Fri Aug 26 13:38:09 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
2.098399	115.723242	0.000000
2.130702	115.408208	0.005005
2.568775	113.669624	0.010010
2.293325	113.506907	0.015014
2.098022	99.177505	0.020019
1.732133	93.062213	0.025024
1.599136	104.101971	0.030029
1.830004	89.323421	0.035034
1.291355	80.773708	0.040038
1.272524	73.240853	0.045043
0.993840	78.267031	0.050048
0.548397	60.284623	0.055053
0.543527	58.254352	0.060058
0.325850	49.468025	0.065062
-0.057875	45.392917	0.070067
-0.256404	39.447732	0.075072
-0.644351	32.892986	0.080077
-1.062655	26.418895	0.085082
-1.587003	28.063409	0.090086
-2.056705	17.048005	0.095091
-2.321709	23.432403	0.100096
-2.331151	18.118988	0.105101
-1.804157	12.491106	0.110106
-2.646739	20.917398	0.115110
-3.014182	9.357749	0.120115
-3.318456	12.869345	0.125120
-3.308538	6.973972	0.130125
-3.468188	7.049481	0.135130
-4.232528	11.338200	0.140134
-4.197418	5.837524	0.145139
-4.253970	8.829676	0.150144
-4.556154	6.235119	0.155149
-5.107185	6.630984	0.160154
-5.909050	5.639101	0.165158
-6.025161	4.986522	0.170163
-5.783633	7.220445	0.175168
-5.662864	6.942258	0.180173
-5.695979	0.126641	0.185178
-6.858833	1.668093	0.190182
-6.739313	-1.469830	0.195187
-7.072972	2.761321	0.200192
-7.411646	-0.330571	0.205197
-7.213958	4.738471	0.210202
-8.050934	4.998529	0.215206
-8.094621	8.615079	0.220211
-8.576548	3.014577	0.225216
-8.830347	12.073666	0.230221
-8.720704	4.049455	0.235226
-8.883946	13.461428	0.240230
-9.030598	4.477411	0.245235
-9.710448	13.368725	0.250240
-9.901684	14.711446	0.255245
-10.227851	14.252917	0.260250
-10.262970	14.875330	0.265254
-10.417253	3.159115	0.270259
-11.155504	6.744606	0.275264
-11.370588	9.723477	0.280269
-11.362268	6.593376	0.285274
-11.934072	17.081327	0.290278
-11.542392	4.368978	0.295283
-11.885356	-0.196503	0.300288
-12.555458	6.788781	0.305293
-12.795719	5.921422	0.310298
-13.430649	14.767780	0.315302
-13.359362	15.962062	0.320307
-13.465612	5.665170	0.325312
-13.677908	8.216516	0.330317
-13.088696	9.848996	0.335322
-13.665775	6.044439	0.340326
-14.346796	13.882444	0.345331
-14.588498	7.760502	0.350336
-14.810305	11.553476	0.355341
-15.427616	15.382721	0.360346
-16.215052	17.754706	0.365350
-15.765286	12.040777	0.370355
-15.742558	13.302729	0.375360
-16.099664	6.828609	0.380365
-16.326905	-3.572821	0.385370
-16.225357	9.512034	0.390374
-16.620096	5.679087	0.395379
-17.094286	-2.497820	0.400384
-17.710652	10.167321	0.405389
-17.708863	-3.680173	0.410394
-17.846428	0.881101	0.415398
-18.004128	3.724492	0.420403
-18.389737	4.562820	0.425408
-19.291486	5.282200	0.430413
-19.133805	11.929801	0.435418
-19.627096	9.830055	0.440422
-19.309616	8.806257	0.445427
-19.235931	1.559575	0.450432
-19.504909	10.798190	0.455437
-19.844097	6.849030	0.460442
-20.327482	9.793748	0.465446
-20.496947	0.180557	0.470451
-20.716707	9.104635	0.475456
-21.548532	10.319311	0.480461
-21.886961	13.216151	0.485466
-21.454629	7.852938	0.490470
-21.946679	6.069363	0.495475
-22.275270	8.787507	0.500480
-22.801313	10.723338	0.505485
-22.532336	8.147417	0.510490
-22.674699	14.386171	0.515494
-23.064474	15.006857	0.520499
-23.320622	11.449713	0.525504
-23.928494	9.307698	0.530509
-23.653940	-0.782734	0.535514
-24.033751	7.119098	0.540518
-24.264773	-2.342142	0.545523
-25.060202	-0.620624	0.550528
-25.307055	7.871088	0.555533
-25.089829	2.104787	0.560538
-25.627690	8.411443	0.565542
-25.201541	3.400359	0.570547
-25.517471	3.516019	0.575552
-25.969371	15.927774	0.580557
-26.431865	1.757110	0.585562
-26.585139	6.257558	0.590566
-27.095817	8.766779	0.595571
-27.050224	5.855494	0.600576
-27.124814	8.733399	0.605581
-27.604759	11.259981	0.610586
-27.872094	11.880585	0.615590
-27.796941	10.688881	0.620595
-27.933128	1.798146	0.625600
-28.848862	14.940155	0.630605
-29.270422	1.819774	0.635610
-29.412735	9.039246	0.640614
-29.536977	11.393391	0.645619
-29.390694	5.258497	0.650624
-30.013755	8.256598	0.655629
-30.411403	7.299853	0.660634
-30.734312	4.680052	0.665638
-30.722896	10.996098	0.670643
-30.694509	9.077710	0.675648
-30.901828	12.422355	0.680653
-30.990464	-2.448733	0.685658
-31.847446	6.539756	0.690662
-32.209912	10.848158	0.695667
-32.278609	6.869539	0.700672
-32.605152	6.812851	0.705677
-32.760730	2.006232	0.710682
-32.469723	5.042342	0.715686
-32.806883	3.940143	0.720691
-33.274388	-6.601039	0.725696
-33.655932	2.234332	0.730701
-33.672439	4.843775	0.735706
-34.237707	6.459859	0.740710
-35.005815	-4.392013	0.745715
-35.578300	0.743159	0.750720
-35.443719	3.436642	0.755725
-34.600930	-0.092292	0.760730
-35.082086	5.538007	0.765734
-34.981507	-2.168424	0.770739
-35.871501	0.902873	0.775744
-36.480161	-7.079093	0.780749
-36.680381	-1.853192	0.785754
-36.981057	6.349518	0.790758
-36.725221	3.452953	0.795763
-36.556828	-1.283889	0.800768
-37.551198	11.762797	0.805773
-37.683285	6.683610	0.810778
-38.167798	0.833586	0.815782
-38.391667	8.590919	0.820787
-38.185372	4.733994	0.825792
-38.146746	11.254603	0.830797
-38.576679	-0.500942	0.835802
-39.517521	5.760893	0.840806
-39.657628	0.657647	0.845811
-39.409458	0.663333	0.850816
-40.075883	2.839311	0.855821
-40.680870	1.462449	0.860826
-40.988760	6.325480	0.865830
-40.620170	0.263539	0.870835
-41.058099	0.654449	0.875840
-41.423484	2.264720	0.880845
-41.046107	-0.808950	0.885850
-41.562259	9.724111	0.890854
-41.532120	-4.270157	0.895859
-42.069243	-1.487910	0.900864
-42.916923	-8.005859	0.905869
-42.384592	-3.536234	0.910874
-42.847524	-2.186012	0.915878
-43.179154	-2.314671	0.920883
-43.856942	8.477665	0.925888
-44.039387	7.727850	0.930893
-44.162506	-4.138735	0.935898
-44.492443	-0.366892	0.940902
-44.443526	1.419309	0.945907
-43.956604	2.232513	0.950912
-44.707090	2.482269	0.955917
-45.164446	-3.235944	0.960922
-45.789154	4.656561	0.965926
-45.780155	-8.186012	0.970931
-45.635247	2.114410	0.975936
-46.063929	6.524865	0.980941
-47.126802	-3.547146	0.985946
-46.958905	3.399405	0.990950
-47.062909	-5.138844	0.995955
-46.976623	-0.764279	1.000960
-47.020003	-4.813273	1.005965
-47.037230	-7.616703	1.010970
-47.631783	-7.112824	1.015974
-48.314739	-6.731219	1.020979
-48.379040	0.431812	1.025984
-48.804936	5.066451	1.030989
-49.195352	-7.062223	1.035994
-49.885884	-1.155727	1.040998
-50.142253	0.298369	1.046003
-49.735214	-10.511846	1.051008
-49.624975	-4.565521	1.056013
-50.029631	-10.488083	1.061018
-50.358659	-8.301365	1.066022
-50.309462	-1.080079	1.071027
-51.032347	-11.641603	1.076032
-51.570510	2.697571	1.081037
-51.167577	-4.404225	1.086042
-51.583654	-3.330207	1.091046
-51.839745	-0.711935	1.096051
-52.782563	-1.934961	1.101056
-52.970798	-5.651365	1.106061
-52.736807	0.829331	1.111066
-53.037639	-1.958415	1.116070
-53.019385	0.316596	1.121075
-53.033274	-7.663063	1.126080
-53.597440	4.288452	1.131085
-54.232756	-11.955945	1.136090
-54.491812	-5.759140	1.141094
-54.686648	-6.766443	1.146099
-54.531143	-4.822838	1.151104
-54.848769	3.708363	1.156109
-54.875508	1.295541	1.161114
-55.644385	-3.782568	1.166118
-56.007135	-2.245472	1.171123
-55.828542	-5.139499	1.176128
-56.649060	-7.599566	1.181133
-56.390758	-7.554331	1.186138
-56.572010	-0.597711	1.191142
-56.841432	4.063184	1.196147
-57.168266	-5.610916	1.201152
-57.760620	-0.017087	1.206157
-57.610827	-3.147068	1.211162
-57.819813	-3.693440	1.216166
-58.319286	-6.080111	1.221171
-58.550188	-3.272780	1.226176
-58.894302	1.700289	1.231181
-59.271182	-6.188053	1.236186
-59.234087	-1.112994	1.241190
-59.708333	-6.610284	1.246195
-59.524851	-5.582163	1.251200
-59.817683	1.996085	1.256205
-59.911127	-3.658570	1.261210
-60.678947	5.255927	1.266214
-60.685286	3.811165	1.271219
-60.861991	-7.313109	1.276224
-61.073836	-1.920890	1.281229
-61.523976	-2.072224	1.286234
-61.886781	-0.402246	1.291238
-62.214306	5.245260	1.296243
-61.715187	-3.861440	1.301248
-62.272831	-2.762218	1.306253
-62.909933	-5.738042	1.311258
-63.283020	-2.348609	1.316262
-63.624948	-7.727300	1.321267
-63.341407	-13.200212	1.326272
-63.642131	-8.246556	1.331277
-63.886635	-8.423580	1.336282
-64.339989	-3.205722	1.341286
-64.735864	-7.993905	1.346291
-64.941152	-11.207798	1.351296
-65.511239	-7.477657	1.356301
-64.643531	-12.487886	1.361306
-64.946096	-4.275398	1.366310
-65.523231	-4.014668	1.371315
-66.193216	-8.241336	1.376320
-66.580040	-7.564164	1.381325
-66.752142	-12.247987	1.386330
-66.790733	-5.519218	1.391334
-66.849104	-6.348459	1.396339
-66.855444	-6.505619	1.401344
-67.797534	-3.894429	1.406349
-67.715466	-10.164845	1.411354
-67.857782	-11.879488	1.416358
-68.267662	-5.776254	1.421363
-68.179853	-13.249745	1.426368
-69.488699	-4.893235	1.431373
-69.587077	-4.526719	1.436378
-69.799130	-4.265887	1.441382
-70.106688	1.954291	1.446387
-69.449393	-0.561871	1.451392
-69.648335	-9.819298	1.456397
-69.711682	-9.262091	1.461402
-69.917673	-12.558129	1.466406
-70.840016	-7.431760	1.471411
-70.601780	-7.130310	1.476416
-71.537511	-8.205746	1.481421
-71.501512	-21.077819	1.486426
-72.232303	-19.948475	1.491430
-72.659010	-15.297896	1.496435
-72.351923	-18.629527	1.501440
-72.555191	-12.802066	1.506445
-72.499646	-11.222535	1.511450
-72.528562	-6.706654	1.516454
-73.290444	-5.926795	1.521459
-73.788254	-11.771578	1.526464
-74.182302	-11.608954	1.531469
-74.028455	1.758799	1.536474
-74.244419	-0.643541	1.541478
-74.420351	-1.081169	1.546483
-74.519010	-2.286937	1.551488
-74.564513	-0.792909	1.556493
-75.077708	-8.843516	1.561498
-75.448279	1.341017	1.566502
-75.558768	6.875639	1.571507
-75.703112	7.945312	1.576512
-76.105595	3.999684	1.581517
-76.234204	1.441378	1.586522
-76.844341	5.022739	1.591526
-77.368733	-2.466163	1.596531
-77.885515	-5.470212	1.601536
-77.879248	1.713466	1.606541
-77.672541	-1.767048	1.611546
-78.079586	3.418292	1.616550
-78.199320	3.674242	1.621555
-78.016237	-2.029795	1.626560
-78.875470	-4.183288	1.631565
-79.660517	-4.997458	1.636570
-79.687429	0.438731	1.641574
-79.591904	-5.985636	1.646579
-79.479215	-3.902493	1.651584
-79.828537	0.637968	1.656589
-79.762520	-3.095877	1.661594
-80.404113	4.096928	1.666598
-81.129425	2.045965	1.671603
-81.302538	-6.373957	1.676608
-81.560084	5.229271	1.681613
-81.513678	-5.328650	1.686618
-81.225972	2.874190	1.691622
-82.030569	-1.654210	1.696627
-82.323127	-3.120843	1.701632
-82.919095	0.217875	1.706637
-83.229679	-3.957188	1.711642
-83.038751	-2.446190	1.716646
-83.340416	-2.829441	1.721651
-83.069405	-3.646693	1.726656
-83.602063	-0.352633	1.731661
-84.352321	-6.243529	1.736666
-84.447671	-1.635049	1.741670
-84.729207	-5.650125	1.746675
-84.617042	-3.598536	1.751680
-84.691860	-7.073179	1.756685
-85.398850	-2.904122	1.761690
-85.529631	-6.673761	1.766694
-85.854479	-6.085329	1.771699
-85.732501	-7.382396	1.776704
-86.609029	1.137750	1.781709
-86.996264	-6.274432	1.786714
-87.366733	-3.742752	1.791718
-87.240682	-4.622853	1.796723
-87.126904	-0.445552	1.801728
-87.360302	-1.358268	1.806733
-86.982598	-1.198751	1.811738
-87.674447	4.401078	1.816742
-88.668236	0.965117	1.821747
-88.611386	-3.928355	1.826752
-88.807515	3.717091	1.831757
-88.628606	-9.721385	1.836762
-89.347332	-4.323010	1.841766
-90.024596	-3.891671	1.846771
-89.995855	-5.250148	1.851776
-90.749603	-1.969119	1.856781
-90.620248	-10.746168	1.861786
-90.268003	-12.363814	1.866790
-90.371132	-7.184670	1.871795
-90.801640	-17.124182	1.876800
-91.519271	-8.546526	1.881805
-91.674281	-15.460207	1.886810
-92.097215	-18.697156	1.891814
-92.125029	-5.029052	1.896819
-92.057064	-16.308468	1.901824
-92.161075	-4.222971	1.906829
-92.765552	-1.794056	1.911834
-93.018101	-3.795245	1.916838
-93.328642	-12.307657	1.921843
-93.627197	-15.880335	1.926848
-93.856060	-7.644525	1.931853
-94.203425	-10.605350	1.936858
-94.679835	-5.175104	1.941862
-95.049398	-10.850036	1.946867
-94.830134	-13.139812	1.951872
-94.904652	-14.852356	1.956877
-94.760336	-16.722354	1.961882
-95.158272	-21.329883	1.966886
-95.756563	-10.268376	1.971891
-95.772119	-19.829585	1.976896
-96.263156	-5.697068	1.981901
-96.707798	-18.393068	1.986906
-97.091620	-2.179753	1.991910
-97.746549	-3.963273	1.996915
-97.623805	-10.512176	2.006912
-96.830791	-13.223579	2.016909
-96.796245	-4.882037	2.026906
-96.200424	-3.020275	2.036902
-95.308685	-1.825454	2.046899
-95.164007	-8.328999	2.056896
-94.777059	-10.698420	2.066893
-94.055591	-3.236747	2.076890
-93.924592	-4.682534	2.086886
-92.852965	1.714130	2.096883
-92.496257	-1.708592	2.106880
-92.251632	-4.825603	2.116877
-91.539023	-4.071709	2.126874
-91.040599	-1.440873	2.136870
-90.920730	-8.925705	2.146867
-89.694498	0.503704	2.156864
-89.457292	-1.706194	2.166861
-89.393684	-3.024283	2.176858
-88.807144	-8.500606	2.186854
-88.338382	-3.787149	2.196851
-87.556506	-5.156887	2.206848
-87.049042	-4.076457	2.216845
-86.687115	-4.405161	2.226842
-85.730533	-10.363569	2.236838
-85.548617	-2.982606	2.246835
-85.598587	-6.373685	2.256832
-84.562969	-9.781740	2.266829
-84.189925	-5.959338	2.276826
-83.371725	-6.821567	2.286822
-82.842318	-10.575275	2.296819
-82.738844	-7.347606	2.306816
-82.300466	-8.312248	2.316813
-81.566754	0.275219	2.326810
-81.095887	-3.044906	2.336806
-80.264344	-3.117290	2.346803
-79.894204	-1.619518	2.356800
-79.794291	-1.989786	2.366797
-79.182678	-6.944177	2.376794
-78.766159	-4.059844	2.386790
-77.702828	-5.562099	2.396787
-77.504759	-7.955964	2.406784
-76.661499	-10.415440	2.416781
-76.878674	-2.785444	2.426778
-76.644900	1.470443	2.436774
-75.912210	-0.721571	2.446771
-74.882644	-0.926153	2.456768
-74.602181	-3.405703	2.466765
-73.919064	3.279527	2.476762
-73.434852	-3.318065	2.486758
-73.152954	-1.800218	2.496755
-72.568211	-1.653616	2.506752
-71.751523	3.179894	2.516749
-71.735657	5.572266	2.526746
-71.504571	5.995669	2.536742
-70.648619	3.724277	2.546739
-69.763930	0.171832	2.556736
-69.343754	2.646966	2.566733
-69.151089	2.072195	2.576730
-68.751835	4.360525	2.586726
-67.923630	7.209271	2.596723
-67.553995	-1.815939	2.606720
-67.038252	-4.531687	2.616717
-65.923898	-1.366379	2.626714
-66.008710	-3.282227	2.636710
-65.953333	0.938083	2.646707
-65.004692	-3.729842	2.656704
-64.386873	5.376168	2.666701
-64.312521	5.532548	2.676698
-63.109452	5.655734	2.686694
-63.157252	7.133053	2.696691
-62.781371	7.080933	2.706688
-62.083212	0.066737	2.716685
-61.594363	4.415954	2.726682
-61.293108	4.999488	2.736678
-60.441174	0.558854	2.746675
-60.042505	-0.450288	2.756672
-59.020618	6.508471	2.766669
-58.745059	-1.773523	2.776666
-58.774408	2.263583	2.786662
-58.347697	2.653360	2.796659
-57.197934	6.091914	2.806656
-57.110311	-2.917896	2.816653
-56.817196	-2.339431	2.826650
-56.145767	-0.245527	2.836646
-55.310794	6.764509	2.846643
-54.505295	-1.048819	2.856640
-54.668068	-1.900856	2.866637
-54.204496	1.780746	2.876634
-53.328831	1.200999	2.886630
-53.080662	5.679553	2.896627
-52.622164	3.001226	2.906624
-51.779839	0.484876	2.916621
-51.546716	1.386284	2.926618
-51.310405	0.202856	2.936614
-50.564067	2.864784	2.946611
-49.890919	0.707383	2.956608
-48.978932	7.737105	2.966605
-48.805461	3.338753	2.976602
-48.768002	0.510579	2.986598
-48.437460	-3.392727	2.996595
-47.499766	3.069144	3.006592
-46.884932	0.455171	3.016589
-45.931458	-8.971373	3.026586
-45.909979	-6.434163	3.036582
-45.671768	-1.323690	3.046579
-45.326635	-0.509411	3.056576
-44.037401	-7.755012	3.066573
-44.060363	-7.491618	3.076570
-43.697289	-3.946418	3.086566
-42.908257	-4.037523	3.096563
-42.543827	-5.345432	3.106560
-42.150564	-2.761574	3.116557
-41.407638	-5.214931	3.126554
-41.192586	-1.605504	3.136550
-40.410483	-0.688205	3.146547
-39.831719	-1.681040	3.156544
-39.489923	-0.178853	3.166541
-38.784906	0.281630	3.176538
-38.195691	5.419815	3.186534
-38.080861	3.786483	3.196531
-37.412737	1.683714	3.206528
-36.848161	0.556878	3.216525
-36.528239	4.422399	3.226522
-36.038154	-0.006242	3.236518
-35.354234	-3.014261	3.246515
-35.227197	-1.174539	3.256512
-34.434321	-6.740008	3.266509
-33.619484	-9.461143	3.276506
-33.595733	-2.027041	3.286502
-32.727750	-4.857818	3.296499
-32.205776	-5.908332	3.306496
-31.996063	-8.544754	3.316493
-31.535121	-8.287014	3.326490
-31.151706	-9.341296	3.336486
-30.625903	-4.313612	3.346483
-29.897297	-7.211384	3.356480
-29.519994	-1.397166	3.366477
-29.138372	0.070312	3.376474
-28.056226	-12.344390	3.386470
-27.871742	-11.273857	3.396467
-27.787266	-6.240814	3.406464
-26.913146	-7.352492	3.416461
-26.647741	-3.598855	3.426458
-25.679330	-7.737685	3.436454
-25.138085	-12.326338	3.446451
-25.319104	-6.767303	3.456448
-24.327884	-8.888699	3.466445
-23.671355	-6.368004	3.476442
-23.842098	-6.347686	3.486438
-22.875840	-6.580421	3.496435
-22.381199	1.613469	3.506432
-21.879811	0.822743	3.516429
-20.835008	0.108961	3.526426
-20.956381	-0.369400	3.536422
-20.792657	-1.525688	3.546419
-20.008533	3.452276	3.556416
-19.608965	-1.975933	3.566413
-18.820647	2.133430	3.576410
-18.088944	-6.653558	3.586406
-17.625189	3.059297	3.596403
-17.874843	-1.064108	3.606400
-16.776334	-3.389102	3.616397
-16.281985	-3.804945	3.626394
-16.350507	-7.883694	3.636390
-15.443971	-3.146529	3.646387
-14.724321	1.686256	3.656384
-14.496586	-6.924068	3.666381
-13.595559	-3.164861	3.676378
-13.513895	-7.726308	3.686374
-12.952063	1.923761	3.696371
-11.953893	5.335238	3.706368
-11.654461	0.068332	3.716365
-11.673144	2.279190	3.726362
-11.344258	1.385447	3.736358
-10.489308	-1.563674	3.746355
-9.402890	-0.003198	3.756352
-9.171580	1.839297	3.766349
-8.942283	1.486896	3.776346
-8.695658	-0.699128	3.786342
-7.736973	2.354211	3.796339
-7.274828	2.250649	3.806336
-6.998772	6.851571	3.816333
-6.316977	9.586906	3.826330
-5.992480	6.549319	3.836326
-5.790751	13.287336	3.846323
-5.055566	16.299451	3.856320
-4.446905	20.082010	3.866317
-3.974626	21.180594	3.876314
-3.656041	32.335196	3.886310
-3.532212	44.708015	3.896307
-2.794228	54.153297	3.906304
-2.115042	61.491714	3.916301
-1.613297	75.323044	3.926298
-1.199533	84.913853	3.936294
-1.036980	94.284029	3.946291
-0.224568	108.925463	3.956288
0.000000	112.900899	3.961293
0.173204	136.528662	3.966298
0.157340	138.701440	3.971302
0.679226	135.162334	3.976307
0.485445	136.859790	3.981312
0.975834	138.466542	3.986317
1.022875	148.741163	3.991322
0.842113	147.326710	3.996326
1.262038	133.455133	4.001331
0.633811	139.086228	4.006336
0.918910	138.826744	4.011341
0.726406	145.041715	4.016346
1.160180	148.678864	4.021350
1.595030	151.237037	4.026355
0.483203	149.410742	4.031360
0.895645	150.074204	4.036365
1.398317	160.540476	4.041370
1.530620	154.129303	4.046374
1.238487	134.629700	4.051379
0.960064	139.776073	4.056384
1.309118	134.163204	4.061389
1.091337	138.009361	4.066394
1.017147	144.778533	4.071398
1.132808	139.512040	4.076403
1.084422	145.666609	4.081408
0.991584	132.311454	4.086413
1.185237	144.825264	4.091418
1.449367	144.939194	4.096422
1.629393	138.425687	4.101427
1.239139	148.262207	4.106432
1.301892	143.826503	4.111437
1.124311	145.262017	4.116442
1.261890	143.725236	4.121446
1.019621	140.839764	4.126451
1.015949	137.056628	4.131456
0.845148	136.289176	4.136461
0.871986	138.119957	4.141466
1.035152	139.616310	4.146470
1.527805	153.194019	4.151475
1.524180	167.314068	4.156480
1.494375	145.733042	4.161485
1.286681	144.832132	4.166490
1.387495	140.121592	4.171494
1.392559	135.577817	4.176499
0.981707	137.546345	4.181504
1.714978	146.398037	4.186509
1.364923	154.681269	4.191514
1.418905	149.576232	4.196518
1.315868	143.119450	4.201523
1.041385	150.027374	4.206528
1.425520	157.598364	4.211533
1.322802	165.074320	4.216538
1.512552	165.468743	4.221542
2.004759	158.729458	4.226547
1.388490	166.794723	4.231552
1.868925	162.600859	4.236557
1.556304	161.580248	4.241562
1.368256	153.311261	4.246566
1.475553	146.989404	4.251571
1.477921	160.478944	4.256576
1.510536	157.183686	4.261581
1.644650	163.006134	4.266586
1.841214	149.558452	4.271590
1.738338	159.919694	4.276595
1.710286	163.973591	4.281600
1.586103	146.887014	4.286605
1.369915	152.688071	4.291610
1.339688	148.665464	4.296614
1.862869	153.468742	4.301619
1.655837	162.169459	4.306624
1.839545	165.861365	4.311629
1.668877	159.256923	4.316634
1.546159	168.808198	4.321638
2.135634	160.152402	4.326643
1.757702	174.052331	4.331648
1.991714	162.626721	4.336653
1.890617	162.788025	4.341658
1.682845	170.827655	4.346662
1.838163	163.808635	4.351667
1.879146	175.273754	4.356672
1.826047	162.358466	4.361677
1.757814	162.568435	4.366682
1.401012	168.277499	4.371686
1.469767	163.407433	4.376691
1.588621	170.181359	4.381696
1.739906	162.659944	4.386701
1.700718	165.630437	4.391706
1.643774	167.689395	4.396710
1.728082	159.137562	4.401715
1.328138	167.355803	4.406720
1.712009	173.743629	4.411725
2.180595	186.179863	4.416730
2.236702	184.965803	4.421734
2.451993	173.274189	4.426739
2.399621	168.331234	4.431744
2.084850	162.179487	4.436749
1.965781	168.718381	4.441754
1.822005	169.819612	4.446758
1.866202	160.286959	4.451763
1.543008	169.913739	4.456768
2.074532	171.745037	4.461773
2.134259	187.500346	4.466778
2.465144	183.519582	4.471782
2.183707	184.620101	4.476787
2.294099	174.039450	4.481792
2.023429	162.176740	4.486797
1.842855	162.527583	4.491802
2.248405	184.265326	4.496806
2.423323	181.542677	4.501811
2.037863	187.784542	4.506816
2.280779	175.908296	4.511821
2.140669	179.748696	4.516826
2.198222	185.712782	4.521830
2.245180	185.870016	4.526835
2.121490	198.863533	4.531840
2.581021	190.202646	4.536845
2.391408	184.632502	4.541850
2.056985	172.150140	4.546854
2.409123	180.513876	4.551859
2.817455	178.049108	4.556864
2.352285	169.946644	4.561869
1.874227	172.409681	4.566874
2.272704	177.441183	4.571878
2.739949	178.206842	4.576883
2.182874	190.435784	4.581888
2.137881	182.090729	4.586893
2.519370	185.745518	4.591898
2.162464	180.302660	4.596902
2.645263	191.097902	4.601907
2.734563	197.632838	4.606912
2.488224	176.743532	4.611917
2.154777	179.876899	4.616922
2.435854	188.950873	4.621926
2.789889	186.023171	4.626931
2.621318	187.220010	4.631936
2.502080	172.027678	4.636941
2.445483	175.962639	4.641946
2.436734	184.047216	4.646950
2.346315	187.705879	4.651955
2.224693	192.280539	4.656960
2.732999	191.913538	4.661965
2.616949	193.054745	4.666970
2.636768	193.497771	4.671974
2.587815	195.644071	4.676979
2.260382	191.677220	4.681984
2.469694	188.085533	4.686989
2.642820	190.020090	4.691994
2.721033	195.158407	4.696998
2.568831	188.687118	4.702003
2.190691	191.001726	4.707008
2.446447	187.083277	4.712013
2.435165	187.379290	4.717018
2.471123	194.324316	4.722022
2.752556	191.116858	4.727027
2.789627	201.835977	4.732032
3.112168	196.119651	4.737037
3.302883	184.087016	4.742042
2.802278	189.002248	4.747046
3.080531	178.873173	4.752051
2.909879	186.160404	4.757056
2.983164	188.300326	4.762061
3.312940	179.684955	4.767066
2.544594	187.217102	4.772070
2.721096	194.184537	4.777075
2.578373	193.178599	4.782080
2.904396	181.140717	4.787085
3.120537	187.247787	4.792090
2.881392	186.680794	4.797094
3.070954	179.311596	4.802099
2.994365	187.878124	4.807104
3.188490	187.237345	4.812109
3.340376	190.513442	4.817114
2.809426	188.413209	4.822118
3.254306	182.918279	4.827123
3.085234	190.043918	4.832128
3.102639	184.387760	4.837133
3.185909	189.269031	4.842138
2.981024	186.817482	4.847142
3.068308	189.455085	4.852147
2.909173	185.278539	4.857152
2.881140	180.293827	4.862157
2.925259	189.344586	4.867162
2.662836	183.697195	4.872166
3.264856	185.738976	4.877171
3.091236	184.393009	4.882176
3.064900	186.298511	4.887181
2.761239	180.208301	4.892186
2.687391	189.293245	4.897190
2.930503	187.094639	4.902195
2.897505	202.968800	4.907200
3.053153	200.647772	4.912205
3.186108	205.147998	4.917210
3.194779	209.031677	4.922214
3.634718	207.207374	4.927219
3.646588	202.763760	4.932224
3.340771	205.054455	4.937229
3.315266	198.443215	4.942234
2.931911	192.545739	4.947238
3.116699	195.794568	4.952243
3.430564	205.502509	4.957248
3.649461	205.670937	4.962253
3.583494	212.062378	4.967258
3.541367	204.412874	4.972262
3.416138	187.487768	4.977267
2.935285	183.108219	4.982272
3.344804	196.056680	4.987277
3.429029	204.171081	4.992282
3.388863	203.098556	4.997286
3.705939	198.028471	5.002291
3.547772	207.341682	5.007296
3.315293	203.511901	5.012301
3.115185	203.932223	5.017306
3.199923	205.877380	5.022310
3.603531	200.651456	5.027315
3.739431	202.689883	5.032320
3.416338	204.394825	5.037325
3.557737	204.863213	5.042330
3.737572	208.163435	5.047334
3.996974	206.813320	5.052339
3.302581	205.491487	5.057344
3.361115	207.352141	5.062349
3.585099	206.988279	5.067354
3.399271	212.272113	5.072358
3.605280	206.719457	5.077363
3.248871	203.279122	5.082368
3.638947	204.335200	5.087373
3.395685	205.787273	5.092378
3.222669	203.659782	5.097382
3.597431	201.061036	5.102387
3.435529	210.558324	5.107392
3.634195	202.336669	5.112397
3.913682	206.026326	5.117402
3.535402	210.973137	5.122406
3.540638	199.659052	5.127411
3.498464	215.885821	5.132416
3.922792	215.500257	5.137421
4.172977	218.444687	5.142426
3.739275	217.034810	5.147430
3.599094	205.373211	5.152435
3.714429	217.687301	5.157440
3.832084	230.292097	5.162445
4.111869	224.813368	5.167450
3.799062	225.871319	5.172454
3.898076	211.265053	5.177459
3.637789	228.769119	5.182464
3.832385	229.545594	5.187469
3.873213	231.677919	5.192474
4.112447	237.240421	5.197478
4.095707	229.596445	5.202483
4.295816	228.774404	5.207488
3.638965	221.356641	5.212493
3.791246	213.774940	5.217498
3.679658	227.203181	5.222502
4.030202	229.546706	5.227507
3.857456	244.449267	5.232512
4.176057	232.687747	5.237517
4.030947	238.382855	5.242522
4.029513	228.623157	5.247526
4.160801	231.959415	5.252531
3.953747	228.701460	5.257536
4.113650	224.943456	5.262541
4.180128	232.127348	5.267546
4.059015	238.467274	5.272550
4.279078	235.876791	5.277555
4.079393	231.592655	5.282560
3.986561	244.790205	5.287565
4.038606	236.059864	5.292570
3.749943	232.966471	5.297574
4.114382	232.590232	5.302579
3.623447	229.515677	5.307584
3.854784	236.300589	5.312589
4.291772	234.596963	5.317594
4.467005	228.890908	5.322598
3.905687	232.882319	5.327603
3.927834	236.169133	5.332608
4.155834	242.986204	5.337613
4.458294	258.580400	5.342618
4.588559	256.250663	5.347622
4.672438	252.631037	5.352627
4.237128	242.862956	5.357632
4.288555	239.011109	5.362637
3.891461	236.804610	5.367642
4.053366	234.400348	5.372646
4.110318	246.710894	5.377651
4.376897	257.574642	5.382656
4.384274	255.048907	5.387661
4.853503	260.426914	5.392666
4.349039	261.910168	5.397670
4.594338	252.342991	5.402675
4.452169	264.368183	5.407680
4.836921	256.364298	5.412685
4.711485	256.564192	5.417690
4.333956	245.436220	5.422694
4.354741	240.304689	5.427699
4.398445	250.399559	5.432704
4.824748	258.068428	5.437709
4.560562	256.369568	5.442714
4.595093	254.814021	5.447718
4.516250	245.819323	5.452723
3.998958	247.035660	5.457728
4.402962	260.089428	5.462733
4.154284	264.658579	5.467738
4.615663	260.024744	5.472742
4.527041	252.161001	5.477747
4.296371	255.423908	5.482752
4.629673	258.614826	5.487757
4.566825	254.910479	5.492762
4.335031	262.991855	5.497766
4.800507	253.165775	5.502771
4.482541	253.395645	5.507776
4.448430	248.997143	5.512781
4.796104	257.298336	5.517786
4.696934	271.601018	5.522790
4.829441	259.643833	5.527795
4.606114	267.075336	5.532800
4.809602	267.853592	5.537805
4.865027	272.289978	5.542810
4.896717	268.488654	5.547814
4.630859	261.993905	5.552819
4.765521	272.080952	5.557824
5.043162	274.964170	5.562829
4.954879	273.921278	5.567834
4.779509	280.143119	5.572838
5.130139	274.175628	5.577843
4.635853	273.515482	5.582848
4.775446	269.668884	5.587853
4.957698	275.208633	5.592858
5.176581	282.694677	5.597862
4.805718	267.446529	5.602867
4.918361	282.146503	5.607872
5.023274	282.525664	5.612877
5.208514	274.590799	5.617882
4.800902	275.204779	5.622886
5.005720	265.181999	5.627891
4.904176	275.875288	5.632896
5.130954	278.497513	5.637901
5.020331	288.281081	5.642906
5.127745	286.657237	5.647910
5.141375	276.980587	5.652915
5.136896	271.169624	5.657920
5.000138	265.515296	5.662925
5.156199	261.729410	5.667930
5.083943	273.841797	5.672934
5.301716	276.262947	5.677939
5.140829	275.370561	5.682944
4.928839	264.197821	5.687949
5.211168	268.633678	5.692954
5.257482	282.508766	5.697958
5.196884	273.232809	5.702963
5.047479	272.088705	5.707968
4.974973	281.059594	5.712973
5.457291	288.115490	5.717978
5.304839	282.783134	5.722982
5.554057	276.306259	5.727987
5.222806	269.467355	5.732992
4.859626	263.278818	5.737997
5.262612	267.873056	5.743002
5.029328	277.862373	5.748006
5.423446	267.626625	5.753011
5.440789	274.735929	5.758016
5.362564	278.430676	5.763021
5.367141	278.717894	5.768026
5.246809	295.706699	5.773030
5.637839	285.648588	5.778035
5.300045	290.823230	5.783040
5.297711	283.290881	5.788045
5.177614	279.883339	5.793050
5.555673	282.697141	5.798054
5.557095	283.294891	5.803059
5.673593	285.358495	5.808064
5.442269	281.569645	5.813069
5.672717	286.924727	5.818074
5.397352	292.798317	5.823078
5.404644	291.082496	5.828083
5.230248	290.426326	5.833088
5.205034	278.518993	5.838093
5.577761	282.355497	5.843098
5.462981	288.881113	5.848102
5.282862	284.673010	5.853107
5.172116	282.488359	5.858112
5.134152	283.652215	5.863117
5.539925	282.674765	5.868122
5.375213	286.433599	5.873126
5.764656	296.262697	5.878131
5.711790	295.306037	5.883136
5.733887	288.620915	5.888141
5.471835	284.153491	5.893146
5.497757	297.459138	5.898150
5.736934	298.209693	5.903155
5.763859	309.082313	5.908160
5.197057	313.321363	5.913165
5.617982	314.394792	5.918170
5.612837	311.200295	5.923174
5.781325	317.700800	5.928179
5.784947	320.326138	5.933184
5.552153	308.764311	5.938189
5.613862	311.133836	5.943194
5.848610	309.816025	5.948198
5.911387	310.261857	5.953203
5.599129	314.287273	5.958208
5.732007	308.445421	5.963213
5.029879	305.653666	5.968218
5.155387	317.121535	5.973222
6.070239	316.593160	5.978227
6.047574	326.584513	5.983232
5.967767	324.442495	5.988237
6.133019	314.704253	5.993242
5.803105	305.830872	5.998246
6.153668	310.287753	6.003251
6.031324	305.586604	6.008256
6.055097	311.834397	6.013261
5.930657	304.469744	6.018266
5.902899	302.363917	6.023270
6.091180	305.488839	6.028275
5.940975	303.373603	6.033280
6.278846	303.431762	6.038285
6.117005	297.591508	6.043290
5.748906	309.164697	6.048294
6.106111	304.407867	6.053299
6.155032	305.355720	6.058304
5.941100	307.920018	6.063309
5.651939	288.033812	6.068314
5.480033	288.611094	6.073318
5.658843	291.822908	6.078323
5.697429	310.226463	6.083328
5.863308	315.303711	6.088333
6.014192	307.304579	6.093338
5.708105	304.985827	6.098342
6.032658	311.753091	6.103347
5.993022	306.833424	6.108352
6.070476	299.351920	6.113357
5.948915	291.157937	6.118362
5.286041	294.918406	6.123366
5.755308	301.296146	6.128371
5.734779	309.157991	6.133376
5.854600	304.147061	6.138381
6.041054	303.213249	6.143386
5.891108	315.793332	6.148390
6.281538	308.221967	6.153395
5.579651	297.660145	6.158400
5.536673	290.640312	6.163405
5.894295	302.404220	6.168410
5.833313	306.536041	6.173414
5.873369	302.502458	6.178419
5.887971	309.950717	6.183424
5.709432	307.295737	6.188429
5.918606	302.916289	6.193434
6.043303	309.581793	6.198438
5.775646	298.753050	6.203443
5.600211	301.460047	6.208448
5.783257	309.913445	6.213453
6.406246	308.174525	6.218458
5.814654	311.639166	6.223462
5.897103	295.453563	6.228467
5.687745	285.014377	6.233472
5.411237	286.746873	6.238477
5.555687	298.256072	6.243482
6.002918	302.856085	6.248486
6.042293	303.397308	6.253491
6.090240	305.006525	6.258496
5.947592	294.632875	6.263501
5.926713	286.268197	6.268506
5.716337	293.077612	6.273510
5.747722	281.316487	6.278515
5.953969	285.792667	6.283520
5.943892	284.319991	6.288525
5.577462	287.199089	6.293530
5.742297	291.150218	6.298534
6.066044	291.387742	6.303539
5.902385	297.538165	6.308544
5.898094	296.706817	6.313549
5.823358	287.638693	6.318554
5.747954	288.691322	6.323558
5.675829	290.898187	6.328563
5.888317	292.105305	6.333568
5.852744	292.772090	6.338573
6.112888	287.157197	6.343578
5.877541	279.202394	6.348582
5.662112	279.833907	6.353587
5.689604	283.572306	6.358592
5.612345	287.048610	6.363597
5.641094	292.558482	6.368602
5.511300	307.685357	6.373606
6.181563	309.960132	6.378611
6.296785	307.506182	6.383616
6.073940	302.184780	6.388621
6.101915	291.243575	6.393626
5.409632	297.900237	6.398630
5.499511	288.066180	6.403635
5.843662	290.132304	6.408640
6.056193	294.895404	6.413645
6.071974	296.772214	6.418650
5.552648	292.192988	6.423654
5.811742	286.106870	6.428659
5.721222	282.251805	6.433664
5.906137	313.107013	6.438669
5.961674	296.536465	6.443674
5.729979	299.274366	6.448678
5.879894	288.070573	6.453683
5.480010	292.723384	6.458688
5.884048	298.431085	6.463693
6.026886	297.095948	6.468698
5.732082	301.137626	6.473702
6.198443	296.832029	6.478707
5.937828	293.560255	6.483712
5.465192	286.018873	6.488717
5.753106	293.854834	6.493722
5.785720	306.634273	6.498726
5.969861	300.040974	6.503731
6.154477	307.497563	6.508736
5.792395	289.040045	6.513741
5.413659	283.322148	6.518746
5.736646	291.934080	6.523750
5.997965	303.039115	6.528755
6.169407	300.848491	6.533760
5.835370	300.862569	6.538765
5.683746	289.158406	6.543770
5.441441	286.763288	6.548774
5.767053	300.196279	6.553779
6.106721	308.229829	6.558784
5.839176	306.604252	6.563789
6.033082	303.195272	6.568794
5.849092	296.871258	6.573798
5.761173	293.597905	6.578803
5.861847	297.100290	6.583808
5.884512	289.494445	6.588813
5.735215	283.206163	6.593818
5.861863	297.967243	6.598822
6.112901	291.066144	6.603827
5.812881	296.326654	6.608832
5.760828	291.813878	6.613837
6.107136	280.354890	6.618842
5.785239	289.943568	6.623846
5.730073	281.802526	6.628851
5.491565	281.668856	6.633856
5.673418	302.793017	6.638861
6.007583	314.547930	6.643866
6.086686	313.409372	6.648870
6.036391	300.025322	6.653875
5.799060	285.752931	6.658880
5.895747	284.801460	6.663885
5.680759	280.908828	6.668890
5.573687	287.445898	6.673894
5.639703	281.200021	6.678899
5.967154	302.526134	6.683904
5.897868	297.127042	6.688909
6.181422	286.902170	6.693914
5.812327	287.184293	6.698918
5.773258	292.486429	6.703923
6.055380	290.269082	6.708928
5.689984	288.937147	6.713933
5.827131	281.629850	6.718938
5.637571	291.802189	6.723942
5.607028	277.266660	6.728947
5.868252	295.632373	6.733952
6.076479	301.076339	6.738957
6.048316	281.782242	6.743962
5.546976	279.367346	6.748966
5.737221	282.422357	6.753971
6.059734	293.055961	6.758976
6.075069	291.753330	6.763981
5.973159	286.466886	6.768986
5.761922	286.427044	6.773990
5.565205	280.702955	6.778995
5.905652	294.035557	6.784000
5.427621	293.856924	6.789005
6.027855	283.418236	6.794010
5.809486	291.000835	6.799014
5.671745	290.525616	6.804019
5.821211	293.504722	6.809024
5.694320	301.968407	6.814029
6.065491	299.490427	6.819034
5.920123	305.055885	6.824038
5.892091	293.427386	6.829043
5.677821	297.526126	6.834048
5.456596	302.037229	6.839053
5.940143	308.782901	6.844058
6.233033	311.382182	6.849062
6.226168	309.700200	6.854067
5.804298	295.757084	6.859072
5.735220	293.584927	6.864077
5.623436	285.335641	6.869082
5.727620	287.600475	6.874086
5.694251	287.931565	6.879091
6.242763	292.019107	6.884096
5.896937	287.757711	6.889101
5.743853	274.475103	6.894106
6.105989	289.424133	6.899110
5.664907	292.694498	6.904115
6.152991	287.151681	6.909120
5.954476	286.309445	6.914125
5.975371	281.386689	6.919130
5.715099	292.212267	6.924134
5.550056	278.849261	6.929139
5.580516	291.220909	6.934144
5.455927	289.724933	6.939149
5.818377	284.334554	6.944154
5.929305	298.822841	6.949158
6.278277	286.964809	6.954163
5.827396	290.334773	6.959168
5.997492	283.977780	6.964173
6.254953	279.230159	6.969178
5.761451	286.852430	6.974182
5.823924	289.620458	6.979187
5.697169	291.813683	6.984192
5.731974	286.711593	6.989197
5.969148	283.112385	6.994202
5.952339	285.247364	6.999206
5.662504	288.563780	7.004211
6.049997	286.225626	7.009216
5.833215	289.777437	7.014221
5.883738	281.733832	7.019226
5.732785	285.613907	7.024230
5.931374	282.479442	7.029235
5.753594	282.377445	7.034240
5.680963	284.312311	7.039245
5.545925	281.859365	7.044250
5.823485	287.264059	7.049254
5.684405	283.040075	7.054259
5.726777	285.728976	7.059264
5.793754	288.274844	7.064269
5.639750	280.471888	7.069274
5.829675	293.808944	7.074278
5.725976	294.457862	7.079283
6.018082	301.195373	7.084288
5.879507	295.746959	7.089293
5.650100	291.552855	7.094298
5.675577	299.964344	7.099302
6.146763	311.932034	7.104307
5.893894	301.524923	7.109312
5.662984	286.409990	7.114317
5.961907	287.657432	7.119322
5.748854	295.106330	7.124326
5.788248	287.681376	7.129331
5.950571	305.227283	7.134336
5.873726	299.092226	7.139341
6.165568	280.861926	7.144346
6.020170	291.201392	7.149350
6.041673	287.847730	7.154355
6.131442	286.805589	7.159360
5.673025	286.392952	7.164365
5.911525	289.355032	7.169370
5.939299	292.957350	7.174374
5.775574	288.528399	7.179379
5.913317	276.813990	7.184384
5.630330	290.003215	7.189389
5.699087	286.202443	7.194394
5.596068	296.633389	7.199398
5.719348	293.918764	7.204403
5.416494	283.421370	7.209408
5.658666	291.251798	7.214413
5.969801	296.572174	7.219418
5.917543	305.539923	7.224422
5.725730	294.079290	7.229427
5.839740	297.690328	7.234432
5.835128	294.502080	7.239437
6.071335	289.409759	7.244442
5.755608	289.443132	7.249446
5.713825	284.748428	7.254451
5.788899	292.525780	7.259456
5.881345	299.411433	7.264461
5.965134	292.545866	7.269466
5.980304	290.930056	7.274470
5.458359	293.516998	7.279475
5.988491	305.437543	7.284480
5.704354	301.644256	7.289485
6.158870	297.672691	7.294490
5.938436	300.386694	7.299494
5.575158	291.176836	7.304499
5.757408	293.081510	7.309504
5.575713	300.595129	7.314509
6.169654	298.670911	7.319514
5.960625	291.645294	7.324518
5.741455	278.762106	7.329523
5.984166	285.301662	7.334528
5.675548	292.543980	7.339533
5.766395	285.060396	7.344538
5.751111	297.429679	7.349542
5.985994	290.913902	7.354547
5.822608	295.020537	7.359552
5.689691	298.825042	7.364557
5.967709	304.384690	7.369562
5.755337	302.117785	7.374566
6.007039	298.174634	7.379571
6.067884	290.056653	7.384576
6.019506	294.907832	7.389581
6.512567	283.055841	7.394586
6.019649	288.865228	7.399590
6.029344	295.842856	7.404595
6.014372	294.731602	7.409600
5.839750	298.384415	7.414605
5.929363	294.868290	7.419610
5.828780	302.353463	7.424614
5.674902	296.015270	7.429619
5.927524	288.088890	7.434624
5.369245	293.494011	7.439629
5.818561	288.779790	7.444634
5.785698	285.741471	7.449638
5.392688	295.287441	7.454643
5.655866	290.459834	7.459648
5.642616	294.261525	7.464653
5.688150	287.626537	7.469658
5.527338	297.297704	7.474662
5.892224	294.320840	7.479667
5.658435	301.032665	7.484672
5.872275	305.748109	7.489677
6.266051	299.628362	7.494682
5.910585	299.433809	7.499686
5.703906	300.563824	7.504691
5.824294	295.062436	7.509696
5.637017	297.242939	7.514701
5.678042	291.054733	7.519706
5.986994	296.884803	7.524710
5.840721	292.690411	7.529715
5.892961	290.426600	7.534720
5.752552	294.431583	7.539725
5.916790	288.648128	7.544730
5.633251	291.587086	7.549734
5.860966	301.548933	7.554739
5.970135	287.418741	7.559744
5.648467	295.049062	7.564749
5.861408	290.422263	7.569754
5.566332	307.435122	7.574758
6.087799	306.689590	7.579763
6.150379	309.245637	7.584768
5.755013	305.074206	7.589773
5.664057	292.449451	7.594778
5.902373	298.565761	7.599782
5.695744	300.024792	7.604787
5.911605	299.842524	7.609792
5.951186	295.043402	7.614797
5.946020	292.532270	7.619802
6.134934	297.393959	7.624806
5.520892	285.337860	7.629811
5.864029	295.430426	7.634816
5.641844	288.577698	7.639821
5.687935	296.470293	7.644826
5.856603	303.040366	7.649830
6.466723	301.970989	7.654835
6.286448	294.858638	7.659840
5.438210	295.243835	7.664845
5.986192	282.177928	7.669850
5.827292	283.309994	7.674854
5.726088	291.396360	7.679859
6.092742	284.882216	7.684864
5.906369	295.538105	7.689869
6.017658	287.450236	7.694874
5.447317	294.268242	7.699878
5.657997	293.947578	7.704883
5.965024	282.842711	7.709888
5.876276	290.012830	7.714893
6.019929	288.762987	7.719898
5.814118	288.155999	7.724902
5.596896	290.875828	7.729907
5.946480	284.003681	7.734912
5.649151	287.096642	7.739917
5.841847	283.963094	7.744922
5.769391	290.045531	7.749926
5.793326	281.613769	7.754931
5.742155	273.839096	7.759936
5.564193	292.314313	7.764941
5.801037	284.017076	7.769946
5.653795	298.045695	7.774950
5.876337	307.426232	7.779955
6.060203	302.671081	7.784960
5.685353	305.678040	7.789965
5.581333	302.255335	7.794970
6.001012	304.749455	7.799974
6.186086	309.146682	7.804979
5.803558	301.584937	7.809984
5.751346	301.890488	7.814989
6.117864	295.006209	7.819994
5.520476	289.923455	7.824998
5.589971	293.003596	7.830003
5.771392	292.064240	7.835008
5.908334	314.305863	7.840013
6.101592	310.049111	7.845018
5.804163	305.198056	7.850022
5.533221	296.442045	7.855027
5.731067	298.863137	7.860032
5.791220	316.984937	7.865037
5.977686	318.597897	7.870042
5.762784	309.178270	7.875046
6.124685	313.241089	7.880051
6.153348	309.066911	7.885056
5.740163	300.465920	7.890061
5.866986	282.523898	7.895066
5.742972	283.305690	7.900070
5.433921	289.488238	7.905075
5.789699	300.654494	7.910080
5.868464	311.120419	7.915085
6.091747	313.448969	7.920090
5.704786	307.681726	7.925094
5.971216	310.493931	7.930099
5.888232	305.065332	7.935104
5.619542	298.659594	7.940109
5.918660	296.945791	7.945114
5.970282	290.774917	7.950118
6.020042	300.115913	7.955123
5.572626	285.629465	7.960128
5.786095	284.475114	7.965146
5.832508	282.281078	7.970163
5.948768	299.183448	7.975181
5.993627	293.900299	7.980198
6.065971	281.945049	7.985216
5.726210	286.781902	7.990234
5.874173	278.746782	7.995251
5.890658	289.391309	8.000269
5.882803	286.309526	8.005286
5.995632	286.566533	8.010304
6.042650	292.778974	8.015322
5.991418	284.127964	8.020339
5.944599	287.379265	8.025357
6.090685	286.731742	8.030374
6.134922	291.240581	8.035392
5.793255	291.981737	8.040410
5.668416	285.216626	8.045427
5.809435	294.488005	8.050445
5.827033	279.612864	8.055462
5.786377	288.063666	8.060480
5.516892	297.247491	8.065498
5.903955	293.583542	8.070515
5.937557	304.402128	8.075533
6.188946	307.294596	8.080550
6.626915	305.475070	8.085568
6.063248	288.797047	8.090586
5.946944	290.607582	8.095603
6.306829	285.095518	8.100621
5.895515	285.998987	8.105638
5.748023	286.283902	8.110656
5.505898	290.329271	8.115674
5.477911	276.007153	8.120691
5.664639	288.966642	8.125709
6.107559	306.521863	8.130726
6.287090	306.519190	8.135744
6.521353	306.050430	8.140762
6.248030	297.689598	8.145779
5.926065	292.791747	8.150797
5.762906	298.550948	8.155814
5.660643	288.522564	8.160832
6.034266	305.328068	8.165850
6.164090	308.353065	8.170867
6.109338	318.068325	8.175885
6.022403	305.806517	8.180902
6.032222	308.626150	8.185920
6.230348	318.024343	8.190938
6.132457	306.303853	8.195955
5.772244	305.025142	8.200973
5.676677	308.744758	8.205990
6.141542	315.750480	8.211008
6.018846	315.599214	8.216026
6.241705	314.854535	8.221043
6.165658	314.585559	8.226061
5.954717	320.162869	8.231078
6.084792	308.154434	8.236096
6.024404	319.094954	8.241114
5.900282	317.520723	8.246131
6.202699	321.582297	8.251149
5.844095	319.435538	8.256166
6.325498	307.470227	8.261184
6.165960	307.271052	8.266202
5.934169	309.667581	8.271219
6.112711	306.941760	8.276237
5.853235	316.837208	8.281254
6.362185	311.756336	8.286272
6.116220	311.939825	8.291290
6.040727	307.357025	8.296307
6.116186	298.149827	8.301325
6.070461	320.798581	8.306342
6.357057	310.125849	8.311360
6.139798	309.531741	8.316378
6.515597	303.180952	8.321395
6.072710	301.403904	8.326413
5.910708	310.406909	8.331430
6.401358	304.312777	8.336448
5.963301	314.248651	8.341466
6.124523	310.686129	8.346483
6.281844	317.275858	8.351501
5.943698	314.605237	8.356518
6.084522	312.942421	8.361536
6.343298	308.326510	8.366554
6.053416	314.490433	8.371571
6.437350	310.890080	8.376589
6.472315	317.060228	8.381606
6.399652	305.105450	8.386624
6.301554	316.026594	8.391642
6.394758	305.737405	8.396659
6.255755	306.996086	8.401677
6.056596	309.311800	8.406694
6.086040	312.204113	8.411712
6.163932	315.227731	8.416730
6.407023	322.962223	8.421747
6.720476	322.048812	8.426765
6.543620	326.563683	8.431782
6.368508	314.126261	8.436800
6.280773	313.508831	8.441818
5.971377	311.256587	8.446835
6.246922	313.495236	8.451853
6.176102	317.731679	8.456870
6.311781	320.373936	8.461888
6.516580	323.907942	8.466906
6.368452	322.258558	8.471923
6.439001	319.451724	8.476941
6.588127	324.051532	8.481958
6.496902	321.866298	8.486976
6.317449	312.553623	8.491994
6.233790	318.319386	8.497011
6.623969	305.219633	8.502029
6.424981	308.690278	8.507046
6.456116	306.918316	8.512064
6.201300	304.073785	8.517082
6.128667	309.585380	8.522099
6.347932	332.486363	8.527117
6.601046	328.723349	8.532134
6.628586	321.745161	8.537152
6.581307	324.848226	8.542170
6.334998	324.223928	8.547187
6.493164	320.362096	8.552205
6.522574	326.955966	8.557223
6.304889	310.542773	8.562240
6.709596	321.606530	8.567258
6.231799	321.687267	8.572275
6.969873	323.408960	8.577293
6.783393	321.525720	8.582311
6.422986	310.587671	8.587328
6.451128	302.192522	8.592346
6.086113	308.806773	8.597363
6.516122	315.212042	8.602381
6.306786	328.479364	8.607399
6.522865	321.421331	8.612416
6.831862	329.420104	8.617434
6.767367	323.784764	8.622451
6.576982	326.506190	8.627469
5.878014	314.996037	8.632487
6.538534	316.878119	8.637504
6.796924	320.943392	8.642522
6.776569	334.313832	8.647539
6.732501	326.078229	8.652557
6.420572	325.044449	8.657575
6.535850	316.342254	8.662592
6.283978	318.722978	8.667610
6.575485	318.743894	8.672627
6.661613	325.600316	8.677645
6.577536	326.216166	8.682663
6.612846	329.984833	8.687680
6.678069	328.854465	8.692698
6.932516	324.349671	8.697715
6.620811	323.934360	8.702733
6.646400	327.269063	8.707751
6.831721	326.161019	8.712768
6.720443	309.582946	8.717786
6.133016	317.986356	8.722803
6.677318	324.484280	8.727821
6.668089	332.914432	8.732839
6.685912	330.623861	8.737856
6.826795	328.415111	8.742874
6.738625	330.164468	8.747891
6.624635	319.866508	8.752909
6.617075	335.642698	8.757927
6.749875	335.495831	8.762944
6.473878	329.063489	8.767962
6.454802	332.181098	8.772979
7.176744	330.052283	8.777997
6.596885	338.703819	8.783015
6.442466	326.127474	8.788032
6.715125	338.199511	8.793050
6.673787	341.175429	8.798067
6.630156	331.639636	8.803085
6.571733	337.155338	8.808103
6.803087	333.313664	8.813120
6.736731	330.117912	8.818138
6.345088	331.428552	8.823155
6.574892	325.772635	8.828173
6.686520	324.584553	8.833191
6.827488	326.266677	8.838208
6.547029	336.452565	8.843226
6.498044	341.471365	8.848243
6.572635	333.144705	8.853261
6.493852	340.055209	8.858279
6.447669	351.867647	8.863296
6.712778	356.812303	8.868314
6.515998	363.132151	8.873331
7.000204	359.885386	8.878349
7.099907	367.373993	8.883367
6.909369	361.423768	8.888384
7.263842	353.700426	8.893402
6.936899	362.602913	8.898419
7.065371	355.937183	8.903437
7.265683	355.196013	8.908455
7.157873	346.856722	8.913472
6.731367	340.952710	8.918490
7.093364	344.897721	8.923507
6.932829	333.865426	8.928525
6.819691	338.319890	8.933543
6.598447	339.711291	8.938560
6.866179	340.906648	8.943578
6.480222	335.119394	8.948595
6.931020	342.480747	8.953613
6.788925	356.334035	8.958631
7.016591	355.594917	8.963648
6.538324	364.520965	8.968666
6.456949	365.931615	8.973683
7.226630	355.092129	8.978701
6.896994	362.754872	8.983719
7.021209	356.910269	8.988736
7.419543	346.100205	8.993754
7.062826	358.768837	8.998771
7.330200	358.973382	9.003789
7.085333	359.737337	9.008807
6.767709	367.953603	9.013824
7.216854	359.171004	9.018842
7.277305	364.166461	9.023859
7.268709	339.699069	9.028877
6.827763	334.037135	9.033895
6.782394	338.023481	9.038912
6.880711	348.497521	9.043930
7.161504	350.713269	9.048947
7.233607	351.639300	9.053965
7.430717	346.401855	9.058983
7.114868	340.808799	9.064000
7.139966	341.707436	9.069018
6.837128	341.082472	9.074035
6.934013	326.210726	9.079053
6.802651	333.984589	9.084071
7.277490	351.396037	9.089088
7.164885	344.950872	9.094106
7.186603	353.464573	9.099123
7.423906	349.053955	9.104141
7.083221	340.132422	9.109159
6.795225	330.767212	9.114176
7.056220	334.538609	9.119194
6.887736	349.023970	9.124211
6.915121	344.705994	9.129229
7.167020	353.846539	9.134247
7.017621	353.456447	9.139264
7.292663	346.872035	9.144282
7.388676	355.329991	9.149299
7.238557	348.685549	9.154317
7.312809	356.638837	9.159335
7.051660	358.336238	9.164352
7.454572	352.473489	9.169370
7.327105	356.305373	9.174387
7.519578	346.451961	9.179405
7.284048	334.951685	9.184423
6.929629	335.972524	9.189440
7.063150	343.146604	9.194458
7.182940	351.922730	9.199475
7.173734	350.901773	9.204493
7.127599	350.221063	9.209511
7.194767	361.015523	9.214528
7.360654	351.544923	9.219546
7.059688	355.081946	9.224563
7.308958	346.614479	9.229581
7.077953	351.497529	9.234599
6.949024	350.772908	9.239616
7.434471	354.875417	9.244634
7.191149	357.251659	9.249651
7.193837	346.761957	9.254669
7.204175	357.517929	9.259687
6.862808	358.722918	9.264704
7.295060	353.594019	9.269722
7.173442	355.986024	9.274739
7.292554	356.286232	9.279757
7.119025	350.513234	9.284775
7.479259	350.504516	9.289792
7.318471	345.963387	9.294810
6.964528	356.930702	9.299827
7.424435	359.752845	9.304845
7.724803	366.206718	9.309863
7.332420	358.949932	9.314880
7.290907	357.785690	9.319898
7.186322	360.948174	9.324915
7.743749	365.992479	9.329933
7.839681	356.447566	9.334951
7.302630	368.812941	9.339968
7.817115	354.592481	9.344986
7.467650	355.107648	9.350003
7.557510	360.698095	9.355021
7.519340	354.771484	9.360039
7.359595	352.631627	9.365056
7.615987	348.940677	9.370074
7.384359	356.351485	9.375091
7.406240	356.846703	9.380109
7.601354	354.960848	9.385127
7.440915	357.841709	9.390144
7.509500	357.253584	9.395162
7.397586	361.610038	9.400179
7.452471	351.661286	9.405197
7.780247	351.386238	9.410215
7.487981	349.491064	9.415232
7.632078	350.260726	9.420250
7.646718	353.054371	9.425267
7.486499	358.488104	9.430285
7.496500	351.537880	9.435303
7.275188	354.560755	9.440320
7.405834	353.164593	9.445338
7.432399	355.618729	9.450355
7.378617	352.279012	9.455373
7.457053	355.924211	9.460391
7.207524	361.097310	9.465408
7.479571	370.121123	9.470426
7.766243	377.893033	9.475443
7.769245	375.538496	9.480461
7.819461	374.287391	9.485479
7.448502	363.505579	9.490496
7.378577	356.119698	9.495514
7.490494	372.095057	9.500531
7.572558	373.612798	9.505549
7.355740	373.845395	9.510567
7.740033	383.637492	9.515584
7.750544	379.088618	9.520602
7.845431	376.546215	9.525619
7.836554	382.776857	9.530637
7.761893	380.374454	9.535655
7.882794	385.647668	9.540672
7.758416	370.475836	9.545690
7.628410	364.639255	9.550707
7.798920	363.874324	9.555725
7.415865	358.692492	9.560743
7.504191	366.921289	9.565760
7.589794	370.981919	9.570778
7.829298	377.770303	9.575795
7.694287	377.242277	9.580813
7.892756	383.393303	9.585831
7.972507	386.120013	9.590848
7.426032	382.923269	9.595866
8.035453	387.208444	9.600883
7.739084	373.000613	9.605901
7.825270	371.406255	9.610919
7.885746	368.443200	9.615936
7.926402	368.787180	9.620954
7.733567	375.336780	9.625971
7.709881	384.684341	9.630989
7.951352	375.785753	9.636007
7.698632	374.515546	9.641024
7.584779	373.343633	9.646042
7.551010	379.347788	9.651059
7.466258	374.687522	9.656077
7.733075	367.457478	9.661095
7.742788	379.677775	9.666112
7.879995	372.215459	9.671130
7.719682	367.791009	9.676147
7.569849	379.594357	9.681165
7.753197	373.671118	9.686183
7.760664	376.705711	9.691200
7.935054	370.105406	9.696218
8.052443	374.281002	9.701235
7.497829	377.958501	9.706253
7.958145	379.537264	9.711271
7.632224	383.188624	9.716288
8.247730	387.485474	9.721306
8.036317	387.164993	9.726323
7.463709	386.651454	9.731341
8.133646	395.357724	9.736359
7.786070	401.069936	9.741376
7.780136	402.481465	9.746394
7.956475	394.975179	9.751411
7.659145	409.619498	9.756429
8.091041	405.418398	9.761447
7.921088	410.017418	9.766464
7.806021	405.503867	9.771482
8.268295	405.731713	9.776499
7.898732	407.117812	9.781517
8.646358	395.732654	9.786535
8.502862	405.546980	9.791552
7.925530	402.298236	9.796570
8.122085	406.079681	9.801587
8.044242	401.705495	9.806605
7.968327	402.667197	9.811623
7.945960	411.083653	9.816640
8.300745	405.947866	9.821658
8.384732	407.468466	9.826675
7.884758	398.038400	9.831693
8.288062	401.440534	9.836711
7.996186	391.283832	9.841728
8.357480	394.929178	9.846746
8.271306	375.800534	9.851763
7.877123	379.834887	9.856781
8.031031	380.003453	9.861799
7.949275	395.639778	9.866816
8.127303	399.714426	9.871834
8.637965	395.283325	9.876851
8.079966	399.103360	9.881869
8.322314	383.322182	9.886887
8.184899	385.249617	9.891904
7.897575	385.010379	9.896922
8.248931	387.372927	9.901939
8.049113	404.895780	9.906957
8.616825	398.350984	9.911975
8.335719	395.718804	9.916992
8.146741	391.989896	9.922010
8.260011	379.611663	9.927027
7.616797	390.583014	9.932045
8.396452	400.411389	9.937063
8.183724	403.360356	9.942080
8.425499	398.772314	9.947098
8.889581	404.149883	9.952115
8.041506	394.837130	9.957133
8.026999	391.595427	9.962151
8.073035	402.980151	9.967168
8.269645	406.225130	9.972186
8.364982	407.914367	9.977203
8.119200	412.427368	9.982221
8.302185	395.049201	9.987239
8.230113	405.635006	9.992256
7.951112	403.068766	9.997274
8.095644	404.892347	10.002291
7.791073	412.645878	10.007309
8.250654	409.712190	10.012327
8.196700	401.159372	10.017344
8.115739	405.372169	10.022362
8.123117	406.876296	10.027379
8.559676	408.525028	10.032397
8.631468	422.682720	10.037415
8.319907	420.478134	10.042432
8.482165	416.984854	10.047450
8.521929	419.541079	10.052467
8.373901	417.260542	10.057485
8.542103	410.427668	10.062503
8.197125	412.652496	10.067520
8.418220	431.469922	10.072538
8.661129	423.117013	10.077555
8.552606	424.964217	10.082573
8.359316	418.317005	10.087591
8.751313	418.688330	10.092608
8.364660	415.567677	10.097626
8.567574	409.411017	10.102643
8.511418	406.330422	10.107661
8.261877	397.845925	10.112679
8.446241	408.057308	10.117696
8.607990	424.176426	10.122714
8.785152	425.070326	10.127731
8.321809	417.818252	10.132749
8.546864	421.024092	10.137767
8.626883	425.350678	10.142784
8.843177	431.972292	10.147802
8.792046	424.185845	10.152819
8.560692	421.214571	10.157837
8.685070	409.916974	10.162855
8.208682	417.643613	10.167872
7.983805	418.817847	10.172890
8.671996	421.153201	10.177907
8.785829	427.740275	10.182925
8.929619	432.331475	10.187943
8.764205	428.277015	10.192960
8.822493	432.253554	10.197978
8.627923	427.525170	10.202995
8.464198	424.581234	10.208013
8.781003	424.879064	10.213031
8.907802	424.127247	10.218048
8.526813	433.615667	10.223066
8.825642	425.411833	10.228083
8.789630	428.207064	10.233101
8.468864	420.260639	10.238119
8.695677	429.780650	10.243136
8.476286	434.087587	10.248154
8.827837	430.078862	10.253171
8.501038	429.710077	10.258189
8.515707	427.745017	10.263207
8.436414	431.828179	10.268224
8.362677	436.554229	10.273242
8.751304	429.131635	10.278259
8.518481	435.510766	10.283277
8.728185	421.331395	10.288295
8.587320	428.021238	10.293312
8.497613	432.200691	10.298330
8.809415	429.895893	10.303347
8.883298	435.810726	10.308365
9.047087	435.239333	10.313383
8.979783	433.081918	10.318400
8.836026	425.679102	10.323418
9.091725	427.012031	10.328435
9.122150	425.805027	10.333453
9.145233	432.444101	10.338471
9.034895	427.876162	10.343488
8.961981	431.595432	10.348506
8.946901	423.516208	10.353523
8.816088	430.617876	10.358541
8.789099	426.052739	10.363559
9.022476	423.514012	10.368576
8.526465	424.320227	10.373594
8.880069	419.197243	10.378611
8.338159	416.697180	10.383629
8.410200	425.013741	10.388647
9.170098	435.892886	10.393664
8.862326	445.985263	10.398682
9.050561	439.266018	10.403699
8.967359	443.472862	10.408717
9.085990	445.593955	10.413735
9.171009	447.616146	10.418752
9.074532	454.649364	10.423770
9.061054	440.801357	10.428787
8.732455	434.629618	10.433805
9.192810	447.249990	10.438823
9.264901	446.916924	10.443840
8.971417	437.195925	10.448858
9.087089	442.242763	10.453875
9.019892	442.436287	10.458893
9.135029	449.193571	10.463911
9.486211	441.221408	10.468928
8.869022	436.467307	10.473946
8.958305	422.268817	10.478963
9.003121	431.391153	10.483981
9.109701	436.455183	10.488999
9.671931	439.599063	10.494016
9.368482	435.913213	10.499034
9.558459	428.704576	10.504051
9.267605	420.131831	10.509069
9.186486	425.515401	10.514087
9.175095	414.119026	10.519104
8.764557	423.930761	10.524122
9.083907	421.277668	10.529139
9.201788	427.248761	10.534157
8.769463	420.793391	10.539175
8.996115	421.231483	10.544192
8.838605	440.906244	10.549210
9.153125	438.509508	10.554227
9.123724	441.546697	10.559245
9.254362	449.147281	10.564263
9.424151	445.766426	10.569280
9.101475	448.050899	10.574298
9.325007	444.472338	10.579315
9.112277	455.758537	10.584333
9.384627	457.129898	10.589351
9.550696	447.510904	10.594368
9.091277	459.977858	10.599386
9.288507	450.656952	10.604403
9.508764	445.081376	10.609421
9.422855	453.204802	10.614439
9.355410	454.963568	10.619456
9.368766	460.111543	10.624474
9.229792	454.468824	10.629491
9.133663	438.793943	10.634509
8.988789	448.157251	10.639527
9.440230	449.967764	10.644544
9.289420	455.387439	10.649562
9.144615	444.097019	10.654579
9.688195	452.696765	10.659597
9.506612	460.248140	10.664615
9.436946	451.915483	10.669632
9.451314	452.900999	10.674650
9.511837	442.793536	10.679667
9.329434	455.618125	10.684685
9.223543	451.557547	10.689703
9.252503	445.374313	10.694720
9.169686	447.100759	10.699738
8.762949	443.326853	10.704755
9.489442	451.560465	10.709773
9.649908	465.972615	10.714791
9.665758	474.468353	10.719808
9.867490	460.845587	10.724826
9.417680	451.956765	10.729843
9.372709	451.083375	10.734861
9.398630	457.816686	10.739879
9.600405	462.701808	10.744896
9.610628	474.757997	10.749914
9.355322	473.311469	10.754931
9.684996	467.109809	10.759949
9.406438	474.338634	10.764967
9.668049	476.030390	10.769984
9.848060	478.280779	10.775002
9.790292	476.285968	10.780019
9.606829	460.883429	10.785037
9.193211	462.961168	10.790055
9.275535	465.886296	10.795072
9.825496	467.495289	10.800090
10.037906	477.825415	10.805107
9.767726	481.550164	10.810125
9.824793	480.916493	10.815143
9.658468	469.279130	10.820160
9.497476	463.646147	10.825178
9.548639	480.804966	10.830195
9.645693	474.147239	10.835213
9.387798	484.503259	10.840231
10.004591	481.109603	10.845248
9.495068	480.725087	10.850266
9.463225	479.669779	10.855283
9.775119	474.830971	10.860301
9.086003	481.208582	10.865319
9.686947	475.529545	10.870336
9.569368	480.312923	10.875354
9.567487	476.182500	10.880371
9.773858	471.237052	10.885389
9.390391	479.050230	10.890407
9.965756	481.573564	10.895424
10.124163	492.196116	10.900442
9.528867	479.129755	10.905459
10.044799	485.322901	10.910477
9.723174	495.761430	10.915495
10.352826	485.032026	10.920512
10.115303	478.792446	10.925530
10.096282	478.382051	10.930547
10.030600	471.270003	10.935565
9.780824	476.929145	10.940583
9.990686	469.061019	10.945600
9.720331	476.768227	10.950618
9.779059	470.034422	10.955635
9.893490	467.520519	10.960653
9.811765	472.405605	10.965671
10.305344	473.509005	10.970688
10.166093	474.190252	10.975706
10.006413	472.129262	10.980723
10.190490	469.453044	10.985741
10.008161	475.931620	10.990759
10.056229	478.764259	10.995776
10.155452	477.171018	11.000794
10.069718	471.908149	11.005811
9.903983	469.775522	11.010829
9.782594	477.904484	11.015847
9.999261	473.525450	11.020864
10.159304	466.984145	11.025882
10.047157	471.160789	11.030899
10.253040	474.457982	11.035917
10.069783	475.524759	11.040935
10.197692	469.562785	11.045952
10.447960	467.441123	11.050970
10.133009	473.934036	11.055987
10.011841	474.353704	11.061005
9.966726	470.775942	11.066023
10.002471	469.615442	11.071040
9.996455	468.840123	11.076058
9.934137	467.824273	11.081075
10.082364	466.321229	11.086093
9.989307	472.498740	11.091111
10.137416	466.745051	11.096128
10.118238	472.844791	11.101146
10.023624	470.593798	11.106163
10.424277	481.658286	11.111181
10.046090	483.613751	11.116199
10.112585	490.413336	11.121216
10.494691	495.399773	11.126234
10.205764	492.374338	11.131251
10.771959	485.031367	11.136269
10.242857	483.406571	11.141287
10.151781	474.720648	11.146304
10.032071	474.575227	11.151322
10.061204	488.562897	11.156339
10.469777	494.046961	11.161357
10.328655	496.331574	11.166375
9.964169	502.087474	11.171392
10.161314	489.519390	11.176410
10.095000	495.853684	11.181427
10.501080	497.346233	11.186445
10.591236	498.714408	11.191463
10.443656	494.467817	11.196480
10.564191	503.253368	11.201498
10.408096	494.662761	11.206515
10.552374	502.128707	11.211533
10.309101	501.832118	11.216551
10.682391	494.531800	11.221568
10.534531	501.528858	11.226586
10.626435	507.308372	11.231603
10.248107	485.179888	11.236621
10.089747	502.065250	11.241639
10.488649	500.602065	11.246656
10.621649	495.358780	11.251674
10.406903	497.850506	11.256691
10.443117	491.479943	11.261709
10.529753	506.938676	11.266727
10.267461	502.365976	11.271744
10.437927	491.648104	11.276762
10.641960	495.226442	11.281779
10.489162	498.421702	11.286797
10.374900	501.058723	11.291815
10.499588	503.677474	11.296832
10.722199	500.875337	11.301850
10.544183	504.282797	11.306867
10.681340	493.074672	11.311885
10.978885	490.011573	11.316903
10.768560	493.278902	11.321920
10.528836	491.441800	11.326938
10.629342	505.235342	11.331955
10.548566	490.482634	11.336973
10.647540	493.449353	11.341991
10.350809	495.559387	11.347008
11.020673	495.455127	11.352026
10.495404	497.490295	11.357043
10.778286	491.478939	11.362061
10.733499	495.581989	11.367079
10.834826	494.909871	11.372096
11.201688	495.979356	11.377114
10.680162	495.442081	11.382131
10.913011	495.674093	11.387149
11.010657	494.671204	11.392167
10.900016	496.477722	11.397184
11.156438	491.881065	11.402202
10.538652	472.494276	11.407219
10.577045	462.832038	11.412237
10.621937	482.276526	11.417255
10.847745	491.673657	11.422272
10.838663	492.542911	11.427290
10.859640	497.623442	11.432307
10.693185	489.236413	11.437325
10.735423	497.317819	11.442343
10.599990	493.138760	11.447360
10.654614	484.357568	11.452378
10.864603	492.693706	11.457395
10.904317	492.785383	11.462413
10.953347	502.885354	11.467431
10.555996	497.001995	11.472448
10.842776	491.529650	11.477466
10.637045	497.150384	11.482483
10.690311	499.846523	11.487501
10.653245	493.635685	11.492519
10.985841	500.400154	11.497536
10.927471	497.685945	11.502554
10.185320	513.737605	11.507571
10.963218	512.354260	11.512589
10.773918	520.803069	11.517607
10.811635	522.753742	11.522624
11.131015	519.832398	11.527642
10.908258	521.034710	11.532659
11.021513	521.512550	11.537677
10.847949	527.983469	11.542695
10.879871	524.425258	11.547712
10.914128	520.257641	11.552730
10.762687	525.869931	11.557747
10.730396	520.153779	11.562765
10.649606	524.877795	11.567783
11.250919	542.620017	11.572800
11.403203	540.485202	11.577818
11.310751	540.108328	11.582835
11.328422	545.817365	11.587853
11.231786	534.573034	11.592871
10.916386	533.839571	11.597888
11.212149	541.392395	11.602906
11.563433	550.321916	11.607923
11.149252	524.879204	11.612941
11.181966	520.806497	11.617959
10.964581	539.048552	11.622976
11.426651	531.365183	11.627994
11.143642	548.560318	11.633011
11.558126	545.217082	11.638029
11.305934	529.844119	11.643047
11.001449	517.754885	11.648064
11.275274	524.941906	11.653082
11.376935	544.122014	11.658099
11.603411	537.011787	11.663117
11.631964	524.375257	11.668135
11.217452	522.035216	11.673152
11.418691	518.592648	11.678170
11.149041	516.763360	11.683187
11.567510	517.206302	11.688205
11.520613	513.559383	11.693223
11.284609	520.737422	11.698240
11.277361	516.014561	11.703258
11.066585	523.816650	11.708275
11.409203	528.919693	11.713293
11.794815	542.072453	11.718311
11.431867	535.984919	11.723328
11.570066	520.986662	11.728346
11.081441	530.302551	11.733363
11.486232	531.599652	11.738381
11.697814	535.896315	11.743399
11.378263	533.206986	11.748416
11.542236	524.790584	11.753434
11.200002	536.049662	11.758451
11.099160	543.048882	11.763469
11.736620	541.930387	11.768487
11.344892	549.375670	11.773504
11.642956	541.856681	11.778522
11.758873	553.896467	11.783539
11.662636	552.967941	11.788557
11.643289	548.505720	11.793575
11.562945	557.038564	11.798592
11.712830	550.085417	11.803610
11.421695	554.252081	11.808627
11.612385	558.870724	11.813645
11.832109	539.403956	11.818663
11.534049	545.663902	11.823680
11.803436	541.854130	11.828698
11.341047	544.434910	11.833715
11.851616	538.709967	11.838733
12.039992	536.203475	11.843751
11.839960	547.948482	11.848768
11.791006	545.851310	11.853786
11.811985	545.371572	11.858803
11.636444	547.459588	11.863821
11.771955	542.537775	11.868839
11.802673	550.791404	11.873856
11.765254	542.721916	11.878874
11.823934	539.292074	11.883891
11.581410	546.471138	11.888909
11.795208	550.398246	11.893927
11.545094	546.470550	11.898944
11.528020	547.934317	11.903962
11.625934	550.030247	11.908979
11.631761	545.658777	11.913997
11.849383	541.295356	11.919015
11.635983	542.161711	11.924032
11.726737	547.890927	11.929050
12.104702	550.053703	11.934067
11.864434	550.583430	11.939085
11.609259	547.372858	11.944103
11.606799	555.088881	11.949120
11.654468	554.658634	11.954138
12.247362	565.522837	11.959155
11.732010	559.257060	11.964173
12.128776	561.647274	11.969191
11.844665	562.878075	11.974208
12.118629	567.439576	11.979226
11.955022	567.458772	11.984243
12.178676	568.345440	11.989261
12.046808	562.805717	11.994279
11.839929	566.018876	11.999296
11.961401	569.512258	12.004314
12.122917	573.065675	12.009331
12.093123	583.941636	12.014349
12.336797	580.050656	12.019367
12.128952	570.874803	12.024384
12.371223	567.012446	12.029402
12.297259	563.855704	12.034419
12.174627	550.529514	12.039437
12.257756	545.435983	12.044455
11.712924	545.340973	12.049472
11.986074	550.675734	12.054490
11.991168	565.509770	12.059507
12.065408	572.421785	12.064525
12.450229	571.560364	12.069543
12.422588	573.641133	12.074560
12.067686	575.823347	12.079578
12.269314	573.740802	12.084595
12.285297	578.979918	12.089613
12.711298	566.499219	12.094631
12.065578	559.158722	12.099648
12.051853	548.794528	12.104666
12.174842	557.163176	12.109683
11.871935	575.469074	12.114701
12.195405	569.927879	12.119719
12.312449	575.226995	12.124736
12.376106	569.751497	12.129754
12.389974	572.592631	12.134771
12.537628	573.522689	12.139789
12.834596	572.258398	12.144807
11.855971	574.168509	12.149824
12.079361	573.231241	12.154842
12.272046	569.158862	12.159859
12.215523	577.284081	12.164877
12.405243	566.746195	12.169895
12.596792	576.274931	12.174912
12.206104	572.874024	12.179930
12.190761	578.143262	12.184947
12.078598	566.961285	12.189965
12.348060	574.972636	12.194983
11.914600	577.182859	12.200000
12.545779	595.898743	12.205018
12.740593	595.265712	12.210035
12.707018	596.176652	12.215053
12.490099	580.141773	12.220071
12.558177	580.143830	12.225088
12.419696	584.838976	12.230106
12.498982	597.474606	12.235123
12.523182	598.461755	12.240141
12.917456	602.202991	12.245159
12.576093	608.081553	12.250176
12.854668	593.806118	12.255194
12.729779	587.132414	12.260211
12.388171	583.670216	12.265229
12.659753	585.518214	12.270247
12.758858	590.147969	12.275264
12.599273	595.158815	12.280282
12.718761	593.218440	12.285299
12.566526	593.362093	12.290317
12.840487	595.367505	12.295335
12.896531	594.219616	12.300352
12.637398	600.205287	12.305370
12.792485	593.535325	12.310387
12.436601	603.663683	12.315405
12.742864	583.381852	12.320423
12.613468	586.791225	12.325440
12.741793	591.968674	12.330458
12.853924	594.056085	12.335475
13.152640	586.732627	12.340493
13.256699	586.157906	12.345511
12.648228	596.855741	12.350528
12.680942	593.638205	12.355546
13.009111	593.448296	12.360563
12.624215	591.712679	12.365581
12.886975	597.099562	12.370599
12.688784	600.459691	12.375616
12.866640	601.681682	12.380634
13.118891	597.738872	12.385651
13.065053	600.918742	12.390669
13.150602	594.404767	12.395687
12.941073	601.417777	12.400704
13.273313	603.347847	12.405722
13.235828	596.262916	12.410739
13.094056	601.340415	12.415757
13.158651	597.622474	12.420775
13.308313	592.827828	12.425792
12.984461	591.253112	12.430810
12.909282	588.812894	12.435827
12.872361	595.347766	12.440845
13.078582	593.273971	12.445863
12.847135	599.454140	12.450880
12.801942	592.184225	12.455898
13.195873	591.485480	12.460915
12.989185	591.533473	12.465933
13.251093	597.128764	12.470951
12.961365	602.964572	12.475968
12.894405	605.461705	12.480986
12.901206	595.722266	12.486003
12.701711	601.903772	12.491021
13.294988	601.322306	12.496039
13.055437	603.193085	12.501056
12.761310	603.081130	12.506074
13.332240	609.363584	12.511091
13.072697	615.100026	12.516109
13.581915	627.687673	12.521127
13.492556	625.609404	12.526144
13.155356	619.098127	12.531162
13.382423	608.245145	12.536179
13.313150	617.931272	12.541197
13.593569	616.641154	12.546215
13.291829	602.045827	12.551232
13.199690	601.896113	12.556250
13.489725	604.669008	12.561267
13.438764	620.048282	12.566285
13.413964	606.615303	12.571303
13.051650	612.077422	12.576320
13.186441	623.984935	12.581338
13.657266	614.192174	12.586355
13.441120	623.538269	12.591373
13.406714	630.599761	12.596391
13.803996	619.354211	12.601408
13.472661	625.903377	12.606426
13.542347	619.697963	12.611443
13.509255	616.437023	12.616461
13.751109	621.322260	12.621479
13.462677	610.458024	12.626496
13.607006	618.252200	12.631514
13.655204	602.447411	12.636531
13.434362	602.377693	12.641549
13.839720	612.381223	12.646567
13.390094	597.547004	12.651584
13.420721	611.326263	12.656602
14.125798	604.722137	12.661619
13.695257	614.552870	12.666637
13.609022	604.944672	12.671655
13.587168	595.878698	12.676672
13.305327	605.815656	12.681690
13.649745	600.914948	12.686707
13.624001	616.299760	12.691725
13.600041	613.583330	12.696743
13.682809	616.691443	12.701760
13.186539	618.633751	12.706778
13.795888	615.405324	12.711795
13.729810	609.296788	12.716813
13.605276	607.681572	12.721831
13.604128	612.986478	12.726848
13.743052	610.430874	12.731866
13.987587	616.792549	12.736883
13.832325	617.217529	12.741901
13.774302	617.867200	12.746919
13.923809	612.100623	12.751936
13.950431	609.953808	12.756954
14.080980	606.837798	12.761971
13.937639	616.762665	12.766989
13.613673	623.320149	12.772007
13.778775	611.369170	12.777024
13.672487	615.794235	12.782042
14.030723	611.042845	12.787059
13.615457	608.917495	12.792077
13.613661	621.288067	12.797095
14.191871	620.282929	12.802112
13.906251	640.981364	12.807130
14.063921	632.139875	12.812147
14.143781	642.989333	12.817165
13.846219	638.630364	12.822183
14.185459	633.613693	12.827200
13.862087	637.488761	12.832218
13.934263	647.676725	12.837235
14.010388	642.271844	12.842253
13.939191	651.103099	12.847271
14.440585	635.316079	12.852288
14.002968	638.779763	12.857306
14.302360	632.245102	12.862323
14.194212	638.677475	12.867341
14.207468	638.255740	12.872359
14.119483	630.225642	12.877376
14.393043	643.509528	12.882394
14.165528	635.838810	12.887411
14.100651	643.785486	12.892429
13.940587	638.426848	12.897447
14.431402	636.103619	12.902464
14.293055	637.106611	12.907482
14.459597	637.879103	12.912499
14.305571	633.478853	12.917517
14.298588	641.050456	12.922535
14.290017	641.323213	12.927552
14.160842	639.371058	12.932570
14.569683	627.666130	12.937587
14.646453	631.658770	12.942605
14.289537	638.287660	12.947623
14.407683	631.339423	12.952640
14.130485	640.322662	12.957658
14.275592	633.739442	12.962675
14.160586	639.140975	12.967693
14.316420	633.972986	12.972711
14.447030	640.566994	12.977728
14.345120	635.164589	12.982746
14.336184	635.099746	12.987763
14.142781	637.430384	12.992781
14.500953	630.457400	12.997799
14.582935	632.789341	13.002816
14.427825	635.044592	13.007834
14.714487	629.606936	13.012851
14.596043	626.283546	13.017869
14.393156	632.620219	13.022887
14.449589	630.266796	13.027904
14.293657	646.990978	13.032922
14.766548	651.237517	13.037939
15.054818	648.781726	13.042957
14.434608	647.682321	13.047975
14.745906	644.907377	13.052992
14.897808	657.433918	13.058010
14.660404	642.399368	13.063027
14.818518	636.303252	13.068045
14.793986	632.807456	13.073063
14.966059	638.760716	13.078080
14.775963	632.551565	13.083098
14.917115	631.100099	13.088115
14.591682	632.895894	13.093133
14.487036	638.308437	13.098151
14.776319	629.339165	13.103168
14.653243	656.651862	13.108186
15.070653	658.373026	13.113203
14.896538	652.473793	13.118221
14.443062	650.250249	13.123239
15.039688	647.468749	13.128256
15.025098	654.864823	13.133274
15.350991	653.466640	13.138291
14.890296	636.825905	13.143309
14.723491	642.169235	13.148327
14.840069	634.082040	13.153344
15.230915	650.888345	13.158362
14.776010	648.103313	13.163379
15.222060	646.402411	13.168397
14.557544	650.560961	13.173415
15.109546	649.187532	13.178432
14.745435	655.672387	13.183450
14.723470	651.314685	13.188467
15.059801	655.112289	13.193485
15.373994	662.580249	13.198503
15.105811	656.951271	13.203520
14.694078	665.280152	13.208538
14.869144	660.973819	13.213555
15.107017	663.776935	13.218573
15.046000	664.644817	13.223591
14.703278	660.409634	13.228608
15.044663	667.138086	13.233626
14.989383	669.781727	13.238643
15.158670	654.377745	13.243661
15.028956	664.616086	13.248679
15.412457	664.909848	13.253696
14.876993	664.870180	13.258714
15.263057	676.066444	13.263731
15.869493	681.668078	13.268749
15.876087	672.556612	13.273767
15.692186	652.032295	13.278784
15.713613	656.213431	13.283802
15.576140	649.484860	13.288819
15.735460	655.083519	13.293837
15.464214	654.939600	13.298855
15.827423	652.216531	13.303872
15.471749	647.595219	13.308890
15.020844	636.380736	13.313907
15.619543	645.486370	13.318925
15.338449	643.665161	13.323943
15.556747	643.943620	13.328960
15.704241	646.905967	13.333978
15.476649	649.645857	13.338995
15.608500	637.731594	13.344013
15.471668	647.030640	13.349031
15.510886	639.782276	13.354048
15.469458	654.475312	13.359066
15.673523	653.298061	13.364083
15.723458	650.690037	13.369101
15.283323	648.495973	13.374119
15.709021	653.093830	13.379136
15.982102	646.822026	13.384154
15.443964	639.944410	13.389171
15.562525	634.305716	13.394189
15.487345	659.010679	13.399207
15.428855	653.967568	13.404224
15.426689	650.408328	13.409242
15.686426	651.589172	13.414259
15.413915	656.538725	13.419277
15.360168	659.109545	13.424295
15.206164	654.665107	13.429312
15.621157	655.452563	13.434330
15.559092	655.635824	13.439347
15.611783	649.653944	13.444365
15.533919	668.183665	13.449383
16.212711	665.862722	13.454400
16.049981	674.594635	13.459418
15.620681	659.706709	13.464435
15.949253	652.309151	13.469453
15.615297	670.291789	13.474471
16.000304	672.491352	13.479488
16.283289	675.694531	13.484506
15.908573	669.829680	13.489523
15.709103	667.191060	13.494541
15.574604	669.045490	13.499559
16.104860	667.997325	13.504576
16.065373	670.900429	13.509594
16.321051	681.056686	13.514611
16.384776	674.378828	13.519629
16.308333	671.686339	13.524647
16.108249	649.757107	13.529664
15.849108	657.248060	13.534682
15.645317	661.969173	13.539699
16.060225	661.005238	13.544717
16.136915	671.997213	13.549735
16.197692	669.933432	13.554752
16.281436	675.793163	13.559770
15.864419	681.648815	13.564787
16.088270	668.044537	13.569805
16.116087	682.528007	13.574823
16.179112	681.098168	13.579840
15.968256	690.759044	13.584858
16.217906	691.171473	13.589875
16.344807	673.767054	13.594893
15.879876	680.983956	13.599911
15.913780	683.935593	13.604928
16.089461	676.476626	13.609946
16.038319	669.775630	13.614963
16.102780	675.733035	13.619981
16.132823	683.627082	13.624999
16.422983	685.945552	13.630016
16.515377	688.613538	13.635034
16.185081	696.923443	13.640051
16.676173	687.645020	13.645069
16.076800	693.806769	13.650087
16.198656	692.904237	13.655104
16.406788	694.067874	13.660122
16.564209	701.970499	13.665139
16.902066	695.669659	13.670157
16.708119	706.776373	13.675175
16.462146	691.348654	13.680192
16.612547	690.422744	13.685210
16.453873	693.391743	13.690227
16.766880	684.642804	13.695245
16.559980	685.321969	13.700263
16.531943	690.116707	13.705280
16.575720	685.505773	13.710298
16.844912	696.205869	13.715315
17.061250	686.301217	13.720333
16.544668	684.179010	13.725351
16.389070	670.952532	13.730368
16.794731	666.256858	13.735386
16.539673	681.822591	13.740403
16.594974	681.946554	13.745421
16.702759	689.310967	13.750439
16.699039	702.325655	13.755456
17.015084	689.208761	13.760474
16.776658	695.232265	13.765491
16.924506	687.872297	13.770509
16.964187	686.323021	13.775527
16.786761	680.632570	13.780544
16.605303	671.036006	13.785562
16.975658	679.246282	13.790579
16.764910	683.987418	13.795597
17.012881	691.393119	13.800615
16.718075	693.266199	13.805632
16.897977	693.825182	13.810650
16.765574	695.761336	13.815667
16.682933	693.495828	13.820685
16.352277	694.831711	13.825703
16.624473	691.614740	13.830720
16.599717	686.642104	13.835738
16.638842	693.045256	13.840755
17.121372	704.740896	13.845773
16.995228	717.241344	13.850791
17.116250	711.810518	13.855808
17.796222	711.414360	13.860826
17.352333	702.612850	13.865843
17.426935	689.356829	13.870861
17.138298	684.235937	13.875879
17.078205	687.741833	13.880896
17.227817	674.931719	13.885914
17.074218	688.480955	13.890931
17.446495	689.003674	13.895949
17.053865	682.412644	13.900967
16.973833	687.966532	13.905984
17.211693	686.313819	13.911002
16.866108	696.560543	13.916019
17.115562	699.074694	13.921037
17.206822	704.226389	13.926055
17.394578	709.808015	13.931072
17.432197	711.528358	13.936090
17.505955	717.272897	13.941107
17.525588	715.852968	13.946125
17.395522	709.694401	13.951143
17.144244	718.339140	13.956160
17.814133	719.086914	13.961178
17.500638	710.034733	13.966195
17.146023	697.303108	13.971213
17.366768	707.010399	13.976231
17.651537	714.558698	13.981248
18.026017	700.631152	13.986266
17.864892	697.812993	13.991283
17.729922	687.997751	13.996301
17.598541	686.178473	14.001319
17.533540	684.967376	14.006336
17.831114	680.796592	14.011354
17.338234	688.974023	14.016371
17.321442	686.881294	14.021389
17.408144	680.203012	14.026407
17.314703	682.439200	14.031424
17.524788	693.804881	14.036442
17.579346	702.468264	14.041459
17.647579	700.027791	14.046477
17.730320	702.766708	14.051495
17.516145	702.178417	14.056512
18.069606	706.024274	14.061530
17.775619	707.326048	14.066547
18.003575	703.254458	14.071565
17.743405	704.033432	14.076583
17.471268	709.298511	14.081600
17.785980	708.040915	14.086618
17.502054	702.259745	14.091635
17.590190	701.476068	14.096653
17.484511	709.378635	14.101671
17.730277	708.800781	14.106688
17.666627	698.901848	14.111706
17.931849	723.743244	14.116723
18.417852	717.384617	14.121741
18.323948	703.662533	14.126759
17.964383	703.393514	14.131776
17.658009	702.753308	14.136794
17.784311	704.289435	14.141811
18.096015	713.537615	14.146829
18.182978	724.931952	14.151847
18.045197	719.241627	14.156864
18.022478	719.598637	14.161882
17.943880	726.771185	14.166899
17.976919	723.332677	14.171917
18.361699	725.781582	14.176935
18.300998	721.098546	14.181952
18.529105	722.710339	14.186970
18.126550	714.808072	14.191987
18.028268	725.656915	14.197005
18.537275	718.815041	14.202023
18.196152	719.704446	14.207040
18.243174	720.574443	14.212058
17.820142	729.047120	14.217075
18.332924	726.837220	14.222093
18.593880	728.794182	14.227111
18.355646	733.148304	14.232128
18.211637	733.072933	14.237146
18.453303	733.855823	14.242163
18.433889	730.595888	14.247181
18.502965	730.102346	14.252199
18.052963	729.036392	14.257216
18.164369	723.603904	14.262234
18.051024	736.152864	14.267251
18.252555	741.972189	14.272269
18.253913	729.226142	14.277287
17.899383	734.702866	14.282304
18.396838	737.074272	14.287322
18.478412	749.842193	14.292339
18.567307	744.334311	14.297357
18.678678	747.949218	14.302375
18.883071	751.038418	14.307392
18.683207	758.801042	14.312410
18.482171	748.601590	14.317427
18.390934	759.039115	14.322445
18.937332	748.805338	14.327463
18.755627	755.514285	14.332480
19.093802	749.866607	14.337498
18.933560	748.061284	14.342515
19.037725	747.707440	14.347533
18.784139	732.965657	14.352551
18.826946	726.234234	14.357568
18.722842	722.223807	14.362586
18.739559	725.780866	14.367603
18.904160	725.739494	14.372621
19.020998	724.190824	14.377639
18.651447	728.716864	14.382656
18.995189	727.110776	14.387674
18.836169	733.547948	14.392691
19.126584	740.707229	14.397709
19.300961	730.518762	14.402727
18.964173	733.209397	14.407744
18.930866	720.973665	14.412762
18.760781	730.303178	14.417779
18.678945	733.266532	14.422797
19.111292	741.893204	14.427815
19.036678	756.058178	14.432832
19.255089	752.486664	14.437850
19.422120	747.799721	14.442867
19.327837	739.322445	14.447885
19.270057	736.917365	14.452903
19.152059	732.909099	14.457920
19.185536	725.390204	14.462938
19.073415	722.665394	14.467955
18.890368	722.867492	14.472973
19.737772	731.940760	14.477991
18.910254	732.713398	14.483008
19.211400	728.242256	14.488026
19.311450	735.478509	14.493043
19.206829	733.569856	14.498061
19.722152	730.987188	14.503079
19.387914	726.652841	14.508096
18.960930	722.721087	14.513114
19.076537	734.963009	14.518131
19.304005	742.128935	14.523149
19.434274	740.862185	14.528167
19.625701	747.658196	14.533184
19.492897	753.169829	14.538202
18.990676	746.466454	14.543219
19.094901	748.129094	14.548237
19.509387	746.313181	14.553255
19.538850	748.530242	14.558272
19.587208	739.888750	14.563290
19.401248	744.420922	14.568307
19.765412	748.138477	14.573325
19.984332	742.480967	14.578343
19.395913	750.222036	14.583360
19.378750	747.589732	14.588378
19.462270	745.351993	14.593395
19.441823	755.485014	14.598413
19.195160	747.627886	14.603431
19.205219	759.157292	14.608448
19.698101	770.251780	14.613466
19.945258	770.102884	14.618483
20.093852	774.292650	14.623501
20.193789	765.510575	14.628519
19.864938	755.103809	14.633536
19.910549	743.619454	14.638554
19.799665	749.534759	14.643571
19.883153	739.240521	14.648589
20.570954	740.730252	14.653607
19.782014	744.488488	14.658624
19.892704	751.817762	14.663642
19.820140	746.921978	14.668659
19.805667	747.672167	14.673677
20.063435	741.260708	14.678695
19.559817	744.829359	14.683712
20.180416	752.053997	14.688730
20.180822	753.395141	14.693747
19.764488	749.105128	14.698765
20.024071	759.582704	14.703783
20.178711	758.094415	14.708800
20.108270	760.279697	14.713818
20.411787	753.422468	14.718835
20.007194	765.830608	14.723853
20.299260	755.371347	14.728871
20.312285	755.198946	14.733888
20.329444	758.086933	14.738906
20.145805	748.143539	14.743923
20.065755	754.372770	14.748941
20.424485	760.839791	14.753959
20.193127	755.283940	14.758976
20.230207	759.364837	14.763994
20.603108	763.781601	14.769011
20.540781	760.638791	14.774029
20.452432	758.885387	14.779047
20.260165	750.596925	14.784064
20.058029	759.051001	14.789082
20.576779	752.185508	14.794099
20.522986	762.967488	14.799117
20.340675	757.419779	14.804135
20.444058	757.350071	14.809152
20.354444	755.347564	14.814170
20.288018	764.250713	14.819187
20.348799	761.969177	14.824205
20.642209	753.097027	14.829223
20.522779	750.455400	14.834240
20.184023	761.351172	14.839258
20.368329	749.902022	14.844275
20.276038	759.882136	14.849293
20.277921	748.865319	14.854311
20.106171	761.095197	14.859328
20.411726	782.863052	14.864346
20.921804	779.022066	14.869363
20.532684	785.488771	14.874381
20.768740	780.825785	14.879399
20.607665	786.881456	14.884416
20.977886	783.406217	14.889434
20.896112	778.549727	14.894451
20.945723	782.789619	14.899469
21.095200	789.491195	14.904487
21.036115	784.779489	14.909504
20.874670	780.247818	14.914522
21.273035	777.124793	14.919539
20.785974	790.318939	14.924557
21.208916	785.491159	14.929575
21.044654	787.874082	14.934592
21.075274	788.203855	14.939610
21.114712	782.441737	14.944627
20.998328	793.798353	14.949645
20.835129	790.207354	14.954663
21.391594	789.562189	14.959680
21.234496	790.012704	14.964698
21.224326	783.652414	14.969715
20.919763	778.953683	14.974733
20.955127	786.253675	14.979751
20.916888	783.665671	14.984768
20.806983	792.537736	14.989786
21.208887	782.550492	14.994803
21.110655	783.465198	14.999821
21.106778	777.769784	15.004839
21.305306	779.556596	15.009856
20.866830	790.477380	15.014874
21.017942	775.527389	15.019891
21.507116	790.201039	15.024909
21.563541	788.721728	15.029927
21.241397	789.046466	15.034944
21.464128	795.004514	15.039962
21.595007	791.026912	15.044979
21.307644	796.168158	15.049997
21.460747	801.815167	15.055015
21.977718	807.490730	15.060032
21.502784	800.275016	15.065050
21.307819	781.775081	15.070067
21.018520	789.081443	15.075085
21.587852	799.037459	15.080103
21.697418	800.494152	15.085120
21.394541	812.725546	15.090138
21.886395	799.385545	15.095155
21.502496	799.467441	15.100173
21.733940	804.673077	15.105191
21.257348	804.191909	15.110208
21.409382	805.992274	15.115226
21.607543	807.444640	15.120243
21.675180	809.617897	15.125261
21.734596	808.570451	15.130279
21.725211	800.212467	15.135296
21.764285	811.207229	15.140314
21.867516	803.746866	15.145331
21.984060	810.270546	15.150349
21.952905	803.774665	15.155367
22.007153	804.514157	15.160384
21.625035	799.537171	15.165402
22.012391	797.488798	15.170419
21.776422	800.936895	15.175437
21.721569	800.800307	15.180455
21.990100	811.128202	15.185472
22.189209	826.288843	15.190490
22.387450	819.886624	15.195507
22.124538	806.689377	15.200525
22.213939	805.302757	15.205543
22.091268	795.889471	15.210560
22.244507	798.914063	15.215578
22.111734	791.537786	15.220595
21.879291	802.682111	15.225613
21.677569	818.429001	15.230631
22.208268	819.305745	15.235648
22.263369	819.833672	15.240666
22.278025	824.094796	15.245683
21.617290	832.610842	15.250701
22.397449	821.242439	15.255719
22.699213	828.797608	15.260736
22.579705	829.087641	15.265754
22.510011	816.526159	15.270771
22.459265	828.907652	15.275789
22.814255	829.183766	15.280807
22.824784	830.157278	15.285824
22.043461	824.005398	15.290842
22.685993	820.724433	15.295859
22.641930	822.091441	15.300877
22.344939	825.754165	15.305895
22.854261	819.802115	15.310912
22.345353	825.170362	15.315930
22.673687	827.249384	15.320947
22.567089	828.222198	15.325965
22.508078	823.150718	15.330983
22.446924	814.668248	15.336000
22.690770	820.506256	15.341018
22.714803	824.393545	15.346035
22.783342	827.541779	15.351053
22.889906	827.310633	15.356071
23.077136	813.651987	15.361088
22.276813	826.689811	15.366106
22.797606	821.947769	15.371123
22.841690	817.579743	15.376141
22.762586	820.205025	15.381159
22.864268	814.988611	15.386176
22.652981	825.283925	15.391194
22.765944	819.093794	15.396211
23.078529	814.627161	15.401229
22.802343	822.632063	15.406247
22.696687	823.216577	15.411264
22.774653	833.586777	15.416282
23.090596	845.488324	15.421299
23.351518	846.242975	15.426317
23.462953	842.896377	15.431335
23.123447	828.565512	15.436352
23.138927	829.468827	15.441370
23.347368	823.828702	15.446387
23.070840	819.479036	15.451405
22.551735	830.920467	15.456423
23.139560	839.380973	15.461440
22.939901	844.372883	15.466458
23.276808	839.138773	15.471475
23.107868	839.546953	15.476493
23.227307	843.488817	15.481511
22.989785	841.704984	15.486528
23.345862	846.222215	15.491546
23.384497	845.698696	15.496563
23.342343	840.466801	15.501581
23.506363	836.894272	15.506599
23.537394	836.618083	15.511616
23.476614	847.480096	15.516634
23.359778	841.997904	15.521651
23.471575	835.574425	15.526669
23.056483	839.473284	15.531687
23.403535	828.910747	15.536704
23.534843	845.877565	15.541722
23.318551	851.219195	15.546739
23.633456	863.701568	15.551757
23.607667	865.924090	15.556775
24.024926	859.863288	15.561792
23.554984	867.873131	15.566810
24.099205	866.510365	15.571827
24.328160	856.821400	15.576845
24.033358	850.543270	15.581863
23.933775	837.058646	15.586880
23.468530	836.102353	15.591898
23.818807	837.900257	15.596915
23.578585	831.683062	15.601933
23.560342	851.087292	15.606951
23.642113	855.129695	15.611968
23.357842	859.639335	15.616986
23.723163	861.699979	15.622003
23.988062	864.334823	15.627021
23.417051	870.365987	15.632039
23.651457	860.032403	15.637056
23.699552	867.308356	15.642074
24.096986	875.249427	15.647091
24.115298	883.098053	15.652109
24.178170	890.314912	15.657127
24.233964	878.557493	15.662144
24.576059	883.685965	15.667162
24.017207	866.463864	15.672179
24.274583	885.427597	15.677197
24.070804	883.909898	15.682215
24.146281	885.365594	15.687232
24.322704	887.553480	15.692250
24.375336	893.235095	15.697267
24.676072	878.700368	15.702285
24.208376	891.405591	15.707303
24.100210	882.261394	15.712320
24.584708	890.700143	15.717338
24.320910	891.236699	15.722355
24.689489	881.655366	15.727373
24.586477	877.805676	15.732391
24.640204	882.792858	15.737408
24.617633	882.638621	15.742426
24.483195	887.992763	15.747443
24.666736	885.777303	15.752461
24.595083	886.536401	15.757479
24.547737	876.940935	15.762496
24.372689	882.295087	15.767514
24.580380	890.556033	15.772531
24.648140	880.087442	15.777549
24.654214	886.123434	15.782567
24.547462	877.143117	15.787584
24.966298	876.696098	15.792602
24.774437	872.074467	15.797619
24.779826	873.067716	15.802637
24.522080	885.437297	15.807655
24.906488	882.243845	15.812672
24.649793	876.909647	15.817690
24.541652	876.692995	15.822707
24.950031	882.625324	15.827725
24.807365	882.420358	15.832743
24.862154	882.506534	15.837760
25.063688	874.226127	15.842778
25.028801	882.032544	15.847795
25.164796	883.002303	15.852813
24.851922	878.453159	15.857831
25.139516	887.427480	15.862848
24.957924	890.264384	15.867866
25.113759	904.775439	15.872883
25.367326	901.223668	15.877901
25.083221	900.693594	15.882919
25.371340	900.494139	15.887936
25.431543	900.226030	15.892954
25.267534	891.835274	15.897971
25.288916	881.575870	15.902989
25.051033	881.363639	15.908007
25.481283	894.213073	15.913024
25.556919	900.695820	15.918042
25.461540	905.516880	15.923059
25.583888	888.895581	15.928077
25.312015	885.488736	15.933095
25.342254	892.354079	15.938112
25.640916	902.917171	15.943130
25.627691	897.109568	15.948147
25.940450	894.441654	15.953165
25.580837	885.475455	15.958183
25.324142	882.063092	15.963200
25.605392	892.824544	15.968218
25.051881	900.181555	15.973235
25.431668	903.240319	15.978253
25.572850	907.087296	15.983271
25.861467	910.169723	15.988288
25.561534	910.087070	15.993306
25.604640	905.113275	15.998323
25.398569	910.525913	16.003341
25.587096	902.187559	16.008359
25.928000	901.793697	16.013376
26.222082	913.610333	16.018394
25.889405	903.993007	16.023411
25.843910	908.863104	16.028429
25.866591	902.844787	16.033447
25.754068	904.336066	16.038464
25.736200	903.751917	16.043482
25.946598	910.450365	16.048499
26.390083	911.795119	16.053517
25.851123	915.050576	16.058535
26.101465	919.448592	16.063552
26.298385	913.131750	16.068570
25.848827	917.768122	16.073587
26.445437	927.271849	16.078605
26.195293	934.480658	16.083623
25.985354	922.622575	16.088640
26.139387	923.851453	16.093658
26.120741	935.297081	16.098675
26.179033	929.661366	16.103693
26.423149	930.907776	16.108711
26.330378	932.007827	16.113728
26.775868	931.695510	16.118746
26.458261	934.256959	16.123763
26.644614	926.420693	16.128781
26.590181	930.569525	16.133799
26.228838	932.544505	16.138816
26.485212	929.793848	16.143834
26.534085	935.084751	16.148851
26.880226	931.916183	16.153869
26.342415	930.949093	16.158887
26.601989	927.140767	16.163904
26.521161	927.655148	16.168922
26.294717	923.155650	16.173939
26.538750	922.003716	16.178957
26.526420	932.359632	16.183975
26.497917	929.107387	16.188992
26.579763	918.895350	16.194010
26.559220	925.159556	16.199027
26.702656	923.859186	16.204045
26.435498	924.270037	16.209063
26.455684	937.562036	16.214080
26.987472	936.715585	16.219098
27.169872	948.540166	16.224115
27.887144	933.034845	16.229133
27.622277	921.166381	16.234151
27.699827	910.784608	16.239168
27.643650	909.871916	16.244186
27.098946	907.085044	16.249203
27.102244	889.390397	16.254221
27.193539	890.846786	16.259239
27.087345	894.211581	16.264256
27.063871	891.589705	16.269274
26.472982	894.610253	16.274291
27.131870	897.546668	16.279309
27.339335	901.563201	16.284327
27.258069	899.316386	16.289344
27.097658	902.323560	16.294362
27.216418	905.918414	16.299379
27.460353	903.254902	16.304397
27.130863	913.335146	16.309415
27.331188	907.907692	16.314432
27.475185	903.561958	16.319450
27.159912	910.645200	16.324467
27.379932	904.940132	16.329485
27.368589	898.359082	16.334503
27.237901	905.400961	16.339520
27.462280	908.291422	16.344538
27.469933	911.812061	16.349555
27.804016	928.485460	16.354573
27.738633	930.168213	16.359591
27.810358	926.307086	16.364608
27.847934	919.781526	16.369626
27.677050	918.299727	16.374643
27.544186	907.676167	16.379661
27.751136	915.930929	16.384679
27.786367	922.644032	16.389696
28.268442	917.137995	16.394714
27.878909	910.723118	16.399731
27.690514	902.582300	16.404749
28.005494	912.577982	16.409767
27.646091	921.993874	16.414784
27.995872	929.929765	16.419802
27.997457	928.272793	16.424819
27.891485	930.551988	16.429837
27.791620	923.183155	16.434855
27.946733	929.524153	16.439872
27.869731	927.513351	16.444890
27.990677	929.943404	16.449907
28.228127	923.579224	16.454925
28.063680	936.152060	16.459943
27.835383	932.151454	16.464960
28.125240	920.789900	16.469978
27.841758	930.332828	16.474995
28.360910	938.308624	16.480013
28.380851	934.992032	16.485031
27.824081	940.942109	16.490048
28.318560	940.123557	16.495066
28.425411	955.996092	16.500083
28.778594	941.314296	16.505101
28.776532	949.087230	16.510119
28.272761	945.435619	16.515136
28.218863	942.102120	16.520154
28.545500	954.434411	16.525171
28.770323	952.165179	16.530189
28.552253	951.646912	16.535207
28.467513	952.288132	16.540224
29.110352	950.572342	16.545242
28.836833	947.667503	16.550259
28.627053	931.211482	16.555277
28.737110	935.542983	16.560295
28.454947	939.452724	16.565312
28.770046	940.451404	16.570330
28.880598	952.340821	16.575347
29.097638	953.670342	16.580365
28.874216	947.182253	16.585383
28.591561	947.589205	16.590400
29.055983	941.912343	16.595418
28.513898	950.978005	16.600435
28.701423	952.129088	16.605453
28.724770	949.054955	16.610471
28.901533	954.843493	16.615488
28.987031	940.963908	16.620506
28.874516	939.870641	16.625523
28.815274	943.805635	16.630541
28.576196	947.257400	16.635559
28.396241	966.052630	16.640576
29.122190	961.628897	16.645594
29.241502	972.245200	16.650611
29.207046	974.699455	16.655629
29.377472	964.950117	16.660647
29.358436	975.464889	16.665664
29.792794	967.078762	16.670682
29.420987	970.090458	16.675699
29.445302	961.020266	16.680717
29.481265	965.202368	16.685735
29.599784	960.090585	16.690752
29.677567	960.999985	16.695770
29.445346	963.775358	16.700787
29.509754	963.219421	16.705805
29.685005	967.332501	16.710823
29.579287	966.537970	16.715840
29.807745	958.499479	16.720858
29.766151	967.534561	16.725875
29.182249	962.121896	16.730893
29.484628	969.323586	16.735911
29.538505	970.167282	16.740928
29.614092	972.689609	16.745946
29.254692	972.903387	16.750963
29.254842	982.238084	16.755981
29.582566	975.941879	16.760999
29.710503	986.193937	16.766016
29.819837	976.368900	16.771034
29.641768	982.626095	16.776051
29.828003	982.511929	16.781069
30.070306	976.064924	16.786087
29.677912	979.638394	16.791104
30.162589	990.311429	16.796122
30.295887	998.606099	16.801139
30.242075	996.594834	16.806157
30.202593	983.239594	16.811175
30.001611	991.289666	16.816192
30.544656	990.605559	16.821210
30.814415	986.745143	16.826227
30.323399	985.571952	16.831245
30.621759	963.839276	16.836263
30.227342	979.363851	16.841280
30.387651	959.072759	16.846298
30.240075	976.373450	16.851315
30.438840	976.421431	16.856333
30.711093	969.925586	16.861351
30.686203	969.064823	16.866368
30.410237	968.056962	16.871386
30.347157	976.461090	16.876403
30.294563	971.587381	16.881421
30.518686	967.942353	16.886439
30.441266	982.369870	16.891456
30.532340	987.477497	16.896474
30.748965	987.715198	16.901491
30.830122	990.855185	16.906509
30.829373	995.576331	16.911527
30.697745	993.378370	16.916544
30.551602	999.905150	16.921562
30.882344	992.705926	16.926579
31.294595	998.404166	16.931597
31.048470	997.347478	16.936615
30.970025	995.655623	16.941632
31.186735	995.937491	16.946650
31.009645	1000.020231	16.951667
31.106482	997.663625	16.956685
31.202597	985.637931	16.961703
30.637792	984.769712	16.966720
30.582703	987.451239	16.971738
30.933725	993.771225	16.976755
30.992792	995.349403	16.981773
31.069574	994.201415	16.986791
31.279264	997.624343	16.991808
31.447514	989.024022	16.996826
31.567109	996.298363	17.001843
31.472484	988.704629	17.006861
31.444223	989.027794	17.011879
31.804344	998.527356	17.016896
31.275046	985.421941	17.021914
31.507874	981.043423	17.026931
31.186937	993.669066	17.031949
31.258041	982.717065	17.036967
31.297099	989.259187	17.041984
31.298456	985.279617	17.047002
31.392739	983.756526	17.052019
31.634905	1007.724613	17.057037
32.004022	1014.837038	17.062055
31.675070	999.885865	17.067072
31.831293	999.738502	17.072090
31.774346	992.669065	17.077107
32.049536	989.278009	17.082125
31.941759	987.896829	17.087143
31.518094	985.179460	17.092160
31.875174	999.905409	17.097178
32.262518	1004.121172	17.102195
31.743910	1001.696288	17.107213
31.976306	1003.739777	17.112231
31.923105	1010.551887	17.117248
31.886874	1011.425393	17.122266
32.013765	1011.803295	17.127283
32.101382	1002.237241	17.132301
32.398563	1004.027650	17.137319
32.213632	1004.981111	17.142336
31.883546	1005.124055	17.147354
31.803132	999.674012	17.152371
31.733868	1011.894417	17.157389
32.280444	1010.143118	17.162407
32.293149	1008.474939	17.167424
32.131863	1012.154441	17.172442
32.368410	1008.889316	17.177459
31.805077	1010.842106	17.182477
32.387484	1020.789901	17.187495
32.653109	1036.530491	17.192512
32.455956	1031.575133	17.197530
32.531924	1029.063984	17.202547
32.377720	1027.557488	17.207565
33.061277	1028.861717	17.212583
32.934733	1025.255496	17.217600
32.420565	1030.618311	17.222618
32.493335	1029.587708	17.227635
32.539935	1037.933764	17.232653
32.877399	1023.923367	17.237671
32.732301	1038.617082	17.242688
32.434261	1030.026226	17.247706
32.848850	1029.343184	17.252723
32.490292	1028.502811	17.257741
32.928674	1028.327296	17.262759
32.988528	1035.172304	17.267776
33.177090	1023.144814	17.272794
32.989923	1035.834864	17.277811
32.519692	1026.639668	17.282829
32.863474	1032.269686	17.287847
32.822686	1040.973326	17.292864
32.550727	1043.915841	17.297882
33.196006	1042.051342	17.302899
33.360605	1052.512322	17.307917
33.067894	1051.857353	17.312935
33.209261	1057.484180	17.317952
33.223860	1047.752747	17.322970
33.647464	1042.937418	17.327987
33.734042	1051.482380	17.333005
33.694188	1053.830190	17.338023
33.350913	1049.992624	17.343040
33.495802	1050.285676	17.348058
33.786100	1037.204092	17.353075
33.459962	1049.751691	17.358093
33.794068	1040.964579	17.363111
33.666173	1046.686974	17.368128
33.563417	1049.369619	17.373146
33.573153	1045.944144	17.378163
33.564324	1052.288621	17.383181
33.583102	1049.376125	17.388199
33.485057	1053.538088	17.393216
33.621813	1041.026353	17.398234
34.059130	1037.430167	17.403251
33.491603	1049.043376	17.408269
33.958916	1050.220332	17.413287
33.709527	1055.043320	17.418304
33.942041	1061.984531	17.423322
34.281023	1066.747475	17.428339
34.073022	1074.934375	17.433357
34.014735	1060.711014	17.438375
34.547880	1063.818511	17.443392
34.239870	1069.389078	17.448410
34.204724	1064.244387	17.453427
34.072725	1064.066161	17.458445
34.270843	1059.645691	17.463463
34.293481	1071.457359	17.468480
33.971381	1069.087076	17.473498
34.116723	1063.557683	17.478515
34.326344	1065.415380	17.483533
34.294736	1065.805338	17.488551
34.390000	1060.611942	17.493568
34.330840	1064.165103	17.498586
34.304792	1063.055211	17.503603
34.513373	1067.418741	17.508621
34.408137	1068.220944	17.513639
34.423415	1064.400133	17.518656
34.551134	1071.887831	17.523674
34.746235	1072.005810	17.528691
34.620274	1068.942280	17.533709
34.671142	1095.685779	17.538727
34.837828	1086.372453	17.543744
34.621698	1102.052411	17.548762
34.842020	1086.141499	17.553779
34.688036	1091.031693	17.558797
34.593395	1089.238211	17.563815
35.185483	1087.962649	17.568832
35.032746	1085.439764	17.573850
35.325483	1081.380093	17.578867
35.539319	1077.588324	17.583885
35.638511	1070.740696	17.588903
35.546328	1059.968702	17.593920
35.247525	1056.313556	17.598938
35.489449	1036.104342	17.603955
35.513296	1049.130771	17.608973
35.131838	1042.780859	17.613991
35.089431	1046.599648	17.619008
34.882131	1042.482141	17.624026
35.087765	1047.398382	17.629043
35.285415	1057.169420	17.634061
35.304926	1061.552919	17.639079
35.694004	1068.087910	17.644096
35.607350	1073.617702	17.649114
35.687995	1070.518849	17.654131
35.625321	1077.679592	17.659149
35.699588	1076.434161	17.664167
35.625744	1078.146648	17.669184
35.341546	1072.643105	17.674202
35.486514	1073.422132	17.679219
35.442640	1070.983284	17.684237
35.771990	1079.196974	17.689255
35.893162	1063.443529	17.694272
35.604842	1069.389721	17.699290
35.663845	1076.013975	17.704307
35.758951	1076.056006	17.709325
35.672167	1072.869612	17.714343
36.104253	1080.171072	17.719360
35.805203	1094.109331	17.724378
35.872677	1097.686963	17.729395
36.092864	1096.371475	17.734413
35.957042	1100.201663	17.739431
36.153492	1090.571280	17.744448
36.024201	1099.724223	17.749466
36.006127	1091.212822	17.754483
36.046983	1089.887387	17.759501
36.215035	1096.226430	17.764519
36.367426	1091.992950	17.769536
36.027897	1100.534851	17.774554
36.075384	1093.212433	17.779571
36.506438	1111.344648	17.784589
36.460001	1119.588463	17.789607
36.560481	1111.661346	17.794624
36.447859	1114.834682	17.799642
36.783666	1110.566329	17.804659
36.939510	1105.413981	17.809677
36.724861	1113.425211	17.814695
36.907582	1106.671860	17.819712
36.793332	1112.887606	17.824730
36.948754	1106.012275	17.829747
36.981628	1110.819734	17.834765
36.779618	1114.499286	17.839783
37.061711	1107.149802	17.844800
37.354319	1107.842728	17.849818
37.105248	1104.113558	17.854835
36.873767	1096.197108	17.859853
36.866092	1089.119961	17.864871
37.107770	1085.222871	17.869888
37.105758	1097.170936	17.874906
37.620512	1099.243057	17.879923
37.091661	1101.029543	17.884941
36.967678	1085.030229	17.889959
37.323775	1088.490340	17.894976
36.817504	1106.250941	17.899994
37.416905	1107.249547	17.905011
37.346331	1105.199855	17.910029
37.311269	1102.879550	17.915047
37.442962	1102.423585	17.920064
37.370494	1116.130925	17.925082
37.102811	1106.661158	17.930099
37.161892	1111.423511	17.935117
37.400477	1111.575745	17.940135
37.313858	1106.988160	17.945152
36.975684	1107.044002	17.950170
37.480506	1115.299816	17.955187
37.768617	1123.276954	17.960205
38.170140	1122.671682	17.965223
37.976322	1116.377735	17.970240
37.665824	1132.473194	17.975258
38.061301	1118.308525	17.980275
38.305030	1110.740954	17.985293
38.204665	1124.881828	17.990311
38.457105	1113.999342	17.995328
38.005084	1111.106490	18.000346
38.174040	1097.043377	18.005363
38.133886	1096.784579	18.010381
37.876943	1097.894422	18.015399
37.928246	1108.164794	18.020416
38.189305	1123.650556	18.025434
38.087693	1127.459645	18.030451
38.163924	1124.639177	18.035469
38.270153	1126.377279	18.040487
38.034987	1123.264471	18.045504
38.004913	1125.714908	18.050522
38.075697	1121.393143	18.055539
38.547003	1124.223104	18.060557
38.205646	1130.212287	18.065575
38.475570	1141.647833	18.070592
38.736248	1151.270256	18.075610
38.649216	1144.729301	18.080627
39.344334	1143.264128	18.085645
38.638312	1133.436564	18.090663
38.577839	1118.452957	18.095680
38.767457	1130.399610	18.100698
38.968767	1139.270729	18.105715
39.079452	1128.463953	18.110733
38.554581	1132.329475	18.115751
38.652869	1139.689242	18.120768
38.600226	1144.740395	18.125786
38.344321	1153.392377	18.130803
38.573378	1148.023492	18.135821
38.672188	1146.430256	18.140839
38.873125	1155.405582	18.145856
38.895767	1169.988084	18.150874
39.212646	1170.023988	18.155891
39.154910	1168.161636	18.160909
39.155808	1176.855696	18.165927
39.660940	1164.624189	18.170944
39.567546	1171.019744	18.175962
39.353076	1160.071071	18.180979
39.647743	1157.506919	18.185997
39.629645	1170.846078	18.191015
39.588892	1165.370875	18.196032
39.554822	1173.461313	18.201050
39.199956	1173.762749	18.206067
39.130271	1165.016354	18.211085
39.101057	1171.304087	18.216103
39.380037	1171.042937	18.221120
39.547002	1184.479524	18.226138
39.644340	1190.747561	18.231155
39.865699	1191.372689	18.236173
39.881083	1189.262267	18.241191
40.054179	1184.665783	18.246208
40.168466	1198.079024	18.251226
39.999769	1189.206023	18.256243
40.279990	1195.016401	18.261261
40.299529	1204.689020	18.266279
40.362655	1182.765485	18.271296
40.124132	1173.108107	18.276314
39.779809	1174.979478	18.281331
40.412620	1181.852101	18.286349
40.223883	1192.112558	18.291367
40.502682	1198.200867	18.296384
40.329417	1190.982205	18.301402
40.332400	1192.941515	18.306419
40.622391	1188.617162	18.311437
40.199726	1192.839165	18.316455
40.266328	1186.406818	18.321472
40.206939	1189.559256	18.326490
40.279929	1192.583787	18.331507
40.437811	1183.360142	18.336525
40.556269	1189.498659	18.341543
40.625597	1189.585729	18.346560
40.465418	1181.632892	18.351578
40.468013	1195.268647	18.356595
40.626156	1198.134755	18.361613
40.785226	1206.842073	18.366631
40.417246	1206.217750	18.371648
40.670104	1210.965740	18.376666
40.675558	1206.272275	18.381683
41.005082	1195.986804	18.386701
40.740542	1208.436561	18.391719
40.837766	1205.316168	18.396736
41.308532	1218.645521	18.401754
41.081910	1233.920132	18.406771
41.347037	1219.261285	18.411789
41.774296	1227.904766	18.416807
41.778209	1219.882184	18.421824
41.436197	1205.794399	18.426842
41.225404	1196.678641	18.431859
41.613218	1193.153248	18.436877
41.575184	1205.110149	18.441895
41.199335	1195.852833	18.446912
41.473367	1202.074429	18.451930
41.509938	1210.816600	18.456947
41.955872	1211.182703	18.461965
41.670053	1221.085909	18.466983
41.738891	1220.444069	18.472000
41.933938	1223.036193	18.477018
41.943071	1231.719531	18.482035
41.875862	1215.026454	18.487053
41.769603	1215.942432	18.492071
42.123242	1216.427045	18.497088
42.427660	1218.951648	18.502106
41.481018	1211.957530	18.507123
42.138932	1215.234975	18.512141
42.424003	1221.398055	18.517159
42.232071	1224.362853	18.522176
42.277727	1204.461715	18.527194
42.043254	1217.266556	18.532211
42.090880	1205.396585	18.537229
42.414096	1223.122829	18.542247
42.164019	1215.834066	18.547264
42.015760	1218.665832	18.552282
42.151574	1219.594613	18.557299
42.441535	1214.907342	18.562317
42.220382	1222.020235	18.567335
42.336527	1218.038520	18.572352
42.542924	1225.293129	18.577370
42.489366	1230.249775	18.582387
42.603520	1228.540535	18.587405
42.555476	1220.330383	18.592423
42.500065	1223.649464	18.597440
42.754777	1224.051651	18.602458
42.691623	1244.138640	18.607475
42.886917	1243.887363	18.612493
43.264535	1244.942598	18.617511
42.994750	1252.485951	18.622528
43.139536	1248.723831	18.627546
42.805045	1243.316427	18.632563
42.850885	1243.568099	18.637581
43.171800	1243.025866	18.642599
42.868762	1239.267200	18.647616
42.986568	1237.522677	18.652634
42.952313	1247.052217	18.657651
42.984414	1234.168479	18.662669
42.960512	1233.465338	18.667687
43.208234	1241.436194	18.672704
43.677502	1261.194156	18.677722
43.412507	1259.796408	18.682739
43.542953	1258.636892	18.687757
43.806679	1262.603722	18.692775
43.219757	1265.497481	18.697792
43.996834	1257.259830	18.702810
43.508213	1258.708710	18.707827
43.481312	1254.812374	18.712845
43.672751	1250.945161	18.717863
43.476238	1260.503126	18.722880
43.443812	1254.190314	18.727898
43.543447	1250.097554	18.732915
43.898510	1250.948019	18.737933
44.033047	1259.775946	18.742951
43.556899	1259.152684	18.747968
44.017701	1269.766490	18.752986
44.124138	1279.857965	18.758003
44.329481	1278.109276	18.763021
44.317903	1270.499335	18.768039
44.284120	1276.734169	18.773056
44.514249	1274.577679	18.778074
44.452755	1278.090221	18.783091
44.578120	1274.053409	18.788109
44.573719	1272.611931	18.793127
44.560553	1273.308290	18.798144
44.917585	1270.652362	18.803162
44.345653	1267.926475	18.808179
44.645720	1265.907419	18.813197
44.794466	1276.244768	18.818215
44.524260	1276.716060	18.823232
44.638074	1273.337453	18.828250
44.596689	1272.971547	18.833267
44.897958	1268.976777	18.838285
44.506800	1268.094130	18.843303
44.602115	1276.489517	18.848320
45.138433	1270.103928	18.853338
44.477284	1266.893316	18.858355
44.510181	1270.801413	18.863373
44.494604	1272.258694	18.868391
44.739179	1291.657199	18.873408
44.614592	1289.467573	18.878426
45.064185	1297.706825	18.883443
45.206302	1291.376291	18.888461
45.028250	1293.082932	18.893479
45.123378	1300.998679	18.898496
45.347812	1308.951101	18.903514
45.347741	1320.438266	18.908531
45.398730	1319.584606	18.913549
45.642311	1315.324253	18.918567
45.256866	1323.961772	18.923584
45.665670	1319.940780	18.928602
45.462782	1317.876950	18.933619
45.537228	1316.069742	18.938637
45.771099	1319.899223	18.943655
45.637812	1319.714882	18.948672
46.217597	1311.905555	18.953690
45.677878	1318.279134	18.958707
45.836470	1314.057260	18.963725
45.685738	1316.485484	18.968743
46.085606	1315.590129	18.973760
46.149687	1310.142740	18.978778
46.244094	1314.158035	18.983795
46.000520	1318.863424	18.988813
45.915913	1316.443508	18.993831
45.528928	1316.828841	18.998848
46.219730	1337.726355	19.003866
46.490926	1340.227746	19.008883
46.473044	1333.896862	19.013901
46.534343	1334.228180	19.018919
46.765180	1329.805705	19.023936
46.951707	1323.796449	19.028954
47.009334	1330.616672	19.033971
47.169912	1323.279707	19.038989
46.811834	1301.973870	19.044007
46.453458	1302.212738	19.049024
46.490263	1296.166842	19.054042
46.826174	1310.321989	19.059059
47.218558	1326.109373	19.064077
47.020229	1319.841303	19.069095
46.751516	1318.816513	19.074112
47.185334	1322.062598	19.079130
47.136477	1315.477767	19.084147
47.420825	1318.826018	19.089165
47.113617	1303.300003	19.094183
46.865022	1315.693704	19.099200
47.288634	1317.335073	19.104218
47.406788	1327.724552	19.109235
47.445661	1325.667261	19.114253
47.634890	1321.951855	19.119271
47.262928	1320.072139	19.124288
47.543596	1326.507340	19.129306
47.615505	1325.069755	19.134323
47.180563	1314.054327	19.139341
47.316196	1316.207593	19.144359
47.378913	1321.398625	19.149376
47.419507	1312.477198	19.154394
47.388708	1317.657543	19.159411
47.554558	1327.566225	19.164429
47.566465	1323.862647	19.169447
47.520938	1339.475227	19.174464
47.524394	1339.632513	19.179482
47.635833	1349.129957	19.184499
47.680953	1352.534395	19.189517
47.986678	1343.271871	19.194535
47.784858	1351.893437	19.199552
48.289072	1347.740819	19.204570
48.560687	1353.259100	19.209587
48.452634	1348.135145	19.214605
48.656180	1329.468452	19.219623
48.430876	1337.601362	19.224640
48.819926	1326.287222	19.229658
48.649742	1320.800564	19.234675
48.796107	1331.419182	19.239693
48.890619	1318.980102	19.244711
48.497132	1331.929703	19.249728
48.580396	1328.091939	19.254746
48.310224	1326.133258	19.259763
48.588990	1328.251616	19.264781
48.707232	1315.808843	19.269799
48.397570	1331.478318	19.274816
48.918751	1330.377883	19.279834
48.710712	1329.630824	19.284851
48.700113	1338.661269	19.289869
49.104030	1347.207457	19.294887
49.045131	1347.238753	19.299904
48.999225	1341.802167	19.304922
49.260870	1358.070682	19.309939
49.152878	1352.823641	19.314957
49.235341	1349.519328	19.319975
49.209887	1360.470828	19.324992
49.317531	1355.114472	19.330010
49.135497	1351.952326	19.335027
49.174918	1356.708339	19.340045
49.630522	1360.001532	19.345063
49.434829	1358.930657	19.350080
49.551630	1358.776806	19.355098
49.411543	1351.451927	19.360115
49.300638	1358.872758	19.365133
49.848209	1373.828135	19.370151
49.617146	1382.359594	19.375168
49.703018	1382.071703	19.380186
49.885422	1378.543541	19.385203
49.843856	1375.116523	19.390221
49.893247	1371.261932	19.395239
49.968330	1369.678682	19.400256
49.934326	1365.022877	19.405274
49.906773	1369.909242	19.410291
49.431343	1382.142646	19.415309
50.226858	1387.099684	19.420327
50.031075	1398.178713	19.425344
50.157713	1394.170078	19.430362
50.013063	1391.910979	19.435379
50.210152	1400.268488	19.440397
50.314142	1389.610920	19.445415
50.386981	1398.287575	19.450432
50.435912	1395.995180	19.455450
50.991535	1417.084249	19.460467
50.668163	1424.683354	19.465485
51.207743	1409.669193	19.470503
50.805192	1402.258925	19.475520
51.200403	1392.742600	19.480538
51.144301	1381.406215	19.485555
51.088480	1380.408236	19.490573
50.951766	1379.804705	19.495591
50.880858	1389.529377	19.500608
50.739292	1377.464683	19.505626
50.945545	1389.942253	19.510643
50.884453	1409.107610	19.515661
51.030422	1409.618251	19.520679
51.058274	1415.922432	19.525696
50.887011	1414.513233	19.530714
51.190956	1420.364174	19.535731
50.966949	1435.089437	19.540749
51.107426	1433.543337	19.545767
51.313045	1444.724001	19.550784
51.391261	1444.573002	19.555802
51.406746	1437.987575	19.560819
51.438108	1442.830073	19.565837
51.593683	1441.871761	19.570855
51.871952	1442.642674	19.575872
51.437744	1434.628247	19.580890
51.908524	1451.189336	19.585907
51.908292	1466.204834	19.590925
52.083720	1465.303391	19.595943
51.724641	1469.278872	19.600960
52.017679	1467.017890	19.605978
52.518966	1461.473982	19.610995
52.369468	1471.898905	19.616013
52.632475	1458.303706	19.621031
52.477094	1461.041944	19.626048
52.110720	1456.734512	19.631066
52.339104	1458.728185	19.636083
52.512034	1469.876085	19.641101
52.404726	1460.478989	19.646119
52.596607	1468.143059	19.651136
52.449621	1465.635004	19.656154
52.455090	1458.347379	19.661171
52.581463	1468.338026	19.666189
52.348340	1464.095052	19.671207
52.365301	1462.041158	19.676224
52.468935	1465.136704	19.681242
52.714200	1473.344735	19.686259
52.549579	1484.087602	19.691277
52.816203	1478.009019	19.696295
52.878709	1480.419844	19.701312
53.036402	1473.089579	19.706330
53.297179	1479.348050	19.711347
53.317601	1487.045135	19.716365
53.251253	1481.662182	19.721383
53.535679	1493.209307	19.726400
53.655297	1502.175378	19.731418
53.669099	1485.917564	19.736435
53.673484	1478.017869	19.741453
53.425323	1477.769360	19.746471
53.775800	1483.767712	19.751488
53.898977	1487.327282	19.756506
54.060655	1480.365626	19.761523
53.664681	1489.077447	19.766541
53.573405	1478.825771	19.771559
53.778068	1494.061858	19.776576
53.767971	1496.742768	19.781594
54.141104	1491.632218	19.786611
53.988512	1503.326286	19.791629
53.994414	1491.752957	19.796647
54.026060	1502.440031	19.801664
54.051368	1505.711883	19.806682
54.101071	1496.104128	19.811699
53.989823	1497.364882	19.816717
54.057398	1494.125977	19.821735
54.229869	1498.501548	19.826752
54.099944	1520.227655	19.831770
54.533250	1520.469498	19.836787
54.369913	1520.946249	19.841805
54.323988	1523.456013	19.846823
54.417522	1529.652178	19.851840
54.623371	1526.486414	19.856858
55.108206	1531.198371	19.861875
54.557142	1527.506663	19.866893
54.678121	1530.545871	19.871911
55.089773	1537.970624	19.876928
54.935044	1551.586964	19.881946
54.964688	1547.467163	19.886963
55.225027	1548.193534	19.891981
55.185920	1550.105787	19.896999
55.058373	1541.851059	19.902016
55.052491	1550.423279	19.907034
55.272330	1537.450131	19.912051
55.190409	1548.461032	19.917069
55.347476	1542.601458	19.922087
55.259024	1550.214534	19.927104
55.080495	1557.131573	19.932122
55.408933	1557.831563	19.937139
55.441453	1565.062888	19.942157
55.704703	1566.167509	19.947175
55.728627	1554.676541	19.952192
55.654488	1567.437735	19.957210
55.720110	1556.135936	19.962227
55.862243	1561.333609	19.967245
55.810152	1562.708235	19.972263
55.970177	1560.553159	19.977280
55.971943	1554.897644	19.982298
55.937091	1556.638819	19.987315
55.976699	1561.237066	19.992333
56.210941	1581.240262	19.997351
56.542619	1578.884886	20.002368
56.645219	1580.633066	20.007386
56.557215	1574.521300	20.012403
56.676901	1572.025359	20.017421
56.846100	1574.397495	20.022439
56.813777	1568.087711	20.027456
56.846026	1570.515883	20.032474
57.048021	1566.725854	20.037491
56.885921	1552.325757	20.042509
56.981224	1550.710941	20.047527
57.336598	1540.941961	20.052544
56.812109	1547.363743	20.057562
56.947971	1542.870795	20.062579
57.090053	1546.676746	20.067597
56.872046	1540.837700	20.072615
57.020815	1553.712503	20.077632
56.871157	1572.147045	20.082650
57.260588	1566.519533	20.087667
57.379451	1578.070399	20.092685
57.317056	1575.893144	20.097703
57.391437	1574.865415	20.102720
57.492697	1574.590905	20.107738
57.673072	1558.461726	20.112755
57.622507	1563.408532	20.117773
57.423769	1565.632822	20.122791
57.262656	1562.726160	20.127808
57.127298	1585.052802	20.132826
57.633753	1589.079746	20.137843
57.631891	1589.828007	20.142861
57.277768	1595.415383	20.147879
57.835611	1597.354622	20.152896
58.158128	1616.533060	20.157914
57.878385	1618.940385	20.162931
57.998025	1616.750563	20.167949
57.959477	1614.339214	20.172967
58.253749	1617.752250	20.177984
58.273457	1623.672758	20.183002
58.212626	1616.231288	20.188019
58.247003	1628.300277	20.193037
58.528112	1637.518989	20.198055
58.904610	1641.515684	20.203072
58.826230	1648.221502	20.208090
58.964169	1642.358563	20.213107
58.627351	1631.501233	20.218125
58.706523	1646.330948	20.223143
58.947941	1637.665274	20.228160
58.764422	1641.086430	20.233178
59.004828	1637.864772	20.238195
59.021444	1638.853160	20.243213
58.793503	1641.119876	20.248231
58.979481	1639.651883	20.253248
59.147598	1637.994163	20.258266
59.011690	1639.186182	20.263283
59.004079	1640.314043	20.268301
58.978434	1649.293338	20.273319
59.327759	1658.255282	20.278336
59.209904	1665.241813	20.283354
59.355150	1659.942629	20.288371
59.331720	1664.705354	20.293389
59.435305	1673.465721	20.298407
59.509680	1659.410580	20.303424
59.571662	1680.188646	20.308442
60.018546	1678.310792	20.313459
60.027820	1689.708376	20.318477
59.989899	1683.904361	20.323495
60.304954	1680.816244	20.328512
60.308919	1688.935708	20.333530
60.219983	1683.830772	20.338547
60.372578	1675.592327	20.343565
60.075414	1687.823431	20.348583
60.515965	1680.442730	20.353600
60.346921	1676.076117	20.358618
60.157096	1677.570028	20.363635
60.420651	1675.086389	20.368653
60.340716	1676.348591	20.373671
60.397103	1673.900362	20.378688
60.305085	1683.082516	20.383706
60.921105	1696.310716	20.388723
60.911484	1694.832146	20.393741
61.007709	1696.508745	20.398759
61.102823	1700.407249	20.403776
61.499137	1708.607651	20.408794
61.424396	1697.772594	20.413811
61.470140	1691.169739	20.418829
60.808820	1691.181217	20.423847
60.995805	1691.338336	20.428864
60.713890	1695.087253	20.433882
61.003460	1693.590503	20.438899
61.645334	1694.879184	20.443917
61.305139	1699.104245	20.448935
61.286934	1693.843123	20.453952
61.202417	1709.613578	20.458970
61.909038	1726.993447	20.463987
61.886405	1723.961054	20.469005
61.696508	1729.017963	20.474023
61.841894	1713.821920	20.479040
62.156888	1730.104560	20.484058
62.005462	1718.931128	20.489075
62.288539	1717.810936	20.494093
62.201062	1726.888261	20.499111
62.453937	1712.631713	20.504128
62.039957	1727.819149	20.509146
62.088585	1722.718031	20.514163
62.217721	1714.369609	20.519181
61.947106	1712.830685	20.524199
62.035127	1724.503215	20.529216
62.146407	1742.673238	20.534234
62.310405	1738.355746	20.539251
62.747779	1735.415836	20.544269
62.602195	1737.783353	20.549287
62.877818	1738.106557	20.554304
62.843968	1732.494402	20.559322
62.760491	1736.991933	20.564339
62.881439	1732.195140	20.569357
62.963375	1752.402126	20.574375
63.244473	1750.540609	20.579392
63.248530	1763.819957	20.584410
63.571930	1764.577545	20.589427
63.597196	1757.245691	20.594445
63.285616	1754.472879	20.599463
63.594350	1747.576588	20.604480
63.384851	1757.414558	20.609498
63.293313	1764.778891	20.614515
63.294073	1767.338228	20.619533
63.497741	1771.330302	20.624551
63.539709	1756.462757	20.629568
63.370892	1760.828411	20.634586
62.967313	1763.759976	20.639603
63.423355	1770.306892	20.644621
63.858667	1787.315641	20.649639
64.037745	1786.404146	20.654656
63.795521	1789.219073	20.659674
63.966757	1790.309631	20.664691
64.029182	1781.132099	20.669709
63.970672	1798.116754	20.674727
64.072330	1811.592386	20.679744
64.418724	1808.691876	20.684762
64.191192	1813.975581	20.689779
64.563378	1810.373604	20.694797
64.178434	1814.510982	20.699815
64.126366	1813.269390	20.704832
64.588147	1817.748323	20.709850
64.705557	1830.505129	20.714867
64.876432	1827.186963	20.719885
64.936062	1834.287941	20.724903
64.893824	1837.330522	20.729920
65.577497	1833.932515	20.734938
65.325724	1837.670457	20.739955
65.340361	1820.383387	20.744973
64.994282	1832.088859	20.749991
65.241175	1830.873305	20.755008
65.181097	1823.630452	20.760026
65.110195	1829.271638	20.765043
65.567936	1824.091015	20.770061
65.590019	1831.462933	20.775079
65.964664	1841.118480	20.780096
65.765991	1838.492183	20.785114
66.098923	1857.820742	20.790131
66.234413	1843.396169	20.795149
65.700943	1839.083099	20.800167
65.909560	1844.942710	20.805184
65.780402	1849.513656	20.810202
65.805807	1851.952399	20.815219
66.100236	1847.807083	20.820237
65.545396	1847.969244	20.825255
66.024019	1849.769363	20.830272
66.345968	1859.638258	20.835290
66.098915	1871.464041	20.840307
66.315028	1861.262120	20.845325
66.659661	1880.279603	20.850343
66.397598	1881.077856	20.855360
66.395234	1881.545332	20.860378
66.591775	1884.408729	20.865395
66.897577	1866.713353	20.870413
66.848138	1885.009532	20.875431
67.090132	1890.605177	20.880448
67.435070	1895.758749	20.885466
67.408135	1897.908993	20.890483
67.404643	1888.233569	20.895501
67.342565	1880.713284	20.900519
67.439304	1891.415704	20.905536
67.550960	1889.602645	20.910554
67.445678	1891.528393	20.915571
67.733262	1876.493115	20.920589
67.580298	1892.116592	20.925607
67.488785	1894.295825	20.930624
67.697902	1891.249413	20.935642
67.353676	1891.542890	20.940659
67.708889	1888.760919	20.945677
67.778003	1897.634064	20.950695
67.643415	1900.877232	20.955712
67.614880	1886.557059	20.960730
67.367738	1897.704355	20.965747
67.813597	1900.478443	20.970765
67.829525	1911.610036	20.975783
67.878965	1915.149613	20.980800
68.013061	1918.265743	20.985818
68.158556	1926.379059	20.990835
68.403649	1931.551343	20.995853
68.548714	1934.324929	21.000871
68.564223	1930.686939	21.005888
68.934900	1932.683760	21.010906
68.886522	1928.762218	21.015923
69.336189	1930.128181	21.020941
69.231504	1937.059117	21.025959
69.097305	1931.610850	21.030976
69.145176	1927.172533	21.035994
68.997196	1931.115248	21.041011
69.075065	1928.464817	21.046029
69.190900	1929.838574	21.051047
69.434527	1923.836007	21.056064
69.288559	1927.601677	21.061082
69.512943	1936.782037	21.066099
69.523985	1935.237112	21.071117
69.557594	1929.178876	21.076135
69.029849	1932.852503	21.081152
69.475294	1932.186718	21.086170
69.603932	1949.003519	21.091187
69.787649	1945.023745	21.096205
69.805457	1952.822427	21.101223
69.985166	1951.942385	21.106240
70.159743	1948.285938	21.111258
69.987430	1952.791043	21.116275
70.025612	1957.683113	21.121293
70.223541	1967.183200	21.126311
70.215989	1973.322670	21.131328
70.515513	1964.774028	21.136346
70.323092	1982.344617	21.141363
70.356019	1971.663050	21.146381
70.526697	1971.743813	21.151399
70.418867	1980.900177	21.156416
70.602198	1976.838403	21.161434
70.766897	1986.312114	21.166451
71.058836	1980.320942	21.171469
70.997041	1992.114806	21.176487
71.091842	1991.519391	21.181504
71.065146	1980.575693	21.186522
71.366544	1995.219614	21.191539
71.071138	1982.307429	21.196557
70.905494	1986.085642	21.201575
71.252311	1994.123462	21.206592
71.273528	1986.126245	21.211610
71.679918	2020.396301	21.216627
71.786626	2012.874930	21.221645
72.159667	2008.660531	21.226663
71.968638	2020.023237	21.231680
72.096128	2021.821236	21.236698
72.114790	2015.298221	21.241715
72.250145	2012.269584	21.246733
72.157654	2003.359064	21.251751
72.125595	2023.666159	21.256768
72.486984	2005.772636	21.261786
72.374163	2018.922041	21.266803
72.292095	2016.744640	21.271821
72.531600	2009.373014	21.276839
71.931414	2008.472378	21.281856
72.181347	2009.746364	21.286874
72.151369	2008.573906	21.291891
72.113322	2009.643411	21.296909
72.322956	2008.780799	21.301927
72.964692	2030.516776	21.306944
73.081011	2026.437020	21.311962
72.512157	2039.834174	21.316979
72.601930	2034.543517	21.321997
72.877213	2035.788311	21.327015
72.823153	2042.588324	21.332032
73.138155	2040.932946	21.337050
73.647959	2049.036937	21.342067
73.716214	2053.217423	21.347085
73.664627	2041.387590	21.352103
73.841706	2054.753829	21.357120
74.011422	2051.205419	21.362138
74.201959	2048.774124	21.367155
73.998727	2036.219948	21.372173
74.059857	2021.087257	21.377191
73.807689	2021.530511	21.382208
73.860490	2025.192668	21.387226
73.638248	2042.749023	21.392243
74.005580	2046.538947	21.397261
74.048207	2039.762873	21.402279
74.262651	2050.661666	21.407296
74.248021	2050.648198	21.412314
74.184935	2048.773963	21.417331
74.066677	2046.071997	21.422349
74.434833	2054.415803	21.427367
74.518562	2064.208288	21.432384
75.015671	2068.634445	21.437402
74.870570	2074.293572	21.442419
74.617013	2059.127789	21.447437
74.792074	2063.916523	21.452455
74.949958	2075.269123	21.457472
74.915623	2066.560965	21.462490
75.060623	2082.302326	21.467507
75.086789	2081.723906	21.472525
75.359413	2082.094923	21.477543
75.031396	2088.637792	21.482560
75.437153	2088.700891	21.487578
75.405586	2087.071064	21.492595
75.320063	2090.947283	21.497613
75.838250	2096.408470	21.502631
75.581417	2107.459570	21.507648
75.877229	2110.840902	21.512666
76.069842	2103.833160	21.517683
75.922696	2108.236552	21.522701
75.986918	2108.725226	21.527719
75.869048	2120.638363	21.532736
76.322415	2108.224917	21.537754
76.277403	2113.174166	21.542771
76.240757	2117.213202	21.547789
76.349296	2129.551862	21.552807
76.483693	2129.515192	21.557824
76.592853	2129.495075	21.562842
76.861309	2128.585428	21.567859
76.501708	2133.511075	21.572877
76.697296	2136.803870	21.577895
76.774589	2134.671074	21.582912
76.883219	2122.456465	21.587930
76.561567	2139.782228	21.592947
77.283472	2138.041398	21.597965
77.749724	2132.146118	21.602983
77.825271	2132.008153	21.608000
78.186125	2126.321797	21.613018
78.081483	2116.693557	21.618035
78.395689	2110.875607	21.623053
77.904061	2104.693951	21.628071
77.982113	2107.029854	21.633088
78.034775	2102.205723	21.638106
77.709446	2110.206226	21.643123
77.932089	2113.267577	21.648141
78.272370	2106.823848	21.653159
78.088634	2105.725818	21.658176
78.093869	2101.900036	21.663194
78.329922	2101.872787	21.668211
78.190522	2101.042421	21.673229
78.535429	2097.962208	21.678247
78.413378	2104.977967	21.683264
78.566653	2097.332540	21.688282
78.038103	2101.284049	21.693299
78.046693	2110.630647	21.698317
78.599988	2120.933904	21.703335
78.322358	2125.894125	21.708352
78.487514	2131.473406	21.713370
78.867339	2136.807818	21.718387
78.910124	2143.614883	21.723405
79.302443	2144.914050	21.728423
79.489643	2151.304140	21.733440
79.407548	2157.086033	21.738458
79.340237	2153.823827	21.743475
79.328054	2155.757200	21.748493
79.338939	2148.755642	21.753511
78.904488	2150.079386	21.758528
79.339339	2153.117172	21.763546
79.721253	2159.836728	21.768563
79.555699	2162.137979	21.773581
79.834844	2167.222975	21.778599
79.784297	2170.626685	21.783616
79.978078	2170.056881	21.788634
80.124667	2179.634505	21.793651
79.878217	2185.943793	21.798669
79.862769	2181.578390	21.803687
80.224568	2182.775010	21.808704
80.255546	2187.327421	21.813722
80.490793	2196.187473	21.818739
80.494375	2212.986121	21.823757
80.416390	2215.248497	21.828775
80.470868	2214.492087	21.833792
80.204539	2213.735129	21.838810
80.661569	2217.533216	21.843827
80.620022	2234.578763	21.848845
81.095293	2232.898416	21.853863
80.844020	2238.801354	21.858880
80.530287	2244.553065	21.863898
81.302364	2252.177636	21.868915
81.337343	2255.568046	21.873933
82.019038	2253.038162	21.878951
81.788174	2250.833403	21.883968
81.771586	2259.865245	21.888986
81.937946	2243.586145	21.894003
81.746305	2253.159661	21.899021
81.811956	2250.369067	21.904039
82.275218	2245.985924	21.909056
82.257100	2251.237153	21.914074
82.440759	2261.295068	21.919091
82.465712	2260.792574	21.924109
82.966333	2255.671428	21.929127
82.540887	2254.150249	21.934144
82.462974	2267.385925	21.939162
82.786626	2263.854534	21.944179
82.694064	2268.760734	21.949197
82.908910	2275.667299	21.954215
82.850745	2267.795930	21.959232
83.172141	2276.260735	21.964250
83.538702	2261.105535	21.969267
83.430825	2270.555560	21.974285
83.302450	2255.363808	21.979303
83.639710	2267.594367	21.984320
83.569828	2256.429993	21.989338
83.451497	2237.399036	21.994355
83.273699	2249.858103	21.999373
83.782315	2251.839796	22.004391
83.682083	2256.904985	22.009408
83.847116	2253.546623	22.014426
83.665105	2260.745356	22.019443
83.927408	2263.822650	22.024461
83.588448	2268.918698	22.029479
83.310360	2266.443565	22.034496
83.625080	2282.704661	22.039514
83.883166	2291.649571	22.044531
83.889221	2294.735206	22.049549
84.119669	2289.899124	22.054567
84.384491	2302.049461	22.059584
84.478682	2315.514011	22.064602
84.492759	2309.398724	22.069619
84.887141	2306.380205	22.074637
84.803424	2308.132217	22.079655
84.959073	2306.653113	22.084672
84.673284	2303.541666	22.089690
84.641839	2311.499659	22.094707
84.827865	2332.861963	22.099725
85.285495	2328.855239	22.104743
85.882021	2337.618084	22.109760
85.007253	2337.388220	22.114778
85.417974	2332.697638	22.119795
85.157553	2341.278307	22.124813
85.378719	2353.725826	22.129831
85.729750	2364.505710	22.134848
85.786599	2356.231364	22.139866
86.284477	2362.813014	22.144883
86.417880	2347.671951	22.149901
86.618715	2346.905372	22.154919
86.871360	2345.786725	22.159936
86.360841	2346.128190	22.164954
86.068296	2350.964557	22.169971
86.401586	2346.772048	22.174989
86.919149	2348.622965	22.180007
86.523190	2355.886606	22.185024
86.528822	2354.260431	22.190042
86.879483	2349.108954	22.195059
86.690240	2362.642916	22.200077
87.091143	2367.759509	22.205095
87.179930	2363.813359	22.210112
87.181620	2370.282906	22.215130
87.708289	2370.390301	22.220147
87.162136	2372.507824	22.225165
87.572003	2370.604104	22.230183
87.479563	2360.506746	22.235200
87.293029	2366.055644	22.240218
87.524308	2367.689188	22.245235
87.439304	2386.338576	22.250253
87.774960	2387.681300	22.255271
87.848318	2388.080192	22.260288
87.810549	2396.285375	22.265306
87.770513	2396.623022	22.270323
87.880752	2408.141052	22.275341
88.031565	2410.352051	22.280359
88.376342	2415.906611	22.285376
88.400747	2428.047125	22.290394
88.681148	2418.674373	22.295411
88.659163	2417.974043	22.300429
88.500560	2415.764325	22.305447
89.018139	2410.754111	22.310464
88.889128	2408.157911	22.315482
89.078356	2410.299809	22.320499
89.227000	2415.566150	22.325517
89.097253	2421.712176	22.330535
89.227722	2428.480449	22.335552
88.975400	2439.240699	22.340570
89.394525	2436.360327	22.345587
89.193204	2445.181168	22.350605
89.384020	2444.144730	22.355623
89.388981	2446.425781	22.360640
89.392553	2453.409493	22.365658
89.904162	2457.350622	22.370675
89.991934	2453.511915	22.375693
90.013996	2451.952605	22.380711
90.251292	2456.952676	22.385728
90.375303	2462.740451	22.390746
90.186328	2454.564296	22.395763
90.460351	2451.965305	22.400781
90.194916	2458.372325	22.405799
90.511477	2465.843832	22.410816
90.542400	2477.778225	22.415834
90.467631	2486.645659	22.420851
90.683966	2491.020957	22.425869
90.638205	2482.494268	22.430887
90.625112	2487.315566	22.435904
90.766435	2505.090342	22.440922
91.230828	2505.115910	22.445939
91.141835	2512.495934	22.450957
91.252459	2507.429125	22.455975
91.356517	2507.580227	22.460992
91.738729	2531.711607	22.466010
91.829994	2525.379087	22.471027
91.541770	2526.474950	22.476045
91.718121	2530.427264	22.481063
91.654410	2527.224393	22.486080
91.735350	2526.788920	22.491098
92.047904	2536.078946	22.496115
92.067063	2544.815013	22.501133
92.149794	2554.267071	22.506151
92.073772	2549.816328	22.511168
92.200886	2553.889931	22.516186
92.309332	2553.178756	22.521203
92.719803	2568.049180	22.526221
92.773570	2572.355127	22.531239
93.117911	2571.954388	22.536256
92.953485	2577.323172	22.541274
92.784398	2576.617334	22.546291
92.778291	2572.812154	22.551309
92.956765	2580.431450	22.556327
92.713265	2581.236309	22.561344
93.183354	2598.530772	22.566362
93.614208	2600.647698	22.571379
93.802651	2602.657188	22.576397
93.597830	2598.797728	22.581415
93.838007	2604.460157	22.586432
93.860264	2618.119184	22.591450
94.113761	2628.573561	22.596467
94.275543	2618.051441	22.601485
94.295509	2622.394224	22.606503
94.443747	2618.006386	22.611520
94.464055	2615.465809	22.616538
94.560233	2620.689883	22.621555
94.779938	2617.906807	22.626573
94.621308	2622.157466	22.631591
94.731954	2611.062602	22.636608
94.659618	2614.845356	22.641626
94.624127	2618.063757	22.646643
95.028291	2624.817897	22.651661
94.813827	2640.454757	22.656679
95.251973	2641.680550	22.661696
95.060243	2641.783025	22.666714
94.934483	2640.802175	22.671731
95.323496	2637.020677	22.676749
95.313563	2656.687526	22.681767
95.624772	2658.630568	22.686784
95.873507	2669.846316	22.691802
95.701767	2663.538916	22.696819
96.279116	2663.467997	22.701837
96.066124	2663.330767	22.706855
96.024079	2658.275060	22.711872
95.733936	2663.622414	22.716890
96.338077	2672.188565	22.721907
96.442956	2679.472196	22.726925
96.138229	2687.472904	22.731943
96.629253	2681.731391	22.736960
96.802897	2689.184215	22.741978
96.614059	2686.707751	22.746995
96.843498	2678.573656	22.752013
96.850298	2701.551794	22.757031
97.256231	2697.934919	22.762048
97.405281	2699.196259	22.767066
97.127076	2695.417636	22.772083
97.462545	2699.307342	22.777101
97.356666	2707.526427	22.782119
97.380462	2700.361686	22.787136
97.507185	2707.149585	22.792154
97.744873	2728.703148	22.797171
98.146402	2723.420559	22.802189
97.920775	2722.676178	22.807207
98.368019	2725.604828	22.812224
98.193530	2723.508007	22.817242
98.014432	2719.294194	22.822259
98.656217	2724.859418	22.827277
97.949575	2723.741768	22.832295
98.238927	2738.403954	22.837312
98.505348	2743.333294	22.842330
98.393614	2739.314132	22.847347
98.728580	2744.639930	22.852365
98.688499	2756.396199	22.857383
99.053218	2759.309299	22.862400
98.804711	2767.544306	22.867418
99.368712	2769.173426	22.872435
99.673579	2764.568647	22.877453
99.389033	2770.470627	22.882471
99.420118	2770.967636	22.887488
99.553829	2781.099897	22.892506
99.455123	2789.510423	22.897523
99.701792	2792.252544	22.902541
99.833149	2785.926315	22.907559
99.824846	2785.656221	22.912576
100.240252	2792.828430	22.917594
100.529568	2807.566425	22.922611
100.435676	2808.272256	22.927629
100.164315	2811.110814	22.932647
100.462762	2812.506704	22.937664
100.502646	2809.729503	22.942682
100.838306	2805.123076	22.947699
101.079099	2809.999615	22.952717
100.942361	2810.226082	22.957735
101.158252	2814.872951	22.962752
101.165316	2828.130527	22.967770
101.472510	2838.548261	22.972787
101.488030	2833.609785	22.977805
101.508343	2840.041885	22.982823
101.418099	2833.664927	22.987840
101.501411	2828.065748	22.992858
101.541934	2832.992409	22.997875
101.658719	2839.560980	23.002893
101.953851	2841.604384	23.007911
101.993598	2848.724641	23.012928
102.321438	2850.996503	23.017946
102.418543	2857.798538	23.022963
102.820666	2850.063551	23.027981
102.511191	2858.560577	23.032999
102.201764	2849.856995	23.038016
102.589102	2855.013713	23.043034
102.261762	2852.198997	23.048051
102.515245	2852.440457	23.053069
102.521925	2875.018014	23.058087
102.506543	2870.516721	23.063104
103.039659	2879.198180	23.068122
102.615586	2878.689834	23.073139
102.913318	2886.868254	23.078157
103.395620	2887.272922	23.083175
103.420806	2892.511284	23.088192
103.604899	2897.680722	23.093210
104.073398	2915.859442	23.098227
104.144181	2919.496890	23.103245
104.104975	2921.159973	23.108263
104.376724	2914.382614	23.113280
104.552539	2908.740603	23.118298
104.524622	2904.077137	23.123315
104.810672	2902.268386	23.128333
104.794650	2906.531626	23.133351
104.526717	2897.796312	23.138368
104.504908	2901.015789	23.143386
104.545348	2895.846178	23.148403
105.098923	2906.171939	23.153421
105.242982	2919.995285	23.158439
105.442186	2925.736786	23.163456
105.446310	2917.505108	23.168474
105.081073	2924.830471	23.173491
105.444537	2917.660101	23.178509
105.169922	2918.867486	23.183527
105.468519	2924.896496	23.188544
106.086559	2932.883045	23.193562
105.767497	2941.940230	23.198579
106.077888	2944.697703	23.203597
106.148524	2943.926122	23.208615
106.421184	2940.677119	23.213632
106.460660	2942.141745	23.218650
106.194539	2949.663145	23.223667
106.208585	2938.908196	23.228685
106.720107	2952.948936	23.233703
106.819968	2960.230307	23.238720
106.669712	2965.032060	23.243738
106.887073	2973.166224	23.248755
107.148795	2968.915280	23.253773
107.440994	2969.785089	23.258791
107.192139	2963.514838	23.263808
107.501600	2969.633698	23.268826
107.486520	2990.614649	23.273843
107.792347	2988.392517	23.278861
107.819419	2996.916114	23.283879
107.940405	2999.368537	23.288896
108.076650	2991.614918	23.293914
107.832420	2989.992870	23.298931
108.064075	2989.426613	23.303949
108.060467	2983.828294	23.308967
108.100731	2999.968656	23.313984
108.055782	3004.135428	23.319002
108.110662	3011.998233	23.324019
108.558530	3004.319179	23.329037
108.518773	3009.649745	23.334055
108.166587	3021.224384	23.339072
108.687231	3032.855660	23.344090
108.520241	3036.697425	23.349107
108.643686	3035.728253	23.354125
109.011626	3051.909172	23.359143
109.286467	3053.715895	23.364160
109.166342	3060.690697	23.369178
109.235517	3060.064520	23.374195
109.846574	3073.060966	23.379213
109.825621	3079.272336	23.384231
110.162046	3080.867483	23.389248
110.049137	3075.333494	23.394266
110.219020	3079.214347	23.399283
110.319801	3071.399937	23.404301
110.466338	3077.922934	23.409319
110.127928	3081.611498	23.414336
110.854211	3079.065093	23.419354
110.640778	3093.461834	23.424371
110.470872	3096.502412	23.429389
110.849602	3098.166721	23.434407
110.740279	3100.216315	23.439424
111.011419	3110.283180	23.444442
111.149013	3120.153071	23.449459
111.510397	3115.028112	23.454477
111.305659	3129.354093	23.459495
111.376061	3129.911269	23.464512
111.453937	3127.279598	23.469530
111.840669	3139.888097	23.474547
112.101874	3148.444747	23.479565
112.575370	3148.759266	23.484583
112.284979	3144.717330	23.489600
112.671441	3137.981994	23.494618
112.373653	3142.106103	23.499635
112.475646	3138.498589	23.504653
112.535563	3139.070022	23.509671
112.390410	3155.895865	23.514688
112.518636	3158.842696	23.519706
112.687384	3161.574913	23.524723
112.651546	3161.204948	23.529741
113.223878	3172.768301	23.534759
112.995263	3181.170830	23.539776
113.604828	3182.849707	23.544794
113.748145	3187.905644	23.549811
113.498893	3186.688344	23.554829
114.171702	3173.290005	23.559847
113.694727	3173.329583	23.564864
114.155752	3186.191664	23.569882
114.411299	3189.819337	23.574899
114.394656	3204.731539	23.579917
114.751022	3206.875917	23.584935
114.413780	3209.282934	23.589952
115.084076	3204.980949	23.594970
114.596429	3202.194292	23.599987
114.433536	3202.749918	23.605005
114.752127	3204.745526	23.610023
114.248659	3217.565268	23.615040
114.664795	3215.426932	23.620058
114.839569	3221.506882	23.625075
115.229346	3232.315974	23.630093
115.669454	3241.898966	23.635111
115.441903	3255.439563	23.640128
115.672790	3249.372261	23.645146
115.449639	3247.911026	23.650163
115.553034	3253.692798	23.655181
115.696901	3266.418102	23.660199
115.889068	3274.281741	23.665216
115.802372	3279.398764	23.670234
116.081265	3276.969329	23.675251
116.185112	3285.695727	23.680269
116.621312	3303.314918	23.685287
116.759063	3296.624557	23.690304
116.945557	3290.816645	23.695322
117.021195	3297.798933	23.700339
116.785107	3302.535235	23.705357
117.017654	3292.295226	23.710375
117.147688	3319.004474	23.715392
117.414918	3324.722887	23.720410
117.549124	3313.150499	23.725427
117.454106	3321.008371	23.730445
117.694341	3319.130965	23.735463
117.859571	3328.267595	23.740480
118.011522	3338.728728	23.745498
118.011998	3342.497142	23.750515
118.261226	3339.955540	23.755533
118.528266	3339.427950	23.760551
118.401372	3345.602252	23.765568
118.455928	3332.520983	23.770586
118.507882	3351.588755	23.775603
118.713060	3361.448256	23.780621
118.902754	3365.711138	23.785639
118.793025	3369.417812	23.790656
118.874786	3367.363079	23.795674
119.721987	3382.011532	23.800691
119.181149	3395.768287	23.805709
119.833201	3385.005268	23.810727
119.989972	3378.772716	23.815744
120.111074	3389.989849	23.820762
120.342614	3381.773050	23.825779
120.527219	3382.530229	23.830797
120.740195	3370.169124	23.835815
120.299765	3373.640075	23.840832
120.722515	3374.767321	23.845850
120.807070	3382.095432	23.850867
120.457198	3374.029125	23.855885
121.060690	3370.580198	23.860903
120.643171	3379.337315	23.865920
120.746936	3391.655494	23.870938
121.205767	3401.668052	23.875955
121.019798	3405.594910	23.880973
121.124915	3403.233544	23.885991
120.768751	3422.292340	23.891008
121.562684	3428.231775	23.896026
121.452218	3423.356939	23.901043
121.190855	3439.500470	23.906061
121.835133	3438.096695	23.911079
122.198215	3448.007407	23.916096
122.281749	3441.981919	23.921114
122.413202	3445.758368	23.926131
122.396629	3453.686146	23.931149
122.679222	3454.355480	23.936167
122.996050	3459.476008	23.941184
123.574980	3458.760985	23.946202
123.416135	3450.989988	23.951219
123.777707	3453.449203	23.956237
123.815216	3445.167899	23.961255
123.843469	3432.302117	23.966272
123.892181	3421.288989	23.971290
123.767331	3418.663588	23.976307
123.522482	3423.584343	23.981325
123.960388	3433.761142	23.986343
124.429756	3442.604298	23.991360
124.516240	3440.302639	23.996378
124.256074	3446.131608	24.001395
124.093269	3452.052730	24.006413
124.453577	3441.859025	24.011431
124.344359	3449.454046	24.016448
124.493351	3449.591849	24.021466
124.862471	3446.794852	24.026483
124.440272	3462.329053	24.031501
124.538576	3468.039094	24.036519
124.597991	3476.677817	24.041536
124.736853	3483.602992	24.046554
125.198120	3490.048732	24.051571
125.046766	3499.155834	24.056589
125.225838	3506.283066	24.061607
125.341475	3522.450036	24.066624
125.709031	3526.205524	24.071642
125.892003	3525.747829	24.076659
125.743287	3520.598021	24.081677
126.185310	3542.224903	24.086695
126.128426	3549.297358	24.091712
126.269502	3548.801998	24.096730
126.576855	3542.732161	24.101747
126.494131	3556.575524	24.106765
126.474588	3565.737886	24.111783
126.451445	3572.050766	24.116800
126.977482	3575.349191	24.121818
127.364276	3583.832841	24.126835
127.368860	3597.135556	24.131853
127.494374	3593.978783	24.136871
127.566999	3595.447770	24.141888
127.473607	3601.115106	24.146906
128.271155	3601.161404	24.151923
128.207851	3615.513094	24.156941
128.556046	3606.678352	24.161959
128.822082	3613.959365	24.166976
128.581051	3611.872799	24.171994
128.442524	3611.146380	24.177011
128.536390	3609.055017	24.182029
128.863355	3609.534389	24.187047
129.137186	3623.041388	24.192064
128.984690	3632.502230	24.197082
129.190674	3627.729568	24.202099
129.044002	3631.101176	24.207117
129.328056	3632.076442	24.212135
129.493005	3641.794018	24.217152
128.985360	3656.476886	24.222170
129.445516	3657.891855	24.227187
129.948183	3680.147017	24.232205
129.803252	3689.445744	24.237223
130.104717	3684.257361	24.242240
130.130891	3681.968219	24.247258
130.308914	3693.340802	24.252275
130.310848	3702.319986	24.257293
130.717703	3695.290895	24.262311
130.541365	3711.585554	24.267328
130.904730	3726.098152	24.272346
131.092733	3734.407668	24.277363
131.091119	3728.240686	24.282381
131.309501	3725.407147	24.287399
131.395124	3744.296500	24.292416
131.599090	3752.972818	24.297434
131.867999	3741.259247	24.302451
131.804877	3750.753580	24.307469
132.029706	3755.986361	24.312487
132.254868	3762.263804	24.317504
132.324747	3769.228235	24.322522
132.514221	3769.893141	24.327539
132.664211	3769.330108	24.332557
132.465963	3773.198989	24.337575
132.496680	3777.862313	24.342592
133.140231	3794.244021	24.347610
133.200411	3792.164194	24.352627
133.389825	3796.799659	24.357645
133.491711	3800.700723	24.362663
133.269563	3798.260853	24.367680
133.356810	3797.650775	24.372698
133.707092	3792.571542	24.377715
133.794366	3821.207184	24.382733
133.905753	3815.729577	24.387751
134.216980	3811.133012	24.392768
134.111253	3815.157934	24.397786
134.578427	3816.035263	24.402803
134.779898	3836.554235	24.407821
135.154355	3831.891008	24.412839
135.134786	3837.468018	24.417856
135.076477	3832.629138	24.422874
135.072409	3826.238411	24.427891
134.900673	3834.607138	24.432909
135.176363	3839.708930	24.437927
135.371135	3853.521942	24.442944
135.553222	3862.337439	24.447962
135.774243	3854.664938	24.452979
135.582442	3865.950022	24.457997
135.663002	3882.135400	24.463015
136.019378	3889.471898	24.468032
136.046531	3890.572394	24.473050
135.946478	3883.035089	24.478067
136.196639	3899.632798	24.483085
136.443018	3906.045863	24.488103
136.897256	3907.998338	24.493120
136.811196	3932.782103	24.498138
137.191339	3925.738145	24.503155
137.480605	3935.133524	24.508173
137.111033	3934.326281	24.513191
137.381211	3941.903472	24.518208
137.474594	3957.468294	24.523226
137.736434	3947.504262	24.528243
137.753554	3956.266581	24.533261
137.972377	3963.687651	24.538279
138.549797	3971.431645	24.543296
138.363743	3977.845780	24.548314
138.775794	3974.145639	24.553331
138.668547	3979.281841	24.558349
138.789180	3983.334684	24.563367
139.221944	3978.416153	24.568384
139.336419	3999.062480	24.573402
139.312462	3998.018361	24.578419
139.375612	4003.475231	24.583437
139.714434	3991.182484	24.588455
139.952143	3992.275455	24.593472
139.897881	3996.661689	24.598490
140.286327	3998.046820	24.603507
140.338953	4010.651136	24.608525
140.277672	4023.086975	24.613543
140.143976	4023.376108	24.618560
140.124905	4022.394353	24.623578
140.460642	4022.477836	24.628595
140.356023	4041.605434	24.633613
140.277948	4049.988085	24.638631
140.811987	4050.192196	24.643648
140.782379	4070.286593	24.648666
141.388545	4062.045880	24.653683
141.673939	4063.797407	24.658701
141.568046	4079.055637	24.663719
142.130308	4084.627358	24.668736
142.341068	4088.508378	24.673754
142.113115	4079.052942	24.678771
142.077271	4090.872547	24.683789
142.210607	4094.973938	24.688807
142.515979	4094.200482	24.693824
142.265608	4094.504626	24.698842
142.530212	4099.343090	24.703859
142.504566	4112.369981	24.708877
142.437155	4117.815650	24.713895
142.717909	4114.735618	24.718912
143.208794	4139.881192	24.723930
143.220625	4136.767275	24.728947
143.076666	4148.594281	24.733965
143.340924	4151.775756	24.738983
143.624598	4155.689627	24.744000
143.308302	4167.218378	24.749018
143.840691	4174.802187	24.754035
144.078849	4186.983202	24.759053
143.933744	4201.101900	24.764071
144.058936	4203.102482	24.769088
144.038494	4219.619519	24.774106
144.163312	4221.298217	24.779123
144.818958	4233.032351	24.784141
144.878428	4243.713568	24.789159
145.397894	4232.453056	24.794176
145.371461	4257.104885	24.799194
145.655796	4254.570316	24.804211
146.328634	4256.312043	24.809229
146.494324	4261.371111	24.814247
146.572579	4253.518665	24.819264
146.374542	4263.567690	24.824282
146.609780	4254.005328	24.829299
147.024824	4256.544708	24.834317
146.830687	4261.571421	24.839335
146.792018	4250.808116	24.844352
146.827755	4265.542598	24.849370
146.942949	4270.218147	24.854387
147.099454	4274.612666	24.859405
146.903868	4276.334940	24.864423
147.395398	4284.171350	24.869440
147.535465	4295.136744	24.874458
147.459088	4307.818166	24.879475
147.504444	4308.874822	24.884493
147.607738	4338.420968	24.889511
148.007403	4331.301219	24.894528
147.955808	4345.320249	24.899546
148.074104	4350.636072	24.904563
148.669599	4355.871289	24.909581
148.976041	4373.937837	24.914599
149.012823	4372.893709	24.919616
149.537025	4375.924282	24.924634
149.405405	4382.314303	24.929651
149.186755	4370.916116	24.934669
149.513916	4378.771845	24.939687
150.175127	4387.326779	24.944704
149.858532	4395.153333	24.949722
150.086390	4409.984275	24.954739
150.297398	4397.774279	24.959757
150.247675	4398.637424	24.964775
150.358353	4401.227367	24.969792
150.480386	4417.681371	24.974810
150.501500	4415.250887	24.979827
151.028688	4423.653106	24.984845
150.924794	4440.890359	24.989863
151.209042	4446.675921	24.994880
151.323678	4439.638382	24.999898
151.396457	4451.725383	25.004915
151.721205	4454.149438	25.009933
151.987968	4469.883402	25.014951
152.244860	4467.716057	25.019968
151.891004	4466.003624	25.024986
152.361158	4465.286564	25.030003
152.663481	4469.787838	25.035021
152.531179	4484.166741	25.040039
152.738515	4489.358270	25.045056
152.823905	4484.780914	25.050074
152.467363	4492.288624	25.055091
153.168804	4491.838564	25.060109
153.146917	4510.603420	25.065127
153.082080	4509.398349	25.070144
153.269926	4516.142694	25.075162
153.880896	4531.737901	25.080179
154.029852	4536.698648	25.085197
153.889955	4539.529631	25.090215
154.410069	4544.347373	25.095232
154.381411	4531.953656	25.100250
154.325177	4550.329354	25.105267
154.840019	4560.131831	25.110285
154.635273	4571.602438	25.115303
154.888210	4561.311193	25.120320
155.099755	4574.345678	25.125338
155.048081	4586.594181	25.130355
155.302609	4579.752598	25.135373
155.087249	4593.844663	25.140391
155.727360	4605.066970	25.145408
155.582770	4612.150338	25.150426
155.324164	4617.553327	25.155443
156.186761	4632.323506	25.160461
156.036502	4644.754686	25.165479
156.386950	4649.693563	25.170496
156.856343	4662.498584	25.175514
156.601495	4662.307879	25.180531
157.220419	4664.370524	25.185549
157.220052	4684.154879	25.190567
157.533711	4676.054123	25.195584
157.710982	4684.706638	25.200602
157.676448	4683.206449	25.205619
157.962732	4689.219032	25.210637
158.167565	4701.566560	25.215655
158.183909	4693.919259	25.220672
158.225209	4703.947046	25.225690
158.260929	4697.758139	25.230707
158.674543	4707.058807	25.235725
158.544482	4735.130017	25.240743
158.631113	4724.438458	25.245760
159.009202	4726.507042	25.250778
159.250004	4741.781293	25.255795
159.560635	4748.509765	25.260813
159.633480	4752.557596	25.265831
159.473872	4758.870040	25.270848
159.589726	4771.225155	25.275866
160.020011	4780.984101	25.280883
160.093290	4778.176148	25.285901
160.005885	4805.417002	25.290919
160.404159	4797.495559	25.295936
160.535665	4805.710203	25.300954
160.579786	4819.294895	25.305971
161.058126	4828.131025	25.310989
160.991628	4834.305899	25.316007
161.266914	4843.072643	25.321024
161.607146	4847.287189	25.326042
161.290036	4857.604438	25.331059
162.113473	4856.636663	25.336077
162.060727	4870.170189	25.341095
162.332652	4880.742951	25.346112
162.373302	4879.240510	25.351130
162.384012	4872.594599	25.356147
162.289508	4874.891443	25.361165
162.468383	4903.445094	25.366183
162.505156	4904.563093	25.371200
163.164592	4902.213081	25.376218
162.820445	4913.339461	25.381235
163.321522	4916.496827	25.386253
163.428306	4930.311735	25.391271
163.530098	4929.513125	25.396288
163.984415	4946.411436	25.401306
163.943138	4952.834939	25.406323
164.307405	4948.346620	25.411341
164.109251	4960.517175	25.416359
164.532460	4966.268643	25.421376
164.934496	4960.893792	25.426394
164.730243	4975.634651	25.431411
165.052562	4973.766392	25.436429
165.060356	4998.619069	25.441447
165.156280	5001.432347	25.446464
165.531032	5004.211684	25.451482
165.345680	5011.311024	25.456499
165.823510	5023.969790	25.461517
166.178099	5028.791339	25.466535
166.376702	5027.093845	25.471552
166.336846	5033.883304	25.476570
166.224656	5042.887233	25.481587
166.618617	5042.759647	25.486605
166.772309	5049.178080	25.491623
166.986326	5058.364808	25.496640
167.113868	5069.383124	25.501658
166.914778	5070.159080	25.506675
167.581190	5084.474079	25.511693
167.673352	5092.246761	25.516711
167.611653	5097.802310	25.521728
167.788724	5090.619071	25.526746
167.727248	5117.332383	25.531763
168.546573	5116.087467	25.536781
168.075251	5119.734004	25.541799
168.434700	5141.580829	25.546816
168.994860	5151.733254	25.551834
168.946490	5163.356650	25.556851
168.819801	5167.984865	25.561869
168.911953	5175.135758	25.566887
168.803856	5198.194932	25.571904
169.328463	5193.252308	25.576922
169.424728	5212.712859	25.581939
170.120231	5218.276816	25.586957
170.271990	5221.078279	25.591975
169.912825	5234.195779	25.596992
170.408852	5233.799782	25.602010
170.688395	5249.267288	25.607027
171.117165	5269.165388	25.612045
171.355846	5274.380671	25.617063
171.313714	5272.244005	25.622080
171.707817	5270.143585	25.627098
171.861679	5279.011515	25.632115
171.682452	5279.623405	25.637133
172.150459	5294.420839	25.642151
171.929637	5289.022918	25.647168
172.854063	5292.158632	25.652186
172.724556	5303.273927	25.657203
173.256592	5302.960705	25.662221
173.102928	5319.609962	25.667239
173.261009	5312.341210	25.672256
173.449098	5309.439543	25.677274
173.058803	5312.719975	25.682292
173.558772	5327.985936	25.687309
173.712817	5333.280700	25.692327
173.819461	5335.625198	25.697344
173.933589	5337.330916	25.702362
173.794194	5357.740543	25.707380
174.222532	5356.057757	25.712397
174.320829	5356.913684	25.717415
174.798285	5373.360567	25.722432
174.930469	5381.310219	25.727450
174.856751	5388.439673	25.732468
174.942101	5388.025542	25.737485
175.278824	5407.221595	25.742503
175.083902	5414.404651	25.747520
175.195640	5411.054004	25.752538
175.483380	5427.467342	25.757556
175.982003	5433.459740	25.762573
176.368279	5435.053654	25.767591
176.429949	5458.897954	25.772608
176.870975	5452.172209	25.777626
176.601097	5459.098647	25.782644
176.839246	5469.670698	25.787661
177.523245	5473.481496	25.792679
177.485552	5488.133706	25.797696
177.539529	5481.373514	25.802714
177.518530	5493.441087	25.807732
177.746655	5511.442049	25.812749
177.860049	5504.783077	25.817767
177.936692	5519.859427	25.822784
178.282175	5532.027795	25.827802
178.376404	5539.955017	25.832820
178.228391	5542.298155	25.837837
178.962249	5548.437047	25.842855
178.735857	5553.522799	25.847872
179.703272	5564.653711	25.852890
179.876295	5579.064856	25.857908
179.890805	5581.291156	25.862925
180.155390	5586.486713	25.867943
180.102664	5580.506982	25.872960
180.431498	5577.210888	25.877978
180.485768	5596.605788	25.882996
180.449530	5598.079261	25.888013
180.845450	5601.152112	25.893031
181.277428	5617.034960	25.898048
181.439282	5625.762926	25.903066
181.183049	5624.211948	25.908084
181.134102	5633.989149	25.913101
181.377303	5640.030852	25.918119
181.515118	5651.701330	25.923136
181.932139	5660.493753	25.928154
182.069406	5677.539960	25.933172
182.223354	5682.402392	25.938189
182.598243	5675.778402	25.943207
182.871448	5693.905103	25.948224
183.020876	5697.325690	25.953242
183.156287	5710.385471	25.958260
183.428148	5702.107686	25.963277
183.650639	5710.213877	25.968295
183.760923	5727.965092	25.973312
183.773742	5726.728910	25.978330
184.391023	5739.527452	25.983348
184.333815	5748.068622	25.988365
184.571624	5749.928736	25.993383
184.320986	5756.217818	25.998400
184.726920	5771.795512	26.003418
184.646714	5789.112426	26.008436
184.652331	5790.942405	26.013453
184.897284	5801.617758	26.018471
184.951587	5817.098719	26.023488
185.463263	5822.918759	26.028506
185.412171	5834.205251	26.033524
185.225086	5848.581134	26.038541
185.889303	5856.934278	26.043559
185.908908	5874.428286	26.048576
186.282552	5884.641727	26.053594
186.335741	5890.586833	26.058612
186.579645	5912.989197	26.063629
186.672520	5914.862423	26.068647
187.022607	5926.840942	26.073664
187.606874	5943.224363	26.078682
187.895921	5937.169208	26.083700
187.862074	5936.423239	26.088717
188.066304	5935.283507	26.093735
188.410909	5959.302218	26.098752
188.306699	5971.357809	26.103770
188.516926	5969.349072	26.108788
188.591816	5978.100216	26.113805
189.094433	5983.874369	26.118823
189.106905	5993.175020	26.123840
189.512020	6006.344541	26.128858
189.257796	6023.215276	26.133876
189.051226	6025.214049	26.138893
189.708012	6029.202817	26.143911
189.864884	6041.066289	26.148928
190.138913	6059.919250	26.153946
190.299035	6073.411058	26.158964
190.287134	6081.610727	26.163981
190.552068	6095.338765	26.168999
190.686484	6102.483442	26.174016
191.265692	6103.977934	26.179034
191.462557	6123.565844	26.184052
191.560996	6140.198696	26.189069
191.942330	6147.248129	26.194087
192.070752	6154.403230	26.199104
192.235343	6150.403420	26.204122
192.408808	6173.580980	26.209140
192.397555	6178.560806	26.214157
192.618862	6178.573736	26.219175
192.821371	6202.706433	26.224192
192.767944	6204.539333	26.229210
193.276076	6217.917091	26.234228
193.476229	6231.147095	26.239245
194.139316	6234.759285	26.244263
194.342878	6249.301943	26.249280
194.206387	6261.309087	26.254298
194.461424	6264.249309	26.259316
194.466953	6267.111581	26.264333
194.410059	6269.459564	26.269351
194.688832	6286.111822	26.274368
195.039750	6310.363607	26.279386
195.614994	6303.768176	26.284404
195.491775	6309.551482	26.289421
196.046467	6313.470978	26.294439
196.299088	6321.247614	26.299456
196.275136	6327.451092	26.304474
196.653776	6325.573931	26.309492
196.924055	6344.888645	26.314509
197.325339	6347.357863	26.319527
197.265514	6347.862810	26.324544
197.291116	6349.516117	26.329562
197.667337	6342.853801	26.334580
197.375494	6357.925079	26.339597
197.629388	6365.085982	26.344615
197.905045	6373.004260	26.349632
197.857307	6392.977778	26.354650
198.178967	6403.448983	26.359668
198.260055	6411.151348	26.364685
198.584006	6409.554168	26.369703
198.743354	6441.080562	26.374720
199.190566	6449.256267	26.379738
199.608187	6443.663904	26.384756
199.175714	6460.165048	26.389773
199.742179	6455.963709	26.394791
199.910308	6476.348804	26.399808
200.092351	6487.091174	26.404826
200.272496	6483.445577	26.409844
200.240141	6497.040270	26.414861
200.425880	6505.954342	26.419879
200.437896	6514.027369	26.424896
200.701346	6525.615712	26.429914
201.078986	6530.677141	26.434932
201.124221	6543.552684	26.439949
201.098358	6567.270008	26.444967
201.675881	6578.187613	26.449984
201.658740	6584.674223	26.455002
202.224065	6581.057028	26.460020
202.550219	6607.371245	26.465037
202.814987	6612.693338	26.470055
202.690405	6611.566876	26.475072
203.130303	6612.565397	26.480090
203.386312	6632.198310	26.485108
203.483366	6634.714933	26.490125
203.963692	6639.368971	26.495143
203.682438	6657.418801	26.500160
203.884861	6661.424786	26.505178
204.211957	6665.322972	26.510196
204.199624	6678.879958	26.515213
204.192842	6693.742981	26.520231
204.527115	6706.608364	26.525248
204.863704	6714.201630	26.530266
205.105057	6724.215167	26.535284
205.438702	6742.402948	26.540301
205.732176	6750.653233	26.545319
205.979214	6762.133795	26.550336
205.597518	6760.062447	26.555354
206.226954	6774.368755	26.560372
206.161699	6788.937910	26.565389
206.857589	6804.266155	26.570407
207.164963	6815.099691	26.575424
206.992561	6827.024407	26.580442
207.522632	6840.033023	26.585460
207.479428	6846.441707	26.590477
207.734638	6860.411749	26.595495
208.131998	6872.699208	26.600512
207.900161	6869.780598	26.605530
208.474532	6885.973846	26.610548
208.291323	6899.829081	26.615565
208.608658	6913.852627	26.620583
209.040318	6931.141438	26.625600
209.333897	6938.122765	26.630618
209.542299	6936.815013	26.635636
209.756887	6954.156582	26.640653
210.164260	6972.528834	26.645671
210.373432	6982.092945	26.650688
210.352920	6976.278208	26.655706
210.578070	6981.698124	26.660724
211.023970	6998.972155	26.665741
211.193521	7000.274803	26.670759
211.131184	7001.089525	26.675776
211.508028	7020.833471	26.680794
211.676538	7033.418681	26.685812
211.697068	7037.730865	26.690829
212.258674	7046.318355	26.695847
212.073790	7054.529606	26.700864
212.051198	7068.707211	26.705882
212.602556	7073.400811	26.710900
212.959971	7085.584144	26.715917
213.060983	7094.956804	26.720935
213.460064	7093.556219	26.725952
213.132163	7101.322550	26.730970
213.714595	7118.970039	26.735988
213.670819	7132.298651	26.741005
213.952956	7133.508017	26.746023
214.437672	7155.536634	26.751040
214.121713	7162.950724	26.756058
214.734603	7169.967660	26.761076
214.583540	7192.688787	26.766093
214.647393	7191.015233	26.771111
215.446826	7201.718725	26.776128
215.287668	7213.243869	26.781146
215.758037	7224.178546	26.786164
215.658079	7247.813579	26.791181
215.528828	7249.588938	26.796199
215.979308	7262.218798	26.801216
216.216342	7284.750186	26.806234
216.803731	7288.011339	26.811252
216.988312	7291.571968	26.816269
217.303549	7313.671357	26.821287
217.452642	7306.049648	26.826304
217.788672	7317.800820	26.831322
217.974460	7320.019606	26.836340
218.074781	7341.691588	26.841357
218.033884	7363.808600	26.846375
218.833238	7361.218681	26.851392
218.458113	7392.381648	26.856410
219.262550	7384.765211	26.861428
219.269586	7400.232771	26.866445
219.161901	7416.640010	26.871463
219.884763	7422.838080	26.876480
219.875728	7441.351397	26.881498
220.330663	7447.660639	26.886516
220.430098	7450.994634	26.891533
220.653946	7470.810237	26.896551
220.976337	7472.411125	26.901568
221.015484	7487.845348	26.906586
221.411114	7485.678151	26.911604
221.492924	7500.515407	26.916621
221.571381	7519.703381	26.921639
222.051081	7522.706694	26.926656
221.964550	7530.606098	26.931674
222.471669	7537.396564	26.936692
222.994037	7553.917346	26.941709
223.340630	7560.183514	26.946727
223.262947	7573.921806	26.951744
223.537375	7574.747262	26.956762
223.329801	7565.198445	26.961780
223.852289	7580.412279	26.966797
223.990226	7589.978328	26.971815
223.966740	7609.580037	26.976832
224.430109	7623.859198	26.981850
224.868118	7636.226078	26.986868
224.963077	7639.103053	26.991885
225.065741	7649.678519	26.996903
225.005131	7655.802917	27.001920
225.334594	7678.576108	27.006938
225.579877	7694.262534	27.011956
226.063378	7702.092207	27.016973
226.271507	7708.642006	27.021991
226.835817	7715.758268	27.027008
226.405667	7731.770866	27.032026
226.963431	7745.347218	27.037044
227.204150	7750.480815	27.042061
227.083788	7757.571097	27.047079
227.351160	7769.307993	27.052096
227.803837	7779.955319	27.057114
227.934854	7797.803177	27.062132
227.860549	7805.426143	27.067149
228.241245	7828.232583	27.072167
228.619436	7826.525817	27.077184
228.876880	7833.516269	27.082202
228.811646	7840.755847	27.087220
229.349003	7858.572072	27.092237
229.572139	7867.209487	27.097255
230.073081	7874.840788	27.102272
229.982819	7879.928085	27.107290
230.667630	7896.834289	27.112308
230.595429	7908.163226	27.117325
230.609231	7910.531982	27.122343
231.264641	7921.198338	27.127360
231.125491	7935.476839	27.132378
231.006648	7945.515552	27.137396
231.495461	7953.874874	27.142413
231.330278	7950.677372	27.147431
232.040700	7970.079966	27.152448
232.036468	7985.407710	27.157466
232.555252	8004.868589	27.162484
232.296615	8015.904608	27.167501
232.869050	8040.828199	27.172519
233.411911	8039.528283	27.177536
233.389595	8060.424648	27.182554
233.220855	8066.906970	27.187572
233.908567	8086.808869	27.192589
233.761115	8103.563864	27.197607
234.588291	8116.075684	27.202624
234.544299	8129.824931	27.207642
234.589382	8136.176121	27.212660
235.262430	8151.610078	27.217677
235.248418	8168.735824	27.222695
235.710653	8177.209881	27.227712
235.730859	8190.519827	27.232730
235.973026	8204.335073	27.237748
236.314754	8211.391472	27.242765
237.098408	8215.105260	27.247783
237.945812	8217.574735	27.252800
237.657050	8217.161960	27.257818
237.426303	8217.766180	27.262836
237.876299	8233.395938	27.267853
237.939098	8238.980411	27.272871
238.489790	8244.087987	27.277888
238.623698	8265.370672	27.282906
239.095501	8267.134634	27.287924
239.258948	8267.857434	27.292941
239.121648	8270.079281	27.297959
239.456447	8279.021521	27.302976
239.738810	8299.971747	27.307994
239.326215	8310.987713	27.313012
239.970659	8320.753103	27.318029
239.639264	8337.555890	27.323047
240.507551	8340.861900	27.328064
240.131909	8361.207464	27.333082
240.185311	8377.243205	27.338100
240.464146	8400.542925	27.343117
240.668326	8421.442320	27.348135
241.112319	8431.119009	27.353152
241.632483	8454.504350	27.358170
241.961963	8481.370061	27.363188
242.310428	8485.672571	27.368205
242.281929	8498.178960	27.373223
242.498257	8511.903748	27.378240
242.713314	8540.583722	27.383258
243.003789	8556.232276	27.388276
243.417540	8565.632766	27.393293
243.235598	8587.372257	27.398311
243.853313	8600.977794	27.403328
243.961223	8618.416468	27.408346
244.314073	8637.067226	27.413364
244.537023	8646.326980	27.418381
244.757251	8654.611626	27.423399
244.984148	8666.036531	27.428416
245.495729	8678.790451	27.433434
245.913592	8696.455610	27.438452
245.860872	8703.049532	27.443469
246.310196	8711.718429	27.448487
246.438257	8720.525744	27.453504
246.706615	8722.002559	27.458522
246.191558	8752.387703	27.463540
246.682762	8750.265467	27.468557
246.768589	8780.844405	27.473575
247.619480	8793.545579	27.478592
247.569531	8807.435170	27.483610
247.371089	8831.141234	27.488628
247.909696	8841.213833	27.493645
248.355749	8863.496771	27.498663
248.473021	8875.481896	27.503680
248.979065	8888.846148	27.508698
249.457989	8908.730929	27.513716
249.710773	8908.836836	27.518733
249.991429	8931.306619	27.523751
249.972898	8945.273506	27.528768
250.488948	8967.094203	27.533786
250.579910	8982.483724	27.538804
250.861975	8987.800658	27.543821
250.820486	9011.946617	27.548839
250.868081	9027.620755	27.553856
251.491081	9032.846738	27.558874
251.403868	9049.574267	27.563892
252.125515	9067.009371	27.568909
252.237921	9101.357492	27.573927
252.622344	9112.319304	27.578944
252.701368	9112.000791	27.583962
252.708295	9133.042201	27.588980
253.606624	9145.505761	27.593997
253.522701	9168.278851	27.599015
253.802088	9171.256796	27.604032
254.300747	9189.361322	27.609050
254.442222	9206.233348	27.614068
255.083042	9216.716458	27.619085
255.250982	9221.962826	27.624103
255.392146	9229.401288	27.629120
255.808408	9240.894939	27.634138
255.480012	9252.716062	27.639156
256.569207	9269.955220	27.644173
256.716153	9278.242083	27.649191
256.603220	9287.986985	27.654208
256.810243	9306.661123	27.659226
256.935553	9315.207103	27.664244
257.128575	9321.652485	27.669261
257.196420	9337.061685	27.674279
257.472166	9360.170506	27.679296
258.146098	9375.283318	27.684314
258.193297	9394.964316	27.689332
258.388665	9404.850714	27.694349
258.705195	9420.227581	27.699367
259.083297	9444.498211	27.704384
259.599153	9444.929402	27.709402
259.248858	9465.010180	27.714420
259.760994	9478.017145	27.719437
260.018367	9501.286864	27.724455
260.573587	9514.160859	27.729472
260.720803	9519.562085	27.734490
260.400006	9543.559629	27.739508
261.317069	9546.877213	27.744525
261.252721	9561.953571	27.749543
261.339543	9584.564827	27.754560
262.079890	9591.212400	27.759578
262.065279	9613.173306	27.764596
262.435014	9613.747226	27.769613
262.622020	9630.094762	27.774631
263.076818	9646.299589	27.779648
263.739214	9636.374307	27.784666
263.497727	9657.110845	27.789684
264.182316	9664.862692	27.794701
264.234955	9675.807033	27.799719
264.426643	9683.007331	27.804736
264.816243	9693.722417	27.809754
264.718592	9715.481679	27.814772
265.219393	9717.588568	27.819789
265.593470	9734.529052	27.824807
265.298053	9745.417117	27.829824
265.849560	9755.046192	27.834842
266.162567	9765.722727	27.839860
266.107677	9777.716295	27.844877
266.885397	9797.827039	27.849895
266.756011	9816.282538	27.854912
267.321124	9828.028064	27.859930
267.240596	9841.860043	27.864948
267.790831	9852.332360	27.869965
267.923192	9875.470461	27.874983
268.058007	9894.983641	27.880000
268.479239	9903.872168	27.885018
268.871825	9921.258276	27.890036
269.098476	9934.518390	27.895053
269.346163	9946.155545	27.900071
269.571138	9962.980529	27.905088
269.748602	9965.469304	27.910106
270.179560	9986.158350	27.915124
270.646607	9999.090612	27.920141
270.890744	10017.402911	27.925159
271.155006	10035.914163	27.930176
271.264057	10042.328666	27.935194
271.310183	10058.812176	27.940212
271.463798	10080.539060	27.945229
271.826545	10093.197152	27.950247
271.848051	10112.478772	27.955264
272.168712	10126.059063	27.960282
272.587893	10161.753766	27.965300
272.862540	10162.497218	27.970317
273.201406	10185.470947	27.975335
273.394688	10208.334761	27.980352
273.999474	10218.464114	27.985370
274.245295	10237.483612	27.990388
274.197269	10248.586043	27.995405
274.866998	10266.017733	28.000423
274.974270	10279.419815	28.005440
275.817879	10292.170520	28.010458
276.087099	10306.987163	28.015476
276.339357	10305.435551	28.020493
277.112922	10308.257811	28.025511
276.530883	10322.417655	28.030528
277.082157	10330.225269	28.035546
277.235309	10338.975772	28.040564
277.599786	10357.613824	28.045581
278.260033	10366.639018	28.050599
277.872235	10383.755539	28.055616
278.409718	10393.898624	28.060634
278.690397	10407.848444	28.065652
279.076057	10425.220316	28.070669
279.142296	10426.949753	28.075687
279.174883	10453.394095	28.080704
279.410088	10453.209115	28.085722
279.691144	10482.459617	28.090740
279.761713	10485.375564	28.095757
280.385688	10507.247578	28.100775
280.574271	10529.894658	28.105792
281.027747	10531.068107	28.110810
281.078323	10538.656965	28.115828
281.200960	10569.062615	28.120845
281.438719	10577.686392	28.125863
281.768368	10597.296271	28.130880
282.409542	10603.189245	28.135898
282.461500	10622.567689	28.140916
282.818870	10632.969437	28.145933
282.980230	10648.213609	28.150951
282.803551	10667.703473	28.155968
283.269186	10677.529527	28.160986
283.578197	10698.610927	28.166004
283.633682	10716.287068	28.171021
284.498345	10736.022190	28.176039
284.278662	10759.329864	28.181056
284.429805	10776.391256	28.186074
285.193613	10799.864767	28.191092
285.671425	10821.519940	28.196109
285.624787	10826.844374	28.201127
286.066107	10859.202704	28.206144
286.891395	10872.095589	28.211162
287.127876	10889.282726	28.216180
287.307318	10899.191344	28.221197
287.692105	10908.499655	28.226215
288.166210	10925.807704	28.231232
288.603240	10922.882196	28.236250
288.835061	10933.341548	28.241268
289.081486	10947.126602	28.246285
289.344852	10956.779059	28.251303
289.820101	10970.740057	28.256320
289.914626	10984.397228	28.261338
289.811865	10985.316298	28.266356
289.912359	11007.797696	28.271373
290.582539	11013.095838	28.276391
290.655353	11032.506192	28.281408
290.940337	11052.865513	28.286426
291.243975	11071.876862	28.291444
291.307132	11082.561477	28.296461
291.803615	11099.439943	28.301479
291.790614	11120.534063	28.306496
292.185094	11123.958559	28.311514
292.672730	11149.117405	28.316532
292.914708	11179.082362	28.321549
293.264214	11189.198313	28.326567
293.707777	11210.685608	28.331584
293.776829	11216.645746	28.336602
294.101608	11231.912315	28.341620
293.860911	11262.337768	28.346637
294.409649	11275.747617	28.351655
294.419540	11307.349777	28.356672
295.120477	11321.800050	28.361690
295.882931	11342.505303	28.366708
295.874313	11365.964009	28.371725
296.673462	11372.786212	28.376743
296.831120	11384.116213	28.381760
296.874834	11398.160502	28.386778
297.534263	11403.605677	28.391796
297.659967	11419.983272	28.396813
298.395534	11434.548229	28.401831
298.140784	11451.547127	28.406848
298.486886	11449.867139	28.411866
299.507535	11458.713614	28.416884
299.315349	11471.304318	28.421901
299.688891	11480.889374	28.426919
299.687121	11488.938297	28.431936
300.052860	11503.857696	28.436954
300.387480	11516.372730	28.441972
300.461104	11533.743693	28.446989
300.693570	11539.302743	28.452007
300.401689	11554.570853	28.457024
300.381949	11570.519691	28.462042
300.900055	11590.862249	28.467060
301.289398	11615.301310	28.472077
301.962008	11632.515960	28.477095
302.047244	11661.552503	28.482112
302.379393	11674.737437	28.487130
302.938934	11693.987446	28.492148
303.276896	11705.608488	28.497165
303.659170	11724.289341	28.502183
303.630485	11749.567269	28.507200
304.210195	11767.658532	28.512218
304.781050	11765.362528	28.517236
304.833593	11789.364822	28.522253
305.405539	11795.594190	28.527271
305.822752	11818.466161	28.532288
306.137618	11824.274549	28.537306
306.214373	11835.601631	28.542324
306.404176	11858.003836	28.547341
306.875839	11860.172350	28.552359
307.299526	11882.089790	28.557376
307.455260	11901.352357	28.562394
307.345295	11907.242699	28.567412
307.532503	11921.994453	28.572429
308.525124	11953.817306	28.577447
308.683449	11967.686296	28.582464
308.717983	11982.114526	28.587482
309.393383	12003.007735	28.592500
309.137787	12016.960148	28.597517
309.476250	12037.877433	28.602535
309.980553	12067.038820	28.607552
310.171731	12067.435375	28.612570
310.771306	12097.210350	28.617588
310.692165	12127.286812	28.622605
311.065281	12146.973650	28.627623
311.562615	12160.328984	28.632640
311.694924	12187.274948	28.637658
311.863519	12199.232117	28.642676
312.651449	12231.627273	28.647693
312.943247	12252.769943	28.652711
313.032596	12269.311824	28.657728
313.113561	12288.491697	28.662746
313.939776	12313.896221	28.667764
313.975862	12332.075821	28.672781
314.240556	12343.853920	28.677799
314.908340	12370.814671	28.682816
315.179282	12383.157052	28.687834
315.889058	12393.141781	28.692852
315.989438	12417.806865	28.697869
316.417103	12422.821081	28.702887
316.876817	12441.016935	28.707904
317.144901	12459.507889	28.712922
317.574872	12453.065546	28.717940
317.438464	12481.218965	28.722957
318.115212	12497.123312	28.727975
318.392218	12508.479620	28.732992
318.403919	12522.125543	28.738010
318.717555	12550.344783	28.743028
318.885936	12559.747606	28.748045
319.490856	12580.816635	28.753063
319.762283	12603.333330	28.758080
319.553526	12617.556777	28.763098
319.828419	12628.218782	28.768116
319.737027	12657.960119	28.773133
320.678962	12679.538871	28.778151
320.993201	12704.205771	28.783168
321.036921	12731.737861	28.788186
321.492571	12740.957110	28.793204
321.779227	12759.994919	28.798221
321.734229	12783.858936	28.803239
322.569431	12805.066043	28.808256
322.404676	12826.113072	28.813274
323.310581	12847.852359	28.818292
323.711634	12861.595801	28.823309
324.087890	12869.488572	28.828327
324.929673	12885.904379	28.833344
325.023149	12901.268316	28.838362
325.627983	12912.273841	28.843380
325.414068	12929.949797	28.848397
325.503096	12941.367210	28.853415
325.897314	12963.865219	28.858432
326.013490	12990.988524	28.863450
326.683029	13005.748140	28.868468
326.659738	13028.368066	28.873485
326.990260	13046.391992	28.878503
327.303834	13071.125790	28.883520
327.714487	13089.020442	28.888538
328.480650	13099.789386	28.893556
328.568818	13123.203635	28.898573
329.000773	13132.966755	28.903591
329.379777	13158.078894	28.908608
329.816853	13177.940008	28.913626
330.509589	13188.505702	28.918644
330.373322	13217.215975	28.923661
331.000986	13220.702451	28.928679
331.184597	13237.558922	28.933696
331.166195	13250.186915	28.938714
332.083817	13266.344937	28.943732
332.076527	13290.573192	28.948749
332.309212	13299.413748	28.953767
332.650544	13317.032044	28.958784
332.541498	13341.822517	28.963802
333.236838	13353.193155	28.968820
333.563500	13388.595778	28.973837
333.890878	13402.227928	28.978855
333.945305	13427.192009	28.983872
334.255766	13458.176250	28.988890
335.128010	13476.700459	28.993908
335.402448	13503.092493	28.998925
335.650336	13511.719202	29.003943
336.374101	13524.923414	29.008960
335.991470	13556.309403	29.013978
336.447376	13570.227981	29.018996
336.938445	13594.963253	29.024013
337.149380	13620.124277	29.029031
338.094663	13648.028926	29.034048
337.862796	13660.049367	29.039066
338.358750	13678.875518	29.044084
338.655178	13705.182303	29.049101
338.925550	13723.017290	29.054119
339.346018	13746.810057	29.059136
339.978406	13761.032884	29.064154
340.843830	13755.570746	29.069172
341.344775	13770.853006	29.074189
341.359836	13778.856076	29.079207
341.520238	13793.979789	29.084224
342.061193	13805.248418	29.089242
342.381096	13818.446237	29.094260
342.093849	13833.740727	29.099277
342.610855	13859.084949	29.104295
342.912879	13864.794916	29.109312
343.050255	13895.358389	29.114330
343.285373	13917.557035	29.119348
343.414164	13935.960592	29.124365
343.829156	13952.314300	29.129383
343.856587	13976.253809	29.134400
344.237811	14009.403779	29.139418
344.636873	14024.007350	29.144436
345.212403	14042.578310	29.149453
345.428146	14072.703540	29.154471
345.672815	14095.504083	29.159488
345.688150	14122.227852	29.164506
346.253584	14149.649203	29.169524
346.877000	14172.656147	29.174541
346.938643	14195.614782	29.179559
347.433149	14226.805320	29.184576
347.605935	14237.297808	29.189594
348.016431	14259.880093	29.194612
348.552851	14290.104171	29.199629
349.445635	14311.575602	29.204647
349.811817	14329.869949	29.209664
349.963830	14351.510436	29.214682
350.633925	14368.753251	29.219700
350.912402	14385.185430	29.224717
351.212126	14402.801741	29.229735
351.786770	14416.332967	29.234752
351.638125	14436.801352	29.239770
352.474361	14450.854011	29.244788
352.749084	14470.947033	29.249805
353.171248	14488.626471	29.254823
353.815011	14504.600812	29.259840
353.786916	14516.271105	29.264858
353.827591	14541.134576	29.269876
354.052752	14567.431547	29.274893
354.331077	14589.959008	29.279911
354.757404	14610.454915	29.284928
355.056053	14634.943591	29.289946
355.761426	14654.249719	29.294964
355.552671	14669.248432	29.299981
355.558467	14708.843729	29.304999
356.072300	14733.330612	29.310016
356.538056	14763.402223	29.315034
356.903791	14793.113639	29.320052
357.541590	14813.118917	29.325069
357.707822	14850.440954	29.330087
358.180052	14878.923207	29.335104
358.485693	14905.069157	29.340122
358.749939	14932.216399	29.345140
359.266617	14951.886968	29.350157
359.583027	14986.046704	29.355175
360.246721	15006.310280	29.360192
360.602450	15040.631374	29.365210
361.179656	15057.447136	29.370228
361.486016	15083.451102	29.375245
362.007431	15108.006767	29.380263
362.281447	15128.899609	29.385280
362.284411	15155.317253	29.390298
362.575720	15175.241053	29.395316
363.759149	15196.245044	29.400333
363.915443	15210.631511	29.405351
364.158335	15230.398682	29.410368
364.344916	15259.153363	29.415386
364.942977	15267.685300	29.420404
365.346212	15284.310433	29.425421
365.845907	15308.004393	29.430439
366.417024	15320.115626	29.435456
366.651607	15338.734619	29.440474
366.976831	15347.798589	29.445492
367.691961	15355.175389	29.450509
367.965704	15378.342453	29.455527
368.541540	15406.509336	29.460544
368.313496	15403.958298	29.465562
368.391852	15407.641241	29.470580
368.713926	15426.221432	29.475597
369.172093	15441.559074	29.480615
369.546945	15457.582399	29.485632
369.848607	15483.802401	29.490650
370.175538	15516.015983	29.495668
370.444554	15530.015629	29.500685
370.269364	15563.289671	29.505703
370.421012	15572.633430	29.510720
371.059851	15608.209507	29.515738
370.994545	15630.062140	29.520756
371.523297	15666.334486	29.525773
371.657422	15709.869172	29.530791
372.019203	15732.988219	29.535808
372.784455	15767.136325	29.540826
373.286957	15798.533481	29.545844
373.616333	15826.297194	29.550861
374.239625	15852.947690	29.555879
374.262824	15881.296057	29.560896
374.699441	15914.494411	29.565914
375.779509	15936.162763	29.570932
376.465581	15966.176707	29.575949
376.792888	15984.813477	29.580967
377.208115	16007.482373	29.585984
377.585415	16022.924662	29.591002
377.808530	16043.737997	29.596020
378.572778	16059.385374	29.601037
378.524211	16077.303804	29.606055
379.102563	16090.867230	29.611072
379.391164	16114.762447	29.616090
379.899317	16130.610826	29.621108
380.164657	16154.775014	29.626125
380.091760	16176.812635	29.631143
380.773829	16200.517211	29.636160
380.915541	16224.609141	29.641178
380.942402	16245.851200	29.646196
381.837558	16271.022905	29.651213
381.944706	16304.074251	29.656231
382.919441	16330.702284	29.661248
383.306251	16349.418580	29.666266
383.275176	16376.891786	29.671284
384.111125	16391.157540	29.676301
384.241625	16417.765524	29.681319
384.613856	16444.872836	29.686336
385.139381	16466.694451	29.691354
385.546582	16494.317522	29.696372
385.688178	16510.513855	29.701389
385.837312	16536.260018	29.706407
385.886548	16569.074481	29.711424
386.382399	16594.570924	29.716442
386.662870	16622.542384	29.721460
387.538427	16653.131163	29.726477
387.892484	16680.623806	29.731495
388.273392	16707.095295	29.736512
388.544825	16727.023807	29.741530
389.123938	16756.686105	29.746548
389.944991	16768.032910	29.751565
390.449360	16800.072580	29.756583
390.560146	16822.003384	29.761600
391.301600	16839.013080	29.766618
391.975719	16849.359472	29.771636
392.281307	16858.165066	29.776653
392.467971	16875.678081	29.781671
392.470040	16894.255823	29.786688
393.067583	16912.996715	29.791706
393.688942	16950.495192	29.796724
393.922224	16948.443808	29.801741
394.372157	16980.587008	29.806759
394.801054	16987.990055	29.811776
394.875942	16994.775463	29.816794
395.159486	17015.340400	29.821812
395.677516	17037.647078	29.826829
395.544120	17055.608052	29.831847
396.162103	17076.531592	29.836864
396.703956	17092.745065	29.841882
396.495573	17135.395075	29.846900
397.027137	17147.561005	29.851917
397.365210	17180.502103	29.856935
397.943106	17206.444569	29.861952
398.635383	17241.342597	29.866970
398.951847	17250.904722	29.871988
399.296908	17277.587882	29.877005
399.850501	17296.465489	29.882023
400.385380	17322.579053	29.887040
400.745099	17348.862055	29.892058
400.635105	17380.619313	29.897076
401.077505	17394.880757	29.902093
401.805784	17426.330710	29.907111
401.679620	17459.587765	29.912128
402.150738	17494.372230	29.917146
402.626063	17507.469442	29.922164
402.610150	17542.737269	29.927181
403.100577	17580.456346	29.932199
403.174742	17612.681211	29.937216
403.978971	17643.876485	29.942234
404.228586	17697.205080	29.947252
404.717096	17722.277753	29.952269
404.986104	17759.311491	29.957287
406.089134	17787.017608	29.962304
406.996665	17809.953119	29.967322
407.574741	17833.881213	29.972340
407.903080	17852.705993	29.977357
408.054410	17883.093618	29.982375
408.628240	17905.670573	29.987392
409.161805	17925.253130	29.992410
409.646043	17953.112675	29.997428
409.978145	17965.916634	30.002445
410.233987	17992.459898	30.007463
410.272041	18018.954980	30.012480
410.614481	18043.640188	30.017498
411.008032	18074.691623	30.022516
411.369837	18095.558235	30.027533
411.472136	18131.064582	30.032551
411.879524	18169.568450	30.037568
412.458437	18199.991083	30.042586
412.575337	18236.923069	30.047604
413.197847	18264.755220	30.052621
413.536444	18304.419825	30.057639
414.139603	18342.476613	30.062656
414.531146	18365.992189	30.067674
414.594788	18405.567140	30.072692
415.508464	18439.425242	30.077709
416.281751	18470.715114	30.082727
416.521509	18494.317650	30.087744
416.938046	18515.403621	30.092762
417.051821	18545.526481	30.097780
417.522246	18577.065832	30.102797
418.562120	18605.294673	30.107815
418.555725	18628.379755	30.112832
419.332866	18648.771668	30.117850
419.332724	18689.765928	30.122868
419.852923	18713.653582	30.127885
420.433368	18740.633786	30.132903
420.708018	18762.576027	30.137920
421.731856	18768.721559	30.142938
422.071691	18799.731979	30.147956
422.443276	18810.079146	30.152973
422.852878	18839.278270	30.157991
423.103940	18857.212649	30.163008
423.232806	18877.295085	30.168026
423.685843	18899.304473	30.173044
424.041202	18916.622501	30.178061
424.458376	18937.967854	30.183079
424.900964	18960.105290	30.188096
425.461515	18992.635783	30.193114
425.690487	19015.773130	30.198132
426.180337	19053.059253	30.203149
426.870003	19073.471549	30.208167
426.532066	19103.791949	30.213184
427.353449	19128.296577	30.218202
427.614205	19158.555446	30.223220
427.734813	19188.949898	30.228237
428.107149	19226.519990	30.233255
428.156286	19261.916644	30.238272
428.595945	19300.853653	30.243290
429.190890	19344.725967	30.248308
429.923562	19380.035377	30.253325
430.910471	19399.308776	30.258343
431.117179	19442.142466	30.263360
431.684616	19465.436142	30.268378
431.734494	19505.994726	30.273396
432.248234	19541.155296	30.278413
433.051498	19560.609073	30.283431
433.175546	19604.479468	30.288448
433.883973	19623.834351	30.293466
434.411930	19670.200724	30.298484
434.853677	19691.069242	30.303501
435.612145	19711.458863	30.308519
435.778284	19751.475479	30.313536
436.272122	19773.340512	30.318554
436.615958	19802.399692	30.323572
437.267929	19833.590609	30.328589
437.793015	19860.656801	30.333607
438.041845	19887.165839	30.338624
438.353880	19904.005014	30.343642
438.815466	19946.048301	30.348660
439.297961	19971.124820	30.353677
439.766202	19995.792924	30.358695
440.173485	20020.925440	30.363712
440.258016	20056.229574	30.368730
440.880546	20081.638238	30.373748
441.177670	20118.242474	30.378765
441.596747	20152.565959	30.383783
442.147197	20187.620893	30.388800
442.816664	20220.275477	30.393818
443.234978	20255.704911	30.398836
443.637598	20290.606139	30.403853
444.016224	20313.304739	30.408871
444.133991	20344.263736	30.413888
444.955613	20374.013866	30.418906
445.267675	20413.958576	30.423924
445.724804	20447.815437	30.428941
446.384582	20472.024696	30.433959
446.632494	20511.531008	30.438976
447.132497	20533.977199	30.443994
447.672748	20559.475111	30.449012
448.193507	20596.967871	30.454029
448.495049	20627.330075	30.459047
448.671215	20665.097745	30.464064
449.252869	20698.411248	30.469082
449.835176	20727.207224	30.474100
450.028202	20762.318831	30.479117
450.743507	20789.255606	30.484135
450.918164	20825.975003	30.489152
451.385001	20845.798348	30.494170
452.197041	20879.354294	30.499188
452.763447	20908.481559	30.504205
453.118152	20923.362641	30.509223
453.583584	20951.362091	30.514240
453.840027	20971.900686	30.519258
454.317851	21002.968944	30.524276
454.385457	21027.365853	30.529293
454.892865	21059.680609	30.534311
455.549814	21095.826285	30.539328
456.192682	21125.005151	30.544346
456.574393	21156.151796	30.549364
456.706794	21183.994920	30.554381
457.117332	21219.402034	30.559399
457.508599	21259.077083	30.564416
458.387578	21285.414092	30.569434
458.550686	21322.970237	30.574452
459.015610	21358.438636	30.579469
459.782479	21393.285121	30.584487
460.282615	21440.816280	30.589504
460.542992	21463.787357	30.594522
460.899715	21493.087137	30.599540
461.117955	21532.423206	30.604557
461.932288	21553.766455	30.609575
461.938257	21593.900222	30.614592
462.683659	21631.429488	30.619610
463.539907	21670.287402	30.624628
463.775021	21703.947211	30.629645
464.219156	21729.606933	30.634663
464.707787	21774.891311	30.639680
465.510658	21802.694117	30.644698
466.033915	21835.292013	30.649716
466.317753	21866.417109	30.654733
467.277855	21900.267677	30.659751
467.435065	21937.636355	30.664768
468.037116	21966.051962	30.669786
468.943577	21991.084018	30.674804
469.301883	22007.823019	30.679821
469.988033	22023.803316	30.684839
470.224244	22061.071469	30.689856
470.604052	22076.158030	30.694874
471.280682	22105.402600	30.699892
471.779530	22137.789965	30.704909
472.171254	22154.119497	30.709927
472.099135	22190.822989	30.714944
472.903950	22216.085990	30.719962
473.312812	22245.277674	30.724980
473.481633	22284.502882	30.729997
473.945011	22305.573014	30.735015
474.506412	22337.344377	30.740032
474.995671	22374.144057	30.745050
475.480515	22409.920863	30.750068
476.089584	22449.419071	30.755085
476.221351	22482.843548	30.760103
476.333887	22510.382019	30.765120
477.182923	22548.579322	30.770138
477.634860	22580.551360	30.775156
478.052085	22614.462395	30.780173
478.866445	22655.180170	30.785191
478.869356	22695.436706	30.790208
479.311491	22725.811851	30.795226
479.637321	22758.050241	30.800244
480.042423	22807.431940	30.805261
480.654404	22838.564352	30.810279
481.129322	22885.439437	30.815296
481.849906	22925.837469	30.820314
482.330770	22954.399742	30.825332
482.934840	22985.514660	30.830349
483.546874	23009.917727	30.835367
483.848526	23050.678219	30.840384
484.096605	23071.744772	30.845402
484.782945	23103.308348	30.850420
485.131449	23134.355864	30.855437
485.854620	23167.897952	30.860455
486.355052	23210.694120	30.865472
486.724544	23240.481063	30.870490
486.938221	23268.226005	30.875508
487.202081	23305.947161	30.880525
487.674660	23324.539907	30.885543
488.509261	23371.568673	30.890560
489.014888	23406.990181	30.895578
489.919873	23442.033630	30.900596
489.919745	23483.871993	30.905613
490.896567	23513.451056	30.910631
491.465613	23549.962460	30.915648
491.959624	23575.420923	30.920666
492.308171	23598.267010	30.925684
492.936451	23635.022113	30.930701
493.420094	23661.082613	30.935719
493.726131	23693.748983	30.940736
494.400041	23735.457666	30.945754
494.952277	23757.829888	30.950772
495.095392	23794.515475	30.955789
495.595478	23826.911728	30.960807
496.981390	23847.662949	30.965824
497.553462	23867.232822	30.970842
498.260142	23895.710742	30.975860
498.850305	23920.459571	30.980877
499.436959	23938.731813	30.985895
499.557212	23958.795499	30.990912
500.342181	23971.273799	30.995930
500.749291	23997.877468	31.000948
501.435854	24020.974741	31.005965
501.581292	24042.311071	31.010983
502.033361	24074.140154	31.016000
502.186487	24103.456535	31.021018
502.518984	24129.515902	31.026036
503.047926	24165.737677	31.031053
503.686046	24197.455842	31.036071
503.819950	24231.363190	31.041088
504.208305	24261.850167	31.046106
505.111655	24297.312453	31.051124
505.246393	24331.055539	31.056141
505.824327	24370.233813	31.061159
506.396817	24412.591635	31.066176
506.328938	24449.153289	31.071194
506.668987	24484.337078	31.076212
507.021144	24530.874949	31.081229
507.821425	24570.221221	31.086247
508.678129	24607.081584	31.091264
508.801544	24656.834013	31.096282
509.596600	24687.359436	31.101300
510.330898	24732.264750	31.106317
510.414838	24775.040645	31.111335
510.965071	24809.655134	31.116352
511.524376	24849.058427	31.121370
512.556056	24891.288904	31.126388
513.047114	24932.194384	31.131405
513.594328	24965.362448	31.136423
514.583058	24993.014410	31.141440
514.899556	25027.330728	31.146458
515.654497	25054.564164	31.151476
516.183365	25086.724160	31.156493
516.400446	25118.231274	31.161511
516.904530	25135.676968	31.166528
517.648283	25168.802133	31.171546
518.476560	25188.674677	31.176564
518.620018	25211.643013	31.181581
519.054806	25236.114323	31.186599
519.341538	25268.261748	31.191616
519.931510	25305.740008	31.196634
520.665662	25320.160870	31.201652
520.960654	25344.793107	31.206669
521.406037	25371.872938	31.211687
521.844058	25395.465510	31.216704
521.978237	25439.138710	31.221722
522.565588	25465.160143	31.226740
522.777524	25508.688676	31.231757
523.122436	25542.135655	31.236775
524.151734	25581.543060	31.241792
524.242096	25614.277743	31.246810
524.912309	25664.674314	31.251828
525.131362	25711.760185	31.256845
525.541128	25746.233846	31.261863
526.422838	25791.750562	31.266880
527.533114	25835.108352	31.271898
528.201444	25871.937173	31.276916
528.393293	25901.433430	31.281933
529.090459	25940.387661	31.286951
530.151030	25972.820213	31.291968
530.414609	26010.590754	31.296986
530.858078	26028.899841	31.302004
531.644367	26073.288158	31.307021
532.290014	26101.506971	31.312039
533.036974	26133.912767	31.317056
533.164462	26176.413111	31.322074
533.633219	26197.309568	31.327092
534.393556	26233.404261	31.332109
534.559639	26271.797179	31.337127
535.388027	26300.171100	31.342144
535.402595	26341.343226	31.347162
535.836070	26380.307759	31.352180
536.359174	26421.539921	31.357197
536.823076	26463.735700	31.362215
537.434914	26496.814073	31.367232
537.862496	26538.143503	31.372250
538.585355	26581.076574	31.377268
539.237521	26631.667976	31.382285
539.427457	26669.514415	31.387303
540.474652	26702.026067	31.392320
540.866305	26755.647720	31.397338
541.740425	26795.915912	31.402356
542.483788	26825.732148	31.407373
542.519067	26854.634804	31.412391
543.467643	26889.386786	31.417408
544.097984	26931.153144	31.422426
544.388533	26963.460683	31.427444
545.141543	27002.294511	31.432461
545.433218	27040.498694	31.437479
546.085672	27062.056347	31.442496
546.551904	27102.856342	31.447514
547.281224	27130.791803	31.452532
547.990645	27172.811797	31.457549
547.901553	27208.269404	31.462567
548.537806	27238.241969	31.467584
549.165549	27286.310723	31.472602
549.406044	27318.007237	31.477620
550.126251	27364.405879	31.482637
550.909183	27400.669789	31.487655
552.117394	27426.559183	31.492672
552.563069	27462.205756	31.497690
553.350055	27488.881318	31.502708
553.983248	27513.223383	31.507725
554.048082	27541.104846	31.512743
554.744865	27560.014241	31.517760
554.531115	27593.153408	31.522778
555.161436	27620.890066	31.527796
555.883358	27654.256573	31.532813
556.260847	27689.977365	31.537831
556.982901	27717.516584	31.542848
557.471445	27761.759033	31.547866
557.604426	27792.025657	31.552884
558.255755	27831.780720	31.557901
558.766348	27869.440432	31.562919
559.255266	27908.443518	31.567936
559.839295	27953.132909	31.572954
560.492066	27987.661050	31.577972
561.226158	28025.665485	31.582989
561.156220	28075.747180	31.588007
562.348577	28106.253865	31.593024
562.479602	28157.802433	31.598042
563.054147	28197.045562	31.603060
563.385662	28246.723874	31.608077
564.316836	28282.410076	31.613095
564.790267	28332.268760	31.618112
565.144748	28373.531144	31.623130
566.003749	28420.043323	31.628148
566.529810	28465.178983	31.633165
567.184790	28520.413979	31.638183
568.179461	28555.610408	31.643200
568.695764	28591.981160	31.648218
569.524508	28633.018543	31.653236
570.103232	28675.738303	31.658253
570.740738	28711.072772	31.663271
571.308404	28740.546257	31.668288
571.974005	28786.792309	31.673306
572.669187	28821.896767	31.678324
573.138339	28849.704437	31.683341
573.737640	28895.449078	31.688359
574.071778	28927.272576	31.693376
574.818344	28967.874653	31.698394
575.200350	29007.073466	31.703412
575.848165	29043.045302	31.708429
576.228881	29072.181765	31.713447
577.112250	29117.004091	31.718464
577.623723	29160.082977	31.723482
577.967348	29197.170657	31.728500
578.661738	29232.832177	31.733517
579.220438	29281.143941	31.738535
580.203859	29309.384168	31.743552
580.682689	29342.095990	31.748570
581.065931	29393.210195	31.753588
581.848571	29429.458804	31.758605
582.051737	29470.949227	31.763623
582.711265	29510.554586	31.768640
583.648319	29549.035939	31.773658
584.162201	29601.268093	31.778676
584.380132	29628.882056	31.783693
584.778438	29663.174524	31.788711
585.367080	29707.803829	31.793728
585.906199	29746.657229	31.798746
586.367165	29793.259782	31.803764
587.466145	29833.555876	31.808781
587.676507	29885.962425	31.813799
588.564714	29922.505204	31.818816
589.138457	29971.018524	31.823834
589.489868	30018.087438	31.828852
590.363480	30041.604963	31.833869
591.141204	30089.479985	31.838887
591.712280	30131.337982	31.843904
591.852330	30161.025467	31.848922
592.583798	30201.309963	31.853940
592.979543	30239.902165	31.858957
593.710647	30277.064219	31.863975
594.215786	30311.252642	31.868992
594.610710	30358.783328	31.874010
595.043940	30402.161455	31.879028
595.954750	30449.093702	31.884045
596.079552	30486.344198	31.889063
596.677593	30529.184917	31.894080
597.604726	30573.712838	31.899098
598.288325	30610.307657	31.904116
599.466218	30649.202390	31.909133
599.839335	30688.487973	31.914151
600.098162	30725.035338	31.919168
601.140788	30758.142066	31.924186
601.596461	30807.048694	31.929204
602.116450	30848.024795	31.934221
602.576829	30887.094889	31.939239
603.294617	30934.886387	31.944256
603.948438	30970.405528	31.949274
604.276717	31016.203406	31.954292
605.073100	31059.893023	31.959309
605.128569	31115.335793	31.964327
605.953059	31154.273854	31.969344
606.636405	31202.368439	31.974362
606.990966	31266.147285	31.979380
607.570090	31302.298128	31.984397
608.262164	31358.249308	31.989415
608.880097	31407.479778	31.994432
609.545765	31453.434710	31.999450
610.100449	31511.253574	32.004468
610.775741	31559.622070	32.009485
611.769249	31605.753880	32.014503
612.524619	31654.780218	32.019520
613.345374	31697.607654	32.024538
613.713008	31740.840763	32.029556
614.955994	31772.596714	32.034573
615.155988	31810.432119	32.039591
615.837039	31852.036263	32.044608
616.776527	31895.844445	32.049626
616.885327	31944.548570	32.054644
618.095432	31981.215574	32.059661
618.452462	32019.949881	32.064679
619.249367	32053.710143	32.069696
620.417574	32089.941344	32.074714
620.712136	32134.836615	32.079732
621.524889	32162.007351	32.084749
622.005807	32200.836500	32.089767
622.474030	32231.607460	32.094784
622.977662	32271.109632	32.099802
623.072514	32306.338776	32.104820
623.873638	32348.424643	32.109837
624.444487	32391.368276	32.114855
625.525284	32431.811359	32.119872
625.927691	32476.519890	32.124890
626.411994	32509.457145	32.129908
626.912854	32555.383277	32.134925
627.201132	32602.790310	32.139943
628.290352	32643.143987	32.144960
628.801883	32697.755035	32.149978
629.453944	32739.333858	32.154996
630.084612	32782.534507	32.160013
630.754522	32821.657811	32.165031
631.139098	32866.458461	32.170048
631.856443	32911.283267	32.175066
632.468091	32959.519524	32.180084
633.254217	32998.448053	32.185101
633.440333	33043.924821	32.190119
634.205020	33084.355162	32.195136
634.725299	33130.083553	32.200154
634.663740	33179.025709	32.205172
635.574818	33231.382206	32.210189
636.388419	33282.072337	32.215207
636.955050	33326.453663	32.220224
637.535665	33371.604203	32.225242
638.319354	33429.601374	32.230260
638.567716	33471.750270	32.235277
639.556064	33526.567431	32.240295
639.770209	33570.896671	32.245312
640.845094	33621.837771	32.250330
641.324627	33680.262315	32.255348
642.192454	33729.984118	32.260365
642.711596	33776.314708	32.265383
643.493058	33831.518917	32.270400
644.157231	33877.068484	32.275418
644.545167	33932.789423	32.280436
645.288338	33974.957137	32.285453
646.549946	34024.352802	32.290471
647.179882	34065.058907	32.295488
648.184882	34109.822535	32.300506
649.022895	34146.968553	32.305524
650.243376	34189.030783	32.310541
650.563852	34224.228031	32.315559
651.197322	34261.108942	32.320576
651.962812	34292.361418	32.325594
652.192653	34340.280949	32.330612
652.905523	34370.416347	32.335629
653.617922	34413.076557	32.340647
653.410072	34465.306847	32.345664
654.393905	34512.799597	32.350682
654.964402	34565.857336	32.355700
655.881770	34602.403818	32.360717
655.929657	34659.545272	32.365735
656.178162	34714.752576	32.370752
657.197911	34772.577615	32.375770
657.402878	34835.948066	32.380788
658.749987	34882.632717	32.385805
659.284449	34937.018414	32.390823
659.637935	34992.222747	32.395840
660.388061	35054.269761	32.400858
661.191193	35108.746850	32.405876
661.895069	35166.375560	32.410893
662.666964	35217.715443	32.415911
663.518405	35270.168502	32.420928
664.186428	35317.168479	32.425946
664.872162	35378.290711	32.430964
665.997200	35421.862423	32.435981
667.019343	35463.211997	32.440999
667.748241	35501.079215	32.446016
668.641776	35530.511616	32.451034
669.695178	35571.135743	32.456052
670.218598	35612.070071	32.461069
671.119373	35642.272879	32.466087
671.530687	35682.453416	32.471104
671.968218	35714.378689	32.476122
672.343384	35749.437189	32.481140
673.114545	35785.173871	32.486157
673.942332	35824.335098	32.491175
674.541370	35878.340116	32.496192
675.066699	35913.337573	32.501210
675.743848	35959.970832	32.506228
676.021255	35997.966128	32.511245
676.556483	36035.263776	32.516263
677.143380	36088.474535	32.521280
677.883066	36129.293997	32.526298
678.450252	36180.326645	32.531316
679.032071	36219.684966	32.536333
679.668410	36269.037803	32.541351
680.374756	36312.429932	32.546368
680.956799	36356.714073	32.551386
681.378343	36400.713465	32.556404
682.027843	36440.061658	32.561421
682.794853	36498.765400	32.566439
683.579462	36548.658555	32.571456
683.822912	36597.327195	32.576474
684.733390	36652.866466	32.581492
684.903664	36708.691833	32.586509
685.887440	36769.069813	32.591527
686.352967	36824.002222	32.596544
687.167840	36872.595184	32.601562
687.617541	36936.452306	32.606580
688.593561	36996.926986	32.611597
689.019331	37054.389128	32.616615
689.727821	37122.088964	32.621632
690.444977	37187.264694	32.626650
691.108555	37248.711919	32.631668
691.849819	37321.446921	32.636685
692.726061	37367.464205	32.641703
693.698217	37437.438321	32.646720
694.381943	37476.416348	32.651738
695.094801	37541.644414	32.656756
695.786836	37600.691673	32.661773
696.463294	37655.719852	32.666791
697.293050	37712.387362	32.671808
698.354109	37764.617921	32.676826
699.260836	37823.727226	32.681844
699.706778	37881.005068	32.686861
700.332937	37933.702117	32.691879
700.679751	37993.619926	32.696896
701.859389	38054.116488	32.701914
702.539093	38109.992677	32.706932
703.056813	38163.156140	32.711949
704.210196	38216.562253	32.716967
704.511330	38272.187942	32.721984
705.231426	38325.807218	32.727002
705.869088	38374.842211	32.732020
705.996004	38444.710897	32.737037
706.973424	38512.019138	32.742055
707.470418	38574.912588	32.747072
708.794492	38633.206640	32.752090
709.690413	38687.646819	32.757108
710.380524	38737.566114	32.762125
711.372049	38778.642326	32.767143
711.999898	38843.697870	32.772160
712.693560	38900.048218	32.777178
713.687935	38947.890715	32.782196
714.141890	39007.876877	32.787213
714.931339	39052.001508	32.792231
715.337224	39106.025773	32.797248
716.002905	39167.952448	32.802266
716.998967	39239.484373	32.807284
717.604878	39284.744724	32.812301
718.366699	39331.384798	32.817319
718.715510	39403.252006	32.822336
719.640161	39456.317370	32.827354
720.441265	39512.576705	32.832372
720.695408	39574.499045	32.837389
721.643088	39629.578586	32.842407
722.149090	39699.208922	32.847424
723.253535	39755.048553	32.852442
724.141552	39806.558453	32.857460
725.016127	39862.434145	32.862477
725.727211	39913.642994	32.867495
726.157723	39978.315285	32.872512
726.937152	40027.565955	32.877530
727.866116	40062.646484	32.882548
728.262652	40122.556137	32.887565
728.580817	40173.162734	32.892583
729.036403	40228.674553	32.897600
730.058911	40285.641353	32.902618
730.656933	40338.184227	32.907636
730.868451	40409.443724	32.912653
731.713577	40448.123740	32.917671
732.329409	40522.122285	32.922688
733.620576	40592.948698	32.927706
734.011668	40653.044063	32.932724
734.736568	40704.366462	32.937741
736.051155	40770.003908	32.942759
736.889515	40840.926915	32.947776
737.710158	40895.371717	32.952794
738.456522	40949.493030	32.957812
739.131754	41004.713338	32.962829
739.951776	41051.411294	32.967847
740.422789	41122.038234	32.972864
741.298080	41177.923521	32.977882
742.191824	41239.820604	32.982900
742.728631	41299.876094	32.987917
743.704259	41350.345132	32.992935
744.571617	41420.411707	32.997952
745.154020	41490.984553	33.002970
746.030358	41538.813195	33.007988
746.518030	41597.182182	33.013005
747.593663	41650.216753	33.018023
748.250327	41708.313072	33.023040
748.932324	41770.674691	33.028058
749.356782	41836.624675	33.033076
750.274796	41907.987792	33.038093
750.794335	41961.862313	33.043111
751.867650	42027.307088	33.048128
752.916637	42091.642704	33.053146
753.843018	42146.308177	33.058164
754.548417	42208.680048	33.063181
755.594778	42269.715101	33.068199
755.928971	42324.840037	33.073216
756.754057	42385.587296	33.078234
757.676885	42444.820537	33.083252
758.177452	42501.064799	33.088269
759.209092	42555.107725	33.093287
760.108911	42617.899554	33.098304
761.024899	42677.545601	33.103322
761.770509	42728.211742	33.108340
762.131835	42775.010078	33.113357
762.993554	42829.921338	33.118375
763.700515	42891.384120	33.123392
764.532846	42946.724014	33.128410
765.750541	43016.241481	33.133428
766.015013	43065.794208	33.138445
766.997388	43131.338653	33.143463
767.587230	43180.739789	33.148480
768.297275	43243.796968	33.153498
769.090111	43294.482359	33.158516
770.010222	43351.548984	33.163533
771.084200	43409.452011	33.168551
771.511129	43466.273127	33.173568
772.495780	43522.172659	33.178586
773.248107	43574.515845	33.183604
773.824763	43640.460188	33.188621
774.305366	43689.942719	33.193639
775.071333	43751.930021	33.198656
775.840867	43812.797388	33.203674
777.061997	43869.584461	33.208692
777.567844	43934.686803	33.213709
778.439642	43971.300548	33.218727
779.103039	44031.173004	33.223744
780.023533	44081.992134	33.228762
780.510129	44122.094371	33.233780
781.212956	44172.220187	33.238797
782.467367	44227.320477	33.243815
783.030214	44288.752649	33.248832
783.408292	44349.340859	33.253850
784.334888	44400.874531	33.258868
784.850000	44453.497082	33.263885
785.962075	44512.630506	33.268903
786.771023	44563.860277	33.273920
787.371090	44621.694762	33.278938
788.311003	44675.390281	33.283956
789.021984	44732.442414	33.288973
789.935560	44798.053104	33.293991
790.518439	44856.377934	33.299008
791.148357	44908.186681	33.304026
792.331240	44979.860067	33.309044
792.642150	45037.911433	33.314061
793.468653	45103.017883	33.319079
794.363345	45163.521563	33.324096
795.309888	45232.784567	33.329114
796.246922	45299.613916	33.334132
797.164998	45357.154107	33.339149
797.849616	45432.233776	33.344167
798.728486	45482.790585	33.349184
799.354159	45550.440880	33.354202
800.123436	45613.312119	33.359220
800.864924	45683.266309	33.364237
801.567631	45747.520963	33.369255
802.513453	45813.148594	33.374272
803.218374	45884.146523	33.379290
804.057668	45947.374694	33.384308
804.654642	46023.956545	33.389325
805.585906	46098.987402	33.394343
806.250170	46171.485460	33.399360
806.770976	46241.602260	33.404378
807.932669	46311.644819	33.409396
808.537551	46395.185160	33.414413
809.654190	46460.066942	33.419431
810.079609	46532.109922	33.424448
810.809928	46605.168430	33.429466
811.885964	46675.307693	33.434484
813.174239	46743.788358	33.439501
814.622260	46813.446306	33.444519
815.236109	46871.803190	33.449536
816.100787	46952.622923	33.454554
817.201124	47001.263517	33.459572
817.884919	47060.539933	33.464589
818.469694	47124.696686	33.469607
819.301739	47186.676904	33.474624
819.966978	47255.180195	33.479642
820.891489	47306.524773	33.484660
821.615515	47372.937968	33.489677
822.291031	47440.649451	33.494695
823.465742	47514.040276	33.499712
824.243502	47573.885422	33.504730
824.983327	47637.057908	33.509748
826.123040	47702.350880	33.514765
826.494609	47770.990015	33.519783
827.388914	47830.868310	33.524800
828.125705	47897.559414	33.529818
828.703748	47962.795065	33.534836
829.571319	48024.221656	33.539853
830.357081	48092.152000	33.544871
831.585228	48160.943662	33.549888
832.479567	48226.814085	33.554906
833.332921	48278.070722	33.559924
833.909938	48343.674559	33.564941
834.776551	48395.043271	33.569959
835.516498	48451.189320	33.574976
836.290633	48507.652836	33.579994
837.321338	48571.295088	33.585012
837.769915	48632.358345	33.590029
838.716411	48699.582220	33.595047
839.833792	48752.608217	33.600064
840.353314	48822.910359	33.605082
840.957107	48883.519921	33.610100
841.700586	48947.245895	33.615117
842.068223	49017.376155	33.620135
843.363632	49089.177955	33.625152
844.191280	49171.770166	33.630170
845.157759	49233.867907	33.635188
846.315641	49302.566406	33.640205
847.048471	49366.598890	33.645223
848.206978	49439.220270	33.650240
848.781490	49504.777223	33.655258
849.604857	49576.660363	33.660276
850.660062	49645.546700	33.665293
851.109652	49715.811859	33.670311
851.971562	49790.486124	33.675328
852.824308	49867.180327	33.680346
854.072330	49938.163353	33.685364
855.133173	50000.545850	33.690381
855.695286	50080.639262	33.695399
856.763635	50139.193184	33.700416
857.559857	50216.061851	33.705434
858.528842	50284.020812	33.710452
859.298151	50356.338718	33.715469
860.335030	50427.210604	33.720487
861.263679	50488.710243	33.725504
861.862494	50563.706366	33.730522
862.523845	50632.138155	33.735540
864.021973	50706.678401	33.740557
864.928282	50772.535313	33.745575
866.331333	50831.171767	33.750592
866.611109	50897.221471	33.755610
867.777779	50950.327141	33.760628
868.380041	51024.912963	33.765645
869.228843	51106.211768	33.770663
870.360420	51160.835586	33.775680
871.224810	51236.311387	33.780698
872.043906	51299.760050	33.785716
872.722113	51367.185362	33.790733
873.408011	51430.825956	33.795751
874.490231	51499.625058	33.800768
875.053746	51577.894860	33.805786
875.764646	51643.506272	33.810804
876.603037	51710.913978	33.815821
877.552735	51797.894135	33.820839
878.441252	51871.128355	33.825856
879.103348	51943.341371	33.830874
879.994076	52010.450739	33.835892
881.237323	52092.634396	33.840909
881.691709	52179.655120	33.845927
882.647682	52244.261976	33.850944
883.732688	52329.495652	33.855962
884.480770	52407.979967	33.860980
885.291542	52476.172482	33.865997
886.417009	52550.080646	33.871015
887.960277	52602.568329	33.876032
888.849948	52678.747252	33.881050
889.315354	52754.074956	33.886068
890.470467	52822.847650	33.891085
891.099074	52889.981375	33.896103
891.939052	52961.227035	33.901120
892.421339	53019.556765	33.906138
893.493192	53082.686206	33.911156
894.195021	53149.404303	33.916173
894.955826	53224.858392	33.921191
896.472262	53280.477702	33.926208
897.359829	53353.216836	33.931226
897.946007	53424.952691	33.936244
898.871920	53488.865286	33.941261
899.299157	53562.853706	33.946279
900.769923	53624.853107	33.951296
901.376556	53690.056216	33.956314
902.444274	53770.577233	33.961332
903.552529	53842.182474	33.966349
904.068940	53919.075317	33.971367
905.338543	53978.499848	33.976384
905.833852	54053.801767	33.981402
906.939089	54119.029702	33.986420
907.939784	54201.815404	33.991437
908.544412	54267.640576	33.996455
909.791297	54339.921842	34.001472
910.780569	54416.382004	34.006490
911.558700	54493.824498	34.011508
912.732031	54562.510872	34.016525
913.366751	54648.924182	34.021543
914.465196	54715.800151	34.026560
915.325673	54786.630503	34.031578
916.513067	54859.447864	34.036596
917.579458	54919.602510	34.041613
918.365146	55001.747371	34.046631
919.590267	55069.155181	34.051648
920.339182	55137.675149	34.056666
921.111028	55213.595866	34.061684
922.275120	55272.103498	34.066701
922.735186	55357.426473	34.071719
924.067583	55422.939074	34.076736
925.108320	55496.692513	34.081754
925.633175	55570.564455	34.086772
926.745275	55653.223994	34.091789
927.788344	55731.793733	34.096807
928.612055	55795.532314	34.101824
929.206310	55874.938134	34.106842
930.323981	55956.806803	34.111860
931.393899	56033.689979	34.116877
932.282229	56106.095746	34.121895
933.017140	56184.259295	34.126912
933.897478	56261.925819	34.131930
934.771435	56346.352543	34.136948
935.605996	56424.533012	34.141965
936.777492	56514.369297	34.146983
937.882387	56590.097011	34.152000
938.407819	56659.023218	34.157018
939.317894	56747.711281	34.162036
940.408713	56820.264901	34.167053
941.169315	56915.837205	34.172071
942.585114	56994.353091	34.177088
943.684445	57060.229252	34.182106
944.349114	57141.944670	34.187124
945.574524	57219.851722	34.192141
945.961937	57299.832432	34.197159
947.393640	57376.252243	34.202176
948.365217	57448.554190	34.207194
948.988212	57532.036859	34.212212
950.220623	57610.608629	34.217229
951.053122	57686.610059	34.222247
951.977884	57760.654369	34.227264
953.118351	57830.709705	34.232282
953.859549	57910.213334	34.237300
954.622199	57984.188632	34.242317
955.548668	58054.853875	34.247335
956.520404	58130.360354	34.252352
957.436912	58206.363007	34.257370
958.380658	58276.437605	34.262388
959.670546	58341.559775	34.267405
959.873709	58423.674174	34.272423
961.245639	58493.556169	34.277440
962.168014	58554.862667	34.282458
963.008615	58644.410333	34.287476
964.131034	58711.173519	34.292493
964.717586	58800.634723	34.297511
965.754848	58879.646086	34.302528
966.804757	58962.155838	34.307546
967.771674	59039.684959	34.312564
968.805472	59124.799124	34.317581
969.796689	59209.167023	34.322599
970.589515	59296.382672	34.327616
971.381602	59375.205957	34.332634
972.126358	59464.923481	34.337652
973.527397	59546.361528	34.342669
974.603621	59639.053576	34.347687
974.898855	59728.240745	34.352704
976.439367	59815.607713	34.357722
977.086927	59911.158842	34.362740
978.076854	60005.498741	34.367757
979.484146	60092.134221	34.372775
980.544294	60189.122330	34.377792
981.275277	60272.091272	34.382810
981.935863	60368.692886	34.387828
983.321856	60461.036019	34.392845
984.606421	60550.464635	34.397863
985.588406	60638.858292	34.402880
987.417836	60713.967127	34.407898
988.121895	60811.741059	34.412916
989.395271	60886.234373	34.417933
990.078237	60979.809274	34.422951
990.958472	61067.251855	34.427968
992.061438	61142.323171	34.432986
992.704576	61239.525943	34.438004
993.585921	61320.905223	34.443021
994.803786	61413.689566	34.448039
995.849683	61495.531215	34.453056
996.919101	61580.610423	34.458074
997.315559	61670.656116	34.463092
998.332598	61749.660933	34.468109
999.488727	61842.665395	34.473127
1000.667386	61934.881773	34.478144
1001.915514	62021.371612	34.483162
1002.558669	62112.595895	34.488180
1004.055765	62197.876528	34.493197
1005.135889	62281.405607	34.498215
1006.196736	62371.704929	34.503232
1007.534033	62445.357435	34.508250
1008.382224	62539.045476	34.513268
1009.156785	62615.862573	34.518285
1010.302376	62701.718740	34.523303
1011.466111	62784.388249	34.528320
1012.804343	62849.369326	34.533338
1013.592676	62937.782391	34.538356
1014.624828	63014.237781	34.543373
1015.670419	63093.046210	34.548391
1016.677656	63174.665218	34.553408
1018.102895	63244.463871	34.558426
1018.631921	63332.019787	34.563444
1019.863919	63403.741765	34.568461
1020.639671	63483.859524	34.573479
1021.593323	63558.828490	34.578496
1022.737731	63622.708608	34.583514
1023.524064	63703.604079	34.588532
1024.612036	63776.818231	34.593549
1025.225490	63848.966962	34.598567
1025.682356	63919.741218	34.603584
1026.976705	63997.918718	34.608602
1027.863487	64088.086780	34.613620
1028.949808	64165.942673	34.618637
1030.049026	64250.247739	34.623655
1030.721736	64337.139089	34.628672
1031.793729	64426.925025	34.633690
1033.082420	64516.930782	34.638708
1033.814845	64603.452909	34.643725
1035.083234	64696.703813	34.648743
1035.836218	64789.826376	34.653760
1036.621742	64881.044973	34.658778
1037.465454	64973.647629	34.663796
1038.758628	65070.238747	34.668813
1039.762075	65165.704120	34.673831
1040.289944	65266.017390	34.678848
1041.888272	65360.447598	34.683866
1042.818495	65469.169840	34.688884
1044.047432	65570.109585	34.693901
1045.058134	65666.164507	34.698919
1046.330160	65763.470650	34.703936
1047.619193	65860.299690	34.708954
1048.681728	65961.032651	34.713972
1050.194594	66046.881121	34.718989
1051.543245	66137.991287	34.724007
1052.328162	66217.236318	34.729024
1053.603091	66305.826104	34.734042
1054.713864	66393.099540	34.739060
1055.814962	66480.824298	34.744077
1057.200910	66570.056175	34.749095
1058.116018	66660.596251	34.754112
1059.338348	66740.996765	34.759130
1060.221528	66826.217795	34.764148
1061.375631	66914.587926	34.769165
1062.759296	66977.521285	34.774183
1063.245503	67067.597740	34.779200
1064.245569	67150.750302	34.784218
1065.264401	67260.422475	34.789236
1066.505632	67349.103455	34.794253
1067.788487	67427.622615	34.799271
1068.784531	67518.007519	34.804288
1070.035087	67603.129643	34.809306
1070.767492	67697.722344	34.814324
1072.017607	67789.341295	34.819341
1072.752900	67871.296437	34.824359
1073.767634	67966.909889	34.829376
1074.985642	68050.139092	34.834394
1075.939285	68155.342477	34.839412
1076.698293	68237.611680	34.844429
1077.766477	68334.256573	34.849447
1078.682074	68439.498703	34.854464
1079.879611	68527.627047	34.859482
1081.249014	68633.109587	34.864500
1082.137387	68731.366899	34.869517
1083.602577	68819.828159	34.874535
1084.409107	68915.870124	34.879552
1085.131183	69005.017554	34.884570
1086.251735	69112.225061	34.889588
1087.645284	69209.056874	34.894605
1088.514946	69297.941731	34.899623
1089.324798	69407.585957	34.904640
1091.436709	69506.504251	34.909658
1092.439158	69601.099909	34.914676
1093.115369	69686.609606	34.919693
1094.710713	69765.549510	34.924711
1095.631815	69860.810977	34.929728
1096.616611	69929.284561	34.934746
1096.994031	70014.873510	34.939764
1098.029669	70098.175708	34.944781
1099.831036	70177.414068	34.949799
1100.495403	70274.198733	34.954816
1101.465078	70363.078009	34.959834
1102.470507	70460.848755	34.964852
1103.190568	70558.037399	34.969869
1104.507155	70652.993254	34.974887
1105.662415	70751.204022	34.979904
1106.670708	70842.434526	34.984922
1107.886063	70943.004938	34.989940
1109.108787	71050.350191	34.994957
1110.234427	71142.943929	34.999975
1111.181738	71254.727550	35.004992
1111.934985	71356.118703	35.010010
1113.301860	71451.221612	35.015028
1114.522361	71551.476942	35.020045
1115.682052	71664.597065	35.025063
1116.731914	71770.389056	35.030080
1118.060170	71874.871633	35.035098
1119.587563	71981.793328	35.040116
1120.602719	72081.804014	35.045133
1121.521238	72183.349949	35.050151
1122.813056	72279.518756	35.055168
1124.343792	72388.430032	35.060186
1125.392516	72490.577485	35.065204
1126.029722	72589.420387	35.070221
1127.577318	72679.712085	35.075239
1128.734211	72786.124771	35.080256
1129.932989	72893.481283	35.085274
1131.530209	72994.228089	35.090292
1132.121177	73096.588459	35.095309
1133.810782	73189.747567	35.100327
1135.005012	73291.216849	35.105344
1136.081437	73366.891966	35.110362
1137.413545	73462.653504	35.115380
1138.396524	73566.157921	35.120397
1139.891632	73657.575725	35.125415
1140.783685	73749.467692	35.130432
1141.904521	73843.452255	35.135450
1143.127930	73943.424897	35.140468
1144.407536	74047.543652	35.145485
1145.757921	74136.110421	35.150503
1146.615377	74230.175343	35.155520
1147.917130	74324.450098	35.160538
1149.022227	74412.156661	35.165556
1149.963338	74507.070845	35.170573
1151.312010	74596.564052	35.175591
1152.811054	74690.632061	35.180608
1153.665973	74778.657429	35.185626
1154.981923	74868.283303	35.190644
1155.668967	74969.141263	35.195661
1157.533211	75056.161778	35.200679
1158.546230	75147.102396	35.205696
1159.155048	75232.000902	35.210714
1160.458033	75331.295014	35.215732
1160.919763	75436.458484	35.220749
1162.442004	75522.989077	35.225767
1163.677429	75629.299552	35.230784
1164.502406	75733.014284	35.235802
1165.931057	75832.189349	35.240820
1166.960895	75937.747691	35.245837
1168.049650	76036.001052	35.250855
1169.044221	76141.591014	35.255872
1170.078600	76243.691726	35.260890
1171.278305	76337.254736	35.265908
1172.252411	76419.300670	35.270925
1173.593902	76518.314480	35.275943
1174.337097	76623.983453	35.280960
1175.446608	76715.218353	35.285978
1176.815501	76821.829428	35.290996
1177.961706	76919.266338	35.296013
1179.238531	77011.362913	35.301031
1180.254206	77112.279062	35.306048
1181.552434	77208.907959	35.311066
1182.774313	77309.020017	35.316084
1184.026221	77404.567401	35.321101
1185.407455	77508.987740	35.326119
1186.460518	77610.887999	35.331136
1187.694399	77714.153955	35.336154
1188.926192	77812.581498	35.341172
1189.806535	77927.507066	35.346189
1191.409884	78034.643783	35.351207
1192.474871	78147.172621	35.356224
1193.565580	78246.979166	35.361242
1195.056939	78350.638162	35.366260
1196.209409	78472.326441	35.371277
1197.330446	78578.615581	35.376295
1199.336301	78664.092784	35.381312
1201.244529	78745.721616	35.386330
1202.504851	78840.601284	35.391348
1203.482918	78931.826043	35.396365
1204.560995	79020.033118	35.401383
1205.744165	79113.988273	35.406400
1206.654314	79216.347469	35.411418
1207.883438	79314.337412	35.416436
1209.035042	79419.421525	35.421453
1209.905277	79503.570535	35.426471
1211.288756	79611.621757	35.431488
1212.114787	79735.165379	35.436506
1213.664036	79827.431709	35.441524
1214.562950	79946.746218	35.446541
1215.921927	80050.533562	35.451559
1217.182387	80176.304599	35.456576
1217.985700	80282.535728	35.461594
1219.353735	80377.720629	35.466612
1220.369216	80500.110618	35.471629
1221.582188	80608.648350	35.476647
1222.684684	80726.946322	35.481664
1224.070085	80843.819811	35.486682
1225.314864	80961.488506	35.491700
1226.838478	81088.895052	35.496717
1227.947706	81204.115339	35.501735
1229.201104	81320.086498	35.506752
1230.028772	81438.366910	35.511770
1231.162758	81541.536008	35.516788
1232.322198	81670.382867	35.521805
1233.764066	81793.193591	35.526823
1235.010314	81910.637989	35.531840
1236.058801	82026.986046	35.536858
1237.607313	82147.361786	35.541876
1238.989410	82265.039914	35.546893
1240.198459	82379.945408	35.551911
1241.748165	82505.314454	35.556928
1242.532151	82631.487427	35.561946
1244.509522	82746.920997	35.566964
1245.497454	82843.807878	35.571981
1246.896413	82962.727964	35.576999
1247.976430	83079.392204	35.582016
1249.061051	83190.734673	35.587034
1250.689524	83301.118672	35.592052
1251.346679	83417.736088	35.597069
1252.912823	83517.297421	35.602087
1254.670587	83614.396541	35.607104
1255.611284	83715.943827	35.612122
1256.784900	83807.280734	35.617140
1257.787543	83914.888302	35.622157
1259.253406	84011.185277	35.627175
1260.316995	84111.371751	35.632192
1261.347919	84224.411827	35.637210
1262.516771	84328.789377	35.642228
1263.879625	84441.867343	35.647245
1265.037037	84550.226136	35.652263
1266.067964	84668.906527	35.657280
1267.020596	84788.005068	35.662298
1268.663020	84900.483801	35.667316
1269.855671	85025.767468	35.672333
1270.728232	85141.978250	35.677351
1271.947875	85270.958768	35.682368
1273.451106	85405.471093	35.687386
1274.955725	85514.425714	35.692404
1276.425077	85643.597116	35.697421
1277.278103	85766.237854	35.702439
1278.973009	85893.981408	35.707456
1279.979356	86014.217089	35.712474
1281.205783	86137.067381	35.717492
1283.037447	86264.170372	35.722509
1284.165729	86386.707535	35.727527
1285.580666	86512.115106	35.732544
1287.227580	86641.757520	35.737562
1288.811018	86754.658153	35.742580
1290.087558	86871.636668	35.747597
1291.107120	86981.052460	35.752615
1292.450395	87103.153672	35.757632
1293.399904	87236.087964	35.762650
1294.932106	87346.996674	35.767668
1296.369490	87469.845099	35.772685
1297.420258	87595.237977	35.777703
1298.881223	87717.006627	35.782720
1299.854087	87848.913608	35.787738
1301.240923	87978.691143	35.792756
1302.615567	88107.482696	35.797773
1303.960323	88226.356878	35.802791
1305.398646	88362.096850	35.807808
1306.794651	88488.681717	35.812826
1308.218109	88603.844763	35.817844
1309.842463	88723.488483	35.822861
1311.259714	88853.265138	35.827879
1312.810773	88954.723079	35.832896
1314.278698	89076.584978	35.837914
1315.622237	89186.871002	35.842932
1316.842668	89303.677838	35.847949
1317.632782	89417.814737	35.852967
1319.026558	89535.698059	35.857984
1320.470815	89654.207648	35.863002
1321.525114	89781.421519	35.868020
1322.886168	89900.680085	35.873037
1324.123536	90032.340186	35.878055
1325.801450	90146.709219	35.883072
1326.963600	90272.184822	35.888090
1328.390609	90404.653491	35.893108
1329.784816	90513.656525	35.898125
1331.031168	90633.037258	35.903143
1332.700442	90752.758193	35.908160
1334.176285	90873.295481	35.913178
1335.444387	90987.541411	35.918196
1336.812853	91102.507232	35.923213
1338.039313	91218.294045	35.928231
1339.229183	91328.079597	35.933248
1340.428936	91448.674839	35.938266
1341.865551	91551.807030	35.943284
1343.196722	91663.548945	35.948301
1344.435521	91770.666956	35.953319
1345.928670	91874.425152	35.958336
1347.018721	91985.090468	35.963354
1348.200961	92084.854736	35.968372
1349.370542	92204.355038	35.973389
1350.397689	92311.736044	35.978407
1351.826287	92427.610097	35.983424
1352.775096	92543.622643	35.988442
1354.472026	92663.080693	35.993460
1355.847283	92784.541145	35.998477
1356.605430	92914.311211	36.003495
1357.962710	93026.561064	36.008512
1360.069378	93155.273066	36.013530
1361.773346	93279.295295	36.018548
1363.139027	93400.645619	36.023565
1363.971195	93525.349553	36.028583
1365.637385	93645.792192	36.033600
1366.711173	93772.424118	36.038618
1367.805487	93897.621106	36.043636
1369.131118	94025.976691	36.048653
1370.625230	94164.788828	36.053671
1371.987322	94296.029769	36.058688
1373.282212	94436.420498	36.063706
1374.900376	94571.285868	36.068724
1376.210125	94702.663438	36.073741
1377.227293	94844.075241	36.078759
1379.330718	94964.201479	36.083776
1381.030551	95089.524538	36.088794
1382.292109	95219.644265	36.093812
1383.988719	95345.868819	36.098829
1385.224808	95482.622901	36.103847
1386.702961	95601.517998	36.108864
1388.029287	95740.375995	36.113882
1389.204219	95875.937135	36.118900
1390.612838	96003.083807	36.123917
1391.706523	96139.292525	36.128935
1393.243000	96277.689225	36.133952
1394.649967	96412.075746	36.138970
1395.910712	96548.741930	36.143988
1397.803990	96693.904618	36.149005
1399.039252	96827.761901	36.154023
1400.560432	96968.027417	36.159040
1401.604282	97106.288953	36.164058
1402.862774	97244.112047	36.169076
1404.429985	97389.252639	36.174093
1405.556786	97535.603322	36.179111
1407.178623	97669.277246	36.184128
1408.650977	97830.685832	36.189146
1410.082802	97967.686483	36.194164
1411.595585	98104.687802	36.199181
1413.152667	98249.567708	36.204199
1415.060262	98381.083153	36.209216
1416.226120	98519.636113	36.214234
1417.407680	98663.828424	36.219252
1419.075091	98786.648589	36.224269
1420.609892	98928.847554	36.229287
1421.968878	99050.664554	36.234304
1423.573589	99197.341487	36.239322
1424.689647	99333.547799	36.244340
1426.570714	99466.250817	36.249357
1427.722696	99605.140247	36.254375
1429.033391	99742.687139	36.259392
1430.712922	99879.796892	36.264410
1431.949409	100014.225198	36.269428
1433.325641	100143.054247	36.274445
1434.551063	100288.020355	36.279463
1435.946549	100417.139084	36.284480
1437.057440	100543.589622	36.289498
1438.568031	100675.505889	36.294516
1439.971511	100793.861570	36.299533
1441.276929	100937.829279	36.304551
1442.794529	101053.214233	36.309568
1444.450558	101183.309684	36.314586
1445.665866	101315.490035	36.319604
1446.939546	101448.942308	36.324621
1448.111344	101584.629632	36.329639
1449.659932	101724.708866	36.334656
1451.305562	101857.635830	36.339674
1453.203547	101986.745972	36.344692
1454.719574	102115.801969	36.349709
1456.302109	102252.695955	36.354727
1457.885812	102384.696508	36.359744
1459.489101	102514.158875	36.364762
1460.539514	102649.438439	36.369780
1461.795525	102781.390162	36.374797
1463.314589	102929.060845	36.379815
1465.004296	103072.699205	36.384832
1466.343344	103211.346681	36.389850
1467.570494	103349.416257	36.394868
1469.274283	103490.379041	36.399885
1471.480559	103625.634842	36.404903
1473.062649	103761.977295	36.409920
1474.854507	103896.601368	36.414938
1475.937086	104023.285267	36.419956
1477.348771	104152.492254	36.424973
1478.638164	104293.282044	36.429991
1480.295731	104436.005739	36.435008
1481.733347	104573.286893	36.440026
1483.204469	104716.370462	36.445044
1484.789727	104853.896050	36.450061
1485.980556	104994.640737	36.455079
1487.520055	105131.553301	36.460096
1488.926004	105272.405142	36.465114
1490.321708	105426.876896	36.470132
1492.041408	105567.871331	36.475149
1493.454336	105719.818525	36.480167
1494.928729	105860.421258	36.485184
1496.547220	106004.045269	36.490202
1497.920556	106149.521246	36.495220
1499.861027	106291.942509	36.500237
1501.128365	106437.093864	36.505255
1502.698465	106587.143870	36.510272
1503.892946	106731.153951	36.515290
1505.488343	106874.595040	36.520308
1506.836503	107019.723620	36.525325
1508.564032	107185.424298	36.530343
1509.966832	107332.029272	36.535360
1511.475859	107480.735936	36.540378
1513.021572	107638.808258	36.545396
1514.745688	107780.432512	36.550413
1516.074538	107940.619550	36.555431
1517.679619	108077.394287	36.560448
1519.084753	108225.499004	36.565466
1520.457427	108386.416761	36.570484
1522.387654	108537.725352	36.575501
1523.773558	108693.341986	36.580519
1524.880078	108837.336544	36.585536
1526.758852	108995.997281	36.590554
1528.061210	109159.364281	36.595572
1529.266193	109293.467038	36.600589
1530.773211	109460.290839	36.605607
1532.376670	109619.948343	36.610624
1534.087483	109772.589925	36.615642
1535.403301	109931.976598	36.620660
1537.295828	110084.020607	36.625677
1538.405442	110233.194363	36.630695
1539.913386	110365.998639	36.635712
1541.717731	110504.489240	36.640730
1542.551192	110653.225869	36.645748
1544.244785	110801.283950	36.650765
1546.225816	110954.877766	36.655783
1547.231654	111098.859252	36.660800
1548.882509	111243.717413	36.665818
1549.980889	111399.124507	36.670836
1551.809785	111548.597683	36.675853
1553.273154	111712.598257	36.680871
1555.153511	111865.209831	36.685888
1556.421667	112021.544357	36.690906
1557.970260	112190.112018	36.695924
1559.584838	112352.557489	36.700941
1561.147647	112516.444826	36.705959
1562.780548	112679.789356	36.710976
1564.489742	112835.361279	36.715994
1565.878258	113007.064825	36.721012
1567.420452	113169.195524	36.726029
1568.832675	113334.467033	36.731047
1570.455568	113503.739508	36.736064
1572.521841	113664.941146	36.741082
1574.299843	113832.605714	36.746100
1576.098911	113994.801598	36.751117
1577.703122	114151.575011	36.756135
1579.306119	114322.870945	36.761152
1581.157417	114475.942008	36.766170
1582.778980	114629.556783	36.771188
1584.544556	114787.791705	36.776205
1586.332204	114947.165338	36.781223
1587.794376	115117.548385	36.786240
1589.602668	115268.016774	36.791258
1590.949890	115435.197707	36.796276
1592.307601	115595.643034	36.801293
1593.850366	115765.686782	36.806311
1595.328657	115936.705274	36.811328
1597.315029	116088.011757	36.816346
1598.767360	116251.527246	36.821364
1600.362151	116408.134202	36.826381
1602.029635	116577.984705	36.831399
1603.397046	116739.448159	36.836416
1605.015846	116904.145545	36.841434
1606.904812	117085.823022	36.846452
1608.145988	117250.276303	36.851469
1610.640000	117403.754144	36.856487
1611.865276	117569.885556	36.861504
1613.729726	117729.614354	36.866522
1614.854053	117900.709639	36.871540
1616.886949	118058.511034	36.876557
1618.535298	118211.755966	36.881575
1620.408887	118384.804325	36.886592
1621.791536	118541.922536	36.891610
1623.442743	118711.950134	36.896628
1624.590395	118872.721280	36.901645
1626.346226	119044.332296	36.906663
1627.766887	119217.328107	36.911680
1629.555466	119380.830254	36.916698
1630.685571	119562.117706	36.921716
1632.050649	119726.511736	36.926733
1633.985819	119899.519351	36.931751
1635.525656	120089.041231	36.936768
1637.292250	120260.021800	36.941786
1638.701934	120440.052158	36.946804
1640.222678	120616.108414	36.951821
1642.000624	120789.905593	36.956839
1643.268284	120972.129647	36.961856
1645.020513	121142.241102	36.966874
1646.680052	121317.999880	36.971892
1648.243682	121486.442403	36.976909
1649.772342	121646.823351	36.981927
1651.226210	121816.273824	36.986944
1652.847049	121975.132238	36.991962
1654.508380	122152.619694	36.996980
1656.399025	122328.055291	37.001997
1657.439352	122501.264531	37.007015
1659.318879	122678.301786	37.012032
1661.142698	122849.957160	37.017050
1662.627204	123032.892830	37.022068
1664.988209	123195.129511	37.027085
1666.820425	123369.931876	37.032103
1668.397571	123544.444881	37.037120
1670.061936	123714.416248	37.042138
1671.524298	123902.116551	37.047156
1672.954039	124071.872243	37.052173
1674.601256	124255.955327	37.057191
1676.324387	124449.922546	37.062208
1678.239399	124625.783161	37.067226
1679.543835	124814.717503	37.072244
1681.217593	125010.077903	37.077261
1682.821513	125201.136788	37.082279
1684.317921	125403.732499	37.087296
1685.986403	125591.192948	37.092314
1687.356180	125794.863294	37.097332
1689.017126	126000.037099	37.102349
1690.525854	126199.653533	37.107367
1692.203281	126416.764945	37.112384
1694.302067	126616.063219	37.117402
1695.950260	126836.518013	37.122420
1697.821183	127043.605452	37.127437
1699.690744	127243.970086	37.132455
1701.184174	127463.576931	37.137472
1703.053519	127671.340179	37.142490
1704.771743	127863.573611	37.147508
1706.560769	128076.375480	37.152525
1708.317475	128283.131664	37.157543
1710.232996	128491.830685	37.162560
1712.366783	128695.700962	37.167578
1713.684331	128900.726951	37.172596
1715.683847	129098.948818	37.177613
1718.006513	129293.898694	37.182631
1719.604251	129493.212642	37.187648
1721.113055	129699.215076	37.192666
1722.986133	129901.203253	37.197684
1724.193845	130109.563708	37.202701
1726.363890	130305.062201	37.207719
1727.989356	130514.184330	37.212736
1729.593482	130716.421247	37.217754
1731.203594	130930.864058	37.222772
1733.202771	131133.587047	37.227789
1735.259601	131337.063309	37.232807
1736.627315	131547.321777	37.237824
1738.376679	131745.607598	37.242842
1740.081753	131944.091547	37.247860
1741.929870	132165.761181	37.252877
1743.861757	132354.923819	37.257895
1745.255896	132565.513017	37.262912
1747.013463	132778.178347	37.267930
1749.268327	132974.500508	37.272948
1751.108175	133173.210170	37.277965
1752.890435	133373.262011	37.282983
1754.242423	133583.317050	37.288000
1756.172633	133773.932605	37.293018
1757.400571	133972.043223	37.298036
1758.985613	134185.782703	37.303053
1761.080596	134393.315049	37.308071
1762.851505	134585.633841	37.313088
1764.395917	134779.790572	37.318106
1766.443229	134961.142625	37.323124
1768.111581	135147.312857	37.328141
1769.712619	135334.420657	37.333159
1771.117796	135534.972355	37.338176
1772.555408	135731.065918	37.343194
1774.205871	135930.692943	37.348212
1775.606481	136143.036559	37.353229
1777.262374	136361.622777	37.358247
1778.933938	136580.816710	37.363264
1780.496003	136789.547050	37.368282
1782.456203	137011.743658	37.373300
1783.918007	137244.614914	37.378317
1785.868808	137468.426806	37.383335
1788.006313	137685.561199	37.388352
1789.866598	137907.143190	37.393370
1792.046371	138128.270438	37.398388
1793.460110	138367.258761	37.403405
1795.194288	138588.356030	37.408423
1796.919764	138816.968330	37.413440
1798.656288	139056.303345	37.418458
1800.420093	139285.977957	37.423476
1802.555106	139511.014670	37.428493
1804.336554	139748.188842	37.433511
1806.025386	139982.954722	37.438528
1808.064807	140223.276458	37.443546
1810.095773	140449.488677	37.448564
1811.970092	140699.102718	37.453581
1813.883385	140927.327966	37.458599
1815.574471	141170.703722	37.463616
1816.974459	141407.793235	37.468634
1818.890137	141646.453485	37.473652
1820.699233	141890.347531	37.478669
1822.579552	142134.219029	37.483687
1824.359125	142391.065145	37.488704
1825.948117	142643.792230	37.493722
1827.882123	142893.014883	37.498740
1829.461646	143149.210783	37.503757
1831.259794	143400.538544	37.508775
1832.965047	143655.600660	37.513792
1834.571773	143919.182791	37.518810
1836.762303	144176.799221	37.523828
1838.271691	144453.027532	37.528845
1840.561697	144712.001950	37.533863
1842.245018	144973.128209	37.538880
1844.125449	145224.985424	37.543898
1846.026200	145496.652930	37.548916
1847.772026	145751.110189	37.553933
1849.686288	146018.272706	37.558951
1851.464700	146285.305460	37.563968
1853.493398	146556.273330	37.568986
1855.632977	146817.845748	37.574004
1857.195424	147081.920871	37.579021
1859.225796	147345.784900	37.584039
1860.991680	147615.618841	37.589056
1862.903352	147879.174049	37.594074
1864.738618	148142.805942	37.599092
1866.430450	148414.546741	37.604109
1868.697976	148675.588188	37.609127
1870.583036	148944.191918	37.614144
1872.594019	149201.810748	37.619162
1874.836679	149467.416723	37.624180
1876.287310	149746.995382	37.629197
1878.266121	150005.206982	37.634215
1880.237406	150261.682035	37.639232
1882.394132	150526.697366	37.644250
1884.226355	150783.425020	37.649268
1885.675395	151040.442007	37.654285
1887.967511	151279.964437	37.659303
1889.615342	151508.062546	37.664320
1891.663046	151748.767480	37.669338
1893.740015	151976.737282	37.674356
1895.424234	152215.901444	37.679373
1897.451031	152459.697284	37.684391
1898.921324	152708.518663	37.689408
1900.607539	152959.325859	37.694426
1902.238576	153208.721060	37.699444
1903.583184	153467.695058	37.704461
1905.525738	153729.941084	37.709479
1907.351748	153990.924372	37.714496
1909.052641	154258.719659	37.719514
1910.928737	154528.380365	37.724532
1912.629904	154812.096647	37.729549
1914.677325	155094.021332	37.734567
1916.690745	155375.356057	37.739584
1918.239847	155660.699673	37.744602
1920.189639	155941.158444	37.749620
1922.775081	156219.970909	37.754637
1924.126837	156510.719174	37.759655
1926.404801	156783.374534	37.764672
1929.006036	157069.627625	37.769690
1931.092421	157353.423281	37.774708
1933.271433	157630.312598	37.779725
1935.096671	157912.386983	37.784743
1937.250971	158182.668683	37.789760
1938.922973	158472.970467	37.794778
1941.388279	158743.460177	37.799796
1942.991867	159022.578223	37.804813
1944.607413	159304.145851	37.809831
1946.691049	159589.475877	37.814848
1948.736414	159887.927399	37.819866
1950.848739	160162.172642	37.824884
1952.480490	160461.986228	37.829901
1954.390744	160749.278287	37.834919
1956.728997	161031.198333	37.839936
1958.123152	161322.293123	37.844954
1960.745927	161606.507448	37.849972
1962.623313	161894.508107	37.854989
1964.577253	162187.906537	37.860007
1966.511922	162484.051604	37.865024
1968.178375	162783.401046	37.870042
1970.221515	163083.328047	37.875060
1971.938507	163380.983830	37.880077
1974.345350	163681.187079	37.885095
1976.120837	163978.950746	37.890112
1977.864678	164283.475034	37.895130
1979.775542	164588.215957	37.900148
1982.103372	164886.012010	37.905165
1984.206846	165191.677935	37.910183
1986.467129	165492.534315	37.915200
1987.737417	165795.615629	37.920218
1989.838705	166098.442002	37.925236
1991.900049	166403.040757	37.930253
1993.471997	166718.699592	37.935271
1995.874381	167018.016996	37.940288
1997.496501	167334.889718	37.945306
2000.138022	167656.137978	37.950324
2001.768318	167957.598372	37.955341
2003.429081	168273.732914	37.960359
2005.281791	168584.760218	37.965376
2007.441095	168889.430759	37.970394
2009.601474	169204.526709	37.975412
2011.430256	169526.824119	37.980429
2012.841729	169834.675054	37.985447
2015.123799	170157.018991	37.990464
2016.655539	170474.465703	37.995482
2019.021362	170765.449722	38.000500
2020.564948	171074.821677	38.005517
2022.390505	171375.719943	38.010535
2024.670643	171690.503201	38.015552
2026.581548	172001.332821	38.020570
2028.202822	172306.634555	38.025588
2030.318087	172635.567119	38.030605
2032.306259	172953.524675	38.035623
2034.282037	173285.084756	38.040640
2036.187749	173620.758549	38.045658
2038.203175	173947.401236	38.050676
2040.235975	174279.947104	38.055693
2041.914650	174627.063253	38.060711
2043.988389	174957.294562	38.065728
2046.045821	175297.726320	38.070746
2048.708408	175640.439882	38.075764
2050.484178	175987.051570	38.080781
2052.027827	176332.697692	38.085799
2054.432450	176675.722408	38.090816
2056.576483	177032.833459	38.095834
2058.631545	177373.109123	38.100852
2060.354757	177734.745793	38.105869
2062.859173	178097.862439	38.110887
2064.943826	178450.379177	38.115904
2066.949183	178798.668369	38.120922
2069.369220	179159.643871	38.125940
2071.342314	179525.465137	38.130957
2073.238522	179887.414071	38.135975
2075.428001	180232.277041	38.140992
2077.949689	180607.058944	38.146010
2079.937234	180970.090151	38.151028
2082.428377	181330.479244	38.156045
2084.475291	181688.068915	38.161063
2086.802068	182037.717604	38.166080
2088.652470	182409.512793	38.171098
2090.695872	182775.564798	38.176116
2093.076767	183132.930235	38.181133
2095.262597	183496.372214	38.186151
2097.320798	183850.260156	38.191168
2099.568967	184214.863472	38.196186
2101.732197	184570.515593	38.201204
2103.926113	184942.190913	38.206221
2105.898262	185291.220851	38.211239
2108.083531	185655.661463	38.216256
2109.996605	186094.844681	38.221274
2112.148051	186459.623620	38.226292
2114.439497	186814.095320	38.231309
2116.232231	187185.130073	38.236327
2119.087407	187544.418601	38.241344
2121.195613	187904.713580	38.246362
2123.608432	188259.958622	38.251380
2125.690989	188624.984342	38.256397
2127.478931	188975.579209	38.261415
2129.725292	189340.226212	38.266432
2131.320740	189706.829909	38.271450
2133.814792	190065.827318	38.276468
2135.953142	190431.002662	38.281485
2138.004696	190799.545508	38.286503
2140.246260	191151.575128	38.291520
2142.550735	191526.939000	38.296538
2144.198731	191886.784917	38.301556
2146.704948	192255.515555	38.306573
2148.398293	192623.713403	38.311591
2150.661515	192997.945243	38.316608
2152.901955	193366.796788	38.321626
2154.725055	193735.358754	38.326644
2156.649688	194104.464812	38.331661
2158.640100	194457.889260	38.336679
2161.310454	194806.052431	38.341696
2163.139086	195160.265993	38.346714
2165.165851	195511.147504	38.351732
2167.030382	195853.723558	38.356749
2168.933213	196223.042144	38.361767
2171.143978	196578.647831	38.366784
2173.077887	196946.845850	38.371802
2175.204146	197316.386580	38.376820
2177.175290	197691.032731	38.381837
2179.175533	198062.423908	38.386855
2181.308165	198449.620715	38.391872
2183.172934	198836.580798	38.396890
2185.528597	199227.377366	38.401908
2187.618226	199617.301866	38.406925
2189.402660	200025.437282	38.411943
2191.835599	200417.901353	38.416960
2194.026193	200822.190696	38.421978
2196.601398	201223.779357	38.426996
2198.719118	201617.438478	38.432013
2200.807708	202039.147222	38.437031
2203.414372	202430.318916	38.442048
2206.325827	202837.117364	38.447066
2208.230171	203244.886363	38.452084
2210.455192	203644.706182	38.457101
2212.522737	204055.601517	38.462119
2215.180186	204457.515017	38.467136
2217.732570	204867.295158	38.472154
2219.753968	205272.941940	38.477172
2221.976428	205685.950486	38.482189
2223.983012	206099.704753	38.487207
2226.590260	206495.990768	38.492224
2228.701429	206900.432879	38.497242
2230.960148	207320.704276	38.502260
2233.796853	207718.328599	38.507277
2235.628423	208128.684596	38.512295
2238.134931	208528.749620	38.517312
2240.153568	208955.081954	38.522330
2242.418309	209361.867048	38.527348
2244.623620	209772.548764	38.532365
2246.716103	210184.518872	38.537383
2249.081174	210604.855728	38.542400
2251.502417	211024.041350	38.547418
2253.474293	211445.609261	38.552436
2255.691263	211857.029070	38.557453
2257.820222	212297.931244	38.562471
2260.356375	212712.401802	38.567488
2262.918795	213132.356003	38.572506
2265.539833	213541.962358	38.577524
2268.307983	213954.518555	38.582541
2270.267565	214377.692807	38.587559
2272.955929	214778.271859	38.592576
2275.460672	215181.598126	38.597594
2277.705027	215587.226279	38.602612
2279.962419	215986.730504	38.607629
2282.316679	216395.822685	38.612647
2284.782600	216803.526071	38.617664
2286.387651	217212.557783	38.622682
2288.661952	217624.305530	38.627700
2290.760701	218025.639936	38.632717
2292.576876	218451.101550	38.637735
2294.585105	218873.104072	38.642752
2296.832593	219304.088074	38.647770
2299.061303	219733.754291	38.652788
2301.004366	220156.047275	38.657805
2302.956164	220593.352920	38.662823
2305.317841	221023.685132	38.667840
2307.873770	221462.218243	38.672858
2309.872484	221875.916909	38.677876
2312.694526	222290.605391	38.682893
2314.543233	222702.498629	38.687911
2316.723169	223103.848571	38.692928
2318.995874	223521.722242	38.697946
2321.266903	223939.977337	38.702964
2323.420447	224363.128386	38.707981
2325.617143	224791.734667	38.712999
2327.671904	225223.513195	38.718016
2329.802418	225662.164476	38.723034
2331.758389	226098.251714	38.728052
2334.488265	226546.539490	38.733069
2336.535557	226991.300677	38.738087
2338.621756	227460.392875	38.743104
2341.198287	227912.743602	38.748122
2343.629629	228358.765802	38.753140
2346.279227	228813.950192	38.758157
2348.757023	229290.500583	38.763175
2350.911163	229738.216748	38.768192
2353.353047	230199.326682	38.773210
2355.762716	230673.016400	38.778228
2358.044826	231134.506377	38.783245
2360.057143	231610.391327	38.788263
2362.558493	232082.186025	38.793280
2365.390684	232556.520104	38.798298
2367.358605	233044.782658	38.803316
2369.429742	233510.114398	38.808333
2371.928974	233997.226462	38.813351
2374.639075	234478.919620	38.818368
2377.505355	234958.149216	38.823386
2379.509279	235445.209863	38.828404
2382.313861	235929.859013	38.833421
2384.847175	236411.044084	38.838439
2387.029122	236898.354730	38.843456
2389.880205	237384.569860	38.848474
2391.771057	237887.750978	38.853492
2394.499898	238365.448134	38.858509
2397.506017	238847.343840	38.863527
2399.360849	239333.152298	38.868544
2401.743146	239824.746102	38.873562
2403.900748	240321.784985	38.878580
2406.246403	240808.022686	38.883597
2408.323966	241315.081195	38.888615
2411.002140	241813.687575	38.893632
2413.960315	242306.330452	38.898650
2416.349653	242803.709666	38.903668
2419.273475	243291.656315	38.908685
2421.597362	243788.510192	38.913703
2423.968440	244280.198825	38.918720
2426.679357	244772.214528	38.923738
2429.275723	245262.722763	38.928756
2431.343768	245753.870939	38.933773
2434.561105	246227.031714	38.938791
2436.857745	246710.825994	38.943808
2439.717148	247187.164722	38.948826
2441.914532	247678.719855	38.953844
2444.978915	248149.537299	38.958861
2447.820439	248622.064781	38.963879
2450.049058	249105.888873	38.968896
2452.266184	249568.604065	38.973914
2454.398635	250057.876584	38.978932
2457.151490	250521.902947	38.983949
2459.364460	251000.897686	38.988967
2461.331745	251483.891970	38.993984
2463.778664	251964.346159	38.999002
2466.078370	252464.838487	39.004020
2468.366557	252944.272866	39.009037
2470.742270	253427.070533	39.014055
2472.591970	253903.928296	39.019072
2474.810872	254364.520835	39.024090
2476.822653	254839.394369	39.029108
2479.526481	255317.308381	39.034125
2482.075557	255789.631138	39.039143
2484.366959	256267.377424	39.044160
2487.262862	256745.815373	39.049178
2489.493868	257233.651850	39.054196
2491.585634	257729.865081	39.059213
2493.997386	258212.208534	39.064231
2496.320596	258721.031509	39.069248
2498.999392	259218.417576	39.074266
2501.920870	259719.777143	39.079284
2504.503685	260207.521895	39.084301
2507.573382	260707.914445	39.089319
2510.126229	261201.197030	39.094336
2512.254592	261685.323327	39.099354
2514.549370	262206.454881	39.104372
2516.928076	262720.001794	39.109389
2519.154309	263235.449639	39.114407
2521.389058	263752.976501	39.119424
2524.170678	264274.962289	39.124442
2526.729825	264815.877287	39.129460
2529.113617	265355.089635	39.134477
2532.185048	265877.962118	39.139495
2534.152255	266425.107412	39.144512
2536.531011	266950.342672	39.149530
2539.229584	267492.517134	39.154548
2542.044617	268028.778006	39.159565
2545.304265	268568.014531	39.164583
2547.674370	269099.589171	39.169600
2550.561516	269630.470802	39.174618
2553.159640	270169.547152	39.179636
2555.909765	270706.996631	39.184653
2558.451829	271237.948106	39.189671
2561.181924	271776.638842	39.194688
2563.791547	272315.548242	39.199706
2565.876215	272858.040854	39.204724
2568.641458	273385.566873	39.209741
2571.503675	273931.461941	39.214759
2573.570995	274487.178767	39.219776
2576.512645	275035.492429	39.224794
2578.746595	275582.058664	39.229812
2581.104245	276134.239982	39.234829
2583.625771	276683.598476	39.239847
2586.054413	277255.062106	39.244864
2588.811951	277810.750494	39.249882
2591.200693	278378.123504	39.254900
2593.477422	278946.068504	39.259917
2596.151673	279515.217208	39.264935
2598.498373	280098.430654	39.269952
2601.209154	280664.847769	39.274970
2603.699786	281241.046357	39.279988
2606.402709	281820.737225	39.285005
2609.297829	282398.209679	39.290023
2611.692589	282980.097751	39.295040
2614.583372	283562.081652	39.300058
2617.164178	284142.864721	39.305076
2619.736328	284713.309232	39.310093
2622.351811	285293.340914	39.315111
2624.917036	285872.588341	39.320128
2627.517691	286452.967993	39.325146
2630.317373	287042.630714	39.330164
2633.268202	287635.971971	39.335181
2636.196835	288204.477953	39.340199
2638.792058	288784.787290	39.345216
2641.751277	289363.358948	39.350234
2644.204475	289919.380450	39.355252
2647.025458	290459.165711	39.360269
2649.511567	290996.307035	39.365287
2652.385451	291541.381481	39.370304
2654.882082	292081.025510	39.375322
2657.526994	292626.633840	39.380340
2659.908971	293169.536095	39.385357
2662.762006	293698.573519	39.390375
2665.442693	294257.795929	39.395392
2667.803299	294796.852997	39.400410
2670.305006	295337.178044	39.405428
2672.947841	295896.060811	39.410445
2675.540431	296454.108212	39.415463
2678.108299	297014.870629	39.420480
2681.155190	297568.469731	39.425498
2683.274962	298134.571620	39.430516
2685.943926	298709.188772	39.435533
2689.041160	299276.777247	39.440551
2691.239302	299857.955000	39.445568
2693.974122	300438.916178	39.450586
2696.671408	301014.418918	39.455604
2699.891935	301605.370535	39.460621
2702.818713	302181.485182	39.465639
2705.363247	302763.694908	39.470656
2707.997511	303346.823542	39.475674
2711.112035	303923.930851	39.480692
2713.944810	304508.970330	39.485709
2716.545815	305095.587738	39.490727
2719.200296	305700.162226	39.495744
2721.715125	306288.505533	39.500762
2724.518997	306884.006007	39.505780
2726.797787	307487.703837	39.510797
2729.512896	308090.971113	39.515815
2732.540103	308705.604735	39.520832
2734.586046	309310.509607	39.525850
2737.499447	309925.780211	39.530868
2740.233620	310545.868066	39.535885
2743.350295	311165.736123	39.540903
2745.842176	311801.531213	39.545920
2748.981284	312410.541824	39.550938
2752.271167	313026.779919	39.555956
2754.830557	313631.854781	39.560973
2758.084991	314243.767674	39.565991
2761.103787	314866.647677	39.571008
2763.611836	315482.746323	39.576026
2766.526513	316097.275999	39.581044
2768.909128	316715.534610	39.586061
2772.015639	317329.839960	39.591079
2774.672091	317956.413575	39.596096
2777.279325	318573.977007	39.601114
2779.954498	319200.555416	39.606132
2782.987688	319817.933522	39.611149
2785.937015	320446.176949	39.616167
2788.463959	321075.491983	39.621184
2791.512184	321695.175436	39.626202
2794.170517	322322.040960	39.631220
2796.937841	322957.355407	39.636237
2799.437409	323585.368699	39.641255
2802.070702	324223.526711	39.646272
2804.783884	324851.157774	39.651290
2807.736574	325490.743545	39.656308
2810.043497	326130.546670	39.661325
2813.281794	326765.450137	39.666343
2816.334855	327411.865984	39.671360
2819.349902	328051.147900	39.676378
2822.540565	328680.167626	39.681396
2825.318113	329301.122983	39.686413
2828.493806	329927.334383	39.691431
2831.142724	330547.249861	39.696448
2833.870396	331152.860102	39.701466
2837.224148	331745.932503	39.706484
2839.545813	332327.537429	39.711501
2841.873075	332922.298881	39.716519
2845.165155	333521.035889	39.721536
2847.326475	334117.326513	39.726554
2850.067588	334709.560168	39.731572
2852.754910	335324.445423	39.736589
2855.731356	335934.582733	39.741607
2858.349202	336536.775486	39.746624
2861.032910	337154.801633	39.751642
2864.080808	337770.655357	39.756660
2866.711711	338400.767795	39.761677
2869.366797	339021.632895	39.766695
2872.413253	339670.149055	39.771712
2875.163755	340309.441881	39.776730
2878.114232	340942.757173	39.781748
2880.889299	341596.429116	39.786765
2883.716375	342241.609914	39.791783
2886.778811	342897.698359	39.796800
2889.439532	343551.275474	39.801818
2892.823714	344200.061313	39.806836
2895.125790	344873.501129	39.811853
2898.409152	345530.646298	39.816871
2900.609084	346203.746068	39.821888
2903.690461	346870.254200	39.826906
2906.935862	347529.876918	39.831924
2909.453696	348227.737602	39.836941
2912.687665	348899.151620	39.841959
2915.679549	349578.450191	39.846976
2918.654951	350265.648358	39.851994
2921.605764	350952.658421	39.857012
2924.340503	351649.297101	39.862029
2927.356774	352336.622627	39.867047
2930.340545	353028.299375	39.872064
2932.858822	353732.025691	39.877082
2935.842819	354427.779281	39.882100
2938.887200	355136.513812	39.887117
2941.890143	355840.574138	39.892135
2945.339007	356552.027766	39.897152
2948.253495	357264.841149	39.902170
2951.031251	357969.141853	39.907188
2953.494127	358683.589785	39.912205
2957.185505	359393.038977	39.917223
2960.353106	360100.829473	39.922240
2963.305913	360825.163386	39.927258
2966.692987	361529.084136	39.932276
2969.598713	362240.160199	39.937293
2973.187133	362939.175262	39.942311
2975.947130	363636.376531	39.947328
2979.614768	364325.639332	39.952346
2982.907954	365004.401162	39.957364
2986.278074	365703.029709	39.962381
2989.784715	366387.428321	39.967399
2993.350079	367050.007408	39.972416
2996.410288	367722.963831	39.977434
2999.566999	368391.404083	39.982452
3002.509328	369053.780344	39.987469
3005.354697	369714.838562	39.992487
3008.511724	370382.091566	39.997504
3010.673251	371051.460045	40.002522
3013.815256	371718.556887	40.007540
3016.559091	372394.643771	40.012557
3019.465204	373060.554239	40.017575
3022.545675	373731.210015	40.022592
3025.398086	374411.816391	40.027610
3028.355121	375082.964991	40.032628
3030.896050	375744.205451	40.037645
3033.868845	376398.775836	40.042663
3036.982202	377043.225936	40.047680
3039.821093	377682.738133	40.052698
3042.746681	378331.290309	40.057716
3045.528585	378974.681492	40.062733
3048.678950	379640.163918	40.067751
3051.474106	380287.624638	40.072768
3054.189195	380958.106149	40.077786
3056.930187	381620.283999	40.082804
3059.781022	382287.772121	40.087821
3063.347178	382971.467847	40.092839
3066.159932	383644.980105	40.097856
3068.705989	384337.865239	40.102874
3072.091659	385027.688562	40.107892
3074.554681	385746.126897	40.112909
3077.561025	386446.201869	40.117927
3080.909420	387151.851264	40.122944
3083.365644	387869.369283	40.127962
3085.950827	388591.328606	40.132980
3089.486360	389326.007479	40.137997
3092.322263	390063.482718	40.143015
3095.353924	390805.589560	40.148032
3098.352391	391549.046369	40.153050
3101.359848	392300.682177	40.158068
3104.773365	393064.586328	40.163085
3108.035604	393828.034254	40.168103
3111.281964	394584.270904	40.173120
3114.374286	395353.367563	40.178138
3118.047401	396110.198459	40.183156
3121.279735	396874.870292	40.188173
3124.473142	397643.674707	40.193191
3127.651718	398400.560015	40.198208
3130.879559	399170.220409	40.203226
3133.972268	399933.144098	40.208244
3137.177007	400699.720442	40.213261
3140.498522	401477.844340	40.218279
3143.413107	402248.109459	40.223296
3146.503891	403022.269111	40.228314
3149.506204	403797.985252	40.233332
3152.454527	404593.167910	40.238349
3155.614285	405373.917239	40.243367
3159.108509	406160.052909	40.248384
3162.156771	406948.558228	40.253402
3165.469956	407745.141452	40.258420
3168.687962	408525.417668	40.263437
3171.861688	409329.201610	40.268455
3175.634437	410119.353736	40.273472
3178.978142	410906.660284	40.278490
3182.363466	411690.795237	40.283508
3185.727452	412480.369118	40.288525
3188.680712	413262.541515	40.293543
3192.461435	414035.703983	40.298560
3195.624465	414814.802702	40.303578
3199.307367	415589.239612	40.308596
3203.065263	416365.912901	40.313613
3205.996465	417124.123468	40.318631
3209.772727	417891.279455	40.323648
3212.626248	418662.546621	40.328666
3215.751786	419427.825853	40.333684
3218.811656	420190.710335	40.338701
3221.664771	420960.476664	40.343719
3225.091164	421734.474126	40.348736
3228.389504	422503.102353	40.353754
3231.607186	423267.163503	40.358772
3234.209788	424044.691148	40.363789
3237.456795	424821.583252	40.368807
3240.616917	425596.790686	40.373824
3243.758770	426366.056010	40.378842
3246.720981	427116.614306	40.383860
3249.405433	427874.315843	40.388877
3251.973391	428629.529750	40.393895
3255.340490	429378.979619	40.398912
3258.490019	430153.405766	40.403930
3261.420012	430914.997032	40.408948
3264.384271	431688.128103	40.413965
3267.027767	432472.650578	40.418983
3270.007002	433270.785650	40.424000
3273.484061	434074.824530	40.429018
3276.600914	434887.426652	40.434036
3279.568310	435684.352392	40.439053
3282.626096	436520.544575	40.444071
3286.151112	437337.830646	40.449088
3289.108153	438184.475808	40.454106
3292.202460	439018.380149	40.459124
3295.510956	439859.590712	40.464141
3298.692286	440730.944136	40.469159
3301.942014	441562.993999	40.474176
3304.941821	442434.195399	40.479194
3308.742245	443306.696330	40.484212
3312.407033	444177.611460	40.489229
3315.824479	445041.654832	40.494247
3318.982366	445918.021494	40.499264
3322.510553	446806.914522	40.504282
3325.949329	447670.426507	40.509300
3329.698807	448546.574804	40.514317
3333.033185	449439.156580	40.519335
3336.738778	450314.670428	40.524352
3340.146909	451205.234282	40.529370
3343.501213	452088.794668	40.534388
3346.924275	452974.976271	40.539405
3349.733096	453860.956740	40.544423
3353.382234	454756.151517	40.549440
3356.821244	455658.652830	40.554458
3360.413866	456554.976127	40.559476
3364.160539	457455.570115	40.564493
3367.453386	458345.538680	40.569511
3371.021277	459238.699118	40.574528
3374.773898	460128.706122	40.579546
3378.421421	461033.368085	40.584564
3382.019937	461925.727947	40.589581
3384.809201	462831.084166	40.594599
3387.962107	463716.405764	40.599616
3391.877812	464615.840321	40.604634
3395.154511	465535.657464	40.609652
3398.852896	466429.025269	40.614669
3401.887548	467338.237613	40.619687
3405.562246	468238.372556	40.624704
3408.856644	469143.309471	40.629722
3412.291506	470044.947040	40.634740
3415.698739	470941.950072	40.639757
3418.999579	471844.820917	40.644775
3422.307366	472747.842461	40.649792
3426.030454	473671.221695	40.654810
3429.592916	474574.102007	40.659828
3433.433457	475476.031413	40.664845
3436.763724	476375.519229	40.669863
3440.820101	477267.180706	40.674880
3444.402594	478157.555424	40.679898
3447.571881	479053.136591	40.684916
3450.988839	479942.479194	40.689933
3454.452217	480839.173582	40.694951
3458.588649	481735.964110	40.699968
3461.903943	482617.611386	40.704986
3465.238363	483515.079866	40.710004
3468.219677	484398.391771	40.715021
3471.813424	485273.372559	40.720026
3475.275091	486112.296637	40.725031
3478.160846	486909.693900	40.730036
3481.764094	487651.530001	40.735040
3484.563699	488335.271726	40.740045
3487.325765	488980.756849	40.745050
3490.090987	489562.429578	40.750055
3492.678173	490098.909652	40.755060
3494.967650	490587.846991	40.760064
3497.420167	491018.620466	40.765069
3499.745437	491409.913361	40.770074
3502.000488	491741.016825	40.775079
3503.665580	492021.811590	40.780084
3505.587204	492264.236692	40.785088
3507.044378	492474.919741	40.790093
3508.654173	492645.636810	40.795098
3509.798154	492763.761570	40.800103
3511.387520	492875.908596	40.805108
3512.110092	492942.495203	40.810112
3513.392059	492972.287487	40.815117
3514.221176	492976.753190	40.820122
3514.790267	492962.022247	40.825127
3515.802145	492924.703307	40.830132
3516.293273	492864.340241	40.835136
3517.192131	492787.806639	40.840141
3517.567657	492689.894983	40.845146
3517.923872	492566.032594	40.850151
3518.136615	492445.524041	40.855156
3518.157461	492310.906263	40.860160
3519.158763	492156.896574	40.865165
3519.172874	491999.100370	40.870170
3519.653490	491814.922061	40.875175
3520.162222	491638.210474	40.880180
3519.817042	491441.582709	40.885184
3520.374467	491233.803600	40.890189
3520.133858	491031.347073	40.895194
3520.174001	490820.612924	40.900199
3520.493488	490595.692644	40.905204
3520.092177	490373.456679	40.910208
3520.513137	490134.070809	40.915213
3520.270013	489924.428788	40.920218
3520.592528	489682.980572	40.925223
3520.096991	489446.756612	40.930228
3520.121907	489205.397626	40.935232
3519.970739	488959.314794	40.940237
3520.058809	488738.241370	40.945242
3520.099347	488485.706898	40.950247
3519.780368	488244.537735	40.955252
3519.354186	487994.391082	40.960256
3519.404853	487765.228166	40.965261
3519.345681	487508.803926	40.970266
3519.503417	487271.434458	40.975271
3519.079509	487021.978712	40.980276
3518.856802	486781.983800	40.985280
3519.402355	486543.835575	40.990285
3518.847947	486291.862662	40.995290
3519.010878	486054.574625	41.000295
3518.802089	485811.177969	41.005300
3518.177215	485578.854630	41.010304
3518.215828	485338.897606	41.015309
3517.789517	485103.858855	41.020314
3517.720795	484866.538098	41.025319
3517.507919	484630.448586	41.030324
3517.299468	484398.598426	41.035328
3517.221288	484165.360484	41.040333
3517.036531	483936.733034	41.045338
3516.732451	483717.265217	41.050343
3516.750228	483482.334880	41.055348
3516.380496	483272.015562	41.060352
3516.540008	483044.180324	41.065357
3516.197271	482839.206496	41.070362
3515.931597	482619.717248	41.075367
3515.893538	482401.351594	41.080372
3515.535953	482184.194727	41.085376
3515.845892	481974.863764	41.090381
3515.262246	481763.951107	41.095386
3515.242783	481556.383768	41.100391
3515.098143	481357.473678	41.105396
3515.087193	481158.186557	41.110400
3514.962416	480932.638693	41.115405
3514.477799	480734.834775	41.120410
3514.478253	480545.897039	41.125415
3514.586275	480344.256632	41.130420
3514.029952	480149.387411	41.135424
3514.041789	479968.223094	41.140429
3513.654893	479777.416151	41.145434
3513.754171	479582.791660	41.150439
3513.781394	479396.160615	41.155444
3513.208041	479217.908760	41.160448
3513.269007	479030.105819	41.165453
3512.939869	478852.923665	41.170458
3512.758750	478679.860604	41.175463
3512.651186	478493.189369	41.180468
3512.561978	478320.411321	41.185472
3512.386449	478152.749325	41.190477
3512.424596	477983.536109	41.195482
3511.907651	477816.378559	41.200487
3511.992906	477641.948700	41.205492
3511.347108	477485.572997	41.210496
3511.492353	477325.534713	41.215501
3511.451196	477182.303992	41.220506
3511.437690	477020.417278	41.225511
3511.491003	476860.135925	41.230516
3511.402498	476710.388215	41.235520
3511.359099	476548.956280	41.240525
3511.274895	476401.075160	41.245530
3510.995499	476244.832485	41.250535
3511.121294	476087.918683	41.255540
3510.544473	475941.929645	41.260544
3510.282843	475789.420215	41.265549
3510.138772	475645.231378	41.270554
3510.365549	475503.612032	41.275559
3510.548496	475365.890485	41.280564
3509.864138	475222.085222	41.285568
3509.794602	475085.007147	41.290573
3509.698766	474955.160600	41.295578
3509.250092	474821.627209	41.300583
3509.628002	474682.251881	41.305588
3509.472392	474565.504071	41.310592
3509.520822	474422.841420	41.315597
3509.326883	474304.227289	41.320602
3509.443259	474169.640097	41.325607
3509.284197	474047.581113	41.330612
3509.117124	473921.478227	41.335616
3509.239917	473800.232918	41.340621
3508.893010	473676.936541	41.345626
3508.667115	473550.688262	41.350631
3508.580152	473425.782349	41.355636
3508.405298	473322.223266	41.360640
3508.620480	473200.301886	41.365645
3508.516955	473087.579728	41.370650
3508.160132	472965.796155	41.375655
3508.039327	472851.861711	41.380660
3508.206043	472751.835331	41.385664
3508.147968	472631.974473	41.390669
3508.104626	472532.383888	41.395674
3508.025005	472420.715091	41.400679
3508.008216	472302.918248	41.405684
3507.628154	472209.293359	41.410688
3507.828863	472104.100778	41.415693
3507.762087	471997.280702	41.420698
3507.512445	471899.336237	41.425703
3507.621573	471802.801579	41.430708
3507.240096	471698.050895	41.435712
3507.317973	471588.981009	41.440717
3507.633265	471496.305589	41.445722
3507.506643	471382.665153	41.450727
3507.098625	471283.882114	41.455732
3506.693007	471203.856358	41.460736
3507.288242	471097.483563	41.465741
3507.320796	471011.877466	41.470746
3506.819730	470914.219038	41.475751
3506.950270	470814.995429	41.480756
3506.652000	470730.551720	41.485760
3507.124264	470649.375393	41.490765
3506.421642	470552.605748	41.495770
3506.526879	470463.850557	41.500775
3506.556767	470378.342699	41.505780
3506.418020	470289.826791	41.510784
3506.575841	470200.606920	41.515789
3506.435273	470108.753071	41.520794
3506.424431	470040.138386	41.525799
3506.317255	469941.704972	41.530804
3506.009460	469866.713994	41.535808
3506.282272	469783.086728	41.540813
3506.305124	469696.817940	41.545818
3506.098402	469615.995008	41.550823
3505.959204	469535.363439	41.555828
3505.899550	469463.163730	41.560832
3506.062140	469376.618690	41.565837
3505.955771	469296.638216	41.570842
3506.078180	469218.037640	41.575847
3506.099067	469136.570133	41.580852
3505.586748	469063.174925	41.585856
3505.615407	468984.486692	41.590861
3505.848171	468912.896461	41.595866
3505.534456	468831.428951	41.600871
3505.916808	468752.077751	41.605876
3505.849873	468690.950373	41.610880
3505.867145	468606.244400	41.615885
3505.794778	468539.402979	41.620890
3505.862097	468465.409224	41.625895
3505.922328	468380.290854	41.630900
3505.704350	468303.660565	41.635904
3505.698146	468223.153614	41.640909
3505.279327	468150.346652	41.645914
3505.542241	468084.766062	41.650919
3505.706202	468016.419202	41.655924
3505.814343	467948.030177	41.660928
3505.588330	467874.382861	41.665933
3505.485854	467785.746756	41.670938
3505.535219	467723.232277	41.675943
3505.341580	467644.167702	41.680948
3504.940468	467577.828715	41.685952
3505.596726	467515.168441	41.690957
3505.244717	467443.106572	41.695962
3505.208249	467382.121352	41.700967
3505.180095	467314.104941	41.705972
3504.996291	467252.889309	41.710976
3505.442968	467178.375632	41.715981
3505.287193	467110.833413	41.720986
3504.992435	467044.678046	41.725991
3505.196876	466970.403432	41.730996
3505.011390	466907.315545	41.736000
3505.305465	466849.210257	41.741005
3505.455922	466783.439745	41.746010
3504.739914	466712.594579	41.751015
3504.778152	466647.903071	41.756020
3504.556634	466594.934653	41.761024
3504.649773	466524.266226	41.766029
3504.890465	466465.611580	41.771034
3504.513246	466419.545139	41.776039
3504.764325	466346.221435	41.781044
3504.757134	466287.756467	41.786048
3504.659027	466227.029500	41.791053
3504.612394	466172.414081	41.796058
3504.760942	466119.184262	41.801063
3504.662924	466049.555113	41.806068
3504.596210	465996.712442	41.811072
3504.769063	465940.241331	41.816077
3504.727110	465879.757254	41.821082
3504.548393	465822.328904	41.826087
3504.645733	465757.220135	41.831092
3504.512168	465701.099369	41.836096
3504.638877	465640.942230	41.841101
3504.976810	465589.350342	41.846106
3504.693696	465525.210288	41.851111
3504.419327	465470.628020	41.856116
3504.578600	465413.398568	41.861120
3504.820368	465347.355314	41.866125
3504.346715	465291.741313	41.871130
3504.395421	465229.672826	41.876135
3504.718298	465175.907093	41.881140
3504.366728	465120.425266	41.886144
3504.155280	465061.279690	41.891149
3504.380165	465009.804776	41.896154
3504.206395	464954.699375	41.901159
3504.307953	464894.239996	41.906164
3504.230638	464851.258567	41.911168
3504.240553	464794.353735	41.916173
3504.603612	464746.599495	41.921178
3504.185818	464696.184669	41.926183
3504.641805	464630.965147	41.931188
3503.882368	464582.424071	41.936192
3504.293386	464526.872200	41.941197
3504.425838	464479.658905	41.946202
3504.808480	464425.021587	41.951207
3504.430217	464365.343124	41.956212
3504.607771	464305.577957	41.961216
3504.540529	464253.792117	41.966221
3504.245836	464198.854809	41.971226
3504.117477	464152.389341	41.976231
3504.647391	464089.381865	41.981236
3504.407397	464042.832301	41.986240
3504.290136	463973.298717	41.991245
3504.338742	463928.879011	41.996250
3504.004234	463875.919600	42.001255
3504.508313	463806.996814	42.006260
3504.155798	463758.642961	42.011264
3504.243024	463713.761424	42.016269
3504.012199	463664.579020	42.021274
3504.082980	463602.855201	42.026279
3504.361339	463550.001737	42.031284
3503.670934	463500.384526	42.036288
3504.036143	463451.816940	42.041293
3504.048196	463413.319993	42.046298
3504.208091	463360.079692	42.051303
3504.363357	463312.606663	42.056308
3503.986603	463255.149794	42.061312
3504.084098	463203.689202	42.066317
3503.857308	463148.181471	42.071322
3503.903923	463108.616154	42.076327
3504.274229	463048.108351	42.081332
3504.025670	463002.113703	42.086336
3504.178193	462951.402576	42.091341
3504.162244	462905.219709	42.096346
3503.875780	462855.638923	42.101351
3503.897736	462806.060584	42.106356
3503.712937	462751.202648	42.111360
3503.719580	462702.587543	42.116365
3503.604774	462663.046306	42.121370
3503.812071	462624.061902	42.126375
3503.967225	462568.088140	42.131380
3503.702688	462530.492219	42.136384
3503.724278	462483.391788	42.141389
3503.654137	462434.787865	42.146394
3503.767750	462386.863441	42.151399
3503.946689	462340.901654	42.156404
3503.720673	462289.083929	42.161408
3503.440045	462251.388718	42.166413
3503.886875	462214.946112	42.171418
3503.665587	462171.120276	42.176423
3503.800060	462118.992994	42.181428
3503.593795	462080.021111	42.186432
3503.632350	462029.527326	42.191437
3503.649242	461989.205193	42.196442
3503.770227	461949.220892	42.201447
3503.598828	461898.101729	42.206452
3503.506741	461852.383157	42.211456
3503.569436	461811.193453	42.216461
3503.515184	461773.563137	42.221466
3503.528505	461732.532695	42.226471
3503.876011	461680.978003	42.231476
3503.621795	461643.682058	42.236480
3503.732228	461596.008857	42.241485
3503.688822	461546.285251	42.246490
3503.520000	461517.930260	42.251495
3504.001601	461463.419790	42.256500
3503.405076	461420.611641	42.261504
3503.273201	461376.820441	42.266509
3503.076435	461338.047748	42.271514
3503.223052	461300.891043	42.276519
3503.292413	461251.604353	42.281524
3503.432915	461220.569981	42.286528
3503.629951	461182.039203	42.291533
3503.969876	461136.049122	42.296538
3503.423624	461100.011634	42.301543
3503.628464	461040.635478	42.306548
3503.122545	461010.308420	42.311552
3503.279572	460957.566979	42.316557
3503.185899	460922.875274	42.321562
3503.258672	460887.702265	42.326567
3503.389711	460846.803157	42.331572
3503.592335	460814.544161	42.336576
3503.530175	460776.153990	42.341581
3503.741626	460740.200206	42.346586
3503.581383	460684.218758	42.351591
3503.717083	460641.851237	42.356596
3503.601230	460602.659541	42.361600
3503.784229	460567.772284	42.366605
3504.006810	460523.518996	42.371610
3503.662314	460475.711094	42.376615
3503.681488	460413.376632	42.381620
3503.521943	460386.536137	42.386624
3503.345761	460333.642253	42.391629
3503.419825	460299.378531	42.396634
3503.511846	460260.609054	42.401639
3503.317049	460213.536041	42.406644
3503.058327	460180.892295	42.411648
3503.207677	460141.759467	42.416653
3503.168937	460105.387936	42.421658
3503.176176	460067.794896	42.426663
3503.240282	460033.380409	42.431668
3503.178483	459995.140219	42.436672
3502.959502	459950.195241	42.441677
3503.231266	459914.888083	42.446682
3503.389600	459879.598505	42.451687
3503.381097	459836.846676	42.456692
3503.092488	459802.031252	42.461696
3503.176538	459757.392785	42.466701
3503.217238	459715.695510	42.471706
3503.393875	459691.786773	42.476711
3503.274137	459640.298660	42.481716
3503.216430	459603.473654	42.486720
3503.199694	459564.972515	42.491725
3503.369534	459538.079438	42.496730
3503.447456	459501.334301	42.501735
3503.406536	459461.470588	42.506740
3503.088200	459418.057580	42.511744
3502.915141	459378.113042	42.516749
3503.272939	459340.868639	42.521754
3502.995941	459303.773535	42.526759
3503.256793	459264.115391	42.531764
3503.326392	459237.035055	42.536768
3502.950557	459195.198950	42.541773
3503.073004	459158.395557	42.546778
3502.787152	459132.028136	42.551783
3503.724437	459090.088634	42.556788
3503.042997	459053.966688	42.561792
3502.998614	459010.560621	42.566797
3503.343229	458977.871305	42.571802
3503.281501	458938.616798	42.576807
3502.837362	458901.648035	42.581812
3503.264897	458876.737759	42.586816
3503.025039	458836.903560	42.591821
3503.205281	458807.528401	42.596826
3502.985175	458770.069107	42.601831
3503.289142	458734.046142	42.606836
3503.098639	458698.454241	42.611840
3502.957074	458659.211522	42.616845
3503.284935	458619.895667	42.621850
3502.823964	458586.926178	42.626855
3503.049617	458552.230602	42.631860
3503.123814	458525.553230	42.636864
3503.064761	458487.056272	42.641869
3502.812031	458448.538768	42.646874
3502.713054	458425.328964	42.651879
3502.663171	458380.707779	42.656884
3502.894422	458360.988488	42.661888
3503.129459	458321.484000	42.666893
3502.852556	458290.306902	42.671898
3502.821023	458263.949181	42.676903
3503.123406	458214.516336	42.681908
3503.142943	458184.608526	42.686912
3502.967578	458148.405933	42.691917
3502.963279	458119.058324	42.696922
3502.869101	458092.355886	42.701927
3503.120486	458067.269458	42.706932
3503.100666	458027.955763	42.711936
3503.261007	457989.524761	42.716941
3503.132676	457952.606026	42.721946
3502.686523	457913.560819	42.726951
3502.971608	457882.143730	42.731956
3502.992437	457849.654476	42.736960
3503.226861	457807.011629	42.741965
3502.948562	457770.773663	42.746970
3503.129860	457741.902551	42.751975
3502.931721	457707.625445	42.756980
3502.881864	457662.951808	42.761984
3502.658818	457633.991632	42.766989
3503.042836	457599.269507	42.771994
3502.911734	457576.620189	42.776999
3503.183715	457539.132260	42.782004
3502.927923	457513.719138	42.787009
3502.910435	457481.083350	42.792013
3502.885186	457439.542661	42.797018
3502.510559	457415.362348	42.802023
3502.583962	457378.056781	42.807028
3502.541398	457351.952405	42.812033
3502.896228	457326.747606	42.817037
3502.989339	457289.286973	42.822042
3502.627044	457256.147787	42.827047
3502.516302	457227.675489	42.832052
3502.792085	457205.265989	42.837057
3502.825618	457165.689025	42.842061
3502.908364	457135.870780	42.847066
3502.732361	457103.562572	42.852071
3502.846622	457066.553601	42.857076
3502.842220	457044.389910	42.862081
3502.824944	457005.225317	42.867085
3502.993546	456977.316386	42.872090
3502.856826	456944.090899	42.877095
3503.162733	456913.782112	42.882100
3503.183340	456882.606793	42.887105
3502.869914	456846.827805	42.892109
3502.748410	456824.176013	42.897114
3502.845302	456787.877614	42.902119
3503.043561	456747.768023	42.907124
3502.864555	456715.358354	42.912129
3502.942958	456684.629129	42.917133
3503.125530	456647.102590	42.922138
3502.703629	456622.371878	42.927143
3502.535879	456584.899720	42.932148
3502.699130	456565.948054	42.937153
3502.589272	456524.367744	42.942157
3503.160673	456499.634103	42.947162
3502.824985	456465.628981	42.952167
3502.567751	456424.779843	42.957172
3503.196949	456397.000732	42.962177
3502.834671	456373.424316	42.967181
3503.308415	456339.849654	42.972186
3502.856315	456297.866610	42.977191
3502.673348	456256.803098	42.982196
3502.667942	456234.031262	42.987201
3502.787088	456205.572128	42.992205
3502.989815	456176.593879	42.997210
3502.453725	456160.382124	43.002215
3502.604228	456124.175216	43.007220
3502.786556	456095.857890	43.012225
3503.053667	456066.363375	43.017229
3502.999487	456023.356226	43.022234
3502.549182	455991.746530	43.027239
3502.837297	455960.376118	43.032244
3502.778904	455924.049483	43.037249
3502.639864	455896.338520	43.042253
3502.944968	455865.015901	43.047258
3502.755849	455824.913868	43.052263
3502.855350	455798.228382	43.057268
3502.705825	455775.782020	43.062273
3502.834615	455742.867183	43.067277
3502.898252	455703.282222	43.072282
3502.414246	455678.003151	43.077287
3502.504878	455645.498930	43.082292
3502.637913	455628.524655	43.087297
3502.591951	455593.511203	43.092301
3502.676214	455567.637464	43.097306
3502.614369	455536.472576	43.102311
3502.762986	455505.780964	43.107316
3502.914308	455480.149702	43.112321
3502.657489	455454.177048	43.117325
3503.041026	455423.904211	43.122330
3502.961086	455388.794421	43.127335
3502.679144	455351.995302	43.132340
3502.650238	455326.493078	43.137345
3502.643076	455298.507605	43.142349
3502.914895	455256.105757	43.147354
3502.946124	455231.606216	43.152359
3502.915290	455205.598027	43.157364
3502.762906	455167.057653	43.162369
3502.796944	455136.939927	43.167373
3502.868047	455104.235306	43.172378
3502.600887	455067.534509	43.177383
3502.823770	455040.120139	43.182388
3502.896165	455019.662657	43.187393
3502.703775	454988.719549	43.192397
3502.875340	454951.393532	43.197402
3502.670418	454926.322996	43.202407
3502.913923	454886.455155	43.207412
3502.813472	454853.979205	43.212417
3502.751133	454825.546074	43.217421
3502.530006	454802.350457	43.222426
3502.397137	454776.256291	43.227431
3502.450183	454741.276344	43.232436
3502.835507	454713.532526	43.237441
3502.720976	454682.171879	43.242445
3502.359860	454655.404504	43.247450
3502.260891	454636.542171	43.252455
3502.270569	454605.415112	43.257460
3502.353476	454590.978174	43.262465
3502.712099	454565.161488	43.267469
3502.501085	454531.335654	43.272474
3501.897849	454508.958275	43.277479
3502.613110	454473.064970	43.282484
3502.673501	454464.401101	43.287489
3502.709994	454429.372499	43.292493
3502.653920	454386.665304	43.297498
3502.302372	454373.915359	43.302503
3502.558773	454339.662141	43.307508
3502.365022	454319.295872	43.312513
3502.393668	454288.620806	43.317517
3502.676856	454260.993394	43.322522
3502.662366	454238.068549	43.327527
3502.799231	454207.325890	43.332532
3502.722379	454187.852293	43.337537
3502.732538	454155.762738	43.342541
3502.956016	454125.411356	43.347546
3502.868566	454091.363000	43.352551
3502.634234	454058.805193	43.357556
3502.497533	454038.632172	43.362561
3502.682729	454005.452246	43.367565
3502.694683	453973.260856	43.372570
3502.576447	453944.075813	43.377575
3502.356759	453910.148911	43.382580
3502.449034	453884.828194	43.387585
3502.680018	453870.873753	43.392589
3502.429868	453836.799612	43.397594
3502.747717	453811.393074	43.402599
3502.721431	453782.395908	43.407604
3502.751052	453748.024994	43.412609
3502.619009	453733.367738	43.417613
3502.757970	453690.577896	43.422618
3502.536220	453662.521990	43.427623
3502.447292	453626.195362	43.432628
3502.712976	453609.147888	43.437633
3502.505426	453578.862641	43.442637
3502.360769	453547.555279	43.447642
3502.191051	453528.854612	43.452647
3502.427581	453493.337502	43.457652
3502.523186	453474.443649	43.462657
3502.123778	453457.955051	43.467661
3502.141223	453421.763293	43.472666
3502.396302	453407.602281	43.477671
3502.425748	453370.092581	43.482676
3502.488697	453349.330947	43.487681
3502.329201	453335.487463	43.492685
3502.596309	453294.650684	43.497690
3502.247339	453272.384009	43.502695
3502.374704	453251.915924	43.507700
3502.330246	453226.109396	43.512705
3502.481259	453200.221797	43.517709
3502.543929	453165.186617	43.522714
3502.459398	453141.005877	43.527719
3502.546180	453115.330609	43.532724
3502.566539	453095.992527	43.537729
3502.505428	453070.340208	43.542733
3502.351996	453039.134543	43.547738
3502.321024	453015.147758	43.552743
3502.390764	452978.187726	43.557748
3502.225913	452961.965858	43.562753
3502.279190	452937.864627	43.567757
3502.395170	452911.374673	43.572762
3502.401861	452889.710174	43.577767
3502.705731	452861.723053	43.582772
3502.586519	452843.216266	43.587777
3502.564492	452806.573853	43.592781
3502.327837	452786.516189	43.597786
3502.605778	452757.166307	43.602791
3502.640795	452719.856829	43.607796
3502.508818	452714.663937	43.612801
3502.591839	452686.913373	43.617805
3502.507565	452651.748197	43.622810
3502.385306	452630.609612	43.627815
3502.354352	452609.203711	43.632820
3502.696933	452571.846062	43.637825
3502.454411	452553.054462	43.642829
3502.683697	452531.152421	43.647834
3502.259853	452498.975552	43.652839
3502.533505	452476.459139	43.657844
3502.562228	452445.629020	43.662849
3502.244140	452420.926856	43.667853
3502.118424	452397.105830	43.672858
3502.296932	452376.426311	43.677863
3502.506329	452350.680241	43.682868
3502.816506	452314.440673	43.687873
3502.526666	452292.568504	43.692877
3502.460063	452263.068954	43.697882
3502.780191	452229.611625	43.702887
3502.503147	452210.065770	43.707892
3502.484109	452178.787062	43.712897
3502.133294	452160.214368	43.717901
3502.366964	452130.414783	43.722906
3502.314487	452113.668475	43.727911
3502.100544	452093.555877	43.732916
3502.600497	452065.132048	43.737921
3502.532590	452039.985480	43.742925
3502.340535	452004.886415	43.747930
3502.501370	451989.017924	43.752935
3502.192078	451963.301391	43.757940
3502.313753	451940.251149	43.762945
3502.091840	451914.267856	43.767949
3502.057412	451887.597310	43.772954
3502.090433	451876.962314	43.777959
3502.076334	451843.657507	43.782964
3502.281468	451821.201548	43.787969
3502.509341	451806.486693	43.792973
3502.396817	451775.474918	43.797978
3502.389134	451749.407430	43.802983
3502.430824	451719.687653	43.807988
3502.593906	451698.452939	43.812993
3502.128115	451678.632157	43.817997
3502.364617	451650.147427	43.823002
3502.292639	451622.672421	43.828007
3502.202875	451598.490397	43.833012
3502.282407	451582.077383	43.838017
3501.990044	451551.295681	43.843021
3502.425972	451527.031757	43.848026
3502.122975	451509.665811	43.853031
3502.263447	451488.282508	43.858036
3502.772461	451474.890361	43.863041
3502.303525	451445.654545	43.868045
3502.529489	451414.690710	43.873050
3502.339533	451397.205825	43.878055
3502.372054	451373.611907	43.883060
3502.471387	451348.134619	43.888065
3502.191450	451325.652280	43.893069
3502.447470	451284.306418	43.898074
3502.267212	451270.110213	43.903079
3502.448045	451240.418607	43.908084
3502.794746	451223.609347	43.913089
3502.090595	451198.914943	43.918093
3502.361646	451167.639943	43.923098
3502.293410	451157.982067	43.928103
3502.225594	451112.585933	43.933108
3502.555841	451102.511673	43.938113
3502.355992	451083.003190	43.943117
3502.652562	451049.547318	43.948122
3502.657500	451019.174023	43.953127
3502.109035	450985.849530	43.958132
3502.596791	450960.007520	43.963137
3502.200625	450940.529431	43.968141
3502.460424	450903.839252	43.973146
3502.116006	450889.921397	43.978151
3501.978252	450869.238727	43.983156
3502.340578	450848.225107	43.988161
3502.281132	450821.860592	43.993165
3502.511376	450805.018440	43.998170
3502.288728	450772.655280	44.003175
3502.459397	450750.203341	44.008180
3501.967813	450726.133287	44.013185
3502.108345	450713.354754	44.018189
3502.371343	450690.331532	44.023194
3502.416486	450662.431850	44.028199
3502.181762	450642.877692	44.033204
3502.370238	450616.221185	44.038209
3502.112145	450598.037411	44.043213
3502.049166	450569.141965	44.048218
3502.199682	450552.970073	44.053223
3502.266104	450533.115822	44.058228
3502.294595	450501.877406	44.063233
3501.727302	450484.399724	44.068237
3502.179359	450473.243085	44.073242
3502.244780	450442.302553	44.078247
3502.020241	450425.935797	44.083252
3502.212454	450397.911573	44.088257
3501.799409	450375.549998	44.093261
3502.171783	450364.101955	44.098266
3502.169328	450340.663987	44.103271
3502.159658	450331.654649	44.108276
3502.109510	450298.909430	44.113281
3501.865640	450274.091499	44.118285
3502.374620	450248.548903	44.123290
3502.180664	450242.554963	44.128295
3502.134522	450214.010688	44.133300
3502.137378	450190.419828	44.138305
3502.113190	450171.186757	44.143309
3502.367842	450150.897805	44.148314
3502.112647	450128.663229	44.153319
3502.323931	450097.395665	44.158324
3502.371328	450076.328904	44.163329
3501.907151	450059.391620	44.168333
3502.354095	450043.628755	44.173338
3502.313355	450024.347478	44.178343
3502.177265	450002.954817	44.183348
3502.305835	449974.838590	44.188353
3502.206826	449968.272920	44.193357
3502.604425	449934.293011	44.198362
3502.199442	449912.385220	44.203367
3502.081472	449891.394600	44.208372
3502.358661	449864.419428	44.213377
3502.177908	449841.616047	44.218381
3502.321576	449814.712203	44.223386
3502.103491	449788.927725	44.228391
3501.991892	449772.644047	44.233396
3502.259499	449751.745136	44.238401
3502.016742	449728.191891	44.243405
3502.216650	449699.608511	44.248410
3502.357140	449680.804912	44.253415
3502.057509	449648.856702	44.258420
3502.274830	449633.432961	44.263425
3502.311465	449614.696079	44.268429
3502.007621	449589.430910	44.273434
3502.259533	449558.915465	44.278439
3502.310119	449546.301975	44.283444
3502.533156	449518.575336	44.288449
3502.119253	449494.440915	44.293453
3502.327766	449478.309658	44.298458
3502.222583	449454.430895	44.303463
3502.259353	449432.808155	44.308468
3502.586471	449404.558891	44.313473
3502.254704	449382.790938	44.318477
3502.426182	449362.210288	44.323482
3502.363234	449337.616039	44.328487
3502.142174	449304.693104	44.333492
3502.270079	449280.524709	44.338497
3502.113847	449270.626382	44.343501
3502.046255	449238.742588	44.348506
3501.978748	449226.754764	44.353511
3502.004705	449207.563486	44.358516
3502.142554	449185.317208	44.363521
3502.112106	449169.881001	44.368525
3502.348185	449143.113654	44.373530
3501.963585	449125.808722	44.378535
3501.683802	449106.513034	44.383540
3501.947204	449086.170898	44.388545
3501.880185	449059.248087	44.393549
3502.178020	449049.430859	44.398554
3501.828220	449032.322928	44.403559
3501.991495	449016.805818	44.408564
3502.040178	448992.294979	44.413569
3501.985935	448983.443783	44.418573
3502.182102	448951.872827	44.423578
3502.015047	448939.191527	44.428583
3502.167552	448928.637446	44.433588
3502.539720	448898.405933	44.438593
3502.000556	448873.530768	44.443597
3502.154850	448839.333526	44.448602
3502.092133	448833.470574	44.453607
3502.093718	448800.208310	44.458612
3501.958141	448778.662233	44.463617
3501.989349	448765.544941	44.468621
3502.023046	448744.833148	44.473626
3502.139063	448723.500992	44.478631
3501.803175	448714.339099	44.483636
3502.028613	448688.787795	44.488641
3502.079207	448673.541064	44.493645
3502.007717	448649.453482	44.498650
3502.134405	448631.207842	44.503655
3501.705087	448626.566308	44.508660
3502.331348	448590.675066	44.513665
3502.211600	448575.859781	44.518669
3502.206232	448550.394826	44.523674
3502.079790	448532.390989	44.528679
3502.035097	448516.652673	44.533684
3502.066459	448488.397375	44.538689
3502.151923	448472.334998	44.543693
3502.046300	448444.100947	44.548698
3501.936186	448419.614044	44.553703
3501.940370	448409.943422	44.558708
3502.028013	448397.373993	44.563713
3501.977540	448373.130888	44.568717
3502.136079	448359.234062	44.573722
3501.628981	448328.682767	44.578727
3502.096203	448321.218328	44.583732
3502.531680	448287.381317	44.588737
3502.281331	448275.522572	44.593741
3502.173700	448242.580051	44.598746
3501.967985	448227.828488	44.603751
3502.180157	448202.632965	44.608756
3502.359695	448185.998778	44.613761
3502.140776	448161.882861	44.618765
3502.018066	448152.991284	44.623770
3501.728223	448125.899242	44.628775
3501.663628	448108.087875	44.633780
3502.338828	448091.224583	44.638785
3502.031085	448077.248212	44.643789
3501.939226	448050.277136	44.648794
3502.077336	448024.890375	44.653799
3501.883548	448005.478871	44.658804
3502.275616	447980.811970	44.663809
3502.047024	447979.531209	44.668813
3501.921314	447952.210849	44.673818
3502.036975	447935.080076	44.678823
3501.779758	447905.552405	44.683828
3502.143232	447887.471690	44.688833
3502.076927	447874.824596	44.693837
3502.225391	447854.904004	44.698842
3502.023988	447840.252714	44.703847
3501.794224	447821.251650	44.708852
3502.212292	447793.441393	44.713857
3502.129115	447775.278181	44.718861
3502.197464	447759.420357	44.723866
3502.120253	447735.433711	44.728871
3501.698988	447711.196791	44.733876
3502.080381	447690.429688	44.738881
3502.026828	447681.071445	44.743885
3502.254572	447658.758675	44.748890
3501.956703	447636.375778	44.753895
3501.613758	447619.518595	44.758900
3502.027115	447593.278311	44.763905
3502.208470	447594.819672	44.768909
3502.240177	447560.639097	44.773914
3502.041726	447546.189633	44.778919
3501.708597	447523.660192	44.783924
3502.141667	447509.466841	44.788929
3502.174017	447490.576536	44.793933
3501.875792	447461.054524	44.798938
3502.025452	447450.955706	44.803943
3502.142858	447433.824190	44.808948
3501.845877	447406.175243	44.813953
3501.992207	447393.140307	44.818957
3501.781892	447373.629437	44.823962
3501.895693	447347.131626	44.828967
3501.762673	447335.304638	44.833972
3502.192833	447323.440637	44.838977
3502.007334	447304.027093	44.843981
3501.752977	447294.953055	44.848986
3502.321605	447263.523730	44.853991
3502.212544	447246.528542	44.858996
3502.325278	447217.802921	44.864001
3501.895338	447208.300478	44.869005
3502.160157	447185.120621	44.874010
3502.098408	447166.852203	44.879015
3502.035098	447149.090328	44.884020
3502.228087	447125.617782	44.889025
3502.268522	447110.624479	44.894029
3502.276459	447082.978224	44.899034
3502.225564	447056.961308	44.904039
3501.998924	447036.946296	44.909044
3501.983721	447010.214910	44.914049
3501.823752	447001.682992	44.919053
3502.280236	446985.156509	44.924058
3502.104605	446956.475350	44.929063
3502.053861	446933.648073	44.934068
3502.114883	446904.524946	44.939073
3501.840904	446889.327226	44.944077
3502.152901	446867.759866	44.949082
3502.094353	446859.667793	44.954087
3502.095686	446826.908281	44.959092
3501.921041	446811.087445	44.964097
3501.910535	446795.899279	44.969101
3502.109562	446773.437997	44.974106
3502.376090	446748.586436	44.979111
3502.012047	446731.174749	44.984116
3502.788494	446696.775397	44.989121
3502.599849	446682.779419	44.994125
3502.361624	446657.145516	44.999130
3502.369984	446642.612519	45.004135
3502.017388	446621.502720	45.009140
3501.865103	446588.007185	45.014145
3501.859780	446576.413000	45.019149
3501.513816	446556.871730	45.024154
3501.778401	446533.286015	45.029159
3501.275244	446530.630136	45.034164
3501.942825	446510.677928	45.039169
3501.900843	446489.519641	45.044173
3501.958595	446473.915517	45.049178
3501.850016	446455.957477	45.054183
3501.929222	446436.704352	45.059188
3501.796166	446423.205863	45.064193
3501.891781	446401.671625	45.069197
3501.929372	446383.640134	45.074202
3501.631169	446364.546931	45.079207
3501.481202	446347.354735	45.084212
3502.092370	446333.791003	45.089217
3502.153743	446322.287546	45.094221
3502.019074	446298.054779	45.099226
3501.994412	446284.134246	45.104231
3501.865700	446268.052620	45.109236
3502.093660	446243.560815	45.114241
3501.805360	446220.364539	45.119245
3501.886867	446203.490627	45.124250
3502.103650	446188.266588	45.129255
3502.002847	446170.458961	45.134260
3501.733579	446157.184009	45.139265
3501.888579	446128.551368	45.144269
3501.940907	446111.580643	45.149274
3501.698110	446100.326919	45.154279
3501.888982	446086.322061	45.159284
3501.750350	446071.760849	45.164289
3501.931360	446056.542267	45.169293
3501.947159	446026.260177	45.174298
3501.768286	446018.895345	45.179303
3501.775334	446000.007435	45.184308
3502.135646	445992.609323	45.189313
3501.947581	445973.093491	45.194317
3501.922946	445955.628248	45.199322
3501.858283	445938.827474	45.204327
3502.144243	445918.731469	45.209332
3501.818127	445897.009089	45.214337
3501.652244	445875.008572	45.219341
3501.722626	445863.807238	45.224346
3501.685521	445850.344030	45.229351
3501.554262	445833.249709	45.234356
3501.772922	445818.632697	45.239361
3501.711488	445816.313058	45.244365
3501.860458	445795.377432	45.249370
3502.313855	445770.191651	45.254375
3502.096286	445755.591836	45.259380
3502.332187	445732.667819	45.264385
3501.838869	445716.439902	45.269389
3501.657153	445706.037238	45.274394
3501.970110	445686.038050	45.279399
3501.815762	445658.414895	45.284404
3501.609724	445648.674250	45.289409
3501.826664	445634.006723	45.294413
3501.838102	445600.230723	45.299418
3501.778132	445590.619226	45.304423
3501.605309	445585.987628	45.309428
3501.854747	445561.289026	45.314433
3501.638661	445553.322162	45.319437
3501.501710	445540.633807	45.324442
3501.847703	445518.249390	45.329447
3501.683008	445508.704783	45.334452
3501.605452	445494.133607	45.339457
3501.834754	445466.956828	45.344461
3501.821309	445461.135758	45.349466
3502.097459	445447.572872	45.354471
3501.934362	445439.192620	45.359476
3502.006989	445418.268444	45.364481
3502.334685	445395.836088	45.369485
3501.738087	445384.636979	45.374490
3501.959498	445347.941549	45.379495
3501.873355	445334.840050	45.384500
3501.875690	445321.015859	45.389505
3501.820479	445294.035008	45.394509
3501.928554	445285.966947	45.399514
3501.987069	445265.348615	45.404519
3501.898219	445254.171687	45.409524
3501.864588	445234.631038	45.414529
3501.761755	445220.012942	45.419533
3501.727783	445210.751660	45.424538
3502.017826	445183.362461	45.429543
3501.632207	445177.700491	45.434548
3502.141536	445166.278515	45.439553
3502.117677	445142.026976	45.444557
3501.694312	445125.483826	45.449562
3502.001545	445089.888549	45.454567
3501.588975	445091.016172	45.459572
3502.016427	445069.732559	45.464577
3501.870670	445044.993486	45.469581
3501.814810	445035.887436	45.474586
3501.858751	445015.625555	45.479591
3501.592777	445003.615197	45.484596
3501.970537	444988.365115	45.489601
3501.581896	444960.828007	45.494605
3501.529096	444952.582283	45.499610
3501.741270	444946.574028	45.504615
3501.884965	444930.955219	45.509620
3501.851934	444912.831997	45.514625
3501.701857	444901.968211	45.519629
3501.938489	444881.068541	45.524634
3501.828507	444864.172560	45.529639
3501.711293	444855.632988	45.534644
3502.020486	444829.202407	45.539649
3502.113369	444809.641620	45.544653
3501.818542	444792.521145	45.549658
3502.167568	444774.540888	45.554663
3501.639033	444752.848652	45.559668
3501.914223	444726.372577	45.564673
3501.970135	444723.173684	45.569677
3501.651766	444700.790380	45.574682
3502.316893	444682.254458	45.579687
3501.964480	444665.142827	45.584692
3501.815946	444643.340689	45.589697
3502.078508	444631.652951	45.594701
3501.795666	444599.288154	45.599706
3502.442629	444589.161015	45.604711
3501.864724	444571.983108	45.609716
3501.891622	444547.419055	45.614721
3502.230657	444543.315210	45.619725
3501.950515	444519.507845	45.624730
3502.122413	444496.339055	45.629735
3501.759040	444474.975262	45.634740
3502.047594	444462.776981	45.639745
3501.987633	444439.188445	45.644749
3501.746130	444433.199982	45.649754
3502.042551	444407.884852	45.654759
3501.976790	444388.044468	45.659764
3502.040989	444376.995110	45.664769
3502.113106	444352.727598	45.669773
3502.048947	444330.557484	45.674778
3502.281628	444309.708422	45.679783
3501.876787	444296.250661	45.684788
3501.920566	444263.226771	45.689793
3502.153727	444252.758724	45.694797
3501.936334	444233.448168	45.699802
3502.284277	444218.505931	45.704807
3501.857116	444198.215182	45.709812
3501.835885	444179.177884	45.714817
3502.012448	444166.743635	45.719821
3502.150270	444140.186816	45.724826
3501.779889	444095.326642	45.729831
3501.773312	444026.912600	45.734836
3501.568365	443923.384549	45.739841
3501.234971	443772.273305	45.744845
3500.784077	443568.258621	45.749850
3500.753304	443319.661725	45.754855
3499.845430	443030.683506	45.759860
3499.432515	442698.373789	45.764865
3499.211992	442316.294774	45.769869
3498.463618	441899.394847	45.774874
3497.731117	441417.603758	45.779879
3496.915162	440914.287484	45.784884
3496.067259	440362.338370	45.789889
3495.514398	439768.184746	45.794893
3494.323199	439121.178684	45.799898
3493.378631	438440.679493	45.804903
3492.084820	437725.003368	45.809908
3491.009764	436953.946233	45.814913
3490.207059	436162.500342	45.819917
3488.578428	435326.160962	45.824922
3487.465482	434444.257606	45.829927
3485.807612	433522.522800	45.834932
3484.544995	432573.624513	45.839937
3483.000536	431582.158278	45.844941
3481.224150	430567.823135	45.849946
3480.074138	429508.082208	45.854951
3478.063048	428407.569295	45.859956
3476.238940	427278.583252	45.864961
3474.415641	426117.499109	45.869965
3472.537724	424922.647552	45.874970
3470.699709	423684.680724	45.879975
3468.547839	422449.932318	45.884980
3466.289056	421156.061293	45.889985
3464.719452	419840.250605	45.894989
3462.229892	418512.634796	45.899994
3460.097043	417130.214751	45.904999
3457.484322	415731.601631	45.910004
3455.472268	414309.220208	45.915009
3452.755330	412868.899527	45.920013
3450.694585	411403.628049	45.925018
3448.361785	409919.988252	45.930023
3445.464581	408401.789147	45.935028
3443.114956	406856.918059	45.940033
3440.426912	405302.606630	45.945037
3437.954414	403717.608856	45.950042
3435.735083	402110.387726	45.955047
3432.393799	400504.142277	45.960052
3430.004140	398857.544130	45.965057
3427.255865	397202.714547	45.970061
3424.247000	395525.019277	45.975066
3421.675903	393828.254658	45.980071
3418.892907	392118.509323	45.985076
3415.695818	390383.374822	45.990081
3412.706765	388654.356237	45.995085
3409.941339	386902.866763	46.000090
3406.988456	385118.328663	46.005095
3404.097074	383343.457180	46.010100
3400.972318	381538.459405	46.015105
3398.014781	379725.260390	46.020109
3395.050838	377902.337744	46.025114
3391.916072	376050.642195	46.030119
3388.369178	374202.922627	46.035124
3385.515138	372334.115431	46.040129
3382.273275	370461.660728	46.045133
3378.786597	368576.823079	46.050138
3376.028599	366681.990906	46.055143
3372.764313	364778.118391	46.060148
3369.069747	362859.704977	46.065153
3365.787838	360929.515383	46.070157
3362.406222	359001.885978	46.075162
3359.229156	357047.137397	46.080167
3355.437517	355104.790083	46.085172
3352.121720	353159.351125	46.090177
3349.025284	351202.473103	46.095181
3345.064643	349239.561261	46.100186
3341.554714	347243.590406	46.105191
3338.345756	345278.649844	46.110196
3334.678616	343292.385716	46.115201
3331.655646	341314.018891	46.120205
3327.916502	339304.781841	46.125210
3324.294681	337311.231701	46.130215
3320.508019	335326.830137	46.135220
3317.185240	333309.034993	46.140225
3313.260943	331302.239133	46.145229
3309.587977	329288.864681	46.150234
3306.199760	327270.891527	46.155239
3302.584180	325273.838941	46.160244
3298.824205	323252.925620	46.165249
3295.112052	321224.580326	46.170253
3291.439005	319209.718639	46.175258
3287.792661	317182.598040	46.180263
3283.846103	315162.709133	46.185268
3280.504327	313136.784311	46.190273
3276.539154	311114.456577	46.195277
3272.764514	309106.849532	46.200282
3269.506171	307068.821609	46.205287
3265.567802	305045.781103	46.210292
3261.758284	303012.689931	46.215297
3257.968698	301000.056782	46.220301
3254.238048	298979.525952	46.225306
3250.554700	296943.871675	46.230311
3246.672687	294930.270331	46.235316
3242.799208	292893.714922	46.240321
3239.146794	290872.585043	46.245325
3235.313266	288847.141526	46.250330
3231.446477	286834.419493	46.255335
3227.787875	284809.715529	46.260340
3223.828693	282796.659308	46.265345
3220.317677	280778.563079	46.270349
3216.175492	278779.172671	46.275354
3212.393273	276765.594476	46.280359
3208.648033	274755.779180	46.285364
3204.701857	272756.106163	46.290369
3200.522711	270750.541536	46.295373
3196.720588	268766.288632	46.300378
3192.920578	266761.470136	46.305383
3188.790860	264784.011350	46.310388
3185.346342	262801.901354	46.315393
3181.137056	260817.684777	46.320397
3177.224415	258849.126074	46.325402
3173.411589	256863.152640	46.330407
3169.484709	254904.339652	46.335412
3165.770264	252944.065601	46.340417
3162.035362	250987.461934	46.345421
3157.816781	249031.903162	46.350426
3154.079882	247079.711287	46.355431
3150.037107	245136.078909	46.360436
3146.035856	243202.787715	46.365441
3142.186122	241253.997746	46.370445
3137.883039	239322.327850	46.375450
3134.054503	237399.485780	46.380455
3130.014189	235487.745079	46.385460
3126.525894	233572.598847	46.390465
3122.792301	231671.160634	46.395469
3118.433203	229776.054463	46.400474
3114.143493	227879.966162	46.405479
3110.179850	225995.311827	46.410484
3106.423572	224111.363642	46.415489
3102.897727	222242.891689	46.420493
3098.492887	220372.547493	46.425498
3094.718378	218524.802633	46.430503
3090.351425	216675.780711	46.435508
3086.337026	214826.915291	46.440513
3082.574473	212990.703182	46.445517
3078.453758	211168.641386	46.450522
3074.908491	209344.744599	46.455527
3070.548180	207528.857643	46.460532
3066.443566	205729.219554	46.465537
3062.437964	203927.595472	46.470541
3058.062984	202140.893676	46.475546
3054.068917	200360.161293	46.480551
3050.132299	198601.366576	46.485556
3046.240978	196837.466620	46.490561
3042.177352	195089.455445	46.495565
3037.945647	193363.699543	46.500570
3034.062481	191631.113753	46.505575
3029.895018	189918.281779	46.510580
3025.664789	188211.138476	46.515585
3021.705334	186506.475326	46.520589
3017.559718	184819.362732	46.525594
3013.232235	183138.621897	46.530599
3009.025919	181475.053718	46.535604
3004.668069	179817.242727	46.540609
3000.737367	178181.446286	46.545613
2996.297810	176550.063202	46.550618
2992.243568	174926.023193	46.555623
2988.089371	173331.603940	46.560628
2983.612012	171740.004564	46.565633
2979.724271	170176.810600	46.570637
2975.546087	168620.594457	46.575642
2971.350155	167068.781075	46.580647
2966.665959	165524.741080	46.585652
2962.118839	164009.507005	46.590657
2957.976450	162513.095292	46.595661
2953.699577	161031.898256	46.600666
2948.879692	159564.566437	46.605671
2944.487211	158126.336057	46.610676
2939.860841	156709.099712	46.615681
2935.500668	155305.880863	46.620685
2930.413832	153928.249348	46.625690
2925.716041	152564.195000	46.630695
2920.745455	151232.921985	46.635700
2916.061377	149928.067775	46.640705
2911.360514	148652.694095	46.645709
2905.910502	147409.827329	46.650714
2900.498712	146198.668714	46.655719
2895.161442	144933.575842	46.660724
2889.967025	143788.276644	46.665729
2884.668192	142677.348806	46.670733
2879.230948	141606.203128	46.675738
2873.897633	140563.132385	46.680743
2868.813353	139556.102466	46.685748
2863.577888	138583.964959	46.690753
2858.693548	137639.248028	46.695757
2854.026971	136737.390243	46.700762
2848.992874	135851.904217	46.705767
2844.485284	135000.269587	46.710772
2839.944393	134162.433632	46.715777
2835.924744	133351.501331	46.720781
2831.327265	132569.028961	46.725786
2827.745066	131792.760268	46.730791
2823.389646	131036.787864	46.735796
2819.134620	130295.784953	46.740801
2815.370815	129577.271225	46.745805
2811.595298	128862.345802	46.750810
2807.946061	128156.621938	46.755815
2803.622906	127473.502910	46.760820
2799.909352	126789.829670	46.765825
2796.473608	126108.630212	46.770829
2792.560803	125457.011350	46.775834
2789.519477	124796.326125	46.780839
2785.671286	124141.780387	46.785844
2781.872943	123497.195960	46.790849
2778.540452	122849.141045	46.795853
2774.549772	122221.077120	46.800858
2771.546830	121584.157955	46.805863
2767.658918	120962.011907	46.810868
2764.153551	120336.115589	46.815873
2761.014478	119697.226513	46.820877
2757.228085	119089.706671	46.825882
2753.576071	118464.690287	46.830887
2749.862996	117855.067803	46.835892
2746.257840	117248.706439	46.840897
2742.676396	116642.847112	46.845901
2739.068114	116043.016362	46.850906
2735.793699	115438.489465	46.855911
2732.049349	114841.738393	46.860916
2728.304219	114242.352404	46.865921
2725.059901	113655.333533	46.870925
2720.694961	113077.004705	46.875930
2717.226846	112494.794796	46.880935
2713.275645	111921.569531	46.885940
2709.273863	111347.166209	46.890945
2705.705203	110775.361977	46.895949
2701.494643	110220.118426	46.900954
2698.038164	109679.628388	46.905959
2694.132016	109128.283212	46.910964
2690.323198	108596.115710	46.915969
2686.140493	108066.620707	46.920973
2682.437532	107561.048105	46.925978
2678.748959	107031.187009	46.930983
2675.318136	106530.545135	46.935988
2670.985124	106013.970116	46.940993
2667.933693	105513.907060	46.945997
2663.855086	105013.426509	46.951002
2660.511829	104524.914992	46.956007
2656.800006	104025.904760	46.961012
2653.129213	103537.903530	46.966017
2649.748953	103056.906170	46.971021
2645.948831	102570.782393	46.976026
2642.691310	102088.585206	46.981031
2639.166006	101606.271531	46.986036
2635.578687	101129.147709	46.991041
2632.685443	100643.839226	46.996045
2628.753611	100165.651949	47.001050
2625.292456	99678.857553	47.006055
2621.998383	99201.881698	47.011060
2618.468805	98733.223374	47.016065
2615.173754	98241.074294	47.021069
2611.687860	97766.920295	47.026074
2608.344042	97270.955709	47.031079
2604.939938	96799.307097	47.036084
2601.529178	96312.441928	47.041089
2598.195492	95823.488176	47.046093
2594.948168	95335.570689	47.051098
2591.249214	94854.186690	47.056103
2587.766150	94362.229260	47.061108
2584.198886	93876.455851	47.066113
2581.113451	93379.509036	47.071117
2577.655558	92894.013694	47.076122
2573.956534	92396.949590	47.081127
2570.867739	91900.116301	47.086132
2567.047187	91401.575310	47.091137
2564.306437	90902.467907	47.096141
2560.812135	90406.205118	47.101146
2557.109966	89903.070970	47.106151
2553.626123	89393.101160	47.111156
2550.199395	88887.946508	47.116161
2546.556193	88387.077646	47.121165
2543.277966	87885.499824	47.126170
2539.755041	87365.673932	47.131175
2536.859550	86867.001409	47.136180
2533.280710	86356.832091	47.141185
2530.010687	85829.333537	47.146189
2526.320501	85323.404708	47.151194
2522.758121	84799.375024	47.156199
2519.156305	84279.718246	47.161204
2515.214597	83767.389934	47.166209
2512.463587	83240.442383	47.171213
2509.175046	82732.921595	47.176218
2505.551647	82197.072193	47.181223
2501.992842	81677.532435	47.186228
2498.473493	81152.978873	47.191233
2494.627839	80625.132662	47.196237
2491.536976	80110.769477	47.201242
2487.990346	79580.864261	47.206247
2484.615922	79051.602814	47.211252
2481.090391	78529.220688	47.216257
2477.724494	77984.889945	47.221261
2473.919628	77463.955878	47.226266
2470.733084	76936.445830	47.231271
2467.144635	76405.071626	47.236276
2463.416623	75869.246631	47.241281
2460.281497	75329.060348	47.246285
2456.586012	74802.636171	47.251290
2453.466987	74259.979846	47.256295
2449.554769	73732.200861	47.261300
2446.229303	73199.249033	47.266305
2442.861181	72663.241628	47.271309
2439.520618	72122.987058	47.276314
2436.060734	71587.701417	47.281319
2431.898612	71049.069633	47.286324
2428.200432	70521.784896	47.291329
2424.993566	69971.434370	47.296333
2421.522596	69438.911515	47.301338
2418.087158	68898.776396	47.306343
2414.987058	68368.585671	47.311348
2411.252758	67821.835248	47.316353
2408.069774	67279.828551	47.321357
2404.411006	66734.517808	47.326362
2400.859463	66190.439789	47.331367
2397.404392	65652.610460	47.336372
2394.127552	65104.514230	47.341377
2390.719312	64563.476465	47.346381
2387.053029	64016.099235	47.351386
2383.010454	63466.913907	47.356391
2380.034917	62930.318507	47.361396
2376.552452	62370.871241	47.366401
2373.533951	61813.312703	47.371405
2369.553029	61272.359368	47.376410
2366.152938	60718.102466	47.381415
2362.917516	60171.536325	47.386420
2359.224988	59619.653332	47.391425
2355.769537	59058.995403	47.396429
2351.938916	58513.466488	47.401434
2348.514352	57948.539920	47.406439
2345.247461	57398.335431	47.411444
2341.356618	56846.654387	47.416449
2338.032857	56290.786336	47.421453
2334.421039	55742.786364	47.426458
2331.356400	55189.162373	47.431463
2327.901558	54634.406585	47.436468
2324.313290	54073.086556	47.441473
2321.200707	53515.118988	47.446477
2317.442311	52963.989756	47.451482
2313.890580	52393.727478	47.456487
2310.533746	51826.113130	47.461492
2307.156184	51256.295636	47.466497
2303.611077	50694.859694	47.471501
2300.124915	50134.436783	47.476506
2296.732102	49575.135692	47.481511
2293.239932	49013.123569	47.486516
2289.818568	48434.895925	47.491521
2286.278515	47859.688745	47.496525
2282.716073	47297.323908	47.501530
2279.414976	46726.871378	47.506535
2275.752296	46149.411778	47.511540
2272.140405	45582.772032	47.516545
2268.745640	45014.115151	47.521549
2264.931878	44443.679848	47.526554
2261.533425	43875.299856	47.531559
2258.432445	43285.448312	47.536564
2254.793361	42729.678111	47.541569
2251.101002	42148.426961	47.546573
2247.560475	41580.438744	47.551578
2244.415576	40997.439844	47.556583
2240.985484	40422.039630	47.561588
2237.420584	39848.159199	47.566593
2234.000964	39265.078173	47.571597
2230.284652	38690.979279	47.576602
2226.815958	38117.491084	47.581607
2223.477952	37534.501124	47.586612
2219.648209	36950.253230	47.591617
2216.437013	36372.574887	47.596621
2212.965089	35799.142885	47.601626
2209.345201	35215.023961	47.606631
2205.715535	34627.208164	47.611636
2202.087652	34051.134746	47.616641
2199.002834	33462.639079	47.621645
2195.752018	32892.154511	47.626650
2191.961987	32310.227864	47.631655
2188.201707	31729.605731	47.636660
2184.788199	31148.293052	47.641665
2181.626631	30560.974862	47.646669
2178.008262	29976.368081	47.651674
2174.305135	29399.408296	47.656679
2170.793898	28810.052438	47.661684
2167.373703	28232.808922	47.666689
2164.318601	27657.983490	47.671693
2160.617395	27068.213177	47.676698
2156.750728	26487.255076	47.681703
2152.956575	25895.271307	47.686708
2149.753227	25318.571071	47.691713
2146.259939	24739.315841	47.696717
2142.353754	24164.373698	47.701722
2138.903650	23573.963283	47.706727
2135.430880	22996.966316	47.711732
2131.877595	22419.593178	47.716737
2128.120171	21830.112218	47.721741
2124.564476	21272.569006	47.726746
2120.612168	20699.856397	47.731751
2117.025928	20121.415381	47.736756
2113.533250	19567.318513	47.741761
2109.969597	18990.319882	47.746765
2106.174668	18438.214915	47.751770
2102.765378	17875.381032	47.756775
2099.275232	17317.202538	47.761780
2095.495141	16764.876910	47.766785
2092.147126	16208.063640	47.771789
2088.182999	15659.091494	47.776794
2084.718722	15102.559513	47.781799
2081.329908	14557.167472	47.786804
2076.958171	14015.528023	47.791809
2073.650055	13467.925669	47.796813
2068.999982	12941.265757	47.801818
2064.979219	12412.610402	47.806823
2061.424210	11905.079388	47.811828
2057.421540	11408.537438	47.816833
2052.598692	10930.816375	47.821837
2047.032625	10499.069231	47.826842
2040.941915	10081.449286	47.831847
2035.903143	9689.662705	47.836852
2030.762944	9323.947506	47.841857
2026.053427	8966.316677	47.846861
2022.029187	8646.853301	47.851866
2017.618101	8322.131874	47.856871
2013.665279	8025.954075	47.861876
2009.233559	7749.804828	47.866881
2005.572783	7463.696600	47.871885
2001.966214	7198.719906	47.876890
1998.519087	6941.757912	47.881895
1995.258125	6685.223117	47.886900
1991.832768	6447.712739	47.891905
1988.778540	6185.177588	47.896909
1984.545421	5947.448130	47.901914
1980.940728	5703.297745	47.906919
1978.108975	5466.995757	47.911924
1974.535457	5231.701529	47.916929
1971.172862	4990.557876	47.921933
1967.185955	4770.052372	47.926938
1963.967389	4537.088455	47.931943
1960.919044	4303.471311	47.936948
1957.679699	4083.278684	47.941953
1954.620341	3851.115221	47.946957
1951.124305	3622.243988	47.951962
1947.887443	3383.994336	47.956967
1944.330617	3152.762135	47.961972
1940.830354	2922.327807	47.966977
1937.557022	2693.322954	47.971981
1933.924541	2464.940127	47.976986
1930.583262	2231.879496	47.981991
1927.010395	1998.310554	47.986996
1923.467189	1768.283724	47.992001
1919.914565	1545.104970	47.997005
1916.208999	1328.995704	48.002010
1912.299157	1102.802732	48.007015
1909.207945	889.045697	48.012020
1904.931646	680.088502	48.017025
1901.452455	472.069569	48.022029
1897.324242	266.191526	48.027034
1892.936458	96.004902	48.032039
1883.786129	46.774992	48.037044
1873.256603	87.561467	48.042049
1867.178472	85.878441	48.047053
1863.072953	90.756812	48.052058
1860.806910	99.645209	48.057063
1858.806313	88.478680	48.062068
1856.931177	98.470481	48.067073
1854.232593	91.579187	48.072077
1851.270669	89.854085	48.077082
1847.889773	97.520799	48.082087
1844.790577	91.571367	48.087092
1841.174256	97.607449	48.092097
1838.011545	100.826835	48.097101
1834.861438	101.854974	48.102106
1831.252475	101.303074	48.107111
1827.889929	97.131504	48.112116
1824.348319	97.901043	48.117121
1820.691595	94.208688	48.122125
1817.417396	98.328101	48.127130
1814.160173	91.084002	48.132135
1811.041321	96.479520	48.137140
1807.709520	108.438076	48.142145
1804.297791	95.295562	48.147149
1800.712414	98.786374	48.152154
1797.390598	98.455537	48.157159
1793.918809	94.652147	48.162164
1790.176668	106.778967	48.167169
1786.965523	98.160976	48.172173
1783.484955	108.371010	48.177178
1779.889895	96.060616	48.182183
1777.030919	100.665891	48.187188
1773.105636	96.208595	48.192193
1770.092184	90.467288	48.197197
1766.579644	95.582400	48.202202
1762.578922	101.466345	48.207207
1759.527676	91.643413	48.212212
1755.898702	105.192105	48.217217
1752.264923	106.861831	48.222221
1749.243691	100.859146	48.227226
1745.349860	102.844590	48.232231
1742.362914	95.903277	48.237236
1738.425781	103.055464	48.242241
1735.652838	101.854607	48.247245
1731.859729	105.627688	48.252250
1728.115086	97.757118	48.257255
1724.516849	101.063277	48.262260
1721.108125	103.229481	48.267265
1717.891367	101.490269	48.272269
1714.555373	97.583496	48.277274
1711.466422	103.211643	48.282279
1708.119547	91.451088	48.287284
1704.300548	100.470456	48.292289
1700.730850	91.607735	48.297293
1697.122060	96.225311	48.302298
1693.338679	95.779663	48.307303
1690.017072	86.792913	48.312308
1686.605618	95.119271	48.317313
1683.125247	96.625923	48.322317
1679.755373	87.703634	48.327322
1676.489227	90.954944	48.332327
1673.044888	89.444145	48.337332
1668.973945	96.341916	48.342337
1665.635667	92.096990	48.347341
1662.076481	99.838913	48.352346
1658.423770	102.906787	48.357351
1655.482711	97.435793	48.362356
1652.201590	95.538930	48.367361
1648.491607	99.865380	48.372365
1644.829973	95.765694	48.377370
1641.240509	98.241603	48.382375
1637.849317	98.756795	48.387380
1634.079725	102.709716	48.392385
1630.808717	100.706878	48.397389
1627.708149	97.500616	48.402394
1624.161869	101.039136	48.407399
1620.784738	89.545896	48.412404
1616.825205	93.838422	48.417409
1613.362333	92.501353	48.422413
1610.120950	90.224993	48.427418
1606.396446	97.454818	48.432423
1602.730260	87.968066	48.437428
1598.949212	81.121903	48.442433
1596.362896	86.637016	48.447437
1592.835467	92.858584	48.452442
1589.241258	91.943749	48.457447
1585.585823	90.073515	48.462452
1582.100667	96.342288	48.467457
1578.432307	95.090988	48.472461
1574.981584	91.907595	48.477466
1571.287102	96.940305	48.482471
1568.193307	84.998025	48.487476
1564.485699	91.045160	48.492481
1561.234208	84.606952	48.497485
1557.959020	93.706191	48.502490
1554.010684	87.949073	48.507495
1550.652043	100.076308	48.512500
1547.132108	90.709168	48.517505
1543.374506	88.674510	48.522509
1540.612598	85.314311	48.527514
1536.612102	94.289164	48.532519
1533.385399	89.248619	48.537524
1529.689847	91.434169	48.542529
1525.963613	95.525878	48.547533
1522.676547	86.321812	48.552538
1518.978902	90.488163	48.557543
1515.674117	86.718926	48.562548
1512.282335	88.224458	48.567553
1508.798627	92.778283	48.572557
1505.338861	81.949653	48.577562
1500.990794	91.870765	48.582567
1497.883659	88.434592	48.587572
1494.390658	92.635531	48.592577
1491.927904	83.334808	48.597581
1488.130382	89.762931	48.602586
1484.423674	102.934579	48.607591
1480.969332	87.691747	48.612596
1477.211901	89.029571	48.617601
1473.410017	84.002631	48.622605
1470.198745	83.325594	48.627610
1466.476129	88.381669	48.632615
1463.198710	87.689619	48.637620
1459.697381	95.479487	48.642625
1456.525837	88.294872	48.647629
1452.789736	85.421664	48.652634
1449.182418	90.583179	48.657639
1446.045483	86.158250	48.662644
1442.400105	95.593515	48.667649
1438.591915	88.931930	48.672653
1435.231225	95.541997	48.677658
1431.538386	87.631782	48.682663
1428.329994	83.800098	48.687668
1424.696311	89.465581	48.692673
1421.468234	91.986496	48.697677
1417.581624	97.068101	48.702682
1413.930435	94.536014	48.707687
1410.757603	89.619976	48.712692
1407.019206	83.080410	48.717697
1403.872325	84.737654	48.722701
1400.477761	81.691074	48.727706
1396.808033	92.250075	48.732711
1393.437515	93.132223	48.737716
1389.508021	93.993810	48.742721
1386.109409	81.830096	48.747725
1382.993727	87.320044	48.752730
1379.193843	83.950583	48.757735
1376.125529	85.529162	48.762740
1372.121940	86.816727	48.767745
1368.709172	90.166806	48.772749
1365.349317	91.790765	48.777754
1361.398192	100.751614	48.782759
1358.438650	92.853820	48.787764
1354.636072	84.568403	48.792769
1351.165803	86.582864	48.797773
1347.759674	87.710999	48.802778
1344.394528	95.859318	48.807783
1341.245882	87.010218	48.812788
1337.619798	90.061315	48.817793
1333.790959	92.795964	48.822797
1330.169246	81.761626	48.827802
1326.324585	78.025828	48.832807
1323.083025	83.010197	48.837812
1319.756857	74.840459	48.842817
1316.010990	81.399750	48.847821
1313.107089	74.828388	48.852826
1309.497430	85.283127	48.857831
1305.956506	77.447367	48.862836
1302.192644	83.838621	48.867841
1298.546423	86.712524	48.872845
1295.015703	91.631177	48.877850
1291.718151	90.119717	48.882855
1288.479107	85.995434	48.887860
1284.689957	85.383053	48.892865
1281.325799	85.441662	48.897869
1277.788922	83.863054	48.902874
1274.091219	83.616083	48.907879
1270.674553	82.085203	48.912884
1267.292849	83.630314	48.917889
1263.758615	86.309623	48.922893
1260.419312	85.219109	48.927898
1256.574746	84.792524	48.932903
1253.327032	83.172074	48.937908
1249.490933	70.823397	48.942913
1245.909536	80.909912	48.947917
1242.703667	72.265892	48.952922
1238.880327	82.665307	48.957927
1235.901445	82.515258	48.962932
1232.578247	83.763370	48.967937
1228.781105	82.677687	48.972941
1225.647085	74.028813	48.977946
1221.793282	82.613851	48.982951
1218.047802	76.050113	48.987956
1214.700234	84.369697	48.992961
1210.818700	88.039520	48.997965
1207.647930	77.564592	49.002970
1204.505469	80.847298	49.007975
1200.518323	74.102886	49.012980
1197.176387	70.443878	49.017985
1193.551285	82.267732	49.022989
1190.251969	78.526161	49.027994
1186.639858	86.602193	49.032999
1183.348677	73.713139	49.038004
1180.107232	80.867786	49.043009
1176.452450	81.965040	49.048013
1172.808432	84.946176	49.053018
1168.915835	84.758027	49.058023
1165.249073	82.633350	49.063028
1161.805852	75.807443	49.068033
1158.619906	73.946442	49.073037
1155.394876	71.908031	49.078042
1151.477172	73.897243	49.083047
1148.009754	75.851167	49.088052
1144.402425	82.335121	49.093057
1141.014996	74.972198	49.098061
1138.246141	66.225375	49.103066
1134.436398	88.274526	49.108071
1130.849955	83.638040	49.113076
1127.082108	77.767482	49.118081
1123.492380	82.116374	49.123085
1120.059656	78.129829	49.128090
1116.519355	77.390151	49.133095
1113.267775	76.789026	49.138100
1109.681710	79.042989	49.143105
1106.301900	86.908862	49.148109
1102.793457	78.954190	49.153114
1099.293428	85.750468	49.158119
1096.044903	78.732917	49.163124
1092.353333	89.655983	49.168129
1088.850844	80.621569	49.173133
1084.766411	81.703455	49.178138
1081.415992	87.634907	49.183143
1077.878870	83.183736	49.188148
1074.904072	80.037058	49.193153
1071.180029	81.281142	49.198157
1067.706866	78.094984	49.203162
1064.025284	86.020486	49.208167
1060.840003	76.006580	49.213172
1057.049994	86.059137	49.218177
1053.317899	82.957575	49.223181
1050.259792	74.401317	49.228186
1046.695779	82.178807	49.233191
1043.122739	80.998154	49.238196
1039.656784	77.285706	49.243201
1035.600408	79.818524	49.248205
1032.575315	80.295769	49.253210
1028.915285	86.462075	49.258215
1025.937458	75.742020	49.263220
1022.112884	72.673842	49.268225
1018.694203	81.099411	49.273229
1015.349823	84.040247	49.278234
1011.471767	80.227438	49.283239
1008.024998	77.568678	49.288244
1004.645337	76.914737	49.293249
1000.967770	79.977038	49.298253
997.670473	82.372721	49.303258
994.118684	81.777211	49.308263
990.813253	86.021751	49.313268
986.824935	83.608638	49.318273
983.398158	83.155017	49.323277
980.015871	76.955556	49.328282
976.596715	86.899769	49.333287
973.149902	79.928922	49.338292
969.533759	76.704924	49.343297
966.364463	85.949035	49.348301
963.200798	74.558746	49.353306
958.955770	88.880339	49.358311
955.456245	71.246609	49.363316
951.912822	80.387607	49.368321
948.235123	92.966287	49.373325
944.756696	73.984709	49.378330
941.762749	76.478705	49.383335
938.156227	71.076604	49.388340
934.767936	72.815756	49.393345
931.090903	83.398045	49.398349
927.476475	74.817677	49.403354
923.629733	88.409736	49.408359
920.332854	88.204816	49.413364
917.257321	82.824461	49.418369
913.164363	85.543317	49.423373
909.866355	85.357556	49.428378
906.392500	82.247455	49.433383
903.225073	82.860761	49.438388
899.599126	76.373383	49.443393
895.741237	79.751658	49.448397
892.764875	75.659308	49.453402
888.736750	77.131076	49.458407
885.574285	75.696712	49.463412
882.110540	71.721359	49.468417
878.620586	81.973979	49.473421
875.205789	70.733532	49.478426
871.676374	82.672207	49.483431
867.842901	71.009728	49.488436
864.590120	68.377738	49.493441
860.243860	71.990222	49.498445
857.230719	70.640182	49.503450
853.938015	73.313565	49.508455
850.481637	72.054668	49.513460
847.132967	75.850377	49.518465
843.540661	86.745341	49.523469
840.037045	68.001832	49.528474
836.506277	74.423266	49.533479
832.987437	75.186192	49.538484
829.369123	77.071889	49.543489
825.678937	87.279754	49.548493
822.125855	71.707625	49.553498
818.890737	83.435978	49.558503
815.262728	75.961869	49.563508
811.990058	78.249333	49.568513
808.059671	79.408511	49.573517
805.278022	71.454653	49.578522
801.664126	84.441002	49.583527
798.342420	75.530362	49.588532
794.744663	73.701873	49.593537
790.868683	82.034127	49.598541
787.353905	76.285582	49.603546
783.397350	83.431347	49.608551
780.007095	77.138249	49.613556
776.713782	71.105304	49.618561
773.456542	70.473462	49.623565
770.373789	73.737413	49.628570
766.254790	74.337514	49.633575
762.718832	70.091855	49.638580
759.530954	77.668440	49.643585
755.882795	78.464161	49.648589
752.580181	77.421779	49.653594
748.943694	78.785145	49.658599
745.536795	75.341951	49.663604
742.061899	82.409576	49.668609
738.307898	77.020974	49.673613
734.827574	78.853565	49.678618
731.041875	77.563693	49.683623
727.559696	70.456034	49.688628
724.084142	67.855579	49.693633
720.641485	74.203194	49.698637
717.420557	68.589250	49.703642
713.990722	66.298047	49.708647
710.674122	69.462367	49.713652
707.094359	64.065634	49.718657
703.198257	71.765123	49.723661
699.889421	74.814345	49.728666
695.868679	69.752007	49.733671
692.368591	74.112288	49.738676
689.682395	71.578778	49.743681
685.961010	76.476533	49.748685
682.297789	75.483969	49.753690
678.857907	80.957984	49.758695
675.315276	69.310385	49.763700
671.890597	75.149018	49.768705
668.221571	77.903147	49.773709
665.010619	64.362665	49.778714
661.146631	71.187149	49.783719
657.844360	64.446958	49.788724
654.240356	67.738279	49.793729
650.771794	73.074394	49.798733
646.981906	60.588962	49.803738
643.554469	75.074333	49.808743
640.256384	68.504330	49.813748
636.860760	65.166965	49.818753
633.037077	69.862355	49.823757
629.894393	66.665944	49.828762
626.641374	72.303855	49.833767
622.696449	72.484583	49.838772
619.277957	70.134681	49.843777
615.654772	70.635473	49.848781
612.472864	74.440042	49.853786
608.617518	68.826804	49.858791
605.515838	66.500350	49.863796
602.106635	66.369900	49.868801
598.113035	72.898200	49.873805
594.604332	59.261725	49.878810
590.898052	68.905800	49.883815
587.501850	68.637289	49.888820
584.247939	69.289401	49.893825
580.767506	76.541389	49.898829
577.457070	61.529493	49.903834
573.695439	76.364274	49.908839
570.030750	71.512280	49.913844
566.618701	70.566051	49.918849
563.224862	70.920418	49.923853
560.002802	66.043812	49.928858
556.150320	69.864194	49.933863
552.798642	65.327298	49.938868
549.158853	62.160832	49.943873
545.523640	70.819437	49.948877
542.228055	68.760452	49.953882
538.547305	71.206380	49.958887
534.995797	60.873123	49.963892
531.786613	67.048366	49.968897
527.910085	71.726684	49.973901
524.753006	61.787595	49.978906
521.117244	69.652207	49.983911
517.382077	65.500874	49.988916
513.985593	66.399810	49.993921
510.859056	71.227122	49.998925
507.239387	62.454678	50.003930
504.115340	67.243639	50.008935
500.247442	64.343638	50.013940
496.489232	60.031388	50.018945
492.854551	68.066671	50.023949
489.751721	66.319362	50.028954
486.022783	65.511059	50.033959
482.201852	72.059944	50.038964
479.304061	65.437145	50.043969
475.686172	80.259045	50.048973
471.958898	72.145579	50.053978
468.436954	66.306465	50.058983
465.368304	70.637564	50.063988
461.902357	70.515965	50.068993
458.382201	87.018380	50.073997
455.007563	79.555515	50.079002
450.507968	78.810245	50.084007
447.222827	76.018840	50.089012
443.886296	80.556157	50.094017
440.295844	82.823530	50.099021
437.626182	74.282838	50.104026
433.920298	69.503719	50.109031
430.115112	66.132073	50.114036
426.445855	69.335504	50.119041
422.642239	75.138238	50.124045
419.716105	68.133894	50.129050
415.942566	73.520671	50.134055
412.861202	73.788447	50.139060
408.997629	71.210481	50.144065
405.529598	76.609808	50.149069
402.290223	69.891506	50.154074
398.408414	74.143567	50.159079
394.915515	68.682746	50.164084
391.790115	67.087656	50.169089
387.730779	79.238549	50.174093
384.029506	69.276641	50.179098
381.096589	72.700791	50.184103
377.593407	74.255414	50.189108
374.432733	73.352332	50.194113
370.610470	69.527787	50.199117
367.559571	66.108323	50.204122
363.617686	68.680345	50.209127
359.742679	71.814578	50.214132
356.160020	70.385589	50.219137
352.981540	70.371107	50.224141
349.675859	68.152375	50.229146
346.095900	65.985835	50.234151
342.493613	64.607360	50.239156
339.029859	67.247312	50.244161
335.102305	71.069916	50.249165
331.989487	65.113351	50.254170
328.268573	63.069995	50.259175
324.714922	70.453617	50.264180
321.591737	64.960562	50.269185
318.233316	69.279840	50.274189
314.581413	72.879203	50.279194
311.167942	67.364906	50.284199
306.965954	78.895788	50.289204
303.817074	67.424253	50.294209
300.142775	68.717633	50.299213
296.855135	68.903645	50.304218
293.746712	63.965101	50.309223
290.331740	64.113992	50.314228
286.681937	60.053814	50.319233
282.609971	74.585747	50.324237
279.536030	64.649581	50.329242
275.630700	63.112658	50.334247
272.268979	77.976931	50.339252
268.963946	63.470458	50.344257
265.203581	67.646679	50.349261
261.967207	68.391010	50.354266
258.500729	66.469400	50.359271
254.866879	67.098447	50.364276
251.208214	70.512215	50.369281
247.414554	78.464706	50.374285
244.488290	73.124496	50.379290
240.694106	71.446891	50.384295
237.298094	76.727456	50.389300
234.358363	66.020617	50.394305
230.295243	63.546515	50.399309
226.701935	59.439589	50.404314
222.945704	65.136890	50.409319
219.411555	72.754758	50.414324
216.397385	65.612302	50.419329
212.923432	70.617109	50.424333
209.906937	65.967977	50.429338
206.084515	66.354316	50.434343
202.393256	71.592266	50.439348
199.081383	70.576711	50.444353
195.240664	75.170400	50.449357
191.611814	74.817944	50.454362
188.092932	76.419327	50.459367
184.782513	80.063615	50.464372
181.255921	69.239352	50.469377
177.697401	71.362584	50.474381
174.549192	65.750067	50.479386
170.817626	81.608367	50.484391
166.846879	77.183735	50.489396
164.058994	76.716172	50.494401
159.968727	81.952978	50.499405
156.823908	75.928658	50.504410
153.540011	77.559898	50.509415
149.944820	83.713015	50.514420
146.469041	76.098286	50.519425
142.687606	83.210515	50.524429
139.467244	72.958660	50.529434
135.652931	78.348651	50.534439
132.090612	76.239508	50.539444
128.781285	68.465997	50.544449
125.187824	66.292104	50.549453
121.809767	71.013079	50.554458
118.252152	76.299833	50.559463
114.878994	72.965380	50.564468
111.749032	61.206218	50.569473
107.694306	72.818585	50.574477
104.551667	63.067154	50.579482
100.867352	60.005771	50.584487
97.036419	77.436056	50.589492
93.736208	70.856994	50.594497
90.400912	72.395006	50.599501
86.466400	78.547176	50.604506
82.991454	65.554122	50.609511
79.534774	63.096358	50.614516
76.243691	65.437383	50.619521
72.443830	73.571181	50.624525
68.931618	66.816331	50.629530
65.335566	71.413070	50.634535
62.376521	65.992578	50.639540
59.097476	67.347835	50.644545
55.331694	67.364722	50.649549
51.530521	68.658908	50.654554
48.029851	67.229858	50.659559
44.584473	77.497717	50.664564
41.568300	65.034339	50.669569
38.092770	70.048900	50.674573
34.713242	61.261319	50.679578
30.877904	62.057806	50.684583
26.931003	68.205581	50.689588
23.447160	63.372990	50.694593
20.023365	72.068316	50.699597
16.609993	55.965320	50.704602
12.858028	66.866184	50.709607
9.098529	68.555672	50.714612
5.954461	64.242803	50.719617
2.611525	68.249663	50.724621