Fri Aug 26 13:43:47 2022

Number of Points = 9931

Depth (nm)	Load (N)	Time (s)
-0.385420	91.058897	0.000000
-0.593431	92.239725	0.005005
-0.401838	88.540084	0.010010
-0.686181	84.892399	0.015014
-0.884333	84.999212	0.020019
-0.998693	72.229550	0.025024
-1.096867	66.515489	0.030029
-1.585393	55.537778	0.035034
-1.516777	51.373253	0.040038
-1.926766	38.032732	0.045043
-2.280690	34.272509	0.050048
-2.454376	31.303609	0.055053
-2.537676	24.555897	0.060058
-3.119171	23.178535	0.065062
-3.461116	12.178029	0.070067
-3.613895	0.610258	0.075072
-3.766744	-10.815130	0.080077
-4.547731	-19.678238	0.085082
-4.814709	-11.332082	0.090086
-5.266642	-14.909362	0.095091
-4.963817	-22.523903	0.100096
-5.368817	-21.616121	0.105101
-5.728017	-20.383288	0.110106
-5.918460	-24.542261	0.115110
-6.242067	-16.497327	0.120115
-6.294562	-23.142253	0.125120
-7.399943	-20.220914	0.130125
-7.482295	-21.574751	0.135130
-7.135722	-25.842644	0.140134
-7.573494	-16.590407	0.145139
-7.927849	-15.396292	0.150144
-8.041882	-16.596505	0.155149
-8.428132	-13.964295	0.160154
-8.792460	-19.605252	0.165158
-9.260182	-13.012134	0.170163
-9.097113	-19.889934	0.175168
-9.193304	-9.634221	0.180173
-9.510040	-21.749068	0.185178
-10.051577	-13.009001	0.190182
-10.619466	-16.270845	0.195187
-10.427434	-19.154313	0.200192
-10.601259	-11.116879	0.205197
-10.527752	-14.143240	0.210202
-10.640530	-16.349686	0.215206
-11.499871	-10.078394	0.220211
-11.748263	-13.601946	0.225216
-12.347959	-11.733740	0.230221
-12.495916	-11.932125	0.235226
-12.525042	-16.673017	0.240230
-12.175550	-9.441535	0.245235
-12.235492	-17.470978	0.250240
-12.871304	-10.218961	0.255245
-13.227961	-9.543323	0.260250
-13.232323	-21.817533	0.265254
-14.278652	-11.148143	0.270259
-14.650900	-22.994927	0.275264
-15.074937	-10.967151	0.280269
-15.032563	-16.010230	0.285274
-14.702895	-19.706038	0.290278
-15.057317	-12.352305	0.295283
-14.880057	-16.340748	0.300288
-15.430871	-4.014829	0.305293
-16.546229	-8.029799	0.310298
-16.070981	-2.497787	0.315302
-16.392248	-9.385599	0.320307
-16.523759	-15.043824	0.325312
-16.238646	-15.980328	0.330317
-17.117191	-23.100896	0.335322
-17.558608	-13.585509	0.340326
-17.711909	-5.658833	0.345331
-17.733149	-13.956886	0.350336
-17.913908	-2.321310	0.355341
-18.514669	-17.353106	0.360346
-19.027615	-14.751788	0.365350
-19.620517	-6.927504	0.370355
-19.241261	-18.755261	0.375360
-19.569679	-10.687431	0.380365
-19.669474	-12.282152	0.385370
-19.675253	-12.293874	0.390374
-19.822180	-8.113941	0.395379
-20.325828	-9.958984	0.400384
-20.825339	-10.649943	0.405389
-20.952340	-8.611733	0.410394
-20.951060	-8.814372	0.415398
-21.275454	-5.786845	0.420403
-21.391099	-15.962056	0.425408
-22.352468	-19.361943	0.430413
-22.499486	-12.638431	0.435418
-22.343624	-18.622962	0.440422
-22.765187	-13.223396	0.445427
-22.684935	-14.109023	0.450432
-22.916436	-10.678359	0.455437
-23.233626	-15.624328	0.460442
-23.598479	-13.517449	0.465446
-24.070524	-16.417741	0.470451
-23.677770	-16.478858	0.475456
-25.041387	-18.370334	0.480461
-24.880585	-17.955591	0.485466
-24.995620	-24.631906	0.490470
-25.483230	-12.034270	0.495475
-25.400383	-19.826525	0.500480
-25.646330	-14.492266	0.505485
-25.475485	-17.881782	0.510490
-26.104985	-15.237007	0.515494
-26.935642	-7.919853	0.520499
-26.505320	-25.067307	0.525504
-27.059652	-12.709211	0.530509
-27.137488	-15.794262	0.535514
-26.848817	-16.810411	0.540518
-27.515831	-9.616809	0.545523
-28.035857	-9.731954	0.550528
-28.371489	-10.344028	0.555533
-28.456471	-5.563157	0.560538
-28.462393	-19.213308	0.565542
-29.319745	-14.188801	0.570547
-29.632034	-14.991164	0.575552
-29.913629	-19.335254	0.580557
-30.258106	-11.891325	0.585562
-30.114211	-8.737401	0.590566
-30.339738	-8.879418	0.595571
-30.465154	-6.142290	0.600576
-30.166990	-6.656899	0.605581
-30.169970	-9.693496	0.610586
-30.738504	-11.974510	0.615590
-31.325804	-10.997217	0.620595
-31.096124	-10.162943	0.625600
-32.024386	-5.551321	0.630605
-32.567322	-14.454655	0.635610
-32.436649	-20.637736	0.640614
-32.792663	-12.606738	0.645619
-33.039840	-14.007676	0.650624
-33.010219	-18.188258	0.655629
-33.254055	-11.699599	0.660634
-33.727337	-14.220062	0.665638
-34.221322	-11.112349	0.670643
-34.161976	-11.542320	0.675648
-34.466496	-8.157233	0.680653
-34.668912	-12.735108	0.685658
-34.610388	-13.664806	0.690662
-35.869831	-7.369182	0.695667
-35.826238	-11.428559	0.700672
-36.041346	-9.901796	0.705677
-36.121177	-17.557995	0.710682
-35.815947	-22.797016	0.715686
-35.718336	-13.419337	0.720691
-36.071827	-19.849725	0.725696
-36.604705	-15.638176	0.730701
-36.798888	-17.825619	0.735706
-37.388435	-19.173250	0.740710
-38.293951	-1.508828	0.745715
-38.361445	-9.628843	0.750720
-38.704165	-14.023527	0.755725
-38.564233	-12.169242	0.760730
-38.290711	-10.126957	0.765734
-38.477282	-7.611253	0.770739
-38.999329	-17.764312	0.775744
-39.660046	-16.440242	0.780749
-40.051880	-21.792186	0.785754
-39.587361	-25.983534	0.790758
-39.908952	-12.861276	0.795763
-40.121958	-17.671609	0.800768
-40.697066	-12.529701	0.805773
-41.062110	-12.972686	0.810778
-41.045291	-13.832618	0.815782
-41.288953	-0.175174	0.820787
-42.123656	-11.412141	0.825792
-42.547672	-13.446745	0.830797
-43.132590	-10.093929	0.835802
-42.469690	-9.592853	0.840806
-42.942006	-9.288335	0.845811
-42.740507	-17.244591	0.850816
-43.144036	-11.620051	0.855821
-43.338132	-6.898119	0.860826
-43.207756	-14.643994	0.865830
-44.151746	-7.166830	0.870835
-43.965875	-18.790474	0.875840
-44.510749	-13.251492	0.880845
-44.693846	-6.531852	0.885850
-44.847031	-20.646272	0.890854
-45.413786	-10.972170	0.895859
-45.720700	-9.190677	0.900864
-45.928798	-19.304033	0.905869
-46.099435	-14.579429	0.910874
-45.993001	-19.433170	0.915878
-46.164525	-6.293146	0.920883
-46.157655	-12.532880	0.925888
-46.892801	-9.045946	0.930893
-47.708666	-17.207619	0.935898
-47.385638	-12.876240	0.940902
-47.802961	-10.707410	0.945907
-48.103470	-27.298161	0.950912
-48.839211	-19.606663	0.955917
-49.345683	-13.295405	0.960922
-48.775311	-15.013451	0.965926
-48.762642	-20.213248	0.970931
-48.634921	-22.014229	0.975936
-48.772614	-13.979261	0.980941
-49.763248	-15.985753	0.985946
-50.361818	-12.061357	0.990950
-50.554819	-10.585490	0.995955
-50.534125	-3.774198	1.000960
-50.806761	4.661426	1.005965
-50.923029	-9.585296	1.010970
-50.950823	-15.262831	1.015974
-51.583446	-17.989428	1.020979
-51.893945	-12.872902	1.025984
-52.207316	-14.864624	1.030989
-52.374115	-20.374987	1.035994
-52.262462	-12.752151	1.040998
-52.373139	-12.899395	1.046003
-52.890657	-12.755512	1.051008
-53.454853	-15.650946	1.056013
-53.917206	-11.652849	1.061018
-53.465922	-18.575521	1.066022
-53.656738	-8.823915	1.071027
-54.034973	-16.468453	1.076032
-54.630016	-9.931439	1.081037
-54.660103	-13.166288	1.086042
-54.626310	-22.055012	1.091046
-55.277366	-13.168187	1.096051
-55.765454	-21.099328	1.101056
-56.552094	-9.875608	1.106061
-56.775022	-10.441957	1.111066
-56.332346	-19.011544	1.116070
-56.345202	-2.723094	1.121075
-56.449301	-17.522176	1.126080
-56.706408	-19.136694	1.131085
-57.313424	-9.845452	1.136090
-57.373029	-16.163416	1.141094
-57.614919	-11.364444	1.146099
-57.612653	-8.827525	1.151104
-58.284788	-6.388075	1.156109
-58.522212	-8.590932	1.161114
-58.819035	-16.023526	1.166118
-59.328872	-3.786245	1.171123
-59.497191	-13.099069	1.176128
-59.388222	-6.972214	1.181133
-59.502703	-0.788421	1.186138
-59.400950	-5.505400	1.191142
-60.481092	-2.325405	1.196147
-60.347297	-13.289233	1.201152
-60.822350	-4.850572	1.206157
-61.037071	-10.897622	1.211162
-61.062976	-10.925192	1.216166
-62.158967	-0.447374	1.221171
-62.229235	-11.784377	1.226176
-62.179744	-4.945933	1.231181
-62.244787	-10.026069	1.236186
-62.813614	-18.811476	1.241190
-62.670175	-8.368459	1.246195
-62.424076	-12.171474	1.251200
-62.535063	-9.332194	1.256205
-63.505521	-8.064297	1.261210
-63.191508	-17.458544	1.266214
-64.131215	-11.924523	1.271219
-65.077271	-9.749297	1.276224
-65.125187	-11.165441	1.281229
-64.808098	-6.152955	1.286234
-65.239166	-13.691193	1.291238
-65.549059	-14.455965	1.296243
-65.368113	-11.127484	1.301248
-65.526938	-0.216636	1.306253
-65.670511	-11.456807	1.311258
-66.237221	-15.889377	1.316262
-67.078054	-9.507077	1.321267
-66.812463	-12.892362	1.326272
-67.153697	-16.515347	1.331277
-67.220221	-10.275751	1.336282
-67.056172	-19.852284	1.341286
-68.132181	-6.644199	1.346291
-68.295666	-12.971299	1.351296
-68.380416	-7.763374	1.356301
-68.446335	-7.658168	1.361306
-68.452899	-10.165879	1.366310
-68.782102	-4.002437	1.371315
-69.195645	-8.227911	1.376320
-69.819689	-12.996392	1.381325
-70.176338	-16.838431	1.386330
-70.104584	-18.545279	1.391334
-70.322855	-8.045945	1.396339
-70.194777	-9.302836	1.401344
-70.098226	-10.266927	1.406349
-70.964875	-10.052866	1.411354
-71.227262	-16.275984	1.416358
-71.462636	-9.481771	1.421363
-71.751303	-16.479052	1.426368
-72.442229	-23.910390	1.431373
-72.950387	-22.670182	1.436378
-72.820207	-18.925689	1.441382
-72.756387	-10.121696	1.446387
-73.096240	-15.842388	1.451392
-72.957367	-12.134048	1.456397
-72.884545	-17.264119	1.461402
-73.623806	-16.908547	1.466406
-74.445974	-7.523696	1.471411
-74.447015	-13.151614	1.476416
-74.607327	-12.104765	1.481421
-74.364123	-14.860164	1.486426
-74.945403	-16.019263	1.491430
-75.746979	-12.465041	1.496435
-75.784909	-12.642593	1.501440
-75.800349	-13.032446	1.506445
-76.013173	-12.344403	1.511450
-75.941211	-11.257792	1.516454
-76.515891	-10.826608	1.521459
-76.797960	-12.797894	1.526464
-77.236401	-17.743963	1.531469
-77.498357	-10.673539	1.536474
-77.427438	-22.924662	1.541478
-77.763542	-15.137204	1.546483
-77.947687	-14.611808	1.551488
-78.610121	-8.086447	1.556493
-78.949477	-11.140270	1.561498
-79.114246	-15.521530	1.566502
-79.277976	-15.771241	1.571507
-78.966460	-19.151021	1.576512
-79.183025	-18.683850	1.581517
-79.593442	-13.909258	1.586522
-79.794586	-10.227068	1.591526
-80.288620	-11.494660	1.596531
-80.285757	-17.433221	1.601536
-80.999875	-20.827310	1.606541
-81.628828	-11.845854	1.611546
-81.536899	-24.138211	1.616550
-82.156150	-16.993177	1.621555
-82.006421	-15.947147	1.626560
-82.000295	-13.205193	1.631565
-82.030117	-12.248262	1.636570
-81.805334	-18.018902	1.641574
-82.492703	-14.071190	1.646579
-82.879421	-18.984183	1.651584
-83.163616	-16.684227	1.656589
-83.515913	-18.685705	1.661594
-83.685776	-11.800457	1.666598
-84.404494	-12.609139	1.671603
-84.204880	-12.599058	1.676608
-84.284987	-12.377752	1.681613
-84.379300	-14.159980	1.686618
-84.948121	-15.330510	1.691622
-85.734571	-10.032314	1.696627
-85.231010	-13.922869	1.701632
-85.808653	-19.075044	1.706637
-86.090842	-16.708964	1.711642
-86.549756	-18.361661	1.716646
-86.727778	-13.787762	1.721651
-86.979531	-24.099951	1.726656
-87.143268	-12.327839	1.731661
-87.567905	-10.350852	1.736666
-86.934615	-11.980623	1.741670
-87.382849	-13.783673	1.746675
-88.262087	-16.506671	1.751680
-88.330365	-13.598115	1.756685
-88.384383	-14.791853	1.761690
-88.482714	-8.749779	1.766694
-89.969252	-3.538723	1.771699
-89.806291	-16.332509	1.776704
-89.927760	-16.484399	1.781709
-90.097400	-22.029117	1.786714
-89.987166	-21.894393	1.791718
-90.427980	-9.395792	1.796723
-90.344022	-19.462872	1.801728
-90.591079	-19.025754	1.806733
-90.720539	-11.333742	1.811738
-91.418385	-15.923057	1.816742
-92.066173	-8.612231	1.821747
-91.930850	-14.321489	1.826752
-92.008541	-11.860704	1.831757
-92.112641	-5.197657	1.836762
-92.215650	-15.495046	1.841766
-93.459273	-18.237236	1.846771
-93.613101	-25.201725	1.851776
-93.623090	-20.856463	1.856781
-93.564655	-10.934870	1.861786
-93.764985	-13.349138	1.866790
-94.100475	-15.299451	1.871795
-93.873270	-23.585559	1.876800
-94.660479	-13.269718	1.881805
-94.827512	-16.951461	1.886810
-94.965074	-21.106010	1.891814
-95.192833	-18.773714	1.896819
-95.584141	-21.952318	1.901824
-96.071143	-13.429547	1.906829
-96.684479	-15.450491	1.911834
-96.357547	-20.806780	1.916838
-96.832204	-7.629056	1.921843
-96.793936	-18.413495	1.926848
-96.705344	-14.836527	1.931853
-96.666581	-13.975692	1.936858
-97.263261	-12.468609	1.941862
-97.687649	-17.369410	1.946867
-98.004214	-27.171650	1.951872
-98.357335	-21.472709	1.956877
-98.781317	-16.471389	1.961882
-98.710875	-20.073051	1.966886
-99.465945	-19.597962	1.971891
-99.453806	-19.030364	1.976896
-99.085950	-18.220769	1.981901
-99.880799	-9.286247	1.986906
-100.361116	-25.678159	1.991910
-100.510608	-16.673286	1.996915
-100.929365	-23.762515	2.006912
-100.745166	-17.534946	2.016909
-100.205988	-16.830075	2.026906
-99.149056	-10.519818	2.036902
-98.682557	-14.985969	2.046899
-98.411417	-17.730157	2.056896
-98.133379	-16.899099	2.066893
-97.179215	-19.901682	2.076890
-97.028964	-13.535783	2.086886
-96.208257	-21.313466	2.096883
-95.541888	-20.846970	2.106880
-95.487964	-23.402119	2.116877
-95.234385	-19.108139	2.126874
-94.558226	-10.552890	2.136870
-94.058985	-17.646985	2.146867
-93.099382	-15.616959	2.156864
-92.929302	-14.376298	2.166861
-92.690737	-9.855071	2.176858
-91.917019	-15.832529	2.186854
-91.351635	-18.381786	2.196851
-90.637932	-14.545903	2.206848
-90.238641	-17.085138	2.216845
-90.226111	-19.842911	2.226842
-89.242749	-14.468338	2.236838
-88.811505	-16.999877	2.246835
-88.708695	-13.743596	2.256832
-87.656968	-8.262460	2.266829
-87.427207	-14.427646	2.276826
-87.038248	-7.227796	2.286822
-86.266495	-19.309084	2.296819
-85.930230	-19.519758	2.306816
-85.292005	-14.807344	2.316813
-85.010264	-14.911331	2.326810
-84.472377	-13.465019	2.336806
-83.678857	-16.730850	2.346803
-83.665526	-16.587145	2.356800
-82.724933	-12.248081	2.366797
-82.214004	-9.201056	2.376794
-81.912840	-12.757680	2.386790
-81.404562	-13.197869	2.396787
-80.661446	-14.925858	2.406784
-80.516521	-13.750970	2.416781
-79.719943	-16.453428	2.426778
-79.204600	-12.998459	2.436774
-79.030929	-18.698763	2.446771
-78.196430	-15.949199	2.456768
-77.686980	-11.207230	2.466765
-77.535898	-9.903425	2.476762
-76.768067	-9.988064	2.486758
-75.831371	-20.736095	2.496755
-76.343096	-17.292268	2.506752
-75.379614	-16.624951	2.516749
-74.593952	-10.963011	2.526746
-74.545344	-14.027332	2.536742
-73.879607	-7.212686	2.546739
-73.325236	-15.081948	2.556736
-72.732383	-14.337918	2.566733
-72.269601	-13.171339	2.576730
-71.804691	-7.896598	2.586726
-71.528420	-7.315511	2.596723
-70.593588	-14.711839	2.606720
-70.629054	-16.486491	2.616717
-69.832618	-19.036878	2.626714
-69.165299	-16.856809	2.636710
-68.893891	-13.832677	2.646707
-67.752303	-16.059849	2.656704
-68.082072	-15.821544	2.666701
-67.412159	-13.882622	2.676698
-66.850724	-16.111328	2.686694
-66.459867	-15.196469	2.696691
-65.897020	-7.158913	2.706688
-64.582278	-16.993326	2.716685
-64.500478	-13.299799	2.726682
-64.632339	-9.528657	2.736678
-64.295979	-14.142434	2.746675
-63.073808	-20.908780	2.756672
-63.032230	-18.700973	2.766669
-62.222784	-18.896625	2.776666
-61.884234	-19.947091	2.786662
-61.540348	-13.437116	2.796659
-60.634438	-14.585423	2.806656
-60.204057	-16.765215	2.816653
-60.063909	-7.721041	2.826650
-59.074732	-13.880928	2.836646
-59.126816	-12.665862	2.846643
-58.136336	-16.060557	2.856640
-57.458537	-15.453293	2.866637
-57.347235	-14.561429	2.876634
-56.804984	-21.902965	2.886630
-56.115417	-17.154196	2.896627
-55.798871	-20.076508	2.906624
-55.472284	-21.844178	2.916621
-54.948407	-11.516651	2.926618
-54.224327	-14.008258	2.936614
-53.506301	-15.323708	2.946611
-53.052322	-19.838593	2.956608
-52.928979	-22.217658	2.966605
-52.270955	-15.914978	2.976602
-51.384157	-19.933403	2.986598
-51.212976	-13.741815	2.996595
-51.190194	-18.123042	3.006592
-50.417227	-14.971102	3.016589
-49.834474	-17.694118	3.026586
-49.166303	-17.506657	3.036582
-48.920120	-16.958898	3.046579
-48.240320	-11.065070	3.056576
-47.384479	-11.692416	3.066573
-47.136708	-21.392379	3.076570
-47.318026	-15.899818	3.086566
-46.279930	-14.661262	3.096563
-45.637439	-14.783404	3.106560
-44.986866	-13.905814	3.116557
-44.162195	-19.302014	3.126554
-44.059148	-13.467269	3.136550
-43.741053	-14.942189	3.146547
-43.742059	-17.865743	3.156544
-43.080853	-15.931800	3.166541
-42.203995	-16.502232	3.176538
-41.324206	-13.490463	3.186534
-40.918348	-21.666040	3.196531
-40.917564	-18.302009	3.206528
-40.398723	-22.918855	3.216525
-40.054436	-16.275899	3.226522
-39.177618	-13.092611	3.236518
-38.605825	-19.998439	3.246515
-38.280818	-14.686077	3.256512
-38.105085	-15.644672	3.266509
-37.227088	-18.448502	3.276506
-36.956233	-17.660672	3.286502
-35.562640	-15.767903	3.296499
-35.540879	-23.465541	3.306496
-35.593403	-17.524215	3.316493
-34.913311	-10.189133	3.326490
-34.112921	-17.992166	3.336486
-33.972529	-19.908236	3.346483
-32.972812	-14.916327	3.356480
-32.661657	-21.138533	3.366477
-32.513014	-20.033912	3.376474
-31.652413	-17.383440	3.386470
-31.351050	-17.531661	3.396467
-30.562650	-20.631974	3.406464
-29.703430	-23.996728	3.416461
-29.973419	-16.241301	3.426458
-29.500403	-9.165404	3.436454
-28.654579	-15.119245	3.446451
-28.133808	-14.091569	3.456448
-27.816010	-20.283133	3.466445
-27.172125	-21.140395	3.476442
-26.698011	-13.244239	3.486438
-26.125625	-19.760534	3.496435
-25.495934	-18.173298	3.506432
-25.454578	-21.084441	3.516429
-24.514579	-19.060862	3.526426
-23.927505	-14.394331	3.536422
-23.591251	-16.939590	3.546419
-23.555870	-19.054713	3.556416
-22.926062	-15.541539	3.566413
-22.358927	-14.964559	3.576410
-21.227376	-13.940116	3.586406
-21.126941	-9.292846	3.596403
-20.713913	-15.635450	3.606400
-20.585337	-14.923665	3.616397
-19.498435	-15.542638	3.626394
-19.296474	-13.144397	3.636390
-18.232837	-10.981682	3.646387
-18.019206	-17.762058	3.656384
-17.946066	-13.655381	3.666381
-17.558422	-16.626777	3.676378
-16.541944	-9.160341	3.686374
-16.232935	-8.891616	3.696371
-15.622614	-11.837497	3.706368
-15.243354	-11.120395	3.716365
-14.736873	-14.050108	3.726362
-13.876287	-18.073955	3.736358
-13.550606	-15.957896	3.746355
-13.614833	-20.088000	3.756352
-12.649334	-13.814182	3.766349
-12.255540	-21.341673	3.776346
-11.356994	-13.517934	3.786342
-10.929238	-11.300562	3.796339
-11.010360	-13.825185	3.806336
-9.885777	-13.749965	3.816333
-9.174176	-21.621533	3.826330
-9.454161	-21.606382	3.836326
-9.254772	-17.690418	3.846323
-7.949412	-23.221646	3.856320
-7.552966	-21.658279	3.866317
-6.951780	-26.661733	3.876314
-6.415637	-21.505784	3.886310
-6.019121	-17.072501	3.896307
-5.890779	-20.165076	3.906304
-5.234686	-18.043442	3.916301
-4.951164	-11.606423	3.926298
-4.572653	-6.986608	3.936294
-4.066426	5.665601	3.946291
-3.665226	17.044918	3.956288
-3.031184	31.530348	3.966285
-2.510262	32.393284	3.976282
-2.253166	57.150089	3.986278
-1.656417	67.491664	3.996275
-0.929797	81.991230	4.006272
-0.616874	98.725102	4.016269
-0.149850	119.217247	4.026266
0.000000	135.728367	4.031270
0.550410	140.584353	4.036275
0.693955	147.699273	4.041280
0.418754	158.549251	4.046285
0.759570	150.609190	4.051290
0.600177	163.405779	4.056294
0.957371	167.924869	4.061299
1.234398	180.425737	4.066304
0.991665	174.120396	4.071309
1.218768	166.473273	4.076314
1.013884	177.682464	4.081318
1.183892	180.085730	4.086323
1.124188	177.570447	4.091328
0.858565	179.332876	4.096333
1.559728	173.465854	4.101338
0.949201	177.199169	4.106342
1.134214	168.448149	4.111347
0.823737	176.994149	4.116352
1.060065	170.395928	4.121357
1.148916	171.403994	4.126362
1.089701	175.624097	4.131366
1.431693	185.691480	4.136371
1.523302	187.183160	4.141376
1.285367	181.139654	4.146381
1.534496	173.580845	4.151386
1.439173	176.734085	4.156390
1.529475	173.983481	4.161395
1.217347	172.757151	4.166400
1.355054	176.551134	4.171405
1.790809	177.587445	4.176410
1.598398	180.135721	4.181414
1.162805	183.490633	4.186419
1.516182	174.001569	4.191424
1.652389	177.795787	4.196429
1.224771	169.057895	4.201434
1.150807	177.491143	4.206438
1.337662	183.697687	4.211443
1.559293	198.994392	4.216448
1.555068	198.874863	4.221453
2.006873	190.098112	4.226458
1.683434	193.922770	4.231462
1.437764	179.993424	4.236467
1.642857	185.295482	4.241472
1.049762	181.164351	4.246477
1.381477	187.142703	4.251482
1.413804	210.131316	4.256486
1.312886	206.901127	4.261491
1.840710	197.581038	4.266496
1.282775	206.054852	4.271501
1.604500	206.087050	4.276506
1.399438	197.295510	4.281510
1.489796	198.717785	4.286515
1.796180	191.719516	4.291520
1.716899	204.358133	4.296525
1.650162	207.978315	4.301530
1.769503	200.506140	4.306534
1.699308	207.401268	4.311539
2.019986	197.313020	4.316544
1.493867	208.366606	4.321549
1.592074	203.947508	4.326554
1.890058	207.536214	4.331558
1.915848	211.240065	4.336563
1.840761	208.205165	4.341568
1.760476	216.851383	4.346573
1.841632	199.179120	4.351578
1.909610	210.219301	4.356582
1.756027	213.966899	4.361587
2.087895	202.500705	4.366592
1.587702	211.841870	4.371597
1.934730	203.268083	4.376602
1.772523	204.119092	4.381606
2.022213	208.512565	4.386611
1.999943	212.983182	4.391616
2.191082	212.124572	4.396621
2.234524	209.454022	4.401626
1.833853	211.316573	4.406630
1.582442	209.296194	4.411635
2.206309	214.030034	4.416640
1.856308	219.336272	4.421645
2.015094	222.756833	4.426650
2.360927	223.860930	4.431654
2.159978	225.483582	4.436659
2.352891	210.577949	4.441664
1.913446	212.848324	4.446669
2.284874	202.616133	4.451674
2.371400	205.060874	4.456678
1.838155	204.865527	4.461683
1.947192	198.929341	4.466688
1.994178	210.168939	4.471693
2.291235	225.254610	4.476698
2.129566	225.887242	4.481702
2.080214	215.736376	4.486707
2.216856	231.732860	4.491712
2.229231	232.053663	4.496717
2.577348	224.732515	4.501722
1.888636	223.691361	4.506726
2.010661	227.778856	4.511731
2.226068	218.241649	4.516736
2.070504	227.019813	4.521741
2.571013	230.121421	4.526746
2.575668	244.597752	4.531750
2.139053	228.992870	4.536755
2.307586	229.846167	4.541760
2.409415	237.255513	4.546765
2.632920	229.308374	4.551770
2.495680	231.651919	4.556774
2.410035	228.090324	4.561779
2.456187	224.713849	4.566784
2.317299	225.640320	4.571789
2.404482	225.699545	4.576794
1.837047	227.455186	4.581798
2.154077	225.523468	4.586803
2.717228	224.407624	4.591808
2.582549	241.344846	4.596813
2.864578	232.274976	4.601818
2.416495	224.391274	4.606822
2.368682	225.948956	4.611827
2.462961	228.528531	4.616832
2.506417	234.830184	4.621837
2.726155	239.772482	4.626842
2.529648	238.082066	4.631846
2.135642	230.686640	4.636851
2.141779	235.769759	4.641856
2.331353	235.898460	4.646861
2.289634	240.482842	4.651866
2.238293	232.382344	4.656870
2.171458	229.770090	4.661875
2.696756	242.649953	4.666880
2.338908	257.220699	4.671885
2.685539	253.085606	4.676890
2.468805	260.136445	4.681894
2.691712	267.311821	4.686899
2.864897	255.863972	4.691904
2.673386	264.752153	4.696909
2.742797	262.213591	4.701914
2.600156	268.503103	4.706918
2.787228	267.423665	4.711923
3.228980	259.043907	4.716928
3.086067	258.161376	4.721933
3.201558	258.390196	4.726938
2.712583	259.004187	4.731942
2.826782	253.459477	4.736947
3.225730	249.047325	4.741952
2.729372	248.143897	4.746957
3.026620	233.706044	4.751962
2.781935	237.088188	4.756966
2.881466	237.521969	4.761971
3.084096	231.039701	4.766976
2.831013	229.361258	4.771981
2.686837	225.220332	4.776986
2.942609	234.380535	4.781990
2.763626	244.139931	4.786995
3.039645	252.661090	4.792000
2.897452	264.910920	4.797005
3.244621	258.203662	4.802010
3.066097	257.187474	4.807014
3.172763	252.352603	4.812019
3.044936	248.939937	4.817024
2.710107	250.042446	4.822029
2.921498	245.966375	4.827034
2.876469	256.312350	4.832038
2.948835	250.220508	4.837043
3.301660	258.128611	4.842048
2.899864	263.737150	4.847053
3.267415	261.478029	4.852058
3.072615	256.800823	4.857062
3.063945	262.142513	4.862067
3.146510	263.939322	4.867072
3.223931	259.523446	4.872077
2.871574	258.395120	4.877082
2.787546	263.811817	4.882086
2.821312	256.495308	4.887091
3.309105	259.317333	4.892096
3.299749	268.173991	4.897101
3.477015	258.206112	4.902106
2.908727	269.592162	4.907110
3.250876	263.923374	4.912115
3.449467	257.378451	4.917120
2.887692	267.950418	4.922125
3.649692	268.350656	4.927130
3.001123	267.157720	4.932134
3.017397	263.966220	4.937139
3.350852	258.330424	4.942144
3.188742	262.199580	4.947149
3.281088	263.504494	4.952154
3.034863	266.965976	4.957158
3.423976	277.725250	4.962163
3.838242	284.677855	4.967168
3.281263	278.370784	4.972173
3.490445	272.501237	4.977178
3.239310	280.424292	4.982182
3.376859	283.677332	4.987187
3.599571	280.532780	4.992192
3.322277	292.344927	4.997197
3.695761	289.793820	5.002202
3.436068	289.331259	5.007206
3.350044	291.670001	5.012211
3.746224	289.368455	5.017216
3.338956	293.275788	5.022221
3.852961	291.677219	5.027226
3.623507	291.165658	5.032230
3.516925	276.762172	5.037235
3.447542	279.889245	5.042240
3.465733	287.435018	5.047245
3.566867	285.521089	5.052250
3.722454	283.772686	5.057254
3.719138	289.762108	5.062259
4.023870	282.216742	5.067264
3.372865	283.751287	5.072269
3.912889	283.898190	5.077274
4.064925	280.679222	5.082278
3.399684	275.113495	5.087283
3.555562	272.567796	5.092288
3.329381	291.009411	5.097293
3.577628	287.364182	5.102298
3.742932	277.322226	5.107302
4.004218	288.743638	5.112307
4.018667	290.702913	5.117312
4.030112	300.812335	5.122317
3.944158	283.510849	5.127322
4.022530	278.693031	5.132326
3.331569	267.354409	5.137331
3.892982	280.652612	5.142336
3.886836	295.086374	5.147341
4.146741	288.484438	5.152346
3.821015	291.733681	5.157350
3.694487	292.152040	5.162355
3.799953	291.645280	5.167360
3.998209	293.699321	5.172365
3.890133	292.355792	5.177370
3.655251	291.126918	5.182374
3.672112	290.191036	5.187379
3.758510	288.393294	5.192384
3.739739	297.007828	5.197389
3.602724	295.472656	5.202394
3.478762	297.614829	5.207398
3.791811	296.579049	5.212403
3.894540	296.404903	5.217408
3.812333	309.964686	5.222413
4.045351	307.849890	5.227418
4.215998	322.480771	5.232422
4.386094	318.711664	5.237427
4.186968	312.614616	5.242432
4.011389	306.991622	5.247437
3.935707	302.359131	5.252442
3.957882	307.509375	5.257446
3.961346	313.867902	5.262451
4.206364	314.968719	5.267456
4.048995	320.282959	5.272461
4.213415	306.653489	5.277466
3.943827	323.624449	5.282470
3.742005	316.490125	5.287475
4.187713	324.203465	5.292480
4.093809	325.584838	5.297485
4.028991	320.438131	5.302490
4.362086	328.596106	5.307494
3.739123	324.399990	5.312499
4.250609	319.913353	5.317504
4.197257	319.048512	5.322509
3.998143	316.782701	5.327514
4.486754	321.404754	5.332518
4.309402	329.398599	5.337523
4.081329	324.195053	5.342528
4.167642	335.852543	5.347533
4.345981	347.100249	5.352538
4.554756	352.544151	5.357542
4.543309	345.225153	5.362547
4.541041	343.548777	5.367552
4.461211	331.567642	5.372557
4.145471	317.414983	5.377562
4.431507	328.193500	5.382566
4.457095	342.587560	5.387571
4.854936	339.112015	5.392576
4.205355	329.219050	5.397581
4.690318	331.924470	5.402586
4.500175	330.144471	5.407590
4.479070	326.712011	5.412595
4.423423	328.081100	5.417600
4.267399	342.705912	5.422605
4.639191	337.326710	5.427610
4.467490	337.018124	5.432614
4.616777	344.442272	5.437619
5.368721	340.538278	5.442624
4.711362	338.486177	5.447629
4.701921	326.082805	5.452634
4.429775	317.096011	5.457638
4.273227	311.340341	5.462643
4.623596	321.808286	5.467648
4.627103	342.438274	5.472653
4.585490	335.022739	5.477658
4.846912	340.815938	5.482662
4.832086	346.683787	5.487667
4.769885	336.515870	5.492672
4.730308	334.886432	5.497677
4.783095	327.241070	5.502682
4.512722	338.065096	5.507686
4.618667	339.602013	5.512691
4.891042	341.274366	5.517696
4.711746	349.942391	5.522701
5.021837	342.184197	5.527706
4.899640	342.937235	5.532710
4.684817	339.088852	5.537715
5.003024	341.883511	5.542720
4.861887	342.588879	5.547725
4.947796	336.627774	5.552730
4.862105	347.511635	5.557734
4.719157	339.627829	5.562739
4.913563	341.239556	5.567744
4.611744	346.386473	5.572749
4.853306	338.756007	5.577754
4.790587	344.840116	5.582758
4.826805	348.045671	5.587763
5.131147	339.143112	5.592768
4.712154	344.210196	5.597773
4.588783	342.384999	5.602778
4.701733	342.981205	5.607782
4.483266	344.065602	5.612787
4.588499	337.383328	5.617792
4.675342	352.694824	5.622797
4.598928	363.453865	5.627802
4.971326	363.721780	5.632806
4.825985	362.978825	5.637811
5.245149	372.572398	5.642816
5.121809	374.755612	5.647821
4.906834	373.352792	5.652826
4.795465	366.808633	5.657830
4.924483	371.698655	5.662835
5.069584	367.566439	5.667840
4.663372	366.142775	5.672845
5.162195	387.201889	5.677850
5.124713	383.310066	5.682854
5.096750	392.951119	5.687859
5.388300	392.918414	5.692864
5.414622	396.631712	5.697869
5.275146	385.444429	5.702874
5.057826	383.589563	5.707878
5.424090	389.483512	5.712883
5.486283	387.025149	5.717888
5.483491	382.324342	5.722893
5.124534	369.102174	5.727898
5.194521	371.413473	5.732902
5.299245	381.821625	5.737907
5.445277	373.256905	5.742912
5.169520	374.919692	5.747917
5.402327	386.086177	5.752922
5.524027	390.613516	5.757926
5.070129	398.419498	5.762931
5.187935	390.162881	5.767936
5.293310	397.340791	5.772941
5.706523	398.908965	5.777946
5.720247	396.746045	5.782950
5.264707	397.120721	5.787955
5.588377	395.203770	5.792960
5.385830	403.660309	5.797965
5.638978	392.146139	5.802970
5.466075	398.525828	5.807974
5.223479	411.009687	5.812979
5.516742	410.979879	5.817984
5.283005	407.457124	5.822989
5.515851	401.833784	5.827994
5.593768	406.927922	5.832998
5.396358	398.252149	5.838003
5.650829	400.591676	5.843008
5.551068	401.689232	5.848013
5.700627	398.711070	5.853018
5.654166	403.134883	5.858022
5.815590	401.072351	5.863027
5.579762	394.446321	5.868032
5.177430	404.117195	5.873037
5.478864	399.745499	5.878042
5.451576	397.750314	5.883046
5.311673	400.274627	5.888051
5.691817	408.409495	5.893056
5.527849	406.777270	5.898061
5.791718	409.820843	5.903066
5.518757	412.106450	5.908070
5.398100	418.136331	5.913075
5.841145	415.969840	5.918080
5.837225	426.809380	5.923085
5.717436	421.247265	5.928090
5.269180	424.838309	5.933094
5.196005	427.833122	5.938099
5.946342	426.292657	5.943104
5.450254	434.475379	5.948109
5.830616	429.104306	5.953114
5.827490	422.929248	5.958118
5.691140	424.772812	5.963123
5.988160	425.802265	5.968128
5.797976	431.602533	5.973133
5.868679	436.767404	5.978138
6.243799	437.810007	5.983142
5.918551	426.594675	5.988147
5.886383	430.503746	5.993152
5.734442	431.387967	5.998157
6.191823	440.194188	6.003162
6.129559	438.508161	6.008166
5.638949	443.020117	6.013171
6.293247	441.776176	6.018176
6.384997	443.419714	6.023181
5.919293	427.689473	6.028186
6.317739	425.580544	6.033190
6.134420	433.720896	6.038195
6.531283	423.206212	6.043200
5.944104	430.783025	6.048205
6.013664	423.236250	6.053210
6.378413	428.092749	6.058214
6.085327	432.909303	6.063219
6.193690	424.040379	6.068224
5.969779	433.436719	6.073229
6.019706	423.583486	6.078234
5.893063	427.228858	6.083238
5.695054	427.892464	6.088243
5.784543	422.057323	6.093248
5.733516	429.183668	6.098253
6.397508	436.195526	6.103258
6.099513	428.759759	6.108262
5.818866	430.771321	6.113267
6.095907	435.758535	6.118272
5.992449	430.532393	6.123277
5.684113	431.567513	6.128282
6.081647	445.637993	6.133286
6.241951	449.672124	6.138291
6.553765	448.114513	6.143296
6.469846	441.524925	6.148301
6.088732	429.970279	6.153306
6.152464	421.649301	6.158310
6.225775	429.313101	6.163315
6.275338	432.402699	6.168320
6.015125	434.259222	6.173325
6.134213	427.941749	6.178330
5.906496	426.091660	6.183334
5.950070	430.444514	6.188339
6.359462	429.586713	6.193344
5.894290	429.507314	6.198349
6.106601	424.026367	6.203354
6.004321	429.945825	6.208358
5.769949	428.549184	6.213363
6.165620	426.203408	6.218368
6.451887	433.312040	6.223373
5.979633	426.181813	6.228378
6.077013	432.206224	6.233382
5.867571	424.880057	6.238387
5.972138	431.102663	6.243392
6.230460	426.598469	6.248397
6.076438	424.787526	6.253402
6.597061	424.753957	6.258406
6.541978	424.563252	6.263411
6.392667	425.545140	6.268416
6.368833	429.927471	6.273421
6.143926	421.173711	6.278426
6.112852	413.250308	6.283430
5.495134	406.481254	6.288435
6.011157	420.786363	6.293440
6.029791	432.375361	6.298445
6.172182	420.593682	6.303450
6.223587	418.497659	6.308454
6.236458	427.256023	6.313459
6.254848	424.333081	6.318464
6.082914	417.418688	6.323469
6.194645	401.813698	6.328474
6.099695	396.285688	6.333478
5.913494	402.904728	6.338483
6.087437	397.875848	6.343488
6.034093	402.351351	6.348493
6.488868	409.297697	6.353498
5.948985	409.283713	6.358502
5.543596	405.139123	6.363507
5.810686	401.740870	6.368512
5.912872	417.012067	6.373517
5.968958	408.768215	6.378522
6.083183	416.033339	6.383526
5.890042	429.246656	6.388531
6.247136	421.984141	6.393536
6.004837	426.156879	6.398541
6.352644	416.038974	6.403546
6.268208	423.556492	6.408550
5.808340	418.012526	6.413555
6.233416	424.356069	6.418560
5.996174	424.200053	6.423565
5.938648	424.825968	6.428570
6.464673	428.771516	6.433574
6.309886	430.203504	6.438579
5.831799	412.668720	6.443584
6.150202	415.074224	6.448589
6.135612	409.755158	6.453594
6.136210	416.275518	6.458598
5.832732	411.877780	6.463603
6.247737	417.150388	6.468608
5.815186	409.257858	6.473613
6.152294	416.039032	6.478618
6.519521	413.368660	6.483622
6.091801	405.883498	6.488627
5.933665	402.443885	6.493632
5.717299	400.822983	6.498637
6.093900	408.759089	6.503642
6.074797	413.966409	6.508646
6.128743	417.289437	6.513651
6.063877	412.022491	6.518656
6.095229	404.605058	6.523661
6.126616	397.545122	6.528666
6.157808	399.232886	6.533670
5.778706	402.512604	6.538675
6.161665	404.806817	6.543680
6.021930	408.492188	6.548685
6.030023	411.379434	6.553690
6.217399	417.411975	6.558694
5.993449	415.956765	6.563699
5.823677	408.788941	6.568704
6.226615	418.695109	6.573709
6.160318	413.077213	6.578714
6.169649	409.630507	6.583718
5.843011	411.696683	6.588723
5.979284	411.077557	6.593728
5.815631	423.172651	6.598733
6.055662	420.749869	6.603738
6.206200	425.674520	6.608742
6.324027	431.091477	6.613747
6.214702	419.814057	6.618752
6.125444	408.046308	6.623757
5.996317	404.016890	6.628762
6.150819	399.297916	6.633766
5.516048	409.061929	6.638771
6.276601	413.233547	6.643776
6.137364	429.852122	6.648781
6.054267	418.406106	6.653786
6.072418	426.461303	6.658790
5.971698	429.261091	6.663795
6.272140	426.230960	6.668800
6.129981	416.122903	6.673805
5.969985	410.617671	6.678810
5.897195	410.483506	6.683814
6.091070	426.018843	6.688819
6.156486	428.473228	6.693824
5.811445	432.845460	6.698829
6.061451	433.401348	6.703834
6.166999	430.806516	6.708838
6.093229	432.418877	6.713843
5.939717	429.374004	6.718848
6.005319	429.313204	6.723853
6.163185	433.293927	6.728858
6.294347	426.183645	6.733862
5.700610	428.664728	6.738867
6.153996	419.103017	6.743872
6.086036	431.167398	6.748877
5.962861	434.948272	6.753882
6.061446	434.062933	6.758886
5.859753	432.452399	6.763891
6.030881	425.981293	6.768896
6.151426	443.103593	6.773901
5.876468	432.453061	6.778906
6.012821	428.031131	6.783910
6.088465	423.530070	6.788915
6.183499	421.389289	6.793920
6.226026	431.908393	6.798925
6.312563	426.190767	6.803930
6.387222	425.587561	6.808934
5.765924	424.475788	6.813939
6.241177	415.537090	6.818944
6.006092	424.353041	6.823949
5.913641	431.185283	6.828954
6.084867	415.517235	6.833958
5.773533	417.403861	6.838963
6.532163	420.281820	6.843968
6.506116	421.162258	6.848973
6.118666	400.851449	6.853978
5.936654	402.948890	6.858982
5.583506	406.180277	6.863987
6.393263	407.085606	6.868992
5.763745	409.129337	6.873997
5.931404	420.524284	6.879002
6.109459	422.698542	6.884006
6.288500	429.115195	6.889011
6.117365	416.531293	6.894016
6.176013	411.735492	6.899021
5.903805	408.440187	6.904026
6.036531	409.773626	6.909030
5.867850	418.209081	6.914035
6.522915	417.360486	6.919040
6.211574	409.401628	6.924045
6.052082	408.246428	6.929050
6.361035	400.624425	6.934054
6.002068	401.132759	6.939059
5.960450	405.726659	6.944064
5.835749	405.059581	6.949069
5.987876	401.233144	6.954074
6.149922	402.641111	6.959078
6.221929	412.912008	6.964083
6.236279	396.426853	6.969088
5.705575	392.842771	6.974093
5.638591	399.740638	6.979098
6.005955	414.366276	6.984102
6.264448	424.092459	6.989107
6.543374	424.881123	6.994112
6.362000	413.488376	6.999117
5.961386	400.222051	7.004122
6.242506	402.193601	7.009126
6.359713	404.136889	7.014131
6.078680	410.777024	7.019136
5.843892	410.000538	7.024141
5.872669	402.589834	7.029146
6.078774	402.662180	7.034150
6.146945	406.463876	7.039155
5.990394	395.997408	7.044160
5.982842	391.601056	7.049165
6.028776	409.019675	7.054170
6.170162	398.389760	7.059174
5.978037	404.000498	7.064179
6.120677	401.361931	7.069184
6.109608	405.286694	7.074189
5.844702	402.815983	7.079194
5.999008	396.132374	7.084198
5.699773	393.964398	7.089203
5.930831	399.844600	7.094208
6.031733	404.612460	7.099213
5.871116	413.419975	7.104218
6.479720	423.635806	7.109222
5.989464	407.510777	7.114227
5.944450	407.324832	7.119232
6.255098	413.670369	7.124237
5.814949	406.187142	7.129242
6.411150	398.352740	7.134246
5.955350	408.455879	7.139251
6.337546	397.918183	7.144256
5.956115	405.643284	7.149261
5.873299	405.418933	7.154266
5.868011	402.281384	7.159270
6.126623	418.626037	7.164275
6.471244	406.955249	7.169280
6.325659	406.269277	7.174285
6.077212	405.165891	7.179290
6.249392	401.519828	7.184294
5.916980	395.633325	7.189299
6.455356	390.092132	7.194304
6.124783	401.311541	7.199309
5.892504	400.446081	7.204314
5.873407	390.853546	7.209318
6.038759	398.506166	7.214323
6.323420	399.825440	7.219328
5.916319	399.531357	7.224333
6.019862	401.160401	7.229338
6.112047	410.504350	7.234342
5.604051	404.360449	7.239347
5.936169	402.692115	7.244352
5.607935	412.022430	7.249357
6.241485	414.344065	7.254362
5.908449	417.205331	7.259366
5.705729	425.791620	7.264371
6.210781	421.755208	7.269376
5.970680	432.030417	7.274381
6.039593	440.561766	7.279386
6.231137	425.830171	7.284390
6.163819	428.039470	7.289395
6.271162	428.924451	7.294400
6.092709	429.047180	7.299405
5.985033	426.257760	7.304410
5.897357	412.825645	7.309414
5.804715	425.827162	7.314419
5.843251	427.396727	7.319424
6.331857	423.467278	7.324429
6.675438	427.374793	7.329434
6.532893	415.251507	7.334438
6.101111	406.248394	7.339443
5.940893	398.402051	7.344448
6.116532	405.837941	7.349453
5.812760	402.028702	7.354458
6.018512	400.664777	7.359462
5.658827	400.897980	7.364467
6.434752	408.825695	7.369472
6.074748	410.767355	7.374477
5.787632	402.788909	7.379482
6.053293	401.393511	7.384486
6.368169	421.351859	7.389491
6.189599	407.351776	7.394496
6.259754	404.398631	7.399501
6.001956	400.142479	7.404506
6.340507	395.894717	7.409510
6.124419	410.215729	7.414515
5.949404	401.533304	7.419520
6.077400	408.470418	7.424525
6.021731	402.594609	7.429530
6.242556	398.729003	7.434534
5.812141	406.493368	7.439539
6.169116	402.255391	7.444544
6.095137	402.570659	7.449549
6.057409	402.813845	7.454554
6.013637	400.574457	7.459558
5.995924	404.285121	7.464563
6.032953	401.371936	7.469568
6.310741	401.436285	7.474573
6.349478	400.677323	7.479578
6.336807	402.020744	7.484582
5.968735	408.310603	7.489587
6.226258	404.334880	7.494592
6.247751	405.492650	7.499597
6.017376	411.745253	7.504602
5.952334	407.902008	7.509606
5.896165	407.097711	7.514611
6.010529	400.584833	7.519616
6.085396	410.064354	7.524621
6.144509	413.339122	7.529626
5.893087	408.329010	7.534630
5.827740	411.525079	7.539635
6.196793	407.987565	7.544640
6.029749	408.219248	7.549645
6.242819	406.363808	7.554650
6.280158	408.828889	7.559654
6.038844	415.532444	7.564659
6.094385	406.450293	7.569664
5.950262	404.555554	7.574669
5.919544	407.278001	7.579674
6.059555	411.827805	7.584678
5.842509	414.136343	7.589683
6.298446	402.473536	7.594688
6.243427	410.084543	7.599693
5.895294	407.139577	7.604698
6.333003	409.861858	7.609702
5.844691	413.206038	7.614707
6.077693	406.842363	7.619712
6.065364	407.714337	7.624717
5.872136	411.673790	7.629722
6.027660	412.196932	7.634726
5.835623	414.416157	7.639731
5.933200	411.262591	7.644736
6.208407	407.274623	7.649741
6.019453	420.898565	7.654746
5.871909	410.633164	7.659750
5.731808	407.766538	7.664755
5.922959	415.247472	7.669760
6.299629	415.976625	7.674765
5.830015	416.853359	7.679770
5.840817	417.319941	7.684774
6.245878	433.480456	7.689779
6.424908	425.135198	7.694784
6.549009	421.860443	7.699789
6.193191	416.072490	7.704794
6.125571	412.242300	7.709798
5.951219	417.663616	7.714803
6.056857	406.957005	7.719808
6.189003	412.450821	7.724813
5.855411	406.567662	7.729818
6.165906	411.290236	7.734822
6.226930	413.527007	7.739827
6.286682	398.809626	7.744832
6.212409	404.000223	7.749837
6.090194	411.647003	7.754842
6.487694	404.144089	7.759846
5.881564	407.196567	7.764851
6.070377	407.138730	7.769856
6.038180	414.534217	7.774861
6.038523	411.920967	7.779866
6.341722	404.663686	7.784870
6.335340	409.929135	7.789875
6.003876	409.218321	7.794880
5.832637	412.269528	7.799885
5.737580	404.814829	7.804890
5.891406	407.875535	7.809894
6.049025	411.922730	7.814899
5.841955	401.780495	7.819904
5.822441	402.451110	7.824909
5.738357	405.836755	7.829914
5.778119	398.740714	7.834918
6.029988	411.429157	7.839923
6.025313	413.065560	7.844928
6.085676	406.981861	7.849933
5.582483	416.731719	7.854938
6.077731	422.659380	7.859942
6.340869	429.524842	7.864947
6.199535	417.338092	7.869952
5.856128	415.869845	7.874957
6.129038	422.047255	7.879962
6.468290	412.756415	7.884966
6.067129	410.439793	7.889971
6.073689	408.676615	7.894976
6.067286	403.055724	7.899981
5.968898	409.762334	7.904986
6.112394	408.841530	7.909990
5.951304	411.951268	7.914995
5.827666	410.872741	7.920000
5.681263	409.038468	7.925005
6.312803	426.308980	7.930010
6.261277	421.147520	7.935014
6.128132	413.154589	7.940019
6.130529	413.075156	7.945024
6.314236	403.732609	7.950029
5.996030	409.290214	7.955034
6.305840	399.526243	7.960038
6.143524	407.017915	7.965043
6.426318	407.783829	7.970048
6.330789	414.986699	7.975053
5.883951	415.954799	7.980058
6.311486	410.095502	7.985062
6.078722	409.125715	7.990067
6.134770	407.386469	7.995072
6.103721	404.556648	8.000077
6.289769	408.102713	8.005082
6.565662	406.601318	8.010086
6.753877	404.528287	8.015091
6.483836	392.184426	8.020096
6.180744	390.444152	8.025101
6.143763	389.621051	8.030106
6.601852	378.420859	8.035123
6.069374	382.170650	8.040141
6.168724	373.272091	8.045158
6.461379	380.446662	8.050176
6.154296	380.118986	8.055194
6.134450	379.844413	8.060211
5.929729	386.821885	8.065229
5.946989	387.784857	8.070246
6.566524	383.911130	8.075264
6.214940	383.454689	8.080282
5.887145	386.077606	8.085299
5.650600	385.742103	8.090317
5.729471	384.032122	8.095334
6.050804	380.230069	8.100352
5.711773	378.395816	8.105370
5.823023	370.278004	8.110387
5.676301	383.302115	8.115405
6.215839	394.291290	8.120422
6.314628	400.407356	8.125440
5.892232	397.090306	8.130458
6.581260	397.008306	8.135475
6.272098	391.218536	8.140493
6.140398	387.234566	8.145510
6.228119	379.366553	8.150528
5.984818	377.580508	8.155546
6.107756	379.429539	8.160563
6.391962	395.166683	8.165581
6.212694	382.442682	8.170598
6.100321	376.568632	8.175616
6.154834	380.612019	8.180634
6.147392	385.453964	8.185651
5.787412	395.806903	8.190669
6.051363	395.412408	8.195686
6.199520	404.105261	8.200704
5.983247	403.836026	8.205722
6.461397	391.833283	8.210739
6.111515	392.891286	8.215757
6.413495	403.002317	8.220774
6.334370	401.380046	8.225792
6.166604	407.758512	8.230810
6.294742	398.139127	8.235827
6.271219	408.638494	8.240845
5.919036	401.687831	8.245862
5.993577	404.576295	8.250880
5.814307	402.329021	8.255898
6.105393	400.885784	8.260915
5.973736	404.298633	8.265933
5.790551	405.393795	8.270950
6.346028	412.505369	8.275968
6.100327	429.410590	8.280986
6.391087	415.370058	8.286003
6.514786	429.803697	8.291021
6.348962	435.717989	8.296038
6.681155	429.433895	8.301056
6.368562	430.508184	8.306074
6.197094	430.396065	8.311091
6.121675	435.895515	8.316109
6.598586	434.921936	8.321126
6.488325	428.457433	8.326144
6.289648	428.261193	8.331162
6.382984	426.047208	8.336179
6.315121	429.686803	8.341197
6.430091	432.723604	8.346214
6.723211	430.633140	8.351232
6.142951	422.222202	8.356250
6.656793	429.889348	8.361267
6.254238	426.430354	8.366285
6.090865	425.518597	8.371302
6.508059	429.628597	8.376320
6.336272	432.719512	8.381338
6.405183	426.990781	8.386355
6.315257	425.382813	8.391373
6.441004	435.934691	8.396390
6.819673	430.104085	8.401408
6.396598	430.065853	8.406426
6.584676	430.093406	8.411443
6.452339	426.955240	8.416461
6.406116	431.131081	8.421478
6.394245	424.310452	8.426496
6.038086	435.357062	8.431514
6.589876	431.891484	8.436531
6.484304	433.788721	8.441549
6.464732	432.965022	8.446566
6.595265	427.961963	8.451584
6.414362	435.819327	8.456602
6.423768	432.185743	8.461619
6.496984	425.541205	8.466637
6.353429	429.665932	8.471654
6.455378	423.692229	8.476672
6.066134	428.022457	8.481690
6.458690	427.118814	8.486707
6.567725	428.133768	8.491725
6.176780	437.576414	8.496742
6.836400	436.037927	8.501760
6.267626	427.735646	8.506778
6.409171	432.554406	8.511795
6.455521	434.115581	8.516813
6.319326	435.276009	8.521830
6.712029	431.513324	8.526848
6.315266	440.836964	8.531866
6.517903	445.087665	8.536883
6.532031	458.512800	8.541901
6.800212	462.699656	8.546918
6.885358	458.057088	8.551936
6.506680	444.461572	8.556954
6.504057	438.810244	8.561971
6.911002	441.618560	8.566989
6.460341	443.317075	8.572007
6.833347	428.935539	8.577024
6.350098	437.887654	8.582042
6.664898	445.872961	8.587059
6.737257	450.560494	8.592077
6.648211	454.244415	8.597095
6.657082	448.048522	8.602112
6.954444	444.527885	8.607130
6.678789	434.135102	8.612147
6.389206	436.638473	8.617165
6.140745	444.957618	8.622183
6.691652	455.014143	8.627200
6.546481	461.086167	8.632218
6.557826	462.551814	8.637235
6.812031	458.567701	8.642253
6.667766	468.385347	8.647271
6.801381	462.987342	8.652288
6.809410	452.705006	8.657306
6.780502	460.081146	8.662323
7.090800	452.705441	8.667341
6.761504	458.326472	8.672359
7.077180	463.064483	8.677376
6.969955	459.291271	8.682394
6.792149	451.549770	8.687411
6.704229	441.225578	8.692429
6.717097	438.790602	8.697447
6.450600	441.716392	8.702464
6.582359	451.573101	8.707482
6.279872	456.798656	8.712499
6.416892	461.905294	8.717517
6.590092	466.466683	8.722535
6.496503	467.481630	8.727552
6.722698	465.654034	8.732570
6.647812	460.682949	8.737587
6.806884	464.432378	8.742605
6.961071	468.334040	8.747623
6.958073	462.790055	8.752640
6.567682	465.353304	8.757658
6.729052	464.078574	8.762675
6.945917	454.196047	8.767693
6.661602	458.986450	8.772711
6.939830	456.756297	8.777728
6.821210	462.521244	8.782746
6.584515	462.056381	8.787763
6.891654	470.614066	8.792781
6.952400	489.765793	8.797799
7.613371	487.024786	8.802816
7.171558	473.375965	8.807834
7.173625	472.451069	8.812851
6.940888	466.848182	8.817869
6.905181	474.143340	8.822887
7.058567	465.753849	8.827904
6.884712	459.087808	8.832922
7.287032	447.421867	8.837939
6.842713	452.038374	8.842957
6.930491	457.521888	8.847975
6.772979	460.276086	8.852992
6.733123	459.625949	8.858010
6.930293	460.706074	8.863027
7.056279	456.246487	8.868045
6.935866	463.671588	8.873063
6.688704	463.836330	8.878080
7.015892	463.715997	8.883098
6.814939	464.864420	8.888115
6.957494	453.343056	8.893133
6.867233	457.320643	8.898151
7.117866	450.007875	8.903168
7.321697	460.635969	8.908186
6.971726	461.226952	8.913203
7.221597	458.859209	8.918221
6.936304	470.093613	8.923239
6.900497	457.710122	8.928256
6.868337	458.125398	8.933274
6.916729	466.291041	8.938291
7.183796	463.087528	8.943309
7.206622	469.376383	8.948327
7.066362	459.855555	8.953344
6.956593	453.687598	8.958362
6.814414	458.051947	8.963379
6.811017	465.275802	8.968397
6.998936	479.513298	8.973415
7.198176	484.149529	8.978432
7.141905	482.129235	8.983450
7.161346	485.998235	8.988467
7.119922	481.643598	8.993485
7.168829	485.145109	8.998503
7.469553	485.376019	9.003520
7.113007	476.460031	9.008538
6.846721	476.397387	9.013555
7.128908	471.594755	9.018573
7.109062	484.999955	9.023591
7.393292	485.088272	9.028608
7.322161	478.163245	9.033626
6.978024	478.415666	9.038643
7.306379	475.963121	9.043661
6.980802	481.842344	9.048679
7.077092	485.689911	9.053696
7.187775	481.914323	9.058714
7.164599	488.513291	9.063731
7.529431	483.000388	9.068749
7.070241	484.656056	9.073767
7.343872	477.516412	9.078784
7.347333	485.345094	9.083802
7.184543	475.998170	9.088819
7.539036	474.920578	9.093837
6.945294	477.010585	9.098855
7.330693	477.171509	9.103872
7.667279	481.770577	9.108890
7.007614	464.804373	9.113907
7.377468	466.346739	9.118925
6.864656	460.897908	9.123943
7.299333	477.066112	9.128960
7.216617	479.205937	9.133978
7.327862	490.334435	9.138995
7.592338	482.483035	9.144013
7.397358	483.226605	9.149031
7.256402	482.150416	9.154048
7.451665	476.572402	9.159066
7.137833	478.195971	9.164083
7.367344	479.144836	9.169101
7.477919	490.973994	9.174119
7.474280	470.254547	9.179136
7.396873	467.117288	9.184154
6.878213	467.592532	9.189171
7.166960	466.342149	9.194189
7.107720	486.932599	9.199207
7.472905	486.269889	9.204224
7.596909	480.860751	9.209242
7.275572	491.296088	9.214259
7.469157	486.721832	9.219277
7.341037	477.928061	9.224295
7.373456	486.620040	9.229312
7.469338	485.942457	9.234330
7.088280	480.523597	9.239347
7.172324	482.574345	9.244365
7.304119	484.879579	9.249383
7.216656	482.618000	9.254400
7.455420	484.082953	9.259418
7.227441	487.343564	9.264435
7.394160	480.075405	9.269453
7.275330	487.967307	9.274471
7.309925	481.193067	9.279488
7.290996	479.940096	9.284506
7.378480	489.216767	9.289523
7.715558	501.809049	9.294541
7.456134	505.547909	9.299559
7.561009	499.494834	9.304576
7.766609	496.326130	9.309594
7.552688	493.273234	9.314611
7.478517	487.724544	9.319629
7.701050	482.965910	9.324647
7.511596	484.197746	9.329664
7.459620	491.757364	9.334682
7.589802	488.739252	9.339699
7.580267	487.292323	9.344717
7.504276	486.881329	9.349735
7.607927	487.123989	9.354752
7.507319	481.655153	9.359770
7.149669	493.970605	9.364787
7.769007	503.962858	9.369805
7.844177	513.503378	9.374823
7.778600	508.079570	9.379840
7.780377	486.147487	9.384858
7.338141	495.787490	9.389875
7.475554	485.358764	9.394893
7.864584	508.397662	9.399911
7.558204	490.202522	9.404928
7.966816	486.260631	9.409946
7.340966	489.510610	9.414963
7.576257	483.601329	9.419981
7.837057	501.910919	9.424999
7.563439	490.220808	9.430016
7.610090	490.753196	9.435034
7.899718	505.482939	9.440051
7.284081	496.856577	9.445069
7.693468	509.103106	9.450087
7.787235	512.228425	9.455104
7.775108	500.150472	9.460122
7.839739	512.172982	9.465139
7.788152	497.579801	9.470157
7.690109	498.096849	9.475175
7.639527	499.445914	9.480192
7.914148	505.717668	9.485210
7.677191	500.001824	9.490227
7.887657	509.757952	9.495245
7.791388	501.385225	9.500263
7.163931	505.070938	9.505280
7.686727	498.895992	9.510298
7.686813	513.689756	9.515315
7.983902	512.428604	9.520333
7.680853	514.287172	9.525351
7.560566	518.039083	9.530368
7.674404	510.305796	9.535386
7.845414	516.256030	9.540403
7.953131	508.580498	9.545421
7.849793	516.268038	9.550439
7.789397	511.597626	9.555456
7.959383	503.779863	9.560474
7.752946	511.193132	9.565491
7.986341	510.143859	9.570509
7.893997	507.813613	9.575527
7.790689	508.173698	9.580544
7.892803	517.687936	9.585562
7.753235	510.842976	9.590579
8.175706	513.809825	9.595597
8.063411	513.335059	9.600615
7.809101	516.890097	9.605632
8.059178	511.546524	9.610650
8.231262	512.359171	9.615667
8.054638	511.869175	9.620685
8.090470	510.743370	9.625703
8.022586	510.788685	9.630720
8.068906	510.488030	9.635738
7.981284	511.536763	9.640755
7.879038	521.527769	9.645773
8.016665	508.536597	9.650791
7.582650	512.419402	9.655808
7.836085	508.908747	9.660826
8.055272	518.963310	9.665843
8.094260	516.227624	9.670861
8.203399	520.029019	9.675879
7.957934	519.145816	9.680896
8.136782	511.771618	9.685914
8.042051	514.001677	9.690931
7.974475	515.567974	9.695949
8.163798	512.679499	9.700967
7.917610	513.030274	9.705984
8.034920	506.258925	9.711002
7.898705	524.554615	9.716019
7.904886	519.249013	9.721037
7.849171	516.117836	9.726055
7.576220	523.399461	9.731072
7.898881	508.612307	9.736090
7.842879	521.657107	9.741107
7.938976	511.572455	9.746125
8.104175	510.978748	9.751143
8.000213	515.210934	9.756160
7.965274	516.481829	9.761178
7.882421	522.099222	9.766195
7.919934	530.648424	9.771213
8.248428	529.205664	9.776231
8.028735	532.991990	9.781248
8.493052	532.206551	9.786266
8.299328	539.412734	9.791283
8.187480	526.716000	9.796301
8.120188	519.380122	9.801319
7.750783	515.445756	9.806336
8.292004	526.715605	9.811354
8.150719	539.975659	9.816371
8.385391	532.311906	9.821389
8.810021	530.109441	9.826407
8.093118	526.727771	9.831424
8.392174	513.411673	9.836442
8.166004	521.175142	9.841459
8.317853	511.801301	9.846477
8.200096	509.424520	9.851495
8.049390	512.458521	9.856512
8.054632	517.793965	9.861530
8.133070	532.553456	9.866547
8.527540	542.792171	9.871565
8.643411	531.420073	9.876583
8.085528	523.128673	9.881600
8.375045	514.569648	9.886618
8.379436	522.035299	9.891635
8.340686	523.019622	9.896653
8.480784	510.214248	9.901671
8.008807	516.920971	9.906688
8.153963	520.505329	9.911706
8.199346	526.137470	9.916723
8.203024	538.021171	9.921741
8.520731	532.932139	9.926759
8.495750	542.286305	9.931776
8.735370	535.628439	9.936794
8.687016	531.454743	9.941811
8.124262	523.072588	9.946829
8.232725	525.233143	9.951847
8.614732	534.962576	9.956864
8.740596	532.459504	9.961882
8.285571	523.855457	9.966899
8.065016	510.557149	9.971917
8.340555	516.702538	9.976935
8.068013	535.773669	9.981952
8.537796	545.432640	9.986970
8.408455	544.209478	9.991987
8.645491	539.085668	9.997005
8.505806	538.886554	10.002023
8.065519	544.837304	10.007040
8.641924	539.603854	10.012058
8.886069	543.775537	10.017075
8.647153	549.884276	10.022093
8.884062	532.406045	10.027111
8.249301	538.295558	10.032128
8.514088	533.243165	10.037146
8.378335	540.784291	10.042163
8.143927	537.876582	10.047181
8.409501	540.227263	10.052199
7.987847	548.242076	10.057216
8.489265	544.430885	10.062234
8.573828	545.872515	10.067251
8.491172	541.691534	10.072269
8.707709	537.170494	10.077287
8.651510	539.710123	10.082304
8.722017	539.554018	10.087322
8.385226	535.153842	10.092339
8.745903	544.795087	10.097357
8.893221	536.788344	10.102375
8.551614	538.599271	10.107392
8.990151	534.873607	10.112410
8.823620	532.150983	10.117427
8.767620	538.565740	10.122445
9.015078	532.266402	10.127463
8.749524	533.513246	10.132480
8.797078	542.284942	10.137498
9.042397	539.406679	10.142515
8.769343	526.157558	10.147533
8.682790	510.960765	10.152551
8.641098	518.042288	10.157568
8.709365	511.253327	10.162586
8.793497	523.174983	10.167603
8.575256	517.430974	10.172621
8.957791	520.120032	10.177639
8.737645	527.163074	10.182656
8.843898	508.521834	10.187674
8.592196	507.500754	10.192691
8.594507	517.415522	10.197709
8.978163	514.872314	10.202727
8.887132	519.746243	10.207744
8.775266	509.435207	10.212762
8.780361	504.805091	10.217779
8.635255	519.507862	10.222797
8.895956	523.055296	10.227815
9.125337	540.085461	10.232832
8.838361	514.067531	10.237850
8.919636	513.322797	10.242867
8.365914	519.363780	10.247885
9.036983	511.613158	10.252903
8.921973	523.619466	10.257920
8.999677	525.314616	10.262938
8.795321	524.074734	10.267955
8.852475	528.395442	10.272973
8.645141	520.286140	10.277991
8.641277	535.071070	10.283008
8.929749	524.117051	10.288026
8.988521	527.979936	10.293043
8.521361	532.316009	10.298061
8.846102	530.899079	10.303079
8.612886	533.516758	10.308096
8.607913	532.138540	10.313114
8.640073	532.370241	10.318131
9.027742	530.990847	10.323149
8.905116	527.024367	10.328167
8.852155	533.558564	10.333184
8.809514	528.004953	10.338202
9.119064	525.337588	10.343219
9.024632	532.310568	10.348237
8.889535	529.772390	10.353255
8.928770	526.115209	10.358272
8.826335	537.980720	10.363290
8.922762	554.381531	10.368307
8.876186	557.550798	10.373325
9.320253	556.661218	10.378343
9.103466	572.586970	10.383360
9.064633	559.629547	10.388378
9.376037	559.880885	10.393395
8.938331	554.467667	10.398413
9.331503	550.632303	10.403431
9.067531	538.028671	10.408448
9.073122	538.390736	10.413466
9.330003	532.695818	10.418483
8.831366	533.937928	10.423501
9.406065	537.035708	10.428519
8.877978	534.337819	10.433536
9.157102	544.004385	10.438554
9.513759	540.528144	10.443571
8.930820	535.961172	10.448589
9.134327	526.935871	10.453607
9.323114	541.794949	10.458624
9.038873	528.689572	10.463642
9.206287	541.835295	10.468659
9.447010	541.737891	10.473677
8.920245	529.557016	10.478695
9.235677	540.988256	10.483712
9.146127	553.157870	10.488730
9.592914	558.585520	10.493747
9.043185	549.368227	10.498765
9.101113	539.103317	10.503783
9.389741	551.990345	10.508800
9.178396	556.390732	10.513818
9.278523	550.003877	10.518835
9.104385	561.426151	10.523853
9.550157	555.629236	10.528871
9.469070	554.509009	10.533888
9.299579	547.873812	10.538906
9.398507	538.754338	10.543923
9.305697	547.825591	10.548941
9.419950	552.086924	10.553959
9.443501	550.514923	10.558976
9.294026	542.750037	10.563994
9.181114	543.720663	10.569011
9.006794	551.659100	10.574029
9.447744	551.019304	10.579047
9.315744	560.456411	10.584064
9.109892	563.489539	10.589082
9.411787	559.674696	10.594099
9.327211	564.247844	10.599117
9.574505	557.421525	10.604135
9.956540	553.420644	10.609152
9.422498	550.875152	10.614170
9.424578	551.846808	10.619187
9.264446	556.845111	10.624205
9.026016	553.859134	10.629223
9.249110	558.453802	10.634240
9.105274	569.334898	10.639258
9.300985	557.092009	10.644275
9.105601	569.754619	10.649293
9.239651	556.224349	10.654311
9.113055	563.830328	10.659328
9.398350	576.544330	10.664346
9.748953	579.405619	10.669363
9.610876	581.759195	10.674381
9.552744	585.384684	10.679399
9.507432	584.956289	10.684416
9.598865	588.476444	10.689434
9.834828	587.426767	10.694451
9.469818	593.293232	10.699469
9.540755	591.208941	10.704487
9.583474	585.500016	10.709504
9.653793	593.201575	10.714522
9.843242	586.217000	10.719539
9.371088	588.354359	10.724557
9.553408	584.513949	10.729575
9.816694	585.886733	10.734592
9.943717	591.111724	10.739610
9.697123	575.384395	10.744627
9.341266	574.272234	10.749645
9.713826	581.311374	10.754663
9.761881	582.244317	10.759680
9.494849	585.589919	10.764698
9.841267	585.494993	10.769715
9.737910	589.155925	10.774733
10.080666	575.653104	10.779751
9.960133	583.529535	10.784768
9.583649	575.149910	10.789786
10.084547	557.425434	10.794803
9.321161	561.930707	10.799821
9.659298	561.938052	10.804839
9.321968	567.377339	10.809856
9.272458	582.185193	10.814874
9.483996	574.411420	10.819891
9.716983	581.664788	10.824909
9.891879	584.550279	10.829927
9.768283	582.521523	10.834944
9.467589	594.840799	10.839962
9.844102	587.136006	10.844979
9.974876	588.280123	10.849997
9.880681	594.991169	10.855015
10.068223	588.615937	10.860032
9.956559	587.730832	10.865050
9.861141	587.912973	10.870067
9.864637	606.571987	10.875085
9.987362	595.599551	10.880103
9.878022	593.915698	10.885120
9.898892	601.766966	10.890138
9.865135	590.626400	10.895155
9.855159	585.787179	10.900173
9.762215	597.477689	10.905191
10.087051	592.668385	10.910208
10.258546	602.143465	10.915226
10.224757	589.999399	10.920243
9.961141	595.916348	10.925261
9.756126	590.861349	10.930279
10.189967	598.029804	10.935296
9.888514	596.262258	10.940314
9.920312	587.386732	10.945331
9.922222	590.835622	10.950349
9.814783	590.050842	10.955367
9.869775	592.926602	10.960384
9.518537	587.705030	10.965402
9.830431	595.741348	10.970419
10.564678	605.065698	10.975437
9.878896	598.422507	10.980455
10.226507	596.796891	10.985472
9.948095	589.556969	10.990490
10.251383	593.432288	10.995507
9.956676	595.699804	11.000525
10.208153	599.958717	11.005543
10.124917	595.225570	11.010560
10.066183	595.566094	11.015578
10.275560	604.940607	11.020595
10.210015	598.383878	11.025613
10.216550	607.332400	11.030631
9.750005	598.891050	11.035648
10.030189	606.866041	11.040666
10.264585	605.958612	11.045683
10.228321	613.512679	11.050701
10.175660	601.920632	11.055719
10.186614	607.801147	11.060736
10.588641	610.629190	11.065754
10.431551	611.250105	11.070771
10.590273	615.921080	11.075789
10.080368	600.578694	11.080807
10.205760	594.531859	11.085824
10.088141	595.724118	11.090842
10.389640	608.094806	11.095859
10.225047	611.326637	11.100877
10.253230	606.260572	11.105895
10.482348	598.383070	11.110912
10.364659	598.862156	11.115930
10.149617	603.815374	11.120947
10.310950	611.812028	11.125965
10.191236	610.353842	11.130983
10.212129	609.823624	11.136000
10.191708	612.408183	11.141018
10.412308	603.399116	11.146035
10.505703	613.896179	11.151053
10.117211	614.783488	11.156071
10.158223	606.717528	11.161088
10.438442	615.052264	11.166106
10.444732	612.735049	11.171123
10.640489	605.105726	11.176141
10.566436	614.281385	11.181159
10.547171	607.928877	11.186176
10.366231	614.571389	11.191194
10.392029	605.084586	11.196211
10.269027	608.922143	11.201229
10.299870	606.017304	11.206247
10.423814	614.411085	11.211264
10.660325	614.617282	11.216282
10.437782	611.915989	11.221299
10.619596	615.500970	11.226317
10.373094	618.395274	11.231335
10.397502	611.262823	11.236352
10.489381	607.692100	11.241370
10.536009	613.188381	11.246387
10.885577	604.231814	11.251405
10.490821	612.302425	11.256423
10.853341	611.425539	11.261440
10.651733	616.868955	11.266458
10.444274	612.426533	11.271475
10.583526	613.073890	11.276493
10.493412	618.462080	11.281511
10.777395	613.072174	11.286528
10.267493	621.873901	11.291546
10.187196	617.676757	11.296563
10.399013	624.949216	11.301581
10.376764	644.016205	11.306599
11.033057	638.685085	11.311616
11.146462	643.789140	11.316634
10.527347	632.266334	11.321651
10.865702	634.192301	11.326669
10.879275	626.714406	11.331687
10.979054	613.542865	11.336704
10.806193	617.492324	11.341722
10.663463	613.547888	11.346739
10.608437	613.524932	11.351757
10.264168	610.394485	11.356775
10.390461	633.966739	11.361792
10.542366	633.034284	11.366810
10.684309	636.634944	11.371827
10.971490	637.672665	11.376845
10.756228	639.643804	11.381863
10.873593	638.966026	11.386880
11.034190	636.466998	11.391898
10.676238	642.745775	11.396915
10.442096	636.950557	11.401933
10.302109	645.902977	11.406951
10.628807	649.768353	11.411968
10.889315	648.149983	11.416986
10.829120	648.206724	11.422003
10.829715	655.354297	11.427021
11.061111	655.747477	11.432039
11.208238	648.980898	11.437056
11.245238	637.611545	11.442074
11.157852	639.253517	11.447091
10.962928	644.153123	11.452109
10.774077	637.120135	11.457127
11.041884	634.585481	11.462144
11.057229	638.524576	11.467162
10.951745	641.308570	11.472179
11.129870	631.113252	11.477197
10.605931	638.064787	11.482215
11.029293	634.773794	11.487232
10.811243	639.329874	11.492250
10.922180	654.286370	11.497267
11.338946	659.699791	11.502285
11.492641	654.118727	11.507303
11.321673	650.219703	11.512320
10.925850	644.178266	11.517338
10.896351	645.041239	11.522355
11.115128	638.396048	11.527373
10.740398	645.314887	11.532391
11.276269	639.942557	11.537408
11.180980	646.489698	11.542426
11.255909	651.170572	11.547443
10.983498	635.560814	11.552461
11.096473	652.426181	11.557479
11.321452	660.737983	11.562496
11.436016	655.828861	11.567514
10.951152	647.683819	11.572531
11.388116	653.526422	11.577549
11.128409	658.675951	11.582567
11.391286	657.666259	11.587584
11.124749	658.521959	11.592602
11.266410	658.840751	11.597619
11.198671	656.456163	11.602637
11.363183	663.013351	11.607655
11.366838	657.629209	11.612672
11.414338	656.466865	11.617690
11.235012	652.184148	11.622707
11.449919	657.556416	11.627725
11.319680	652.780081	11.632743
11.004755	646.959568	11.637760
11.152448	653.383676	11.642778
11.380362	666.084586	11.647795
11.599807	661.525194	11.652813
11.312894	668.291518	11.657831
11.621312	660.199678	11.662848
11.723656	664.557563	11.667866
11.304400	656.645290	11.672883
11.244406	653.521066	11.677901
11.412140	660.046194	11.682919
11.395296	668.941585	11.687936
11.554987	664.621860	11.692954
11.372737	663.195496	11.697971
11.127909	665.303781	11.702989
11.396660	667.508823	11.708007
11.592711	660.362251	11.713024
11.439378	661.591631	11.718042
11.171024	669.500582	11.723059
11.653827	655.912782	11.728077
11.463862	663.503423	11.733095
11.526681	671.029465	11.738112
11.696418	663.716582	11.743130
11.096349	667.533758	11.748147
11.347454	675.532241	11.753165
11.276681	674.729125	11.758183
11.613172	668.415877	11.763200
11.743057	663.431787	11.768218
11.495298	669.478830	11.773235
11.581398	668.919524	11.778253
11.554177	666.935710	11.783271
11.348091	668.081789	11.788288
11.350996	678.091224	11.793306
11.481952	684.858765	11.798323
11.429197	683.712028	11.803341
11.629561	696.155326	11.808359
11.668757	696.423803	11.813376
11.741706	687.538664	11.818394
11.557887	689.463890	11.823411
11.839896	683.320059	11.828429
11.555535	692.891408	11.833447
11.810318	690.115785	11.838464
11.753299	688.307016	11.843482
11.587705	686.698182	11.848499
11.827442	684.944192	11.853517
11.891996	690.926839	11.858535
11.797771	685.299161	11.863552
12.150479	683.959912	11.868570
11.921452	686.955645	11.873587
12.069060	679.870255	11.878605
12.083082	686.242606	11.883623
12.221400	686.621877	11.888640
12.162691	681.566163	11.893658
12.100937	688.587763	11.898675
12.174680	677.900604	11.903693
11.880214	670.915603	11.908711
11.567461	663.100350	11.913728
11.807663	667.686071	11.918746
11.863083	678.681373	11.923763
12.046159	675.257377	11.928781
11.959194	687.385657	11.933799
11.834626	689.437352	11.938816
12.068303	688.476385	11.943834
11.971886	690.653081	11.948851
12.144749	689.913013	11.953869
11.938342	685.287379	11.958887
11.806771	678.472666	11.963904
11.935954	682.801131	11.968922
11.769423	682.211732	11.973939
11.946495	681.603549	11.978957
11.901466	687.022608	11.983975
12.158302	680.996302	11.988992
12.258617	686.632564	11.994010
12.103788	688.073611	11.999027
11.951352	688.577043	12.004045
11.864469	689.426863	12.009063
11.717686	687.815101	12.014080
12.036617	683.707256	12.019098
11.712094	695.370772	12.024115
12.124686	699.090246	12.029133
12.138299	716.753756	12.034151
12.255429	705.646429	12.039168
12.652664	709.302027	12.044186
11.861609	705.430111	12.049203
12.296269	711.181576	12.054221
12.293726	715.842973	12.059239
12.283640	720.202598	12.064256
12.636761	710.772070	12.069274
12.221194	708.517367	12.074291
12.154581	694.260868	12.079309
12.172171	705.681783	12.084327
12.024624	706.878709	12.089344
12.574140	719.750484	12.094362
12.356750	721.914462	12.099379
12.285069	716.299043	12.104397
12.664418	711.910395	12.109415
12.159580	705.444112	12.114432
12.277887	708.013397	12.119450
12.052074	715.268827	12.124467
12.060859	710.953653	12.129485
12.251616	715.250449	12.134503
12.185233	718.703686	12.139520
12.340850	713.769223	12.144538
12.315609	716.802657	12.149555
12.238096	723.066201	12.154573
12.422059	722.570548	12.159591
12.197171	711.301881	12.164608
12.309575	715.203791	12.169626
12.037479	718.411355	12.174643
12.572204	730.726883	12.179661
12.889330	732.368997	12.184679
12.879989	737.160842	12.189696
12.656465	714.613481	12.194714
12.158009	715.262303	12.199731
12.491253	725.920898	12.204749
12.937369	737.407654	12.209767
12.520199	718.693060	12.214784
12.643424	715.060632	12.219802
12.387351	725.978233	12.224819
12.784137	733.524886	12.229837
13.062422	734.191624	12.234855
12.607424	724.445111	12.239872
12.574168	718.072653	12.244890
12.671129	720.370718	12.249907
12.646581	715.606311	12.254925
12.660443	720.375604	12.259943
12.224209	721.835221	12.264960
12.529053	733.078891	12.269978
12.806018	746.217175	12.274995
12.799904	736.006304	12.280013
12.862152	736.126029	12.285031
12.731884	742.094846	12.290048
13.164785	738.972757	12.295066
13.143692	745.038182	12.300083
12.787069	734.758811	12.305101
12.826583	733.323159	12.310119
12.490109	723.570816	12.315136
12.998150	720.859896	12.320154
12.661413	747.543331	12.325171
13.051609	747.965435	12.330189
13.173155	745.339933	12.335207
12.696029	742.870755	12.340224
13.055002	736.058537	12.345242
12.558697	734.968233	12.350259
12.813336	744.026513	12.355277
12.928244	745.700114	12.360295
12.813972	744.897456	12.365312
12.929557	744.576545	12.370330
12.703199	748.856245	12.375347
12.574570	750.264815	12.380365
12.817668	749.699997	12.385383
12.676742	750.908517	12.390400
12.811304	748.754343	12.395418
12.896021	753.099216	12.400435
13.200926	751.398187	12.405453
13.100614	747.898383	12.410471
12.745518	755.511618	12.415488
12.751364	750.234402	12.420506
13.064302	760.896179	12.425523
13.595233	761.567763	12.430541
13.067100	752.526877	12.435559
13.090610	754.457698	12.440576
13.157250	755.198414	12.445594
13.300757	769.783874	12.450611
13.149814	758.320632	12.455629
13.303124	747.955548	12.460647
13.476976	744.384657	12.465664
13.567578	736.960993	12.470682
13.514605	746.082946	12.475699
13.223903	742.893644	12.480717
13.241293	745.308239	12.485735
13.019512	746.418898	12.490752
13.140548	738.188946	12.495770
13.036377	746.466831	12.500787
13.144315	745.623264	12.505805
12.880193	743.139857	12.510823
13.140321	752.332982	12.515840
13.547813	756.640224	12.520858
13.536717	775.629880	12.525875
13.075025	759.175353	12.530893
13.523395	760.172206	12.535911
13.555787	771.483565	12.540928
13.429048	757.782314	12.545946
13.042205	757.069429	12.550963
13.339731	769.699616	12.555981
13.852681	771.708865	12.560999
13.170605	767.674805	12.566016
13.616730	768.031400	12.571034
13.756386	766.592776	12.576051
13.644781	762.592970	12.581069
13.439732	747.979296	12.586087
13.131964	751.779382	12.591104
13.411436	768.454838	12.596122
13.596952	768.703690	12.601139
13.330207	774.457088	12.606157
13.648677	771.917683	12.611175
13.508788	771.264174	12.616192
13.342453	775.837483	12.621210
13.418207	774.809583	12.626227
13.339145	767.923546	12.631245
13.565607	776.907338	12.636263
13.626741	778.403127	12.641280
13.854068	772.192043	12.646298
13.770122	772.508094	12.651315
13.756438	775.299905	12.656333
13.818877	766.914966	12.661351
13.707774	775.591563	12.666368
14.078748	771.286253	12.671386
13.636792	775.848827	12.676403
13.444686	776.816016	12.681421
13.717180	767.050884	12.686439
13.373354	779.055121	12.691456
13.406572	767.553733	12.696474
13.428816	778.857210	12.701491
13.379177	776.608639	12.706509
13.485854	769.094098	12.711527
13.550293	784.925763	12.716544
13.707113	794.687244	12.721562
13.911015	803.478908	12.726579
13.740717	799.945810	12.731597
14.128829	786.158065	12.736615
14.129627	801.450559	12.741632
13.834933	800.259436	12.746650
14.178806	793.727250	12.751667
13.681772	793.877251	12.756685
14.004721	789.434250	12.761703
13.926026	803.404257	12.766720
13.758844	792.142332	12.771738
13.832754	798.435973	12.776755
13.623365	796.351124	12.781773
13.980795	795.834773	12.786791
13.986759	798.017632	12.791808
13.841817	803.408102	12.796826
13.748806	796.205499	12.801843
13.642012	801.179786	12.806861
14.102906	795.512980	12.811879
13.823085	797.065011	12.816896
13.650166	800.269771	12.821914
14.010754	812.675582	12.826931
13.795700	823.416447	12.831949
14.224452	819.619668	12.836967
13.813281	822.672183	12.841984
14.083394	823.870359	12.847002
14.513380	821.026413	12.852019
13.884882	828.461347	12.857037
14.374013	819.116880	12.862055
14.140087	821.857785	12.867072
14.078840	820.381011	12.872090
14.262857	809.947996	12.877107
13.895745	820.002498	12.882125
14.457613	809.889339	12.887143
14.256623	823.067383	12.892160
14.174306	823.332690	12.897178
14.433060	824.378004	12.902195
14.187039	816.681677	12.907213
14.519136	820.022401	12.912231
14.057864	828.374858	12.917248
13.909214	830.919455	12.922266
14.441096	828.413084	12.927283
14.125134	836.626159	12.932301
14.357342	824.500477	12.937319
14.283441	827.812899	12.942336
14.326194	831.015642	12.947354
14.317271	834.971182	12.952371
13.929954	843.965365	12.957389
14.630767	843.881531	12.962407
14.630124	848.163980	12.967424
14.554226	859.104101	12.972442
14.578973	854.499236	12.977459
14.194385	863.593987	12.982477
14.908335	859.680213	12.987495
14.821588	844.438987	12.992512
14.201987	847.328303	12.997530
14.639142	846.607039	13.002547
14.526441	858.692106	13.007565
14.463338	857.294511	13.012583
14.510052	851.291397	13.017600
14.145778	856.308944	13.022618
14.682335	850.223251	13.027635
14.226988	848.861482	13.032653
14.386678	849.250052	13.037671
14.486239	851.692893	13.042688
14.384803	852.576543	13.047706
14.393386	845.247653	13.052723
14.513670	856.475955	13.057741
14.497715	866.586260	13.062759
14.931254	867.967272	13.067776
14.702310	870.789457	13.072794
14.925702	872.023312	13.077811
14.991373	877.696585	13.082829
14.877375	863.305320	13.087847
14.954026	860.484824	13.092864
14.750580	848.647857	13.097882
15.045215	850.179878	13.102899
15.037694	850.048542	13.107917
14.918363	845.254678	13.112935
15.111504	843.937106	13.117952
14.887433	850.479126	13.122970
14.884382	838.841332	13.127987
14.783366	855.771765	13.133005
15.242951	847.170324	13.138023
15.140943	841.288195	13.143040
14.898226	848.356967	13.148058
15.102070	845.510359	13.153075
14.891087	840.197449	13.158093
15.163926	847.274311	13.163111
15.344151	853.191667	13.168128
15.087002	853.001369	13.173146
15.218125	848.966908	13.178163
15.023102	850.849715	13.183181
14.997838	851.361753	13.188199
15.127467	853.522209	13.193216
14.691511	848.856534	13.198234
15.071640	857.024354	13.203251
14.880201	853.450357	13.208269
14.912759	852.675325	13.213287
14.856117	850.964308	13.218304
14.937885	866.979536	13.223322
15.332040	878.304064	13.228339
15.316130	876.996947	13.233357
15.183165	877.667763	13.238375
15.429251	876.906820	13.243392
15.309688	877.919523	13.248410
15.013264	865.648907	13.253427
15.108091	871.790998	13.258445
15.328071	874.079397	13.263463
15.434532	877.045018	13.268480
15.458891	883.904968	13.273498
15.577094	881.983693	13.278515
15.655475	872.283439	13.283533
15.553510	859.689068	13.288551
15.453916	858.385515	13.293568
15.179990	856.051937	13.298586
15.475987	844.601102	13.303603
15.194101	853.058181	13.308621
15.381049	847.452945	13.313639
15.153405	858.574478	13.318656
15.379092	872.535017	13.323674
15.679169	865.321675	13.328691
15.629403	877.860848	13.333709
15.604755	881.418069	13.338727
15.148446	876.843916	13.343744
15.159103	878.189786	13.348762
15.673954	872.558735	13.353779
15.177001	883.012175	13.358797
15.220608	880.446123	13.363815
15.314292	876.048264	13.368832
15.282158	880.897343	13.373850
15.408658	874.566226	13.378867
15.302881	879.000747	13.383885
15.644707	891.744041	13.388903
15.668699	899.765364	13.393920
15.594716	902.812730	13.398938
15.862082	905.021173	13.403955
15.833671	904.347148	13.408973
15.910087	908.409335	13.413991
15.797475	894.024141	13.419008
15.631338	884.731171	13.424026
15.888002	881.623874	13.429043
15.525630	892.021653	13.434061
16.017325	899.361099	13.439079
15.977442	899.187466	13.444096
15.572473	907.143038	13.449114
16.093564	890.103039	13.454131
15.756387	891.578803	13.459149
15.630224	898.951333	13.464167
15.942348	905.264726	13.469184
15.697461	906.839729	13.474202
15.797471	907.105052	13.479219
15.803647	909.505637	13.484237
16.039265	908.519110	13.489255
16.287892	902.677041	13.494272
15.736660	909.039651	13.499290
16.103233	901.361517	13.504307
15.951919	898.330361	13.509325
16.169037	903.992686	13.514343
16.204548	906.716899	13.519360
15.792953	899.923610	13.524378
16.086532	905.706572	13.529395
15.953105	900.249028	13.534413
16.021034	908.033145	13.539431
16.150214	906.602453	13.544448
15.940945	911.109898	13.549466
16.097961	902.315703	13.554483
15.938288	901.895639	13.559501
15.858714	904.369533	13.564519
15.866969	900.900132	13.569536
15.763805	905.665604	13.574554
16.020338	899.188003	13.579571
15.977149	907.551140	13.584589
15.873419	919.432885	13.589607
16.343998	924.759115	13.594624
16.358403	929.083420	13.599642
16.467333	925.402684	13.604659
16.625387	932.058804	13.609677
16.589415	934.323946	13.614695
16.390736	919.362009	13.619712
16.112391	924.154762	13.624730
16.576726	928.289097	13.629747
16.464236	919.003535	13.634765
16.174964	924.274505	13.639783
16.496250	922.312140	13.644800
16.315576	930.977554	13.649818
16.805235	928.711269	13.654835
16.718804	927.796972	13.659853
16.317467	916.943802	13.664871
16.484885	899.315090	13.669888
16.031245	912.485200	13.674906
16.258284	924.381718	13.679923
16.745592	930.238665	13.684941
16.364032	933.053064	13.689959
16.799967	927.513177	13.694976
16.327916	929.625313	13.699994
16.533898	933.405406	13.705011
16.260456	924.331090	13.710029
16.199150	928.742921	13.715047
16.672656	928.643985	13.720064
16.392461	940.341784	13.725082
16.340428	933.473565	13.730099
16.453104	929.997367	13.735117
16.156298	945.206935	13.740135
16.689846	951.776198	13.745152
16.688238	952.429720	13.750170
16.960713	959.386766	13.755187
16.817902	956.874973	13.760205
16.646286	963.027023	13.765223
16.657739	949.102141	13.770240
16.750883	953.054439	13.775258
16.909866	958.066283	13.780275
17.052720	956.434646	13.785293
16.899381	956.171381	13.790311
17.031915	955.942501	13.795328
16.889789	957.406837	13.800346
17.036811	952.142293	13.805363
17.256050	953.136964	13.810381
17.209936	952.172209	13.815399
17.083033	952.902042	13.820416
17.175470	957.198426	13.825434
17.155852	949.627736	13.830451
17.026747	933.812371	13.835469
16.827626	929.352793	13.840487
17.155160	936.698879	13.845504
17.286410	940.960815	13.850522
17.046046	938.404255	13.855539
16.906678	933.922749	13.860557
16.926482	938.564946	13.865575
17.423247	947.525673	13.870592
17.053031	946.033879	13.875610
17.026257	946.574557	13.880627
17.226190	942.791287	13.885645
17.118104	952.054468	13.890663
17.363316	952.619070	13.895680
17.245562	953.218093	13.900698
17.164613	961.217913	13.905715
17.284524	956.951648	13.910733
17.000632	947.613864	13.915751
17.236842	944.806381	13.920768
16.982350	957.465845	13.925786
16.847811	957.221744	13.930803
16.979775	956.636353	13.935821
16.965065	959.125401	13.940839
16.984137	956.894512	13.945856
17.022927	963.963680	13.950874
17.363583	972.639463	13.955891
17.656845	972.865231	13.960909
17.647496	981.090592	13.965927
17.802870	975.796340	13.970944
17.029696	960.485165	13.975962
17.428451	974.589248	13.980979
17.693353	979.805510	13.985997
17.383049	980.112627	13.991015
17.490730	982.352254	13.996032
17.557979	992.992464	14.001050
17.665835	986.973473	14.006067
17.412176	972.957307	14.011085
17.388541	972.348806	14.016103
17.598068	975.882209	14.021120
17.666544	978.727531	14.026138
17.981974	976.084431	14.031155
17.773477	979.686074	14.036173
17.811881	987.313879	14.041191
17.798583	980.139816	14.046208
17.503131	979.384290	14.051226
17.580512	975.960915	14.056243
17.734571	971.585190	14.061261
17.510180	986.884503	14.066279
17.680799	982.092794	14.071296
17.101553	989.113034	14.076314
17.397721	976.257781	14.081331
17.711457	975.290645	14.086349
17.201632	991.170878	14.091367
17.638312	986.924713	14.096384
17.681538	1007.777517	14.101402
18.016867	1012.790323	14.106419
18.167293	995.375596	14.111437
18.311351	998.818213	14.116455
18.453756	997.233979	14.121472
17.829001	992.452496	14.126490
18.047619	991.272956	14.131507
18.098305	995.282365	14.136525
17.684276	996.981539	14.141543
18.005561	986.261966	14.146560
18.076816	1008.344304	14.151578
18.195166	1006.773282	14.156595
18.524225	1004.020760	14.161613
18.063293	990.084189	14.166631
17.887362	976.434609	14.171648
18.113217	988.994061	14.176666
18.194979	990.275221	14.181683
18.435946	990.354500	14.186701
17.815812	986.165581	14.191719
18.202489	987.235168	14.196736
17.969276	998.158843	14.201754
17.961346	1007.823017	14.206771
18.180759	1004.412236	14.211789
18.271488	1001.867232	14.216807
18.265014	994.938248	14.221824
18.065817	999.179065	14.226842
18.450696	1002.776689	14.231859
18.618863	995.195675	14.236877
18.316659	1006.871698	14.241895
18.002086	1008.233501	14.246912
18.461379	1003.437867	14.251930
18.363119	1006.302841	14.256947
18.507843	1000.505319	14.261965
18.226674	1001.107697	14.266983
18.373147	1002.713293	14.272000
18.355029	1005.821405	14.277018
18.414835	1000.355835	14.282035
18.371984	1000.132171	14.287053
18.223347	1005.210858	14.292071
18.310152	1011.581460	14.297088
18.441045	1026.607744	14.302106
18.329584	1025.520617	14.307123
18.485389	1019.150173	14.312141
18.427569	1025.139361	14.317159
18.460626	1023.367026	14.322176
18.735076	1028.300953	14.327194
18.065223	1028.215934	14.332211
18.959719	1023.197903	14.337229
18.476201	1023.437317	14.342247
18.534953	1023.286194	14.347264
18.312332	1019.224721	14.352282
18.797849	1028.673227	14.357299
18.405428	1030.116579	14.362317
18.811592	1037.958542	14.367335
19.062695	1038.500139	14.372352
18.830853	1044.330239	14.377370
19.272987	1048.420723	14.382387
19.257856	1032.300352	14.387405
18.862547	1020.281706	14.392423
18.957968	1020.109095	14.397440
19.022444	1018.555927	14.402458
19.007863	1029.338285	14.407475
19.239135	1018.670577	14.412493
19.095848	1016.468114	14.417511
18.839685	1011.730222	14.422528
18.952842	1012.851864	14.427546
18.544328	1012.921813	14.432563
19.086308	1016.106821	14.437581
18.987300	1036.925001	14.442599
19.290831	1040.771980	14.447616
19.026321	1033.703278	14.452634
19.193125	1040.178198	14.457651
19.403175	1036.472228	14.462669
18.972832	1026.759579	14.467687
18.582210	1032.513412	14.472704
19.137053	1033.272801	14.477722
18.840299	1042.385525	14.482739
19.445063	1047.615163	14.487757
19.171072	1047.752528	14.492775
19.098467	1039.063443	14.497792
19.316158	1038.884419	14.502810
18.951377	1042.974304	14.507827
18.827684	1037.707703	14.512845
19.063730	1053.187845	14.517863
18.963434	1046.443860	14.522880
19.491798	1061.259968	14.527898
19.250283	1071.471778	14.532915
19.426168	1069.617241	14.537933
19.483689	1066.370508	14.542951
19.345632	1065.464242	14.547968
19.239007	1061.971671	14.552986
19.494659	1066.028078	14.558003
19.672956	1065.337642	14.563021
19.561157	1065.351926	14.568039
19.501218	1069.378576	14.573056
19.757052	1070.935593	14.578074
19.566047	1072.252916	14.583091
19.584575	1057.216020	14.588109
19.791509	1071.072338	14.593127
19.644827	1068.605313	14.598144
20.178156	1072.211395	14.603162
19.756759	1063.201069	14.608179
19.739472	1054.601192	14.613197
19.429987	1049.843191	14.618215
19.792062	1065.707658	14.623232
19.805102	1066.349437	14.628250
18.973198	1069.729428	14.633267
19.202602	1067.926518	14.638285
19.102095	1074.215855	14.643303
19.132381	1082.046933	14.648320
20.007303	1081.775048	14.653338
20.185704	1094.341963	14.658355
20.046226	1088.367758	14.663373
19.873640	1081.275258	14.668391
19.891116	1085.444491	14.673408
20.391855	1083.053386	14.678426
20.262517	1093.137292	14.683443
19.765856	1083.744202	14.688461
19.604438	1073.128134	14.693479
19.795122	1088.274546	14.698496
20.197253	1095.422894	14.703514
20.037822	1105.628255	14.708531
19.974621	1104.423158	14.713549
19.872854	1101.901799	14.718567
19.728930	1101.826412	14.723584
20.088089	1102.363811	14.728602
19.739853	1102.430686	14.733619
19.882545	1094.074123	14.738637
20.040509	1105.618604	14.743655
19.896720	1096.296798	14.748672
20.048637	1095.995472	14.753690
20.107444	1100.650572	14.758707
20.217004	1117.731503	14.763725
20.523194	1121.821080	14.768743
20.383638	1123.909871	14.773760
20.644102	1106.162328	14.778778
20.375741	1109.356756	14.783795
20.513210	1097.340314	14.788813
20.548691	1094.141187	14.793831
20.230582	1100.000515	14.798848
20.602026	1103.758039	14.803866
20.630126	1100.787276	14.808883
20.571625	1098.943983	14.813901
20.509141	1097.372706	14.818919
20.331552	1097.507685	14.823936
20.619341	1090.091042	14.828954
20.117754	1098.244775	14.833971
20.350529	1093.550656	14.838989
20.625995	1106.503250	14.844007
20.365433	1121.246582	14.849024
20.697194	1123.145228	14.854042
20.589043	1120.564901	14.859059
20.509903	1120.028152	14.864077
20.625996	1115.279611	14.869095
20.865987	1123.516709	14.874112
21.117312	1115.496669	14.879130
21.209397	1115.801098	14.884147
20.443663	1102.896495	14.889165
20.714712	1103.094165	14.894183
20.582400	1111.215657	14.899200
21.044945	1109.335419	14.904218
20.646865	1118.454490	14.909235
20.632236	1114.370079	14.914253
20.949344	1119.496203	14.919271
20.814639	1118.721956	14.924288
20.845673	1108.599760	14.929306
20.901727	1125.174638	14.934323
20.822281	1120.548058	14.939341
21.259225	1122.414548	14.944359
21.072805	1123.324067	14.949376
21.139772	1115.294861	14.954394
21.075692	1127.817503	14.959411
21.141582	1115.528173	14.964429
20.977965	1119.141792	14.969447
20.769785	1127.019485	14.974464
20.777869	1117.907549	14.979482
20.814677	1127.444903	14.984499
20.954555	1126.214498	14.989517
21.248128	1122.621736	14.994535
20.887945	1126.057680	14.999552
21.021913	1110.781861	15.004570
20.961363	1122.657018	15.009587
21.134532	1121.749629	15.014605
21.384963	1130.695154	15.019623
21.000379	1148.089733	15.024640
21.331324	1136.232487	15.029658
21.508722	1135.415957	15.034675
21.352860	1138.908453	15.039693
21.653368	1141.966981	15.044711
21.783002	1143.057664	15.049728
21.517734	1126.382867	15.054746
21.098657	1115.933120	15.059763
21.395974	1131.571046	15.064781
21.880359	1135.604480	15.069799
21.734687	1133.250897	15.074816
21.664002	1124.567783	15.079834
21.340686	1116.043926	15.084851
21.119617	1113.361261	15.089869
21.377024	1115.195745	15.094887
21.066886	1136.532901	15.099904
21.443199	1136.755209	15.104922
21.300512	1139.119042	15.109939
21.232050	1135.822484	15.114957
21.536477	1134.250881	15.119975
21.507970	1142.958977	15.124992
21.696098	1137.571216	15.130010
21.832244	1141.239152	15.135027
21.579173	1150.831119	15.140045
21.775808	1158.140874	15.145063
21.699727	1163.883646	15.150080
22.229312	1162.166532	15.155098
21.804917	1163.204622	15.160115
21.716572	1164.831013	15.165133
22.132381	1161.304418	15.170151
21.901602	1166.711518	15.175168
21.997435	1160.161014	15.180186
22.078482	1174.204268	15.185203
21.952782	1167.177017	15.190221
21.878292	1164.392628	15.195239
21.732756	1165.829109	15.200256
22.206448	1161.965302	15.205274
22.080016	1165.806668	15.210291
22.150692	1171.734874	15.215309
22.325417	1162.802095	15.220327
22.074794	1170.487602	15.225344
22.208260	1170.539438	15.230362
21.778573	1164.421045	15.235379
21.835551	1165.895423	15.240397
21.944993	1166.326538	15.245415
21.657384	1171.676215	15.250432
21.942798	1181.411576	15.255450
21.826531	1166.206228	15.260467
21.805136	1170.308950	15.265485
22.242346	1172.503606	15.270503
22.569016	1192.498304	15.275520
22.397442	1192.783825	15.280538
22.283050	1186.225017	15.285555
22.050625	1196.419704	15.290573
22.592096	1188.887784	15.295591
22.796418	1195.789262	15.300608
22.775661	1190.493967	15.305626
22.538595	1186.027608	15.310643
22.662417	1187.412686	15.315661
22.561858	1183.755046	15.320679
22.217668	1181.918355	15.325696
22.634883	1185.201715	15.330714
22.622536	1188.738147	15.335731
22.333200	1194.331096	15.340749
22.931741	1194.288432	15.345767
22.468475	1189.058878	15.350784
22.453280	1185.037654	15.355802
22.579385	1186.987262	15.360819
22.158146	1191.543559	15.365837
22.302453	1183.593799	15.370855
22.501025	1187.245714	15.375872
22.551163	1190.431593	15.380890
22.643702	1197.309451	15.385907
22.442881	1208.635307	15.390925
23.142552	1210.255776	15.395943
22.861315	1216.323994	15.400960
22.984527	1214.868961	15.405978
23.008622	1214.562287	15.410995
22.955737	1220.938935	15.416013
23.060843	1216.791677	15.421031
22.940112	1216.068898	15.426048
22.769344	1218.162560	15.431066
23.033838	1214.164055	15.436083
22.829024	1218.513095	15.441101
23.111140	1216.250685	15.446119
23.173291	1225.762056	15.451136
23.204903	1217.050347	15.456154
23.155590	1221.198453	15.461171
23.108729	1214.670145	15.466189
23.283227	1207.476219	15.471207
23.114294	1213.593222	15.476224
23.213582	1213.173857	15.481242
23.184256	1200.006205	15.486259
22.759896	1219.780197	15.491277
23.267854	1210.233781	15.496295
23.150680	1210.520300	15.501312
23.150125	1216.977160	15.506330
23.008004	1218.848613	15.511347
22.947027	1234.356223	15.516365
23.470990	1224.864112	15.521383
23.642043	1238.880781	15.526400
23.579522	1238.237300	15.531418
23.727694	1242.225275	15.536435
23.217893	1240.070381	15.541453
23.412931	1243.950075	15.546471
23.384677	1243.815653	15.551488
23.148969	1240.693437	15.556506
23.882162	1239.190767	15.561523
23.440506	1238.618939	15.566541
23.662259	1248.067603	15.571559
23.843256	1242.624115	15.576576
23.935788	1244.386453	15.581594
23.767250	1232.398629	15.586611
23.620773	1240.203649	15.591629
23.677454	1238.213020	15.596647
23.807553	1235.595582	15.601664
23.616937	1244.464666	15.606682
23.688129	1232.903418	15.611699
23.283153	1244.687115	15.616717
23.425344	1236.911229	15.621735
23.242986	1245.081598	15.626752
23.555132	1257.148124	15.631770
23.885669	1262.360562	15.636787
23.839602	1271.772041	15.641805
23.993526	1277.296003	15.646823
24.202186	1281.511254	15.651840
24.246744	1277.259801	15.656858
24.061227	1272.296246	15.661875
23.965274	1283.365981	15.666893
24.515353	1267.605521	15.671911
24.263843	1273.000101	15.676928
24.136454	1272.552910	15.681946
24.367048	1273.299679	15.686963
24.156187	1277.555001	15.691981
24.380375	1270.378559	15.696999
24.286586	1276.477573	15.702016
24.279220	1272.830651	15.707034
24.301338	1260.661645	15.712051
24.426649	1270.399890	15.717069
24.159298	1261.516956	15.722087
24.500260	1262.981842	15.727104
24.413481	1265.535802	15.732122
24.498792	1263.143083	15.737139
24.138537	1270.773118	15.742157
24.289683	1270.096369	15.747175
24.338925	1263.745585	15.752192
24.227238	1263.744072	15.757210
24.328483	1272.665559	15.762227
24.430759	1276.102112	15.767245
24.497389	1271.313893	15.772263
24.468276	1269.049441	15.777280
24.306755	1266.325924	15.782298
24.730602	1262.981094	15.787315
24.400657	1264.070756	15.792333
24.553692	1266.457991	15.797351
24.645960	1271.742242	15.802368
24.491813	1279.920858	15.807386
24.709071	1273.995190	15.812403
24.730033	1283.588743	15.817421
25.134060	1282.692741	15.822439
24.917183	1298.764321	15.827456
24.684765	1287.562732	15.832474
24.761931	1282.649794	15.837491
24.957114	1291.588223	15.842509
25.266154	1293.626125	15.847527
25.363073	1285.547998	15.852544
24.621115	1272.298743	15.857562
24.748826	1277.451246	15.862579
24.895358	1280.874597	15.867597
24.943255	1290.467117	15.872615
24.844815	1291.545982	15.877632
24.908788	1294.638208	15.882650
25.077946	1288.720024	15.887667
25.085785	1291.855703	15.892685
25.040296	1301.393340	15.897703
25.143496	1295.930391	15.902720
24.972440	1288.335798	15.907738
24.996701	1285.561261	15.912755
24.873002	1295.688584	15.917773
24.891746	1295.398521	15.922791
25.122439	1294.239172	15.927808
25.055587	1315.721700	15.932826
25.502152	1319.742129	15.937843
25.557348	1320.295303	15.942861
25.525579	1308.806841	15.947879
25.742217	1313.099752	15.952896
25.434796	1298.422671	15.957914
25.412672	1298.211554	15.962931
25.235569	1289.241972	15.967949
25.579907	1302.982404	15.972967
25.443288	1309.665609	15.977984
25.628574	1320.016238	15.983002
25.783982	1313.383818	15.988019
25.581753	1310.417324	15.993037
25.652627	1306.120741	15.998055
25.826533	1301.823896	16.003072
25.330303	1312.488912	16.008090
25.374707	1299.139295	16.013107
24.894590	1306.652308	16.018125
25.394992	1304.961815	16.023143
25.713915	1303.908649	16.028160
25.440071	1307.154459	16.033178
25.619465	1307.912357	16.038195
25.730210	1322.629602	16.043213
25.761594	1327.412108	16.048231
26.347845	1330.381999	16.053248
26.136268	1337.559724	16.058266
26.302124	1331.623105	16.063283
25.747906	1320.812426	16.068301
25.835682	1325.677670	16.073319
26.437674	1325.167410	16.078336
26.266149	1327.485265	16.083354
26.079470	1317.573573	16.088371
26.008041	1316.145680	16.093389
26.063756	1327.845081	16.098407
26.226006	1328.905451	16.103424
25.962652	1331.262850	16.108442
26.177585	1332.340264	16.113459
26.349035	1329.107303	16.118477
26.271641	1331.060208	16.123495
26.032768	1326.565693	16.128512
26.208168	1329.542747	16.133530
26.345166	1325.955388	16.138547
26.596318	1327.061876	16.143565
26.395635	1333.827649	16.148583
26.970032	1328.016772	16.153600
26.265398	1339.291764	16.158618
26.226019	1327.204871	16.163635
26.531097	1327.122691	16.168653
26.275512	1338.738023	16.173671
26.823870	1334.556440	16.178688
26.496407	1326.184606	16.183706
26.636702	1333.320169	16.188723
26.567351	1335.003578	16.193741
26.438817	1331.501742	16.198759
26.493124	1326.349354	16.203776
26.304935	1330.572755	16.208794
26.319458	1329.532267	16.213811
26.887067	1339.220622	16.218829
26.708932	1341.719389	16.223847
26.836265	1336.088568	16.228864
26.564197	1352.878847	16.233882
26.621863	1358.537741	16.238899
27.331392	1358.430460	16.243917
27.186626	1359.601749	16.248935
27.310874	1345.176157	16.253952
26.587856	1337.639078	16.258970
26.986281	1336.624024	16.263987
26.969914	1340.290501	16.269005
26.890239	1344.452829	16.274023
27.040006	1351.454380	16.279040
27.068016	1355.076080	16.284058
27.186611	1348.537742	16.289075
26.847774	1358.853231	16.294093
26.893049	1363.428457	16.299111
27.052950	1359.569281	16.304128
26.914669	1361.878809	16.309146
26.833091	1365.571223	16.314163
27.265503	1360.498811	16.319181
26.877836	1360.309893	16.324199
27.129595	1355.499140	16.329216
27.392015	1364.853172	16.334234
27.226601	1373.330232	16.339251
27.516948	1373.644823	16.344269
27.587533	1381.040567	16.349287
27.704782	1374.843257	16.354304
26.943102	1372.803302	16.359322
27.633288	1375.043804	16.364339
27.989743	1376.531533	16.369357
27.689075	1370.998898	16.374375
27.566329	1357.627924	16.379392
27.361888	1358.227834	16.384410
27.417938	1375.670794	16.389427
27.312961	1376.567644	16.394445
27.301613	1386.014805	16.399463
27.760923	1376.526368	16.404480
27.918851	1383.454077	16.409498
27.728561	1379.264411	16.414515
27.726744	1376.702204	16.419533
27.652775	1381.851424	16.424551
27.865537	1379.792297	16.429568
27.886769	1384.358648	16.434586
27.561429	1388.410912	16.439603
27.899713	1381.989837	16.444621
27.499624	1379.921986	16.449639
28.155639	1378.472347	16.454656
27.858052	1390.289912	16.459674
28.016468	1397.097630	16.464691
27.989591	1393.138139	16.469709
27.684641	1405.789997	16.474727
28.069140	1392.018128	16.479744
28.194808	1398.909840	16.484762
28.414401	1396.016511	16.489779
28.343897	1400.003855	16.494797
28.015205	1404.987612	16.499815
28.127354	1394.028956	16.504832
28.524907	1395.832182	16.509850
28.406496	1397.731520	16.514867
28.370453	1399.706397	16.519885
28.248018	1395.973223	16.524903
28.097002	1386.769155	16.529920
28.180917	1393.159279	16.534938
28.555775	1398.456375	16.539955
28.415865	1392.264383	16.544973
28.375321	1395.546469	16.549991
28.432510	1397.885529	16.555008
28.072721	1396.871756	16.560026
28.186889	1404.961317	16.565043
28.629563	1414.426166	16.570061
28.586942	1421.861644	16.575079
28.962405	1418.041478	16.580096
28.717992	1417.779762	16.585114
29.111333	1408.131166	16.590131
28.932755	1408.518767	16.595149
28.744510	1415.200582	16.600167
28.768375	1408.301428	16.605184
28.837208	1423.479721	16.610202
28.763602	1419.991406	16.615219
29.025546	1416.621262	16.620237
28.584455	1430.285262	16.625255
28.959338	1421.639929	16.630272
28.892304	1431.941545	16.635290
28.729861	1421.221286	16.640307
28.920336	1416.069762	16.645325
28.832839	1424.973374	16.650343
28.806989	1419.173872	16.655360
29.051800	1423.348815	16.660378
29.063988	1422.062530	16.665395
29.099866	1409.092857	16.670413
29.014849	1423.083267	16.675431
28.928143	1420.783581	16.680448
28.868619	1443.000428	16.685466
29.468115	1445.576954	16.690483
29.639912	1446.146691	16.695501
29.836861	1454.769344	16.700519
29.631059	1427.519292	16.705536
29.459098	1421.297566	16.710554
29.318728	1413.458299	16.715571
29.616730	1408.728695	16.720589
29.212075	1418.565314	16.725607
29.212055	1420.531428	16.730624
29.666823	1434.459897	16.735642
29.574249	1436.200581	16.740659
29.846197	1433.131836	16.745677
29.632002	1428.223195	16.750695
29.660007	1435.063855	16.755712
29.507782	1443.879723	16.760730
29.483556	1445.306807	16.765747
29.593360	1444.595463	16.770765
29.637596	1446.762974	16.775783
29.981891	1429.396537	16.780800
29.980661	1436.775083	16.785818
30.010912	1440.620515	16.790835
29.660483	1439.905087	16.795853
29.987637	1438.651814	16.800871
30.275470	1434.381382	16.805888
29.988593	1438.241475	16.810906
29.955268	1426.869945	16.815923
29.866221	1434.596680	16.820941
29.710216	1437.079392	16.825959
29.889160	1430.193954	16.830976
30.131363	1434.243072	16.835994
29.788985	1437.521667	16.841011
30.033690	1434.214165	16.846029
30.317480	1439.954644	16.851047
30.172549	1442.946876	16.856064
30.243435	1444.614774	16.861082
30.437149	1459.066748	16.866099
30.507831	1449.171718	16.871117
29.937122	1447.165138	16.876135
30.269349	1458.209341	16.881152
30.614667	1468.513049	16.886170
30.828573	1459.684476	16.891187
30.882840	1453.332842	16.896205
30.650912	1442.632857	16.901223
30.599648	1435.502391	16.906240
30.450266	1428.797461	16.911258
30.288454	1421.302358	16.916275
30.429225	1439.249745	16.921293
30.038297	1454.546984	16.926311
30.310155	1461.277102	16.931328
30.519523	1457.034660	16.936346
30.298669	1452.190167	16.941363
30.649857	1446.906314	16.946381
30.225088	1461.909024	16.951399
30.529288	1474.712244	16.956416
30.890690	1482.561373	16.961434
30.469544	1488.392688	16.966451
30.838778	1484.639750	16.971469
30.612230	1479.638344	16.976487
30.919042	1483.371298	16.981504
31.194412	1489.494961	16.986522
31.200063	1480.547321	16.991539
31.556912	1475.486643	16.996557
30.976690	1478.177421	17.001575
31.075387	1478.733294	17.006592
31.188884	1488.808017	17.011610
31.135337	1488.595479	17.016627
31.162363	1485.848883	17.021645
31.082120	1480.670062	17.026663
31.055630	1479.784274	17.031680
31.587022	1471.723626	17.036698
31.105110	1477.665385	17.041715
31.294637	1479.759786	17.046733
31.313836	1473.214787	17.051751
31.164906	1476.936645	17.056768
31.298346	1482.823624	17.061786
31.545904	1489.633277	17.066803
31.842723	1504.378507	17.071821
31.731339	1498.633322	17.076839
31.665068	1482.182832	17.081856
31.704632	1476.594035	17.086874
31.632411	1478.883825	17.091891
31.524019	1468.650589	17.096909
31.599998	1485.143803	17.101927
31.699002	1493.636556	17.106944
31.989767	1493.982643	17.111962
31.861852	1507.616877	17.116979
31.763827	1499.310226	17.121997
32.192480	1506.479858	17.127015
31.867626	1502.705593	17.132032
31.872950	1496.762355	17.137050
31.750487	1499.066282	17.142067
32.080620	1493.571096	17.147085
32.284849	1491.058845	17.152103
31.693812	1498.273624	17.157120
32.267470	1507.225819	17.162138
32.041939	1509.807728	17.167155
32.210177	1507.452559	17.172173
32.044517	1503.161197	17.177191
32.268214	1499.336241	17.182208
31.895522	1507.227091	17.187226
31.933641	1506.451165	17.192243
32.138267	1497.160110	17.197261
31.821226	1497.853296	17.202279
31.562607	1500.131084	17.207296
32.356340	1509.292015	17.212314
32.162524	1526.041870	17.217331
32.474352	1529.366949	17.222349
32.342716	1525.647804	17.227367
32.383680	1529.870289	17.232384
32.665482	1522.277673	17.237402
32.880889	1514.300917	17.242419
32.806529	1518.301510	17.247437
32.780359	1524.257535	17.252455
32.943024	1517.444028	17.257472
33.146231	1510.352808	17.262490
32.936877	1525.041162	17.267507
33.040044	1517.728828	17.272525
32.647786	1513.229744	17.277543
32.346560	1513.074703	17.282560
32.657985	1521.269306	17.287578
32.454784	1528.142842	17.292595
32.506184	1526.885159	17.297613
32.897198	1518.698021	17.302631
32.511152	1532.558659	17.307648
32.956818	1524.946840	17.312666
32.806540	1544.186205	17.317683
32.766143	1543.324670	17.322701
33.181335	1547.706647	17.327719
32.973184	1556.998344	17.332736
33.162403	1548.167260	17.337754
32.949755	1545.502153	17.342771
33.261474	1551.187826	17.347789
33.072850	1543.226625	17.352807
33.065359	1551.799103	17.357824
33.412131	1539.964373	17.362842
32.981183	1546.150687	17.367859
33.141589	1545.993201	17.372877
33.277874	1557.096376	17.377895
33.335823	1570.316707	17.382912
33.639241	1563.960956	17.387930
33.736579	1563.816445	17.392947
34.060847	1562.361639	17.397965
33.901834	1554.821862	17.402983
33.453528	1550.826963	17.408000
33.943883	1550.037429	17.413018
33.398228	1550.273899	17.418035
33.743897	1557.320770	17.423053
33.978357	1564.040971	17.428071
34.083322	1570.020777	17.433088
34.053161	1541.203149	17.438106
34.040439	1546.128283	17.443123
33.877770	1546.753254	17.448141
34.145484	1541.690655	17.453159
33.968633	1544.599510	17.458176
34.424438	1540.870953	17.463194
33.872732	1541.449195	17.468211
33.591838	1548.511564	17.473229
33.790963	1550.011180	17.478247
33.780096	1563.624077	17.483264
33.753512	1562.498456	17.488282
34.042028	1565.211781	17.493299
34.069780	1565.074948	17.498317
34.129174	1568.780169	17.503335
33.877079	1570.189092	17.508352
34.232331	1563.415011	17.513370
34.136183	1579.569033	17.518387
34.574967	1582.091705	17.523405
34.439550	1584.861570	17.528423
34.872538	1587.650236	17.533440
34.774698	1584.740027	17.538458
34.459777	1577.764165	17.543475
34.635598	1592.099111	17.548493
34.470657	1590.641573	17.553511
34.261470	1593.022131	17.558528
34.635455	1586.194631	17.563546
34.229562	1588.438555	17.568563
34.497416	1579.888706	17.573581
34.735211	1596.827052	17.578599
34.460304	1585.070149	17.583616
34.690839	1590.664332	17.588634
34.507989	1586.757485	17.593651
34.623991	1595.462238	17.598669
34.848240	1598.876706	17.603687
34.949783	1606.785285	17.608704
35.266536	1606.256311	17.613722
35.541239	1613.083876	17.618739
35.225440	1597.599952	17.623757
35.137823	1591.346100	17.628775
34.778376	1585.349171	17.633792
35.216310	1588.720900	17.638810
35.273343	1606.126062	17.643827
35.565502	1603.909379	17.648845
35.264387	1593.475699	17.653863
35.059248	1600.797697	17.658880
35.373571	1597.220546	17.663898
35.546341	1609.321635	17.668915
35.171372	1601.872266	17.673933
35.435722	1601.616544	17.678951
35.334363	1618.784443	17.683968
35.307656	1608.926578	17.688986
35.475654	1615.606653	17.694003
35.731162	1612.941231	17.699021
35.575855	1605.252530	17.704039
35.666517	1606.491323	17.709056
35.677459	1599.360575	17.714074
35.718841	1598.902878	17.719091
35.606124	1606.507139	17.724109
35.749418	1608.084881	17.729127
35.444061	1611.477666	17.734144
35.552921	1609.456781	17.739162
35.369817	1622.304419	17.744179
35.976349	1631.371481	17.749197
36.174550	1633.442460	17.754215
36.080569	1633.930505	17.759232
36.101946	1634.788760	17.764250
36.052425	1634.856465	17.769267
36.027872	1631.590849	17.774285
36.027154	1632.174829	17.779303
35.930364	1633.149314	17.784320
36.313731	1628.728259	17.789338
36.622045	1628.620328	17.794355
36.222514	1632.453820	17.799373
36.066339	1621.798738	17.804391
35.815495	1630.532222	17.809408
36.182537	1634.817574	17.814426
36.391369	1639.783979	17.819443
36.461334	1643.083619	17.824461
36.922345	1644.561405	17.829479
36.744490	1642.632494	17.834496
36.422859	1630.257975	17.839514
36.435555	1633.301438	17.844531
36.313077	1644.820503	17.849549
36.808999	1649.799018	17.854567
36.431767	1651.359976	17.859584
36.777900	1651.290339	17.864602
36.750616	1651.136828	17.869619
37.060353	1653.742719	17.874637
37.077246	1645.399173	17.879655
36.881163	1656.412144	17.884672
37.052752	1642.231411	17.889690
37.144592	1656.721498	17.894707
36.693812	1649.324939	17.899725
36.936518	1647.469407	17.904743
36.805957	1651.425131	17.909760
36.901757	1647.733667	17.914778
36.851735	1650.300894	17.919795
37.122995	1644.139474	17.924813
37.272127	1647.082800	17.929831
37.196518	1652.724668	17.934848
37.192979	1648.048261	17.939866
36.954519	1655.526951	17.944883
37.290001	1668.852469	17.949901
37.526230	1674.606741	17.954919
37.519577	1676.157342	17.959936
37.673911	1670.837800	17.964954
37.592967	1665.558046	17.969971
37.391248	1669.670022	17.974989
38.005090	1668.406813	17.980007
37.629679	1669.099625	17.985024
37.533522	1675.647277	17.990042
37.774584	1673.233410	17.995059
37.714666	1672.504299	18.000077
37.719892	1670.821441	18.005095
37.587544	1680.701015	18.010112
37.274445	1668.363012	18.015130
37.749408	1672.723091	18.020147
37.538453	1672.219471	18.025165
37.918436	1666.662822	18.030183
37.762841	1668.312352	18.035200
37.798506	1675.653694	18.040218
38.024095	1676.394948	18.045235
38.040388	1693.194299	18.050253
38.431863	1690.520321	18.055271
37.980039	1699.742730	18.060288
38.445753	1693.743526	18.065306
38.483482	1696.316033	18.070323
38.386315	1700.607403	18.075341
38.225236	1696.122773	18.080359
38.302210	1692.888677	18.085376
38.460642	1699.680728	18.090394
38.536010	1694.528110	18.095411
38.296445	1705.068188	18.100429
38.352677	1686.881642	18.105447
38.102095	1696.154770	18.110464
38.096487	1692.195057	18.115482
38.387373	1689.539895	18.120499
38.361642	1697.181145	18.125517
38.799595	1694.332668	18.130535
38.935740	1709.784753	18.135552
39.119209	1706.054380	18.140570
39.088130	1700.233510	18.145587
38.913465	1702.397264	18.150605
38.789021	1695.827210	18.155623
38.964176	1692.902882	18.160640
38.886835	1694.739051	18.165658
39.025063	1695.124671	18.170675
39.125935	1708.013366	18.175693
39.148337	1705.968061	18.180711
39.432880	1710.443005	18.185728
39.375324	1684.251944	18.190746
39.266088	1689.592939	18.195763
39.064394	1693.865867	18.200781
39.036123	1689.057598	18.205799
39.474044	1708.508524	18.210816
39.480284	1711.849657	18.215834
39.791692	1706.420440	18.220851
39.560008	1699.699820	18.225869
39.265284	1683.524559	18.230887
39.267675	1697.558381	18.235904
39.328034	1709.383544	18.240922
39.197252	1710.145570	18.245939
39.572454	1710.522697	18.250957
39.796669	1706.748110	18.255975
39.733353	1714.310011	18.260992
39.576254	1715.543204	18.266010
39.760282	1711.976849	18.271027
39.612843	1710.993114	18.276045
39.795858	1697.482759	18.281063
39.603469	1708.368952	18.286080
39.364403	1716.198063	18.291098
39.892797	1717.387647	18.296115
39.681641	1733.102112	18.301133
39.985987	1735.383800	18.306151
40.015824	1730.011037	18.311168
39.810531	1729.509691	18.316186
39.983778	1732.755397	18.321203
39.941059	1742.520062	18.326221
40.112003	1730.491670	18.331239
40.169258	1731.423241	18.336256
40.105851	1728.690688	18.341274
40.164887	1726.702795	18.346291
39.896681	1735.947129	18.351309
40.466095	1746.809413	18.356327
40.822457	1753.659033	18.361344
40.752852	1766.744730	18.366362
40.959342	1752.460643	18.371379
40.744717	1749.028934	18.376397
41.161087	1738.051105	18.381415
40.776810	1726.535205	18.386432
40.549095	1725.128456	18.391450
40.790453	1716.144000	18.396467
40.705943	1713.932299	18.401485
40.758546	1724.808761	18.406503
40.895213	1729.174187	18.411520
40.695865	1739.868974	18.416538
41.175977	1739.718515	18.421555
41.108170	1744.718553	18.426573
40.964945	1729.103502	18.431591
41.336311	1738.869968	18.436608
41.102001	1739.749102	18.441626
41.187912	1736.813415	18.446643
41.076932	1745.427346	18.451661
41.076685	1741.220629	18.456679
41.323370	1736.334823	18.461696
41.247435	1744.763412	18.466714
41.397195	1745.175641	18.471731
41.108915	1739.836625	18.476749
41.182569	1736.830261	18.481767
41.410663	1737.059875	18.486784
40.955047	1739.100115	18.491802
41.168571	1752.009173	18.496819
41.348339	1765.516802	18.501837
41.194052	1768.819822	18.506855
41.444364	1757.107267	18.511872
41.135441	1761.415841	18.516890
41.529725	1763.399500	18.521907
41.732824	1774.924764	18.526925
41.836346	1775.034915	18.531943
41.804976	1784.974566	18.536960
41.964051	1794.120846	18.541978
42.021464	1785.332257	18.546995
41.755639	1788.311810	18.552013
42.131864	1788.578325	18.557031
41.856686	1791.878079	18.562048
41.933718	1791.310683	18.567066
42.205644	1793.663699	18.572083
42.229975	1784.981250	18.577101
42.497522	1785.832744	18.582119
42.383667	1788.009132	18.587136
42.363612	1778.525689	18.592154
42.007833	1780.556701	18.597171
42.273720	1779.382373	18.602189
42.214014	1782.288808	18.607207
42.920731	1789.844462	18.612224
42.687196	1798.575332	18.617242
42.579082	1780.076598	18.622259
42.588378	1784.790080	18.627277
42.419976	1779.763757	18.632295
42.891478	1788.933976	18.637312
42.848642	1806.200244	18.642330
43.093920	1804.988097	18.647347
42.675599	1795.494067	18.652365
42.700741	1804.216225	18.657383
42.652970	1795.437696	18.662400
42.887251	1813.225729	18.667418
43.031714	1810.552320	18.672435
42.997576	1808.496871	18.677453
43.095474	1812.587479	18.682471
42.982612	1809.998317	18.687488
43.014467	1809.570501	18.692506
43.007023	1803.297780	18.697523
42.895508	1806.136543	18.702541
43.003612	1797.939676	18.707559
43.509104	1804.548340	18.712576
43.289119	1806.274182	18.717594
43.440283	1822.052238	18.722611
43.583356	1820.878094	18.727629
43.548846	1830.041909	18.732647
43.734286	1827.507289	18.737664
43.298401	1830.478612	18.742682
43.783305	1824.820369	18.747699
43.739146	1828.699562	18.752717
43.283354	1821.246905	18.757735
43.670690	1821.956671	18.762752
43.324825	1825.747134	18.767770
43.902055	1817.149004	18.772787
43.851019	1826.230180	18.777805
43.573691	1819.715443	18.782823
43.960593	1825.998586	18.787840
43.324615	1837.938562	18.792858
43.884439	1839.782843	18.797875
44.307889	1850.573240	18.802893
43.858224	1851.599521	18.807911
44.301414	1851.770401	18.812928
43.968967	1856.941065	18.817946
44.351098	1846.899491	18.822963
44.391748	1845.769696	18.827981
44.600241	1846.942822	18.832999
44.680255	1847.252299	18.838016
44.198442	1845.875635	18.843034
44.518483	1843.077052	18.848051
44.498815	1846.071939	18.853069
44.374628	1841.546814	18.858087
44.371690	1850.203936	18.863104
44.505353	1872.340744	18.868122
44.575008	1870.707798	18.873139
44.844011	1880.840585	18.878157
45.154409	1875.310485	18.883175
45.090197	1871.192594	18.888192
44.888701	1872.063469	18.893210
44.670446	1863.485025	18.898227
44.968163	1876.046539	18.903245
44.859302	1868.874373	18.908263
45.408875	1862.369736	18.913280
45.073233	1867.938544	18.918298
45.107923	1872.957374	18.923315
45.113046	1874.900647	18.928333
45.418519	1867.035948	18.933351
45.303595	1857.450465	18.938368
44.961009	1868.786187	18.943386
45.224554	1869.739297	18.948403
45.154537	1866.114632	18.953421
45.333860	1865.341953	18.958439
45.678057	1875.803867	18.963456
45.338485	1889.020051	18.968474
45.246648	1885.424026	18.973491
45.403596	1892.203758	18.978509
45.557245	1893.609495	18.983527
45.508883	1894.989878	18.988544
45.405288	1892.891583	18.993562
45.633719	1893.739705	18.998579
45.365777	1889.612503	19.003597
45.385519	1898.660605	19.008615
45.885985	1912.127882	19.013632
46.336097	1913.642103	19.018650
45.998714	1909.863390	19.023667
46.099333	1911.722368	19.028685
45.637080	1913.331300	19.033703
46.569868	1910.661376	19.038720
46.027147	1915.006387	19.043738
46.199895	1910.924179	19.048755
46.158945	1912.445426	19.053773
46.384918	1919.066093	19.058791
46.634154	1902.035901	19.063808
46.295650	1909.691224	19.068826
46.168893	1901.966390	19.073843
46.714967	1912.513663	19.078861
47.077591	1914.133027	19.083879
46.921337	1901.050895	19.088896
46.715270	1903.364734	19.093914
46.445051	1899.086400	19.098931
46.720286	1900.394310	19.103949
46.944580	1900.968513	19.108967
47.370037	1904.765138	19.113984
46.895170	1909.150078	19.119002
46.662221	1903.016577	19.124019
46.778787	1903.339300	19.129037
46.798415	1917.531562	19.134055
47.303153	1903.008409	19.139072
47.233153	1918.802049	19.144090
47.233014	1922.503990	19.149107
47.362751	1915.083211	19.154125
46.905351	1922.160583	19.159143
47.247751	1915.057000	19.164160
47.161973	1929.486596	19.169178
47.410731	1915.552417	19.174195
47.620593	1919.979079	19.179213
47.107241	1925.439870	19.184231
47.503242	1921.660583	19.189248
47.778522	1932.502502	19.194266
47.804236	1947.135668	19.199283
47.870767	1942.776490	19.204301
47.998055	1949.447249	19.209319
47.830160	1942.543030	19.214336
47.656067	1932.430214	19.219354
47.845320	1946.435137	19.224371
47.905380	1940.050869	19.229389
48.238303	1957.678516	19.234407
48.190417	1951.478315	19.239424
48.275853	1945.437245	19.244442
48.017103	1943.227396	19.249459
48.187919	1948.572204	19.254477
47.964915	1952.261510	19.259495
48.007850	1947.846043	19.264512
47.783662	1943.216536	19.269530
47.874452	1949.340692	19.274547
48.240059	1952.480747	19.279565
48.137184	1976.090454	19.284583
48.566917	1970.484939	19.289600
48.535961	1976.173607	19.294618
48.458944	1982.699455	19.299635
48.628475	1972.441594	19.304653
48.344802	1979.886431	19.309671
48.724017	1980.184042	19.314688
48.841447	1982.842015	19.319706
48.863602	1978.300382	19.324723
48.697156	1975.337672	19.329741
48.565584	1975.954660	19.334759
48.389210	1984.512613	19.339776
48.651063	1994.845400	19.344794
48.776591	2003.113351	19.349811
49.243931	2000.115079	19.354829
49.201776	2000.197418	19.359847
49.188561	1997.554843	19.364864
49.544715	1994.592818	19.369882
49.216063	1996.644878	19.374899
49.656000	1984.318805	19.379917
49.453758	1994.155783	19.384935
49.871157	1984.575718	19.389952
49.954877	1992.231613	19.394970
49.398172	1992.883232	19.399987
49.519254	1978.833178	19.405005
49.348922	1984.710812	19.410023
49.649636	1982.101416	19.415040
49.974557	1983.243801	19.420058
49.729341	1985.601616	19.425075
49.919252	1989.103561	19.430093
49.880328	1989.990157	19.435111
49.968659	1982.436937	19.440128
49.979447	1986.519055	19.445146
49.537936	1990.024631	19.450163
49.991294	1988.912624	19.455181
49.817650	2005.473587	19.460199
50.063677	2008.767975	19.465216
50.388866	2013.650094	19.470234
50.288449	2006.258800	19.475251
50.271495	2004.680353	19.480269
50.118346	2011.038178	19.485287
50.194132	2012.112051	19.490304
50.497536	2006.478854	19.495322
50.729437	2023.273350	19.500339
51.054905	2023.752907	19.505357
50.301273	2012.912889	19.510375
51.141500	2020.315307	19.515392
50.785998	2023.469813	19.520410
50.360496	2023.602370	19.525427
51.078678	2024.109149	19.530445
50.949836	2026.319458	19.535463
51.051381	2030.393768	19.540480
51.446938	2026.450421	19.545498
51.388713	2033.658199	19.550515
51.405679	2018.756442	19.555533
51.435309	2009.097877	19.560551
50.905268	2007.296346	19.565568
51.070878	2004.244060	19.570586
51.217846	2018.378706	19.575603
51.391366	2021.100538	19.580621
51.443210	2028.799282	19.585639
51.455161	2029.270844	19.590656
51.459298	2024.208121	19.595674
51.458379	2024.337690	19.600691
51.897935	2028.176330	19.605709
51.481164	2038.848340	19.610727
51.500838	2035.632571	19.615744
51.436766	2030.375329	19.620762
51.354045	2025.644878	19.625779
51.470980	2026.731281	19.630797
51.953134	2035.593844	19.635815
51.875443	2046.030022	19.640832
51.781648	2057.674280	19.645850
51.785668	2056.692192	19.650867
52.281458	2051.966340	19.655885
51.995033	2050.366726	19.660903
52.061187	2054.459176	19.665920
52.200548	2053.452860	19.670938
52.272744	2049.736585	19.675955
52.248367	2044.618332	19.680973
52.386984	2047.238301	19.685991
52.202462	2044.076414	19.691008
52.129073	2048.260019	19.696026
52.107281	2066.192319	19.701043
53.004076	2061.599699	19.706061
52.807079	2061.153857	19.711079
53.195106	2054.961493	19.716096
53.308138	2067.277330	19.721114
53.151420	2064.947434	19.726131
53.206663	2036.772145	19.731149
52.892904	2029.549761	19.736167
52.868219	2025.261572	19.741184
53.427672	2038.378921	19.746202
53.170252	2042.048356	19.751219
52.914695	2034.081577	19.756237
53.097558	2038.430418	19.761255
52.954359	2048.185647	19.766272
53.407483	2054.398598	19.771290
53.136998	2062.605153	19.776307
53.412123	2058.166131	19.781325
53.648395	2064.731599	19.786343
53.442853	2053.152943	19.791360
53.168021	2051.453690	19.796378
53.462565	2055.636818	19.801395
53.304157	2048.349213	19.806413
53.641742	2060.519626	19.811431
53.665593	2076.103125	19.816448
53.945569	2077.997315	19.821466
53.545177	2089.039205	19.826483
54.048111	2073.241195	19.831501
53.761592	2078.026059	19.836519
54.135246	2083.692793	19.841536
54.129504	2067.601585	19.846554
54.137508	2073.830195	19.851571
54.123964	2076.334997	19.856589
54.157229	2075.013825	19.861607
54.160197	2072.075217	19.866624
53.880227	2077.868962	19.871642
53.936644	2099.298524	19.876659
54.440507	2096.184091	19.881677
54.663511	2116.031857	19.886695
54.501348	2106.844933	19.891712
54.766833	2106.510129	19.896730
54.527285	2112.486948	19.901747
54.502297	2110.300646	19.906765
54.406051	2108.671416	19.911783
54.277867	2115.760726	19.916800
54.724669	2118.162302	19.921818
54.779814	2128.880816	19.926835
54.894522	2135.067587	19.931853
55.059310	2139.438203	19.936871
55.192769	2135.702904	19.941888
55.107334	2125.064911	19.946906
55.203596	2131.371323	19.951923
55.266650	2135.893483	19.956941
55.204633	2126.523691	19.961959
55.137198	2141.244105	19.966976
55.600791	2145.558733	19.971994
55.421099	2155.606893	19.977011
55.632840	2159.073913	19.982029
55.468226	2147.731832	19.987047
55.208717	2146.165890	19.992064
55.443840	2145.412915	19.997082
55.258415	2163.721100	20.002099
55.679224	2152.691832	20.007117
55.804644	2158.621311	20.012135
55.511245	2157.489854	20.017152
55.636281	2167.607347	20.022170
55.894739	2175.984076	20.027187
56.213154	2172.841696	20.032205
56.362497	2181.380590	20.037223
55.940141	2180.540622	20.042240
56.514147	2176.115001	20.047258
56.502197	2174.576788	20.052275
56.228215	2176.513053	20.057293
56.345463	2171.849263	20.062311
56.114698	2170.944750	20.067328
56.465708	2171.455050	20.072346
56.523944	2178.774149	20.077363
56.083284	2177.125949	20.082381
56.450356	2180.789706	20.087399
56.265137	2195.689457	20.092416
56.817193	2194.546292	20.097434
56.821273	2202.637575	20.102451
56.659261	2198.061441	20.107469
56.876372	2192.072374	20.112487
57.085914	2203.360215	20.117504
57.121012	2213.340251	20.122522
56.739428	2221.816652	20.127539
57.157447	2217.443711	20.132557
57.520796	2210.810144	20.137575
57.754006	2218.591191	20.142592
57.604841	2208.417530	20.147610
57.652116	2217.988553	20.152627
57.976699	2212.992655	20.157645
58.152135	2205.694035	20.162663
57.644618	2199.855657	20.167680
57.466839	2187.259529	20.172698
57.497996	2201.273487	20.177715
57.682727	2208.307803	20.182733
57.837329	2204.193639	20.187751
57.978806	2211.149479	20.192768
58.066493	2210.877071	20.197786
58.099688	2211.408450	20.202803
57.659904	2213.774496	20.207821
57.959027	2209.883995	20.212839
57.782246	2215.816360	20.217856
58.287230	2208.769403	20.222874
58.135700	2209.096002	20.227891
57.869944	2228.997898	20.232909
58.470273	2235.222710	20.237927
57.887889	2247.416557	20.242944
58.305246	2243.517108	20.247962
58.210480	2243.629731	20.252979
58.046324	2247.186852	20.257997
58.412844	2267.567892	20.263015
58.559133	2270.032056	20.268032
58.946632	2263.423114	20.273050
59.051995	2272.483323	20.278067
58.844110	2270.710506	20.283085
58.555476	2261.536880	20.288103
58.667606	2264.546034	20.293120
58.834548	2266.539898	20.298138
58.856594	2282.527822	20.303155
59.075330	2282.913544	20.308173
59.376541	2287.038882	20.313191
58.993971	2292.132263	20.318208
59.620439	2283.927055	20.323226
59.348989	2283.142485	20.328243
59.423072	2282.714396	20.333261
59.735158	2270.647887	20.338279
59.628014	2274.347624	20.343296
59.735445	2273.286304	20.348314
60.195812	2280.012631	20.353331
59.802726	2288.175256	20.358349
59.810972	2282.161871	20.363367
59.447820	2284.976768	20.368384
59.718876	2278.004077	20.373402
59.889902	2289.790302	20.378419
59.937753	2299.919887	20.383437
60.365001	2297.413829	20.388455
60.255176	2307.116662	20.393472
60.336426	2304.541390	20.398490
60.402307	2309.186237	20.403507
60.267316	2308.500348	20.408525
60.603563	2300.068904	20.413543
60.338349	2305.838332	20.418560
60.759734	2300.521209	20.423578
60.957269	2302.693361	20.428595
60.446169	2308.494761	20.433613
60.352999	2306.053948	20.438631
60.553808	2314.076780	20.443648
60.768843	2320.800291	20.448666
60.829310	2330.072658	20.453683
60.837917	2332.103805	20.458701
61.310208	2324.822039	20.463719
61.092082	2330.697759	20.468736
61.300668	2335.569718	20.473754
61.520879	2333.225285	20.478771
61.072101	2330.688347	20.483789
61.289800	2325.030523	20.488807
61.118947	2328.721254	20.493824
61.485238	2323.703052	20.498842
61.629017	2323.709104	20.503859
61.116052	2321.049610	20.508877
61.550073	2329.376985	20.513895
61.563133	2348.585471	20.518912
61.593716	2347.712846	20.523930
61.856806	2355.609229	20.528947
61.661440	2349.958900	20.533965
61.901111	2349.104218	20.538983
61.907832	2359.824098	20.544000
61.790629	2357.983502	20.549018
62.321301	2357.948253	20.554035
62.037310	2374.327909	20.559053
61.985048	2376.229675	20.564071
62.153980	2384.939196	20.569088
62.317603	2379.466510	20.574106
62.375215	2378.416096	20.579123
62.251001	2379.906161	20.584141
62.524469	2373.674716	20.589159
62.334809	2382.481095	20.594176
62.624278	2385.939213	20.599194
62.992311	2379.794034	20.604211
62.695337	2384.081960	20.609229
63.071007	2385.538381	20.614247
63.084554	2395.436662	20.619264
63.396775	2394.870501	20.624282
63.085945	2384.961765	20.629299
63.087364	2392.816848	20.634317
63.643998	2385.764937	20.639335
63.481968	2394.039968	20.644352
63.509642	2388.298094	20.649370
63.952686	2385.644389	20.654387
63.756267	2373.328759	20.659405
63.546003	2364.972905	20.664423
63.673298	2367.802979	20.669440
63.597864	2361.101965	20.674458
63.802959	2358.207584	20.679475
63.424307	2365.282337	20.684493
63.556926	2378.845111	20.689511
63.468250	2379.171394	20.694528
63.977563	2378.249481	20.699546
63.841695	2383.803124	20.704563
63.658829	2375.383035	20.709581
64.435299	2381.069205	20.714599
63.882804	2386.687715	20.719616
63.969052	2386.090461	20.724634
64.321481	2394.269615	20.729651
64.240451	2403.033842	20.734669
64.194262	2408.611403	20.739687
64.154783	2406.540936	20.744704
64.229723	2403.546884	20.749722
64.432535	2400.517144	20.754739
64.248353	2414.397529	20.759757
64.320261	2419.177174	20.764775
64.560490	2427.048743	20.769792
64.769745	2428.666786	20.774810
65.069650	2427.723822	20.779827
64.844706	2436.964936	20.784845
64.982191	2434.169437	20.789863
64.878276	2427.984106	20.794880
64.829633	2449.159027	20.799898
65.246590	2449.510736	20.804915
65.184897	2454.238603	20.809933
65.489552	2451.492819	20.814951
65.432047	2453.190269	20.819968
65.241571	2457.635211	20.824986
65.537646	2453.877684	20.830003
65.350267	2458.757673	20.835021
65.445750	2468.769478	20.840039
65.786566	2475.378784	20.845056
65.822139	2472.438190	20.850074
65.920967	2473.410668	20.855091
66.145530	2475.843738	20.860109
66.357406	2467.516791	20.865127
66.451880	2469.499869	20.870144
66.257076	2471.054585	20.875162
66.286723	2469.490934	20.880179
66.121662	2471.637505	20.885197
66.568104	2469.683893	20.890215
66.078373	2468.210574	20.895232
66.239379	2467.121965	20.900250
66.417575	2482.113705	20.905267
66.310070	2497.430824	20.910285
66.565755	2496.418997	20.915303
66.637909	2494.507877	20.920320
66.382647	2495.750094	20.925338
67.079393	2490.929721	20.930355
67.007738	2499.329594	20.935373
67.487905	2497.064595	20.940391
67.114895	2499.041561	20.945408
67.257789	2489.494499	20.950426
67.677556	2496.852120	20.955443
67.592177	2487.586768	20.960461
67.604834	2489.001881	20.965479
67.689651	2484.857489	20.970496
67.545364	2489.711842	20.975514
67.647100	2478.028262	20.980531
67.367856	2488.960010	20.985549
67.337756	2495.923739	20.990567
67.659129	2508.712404	20.995584
67.414877	2506.105725	21.000602
67.945251	2512.470923	21.005619
67.534343	2521.823091	21.010637
68.070390	2501.661090	21.015655
68.122805	2508.656161	21.020672
68.001495	2514.381159	21.025690
68.180692	2518.392994	21.030707
68.079439	2530.613116	21.035725
68.274083	2533.237057	21.040743
68.344423	2527.043497	21.045760
68.192873	2531.457149	21.050778
68.677106	2528.336232	21.055795
68.241967	2530.771028	21.060813
68.976491	2532.083222	21.065831
68.710977	2524.745821	21.070848
68.488893	2530.824208	21.075866
68.567647	2534.744381	21.080883
69.058107	2542.476049	21.085901
69.058810	2544.707281	21.090919
69.215551	2543.174332	21.095936
69.300869	2549.574120	21.100954
69.734124	2542.579230	21.105971
69.658904	2546.349797	21.110989
69.282707	2550.842613	21.116007
69.501489	2544.534411	21.121024
69.464858	2541.895402	21.126042
69.499165	2544.055125	21.131059
69.112791	2543.032798	21.136077
69.165235	2548.045898	21.141095
69.697422	2554.000546	21.146112
69.853999	2571.612071	21.151130
70.059056	2570.305144	21.156147
69.895132	2575.089988	21.161165
70.250870	2570.471020	21.166183
70.094287	2568.911107	21.171200
70.065355	2572.257878	21.176218
69.822019	2563.749278	21.181235
69.965347	2592.036566	21.186253
70.195877	2591.098083	21.191271
70.678690	2592.752451	21.196288
70.809475	2595.881841	21.201306
70.935918	2584.604629	21.206323
70.239900	2592.435832	21.211341
70.669503	2593.817598	21.216359
70.835521	2591.907633	21.221376
70.692415	2596.534596	21.226394
71.094914	2602.096012	21.231411
70.882926	2618.549893	21.236429
70.910790	2625.473087	21.241447
71.242972	2616.653935	21.246464
71.148942	2615.494564	21.251482
71.557522	2608.894838	21.256499
71.231500	2610.956024	21.261517
71.214255	2614.660770	21.266535
71.616711	2616.245594	21.271552
71.679951	2628.960918	21.276570
72.052430	2623.793336	21.281587
71.975718	2634.179206	21.286605
72.039695	2631.950585	21.291623
72.126495	2628.547520	21.296640
72.311162	2618.419487	21.301658
72.237968	2619.204145	21.306675
72.076249	2623.423729	21.311693
72.108973	2622.336147	21.316711
72.222894	2620.923476	21.321728
72.176456	2629.133278	21.326746
71.997668	2621.949604	21.331763
72.406728	2619.525235	21.336781
72.123997	2622.876813	21.341799
72.337717	2632.472640	21.346816
72.740304	2644.705920	21.351834
72.875979	2647.465301	21.356851
72.942598	2659.410047	21.361869
72.771182	2664.420160	21.366887
72.989988	2650.373301	21.371904
72.738033	2656.958191	21.376922
72.910307	2651.307337	21.381939
72.714683	2652.562372	21.386957
72.876798	2652.903266	21.391975
72.949239	2667.315135	21.396992
73.341510	2679.657350	21.402010
73.421899	2668.551370	21.407027
73.437608	2676.691553	21.412045
73.515933	2678.052271	21.417063
73.818338	2667.647084	21.422080
73.636612	2672.535719	21.427098
73.687319	2673.540948	21.432115
73.801072	2689.786377	21.437133
73.640519	2696.802054	21.442151
74.021746	2698.093522	21.447168
74.011611	2709.172869	21.452186
73.960778	2700.940370	21.457203
73.889915	2696.207895	21.462221
74.216096	2716.507358	21.467239
74.336327	2714.449862	21.472256
74.513073	2725.301292	21.477274
74.590746	2721.337853	21.482291
74.483100	2717.687313	21.487309
74.600755	2728.267056	21.492327
74.750582	2721.969528	21.497344
74.582199	2725.615771	21.502362
75.144593	2720.150328	21.507379
74.980520	2720.093849	21.512397
74.837205	2739.456499	21.517415
75.095571	2742.727010	21.522432
75.106711	2744.183407	21.527450
75.119879	2738.803470	21.532467
75.196937	2738.636859	21.537485
75.151751	2737.712891	21.542503
75.383289	2750.165394	21.547520
75.603541	2758.248519	21.552538
75.734909	2751.240585	21.557555
75.878969	2763.107065	21.562573
75.664299	2759.258568	21.567591
76.307810	2754.922979	21.572608
76.216453	2761.454500	21.577626
76.301325	2764.903517	21.582643
76.089958	2757.870041	21.587661
75.746612	2766.340743	21.592679
76.491910	2768.399265	21.597696
76.380704	2772.506869	21.602714
76.314065	2774.076372	21.607731
76.548712	2782.665394	21.612749
76.505088	2790.376173	21.617767
76.924956	2781.963045	21.622784
76.866297	2785.320795	21.627802
76.713708	2782.175898	21.632819
76.896015	2784.262110	21.637837
76.782734	2791.235747	21.642855
76.910512	2784.566058	21.647872
76.685118	2792.327231	21.652890
76.986681	2806.495238	21.657907
77.544739	2814.421645	21.662925
77.115548	2818.389402	21.667943
77.545424	2804.716694	21.672960
77.799774	2810.253900	21.677978
77.413305	2809.386219	21.682995
77.531922	2806.498919	21.688013
77.370083	2812.233478	21.693031
77.542107	2804.950927	21.698048
77.776764	2828.704881	21.703066
77.735137	2830.283120	21.708083
77.917377	2838.918200	21.713101
78.075500	2844.258941	21.718119
77.888695	2839.411924	21.723136
78.151421	2835.893060	21.728154
78.020751	2833.170810	21.733171
78.251417	2844.380022	21.738189
78.292002	2851.948317	21.743207
78.576175	2856.852835	21.748224
78.920832	2856.467820	21.753242
78.681922	2856.833282	21.758259
78.681915	2862.836176	21.763277
78.657632	2858.377296	21.768295
78.886306	2856.467017	21.773312
78.535671	2867.103971	21.778330
78.991007	2877.782719	21.783347
79.131319	2875.340193	21.788365
79.053750	2887.863010	21.793383
79.330928	2873.832137	21.798400
79.558171	2881.415569	21.803418
79.553962	2879.143880	21.808435
79.665589	2882.329956	21.813453
79.268191	2886.207564	21.818471
79.679077	2891.922413	21.823488
79.666086	2905.290486	21.828506
79.968434	2897.798242	21.833523
80.103916	2907.797752	21.838541
79.526277	2913.792757	21.843559
80.116197	2900.988231	21.848576
80.151067	2914.427761	21.853594
79.849665	2925.164390	21.858611
80.485202	2927.397825	21.863629
80.209866	2933.898087	21.868647
80.366525	2932.974244	21.873664
80.230846	2925.941541	21.878682
80.393052	2944.073310	21.883699
81.087588	2943.132001	21.888717
81.067847	2944.129277	21.893735
81.138301	2943.278821	21.898752
81.134119	2946.085271	21.903770
81.409656	2944.751564	21.908787
81.824648	2940.337891	21.913805
81.380112	2939.056329	21.918823
81.928444	2935.029033	21.923840
81.744394	2941.770728	21.928858
81.847097	2939.498166	21.933875
82.076918	2937.868592	21.938893
82.103446	2941.263606	21.943911
81.936060	2940.551175	21.948928
82.237288	2940.438031	21.953946
81.903187	2944.293172	21.958963
81.850950	2933.520131	21.963981
81.704506	2951.434850	21.968999
81.770396	2933.198194	21.974016
82.311430	2930.084146	21.979034
82.024211	2931.691162	21.984051
82.155766	2943.774323	21.989069
82.279116	2950.244078	21.994087
82.341962	2951.780813	21.999104
82.734916	2959.587810	22.004122
82.337450	2959.312023	22.009139
82.639410	2958.378181	22.014157
82.948221	2967.261886	22.019175
82.778153	2971.912079	22.024192
82.757853	2977.018683	22.029210
82.676945	2979.111182	22.034227
83.123934	2979.562379	22.039245
82.984196	2984.917976	22.044263
83.215376	2990.193732	22.049280
83.335989	3000.214545	22.054298
83.251140	3002.919945	22.059315
83.541276	2998.478356	22.064333
83.454953	3012.470209	22.069351
83.639291	3009.222317	22.074368
83.812158	3011.171157	22.079386
83.671271	3019.894507	22.084403
84.158018	3028.286590	22.089421
84.010034	3038.800566	22.094439
84.157356	3034.106623	22.099456
84.331838	3030.045985	22.104474
84.217479	3031.897522	22.109491
84.220482	3024.183562	22.114509
84.470908	3040.152385	22.119527
84.096634	3051.645277	22.124544
84.504481	3049.132669	22.129562
84.589252	3052.578602	22.134579
84.477070	3047.082376	22.139597
84.727323	3067.245720	22.144615
84.811432	3079.285861	22.149632
84.721922	3079.978396	22.154650
84.693333	3083.489326	22.159667
85.063336	3077.337292	22.164685
85.088757	3092.141868	22.169703
85.296552	3093.517179	22.174720
85.707167	3095.309080	22.179738
85.175348	3103.929217	22.184755
85.562477	3098.165869	22.189773
85.605544	3118.948567	22.194791
85.992307	3118.197194	22.199808
86.258856	3118.815357	22.204826
85.953283	3126.115738	22.209843
86.203317	3124.268384	22.214861
86.224100	3131.457989	22.219879
86.271222	3126.596566	22.224896
86.067182	3126.268569	22.229914
86.195358	3143.831423	22.234931
86.547850	3137.426449	22.239949
86.458445	3153.088483	22.244967
86.426927	3151.123999	22.249984
86.963336	3153.009942	22.255002
86.530797	3149.946439	22.260019
86.791168	3162.495735	22.265037
86.870349	3170.708318	22.270055
87.127488	3175.396204	22.275072
87.414882	3173.672430	22.280090
87.308747	3173.184006	22.285107
87.222948	3174.576628	22.290125
87.566168	3183.511893	22.295143
88.142759	3183.942917	22.300160
88.615051	3182.565935	22.305178
88.326981	3173.884110	22.310195
88.498678	3147.175487	22.315213
88.502824	3154.282477	22.320231
88.645765	3164.984785	22.325248
88.242877	3152.221034	22.330266
88.305260	3145.065880	22.335283
88.717943	3142.520946	22.340301
88.266948	3147.281202	22.345319
88.354599	3153.311575	22.350336
88.629923	3147.505652	22.355354
88.348121	3149.380114	22.360371
88.292993	3159.352630	22.365389
88.817612	3175.846987	22.370407
88.752912	3187.216019	22.375424
88.700700	3180.451118	22.380442
88.484055	3188.220567	22.385459
88.975154	3190.501773	22.390477
89.126762	3204.185304	22.395495
89.187037	3201.673136	22.400512
89.364935	3202.336666	22.405530
89.186776	3212.678698	22.410547
89.749713	3204.075824	22.415565
89.697906	3210.825435	22.420583
89.653585	3219.069894	22.425600
90.088345	3224.339273	22.430618
90.023654	3231.838904	22.435635
90.418732	3221.532590	22.440653
90.307698	3222.714527	22.445671
90.345308	3223.835447	22.450688
90.387385	3232.060148	22.455706
90.367341	3224.251851	22.460723
90.362795	3225.221527	22.465741
90.476812	3226.204306	22.470759
90.494387	3231.472361	22.475776
90.609613	3247.998962	22.480794
90.673482	3258.612640	22.485811
90.617409	3260.638182	22.490829
90.561261	3257.680179	22.495847
90.739543	3266.559105	22.500864
90.941360	3271.135695	22.505882
91.136894	3287.637204	22.510899
91.040206	3275.093965	22.515917
91.290617	3284.693897	22.520935
91.365675	3296.666158	22.525952
91.880703	3300.499637	22.530970
91.893833	3296.053761	22.535987
91.774507	3296.924534	22.541005
92.045855	3297.156906	22.546023
92.156711	3298.903970	22.551040
92.162948	3292.634911	22.556058
92.325307	3310.909053	22.561075
92.297777	3313.154244	22.566093
92.596125	3320.758353	22.571111
92.367073	3320.617303	22.576128
92.674229	3313.171482	22.581146
92.674339	3320.010891	22.586163
92.748536	3325.153380	22.591181
92.845881	3323.345560	22.596199
92.784027	3329.446611	22.601216
93.279012	3333.172752	22.606234
93.012558	3341.117298	22.611251
93.313189	3336.244754	22.616269
93.430706	3351.401320	22.621287
93.306738	3344.874772	22.626304
93.424658	3343.616074	22.631322
93.375170	3347.010375	22.636339
93.799890	3353.985684	22.641357
94.034586	3367.012545	22.646375
93.531345	3372.314385	22.651392
94.234221	3377.886089	22.656410
93.756016	3378.449781	22.661427
94.074496	3375.089409	22.666445
94.246233	3384.234530	22.671463
94.317834	3389.652028	22.676480
94.456630	3397.322041	22.681498
94.438846	3397.608899	22.686515
94.292126	3389.113270	22.691533
94.394600	3403.350620	22.696551
94.443299	3407.742776	22.701568
94.864323	3413.348905	22.706586
94.848391	3420.408626	22.711603
94.885733	3415.652802	22.716621
95.155526	3414.512482	22.721639
95.137621	3411.621091	22.726656
95.474129	3420.750046	22.731674
95.432200	3435.114057	22.736691
95.748245	3432.779812	22.741709
95.749192	3431.529851	22.746727
95.518619	3441.693960	22.751744
96.015830	3433.069650	22.756762
95.867183	3434.841349	22.761779
95.980469	3436.439709	22.766797
96.093662	3435.655167	22.771815
95.977516	3458.602934	22.776832
96.612722	3445.137644	22.781850
96.574170	3453.176160	22.786867
96.649023	3456.794148	22.791885
96.515611	3460.599216	22.796903
96.651676	3455.556579	22.801920
96.766987	3446.262643	22.806938
96.616373	3457.525287	22.811955
96.884731	3476.796229	22.816973
96.983500	3476.206459	22.821991
97.511027	3479.450981	22.827008
97.071452	3472.234977	22.832026
97.361888	3479.212304	22.837043
97.605213	3480.976636	22.842061
97.587778	3471.157335	22.847079
97.489350	3493.736271	22.852096
97.962649	3502.367386	22.857114
97.952459	3511.843891	22.862131
97.758929	3504.583254	22.867149
97.957431	3497.627702	22.872167
97.963799	3507.562430	22.877184
98.199875	3504.151741	22.882202
98.270864	3520.846445	22.887219
98.178511	3520.368491	22.892237
98.755635	3518.088273	22.897255
98.368338	3520.503126	22.902272
98.823619	3521.978810	22.907290
98.867573	3533.937134	22.912307
99.466481	3538.344658	22.917325
99.616171	3540.912623	22.922343
98.920329	3545.619573	22.927360
99.495038	3539.403951	22.932378
99.419680	3542.571914	22.937395
99.369441	3550.457639	22.942413
99.474374	3542.462467	22.947431
99.291213	3544.400517	22.952448
99.439789	3552.618251	22.957466
99.711799	3565.232297	22.962483
99.446477	3564.266811	22.967501
99.435376	3560.809377	22.972519
99.572770	3594.600424	22.977536
100.368508	3587.917973	22.982554
100.041503	3595.695310	22.987571
100.343980	3590.576227	22.992589
100.614294	3607.441976	22.997607
100.487075	3624.514818	23.002624
100.521903	3615.593134	23.007642
100.685329	3615.498287	23.012659
100.728685	3622.024926	23.017677
100.961593	3633.082783	23.022695
100.934917	3657.569729	23.027712
101.151181	3639.046982	23.032730
101.295488	3645.327508	23.037747
101.234021	3644.447059	23.042765
101.487147	3641.374560	23.047783
101.398744	3661.007397	23.052800
101.680228	3669.008806	23.057818
101.585827	3666.208190	23.062835
101.620579	3666.420592	23.067853
101.396909	3672.815231	23.072871
101.722074	3686.904509	23.077888
101.893997	3689.061882	23.082906
102.755512	3693.267591	23.087923
102.544240	3697.318391	23.092941
102.941190	3685.884751	23.097959
102.634656	3686.712096	23.102976
102.475266	3692.424459	23.107994
102.509569	3696.957801	23.113011
102.800929	3715.789858	23.118029
103.238787	3712.142559	23.123047
103.292056	3711.888114	23.128064
103.136581	3713.405249	23.133082
103.471316	3712.851327	23.138099
103.358674	3709.962013	23.143117
103.882761	3721.618460	23.148135
103.959941	3734.704830	23.153152
103.988831	3736.590948	23.158170
104.303950	3731.431982	23.163187
104.146587	3732.232949	23.168205
104.303168	3729.153373	23.173223
104.274418	3730.199439	23.178240
104.412702	3733.346798	23.183258
104.680728	3730.208840	23.188275
104.523699	3727.986086	23.193293
105.029087	3721.232010	23.198311
104.794353	3727.934546	23.203328
104.758892	3732.137886	23.208346
105.254906	3731.088575	23.213363
105.213998	3730.148109	23.218381
105.522590	3728.638763	23.223399
105.564854	3749.968341	23.228416
105.411888	3748.388824	23.233434
105.808265	3757.786378	23.238451
105.647046	3750.899359	23.243469
105.660899	3741.371725	23.248487
105.796317	3750.254408	23.253504
105.907348	3751.240837	23.258522
105.883887	3751.118274	23.263539
105.573781	3753.735762	23.268557
106.208470	3765.321362	23.273575
105.959289	3770.975136	23.278592
106.205386	3774.272997	23.283610
106.173015	3771.655237	23.288627
106.237116	3786.735267	23.293645
106.447008	3794.227099	23.298663
106.628829	3791.781144	23.303680
106.366966	3805.905099	23.308698
106.825101	3832.933329	23.313715
106.967580	3830.689181	23.318733
107.148899	3816.202221	23.323751
107.088064	3831.162864	23.328768
107.515727	3851.776060	23.333786
107.696318	3849.011507	23.338803
107.781252	3848.518567	23.343821
107.734355	3848.219746	23.348839
107.643039	3855.281905	23.353856
107.698227	3840.072845	23.358874
108.032427	3849.158189	23.363891
107.612649	3860.040053	23.368909
108.018746	3872.677626	23.373927
108.325883	3876.224815	23.378944
108.660641	3888.046566	23.383962
108.768409	3877.383768	23.388979
108.450637	3887.624828	23.393997
108.759548	3882.065942	23.399015
109.007524	3884.394561	23.404032
108.870122	3880.764198	23.409050
108.684584	3892.143019	23.414067
108.823886	3901.388141	23.419085
109.374730	3907.463433	23.424103
109.288413	3910.087133	23.429120
109.472702	3905.062113	23.434138
109.922845	3914.299878	23.439155
109.971413	3928.798536	23.444173
109.976833	3925.660399	23.449191
109.855641	3932.380051	23.454208
109.941385	3934.544558	23.459226
110.353642	3929.095818	23.464243
110.048811	3929.701970	23.469261
110.416951	3936.143438	23.474279
110.429844	3950.136352	23.479296
110.322682	3957.879616	23.484314
110.744566	3958.413657	23.489331
110.852874	3964.851401	23.494349
110.818517	3961.713138	23.499367
111.096337	3973.647967	23.504384
111.189406	3984.046057	23.509402
111.210367	3980.621426	23.514419
110.833595	3977.760566	23.519437
111.434116	3988.000745	23.524455
111.452779	3998.366239	23.529472
111.796790	4008.160299	23.534490
111.834254	4005.304381	23.539507
111.909074	4016.488087	23.544525
112.273654	4026.632458	23.549543
112.296670	4027.225445	23.554560
112.429625	4030.563063	23.559578
112.602428	4026.063741	23.564595
112.382873	4030.403126	23.569613
112.427700	4035.064322	23.574631
112.557453	4042.025854	23.579648
112.649508	4051.887572	23.584666
113.108717	4046.002232	23.589683
112.921048	4052.438744	23.594701
113.377138	4061.776660	23.599719
113.350022	4070.672180	23.604736
113.501525	4072.845403	23.609754
113.932256	4060.191097	23.614771
114.023744	4067.123877	23.619789
114.190732	4066.343559	23.624807
114.152341	4063.572035	23.629824
113.793510	4070.155141	23.634842
114.090656	4077.024342	23.639859
114.143501	4094.306316	23.644877
114.226544	4099.308771	23.649895
114.498678	4094.610902	23.654912
114.365587	4104.378294	23.659930
115.063482	4106.378077	23.664947
114.981840	4123.813581	23.669965
114.975158	4126.273412	23.674983
115.436120	4121.170538	23.680000
115.287810	4123.949110	23.685018
115.255820	4113.295307	23.690035
115.203904	4121.961148	23.695053
115.388050	4119.587382	23.700071
115.492245	4136.394269	23.705088
115.621877	4142.535220	23.710106
115.889542	4144.425237	23.715123
115.821117	4146.332862	23.720141
115.820000	4146.216286	23.725159
116.231149	4168.246438	23.730176
116.489015	4175.835118	23.735194
116.633121	4165.005522	23.740211
116.520726	4171.231509	23.745229
116.621750	4172.781342	23.750247
116.697906	4165.257509	23.755264
116.841639	4169.073233	23.760282
116.758385	4178.182706	23.765299
117.002746	4186.051248	23.770317
116.921819	4181.951211	23.775335
117.118437	4183.293627	23.780352
116.988660	4204.606338	23.785370
117.424279	4205.289752	23.790387
117.876290	4214.678884	23.795405
117.998408	4216.815668	23.800423
117.860813	4222.114483	23.805440
118.000897	4227.884547	23.810458
118.489327	4232.233693	23.815475
118.537913	4241.354235	23.820493
118.488077	4245.004420	23.825511
118.666838	4242.498911	23.830528
118.538562	4238.352575	23.835546
118.951659	4237.249864	23.840563
118.983264	4234.994522	23.845581
119.233836	4236.861960	23.850599
119.200964	4248.715934	23.855616
119.246670	4247.556795	23.860634
119.429795	4255.788409	23.865651
119.457081	4252.331179	23.870669
119.304173	4256.814901	23.875687
119.695568	4253.351483	23.880704
119.570896	4269.799587	23.885722
119.694850	4280.243539	23.890739
119.510880	4283.759956	23.895757
120.206925	4292.277864	23.900775
120.222372	4304.373702	23.905792
120.376450	4309.106337	23.910810
120.716910	4304.006391	23.915827
120.824810	4309.560549	23.920845
120.631331	4310.064155	23.925863
120.979456	4329.200492	23.930880
121.503606	4330.135260	23.935898
121.327196	4326.441441	23.940915
121.532256	4322.457818	23.945933
121.211124	4320.557235	23.950951
121.738851	4320.326759	23.955968
121.497733	4330.988552	23.960986
122.001520	4344.848530	23.966003
121.946330	4351.933666	23.971021
121.816521	4360.472869	23.976039
121.999835	4344.804704	23.981056
122.069989	4355.276014	23.986074
122.209767	4369.363127	23.991091
122.397789	4378.285273	23.996109
122.374521	4379.055921	24.001127
122.347680	4380.130134	24.006144
122.611482	4394.898665	24.011162
122.875960	4399.333220	24.016179
123.048742	4404.732114	24.021197
123.265733	4410.894275	24.026215
123.831513	4425.038204	24.031232
123.697884	4425.816566	24.036250
124.209514	4414.806503	24.041267
124.019314	4416.231255	24.046285
123.954032	4415.910036	24.051303
124.093949	4413.681997	24.056320
123.946532	4410.810610	24.061338
123.957135	4410.565954	24.066355
124.439384	4428.163310	24.071373
124.568974	4441.671296	24.076391
124.795462	4433.978755	24.081408
124.722932	4449.648753	24.086426
124.978419	4438.921593	24.091443
125.131398	4442.009974	24.096461
124.784616	4438.784547	24.101479
125.175430	4436.719449	24.106496
125.054513	4452.494831	24.111514
125.372372	4465.452724	24.116531
125.430500	4467.470090	24.121549
125.227944	4466.655755	24.126567
125.686290	4476.031412	24.131584
125.756762	4489.933714	24.136602
125.915641	4492.345723	24.141619
125.991899	4485.478265	24.146637
126.002108	4506.340272	24.151655
126.450182	4505.039562	24.156672
126.323519	4523.322054	24.161690
126.228898	4525.640968	24.166707
126.640121	4521.902965	24.171725
126.654317	4539.497549	24.176743
126.994579	4531.392706	24.181760
126.868435	4535.376779	24.186778
127.368480	4557.605044	24.191795
127.519836	4556.031733	24.196813
127.678238	4563.462461	24.201831
127.961301	4553.412718	24.206848
127.580672	4566.327926	24.211866
127.794789	4561.140262	24.216883
127.982281	4579.045636	24.221901
127.768738	4591.859095	24.226919
128.325449	4590.374177	24.231936
128.521093	4599.036423	24.236954
128.522471	4611.039965	24.241971
128.548311	4615.612732	24.246989
128.533550	4619.042897	24.252007
128.494347	4621.312163	24.257024
128.391881	4637.823426	24.262042
128.822075	4639.997518	24.267059
129.274020	4647.006969	24.272077
129.348898	4662.152335	24.277095
129.927137	4664.031931	24.282112
129.760506	4669.638411	24.287130
129.740105	4671.731153	24.292147
130.169512	4683.399809	24.297165
129.974845	4688.612954	24.302183
130.697278	4694.693363	24.307200
130.436233	4696.208077	24.312218
130.620096	4696.567722	24.317235
130.887475	4711.263357	24.322253
130.483285	4710.546688	24.327271
130.872198	4712.522050	24.332288
130.972307	4717.843973	24.337306
131.082912	4717.145003	24.342323
131.577763	4732.887887	24.347341
131.742148	4729.002045	24.352359
131.984916	4730.258407	24.357376
131.971640	4723.660467	24.362394
132.259278	4727.359213	24.367411
132.674996	4722.143273	24.372429
132.142722	4727.989769	24.377447
132.321494	4727.627391	24.382464
132.707038	4724.155326	24.387482
132.624734	4723.650524	24.392499
132.659755	4735.314331	24.397517
132.832600	4745.309043	24.402535
132.891521	4733.340281	24.407552
132.648829	4750.971909	24.412570
132.970016	4744.678563	24.417587
133.233840	4762.856311	24.422605
133.414032	4777.622390	24.427623
133.721082	4782.495466	24.432640
133.713333	4786.233900	24.437658
134.199356	4780.934400	24.442675
133.959038	4776.489743	24.447693
133.712877	4783.731035	24.452711
133.873316	4788.169259	24.457728
133.862950	4800.348358	24.462746
134.336070	4808.449851	24.467763
134.577523	4824.106010	24.472781
134.652692	4835.893044	24.477799
134.672887	4826.947790	24.482816
134.508122	4838.222964	24.487834
134.859240	4846.933721	24.492851
134.905312	4857.671054	24.497869
135.172647	4861.559217	24.502887
135.217522	4875.544711	24.507904
135.731804	4877.686802	24.512922
135.538380	4878.263012	24.517939
135.651508	4878.084455	24.522957
135.849618	4885.894219	24.527975
136.146947	4889.256907	24.532992
136.327495	4904.386023	24.538010
136.461067	4902.673412	24.543027
136.521918	4918.288328	24.548045
136.438679	4923.499974	24.553063
136.844073	4924.620555	24.558080
137.040320	4928.885948	24.563098
136.825566	4949.019630	24.568115
137.214491	4947.147314	24.573133
137.549446	4941.138993	24.578151
137.986176	4946.967265	24.583168
138.077331	4964.215696	24.588186
138.396241	4966.344025	24.593203
138.478841	4967.978863	24.598221
138.480703	4968.963418	24.603239
138.540614	4962.076230	24.608256
138.399266	4963.086237	24.613274
138.480579	4969.004571	24.618291
138.605520	4970.228792	24.623309
138.545945	4989.495588	24.628327
138.679434	4989.238105	24.633344
139.345644	4991.261863	24.638362
139.455490	5000.218584	24.643379
139.413870	5002.396735	24.648397
139.394554	5012.371010	24.653415
139.450836	5019.372765	24.658432
139.728481	5021.905239	24.663450
139.774186	5034.659708	24.668467
140.132622	5033.246660	24.673485
140.037422	5038.207684	24.678503
139.798200	5046.316027	24.683520
140.557394	5058.729009	24.688538
140.433306	5065.427435	24.693555
140.827916	5065.460726	24.698573
140.706375	5085.030821	24.703591
141.066847	5078.478727	24.708608
141.446696	5089.000095	24.713626
140.763756	5094.759688	24.718643
141.217415	5107.595892	24.723661
141.181716	5118.680696	24.728679
141.733680	5116.287414	24.733696
141.974905	5133.702029	24.738714
141.732574	5147.378922	24.743731
142.479631	5144.727996	24.748749
142.154981	5150.431824	24.753767
142.495043	5160.536460	24.758784
142.464261	5167.346656	24.763802
142.700547	5169.402649	24.768819
143.112791	5170.323322	24.773837
142.994824	5168.413112	24.778855
143.592786	5177.773710	24.783872
143.417758	5179.186689	24.788890
143.167809	5186.280377	24.793907
143.621381	5198.232843	24.798925
143.336928	5206.316734	24.803943
143.586512	5202.954129	24.808960
143.779810	5213.772915	24.813978
143.656064	5231.547470	24.818995
143.917574	5226.576350	24.824013
144.019150	5236.250997	24.829031
144.226104	5244.141607	24.834048
144.867613	5257.106496	24.839066
144.722311	5276.923547	24.844083
145.050860	5273.914789	24.849101
145.075251	5268.342963	24.854119
145.128084	5274.117475	24.859136
145.417306	5287.948453	24.864154
145.495711	5294.984749	24.869171
145.788103	5293.493581	24.874189
145.958409	5301.961249	24.879207
145.790558	5313.186694	24.884224
146.136702	5308.360200	24.889242
146.130630	5317.511888	24.894259
146.333808	5316.063018	24.899277
146.644411	5334.833792	24.904295
146.675367	5329.608141	24.909312
147.059722	5333.064685	24.914330
146.803740	5337.242756	24.919347
147.114561	5351.730131	24.924365
147.248338	5364.382737	24.929383
147.480852	5361.373134	24.934400
147.878206	5364.502540	24.939418
147.861445	5389.043942	24.944435
148.483992	5380.493896	24.949453
148.303313	5381.008163	24.954471
147.908823	5382.849891	24.959488
148.322170	5388.432581	24.964506
148.594062	5408.484692	24.969523
148.926594	5407.792180	24.974541
148.709158	5411.446597	24.979559
148.890537	5418.949856	24.984576
149.127426	5423.878221	24.989594
149.283197	5429.977662	24.994611
149.893001	5429.384024	24.999629
149.871773	5431.628496	25.004647
149.694378	5433.701577	25.009664
150.028733	5448.403165	25.014682
150.380197	5454.983505	25.019699
150.675861	5450.385790	25.024717
150.224365	5462.700298	25.029735
150.427979	5453.328457	25.034752
150.736087	5469.404083	25.039770
150.362229	5486.226675	25.044787
150.657442	5480.177017	25.049805
151.265249	5500.697760	25.054823
151.297733	5511.238732	25.059840
151.605532	5504.192797	25.064858
151.555459	5504.235348	25.069875
151.899703	5509.431111	25.074893
151.873505	5526.537363	25.079911
151.893257	5536.445867	25.084928
151.877153	5537.856227	25.089946
152.342127	5540.094459	25.094963
152.332575	5551.500580	25.099981
152.940276	5570.746174	25.104999
152.376612	5567.816302	25.110016
152.756656	5557.886639	25.115034
152.538093	5565.070283	25.120051
152.856880	5578.619103	25.125069
152.931604	5590.883336	25.130087
152.946338	5592.219454	25.135104
153.165573	5601.879135	25.140122
153.379016	5622.480353	25.145139
153.846383	5629.566699	25.150157
153.843079	5636.606378	25.155175
154.192614	5641.924461	25.160192
153.951145	5643.366760	25.165210
154.457160	5659.575883	25.170227
154.505264	5656.847468	25.175245
154.809017	5674.372816	25.180263
155.116935	5682.074286	25.185280
155.509932	5682.612882	25.190298
155.317325	5686.648590	25.195315
155.979880	5679.629427	25.200333
156.043381	5681.829172	25.205351
156.093318	5691.477379	25.210368
156.171807	5690.868601	25.215386
156.196386	5695.403957	25.220403
156.383537	5697.366650	25.225421
156.253613	5698.176055	25.230439
156.183571	5713.982487	25.235456
156.745361	5719.832575	25.240474
156.873147	5728.010343	25.245491
157.123875	5725.389260	25.250509
157.458894	5737.505743	25.255527
157.698167	5751.164926	25.260544
157.587303	5748.505439	25.265562
157.696440	5747.137465	25.270579
157.886728	5748.604092	25.275597
158.135969	5769.278817	25.280615
158.314446	5768.272522	25.285632
158.777351	5764.412586	25.290650
158.541269	5766.621104	25.295667
158.417087	5775.194817	25.300685
158.869736	5779.442587	25.305703
158.866105	5791.412965	25.310720
159.283756	5783.087185	25.315738
159.536428	5801.611777	25.320755
159.461506	5816.696200	25.325773
159.719481	5814.774740	25.330791
159.616415	5814.058490	25.335808
160.063597	5822.612715	25.340826
160.536748	5827.788500	25.345843
160.614930	5826.728372	25.350861
161.100601	5823.338367	25.355879
160.611279	5838.099064	25.360896
161.178362	5834.244990	25.365914
160.977157	5829.797140	25.370931
160.911638	5840.833364	25.375949
161.189134	5855.064331	25.380967
161.155032	5862.733899	25.385984
161.504850	5858.528540	25.391002
161.652126	5873.723619	25.396019
161.653034	5890.093660	25.401037
161.941116	5889.357546	25.406055
162.038116	5907.988555	25.411072
162.065185	5904.979283	25.416090
162.337609	5917.162450	25.421107
162.482098	5917.613480	25.426125
162.725533	5933.014600	25.431143
162.379298	5942.674114	25.436160
162.879441	5947.571106	25.441178
163.026042	5966.901535	25.446195
163.189166	5970.083296	25.451213
163.733024	5971.195016	25.456231
163.498237	5993.047013	25.461248
163.787412	5994.624530	25.466266
163.657224	5994.666929	25.471283
163.765681	6010.281683	25.476301
164.053376	6007.758974	25.481319
164.389824	6026.668487	25.486336
164.630264	6030.097066	25.491354
165.070544	6041.569194	25.496371
165.194873	6040.628135	25.501389
165.314793	6040.164413	25.506407
165.366003	6057.754702	25.511424
165.466704	6067.919207	25.516442
165.763014	6067.636360	25.521459
165.689919	6066.868085	25.526477
165.999175	6086.687848	25.531495
165.939267	6092.060340	25.536512
166.097080	6089.400009	25.541530
165.875615	6100.646911	25.546547
166.397789	6109.631525	25.551565
167.003905	6120.800100	25.556583
166.824757	6138.754623	25.561600
167.158653	6133.257455	25.566618
167.235727	6136.342160	25.571635
167.299638	6147.569914	25.576653
167.736450	6156.791964	25.581671
167.689361	6166.474468	25.586688
167.931577	6187.109725	25.591706
168.241241	6192.431021	25.596723
168.280228	6191.897823	25.601741
168.839687	6204.835129	25.606759
169.080812	6214.605366	25.611776
169.264852	6213.617122	25.616794
169.279119	6216.317036	25.621811
169.539872	6208.653137	25.626829
170.057094	6207.025881	25.631847
169.883053	6224.386240	25.636864
170.012817	6222.850873	25.641882
170.112625	6222.185095	25.646899
170.152242	6223.602615	25.651917
170.479334	6234.505348	25.656935
170.355863	6249.130500	25.661952
170.568943	6252.743311	25.666970
170.512719	6258.232074	25.671988
171.088382	6269.579099	25.677005
171.405059	6265.590304	25.682023
171.354061	6275.816423	25.687040
171.718302	6273.606897	25.692058
171.558281	6283.035572	25.697076
171.796486	6298.652470	25.702093
172.079621	6302.705788	25.707111
172.010731	6300.367980	25.712128
171.902128	6316.275637	25.717146
172.306208	6326.591924	25.722164
172.391711	6336.140235	25.727181
172.874614	6343.268636	25.732199
173.085542	6349.050443	25.737216
173.200884	6352.403859	25.742234
173.712985	6368.953590	25.747252
173.608331	6379.740540	25.752269
173.848807	6380.981594	25.757287
173.737057	6393.553187	25.762304
174.030043	6395.452129	25.767322
174.226116	6404.636024	25.772340
174.335805	6406.888644	25.777357
174.594572	6406.204425	25.782375
174.736159	6427.878390	25.787392
174.487667	6429.410229	25.792410
174.853042	6432.860470	25.797428
175.229270	6452.471333	25.802445
175.272639	6453.446349	25.807463
175.221801	6464.420686	25.812480
175.338212	6462.429655	25.817498
175.603260	6477.638469	25.822516
175.698165	6483.788776	25.827533
175.858077	6496.627503	25.832551
176.336147	6505.095166	25.837568
176.337615	6514.782922	25.842586
176.762561	6524.246916	25.847604
176.940031	6538.124654	25.852621
177.108725	6536.823110	25.857639
177.263223	6559.849453	25.862656
177.519809	6560.968056	25.867674
177.227821	6567.121806	25.872692
177.765807	6579.415593	25.877709
178.300874	6588.351087	25.882727
178.434147	6587.083465	25.887744
178.512686	6599.013168	25.892762
178.789196	6605.428819	25.897780
178.869320	6621.462038	25.902797
179.133558	6618.406254	25.907815
178.995358	6619.905154	25.912832
178.878944	6636.451966	25.917850
179.368030	6640.230227	25.922868
179.455130	6649.800550	25.927885
180.000490	6649.071703	25.932903
179.967376	6665.027888	25.937920
179.869093	6675.902410	25.942938
180.436465	6689.984726	25.947956
180.269799	6691.507004	25.952973
180.861234	6702.390959	25.957991
180.826794	6709.874687	25.963008
181.172895	6717.453852	25.968026
181.653262	6720.071805	25.973044
181.548024	6741.216354	25.978061
181.905156	6737.221160	25.983079
181.915762	6736.976472	25.988096
182.069509	6733.915774	25.993114
182.434725	6745.415817	25.998132
182.559265	6750.279959	26.003149
182.917286	6746.647651	26.008167
182.855428	6748.421940	26.013184
183.219329	6766.406174	26.018202
183.230984	6770.697583	26.023220
183.419979	6775.655869	26.028237
183.734289	6771.307464	26.033255
183.686366	6782.010057	26.038272
183.936289	6799.680609	26.043290
184.340918	6788.199640	26.048308
184.333199	6802.570455	26.053325
184.604750	6812.929748	26.058343
184.905397	6824.357818	26.063360
184.823270	6829.443562	26.068378
185.157502	6825.262508	26.073396
185.361077	6841.286171	26.078413
185.618059	6848.052192	26.083431
185.437572	6853.247960	26.088448
185.400917	6855.318229	26.093466
185.853413	6856.150651	26.098484
186.015532	6863.521763	26.103501
186.133460	6869.633891	26.108519
186.258444	6884.953240	26.113536
186.274435	6898.758533	26.118554
186.731810	6905.666999	26.123572
186.896152	6925.709113	26.128589
187.355032	6924.261346	26.133607
187.105484	6932.577320	26.138624
187.407155	6932.981808	26.143642
187.907325	6946.727539	26.148660
187.464031	6956.156466	26.153677
188.111319	6961.280212	26.158695
188.471588	6973.071594	26.163712
188.557391	6976.259256	26.168730
188.747130	6973.322344	26.173748
188.639588	6982.809500	26.178765
188.946984	6991.878499	26.183783
189.095240	6995.744623	26.188800
189.140791	7005.413148	26.193818
189.771293	7008.819066	26.198836
189.670901	7025.186952	26.203853
189.599492	7018.887659	26.208871
189.917429	7032.766001	26.213888
189.912751	7049.611469	26.218906
190.389665	7059.392802	26.223924
190.456501	7075.055984	26.228941
190.633463	7080.777019	26.233959
190.999308	7094.048155	26.238976
191.301206	7099.784469	26.243994
192.046227	7093.676879	26.249012
192.004188	7118.922196	26.254029
192.051315	7129.932188	26.259047
192.351550	7120.386612	26.264064
192.298639	7116.669838	26.269082
192.507177	7131.556528	26.274100
192.576162	7145.918827	26.279117
192.521764	7152.023154	26.284135
192.937125	7172.600999	26.289152
193.172975	7173.299854	26.294170
193.263829	7174.520062	26.299188
193.381400	7187.561589	26.304205
193.675471	7203.183189	26.309223
194.008489	7223.925439	26.314240
193.811266	7228.558844	26.319258
194.399305	7230.487703	26.324276
194.271733	7245.369990	26.329293
194.747101	7246.284105	26.334311
195.260519	7260.959279	26.339328
194.896453	7269.792015	26.344346
195.185762	7273.336338	26.349364
195.389560	7299.632740	26.354381
195.796146	7305.681133	26.359399
196.166740	7318.673890	26.364416
196.017256	7319.824192	26.369434
196.397654	7323.265951	26.374452
196.288904	7341.580042	26.379469
196.574850	7344.149434	26.384487
196.677822	7348.095291	26.389504
197.066281	7377.778775	26.394522
197.735039	7381.535533	26.399540
197.574032	7394.390127	26.404557
197.387915	7401.408437	26.409575
197.733397	7408.148260	26.414592
197.906555	7420.635160	26.419610
198.452199	7425.648588	26.424628
198.430803	7431.214358	26.429645
198.759830	7440.914744	26.434663
199.162703	7453.760512	26.439680
198.797380	7466.163964	26.444698
198.977912	7474.387969	26.449716
199.502415	7484.247357	26.454733
199.590406	7493.123468	26.459751
200.191040	7506.484625	26.464768
200.259764	7515.385844	26.469786
200.182556	7515.969294	26.474804
200.066578	7527.124880	26.479821
200.095060	7540.556197	26.484839
200.804088	7550.873054	26.489856
200.292879	7574.117961	26.494874
200.991109	7570.088425	26.499892
201.026608	7594.091133	26.504909
201.345784	7601.463346	26.509927
201.645645	7605.318624	26.514944
201.661787	7622.461281	26.519962
202.320245	7623.741525	26.524980
202.502526	7646.875399	26.529997
202.624422	7645.502141	26.535015
202.825223	7652.990668	26.540032
202.933555	7667.618743	26.545050
203.348920	7673.258650	26.550068
203.583438	7681.783720	26.555085
203.832022	7689.776243	26.560103
204.492163	7692.628374	26.565120
203.954297	7696.421523	26.570138
204.302831	7702.428575	26.575156
204.506037	7716.880916	26.580173
204.647405	7713.793571	26.585191
205.210973	7732.423249	26.590208
205.306954	7745.866306	26.595226
205.333191	7744.959374	26.600244
205.376111	7752.624055	26.605261
205.424056	7766.071448	26.610279
205.953050	7779.608118	26.615296
206.029910	7804.548584	26.620314
206.305156	7803.729159	26.625332
206.273385	7815.923069	26.630349
206.831215	7828.277748	26.635367
207.078565	7832.330666	26.640384
207.267690	7847.561908	26.645402
207.416025	7859.216382	26.650420
207.250429	7868.608853	26.655437
207.644181	7879.836827	26.660455
208.191849	7887.063088	26.665472
207.636012	7900.459361	26.670490
207.883474	7913.061306	26.675508
208.318331	7934.726120	26.680525
208.469146	7943.990444	26.685543
208.874216	7951.415721	26.690560
209.243437	7965.921335	26.695578
209.557026	7977.221831	26.700596
209.745436	7988.753340	26.705613
210.083215	7995.538776	26.710631
210.544786	7995.668995	26.715648
210.662253	8011.934387	26.720666
210.803252	8019.224014	26.725684
210.604692	8025.426842	26.730701
210.801250	8041.421076	26.735719
211.372829	8045.562469	26.740736
211.116585	8061.860832	26.745754
211.297548	8072.241255	26.750772
211.801310	8081.286536	26.755789
212.279449	8094.932380	26.760807
212.426754	8099.670214	26.765824
212.296053	8098.961332	26.770842
212.721869	8109.843501	26.775860
212.621114	8120.280439	26.780877
213.064350	8136.337373	26.785895
213.283407	8136.009702	26.790912
213.533750	8153.564685	26.795930
213.780898	8165.525981	26.800948
213.924153	8175.369330	26.805965
214.038545	8185.807536	26.810983
214.211095	8188.628320	26.816000
214.430966	8210.639473	26.821018
214.607760	8204.118024	26.826036
214.790415	8217.541618	26.831053
214.790111	8230.561195	26.836071
214.951319	8243.656660	26.841088
214.743929	8262.804688	26.846106
215.344874	8271.787578	26.851124
215.820675	8284.565748	26.856141
216.113530	8302.051113	26.861159
216.515835	8307.121828	26.866176
216.468662	8319.732039	26.871194
216.928822	8331.486644	26.876212
217.190327	8336.999173	26.881229
217.274389	8352.894381	26.886247
217.268591	8359.357756	26.891264
217.587392	8372.030992	26.896282
217.973801	8378.515395	26.901300
218.113214	8392.195253	26.906317
218.013029	8405.126322	26.911335
218.504486	8409.286587	26.916352
218.683525	8429.094430	26.921370
219.074591	8427.338248	26.926388
219.497783	8449.491668	26.931405
219.262330	8463.343595	26.936423
219.637390	8467.711418	26.941440
220.049889	8477.872914	26.946458
220.345341	8493.814258	26.951476
220.531472	8491.524864	26.956493
220.712068	8503.941887	26.961511
221.244110	8514.678318	26.966528
221.123541	8517.232239	26.971546
221.421142	8539.364278	26.976564
221.924345	8542.733480	26.981581
221.521658	8548.892493	26.986599
222.171153	8556.684067	26.991616
222.184194	8574.042771	26.996634
222.347663	8573.856345	27.001652
222.698661	8583.348704	27.006669
222.435622	8593.950086	27.011687
223.523096	8606.323858	27.016704
223.732532	8617.558879	27.021722
223.654849	8624.851221	27.026740
223.856972	8632.952415	27.031757
223.888513	8644.552955	27.036775
224.189110	8647.006596	27.041792
224.604239	8658.989418	27.046810
224.997820	8657.576945	27.051828
225.079679	8660.127784	27.056845
225.150368	8680.524198	27.061863
225.725347	8680.949319	27.066880
226.098207	8683.536941	27.071898
226.158586	8679.615946	27.076916
226.354554	8691.686579	27.081933
226.510593	8707.223607	27.086951
226.980901	8699.374510	27.091968
226.803550	8708.276732	27.096986
226.706490	8723.935262	27.102004
227.253166	8733.684530	27.107021
227.357777	8751.076502	27.112039
227.630319	8751.447684	27.117056
227.752055	8763.905616	27.122074
227.778038	8780.204872	27.127092
228.218857	8780.837152	27.132109
228.552359	8805.230721	27.137127
228.712786	8810.711772	27.142144
228.900177	8820.681192	27.147162
228.992855	8832.411245	27.152180
229.570348	8832.324528	27.157197
229.212796	8843.622702	27.162215
229.753022	8854.515914	27.167232
229.644645	8859.637876	27.172250
230.170120	8882.489400	27.177268
230.322145	8891.937126	27.182285
230.578543	8908.768904	27.187303
230.751370	8911.065674	27.192320
231.442891	8932.660131	27.197338
231.251526	8940.267066	27.202356
231.532595	8946.919613	27.207373
231.491320	8961.849834	27.212391
231.844986	8967.326104	27.217408
231.952890	8983.915869	27.222426
232.141897	9004.142677	27.227444
232.385998	9013.475101	27.232461
232.526234	9039.228224	27.237479
232.775752	9053.563902	27.242496
232.681686	9071.359649	27.247514
233.212546	9101.004797	27.252532
233.581724	9107.990972	27.257549
233.482861	9124.253138	27.262567
234.290084	9139.158745	27.267584
234.265616	9161.562674	27.272602
234.516215	9170.742621	27.277620
234.875928	9187.890071	27.282637
235.078788	9205.668134	27.287655
235.264078	9218.785799	27.292672
235.912389	9221.548459	27.297690
236.183686	9252.254028	27.302708
236.579159	9248.817464	27.307725
236.900274	9259.710300	27.312743
236.837930	9269.911430	27.317760
236.766096	9280.903341	27.322778
236.913572	9290.257263	27.327796
237.727454	9298.295078	27.332813
238.087149	9324.478538	27.337831
237.984194	9324.737704	27.342848
238.198043	9332.316442	27.347866
238.005734	9359.558306	27.352884
238.801717	9370.661425	27.357901
238.857767	9382.470145	27.362919
239.112359	9385.388842	27.367936
239.075357	9405.253466	27.372954
239.305699	9414.945000	27.377972
239.792973	9429.294469	27.382989
239.558303	9456.726190	27.388007
240.171230	9461.805479	27.393024
240.733803	9475.792810	27.398042
240.720826	9502.176615	27.403060
240.946465	9509.292636	27.408077
241.441202	9529.055664	27.413095
241.836426	9536.839883	27.418112
242.060293	9556.919791	27.423130
242.191173	9561.168029	27.428148
242.520001	9568.208020	27.433165
242.495544	9588.020370	27.438183
242.842898	9596.317225	27.443200
243.382258	9606.882664	27.448218
243.044745	9616.571150	27.453236
243.603871	9635.541272	27.458253
243.717419	9644.281834	27.463271
244.135820	9651.945675	27.468288
244.154388	9671.309401	27.473306
244.507665	9694.946479	27.478324
244.805104	9698.218484	27.483341
245.053898	9697.769340	27.488359
245.334679	9706.752262	27.493376
245.500894	9721.871799	27.498394
245.532282	9726.937509	27.503412
246.065574	9737.882839	27.508429
246.735638	9730.813628	27.513447
247.087228	9727.658492	27.518464
247.303164	9728.300561	27.523482
247.520485	9747.788130	27.528500
247.789842	9755.014257	27.533517
247.862448	9760.253524	27.538535
248.037347	9762.076488	27.543552
248.073142	9768.173950	27.548570
248.395234	9783.142978	27.553588
248.470294	9789.253278	27.558605
248.684763	9794.116854	27.563623
248.801486	9800.365906	27.568640
248.890871	9806.931787	27.573658
249.144576	9828.131334	27.578676
249.602455	9841.184900	27.583693
249.893374	9862.006133	27.588711
249.781611	9873.449787	27.593728
250.089410	9896.892137	27.598746
250.657563	9915.829568	27.603764
250.607671	9929.795775	27.608781
250.825852	9941.364913	27.613799
251.404479	9957.121355	27.618816
251.643491	9973.685279	27.623834
251.459198	9989.364771	27.628852
252.094533	10003.637961	27.633869
252.070808	10011.926471	27.638887
252.541993	10037.547365	27.643904
252.850700	10048.698340	27.648922
252.918746	10067.982157	27.653940
253.201813	10069.633602	27.658957
253.517445	10093.261262	27.663975
253.606530	10107.922680	27.668992
254.341415	10117.223455	27.674010
254.531196	10145.152113	27.679028
254.898396	10152.325275	27.684045
255.164037	10160.369889	27.689063
255.057581	10176.173186	27.694080
255.658251	10186.606275	27.699098
255.729803	10212.794803	27.704116
256.316593	10200.696101	27.709133
256.277708	10220.685025	27.714151
256.677708	10233.533179	27.719168
256.730325	10245.797640	27.724186
256.752053	10254.565414	27.729204
257.154156	10265.563055	27.734221
257.291023	10291.031119	27.739239
257.479289	10296.100977	27.744256
257.721378	10312.304785	27.749274
257.587288	10338.430783	27.754292
258.290191	10347.733497	27.759309
258.635491	10364.691680	27.764327
259.141064	10374.006184	27.769344
259.540996	10389.784500	27.774362
259.455401	10418.864679	27.779380
259.875476	10419.828619	27.784397
260.117356	10437.955414	27.789415
260.052728	10453.139900	27.794432
260.831381	10462.276167	27.799450
260.975790	10476.518800	27.804468
261.137939	10491.238607	27.809485
261.281814	10505.266643	27.814503
261.782681	10525.718091	27.819520
261.910196	10523.882769	27.824538
262.071422	10544.087162	27.829556
262.261232	10554.211850	27.834573
262.560108	10564.723712	27.839591
262.788357	10587.219466	27.844608
263.201828	10587.278267	27.849626
263.321883	10612.992509	27.854644
263.494133	10621.853845	27.859661
264.323991	10626.634462	27.864679
264.120884	10638.610623	27.869696
264.862439	10656.271476	27.874714
265.089128	10665.196978	27.879732
265.123966	10668.936291	27.884749
265.737162	10681.776823	27.889767
265.834375	10687.899757	27.894784
265.954932	10685.860269	27.899802
265.783568	10713.110323	27.904820
266.002080	10721.699281	27.909837
266.154464	10737.121752	27.914855
266.483484	10758.203280	27.919872
266.796829	10778.958898	27.924890
266.774769	10798.254341	27.929908
267.329405	10812.648072	27.934925
267.744430	10834.234117	27.939943
268.426756	10853.732543	27.944960
268.637338	10868.555618	27.949978
268.669550	10885.253588	27.954996
269.049988	10889.548529	27.960013
269.267988	10908.585690	27.965031
269.631423	10922.491449	27.970048
269.782191	10933.875936	27.975066
269.884067	10951.008322	27.980084
270.408172	10963.986061	27.985101
270.541735	10986.238124	27.990119
270.448982	11007.366653	27.995136
271.413613	11018.769729	28.000154
271.339041	11041.635238	28.005172
271.860882	11048.873082	28.010189
272.238758	11058.305693	28.015207
272.687244	11076.347266	28.020224
272.908988	11088.548060	28.025242
272.812341	11103.763319	28.030260
272.957441	11118.142107	28.035277
273.531635	11122.567971	28.040295
273.364427	11142.562071	28.045312
273.740326	11155.528285	28.050330
273.950260	11184.929917	28.055348
274.393739	11195.441725	28.060365
274.508241	11207.447739	28.065383
274.428512	11229.708038	28.070400
275.653770	11246.438460	28.075418
275.694425	11259.523246	28.080436
275.773038	11270.322400	28.085453
275.962935	11295.496243	28.090471
276.840174	11309.221258	28.095488
276.869054	11323.381483	28.100506
277.296607	11330.012081	28.105524
277.614316	11334.799995	28.110541
278.010707	11347.036919	28.115559
277.958728	11359.173149	28.120576
278.469071	11381.098632	28.125594
278.458193	11389.799391	28.130612
278.835395	11392.471976	28.135629
279.418523	11411.386496	28.140647
279.645121	11420.315532	28.145664
279.520876	11432.930377	28.150682
279.630212	11454.419483	28.155700
279.593500	11472.622231	28.160717
280.133348	11481.780393	28.165735
280.541333	11503.374624	28.170752
280.726667	11525.698207	28.175770
280.796042	11533.360330	28.180788
280.957253	11559.407325	28.185805
281.460952	11575.157859	28.190823
281.657712	11593.040193	28.195840
281.854756	11599.438381	28.200858
282.016256	11621.914196	28.205876
282.158470	11646.789649	28.210893
282.529976	11661.938791	28.215911
282.873535	11678.617415	28.220928
283.067626	11698.843199	28.225946
283.353645	11725.931947	28.230964
283.529482	11743.925042	28.235981
284.308675	11756.456289	28.240999
284.434093	11786.029902	28.246016
284.846474	11787.080371	28.251034
285.542249	11820.474365	28.256052
285.205855	11836.125402	28.261069
285.939286	11849.008017	28.266087
286.272515	11868.593430	28.271104
286.712216	11882.222790	28.276122
287.207122	11887.122195	28.281140
287.554439	11893.945471	28.286157
287.867410	11898.396402	28.291175
287.922352	11921.871188	28.296192
288.298917	11917.294023	28.301210
288.674076	11938.006571	28.306228
288.840283	11952.578487	28.311245
288.945326	11963.187625	28.316263
289.016469	11981.446700	28.321280
289.638739	11994.703535	28.326298
290.054737	12002.027697	28.331316
290.331199	12006.939039	28.336333
290.598188	12022.878370	28.341351
290.873145	12033.798963	28.346368
291.076801	12050.967031	28.351386
291.239532	12056.012925	28.356404
291.536032	12077.577810	28.361421
291.857193	12091.563647	28.366439
292.135384	12111.003156	28.371456
291.868172	12128.689832	28.376474
292.351205	12142.164225	28.381492
292.817478	12172.462168	28.386509
293.096273	12178.282602	28.391527
293.274169	12195.814789	28.396544
293.677970	12218.986178	28.401562
294.186478	12245.093732	28.406580
293.896946	12258.824266	28.411597
294.315604	12274.973867	28.416615
294.701299	12293.263216	28.421632
294.851619	12316.502608	28.426650
295.398254	12341.284442	28.431668
295.548108	12364.814474	28.436685
295.950983	12377.433146	28.441703
296.224900	12403.078524	28.446720
296.576474	12413.624273	28.451738
296.997723	12431.241944	28.456756
297.355605	12455.718596	28.461773
297.963949	12471.624111	28.466791
298.464716	12478.559493	28.471808
299.001369	12482.012633	28.476826
299.090655	12487.540579	28.481844
299.086788	12505.552907	28.486861
299.561839	12502.273885	28.491879
299.712739	12523.505125	28.496896
299.951858	12533.345328	28.501914
300.638296	12541.429664	28.506932
300.252655	12563.900213	28.511949
300.987049	12566.839449	28.516967
300.562583	12583.685813	28.521984
301.173664	12594.781761	28.527002
301.378700	12605.145178	28.532020
301.269796	12630.720998	28.537037
301.853352	12652.983924	28.542055
301.813276	12665.706486	28.547072
302.005903	12691.257548	28.552090
302.473576	12708.956669	28.557108
302.571737	12736.341373	28.562125
303.135998	12758.885312	28.567143
303.512441	12788.437210	28.572160
303.533043	12806.746004	28.577178
304.276831	12823.890686	28.582196
304.649476	12846.057208	28.587213
305.012489	12851.523699	28.592231
305.408645	12880.832680	28.597248
305.587903	12895.665392	28.602266
306.132742	12913.400059	28.607284
306.243102	12940.366330	28.612301
306.602281	12941.519884	28.617319
307.010474	12959.604280	28.622336
307.628267	12977.011868	28.627354
308.140021	12987.286694	28.632372
307.884002	12995.388481	28.637389
308.094681	13015.246793	28.642407
308.325869	13037.972392	28.647424
308.683501	13056.784736	28.652442
309.181410	13071.419560	28.657460
309.154608	13096.768496	28.662477
309.645992	13108.612843	28.667495
309.980413	13133.390865	28.672512
309.865129	13150.309595	28.677530
310.249011	13163.298061	28.682548
310.443444	13197.884116	28.687565
310.774650	13224.172209	28.692583
311.306780	13246.374371	28.697600
311.775577	13271.936908	28.702618
312.428403	13285.461477	28.707636
312.579639	13295.123130	28.712653
312.969170	13309.456068	28.717671
313.401002	13335.952859	28.722688
314.029145	13347.902381	28.727706
314.088706	13366.224599	28.732724
314.205576	13373.330606	28.737741
314.750789	13389.511989	28.742759
314.734214	13408.963992	28.747776
314.746379	13429.592589	28.752794
315.479439	13442.378466	28.757812
315.519721	13462.652197	28.762829
315.913854	13471.429811	28.767847
316.737552	13498.838455	28.772864
316.677162	13512.363696	28.777882
316.946896	13522.032281	28.782900
317.303261	13554.114824	28.787917
317.901634	13563.116475	28.792935
317.899976	13585.490560	28.797952
318.326244	13595.305340	28.802970
318.647552	13611.445981	28.807988
318.672775	13627.796943	28.813005
319.053917	13651.652575	28.818023
319.232676	13680.785062	28.823040
319.510122	13696.016805	28.828058
320.065324	13717.941191	28.833076
320.545835	13746.881537	28.838093
320.723523	13768.523696	28.843111
320.926180	13782.188181	28.848128
321.523212	13798.178686	28.853146
321.692336	13805.478829	28.858164
321.467029	13839.041909	28.863181
322.140921	13845.183463	28.868199
322.356278	13865.139836	28.873216
322.356644	13888.173976	28.878234
322.703459	13903.840360	28.883252
323.416134	13926.198376	28.888269
323.843495	13948.840843	28.893287
324.095091	13974.681309	28.898304
324.225925	13987.700265	28.903322
325.083788	14009.369443	28.908340
325.155961	14033.519980	28.913357
325.467698	14042.275950	28.918375
326.208278	14070.506809	28.923392
326.372116	14080.252167	28.928410
326.793390	14098.382988	28.933428
326.480836	14112.026864	28.938445
326.816365	14128.869967	28.943463
327.214633	14152.549874	28.948480
327.902505	14178.089004	28.953498
328.366199	14190.389938	28.958516
328.341356	14210.532496	28.963533
328.867161	14218.295184	28.968551
329.054566	14254.561169	28.973568
329.370345	14275.159208	28.978586
330.061348	14296.166243	28.983604
330.332980	14308.500312	28.988621
330.867154	14326.727464	28.993639
330.934863	14337.116369	28.998656
330.901171	14357.184667	29.003674
331.630287	14381.195475	29.008692
331.741614	14390.418617	29.013709
331.980494	14416.877484	29.018727
332.530558	14443.799547	29.023744
332.781267	14457.734946	29.028762
332.949611	14480.746812	29.033780
333.432115	14509.406945	29.038797
333.648371	14531.445044	29.043815
334.094394	14551.925207	29.048832
334.653511	14574.671075	29.053850
334.909678	14590.756372	29.058868
335.136810	14616.096227	29.063885
335.386486	14643.024283	29.068903
335.645604	14658.992330	29.073920
335.866676	14678.468638	29.078938
336.572668	14698.665314	29.083956
336.639967	14736.214154	29.088973
337.087462	14753.334084	29.093991
337.715493	14777.228490	29.099008
337.705542	14800.344294	29.104026
338.021585	14812.949691	29.109044
338.554070	14836.312693	29.114061
338.909491	14850.456305	29.119079
339.384676	14867.022513	29.124096
340.017280	14886.924477	29.129114
340.417698	14895.869156	29.134132
340.718485	14906.664224	29.139149
340.840243	14928.010073	29.144167
341.318808	14937.823725	29.149184
341.373542	14961.539175	29.154202
342.167778	14978.292670	29.159220
342.174782	15005.612730	29.164237
342.141557	15020.034886	29.169255
342.812120	15038.336233	29.174272
342.745192	15059.354733	29.179290
343.349763	15071.324808	29.184308
343.415692	15109.263049	29.189325
343.773909	15121.903142	29.194343
344.513465	15133.912247	29.199360
344.749781	15155.041551	29.204378
344.703643	15173.233533	29.209396
344.975324	15197.932434	29.214413
345.383810	15222.452159	29.219431
346.398843	15234.453181	29.224448
346.456635	15246.701140	29.229466
346.781351	15268.969546	29.234484
347.090770	15286.503068	29.239501
347.372601	15306.753793	29.244519
347.638166	15316.926096	29.249536
348.021186	15344.854483	29.254554
348.254375	15363.252658	29.259572
348.448983	15383.441246	29.264589
348.047442	15418.894729	29.269607
348.484754	15441.663755	29.274624
348.866652	15475.264671	29.279642
349.452029	15504.462976	29.284660
349.376016	15540.222885	29.289677
350.328611	15569.651520	29.294695
350.950545	15602.833144	29.299712
351.082173	15623.723447	29.304730
351.545020	15652.821041	29.309748
352.025880	15682.298026	29.314765
352.099690	15703.412178	29.319783
353.021417	15726.084021	29.324800
353.104996	15763.635505	29.329818
353.955670	15776.392020	29.334836
353.955460	15799.725437	29.339853
353.966471	15818.177589	29.344871
354.709980	15837.564272	29.349888
355.373842	15860.364852	29.354906
355.452361	15883.840871	29.359924
356.044952	15904.435478	29.364941
356.093844	15928.494131	29.369959
356.770834	15961.023513	29.374976
356.723298	15987.146993	29.379994
357.770323	15990.104434	29.385012
358.335295	16014.774522	29.390029
358.314493	16026.400395	29.395047
359.082949	16048.606945	29.400064
359.457293	16063.313851	29.405082
359.788364	16070.561227	29.410100
360.287347	16086.960559	29.415117
360.323155	16099.288286	29.420135
360.885250	16106.171244	29.425152
360.858162	16126.944680	29.430170
361.158637	16143.356015	29.435188
361.469192	16168.514393	29.440205
361.506553	16188.229293	29.445223
362.210467	16203.352434	29.450240
362.235366	16228.504829	29.455258
362.590594	16253.618464	29.460276
363.052132	16274.685518	29.465293
363.357550	16304.130765	29.470311
363.567359	16320.932212	29.475328
364.457216	16333.364007	29.480346
364.830309	16350.165326	29.485364
365.591247	16371.400645	29.490381
365.783968	16382.980858	29.495399
366.515026	16390.958838	29.500416
366.735212	16412.496315	29.505434
366.776331	16427.482782	29.510452
367.319737	16447.583449	29.515469
367.342101	16463.675141	29.520487
367.566179	16477.644588	29.525504
367.661240	16510.878228	29.530522
368.107108	16532.687070	29.535540
368.577150	16550.907386	29.540557
368.510783	16573.999371	29.545575
369.100861	16589.210025	29.550592
369.327554	16618.513249	29.555610
369.034392	16646.773053	29.560628
369.475408	16662.445991	29.565645
369.547575	16702.922629	29.570663
370.659801	16725.095398	29.575680
370.917366	16768.038471	29.580698
371.234725	16781.121888	29.585716
371.719120	16812.409848	29.590733
372.607706	16845.021494	29.595751
372.823055	16858.474592	29.600768
372.858457	16885.110683	29.605786
373.439005	16908.487689	29.610804
374.130290	16934.181590	29.615821
374.216290	16966.056128	29.620839
374.916603	16981.622633	29.625856
375.210298	17002.858748	29.630874
375.723504	17029.657540	29.635892
376.167879	17053.633924	29.640909
376.272302	17075.648147	29.645927
376.565925	17100.245013	29.650944
377.098138	17119.659576	29.655962
377.358754	17141.529535	29.660980
377.810341	17177.431448	29.665997
378.155307	17191.647909	29.671015
378.936067	17217.464075	29.676032
378.905630	17245.788085	29.681050
378.988262	17263.415577	29.686068
379.350412	17289.312802	29.691085
379.449251	17316.931390	29.696103
380.268423	17340.246504	29.701120
380.685455	17374.600167	29.706138
380.961018	17400.422582	29.711156
381.787879	17429.788375	29.716173
381.668207	17465.681844	29.721191
382.356386	17484.586078	29.726208
382.650926	17514.006444	29.731226
383.114708	17534.325952	29.736244
383.769609	17563.042787	29.741261
383.847227	17594.344808	29.746279
384.142695	17607.779640	29.751296
384.628445	17638.140110	29.756314
384.934641	17663.316916	29.761332
385.228289	17688.963180	29.766349
385.878864	17725.703747	29.771367
386.410126	17749.430577	29.776384
386.549002	17782.650112	29.781402
386.870937	17816.833010	29.786420
387.368617	17828.701430	29.791437
387.600627	17858.552151	29.796455
388.211754	17875.690464	29.801472
388.734457	17906.696280	29.806490
388.865926	17926.676267	29.811508
389.867417	17957.449695	29.816525
389.786690	17975.839230	29.821543
390.180808	18008.520353	29.826560
391.020672	18024.385001	29.831578
391.295706	18050.224160	29.836596
391.857944	18064.502200	29.841613
391.993845	18090.615766	29.846631
392.094400	18107.536858	29.851648
392.207978	18133.319139	29.856666
392.538476	18160.034235	29.861684
393.058326	18183.921309	29.866701
393.342148	18226.032808	29.871719
393.707718	18242.148360	29.876736
394.025664	18267.627357	29.881754
394.571561	18298.112166	29.886772
395.008352	18321.071051	29.891789
395.275732	18342.742319	29.896807
395.339543	18362.903859	29.901824
396.101201	18394.726106	29.906842
396.459116	18428.304328	29.911860
397.028558	18455.620693	29.916877
397.561835	18475.165964	29.921895
398.049173	18498.995314	29.926912
398.483688	18521.809490	29.931930
398.754698	18548.224829	29.936948
399.283525	18568.541617	29.941965
399.334865	18599.299734	29.946983
400.018200	18619.453537	29.952000
400.088042	18648.117766	29.957018
400.207739	18674.525245	29.962036
400.738163	18700.009637	29.967053
401.269539	18741.584633	29.972071
401.604792	18765.033666	29.977088
402.143006	18793.580970	29.982106
402.604817	18831.433324	29.987124
403.099940	18849.999376	29.992141
403.323596	18883.106517	29.997159
403.644601	18900.145602	30.002176
404.489167	18923.648206	30.007194
405.094291	18951.187148	30.012212
405.616014	18969.041603	30.017229
406.528515	19004.480304	30.022247
406.602809	19014.393733	30.027264
407.249897	19037.270187	30.032282
407.180946	19052.443241	30.037300
407.664867	19075.016625	30.042317
407.673824	19098.870646	30.047335
408.280428	19123.257101	30.052352
408.560443	19147.542807	30.057370
408.829558	19174.136186	30.062388
409.366508	19204.396378	30.067405
409.889272	19238.398892	30.072423
410.328026	19261.358585	30.077440
410.381081	19286.551639	30.082458
410.812794	19324.024259	30.087476
411.329229	19337.280584	30.092493
411.553020	19372.921942	30.097511
412.097107	19407.129917	30.102528
412.737513	19428.200999	30.107546
412.756910	19458.807504	30.112564
413.662660	19485.327469	30.117581
413.638565	19514.456158	30.122599
414.190933	19546.894113	30.127616
414.431043	19582.678623	30.132634
414.663220	19603.484923	30.137652
415.332861	19638.716196	30.142669
415.709733	19661.231112	30.147687
416.374985	19705.889378	30.152704
416.709011	19731.633141	30.157722
417.045099	19758.823405	30.162740
417.175772	19781.939077	30.167757
417.598413	19809.741405	30.172775
417.720147	19853.947606	30.177792
418.419052	19886.792930	30.182810
418.693163	19931.057716	30.187828
419.218333	19957.517532	30.192845
419.634385	19989.939539	30.197863
419.893451	20034.307987	30.202880
420.453034	20064.351182	30.207898
420.981388	20099.017712	30.212916
421.295808	20133.787107	30.217933
421.733438	20155.838242	30.222951
422.231322	20177.766297	30.227968
422.947535	20204.518924	30.232986
423.190546	20239.666068	30.238004
423.774480	20259.369517	30.243021
424.063046	20294.661300	30.248039
424.351859	20313.823172	30.253056
425.128277	20345.279871	30.258074
425.536816	20382.259006	30.263092
426.256929	20402.737474	30.268109
426.786641	20420.156072	30.273127
427.344902	20443.673497	30.278144
427.700265	20459.129079	30.283162
427.935557	20485.306200	30.288180
428.781948	20495.093864	30.293197
428.875356	20516.068055	30.298215
429.184398	20542.341178	30.303232
429.642718	20556.037013	30.308250
429.977651	20583.443420	30.313268
430.430315	20608.455922	30.318285
431.083655	20638.270587	30.323303
431.489407	20661.357111	30.328320
432.045767	20677.350208	30.333338
432.127478	20709.939185	30.338356
432.781987	20730.788347	30.343373
433.144629	20759.555410	30.348391
433.100158	20788.303757	30.353408
433.891895	20813.832372	30.358426
434.062793	20852.921758	30.363444
434.192244	20881.504166	30.368461
434.502889	20919.586287	30.373479
435.177448	20954.977124	30.378496
435.563103	20981.858097	30.383514
435.975003	21019.874104	30.388532
436.599586	21058.830088	30.393549
437.237998	21086.625913	30.398567
437.337652	21116.325318	30.403584
438.115093	21144.560817	30.408602
438.490810	21184.901592	30.413620
439.116007	21216.433780	30.418637
439.392056	21232.035005	30.423655
439.810489	21274.782915	30.428672
440.572072	21297.265097	30.433690
440.733416	21330.196533	30.438708
441.251997	21365.245928	30.443725
441.507882	21394.618149	30.448743
442.018423	21435.469193	30.453760
442.552641	21452.319353	30.458778
443.065815	21487.053887	30.463796
443.868772	21517.219383	30.468813
444.446441	21545.082181	30.473831
444.793628	21581.668748	30.478848
445.316785	21590.022453	30.483866
445.666746	21624.277163	30.488884
446.071160	21637.678862	30.493901
446.306389	21657.602285	30.498919
446.681179	21692.548279	30.503936
447.121455	21716.281472	30.508954
447.102746	21753.702494	30.513972
447.549495	21781.630238	30.518989
448.646112	21810.448856	30.524007
449.319519	21832.395669	30.529024
449.630593	21856.174419	30.534042
450.110006	21888.412782	30.539060
450.430679	21912.063734	30.544077
451.070618	21929.188499	30.549095
451.455318	21959.546159	30.554112
451.439141	21979.047791	30.559130
451.748751	22004.476093	30.564148
452.227094	22029.012514	30.569165
452.777524	22058.914863	30.574183
453.108557	22093.135423	30.579200
453.782395	22119.606608	30.584218
453.988121	22143.282051	30.589236
454.228878	22172.310263	30.594253
454.572906	22200.684258	30.599271
454.891072	22240.720223	30.604288
455.624100	22275.870546	30.609306
455.513327	22316.169318	30.614324
456.263789	22355.449480	30.619341
456.795902	22381.519728	30.624359
457.239711	22419.015335	30.629376
457.978843	22456.332345	30.634394
458.581462	22496.728943	30.639412
458.902807	22532.992723	30.644429
459.457399	22559.325094	30.649447
459.724365	22589.727326	30.654464
460.003900	22626.699168	30.659482
460.711780	22658.410357	30.664500
461.832438	22672.724900	30.669517
462.325087	22701.266041	30.674535
462.345916	22743.383963	30.679552
462.900100	22757.698292	30.684570
463.349718	22788.963348	30.689588
463.943515	22822.828323	30.694605
464.224863	22856.615621	30.699623
464.790594	22890.485082	30.704640
465.204234	22921.724354	30.709658
465.474196	22960.290664	30.714676
465.965743	22988.484852	30.719693
466.399147	23024.125473	30.724711
466.951975	23064.530981	30.729728
467.571480	23096.067062	30.734746
467.853851	23130.176932	30.739764
468.289744	23167.062252	30.744781
468.822030	23195.212478	30.749799
469.124764	23235.309726	30.754816
469.229205	23272.183651	30.759834
470.031506	23306.029631	30.764852
470.320939	23354.520806	30.769869
470.851466	23384.914822	30.774887
471.038502	23434.654341	30.779904
471.763983	23476.885285	30.784922
472.558987	23520.205012	30.789940
472.490783	23566.837707	30.794957
473.414512	23606.617861	30.799975
473.653425	23646.883850	30.804992
474.393249	23684.234662	30.810010
474.824615	23716.919501	30.815028
475.043816	23755.476298	30.820045
475.654956	23791.798369	30.825063
475.991321	23827.866282	30.830080
476.792508	23865.713414	30.835098
477.333746	23909.218835	30.840116
477.679501	23952.223971	30.845133
478.436387	23979.480933	30.850151
478.708666	24022.668278	30.855168
479.444707	24061.410614	30.860186
479.771798	24097.398309	30.865204
479.942531	24131.337696	30.870221
480.411316	24161.420229	30.875239
480.805530	24201.372475	30.880256
481.584510	24244.677316	30.885274
482.230611	24280.546167	30.890292
482.452595	24308.841066	30.895309
483.418686	24341.348896	30.900327
483.486952	24373.238230	30.905344
484.051772	24405.619054	30.910362
484.236150	24433.275412	30.915380
485.051203	24468.960316	30.920397
485.642246	24492.831348	30.925415
486.397234	24537.018950	30.930432
486.888953	24548.696479	30.935450
487.673974	24578.041597	30.940468
488.045242	24617.631724	30.945485
488.558602	24624.389434	30.950503
489.788702	24643.863967	30.955520
490.143305	24648.649466	30.960538
490.297944	24673.441773	30.965556
490.258261	24697.310129	30.970573
491.446787	24719.167312	30.975591
491.699724	24749.221139	30.980608
492.082317	24774.534196	30.985626
491.926293	24798.585090	30.990644
492.551027	24832.259087	30.995661
492.934129	24858.058769	31.000679
493.156365	24907.733284	31.005696
493.631395	24935.250296	31.010714
494.061413	24981.865606	31.015732
494.328504	25016.404488	31.020749
495.390029	25057.670136	31.025767
495.578043	25097.150711	31.030784
496.008379	25132.852456	31.035802
497.100655	25166.207767	31.040820
497.368740	25212.482287	31.045837
497.855244	25249.433095	31.050855
498.157322	25279.796047	31.055872
499.189193	25328.125877	31.060890
499.538249	25362.469326	31.065908
500.120686	25398.716634	31.070925
500.354008	25429.235868	31.075943
500.742479	25468.332065	31.080960
501.145591	25501.504517	31.085978
501.965459	25545.064917	31.090996
502.335268	25586.774283	31.096013
503.312503	25608.128161	31.101031
503.822632	25656.363053	31.106048
504.158880	25690.197158	31.111066
504.776932	25716.530145	31.116084
504.905918	25755.793692	31.121101
505.885634	25784.857482	31.126119
505.866319	25817.059774	31.131136
506.417057	25850.096064	31.136154
507.269696	25892.451356	31.141172
507.274829	25934.477327	31.146189
508.073361	25971.045937	31.151207
508.229702	26006.178866	31.156224
508.876189	26029.676549	31.161242
510.086303	26076.956620	31.166260
510.484226	26111.546535	31.171277
511.132826	26141.547170	31.176295
511.613866	26175.568107	31.181312
512.114739	26199.929204	31.186330
512.528605	26229.644199	31.191348
513.053077	26264.890907	31.196365
513.454361	26289.128578	31.201383
513.726854	26335.423954	31.206400
514.184655	26372.431853	31.211418
514.600302	26403.094819	31.216436
515.113902	26445.737895	31.221453
515.930809	26483.985690	31.226471
515.964905	26532.808707	31.231488
516.394867	26560.998562	31.236506
517.135237	26590.309339	31.241524
517.384830	26627.767241	31.246541
518.561242	26660.265055	31.251559
518.713824	26689.218757	31.256576
519.291218	26724.957315	31.261594
519.790811	26747.416934	31.266612
520.105410	26794.819140	31.271629
520.616429	26819.508051	31.276647
520.987946	26858.091336	31.281664
521.733763	26901.621960	31.286682
522.301048	26943.878522	31.291700
522.112957	26976.936874	31.296717
522.910005	27011.030107	31.301735
523.522441	27059.435712	31.306752
524.144077	27101.450297	31.311770
524.802328	27140.747905	31.316788
524.855176	27186.365240	31.321805
525.832129	27225.234186	31.326823
526.193267	27269.166777	31.331840
526.726449	27308.503142	31.336858
527.154612	27351.698649	31.341876
527.762815	27398.955437	31.346893
528.292591	27435.682306	31.351911
528.893553	27483.281713	31.356928
529.373314	27539.672699	31.361946
530.258397	27570.504527	31.366964
530.516103	27612.134402	31.371981
531.237037	27654.924718	31.376999
531.524361	27695.406169	31.382016
532.273133	27737.610853	31.387034
532.950304	27767.419844	31.392052
533.648020	27809.942325	31.397069
533.936763	27851.662665	31.402087
534.518421	27892.471592	31.407104
535.120264	27937.493193	31.412122
535.828289	27967.986604	31.417140
535.836959	28023.093371	31.422157
537.020273	28054.878143	31.427175
537.466055	28098.464365	31.432192
537.932213	28138.596513	31.437210
538.804510	28171.934166	31.442228
539.070198	28219.701262	31.447245
539.651519	28249.639652	31.452263
540.326219	28273.299888	31.457280
541.038112	28301.669495	31.462298
541.763497	28339.069127	31.467316
542.345712	28371.738043	31.472333
543.134745	28399.526925	31.477351
543.263075	28440.805722	31.482368
543.617881	28472.821256	31.487386
544.060439	28508.956864	31.492404
544.587442	28546.179179	31.497421
544.768427	28589.535887	31.502439
545.576521	28630.879902	31.507456
546.097478	28663.697877	31.512474
546.869314	28694.188764	31.517492
547.542064	28734.018134	31.522509
548.007466	28770.782718	31.527527
548.219036	28797.132431	31.532544
548.649574	28855.184427	31.537562
549.213971	28887.951755	31.542580
549.923173	28938.919310	31.547597
550.518554	28975.961104	31.552615
550.959579	29014.765208	31.557632
551.350992	29058.482039	31.562650
552.089051	29093.978526	31.567668
552.510701	29148.391958	31.572685
552.818316	29180.510760	31.577703
553.731475	29221.220175	31.582720
553.840725	29253.730260	31.587738
554.174921	29291.641317	31.592756
554.873352	29339.109790	31.597773
555.553162	29384.381602	31.602791
556.110127	29432.270529	31.607808
556.392947	29463.831075	31.612826
556.927567	29500.895921	31.617844
557.447243	29551.559496	31.622861
557.942836	29593.156377	31.627879
558.741608	29644.257127	31.632896
559.346127	29694.161973	31.637914
560.057054	29727.824377	31.642932
560.499011	29780.030296	31.647949
561.314481	29818.335160	31.652967
562.268044	29852.061132	31.657984
562.548958	29878.237093	31.663002
563.935591	29910.587290	31.668020
563.731236	29946.946244	31.673037
564.171022	29985.720773	31.678055
564.570991	30019.242432	31.683072
565.177803	30075.102308	31.688090
565.795837	30114.310772	31.693108
566.125074	30156.396133	31.698125
566.505106	30209.004691	31.703143
567.424491	30260.549642	31.708160
567.772862	30306.387098	31.713178
568.721750	30345.670921	31.718196
569.238885	30406.412969	31.723213
569.745033	30438.970601	31.728231
570.617087	30483.595431	31.733248
570.956070	30533.644792	31.738266
571.724790	30567.786312	31.743284
572.072199	30611.064488	31.748301
572.840678	30657.058569	31.753319
573.291142	30696.174123	31.758336
574.085476	30747.708154	31.763354
574.916379	30792.782552	31.768372
575.711266	30835.719722	31.773389
576.345324	30877.038470	31.778407
576.736960	30915.487213	31.783424
577.121513	30959.101690	31.788442
577.430999	30992.063773	31.793460
577.488222	31037.120075	31.798477
578.376363	31074.297078	31.803495
579.463193	31125.078520	31.808512
579.691464	31179.413639	31.813530
580.248406	31218.918179	31.818548
581.216411	31264.686588	31.823565
581.419840	31311.256843	31.828583
582.291855	31349.637933	31.833600
582.475646	31397.324020	31.838618
583.554419	31434.895537	31.843636
583.761747	31482.034504	31.848653
584.534854	31526.588492	31.853671
585.303572	31568.564063	31.858688
585.751707	31617.543354	31.863706
586.231724	31651.858043	31.868724
586.928918	31694.110510	31.873741
587.694237	31735.827764	31.878759
588.444728	31770.119508	31.883776
589.125020	31814.675921	31.888794
589.512555	31851.306411	31.893812
590.416129	31889.462332	31.898829
591.170906	31928.924786	31.903847
592.121269	31953.058410	31.908864
592.202570	31996.924574	31.913882
592.856071	32020.693581	31.918900
593.040259	32057.748035	31.923917
593.649480	32091.613462	31.928935
594.002910	32123.577994	31.933952
594.308883	32159.551621	31.938970
594.927548	32191.689907	31.943988
595.349738	32241.578718	31.949005
595.646802	32282.295267	31.954023
596.443258	32328.491004	31.959040
596.650542	32387.112402	31.964058
597.237355	32426.153099	31.969076
598.041163	32478.454902	31.974093
598.549251	32532.377012	31.979111
599.203345	32576.660977	31.984128
599.799309	32624.431117	31.989146
600.412145	32669.549867	31.994164
601.359870	32723.283916	31.999181
601.720336	32770.578977	32.004199
602.461480	32823.675320	32.009216
602.900356	32868.530772	32.014234
603.905679	32920.087933	32.019252
604.571394	32961.108770	32.024269
604.931735	33020.245487	32.029287
605.530231	33059.772347	32.034304
605.789106	33114.935940	32.039322
606.409390	33166.642158	32.044340
607.311971	33223.242085	32.049357
607.728911	33275.542891	32.054375
608.136277	33323.622162	32.059392
608.930843	33387.642517	32.064410
609.751136	33435.164638	32.069428
610.207102	33492.833716	32.074445
610.852390	33548.165893	32.079463
611.637548	33606.580629	32.084480
612.023406	33647.734890	32.089498
612.980641	33700.148635	32.094516
613.572355	33757.152443	32.099533
613.736874	33803.569943	32.104551
615.223862	33852.746807	32.109568
615.612631	33914.037508	32.114586
616.374430	33961.746954	32.119604
616.808214	34006.776339	32.124621
617.204371	34061.016962	32.129639
618.153176	34115.121113	32.134656
618.948030	34158.710026	32.139674
619.683187	34192.186238	32.144692
620.615645	34244.914997	32.149709
621.158001	34288.537164	32.154727
622.076878	34325.342172	32.159744
622.492490	34373.074832	32.164762
623.002684	34411.555825	32.169780
623.650956	34450.932145	32.174797
623.743255	34499.638497	32.179815
624.507851	34531.100129	32.184832
625.154344	34597.202022	32.189850
626.145602	34637.031095	32.194868
626.664874	34674.531170	32.199885
627.618376	34717.192429	32.204903
628.543009	34751.126868	32.209920
629.163325	34790.482886	32.214938
629.323949	34825.421534	32.219956
630.320339	34861.248065	32.224973
630.750591	34901.613874	32.229991
631.253088	34941.380513	32.235008
631.599138	34994.467986	32.240026
632.019841	35026.059765	32.245044
632.582189	35081.231856	32.250061
633.104924	35141.006812	32.255079
633.677154	35166.556065	32.260096
634.482463	35217.460843	32.265114
634.905764	35259.952831	32.270132
635.678000	35293.165793	32.275149
635.887633	35342.039180	32.280167
636.780873	35389.731401	32.285184
637.276370	35441.386767	32.290202
637.523765	35486.151161	32.295220
638.464698	35545.912742	32.300237
638.767372	35602.789502	32.305255
639.407189	35642.030261	32.310272
640.522537	35690.314540	32.315290
641.204198	35746.456149	32.320308
641.700146	35792.731587	32.325325
642.480921	35847.093964	32.330343
642.736628	35891.548100	32.335360
643.332727	35952.199126	32.340378
644.336770	35998.819551	32.345396
644.893605	36052.654578	32.350413
645.603054	36121.666296	32.355431
646.430979	36168.832991	32.360448
646.954817	36222.193042	32.365466
647.286858	36279.553911	32.370484
648.248967	36328.160678	32.375501
648.492593	36384.783159	32.380519
649.487535	36437.008147	32.385536
649.991192	36489.998953	32.390554
650.854296	36544.698067	32.395572
651.924541	36601.186120	32.400589
652.243154	36656.684790	32.405607
653.105424	36707.710740	32.410624
654.054867	36739.886689	32.415642
655.082195	36780.586776	32.420660
656.242573	36821.354752	32.425677
656.878368	36857.177569	32.430695
657.644387	36893.353239	32.435712
658.176166	36929.179723	32.440730
658.577182	36969.383292	32.445748
659.440737	36998.809775	32.450765
659.952782	37052.451962	32.455783
660.568734	37100.532648	32.460800
661.054268	37134.924982	32.465818
661.355984	37187.575889	32.470836
662.155457	37228.944628	32.475853
662.782480	37281.709530	32.480871
663.439550	37325.427588	32.485888
663.933466	37376.316460	32.490906
664.363478	37427.828762	32.495924
665.178140	37474.235293	32.500941
665.607711	37541.006131	32.505959
666.382296	37584.788629	32.510976
666.876531	37636.342023	32.515994
667.483524	37700.885205	32.521012
668.435358	37748.586244	32.526029
668.674401	37806.711855	32.531047
669.832314	37857.296156	32.536064
670.322368	37907.149846	32.541082
671.088744	37977.897655	32.546100
671.790808	38021.774542	32.551117
672.090716	38078.291570	32.556135
672.776905	38131.188472	32.561152
673.812070	38184.518092	32.566170
674.183670	38246.943235	32.571188
674.889464	38299.255732	32.576205
675.388639	38353.845394	32.581223
676.230676	38411.018763	32.586240
676.723568	38480.324754	32.591258
677.578659	38537.787315	32.596276
678.399081	38592.523607	32.601293
679.126401	38647.932194	32.606311
679.620618	38686.720620	32.611328
680.141622	38741.219334	32.616346
680.707761	38793.826694	32.621364
681.359926	38845.124425	32.626381
682.019660	38899.949750	32.631399
683.001867	38945.827483	32.636416
683.995880	38989.768402	32.641434
684.362894	39042.103824	32.646452
685.140276	39092.889397	32.651469
685.474082	39150.725637	32.656487
686.317019	39205.548515	32.661504
687.259625	39258.812998	32.666522
687.589118	39315.847222	32.671540
688.537606	39360.150119	32.676557
689.293822	39418.123683	32.681575
689.657208	39479.238300	32.686592
690.550079	39519.604060	32.691610
691.020614	39596.594364	32.696628
692.019759	39652.450159	32.701645
692.355511	39703.634763	32.706663
693.362642	39758.762332	32.711680
693.860573	39807.145699	32.716698
694.750276	39871.050591	32.721716
695.419068	39930.809866	32.726733
696.042928	39993.131221	32.731751
696.679126	40046.869056	32.736768
697.582684	40114.408856	32.741786
698.107861	40172.679693	32.746804
699.068129	40226.993613	32.751821
699.731646	40294.331023	32.756839
700.595603	40340.065697	32.761856
701.351793	40401.406352	32.766874
701.988683	40456.156961	32.771892
702.528851	40512.358361	32.776909
703.389090	40575.637493	32.781927
703.759294	40633.687045	32.786944
704.756667	40697.514367	32.791962
705.184512	40758.489740	32.796980
706.107298	40819.192183	32.801997
706.716083	40869.261896	32.807015
707.395136	40934.758492	32.812032
708.343931	40981.651311	32.817050
708.919265	41051.654695	32.822068
709.228001	41108.235175	32.827085
710.539118	41175.784394	32.832103
710.959976	41233.169917	32.837120
711.757496	41291.957903	32.842138
712.415061	41363.998606	32.847156
712.918229	41415.743023	32.852173
713.876263	41478.756574	32.857191
714.477171	41550.420916	32.862208
715.268023	41596.618650	32.867226
715.769573	41659.767028	32.872244
717.086962	41727.949434	32.877261
717.254410	41780.082176	32.882279
718.295753	41841.932730	32.887296
719.442471	41897.714397	32.892314
720.168023	41954.409268	32.897332
720.879766	42003.972233	32.902349
721.546321	42061.960470	32.907367
722.330779	42117.571401	32.912384
723.188049	42168.307447	32.917402
724.310287	42223.764871	32.922420
724.351646	42277.069519	32.927437
725.598913	42326.638395	32.932455
725.844316	42381.644512	32.937472
726.597999	42434.478144	32.942490
727.092495	42492.487977	32.947508
727.937069	42544.200887	32.952525
728.487440	42589.160537	32.957543
728.906703	42639.738164	32.962560
729.758926	42684.752218	32.967578
730.560031	42756.914297	32.972596
731.192082	42794.297116	32.977613
731.811596	42853.755811	32.982631
732.235206	42916.249495	32.987648
733.632579	42970.382017	32.992666
734.047895	43025.015419	32.997684
734.808919	43079.538216	33.002701
736.198548	43131.604081	33.007719
736.420551	43197.393629	33.012736
737.379967	43231.064061	33.017754
737.960379	43294.957532	33.022772
738.318582	43344.110500	33.027789
739.367396	43413.567004	33.032807
739.895734	43486.785939	33.037824
741.191545	43541.606133	33.042842
741.450839	43600.629557	33.047860
742.142094	43649.275950	33.052877
743.176355	43711.834953	33.057895
743.491650	43778.592102	33.062912
744.252044	43838.746260	33.067930
744.781795	43910.454660	33.072948
745.492443	43977.416523	33.077965
746.801784	44050.743453	33.082983
747.208217	44124.059373	33.088000
748.127865	44172.576482	33.093018
748.971766	44243.851215	33.098036
749.587522	44305.793910	33.103053
750.752721	44361.477734	33.108071
751.458667	44426.303724	33.113088
752.087410	44491.900963	33.118106
752.494738	44563.453418	33.123124
752.986685	44622.411714	33.128141
754.270663	44685.200255	33.133159
755.021088	44764.094355	33.138176
755.942539	44824.959864	33.143194
757.008725	44901.502832	33.148212
757.762004	44954.968769	33.153229
758.387295	45016.785449	33.158247
758.854900	45090.126655	33.163264
759.354811	45146.067819	33.168282
760.411261	45219.804853	33.173300
760.688400	45287.401115	33.178317
761.310515	45350.440051	33.183335
762.181136	45424.617853	33.188352
763.046953	45494.678656	33.193370
763.961561	45574.891099	33.198388
764.683423	45649.617835	33.203405
765.549922	45715.333476	33.208423
766.481614	45791.875129	33.213440
767.537540	45858.586471	33.218458
768.512360	45914.986992	33.223476
769.087653	45980.305939	33.228493
770.066603	46031.038212	33.233511
770.769313	46102.056197	33.238528
771.673314	46166.647655	33.243546
772.424057	46222.729585	33.248564
773.097776	46294.663615	33.253581
773.784057	46345.340944	33.258599
774.592150	46404.343284	33.263616
775.339419	46475.981779	33.268634
776.158290	46521.166945	33.273652
776.873867	46592.677900	33.278669
777.753648	46649.114040	33.283687
778.299211	46712.573582	33.288704
778.902472	46761.506148	33.293722
779.740628	46820.087383	33.298740
780.146273	46883.974054	33.303757
781.309158	46941.233522	33.308775
781.230751	47006.195404	33.313792
782.845384	47067.351317	33.318810
783.291210	47138.450516	33.323828
783.736137	47204.913030	33.328845
784.536449	47268.834245	33.333863
785.383456	47349.683505	33.338880
785.851204	47415.156204	33.343898
786.298343	47487.508880	33.348916
787.338957	47569.189150	33.353933
788.434079	47635.437844	33.358951
789.452577	47700.850940	33.363968
790.395903	47770.248832	33.368986
791.398409	47835.044830	33.374004
792.016536	47903.266449	33.379021
792.998940	47968.363295	33.384039
793.576767	48044.651367	33.389056
794.481341	48109.608901	33.394074
795.579333	48180.932497	33.399092
796.375659	48249.924545	33.404109
797.313336	48299.782650	33.409127
797.617855	48366.827153	33.414144
798.688397	48432.133035	33.419162
799.577593	48503.857082	33.424180
800.249820	48568.244754	33.429197
801.723522	48641.149875	33.434215
802.652498	48708.895321	33.439232
802.873840	48765.451887	33.444250
803.731340	48826.344495	33.449268
804.478986	48888.880299	33.454285
805.257043	48964.438034	33.459303
806.446876	49026.924364	33.464320
806.776754	49093.935424	33.469338
807.693835	49166.631521	33.474356
808.287230	49239.783145	33.479373
809.216237	49302.380425	33.484391
809.899242	49376.619384	33.489408
810.789507	49445.454913	33.494426
811.915023	49507.857671	33.499444
812.799695	49581.888754	33.504461
813.518044	49648.145020	33.509479
814.584409	49720.699431	33.514496
815.242171	49788.370089	33.519514
816.495566	49850.931027	33.524532
817.020281	49910.815416	33.529549
817.778822	49981.292741	33.534567
818.980119	50044.621546	33.539584
819.427818	50101.424561	33.544602
820.292852	50165.862642	33.549620
820.536283	50244.829470	33.554637
821.756061	50306.435186	33.559655
823.036723	50373.795488	33.564672
823.673918	50441.876201	33.569690
824.478824	50503.395178	33.574708
825.037468	50567.591035	33.579725
825.965105	50632.666039	33.584743
826.727481	50698.981754	33.589760
827.283691	50760.761580	33.594778
828.109259	50834.654051	33.599796
828.739125	50907.552225	33.604813
829.992607	50969.692279	33.609831
831.025545	51043.603757	33.614848
831.679334	51103.452174	33.619866
832.651280	51167.129805	33.624884
833.416832	51217.274150	33.629901
834.547832	51272.417187	33.634919
835.588808	51334.167377	33.639936
836.332909	51384.733024	33.644954
837.157212	51440.626533	33.649972
837.637223	51495.150125	33.654989
838.618124	51548.279793	33.660007
839.698086	51609.385590	33.665024
839.907614	51675.068849	33.670042
841.048698	51736.741258	33.675060
841.394519	51789.173089	33.680077
842.722291	51843.730048	33.685095
843.144234	51913.949304	33.690112
843.756883	51975.445182	33.695130
844.866131	52053.176108	33.700148
845.171681	52123.477389	33.705165
846.167951	52187.596964	33.710183
847.045854	52262.181871	33.715200
847.976591	52340.599608	33.720218
848.531800	52413.526796	33.725236
849.667644	52484.927468	33.730253
850.042240	52559.275295	33.735271
851.000333	52638.828745	33.740288
851.686994	52728.827364	33.745306
852.558935	52802.510076	33.750324
853.471932	52894.562230	33.755341
854.547784	52969.213501	33.760359
855.520970	53043.963254	33.765376
856.147417	53131.188595	33.770394
856.928538	53209.645199	33.775412
857.768445	53285.182130	33.780429
858.753336	53375.630384	33.785447
859.681496	53453.735871	33.790464
860.518482	53533.425121	33.795482
861.633128	53612.584173	33.800500
862.643856	53687.899649	33.805517
863.650067	53774.834138	33.810535
864.350649	53846.104232	33.815552
865.000454	53927.899526	33.820570
866.620143	53996.698314	33.825588
866.875074	54084.149559	33.830605
867.792433	54169.340153	33.835623
868.738810	54244.597823	33.840640
869.818152	54317.601227	33.845658
871.098662	54397.945770	33.850676
872.128796	54471.052231	33.855693
872.932153	54546.826723	33.860711
873.922999	54613.073717	33.865728
874.312671	54695.165295	33.870746
876.136510	54733.723784	33.875764
877.274987	54793.753014	33.880781
878.589852	54836.409307	33.885799
879.612284	54893.653459	33.890816
879.660645	54963.984306	33.895834
880.756351	55009.965716	33.900852
881.453530	55083.448647	33.905869
882.016305	55145.745315	33.910887
882.331918	55209.795594	33.915904
883.442376	55300.598743	33.920922
884.244178	55368.415069	33.925940
885.242381	55444.117811	33.930957
886.141669	55511.520684	33.935975
887.098252	55582.015751	33.940992
887.526022	55657.542176	33.946010
888.538727	55724.459697	33.951028
889.737078	55809.618795	33.956045
890.378977	55873.480849	33.961063
891.263271	55940.001286	33.966080
891.844859	56008.537199	33.971098
892.729785	56065.647376	33.976116
893.037405	56137.561448	33.981133
893.908858	56207.457753	33.986151
894.715788	56282.718299	33.991168
895.065418	56365.961039	33.996186
896.685641	56443.228238	34.001204
897.987705	56528.076319	34.006221
898.712560	56598.306696	34.011239
899.746241	56672.356041	34.016256
900.350360	56760.737420	34.021274
901.472958	56825.761301	34.026292
902.059170	56913.462528	34.031309
902.989832	56988.288341	34.036327
903.909111	57068.710822	34.041344
904.574106	57143.173430	34.046362
905.375473	57224.070463	34.051380
906.462580	57312.030609	34.056397
907.074444	57396.565177	34.061415
908.634464	57482.344813	34.066432
909.410178	57574.639069	34.071450
910.511636	57654.990857	34.076468
911.380476	57732.853860	34.081485
912.269038	57823.682170	34.086503
913.164088	57901.541641	34.091520
914.100082	57986.432888	34.096538
915.073809	58068.888199	34.101556
915.600236	58152.546326	34.106573
916.703857	58237.665529	34.111591
918.049436	58328.114476	34.116608
918.786187	58417.234473	34.121626
920.051424	58500.019302	34.126644
920.330489	58581.033848	34.131661
921.366653	58670.975274	34.136679
922.485751	58762.150988	34.141696
923.200385	58856.883764	34.146714
924.187929	58945.732487	34.151732
925.474773	59015.876119	34.156749
926.874379	59100.629495	34.161767
927.849598	59173.790552	34.166784
928.833432	59253.355817	34.171802
929.767064	59332.821559	34.176820
931.052086	59408.403565	34.181837
931.829953	59486.273725	34.186855
933.021333	59556.724937	34.191872
933.643534	59637.088300	34.196890
934.216661	59709.503389	34.201908
935.141459	59792.086120	34.206925
935.819291	59872.030180	34.211943
937.023079	59952.082519	34.216960
937.746172	60041.178962	34.221978
938.940381	60105.187810	34.226996
940.272403	60193.430472	34.232013
941.142623	60268.813878	34.237031
942.460908	60342.463070	34.242048
942.986930	60415.495237	34.247066
943.961271	60491.439123	34.252084
945.267420	60558.469993	34.257101
946.201109	60632.831889	34.262119
947.124558	60701.049414	34.267136
947.843576	60781.192593	34.272154
949.114395	60854.065826	34.277172
949.669152	60923.366788	34.282189
950.350497	61011.428849	34.287207
951.517251	61081.103401	34.292224
951.903527	61161.312277	34.297242
953.808135	61227.985971	34.302260
954.760168	61300.973455	34.307277
955.347782	61368.175360	34.312295
956.418975	61436.568163	34.317312
957.350795	61510.483587	34.322330
958.251555	61568.769022	34.327348
958.622445	61633.808886	34.332365
958.921796	61718.628687	34.337383
960.197237	61784.129497	34.342400
960.975112	61872.970872	34.347418
962.234834	61950.172515	34.352436
963.051135	62041.230372	34.357453
963.576494	62127.738185	34.362471
964.856048	62204.836256	34.367488
965.501044	62296.111621	34.372506
966.450509	62383.807687	34.377524
967.379107	62475.438370	34.382541
968.774114	62563.141681	34.387559
969.922172	62641.223779	34.392576
970.954854	62736.536094	34.397594
971.841870	62822.439306	34.402612
972.572577	62913.342779	34.407629
973.643021	63000.617056	34.412647
974.441414	63083.768609	34.417664
975.433652	63178.386247	34.422682
976.500343	63265.896266	34.427700
977.575890	63355.899405	34.432717
978.796685	63450.596450	34.437735
979.740577	63535.398106	34.442752
980.860707	63626.072643	34.447770
982.098259	63715.228899	34.452788
983.346131	63794.071409	34.457805
983.823627	63884.903895	34.462823
985.036244	63969.829794	34.467840
985.812001	64057.103003	34.472858
986.533763	64151.399263	34.477876
987.444212	64237.423992	34.482893
988.500497	64343.304653	34.487911
990.539562	64411.643639	34.492928
991.756183	64494.665158	34.497946
992.990205	64567.820949	34.502964
994.715522	64622.642580	34.507981
995.906994	64691.987913	34.512999
996.969704	64759.764454	34.518016
997.315165	64838.440519	34.523034
998.383197	64899.024811	34.528052
998.811909	64975.352272	34.533069
999.797171	65048.516534	34.538087
1000.821673	65127.436002	34.543104
1001.865704	65211.999841	34.548122
1002.356357	65295.523199	34.553140
1003.346915	65365.870299	34.558157
1003.940294	65464.825727	34.563175
1004.856472	65552.025299	34.568192
1005.570559	65648.930413	34.573210
1006.679910	65740.418316	34.578228
1007.851861	65825.325170	34.583245
1008.343827	65921.727766	34.588263
1009.378153	66024.067186	34.593280
1010.503664	66112.071811	34.598298
1011.631895	66212.270117	34.603316
1013.047551	66304.028939	34.608333
1013.965650	66400.797546	34.613351
1015.126643	66491.381097	34.618368
1015.715188	66591.918158	34.623386
1016.681827	66682.741575	34.628404
1017.875574	66774.891194	34.633421
1018.683115	66876.231022	34.638439
1020.139538	66965.636973	34.643456
1020.843721	67056.686188	34.648474
1021.411907	67139.962964	34.653492
1022.848540	67223.864600	34.658509
1023.771137	67313.025632	34.663527
1025.014344	67397.458131	34.668544
1025.920235	67487.819018	34.673562
1026.845974	67572.016595	34.678580
1028.079127	67651.240682	34.683597
1028.962907	67738.579437	34.688615
1029.789601	67828.358692	34.693632
1030.927990	67917.931454	34.698650
1032.022997	68010.905020	34.703668
1033.473146	68086.418021	34.708685
1034.220562	68185.227091	34.713703
1035.138309	68271.308710	34.718720
1036.316111	68362.491466	34.723738
1037.556766	68451.765250	34.728756
1038.774760	68535.230346	34.733773
1039.805594	68630.280288	34.738791
1041.013355	68711.461787	34.743808
1041.944952	68798.277501	34.748826
1042.755133	68885.523976	34.753844
1044.031781	68971.666047	34.758861
1044.867073	69068.451308	34.763879
1046.233679	69162.532831	34.768896
1046.933701	69247.923441	34.773914
1047.955996	69356.704961	34.778932
1049.149425	69436.998174	34.783949
1051.056730	69506.675783	34.788967
1052.450173	69590.585553	34.793984
1053.469490	69679.163533	34.799002
1054.509627	69760.501066	34.804020
1055.605378	69836.789888	34.809037
1056.285704	69915.220516	34.814055
1057.177934	70002.261694	34.819072
1057.671867	70083.830900	34.824090
1059.364881	70172.622305	34.829108
1060.950229	70257.555498	34.834125
1061.022662	70346.954355	34.839143
1062.473653	70441.432649	34.844160
1063.517550	70536.842168	34.849178
1064.182348	70630.911620	34.854196
1065.536353	70717.807328	34.859213
1066.416593	70808.715750	34.864231
1067.352744	70898.286002	34.869248
1068.442600	70993.823018	34.874266
1069.573217	71092.963478	34.879284
1071.283512	71175.347277	34.884301
1072.705156	71263.336106	34.889319
1073.736659	71350.119478	34.894336
1074.635671	71431.072590	34.899354
1075.374338	71519.345899	34.904372
1076.530963	71617.281132	34.909389
1077.588918	71706.657883	34.914407
1078.618547	71797.242526	34.919424
1079.079707	71882.140689	34.924442
1079.996962	71983.407469	34.929460
1081.375290	72066.162373	34.934477
1082.379565	72175.256089	34.939495
1083.352549	72283.747195	34.944512
1084.655327	72368.908548	34.949530
1085.920267	72469.147848	34.954548
1087.012612	72565.944071	34.959565
1088.013009	72667.377854	34.964583
1089.002687	72754.577667	34.969600
1089.988180	72855.317889	34.974618
1090.977697	72951.460256	34.979636
1092.181351	73047.962276	34.984653
1093.081543	73154.251800	34.989671
1093.755003	73237.234086	34.994688
1094.862504	73327.457222	34.999706
1095.806660	73415.920211	35.004724
1097.190625	73519.020103	35.009741
1098.349274	73614.897899	35.014759
1098.967941	73718.079689	35.019776
1100.442887	73803.928157	35.024794
1101.271300	73895.640589	35.029812
1102.687680	73996.761386	35.034829
1103.901011	74102.866635	35.039847
1104.709286	74195.330536	35.044864
1105.833561	74295.129984	35.049882
1107.187677	74397.883273	35.054900
1108.368909	74494.723358	35.059917
1109.259408	74592.609692	35.064935
1109.862667	74699.597588	35.069952
1111.173598	74793.758617	35.074970
1112.516021	74904.926213	35.079988
1113.660320	75008.626496	35.085005
1114.775096	75120.653748	35.090023
1116.086177	75227.052240	35.095040
1117.315650	75332.007183	35.100058
1118.430659	75431.571640	35.105076
1120.039356	75538.735714	35.110093
1120.880010	75643.980398	35.115111
1122.269496	75735.548462	35.120128
1123.599896	75819.753866	35.125146
1124.420836	75924.470702	35.130164
1125.980767	76017.900578	35.135181
1127.260031	76111.551804	35.140199
1128.335626	76216.534144	35.145216
1129.319277	76305.469212	35.150234
1130.389024	76406.260362	35.155252
1131.713699	76500.311218	35.160269
1132.663075	76601.071160	35.165287
1133.690600	76712.814589	35.170304
1134.638994	76812.549411	35.175322
1135.928306	76924.924338	35.180340
1136.927851	77013.111872	35.185357
1138.120295	77120.156994	35.190375
1138.949031	77226.182403	35.195392
1140.370755	77319.764957	35.200410
1141.697948	77420.101764	35.205428
1142.793563	77527.784277	35.210445
1144.325742	77634.449178	35.215463
1145.530803	77728.396223	35.220480
1147.156200	77822.835551	35.225498
1147.768879	77919.839748	35.230516
1148.875419	78012.624987	35.235533
1149.967179	78128.101272	35.240551
1151.156075	78225.637594	35.245568
1152.217627	78311.678767	35.250586
1153.404183	78426.824851	35.255604
1154.020355	78531.507576	35.260621
1155.245880	78634.537655	35.265639
1156.630654	78745.929755	35.270656
1157.912070	78848.166499	35.275674
1159.127502	78956.811441	35.280692
1160.491178	79044.226742	35.285709
1161.527353	79157.042958	35.290727
1162.569594	79260.750003	35.295744
1164.219516	79358.041220	35.300762
1164.839612	79464.411800	35.305780
1165.749738	79560.146620	35.310797
1167.135804	79661.369262	35.315815
1168.131209	79768.924129	35.320832
1169.249564	79875.738152	35.325850
1170.185493	79988.725388	35.330868
1171.685962	80077.541580	35.335885
1172.695856	80177.671789	35.340903
1173.410050	80260.200455	35.345920
1174.815337	80361.371984	35.350938
1175.772371	80464.032593	35.355956
1176.634314	80565.061392	35.360973
1177.702434	80676.535887	35.365991
1179.029475	80782.864821	35.371008
1180.693528	80893.043844	35.376026
1181.578651	81010.553403	35.381044
1182.371656	81113.165915	35.386061
1183.700602	81221.345952	35.391079
1184.746798	81340.618216	35.396096
1186.263545	81444.424247	35.401114
1187.598465	81567.808147	35.406132
1188.402354	81673.651764	35.411149
1190.091049	81787.187929	35.416167
1191.041521	81910.873900	35.421184
1192.365013	82015.459640	35.426202
1193.715728	82120.244248	35.431220
1195.014877	82240.861974	35.436237
1196.301958	82345.631986	35.441255
1197.238110	82465.331587	35.446272
1198.593872	82566.974910	35.451290
1200.086601	82686.778867	35.456308
1201.252645	82804.416904	35.461325
1202.282597	82915.082661	35.466343
1203.052131	83025.244565	35.471360
1204.642363	83138.953539	35.476378
1205.692051	83261.375617	35.481396
1207.178158	83376.039356	35.486413
1208.375668	83486.757283	35.491431
1209.786900	83604.955987	35.496448
1211.166880	83715.557709	35.501466
1212.116389	83829.774636	35.506484
1213.569493	83938.705993	35.511501
1215.026377	84040.959717	35.516519
1216.652309	84155.313404	35.521536
1218.378717	84245.552050	35.526554
1219.948684	84342.834975	35.531572
1220.711731	84448.049092	35.536589
1222.230884	84546.759759	35.541607
1223.326406	84643.103879	35.546624
1224.500079	84740.614562	35.551642
1225.378935	84839.679321	35.556660
1226.565534	84937.606807	35.561677
1227.974092	85052.390714	35.566695
1229.032775	85161.388116	35.571712
1230.298275	85246.975303	35.576730
1231.252245	85360.640101	35.581748
1232.539140	85463.267482	35.586765
1233.696079	85575.431661	35.591783
1234.485901	85690.884631	35.596800
1235.710815	85794.042364	35.601818
1237.105128	85917.233120	35.606836
1238.101741	86050.661585	35.611853
1239.574548	86150.702809	35.616871
1240.735437	86276.567125	35.621888
1241.921574	86374.752991	35.626906
1243.264122	86496.585720	35.631924
1243.868274	86610.436591	35.636941
1245.343359	86729.677285	35.641959
1246.645336	86854.825190	35.646976
1247.786456	86971.698518	35.651994
1249.157890	87099.092274	35.657012
1249.998771	87226.581839	35.662029
1251.556617	87324.966493	35.667047
1252.922689	87450.233696	35.672064
1254.591909	87544.926818	35.677082
1255.868298	87646.942608	35.682100
1256.946523	87751.169237	35.687117
1258.134899	87849.385060	35.692135
1259.372387	87959.543653	35.697152
1260.596412	88048.883907	35.702170
1261.513176	88157.242983	35.707188
1262.774683	88268.032618	35.712205
1264.310590	88376.942433	35.717223
1265.516028	88494.914338	35.722240
1266.559056	88601.227771	35.727258
1267.906179	88717.277608	35.732276
1269.043215	88836.123269	35.737293
1270.809371	88939.904863	35.742311
1271.164566	89059.151916	35.747328
1272.788263	89173.779151	35.752346
1273.885922	89300.008451	35.757364
1274.892697	89421.259257	35.762381
1276.583907	89540.350983	35.767399
1277.905936	89666.711669	35.772416
1278.988253	89790.981106	35.777434
1280.167929	89920.647385	35.782452
1281.161580	90050.571302	35.787469
1282.443307	90166.801737	35.792487
1283.698457	90309.093296	35.797504
1285.405733	90435.802826	35.802522
1287.097624	90564.910583	35.807540
1288.338124	90691.807913	35.812557
1290.293462	90800.167059	35.817575
1291.454541	90923.275643	35.822592
1293.165223	91036.426353	35.827610
1294.433492	91162.091997	35.832628
1295.899392	91288.018903	35.837645
1297.306215	91397.416119	35.842663
1298.311359	91510.995278	35.847680
1299.554309	91622.383275	35.852698
1300.897456	91744.706441	35.857716
1301.743435	91862.050531	35.862733
1303.621825	91982.555000	35.867751
1304.732779	92103.648346	35.872768
1305.712797	92214.623180	35.877786
1307.438229	92346.737144	35.882804
1308.701033	92465.019957	35.887821
1310.142179	92588.598709	35.892839
1311.806572	92702.130420	35.897856
1312.791691	92821.484469	35.902874
1314.234092	92931.426691	35.907892
1315.451099	93058.755871	35.912909
1316.823544	93164.032904	35.917927
1318.241720	93291.496513	35.922944
1319.779977	93406.939008	35.927962
1320.860041	93533.619722	35.932980
1322.196698	93645.558236	35.937997
1323.562917	93760.800696	35.943015
1324.577156	93886.174927	35.948032
1325.728054	93999.512536	35.953050
1327.148321	94127.232794	35.958068
1328.442518	94251.005911	35.963085
1329.617894	94374.405091	35.968103
1330.859715	94500.088627	35.973120
1332.033758	94624.465002	35.978138
1333.519434	94753.609974	35.983156
1334.529139	94884.287231	35.988173
1336.122609	95012.681338	35.993191
1337.767822	95147.811251	35.998208
1338.840649	95267.224520	36.003226
1340.452517	95390.318978	36.008244
1341.400747	95511.438425	36.013261
1342.959517	95628.850760	36.018279
1344.227431	95745.142647	36.023296
1345.557111	95852.425596	36.028314
1347.250980	95970.908305	36.033332
1347.980435	96085.396583	36.038349
1349.322584	96187.164766	36.043367
1350.600044	96313.724727	36.048384
1351.947566	96429.322274	36.053402
1353.562918	96540.936326	36.058420
1355.152937	96657.181473	36.063437
1356.292980	96776.678787	36.068455
1357.505732	96896.279324	36.073472
1358.627788	97017.339518	36.078490
1360.232167	97139.820901	36.083508
1361.455087	97282.187848	36.088525
1362.452650	97402.584379	36.093543
1363.777441	97545.304270	36.098560
1365.210011	97665.355214	36.103578
1366.656553	97796.661168	36.108596
1367.847264	97944.119385	36.113613
1369.180343	98073.352513	36.118631
1370.805427	98217.892157	36.123648
1371.926924	98356.159803	36.128666
1373.626385	98491.054806	36.133684
1374.644721	98629.022775	36.138701
1376.417908	98778.397139	36.143719
1378.081518	98902.410018	36.148736
1379.778395	99045.167471	36.153754
1381.081526	99182.370914	36.158772
1382.206318	99324.077721	36.163789
1383.419871	99448.872687	36.168807
1385.219463	99585.214598	36.173824
1386.489263	99717.253217	36.178842
1388.088966	99850.420019	36.183860
1389.468435	99985.764127	36.188877
1391.004622	100121.578829	36.193895
1392.738736	100249.084909	36.198912
1393.978919	100388.788082	36.203930
1395.207399	100521.774564	36.208948
1396.625961	100666.015097	36.213965
1398.027456	100794.031492	36.218983
1399.533897	100930.488106	36.224000
1400.913638	101064.163223	36.229018
1402.434586	101185.430665	36.234036
1403.950211	101323.827211	36.239053
1405.362157	101443.109473	36.244071
1406.595056	101584.200818	36.249088
1408.221164	101719.158789	36.254106
1410.260037	101852.379563	36.259124
1410.982337	101990.724922	36.264141
1412.493811	102118.615300	36.269159
1414.570055	102255.128229	36.274176
1415.222917	102377.359298	36.279194
1416.663902	102507.201942	36.284212
1417.627186	102641.632961	36.289229
1419.424338	102785.228044	36.294247
1420.955530	102914.297546	36.299264
1422.144443	103055.287955	36.304282
1423.546537	103193.253633	36.309300
1424.825609	103338.275692	36.314317
1426.129273	103490.546787	36.319335
1427.693084	103624.254397	36.324352
1429.115504	103766.010249	36.329370
1430.559236	103890.570830	36.334388
1432.205159	104030.670128	36.339405
1433.389704	104179.679078	36.344423
1434.827320	104314.816474	36.349440
1436.325359	104450.147877	36.354458
1437.533760	104582.507274	36.359476
1438.547206	104718.904162	36.364493
1440.060584	104840.414443	36.369511
1441.555983	104965.604955	36.374528
1442.391057	105100.027829	36.379546
1444.241520	105245.577854	36.384564
1445.292937	105382.339229	36.389581
1446.662435	105516.934177	36.394599
1448.223383	105653.693424	36.399616
1449.801351	105805.108188	36.404634
1451.228466	105942.117667	36.409652
1452.931304	106082.457586	36.414669
1454.323251	106223.949614	36.419687
1456.717329	106339.913970	36.424704
1458.311371	106486.029123	36.429722
1459.563835	106615.828313	36.434740
1460.682574	106749.490836	36.439757
1462.462601	106889.822079	36.444775
1463.822597	107029.458471	36.449792
1465.006673	107177.656528	36.454810
1466.491034	107316.704133	36.459828
1468.005321	107466.994994	36.464845
1469.072142	107604.232082	36.469863
1471.192600	107750.473596	36.474880
1472.096786	107902.877496	36.479898
1473.662641	108052.211864	36.484916
1475.147053	108185.696271	36.489933
1476.415910	108341.950942	36.494951
1478.276663	108490.417073	36.499968
1479.929645	108646.955712	36.504986
1481.410528	108788.888313	36.510004
1483.033162	108935.529352	36.515021
1484.295067	109086.842972	36.520039
1485.749230	109240.498649	36.525056
1487.850308	109397.008970	36.530074
1489.154904	109528.484907	36.535092
1490.297560	109684.029764	36.540109
1491.737884	109844.347795	36.545127
1493.505111	109976.400147	36.550144
1495.025453	110142.591136	36.555162
1496.500759	110290.744502	36.560180
1497.999792	110440.581414	36.565197
1499.460185	110595.776511	36.570215
1501.295589	110742.404696	36.575232
1502.328879	110917.793089	36.580250
1504.188024	111055.770118	36.585268
1505.655474	111203.839776	36.590285
1507.266011	111358.292005	36.595303
1509.305846	111505.931434	36.600320
1510.779826	111649.639439	36.605338
1512.188179	111793.649922	36.610356
1514.218035	111940.671303	36.615373
1515.255322	112088.824285	36.620391
1517.107630	112219.185087	36.625408
1518.210606	112365.249154	36.630426
1519.928158	112506.234121	36.635444
1521.888850	112648.703651	36.640461
1523.070110	112798.105369	36.645479
1525.065536	112935.370955	36.650496
1526.447454	113081.191607	36.655514
1527.627496	113225.332161	36.660532
1529.024745	113365.089441	36.665549
1530.260934	113513.306121	36.670567
1531.902864	113659.684715	36.675584
1532.988577	113815.028220	36.680602
1534.593973	113957.393352	36.685620
1536.180849	114109.248509	36.690637
1537.468390	114259.565560	36.695655
1538.952541	114402.331786	36.700672
1540.317868	114544.051715	36.705690
1541.610980	114680.697632	36.710708
1543.447974	114831.426151	36.715725
1544.549975	114975.446286	36.720743
1545.961332	115116.108588	36.725760
1547.752153	115270.930014	36.730778
1549.128565	115407.844705	36.735796
1550.656992	115569.113168	36.740813
1552.175139	115729.851244	36.745831
1553.733949	115887.286056	36.750848
1554.720714	116047.296494	36.755866
1556.535538	116210.298841	36.760884
1558.137257	116372.916522	36.765901
1559.539026	116526.928618	36.770919
1561.457766	116698.960229	36.775936
1562.895227	116857.052221	36.780954
1564.808585	117016.212339	36.785972
1566.464601	117182.858496	36.790989
1568.120157	117345.713037	36.796007
1569.739247	117499.213343	36.801024
1571.413914	117666.137792	36.806042
1572.927097	117827.228166	36.811060
1574.548983	117982.975062	36.816077
1576.169212	118153.702643	36.821095
1577.882381	118310.971450	36.826112
1579.289574	118482.875240	36.831130
1580.949147	118659.040459	36.836148
1582.541738	118824.815869	36.841165
1583.975937	118995.360570	36.846183
1585.753634	119149.565907	36.851200
1587.124957	119324.371117	36.856218
1588.979549	119494.662359	36.861236
1590.676002	119652.408647	36.866253
1592.226339	119826.566753	36.871271
1594.011207	119999.344581	36.876288
1595.640331	120162.963737	36.881306
1596.902189	120342.192204	36.886324
1598.417778	120505.779750	36.891341
1599.672763	120690.173605	36.896359
1601.309509	120857.181371	36.901376
1603.442733	121040.323937	36.906394
1604.981820	121213.056661	36.911412
1606.598971	121382.708221	36.916429
1608.113676	121559.429387	36.921447
1610.331524	121724.346194	36.926464
1611.540833	121912.748790	36.931482
1613.448014	122079.643604	36.936500
1614.946170	122253.364075	36.941517
1616.308951	122435.770508	36.946535
1618.204182	122610.280679	36.951552
1619.558371	122787.933039	36.956570
1620.887009	122962.393414	36.961588
1622.731320	123132.359704	36.966605
1624.080274	123328.739287	36.971623
1625.763889	123500.723821	36.976640
1627.564479	123678.906933	36.981658
1629.262647	123863.665368	36.986676
1631.035723	124038.315019	36.991693
1632.664021	124217.592972	36.996711
1634.253803	124399.782822	37.001728
1635.585636	124576.254169	37.006746
1637.045374	124762.068751	37.011764
1639.040779	124937.550378	37.016781
1640.632818	125130.856297	37.021799
1642.322594	125306.767687	37.026816
1644.240648	125480.132414	37.031834
1645.575320	125661.416200	37.036852
1647.450243	125818.931072	37.041869
1648.623542	125991.031072	37.046887
1650.104832	126146.883113	37.051904
1652.105431	126324.323672	37.056922
1653.386113	126488.238873	37.061940
1654.945759	126656.894209	37.066957
1656.053620	126837.520755	37.071975
1657.926206	127007.676614	37.076992
1659.115199	127189.484642	37.082010
1660.662174	127374.955031	37.087028
1662.674335	127556.661933	37.092045
1664.108906	127754.432542	37.097063
1665.858591	127932.972121	37.102080
1667.402670	128128.659469	37.107098
1668.903172	128320.548349	37.112116
1670.888846	128513.149212	37.117133
1672.839602	128712.239637	37.122151
1675.301644	128890.038079	37.127168
1676.925617	129075.288380	37.132186
1678.679444	129263.031417	37.137204
1680.226091	129442.154609	37.142221
1681.742825	129638.436897	37.147239
1683.529333	129822.574051	37.152256
1684.762286	130018.559702	37.157274
1686.016264	130220.379377	37.162292
1687.805338	130422.319733	37.167309
1689.438717	130633.395213	37.172327
1691.019553	130840.483196	37.177344
1692.429093	131053.397282	37.182362
1694.330940	131261.921842	37.187380
1696.389353	131467.415948	37.192397
1697.795242	131675.639058	37.197415
1699.393119	131885.013303	37.202432
1701.642630	132083.184826	37.207450
1703.356624	132301.894335	37.212468
1705.731226	132494.934836	37.217485
1707.329867	132705.074227	37.222503
1709.121739	132911.745943	37.227520
1710.931733	133106.793005	37.232538
1712.225893	133319.177871	37.237556
1714.060219	133531.606580	37.242573
1715.801399	133736.285241	37.247591
1717.616255	133945.457943	37.252608
1719.723717	134137.037269	37.257626
1721.682998	134343.385114	37.262644
1724.072162	134524.580728	37.267661
1725.966978	134720.636840	37.272679
1727.155302	134924.074668	37.277696
1729.039347	135113.269336	37.282714
1730.623982	135309.985391	37.287732
1732.166707	135506.010917	37.292749
1733.640800	135709.496654	37.297767
1734.742057	135909.462909	37.302784
1736.317768	136115.066485	37.307802
1738.064312	136334.882103	37.312820
1740.000195	136546.573330	37.317837
1741.645844	136763.792660	37.322855
1743.312853	136986.199807	37.327872
1744.821002	137205.434927	37.332890
1746.266897	137429.718662	37.337908
1748.466910	137650.789777	37.342925
1749.835976	137858.400294	37.347943
1751.801857	138084.535163	37.352960
1753.517215	138301.446342	37.357978
1755.346580	138535.827853	37.362996
1756.966820	138748.492021	37.368013
1758.554831	138974.740789	37.373031
1760.316964	139194.428016	37.378048
1761.719220	139407.014887	37.383066
1762.986744	139619.902877	37.388084
1765.323319	139830.100028	37.393101
1766.960901	140043.630312	37.398119
1768.435720	140259.166631	37.403136
1770.717270	140468.245709	37.408154
1772.418751	140684.789315	37.413172
1774.167525	140880.120198	37.418189
1776.246537	141102.254346	37.423207
1778.042315	141319.268398	37.428224
1779.970518	141524.282535	37.433242
1781.837022	141739.269606	37.438260
1783.486186	141942.006485	37.443277
1785.610274	142165.229947	37.448295
1786.888237	142381.301373	37.453312
1788.746318	142588.247293	37.458330
1790.135477	142822.286876	37.463348
1792.264607	143042.911849	37.468365
1794.078011	143262.089363	37.473383
1795.655392	143480.466948	37.478400
1797.860735	143711.451998	37.483418
1799.444105	143943.804089	37.488436
1801.402468	144165.742507	37.493453
1802.902193	144400.191179	37.498471
1805.179796	144642.160337	37.503488
1806.893267	144863.403845	37.508506
1808.542869	145093.326832	37.513524
1810.452111	145337.323912	37.518541
1811.727912	145571.013303	37.523559
1813.374700	145813.124337	37.528576
1815.597419	146055.083427	37.533594
1817.050275	146307.126859	37.538612
1818.645413	146543.893293	37.543629
1820.602347	146798.437216	37.548647
1821.892857	147061.970786	37.553664
1824.152352	147316.889027	37.558682
1825.691300	147575.106485	37.563700
1827.499341	147838.461915	37.568717
1829.841915	148092.203311	37.573735
1831.721497	148346.766865	37.578752
1833.692916	148595.922938	37.583770
1835.269578	148863.457365	37.588788
1837.134711	149121.999766	37.593805
1839.182704	149382.114278	37.598823
1840.768101	149640.905826	37.603840
1842.744507	149903.585318	37.608858
1844.424500	150164.865213	37.613876
1846.609784	150428.492135	37.618893
1848.245564	150689.794149	37.623911
1850.298291	150960.108252	37.628928
1852.585612	151212.718007	37.633946
1854.149497	151475.926302	37.638964
1856.234679	151742.316959	37.643981
1858.024952	152005.124448	37.648999
1860.030527	152264.218532	37.654016
1862.043524	152527.933173	37.659034
1863.935206	152779.672366	37.664052
1865.511068	153051.061069	37.669069
1867.276323	153299.344181	37.674087
1869.259816	153566.546436	37.679104
1870.738930	153828.662012	37.684122
1872.711756	154102.596272	37.689140
1875.141409	154348.203706	37.694157
1877.304598	154603.221951	37.699175
1878.998044	154854.633123	37.704192
1881.061558	155098.879019	37.709210
1882.852491	155356.103877	37.714228
1884.934596	155612.027822	37.719245
1886.899816	155841.477831	37.724263
1888.402099	156079.556866	37.729280
1890.288436	156304.971442	37.734298
1891.574145	156548.468569	37.739316
1893.439874	156787.103256	37.744333
1895.357288	157027.736623	37.749351
1897.046764	157290.444494	37.754368
1898.470155	157531.067928	37.759386
1900.786933	157774.295375	37.764404
1902.143551	158038.873709	37.769421
1904.050782	158303.075530	37.774439
1905.497167	158567.756472	37.779456
1907.274142	158836.106772	37.784474
1908.983726	159121.416724	37.789492
1910.761256	159394.771274	37.794509
1912.275563	159685.611259	37.799527
1913.771679	159983.069697	37.804544
1915.880552	160254.370639	37.809562
1917.555142	160560.183001	37.814580
1919.572336	160865.981627	37.819597
1921.903409	161167.492586	37.824615
1923.481875	161464.043882	37.829632
1925.563339	161760.594458	37.834650
1927.916204	162070.053807	37.839668
1929.881312	162377.061241	37.844685
1931.875662	162670.963489	37.849703
1933.646517	162982.726896	37.854720
1935.458777	163289.864031	37.859738
1937.640769	163599.788978	37.864756
1939.905219	163915.834766	37.869773
1941.720358	164211.727055	37.874791
1943.285278	164530.969822	37.879808
1945.918002	164842.493664	37.884826
1948.013731	165158.520852	37.889844
1950.054679	165468.006725	37.894861
1952.134017	165773.298221	37.899879
1953.855924	166094.834742	37.904896
1956.007354	166400.689177	37.909914
1957.868244	166720.264438	37.914932
1959.256405	167034.467884	37.919949
1961.483657	167350.738697	37.924967
1963.264677	167676.006231	37.929984
1965.203725	167990.559943	37.935002
1967.125550	168310.666283	37.940020
1969.435550	168629.621720	37.945037
1971.493144	168949.912963	37.950055
1973.398763	169276.222306	37.955072
1975.540109	169589.316827	37.960090
1978.118520	169905.874496	37.965108
1980.249549	170219.849448	37.970125
1982.414840	170524.081596	37.975143
1984.352884	170834.140353	37.980160
1986.390682	171140.375667	37.985178
1988.674677	171452.655999	37.990196
1990.251635	171764.196938	37.995213
1992.284496	172061.434263	38.000231
1994.495281	172377.323227	38.005248
1996.646720	172691.026044	38.010266
1998.621955	172996.110434	38.015284
2000.781798	173300.443529	38.020301
2002.686878	173597.782887	38.025319
2004.188391	173916.201125	38.030336
2006.143506	174225.407572	38.035354
2008.107987	174532.340839	38.040372
2009.810226	174860.597953	38.045389
2012.071859	175176.718903	38.050407
2013.713325	175491.401144	38.055424
2015.718911	175803.107366	38.060442
2017.705358	176109.941652	38.065460
2019.679587	176402.379181	38.070477
2021.968574	176691.251337	38.075495
2024.356390	176987.702720	38.080512
2026.143557	177284.642288	38.085530
2027.763616	177574.142241	38.090548
2029.846899	177887.139447	38.095565
2031.783341	178184.566886	38.100583
2033.698928	178487.890735	38.105600
2035.567511	178803.185052	38.110618
2037.903495	179093.061275	38.115636
2039.353584	179408.219739	38.120653
2041.692799	179722.834600	38.125671
2043.613449	180043.890511	38.130688
2045.364809	180368.758178	38.135706
2047.232126	180689.850109	38.140724
2049.254735	181016.201765	38.145741
2051.124584	181345.270547	38.150759
2052.882059	181693.914477	38.155776
2054.873957	182036.453090	38.160794
2056.884036	182379.828276	38.165812
2058.795117	182727.690228	38.170829
2060.909994	183078.010786	38.175847
2062.662231	183445.964829	38.180864
2064.580378	183802.287303	38.185882
2066.708783	184164.140675	38.190900
2068.635988	184539.157869	38.195917
2070.966795	184914.977238	38.200935
2072.834475	185281.675673	38.205952
2074.656883	185660.751837	38.210970
2076.863700	186040.582365	38.215988
2078.757487	186420.437620	38.221005
2080.934892	186871.723920	38.226023
2083.120256	187256.591324	38.231040
2085.646418	187634.854009	38.236058
2087.843517	188016.674398	38.241076
2089.979735	188398.023020	38.246093
2092.102661	188786.563195	38.251111
2094.293520	189169.353791	38.256128
2096.479343	189543.256493	38.261146
2098.647758	189928.694784	38.266164
2100.934975	190300.425207	38.271181
2103.787025	190688.579090	38.276199
2105.138495	191073.284761	38.281216
2107.544933	191442.257057	38.286234
2109.900585	191815.200882	38.291252
2112.342584	192206.090634	38.296269
2114.245068	192564.120969	38.301287
2116.498910	192944.221698	38.306304
2118.624299	193323.276751	38.311322
2120.953849	193686.908247	38.316340
2123.316484	194059.629176	38.321357
2125.549703	194412.050514	38.326375
2127.787272	194796.020287	38.331392
2129.825818	195161.453906	38.336410
2131.733185	195541.641661	38.341428
2133.710937	195921.133701	38.346445
2136.304036	196274.113604	38.351463
2138.544412	196644.092064	38.356480
2139.978973	197027.837523	38.361498
2142.390362	197390.856724	38.366516
2144.117403	197771.053252	38.371533
2145.868021	198154.269909	38.376551
2148.243095	198533.453105	38.381568
2150.421519	198924.759145	38.386586
2152.489042	199297.590870	38.391604
2154.615924	199692.234550	38.396621
2156.110207	200074.810109	38.401639
2158.523547	200435.219953	38.406656
2160.181714	200811.268843	38.411674
2162.447656	201174.802338	38.416692
2164.286177	201542.950156	38.421709
2166.149610	201928.317673	38.426727
2168.597447	202306.025206	38.431744
2170.340744	202700.913640	38.436762
2172.780535	203075.372579	38.441780
2173.765659	203474.089488	38.446797
2176.130141	203866.978630	38.451815
2178.372994	204272.334829	38.456832
2180.349250	204683.525204	38.461850
2182.718133	205087.669597	38.466868
2185.050889	205504.039194	38.471885
2187.216810	205922.112209	38.476903
2189.018974	206336.254434	38.481920
2190.917846	206760.645225	38.486938
2193.148785	207180.692072	38.491956
2195.324356	207623.763517	38.496973
2197.623368	208058.662232	38.501991
2200.000166	208498.452476	38.507008
2201.850109	208931.009414	38.512026
2204.144130	209365.250843	38.517044
2206.218427	209811.822425	38.522061
2208.612925	210269.192186	38.527079
2210.788278	210714.809683	38.532096
2213.150814	211153.209618	38.537114
2215.384870	211603.468256	38.542132
2217.906531	212057.112317	38.547149
2220.259538	212505.677211	38.552167
2222.779188	212947.916743	38.557184
2224.882983	213400.357656	38.562202
2227.778674	213845.639143	38.567220
2229.717866	214278.444444	38.572237
2232.436365	214727.565198	38.577255
2235.160649	215169.521747	38.582272
2237.659946	215607.042761	38.587290
2240.124799	216032.655236	38.592308
2242.413885	216461.750423	38.597325
2245.094352	216896.932857	38.602343
2247.787571	217322.257021	38.607360
2249.750858	217739.311879	38.612378
2252.311872	218157.163198	38.617396
2254.314884	218590.013796	38.622413
2256.614454	219020.989492	38.627431
2258.872627	219442.699495	38.632448
2260.753840	219870.184340	38.637466
2263.696563	220290.010076	38.642484
2265.268597	220724.402637	38.647501
2267.877477	221148.167617	38.652519
2270.180032	221578.712548	38.657536
2272.551142	221998.932962	38.662554
2274.858050	222420.459142	38.667572
2277.391348	222833.897151	38.672589
2279.244091	223256.866114	38.677607
2281.682486	223682.462285	38.682624
2283.433246	224115.710583	38.687642
2285.909040	224540.589798	38.692660
2287.816380	224983.010153	38.697677
2290.093615	225426.211322	38.702695
2291.966870	225859.898037	38.707712
2294.276379	226308.302047	38.712730
2296.590754	226744.435100	38.717748
2298.579865	227194.413156	38.722765
2300.995690	227641.885947	38.727783
2302.864021	228087.386125	38.732800
2305.046372	228542.516280	38.737818
2307.606771	228993.878473	38.742836
2309.650350	229424.718250	38.747853
2311.585033	229857.099056	38.752871
2313.885631	230300.905360	38.757888
2315.678062	230736.686650	38.762906
2318.150997	231181.151600	38.767924
2319.878480	231625.783114	38.772941
2322.639782	232076.807688	38.777959
2325.356691	232516.762735	38.782976
2327.603621	232969.619600	38.787994
2329.989910	233419.837817	38.793012
2332.547253	233868.504807	38.798029
2334.886818	234321.879608	38.803047
2337.699105	234763.977319	38.808064
2339.864566	235219.131219	38.813082
2342.104030	235671.707346	38.818100
2344.587100	236125.616874	38.823117
2346.825191	236583.654014	38.828135
2349.345488	237036.794577	38.833152
2351.508870	237496.823714	38.838170
2353.794491	237962.091781	38.843188
2356.580120	238436.020236	38.848205
2358.881683	238893.765048	38.853223
2360.917812	239362.321599	38.858240
2363.087662	239833.498579	38.863258
2365.738757	240316.285495	38.868276
2367.837482	240791.790562	38.873293
2370.624982	241274.529186	38.878311
2373.272185	241748.880268	38.883328
2375.765784	242216.344690	38.888346
2378.359194	242691.108834	38.893364
2380.153680	243175.598781	38.898381
2382.262245	243667.253341	38.903399
2385.350904	244137.974618	38.908416
2387.339554	244626.800616	38.913434
2389.397177	245120.974806	38.918452
2391.844762	245616.433512	38.923469
2394.475130	246109.068276	38.928487
2396.854792	246601.588437	38.933504
2398.871488	247108.592588	38.938522
2401.544912	247600.150011	38.943540
2403.980316	248103.428370	38.948557
2405.956790	248608.808972	38.953575
2408.652290	249118.318460	38.958592
2410.834910	249625.289845	38.963610
2412.992210	250143.135849	38.968628
2415.810810	250647.312577	38.973645
2418.501001	251169.467040	38.978663
2421.091579	251676.241687	38.983680
2422.868118	252187.993167	38.988698
2425.654113	252710.940500	38.993716
2428.045117	253225.768134	38.998733
2430.589904	253747.352312	39.003751
2433.146844	254254.225218	39.008768
2435.399312	254772.752211	39.013786
2438.067163	255291.695286	39.018804
2440.316524	255808.771048	39.023821
2442.436357	256326.957261	39.028839
2445.039184	256854.083705	39.033856
2447.345681	257380.009508	39.038874
2449.815503	257904.891724	39.043892
2452.303700	258422.529690	39.048909
2454.709780	258954.682100	39.053927
2457.755564	259469.892073	39.058944
2460.198341	259999.798981	39.063962
2462.927854	260510.456241	39.068980
2465.625970	261032.038287	39.073997
2467.759131	261556.220525	39.079015
2470.362653	262060.184941	39.084032
2472.636767	262550.228414	39.089050
2475.220102	263036.691036	39.094068
2477.541788	263530.431136	39.099085
2479.301255	264029.006203	39.104103
2481.724657	264525.519867	39.109120
2483.916925	265030.601345	39.114138
2486.103829	265549.066596	39.119156
2488.645175	266055.815898	39.124173
2490.946686	266581.598415	39.129191
2493.190765	267099.335688	39.134208
2495.359369	267632.981578	39.139226
2498.196217	268158.672412	39.144244
2500.952005	268685.490528	39.149261
2503.044293	269231.660873	39.154279
2505.494903	269768.806754	39.159296
2508.045412	270316.677326	39.164314
2510.200836	270858.866210	39.169332
2512.847453	271412.124987	39.174349
2515.015340	271975.410671	39.179367
2517.404386	272530.353427	39.184384
2519.902362	273100.488619	39.189402
2522.455285	273667.335287	39.194420
2525.221555	274236.303724	39.199437
2527.685499	274808.896303	39.204455
2530.514349	275376.729816	39.209472
2532.905195	275963.141489	39.214490
2536.166149	276536.588495	39.219508
2538.843400	277103.849458	39.224525
2541.333274	277689.064949	39.229543
2543.705832	278269.037467	39.234560
2546.331639	278839.798526	39.239578
2548.483909	279429.091354	39.244596
2551.787416	280008.956693	39.249613
2553.940316	280596.259542	39.254631
2556.418096	281180.104335	39.259648
2559.063424	281769.378230	39.264666
2561.603802	282361.584033	39.269684
2564.741641	282952.727035	39.274701
2567.645843	283539.102087	39.279719
2570.288459	284115.076236	39.284736
2573.228015	284703.696115	39.289754
2575.405559	285288.163538	39.294772
2578.092218	285870.718471	39.299789
2580.061272	286464.222769	39.304807
2583.442192	287055.902399	39.309824
2585.964441	287633.084473	39.314842
2588.295297	288237.892414	39.319860
2591.216715	288817.464998	39.324877
2593.754830	289420.325323	39.329895
2596.622917	290003.628109	39.334912
2599.552683	290582.370944	39.339930
2602.011494	291176.847911	39.344948
2604.540536	291751.376666	39.349965
2606.974780	292341.402972	39.354983
2609.758540	292925.681827	39.360000
2612.408992	293516.704136	39.365018
2614.931977	294099.311133	39.370036
2617.998674	294679.492017	39.375053
2620.325747	295263.260636	39.380071
2622.706271	295848.513085	39.385088
2625.596865	296450.995323	39.390106
2627.957565	297045.708742	39.395124
2630.793392	297627.038690	39.400141
2633.068098	298215.355506	39.405159
2635.759358	298806.927132	39.410176
2638.556190	299395.429597	39.415194
2640.941975	299990.590412	39.420212
2643.565775	300571.719651	39.425229
2646.035188	301148.830280	39.430247
2648.764648	301711.195673	39.435264
2651.582488	302267.626502	39.440282
2653.790947	302834.706811	39.445300
2656.176939	303402.134206	39.450317
2659.001026	303984.439151	39.455335
2661.588564	304551.086573	39.460352
2664.189842	305121.533348	39.465370
2666.596273	305702.970136	39.470388
2669.268412	306281.795173	39.475405
2672.017142	306882.609358	39.480423
2674.705646	307454.869414	39.485440
2677.664573	308044.595183	39.490458
2680.020748	308637.631360	39.495476
2682.469390	309233.031964	39.500493
2685.412440	309843.501545	39.505511
2687.881331	310448.833957	39.510528
2690.703522	311046.337035	39.515546
2693.078758	311666.618405	39.520564
2695.764426	312279.863625	39.525581
2698.141063	312904.417933	39.530599
2700.628768	313520.165075	39.535616
2703.274004	314165.091786	39.540634
2705.404279	314804.023923	39.545652
2708.741556	315437.404321	39.550669
2711.095291	316089.912303	39.555687
2713.598988	316748.605241	39.560704
2716.788267	317398.248742	39.565722
2719.592377	318044.973514	39.570740
2722.385120	318705.851135	39.575757
2725.101216	319362.315151	39.580775
2728.163601	320018.182484	39.585792
2730.677809	320680.621481	39.590810
2733.702409	321344.620268	39.595828
2736.537824	322003.842220	39.600845
2739.864523	322657.800973	39.605863
2742.227426	323317.101337	39.610880
2745.247606	323972.990381	39.615898
2748.304460	324630.208168	39.620916
2751.660457	325272.829989	39.625933
2754.577546	325927.968164	39.630951
2757.630153	326581.856824	39.635968
2760.322559	327224.348125	39.640986
2763.162754	327881.800860	39.646004
2766.472549	328518.517428	39.651021
2769.021450	329169.042485	39.656039
2771.986734	329809.013996	39.661056
2774.800954	330439.002745	39.666074
2777.421620	331092.808183	39.671092
2780.198192	331735.821755	39.676109
2781.986886	332385.954737	39.681127
2784.875692	333044.885880	39.686144
2787.923844	333704.389628	39.691162
2789.855553	334373.086422	39.696180
2792.844256	335031.967343	39.701197
2796.295562	335686.858180	39.706215
2798.735056	336351.508670	39.711232
2801.952933	337016.381164	39.716250
2804.104737	337683.233782	39.721268
2807.068823	338346.726461	39.726285
2809.919893	339008.220784	39.731303
2812.540273	339685.337593	39.736320
2815.531218	340352.644396	39.741338
2817.833420	341024.382903	39.746356
2820.525453	341695.490010	39.751373
2823.447670	342370.403487	39.756391
2826.258103	343057.317257	39.761408
2829.273273	343720.878920	39.766426
2831.919959	344374.594609	39.771444
2834.876529	345019.348292	39.776461
2837.540247	345670.399161	39.781479
2839.985230	346327.836690	39.786496
2843.003058	346964.860137	39.791514
2845.861366	347623.450626	39.796532
2848.476802	348274.230464	39.801549
2850.958973	348929.607915	39.806567
2853.333027	349602.611953	39.811584
2856.028168	350265.993054	39.816602
2858.954739	350958.534145	39.821620
2861.453892	351637.511424	39.826637
2864.069060	352341.354368	39.831655
2866.669310	353042.141776	39.836672
2869.953974	353745.089113	39.841690
2872.369979	354452.719567	39.846708
2874.990214	355166.716489	39.851725
2878.540320	355883.138354	39.856743
2881.191901	356604.043987	39.861760
2884.102039	357315.538400	39.866778
2887.031454	358053.656032	39.871796
2890.222963	358774.452403	39.876813
2893.384145	359508.291003	39.881831
2896.060718	360236.940291	39.886848
2899.282926	360974.764234	39.891866
2902.183912	361709.502426	39.896884
2905.355627	362446.132092	39.901901
2908.412153	363192.823581	39.906919
2911.280522	363936.686894	39.911936
2914.441038	364661.325766	39.916954
2917.415774	365409.621115	39.921972
2920.595732	366131.179258	39.926989
2924.016439	366866.924299	39.932007
2926.645800	367610.224121	39.937024
2929.883251	368331.692862	39.942042
2932.920973	369076.918277	39.947060
2936.173388	369798.195439	39.952077
2939.293025	370529.965162	39.957095
2942.061843	371251.736430	39.962112
2945.715982	371985.817408	39.967130
2948.569057	372713.745414	39.972148
2952.056278	373434.714768	39.977165
2955.016361	374158.027467	39.982183
2957.666081	374889.324540	39.987200
2960.502951	375615.328661	39.992218
2963.782505	376348.439201	39.997236
2966.382417	377076.315662	40.002253
2969.697332	377795.346831	40.007271
2971.925073	378540.264689	40.012288
2975.073365	379271.542420	40.017306
2977.983666	380011.854501	40.022324
2980.908192	380741.175909	40.027341
2984.327670	381486.027813	40.032359
2987.064363	382231.800512	40.037376
2990.134516	382951.463452	40.042394
2993.293946	383686.288387	40.047412
2995.897108	384431.993007	40.052429
2999.171332	385167.517406	40.057447
3002.131268	385914.414776	40.062464
3005.181055	386657.097756	40.067482
3007.798463	387403.320707	40.072500
3010.413897	388157.042452	40.077517
3014.022487	388905.117507	40.082535
3017.118416	389649.704952	40.087552
3019.982683	390398.382541	40.092570
3023.086409	391147.557139	40.097588
3025.991825	391898.360083	40.102605
3028.751820	392621.414591	40.107623
3031.351198	393354.042320	40.112640
3034.177989	394076.536721	40.117658
3037.455927	394815.596669	40.122676
3040.358238	395531.403007	40.127693
3043.706318	396257.193372	40.132711
3046.394407	396989.139385	40.137728
3049.408508	397711.798426	40.142746
3052.653217	398434.500674	40.147764
3055.274375	399167.705659	40.152781
3058.625932	399904.469212	40.157799
3060.933248	400655.848659	40.162816
3064.551182	401392.472930	40.167834
3067.710512	402137.091542	40.172852
3070.224534	402893.073135	40.177869
3073.385493	403658.089718	40.182887
3076.305639	404420.182720	40.187904
3079.074975	405180.856557	40.192922
3081.962556	405957.022458	40.197940
3084.700473	406742.496056	40.202957
3088.078625	407523.591840	40.207975
3091.090034	408320.808365	40.212992
3094.059811	409123.214410	40.218010
3097.399297	409925.533769	40.223028
3100.299103	410723.895239	40.228045
3103.846649	411530.778268	40.233063
3106.341020	412342.753273	40.238080
3110.034307	413158.103188	40.243098
3113.171779	413973.255871	40.248116
3116.201046	414797.297586	40.253133
3119.472487	415607.966350	40.258151
3122.590777	416437.495155	40.263168
3125.544065	417268.736925	40.268186
3128.546967	418089.468643	40.273204
3132.107327	418930.059073	40.278221
3135.313295	419761.921624	40.283239
3138.177252	420600.226827	40.288256
3141.596075	421432.343456	40.293274
3145.116112	422269.821576	40.298292
3147.616097	423114.351838	40.303309
3151.277681	423957.453006	40.308327
3154.477274	424802.765354	40.313344
3157.840336	425647.107009	40.318362
3160.839077	426485.959354	40.323380
3163.933497	427336.895102	40.328397
3167.339263	428183.954806	40.333415
3170.873799	429042.989623	40.338432
3174.044113	429880.661899	40.343450
3177.254483	430727.845781	40.348468
3180.282903	431587.960907	40.353485
3183.892895	432437.384533	40.358503
3186.852940	433289.348825	40.363520
3189.589539	434146.819196	40.368538
3193.120988	434991.190859	40.373556
3196.353774	435855.077875	40.378573
3199.929298	436696.740150	40.383591
3202.896487	437553.214461	40.388608
3206.343497	438400.986114	40.393626
3209.805097	439250.132301	40.398644
3213.090237	440105.532514	40.403661
3216.263062	440959.698860	40.408679
3219.196106	441806.791173	40.413696
3222.502613	442647.624104	40.418714
3225.981359	443498.747330	40.423732
3229.423330	444342.715191	40.428749
3232.962381	445184.760531	40.433767
3236.609377	446031.851569	40.438784
3239.526886	446876.794761	40.443802
3242.871212	447700.118885	40.448820
3245.584842	448504.465731	40.453837
3248.551207	449298.941134	40.458855
3251.882196	450108.422634	40.463872
3255.075328	450912.940864	40.468890
3257.950632	451717.724830	40.473908
3260.810880	452529.240156	40.478925
3264.169897	453343.114575	40.483943
3267.128436	454174.733397	40.488960
3269.582907	454992.155918	40.493978
3273.102694	455824.770488	40.498996
3276.349622	456677.224872	40.504013
3279.411923	457524.316139	40.509031
3282.472731	458377.978001	40.514048
3285.655275	459243.035104	40.519066
3288.933305	460098.092185	40.524084
3291.980966	460974.034303	40.529101
3295.264697	461850.096678	40.534119
3298.245836	462729.743617	40.539136
3301.111424	463632.774231	40.544154
3304.740632	464529.533032	40.549172
3308.158152	465444.590335	40.554189
3311.233678	466352.437008	40.559207
3314.916286	467269.774773	40.564224
3317.879751	468182.835910	40.569242
3321.135210	469106.847432	40.574260
3323.910107	470038.094381	40.579277
3327.418691	470971.796974	40.584295
3331.015000	471921.519929	40.589312
3334.020776	472869.665840	40.594330
3337.768789	473811.085802	40.599348
3341.255917	474769.987813	40.604365
3344.984132	475707.821276	40.609383
3349.328852	476652.209293	40.614400
3352.527337	477585.225896	40.619418
3356.481378	478527.648117	40.624436
3359.924341	479468.632136	40.629453
3363.360362	480399.278949	40.634471
3366.879392	481335.401934	40.639488
3370.128439	482268.840039	40.644506
3374.125921	483198.225589	40.649524
3377.729933	484143.137483	40.654541
3381.223295	485070.272353	40.659559
3384.561374	485999.290440	40.664576
3387.698302	486935.790773	40.669594
3391.172486	487867.748113	40.674612
3394.715214	488795.859771	40.679629
3398.490075	489728.764956	40.684647
3401.837337	490659.211206	40.689664
3404.998945	491591.341579	40.694682
3408.474023	492513.494211	40.699700
3411.957360	493451.452534	40.704717
3415.630674	494384.588878	40.709735
3418.913624	495319.892780	40.714752
3422.431355	496249.512264	40.719770
3426.166992	497180.247791	40.724788
3428.972244	498118.570721	40.729805
3432.077163	499055.427881	40.734823
3435.682122	499988.623593	40.739840
3438.822653	500941.512912	40.744858
3442.295243	501879.540870	40.749876
3445.509604	502842.511215	40.754893
3448.701318	503795.204824	40.759911
3453.060608	504742.420156	40.764928
3456.194418	505689.361001	40.769946
3459.548047	506642.343291	40.774964
3462.758198	507598.705275	40.779981
3466.489040	508552.909385	40.784999
3470.382270	509477.340836	40.790004
3473.646055	510382.341691	40.795008
3476.780370	511223.564146	40.800013
3479.905563	512011.589973	40.805018
3483.359968	512759.081720	40.810023
3486.654534	513452.912016	40.815028
3489.458558	514084.317282	40.820032
3492.461750	514657.786427	40.825037
3495.054043	515180.529788	40.830042
3497.372270	515640.634712	40.835047
3499.393829	516049.251564	40.840052
3501.387477	516422.977930	40.845056
3503.468477	516738.107250	40.850061
3504.843644	517017.197836	40.855066
3506.576231	517259.531973	40.860071
3508.130411	517454.660399	40.865076
3509.406754	517618.175497	40.870080
3510.762437	517730.365377	40.875085
3511.751403	517827.238375	40.880090
3512.905640	517888.550786	40.885095
3514.107743	517917.849574	40.890100
3514.593985	517923.217470	40.895104
3515.598056	517900.027054	40.900109
3516.242124	517872.507542	40.905114
3516.737569	517798.387955	40.910119
3517.368567	517720.214571	40.915124
3517.699086	517629.486479	40.920128
3518.388019	517517.481724	40.925133
3518.804236	517388.884855	40.930138
3519.205537	517237.757836	40.935143
3519.879126	517081.394951	40.940148
3519.739161	516914.924319	40.945152
3520.250373	516728.993899	40.950157
3520.213975	516550.001677	40.955162
3520.290695	516347.246985	40.960167
3520.137202	516144.121850	40.965172
3520.346375	515946.129539	40.970176
3520.710776	515728.298682	40.975181
3520.963893	515504.381860	40.980186
3520.572161	515287.266639	40.985191
3520.894845	515049.014383	40.990196
3520.976067	514818.055271	40.995200
3520.918021	514577.635899	41.000205
3520.776758	514340.451932	41.005210
3520.723178	514091.099749	41.010215
3520.685709	513848.799085	41.015220
3520.545691	513603.888366	41.020224
3520.531152	513353.256369	41.025229
3520.375552	513113.330976	41.030234
3520.120048	512859.399809	41.035239
3520.290561	512607.817992	41.040244
3520.006057	512356.907519	41.045248
3520.163982	512112.176289	41.050253
3519.760332	511862.183093	41.055258
3519.677275	511606.336536	41.060263
3519.737568	511357.018497	41.065268
3519.407959	511109.925088	41.070272
3519.576488	510861.438654	41.075277
3519.066033	510607.758363	41.080282
3518.590911	510354.975735	41.085287
3518.770121	510117.417894	41.090292
3518.380601	509877.574224	41.095296
3518.339203	509633.536773	41.100301
3518.428157	509403.697199	41.105306
3518.221804	509167.545044	41.110311
3518.144902	508928.191345	41.115316
3517.995768	508694.544154	41.120320
3517.695840	508453.552712	41.125325
3517.532723	508208.601690	41.130330
3516.952423	507971.579848	41.135335
3517.125307	507753.654436	41.140340
3516.775991	507534.646802	41.145344
3516.591989	507307.035018	41.150349
3516.518486	507087.069612	41.155354
3516.374939	506864.942653	41.160359
3516.569832	506641.397578	41.165364
3516.031853	506430.574183	41.170368
3515.492070	506215.510543	41.175373
3515.830067	506005.957023	41.180378
3515.664285	505799.505631	41.185383
3515.470994	505579.132014	41.190388
3514.767574	505386.782737	41.195392
3514.816779	505171.863964	41.200397
3515.090809	504973.303144	41.205402
3514.863202	504770.075296	41.210407
3515.015061	504569.762134	41.215412
3514.965746	504377.347964	41.220416
3514.701397	504166.448609	41.225421
3514.456326	503970.225054	41.230426
3514.198578	503774.051249	41.235431
3514.368082	503574.226006	41.240436
3514.001382	503390.879400	41.245440
3513.933735	503202.841981	41.250445
3513.360039	503012.862595	41.255450
3513.519666	502833.665354	41.260455
3513.132742	502641.028234	41.265460
3512.815491	502475.726214	41.270464
3513.263099	502287.798536	41.275469
3513.166899	502118.471766	41.280474
3513.009829	501933.005185	41.285479
3512.471406	501744.921141	41.290484
3512.518248	501580.107310	41.295488
3512.201847	501405.255700	41.300493
3512.194933	501242.363963	41.305498
3512.132880	501085.029945	41.310503
3512.424697	500910.229121	41.315508
3512.081906	500752.380087	41.320512
3511.984895	500582.934606	41.325517
3511.598828	500427.864365	41.330522
3511.585461	500269.151381	41.335527
3511.727460	500100.773357	41.340532
3511.219957	499957.324345	41.345536
3511.149390	499796.949709	41.350541
3510.854425	499644.683160	41.355546
3510.670998	499502.340019	41.360551
3510.972181	499353.308606	41.365556
3510.597605	499217.149687	41.370560
3510.617842	499061.042781	41.375565
3510.536634	498919.334178	41.380570
3510.369020	498776.779640	41.385575
3510.457794	498626.713995	41.390580
3510.332446	498500.856352	41.395584
3510.278086	498358.683906	41.400589
3509.953528	498217.612067	41.405594
3509.962983	498090.922363	41.410599
3509.549127	497955.666372	41.415604
3509.732906	497824.152203	41.420608
3509.537170	497681.995215	41.425613
3509.459642	497555.617288	41.430618
3509.681627	497431.463085	41.435623
3509.560209	497308.219373	41.440628
3509.110052	497195.827803	41.445632
3509.259646	497058.507303	41.450637
3509.005305	496939.319367	41.455642
3508.854596	496821.426769	41.460647
3509.189761	496689.071277	41.465652
3508.648976	496579.919740	41.470656
3508.643463	496457.862386	41.475661
3508.557247	496338.391045	41.480666
3508.295142	496223.388353	41.485671
3508.514629	496112.954022	41.490676
3508.414149	496012.412407	41.495680
3508.536388	495896.640640	41.500685
3508.335202	495779.353371	41.505690
3508.376775	495670.457877	41.510695
3508.518561	495553.115450	41.515700
3508.321350	495444.457386	41.520704
3508.069011	495333.484886	41.525709
3508.081707	495227.367205	41.530714
3507.894055	495119.664463	41.535719
3507.701621	495011.052971	41.540724
3507.624149	494914.236167	41.545728
3507.744772	494816.529665	41.550733
3507.629721	494710.226236	41.555738
3507.355465	494608.187606	41.560743
3507.366898	494507.214510	41.565748
3507.559293	494409.948547	41.570752
3507.465660	494314.039108	41.575757
3507.863468	494216.083593	41.580762
3507.320740	494115.194078	41.585767
3507.786914	494009.653493	41.590772
3507.265034	493924.663008	41.595776
3507.747815	493819.068006	41.600781
3507.630590	493716.241520	41.605786
3507.211262	493607.655116	41.610791
3507.608107	493514.239153	41.615796
3507.227445	493419.075485	41.620800
3507.347842	493318.329847	41.625805
3507.272330	493228.065485	41.630810
3507.112748	493142.761728	41.635815
3507.368421	493036.742138	41.640820
3507.080961	492954.133219	41.645824
3507.113381	492851.327999	41.650829
3506.853993	492755.333380	41.655834
3506.749490	492666.332443	41.660839
3506.732480	492573.378959	41.665844
3506.307903	492484.022810	41.670848
3506.387589	492394.890617	41.675853
3506.682740	492319.862475	41.680858
3506.687995	492237.355541	41.685863
3506.967044	492145.666174	41.690868
3506.581349	492058.826136	41.695872
3506.531514	491972.185805	41.700877
3506.531304	491874.428420	41.705882
3506.316614	491794.629506	41.710887
3506.389103	491710.291402	41.715892
3506.458209	491626.609796	41.720896
3506.360618	491547.346801	41.725901
3506.382693	491468.721217	41.730906
3506.049225	491389.999062	41.735911
3506.298874	491303.005303	41.740916
3505.897275	491232.271392	41.745920
3506.101851	491148.162077	41.750925
3505.809036	491071.906296	41.755930
3505.733261	490989.152654	41.760935
3506.126782	490915.465658	41.765940
3506.102788	490849.569492	41.770944
3506.132364	490762.051388	41.775949
3506.026216	490693.793901	41.780954
3505.557850	490618.724620	41.785959
3505.452094	490541.831070	41.790964
3505.438158	490478.507180	41.795968
3505.408947	490417.811381	41.800973
3505.580272	490332.137218	41.805978
3505.266311	490274.616148	41.810983
3505.038510	490200.971862	41.815988
3505.438226	490137.582179	41.820992
3505.260144	490073.575133	41.825997
3505.592313	490014.387007	41.831002
3505.342178	489949.633137	41.836007
3505.599295	489865.155015	41.841012
3505.381269	489803.375108	41.846016
3505.292322	489732.131017	41.851021
3505.484009	489665.943633	41.856026
3505.373155	489599.247515	41.861031
3505.404257	489540.962935	41.866036
3505.043561	489477.436315	41.871040
3505.229427	489399.330033	41.876045
3505.211058	489339.638295	41.881050
3505.197099	489276.359898	41.886055
3505.211489	489211.359704	41.891060
3505.434569	489145.215675	41.896064
3505.492116	489068.945803	41.901069
3505.256462	489007.518933	41.906074
3505.115613	488944.965964	41.911079
3505.262622	488876.509399	41.916084
3505.339547	488809.477572	41.921088
3505.279929	488749.385901	41.926093
3505.462938	488679.609717	41.931098
3505.247965	488610.854752	41.936103
3505.179435	488540.662526	41.941108
3505.343358	488484.625997	41.946112
3505.285162	488422.563084	41.951117
3505.314272	488352.556824	41.956122
3505.169474	488283.940985	41.961127
3505.187307	488212.925706	41.966132
3505.211094	488160.546292	41.971136
3505.075614	488095.110101	41.976141
3505.252411	488028.160317	41.981146
3504.936615	487962.095018	41.986151
3505.043255	487900.206364	41.991156
3505.143328	487851.450592	41.996160
3505.133595	487777.104045	42.001165
3505.241767	487717.386272	42.006170
3505.223521	487640.868521	42.011175
3505.117756	487590.174105	42.016180
3504.644319	487533.980731	42.021184
3504.920588	487465.295697	42.026189
3505.131632	487402.277579	42.031194
3504.719203	487348.852059	42.036199
3504.789804	487286.612966	42.041204
3505.040540	487227.982322	42.046208
3504.879871	487157.949621	42.051213
3504.782819	487095.937886	42.056218
3504.400599	487042.304553	42.061223
3504.855730	486985.004965	42.066228
3504.828449	486923.941386	42.071232
3504.589419	486872.760225	42.076237
3504.679007	486822.285428	42.081242
3504.901262	486764.768701	42.086247
3504.717972	486699.839109	42.091252
3504.742072	486657.304326	42.096256
3504.284512	486592.922082	42.101261
3504.650853	486528.209309	42.106266
3504.385555	486475.465027	42.111271
3504.387594	486418.587425	42.116276
3504.530994	486363.455570	42.121280
3504.324896	486315.348720	42.126285
3504.112032	486258.958589	42.131290
3504.318429	486205.230738	42.136295
3504.340632	486153.400369	42.141300
3504.368699	486112.530415	42.146304
3504.338265	486061.263579	42.151309
3504.632566	486003.631770	42.156314
3504.413784	485948.605306	42.161319
3504.381299	485894.458917	42.166324
3504.483329	485846.151110	42.171328
3504.298026	485792.230201	42.176333
3504.177137	485730.772337	42.181338
3504.012697	485685.738457	42.186343
3504.226671	485632.563101	42.191348
3504.330805	485590.518073	42.196352
3504.153725	485537.605305	42.201357
3504.595459	485483.535228	42.206362
3504.160824	485435.259131	42.211367
3504.144629	485389.544610	42.216372
3504.313052	485340.214566	42.221376
3504.202712	485288.199852	42.226381
3504.048609	485239.071224	42.231386
3503.987598	485183.512314	42.236391
3504.499963	485132.157928	42.241396
3504.295929	485085.158295	42.246400
3504.295643	485045.148721	42.251405
3504.436509	484981.121278	42.256410
3504.348132	484937.538390	42.261415
3504.513261	484890.430201	42.266420
3504.674737	484835.795261	42.271424
3504.408531	484781.378234	42.276429
3504.315779	484720.366639	42.281434
3504.393672	484670.593885	42.286439
3504.563120	484611.359726	42.291444
3504.411927	484553.791842	42.296448
3504.574875	484516.281446	42.301453
3504.392598	484451.948470	42.306458
3504.033985	484406.082253	42.311463
3504.285132	484353.603993	42.316468
3504.418520	484310.641587	42.321472
3503.980472	484249.126154	42.326477
3504.362691	484198.900370	42.331482
3504.244213	484162.291754	42.336487
3504.440082	484104.314553	42.341492
3504.454437	484055.964286	42.346496
3504.082175	484004.238623	42.351501
3504.183394	483950.569837	42.356506
3504.056725	483900.674884	42.361511
3503.983775	483850.670369	42.366516
3504.107918	483807.000713	42.371520
3503.898176	483758.330743	42.376525
3504.103800	483716.618491	42.381530
3503.687470	483664.898556	42.386535
3504.096496	483606.431635	42.391540
3504.383616	483568.394410	42.396544
3504.081336	483521.556895	42.401549
3504.307776	483467.008077	42.406554
3504.310473	483421.032205	42.411559
3504.354929	483371.816243	42.416564
3504.053659	483322.957063	42.421568
3503.872360	483271.502384	42.426573
3504.192651	483218.605354	42.431578
3503.945962	483181.003914	42.436583
3503.915133	483127.908598	42.441588
3504.099823	483090.542953	42.446592
3503.839944	483043.545831	42.451597
3504.132530	482998.938270	42.456602
3503.885013	482950.776894	42.461607
3504.183861	482899.751512	42.466612
3503.936596	482860.684185	42.471616
3503.958097	482819.857103	42.476621
3503.889724	482764.189641	42.481626
3504.062641	482718.084159	42.486631
3504.130488	482666.588715	42.491636
3503.877930	482626.763751	42.496640
3504.021750	482588.241186	42.501645
3504.436535	482533.962952	42.506650
3503.882703	482497.216066	42.511655
3504.142437	482439.778521	42.516660
3503.999205	482395.085480	42.521664
3503.938145	482342.244827	42.526669
3504.270822	482284.643784	42.531674
3503.904523	482246.300811	42.536679
3503.893707	482198.555019	42.541684
3504.134815	482158.298355	42.546688
3503.798539	482106.156579	42.551693
3503.911839	482051.014103	42.556698
3503.539455	482018.734760	42.561703
3503.777695	481972.869554	42.566708
3503.484864	481932.442761	42.571712
3503.235378	481875.132914	42.576717
3503.914191	481852.997274	42.581722
3503.573041	481801.006823	42.586727
3503.371602	481756.674711	42.591732
3503.408407	481726.251153	42.596736
3503.473336	481678.845687	42.601741
3503.761417	481638.883549	42.606746
3503.539291	481587.934965	42.611751
3503.708881	481562.442219	42.616756
3504.102088	481515.540991	42.621760
3503.736045	481480.177297	42.626765
3503.703293	481430.057722	42.631770
3503.760372	481389.625608	42.636775
3503.863883	481355.805498	42.641780
3503.542866	481311.541265	42.646784
3503.497843	481267.638196	42.651789
3503.919861	481222.449615	42.656794
3504.022979	481174.581918	42.661799
3503.996407	481140.023639	42.666804
3503.509733	481098.108960	42.671808
3503.748131	481049.310289	42.676813
3504.112552	481000.643447	42.681818
3503.733318	480961.996162	42.686823
3503.708109	480921.221935	42.691828
3503.549848	480874.303550	42.696832
3503.449825	480833.944984	42.701837
3503.869523	480790.776763	42.706842
3503.855794	480754.093333	42.711847
3503.600145	480709.109795	42.716852
3503.544589	480667.076348	42.721856
3503.190867	480631.506700	42.726861
3503.504322	480587.040632	42.731866
3503.145580	480552.785412	42.736871
3503.322160	480518.547878	42.741876
3503.720668	480486.347550	42.746880
3503.758895	480440.862726	42.751885
3503.534310	480400.067643	42.756890
3503.549364	480358.173982	42.761895
3503.751280	480317.767109	42.766900
3503.621795	480274.379740	42.771904
3503.569376	480233.052106	42.776909
3504.099789	480191.835800	42.781914
3503.854531	480159.229653	42.786919
3503.679961	480120.497920	42.791924
3503.801438	480073.432554	42.796929
3503.435275	480032.203749	42.801933
3503.756034	479986.218849	42.806938
3503.496330	479947.601007	42.811943
3503.529794	479909.897594	42.816948
3503.489049	479867.910248	42.821953
3503.261959	479834.744728	42.826957
3503.831129	479793.672957	42.831962
3503.525081	479756.123078	42.836967
3503.539935	479718.118898	42.841972
3503.422642	479661.690040	42.846977
3503.136036	479628.887093	42.851981
3503.577514	479600.619988	42.856986
3503.348135	479553.708742	42.861991
3503.539640	479521.033311	42.866996
3503.494081	479486.929181	42.872001
3503.512205	479450.237765	42.877005
3503.970988	479403.067379	42.882010
3503.400443	479361.363274	42.887015
3503.446357	479320.573844	42.892020
3503.537592	479279.019219	42.897025
3503.592464	479231.658498	42.902029
3503.545948	479193.359391	42.907034
3503.493647	479157.032008	42.912039
3503.550517	479122.254182	42.917044
3503.410221	479081.290968	42.922049
3503.280848	479042.044195	42.927053
3503.749385	479001.541937	42.932058
3503.664008	478969.413824	42.937063
3503.193996	478927.339171	42.942068
3503.324937	478885.777337	42.947073
3503.296353	478843.027323	42.952077
3503.778541	478811.871854	42.957082
3503.738102	478772.762188	42.962087
3503.542423	478725.641095	42.967092
3503.575920	478688.743374	42.972097
3503.199727	478650.999637	42.977101
3503.492215	478606.581811	42.982106
3503.095528	478583.648745	42.987111
3503.361335	478537.617658	42.992116
3503.424641	478498.693326	42.997121
3503.520744	478452.637862	43.002125
3503.381646	478413.643741	43.007130
3503.578914	478382.531770	43.012135
3503.518454	478339.835901	43.017140
3503.400164	478309.834208	43.022145
3503.104377	478274.452397	43.027149
3503.491256	478228.856429	43.032154
3503.216643	478199.990718	43.037159
3503.604774	478153.636250	43.042164
3503.299048	478124.168769	43.047169
3503.283950	478085.862103	43.052173
3503.518062	478049.993015	43.057178
3503.513031	478012.493243	43.062183
3503.498215	477971.002240	43.067188
3503.870878	477922.425744	43.072193
3503.679844	477894.809979	43.077197
3503.573142	477839.889205	43.082202
3503.767020	477808.574479	43.087207
3503.684076	477768.963553	43.092212
3503.534606	477726.279890	43.097217
3503.542298	477687.766557	43.102221
3503.944312	477647.675536	43.107226
3503.596139	477605.376258	43.112231
3503.538254	477563.638191	43.117236
3503.539738	477515.724713	43.122241
3503.199838	477477.820919	43.127245
3503.412572	477441.953792	43.132250
3503.245246	477416.658429	43.137255
3503.500085	477372.495732	43.142260
3503.605330	477333.460944	43.147265
3503.134120	477305.129625	43.152269
3503.494409	477259.484483	43.157274
3503.123343	477227.195140	43.162279
3503.271817	477192.449386	43.167284
3503.244054	477139.333448	43.172289
3503.150189	477114.582145	43.177293
3503.310978	477069.169676	43.182298
3503.175074	477041.240597	43.187303
3503.508960	477006.516129	43.192308
3503.713886	476973.176322	43.197313
3503.125022	476931.468686	43.202317
3503.550975	476887.126392	43.207322
3503.622082	476854.413683	43.212327
3503.091547	476814.718410	43.217332
3503.643008	476780.262857	43.222337
3503.051303	476732.894234	43.227341
3503.115635	476710.240535	43.232346
3503.082302	476673.500183	43.237351
3503.051745	476637.315303	43.242356
3503.121583	476609.757808	43.247361
3503.069936	476571.251018	43.252365
3503.233638	476537.461818	43.257370
3503.055513	476509.336202	43.262375
3503.180982	476473.480484	43.267380
3503.404574	476437.710507	43.272385
3503.075371	476405.463534	43.277389
3503.665309	476368.221134	43.282394
3503.544939	476331.038635	43.287399
3503.162694	476296.676796	43.292404
3503.576944	476255.670571	43.297409
3502.847672	476221.665846	43.302413
3503.362661	476180.744845	43.307418
3502.768575	476150.358223	43.312423
3502.605380	476121.168139	43.317428
3502.876263	476080.689237	43.322433
3502.984126	476058.230027	43.327437
3503.323136	476025.473938	43.332442
3503.299549	475991.055632	43.337447
3502.945029	475960.580824	43.342452
3503.350885	475929.381076	43.347457
3503.329784	475897.843335	43.352461
3503.454072	475865.221426	43.357466
3503.647866	475822.732002	43.362471
3503.306844	475785.329840	43.367476
3503.279789	475743.885513	43.372481
3503.342601	475713.800219	43.377485
3503.185087	475672.376009	43.382490
3503.006137	475637.172364	43.387495
3502.715449	475609.921992	43.392500
3502.779365	475569.777296	43.397505
3502.971433	475549.932751	43.402509
3503.263944	475511.572055	43.407514
3503.227025	475488.982937	43.412519
3503.375967	475448.066488	43.417524
3503.614071	475410.320594	43.422529
3503.314760	475373.264819	43.427533
3503.466817	475326.989461	43.432538
3503.234858	475290.479047	43.437543
3503.210069	475253.228631	43.442548
3503.082033	475223.525959	43.447553
3502.980872	475194.172892	43.452557
3503.330327	475157.976093	43.457562
3503.343878	475123.449054	43.462567
3502.937442	475086.864231	43.467572
3503.374622	475050.602991	43.472577
3503.420808	475011.015704	43.477581
3503.366553	474976.852748	43.482586
3502.893050	474940.025280	43.487591
3503.002265	474909.627965	43.492596
3503.488276	474875.178523	43.497601
3503.164477	474844.342969	43.502605
3503.507993	474803.445156	43.507610
3503.056068	474772.326102	43.512615
3502.887306	474733.327633	43.517620
3503.142613	474703.058847	43.522625
3502.921738	474679.284010	43.527629
3503.420970	474638.462650	43.532634
3502.856634	474611.404822	43.537639
3502.427222	474580.635749	43.542644
3503.219782	474545.632395	43.547649
3502.890995	474516.920126	43.552653
3502.883869	474480.120135	43.557658
3502.958490	474453.468124	43.562663
3502.899894	474428.858847	43.567668
3502.734702	474396.683424	43.572673
3503.050180	474377.829261	43.577677
3503.024784	474338.302015	43.582682
3502.960839	474312.176848	43.587687
3502.764930	474287.335966	43.592692
3502.928801	474245.352561	43.597697
3502.832127	474221.861034	43.602701
3502.910651	474182.165580	43.607706
3503.228404	474155.273035	43.612711
3502.893783	474132.121718	43.617716
3503.434666	474087.399971	43.622721
3502.924586	474056.541347	43.627725
3503.198190	474019.342756	43.632730
3503.161010	473985.933335	43.637735
3503.458664	473948.629735	43.642740
3503.063440	473907.945722	43.647745
3502.677603	473876.410232	43.652749
3503.004130	473842.438389	43.657754
3502.948466	473804.987226	43.662759
3502.850347	473793.981932	43.667764
3502.901019	473760.255056	43.672769
3502.939437	473728.349939	43.677773
3503.406592	473694.962544	43.682778
3503.151844	473671.747585	43.687783
3503.072277	473636.726325	43.692788
3503.097190	473590.819659	43.697793
3503.355828	473576.573810	43.702797
3503.411731	473525.404531	43.707802
3503.343638	473497.104871	43.712807
3503.417510	473459.733861	43.717812
3503.218497	473414.923183	43.722817
3503.000473	473381.085667	43.727821
3503.045480	473348.218242	43.732826
3503.262251	473316.486780	43.737831
3502.982851	473281.495850	43.742836
3503.231582	473250.416498	43.747841
3502.983802	473225.480949	43.752845
3503.073079	473192.201879	43.757850
3503.039292	473165.969061	43.762855
3502.861447	473130.304785	43.767860
3502.974492	473090.500177	43.772865
3502.845082	473065.293184	43.777869
3502.657739	473029.427942	43.782874
3502.806136	473000.942062	43.787879
3502.983324	472975.080551	43.792884
3503.034933	472942.969615	43.797889
3502.946808	472916.340403	43.802893
3502.889230	472883.589114	43.807898
3502.721814	472852.371536	43.812903
3502.575185	472824.082924	43.817908
3502.989817	472792.774657	43.822913
3502.614099	472778.525711	43.827917
3502.987141	472742.269294	43.832922
3502.852867	472715.444709	43.837927
3502.785596	472683.756214	43.842932
3503.247970	472649.457400	43.847937
3503.045699	472618.143682	43.852941
3503.183352	472584.097488	43.857946
3502.910187	472545.362786	43.862951
3502.844726	472522.268398	43.867956
3503.147205	472484.910133	43.872961
3502.922603	472463.357144	43.877965
3502.987663	472434.883242	43.882970
3502.887823	472413.361331	43.887975
3502.886434	472374.685045	43.892980
3502.873876	472328.679532	43.897985
3503.303006	472310.260309	43.902989
3503.043468	472271.320603	43.907994
3502.888492	472242.273910	43.912999
3502.947998	472205.711185	43.918004
3503.371002	472168.131207	43.923009
3502.754271	472149.015061	43.928013
3502.953575	472105.099398	43.933018
3502.945418	472084.321162	43.938023
3502.816418	472052.186018	43.943028
3502.848707	472007.234351	43.948033
3502.613263	471994.277416	43.953037
3502.900686	471958.234817	43.958042
3503.075515	471929.237363	43.963047
3503.058997	471899.005656	43.968052
3503.226974	471876.733533	43.973057
3502.886384	471841.091758	43.978061
3503.058911	471809.718164	43.983066
3503.011034	471776.760904	43.988071
3502.657363	471745.469069	43.993076
3502.701776	471708.553664	43.998081
3502.794562	471690.944479	44.003085
3503.220887	471661.553496	44.008090
3503.032865	471630.539023	44.013095
3502.857678	471596.539453	44.018100
3502.712149	471564.304801	44.023105
3502.667341	471536.554272	44.028109
3502.818806	471509.784359	44.033114
3502.946398	471475.787982	44.038119
3503.181583	471462.201224	44.043124
3502.798365	471416.705866	44.048129
3503.042134	471391.185411	44.053133
3502.870920	471359.712763	44.058138
3503.116583	471323.422461	44.063143
3502.578527	471291.804524	44.068148
3503.206495	471263.999402	44.073153
3502.677262	471241.784349	44.078157
3502.743657	471209.768826	44.083162
3502.956050	471189.410183	44.088167
3502.926065	471163.426360	44.093172
3502.821825	471116.673283	44.098177
3502.798840	471093.266896	44.103181
3502.755840	471060.155749	44.108186
3502.754922	471029.262706	44.113191
3502.454997	471004.786929	44.118196
3502.546262	470972.767073	44.123201
3502.672757	470949.691154	44.128205
3502.484010	470927.978873	44.133210
3502.854962	470903.752483	44.138215
3502.510058	470877.614963	44.143220
3502.617322	470846.755304	44.148225
3502.511774	470834.030046	44.153229
3503.062575	470800.876536	44.158234
3502.871991	470760.152813	44.163239
3502.813242	470738.470614	44.168244
3502.805319	470711.117448	44.173249
3502.507335	470685.376823	44.178253
3502.380754	470660.620743	44.183258
3502.383581	470636.198428	44.188263
3502.392006	470615.415748	44.193268
3502.560215	470583.079780	44.198273
3502.560143	470572.309869	44.203277
3502.066113	470538.155465	44.208282
3502.842213	470519.477988	44.213287
3502.681873	470503.777762	44.218292
3503.075581	470471.558176	44.223297
3502.820691	470446.012722	44.228301
3502.614560	470412.824528	44.233306
3503.165344	470387.558121	44.238311
3502.674557	470351.279144	44.243316
3502.434122	470319.511888	44.248321
3502.200076	470301.143047	44.253325
3502.107578	470272.791033	44.258330
3502.625709	470263.962845	44.263335
3502.455445	470232.336193	44.268340
3502.722502	470201.248199	44.273345
3502.387062	470194.575374	44.278349
3502.549156	470157.890988	44.283354
3502.684011	470137.290286	44.288359
3502.356979	470115.547884	44.293364
3502.682622	470083.338131	44.298369
3502.364297	470062.504468	44.303373
3502.534346	470025.616290	44.308378
3502.414596	470008.139504	44.313383
3502.055778	469994.997923	44.318388
3502.505871	469959.077318	44.323393
3502.602685	469941.263370	44.328397
3502.334681	469912.280698	44.333402
3502.612402	469900.000728	44.338407
3502.174823	469867.251970	44.343412
3502.403247	469852.350237	44.348417
3502.437495	469825.292428	44.353421
3502.314349	469799.776035	44.358426
3502.815196	469775.780602	44.363431
3502.263696	469754.477177	44.368436
3502.366706	469731.251507	44.373441
3502.404485	469712.839709	44.378445
3502.312463	469689.644330	44.383450
3502.440344	469673.392802	44.388455
3502.427389	469645.634121	44.393460
3502.501792	469623.778034	44.398465
3502.349166	469599.631203	44.403469
3502.490283	469585.703572	44.408474
3502.598015	469555.650479	44.413479
3502.441822	469528.166721	44.418484
3502.646007	469505.026122	44.423489
3502.363860	469486.006492	44.428493
3502.465642	469453.021279	44.433498
3502.699130	469435.842884	44.438503
3502.572127	469412.804259	44.443508
3502.511096	469391.322907	44.448513
3502.250809	469367.849858	44.453517
3502.355954	469331.627599	44.458522
3502.524318	469319.920452	44.463527
3502.571399	469299.484065	44.468532
3502.331054	469269.282347	44.473537
3502.440684	469238.924980	44.478541
3502.400503	469228.969508	44.483546
3502.510151	469194.212699	44.488551
3502.241581	469175.089462	44.493556
3502.654957	469154.140788	44.498561
3502.529434	469136.866246	44.503565
3502.369852	469105.690878	44.508570
3502.841239	469085.643308	44.513575
3502.462895	469073.161410	44.518580
3502.690038	469034.643965	44.523585
3502.831559	469016.417519	44.528589
3502.715874	468989.937921	44.533594
3502.393775	468961.821653	44.538599
3502.407094	468936.484961	44.543604
3502.409898	468912.110665	44.548609
3502.480781	468896.423493	44.553613
3502.468565	468864.567349	44.558618
3502.830847	468841.097809	44.563623
3502.377103	468822.356959	44.568628
3502.648910	468798.345183	44.573633
3502.545980	468768.171734	44.578637
3502.797325	468750.180750	44.583642
3502.797035	468713.670132	44.588647
3502.479097	468682.468038	44.593652
3502.472852	468656.122582	44.598657
3502.293543	468639.968410	44.603661
3502.409757	468618.256196	44.608666
3502.699675	468596.415784	44.613671
3502.387442	468573.000258	44.618676
3502.753941	468543.714169	44.623681
3502.620742	468522.596904	44.628685
3502.439081	468504.167339	44.633690
3502.694420	468471.206844	44.638695
3502.477544	468449.040544	44.643700
3502.477918	468412.074031	44.648705
3502.331258	468399.555569	44.653709
3502.458948	468371.469444	44.658714
3502.608058	468355.516738	44.663719
3502.496465	468330.451407	44.668724
3502.830468	468297.225475	44.673729
3502.450664	468278.067940	44.678733
3502.398903	468250.262385	44.683738
3502.679550	468224.276162	44.688743
3502.549405	468199.668654	44.693748
3502.820846	468178.133990	44.698753
3502.573985	468154.859412	44.703757
3502.688763	468126.420887	44.708762
3502.372489	468101.488202	44.713767
3502.522988	468075.774853	44.718772
3502.871295	468043.608176	44.723777
3502.399114	468030.330955	44.728781
3502.271953	467996.265907	44.733786
3502.567554	467965.674983	44.738791
3502.650090	467943.259130	44.743796
3502.754885	467928.678334	44.748801
3502.588994	467897.906244	44.753805
3502.761125	467868.194068	44.758810
3502.691178	467838.367795	44.763815
3502.114162	467815.750975	44.768820
3502.593671	467780.326788	44.773825
3502.565410	467764.856262	44.778829
3502.578535	467747.760983	44.783834
3502.722824	467715.271415	44.788839
3502.488433	467694.977995	44.793844
3502.642891	467666.583081	44.798849
3502.604090	467666.083431	44.803853
3502.564059	467627.907730	44.808858
3502.434660	467596.573109	44.813863
3502.374833	467584.900249	44.818868
3502.737114	467554.449911	44.823873
3502.483988	467537.598137	44.828877
3502.150016	467507.053768	44.833882
3502.387367	467488.254435	44.838887
3502.255857	467462.887458	44.843892
3502.247951	467444.227386	44.848897
3502.602398	467419.846751	44.853901
3502.587523	467395.928134	44.858906
3502.880266	467364.072229	44.863911
3502.634499	467342.970980	44.868916
3502.465467	467321.099167	44.873921
3502.366080	467301.289988	44.878925
3502.648902	467270.952644	44.883930
3502.198650	467234.761661	44.888935
3502.391385	467228.410028	44.893940
3502.224084	467194.349582	44.898945
3502.310345	467175.826276	44.903949
3502.333088	467154.328990	44.908954
3502.297182	467128.845480	44.913959
3502.273158	467120.605735	44.918964
3502.565426	467083.590846	44.923969
3502.449131	467064.441476	44.928973
3502.267421	467035.642634	44.933978
3502.373766	467025.814762	44.938983
3502.278522	467014.298735	44.943988
3502.444437	466976.949253	44.948993
3502.441040	466967.593590	44.953997
3502.211924	466952.457010	44.959002
3502.727503	466921.678217	44.964007
3502.704047	466903.576277	44.969012
3502.601872	466878.001547	44.974017
3502.480644	466847.776884	44.979021
3502.675376	466823.470807	44.984026
3502.341778	466798.285989	44.989031
3502.510187	466785.616133	44.994036
3502.687712	466749.478129	44.999041
3502.316352	466723.034703	45.004045
3502.343224	466704.621266	45.009050
3502.422694	466680.484642	45.014055
3502.335739	466655.008351	45.019060
3502.314920	466629.015979	45.024065
3502.176077	466607.846585	45.029069
3502.201653	466591.152784	45.034074
3502.549346	466562.827073	45.039079
3502.089107	466557.082550	45.044084
3501.938805	466523.928448	45.049089
3502.175126	466511.551270	45.054093
3502.093629	466498.717783	45.059098
3502.442397	466459.517968	45.064103
3502.171112	466458.042944	45.069108
3502.514442	466422.738221	45.074113
3502.547639	466419.597385	45.079117
3502.546492	466388.291111	45.084122
3502.273846	466362.489239	45.089127
3502.305796	466340.028527	45.094132
3502.579026	466317.530239	45.099137
3502.298647	466290.616783	45.104141
3502.128099	466282.247697	45.109146
3502.443783	466256.859873	45.114151
3502.311315	466250.861933	45.119156
3502.320987	466211.006234	45.124161
3502.656066	466194.820217	45.129165
3502.744376	466172.198780	45.134170
3502.589718	466143.394190	45.139175
3502.384246	466132.451051	45.144180
3502.432187	466096.331802	45.149185
3502.233727	466075.727356	45.154189
3502.475928	466049.844884	45.159194
3501.796712	466019.604398	45.164199
3502.436645	466014.093103	45.169204
3502.554384	465983.222765	45.174209
3502.593632	465968.852766	45.179213
3502.166020	465946.715926	45.184218
3502.374171	465928.728622	45.189223
3502.287641	465912.001012	45.194228
3502.473027	465890.679101	45.199233
3502.707741	465855.339507	45.204237
3502.347019	465840.778751	45.209242
3502.355199	465810.886119	45.214247
3502.396186	465785.186284	45.219252
3502.267093	465767.200708	45.224257
3502.428540	465746.641006	45.229261
3502.250757	465724.819041	45.234266
3502.404995	465708.205495	45.239271
3502.221458	465671.716728	45.244276
3502.285684	465658.000091	45.249281
3502.262634	465635.597572	45.254285
3502.128066	465630.307831	45.259290
3502.667097	465598.865445	45.264295
3502.252323	465587.701628	45.269300
3502.143421	465551.150405	45.274305
3502.022322	465534.630112	45.279309
3502.404934	465525.466468	45.284314
3502.699410	465495.376987	45.289319
3501.912293	465475.015139	45.294324
3502.076654	465459.967712	45.299329
3502.399554	465445.451968	45.304333
3502.322345	465415.319025	45.309338
3502.263259	465399.547631	45.314343
3502.295310	465369.903393	45.319348
3502.168482	465359.605038	45.324353
3502.571701	465332.785983	45.329357
3502.389986	465313.594209	45.334362
3502.452131	465285.715412	45.339367
3502.277378	465270.922903	45.344372
3502.273216	465241.284073	45.349377
3502.841001	465224.757435	45.354381
3502.426220	465195.283580	45.359386
3502.575089	465174.573398	45.364391
3502.428747	465152.695217	45.369396
3502.491739	465124.866600	45.374401
3502.485662	465110.401760	45.379405
3502.596464	465078.569822	45.384410
3502.423040	465055.886451	45.389415
3502.005029	465033.746909	45.394420
3501.616328	465018.431090	45.399425
3502.265928	464994.456221	45.404429
3502.011982	464987.970930	45.409434
3501.985032	464969.007580	45.414439
3501.959599	464957.479274	45.419444
3502.191101	464921.581835	45.424449
3502.311591	464915.746374	45.429453
3502.223235	464898.309912	45.434458
3502.336680	464873.406694	45.439463
3502.494485	464860.130070	45.444468
3502.556712	464839.938764	45.449473
3502.601398	464811.202027	45.454477
3502.167541	464791.087859	45.459482
3502.434625	464759.939130	45.464487
3502.371840	464754.182715	45.469492
3502.232537	464726.081433	45.474497
3502.546970	464711.920443	45.479501
3502.103970	464683.916931	45.484506
3502.280383	464660.470451	45.489511
3502.234671	464651.979961	45.494516
3502.073363	464632.986559	45.499521
3502.585223	464616.619773	45.504525
3502.188193	464585.675229	45.509530
3502.353332	464561.218738	45.514535
3502.406941	464534.705725	45.519540
3502.697213	464519.132049	45.524545
3502.666518	464486.714032	45.529549
3502.606440	464468.564581	45.534554
3502.524578	464437.267230	45.539559
3502.474389	464409.809118	45.544564
3502.382492	464402.944310	45.549569
3502.478991	464366.560878	45.554573
3502.429214	464342.643335	45.559578
3502.234240	464310.705782	45.564583
3502.455417	464305.056772	45.569588
3502.141913	464268.484019	45.574593
3502.275625	464252.782714	45.579597
3502.411437	464246.843473	45.584602
3502.384638	464220.595390	45.589607
3502.382317	464196.872586	45.594612
3502.017538	464181.704029	45.599617
3502.208735	464151.375307	45.604621
3502.194489	464135.798083	45.609626
3502.150288	464119.922009	45.614631
3502.259909	464108.776768	45.619636
3502.080693	464087.205814	45.624641
3501.673574	464055.503123	45.629645
3501.877373	464046.214756	45.634650
3502.355270	464032.331257	45.639655
3502.462779	464013.194160	45.644660
3502.474426	463983.348325	45.649665
3502.370685	463967.886039	45.654669
3501.902191	463948.990252	45.659674
3502.422574	463940.006645	45.664679
3502.230548	463914.390798	45.669684
3502.335843	463894.444576	45.674689
3502.220152	463873.217548	45.679693
3501.920496	463866.536602	45.684698
3502.714072	463831.206965	45.689703
3502.582357	463812.359785	45.694708
3502.362154	463780.273404	45.699713
3502.424622	463757.855079	45.704717
3502.459539	463737.312618	45.709722
3502.383520	463708.289282	45.714727
3502.356204	463695.293470	45.719732
3502.735179	463673.331622	45.724737
3502.539820	463648.272315	45.729741
3502.306977	463624.888085	45.734746
3502.632451	463593.879874	45.739751
3502.213070	463573.610245	45.744756
3501.998773	463555.888487	45.749761
3502.304745	463535.961200	45.754765
3502.271959	463505.109745	45.759770
3502.319719	463496.401790	45.764775
3502.373119	463479.902911	45.769780
3502.173082	463446.750480	45.774785
3502.533314	463430.861409	45.779789
3502.272225	463412.489179	45.784794
3502.466945	463389.948617	45.789799
3502.359790	463381.315295	45.794804
3502.310488	463341.613737	45.799809
3502.624221	463259.920389	45.804813
3501.780746	463155.086747	45.809818
3502.002838	462983.565950	45.814823
3501.620123	462782.645472	45.819828
3501.257073	462515.348792	45.824833
3501.197816	462211.981682	45.829837
3500.585775	461860.685805	45.834842
3500.180450	461467.663851	45.839847
3499.543149	461036.016740	45.844852
3498.428231	460550.095845	45.849857
3498.061384	460030.399175	45.854861
3496.977975	459457.924926	45.859866
3496.430523	458837.886993	45.864871
3495.340157	458185.122311	45.869876
3494.433275	457495.213003	45.874881
3493.574420	456749.401544	45.879885
3492.435589	455977.235659	45.884890
3491.371962	455151.530226	45.889895
3489.982945	454288.232219	45.894900
3488.848627	453389.321179	45.899905
3487.397222	452449.312988	45.904909
3485.827230	451469.942119	45.909914
3483.963735	450435.485930	45.914919
3482.655547	449378.405948	45.919924
3480.995714	448288.308893	45.924929
3479.183008	447151.538243	45.929933
3477.402278	446002.336748	45.934938
3475.704213	444807.374628	45.939943
3474.316986	443584.889515	45.944948
3472.197494	442324.707161	45.949953
3470.080208	441021.793186	45.954957
3468.087532	439695.671912	45.959962
3466.372783	438346.771078	45.964967
3464.291933	436951.984661	45.969972
3461.756604	435531.075682	45.974977
3459.888917	434086.955131	45.979981
3457.269736	432628.048103	45.984986
3455.506950	431133.021194	45.989991
3452.996536	429610.275883	45.994996
3450.610226	428061.850332	46.000001
3448.484279	426487.363493	46.005005
3445.816775	424884.806028	46.010010
3443.549426	423261.832714	46.015015
3440.834900	421639.256643	46.020020
3438.252903	419952.343006	46.025025
3435.688593	418259.813699	46.030029
3432.907184	416558.510351	46.035034
3430.464360	414826.436768	46.040039
3427.970519	413079.623924	46.045044
3424.820832	411309.337866	46.050049
3422.335802	409515.470208	46.055053
3419.501002	407709.589099	46.060058
3416.606100	405888.857549	46.065063
3413.711080	404044.942812	46.070068
3410.710916	402180.343598	46.075073
3407.900348	400300.339160	46.080077
3404.973094	398413.146177	46.085082
3402.180295	396498.727578	46.090087
3398.848641	394580.837607	46.095092
3395.903948	392640.854896	46.100097
3392.739907	390692.374734	46.105101
3389.449717	388732.133008	46.110106
3386.490782	386758.280463	46.115111
3382.898900	384776.551718	46.120116
3379.754341	382789.724249	46.125121
3376.951770	380780.851988	46.130125
3373.317590	378761.288775	46.135130
3370.226643	376734.833133	46.140135
3367.021684	374696.787297	46.145140
3363.523551	372651.522355	46.150145
3360.124834	370594.176445	46.155149
3357.010092	368534.857157	46.160154
3353.522825	366468.383686	46.165159
3350.580510	364390.573855	46.170164
3346.928164	362297.175871	46.175169
3343.711352	360205.519797	46.180173
3340.524658	358097.372964	46.185178
3336.846920	355976.856568	46.190183
3333.443197	353858.542943	46.195188
3329.670418	351738.467842	46.200193
3326.150658	349598.944958	46.205197
3322.131385	347471.944922	46.210202
3318.934515	345327.672687	46.215207
3315.417513	343197.147096	46.220212
3311.785550	341048.327769	46.225217
3308.433180	338904.420107	46.230221
3304.804075	336755.494332	46.235226
3301.410067	334590.638259	46.240231
3297.447574	332433.451901	46.245236
3293.837048	330257.546845	46.250241
3290.354100	328089.869176	46.255245
3286.504383	325933.475923	46.260250
3282.977643	323762.265233	46.265255
3279.091337	321587.969805	46.270260
3275.195041	319412.089242	46.275265
3271.690711	317238.481519	46.280269
3267.717540	315063.415948	46.285274
3264.387403	312884.253616	46.290279
3260.534360	310711.585605	46.295284
3256.664328	308534.775790	46.300289
3252.915337	306367.903333	46.305293
3248.812253	304194.987081	46.310298
3244.884994	302014.801032	46.315303
3241.072873	299859.833007	46.320308
3237.485714	297681.176262	46.325313
3233.510254	295506.568977	46.330317
3229.738074	293350.762249	46.335322
3226.037711	291183.946923	46.340327
3221.906214	289024.149512	46.345332
3218.285334	286872.143119	46.350337
3214.706178	284721.384789	46.355341
3211.021459	282565.917130	46.360346
3207.496324	280405.064414	46.365351
3203.445531	278254.822623	46.370356
3199.235295	276116.232930	46.375361
3195.522618	273953.066089	46.380365
3191.576029	271811.116174	46.385370
3187.894771	269670.015411	46.390375
3183.850598	267539.030941	46.395380
3179.733460	265410.506902	46.400385
3176.143845	263275.745301	46.405389
3172.141363	261154.375347	46.410394
3168.317673	259029.220627	46.415399
3164.425759	256914.455390	46.420404
3159.994175	254801.166178	46.425409
3156.257372	252694.485832	46.430413
3151.910035	250596.071684	46.435418
3148.402676	248489.834371	46.440423
3143.967937	246401.263994	46.445428
3140.187891	244323.597362	46.450433
3136.774835	242240.072741	46.455437
3132.528878	240179.530885	46.460442
3128.481306	238102.082979	46.465447
3124.638793	236061.392472	46.470452
3120.361590	234015.308786	46.475457
3116.614550	231962.588630	46.480461
3112.528560	229929.806135	46.485466
3108.653570	227899.227873	46.490471
3104.805109	225876.742493	46.495476
3101.103900	223859.429774	46.500481
3096.718793	221842.531002	46.505485
3092.519741	219843.766548	46.510490
3088.533673	217851.902269	46.515495
3084.666101	215859.161288	46.520500
3080.506958	213890.084719	46.525505
3076.653156	211909.409207	46.530509
3072.508689	209947.129387	46.535514
3067.964229	207992.159645	46.540519
3064.042078	206060.081685	46.545524
3059.965199	204124.352988	46.550529
3056.037147	202204.512584	46.555533
3051.826489	200299.202682	46.560538
3047.462566	198388.234693	46.565543
3043.256634	196498.327287	46.570548
3039.074245	194634.671820	46.575553
3034.654961	192765.553614	46.580557
3030.362283	190920.203023	46.585562
3026.566008	189069.940422	46.590567
3022.286611	187248.965993	46.595572
3017.803194	185443.842245	46.600577
3013.761823	183636.313747	46.605581
3009.581499	181859.803636	46.610586
3005.365790	180088.170828	46.615591
3001.378645	178339.045999	46.620596
2996.869893	176580.604349	46.625601
2992.646450	174855.598540	46.630605
2987.992983	173146.978683	46.635610
2983.441848	171444.503607	46.640615
2979.424364	169770.256582	46.645620
2974.927512	168112.823496	46.650625
2970.682462	166463.549327	46.655629
2965.827780	164833.324446	46.660634
2961.524125	163226.944758	46.665639
2956.834327	161638.929544	46.670644
2951.836863	160074.166432	46.675649
2947.662118	158536.029698	46.680653
2942.497471	157015.687645	46.685658
2937.708524	155520.957930	46.690663
2933.106264	154064.518998	46.695668
2927.927927	152623.771121	46.700673
2922.584648	151219.265781	46.705677
2916.932816	149854.739114	46.710682
2911.642914	148525.045199	46.715687
2906.397735	147193.189114	46.720692
2900.146139	145899.633974	46.725697
2894.561913	144688.295706	46.730701
2888.912385	143524.431821	46.735706
2883.433346	142392.098064	46.740711
2878.307706	141302.804295	46.745716
2872.883166	140246.445487	46.750721
2868.046508	139226.660452	46.755725
2863.009429	138248.900532	46.760730
2858.217212	137292.038557	46.765735
2853.487917	136368.683902	46.770740
2849.338630	135475.726470	46.775745
2844.745200	134597.549249	46.780749
2840.369807	133750.357254	46.785754
2836.159075	132919.171709	46.790759
2831.945022	132106.994675	46.795764
2827.434710	131324.238129	46.800769
2823.399987	130553.658811	46.805773
2819.461991	129797.553886	46.810778
2815.516748	129046.551539	46.815783
2812.140081	128318.089790	46.820788
2808.207243	127603.438925	46.825793
2804.567833	126883.577951	46.830797
2800.402641	126195.901619	46.835802
2796.804320	125493.254840	46.840807
2793.203358	124820.369550	46.845812
2789.754639	124145.589463	46.850817
2786.077030	123475.053372	46.855821
2782.458083	122806.401712	46.860826
2778.952438	122139.854881	46.865831
2775.448101	121486.469136	46.870836
2771.642676	120833.153898	46.875841
2768.130995	120181.698806	46.880845
2764.639641	119548.818303	46.885850
2761.146340	118913.010985	46.890855
2757.646348	118269.865168	46.895860
2753.531219	117645.798739	46.900865
2749.859391	117012.937709	46.905869
2746.203284	116402.655639	46.910874
2742.457897	115794.686295	46.915879
2738.630469	115185.862339	46.920884
2734.489151	114582.857321	46.925889
2731.291726	113989.836538	46.930893
2727.376061	113407.630380	46.935898
2723.401173	112825.875100	46.940903
2720.010609	112245.055440	46.945908
2715.615813	111675.462862	46.950913
2711.936092	111106.797945	46.955917
2708.122419	110563.794094	46.960922
2704.035495	110010.581205	46.965927
2700.275104	109470.789756	46.970932
2696.462142	108942.469466	46.975937
2692.862843	108410.030338	46.980941
2688.926878	107887.389844	46.985946
2685.886686	107375.843166	46.990951
2682.004414	106854.684670	46.995956
2678.588413	106347.953578	47.000961
2675.112399	105842.370746	47.005965
2671.048171	105324.225920	47.010970
2667.921619	104820.078568	47.015975
2664.672389	104311.241887	47.020980
2661.272938	103815.465446	47.025985
2657.779790	103310.914841	47.030989
2654.341420	102804.634691	47.035994
2650.790040	102298.684940	47.040999
2647.659778	101788.737155	47.046004
2643.863861	101286.628797	47.051009
2640.705435	100779.395726	47.056013
2637.033605	100276.902315	47.061018
2633.906165	99765.244491	47.066023
2630.328540	99256.105080	47.071028
2626.436708	98751.127766	47.076033
2623.589089	98238.561057	47.081037
2619.916552	97737.276732	47.086042
2616.525032	97224.645790	47.091047
2613.571227	96711.141696	47.096052
2609.740082	96199.231261	47.101057
2606.594379	95680.728654	47.106061
2602.951575	95169.263254	47.111066
2599.567104	94641.411223	47.116071
2596.212344	94130.667865	47.121076
2592.724966	93610.041907	47.126081
2589.317449	93078.293648	47.131085
2586.039351	92558.720359	47.136090
2582.433409	92029.892976	47.141095
2579.354456	91504.703066	47.146100
2575.290214	90979.396068	47.151105
2572.304887	90439.089753	47.156109
2568.792068	89916.409180	47.161114
2565.382185	89377.242665	47.166119
2561.990608	88849.339953	47.171124
2558.180179	88312.846966	47.176129
2555.065929	87776.585708	47.181133
2551.700949	87241.872385	47.186138
2548.016004	86696.153107	47.191143
2544.747148	86162.156006	47.196148
2540.847134	85624.112758	47.201153
2537.878084	85076.673660	47.206157
2534.333566	84535.355922	47.211162
2530.526657	83985.133473	47.216167
2527.461664	83438.960001	47.221172
2523.786657	82897.757049	47.226177
2520.430702	82343.520154	47.231181
2516.827377	81802.441278	47.236186
2513.169251	81257.837471	47.241191
2510.067407	80706.095509	47.246196
2506.334091	80159.822711	47.251201
2502.942413	79608.236457	47.256205
2499.309788	79059.607176	47.261210
2495.884593	78501.545281	47.266215
2492.602807	77954.458253	47.271220
2488.733066	77411.410688	47.276225
2485.534333	76855.544149	47.281229
2482.297880	76294.526053	47.286234
2478.515869	75726.568983	47.291239
2475.443089	75171.238013	47.296244
2471.757107	74608.915245	47.301249
2468.255982	74051.883516	47.306253
2464.887241	73481.852381	47.311258
2461.482078	72930.124346	47.316263
2457.560426	72358.133568	47.321268
2454.073615	71796.004272	47.326273
2450.898689	71224.099637	47.331277
2447.446382	70662.192373	47.336282
2443.747261	70098.196202	47.341287
2440.553784	69525.144477	47.346292
2436.805038	68959.168356	47.351297
2433.053064	68391.554666	47.356301
2429.815990	67816.713038	47.361306
2426.254974	67244.848270	47.366311
2423.356281	66681.005344	47.371316
2419.159025	66119.205025	47.376321
2415.999462	65540.778235	47.381325
2412.248113	64968.423028	47.386330
2408.964176	64398.261245	47.391335
2405.642063	63824.329308	47.396340
2402.326304	63252.992634	47.401345
2398.662449	62680.993375	47.406349
2395.081497	62101.201054	47.411354
2391.639552	61524.135897	47.416359
2388.281389	60939.233815	47.421364
2384.601631	60366.205441	47.426369
2381.266317	59778.363937	47.431373
2377.276561	59203.735777	47.436378
2373.427634	58627.328900	47.441383
2370.593683	58062.751381	47.446388
2367.209122	57483.285474	47.451393
2363.441507	56904.254798	47.456397
2360.195305	56318.919969	47.461402
2356.710587	55739.822674	47.466407
2353.827676	55151.414496	47.471412
2349.946974	54575.801512	47.476417
2346.889462	53982.995762	47.481421
2342.997253	53392.098473	47.486426
2339.865040	52803.248364	47.491431
2336.628571	52211.435043	47.496436
2332.554227	51628.851154	47.501441
2329.384485	51024.808141	47.506445
2326.033695	50438.297429	47.511450
2322.604411	49835.049018	47.516455
2319.197630	49231.578236	47.521460
2315.104138	48634.737890	47.526465
2311.891914	48035.638536	47.531469
2308.424183	47438.288140	47.536474
2304.938682	46836.294672	47.541479
2301.504285	46236.700249	47.546484
2297.706808	45643.368009	47.551489
2294.530461	45033.390105	47.556493
2291.063681	44429.599994	47.561498
2286.988138	43834.095054	47.566503
2283.590070	43230.142875	47.571508
2280.043976	42630.225072	47.576513
2276.602378	42025.171177	47.581517
2273.362254	41427.330990	47.586522
2269.626376	40834.200172	47.591527
2266.278690	40231.558845	47.596532
2262.580055	39632.710502	47.601537
2259.291445	39028.330735	47.606541
2255.949709	38421.972716	47.611546
2252.440709	37810.490935	47.616551
2248.953647	37201.641337	47.621556
2245.378914	36602.287274	47.626561
2242.077912	35992.118218	47.631565
2238.260726	35392.144931	47.636570
2234.867677	34774.792393	47.641575
2231.487086	34162.552154	47.646580
2227.700493	33579.403764	47.651585
2224.260406	32961.192570	47.656589
2220.691684	32354.256979	47.661594
2217.356316	31752.632848	47.666599
2214.197289	31136.428349	47.671604
2210.511973	30534.298204	47.676609
2206.808344	29923.449300	47.681613
2203.200764	29322.128227	47.686618
2199.586162	28710.300203	47.691623
2196.306024	28094.750416	47.696628
2192.821782	27485.467093	47.701633
2189.441601	26875.723254	47.706637
2185.700185	26256.828495	47.711642
2181.979741	25664.161325	47.716647
2178.424392	25050.349691	47.721652
2174.968750	24452.139508	47.726657
2171.642782	23839.045131	47.731661
2167.908309	23234.294248	47.736666
2164.343668	22624.891726	47.741671
2161.452422	22020.388606	47.746676
2157.520458	21428.975881	47.751681
2154.162428	20808.315131	47.756685
2150.615621	20204.508060	47.761690
2147.051131	19599.822888	47.766695
2143.281609	18990.817961	47.771700
2139.589377	18391.548510	47.776705
2136.124891	17787.397991	47.781709
2132.549859	17189.642093	47.786714
2128.950941	16586.959108	47.791719
2125.516735	15994.987710	47.796724
2121.087002	15398.037852	47.801729
2117.651511	14807.202018	47.806733
2113.871357	14220.250126	47.811738
2109.872222	13647.002381	47.816743
2105.747127	13078.135224	47.821748
2101.775591	12526.695629	47.826753
2097.229544	11982.063470	47.831757
2092.408246	11462.881798	47.836762
2087.307731	10966.721152	47.841767
2081.117682	10520.337360	47.846772
2075.122276	10120.652808	47.851777
2069.881650	9730.697384	47.856781
2065.121582	9355.406751	47.861786
2059.980220	9012.082551	47.866791
2055.378703	8689.051971	47.871796
2051.237626	8388.750825	47.876801
2047.266776	8095.821756	47.881805
2043.920190	7821.290457	47.886810
2039.967948	7550.320031	47.891815
2036.339782	7290.257116	47.896820
2032.194305	7042.419046	47.901825
2028.829785	6801.672391	47.906829
2025.694598	6562.975671	47.911834
2022.080214	6330.420403	47.916839
2018.948167	6103.407318	47.921844
2015.266500	5880.995490	47.926849
2012.132739	5653.731916	47.931853
2008.835801	5430.442886	47.936858
2005.554629	5214.255525	47.941863
2002.569107	4979.964505	47.946868
1998.924088	4761.911923	47.951873
1995.701944	4525.818660	47.956877
1992.387878	4303.141063	47.961882
1988.681272	4087.884561	47.966887
1985.662030	3860.521160	47.971892
1982.067808	3639.312971	47.976897
1978.895517	3424.383081	47.981901
1975.155145	3204.019362	47.986906
1971.902262	2991.233559	47.991911
1968.417233	2765.063926	47.996916
1965.041644	2547.771351	48.001921
1961.498307	2326.375187	48.006925
1958.218402	2111.825768	48.011930
1954.533470	1905.128634	48.016935
1950.994116	1682.202083	48.021940
1947.497361	1471.566808	48.026945
1943.681937	1262.726932	48.031949
1939.778678	1057.481520	48.036954
1936.281157	864.786423	48.041959
1932.711373	663.995800	48.046964
1928.020401	502.454641	48.051969
1923.147109	338.861578	48.056973
1917.996792	207.754026	48.061978
1912.982562	94.178536	48.066983
1908.324438	-2.785305	48.071988
1899.795762	23.756763	48.076993
1891.189380	92.625553	48.081997
1887.774882	102.414028	48.087002
1885.495608	97.868207	48.092007
1884.028895	94.379152	48.097012
1882.089130	96.123736	48.102017
1879.154906	88.266208	48.107021
1876.620959	95.785293	48.112026
1872.729427	102.395716	48.117031
1869.523525	94.852548	48.122036
1866.189953	92.726545	48.127041
1862.904527	99.093940	48.132045
1859.388826	100.694662	48.137050
1855.722072	105.634464	48.142055
1852.460739	102.206422	48.147060
1848.919091	97.660927	48.152065
1846.239552	91.304491	48.157069
1842.724078	93.443009	48.162074
1839.406277	101.286570	48.167079
1835.933395	91.130607	48.172084
1832.697079	96.240694	48.177089
1828.913665	99.733854	48.182093
1825.786582	87.265187	48.187098
1822.083551	92.849702	48.192103
1818.370043	90.112130	48.197108
1815.183192	95.869406	48.202113
1811.419316	95.949047	48.207117
1808.493336	88.292723	48.212122
1804.875780	93.054027	48.217127
1801.650506	87.421605	48.222132
1798.172250	92.730696	48.227137
1794.370348	95.533883	48.232141
1791.551470	105.489082	48.237146
1787.732902	102.084500	48.242151
1784.141114	91.054887	48.247156
1780.773752	98.270255	48.252161
1777.097212	94.410144	48.257165
1773.646240	100.448972	48.262170
1769.934185	98.261663	48.267175
1767.144578	98.759141	48.272180
1764.019580	91.323620	48.277185
1759.782293	85.899331	48.282189
1756.759479	86.594455	48.287194
1752.788963	100.433592	48.292199
1749.565611	90.406484	48.297204
1746.059682	97.032824	48.302209
1742.280211	93.188737	48.307213
1739.326632	94.689324	48.312218
1735.956126	103.588278	48.317223
1732.401089	97.358624	48.322228
1728.652871	101.966266	48.327233
1724.812656	99.207295	48.332237
1721.864343	92.402331	48.337242
1718.073426	98.930662	48.342247
1714.748695	96.069317	48.347252
1711.302151	92.723902	48.352257
1707.922979	90.472136	48.357261
1704.358550	91.450875	48.362266
1700.891669	99.735249	48.367271
1697.926254	88.915044	48.372276
1694.131842	94.662482	48.377281
1690.033225	94.376625	48.382285
1687.097935	97.952923	48.387290
1683.489999	97.631824	48.392295
1680.128655	90.448232	48.397300
1676.649643	97.873967	48.402305
1672.951278	96.402699	48.407309
1670.118047	86.492056	48.412314
1666.128228	103.349208	48.417319
1662.670883	97.294182	48.422324
1659.163716	89.880194	48.427329
1655.337868	92.506786	48.432333
1652.194466	88.085994	48.437338
1648.076107	96.535039	48.442343
1645.383281	87.792100	48.447348
1642.093990	89.405053	48.452353
1638.296725	90.369417	48.457357
1634.860016	92.365978	48.462362
1630.660378	89.504777	48.467367
1627.419080	86.333069	48.472372
1624.299184	96.237037	48.477377
1620.358182	93.262816	48.482381
1617.338557	82.568123	48.487386
1613.755254	94.167195	48.492391
1610.622527	83.053514	48.497396
1607.107236	87.605924	48.502401
1603.053224	87.955366	48.507405
1599.806177	84.620044	48.512410
1596.037305	95.150194	48.517415
1592.469067	85.565931	48.522420
1589.595570	87.117337	48.527425
1585.962335	84.636213	48.532429
1582.512459	86.195073	48.537434
1578.886004	90.704676	48.542439
1575.263621	87.199989	48.547444
1571.724541	92.584995	48.552449
1568.241725	93.117615	48.557453
1565.035811	87.653050	48.562458
1561.418165	88.118073	48.567463
1557.815730	88.520619	48.572468
1554.532931	92.030789	48.577473
1550.852298	88.402296	48.582477
1547.769408	82.317484	48.587482
1544.102560	88.934073	48.592487
1540.300582	82.628996	48.597492
1536.944678	90.386740	48.602497
1532.885334	80.404374	48.607501
1529.741247	73.740644	48.612506
1526.141590	86.104707	48.617511
1522.916284	84.461754	48.622516
1519.666873	80.604800	48.627521
1515.988341	84.815633	48.632525
1512.700979	78.917673	48.637530
1508.908932	81.978770	48.642535
1505.582670	81.563229	48.647540
1502.003651	82.427199	48.652545
1498.235761	79.017936	48.657549
1495.125650	79.729830	48.662554
1491.242848	82.735452	48.667559
1488.024234	80.892148	48.672564
1484.516478	71.096023	48.677569
1481.029794	85.767818	48.682573
1477.777236	81.756338	48.687578
1473.825729	84.237990	48.692583
1470.589461	73.779524	48.697588
1467.111342	82.584491	48.702593
1463.392699	87.734862	48.707597
1459.974264	74.118907	48.712602
1455.956082	86.304507	48.717607
1452.981192	77.735215	48.722612
1449.554462	75.876854	48.727617
1446.051534	66.374210	48.732621
1442.872981	68.276819	48.737626
1438.909044	84.443395	48.742631
1435.483797	74.909675	48.747636
1431.750332	82.789460	48.752641
1427.723880	71.612450	48.757645
1424.693345	71.992431	48.762650
1421.669443	69.122265	48.767655
1417.961303	75.197964	48.772660
1414.462569	73.062917	48.777665
1410.960023	75.651861	48.782669
1407.564127	68.343987	48.787674
1404.132530	87.233903	48.792679
1400.621686	68.358466	48.797684
1397.099478	72.763268	48.802689
1393.089236	64.624057	48.807693
1389.992627	68.276093	48.812698
1386.401887	69.853729	48.817703
1382.412597	75.900425	48.822708
1379.239816	75.568573	48.827713
1375.853559	78.949326	48.832717
1373.074768	81.833739	48.837722
1369.385363	78.519843	48.842727
1365.572981	69.290001	48.847732
1362.084151	68.124673	48.852737
1358.279998	77.660581	48.857741
1354.841236	78.872886	48.862746
1351.324474	73.529504	48.867751
1348.050762	72.365495	48.872756
1344.775357	71.673141	48.877761
1340.807085	73.119722	48.882765
1337.318093	71.397612	48.887770
1333.741132	83.941634	48.892775
1330.474325	78.160723	48.897780
1327.150797	81.519060	48.902785
1323.455705	79.591754	48.907789
1319.694891	82.834662	48.912794
1315.949405	85.328553	48.917799
1312.956226	86.784712	48.922804
1309.691997	86.865726	48.927809
1306.126471	82.251260	48.932813
1302.484847	72.504477	48.937818
1298.721782	79.297399	48.942823
1295.549227	77.231817	48.947828
1291.884732	81.684084	48.952833
1288.531261	81.915029	48.957837
1285.416100	80.976279	48.962842
1281.701839	93.449931	48.967847
1278.083661	77.799211	48.972852
1274.761108	83.501696	48.977857
1270.563184	78.568063	48.982861
1267.568905	77.518753	48.987866
1263.967561	81.752389	48.992871
1260.490565	72.040100	48.997876
1256.874940	75.326850	49.002881
1253.119749	78.407540	49.007885
1249.836044	70.626656	49.012890
1246.193355	73.218444	49.017895
1242.638441	77.204413	49.022900
1239.551157	74.100529	49.027905
1236.308629	72.808295	49.032909
1232.680756	65.659942	49.037914
1229.098709	75.224555	49.042919
1224.913762	80.289336	49.047924
1221.867931	66.397148	49.052929
1218.290370	78.153501	49.057933
1215.118448	69.997727	49.062938
1211.321712	80.529048	49.067943
1207.533085	78.863083	49.072948
1204.226686	67.067855	49.077953
1200.814257	67.377588	49.082957
1197.736286	69.340489	49.087962
1194.139737	75.079297	49.092967
1190.409345	74.426142	49.097972
1187.026593	70.602643	49.102977
1183.265849	70.125053	49.107981
1180.188205	68.946363	49.112986
1176.390749	70.581504	49.117991
1173.034923	70.281328	49.122996
1169.273221	67.497561	49.128001
1165.615707	73.745723	49.133005
1162.677072	69.255161	49.138010
1158.925795	79.630714	49.143015
1155.141450	69.634100	49.148020
1152.356243	75.423788	49.153025
1148.015208	78.573530	49.158029
1144.966339	65.314570	49.163034
1141.074380	75.810094	49.168039
1137.559819	68.720047	49.173044
1134.420086	68.974685	49.178049
1130.856424	77.562025	49.183053
1127.779690	76.588837	49.188058
1124.210856	70.326635	49.193063
1120.396144	63.318115	49.198068
1117.046643	72.909806	49.203073
1112.964277	67.499481	49.208077
1109.951257	58.591349	49.213082
1106.561170	70.403936	49.218087
1103.106249	75.383566	49.223092
1100.063902	69.830339	49.228097
1095.796914	77.960858	49.233101
1092.135815	75.072857	49.238106
1088.740925	70.802017	49.243111
1085.199872	79.303584	49.248116
1082.121291	68.763703	49.253121
1078.155087	75.471200	49.258125
1074.888972	72.657758	49.263130
1071.375079	78.602004	49.268135
1068.003859	78.965446	49.273140
1064.503659	71.550479	49.278145
1060.988356	78.953404	49.283149
1056.860268	69.016644	49.288154
1053.302641	73.009376	49.293159
1049.929563	76.831017	49.298164
1046.815411	62.683754	49.303169
1043.281100	73.389358	49.308173
1040.020323	67.493662	49.313178
1036.363858	65.981153	49.318183
1032.698271	75.951072	49.323188
1029.611589	66.418515	49.328193
1025.707729	76.292649	49.333197
1022.571473	73.503292	49.338202
1018.643767	69.742498	49.343207
1015.540327	76.926294	49.348212
1012.015709	65.465624	49.353217
1007.682824	72.132128	49.358221
1004.306714	62.869251	49.363226
1001.183142	70.701570	49.368231
997.833528	68.537037	49.373236
994.396811	60.647145	49.378241
990.540993	65.822058	49.383245
987.586522	67.955573	49.388250
983.657252	71.705611	49.393255
979.823386	72.150568	49.398260
976.530777	69.958182	49.403265
973.072967	68.807054	49.408269
969.938195	69.431087	49.413274
966.556931	75.190182	49.418279
962.572135	77.550518	49.423284
959.155471	69.091207	49.428289
955.971211	77.398038	49.433293
952.739616	70.232340	49.438298
948.648829	71.100099	49.443303
945.099150	67.327929	49.448308
941.757781	66.908472	49.453313
937.923380	69.163143	49.458317
934.698739	67.187968	49.463322
931.233289	64.674489	49.468327
927.907474	68.485616	49.473332
924.334591	67.507428	49.478337
920.498252	75.165970	49.483341
917.153707	58.238928	49.488346
913.682165	67.223210	49.493351
910.220335	68.961156	49.498356
906.673196	68.788864	49.503361
903.036384	72.003014	49.508365
899.668361	66.453058	49.513370
896.182460	75.487036	49.518375
892.681611	75.361322	49.523380
889.332173	63.123619	49.528385
885.530579	66.774699	49.533389
882.161522	71.630249	49.538394
878.930653	67.118779	49.543399
875.439045	75.375381	49.548404
871.913805	68.366136	49.553409
867.814240	75.888491	49.558413
864.379674	62.132824	49.563418
861.075399	68.129870	49.568423
857.513164	63.306163	49.573428
854.255528	61.045077	49.578433
850.411218	74.848727	49.583437
847.547966	64.382939	49.588442
844.088161	75.978599	49.593447
840.402747	65.049187	49.598452
836.693633	69.375558	49.603457
832.801317	81.310625	49.608461
829.586600	73.205869	49.613466
826.306238	69.107062	49.618471
822.409712	73.943488	49.623476
819.138017	72.111690	49.628481
815.280658	76.783836	49.633485
812.218463	69.737321	49.638490
808.682939	67.459388	49.643495
805.317364	62.348819	49.648500
801.513798	69.268292	49.653505
798.003272	70.302002	49.658509
794.375270	65.013992	49.663514
790.797460	73.932569	49.668519
787.700606	68.112634	49.673524
784.295151	68.171395	49.678529
780.667707	55.815651	49.683533
777.336201	58.378024	49.688538
773.813347	55.661537	49.693543
769.772841	70.852943	49.698548
766.780548	60.926104	49.703553
762.867059	69.748242	49.708557
759.569246	55.427166	49.713562
756.024697	69.196804	49.718567
752.531798	60.670313	49.723572
749.307643	65.433714	49.728577
745.469635	66.803139	49.733581
742.033244	69.093949	49.738586
738.466259	68.137012	49.743591
734.831457	73.030778	49.748596
731.425844	66.828656	49.753601
727.707178	77.540823	49.758605
724.876387	56.228094	49.763610
721.308310	63.876522	49.768615
717.464618	67.803084	49.773620
713.918932	65.776677	49.778625
710.223957	76.213080	49.783629
706.949469	68.819990	49.788634
703.657292	71.537596	49.793639
699.959871	58.863739	49.798644
696.614473	55.572325	49.803649
693.021889	66.802684	49.808653
689.727986	63.114121	49.813658
686.011774	65.103655	49.818663
682.417507	70.190426	49.823668
679.021725	54.299620	49.828673
675.204116	60.806845	49.833677
671.968234	66.805910	49.838682
668.792007	67.771776	49.843687
664.826660	64.624327	49.848692
661.629674	69.927658	49.853697
657.860536	69.388169	49.858701
654.228574	64.673424	49.863706
651.033816	67.366378	49.868711
647.590327	69.927215	49.873716
644.215286	56.532490	49.878721
640.429373	63.762429	49.883725
637.127653	62.840140	49.888730
633.609473	58.120342	49.893735
629.629139	69.803362	49.898740
626.256938	60.802537	49.903745
622.592637	61.094598	49.908749
619.437231	62.629852	49.913754
615.988148	63.075067	49.918759
612.397856	61.251766	49.923764
608.835271	54.441373	49.928769
605.359435	66.419168	49.933773
602.032488	59.088050	49.938778
598.473753	49.249430	49.943783
594.689539	65.365855	49.948788
591.730223	56.680405	49.953793
587.978486	69.998257	49.958797
584.833817	62.126251	49.963802
581.112737	63.392075	49.968807
577.305513	65.800740	49.973812
573.641918	64.134385	49.978817
570.078298	65.951487	49.983821
566.818572	63.763528	49.988826
563.397720	65.245202	49.993831
559.995732	66.508809	49.998836
556.596755	60.147505	50.003841
552.890775	63.008635	50.008845
549.478193	59.607481	50.013850
545.584559	62.652844	50.018855
542.194065	61.741224	50.023860
538.848865	64.040004	50.028865
535.523093	55.101574	50.033869
532.028391	60.122237	50.038874
528.337988	58.535991	50.043879
524.816917	64.769281	50.048884
521.361515	56.670424	50.053889
517.674273	69.788417	50.058893
514.165485	61.289756	50.063898
511.133757	60.417199	50.068903
507.664391	72.134572	50.073908
504.262081	61.572443	50.078913
500.066719	66.626258	50.083917
496.861131	57.087010	50.088922
493.220647	58.593392	50.093927
489.750080	58.519961	50.098932
486.801988	56.536594	50.103937
482.451271	65.009211	50.108941
479.016712	55.594196	50.113946
475.786906	67.900679	50.118951
472.475778	56.081043	50.123956
468.857128	61.861306	50.128961
465.212108	65.959441	50.133965
461.766879	54.647890	50.138970
458.306879	55.816139	50.143975
454.312283	57.564310	50.148980
450.979019	60.032079	50.153985
447.601393	63.924077	50.158989
444.579768	61.224519	50.163994
440.945002	56.238175	50.168999
437.646878	53.521556	50.174004
433.976384	55.823532	50.179009
429.693120	59.078259	50.184013
426.688159	59.251882	50.189018
423.552353	54.924998	50.194023
419.732629	55.579794	50.199028
416.389986	61.443639	50.204033
412.520964	67.566598	50.209037
409.074530	56.223609	50.214042
405.796641	55.338769	50.219047
401.947931	58.614430	50.224052
398.350960	54.773785	50.229057
395.018620	53.432365	50.234061
391.865652	57.605758	50.239066
388.642334	54.219458	50.244071
384.795055	51.873069	50.249076
381.465802	48.038204	50.254081
377.311356	58.954256	50.259085
374.114839	52.039465	50.264090
370.625271	56.831558	50.269095
367.190447	56.809526	50.274100
363.898917	45.752478	50.279105
360.230166	45.833302	50.284109
356.637858	55.668449	50.289114
353.298625	51.287828	50.294119
349.606916	59.040945	50.299124
346.270071	48.193429	50.304129
342.519361	53.794949	50.309133
339.144104	49.821725	50.314138
335.715532	48.922389	50.319143
332.238847	56.363628	50.324148
328.582015	51.396561	50.329153
324.897954	55.734897	50.334157
321.662202	51.739957	50.339162
318.244352	43.746028	50.344167
314.479589	54.705815	50.349172
311.239581	47.551043	50.354177
307.657115	58.390706	50.359181
304.171264	58.768920	50.364186
300.809011	54.581711	50.369191
296.753195	56.440671	50.374196
293.709406	55.737693	50.379201
289.876245	59.586734	50.384205
286.158585	62.414913	50.389210
283.511804	50.634261	50.394215
279.770271	59.391693	50.399220
276.246850	50.933330	50.404225
272.593811	63.656871	50.409229
269.086063	60.159850	50.414234
265.561398	58.652243	50.419239
262.123425	57.903073	50.424244
258.419425	54.208825	50.429249
254.787285	57.128094	50.434253
251.651334	59.261454	50.439258
248.088227	50.951640	50.444263
244.612347	54.118657	50.449268
241.029682	51.285020	50.454273
237.926954	51.777597	50.459277
234.394933	53.456945	50.464282
230.876395	56.829916	50.469287
226.933636	62.888444	50.474292
223.574419	63.025497	50.479297
219.741000	63.075031	50.484301
216.314204	61.542704	50.489306
212.910214	56.564765	50.494311
209.747948	63.985538	50.499316
206.237732	58.258532	50.504321
202.542896	62.608052	50.509325
198.987482	63.025584	50.514330
196.035180	55.506508	50.519335
191.716063	74.854061	50.524340
188.780260	57.294122	50.529345
184.584059	64.056481	50.534349
181.476072	67.650270	50.539354
178.267834	64.663438	50.544359
174.488544	75.131975	50.549364
170.877645	67.019430	50.554369
167.209537	60.652645	50.559373
163.790391	63.048398	50.564378
160.387576	60.781540	50.569383
157.146985	66.585228	50.574388
153.694386	53.253320	50.579393
150.245485	64.385401	50.584397
146.621340	59.223457	50.589402
143.163266	54.215989	50.594407
139.406103	62.112188	50.599412
135.927758	67.241070	50.604417
132.323484	68.545715	50.609421
128.608232	66.159832	50.614426
125.334719	52.676667	50.619431
121.800397	58.127466	50.624436
118.625049	58.451036	50.629441
114.855536	55.551600	50.634445
111.508989	61.678662	50.639450
108.139661	56.670036	50.644455
104.291102	59.626182	50.649460
101.085691	53.117775	50.654465
97.406770	59.021347	50.659469
94.022239	57.469803	50.664474
90.612403	45.763706	50.669479
86.868324	46.900304	50.674484
83.285056	54.326519	50.679489
79.739666	46.153186	50.684493
76.290960	54.387329	50.689498
73.112503	54.923353	50.694503
69.005322	58.644246	50.699508
65.747458	48.471011	50.704513
62.597414	55.545049	50.709517
58.993756	50.212262	50.714522
55.752295	51.938141	50.719527
51.860573	51.576014	50.724532
48.343065	50.522894	50.729537
44.249200	44.741267	50.734541
41.718586	53.082398	50.739546
37.972339	49.951573	50.744551
34.050691	58.294155	50.749556
30.796334	55.150018	50.754561
27.447049	43.523093	50.759565
23.924676	52.664021	50.764570
20.442504	52.035661	50.769575
16.793853	56.191354	50.774580
13.526582	46.886437	50.779585
9.822318	50.674315	50.784589
6.422354	48.138130	50.789594
3.196083	48.469643	50.794599