
855.566757	49315.745046	33.725389
856.440314	49400.595881	33.730407
857.443548	49478.973558	33.735424
858.572049	49552.403451	33.740442
859.084978	49639.842018	33.745460
860.070537	49708.948157	33.750477
860.672259	49784.959887	33.755495
861.631997	49870.520307	33.760512
862.788585	49945.357976	33.765530
863.557192	50034.953676	33.770548
864.463799	50112.171757	33.775565
865.873689	50182.345790	33.780583
866.349365	50262.326735	33.785600
867.391077	50338.993083	33.790618
867.930622	50414.896364	33.795636
868.471451	50487.376773	33.800653
869.575488	50580.674312	33.805671
870.437999	50665.423982	33.810688
871.330098	50738.666695	33.815706
872.323599	50818.638562	33.820724
872.732873	50900.504886	33.825741
873.806835	50991.315875	33.830759
874.745873	51083.635114	33.835776
875.537932	51166.360236	33.840794
876.653710	51250.857507	33.845812
877.271256	51327.536224	33.850829
878.086044	51412.485883	33.855847
879.070319	51503.255900	33.860864
879.887684	51582.637754	33.865882
881.113780	51652.655055	33.870900
882.239994	51747.263615	33.875917
883.209532	51816.454499	33.880935
884.223318	51898.926265	33.885952
885.157461	51965.073289	33.890970
886.049424	52040.876429	33.895988
887.231437	52118.842955	33.901005
888.112426	52177.538770	33.906023
888.733145	52260.402035	33.911040
889.739421	52331.759073	33.916058
890.496871	52403.104442	33.921076
891.015842	52472.202900	33.926093
891.846713	52539.278805	33.931111
892.801623	52603.045240	33.936128
893.792483	52671.355814	33.941146
894.612052	52748.608900	33.946164
895.391208	52816.946528	33.951181
896.505957	52876.689749	33.956199
897.210107	52957.644203	33.961216
897.895138	53026.598227	33.966234
898.705676	53098.760065	33.971252
899.333432	53183.941469	33.976269
900.406907	53255.423757	33.981287
901.368163	53328.916989	33.986304
901.861288	53420.568240	33.991322
902.967660	53498.000633	33.996340
903.727445	53589.693298	34.001357
905.009035	53657.252778	34.006375
905.567277	53746.661423	34.011392
906.480798	53831.509613	34.016410
907.268477	53920.693367	34.021428
908.390759	54007.167622	34.026445
909.693574	54086.450791	34.031463
910.579061	54169.431476	34.036480
911.542266	54258.886608	34.041498
912.260776	54333.996460	34.046516
913.278599	54422.026223	34.051533
914.676564	54493.594663	34.056551
915.882195	54583.095556	34.061568
916.913597	54646.153224	34.066586
918.653523	54706.822629	34.071604
919.299881	54777.698925	34.076621
920.425213	54834.597805	34.081639
921.132815	54906.255979	34.086656
922.144276	54962.869139	34.091674
922.971500	55036.230368	34.096692
923.781338	55110.442521	34.101709
924.575362	55179.784579	34.106727
925.265000	55247.459757	34.111744
926.033838	55325.526582	34.116762
926.742951	55414.392813	34.121780
927.706412	55483.747356	34.126797
928.804168	55557.675615	34.131815
929.437006	55644.067520	34.136832
930.358565	55731.971593	34.141850
931.415913	55809.438198	34.146868
932.222238	55895.905269	34.151885
933.417151	55965.839057	34.156903
934.513141	56057.969942	34.161920
935.336593	56122.665034	34.166938
936.530465	56195.150065	34.171956
937.052962	56282.371521	34.176973
938.305769	56359.847467	34.181991
939.031072	56440.051145	34.187008
940.162771	56525.685106	34.192026
940.728417	56599.648805	34.197044
941.473186	56689.045857	34.202061
942.793931	56763.424135	34.207079
943.603685	56852.153495	34.212096
944.090037	56933.104844	34.217114
945.333056	57016.077812	34.222132
946.212833	57107.385692	34.227149
947.376483	57191.915855	34.232167
948.026477	57275.482011	34.237184
948.654875	57373.038640	34.242202
949.587697	57449.776821	34.247220
950.684726	57557.203954	34.252237
951.749379	57635.327229	34.257255
952.771899	57732.007533	34.262272
953.447219	57814.786831	34.267290
954.410582	57884.616715	34.272308
955.164458	57967.080518	34.277325
956.069109	58053.837550	34.282343
956.668936	58148.882809	34.287360
957.695207	58226.520312	34.292378
958.938596	58315.807834	34.297396
959.415713	58411.018797	34.302413
960.387753	58494.912479	34.307431
961.164739	58592.204081	34.312448
961.885631	58685.707272	34.317466
963.110047	58782.069216	34.322484
964.030276	58879.846018	34.327501
965.393834	58972.016069	34.332519
966.651381	59061.443388	34.337536
967.586669	59146.319768	34.342554
969.539864	59224.278235	34.347572
970.704929	59310.568848	34.352589
971.985525	59381.461324	34.357607
973.009214	59467.008642	34.362624
973.544683	59537.093464	34.367642
974.862244	59612.278556	34.372660
975.620740	59692.544869	34.377677
976.499819	59768.355692	34.382695
977.525473	59859.904461	34.387712
978.031404	59944.844136	34.392730
979.176844	60020.228180	34.397748
979.937428	60114.825714	34.402765
981.044573	60202.812183	34.407783
981.971127	60288.548410	34.412800
982.533828	60381.551062	34.417818
984.084252	60456.405021	34.422836
984.528756	60554.256278	34.427853
985.795278	60636.731645	34.432871
986.936235	60734.063780	34.437888
987.861732	60836.151858	34.442906
989.035371	60920.990991	34.447924
989.761014	61018.104062	34.452941
990.819963	61104.645419	34.457959
991.984868	61197.538442	34.462976
992.543954	61292.247851	34.467994
993.931662	61393.247186	34.473012
994.993037	61480.998508	34.478029
995.689486	61577.687899	34.483047
996.942005	61669.417013	34.488064
997.513663	61763.075499	34.493082
998.830708	61844.787462	34.498100
1000.183376	61942.920670	34.503117
1001.048186	62032.894760	34.508135
1002.439876	62117.033092	34.513152
1002.932185	62208.306507	34.518170
1004.179501	62295.500056	34.523188
1005.349483	62387.858718	34.528205
1006.305522	62478.459579	34.533223
1007.795889	62564.685706	34.538240
1008.295788	62663.150755	34.543258
1009.300212	62735.640514	34.548276
1010.001247	62829.713361	34.553293
1011.226699	62915.184328	34.558311
1012.410185	63003.396828	34.563328
1012.999388	63100.305109	34.568346
1013.872403	63186.452246	34.573364
1015.210643	63281.434149	34.578381
1016.138990	63375.530653	34.583399
1017.210158	63467.155396	34.588416
1017.920084	63558.975977	34.593434
1019.219437	63643.273138	34.598452
1019.988517	63749.575733	34.603469
1020.572105	63831.123546	34.608487
1022.383641	63909.036656	34.613504
1023.732403	63989.111138	34.618522
1025.206163	64057.264880	34.623540
1026.374866	64127.093263	34.628557
1027.086697	64194.549330	34.633575
1028.326096	64262.233661	34.638592
1029.050822	64335.284402	34.643610
1029.908827	64412.068713	34.648628
1030.992165	64493.262346	34.653645
1031.380109	64568.683233	34.658663
1032.499686	64650.897316	34.663680
1033.605644	64740.596766	34.668698
1034.539335	64821.181678	34.673716
1035.393107	64910.351219	34.678733
1036.281357	65005.346416	34.683751
1037.059239	65099.346214	34.688768
1038.169720	65192.085390	34.693786
1039.053629	65292.780151	34.698804
1040.365873	65391.984180	34.703821
1040.941037	65490.511961	34.708839
1042.224702	65589.746541	34.713856
1042.833438	65695.056718	34.718874
1044.139913	65800.695567	34.723892
1045.346230	65902.108632	34.728909
1046.064401	66009.460682	34.733927
1047.632330	66112.236468	34.738944
1048.451169	66229.279393	34.743962
1049.721289	66320.465727	34.748980
1050.517945	66428.174543	34.753997
1051.665083	66537.583011	34.759015
1052.755258	66635.009422	34.764032
1053.621063	66743.259630	34.769050
1054.795732	66850.936723	34.774068
1055.977624	66952.345129	34.779085
1056.988731	67067.855133	34.784103
1058.346190	67171.434066	34.789120
1059.262488	67273.733499	34.794138
1060.177729	67378.585077	34.799156
1061.394538	67481.573014	34.804173
1062.307089	67599.133164	34.809191
1063.840535	67693.784748	34.814208
1064.903735	67803.186392	34.819226
1065.776144	67901.354342	34.824244
1067.472665	68006.871999	34.829261
1068.345673	68109.884324	34.834279
1069.943456	68200.171616	34.839296
1070.900421	68301.626723	34.844314
1071.803158	68392.060870	34.849332
1072.895474	68491.032630	34.854349
1073.659203	68593.880287	34.859367
1075.340236	68682.807660	34.864384
1076.467976	68782.750121	34.869402
1077.747254	68865.890096	34.874420
1078.810268	68963.361266	34.879437
1079.810515	69061.298468	34.884455
1081.030317	69138.357340	34.889472
1081.816421	69234.777225	34.894490
1082.994388	69328.907639	34.899508
1084.574608	69424.482785	34.904525
1085.130372	69513.524862	34.909543
1086.246712	69611.458744	34.914560
1087.390412	69697.237613	34.919578
1088.462682	69781.894451	34.924596
1089.501495	69875.877551	34.929613
1090.461642	69971.601893	34.934631
1091.526079	70061.212546	34.939648
1092.562010	70167.443428	34.944666
1093.371371	70258.284903	34.949684
1094.540975	70350.805636	34.954701
1095.413215	70435.837681	34.959719
1096.818241	70517.918582	34.964736
1097.460753	70610.642595	34.969754
1098.355471	70692.442542	34.974772
1099.421162	70802.850670	34.979789
1100.649479	70893.223882	34.984807
1101.653873	70986.545129	34.989824
1102.519885	71095.706448	34.994842
1104.056863	71174.064454	34.999860
1105.230291	71269.386758	35.004877
1106.204953	71365.905512	35.009895
1107.208500	71462.698753	35.014912
1108.262313	71561.713553	35.019930
1109.186240	71667.309398	35.024948
1110.627782	71762.541103	35.029965
1111.702238	71862.440377	35.034983
1113.564971	71951.477317	35.040000
1114.470833	72043.817125	35.045018
1115.802696	72142.676850	35.050036
1117.066486	72227.235818	35.055053
1117.976381	72318.423426	35.060071
1119.347396	72406.094604	35.065088
1120.412390	72499.652443	35.070106
1121.593343	72600.766483	35.075124
1122.744381	72689.068118	35.080141
1123.887842	72789.530114	35.085159
1124.980238	72884.224947	35.090176
1125.699348	72987.755485	35.095194
1126.663690	73089.221751	35.100212
1127.704678	73191.753060	35.105229
1128.616117	73303.601593	35.110247
1129.851163	73405.837544	35.115264
1130.741234	73511.002734	35.120282
1132.072643	73623.471200	35.125300
1133.394070	73721.097195	35.130317
1134.165279	73837.010240	35.135335
1135.296222	73941.582336	35.140352
1136.543698	74052.583752	35.145370
1137.842877	74160.373044	35.150388
1139.164108	74260.192293	35.155405
1140.260178	74377.387073	35.160423
1141.548602	74483.950719	35.165440
1142.825282	74588.224006	35.170458
1143.758467	74696.718416	35.175476
1144.873604	74805.070946	35.180493
1145.950504	74912.517877	35.185511
1147.593926	75023.347697	35.190528
1148.709255	75125.773539	35.195546
1150.071703	75234.469308	35.200564
1151.024123	75342.836672	35.205581
1151.974626	75449.887426	35.210599
1153.452643	75546.355703	35.215616
1154.757603	75646.689323	35.220634
1155.724647	75749.077288	35.225652
1157.173142	75851.758042	35.230669
1158.235949	75953.992542	35.235687
1159.317620	76057.643203	35.240704
1160.449200	76160.387128	35.245722
1161.285325	76265.381518	35.250740
1162.937703	76365.448392	35.255757
1163.692749	76471.798926	35.260775
1165.086948	76583.003304	35.265792
1166.187878	76685.196631	35.270810
1167.173910	76784.988755	35.275828
1168.010447	76885.779908	35.280845
1169.431422	76998.109222	35.285863
1170.624065	77095.818194	35.290880
1171.535484	77190.505735	35.295898
1172.390022	77281.136151	35.300916
1173.537495	77385.795054	35.305933
1174.370459	77489.920599	35.310951
1175.584291	77592.619138	35.315968
1176.660854	77697.226935	35.320986
1177.892978	77816.264960	35.326004
1179.320776	77918.538716	35.331021
1180.051444	78032.069180	35.336039
1180.916437	78147.023362	35.341056
1182.319507	78260.526119	35.346074
1183.072956	78372.382260	35.351092
1184.350599	78489.921287	35.356109
1185.795947	78624.283476	35.361127
1187.173700	78739.895085	35.366144
1188.519072	78857.070427	35.371162
1189.559123	78979.804551	35.376180
1190.867307	79098.709614	35.381197
1191.818381	79217.506084	35.386215
1192.947068	79335.895361	35.391232
1194.363580	79454.949788	35.396250
1195.452125	79580.111408	35.401268
1196.996225	79696.486592	35.406285
1198.263431	79827.778529	35.411303
1199.473163	79940.710197	35.416320
1200.864601	80065.282101	35.421338
1202.061473	80175.581593	35.426356
1203.537712	80289.727425	35.431373
1205.012781	80409.676337	35.436391
1206.607334	80518.635715	35.441408
1207.879582	80632.662676	35.446426
1208.834044	80740.987745	35.451444
1210.534477	80840.404654	35.456461
1211.093291	80959.396326	35.461479
1212.464947	81064.351021	35.466496
1214.111688	81180.463051	35.471514
1215.695878	81290.085865	35.476532
1217.050995	81392.485135	35.481549
1217.795696	81504.063865	35.486567
1219.142068	81611.507781	35.491584
1220.447000	81705.934157	35.496602
1222.092294	81808.302449	35.501620
1223.348355	81905.879189	35.506637
1224.161362	82003.917993	35.511655
1225.641213	82117.209178	35.516672
1226.880836	82205.553208	35.521690
1227.874314	82319.921834	35.526708
1229.071501	82429.077195	35.531725
1230.130562	82527.155540	35.536743
1231.488408	82644.091458	35.541760
1232.592489	82750.234406	35.546778
1233.518619	82857.406394	35.551796
1234.800485	82980.095113	35.556813
1235.915399	83091.711190	35.561831
1237.192787	83201.021760	35.566848
1238.273863	83319.257907	35.571866
1239.000750	83438.246550	35.576884
1240.477210	83552.532304	35.581901
1241.523667	83678.098867	35.586919
1242.673665	83798.353562	35.591936
1243.977683	83916.443453	35.596954
1245.182740	84051.794050	35.601972
1246.038848	84168.788998	35.606989
1247.651126	84298.489579	35.612007
1249.141626	84417.528167	35.617024
1250.643356	84533.917282	35.622042
1251.803003	84650.904967	35.627060
1253.216263	84759.288050	35.632077
1254.816716	84865.437642	35.637095
1255.910009	84965.039580	35.642112
1256.926977	85056.404830	35.647130
1258.212245	85172.183999	35.652148
1259.183554	85282.183730	35.657165
1261.079093	85379.926274	35.662183
1262.612323	85473.518665	35.667200
1263.854111	85567.055353	35.672218
1265.047082	85674.348421	35.677236
1266.624395	85768.897936	35.682253
1268.031506	85858.823816	35.687271
1268.863498	85962.740167	35.692288
1270.318519	86054.116423	35.697306
1271.453245	86153.639988	35.702324
1272.571550	86246.006960	35.707341
1273.802382	86354.272374	35.712359
1274.903562	86470.161428	35.717376
1276.079116	86570.262967	35.722394
1277.206295	86699.150159	35.727412
1278.466038	86806.449696	35.732429
1279.347119	86918.560550	35.737447
1280.724618	87039.072138	35.742464
1282.119646	87163.269066	35.747482
1283.197491	87279.887279	35.752500
1284.547126	87397.667509	35.757517
1286.032156	87521.345062	35.762535
1286.620759	87653.095509	35.767552
1288.179488	87780.437644	35.772570
1289.314466	87917.109803	35.777588
1290.777877	88041.502569	35.782605
1292.169664	88173.624559	35.787623
1292.930078	88301.726837	35.792640
1294.534506	88436.744270	35.797658
1295.938754	88571.970898	35.802676
1297.084808	88711.116187	35.807693
1298.685587	88847.479377	35.812711
1299.601462	88985.724000	35.817728
1301.289139	89106.259151	35.822746
1302.289517	89241.196860	35.827764
1304.458097	89373.786267	35.832781
1305.490334	89504.854949	35.837799
1306.774959	89629.903210	35.842816
1308.783316	89755.130832	35.847834
1310.032726	89878.360683	35.852852
1311.254439	90005.790209	35.857869
1312.441147	90125.786483	35.862887
1314.200355	90263.145380	35.867904
1315.704847	90380.647251	35.872922
1316.698152	90498.900845	35.877940
1317.728097	90616.186014	35.882957
1319.512892	90745.077221	35.887975
1320.503509	90882.520571	35.892992
1321.800046	90996.432562	35.898010
1322.968536	91123.304813	35.903028
1324.008516	91247.269953	35.908045
1325.552242	91369.522268	35.913063
1327.085303	91500.217562	35.918080
1328.393937	91622.735627	35.923098
1329.888581	91754.565985	35.928116
1331.120165	91877.147771	35.933133
1332.786534	91998.686472	35.938151
1334.022624	92133.815976	35.943168
1335.248515	92261.812079	35.948186
1336.762694	92376.202371	35.953204
1338.770352	92488.399674	35.958221
1340.120635	92599.660413	35.963239
1341.371308	92708.731715	35.968256
1342.792233	92809.158278	35.973274
1343.792769	92928.307471	35.978292
1345.121205	93026.949368	35.983309
1346.003121	93136.307740	35.988327
1346.814606	93245.360600	35.993344
1348.588399	93348.598484	35.998362
1349.574001	93455.926586	36.003380
1351.227058	93568.690051	36.008397
1352.377716	93676.500227	36.013415
1353.597927	93804.478340	36.018432
1355.085083	93923.276820	36.023450
1356.046397	94031.041663	36.028468
1357.574280	94155.804610	36.033485
1359.030653	94269.082913	36.038503
1360.103912	94395.337200	36.043520
1361.493869	94523.114430	36.048538
1362.764519	94659.238378	36.053556
1363.912465	94791.554091	36.058573
1365.354216	94920.402301	36.063591
1366.536342	95057.568481	36.068608
1368.083083	95186.109921	36.073626
1369.370602	95324.312938	36.078644
1370.635123	95462.900416	36.083661
1372.353122	95592.937951	36.088679
1373.469891	95733.919971	36.093696
1375.173776	95867.269196	36.098714
1376.638732	96007.133497	36.103732
1378.131924	96145.219415	36.108749
1379.244991	96286.356616	36.113767
1380.212414	96420.469302	36.118784
1382.074640	96563.139018	36.123802
1383.483811	96707.058773	36.128820
1384.523565	96851.962043	36.133837
1386.377391	96989.133572	36.138855
1387.465443	97135.627828	36.143872
1388.823182	97285.630148	36.148890
1390.341119	97432.109576	36.153908
1391.616507	97578.095028	36.158925
1393.050337	97716.323852	36.163943
1394.617838	97855.445184	36.168960
1396.073181	98001.924317	36.173978
1397.463647	98150.746726	36.178996
1398.799783	98301.048784	36.184013
1400.378164	98441.755580	36.189031
1401.764950	98591.544057	36.194048
1403.284419	98728.711785	36.199066
1405.058785	98871.037964	36.204084
1406.043655	99020.472675	36.209101
1408.263574	99157.812117	36.214119
1409.633864	99286.892164	36.219136
1411.940038	99400.348289	36.224154
1413.789752	99523.459805	36.229172
1414.698032	99653.082293	36.234189
1416.448689	99768.122097	36.239207
1417.892700	99900.146941	36.244224
1419.869425	100010.043464	36.249242
1420.893083	100122.966477	36.254260
1422.144109	100235.854496	36.259277
1423.711056	100360.635944	36.264295
1424.846329	100482.024091	36.269312
1426.051176	100610.678808	36.274330
1427.196278	100733.105930	36.279348
1428.542996	100868.699620	36.284365
1430.130139	100981.613991	36.289383
1431.290949	101109.707043	36.294400
1432.540457	101239.549015	36.299418
1434.260407	101370.256446	36.304436
1435.329292	101502.257465	36.309453
1437.361165	101614.179323	36.314471
1438.659242	101733.087274	36.319488
1439.563218	101840.989033	36.324506
1440.933507	101961.915070	36.329524
1442.180327	102083.050944	36.334541
1443.830791	102202.184672	36.339559
1444.948577	102323.912040	36.344576
1446.167456	102444.571824	36.349594
1447.801396	102568.400431	36.354612
1448.759477	102702.540819	36.359629
1450.057683	102830.822078	36.364647
1451.545052	102976.126996	36.369664
1452.998171	103113.729313	36.374682
1454.778949	103240.288839	36.379700
1456.269879	103379.838886	36.384717
1457.996844	103507.713715	36.389735
1459.886255	103643.627453	36.394752
1461.027936	103766.421438	36.399770
1462.735798	103902.871648	36.404788
1463.874555	104044.038804	36.409805
1465.763149	104180.842392	36.414823
1466.827165	104320.792492	36.419840
1467.938255	104458.770595	36.424858
1469.773991	104600.161278	36.429876
1470.680872	104757.254502	36.434893
1472.129241	104891.302057	36.439911
1473.479953	105042.812066	36.444928
1475.201004	105196.610799	36.449946
1476.525607	105349.127922	36.454964
1477.916262	105501.787609	36.459981
1479.748928	105638.745329	36.464999
1481.468587	105801.042323	36.470016
1482.359228	105951.537582	36.475034
1484.341976	106102.839865	36.480052
1485.669414	106262.740259	36.485069
1487.368271	106414.202237	36.490087
1489.092636	106560.335373	36.495104
1490.407182	106712.492490	36.500122
1491.817382	106857.712127	36.505140
1493.177779	107023.735401	36.510157
1495.101111	107170.043065	36.515175
1496.883750	107318.224557	36.520192
1498.393569	107466.322351	36.525210
1499.800477	107612.217758	36.530228
1501.082496	107761.949998	36.535245
1502.812312	107908.202173	36.540263
1504.426100	108057.807981	36.545280
1505.657998	108214.803197	36.550298
1507.848027	108355.659841	36.555316
1509.698968	108495.847044	36.560333
1511.928072	108626.275271	36.565351
1513.598788	108753.075460	36.570368
1515.001812	108875.948711	36.575386
1516.794367	109005.964448	36.580404
1518.016874	109143.563763	36.585421
1519.327611	109271.867491	36.590439
1520.580295	109402.133590	36.595456
1521.821654	109547.314755	36.600474
1523.331123	109681.866143	36.605492
1524.154672	109824.361708	36.610509
1525.688285	109978.299841	36.615527
1527.310698	110126.125181	36.620544
1528.747575	110276.706487	36.625562
1530.334744	110418.388146	36.630580
1531.952246	110569.652747	36.635597
1533.257051	110717.770956	36.640615
1534.858574	110864.423283	36.645632
1536.205556	111022.579914	36.650650
1537.532906	111159.701607	36.655668
1538.849934	111308.441787	36.660685
1540.270546	111450.369101	36.665703
1541.518130	111589.825617	36.670720
1542.786025	111742.531955	36.675738
1544.598608	111887.735312	36.680756
1545.640032	112052.234267	36.685773
1547.168065	112202.606671	36.690791
1548.486105	112360.228436	36.695808
1550.024674	112524.905830	36.700826
1551.425879	112680.398161	36.705844
1553.235480	112847.672729	36.710861
1554.433998	113007.877739	36.715879
1556.127752	113175.958162	36.720896
1557.622270	113358.629691	36.725914
1559.564970	113521.371764	36.730932
1561.049870	113687.572037	36.735949
1562.898460	113852.029694	36.740967
1564.685995	114020.137496	36.745984
1566.761207	114182.570219	36.751002
1568.560425	114334.279035	36.756020
1570.117717	114496.311828	36.761037
1571.531815	114662.514900	36.766055
1573.201112	114829.401929	36.771072
1574.512445	114997.791286	36.776090
1576.212293	115151.459449	36.781108
1577.715524	115315.305266	36.786125
1579.094759	115481.542846	36.791143
1581.075972	115646.558685	36.796160
1582.987979	115809.112815	36.801178
1584.945854	115967.018459	36.806196
1586.393945	116131.396501	36.811213
1587.880468	116290.898886	36.816231
1589.907197	116449.531507	36.821248
1591.426196	116613.951387	36.826266
1592.734734	116775.259239	36.831284
1594.138947	116942.184403	36.836301
1596.059894	117104.362314	36.841319
1597.514324	117268.300470	36.846336
1599.232681	117437.512751	36.851354
1600.662569	117598.868692	36.856372
1601.989385	117767.280904	36.861389
1603.809954	117944.622595	36.866407
1605.687625	118100.025663	36.871424
1606.983726	118273.480453	36.876442
1609.063450	118429.538368	36.881460
1611.188621	118578.359906	36.886477
1612.881933	118735.417852	36.891495
1615.350571	118888.715403	36.896512
1616.411040	119046.532713	36.901530
1618.071363	119191.649096	36.906548
1619.741335	119340.772792	36.911565
1621.703460	119478.435621	36.916583
1623.704740	119625.327146	36.921600
1624.928223	119777.464837	36.926618
1626.799319	119918.847302	36.931636
1628.420237	120067.093548	36.936653
1629.679339	120215.295204	36.941671
1631.228345	120356.983107	36.946688
1632.367518	120508.870440	36.951706
1634.101886	120661.781997	36.956724
1635.370131	120824.965338	36.961741
1636.849400	120982.078502	36.966759
1638.391479	121139.030309	36.971776
1639.419560	121304.993003	36.976794
1641.296491	121462.147699	36.981812
1642.415267	121635.987805	36.986829
1644.159668	121804.796776	36.991847
1645.829817	121966.958284	36.996864
1647.072716	122132.713474	37.001882
1648.997398	122289.356659	37.006900
1649.843022	122459.538819	37.011917
1651.374337	122627.027162	37.016935
1652.864074	122791.478169	37.021952
1654.452413	122970.414106	37.026970
1655.835788	123135.542750	37.031988
1658.345981	123307.714849	37.037005
1659.901374	123473.312871	37.042023
1661.480597	123652.494340	37.047040
1663.240468	123829.948599	37.052058
1665.032925	124005.203918	37.057076
1666.760911	124182.690082	37.062093
1668.200714	124357.151875	37.067111
1669.941060	124534.980201	37.072128
1671.514631	124723.910251	37.077146
1672.846005	124906.205957	37.082164
1674.797745	125090.308868	37.087181
1676.083368	125277.066240	37.092199
1677.696378	125467.845838	37.097216
1679.050521	125673.674650	37.102234
1680.864397	125864.602463	37.107252
1682.661831	126072.064289	37.112269
1683.997626	126285.777397	37.117287
1685.693389	126479.339915	37.122304
1687.320323	126693.745670	37.127322
1688.613559	126901.670782	37.132340
1690.056009	127119.900828	37.137357
1691.882525	127340.520832	37.142375
1693.678207	127569.380677	37.147392
1695.038163	127785.381482	37.152410
1696.962891	128008.882417	37.157428
1698.955249	128240.316218	37.162445
1700.623718	128462.007140	37.167463
1703.034423	128665.745322	37.172480
1704.978644	128882.764682	37.177498
1706.893410	129092.760895	37.182516
1708.799473	129312.440097	37.187533
1710.689861	129525.994777	37.192551
1712.345478	129737.810804	37.197568
1713.978323	129949.923255	37.202586
1715.751144	130157.663071	37.207604
1717.415221	130367.742703	37.212621
1718.959940	130584.566541	37.217639
1720.562440	130786.334552	37.222656
1722.200178	131014.679461	37.227674
1723.771771	131230.017887	37.232692
1725.587573	131452.462821	37.237709
1727.340577	131679.790959	37.242727
1729.229626	131892.088864	37.247744
1731.117340	132116.581532	37.252762
1733.300542	132337.083273	37.257780
1735.381153	132541.576539	37.262797
1736.736766	132754.380404	37.267815
1738.689811	132963.514134	37.272832
1740.380911	133180.340901	37.277850
1741.959967	133396.158390	37.282868
1743.847562	133601.739816	37.287885
1745.519958	133816.821579	37.292903
1746.977518	134030.745067	37.297920
1748.734121	134243.087680	37.302938
1750.107114	134460.147889	37.307956
1752.384277	134679.060622	37.312973
1753.867199	134902.323537	37.317991
1756.131093	135113.360496	37.323008
1757.613348	135318.606897	37.328026
1759.283721	135534.534760	37.333044
1761.677332	135748.942573	37.338061
1762.733087	135947.647043	37.343079
1764.737313	136138.210374	37.348096
1766.320493	136335.844678	37.353114
1767.778596	136531.329383	37.358132
1770.013754	136725.983367	37.363149
1771.845839	136918.924354	37.368167
1773.873614	137100.973246	37.373184
1776.304895	137289.152698	37.378202
1777.971437	137475.548463	37.383220
1779.750956	137662.054298	37.388237
1781.267945	137858.601457	37.393255
1782.536835	138041.926974	37.398272
1783.920916	138249.397222	37.403290
1785.672998	138460.262844	37.408308
1787.666992	138662.284766	37.413325
1788.954833	138888.465520	37.418343
1790.614853	139095.465119	37.423360
1792.658937	139306.555612	37.428378
1794.155490	139524.343989	37.433396
1796.038915	139735.436030	37.438413
1797.863790	139965.738939	37.443431
1799.632959	140180.657918	37.448448
1801.346791	140405.332921	37.453466
1803.330413	140641.375967	37.458484
1805.433378	140863.974741	37.463501
1806.708497	141101.183663	37.468519
1808.815402	141318.999484	37.473536
1810.360443	141554.836089	37.478554
1812.031256	141790.679653	37.483572
1813.868498	142027.627972	37.488589
1815.463776	142269.640809	37.493607
1817.423103	142510.138697	37.498624
1819.096966	142757.700485	37.503642
1820.800547	142994.179344	37.508660
1822.712946	143242.785221	37.513677
1824.063674	143493.840385	37.518695
1826.253006	143744.372868	37.523712
1827.925919	143994.860076	37.528730
1829.473583	144254.252213	37.533748
1831.503815	144499.076625	37.538765
1833.277893	144772.130602	37.543783
1835.250303	145026.104692	37.548800
1837.355598	145283.600432	37.553818
1839.174744	145531.788016	37.558836
1841.410068	145786.486532	37.563853
1843.210373	146046.978179	37.568871
1845.215341	146297.323627	37.573888
1847.037063	146546.988054	37.578906
1849.314878	146805.784640	37.583924
1851.460748	147041.134858	37.588941
1853.666419	147286.389632	37.593959
1855.769550	147518.854802	37.598976
1857.606421	147748.354319	37.603994
1859.484060	147990.858421	37.609012
1861.753843	148219.416844	37.614029
1863.453725	148458.904542	37.619047
1865.268412	148688.906653	37.624064
1867.239838	148917.044912	37.629082
1868.777390	149171.868666	37.634100
1870.854156	149389.216302	37.639117
1872.240538	149631.829794	37.644135
1874.380438	149867.993278	37.649152
1875.955896	150104.956465	37.654170
1877.868195	150364.398651	37.659188
1879.070037	150611.081719	37.664205
1880.855142	150856.532739	37.669223
1882.662759	151115.258606	37.674240
1884.512273	151366.617006	37.679258
1885.798376	151611.895224	37.684276
1887.929980	151843.816304	37.689293
1889.492780	152088.634702	37.694311
1891.063127	152330.038424	37.699328
1892.886443	152572.673197	37.704346
1894.415121	152830.143095	37.709364
1896.378610	153078.660849	37.714381
1897.972224	153342.279495	37.719399
1899.687242	153605.258481	37.724416
1901.525750	153862.139060	37.729434
1903.047338	154144.293180	37.734452
1905.637615	154396.781291	37.739469
1907.671705	154654.980594	37.744487
1910.228831	154929.868715	37.749504
1912.135108	155186.528919	37.754522
1913.880556	155458.410407	37.759540
1916.031951	155713.549569	37.764557
1917.731890	155979.829669	37.769575
1919.763736	156253.574476	37.774592
1922.030819	156512.304370	37.779610
1923.776397	156791.021730	37.784628
1925.350231	157063.165903	37.789645
1927.387529	157343.439997	37.794663
1929.531428	157617.338728	37.799680
1931.405965	157892.981750	37.804698
1933.202536	158172.637072	37.809716
1935.201970	158443.337556	37.814733
1937.200760	158730.479417	37.819751
1939.623151	159004.963181	37.824768
1941.748679	159274.010083	37.829786
1942.801899	159554.155624	37.834804
1944.900320	159836.044062	37.839821
1947.385632	160128.220261	37.844839
1949.328902	160404.054379	37.849856
1950.979121	160685.775228	37.854874
1953.276683	160972.817573	37.859892
1955.170671	161260.990467	37.864909
1956.905432	161550.319369	37.869927
1959.050433	161827.017037	37.874944
1961.256133	162117.075056	37.879962
1963.686996	162393.375214	37.884980
1966.109703	162663.164871	37.889997
1968.486389	162928.773181	37.895015
1970.615300	163200.781805	37.900032
1972.710235	163460.913414	37.905050
1974.438690	163732.097863	37.910068
1976.166918	163990.815911	37.915085
1978.160995	164268.842516	37.920103
1980.268296	164540.250649	37.925120
1982.507852	164807.144837	37.930138
1984.578697	165074.701166	37.935156
1986.230753	165338.273606	37.940173
1988.096655	165613.342124	37.945191
1989.811458	165887.940115	37.950208
1991.577643	166164.740411	37.955226
1992.926693	166457.959908	37.960244
1994.649254	166751.249494	37.965261
1996.807156	167040.587396	37.970279
1998.430550	167344.001474	37.975296
2000.374498	167629.921624	37.980314
2002.169801	167933.768595	37.985332
2004.250388	168233.242843	37.990349
2006.267668	168531.115704	37.995367
2008.275011	168829.905542	38.000384
2010.008488	169137.068509	38.005402
2012.079762	169441.526525	38.010420
2013.999242	169742.987529	38.015437
2016.095496	170040.333776	38.020455
2017.892846	170332.191754	38.025472
2019.939602	170613.308257	38.030490
2021.520772	170909.163725	38.035508
2023.937619	171198.655894	38.040525
2026.018296	171477.281706	38.045543
2027.594366	171772.214480	38.050560
2029.693788	172067.422491	38.055578
2031.646885	172367.238255	38.060596
2033.510781	172672.732231	38.065613
2035.808945	172973.575972	38.070631
2037.318456	173271.356495	38.075648
2039.583858	173581.235796	38.080666
2041.548624	173897.232687	38.085684
2043.824049	174202.287711	38.090701
2046.023404	174513.539652	38.095719
2047.748285	174835.596461	38.100736
2049.838152	175148.213911	38.105754
2051.752218	175471.234280	38.110772
2053.675866	175801.911429	38.115789
2055.577184	176129.774397	38.120807
2057.708548	176467.139259	38.125824
2060.030616	176795.510822	38.130842
2061.716788	177132.185783	38.135860
2063.578208	177462.688799	38.140877
2066.005930	177799.352615	38.145895
2067.854934	178150.457143	38.150912
2069.840999	178500.932252	38.155930
2072.294002	178840.339126	38.160948
2074.764859	179163.972824	38.165965
2077.741650	179478.512909	38.170983
2080.281149	179807.573348	38.176000
2082.886098	180125.907046	38.181018
2085.152547	180448.205804	38.186036
2087.448667	180759.173700	38.191053
2089.395967	181078.730632	38.196071
2090.921238	181404.653055	38.201088
2093.473379	181728.664361	38.206106
2095.088467	182049.139911	38.211124
2096.964413	182372.014195	38.216141
2099.088508	182705.873832	38.221159
2100.733996	183034.780255	38.226176
2103.229248	183366.120812	38.231194
2104.920275	183701.676843	38.236212
2107.016734	184052.105347	38.241229
2109.089865	184387.883669	38.246247
2110.904527	184743.743038	38.251264
2112.810737	185085.061256	38.256282
2114.796104	185443.969831	38.261300
2117.168988	185793.574104	38.266317
2119.022037	186146.714769	38.271335
2121.176034	186575.982250	38.276352
2123.328624	186914.347339	38.281370
2124.949534	187280.761069	38.286388
2126.879591	187646.416769	38.291405
2128.996105	188001.326060	38.296423
2131.185076	188373.420853	38.301440
2133.407821	188748.026244	38.306458
2135.898319	189103.592126	38.311476
2137.958692	189466.846080	38.316493
2140.750720	189835.295956	38.321511
2143.159037	190198.548921	38.326528
2145.760373	190526.314310	38.331546
2147.874506	190876.915105	38.336564
2150.092851	191227.449936	38.341581
2152.417749	191573.244748	38.346599
2154.140418	191922.512559	38.351616
2156.692794	192272.871487	38.356634
2158.558464	192610.231562	38.361652
2160.425780	192947.363702	38.366669
2163.845932	193235.841200	38.371687
2165.951205	193555.309818	38.376704
2167.617873	193850.869049	38.381722
2169.920280	194165.152142	38.386740
2172.085718	194485.883780	38.391757
2173.840936	194800.685395	38.396775
2175.877583	195129.262194	38.401792
2178.113422	195448.080142	38.406810
2179.721350	195777.487296	38.411828
2181.679021	196112.429116	38.416845
2183.629255	196457.965297	38.421863
2185.610931	196811.549710	38.426880
2187.351838	197157.831443	38.431898
2189.260387	197522.453282	38.436916
2190.958279	197896.482042	38.441933
2193.160806	198258.951647	38.446951
2195.430131	198632.258309	38.451968
2197.622599	199011.928326	38.456986
2199.890344	199394.991434	38.462004
2201.789527	199785.530231	38.467021
2204.303364	200158.954981	38.472039
2206.181128	200547.035004	38.477056
2208.422869	200946.007648	38.482074
2210.343889	201344.065895	38.487092
2212.647085	201738.255275	38.492109
2215.053490	202134.893541	38.497127
2217.318949	202525.991533	38.502144
2219.751053	202924.964631	38.507162
2222.138023	203330.397888	38.512180
2224.387610	203743.042362	38.517197
2226.167483	204152.661740	38.522215
2228.523445	204559.753700	38.527232
2230.543854	204967.864052	38.532250
2233.296973	205374.997534	38.537268
2235.304298	205804.195971	38.542285
2237.767841	206209.089954	38.547303
2239.848811	206633.350503	38.552320
2242.122937	207052.272616	38.557338
2244.417466	207469.363346	38.562356
2246.332441	207898.453383	38.567373
2248.552543	208314.896790	38.572391
2251.099979	208741.756113	38.577408
2253.422999	209162.630563	38.582426
2255.480282	209596.147118	38.587444
2257.677688	210026.645025	38.592461
2260.219496	210463.288475	38.597479
2262.518926	210888.335610	38.602496
2264.519353	211334.591007	38.607514
2266.991658	211757.351671	38.612532
2269.942550	212174.805351	38.617549
2272.547858	212588.579079	38.622567
2275.145656	213015.716817	38.627584
2277.064274	213436.025644	38.632602
2279.263743	213859.466758	38.637620
2281.652329	214280.109969	38.642637
2283.940005	214698.508459	38.647655
2286.333503	215125.883883	38.652672
2288.497131	215543.819959	38.657690
2291.186852	215972.674447	38.662708
2293.356706	216386.926881	38.667725
2295.504496	216794.324112	38.672743
2297.718943	217211.618847	38.677760
2300.215914	217643.477219	38.682778
2302.451466	218051.547788	38.687796
2304.618366	218485.820809	38.692813
2307.105051	218901.245487	38.697831
2309.448245	219311.764423	38.702848
2311.834176	219703.478035	38.707866
2314.025263	220091.767261	38.712884
2315.604955	220492.650622	38.717901
2318.120495	220878.349375	38.722919
2320.485447	221288.027748	38.727936
2322.886315	221689.952488	38.732954
2324.467208	222092.919550	38.737972
2326.496128	222504.352805	38.742989
2329.005335	222914.263424	38.748007
2331.176238	223338.580119	38.753024
2333.565541	223753.971510	38.758042
2335.519907	224174.994174	38.763060
2338.093780	224604.202237	38.768077
2340.578098	225035.227987	38.773095
2342.693443	225471.874696	38.778112
2344.536506	225908.487586	38.783130
2346.954762	226345.061771	38.788148
2349.394766	226790.117519	38.793165
2351.719469	227227.900193	38.798183
2353.968939	227688.151728	38.803200
2355.796910	228148.265534	38.808218
2358.425269	228605.790468	38.813236
2360.715429	229061.411783	38.818253
2363.698651	229512.835027	38.823271
2366.399573	229968.239651	38.828288
2368.594669	230440.260814	38.833306
2371.035808	230899.643046	38.838324
2373.295777	231370.103958	38.843341
2375.878797	231820.165703	38.848359
2378.223386	232291.552789	38.853376
2380.510537	232769.274051	38.858394
2383.150796	233235.736843	38.863412
2385.471712	233712.689950	38.868429
2388.114036	234185.553385	38.873447
2390.216020	234656.976226	38.878464
2392.563678	235143.805888	38.883482
2395.125073	235620.795884	38.888500
2397.507271	236089.302960	38.893517
2399.468978	236574.946245	38.898535
2401.852422	237059.253096	38.903552
2403.921197	237554.150803	38.908570
2406.568566	238049.059383	38.913588
2409.094746	238545.815154	38.918605
2411.465325	239043.127851	38.923623
2413.780186	239531.201542	38.928640
2415.732413	240035.741521	38.933658
2418.395981	240527.163360	38.938676
2421.056690	241033.903022	38.943693
2424.351780	241530.051429	38.948711
2427.101107	242018.561227	38.953728
2429.633767	242503.369525	38.958746
2432.585146	242983.513727	38.963764
2434.849585	243464.779996	38.968781
2437.617305	243931.969844	38.973799
2440.297130	244416.192441	38.978816
2442.381617	244900.481221	38.983834
2445.121854	245368.764631	38.988852
2447.294370	245850.675073	38.993869
2449.691880	246334.530786	38.998887
2452.070098	246808.989315	39.003904
2454.306745	247293.960030	39.008922
2456.967431	247777.567990	39.013940
2459.171011	248272.524563	39.018957
2461.325008	248750.696475	39.023975
2463.629321	249235.626157	39.028992
2466.054687	249732.169928	39.034010
2468.687642	250217.045718	39.039028
2471.238783	250696.801599	39.044045
2473.468711	251159.332632	39.049063
2475.972305	251623.496289	39.054080
2478.045440	252092.374138	39.059098
2480.681376	252557.784541	39.064116
2483.226296	253015.688757	39.069133
2485.855245	253474.442163	39.074151
2488.685425	253939.487844	39.079168
2490.760807	254413.692464	39.084186
2493.581723	254873.173636	39.089204
2495.973630	255349.993028	39.094221
2498.191005	255817.464857	39.099239
2500.563275	256284.326751	39.104256
2502.605249	256772.803992	39.109274
2505.108229	257249.396202	39.114292
2507.735307	257742.833585	39.119309
2509.936301	258247.689558	39.124327
2513.232558	258726.946916	39.129344
2515.444216	259221.001989	39.134362
2518.135853	259713.786549	39.139380
2520.789802	260212.747271	39.144397
2523.309233	260702.836717	39.149415
2526.305229	261199.403211	39.154432
2528.488507	261708.108303	39.159450
2530.983383	262210.285636	39.164468
2532.986613	262712.003838	39.169485
2535.716649	263220.312205	39.174503
2538.062464	263740.209444	39.179520
2540.406800	264263.126953	39.184538
2543.067606	264777.610840	39.189556
2545.638273	265311.358884	39.194573
2547.299458	265842.731199	39.199591
2550.298304	266370.768506	39.204608
2552.856827	266922.086141	39.209626
2555.520199	267439.604092	39.214644
2558.824749	267971.471340	39.219661
2561.359545	268502.058546	39.224679
2564.618785	269039.870190	39.229696
2567.265006	269562.586068	39.234714
2570.218774	270081.822428	39.239732
2572.677251	270613.781095	39.244749
2574.659867	271138.623157	39.249767
2577.878562	271661.847542	39.254784
2580.497682	272191.511524	39.259802
2583.266607	272709.237683	39.264820
2586.110992	273230.326844	39.269837
2588.503674	273753.108558	39.274855
2591.187838	274271.676628	39.279872
2593.458683	274806.966045	39.284890
2596.153727	275332.509949	39.289908
2598.741827	275851.108551	39.294925
2600.812433	276386.825232	39.299943
2603.377631	276912.379179	39.304960
2605.871138	277456.632169	39.309978
2608.576483	277998.334280	39.314996
2610.839982	278547.034374	39.320013
2613.251723	279086.082694	39.325031
2615.744088	279636.364722	39.330048
2618.306654	280197.069158	39.335066
2621.150482	280755.033797	39.340084
2624.088821	281299.088722	39.345101
2626.596767	281843.638309	39.350119
2629.303011	282398.031308	39.355136
2631.865550	282949.649077	39.360154
2634.206501	283504.344331	39.365172
2637.307319	284051.400489	39.370189
2639.565543	284602.722628	39.375207
2642.145731	285158.332525	39.380224
2644.712047	285716.631755	39.385242
2647.060617	286240.832411	39.390260
2650.222609	286767.365499	39.395277
2652.569944	287292.446899	39.400295
2655.322875	287810.579751	39.405312
2658.106656	288336.422890	39.410330
2661.222689	288845.197599	39.415348
2664.599436	289363.881241	39.420365
2667.538985	289862.721892	39.425383
2670.076113	290375.256329	39.430400
2672.675779	290891.052317	39.435418
2674.728534	291410.483882	39.440436
2677.403126	291937.761585	39.445453
2680.149135	292449.687916	39.450471
2682.767328	292987.654727	39.455488
2685.421399	293510.275704	39.460506
2687.766328	294047.158474	39.465524
2690.477368	294582.532257	39.470541
2692.625848	295132.816053	39.475559
2695.244129	295693.507240	39.480576
2697.657970	296254.910357	39.485594
2700.055781	296820.702737	39.490612
2703.076374	297382.228968	39.495629
2705.727051	297951.245910	39.500647
2708.227759	298530.765591	39.505664
2710.950330	299106.106613	39.510682
2713.757736	299681.758524	39.515700
2716.917443	300261.106878	39.520717
2719.349708	300835.662692	39.525735
2722.392641	301417.301752	39.530752
2725.103788	302009.851426	39.535770
2727.624593	302602.601868	39.540788
2730.452682	303185.956008	39.545805
2733.275724	303789.028817	39.550823
2736.582994	304369.553643	39.555840
2738.757832	304966.215164	39.560858
2741.506478	305564.024322	39.565876
2744.341110	306157.269367	39.570893
2746.871386	306768.907314	39.575911
2749.637472	307372.835340	39.580928
2752.331636	307981.107788	39.585946
2754.746848	308589.010073	39.590964
2757.822877	309210.559354	39.595981
2760.215640	309823.627885	39.600999
2763.208462	310433.168746	39.606016
2766.215250	311059.096212	39.611034
2768.969938	311692.491419	39.616052
2771.880757	312298.112582	39.621069
2774.316844	312935.906247	39.626087
2777.548692	313542.172078	39.631104
2780.458840	314165.890661	39.636122
2783.368104	314793.204849	39.641140
2786.321470	315400.047968	39.646157
2789.163571	316024.868536	39.651175
2792.265079	316645.198866	39.656192
2795.197763	317252.071103	39.661210
2798.495625	317856.264341	39.666228
2801.552644	318458.355111	39.671245
2804.330375	319065.835677	39.676263
2807.093239	319671.914397	39.681280
2809.835850	320275.221787	39.686298
2812.532915	320885.582374	39.691316
2815.803904	321478.234238	39.696333
2818.442165	322084.095369	39.701351
2821.475930	322672.656682	39.706368
2824.044314	323277.065197	39.711386
2826.652908	323886.127582	39.716404
2829.578584	324482.114906	39.721421
2832.220522	325076.691496	39.726439
2835.185210	325656.416711	39.731456
2838.125452	326214.875094	39.736474
2840.411892	326774.746905	39.741492
2843.491367	327348.086986	39.746509
2845.871275	327929.342232	39.751527
2848.622527	328500.940855	39.756544
2850.934416	329078.714026	39.761562
2853.637654	329676.232285	39.766580
2856.193561	330259.683901	39.771597
2858.485975	330876.605237	39.776615
2861.146505	331479.962945	39.781632
2863.934779	332106.377143	39.786650
2866.371475	332730.755593	39.791668
2868.934276	333354.571458	39.796685
2871.663256	334015.667158	39.801703
2873.933909	334658.304446	39.806720
2877.074767	335307.821908	39.811738
2880.145758	335972.254355	39.816756
2882.873315	336616.587735	39.821773
2885.587161	337280.620962	39.826791
2888.984521	337962.392746	39.831808
2891.529796	338625.387730	39.836826
2894.904867	339305.108535	39.841844
2897.908287	339981.221939	39.846861
2900.639857	340659.723604	39.851879
2903.723943	341347.364068	39.856896
2906.847053	342024.738738	39.861914
2910.116048	342698.526979	39.866932
2913.430786	343378.128135	39.871949
2916.046307	344064.469257	39.876967
2918.989946	344753.256295	39.881984
2921.782053	345437.158643	39.887002
2925.120012	346122.813521	39.892020
2928.204214	346813.667150	39.897037
2931.375094	347496.150290	39.902055
2934.500718	348179.006911	39.907072
2937.925966	348871.058211	39.912090
2940.449337	349546.297216	39.917108
2943.597215	350227.485265	39.922125
2946.600831	350906.577071	39.927143
2949.798285	351593.839539	39.932160
2953.128207	352274.905671	39.937178
2956.141454	352962.826854	39.942196
2959.450363	353630.607407	39.947213
2962.578144	354312.726461	39.952231
2965.444656	354983.716489	39.957248
2968.175126	355659.555568	39.962266
2971.038408	356340.657792	39.967284
2974.286557	357015.930654	39.972301
2977.279497	357693.966324	39.977319
2980.100631	358378.934232	39.982336
2983.489443	359062.252224	39.987354
2986.130255	359746.964081	39.992372
2989.196703	360414.661947	39.997389
2991.726206	361099.943539	40.002407
2994.188446	361791.353862	40.007424
2997.295988	362476.970268	40.012442
3000.487143	363181.237458	40.017460
3003.554395	363872.125091	40.022477
3006.366018	364570.005962	40.027495
3009.439542	365271.124128	40.032512
3012.127475	365977.835555	40.037530
3014.783730	366681.138808	40.042548
3017.797622	367379.402276	40.047565
3020.645762	368096.731111	40.052583
3023.774402	368813.998283	40.057600
3027.098655	369514.340542	40.062618
3029.565873	370215.026875	40.067636
3032.688615	370901.860209	40.072653
3035.283651	371597.120362	40.077671
3037.998279	372279.017094	40.082688
3040.913732	372960.485760	40.087706
3043.813087	373661.220909	40.092724
3046.953798	374349.080871	40.097741
3049.831709	375052.089328	40.102759
3052.349774	375752.450199	40.107776
3056.109139	376453.689141	40.112794
3058.631734	377179.903165	40.117812
3061.619394	377882.618236	40.122829
3065.169383	378603.541986	40.127847
3068.483256	379320.961933	40.132864
3071.947600	380020.658569	40.137882
3075.114632	380739.354634	40.142900
3078.611515	381452.381999	40.147917
3082.236863	382163.065022	40.152935
3085.253498	382865.060036	40.157952
3088.451111	383577.771658	40.162970
3091.449256	384299.586597	40.167988
3094.683493	385009.618853	40.173005
3097.918842	385730.571362	40.178023
3101.213350	386446.226820	40.183040
3104.173461	387157.685076	40.188058
3107.151739	387879.806424	40.193076
3110.609141	388605.276127	40.198093
3113.654060	389323.749676	40.203111
3117.489476	390041.294477	40.208128
3120.880205	390744.151697	40.213146
3124.186606	391455.964778	40.218164
3127.799884	392156.974573	40.223181
3131.316033	392865.625135	40.228199
3134.334234	393577.421105	40.233216
3137.703116	394301.141216	40.238234
3140.272790	395003.294271	40.243252
3143.862988	395705.926116	40.248269
3146.874998	396416.626314	40.253287
3149.796484	397138.203826	40.258304
3152.964576	397850.558015	40.263322
3155.578405	398575.176919	40.268340
3158.314268	399297.324651	40.273357
3161.189304	400035.727811	40.278375
3164.037543	400780.033963	40.283392
3167.362170	401520.395242	40.288410
3170.461303	402263.551627	40.293428
3173.242831	403014.730191	40.298445
3176.182352	403765.403988	40.303463
3179.214947	404534.207310	40.308480
3182.398983	405298.254474	40.313498
3185.424148	406067.361078	40.318516
3188.514368	406835.925187	40.323533
3191.770383	407611.015404	40.328551
3195.102858	408389.709993	40.333568
3198.985822	409152.858908	40.338586
3202.368015	409926.229390	40.343604
3205.317121	410689.976344	40.348621
3208.451169	411463.685408	40.353639
3211.831968	412246.283357	40.358656
3215.140588	413015.205032	40.363674
3218.496554	413790.364915	40.368692
3221.809809	414561.557791	40.373709
3225.473482	415324.676034	40.378727
3228.505439	416094.693958	40.383744
3231.966920	416863.554953	40.388762
3234.880576	417633.130797	40.393780
3237.962676	418405.737549	40.398797
3241.701389	419168.048055	40.403815
3244.738977	419927.354886	40.408832
3248.072258	420656.851872	40.413850
3250.872988	421388.580585	40.418868
3253.982357	422124.584228	40.423885
3256.909087	422859.174125	40.428903
3259.692916	423599.777130	40.433920
3262.568968	424335.080425	40.438938
3265.759582	425105.447971	40.443956
3268.966544	425860.616045	40.448973
3272.077891	426618.500838	40.453991
3275.445304	427390.270428	40.459008
3278.844957	428156.798309	40.464026
3281.793454	428926.905540	40.469044
3285.162805	429716.025041	40.474061
3287.788825	430487.992196	40.479079
3291.010961	431290.972199	40.484096
3293.975422	432091.280707	40.489114
3297.441186	432905.377249	40.494132
3300.010336	433726.250439	40.499149
3303.376936	434550.249722	40.504167
3307.120188	435380.067815	40.509184
3310.682113	436209.271975	40.514202
3314.103334	437049.629333	40.519220
3317.398951	437887.442872	40.524237
3321.032583	438719.710147	40.529255
3324.100686	439568.499498	40.534272
3327.092480	440410.896890	40.539290
3331.067086	441251.133356	40.544308
3334.252740	442112.116149	40.549325
3337.861899	442953.141187	40.554343
3341.255333	443815.326203	40.559360
3345.310446	444673.428313	40.564378
3348.692119	445515.937991	40.569396
3351.920759	446362.018642	40.574413
3356.073888	447213.269533	40.579431
3359.214038	448070.496257	40.584448
3362.747668	448909.643999	40.589466
3366.180459	449758.413076	40.594484
3369.695547	450614.046848	40.599501
3373.310981	451458.718164	40.604519
3376.699037	452319.086737	40.609536
3380.092001	453166.286601	40.614554
3383.556287	454023.178139	40.619572
3386.899174	454869.900279	40.624589
3390.124590	455728.159486	40.629607
3393.087772	456604.790690	40.634624
3396.250877	457464.387649	40.639642
3399.927132	458323.307047	40.644660
3403.417586	459205.175860	40.649677
3406.866266	460075.045662	40.654695
3410.486625	460942.674766	40.659712
3413.979235	461808.463157	40.664730
3417.401513	462676.741419	40.669748
3420.283430	463549.802187	40.674765
3424.256125	464419.671437	40.679783
3427.555465	465295.856398	40.684800
3432.738993	466129.780335	40.689818
3437.341494	466953.310899	40.694836
3441.185606	467782.669251	40.699853
3445.132626	468599.511405	40.704871
3448.927748	469421.027589	40.709888
3452.527832	470221.249477	40.714906
3455.855601	471020.718282	40.719924
3459.093357	471842.855768	40.724941
3462.607598	472635.055509	40.729959
3465.285893	473439.146317	40.734976
3468.639093	474246.520996	40.739994
3471.619490	475066.115087	40.745012
3474.705759	475869.126845	40.750016
3477.918838	476637.829761	40.755021
3480.804717	477369.246658	40.760026
3483.878366	478047.129655	40.765031
3486.902393	478670.814906	40.770036
3489.751335	479253.922461	40.775040
3492.683456	479781.559454	40.780045
3495.064171	480252.617355	40.785050
3497.133293	480679.494649	40.790055
3499.185326	481060.329989	40.795060
3501.443104	481405.753690	40.800064
3503.332814	481694.281819	40.805069
3504.745419	481951.147684	40.810074
3506.353977	482159.018492	40.815079
3507.938080	482332.936777	40.820084
3509.291775	482472.986243	40.825088
3510.685788	482576.043624	40.830093
3511.528711	482664.483277	40.835098
3512.640705	482698.162067	40.840103
3513.514246	482717.528812	40.845108
3514.410611	482714.812592	40.850112
3515.405281	482693.487875	40.855117
3515.997669	482637.363378	40.860122
3517.149815	482562.861375	40.865127
3517.557153	482472.862474	40.870132
3518.109988	482370.208904	40.875136
3518.443111	482232.321387	40.880141
3518.867716	482099.066899	40.885146
3519.088174	481951.796432	40.890151
3519.531872	481785.592400	40.895156
3519.248910	481618.185945	40.900160
3519.952306	481428.189310	40.905165
3519.957156	481241.836161	40.910170
3520.494766	481052.719793	40.915175
3520.413428	480842.423939	40.920180
3520.172534	480642.357498	40.925184
3520.101252	480431.145019	40.930189
3520.093930	480216.786713	40.935194
3520.096888	479997.572664	40.940199
3520.296856	479769.127654	40.945204
3520.122875	479552.158476	40.950208
3520.268052	479313.759998	40.955213
3520.210554	479081.959233	40.960218
3520.056049	478853.960477	40.965223
3520.057504	478615.068488	40.970228
3519.953720	478384.224961	40.975232
3520.081214	478134.945681	40.980237
3519.921653	477892.631203	40.985242
3519.379580	477656.235336	40.990247
3519.582180	477420.781464	40.995252
3519.238650	477173.834839	41.000256
3519.416471	476932.969567	41.005261
3519.248781	476706.913334	41.010266
3519.133285	476462.851807	41.015271
3518.999691	476227.938147	41.020276
3518.628835	475990.277916	41.025280
3519.011317	475743.196260	41.030285
3518.486826	475507.423039	41.035290
3517.828313	475270.959536	41.040295
3518.298505	475035.176260	41.045300
3517.703889	474810.524612	41.050304
3517.002331	474572.035548	41.055309
3517.429397	474361.423448	41.060314
3517.177956	474137.972829	41.065319
3517.019669	473913.190253	41.070324
3516.962099	473699.864552	41.075328
3516.924594	473482.185256	41.080333
3516.336438	473254.224963	41.085338
3516.664649	473039.768899	41.090343
3516.665984	472819.445785	41.095348
3516.234569	472615.668605	41.100352
3516.132600	472390.805639	41.105357
3515.678055	472188.796236	41.110362
3515.637981	471972.765570	41.115367
3515.291809	471769.520697	41.120372
3515.332039	471576.982487	41.125376
3514.887237	471365.961678	41.130381
3514.916936	471182.268604	41.135386
3514.362728	470980.664269	41.140391
3514.605872	470786.264956	41.145396
3514.053401	470596.891779	41.150400
3514.162004	470417.677990	41.155405
3514.016355	470227.832743	41.160410
3513.716510	470040.133025	41.165415
3513.804944	469850.651520	41.170420
3513.407340	469685.717428	41.175424
3513.491463	469492.642294	41.180429
3513.570351	469333.597388	41.185434
3513.097778	469150.212618	41.190439
3512.874583	468977.608595	41.195444
3512.660203	468810.058267	41.200448
3512.676648	468636.300881	41.205453
3512.505570	468472.887076	41.210458
3512.496574	468311.620956	41.215463
3512.619403	468138.853206	41.220468
3512.286686	467983.753330	41.225472
3512.324026	467824.042970	41.230477
3512.007186	467657.255513	41.235482
3511.655390	467500.181777	41.240487
3511.727780	467339.298137	41.245492
3511.220344	467189.882236	41.250496
3511.396000	467028.372641	41.255501
3511.015567	466888.442200	41.260506
3510.697914	466745.972069	41.265511
3510.755387	466611.433256	41.270516
3510.602305	466464.383330	41.275520
3511.056319	466328.971325	41.280525
3510.639837	466182.617401	41.285530
3510.433665	466046.648348	41.290535
3510.399853	465900.991069	41.295540
3510.405375	465775.254101	41.300544
3510.370401	465621.451533	41.305549
3510.110520	465489.077377	41.310554
3510.065436	465370.325115	41.315559
3510.219843	465228.628459	41.320564
3509.974886	465108.286903	41.325568
3510.160218	464966.684387	41.330573
3509.908579	464834.404952	41.335578
3509.840559	464709.177258	41.340583
3509.878130	464578.671728	41.345588
3509.398395	464445.413102	41.350592
3509.540512	464328.293559	41.355597
3508.961202	464201.371277	41.360602
3508.823415	464080.449292	41.365607
3509.270667	463960.295318	41.370612
3508.928030	463852.099988	41.375616
3508.882360	463725.799262	41.380621
3508.795762	463610.683113	41.385626
3508.365823	463502.600301	41.390631
3508.711812	463386.049522	41.395636
3508.680204	463283.973534	41.400640
3508.342749	463171.523875	41.405645
3508.402978	463064.626634	41.410650
3507.781857	462963.753346	41.415655
3508.241699	462852.442160	41.420660
3508.378129	462753.675551	41.425664
3508.365934	462638.945923	41.430669
3508.424958	462531.843167	41.435674
3507.919879	462433.579226	41.440679
3507.861934	462323.103968	41.445684
3507.708819	462228.477011	41.450688
3507.522625	462130.212283	41.455693
3507.738357	462024.650203	41.460698
3507.736266	461926.355650	41.465703
3507.577008	461830.057986	41.470708
3507.260593	461740.968007	41.475712
3507.569431	461646.367113	41.480717
3507.130106	461555.322272	41.485722
3507.073147	461474.285004	41.490727
3507.392728	461374.773632	41.495732
3507.084901	461287.703592	41.500736
3507.231142	461185.890896	41.505741
3507.390955	461101.428491	41.510746
3506.650941	461016.751550	41.515751
3506.767105	460921.873078	41.520756
3506.404513	460841.386295	41.525760
3506.482576	460758.149141	41.530765
3506.678764	460671.604650	41.535770
3506.610798	460597.749164	41.540775
3506.699717	460514.610325	41.545780
3506.610902	460431.852899	41.550784
3506.558802	460348.077478	41.555789
3506.621369	460265.295692	41.560794
3506.326949	460189.804077	41.565799
3506.481876	460110.751168	41.570804
3506.436358	460028.642792	41.575808
3506.565920	459944.482970	41.580813
3506.191166	459874.365566	41.585818
3506.045626	459793.384732	41.590823
3506.415526	459721.481170	41.595828
3506.341159	459642.107618	41.600832
3506.395090	459564.383415	41.605837
3506.249448	459490.585856	41.610842
3506.154952	459409.595274	41.615847
3506.340633	459331.849521	41.620852
3505.912347	459261.484965	41.625856
3505.723526	459174.588077	41.630861
3505.937738	459110.447613	41.635866
3505.685726	459043.495380	41.640871
3505.992388	458974.179037	41.645876
3505.826786	458908.022403	41.650880
3505.884169	458835.607200	41.655885
3506.080163	458760.791985	41.660890
3505.548330	458686.393299	41.665895
3505.944603	458609.724703	41.670900
3505.714771	458543.779066	41.675904
3505.643340	458472.495575	41.680909
3505.649877	458405.804236	41.685914
3505.578830	458341.604111	41.690919
3505.454360	458263.851219	41.695924
3505.570069	458197.799893	41.700928
3505.588291	458128.676851	41.705933
3505.651568	458058.433306	41.710938
3505.130382	458001.133070	41.715943
3505.421479	457929.790933	41.720948
3505.032693	457870.293811	41.725952
3505.166263	457807.780314	41.730957
3505.402274	457752.385487	41.735962
3504.974966	457692.286530	41.740967
3505.662396	457625.688644	41.745972
3505.308630	457572.054886	41.750976
3505.509586	457505.633447	41.755981
3505.231218	457445.156241	41.760986
3505.023594	457383.655761	41.765991
3505.486784	457312.739736	41.770996
3505.718008	457266.047811	41.776000
3505.220500	457189.309615	41.781005
3505.156143	457130.923352	41.786010
3504.710630	457065.359883	41.791015
3505.226371	457001.012888	41.796020
3505.088773	456949.519537	41.801024
3505.112932	456888.588488	41.806029
3505.039776	456826.862699	41.811034
3504.721388	456771.399210	41.816039
3504.894906	456704.017499	41.821044
3504.870410	456657.515551	41.826048
3504.772796	456606.318594	41.831053
3504.820386	456549.127482	41.836058
3504.980040	456499.003490	41.841063
3505.099213	456443.470868	41.846068
3504.685420	456385.136485	41.851072
3504.732100	456329.766600	41.856077
3505.188599	456266.994901	41.861082
3504.962998	456217.891566	41.866087
3505.367276	456147.890889	41.871092
3505.067294	456093.130869	41.876096
3505.061911	456027.596223	41.881101
3505.257883	455974.631102	41.886106
3504.838572	455915.992371	41.891111
3504.857120	455852.325803	41.896116
3504.817629	455800.915014	41.901120
3504.723281	455743.186674	41.906125
3504.755692	455687.563940	41.911130
3504.500608	455631.125435	41.916135
3504.821063	455577.836098	41.921140
3504.584814	455521.242484	41.926144
3504.842275	455461.332929	41.931149
3504.815293	455404.099072	41.936154
3505.063574	455363.421822	41.941159
3505.122260	455292.762990	41.946164
3504.862785	455246.850557	41.951168
3504.577298	455187.530647	41.956173
3504.418523	455134.770021	41.961178
3504.525893	455082.777572	41.966183
3504.670680	455027.489526	41.971188
3504.383312	454978.038062	41.976192
3504.347807	454927.383239	41.981197
3504.409984	454875.042940	41.986202
3504.571194	454827.039546	41.991207
3504.559064	454772.382438	41.996212
3504.518679	454717.527116	42.001216
3504.500224	454672.031170	42.006221
3504.541115	454614.278074	42.011226
3504.400758	454567.434338	42.016231
3504.300573	454518.762228	42.021236
3504.631522	454472.401618	42.026240
3504.220732	454416.793220	42.031245
3504.617210	454361.514529	42.036250
3503.982539	454312.216460	42.041255
3504.446279	454264.619963	42.046260
3504.325041	454217.924157	42.051264
3504.310676	454173.843421	42.056269
3504.362700	454122.615932	42.061274
3503.867422	454072.839992	42.066279
3504.004871	454013.905823	42.071284
3504.131983	453988.731663	42.076288
3503.949369	453935.667480	42.081293
3504.175380	453902.885902	42.086298
3504.117724	453865.998150	42.091303
3504.288581	453806.551961	42.096308
3504.133868	453772.715900	42.101312
3503.923517	453723.653835	42.106317
3504.356500	453670.391834	42.111322
3504.430252	453643.757697	42.116327
3504.195862	453580.830864	42.121332
3504.684794	453539.555209	42.126336
3504.396078	453487.569081	42.131341
3504.256010	453430.548870	42.136346
3503.750396	453384.872345	42.141351
3503.950515	453337.567448	42.146356
3504.120993	453312.031278	42.151360
3504.127908	453261.162614	42.156365
3504.161488	453214.541295	42.161370
3503.847269	453177.793262	42.166375
3504.345494	453122.292408	42.171380
3504.475894	453082.691163	42.176384
3504.330937	453034.578699	42.181389
3504.130101	452988.296955	42.186394
3504.180898	452941.267316	42.191399
3504.239280	452885.176164	42.196404
3504.062489	452838.789057	42.201408
3503.978688	452791.375039	42.206413
3504.387272	452742.416406	42.211418
3503.997048	452698.896647	42.216423
3503.990304	452654.406014	42.221428
3504.039850	452608.134932	42.226432
3504.017720	452572.605604	42.231437
3504.041892	452530.843145	42.236442
3503.872015	452493.311981	42.241447
3504.224020	452441.476166	42.246452
3504.186136	452402.557613	42.251456
3503.864632	452358.570773	42.256461
3504.135189	452314.339840	42.261466
3504.043874	452263.635457	42.266471
3504.194399	452221.295818	42.271476
3504.270653	452170.463859	42.276480
3504.135183	452117.336280	42.281485
3504.068183	452083.432729	42.286490
3504.277467	452032.630294	42.291495
3504.012314	451988.481915	42.296500
3504.118032	451949.388171	42.301504
3503.833438	451906.609310	42.306509
3504.341958	451862.795794	42.311514
3503.805506	451817.727456	42.316519
3503.604177	451777.668741	42.321524
3503.812623	451735.521410	42.326528
3503.831523	451692.087380	42.331533
3503.618771	451651.321491	42.336538
3503.741821	451621.183927	42.341543
3504.136047	451570.402016	42.346548
3503.990278	451534.383663	42.351552
3503.781842	451483.239710	42.356557
3503.977266	451435.728012	42.361562
3503.400362	451396.536802	42.366567
3503.649249	451346.789271	42.371572
3503.984990	451317.883600	42.376576
3503.936918	451274.914559	42.381581
3503.976485	451236.386371	42.386586
3503.768647	451204.983466	42.391591
3503.959431	451158.028577	42.396596
3503.758180	451129.155544	42.401600
3503.623603	451078.606388	42.406605
3503.980547	451039.572801	42.411610
3503.790915	451002.294677	42.416615
3503.781033	450952.738182	42.421620
3503.748515	450910.069572	42.426624
3503.664162	450875.103380	42.431629
3503.580984	450828.190259	42.436634
3503.725744	450801.743309	42.441639
3503.794202	450755.160751	42.446644
3503.979007	450715.798894	42.451648
3503.976532	450675.858631	42.456653
3504.144433	450633.664394	42.461658
3503.690019	450599.008360	42.466663
3503.780021	450558.192867	42.471668
3503.509329	450510.295647	42.476672
3503.515712	450467.468062	42.481677
3503.768551	450432.499159	42.486682
3503.279740	450392.482076	42.491687
3503.539899	450347.235443	42.496692
3503.347811	450318.359677	42.501696
3503.194914	450290.490226	42.506701
3503.451902	450250.711133	42.511706
3503.002573	450216.357306	42.516711
3503.543284	450189.290983	42.521716
3503.740198	450160.607546	42.526720
3503.641833	450117.896675	42.531725
3503.792339	450079.956221	42.536730
3503.641484	450042.771316	42.541735
3503.496812	450016.773239	42.546740
3503.304571	449965.521186	42.551744
3503.477053	449928.994465	42.556749
3503.271697	449896.120782	42.561754
3503.380342	449872.108044	42.566759
3503.187438	449832.651156	42.571764
3503.482641	449801.066264	42.576768
3503.332018	449767.778834	42.581773
3503.560034	449735.343665	42.586778
3503.169600	449697.486582	42.591783
3503.008992	449656.252417	42.596788
3503.082486	449644.091052	42.601792
3503.305040	449608.619013	42.606797
3503.692568	449565.122468	42.611802
3503.336450	449531.917205	42.616807
3503.961274	449504.128014	42.621812
3503.786034	449465.983831	42.626816
3502.887275	449420.560834	42.631821
3503.428965	449379.318000	42.636826
3503.276928	449356.712032	42.641831
3503.289607	449318.740798	42.646836
3503.264469	449289.229890	42.651840
3502.904017	449263.821189	42.656845
3503.476316	449229.407750	42.661850
3503.202319	449196.847228	42.666855
3503.552748	449154.266738	42.671860
3503.401247	449131.457899	42.676864
3502.991299	449091.628153	42.681869
3503.309089	449053.254497	42.686874
3502.979717	449028.498772	42.691879
3503.223751	448989.326431	42.696884
3503.116446	448963.624780	42.701888
3503.043029	448936.449640	42.706893
3503.229333	448909.790940	42.711898
3503.671955	448877.371462	42.716903
3503.649966	448835.455699	42.721908
3503.518289	448795.683252	42.726912
3503.260087	448761.195650	42.731917
3503.128992	448720.258518	42.736922
3503.407979	448700.166655	42.741927
3503.392896	448666.248571	42.746932
3503.515063	448634.384801	42.751936
3502.785552	448597.691982	42.756941
3503.482973	448570.396341	42.761946
3503.473456	448543.666318	42.766951
3503.431020	448513.853069	42.771956
3503.595431	448475.147659	42.776960
3503.205993	448436.173954	42.781965
3503.303476	448396.972510	42.786970
3503.368955	448368.559822	42.791975
3503.149634	448338.318153	42.796980
3503.241584	448300.585588	42.801985
3503.165961	448273.460425	42.806989
3503.708441	448234.999442	42.811994
3503.471109	448201.520103	42.816999
3502.886232	448158.222126	42.822004
3503.443624	448135.301718	42.827009
3503.223866	448093.718788	42.832013
3503.334730	448060.033116	42.837018
3503.233516	448031.747099	42.842023
3503.307060	447996.801383	42.847028
3503.367459	447964.591642	42.852033
3502.991626	447941.158027	42.857037
3503.225329	447903.453207	42.862042
3503.135986	447877.595330	42.867047
3503.049639	447843.129868	42.872052
3503.623879	447810.941154	42.877057
3503.107178	447785.706579	42.882061
3503.427941	447735.279711	42.887066
3502.966268	447715.150125	42.892071
3503.440742	447680.090780	42.897076
3503.158753	447641.706210	42.902081
3503.103095	447618.272985	42.907085
3503.446205	447582.474436	42.912090
3503.342328	447555.150073	42.917095
3503.375726	447510.640463	42.922100
3503.532133	447472.237946	42.927105
3503.222517	447431.528209	42.932109
3503.501013	447407.181985	42.937114
3503.201946	447382.014243	42.942119
3503.189778	447350.118494	42.947124
3503.563234	447316.441213	42.952129
3503.659553	447279.566583	42.957133
3503.619660	447249.902757	42.962138
3503.436951	447210.995514	42.967143
3503.461061	447178.081184	42.972148
3503.529598	447134.830981	42.977153
3503.312175	447104.283170	42.982157
3503.300815	447062.918612	42.987162
3503.467743	447024.412251	42.992167
3503.434750	446990.544457	42.997172
3503.640897	446960.841874	43.002177
3503.901038	446927.839731	43.007181
3503.849116	446883.848191	43.012186
3503.591586	446849.761913	43.017191
3503.494514	446800.106337	43.022196
3503.448833	446764.569215	43.027201
3503.346343	446725.749719	43.032205
3503.341903	446690.611100	43.037210
3503.418211	446665.839653	43.042215
3503.465361	446632.211889	43.047220
3503.368491	446593.492503	43.052225
3503.072450	446564.019322	43.057229
3503.186344	446541.722898	43.062234
3503.085752	446510.447042	43.067239
3502.904373	446470.626607	43.072244
3502.928211	446439.128731	43.077249
3502.652674	446420.994098	43.082253
3503.043104	446389.135287	43.087258
3503.093270	446353.835622	43.092263
3503.232111	446320.901893	43.097268
3503.216835	446284.751497	43.102273
3503.073056	446264.824008	43.107277
3503.202797	446225.663505	43.112282
3503.186456	446206.475637	43.117287
3503.319763	446167.162551	43.122292
3503.221600	446134.518541	43.127297
3503.147499	446104.351831	43.132301
3503.142892	446063.439672	43.137306
3503.080350	446050.284376	43.142311
3502.943400	446007.974910	43.147316
3502.771669	445979.392872	43.152321
3502.727195	445947.550335	43.157325
3503.145833	445920.344756	43.162330
3503.181879	445899.325544	43.167335
3503.133249	445871.433076	43.172340
3503.020418	445840.208614	43.177345
3502.715047	445811.950923	43.182349
3503.100356	445789.459441	43.187354
3502.589046	445767.411271	43.192359
3502.812969	445729.197130	43.197364
3502.788568	445709.554273	43.202369
3503.013772	445686.226771	43.207373
3503.138128	445655.218264	43.212378
3502.803471	445629.699192	43.217383
3503.022444	445591.789351	43.222388
3503.743975	445566.865378	43.227393
3503.321812	445537.511441	43.232397
3503.395856	445496.332597	43.237402
3503.519071	445471.096508	43.242407
3502.990492	445430.365746	43.247412
3502.981544	445388.541299	43.252417
3502.883751	445372.605983	43.257421
3502.929385	445327.177692	43.262426
3502.898465	445307.484783	43.267431
3503.059707	445285.584560	43.272436
3503.100294	445252.866752	43.277441
3503.109493	445227.091063	43.282445
3502.711029	445195.707405	43.287450
3502.695754	445170.897552	43.292455
3503.034706	445142.538565	43.297460
3502.954122	445117.485617	43.302465
3503.223480	445096.581094	43.307469
3503.001345	445063.245544	43.312474
3502.896258	445046.197052	43.317479
3502.787330	445003.678361	43.322484
3503.148769	444976.581563	43.327489
3502.460615	444952.281227	43.332493
3502.711907	444916.036017	43.337498
3502.719222	444900.134572	43.342503
3502.650236	444871.079077	43.347508
3503.134602	444849.381244	43.352513
3502.789532	444824.622245	43.357517
3502.944885	444797.050871	43.362522
3503.032100	444772.275171	43.367527
3502.875889	444738.827499	43.372532
3502.835249	444704.551563	43.377537
3503.102589	444685.064769	43.382541
3503.007504	444648.012075	43.387546
3502.758004	444620.554076	43.392551
3502.932655	444608.474891	43.397556
3502.640646	444567.452208	43.402561
3502.589066	444547.204672	43.407565
3502.354975	444517.718561	43.412570
3502.714833	444511.231432	43.417575
3502.706172	444485.406845	43.422580
3502.957280	444459.997552	43.427585
3502.929845	444439.442305	43.432589
3502.997515	444411.884000	43.437594
3502.697394	444381.850913	43.442599
3503.101396	444353.379312	43.447604
3503.013013	444324.731091	43.452609
3502.596139	444295.273067	43.457613
3502.754000	444270.536340	43.462618
3503.015930	444247.910260	43.467623
3503.262731	444226.755063	43.472628
3503.226253	444189.388489	43.477633
3502.945758	444158.491104	43.482637
3502.999699	444115.641180	43.487642
3502.837780	444099.714741	43.492647
3503.231338	444071.193691	43.497652
3502.623200	444036.042658	43.502657
3502.468496	444020.520151	43.507661
3502.698013	443985.947640	43.512666
3502.960214	443965.397435	43.517671
3503.101440	443932.053937	43.522676
3503.171908	443908.495062	43.527681
3502.517373	443891.986771	43.532685
3502.636976	443860.013810	43.537690
3502.725856	443842.376971	43.542695
3502.888518	443814.144661	43.547700
3502.601897	443784.159142	43.552705
3502.446757	443776.485869	43.557709
3502.638180	443736.095088	43.562714
3502.839395	443717.123976	43.567719
3502.578517	443699.338863	43.572724
3502.727247	443675.413024	43.577729
3502.284509	443649.705459	43.582733
3502.628811	443627.217727	43.587738
3502.696506	443599.607567	43.592743
3502.564541	443576.991320	43.597748
3502.840116	443561.097621	43.602753
3502.782944	443537.203644	43.607757
3502.633622	443509.171344	43.612762
3502.576256	443483.049085	43.617767
3502.830123	443463.461818	43.622772
3503.131692	443424.369910	43.627777
3502.272573	443413.109160	43.632781
3502.223134	443378.984063	43.637786
3502.498281	443379.650274	43.642791
3502.862398	443346.321681	43.647796
3502.974669	443322.907484	43.652801
3503.008427	443293.377738	43.657805
3502.575350	443265.794365	43.662810
3502.751584	443240.952120	43.667815
3503.066143	443214.265181	43.672820
3502.830860	443182.802061	43.677825
3502.063386	443176.692466	43.682829
3502.477037	443152.471514	43.687834
3502.499481	443138.591915	43.692839
3502.323840	443111.727895	43.697844
3502.555428	443091.333416	43.702849
3502.612947	443077.093811	43.707853
3502.536238	443047.783437	43.712858
3502.532543	443019.879665	43.717863
3502.153618	443008.746516	43.722868
3502.799170	442992.693472	43.727873
3502.572422	442971.205388	43.732877
3502.620556	442934.734697	43.737882
3502.369569	442922.467432	43.742887
3502.572880	442898.430812	43.747892
3502.588364	442864.446597	43.752897
3502.889194	442853.005001	43.757901
3502.875888	442834.724739	43.762906
3502.852160	442804.139644	43.767911
3502.454875	442775.638384	43.772916
3502.556468	442751.769334	43.777921
3502.490773	442738.814742	43.782925
3502.886516	442711.152213	43.787930
3502.650897	442682.980162	43.792935
3502.600098	442660.299524	43.797940
3502.857298	442628.809473	43.802945
3502.706966	442618.501470	43.807949
3502.563006	442582.363847	43.812954
3502.660803	442570.447229	43.817959
3502.677584	442546.084669	43.822964
3502.343859	442513.470911	43.827969
3502.376821	442502.982387	43.832973
3502.491096	442479.921330	43.837978
3502.520454	442460.064076	43.842983
3502.520968	442443.807068	43.847988
3502.602179	442418.826579	43.852993
3502.643728	442406.867965	43.857997
3502.369917	442377.435271	43.863002
3502.665367	442355.814571	43.868007
3502.793317	442332.447333	43.873012
3502.660682	442301.574489	43.878017
3502.639942	442284.206456	43.883021
3502.556456	442254.490726	43.888026
3502.434000	442241.645911	43.893031
3502.563379	442209.314073	43.898036
3502.932274	442196.088895	43.903041
3502.718628	442172.825259	43.908045
3502.894053	442138.257730	43.913050
3502.758012	442115.944213	43.918055
3502.333194	442087.547473	43.923060
3502.897054	442065.631441	43.928065
3502.474796	442047.819211	43.933069
3502.906415	442016.452924	43.938074
3502.822148	442008.362723	43.943079
3502.711388	441979.106611	43.948084
3502.823512	441949.005433	43.953089
3502.446264	441919.689405	43.958093
3502.591513	441885.278042	43.963098
3502.538262	441879.715273	43.968103
3502.433306	441858.916000	43.973108
3502.926491	441843.999903	43.978113
3502.602093	441828.501969	43.983117
3503.078883	441798.394448	43.988122
3502.858375	441769.661552	43.993127
3502.638767	441737.383203	43.998132
3502.607262	441717.990452	44.003137
3502.785097	441690.816143	44.008141
3502.663927	441658.826221	44.013146
3502.521067	441649.276222	44.018151
3502.569882	441626.274944	44.023156
3502.792322	441596.257325	44.028161
3502.691864	441580.420455	44.033165
3502.628406	441544.673471	44.038170
3502.801874	441524.488914	44.043175
3502.735562	441499.682094	44.048180
3502.773848	441471.566883	44.053185
3502.676993	441457.248770	44.058189
3503.070521	441424.418643	44.063194
3502.979102	441401.844092	44.068199
3502.741261	441378.988412	44.073204
3502.859003	441344.630984	44.078209
3502.408841	441325.049734	44.083213
3502.535769	441298.490551	44.088218
3502.717025	441280.178490	44.093223
3502.603077	441253.808671	44.098228
3502.928685	441221.596535	44.103233
3502.667921	441197.477998	44.108237
3502.319100	441174.993876	44.113242
3502.393512	441154.013963	44.118247
3502.352641	441138.521985	44.123252
3502.820014	441120.266541	44.128257
3502.562051	441096.653923	44.133261
3502.755979	441066.082759	44.138266
3502.569741	441050.815923	44.143271
3502.707131	441026.888452	44.148276
3502.671038	440996.606213	44.153281
3502.549877	440969.831927	44.158285
3502.449096	440955.514041	44.163290
3502.597594	440939.030102	44.168295
3502.272019	440919.783582	44.173300
3502.660070	440889.181923	44.178305
3502.569009	440870.253402	44.183309
3502.221219	440840.475255	44.188314
3502.552631	440832.421159	44.193319
3502.285646	440810.278408	44.198324
3502.612954	440786.878219	44.203329
3502.626561	440763.628115	44.208333
3502.952508	440743.824186	44.213338
3502.780955	440714.018414	44.218343
3502.674100	440697.016855	44.223348
3502.745768	440668.439400	44.228353
3502.976569	440653.107344	44.233357
3502.617219	440625.508588	44.238362
3502.564769	440597.406187	44.243367
3502.519688	440573.759783	44.248372
3502.774972	440535.631383	44.253377
3502.334069	440538.536425	44.258381
3502.430625	440505.548306	44.263386
3502.831980	440488.467475	44.268391
3502.886912	440470.680784	44.273396
3502.991266	440441.287496	44.278401
3502.863618	440415.273182	44.283405
3502.931512	440378.541181	44.288410
3502.917009	440365.273076	44.293415
3502.828133	440342.848806	44.298420
3502.786026	440307.146792	44.303425
3502.505675	440293.413500	44.308429
3502.882711	440257.798121	44.313434
3502.940628	440229.677996	44.318439
3502.696639	440204.289303	44.323444
3502.758006	440177.991994	44.328449
3502.486837	440163.345462	44.333453
3502.797219	440133.666379	44.338458
3502.902235	440107.311527	44.343463
3502.798893	440085.902224	44.348468
3502.878903	440053.726306	44.353473
3503.004012	440035.168515	44.358477
3502.811295	440002.325832	44.363482
3502.863797	439978.055677	44.368487
3502.862666	439949.387157	44.373492
3503.212298	439917.979476	44.378497
3502.691696	439897.951831	44.383501
3502.609879	439864.027964	44.388506
3502.804188	439848.397022	44.393511
3502.740835	439824.651216	44.398516
3502.646578	439795.541087	44.403521
3502.471194	439783.867818	44.408525
3502.663507	439749.546523	44.413530
3502.550664	439734.925673	44.418535
3502.620978	439691.607184	44.423540
3502.485333	439682.460278	44.428545
3502.174794	439662.804912	44.433549
3502.500391	439644.570104	44.438554
3502.252553	439626.880384	44.443559
3502.226495	439612.296586	44.448564
3502.240232	439593.147862	44.453569
3502.061809	439571.850963	44.458573
3502.106932	439557.104088	44.463578
3501.927338	439529.425099	44.468583
3502.223240	439526.086668	44.473588
3502.234363	439503.443228	44.478593
3502.331130	439490.967636	44.483597
3502.319718	439471.518786	44.488602
3502.809983	439453.714046	44.493607
3502.662447	439435.198093	44.498612
3502.838279	439407.666229	44.503617
3502.246669	439394.436593	44.508621
3502.329781	439365.652771	44.513626
3502.638841	439337.745501	44.518631
3502.528326	439321.958946	44.523636
3502.635374	439300.262745	44.528641
3502.471605	439279.317809	44.533645
3502.573174	439263.346242	44.538650
3502.512983	439232.406423	44.543655
3502.348111	439223.263842	44.548660
3502.751267	439191.238784	44.553665
3502.307157	439182.240943	44.558669
3502.493965	439145.842614	44.563674
3502.523691	439126.994852	44.568679
3502.537029	439109.517273	44.573684
3502.467874	439093.014938	44.578689
3502.448720	439070.730267	44.583693
3502.612087	439055.913947	44.588698
3502.571406	439026.085141	44.593703
3502.539396	439015.554127	44.598708
3502.916257	438992.498583	44.603713
3502.402353	438972.164987	44.608717
3502.448501	438949.262162	44.613722
3502.537163	438929.442603	44.618727
3502.282456	438908.916641	44.623732
3502.508942	438889.126247	44.628737
3502.156908	438865.221541	44.633741
3502.172365	438838.271004	44.638746
3502.124662	438829.464582	44.643751
3502.496803	438810.613876	44.648756
3502.577424	438797.279213	44.653761
3502.308325	438773.260176	44.658765
3502.166427	438741.724413	44.663770
3502.483969	438731.746704	44.668775
3502.318141	438709.687052	44.673780
3502.360959	438691.697952	44.678785
3502.751397	438672.894918	44.683789
3502.693424	438643.625404	44.688794
3502.524097	438624.200258	44.693799
3502.603323	438609.295373	44.698804
3502.793354	438583.026479	44.703809
3502.346340	438561.516962	44.708813
3502.412918	438535.267213	44.713818
3502.489859	438516.208876	44.718823
3502.102983	438493.068952	44.723828
3502.263823	438484.179262	44.728833
3502.749004	438458.218855	44.733837
3502.577626	438435.045326	44.738842
3502.679026	438408.941950	44.743847
3502.547750	438400.654890	44.748852
3502.509858	438369.608881	44.753857
3502.490259	438349.957531	44.758861
3502.463425	438326.457442	44.763866
3502.632393	438304.801123	44.768871
3502.338801	438282.659545	44.773876
3502.355153	438267.004336	44.778881
3502.196550	438247.070574	44.783885
3502.281601	438228.365279	44.788890
3502.466490	438212.379862	44.793895
3502.243553	438192.000148	44.798900
3502.411465	438169.837278	44.803905
3502.079268	438149.879771	44.808909
3502.002070	438143.357154	44.813914
3502.556729	438127.618063	44.818919
3502.293735	438107.092523	44.823924
3502.034236	438087.427576	44.828929
3502.401942	438065.233494	44.833933
3502.528975	438050.675328	44.838938
3502.350207	438027.451795	44.843943
3502.286606	438016.418576	44.848948
3502.375116	437989.050213	44.853953
3502.106814	437973.033804	44.858957
3502.441850	437954.238682	44.863962
3502.403365	437930.486632	44.868967
3502.185001	437922.770141	44.873972
3502.211021	437898.248159	44.878977
3501.993912	437886.276270	44.883981
3502.150947	437876.272433	44.888986
3502.317104	437852.387128	44.893991
3502.105151	437836.209863	44.898996
3502.480773	437819.991808	44.904001
3502.304062	437801.377484	44.909005
3502.151986	437786.710577	44.914010
3502.186852	437761.072582	44.919015
3502.274399	437759.184673	44.924020
3502.531173	437740.756121	44.929025
3502.097692	437724.461262	44.934029
3502.311035	437711.763732	44.939034
3502.930084	437681.526207	44.944039
3502.425095	437670.409500	44.949044
3502.380039	437642.352217	44.954049
3502.613715	437627.371871	44.959053
3502.567600	437610.155454	44.964058
3502.714056	437579.434073	44.969063
3502.501729	437557.025714	44.974068
3502.523387	437540.355924	44.979073
3502.093828	437515.347107	44.984077
3502.467285	437501.712677	44.989082
3502.397755	437474.621459	44.994087
3502.235299	437465.882919	44.999092
3502.678134	437431.265161	45.004097
3502.454632	437422.485443	45.009101
3502.706087	437391.139521	45.014106
3502.708585	437371.787673	45.019111
3502.377691	437358.819990	45.024116
3502.749421	437332.065171	45.029121
3502.673460	437306.494470	45.034125
3502.686383	437280.251341	45.039130
3502.939335	437258.124838	45.044135
3502.649796	437235.728116	45.049140
3502.665147	437208.116724	45.054145
3502.400083	437184.753616	45.059149
3502.274921	437161.622003	45.064154
3502.726765	437135.158397	45.069159
3502.555953	437131.790859	45.074164
3502.647554	437106.092497	45.079169
3502.634041	437082.994075	45.084173
3502.455006	437054.196889	45.089178
3502.549090	437031.385616	45.094183
3502.385841	437018.999525	45.099188
3502.594447	436992.218957	45.104193
3502.347242	436976.755679	45.109197
3501.966544	436956.095236	45.114202
3502.375969	436941.188323	45.119207
3502.323882	436921.084620	45.124212
3502.598840	436901.183302	45.129217
3502.369270	436882.728285	45.134221
3502.312587	436862.219958	45.139226
3502.371728	436832.524159	45.144231
3501.994718	436830.657790	45.149236
3502.476169	436811.281504	45.154241
3502.341140	436786.073917	45.159245
3502.122423	436771.213960	45.164250
3502.588046	436748.597834	45.169255
3502.270761	436732.841304	45.174260
3502.365179	436702.379913	45.179265
3502.430939	436680.383192	45.184269
3502.289732	436671.894283	45.189274
3502.441122	436646.135339	45.194279
3502.215616	436637.000948	45.199284
3502.307947	436608.971430	45.204289
3502.375560	436599.842069	45.209293
3502.379677	436580.742471	45.214298
3502.599605	436554.871418	45.219303
3502.114083	436545.828106	45.224308
3502.282753	436517.786575	45.229313
3502.465325	436504.687748	45.234317
3502.283409	436490.379113	45.239322
3502.268416	436460.643614	45.244327
3501.994926	436451.516601	45.249332
3502.137684	436428.190428	45.254337
3502.167560	436420.384037	45.259341
3501.774963	436400.839384	45.264346
3502.281017	436376.747361	45.269351
3502.202468	436375.543756	45.274356
3502.080806	436349.776244	45.279361
3502.046774	436331.948862	45.284365
3501.997165	436333.932403	45.289370
3502.417820	436309.650941	45.294375
3502.314647	436294.012715	45.299380
3502.652635	436275.418132	45.304385
3502.368658	436255.856429	45.309389
3501.922988	436243.007170	45.314394
3502.298925	436220.049749	45.319399
3502.375018	436216.643628	45.324404
3502.458650	436188.564188	45.329409
3502.100194	436167.038184	45.334413
3501.964344	436157.433658	45.339418
3502.225490	436140.725382	45.344423
3502.097174	436125.648209	45.349428
3502.428441	436107.409142	45.354433
3502.319257	436082.855211	45.359437
3502.328757	436074.798541	45.364442
3502.568189	436049.177082	45.369447
3502.146684	436027.255437	45.374452
3502.619030	436000.787078	45.379457
3502.446789	435990.681511	45.384461
3502.113579	435976.244049	45.389466
3502.321102	435944.649289	45.394471
3502.219316	435933.215512	45.399476
3502.244513	435912.085481	45.404481
3502.414542	435891.794148	45.409485
3502.117972	435872.993948	45.414490
3502.380638	435861.098116	45.419495
3502.224859	435845.113073	45.424500
3502.281723	435824.332654	45.429505
3502.319142	435816.271532	45.434509
3502.572561	435794.953870	45.439514
3502.313182	435777.667666	45.444519
3502.218822	435755.745465	45.449524
3502.081098	435734.184627	45.454529
3502.226300	435735.631288	45.459533
3502.158328	435707.169434	45.464538
3502.284584	435699.398415	45.469543
3502.216606	435670.075239	45.474548
3501.920315	435658.570241	45.479553
3502.216651	435655.231074	45.484557
3502.223662	435631.215777	45.489562
3502.196402	435605.077934	45.494567
3502.131653	435606.810591	45.499572
3502.026204	435576.530506	45.504577
3501.995611	435566.655989	45.509581
3502.228170	435549.546344	45.514586
3502.334299	435524.451563	45.519591
3502.336107	435521.310195	45.524596
3502.209376	435501.317947	45.529601
3502.010204	435477.030562	45.534605
3501.720011	435476.011825	45.539610
3501.777003	435459.334727	45.544615
3501.610942	435440.361805	45.549620
3501.974436	435410.008484	45.554625
3502.248578	435418.781321	45.559629
3502.537806	435403.486616	45.564634
3502.445334	435383.894223	45.569639
3502.075546	435375.440310	45.574644
3502.161868	435350.703030	45.579649
3502.288180	435343.691815	45.584653
3502.357436	435322.554281	45.589658
3502.087396	435295.187202	45.594663
3502.479562	435286.006714	45.599668
3502.320433	435255.785142	45.604673
3502.503213	435250.994321	45.609677
3502.166630	435218.875073	45.614682
3502.099623	435200.697126	45.619687
3502.041113	435195.183877	45.624692
3502.233845	435181.829250	45.629697
3502.127023	435161.276244	45.634701
3502.027313	435149.183044	45.639706
3502.044582	435128.205379	45.644711
3502.215331	435116.070070	45.649716
3502.193406	435105.434004	45.654721
3502.417344	435084.626789	45.659725
3502.116879	435074.490029	45.664730
3502.085044	435047.034866	45.669735
3502.094125	435033.708715	45.674740
3502.001799	435020.803651	45.679745
3502.384262	435003.112885	45.684749
3502.347793	434989.287145	45.689754
3502.201516	434974.363858	45.694759
3502.288647	434963.710743	45.699764
3502.440915	434946.663723	45.704769
3502.554854	434926.886752	45.709773
3502.304415	434910.915663	45.714778
3502.423801	434880.244843	45.719783
3502.206526	434873.844240	45.724788
3502.294542	434857.060464	45.729793
3502.254306	434828.086347	45.734797
3502.212723	434813.146644	45.739802
3502.378447	434785.761697	45.744807
3502.044283	434786.320386	45.749812
3502.221304	434759.896284	45.754817
3502.443885	434723.483980	45.759821
3502.244957	434653.343301	45.764826
3502.082070	434537.293542	45.769831
3501.875606	434380.159565	45.774836
3501.688331	434166.325223	45.779841
3500.997415	433914.667651	45.784845
3500.693651	433624.996089	45.789850
3500.404465	433279.125941	45.794855
3499.565758	432890.366916	45.799860
3498.919523	432471.724852	45.804865
3498.031053	431994.078167	45.809869
3497.195948	431489.098382	45.814874
3496.530992	430925.600003	45.819879
3495.531811	430337.914047	45.824884
3494.513187	429703.640267	45.829889
3493.692653	429029.987654	45.834893
3492.493774	428315.724252	45.839898
3491.669212	427557.687628	45.844903
3489.978690	426757.282387	45.849908
3488.817141	425926.552992	45.854913
3487.683832	425060.302002	45.859917
3485.960533	424137.127663	45.864922
3484.785251	423189.137910	45.869927
3483.142471	422207.057874	45.874932
3481.232869	421198.659417	45.879937
3479.783490	420145.623712	45.884941
3477.722259	419052.421022	45.889946
3476.164392	417929.469701	45.894951
3474.423318	416772.612520	45.899956
3472.477329	415597.365914	45.904961
3470.308863	414377.814084	45.909965
3468.084529	413147.956428	45.914970
3466.377431	411866.668455	45.919975
3463.874136	410573.863656	45.924980
3461.505950	409242.053206	45.929985
3459.457055	407900.575284	45.934989
3457.325987	406517.680890	45.939994
3455.348105	405118.035494	45.944999
3452.495677	403689.263680	45.950004
3450.139614	402235.054601	45.955009
3447.810418	400766.438623	45.960013
3445.220647	399271.379959	45.965018
3442.765514	397742.605841	45.970023
3439.937589	396209.527050	45.975028
3437.490008	394655.377118	45.980033
3435.244045	393064.342493	45.985037
3432.230946	391456.315977	45.990042
3429.438198	389832.385438	45.995047
3426.410036	388192.822832	46.000052
3423.527961	386535.891165	46.005057
3420.951359	384871.541667	46.010061
3417.859520	383181.822811	46.015066
3415.267904	381473.606756	46.020071
3412.089870	379759.478431	46.025076
3409.172912	378025.566384	46.030081
3406.076609	376279.911701	46.035085
3403.308932	374518.852961	46.040090
3400.029394	372751.079716	46.045095
3396.993350	370956.812310	46.050100
3393.833304	369160.467636	46.055105
3390.690534	367345.408858	46.060109
3387.250691	365523.091097	46.065114
3384.559119	363688.193630	46.070119
3381.044034	361858.875251	46.075124
3377.856544	359998.720576	46.080129
3374.735553	358133.866803	46.085133
3371.142160	356259.417014	46.090138
3367.886664	354378.828872	46.095143
3364.283559	352489.286427	46.100148
3361.245492	350593.443996	46.105153
3357.823483	348687.229805	46.110157
3354.269033	346786.316314	46.115162
3350.969122	344863.746404	46.120167
3347.857966	342942.106960	46.125172
3343.947287	340998.490772	46.130177
3340.485829	339060.470241	46.135181
3336.953222	337136.800851	46.140186
3333.471863	335181.410676	46.145191
3329.954442	333231.213564	46.150196
3326.309541	331281.673628	46.155201
3323.085497	329320.269431	46.160205
3319.270081	327364.404814	46.165210
3315.829092	325384.067746	46.170215
3311.949164	323419.933523	46.175220
3308.688523	321447.876638	46.180225
3305.150317	319476.026155	46.185229
3301.389789	317491.526745	46.190234
3297.610723	315504.219181	46.195239
3293.928686	313535.664481	46.200244
3289.952065	311542.185944	46.205249
3286.519021	309564.850966	46.210253
3282.517185	307591.723198	46.215258
3279.218107	305592.526172	46.220263
3275.507500	303615.863934	46.225268
3271.931859	301629.969238	46.230273
3268.176295	299643.418427	46.235277
3264.183716	297652.811541	46.240282
3260.646489	295667.333002	46.245287
3256.732709	293674.616463	46.250292
3252.894030	291685.233270	46.255297
3249.192327	289694.772107	46.260301
3245.393933	287719.309164	46.265306
3241.310898	285729.702225	46.270311
3237.405161	283757.677882	46.275316
3233.371109	281774.212553	46.280321
3230.243945	279809.850855	46.285325
3225.798138	277842.002472	46.290330
3222.272787	275868.691035	46.295335
3218.235973	273902.057013	46.300340
3214.380206	271941.969512	46.305345
3210.824072	269984.643849	46.310349
3206.673248	268029.813797	46.315354
3202.881891	266075.652230	46.320359
3198.943312	264122.647298	46.325364
3194.913781	262173.236770	46.330369
3191.127363	260232.463742	46.335373
3187.178434	258299.935177	46.340378
3183.523329	256366.898261	46.345383
3179.222927	254434.137546	46.350388
3175.597449	252507.561404	46.355393
3171.667876	250597.256372	46.360397
3168.421128	248682.468005	46.365402
3164.461601	246761.937924	46.370407
3160.059624	244854.089873	46.375412
3156.302938	242945.385853	46.380417
3152.451268	241040.527047	46.385421
3148.650788	239131.877400	46.390426
3144.434000	237234.181235	46.395431
3140.447809	235346.524745	46.400436
3136.395171	233475.323166	46.405441
3132.707894	231596.188238	46.410445
3128.418632	229739.019864	46.415450
3124.591184	227870.773658	46.420455
3120.822458	226021.083489	46.425460
3116.498936	224173.058542	46.430465
3112.781936	222333.498155	46.435469
3108.610146	220497.577057	46.440474
3104.515090	218668.575923	46.445479
3100.367451	216862.281518	46.450484
3096.674165	215053.580410	46.455489
3092.813331	213248.555970	46.460493
3088.646199	211465.364696	46.465498
3085.088770	209670.145066	46.470503
3080.897650	207886.624726	46.475508
3076.796125	206105.167270	46.480513
3073.068176	204335.662215	46.485517
3068.833627	202579.622806	46.490522
3064.378787	200824.934008	46.495527
3060.497415	199095.743490	46.500532
3056.361799	197360.958485	46.505537
3052.857497	195632.488192	46.510541
3048.625636	193920.935191	46.515546
3044.057579	192212.869731	46.520551
3040.063569	190520.323609	46.525556
3036.143160	188845.234153	46.530561
3032.140035	187169.597250	46.535565
3027.843839	185512.162866	46.540570
3023.661004	183844.883506	46.545575
3019.370981	182209.503762	46.550580
3014.993796	180583.383606	46.555585
3011.239957	178963.586725	46.560589
3006.932024	177363.842699	46.565594
3002.660416	175767.369667	46.570599
2998.854377	174180.377722	46.575604
2994.521463	172626.928908	46.580609
2990.152790	171070.423706	46.585613
2985.711108	169534.915252	46.590618
2981.185950	168006.555233	46.595623
2976.625482	166510.794695	46.600628
2972.584738	165028.300064	46.605633
2968.288790	163544.121314	46.610637
2963.208372	162096.590009	46.615642
2958.926777	160656.387466	46.620647
2954.323898	159242.346936	46.625652
2950.036152	157854.050106	46.630657
2945.700340	156478.621700	46.635661
2940.658327	155125.238060	46.640666
2935.775201	153801.361346	46.645671
2931.165636	152500.240092	46.650676
2926.291030	151219.870029	46.655681
2921.624092	149958.356914	46.660685
2916.525464	148744.838524	46.665690
2911.491213	147547.206002	46.670695
2906.155027	146382.465004	46.675700
2900.944088	145165.789863	46.680705
2896.045131	144065.368412	46.685709
2890.381876	142999.253713	46.690714
2885.137067	141967.743302	46.695719
2880.099321	140977.102586	46.700724
2875.050146	139997.425904	46.705729
2870.752652	139054.281418	46.710733
2865.716455	138139.578513	46.715738
2860.996952	137245.479920	46.720743
2855.993989	136386.543017	46.725748
2851.907769	135545.926315	46.730753
2848.083424	134733.717312	46.735757
2843.234600	133937.495160	46.740762
2838.875601	133152.774614	46.745767
2835.100616	132393.635322	46.750772
2831.000984	131643.362500	46.755777
2827.534462	130907.327452	46.760781
2822.952350	130191.500365	46.765786
2819.203664	129483.849103	46.770791
2815.540446	128787.059149	46.775796
2811.813189	128095.950972	46.780801
2808.070024	127412.475679	46.785805
2804.300682	126749.353817	46.790810
2800.622805	126082.476298	46.795815
2797.078624	125414.278822	46.800820
2793.111627	124756.727327	46.805825
2790.074906	124113.222832	46.810829
2786.400285	123470.819964	46.815834
2782.883327	122831.277204	46.820839
2779.445193	122186.289297	46.825844
2775.672905	121558.036751	46.830849
2772.264587	120923.200928	46.835853
2768.415260	120297.257127	46.840858
2765.120903	119674.581684	46.845863
2761.486425	119044.987766	46.850868
2757.738499	118446.068832	46.855873
2754.529654	117824.783671	46.860877
2750.535415	117211.375110	46.865882
2747.048436	116594.044718	46.870887
2743.619237	115994.212418	46.875892
2739.674490	115388.277589	46.880897
2736.094918	114794.083004	46.885901
2732.290494	114199.716885	46.890906
2728.226947	113616.411900	46.895911
2724.816027	113029.365614	46.900916
2721.019954	112458.714246	46.905921
2717.277487	111886.118321	46.910925
2713.383832	111324.171385	46.915930
2709.367154	110753.047613	46.920935
2705.674114	110196.719595	46.925940
2701.245091	109657.563718	46.930945
2697.823839	109126.039866	46.935949
2693.657978	108604.657936	46.940954
2690.122057	108071.706034	46.945959
2686.452852	107559.657412	46.950964
2682.710719	107045.085253	46.955969
2679.123288	106524.369398	46.960973
2675.310742	106032.794683	46.965978
2671.736628	105518.727906	46.970983
2668.333359	105025.260886	46.975988
2664.153221	104531.108454	46.980993
2660.574553	104032.649518	46.985997
2657.420703	103553.986860	46.991002
2654.152503	103063.578454	46.996007
2650.446217	102580.185615	47.001012
2647.063933	102086.326687	47.006017
2643.674681	101603.051390	47.011021
2640.083356	101117.653926	47.016026
2636.614477	100637.582883	47.021031
2633.368075	100144.240580	47.026036
2629.966743	99660.436787	47.031041
2626.678493	99161.587285	47.036045
2623.397027	98679.673316	47.041050
2620.018561	98179.150105	47.046055
2616.476405	97685.739115	47.051060
2612.675974	97198.488903	47.056065
2609.358846	96704.168584	47.061069
2606.121112	96212.664928	47.066074
2602.824625	95712.892408	47.071079
2599.483235	95232.717818	47.076084
2595.726304	94731.202749	47.081089
2592.620747	94218.030570	47.086093
2589.107639	93731.793637	47.091098
2585.359951	93214.811530	47.096103
2582.475611	92711.833874	47.101108
2578.724220	92210.333642	47.106113
2575.349923	91690.053635	47.111117
2571.967774	91191.676694	47.116122
2568.099300	90676.497312	47.121127
2565.147674	90175.821212	47.126132
2561.357404	89661.625442	47.131137
2558.166174	89136.926880	47.136141
2554.450678	88634.908988	47.141146
2551.117678	88112.766235	47.146151
2547.889591	87601.377316	47.151156
2544.460645	87090.828942	47.156161
2540.868205	86567.165967	47.161165
2537.615060	86053.305249	47.166170
2534.418671	85521.951596	47.171175
2530.709494	84996.950378	47.176180
2527.125096	84467.277164	47.181185
2523.413848	83937.595351	47.186189
2519.707170	83417.576843	47.191194
2516.382899	82889.632653	47.196199
2513.093265	82370.635405	47.201204
2509.316604	81848.674938	47.206209
2505.903872	81314.054445	47.211213
2502.500252	80792.576298	47.216218
2498.957560	80258.669348	47.221223
2495.576324	79730.856796	47.226228
2491.349955	79203.554124	47.231233
2488.708023	78676.408651	47.236237
2485.082634	78153.973087	47.241242
2481.634709	77622.083531	47.246247
2478.571461	77081.470325	47.251252
2475.017486	76546.747998	47.256257
2471.460033	76003.934435	47.261261
2467.840113	75475.136073	47.266266
2464.472251	74929.952509	47.271271
2461.187653	74391.446591	47.276276
2457.383851	73852.118007	47.281281
2453.750275	73309.535777	47.286285
2450.617113	72775.648356	47.291290
2447.310112	72226.053553	47.296295
2443.642007	71680.487994	47.301300
2439.869006	71134.924680	47.306305
2436.619819	70597.607700	47.311309
2432.348614	70048.989372	47.316314
2429.401185	69506.956482	47.321319
2426.134729	68964.210100	47.326324
2422.452395	68421.482703	47.331329
2419.345538	67866.844877	47.336333
2415.551441	67311.551570	47.341338
2412.080471	66765.455690	47.346343
2408.848233	66224.710603	47.351348
2404.992872	65672.249059	47.356353
2402.007979	65115.392499	47.361357
2398.522488	64561.990036	47.366362
2394.670904	64011.944394	47.371367
2391.513277	63462.221719	47.376372
2387.421339	62910.543149	47.381377
2384.312785	62347.915831	47.386381
2380.749418	61801.770833	47.391386
2377.508134	61232.957478	47.396391
2374.251552	60678.380997	47.401396
2370.583829	60133.647289	47.406401
2367.106548	59557.643511	47.411405
2363.748055	59004.777078	47.416410
2360.393578	58441.401925	47.421415
2356.847574	57867.961703	47.426420
2353.059689	57296.304972	47.431425
2349.788676	56732.442800	47.436429
2346.021224	56177.871128	47.441434
2342.501045	55623.134278	47.446439
2338.949389	55049.115265	47.451444
2335.926699	54488.960030	47.456449
2332.460728	53915.932191	47.461453
2329.024493	53347.722455	47.466458
2325.684977	52777.811257	47.471463
2322.118721	52215.441187	47.476468
2318.530358	51638.903860	47.481473
2315.172182	51057.714311	47.486477
2311.755311	50493.040981	47.491482
2307.753067	49908.967489	47.496487
2304.215682	49321.195629	47.501492
2300.570606	48755.629990	47.506497
2297.950504	48184.768614	47.511501
2294.071796	47593.910295	47.516506
2290.282037	47024.255846	47.521511
2286.769229	46445.217969	47.526516
2283.273883	45877.335111	47.531521
2279.969573	45289.396700	47.536525
2276.704136	44717.448643	47.541530
2272.935839	44142.860304	47.546535
2269.787228	43552.463855	47.551540
2266.360253	42974.168299	47.556545
2262.762033	42381.837504	47.561549
2259.067576	41807.482136	47.566554
2255.437015	41221.186035	47.571559
2251.991248	40637.248211	47.576564
2248.511107	40064.991204	47.581569
2245.340357	39473.363626	47.586573
2242.032859	38894.491459	47.591578
2238.305404	38306.380623	47.596583
2235.041311	37710.282837	47.601588
2231.309551	37131.067598	47.606593
2227.936743	36534.715099	47.611597
2224.135183	35947.644031	47.616602
2221.040024	35356.473014	47.621607
2217.284425	34759.221944	47.626612
2213.603421	34180.167860	47.631617
2210.437226	33580.665249	47.636621
2206.989815	33002.164996	47.641626
2203.478505	32405.595527	47.646631
2200.077910	31806.940710	47.651636
2196.351999	31215.730799	47.656641
2192.455607	30613.004656	47.661645
2189.253361	30023.540775	47.666650
2185.610752	29439.010184	47.671655
2182.463782	28842.334492	47.676660
2178.413550	28251.595877	47.681665
2174.983149	27662.387372	47.686669
2171.580166	27079.116180	47.691674
2167.798083	26490.965806	47.696679
2164.520918	25899.319800	47.701684
2161.046330	25303.293090	47.706689
2157.591756	24715.447589	47.711693
2153.966921	24123.496063	47.716698
2150.668315	23528.464003	47.721703
2147.085953	22943.661695	47.726708
2143.246580	22352.879402	47.731713
2140.066351	21762.715285	47.736717
2136.444136	21181.385571	47.741722
2132.749358	20589.854309	47.746727
2129.169342	19994.573164	47.751732
2125.303169	19412.244270	47.756737
2121.945249	18830.797367	47.761741
2118.630253	18252.401259	47.766746
2114.603192	17675.317536	47.771751
2111.316991	17087.666897	47.776756
2107.421940	16507.126880	47.781761
2104.046741	15931.459904	47.786765
2100.460732	15347.572553	47.791770
2096.699217	14790.095496	47.796775
2093.184640	14219.941232	47.801780
2089.408768	13649.480606	47.806785
2085.832986	13079.056628	47.811789
2081.794842	12514.328508	47.816794
2078.082188	11966.835826	47.821799
2074.149104	11404.467246	47.826804
2070.187880	10870.407434	47.831809
2066.046289	10346.150107	47.836813
2060.307629	9872.403630	47.841818
2053.319345	9442.418618	47.846823
2047.759677	9013.151815	47.851828
2042.398401	8622.454070	47.856833
2037.838082	8255.099851	47.861837
2032.910819	7904.610231	47.866842
2028.521847	7575.907403	47.871847
2024.351561	7269.701425	47.876852
2020.427282	6988.018804	47.881857
2016.426101	6696.259724	47.886861
2012.908319	6423.371466	47.891866
2009.221780	6160.495222	47.896871
2005.669658	5911.536127	47.901876
2001.758418	5656.025293	47.906881
1998.453726	5407.575725	47.911885
1994.646000	5173.394727	47.916890
1991.150971	4938.443394	47.921895
1988.398638	4706.907947	47.926900
1984.811820	4480.492543	47.931905
1981.403241	4250.416286	47.936909
1978.228813	4029.894639	47.941914
1974.937471	3799.679287	47.946919
1971.742526	3570.638482	47.951924
1968.695652	3354.952954	47.956929
1965.488642	3112.167876	47.961933
1962.137475	2888.229160	47.966938
1958.176746	2652.946494	47.971943
1955.106723	2418.211732	47.976948
1951.388862	2202.843775	47.981953
1948.307451	1969.031076	47.986957
1945.008808	1750.961328	47.991962
1940.919415	1524.917562	47.996967
1937.388270	1296.616159	48.001972
1933.632665	1089.047560	48.006977
1929.662161	875.323174	48.011981
1926.292600	666.895791	48.016986
1922.204050	478.441758	48.021991
1918.478702	273.228644	48.026996
1913.386934	120.175480	48.032001
1904.031766	96.869159	48.037005
1894.844329	110.077583	48.042010
1888.466978	115.742968	48.047015
1884.930015	114.170635	48.052020
1882.218428	109.049874	48.057025
1880.627526	107.025971	48.062029
1878.486032	104.999176	48.067034
1875.820071	104.813030	48.072039
1872.749490	102.108271	48.077044
1869.616919	108.856831	48.082049
1865.912161	110.486980	48.087053
1862.199468	99.574261	48.092058
1858.894973	97.146353	48.097063
1856.015655	98.182968	48.102068
1852.386222	99.712810	48.107073
1849.340802	97.972233	48.112077
1846.538316	104.321410	48.117082
1842.365227	114.958764	48.122087
1838.737518	101.840371	48.127092
1835.136865	109.114192	48.132097
1832.053351	111.849864	48.137101
1828.696623	109.762276	48.142106
1825.380836	105.899803	48.147111
1822.861137	98.642158	48.152116
1818.711477	103.147761	48.157121
1814.979567	102.947190	48.162125
1812.123526	101.449220	48.167130
1808.345297	103.755187	48.172135
1805.213091	98.734703	48.177140
1801.242167	110.090388	48.182145
1798.141154	102.995984	48.187149
1794.760736	100.959543	48.192154
1790.838356	101.661801	48.197159
1787.518504	101.514157	48.202164
1784.192860	98.788996	48.207169
1780.889482	100.492720	48.212173
1777.650389	99.101827	48.217178
1774.415039	116.695752	48.222183
1771.042195	94.230085	48.227188
1766.801124	106.380775	48.232193
1763.367282	101.976709	48.237197
1760.002674	96.685523	48.242202
1756.344603	103.503216	48.247207
1753.260153	94.017647	48.252212
1749.636639	108.036881	48.257217
1745.936536	102.459395	48.262221
1742.873002	93.808955	48.267226
1739.438515	98.402566	48.272231
1736.502630	94.417704	48.277236
1732.500279	104.253373	48.282241
1728.974086	107.181332	48.287245
1725.470546	106.847151	48.292250
1721.243676	111.469182	48.297255
1718.466677	102.271115	48.302260
1714.960609	100.864833	48.307265
1711.561613	95.471440	48.312269
1708.025135	92.886668	48.317274
1704.495194	96.362532	48.322279
1701.724651	94.148923	48.327284
1697.579351	102.545209	48.332289
1694.287066	102.965913	48.337293
1690.725036	101.081134	48.342298
1687.057076	105.916728	48.347303
1683.658630	103.364256	48.352308
1680.326169	107.663587	48.357313
1676.338592	107.831846	48.362317
1673.319861	101.942680	48.367322
1669.661575	104.033839	48.372327
1666.429687	88.680422	48.377332
1662.847126	100.731780	48.382337
1659.465189	105.706353	48.387341
1655.860977	96.921781	48.392346
1652.210313	102.102692	48.397351
1648.964702	92.705498	48.402356
1645.290276	87.759939	48.407361
1641.530626	90.082007	48.412365
1638.635659	89.555040	48.417370
1635.019507	100.194289	48.422375
1631.722197	100.125406	48.427380
1627.944554	89.678420	48.432385
1624.176458	92.245409	48.437389
1620.772905	97.220183	48.442394
1616.920065	97.607919	48.447399
1613.910213	89.088349	48.452404
1610.503467	98.628837	48.457409
1606.902704	95.886406	48.462413
1604.015125	90.625398	48.467418
1600.299565	102.593055	48.472423
1596.807321	96.116387	48.477428
1592.623954	106.666755	48.482433
1589.195529	96.342586	48.487437
1585.702182	99.357190	48.492442
1582.363514	102.812783	48.497447
1579.355531	93.293196	48.502452
1575.607972	102.339412	48.507457
1572.053998	97.071397	48.512461
1568.929483	95.472869	48.517466
1564.925871	99.186979	48.522471
1561.917580	93.384789	48.527476
1557.972124	103.274878	48.532481
1554.128631	100.269680	48.537485
1550.950268	91.608670	48.542490
1547.465776	95.052160	48.547495
1544.259958	93.577019	48.552500
1540.392187	96.887179	48.557505
1536.811234	97.134531	48.562509
1533.783340	91.202522	48.567514
1530.201576	96.755520	48.572519
1526.549809	94.334243	48.577524
1523.220258	101.765188	48.582529
1519.772578	91.678145	48.587533
1516.284176	94.065571	48.592538
1512.658541	98.163772	48.597543
1509.284310	98.258730	48.602548
1505.442937	93.696671	48.607553
1502.060758	105.175850	48.612557
1498.909391	98.101984	48.617562
1495.134011	96.639568	48.622567
1491.736441	88.727683	48.627572
1487.827100	89.949951	48.632577
1484.517300	95.827610	48.637581
1481.249402	90.964328	48.642586
1477.419088	104.617115	48.647591
1474.320582	94.887011	48.652596
1470.599491	90.217653	48.657601
1467.041370	102.053239	48.662605
1463.895506	98.863541	48.667610
1460.082594	96.919762	48.672615
1456.856409	90.126465	48.677620
1453.183761	87.186438	48.682625
1449.930928	89.882046	48.687629
1446.333056	87.411263	48.692634
1442.514047	94.861445	48.697639
1438.919132	94.506713	48.702644
1435.457099	96.969134	48.707649
1432.328144	98.047796	48.712653
1429.045272	94.154942	48.717658
1425.173074	99.006521	48.722663
1421.750383	91.870498	48.727668
1418.190125	89.390700	48.732673
1414.412040	95.448815	48.737677
1411.047431	85.573488	48.742682
1407.350853	93.298837	48.747687
1404.043673	90.491754	48.752692
1400.674381	97.229710	48.757697
1396.910649	96.803185	48.762701
1393.800801	88.463726	48.767706
1390.071897	98.892739	48.772711
1386.858704	87.744189	48.777716
1383.406702	99.088702	48.782721
1379.394417	98.473079	48.787725
1376.150808	83.770113	48.792730
1372.670107	95.489242	48.797735
1369.280849	91.850232	48.802740
1365.669206	105.519601	48.807745
1361.715805	96.125057	48.812749
1359.022477	93.241415	48.817754
1355.093326	96.437760	48.822759
1351.870964	86.176478	48.827764
1348.089573	89.216949	48.832769
1344.261807	87.648814	48.837773
1341.289583	86.940912	48.842778
1337.628709	94.369648	48.847783
1334.618124	91.633464	48.852788
1330.978847	87.166524	48.857793
1326.931127	95.639381	48.862797
1323.872205	94.992431	48.867802
1320.072461	100.405368	48.872807
1316.126139	94.581541	48.877812
1313.298388	91.298056	48.882817
1309.607329	100.145663	48.887821
1305.958259	89.849567	48.892826
1302.471773	94.827774	48.897831
1299.070516	92.933834	48.902836
1296.166890	90.484721	48.907841
1292.256141	96.389490	48.912845
1288.943331	94.342582	48.917850
1285.080229	93.643641	48.922855
1281.677008	91.515896	48.927860
1278.234216	91.447546	48.932865
1274.700273	92.668350	48.937869
1271.799992	88.105375	48.942874
1267.537341	94.957080	48.947879
1263.985851	94.987906	48.952884
1260.130183	91.149431	48.957889
1256.649505	96.430451	48.962893
1253.884496	84.019456	48.967898
1250.238721	91.989999	48.972903
1246.661700	90.648596	48.977908
1243.327771	90.500031	48.982913
1239.686997	97.470073	48.987917
1236.216213	89.269076	48.992922
1232.037417	96.765779	48.997927
1228.936522	90.218764	49.002932
1225.732703	93.438259	49.007937
1222.321147	92.292562	49.012941
1218.859130	93.451558	49.017946
1214.997806	94.448085	49.022951
1211.253201	88.928231	49.027956
1207.985676	94.663284	49.032961
1204.747850	87.232773	49.037965
1201.571693	87.192529	49.042970
1197.613432	90.453529	49.047975
1194.258147	84.623148	49.052980
1190.805651	83.648340	49.057985
1187.026777	80.313606	49.062989
1183.692955	81.911385	49.067994
1180.009549	87.486549	49.072999
1176.297596	89.079913	49.078004
1172.794850	84.904951	49.083009
1169.295701	96.073308	49.088013
1166.018157	86.127527	49.093018
1162.504610	92.274191	49.098023
1159.331541	89.538010	49.103028
1155.880064	90.303074	49.108033
1152.052165	79.003490	49.113037
1148.598042	84.878316	49.118042
1145.152413	88.967504	49.123047
1141.333760	89.751759	49.128052
1137.918676	83.421342	49.133057
1134.248568	80.012739	49.138061
1131.243283	85.637373	49.143066
1127.510694	91.938354	49.148071
1124.263047	89.922451	49.153076
1120.665227	83.778665	49.158081
1117.262673	81.530618	49.163085
1113.825471	88.794835	49.168090
1110.089999	87.285129	49.173095
1106.251850	82.279717	49.178100
1102.949743	85.590446	49.183105
1099.415753	96.033416	49.188109
1096.036256	82.857580	49.193114
1092.297482	93.781668	49.198119
1089.053703	94.640957	49.203124
1085.590524	94.930133	49.208129
1082.258595	89.624468	49.213133
1078.818742	83.563665	49.218138
1074.859294	90.558007	49.223143
1071.249343	88.468796	49.228148
1068.039683	87.253726	49.233153
1064.517550	95.021539	49.238157
1061.111755	89.518572	49.243162
1057.396682	91.814772	49.248167
1053.770657	87.605233	49.253172
1050.534505	84.360042	49.258177
1046.793529	89.741701	49.263181
1043.122083	82.419844	49.268186
1039.862521	84.123134	49.273191
1036.545122	78.410266	49.278196
1033.437289	83.990756	49.283201
1029.509747	82.798854	49.288205
1025.884999	84.362840	49.293210
1022.461066	88.878921	49.298215
1018.925062	86.787697	49.303220
1016.015831	87.655027	49.308225
1012.099373	85.648335	49.313229
1008.865074	76.164084	49.318234
1004.800299	91.555415	49.323239
1001.174593	87.314198	49.328244
997.661293	88.370470	49.333249
994.288149	95.627887	49.338253
991.346333	90.457659	49.343258
987.641610	87.551163	49.348263
983.965121	85.155952	49.353268
980.506850	87.858265	49.358273
976.869412	85.137445	49.363277
973.409164	76.105978	49.368282
969.961283	85.953425	49.373287
966.585803	84.602832	49.378292
962.909155	87.604888	49.383297
959.102252	86.868768	49.388301
955.807448	78.251301	49.393306
952.392143	81.677737	49.398311
949.217907	76.274785	49.403316
945.597060	74.658677	49.408321
941.808988	87.725922	49.413325
938.618909	79.038374	49.418330
934.751453	81.076738	49.423335
931.380733	85.600360	49.428340
927.579654	82.164720	49.433345
924.367410	84.683210	49.438349
921.417687	78.008315	49.443354
917.134381	91.019778	49.448359
913.827845	78.835515	49.453364
910.292693	78.873330	49.458369
906.558103	87.901725	49.463373
903.238241	79.905086	49.468378
899.972256	80.919706	49.473383
896.399324	87.274940	49.478388
892.431145	85.776178	49.483393
889.247239	93.867827	49.488397
886.177718	82.051624	49.493402
882.449763	75.697191	49.498407
878.872237	79.382996	49.503412
875.561401	85.675286	49.508417
871.781246	93.733203	49.513421
868.603879	78.646732	49.518426
864.854931	73.617988	49.523431
861.375932	80.145256	49.528436
858.385212	71.252692	49.533441
854.303841	76.874007	49.538445
850.740751	76.795958	49.543450
847.232443	84.767264	49.548455
843.853103	80.649071	49.553460
840.182939	69.600248	49.558465
836.356207	86.947636	49.563469
833.061154	75.131756	49.568474
829.602569	86.692422	49.573479
826.470143	75.154941	49.578484
823.195346	77.803396	49.583489
819.472518	77.750217	49.588493
816.110105	76.002150	49.593498
812.111382	77.687648	49.598503
808.886462	80.875657	49.603508
805.431736	69.635122	49.608513
801.528641	82.280520	49.613517
798.390809	70.822981	49.618522
794.887698	72.393367	49.623527
791.633113	76.525605	49.628532
788.034789	69.138637	49.633537
784.088713	83.246016	49.638541
780.570253	72.135626	49.643546
777.086396	84.437361	49.648551
773.757073	78.599845	49.653556
770.195150	67.670228	49.658561
766.482193	71.797893	49.663565
762.974886	65.032661	49.668570
759.727866	75.082953	49.673575
756.505826	79.586605	49.678580
753.058310	73.384689	49.683585
749.301566	74.538994	49.688589
745.865209	70.787189	49.693594
742.487893	73.809105	49.698599
738.563075	74.518188	49.703604
735.001138	69.181952	49.708609
731.300595	70.871662	49.713613
728.268825	66.278616	49.718618
724.513233	77.464745	49.723623
721.090156	69.515848	49.728628
718.248307	70.733374	49.733633
714.241733	74.210744	49.738637
710.644487	83.600571	49.743642
706.863903	79.639771	49.748647
703.659687	79.021833	49.753652
700.409717	77.129730	49.758657
696.938984	78.679269	49.763661
693.381428	70.377998	49.768666
689.522939	76.470820	49.773671
686.140553	72.631530	49.778676
682.375235	74.976718	49.783681
679.033444	78.768210	49.788685
675.908151	81.156131	49.793690
672.416323	78.672112	49.798695
668.497801	75.153560	49.803700
665.224022	62.486551	49.808705
661.351749	78.755879	49.813709
658.377599	71.344533	49.818714
654.957333	75.755668	49.823719
651.196403	73.952605	49.828724
647.983374	71.482136	49.833729
644.160088	76.648854	49.838733
640.520973	66.781621	49.843738
637.152773	74.721632	49.848743
633.574854	74.266279	49.853748
629.978046	74.747149	49.858753
626.486237	68.476224	49.863757
622.860724	75.902652	49.868762
619.542901	79.763182	49.873767
615.910019	69.085084	49.878772
613.150523	73.244665	49.883777
609.048017	77.913866	49.888781
605.757480	76.452024	49.893786
602.509623	79.785986	49.898791
598.523499	84.443400	49.903796
595.300853	72.407500	49.908801
591.636655	77.119199	49.913805
588.003921	65.884280	49.918810
584.543154	79.599743	49.923815
581.208782	73.579555	49.928820
577.946284	62.954539	49.933825
573.911699	73.345732	49.938829
570.367372	69.882838	49.943834
566.972125	75.650462	49.948839
563.268860	65.654032	49.953844
559.876216	66.245493	49.958849
556.425328	70.642420	49.963853
553.002678	75.835359	49.968858
549.733295	73.468586	49.973863
545.945094	77.585842	49.978868
542.410141	84.526794	49.983873
538.987515	84.357317	49.988877
535.513612	77.510994	49.993882
532.120069	73.983505	49.998887
528.619653	81.308211	50.003892
525.581182	73.571552	50.008897
521.762250	79.500048	50.013901
518.223972	66.678098	50.018906
514.307333	79.917217	50.023911
510.914575	74.048495	50.028916
507.720182	64.659375	50.033921
504.115074	75.812593	50.038925
500.513490	73.820237	50.043930
496.874653	81.815046	50.048935
493.309759	76.729241	50.053940
490.119394	72.746197	50.058945
486.200746	76.301652	50.063949
483.112178	65.905834	50.068954
479.512707	72.701810	50.073959
475.850277	76.685602	50.078964
472.499447	72.695905	50.083969
469.002237	78.523702	50.088973
465.353634	74.358906	50.093978
461.774836	78.041786	50.098983
458.142074	78.756059	50.103988
454.932879	68.910520	50.108993
451.703161	71.441264	50.113997
448.292986	69.074279	50.119002
444.708470	79.234070	50.124007
440.887291	73.046091	50.129012
437.477472	71.419349	50.134017
433.838898	78.433384	50.139021
430.531120	72.874142	50.144026
427.008264	70.512048	50.149031
423.580684	75.044560	50.154036
420.092264	70.835854	50.159041
416.216002	81.091685	50.164045
412.739395	67.260442	50.169050
409.029321	80.144713	50.174055
405.529731	73.460599	50.179060
402.318255	67.971790	50.184065
398.840096	73.840917	50.189069
394.954755	67.245334	50.194074
392.086856	79.523945	50.199079
388.335954	74.163406	50.204084
385.146405	70.683275	50.209089
381.583966	72.487564	50.214093
378.106691	75.180240	50.219098
374.502556	73.267392	50.224103
370.910163	74.620779	50.229108
367.325587	63.691620	50.234113
363.860479	74.111224	50.239117
360.450725	73.110888	50.244122
356.302108	76.673689	50.249127
353.093693	76.986564	50.254132
350.460058	72.261991	50.259137
346.134371	76.469274	50.264141
342.914455	70.931169	50.269146
339.351736	75.051307	50.274151
335.836310	81.078099	50.279156
332.587259	72.342906	50.284161
329.120200	74.160826	50.289165
325.480832	74.350978	50.294170
321.703440	81.614419	50.299175
318.191496	77.450519	50.304180
314.889380	74.146105	50.309185
311.394580	76.069583	50.314189
308.047856	72.942954	50.319194
304.250106	73.319113	50.324199
300.794811	73.648285	50.329204
297.028436	68.631850	50.334209
293.423063	69.835412	50.339213
290.014926	68.496324	50.344218
286.416515	77.060637	50.349223
283.389074	68.316265	50.354228
280.366595	70.555343	50.359233
276.781439	75.495205	50.364237
273.334561	70.264522	50.369242
269.324538	70.673734	50.374247
265.608522	72.786678	50.379252
262.370356	66.941392	50.384257
258.592386	73.518411	50.389261
255.022373	69.357237	50.394266
251.469134	70.391342	50.399271
248.514416	78.181585	50.404276
245.144109	75.694532	50.409281
240.849542	71.680964	50.414285
237.860452	73.674411	50.419290
234.056586	74.010405	50.424295
230.482226	83.735208	50.429300
227.199401	70.354717	50.434305
223.793555	80.056446	50.439309
220.278408	75.760189	50.444314
216.932030	62.000472	50.449319
213.083716	69.692562	50.454324
209.909223	62.866131	50.459329
206.153923	73.115794	50.464333
202.748776	70.362098	50.469338
199.415957	74.057328	50.474343
195.793316	77.819827	50.479348
192.360220	73.640511	50.484353
188.659114	73.758039	50.489357
185.192122	75.648731	50.494362
181.290749	74.702815	50.499367
177.908004	74.125394	50.504372
174.792763	64.031179	50.509377
171.105631	70.110024	50.514381
167.750730	75.314596	50.519386
164.184643	68.792740	50.524391
160.442305	72.902898	50.529396
157.225859	71.518167	50.534401
153.562244	69.399487	50.539405
150.692146	81.817645	50.544410
147.086794	70.622857	50.549415
143.277880	82.263393	50.554420
139.323101	76.618278	50.559425
136.213674	69.648855	50.564429
132.734294	69.896382	50.569434
129.343088	71.860700	50.574439
125.498622	68.479411	50.579444
122.088635	76.960619	50.584449
118.281084	77.211786	50.589453
115.033075	70.687872	50.594458
111.682578	78.890908	50.599463
107.958964	88.743359	50.604468
104.733708	74.360545	50.609473
101.204028	79.880229	50.614477
97.816382	70.046731	50.619482
94.396538	73.714394	50.624487
90.644737	77.803889	50.629492
86.878317	67.339690	50.634497
83.567214	69.747108	50.639501
80.091552	66.387500	50.644506
76.497862	63.017796	50.649511
72.956818	71.082825	50.654516
69.381222	66.511280	50.659521
66.058647	68.246629	50.664525
62.239270	67.575860	50.669530
59.180231	71.187351	50.674535
55.529198	74.631594	50.679540
52.391777	71.494565	50.684545
48.597609	73.879125	50.689549
44.974081	75.645514	50.694554
41.554882	73.684946	50.699559
37.827622	81.323409	50.704564
34.424418	71.410092	50.709569
31.127766	73.078135	50.714573
27.626723	68.805028	50.719578
24.478114	74.385606	50.724583
20.555494	71.013341	50.729588
17.550935	64.695146	50.734593
13.404768	66.685277	50.739597
10.206865	63.333053	50.744602
6.741994	67.823957	50.749607
2.873995	69.270924	50.754612