Fri Aug 26 13:40:50 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.204029	104.247112	0.000000
1.368293	93.711909	0.005005
0.911857	91.343834	0.010010
1.051611	89.120209	0.015014
0.928461	91.645033	0.020019
0.754906	83.997068	0.025024
0.550513	69.251512	0.030029
0.167781	66.884620	0.035034
-0.035835	60.013276	0.040038
0.207929	43.236503	0.045043
-0.420474	54.220488	0.050048
-0.606921	45.793126	0.055053
-0.508421	38.447660	0.060058
-1.467707	33.104968	0.065062
-1.828447	21.041256	0.070067
-2.308967	21.650764	0.075072
-1.974019	7.609032	0.080077
-2.201302	21.725820	0.085082
-2.761232	15.115607	0.090086
-3.032010	9.099433	0.095091
-3.127554	14.476715	0.100096
-3.740758	6.441672	0.105101
-4.005033	-3.365550	0.110106
-4.482555	3.684657	0.115110
-4.228429	-1.261676	0.120115
-4.732317	3.461035	0.125120
-4.370047	2.683358	0.130125
-4.825371	0.261341	0.135130
-5.394849	-1.162176	0.140134
-5.720426	0.875317	0.145139
-5.742243	7.272464	0.150144
-6.333186	0.151413	0.155149
-7.130895	6.574454	0.160154
-7.221135	3.276211	0.165158
-7.031071	3.686402	0.170163
-7.660737	7.387860	0.175168
-7.413030	3.701654	0.180173
-7.535464	0.092060	0.185178
-7.673496	0.040824	0.190182
-7.904508	-9.224263	0.195187
-8.478980	4.285366	0.200192
-8.780165	-0.245488	0.205197
-8.919151	4.828518	0.210202
-8.979925	19.299015	0.215206
-9.242946	-4.570780	0.220211
-9.782793	13.824449	0.225216
-9.951478	4.812232	0.230221
-10.241541	7.391505	0.235226
-10.474029	0.015335	0.240230
-10.329938	-4.901210	0.245235
-11.249077	6.396921	0.250240
-11.288463	8.301273	0.255245
-11.576297	5.998705	0.260250
-11.969998	3.124183	0.265254
-11.669184	3.115348	0.270259
-11.736851	5.666322	0.275264
-12.685772	-0.155682	0.280269
-12.473590	3.781684	0.285274
-12.920789	8.928988	0.290278
-12.874897	2.025147	0.295283
-13.226641	8.217408	0.300288
-14.196241	0.709241	0.305293
-14.446299	5.344977	0.310298
-14.960822	-5.457790	0.315302
-14.660520	-2.309236	0.320307
-14.853798	7.667371	0.325312
-14.736876	0.524690	0.330317
-14.529678	4.570396	0.335322
-15.478763	8.960642	0.340326
-15.726708	7.873028	0.345331
-16.265001	12.911134	0.350336
-16.180796	-3.565513	0.355341
-15.975008	0.084957	0.360346
-16.783529	4.431171	0.365350
-16.885170	6.591979	0.370355
-17.096358	5.691624	0.375360
-17.652060	6.993019	0.380365
-17.382393	-4.646826	0.385370
-18.503802	-0.277206	0.390374
-18.403104	-8.610048	0.395379
-18.731403	6.841690	0.400384
-18.619577	1.961803	0.405389
-18.797728	7.399399	0.410394
-19.205693	8.016592	0.415398
-19.156718	-6.341257	0.420403
-20.071297	10.274239	0.425408
-20.438680	5.139945	0.430413
-20.123473	-4.827098	0.435418
-20.324768	7.697485	0.440422
-20.547577	2.838064	0.445427
-20.836290	5.964436	0.450432
-21.480578	-4.273981	0.455437
-21.305248	5.009342	0.460442
-21.948455	3.967451	0.465446
-21.551073	0.169361	0.470451
-21.730512	0.260608	0.475456
-22.178859	9.460711	0.480461
-22.929967	6.360273	0.485466
-23.390145	-0.831754	0.490470
-22.844722	-2.090348	0.495475
-23.068562	-0.597023	0.500480
-24.346685	-11.135367	0.505485
-24.296359	-4.205312	0.510490
-24.471233	-2.311502	0.515494
-24.376537	-13.000317	0.520499
-24.868652	-4.511552	0.525504
-24.997226	-2.245315	0.530509
-24.863062	-7.036931	0.535514
-25.741994	2.176428	0.540518
-25.924095	-3.752311	0.545523
-26.084638	-4.597279	0.550528
-26.139532	-2.519677	0.555533
-26.481578	-11.175874	0.560538
-26.628363	-0.548475	0.565542
-27.085898	-6.152765	0.570547
-27.529390	-7.494659	0.575552
-27.291874	-2.204040	0.580557
-27.498978	1.387334	0.585562
-27.724762	1.210561	0.590566
-27.991797	-0.652335	0.595571
-28.686912	4.267822	0.600576
-28.866199	-2.142228	0.605581
-29.047264	1.644400	0.610586
-29.142656	2.032599	0.615590
-29.846467	-1.780693	0.620595
-30.279514	5.132880	0.625600
-30.608020	8.186357	0.630605
-30.622078	-4.570367	0.635610
-30.672167	6.750635	0.640614
-30.533678	1.012416	0.645619
-30.708409	-8.508197	0.650624
-30.287599	2.495885	0.655629
-31.047687	-1.432026	0.660634
-31.625790	2.982712	0.665638
-31.866469	-1.456325	0.670643
-32.311283	0.511151	0.675648
-32.930460	4.394466	0.680653
-33.000586	6.091640	0.685658
-33.561547	2.797089	0.690662
-33.373292	0.986686	0.695667
-33.701615	4.112898	0.700672
-33.909886	-0.229948	0.705677
-33.471646	-2.465236	0.710682
-33.932006	-5.386322	0.715686
-34.449797	-13.616536	0.720691
-34.927556	-13.010622	0.725696
-35.139398	1.359995	0.730701
-34.826456	-1.554947	0.735706
-35.801437	0.415983	0.740710
-36.481984	-1.676748	0.745715
-36.532691	1.029766	0.750720
-36.047004	0.495455	0.755725
-35.838559	-7.423908	0.760730
-36.731430	-8.790744	0.765734
-36.643870	-13.356810	0.770739
-37.470593	-4.347730	0.775744
-38.026652	-2.641334	0.780749
-37.770385	-4.247198	0.785754
-38.134306	3.898920	0.790758
-38.008018	-7.864125	0.795763
-38.156735	-8.992496	0.800768
-38.910707	-4.740196	0.805773
-39.175331	-12.465682	0.810778
-39.463976	-3.635289	0.815782
-39.253471	-10.542607	0.820787
-39.287397	2.731001	0.825792
-40.202489	-4.070666	0.830797
-40.766978	-0.483758	0.835802
-41.042650	2.754474	0.840806
-41.055990	-6.294576	0.845811
-41.248421	-2.673851	0.850816
-41.284590	-2.051274	0.855821
-41.433205	0.477502	0.860826
-41.399790	0.092699	0.865830
-41.814270	-7.153893	0.870835
-42.209287	2.794011	0.875840
-42.817158	1.050619	0.880845
-42.574933	-1.400913	0.885850
-42.678324	-8.135978	0.890854
-43.380649	-6.251791	0.895859
-44.087738	-1.690426	0.900864
-44.354656	-4.597339	0.905869
-44.236329	-9.443433	0.910874
-44.368922	-1.684499	0.915878
-43.976717	-15.570614	0.920883
-44.204589	-13.032663	0.925888
-45.111642	-0.094494	0.930893
-45.193451	-3.080847	0.935898
-45.332366	-2.382163	0.940902
-45.462150	-13.304934	0.945907
-46.417753	-9.710913	0.950912
-46.776582	2.420591	0.955917
-46.985221	-5.440160	0.960922
-46.678503	5.553213	0.965926
-46.672389	-9.845120	0.970931
-47.102483	3.876135	0.975936
-47.963782	-5.265507	0.980941
-47.781106	-5.796931	0.985946
-48.881096	-2.784682	0.990950
-48.233315	-13.129355	0.995955
-48.545610	-4.523062	1.000960
-48.815268	-0.868167	1.005965
-48.649965	-8.638448	1.010970
-48.995659	-0.919098	1.015974
-49.399334	-8.540681	1.020979
-50.200811	-4.290475	1.025984
-50.418365	-1.383984	1.030989
-50.509576	-20.474934	1.035994
-50.546788	-8.551695	1.040998
-50.418399	-13.396191	1.046003
-51.053964	-5.321674	1.051008
-51.726589	-11.370181	1.056013
-51.702530	-10.181200	1.061018
-51.900460	2.532670	1.066022
-51.984457	0.714039	1.071027
-51.633690	-2.510501	1.076032
-52.350286	-1.791473	1.081037
-52.634993	-0.798017	1.086042
-53.066565	1.553360	1.091046
-52.938767	-10.678135	1.096051
-53.712493	1.714113	1.101056
-54.396453	-0.068050	1.106061
-54.447401	-7.149788	1.111066
-54.663386	-5.230596	1.116070
-54.652019	-7.573419	1.121075
-54.634972	-9.496363	1.126080
-54.501642	-7.732796	1.131085
-54.999541	-3.801929	1.136090
-55.643476	5.621605	1.141094
-55.946902	-7.558278	1.146099
-56.001285	-2.630321	1.151104
-56.315942	-14.122233	1.156109
-56.227822	-11.687263	1.161114
-57.026602	-11.274967	1.166118
-57.190739	-8.092067	1.171123
-57.300115	-9.052563	1.176128
-57.578413	1.626947	1.181133
-57.954634	-5.176366	1.186138
-58.189773	1.861408	1.191142
-58.564127	-7.387685	1.196147
-58.971741	-1.306948	1.201152
-58.927011	-2.693221	1.206157
-58.877698	-15.602164	1.211162
-59.160685	-2.824438	1.216166
-59.265679	-3.763471	1.221171
-59.777899	-6.505645	1.226176
-60.234973	-2.163535	1.231181
-60.633356	4.311221	1.236186
-60.789010	-0.685198	1.241190
-60.435051	-5.827399	1.246195
-60.737820	-3.385349	1.251200
-61.488526	-10.627043	1.256205
-61.849270	-3.819642	1.261210
-62.038240	4.058798	1.266214
-61.644642	0.166388	1.271219
-62.206302	6.789949	1.276224
-62.901721	3.358152	1.281229
-63.134269	-5.055676	1.286234
-63.792162	-0.644334	1.291238
-63.472534	-11.671877	1.296243
-63.608151	-7.689854	1.301248
-63.498675	-4.495773	1.306253
-63.598565	-12.212107	1.311258
-64.430809	-9.921728	1.316262
-64.757556	-7.912527	1.321267
-65.220310	-13.177491	1.326272
-64.963590	-10.192991	1.331277
-64.641925	-5.807622	1.336282
-65.495320	7.954233	1.341286
-66.168469	-10.865791	1.346291
-66.331587	-7.993086	1.351296
-66.577239	-9.251892	1.356301
-66.390443	-11.419556	1.361306
-66.947494	-5.204826	1.366310
-66.622116	-11.677629	1.371315
-67.143557	-11.359132	1.376320
-67.961791	-13.711985	1.381325
-67.936718	-9.201347	1.386330
-67.844228	-0.525205	1.391334
-67.876960	-7.407306	1.396339
-68.498641	-3.855784	1.401344
-68.739872	-10.309967	1.406349
-68.759212	-9.493865	1.411354
-69.635357	-2.027270	1.416358
-69.968961	-5.135763	1.421363
-70.260068	-6.710183	1.426368
-70.612145	-5.424674	1.431373
-70.596362	-13.174835	1.436378
-70.745458	-3.856826	1.441382
-70.438841	-6.444928	1.446387
-70.411730	-9.223620	1.451392
-71.214242	-2.299981	1.456397
-71.857818	-3.765740	1.461402
-72.375339	-7.832650	1.466406
-72.326779	-7.890793	1.471411
-72.170941	-4.052222	1.476416
-72.411180	-7.981978	1.481421
-72.360375	-11.460358	1.486426
-73.118530	-2.212028	1.491430
-73.279799	-4.739935	1.496435
-73.715076	-1.094054	1.501440
-73.796075	-2.463915	1.506445
-73.817209	-10.053311	1.511450
-74.906541	-2.999596	1.516454
-74.901751	-5.683068	1.521459
-75.032973	-2.979838	1.526464
-75.342954	-2.985319	1.531469
-75.013347	-8.522344	1.536474
-75.052259	-1.758725	1.541478
-75.526790	-9.119346	1.546483
-75.758507	-5.669669	1.551488
-76.406934	-2.544238	1.556493
-76.601036	-2.362125	1.561498
-77.578100	-1.580396	1.566502
-77.562043	-8.381510	1.571507
-77.807332	-9.479027	1.576512
-78.178119	-7.152933	1.581517
-77.771259	-4.868827	1.586522
-77.969526	-0.424650	1.591526
-77.939729	-7.076049	1.596531
-78.079632	2.069694	1.601536
-78.634102	-2.377428	1.606541
-79.402658	-6.117362	1.611546
-79.615630	-0.955913	1.616550
-79.599178	9.870690	1.621555
-79.534704	-0.816585	1.626560
-80.093441	0.279647	1.631565
-80.255633	-4.886589	1.636570
-80.854464	6.371156	1.641574
-80.663291	-4.149189	1.646579
-80.735525	0.300675	1.651584
-81.470646	4.021715	1.656589
-81.791974	-0.468035	1.661594
-82.463403	-2.479929	1.666598
-82.330388	0.514342	1.671603
-82.268794	3.079988	1.676608
-82.402538	7.624849	1.681613
-82.805691	-4.751760	1.686618
-83.641028	2.180155	1.691622
-83.533281	-1.683565	1.696627
-84.105208	-8.234948	1.701632
-83.793457	-10.213268	1.706637
-83.949463	-3.330182	1.711642
-84.183546	2.729863	1.716646
-84.226587	-3.875397	1.721651
-84.813390	-2.942468	1.726656
-85.386618	1.253219	1.731661
-85.686445	-5.748640	1.736666
-85.618752	0.678854	1.741670
-85.522609	-1.395605	1.746675
-85.735102	-8.958370	1.751680
-86.350044	-0.994627	1.756685
-86.657923	-6.666505	1.761690
-86.849370	2.145591	1.766694
-87.512631	0.964461	1.771699
-87.886241	-10.299979	1.776704
-88.375698	-5.304283	1.781709
-88.327765	2.951706	1.786714
-87.858985	7.915262	1.791718
-88.290769	-8.208958	1.796723
-88.651135	-9.124048	1.801728
-88.953789	-8.747870	1.806733
-88.830270	-2.189869	1.811738
-89.369730	-4.899328	1.816742
-89.900025	-7.948722	1.821747
-90.103864	-4.114259	1.826752
-90.367194	-8.502310	1.831757
-90.282361	-6.591992	1.836762
-90.546113	-2.210382	1.841766
-91.068131	-3.391358	1.846771
-91.611712	-6.413374	1.851776
-91.637718	0.028708	1.856781
-91.410462	5.548706	1.861786
-91.703959	-0.603122	1.866790
-91.638273	-14.365630	1.871795
-92.387155	-4.666346	1.876800
-93.173985	8.765616	1.881805
-92.846333	-1.272962	1.886810
-92.866823	2.273537	1.891814
-93.123067	-7.496961	1.896819
-93.538889	-1.769274	1.901824
-94.192257	4.077654	1.906829
-94.048907	-9.118004	1.911834
-94.407875	0.042864	1.916838
-94.511530	-0.538887	1.921843
-94.771284	-7.996221	1.926848
-95.693577	-4.144803	1.931853
-95.788764	1.251397	1.936858
-96.007597	-0.887911	1.941862
-95.725698	1.121433	1.946867
-95.788472	-1.130755	1.951872
-96.062010	5.492233	1.956877
-96.347786	-3.454286	1.961882
-97.047766	9.979972	1.966886
-97.111750	-0.557592	1.971891
-97.451498	-7.556397	1.976896
-97.772136	8.042830	1.981901
-98.127987	3.058601	1.986906
-98.643717	0.908574	1.991910
-98.823223	-6.001291	1.996915
-98.644420	1.010889	2.006912
-98.325922	0.907521	2.016909
-97.780587	1.478396	2.026906
-97.757453	4.395474	2.036902
-97.107531	7.420861	2.046899
-96.533716	6.786749	2.056896
-95.855108	0.051194	2.066893
-95.190544	-0.248602	2.076890
-95.188088	7.144469	2.086886
-94.696495	9.079483	2.096883
-93.928591	6.020379	2.106880
-93.463552	3.176320	2.116877
-92.766048	3.698161	2.126874
-92.241378	8.748196	2.136870
-92.119183	14.887229	2.146867
-92.048166	5.233803	2.156864
-91.123860	9.097086	2.166861
-90.071740	-4.006656	2.176858
-89.727245	3.320488	2.186854
-89.855953	2.653213	2.196851
-89.202793	2.260162	2.206848
-88.349913	0.619623	2.216845
-87.910630	2.784519	2.226842
-87.252783	2.894400	2.236838
-87.055015	11.207369	2.246835
-86.291917	9.245034	2.256832
-85.789585	3.899030	2.266829
-85.629196	2.274449	2.276826
-85.110552	1.405015	2.286822
-84.150610	3.108722	2.296819
-83.965766	1.036857	2.306816
-83.523803	-3.853102	2.316813
-82.328603	0.386136	2.326810
-82.292577	0.681530	2.336806
-82.133990	6.526636	2.346803
-81.833799	2.564708	2.356800
-81.102436	3.429723	2.366797
-80.242893	2.687770	2.376794
-79.645411	-0.363804	2.386790
-79.205499	-4.562888	2.396787
-79.579752	-2.854179	2.406784
-78.436808	-2.984547	2.416781
-78.025506	4.794679	2.426778
-77.226096	6.833814	2.436774
-76.938290	6.643363	2.446771
-76.657166	3.732908	2.456768
-75.576131	-1.852080	2.466765
-75.141473	-1.530057	2.476762
-74.933660	-0.843276	2.486758
-74.773390	5.936035	2.496755
-73.881261	2.480635	2.506752
-73.382676	-2.810933	2.516749
-72.278487	-4.702835	2.526746
-71.998983	4.649078	2.536742
-72.588459	2.529887	2.546739
-71.399057	7.780523	2.556736
-70.788169	2.205381	2.566733
-70.887107	0.944281	2.576730
-70.203395	3.052114	2.586726
-69.294633	4.760623	2.596723
-68.617968	6.606636	2.606720
-68.135547	0.858268	2.616717
-68.266351	5.855144	2.626714
-67.560496	8.517043	2.636710
-67.138375	8.429219	2.646707
-65.887327	3.685705	2.656704
-65.684990	4.408184	2.666701
-65.363523	10.915320	2.676698
-65.314239	4.429797	2.686694
-64.517623	3.371370	2.696691
-63.989104	2.595430	2.706688
-63.182286	-2.129600	2.716685
-63.041134	-0.627846	2.726682
-62.321674	1.883053	2.736678
-61.602406	4.568204	2.746675
-61.579749	6.088408	2.756672
-61.112678	3.627322	2.766669
-60.034635	6.988349	2.776666
-59.682235	-3.960122	2.786662
-59.643573	8.657165	2.796659
-59.115284	5.150714	2.806656
-58.461631	6.126028	2.816653
-57.114598	5.114944	2.826650
-57.365167	-1.719851	2.836646
-56.952581	4.225086	2.846643
-56.585088	3.635769	2.856640
-55.722577	9.187551	2.866637
-55.334900	1.049659	2.876634
-54.921039	3.810872	2.886630
-54.040561	9.043087	2.896627
-54.068104	5.879760	2.906624
-53.355139	1.501950	2.916621
-52.204129	-1.366554	2.926618
-52.148166	4.747946	2.936614
-52.177461	-0.062305	2.946611
-51.578174	0.744084	2.956608
-50.963322	-2.769509	2.966605
-50.638821	-3.352132	2.976602
-49.367428	0.115001	2.986598
-49.413248	-0.384621	2.996595
-48.957035	3.057386	3.006592
-47.793786	2.144607	3.016589
-47.664322	5.168671	3.026586
-47.753379	-0.221465	3.036582
-47.016714	6.170341	3.046579
-46.437024	-1.411424	3.056576
-46.055734	-1.458046	3.066573
-45.037784	-1.708329	3.076570
-45.031819	-6.476553	3.086566
-44.205773	-4.457403	3.096563
-43.795306	-1.724171	3.106560
-43.333490	-2.385192	3.116557
-42.593788	-1.603833	3.126554
-41.975885	0.634619	3.136550
-41.611354	-1.050256	3.146547
-42.012974	1.628859	3.156544
-41.010990	6.544394	3.166541
-40.457123	7.319842	3.176538
-39.739999	-2.915670	3.186534
-39.046491	-1.946561	3.196531
-39.200828	2.677024	3.206528
-38.178651	-0.377320	3.216525
-37.410728	-0.233893	3.226522
-37.425397	-4.270337	3.236518
-36.728372	0.619821	3.246515
-36.161420	5.707624	3.256512
-36.050490	-0.942713	3.266509
-35.473740	0.640100	3.276506
-34.677909	-1.390684	3.286502
-34.269786	6.072272	3.296499
-33.360565	-2.663156	3.306496
-33.133827	3.589475	3.316493
-32.834523	-6.166015	3.326490
-32.735411	-0.542890	3.336486
-31.910561	1.612658	3.346483
-31.316190	9.588293	3.356480
-30.099510	4.552367	3.366477
-29.875745	-5.546143	3.376474
-30.230199	0.987039	3.386470
-29.603768	1.051130	3.396467
-28.970485	-9.155487	3.406464
-28.595671	-1.113996	3.416461
-27.592288	-7.649869	3.426458
-27.276799	-3.428875	3.436454
-26.740159	2.708984	3.446451
-26.058754	0.094155	3.456448
-25.350863	1.352452	3.466445
-25.541942	-1.855101	3.476442
-24.936714	-7.831655	3.486438
-24.035178	-0.895336	3.496435
-23.940256	-1.255320	3.506432
-23.556080	4.814415	3.516429
-22.863584	-0.656228	3.526426
-22.127560	3.347243	3.536422
-21.576420	6.254971	3.546419
-21.497281	9.578299	3.556416
-20.778029	6.596460	3.566413
-19.966934	0.758905	3.576410
-20.128023	2.554798	3.586406
-18.988219	2.976099	3.596403
-18.609643	0.744195	3.606400
-18.416961	-4.864030	3.616397
-17.851204	-2.855034	3.626394
-17.171566	-4.234189	3.636390
-17.042343	-0.899654	3.646387
-16.063139	-2.502842	3.656384
-15.251769	-0.269169	3.666381
-15.570550	0.075133	3.676378
-15.094552	2.503568	3.686374
-14.249062	-3.218969	3.696371
-13.561378	-0.069583	3.706368
-12.886683	-3.757212	3.716365
-12.534690	-2.136237	3.726362
-12.270856	4.839189	3.736358
-12.348675	1.607665	3.746355
-11.409555	-7.084902	3.756352
-10.312140	-4.154527	3.766349
-9.744501	-2.215514	3.776346
-9.931312	0.810279	3.786342
-9.508660	-1.586872	3.796339
-8.770854	-0.615156	3.806336
-8.203938	-4.944884	3.816333
-8.089774	-3.657498	3.826330
-7.331650	-0.835848	3.836326
-6.852445	1.012401	3.846323
-5.640245	-0.117065	3.856320
-5.291783	0.655521	3.866317
-5.348937	1.351881	3.876314
-5.206913	6.128891	3.886310
-4.359764	9.617735	3.896307
-4.023953	13.601161	3.906304
-3.563089	23.187772	3.916301
-2.982808	23.908426	3.926298
-2.291849	32.816176	3.936294
-2.285216	44.947490	3.946291
-2.085710	62.189958	3.956288
-1.359960	75.318024	3.966285
-0.654144	88.417526	3.976282
-0.248189	101.649253	3.986278
0.000000	121.082527	3.991283
0.457451	127.927101	3.996288
0.805023	140.496032	4.001293
0.699254	140.398645	4.006298
1.239025	142.867717	4.011302
0.772142	137.397708	4.016307
0.959169	134.897806	4.021312
0.844087	138.427425	4.026317
0.734900	136.593719	4.031322
1.124761	138.504018	4.036326
1.237323	141.814702	4.041331
1.135562	139.268016	4.046336
1.279038	143.099055	4.051341
1.089471	141.549939	4.056346
1.155091	135.905276	4.061350
0.824981	145.915920	4.066355
1.430177	134.302834	4.071360
0.873035	138.378994	4.076365
1.091731	143.672588	4.081370
1.327241	145.546810	4.086374
1.268117	158.425840	4.091379
1.562383	150.559480	4.096384
1.353918	146.741795	4.101389
1.206874	137.064935	4.106394
1.415578	140.275231	4.111398
1.140745	143.427939	4.116403
1.065522	135.584313	4.121408
1.262364	143.665334	4.126413
1.289518	148.533185	4.131418
1.648814	149.869293	4.136422
1.329525	143.164619	4.141427
1.218886	143.378029	4.146432
1.118590	143.687902	4.151437
1.757321	161.418906	4.156442
1.835643	148.581249	4.161446
1.737974	147.707503	4.166451
1.504460	138.066251	4.171456
1.541204	148.823349	4.176461
1.335187	146.751626	4.181466
1.453359	137.770606	4.186470
1.405165	142.716624	4.191475
1.436571	147.865379	4.196480
1.661238	143.360179	4.201485
1.416004	150.089546	4.206490
1.840701	149.390726	4.211494
1.424486	143.068129	4.216499
1.624654	142.568778	4.221504
1.467436	138.240093	4.226509
1.274312	143.806609	4.231514
1.307909	145.000443	4.236518
1.369233	148.376052	4.241523
1.419082	147.703958	4.246528
1.659613	158.821628	4.251533
1.680809	159.109422	4.256538
2.108021	163.234801	4.261542
1.734385	163.024100	4.266547
1.699063	149.296164	4.271552
1.618875	143.455907	4.276557
1.415158	151.137401	4.281562
1.760976	158.647919	4.286566
1.755297	162.122546	4.291571
1.840031	172.239453	4.296576
2.171971	172.156172	4.301581
1.502441	157.400707	4.306586
1.457206	151.713189	4.311590
1.751864	167.915939	4.316595
2.245493	164.118646	4.321600
2.155089	162.212413	4.326605
1.860282	157.104737	4.331610
1.957251	148.538290	4.336614
1.761998	150.005030	4.341619
1.772027	138.130276	4.346624
1.573989	141.954379	4.351629
1.368938	156.589816	4.356634
1.497513	165.798249	4.361638
1.771446	173.743897	4.366643
2.192004	161.185131	4.371648
2.067440	169.964757	4.376653
1.901808	168.323329	4.381658
2.348019	164.448000	4.386662
2.089577	165.026098	4.391667
2.433827	169.676910	4.396672
2.081557	156.298865	4.401677
1.726646	149.061912	4.406682
1.738270	165.065124	4.411686
1.935582	174.348279	4.416691
2.215017	170.862737	4.421696
2.129043	165.453633	4.426701
2.075213	167.743055	4.431706
2.354764	163.384324	4.436710
2.242874	166.527485	4.441715
2.258987	160.697539	4.446720
1.913445	156.360206	4.451725
2.045627	169.709319	4.456730
2.187976	162.511995	4.461734
1.884662	165.634341	4.466739
2.242411	173.279045	4.471744
1.964790	180.291870	4.476749
2.066940	176.789638	4.481754
2.187372	170.361331	4.486758
2.218550	175.750568	4.491763
2.073827	173.213730	4.496768
2.010890	175.934830	4.501773
2.031740	179.057326	4.506778
2.176567	167.974628	4.511782
1.727843	169.461852	4.516787
2.152569	171.920368	4.521792
2.464854	166.797259	4.526797
2.113089	172.119572	4.531802
2.675901	172.652060	4.536806
2.327390	177.464516	4.541811
2.528478	168.913485	4.546816
2.390069	173.459117	4.551821
2.119434	172.498408	4.556826
2.452594	177.046547	4.561830
2.362776	181.037301	4.566835
2.530660	175.689906	4.571840
2.654406	175.917442	4.576845
2.220726	180.739997	4.581850
2.669969	177.443145	4.586854
2.299588	173.078039	4.591859
2.254620	173.284389	4.596864
2.561223	184.024802	4.601869
2.842552	191.966143	4.606874
2.622445	178.434629	4.611878
2.405277	180.021840	4.616883
2.312602	180.086924	4.621888
2.773935	184.320888	4.626893
2.568221	175.213112	4.631898
2.781565	169.146816	4.636902
2.505896	185.966712	4.641907
2.504217	178.867734	4.646912
2.723442	188.463851	4.651917
2.848013	185.113147	4.656922
2.538407	178.106404	4.661926
2.141455	183.818559	4.666931
2.625459	184.916960	4.671936
2.592632	191.265269	4.676941
2.646819	191.560581	4.681946
3.066614	195.744069	4.686950
2.893987	194.163838	4.691955
2.943525	198.828906	4.696960
2.752599	199.352202	4.701965
2.793661	193.331704	4.706970
2.827334	197.803095	4.711974
2.800309	205.188190	4.716979
2.847280	198.062647	4.721984
2.386318	187.814556	4.726989
2.437492	200.562552	4.731994
2.761880	200.588011	4.736998
2.892470	193.553852	4.742003
2.957230	197.985602	4.747008
2.796610	200.674460	4.752013
2.841277	202.012103	4.757018
3.075906	199.653473	4.762022
2.659924	198.430661	4.767027
2.556746	201.718001	4.772032
2.808335	193.291969	4.777037
2.708688	208.584900	4.782042
2.733781	203.006635	4.787046
2.813692	206.059830	4.792051
2.853204	196.496257	4.797056
3.097245	208.739680	4.802061
2.959668	206.049867	4.807066
3.241753	212.693994	4.812070
2.678566	212.566587	4.817075
3.230109	212.284602	4.822080
3.398121	216.538933	4.827085
2.743259	214.644650	4.832090
3.205594	207.236140	4.837094
2.842524	207.957077	4.842099
3.179035	222.517740	4.847104
3.396043	225.622358	4.852109
3.173243	222.616789	4.857114
2.828050	214.150790	4.862118
2.784709	223.316419	4.867123
2.949192	235.483663	4.872128
3.288337	222.279485	4.877133
3.054540	235.271186	4.882138
3.568253	220.878759	4.887142
3.280561	231.961661	4.892147
3.521387	222.996302	4.897152
3.314439	228.995256	4.902157
3.209232	221.985145	4.907162
3.507751	215.045051	4.912166
3.324676	224.504513	4.917171
3.608039	214.453721	4.922176
3.212599	225.063025	4.927181
3.070824	213.629462	4.932186
3.566535	218.743911	4.937190
3.248295	227.503101	4.942195
3.037349	224.786745	4.947200
3.331155	228.129336	4.952205
3.315699	223.088877	4.957210
3.461830	212.828504	4.962214
3.442980	221.645478	4.967219
3.523499	227.340253	4.972224
3.403631	218.155815	4.977229
3.188149	225.798045	4.982234
3.631800	222.764641	4.987238
3.202606	223.321872	4.992243
3.036620	223.458481	4.997248
3.566734	219.971863	5.002253
3.272205	225.231498	5.007258
3.532388	222.331060	5.012262
3.695592	229.560000	5.017267
3.726895	227.201387	5.022272
3.695706	228.345203	5.027277
3.258616	229.697747	5.032282
3.317226	218.362692	5.037286
3.174660	226.078989	5.042291
3.176564	230.454097	5.047296
3.860592	243.736327	5.052301
3.423342	247.765371	5.057306
3.809167	245.329411	5.062310
3.788988	255.949908	5.067315
3.755149	252.538435	5.072320
3.588359	247.638587	5.077325
3.272024	257.944536	5.082330
3.601398	243.501699	5.087334
3.772753	250.925527	5.092339
3.927765	249.256314	5.097344
3.773546	255.209103	5.102349
3.783646	249.835634	5.107354
3.953773	247.075761	5.112358
3.799593	249.950281	5.117363
3.759778	255.704928	5.122368
3.779912	259.403340	5.127373
3.782734	254.230315	5.132378
3.739837	252.436895	5.137382
3.841709	258.919276	5.142387
4.116278	251.672856	5.147392
3.842770	248.311355	5.152397
3.672646	250.723296	5.157402
3.749874	251.217498	5.162406
3.928204	255.188664	5.167411
3.933992	252.868820	5.172416
4.205720	250.235494	5.177421
3.517529	248.147084	5.182426
3.836135	247.955149	5.187430
3.834934	246.329240	5.192435
4.007746	248.697278	5.197440
3.907471	249.605085	5.202445
4.198382	249.740158	5.207450
4.318058	252.110142	5.212454
4.205233	260.334340	5.217459
4.091894	256.302508	5.222464
3.860127	253.877284	5.227469
3.806162	254.936066	5.232474
4.083611	246.645185	5.237478
3.620199	255.003057	5.242483
3.939231	256.744066	5.247488
4.264158	257.838767	5.252493
3.748741	255.365959	5.257498
3.998895	265.454001	5.262502
4.087424	272.055521	5.267507
4.342706	270.604807	5.272512
4.545636	269.728544	5.277517
4.287605	279.762841	5.282522
4.068955	252.601883	5.287526
4.030357	265.563215	5.292531
4.351162	261.833938	5.297536
4.631487	277.785925	5.302541
4.010256	267.113497	5.307546
3.959237	260.996583	5.312550
4.175825	272.440748	5.317555
4.368684	279.709383	5.322560
4.475323	266.373697	5.327565
4.413203	275.387256	5.332570
4.434000	264.260535	5.337574
4.215713	277.509275	5.342579
4.376268	276.111273	5.347584
4.768643	279.647331	5.352589
4.561508	271.877966	5.357594
4.068791	263.640552	5.362598
4.389105	275.460866	5.367603
4.384188	275.268683	5.372608
4.419208	271.261204	5.377613
4.294425	274.906254	5.382618
4.383177	274.417919	5.387622
4.654116	273.363392	5.392627
4.385427	269.146941	5.397632
4.498450	268.540935	5.402637
4.353983	277.485060	5.407642
4.678579	273.030706	5.412646
4.665297	276.712178	5.417651
4.096998	267.730409	5.422656
4.732871	276.628966	5.427661
4.560185	272.808846	5.432666
4.417890	276.124436	5.437670
4.427085	280.273798	5.442675
4.578805	279.190377	5.447680
4.597562	278.785705	5.452685
4.622734	279.262703	5.457690
4.856279	266.865855	5.462694
4.565610	281.755166	5.467699
4.502992	275.481869	5.472704
4.692391	271.886942	5.477709
4.128328	285.714696	5.482714
4.253315	280.035434	5.487718
4.833155	284.231989	5.492723
4.926558	298.653399	5.497728
4.920895	290.096536	5.502733
5.006432	274.615984	5.507738
4.881267	278.808411	5.512742
4.517616	279.399730	5.517747
4.792111	285.801462	5.522752
4.974103	284.381140	5.527757
4.560878	279.348813	5.532762
5.191664	280.854628	5.537766
4.775446	284.807641	5.542771
4.816373	274.557285	5.547776
4.796732	278.100546	5.552781
4.632017	287.690057	5.557786
4.849271	293.091487	5.562790
5.030917	302.003832	5.567795
5.390821	299.995835	5.572800
5.049908	294.104376	5.577805
4.705159	289.456846	5.582810
5.277486	277.614672	5.587814
4.896780	290.246480	5.592819
5.108366	281.057859	5.597824
4.608410	282.154444	5.602829
5.173965	296.068915	5.607834
5.106236	295.731491	5.612838
4.914072	295.299548	5.617843
4.831132	295.173296	5.622848
5.119977	291.303459	5.627853
4.896537	303.287545	5.632858
5.351918	295.655458	5.637862
5.349059	302.916611	5.642867
5.164370	295.460110	5.647872
5.102860	290.398329	5.652877
4.839936	301.217995	5.657882
5.025523	302.891203	5.662886
5.053500	302.045341	5.667891
4.935180	302.832577	5.672896
5.103577	300.104603	5.677901
4.913806	304.313422	5.682906
5.196687	299.087289	5.687910
5.513131	301.939161	5.692915
5.127529	303.150819	5.697920
5.433718	298.231098	5.702925
5.159851	292.370329	5.707930
5.377397	298.689185	5.712934
5.375370	307.285287	5.717939
5.271370	302.356666	5.722944
5.225003	297.004629	5.727949
5.414820	298.787906	5.732954
5.217395	297.736699	5.737958
4.870736	300.337481	5.742963
5.048338	311.553628	5.747968
5.212346	304.748336	5.752973
5.014228	306.582523	5.757978
5.271599	317.023804	5.762982
5.515513	334.882891	5.767987
5.139116	324.112199	5.772992
5.863569	323.834929	5.777997
5.822368	323.575630	5.783002
5.578649	313.768195	5.788006
5.236763	318.604968	5.793011
5.426407	319.021559	5.798016
5.530578	320.264527	5.803021
5.444234	326.731945	5.808026
5.664160	321.863614	5.813030
5.533688	330.027317	5.818035
5.193960	327.549291	5.823040
5.669043	322.296390	5.828045
5.405480	322.609540	5.833050
5.758110	314.582163	5.838054
5.723604	326.644414	5.843059
5.556019	337.901667	5.848064
5.951506	321.721094	5.853069
5.724115	327.463841	5.858074
5.767390	327.944349	5.863078
5.790441	332.237097	5.868083
5.874534	318.572694	5.873088
5.592782	304.054118	5.878093
5.496978	306.517769	5.883098
5.662365	317.096756	5.888102
5.594742	327.901849	5.893107
5.565649	327.852632	5.898112
5.628668	321.199097	5.903117
5.467992	326.779599	5.908122
5.612636	320.138665	5.913126
5.488079	322.901018	5.918131
5.713990	320.844280	5.923136
5.793029	317.503804	5.928141
5.413280	327.360930	5.933146
5.835669	324.653516	5.938150
5.644576	330.219774	5.943155
5.884521	323.450107	5.948160
5.889914	325.562652	5.953165
5.768001	324.107388	5.958170
6.043028	335.447584	5.963174
6.184134	341.882759	5.968179
5.840432	323.567884	5.973184
6.074308	311.155135	5.978189
5.672997	325.568172	5.983194
6.047247	329.581617	5.988198
6.233478	330.397365	5.993203
6.225914	326.285774	5.998208
5.892219	325.021668	6.003213
5.685717	326.053585	6.008218
5.818997	327.143327	6.013222
5.970152	337.904873	6.018227
5.792377	345.329316	6.023232
6.312313	340.360485	6.028237
6.049535	349.386341	6.033242
5.804790	333.273803	6.038246
5.909307	326.968138	6.043251
5.977786	339.390842	6.048256
6.394940	342.869272	6.053261
5.746677	338.686593	6.058266
5.822510	334.685400	6.063270
6.087069	340.822948	6.068275
5.761886	353.604342	6.073280
6.402315	338.831428	6.078285
5.809781	340.173381	6.083290
6.441490	343.270398	6.088294
5.924347	344.667051	6.093299
5.896790	327.834179	6.098304
6.220630	321.038796	6.103309
5.950856	327.129822	6.108314
5.728004	327.651765	6.113318
5.835548	333.076616	6.118323
5.665802	340.942724	6.123328
6.441622	343.134632	6.128333
6.005983	345.214609	6.133338
5.927045	334.941753	6.138342
6.155198	336.117963	6.143347
5.968426	322.328053	6.148352
6.397626	326.997318	6.153357
5.844022	343.038075	6.158362
6.152192	329.658308	6.163366
5.990269	338.162264	6.168371
6.177516	330.302997	6.173376
6.000000	330.355982	6.178381
5.346726	327.411091	6.183386
5.785913	336.314992	6.188390
5.940215	334.354822	6.193395
6.017036	347.662068	6.198400
6.236610	339.427611	6.203405
6.174107	336.349609	6.208410
6.230562	333.395454	6.213414
6.347296	328.369184	6.218419
5.824213	327.719849	6.223424
6.165337	325.135817	6.228429
6.095605	333.732983	6.233434
6.096301	334.954098	6.238438
6.054802	329.506383	6.243443
6.122703	339.227380	6.248448
6.114541	330.740488	6.253453
5.856885	333.378036	6.258458
5.757868	324.911619	6.263462
5.868482	329.124295	6.268467
5.951629	340.279238	6.273472
6.346161	338.436685	6.278477
5.951893	336.622035	6.283482
5.894745	327.978258	6.288486
5.927491	331.519700	6.293491
5.963287	331.102883	6.298496
5.929769	338.618756	6.303501
6.004940	335.512992	6.308506
6.008456	336.879199	6.313510
6.136267	332.838277	6.318515
6.055337	336.834009	6.323520
6.107200	328.280825	6.328525
6.005961	328.970492	6.333530
5.973999	322.233669	6.338534
6.391550	333.061300	6.343539
5.869472	329.757467	6.348544
6.234211	331.795082	6.353549
6.022074	327.383154	6.358554
6.119748	334.979838	6.363558
5.994753	332.832203	6.368563
6.273504	333.298195	6.373568
6.093089	328.220115	6.378573
5.693373	325.732447	6.383578
6.098546	324.675999	6.388582
6.055099	325.052953	6.393587
6.462296	330.234999	6.398592
5.859826	312.023699	6.403597
5.515295	311.653443	6.408602
5.710667	315.397347	6.413606
6.143508	320.711436	6.418611
6.040927	330.727887	6.423616
6.269213	318.353968	6.428621
5.956819	326.552322	6.433626
5.990391	315.372961	6.438630
5.726126	312.804095	6.443635
5.823937	324.409153	6.448640
5.971854	325.578873	6.453645
6.462548	328.530167	6.458650
5.914767	324.996223	6.463654
5.893132	327.600187	6.468659
5.838873	336.745428	6.473664
5.742647	333.194960	6.478669
5.797084	341.991092	6.483674
5.920288	327.880838	6.488678
5.907971	327.275363	6.493683
5.988522	333.122024	6.498688
6.044189	333.458236	6.503693
5.595396	340.421846	6.508698
5.745438	336.696995	6.513702
5.989947	338.370523	6.518707
5.787240	342.309288	6.523712
5.857003	330.738311	6.528717
5.748860	334.953412	6.533722
6.054740	331.938276	6.538726
5.767052	331.862884	6.543731
5.434019	341.706417	6.548736
5.576765	341.646265	6.553741
5.868886	355.435678	6.558746
6.398231	345.147201	6.563750
6.147644	351.431397	6.568755
6.038993	358.803955	6.573760
6.343133	343.415855	6.578765
5.895863	346.690358	6.583770
5.870222	341.664105	6.588774
5.903981	338.466714	6.593779
5.449074	338.591361	6.598784
5.984682	348.983013	6.603789
6.143114	354.833374	6.608794
6.316868	349.965896	6.613798
6.001067	336.911061	6.618803
6.068549	350.254564	6.623808
5.906904	338.061562	6.628813
6.077045	342.347230	6.633818
5.918896	327.018466	6.638822
6.153005	334.922932	6.643827
5.747085	329.414898	6.648832
5.966859	332.136297	6.653837
6.114973	345.979762	6.658842
6.399516	338.076869	6.663846
6.138317	332.587430	6.668851
5.750390	338.016660	6.673856
6.062399	330.887763	6.678861
5.820639	328.087605	6.683866
5.942006	336.291194	6.688870
6.049253	330.953194	6.693875
5.469428	330.233601	6.698880
6.204892	338.360560	6.703885
6.195562	348.707345	6.708890
6.023973	336.262797	6.713894
6.006358	336.825551	6.718899
5.778482	338.610592	6.723904
5.744928	330.985015	6.728909
5.889339	344.522176	6.733914
6.057939	340.104749	6.738918
6.157147	347.419630	6.743923
6.264732	351.262630	6.748928
6.144574	338.797418	6.753933
5.775506	333.720236	6.758938
5.924575	321.013805	6.763942
5.726344	326.929179	6.768947
6.145198	349.933688	6.773952
6.100678	338.744325	6.778957
5.858734	337.168546	6.783962
5.767179	340.988766	6.788966
6.092868	340.564778	6.793971
5.971570	348.163923	6.798976
6.024264	347.162354	6.803981
6.030044	352.571418	6.808986
5.816750	347.903405	6.813990
6.170154	355.469772	6.818995
6.029627	361.461593	6.824000
6.119011	356.069421	6.829005
5.726788	351.666543	6.834010
5.884367	342.508445	6.839014
6.413093	351.670491	6.844019
5.738059	356.033969	6.849024
5.976476	344.822696	6.854029
5.820366	345.770839	6.859034
5.953221	351.780202	6.864038
6.238336	353.444246	6.869043
5.688207	355.893220	6.874048
6.161809	345.676696	6.879053
6.002171	367.607055	6.884058
6.053413	360.724388	6.889062
5.956135	347.493155	6.894067
5.825867	347.750752	6.899072
6.192929	347.927752	6.904077
6.010481	358.700123	6.909082
5.804232	337.586102	6.914086
5.888058	349.095279	6.919091
5.848432	359.184200	6.924096
6.135686	353.356266	6.929101
6.314999	360.294855	6.934106
6.141522	350.340425	6.939110
5.771206	335.117453	6.944115
5.946942	341.281485	6.949120
6.128527	344.749137	6.954125
5.868408	342.885126	6.959130
5.905547	341.069745	6.964134
5.800381	339.115172	6.969139
5.907535	347.890444	6.974144
6.142663	351.827480	6.979149
6.077063	358.158804	6.984154
6.180310	349.894998	6.989158
5.812018	336.838844	6.994163
5.479805	354.252987	6.999168
5.971918	348.149555	7.004173
6.000537	362.729797	7.009178
6.372283	359.324758	7.014182
6.015694	364.211287	7.019187
6.002593	366.674725	7.024192
6.128749	352.443771	7.029197
6.144089	345.803977	7.034202
5.914526	335.535589	7.039206
6.018332	329.796336	7.044211
5.748010	342.983625	7.049216
6.017206	333.849281	7.054221
6.182276	353.846667	7.059226
5.808560	343.281186	7.064230
6.149277	339.583594	7.069235
5.855823	346.326871	7.074240
6.165272	339.818454	7.079245
5.776995	340.163677	7.084250
6.049571	348.049504	7.089254
6.138014	342.182927	7.094259
5.552384	348.788201	7.099264
5.959296	345.539038	7.104269
5.830970	364.623517	7.109274
6.077948	364.142181	7.114278
6.072080	361.779846	7.119283
6.093616	358.603336	7.124288
6.224895	358.981560	7.129293
5.980066	352.034264	7.134298
5.888654	349.141092	7.139302
6.018534	349.317057	7.144307
6.073105	346.489740	7.149312
6.188915	338.382168	7.154317
5.862282	337.351076	7.159322
5.749719	336.691607	7.164326
5.874260	344.546698	7.169331
6.105049	352.233393	7.174336
6.406503	351.645502	7.179341
5.776716	340.718101	7.184346
5.610491	338.114986	7.189350
6.032683	346.300215	7.194355
5.655682	351.303812	7.199360
6.227048	349.531801	7.204365
6.063153	357.479262	7.209370
5.946900	358.845135	7.214374
6.401020	359.739396	7.219379
5.937679	355.303299	7.224384
6.211518	331.953730	7.229389
5.910845	333.639375	7.234394
5.850392	340.602632	7.239398
5.889893	333.848351	7.244403
6.082558	345.792988	7.249408
5.954004	336.407365	7.254413
6.033740	343.241230	7.259418
6.273358	340.340812	7.264422
6.426781	322.998884	7.269427
5.744803	334.823434	7.274432
6.091498	333.526158	7.279437
5.747923	335.525362	7.284442
5.852284	332.532111	7.289446
6.295931	327.590981	7.294451
5.996716	336.429518	7.299456
6.130501	327.294114	7.304461
6.070171	325.870390	7.309466
5.729686	326.404320	7.314470
5.763034	334.526702	7.319475
5.968539	338.360781	7.324480
6.388233	333.973861	7.329485
6.424408	338.372133	7.334490
5.866260	338.645729	7.339494
5.874174	328.216988	7.344499
5.820861	335.900454	7.349504
6.253018	325.870725	7.354509
5.894399	325.603900	7.359514
5.967172	328.367168	7.364518
6.268469	335.590469	7.369523
6.238116	339.132246	7.374528
6.564266	327.290403	7.379533
6.363964	333.917933	7.384538
6.287472	333.964680	7.389542
6.179036	319.267250	7.394547
5.742515	312.615565	7.399552
5.951498	308.849906	7.404557
6.001344	319.972057	7.409562
5.763342	323.368994	7.414566
5.844493	323.514580	7.419571
5.666391	334.381171	7.424576
5.834795	327.999121	7.429581
6.168208	330.981231	7.434586
6.205019	332.177741	7.439590
6.090651	320.774642	7.444595
5.931626	328.623258	7.449600
6.080895	326.660708	7.454605
5.898639	331.906057	7.459610
5.860599	337.109971	7.464614
6.077883	328.527868	7.469619
5.997064	343.014404	7.474624
5.618783	328.937937	7.479629
6.189554	334.138808	7.484634
6.005586	334.025121	7.489638
6.140834	335.035465	7.494643
6.135213	328.750112	7.499648
6.224993	327.280870	7.504653
6.084711	334.496994	7.509658
5.883200	326.188901	7.514662
6.095232	318.895244	7.519667
6.143161	323.566924	7.524672
6.080601	312.462642	7.529677
5.916152	314.019511	7.534682
5.616309	308.045724	7.539686
5.994808	318.556730	7.544691
5.737644	331.567958	7.549696
6.024401	329.090465	7.554701
5.740064	331.526527	7.559706
5.693627	336.383741	7.564710
6.045291	324.718259	7.569715
5.753387	333.289905	7.574720
5.783499	332.671496	7.579725
5.777569	320.577647	7.584730
5.950440	329.260422	7.589734
5.903622	327.379022	7.594739
5.865203	341.482475	7.599744
6.182479	328.746687	7.604749
5.891537	336.252019	7.609754
5.900526	336.956161	7.614758
5.834052	333.894597	7.619763
5.765669	329.722874	7.624768
6.052987	333.193043	7.629773
6.003184	341.568815	7.634778
6.087839	336.636120	7.639782
6.309824	334.507227	7.644787
5.855632	339.842373	7.649792
6.298198	327.419266	7.654797
6.180822	331.673767	7.659802
5.855503	335.299433	7.664806
5.995197	323.347421	7.669811
6.002859	332.704478	7.674816
6.063687	335.574008	7.679821
5.818394	333.628598	7.684826
5.797906	325.368249	7.689830
5.863189	330.040392	7.694835
5.780214	333.840293	7.699840
5.891723	328.121986	7.704845
5.963119	332.780523	7.709850
5.820548	335.147057	7.714854
6.176270	334.006561	7.719859
6.057339	336.015081	7.724864
6.115286	335.648597	7.729869
6.043168	332.303180	7.734874
5.936043	330.412186	7.739878
6.062523	330.316602	7.744883
5.720248	331.002669	7.749888
5.846306	337.965359	7.754893
5.569549	340.026925	7.759898
5.749504	339.894541	7.764902
6.279294	339.429284	7.769907
6.151074	347.374350	7.774912
6.308985	337.339858	7.779917
5.950984	341.622335	7.784922
5.839013	341.494275	7.789926
5.771798	334.130197	7.794931
5.747457	340.860045	7.799936
6.063689	334.711236	7.804941
6.040898	334.699002	7.809946
5.877473	334.635900	7.814950
6.140334	336.885527	7.819955
5.870184	346.728764	7.824960
5.925045	348.463457	7.829965
5.984160	343.189894	7.834970
6.162457	344.661764	7.839974
5.989764	339.351529	7.844979
5.921875	342.547980	7.849984
5.885580	333.761751	7.854989
5.934841	346.054577	7.859994
6.062012	354.004174	7.864998
5.901692	346.445783	7.870003
6.044534	352.409300	7.875008
5.935891	354.836992	7.880013
6.054642	352.417290	7.885018
5.937999	352.849933	7.890022
6.041248	354.437890	7.895027
5.788448	352.506302	7.900032
6.190873	348.805427	7.905037
6.130398	352.171565	7.910042
6.078408	341.780616	7.915046
5.867225	333.961235	7.920051
5.644606	344.088130	7.925056
6.237635	350.838916	7.930061
5.941408	348.344623	7.935066
6.019000	351.967671	7.940070
6.143090	345.083158	7.945075
5.871140	345.884824	7.950080
5.847518	331.895502	7.955085
6.143287	353.387950	7.960090
5.782831	347.584936	7.965094
6.340636	344.008564	7.970099
5.996738	347.298609	7.975104
6.187134	339.141459	7.980109
5.955859	346.438193	7.985114
6.042719	323.168366	7.990118
5.875299	328.363004	7.995136
5.944735	342.981717	8.000154
6.054471	337.691614	8.005171
5.770554	346.290763	8.010189
5.833856	346.675397	8.015206
6.183192	348.804739	8.020224
6.163444	350.732785	8.025242
5.991350	337.641669	8.030259
5.833786	335.242716	8.035277
6.008663	346.061418	8.040294
6.060788	343.797064	8.045312
6.101485	352.632838	8.050330
5.957456	338.978804	8.055347
6.161346	350.329448	8.060365
6.147280	343.670142	8.065382
6.111575	342.463977	8.070400
5.958282	347.549509	8.075418
5.880450	337.634058	8.080435
6.033126	355.669988	8.085453
6.260829	354.870909	8.090470
6.419456	350.106492	8.095488
5.840576	353.876123	8.100506
5.952006	346.695532	8.105523
6.235352	341.892765	8.110541
5.919750	347.612604	8.115558
6.577279	340.719354	8.120576
5.993622	351.050279	8.125594
6.181994	344.283719	8.130611
6.192084	338.680945	8.135629
6.217116	343.372659	8.140646
6.573869	338.148232	8.145664
6.363105	344.694300	8.150682
6.248945	339.473768	8.155699
6.300354	342.914902	8.160717
5.940514	339.446129	8.165734
5.978697	338.136946	8.170752
6.217987	350.921045	8.175770
5.908635	337.087637	8.180787
5.823453	341.017071	8.185805
5.747393	339.952881	8.190822
6.242075	345.455048	8.195840
6.219156	362.271850	8.200858
6.274304	363.364616	8.205875
6.390031	351.863294	8.210893
6.142928	357.572471	8.215910
6.273703	339.697597	8.220928
6.218503	357.819540	8.225946
6.451537	347.855683	8.230963
6.071275	338.211368	8.235981
6.091136	344.910866	8.240998
6.579117	349.710373	8.246016
6.278297	347.021316	8.251034
6.037093	340.933832	8.256051
6.009954	345.248683	8.261069
6.231475	365.148347	8.266086
6.261298	356.408952	8.271104
6.265434	364.852815	8.276122
6.051147	357.502038	8.281139
6.262029	364.272782	8.286157
6.407481	367.052374	8.291174
6.573517	367.771289	8.296192
6.267262	366.550444	8.301210
6.525609	370.072966	8.306227
6.608362	352.499030	8.311245
5.967142	350.585611	8.316262
6.308437	352.126102	8.321280
6.698598	359.373832	8.326298
6.120091	351.495974	8.331315
6.335644	348.710741	8.336333
6.212490	357.846567	8.341350
6.210949	353.492074	8.346368
6.225715	361.833300	8.351386
6.420029	361.774682	8.356403
6.679456	362.068823	8.361421
6.543331	359.745420	8.366438
6.428833	346.866224	8.371456
6.038394	348.388107	8.376474
6.268853	353.189842	8.381491
6.730444	352.856094	8.386509
6.520643	362.819566	8.391526
6.316841	343.687193	8.396544
6.483629	353.803454	8.401562
6.478125	355.666169	8.406579
6.430959	338.914004	8.411597
6.209169	329.046217	8.416614
6.436582	349.771720	8.421632
6.457601	350.519524	8.426650
6.510950	360.552470	8.431667
6.536570	361.930685	8.436685
6.079844	356.687750	8.441702
6.532473	358.034192	8.446720
6.705052	364.047237	8.451738
6.240172	361.005046	8.456755
6.741407	354.044611	8.461773
6.294658	358.765605	8.466790
6.666847	362.418715	8.471808
6.338283	360.721688	8.476826
6.277395	358.806270	8.481843
6.475497	359.078404	8.486861
6.078276	354.930675	8.491878
6.488085	357.501858	8.496896
6.180777	365.224237	8.501914
6.611248	362.588567	8.506931
6.487828	354.516782	8.511949
6.098760	361.204220	8.516966
6.522519	359.809758	8.521984
6.353993	362.663479	8.527002
6.286058	363.087481	8.532019
6.694516	363.658204	8.537037
6.503899	364.533629	8.542054
6.590004	367.824206	8.547072
6.495937	370.716826	8.552090
6.350065	370.149471	8.557107
6.364041	363.826600	8.562125
6.410211	380.525372	8.567143
6.669318	384.451700	8.572160
7.078171	386.158391	8.577178
6.811142	377.648233	8.582195
6.690000	367.799465	8.587213
6.486467	375.057591	8.592231
6.770687	370.216813	8.597248
6.658431	360.546537	8.602266
6.257835	363.789822	8.607283
6.519654	359.299654	8.612301
6.304147	375.546884	8.617319
6.502169	372.988427	8.622336
6.796381	382.999663	8.627354
6.530909	389.115632	8.632371
6.853653	387.796853	8.637389
6.755030	387.190584	8.642407
6.719780	381.440230	8.647424
7.279150	390.072197	8.652442
6.978112	384.612519	8.657459
6.759786	363.753097	8.662477
6.407100	360.078090	8.667495
6.583122	365.831838	8.672512
6.879195	364.640283	8.677530
6.730681	363.372789	8.682547
6.832565	363.104512	8.687565
6.872020	361.602637	8.692583
6.476014	353.740541	8.697600
6.688493	356.888371	8.702618
6.692223	350.756438	8.707635
6.763958	347.952574	8.712653
6.463870	361.325560	8.717671
6.868516	372.941591	8.722688
7.057316	372.158035	8.727706
6.858400	367.190520	8.732723
6.938285	364.543166	8.737741
6.674518	360.194787	8.742759
6.679304	371.185146	8.747776
6.384521	360.268413	8.752794
6.420963	376.119830	8.757811
6.686701	382.598033	8.762829
6.639924	382.592730	8.767847
6.831468	388.931018	8.772864
6.927869	387.230935	8.777882
7.028391	386.906069	8.782899
6.822518	382.816899	8.787917
6.952739	391.480971	8.792935
6.865481	381.396559	8.797952
6.880094	384.912854	8.802970
6.976505	390.246683	8.807987
7.067788	385.319182	8.813005
7.189185	387.269434	8.818023
6.981008	385.862914	8.823040
7.293735	382.567111	8.828058
6.538925	366.549913	8.833075
6.832622	357.715789	8.838093
6.798069	375.790356	8.843111
7.226060	381.321852	8.848128
7.063482	365.439653	8.853146
6.831201	369.499286	8.858163
6.674486	361.981762	8.863181
6.948025	374.230399	8.868199
7.211417	377.707959	8.873216
7.100308	362.325806	8.878234
6.750106	370.777505	8.883251
7.012418	360.815393	8.888269
7.052264	368.789820	8.893287
6.524952	363.024570	8.898304
7.014413	376.407174	8.903322
6.707758	385.388559	8.908339
7.060222	388.530377	8.913357
6.994356	391.011533	8.918375
7.223732	395.630421	8.923392
7.025237	389.605695	8.928410
6.693128	397.347728	8.933427
7.111829	399.876509	8.938445
7.064060	395.014834	8.943463
6.852876	393.211171	8.948480
7.496791	384.489754	8.953498
7.417717	398.639355	8.958515
7.045128	379.631048	8.963533
6.687951	381.946130	8.968551
7.150552	381.728982	8.973568
7.295708	378.904215	8.978586
6.960116	387.842772	8.983603
6.984598	376.964678	8.988621
7.253674	383.180444	8.993639
6.900304	388.350785	8.998656
7.145502	386.971500	9.003674
7.093872	381.924247	9.008691
7.334997	382.921790	9.013709
7.390461	373.550424	9.018727
7.154806	370.466230	9.023744
7.128400	348.737546	9.028762
6.548891	366.799128	9.033779
6.567894	373.716509	9.038797
6.818686	383.374763	9.043815
6.750886	381.817006	9.048832
7.017401	378.408485	9.053850
6.794394	378.238127	9.058867
7.007436	387.315313	9.063885
6.831634	390.615116	9.068903
6.741802	393.585971	9.073920
7.400232	403.490021	9.078938
7.058854	410.106939	9.083955
7.918942	409.714301	9.088973
7.376782	402.225215	9.093991
7.307300	395.483005	9.099008
7.242011	385.483527	9.104026
7.206659	382.289254	9.109043
6.930152	387.179398	9.114061
7.297695	394.998679	9.119079
7.110236	397.249472	9.124096
7.575219	397.827174	9.129114
7.380502	397.068618	9.134131
7.162557	383.356635	9.139149
7.228094	385.041044	9.144167
7.392631	394.103696	9.149184
7.178948	379.346537	9.154202
7.360397	390.915284	9.159219
7.248685	387.423646	9.164237
7.385772	384.922009	9.169255
7.128948	394.040798	9.174272
7.482034	394.232001	9.179290
7.354648	401.569795	9.184307
7.217665	397.542476	9.189325
7.694282	388.531541	9.194343
7.390426	393.407011	9.199360
7.184995	388.005027	9.204378
7.153522	392.866488	9.209395
7.287675	404.354250	9.214413
7.472672	404.126678	9.219431
7.796502	416.667300	9.224448
7.742067	388.379199	9.229466
7.364615	386.147012	9.234483
7.441542	385.141046	9.239501
7.657266	373.254932	9.244519
7.292286	391.172690	9.249536
7.427425	383.164771	9.254554
7.355025	382.898384	9.259571
7.032500	393.270723	9.264589
7.252741	379.187578	9.269607
7.318782	394.185538	9.274624
7.791553	396.286200	9.279642
7.419940	392.847649	9.284659
7.305696	395.487808	9.289677
7.471537	398.737576	9.294695
7.622094	404.558414	9.299712
7.398444	399.474826	9.304730
7.606083	396.706597	9.309747
7.471441	394.408203	9.314765
7.088511	391.593075	9.319783
7.114139	403.640503	9.324800
7.197542	409.771584	9.329818
7.292610	416.935902	9.334835
7.400443	403.485589	9.339853
7.905980	406.092365	9.344871
7.453551	411.054085	9.349888
7.862376	404.701279	9.354906
7.880672	411.751322	9.359923
7.608790	405.678060	9.364941
7.939506	412.783597	9.369959
7.710803	413.103249	9.374976
7.531669	401.054544	9.379994
7.183776	404.460035	9.385011
7.525016	412.100392	9.390029
7.556569	409.946525	9.395047
6.956673	415.350906	9.400064
7.447300	412.298785	9.405082
7.532873	416.441477	9.410099
7.480412	407.285702	9.415117
7.386170	405.397562	9.420135
7.339333	416.197180	9.425152
7.637871	408.368926	9.430170
7.590729	409.947812	9.435187
7.735402	419.628919	9.440205
7.791036	417.398722	9.445223
7.952356	419.860288	9.450240
7.668091	411.412753	9.455258
7.584196	409.346286	9.460275
7.514646	415.990307	9.465293
7.889917	414.982068	9.470311
7.455853	423.604632	9.475328
7.786102	412.622108	9.480346
7.597454	410.411012	9.485363
7.744086	421.303581	9.490381
7.910701	416.809288	9.495399
7.826430	416.989694	9.500416
7.991101	416.383454	9.505434
7.686350	415.995461	9.510451
7.337719	414.465647	9.515469
7.703711	413.846996	9.520487
7.522148	418.409958	9.525504
7.982873	425.583616	9.530522
7.691523	425.108334	9.535539
7.514258	426.631745	9.540557
7.724326	427.126067	9.545575
8.002198	442.892619	9.550592
7.721189	440.329845	9.555610
7.929798	440.108063	9.560627
7.859436	444.101480	9.565645
7.809699	444.885549	9.570663
8.404200	448.229524	9.575680
8.162749	435.363718	9.580698
7.595440	422.179447	9.585715
7.448681	419.750399	9.590733
7.841558	421.784613	9.595751
7.904526	440.576172	9.600768
8.338261	445.526155	9.605786
8.239044	434.780888	9.610803
7.633472	430.801274	9.615821
7.847327	412.821877	9.620839
7.475473	423.542723	9.625856
7.863986	434.732139	9.630874
8.059053	434.667092	9.635891
8.111805	439.057885	9.640909
8.199230	429.880318	9.645927
7.976313	423.329235	9.650944
7.626525	414.708874	9.655962
8.239963	428.476136	9.660979
7.890175	429.045004	9.665997
7.799435	416.947813	9.671015
7.712481	432.111629	9.676032
7.736339	443.638678	9.681050
8.303300	437.949170	9.686067
7.842273	452.625318	9.691085
8.016672	440.682480	9.696103
8.151877	435.322115	9.701120
7.838875	434.338989	9.706138
8.155865	440.471580	9.711155
7.971517	449.534934	9.716173
7.963022	440.924535	9.721191
8.094156	441.140828	9.726208
7.929531	445.593868	9.731226
8.254176	437.698423	9.736243
7.764795	445.184111	9.741261
8.388929	441.407489	9.746279
8.055450	445.688013	9.751296
7.938656	444.024275	9.756314
8.171166	442.164147	9.761331
7.916376	444.434895	9.766349
8.214174	441.722045	9.771367
8.078783	445.836035	9.776384
8.015422	441.598437	9.781402
8.531170	437.463170	9.786419
8.170621	441.814176	9.791437
8.234015	445.436491	9.796455
8.245341	455.100512	9.801472
8.141834	440.752160	9.806490
8.386488	444.311542	9.811507
8.151777	442.969105	9.816525
8.499476	445.600461	9.821543
8.415313	441.719534	9.826560
8.027443	438.308751	9.831578
8.277017	434.805032	9.836595
8.120386	441.434221	9.841613
8.613557	435.437482	9.846631
8.043210	437.943544	9.851648
8.289880	431.912606	9.856666
8.104338	422.846968	9.861683
7.995010	434.461016	9.866701
8.334561	435.436926	9.871719
8.143914	444.488636	9.876736
8.252797	447.106685	9.881754
8.712782	443.794255	9.886771
8.475190	451.206030	9.891789
8.447252	434.251976	9.896807
8.031684	421.053547	9.901824
8.465565	431.696282	9.906842
8.320310	419.206811	9.911859
7.896214	428.623047	9.916877
8.310299	427.350000	9.921895
8.312951	441.325973	9.926912
7.715284	450.387412	9.931930
8.156935	448.693527	9.936947
7.879334	447.433503	9.941965
7.983567	444.176462	9.946983
8.470946	442.923560	9.952000
8.459266	444.317055	9.957018
8.425691	445.474130	9.962035
8.255584	445.289224	9.967053
8.143501	446.811955	9.972071
8.291930	447.060267	9.977088
8.265560	460.308664	9.982106
8.548885	447.859736	9.987123
8.226496	463.300064	9.992141
8.526162	461.767133	9.997159
8.867475	460.716843	10.002176
8.387069	460.078501	10.007194
8.670662	443.034910	10.012211
8.231237	448.272313	10.017229
8.386023	459.100523	10.022247
8.487360	461.634546	10.027264
8.685335	462.168620	10.032282
8.715234	459.904557	10.037299
8.345378	451.025383	10.042317
8.544381	456.340104	10.047335
8.659929	449.259810	10.052352
8.070483	448.076741	10.057370
8.465598	456.535508	10.062387
8.523137	455.838655	10.067405
8.343155	458.306030	10.072423
8.519412	467.224890	10.077440
8.543753	466.886638	10.082458
8.814618	459.911540	10.087475
8.508641	462.401689	10.092493
8.589812	451.199159	10.097511
8.895301	461.315975	10.102528
8.663979	467.300428	10.107546
8.822533	464.609254	10.112563
8.834604	460.602892	10.117581
8.596048	456.477771	10.122599
8.653116	453.729820	10.127616
8.437678	446.540123	10.132634
8.770695	461.013757	10.137651
8.699378	463.710355	10.142669
8.501227	471.955401	10.147687
9.025441	459.225975	10.152704
8.416037	462.479699	10.157722
8.855123	465.491285	10.162739
8.349626	471.650964	10.167757
8.613643	462.556334	10.172775
8.572975	459.094645	10.177792
8.867660	464.104150	10.182810
8.502330	459.209854	10.187827
8.558700	469.400174	10.192845
8.466761	470.597894	10.197863
8.593628	467.166920	10.202880
8.426584	470.900854	10.207898
8.824987	467.869394	10.212915
8.635363	472.951151	10.217933
8.713860	469.874829	10.222951
8.666968	473.943490	10.227968
8.321283	477.203491	10.232986
9.070255	477.434037	10.238003
8.634505	478.098337	10.243021
8.692188	486.944155	10.248039
8.780713	490.313270	10.253056
9.010919	491.994140	10.258074
8.988234	485.904141	10.263091
9.095910	495.209216	10.268109
9.144769	483.876003	10.273127
8.965135	480.732577	10.278144
8.691632	472.128711	10.283162
8.729368	472.141806	10.288179
9.164537	476.577203	10.293197
8.906191	474.847143	10.298215
8.957560	465.760375	10.303232
8.628996	476.663851	10.308250
8.769118	473.865098	10.313267
8.753770	488.150008	10.318285
9.004469	493.724921	10.323303
9.001942	497.969708	10.328320
8.895418	494.142742	10.333338
9.311639	485.611354	10.338355
9.060508	490.393439	10.343373
9.025214	490.073939	10.348391
9.164149	478.963378	10.353408
8.884486	473.916891	10.358426
8.839985	478.120873	10.363443
8.928397	484.065017	10.368461
9.077512	494.483896	10.373479
9.253829	489.606240	10.378496
9.056358	497.772301	10.383514
9.193926	483.411625	10.388531
8.880987	473.750444	10.393549
9.162420	489.238785	10.398567
9.025621	483.557855	10.403584
9.277874	495.642640	10.408602
9.101314	481.861025	10.413619
8.547245	479.804640	10.418637
8.480248	487.751575	10.423655
8.867797	486.981250	10.428672
9.081003	492.101275	10.433690
9.193742	499.830892	10.438707
9.147766	484.116616	10.443725
8.958584	486.389777	10.448743
9.564060	484.032940	10.453760
9.068146	487.480427	10.458778
9.223308	485.802743	10.463795
9.275373	491.995534	10.468813
9.030016	488.647755	10.473831
9.428915	488.046068	10.478848
9.196323	503.409336	10.483866
8.959433	491.249647	10.488883
9.230584	494.388366	10.493901
8.970677	491.932747	10.498919
9.118726	486.529342	10.503936
8.888854	490.894727	10.508954
8.923473	494.792918	10.513971
9.093491	497.171093	10.518989
9.126298	507.043227	10.524007
9.386247	512.496791	10.529024
9.330265	510.810955	10.534042
9.442145	511.923298	10.539059
9.536078	509.179066	10.544077
9.164438	507.283614	10.549095
9.282531	493.191038	10.554112
9.220834	511.910568	10.559130
8.996692	516.997712	10.564147
9.057784	516.675827	10.569165
9.385240	515.558267	10.574183
9.191785	512.057242	10.579200
9.012574	526.661173	10.584218
9.112888	517.137588	10.589235
9.097711	520.608057	10.594253
9.129903	523.588336	10.599271
9.586402	521.485052	10.604288
9.444930	525.148748	10.609306
9.878560	514.285759	10.614323
9.674592	518.347329	10.619341
9.339033	518.020932	10.624359
9.440391	515.385991	10.629376
9.550249	511.780939	10.634394
9.365644	516.653654	10.639411
9.373012	512.433428	10.644429
9.327160	518.483691	10.649447
9.385735	515.501977	10.654464
9.542616	520.431973	10.659482
9.571281	514.012092	10.664499
9.774691	521.200606	10.669517
9.395322	523.863129	10.674535
9.358471	514.903675	10.679552
9.147412	513.058956	10.684570
9.225134	523.287006	10.689587
9.745741	533.805852	10.694605
9.819159	543.239356	10.699623
10.133750	535.156094	10.704640
9.851617	526.499900	10.709658
9.515225	511.168472	10.714675
9.637536	514.926788	10.719693
9.737101	513.955159	10.724711
9.624893	512.306478	10.729728
9.773443	512.955542	10.734746
9.741229	514.809810	10.739763
9.537055	512.231906	10.744781
9.459517	516.898612	10.749799
9.520851	516.305302	10.754816
9.653240	526.622668	10.759834
9.707515	510.656085	10.764851
9.827194	504.932060	10.769869
9.341488	516.172437	10.774887
9.738388	514.226750	10.779904
9.894702	514.735755	10.784922
9.742214	505.384074	10.789939
9.822268	510.521680	10.794957
9.704035	514.724528	10.799975
9.605011	509.362741	10.804992
9.461006	521.086381	10.810010
9.571696	517.310794	10.815027
9.961273	530.440835	10.820045
9.616264	529.352239	10.825063
10.129890	532.248095	10.830080
9.706597	525.731327	10.835098
9.748213	519.694418	10.840115
9.791416	524.803053	10.845133
9.900458	535.225040	10.850151
10.244284	531.078651	10.855168
9.992051	517.330880	10.860186
9.966366	526.003513	10.865203
9.851275	510.457758	10.870221
9.779513	511.693363	10.875239
9.697953	507.092527	10.880256
9.410533	511.148155	10.885274
9.774857	529.476341	10.890291
9.632773	531.372962	10.895309
9.891002	534.712508	10.900327
9.940477	536.680286	10.905344
9.808939	543.772644	10.910362
9.654988	544.610811	10.915379
9.607590	537.937689	10.920397
9.590476	538.230711	10.925415
9.866666	534.927947	10.930432
9.714989	538.700526	10.935450
9.869884	534.779203	10.940467
10.132423	543.391191	10.945485
9.671841	541.354956	10.950503
10.393798	549.889106	10.955520
10.139754	544.251656	10.960538
9.736264	537.024933	10.965555
10.139154	545.542490	10.970573
9.920101	555.195099	10.975591
10.352371	554.534568	10.980608
10.728509	557.786335	10.985626
9.893847	541.159746	10.990643
10.237849	533.453741	10.995661
9.975800	541.689833	11.000679
10.186642	537.863936	11.005696
9.969448	541.233325	11.010714
10.052993	536.613086	11.015731
9.768348	531.911325	11.020749
10.120974	541.579056	11.025767
10.265646	549.556176	11.030784
10.105858	554.589132	11.035802
10.075418	555.032546	11.040819
10.359534	557.891559	11.045837
10.613536	564.131826	11.050855
10.275433	551.151603	11.055872
10.042853	539.559229	11.060890
10.041095	532.008040	11.065907
10.331922	541.319335	11.070925
10.071417	542.833626	11.075943
10.194567	550.684716	11.080960
10.597019	557.088051	11.085978
9.936839	558.232245	11.090995
10.455312	555.497643	11.096013
10.389801	553.633414	11.101031
10.233601	541.445349	11.106048
10.302230	551.482336	11.111066
10.215270	553.619674	11.116083
10.496537	549.568224	11.121101
10.454299	547.107108	11.126119
10.246544	536.514372	11.131136
10.293909	540.994387	11.136154
10.154798	553.398910	11.141171
10.115626	552.073355	11.146189
10.432559	560.891468	11.151207
10.385850	559.466105	11.156224
10.402866	559.886351	11.161242
10.451930	560.967454	11.166259
10.496011	550.856185	11.171277
10.476730	557.833245	11.176295
10.597917	559.994979	11.181312
10.971202	557.412364	11.186330
10.353602	539.432912	11.191347
10.238151	532.729363	11.196365
10.442283	544.032758	11.201383
10.582491	552.389254	11.206400
10.588819	555.379877	11.211418
10.615494	556.571757	11.216435
10.410601	558.635944	11.221453
10.452933	562.065911	11.226471
10.384638	552.521224	11.231488
10.750128	561.252886	11.236506
10.755156	567.699168	11.241523
10.736101	549.860034	11.246541
10.310889	551.239031	11.251559
10.678577	554.293306	11.256576
10.690361	553.638286	11.261594
10.406938	555.894572	11.266611
10.632913	556.424289	11.271629
10.844257	559.288322	11.276647
10.615432	563.480000	11.281664
10.514284	558.730728	11.286682
10.824241	571.459804	11.291699
10.773825	557.570130	11.296717
10.744878	553.746851	11.301735
10.211597	550.282950	11.306752
10.255703	562.346542	11.311770
10.249445	566.787578	11.316787
10.597764	555.578100	11.321805
10.308588	549.892472	11.326823
10.070168	558.314233	11.331840
10.407886	557.835674	11.336858
10.547259	583.037269	11.341875
10.909157	583.353329	11.346893
11.038030	582.752657	11.351911
10.912048	581.080869	11.356928
10.706936	575.887052	11.361946
10.526339	585.136076	11.366963
11.117904	575.135203	11.371981
11.186224	581.088819	11.376999
10.747072	571.235805	11.382016
10.606011	563.605310	11.387034
10.832412	569.480663	11.392051
11.174104	584.350661	11.397069
11.209881	573.536958	11.402087
10.864099	565.228310	11.407104
11.055832	561.578945	11.412122
10.608230	565.208264	11.417139
10.514094	571.439624	11.422157
11.044589	570.523968	11.427175
10.524619	577.408585	11.432192
10.835763	577.716768	11.437210
10.501071	583.988742	11.442227
10.945219	586.715551	11.447245
11.037658	587.815147	11.452263
11.219876	587.597473	11.457280
11.196710	588.023977	11.462298
11.248712	588.145299	11.467315
11.217789	592.760588	11.472333
11.331732	589.107550	11.477351
10.691325	568.010660	11.482368
10.750838	567.641685	11.487386
11.353454	575.932509	11.492403
11.144139	574.655532	11.497421
11.262353	581.481811	11.502439
10.886405	581.142767	11.507456
10.845631	575.541527	11.512474
10.846708	586.895498	11.517491
11.268559	580.363885	11.522509
10.926238	594.624053	11.527527
10.679642	581.569602	11.532544
10.855770	590.324450	11.537562
10.750676	593.894136	11.542579
10.594833	592.318511	11.547597
10.708328	597.040698	11.552615
11.192028	606.366177	11.557632
11.422090	614.323720	11.562650
11.089108	623.798453	11.567667
11.088086	618.620182	11.572685
11.486735	618.955766	11.577703
11.363323	620.051104	11.582720
11.433754	599.771271	11.587738
11.234515	602.064947	11.592755
11.363187	603.575452	11.597773
11.443625	592.344546	11.602791
11.026168	589.752503	11.607808
11.692798	586.919092	11.612826
11.006763	598.304315	11.617843
11.175303	596.375240	11.622861
11.324972	596.926306	11.627879
11.340122	608.773541	11.632896
11.582214	597.160872	11.637914
11.153248	599.417734	11.642931
11.300316	594.484646	11.647949
11.560252	599.758365	11.652967
11.477138	596.981727	11.657984
11.654015	600.179323	11.663002
11.585141	587.942918	11.668019
11.486045	588.920863	11.673037
11.736367	590.554432	11.678055
11.580728	588.997710	11.683072
11.573843	587.424138	11.688090
11.529018	598.258266	11.693107
11.370087	584.906153	11.698125
11.378697	590.812267	11.703143
11.031684	591.588981	11.708160
11.492229	586.102180	11.713178
11.548946	587.693312	11.718195
11.501053	589.916087	11.723213
11.694327	587.888491	11.728231
11.522670	598.278483	11.733248
11.365730	584.575780	11.738266
11.518333	599.989607	11.743283
11.599661	593.391091	11.748301
11.493068	589.059208	11.753319
11.316829	593.652942	11.758336
11.287061	598.309076	11.763354
11.410165	610.527651	11.768371
11.734608	619.720150	11.773389
12.098875	615.087740	11.778407
11.974618	620.866234	11.783424
11.664185	598.916390	11.788442
11.662764	597.957323	11.793459
11.539479	596.875225	11.798477
11.729120	600.190749	11.803495
11.603461	610.908088	11.808512
12.037426	607.078993	11.813530
11.640678	607.945499	11.818547
11.632448	601.370392	11.823565
12.139045	609.572043	11.828583
11.668767	596.782772	11.833600
11.819243	593.370188	11.838618
11.870832	588.761222	11.843635
12.070156	589.380294	11.848653
11.732662	583.938853	11.853671
11.670239	585.942993	11.858688
11.661205	582.044027	11.863706
11.561349	596.294847	11.868723
11.742492	614.468612	11.873741
11.966309	613.761642	11.878759
11.515686	618.085691	11.883776
11.857722	615.384861	11.888794
12.071646	621.640855	11.893811
12.186169	612.127630	11.898829
12.107487	618.653234	11.903847
11.863492	612.146386	11.908864
11.955878	611.642909	11.913882
12.177723	611.889261	11.918899
11.686222	606.923053	11.923917
11.844342	600.404093	11.928935
11.852613	612.971896	11.933952
12.208063	615.289659	11.938970
12.307387	616.085240	11.943987
11.840011	618.436444	11.949005
11.938016	614.602853	11.954023
11.625998	622.111490	11.959040
12.029717	621.711012	11.964058
12.300001	618.686852	11.969075
12.063511	618.755266	11.974093
11.989053	626.876987	11.979111
12.063720	624.198851	11.984128
12.139859	614.300296	11.989146
11.986789	618.290851	11.994163
11.965746	616.183016	11.999181
12.188863	615.378329	12.004199
11.901700	630.453570	12.009216
12.064686	627.452425	12.014234
12.732890	618.058110	12.019251
11.967173	615.690692	12.024269
12.327810	613.618102	12.029287
12.199598	621.748191	12.034304
12.224195	623.678828	12.039322
11.956764	623.865664	12.044339
11.703498	617.095182	12.049357
12.011396	622.831636	12.054375
11.839184	620.867254	12.059392
11.828461	610.941201	12.064410
12.432368	623.495165	12.069427
11.902481	633.751611	12.074445
12.212880	644.104444	12.079463
12.167600	647.084182	12.084480
12.287057	647.150824	12.089498
12.278600	644.021741	12.094515
12.156154	645.962652	12.099533
12.418595	639.174981	12.104551
12.196161	634.854811	12.109568
12.217717	645.217904	12.114586
12.084472	638.195206	12.119603
11.898492	639.186681	12.124621
12.147519	639.138479	12.129639
12.225998	644.863325	12.134656
12.538609	652.290501	12.139674
12.555460	652.827536	12.144691
12.410412	648.466913	12.149709
12.437736	639.812972	12.154727
12.774494	654.939408	12.159744
12.261788	647.713865	12.164762
12.373654	640.949638	12.169779
12.389225	662.213397	12.174797
12.467378	667.521751	12.179815
12.489029	672.993532	12.184832
12.717346	669.272180	12.189850
12.687869	662.659333	12.194867
12.646480	670.040651	12.199885
12.321266	668.033815	12.204903
12.471327	665.665814	12.209920
12.422441	667.522694	12.214938
12.890224	662.741616	12.219955
12.491913	666.943927	12.224973
12.930556	667.655123	12.229991
12.598667	661.045183	12.235008
12.641734	673.907400	12.240026
12.709869	660.570368	12.245043
12.692689	668.260329	12.250061
12.649165	669.652488	12.255079
12.763502	663.932400	12.260096
12.681233	667.798337	12.265114
12.739904	669.329214	12.270131
12.286998	669.024240	12.275149
12.570196	661.330803	12.280167
12.698515	673.807376	12.285184
12.600136	670.357786	12.290202
12.886160	661.073443	12.295219
12.290846	669.462465	12.300237
12.426001	658.008412	12.305255
12.479732	665.785157	12.310272
12.517337	681.235892	12.315290
12.819893	683.767020	12.320307
13.100368	694.771457	12.325325
13.137533	686.097027	12.330343
13.036190	689.003454	12.335360
13.054213	677.151075	12.340378
13.451570	681.147459	12.345395
12.598615	670.948578	12.350413
12.964630	672.655656	12.355431
13.122420	669.361834	12.360448
13.121867	671.154387	12.365466
12.738978	657.120749	12.370483
12.876573	666.648464	12.375501
13.025038	671.747064	12.380519
13.173749	674.642957	12.385536
13.264304	675.452529	12.390554
13.117370	660.542738	12.395571
13.044393	661.213675	12.400589
12.501162	655.624371	12.405607
13.012614	672.500272	12.410624
13.338398	681.152972	12.415642
13.368194	684.865770	12.420659
13.180880	680.404427	12.425677
13.351037	665.413704	12.430695
13.263510	671.461040	12.435712
13.048655	661.598299	12.440730
13.144983	656.632070	12.445747
12.942487	669.068631	12.450765
12.832331	673.144032	12.455783
13.437309	681.639657	12.460800
13.000041	693.226040	12.465818
13.648432	692.904227	12.470835
13.590383	677.611366	12.475853
13.445041	668.065991	12.480871
13.391390	671.971653	12.485888
13.156000	675.823564	12.490906
13.483299	668.195839	12.495923
13.325036	670.173886	12.500941
13.034414	658.609406	12.505959
13.071690	664.031416	12.510976
13.023965	670.407057	12.515994
13.325413	678.148395	12.521011
13.591650	689.631555	12.526029
13.722615	684.637835	12.531047
13.499945	665.612190	12.536064
12.898606	671.726902	12.541082
13.811834	659.997076	12.546099
13.383270	657.166920	12.551117
13.394608	658.686232	12.556135
13.026412	660.788478	12.561152
13.113682	677.143471	12.566170
13.653677	688.871174	12.571187
13.358090	688.090442	12.576205
13.681422	688.396730	12.581223
13.826212	683.321966	12.586240
13.126406	689.108044	12.591258
13.730174	695.536888	12.596275
13.663295	698.116070	12.601293
13.746358	693.606315	12.606311
13.820252	689.268396	12.611328
13.554030	675.494279	12.616346
13.594630	667.642958	12.621363
13.432917	668.185705	12.626381
13.093324	681.684998	12.631399
13.476300	679.394335	12.636416
13.742232	690.845986	12.641434
13.820204	678.993738	12.646451
13.512303	689.591182	12.651469
13.284625	698.106007	12.656487
13.752253	688.723949	12.661504
13.600055	695.027506	12.666522
13.717896	689.565630	12.671539
13.261413	684.442475	12.676557
13.500367	685.948439	12.681575
13.918210	680.177935	12.686592
13.536664	692.307887	12.691610
13.649531	688.030170	12.696627
13.628572	691.097645	12.701645
13.765719	691.262514	12.706663
13.844593	704.535730	12.711680
14.015180	714.758898	12.716698
13.960581	698.550332	12.721715
13.883717	693.743596	12.726733
13.542304	695.279964	12.731751
13.921073	706.105008	12.736768
13.854336	720.795723	12.741786
14.279382	711.732697	12.746803
14.159402	713.228279	12.751821
13.903355	705.603003	12.756839
14.250900	695.526452	12.761856
13.861632	698.521889	12.766874
13.800364	690.733754	12.771891
13.876295	700.274244	12.776909
14.023415	697.805714	12.781927
13.670731	703.932213	12.786944
13.840643	708.667735	12.791962
14.228984	719.156793	12.796979
13.981922	716.001734	12.801997
13.803496	726.033104	12.807015
14.133181	720.475122	12.812032
14.014053	715.990530	12.817050
13.898166	722.335778	12.822067
13.972824	720.317169	12.827085
14.096375	723.311658	12.832103
14.356022	716.988280	12.837120
14.337563	718.688955	12.842138
14.286162	710.615262	12.847155
14.097359	720.241161	12.852173
14.016451	726.514694	12.857191
14.103548	719.921545	12.862208
13.888447	720.381091	12.867226
14.068222	723.556169	12.872243
14.294099	720.229647	12.877261
13.962113	721.931801	12.882279
14.223314	711.644630	12.887296
13.764436	725.414983	12.892314
14.320602	736.862500	12.897331
14.585015	744.518118	12.902349
14.317147	743.862451	12.907367
14.247682	730.455275	12.912384
14.329796	735.538978	12.917402
14.396504	736.383823	12.922419
14.311444	743.907666	12.927437
14.476555	749.057343	12.932455
14.439465	741.855537	12.937472
14.290548	755.060118	12.942490
14.496287	747.770011	12.947507
14.697273	744.643014	12.952525
14.738152	755.044185	12.957543
14.820110	733.724180	12.962560
14.140530	727.689038	12.967578
14.303826	725.353681	12.972595
14.511202	734.239429	12.977613
14.471097	745.035043	12.982631
14.544409	742.076242	12.987648
14.529458	753.215072	12.992666
14.646074	751.701150	12.997683
14.826954	749.034859	13.002701
14.175895	748.577704	13.007719
14.459762	743.184633	13.012736
14.297550	748.997479	13.017754
14.364623	753.600707	13.022771
14.414055	744.116480	13.027789
14.045608	748.639197	13.032807
14.543914	750.568675	13.037824
14.885826	752.402586	13.042842
14.697110	760.144540	13.047859
14.438413	757.603491	13.052877
14.652263	767.860978	13.057895
15.072134	759.534013	13.062912
14.812396	776.599510	13.067930
14.701194	767.162371	13.072947
14.652442	768.536417	13.077965
14.560305	764.142282	13.082983
15.168705	767.941731	13.088000
15.034279	769.259692	13.093018
14.609694	774.709466	13.098035
14.948173	772.936944	13.103053
14.708044	772.157041	13.108071
14.944651	764.256225	13.113088
14.768000	769.452808	13.118106
14.769686	773.179469	13.123123
14.963266	775.462498	13.128141
14.835364	774.633564	13.133159
15.186613	765.916505	13.138176
14.914782	769.979231	13.143194
14.977312	767.640623	13.148211
14.999412	770.931774	13.153229
15.316252	768.626151	13.158247
15.067691	766.115080	13.163264
14.998591	763.945284	13.168282
15.167404	774.727323	13.173299
15.216548	774.369425	13.178317
15.175939	776.982397	13.183335
14.921297	775.734552	13.188352
14.952162	773.249400	13.193370
15.029948	771.173495	13.198387
15.313605	764.066903	13.203405
14.983283	767.138378	13.208423
15.273171	771.290366	13.213440
15.337867	766.114443	13.218458
15.016188	776.051385	13.223475
15.017585	777.363977	13.228493
14.494562	775.157561	13.233511
15.308795	772.932281	13.238528
15.012076	777.402814	13.243546
15.058286	773.507828	13.248563
15.204912	780.790493	13.253581
15.327396	789.768378	13.258599
15.708998	794.294245	13.263616
15.494801	783.323680	13.268634
15.280446	774.379109	13.273651
15.550336	765.952420	13.278669
15.137455	768.295159	13.283687
15.074404	768.560624	13.288704
15.106539	789.610524	13.293722
15.393848	796.356912	13.298739
15.813830	795.505788	13.303757
15.724568	792.411350	13.308775
15.647077	788.857502	13.313792
15.617348	778.688170	13.318810
15.520100	777.674588	13.323827
15.295450	765.168834	13.328845
15.428766	781.548310	13.333863
15.682302	782.108457	13.338880
15.633478	785.549503	13.343898
15.462845	789.823689	13.348915
15.928034	777.421953	13.353933
15.171176	768.423000	13.358951
15.658811	773.105915	13.363968
15.764405	782.736502	13.368986
15.560947	787.902551	13.374003
15.904135	794.454051	13.379021
15.707267	791.783453	13.384039
16.010798	781.262441	13.389056
15.812375	773.151652	13.394074
15.653261	768.278810	13.399091
15.711104	762.062573	13.404109
15.585000	759.560837	13.409127
15.861842	774.419002	13.414144
15.915406	760.304705	13.419162
15.803399	770.000722	13.424179
15.788629	765.177988	13.429197
15.674462	766.584309	13.434215
15.747053	761.435560	13.439232
15.935345	776.219153	13.444250
15.818561	788.203810	13.449267
16.168824	778.682193	13.454285
15.775129	775.777164	13.459303
16.017027	778.242013	13.464320
15.992322	772.556160	13.469338
15.738039	765.246154	13.474355
15.862798	786.770764	13.479373
15.755146	788.611560	13.484391
15.731245	786.661935	13.489408
16.105238	789.737360	13.494426
15.916476	800.773897	13.499443
15.693246	790.984969	13.504461
16.130006	803.170621	13.509479
15.697735	794.493491	13.514496
15.869995	790.474737	13.519514
15.768491	799.897744	13.524531
16.043416	799.782395	13.529549
15.881357	797.806944	13.534567
15.879424	799.580791	13.539584
16.119148	808.530965	13.544602
16.002847	813.992711	13.549619
16.090326	813.048193	13.554637
16.150351	819.138875	13.559655
16.026426	826.170201	13.564672
16.400601	825.676492	13.569690
16.078988	828.424738	13.574707
16.340030	818.462569	13.579725
16.105727	823.551382	13.584743
16.244302	818.726848	13.589760
16.293055	816.586033	13.594778
16.075318	818.251474	13.599795
16.239563	811.882957	13.604813
16.362769	812.365570	13.609831
16.185283	812.390085	13.614848
16.434054	818.208390	13.619866
16.197660	815.723818	13.624883
16.071916	814.853522	13.629901
15.942234	814.163715	13.634919
16.214257	822.632355	13.639936
16.692294	842.028724	13.644954
16.438908	855.574684	13.649971
17.056876	832.129356	13.654989
16.547005	823.912406	13.660007
16.614712	815.709671	13.665024
16.534534	817.101237	13.670042
16.459252	814.897685	13.675059
16.692674	808.884462	13.680077
16.819952	817.678584	13.685095
16.310508	819.294771	13.690112
16.606989	809.838315	13.695130
16.600809	816.687208	13.700147
16.625765	812.984865	13.705165
16.379069	819.135925	13.710183
16.564822	827.671647	13.715200
16.896603	833.959857	13.720218
16.923370	838.174918	13.725235
16.889842	828.337500	13.730253
16.563627	822.761690	13.735271
16.524437	835.573717	13.740288
16.819732	837.465387	13.745306
16.707988	847.704188	13.750323
17.250547	830.815562	13.755341
17.067580	830.900889	13.760359
16.756272	823.082201	13.765376
16.669601	813.950477	13.770394
16.858187	820.668064	13.775411
17.305459	832.138908	13.780429
17.084310	820.535105	13.785447
16.853212	816.433983	13.790464
16.796357	806.016402	13.795482
16.820256	810.411779	13.800499
16.675355	808.528327	13.805517
16.684812	830.907205	13.810535
16.973449	833.506792	13.815552
17.324938	828.592302	13.820570
17.035288	834.945710	13.825587
16.951216	830.020143	13.830605
17.017361	838.618672	13.835623
17.316513	843.056405	13.840640
16.852188	835.005922	13.845658
16.732729	845.072359	13.850675
17.343926	840.085874	13.855693
17.213455	825.372192	13.860711
17.206840	840.356593	13.865728
17.580622	834.028026	13.870746
17.067396	836.578895	13.875763
17.233396	832.475903	13.880781
17.021088	832.256538	13.885799
17.070626	844.575088	13.890816
17.230574	838.254567	13.895834
16.719702	836.955097	13.900851
16.823966	829.797517	13.905869
17.067609	839.034267	13.910887
16.953163	839.714823	13.915904
17.410037	838.179474	13.920922
17.446960	849.013649	13.925939
17.317283	849.166416	13.930957
17.447203	840.067227	13.935975
17.247345	858.975886	13.940992
17.630181	852.491272	13.946010
17.633634	865.078937	13.951027
17.409661	855.488900	13.956045
17.500672	847.695921	13.961063
17.526545	845.366166	13.966080
17.010774	836.765130	13.971098
17.379311	856.740281	13.976115
17.394164	852.512498	13.981133
17.577925	856.059353	13.986151
17.514399	861.547610	13.991168
17.823006	859.259037	13.996186
17.780588	862.071113	14.001203
17.593085	858.619584	14.006221
18.038689	856.972383	14.011239
17.695717	861.825669	14.016256
17.858489	851.566365	14.021274
17.610991	852.053048	14.026291
17.935691	859.468962	14.031309
17.704781	848.365263	14.036327
17.725221	863.310759	14.041344
18.004957	856.144782	14.046362
17.489058	850.576406	14.051379
17.665876	848.560811	14.056397
17.748887	856.553981	14.061415
17.518590	850.635033	14.066432
17.876578	855.805202	14.071450
18.000620	865.303577	14.076467
17.661679	859.316337	14.081485
17.906785	857.078676	14.086503
17.588193	866.816377	14.091520
18.047736	866.145278	14.096538
18.163011	858.553638	14.101555
17.751351	858.655637	14.106573
18.105292	859.525193	14.111591
17.496809	868.787336	14.116608
17.918800	851.743898	14.121626
17.659688	864.344041	14.126643
18.265174	857.749023	14.131661
18.405907	860.794507	14.136679
17.904773	863.308785	14.141696
17.984858	857.919006	14.146714
18.014946	851.647100	14.151731
18.360350	860.826993	14.156749
18.169205	850.979390	14.161767
17.880135	860.447411	14.166784
18.083132	861.214239	14.171802
18.053604	858.334545	14.176819
17.990459	854.298781	14.181837
18.017253	859.315396	14.186855
18.054956	877.779999	14.191872
18.156961	879.843775	14.196890
18.340530	889.118306	14.201907
18.221770	887.527414	14.206925
18.570523	874.408456	14.211943
18.533740	882.193077	14.216960
18.375001	875.925317	14.221978
18.355685	881.687555	14.226995
18.393001	878.485035	14.232013
18.561685	875.640747	14.237031
18.588200	878.009759	14.242048
18.236224	882.274332	14.247066
18.506713	876.078595	14.252083
18.584145	879.629387	14.257101
18.633868	868.923784	14.262119
18.611719	866.248062	14.267136
18.396198	863.261629	14.272154
18.651160	874.655148	14.277171
18.516452	876.320290	14.282189
18.347522	869.915267	14.287207
18.368047	875.715481	14.292224
18.881598	880.306030	14.297242
18.764590	876.919259	14.302259
18.263995	883.267659	14.307277
18.515005	877.346346	14.312295
18.650541	880.313750	14.317312
18.843392	873.590473	14.322330
18.498246	877.017715	14.327347
18.568570	883.242512	14.332365
18.702657	875.430191	14.337383
18.748656	873.453895	14.342400
18.947012	882.650383	14.347418
18.939935	879.110800	14.352435
18.397230	884.831456	14.357453
18.485507	872.248503	14.362471
18.371267	883.415496	14.367488
18.805063	880.810791	14.372506
19.322987	887.341431	14.377523
18.859159	884.699760	14.382541
19.408879	879.789107	14.387559
19.077878	875.441601	14.392576
18.729519	868.196691	14.397594
18.828499	874.174033	14.402611
19.029497	874.452036	14.407629
18.946652	875.619966	14.412647
19.317064	885.868924	14.417664
19.037691	875.511193	14.422682
19.230483	874.891093	14.427699
19.267759	874.973686	14.432717
18.867508	862.940160	14.437735
18.761517	874.920039	14.442752
18.951617	887.163087	14.447770
18.739788	887.906143	14.452787
18.971626	894.468705	14.457805
19.269368	895.962379	14.462823
18.896168	903.348119	14.467840
19.320382	900.886910	14.472858
19.291609	901.841301	14.477875
19.458308	896.983966	14.482893
19.313516	895.305609	14.487911
19.122003	898.159839	14.492928
19.031390	897.978329	14.497946
19.304082	895.073665	14.502963
19.110713	901.639318	14.507981
19.293243	890.767861	14.512999
19.323980	894.310147	14.518016
19.271075	892.021053	14.523034
19.299989	898.997054	14.528051
19.379198	914.381555	14.533069
19.604177	914.573776	14.538087
19.431688	921.268726	14.543104
19.437884	912.128805	14.548122
19.646551	914.810280	14.553139
19.737073	916.118474	14.558157
19.936765	922.215848	14.563175
19.556691	909.150381	14.568192
19.787403	905.785203	14.573210
19.711856	899.195221	14.578227
19.643080	901.717925	14.583245
19.424871	895.342655	14.588263
19.568011	907.040776	14.593280
19.197624	915.637883	14.598298
19.605982	917.104869	14.603315
19.657345	924.064761	14.608333
19.913785	915.835751	14.613351
19.632191	921.458962	14.618368
19.851317	917.543333	14.623386
20.130814	914.066420	14.628403
19.764528	917.878804	14.633421
20.103996	912.009978	14.638439
19.801446	921.502220	14.643456
19.846990	917.231774	14.648474
20.129401	905.789347	14.653491
19.924949	923.408097	14.658509
20.301648	916.599376	14.663527
19.805109	919.103478	14.668544
19.676228	912.745851	14.673562
20.318248	922.431847	14.678579
19.767850	920.021396	14.683597
20.207715	908.702772	14.688615
20.052734	917.783881	14.693632
20.066653	912.432789	14.698650
20.179261	915.735121	14.703667
20.270518	915.572630	14.708685
19.963450	914.866257	14.713703
20.105955	914.156157	14.718720
20.100572	918.767553	14.723738
20.143560	914.052548	14.728755
20.298492	912.854531	14.733773
19.981764	913.086914	14.738791
20.240746	921.788000	14.743808
20.009751	911.488986	14.748826
20.080947	915.757107	14.753843
20.172389	920.997198	14.758861
20.090567	931.016798	14.763879
20.288547	934.555144	14.768896
20.355324	936.763264	14.773914
20.420039	932.407781	14.778931
20.445201	939.406472	14.783949
20.865569	942.294827	14.788967
20.618508	933.563546	14.793984
20.575401	928.132967	14.799002
20.644455	912.536100	14.804019
20.389022	925.463909	14.809037
20.623879	921.504806	14.814055
20.653863	916.081785	14.819072
20.178582	922.019168	14.824090
20.483920	927.560465	14.829107
20.236781	941.427402	14.834125
20.578885	941.187987	14.839143
20.609563	942.284598	14.844160
20.384176	948.126279	14.849178
20.721439	934.699804	14.854195
20.732055	947.709280	14.859213
20.747330	935.371173	14.864231
20.482629	936.914552	14.869248
20.596018	943.356722	14.874266
20.981512	937.127279	14.879283
20.518404	948.424367	14.884301
20.665589	934.295356	14.889319
20.625934	946.754093	14.894336
20.667827	954.914652	14.899354
20.774657	946.263963	14.904371
20.593964	955.901348	14.909389
21.036277	957.858502	14.914407
21.259656	965.741506	14.919424
20.993953	964.586887	14.924442
21.215000	963.883491	14.929459
21.081517	962.667261	14.934477
20.964815	961.016082	14.939495
21.136016	943.311030	14.944512
20.591926	943.026559	14.949530
21.129270	951.548623	14.954547
20.990225	960.602028	14.959565
21.473150	956.995605	14.964583
21.599054	966.834564	14.969600
21.125738	958.580302	14.974618
21.208500	947.411925	14.979635
21.246445	950.858428	14.984653
21.116393	953.466417	14.989671
21.202262	949.764029	14.994688
21.307488	960.350958	14.999706
21.052912	959.595385	15.004723
21.121876	964.908415	15.009741
21.286299	960.117687	15.014759
21.604881	960.333204	15.019776
21.327279	963.096708	15.024794
21.520146	962.116839	15.029811
21.155326	955.726506	15.034829
21.358831	954.842809	15.039847
21.509199	954.437590	15.044864
21.414721	962.840286	15.049882
21.633387	947.450463	15.054899
21.314974	954.893964	15.059917
21.133566	952.924665	15.064935
21.456944	949.958453	15.069952
21.215217	958.128458	15.074970
21.389003	949.786072	15.079987
21.459258	967.908037	15.085005
21.614330	980.749881	15.090023
21.874379	976.849959	15.095040
21.969385	986.289804	15.100058
21.830226	965.221695	15.105075
21.811715	954.413058	15.110093
21.372344	950.079251	15.115111
21.891513	972.300053	15.120128
21.919071	985.837084	15.125146
21.855149	972.450953	15.130163
22.053675	975.755697	15.135181
21.664288	962.928321	15.140199
21.944635	968.230530	15.145216
21.718760	972.478646	15.150234
22.103921	975.255726	15.155251
21.806041	978.820792	15.160269
21.701772	981.371123	15.165287
22.194995	983.673796	15.170304
21.798521	980.743919	15.175322
22.105307	977.837089	15.180339
21.895593	985.670770	15.185357
22.174581	977.662279	15.190375
22.323868	978.992885	15.195392
22.073014	975.279803	15.200410
22.174224	974.449901	15.205427
22.454592	979.070470	15.210445
22.441394	980.290678	15.215463
22.297890	964.278744	15.220480
22.199566	954.722738	15.225498
22.102497	962.535715	15.230515
22.326036	974.375993	15.235533
22.093442	968.552036	15.240551
22.295719	963.288364	15.245568
21.989053	976.088490	15.250586
22.442657	973.423884	15.255603
22.323405	970.460314	15.260621
22.596327	980.781309	15.265639
22.550685	974.009921	15.270656
22.299008	977.924392	15.275674
22.631480	976.010778	15.280691
22.152167	980.386716	15.285709
22.611194	990.599848	15.290727
22.412017	973.296408	15.295744
22.154190	981.604628	15.300762
22.466642	974.420887	15.305779
22.516397	967.713542	15.310797
22.159274	979.265542	15.315815
22.557771	976.745213	15.320832
22.227583	981.874245	15.325850
22.477679	976.508453	15.330867
22.319162	976.201817	15.335885
22.383660	996.218152	15.340903
22.571001	997.530211	15.345920
22.923741	1009.154741	15.350938
22.920585	1001.404758	15.355955
22.971045	1008.891834	15.360973
22.596538	1006.693822	15.365991
22.849198	995.558922	15.371008
22.899671	1001.095743	15.376026
22.703355	1000.510975	15.381043
22.978405	1001.235033	15.386061
23.075552	1004.044337	15.391079
22.969114	992.763381	15.396096
22.781277	994.670330	15.401114
22.846151	989.358618	15.406131
23.036300	993.390491	15.411149
22.979572	991.262922	15.416167
23.179198	988.524250	15.421184
23.282077	993.333400	15.426202
23.025881	985.767985	15.431219
23.188922	983.530462	15.436237
23.152461	987.676510	15.441255
23.373535	994.404883	15.446272
23.257525	989.017194	15.451290
23.107411	989.214169	15.456307
23.032073	996.310580	15.461325
23.413008	986.383298	15.466343
23.573969	990.230370	15.471360
23.285598	990.161698	15.476378
23.390461	999.126654	15.481395
23.405145	993.100090	15.486413
23.214791	996.620016	15.491431
23.850061	994.823354	15.496448
23.251651	991.811309	15.501466
23.243804	996.009707	15.506483
23.388635	988.514394	15.511501
23.306106	999.518735	15.516519
23.494424	997.596005	15.521536
23.265794	993.030564	15.526554
23.069539	991.896687	15.531571
23.686730	989.922963	15.536589
23.780208	1006.482415	15.541607
23.648274	992.548291	15.546624
23.576373	998.325066	15.551642
23.311717	1000.411231	15.556659
23.437950	1007.886509	15.561677
23.733544	1019.459984	15.566695
23.684322	1012.793278	15.571712
23.708760	1013.335455	15.576730
23.488108	1018.889248	15.581747
23.537065	1016.985058	15.586765
23.653123	1020.444660	15.591783
24.185187	1014.965528	15.596800
24.011123	1014.759140	15.601818
23.869387	1025.128943	15.606835
24.069943	1008.347046	15.611853
23.860681	1022.324911	15.616871
24.315051	1018.565135	15.621888
23.966467	1023.078517	15.626906
23.831905	1020.167814	15.631923
24.232845	1016.829760	15.636941
24.161770	1016.039303	15.641959
24.166967	1009.963718	15.646976
24.177710	1020.155146	15.651994
23.881373	1020.627347	15.657011
23.742388	1008.398412	15.662029
23.836249	1012.864995	15.667047
24.038969	1012.700928	15.672064
24.093310	1006.440971	15.677082
23.953492	1011.691848	15.682099
24.238421	1016.172864	15.687117
24.325791	1018.447215	15.692135
24.748280	1024.588829	15.697152
24.249468	1023.281155	15.702170
24.289728	1013.122883	15.707187
24.203481	1018.952390	15.712205
24.220857	1031.907228	15.717223
24.268755	1030.624884	15.722240
24.723882	1024.709611	15.727258
24.513981	1031.842765	15.732275
24.578738	1032.321861	15.737293
24.199366	1034.504784	15.742311
24.481144	1027.335266	15.747328
24.570284	1030.344632	15.752346
24.274216	1027.070917	15.757363
24.818748	1028.933270	15.762381
24.795848	1034.598288	15.767399
24.834731	1027.621219	15.772416
24.398520	1035.546990	15.777434
24.632949	1046.132788	15.782451
24.511193	1027.441333	15.787469
24.549612	1039.774373	15.792487
24.680635	1034.035789	15.797504
24.690741	1039.304356	15.802522
24.719969	1035.822205	15.807539
24.915464	1033.226178	15.812557
24.918875	1028.372140	15.817575
24.741087	1027.276411	15.822592
25.118071	1033.595524	15.827610
24.966298	1034.969852	15.832627
24.908207	1025.309716	15.837645
25.009210	1036.866163	15.842663
24.940863	1053.059540	15.847680
25.398738	1054.689239	15.852698
24.988553	1050.101559	15.857715
25.062945	1042.424689	15.862733
24.754627	1045.057291	15.867751
25.069557	1053.229032	15.872768
25.324182	1055.698249	15.877786
25.150208	1046.759877	15.882803
25.071420	1047.501160	15.887821
25.290230	1055.129299	15.892839
25.013942	1049.056501	15.897856
25.337700	1049.403755	15.902874
25.231556	1050.998195	15.907891
25.454287	1050.783676	15.912909
25.255557	1054.169220	15.917927
25.177953	1045.061212	15.922944
25.022907	1054.906094	15.927962
25.264814	1050.964799	15.932979
25.506351	1045.625564	15.937997
25.777261	1050.149796	15.943015
25.581421	1045.187923	15.948032
25.758755	1058.824764	15.953050
25.586382	1044.546606	15.958067
25.593496	1042.759380	15.963085
25.681150	1054.725009	15.968103
25.369281	1050.993009	15.973120
25.531766	1051.153937	15.978138
25.631347	1054.653979	15.983155
25.668644	1047.216409	15.988173
25.570563	1043.157640	15.993191
25.682542	1047.722395	15.998208
25.722100	1049.657061	16.003226
25.644495	1052.948009	16.008243
25.732067	1065.292348	16.013261
25.727008	1064.769317	16.018279
25.954911	1071.095876	16.023296
26.149342	1064.432240	16.028314
25.969248	1077.351585	16.033331
26.019132	1068.463553	16.038349
26.061061	1064.373513	16.043367
26.183924	1071.751514	16.048384
26.143637	1061.962355	16.053402
26.093747	1081.851431	16.058419
26.389026	1073.332283	16.063437
26.175272	1058.457807	16.068455
26.016792	1049.949359	16.073472
26.290821	1056.357092	16.078490
26.144103	1066.216462	16.083507
26.387403	1057.781153	16.088525
26.186346	1055.130102	16.093543
26.282408	1054.768049	16.098560
26.471991	1058.443425	16.103578
26.342400	1055.632926	16.108595
26.501017	1038.952202	16.113613
26.422485	1036.616587	16.118631
26.175887	1034.427058	16.123648
26.171132	1048.682367	16.128666
26.349067	1061.975140	16.133683
26.567668	1061.259498	16.138701
26.674287	1073.342105	16.143719
26.307742	1074.440612	16.148736
26.433328	1062.908894	16.153754
26.408585	1073.541372	16.158771
26.254064	1063.523849	16.163789
26.287629	1066.115847	16.168807
26.491834	1071.751830	16.173824
26.715000	1065.541304	16.178842
26.385728	1072.885562	16.183859
26.646042	1071.459691	16.188877
26.617737	1070.621548	16.193895
26.558112	1070.012339	16.198912
27.073033	1075.751422	16.203930
27.137719	1086.420476	16.208947
27.001156	1083.020932	16.213965
26.710039	1080.525908	16.218983
26.644665	1076.452572	16.224000
26.851232	1078.219229	16.229018
27.016451	1091.081664	16.234035
26.900431	1088.060768	16.239053
27.406291	1092.261256	16.244071
26.622171	1088.536504	16.249088
27.206412	1094.564598	16.254106
27.073466	1096.327314	16.259123
27.053254	1094.904093	16.264141
27.208061	1093.753421	16.269159
27.108487	1101.226026	16.274176
27.265499	1096.947649	16.279194
27.387050	1094.341037	16.284211
27.278225	1091.675620	16.289229
27.137193	1089.305548	16.294247
27.114205	1093.222308	16.299264
27.239631	1091.628091	16.304282
26.955908	1091.441932	16.309299
27.544425	1093.837079	16.314317
27.302430	1088.847666	16.319335
27.013912	1102.740106	16.324352
27.426937	1097.045957	16.329370
27.288849	1089.856579	16.334387
27.666258	1093.837228	16.339405
27.512624	1097.007480	16.344423
27.117084	1088.340265	16.349440
27.413743	1086.255492	16.354458
27.235862	1105.432386	16.359475
27.724604	1108.603609	16.364493
28.085041	1109.983400	16.369511
27.965186	1117.623269	16.374528
27.714303	1099.204305	16.379546
27.773947	1096.660978	16.384563
27.802739	1098.966550	16.389581
27.888773	1099.641148	16.394599
27.515530	1110.712911	16.399616
27.773849	1116.059619	16.404634
27.879552	1113.089402	16.409651
27.831143	1123.176491	16.414669
27.718483	1113.433286	16.419687
27.450243	1116.690811	16.424704
27.924666	1114.092370	16.429722
28.124267	1115.901141	16.434739
27.706026	1112.024745	16.439757
27.900074	1110.618657	16.444775
27.680191	1112.915611	16.449792
27.818986	1120.278529	16.454810
28.231965	1128.356145	16.459827
28.030823	1136.131753	16.464845
28.340581	1134.568793	16.469863
28.633372	1146.420495	16.474880
28.544165	1145.983145	16.479898
28.294145	1124.127387	16.484915
28.322419	1123.835847	16.489933
28.584348	1121.324137	16.494951
28.251338	1120.321997	16.499968
28.630990	1120.676329	16.504986
28.368391	1109.444858	16.510003
28.113667	1111.318053	16.515021
28.204015	1125.593330	16.520039
28.012945	1137.375195	16.525056
28.478108	1124.657646	16.530074
29.043816	1127.794799	16.535091
28.901192	1122.193465	16.540109
28.609228	1122.027523	16.545127
28.578112	1120.183126	16.550144
28.886699	1126.093204	16.555162
28.519744	1126.936160	16.560179
28.856225	1126.003349	16.565197
28.969923	1119.226032	16.570215
28.825031	1127.352636	16.575232
28.911829	1120.301799	16.580250
28.801018	1125.027492	16.585267
28.654945	1125.255397	16.590285
29.061049	1116.952500	16.595303
28.921668	1119.397866	16.600320
29.298428	1125.325731	16.605338
29.122679	1130.190923	16.610355
29.022233	1130.642094	16.615373
29.172585	1124.512312	16.620391
28.994234	1129.235899	16.625408
28.992298	1130.801498	16.630426
28.901108	1128.559359	16.635443
28.989728	1127.696697	16.640461
29.129418	1125.790991	16.645479
28.875714	1123.482638	16.650496
29.124671	1126.823740	16.655514
29.231523	1126.261192	16.660531
28.931706	1129.189125	16.665549
29.004597	1124.516745	16.670567
28.837416	1126.565657	16.675584
29.268980	1141.721928	16.680602
29.242077	1145.560415	16.685619
29.022157	1153.698712	16.690637
29.540961	1146.129329	16.695655
29.444869	1153.475183	16.700672
29.749715	1143.146255	16.705690
29.287028	1143.941001	16.710707
29.179604	1144.670967	16.715725
29.803021	1141.613829	16.720743
29.443851	1146.545452	16.725760
29.708835	1149.682093	16.730778
29.705930	1151.049031	16.735795
29.873040	1150.944155	16.740813
29.680342	1141.184994	16.745831
29.955828	1147.684051	16.750848
30.027229	1151.762850	16.755866
30.327842	1144.984823	16.760883
29.513485	1148.062297	16.765901
29.946802	1141.336193	16.770919
29.550457	1148.375347	16.775936
30.166771	1136.656726	16.780954
30.285467	1141.258329	16.785971
30.168948	1154.193077	16.790989
29.979001	1143.635076	16.796007
30.129663	1152.274246	16.801024
29.977898	1153.197307	16.806042
29.954476	1143.231910	16.811059
30.032203	1147.271855	16.816077
29.895614	1146.270688	16.821095
30.105022	1165.873336	16.826112
29.889496	1158.168973	16.831130
30.070307	1156.310510	16.836147
30.188652	1158.624237	16.841165
30.347388	1150.473447	16.846183
30.089391	1159.955723	16.851200
30.063935	1156.838664	16.856218
30.267843	1160.082645	16.861235
29.985562	1167.905614	16.866253
30.200256	1169.882452	16.871271
30.390060	1179.964042	16.876288
30.198283	1178.621175	16.881306
30.461739	1173.486771	16.886323
30.434168	1177.805046	16.891341
30.685814	1183.039205	16.896359
30.832326	1181.170301	16.901376
31.034814	1187.257864	16.906394
30.982771	1183.450668	16.911411
30.846996	1190.010616	16.916429
30.927392	1173.108418	16.921447
31.051651	1184.756013	16.926464
31.027498	1184.374806	16.931482
31.126403	1178.117317	16.936499
31.001672	1178.834201	16.941517
31.300876	1171.456786	16.946535
31.217696	1154.261340	16.951552
31.093826	1155.606087	16.956570
31.032227	1147.186649	16.961587
30.752431	1150.250322	16.966605
31.012483	1146.154704	16.971623
30.936539	1161.295335	16.976640
31.064920	1170.468154	16.981658
31.223172	1174.615486	16.986675
30.614107	1180.684236	16.991693
30.594298	1169.904071	16.996711
30.482221	1172.884830	17.001728
30.860808	1184.783159	17.006746
31.359680	1190.799331	17.011763
31.211886	1201.731908	17.016781
31.353424	1200.621164	17.021799
31.522204	1206.799188	17.026816
31.475484	1205.168648	17.031834
31.889406	1200.477865	17.036851
31.382117	1206.041631	17.041869
31.712579	1205.400085	17.046887
31.539044	1209.677978	17.051904
31.613191	1205.702809	17.056922
31.699612	1201.545850	17.061939
31.850220	1203.242339	17.066957
31.991444	1197.416908	17.071975
32.117655	1213.498089	17.076992
31.782140	1205.951241	17.082010
31.781358	1186.827376	17.087027
31.776382	1192.764207	17.092045
31.782867	1199.715416	17.097063
31.869984	1200.364603	17.102080
31.778209	1208.053788	17.107098
31.658435	1203.341957	17.112115
31.817663	1209.174332	17.117133
31.828047	1202.558235	17.122151
31.770158	1198.045052	17.127168
31.545486	1198.370401	17.132186
32.084259	1196.828583	17.137203
31.855706	1203.204167	17.142221
31.742257	1205.080622	17.147239
32.437898	1220.460930	17.152256
32.304504	1222.684473	17.157274
32.772429	1213.440950	17.162291
32.294013	1206.566442	17.167309
32.395687	1194.987870	17.172327
32.329305	1194.849921	17.177344
31.951574	1194.148226	17.182362
32.698295	1202.483180	17.187379
32.590994	1217.284761	17.192397
32.666939	1209.500281	17.197415
32.440705	1209.526074	17.202432
32.498078	1217.510775	17.207450
32.654143	1210.433339	17.212467
32.889176	1216.197111	17.217485
32.697059	1207.835834	17.222503
32.344340	1196.435304	17.227520
32.409317	1218.496760	17.232538
32.637822	1223.422112	17.237555
32.579302	1220.811959	17.242573
32.709573	1215.947586	17.247591
32.920758	1219.607008	17.252608
32.591275	1220.513562	17.257626
32.904842	1207.497667	17.262643
32.789193	1212.918408	17.267661
32.991271	1216.623429	17.272679
32.988054	1215.835021	17.277696
32.549541	1219.138010	17.282714
32.975429	1218.945507	17.287731
32.817913	1225.382621	17.292749
32.938226	1225.685816	17.297767
33.220677	1218.263653	17.302784
33.111708	1227.208369	17.307802
33.116817	1229.432439	17.312819
33.444173	1243.560457	17.317837
33.221624	1244.336754	17.322855
33.566669	1238.902451	17.327872
32.926140	1237.563176	17.332890
33.189329	1233.183030	17.337907
32.759495	1239.217582	17.342925
32.931312	1244.666159	17.347943
33.204292	1228.185202	17.352960
32.881898	1237.570249	17.357978
33.392162	1249.451275	17.362995
33.554110	1264.592825	17.368013
33.855637	1265.615729	17.373031
34.148170	1264.323682	17.378048
33.723274	1248.935969	17.383066
33.996978	1242.764851	17.388083
33.556756	1228.319966	17.393101
33.628525	1235.087457	17.398119
33.657966	1247.639788	17.403136
33.679731	1251.391824	17.408154
33.929141	1247.212634	17.413171
34.020930	1258.612871	17.418189
33.846408	1260.798640	17.423207
34.006822	1252.720125	17.428224
33.695204	1256.792311	17.433242
33.999393	1257.622297	17.438259
34.232752	1264.812762	17.443277
34.263884	1256.883761	17.448295
34.305098	1256.577581	17.453312
34.404106	1257.815051	17.458330
34.659477	1260.738615	17.463347
34.490801	1254.866742	17.468365
34.089570	1259.902774	17.473383
33.958429	1253.558000	17.478400
34.239649	1255.439284	17.483418
34.416172	1259.388133	17.488435
34.126077	1262.093668	17.493453
34.216011	1266.087557	17.498471
34.275018	1248.576394	17.503488
34.076853	1254.660088	17.508506
34.315492	1251.505050	17.513523
34.465920	1258.695801	17.518541
34.401073	1268.526757	17.523559
34.730960	1276.955048	17.528576
34.573465	1285.910504	17.533594
34.794758	1283.250465	17.538611
34.764315	1286.685591	17.543629
34.774247	1289.309703	17.548647
34.963273	1279.793990	17.553664
34.480594	1279.724011	17.558682
34.718044	1281.940315	17.563699
34.933246	1281.843730	17.568717
34.770845	1275.390207	17.573735
34.698262	1273.334500	17.578752
34.682903	1278.660752	17.583770
35.031895	1273.888541	17.588787
35.268208	1275.174062	17.593805
34.999812	1276.159469	17.598823
35.330333	1275.199177	17.603840
34.838479	1273.600067	17.608858
35.205406	1278.055759	17.613875
35.388132	1274.088916	17.618893
35.176872	1273.869382	17.623911
34.953836	1267.494729	17.628928
35.232460	1279.487580	17.633946
35.447778	1283.862738	17.638963
35.721433	1286.985431	17.643981
35.169905	1285.465038	17.648999
35.655137	1276.247190	17.654016
35.265213	1282.603746	17.659034
35.602499	1284.359539	17.664051
35.738560	1288.652364	17.669069
35.728512	1282.288726	17.674087
35.941988	1288.854294	17.679104
35.752875	1280.890145	17.684122
35.750685	1276.551306	17.689139
36.057927	1274.486955	17.694157
35.889437	1267.598883	17.699175
36.187716	1260.376209	17.704192
35.941443	1261.998797	17.709210
35.880018	1261.563431	17.714227
35.970970	1258.608110	17.719245
35.687013	1260.148202	17.724263
35.792747	1267.598379	17.729280
36.002791	1282.309580	17.734298
36.009844	1287.057990	17.739315
36.365303	1289.659863	17.744333
35.966941	1293.868640	17.749351
35.886648	1275.381907	17.754368
35.840731	1281.123170	17.759386
35.746877	1291.040706	17.764403
36.125682	1284.783782	17.769421
35.986906	1286.866159	17.774439
36.044666	1283.392140	17.779456
36.414390	1302.351443	17.784474
36.231182	1308.227699	17.789491
36.625261	1303.486330	17.794509
36.557333	1314.987209	17.799527
36.771267	1307.812362	17.804544
36.806003	1306.784512	17.809562
36.610864	1300.184598	17.814579
37.038839	1313.577484	17.819597
36.684888	1311.679189	17.824615
36.819585	1305.236203	17.829632
36.641343	1309.300258	17.834650
36.723558	1308.003084	17.839667
36.996838	1305.467491	17.844685
36.362194	1315.418745	17.849703
36.523267	1308.804394	17.854720
36.755298	1309.465736	17.859738
36.623948	1311.016786	17.864755
36.747494	1305.500185	17.869773
36.875637	1305.325636	17.874791
36.870777	1312.310214	17.879808
37.129871	1320.194127	17.884826
37.079203	1322.183895	17.889843
37.464118	1331.070703	17.894861
37.160049	1335.211159	17.899879
37.399489	1327.041411	17.904896
37.217211	1322.291943	17.909914
37.341272	1327.501829	17.914931
37.166077	1320.554820	17.919949
36.938472	1332.077415	17.924967
36.713043	1326.208042	17.929984
36.894486	1336.350983	17.935002
36.463128	1330.882901	17.940019
36.982520	1344.621338	17.945037
37.293078	1352.386799	17.950055
37.742005	1355.513773	17.955072
38.147391	1349.965901	17.960090
38.319041	1352.552220	17.965107
37.981720	1358.641836	17.970125
37.931097	1345.152368	17.975143
38.132552	1344.556150	17.980160
37.948421	1354.412037	17.985178
37.734335	1354.710494	17.990195
37.872168	1349.690272	17.995213
37.948786	1358.091763	18.000231
38.351859	1357.385258	18.005248
38.136997	1348.118584	18.010266
38.088985	1351.209319	18.015283
38.584910	1344.132565	18.020301
38.151534	1332.432080	18.025319
38.455629	1330.898388	18.030336
38.195983	1325.703373	18.035354
38.038364	1326.778833	18.040371
38.203036	1333.702309	18.045389
37.953456	1350.482751	18.050407
38.023300	1349.774481	18.055424
38.488926	1351.141070	18.060442
38.224394	1350.589001	18.065459
38.201832	1341.465960	18.070477
38.388809	1347.597018	18.075495
38.508522	1349.535016	18.080512
38.205549	1350.197606	18.085530
38.221339	1353.076437	18.090547
38.369975	1360.008732	18.095565
38.551613	1371.688542	18.100583
38.570848	1369.814188	18.105600
38.760550	1370.068712	18.110618
38.549984	1379.142931	18.115635
38.804785	1368.042180	18.120653
38.812703	1371.701724	18.125671
38.879271	1375.623537	18.130688
38.498476	1372.473402	18.135706
38.809049	1380.428221	18.140723
39.384681	1393.274313	18.145741
38.793631	1385.063428	18.150759
39.009658	1392.089385	18.155776
39.429970	1388.117084	18.160794
39.186443	1392.361736	18.165811
39.624815	1398.437892	18.170829
39.455332	1394.598443	18.175847
39.510739	1383.863243	18.180864
39.601576	1390.545773	18.185882
39.129760	1384.115138	18.190899
39.517141	1382.309697	18.195917
39.666267	1387.622995	18.200935
39.482004	1391.968874	18.205952
39.868114	1389.712349	18.210970
39.734752	1379.464134	18.215987
39.467330	1365.235232	18.221005
39.405181	1382.706047	18.226023
39.613647	1383.052324	18.231040
39.437731	1388.018597	18.236058
39.376614	1383.972930	18.241075
39.749441	1387.976451	18.246093
39.692655	1395.145871	18.251111
39.591914	1382.071278	18.256128
39.868444	1381.807354	18.261146
39.545064	1390.148060	18.266163
39.705501	1389.940080	18.271181
39.606930	1409.502585	18.276199
39.982667	1415.168774	18.281216
40.492119	1420.804680	18.286234
40.142225	1422.534933	18.291251
40.608158	1415.390237	18.296269
40.149779	1425.686495	18.301287
40.188063	1418.630470	18.306304
40.665668	1401.180216	18.311322
40.450874	1412.934399	18.316339
40.736659	1408.699015	18.321357
40.657207	1404.129176	18.326375
40.308565	1407.844242	18.331392
40.697232	1409.882384	18.336410
40.289034	1406.171618	18.341427
40.829950	1408.302820	18.346445
40.612665	1415.206902	18.351463
41.045911	1408.029427	18.356480
40.538801	1404.422425	18.361498
40.409541	1410.978284	18.366515
40.389108	1405.720755	18.371533
40.780003	1409.074525	18.376551
40.563954	1411.367765	18.381568
40.730429	1417.896516	18.386586
40.395322	1415.701785	18.391603
40.692531	1418.113930	18.396621
40.761845	1436.637308	18.401639
40.936003	1433.356577	18.406656
41.121116	1444.931752	18.411674
40.801016	1436.662878	18.416691
41.434646	1436.766234	18.421709
40.995095	1442.104930	18.426727
40.938509	1439.898390	18.431744
41.152170	1439.906186	18.436762
41.245295	1447.784438	18.441779
41.265252	1452.161652	18.446797
41.377529	1451.875962	18.451815
41.257084	1463.672293	18.456832
41.730252	1460.872026	18.461850
41.849269	1472.328121	18.466867
41.948284	1467.146651	18.471885
41.751198	1452.673197	18.476903
41.634401	1461.234238	18.481920
42.101012	1453.379360	18.486938
41.916607	1451.378912	18.491955
41.818365	1460.662904	18.496973
41.875772	1452.126962	18.501991
41.741384	1458.462729	18.507008
41.582144	1456.578284	18.512026
41.574100	1454.970102	18.517043
41.669311	1449.271675	18.522061
41.652291	1446.377315	18.527079
41.771411	1453.781304	18.532096
42.120195	1456.289567	18.537114
42.249938	1468.952671	18.542131
42.288854	1472.818850	18.547149
42.290347	1474.153569	18.552167
42.647272	1478.550909	18.557184
42.586464	1461.487385	18.562202
42.335659	1466.171848	18.567219
42.010802	1472.755027	18.572237
42.461994	1470.305321	18.577255
42.592206	1468.565158	18.582272
42.754783	1458.952481	18.587290
42.761716	1466.506487	18.592307
42.806998	1469.611119	18.597325
42.814541	1468.464416	18.602343
42.718319	1471.783586	18.607360
42.669985	1470.383649	18.612378
42.498734	1464.944455	18.617395
42.864494	1456.376282	18.622413
42.851559	1457.280899	18.627431
42.723063	1461.450853	18.632448
42.818889	1453.669483	18.637466
42.592773	1470.323307	18.642483
42.562236	1467.743475	18.647501
42.776910	1466.583458	18.652519
43.097908	1484.054679	18.657536
43.467058	1485.594091	18.662554
43.355266	1483.714879	18.667571
43.218816	1486.478577	18.672589
43.363326	1481.791797	18.677607
43.481846	1478.428202	18.682624
43.729066	1472.242193	18.687642
43.301648	1479.169549	18.692659
43.733036	1473.156839	18.697677
43.495829	1483.346110	18.702695
43.507597	1475.887090	18.707712
43.777593	1471.389060	18.712730
43.943337	1477.245755	18.717747
43.727211	1483.108259	18.722765
43.759543	1477.271289	18.727783
43.774270	1472.014578	18.732800
44.063630	1476.457151	18.737818
43.607063	1478.409147	18.742835
43.656717	1483.886286	18.747853
44.112885	1478.330467	18.752871
44.111427	1484.071185	18.757888
44.220907	1476.770522	18.762906
44.040956	1476.116917	18.767923
44.043095	1475.090976	18.772941
44.413385	1476.705950	18.777959
43.800281	1476.659432	18.782976
44.327701	1482.504000	18.787994
44.322833	1472.620737	18.793011
44.116876	1480.801191	18.798029
44.188624	1478.211745	18.803047
44.163125	1491.208306	18.808064
44.088606	1486.602964	18.813082
44.376608	1500.387016	18.818099
44.335360	1503.839645	18.823117
44.450190	1504.863229	18.828135
44.595107	1508.343679	18.833152
44.788112	1498.584230	18.838170
44.783763	1516.090358	18.843187
44.329460	1511.162284	18.848205
44.692458	1495.083636	18.853223
44.490968	1504.803451	18.858240
44.477797	1501.264693	18.863258
44.993440	1513.138748	18.868275
44.948066	1518.431875	18.873293
45.223102	1520.528747	18.878311
45.259336	1521.211115	18.883328
45.620115	1519.621243	18.888346
45.254826	1517.494315	18.893363
45.109778	1522.701975	18.898381
45.519198	1513.180225	18.903399
45.244112	1518.537519	18.908416
45.492703	1522.866530	18.913434
45.572451	1516.463581	18.918451
45.252739	1514.244350	18.923469
45.974602	1512.547766	18.928487
45.375811	1509.945949	18.933504
45.272683	1507.408972	18.938522
45.311580	1501.908645	18.943539
45.208827	1518.073088	18.948557
45.381944	1510.042972	18.953575
45.436679	1507.708636	18.958592
45.695308	1509.277882	18.963610
45.478156	1515.049037	18.968627
45.822609	1531.576213	18.973645
45.976710	1530.798012	18.978663
45.546108	1529.549106	18.983680
45.851700	1536.160384	18.988698
46.190481	1534.106873	18.993715
46.070898	1527.286825	18.998733
46.040374	1529.383935	19.003751
46.026137	1541.870690	19.008768
46.013909	1534.308082	19.013786
45.960786	1534.149130	19.018803
45.932347	1533.358324	19.023821
46.595404	1542.403906	19.028839
46.559434	1558.384416	19.033856
46.628237	1557.199767	19.038874
46.628706	1560.153600	19.043891
46.434510	1568.960276	19.048909
47.099008	1556.530126	19.053927
46.509776	1555.750890	19.058944
46.738430	1550.366174	19.063962
46.735297	1550.477153	19.068979
46.672993	1552.434045	19.073997
46.766477	1546.776881	19.079015
46.948682	1557.980193	19.084032
46.956458	1540.763901	19.089050
47.307301	1537.461954	19.094067
46.677112	1546.986604	19.099085
47.159354	1537.822737	19.104103
47.092831	1546.079343	19.109120
46.869886	1547.616271	19.114138
46.903432	1548.116020	19.119155
46.895800	1547.820596	19.124173
47.055104	1556.944617	19.129191
47.334912	1566.605310	19.134208
47.652726	1577.850638	19.139226
47.407475	1580.391445	19.144243
47.114947	1583.435083	19.149261
47.460401	1569.751232	19.154279
47.807493	1578.656676	19.159296
47.324339	1573.272323	19.164314
47.326325	1577.254729	19.169331
47.335538	1578.966956	19.174349
47.300297	1577.672270	19.179367
47.464152	1584.536011	19.184384
47.588357	1590.112029	19.189402
47.817025	1604.154712	19.194419
47.997116	1604.839932	19.199437
48.109178	1592.593600	19.204455
48.095059	1598.431002	19.209472
47.861330	1600.799603	19.214490
48.142396	1606.237594	19.219507
48.083623	1608.613670	19.224525
47.895957	1608.633458	19.229543
47.975445	1615.576619	19.234560
48.334653	1621.201266	19.239578
48.454909	1623.562094	19.244595
48.647600	1628.761383	19.249613
48.523788	1623.340002	19.254631
48.757476	1621.574246	19.259648
48.575511	1626.648826	19.264666
48.875121	1623.645179	19.269683
48.694618	1627.293085	19.274701
48.974460	1624.920531	19.279719
48.713936	1624.658167	19.284736
48.543229	1630.516804	19.289754
49.020357	1618.551292	19.294771
48.510581	1621.729747	19.299789
48.710878	1613.212507	19.304807
48.764307	1619.904103	19.309824
48.741435	1616.527781	19.314842
49.038638	1611.498453	19.319859
48.791208	1626.943894	19.324877
48.893543	1618.334604	19.329895
48.947797	1639.195870	19.334912
49.190429	1643.055615	19.339930
48.976038	1635.174140	19.344947
49.560101	1639.129050	19.349965
49.650303	1642.176225	19.354983
49.429092	1638.101777	19.360000
49.854625	1641.901486	19.365018
49.925070	1633.372895	19.370035
49.698833	1642.127791	19.375053
49.895228	1633.507005	19.380071
49.952132	1633.037427	19.385088
49.710485	1635.205291	19.390106
49.860937	1627.194430	19.395123
49.818953	1630.621952	19.400141
49.653219	1634.441132	19.405159
49.947324	1635.610383	19.410176
49.559956	1628.248157	19.415194
49.427303	1630.888207	19.420211
50.370891	1652.198013	19.425229
50.241916	1655.392926	19.430247
50.260931	1657.166752	19.435264
50.217793	1657.555364	19.440282
50.223605	1646.190244	19.445299
50.419132	1646.361813	19.450317
50.636726	1648.142591	19.455335
50.636452	1648.735972	19.460352
50.776410	1652.952538	19.465370
51.277512	1650.763285	19.470387
51.191368	1651.019735	19.475405
50.952223	1645.401706	19.480423
50.699195	1627.575829	19.485440
50.565945	1629.057773	19.490458
50.900193	1642.074174	19.495475
50.747607	1645.676711	19.500493
50.805454	1646.311537	19.505511
51.093351	1646.004813	19.510528
50.945601	1649.767547	19.515546
50.967302	1639.971576	19.520563
50.979412	1649.569849	19.525581
51.089424	1645.061970	19.530599
51.190914	1649.473876	19.535616
50.945205	1650.998578	19.540634
51.131315	1647.132114	19.545651
50.788743	1663.251974	19.550669
51.147163	1660.415892	19.555687
51.369185	1681.345762	19.560704
51.146717	1693.461092	19.565722
51.411901	1687.707722	19.570739
51.067254	1692.798182	19.575757
51.785000	1689.120340	19.580775
51.650262	1700.846468	19.585792
51.840106	1708.324760	19.590810
52.245860	1699.321046	19.595827
51.783942	1706.165496	19.600845
51.837575	1705.185174	19.605863
52.106973	1698.058342	19.610880
51.894933	1713.684544	19.615898
51.751174	1697.066063	19.620915
52.092277	1706.849835	19.625933
52.005004	1695.467618	19.630951
52.195951	1695.611498	19.635968
51.986247	1699.084081	19.640986
52.142112	1700.132846	19.646003
52.032282	1701.585902	19.651021
52.042241	1711.212947	19.656039
51.837139	1718.307757	19.661056
52.000265	1728.346474	19.666074
52.057018	1721.767147	19.671091
52.172775	1732.917797	19.676109
52.681537	1752.610186	19.681127
52.925687	1753.228632	19.686144
52.931063	1760.691485	19.691162
52.782359	1748.403593	19.696179
53.080379	1745.813593	19.701197
53.413130	1738.531711	19.706215
53.376863	1735.223725	19.711232
53.051099	1736.530520	19.716250
53.318028	1737.767127	19.721267
53.467018	1739.312437	19.726285
53.098149	1743.463075	19.731303
53.283061	1735.797103	19.736320
53.147627	1747.201471	19.741338
53.536974	1741.946316	19.746355
53.514813	1740.141486	19.751373
53.328673	1747.144990	19.756391
53.859109	1733.757269	19.761408
53.456778	1736.852743	19.766426
53.113902	1734.760168	19.771443
53.596135	1732.914678	19.776461
53.567687	1738.337782	19.781479
53.693744	1735.089732	19.786496
53.634201	1745.415597	19.791514
53.720251	1760.402124	19.796531
53.721509	1764.772858	19.801549
53.845681	1769.995479	19.806567
53.956189	1766.636233	19.811584
53.928411	1759.391539	19.816602
54.289261	1758.546423	19.821619
54.058870	1764.483825	19.826637
54.153578	1766.646674	19.831655
53.968938	1757.823216	19.836672
54.163344	1771.786157	19.841690
54.358629	1784.420345	19.846707
54.307371	1785.870601	19.851725
54.526143	1785.091788	19.856743
54.516659	1779.949211	19.861760
54.490702	1780.391957	19.866778
54.666546	1779.749219	19.871795
54.551907	1780.130031	19.876813
54.739917	1779.952469	19.881831
55.139688	1782.500179	19.886848
54.678571	1798.632306	19.891866
55.272750	1796.927174	19.896883
55.224666	1799.724501	19.901901
55.032253	1809.010712	19.906919
55.640747	1796.633298	19.911936
55.310256	1798.622504	19.916954
55.417782	1791.394602	19.921971
55.093877	1786.411434	19.926989
55.387195	1792.803807	19.932007
55.725712	1795.162234	19.937024
55.508706	1797.626090	19.942042
55.495339	1797.255813	19.947059
55.746087	1802.215734	19.952077
55.598980	1797.631080	19.957095
55.960121	1797.066792	19.962112
55.462722	1801.534108	19.967130
55.593622	1794.801195	19.972147
55.683124	1799.038275	19.977165
55.158789	1797.311625	19.982183
55.899257	1790.117725	19.987200
55.623397	1800.843384	19.992218
55.800747	1809.589175	19.997235
56.025031	1814.890899	20.002253
56.072673	1816.486710	20.007271
56.225600	1811.874274	20.012288
56.113822	1818.503302	20.017306
56.087790	1811.826375	20.022323
56.163783	1811.659941	20.027341
55.848870	1820.753786	20.032359
56.495983	1817.506649	20.037376
56.560095	1831.909657	20.042394
56.447634	1847.599369	20.047411
56.213755	1842.337073	20.052429
56.580710	1847.461955	20.057447
56.447475	1844.418362	20.062464
56.839272	1848.598921	20.067482
56.590668	1848.416751	20.072499
56.903920	1844.659840	20.077517
56.916797	1855.290083	20.082535
57.154466	1856.698516	20.087552
57.076980	1861.223549	20.092570
57.198853	1857.155596	20.097587
57.305303	1853.150006	20.102605
57.592468	1857.107009	20.107623
57.525331	1861.668302	20.112640
57.099559	1869.946275	20.117658
57.339804	1864.064184	20.122675
57.277049	1858.364973	20.127693
57.681867	1865.579481	20.132711
57.615123	1854.392788	20.137728
57.646617	1855.151648	20.142746
57.562978	1863.644601	20.147763
57.888466	1866.629935	20.152781
57.769406	1881.194049	20.157799
58.047467	1876.637856	20.162816
57.879909	1878.961475	20.167834
58.300743	1885.785322	20.172851
58.212765	1885.426660	20.177869
58.114521	1888.285460	20.182887
58.062500	1880.145060	20.187904
58.374112	1880.099736	20.192922
58.318795	1882.825616	20.197939
58.544408	1879.063408	20.202957
58.777959	1884.647741	20.207975
58.587165	1875.512749	20.212992
58.506923	1878.706426	20.218010
58.221641	1878.981260	20.223027
58.601593	1881.207012	20.228045
58.345005	1874.543867	20.233063
58.730337	1884.393436	20.238080
58.961787	1898.458010	20.243098
58.820019	1898.366506	20.248115
59.037421	1898.200147	20.253133
58.700029	1897.731989	20.258151
59.050123	1895.973331	20.263168
58.978751	1897.032240	20.268186
59.240456	1899.967548	20.273203
59.678156	1889.952031	20.278221
59.059903	1889.631747	20.283239
59.118960	1897.474475	20.288256
59.164636	1904.072707	20.293274
59.462560	1897.632497	20.298291
59.863467	1910.326282	20.303309
59.451649	1906.931564	20.308327
59.504444	1913.402455	20.313344
59.629099	1925.792111	20.318362
59.563228	1920.550973	20.323379
59.848729	1920.787435	20.328397
59.809456	1923.277286	20.333415
59.783852	1933.698964	20.338432
60.098493	1923.756239	20.343450
60.391015	1923.846435	20.348467
60.174681	1913.412010	20.353485
60.363464	1921.960410	20.358503
60.429842	1914.947154	20.363520
59.889851	1918.212418	20.368538
60.023716	1917.954920	20.373555
60.128567	1924.846914	20.378573
60.376309	1934.332912	20.383591
60.265505	1947.346242	20.388608
60.659451	1949.809674	20.393626
60.491687	1946.342236	20.398643
60.542148	1944.226267	20.403661
60.633029	1944.429912	20.408679
60.580564	1942.519323	20.413696
60.594828	1939.260239	20.418714
60.807877	1954.003085	20.423731
60.954972	1957.855682	20.428749
60.468938	1955.599171	20.433767
60.920623	1960.802416	20.438784
60.741814	1958.687426	20.443802
60.991492	1974.137824	20.448819
61.319919	1985.792026	20.453837
61.572197	1986.424995	20.458855
61.778452	1983.975486	20.463872
61.678416	1982.719262	20.468890
61.454540	1992.281875	20.473907
61.675995	1981.665636	20.478925
61.663278	1988.118351	20.483943
61.939344	1982.647225	20.488960
61.993443	1981.379628	20.493978
61.966027	1994.143315	20.498995
62.239727	1979.296321	20.504013
62.137651	1981.051162	20.509031
61.681621	1984.622113	20.514048
61.858705	1986.002119	20.519066
62.231875	1985.988238	20.524083
62.389316	1973.639903	20.529101
61.946327	1983.621648	20.534119
62.461193	1995.221582	20.539136
62.569282	2000.771834	20.544154
62.300051	2014.466311	20.549171
62.424657	2008.999823	20.554189
62.157068	2004.446499	20.559207
62.166395	2005.290871	20.564224
62.370115	2008.980022	20.569242
62.495693	2020.381797	20.574259
63.078490	2024.387487	20.579277
62.931424	2030.611816	20.584295
63.147783	2038.953999	20.589312
62.956397	2026.931347	20.594330
63.170772	2030.262224	20.599347
63.289523	2035.012379	20.604365
63.062254	2031.689893	20.609383
63.142009	2033.624720	20.614400
63.332283	2033.853918	20.619418
63.041923	2037.856696	20.624435
63.446649	2032.879939	20.629453
63.229436	2052.843487	20.634471
63.629781	2057.912737	20.639488
63.845414	2054.240412	20.644506
63.990350	2058.781360	20.649523
63.713618	2066.310354	20.654541
63.987504	2057.080829	20.659559
64.010562	2055.688666	20.664576
63.943422	2055.976878	20.669594
63.994873	2054.021695	20.674611
64.137652	2054.539166	20.679629
64.051796	2053.353316	20.684647
64.141591	2057.012876	20.689664
64.356732	2047.271774	20.694682
64.270519	2048.935785	20.699699
64.353037	2049.620435	20.704717
64.054584	2044.794183	20.709735
64.611064	2063.605295	20.714752
64.819440	2071.456410	20.719770
65.007364	2070.190063	20.724787
64.808048	2060.554509	20.729805
64.866733	2067.005603	20.734823
64.874456	2064.643799	20.739840
65.167581	2055.206144	20.744858
64.953692	2064.669407	20.749875
65.028466	2059.251690	20.754893
65.066509	2056.323411	20.759911
65.082826	2053.234407	20.764928
65.472131	2058.586253	20.769946
65.269817	2056.228749	20.774963
65.552192	2056.109079	20.779981
65.305895	2059.199249	20.784999
65.082756	2062.364712	20.790016
65.243095	2065.173812	20.795034
65.418793	2079.808965	20.800051
65.704288	2083.494868	20.805069
65.737958	2077.338744	20.810087
65.716672	2086.178715	20.815104
65.802082	2075.309035	20.820122
65.658169	2079.711917	20.825139
65.926927	2084.807973	20.830157
66.459591	2089.051867	20.835175
66.393046	2092.423338	20.840192
66.453332	2091.612380	20.845210
66.472422	2082.122699	20.850227
66.126465	2079.519301	20.855245
66.370998	2090.309284	20.860263
66.507920	2099.124630	20.865280
66.532789	2089.621420	20.870298
66.536085	2096.756520	20.875315
66.905949	2095.676447	20.880333
66.864587	2089.513065	20.885351
66.798190	2095.153632	20.890368
67.072067	2097.922970	20.895386
67.107232	2090.917660	20.900403
67.284168	2084.906493	20.905421
67.014991	2082.660385	20.910439
66.837796	2092.913246	20.915456
66.978379	2088.848639	20.920474
66.946189	2104.532390	20.925491
66.810072	2116.214821	20.930509
66.963669	2114.126958	20.935527
66.869425	2107.053425	20.940544
67.572310	2122.954119	20.945562
67.664251	2142.421490	20.950579
67.938903	2142.359829	20.955597
67.978541	2146.503765	20.960615
67.544735	2141.300911	20.965632
67.744615	2134.939000	20.970650
67.459011	2140.746261	20.975667
67.455358	2139.759055	20.980685
67.708390	2135.266657	20.985703
68.015857	2163.638134	20.990720
68.038579	2156.505342	20.995738
68.130502	2161.685760	21.000755
68.462653	2160.573684	21.005773
68.367489	2157.047562	21.010791
68.169104	2166.066632	21.015808
68.781451	2162.313583	21.020826
68.576060	2162.468680	21.025843
68.519987	2161.142480	21.030861
68.810324	2155.369265	21.035879
68.631331	2173.916288	21.040896
69.093397	2168.015341	21.045914
69.027028	2175.095043	21.050931
69.468863	2187.211425	21.055949
69.133191	2186.900789	21.060967
68.938875	2187.353978	21.065984
69.288419	2189.297312	21.071002
69.343779	2198.766065	21.076019
69.356376	2193.926059	21.081037
69.656316	2183.272233	21.086055
69.100963	2190.484880	21.091072
69.218439	2182.614612	21.096090
69.373662	2189.249545	21.101107
69.392725	2200.551248	21.106125
69.701982	2195.848100	21.111143
69.500512	2209.964542	21.116160
70.141168	2209.675475	21.121178
70.047094	2214.016978	21.126195
69.915242	2204.339283	21.131213
69.912052	2211.406007	21.136231
70.417978	2229.171074	21.141248
70.634319	2223.456697	21.146266
70.293681	2217.040050	21.151283
70.255471	2230.654540	21.156301
70.653520	2230.510548	21.161319
70.485956	2238.811608	21.166336
70.359853	2230.247059	21.171354
70.390422	2229.869933	21.176371
70.465406	2232.799652	21.181389
70.491749	2231.252322	21.186407
70.660338	2252.418410	21.191424
71.242331	2246.110582	21.196442
71.178062	2251.340592	21.201459
71.403380	2253.113916	21.206477
71.531168	2246.640108	21.211495
71.423614	2253.568455	21.216512
71.344948	2249.111892	21.221530
71.039178	2255.263173	21.226547
71.145558	2266.166295	21.231565
71.545283	2253.694833	21.236583
71.534185	2258.619906	21.241600
71.359151	2266.253077	21.246618
71.545489	2265.816982	21.251635
71.566930	2276.212599	21.256653
71.920332	2275.794677	21.261671
71.907344	2278.084814	21.266688
72.532928	2276.743999	21.271706
71.726696	2278.605345	21.276723
72.004483	2280.837587	21.281741
71.940754	2277.076161	21.286759
72.018647	2294.500815	21.291776
72.279183	2294.037388	21.296794
72.575741	2299.776152	21.301811
72.128250	2304.819677	21.306829
72.415960	2294.688425	21.311847
72.294361	2294.218218	21.316864
72.574853	2295.746259	21.321882
73.140892	2313.233793	21.326899
72.962195	2319.636726	21.331917
73.187929	2320.583126	21.336935
73.305572	2323.285300	21.341952
73.489717	2318.475360	21.346970
73.215205	2300.156668	21.351987
72.916969	2310.261231	21.357005
73.360558	2306.061032	21.362023
73.137167	2320.187285	21.367040
73.071894	2319.301187	21.372058
73.330991	2326.421799	21.377075
73.328529	2322.410970	21.382093
73.587666	2318.763378	21.387111
73.462211	2335.837859	21.392128
73.896853	2335.208460	21.397146
74.155344	2333.069525	21.402163
74.074216	2343.367535	21.407181
74.086703	2328.699785	21.412199
74.063959	2331.262862	21.417216
74.350701	2329.274172	21.422234
74.414099	2324.167432	21.427251
74.237519	2328.900526	21.432269
74.526609	2326.920938	21.437287
74.487759	2325.778247	21.442304
74.349270	2322.312489	21.447322
74.938508	2328.901993	21.452339
74.699476	2346.300297	21.457357
75.269874	2338.192176	21.462375
75.187131	2344.665390	21.467392
75.049535	2331.075103	21.472410
75.168906	2326.903286	21.477427
75.104054	2339.925526	21.482445
75.322754	2340.620545	21.487463
75.571064	2341.528716	21.492480
75.477908	2341.890414	21.497498
75.485266	2346.459168	21.502515
75.431050	2347.187210	21.507533
75.523124	2349.934396	21.512551
75.857082	2347.158825	21.517568
75.543620	2344.521924	21.522586
76.056177	2348.841599	21.527603
75.619139	2348.783440	21.532621
75.892414	2348.078174	21.537639
75.867406	2348.968935	21.542656
75.656438	2346.151966	21.547674
76.228040	2357.664404	21.552691
75.844752	2373.459862	21.557709
76.481279	2372.492899	21.562727
76.164738	2376.439864	21.567744
76.320686	2378.003082	21.572762
76.307653	2369.266219	21.577779
76.113853	2381.712085	21.582797
76.520407	2388.954940	21.587815
76.332271	2387.721872	21.592832
76.438066	2393.171612	21.597850
76.976230	2399.731222	21.602867
76.515774	2404.814665	21.607885
76.583993	2410.377565	21.612903
76.716459	2423.201877	21.617920
77.018259	2426.809569	21.622938
77.256069	2419.431734	21.627955
77.193274	2422.565983	21.632973
77.172545	2431.573306	21.637991
77.636686	2437.169252	21.643008
77.553378	2435.364404	21.648026
77.774894	2448.178025	21.653043
77.749677	2442.643208	21.658061
77.965877	2446.207424	21.663079
77.771373	2423.713385	21.668096
77.935445	2440.029632	21.673114
78.000593	2434.206177	21.678131
77.684487	2439.200879	21.683149
77.851794	2437.076128	21.688167
78.105704	2444.964503	21.693184
78.292226	2452.083840	21.698202
78.141536	2461.471196	21.703219
78.795592	2461.378869	21.708237
78.593985	2454.157802	21.713255
78.814311	2453.533363	21.718272
78.792920	2458.305449	21.723290
78.836517	2448.975870	21.728307
78.695022	2456.433475	21.733325
78.816829	2453.167022	21.738343
79.343785	2462.912806	21.743360
79.226435	2478.307167	21.748378
79.335405	2471.851987	21.753395
79.061582	2481.214341	21.758413
79.336961	2475.670584	21.763431
79.343724	2470.313828	21.768448
79.554947	2476.138524	21.773466
79.256740	2465.855387	21.778483
79.007016	2469.564737	21.783501
79.499757	2492.157650	21.788519
80.072406	2499.674510	21.793536
79.876362	2501.207330	21.798554
80.295366	2502.808504	21.803571
79.965873	2505.709718	21.808589
80.151395	2505.854451	21.813607
80.409548	2497.779094	21.818624
80.140725	2503.766907	21.823642
80.308370	2497.763360	21.828659
80.432296	2509.929458	21.833677
80.586992	2515.712472	21.838695
80.884951	2519.317625	21.843712
80.916770	2525.419594	21.848730
80.920647	2522.629111	21.853747
80.699338	2529.366978	21.858765
80.986817	2530.199628	21.863783
81.046639	2526.049660	21.868800
80.869830	2527.380659	21.873818
80.985760	2524.538013	21.878835
81.189726	2525.424694	21.883853
81.147566	2541.590094	21.888871
81.414617	2542.659471	21.893888
81.410189	2539.374784	21.898906
81.693051	2537.897949	21.903923
81.695625	2541.987783	21.908941
81.767024	2541.623230	21.913959
81.676116	2533.633763	21.918976
81.675326	2548.299933	21.923994
82.384193	2551.279346	21.929011
82.514114	2560.222250	21.934029
82.431937	2569.406478	21.939047
82.277614	2564.245199	21.944064
82.186629	2566.244539	21.949082
82.381470	2561.224571	21.954099
82.424787	2563.575411	21.959117
82.579032	2560.215519	21.964135
82.783798	2559.079068	21.969152
82.471305	2557.474004	21.974170
82.459941	2561.648068	21.979187
82.401333	2571.582917	21.984205
82.902182	2581.184498	21.989223
83.003956	2580.786810	21.994240
83.288185	2587.272409	21.999258
83.362681	2575.154339	22.004275
83.530737	2577.741398	22.009293
83.170398	2582.673594	22.014311
83.285145	2577.710276	22.019328
83.163420	2592.657261	22.024346
83.561208	2603.994934	22.029363
84.035743	2603.801160	22.034381
83.587339	2587.525949	22.039399
83.812614	2599.250265	22.044416
83.879769	2592.407049	22.049434
84.147141	2582.581781	22.054451
84.353101	2584.190883	22.059469
84.186060	2584.365260	22.064487
84.509640	2580.994780	22.069504
84.310653	2585.198062	22.074522
84.798998	2585.396641	22.079539
84.398569	2593.535291	22.084557
84.556838	2598.380435	22.089575
84.543950	2605.174250	22.094592
84.633570	2610.913774	22.099610
84.636593	2613.037348	22.104627
84.849040	2612.363634	22.109645
85.020822	2608.142563	22.114663
84.989120	2603.817465	22.119680
85.149850	2629.397349	22.124698
85.333092	2635.822944	22.129715
85.784340	2630.043461	22.134733
85.607730	2636.313628	22.139751
85.678897	2635.986981	22.144768
85.324109	2637.077435	22.149786
85.523031	2631.599188	22.154803
85.888502	2635.743003	22.159821
85.753121	2639.942707	22.164839
86.461574	2635.442399	22.169856
86.050971	2663.282636	22.174874
85.996181	2655.530507	22.179891
86.275493	2650.478427	22.184909
86.091641	2660.754740	22.189927
86.483162	2658.768637	22.194944
86.395051	2657.794552	22.199962
86.372977	2654.310605	22.204979
86.736967	2665.268542	22.209997
86.702316	2692.283374	22.215015
86.948337	2679.198028	22.220032
86.862557	2678.693829	22.225050
86.916562	2683.829805	22.230067
86.834849	2683.530116	22.235085
86.925953	2683.310826	22.240103
87.302747	2693.676608	22.245120
87.068379	2705.138016	22.250138
86.872709	2699.923170	22.255155
87.220764	2701.917290	22.260173
87.482479	2704.054251	22.265191
87.764622	2715.795038	22.270208
87.892791	2725.255889	22.275226
87.984059	2726.207467	22.280243
88.237191	2724.132441	22.285261
88.388717	2724.938927	22.290279
87.918969	2726.530160	22.295296
88.212265	2728.580150	22.300314
88.253193	2725.020103	22.305331
88.199776	2724.356218	22.310349
88.142547	2740.511519	22.315367
88.245935	2744.588859	22.320384
88.328688	2751.238440	22.325402
88.181244	2756.683534	22.330419
88.493933	2756.294033	22.335437
88.662191	2775.803863	22.340455
88.921440	2768.337333	22.345472
89.308992	2766.389709	22.350490
89.512176	2770.782903	22.355507
89.413489	2761.882445	22.360525
89.483490	2770.519178	22.365543
89.646900	2760.814148	22.370560
89.684544	2767.243522	22.375578
89.501004	2751.873741	22.380595
89.672638	2755.867869	22.385613
89.670387	2755.710453	22.390631
89.953398	2758.238612	22.395648
89.929841	2775.464917	22.400666
90.011066	2778.756701	22.405683
90.186026	2776.100501	22.410701
89.809301	2778.930210	22.415719
90.241666	2788.274300	22.420736
90.509879	2788.115804	22.425754
90.464977	2798.641984	22.430771
90.539721	2801.641267	22.435789
90.468986	2806.963971	22.440807
90.524899	2805.077445	22.445824
90.838431	2805.789278	22.450842
90.770304	2796.915605	22.455859
90.672722	2805.471140	22.460877
91.449250	2825.211395	22.465895
91.780274	2819.377980	22.470912
91.562678	2828.501367	22.475930
91.549280	2824.126024	22.480947
92.099084	2836.781506	22.485965
91.762766	2828.489261	22.490983
92.019875	2821.464892	22.496000
91.992953	2826.392584	22.501018
91.908904	2823.489501	22.506035
91.878530	2822.064569	22.511053
91.930701	2824.884319	22.516071
92.409930	2824.538321	22.521088
92.130198	2824.730245	22.526106
92.029611	2830.742471	22.531123
92.207335	2848.218397	22.536141
92.094616	2852.626079	22.541159
92.089315	2857.285303	22.546176
92.041191	2861.001218	22.551194
92.469489	2871.434830	22.556211
92.631051	2872.915161	22.561229
92.686701	2885.025866	22.566247
92.845216	2896.662932	22.571264
92.857224	2906.044126	22.576282
92.684826	2908.580088	22.581299
93.439769	2904.157691	22.586317
93.291128	2926.955163	22.591335
93.846906	2922.756291	22.596352
94.049926	2922.355457	22.601370
94.163014	2927.138291	22.606387
94.538040	2921.184374	22.611405
94.413417	2912.407811	22.616423
94.561729	2903.617162	22.621440
94.419970	2894.047944	22.626458
94.281570	2884.601294	22.631475
94.612468	2889.934081	22.636493
94.483246	2898.267349	22.641511
94.344488	2900.441435	22.646528
94.559582	2901.765098	22.651546
94.680249	2903.576875	22.656563
95.069830	2914.057569	22.661581
94.995110	2908.530315	22.666599
95.210598	2911.633947	22.671616
94.907985	2910.327139	22.676634
95.194579	2908.268975	22.681651
95.216162	2903.206454	22.686669
94.725714	2907.464657	22.691687
95.190593	2917.229824	22.696704
95.327925	2929.971683	22.701722
95.472993	2942.421987	22.706739
95.505891	2927.343435	22.711757
95.432909	2931.811226	22.716775
95.292831	2949.024278	22.721792
95.752585	2957.925497	22.726810
95.800470	2958.202126	22.731827
96.332839	2949.092862	22.736845
96.221495	2953.737060	22.741863
96.225581	2959.508949	22.746880
96.276115	2966.460299	22.751898
96.183445	2983.148403	22.756915
96.579825	2982.603844	22.761933
96.657891	2977.466230	22.766951
96.579313	2986.069390	22.771968
96.909125	2990.802718	22.776986
96.685459	3006.921049	22.782003
97.261724	3007.737166	22.787021
97.052230	3009.837065	22.792039
97.247773	3005.795255	22.797056
97.418765	3011.942000	22.802074
97.095281	3025.001848	22.807091
97.257990	3024.623068	22.812109
97.296734	3033.132238	22.817127
97.785963	3032.696309	22.822144
98.068369	3038.809936	22.827162
97.616747	3059.265576	22.832179
98.153841	3047.987280	22.837197
98.177790	3049.952999	22.842215
98.659123	3049.278435	22.847232
98.827900	3047.670986	22.852250
98.641426	3056.751769	22.857267
98.607361	3045.174199	22.862285
98.603237	3045.982840	22.867303
98.706488	3054.409386	22.872320
99.002830	3064.724787	22.877338
99.227796	3073.470095	22.882355
99.168673	3075.660210	22.887373
99.014820	3085.995217	22.892391
98.921453	3093.382471	22.897408
99.203461	3084.473079	22.902426
99.245356	3097.801173	22.907443
99.010382	3106.810629	22.912461
99.272492	3107.975494	22.917479
99.443082	3110.227687	22.922496
99.848438	3118.897590	22.927514
99.988917	3127.062728	22.932531
100.188585	3132.311868	22.937549
100.431589	3130.853816	22.942567
100.221450	3126.752053	22.947584
100.446855	3119.868217	22.952602
100.107529	3127.612547	22.957619
100.684681	3135.226816	22.962637
100.786630	3149.467185	22.967655
100.590290	3148.342649	22.972672
101.191982	3137.028991	22.977690
100.841445	3145.169589	22.982707
101.472214	3144.979892	22.987725
101.181586	3135.077081	22.992743
100.872662	3147.869637	22.997760
101.773343	3152.447849	23.002778
101.631912	3162.525321	23.007795
101.994727	3155.793665	23.012813
102.248202	3165.042715	23.017831
101.847241	3145.524581	23.022848
101.959107	3139.075023	23.027866
101.827636	3154.888770	23.032883
102.296207	3157.091420	23.037901
102.183681	3156.824925	23.042919
101.989179	3157.366536	23.047936
102.133995	3149.163352	23.052954
102.157548	3159.619118	23.057971
102.689794	3175.594662	23.062989
102.699159	3178.932425	23.068007
102.737660	3186.434900	23.073024
103.027559	3186.127842	23.078042
102.795885	3181.044707	23.083059
103.083616	3187.214365	23.088077
102.793122	3180.032093	23.093095
102.620270	3193.507312	23.098112
103.393474	3199.039599	23.103130
103.357757	3211.290995	23.108147
102.670459	3208.298715	23.113165
103.402309	3214.860033	23.118183
103.465346	3234.228936	23.123200
104.002273	3228.233931	23.128218
104.100894	3227.322270	23.133235
104.221328	3224.908048	23.138253
104.269486	3231.484290	23.143271
104.490512	3243.632611	23.148288
104.780675	3248.362713	23.153306
104.689566	3248.023447	23.158323
104.728417	3258.887188	23.163341
104.941782	3251.717967	23.168359
104.971216	3259.606933	23.173376
105.067155	3249.094705	23.178394
104.888639	3243.959089	23.183411
105.237137	3243.851213	23.188429
105.512438	3256.499232	23.193447
105.326475	3263.904128	23.198464
105.801006	3274.516990	23.203482
105.889775	3265.729123	23.208499
105.624787	3260.767929	23.213517
106.005698	3270.031910	23.218535
105.785342	3275.876719	23.223552
106.159324	3270.775009	23.228570
105.871018	3273.745679	23.233587
106.151933	3283.293508	23.238605
106.262155	3299.382211	23.243623
106.142991	3304.901971	23.248640
106.519571	3287.336216	23.253658
106.670896	3292.422497	23.258675
106.800855	3294.267584	23.263693
107.059380	3315.455642	23.268711
106.496583	3317.241312	23.273728
107.043981	3307.854942	23.278746
107.135810	3312.404478	23.283763
107.279649	3311.937102	23.288781
107.354351	3321.876859	23.293799
107.146731	3335.600622	23.298816
107.293421	3340.548767	23.303834
107.415271	3345.784835	23.308851
107.453142	3348.774170	23.313869
107.833225	3353.714387	23.318887
108.224661	3370.804059	23.323904
107.874990	3374.620683	23.328922
108.030450	3378.494378	23.333939
108.275669	3373.696741	23.338957
108.473776	3384.008684	23.343975
108.529954	3389.513795	23.348992
108.857831	3385.757445	23.354010
108.778747	3394.720681	23.359027
108.836960	3395.942560	23.364045
108.957605	3389.478922	23.369063
108.359872	3388.637796	23.374080
108.993286	3403.950778	23.379098
109.324850	3409.072153	23.384115
109.520327	3412.456731	23.389133
109.591484	3406.395313	23.394151
109.545714	3401.330513	23.399168
109.802047	3407.666101	23.404186
109.644009	3412.668023	23.409203
109.483307	3422.360430	23.414221
110.078559	3428.472825	23.419239
110.089691	3432.125977	23.424256
110.277183	3424.540946	23.429274
109.978709	3438.641891	23.434291
110.276803	3443.992576	23.439309
110.536910	3450.479088	23.444327
110.720690	3455.879136	23.449344
110.813073	3454.195172	23.454362
110.811900	3448.245998	23.459379
111.052275	3465.330874	23.464397
111.538721	3460.483033	23.469415
111.534096	3475.551391	23.474432
111.511391	3466.051705	23.479450
111.395285	3477.851839	23.484467
111.490938	3469.413137	23.489485
112.022834	3466.041623	23.494503
111.611938	3477.682502	23.499520
112.244548	3482.649718	23.504538
112.444275	3485.667531	23.509555
112.762732	3477.241480	23.514573
112.777364	3479.884119	23.519591
112.942232	3475.212588	23.524608
113.042561	3460.845856	23.529626
112.618134	3467.896597	23.534643
113.134905	3474.680868	23.539661
113.327761	3473.694556	23.544679
113.085224	3478.122602	23.549696
113.052988	3474.213993	23.554714
113.042607	3465.084817	23.559731
113.152589	3474.820327	23.564749
112.925840	3470.339173	23.569767
113.156624	3496.348094	23.574784
113.051055	3501.184061	23.579802
113.558060	3498.422404	23.584819
113.549537	3514.015328	23.589837
113.946760	3523.617769	23.594855
114.258079	3532.255171	23.599872
114.415751	3527.010321	23.604890
114.073578	3519.870676	23.609907
114.227803	3534.993257	23.614925
114.466274	3550.762378	23.619943
114.642085	3554.146889	23.624960
114.590672	3557.585714	23.629978
114.883017	3557.556016	23.634995
114.879793	3561.697483	23.640013
115.363010	3572.735257	23.645031
115.164813	3566.740970	23.650048
115.579432	3577.054032	23.655066
115.569415	3573.182973	23.660083
115.413911	3581.877299	23.665101
115.332775	3576.335057	23.670119
115.498045	3592.677416	23.675136
115.427612	3591.817307	23.680154
116.082845	3596.894656	23.685171
115.774112	3604.981609	23.690189
116.102685	3612.473817	23.695207
116.083843	3621.121635	23.700224
116.476124	3624.153679	23.705242
116.446134	3614.039589	23.710259
116.234960	3636.137547	23.715277
116.602236	3642.777878	23.720295
116.626268	3650.996103	23.725312
116.909651	3642.168284	23.730330
117.030871	3645.040537	23.735347
116.860639	3670.998521	23.740365
116.999571	3670.522433	23.745383
116.984079	3680.810989	23.750400
117.317046	3688.927476	23.755418
117.563503	3697.073217	23.760435
117.567175	3697.258899	23.765453
117.410179	3706.793071	23.770471
118.037784	3717.533862	23.775488
118.242536	3726.550915	23.780506
118.395701	3718.993198	23.785523
117.937871	3730.174425	23.790541
118.238323	3740.243389	23.795559
118.727810	3750.305021	23.800576
118.873337	3756.313955	23.805594
118.970841	3749.314076	23.810611
118.821024	3758.815595	23.815629
119.479726	3764.892977	23.820647
119.238580	3774.863222	23.825664
119.448677	3779.394462	23.830682
119.861106	3769.943650	23.835699
119.635285	3776.420716	23.840717
119.775862	3780.997499	23.845735
119.728670	3776.633499	23.850752
119.917799	3800.007577	23.855770
120.253409	3797.717589	23.860787
120.232288	3802.581520	23.865805
120.232973	3794.627732	23.870823
120.199263	3798.370002	23.875840
120.278821	3814.432376	23.880858
120.849308	3816.467742	23.885875
120.809730	3821.252490	23.890893
120.879200	3819.215404	23.895911
121.457974	3815.801809	23.900928
121.391054	3828.011138	23.905946
121.453022	3835.844791	23.910963
121.379783	3839.309162	23.915981
121.701250	3833.019254	23.920999
121.783641	3839.353670	23.926016
121.890975	3830.016608	23.931034
121.424638	3834.672115	23.936051
121.738960	3859.781650	23.941069
122.005383	3855.163648	23.946087
122.399463	3858.899296	23.951104
122.311529	3873.147706	23.956122
122.584753	3879.095769	23.961139
122.582457	3879.882070	23.966157
122.881849	3879.043274	23.971175
122.941351	3881.972518	23.976192
122.868337	3879.212733	23.981210
123.319126	3892.705003	23.986227
123.385317	3898.082461	23.991245
123.676265	3896.168696	23.996263
123.772611	3901.967555	24.001280
123.708796	3902.192152	24.006298
124.117833	3902.109568	24.011315
123.890690	3905.875663	24.016333
124.003341	3913.063895	24.021351
124.160331	3922.672390	24.026368
124.554278	3929.889427	24.031386
124.412163	3912.646855	24.036403
124.207697	3919.811868	24.041421
124.699803	3921.032510	24.046439
124.940821	3918.905579	24.051456
124.608433	3926.586044	24.056474
124.682428	3931.539358	24.061491
125.105543	3936.021691	24.066509
125.066673	3943.665934	24.071527
125.283910	3940.772575	24.076544
125.101265	3950.058367	24.081562
125.453563	3961.883735	24.086579
125.532525	3975.080456	24.091597
125.740617	3975.508910	24.096615
125.886420	3973.065388	24.101632
125.693508	3990.265565	24.106650
126.086400	3997.675326	24.111667
126.027386	3992.145294	24.116685
126.350215	4006.244639	24.121703
126.667978	4013.366257	24.126720
126.923127	4013.134037	24.131738
127.013200	4017.583023	24.136755
127.315357	4018.924778	24.141773
127.444459	4012.462757	24.146791
127.372634	4009.245108	24.151808
127.534504	4021.501009	24.156826
127.760165	4032.774854	24.161843
127.664979	4032.653991	24.166861
127.547119	4036.608257	24.171879
127.671854	4032.892871	24.176896
127.832422	4044.546142	24.181914
128.199569	4042.295403	24.186931
128.217172	4062.947406	24.191949
128.318311	4063.228387	24.196967
128.596562	4059.564846	24.201984
128.459584	4078.233538	24.207002
128.649245	4083.452951	24.212019
128.943122	4086.819180	24.217037
129.022839	4082.470067	24.222055
129.109094	4088.352620	24.227072
129.460180	4096.201342	24.232090
129.734205	4112.543021	24.237107
129.365225	4117.903076	24.242125
129.324000	4115.712751	24.247143
130.036883	4117.432449	24.252160
130.098167	4122.577171	24.257178
130.122655	4141.220789	24.262195
130.315875	4150.874266	24.267213
130.064414	4147.873937	24.272231
130.354803	4147.099658	24.277248
130.346322	4158.975013	24.282266
130.776943	4166.861884	24.287283
131.163490	4169.875977	24.292301
130.680845	4168.180472	24.297319
130.982665	4167.855764	24.302336
131.041094	4187.478911	24.307354
131.090252	4189.503955	24.312371
131.283036	4192.545063	24.317389
131.249122	4207.811126	24.322407
131.830509	4209.926906	24.327424
131.444275	4220.917378	24.332442
131.897623	4212.867680	24.337459
132.101285	4234.573526	24.342477
132.080841	4242.145587	24.347495
132.323587	4237.436485	24.352512
132.499900	4241.344995	24.357530
132.446384	4253.899719	24.362547
132.587823	4249.073821	24.367565
132.761897	4261.312204	24.372583
133.276755	4251.930415	24.377600
133.473933	4259.020405	24.382618
133.715856	4267.507992	24.387635
133.664924	4272.970079	24.392653
133.585101	4281.681364	24.397671
134.207792	4281.183600	24.402688
133.932264	4280.541613	24.407706
134.158220	4283.968955	24.412723
133.950838	4270.214470	24.417741
134.359841	4277.088420	24.422759
134.085478	4278.819805	24.427776
133.951924	4294.909473	24.432794
134.325426	4301.356544	24.437811
134.392904	4305.878558	24.442829
134.491990	4321.603772	24.447847
134.860559	4328.083184	24.452864
135.030202	4335.284805	24.457882
135.366753	4342.927580	24.462899
135.459427	4350.093846	24.467917
135.496611	4354.683716	24.472935
136.090191	4347.196048	24.477952
135.873023	4354.719875	24.482970
135.977617	4364.778650	24.487987
136.428934	4377.065481	24.493005
136.426174	4374.717632	24.498023
136.627492	4368.402058	24.503040
136.456095	4371.424143	24.508058
136.649889	4372.457694	24.513075
136.861719	4385.110075	24.518093
136.897347	4398.585297	24.523111
137.007917	4396.478621	24.528128
137.042348	4411.494333	24.533146
137.503616	4416.501113	24.538163
137.410480	4426.385544	24.543181
137.422875	4427.516780	24.548199
137.764759	4426.854414	24.553216
137.938318	4431.792363	24.558234
137.750958	4450.270433	24.563251
138.122483	4447.640200	24.568269
138.025435	4455.511505	24.573287
138.065802	4467.209014	24.578304
138.273083	4475.061353	24.583322
138.489661	4488.486374	24.588339
138.901384	4503.837967	24.593357
138.971811	4508.454264	24.598375
139.011877	4502.362599	24.603392
139.613334	4517.208053	24.608410
139.972249	4517.351061	24.613427
140.042763	4510.459250	24.618445
139.861948	4510.923016	24.623463
140.092485	4516.322416	24.628480
140.069546	4512.844556	24.633498
140.009002	4518.920548	24.638515
140.442534	4531.080842	24.643533
140.240183	4546.174564	24.648551
141.020063	4538.875601	24.653568
140.907339	4542.807083	24.658586
140.737449	4540.027560	24.663603
141.298873	4533.580110	24.668621
141.193192	4544.385062	24.673639
141.447711	4545.879467	24.678656
141.714919	4554.076023	24.683674
141.595018	4560.170739	24.688691
141.566131	4557.252475	24.693709
141.539171	4568.231410	24.698727
141.839225	4579.172063	24.703744
141.784723	4585.995197	24.708762
141.720050	4586.213624	24.713779
142.277008	4589.131816	24.718797
142.013995	4607.707047	24.723815
142.459085	4614.938492	24.728832
142.530207	4631.640494	24.733850
142.610197	4639.588475	24.738867
142.634253	4633.650766	24.743885
142.588109	4649.635605	24.748903
143.300938	4656.052067	24.753920
143.393299	4661.712909	24.758938
143.259311	4663.472976	24.763955
143.895927	4679.247380	24.768973
143.973618	4673.613790	24.773991
144.318737	4680.406306	24.779008
144.112119	4688.840826	24.784026
144.163351	4689.719833	24.789043
144.497566	4703.136168	24.794061
144.811587	4717.590956	24.799079
144.860709	4719.265705	24.804096
145.034421	4720.488630	24.809114
145.035564	4725.090518	24.814131
145.483107	4738.981634	24.819149
145.071969	4744.332654	24.824167
145.389340	4734.766729	24.829184
145.629644	4747.806325	24.834202
145.521431	4756.613793	24.839219
145.679395	4766.020575	24.844237
145.600697	4768.835753	24.849255
146.185817	4796.723100	24.854272
146.436956	4793.657039	24.859290
146.280137	4797.658569	24.864307
146.415216	4803.862020	24.869325
146.431263	4819.505902	24.874343
146.960035	4817.015269	24.879360
147.222840	4825.907046	24.884378
147.077556	4842.769191	24.889395
147.666649	4843.684409	24.894413
147.642996	4842.914806	24.899431
147.592581	4857.173931	24.904448
147.976089	4867.615677	24.909466
147.946451	4868.336837	24.914483
148.244376	4871.579483	24.919501
148.409560	4883.232576	24.924519
148.701138	4892.113593	24.929536
149.158591	4887.699164	24.934554
148.938652	4895.176300	24.939571
149.439146	4884.666422	24.944589
149.387478	4886.031766	24.949607
149.512598	4877.082794	24.954624
149.739378	4883.818057	24.959642
149.989669	4900.849088	24.964659
150.062268	4899.202791	24.969677
150.109537	4909.292888	24.974695
150.326538	4907.785087	24.979712
150.443117	4906.936832	24.984730
150.409779	4897.946235	24.989747
150.427346	4900.070970	24.994765
150.688538	4906.851386	24.999783
150.905982	4933.116967	25.004800
150.993582	4924.783005	25.009818
151.058644	4927.304372	25.014835
151.048311	4921.065748	25.019853
151.464294	4938.863283	25.024871
151.395668	4946.765096	25.029888
151.423963	4948.181125	25.034906
151.287864	4954.578356	25.039923
151.791514	4977.551466	25.044941
151.709580	4981.273080	25.049959
151.762428	4979.563566	25.054976
151.863314	4992.779710	25.059994
151.975268	5008.667652	25.065011
152.270751	5016.380236	25.070029
152.523251	5018.948188	25.075047
152.726085	5029.310839	25.080064
153.293381	5031.937102	25.085082
152.845836	5050.825595	25.090099
153.140908	5052.945020	25.095117
153.442350	5054.732026	25.100135
153.367896	5053.544201	25.105152
153.868206	5077.433331	25.110170
153.591147	5072.524017	25.115187
154.252649	5075.596463	25.120205
154.604754	5093.050571	25.125223
154.523306	5091.090500	25.130240
154.985683	5092.896644	25.135258
155.265878	5099.967726	25.140275
155.366920	5092.771077	25.145293
155.086502	5100.137767	25.150311
155.234751	5101.828683	25.155328
155.387762	5115.384012	25.160346
155.280763	5124.317728	25.165363
155.588979	5116.413331	25.170381
156.147131	5139.267685	25.175399
155.737573	5151.253480	25.180416
156.461417	5154.773922	25.185434
155.972570	5162.573960	25.190451
156.273919	5164.768177	25.195469
156.656143	5179.525206	25.200487
156.359707	5177.645944	25.205504
156.451410	5188.272192	25.210522
156.652505	5198.272214	25.215539
157.410219	5211.698748	25.220557
157.339227	5220.052425	25.225575
157.150529	5226.625234	25.230592
157.768552	5224.070149	25.235610
157.936937	5249.444226	25.240627
157.974827	5240.653855	25.245645
157.984441	5248.846640	25.250663
157.780533	5268.300316	25.255680
158.372653	5268.362834	25.260698
158.559501	5291.032137	25.265715
158.858899	5293.075162	25.270733
159.066685	5302.957410	25.275751
159.561579	5303.060317	25.280768
159.967232	5309.471179	25.285786
159.610145	5330.924739	25.290803
159.823268	5335.695794	25.295821
160.172241	5343.393877	25.300839
159.953451	5335.287350	25.305856
160.120098	5329.065223	25.310874
160.134140	5344.870851	25.315891
160.420648	5350.239691	25.320909
160.911926	5354.374022	25.325927
160.582074	5357.285210	25.330944
160.926210	5356.480420	25.335962
160.808605	5364.377413	25.340979
161.433888	5364.434769	25.345997
161.623042	5375.655161	25.351015
161.678357	5383.348476	25.356032
161.889422	5386.680496	25.361050
162.093310	5380.196876	25.366067
162.360385	5392.355257	25.371085
162.685592	5406.742567	25.376103
162.501574	5410.574857	25.381120
162.886573	5406.332568	25.386138
162.887103	5417.724396	25.391155
162.902184	5414.341453	25.396173
163.336506	5410.912178	25.401191
162.895125	5433.897269	25.406208
163.226057	5434.268757	25.411226
163.276665	5450.734810	25.416243
163.386085	5440.692691	25.421261
163.684315	5456.848737	25.426279
163.568253	5463.580775	25.431296
164.211752	5465.939561	25.436314
164.286790	5490.441524	25.441331
164.254852	5488.483170	25.446349
164.171729	5496.283313	25.451367
164.706129	5505.950682	25.456384
165.100413	5512.022480	25.461402
164.818457	5516.447686	25.466419
165.244384	5524.897747	25.471437
165.537564	5535.972624	25.476455
165.909501	5547.814913	25.481472
165.757448	5544.820969	25.486490
165.730469	5546.633904	25.491507
166.071203	5564.415360	25.496525
166.123882	5570.966496	25.501543
166.463634	5569.752029	25.506560
166.692356	5591.679712	25.511578
166.364919	5592.523022	25.516595
167.027283	5597.167386	25.521613
167.256145	5609.407619	25.526631
167.138887	5616.815403	25.531648
167.395530	5618.195932	25.536666
167.376868	5626.690006	25.541683
167.601809	5633.722551	25.546701
167.767275	5630.518174	25.551719
168.000007	5654.055152	25.556736
168.053076	5667.740089	25.561754
167.726275	5673.081405	25.566771
168.531530	5682.634098	25.571789
169.183581	5687.172768	25.576807
169.135334	5697.085623	25.581824
169.296662	5706.220904	25.586842
169.277330	5714.557295	25.591859
169.511061	5722.412370	25.596877
169.813449	5711.235259	25.601895
169.830638	5738.716895	25.606912
169.969469	5731.034312	25.611930
170.153732	5740.503793	25.616947
170.256700	5758.559200	25.621965
170.493256	5759.267360	25.626983
170.569544	5765.019432	25.632000
170.911569	5768.899317	25.637018
170.921909	5783.771555	25.642035
170.799448	5797.944779	25.647053
171.188372	5798.291464	25.652071
171.407338	5820.707057	25.657088
171.537290	5818.164747	25.662106
171.901681	5833.572185	25.667123
171.759345	5836.160691	25.672141
172.127909	5837.659546	25.677159
172.668234	5865.896424	25.682176
172.692725	5875.993760	25.687194
172.288632	5873.127387	25.692212
172.448220	5888.102737	25.697229
173.172172	5891.964223	25.702247
173.008794	5909.897103	25.707264
173.289514	5905.276359	25.712282
173.390095	5922.334813	25.717300
173.494741	5928.698061	25.722317
173.925096	5938.811158	25.727335
174.146710	5953.158209	25.732352
174.588268	5951.135558	25.737370
174.505179	5953.298183	25.742388
174.822373	5973.059743	25.747405
175.094038	5968.159454	25.752423
175.220956	5971.046973	25.757440
175.220184	5968.357694	25.762458
175.487738	5973.606562	25.767476
175.138994	5977.246810	25.772493
175.891473	5982.256039	25.777511
175.772316	5999.014174	25.782528
175.907583	5998.680646	25.787546
176.360047	6005.015021	25.792564
176.266358	6021.958610	25.797581
176.645738	6015.961973	25.802599
176.685267	6023.579101	25.807616
177.137079	6032.505176	25.812634
177.279960	6033.417329	25.817652
177.280962	6042.366246	25.822669
177.802793	6033.395979	25.827687
177.866228	6043.468405	25.832704
178.410958	6059.504536	25.837722
178.421621	6064.960728	25.842740
178.056811	6060.509893	25.847757
178.076749	6063.032130	25.852775
178.561248	6064.557147	25.857792
178.841455	6075.312397	25.862810
179.158165	6075.948115	25.867828
178.489978	6085.948228	25.872845
179.139309	6095.140307	25.877863
179.645631	6108.641369	25.882880
179.760141	6105.549012	25.887898
180.047625	6109.238594	25.892916
180.290780	6121.802081	25.897933
180.249717	6128.677363	25.902951
180.524981	6138.199172	25.907968
180.769165	6136.084121	25.912986
180.465488	6139.625842	25.918004
180.291622	6149.217581	25.923021
180.705732	6155.917839	25.928039
180.710400	6168.016580	25.933056
181.387367	6189.117601	25.938074
181.589088	6207.546346	25.943092
181.617123	6203.712995	25.948109
182.009433	6212.733652	25.953127
182.135358	6215.479315	25.958144
182.176317	6229.864181	25.963162
182.407974	6231.845257	25.968180
182.807953	6247.777825	25.973197
183.056048	6256.884090	25.978215
182.710111	6259.374931	25.983232
182.953002	6269.264865	25.988250
183.569011	6277.534164	25.993268
183.521523	6293.410171	25.998285
183.491661	6300.129096	26.003303
183.950517	6312.753833	26.008320
183.535688	6308.209710	26.013338
183.858518	6324.643641	26.018356
184.146316	6337.130879	26.023373
184.468787	6349.151851	26.028391
184.530661	6365.130848	26.033408
184.530934	6380.245046	26.038426
185.189565	6397.188651	26.043444
185.325880	6407.609794	26.048461
185.575425	6415.746809	26.053479
185.856036	6425.927685	26.058496
185.796729	6429.289364	26.063514
185.943891	6429.351720	26.068532
186.254040	6450.835293	26.073549
186.332047	6448.241007	26.078567
186.428683	6469.353786	26.083584
186.549921	6475.275859	26.088602
187.081742	6483.596240	26.093620
186.707280	6495.419614	26.098637
186.977392	6501.148056	26.103655
187.229806	6516.387260	26.108672
187.748136	6533.510671	26.113690
188.071100	6534.505297	26.118708
188.244818	6545.634113	26.123725
188.560649	6552.551847	26.128743
188.598412	6564.775124	26.133760
188.706171	6566.854444	26.138778
189.147466	6580.400705	26.143796
189.521468	6584.784020	26.148813
189.716904	6582.641783	26.153831
189.478226	6586.003007	26.158848
189.271392	6588.355435	26.163866
189.349919	6602.908365	26.168884
189.824961	6622.977510	26.173901
189.856330	6625.100297	26.178919
190.005193	6638.881534	26.183936
190.562534	6650.730399	26.188954
191.191947	6646.576043	26.193972
190.995165	6658.128790	26.198989
191.220710	6669.786257	26.204007
191.367580	6677.289087	26.209024
191.501073	6682.237045	26.214042
191.869880	6688.461571	26.219060
191.946111	6702.260477	26.224077
192.181898	6706.059245	26.229095
192.503169	6718.367912	26.234112
192.504455	6728.033701	26.239130
193.114459	6724.204337	26.244148
192.858376	6737.553085	26.249165
193.308122	6734.430527	26.254183
193.758102	6739.613334	26.259200
193.900565	6734.969713	26.264218
194.144173	6747.303118	26.269236
194.188903	6764.421561	26.274253
194.910857	6767.737431	26.279271
194.501578	6777.287231	26.284288
194.571599	6773.772370	26.289306
194.837377	6787.548143	26.294324
194.823404	6802.061968	26.299341
194.735181	6797.574203	26.304359
194.688190	6817.797442	26.309376
194.842033	6831.252902	26.314394
195.760254	6845.287012	26.319412
195.585510	6861.527410	26.324429
195.918562	6862.479447	26.329447
196.347603	6881.100767	26.334464
196.624204	6892.488415	26.339482
196.643229	6903.900388	26.344500
196.966405	6909.418663	26.349517
197.208326	6903.743033	26.354535
197.330652	6921.408292	26.359552
197.268753	6929.088940	26.364570
197.811715	6929.307495	26.369588
198.003906	6943.940860	26.374605
197.985351	6968.045837	26.379623
198.057728	6959.820648	26.384640
198.223217	6977.586572	26.389658
198.620885	6978.528555	26.394676
198.396289	6983.440798	26.399693
198.628332	7009.505063	26.404711
198.730284	7013.154265	26.409728
198.834442	7033.998196	26.414746
199.571039	7035.875493	26.419764
199.411600	7058.080033	26.424781
199.899920	7069.188598	26.429799
200.112723	7071.696731	26.434816
200.170836	7092.857265	26.439834
200.296038	7094.289941	26.444852
200.454920	7091.900792	26.449869
200.329198	7107.426651	26.454887
201.143678	7121.698103	26.459904
200.846292	7138.693377	26.464922
201.576647	7132.960574	26.469940
201.931662	7156.540430	26.474957
201.975290	7166.026233	26.479975
202.233185	7171.627358	26.484992
202.068462	7187.282472	26.490010
202.399445	7198.172536	26.495028
202.906828	7210.960808	26.500045
203.042327	7218.333044	26.505063
203.111767	7230.747556	26.510080
203.141279	7236.160123	26.515098
203.471162	7243.050678	26.520116
203.521785	7261.223050	26.525133
203.704786	7275.207801	26.530151
204.536716	7277.714278	26.535168
204.243702	7286.381266	26.540186
204.695961	7303.316805	26.545204
204.543849	7320.059179	26.550221
204.942695	7319.100576	26.555239
205.159127	7327.625132	26.560256
204.909595	7342.387566	26.565274
205.622071	7357.470610	26.570292
205.931403	7366.962502	26.575309
205.864561	7385.165912	26.580327
206.343136	7396.115193	26.585344
206.434761	7409.943803	26.590362
206.571619	7409.682611	26.595380
207.242726	7398.620697	26.600397
207.243468	7409.376047	26.605415
207.642785	7415.615014	26.610432
208.067551	7426.152828	26.615450
208.362548	7424.957838	26.620468
208.682726	7421.110318	26.625485
208.383649	7422.637488	26.630503
208.978354	7426.402625	26.635520
209.001420	7439.361166	26.640538
209.304245	7430.215965	26.645556
209.346317	7443.244158	26.650573
209.582065	7445.025848	26.655591
209.409972	7456.581566	26.660608
209.300116	7473.096521	26.665626
209.509875	7474.225630	26.670644
209.286020	7495.815666	26.675661
209.907104	7509.511411	26.680679
210.073135	7527.498764	26.685696
210.551976	7553.342279	26.690714
210.751146	7557.254260	26.695732
211.028612	7560.964639	26.700749
211.225723	7576.696340	26.705767
211.870082	7583.007706	26.710784
211.758499	7582.649445	26.715802
212.232487	7599.379833	26.720820
212.372668	7616.654683	26.725837
212.189141	7613.207549	26.730855
212.789087	7632.614348	26.735872
212.882768	7636.347042	26.740890
212.949293	7627.642617	26.745908
213.126511	7649.362961	26.750925
213.414228	7657.822905	26.755943
213.429100	7668.131082	26.760960
213.720407	7688.239472	26.765978
213.671495	7689.191040	26.770996
214.146398	7700.892421	26.776013
214.271052	7713.282879	26.781031
214.673140	7716.576116	26.786048
214.534497	7735.034134	26.791066
214.813538	7740.954147	26.796084
215.002903	7752.504287	26.801101
214.872917	7775.898423	26.806119
215.396228	7783.854521	26.811136
215.583032	7803.095367	26.816154
215.909420	7807.177012	26.821172
216.413867	7814.785641	26.826189
216.203725	7833.324340	26.831207
216.369396	7856.107457	26.836224
216.563646	7857.889334	26.841242
217.214578	7874.197809	26.846260
217.383575	7887.121317	26.851277
217.117727	7904.961606	26.856295
217.488724	7909.045799	26.861312
217.908195	7934.712833	26.866330
217.764091	7943.334847	26.871348
218.154836	7954.781151	26.876365
218.179192	7961.526970	26.881383
218.888804	7982.435563	26.886400
219.021250	7998.076669	26.891418
219.477011	8007.438759	26.896436
219.785167	8019.327309	26.901453
219.825888	8042.338469	26.906471
220.488158	8046.689886	26.911488
220.265303	8059.835528	26.916506
220.420306	8067.378701	26.921524
220.808665	8065.635607	26.926541
220.747129	8083.703132	26.931559
221.043132	8090.804484	26.936576
221.469448	8103.224007	26.941594
221.745019	8116.746696	26.946612
221.943043	8113.988269	26.951629
221.865639	8135.335264	26.956647
222.380069	8136.489592	26.961664
222.749898	8150.846861	26.966682
223.080301	8170.886552	26.971700
223.535500	8168.555313	26.976717
223.348463	8175.526698	26.981735
223.688061	8179.104407	26.986752
223.967228	8196.140330	26.991770
224.061279	8202.139805	26.996788
224.177781	8205.171365	27.001805
223.980932	8219.572714	27.006823
224.461056	8238.001197	27.011840
224.847971	8251.999143	27.016858
224.856467	8251.098110	27.021876
225.152360	8268.917591	27.026893
224.951729	8289.810397	27.031911
225.198973	8296.881537	27.036928
225.741926	8314.179574	27.041946
226.034324	8327.652443	27.046964
226.367115	8334.154643	27.051981
226.341118	8355.598071	27.056999
226.680779	8360.984781	27.062016
226.745862	8371.433914	27.067034
227.239170	8387.685303	27.072052
227.634298	8397.467446	27.077069
227.436069	8410.126477	27.082087
228.075891	8415.993697	27.087104
228.199465	8424.359582	27.092122
228.163402	8435.765296	27.097140
228.596136	8453.781487	27.102157
228.797103	8467.189766	27.107175
229.153878	8469.167394	27.112192
229.093151	8484.756905	27.117210
229.024676	8502.147154	27.122228
229.329613	8508.309633	27.127245
229.666834	8520.727524	27.132263
229.993775	8537.446934	27.137280
230.218673	8557.983344	27.142298
230.546682	8564.009654	27.147316
230.727413	8573.815799	27.152333
230.643128	8587.950502	27.157351
231.240172	8609.429821	27.162368
231.178053	8609.398487	27.167386
231.388288	8632.305064	27.172404
231.952896	8643.345881	27.177421
231.859337	8660.834896	27.182439
232.417721	8673.843559	27.187456
232.240726	8683.396062	27.192474
232.552183	8694.501579	27.197492
233.228741	8702.677314	27.202509
233.457008	8714.130445	27.207527
233.356281	8735.683817	27.212544
233.952068	8745.785342	27.217562
233.905908	8758.342008	27.222580
234.188895	8772.688026	27.227597
234.060515	8799.050877	27.232615
234.344590	8804.376916	27.237632
234.948069	8808.087306	27.242650
235.034630	8822.659684	27.247668
235.617350	8846.711392	27.252685
235.759195	8858.342237	27.257703
235.776394	8870.633389	27.262720
236.719908	8880.055744	27.267738
236.880101	8886.231414	27.272756
237.371291	8902.493058	27.277773
237.176701	8918.125875	27.282791
237.179693	8913.471850	27.287808
237.671197	8919.905349	27.292826
237.649182	8938.516894	27.297844
237.900351	8954.673882	27.302861
238.331660	8966.600699	27.307879
238.070801	8967.556915	27.312896
238.277283	8969.100213	27.317914
238.177461	9004.030519	27.322932
238.945258	9016.564822	27.327949
238.985704	9043.773108	27.332967
239.447001	9055.212271	27.337984
239.932834	9070.218353	27.343002
240.375886	9082.632775	27.348020
240.303490	9086.675762	27.353037
240.637586	9106.239165	27.358055
240.784906	9109.922764	27.363072
241.171874	9123.457263	27.368090
241.234695	9126.670975	27.373108
241.420755	9148.094934	27.378125
241.506441	9162.711916	27.383143
241.758984	9186.831258	27.388160
242.563820	9180.735791	27.393178
242.458512	9188.332579	27.398196
243.236164	9202.589289	27.403213
243.162314	9202.048319	27.408231
243.236884	9214.933786	27.413248
243.970739	9214.295481	27.418266
243.792167	9232.113988	27.423284
244.065257	9248.312020	27.428301
244.552453	9259.333687	27.433319
244.682796	9257.820086	27.438336
244.812606	9269.781410	27.443354
245.064460	9283.520178	27.448372
245.280496	9283.514995	27.453389
245.566306	9297.387403	27.458407
245.727335	9300.835274	27.463424
246.061660	9301.345240	27.468442
245.926864	9328.969561	27.473460
246.113336	9341.019983	27.478477
246.373488	9346.081541	27.483495
246.447580	9372.978824	27.488512
246.914798	9381.386358	27.493530
247.052813	9398.982090	27.498548
247.205776	9409.364455	27.503565
247.705449	9431.396616	27.508583
247.873546	9442.966911	27.513600
248.250982	9446.706310	27.518618
248.391153	9472.832563	27.523636
248.328619	9476.188983	27.528653
248.948947	9493.154045	27.533671
249.514904	9494.540391	27.538688
249.939733	9492.090588	27.543706
250.147999	9521.331954	27.548724
250.181898	9517.774837	27.553741
250.525683	9532.332984	27.558759
250.993021	9543.730466	27.563776
251.504831	9541.080838	27.568794
251.289408	9560.689230	27.573812
251.529339	9570.044675	27.578829
251.885249	9574.052659	27.583847
251.691901	9589.954212	27.588864
252.098243	9603.517619	27.593882
252.255060	9612.832352	27.598900
252.657007	9625.345098	27.603917
252.526910	9635.645369	27.608935
252.849733	9654.475469	27.613952
253.499084	9667.991618	27.618970
253.099059	9677.614084	27.623988
253.302652	9702.085858	27.629005
254.108215	9713.465517	27.634023
254.291274	9741.132526	27.639040
254.226653	9746.090051	27.644058
254.452405	9772.683305	27.649076
255.071014	9789.061655	27.654093
255.401843	9801.089901	27.659111
255.403806	9829.520880	27.664128
256.038458	9834.789479	27.669146
255.634671	9850.856623	27.674164
255.915139	9869.879815	27.679181
256.308475	9881.440575	27.684199
256.716197	9907.026933	27.689216
256.754471	9920.827841	27.694234
257.277733	9943.027431	27.699252
257.322674	9956.975720	27.704269
257.761850	9978.294928	27.709287
258.323002	9987.632147	27.714304
258.360547	10001.606880	27.719322
258.531022	10026.204214	27.724340
258.770408	10035.383170	27.729357
259.247054	10044.897754	27.734375
259.299781	10062.747349	27.739392
259.867855	10076.225934	27.744410
259.921890	10089.108890	27.749428
260.164123	10108.646608	27.754445
260.828718	10122.968991	27.759463
260.724512	10146.961997	27.764480
261.100944	10141.204450	27.769498
261.353177	10165.997624	27.774516
261.748924	10173.399984	27.779533
262.323644	10184.515927	27.784551
262.140795	10182.394285	27.789568
262.889263	10198.686477	27.794586
262.823664	10214.369761	27.799604
263.178969	10214.709149	27.804621
263.031527	10215.603567	27.809639
263.109960	10227.197783	27.814656
263.899387	10237.977226	27.819674
263.769490	10260.705126	27.824692
263.731118	10274.148818	27.829709
264.328938	10270.320637	27.834727
264.866152	10295.044356	27.839744
265.234353	10286.506417	27.844762
265.687034	10307.388186	27.849780
265.940228	10318.929992	27.854797
266.110857	10322.259737	27.859815
265.928379	10336.082691	27.864832
266.384472	10335.591792	27.869850
266.794057	10357.926398	27.874868
266.525801	10376.381963	27.879885
267.164425	10385.337910	27.884903
267.029791	10412.613345	27.889920
267.515565	10416.752850	27.894938
268.277259	10427.179938	27.899956
268.608638	10442.220653	27.904973
268.491306	10438.525878	27.909991
268.941523	10454.722646	27.915008
269.570573	10466.578600	27.920026
269.371090	10472.030922	27.925044
269.447213	10495.314307	27.930061
269.788252	10501.525509	27.935079
269.799111	10525.649485	27.940096
269.854682	10533.755374	27.945114
270.283354	10554.953741	27.950132
270.327296	10578.826358	27.955149
270.474851	10603.488014	27.960167
270.718953	10635.794552	27.965184
270.870328	10651.103422	27.970202
271.253569	10669.861996	27.975220
271.675355	10688.361995	27.980237
272.312575	10706.367488	27.985255
272.335488	10729.924672	27.990272
273.145374	10748.016991	27.995290
273.657225	10765.306378	28.000308
273.911431	10783.835719	28.005325
274.405800	10779.167876	28.010343
274.747639	10792.356987	28.015360
274.889070	10794.816752	28.020378
275.096580	10811.291583	28.025396
275.391530	10823.667081	28.030413
275.839054	10832.656154	28.035431
275.884444	10842.936085	28.040448
275.752791	10855.674821	28.045466
276.176766	10870.032086	28.050484
276.372460	10882.745136	28.055501
276.716073	10892.609244	28.060519
276.501261	10905.806161	28.065536
276.892383	10923.591267	28.070554
277.327793	10935.414519	28.075572
277.319910	10954.862607	28.080589
277.664850	10980.908576	28.085607
277.754043	11001.386723	28.090624
278.452707	11026.455703	28.095642
278.779455	11043.944671	28.100660
278.766637	11065.559675	28.105677
279.163429	11077.152217	28.110695
279.188476	11105.433144	28.115712
279.796066	11118.972641	28.120730
280.039692	11134.494886	28.125748
280.361315	11157.103060	28.130765
280.649714	11167.831591	28.135783
280.417261	11188.265293	28.140800
280.900803	11193.298894	28.145818
281.326389	11213.232330	28.150836
281.329467	11234.087251	28.155853
282.085877	11243.423124	28.160871
282.107534	11268.638877	28.165888
282.464699	11289.729226	28.170906
282.568551	11305.721742	28.175924
282.748216	11323.969573	28.180941
282.769226	11334.215680	28.185959
283.662722	11354.467953	28.190976
283.847114	11373.750768	28.195994
284.532533	11385.118588	28.201012
284.386437	11411.538413	28.206029
284.913597	11432.517204	28.211047
284.840682	11447.836385	28.216064
285.029092	11463.152785	28.221082
286.105025	11469.126755	28.226100
286.050461	11492.261218	28.231117
286.524360	11503.769398	28.236135
286.734406	11526.111209	28.241152
287.139637	11536.698618	28.246170
287.766375	11550.090201	28.251188
287.517957	11570.119477	28.256205
287.727365	11580.257448	28.261223
288.331019	11598.941593	28.266240
288.160808	11618.368278	28.271258
288.757801	11630.473100	28.276276
288.960084	11659.358785	28.281293
289.309716	11668.786619	28.286311
289.622631	11670.319891	28.291328
289.871642	11680.019161	28.296346
290.352752	11708.586802	28.301364
290.861319	11728.687852	28.306381
291.421300	11730.934172	28.311399
292.067629	11739.204377	28.316416
292.411364	11736.466941	28.321434
292.725128	11736.525488	28.326452
292.943286	11736.024236	28.331469
293.322676	11748.665071	28.336487
293.740276	11760.652657	28.341504
293.892249	11749.122735	28.346522
294.243343	11747.296698	28.351540
293.990101	11749.132836	28.356557
294.299075	11753.641187	28.361575
294.708887	11776.286902	28.366592
294.395680	11780.333228	28.371610
294.989702	11796.278269	28.376628
295.147094	11800.879699	28.381645
295.515288	11822.221541	28.386663
295.559302	11830.768699	28.391680
296.123587	11848.619298	28.396698
296.210576	11860.042684	28.401716
296.269205	11881.309640	28.406733
296.592134	11886.810503	28.411751
296.812835	11904.774641	28.416768
296.972906	11927.993059	28.421786
297.529142	11947.183840	28.426804
297.382288	11974.671855	28.431821
298.194631	11988.707434	28.436839
298.435675	12008.585193	28.441856
298.568479	12031.545899	28.446874
298.867704	12037.587296	28.451892
299.367446	12069.818619	28.456909
299.726865	12085.825693	28.461927
299.627086	12089.368366	28.466944
300.172345	12114.686884	28.471962
300.352759	12121.413073	28.476980
300.229092	12143.406550	28.481997
300.508356	12162.618568	28.487015
301.110748	12181.126663	28.492032
301.232672	12202.523066	28.497050
301.751189	12207.491503	28.502068
301.830223	12225.196970	28.507085
302.550188	12246.370852	28.512103
302.740515	12260.885554	28.517120
302.905168	12282.228031	28.522138
302.880412	12300.533900	28.527156
303.496985	12337.143001	28.532173
303.894116	12347.305842	28.537191
304.035500	12370.666655	28.542208
304.134853	12390.759496	28.547226
305.005439	12397.959353	28.552244
304.877331	12438.675932	28.557261
305.442252	12441.398387	28.562279
306.021113	12459.695695	28.567296
306.165484	12488.645353	28.572314
306.599713	12491.192383	28.577332
306.554539	12518.441163	28.582349
306.964601	12532.722928	28.587367
307.532018	12553.583030	28.592384
307.784040	12580.425649	28.597402
308.546791	12586.281382	28.602420
308.362480	12607.757499	28.607437
308.702347	12620.307185	28.612455
309.114911	12647.147010	28.617472
309.058745	12667.908540	28.622490
309.559840	12676.514390	28.627508
309.932151	12702.735325	28.632525
310.141306	12710.647726	28.637543
310.488604	12729.319228	28.642560
310.887364	12754.235118	28.647578
311.219862	12772.327938	28.652596
311.443128	12792.262974	28.657613
311.671040	12806.330157	28.662631
312.046469	12828.038318	28.667648
312.188373	12851.870155	28.672666
312.718199	12871.741760	28.677684
312.991742	12895.158435	28.682701
313.088988	12923.756109	28.687719
313.771694	12938.406251	28.692736
313.753092	12954.678173	28.697754
314.097141	12974.724069	28.702772
313.998928	13005.941698	28.707789
314.371210	13024.748547	28.712807
315.670664	13045.738381	28.717824
315.546822	13068.705570	28.722842
315.869951	13079.865570	28.727860
316.021592	13106.705619	28.732877
316.141410	13119.062532	28.737895
316.977232	13133.180578	28.742912
317.441518	13161.288846	28.747930
317.708443	13178.047026	28.752948
317.926810	13199.233760	28.757965
318.011011	13198.914377	28.762983
318.539323	13224.628601	28.768000
318.519044	13253.671381	28.773018
319.132255	13265.856841	28.778036
319.409160	13287.918760	28.783053
319.865063	13297.485605	28.788071
320.046127	13319.003540	28.793088
320.467154	13337.743114	28.798106
321.014211	13360.874629	28.803124
321.022351	13368.828075	28.808141
321.225608	13391.558418	28.813159
321.554405	13404.460875	28.818176
321.578139	13419.542402	28.823194
322.237132	13432.447156	28.828212
322.828505	13451.299269	28.833229
322.978648	13454.389606	28.838247
323.323866	13476.627425	28.843264
323.490594	13503.061478	28.848282
324.073865	13513.508604	28.853300
324.077080	13530.671310	28.858317
324.226215	13549.908160	28.863335
324.704156	13567.439099	28.868352
324.924664	13587.785933	28.873370
325.106613	13612.468288	28.878388
325.718428	13627.486848	28.883405
325.747565	13653.816215	28.888423
326.429378	13671.842884	28.893440
326.511047	13702.711549	28.898458
326.638457	13719.592983	28.903476
326.953505	13728.755655	28.908493
327.382506	13756.197663	28.913511
327.961257	13771.426751	28.918528
328.030703	13801.482732	28.923546
328.358209	13816.776235	28.928564
329.013305	13847.584285	28.933581
329.491177	13871.914587	28.938599
329.636688	13886.848051	28.943616
329.504950	13918.097666	28.948634
330.063997	13926.294007	28.953652
330.627081	13958.531330	28.958669
330.744657	13986.521115	28.963687
330.718293	14004.614141	28.968704
331.560568	14037.853424	28.973722
332.038892	14045.879221	28.978740
332.724656	14069.539499	28.983757
332.807763	14100.320163	28.988775
333.254890	14110.163533	28.993792
333.565297	14134.198128	28.998810
333.697318	14143.793720	29.003828
334.288342	14167.269916	29.008845
334.520396	14186.810304	29.013863
334.661393	14212.709333	29.018880
335.170789	14234.177192	29.023898
335.537554	14242.908889	29.028916
335.892182	14269.280019	29.033933
335.874047	14289.753184	29.038951
336.071297	14306.118983	29.043968
336.631881	14326.265238	29.048986
337.230950	14337.310387	29.054004
337.689981	14364.255948	29.059021
337.715624	14389.655259	29.064039
338.108785	14403.836858	29.069056
338.901862	14439.200395	29.074074
339.043960	14446.419718	29.079092
339.510319	14467.708217	29.084109
339.807965	14485.173334	29.089127
340.479243	14487.551097	29.094144
340.695916	14509.825933	29.099162
340.818043	14523.162402	29.104180
341.273558	14538.104962	29.109197
341.282582	14551.358001	29.114215
342.118158	14562.979127	29.119232
342.062893	14591.344100	29.124250
342.482882	14593.634675	29.129268
342.690501	14610.687583	29.134285
342.757883	14642.100030	29.139303
342.713818	14659.839572	29.144320
343.616128	14675.666424	29.149338
343.735774	14699.535632	29.154356
344.415033	14712.526534	29.159373
344.423545	14735.582510	29.164391
344.794607	14749.458315	29.169408
345.130917	14772.892805	29.174426
345.538339	14794.765621	29.179444
346.367067	14806.849049	29.184461
346.185879	14830.146265	29.189479
346.681026	14847.846249	29.194496
346.828724	14866.569885	29.199514
346.974901	14889.405653	29.204532
347.508273	14903.881610	29.209549
347.680089	14931.962245	29.214567
348.180547	14954.465020	29.219584
348.384693	14994.317401	29.224602
348.857626	15005.932095	29.229620
349.035578	15033.519254	29.234637
349.030960	15053.290025	29.239655
349.637528	15075.962756	29.244672
349.831347	15099.220867	29.249690
350.494148	15124.190356	29.254708
350.887609	15144.890912	29.259725
351.661067	15176.355383	29.264743
352.048189	15194.322003	29.269760
352.333271	15217.259707	29.274778
352.862147	15233.050418	29.279796
353.040392	15248.497798	29.284813
353.336518	15278.037619	29.289831
353.844786	15292.015629	29.294848
353.945601	15316.949693	29.299866
354.555600	15335.576552	29.304884
355.006421	15356.761087	29.309901
355.032487	15383.892352	29.314919
355.529208	15396.564739	29.319936
355.964131	15416.791721	29.324954
356.058988	15450.219319	29.329972
356.680326	15458.599280	29.334989
356.840509	15480.846147	29.340007
357.579754	15503.921934	29.345024
357.530555	15514.793929	29.350042
357.778565	15533.957388	29.355060
358.567981	15549.834130	29.360077
358.873293	15579.221392	29.365095
358.977920	15587.972411	29.370112
359.729619	15609.280931	29.375130
359.906343	15635.277395	29.380148
360.258882	15648.364020	29.385165
360.810713	15677.169835	29.390183
360.812404	15690.102664	29.395200
361.060962	15716.744974	29.400218
361.691203	15744.821759	29.405236
362.169636	15762.417815	29.410253
362.459622	15786.710337	29.415271
362.860316	15801.987728	29.420288
362.798600	15818.622539	29.425306
363.153020	15846.372896	29.430324
363.606104	15867.355516	29.435341
363.631670	15904.054045	29.440359
364.412948	15925.121441	29.445376
364.982930	15950.839189	29.450394
365.106755	15986.290842	29.455412
365.960323	15996.400380	29.460429
366.138742	16011.096673	29.465447
366.104421	16036.959148	29.470464
366.614326	16062.935907	29.475482
366.538743	16088.031087	29.480500
367.074194	16105.312226	29.485517
367.533341	16135.172250	29.490535
367.776049	16156.187939	29.495552
368.365231	16175.428418	29.500570
368.576256	16195.147847	29.505588
368.967595	16216.314172	29.510605
369.352479	16229.408793	29.515623
369.467352	16265.216090	29.520640
370.190040	16284.034783	29.525658
370.458210	16314.085893	29.530676
371.254926	16339.238261	29.535693
371.129135	16360.254692	29.540711
371.054396	16378.092194	29.545728
371.531157	16416.853361	29.550746
372.132120	16436.537600	29.555764
372.392394	16455.835883	29.560781
372.799950	16492.548711	29.565799
373.047432	16514.094658	29.570816
373.831093	16545.465046	29.575834
374.064013	16568.728332	29.580852
374.664362	16592.654560	29.585869
374.753441	16618.602835	29.590887
375.292816	16646.710882	29.595904
375.729517	16672.469299	29.600922
376.013933	16695.099354	29.605940
376.214750	16718.336235	29.610957
376.947873	16748.884158	29.615975
377.526896	16761.092984	29.620992
377.707396	16780.429280	29.626010
378.108067	16812.734617	29.631028
378.638824	16831.760602	29.636045
378.831721	16854.998881	29.641063
378.986776	16885.400132	29.646080
379.420394	16910.060207	29.651098
380.010304	16936.913221	29.656116
380.295870	16961.965951	29.661133
380.307173	16996.363107	29.666151
380.536210	17020.344517	29.671168
381.417387	17056.744645	29.676186
381.563042	17086.035891	29.681204
382.388127	17109.577184	29.686221
382.528421	17151.519120	29.691239
382.596878	17168.826544	29.696256
383.394040	17193.831515	29.701274
383.453995	17218.294318	29.706292
383.974994	17253.654890	29.711309
384.873583	17276.464805	29.716327
385.063640	17303.254240	29.721344
385.506181	17328.943141	29.726362
385.852801	17359.103695	29.731380
386.782265	17370.718244	29.736397
386.602810	17386.621010	29.741415
387.099521	17418.754485	29.746432
387.596489	17440.954351	29.751450
387.885184	17462.558116	29.756468
388.259119	17489.063340	29.761485
388.906940	17521.568282	29.766503
389.324428	17534.851390	29.771520
389.764422	17551.520141	29.776538
389.647312	17591.983839	29.781556
390.159669	17606.762024	29.786573
390.648047	17625.814345	29.791591
390.489443	17653.116539	29.796608
391.234972	17683.164961	29.801626
392.022027	17707.900536	29.806644
392.172038	17732.779540	29.811661
392.580987	17749.450137	29.816679
392.801577	17772.795761	29.821696
393.267832	17793.494164	29.826714
393.539999	17818.404798	29.831732
393.982891	17829.296249	29.836749
394.584150	17853.031230	29.841767
394.658631	17876.500802	29.846784
395.175542	17885.624573	29.851802
395.127620	17919.195559	29.856820
395.828419	17945.157779	29.861837
396.078174	17968.000036	29.866855
396.318769	17997.173649	29.871872
396.919557	18018.224068	29.876890
397.056144	18048.759531	29.881908
397.842600	18067.033078	29.886925
398.059281	18088.358159	29.891943
398.387081	18130.936346	29.896960
398.744461	18159.757206	29.901978
399.341004	18177.106508	29.906996
399.638599	18202.790710	29.912013
400.311792	18231.101344	29.917031
400.634094	18257.059735	29.922048
401.292473	18277.956172	29.927066
401.597581	18315.389649	29.932084
401.927421	18338.055624	29.937101
402.359001	18358.974822	29.942119
402.318634	18394.567019	29.947136
402.662418	18414.615510	29.952154
403.123869	18446.042317	29.957172
403.723450	18475.975711	29.962189
404.209638	18509.117110	29.967207
404.441971	18532.562902	29.972224
405.082607	18558.990170	29.977242
405.391818	18595.299042	29.982260
405.718903	18617.062374	29.987277
406.455097	18652.837389	29.992295
406.837648	18675.893554	29.997312
407.747647	18698.374869	30.002330
407.716637	18713.965007	30.007348
407.844272	18746.360308	30.012365
408.518123	18769.131169	30.017383
409.036534	18805.742695	30.022400
409.428001	18826.182193	30.027418
409.666644	18850.941436	30.032436
409.786468	18873.046882	30.037453
410.494737	18893.816185	30.042471
410.837439	18925.698169	30.047488
411.645710	18954.854341	30.052506
411.656229	18985.688878	30.057524
412.119364	19006.938696	30.062541
413.014798	19023.692596	30.067559
412.811191	19066.222896	30.072576
413.758284	19085.464266	30.077594
414.107778	19105.487312	30.082612
414.317042	19130.548414	30.087629
414.841778	19156.255376	30.092647
414.847507	19186.819319	30.097664
415.661671	19208.937088	30.102682
415.689189	19234.260370	30.107700
416.181778	19270.725169	30.112717
416.574629	19296.351766	30.117735
416.862093	19332.930745	30.122752
417.788636	19349.623225	30.127770
417.930316	19388.853172	30.132788
418.351989	19412.099971	30.137805
419.166611	19439.328975	30.142823
419.572712	19468.024156	30.147840
419.880015	19494.277153	30.152858
420.239306	19525.784790	30.157876
420.406313	19545.849335	30.162893
420.861283	19565.054076	30.167911
421.073811	19595.169491	30.172928
421.556007	19611.969281	30.177946
421.379290	19650.819713	30.182964
421.769762	19687.010570	30.187981
422.356481	19708.090287	30.192999
422.599894	19748.404421	30.198016
423.531218	19773.796188	30.203034
423.434511	19814.542479	30.208052
424.148790	19848.882636	30.213069
424.648587	19872.692749	30.218087
424.656462	19898.538017	30.223104
425.183405	19929.312603	30.228122
425.610791	19968.796178	30.233140
426.078427	20000.818420	30.238157
426.642728	20039.775390	30.243175
427.258210	20080.253413	30.248192
427.458802	20107.054554	30.253210
427.869504	20138.795260	30.258228
428.795326	20178.454381	30.263245
429.199444	20210.088822	30.268263
429.485475	20246.789779	30.273280
429.960671	20279.563143	30.278298
430.055659	20300.176704	30.283316
430.929465	20338.511147	30.288333
431.424674	20360.180757	30.293351
431.830139	20400.483644	30.298368
432.283417	20417.345492	30.303386
432.988698	20445.332139	30.308404
433.449777	20476.155749	30.313421
433.967323	20513.351881	30.318439
434.104752	20527.697854	30.323456
434.521903	20555.350428	30.328474
435.044217	20584.730468	30.333492
435.059706	20615.484668	30.338509
436.151759	20645.117280	30.343527
436.656120	20671.644452	30.348544
437.077652	20701.899623	30.353562
437.515024	20729.606159	30.358580
437.744642	20755.140038	30.363597
438.185192	20780.135659	30.368615
438.415487	20811.172634	30.373632
439.374952	20837.843998	30.378650
439.644730	20856.105840	30.383668
440.307534	20876.568430	30.388685
440.823925	20892.978589	30.393703
441.103929	20912.426715	30.398720
441.594724	20935.696159	30.403738
442.100612	20961.124114	30.408756
442.378322	20993.303913	30.413773
442.932912	21023.507276	30.418791
443.053913	21055.086066	30.423808
443.609179	21085.655879	30.428826
443.670906	21098.478715	30.433844
444.131982	21138.357455	30.438861
444.863221	21166.998195	30.443879
445.303813	21200.941055	30.448896
445.739083	21216.397414	30.453914
446.239569	21247.298240	30.458932
446.737617	21283.721717	30.463949
447.405104	21306.863001	30.468967
447.571185	21335.257097	30.473984
447.894404	21353.763817	30.479002
448.854335	21380.884453	30.484020
448.721256	21417.027329	30.489037
449.234332	21437.115756	30.494055
449.680402	21472.119719	30.499072
450.020677	21499.362261	30.504090
450.544731	21531.776282	30.509108
450.792317	21564.037526	30.514125
451.042932	21586.169905	30.519143
451.463783	21612.496524	30.524160
452.118765	21643.759347	30.529178
452.403963	21666.562507	30.534196
452.926950	21703.267209	30.539213
453.027586	21726.320316	30.544231
453.453102	21770.104373	30.549248
454.247229	21800.928764	30.554266
455.059724	21823.940668	30.559284
454.968276	21863.572014	30.564301
455.885165	21891.590968	30.569319
455.826373	21925.031516	30.574336
456.705774	21956.702197	30.579354
457.081951	21979.219858	30.584372
457.710355	22010.980249	30.589389
458.208705	22039.791208	30.594407
458.434959	22080.675156	30.599424
458.788961	22113.059741	30.604442
459.571599	22140.986216	30.609460
459.605617	22186.317017	30.614477
460.243498	22210.708743	30.619495
460.570927	22250.831695	30.624512
461.282087	22277.985981	30.629530
461.769461	22306.274589	30.634548
461.848748	22346.758617	30.639565
462.575123	22369.841436	30.644583
463.101858	22398.250422	30.649600
463.748809	22436.017686	30.654618
464.052708	22465.371353	30.659636
464.195305	22507.987898	30.664653
464.671327	22530.932955	30.669671
465.129093	22577.538255	30.674688
465.742746	22626.002387	30.679706
466.573417	22654.111675	30.684724
467.040168	22691.326153	30.689741
467.913891	22712.819376	30.694759
468.202872	22742.460122	30.699776
468.264035	22790.492526	30.704794
469.167326	22819.917696	30.709812
469.123988	22853.079377	30.714829
469.840975	22875.071090	30.719847
470.489673	22905.534399	30.724864
470.922662	22944.953569	30.729882
471.675657	22972.708909	30.734900
471.243604	23010.771624	30.739917
472.484297	23044.548866	30.744935
472.838194	23071.197479	30.749952
472.898228	23107.780976	30.754970
473.562133	23135.916911	30.759988
473.903331	23172.760066	30.765005
474.616184	23196.629505	30.770023
475.404719	23227.033625	30.775040
475.726704	23263.102707	30.780058
476.312745	23290.593812	30.785076
476.918494	23330.087956	30.790093
477.120391	23347.320040	30.795111
477.590925	23384.522592	30.800128
478.099171	23415.716280	30.805146
478.760364	23442.671417	30.810164
479.227568	23473.258640	30.815181
479.279296	23499.891679	30.820199
480.211713	23533.730386	30.825216
480.061188	23569.804075	30.830234
480.814177	23594.862048	30.835252
481.078113	23650.422573	30.840269
481.543710	23678.451130	30.845287
481.963187	23713.450563	30.850304
482.671376	23743.710006	30.855322
483.051818	23772.371226	30.860340
483.621529	23814.999913	30.865357
484.049128	23833.549578	30.870375
484.872921	23864.865464	30.875392
484.860559	23892.204112	30.880410
485.617798	23911.157512	30.885428
485.648459	23945.649157	30.890445
486.338261	23977.358912	30.895463
486.518380	24012.674177	30.900480
486.870782	24046.224901	30.905498
487.552870	24088.015180	30.910516
488.051404	24125.834044	30.915533
488.294738	24168.842898	30.920551
488.993562	24207.812437	30.925568
489.343183	24243.721012	30.930586
490.009776	24284.382965	30.935604
490.556350	24322.118890	30.940621
490.789004	24348.788090	30.945639
491.306261	24395.028190	30.950656
491.869902	24435.921336	30.955674
492.659216	24481.411517	30.960692
493.244659	24522.844912	30.965709
493.459260	24556.487459	30.970727
493.833207	24599.040868	30.975744
494.193195	24634.803186	30.980762
494.965530	24670.349709	30.985780
495.279701	24714.189191	30.990797
495.786160	24752.481964	30.995815
496.661223	24802.206189	31.000832
496.655640	24846.411710	31.005850
497.577114	24887.313268	31.010868
497.802633	24920.126875	31.015885
498.411949	24971.485402	31.020903
499.170505	25004.412070	31.025920
499.755070	25037.359559	31.030938
500.233854	25078.317785	31.035956
500.742809	25117.432409	31.040973
501.092052	25158.429924	31.045991
502.048849	25202.220988	31.051008
502.592080	25232.148155	31.056026
502.971898	25266.853143	31.061044
503.455345	25305.573970	31.066061
504.077610	25338.358095	31.071079
504.494537	25375.989800	31.076096
504.939461	25409.269302	31.081114
505.678970	25434.704548	31.086132
506.294987	25473.999109	31.091149
506.742566	25500.048654	31.096167
507.711454	25531.502561	31.101184
508.251290	25561.822569	31.106202
508.977013	25597.712940	31.111220
508.784706	25623.457800	31.116237
509.667730	25649.667261	31.121255
510.197366	25679.186430	31.126272
510.461540	25722.789430	31.131290
510.936481	25748.563290	31.136308
511.298204	25779.638126	31.141325
511.877078	25802.830053	31.146343
512.760619	25839.391462	31.151360
513.177492	25869.029582	31.156378
513.787117	25892.229465	31.161396
514.454424	25923.497104	31.166413
514.673066	25946.751597	31.171431
515.368378	25963.157065	31.176448
515.514843	25992.982819	31.181466
516.487188	26022.541011	31.186484
516.423827	26057.379556	31.191501
516.605298	26090.694881	31.196519
517.691461	26114.629777	31.201536
517.973000	26147.954897	31.206554
518.309887	26174.085748	31.211572
518.574482	26207.230327	31.216589
518.944206	26235.833544	31.221607
519.747872	26272.781052	31.226624
520.127863	26317.713451	31.231642
520.412524	26347.802613	31.236660
521.165860	26379.563163	31.241677
521.805158	26416.542842	31.246695
522.155686	26438.336421	31.251712
522.585197	26491.812415	31.256730
523.106680	26522.067208	31.261748
523.241148	26555.542297	31.266765
524.074454	26599.463073	31.271783
524.628696	26645.639399	31.276800
525.101412	26688.365138	31.281818
525.621593	26728.094191	31.286836
526.482205	26766.285110	31.291853
526.716934	26808.397184	31.296871
527.510313	26848.842354	31.301888
527.668329	26892.015681	31.306906
528.291709	26928.733332	31.311924
528.920447	26961.380052	31.316941
529.461175	27005.897111	31.321959
530.141476	27031.861848	31.326976
530.469396	27091.403629	31.331994
531.149129	27122.582712	31.337012
531.660505	27169.670693	31.342029
532.063787	27209.431531	31.347047
532.895240	27244.922845	31.352064
533.307681	27281.800380	31.357082
533.720263	27334.472247	31.362100
534.606757	27376.907496	31.367117
534.866921	27419.174886	31.372135
535.588907	27456.105674	31.377152
535.735348	27499.086166	31.382170
536.571573	27537.282338	31.387188
537.213735	27580.640893	31.392205
537.621119	27621.223541	31.397223
538.306785	27663.949789	31.402240
538.495275	27703.846158	31.407258
539.029108	27752.139185	31.412276
539.759247	27789.081951	31.417293
540.402194	27836.467017	31.422311
541.285892	27878.556129	31.427328
541.657947	27918.449625	31.432346
542.215046	27959.875541	31.437364
542.984883	27995.030138	31.442381
543.167971	28031.597115	31.447399
543.306670	28069.928158	31.452416
543.868621	28117.307527	31.457434
544.755531	28160.294232	31.462452
545.436244	28194.331678	31.467469
545.893580	28242.207983	31.472487
546.759549	28277.373385	31.477504
546.993173	28323.034594	31.482522
547.752710	28362.969769	31.487540
548.554951	28397.873516	31.492557
548.754557	28434.849482	31.497575
549.571129	28468.531246	31.502592
550.005715	28508.131735	31.507610
550.522842	28547.896430	31.512628
550.894464	28583.120356	31.517645
551.538788	28628.471808	31.522663
552.051033	28652.075579	31.527680
552.550276	28699.756814	31.532698
553.142683	28733.859475	31.537716
553.852674	28773.916940	31.542733
553.701908	28809.083524	31.547751
554.473497	28844.688086	31.552768
554.812277	28888.172504	31.557786
555.398606	28920.942751	31.562804
556.054502	28963.758531	31.567821
556.305437	29014.260286	31.572839
557.783015	29044.351037	31.577856
557.910148	29080.119543	31.582874
558.366345	29129.692077	31.587892
558.686940	29152.763710	31.592909
559.241869	29200.134045	31.597927
559.755496	29233.232151	31.602944
560.761857	29284.811610	31.607962
560.622987	29332.612621	31.612980
561.747672	29377.107168	31.617997
562.015439	29430.186246	31.623015
562.690753	29460.788080	31.628032
563.181970	29511.506491	31.633050
563.606531	29556.217874	31.638068
564.686719	29601.649014	31.643085
564.972419	29655.092496	31.648103
565.850269	29690.037251	31.653120
566.060486	29740.983281	31.658138
566.589320	29787.859678	31.663156
567.628966	29829.745231	31.668173
568.084632	29883.643246	31.673191
568.532773	29923.016806	31.678208
568.920769	29970.364339	31.683226
569.412660	30019.339286	31.688244
570.376867	30056.945037	31.693261
570.792510	30107.095144	31.698279
571.494746	30154.868265	31.703296
571.963079	30194.384587	31.708314
572.601745	30246.055310	31.713332
573.143489	30292.014281	31.718349
573.652818	30333.572544	31.723367
574.731865	30358.253142	31.728384
575.596680	30405.426308	31.733402
576.087984	30439.319984	31.738420
576.908876	30475.747785	31.743437
577.024084	30521.678851	31.748455
577.730348	30558.655626	31.753472
578.487318	30599.259294	31.758490
579.239536	30634.155680	31.763508
579.743197	30671.006166	31.768525
580.370492	30713.962798	31.773543
580.887698	30747.309318	31.778560
581.194547	30777.799801	31.783578
581.615228	30827.356673	31.788596
582.276777	30864.625418	31.793613
582.858515	30912.754086	31.798631
583.346647	30944.455579	31.803648
584.076369	30986.012455	31.808666
584.424248	31033.918635	31.813684
585.340950	31070.869891	31.818701
586.016575	31118.383890	31.823719
586.813033	31154.677624	31.828736
587.297934	31184.932384	31.833754
588.058311	31216.870056	31.838772
588.108519	31254.335818	31.843789
588.494932	31301.933190	31.848807
589.143711	31344.211392	31.853824
589.566514	31392.132024	31.858842
589.941925	31438.802164	31.863860
590.822347	31478.484368	31.868877
591.382469	31527.667205	31.873895
592.234434	31565.754659	31.878912
593.053912	31613.297973	31.883930
593.414483	31646.360571	31.888948
593.718423	31677.352237	31.893965
594.069564	31715.985729	31.898983
594.854393	31762.744581	31.904000
595.175464	31801.711637	31.909018
595.471161	31849.197956	31.914036
596.125683	31891.185585	31.919053
596.789303	31946.283009	31.924071
597.052243	31996.903988	31.929088
597.706320	32041.509166	31.934106
598.325738	32108.700981	31.939124
599.066444	32156.061830	31.944141
599.649085	32209.781779	31.949159
600.504906	32261.240402	31.954176
600.786121	32302.762271	31.959194
600.842873	32349.231192	31.964212
602.061353	32401.278528	31.969229
602.717691	32463.907725	31.974247
603.174853	32505.130768	31.979264
603.944233	32556.925993	31.984282
604.644807	32619.637278	31.989300
605.390130	32666.176726	31.994317
606.165229	32720.272632	31.999335
606.901266	32778.749525	32.004352
607.660649	32823.984822	32.009370
607.800862	32868.399924	32.014388
608.407231	32912.451742	32.019405
609.058239	32966.706688	32.024423
609.903614	33017.277408	32.029440
610.271562	33066.095514	32.034458
610.721467	33127.658811	32.039476
611.621080	33172.462102	32.044493
612.576483	33219.324115	32.049511
613.114358	33267.041489	32.054528
613.844513	33318.041808	32.059546
614.097925	33362.471947	32.064564
615.069764	33407.574282	32.069581
615.645246	33454.274691	32.074599
616.308503	33501.448345	32.079616
616.830316	33552.367870	32.084634
617.156375	33606.523331	32.089652
617.831466	33655.554206	32.094669
618.401822	33702.875542	32.099687
619.122329	33756.919408	32.104704
620.005681	33810.957030	32.109722
620.388223	33859.572402	32.114740
621.554083	33905.840512	32.119757
621.903755	33963.173312	32.124775
622.486158	34006.365013	32.129792
623.383243	34040.473252	32.134810
623.855569	34091.351211	32.139828
624.695257	34133.061633	32.144845
625.443565	34178.295262	32.149863
626.010175	34228.653089	32.154880
626.551102	34270.132109	32.159898
627.236878	34309.439054	32.164916
627.993288	34361.645400	32.169933
628.729383	34407.102706	32.174951
628.843731	34448.395588	32.179968
629.885535	34487.299709	32.184986
630.106368	34530.036656	32.190004
631.157184	34575.590750	32.195021
631.268510	34620.785396	32.200039
632.034194	34666.270269	32.205056
632.471645	34705.894802	32.210074
633.034520	34771.055477	32.215092
633.887672	34808.864154	32.220109
634.618722	34847.090226	32.225127
634.958917	34897.269933	32.230144
635.854005	34938.277848	32.235162
635.772775	34981.777183	32.240180
636.437962	35020.519629	32.245197
637.296877	35066.989823	32.250215
637.861600	35116.262578	32.255232
638.602247	35166.203551	32.260250
638.922728	35220.016286	32.265268
639.501092	35266.890984	32.270285
639.970888	35315.837558	32.275303
640.695676	35369.853288	32.280320
641.283527	35417.491889	32.285338
642.022093	35480.414455	32.290356
642.492752	35535.582968	32.295373
643.590798	35591.241975	32.300391
644.129715	35643.276699	32.305408
645.132704	35689.649961	32.310426
645.687066	35733.747403	32.315444
646.246677	35788.795241	32.320461
646.772922	35846.889700	32.325479
647.091653	35899.300762	32.330496
648.282969	35961.035131	32.335514
649.294699	36017.846814	32.340532
649.786813	36061.878754	32.345549
650.299578	36107.285966	32.350567
650.350442	36168.572505	32.355584
651.368573	36217.751949	32.360602
652.237672	36279.802969	32.365620
652.615951	36337.725793	32.370637
653.368837	36396.115267	32.375655
653.804052	36442.673408	32.380672
654.794874	36499.331559	32.385690
655.476132	36564.612106	32.390708
655.994424	36605.428988	32.395725
656.734128	36661.475387	32.400743
657.606565	36719.689062	32.405760
658.680106	36759.774848	32.410778
659.317900	36810.791666	32.415796
659.823785	36859.717212	32.420813
660.907884	36915.811839	32.425831
660.801256	36964.630635	32.430848
662.044706	37012.126494	32.435866
662.788135	37059.915287	32.440884
663.389292	37107.675749	32.445901
663.747795	37149.656725	32.450919
664.223533	37216.438249	32.455936
665.414274	37259.813789	32.460954
665.617344	37321.440372	32.465972
666.213649	37377.422450	32.470989
666.798471	37431.926809	32.476007
667.138470	37488.410678	32.481024
667.882255	37532.096636	32.486042
669.006695	37601.965341	32.491060
669.277461	37650.018735	32.496077
670.313960	37713.495920	32.501095
670.751062	37775.662806	32.506112
671.455461	37824.161282	32.511130
672.270754	37867.052688	32.516148
672.654076	37919.692625	32.521165
673.537692	37980.791491	32.526183
674.091065	38045.698092	32.531200
675.073200	38098.928188	32.536218
675.520846	38150.110595	32.541236
676.330536	38201.243088	32.546253
677.067864	38253.841383	32.551271
677.827114	38316.218951	32.556288
678.384226	38362.091997	32.561306
679.326309	38410.757154	32.566324
679.978864	38447.623375	32.571341
680.832258	38501.892613	32.576359
680.945166	38544.850450	32.581376
681.947758	38578.045286	32.586394
682.627611	38636.471219	32.591412
683.125681	38673.918359	32.596429
683.904237	38723.899711	32.601447
684.565564	38776.498469	32.606464
685.441990	38822.063517	32.611482
686.237948	38861.709531	32.616500
686.687616	38911.476920	32.621517
687.092906	38953.915776	32.626535
687.508077	39006.837984	32.631552
688.434887	39051.181510	32.636570
689.299806	39110.572754	32.641588
689.699481	39178.624331	32.646605
690.517916	39221.397799	32.651623
691.118650	39282.841621	32.656640
691.725018	39340.528363	32.661658
692.412937	39399.195414	32.666676
692.997046	39451.434729	32.671693
693.887979	39507.958289	32.676711
694.393229	39569.715014	32.681728
695.174800	39631.991733	32.686746
696.114119	39687.641849	32.691764
696.546772	39754.330450	32.696781
697.460016	39807.018982	32.701799
698.030258	39874.584543	32.706816
699.109684	39932.104361	32.711834
699.665591	39986.094792	32.716852
699.629750	40044.522111	32.721869
700.928409	40098.156882	32.726887
701.372395	40166.868695	32.731904
701.854877	40233.019785	32.736922
702.950134	40300.321542	32.741940
703.780507	40360.303414	32.746957
704.262772	40418.107206	32.751975
705.146857	40482.432091	32.756992
705.849517	40546.039151	32.762010
706.563685	40606.368651	32.767028
707.348235	40671.158610	32.772045
708.542641	40729.415229	32.777063
709.011694	40787.285300	32.782080
710.005443	40840.823914	32.787098
710.365864	40898.458219	32.792116
711.084978	40961.374580	32.797133
711.950337	41014.737553	32.802151
713.053085	41073.825204	32.807168
713.717762	41120.149030	32.812186
714.819837	41167.517959	32.817204
715.057097	41228.239640	32.822221
715.847049	41272.001872	32.827239
716.524000	41329.834695	32.832256
717.206990	41389.108709	32.837274
717.990024	41426.130450	32.842292
718.667170	41493.241680	32.847309
719.399705	41545.254212	32.852327
720.034252	41604.903173	32.857344
720.453688	41655.883215	32.862362
721.152455	41706.155814	32.867380
721.655564	41772.346308	32.872397
722.231261	41832.371875	32.877415
723.108851	41889.479240	32.882432
723.690335	41954.671445	32.887450
724.665594	42016.387238	32.892468
725.727693	42082.270288	32.897485
726.391401	42129.121349	32.902503
726.812472	42185.225355	32.907520
727.579227	42233.648095	32.912538
728.142721	42271.780644	32.917556
728.849640	42341.419722	32.922573
729.868933	42396.210469	32.927591
730.403015	42456.497211	32.932608
730.564424	42513.218029	32.937626
731.686886	42562.060481	32.942644
732.284572	42627.941566	32.947661
733.063485	42680.411283	32.952679
733.665783	42745.229428	32.957696
734.663695	42806.153309	32.962714
735.483150	42852.001311	32.967732
736.239283	42923.241090	32.972749
737.248577	42988.458313	32.977767
737.870019	43041.832570	32.982784
738.277567	43104.228012	32.987802
739.061767	43157.545587	32.992820
739.696734	43224.428321	32.997837
740.374674	43284.321759	33.002855
741.263808	43354.340475	33.007872
741.884118	43418.588542	33.012890
742.466793	43479.161469	33.017908
743.078942	43549.869077	33.022925
744.182698	43609.671811	33.027943
744.765759	43674.204724	33.032960
745.500634	43741.054493	33.037978
746.453310	43806.972387	33.042996
747.338844	43887.467811	33.048013
748.041171	43944.772243	33.053031
748.873112	44007.173744	33.058048
749.787538	44072.820074	33.063066
750.715679	44137.218389	33.068084
751.189083	44206.558136	33.073101
752.074253	44256.934043	33.078119
753.136407	44318.516248	33.083136
753.756341	44384.456029	33.088154
754.851869	44441.529752	33.093172
755.437766	44505.179093	33.098189
756.564874	44557.042431	33.103207
757.044463	44612.327514	33.108224
757.884937	44671.478306	33.113242
758.212300	44733.416409	33.118260
758.830268	44796.884480	33.123277
759.741907	44855.328883	33.128295
760.463489	44933.007164	33.133312
761.154430	44999.450077	33.138330
762.144163	45058.787404	33.143348
762.425691	45119.721632	33.148365
763.354572	45187.918192	33.153383
764.162661	45252.673679	33.158400
764.874049	45324.168504	33.163418
765.405404	45388.398159	33.168436
766.052496	45466.621242	33.173453
767.240192	45532.615201	33.178471
767.852481	45596.345780	33.183488
768.586810	45666.617276	33.188506
769.247000	45741.840908	33.193524
770.065043	45809.057155	33.198541
770.949823	45868.545811	33.203559
771.774178	45938.601722	33.208576
772.180236	46011.000248	33.213594
773.748381	46073.621871	33.218612
774.169816	46149.605178	33.223629
775.097298	46214.281603	33.228647
776.017576	46276.207588	33.233664
776.595325	46334.834352	33.238682
777.453730	46386.193418	33.243700
778.121059	46447.204041	33.248717
779.113638	46507.468349	33.253735
779.719567	46567.691792	33.258752
780.694473	46627.699809	33.263770
781.280731	46680.923787	33.268788
782.389170	46741.683091	33.273805
782.537179	46795.911807	33.278823
783.115073	46846.992966	33.283840
783.475558	46917.029246	33.288858
784.446642	46988.153665	33.293876
785.200984	47061.020089	33.298893
786.112606	47140.359166	33.303911
786.675085	47210.276346	33.308928
787.631907	47279.056914	33.313946
788.164330	47343.861342	33.318964
788.699574	47428.776429	33.323981
789.893464	47503.701453	33.328999
791.123964	47569.372096	33.334016
791.678095	47646.573401	33.339034
792.633195	47717.993614	33.344052
793.005823	47796.830556	33.349069
794.298415	47866.686720	33.354087
795.075106	47924.552794	33.359104
795.728007	48002.100535	33.364122
797.447069	48075.313506	33.369140
798.018205	48139.576444	33.374157
798.724886	48202.293803	33.379175
799.846120	48260.847290	33.384192
800.056548	48333.195141	33.389210
801.316414	48394.776733	33.394228
801.679910	48467.879337	33.399245
802.605143	48541.622280	33.404263
803.623891	48603.463398	33.409280
804.230179	48666.134399	33.414298
804.976764	48722.919032	33.419316
806.088147	48802.966710	33.424333
806.882019	48877.218332	33.429351
807.604432	48940.732428	33.434368
808.575873	49012.255391	33.439386
809.337347	49079.642010	33.444404
809.992899	49148.987600	33.449421
811.068917	49217.413846	33.454439
811.917803	49275.683353	33.459456
812.376754	49356.226788	33.464474
813.397732	49415.861741	33.469492
814.062175	49497.069624	33.474509
814.328198	49558.277621	33.479527
815.775004	49639.788117	33.484544
816.525599	49704.957569	33.489562
817.280788	49775.966153	33.494580
817.779032	49853.499976	33.499597
818.745926	49919.629683	33.504615
819.755795	49996.831274	33.509632
820.211318	50074.828030	33.514650
821.268989	50145.727404	33.519668
822.057147	50220.806777	33.524685
822.985600	50303.336712	33.529703
823.873779	50362.115350	33.534720
824.908599	50444.844353	33.539738
825.317373	50514.631090	33.544756
826.308330	50592.811989	33.549773
826.792011	50659.170894	33.554791
827.772884	50730.919201	33.559808
828.398327	50820.692063	33.564826
829.399081	50899.916454	33.569844
830.210293	50977.468616	33.574861
830.842337	51054.055562	33.579879
832.083400	51116.311761	33.584896
832.573034	51188.397375	33.589914
833.434556	51249.067937	33.594932
834.223834	51316.861734	33.599949
835.209007	51394.255343	33.604967
836.114404	51460.785014	33.609984
836.781622	51531.888633	33.615002
837.675493	51591.865382	33.620020
838.756431	51665.796600	33.625037
839.201625	51732.354397	33.630055
840.712527	51798.107426	33.635072
841.075747	51875.789283	33.640090
841.943027	51934.467613	33.645108
843.084660	52010.269726	33.650125
843.582668	52078.547686	33.655143
844.104120	52149.739165	33.660160
845.203716	52222.922612	33.665178
846.268913	52305.242255	33.670196
847.538497	52372.053208	33.675213
847.886543	52451.776819	33.680231
849.337208	52521.369451	33.685248
849.921564	52586.566584	33.690266
850.526587	52655.082681	33.695284
851.045100	52725.751186	33.700301
852.486434	52801.604141	33.705319
853.462919	52865.658985	33.710336
854.471961	52938.023524	33.715354
854.816524	53007.998605	33.720372
855.934771	53084.364696	33.725389
856.883863	53153.866446	33.730407
858.006628	53229.808350	33.735424
858.687361	53305.812981	33.740442
859.835043	53365.432077	33.745460
860.763421	53429.173238	33.750477
861.401640	53499.635614	33.755495
862.295451	53564.262094	33.760512
863.176306	53638.920460	33.765530
864.069456	53706.173506	33.770548
864.603157	53781.322989	33.775565
865.351679	53857.046756	33.780583
866.452718	53927.596572	33.785600
867.124717	54003.959193	33.790618
867.830530	54080.107973	33.795636
868.794330	54154.666476	33.800653
869.248854	54244.789212	33.805671
870.306854	54319.023498	33.810688
871.128431	54392.522795	33.815706
872.174862	54482.617583	33.820724
873.516663	54551.334611	33.825741
874.299489	54631.947175	33.830759
874.698082	54706.006888	33.835776
875.741382	54781.795323	33.840794
876.295471	54866.475350	33.845812
877.149989	54943.704882	33.850829
878.001344	55028.130383	33.855847
879.164418	55095.845315	33.860864
880.250771	55190.347397	33.865882
881.186059	55270.103070	33.870900
882.236099	55338.924764	33.875917
883.640999	55418.993867	33.880935
884.872720	55482.168114	33.885952
885.587645	55547.960663	33.890970
886.289393	55619.501643	33.895988
886.848117	55684.243054	33.901005
887.660628	55757.127819	33.906023
889.074696	55825.381657	33.911040
889.789442	55893.712908	33.916058
890.559283	55963.503991	33.921076
891.760766	56016.394225	33.926093
892.527567	56075.965558	33.931111
893.594849	56137.483759	33.936128
893.782353	56200.955368	33.941146
894.810826	56259.802943	33.946164
895.876196	56320.448571	33.951181
896.697530	56385.214299	33.956199
897.113420	56452.695012	33.961216
897.874925	56517.748873	33.966234
898.482589	56595.901890	33.971252
899.364093	56676.911079	33.976269
900.273415	56749.100314	33.981287
900.853446	56827.138144	33.986304
902.211771	56907.877702	33.991322
903.331853	56976.421098	33.996340
904.195986	57050.991570	34.001357
904.962156	57129.963390	34.006375
906.010221	57204.290528	34.011392
906.995975	57282.576801	34.016410
907.573975	57363.433036	34.021428
908.968907	57445.352211	34.026445
909.302687	57522.506620	34.031463
910.211453	57597.622461	34.036480
911.016431	57680.197547	34.041498
911.920643	57769.592768	34.046516
912.982676	57849.989228	34.051533
914.205990	57938.955667	34.056551
915.397667	58012.617395	34.061568
915.932134	58092.122113	34.066586
916.783255	58185.533444	34.071604
917.856176	58264.397954	34.076621
918.790791	58346.309577	34.081639
919.568997	58433.112945	34.086656
920.560351	58520.959407	34.091674
921.608069	58617.202596	34.096692
922.390906	58683.600799	34.101709
923.131768	58774.689761	34.106727
924.170181	58857.359128	34.111744
925.036995	58948.239260	34.116762
926.091409	59036.723368	34.121780
927.124872	59121.166615	34.126797
927.833492	59219.654935	34.131815
929.331266	59297.197140	34.136832
929.640270	59387.475846	34.141850
930.624306	59481.048714	34.146868
932.087175	59548.558685	34.151885
932.511144	59651.586973	34.156903
933.759174	59737.764889	34.161920
934.507655	59836.471038	34.166938
935.448764	59912.867605	34.171956
936.848859	59990.889288	34.176973
937.901873	60080.592694	34.181991
938.857059	60160.222264	34.187008
940.263986	60235.800442	34.192026
940.633052	60309.508593	34.197044
942.167377	60395.764537	34.202061
942.748173	60482.852820	34.207079
943.650556	60560.327162	34.212096
944.483710	60640.964732	34.217114
945.337843	60729.479842	34.222132
946.204423	60799.978800	34.227149
946.866788	60891.904447	34.232167
948.039413	60970.154564	34.237184
949.393926	61056.200297	34.242202
950.061153	61133.269969	34.247220
951.968562	61214.913232	34.252237
952.488168	61280.973372	34.257255
953.542154	61353.875432	34.262272
954.520069	61422.573815	34.267290
955.232962	61498.985544	34.272308
955.807263	61560.486686	34.277325
957.121900	61628.455925	34.282343
957.963987	61705.525493	34.287360
958.984753	61781.782566	34.292378
959.655880	61847.687712	34.297396
960.858658	61920.777184	34.302413
961.475168	62002.282186	34.307431
962.094293	62070.398890	34.312448
962.913739	62154.993545	34.317466
964.014279	62236.284713	34.322484
964.731445	62308.950845	34.327501
965.817531	62399.410872	34.332519
967.067671	62476.659879	34.337536
968.320760	62548.027894	34.342554
969.018536	62639.745656	34.347572
969.899807	62715.451276	34.352589
970.778677	62801.982285	34.357607
971.875454	62879.724865	34.362624
973.323125	62959.369139	34.367642
974.432403	63043.928049	34.372660
975.436601	63115.697273	34.377677
976.587643	63192.793021	34.382695
977.522238	63274.480591	34.387712
978.616586	63352.433934	34.392730
978.863667	63437.856394	34.397748
980.103278	63514.426587	34.402765
981.048126	63596.265550	34.407783
981.884951	63674.196682	34.412800
982.894620	63753.576166	34.417818
983.470973	63844.228423	34.422836
984.422948	63943.641030	34.427853
985.497698	64036.381460	34.432871
986.441889	64132.478797	34.437888
987.257770	64219.695587	34.442906
987.943198	64328.951056	34.447924
988.915641	64422.702760	34.452941
989.945048	64525.840738	34.457959
991.205029	64635.286660	34.462976
992.336527	64726.317843	34.467994
993.316540	64827.318618	34.473012
994.369580	64919.331327	34.478029
995.201938	65014.050339	34.483047
996.195684	65111.675780	34.488064
997.150996	65210.561099	34.493082
998.600246	65308.920426	34.498100
999.695035	65408.582508	34.503117
1001.003773	65494.549454	34.508135
1001.560461	65596.720800	34.513152
1002.542750	65682.954457	34.518170
1003.421988	65784.531888	34.523188
1004.872260	65869.344825	34.528205
1006.167448	65957.562985	34.533223
1006.970196	66045.870768	34.538240
1008.372233	66129.242263	34.543258
1009.395971	66219.016728	34.548276
1010.372317	66301.321778	34.553293
1011.407241	66388.081465	34.558311
1012.290996	66470.395146	34.563328
1013.514284	66563.299043	34.568346
1015.013177	66642.548183	34.573364
1015.781886	66720.809590	34.578381
1017.276812	66796.856206	34.583399
1017.579562	66893.519769	34.588416
1018.416404	66970.030225	34.593434
1019.191445	67062.727144	34.598452
1020.531934	67150.777789	34.603469
1021.561380	67231.849302	34.608487
1021.751012	67314.989212	34.613504
1023.310656	67370.412377	34.618522
1024.590810	67453.718556	34.623540
1025.514829	67537.707259	34.628557
1026.320523	67610.837149	34.633575
1027.180415	67697.191673	34.638592
1028.380390	67759.566691	34.643610
1029.317539	67858.154915	34.648628
1030.014378	67950.069452	34.653645
1030.641078	68017.251358	34.658663
1031.264851	68130.686347	34.663680
1032.676974	68219.172740	34.668698
1033.467427	68321.989793	34.673716
1034.602641	68414.698866	34.678733
1035.781606	68521.768126	34.683751
1036.256426	68616.860141	34.688768
1037.512399	68721.201928	34.693786
1038.304049	68826.395224	34.698804
1039.592034	68934.639609	34.703821
1040.921568	69026.845754	34.708839
1041.838899	69142.854561	34.713856
1042.920496	69235.891530	34.718874
1043.867790	69340.986714	34.723892
1044.918219	69454.696713	34.728909
1046.151119	69556.740643	34.733927
1047.275213	69668.407553	34.738944
1049.046257	69750.986243	34.743962
1049.964300	69850.180277	34.748980
1051.019348	69950.854063	34.753997
1052.360181	70040.396265	34.759015
1053.389994	70142.144845	34.764032
1054.432047	70233.177942	34.769050
1055.348152	70330.284507	34.774068
1056.451419	70418.389599	34.779085
1057.904528	70506.085930	34.784103
1059.032486	70608.447946	34.789120
1060.103368	70699.908781	34.794138
1061.000861	70789.167966	34.799156
1062.722390	70870.459813	34.804173
1064.093518	70953.731478	34.809191
1064.891843	71046.667057	34.814208
1066.218284	71115.331173	34.819226
1067.650832	71195.301227	34.824244
1068.466885	71285.904586	34.829261
1069.275434	71368.315284	34.834279
1070.121649	71448.896639	34.839296
1071.418788	71540.565832	34.844314
1072.259490	71632.623017	34.849332
1073.244423	71719.047483	34.854349
1074.247595	71809.838831	34.859367
1074.873074	71899.536761	34.864384
1075.952479	71989.177006	34.869402
1077.341603	72081.353040	34.874420
1078.259436	72172.222250	34.879437
1079.892015	72269.680438	34.884455
1080.599909	72365.661762	34.889472
1081.683633	72455.328254	34.894490
1082.895728	72540.580179	34.899508
1083.621067	72645.108941	34.904525
1084.786951	72729.102125	34.909543
1085.874660	72828.040394	34.914560
1086.656479	72923.657604	34.919578
1087.455152	73016.093468	34.924596
1088.729929	73126.934747	34.929613
1089.854226	73219.371297	34.934631
1090.742559	73330.678883	34.939648
1091.846423	73422.308713	34.944666
1092.852695	73526.873221	34.949684
1093.779169	73618.670664	34.954701
1094.989921	73701.608679	34.959719
1095.933549	73795.227958	34.964736
1096.929390	73888.890103	34.969754
1098.221579	73985.242321	34.974772
1099.584789	74086.586952	34.979789
1100.673064	74177.259184	34.984807
1101.428705	74275.063914	34.989824
1102.494216	74360.559832	34.994842
1103.033168	74469.608639	34.999860
1104.065761	74562.494784	35.004877
1105.678715	74673.429196	35.009895
1106.364956	74784.115656	35.014912
1107.296515	74883.934528	35.019930
1108.643579	74993.632337	35.024948
1109.877122	75098.243625	35.029965
1111.278982	75201.993122	35.034983
1112.489766	75316.476126	35.040000
1113.465051	75430.362936	35.045018
1114.771821	75522.715726	35.050036
1115.713250	75633.834638	35.055053
1117.060145	75736.682741	35.060071
1118.112299	75846.062594	35.065088
1119.082459	75960.370451	35.070106
1120.752528	76063.954853	35.075124
1121.807801	76165.418606	35.080141
1123.145001	76276.136547	35.085159
1123.935495	76382.240505	35.090176
1124.859270	76479.317717	35.095194
1126.058893	76599.533499	35.100212
1127.425047	76707.867245	35.105229
1128.696096	76809.945861	35.110247
1129.591413	76909.815873	35.115264
1131.316158	77025.049499	35.120282
1132.724031	77114.085771	35.125300
1133.618627	77220.164132	35.130317
1135.134450	77316.480800	35.135335
1136.252578	77422.677168	35.140352
1137.186353	77526.964481	35.145370
1138.474517	77620.315406	35.150388
1139.415899	77723.601532	35.155405
1140.786816	77815.724132	35.160423
1141.888654	77924.040521	35.165440
1143.168326	78008.640563	35.170458
1144.619871	78109.834533	35.175476
1145.685053	78210.670971	35.180493
1147.354903	78300.975149	35.185511
1148.133461	78395.041446	35.190528
1149.326067	78484.014349	35.195546
1150.624577	78576.188784	35.200564
1151.777257	78671.084567	35.205581
1152.396717	78763.897396	35.210599
1153.327913	78864.909113	35.215616
1154.785224	78968.487003	35.220634
1156.223093	79056.790163	35.225652
1156.449990	79162.473236	35.230669
1158.205457	79264.916341	35.235687
1159.211304	79368.046595	35.240704
1160.147647	79471.732804	35.245722
1161.343227	79557.060144	35.250740
1162.290312	79676.695311	35.255757
1163.660752	79771.396291	35.260775
1164.738185	79877.621150	35.265792
1165.651934	79986.557694	35.270810
1166.874553	80087.541185	35.275828
1167.736373	80201.452869	35.280845
1168.664176	80304.674770	35.285863
1170.216524	80412.791450	35.290880
1171.014396	80514.868801	35.295898
1172.361807	80609.310173	35.300916
1173.488420	80722.207247	35.305933
1174.604879	80824.033434	35.310951
1175.271242	80924.257704	35.315968
1176.354410	81027.749492	35.320986
1177.999570	81132.712523	35.326004
1178.789010	81237.530416	35.331021
1179.943019	81346.029452	35.336039
1181.318788	81452.695318	35.341056
1182.134740	81575.044984	35.346074
1183.405557	81687.366045	35.351092
1184.572605	81804.252126	35.356109
1185.895593	81910.319801	35.361127
1187.366102	82033.165056	35.366144
1188.478990	82146.171362	35.371162
1190.363307	82260.312365	35.376180
1190.989373	82373.293997	35.381197
1192.401427	82471.633927	35.386215
1194.004483	82585.820028	35.391232
1195.110645	82685.690712	35.396250
1196.643019	82799.356534	35.401268
1197.718713	82909.014096	35.406285
1199.033625	83023.677602	35.411303
1199.670451	83133.264971	35.416320
1201.138217	83252.352880	35.421338
1202.332492	83352.427595	35.426356
1203.470818	83466.778276	35.431373
1204.758609	83579.420979	35.436391
1206.021824	83696.071842	35.441408
1206.638540	83811.949542	35.446426
1208.171236	83923.440473	35.451444
1209.126290	84044.398062	35.456461
1210.298466	84170.707434	35.461479
1211.599625	84291.979651	35.466496
1212.683036	84413.045528	35.471514
1214.409199	84529.120901	35.476532
1215.647535	84652.647174	35.481549
1217.242745	84759.265986	35.486567
1218.556160	84872.898138	35.491584
1219.611674	84978.436033	35.496602
1221.216772	85086.853821	35.501620
1222.317280	85216.853591	35.506637
1223.823267	85317.925705	35.511655
1224.831821	85428.401677	35.516672
1226.168002	85546.505916	35.521690
1227.526739	85650.491185	35.526708
1228.537147	85760.740055	35.531725
1229.770632	85877.809903	35.536743
1231.230246	85988.293837	35.541760
1232.174952	86092.763304	35.546778
1233.846906	86201.897156	35.551796
1235.108080	86318.292878	35.556813
1236.190757	86424.326025	35.561831
1237.244451	86530.262695	35.566848
1238.365571	86632.565114	35.571866
1239.876950	86747.631085	35.576884
1240.779688	86869.014164	35.581901
1241.325652	86985.536552	35.586919
1242.827109	87098.552592	35.591936
1244.077305	87227.993181	35.596954
1245.597100	87333.201272	35.601972
1246.681751	87451.757918	35.606989
1247.873126	87569.398702	35.612007
1249.449492	87689.729921	35.617024
1250.478418	87805.344028	35.622042
1251.891823	87916.932290	35.627060
1252.886150	88035.518027	35.632077
1253.878881	88146.551690	35.637095
1255.118107	88244.304615	35.642112
1255.936811	88362.247361	35.647130
1257.112174	88469.439370	35.652148
1258.437031	88583.553122	35.657165
1259.730229	88703.780495	35.662183
1261.213613	88817.959187	35.667200
1261.786713	88941.429785	35.672218
1263.481223	89058.896826	35.677236
1264.517776	89179.204096	35.682253
1266.070635	89295.629599	35.687271
1267.526628	89406.177681	35.692288
1268.814616	89536.522319	35.697306
1270.184030	89651.609079	35.702324
1271.321023	89772.904299	35.707341
1272.835812	89897.170110	35.712359
1274.241299	90012.024531	35.717376
1275.372470	90131.674591	35.722394
1276.774948	90251.295575	35.727412
1278.409251	90379.727010	35.732429
1278.974342	90492.217421	35.737447
1280.610626	90610.700857	35.742464
1281.807905	90732.890413	35.747482
1283.376641	90842.805267	35.752500
1284.321887	90969.534155	35.757517
1285.770333	91091.584687	35.762535
1287.292751	91220.620132	35.767552
1288.912240	91357.777630	35.772570
1290.068215	91461.992396	35.777588
1291.237118	91587.269596	35.782605
1292.180230	91717.056381	35.787623
1293.746456	91844.642843	35.792640
1294.963932	91972.220757	35.797658
1296.307170	92093.138375	35.802676
1297.668040	92227.437695	35.807693
1298.625227	92348.936065	35.812711
1300.317699	92470.713378	35.817728
1301.693457	92596.380808	35.822746
1303.250427	92712.945671	35.827764
1304.401474	92837.951982	35.832781
1305.961285	92968.243830	35.837799
1307.325561	93089.846563	35.842816
1308.437460	93210.145555	35.847834
1309.843661	93320.234129	35.852852
1311.566241	93444.824426	35.857869
1312.567438	93580.440491	35.862887
1314.177775	93687.279220	35.867904
1315.346826	93821.171799	35.872922
1316.511934	93926.382228	35.877940
1318.291016	94047.404530	35.882957
1319.603619	94177.854079	35.887975
1321.081229	94286.021079	35.892992
1322.062301	94406.902829	35.898010
1323.339700	94528.195236	35.903028
1324.233777	94659.117570	35.908045
1325.585719	94773.808227	35.913063
1327.131552	94899.699458	35.918080
1328.084208	95024.111783	35.923098
1329.380390	95163.440809	35.928116
1331.028144	95287.834729	35.933133
1331.794420	95402.859708	35.938151
1333.483303	95533.700052	35.943168
1334.529390	95674.033638	35.948186
1335.980423	95798.574303	35.953204
1337.559639	95929.319299	35.958221
1338.841619	96055.002765	35.963239
1341.164880	96159.381376	35.968256
1342.221624	96281.069898	35.973274
1343.602580	96381.894566	35.978292
1344.715740	96484.180949	35.983309
1345.756104	96592.614181	35.988327
1347.001109	96695.945518	35.993344
1348.107219	96816.246746	35.998362
1349.464512	96923.592352	36.003380
1350.789506	97037.877224	36.008397
1351.791952	97166.688970	36.013415
1353.216093	97278.563475	36.018432
1354.281529	97404.957898	36.023450
1355.562701	97524.309210	36.028468
1356.656958	97655.935495	36.033485
1358.048052	97794.805104	36.038503
1359.462440	97926.281274	36.043520
1360.810381	98071.864704	36.048538
1362.039177	98203.510353	36.053556
1363.395763	98343.034243	36.058573
1364.976891	98488.494550	36.063591
1366.646740	98616.244877	36.068608
1367.982318	98760.400903	36.073626
1368.946109	98888.794648	36.078644
1370.361024	99033.586082	36.083661
1371.310074	99176.422357	36.088679
1373.201162	99312.951577	36.093696
1374.801834	99456.511689	36.098714
1376.040576	99600.737282	36.103732
1377.923425	99734.467919	36.108749
1379.039121	99875.138910	36.113767
1380.719501	100011.779963	36.118784
1382.128358	100162.840053	36.123802
1383.544678	100302.870281	36.128820
1384.917768	100447.154819	36.133837
1385.914600	100587.137472	36.138855
1387.340618	100725.481901	36.143872
1388.989687	100868.926671	36.148890
1390.364043	101014.202398	36.153908
1391.855805	101150.712810	36.158925
1393.446965	101294.675587	36.163943
1394.750894	101428.034255	36.168960
1396.162796	101573.217888	36.173978
1397.566903	101714.638006	36.178996
1399.006714	101855.710871	36.184013
1400.467263	102003.120185	36.189031
1401.938668	102143.910456	36.194048
1403.520445	102286.142150	36.199066
1404.570598	102432.919970	36.204084
1406.388025	102563.300009	36.209101
1407.215023	102706.918839	36.214119
1408.856266	102850.005850	36.219136
1410.406198	103001.792482	36.224154
1411.848435	103145.532997	36.229172
1413.379744	103283.808461	36.234189
1414.811704	103421.022278	36.239207
1416.278128	103560.805084	36.244224
1417.972578	103703.557860	36.249242
1419.624103	103843.921630	36.254260
1421.059491	103979.539689	36.259277
1422.415405	104133.326931	36.264295
1423.900067	104253.115102	36.269312
1425.165807	104387.062238	36.274330
1426.324214	104522.548111	36.279348
1427.856296	104652.194677	36.284365
1429.400306	104798.487685	36.289383
1430.759709	104932.498503	36.294400
1432.172125	105075.047461	36.299418
1433.551530	105207.420632	36.304436
1435.237572	105346.631520	36.309453
1436.173960	105482.739079	36.314471
1437.418332	105603.609193	36.319488
1439.017870	105732.019515	36.324506
1439.998863	105858.193553	36.329524
1441.391475	105985.369085	36.334541
1442.867823	106127.253199	36.339559
1444.227508	106257.021537	36.344576
1445.318615	106394.275221	36.349594
1446.544236	106551.048189	36.354612
1448.361239	106684.804539	36.359629
1449.334419	106824.982017	36.364647
1450.789461	106961.369824	36.369664
1452.395657	107127.507465	36.374682
1453.668710	107275.641249	36.379700
1455.171409	107424.018896	36.384717
1456.146496	107580.264976	36.389735
1457.921032	107738.847316	36.394752
1459.561128	107886.837850	36.399770
1460.925063	108049.264278	36.404788
1462.752820	108203.136040	36.409805
1463.949641	108365.628010	36.414823
1465.340379	108519.734051	36.419840
1467.167218	108681.127678	36.424858
1468.598529	108839.413442	36.429876
1470.289050	108983.216194	36.434893
1472.145896	109134.652866	36.439911
1474.124253	109285.589413	36.444928
1475.434176	109436.516525	36.449946
1476.566638	109596.526133	36.454964
1478.618227	109741.074721	36.459981
1480.163190	109887.161086	36.464999
1481.236122	110044.823329	36.470016
1482.977227	110192.351452	36.475034
1484.419195	110343.350694	36.480052
1485.685002	110496.939628	36.485069
1487.288870	110660.152497	36.490087
1488.606735	110806.151219	36.495104
1490.403580	110949.159256	36.500122
1491.477057	111109.299070	36.505140
1493.197153	111268.020081	36.510157
1494.600885	111428.883514	36.515175
1496.060412	111580.696941	36.520192
1497.721791	111740.633967	36.525210
1499.124856	111907.206461	36.530228
1501.232140	112058.451880	36.535245
1502.616859	112211.801467	36.540263
1504.249879	112360.078321	36.545280
1505.698208	112514.624094	36.550298
1506.757720	112685.210482	36.555316
1508.541356	112836.458839	36.560333
1510.205790	112993.090956	36.565351
1511.869449	113143.547620	36.570368
1513.496288	113292.285850	36.575386
1514.668985	113455.007925	36.580404
1516.254458	113599.074067	36.585421
1517.766391	113745.498485	36.590439
1519.083007	113908.212881	36.595456
1520.906433	114059.384079	36.600474
1522.416168	114213.724656	36.605492
1524.420544	114363.220213	36.610509
1525.738756	114516.805559	36.615527
1527.170990	114669.409914	36.620544
1528.890172	114809.934234	36.625562
1530.098166	114973.773705	36.630580
1531.742051	115123.201655	36.635597
1533.511117	115274.766840	36.640615
1534.729690	115426.126622	36.645632
1536.364691	115565.398637	36.650650
1537.408236	115723.902102	36.655668
1538.932409	115864.714477	36.660685
1540.073183	116006.728554	36.665703
1541.428317	116149.597644	36.670720
1543.090580	116297.797221	36.675738
1544.207766	116446.538830	36.680756
1546.039200	116592.950265	36.685773
1547.744125	116753.714320	36.690791
1549.304739	116898.076331	36.695808
1550.439711	117046.221443	36.700826
1551.734573	117216.284980	36.705844
1553.756266	117369.683919	36.710861
1554.886647	117529.221633	36.715879
1556.191003	117692.423940	36.720896
1557.957633	117853.195805	36.725914
1559.140127	118034.810185	36.730932
1561.102916	118193.713804	36.735949
1562.824912	118359.822055	36.740967
1564.497616	118532.762755	36.745984
1565.909123	118689.927755	36.751002
1567.253877	118873.753324	36.756020
1568.860676	119038.106690	36.761037
1570.694466	119218.204741	36.766055
1572.243578	119382.936421	36.771072
1574.232427	119556.352635	36.776090
1575.744998	119724.414800	36.781108
1577.482489	119889.106659	36.786125
1579.362931	120069.150723	36.791143
1580.815100	120232.264834	36.796160
1582.688321	120406.134170	36.801178
1584.229515	120579.573947	36.806196
1585.466744	120739.971065	36.811213
1587.629591	120906.985827	36.816231
1589.517929	121070.149759	36.821248
1591.050149	121234.930059	36.826266
1592.798340	121392.294748	36.831284
1594.356772	121551.249875	36.836301
1596.005794	121717.815327	36.841319
1597.224220	121887.962311	36.846336
1598.833277	122059.520728	36.851354
1600.537022	122219.724487	36.856372
1602.450339	122383.613096	36.861389
1603.885829	122545.534407	36.866407
1605.212891	122720.044564	36.871424
1607.074088	122880.518278	36.876442
1608.287702	123056.557160	36.881460
1610.039459	123232.969751	36.886477
1611.667146	123401.968622	36.891495
1613.114676	123573.140145	36.896512
1614.517390	123757.246216	36.901530
1615.999626	123937.928263	36.906548
1617.488117	124115.603593	36.911565
1619.206483	124288.715041	36.916583
1620.530487	124483.784713	36.921600
1622.133364	124669.398845	36.926618
1623.615777	124853.725910	36.931636
1625.514687	125034.830129	36.936653
1626.987722	125227.622069	36.941671
1628.297051	125415.518112	36.946688
1630.017051	125597.198212	36.951706
1631.684003	125805.262509	36.956724
1633.368032	125985.237275	36.961741
1635.134461	126178.038817	36.966759
1636.415343	126381.560925	36.971776
1638.167448	126571.600870	36.976794
1639.783734	126760.876258	36.981812
1641.500341	126951.710070	36.986829
1643.282706	127148.142130	36.991847
1644.419429	127337.050771	36.996864
1646.503071	127510.791511	37.001882
1648.296709	127691.238811	37.006900
1649.628583	127860.644878	37.011917
1651.339364	128030.119535	37.016935
1652.634836	128217.624587	37.021952
1654.662102	128385.313288	37.026970
1656.165441	128559.351735	37.031988
1657.748942	128743.376065	37.037005
1659.329224	128924.813473	37.042023
1660.914740	129120.384691	37.047040
1662.439898	129302.187559	37.052058
1663.925259	129497.649244	37.057076
1665.723180	129685.387165	37.062093
1667.462217	129877.106334	37.067111
1668.855853	130081.923143	37.072128
1670.458584	130286.340449	37.077146
1672.001892	130480.719187	37.082164
1673.999294	130692.600928	37.087181
1675.868116	130889.633398	37.092199
1677.318816	131099.445285	37.097216
1679.028135	131302.099911	37.102234
1680.481725	131514.374870	37.107252
1681.870624	131719.809291	37.112269
1683.917109	131929.456366	37.117287
1685.508810	132141.103871	37.122304
1687.616849	132355.349305	37.127322
1689.002234	132570.076234	37.132340
1690.377501	132788.244394	37.137357
1692.542684	133007.749892	37.142375
1693.839376	133220.996567	37.147392
1695.752036	133432.511561	37.152410
1697.349008	133653.656752	37.157428
1699.170455	133882.952435	37.162445
1701.024648	134091.205960	37.167463
1702.422492	134326.495601	37.172480
1704.539051	134542.628346	37.177498
1706.440692	134763.033757	37.182516
1708.161593	134987.046737	37.187533
1710.262069	135197.094347	37.192551
1712.186040	135419.961232	37.197568
1713.894863	135631.150421	37.202586
1715.738155	135849.425750	37.207604
1717.371811	136055.337132	37.212621
1719.882827	136254.818886	37.217639
1721.119933	136477.226863	37.222656
1722.903610	136676.874431	37.227674
1724.564003	136889.384055	37.232692
1726.136465	137102.695119	37.237709
1728.208548	137298.341305	37.242727
1730.148070	137509.884007	37.247744
1731.747118	137714.970729	37.252762
1733.423212	137919.526082	37.257780
1735.334465	138133.804395	37.262797
1737.453857	138335.957622	37.267815
1738.411116	138548.140176	37.272832
1740.084826	138755.427971	37.277850
1742.059527	138962.416035	37.282868
1743.542152	139168.517135	37.287885
1745.827664	139380.204859	37.292903
1746.983899	139610.305485	37.297920
1748.560369	139831.077747	37.302938
1750.147315	140038.257800	37.307956
1751.867421	140250.875007	37.312973
1753.725707	140465.362571	37.317991
1755.253753	140709.345041	37.323008
1757.344862	140915.892056	37.328026
1758.454518	141142.682355	37.333044
1760.058994	141371.478025	37.338061
1762.025693	141579.798608	37.343079
1763.560525	141779.722383	37.348096
1765.182360	141988.123783	37.353114
1767.082475	142200.746993	37.358132
1768.434875	142416.654560	37.363149
1770.096040	142626.283621	37.368167
1771.854329	142858.666682	37.373184
1773.434503	143075.912374	37.378202
1774.951602	143302.433586	37.383220
1776.922265	143521.257663	37.388237
1778.785972	143738.779436	37.393255
1780.960494	143975.303883	37.398272
1782.729182	144199.175574	37.403290
1784.641904	144424.904229	37.408308
1786.215610	144653.148871	37.413325
1788.155690	144897.570391	37.418343
1789.741897	145127.185962	37.423360
1791.796779	145347.426435	37.428378
1793.514312	145591.847883	37.433396
1794.958060	145828.647108	37.438413
1796.642921	146077.213593	37.443431
1798.331260	146323.597690	37.448448
1799.810221	146567.274033	37.453466
1802.011629	146824.292949	37.458484
1803.398704	147076.210628	37.463501
1805.356763	147324.727942	37.468519
1807.586028	147580.096267	37.473536
1809.183392	147830.017543	37.478554
1811.310949	148076.189331	37.483572
1813.028372	148338.456971	37.488589
1814.750373	148595.483103	37.493607
1816.483844	148851.607514	37.498624
1818.696506	149106.363914	37.503642
1820.701133	149366.484948	37.508660
1822.783682	149621.390999	37.513677
1824.536037	149855.863070	37.518695
1826.385844	150126.305968	37.523712
1828.109719	150368.616365	37.528730
1830.242532	150628.012760	37.533748
1832.288766	150877.231160	37.538765
1833.987393	151130.452436	37.543783
1836.112364	151384.954037	37.548800
1838.294849	151634.941691	37.553818
1840.328827	151875.192279	37.558836
1841.815338	152130.774111	37.563853
1844.084142	152379.571212	37.568871
1845.576236	152636.131921	37.573888
1847.551485	152877.487662	37.578906
1849.484462	153119.282618	37.583924
1851.188054	153367.207372	37.588941
1852.970778	153625.631471	37.593959
1854.830943	153875.933250	37.598976
1856.512839	154128.510726	37.603994
1858.371611	154376.060327	37.609012
1859.993529	154626.961039	37.614029
1861.967182	154888.217355	37.619047
1863.718355	155147.808455	37.624064
1865.237562	155400.962728	37.629082
1867.046054	155676.313628	37.634100
1868.282395	155942.843389	37.639117
1870.089310	156217.524293	37.644135
1872.087581	156486.299129	37.649152
1873.698167	156766.154455	37.654170
1875.574080	157032.856221	37.659188
1877.033810	157324.023232	37.664205
1878.936543	157589.809309	37.669223
1880.799076	157873.451781	37.674240
1882.424901	158156.650030	37.679258
1884.342929	158416.991283	37.684276
1886.126970	158701.056114	37.689293
1887.870478	158962.632903	37.694311
1889.759476	159234.534706	37.699328
1891.722286	159499.989770	37.704346
1893.590190	159772.290795	37.709364
1895.594918	160058.016055	37.714381
1897.510337	160325.576777	37.719399
1899.103570	160607.356878	37.724416
1900.879460	160896.358938	37.729434
1902.584958	161172.081064	37.734452
1904.487771	161461.116751	37.739469
1906.522040	161746.273824	37.744487
1908.661861	162042.245184	37.749504
1910.372408	162342.118848	37.754522
1912.607202	162627.375608	37.759540
1914.144360	162927.037766	37.764557
1916.279728	163227.776235	37.769575
1918.220810	163517.399250	37.774592
1919.902088	163820.305965	37.779610
1921.893808	164117.947660	37.784628
1923.782463	164427.503049	37.789645
1925.797093	164720.420915	37.794663
1928.528023	165023.969645	37.799680
1930.557999	165321.267978	37.804698
1932.423394	165619.672432	37.809716
1934.082164	165920.370330	37.814733
1936.669686	166225.178344	37.819751
1938.517122	166531.994689	37.824768
1940.353573	166826.282550	37.829786
1942.281095	167134.473049	37.834804
1944.234676	167438.077341	37.839821
1946.100849	167742.547243	37.844839
1948.113478	168044.278551	37.849856
1950.114921	168354.608691	37.854874
1951.933790	168658.823280	37.859892
1953.584049	168975.610053	37.864909
1955.819515	169284.320697	37.869927
1958.477965	169580.866484	37.874944
1960.160756	169881.933157	37.879962
1962.717683	170187.778855	37.884980
1964.506554	170487.472915	37.889997
1966.444408	170788.033821	37.895015
1968.424450	171098.391758	37.900032
1970.535382	171405.226128	37.905050
1972.784627	171711.837071	37.910068
1974.990522	172009.770900	37.915085
1976.604850	172316.800555	37.920103
1978.384082	172622.231278	37.925120
1980.313805	172927.258868	37.930138
1982.231215	173227.591422	37.935156
1983.925387	173545.635199	37.940173
1985.515116	173875.251561	37.945191
1987.835717	174190.229176	37.950208
1989.097784	174510.210706	37.955226
1991.483141	174822.298328	37.960244
1993.209199	175148.863961	37.965261
1995.318684	175456.578072	37.970279
1996.992191	175790.722546	37.975296
1998.983503	176123.257054	37.980314
2001.107161	176441.626470	37.985332
2002.939768	176772.512137	37.990349
2004.702635	177108.171855	37.995367
2006.986815	177441.631157	38.000384
2008.904403	177776.723441	38.005402
2010.988046	178108.845157	38.010420
2013.006111	178446.057789	38.015437
2014.979479	178775.532558	38.020455
2017.053228	179092.599086	38.025472
2018.881900	179413.108158	38.030490
2020.867663	179717.923718	38.035508
2022.724068	180034.875094	38.040525
2024.701627	180345.383142	38.045543
2026.450412	180660.397872	38.050560
2028.536168	180985.241010	38.055578
2030.994082	181299.665045	38.060596
2033.045268	181624.211068	38.065613
2034.618434	181945.073713	38.070631
2037.174555	182280.515431	38.075648
2039.085135	182603.918448	38.080666
2040.695274	182920.918152	38.085684
2042.820173	183255.922490	38.090701
2044.832296	183598.819096	38.095719
2046.815725	183936.946448	38.100736
2048.719726	184283.646702	38.105754
2050.668712	184621.629394	38.110772
2052.674834	184962.880807	38.115789
2054.644718	185320.927748	38.120807
2056.526946	185668.575991	38.125824
2058.668125	186056.925367	38.130842
2060.614781	186461.993801	38.135860
2063.014868	186830.291190	38.140877
2064.854606	187199.159675	38.145895
2066.984821	187561.685162	38.150912
2068.988648	187922.580580	38.155930
2071.237905	188290.347732	38.160948
2073.080330	188655.309271	38.165965
2075.619209	189029.764786	38.170983
2077.939085	189383.478494	38.176000
2080.258180	189755.227465	38.181018
2082.097747	190117.882849	38.186036
2084.515928	190482.100349	38.191053
2086.303794	190860.971456	38.196071
2088.691909	191219.328492	38.201088
2090.601513	191594.169771	38.206106
2092.843843	191974.167555	38.211124
2094.632461	192340.470030	38.216141
2096.932884	192723.204392	38.221159
2098.939454	193089.221184	38.226176
2100.973263	193472.964589	38.231194
2103.229967	193850.832269	38.236212
2105.298825	194233.277080	38.241229
2107.137620	194607.935307	38.246247
2109.276758	194991.209652	38.251264
2111.480808	195380.825308	38.256282
2113.262293	195758.747075	38.261300
2115.664671	196143.304623	38.266317
2117.717708	196530.025936	38.271335
2120.103606	196909.203085	38.276352
2122.405827	197304.981492	38.281370
2124.442642	197684.977092	38.286388
2126.633019	198072.925922	38.291405
2128.905423	198460.227970	38.296423
2130.998188	198835.213700	38.301440
2132.681537	199235.208729	38.306458
2135.043543	199620.213642	38.311476
2137.873508	199994.630251	38.316493
2139.922525	200384.715356	38.321511
2142.070280	200758.020640	38.326528
2144.440960	201140.182855	38.331546
2146.322344	201515.614304	38.336564
2149.320263	201896.334326	38.341581
2150.792587	202261.035118	38.346599
2153.153154	202632.533302	38.351616
2155.321460	203014.756635	38.356634
2157.143100	203381.107358	38.361652
2158.932031	203739.436701	38.366669
2160.873826	204112.349457	38.371687
2162.891467	204462.414154	38.376704
2164.545404	204830.216387	38.381722
2166.540756	205198.144004	38.386740
2168.609749	205582.217035	38.391757
2170.663694	205951.915125	38.396775
2173.122002	206336.360848	38.401792
2175.136960	206721.460545	38.406810
2177.258065	207103.953314	38.411828
2178.977456	207487.220561	38.416845
2181.279280	207893.514638	38.421863
2183.387250	208282.971932	38.426880
2185.580753	208672.594393	38.431898
2187.656552	209086.292660	38.436916
2189.917999	209487.972401	38.441933
2192.093865	209896.601212	38.446951
2193.776368	210298.600978	38.451968
2196.273282	210723.617095	38.456986
2198.505226	211135.668571	38.462004
2200.585413	211556.889523	38.467021
2202.778239	211979.846412	38.472039
2204.935165	212397.703389	38.477056
2207.548271	212827.556643	38.482074
2209.798470	213252.665688	38.487092
2212.087367	213675.228909	38.492109
2214.336799	214103.717860	38.497127
2216.205478	214537.601375	38.502144
2218.542087	214967.805263	38.507162
2220.873450	215401.643201	38.512180
2223.133941	215829.853013	38.517197
2225.207368	216270.794296	38.522215
2227.867935	216700.568591	38.527232
2230.234224	217149.111745	38.532250
2232.374201	217573.861711	38.537268
2234.962293	218008.272001	38.542285
2237.081440	218449.716313	38.547303
2239.533330	218876.908393	38.552320
2241.952165	219312.336816	38.557338
2244.383193	219730.361922	38.562356
2247.117175	220162.185323	38.567373
2249.845184	220577.929178	38.572391
2252.462349	220996.205509	38.577408
2254.458441	221419.964362	38.582426
2256.635122	221844.965510	38.587444
2259.242762	222253.514154	38.592461
2261.086984	222684.511930	38.597479
2263.465671	223102.648426	38.602496
2265.507517	223530.287783	38.607514
2267.657913	223954.938076	38.612532
2269.726074	224382.370299	38.617549
2271.702847	224823.535025	38.622567
2274.157292	225249.586239	38.627584
2276.723527	225680.472269	38.632602
2278.376129	226114.066309	38.637620
2280.650028	226543.727631	38.642637
2282.486726	226987.632450	38.647655
2284.875310	227434.982498	38.652672
2287.150248	227883.493343	38.657690
2289.070067	228334.726785	38.662708
2291.417252	228778.983689	38.667725
2293.741361	229234.853704	38.672743
2296.423234	229674.637915	38.677760
2298.655134	230114.364956	38.682778
2301.178656	230566.494389	38.687796
2303.866208	231002.060047	38.692813
2306.054210	231447.585369	38.697831
2308.584780	231878.907090	38.702848
2310.934050	232303.067429	38.707866
2313.047684	232717.991715	38.712884
2315.445244	233122.684550	38.717901
2317.298304	233537.623401	38.722919
2319.833954	233951.312527	38.727936
2321.842338	234376.667541	38.732954
2323.869764	234799.885293	38.737972
2326.347908	235216.732362	38.742989
2329.320960	235623.645339	38.748007
2331.620130	236052.941911	38.753024
2333.946858	236473.469442	38.758042
2336.331488	236909.331354	38.763060
2338.671936	237335.419209	38.768077
2340.532621	237763.283265	38.773095
2342.463240	238209.655153	38.778112
2344.768215	238649.744301	38.783130
2346.581847	239110.409983	38.788148
2348.626206	239550.081169	38.793165
2350.893004	240027.746104	38.798183
2352.638724	240505.821588	38.803200
2355.041487	240981.634716	38.808218
2357.298517	241456.504361	38.813236
2359.383497	241936.760020	38.818253
2361.678984	242430.877593	38.823271
2363.897575	242929.578722	38.828288
2366.438481	243424.926246	38.833306
2368.829216	243927.764597	38.838324
2371.070293	244434.460982	38.843341
2373.259559	244950.944411	38.848359
2375.587532	245457.040622	38.853376
2378.099653	245976.545058	38.858394
2380.466871	246499.906539	38.863412
2383.102599	247008.161042	38.868429
2385.395903	247534.960629	38.873447
2387.947171	248061.261355	38.878464
2390.489126	248579.433227	38.883482
2392.760866	249107.146170	38.888500
2395.513904	249634.731826	38.893517
2398.009143	250155.243348	38.898535
2400.789648	250663.973054	38.903552
2403.268828	251189.488079	38.908570
2406.161715	251711.634748	38.913588
2409.078649	252213.911630	38.918605
2411.672939	252721.063452	38.923623
2414.431768	253234.614629	38.928640
2417.158256	253736.763716	38.933658
2419.294798	254240.831809	38.938676
2421.981837	254734.601060	38.943693
2424.563529	255234.862349	38.948711
2426.823442	255734.740095	38.953728
2429.404165	256237.512635	38.958746
2431.651593	256730.454120	38.963764
2434.394631	257231.622787	38.968781
2436.223563	257737.580157	38.973799
2438.633595	258238.771345	38.978816
2441.317512	258736.768227	38.983834
2443.340086	259247.312354	38.988852
2445.982063	259747.521542	38.993869
2448.417261	260268.335187	38.998887
2450.470943	260773.965731	39.003904
2453.039254	261280.606213	39.008922
2455.449988	261798.597438	39.013940
2457.778356	262309.969729	39.018957
2460.460901	262807.390843	39.023975
2462.899945	263326.970799	39.028992
2465.268728	263848.616585	39.034010
2467.494639	264360.833462	39.039028
2469.902230	264869.057292	39.044045
2472.224491	265369.646759	39.049063
2474.654980	265858.177770	39.054080
2477.028910	266353.395190	39.059098
2479.534461	266854.710830	39.064116
2481.967866	267341.938863	39.069133
2484.468945	267844.545530	39.074151
2486.403751	268352.393623	39.079168
2488.743692	268849.229291	39.084186
2490.865795	269361.843169	39.089204
2493.296321	269879.384278	39.094221
2495.698635	270414.451478	39.099239
2497.979334	270939.095988	39.104256
2500.344210	271474.696147	39.109274
2502.620723	272019.957903	39.114292
2505.209046	272553.891360	39.119309
2508.060070	273093.342661	39.124327
2510.535391	273643.871371	39.129344
2513.312150	274176.140082	39.134362
2515.914132	274733.296006	39.139380
2518.382898	275277.237360	39.144397
2521.047230	275818.097139	39.149415
2524.028171	276371.018051	39.154432
2526.705503	276918.090556	39.159450
2528.921024	277474.297504	39.164468
2531.884869	278019.235394	39.169485
2534.891811	278560.353463	39.174503
2537.290665	279101.740153	39.179520
2540.329532	279650.210244	39.184538
2542.832971	280194.772691	39.189556
2546.339136	280724.344610	39.194573
2548.399967	281272.548753	39.199591
2551.099005	281819.379783	39.204608
2553.755704	282351.357701	39.209626
2556.344025	282891.976308	39.214644
2558.890414	283435.111348	39.219661
2561.424280	283969.584953	39.224679
2563.760784	284519.448231	39.229696
2566.367845	285059.260132	39.234714
2568.737937	285615.711724	39.239732
2571.288602	286172.308435	39.244749
2573.866274	286720.008956	39.249767
2576.244462	287283.860222	39.254784
2578.630865	287840.874932	39.259802
2581.116187	288392.435659	39.264820
2583.699663	288966.067272	39.269837
2586.545289	289533.533648	39.274855
2588.564483	290108.791782	39.279872
2591.076481	290673.989333	39.284890
2593.596619	291252.434561	39.289908
2596.305676	291823.050118	39.294925
2599.213151	292398.910732	39.299943
2601.967471	292991.801151	39.304960
2604.605944	293561.751378	39.309978
2607.135386	294133.236563	39.314996
2609.572401	294707.701229	39.320013
2612.383324	295289.947385	39.325031
2614.785053	295869.280955	39.330048
2617.195114	296455.411626	39.335066
2620.088144	297038.313038	39.340084
2622.623427	297626.291043	39.345101
2625.521500	298204.482967	39.350119
2627.911193	298798.716871	39.355136
2630.608971	299382.538496	39.360154
2632.977025	299976.864757	39.365172
2635.089062	300559.901944	39.370189
2637.738645	301149.348203	39.375207
2640.767481	301743.806278	39.380224
2643.682768	302321.089166	39.385242
2646.039902	302889.948468	39.390260
2648.931648	303459.023090	39.395277
2651.440389	304022.921820	39.400295
2654.060992	304578.953129	39.405312
2656.902056	305127.455712	39.410330
2659.783234	305685.084561	39.415348
2662.062275	306240.694153	39.420365
2665.405882	306799.228816	39.425383
2667.900368	307357.432524	39.430400
2670.509250	307913.987681	39.435418
2673.066101	308487.145123	39.440436
2675.905928	309046.519885	39.445453
2678.577767	309615.204335	39.450471
2680.967287	310189.560886	39.455488
2684.200533	310751.088460	39.460506
2686.664312	311313.160697	39.465524
2689.264670	311898.581069	39.470541
2691.973715	312482.530592	39.475559
2694.472382	313058.256954	39.480576
2697.009590	313652.320093	39.485594
2699.548672	314245.309391	39.490612
2702.152757	314847.925164	39.495629
2704.620271	315434.235458	39.500647
2706.691276	316049.937848	39.505664
2709.560179	316660.584262	39.510682
2712.314263	317276.442758	39.515700
2715.034940	317898.515508	39.520717
2717.603822	318527.784957	39.525735
2719.861776	319148.744739	39.530752
2723.141455	319779.179848	39.535770
2725.967732	320410.589903	39.540788
2728.709550	321041.953104	39.545805
2731.338961	321691.011267	39.550823
2734.004876	322341.703234	39.555840
2736.980413	322982.719951	39.560858
2739.327543	323626.108364	39.565876
2742.107132	324277.716854	39.570893
2745.052202	324922.717575	39.575911
2747.777043	325582.560408	39.580928
2750.728087	326239.211161	39.585946
2753.334359	326894.458720	39.590964
2755.984108	327553.875244	39.595981
2759.363982	328205.479717	39.600999
2761.825382	328871.525774	39.606016
2764.943555	329528.223476	39.611034
2767.881743	330189.479493	39.616052
2770.333907	330855.163562	39.621069
2773.781766	331499.675387	39.626087
2776.428728	332165.281227	39.631104
2779.838668	332808.686136	39.636122
2782.566599	333467.762334	39.641140
2785.161253	334114.240062	39.646157
2788.304156	334750.043222	39.651175
2790.456325	335416.176255	39.656192
2793.638468	336076.886239	39.661210
2796.069403	336738.056432	39.666228
2798.628711	337406.195609	39.671245
2801.616454	338062.258257	39.676263
2804.379565	338729.707302	39.681280
2807.257546	339386.929779	39.686298
2810.100925	340049.269041	39.691316
2812.317825	340720.925659	39.696333
2815.186773	341379.127346	39.701351
2817.926426	342049.688226	39.706368
2821.090735	342730.568466	39.711386
2823.791423	343406.384590	39.716404
2826.189733	344071.202695	39.721421
2829.358155	344732.008017	39.726439
2832.345979	345389.810886	39.731456
2834.884903	346014.780008	39.736474
2837.712047	346645.423825	39.741492
2840.549849	347294.743222	39.746509
2843.574585	347930.277035	39.751527
2845.571267	348574.808407	39.756544
2848.341201	349236.069188	39.761562
2851.124203	349886.893249	39.766580
2853.961486	350543.755981	39.771597
2856.855079	351206.935541	39.776615
2859.496655	351886.697406	39.781632
2861.906527	352554.539192	39.786650
2864.577205	353229.171994	39.791668
2867.131016	353918.995251	39.796685
2869.871730	354611.613931	39.801703
2872.601514	355317.503575	39.806720
2875.000601	356026.369587	39.811738
2878.220958	356731.669354	39.816756
2880.750959	357453.031207	39.821773
2884.251124	358187.178926	39.826791
2886.679385	358910.905355	39.831808
2889.921911	359635.628617	39.836826
2893.013677	360373.057325	39.841844
2895.616610	361112.115639	39.846861
2898.895370	361838.453358	39.851879
2901.766696	362585.823298	39.856896
2904.587089	363319.749353	39.861914
2908.145639	364063.882963	39.866932
2910.761325	364802.188613	39.871949
2914.069813	365542.522010	39.876967
2916.856147	366286.820610	39.881984
2919.919441	367037.012366	39.887002
2923.070930	367777.541093	39.892020
2925.796059	368521.309956	39.897037
2929.315349	369271.042784	39.902055
2932.640354	370009.408584	39.907072
2935.498586	370754.567794	39.912090
2938.548361	371493.393539	39.917108
2941.617005	372244.054703	39.922125
2944.730136	372971.809535	39.927143
2947.922164	373719.801785	39.932160
2950.808003	374462.323530	39.937178
2954.166833	375204.143463	39.942196
2956.579050	375947.179826	39.947213
2959.922502	376686.124206	39.952231
2962.994712	377428.662410	39.957248
2965.749732	378166.846966	39.962266
2969.262650	378899.649576	39.967284
2972.002658	379640.278024	39.972301
2975.524639	380369.086960	39.977319
2978.681121	381107.684259	39.982336
2981.941776	381832.491158	39.987354
2984.656071	382564.176035	39.992372
2988.077238	383292.842967	39.997389
2990.924384	384026.390610	40.002407
2993.636980	384746.996868	40.007424
2996.746172	385473.168512	40.012442
2999.826117	386193.702009	40.017460
3002.540352	386936.480491	40.022477
3005.604364	387658.696637	40.027495
3008.598262	388398.830784	40.032512
3011.324633	389129.767717	40.037530
3014.521996	389867.750200	40.042548
3016.640371	390606.308996	40.047565
3019.718006	391353.861791	40.052583
3022.512985	392099.005226	40.057600
3025.568188	392850.819807	40.062618
3028.972842	393587.164278	40.067636
3031.489526	394304.840190	40.072653
3034.836445	395018.821402	40.077671
3037.752235	395738.164423	40.082688
3040.535983	396450.772909	40.087706
3043.404191	397167.346292	40.092724
3046.398763	397890.054427	40.097741
3049.382550	398609.249121	40.102759
3052.326053	399342.247515	40.107776
3055.445972	400071.601486	40.112794
3058.597306	400802.496838	40.117812
3061.387948	401531.501838	40.122829
3064.567123	402272.925091	40.127847
3067.550347	403010.356484	40.132864
3070.091454	403768.887117	40.137882
3073.514202	404518.499852	40.142900
3076.407638	405287.299883	40.147917
3079.413304	406039.305673	40.152935
3082.482446	406808.633696	40.157952
3085.294511	407585.009022	40.162970
3088.492296	408356.945603	40.167988
3091.513095	409136.422110	40.173005
3094.465747	409926.355328	40.178023
3097.763156	410715.649971	40.183040
3101.162516	411507.885307	40.188058
3104.131794	412296.162029	40.193076
3107.097858	413108.339608	40.198093
3110.117625	413907.021920	40.203111
3113.190176	414701.872415	40.208128
3116.194282	415524.272422	40.213146
3119.706651	416329.211939	40.218164
3122.923821	417147.014260	40.223181
3126.152053	417949.761471	40.228199
3129.561358	418764.891678	40.233216
3132.518687	419578.897306	40.238234
3135.701087	420399.815155	40.243252
3139.249580	421214.069453	40.248269
3142.390512	422031.288095	40.253287
3145.642222	422853.817122	40.258304
3148.877584	423677.883210	40.263322
3152.397470	424486.450269	40.268340
3155.542874	425304.751044	40.273357
3158.728586	426129.433390	40.278375
3162.008247	426950.528470	40.283392
3164.736654	427786.437568	40.288410
3168.359760	428591.639101	40.293428
3171.398626	429428.088324	40.298445
3174.409398	430260.007901	40.303463
3177.623033	431085.138304	40.308480
3180.598408	431923.766304	40.313498
3183.818147	432753.425102	40.318516
3187.299246	433589.679128	40.323533
3190.101344	434438.030634	40.328551
3193.125141	435273.221939	40.333568
3196.228942	436126.657401	40.338586
3199.410950	436974.130695	40.343604
3202.685289	437822.158378	40.348621
3205.585658	438683.040033	40.353639
3208.977346	439529.507978	40.358656
3211.922740	440384.848637	40.363674
3215.358445	441229.566141	40.368692
3218.970796	442102.658926	40.373709
3221.868000	442945.210451	40.378727
3225.404817	443812.324597	40.383744
3228.265105	444655.915366	40.388762
3231.554911	445516.674181	40.393780
3235.269991	446374.447658	40.398797
3238.463580	447234.938655	40.403815
3241.735767	448054.825066	40.408832
3244.852103	448887.525142	40.413850
3248.295685	449693.423704	40.418868
3251.782355	450507.156442	40.423885
3254.601938	451313.937784	40.428903
3258.178848	452123.897108	40.433920
3261.275503	452929.602941	40.438938
3264.392411	453740.115504	40.443956
3267.376293	454553.388091	40.448973
3271.130969	455371.702558	40.453991
3274.389536	456181.777770	40.459008
3277.648462	457003.424594	40.464026
3281.206021	457821.705460	40.469044
3284.148212	458645.898011	40.474061
3287.157365	459469.283828	40.479079
3290.925558	460298.769855	40.484096
3293.720802	461142.446293	40.489114
3297.458204	461972.057910	40.494132
3300.842960	462813.289287	40.499149
3303.928079	463660.075673	40.504167
3307.453917	464501.100361	40.509184
3310.429889	465359.473054	40.514202
3314.015971	466210.694691	40.519220
3317.418201	467061.952049	40.524237
3320.497085	467936.571087	40.529255
3323.951118	468790.556674	40.534272
3326.919186	469654.862975	40.539290
3330.279028	470522.694268	40.544308
3333.294720	471397.190247	40.549325
3336.626097	472281.323175	40.554343
3340.178168	473156.397900	40.559360
3343.362923	474058.358414	40.564378
3346.678075	474944.012852	40.569396
3350.156932	475840.685114	40.574413
3353.601614	476731.918192	40.579431
3356.651610	477625.582832	40.584448
3359.973378	478545.468849	40.589466
3363.383841	479453.341418	40.594484
3366.715258	480376.799325	40.599501
3369.956515	481284.139326	40.604519
3373.340238	482205.868900	40.609536
3376.585391	483137.846268	40.614554
3379.827618	484067.097599	40.619572
3383.435962	484991.399026	40.624589
3386.834425	485925.049629	40.629607
3390.246277	486857.281255	40.634624
3393.747397	487790.298843	40.639642
3397.546852	488720.039378	40.644660
3400.605201	489655.077354	40.649677
3403.909325	490599.740987	40.654695
3407.678844	491542.812568	40.659712
3411.679798	492477.277603	40.664730
3416.059013	493391.380529	40.669748
3419.938479	494309.936855	40.674765
3423.231657	495227.621435	40.679783
3427.393230	496129.505185	40.684800
3430.941438	497041.146713	40.689818
3434.820878	497935.160126	40.694836
3438.186954	498832.018236	40.699853
3440.999990	499730.971426	40.704871
3444.790705	500638.425322	40.709888
3448.073007	501541.371759	40.714906
3450.996869	502445.223698	40.719924
3454.360621	503362.136292	40.724941
3457.083791	504278.637289	40.729959
3460.578562	505180.870002	40.734976
3463.602105	506107.673926	40.739994
3467.464957	507034.538569	40.745012
3470.620233	507948.522372	40.750016
3473.574962	508826.990544	40.755021
3477.393583	509661.594542	40.760026
3480.614266	510441.121764	40.765031
3483.938979	511173.237901	40.770036
3487.127863	511848.205093	40.775040
3489.573470	512469.000178	40.780045
3492.550746	513034.272259	40.785050
3494.911769	513550.408230	40.790055
3497.196069	514012.388675	40.795060
3499.629352	514419.024292	40.800064
3501.570429	514796.232019	40.805069
3503.276508	515105.105494	40.810074
3504.743951	515378.216366	40.815079
3506.334132	515613.544469	40.820084
3508.007309	515806.812993	40.825088
3509.200856	515972.478204	40.830093
3509.989480	516107.706526	40.835098
3511.290811	516216.640865	40.840103
3512.427733	516280.937467	40.845108
3513.397222	516315.367289	40.850112
3513.860474	516339.592377	40.855117
3515.041833	516327.260016	40.860122
3515.910058	516289.368552	40.865127
3516.138564	516240.335259	40.870132
3516.665283	516164.689553	40.875136
3517.090752	516081.245655	40.880141
3517.836030	515980.359954	40.885146
3518.279108	515868.682248	40.890151
3518.566888	515738.627744	40.895156
3519.167967	515589.316414	40.900160
3519.030235	515428.069905	40.905165
3520.004469	515261.960075	40.910170
3519.491792	515078.334066	40.915175
3519.947474	514892.588768	40.920180
3520.140619	514697.000501	40.925184
3520.374407	514496.916148	40.930189
3520.389799	514285.972937	40.935194
3520.290784	514065.616292	40.940199
3520.708929	513846.738626	40.945204
3520.765045	513617.174625	40.950208
3520.576114	513398.636455	40.955213
3520.798004	513156.030750	40.960218
3520.863050	512919.949585	40.965223
3520.212907	512675.303074	40.970228
3520.580007	512438.965060	40.975232
3520.526929	512201.780795	40.980237
3520.460649	511960.459711	40.985242
3520.067193	511707.688292	40.990247
3519.909720	511468.995050	40.995252
3520.195083	511212.881746	41.000256
3519.830565	510972.043862	41.005261
3520.364533	510720.471861	41.010266
3520.155393	510466.439045	41.015271
3519.764777	510216.716522	41.020276
3519.778138	509958.353243	41.025280
3519.246500	509707.080215	41.030285
3519.490060	509447.310043	41.035290
3519.478701	509213.952155	41.040295
3519.132041	508958.350035	41.045300
3519.098948	508713.487916	41.050304
3519.004999	508474.280015	41.055309
3518.658191	508215.486923	41.060314
3518.281352	507976.617258	41.065319
3518.425311	507731.054879	41.070324
3518.354210	507485.420834	41.075328
3517.902511	507249.677910	41.080333
3517.915814	507001.903814	41.085338
3517.413312	506767.421861	41.090343
3517.133755	506539.055553	41.095348
3517.370735	506307.275829	41.100352
3516.859703	506085.496134	41.105357
3517.228377	505850.359065	41.110362
3516.580402	505635.454438	41.115367
3516.520528	505409.255550	41.120372
3516.490405	505180.273758	41.125376
3516.334066	504961.145668	41.130381
3516.235612	504739.684491	41.135386
3515.834658	504527.247314	41.140391
3515.844426	504312.724994	41.145396
3515.752953	504096.499826	41.150400
3515.606763	503889.361574	41.155405
3515.216932	503679.987808	41.160410
3515.134697	503468.847658	41.165415
3515.067456	503281.819945	41.170420
3515.152662	503063.886738	41.175424
3514.868106	502858.622090	41.180429
3514.527851	502655.684257	41.185434
3514.530321	502459.249863	41.190439
3513.968290	502259.217115	41.195444
3513.853051	502067.841654	41.200448
3513.613482	501881.680458	41.205453
3513.824716	501687.423375	41.210458
3513.448886	501506.778851	41.215463
3513.342495	501316.905961	41.220468
3513.859976	501137.530785	41.225472
3513.037000	500950.691486	41.230477
3512.918376	500770.451956	41.235482
3512.754240	500598.342158	41.240487
3512.637469	500421.378249	41.245492
3512.578618	500252.477786	41.250496
3512.357314	500072.548400	41.255501
3512.455413	499903.871813	41.260506
3512.164198	499738.988497	41.265511
3511.517173	499572.846505	41.270516
3511.473772	499412.311710	41.275520
3511.753479	499252.128633	41.280525
3511.613569	499093.523211	41.285530
3511.656079	498936.553222	41.290535
3511.331792	498781.102300	41.295540
3511.468611	498625.729392	41.300544
3511.166582	498473.754310	41.305549
3511.200358	498312.438376	41.310554
3510.968043	498164.133768	41.315559
3510.951927	498011.857048	41.320564
3510.744365	497858.548580	41.325568
3510.544416	497722.297886	41.330573
3510.823536	497579.863851	41.335578
3510.829851	497439.439454	41.340583
3510.187600	497289.069831	41.345588
3510.085352	497148.508128	41.350592
3510.037539	497004.655582	41.355597
3510.015717	496875.133318	41.360602
3510.367992	496736.465603	41.365607
3509.805681	496599.857104	41.370612
3509.878107	496455.475715	41.375616
3509.911580	496327.050592	41.380621
3510.099106	496196.783096	41.385626
3509.525328	496060.423802	41.390631
3509.283639	495930.877008	41.395636
3509.414406	495805.057238	41.400640
3509.405571	495680.974513	41.405645
3509.118999	495542.596967	41.410650
3509.303245	495424.994289	41.415655
3508.976015	495298.130873	41.420660
3508.862026	495173.202054	41.425664
3508.877474	495055.521754	41.430669
3508.922805	494941.773662	41.435674
3508.901955	494819.906936	41.440679
3508.923449	494700.607374	41.445684
3509.114204	494575.222233	41.450688
3508.787951	494454.258299	41.455693
3508.215712	494337.522042	41.460698
3508.116222	494221.115201	41.465703
3508.203883	494114.321401	41.470708
3508.738971	494002.660887	41.475712
3508.428387	493892.241873	41.480717
3508.111129	493762.889921	41.485722
3508.326823	493654.810704	41.490727
3508.254714	493543.847119	41.495732
3508.057352	493428.610588	41.500736
3507.914100	493336.034731	41.505741
3507.879602	493217.034975	41.510746
3507.574229	493115.394726	41.515751
3507.780656	493022.358591	41.520756
3507.655479	492924.172880	41.525760
3507.608386	492818.148174	41.530765
3507.544048	492702.986347	41.535770
3506.912897	492601.999218	41.540775
3507.450482	492509.766746	41.545780
3507.529727	492418.059469	41.550784
3507.456385	492321.780487	41.555789
3507.330468	492220.712174	41.560794
3507.199561	492118.280620	41.565799
3507.234622	492027.688707	41.570804
3507.066346	491924.958688	41.575808
3507.001696	491824.383126	41.580813
3506.995520	491728.140390	41.585818
3506.838206	491650.603927	41.590823
3507.021199	491559.935686	41.595828
3506.995111	491454.655542	41.600832
3506.704532	491378.400822	41.605837
3506.551714	491276.168941	41.610842
3506.442124	491193.926500	41.615847
3506.702446	491106.525814	41.620852
3506.641709	491016.447710	41.625856
3506.542462	490930.970376	41.630861
3506.563467	490844.059896	41.635866
3506.890910	490757.656715	41.640871
3506.675916	490675.074365	41.645876
3506.781804	490573.706454	41.650880
3506.654486	490482.423551	41.655885
3506.434469	490403.779459	41.660890
3506.300003	490317.193147	41.665895
3505.873438	490247.670385	41.670900
3506.195622	490155.204557	41.675904
3506.126264	490080.625888	41.680909
3506.161996	489999.162355	41.685914
3506.130462	489923.971018	41.690919
3506.265392	489843.046725	41.695924
3505.983659	489758.702211	41.700928
3505.798935	489689.745281	41.705933
3506.093979	489601.825497	41.710938
3505.997975	489532.551033	41.715943
3506.050460	489453.354584	41.720948
3505.669092	489371.094041	41.725952
3505.928258	489289.490929	41.730957
3505.736533	489208.361573	41.735962
3505.789039	489147.445857	41.740967
3505.702168	489071.248836	41.745972
3505.769437	488992.148696	41.750976
3505.548011	488932.032312	41.755981
3505.476279	488858.710634	41.760986
3505.915636	488786.672710	41.765991
3505.516238	488705.572994	41.770996
3505.619826	488623.636990	41.776000
3505.967912	488572.723600	41.781005
3505.424656	488487.049079	41.786010
3505.608029	488413.938097	41.791015
3505.413088	488340.986648	41.796020
3505.435124	488269.465785	41.801024
3505.375083	488210.281073	41.806029
3505.353561	488131.644853	41.811034
3505.418667	488063.853863	41.816039
3505.450327	487992.279698	41.821044
3505.589831	487917.910478	41.826048
3505.352715	487859.509583	41.831053
3505.286479	487792.646976	41.836058
3505.409240	487726.461788	41.841063
3505.141005	487663.115141	41.846068
3505.099245	487585.691478	41.851072
3505.382908	487527.511331	41.856077
3505.276730	487459.390753	41.861082
3505.522497	487389.750325	41.866087
3505.119417	487325.615111	41.871092
3505.323751	487257.697868	41.876096
3505.314583	487183.146178	41.881101
3505.064628	487117.268912	41.886106
3504.925966	487062.637953	41.891111
3504.569641	486997.483875	41.896116
3504.961927	486931.455360	41.901120
3504.843014	486859.141668	41.906125
3504.911187	486808.771093	41.911130
3504.985591	486751.176196	41.916135
3504.605672	486681.730946	41.921140
3504.891308	486632.689780	41.926144
3504.724791	486583.163182	41.931149
3504.885497	486515.249447	41.936154
3505.190303	486462.769901	41.941159
3504.787714	486398.529712	41.946164
3505.199340	486318.250894	41.951168
3504.924024	486267.325839	41.956173
3504.967488	486198.317657	41.961178
3504.924412	486132.252435	41.966183
3505.083179	486084.795197	41.971188
3505.181455	486011.736530	41.976192
3504.863976	485948.289446	41.981197
3504.637931	485880.837215	41.986202
3504.974921	485818.954740	41.991207
3504.666122	485762.577620	41.996212
3504.705944	485699.983185	42.001216
3504.786650	485647.232646	42.006221
3504.645854	485591.637006	42.011226
3504.609647	485527.538234	42.016231
3504.494751	485472.493809	42.021236
3504.899053	485406.861024	42.026240
3504.577159	485359.223772	42.031245
3504.340804	485292.326254	42.036250
3504.895241	485239.652155	42.041255
3504.776292	485184.859920	42.046260
3505.031029	485135.667256	42.051264
3504.569076	485067.136805	42.056269
3504.528734	485012.180174	42.061274
3504.684308	484953.656623	42.066279
3504.486868	484900.542678	42.071284
3504.684013	484847.872330	42.076288
3504.536282	484791.315049	42.081293
3504.646496	484724.916847	42.086298
3504.871893	484661.986225	42.091303
3504.749881	484622.044949	42.096308
3504.773159	484550.658170	42.101312
3504.521636	484493.156091	42.106317
3504.742896	484426.284659	42.111322
3504.636887	484375.276501	42.116327
3504.605471	484322.538898	42.121332
3504.518217	484251.471061	42.126336
3504.564801	484209.380648	42.131341
3504.783885	484152.966038	42.136346
3504.540853	484091.571086	42.141351
3504.031517	484041.028757	42.146356
3504.512072	483979.066075	42.151360
3504.570858	483925.656316	42.156365
3504.284912	483873.310442	42.161370
3504.538384	483832.752972	42.166375
3504.259405	483769.088878	42.171380
3504.370184	483712.032743	42.176384
3504.253520	483666.631829	42.181389
3504.377893	483608.562762	42.186394
3504.566646	483562.204619	42.191399
3504.436711	483506.700857	42.196404
3504.435405	483441.729154	42.201408
3504.463494	483397.365905	42.206413
3504.538473	483340.364502	42.211418
3504.868464	483285.495703	42.216423
3504.480360	483224.574611	42.221428
3504.176012	483165.408571	42.226432
3504.242062	483118.411398	42.231437
3504.208589	483058.444945	42.236442
3504.112333	483007.127641	42.241447
3504.123284	482956.905018	42.246452
3504.784708	482906.631537	42.251456
3504.188261	482851.450657	42.256461
3504.195774	482804.613222	42.261466
3504.320765	482753.159606	42.266471
3504.285492	482695.920382	42.271476
3504.694988	482640.834847	42.276480
3504.477137	482589.282466	42.281485
3504.019103	482525.135901	42.286490
3504.206241	482472.408550	42.291495
3504.335855	482434.393008	42.296500
3504.542248	482382.420247	42.301504
3504.392429	482337.020622	42.306509
3504.343889	482276.649305	42.311514
3504.036354	482222.987564	42.316519
3503.728758	482174.681480	42.321524
3504.277019	482123.008346	42.326528
3504.248561	482073.951138	42.331533
3503.996346	482022.200127	42.336538
3504.301865	481962.176718	42.341543
3504.042184	481923.614188	42.346548
3504.072905	481867.877492	42.351552
3504.293733	481814.081602	42.356557
3503.942612	481769.065351	42.361562
3503.709489	481720.139940	42.366567
3503.401929	481676.127207	42.371572
3504.131129	481632.508831	42.376576
3503.825767	481597.186426	42.381581
3503.803445	481538.475628	42.386586
3503.941693	481491.917095	42.391591
3503.815866	481449.138668	42.396596
3503.997710	481401.764620	42.401600
3503.751261	481358.549953	42.406605
3503.693365	481309.040170	42.411610
3503.926353	481271.056253	42.416615
3503.551876	481222.151285	42.421620
3503.909765	481180.408509	42.426624
3504.035375	481135.568905	42.431629
3503.875812	481084.356213	42.436634
3504.164990	481041.309975	42.441639
3503.591109	480995.972457	42.446644
3503.740292	480939.759260	42.451648
3503.832264	480908.971768	42.456653
3503.804539	480854.958620	42.461658
3503.942082	480813.299691	42.466663
3503.625217	480770.448082	42.471668
3504.021010	480725.312610	42.476672
3503.838573	480689.312127	42.481677
3503.519283	480638.223901	42.486682
3503.761091	480586.088091	42.491687
3503.399635	480551.277382	42.496692
3503.739027	480503.775051	42.501696
3503.783510	480461.523289	42.506701
3503.825853	480414.824898	42.511706
3503.839871	480368.939298	42.516711
3503.858286	480330.834908	42.521716
3503.900965	480271.250213	42.526720
3503.691808	480234.595922	42.531725
3503.579328	480198.280233	42.536730
3503.742199	480139.990199	42.541735
3504.036674	480104.672166	42.546740
3503.632537	480066.228624	42.551744
3503.577899	480016.310003	42.556749
3503.855812	479963.509582	42.561754
3504.083197	479921.025776	42.566759
3503.593075	479880.927543	42.571764
3503.737957	479832.442782	42.576768
3503.718991	479792.321540	42.581773
3503.809813	479745.512558	42.586778
3504.059442	479702.165617	42.591783
3503.562476	479669.648107	42.596788
3503.606954	479613.446480	42.601792
3503.939940	479577.009508	42.606797
3504.016222	479534.851390	42.611802
3503.963357	479488.367218	42.616807
3503.788625	479443.064190	42.621812
3503.789103	479388.485746	42.626816
3503.658846	479356.314812	42.631821
3503.479157	479310.456282	42.636826
3503.920060	479254.494908	42.641831
3503.956946	479215.222626	42.646836
3504.052889	479166.895051	42.651840
3503.581872	479131.340214	42.656845
3503.639032	479085.545250	42.661850
3503.996485	479040.309865	42.666855
3503.515862	479000.410066	42.671860
3503.664303	478947.424260	42.676864
3503.483144	478907.123867	42.681869
3503.805361	478865.178383	42.686874
3503.642935	478821.438319	42.691879
3503.960595	478784.243851	42.696884
3503.904178	478723.051548	42.701888
3504.117463	478692.190326	42.706893
3503.861425	478642.854633	42.711898
3503.842038	478587.872223	42.716903
3503.745305	478553.218070	42.721908
3503.754698	478496.512562	42.726912
3503.498534	478460.518478	42.731917
3503.773227	478415.900658	42.736922
3503.774035	478377.238382	42.741927
3503.121465	478336.605587	42.746932
3503.456976	478288.136982	42.751936
3503.654480	478260.916198	42.756941
3503.444938	478217.181802	42.761946
3503.779176	478163.406379	42.766951
3503.330519	478125.015591	42.771956
3503.457895	478079.257340	42.776960
3503.572651	478047.399405	42.781965
3503.496390	478008.444986	42.786970
3503.625656	477974.613586	42.791975
3503.634471	477922.555815	42.796980
3503.696154	477877.312611	42.801985
3503.581150	477829.468661	42.806989
3503.375430	477792.050077	42.811994
3503.780909	477741.496752	42.816999
3503.407707	477713.605729	42.822004
3503.667392	477672.829279	42.827009
3503.654227	477632.448972	42.832013
3503.627591	477598.944283	42.837018
3503.906032	477547.702534	42.842023
3503.473329	477511.430526	42.847028
3503.453943	477456.444208	42.852033
3503.649313	477418.659082	42.857037
3503.731649	477379.223570	42.862042
3503.913604	477329.006975	42.867047
3503.743298	477287.942659	42.872052
3503.645073	477232.715128	42.877057
3503.429694	477197.166724	42.882061
3503.534021	477157.373444	42.887066
3503.384954	477101.749030	42.892071
3503.638986	477076.640233	42.897076
3503.157924	477028.901389	42.902081
3503.193082	476998.317325	42.907085
3503.386976	476968.719369	42.912090
3503.256314	476926.889806	42.917095
3503.146392	476885.461254	42.922100
3503.334542	476849.899827	42.927105
3503.415129	476816.578986	42.932109
3502.884954	476772.839980	42.937114
3503.595592	476741.897594	42.942119
3503.570726	476704.852671	42.947124
3503.317788	476664.153421	42.952129
3503.391273	476624.970148	42.957133
3503.255265	476588.599328	42.962138
3503.707162	476540.309490	42.967143
3503.344524	476504.378102	42.972148
3503.584886	476460.366703	42.977153
3503.439149	476430.365699	42.982157
3503.265379	476385.761453	42.987162
3503.460900	476344.182880	42.992167
3503.393604	476312.602545	42.997172
3503.554487	476265.266981	43.002177
3503.541400	476224.731473	43.007181
3503.657827	476196.508879	43.012186
3503.371403	476152.982977	43.017191
3503.217184	476111.154949	43.022196
3503.050186	476066.093846	43.027201
3503.061375	476031.973436	43.032205
3503.100778	476005.986530	43.037210
3503.287525	475967.997141	43.042215
3503.419657	475936.283938	43.047220
3503.239657	475885.815867	43.052225
3503.276900	475865.894678	43.057229
3503.400775	475814.924176	43.062234
3503.702143	475778.028535	43.067239
3503.201207	475738.629203	43.072244
3503.469532	475703.254949	43.077249
3503.163786	475656.495678	43.082253
3503.136289	475634.309641	43.087258
3503.852333	475602.151084	43.092263
3503.195087	475570.003972	43.097268
3503.355905	475514.073089	43.102273
3503.581115	475478.553407	43.107277
3503.276756	475438.617268	43.112282
3503.814708	475394.455546	43.117287
3503.443784	475358.522882	43.122292
3503.639767	475313.403185	43.127297
3503.531080	475272.121922	43.132301
3503.206062	475222.028175	43.137306
3503.639532	475187.031480	43.142311
3503.397501	475159.418886	43.147316
3503.383814	475113.977414	43.152321
3503.180778	475071.193844	43.157325
3503.200414	475034.138143	43.162330
3503.715112	474992.860258	43.167335
3503.420980	474961.262018	43.172340
3503.217177	474932.227695	43.177345
3503.179768	474892.349761	43.182349
3503.165158	474850.496730	43.187354
3503.448857	474801.823453	43.192359
3503.197405	474773.857813	43.197364
3503.363280	474731.369785	43.202369
3503.276176	474696.655237	43.207373
3503.352161	474658.578896	43.212378
3503.423728	474626.720890	43.217383
3503.012335	474597.566617	43.222388
3503.410969	474547.610919	43.227393
3503.188469	474516.708373	43.232397
3503.252555	474479.745585	43.237402
3503.196662	474428.849227	43.242407
3503.195360	474398.771407	43.247412
3503.092080	474356.273726	43.252417
3503.226137	474331.179318	43.257421
3502.983052	474303.059906	43.262426
3503.178847	474263.548543	43.267431
3503.063469	474233.033200	43.272436
3503.081672	474199.716651	43.277441
3503.236863	474162.890618	43.282445
3502.896158	474124.978968	43.287450
3502.947580	474089.786589	43.292455
3503.183263	474061.238387	43.297460
3503.388467	474023.848179	43.302465
3503.103101	473993.914916	43.307469
3502.975924	473957.334567	43.312474
3503.292276	473920.129034	43.317479
3503.441954	473880.371150	43.322484
3502.868412	473839.613539	43.327489
3502.976570	473810.478103	43.332493
3503.176313	473777.031328	43.337498
3503.295358	473741.827671	43.342503
3503.492629	473710.706603	43.347508
3503.301969	473668.473481	43.352513
3503.260086	473630.564726	43.357517
3502.885884	473591.595408	43.362522
3503.151877	473560.008372	43.367527
3503.111031	473523.514718	43.372532
3503.159026	473482.962816	43.377537
3503.360990	473458.159816	43.382541
3502.673349	473417.014462	43.387546
3503.298386	473381.023521	43.392551
3503.028613	473349.570002	43.397556
3502.826164	473316.083755	43.402561
3503.051150	473291.479137	43.407565
3503.006524	473257.310996	43.412570
3503.549264	473221.888614	43.417575
3503.021806	473190.171555	43.422580
3503.335836	473141.033574	43.427585
3503.038117	473109.634494	43.432589
3503.034705	473082.031775	43.437594
3503.223989	473043.327344	43.442599
3502.925371	473008.490425	43.447604
3503.278181	472969.912039	43.452609
3503.424383	472935.359635	43.457613
3503.074324	472905.687208	43.462618
3503.124204	472866.599601	43.467623
3502.907070	472842.416997	43.472628
3502.818550	472800.064609	43.477633
3503.102299	472771.354993	43.482637
3502.737616	472742.139552	43.487642
3503.186349	472702.787258	43.492647
3502.923847	472669.005682	43.497652
3503.062050	472628.639839	43.502657
3503.254092	472594.888490	43.507661
3503.151288	472574.125574	43.512666
3503.445041	472524.533875	43.517671
3503.151761	472492.981241	43.522676
3503.052349	472459.325523	43.527681
3503.242684	472423.754017	43.532685
3502.812965	472386.762192	43.537690
3503.166737	472353.237964	43.542695
3503.017565	472319.640259	43.547700
3503.010594	472293.047914	43.552705
3502.961714	472259.535593	43.557709
3503.050941	472221.148128	43.562714
3503.042843	472188.084338	43.567719
3502.710817	472150.267841	43.572724
3502.891593	472119.854117	43.577729
3502.862916	472093.922086	43.582733
3502.843924	472059.090180	43.587738
3502.970155	472033.942886	43.592743
3503.035224	472001.120126	43.597748
3502.788391	471965.666210	43.602753
3502.936383	471930.150778	43.607757
3502.859091	471906.349495	43.612762
3503.217320	471871.761844	43.617767
3503.084443	471834.368658	43.622772
3502.855149	471796.990390	43.627777
3503.149907	471771.563671	43.632781
3503.023448	471741.399291	43.637786
3502.868948	471712.351533	43.642791
3502.952967	471684.378925	43.647796
3502.300253	471642.313565	43.652801
3502.399364	471611.203764	43.657805
3502.435692	471585.260810	43.662810
3503.229748	471553.233794	43.667815
3502.733688	471525.907344	43.672820
3502.484081	471493.385334	43.677825
3502.907172	471473.904313	43.682829
3502.755633	471452.894751	43.687834
3503.138211	471414.105818	43.692839
3502.685885	471387.429620	43.697844
3502.752176	471356.526685	43.702849
3502.732837	471326.749358	43.707853
3502.561647	471299.675341	43.712858
3502.923771	471267.765544	43.717863
3502.551519	471248.458582	43.722868
3502.798418	471220.156467	43.727873
3502.747934	471184.619742	43.732877
3502.677080	471167.136554	43.737882
3503.062305	471118.689272	43.742887
3502.769890	471099.369710	43.747892
3503.101216	471063.621623	43.752897
3502.962663	471032.345459	43.757901
3502.670437	471007.413392	43.762906
3502.749461	470973.726847	43.767911
3502.684049	470946.231290	43.772916
3503.014351	470910.786402	43.777921
3502.739272	470882.969430	43.782925
3502.652093	470861.494032	43.787930
3502.673845	470825.439663	43.792935
3502.352649	470797.376910	43.797940
3502.396224	470779.622689	43.802945
3502.454105	470742.854639	43.807949
3502.436248	470722.328965	43.812954
3502.512528	470688.895077	43.817959
3502.747403	470665.447916	43.822964
3502.321060	470640.030531	43.827969
3502.187541	470612.646139	43.832973
3502.406407	470596.785843	43.837978
3502.442502	470570.436814	43.842983
3502.520473	470557.177132	43.847988
3502.715640	470522.409758	43.852993
3502.620393	470503.109375	43.857997
3502.217242	470476.676857	43.863002
3502.752672	470445.395821	43.868007
3502.450185	470420.919532	43.873012
3502.454456	470384.057895	43.878017
3502.774960	470362.973480	43.883021
3502.604231	470328.869402	43.888026
3502.852143	470302.031906	43.893031
3502.775997	470280.301211	43.898036
3502.624654	470251.048115	43.903041
3502.602971	470219.853345	43.908045
3502.664649	470203.410359	43.913050
3502.808544	470169.105297	43.918055
3502.336047	470148.750783	43.923060
3502.664510	470121.344247	43.928065
3503.114187	470098.419065	43.933069
3502.788971	470078.395498	43.938074
3503.046554	470033.959502	43.943079
3502.850327	470008.100809	43.948084
3502.921310	469980.026195	43.953089
3502.302491	469943.462792	43.958093
3502.350687	469912.104869	43.963098
3503.121266	469884.275183	43.968103
3502.873730	469857.210668	43.973108
3502.565869	469831.267938	43.978113
3502.867365	469794.105900	43.983117
3502.800975	469769.440204	43.988122
3502.991805	469738.110320	43.993127
3502.836234	469712.952759	43.998132
3502.772878	469678.729494	44.003137
3502.922946	469649.529558	44.008141
3502.796035	469623.760607	44.013146
3502.948568	469591.374515	44.018151
3502.576583	469562.811893	44.023156
3502.823457	469527.579277	44.028161
3502.900517	469498.693835	44.033165
3502.466950	469481.619262	44.038170
3503.052968	469447.749567	44.043175
3502.738981	469422.717348	44.048180
3502.788429	469390.599737	44.053185
3502.792000	469359.500543	44.058189
3502.519414	469331.933393	44.063194
3502.359442	469298.128909	44.068199
3502.141549	469278.087667	44.073204
3502.091049	469257.413545	44.078209
3502.457524	469230.758126	44.083213
3502.512014	469220.838471	44.088218
3502.279551	469181.078072	44.093223
3502.590337	469164.595286	44.098228
3502.514464	469141.447154	44.103233
3502.412256	469110.768494	44.108237
3502.370204	469094.138273	44.113242
3502.872187	469061.696764	44.118247
3502.453952	469028.791572	44.123252
3502.851251	469009.412793	44.128257
3502.929411	468976.581957	44.133261
3502.637706	468952.354647	44.138266
3502.659999	468923.072175	44.143271
3502.794324	468899.183038	44.148276
3502.586028	468865.182915	44.153281
3502.839813	468834.448345	44.158285
3502.639093	468814.960123	44.163290
3502.525466	468770.477357	44.168295
3502.758274	468755.523363	44.173300
3502.684741	468732.930553	44.178305
3502.644692	468702.696583	44.183309
3502.414521	468684.527584	44.188314
3502.642617	468653.695539	44.193319
3502.806937	468625.654669	44.198324
3502.671365	468594.525119	44.203329
3502.427044	468571.503541	44.208333
3502.548603	468539.120209	44.213338
3502.739586	468514.463159	44.218343
3502.508699	468486.382413	44.223348
3502.546464	468453.202838	44.228353
3502.628096	468424.769937	44.233357
3502.703412	468402.861492	44.238362
3502.747177	468372.512737	44.243367
3502.798048	468341.909970	44.248372
3502.535466	468310.041099	44.253377
3502.940682	468288.789150	44.258381
3502.483386	468255.483936	44.263386
3502.837943	468230.851580	44.268391
3502.835831	468198.031693	44.273396
3502.671846	468173.125950	44.278401
3502.783618	468142.867334	44.283405
3502.659187	468119.118480	44.288410
3502.476176	468082.533706	44.293415
3502.723356	468067.627427	44.298420
3502.601612	468032.398424	44.303425
3502.644923	468006.448751	44.308429
3502.587204	467991.488709	44.313434
3502.538683	467957.259574	44.318439
3502.301659	467942.327389	44.323444
3502.469096	467908.924263	44.328449
3502.487198	467888.895185	44.333453
3502.136733	467861.792847	44.338458
3502.643805	467830.511289	44.343463
3502.590695	467821.163830	44.348468
3502.441164	467790.034942	44.353473
3502.531812	467759.273197	44.358477
3502.357206	467738.161345	44.363482
3502.510215	467710.929842	44.368487
3502.365552	467685.767500	44.373492
3502.427401	467668.108238	44.378497
3502.497640	467636.287426	44.383501
3502.590053	467618.572783	44.388506
3502.414846	467589.065829	44.393511
3502.504596	467561.843926	44.398516
3502.423515	467538.643794	44.403521
3502.807485	467507.532504	44.408525
3502.251786	467493.054085	44.413530
3502.548913	467451.538227	44.418535
3502.529017	467428.985868	44.423540
3502.234514	467407.740534	44.428545
3502.363086	467379.652552	44.433549
3502.469668	467369.369674	44.438554
3502.572905	467333.497303	44.443559
3502.879429	467313.321504	44.448564
3502.790647	467289.818785	44.453569
3502.675682	467261.970795	44.458573
3502.631968	467235.578302	44.463578
3502.904020	467197.100120	44.468583
3502.920043	467173.378633	44.473588
3502.611326	467152.640922	44.478593
3502.656034	467117.788669	44.483597
3502.567220	467089.986896	44.488602
3502.738818	467060.475612	44.493607
3502.762649	467027.244786	44.498612
3502.467855	466997.856541	44.503617
3502.676188	466973.396805	44.508621
3502.535162	466954.048831	44.513626
3502.725804	466921.348155	44.518631
3502.889398	466895.630906	44.523636
3502.925918	466867.556387	44.528641
3502.834373	466834.747728	44.533645
3502.671338	466799.219092	44.538650
3502.868960	466766.517026	44.543655
3502.506856	466747.860689	44.548660
3502.629851	466722.200066	44.553665
3502.687237	466683.804681	44.558669
3502.437740	466672.008955	44.563674
3502.485123	466634.424216	44.568679
3502.477499	466612.627473	44.573684
3502.486769	466591.940731	44.578689
3502.529872	466565.533669	44.583693
3502.360565	466542.548182	44.588698
3502.315726	466520.150202	44.593703
3502.556766	466500.944551	44.598708
3502.581988	466471.910186	44.603713
3502.370914	466443.468877	44.608717
3502.322326	466427.696794	44.613722
3502.416016	466398.702224	44.618727
3502.757062	466361.829816	44.623732
3502.001456	466344.094054	44.628737
3502.554170	466307.896655	44.633741
3502.241504	466301.168123	44.638746
3502.263749	466271.982146	44.643751
3502.692761	466255.478088	44.648756
3502.443283	466232.302344	44.653761
3502.492829	466206.096017	44.658765
3502.166165	466176.761862	44.663770
3502.372202	466150.783980	44.668775
3502.678448	466131.163145	44.673780
3502.747379	466113.298829	44.678785
3502.940974	466070.328922	44.683789
3502.816009	466053.759141	44.688794
3502.644363	466005.788198	44.693799
3502.767979	465991.101606	44.698804
3502.406135	465969.308568	44.703809
3502.896402	465931.501601	44.708813
3502.498708	465913.355643	44.713818
3502.480773	465888.626067	44.718823
3502.528738	465867.325478	44.723828
3502.357763	465844.187558	44.728833
3502.462935	465809.677213	44.733837
3502.386022	465791.228316	44.738842
3502.847894	465769.205682	44.743847
3502.686504	465747.836364	44.748852
3502.657592	465713.650155	44.753857
3502.708030	465679.552684	44.758861
3502.267805	465663.587935	44.763866
3502.484395	465631.335906	44.768871
3502.450558	465600.893029	44.773876
3502.003796	465582.299141	44.778881
3502.439295	465558.054881	44.783885
3502.627908	465539.008024	44.788890
3502.640916	465509.973893	44.793895
3502.800755	465490.021041	44.798900
3503.044565	465449.570668	44.803905
3502.994472	465428.082465	44.808909
3502.491830	465386.888256	44.813914
3502.426817	465367.324301	44.818919
3502.785876	465333.683895	44.823924
3502.167169	465317.847748	44.828929
3502.717678	465295.658963	44.833933
3503.191683	465265.945722	44.838938
3502.894047	465216.070109	44.843943
3502.505358	465190.385607	44.848948
3502.273787	465173.275167	44.853953
3502.341537	465141.197099	44.858957
3502.079093	465127.379104	44.863962
3502.306621	465106.403667	44.868967
3502.107675	465093.840260	44.873972
3502.523385	465062.061954	44.878977
3502.747095	465041.744571	44.883981
3502.130754	465012.453454	44.888986
3502.410185	464993.240106	44.893991
3502.839887	464962.268717	44.898996
3502.696252	464929.818497	44.904001
3502.674757	464906.099637	44.909005
3502.521391	464887.004097	44.914010
3502.778732	464861.370304	44.919015
3502.716931	464831.891417	44.924020
3502.739259	464796.430851	44.929025
3502.428561	464774.425977	44.934029
3502.385082	464748.434175	44.939034
3502.341946	464720.014389	44.944039
3502.414842	464703.817133	44.949044
3502.464319	464675.129954	44.954049
3502.519500	464647.251139	44.959053
3502.302832	464618.655861	44.964058
3502.075606	464598.964511	44.969063
3502.234907	464575.722866	44.974068
3502.260687	464552.552549	44.979073
3502.228767	464527.873729	44.984077
3502.249590	464521.598400	44.989082
3502.292922	464491.242670	44.994087
3502.554852	464479.112904	44.999092
3502.436931	464457.178780	45.004097
3502.597409	464422.859312	45.009101
3502.480917	464399.812087	45.014106
3502.429422	464382.875150	45.019111
3502.789726	464358.084465	45.024116
3502.504440	464322.771935	45.029121
3502.319348	464299.077678	45.034125
3502.458593	464288.029095	45.039130
3502.044965	464255.518425	45.044135
3502.238996	464229.994690	45.049140
3501.863537	464216.244114	45.054145
3502.081537	464197.747577	45.059149
3502.157955	464175.378184	45.064154
3502.258443	464159.833687	45.069159
3502.292917	464125.381474	45.074164
3502.158703	464124.694236	45.079169
3502.244030	464085.378074	45.084173
3502.173162	464075.778372	45.089178
3502.003979	464048.186396	45.094183
3502.422576	464035.930767	45.099188
3502.348649	464011.510645	45.104193
3502.295751	463981.674804	45.109197
3502.124165	463962.378718	45.114202
3502.429632	463941.693206	45.119207
3502.118758	463923.531585	45.124212
3501.962669	463903.777770	45.129217
3502.050145	463888.083298	45.134221
3501.506429	463868.845012	45.139226
3501.899009	463850.169178	45.144231
3502.270054	463837.920806	45.149236
3502.481840	463811.786672	45.154241
3502.034972	463799.513798	45.159245
3502.009641	463777.362047	45.164250
3502.283717	463755.770683	45.169255
3502.419339	463740.625005	45.174260
3502.018869	463717.570456	45.179265
3502.162547	463684.567289	45.184269
3502.142969	463673.593605	45.189274
3502.155194	463653.105125	45.194279
3502.344313	463629.554035	45.199284
3502.444137	463617.954721	45.204289
3502.570271	463586.016364	45.209293
3502.513009	463570.141783	45.214298
3502.524584	463537.867070	45.219303
3502.464371	463518.300223	45.224308
3501.979424	463495.814948	45.229313
3502.015169	463463.182239	45.234317
3502.674760	463450.534593	45.239322
3502.639964	463422.010155	45.244327
3502.775998	463403.424336	45.249332
3502.722172	463369.338419	45.254337
3502.669584	463343.244702	45.259341
3502.620429	463323.372398	45.264346
3502.464499	463283.231966	45.269351
3502.724855	463266.397138	45.274356
3502.143368	463244.179478	45.279361
3502.565046	463214.420192	45.284365
3502.504548	463194.549501	45.289370
3502.218252	463164.748540	45.294375
3502.371662	463132.349813	45.299380
3502.078500	463104.067388	45.304385
3502.353529	463093.654514	45.309389
3502.361424	463066.994515	45.314394
3502.199695	463051.540392	45.319399
3502.582862	463026.390101	45.324404
3502.180841	463019.522395	45.329409
3502.274471	462981.922308	45.334413
3502.199873	462978.038811	45.339418
3502.398705	462945.531486	45.344423
3502.138060	462917.648381	45.349428
3502.001051	462910.334700	45.354433
3502.318520	462881.349845	45.359437
3502.198280	462868.418427	45.364442
3502.263419	462844.177327	45.369447
3502.468149	462818.194520	45.374452
3501.986169	462794.139661	45.379457
3502.117303	462779.246759	45.384461
3502.087590	462761.495419	45.389466
3502.064339	462739.544335	45.394471
3502.367000	462714.001414	45.399476
3502.170162	462698.097149	45.404481
3502.576950	462667.580416	45.409485
3502.181183	462659.548085	45.414490
3502.200592	462624.690468	45.419495
3502.534961	462604.656466	45.424500
3501.909944	462584.872908	45.429505
3502.451896	462561.467781	45.434509
3502.165877	462545.071374	45.439514
3502.265689	462528.260799	45.444519
3502.212710	462504.695235	45.449524
3502.047410	462481.551818	45.454529
3502.393533	462454.585287	45.459533
3502.367613	462439.716527	45.464538
3502.421258	462419.270701	45.469543
3502.491242	462390.576461	45.474548
3502.360582	462374.054538	45.479553
3502.430002	462356.084997	45.484557
3502.328649	462328.934959	45.489562
3502.046533	462302.116536	45.494567
3502.518260	462280.441954	45.499572
3501.958258	462269.349104	45.504577
3502.387738	462243.178682	45.509581
3502.517468	462225.857268	45.514586
3502.226451	462192.412961	45.519591
3502.506230	462168.137497	45.524596
3502.210697	462152.450434	45.529601
3502.289672	462121.477849	45.534605
3502.078165	462110.482431	45.539610
3501.981037	462078.373628	45.544615
3502.273212	462072.055167	45.549620
3502.379835	462042.494627	45.554625
3502.367429	462018.922077	45.559629
3502.300995	461997.836771	45.564634
3502.281759	461984.433660	45.569639
3502.392877	461958.970004	45.574644
3502.044569	461948.501662	45.579649
3502.275469	461914.672057	45.584653
3502.417144	461888.292929	45.589658
3502.375376	461864.117660	45.594663
3502.447230	461845.641305	45.599668
3502.341313	461811.914499	45.604673
3502.630411	461798.665620	45.609677
3502.626269	461768.160636	45.614682
3502.410535	461736.828494	45.619687
3502.589993	461722.129508	45.624692
3502.334571	461699.504952	45.629697
3502.694927	461664.137004	45.634701
3502.398640	461657.808782	45.639706
3502.328680	461631.563372	45.644711
3502.558013	461597.379250	45.649716
3502.085776	461586.120524	45.654721
3502.420411	461553.336459	45.659725
3502.125338	461548.070409	45.664730
3502.020472	461513.988716	45.669735
3502.676957	461490.969027	45.674740
3502.240154	461468.170027	45.679745
3502.386760	461445.887300	45.684749
3502.504062	461420.270105	45.689754
3502.188147	461393.000193	45.694759
3502.329860	461371.780542	45.699764
3502.130627	461354.560026	45.704769
3502.179614	461325.108395	45.709773
3502.385178	461307.926024	45.714778
3502.414897	461296.943134	45.719783
3502.358986	461268.772511	45.724788
3502.391690	461251.819348	45.729793
3502.421040	461218.019728	45.734797
3502.255102	461202.261031	45.739802
3502.262548	461184.350491	45.744807
3502.333834	461154.793914	45.749812
3502.260643	461132.393208	45.754817
3501.799791	461098.366082	45.759821
3501.639204	461034.392291	45.764826
3501.758490	460931.519829	45.769831
3502.140647	460766.174397	45.774836
3501.556991	460558.985154	45.779841
3501.357655	460305.541162	45.784845
3500.714380	460010.826395	45.789850
3500.163247	459656.591319	45.794855
3499.902072	459258.992623	45.799860
3499.524429	458836.963824	45.804865
3498.921988	458327.118324	45.809869
3497.848374	457812.169783	45.814874
3497.251534	457249.261264	45.819879
3496.284943	456626.728944	45.824884
3495.446958	455967.717501	45.829889
3494.298613	455270.772930	45.834893
3493.188264	454532.749309	45.839898
3492.001048	453752.191663	45.844903
3490.926665	452930.937727	45.849908
3489.431332	452069.621848	45.854913
3488.245305	451168.985273	45.859917
3486.883061	450243.069809	45.864922
3485.356643	449258.203629	45.869927
3484.078379	448240.285740	45.874932
3482.641749	447182.336287	45.879937
3480.775446	446092.239193	45.884941
3478.594646	444974.325959	45.889946
3476.953957	443819.546048	45.894951
3475.435588	442626.033483	45.899956
3473.661201	441415.112104	45.904961
3471.562473	440158.577035	45.909965
3469.629466	438878.580654	45.914970
3467.918568	437554.796146	45.919975
3466.028340	436209.416517	45.924980
3463.855230	434828.875697	45.929985
3461.644905	433412.064520	45.934989
3459.353633	431972.309454	45.939994
3456.822961	430516.016061	45.944999
3454.646851	429028.391795	45.950004
3452.398943	427510.003644	45.955009
3449.986084	425968.361778	45.960013
3447.726067	424400.218752	45.965018
3444.959195	422816.723730	45.970023
3442.505546	421208.671292	45.975028
3440.058264	419574.025666	45.980033
3437.430754	417912.709315	45.985037
3434.841890	416246.590443	45.990042
3432.460716	414544.554100	45.995047
3429.716564	412815.963479	46.000052
3427.046872	411086.817455	46.005057
3424.137587	409323.330634	46.010061
3421.685562	407553.239518	46.015066
3418.724809	405749.043176	46.020071
3415.988178	403928.379828	46.025076
3412.715999	402097.657524	46.030081
3409.786980	400250.445871	46.035085
3406.833553	398392.889987	46.040090
3403.688979	396528.872445	46.045095
3400.854224	394632.173877	46.050100
3397.465562	392735.208709	46.055105
3394.766048	390824.636189	46.060109
3391.648027	388901.109608	46.065114
3388.237692	386961.637686	46.070119
3385.122407	385009.402451	46.075124
3381.883206	383041.852662	46.080129
3378.837447	381065.946032	46.085133
3375.239458	379075.246524	46.090138
3372.158829	377084.824914	46.095143
3368.879582	375083.796669	46.100148
3365.566643	373071.856355	46.105153
3362.372026	371048.344871	46.110157
3358.962977	369011.890864	46.115162
3355.108592	366976.274712	46.120167
3351.991864	364932.599414	46.125172
3348.787978	362890.802219	46.130177
3345.132061	360828.401786	46.135181
3341.759418	358767.950854	46.140186
3338.407540	356697.522089	46.145191
3335.057018	354605.375904	46.150196
3331.199327	352522.803922	46.155201
3328.001091	350426.267141	46.160205
3324.729381	348327.802263	46.165210
3320.946995	346225.063983	46.170215
3317.457405	344120.852686	46.175220
3313.778632	342005.634028	46.180225
3310.213337	339887.625509	46.185229
3306.774186	337765.886106	46.190234
3302.858856	335644.198827	46.195239
3299.295806	333516.180620	46.200244
3295.337336	331403.644634	46.205249
3291.741504	329283.204138	46.210253
3288.231816	327152.741087	46.215258
3284.522240	325023.162973	46.220263
3281.054773	322889.671753	46.225268
3276.752850	320748.875022	46.230273
3273.878864	318617.264778	46.235277
3270.147490	316491.994551	46.240282
3266.078664	314354.412108	46.245287
3262.384998	312205.552287	46.250292
3258.840310	310076.063865	46.255297
3255.097866	307938.038368	46.260301
3251.323051	305788.295653	46.265306
3247.319264	303645.445906	46.270311
3243.430884	301500.250921	46.275316
3239.579817	299368.632633	46.280321
3235.774991	297236.212582	46.285325
3231.997521	295111.141316	46.290330
3228.212866	292974.514304	46.295335
3224.669665	290849.077040	46.300340
3220.427712	288718.101535	46.305345
3216.682258	286600.394943	46.310349
3213.381894	284468.932117	46.315354
3209.320390	282352.263315	46.320359
3205.113556	280238.202928	46.325364
3200.983697	278121.983240	46.330369
3197.196387	276019.376489	46.335373
3193.439036	273911.058205	46.340378
3189.362529	271813.355102	46.345383
3185.991408	269715.034343	46.350388
3181.775661	267622.807122	46.355393
3177.830920	265531.333245	46.360397
3173.486669	263451.032529	46.365402
3169.760747	261377.802352	46.370407
3166.276353	259303.249361	46.375412
3162.436960	257234.446183	46.380417
3158.510657	255163.790034	46.385421
3154.581096	253092.033986	46.390426
3150.503580	251047.369282	46.395431
3146.762314	248981.692229	46.400436
3142.449908	246933.627086	46.405441
3138.346995	244891.696361	46.410445
3134.445612	242857.864612	46.415450
3130.956322	240820.156685	46.420455
3126.763156	238800.956790	46.425460
3122.320263	236786.112463	46.430465
3118.954788	234769.510491	46.435469
3114.683515	232757.497610	46.440474
3110.788547	230772.212656	46.445479
3106.974767	228783.191788	46.450484
3103.167882	226796.255417	46.455489
3099.109471	224817.303568	46.460493
3095.098852	222845.705769	46.465498
3090.805257	220891.066220	46.470503
3086.977642	218933.404341	46.475508
3082.406939	216994.711461	46.480513
3078.619452	215058.196972	46.485517
3075.067974	213121.579194	46.490522
3070.649380	211204.896928	46.495527
3066.825188	209298.908329	46.500532
3062.408077	207401.507500	46.505537
3058.420358	205507.112182	46.510541
3054.079510	203618.672622	46.515546
3049.802835	201746.592406	46.520551
3046.060033	199883.414102	46.525556
3041.853876	198042.180306	46.530561
3037.646725	196200.562217	46.535565
3033.562888	194379.678811	46.540570
3029.369958	192569.253305	46.545575
3025.061276	190753.906730	46.550580
3020.626800	188968.529174	46.555585
3016.498817	187183.794718	46.560589
3011.888153	185425.036883	46.565594
3008.001154	183671.238772	46.570599
3003.698391	181934.877419	46.575604
2999.192105	180228.244027	46.580609
2995.084074	178522.217692	46.585613
2990.650291	176826.791364	46.590618
2986.293980	175160.222107	46.595623
2982.212018	173508.004332	46.600628
2977.815347	171864.348652	46.605633
2973.257941	170234.489028	46.610637
2969.010771	168630.687162	46.615642
2964.831425	167031.505966	46.620647
2960.049094	165472.156730	46.625652
2954.945173	163922.223502	46.630657
2950.785820	162389.031919	46.635661
2946.142247	160876.520588	46.640666
2941.162275	159394.377099	46.645671
2936.580604	157928.192925	46.650676
2931.702223	156504.331752	46.655681
2926.829545	155094.567166	46.660685
2921.536767	153717.431165	46.665690
2916.516356	152376.759383	46.670695
2911.534431	151061.145666	46.675700
2905.604063	149801.054594	46.680705
2900.293600	148571.882603	46.685709
2895.118614	147283.356281	46.690714
2889.318153	146116.670348	46.695719
2883.729148	144985.631759	46.700724
2878.318812	143907.955524	46.705729
2873.359683	142847.994844	46.710733
2868.143296	141833.367437	46.715738
2863.552107	140853.525758	46.720743
2858.530401	139888.237170	46.725748
2853.498933	138970.565677	46.730753
2848.873170	138070.177094	46.735757
2844.982939	137204.512441	46.740762
2840.271711	136357.273452	46.745767
2836.299014	135525.659479	46.750772
2832.086298	134724.884470	46.755777
2828.359679	133923.857324	46.760781
2824.239973	133144.290080	46.765786
2819.916573	132386.393947	46.770791
2816.037602	131628.963373	46.775796
2811.925913	130895.624016	46.780801
2808.111481	130172.846928	46.785805
2804.329008	129469.742363	46.790810
2800.310641	128765.808527	46.795815
2797.101159	128083.307712	46.800820
2793.490231	127386.049667	46.805825
2789.672937	126702.788479	46.810829
2786.269800	126034.304582	46.815834
2782.585511	125368.622647	46.820839
2779.081877	124702.402064	46.825844
2775.217979	124052.121126	46.830849
2771.948267	123397.993703	46.835853
2768.432727	122754.255017	46.840858
2765.032381	122109.656800	46.845863
2761.593405	121457.292022	46.850868
2758.031977	120811.888165	46.855873
2754.004933	120170.776885	46.860877
2750.552118	119545.635685	46.865882
2746.921543	118917.315015	46.870887
2743.773595	118287.403622	46.875892
2739.587349	117667.315966	46.880897
2735.886064	117046.183920	46.885901
2732.173813	116432.362811	46.890906
2728.107105	115833.471625	46.895911
2724.202214	115238.633905	46.900916
2720.193846	114643.287863	46.905921
2716.621174	114052.372121	46.910925
2712.504792	113478.791943	46.915930
2708.669485	112910.479126	46.920935
2705.207964	112353.954278	46.925940
2701.272509	111797.740677	46.930945
2697.563715	111245.263843	46.935949
2694.041251	110698.983698	46.940954
2689.832250	110168.304111	46.945959
2686.310656	109635.338837	46.950964
2682.449932	109107.634196	46.955969
2678.822130	108576.303487	46.960973
2675.194349	108052.888350	46.965978
2671.563629	107528.540863	46.970983
2668.495761	107010.279361	46.975988
2664.572601	106507.426333	46.980993
2661.491629	105990.415442	46.985997
2657.726535	105484.362196	46.991002
2654.346655	104975.726939	46.996007
2651.062686	104456.889757	47.001012
2647.284934	103948.776881	47.006017
2643.523906	103442.969869	47.011021
2640.423159	102929.733560	47.016026
2636.844842	102435.645736	47.021031
2633.771516	101925.967077	47.026036
2630.261725	101424.460791	47.031041
2626.634110	100908.656123	47.036045
2623.485205	100395.047517	47.041050
2619.813477	99881.769898	47.046055
2616.417781	99370.529153	47.051060
2613.087275	98865.348784	47.056065
2609.915093	98344.049182	47.061069
2606.325563	97826.661169	47.066074
2602.749788	97321.835733	47.071079
2599.552455	96792.152302	47.076084
2596.152675	96274.188275	47.081089
2592.432509	95753.804569	47.086093
2589.142997	95229.994907	47.091098
2585.694228	94711.416310	47.096103
2582.559071	94184.715602	47.101108
2578.839362	93667.429305	47.106113
2575.351028	93146.761034	47.111117
2572.172580	92606.294208	47.116122
2568.600749	92087.067450	47.121127
2565.548393	91546.383807	47.126132
2561.556896	91014.331011	47.131137
2558.382277	90484.040972	47.136141
2555.068198	89946.336436	47.141146
2551.094825	89414.067785	47.146151
2547.988487	88878.637157	47.151156
2544.545599	88337.665636	47.156161
2540.988002	87791.894039	47.161165
2537.759245	87244.734705	47.166170
2534.077100	86710.944899	47.171175
2530.626964	86173.266697	47.176180
2527.081234	85624.256039	47.181185
2523.710803	85079.306379	47.186189
2520.291302	84531.948298	47.191194
2516.755616	83990.144600	47.196199
2513.100529	83439.515805	47.201204
2509.572945	82891.761308	47.206209
2506.146260	82343.239528	47.211213
2503.038895	81793.154428	47.216218
2499.698804	81247.409533	47.221223
2496.505374	80688.315653	47.226228
2492.756314	80138.997908	47.231233
2489.256196	79573.966301	47.236237
2486.370036	79015.899660	47.241242
2482.387657	78449.022813	47.246247
2478.927439	77882.241483	47.251252
2475.654304	77329.705004	47.256257
2471.932345	76756.091547	47.261261
2468.727380	76187.197475	47.266266
2464.913091	75614.155883	47.271271
2461.746242	75048.226067	47.276276
2458.175529	74481.977340	47.281281
2454.329257	73923.885128	47.286285
2450.631391	73349.794362	47.291290
2447.167934	72786.345823	47.296295
2443.947252	72206.808859	47.301300
2440.149456	71639.106865	47.306305
2436.648802	71075.408585	47.311309
2433.369432	70501.282884	47.316314
2429.865995	69936.904894	47.321319
2426.208527	69364.970706	47.326324
2422.614148	68793.648734	47.331329
2419.443701	68230.309860	47.336333
2415.999588	67652.337212	47.341338
2412.458173	67088.681204	47.346343
2409.500261	66509.160677	47.351348
2405.498350	65929.568273	47.356353
2402.261896	65358.330784	47.361357
2398.786147	64772.722994	47.366362
2395.239698	64194.648197	47.371367
2391.671964	63624.586930	47.376372
2388.180939	63042.614176	47.381377
2384.597916	62463.512551	47.386381
2381.386081	61873.267009	47.391386
2377.553039	61297.544329	47.396391
2374.402499	60706.803115	47.401396
2370.676376	60131.732046	47.406401
2367.287085	59551.317085	47.411405
2364.081869	58965.791832	47.416410
2360.430629	58385.756383	47.421415
2356.868387	57793.062247	47.426420
2353.399227	57202.075024	47.431425
2349.753883	56622.379308	47.436429
2346.500629	56026.463798	47.441434
2343.093761	55437.883382	47.446439
2339.496621	54835.459149	47.451444
2336.169046	54253.728741	47.456449
2332.175370	53676.024323	47.461453
2329.445651	53077.132479	47.466458
2325.760391	52481.988895	47.471463
2322.137024	51892.388856	47.476468
2318.750904	51310.042820	47.481473
2315.063754	50698.737507	47.486477
2311.785758	50094.171870	47.491482
2308.378264	49501.211880	47.496487
2305.096583	48902.526391	47.501492
2301.378516	48297.695984	47.506497
2297.804210	47707.167931	47.511501
2294.640386	47096.371989	47.516506
2291.131002	46501.095806	47.521511
2287.519957	45893.433525	47.526516
2283.970499	45290.597866	47.531521
2280.311482	44683.381686	47.536525
2277.128725	44077.699609	47.541530
2273.527558	43470.342587	47.546535
2270.052572	42856.926779	47.551540
2266.750092	42249.664554	47.556545
2263.059669	41641.819999	47.561549
2259.772559	41031.811745	47.566554
2255.987140	40422.703278	47.571559
2252.542080	39813.812466	47.576564
2249.046116	39199.830194	47.581569
2245.369530	38586.698599	47.586573
2242.547901	37971.511409	47.591578
2238.805653	37368.644295	47.596583
2235.408467	36752.193230	47.601588
2231.658671	36137.418626	47.606593
2227.876288	35520.378460	47.611597
2224.719961	34899.664693	47.616602
2221.251854	34302.971279	47.621607
2217.513790	33692.183021	47.626612
2213.883799	33066.431077	47.631617
2210.379192	32464.737584	47.636621
2207.131795	31827.060274	47.641626
2203.305014	31230.960123	47.646631
2199.666405	30609.586516	47.651636
2196.611830	29995.612367	47.656641
2193.359623	29384.519943	47.661645
2189.762557	28764.507242	47.666650
2186.280005	28153.867520	47.671655
2182.070031	27540.102271	47.676660
2178.662481	26922.270421	47.681665
2174.982970	26309.194801	47.686669
2171.975837	25706.012283	47.691674
2168.469925	25089.937053	47.696679
2165.058602	24475.405527	47.701684
2161.355563	23861.432399	47.706689
2157.821677	23247.578515	47.711693
2154.193587	22629.532757	47.716698
2150.742709	22020.594448	47.721703
2146.998932	21406.393038	47.726708
2143.263097	20795.953149	47.731713
2139.958497	20190.247426	47.736717
2136.416815	19579.403395	47.741722
2132.414257	18975.794730	47.746727
2129.402053	18369.472835	47.751732
2125.601841	17766.826542	47.756737
2122.404338	17170.603095	47.761741
2118.684599	16559.302169	47.766746
2114.871395	15961.872451	47.771751
2110.909759	15351.850781	47.776756
2107.515763	14751.192377	47.781761
2103.670836	14161.818459	47.786765
2100.285230	13574.531534	47.791770
2095.791793	12998.221512	47.796775
2091.867075	12427.336418	47.801780
2087.728523	11876.423884	47.806785
2083.072036	11329.805733	47.811789
2078.342735	10803.053408	47.816794
2073.728309	10302.660114	47.821799
2069.729800	9789.374026	47.826804
2065.861511	9300.688903	47.831809
2061.834103	8826.490648	47.836813
2058.106288	8351.561557	47.841818
2053.908444	7893.024230	47.846823
2050.126691	7435.813470	47.851828
2046.135700	6995.512440	47.856833
2042.744774	6560.815781	47.861837
2038.506707	6129.299435	47.866842
2034.767061	5716.621562	47.871847
2031.410122	5296.171769	47.876852
2027.795082	4885.180038	47.881857
2023.831736	4475.802388	47.886861
2020.444977	4084.653500	47.891866
2016.466603	3694.817064	47.896871
2013.096184	3313.235438	47.901876
2008.652963	2942.777001	47.906881
2003.941175	2605.449157	47.911885
1999.365253	2273.165881	47.916890
1994.553404	1955.075043	47.921895
1990.193511	1655.096596	47.926900
1985.687329	1379.581007	47.931905
1981.301040	1116.342715	47.936909
1977.230279	856.637506	47.941914
1972.833058	623.860209	47.946919
1968.359740	400.241073	47.951924
1963.940224	210.715021	47.956929
1957.010714	91.300137	47.961933
1946.399388	107.669244	47.966938
1939.255508	112.277021	47.971943
1934.594253	106.795313	47.976948
1931.962502	105.888839	47.981953
1930.001071	114.676053	47.986957
1928.249937	97.469131	47.991962
1925.963291	113.431631	47.996967
1923.317238	101.109555	48.001972
1919.949302	114.060815	48.006977
1916.696478	110.606142	48.011981
1914.150319	103.355765	48.016986
1910.345948	109.130055	48.021991
1906.935799	103.532728	48.026996
1903.415470	98.654895	48.032001
1900.289182	103.055002	48.037005
1897.571891	105.385664	48.042010
1894.357928	114.446908	48.047015
1890.362445	106.074360	48.052020
1887.070935	101.322265	48.057025
1883.463662	110.093549	48.062029
1880.484543	106.659556	48.067034
1877.086795	105.780556	48.072039
1873.495428	111.632426	48.077044
1870.323298	103.508221	48.082049
1867.025607	109.586463	48.087053
1863.576174	104.390719	48.092058
1860.371581	101.377793	48.097063
1856.418551	104.546180	48.102068
1853.361734	101.152757	48.107073
1850.214089	109.542462	48.112077
1846.536062	99.782268	48.117082
1842.897226	106.046480	48.122087
1839.920443	104.719158	48.127092
1836.516547	107.511019	48.132097
1832.991117	115.639991	48.137101
1828.890045	106.742892	48.142106
1825.777884	111.495141	48.147111
1822.558001	107.358317	48.152116
1819.179232	104.135226	48.157121
1815.236980	104.173032	48.162125
1811.907836	94.902706	48.167130
1808.411172	99.082054	48.172135
1805.510703	101.770254	48.177140
1802.164933	102.714958	48.182145
1797.989155	106.949385	48.187149
1794.930240	97.792023	48.192154
1791.284567	100.937886	48.197159
1787.908859	105.579295	48.202164
1784.572957	105.513241	48.207169
1780.799006	100.557840	48.212173
1777.415511	104.251349	48.217178
1774.137359	115.258771	48.222183
1770.215519	106.438191	48.227188
1767.032242	96.085326	48.232193
1763.608713	100.319732	48.237197
1760.413145	101.785219	48.242202
1756.474834	100.487334	48.247207
1752.982680	100.100759	48.252212
1749.768823	99.566468	48.257217
1745.945975	97.276193	48.262221
1743.155067	104.759339	48.267226
1739.439365	104.110169	48.272231
1735.471751	103.430606	48.277236
1732.239504	106.502638	48.282241
1728.695363	115.384321	48.287245
1725.385063	99.293287	48.292250
1721.935954	102.465509	48.297255
1718.444513	100.085693	48.302260
1715.338497	105.355834	48.307265
1711.339604	111.106626	48.312269
1707.471696	97.494146	48.317274
1704.425824	102.947912	48.322279
1700.777069	106.356849	48.327284
1697.986874	98.932516	48.332289
1694.443050	100.569266	48.337293
1690.407186	104.146020	48.342298
1686.920067	103.258802	48.347303
1683.626824	104.084609	48.352308
1680.071286	101.553424	48.357313
1676.492628	104.764794	48.362317
1672.919404	95.937433	48.367322
1669.752132	107.550841	48.372327
1666.125771	100.661608	48.377332
1662.851112	94.363033	48.382337
1659.112279	96.621750	48.387341
1655.885757	88.031494	48.392346
1651.705002	101.618603	48.397351
1648.105479	96.990407	48.402356
1645.162244	95.496531	48.407361
1641.873655	98.713375	48.412365
1638.225231	96.750301	48.417370
1634.875512	98.454919	48.422375
1631.453576	102.999127	48.427380
1627.982666	95.440312	48.432385
1624.159901	95.317174	48.437389
1620.838614	99.364834	48.442394
1616.988427	90.416080	48.447399
1613.769144	92.423096	48.452404
1610.404442	92.054661	48.457409
1606.553611	99.038398	48.462413
1603.451204	94.829537	48.467418
1599.617136	103.101456	48.472423
1595.931310	100.116004	48.477428
1592.915560	96.121443	48.482433
1589.045686	96.489687	48.487437
1585.963411	96.599307	48.492442
1582.143020	97.171818	48.497447
1578.874605	88.822208	48.502452
1575.043486	92.541105	48.507457
1572.193326	100.903489	48.512461
1569.114051	96.380989	48.517466
1564.755729	99.783317	48.522471
1561.217223	90.599403	48.527476
1557.648182	92.942430	48.532481
1553.931287	99.614263	48.537485
1551.152340	98.711746	48.542490
1547.520249	88.017500	48.547495
1543.788363	94.375295	48.552500
1540.424107	93.241183	48.557505
1536.715050	99.971907	48.562509
1533.168564	90.871497	48.567514
1529.934236	94.064083	48.572519
1526.541710	89.470125	48.577524
1523.539815	94.771520	48.582529
1519.100529	91.906516	48.587533
1515.689216	88.542998	48.592538
1512.098161	97.634455	48.597543
1508.493507	98.644786	48.602548
1505.256969	93.213481	48.607553
1501.889633	96.477390	48.612557
1498.831809	78.790592	48.617562
1494.655148	97.885050	48.622567
1491.146524	83.590296	48.627572
1488.148275	81.339386	48.632577
1484.384198	90.770976	48.637581
1481.360511	96.420608	48.642586
1477.783750	91.073899	48.647591
1473.981273	94.801000	48.652596
1470.211814	99.111410	48.657601
1466.768946	100.479370	48.662605
1463.458465	87.555296	48.667610
1459.800550	90.174750	48.672615
1456.675312	86.845805	48.677620
1452.893629	88.614508	48.682625
1449.015725	89.591445	48.687629
1445.719045	91.509281	48.692634
1442.156500	93.503299	48.697639
1438.834884	93.719786	48.702644
1435.670141	91.918729	48.707649
1432.315127	96.990358	48.712653
1428.615916	85.341657	48.717658
1425.180523	98.189500	48.722663
1421.301819	96.635609	48.727668
1417.580739	91.143697	48.732673
1414.187663	97.407636	48.737677
1411.175857	93.017021	48.742682
1407.591678	89.421000	48.747687
1403.851487	93.736349	48.752692
1400.763247	88.028883	48.757697
1396.900186	101.857602	48.762701
1393.516832	95.835406	48.767706
1389.765176	100.725171	48.772711
1386.277380	101.878672	48.777716
1382.844561	98.483716	48.782721
1379.501336	102.420912	48.787725
1376.008360	96.162686	48.792730
1372.322553	94.262408	48.797735
1368.246026	97.725295	48.802740
1365.536450	89.959440	48.807745
1361.961038	100.200051	48.812749
1358.123368	97.931114	48.817754
1354.843570	95.331740	48.822759
1351.360599	91.479533	48.827764
1348.432682	92.008065	48.832769
1344.617918	94.050840	48.837773
1341.010355	95.985437	48.842778
1337.287240	91.449288	48.847783
1333.470227	97.111678	48.852788
1330.238569	91.771386	48.857793
1326.692683	103.295025	48.862797
1323.840582	84.468950	48.867802
1320.440665	95.017594	48.872807
1316.718239	98.482316	48.877812
1312.911924	95.594748	48.882817
1309.227452	88.559601	48.887821
1305.445609	86.614171	48.892826
1302.293567	92.875397	48.897831
1298.936368	87.715999	48.902836
1295.692177	84.386608	48.907841
1292.122840	91.823241	48.912845
1288.735248	89.129926	48.917850
1285.007661	86.824884	48.922855
1281.226648	97.056368	48.927860
1277.676365	87.162510	48.932865
1274.047126	89.537075	48.937869
1271.130487	84.824790	48.942874
1267.067953	90.655109	48.947879
1263.593775	99.820128	48.952884
1260.516574	90.947272	48.957889
1257.041199	97.986477	48.962893
1253.399965	91.020538	48.967898
1249.975118	93.837844	48.972903
1246.324040	92.583897	48.977908
1243.010479	92.118955	48.982913
1239.283355	86.684960	48.987917
1236.312289	89.203849	48.992922
1232.026045	96.710948	48.997927
1228.570030	87.131450	49.002932
1225.313017	87.546705	49.007937
1221.612907	94.269722	49.012941
1218.645807	82.045213	49.017946
1214.944456	85.456042	49.022951
1211.628926	85.212869	49.027956
1207.889919	78.398199	49.032961
1204.204898	77.997410	49.037965
1200.578636	80.921998	49.042970
1197.281013	85.858157	49.047975
1193.258130	90.780659	49.052980
1190.625560	80.671211	49.057985
1187.054176	78.648747	49.062989
1183.823335	78.920730	49.067994
1179.877337	91.825899	49.072999
1176.361139	92.749728	49.078004
1172.733717	91.232685	49.083009
1168.975629	90.394028	49.088013
1165.696589	90.657697	49.093018
1162.369258	88.043601	49.098023
1158.807234	91.141690	49.103028
1155.192359	77.227380	49.108033
1151.783027	88.106510	49.113037
1148.248797	83.832050	49.118042
1145.116200	87.543489	49.123047
1141.382007	94.246506	49.128052
1137.775880	79.407041	49.133057
1134.102150	83.541224	49.138061
1130.765112	78.970325	49.143066
1127.706321	86.014289	49.148071
1123.764933	95.764551	49.153076
1120.607366	79.931472	49.158081
1116.783481	84.639510	49.163085
1112.851813	78.822933	49.168090
1109.585850	87.933394	49.173095
1105.946248	79.992816	49.178100
1103.027856	85.353993	49.183105
1099.230122	83.240226	49.188109
1095.910967	76.803139	49.193114
1092.266628	86.586251	49.198119
1088.769284	81.717615	49.203124
1085.805969	83.922103	49.208129
1081.884587	83.732121	49.213133
1078.142311	78.778229	49.218138
1074.672392	79.868867	49.223143
1071.040805	87.748623	49.228148
1067.709409	81.303953	49.233153
1064.106955	91.915762	49.238157
1060.663456	84.590056	49.243162
1057.229976	80.179708	49.248167
1053.485620	81.594634	49.253172
1050.225648	87.537319	49.258177
1046.536468	74.495126	49.263181
1043.085180	86.367855	49.268186
1039.770336	81.344271	49.273191
1036.396584	90.003289	49.278196
1033.196965	86.496154	49.283201
1029.485195	88.677949	49.288205
1025.924225	82.727755	49.293210
1022.497469	89.743582	49.298215
1018.636461	92.736366	49.303220
1015.470825	86.436740	49.308225
1011.568153	83.867930	49.313229
1007.955435	82.127163	49.318234
1004.723922	84.310132	49.323239
1000.612249	87.566557	49.328244
997.711634	82.389917	49.333249
994.508159	74.046124	49.338253
991.208815	89.153793	49.343258
987.044914	84.154816	49.348263
983.444023	87.635447	49.353268
980.176922	84.268535	49.358273
976.238172	94.508762	49.363277
972.979523	80.931339	49.368282
969.802937	82.039600	49.373287
966.471782	81.915942	49.378292
962.865101	79.630089	49.383297
959.182965	86.287048	49.388301
955.697190	73.244850	49.393306
952.097326	68.477617	49.398311
948.438139	81.300172	49.403316
945.361703	74.056555	49.408321
941.432326	81.558737	49.413325
937.691037	78.572522	49.418330
934.624902	77.752733	49.423335
931.342717	75.577721	49.428340
927.893817	71.555764	49.433345
924.377379	72.283508	49.438349
920.464074	73.433689	49.443354
916.973723	77.782947	49.448359
913.368186	73.699955	49.453364
910.329432	70.522132	49.458369
906.970116	77.900777	49.463373
903.130214	72.829238	49.468378
899.468227	72.807705	49.473383
896.057218	78.906781	49.478388
892.990355	72.639260	49.483393
889.349462	79.011397	49.488397
885.518568	82.856862	49.493402
882.122979	75.378205	49.498407
878.187502	81.204592	49.503412
874.964608	76.789966	49.508417
871.142622	88.764694	49.513421
868.279166	87.483101	49.518426
864.801630	77.492589	49.523431
861.033067	82.429312	49.528436
857.642621	84.004299	49.533441
854.215216	90.321063	49.538445
850.564386	80.107597	49.543450
846.780291	82.648674	49.548455
842.863106	85.988733	49.553460
840.103931	86.101910	49.558465
836.607581	86.750609	49.563469
833.152917	85.481959	49.568474
829.504079	83.243814	49.573479
826.477756	78.412627	49.578484
823.000237	75.442317	49.583489
818.879973	83.119751	49.588493
815.218568	79.001179	49.593498
812.313271	80.823343	49.598503
808.933304	84.611276	49.603508
805.170895	78.920264	49.608513
801.486581	83.692021	49.613517
798.052180	77.535509	49.618522
794.568414	79.877983	49.623527
790.819174	80.230705	49.628532
787.426113	78.667741	49.633537
783.966331	77.725754	49.638541
780.404108	74.854054	49.643546
776.901886	81.600073	49.648551
773.676134	85.749971	49.653556
770.141670	83.225118	49.658561
766.650838	86.479834	49.663565
763.096342	73.508489	49.668570
759.580191	80.114311	49.673575
755.648178	79.334421	49.678580
752.612947	76.070650	49.683585
749.243030	83.292772	49.688589
745.424501	87.367274	49.693594
742.067281	77.611151	49.698599
738.432527	78.290898	49.703604
734.802697	71.190411	49.708609
731.432223	82.496919	49.713613
727.952342	81.339774	49.718618
724.630852	65.228610	49.723623
720.530306	72.811232	49.728628
717.471627	69.997195	49.733633
713.942187	77.702881	49.738637
710.301866	75.495066	49.743642
706.726666	75.418920	49.748647
703.153290	75.266562	49.753652
699.845396	69.349798	49.758657
696.561387	80.494153	49.763661
693.304987	74.370061	49.768666
689.811966	70.516357	49.773671
686.227960	73.956421	49.778676
682.845367	74.815213	49.783681
678.324425	74.183960	49.788685
675.028566	70.182511	49.793690
671.967113	80.770216	49.798695
668.315903	74.796171	49.803700
664.754016	66.378527	49.808705
661.145968	76.889972	49.813709
658.335496	77.802070	49.818714
654.481786	72.330939	49.823719
651.174018	78.325377	49.828724
647.467739	67.608080	49.833729
643.554511	74.547797	49.838733
640.321588	77.170768	49.843738
636.799946	71.170233	49.848743
632.914297	74.745843	49.853748
630.016439	73.475961	49.858753
626.582977	72.890555	49.863757
622.845830	68.090965	49.868762
619.056117	73.565660	49.873767
615.640203	75.878608	49.878772
612.531688	73.246344	49.883777
608.954637	74.388511	49.888781
605.538142	80.146785	49.893786
602.166757	79.403026	49.898791
598.360994	81.238842	49.903796
594.960925	58.164063	49.908801
591.396374	76.849978	49.913805
587.656995	76.774096	49.918810
584.489759	69.978101	49.923815
580.263414	82.686480	49.928820
577.319333	76.991501	49.933825
573.952526	72.355723	49.938829
570.413058	73.865356	49.943834
567.295775	75.154246	49.948839
563.480326	76.865027	49.953844
559.956847	77.068742	49.958849
556.019100	70.554048	49.963853
552.520542	71.674510	49.968858
549.006488	61.800487	49.973863
545.508898	63.812953	49.978868
542.511509	68.234191	49.983873
538.775760	75.431018	49.988877
535.240430	77.234232	49.993882
531.916708	63.489891	49.998887
528.316609	70.045521	50.003892
525.258434	73.467015	50.008897
521.681532	68.674134	50.013901
518.191186	68.341201	50.018906
514.100719	66.478733	50.023911
510.210983	80.273631	50.028916
507.301969	69.482868	50.033921
503.619647	77.921029	50.038925
499.894111	73.901077	50.043930
496.855644	72.083641	50.048935
493.018744	74.322938	50.053940
489.549540	76.112700	50.058945
486.215994	78.624804	50.063949
482.906942	71.354209	50.068954
479.334460	68.715102	50.073959
475.779554	72.504987	50.078964
472.215812	67.681594	50.083969
468.672356	77.822334	50.088973
465.146305	74.543268	50.093978
461.737483	69.303463	50.098983
458.188992	80.229578	50.103988
454.786599	68.813301	50.108993
451.041126	71.092153	50.113997
447.252585	77.401890	50.119002
444.353356	73.607640	50.124007
441.318734	75.699900	50.129012
437.628771	81.064175	50.134017
433.849604	80.526287	50.139021
429.962019	78.809412	50.144026
426.481646	77.899152	50.149031
423.107396	78.721876	50.154036
419.883547	82.248265	50.159041
416.278487	81.363744	50.164045
412.496518	72.654554	50.169050
409.248739	83.382002	50.174055
405.314990	85.658534	50.179060
402.029770	77.042848	50.184065
398.398925	82.872473	50.189069
395.199729	80.415703	50.194074
391.846143	72.332668	50.199079
388.266082	80.878301	50.204084
384.649160	76.547239	50.209089
380.916742	79.871240	50.214093
377.645306	76.922697	50.219098
374.219695	74.393615	50.224103
370.643160	79.537763	50.229108
367.156446	68.520601	50.234113
363.770932	71.812741	50.239117
359.953098	75.479062	50.244122
356.898862	74.559416	50.249127
353.116058	77.976682	50.254132
349.519657	75.762086	50.259137
346.332743	78.460179	50.264141
342.931186	78.287448	50.269146
338.984156	74.599392	50.274151
335.667629	71.382638	50.279156
332.294406	72.860091	50.284161
328.586213	74.377039	50.289165
325.077571	74.600621	50.294170
321.535982	81.185127	50.299175
318.020754	80.027215	50.304180
314.455952	71.059618	50.309185
311.204738	78.611288	50.314189
307.240237	77.675179	50.319194
304.053812	73.052491	50.324199
300.140964	85.405205	50.329204
296.395456	72.653533	50.334209
293.354461	73.851485	50.339213
289.962736	75.607062	50.344218
286.836246	65.615811	50.349223
283.387406	80.553756	50.354228
279.809642	70.246793	50.359233
276.170013	73.091302	50.364237
272.452730	81.193248	50.369242
269.152618	77.667072	50.374247
265.615562	80.865762	50.379252
261.743980	76.593352	50.384257
258.144045	80.102379	50.389261
254.856053	76.207335	50.394266
251.889808	69.933749	50.399271
247.882014	74.768574	50.404276
244.732525	62.579008	50.409281
240.733717	71.832062	50.414285
237.240869	74.957434	50.419290
233.987188	69.215805	50.424295
230.343975	71.934330	50.429300
227.157305	66.036742	50.434305
223.658161	76.664126	50.439309
219.837111	83.035894	50.444314
216.896853	71.762851	50.449319
212.721113	79.983632	50.454324
209.558432	73.443251	50.459329
205.725030	77.406234	50.464333
202.531221	70.940302	50.469338
199.044092	74.510864	50.474343
195.269224	78.920303	50.479348
191.728137	71.429633	50.484353
188.374793	77.820331	50.489357
184.965743	75.003971	50.494362
181.685259	69.083032	50.499367
177.918713	80.255073	50.504372
174.426016	74.190009	50.509377
171.064037	77.437379	50.514381
167.522061	86.119464	50.519386
164.299710	67.879690	50.524391
160.154434	80.265430	50.529396
156.810699	77.752108	50.534401
153.506598	82.069276	50.539405
150.191636	73.913841	50.544410
146.441794	72.631137	50.549415
142.565555	68.498678	50.554420
139.266133	64.374489	50.559425
135.713003	70.157235	50.564429
132.544669	65.867110	50.569434
128.904548	68.363711	50.574439
125.307862	64.738208	50.579444
121.896647	58.828147	50.584449
118.463178	56.600879	50.589453
114.521369	66.828962	50.594458
111.083228	58.771811	50.599463
107.595842	70.229407	50.604468
104.577759	67.326882	50.609473
101.189672	65.627208	50.614477
97.653185	60.745859	50.619482
94.235259	62.594122	50.624487
90.203954	71.463118	50.629492
86.828806	71.397039	50.634497
83.401258	65.220615	50.639501
79.461448	68.165666	50.644506
76.575519	70.396159	50.649511
73.126870	72.280845	50.654516
69.485941	58.918194	50.659521
65.772356	66.484918	50.664525
62.173503	71.907808	50.669530
58.636994	70.648850	50.674535
55.027050	66.800805	50.679540
51.804328	70.001196	50.684545
48.259034	66.336069	50.689549
44.479938	66.877037	50.694554
41.381825	72.152366	50.699559
37.793624	71.110260	50.704564
34.210247	63.126355	50.709569
30.740119	73.059554	50.714573
27.559874	69.688758	50.719578
24.150832	64.825544	50.724583
20.405462	65.288501	50.729588
16.755726	68.539562	50.734593
13.418183	69.761571	50.739597
9.571810	67.816899	50.744602
6.198436	55.678071	50.749607
2.884346	70.993651	50.754612