Fri Aug 26 13:46:26 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.969358	102.090574	0.000000
1.333781	100.863296	0.005005
1.146893	108.042288	0.010010
1.356164	97.234289	0.015014
0.869957	90.489154	0.020019
0.708008	80.359041	0.025024
0.316048	65.740717	0.030029
0.065105	52.552567	0.035034
-0.434259	41.060857	0.040038
-0.726993	41.609472	0.045043
-1.144952	30.361351	0.050048
-1.195434	15.411501	0.055053
-1.517276	18.043163	0.060058
-1.574013	9.820206	0.065062
-2.049983	11.969682	0.070067
-2.370893	1.813745	0.075072
-2.886931	-6.312384	0.080077
-3.375895	-5.809145	0.085082
-3.081070	-15.048575	0.090086
-3.505704	-15.292481	0.095091
-3.540394	-24.974129	0.100096
-3.960531	-23.497715	0.105101
-4.341592	-18.113963	0.110106
-4.500605	-26.393742	0.115110
-5.025898	-23.069209	0.120115
-5.490515	-27.754966	0.125120
-5.328991	-27.928789	0.130125
-5.929440	-21.261242	0.135130
-5.822973	-31.088246	0.140134
-6.274626	-22.488738	0.145139
-7.029095	-31.292714	0.150144
-6.814376	-27.520272	0.155149
-7.159820	-21.158174	0.160154
-6.853161	-32.867076	0.165158
-7.127780	-29.534118	0.170163
-7.384423	-22.518319	0.175168
-8.023146	-28.847370	0.180173
-8.839428	-20.491635	0.185178
-8.807486	-33.385256	0.190182
-9.093389	-17.978094	0.195187
-8.596075	-27.071880	0.200192
-8.850190	-19.110546	0.205197
-9.636774	-23.224174	0.210202
-9.972100	-24.231767	0.215206
-10.130900	-25.001099	0.220211
-10.287021	-24.486411	0.225216
-9.920728	-18.997565	0.230221
-10.590365	-25.827985	0.235226
-10.978969	-31.683468	0.240230
-11.260238	-15.255171	0.245235
-11.528328	-22.182912	0.250240
-11.342314	-27.855789	0.255245
-12.713766	-28.977297	0.260250
-12.746832	-32.689406	0.265254
-12.823756	-23.455407	0.270259
-13.135256	-9.762109	0.275264
-12.932581	-32.904036	0.280269
-13.041177	-20.957030	0.285274
-13.045560	-28.903392	0.290278
-13.458628	-28.241134	0.295283
-14.106129	-22.970917	0.300288
-14.331949	-22.951559	0.305293
-14.450092	-13.761756	0.310298
-14.377455	-24.921715	0.315302
-15.234479	-18.366074	0.320307
-15.561795	-10.311084	0.325312
-15.565165	-19.209864	0.330317
-15.674114	-12.552403	0.335322
-15.508904	-12.188981	0.340326
-15.903782	-18.116255	0.345331
-16.640068	-17.362545	0.350336
-16.708031	-19.193185	0.355341
-17.088707	-12.816108	0.360346
-17.197111	-23.100026	0.365350
-17.379964	-22.239502	0.370355
-17.804439	-14.814769	0.375360
-18.289329	-21.310137	0.380365
-18.495396	-11.296751	0.385370
-18.354629	-22.037064	0.390374
-18.689384	-19.017433	0.395379
-18.951556	-15.480775	0.400384
-19.361186	-17.384764	0.405389
-19.586625	-20.041904	0.410394
-19.878127	-18.256500	0.415398
-19.819502	-21.106559	0.420403
-19.861057	-20.476836	0.425408
-20.086959	-24.563868	0.430413
-20.956174	-14.143524	0.435418
-21.379726	-18.402258	0.440422
-21.291418	-13.562966	0.445427
-21.280042	-22.391276	0.450432
-21.251703	-18.656250	0.455437
-22.664786	-10.713773	0.460442
-22.318535	-27.743758	0.465446
-22.826446	-19.239890	0.470451
-22.887436	-19.157614	0.475456
-22.829462	-12.352142	0.480461
-23.101049	-14.182716	0.485466
-23.508157	-17.042517	0.490470
-24.423125	-19.200008	0.495475
-24.502398	-20.468922	0.500480
-24.151410	-24.487594	0.505485
-24.519425	-12.338847	0.510490
-24.805767	-20.216002	0.515494
-24.669468	-14.960256	0.520499
-25.014374	-15.393738	0.525504
-25.389176	-20.517408	0.530509
-25.854816	-24.342495	0.535514
-26.030124	-18.206196	0.540518
-25.999908	-21.225833	0.545523
-26.835508	-22.282079	0.550528
-27.025938	-26.602416	0.555533
-27.449315	-12.973959	0.560538
-27.532336	-24.527282	0.565542
-27.062685	-18.450275	0.570547
-27.501665	-22.886932	0.575552
-28.034227	-26.106835	0.580557
-28.513551	-13.690832	0.585562
-28.324678	-33.467655	0.590566
-28.678795	-31.106212	0.595571
-28.703064	-21.557720	0.600576
-29.434348	-23.212318	0.605581
-30.196673	-22.761427	0.610586
-30.080473	-26.800487	0.615590
-30.430399	-23.386203	0.620595
-30.763175	-16.997605	0.625600
-30.261647	-27.348011	0.630605
-30.487645	-21.150039	0.635610
-30.405816	-26.926912	0.640614
-30.779298	-25.884854	0.645619
-31.763357	-21.966891	0.650624
-31.800038	-25.295638	0.655629
-32.108046	-14.241364	0.660634
-32.331457	-26.494137	0.665638
-33.135111	-24.337938	0.670643
-33.366419	-21.865905	0.675648
-33.290553	-23.000792	0.680653
-33.261261	-13.463799	0.685658
-33.131224	-16.903924	0.690662
-33.348575	-19.211160	0.695667
-34.283551	-20.460734	0.700672
-34.410808	-19.368430	0.705677
-35.115216	-17.534555	0.710682
-34.899169	-19.694142	0.715686
-34.815211	-25.876293	0.720691
-34.958125	-15.961325	0.725696
-35.143569	-18.884111	0.730701
-35.957075	-15.207829	0.735706
-36.199229	-22.955826	0.740710
-36.197899	-14.262336	0.745715
-36.305484	-18.450045	0.750720
-36.516450	-26.879915	0.755725
-37.434900	-26.876098	0.760730
-37.422108	-30.396038	0.765734
-37.415925	-26.910655	0.770739
-37.669681	-26.232074	0.775744
-37.635976	-30.663234	0.780749
-38.924405	-19.443659	0.785754
-39.014872	-23.162651	0.790758
-39.208093	-26.802371	0.795763
-39.082937	-25.202058	0.800768
-39.178155	-27.987036	0.805773
-39.221979	-20.669027	0.810778
-39.587379	-17.549716	0.815782
-40.101325	-13.591056	0.820787
-40.515687	-18.578856	0.825792
-40.456544	-31.688674	0.830797
-40.912061	-22.484312	0.835802
-40.805833	-20.086978	0.840806
-41.613428	-16.617253	0.845811
-42.212630	-15.647614	0.850816
-42.241324	-27.876920	0.855821
-42.344729	-16.427414	0.860826
-42.468617	-16.705490	0.865830
-42.409389	-17.562550	0.870835
-42.722545	-13.527590	0.875840
-42.642456	-24.403980	0.880845
-43.501896	-15.978252	0.885850
-43.659177	-17.159093	0.890854
-43.948033	-24.020326	0.895859
-44.120297	-24.581925	0.900864
-43.447267	-25.632626	0.905869
-44.401414	-17.144698	0.910874
-44.862410	-22.454255	0.915878
-45.209504	-14.797971	0.920883
-45.361113	-13.825257	0.925888
-45.012519	-9.918639	0.930893
-45.861694	-14.933649	0.935898
-46.173059	-19.181376	0.940902
-46.438305	-17.349441	0.945907
-47.273421	-17.266852	0.950912
-46.563415	-17.535565	0.955917
-47.088455	-7.630697	0.960922
-47.191441	-12.651162	0.965926
-47.719226	-17.175229	0.970931
-48.118924	-15.043960	0.975936
-48.075614	-16.411051	0.980941
-48.688902	-11.861141	0.985946
-48.698835	-11.489432	0.990950
-48.394260	-12.090475	0.995955
-48.841721	-7.180419	1.000960
-49.635967	-20.701518	1.005965
-49.892424	-14.587384	1.010970
-49.864240	-19.549178	1.015974
-49.615052	-21.622180	1.020979
-50.158208	-15.953771	1.025984
-50.599396	-12.870113	1.030989
-50.985396	-14.559490	1.035994
-51.047644	-16.014546	1.040998
-51.077475	-21.255199	1.046003
-51.423994	-21.795993	1.051008
-51.906331	-23.587424	1.056013
-52.332462	-22.764950	1.061018
-52.388851	-23.512263	1.066022
-52.374805	-23.115815	1.071027
-52.635074	-14.511304	1.076032
-53.331802	-30.046999	1.081037
-53.558111	-21.245306	1.086042
-53.556907	-20.441913	1.091046
-53.607922	-22.297336	1.096051
-53.813545	-24.236251	1.101056
-54.593601	-17.474303	1.106061
-55.284626	-16.341675	1.111066
-55.545364	-14.716078	1.116070
-55.432108	-15.897915	1.121075
-55.449723	-14.939737	1.126080
-55.339840	-21.581488	1.131085
-55.596496	-18.267145	1.136090
-55.452720	-16.014857	1.141094
-56.087242	-15.001754	1.146099
-57.207208	-9.534590	1.151104
-56.992344	-20.517384	1.156109
-57.175945	-18.299543	1.161114
-57.119763	-18.855583	1.166118
-57.203530	-21.819508	1.171123
-57.982094	-24.010889	1.176128
-58.265930	-19.879259	1.181133
-58.661863	-18.378140	1.186138
-58.815242	-20.913626	1.191142
-58.734977	-16.515994	1.196147
-59.086368	-16.923157	1.201152
-59.176047	-23.698346	1.206157
-59.941665	-15.138535	1.211162
-59.847876	-18.300943	1.216166
-59.912290	-8.562705	1.221171
-60.186625	-8.004301	1.226176
-60.562798	-20.100418	1.231181
-61.466458	-17.318063	1.236186
-61.290401	-21.806189	1.241190
-61.394304	-18.335301	1.246195
-61.921508	-16.873853	1.251200
-61.532700	-27.485106	1.256205
-61.757030	-22.622451	1.261210
-62.229829	-27.588494	1.266214
-62.404756	-31.999824	1.271219
-62.951699	-17.830134	1.276224
-62.846295	-24.303514	1.281229
-63.522677	-21.341421	1.286234
-63.560246	-14.742531	1.291238
-63.780326	-22.016254	1.296243
-64.094087	-10.277738	1.301248
-64.296567	-24.049152	1.306253
-64.686071	-17.177177	1.311258
-64.959662	-15.951361	1.316262
-65.435458	-22.403849	1.321267
-65.769189	-18.267614	1.326272
-65.586406	-18.223293	1.331277
-65.862549	-14.674969	1.336282
-66.065184	-22.780281	1.341286
-66.330712	-18.613537	1.346291
-67.108260	-14.623326	1.351296
-67.206310	-18.141828	1.356301
-67.478807	-17.596365	1.361306
-67.494110	-27.043752	1.366310
-67.488487	-19.657517	1.371315
-67.925568	-20.424647	1.376320
-67.508226	-27.728013	1.381325
-68.488817	-16.018550	1.386330
-68.851930	-9.223444	1.391334
-68.786187	-18.841636	1.396339
-68.863416	-14.739010	1.401344
-69.004545	-16.482330	1.406349
-70.179905	-11.449451	1.411354
-70.415171	-17.464846	1.416358
-70.584352	-14.932886	1.421363
-70.855955	-13.811780	1.426368
-70.559993	-18.460939	1.431373
-70.868883	-17.941446	1.436378
-71.008682	-19.773555	1.441382
-70.674335	-26.231962	1.446387
-71.156763	-17.463155	1.451392
-71.424203	-27.235102	1.456397
-71.855214	-23.419067	1.461402
-72.876189	-18.922737	1.466406
-73.188610	-16.260911	1.471411
-73.622290	-21.663301	1.476416
-73.593927	-28.700466	1.481421
-73.568375	-11.911837	1.486426
-73.487205	-18.761082	1.491430
-73.411086	-22.148519	1.496435
-73.690900	-18.090279	1.501440
-74.343905	-11.259529	1.506445
-74.609534	-20.361070	1.511450
-74.890869	-19.039140	1.516454
-74.753779	-17.364758	1.521459
-75.382069	-13.268077	1.526464
-75.851877	-23.720336	1.531469
-75.976176	-25.703549	1.536474
-76.198265	-24.004880	1.541478
-76.190511	-23.022179	1.546483
-76.688952	-13.896549	1.551488
-77.055791	-30.030914	1.556493
-77.510091	-22.231397	1.561498
-77.886636	-30.088172	1.566502
-77.739625	-28.127445	1.571507
-78.023016	-28.039014	1.576512
-77.988083	-27.443345	1.581517
-78.053475	-18.309217	1.586522
-78.441336	-23.661794	1.591526
-78.901476	-30.303371	1.596531
-79.624030	-25.904125	1.601536
-79.563572	-33.740358	1.606541
-79.566894	-23.242878	1.611546
-79.586042	-19.642824	1.616550
-79.939995	-19.774351	1.621555
-80.752503	-18.357063	1.626560
-80.826387	-22.432962	1.631565
-81.100945	-23.083034	1.636570
-81.053870	-25.355511	1.641574
-81.181894	-24.380143	1.646579
-81.779390	-22.290841	1.651584
-81.684777	-20.695264	1.656589
-82.437039	-21.751829	1.661594
-82.555911	-28.582578	1.666598
-82.490787	-24.764701	1.671603
-82.788468	-20.067788	1.676608
-83.145528	-22.327960	1.681613
-83.893925	-20.607453	1.686618
-84.075278	-21.550437	1.691622
-83.595859	-28.221249	1.696627
-84.068493	-30.409643	1.701632
-84.162767	-31.824911	1.706637
-84.999945	-34.143200	1.711642
-85.392024	-25.249264	1.716646
-84.948003	-26.235836	1.721651
-85.447050	-26.990154	1.726656
-85.312555	-31.705915	1.731661
-85.877221	-18.795759	1.736666
-86.656206	-27.194129	1.741670
-86.891667	-33.633414	1.746675
-86.993770	-26.670155	1.751680
-86.823050	-37.661881	1.756685
-86.760230	-26.883648	1.761690
-86.961742	-26.694074	1.766694
-87.675977	-27.949542	1.771699
-88.460800	-25.726673	1.776704
-88.521207	-34.692486	1.781709
-88.411962	-21.036243	1.786714
-88.411753	-28.094333	1.791718
-88.342632	-28.848533	1.796723
-89.369087	-22.424696	1.801728
-89.522388	-31.489938	1.806733
-90.007812	-28.415213	1.811738
-90.171569	-26.203627	1.816742
-89.844736	-29.478244	1.821747
-90.476709	-18.772154	1.826752
-90.927083	-25.829688	1.831757
-91.916764	-18.614339	1.836762
-91.445863	-26.492335	1.841766
-91.088990	-20.037119	1.846771
-91.465824	-18.266901	1.851776
-91.513368	-21.903992	1.856781
-92.134504	-21.509882	1.861786
-93.099115	-21.378657	1.866790
-92.672655	-27.541369	1.871795
-93.067359	-16.793130	1.876800
-93.270795	-26.233368	1.881805
-93.135613	-23.552654	1.886810
-93.480569	-27.067509	1.891814
-93.674707	-23.623701	1.896819
-94.260512	-20.852874	1.901824
-94.500414	-16.892593	1.906829
-94.421514	-20.932172	1.911834
-94.876828	-23.657918	1.916838
-95.337248	-15.313301	1.921843
-95.630088	-16.403435	1.926848
-95.997191	-16.301970	1.931853
-96.122512	-21.141788	1.936858
-96.115961	-19.681191	1.941862
-95.958340	-21.195789	1.946867
-96.488489	-15.368062	1.951872
-96.775540	-26.105027	1.956877
-97.263178	-20.492720	1.961882
-97.644194	-21.898143	1.966886
-97.941443	-21.443735	1.971891
-98.633706	-25.018406	1.976896
-98.208226	-29.671909	1.981901
-98.979904	-20.674578	1.986906
-99.253052	-27.946360	1.991910
-98.953098	-30.172791	1.996915
-99.127309	-18.485429	2.006912
-98.973350	-22.358108	2.016909
-97.985321	-27.463007	2.026906
-98.024692	-19.268371	2.036902
-97.966913	-25.473332	2.046899
-96.943720	-20.919091	2.056896
-96.476835	-17.877915	2.066893
-96.223416	-19.323793	2.076890
-95.179940	-21.006720	2.086886
-95.380385	-14.659106	2.096883
-94.363478	-19.160308	2.106880
-93.643211	-21.116015	2.116877
-93.749647	-17.953895	2.126874
-93.226762	-19.685642	2.136870
-92.551949	-19.711485	2.146867
-91.878212	-17.795368	2.156864
-91.084055	-21.270400	2.166861
-90.780069	-19.407581	2.176858
-90.712250	-24.676470	2.186854
-90.263906	-22.905817	2.196851
-89.368635	-18.882836	2.206848
-89.176024	-22.419424	2.216845
-88.494584	-21.090528	2.226842
-88.172805	-19.423709	2.236838
-87.674818	-22.364803	2.246835
-86.711055	-20.420986	2.256832
-86.679263	-21.822854	2.266829
-85.827028	-18.109940	2.276826
-85.302151	-22.924157	2.286822
-85.302233	-22.334921	2.296819
-84.282711	-16.303964	2.306816
-83.765765	-17.686340	2.316813
-83.722855	-14.946601	2.326810
-82.511411	-18.334556	2.336806
-82.425464	-20.609635	2.346803
-82.498905	-14.186764	2.356800
-81.464632	-9.966852	2.366797
-81.123684	-26.244808	2.376794
-80.209253	-14.349935	2.386790
-79.387863	-16.226357	2.396787
-79.708690	-14.253583	2.406784
-79.366837	-14.322615	2.416781
-78.375515	-20.235790	2.426778
-78.066292	-16.799445	2.436774
-77.305821	-20.766559	2.446771
-76.858349	-27.054369	2.456768
-76.720400	-14.956238	2.466765
-75.920810	-22.309367	2.476762
-75.110149	-24.779643	2.486758
-75.327215	-17.612178	2.496755
-74.547216	-17.939490	2.506752
-74.157223	-21.199545	2.516749
-73.126098	-17.669700	2.526746
-72.354813	-20.279560	2.536742
-72.400126	-18.010741	2.546739
-72.348443	-18.870863	2.556736
-71.534331	-19.634293	2.566733
-71.047409	-23.517635	2.576730
-70.449250	-17.836038	2.586726
-69.531999	-19.201549	2.596723
-69.595626	-12.257536	2.606720
-69.206823	-11.614812	2.616717
-68.220490	-10.878230	2.626714
-67.936499	-16.991708	2.636710
-67.506247	-22.893548	2.646707
-66.580038	-20.699971	2.656704
-66.351351	-15.065380	2.666701
-66.148630	-17.330132	2.676698
-65.590473	-16.754957	2.686694
-65.222160	-21.652499	2.696691
-63.982876	-21.082008	2.706688
-63.916093	-16.968042	2.716685
-63.667842	-21.717015	2.726682
-62.623496	-14.277131	2.736678
-62.481022	-12.921336	2.746675
-62.242682	-15.860016	2.756672
-61.050429	-16.625304	2.766669
-61.078248	-22.110544	2.776666
-60.626022	-12.525804	2.786662
-59.891721	-16.773937	2.796659
-59.608099	-14.616519	2.806656
-58.519981	-13.822927	2.816653
-58.163748	-13.409541	2.826650
-57.847264	-16.921070	2.836646
-57.915301	-18.966274	2.846643
-57.066605	-10.064129	2.856640
-56.416400	-8.017638	2.866637
-55.354767	-19.415530	2.876634
-55.240661	-16.218058	2.886630
-55.124159	-18.025909	2.896627
-54.751947	-19.959101	2.906624
-53.899290	-17.880779	2.916621
-53.694406	-21.872257	2.926618
-52.949644	-23.825442	2.936614
-52.225280	-18.651319	2.946611
-51.424971	-22.092464	2.956608
-51.334694	-18.416128	2.966605
-50.639533	-24.096296	2.976602
-50.627880	-20.166975	2.986598
-49.989037	-23.877575	2.996595
-49.431806	-15.348186	3.006592
-48.949756	-26.320059	3.016589
-47.812575	-19.081524	3.026586
-47.682813	-23.165840	3.036582
-47.462029	-23.554964	3.046579
-47.274384	-20.723723	3.056576
-46.547055	-24.223194	3.066573
-45.883386	-20.290857	3.076570
-45.505674	-19.678083	3.086566
-44.948198	-20.835527	3.096563
-43.973540	-23.952204	3.106560
-43.510677	-19.472268	3.116557
-43.374572	-19.721500	3.126554
-43.283411	-22.095589	3.136550
-42.211402	-29.221879	3.146547
-41.726071	-23.985197	3.156544
-41.619921	-19.227983	3.166541
-40.396236	-25.975593	3.176538
-40.030111	-22.114134	3.186534
-40.322740	-30.554776	3.196531
-39.287840	-26.059374	3.206528
-38.921443	-26.597877	3.216525
-38.774827	-16.332016	3.226522
-37.694434	-29.022074	3.236518
-37.243144	-23.244752	3.246515
-36.664721	-24.852102	3.256512
-35.922697	-22.271897	3.266509
-35.544566	-22.026640	3.276506
-35.706694	-22.511362	3.286502
-35.180040	-23.743199	3.296499
-34.677117	-26.200405	3.306496
-33.886554	-21.800000	3.316493
-33.267315	-22.868862	3.326490
-32.843255	-24.597891	3.336486
-31.717794	-30.620644	3.346483
-31.848295	-19.722447	3.356480
-31.594738	-22.989768	3.366477
-30.925231	-20.977959	3.376474
-30.424883	-24.052464	3.386470
-30.069361	-27.902676	3.396467
-29.089807	-25.859949	3.406464
-29.196827	-17.740303	3.416461
-28.189902	-18.308846	3.426458
-27.415342	-23.675104	3.436454
-27.264241	-26.866287	3.446451
-26.953618	-21.345819	3.456448
-26.393299	-19.716138	3.466445
-25.498741	-28.683736	3.476442
-25.560059	-27.673166	3.486438
-24.623775	-28.278225	3.496435
-24.086085	-30.927737	3.506432
-24.112095	-23.527100	3.516429
-23.064361	-25.004788	3.526426
-22.413366	-28.596907	3.536422
-22.272312	-28.203868	3.546419
-22.388086	-21.460805	3.556416
-21.057432	-19.672307	3.566413
-20.828056	-18.307867	3.576410
-20.593002	-22.079139	3.586406
-19.740119	-24.866421	3.596403
-19.527579	-18.785838	3.606400
-18.959254	-20.898446	3.616397
-18.405059	-17.915208	3.626394
-17.922693	-26.147079	3.636390
-17.120264	-23.674477	3.646387
-16.810531	-24.920055	3.656384
-15.823341	-26.860302	3.666381
-15.599858	-25.494946	3.676378
-15.325479	-25.531297	3.686374
-15.030940	-27.487240	3.696371
-14.144862	-23.893628	3.706368
-13.912485	-20.362957	3.716365
-13.267390	-26.466136	3.726362
-12.358502	-23.858059	3.736358
-12.237501	-21.098801	3.746355
-12.106767	-29.652879	3.756352
-11.297823	-22.999941	3.766349
-10.662437	-26.399568	3.776346
-10.503802	-27.900377	3.786342
-9.482468	-26.842970	3.796339
-9.168671	-27.180054	3.806336
-9.122895	-26.921062	3.816333
-7.926122	-26.625874	3.826330
-7.537649	-31.079910	3.836326
-7.714761	-24.384315	3.846323
-6.846555	-20.591523	3.856320
-6.573457	-24.045613	3.866317
-5.696601	-19.307028	3.876314
-5.130081	-23.734936	3.886310
-4.991702	-18.824354	3.896307
-4.401260	-4.804182	3.906304
-4.242612	-10.609890	3.916301
-3.510416	10.376155	3.926298
-3.161484	9.723166	3.936294
-2.677291	26.873752	3.946291
-2.290803	45.718448	3.956288
-1.912652	56.781412	3.966285
-1.420373	70.854940	3.976282
-0.807694	84.187496	3.986278
-0.138591	105.243664	3.996275
0.000000	113.084008	4.001280
0.428762	125.656109	4.006285
0.124808	122.932079	4.011290
0.405512	125.874891	4.016294
1.091753	141.779383	4.021299
1.001733	158.127446	4.026304
0.904295	148.385872	4.031309
0.801146	151.995878	4.036314
1.012070	150.520421	4.041318
1.168907	159.945904	4.046323
1.116970	160.760744	4.051328
1.049337	156.759755	4.056333
1.061301	163.040962	4.061338
1.398223	161.109299	4.066342
1.458407	157.724307	4.071347
0.923004	145.456714	4.076352
1.001357	140.657900	4.081357
0.988407	154.130839	4.086362
1.028748	156.579584	4.091366
1.177390	162.042265	4.096371
1.027686	168.130351	4.101376
1.139114	159.960234	4.106381
1.055029	158.008702	4.111386
1.326796	154.188981	4.116390
1.461235	157.847416	4.121395
1.150003	168.389793	4.126400
1.295706	158.303481	4.131405
1.198073	163.092680	4.136410
1.323538	151.487797	4.141414
1.228680	158.870773	4.146419
0.814230	164.376835	4.151424
1.290607	154.998321	4.156429
1.322695	159.384518	4.161434
1.247103	158.874298	4.166438
1.416624	165.428360	4.171443
1.482056	170.189009	4.176448
1.111644	164.324301	4.181453
1.027014	166.033223	4.186458
1.192982	161.910442	4.191462
0.976053	165.753296	4.196467
1.415893	179.313940	4.201472
1.959499	177.106493	4.206477
1.251986	174.597144	4.211482
1.343958	169.986022	4.216486
1.361117	168.448985	4.221491
1.884700	179.291650	4.226496
1.569379	181.511043	4.231501
1.570724	178.821726	4.236506
1.267443	176.888502	4.241510
1.498448	177.248011	4.246515
1.631463	192.109252	4.251520
2.043741	180.235073	4.256525
1.848533	174.700578	4.261530
1.517097	168.228702	4.266534
1.445432	163.291892	4.271539
1.681157	166.637173	4.276544
1.484677	172.216865	4.281549
1.493997	170.930979	4.286554
1.754247	167.650873	4.291558
1.733095	163.459153	4.296563
1.507338	172.314641	4.301568
2.042419	174.945780	4.306573
1.417502	172.009130	4.311578
1.489552	171.675234	4.316582
1.578101	185.480398	4.321587
1.721496	187.938411	4.326592
1.822282	184.341454	4.331597
1.991631	182.885121	4.336602
2.221987	191.827788	4.341606
1.873339	176.927389	4.346611
1.414679	167.792525	4.351616
2.199675	173.886940	4.356621
1.899809	164.050328	4.361626
1.892915	166.054023	4.366630
1.801773	161.718180	4.371635
1.495405	169.387186	4.376640
1.960513	175.480788	4.381645
1.972576	178.993770	4.386650
2.262680	184.140210	4.391654
1.977116	171.197801	4.396659
1.614897	170.798645	4.401664
1.932162	180.328872	4.406669
1.995114	178.265862	4.411674
2.066625	181.152671	4.416678
2.227304	180.754357	4.421683
1.846680	164.884535	4.426688
2.296714	158.275172	4.431693
1.709700	158.806335	4.436698
1.879417	178.470632	4.441702
2.489274	184.744176	4.446707
2.249925	179.001422	4.451712
1.884704	167.893695	4.456717
1.808055	166.924907	4.461722
1.881238	180.609076	4.466726
2.084066	180.972973	4.471731
1.970757	188.403125	4.476736
2.256251	187.128021	4.481741
1.988050	193.452859	4.486746
2.370814	187.901137	4.491750
2.426605	185.804440	4.496755
2.085298	196.288242	4.501760
2.200955	191.230512	4.506765
1.986933	194.183926	4.511770
1.935352	196.858955	4.516774
1.966133	189.074695	4.521779
1.799552	193.991693	4.526784
1.920718	186.699550	4.531789
1.757063	193.479499	4.536794
2.094175	194.382459	4.541798
2.277054	204.006387	4.546803
2.285805	213.072150	4.551808
2.715070	209.863796	4.556813
2.519395	205.689747	4.561818
2.378983	203.478067	4.566822
2.264732	191.793424	4.571827
1.905999	196.420809	4.576832
2.497584	202.172033	4.581837
2.115977	214.193342	4.586842
2.239585	211.874116	4.591846
2.471559	213.296473	4.596851
2.503789	215.471248	4.601856
2.495061	213.428885	4.606861
2.451278	221.503108	4.611866
2.491774	210.145529	4.616870
2.626756	210.146675	4.621875
2.339644	215.297576	4.626880
2.510914	215.571476	4.631885
2.478844	216.718575	4.636890
2.276005	217.231053	4.641894
2.373193	224.900524	4.646899
2.150888	221.923326	4.651904
2.393451	218.664947	4.656909
2.739920	220.784470	4.661914
2.362754	214.708830	4.666918
2.496943	216.083137	4.671923
2.410979	214.245784	4.676928
2.726258	210.182001	4.681933
2.463104	216.695883	4.686938
2.477426	221.904255	4.691942
2.893485	227.325320	4.696947
2.673491	234.936614	4.701952
2.769501	226.322787	4.706957
2.435633	221.496386	4.711962
2.554027	233.677135	4.716966
3.042225	234.948871	4.721971
2.951575	242.910181	4.726976
3.155539	228.363451	4.731981
2.804740	222.473524	4.736986
2.583330	220.704715	4.741990
2.488002	214.455482	4.746995
2.711993	227.559400	4.752000
2.770673	228.898010	4.757005
3.028133	241.057112	4.762010
3.013322	237.895748	4.767014
3.133713	229.157904	4.772019
2.874952	227.097522	4.777024
3.052542	212.162616	4.782029
2.990234	215.506854	4.787034
2.761281	220.895469	4.792038
3.044522	212.774505	4.797043
3.136233	221.969721	4.802048
2.703108	212.539800	4.807053
2.658976	209.528536	4.812058
2.875118	226.974246	4.817062
3.143238	231.311056	4.822067
3.333977	235.501732	4.827072
3.067104	226.311667	4.832077
3.009252	220.316020	4.837082
3.098123	217.837691	4.842086
2.916319	210.561073	4.847091
2.464306	225.193896	4.852096
2.970505	231.600652	4.857101
2.984586	239.004665	4.862106
3.212413	239.079938	4.867110
3.276722	239.446421	4.872115
2.858968	233.554260	4.877120
3.036307	234.975633	4.882125
3.035309	238.898776	4.887130
2.987541	238.447495	4.892134
3.148172	249.501734	4.897139
2.960445	246.142670	4.902144
3.180908	244.662556	4.907149
2.969366	249.510642	4.912154
2.977656	241.071814	4.917158
3.194222	238.386942	4.922163
2.732491	240.746194	4.927168
3.182408	236.303946	4.932173
3.309546	251.564776	4.937178
3.433605	263.130908	4.942182
3.597128	244.189769	4.947187
3.091470	249.982135	4.952192
3.331106	242.295045	4.957197
3.253232	239.276375	4.962202
3.498835	255.866494	4.967206
3.497048	245.084940	4.972211
3.284995	249.025126	4.977216
3.267007	244.076773	4.982221
3.432640	245.341785	4.987226
3.335768	260.178766	4.992230
3.657546	259.616165	4.997235
3.065784	258.066362	5.002240
3.886672	265.667464	5.007245
3.435379	260.644204	5.012250
3.245832	252.353230	5.017254
4.018001	252.834123	5.022259
3.290598	255.380270	5.027264
3.167887	254.402831	5.032269
3.427986	276.925795	5.037274
3.680880	263.507184	5.042278
3.619536	256.139027	5.047283
3.620005	267.626330	5.052288
3.782451	267.338468	5.057293
3.694376	269.509835	5.062298
3.131715	263.535824	5.067302
3.765653	269.008398	5.072307
3.552396	268.285496	5.077312
3.463779	264.040982	5.082317
3.433352	271.328553	5.087322
3.504605	279.233035	5.092326
3.877218	272.347788	5.097331
3.283471	277.979875	5.102336
3.762706	269.540474	5.107341
3.833642	265.865891	5.112346
3.857691	274.546497	5.117350
3.953349	264.923489	5.122355
3.888788	275.772365	5.127360
3.786072	269.084511	5.132365
4.116559	261.177627	5.137370
3.661159	271.653928	5.142374
4.014425	267.467161	5.147379
3.947118	270.524292	5.152384
4.135842	263.961903	5.157389
3.521296	265.338897	5.162394
3.784487	274.178418	5.167398
4.058069	266.308866	5.172403
3.956403	277.233121	5.177408
4.044065	259.604055	5.182413
3.822707	271.442268	5.187418
3.606539	262.399311	5.192422
3.877518	262.091387	5.197427
3.689055	268.989120	5.202432
3.788614	262.276102	5.207437
4.093120	272.048805	5.212442
4.072509	269.131943	5.217446
3.909929	267.543791	5.222451
3.759568	264.656622	5.227456
3.718527	276.890698	5.232461
3.763162	267.323087	5.237466
3.633846	279.555090	5.242470
3.691391	270.523296	5.247475
3.747716	282.359409	5.252480
3.887211	292.619715	5.257485
3.849829	293.891030	5.262490
3.804877	293.806299	5.267494
4.050694	291.971063	5.272499
4.153042	302.392179	5.277504
4.439199	296.371419	5.282509
4.429631	295.151738	5.287514
4.069940	294.828114	5.292518
4.259252	293.517358	5.297523
3.756236	306.449794	5.302528
4.034973	295.339800	5.307533
4.224198	300.416561	5.312538
3.758426	293.497327	5.317542
4.254276	294.467325	5.322547
3.996476	301.410667	5.327552
4.274160	293.050090	5.332557
4.172118	293.157742	5.337562
3.935215	292.160115	5.342566
3.951258	290.711825	5.347571
4.062773	313.011200	5.352576
4.482811	310.481297	5.357581
4.734522	317.215603	5.362586
4.389077	317.111220	5.367590
4.940171	316.228180	5.372595
4.626130	313.951773	5.377600
4.484315	302.113164	5.382605
4.757389	309.831215	5.387610
4.272763	303.762785	5.392614
4.204901	297.645286	5.397619
3.821663	298.565497	5.402624
4.461852	296.042447	5.407629
4.254991	303.094914	5.412634
4.181602	314.672839	5.417638
4.745780	317.188740	5.422643
4.367635	326.561568	5.427648
4.069174	319.695368	5.432653
4.291235	328.949437	5.437658
4.259431	316.922850	5.442662
4.492289	325.580461	5.447667
4.433121	328.857794	5.452672
4.634064	324.210684	5.457677
4.948871	316.170178	5.462682
4.880061	321.590836	5.467686
4.640054	324.871015	5.472691
4.554671	322.726681	5.477696
4.808363	315.429670	5.482701
4.349345	325.637651	5.487706
4.398448	328.989874	5.492710
4.798222	324.568066	5.497715
4.564057	323.876890	5.502720
4.371990	326.197331	5.507725
4.450371	332.487239	5.512730
4.493063	324.236001	5.517734
4.524444	325.537740	5.522739
4.996234	323.638845	5.527744
4.610950	331.218968	5.532749
5.042984	330.196280	5.537754
4.813524	332.952808	5.542758
4.715646	324.729783	5.547763
4.918138	326.628130	5.552768
4.577553	326.874161	5.557773
4.974993	340.403565	5.562778
5.107108	341.215066	5.567782
4.817340	331.743779	5.572787
4.766517	333.757496	5.577792
4.845813	334.146957	5.582797
4.742275	343.458056	5.587802
4.786983	340.603778	5.592806
5.237537	344.538895	5.597811
4.950542	352.660536	5.602816
5.084198	353.389541	5.607821
4.834258	341.396901	5.612826
4.597321	350.750920	5.617830
4.997033	349.666825	5.622835
4.935676	350.464158	5.627840
5.283482	350.346748	5.632845
4.952995	350.534260	5.637850
4.776858	354.418258	5.642854
4.838714	346.407632	5.647859
4.975583	351.638090	5.652864
4.790538	347.411733	5.657869
4.945257	355.293762	5.662874
5.066926	346.786612	5.667878
5.211730	341.933106	5.672883
5.070002	360.130680	5.677888
5.187677	357.040415	5.682893
5.156896	347.895786	5.687898
4.975588	357.405659	5.692902
5.100483	357.231209	5.697907
5.118299	345.810636	5.702912
5.108858	350.978454	5.707917
5.034036	352.780777	5.712922
5.102379	354.937292	5.717926
5.229429	343.809757	5.722931
5.152087	363.079297	5.727936
5.390141	372.489085	5.732941
5.419751	361.905048	5.737946
5.436669	356.565256	5.742950
5.456886	356.413431	5.747955
5.257441	356.773526	5.752960
5.176751	352.742888	5.757965
5.271803	353.544342	5.762970
5.204305	364.482314	5.767974
5.351126	369.521405	5.772979
5.561093	378.540105	5.777984
5.732528	369.063428	5.782989
5.877976	358.208261	5.787994
5.578579	361.779263	5.792998
5.628380	350.451782	5.798003
5.622647	354.204847	5.803008
5.307089	359.243161	5.808013
5.544478	351.344406	5.813018
4.895236	361.680100	5.818022
5.229418	353.886493	5.823027
5.400358	352.898129	5.828032
5.383896	350.467818	5.833037
5.633373	361.030574	5.838042
5.534092	360.754987	5.843046
5.714350	363.628059	5.848051
5.427673	354.830147	5.853056
5.538473	369.989221	5.858061
5.515950	374.323863	5.863066
5.638535	378.126556	5.868070
5.755415	374.913027	5.873075
5.508084	374.840822	5.878080
5.950434	375.047209	5.883085
5.610735	363.875275	5.888090
5.159593	377.609594	5.893094
5.787188	379.498707	5.898099
5.668198	375.575266	5.903104
5.757201	373.264572	5.908109
5.896527	378.510474	5.913114
5.807033	380.087298	5.918118
5.690617	376.372261	5.923123
5.692247	383.825728	5.928128
5.842291	380.489977	5.933133
5.674652	381.303859	5.938138
6.135177	380.941112	5.943142
6.137821	379.937820	5.948147
5.850729	368.112295	5.953152
5.836558	363.242407	5.958157
5.642128	348.428582	5.963162
5.610398	366.251538	5.968166
5.888991	379.432487	5.973171
6.012941	370.434595	5.978176
5.844969	382.840364	5.983181
6.245033	380.629932	5.988186
5.624344	381.849705	5.993190
6.103439	378.630399	5.998195
6.156407	383.468975	6.003200
5.598841	378.645723	6.008205
5.998164	371.272231	6.013210
5.871174	380.991956	6.018214
6.019196	375.059114	6.023219
5.820910	378.244223	6.028224
6.067989	371.748638	6.033229
5.834128	382.016506	6.038234
5.688629	380.973005	6.043238
5.906016	383.938374	6.048243
5.611305	389.065199	6.053248
5.753413	388.745700	6.058253
5.493913	382.800377	6.063258
5.631207	383.968573	6.068262
5.665648	379.578323	6.073267
5.976774	380.618215	6.078272
5.892524	384.563843	6.083277
6.102437	385.549892	6.088282
5.653622	392.057943	6.093286
6.240079	384.307302	6.098291
5.747697	379.388480	6.103296
6.032240	381.312023	6.108301
5.878272	385.208395	6.113306
5.864723	391.522128	6.118310
5.641269	387.191012	6.123315
5.790021	392.011513	6.128320
5.830902	404.096881	6.133325
6.239580	398.797319	6.138330
5.861269	408.711211	6.143334
6.090116	400.968786	6.148339
5.889018	391.993019	6.153344
5.866045	392.300329	6.158349
5.897580	390.080836	6.163354
5.464795	405.239153	6.168358
5.812923	399.980656	6.173363
6.014046	407.406236	6.178368
5.937100	407.241065	6.183373
6.135512	409.162202	6.188378
5.934422	413.667023	6.193382
6.067210	406.493202	6.198387
5.906881	414.753336	6.203392
5.885930	408.017898	6.208397
6.338258	408.624524	6.213402
5.733395	408.190375	6.218406
6.278031	408.874377	6.223411
6.145406	400.938298	6.228416
5.868055	401.338997	6.233421
6.342294	387.477711	6.238426
5.941694	378.333699	6.243430
6.222417	378.470339	6.248435
5.892769	375.905292	6.253440
5.909559	387.320529	6.258445
5.952726	374.478648	6.263450
5.872382	384.539120	6.268454
6.052157	378.307108	6.273459
5.946084	389.260592	6.278464
5.835874	390.274338	6.283469
6.028356	381.341699	6.288474
5.661018	388.378058	6.293478
6.020673	381.706756	6.298483
5.958336	388.107176	6.303488
6.026378	386.150916	6.308493
6.083242	384.911395	6.313498
5.932599	384.083828	6.318502
6.048265	383.942451	6.323507
5.946458	383.148408	6.328512
5.935094	378.448919	6.333517
6.022476	382.380478	6.338522
6.075818	381.755266	6.343526
6.341901	376.677226	6.348531
6.008817	374.985899	6.353536
6.165989	382.035502	6.358541
6.378241	376.845622	6.363546
5.833298	389.414492	6.368550
5.681274	380.851863	6.373555
5.793875	382.767376	6.378560
5.975126	382.369018	6.383565
6.227931	375.777628	6.388570
5.835105	383.653173	6.393574
5.549174	376.576194	6.398579
5.871005	383.201533	6.403584
5.783892	378.301869	6.408589
5.691719	376.667944	6.413594
5.628353	380.841270	6.418598
5.948275	385.714211	6.423603
5.754567	385.098990	6.428608
5.642253	383.249904	6.433613
6.144704	383.241292	6.438618
5.947179	382.332440	6.443622
6.073406	383.350501	6.448627
6.027893	388.242376	6.453632
5.925019	375.011950	6.458637
6.335338	380.358026	6.463642
5.970254	383.100876	6.468646
6.123669	389.951754	6.473651
5.797883	391.448311	6.478656
5.917741	393.207673	6.483661
5.982882	381.197586	6.488666
6.114049	387.548897	6.493670
6.035917	385.042763	6.498675
5.990159	390.852153	6.503680
5.857499	381.486090	6.508685
6.242168	379.211617	6.513690
5.728882	385.245656	6.518694
6.151089	388.242410	6.523699
6.196569	381.487147	6.528704
6.066130	378.391217	6.533709
6.450786	380.855986	6.538714
6.039724	381.922900	6.543718
6.144992	386.076299	6.548723
5.840733	386.300856	6.553728
6.046020	386.683356	6.558733
6.020098	383.675555	6.563738
5.936387	389.756605	6.568742
5.958820	380.243011	6.573747
5.933627	379.633190	6.578752
6.176625	381.085480	6.583757
5.759734	361.456313	6.588762
5.406396	374.776775	6.593766
5.955193	381.708457	6.598771
5.984887	377.812485	6.603776
5.909986	381.914842	6.608781
6.101111	377.411614	6.613786
5.967798	379.634330	6.618790
5.876042	380.379450	6.623795
5.769185	385.616228	6.628800
6.084054	387.310426	6.633805
6.294747	390.808342	6.638810
6.149157	388.875852	6.643814
6.192524	373.490315	6.648819
6.058624	369.603998	6.653824
5.808790	361.252758	6.658829
6.012563	358.876740	6.663834
5.758143	361.197402	6.668838
6.302573	351.153303	6.673843
6.072492	353.005110	6.678848
6.006517	350.826114	6.683853
5.643427	347.010287	6.688858
5.498668	359.700323	6.693862
5.710495	369.285032	6.698867
5.807235	376.568666	6.703872
5.923833	375.633053	6.708877
6.193168	380.548670	6.713882
5.774618	388.662337	6.718886
6.156557	387.562025	6.723891
5.797114	384.593497	6.728896
5.786817	383.117663	6.733901
5.906276	379.460812	6.738906
5.737164	388.361371	6.743910
5.929757	385.420786	6.748915
6.005824	384.769890	6.753920
5.858218	385.153551	6.758925
6.099373	381.721358	6.763930
5.650337	386.957630	6.768934
5.963187	380.692243	6.773939
6.011131	386.793922	6.778944
6.080282	383.261961	6.783949
6.193487	383.756873	6.788954
6.181908	384.201612	6.793958
5.881177	386.153006	6.798963
6.279229	380.038867	6.803968
5.870288	376.862914	6.808973
6.012282	372.272425	6.813978
5.658806	375.155834	6.818982
5.910935	385.556842	6.823987
6.155949	384.047584	6.828992
6.119990	379.260177	6.833997
5.914273	367.950322	6.839002
5.604136	375.003079	6.844006
5.911172	371.794745	6.849011
6.294444	377.670208	6.854016
5.651449	380.649314	6.859021
5.780484	383.552510	6.864026
5.975807	394.433761	6.869030
5.963390	386.700432	6.874035
6.089884	393.612450	6.879040
6.315497	393.624795	6.884045
6.030812	374.626753	6.889050
5.750902	360.648792	6.894054
5.644383	366.492944	6.899059
5.708197	376.635370	6.904064
5.746452	385.187270	6.909069
6.188705	382.160359	6.914074
5.973788	388.394713	6.919078
6.423737	385.616536	6.924083
5.991611	375.673851	6.929088
5.735145	376.087116	6.934093
6.078480	382.557249	6.939098
5.888723	391.609718	6.944102
6.110674	378.376171	6.949107
5.936403	382.810370	6.954112
5.550390	380.703346	6.959117
5.865952	373.940836	6.964122
6.100701	392.105137	6.969126
5.975367	386.300272	6.974131
5.900671	388.706849	6.979136
6.173406	387.250222	6.984141
6.121709	383.939554	6.989146
5.781862	372.634761	6.994150
5.874059	362.436444	6.999155
5.680733	380.768621	7.004160
5.588389	390.403865	7.009165
6.245388	384.695490	7.014170
6.018321	391.232290	7.019174
6.114008	384.766598	7.024179
6.045400	385.710592	7.029184
6.059993	385.664044	7.034189
5.868149	378.964716	7.039194
5.584751	385.032563	7.044198
6.340520	381.479118	7.049203
6.090027	379.373140	7.054208
5.781919	371.654218	7.059213
6.009442	374.273163	7.064218
5.885424	372.906784	7.069222
5.810455	376.072692	7.074227
5.951621	383.852442	7.079232
5.929235	381.701456	7.084237
6.649892	377.024034	7.089242
5.892272	372.491355	7.094246
5.847512	360.020673	7.099251
5.804827	357.328693	7.104256
5.514079	352.815076	7.109261
5.645333	353.421071	7.114266
6.019264	385.689651	7.119270
5.835180	378.040001	7.124275
5.953640	377.664074	7.129280
5.877297	380.580264	7.134285
6.103088	375.094052	7.139290
5.831959	380.622157	7.144294
5.955268	367.549506	7.149299
6.199280	377.901155	7.154304
5.707784	388.566639	7.159309
6.319947	375.898754	7.164314
6.181261	384.797737	7.169318
6.100331	377.603420	7.174323
5.975043	364.205651	7.179328
5.956526	366.957813	7.184333
5.976370	351.908147	7.189338
5.859518	362.993005	7.194342
6.001736	357.311005	7.199347
5.743023	361.147752	7.204352
5.949029	363.093012	7.209357
6.072071	365.766187	7.214362
5.961986	363.745915	7.219366
5.916892	352.800198	7.224371
5.941029	352.521214	7.229376
5.557735	363.615919	7.234381
6.149803	364.782909	7.239386
6.108698	377.570713	7.244390
6.046700	359.724407	7.249395
5.797180	359.529159	7.254400
5.593082	364.053418	7.259405
6.147652	376.580800	7.264410
5.919922	380.801863	7.269414
6.343630	378.011955	7.274419
6.096092	360.567854	7.279424
5.831857	349.308250	7.284429
5.963193	347.607891	7.289434
5.847708	357.885788	7.294438
5.872971	356.426566	7.299443
5.780356	351.388563	7.304448
5.736100	361.051104	7.309453
6.222435	370.991702	7.314458
6.063063	377.125657	7.319462
5.798255	361.440104	7.324467
6.014353	362.270167	7.329472
5.755576	359.377717	7.334477
6.026068	366.264140	7.339482
6.067988	374.128939	7.344486
5.787710	366.029206	7.349491
5.852168	362.456851	7.354496
6.040402	374.231359	7.359501
6.365225	360.304774	7.364506
5.928787	360.271504	7.369510
5.664879	354.143381	7.374515
5.870588	365.893017	7.379520
6.074207	373.039787	7.384525
6.015526	360.128353	7.389530
5.658343	366.141245	7.394534
6.027947	378.994816	7.399539
6.123588	369.194586	7.404544
5.879185	371.836388	7.409549
6.101932	355.723758	7.414554
5.840525	361.307290	7.419558
5.758219	363.721376	7.424563
6.167466	372.924178	7.429568
5.776716	368.720353	7.434573
6.064512	372.282189	7.439578
5.869549	367.962461	7.444582
5.740745	368.453924	7.449587
6.274488	378.497875	7.454592
6.126260	380.340104	7.459597
6.165286	361.424552	7.464602
5.878306	366.085101	7.469606
5.846092	364.305801	7.474611
5.796198	361.032821	7.479616
5.708187	358.572521	7.484621
6.059883	349.178518	7.489626
5.978502	370.096985	7.494630
5.764115	364.559090	7.499635
6.076758	360.207786	7.504640
5.735071	371.650354	7.509645
6.024107	367.375489	7.514650
5.847020	374.869432	7.519654
6.061489	387.955968	7.524659
6.169245	381.779460	7.529664
5.752220	370.774583	7.534669
6.023123	363.553965	7.539674
5.759292	367.771155	7.544678
5.988516	379.843001	7.549683
6.171281	377.274102	7.554688
5.870509	371.167531	7.559693
5.919265	359.574455	7.564698
5.879601	373.336454	7.569702
6.087324	374.417754	7.574707
6.021178	359.296050	7.579712
5.853531	363.982311	7.584717
5.847954	357.564032	7.589722
6.000823	361.865036	7.594726
5.891497	362.609727	7.599731
5.921496	368.391496	7.604736
5.947973	372.857712	7.609741
5.937404	365.070322	7.614746
5.731749	371.850550	7.619750
5.976192	377.054776	7.624755
6.100550	377.740938	7.629760
5.999811	376.310823	7.634765
6.137479	363.017645	7.639770
5.852223	368.516308	7.644774
5.567859	360.448851	7.649779
6.175781	378.972646	7.654784
5.983996	376.439917	7.659789
6.029862	368.270421	7.664794
5.997475	360.407337	7.669798
6.127318	357.837190	7.674803
5.866134	364.259071	7.679808
5.786593	363.714659	7.684813
6.071376	360.231385	7.689818
5.813578	359.452140	7.694822
5.872395	359.661294	7.699827
6.253421	365.957876	7.704832
6.206518	360.343286	7.709837
6.207020	360.624794	7.714842
6.101833	357.164274	7.719846
5.705870	354.815196	7.724851
5.839755	350.159537	7.729856
5.890291	362.002932	7.734861
6.527878	354.196887	7.739866
6.215705	354.821303	7.744870
5.967997	357.216848	7.749875
6.156931	359.449499	7.754880
6.141146	362.308802	7.759885
6.118928	357.035214	7.764890
6.284479	366.396176	7.769894
6.061435	358.031275	7.774899
6.075020	355.928475	7.779904
6.128738	356.053003	7.784909
6.035869	334.383445	7.789914
5.916418	332.880318	7.794918
5.549806	332.038923	7.799923
5.929438	340.050440	7.804928
6.087122	347.362538	7.809933
6.192605	353.657724	7.814938
5.784579	350.152608	7.819942
6.143510	335.072307	7.824947
5.942762	336.967001	7.829952
5.725559	337.276078	7.834957
5.505827	339.857088	7.839962
5.862003	359.641249	7.844966
5.761580	354.579151	7.849971
5.924691	355.749653	7.854976
5.771818	358.313928	7.859981
5.763322	355.164215	7.864986
5.829917	358.029673	7.869990
5.657382	366.063898	7.874995
5.917014	367.886915	7.880000
5.831085	363.404680	7.885005
5.346980	366.789310	7.890010
5.346879	369.560751	7.895014
5.416586	377.987530	7.900019
6.003784	380.537820	7.905024
6.331360	385.744924	7.910029
6.086875	381.907458	7.915034
5.800605	390.506725	7.920038
5.857218	391.696974	7.925043
6.139553	384.537842	7.930048
5.725044	390.784291	7.935053
5.732342	386.259062	7.940058
5.687140	388.170671	7.945062
5.945132	390.917751	7.950067
6.145226	380.474836	7.955072
6.251915	379.430036	7.960077
6.585089	381.156184	7.965082
6.357634	374.326362	7.970086
5.936973	362.879136	7.975091
5.754307	359.250347	7.980096
5.729989	366.318710	7.985101
5.803071	358.353786	7.990106
5.709672	364.097820	7.995110
5.718926	380.943151	8.000115
5.857576	386.281513	8.005133
6.120324	388.878738	8.010150
6.179040	382.365835	8.015168
6.126555	380.051472	8.020186
5.906478	379.520894	8.025203
6.302393	368.613335	8.030221
6.025227	371.341954	8.035238
5.527208	361.204710	8.040256
5.922503	363.929609	8.045274
6.175915	372.804849	8.050291
6.026402	373.055350	8.055309
5.891001	385.045792	8.060326
6.023077	385.476502	8.065344
5.956986	386.222073	8.070362
6.318602	386.635978	8.075379
6.141214	379.588666	8.080397
5.771224	373.697907	8.085414
5.595614	369.294749	8.090432
6.092154	383.888026	8.095450
5.925493	389.796107	8.100467
6.245471	395.265524	8.105485
6.161884	388.260406	8.110502
6.297664	394.320205	8.115520
6.385525	386.152362	8.120538
5.780085	375.214524	8.125555
5.816665	372.580197	8.130573
5.965007	376.596336	8.135590
5.848018	376.554611	8.140608
6.150855	380.401537	8.145626
6.252715	383.986281	8.150643
6.466027	383.729035	8.155661
6.294126	376.393706	8.160678
6.230431	372.134060	8.165696
5.916303	365.224802	8.170714
5.736926	368.569323	8.175731
6.271612	375.687259	8.180749
6.235712	379.312385	8.185766
6.277906	378.703105	8.190784
6.196474	372.088957	8.195802
5.979437	359.708485	8.200819
5.951087	367.040306	8.205837
5.802452	381.563629	8.210854
6.178626	383.423706	8.215872
6.144284	377.947722	8.220890
5.994739	382.108067	8.225907
6.302998	368.699110	8.230925
6.187977	384.384787	8.235942
6.169110	384.289917	8.240960
6.010292	381.992109	8.245978
6.165458	390.100055	8.250995
6.599195	382.837677	8.256013
6.342953	396.932821	8.261030
6.484857	381.766816	8.266048
6.355435	383.509964	8.271066
6.079077	375.433546	8.276083
6.744873	374.657749	8.281101
6.383057	364.385693	8.286118
6.087043	360.783881	8.291136
6.251699	359.956730	8.296154
5.976189	359.586254	8.301171
6.369838	359.622806	8.306189
6.399390	372.114548	8.311206
5.999710	354.006632	8.316224
6.093240	359.719567	8.321242
6.306394	375.164802	8.326259
6.450799	372.308571	8.331277
6.397858	377.529947	8.336294
6.261182	376.042848	8.341312
6.516290	368.704152	8.346330
6.085977	376.811736	8.351347
6.517130	382.412154	8.356365
6.036504	366.551022	8.361382
5.994659	371.379370	8.366400
6.124467	373.994135	8.371418
6.080461	386.563608	8.376435
6.469333	386.323207	8.381453
6.233210	390.528591	8.386470
6.377774	383.936053	8.391488
6.351528	377.868703	8.396506
6.276618	376.378298	8.401523
6.334575	382.923557	8.406541
6.438865	381.862819	8.411558
6.607538	384.970125	8.416576
6.577307	375.760378	8.421594
6.466381	378.766057	8.426611
6.408069	384.256500	8.431629
6.609885	380.277388	8.436646
6.231394	384.975127	8.441664
6.497554	380.749323	8.446682
6.074755	383.235545	8.451699
6.187321	378.232123	8.456717
6.476988	387.474091	8.461734
6.246212	388.680782	8.466752
6.297143	386.410274	8.471770
6.067057	386.663853	8.476787
5.894261	385.608389	8.481805
6.344483	384.058312	8.486822
6.008132	393.811141	8.491840
6.266057	395.156327	8.496858
6.537943	404.697703	8.501875
6.526027	404.380855	8.506893
6.767863	412.686745	8.511910
6.385237	400.221580	8.516928
6.635853	398.446972	8.521946
6.418625	406.537171	8.526963
6.723162	400.787522	8.531981
6.807494	400.319996	8.536998
6.335080	390.686807	8.542016
6.341017	380.521578	8.547034
6.362641	396.902321	8.552051
6.888405	402.633175	8.557069
6.436947	401.097259	8.562087
6.215393	389.844035	8.567104
6.855925	396.853986	8.572122
6.536520	400.709440	8.577139
6.260429	391.244489	8.582157
6.457455	401.545406	8.587175
6.661684	403.637374	8.592192
7.065316	408.715093	8.597210
6.498146	406.506106	8.602227
6.432654	388.314567	8.607245
6.636246	392.751275	8.612263
6.580476	395.723123	8.617280
6.829135	385.040443	8.622298
6.174315	392.286786	8.627315
6.515747	398.876272	8.632333
6.933077	405.621193	8.637351
6.711374	400.647720	8.642368
6.687886	390.133634	8.647386
6.629730	396.595996	8.652403
6.238528	402.138275	8.657421
6.428410	408.347438	8.662439
6.805817	415.650816	8.667456
6.721196	409.002439	8.672474
6.687767	417.944451	8.677491
6.745020	414.357050	8.682509
6.485222	407.354114	8.687527
6.570312	414.561001	8.692544
6.785043	413.388396	8.697562
6.702768	417.437295	8.702579
6.726249	415.142656	8.707597
7.178316	411.402271	8.712615
6.636831	415.096654	8.717632
7.012836	411.099882	8.722650
6.619849	397.557100	8.727667
6.538226	398.377670	8.732685
6.762241	398.727797	8.737703
6.779048	414.910501	8.742720
6.777050	411.212411	8.747738
6.490665	416.990827	8.752755
6.637511	419.937445	8.757773
6.873268	419.458964	8.762791
6.931586	419.513014	8.767808
6.910635	406.489784	8.772826
6.611801	413.014869	8.777843
6.522849	415.884595	8.782861
6.771142	416.833671	8.787879
6.534286	412.032959	8.792896
6.922358	410.401043	8.797914
6.428705	420.377183	8.802931
6.569103	423.611969	8.807949
6.614151	417.079093	8.812967
6.290318	418.464368	8.817984
6.943392	411.290899	8.823002
6.559268	407.592348	8.828019
6.783430	413.417498	8.833037
6.781061	411.959975	8.838055
7.011475	411.479171	8.843072
6.805055	405.859565	8.848090
6.648047	406.994815	8.853107
6.637749	418.186356	8.858125
7.125603	425.794419	8.863143
6.848089	429.217344	8.868160
7.140657	418.982220	8.873178
7.130214	421.274863	8.878195
7.055182	415.540128	8.883213
7.140195	413.709255	8.888231
6.703944	407.191362	8.893248
6.776938	414.011987	8.898266
6.707709	420.820047	8.903283
6.857797	411.086769	8.908301
7.107095	403.187259	8.913319
6.721678	412.758399	8.918336
7.095431	412.409904	8.923354
7.009125	414.903697	8.928371
6.834981	404.144829	8.933389
7.114598	417.888328	8.938407
6.824712	424.042813	8.943424
6.906369	418.880099	8.948442
6.848542	428.103612	8.953459
7.181826	431.327302	8.958477
7.402611	423.820366	8.963495
6.634631	428.064387	8.968512
7.105329	424.889115	8.973530
7.170173	427.706497	8.978547
6.895828	421.157079	8.983565
7.086231	419.701098	8.988583
6.982563	430.844072	8.993600
7.023228	428.376351	8.998618
7.128479	433.730896	9.003635
7.039409	445.597406	9.008653
7.245447	426.123381	9.013671
7.076942	425.243962	9.018688
7.111843	418.062601	9.023706
7.084246	412.560311	9.028723
6.887452	415.901241	9.033741
7.204687	418.950711	9.038759
7.089239	418.176635	9.043776
7.326665	411.367667	9.048794
7.194771	415.916572	9.053811
6.957070	414.514623	9.058829
7.030446	412.448889	9.063847
7.140190	412.876765	9.068864
7.009116	411.726445	9.073882
7.167814	429.654233	9.078899
7.298469	432.499237	9.083917
7.431692	415.889268	9.088935
7.001092	412.601875	9.093952
6.894608	408.645513	9.098970
7.238949	414.761205	9.103987
6.974436	425.948153	9.109005
7.520566	433.910045	9.114023
7.353773	434.737566	9.119040
7.176421	423.556330	9.124058
7.252603	419.511567	9.129075
7.128416	419.546697	9.134093
7.445506	405.577788	9.139111
6.980461	416.038598	9.144128
7.087229	409.167927	9.149146
7.623838	416.509631	9.154163
7.148246	423.699682	9.159181
7.418556	411.391611	9.164199
7.215303	410.978328	9.169216
7.425694	416.991806	9.174234
7.462313	418.769062	9.179251
7.591091	420.882246	9.184269
7.552421	410.812303	9.189287
7.450293	411.607665	9.194304
7.587158	409.942281	9.199322
7.185269	413.772712	9.204339
7.255535	416.860634	9.209357
7.412397	410.890989	9.214375
7.239107	418.513628	9.219392
7.310975	418.183735	9.224410
7.225159	414.779547	9.229427
7.299513	416.743422	9.234445
7.148756	415.634034	9.239463
6.899042	411.756773	9.244480
6.925232	421.140761	9.249498
7.227114	416.855742	9.254515
7.007776	422.327089	9.259533
7.447544	438.055817	9.264551
7.417118	433.295538	9.269568
7.423906	435.964178	9.274586
7.855577	429.847604	9.279603
7.395292	426.085172	9.284621
7.253138	419.950652	9.289639
7.301819	426.027179	9.294656
7.711780	424.432877	9.299674
7.254796	426.466858	9.304691
7.291893	436.477130	9.309709
7.717319	438.575686	9.314727
7.462448	433.042507	9.319744
7.503785	432.651098	9.324762
7.068363	423.403432	9.329779
7.289435	434.770390	9.334797
7.503335	434.620344	9.339815
7.597730	436.252913	9.344832
7.749815	444.541236	9.349850
7.408521	431.902363	9.354867
7.337491	444.450840	9.359885
7.492731	439.800501	9.364903
7.213999	434.330993	9.369920
7.171691	440.513206	9.374938
7.355302	438.963611	9.379955
7.624063	438.303275	9.384973
7.583983	438.318999	9.389991
7.745951	439.448766	9.395008
7.701263	447.183932	9.400026
7.640982	435.028298	9.405043
7.785389	442.642506	9.410061
7.768510	436.220245	9.415079
8.128772	442.983532	9.420096
7.414962	439.115410	9.425114
7.618503	432.542073	9.430131
7.600362	429.714296	9.435149
7.588847	423.464766	9.440167
7.428941	428.683877	9.445184
7.374820	435.196114	9.450202
7.873910	428.456848	9.455219
7.505577	439.975534	9.460237
7.602617	437.388586	9.465255
7.555632	445.016817	9.470272
7.660283	439.601219	9.475290
7.866724	437.915533	9.480307
7.490174	445.137506	9.485325
7.443269	434.652285	9.490343
7.567056	442.686250	9.495360
7.696549	440.804271	9.500378
7.673243	440.826850	9.505395
7.314938	441.908240	9.510413
7.651760	438.270995	9.515431
7.678184	435.433123	9.520448
7.368792	431.442079	9.525466
7.579352	437.973065	9.530483
7.717278	436.108707	9.535501
7.729382	436.264622	9.540519
7.992660	434.601642	9.545536
7.839087	438.696359	9.550554
7.713727	437.014998	9.555571
7.705346	424.068690	9.560589
7.551098	439.984575	9.565607
7.731103	433.679976	9.570624
7.518065	435.098492	9.575642
7.893838	428.788660	9.580659
7.395097	441.668803	9.585677
7.531776	445.077733	9.590695
8.176554	453.008496	9.595712
7.667078	466.414166	9.600730
8.028512	461.214190	9.605747
7.412502	470.335293	9.610765
7.779221	465.251253	9.615783
7.811777	465.536521	9.620800
7.376128	478.968573	9.625818
7.939462	467.485803	9.630835
7.677447	468.760476	9.635853
7.663046	464.221746	9.640871
7.527968	464.025054	9.645888
7.685631	466.925816	9.650906
7.729817	467.887739	9.655923
7.573034	473.059043	9.660941
7.996827	466.028542	9.665959
7.927280	469.198199	9.670976
7.865122	484.089975	9.675994
8.020223	478.224719	9.681011
8.205669	480.486870	9.686029
8.003375	473.664295	9.691047
7.949891	476.124585	9.696064
7.622652	465.298003	9.701082
8.059693	473.873317	9.706099
7.868390	487.601832	9.711117
8.206156	488.489646	9.716135
8.104355	474.099932	9.721152
7.654766	472.238686	9.726170
8.044740	476.425499	9.731187
7.926032	488.369233	9.736205
8.124397	487.874483	9.741223
8.159618	486.035577	9.746240
8.169640	479.243056	9.751258
7.986591	473.042305	9.756275
7.880467	472.427713	9.761293
7.781985	478.754378	9.766311
8.170946	483.686087	9.771328
8.220011	488.995750	9.776346
8.253193	484.395960	9.781363
8.130446	484.541314	9.786381
7.899081	477.303561	9.791399
7.923484	470.814903	9.796416
7.772169	480.864003	9.801434
8.194844	486.756094	9.806451
8.181537	488.152985	9.811469
7.997690	492.097800	9.816487
8.005350	491.951463	9.821504
8.066507	492.525755	9.826522
8.786363	493.496084	9.831539
8.402808	479.888658	9.836557
8.404021	484.303252	9.841575
8.263467	478.386203	9.846592
7.811011	468.368030	9.851610
8.138232	475.385771	9.856627
8.310701	479.451823	9.861645
8.516577	486.804027	9.866663
8.115456	476.698965	9.871680
7.986078	471.512291	9.876698
8.244232	482.450647	9.881715
8.417484	493.285470	9.886733
8.027667	479.808401	9.891751
7.982274	485.748123	9.896768
8.062059	493.091561	9.901786
8.427512	496.954009	9.906803
8.570753	486.811520	9.911821
8.422854	495.370625	9.916839
8.376396	496.387687	9.921856
7.926294	494.056325	9.926874
7.998742	488.932892	9.931891
8.072307	496.536064	9.936909
8.164903	495.997824	9.941927
8.552051	494.937218	9.946944
8.150293	495.511004	9.951962
8.410023	488.335634	9.956979
8.155104	486.103266	9.961997
8.219759	493.786715	9.967015
8.459311	495.765901	9.972032
8.034698	494.604477	9.977050
8.508644	495.411131	9.982067
8.787777	498.160448	9.987085
8.442500	494.979670	9.992103
8.578585	494.661867	9.997120
8.323591	505.402435	10.002138
8.401433	495.901256	10.007155
8.023858	496.837334	10.012173
8.228942	495.300169	10.017191
8.741561	492.497037	10.022208
8.632169	501.195310	10.027226
8.608372	485.528021	10.032243
8.641444	492.048793	10.037261
8.435555	496.050687	10.042279
8.769435	493.385833	10.047296
8.493247	496.931635	10.052314
8.879341	491.570028	10.057331
8.912875	489.472621	10.062349
8.344318	471.431902	10.067367
8.386567	461.308308	10.072384
8.206664	473.608681	10.077402
8.584165	484.149778	10.082419
8.628575	479.321034	10.087437
8.606863	493.679526	10.092455
8.681753	490.297637	10.097472
8.388714	489.074704	10.102490
8.694145	489.238595	10.107507
8.400487	491.603743	10.112525
8.771152	489.744167	10.117543
8.868721	481.398052	10.122560
8.284318	471.753854	10.127578
8.307464	478.465506	10.132595
8.313976	485.530028	10.137613
8.549123	486.702051	10.142631
8.746380	486.500950	10.147648
8.607328	499.378778	10.152666
8.443715	495.339776	10.157683
8.630965	491.217747	10.162701
8.487638	498.539123	10.167719
8.147281	491.504517	10.172736
8.466098	498.021826	10.177754
8.735656	487.007642	10.182771
8.820816	495.356899	10.187789
8.390023	496.294951	10.192807
8.258405	491.099153	10.197824
8.180256	502.922977	10.202842
8.380018	513.741062	10.207859
8.360774	523.378321	10.212877
8.646472	526.246535	10.217895
8.756781	525.759183	10.222912
8.989816	527.310217	10.227930
8.721571	527.576051	10.232947
9.142927	523.288182	10.237965
9.000806	526.488083	10.242983
8.893176	520.761545	10.248000
8.727005	517.350914	10.253018
9.022949	523.452090	10.258035
9.249809	510.850928	10.263053
8.621864	501.090422	10.268071
8.897716	496.509648	10.273088
8.599999	498.017090	10.278106
8.481346	501.942289	10.283123
8.975725	515.529355	10.288141
8.713920	527.495395	10.293159
9.010783	524.703761	10.298176
8.852541	535.782717	10.303194
9.055298	535.482934	10.308211
9.114866	536.458244	10.313229
8.696622	522.982413	10.318247
9.306603	500.065696	10.323264
8.715952	502.489710	10.328282
8.575014	506.528828	10.333299
8.655528	512.202815	10.338317
8.564714	519.863146	10.343335
8.660978	523.316252	10.348352
8.826621	520.090633	10.353370
8.563275	523.811158	10.358387
8.741568	530.763750	10.363405
8.706440	521.302237	10.368423
9.064563	523.155673	10.373440
8.716236	524.579482	10.378458
8.734630	519.849447	10.383475
9.084307	519.144953	10.388493
8.989665	527.623201	10.393511
9.262517	526.905423	10.398528
9.005808	520.343755	10.403546
8.873481	534.517540	10.408563
9.070793	523.735478	10.413581
8.850474	533.299912	10.418599
9.296703	526.499414	10.423616
8.950422	521.049864	10.428634
8.981172	520.246710	10.433651
9.092453	529.358743	10.438669
8.968212	543.389270	10.443687
9.150855	536.513049	10.448704
9.061326	550.793787	10.453722
9.249842	542.856343	10.458739
9.304702	538.713892	10.463757
9.052199	520.320971	10.468775
8.968242	523.028998	10.473792
9.080744	540.383448	10.478810
9.075410	550.624443	10.483827
9.555283	549.842875	10.488845
9.168102	538.568009	10.493863
9.286371	526.864175	10.498880
9.331762	528.409712	10.503898
8.668606	526.452330	10.508915
9.354183	525.884877	10.513933
9.553174	538.675389	10.518951
9.112581	533.347811	10.523968
8.971911	541.340948	10.528986
9.227733	541.130728	10.534003
9.577521	545.762454	10.539021
8.968400	545.371335	10.544039
9.550935	536.955998	10.549056
9.091236	535.648561	10.554074
9.061367	547.726819	10.559091
9.158181	545.165136	10.564109
9.209207	550.827948	10.569127
9.107330	545.564390	10.574144
9.207657	547.943939	10.579162
9.482666	545.906755	10.584179
9.217751	538.229251	10.589197
9.293716	547.659203	10.594215
9.184654	548.001234	10.599232
9.253279	538.343684	10.604250
8.981877	547.275478	10.609267
9.488470	536.009773	10.614285
9.320790	542.239941	10.619303
9.347506	536.255806	10.624320
9.485186	538.945106	10.629338
9.150488	541.319806	10.634355
9.446326	544.214846	10.639373
9.047155	545.807512	10.644391
9.057039	545.061251	10.649408
9.437517	552.430477	10.654426
9.442542	550.075581	10.659443
9.393289	551.339223	10.664461
9.590592	560.450501	10.669479
9.291012	556.278028	10.674496
9.419743	558.059890	10.679514
9.155499	571.055088	10.684531
9.578553	562.090237	10.689549
9.194473	568.764345	10.694567
9.582254	566.655953	10.699584
9.534862	566.335158	10.704602
9.361112	568.463906	10.709619
9.626288	559.804492	10.714637
9.712140	571.473445	10.719655
9.724433	568.259071	10.724672
9.610051	563.426627	10.729690
9.491253	574.265946	10.734707
9.653042	567.635946	10.739725
9.615240	574.634823	10.744743
9.439327	567.410489	10.749760
9.671623	570.012481	10.754778
9.373163	580.270732	10.759795
9.699653	566.316012	10.764813
9.648528	562.559271	10.769831
9.813894	573.994948	10.774848
9.640424	568.082994	10.779866
9.745568	573.866770	10.784883
9.662813	560.919319	10.789901
9.645719	565.614483	10.794919
9.658246	572.832731	10.799936
9.983889	563.778909	10.804954
9.679583	572.690593	10.809971
9.720021	563.838960	10.814989
9.722850	573.356049	10.820007
9.548462	565.430918	10.825024
9.834456	564.720560	10.830042
9.782004	557.420205	10.835059
10.012858	564.402494	10.840077
9.810311	565.992950	10.845095
9.579834	571.507101	10.850112
9.681840	567.966347	10.855130
9.383897	574.838477	10.860147
9.554235	567.351958	10.865165
9.491569	570.649944	10.870183
9.879067	567.613828	10.875200
9.796508	570.731882	10.880218
9.336416	565.079141	10.885235
9.716764	565.228213	10.890253
9.612648	569.570869	10.895271
10.162874	589.444867	10.900288
9.978937	579.460560	10.905306
9.702000	578.301382	10.910323
9.776242	566.812651	10.915341
9.631242	582.610463	10.920359
9.641299	601.606096	10.925376
9.864010	598.160148	10.930394
10.292853	598.352161	10.935411
10.313174	601.094455	10.940429
10.206758	588.665044	10.945447
10.285144	579.788560	10.950464
10.095638	571.752176	10.955482
9.696752	575.336031	10.960499
9.707996	572.724554	10.965517
9.964041	565.016417	10.970535
10.029343	572.690333	10.975552
9.797226	579.561682	10.980570
10.095277	594.488982	10.985587
10.165227	592.439539	10.990605
10.014411	586.741794	10.995623
10.162575	590.477154	11.000640
10.149841	574.271599	11.005658
9.853351	580.158934	11.010675
10.010229	582.068954	11.015693
9.893202	591.074560	11.020711
10.216945	598.645135	11.025728
10.498710	593.997147	11.030746
10.089604	588.740386	11.035763
10.164178	579.580485	11.040781
10.015812	575.179345	11.045799
10.029115	585.976014	11.050816
10.326550	598.716529	11.055834
9.794664	602.216960	11.060851
10.311256	595.108847	11.065869
10.240564	590.522047	11.070887
10.158425	598.569210	11.075904
10.230665	591.940521	11.080922
9.975757	596.947264	11.085939
10.328847	593.055000	11.090957
10.745205	594.710036	11.095975
10.239324	585.523747	11.100992
10.301342	569.417007	11.106010
9.852924	569.906545	11.111027
10.393277	585.376755	11.116045
10.410623	582.316221	11.121063
10.053755	579.231903	11.126080
10.149336	589.608681	11.131098
10.218524	586.732571	11.136115
10.193725	589.311481	11.141133
10.459446	593.028538	11.146151
10.117272	590.263810	11.151168
10.358229	592.854990	11.156186
10.145266	593.904293	11.161203
10.085406	599.710612	11.166221
10.276512	597.708574	11.171239
9.989913	597.279862	11.176256
10.204228	589.467763	11.181274
10.036426	600.002316	11.186291
10.086966	589.754286	11.191309
10.502358	594.407367	11.196327
10.258264	599.156817	11.201344
10.351379	603.781185	11.206362
10.321840	609.428158	11.211379
10.472092	612.623576	11.216397
10.942209	615.759726	11.221415
10.458666	611.051015	11.226432
10.669720	598.221887	11.231450
10.089875	595.907556	11.236467
10.116105	604.357554	11.241485
10.739485	609.366404	11.246503
10.659797	621.487181	11.251520
10.713268	609.865962	11.256538
10.590671	611.204141	11.261555
10.303021	592.359044	11.266573
10.483225	608.955124	11.271591
10.503346	609.961826	11.276608
10.976009	613.990637	11.281626
10.490955	611.450115	11.286643
10.435514	607.990669	11.291661
11.048178	609.640388	11.296679
10.670467	611.693604	11.301696
10.406512	599.528545	11.306714
10.182679	604.148614	11.311731
10.260903	610.984279	11.316749
10.514297	616.915394	11.321767
10.614170	623.839208	11.326784
10.701562	618.751279	11.331802
10.677178	618.789805	11.336819
10.429139	606.852628	11.341837
10.761149	614.986789	11.346855
10.562789	627.009287	11.351872
10.719291	617.489485	11.356890
10.419731	627.593305	11.361907
10.539650	614.513278	11.366925
10.578882	611.067493	11.371943
10.160035	621.016320	11.376960
10.980191	628.074134	11.381978
10.886613	628.009828	11.386995
10.607443	629.817338	11.392013
10.827947	619.246194	11.397031
10.975632	632.918886	11.402048
11.050689	626.854613	11.407066
10.824915	613.342435	11.412083
10.661494	621.525335	11.417101
11.042630	611.127995	11.422119
10.824286	620.584874	11.427136
10.943814	609.571884	11.432154
10.697028	620.345955	11.437171
10.707455	614.667275	11.442189
11.098404	620.548573	11.447207
10.673041	622.583963	11.452224
10.892344	627.024595	11.457242
11.081364	639.668415	11.462259
11.154974	630.514949	11.467277
11.068063	620.749033	11.472295
11.077476	611.113285	11.477312
10.801070	611.452971	11.482330
11.086356	610.452399	11.487347
10.850903	616.513271	11.492365
11.371820	612.301395	11.497383
11.175386	624.743297	11.502400
11.185711	614.993801	11.507418
11.351732	613.794055	11.512435
11.210450	619.802398	11.517453
11.039982	617.285476	11.522471
10.648580	622.569088	11.527488
10.744310	614.696549	11.532506
11.187574	619.818649	11.537523
11.295194	613.812424	11.542541
11.296069	615.270230	11.547559
10.948594	617.971965	11.552576
10.850566	616.122236	11.557594
10.983698	618.935327	11.562611
11.049955	618.502167	11.567629
11.249413	622.453601	11.572647
10.947952	626.738637	11.577664
11.249593	623.375065	11.582682
11.060681	617.995654	11.587699
11.268839	620.790753	11.592717
11.419404	613.528191	11.597735
11.187823	615.050591	11.602752
10.838592	616.351476	11.607770
11.232670	616.403741	11.612787
10.848372	639.534800	11.617805
11.491012	635.095692	11.622823
11.232000	640.185134	11.627840
11.444827	638.343806	11.632858
11.645781	639.303420	11.637875
11.151852	640.617369	11.642893
11.395651	629.408299	11.647911
11.333372	636.631909	11.652928
11.683559	629.574937	11.657946
11.332516	627.016703	11.662963
11.075296	619.760828	11.667981
11.198973	621.821183	11.672999
11.693310	636.575952	11.678016
11.630252	629.756883	11.683034
11.527789	624.594375	11.688051
11.227368	621.242495	11.693069
11.222332	609.087607	11.698087
11.295693	623.298863	11.703104
11.505835	634.948506	11.708122
11.714073	625.187124	11.713139
11.229592	625.344621	11.718157
11.464308	625.248135	11.723175
11.237344	632.282797	11.728192
11.496649	633.873931	11.733210
11.574379	633.577833	11.738227
11.619708	645.505599	11.743245
11.932889	632.957180	11.748263
11.344156	625.970659	11.753280
11.407825	623.874856	11.758298
11.611676	635.497078	11.763315
11.462450	647.988448	11.768333
11.805956	636.555574	11.773351
11.621995	629.607012	11.778368
11.102370	626.317662	11.783386
11.499889	630.389733	11.788403
11.511090	641.114182	11.793421
11.442122	626.880172	11.798439
11.609754	640.199483	11.803456
11.578585	643.763967	11.808474
11.760647	647.244762	11.813491
11.785838	641.743649	11.818509
11.686345	632.778074	11.823527
11.464343	637.154879	11.828544
11.401675	648.575618	11.833562
11.870911	637.448204	11.838579
11.852911	635.191552	11.843597
12.035584	635.100013	11.848615
12.109602	643.511033	11.853632
11.582819	639.787309	11.858650
11.606509	639.212458	11.863667
11.498206	638.677092	11.868685
12.029434	633.510589	11.873703
11.778007	639.671782	11.878720
11.699668	638.409099	11.883738
11.577792	643.003837	11.888755
11.360267	640.563663	11.893773
11.652205	634.595003	11.898791
11.800439	644.607023	11.903808
11.532156	643.231907	11.908826
11.509214	641.670275	11.913843
11.734661	639.808048	11.918861
12.061296	646.302104	11.923879
11.574918	654.525835	11.928896
11.808621	659.876228	11.933914
12.338918	659.777900	11.938931
12.073451	669.440951	11.943949
11.960249	665.236278	11.948967
12.216591	657.155684	11.953984
11.931253	652.700114	11.959002
11.799140	645.926503	11.964019
11.681559	657.106497	11.969037
11.707355	658.304815	11.974055
11.932806	659.642455	11.979072
11.912366	668.677242	11.984090
11.765660	655.395709	11.989107
11.822726	670.994887	11.994125
12.049552	669.154532	11.999143
11.697899	670.380061	12.004160
11.389136	673.025286	12.009178
11.946586	664.784202	12.014195
11.620798	675.403355	12.019213
12.296253	679.072415	12.024231
12.301298	685.654424	12.029248
12.457698	688.523862	12.034266
12.240742	676.395613	12.039283
12.030978	680.445487	12.044301
12.074318	678.400178	12.049319
12.056355	679.703137	12.054336
12.404207	689.715660	12.059354
12.786397	675.080020	12.064371
12.430388	671.976617	12.069389
11.909928	662.445431	12.074407
12.113871	664.054654	12.079424
12.224096	661.175298	12.084442
12.354783	662.467734	12.089459
12.196116	667.765614	12.094477
12.192827	667.078203	12.099495
12.494161	669.675772	12.104512
12.524722	670.321103	12.109530
12.268277	664.289497	12.114547
11.939579	658.928682	12.119565
12.308771	669.859332	12.124583
12.729421	667.212499	12.129600
12.484070	665.496152	12.134618
12.530603	655.996607	12.139635
12.342990	665.754828	12.144653
12.194431	655.537760	12.149671
12.282973	654.561505	12.154688
12.023700	663.163277	12.159706
12.529920	667.622361	12.164723
12.450705	684.138985	12.169741
12.593020	692.097597	12.174759
12.924617	683.115368	12.179776
12.430907	679.922955	12.184794
12.149380	664.213588	12.189811
12.403021	668.800357	12.194829
12.538510	683.358581	12.199847
12.507325	685.884852	12.204864
12.587208	686.626643	12.209882
12.777981	683.801011	12.214899
12.806983	683.503033	12.219917
12.343244	672.732290	12.224935
12.926290	664.812257	12.229952
12.569434	670.241977	12.234970
12.672437	660.863021	12.239987
12.346691	664.129404	12.245005
12.666429	675.657872	12.250023
12.721773	676.747453	12.255040
12.518515	675.478971	12.260058
12.735970	675.284190	12.265075
12.479678	682.623230	12.270093
12.517411	682.816180	12.275111
13.037737	686.635623	12.280128
12.521957	690.610072	12.285146
12.332681	688.733519	12.290163
12.644758	695.920957	12.295181
12.724087	686.015516	12.300199
12.903590	681.790511	12.305216
12.892685	692.701463	12.310234
12.877915	681.633602	12.315251
12.819391	690.538634	12.320269
12.967874	690.222053	12.325287
12.670135	690.691289	12.330304
12.892996	697.425576	12.335322
12.798280	686.382781	12.340339
12.873753	689.318466	12.345357
12.649847	687.456772	12.350375
13.026835	680.660685	12.355392
12.740529	694.596648	12.360410
13.110862	688.076140	12.365427
12.880405	694.183597	12.370445
12.709124	692.436780	12.375463
13.143287	693.113943	12.380480
12.969039	690.887923	12.385498
13.088743	689.998330	12.390515
12.994749	688.198457	12.395533
12.645779	681.490153	12.400551
13.059562	687.020792	12.405568
13.031598	691.013961	12.410586
12.817944	682.324902	12.415603
13.287315	685.682079	12.420621
12.982418	693.628273	12.425639
12.895460	686.519424	12.430656
12.573539	690.899177	12.435674
12.877168	683.991438	12.440691
12.949461	684.096960	12.445709
12.953230	684.894780	12.450727
13.107040	683.542302	12.455744
12.854617	688.914744	12.460762
13.160344	699.400875	12.465779
13.179713	704.475393	12.470797
13.306448	714.743256	12.475815
13.364325	702.859367	12.480832
12.806579	698.007556	12.485850
13.049651	701.933283	12.490867
13.235697	714.760650	12.495885
13.137644	717.445655	12.500903
13.430107	711.287546	12.505920
13.374144	712.290321	12.510938
13.379534	707.922011	12.515955
13.188513	710.602556	12.520973
12.964016	717.614778	12.525991
13.342774	712.197445	12.531008
13.233287	712.744666	12.536026
13.470499	711.934603	12.541043
13.555770	711.091395	12.546061
13.681408	717.140261	12.551079
13.783085	708.705040	12.556096
13.376250	688.631897	12.561114
13.076341	700.067516	12.566131
13.131364	700.731129	12.571149
13.186747	708.154192	12.576167
13.303535	704.974015	12.581184
13.359568	713.236395	12.586202
13.656463	706.976614	12.591219
13.671787	710.098387	12.596237
13.405296	718.171151	12.601255
13.572893	711.685356	12.606272
13.187983	722.354766	12.611290
13.313000	707.632912	12.616307
13.268511	712.616393	12.621325
13.155965	716.291389	12.626343
13.332048	712.710672	12.631360
13.357230	719.198043	12.636378
13.224864	716.987588	12.641395
13.215501	723.530830	12.646413
13.498310	730.268418	12.651431
13.380890	734.714168	12.656448
13.972037	736.244177	12.661466
13.618507	743.355392	12.666483
13.804997	739.905589	12.671501
13.843785	743.332973	12.676519
14.162614	731.676670	12.681536
13.771640	716.214665	12.686554
13.522179	715.448818	12.691571
13.344408	720.266866	12.696589
13.694689	742.737752	12.701607
13.898492	727.318827	12.706624
13.530723	735.334787	12.711642
13.300379	739.293207	12.716659
13.676967	739.285082	12.721677
13.447522	735.887416	12.726695
13.502908	733.903339	12.731712
13.503042	738.122511	12.736730
13.687061	730.640105	12.741747
13.874493	731.292571	12.746765
13.503964	744.187681	12.751783
14.203597	747.389102	12.756800
14.134821	744.095804	12.761818
14.026696	737.858049	12.766835
13.830505	737.412100	12.771853
13.904786	734.610910	12.776871
13.524234	735.067796	12.781888
14.143073	744.050422	12.786906
14.173769	747.845129	12.791923
13.863343	741.840835	12.796941
13.870869	736.405558	12.801959
13.958298	748.131184	12.806976
14.047831	757.571757	12.811994
14.272554	751.392624	12.817011
14.391990	734.156520	12.822029
14.119973	740.242061	12.827047
14.176363	740.523623	12.832064
13.993646	731.937017	12.837082
13.884913	732.471498	12.842099
14.173425	727.377470	12.847117
14.027373	729.883764	12.852135
14.086377	730.281680	12.857152
14.327660	735.009241	12.862170
14.214417	735.588605	12.867187
14.432601	738.000322	12.872205
14.013229	734.663784	12.877223
14.262222	726.966143	12.882240
14.283255	729.140320	12.887258
14.063535	729.161923	12.892275
14.008073	729.590283	12.897293
13.823701	743.548282	12.902311
14.138831	751.473703	12.907328
14.319919	755.197660	12.912346
14.439896	752.480867	12.917363
14.266174	751.977773	12.922381
14.274307	763.068835	12.927399
14.122166	757.876154	12.932416
14.094378	759.594047	12.937434
14.130805	757.483535	12.942451
14.330606	756.054465	12.947469
14.131155	758.922516	12.952487
14.351655	759.266887	12.957504
14.327907	770.214599	12.962522
14.056064	771.465577	12.967539
14.300804	754.105806	12.972557
14.596912	757.972796	12.977575
14.293221	756.022534	12.982592
14.590329	770.284274	12.987610
14.290753	771.217688	12.992627
14.453668	767.900934	12.997645
14.394515	784.045310	13.002663
14.321393	776.621855	13.007680
14.425179	782.989717	13.012698
14.519356	784.852719	13.017715
14.492291	778.283602	13.022733
14.457956	789.674774	13.027751
14.870642	788.433456	13.032768
14.805254	788.408940	13.037786
14.221434	791.668192	13.042803
14.798767	784.285467	13.047821
14.673451	787.208251	13.052839
14.730023	780.929059	13.057856
15.036678	784.220074	13.062874
14.527948	786.479896	13.067891
14.926840	777.559723	13.072909
14.836787	788.609286	13.077927
14.826522	778.790324	13.082944
14.896218	779.388542	13.087962
14.484637	784.833129	13.092979
14.476377	779.980947	13.097997
14.566872	788.995366	13.103015
14.716241	783.061477	13.108032
15.118880	780.755093	13.113050
14.863569	792.966445	13.118067
14.972934	782.194765	13.123085
14.424852	788.140274	13.128103
14.189956	785.169468	13.133120
14.774260	782.011159	13.138138
14.430203	789.834108	13.143155
14.640884	792.505769	13.148173
14.985243	811.651542	13.153191
14.915954	809.383919	13.158208
14.862770	809.316479	13.163226
14.918605	816.477592	13.168243
15.416183	798.481981	13.173261
15.412465	816.391266	13.178279
15.311592	811.250546	13.183296
15.025611	805.507505	13.188314
15.107098	806.463640	13.193331
15.097240	789.203432	13.198349
14.968555	792.880957	13.203367
15.093511	797.304763	13.208384
15.152145	809.555606	13.213402
15.709034	817.418169	13.218419
15.290659	788.573816	13.223437
15.048733	784.913004	13.228455
14.844538	780.810830	13.233472
14.952880	783.198631	13.238490
15.031657	803.250410	13.243507
15.506486	799.550581	13.248525
15.149949	812.453029	13.253543
15.072049	814.371228	13.258560
15.210340	810.291461	13.263578
14.944000	816.562332	13.268595
15.049523	804.923414	13.273613
15.304601	811.772645	13.278631
15.195754	810.397937	13.283648
15.126868	811.598385	13.288666
15.007489	815.684708	13.293683
15.000972	811.621175	13.298701
15.165338	820.576773	13.303719
15.676090	819.408545	13.308736
15.436196	800.783003	13.313754
15.239784	811.678731	13.318771
15.483961	811.476633	13.323789
15.377755	813.582270	13.328807
15.543563	799.778615	13.333824
15.439400	808.056513	13.338842
15.285818	815.360681	13.343859
15.523583	805.114934	13.348877
15.663022	813.702036	13.353895
15.335125	814.848139	13.358912
15.488994	817.228856	13.363930
15.675819	825.937970	13.368947
15.690844	830.300008	13.373965
15.797840	827.257030	13.378983
15.579963	816.107102	13.384000
15.623349	807.772426	13.389018
15.362624	810.934041	13.394035
15.501028	816.674848	13.399053
15.989080	833.122224	13.404071
15.429170	836.428252	13.409088
16.102156	836.086808	13.414106
15.750566	845.293160	13.419123
15.724701	816.662197	13.424141
15.766940	816.819734	13.429159
15.650328	812.593467	13.434176
15.789651	815.853737	13.439194
16.056438	829.637421	13.444211
15.669563	821.786284	13.449229
15.882027	823.031287	13.454247
15.570487	839.552670	13.459264
16.127063	836.288218	13.464282
15.743655	836.890714	13.469299
15.960497	829.166478	13.474317
15.999198	833.408069	13.479335
15.536839	833.969210	13.484352
15.824912	830.184846	13.489370
15.905970	828.578603	13.494387
16.067292	842.129415	13.499405
16.102287	832.839851	13.504423
15.771005	836.053479	13.509440
16.223956	835.929326	13.514458
16.144151	835.244353	13.519475
15.976164	833.743156	13.524493
16.089934	832.968086	13.529511
15.853755	839.827544	13.534528
15.830441	830.458699	13.539546
16.197690	842.513195	13.544563
16.271165	831.920638	13.549581
16.329726	840.258420	13.554599
16.047651	840.807270	13.559616
16.076440	837.517698	13.564634
16.055079	843.264455	13.569651
15.892088	842.242148	13.574669
16.113008	840.254377	13.579687
15.963836	833.824168	13.584704
16.005354	834.142760	13.589722
16.162518	830.574432	13.594739
16.064477	826.821784	13.599757
16.243329	830.318893	13.604775
15.834010	834.652330	13.609792
16.020986	832.802384	13.614810
16.082456	839.807998	13.619827
16.202928	855.552096	13.624845
16.327426	854.481873	13.629863
15.956785	860.753220	13.634880
16.313383	862.262955	13.639898
16.394691	864.645509	13.644915
16.089326	859.198951	13.649933
16.376302	863.168370	13.654951
16.127322	869.338729	13.659968
16.074365	864.969997	13.664986
16.166330	866.129626	13.670003
15.987264	871.396029	13.675021
16.190301	877.603308	13.680039
16.153359	890.575971	13.685056
16.487094	887.800630	13.690074
16.545226	895.071868	13.695091
16.606439	886.778560	13.700109
16.707625	878.258131	13.705127
16.489960	888.481889	13.710144
16.452085	883.015766	13.715162
16.989747	879.968841	13.720179
16.732437	881.640432	13.725197
16.789867	881.552614	13.730215
16.858692	887.102311	13.735232
16.926717	886.984441	13.740250
16.634864	887.209775	13.745267
16.600050	883.103296	13.750285
16.622868	882.563286	13.755303
16.521368	884.873321	13.760320
16.703768	881.701832	13.765338
17.096966	882.255997	13.770355
16.612503	882.990990	13.775373
17.144980	877.918894	13.780391
16.702087	881.004744	13.785408
17.305273	876.858891	13.790426
17.560793	876.847526	13.795443
16.850491	866.960789	13.800461
16.767440	857.591763	13.805479
17.037351	869.831842	13.810496
16.628086	877.901661	13.815514
17.032103	874.771406	13.820531
16.702673	873.850750	13.825549
17.255689	874.935439	13.830567
16.701188	890.286053	13.835584
17.173576	880.789511	13.840602
17.016254	882.319305	13.845619
17.383294	882.186437	13.850637
17.146846	875.902343	13.855655
16.671662	883.512225	13.860672
16.846865	883.835249	13.865690
17.169022	884.769695	13.870707
16.911371	883.916755	13.875725
17.113355	875.775100	13.880743
17.154948	880.858831	13.885760
17.212859	882.588638	13.890778
17.234638	880.281582	13.895795
16.906417	888.269362	13.900813
17.244629	881.031123	13.905831
17.210129	881.210076	13.910848
17.090324	874.604872	13.915866
17.035248	871.053802	13.920883
17.107648	886.549798	13.925901
17.188333	875.432241	13.930919
16.951733	879.069782	13.935936
17.296794	876.942760	13.940954
17.511280	874.788733	13.945971
17.283991	877.115196	13.950989
17.460809	881.903326	13.956007
17.056072	884.976924	13.961024
17.400380	898.035397	13.966042
17.512345	906.001985	13.971059
17.234161	900.475445	13.976077
17.574450	912.808735	13.981095
17.885864	911.081415	13.986112
17.294971	902.179590	13.991130
17.568872	900.028932	13.996147
17.511275	908.785609	14.001165
17.682526	902.053029	14.006183
17.429068	900.293740	14.011200
17.309532	895.714466	14.016218
17.372946	910.375613	14.021235
17.365043	912.289236	14.026253
17.742286	900.942457	14.031271
17.555574	915.513167	14.036288
17.691567	910.262957	14.041306
17.415293	902.839522	14.046323
17.787481	903.526344	14.051341
17.873697	899.940647	14.056359
17.461639	910.601773	14.061376
17.636655	914.077406	14.066394
17.763797	903.233459	14.071411
17.509630	910.584884	14.076429
17.707710	902.557431	14.081447
17.439920	901.677667	14.086464
17.940948	897.740215	14.091482
17.747117	896.198856	14.096499
17.814981	908.587182	14.101517
18.042352	906.525816	14.106535
17.763400	912.151759	14.111552
18.404639	910.773864	14.116570
18.025015	911.277945	14.121587
17.894705	906.659322	14.126605
18.118718	896.781729	14.131623
18.014488	900.061001	14.136640
18.119112	901.550013	14.141658
18.467191	897.024162	14.146675
17.858976	904.168782	14.151693
18.218588	898.590276	14.156711
17.924222	900.419114	14.161728
18.239406	899.701042	14.166746
18.398417	902.702649	14.171763
18.006295	905.335640	14.176781
18.014893	906.306284	14.181799
17.888413	913.691478	14.186816
17.914933	905.106924	14.191834
18.273240	913.038317	14.196851
17.948260	911.763523	14.201869
18.321056	901.831205	14.206887
18.444164	911.238232	14.211904
18.194204	912.097657	14.216922
18.463651	914.368876	14.221939
18.258452	908.206134	14.226957
18.044705	898.835345	14.231975
18.115346	904.813944	14.236992
18.229375	915.279557	14.242010
18.392168	914.777711	14.247027
18.185286	925.447925	14.252045
18.170549	928.419785	14.257063
18.030999	927.532677	14.262080
17.900776	925.732108	14.267098
18.610844	922.629932	14.272115
18.445032	926.603592	14.277133
18.403083	925.865386	14.282151
18.559111	931.199552	14.287168
18.473101	923.471936	14.292186
18.495123	928.372540	14.297203
18.382598	923.662781	14.302221
18.706820	925.388998	14.307239
18.417288	920.539546	14.312256
18.179180	928.901470	14.317274
18.582319	930.523883	14.322291
18.732185	946.260329	14.327309
18.780205	949.818857	14.332327
18.922595	947.164816	14.337344
18.544621	935.604247	14.342362
18.734861	930.437101	14.347379
18.599120	946.296909	14.352397
18.904325	941.601000	14.357415
18.973321	954.288977	14.362432
18.970155	945.232509	14.367450
18.750615	939.753629	14.372467
18.453961	938.676390	14.377485
18.793129	954.752591	14.382503
19.131016	949.881183	14.387520
18.875168	955.888542	14.392538
19.267825	953.473240	14.397555
18.863069	952.942996	14.402573
18.428939	934.647351	14.407591
18.623506	951.175244	14.412608
18.832307	959.325591	14.417626
18.938431	943.284228	14.422643
18.798837	949.109386	14.427661
18.767672	954.160286	14.432679
19.031014	950.262985	14.437696
18.694485	952.205687	14.442714
18.951828	946.627310	14.447731
18.596669	956.762063	14.452749
19.130139	961.043413	14.457767
19.165172	964.073801	14.462784
19.122918	961.808261	14.467802
19.508341	974.074608	14.472819
19.223190	966.018224	14.477837
19.072037	967.818458	14.482855
19.357636	960.231780	14.487872
19.326849	966.235659	14.492890
19.127628	954.953354	14.497907
19.317084	960.758842	14.502925
19.414171	968.989702	14.507943
19.294299	960.377422	14.512960
19.050354	966.304038	14.517978
19.403593	966.208032	14.522995
19.331970	982.070511	14.528013
19.482547	976.508748	14.533031
19.613575	980.549810	14.538048
19.584666	978.736618	14.543066
19.674988	962.025524	14.548083
19.362353	961.061223	14.553101
19.600197	955.369117	14.558119
19.469956	950.397028	14.563136
19.224900	958.116275	14.568154
19.713967	964.219092	14.573171
19.645933	973.971486	14.578189
19.306613	968.454443	14.583207
19.533598	965.888212	14.588224
19.644287	973.416381	14.593242
19.767158	970.260456	14.598259
19.775891	969.252430	14.603277
19.589148	977.685273	14.608295
19.772395	971.114897	14.613312
19.321676	969.108609	14.618330
19.645252	964.649671	14.623347
19.520471	979.961858	14.628365
19.500129	974.906381	14.633383
19.823995	970.295920	14.638400
19.426034	978.401894	14.643418
19.963684	973.044949	14.648435
19.662392	975.468152	14.653453
19.756395	973.623200	14.658471
19.995620	966.453987	14.663488
19.391213	974.093494	14.668506
19.910947	973.577097	14.673523
19.378772	978.245270	14.678541
19.586657	995.708387	14.683559
19.899289	992.406151	14.688576
19.918477	1013.874909	14.693594
19.672259	995.278550	14.698611
20.243195	1007.134191	14.703629
19.816732	1000.213773	14.708647
19.915920	1003.174219	14.713664
19.587806	1004.528647	14.718682
19.814882	1006.052250	14.723699
19.856228	1002.656553	14.728717
20.192176	1005.513866	14.733735
20.796768	1012.258265	14.738752
20.467673	1001.248611	14.743770
20.281785	994.505330	14.748787
20.227801	987.056718	14.753805
20.199701	986.619305	14.758823
20.017017	986.076574	14.763840
19.974932	996.295146	14.768858
20.696119	988.924654	14.773875
20.456955	995.756235	14.778893
20.287145	989.130372	14.783911
20.075097	985.120890	14.788928
20.585078	992.145095	14.793946
20.581819	994.174765	14.798963
20.397977	991.246469	14.803981
20.326921	980.326038	14.808999
20.379089	984.139542	14.814016
20.314145	1003.099944	14.819034
20.939239	1006.884210	14.824051
20.482348	1005.033511	14.829069
20.233844	997.204932	14.834087
20.652651	1004.691453	14.839104
20.645420	1006.971048	14.844122
21.181401	998.546965	14.849139
20.969725	985.240588	14.854157
20.464808	980.484614	14.859175
20.661075	982.928178	14.864192
20.512351	991.837937	14.869210
20.621524	984.445972	14.874227
20.800544	989.325304	14.879245
20.581670	996.829057	14.884263
20.811808	984.965496	14.889280
20.428438	990.816000	14.894298
20.425744	1004.540792	14.899315
20.824313	1010.824970	14.904333
20.622222	1023.447908	14.909351
20.953033	1017.987456	14.914368
20.718461	1020.766345	14.919386
20.886645	1015.684658	14.924403
20.842286	1015.063587	14.929421
20.788413	1014.232561	14.934439
21.044461	1010.822368	14.939456
20.775071	1010.353096	14.944474
20.788503	1008.710030	14.949491
21.052387	1018.268761	14.954509
20.681917	1020.974136	14.959527
21.129362	1006.239704	14.964544
20.665228	1017.376053	14.969562
20.692585	1016.737504	14.974579
21.173151	1026.811604	14.979597
21.103784	1033.885002	14.984615
21.713973	1041.622603	14.989632
21.467300	1030.770509	14.994650
21.613389	1018.585502	14.999667
21.142931	1021.208616	15.004685
21.038583	1016.813136	15.009703
20.949372	1017.622292	15.014720
21.147150	1018.329962	15.019738
21.073878	1024.876953	15.024755
21.447473	1032.383149	15.029773
21.242984	1038.044873	15.034791
21.515873	1038.144411	15.039808
21.538092	1034.101600	15.044826
21.504300	1034.359338	15.049843
21.513501	1015.745281	15.054861
21.260678	1015.910891	15.059879
21.248392	1017.399180	15.064896
21.421815	1031.336410	15.069914
21.593361	1042.616795	15.074931
21.405717	1038.313172	15.079949
21.656774	1039.542714	15.084967
21.927011	1035.969364	15.089984
21.590049	1039.837154	15.095002
21.677140	1042.414489	15.100019
21.784431	1037.291785	15.105037
21.832712	1038.833761	15.110055
21.646607	1020.979086	15.115072
21.765386	1019.597324	15.120090
21.574095	1037.122632	15.125107
21.938800	1032.912889	15.130125
21.558064	1023.444960	15.135143
21.955967	1022.303756	15.140160
21.785641	1031.882763	15.145178
21.969267	1041.444535	15.150195
22.091023	1019.149115	15.155213
21.790243	1017.548658	15.160231
21.628297	1006.733880	15.165248
21.566175	1033.302393	15.170266
21.757220	1036.362151	15.175283
22.203900	1039.404198	15.180301
21.909797	1039.412136	15.185319
21.972021	1037.221836	15.190336
22.029339	1044.628959	15.195354
21.713075	1039.373388	15.200371
22.163750	1042.121328	15.205389
21.643177	1040.668697	15.210407
21.761530	1037.361988	15.215424
21.751316	1039.623117	15.220442
22.126069	1034.342009	15.225459
22.200023	1026.002471	15.230477
21.475408	1033.165266	15.235495
21.701724	1046.046561	15.240512
21.544095	1058.230261	15.245530
22.086964	1071.302127	15.250547
22.678010	1067.104473	15.255565
22.176064	1078.196254	15.260583
22.129498	1068.095611	15.265600
22.612744	1072.817148	15.270618
22.347565	1065.843191	15.275635
22.463903	1059.728163	15.280653
22.511819	1070.977322	15.285671
22.426466	1062.574211	15.290688
22.605039	1068.564462	15.295706
22.752812	1072.034901	15.300723
22.807123	1059.807351	15.305741
22.452902	1067.411100	15.310759
22.319001	1053.937930	15.315776
22.372399	1056.148132	15.320794
22.722808	1076.258911	15.325811
22.388558	1062.943158	15.330829
22.372598	1066.224497	15.335847
22.602923	1067.242677	15.340864
22.477647	1068.792744	15.345882
22.443347	1069.852125	15.350899
22.428321	1072.975531	15.355917
21.979005	1060.668605	15.360935
22.430393	1077.595280	15.365952
22.552993	1089.732216	15.370970
22.537249	1097.494714	15.375987
22.805161	1087.461861	15.381005
22.757912	1088.343381	15.386023
22.981577	1078.958042	15.391040
23.003918	1078.093056	15.396058
22.966494	1081.765898	15.401075
23.301469	1075.894531	15.406093
23.032230	1078.751409	15.411111
23.286978	1080.939732	15.416128
23.197686	1077.848379	15.421146
23.090325	1083.321428	15.426163
23.210953	1067.558558	15.431181
22.843666	1069.231510	15.436199
23.014264	1073.648280	15.441216
23.329453	1069.515666	15.446234
23.551602	1070.430979	15.451251
23.512795	1046.948711	15.456269
23.130934	1053.190314	15.461287
23.512607	1046.898281	15.466304
23.311370	1050.754410	15.471322
22.877203	1044.908132	15.476339
23.251511	1027.483741	15.481357
23.347656	1048.716501	15.486375
23.296377	1039.276162	15.491392
23.414558	1038.238468	15.496410
23.499975	1043.523703	15.501427
23.084480	1032.820967	15.506445
23.398086	1042.327789	15.511463
23.700671	1042.675164	15.516480
23.556170	1039.712332	15.521498
23.411555	1041.467376	15.526515
23.478604	1035.397899	15.531533
23.190029	1044.651346	15.536551
23.233485	1043.874592	15.541568
23.205248	1044.778396	15.546586
22.940990	1057.549890	15.551603
23.205357	1060.162741	15.556621
23.629139	1067.758966	15.561639
23.757072	1064.529654	15.566656
23.928985	1059.904960	15.571674
23.555472	1067.615853	15.576691
23.416498	1062.149638	15.581709
23.635402	1073.189142	15.586727
23.515024	1062.803352	15.591744
23.518215	1065.185472	15.596762
23.421925	1067.112873	15.601779
23.455028	1065.242680	15.606797
23.601822	1080.503203	15.611815
23.635719	1090.296594	15.616832
24.158584	1090.167866	15.621850
23.761551	1088.490872	15.626867
23.902584	1087.061459	15.631885
23.988522	1092.801057	15.636903
24.219439	1086.655558	15.641920
24.060405	1090.315778	15.646938
23.696697	1092.524655	15.651955
23.937847	1093.055164	15.656973
23.784025	1092.062973	15.661991
23.980908	1095.847658	15.667008
23.880149	1089.614944	15.672026
24.018134	1097.274614	15.677043
23.999352	1078.197794	15.682061
24.184534	1090.637407	15.687079
24.126441	1090.337204	15.692096
24.309989	1091.510990	15.697114
24.212394	1091.131731	15.702131
24.372701	1083.214218	15.707149
24.258364	1097.297287	15.712167
24.017744	1098.483467	15.717184
24.361803	1102.232616	15.722202
24.339329	1111.059662	15.727219
24.796316	1108.249320	15.732237
24.532976	1102.723561	15.737255
24.162184	1096.867399	15.742272
24.504704	1093.437416	15.747290
24.310125	1099.151265	15.752307
24.518647	1114.070850	15.757325
24.317892	1119.097709	15.762343
24.214900	1122.244286	15.767360
24.478728	1109.482314	15.772378
24.483753	1118.456560	15.777395
24.579990	1115.566685	15.782413
24.454015	1109.322111	15.787431
24.755184	1109.511920	15.792448
24.836249	1110.250389	15.797466
24.835199	1109.572078	15.802483
24.445467	1119.794356	15.807501
24.512136	1113.415647	15.812519
24.688944	1110.544786	15.817536
24.984292	1110.833330	15.822554
24.952156	1120.176276	15.827571
24.977615	1117.347913	15.832589
24.758598	1118.716921	15.837607
24.613391	1117.164816	15.842624
24.388041	1115.596787	15.847642
25.008980	1133.062000	15.852659
25.329428	1127.609440	15.857677
25.001991	1137.635838	15.862695
25.092134	1150.569968	15.867712
25.297630	1126.017620	15.872730
25.075284	1118.866562	15.877747
25.033155	1114.423500	15.882765
25.049048	1110.851866	15.887783
25.251420	1132.516307	15.892800
25.303694	1118.805820	15.897818
24.963766	1116.624476	15.902835
24.787838	1126.927077	15.907853
25.310992	1138.837582	15.912871
25.038820	1136.866590	15.917888
25.240496	1140.899845	15.922906
24.997242	1143.717973	15.927923
25.239201	1134.941977	15.932941
25.478601	1134.702750	15.937959
24.960712	1140.902447	15.942976
25.179250	1141.777302	15.947994
25.706774	1140.032092	15.953011
25.388833	1138.973933	15.958029
25.544057	1143.790742	15.963047
25.275978	1148.594564	15.968064
25.949479	1138.100905	15.973082
25.569751	1145.838046	15.978099
25.556855	1144.486242	15.983117
25.990618	1136.617647	15.988135
25.477864	1149.431053	15.993152
25.555908	1147.449714	15.998170
25.601643	1151.734466	16.003187
25.648386	1142.676438	16.008205
25.981148	1133.330888	16.013223
25.787300	1145.059544	16.018240
25.744421	1139.338505	16.023258
25.646709	1146.671978	16.028275
25.684341	1146.218016	16.033293
26.265903	1158.018455	16.038311
25.491081	1151.641361	16.043328
26.107509	1148.638932	16.048346
26.262789	1163.604718	16.053363
26.054949	1152.661297	16.058381
26.059950	1143.515095	16.063399
25.697253	1139.203988	16.068416
26.441033	1145.469180	16.073434
26.094459	1151.017364	16.078451
25.740376	1138.241125	16.083469
26.218989	1159.086267	16.088487
26.087222	1158.011744	16.093504
26.378770	1158.209363	16.098522
26.440073	1161.283031	16.103539
26.250477	1152.324911	16.108557
26.295333	1147.467514	16.113575
26.005273	1156.263662	16.118592
26.615653	1153.176968	16.123610
26.461456	1166.183866	16.128627
26.258023	1161.387214	16.133645
26.362202	1153.090248	16.138663
26.496347	1159.027488	16.143680
26.323488	1164.258298	16.148698
26.381586	1161.131359	16.153715
26.276437	1161.965094	16.158733
26.169314	1164.181367	16.163751
25.763434	1170.145886	16.168768
25.966073	1158.147637	16.173786
26.223941	1171.630020	16.178803
26.574924	1184.624548	16.183821
26.607187	1176.098930	16.188839
26.348746	1186.202975	16.193856
26.432040	1188.042468	16.198874
26.587036	1189.255419	16.203891
26.469589	1182.839080	16.208909
26.834388	1174.611979	16.213927
27.030069	1184.654786	16.218944
26.614557	1185.940784	16.223962
26.480752	1190.436535	16.228979
26.769722	1187.671274	16.233997
26.661483	1181.859412	16.239015
26.753755	1182.201666	16.244032
26.881784	1180.281968	16.249050
27.113213	1188.507792	16.254067
26.797314	1188.916752	16.259085
26.991538	1185.200574	16.264103
26.578159	1189.701984	16.269120
27.354088	1204.773142	16.274138
27.100244	1210.600395	16.279155
26.934003	1213.280312	16.284173
27.280173	1211.964116	16.289191
27.406248	1212.241147	16.294208
27.380597	1206.902410	16.299226
27.341035	1200.530742	16.304243
27.327475	1197.727376	16.309261
27.371198	1189.578661	16.314279
27.283714	1200.609144	16.319296
27.307635	1198.080807	16.324314
27.365834	1194.537283	16.329331
27.403585	1206.668575	16.334349
27.630790	1208.810710	16.339367
27.615085	1212.221422	16.344384
27.183282	1200.558609	16.349402
27.575837	1207.998811	16.354419
27.208466	1212.603516	16.359437
27.462114	1200.117617	16.364455
27.456988	1204.385054	16.369472
27.940392	1208.390240	16.374490
27.995921	1199.927259	16.379507
27.734544	1203.291013	16.384525
28.031636	1208.224606	16.389543
27.962578	1193.728226	16.394560
27.713271	1184.280773	16.399578
27.247430	1191.106696	16.404595
27.509605	1191.917955	16.409613
27.643739	1198.521080	16.414631
27.761036	1196.476820	16.419648
27.849289	1195.238651	16.424666
27.815662	1200.081722	16.429683
27.525746	1196.399895	16.434701
28.080476	1196.685925	16.439719
27.971455	1200.344692	16.444736
28.160223	1195.146142	16.449754
28.010279	1199.859002	16.454771
27.759718	1201.466455	16.459789
28.029371	1200.575582	16.464807
27.862579	1197.089178	16.469824
27.686647	1200.341799	16.474842
28.231020	1203.602193	16.479859
28.301446	1224.551990	16.484877
28.672919	1214.313594	16.489895
28.473051	1216.490665	16.494912
28.090103	1206.076246	16.499930
28.315038	1199.934794	16.504947
28.422765	1219.168342	16.509965
28.441433	1209.619192	16.514983
28.526094	1223.901751	16.520000
28.613519	1199.099442	16.525018
28.406255	1208.160434	16.530035
28.351687	1212.135772	16.535053
28.561197	1212.690145	16.540071
28.364590	1206.421821	16.545088
28.219336	1211.370637	16.550106
28.507189	1230.080693	16.555123
28.379179	1221.062457	16.560141
28.588270	1222.456336	16.565159
28.626043	1230.911146	16.570176
28.237666	1223.659664	16.575194
28.789477	1212.045669	16.580211
27.918973	1224.738104	16.585229
28.220039	1216.593491	16.590247
28.418474	1225.405134	16.595264
28.788653	1244.900802	16.600282
29.209443	1242.260176	16.605299
28.992511	1239.021411	16.610317
28.831578	1234.716737	16.615335
29.100970	1236.915423	16.620352
29.172920	1246.911258	16.625370
29.689145	1234.870445	16.630387
28.969527	1230.059468	16.635405
29.090126	1211.153308	16.640423
29.061581	1216.519454	16.645440
28.898813	1213.745628	16.650458
28.981560	1222.026175	16.655475
29.064571	1241.105805	16.660493
29.507723	1236.063296	16.665511
29.383872	1246.723930	16.670528
29.191046	1242.509426	16.675546
29.673398	1238.795713	16.680563
29.300318	1238.137452	16.685581
29.170854	1220.267447	16.690599
29.311237	1232.329128	16.695616
29.507835	1227.504888	16.700634
29.498911	1228.039623	16.705651
29.368534	1241.279551	16.710669
29.742878	1233.426477	16.715687
29.738557	1244.633386	16.720704
29.650247	1238.717417	16.725722
29.871846	1228.776901	16.730739
29.295503	1220.197697	16.735757
29.549744	1225.125342	16.740775
29.507886	1229.543671	16.745792
29.488644	1232.118654	16.750810
29.732559	1233.333543	16.755827
29.656815	1240.332277	16.760845
29.605353	1233.820439	16.765863
29.829892	1239.374404	16.770880
29.451781	1246.211935	16.775898
29.892468	1235.628236	16.780915
29.653623	1248.427468	16.785933
29.481380	1236.604298	16.790951
29.615796	1242.005039	16.795968
29.429901	1245.088807	16.800986
29.894254	1247.875675	16.806003
30.040251	1255.979133	16.811021
29.810576	1246.803144	16.816039
29.808108	1251.524613	16.821056
29.865080	1250.651072	16.826074
30.124535	1248.360611	16.831091
30.399881	1251.479864	16.836109
29.890510	1247.885842	16.841127
30.035277	1247.333146	16.846144
29.918195	1257.279523	16.851162
30.376852	1259.278331	16.856179
30.077912	1278.767763	16.861197
30.358131	1275.132851	16.866215
30.714404	1278.630827	16.871232
30.861326	1279.968119	16.876250
30.786635	1260.492710	16.881267
30.535823	1256.397684	16.886285
30.672603	1249.376851	16.891303
30.584106	1249.605241	16.896320
30.229366	1248.385548	16.901338
30.442358	1240.485009	16.906355
30.416108	1255.794715	16.911373
30.556604	1262.289576	16.916391
30.641715	1272.040380	16.921408
30.534092	1269.908054	16.926426
30.618073	1263.750657	16.931443
30.483103	1274.633945	16.936461
30.477600	1269.181599	16.941479
30.898834	1266.301059	16.946496
30.597462	1276.118350	16.951514
30.622429	1270.856919	16.956531
30.547215	1279.146307	16.961549
30.526263	1283.432007	16.966567
30.927119	1287.749863	16.971584
30.996477	1295.022672	16.976602
31.280471	1293.671970	16.981619
31.111803	1303.124632	16.986637
31.250592	1301.064390	16.991655
31.423542	1301.857988	16.996672
31.001260	1296.571510	17.001690
31.351258	1289.324960	17.006707
31.088245	1310.484564	17.011725
31.230209	1296.731574	17.016743
31.321629	1296.856212	17.021760
31.211239	1304.532551	17.026778
31.524855	1295.666424	17.031795
31.457602	1297.223255	17.036813
31.290857	1299.836992	17.041831
31.650034	1293.895514	17.046848
31.637655	1305.614956	17.051866
31.557913	1291.110693	17.056883
31.526469	1300.349485	17.061901
31.583620	1302.751637	17.066919
31.473011	1291.202857	17.071936
31.494814	1294.834964	17.076954
31.467774	1290.989112	17.081971
31.374425	1298.782716	17.086989
31.479750	1291.618441	17.092007
31.828698	1286.899853	17.097024
31.776472	1297.517808	17.102042
31.940222	1298.546368	17.107059
31.779070	1300.231427	17.112077
31.659301	1303.153431	17.117095
31.563756	1289.689890	17.122112
31.419694	1299.517415	17.127130
31.848932	1310.985066	17.132147
32.047058	1312.301764	17.137165
32.047231	1323.498556	17.142183
32.068266	1317.338318	17.147200
31.852108	1319.811428	17.152218
31.928074	1316.432371	17.157235
31.749353	1334.019130	17.162253
31.886987	1321.443911	17.167271
32.190305	1321.207354	17.172288
31.928057	1323.949573	17.177306
32.357400	1317.681582	17.182323
31.996418	1325.093989	17.187341
31.978742	1340.995725	17.192359
32.426237	1343.311861	17.197376
32.694690	1343.336353	17.202394
32.714002	1335.065140	17.207411
32.664873	1336.496076	17.212429
32.707890	1335.962375	17.217447
32.752078	1323.679415	17.222464
32.554011	1317.969857	17.227482
32.520874	1317.129277	17.232499
32.417836	1316.725614	17.237517
32.452558	1318.033040	17.242535
32.583519	1326.713228	17.247552
32.719132	1330.365491	17.252570
32.902084	1332.107432	17.257587
33.029061	1334.435601	17.262605
33.020015	1342.695782	17.267623
33.063289	1327.111984	17.272640
32.525833	1326.450910	17.277658
32.654682	1326.317256	17.282675
32.764774	1328.430302	17.287693
32.687277	1341.068779	17.292711
33.161179	1336.103506	17.297728
32.943967	1340.896303	17.302746
33.313296	1339.238821	17.307763
33.013788	1332.282728	17.312781
32.721450	1338.131794	17.317799
33.517534	1330.686386	17.322816
33.245103	1332.628616	17.327834
33.299170	1332.011143	17.332851
33.468301	1332.751689	17.337869
33.369884	1329.519701	17.342887
33.347999	1327.332994	17.347904
33.099993	1334.932942	17.352922
33.304175	1336.965069	17.357939
33.113163	1328.259545	17.362957
33.161520	1327.090695	17.367975
32.805018	1333.019178	17.372992
33.137858	1350.046621	17.378010
33.598463	1353.509434	17.383027
33.538995	1356.166436	17.388045
33.189348	1349.240234	17.393063
33.366191	1346.312525	17.398080
33.524722	1354.575023	17.403098
33.486719	1351.494571	17.408115
33.508161	1354.568167	17.413133
33.582548	1371.875713	17.418151
34.200879	1374.310423	17.423168
34.075720	1367.062082	17.428186
33.567537	1363.638266	17.433203
33.712076	1370.173563	17.438221
33.619577	1378.402572	17.443239
33.978304	1376.576323	17.448256
33.539512	1378.648601	17.453274
34.347370	1379.510609	17.458291
34.212778	1372.746575	17.463309
34.252581	1385.051238	17.468327
34.549327	1377.872904	17.473344
34.372347	1383.208561	17.478362
34.381644	1378.508118	17.483379
34.215103	1376.861481	17.488397
34.545425	1379.479890	17.493415
34.340167	1379.811667	17.498432
34.255759	1380.194056	17.503450
34.339861	1374.866582	17.508467
34.521368	1372.875421	17.513485
34.301639	1379.918718	17.518503
34.546619	1373.673100	17.523520
34.061063	1377.573566	17.528538
34.286935	1369.999170	17.533555
34.384886	1373.310166	17.538573
34.234246	1385.388860	17.543591
34.473661	1387.279806	17.548608
34.744227	1405.102796	17.553626
34.662103	1398.138078	17.558643
34.435958	1404.974100	17.563661
35.035411	1411.186118	17.568679
35.058595	1398.805391	17.573696
34.960538	1403.185175	17.578714
34.920142	1406.173733	17.583731
35.017368	1401.958213	17.588749
34.942585	1405.321356	17.593767
35.411781	1399.517349	17.598784
34.880468	1406.435599	17.603802
35.167227	1413.889204	17.608819
35.139096	1401.964591	17.613837
35.084200	1404.027594	17.618855
34.890417	1395.944166	17.623872
35.092342	1399.926948	17.628890
34.794357	1398.897225	17.633907
35.334765	1397.301464	17.638925
34.926238	1398.687375	17.643943
35.393418	1389.863565	17.648960
35.283542	1397.363138	17.653978
35.106538	1403.386774	17.658995
35.558673	1396.651301	17.664013
34.763181	1403.752693	17.669031
35.093169	1411.316331	17.674048
35.120019	1426.229750	17.679066
35.311535	1423.672132	17.684083
35.717566	1422.576977	17.689101
35.760131	1418.458327	17.694119
35.946191	1417.195447	17.699136
35.631934	1427.330409	17.704154
35.565495	1425.759701	17.709171
35.550580	1421.391222	17.714189
35.850495	1425.191495	17.719207
35.984584	1413.942210	17.724224
35.771757	1427.270853	17.729242
35.790327	1424.759097	17.734259
36.296779	1411.353215	17.739277
36.360538	1415.291240	17.744295
36.624717	1392.241028	17.749312
36.635797	1401.930845	17.754330
36.574687	1406.588902	17.759347
36.904198	1400.576268	17.764365
36.383723	1393.717670	17.769383
36.378161	1384.749714	17.774400
36.189356	1378.678931	17.779418
36.501776	1373.716698	17.784435
36.519083	1378.431966	17.789453
36.510278	1391.126056	17.794471
36.652462	1369.672777	17.799488
36.401057	1384.061437	17.804506
36.374517	1374.727521	17.809523
36.894025	1365.564215	17.814541
36.529823	1369.351110	17.819559
36.426545	1362.156169	17.824576
36.730972	1373.823175	17.829594
36.536911	1374.841177	17.834611
36.598537	1368.725094	17.839629
36.545514	1371.744014	17.844647
36.567756	1367.445503	17.849664
36.399836	1374.322940	17.854682
36.692907	1389.248528	17.859699
37.091840	1387.393927	17.864717
36.753426	1394.752356	17.869735
37.083646	1396.941592	17.874752
37.022974	1396.875315	17.879770
37.045914	1405.502932	17.884787
37.045009	1402.823796	17.889805
36.812560	1400.461580	17.894823
36.984030	1404.013601	17.899840
36.724088	1403.413458	17.904858
36.719321	1399.052871	17.909875
37.266702	1396.562928	17.914893
36.789193	1393.973778	17.919911
36.745490	1403.359699	17.924928
36.964556	1414.961127	17.929946
36.961439	1419.913117	17.934963
37.217761	1424.976195	17.939981
37.092654	1423.177935	17.944999
37.511636	1422.907589	17.950016
37.382739	1413.084658	17.955034
37.188948	1427.884108	17.960051
37.322940	1424.309802	17.965069
37.480963	1437.441857	17.970087
37.400572	1437.056756	17.975104
37.543159	1440.660619	17.980122
37.630071	1446.816749	17.985139
37.994755	1445.062150	17.990157
37.823653	1454.026117	17.995175
37.764213	1442.945803	18.000192
38.079972	1447.128624	18.005210
37.854393	1448.123134	18.010227
38.034063	1442.758670	18.015245
38.041920	1450.129481	18.020263
37.900235	1440.658823	18.025280
37.811736	1437.677738	18.030298
37.894597	1440.180048	18.035315
38.549030	1436.916033	18.040333
38.118433	1447.801273	18.045351
37.908804	1442.759354	18.050368
38.140341	1435.193516	18.055386
37.978115	1443.932032	18.060403
38.649146	1450.224439	18.065421
38.319574	1456.353898	18.070439
38.221271	1465.499042	18.075456
38.869067	1465.464472	18.080474
38.552781	1459.555522	18.085491
38.678880	1447.830929	18.090509
38.300249	1449.688720	18.095527
38.193788	1456.768061	18.100544
38.612344	1460.347896	18.105562
38.398940	1460.289619	18.110579
38.835911	1453.973056	18.115597
38.766267	1464.795795	18.120615
38.973902	1463.993461	18.125632
38.757429	1454.897360	18.130650
38.697557	1460.069639	18.135667
38.962757	1455.076866	18.140685
39.012302	1463.078669	18.145703
38.754652	1467.079371	18.150720
38.854929	1458.262158	18.155738
38.534351	1455.165724	18.160755
38.816962	1470.070917	18.165773
39.528963	1470.739569	18.170791
39.223221	1473.024675	18.175808
39.173018	1469.974505	18.180826
39.212267	1470.138826	18.185843
39.183480	1476.625408	18.190861
39.401984	1478.027309	18.195879
39.369519	1489.090430	18.200896
39.268919	1476.965609	18.205914
39.087347	1479.720537	18.210931
39.261811	1479.639741	18.215949
39.216923	1484.554071	18.220967
39.471247	1491.267981	18.225984
39.417550	1484.945750	18.231002
39.135056	1483.058378	18.236019
39.780913	1475.579495	18.241037
39.262361	1481.533257	18.246055
39.364041	1500.477713	18.251072
40.045528	1499.547951	18.256090
39.659926	1509.144952	18.261107
39.640364	1507.869899	18.266125
39.764445	1505.524742	18.271143
40.040458	1508.407249	18.276160
40.298913	1508.142961	18.281178
39.937733	1514.851724	18.286195
39.615046	1504.213150	18.291213
39.889781	1510.078124	18.296231
40.174577	1506.723323	18.301248
40.154966	1503.621046	18.306266
39.827897	1505.808490	18.311283
40.046967	1500.949120	18.316301
40.242071	1508.325515	18.321319
40.070821	1519.078900	18.326336
40.307340	1521.645661	18.331354
40.292749	1526.886649	18.336371
40.615623	1527.107799	18.341389
40.363906	1529.927305	18.346407
40.335234	1534.902241	18.351424
40.578764	1530.073769	18.356442
40.567838	1542.307543	18.361459
40.549907	1534.136711	18.366477
40.744559	1534.510370	18.371495
40.267692	1537.459607	18.376512
40.616938	1535.596949	18.381530
40.604582	1546.413974	18.386547
40.703940	1530.887539	18.391565
40.746262	1536.662474	18.396583
41.054541	1547.906112	18.401600
40.938086	1546.538843	18.406618
40.977708	1548.309433	18.411635
41.252627	1559.368921	18.416653
41.158051	1562.766733	18.421671
41.058090	1564.322368	18.426688
41.385476	1561.721486	18.431706
41.023102	1558.842982	18.436723
41.307887	1556.583253	18.441741
41.204550	1558.265647	18.446759
40.778298	1556.814066	18.451776
41.144533	1557.527088	18.456794
40.925685	1560.016429	18.461811
41.341682	1554.618293	18.466829
41.501705	1555.420227	18.471847
41.217098	1562.454761	18.476864
41.474235	1566.113400	18.481882
41.521851	1576.905327	18.486899
41.792250	1575.843903	18.491917
42.105153	1572.071297	18.496935
41.795223	1573.318792	18.501952
42.292253	1567.671346	18.506970
41.753543	1565.618726	18.511987
41.656557	1557.589582	18.517005
41.916691	1558.675735	18.522023
42.236289	1576.996200	18.527040
42.471465	1569.429738	18.532058
42.157525	1557.533741	18.537075
42.170015	1552.435118	18.542093
42.157421	1554.964930	18.547111
41.927654	1551.715482	18.552128
42.023894	1551.615307	18.557146
41.833711	1557.265500	18.562163
42.221973	1569.506570	18.567181
42.365392	1572.952538	18.572199
42.525145	1573.012890	18.577216
42.457796	1569.409942	18.582234
42.133476	1571.862057	18.587251
42.326922	1573.154257	18.592269
42.386346	1558.192602	18.597287
42.344868	1570.607880	18.602304
42.408826	1573.939985	18.607322
42.418780	1563.009740	18.612339
42.184594	1567.101486	18.617357
42.209351	1570.171447	18.622375
42.297225	1591.295687	18.627392
42.606058	1584.121701	18.632410
42.485498	1596.520906	18.637427
42.581911	1600.993540	18.642445
42.901665	1596.560288	18.647463
42.571662	1597.337531	18.652480
43.214863	1607.165731	18.657498
43.167086	1622.346557	18.662515
43.176405	1617.601865	18.667533
43.344804	1609.351494	18.672551
43.119399	1614.047808	18.677568
43.400239	1603.223688	18.682586
43.070654	1608.292833	18.687603
43.135498	1612.205486	18.692621
43.292611	1613.487567	18.697639
43.494613	1622.892153	18.702656
43.300264	1612.930977	18.707674
43.696752	1619.199917	18.712691
43.289474	1620.831807	18.717709
43.183135	1613.337434	18.722727
43.198572	1623.506384	18.727744
43.400848	1611.201769	18.732762
43.520546	1621.903604	18.737779
43.231548	1624.675280	18.742797
43.908260	1634.605576	18.747815
43.707564	1648.024014	18.752832
43.901912	1633.621969	18.757850
43.787242	1641.292807	18.762867
43.832193	1643.949374	18.767885
44.147858	1633.804636	18.772903
43.916427	1645.848747	18.777920
44.295411	1628.344146	18.782938
43.950250	1638.054842	18.787955
43.813361	1633.733704	18.792973
44.100028	1630.495355	18.797991
44.025098	1641.839742	18.803008
44.080777	1645.270982	18.808026
44.023971	1648.369435	18.813043
44.081680	1660.352758	18.818061
44.451146	1659.960728	18.823079
44.322500	1663.947700	18.828096
44.464831	1658.456438	18.833114
44.748850	1654.530519	18.838131
44.914919	1658.424266	18.843149
44.976478	1652.876152	18.848167
44.931003	1655.969686	18.853184
44.509350	1651.503529	18.858202
44.729218	1651.257870	18.863219
44.999228	1661.671233	18.868237
44.595451	1656.722599	18.873255
44.662974	1659.766982	18.878272
44.978104	1653.046433	18.883290
45.161727	1656.675509	18.888307
44.888900	1659.163800	18.893325
45.260050	1647.284157	18.898343
44.959662	1648.675341	18.903360
44.665628	1659.804539	18.908378
45.200503	1670.186137	18.913395
45.002959	1673.451676	18.918413
45.350706	1674.817692	18.923431
45.266742	1677.080916	18.928448
45.515820	1672.926899	18.933466
45.431880	1664.453853	18.938483
45.056581	1672.234713	18.943501
45.810669	1667.225725	18.948519
45.807395	1667.787996	18.953536
45.793876	1661.907579	18.958554
45.838351	1658.889974	18.963571
45.844530	1674.321225	18.968589
45.704776	1664.824900	18.973607
45.755908	1667.944421	18.978624
45.896971	1663.494792	18.983642
46.207907	1654.906621	18.988659
46.252084	1662.530646	18.993677
46.228520	1653.868321	18.998695
46.252813	1668.769717	19.003712
46.034867	1657.259503	19.008730
46.428725	1649.987044	19.013747
46.351242	1664.512956	19.018765
46.007208	1657.854007	19.023783
46.342448	1656.662560	19.028800
46.354180	1651.368363	19.033818
46.607960	1659.190130	19.038835
46.379538	1654.734913	19.043853
46.594127	1657.570202	19.048871
46.513838	1659.110159	19.053888
46.070436	1653.031583	19.058906
46.247173	1650.555131	19.063923
46.300735	1659.503156	19.068941
46.406083	1652.736372	19.073959
46.452842	1655.411595	19.078976
46.517223	1668.801402	19.083994
46.819268	1667.949645	19.089011
46.617555	1682.756850	19.094029
46.822105	1677.880758	19.099047
46.596703	1678.288261	19.104064
46.461726	1684.460086	19.109082
46.711034	1683.910035	19.114099
46.801306	1703.875830	19.119117
46.935832	1706.515304	19.124135
46.723963	1708.927838	19.129152
46.816290	1705.331561	19.134170
47.223370	1693.850245	19.139187
47.357321	1701.062669	19.144205
47.657004	1689.118384	19.149223
47.766110	1691.083301	19.154240
47.306677	1697.179411	19.159258
47.829125	1690.959912	19.164275
47.445697	1694.680439	19.169293
47.715209	1694.341842	19.174311
47.815324	1684.789225	19.179328
47.699030	1694.208692	19.184346
48.129151	1691.585483	19.189363
47.664446	1694.545476	19.194381
47.895368	1693.575401	19.199399
48.022794	1693.530331	19.204416
47.729310	1690.297090	19.209434
48.333036	1687.833049	19.214451
47.934301	1686.680136	19.219469
47.665663	1692.112209	19.224487
48.011230	1684.809384	19.229504
48.111447	1707.759089	19.234522
48.215275	1706.385914	19.239539
48.300909	1714.678864	19.244557
48.491168	1705.683414	19.249575
48.549529	1713.160082	19.254592
48.653771	1715.447659	19.259610
48.589210	1710.752315	19.264627
48.611906	1728.421714	19.269645
48.344401	1709.569140	19.274663
48.399719	1716.503473	19.279680
48.057054	1713.085376	19.284698
49.010537	1716.746084	19.289715
48.406173	1717.704907	19.294733
48.622793	1710.497889	19.299751
48.647720	1719.002269	19.304768
48.604547	1708.727161	19.309786
48.703506	1719.015708	19.314803
48.720481	1716.917579	19.319821
48.895488	1732.013318	19.324839
48.928824	1727.119687	19.329856
48.862666	1729.894555	19.334874
49.166573	1739.434819	19.339891
48.716824	1751.380444	19.344909
48.942400	1741.653625	19.349927
48.719298	1737.882385	19.354944
48.729864	1747.746043	19.359962
49.232133	1760.089417	19.364979
49.389836	1764.262208	19.369997
49.349279	1774.834447	19.375015
49.328179	1756.965967	19.380032
49.153436	1756.305208	19.385050
49.591470	1752.614070	19.390067
49.541205	1761.439453	19.395085
49.872617	1775.826051	19.400103
49.959422	1780.495890	19.405120
49.819948	1779.839107	19.410138
50.114675	1774.608112	19.415155
50.091232	1782.375263	19.420173
50.437338	1770.796091	19.425191
50.170375	1755.982919	19.430208
50.111523	1762.742536	19.435226
50.036278	1760.175910	19.440243
50.204763	1767.370361	19.445261
50.622634	1775.365452	19.450279
50.286968	1764.567792	19.455296
49.987217	1761.035704	19.460314
50.201239	1774.632672	19.465331
50.260537	1783.870208	19.470349
50.432665	1775.442451	19.475367
50.697531	1774.568075	19.480384
50.368269	1782.600597	19.485402
50.667539	1778.760641	19.490419
50.501474	1785.536959	19.495437
50.410132	1784.383519	19.500455
50.525988	1777.766534	19.505472
50.395392	1781.798018	19.510490
50.826425	1795.534787	19.515507
50.861153	1806.884297	19.520525
51.158867	1796.963174	19.525543
51.338441	1802.716826	19.530560
51.094778	1803.294437	19.535578
51.613898	1799.691654	19.540595
51.543696	1799.648951	19.545613
51.392210	1801.424073	19.550631
51.476468	1795.585195	19.555648
51.411695	1799.221416	19.560666
51.629834	1785.348889	19.565683
51.551514	1793.635844	19.570701
51.302530	1792.241852	19.575719
51.915872	1797.931123	19.580736
51.651263	1797.644125	19.585754
51.620509	1787.755212	19.590771
51.295506	1797.740574	19.595789
51.394932	1797.264350	19.600807
51.770781	1794.182506	19.605824
51.835947	1797.669104	19.610842
51.791420	1794.589591	19.615859
51.693943	1790.953419	19.620877
51.769121	1788.098274	19.625895
51.690349	1797.713931	19.630912
51.933894	1798.016865	19.635930
52.253902	1814.270401	19.640947
52.247632	1821.892881	19.645965
52.076291	1819.552653	19.650983
51.916612	1815.907225	19.656000
52.056082	1822.989447	19.661018
52.402111	1820.764333	19.666035
52.154308	1820.853425	19.671053
52.141671	1819.406853	19.676071
52.321977	1825.409714	19.681088
52.081939	1835.407115	19.686106
52.297888	1842.805652	19.691123
52.673477	1847.086553	19.696141
52.590849	1843.037792	19.701159
52.640570	1841.928658	19.706176
52.475993	1847.010050	19.711194
53.069328	1834.789567	19.716211
53.076908	1845.281768	19.721229
53.106679	1838.753905	19.726247
53.198848	1842.106916	19.731264
53.035374	1848.400002	19.736282
53.220490	1860.603471	19.741299
53.177996	1861.578966	19.746317
53.244300	1876.259393	19.751335
53.383530	1865.652829	19.756352
53.299760	1864.955810	19.761370
53.512751	1864.376694	19.766387
53.579660	1858.821372	19.771405
53.818071	1866.617221	19.776423
53.685046	1862.674134	19.781440
53.317140	1866.966654	19.786458
53.357571	1869.901678	19.791475
53.573837	1864.054849	19.796493
53.521474	1867.455614	19.801511
53.952942	1860.028887	19.806528
53.606108	1871.554614	19.811546
53.935723	1881.640079	19.816563
53.779759	1884.883403	19.821581
53.941824	1879.057631	19.826599
53.636348	1883.116366	19.831616
53.765952	1893.046780	19.836634
53.771337	1886.765702	19.841651
53.893750	1887.990087	19.846669
54.141655	1912.498171	19.851687
54.465795	1905.103916	19.856704
54.322327	1901.096172	19.861722
54.189396	1906.586078	19.866739
54.476909	1906.389847	19.871757
54.455021	1908.267882	19.876775
55.058352	1905.567181	19.881792
54.429883	1919.210220	19.886810
54.680256	1922.109410	19.891827
54.754330	1922.748012	19.896845
54.563775	1922.061305	19.901863
54.923719	1925.363173	19.906880
55.012359	1924.872846	19.911898
54.957644	1918.010958	19.916915
54.997688	1928.775873	19.921933
54.920489	1918.783663	19.926951
55.290259	1911.413860	19.931968
55.541608	1920.700464	19.936986
55.385619	1918.004370	19.942003
55.469141	1916.208292	19.947021
55.436645	1922.840786	19.952039
55.647611	1928.239284	19.957056
55.134282	1921.095336	19.962074
55.432293	1928.339115	19.967091
55.748030	1945.022640	19.972109
55.844192	1952.575577	19.977127
56.212340	1945.673088	19.982144
56.043279	1934.918815	19.987162
55.827487	1928.482804	19.992179
55.734051	1922.318088	19.997197
55.832597	1932.799333	20.002215
56.269127	1939.415614	20.007232
56.427937	1941.600047	20.012250
56.224629	1938.412682	20.017267
56.334044	1935.921426	20.022285
56.071644	1942.536071	20.027303
56.479612	1928.678061	20.032320
56.375228	1936.498908	20.037338
56.618911	1940.383788	20.042355
56.859297	1937.824801	20.047373
56.318156	1940.550573	20.052391
56.904184	1940.828590	20.057408
56.355451	1936.934431	20.062426
56.404337	1932.366538	20.067443
56.831357	1933.635022	20.072461
56.518651	1932.478166	20.077479
56.607965	1932.350664	20.082496
56.228911	1936.480828	20.087514
56.399536	1950.308756	20.092531
56.922378	1950.404101	20.097549
56.894948	1958.235068	20.102567
57.380735	1953.561275	20.107584
57.160438	1957.843459	20.112602
57.232555	1962.395708	20.117619
57.503927	1949.811849	20.122637
57.098568	1961.870628	20.127655
57.186272	1957.053679	20.132672
57.328389	1971.248992	20.137690
57.070044	1979.371550	20.142707
57.777205	1980.022044	20.147725
57.784910	1984.492805	20.152743
57.774325	1974.452321	20.157760
57.715581	1989.114439	20.162778
57.935184	1971.687969	20.167795
57.920553	1981.495716	20.172813
57.876261	1982.433627	20.177831
58.121288	1985.131680	20.182848
58.255951	1984.735176	20.187866
57.883352	1977.657660	20.192883
58.275810	1969.173416	20.197901
58.092890	1973.733816	20.202919
58.303334	1977.617569	20.207936
57.999545	1980.426317	20.212954
58.433002	1998.114082	20.217971
58.822661	2006.347209	20.222989
58.242523	2012.661041	20.228007
58.431973	2006.373355	20.233024
58.435520	2015.954220	20.238042
58.274823	2006.423103	20.243059
58.656500	2009.027298	20.248077
58.417074	2007.098449	20.253095
58.447805	2016.182757	20.258112
58.230741	2023.828674	20.263130
58.773912	2023.681004	20.268147
59.221471	2033.691385	20.273165
59.117099	2036.355480	20.278183
59.270929	2029.480016	20.283200
59.267271	2026.321514	20.288218
58.991200	2034.188070	20.293235
59.492447	2019.128837	20.298253
59.360016	2024.038009	20.303271
59.490889	2027.160958	20.308288
59.392678	2032.254161	20.313306
59.509570	2042.817824	20.318323
59.753079	2042.997687	20.323341
59.738866	2059.451812	20.328359
59.668144	2053.390817	20.333376
60.037215	2057.268825	20.338394
59.768078	2056.184075	20.343411
60.214476	2054.839592	20.348429
59.938714	2052.039044	20.353447
59.934514	2054.239402	20.358464
60.272046	2049.153149	20.363482
60.089447	2052.855105	20.368499
60.349933	2048.797058	20.373517
60.027524	2054.420656	20.378535
60.271235	2050.564045	20.383552
60.116146	2059.528977	20.388570
60.016274	2054.261505	20.393587
59.798657	2047.832046	20.398605
60.062906	2065.748203	20.403623
60.560856	2071.184118	20.408640
60.562631	2079.392459	20.413658
60.397528	2082.731920	20.418675
60.906933	2074.024282	20.423693
60.754525	2081.259353	20.428711
60.758756	2087.122451	20.433728
60.833880	2103.408066	20.438746
61.238822	2108.448200	20.443763
60.925914	2096.561150	20.448781
60.882816	2104.729150	20.453799
60.822446	2096.561513	20.458816
60.906146	2093.771267	20.463834
60.878456	2102.975173	20.468851
61.440570	2113.056131	20.473869
61.478708	2122.079377	20.478887
61.551324	2116.658792	20.483904
61.805971	2110.174718	20.488922
61.673166	2112.407730	20.493939
61.676768	2118.245689	20.498957
61.681934	2116.890999	20.503975
61.853321	2110.606089	20.508992
62.178241	2112.367031	20.514010
62.234518	2121.668331	20.519027
62.092716	2120.090360	20.524045
61.804635	2122.041422	20.529063
62.117427	2119.196568	20.534080
62.538468	2123.470461	20.539098
62.273869	2117.363886	20.544115
62.263494	2112.246572	20.549133
62.444322	2133.255989	20.554151
62.473176	2126.428350	20.559168
62.565115	2128.967215	20.564186
62.580363	2136.523359	20.569203
63.109573	2117.505284	20.574221
63.298775	2129.679897	20.579239
63.272334	2123.343728	20.584256
63.442879	2106.988319	20.589274
62.988883	2107.907970	20.594291
63.057996	2107.998217	20.599309
62.605046	2108.324387	20.604327
62.470273	2099.742279	20.609344
62.913905	2115.273067	20.614362
62.696516	2123.774339	20.619379
63.107961	2129.283703	20.624397
63.102355	2133.440979	20.629415
63.231188	2138.085433	20.634432
63.225141	2132.863292	20.639450
63.488529	2144.174259	20.644467
63.430002	2146.856480	20.649485
63.586407	2156.640850	20.654503
63.475832	2151.397106	20.659520
63.620183	2151.942720	20.664538
63.666311	2149.903121	20.669555
63.814917	2141.936467	20.674573
64.022421	2146.795903	20.679591
63.827059	2149.079687	20.684608
64.011870	2144.168670	20.689626
64.050736	2151.522319	20.694643
64.217317	2152.929203	20.699661
64.482830	2174.316822	20.704679
64.772416	2172.999901	20.709696
64.469117	2163.049068	20.714714
64.149456	2157.818941	20.719731
64.400505	2163.454279	20.724749
64.151635	2171.632255	20.729767
63.933840	2175.809954	20.734784
64.069291	2176.625211	20.739802
64.251355	2185.547181	20.744819
64.657166	2193.140376	20.749837
65.021252	2189.905654	20.754855
64.661039	2203.993160	20.759872
65.156832	2194.526997	20.764890
64.926897	2196.901381	20.769907
65.300407	2189.142699	20.774925
65.208060	2197.681345	20.779943
65.108374	2196.096809	20.784960
65.669026	2196.729095	20.789978
65.202568	2215.077921	20.794995
65.496782	2207.713449	20.800013
65.558203	2214.211501	20.805031
65.866978	2220.696292	20.810048
65.943948	2216.619441	20.815066
65.516616	2213.369071	20.820083
66.180621	2206.758108	20.825101
66.139108	2203.201505	20.830119
66.033640	2208.049723	20.835136
65.930462	2215.586467	20.840154
65.859824	2210.207094	20.845171
66.204821	2204.750387	20.850189
65.683196	2208.369453	20.855207
65.848470	2216.454566	20.860224
66.129221	2217.206175	20.865242
66.375243	2230.334580	20.870259
66.035933	2232.113740	20.875277
66.523932	2233.966075	20.880295
66.180120	2236.197239	20.885312
66.652228	2229.641393	20.890330
66.498972	2233.218890	20.895347
66.691766	2241.422813	20.900365
67.142926	2256.883121	20.905383
66.926539	2249.260440	20.910400
67.125006	2256.166383	20.915418
67.219695	2260.263889	20.920435
67.514748	2257.642694	20.925453
67.368695	2249.807080	20.930471
67.492857	2248.405450	20.935488
67.815949	2246.786646	20.940506
67.608778	2239.115195	20.945523
67.943855	2237.898489	20.950541
67.889873	2231.058459	20.955559
67.615514	2223.078723	20.960576
67.478670	2219.701070	20.965594
67.831711	2233.008485	20.970611
67.609094	2233.140997	20.975629
67.827327	2229.591287	20.980647
67.926814	2229.866163	20.985664
68.262162	2231.956871	20.990682
68.354360	2234.625106	20.995699
68.556848	2238.194557	21.000717
68.543860	2234.668222	21.005735
68.145186	2236.301983	21.010752
68.273510	2231.068360	21.015770
67.946095	2235.774407	21.020787
68.182926	2230.517579	21.025805
68.360169	2228.779465	21.030823
68.627525	2234.093534	21.035840
68.541480	2233.658800	21.040858
68.622036	2228.183294	21.045875
68.389767	2229.232539	21.050893
68.653278	2257.415369	21.055911
68.676087	2261.609279	21.060928
68.933780	2262.948335	21.065946
68.767019	2258.259291	21.070963
68.731986	2255.850443	21.075981
68.908908	2255.396858	21.080999
69.249869	2272.988839	21.086016
69.474979	2280.275671	21.091034
69.301286	2279.614728	21.096051
69.463435	2286.046628	21.101069
69.381879	2285.611194	21.106087
69.766962	2279.097282	21.111104
69.998300	2266.017635	21.116122
70.268263	2257.571263	21.121139
70.291088	2263.229542	21.126157
70.005807	2261.266776	21.131175
70.014717	2273.804092	21.136192
69.825227	2265.826903	21.141210
69.856246	2258.948380	21.146227
70.139916	2262.208534	21.151245
70.061292	2265.742859	21.156263
70.238400	2276.893765	21.161280
70.516972	2274.745374	21.166298
70.629573	2282.788223	21.171315
70.759791	2294.719655	21.176333
70.814440	2289.964571	21.181351
70.404594	2292.767787	21.186368
70.476241	2294.852219	21.191386
70.689098	2293.723971	21.196403
70.987066	2289.555887	21.201421
71.151913	2281.403596	21.206439
70.721822	2286.854673	21.211456
71.069375	2283.998069	21.216474
70.923043	2284.412210	21.221491
71.104950	2294.517751	21.226509
71.481031	2296.393830	21.231527
71.317886	2317.605350	21.236544
71.366448	2313.479248	21.241562
71.468117	2314.312395	21.246579
71.525508	2315.404914	21.251597
71.419019	2307.108654	21.256615
71.036986	2309.229006	21.261632
71.592860	2317.953980	21.266650
71.678197	2330.712979	21.271667
71.352654	2337.435436	21.276685
71.654088	2339.594556	21.281703
71.482847	2355.618939	21.286720
71.871817	2361.220242	21.291738
72.143104	2364.027881	21.296755
72.218719	2365.657241	21.301773
72.087315	2366.144803	21.306791
72.413023	2365.295643	21.311808
72.396959	2361.507815	21.316826
72.832118	2356.403119	21.321843
72.496255	2358.106011	21.326861
72.838334	2358.510387	21.331879
72.924025	2375.050239	21.336896
73.051793	2370.933884	21.341914
73.304663	2380.005883	21.346931
72.853258	2374.414328	21.351949
73.079422	2372.119442	21.356967
73.344156	2381.407358	21.361984
73.299331	2375.919768	21.367002
73.057551	2375.881685	21.372019
73.052733	2370.981194	21.377037
73.131581	2369.993733	21.382055
73.066683	2378.998435	21.387072
73.002116	2378.361525	21.392090
73.372753	2391.559015	21.397107
73.520551	2401.045040	21.402125
73.616983	2402.519674	21.407143
73.927430	2404.832043	21.412160
74.142554	2407.301273	21.417178
73.969876	2388.354318	21.422195
74.128343	2405.365736	21.427213
74.216430	2395.095045	21.432231
74.014604	2403.016479	21.437248
74.076979	2416.804813	21.442266
74.425033	2415.096896	21.447283
74.387901	2420.092331	21.452301
74.621676	2417.543774	21.457319
74.470705	2432.788694	21.462336
74.453661	2423.048784	21.467354
75.153402	2422.422271	21.472371
75.184088	2419.416153	21.477389
75.235740	2420.017236	21.482407
74.723505	2418.702052	21.487424
75.310642	2417.089463	21.492442
74.912937	2420.178004	21.497459
75.067424	2425.055239	21.502477
75.246565	2438.134246	21.507495
75.099758	2439.062893	21.512512
75.246942	2439.090490	21.517530
75.199376	2439.725958	21.522547
75.296604	2447.518794	21.527565
75.485469	2444.144039	21.532583
75.440423	2459.621815	21.537600
75.596031	2460.332954	21.542618
75.940876	2457.779722	21.547635
76.014870	2463.082937	21.552653
75.754936	2458.727104	21.557671
75.841818	2469.895333	21.562688
75.798458	2477.511243	21.567706
76.114937	2483.802414	21.572723
76.245235	2485.104513	21.577741
76.175340	2489.562234	21.582759
76.410067	2490.245276	21.587776
76.259899	2486.992731	21.592794
76.366159	2492.543412	21.597811
76.711591	2504.214243	21.602829
77.038169	2514.467809	21.607847
76.975771	2515.904060	21.612864
76.847360	2519.805973	21.617882
77.101084	2504.302001	21.622899
76.935679	2526.176882	21.627917
77.089733	2507.762795	21.632935
77.089037	2512.790456	21.637952
77.200320	2510.434537	21.642970
77.624101	2508.440248	21.647987
77.356640	2524.050544	21.653005
77.743769	2522.882524	21.658023
77.709482	2532.021401	21.663040
77.961988	2540.336094	21.668058
77.910329	2532.693957	21.673075
77.748533	2535.161924	21.678093
77.782881	2528.468985	21.683111
78.137934	2533.087789	21.688128
78.153668	2529.626357	21.693146
78.057067	2534.473282	21.698163
78.271157	2526.193284	21.703181
77.972580	2520.650477	21.708199
77.955403	2518.873173	21.713216
77.749305	2527.634828	21.718234
78.093331	2536.134099	21.723251
78.137399	2550.622868	21.728269
78.579097	2556.411697	21.733287
78.747357	2559.831896	21.738304
78.423056	2571.957363	21.743322
79.223281	2572.858499	21.748339
78.923596	2572.308686	21.753357
79.020245	2575.064647	21.758375
79.076550	2577.265118	21.763392
79.246158	2569.437026	21.768410
79.249260	2568.363510	21.773427
79.001936	2577.690225	21.778445
79.115544	2576.672092	21.783463
79.125419	2594.978703	21.788480
79.187386	2593.766624	21.793498
79.728576	2585.299963	21.798515
80.021053	2593.640017	21.803533
80.428561	2579.305017	21.808551
80.112517	2582.608106	21.813568
80.200636	2590.023699	21.818586
80.362000	2585.002596	21.823603
80.496804	2587.777868	21.828621
80.523296	2579.691167	21.833639
80.654952	2584.057567	21.838656
80.343123	2582.136770	21.843674
80.517873	2589.469443	21.848691
80.998476	2601.911456	21.853709
80.828461	2605.848269	21.858727
80.995930	2611.708216	21.863744
80.984886	2610.706333	21.868762
81.135417	2609.821315	21.873779
81.214734	2617.096268	21.878797
81.298845	2613.075024	21.883815
81.285491	2607.711861	21.888832
81.257097	2602.925439	21.893850
81.167512	2591.599779	21.898867
81.113630	2598.876526	21.903885
81.288079	2599.758320	21.908903
81.570684	2602.832498	21.913920
81.301470	2608.896142	21.918938
81.786661	2617.297728	21.923955
81.620167	2632.147574	21.928973
81.772433	2630.574269	21.933991
81.874637	2628.421735	21.939008
81.196015	2630.806068	21.944026
81.925709	2637.670479	21.949043
81.663804	2648.782662	21.954061
82.180412	2658.921512	21.959079
82.543754	2654.247668	21.964096
82.296306	2661.033830	21.969114
82.424440	2646.148938	21.974131
82.677937	2657.625884	21.979149
83.017134	2665.112879	21.984167
83.298019	2668.638650	21.989184
83.405475	2667.529945	21.994202
82.874894	2650.270112	21.999219
82.799635	2648.987868	22.004237
82.709625	2664.592751	22.009255
82.976433	2668.051281	22.014272
83.002992	2678.004487	22.019290
83.454927	2674.033267	22.024307
83.168040	2658.565991	22.029325
83.350843	2669.466927	22.034343
83.351225	2684.738993	22.039360
83.557921	2693.395431	22.044378
83.871994	2691.910546	22.049395
83.901625	2701.064806	22.054413
83.776974	2700.430927	22.059431
83.870151	2699.444373	22.064448
83.681427	2693.969622	22.069466
83.779377	2696.053162	22.074483
84.086398	2713.161672	22.079501
84.289009	2714.168485	22.084519
84.451313	2716.895310	22.089536
84.527030	2711.704455	22.094554
84.737175	2712.183034	22.099571
84.822106	2705.668361	22.104589
84.745063	2704.746181	22.109607
84.988434	2706.548284	22.114624
84.514354	2716.532117	22.119642
85.106560	2730.285543	22.124659
85.336496	2729.239822	22.129677
85.168993	2730.922847	22.134695
85.175146	2729.949841	22.139712
85.313174	2733.336908	22.144730
85.440704	2729.927465	22.149747
85.319011	2734.279694	22.154765
84.983059	2738.681062	22.159783
85.708865	2748.433913	22.164800
85.672016	2758.845197	22.169818
85.659858	2753.014707	22.174835
85.764692	2763.138824	22.179853
85.674044	2765.478972	22.184871
86.125898	2776.221310	22.189888
86.584288	2776.033184	22.194906
86.855992	2775.482772	22.199923
86.912699	2783.723912	22.204941
86.770176	2767.729095	22.209959
86.583622	2758.977993	22.214976
86.653668	2776.035089	22.219994
87.065513	2766.524888	22.225011
86.770848	2779.857809	22.230029
87.175831	2780.009385	22.235047
86.769216	2766.444827	22.240064
86.949677	2774.982302	22.245082
87.063214	2767.061860	22.250099
86.959663	2764.417438	22.255117
86.921441	2786.342269	22.260135
87.199150	2794.520601	22.265152
87.258799	2795.597017	22.270170
87.354078	2803.668046	22.275187
87.627937	2791.111617	22.280205
87.739724	2807.430036	22.285223
88.278963	2817.666447	22.290240
87.790310	2828.558403	22.295258
88.112555	2812.664768	22.300275
88.401327	2817.751596	22.305293
88.480406	2818.026503	22.310311
88.460066	2815.517454	22.315328
88.071392	2828.498943	22.320346
88.343130	2818.262539	22.325363
88.327271	2813.205843	22.330381
88.180596	2820.052122	22.335399
88.887800	2830.256077	22.340416
88.572815	2842.102540	22.345434
89.040659	2837.128332	22.350451
89.275182	2838.464728	22.355469
89.321015	2846.221555	22.360487
89.175391	2837.492447	22.365504
89.180604	2843.958450	22.370522
88.852027	2842.791379	22.375539
88.919988	2843.494087	22.380557
89.170695	2852.232119	22.385575
89.517487	2862.725756	22.390592
89.320838	2857.267969	22.395610
89.323596	2863.724893	22.400627
89.510943	2856.998542	22.405645
89.476101	2876.865194	22.410663
89.840207	2874.753913	22.415680
89.797548	2884.168852	22.420698
89.630724	2886.625026	22.425715
89.936231	2891.813420	22.430733
90.008597	2907.225959	22.435751
90.287722	2905.954801	22.440768
90.213930	2906.010491	22.445786
90.533806	2917.527767	22.450803
91.243087	2928.084936	22.455821
90.802751	2933.411558	22.460839
91.121769	2929.113807	22.465856
91.182994	2933.882613	22.470874
91.204020	2930.104671	22.475891
91.974854	2930.454932	22.480909
91.562310	2924.664631	22.485927
91.596124	2920.111458	22.490944
91.320561	2925.374550	22.495962
91.626928	2915.593489	22.500979
91.420089	2918.535622	22.505997
91.338486	2933.142105	22.511015
91.734985	2934.674216	22.516032
91.686535	2949.041999	22.521050
91.657780	2955.450209	22.526067
91.838360	2954.352194	22.531085
91.763007	2966.293986	22.536103
92.479618	2968.401168	22.541120
92.477597	2982.493481	22.546138
92.368227	2976.728551	22.551155
92.696754	2980.145972	22.556173
92.768204	2972.591787	22.561191
93.069900	2971.301329	22.566208
93.177827	2963.274367	22.571226
93.108842	2974.880628	22.576243
93.445388	2970.387616	22.581261
93.120559	2979.669795	22.586279
93.237152	2991.944671	22.591296
93.384276	3001.099728	22.596314
93.350273	2997.049446	22.601331
93.633477	2997.251546	22.606349
93.500869	3006.958291	22.611367
93.610202	2992.060259	22.616384
93.132197	3003.862776	22.621402
93.435792	3012.460095	22.626419
93.543829	3015.119669	22.631437
93.832052	3030.940562	22.636455
94.141958	3024.993562	22.641472
94.174294	3038.793364	22.646490
94.376220	3049.315977	22.651507
94.545527	3051.098086	22.656525
94.220042	3047.576060	22.661543
94.819578	3051.863417	22.666560
94.539656	3053.431417	22.671578
94.551551	3056.797154	22.676595
94.964462	3066.355875	22.681613
94.781029	3079.141472	22.686631
94.816252	3078.615245	22.691648
94.943697	3080.732111	22.696666
95.109810	3081.204931	22.701683
95.211587	3075.646961	22.706701
95.622718	3081.926762	22.711719
95.540884	3084.161427	22.716736
95.456858	3097.196673	22.721754
95.339947	3086.840728	22.726771
96.097924	3088.348134	22.731789
95.978169	3095.439659	22.736807
95.859602	3095.022591	22.741824
96.043911	3103.578560	22.746842
96.070887	3111.205880	22.751859
96.677836	3112.651587	22.756877
96.358644	3114.926366	22.761895
96.332851	3111.774275	22.766912
96.927327	3110.798022	22.771930
97.004651	3115.232977	22.776947
97.211961	3110.930483	22.781965
96.896130	3119.311838	22.786983
96.798509	3109.928118	22.792000
96.879149	3113.504091	22.797018
96.894001	3127.846381	22.802035
97.115081	3126.581088	22.807053
97.065405	3140.191744	22.812071
97.440158	3141.619951	22.817088
97.334029	3139.417733	22.822106
97.358265	3150.813913	22.827123
97.811973	3156.623161	22.832141
97.940119	3157.341761	22.837159
97.929191	3165.940781	22.842176
98.021727	3167.106784	22.847194
97.949969	3159.451729	22.852211
98.095846	3170.254566	22.857229
97.609965	3192.227495	22.862247
98.195674	3185.274881	22.867264
98.323848	3192.993788	22.872282
98.474842	3207.889362	22.877299
98.676167	3215.132937	22.882317
98.608833	3217.447420	22.887335
98.829952	3201.780649	22.892352
98.951577	3214.903895	22.897370
98.690635	3228.320269	22.902387
99.518008	3223.207920	22.907405
99.434218	3230.849380	22.912423
99.501023	3229.595475	22.917440
99.899954	3227.150493	22.922458
99.726270	3232.189506	22.927475
99.854931	3228.461023	22.932493
100.052461	3224.267333	22.937511
99.765697	3229.456510	22.942528
100.130551	3230.592743	22.947546
100.372922	3250.688076	22.952563
100.712566	3251.143352	22.957581
100.485360	3246.905321	22.962599
100.465409	3253.451136	22.967616
100.240866	3255.218838	22.972634
99.861494	3251.686224	22.977651
100.577745	3264.840017	22.982669
100.530937	3277.629732	22.987687
100.668522	3277.437895	22.992704
101.126423	3277.227750	22.997722
101.033851	3283.829069	23.002739
100.934983	3280.571548	23.007757
101.092111	3290.899284	23.012775
101.470261	3295.385288	23.017792
101.408010	3302.925584	23.022810
101.433284	3303.054224	23.027827
101.773823	3298.301705	23.032845
101.943180	3296.788805	23.037863
102.073805	3310.731320	23.042880
102.179703	3315.111377	23.047898
102.121493	3327.827155	23.052915
102.463022	3327.085955	23.057933
102.140307	3324.412450	23.062951
102.396209	3321.724607	23.067968
102.278831	3318.065973	23.072986
102.112975	3326.689191	23.078003
102.588314	3329.884983	23.083021
103.039231	3345.791289	23.088039
102.565919	3344.526784	23.093056
102.632616	3346.697325	23.098074
102.549676	3351.782211	23.103091
102.827153	3364.319504	23.108109
103.349962	3375.429895	23.113127
103.607545	3373.874847	23.118144
103.894965	3359.687328	23.123162
103.884389	3356.678009	23.128179
103.970467	3350.024052	23.133197
104.255812	3351.535632	23.138215
104.266608	3349.615020	23.143232
104.522174	3344.399138	23.148250
104.438425	3349.174845	23.153267
104.521848	3348.044591	23.158285
104.591300	3343.851878	23.163303
104.447943	3360.074808	23.168320
104.627738	3357.364091	23.173338
104.756039	3374.033945	23.178355
104.620862	3374.323282	23.183373
104.809906	3376.206504	23.188391
105.070994	3368.073456	23.193408
105.010726	3373.142193	23.198426
105.112531	3393.411066	23.203443
105.156150	3392.773057	23.208461
105.451703	3397.606501	23.213479
105.480448	3401.272672	23.218496
105.479191	3395.875828	23.223514
105.479240	3413.525163	23.228531
105.646624	3418.744684	23.233549
105.706552	3429.538966	23.238567
105.829907	3426.594000	23.243584
105.791063	3431.151273	23.248602
106.039279	3450.261191	23.253619
106.232549	3453.747104	23.258637
106.041637	3448.540738	23.263655
106.391835	3462.120942	23.268672
106.614508	3472.874131	23.273690
106.749904	3467.657986	23.278707
106.764020	3471.500038	23.283725
106.724313	3473.721880	23.288743
106.831600	3491.796461	23.293760
107.166987	3488.386075	23.298778
107.280420	3503.148869	23.303795
107.626197	3498.206111	23.308813
107.269368	3497.027613	23.313831
107.825145	3510.651595	23.318848
108.008511	3514.489399	23.323866
108.130889	3519.703332	23.328883
108.387792	3525.934709	23.333901
108.248162	3528.497203	23.338919
108.044716	3525.473697	23.343936
108.454723	3517.165899	23.348954
108.107991	3520.808492	23.353971
108.257053	3516.489721	23.358989
108.580182	3527.123147	23.364007
108.658484	3546.931892	23.369024
108.642957	3545.482474	23.374042
108.845933	3543.673949	23.379059
109.041188	3547.042792	23.384077
109.105184	3549.702990	23.389095
108.916842	3547.904890	23.394112
109.101019	3559.743545	23.399130
109.318100	3575.913708	23.404147
109.378654	3582.036802	23.409165
109.681781	3576.441017	23.414183
109.463495	3583.636447	23.419200
109.806428	3591.445181	23.424218
109.945294	3594.049542	23.429235
110.111772	3592.963153	23.434253
110.064552	3594.384503	23.439271
109.724668	3601.005505	23.444288
110.569556	3610.566698	23.449306
110.657808	3613.469313	23.454323
110.459334	3618.247172	23.459341
110.873278	3622.816059	23.464359
110.873981	3619.056918	23.469376
111.561831	3636.706697	23.474394
111.512697	3653.076188	23.479411
111.580455	3637.521290	23.484429
111.710048	3635.152907	23.489447
111.314840	3639.724685	23.494464
111.879286	3633.681045	23.499482
111.609527	3637.327458	23.504499
112.072071	3641.570006	23.509517
112.008287	3634.421658	23.514535
111.294463	3640.277122	23.519552
112.051717	3645.499558	23.524570
112.111894	3662.215003	23.529587
111.937637	3665.811834	23.534605
112.547213	3665.953661	23.539623
112.184111	3667.894473	23.544640
112.542422	3680.239497	23.549658
112.801821	3687.906623	23.554675
112.874362	3686.951635	23.559693
113.155663	3682.037803	23.564711
112.941346	3690.053276	23.569728
113.510395	3695.557526	23.574746
113.620992	3705.949557	23.579763
113.335161	3711.583753	23.584781
113.603664	3700.832889	23.589799
113.236868	3705.239292	23.594816
113.576711	3714.538300	23.599834
113.886508	3733.036091	23.604851
113.706790	3739.853143	23.609869
114.023876	3724.956880	23.614887
114.488036	3736.669997	23.619904
114.201126	3749.377491	23.624922
114.687207	3755.099832	23.629939
114.704148	3754.791057	23.634957
115.108303	3753.724467	23.639975
114.751427	3748.120918	23.644992
115.011291	3750.375058	23.650010
114.933032	3756.564011	23.655027
114.921746	3775.714676	23.660045
115.123215	3778.429254	23.665063
115.321406	3781.071749	23.670080
115.647445	3783.558621	23.675098
115.527385	3792.304337	23.680115
115.439306	3793.328064	23.685133
115.924569	3800.477168	23.690151
115.840885	3808.535480	23.695168
116.092132	3805.144448	23.700186
116.058862	3796.413163	23.705203
116.271452	3816.021389	23.710221
116.797622	3819.629137	23.715239
116.519374	3831.899779	23.720256
116.773422	3825.475152	23.725274
117.070759	3823.569846	23.730291
117.150393	3823.399652	23.735309
117.493449	3814.524548	23.740327
117.008380	3823.658514	23.745344
117.334453	3819.665611	23.750362
117.632381	3817.009027	23.755379
117.642133	3813.971217	23.760397
117.494160	3814.814896	23.765415
117.530295	3826.585243	23.770432
118.305766	3836.693928	23.775450
117.653943	3838.465084	23.780467
118.205702	3840.086728	23.785485
118.005316	3834.556631	23.790503
118.143766	3848.911813	23.795520
118.262908	3864.030670	23.800538
118.554001	3862.429332	23.805555
118.249370	3877.636273	23.810573
118.892836	3856.013605	23.815591
119.249586	3855.683484	23.820608
119.424444	3851.111273	23.825626
119.694107	3847.679491	23.830643
119.503657	3848.791753	23.835661
119.624947	3843.580853	23.840679
119.709375	3862.479990	23.845696
119.874230	3869.789476	23.850714
119.985271	3867.111481	23.855731
120.056616	3871.547554	23.860749
120.191472	3868.714351	23.865767
119.711211	3871.639239	23.870784
119.682548	3874.007754	23.875802
120.087811	3881.437628	23.880819
120.105732	3885.370708	23.885837
120.556894	3885.474077	23.890855
120.550269	3902.787210	23.895872
120.602851	3914.169990	23.900890
120.973033	3919.058238	23.905907
121.283469	3927.749619	23.910925
121.027387	3920.694222	23.915943
121.017681	3927.917284	23.920960
121.265666	3939.405377	23.925978
121.251794	3939.776837	23.930995
121.430735	3942.226664	23.936013
121.871481	3938.146444	23.941031
121.849303	3955.345267	23.946048
121.691283	3959.810759	23.951066
121.813851	3957.604397	23.956083
121.893842	3973.404883	23.961101
122.251763	3983.360877	23.966119
122.432930	3985.422141	23.971136
122.440461	3993.456865	23.976154
122.610249	3994.326830	23.981171
122.433098	4008.396710	23.986189
122.466645	4007.596121	23.991207
122.780511	4024.401812	23.996224
122.691484	4028.168509	24.001242
123.462300	4031.378395	24.006259
123.524394	4030.153575	24.011277
123.611661	4017.502251	24.016295
123.803452	4038.950914	24.021312
123.790127	4046.354495	24.026330
123.900818	4044.168909	24.031347
124.137547	4057.858762	24.036365
124.362886	4047.070224	24.041383
124.573581	4054.663027	24.046400
124.743171	4061.706725	24.051418
124.949376	4076.143072	24.056435
124.934339	4081.624753	24.061453
124.772804	4066.382939	24.066471
124.807305	4075.650766	24.071488
124.781961	4070.737227	24.076506
124.748067	4071.376935	24.081523
124.598014	4086.206479	24.086541
125.341972	4083.268942	24.091559
125.249609	4103.758221	24.096576
125.262296	4108.749524	24.101594
125.588921	4125.067252	24.106611
125.538569	4128.682759	24.111629
125.986616	4124.778114	24.116647
125.860886	4147.630394	24.121664
126.281112	4151.466177	24.126682
126.346504	4149.420196	24.131699
126.192563	4167.318340	24.136717
126.812150	4173.619728	24.141735
126.686473	4176.265361	24.146752
127.001136	4180.155461	24.151770
126.898978	4183.665418	24.156787
127.054229	4194.369564	24.161805
127.383927	4198.131075	24.166823
127.677323	4198.795583	24.171840
127.856716	4209.120379	24.176858
127.891380	4208.439547	24.181875
127.258240	4213.840748	24.186893
127.650061	4218.889837	24.191911
127.784112	4234.786293	24.196928
127.964647	4233.416766	24.201946
128.178441	4230.757440	24.206963
128.745905	4245.724752	24.211981
128.941069	4247.607114	24.216999
129.151466	4250.673882	24.222016
129.238999	4251.824953	24.227034
129.603026	4242.539210	24.232051
129.481378	4245.247352	24.237069
129.795156	4238.942689	24.242087
129.647867	4240.537484	24.247104
129.600158	4246.993292	24.252122
129.938737	4236.209106	24.257139
129.442293	4249.852280	24.262157
130.149443	4261.543691	24.267175
130.308334	4268.181970	24.272192
130.199045	4272.475823	24.277210
130.212841	4273.540530	24.282227
130.163484	4278.371098	24.287245
130.426564	4283.860040	24.292263
130.240657	4292.117549	24.297280
130.357322	4300.659369	24.302298
130.450997	4304.069420	24.307315
131.005918	4319.969865	24.312333
131.184428	4326.721895	24.317351
131.229865	4328.876928	24.322368
130.861981	4344.160390	24.327386
131.395471	4347.322062	24.332403
131.270239	4361.901773	24.337421
131.837395	4358.041661	24.342439
131.914679	4373.063302	24.347456
132.121612	4377.718271	24.352474
132.336307	4372.410611	24.357491
132.262793	4392.193418	24.362509
132.184714	4395.229371	24.367527
132.627817	4393.755826	24.372544
132.740669	4395.385885	24.377562
132.951074	4408.710810	24.382579
132.805838	4418.385557	24.387597
132.885109	4422.804750	24.392615
133.391313	4427.725617	24.397632
133.381078	4422.746503	24.402650
133.558743	4425.846804	24.407667
133.569426	4441.478577	24.412685
133.793775	4442.314819	24.417703
134.064412	4440.612457	24.422720
133.943208	4441.142673	24.427738
134.316907	4439.477924	24.432755
134.374138	4455.471756	24.437773
134.810889	4453.882410	24.442791
135.339601	4448.443773	24.447808
134.978644	4460.550960	24.452826
135.405978	4457.053484	24.457843
135.531904	4451.999505	24.462861
135.502538	4446.786636	24.467879
135.483863	4452.698260	24.472896
135.269183	4452.409752	24.477914
135.724966	4446.979313	24.482931
135.483494	4451.726209	24.487949
135.767895	4468.694719	24.492967
135.962709	4471.290496	24.497984
135.974932	4475.716984	24.503002
136.134105	4477.522909	24.508019
136.417312	4494.955614	24.513037
136.158098	4502.893214	24.518055
136.292822	4502.913288	24.523072
136.212158	4518.171116	24.528090
136.409512	4516.757918	24.533107
136.707670	4541.716280	24.538125
136.811479	4550.528511	24.543143
137.332128	4552.246601	24.548160
137.060660	4568.007634	24.553178
137.140290	4582.833388	24.558195
137.235994	4583.260397	24.563213
137.202500	4593.789002	24.568231
137.759907	4609.676690	24.573248
138.030865	4615.896788	24.578266
138.575351	4621.916484	24.583283
138.691965	4628.432066	24.588301
138.757627	4632.698766	24.593319
139.354764	4622.603221	24.598336
139.371609	4618.213238	24.603354
139.610570	4619.994129	24.608371
139.539505	4614.342654	24.613389
139.255167	4625.683646	24.618407
139.904341	4615.883017	24.623424
139.761619	4621.375271	24.628442
139.847713	4616.431609	24.633459
139.935048	4627.399097	24.638477
140.106917	4644.669367	24.643495
139.910441	4640.041141	24.648512
140.370683	4653.516732	24.653530
140.416520	4636.484042	24.658547
140.548789	4655.319743	24.663565
140.931025	4659.919085	24.668583
141.180339	4667.304124	24.673600
141.003837	4672.129341	24.678618
140.962585	4664.380518	24.683635
141.231293	4666.983758	24.688653
141.119063	4671.372855	24.693671
141.390561	4684.221324	24.698688
141.137905	4695.282820	24.703706
141.314063	4702.054296	24.708723
141.259359	4706.238748	24.713741
141.596322	4713.913174	24.718759
142.089644	4738.229080	24.723776
141.878423	4742.983967	24.728794
141.756506	4747.926962	24.733811
142.017118	4759.451488	24.738829
142.389520	4772.817744	24.743847
142.546529	4772.547115	24.748864
142.915035	4788.145573	24.753882
143.201960	4796.878911	24.758899
143.350936	4792.572477	24.763917
143.258269	4799.751987	24.768935
143.621837	4803.413659	24.773952
144.199260	4797.702197	24.778970
144.202768	4797.101948	24.783987
144.603956	4799.741397	24.789005
144.332891	4790.936180	24.794023
144.571888	4786.884026	24.799040
144.801546	4797.873649	24.804058
144.942970	4810.811901	24.809075
145.260190	4817.990731	24.814093
144.821521	4821.016611	24.819111
145.276063	4814.049080	24.824128
145.334349	4826.230121	24.829146
145.349304	4825.407139	24.834163
145.685000	4828.145168	24.839181
145.497967	4837.129077	24.844199
146.093954	4836.218790	24.849216
145.724463	4840.114545	24.854234
145.813917	4846.422954	24.859251
146.305174	4868.046926	24.864269
146.294275	4876.372145	24.869287
146.450967	4880.804647	24.874304
146.076156	4881.866764	24.879322
146.511574	4899.465547	24.884339
146.740266	4903.410223	24.889357
146.914194	4913.581607	24.894375
147.155911	4922.274698	24.899392
147.380417	4934.164791	24.904410
147.214443	4927.760979	24.909427
147.731833	4955.943227	24.914445
147.562737	4961.559634	24.919463
147.787387	4966.104678	24.924480
147.826309	4975.949907	24.929498
148.087719	4983.970795	24.934515
148.381777	4993.640583	24.939533
148.353532	4991.741657	24.944551
149.012540	5002.759252	24.949568
149.203229	5007.858817	24.954586
149.515667	5005.367095	24.959603
149.197913	5006.085751	24.964621
149.027982	5019.356708	24.969639
149.209998	5022.125006	24.974656
149.481047	5034.184680	24.979674
149.550851	5034.025475	24.984691
149.975672	5049.735336	24.989709
149.780043	5065.851142	24.994727
150.156559	5057.759340	24.999744
150.141510	5072.243555	25.004762
150.574473	5080.013667	25.009779
150.447542	5071.873982	25.014797
150.433950	5083.229923	25.019815
150.866332	5098.152688	25.024832
150.852331	5112.466322	25.029850
151.016314	5108.956064	25.034867
151.232788	5125.370756	25.039885
151.608603	5132.802576	25.044903
151.847460	5132.468696	25.049920
152.053171	5146.243114	25.054938
152.553882	5159.902171	25.059955
152.449473	5161.253634	25.064973
152.308529	5165.738858	25.069991
152.606626	5169.909523	25.075008
152.407388	5169.284011	25.080026
152.531894	5173.721596	25.085043
152.933794	5174.972137	25.090061
152.616168	5182.909657	25.095079
153.200407	5190.353242	25.100096
153.316102	5202.790742	25.105114
153.221090	5209.090118	25.110131
153.491700	5221.396191	25.115149
153.657040	5224.801571	25.120167
153.837746	5233.835743	25.125184
153.813393	5253.454008	25.130202
153.709748	5253.062973	25.135219
154.209237	5256.984505	25.140237
154.149480	5269.342045	25.145255
154.556556	5270.086748	25.150272
154.689991	5288.537832	25.155290
154.680554	5302.279578	25.160307
155.058837	5301.794572	25.165325
155.801866	5312.502564	25.170343
155.728463	5311.513396	25.175360
156.009590	5315.841405	25.180378
156.157739	5314.492624	25.185395
156.580483	5312.356155	25.190413
156.263798	5313.907974	25.195431
156.250030	5310.857792	25.200448
156.908981	5321.616757	25.205466
156.857974	5327.167544	25.210483
156.973280	5337.818613	25.215501
156.974196	5333.206825	25.220519
156.900801	5338.404415	25.225536
157.138857	5349.954925	25.230554
157.187091	5363.211104	25.235571
157.771623	5358.975611	25.240589
157.580836	5372.448932	25.245607
157.918674	5395.543103	25.250624
157.797362	5391.127096	25.255642
157.815421	5399.498551	25.260659
158.119697	5407.585553	25.265677
158.179996	5421.095574	25.270695
158.736722	5430.342762	25.275712
158.713571	5444.774873	25.280730
158.873000	5448.032859	25.285747
158.766264	5454.460407	25.290765
158.863961	5476.591449	25.295783
159.258084	5476.741592	25.300800
159.294862	5485.103859	25.305818
159.627474	5496.197825	25.310835
159.693158	5498.725472	25.315853
159.503721	5510.992887	25.320871
159.849717	5511.362012	25.325888
160.485565	5528.781844	25.330906
160.427118	5542.581906	25.335923
160.863717	5532.431942	25.340941
161.060088	5536.031413	25.345959
161.062216	5551.880119	25.350976
161.221258	5557.414056	25.355994
161.407808	5566.965157	25.361011
161.397267	5576.070309	25.366029
161.723586	5587.566192	25.371047
162.133980	5581.921528	25.376064
162.282877	5582.292932	25.381082
162.289012	5594.836140	25.386099
162.351725	5585.767081	25.391117
162.633667	5598.538816	25.396135
162.750728	5600.982721	25.401152
162.920254	5601.379323	25.406170
162.556800	5614.952306	25.411187
163.183356	5621.672942	25.416205
162.867006	5638.145801	25.421223
163.137402	5636.793746	25.426240
163.799753	5648.499346	25.431258
163.625719	5665.887572	25.436275
163.993268	5665.303219	25.441293
163.456848	5673.590671	25.446311
164.236356	5688.624021	25.451328
163.990834	5695.411014	25.456346
163.871893	5702.714920	25.461363
164.726691	5715.400705	25.466381
164.570938	5715.260829	25.471399
164.512691	5728.656959	25.476416
165.229514	5734.956386	25.481434
165.348764	5751.847641	25.486451
165.966625	5756.082295	25.491469
165.762510	5765.609096	25.496487
165.872417	5768.675985	25.501504
166.445725	5773.466825	25.506522
166.109546	5787.878498	25.511539
166.479460	5796.261643	25.516557
166.521821	5798.382607	25.521575
166.650383	5799.647340	25.526592
166.651813	5812.188274	25.531610
166.791902	5820.771355	25.536627
167.134082	5822.810920	25.541645
167.240397	5840.976380	25.546663
167.589773	5842.314062	25.551680
167.816527	5841.202375	25.556698
167.641107	5857.290481	25.561715
168.268861	5869.774978	25.566733
168.291925	5868.565581	25.571751
168.669804	5876.429841	25.576768
169.154877	5882.736991	25.581786
169.192105	5891.061495	25.586803
169.155384	5884.289995	25.591821
169.262652	5888.361116	25.596839
168.934808	5885.877420	25.601856
169.444031	5899.500987	25.606874
169.598551	5908.103958	25.611891
169.866368	5911.499827	25.616909
170.493556	5928.981367	25.621927
170.419522	5924.538930	25.626944
170.604621	5931.663013	25.631962
170.358355	5931.792913	25.636979
170.716384	5938.937426	25.641997
170.771653	5950.324221	25.647015
170.791152	5958.171710	25.652032
171.057116	5960.785035	25.657050
171.394666	5972.740280	25.662067
171.632012	5975.907315	25.667085
171.476666	5984.141891	25.672103
171.775281	5994.395480	25.677120
171.822232	5998.248739	25.682138
172.217546	6002.912678	25.687156
172.535705	6027.772113	25.692173
172.623706	6035.299620	25.697191
172.838345	6036.610945	25.702208
173.304093	6034.960134	25.707226
173.194215	6033.537833	25.712244
173.361860	6055.683941	25.717261
173.506691	6060.355326	25.722279
173.187313	6063.384931	25.727296
173.628139	6079.494085	25.732314
173.707005	6096.736021	25.737332
173.854913	6089.692639	25.742349
173.921006	6110.449919	25.747367
173.913832	6117.525095	25.752384
174.341860	6119.017855	25.757402
174.757159	6137.842594	25.762420
174.902371	6144.534196	25.767437
175.378088	6147.339014	25.772455
175.143622	6152.520877	25.777472
175.322609	6154.125016	25.782490
175.625848	6166.909617	25.787508
175.754526	6162.820673	25.792525
175.766048	6161.167966	25.797543
176.214612	6186.837515	25.802560
176.166817	6189.165117	25.807578
175.840404	6200.908218	25.812596
176.145455	6211.353483	25.817613
176.442207	6218.289837	25.822631
176.566250	6242.295921	25.827648
177.241980	6235.040883	25.832666
177.549536	6246.256005	25.837684
178.067367	6253.618825	25.842701
178.716067	6247.169785	25.847719
178.823041	6247.775011	25.852736
179.117230	6245.942551	25.857754
179.165901	6251.920034	25.862772
178.972117	6248.029638	25.867789
179.430042	6249.647178	25.872807
179.173010	6246.259070	25.877824
179.551550	6246.427432	25.882842
179.425350	6246.623870	25.887860
179.321978	6245.446760	25.892877
179.173556	6251.799005	25.897895
179.468777	6266.084342	25.902912
179.575265	6272.583151	25.907930
179.803645	6281.724061	25.912948
180.040904	6291.504398	25.917965
180.394903	6305.032482	25.922983
180.397893	6314.454720	25.928000
180.886083	6321.648566	25.933018
180.260647	6334.391626	25.938036
180.547317	6350.168314	25.943053
180.951873	6377.884204	25.948071
181.205541	6377.096591	25.953088
181.596737	6403.299388	25.958106
181.682371	6412.576229	25.963124
181.586552	6417.253605	25.968141
182.103429	6433.392269	25.973159
181.881161	6443.039045	25.978176
182.718768	6445.134130	25.983194
182.831458	6460.622331	25.988212
182.830507	6461.241210	25.993229
183.064172	6479.501120	25.998247
183.459916	6489.342120	26.003264
183.625645	6482.822983	26.008282
183.562827	6500.860753	26.013300
183.539042	6509.498082	26.018317
183.897878	6522.564695	26.023335
183.962687	6537.555340	26.028352
184.173823	6542.260720	26.033370
184.567213	6558.099891	26.038388
184.699368	6573.379970	26.043405
185.245894	6575.375180	26.048423
184.819382	6593.049820	26.053440
185.105109	6586.553001	26.058458
185.082897	6607.018390	26.063476
185.439175	6620.287501	26.068493
186.021990	6616.452896	26.073511
186.372298	6639.953922	26.078528
186.499047	6648.507902	26.083546
186.767993	6649.908676	26.088564
186.667096	6653.611471	26.093581
187.109975	6644.927799	26.098599
187.130875	6663.239958	26.103616
187.346688	6664.589027	26.108634
187.290874	6667.972289	26.113652
187.308083	6679.333897	26.118669
188.034346	6681.471600	26.123687
188.165311	6695.501896	26.128704
188.234964	6696.100320	26.133722
188.274978	6693.726548	26.138740
188.193488	6714.876830	26.143757
188.747951	6718.345023	26.148775
188.390594	6729.897561	26.153792
188.540854	6742.558015	26.158810
188.948388	6746.813023	26.163828
189.233697	6773.253808	26.168845
189.576092	6778.579636	26.173863
189.597209	6784.479507	26.178880
189.842996	6799.262255	26.183898
189.996117	6805.776091	26.188916
189.902503	6827.856479	26.193933
190.369429	6825.643512	26.198951
190.704388	6841.993953	26.203968
191.001977	6844.949727	26.208986
191.010777	6862.433738	26.214004
191.063107	6868.372971	26.219021
191.521014	6882.065242	26.224039
191.254610	6888.830673	26.229056
191.799247	6905.123271	26.234074
192.227628	6909.842275	26.239092
192.470569	6930.323566	26.244109
192.741232	6929.804768	26.249127
192.770989	6940.031298	26.254144
192.891417	6937.704954	26.259162
193.047224	6950.617232	26.264180
193.066656	6966.091968	26.269197
193.616522	6970.012346	26.274215
193.733671	6994.781278	26.279232
193.704995	6992.446573	26.284250
194.183029	7008.683340	26.289268
194.503930	7020.648179	26.294285
194.597143	7015.847973	26.299303
194.552278	7027.920270	26.304320
194.824383	7046.130566	26.309338
194.879766	7050.244749	26.314356
194.976982	7060.972246	26.319373
195.445584	7067.411803	26.324391
195.480491	7076.109711	26.329408
196.096970	7091.008607	26.334426
196.379869	7099.399588	26.339444
195.948524	7102.516243	26.344461
195.832770	7107.471542	26.349479
196.264775	7123.358857	26.354496
196.532360	7134.782785	26.359514
196.558225	7144.451277	26.364532
196.619237	7170.895988	26.369549
197.334027	7175.513648	26.374567
197.524416	7195.432031	26.379584
198.043900	7201.096604	26.384602
197.825428	7204.397956	26.389620
197.895524	7221.020420	26.394637
197.821304	7229.119808	26.399655
198.116340	7243.194429	26.404672
198.376575	7257.129265	26.409690
198.654185	7269.688179	26.414708
199.136782	7285.596170	26.419725
199.502140	7280.330508	26.424743
199.509449	7289.673653	26.429760
199.747189	7305.174667	26.434778
199.847110	7304.290994	26.439796
199.932274	7316.665236	26.444813
200.498608	7320.422127	26.449831
201.191558	7316.548134	26.454848
201.557222	7303.406073	26.459866
201.681428	7307.866323	26.464884
201.766709	7314.873900	26.469901
202.127218	7300.918175	26.474919
201.501239	7303.054974	26.479936
201.927342	7320.502864	26.484954
202.185005	7329.109388	26.489972
202.106149	7338.349170	26.494989
202.573936	7337.042027	26.500007
202.590743	7360.977880	26.505024
202.715618	7372.446272	26.510042
202.899679	7367.590792	26.515060
202.983753	7384.713169	26.520077
203.090111	7391.499670	26.525095
203.154661	7404.881064	26.530112
203.162878	7422.678229	26.535130
203.730278	7429.456103	26.540148
204.344956	7446.300203	26.545165
204.593404	7439.540554	26.550183
204.851129	7455.733097	26.555200
204.994534	7473.146223	26.560218
205.130154	7464.197473	26.565236
205.793058	7470.174430	26.570253
205.993145	7474.992262	26.575271
206.498383	7485.018793	26.580288
206.234708	7485.643884	26.585306
206.518320	7485.795473	26.590324
206.623007	7492.929528	26.595341
206.515103	7482.815911	26.600359
206.350425	7504.093701	26.605376
206.494360	7512.534918	26.610394
206.999890	7520.484192	26.615412
207.027527	7542.871722	26.620429
207.252209	7543.000916	26.625447
207.373117	7559.202224	26.630464
207.427735	7576.834469	26.635482
207.883539	7593.100472	26.640500
207.504327	7605.073671	26.645517
208.075790	7614.878451	26.650535
208.503277	7641.569847	26.655552
208.267234	7645.972617	26.660570
208.904331	7663.362728	26.665588
208.927836	7690.164444	26.670605
209.341692	7693.844131	26.675623
209.495347	7701.248453	26.680640
210.107576	7715.324565	26.685658
210.433851	7738.205671	26.690676
210.216577	7751.277618	26.695693
210.650047	7757.883893	26.700711
210.604566	7762.197041	26.705728
210.834880	7776.531546	26.710746
211.117561	7775.777243	26.715764
211.507172	7786.664842	26.720781
211.594134	7805.722362	26.725799
212.041978	7816.105274	26.730816
212.193353	7826.790060	26.735834
212.855290	7828.117115	26.740852
212.470657	7843.854386	26.745869
212.767440	7835.439143	26.750887
213.060300	7854.341537	26.755904
213.234047	7860.079085	26.760922
213.529463	7874.725539	26.765940
213.725972	7882.009612	26.770957
213.993258	7894.295907	26.775975
213.960008	7898.749245	26.780992
214.340332	7901.266123	26.786010
214.455135	7912.569102	26.791028
214.493204	7928.215379	26.796045
214.461970	7917.941209	26.801063
214.774667	7935.044289	26.806080
215.137914	7942.618123	26.811098
215.439215	7952.563011	26.816116
215.124231	7972.980793	26.821133
215.300762	7983.636498	26.826151
215.722022	7991.365482	26.831168
215.689083	8007.392247	26.836186
216.157671	8023.164153	26.841204
216.136251	8046.746955	26.846221
216.229987	8051.834054	26.851239
217.245035	8071.631311	26.856256
217.074916	8078.527407	26.861274
217.401990	8092.559808	26.866292
217.847818	8108.073301	26.871309
218.397066	8120.006464	26.876327
218.606948	8123.875845	26.881344
218.582335	8133.306470	26.886362
218.872511	8150.747899	26.891380
218.895175	8159.978600	26.896397
219.085160	8161.707486	26.901415
219.357327	8170.451055	26.906432
219.813814	8182.414485	26.911450
220.054351	8185.098388	26.916468
219.992359	8204.242650	26.921485
220.608855	8203.007007	26.926503
220.513683	8221.329318	26.931520
220.826337	8227.840921	26.936538
221.290239	8220.914849	26.941556
221.504479	8235.116463	26.946573
221.772799	8246.641993	26.951591
221.605490	8257.111456	26.956608
221.752713	8267.771888	26.961626
222.222168	8264.721751	26.966644
222.599087	8277.932024	26.971661
222.733170	8286.630849	26.976679
223.257308	8303.881304	26.981696
223.007715	8305.179831	26.986714
223.281886	8304.363692	26.991732
223.463206	8328.780314	26.996749
223.756462	8336.226298	27.001767
223.569466	8335.144154	27.006784
223.873836	8353.739037	27.011802
224.303582	8364.860666	27.016820
224.631665	8381.608179	27.021837
224.603451	8391.819284	27.026855
224.812489	8412.582168	27.031872
224.906326	8420.254969	27.036890
225.235931	8437.169619	27.041908
225.088395	8455.374032	27.046925
225.363252	8463.890014	27.051943
225.742441	8479.205830	27.056960
226.209124	8493.917668	27.061978
226.614653	8491.218409	27.066996
227.300291	8503.657815	27.072013
227.659247	8508.094438	27.077031
227.645792	8502.694826	27.082048
227.743468	8511.039521	27.087066
228.230555	8522.824771	27.092084
228.547801	8538.150280	27.097101
228.339699	8536.904086	27.102119
228.721096	8541.611887	27.107136
228.670255	8550.216501	27.112154
229.206609	8564.466089	27.117172
229.391219	8564.768856	27.122189
229.379072	8572.158300	27.127207
229.366857	8576.475930	27.132224
228.839590	8587.702489	27.137242
229.278346	8596.660262	27.142260
230.148391	8616.461741	27.147277
229.977227	8625.211406	27.152295
230.814479	8642.135608	27.157312
230.492680	8654.523595	27.162330
230.691773	8666.517942	27.167348
230.928804	8674.528464	27.172365
230.799511	8695.609535	27.177383
231.483338	8711.272751	27.182400
231.778904	8734.450329	27.187418
231.940004	8735.988026	27.192436
232.315344	8757.530466	27.197453
232.256208	8759.402378	27.202471
232.507183	8778.473253	27.207488
232.638559	8794.740315	27.212506
233.019132	8802.611732	27.217524
233.403333	8826.549116	27.222541
233.334534	8841.755025	27.227559
233.824008	8847.083815	27.232576
233.723494	8870.942023	27.237594
234.419169	8889.249212	27.242612
234.771441	8898.308996	27.247629
234.759896	8919.687702	27.252647
235.212429	8918.878498	27.257664
235.524503	8937.295970	27.262682
235.885184	8933.179765	27.267700
236.365919	8953.004332	27.272717
235.946118	8976.716642	27.277735
236.733912	8967.432002	27.282752
236.390188	8997.974008	27.287770
236.918714	9005.882463	27.292788
237.223577	9020.540986	27.297805
237.803224	9027.210205	27.302823
238.028102	9029.590428	27.307840
238.111643	9044.602299	27.312858
238.474564	9049.710908	27.317876
238.555030	9069.162230	27.322893
238.575702	9079.388204	27.327911
239.024990	9087.226944	27.332928
239.937302	9082.712266	27.337946
240.369656	9079.061601	27.342964
240.325010	9084.688303	27.347981
240.490608	9093.079515	27.352999
240.772560	9081.887720	27.358016
240.734166	9091.699838	27.363034
240.761477	9083.297570	27.368052
241.220555	9101.310304	27.373069
241.139123	9118.024370	27.378087
241.237298	9112.973432	27.383104
241.510909	9140.293973	27.388122
241.572195	9146.324104	27.393140
242.248588	9156.605892	27.398157
242.160004	9163.871714	27.403175
242.432968	9175.583375	27.408192
242.404926	9185.873821	27.413210
242.838074	9207.395157	27.418228
243.290576	9218.027554	27.423245
243.181868	9243.071458	27.428263
243.511574	9247.866418	27.433280
243.324165	9274.103403	27.438298
243.722638	9284.305400	27.443316
244.245910	9296.344402	27.448333
244.082789	9320.225563	27.453351
244.363912	9342.799970	27.458368
244.517396	9360.661630	27.463386
244.846942	9369.418936	27.468404
245.020248	9384.871745	27.473421
244.874092	9406.063593	27.478439
245.253024	9429.248005	27.483456
245.619680	9447.884808	27.488474
245.770821	9457.594995	27.493492
246.203934	9483.053709	27.498509
245.989838	9510.018184	27.503527
246.617667	9524.162713	27.508544
246.884383	9549.666367	27.513562
247.628588	9566.665893	27.518580
247.948301	9582.260249	27.523597
248.215442	9602.210326	27.528615
248.750232	9605.789484	27.533632
248.832463	9620.650478	27.538650
249.308721	9630.663751	27.543668
249.094557	9637.216828	27.548685
249.352297	9661.421246	27.553703
249.650973	9655.754854	27.558720
249.925260	9675.328184	27.563738
249.996618	9688.397604	27.568756
250.397039	9701.794673	27.573773
250.335744	9724.021882	27.578791
250.745688	9736.135645	27.583808
251.617140	9747.972343	27.588826
251.871763	9747.389668	27.593844
252.312229	9755.602624	27.598861
252.469225	9772.444336	27.603879
252.995191	9774.651489	27.608896
252.995977	9785.704996	27.613914
253.017857	9779.608069	27.618932
253.206462	9798.929658	27.623949
253.424696	9814.634727	27.628967
253.695108	9824.635951	27.633984
253.684794	9843.979083	27.639002
253.934437	9856.143140	27.644020
254.579342	9866.146071	27.649037
254.028607	9884.152603	27.654055
254.509533	9889.350422	27.659072
254.729675	9905.093157	27.664090
254.831324	9936.763980	27.669108
255.473080	9943.442807	27.674125
255.608554	9970.593482	27.679143
255.660969	9975.971701	27.684160
256.186801	10003.715213	27.689178
256.737210	10023.609013	27.694196
257.274279	10029.527470	27.699213
257.205423	10043.547220	27.704231
257.307851	10052.690671	27.709248
257.752792	10070.596043	27.714266
258.138555	10078.675580	27.719284
258.344362	10080.724232	27.724301
258.501286	10098.791292	27.729319
258.925125	10117.391450	27.734336
259.340459	10134.385867	27.739354
259.340259	10148.909653	27.744372
259.986971	10132.223509	27.749389
260.373287	10143.911820	27.754407
260.474900	10158.969139	27.759424
261.403617	10159.730723	27.764442
261.084382	10163.465053	27.769460
261.223332	10168.049994	27.774477
261.654495	10180.359657	27.779495
261.844949	10184.661895	27.784512
261.701779	10182.950820	27.789530
261.788569	10194.698425	27.794548
262.140441	10201.880292	27.799565
262.204312	10214.525006	27.804583
262.412274	10232.176953	27.809600
262.905926	10239.570406	27.814618
263.055661	10260.682429	27.819636
263.444841	10266.014618	27.824653
262.911816	10283.646209	27.829671
263.173144	10290.870624	27.834688
263.711710	10310.949702	27.839706
263.528027	10342.539342	27.844724
264.031732	10367.498886	27.849741
263.916298	10380.935712	27.854759
264.526604	10410.343246	27.859776
264.923249	10420.868208	27.864794
264.991579	10444.285372	27.869812
265.462339	10478.431874	27.874829
265.594417	10496.553707	27.879847
266.087330	10517.855713	27.884864
266.375816	10533.477831	27.889882
266.427059	10543.346222	27.894900
266.976099	10560.260222	27.899917
267.297361	10585.665240	27.904935
267.686992	10600.169732	27.909952
268.161651	10607.057945	27.914970
267.856417	10629.207387	27.919988
268.572477	10654.295283	27.925005
268.756905	10682.004551	27.930023
269.186394	10684.643616	27.935040
269.617584	10697.578788	27.940058
269.623991	10714.725808	27.945076
269.953039	10726.922276	27.950093
270.248837	10747.405884	27.955111
270.330580	10758.769422	27.960128
270.569189	10780.420749	27.965146
270.996961	10795.917207	27.970164
271.745611	10816.415639	27.975181
271.345220	10824.911537	27.980199
271.482437	10843.465478	27.985216
272.032509	10856.205434	27.990234
272.353899	10884.367297	27.995252
273.035778	10890.105614	28.000269
273.198029	10906.533906	28.005287
273.577611	10924.254514	28.010304
273.940557	10938.438204	28.015322
274.062297	10955.419089	28.020340
274.264474	10953.420524	28.025357
274.426690	10969.921500	28.030375
274.722662	10978.728998	28.035392
274.995016	10990.899733	28.040410
275.093924	11018.660704	28.045428
275.475750	11020.344206	28.050445
275.913601	11033.897442	28.055463
276.166799	11055.278430	28.060480
276.350221	11063.399371	28.065498
276.724043	11086.018296	28.070516
277.293875	11092.014090	28.075533
277.667867	11097.604641	28.080551
277.848830	11113.641830	28.085568
278.250801	11118.280781	28.090586
277.922664	11133.339484	28.095604
278.436032	11145.046536	28.100621
278.306985	11167.286011	28.105639
278.470634	11183.922724	28.110656
278.916864	11198.283098	28.115674
278.930265	11222.205518	28.120692
279.406440	11237.672705	28.125709
279.775358	11258.341256	28.130727
279.760650	11274.487984	28.135744
280.065449	11291.128078	28.140762
280.211972	11312.914345	28.145780
280.850656	11322.271739	28.150797
281.041688	11333.587037	28.155815
281.226507	11349.197560	28.160832
281.520679	11365.908841	28.165850
282.085124	11377.784909	28.170868
282.700717	11396.094414	28.175885
282.974448	11408.104173	28.180903
282.964216	11417.651053	28.185920
283.522597	11435.672694	28.190938
283.191779	11438.739678	28.195956
283.967375	11446.752804	28.200973
284.212146	11449.051304	28.205991
284.724152	11472.290168	28.211008
285.437363	11464.894661	28.216026
285.528405	11480.362016	28.221044
285.660426	11500.126763	28.226061
286.065136	11507.237758	28.231079
285.908306	11506.485430	28.236096
286.075490	11528.909717	28.241114
285.917576	11546.376735	28.246132
286.341975	11562.483767	28.251149
286.514944	11587.250144	28.256167
286.575109	11601.759345	28.261184
286.846679	11629.232261	28.266202
287.130613	11648.029394	28.271220
287.750200	11670.370788	28.276237
287.972621	11698.116695	28.281255
288.385510	11723.767918	28.286272
288.759455	11745.121423	28.291290
288.779966	11761.888294	28.296308
288.902390	11786.081802	28.301325
289.590665	11811.039803	28.306343
289.470011	11829.107545	28.311360
290.184939	11855.769728	28.316378
290.403104	11880.475776	28.321396
290.697577	11903.676416	28.326413
291.064465	11917.320282	28.331431
291.398980	11939.633753	28.336448
292.080625	11943.837823	28.341466
292.423997	11965.992065	28.346484
292.505222	11980.551959	28.351501
293.044850	11992.043892	28.356519
292.908880	12008.633255	28.361536
293.279458	12024.752221	28.366554
293.609734	12059.832886	28.371572
293.852753	12058.383595	28.376589
294.426233	12086.081736	28.381607
294.208914	12110.401181	28.386624
294.576243	12123.391491	28.391642
295.189936	12140.233706	28.396660
295.674019	12150.029241	28.401677
296.022277	12171.415650	28.406695
295.815554	12190.378130	28.411712
296.830596	12194.353523	28.416730
296.654325	12217.053141	28.421748
297.320380	12233.852553	28.426765
297.470864	12237.684678	28.431783
297.423217	12260.418004	28.436800
297.973052	12276.780841	28.441818
298.154877	12298.840633	28.446836
298.743261	12302.538285	28.451853
299.573753	12315.402941	28.456871
299.428139	12321.946280	28.461888
299.894852	12333.756072	28.466906
300.139347	12350.346499	28.471924
300.180229	12346.282499	28.476941
300.386750	12353.844647	28.481959
300.458315	12369.539964	28.486976
300.942365	12373.433863	28.491994
300.728016	12388.589531	28.497012
301.003428	12411.417999	28.502029
301.351097	12428.008221	28.507047
301.920826	12445.489099	28.512064
301.903846	12468.104223	28.517082
302.157030	12490.225758	28.522100
302.678933	12505.330052	28.527117
303.162176	12523.051823	28.532135
303.149347	12545.284308	28.537152
303.239273	12558.292845	28.542170
303.743943	12582.181564	28.547188
304.030950	12603.233806	28.552205
304.519569	12622.840011	28.557223
304.462787	12637.939771	28.562240
305.040768	12657.772089	28.567258
305.222865	12686.795152	28.572276
305.793326	12709.259112	28.577293
306.021442	12718.381140	28.582311
306.360851	12741.234779	28.587328
306.553419	12754.669560	28.592346
306.530035	12786.241512	28.597364
307.066723	12803.263673	28.602381
307.517018	12821.404526	28.607399
308.156854	12830.996175	28.612416
308.664565	12844.334591	28.617434
308.867533	12871.223180	28.622452
309.161128	12887.891698	28.627469
309.780489	12900.770680	28.632487
309.967867	12921.169335	28.637504
310.519667	12918.048798	28.642522
310.574678	12936.248142	28.647540
310.608853	12949.884559	28.652557
311.187947	12967.528671	28.657575
311.327351	12984.552850	28.662592
311.648079	12989.132288	28.667610
311.737039	13014.999911	28.672628
311.832122	13036.540401	28.677645
312.898493	13049.769883	28.682663
313.104341	13064.699626	28.687680
313.489791	13085.405509	28.692698
313.464716	13097.879703	28.697716
313.991768	13103.604919	28.702733
314.505498	13124.202454	28.707751
314.693345	13134.894082	28.712768
314.616472	13149.498441	28.717786
315.265855	13166.588649	28.722804
314.800857	13199.010030	28.727821
315.308071	13208.455154	28.732839
315.694855	13238.274555	28.737856
316.091891	13258.081994	28.742874
316.359631	13268.900205	28.747892
316.477097	13297.482695	28.752909
316.870940	13313.403357	28.757927
316.742363	13342.791582	28.762944
317.622812	13367.857523	28.767962
317.812600	13386.020529	28.772980
318.138343	13413.771825	28.777997
318.501067	13430.714270	28.783015
318.392043	13464.021735	28.788032
318.809781	13479.897765	28.793050
319.205408	13492.688827	28.798068
320.037739	13523.462472	28.803085
320.207437	13534.286626	28.808103
320.153072	13564.238378	28.813120
320.559744	13586.627831	28.818138
321.518138	13610.399848	28.823156
321.353568	13616.933954	28.828173
322.271107	13632.514405	28.833191
322.240333	13648.037241	28.838208
322.875421	13653.524752	28.843226
323.194216	13671.642684	28.848244
323.079137	13689.439756	28.853261
323.845619	13697.812120	28.858279
324.067499	13711.530390	28.863296
324.434887	13714.457459	28.868314
324.984691	13724.619380	28.873332
325.001560	13741.830687	28.878349
325.629363	13759.553223	28.883367
325.119281	13770.773874	28.888384
325.697536	13789.116792	28.893402
326.234994	13812.417746	28.898420
326.329437	13825.407505	28.903437
326.866593	13851.241231	28.908455
326.987065	13867.192289	28.913472
327.014293	13883.382091	28.918490
327.303790	13903.165895	28.923508
327.075599	13934.815859	28.928525
328.019241	13951.336744	28.933543
328.797665	13976.754124	28.938560
329.033935	13998.741109	28.943578
329.977650	14008.286053	28.948596
329.844085	14033.930757	28.953613
330.363825	14036.174138	28.958631
330.513935	14062.643164	28.963648
331.253834	14080.354865	28.968666
331.332779	14090.306069	28.973684
331.461158	14110.358339	28.978701
332.104465	14132.225265	28.983719
332.370463	14148.927615	28.988736
332.713228	14159.602020	28.993754
333.075145	14176.930537	28.998772
332.669402	14196.301812	29.003789
332.980847	14212.883453	29.008807
333.420571	14233.023176	29.013824
333.526288	14263.933255	29.018842
334.167896	14291.781932	29.023860
334.702382	14317.863038	29.028877
334.974493	14333.051899	29.033895
335.015975	14352.849519	29.038912
335.276804	14383.966183	29.043930
335.613858	14406.073745	29.048948
335.942301	14441.762306	29.053965
336.484521	14470.157272	29.058983
336.612019	14487.696261	29.064000
336.637685	14520.716174	29.069018
337.415273	14543.169019	29.074036
337.635177	14572.217508	29.079053
338.384827	14585.898459	29.084071
338.632818	14620.008209	29.089088
338.470655	14633.044785	29.094106
339.316870	14654.849145	29.099124
339.594187	14674.196674	29.104141
340.044905	14702.779928	29.109159
340.652785	14724.482517	29.114176
340.969499	14738.688905	29.119194
341.866479	14755.543045	29.124212
341.563155	14774.712633	29.129229
342.024294	14794.454853	29.134247
342.248838	14813.592830	29.139264
342.673534	14834.288201	29.144282
343.299559	14847.761204	29.149300
343.358856	14860.194996	29.154317
343.928760	14864.950852	29.159335
344.235020	14881.878121	29.164352
344.459487	14893.041918	29.169370
344.896622	14902.997788	29.174388
344.935539	14928.787383	29.179405
345.280152	14941.164176	29.184423
345.442362	14955.663222	29.189440
346.053873	14983.839731	29.194458
346.255540	14986.439087	29.199476
346.602113	15007.746856	29.204493
346.784992	15027.797924	29.209511
346.850768	15056.394266	29.214528
347.040033	15077.376048	29.219546
347.695159	15101.190838	29.224564
347.736406	15126.175005	29.229581
348.171195	15150.687375	29.234599
348.774930	15183.943733	29.239616
348.800173	15201.114001	29.244634
349.443588	15230.163882	29.249652
349.554428	15266.907961	29.254669
349.870598	15284.374096	29.259687
350.197142	15314.493533	29.264704
350.575758	15335.319793	29.269722
351.195210	15356.853917	29.274740
351.488281	15393.974121	29.279757
352.031481	15409.794337	29.284775
352.411938	15439.791884	29.289792
352.735350	15468.048702	29.294810
353.048423	15481.656148	29.299828
353.542951	15508.329380	29.304845
353.743433	15523.593508	29.309863
354.436803	15558.965215	29.314880
354.400896	15581.106940	29.319898
355.132311	15598.846649	29.324916
355.122438	15629.941166	29.329933
355.529276	15657.076729	29.334951
356.077774	15669.817037	29.339968
356.653328	15695.682036	29.344986
357.010864	15712.017781	29.350004
357.456835	15741.187610	29.355021
357.590244	15756.999273	29.360039
358.189934	15770.571779	29.365056
358.192332	15798.534810	29.370074
358.867469	15812.809372	29.375092
358.508843	15833.334057	29.380109
359.184465	15863.557930	29.385127
359.798735	15886.521007	29.390144
359.981784	15904.760108	29.395162
360.853807	15924.389000	29.400180
361.297444	15940.689428	29.405197
361.700279	15951.020709	29.410215
362.317702	15966.624543	29.415232
362.473432	15983.408834	29.420250
362.452796	16000.271131	29.425268
362.684414	16017.302619	29.430285
363.146039	16044.954484	29.435303
363.551684	16055.455933	29.440320
364.121957	16072.229457	29.445338
364.308411	16097.798685	29.450356
364.425924	16112.652984	29.455373
365.028108	16132.200924	29.460391
365.961815	16155.054586	29.465408
366.052161	16167.288577	29.470426
366.313297	16183.961884	29.475444
366.355061	16208.994760	29.480461
366.666313	16233.142434	29.485479
366.953769	16252.208891	29.490496
367.188897	16270.155981	29.495514
367.848378	16290.112066	29.500532
367.917432	16319.878379	29.505549
368.269860	16334.266740	29.510567
368.632499	16353.716390	29.515584
368.653676	16381.595229	29.520602
369.113269	16404.134520	29.525620
369.372891	16428.985322	29.530637
369.916430	16451.511599	29.535655
370.426079	16470.944798	29.540672
370.695161	16496.580654	29.545690
371.230390	16516.891110	29.550708
371.701354	16535.758727	29.555725
372.010990	16561.656821	29.560743
372.914339	16572.065279	29.565760
372.964640	16586.665102	29.570778
373.721523	16600.937004	29.575796
373.825685	16625.373243	29.580813
374.073112	16644.433689	29.585831
374.448121	16668.717273	29.590848
374.683986	16690.347363	29.595866
374.972367	16697.311033	29.600884
375.280175	16737.583657	29.605901
375.787545	16765.030459	29.610919
376.366334	16780.691508	29.615936
376.722609	16800.910104	29.620954
377.003426	16819.153805	29.625972
377.267678	16840.334303	29.630989
378.124137	16872.192961	29.636007
378.228919	16881.689937	29.641024
378.730098	16906.759587	29.646042
378.999668	16929.515428	29.651060
379.229597	16957.034122	29.656077
379.400968	16971.688034	29.661095
379.937611	17001.426826	29.666112
379.765348	17023.888339	29.671130
380.255640	17052.753209	29.676148
380.947589	17082.600605	29.681165
381.189344	17112.382318	29.686183
381.336253	17139.345668	29.691200
381.642780	17179.846829	29.696218
382.330030	17204.970021	29.701236
382.366064	17244.897520	29.706253
382.827430	17282.588979	29.711271
383.352989	17308.176512	29.716288
383.675942	17341.530868	29.721306
383.816394	17377.557390	29.726324
384.316002	17417.792101	29.731341
384.898866	17446.128306	29.736359
385.679988	17476.688897	29.741376
385.972780	17503.560557	29.746394
386.655862	17523.988037	29.751412
387.061884	17553.324769	29.756429
387.264338	17576.496119	29.761447
387.889492	17601.218881	29.766464
388.004391	17628.611148	29.771482
388.081365	17657.544429	29.776500
388.916666	17675.500470	29.781517
388.998286	17706.492500	29.786535
389.597112	17736.127988	29.791552
390.111942	17763.723506	29.796570
390.246446	17784.246142	29.801588
390.732199	17809.824745	29.806605
391.047697	17838.841192	29.811623
391.403675	17863.991547	29.816640
392.306310	17892.076475	29.821658
392.956882	17907.970484	29.826676
393.284179	17928.387451	29.831693
394.244280	17936.854739	29.836711
395.508025	17922.475770	29.841728
395.985513	17923.064763	29.846746
395.917111	17922.380531	29.851764
396.022573	17919.401336	29.856781
396.118629	17939.089927	29.861799
396.741730	17938.424385	29.866816
396.886046	17944.258036	29.871834
396.983651	17958.065035	29.876852
397.438227	17973.218904	29.881869
397.684162	17990.401525	29.886887
397.943147	17997.120712	29.891904
398.002361	18024.105268	29.896922
398.173013	18031.450995	29.901940
398.718358	18055.030701	29.906957
398.647678	18088.883523	29.911975
399.404584	18109.953974	29.916992
399.443972	18145.539656	29.922010
399.979192	18168.603056	29.927028
400.335920	18197.215630	29.932045
400.560670	18236.859945	29.937063
401.042531	18266.419697	29.942080
401.190914	18293.466554	29.947098
401.578888	18325.340537	29.952116
402.468957	18352.309915	29.957133
402.618230	18394.284787	29.962151
402.970400	18417.459107	29.967168
403.154552	18451.569808	29.972186
403.751500	18480.770829	29.977204
404.054205	18513.144838	29.982221
404.786689	18550.120596	29.987239
405.672374	18564.474988	29.992256
405.579407	18604.131612	29.997274
406.084840	18637.118650	30.002292
406.523817	18671.733370	30.007309
407.006265	18704.863087	30.012327
407.368315	18723.715059	30.017344
408.160156	18764.510401	30.022362
408.065162	18785.303574	30.027380
408.423018	18809.336662	30.032397
408.686794	18840.769647	30.037415
409.556508	18876.821254	30.042432
409.662044	18906.048878	30.047450
409.955609	18942.158713	30.052468
410.468551	18978.998893	30.057485
410.757690	19010.042829	30.062503
411.842840	19025.813245	30.067520
412.330243	19048.632433	30.072538
412.530134	19072.703075	30.077556
413.213497	19099.617228	30.082573
413.421770	19125.771451	30.087591
413.983908	19153.765917	30.092608
414.233441	19176.862358	30.097626
414.827400	19205.900677	30.102644
415.163200	19227.164258	30.107661
415.171179	19261.752362	30.112679
415.856849	19281.287346	30.117696
416.525657	19311.634570	30.122714
416.477209	19340.634110	30.127732
416.658616	19368.056385	30.132749
416.982400	19411.219288	30.137767
417.758666	19428.415388	30.142784
418.280497	19464.869722	30.147802
418.411458	19498.731511	30.152820
419.399976	19534.367825	30.157837
419.382163	19562.282586	30.162855
419.826589	19593.347502	30.167872
420.412446	19621.490575	30.172890
420.641595	19656.885217	30.177908
420.784865	19671.918298	30.182925
421.037565	19715.686817	30.187943
421.656358	19744.791570	30.192960
422.246264	19769.560497	30.197978
422.387241	19803.958275	30.202996
423.307105	19824.013318	30.208013
423.445659	19853.622613	30.213031
423.797978	19875.294992	30.218048
424.468390	19902.705069	30.223066
424.707146	19935.817959	30.228084
425.520932	19956.218184	30.233101
425.730920	19994.181495	30.238119
425.858265	20013.867314	30.243136
426.701618	20046.469285	30.248154
426.710201	20075.998064	30.253172
427.657593	20100.370588	30.258189
427.670895	20133.954852	30.263207
428.126260	20157.532167	30.268224
428.767523	20196.148978	30.273242
428.797098	20223.747724	30.278260
429.387347	20257.084430	30.283277
429.602965	20297.505159	30.288295
430.195859	20318.704634	30.293312
430.736310	20357.615452	30.298330
430.942182	20389.685434	30.303348
431.514756	20423.044129	30.308365
431.774169	20457.917428	30.313383
432.388786	20490.732657	30.318400
432.634165	20521.545723	30.323418
433.110370	20567.941272	30.328436
433.603206	20601.856044	30.333453
434.251597	20640.820120	30.338471
434.586775	20663.829169	30.343488
434.986847	20698.851588	30.348506
435.233016	20741.587240	30.353524
436.015360	20775.482514	30.358541
436.640223	20808.397771	30.363559
437.187013	20818.819818	30.368576
437.753341	20847.359427	30.373594
438.590419	20881.909776	30.378612
439.061581	20900.721594	30.383629
439.437588	20927.130118	30.388647
440.274500	20937.393334	30.393664
440.751312	20951.768923	30.398682
441.342850	20971.895218	30.403700
441.826077	20983.085437	30.408717
441.917291	21013.367271	30.413735
442.390299	21029.360984	30.418752
442.951543	21046.035982	30.423770
442.977777	21071.968418	30.428788
443.193170	21095.521040	30.433805
443.397542	21117.767518	30.438823
443.869483	21149.399269	30.443840
444.536478	21170.291172	30.448858
444.860920	21190.174949	30.453876
445.060065	21225.450730	30.458893
445.721980	21265.936661	30.463911
446.013434	21281.112186	30.468928
446.390021	21305.530850	30.473946
447.066169	21337.055293	30.478964
448.222921	21354.421322	30.483981
448.792218	21376.232181	30.488999
449.210454	21392.127304	30.494016
449.293420	21417.918679	30.499034
449.563430	21437.646902	30.504052
450.513265	21455.007324	30.509069
450.718968	21482.106539	30.514087
450.843567	21504.321646	30.519104
451.039483	21523.789799	30.524122
451.673531	21544.004840	30.529140
452.184348	21578.474522	30.534157
452.374639	21588.200585	30.539175
452.826064	21621.491722	30.544192
453.258730	21645.819940	30.549210
453.492404	21671.821968	30.554228
453.776442	21696.710456	30.559245
454.344330	21729.516078	30.564263
454.886487	21756.588565	30.569280
454.928258	21784.655173	30.574298
455.442021	21818.391870	30.579316
456.093212	21853.623677	30.584333
456.790042	21879.200038	30.589351
456.582255	21915.595601	30.594368
457.145856	21946.708882	30.599386
457.367732	21989.248832	30.604404
457.705191	22012.278062	30.609421
458.635348	22062.865191	30.614439
458.979923	22095.876790	30.619456
459.336646	22142.294656	30.624474
459.529382	22184.207702	30.629492
460.321398	22218.672639	30.634509
460.767139	22254.802801	30.639527
461.414933	22283.799394	30.644544
462.119557	22326.391291	30.649562
462.111055	22365.675886	30.654580
462.755349	22401.250954	30.659597
463.186434	22432.215025	30.664615
463.418013	22478.501514	30.669632
463.908189	22502.259468	30.674650
464.495274	22554.360894	30.679668
465.331455	22584.946202	30.684685
465.986719	22620.456770	30.689703
466.352667	22659.595191	30.694720
467.092674	22697.872970	30.699738
467.084387	22727.515769	30.704756
468.150155	22754.204808	30.709773
469.033215	22789.402189	30.714791
468.902666	22819.550709	30.719808
469.405912	22848.046170	30.724826
469.720799	22882.201095	30.729844
470.176894	22904.524140	30.734861
470.915648	22941.911627	30.739879
471.151015	22969.715977	30.744896
471.498221	23003.082538	30.749914
472.284880	23049.220757	30.754932
472.845417	23076.702922	30.759949
473.315171	23113.500719	30.764967
473.507700	23142.575766	30.769984
474.140194	23174.836621	30.775002
474.515864	23210.631894	30.780020
474.965503	23241.606980	30.785037
475.184108	23277.452101	30.790055
475.570924	23320.525303	30.795072
476.227780	23349.281927	30.800090
476.699317	23386.174736	30.805108
477.323566	23418.664756	30.810125
478.389526	23449.373605	30.815143
479.458042	23458.053928	30.820160
479.893828	23485.265406	30.825178
480.340274	23514.509997	30.830196
480.909427	23520.095922	30.835213
481.348475	23546.359117	30.840231
481.471605	23572.842143	30.845248
482.016983	23582.703481	30.850266
482.050490	23624.960313	30.855284
482.504825	23647.221278	30.860301
482.989345	23679.177396	30.865319
483.050009	23701.828302	30.870336
483.865706	23725.126305	30.875354
484.357527	23748.487394	30.880372
484.713334	23779.484246	30.885389
485.336150	23805.466409	30.890407
485.350824	23837.824523	30.895424
485.844270	23873.798549	30.900442
486.129932	23896.395690	30.905460
487.192110	23922.341204	30.910477
487.545470	23945.174310	30.915495
487.823607	23979.185181	30.920512
488.485275	24018.760504	30.925530
488.669118	24050.669239	30.930548
489.065917	24082.620704	30.935565
489.630653	24117.016901	30.940583
489.869071	24159.982318	30.945600
490.328506	24197.150244	30.950618
490.764219	24226.915733	30.955636
491.099866	24277.474683	30.960653
492.058616	24316.208115	30.965671
492.101247	24365.075092	30.970688
493.172109	24403.715410	30.975706
493.350444	24434.867296	30.980724
493.963605	24477.218954	30.985741
494.687851	24504.172060	30.990759
495.286638	24547.638313	30.995776
496.110131	24573.021494	31.000794
496.375567	24605.461880	31.005812
496.976181	24642.071507	31.010829
497.602849	24680.787833	31.015847
497.975914	24709.034493	31.020864
498.816291	24736.456430	31.025882
499.159995	24773.504418	31.030900
499.758861	24796.913266	31.035917
500.474074	24834.048878	31.040935
500.698464	24869.314568	31.045952
501.287850	24893.268481	31.050970
501.545135	24927.884564	31.055988
501.845205	24959.643947	31.061005
502.201075	24992.513248	31.066023
502.572912	25028.375577	31.071040
503.124548	25060.987011	31.076058
503.485900	25101.110476	31.081076
504.059439	25150.345406	31.086093
504.627244	25184.054130	31.091111
504.526373	25233.015078	31.096128
505.436907	25279.177095	31.101146
506.002374	25322.928283	31.106164
506.417555	25372.188411	31.111181
507.193886	25402.850570	31.116199
507.637725	25448.801247	31.121216
508.494022	25475.968934	31.126234
508.870384	25524.451839	31.131252
509.551716	25562.990729	31.136269
510.290776	25602.222194	31.141287
510.783131	25633.011070	31.146304
511.166604	25661.067860	31.151322
511.515483	25707.311980	31.156340
511.831534	25746.356789	31.161357
512.639369	25772.344308	31.166375
513.141042	25822.009178	31.171392
513.281703	25851.405909	31.176410
513.811017	25892.509653	31.181428
514.216121	25939.459691	31.186445
514.833958	25967.455145	31.191463
515.079614	26015.725747	31.196480
515.765891	26052.994518	31.201498
516.549334	26092.656101	31.206516
516.753365	26132.249966	31.211533
517.527282	26171.255920	31.216551
517.653699	26209.003970	31.221568
518.264454	26231.470978	31.226586
518.886481	26268.042319	31.231604
519.037933	26314.438645	31.236621
519.678336	26351.980548	31.241639
519.990883	26393.776335	31.246656
520.857666	26436.730962	31.251674
521.243136	26475.835898	31.256692
521.491537	26516.706567	31.261709
522.400131	26548.272605	31.266727
523.377032	26587.456325	31.271744
523.810232	26627.976129	31.276762
524.581726	26662.243385	31.281780
525.024982	26691.442552	31.286797
525.859156	26721.655315	31.291815
526.432217	26763.202749	31.296832
526.898121	26793.618313	31.301850
527.453163	26827.704663	31.306868
527.593649	26854.903489	31.311885
528.571046	26887.792891	31.316903
528.855445	26928.052057	31.321920
529.317939	26958.228235	31.326938
529.811929	26993.992886	31.331956
530.110100	27027.929958	31.336973
530.460116	27065.758561	31.341991
530.890582	27112.208084	31.347008
531.514152	27153.065875	31.352026
531.955766	27196.511761	31.357044
532.484284	27245.101517	31.362061
533.041831	27282.999342	31.367079
533.856978	27336.980104	31.372096
534.289207	27376.490317	31.377114
534.876026	27415.647887	31.382132
535.319327	27466.880677	31.387149
535.800034	27505.669402	31.392167
536.208912	27552.458270	31.397184
536.426606	27592.634334	31.402202
537.708651	27636.980544	31.407220
538.070629	27676.205221	31.412237
539.146993	27715.299800	31.417255
539.723103	27755.331904	31.422272
540.144389	27786.109846	31.427290
541.097988	27827.505417	31.432308
541.638862	27860.009287	31.437325
542.276799	27881.848178	31.442343
542.381233	27923.951298	31.447360
543.554970	27948.380397	31.452378
544.128282	27978.818942	31.457396
544.641425	28008.078653	31.462413
545.063326	28038.932728	31.467431
545.259572	28054.728668	31.472448
545.832971	28085.862613	31.477466
546.686662	28128.664859	31.482484
547.071834	28171.262029	31.487501
547.536385	28193.558044	31.492519
547.827724	28232.857996	31.497536
547.800179	28276.158009	31.502554
548.339585	28317.852919	31.507572
548.750688	28352.533090	31.512589
549.564785	28398.034630	31.517607
550.219235	28441.342594	31.522624
550.550669	28484.479715	31.527642
551.332538	28526.940025	31.532660
551.699877	28572.214433	31.537677
552.060201	28621.876568	31.542695
552.787542	28653.379297	31.547712
553.383820	28700.956997	31.552730
554.056912	28725.654591	31.557748
553.994547	28772.153022	31.562765
554.645123	28810.165626	31.567783
555.101319	28849.851948	31.572800
555.739022	28893.043385	31.577818
556.526560	28945.857057	31.582836
556.355961	28989.983587	31.587853
557.662124	29033.520032	31.592871
558.237855	29081.285119	31.597888
558.288221	29120.731747	31.602906
559.281597	29166.137562	31.607924
559.297544	29201.974193	31.612941
560.057992	29245.981617	31.617959
560.706350	29304.335982	31.622976
561.290815	29355.229177	31.627994
561.744174	29399.765124	31.633012
561.643350	29463.590370	31.638029
562.926865	29500.627117	31.643047
563.492060	29563.710578	31.648064
563.987832	29611.527275	31.653082
564.621868	29659.328879	31.658100
565.348331	29709.189491	31.663117
565.894028	29756.410901	31.668135
566.281560	29805.730335	31.673152
566.930727	29859.724651	31.678170
567.800679	29905.138677	31.683188
568.512307	29957.688648	31.688205
569.054922	29991.371358	31.693223
569.938055	30032.523208	31.698240
570.702464	30079.629139	31.703258
571.389370	30120.982384	31.708276
571.517244	30167.043485	31.713293
572.006391	30201.790492	31.718311
572.917761	30244.158351	31.723328
573.437544	30288.591068	31.728346
573.946645	30332.956010	31.733364
574.159262	30382.095458	31.738381
574.988593	30419.432135	31.743399
575.757900	30466.860572	31.748416
576.091922	30510.918128	31.753434
577.040123	30542.471557	31.758452
577.317574	30600.210969	31.763469
577.951905	30632.293814	31.768487
578.992826	30677.569148	31.773504
579.205571	30719.604253	31.778522
579.793587	30763.300422	31.783540
580.411223	30807.782238	31.788557
580.795840	30848.204196	31.793575
581.487298	30897.889819	31.798592
581.802572	30942.166140	31.803610
582.306253	30985.414448	31.808628
583.199845	31038.356060	31.813645
583.536237	31081.561076	31.818663
584.024007	31130.058934	31.823680
584.819873	31180.607662	31.828698
585.456774	31221.749650	31.833716
585.890547	31268.922413	31.838733
586.477362	31311.418849	31.843751
587.299025	31354.770143	31.848768
588.394774	31395.322683	31.853786
589.216224	31429.040193	31.858804
589.463413	31468.454350	31.863821
590.002493	31510.617264	31.868839
590.510623	31553.587919	31.873856
590.760523	31594.658141	31.878874
591.760251	31631.350972	31.883892
592.106197	31675.845342	31.888909
592.877626	31718.098939	31.893927
593.182269	31750.019909	31.898944
593.876220	31784.737698	31.903962
594.191853	31826.196408	31.908980
594.844697	31861.243127	31.913997
595.292457	31904.925611	31.919015
596.052981	31944.146969	31.924032
596.398507	31992.928179	31.929050
596.932872	32041.774931	31.934068
597.333990	32077.777850	31.939085
597.676368	32134.575817	31.944103
598.502379	32176.189677	31.949120
599.020673	32225.462920	31.954138
600.244506	32271.964979	31.959156
600.499042	32319.869750	31.964173
601.062918	32361.600651	31.969191
601.621833	32413.042713	31.974208
602.174147	32469.973280	31.979226
602.914028	32513.447199	31.984244
602.932809	32568.501320	31.989261
603.938643	32622.700200	31.994279
604.916095	32671.713363	31.999296
605.153326	32728.301729	32.004314
605.813643	32778.066244	32.009332
606.870168	32832.750889	32.014349
607.328416	32873.525679	32.019367
608.681345	32912.359511	32.024384
609.290452	32937.432470	32.029402
610.404404	32978.497353	32.034420
611.336768	33015.487608	32.039437
611.636974	33056.344257	32.044455
611.924122	33092.872433	32.049472
612.325340	33131.955982	32.054490
613.162205	33166.786593	32.059508
613.428403	33210.487435	32.064525
614.136573	33253.582188	32.069543
614.340917	33295.781862	32.074560
614.904570	33344.905281	32.079578
615.414283	33380.558473	32.084596
615.923458	33436.158103	32.089613
616.510174	33493.838440	32.094631
617.581499	33537.699124	32.099648
617.997305	33593.301063	32.104666
618.373935	33651.355934	32.109684
619.512739	33686.993905	32.114701
620.171335	33736.229905	32.119719
620.820403	33783.513935	32.124736
621.546714	33834.124193	32.129754
621.825541	33884.108784	32.134772
622.685881	33921.390036	32.139789
623.736346	33947.647310	32.144807
624.897309	33984.059978	32.149824
625.579182	34014.010033	32.154842
625.859834	34053.069814	32.159860
626.441729	34086.576030	32.164877
626.966011	34135.182678	32.169895
627.588156	34164.528979	32.174912
627.802134	34206.577249	32.179930
628.229585	34250.944292	32.184948
628.943046	34287.857073	32.189965
629.666098	34346.334117	32.194983
630.371272	34387.825781	32.200000
630.574577	34433.644323	32.205018
631.201132	34476.280114	32.210036
631.541276	34525.883662	32.215053
631.839095	34574.798445	32.220071
632.487968	34631.346830	32.225088
632.875266	34690.857083	32.230106
633.568918	34738.262771	32.235124
634.044963	34802.330702	32.240141
634.557947	34856.207445	32.245159
635.105962	34900.278895	32.250176
635.816921	34964.980942	32.255194
636.579243	35023.238783	32.260212
637.332123	35069.080635	32.265229
637.733090	35130.221232	32.270247
638.406648	35188.689349	32.275264
639.051312	35242.337930	32.280282
639.926745	35296.551378	32.285300
640.908372	35359.037494	32.290317
641.453467	35412.632458	32.295335
642.271358	35458.224772	32.300352
642.850427	35520.647577	32.305370
643.514554	35572.068358	32.310388
643.829326	35614.780276	32.315405
644.497589	35673.591987	32.320423
645.465063	35736.340655	32.325440
645.669141	35784.077815	32.330458
646.026149	35849.545825	32.335476
646.843912	35907.013435	32.340493
647.354783	35973.981687	32.345511
648.949453	36029.773258	32.350528
649.484510	36083.978481	32.355546
650.264598	36136.198234	32.360564
650.815965	36189.098662	32.365581
651.627411	36238.228186	32.370599
652.461005	36283.813508	32.375616
653.045177	36345.959736	32.380634
653.565810	36385.719935	32.385652
655.045792	36425.021037	32.390669
655.689039	36468.967112	32.395687
657.171763	36495.097047	32.400704
657.602713	36530.672980	32.405722
658.069046	36569.259566	32.410740
658.813601	36606.620495	32.415757
659.276894	36649.146973	32.420775
660.165085	36677.178087	32.425792
660.149221	36721.986060	32.430810
661.303778	36765.442150	32.435828
661.799095	36801.836846	32.440845
662.126497	36857.954337	32.445863
662.940730	36890.885039	32.450880
663.223605	36944.486750	32.455898
663.712879	37007.990196	32.460916
664.376383	37051.801534	32.465933
664.582943	37107.059566	32.470951
665.510154	37167.118711	32.475968
665.812356	37222.823750	32.480986
666.498248	37272.057408	32.486004
667.260949	37338.605027	32.491021
667.835241	37401.520988	32.496039
668.413566	37440.072744	32.501056
669.283229	37506.104692	32.506074
670.076868	37559.697990	32.511092
671.102752	37612.268823	32.516109
671.552565	37668.521146	32.521127
672.146313	37725.364581	32.526144
672.704347	37790.800931	32.531162
673.147300	37834.401593	32.536180
673.915576	37888.138777	32.541197
674.672673	37950.085697	32.546215
675.667336	38010.674206	32.551232
676.176109	38067.417953	32.556250
676.634894	38130.417269	32.561268
677.600642	38184.086514	32.566285
678.236907	38237.434093	32.571303
679.052960	38278.663156	32.576320
679.669900	38332.924575	32.581338
679.989567	38382.274707	32.586356
680.825655	38414.546701	32.591373
681.096087	38477.222233	32.596391
682.124947	38531.255615	32.601408
682.714546	38588.316983	32.606426
683.297328	38641.212263	32.611444
683.884682	38692.045439	32.616461
684.506795	38760.016888	32.621479
685.329255	38811.863483	32.626496
685.651863	38866.077209	32.631514
686.316306	38937.122287	32.636532
687.202712	38988.927735	32.641549
687.681886	39058.819509	32.646567
688.709321	39111.273619	32.651584
689.136142	39175.419254	32.656602
689.632187	39233.458114	32.661620
690.299668	39300.387091	32.666637
690.975427	39377.363642	32.671655
691.842951	39422.362244	32.676672
692.637217	39502.779968	32.681690
693.409133	39570.635788	32.686708
693.863122	39630.231627	32.691725
694.786618	39701.017550	32.696743
695.717405	39757.877120	32.701760
696.709897	39822.176925	32.706778
697.245445	39879.756040	32.711796
698.120722	39949.848315	32.716813
699.011958	40002.831717	32.721831
699.604822	40050.897288	32.726848
700.162000	40112.211187	32.731866
700.937165	40171.486579	32.736884
702.317613	40219.480515	32.741901
702.612410	40293.768627	32.746919
703.356555	40329.947156	32.751936
704.338122	40396.229828	32.756954
705.033453	40452.185570	32.761972
705.813529	40504.896588	32.766989
706.610055	40565.257495	32.772007
707.097768	40601.659798	32.777024
708.035571	40655.763260	32.782042
709.374233	40694.765334	32.787060
709.875600	40739.912212	32.792077
710.684144	40794.289112	32.797095
711.149867	40846.164491	32.802112
711.947834	40891.031511	32.807130
712.524619	40932.941642	32.812148
713.025045	40990.282516	32.817165
713.575667	41039.691289	32.822183
714.065585	41094.029996	32.827200
714.598952	41155.002698	32.832218
715.349135	41207.517690	32.837236
716.117359	41263.641253	32.842253
716.660570	41328.319025	32.847271
717.458274	41389.206961	32.852288
717.849881	41456.558666	32.857306
718.639012	41519.801011	32.862324
719.165889	41581.338793	32.867341
719.811418	41651.200354	32.872359
720.785200	41708.342934	32.877376
721.484141	41782.731314	32.882394
721.902241	41844.312066	32.887412
723.018381	41913.234733	32.892429
723.516210	41979.262313	32.897447
724.377054	42041.786641	32.902464
725.064889	42111.168733	32.907482
725.287638	42183.754170	32.912500
725.905952	42234.723629	32.917517
726.796776	42295.447793	32.922535
727.564672	42364.767625	32.927552
729.846409	42386.043113	32.932570
730.956271	42421.921515	32.937588
732.361576	42455.394842	32.942605
733.133637	42487.037737	32.947623
733.638378	42520.847422	32.952640
734.318124	42548.981865	32.957658
734.453759	42592.652570	32.962676
735.349358	42621.809749	32.967693
735.781190	42685.167998	32.972711
736.326808	42721.337121	32.977728
736.756961	42765.316513	32.982746
736.909514	42827.289226	32.987764
737.861736	42873.236827	32.992781
738.442997	42942.827881	32.997799
739.154933	42999.084820	33.002816
739.948055	43058.175493	33.007834
740.245165	43121.530668	33.012852
741.220598	43190.175646	33.017869
741.581906	43264.596296	33.022887
742.243749	43332.240580	33.027904
743.101961	43387.330908	33.032922
743.487891	43458.857833	33.037940
744.231713	43532.909912	33.042957
744.923088	43608.880586	33.047975
745.851136	43684.378245	33.052992
746.890430	43751.515969	33.058010
747.313100	43833.253503	33.063028
748.018794	43900.348731	33.068045
749.186591	43977.410341	33.073063
749.884842	44043.526753	33.078080
750.958833	44100.533438	33.083098
752.138299	44180.041808	33.088116
752.833486	44248.018937	33.093133
753.372065	44303.515517	33.098151
754.236256	44359.625707	33.103168
755.253676	44419.539017	33.108186
755.720491	44483.833117	33.113204
756.748725	44543.593269	33.118221
757.134239	44609.146487	33.123239
758.209839	44671.600553	33.128256
759.073113	44736.883687	33.133274
759.473442	44807.147627	33.138292
760.748526	44862.891503	33.143309
761.842663	44912.344531	33.148327
762.443009	44975.676769	33.153344
763.199767	45040.749657	33.158362
763.742861	45103.585128	33.163380
764.622803	45156.184204	33.168397
765.358050	45220.951014	33.173415
765.725380	45283.858632	33.178432
766.719526	45334.656536	33.183450
767.300524	45406.247915	33.188468
768.032725	45473.267851	33.193485
768.940918	45539.786167	33.198503
769.615039	45607.106526	33.203520
771.050360	45663.523285	33.208538
771.481436	45720.842949	33.213556
772.379519	45781.436370	33.218573
773.242659	45829.953230	33.223591
773.503697	45910.635511	33.228608
774.146009	45954.917129	33.233626
775.038172	46026.088830	33.238644
775.727941	46093.060293	33.243661
776.432409	46162.825687	33.248679
777.134331	46228.675991	33.253696
777.980193	46286.900387	33.258714
778.373218	46349.541309	33.263732
779.437532	46412.925578	33.268749
780.412954	46468.701131	33.273767
780.625851	46531.098584	33.278784
781.580074	46589.800320	33.283802
782.188373	46658.386616	33.288820
783.129036	46709.031487	33.293837
784.279488	46768.006789	33.298855
785.047288	46827.914803	33.303872
785.865311	46892.104211	33.308890
786.429261	46964.437031	33.313908
787.656742	47011.887560	33.318925
787.874675	47082.256604	33.323943
788.465409	47148.247102	33.328960
789.715646	47210.301497	33.333978
790.224548	47286.313070	33.338996
790.972322	47358.422426	33.344013
791.674864	47424.004102	33.349031
792.441150	47500.735472	33.354048
793.224419	47566.254384	33.359066
794.035125	47643.004626	33.364084
794.934717	47708.524821	33.369101
796.128541	47776.188298	33.374119
797.025149	47848.124215	33.379136
798.180962	47910.283799	33.384154
798.265521	47977.449962	33.389172
799.441184	48043.706291	33.394189
800.127883	48112.708661	33.399207
800.863196	48181.064707	33.404224
802.087212	48254.519892	33.409242
802.218650	48330.517808	33.414260
802.988824	48401.279462	33.419277
803.987937	48469.582658	33.424295
804.608883	48550.370168	33.429312
805.303133	48621.479631	33.434330
805.816327	48704.878335	33.439348
806.918680	48781.783149	33.444365
807.864595	48857.371339	33.449383
808.645149	48934.889829	33.454400
809.711009	49001.539312	33.459418
810.327395	49079.039561	33.464436
811.323237	49151.388037	33.469453
812.024673	49226.205693	33.474471
812.864336	49305.734453	33.479488
813.752305	49377.942271	33.484506
814.225595	49462.216714	33.489524
815.043138	49543.938802	33.494541
816.130018	49614.123469	33.499559
816.999987	49701.329615	33.504576
818.199880	49772.591715	33.509594
818.416796	49853.661838	33.514612
819.488897	49914.808645	33.519629
820.584858	49983.626425	33.524647
821.196788	50070.969048	33.529664
821.869605	50148.154110	33.534682
822.599154	50223.919687	33.539700
823.511565	50298.853522	33.544717
824.494120	50368.727734	33.549735
825.297163	50446.488264	33.554752
826.658488	50519.960994	33.559770
827.108377	50593.151925	33.564788
827.992538	50667.104335	33.569805
828.817781	50733.979799	33.574823
829.278114	50808.188450	33.579840
830.433441	50873.867728	33.584858
831.522365	50942.721110	33.589876
832.378753	51014.736521	33.594893
833.509507	51068.208727	33.599911
834.013703	51128.985281	33.604928
834.958301	51187.738328	33.609946
835.146422	51250.456244	33.614964
836.212655	51323.104311	33.619981
837.217056	51375.609845	33.624999
838.003263	51439.070372	33.630016
838.658637	51502.753913	33.635034
839.352727	51577.447485	33.640052
840.294332	51640.523716	33.645069
841.416118	51693.568507	33.650087
842.460206	51774.516615	33.655104
843.174190	51831.775968	33.660122
843.900309	51905.984731	33.665140
844.494912	51967.179676	33.670157
845.745522	52033.100514	33.675175
846.379198	52112.329345	33.680192
847.444397	52174.723405	33.685210
848.110846	52248.094664	33.690228
848.790030	52329.917761	33.695245
849.484254	52394.977105	33.700263
850.319306	52474.625079	33.705280
851.369647	52545.741849	33.710298
851.671382	52626.852777	33.715316
852.757055	52704.602204	33.720333
853.618725	52780.849139	33.725351
853.990464	52867.935973	33.730368
854.845151	52948.284881	33.735386
856.037948	53023.493941	33.740404
857.291175	53101.939971	33.745421
858.363250	53168.739736	33.750439
859.810777	53248.902478	33.755456
860.892793	53318.175287	33.760474
861.718224	53387.545193	33.765492
862.265975	53444.663536	33.770509
863.521792	53507.708571	33.775527
864.121302	53583.688869	33.780544
865.224684	53658.369694	33.785562
865.584028	53722.206629	33.790580
866.615640	53783.724314	33.795597
867.630084	53862.842858	33.800615
868.417706	53940.478264	33.805632
868.928934	53999.407115	33.810650
869.800516	54081.744270	33.815668
870.651578	54160.901907	33.820685
871.314416	54233.938244	33.825703
872.279523	54320.324284	33.830720
873.191664	54391.993408	33.835738
874.093688	54463.297295	33.840756
874.890351	54538.364053	33.845773
875.892066	54615.120388	33.850791
876.619648	54694.393962	33.855808
877.491498	54774.550277	33.860826
877.806655	54854.673284	33.865844
878.428302	54944.874038	33.870861
879.922717	55031.192944	33.875879
880.737977	55113.346292	33.880896
881.458716	55192.603617	33.885914
882.555811	55276.631138	33.890932
883.164877	55364.544594	33.895949
884.359814	55443.994736	33.900967
885.089976	55526.763960	33.905984
885.892924	55603.098799	33.911002
886.989485	55684.381316	33.916020
888.042399	55765.797476	33.921037
889.441191	55845.982976	33.926055
890.062046	55930.548927	33.931072
890.699635	56006.556407	33.936090
891.541125	56071.558696	33.941108
892.653051	56154.814937	33.946125
893.401688	56221.743316	33.951143
893.709133	56282.994194	33.956160
894.354745	56365.741529	33.961178
895.462770	56450.822054	33.966196
895.940589	56532.918923	33.971213
897.090394	56610.038384	33.976231
898.261374	56684.332196	33.981248
899.234145	56757.821702	33.986266
900.408487	56851.183961	33.991284
901.018269	56926.192429	33.996301
902.019383	57004.007158	34.001319
902.736313	57094.916384	34.006336
903.814752	57164.973135	34.011354
904.839041	57251.436574	34.016372
905.558381	57337.979439	34.021389
906.709834	57413.639266	34.026407
907.480793	57500.459482	34.031424
908.382395	57572.082878	34.036442
909.533757	57648.389011	34.041460
910.409166	57729.472419	34.046477
911.117985	57816.056619	34.051495
911.684867	57908.650484	34.056512
912.511339	57990.565163	34.061530
913.948926	58079.422920	34.066548
914.657604	58174.476730	34.071565
916.012415	58251.113866	34.076583
917.280784	58350.764795	34.081600
917.672251	58427.875236	34.086618
918.600688	58512.927742	34.091636
919.643742	58599.393107	34.096653
920.648778	58678.155699	34.101671
921.491791	58776.032790	34.106688
922.405429	58854.215232	34.111706
923.207650	58940.921844	34.116724
923.925300	59027.122927	34.121741
925.266379	59115.467860	34.126759
926.168176	59195.893836	34.131776
927.198605	59277.629227	34.136794
928.199545	59369.819335	34.141812
929.241516	59452.116835	34.146829
930.442436	59527.927502	34.151847
931.486595	59616.611635	34.156864
932.174136	59699.528467	34.161882
933.016715	59777.332518	34.166900
933.714369	59872.249127	34.171917
934.515899	59956.142828	34.176935
935.712643	60035.645863	34.181952
936.746738	60123.042173	34.186970
937.848088	60210.384020	34.191988
937.883814	60289.910369	34.197005
939.019853	60384.773393	34.202023
940.220609	60482.943472	34.207040
941.575393	60569.886363	34.212058
942.414942	60658.992251	34.217076
943.163627	60754.581629	34.222093
944.016120	60841.439099	34.227111
945.413112	60930.788353	34.232128
945.883100	61008.629006	34.237146
946.637727	61098.806795	34.242164
947.817064	61193.951059	34.247181
948.285877	61277.590919	34.252199
949.437654	61373.322519	34.257216
950.214379	61465.295913	34.262234
951.082390	61553.830925	34.267252
952.078047	61654.272102	34.272269
953.322382	61740.198216	34.277287
954.610776	61826.086122	34.282304
955.532576	61903.739008	34.287322
956.758789	61976.983325	34.292340
957.639774	62048.654764	34.297357
958.488787	62117.691728	34.302375
959.668814	62203.015445	34.307392
960.534223	62274.506391	34.312410
961.113095	62340.857731	34.317428
962.065269	62436.440958	34.322445
962.716053	62500.743209	34.327463
963.797262	62585.716478	34.332480
964.849219	62680.234294	34.337498
965.620320	62760.388463	34.342516
966.766514	62861.057997	34.347533
967.604189	62943.835804	34.352551
968.578735	63031.258050	34.357568
969.379165	63130.115043	34.362586
970.326303	63207.071734	34.367604
971.321191	63311.837093	34.372621
972.286382	63407.270105	34.377639
972.972103	63502.727993	34.382656
974.342374	63593.971199	34.387674
975.473701	63684.530254	34.392692
976.287127	63775.499964	34.397709
977.603420	63871.209288	34.402727
978.373366	63952.494319	34.407744
979.109740	64057.106802	34.412762
980.300171	64143.796651	34.417780
981.505751	64241.449141	34.422797
982.228355	64331.092912	34.427815
983.338529	64435.268950	34.432832
984.317170	64534.432963	34.437850
985.344682	64629.525416	34.442868
986.100469	64728.022170	34.447885
987.276532	64816.470211	34.452903
988.579837	64921.555166	34.457920
989.588438	65010.264198	34.462938
991.073994	65091.593473	34.467956
992.174378	65189.247037	34.472973
993.289169	65274.857327	34.477991
994.134439	65347.841653	34.483008
994.987302	65434.006062	34.488026
996.685298	65519.342805	34.493044
997.508018	65597.927953	34.498061
998.585034	65678.803578	34.503079
999.433008	65760.607792	34.508096
1000.252593	65846.778790	34.513114
1001.702549	65922.563951	34.518132
1002.625281	66006.984724	34.523149
1003.418368	66089.032796	34.528167
1004.937104	66165.662681	34.533184
1005.778801	66242.892018	34.538202
1007.188998	66316.209064	34.543220
1007.985133	66392.198706	34.548237
1009.023943	66470.974524	34.553255
1010.170412	66541.984394	34.558272
1011.241474	66622.452434	34.563290
1011.875702	66686.698358	34.568308
1012.952267	66769.071719	34.573325
1013.813463	66843.900290	34.578343
1014.896826	66926.019849	34.583360
1015.387165	67025.402613	34.588378
1016.541745	67094.019512	34.593396
1017.250659	67180.383216	34.598413
1018.150820	67267.990056	34.603431
1019.143875	67354.595034	34.608448
1019.355257	67455.865345	34.613466
1020.881030	67543.603683	34.618484
1021.822265	67631.604262	34.623501
1022.502396	67711.117220	34.628519
1023.270747	67802.842910	34.633536
1024.063549	67896.382284	34.638554
1025.614995	67978.400710	34.643572
1026.847101	68054.960607	34.648589
1027.808378	68142.902840	34.653607
1029.076233	68224.915547	34.658624
1030.127129	68318.859504	34.663642
1031.297299	68389.997465	34.668660
1032.437420	68472.258788	34.673677
1033.078289	68565.482339	34.678695
1033.927455	68655.963811	34.683712
1034.735744	68749.991430	34.688730
1035.806007	68849.531608	34.693748
1036.971761	68951.919293	34.698765
1038.092800	69043.189276	34.703783
1039.030695	69131.600756	34.708800
1040.262462	69233.510725	34.713818
1041.416203	69318.292726	34.718836
1042.536886	69406.461409	34.723853
1043.727183	69501.964636	34.728871
1045.037179	69594.030310	34.733888
1045.776966	69697.519371	34.738906
1046.750492	69780.500988	34.743924
1047.678309	69876.692323	34.748941
1048.805071	69971.257362	34.753959
1050.086582	70064.063661	34.758976
1050.953548	70167.237190	34.763994
1051.989610	70264.451581	34.769012
1053.164609	70364.456195	34.774029
1053.847730	70456.704827	34.779047
1055.158829	70564.756247	34.784064
1056.048694	70665.161004	34.789082
1057.210001	70758.647047	34.794100
1058.295779	70858.363496	34.799117
1059.233925	70973.554171	34.804135
1060.580619	71073.674091	34.809152
1061.353325	71183.230324	34.814170
1062.114140	71289.926620	34.819188
1063.463529	71383.841558	34.824205
1064.173519	71487.329699	34.829223
1065.346952	71599.218961	34.834240
1066.508352	71715.416674	34.839258
1067.057906	71817.436619	34.844276
1068.425543	71923.496439	34.849293
1069.513289	72049.066607	34.854311
1070.788265	72153.507971	34.859328
1071.618753	72270.519559	34.864346
1073.292312	72382.904245	34.869364
1074.168018	72491.170701	34.874381
1075.421310	72596.491108	34.879399
1076.657443	72698.749561	34.884416
1077.216214	72806.901992	34.889434
1078.197297	72906.908490	34.894452
1079.600695	73019.413932	34.899469
1080.257356	73132.973348	34.904487
1081.745051	73224.783487	34.909504
1082.739991	73352.578134	34.914522
1084.087088	73449.654573	34.919540
1085.268901	73560.081607	34.924557
1086.520818	73659.706809	34.929575
1087.864143	73763.092619	34.934592
1088.828505	73860.546785	34.939610
1090.159829	73955.296978	34.944628
1090.951962	74067.091379	34.949645
1091.979509	74166.740737	34.954663
1093.426512	74258.016135	34.959680
1094.198984	74354.564676	34.964698
1095.229776	74444.752868	34.969716
1096.212045	74524.524512	34.974733
1097.139208	74618.225332	34.979751
1098.166115	74721.372782	34.984768
1099.072368	74813.494235	34.989786
1100.205063	74906.708079	34.994804
1101.432884	75003.998742	34.999821
1102.203107	75106.832966	35.004839
1103.235863	75204.788051	35.009856
1103.970157	75313.721327	35.014874
1105.166156	75424.407191	35.019892
1106.663916	75535.173208	35.024909
1107.651143	75653.302602	35.029927
1108.958138	75745.820881	35.034944
1109.892302	75857.891977	35.039962
1110.755455	75967.111843	35.044980
1112.056443	76077.708046	35.049997
1112.892055	76196.458769	35.055015
1114.345776	76297.835762	35.060032
1115.719807	76414.160205	35.065050
1116.530524	76524.264522	35.070068
1118.281080	76636.515782	35.075085
1119.312826	76760.318050	35.080103
1120.499602	76853.960897	35.085120
1121.896624	76963.089011	35.090138
1122.831630	77059.849957	35.095156
1124.375789	77157.213147	35.100173
1125.682063	77266.027246	35.105191
1126.762509	77357.864240	35.110208
1127.945059	77463.924168	35.115226
1129.447926	77558.825016	35.120244
1130.699051	77649.876361	35.125261
1131.553044	77756.115244	35.130279
1132.782284	77848.830149	35.135296
1133.855173	77951.995425	35.140314
1135.291475	78051.557484	35.145332
1136.510969	78143.603501	35.150349
1137.651137	78247.266139	35.155367
1138.679335	78331.944405	35.160384
1139.533848	78434.208046	35.165402
1140.711316	78533.824815	35.170420
1141.645162	78631.807654	35.175437
1142.374608	78742.148924	35.180455
1144.145590	78835.099547	35.185472
1145.243572	78938.087267	35.190490
1146.289875	79041.678832	35.195508
1147.763336	79140.643639	35.200525
1148.646287	79248.467348	35.205543
1149.654075	79346.137173	35.210560
1150.731213	79457.339322	35.215578
1151.861809	79568.280223	35.220596
1153.166065	79666.462456	35.225613
1153.912800	79772.852507	35.230631
1154.975450	79881.689552	35.235648
1155.897330	79995.578484	35.240666
1156.859134	80108.321463	35.245684
1158.205137	80217.255077	35.250701
1159.356300	80336.177311	35.255719
1160.605248	80451.765529	35.260736
1161.789022	80562.689457	35.265754
1162.787182	80678.038929	35.270772
1164.061166	80793.916061	35.275789
1165.413947	80905.739902	35.280807
1166.335880	81008.876735	35.285824
1168.039482	81128.235800	35.290842
1168.667942	81247.674038	35.295860
1169.803520	81359.622189	35.300877
1170.722425	81470.578279	35.305895
1172.347594	81575.292787	35.310912
1173.433377	81674.631026	35.315930
1174.340229	81773.604707	35.320948
1175.831297	81884.245318	35.325965
1176.450628	81991.461843	35.330983
1177.841317	82100.332488	35.336000
1179.005726	82199.888401	35.341018
1179.835344	82314.472634	35.346036
1181.119519	82429.987509	35.351053
1182.320132	82547.061607	35.356071
1183.253534	82663.556948	35.361088
1184.806490	82778.727329	35.366106
1185.647104	82891.158265	35.371124
1187.209629	83007.443064	35.376141
1188.152758	83132.060445	35.381159
1189.520846	83245.018855	35.386176
1190.659039	83366.616700	35.391194
1191.884193	83491.077725	35.396212
1193.323761	83595.321796	35.401229
1194.684667	83717.127214	35.406247
1196.079061	83827.461037	35.411264
1197.150388	83949.109790	35.416282
1198.389034	84062.585748	35.421300
1200.511385	84159.237216	35.426317
1201.416485	84261.983073	35.431335
1203.123979	84372.903809	35.436352
1204.115217	84476.739394	35.441370
1205.295122	84582.193211	35.446388
1206.804456	84689.053302	35.451405
1208.357972	84792.739157	35.456423
1209.146444	84896.544467	35.461440
1210.351222	84994.900125	35.466458
1211.215777	85110.440499	35.471476
1212.451719	85214.456073	35.476493
1213.800665	85321.318139	35.481511
1214.633232	85428.603103	35.486528
1216.028888	85550.043434	35.491546
1217.190016	85661.801802	35.496564
1218.669410	85771.521644	35.501581
1219.926722	85881.073725	35.506599
1221.193374	85990.460037	35.511616
1223.030019	86088.632372	35.516634
1224.352965	86190.002223	35.521652
1225.434318	86282.032983	35.526669
1226.612334	86389.381784	35.531687
1227.564024	86496.854913	35.536704
1228.754447	86605.228995	35.541722
1229.649884	86728.006635	35.546740
1231.138238	86838.071259	35.551757
1231.885534	86951.723768	35.556775
1233.198989	87052.844666	35.561792
1234.326196	87171.140216	35.566810
1235.642323	87299.215066	35.571828
1237.130253	87412.373922	35.576845
1238.136444	87529.257801	35.581863
1239.324088	87651.068765	35.586880
1240.477000	87761.049682	35.591898
1241.545390	87880.054230	35.596916
1242.682542	87990.608718	35.601933
1243.983191	88121.363452	35.606951
1245.062590	88232.586808	35.611968
1247.064840	88327.408025	35.616986
1248.474711	88448.009153	35.622004
1249.976233	88548.814467	35.627021
1250.925817	88657.727864	35.632039
1252.406607	88771.209882	35.637056
1253.637551	88874.580305	35.642074
1255.001849	88968.970628	35.647092
1256.123198	89064.400225	35.652109
1256.983451	89170.047135	35.657127
1257.866320	89270.051425	35.662144
1259.594826	89369.227411	35.667162
1260.203812	89471.467443	35.672180
1261.256066	89577.364724	35.677197
1262.420800	89685.488022	35.682215
1263.945875	89794.049881	35.687232
1265.808713	89901.330258	35.692250
1266.682657	90009.804154	35.697268
1268.182676	90119.068129	35.702285
1269.459660	90225.655116	35.707303
1270.397500	90336.312748	35.712320
1271.515199	90457.297026	35.717338
1272.822512	90579.000018	35.722356
1273.854744	90693.674462	35.727373
1274.855209	90823.271155	35.732391
1276.186825	90947.189744	35.737408
1277.949788	91062.981208	35.742426
1278.969307	91188.508241	35.747444
1280.158355	91312.336463	35.752461
1281.635885	91442.267129	35.757479
1282.430006	91568.109652	35.762496
1283.984907	91696.521171	35.767514
1285.120947	91830.042707	35.772532
1286.412600	91963.033647	35.777549
1287.617751	92094.771218	35.782567
1288.653352	92229.552217	35.787584
1290.324757	92366.465525	35.792602
1291.898839	92498.819164	35.797620
1293.366134	92633.484065	35.802637
1294.625657	92771.464585	35.807655
1296.073634	92894.460481	35.812672
1297.752873	93017.560298	35.817690
1298.750844	93155.418496	35.822708
1299.955945	93280.963327	35.827725
1301.080861	93410.678461	35.832743
1302.644491	93537.866953	35.837760
1304.189706	93669.203506	35.842778
1305.013768	93806.800185	35.847796
1306.480629	93927.046846	35.852813
1308.022506	94060.819181	35.857831
1309.382344	94207.092673	35.862848
1310.637152	94324.167107	35.867866
1311.856857	94463.264176	35.872884
1313.061449	94601.185429	35.877901
1314.731415	94729.794598	35.882919
1316.064779	94860.256589	35.887936
1317.774518	94991.142211	35.892954
1318.827863	95113.156359	35.897972
1319.918961	95247.472989	35.902989
1321.447505	95377.577216	35.908007
1322.856884	95500.285324	35.913024
1324.397573	95628.956373	35.918042
1325.411117	95766.088628	35.923060
1326.134927	95891.769692	35.928077
1328.001710	96034.994108	35.933095
1329.185609	96165.877791	35.938112
1330.326537	96285.018157	35.943130
1331.476850	96426.289714	35.948148
1333.492804	96548.032889	35.953165
1334.633112	96684.388880	35.958183
1336.050007	96826.267224	35.963200
1337.905297	96938.441109	35.968218
1339.127279	97056.557697	35.973236
1340.417234	97179.493800	35.978253
1341.842751	97308.950255	35.983271
1343.231777	97418.434991	35.988288
1345.547454	97501.839990	35.993306
1346.490455	97611.559612	35.998324
1347.683198	97712.937658	36.003341
1349.077239	97818.505973	36.008359
1350.054671	97928.272041	36.013376
1351.034748	98027.161560	36.018394
1352.455458	98144.008977	36.023412
1353.649769	98257.393299	36.028429
1355.262077	98378.496476	36.033447
1355.788690	98495.040663	36.038464
1357.506647	98613.225308	36.043482
1358.603180	98743.588176	36.048500
1359.911274	98870.977600	36.053517
1361.605629	98988.660233	36.058535
1362.599060	99127.255394	36.063552
1363.765119	99245.617021	36.068570
1365.109085	99389.153523	36.073588
1366.598955	99512.967613	36.078605
1368.163526	99644.960045	36.083623
1369.435697	99784.921834	36.088640
1371.258344	99902.765338	36.093658
1372.792421	100038.567333	36.098676
1374.559753	100161.630801	36.103693
1375.814446	100294.447452	36.108711
1376.926769	100420.998750	36.113728
1378.127688	100549.463746	36.118746
1379.579896	100674.758763	36.123764
1380.402862	100812.221364	36.128781
1381.980701	100946.752593	36.133799
1383.246645	101088.597302	36.138816
1384.847087	101221.021635	36.143834
1386.326765	101363.379423	36.148852
1388.126037	101499.019483	36.153869
1389.255205	101636.805567	36.158887
1390.364392	101791.317713	36.163904
1391.914270	101913.483493	36.168922
1393.218212	102069.881037	36.173940
1394.404283	102208.877778	36.178957
1396.080357	102336.616595	36.183975
1398.252496	102456.494203	36.188992
1400.103750	102587.858090	36.194010
1401.522158	102711.771566	36.199028
1402.715588	102852.088438	36.204045
1404.095550	102981.891728	36.209063
1405.654768	103108.852984	36.214080
1407.276549	103238.163215	36.219098
1408.059337	103363.661470	36.224116
1409.296419	103504.164496	36.229133
1410.782691	103641.041236	36.234151
1411.804518	103785.813671	36.239168
1413.279008	103917.444346	36.244186
1414.672939	104059.941253	36.249204
1415.805161	104203.138810	36.254221
1417.306422	104352.340129	36.259239
1418.743329	104510.135888	36.264256
1419.806548	104640.679631	36.269274
1420.914092	104789.804711	36.274292
1422.501212	104948.225794	36.279309
1424.067559	105084.487386	36.284327
1425.129012	105244.031387	36.289344
1426.628395	105404.027840	36.294362
1427.637467	105567.600912	36.299380
1429.476086	105727.393945	36.304397
1431.236104	105874.330145	36.309415
1432.292068	106022.543099	36.314432
1434.084308	106173.127330	36.319450
1435.236407	106324.179580	36.324468
1436.742143	106468.190864	36.329485
1438.259540	106595.362039	36.334503
1439.525958	106736.596772	36.339520
1441.030206	106870.301194	36.344538
1442.709399	107004.688994	36.349556
1443.760754	107150.625172	36.354573
1445.718613	107288.876188	36.359591
1446.876454	107434.188354	36.364608
1448.257168	107570.032336	36.369626
1449.917418	107714.012145	36.374644
1451.274427	107849.937005	36.379661
1452.791788	107997.655588	36.384679
1453.787318	108135.628664	36.389696
1455.493202	108278.880948	36.394714
1457.329331	108429.988188	36.399732
1458.896159	108565.870534	36.404749
1460.989388	108689.092259	36.409767
1462.475053	108837.909907	36.414784
1464.147308	108969.757641	36.419802
1465.616299	109107.610178	36.424820
1466.916616	109249.902459	36.429837
1468.717152	109377.661215	36.434855
1469.965963	109522.219828	36.439872
1471.626007	109652.778593	36.444890
1473.332547	109786.424789	36.449908
1474.432802	109921.915855	36.454925
1476.345884	110066.791807	36.459943
1477.676632	110202.641200	36.464960
1479.346020	110328.001732	36.469978
1480.801044	110468.182483	36.474996
1482.153407	110601.354297	36.480013
1483.364022	110737.630259	36.485031
1484.432668	110883.477983	36.490048
1485.775650	111027.711103	36.495066
1487.612531	111174.454977	36.500084
1488.836917	111332.797020	36.505101
1490.762515	111477.055425	36.510119
1491.837404	111622.993994	36.515136
1493.255268	111770.490367	36.520154
1494.994920	111925.749274	36.525172
1496.337159	112070.760339	36.530189
1497.760427	112221.301389	36.535207
1499.315223	112382.779843	36.540224
1500.805093	112519.919600	36.545242
1502.421775	112694.236739	36.550260
1503.644106	112856.453908	36.555277
1505.722488	113003.890609	36.560295
1506.775071	113151.538304	36.565312
1508.334486	113306.945391	36.570330
1509.714913	113469.254854	36.575348
1511.061199	113633.523455	36.580365
1513.315833	113787.048860	36.585383
1514.515829	113951.430450	36.590400
1516.017564	114101.269607	36.595418
1517.569783	114253.561960	36.600436
1518.721732	114409.836205	36.605453
1520.336640	114567.763919	36.610471
1521.791069	114733.897710	36.615488
1523.251872	114883.429384	36.620506
1524.720438	115057.096069	36.625524
1525.956578	115222.581176	36.630541
1527.861941	115379.630109	36.635559
1529.533822	115548.283038	36.640576
1530.912240	115713.202835	36.645594
1532.841511	115866.483228	36.650612
1534.338661	116020.186645	36.655629
1536.407036	116170.643650	36.660647
1537.861723	116317.987892	36.665664
1539.441782	116459.770555	36.670682
1540.265066	116592.450673	36.675700
1541.760575	116732.319650	36.680717
1543.684702	116868.101757	36.685735
1544.966278	117009.755404	36.690752
1546.713475	117151.742996	36.695770
1548.323808	117293.448020	36.700788
1549.836066	117430.108034	36.705805
1551.401172	117573.558831	36.710823
1552.974288	117716.958195	36.715840
1554.312131	117871.163347	36.720858
1555.721679	118006.078384	36.725876
1557.364513	118154.034781	36.730893
1558.967742	118296.340844	36.735911
1560.960296	118456.344565	36.740928
1561.649299	118610.869358	36.745946
1563.227231	118773.678728	36.750964
1564.542697	118931.417896	36.755981
1566.167156	119100.335232	36.760999
1567.746109	119260.317929	36.766016
1568.740923	119428.548290	36.771034
1570.419965	119615.065377	36.776052
1571.604357	119795.457626	36.781069
1573.280078	119966.692086	36.786087
1574.818118	120152.168229	36.791104
1576.466585	120332.719096	36.796122
1578.247733	120509.520838	36.801140
1579.511687	120698.530583	36.806157
1581.287700	120871.871826	36.811175
1583.064901	121062.693515	36.816192
1584.493507	121238.361075	36.821210
1586.577277	121418.595562	36.826228
1587.822087	121608.513361	36.831245
1589.990904	121788.102065	36.836263
1591.296404	121970.033197	36.841280
1593.059770	122150.358990	36.846298
1594.361805	122333.662364	36.851316
1596.386779	122528.270953	36.856333
1597.841206	122704.220162	36.861351
1599.382235	122885.852484	36.866368
1600.856620	123079.255565	36.871386
1602.624329	123255.386812	36.876404
1604.189143	123448.143338	36.881421
1606.449814	123634.906295	36.886439
1607.750135	123814.931190	36.891456
1609.213846	124010.420947	36.896474
1610.897637	124178.260083	36.901492
1612.629774	124374.864267	36.906509
1614.454983	124558.629310	36.911527
1616.048094	124743.699932	36.916544
1617.491965	124932.016926	36.921562
1619.448092	125108.786705	36.926580
1620.824197	125296.481637	36.931597
1622.495255	125472.320531	36.936615
1623.932082	125661.035298	36.941632
1625.678009	125847.977473	36.946650
1627.501963	126041.403870	36.951668
1628.928162	126219.555001	36.956685
1630.680855	126402.540453	36.961703
1632.609084	126587.960624	36.966720
1634.129334	126763.879316	36.971738
1635.867052	126938.546981	36.976756
1637.482315	127121.493600	36.981773
1639.095577	127302.436809	36.986791
1640.728919	127481.182839	36.991808
1642.119791	127671.994691	36.996826
1643.883017	127848.387678	37.001844
1645.514397	128024.675063	37.006861
1646.978683	128180.385195	37.011879
1648.815467	128341.671069	37.016896
1650.051496	128515.941361	37.021914
1652.088016	128683.921739	37.026932
1653.600954	128848.913933	37.031949
1655.188149	129021.050940	37.036967
1656.986608	129198.789023	37.041984
1658.033377	129367.129185	37.047002
1659.696738	129526.264353	37.052020
1660.956482	129722.663144	37.057037
1662.269589	129907.635595	37.062055
1664.013353	130095.307761	37.067072
1665.362416	130295.501636	37.072090
1666.907327	130489.461592	37.077108
1668.242410	130688.339948	37.082125
1670.059259	130894.224156	37.087143
1671.586968	131106.282694	37.092160
1672.740073	131323.831104	37.097178
1674.681229	131531.259661	37.102196
1676.516405	131749.338473	37.107213
1678.214252	131974.786300	37.112231
1679.822968	132179.326017	37.117248
1681.717071	132397.360855	37.122266
1683.496791	132610.504134	37.127284
1685.214924	132830.433739	37.132301
1687.203240	133047.721228	37.137319
1688.743422	133254.953959	37.142336
1690.262885	133492.872321	37.147354
1692.380575	133696.439017	37.152372
1694.217338	133925.923019	37.157389
1695.868069	134137.266582	37.162407
1697.466506	134351.893057	37.167424
1699.105857	134582.172520	37.172442
1700.883963	134794.565266	37.177460
1702.044228	135021.457426	37.182477
1704.544181	135253.788951	37.187495
1706.229126	135472.353706	37.192512
1707.734691	135697.393654	37.197530
1709.137385	135922.501492	37.202548
1711.201090	136152.101178	37.207565
1713.105374	136367.666780	37.212583
1715.236568	136590.456564	37.217600
1717.443369	136813.882845	37.222618
1718.801936	137027.341184	37.227636
1720.829627	137240.341060	37.232653
1722.762745	137460.107662	37.237671
1724.463934	137663.338347	37.242688
1726.334446	137888.497272	37.247706
1727.536981	138098.888504	37.252724
1729.654775	138322.500936	37.257741
1731.120274	138543.957114	37.262759
1733.168711	138754.549603	37.267776
1734.270103	138983.158379	37.272794
1736.245927	139196.721001	37.277812
1738.112687	139413.664529	37.282829
1739.844334	139643.815492	37.287847
1741.429940	139858.990091	37.292864
1742.687482	140088.100239	37.297882
1744.311937	140317.497034	37.302900
1745.599400	140552.366322	37.307917
1747.084604	140783.842933	37.312935
1749.404558	141012.043415	37.317952
1750.898538	141247.594661	37.322970
1752.885225	141482.055099	37.327988
1754.348948	141717.359532	37.333005
1756.214931	141953.478187	37.338023
1758.032409	142187.866854	37.343040
1759.483014	142427.923265	37.348058
1761.616356	142646.616715	37.353076
1763.617858	142859.874392	37.358093
1764.615156	143075.332602	37.363111
1766.116402	143299.191202	37.368128
1768.005827	143534.818880	37.373146
1770.106315	143743.064527	37.378164
1771.649816	143980.423450	37.383181
1773.208038	144210.800794	37.388199
1774.614319	144446.139935	37.393216
1776.808359	144680.532611	37.398234
1778.244633	144909.003000	37.403252
1780.263484	145154.352838	37.408269
1781.796783	145404.526237	37.413287
1783.446342	145634.883207	37.418304
1785.413769	145880.955326	37.423322
1787.247575	146134.169731	37.428340
1789.204673	146381.997394	37.433357
1790.987316	146615.955366	37.438375
1792.950658	146865.180543	37.443392
1794.606358	147118.402141	37.448410
1796.681987	147369.198826	37.453428
1798.356292	147623.245007	37.458445
1799.869920	147882.864095	37.463463
1801.862663	148129.564948	37.468480
1803.364136	148396.727909	37.473498
1805.371247	148655.322068	37.478516
1807.260870	148915.953940	37.483533
1808.556454	149169.139971	37.488551
1810.429178	149436.453496	37.493568
1812.297541	149709.074724	37.498586
1814.477298	149964.297430	37.503604
1816.019388	150237.162522	37.508621
1818.112351	150506.846117	37.513639
1820.485536	150769.290359	37.518656
1822.705099	151017.149756	37.523674
1825.006112	151274.327248	37.528692
1827.196308	151518.893217	37.533709
1828.682869	151762.795486	37.538727
1830.908943	152012.930523	37.543744
1832.389376	152281.664656	37.548762
1834.108593	152536.729914	37.553780
1836.266152	152792.845171	37.558797
1837.823648	153042.606548	37.563815
1840.288050	153279.762530	37.568832
1842.316114	153534.365383	37.573850
1844.285852	153768.439634	37.578868
1846.212515	154012.752934	37.583885
1847.936751	154256.743358	37.588903
1849.937601	154501.212237	37.593920
1851.562366	154739.228583	37.598938
1853.179535	154987.719841	37.603956
1854.945261	155235.173509	37.608973
1856.937831	155487.721448	37.613991
1858.409763	155735.476871	37.619008
1859.791558	155994.355024	37.624026
1861.363453	156255.857892	37.629044
1863.349521	156512.486227	37.634061
1864.557534	156777.196305	37.639079
1866.599904	157053.355262	37.644096
1868.460337	157322.701359	37.649114
1870.298699	157593.067696	37.654132
1872.113974	157869.075366	37.659149
1873.675625	158146.532916	37.664167
1875.620570	158417.483046	37.669184
1877.365564	158705.971955	37.674202
1879.095670	158990.173613	37.679220
1880.416179	159271.380813	37.684237
1881.816780	159561.184190	37.689255
1883.684689	159834.882083	37.694272
1885.466189	160128.640553	37.699290
1887.183116	160403.964073	37.704308
1888.843352	160688.679563	37.709325
1890.773511	160964.492884	37.714343
1892.638189	161255.628444	37.719360
1894.427316	161548.554491	37.724378
1896.289865	161845.317254	37.729396
1897.893504	162130.733627	37.734413
1899.492980	162435.728825	37.739431
1901.563891	162752.713156	37.744448
1903.349251	163063.712926	37.749466
1905.317733	163365.062140	37.754484
1907.430743	163669.640437	37.759501
1909.334911	163990.490952	37.764519
1910.886971	164296.848041	37.769536
1912.845057	164621.743304	37.774554
1914.557012	164952.429872	37.779572
1916.659708	165271.376631	37.784589
1918.497059	165609.499671	37.789607
1920.541871	165940.266254	37.794624
1922.730995	166268.244145	37.799642
1924.450209	166593.668550	37.804660
1926.845438	166918.798834	37.809677
1928.363964	167247.203178	37.814695
1931.188252	167576.904069	37.819712
1933.330725	167905.189011	37.824730
1935.314921	168233.614391	37.829748
1937.942512	168543.314755	37.834765
1939.798645	168861.580033	37.839783
1942.364896	169175.787428	37.844800
1944.371944	169486.769283	37.849818
1946.296383	169795.924245	37.854836
1948.296870	170107.595431	37.859853
1949.730075	170417.032635	37.864871
1951.804629	170737.379900	37.869888
1954.015917	171055.028128	37.874906
1955.821905	171376.334163	37.879924
1957.735648	171695.466236	37.884941
1959.791710	172014.983833	37.889959
1961.899727	172329.948957	37.894976
1964.029951	172649.343405	37.899994
1965.913525	172969.399758	37.905012
1968.398665	173278.151707	37.910029
1970.210684	173579.479854	37.915047
1972.362433	173874.153413	37.920064
1974.829756	174197.984120	37.925082
1976.711317	174511.926735	37.930100
1978.529533	174812.687234	37.935117
1979.878100	175133.838826	37.940135
1981.875423	175454.306621	37.945152
1983.754325	175773.714774	37.950170
1985.236358	176105.261930	37.955188
1986.933879	176432.091237	37.960205
1988.694200	176768.524676	37.965223
1990.586772	177101.764308	37.970240
1992.501086	177439.497118	37.975258
1994.217028	177788.360602	37.980276
1996.232623	178132.201072	37.985293
1997.991829	178480.120969	37.990311
2000.024511	178808.875611	37.995328
2003.195178	179131.257454	38.000346
2006.172039	179454.381778	38.005364
2008.855839	179760.358805	38.010381
2010.682530	180087.143909	38.015399
2012.533690	180393.963839	38.020416
2014.753840	180709.616605	38.025434
2016.253121	181033.535372	38.030452
2018.130087	181329.890556	38.035469
2019.766396	181624.277710	38.040487
2021.586113	181919.881767	38.045504
2023.155947	182233.685347	38.050522
2024.793994	182545.422106	38.055540
2026.698926	182860.750325	38.060557
2028.324468	183191.946294	38.065575
2030.235818	183524.318060	38.070592
2032.066747	183845.223319	38.075610
2034.498501	184175.713033	38.080628
2036.691244	184513.886093	38.085645
2038.383809	184843.400947	38.090663
2040.721559	185178.048666	38.095680
2042.546113	185502.846352	38.100698
2044.513992	185859.828850	38.105716
2046.158376	186269.439313	38.110733
2048.199180	186632.280373	38.115751
2049.795310	186970.427497	38.120768
2051.900183	187334.810390	38.125786
2054.182278	187705.948640	38.130804
2056.203998	188074.741134	38.135821
2058.267837	188437.533996	38.140839
2059.707764	188802.279353	38.145856
2061.538974	189175.067592	38.150874
2063.353524	189570.846670	38.155892
2065.182259	189956.871301	38.160909
2067.169278	190358.595317	38.165927
2068.958003	190768.987687	38.170944
2071.093682	191167.694149	38.175962
2072.801878	191578.940107	38.180980
2075.098618	191990.019690	38.185997
2077.042481	192414.770323	38.191015
2079.602695	192820.502991	38.196032
2081.553719	193231.894573	38.201050
2083.658428	193652.230097	38.206068
2085.690913	194073.187880	38.211085
2087.992024	194490.549093	38.216103
2089.898522	194914.704355	38.221120
2092.449705	195332.384949	38.226138
2094.803331	195758.530819	38.231156
2097.046652	196172.019922	38.236173
2099.064888	196596.290104	38.241191
2101.279510	197005.061496	38.246208
2103.572394	197428.478603	38.251226
2105.696756	197851.948588	38.256244
2108.150527	198255.758407	38.261261
2111.153962	198670.431960	38.266279
2113.345913	199075.148410	38.271296
2116.163806	199463.079455	38.276314
2118.639487	199861.377942	38.281332
2121.019163	200245.619644	38.286349
2123.297475	200639.048212	38.291367
2125.076300	201019.397145	38.296384
2127.252140	201404.384586	38.301402
2130.009631	201784.760786	38.306420
2132.242334	202155.973059	38.311437
2134.505231	202532.109500	38.316455
2136.305996	202918.505058	38.321472
2138.237731	203277.674984	38.326490
2140.088990	203666.452132	38.331508
2142.204061	204042.386129	38.336525
2144.411100	204428.061192	38.341543
2146.608593	204817.320307	38.346560
2148.783495	205202.112832	38.351578
2150.427993	205585.388277	38.356596
2152.532419	205965.569934	38.361613
2154.929051	206353.530917	38.366631
2156.623976	206734.616013	38.371648
2159.301507	207092.533749	38.376666
2160.860457	207465.995000	38.381684
2162.862667	207842.080623	38.386701
2164.638772	208198.844877	38.391719
2166.375248	208575.684351	38.396736
2168.402859	208951.666216	38.401754
2170.076303	209343.555411	38.406772
2172.135380	209731.904963	38.411789
2173.987051	210142.185058	38.416807
2175.507211	210540.755636	38.421824
2177.910795	210952.170464	38.426842
2179.867928	211375.569607	38.431860
2181.925228	211800.122359	38.436877
2183.929075	212231.339774	38.441895
2186.341877	212646.591540	38.446912
2188.514441	213067.292219	38.451930
2190.622141	213510.130102	38.456948
2192.522364	213946.040267	38.461965
2194.888348	214387.721350	38.466983
2196.562399	214849.376376	38.472000
2199.334569	215288.531184	38.477018
2201.062503	215749.721658	38.482036
2203.481182	216211.618082	38.487053
2205.821371	216656.760698	38.492071
2208.314466	217111.762066	38.497088
2210.643202	217567.399152	38.502106
2213.165554	218030.170430	38.507124
2215.308964	218470.925082	38.512141
2217.655728	218912.308942	38.517159
2220.093241	219382.817361	38.522176
2222.790795	219836.595246	38.527194
2224.708987	220305.584702	38.532212
2226.963335	220764.284326	38.537229
2229.026239	221224.563654	38.542247
2230.922190	221689.314914	38.547264
2233.612107	222159.125261	38.552282
2235.371752	222624.609470	38.557300
2237.704533	223102.274825	38.562317
2239.997794	223568.235204	38.567335
2241.725807	224051.710879	38.572352
2244.171972	224524.176539	38.577370
2246.079273	225012.832334	38.582388
2248.430784	225497.430605	38.587405
2250.852045	225983.135824	38.592423
2252.846361	226473.912089	38.597440
2255.826945	226942.966754	38.602458
2258.497355	227429.623861	38.607476
2261.246789	227902.321737	38.612493
2264.067026	228369.724436	38.617511
2265.938805	228845.099062	38.622528
2268.499976	229308.781985	38.627546
2270.786133	229776.775408	38.632564
2273.178925	230246.504906	38.637581
2275.691741	230705.037718	38.642599
2278.132523	231178.392032	38.647616
2280.627864	231634.818504	38.652634
2282.684080	232086.816518	38.657652
2285.279167	232551.051281	38.662669
2287.533425	233009.749868	38.667687
2289.553738	233470.567617	38.672704
2291.518991	233936.880782	38.677722
2293.808079	234400.907582	38.682740
2295.907732	234866.690875	38.687757
2298.399104	235328.094081	38.692775
2300.504034	235801.166469	38.697792
2303.155489	236263.051815	38.702810
2305.086469	236729.443590	38.707828
2307.160292	237181.408659	38.712845
2309.702231	237624.180395	38.717863
2311.808352	238062.700774	38.722880
2314.275724	238512.418156	38.727898
2316.114846	238962.054860	38.732916
2318.655488	239405.078439	38.737933
2320.288904	239852.662763	38.742951
2322.227025	240319.429396	38.747968
2324.786842	240776.623037	38.752986
2326.547062	241246.286388	38.758004
2328.929611	241720.704095	38.763021
2331.361065	242190.820166	38.768039
2333.127080	242675.417137	38.773056
2335.625458	243152.837089	38.778074
2338.110904	243630.232686	38.783092
2340.740199	244110.297631	38.788109
2343.045415	244597.423214	38.793127
2345.729908	245074.098877	38.798144
2348.371757	245548.316028	38.803162
2351.030328	246035.891387	38.808180
2353.107525	246527.188646	38.813197
2355.654288	247013.102442	38.818215
2357.539178	247504.477980	38.823232
2360.226925	247998.877215	38.828250
2362.418541	248496.070405	38.833268
2364.779246	248986.148633	38.838285
2367.555658	249478.243801	38.843303
2369.575087	249985.950776	38.848320
2372.154724	250485.338730	38.853338
2374.223926	250983.610717	38.858356
2376.383346	251497.082973	38.863373
2378.860890	252006.566763	38.868391
2381.394054	252516.954704	38.873408
2384.073360	253023.330119	38.878426
2386.590529	253539.457922	38.883444
2389.246162	254045.300114	38.888461
2391.450399	254557.789789	38.893479
2393.143420	255084.023158	38.898496
2395.819124	255598.823418	38.903514
2398.605596	256121.097883	38.908532
2400.852355	256642.260465	38.913549
2402.923130	257162.737160	38.918567
2405.315314	257688.749973	38.923584
2407.948847	258209.490495	38.928602
2410.662073	258741.443598	38.933620
2412.768691	259273.133218	38.938637
2415.626754	259796.880223	38.943655
2417.920455	260323.710026	38.948672
2420.636755	260846.788679	38.953690
2423.172380	261378.986373	38.958708
2425.064863	261907.293882	38.963725
2428.134250	262430.361186	38.968743
2430.630174	262950.848303	38.973760
2433.111186	263480.885572	38.978778
2435.344697	263995.236428	38.983796
2437.607678	264523.422936	38.988813
2440.293407	265062.361129	38.993831
2442.161308	265598.223509	38.998848
2444.460823	266127.107382	39.003866
2447.131249	266670.890747	39.008884
2449.248807	267220.116342	39.013901
2451.644031	267749.103745	39.018919
2453.920781	268306.451454	39.023936
2456.366132	268849.597412	39.028954
2458.766062	269393.610875	39.033972
2461.254523	269946.776107	39.038989
2464.807248	270461.573945	39.044007
2467.028717	271005.148559	39.049024
2469.806633	271524.251595	39.054042
2472.685949	272037.189648	39.059060
2475.019741	272536.418870	39.064077
2477.788387	273028.415562	39.069095
2480.161116	273528.699715	39.074112
2483.594880	273999.863360	39.079130
2486.975127	274459.553377	39.084148
2489.564394	274926.195664	39.089165
2492.240596	275394.828128	39.094183
2494.157224	275872.464850	39.099200
2496.559252	276345.756681	39.104218
2499.004721	276830.086257	39.109236
2500.769923	277318.023400	39.114253
2503.144741	277793.088626	39.119271
2505.596564	278298.664468	39.124288
2507.716972	278789.051363	39.129306
2509.800891	279296.176281	39.134324
2511.897226	279808.832024	39.139341
2514.512071	280315.969098	39.144359
2516.228218	280846.910472	39.149376
2518.604508	281383.535270	39.154394
2521.112180	281912.949107	39.159412
2522.983766	282464.855729	39.164429
2525.808137	283010.566093	39.169447
2528.320350	283571.811059	39.174464
2530.449152	284125.645534	39.179482
2532.915171	284694.532199	39.184500
2535.153418	285264.313013	39.189517
2537.742203	285839.849532	39.194535
2539.780306	286417.676049	39.199552
2542.351262	287005.622471	39.204570
2544.727434	287611.622532	39.209588
2546.939211	288220.791233	39.214605
2549.783333	288816.118903	39.219623
2552.298755	289421.877404	39.224640
2554.576933	290037.036504	39.229658
2557.409234	290645.857222	39.234676
2560.185630	291269.559772	39.239693
2562.541896	291887.278517	39.244711
2565.387777	292511.643325	39.249728
2568.509625	293128.189467	39.254746
2571.485386	293739.013985	39.259764
2573.711865	294344.591711	39.264781
2576.888844	294952.528903	39.269799
2579.829772	295566.589932	39.274816
2582.645304	296182.035026	39.279834
2585.215332	296785.223778	39.284852
2588.452033	297373.755015	39.289869
2591.145299	297974.957170	39.294887
2593.802251	298580.423717	39.299904
2596.569692	299183.327797	39.304922
2599.124964	299771.381507	39.309940
2601.827974	300378.547647	39.314957
2604.629625	300954.872405	39.319975
2607.666538	301547.706307	39.324992
2610.103261	302138.367734	39.330010
2612.880863	302720.592294	39.335028
2615.613254	303293.678735	39.340045
2618.374771	303879.650084	39.345063
2620.689324	304467.994448	39.350080
2623.343372	305049.831618	39.355098
2625.986373	305630.445487	39.360116
2628.180696	306233.282846	39.365133
2630.761957	306809.272993	39.370151
2633.368806	307400.888775	39.375168
2635.713441	308002.260105	39.380186
2638.461814	308593.484340	39.385204
2640.424780	309193.123793	39.390221
2642.826650	309789.413294	39.395239
2645.334252	310378.825911	39.400256
2647.542013	310966.552040	39.405274
2649.925360	311528.151675	39.410292
2652.803667	312107.815064	39.415309
2655.549989	312700.207599	39.420327
2657.864018	313287.127017	39.425344
2660.353171	313893.935113	39.430362
2663.072864	314485.217773	39.435380
2665.530536	315084.934177	39.440397
2668.487813	315685.707018	39.445415
2670.909515	316295.107867	39.450432
2673.494605	316901.099734	39.455450
2675.757526	317521.370587	39.460468
2678.251479	318140.759377	39.465485
2680.612105	318776.376306	39.470503
2683.418583	319415.746556	39.475520
2685.934900	320049.569742	39.480538
2688.712535	320699.989731	39.485556
2691.507440	321349.762795	39.490573
2693.890177	322003.066533	39.495591
2696.511233	322664.366984	39.500608
2699.221871	323342.491820	39.505626
2701.909270	324001.299540	39.510644
2705.116958	324668.541422	39.515661
2708.019241	325329.476698	39.520679
2711.653527	325990.718735	39.525696
2714.066957	326647.344605	39.530714
2717.218704	327292.528952	39.535732
2719.651095	327965.140199	39.540749
2722.719593	328627.035931	39.545767
2725.562595	329285.733603	39.550784
2728.488544	329950.293288	39.555802
2731.224250	330609.619706	39.560820
2734.255637	331287.180377	39.565837
2736.707042	331943.052728	39.570855
2739.168763	332607.842045	39.575872
2741.628935	333288.804948	39.580890
2744.678665	333973.392937	39.585908
2747.127240	334646.494544	39.590925
2749.848431	335327.633650	39.595943
2752.296882	336012.404754	39.600960
2755.194357	336707.924537	39.605978
2757.935167	337393.436192	39.610996
2760.804648	338077.494514	39.616013
2763.165252	338773.515061	39.621031
2766.038138	339481.287426	39.626048
2768.602790	340184.731263	39.631066
2771.362471	340885.822826	39.636084
2773.914907	341601.719060	39.641101
2776.687003	342310.236943	39.646119
2780.123531	343009.887377	39.651136
2782.894086	343719.949245	39.656154
2785.891159	344423.697249	39.661172
2788.413343	345132.881015	39.666189
2791.293931	345845.164186	39.671207
2794.455676	346554.624536	39.676224
2797.332237	347263.886111	39.681242
2800.266721	347963.208790	39.686260
2803.036358	348667.943528	39.691277
2805.986612	349374.080499	39.696295
2809.125120	350078.499531	39.701312
2812.071955	350783.871394	39.706330
2815.088698	351463.152135	39.711348
2817.903871	352156.217485	39.716365
2821.185376	352854.367555	39.721383
2823.968041	353551.058829	39.726400
2826.497055	354239.889606	39.731418
2829.367666	354923.936722	39.736436
2832.128874	355584.865222	39.741453
2834.818875	356244.295145	39.746471
2837.227877	356890.673897	39.751488
2839.416170	357562.144837	39.756506
2842.570675	358223.615172	39.761524
2845.422430	358899.922216	39.766541
2847.949926	359568.127890	39.771559
2850.956510	360236.852674	39.776576
2853.354397	360921.524845	39.781594
2856.107246	361598.192662	39.786612
2858.718585	362287.286849	39.791629
2861.496699	362983.866791	39.796647
2864.768310	363673.054202	39.801664
2867.652626	364370.852184	39.806682
2870.366758	365066.404454	39.811700
2873.441932	365759.222931	39.816717
2876.305130	366475.246336	39.821735
2879.540494	367182.805896	39.826752
2881.949873	367899.954234	39.831770
2885.075857	368604.353412	39.836788
2887.930890	369336.220601	39.841805
2890.818690	370058.181410	39.846823
2893.625333	370769.874149	39.851840
2896.218329	371504.589062	39.856858
2899.092178	372233.033245	39.861876
2902.301505	372963.128997	39.866893
2905.172790	373697.767867	39.871911
2908.231335	374432.864655	39.876928
2910.987233	375177.185271	39.881946
2914.265434	375905.342461	39.886964
2917.551917	376655.240104	39.891981
2920.793205	377393.242886	39.896999
2923.860221	378126.692704	39.902016
2927.066648	378861.747178	39.907034
2930.025951	379595.603872	39.912052
2933.039259	380317.020141	39.917069
2936.055386	381061.541666	39.922087
2938.923824	381792.564930	39.927104
2942.648311	382510.998537	39.932122
2946.754406	383217.145202	39.937140
2949.977069	383933.565849	39.942157
2952.548647	384645.965065	39.947175
2955.421860	385358.424103	39.952192
2958.488440	386086.128903	39.957210
2961.280092	386795.242820	39.962228
2964.234379	387514.237996	39.967245
2966.762485	388236.748003	39.972263
2970.141324	388950.571450	39.977280
2972.923040	389668.645213	39.982298
2976.022661	390382.091107	39.987316
2978.752040	391105.195214	39.992333
2981.864398	391836.776009	39.997351
2984.633927	392553.552140	40.002368
2987.791241	393277.031710	40.007386
2990.911339	393994.318328	40.012404
2993.779198	394727.419611	40.017421
2996.742294	395455.927064	40.022439
3000.009640	396182.896761	40.027456
3002.967357	396913.689374	40.032474
3005.910975	397647.600348	40.037492
3009.087471	398372.542626	40.042509
3011.647720	399092.850641	40.047527
3014.693734	399817.616654	40.052544
3017.208041	400560.513520	40.057562
3019.909229	401294.398386	40.062580
3023.363581	402031.989453	40.067597
3026.327585	402780.515001	40.072615
3029.179972	403497.957915	40.077632
3031.768140	404209.042498	40.082650
3034.928801	404927.505775	40.087668
3037.402940	405634.970150	40.092685
3039.845175	406364.632973	40.097703
3043.164226	407083.559464	40.102720
3045.482589	407809.297992	40.107738
3048.535113	408542.185044	40.112756
3051.970184	409278.631419	40.117773
3054.712913	410015.616319	40.122791
3057.935518	410756.903609	40.127808
3060.753479	411506.880238	40.132826
3063.788763	412257.404342	40.137844
3067.075619	413005.131485	40.142861
3069.919781	413772.479281	40.147879
3073.091261	414531.452624	40.152896
3076.321975	415315.378650	40.157914
3079.077317	416071.327041	40.162932
3082.525070	416835.688983	40.167949
3086.126505	417611.582020	40.172967
3088.929145	418380.945190	40.177984
3092.363042	419153.418766	40.183002
3095.484840	419942.197027	40.188020
3099.032262	420705.896834	40.193037
3101.959835	421487.263230	40.198055
3105.144836	422257.687945	40.203072
3108.432962	423063.463857	40.208090
3111.014154	423838.625832	40.213108
3114.174594	424650.679556	40.218125
3116.878228	425451.294830	40.223143
3119.639084	426252.223439	40.228160
3122.953042	427072.902603	40.233178
3125.959623	427879.491544	40.238196
3128.995234	428692.412944	40.243213
3131.730189	429527.286477	40.248231
3135.394819	430348.180724	40.253248
3138.550297	431171.040792	40.258266
3141.793320	431997.896263	40.263284
3145.191100	432836.822604	40.268301
3148.015842	433666.401784	40.273319
3151.487101	434501.100750	40.278336
3154.320325	435346.070962	40.283354
3157.848479	436180.183113	40.288372
3162.244492	436989.566265	40.293389
3166.050885	437801.886970	40.298407
3170.231838	438596.885363	40.303424
3173.814008	439406.999684	40.308442
3176.941037	440202.094624	40.313460
3180.158220	440994.262318	40.318477
3182.786756	441792.449183	40.323495
3186.208599	442590.023846	40.328512
3189.788262	443387.539748	40.333530
3193.139460	444175.459802	40.338548
3196.787622	444951.834525	40.343565
3199.569754	445756.190885	40.348583
3203.246026	446525.272249	40.353600
3206.324035	447312.544631	40.358618
3209.238494	448097.636892	40.363636
3212.204184	448884.656599	40.368653
3215.006273	449679.140831	40.373671
3217.992539	450473.005903	40.378688
3221.065762	451281.666700	40.383706
3223.705223	452076.625415	40.388724
3226.624218	452889.730802	40.393741
3229.322264	453715.454358	40.398759
3232.651306	454544.827278	40.403776
3235.653288	455368.709747	40.408794
3238.579071	456184.287118	40.413812
3241.668817	457000.608504	40.418829
3245.030856	457807.915620	40.423847
3248.473978	458595.741544	40.428864
3252.230033	459381.110871	40.433882
3255.500732	460161.120093	40.438900
3259.070929	460940.340779	40.443917
3262.322168	461730.828392	40.448935
3265.001564	462509.762855	40.453952
3267.993050	463316.616280	40.458970
3271.171258	464123.957192	40.463988
3274.636031	464909.470307	40.469005
3277.732295	465726.181586	40.474023
3281.061137	466530.810582	40.479040
3284.916817	467331.283283	40.484058
3287.942674	468150.056058	40.489076
3291.509122	468958.919077	40.494093
3294.607031	469782.492496	40.499111
3297.823702	470605.148866	40.504128
3300.731024	471432.754435	40.509146
3303.862381	472270.621220	40.514164
3307.373217	473098.300581	40.519181
3310.338289	473958.546069	40.524199
3313.083965	474802.040146	40.529216
3316.524195	475667.818259	40.534234
3319.306052	476542.626166	40.539252
3322.639772	477416.443379	40.544269
3325.787128	478303.096318	40.549287
3329.252387	479189.751139	40.554304
3332.168703	480083.901600	40.559322
3335.751929	480983.592999	40.564340
3338.964740	481882.433764	40.569357
3341.808029	482799.473337	40.574375
3345.227526	483715.663862	40.579392
3348.488217	484646.942053	40.584410
3351.854567	485574.016097	40.589428
3355.546041	486505.014551	40.594445
3359.270191	487429.956237	40.599463
3363.184549	488353.855291	40.604480
3366.797196	489269.886917	40.609498
3370.530603	490199.394514	40.614516
3373.641484	491109.398985	40.619533
3377.638574	492045.904375	40.624551
3380.567170	492966.703966	40.629568
3384.244289	493893.675771	40.634586
3387.520967	494822.263738	40.639604
3391.114601	495740.774559	40.644621
3394.528128	496662.982387	40.649639
3398.089375	497598.703252	40.654656
3401.465869	498515.212542	40.659674
3404.643936	499452.888704	40.664692
3408.426322	500371.282607	40.669709
3412.119179	501317.517479	40.674727
3415.428192	502245.983707	40.679744
3419.014329	503172.787062	40.684762
3422.565019	504105.373926	40.689780
3425.964515	505029.016971	40.694797
3429.537207	505949.202180	40.699815
3433.432948	506875.114212	40.704832
3437.160767	507789.873305	40.709850
3440.477611	508704.486348	40.714868
3444.105170	509612.100061	40.719885
3447.833907	510537.647350	40.724903
3451.432435	511447.058448	40.729920
3454.590228	512343.553195	40.734938
3457.925046	513274.211205	40.739956
3461.127204	514183.153305	40.744973
3464.607641	515087.366192	40.749991
3468.560386	515988.680812	40.755008
3472.099574	516873.477640	40.760013
3475.524696	517729.129517	40.765018
3479.024375	518538.750778	40.770023
3482.032198	519290.442897	40.775028
3484.653143	519994.076529	40.780032
3488.185523	520641.797302	40.785037
3490.820908	521225.983212	40.790042
3493.874540	521760.798603	40.795047
3496.063450	522235.514975	40.800052
3498.405120	522678.750394	40.805056
3500.268108	523065.464677	40.810061
3502.120513	523410.553495	40.815066
3503.445150	523697.776937	40.820071
3504.986898	523953.069580	40.825076
3506.416144	524182.076682	40.830080
3508.117337	524363.731746	40.835085
3509.310523	524514.279177	40.840090
3510.413096	524627.911990	40.845095
3511.512933	524706.884449	40.850100
3512.137128	524764.167403	40.855104
3513.079508	524797.672886	40.860109
3513.484623	524807.937214	40.865114
3514.701037	524800.392853	40.870119
3515.114170	524778.918195	40.875124
3515.858897	524720.817788	40.880128
3516.254559	524654.005697	40.885133
3516.698483	524582.299082	40.890138
3516.952925	524464.575602	40.895143
3517.590046	524353.794221	40.900148
3518.003541	524218.159256	40.905152
3518.565050	524077.965678	40.910157
3519.018188	523924.134348	40.915162
3519.248057	523756.078102	40.920167
3518.873841	523587.559548	40.925172
3519.249439	523398.567630	40.930176
3519.511022	523212.462640	40.935181
3519.600339	523014.843930	40.940186
3519.685495	522816.819879	40.945191
3519.697575	522607.870612	40.950196
3519.399742	522388.687499	40.955200
3519.696708	522186.791838	40.960205
3519.684312	521962.216319	40.965210
3520.045704	521740.551831	40.970215
3519.599633	521520.269093	40.975220
3519.707360	521297.175491	40.980224
3519.487998	521063.294965	40.985229
3519.455223	520834.974890	40.990234
3519.322787	520599.157901	40.995239
3519.747695	520361.284708	41.000244
3519.039777	520130.638900	41.005248
3519.133734	519894.068878	41.010253
3519.032405	519659.742570	41.015258
3519.301197	519420.818852	41.020263
3519.047257	519184.542595	41.025268
3518.650724	518944.605278	41.030272
3518.813226	518707.953546	41.035277
3518.675647	518474.570063	41.040282
3518.708684	518232.436516	41.045287
3518.350337	518001.649792	41.050292
3518.177383	517761.354444	41.055296
3518.297923	517521.362031	41.060301
3517.595658	517296.010189	41.065306
3517.756201	517059.783858	41.070311
3517.627048	516839.224716	41.075316
3517.348883	516603.411641	41.080320
3517.329443	516369.368967	41.085325
3516.693950	516151.851687	41.090330
3517.046547	515929.438634	41.095335
3516.587051	515710.727551	41.100340
3516.678171	515485.071285	41.105344
3516.651397	515253.480962	41.110349
3515.999753	515050.820570	41.115354
3516.355136	514826.322332	41.120359
3516.203035	514620.250537	41.125364
3515.680223	514403.393940	41.130368
3515.918020	514183.693081	41.135373
3515.458024	513986.936437	41.140378
3515.254300	513768.053954	41.145383
3514.903040	513563.257875	41.150388
3514.861173	513352.259421	41.155392
3515.187728	513160.108106	41.160397
3514.583370	512964.115728	41.165402
3514.941484	512764.693394	41.170407
3514.238672	512563.164281	41.175412
3514.425320	512365.477282	41.180416
3514.594982	512173.841005	41.185421
3514.374471	511990.280337	41.190426
3513.800754	511783.626973	41.195431
3513.537860	511604.555689	41.200436
3513.827878	511406.939886	41.205440
3513.403744	511224.863224	41.210445
3513.073425	511054.115908	41.215450
3513.253060	510866.090973	41.220455
3513.082083	510695.163201	41.225460
3512.700449	510514.482713	41.230464
3512.977204	510328.553520	41.235469
3512.358496	510160.412162	41.240474
3511.996079	509992.783659	41.245479
3512.688668	509832.957310	41.250484
3512.312958	509659.628040	41.255488
3512.532683	509484.791835	41.260493
3512.023128	509332.207587	41.265498
3512.451420	509159.957477	41.270503
3512.750458	508987.927122	41.275508
3511.972705	508822.871100	41.280512
3512.197540	508653.521328	41.285517
3511.963527	508492.613510	41.290522
3512.044822	508327.619771	41.295527
3511.575574	508169.468524	41.300532
3511.204835	508008.021648	41.305536
3511.469014	507843.750396	41.310541
3511.074649	507689.415538	41.315546
3510.675113	507539.316816	41.320551
3510.934191	507393.098868	41.325556
3510.903604	507238.954707	41.330560
3511.029785	507087.155263	41.335565
3510.631753	506947.138487	41.340570
3510.317204	506791.116834	41.345575
3510.189702	506657.158740	41.350580
3510.202184	506517.225182	41.355584
3509.703194	506372.325368	41.360589
3509.534203	506245.432120	41.365594
3509.852976	506118.562733	41.370599
3509.945180	505990.214092	41.375604
3509.700076	505855.863198	41.380608
3509.611141	505708.471393	41.385613
3509.640999	505582.651146	41.390618
3509.375316	505454.555174	41.395623
3509.250048	505325.729926	41.400628
3508.915384	505198.600916	41.405632
3509.414883	505081.128140	41.410637
3509.001360	504964.250527	41.415642
3508.828281	504829.828336	41.420647
3509.138156	504703.300934	41.425652
3508.506640	504587.866791	41.430656
3508.909606	504467.124690	41.435661
3508.722431	504358.279147	41.440666
3509.081085	504230.175978	41.445671
3508.741824	504107.881432	41.450676
3508.651453	504000.884867	41.455680
3509.044983	503871.965831	41.460685
3508.571504	503772.040224	41.465690
3508.512922	503639.859504	41.470695
3508.694594	503524.542546	41.475700
3508.641599	503409.109816	41.480704
3508.463251	503296.571636	41.485709
3508.146766	503183.700881	41.490714
3508.417939	503065.641702	41.495719
3507.942534	502959.100966	41.500724
3507.941319	502853.545253	41.505728
3507.731602	502740.048927	41.510733
3507.566265	502641.631713	41.515738
3507.872272	502521.090228	41.520743
3507.945341	502431.010555	41.525748
3507.699583	502328.516577	41.530752
3508.118401	502226.675347	41.535757
3507.587402	502128.362001	41.540762
3507.753302	502007.938965	41.545767
3507.542450	501914.166212	41.550772
3507.214901	501812.084989	41.555776
3507.384935	501715.678182	41.560781
3506.986326	501620.469374	41.565786
3507.110201	501504.691149	41.570791
3507.415730	501414.770833	41.575796
3507.116351	501320.049233	41.580800
3507.114241	501217.156244	41.585805
3506.830306	501139.537951	41.590810
3506.890549	501043.698863	41.595815
3506.849765	500956.201382	41.600820
3506.587523	500863.994216	41.605824
3506.817389	500764.846732	41.610829
3506.691190	500689.371459	41.615834
3506.690696	500591.974443	41.620839
3506.774480	500505.766960	41.625844
3506.477339	500417.044499	41.630848
3506.697611	500327.483993	41.635853
3506.733155	500251.375691	41.640858
3506.754726	500156.091908	41.645863
3506.705568	500058.295168	41.650868
3506.612166	499973.070979	41.655872
3506.884907	499884.155661	41.660877
3506.786764	499793.581613	41.665882
3506.518848	499712.723288	41.670887
3506.350765	499625.035756	41.675892
3506.369780	499542.718726	41.680896
3506.669346	499454.250838	41.685901
3506.292320	499372.600106	41.690906
3506.451317	499284.304473	41.695911
3506.471043	499204.054677	41.700916
3506.134347	499120.276531	41.705920
3506.206582	499033.607930	41.710925
3506.508616	498957.653306	41.715930
3506.398902	498876.261033	41.720935
3506.042920	498797.026421	41.725940
3505.911970	498702.261615	41.730944
3505.722938	498622.444893	41.735949
3505.777952	498559.750252	41.740954
3505.712491	498478.853607	41.745959
3505.882643	498401.402459	41.750964
3505.344397	498338.546829	41.755968
3505.589664	498253.966553	41.760973
3505.820908	498183.470030	41.765978
3505.941243	498114.908423	41.770983
3505.804614	498034.121352	41.775988
3505.592222	497956.525493	41.780992
3505.627353	497885.603794	41.785997
3505.898119	497814.594611	41.791002
3505.535272	497739.494275	41.796007
3505.638811	497669.620861	41.801012
3505.473592	497591.914790	41.806016
3505.910684	497516.335508	41.811021
3505.552612	497447.390958	41.816026
3505.394145	497372.761705	41.821031
3505.351942	497307.300672	41.826036
3505.694621	497239.053723	41.831040
3505.627408	497159.916781	41.836045
3505.556777	497101.576486	41.841050
3505.551319	497022.833015	41.846055
3505.536904	496947.169648	41.851060
3505.635783	496887.489714	41.856064
3505.918850	496811.072670	41.861069
3505.461670	496743.149811	41.866074
3505.536057	496664.392004	41.871079
3505.611347	496595.174122	41.876084
3505.359335	496527.016428	41.881088
3505.285085	496453.227565	41.886093
3505.106908	496381.372727	41.891098
3505.059591	496314.797544	41.896103
3505.307224	496251.659278	41.901108
3504.942057	496183.820490	41.906112
3505.125545	496113.725358	41.911117
3505.022190	496051.902868	41.916122
3504.748520	495980.818154	41.921127
3505.317262	495922.020348	41.926132
3505.302356	495857.810677	41.931136
3505.254669	495786.740348	41.936141
3505.090748	495722.149427	41.941146
3504.854212	495647.473135	41.946151
3504.903007	495589.360705	41.951156
3504.999371	495523.365397	41.956160
3505.031154	495462.630035	41.961165
3505.005745	495403.720705	41.966170
3504.775354	495339.441359	41.971175
3504.786328	495279.314282	41.976180
3504.958834	495221.585029	41.981184
3505.090890	495151.392392	41.986189
3504.909031	495093.011013	41.991194
3504.713094	495033.117074	41.996199
3504.906738	494974.121471	42.001204
3504.604533	494921.715287	42.006208
3504.513864	494844.992886	42.011213
3504.772402	494790.580564	42.016218
3504.741683	494731.820854	42.021223
3504.996357	494669.432048	42.026228
3504.325401	494608.499643	42.031232
3504.678132	494554.172771	42.036237
3504.203396	494506.537626	42.041242
3504.639317	494447.249807	42.046247
3504.678818	494388.528303	42.051252
3504.554644	494331.700036	42.056256
3504.828887	494267.690939	42.061261
3504.975262	494218.595082	42.066266
3504.414672	494155.068820	42.071271
3504.646438	494100.102789	42.076276
3504.192134	494052.614475	42.081280
3504.387910	493993.715638	42.086285
3504.317863	493936.826957	42.091290
3504.236311	493882.009856	42.096295
3504.244330	493830.409855	42.101300
3504.258692	493785.321678	42.106304
3504.227437	493732.869151	42.111309
3504.126409	493684.718831	42.116314
3504.301939	493620.065971	42.121319
3504.045671	493560.427950	42.126324
3504.219625	493528.592774	42.131328
3504.378692	493465.456482	42.136333
3504.287501	493415.082231	42.141338
3503.927673	493364.497166	42.146343
3504.094937	493312.012273	42.151348
3503.971016	493266.893563	42.156352
3504.238546	493210.202038	42.161357
3504.183092	493170.373854	42.166362
3504.253663	493119.317063	42.171367
3504.171173	493068.990785	42.176372
3504.269455	493020.100443	42.181376
3504.108163	492952.871593	42.186381
3503.599631	492914.375510	42.191386
3504.194704	492870.961408	42.196391
3504.366203	492821.352146	42.201396
3504.123793	492764.536325	42.206400
3503.880005	492714.839859	42.211405
3503.935060	492671.256754	42.216410
3503.888220	492611.582367	42.221415
3504.278221	492563.856958	42.226420
3504.157589	492525.249021	42.231424
3504.109534	492464.513896	42.236429
3503.954028	492417.125373	42.241434
3504.113018	492372.464877	42.246439
3504.030484	492319.611442	42.251444
3504.303018	492272.105360	42.256448
3504.208308	492214.810036	42.261453
3503.896198	492164.768927	42.266458
3503.654532	492116.938421	42.271463
3503.733306	492073.905326	42.276468
3504.038695	492033.109082	42.281472
3504.144148	491975.983677	42.286477
3503.825834	491923.519002	42.291482
3503.798782	491879.239455	42.296487
3503.670152	491832.198369	42.301492
3503.799190	491796.831875	42.306496
3504.064570	491753.162887	42.311501
3503.884313	491716.884929	42.316506
3503.988829	491658.142617	42.321511
3504.090481	491606.873872	42.326516
3503.916233	491564.686627	42.331520
3503.996121	491513.319959	42.336525
3503.997875	491473.377386	42.341530
3503.917893	491415.420280	42.346535
3503.941929	491372.797672	42.351540
3503.994366	491319.616748	42.356544
3503.868429	491278.532108	42.361549
3503.951149	491234.587064	42.366554
3504.121550	491185.427057	42.371559
3503.952497	491131.976957	42.376564
3503.762825	491086.609451	42.381568
3503.961704	491036.333587	42.386573
3503.951489	490995.028178	42.391578
3503.865213	490948.785709	42.396583
3503.821498	490900.314566	42.401588
3503.907969	490856.721326	42.406592
3504.001725	490806.410557	42.411597
3503.452688	490763.420923	42.416602
3503.134994	490714.082846	42.421607
3503.415633	490672.175811	42.426612
3503.214249	490631.909133	42.431616
3503.539603	490593.933833	42.436621
3503.605423	490557.614796	42.441626
3503.334318	490515.439692	42.446631
3503.580755	490480.859838	42.451636
3503.545835	490447.081181	42.456640
3503.626001	490401.265633	42.461645
3503.247206	490358.955352	42.466650
3503.644983	490317.483606	42.471655
3503.895732	490273.408624	42.476660
3503.524212	490235.742870	42.481664
3503.612531	490185.834888	42.486669
3503.512367	490142.066633	42.491674
3503.431206	490099.557810	42.496679
3503.277057	490066.907872	42.501684
3503.312955	490037.207840	42.506688
3503.519174	489983.594285	42.511693
3503.367673	489948.267126	42.516698
3503.126809	489916.286873	42.521703
3503.789554	489875.378703	42.526708
3503.798790	489833.562087	42.531712
3503.508739	489787.398285	42.536717
3503.469875	489738.821668	42.541722
3503.802608	489699.176422	42.546727
3503.774019	489657.971233	42.551732
3503.346262	489619.353158	42.556736
3503.582105	489572.803854	42.561741
3503.285733	489528.811851	42.566746
3503.750171	489488.388024	42.571751
3503.868825	489447.613875	42.576756
3503.637708	489402.247776	42.581760
3503.895192	489359.532675	42.586765
3503.848380	489318.127388	42.591770
3503.686050	489276.537951	42.596775
3503.754211	489225.064346	42.601780
3503.862489	489192.826225	42.606784
3503.595116	489132.717893	42.611789
3503.476445	489104.151176	42.616794
3503.591965	489066.154209	42.621799
3503.835635	489016.167710	42.626804
3503.447772	488969.309584	42.631808
3503.464214	488923.550003	42.636813
3503.134812	488888.904624	42.641818
3503.453881	488841.683575	42.646823
3503.368473	488791.090984	42.651828
3503.082445	488759.569869	42.656832
3503.590534	488706.005851	42.661837
3503.327378	488684.582069	42.666842
3503.112310	488646.382974	42.671847
3503.672567	488610.638917	42.676852
3503.634933	488580.543441	42.681856
3503.712638	488537.904521	42.686861
3503.774650	488496.985127	42.691866
3503.767680	488453.551053	42.696871
3503.842881	488402.831169	42.701876
3503.536591	488360.352520	42.706880
3503.874565	488318.076537	42.711885
3503.613398	488276.095698	42.716890
3503.843721	488235.351438	42.721895
3503.586792	488177.914577	42.726900
3503.648865	488150.833158	42.731904
3503.469954	488096.161739	42.736909
3503.611683	488055.481294	42.741914
3503.425604	488012.528404	42.746919
3503.197624	487973.976083	42.751924
3503.014191	487934.457084	42.756928
3503.234917	487887.601946	42.761933
3503.280413	487864.007647	42.766938
3503.534062	487822.854596	42.771943
3503.409870	487790.498165	42.776948
3503.175590	487756.694053	42.781952
3503.081473	487717.413137	42.786957
3503.327542	487687.928366	42.791962
3502.849323	487648.151448	42.796967
3503.286718	487608.585508	42.801972
3503.208943	487565.412474	42.806977
3503.163136	487536.831485	42.811981
3503.218544	487491.667663	42.816986
3503.316405	487462.811634	42.821991
3503.607365	487417.711958	42.826996
3503.469134	487391.620047	42.832001
3503.425904	487342.177818	42.837005
3503.444517	487304.292574	42.842010
3503.456861	487262.367410	42.847015
3503.664653	487218.694372	42.852020
3503.323812	487178.137202	42.857025
3503.588972	487132.283048	42.862029
3503.714615	487108.068990	42.867034
3503.502860	487057.136751	42.872039
3503.191836	487012.786201	42.877044
3503.351592	486979.676721	42.882049
3503.134343	486937.988442	42.887053
3503.007523	486907.398444	42.892058
3503.249062	486873.013228	42.897063
3503.559742	486825.989317	42.902068
3503.201303	486792.707515	42.907073
3503.435609	486758.828285	42.912077
3503.320493	486728.387644	42.917082
3503.546901	486676.274699	42.922087
3503.759932	486636.084515	42.927092
3503.376240	486596.593230	42.932097
3503.620163	486552.205505	42.937101
3503.699257	486512.894552	42.942106
3503.526988	486476.350294	42.947111
3503.447734	486440.498653	42.952116
3503.226263	486400.274441	42.957121
3503.611565	486354.954917	42.962125
3503.730812	486307.757161	42.967130
3503.445428	486269.714620	42.972135
3503.119303	486220.666397	42.977140
3503.414877	486190.766946	42.982145
3503.265852	486143.509406	42.987149
3503.440292	486110.698854	42.992154
3503.491188	486075.432276	42.997159
3503.689378	486024.786422	43.002164
3503.433897	485987.142642	43.007169
3503.051947	485940.678439	43.012173
3503.467558	485908.031985	43.017178
3503.327813	485875.370853	43.022183
3503.715225	485837.172033	43.027188
3503.023740	485800.757483	43.032193
3503.349670	485760.749508	43.037197
3503.326548	485725.190557	43.042202
3503.352486	485688.361011	43.047207
3503.515752	485644.740954	43.052212
3503.018545	485598.445201	43.057217
3503.296762	485567.486419	43.062221
3503.584051	485534.960177	43.067226
3503.333062	485490.949508	43.072231
3503.580522	485449.083852	43.077236
3503.453603	485409.094920	43.082241
3503.340184	485359.556213	43.087245
3503.277136	485331.428458	43.092250
3502.804441	485298.060170	43.097255
3503.227358	485261.268864	43.102260
3502.763883	485228.656739	43.107265
3503.126642	485191.773596	43.112269
3503.082144	485159.702330	43.117274
3503.214194	485118.308390	43.122279
3503.460196	485080.230741	43.127284
3503.065293	485053.568602	43.132289
3503.516687	485002.576894	43.137293
3503.288346	484972.605063	43.142298
3503.417829	484931.109987	43.147303
3503.480355	484896.142014	43.152308
3503.264894	484856.114913	43.157313
3503.117922	484821.330924	43.162317
3503.453649	484783.541692	43.167322
3502.928779	484753.312471	43.172327
3503.235004	484707.343687	43.177332
3503.113668	484675.384412	43.182337
3503.226436	484639.397671	43.187341
3503.186863	484603.586109	43.192346
3503.208905	484564.077000	43.197351
3503.331994	484528.391509	43.202356
3502.975222	484494.397219	43.207361
3502.990725	484452.261851	43.212365
3503.113905	484421.628021	43.217370
3502.737615	484389.152117	43.222375
3503.017650	484354.553231	43.227380
3502.529221	484333.461552	43.232385
3502.799378	484286.335183	43.237389
3502.722381	484266.038224	43.242394
3502.746253	484240.319913	43.247399
3502.898704	484211.348271	43.252404
3503.010311	484177.684560	43.257409
3503.180245	484136.433665	43.262413
3502.929291	484102.826212	43.267418
3503.336222	484063.104374	43.272423
3503.195152	484040.947833	43.277428
3502.804206	484008.119767	43.282433
3503.155665	483970.275589	43.287437
3503.499583	483936.171039	43.292442
3503.174217	483897.825756	43.297447
3503.692632	483870.716330	43.302452
3502.943998	483824.707000	43.307457
3502.899471	483782.225507	43.312461
3502.860191	483751.059901	43.317466
3502.815771	483718.834080	43.322471
3502.888927	483694.016584	43.327476
3502.877800	483665.877728	43.332481
3502.933139	483633.939338	43.337485
3502.488888	483597.784254	43.342490
3502.647505	483569.568288	43.347495
3503.111444	483540.597448	43.352500
3503.019213	483514.997049	43.357505
3502.789145	483480.627165	43.362509
3502.967779	483449.022866	43.367514
3502.825480	483411.001552	43.372519
3502.859715	483371.538037	43.377524
3502.521154	483355.221364	43.382529
3502.558005	483321.870573	43.387533
3503.059234	483286.376004	43.392538
3502.785454	483260.904484	43.397543
3502.943538	483230.262878	43.402548
3502.648011	483200.298079	43.407553
3502.803501	483166.120120	43.412557
3502.663350	483146.488332	43.417562
3502.932039	483118.001803	43.422567
3502.709853	483087.065425	43.427572
3502.582875	483058.539311	43.432577
3502.885079	483023.226686	43.437581
3503.030993	482995.112705	43.442586
3502.565214	482959.262632	43.447591
3502.777632	482938.615761	43.452596
3503.036935	482917.557373	43.457601
3502.988659	482874.720320	43.462605
3503.136433	482848.121515	43.467610
3503.050492	482819.538053	43.472615
3503.040674	482778.311536	43.477620
3503.020407	482743.149508	43.482625
3503.073270	482703.075107	43.487629
3503.337068	482688.735522	43.492634
3503.184068	482644.196285	43.497639
3503.221902	482605.387099	43.502644
3503.178407	482563.457902	43.507649
3502.995741	482522.409183	43.512653
3502.912068	482488.418535	43.517658
3502.830242	482457.711696	43.522663
3502.924562	482421.975332	43.527668
3502.763985	482396.080578	43.532673
3502.893358	482366.149108	43.537677
3502.935245	482349.772179	43.542682
3502.707838	482320.552980	43.547687
3503.313276	482279.936772	43.552692
3502.765360	482242.582046	43.557697
3502.813199	482206.448212	43.562701
3502.982556	482182.927034	43.567706
3502.970398	482141.143409	43.572711
3503.119514	482115.351577	43.577716
3503.122206	482078.769733	43.582721
3503.215651	482049.146410	43.587725
3503.262963	482007.959500	43.592730
3502.995095	481967.175217	43.597735
3503.134160	481923.093751	43.602740
3502.797197	481900.964652	43.607745
3502.842126	481860.181944	43.612749
3502.831065	481833.656660	43.617754
3502.922733	481803.224706	43.622759
3502.889838	481764.525498	43.627764
3502.885226	481748.660456	43.632769
3502.952489	481698.980927	43.637773
3502.800383	481679.702853	43.642778
3502.849538	481654.026875	43.647783
3503.008701	481616.863793	43.652788
3502.884469	481588.081927	43.657793
3502.488577	481555.552637	43.662797
3502.739068	481526.813405	43.667802
3502.531550	481500.570772	43.672807
3502.805659	481472.585697	43.677812
3502.796985	481452.628149	43.682817
3502.916965	481416.178095	43.687821
3502.551543	481381.167778	43.692826
3502.612822	481350.436500	43.697831
3502.696267	481325.108353	43.702836
3503.007402	481292.872731	43.707841
3502.652889	481261.346981	43.712845
3502.667497	481228.854194	43.717850
3502.575539	481201.835135	43.722855
3503.037943	481163.714259	43.727860
3502.770435	481142.280698	43.732865
3502.868523	481115.585627	43.737869
3503.020295	481078.371893	43.742874
3502.859856	481046.967102	43.747879
3502.921732	481007.190146	43.752884
3502.909857	480981.421506	43.757889
3502.487524	480951.168947	43.762893
3503.005050	480931.937343	43.767898
3503.001777	480900.305680	43.772903
3502.937740	480869.795087	43.777908
3502.646194	480839.724085	43.782913
3502.648037	480796.115589	43.787917
3502.419682	480763.558586	43.792922
3502.392244	480733.143095	43.797927
3502.809343	480707.105127	43.802932
3502.540070	480683.094117	43.807937
3502.399620	480654.464659	43.812941
3502.628038	480638.461171	43.817946
3502.738666	480613.734028	43.822951
3502.909290	480581.569348	43.827956
3502.816942	480557.075828	43.832961
3502.759211	480515.699226	43.837965
3502.585967	480494.199581	43.842970
3502.816530	480466.926944	43.847975
3502.751187	480426.814595	43.852980
3502.922031	480406.423527	43.857985
3502.643640	480368.365473	43.862989
3502.829428	480352.115667	43.867994
3502.472866	480314.221245	43.872999
3502.854819	480283.437984	43.878004
3502.632073	480262.349987	43.883009
3502.467485	480225.284534	43.888013
3502.621764	480206.613903	43.893018
3502.371554	480178.505990	43.898023
3502.755407	480154.392539	43.903028
3502.396746	480130.293530	43.908033
3502.176713	480095.055593	43.913037
3502.414376	480083.244366	43.918042
3502.712889	480061.418053	43.923047
3502.689400	480023.976437	43.928052
3502.681792	479995.779912	43.933057
3503.043046	479969.749420	43.938061
3502.771534	479941.492798	43.943066
3502.773347	479913.648397	43.948071
3502.753317	479875.397348	43.953076
3502.403778	479846.142017	43.958081
3502.423821	479819.355829	43.963085
3502.889986	479789.417584	43.968090
3502.642011	479768.181250	43.973095
3502.745469	479729.001012	43.978100
3502.746632	479703.329324	43.983105
3502.511841	479681.029595	43.988109
3502.672505	479658.314555	43.993114
3502.533732	479630.693671	43.998119
3502.682226	479597.418667	44.003124
3502.598392	479578.582209	44.008129
3502.632381	479543.101372	44.013133
3502.607935	479527.641460	44.018138
3502.556524	479490.202924	44.023143
3502.814859	479466.714382	44.028148
3502.599649	479441.025403	44.033153
3502.832159	479413.346364	44.038157
3502.589518	479384.932647	44.043162
3502.700546	479348.934031	44.048167
3502.502209	479314.802762	44.053172
3502.937049	479299.523836	44.058177
3502.677132	479267.271873	44.063181
3502.806038	479236.525955	44.068186
3502.634993	479207.140593	44.073191
3502.453901	479179.525507	44.078196
3502.322193	479152.610197	44.083201
3502.250913	479124.371491	44.088205
3502.560996	479102.087230	44.093210
3501.914678	479079.193717	44.098215
3502.593679	479059.833644	44.103220
3502.545142	479041.951250	44.108225
3502.802213	479004.413026	44.113229
3502.852750	478984.695827	44.118234
3502.477777	478961.810457	44.123239
3503.079980	478927.654854	44.128244
3502.435036	478896.776013	44.133249
3502.513195	478868.058763	44.138253
3502.710581	478841.698160	44.143258
3502.455107	478816.267119	44.148263
3502.716113	478783.073973	44.153268
3502.461423	478759.563142	44.158273
3502.843103	478723.217765	44.163277
3502.714583	478713.484009	44.168282
3502.374890	478682.860476	44.173287
3502.295839	478651.842560	44.178292
3502.247599	478635.981178	44.183297
3502.443859	478606.638621	44.188301
3502.426822	478586.830368	44.193306
3502.585376	478553.501071	44.198311
3502.740302	478522.193801	44.203316
3502.421294	478511.276643	44.208321
3502.473958	478481.198126	44.213325
3502.628600	478453.074685	44.218330
3502.459796	478427.932766	44.223335
3502.945981	478401.577031	44.228340
3502.425359	478381.189882	44.233345
3502.691108	478334.147438	44.238349
3502.788454	478310.682239	44.243354
3502.664545	478289.980545	44.248359
3502.969457	478252.736336	44.253364
3502.491098	478231.584331	44.258369
3502.661832	478200.071810	44.263373
3502.488507	478174.374261	44.268378
3502.437062	478142.239187	44.273383
3502.853246	478120.644595	44.278388
3502.521068	478095.931890	44.283393
3502.359899	478062.499699	44.288397
3502.473044	478034.483056	44.293402
3502.227922	478010.160989	44.298407
3502.652427	477989.373563	44.303412
3502.129133	477968.228199	44.308417
3502.236462	477944.861988	44.313421
3502.343676	477916.492280	44.318426
3502.335225	477895.216162	44.323431
3502.400908	477862.657975	44.328436
3502.655770	477851.347820	44.333441
3502.359098	477828.044305	44.338445
3502.136743	477797.451347	44.343450
3502.219340	477781.669834	44.348455
3502.498240	477749.330940	44.353460
3502.378572	477735.855191	44.358465
3502.358755	477705.028375	44.363469
3502.463776	477678.427515	44.368474
3502.411823	477656.905144	44.373479
3502.512849	477634.802986	44.378484
3502.124131	477606.257193	44.383489
3502.180132	477586.082540	44.388493
3502.347359	477562.453742	44.393498
3501.859293	477546.760799	44.398503
3502.511586	477515.374155	44.403508
3502.217068	477505.210617	44.408513
3502.085515	477481.476568	44.413517
3502.433693	477457.162415	44.418522
3502.304058	477439.189756	44.423527
3502.315359	477413.310623	44.428532
3502.236900	477388.961673	44.433537
3501.997938	477381.114337	44.438541
3502.205437	477341.507690	44.443546
3501.999334	477331.633534	44.448551
3501.996675	477305.756399	44.453556
3502.058074	477283.508295	44.458561
3502.157412	477278.741883	44.463565
3502.254750	477250.928493	44.468570
3502.198295	477244.518417	44.473575
3502.213450	477209.186931	44.478580
3502.109627	477193.686559	44.483585
3501.970082	477171.974994	44.488589
3502.319838	477155.848034	44.493594
3501.962242	477126.134058	44.498599
3502.240691	477101.678587	44.503604
3502.386314	477081.994780	44.508609
3502.275951	477063.867070	44.513613
3502.258172	477050.779230	44.518618
3502.378340	477018.311929	44.523623
3502.293764	477002.707291	44.528628
3502.056585	476976.461772	44.533633
3502.423779	476958.613432	44.538637
3502.116472	476933.895054	44.543642
3502.129306	476913.675726	44.548647
3502.369808	476883.969314	44.553652
3502.260590	476864.425982	44.558657
3502.074697	476839.435846	44.563661
3502.258467	476821.110459	44.568666
3502.178992	476801.410791	44.573671
3502.506263	476784.882608	44.578676
3502.515466	476759.710357	44.583681
3502.501837	476735.704130	44.588685
3502.582152	476703.545656	44.593690
3502.482515	476688.397952	44.598695
3502.507278	476660.898095	44.603700
3502.404158	476633.519179	44.608705
3502.385331	476607.693975	44.613709
3502.408865	476573.926657	44.618714
3501.920607	476562.983954	44.623719
3502.236181	476530.586346	44.628724
3502.244653	476530.433410	44.633729
3502.589387	476492.066922	44.638733
3502.507741	476483.689216	44.643738
3502.404442	476449.688650	44.648743
3502.696905	476432.104078	44.653748
3502.497016	476395.843906	44.658753
3502.253882	476372.782660	44.663757
3502.684120	476346.634430	44.668762
3502.525828	476323.155548	44.673767
3502.374527	476294.418829	44.678772
3502.565265	476274.373191	44.683777
3502.269435	476250.258515	44.688781
3502.232122	476229.995583	44.693786
3502.226563	476210.789141	44.698791
3502.549325	476171.869305	44.703796
3502.662586	476165.432387	44.708801
3502.597447	476131.020840	44.713805
3502.357992	476105.835711	44.718810
3502.298384	476083.048764	44.723815
3502.414113	476047.244150	44.728820
3502.320700	476037.098927	44.733825
3502.125863	476020.398473	44.738829
3502.274590	475997.124070	44.743834
3502.256164	475976.605147	44.748839
3502.429091	475939.831012	44.753844
3502.157245	475934.060486	44.758849
3502.054273	475912.493161	44.763853
3502.541667	475893.310723	44.768858
3502.301132	475851.091143	44.773863
3502.221093	475824.667643	44.778868
3502.045113	475810.390284	44.783873
3502.474158	475792.733213	44.788877
3502.444395	475773.075092	44.793882
3502.029950	475755.852520	44.798887
3502.249821	475726.399912	44.803892
3502.005044	475703.135770	44.808897
3502.147090	475688.859361	44.813901
3502.235896	475669.384852	44.818906
3502.361665	475647.528840	44.823911
3502.566302	475612.770918	44.828916
3502.092502	475592.979484	44.833921
3502.332792	475568.931999	44.838925
3501.923886	475551.101773	44.843930
3502.162842	475530.592777	44.848935
3502.612381	475514.701384	44.853940
3502.474660	475496.323419	44.858945
3502.402409	475464.792781	44.863949
3502.181192	475441.524593	44.868954
3502.148310	475416.761169	44.873959
3502.010515	475402.022572	44.878964
3502.279684	475385.653639	44.883969
3502.288074	475364.725376	44.888973
3502.594569	475333.034445	44.893978
3502.228381	475317.017053	44.898983
3502.188755	475296.146722	44.903988
3502.294772	475278.893196	44.908993
3502.263818	475251.146853	44.913997
3502.414178	475233.330342	44.919002
3501.997362	475214.742743	44.924007
3502.343251	475189.768383	44.929012
3502.053863	475175.457558	44.934017
3502.146808	475146.832425	44.939021
3502.131882	475117.566889	44.944026
3502.161948	475098.656869	44.949031
3502.420393	475082.794789	44.954036
3502.260618	475063.156032	44.959041
3502.425204	475043.062383	44.964045
3502.717917	475014.507027	44.969050
3502.277975	474988.946949	44.974055
3502.348684	474965.531547	44.979060
3502.414321	474943.532289	44.984065
3502.250632	474922.124734	44.989069
3502.442841	474896.516689	44.994074
3502.030622	474874.844447	44.999079
3502.244543	474845.947205	45.004084
3502.182301	474831.044678	45.009089
3502.252586	474809.347814	45.014093
3502.314581	474784.164254	45.019098
3502.309258	474768.848412	45.024103
3502.361915	474747.508058	45.029108
3502.374559	474718.945212	45.034113
3502.233608	474700.920694	45.039117
3502.395626	474677.237913	45.044122
3502.145534	474660.241342	45.049127
3502.266792	474625.595370	45.054132
3502.139527	474618.588656	45.059137
3502.207042	474593.707244	45.064141
3502.194795	474575.662558	45.069146
3502.334901	474542.580548	45.074151
3502.474091	474530.527797	45.079156
3502.149910	474500.298247	45.084161
3502.209326	474480.270815	45.089165
3502.174436	474457.781028	45.094170
3501.832037	474444.792132	45.099175
3502.240069	474421.171796	45.104180
3501.862493	474399.139663	45.109185
3501.913997	474391.447866	45.114189
3502.203516	474361.425865	45.119194
3502.230034	474341.757240	45.124199
3502.215479	474320.477333	45.129204
3502.254093	474301.918912	45.134209
3502.337115	474287.903208	45.139213
3502.099711	474278.689213	45.144218
3502.141528	474249.362722	45.149223
3502.383575	474223.543649	45.154228
3502.332430	474206.515641	45.159233
3501.911821	474185.045984	45.164237
3502.211498	474167.862239	45.169242
3501.895051	474138.742954	45.174247
3502.185819	474121.055025	45.179252
3502.606066	474093.944211	45.184257
3502.261884	474079.287073	45.189261
3502.411608	474045.292608	45.194266
3502.449875	474028.301052	45.199271
3502.676696	473998.035372	45.204276
3502.487583	473977.742677	45.209281
3502.256158	473961.804070	45.214285
3502.373395	473931.706977	45.219290
3501.918271	473913.831576	45.224295
3502.363830	473894.552175	45.229300
3502.653243	473867.360237	45.234305
3502.556655	473851.349986	45.239309
3502.389069	473820.285948	45.244314
3502.120045	473794.040189	45.249319
3502.178855	473771.737081	45.254324
3502.226744	473747.716828	45.259329
3501.816858	473722.251172	45.264333
3502.234204	473701.813205	45.269338
3502.179474	473685.846830	45.274343
3501.854925	473667.698070	45.279348
3502.156301	473644.497629	45.284353
3502.252286	473634.220313	45.289357
3502.696214	473612.969239	45.294362
3501.879746	473591.863716	45.299367
3502.246829	473566.378017	45.304372
3502.084478	473555.382543	45.309377
3501.885899	473528.720961	45.314381
3502.128073	473506.136183	45.319386
3501.996059	473492.052146	45.324391
3502.347185	473474.050795	45.329396
3502.294838	473454.191149	45.334401
3502.138592	473429.241660	45.339405
3502.540466	473409.210167	45.344410
3502.140281	473390.516767	45.349415
3502.215984	473358.857887	45.354420
3501.847572	473336.822880	45.359425
3501.878734	473327.061003	45.364429
3502.163348	473303.357138	45.369434
3502.271235	473298.942105	45.374439
3502.195642	473269.733221	45.379444
3502.155411	473253.561946	45.384449
3502.055144	473236.186678	45.389453
3502.361496	473212.630963	45.394458
3501.854840	473191.375596	45.399463
3502.061667	473157.471495	45.404468
3502.156060	473153.867405	45.409473
3501.903886	473142.784518	45.414477
3502.371124	473115.917537	45.419482
3502.242054	473090.710522	45.424487
3502.102420	473077.031753	45.429492
3502.182754	473057.049863	45.434497
3501.800400	473030.618281	45.439501
3502.241174	473020.034146	45.444506
3502.320304	472990.244572	45.449511
3502.082729	472978.754855	45.454516
3502.085208	472956.560505	45.459521
3502.153176	472943.860434	45.464525
3502.484693	472918.834259	45.469530
3502.406778	472904.741293	45.474535
3502.586011	472866.695291	45.479540
3502.370231	472852.623733	45.484545
3502.148675	472828.290157	45.489549
3502.241799	472802.795338	45.494554
3502.010125	472770.778694	45.499559
3502.170793	472755.030668	45.504564
3502.160053	472742.696583	45.509569
3501.965788	472723.110910	45.514573
3502.173603	472694.210786	45.519578
3502.158283	472670.097663	45.524583
3502.233255	472650.368892	45.529588
3502.048577	472636.039523	45.534593
3501.976005	472622.602719	45.539597
3502.344313	472585.942231	45.544602
3501.902539	472571.905598	45.549607
3502.367414	472551.509349	45.554612
3502.079365	472544.122301	45.559617
3501.930650	472520.686957	45.564621
3502.085536	472493.817000	45.569626
3502.096631	472487.546192	45.574631
3502.354645	472469.052649	45.579636
3501.806710	472452.706796	45.584641
3501.673019	472430.634033	45.589645
3502.225862	472402.690851	45.594650
3502.091682	472397.302092	45.599655
3502.230898	472361.637342	45.604660
3502.269971	472352.632015	45.609665
3502.136512	472323.986572	45.614669
3501.921662	472310.672767	45.619674
3501.767185	472302.253667	45.624679
3501.866719	472269.173339	45.629684
3502.026606	472272.434741	45.634689
3502.047922	472250.084823	45.639693
3502.057212	472232.590319	45.644698
3502.054558	472213.682028	45.649703
3501.975882	472187.151260	45.654708
3502.145126	472182.170237	45.659713
3501.969342	472152.671590	45.664717
3502.057605	472136.024185	45.669722
3502.242185	472116.075478	45.674727
3502.024367	472090.375139	45.679732
3502.104129	472082.880086	45.684737
3501.709238	472057.965629	45.689741
3502.401586	472036.319935	45.694746
3502.207526	472023.306012	45.699751
3502.076194	472004.366943	45.704756
3502.257821	471980.727741	45.709761
3502.204526	471961.018096	45.714765
3502.118358	471934.639761	45.719770
3502.026065	471919.638118	45.724775
3502.272438	471895.634805	45.729780
3502.385753	471879.488830	45.734785
3502.193545	471863.643179	45.739789
3502.596606	471834.256118	45.744794
3502.091907	471816.942270	45.749799
3502.031490	471785.301515	45.754804
3502.247673	471770.201173	45.759809
3502.183516	471746.043725	45.764813
3502.210740	471707.513080	45.769818
3502.298256	471646.119920	45.774823
3501.953266	471524.020537	45.779828
3502.089299	471365.593387	45.784833
3501.834132	471161.568737	45.789837
3501.605424	470892.413457	45.794842
3501.154073	470593.911267	45.799847
3500.652863	470237.212111	45.804852
3499.929413	469849.492677	45.809857
3498.902047	469410.890777	45.814861
3498.692438	468922.947145	45.819866
3497.893408	468400.238263	45.824871
3497.199642	467826.672155	45.829876
3496.282540	467210.335917	45.834881
3494.995890	466555.748818	45.839885
3494.615642	465860.330725	45.844890
3493.432683	465117.918984	45.849895
3492.297685	464336.316468	45.854900
3491.173479	463510.465172	45.859905
3489.715053	462648.152282	45.864909
3488.500406	461740.631588	45.869914
3487.011916	460808.517226	45.874919
3485.782232	459818.582445	45.879924
3484.455926	458810.795070	45.884929
3482.633178	457755.157140	45.889933
3481.338334	456657.472160	45.894938
3479.409876	455528.945835	45.899943
3477.933657	454363.127767	45.904948
3475.956114	453157.527377	45.909953
3474.000328	451918.939663	45.914957
3472.003440	450655.315652	45.919962
3469.716293	449375.599425	45.924967
3468.466118	448039.685708	45.929972
3466.811546	446683.027645	45.934977
3464.654810	445282.242191	45.939981
3462.111981	443864.293434	45.944986
3460.058597	442424.433218	45.949991
3458.244472	440940.512013	45.954996
3455.931868	439443.533214	45.960001
3453.423622	437908.777529	45.965005
3451.271353	436345.117876	45.970010
3448.481451	434766.787704	45.975015
3446.475550	433161.757202	45.980020
3443.911798	431522.071190	45.985025
3441.724141	429867.290435	45.990029
3439.338621	428174.846698	45.995034
3436.585454	426483.431833	46.000039
3433.811650	424760.145718	46.005044
3431.181907	423005.260060	46.010049
3428.215854	421244.598198	46.015053
3425.471451	419462.862064	46.020058
3422.793730	417669.097860	46.025063
3420.126662	415835.826514	46.030068
3417.347999	414012.203063	46.035073
3414.242804	412158.956055	46.040077
3411.754599	410270.910820	46.045082
3408.127628	408381.054119	46.050087
3405.286812	406480.817931	46.055092
3402.662532	404565.317633	46.060097
3399.820168	402634.415785	46.065101
3397.188273	400676.828475	46.070106
3393.858177	398711.064247	46.075111
3390.472129	396735.297287	46.080116
3387.533718	394728.484804	46.085121
3384.282129	392733.482883	46.090125
3381.133153	390713.018557	46.095130
3377.913450	388699.025104	46.100135
3374.718871	386648.889676	46.105140
3371.715094	384601.782551	46.110145
3368.093352	382537.086897	46.115149
3365.001371	380457.466244	46.120154
3361.631603	378384.352570	46.125159
3358.245838	376284.995764	46.130164
3354.967046	374195.034973	46.135169
3351.849927	372082.637075	46.140173
3348.541685	369972.572496	46.145178
3345.035951	367848.839252	46.150183
3341.866254	365702.613285	46.155188
3338.346179	363561.721051	46.160193
3334.411451	361413.546547	46.165197
3331.498910	359258.197441	46.170202
3327.532620	357104.689804	46.175207
3324.126529	354923.977806	46.180212
3320.537354	352764.469759	46.185217
3316.646164	350582.544014	46.190221
3313.261876	348400.622223	46.195226
3309.768470	346225.336773	46.200231
3306.348497	344039.322938	46.205236
3302.601074	341856.526817	46.210241
3298.576169	339655.482043	46.215245
3295.372897	337461.040132	46.220250
3291.400585	335274.622317	46.225255
3287.961280	333058.516034	46.230260
3284.289050	330860.553374	46.235265
3280.673990	328650.400563	46.240269
3277.060177	326463.221524	46.245274
3273.031936	324246.835923	46.250279
3269.490845	322044.451507	46.255284
3265.727952	319827.561774	46.260289
3261.935264	317621.681844	46.265293
3258.478661	315405.996759	46.270298
3254.552168	313198.928325	46.275303
3250.834024	310980.501205	46.280308
3247.066123	308771.191094	46.285313
3242.991754	306566.944596	46.290317
3239.591787	304341.780800	46.295322
3235.688974	302138.971295	46.300327
3232.074401	299928.746904	46.305332
3228.068582	297721.574467	46.310337
3224.233591	295510.089697	46.315341
3220.296055	293313.148446	46.320346
3216.412430	291117.493583	46.325351
3212.802249	288906.495950	46.330356
3208.908944	286701.016544	46.335361
3204.863649	284516.669554	46.340365
3201.349890	282324.227985	46.345370
3197.294670	280133.178965	46.350375
3193.572290	277940.333865	46.355380
3189.413527	275759.131080	46.360385
3185.325725	273587.789201	46.365389
3181.813813	271408.358201	46.370394
3177.662538	269246.848802	46.375399
3173.722813	267073.517980	46.380404
3169.936224	264898.052979	46.385409
3165.578569	262749.445980	46.390413
3162.149753	260595.559606	46.395418
3158.190872	258456.206196	46.400423
3154.428388	256308.279921	46.405428
3150.241252	254174.850261	46.410433
3145.980772	252034.244175	46.415437
3142.416746	249888.839755	46.420442
3138.053757	247779.594575	46.425447
3134.197356	245656.926924	46.430452
3130.321503	243541.167694	46.435457
3126.507979	241442.876026	46.440461
3122.330843	239344.216559	46.445466
3117.905484	237266.923824	46.450471
3114.260899	235178.775083	46.455476
3110.721797	233109.676093	46.460481
3106.550397	231038.783100	46.465485
3102.699566	228970.279712	46.470490
3098.717188	226916.132521	46.475495
3094.222504	224863.184499	46.480500
3090.410664	222820.955483	46.485505
3086.432549	220792.050155	46.490509
3082.564765	218766.392680	46.495514
3078.305897	216758.070940	46.500519
3074.729791	214738.725762	46.505524
3070.432860	212734.759402	46.510529
3066.022117	210744.576465	46.515533
3061.853875	208758.750862	46.520538
3057.846924	206794.335102	46.525543
3053.669469	204834.369688	46.530548
3050.109659	202879.421308	46.535553
3045.911512	200941.274635	46.540557
3041.747043	199003.018190	46.545562
3037.531127	197088.707391	46.550567
3033.225630	195166.719989	46.555572
3029.090256	193262.356079	46.560577
3024.965616	191367.212335	46.565581
3020.795739	189487.945062	46.570586
3016.477793	187631.853976	46.575591
3012.419551	185779.497835	46.580596
3007.975686	183942.564370	46.585601
3003.765148	182125.566762	46.590605
2999.732344	180299.588436	46.595610
2995.174390	178514.977549	46.600615
2990.686978	176725.262001	46.605620
2986.301500	174962.468611	46.610625
2982.049516	173219.132153	46.615629
2977.745595	171472.914976	46.620634
2973.532645	169753.761938	46.625639
2969.253936	168061.111241	46.630644
2964.564581	166384.539871	46.635649
2959.745180	164722.183954	46.640653
2955.424205	163080.029958	46.645658
2950.646006	161460.199030	46.650663
2945.910348	159866.023804	46.655668
2941.129374	158292.311468	46.660673
2936.287953	156751.065429	46.665677
2931.393615	155225.496275	46.670682
2925.975300	153747.213116	46.675687
2920.637194	152289.737801	46.680692
2915.276627	150835.778368	46.685697
2909.816953	149415.150236	46.690701
2904.252841	148079.401813	46.695706
2898.656780	146784.424472	46.700711
2892.344538	145524.023557	46.705716
2887.394225	144315.534820	46.710721
2881.558197	143152.039378	46.715725
2875.687409	142011.491988	46.720730
2870.402751	140927.511592	46.725735
2864.955879	139871.813315	46.730740
2859.750952	138858.505844	46.735745
2854.791780	137882.535278	46.740749
2850.636609	136953.990426	46.745754
2845.516423	136037.153379	46.750759
2840.983671	135140.102057	46.755764
2836.920861	134271.733343	46.760769
2831.946848	133437.082015	46.765773
2827.939144	132611.887744	46.770778
2823.990579	131825.918003	46.775783
2819.756434	131041.100913	46.780788
2815.736208	130274.518521	46.785793
2811.343228	129535.712295	46.790797
2807.727645	128790.221808	46.795802
2803.938100	128078.186171	46.800807
2800.482476	127365.055013	46.805812
2797.220296	126675.373019	46.810817
2792.995823	125988.904912	46.815821
2789.581746	125290.430154	46.820826
2785.893051	124613.822545	46.825831
2782.124348	123934.873140	46.830836
2778.659527	123270.513858	46.835841
2774.806099	122609.240315	46.840845
2771.534188	121952.109646	46.845850
2767.261290	121316.740125	46.850855
2763.955517	120670.255409	46.855860
2760.441799	120027.043986	46.860865
2756.857232	119399.674159	46.865869
2753.242609	118771.734325	46.870874
2749.277430	118149.085885	46.875879
2745.666311	117534.416569	46.880884
2742.149521	116914.554464	46.885889
2738.289604	116314.694503	46.890893
2734.476374	115709.369222	46.895898
2730.695965	115120.222797	46.900903
2726.921855	114533.399007	46.905908
2723.304626	113954.405403	46.910913
2719.332484	113380.829194	46.915917
2715.516841	112812.374437	46.920922
2711.963511	112253.703387	46.925927
2707.949074	111700.910504	46.930932
2704.039911	111142.744477	46.935937
2699.777512	110615.397031	46.940941
2696.244188	110068.555652	46.945946
2692.775131	109542.715438	46.950951
2688.894729	109020.595854	46.955956
2685.432579	108498.584279	46.960961
2681.855422	107986.095002	46.965965
2678.310053	107468.358033	46.970970
2675.066050	106964.692871	46.975975
2671.173498	106448.487268	46.980980
2667.853795	105942.738712	46.985985
2664.186371	105443.827283	46.990989
2661.009587	104936.482519	46.995994
2657.476836	104435.111688	47.000999
2653.829330	103926.291919	47.006004
2650.668337	103418.980388	47.011009
2646.838738	102929.842991	47.016013
2643.377765	102418.309844	47.021018
2640.256512	101914.370851	47.026023
2636.783656	101412.083114	47.031028
2633.122246	100916.238397	47.036033
2629.941562	100406.459775	47.041037
2626.398836	99898.410498	47.046042
2623.106088	99399.379573	47.051047
2619.722582	98899.633369	47.056052
2616.398826	98375.153493	47.061057
2612.675945	97866.719596	47.066061
2609.705841	97350.640358	47.071066
2606.335880	96845.993262	47.076071
2602.684165	96330.201985	47.081076
2599.634056	95811.224761	47.086081
2596.090873	95286.131386	47.091085
2592.839181	94768.562629	47.096090
2588.934585	94247.698490	47.101095
2585.328576	93726.250254	47.106100
2582.104156	93197.050955	47.111105
2578.496895	92672.291549	47.116109
2575.091473	92152.007924	47.121114
2571.462440	91629.391894	47.126119
2568.300615	91099.622088	47.131124
2564.910654	90571.358283	47.136129
2561.431754	90045.747710	47.141133
2558.151978	89510.903838	47.146138
2554.638925	88980.069935	47.151143
2551.215267	88453.729227	47.156148
2547.664763	87911.257000	47.161153
2544.188178	87366.902971	47.166157
2540.497137	86832.362119	47.171162
2537.362924	86303.105561	47.176167
2533.827909	85762.296874	47.181172
2530.450863	85225.081546	47.186177
2526.400935	84680.244503	47.191181
2523.655035	84142.493803	47.196186
2519.886193	83603.375318	47.201191
2516.370432	83057.266514	47.206196
2513.169879	82501.389014	47.211201
2509.654866	81957.511489	47.216205
2506.525679	81413.609807	47.221210
2502.853211	80872.483268	47.226215
2498.998712	80304.188839	47.231220
2495.884241	79761.155258	47.236225
2492.175857	79204.202782	47.241229
2488.915753	78651.992638	47.246234
2484.851870	78099.982140	47.251239
2482.024824	77549.631791	47.256244
2478.830362	76987.106883	47.261249
2474.964914	76421.751661	47.266253
2471.695240	75858.055318	47.271258
2468.641393	75304.026624	47.276263
2464.417232	74738.546510	47.281268
2461.198780	74168.655039	47.286273
2457.378807	73613.726452	47.291277
2453.810355	73045.665795	47.296282
2450.381982	72484.757088	47.301287
2447.236019	71913.962986	47.306292
2443.761087	71351.853922	47.311297
2439.829296	70787.910733	47.316301
2436.709401	70217.828731	47.321306
2433.282582	69650.111374	47.326311
2429.836550	69081.044574	47.331316
2426.432565	68513.024813	47.336321
2422.544489	67933.952464	47.341325
2419.267796	67363.176971	47.346330
2415.806741	66799.526761	47.351335
2412.262158	66232.182429	47.356340
2408.877634	65642.807212	47.361345
2405.387905	65074.877248	47.366349
2401.869398	64500.452559	47.371354
2398.523138	63928.610046	47.376359
2394.791116	63353.013579	47.381364
2391.568249	62764.918300	47.386369
2388.137771	62187.994447	47.391373
2384.648187	61601.485033	47.396378
2381.092784	61029.665600	47.401383
2377.665788	60460.047866	47.406388
2374.582915	59861.852814	47.411393
2370.876027	59279.024421	47.416397
2367.360594	58689.371498	47.421402
2363.745287	58105.782863	47.426407
2360.272141	57517.249661	47.431412
2356.984037	56928.613221	47.436417
2353.327524	56344.166373	47.441421
2349.814876	55747.453462	47.446426
2346.102673	55162.815813	47.451431
2342.799956	54569.234009	47.456436
2339.624820	53981.173069	47.461441
2335.915191	53394.402667	47.466445
2332.697888	52798.574642	47.471450
2329.110735	52206.872997	47.476455
2325.760245	51597.178156	47.481460
2322.140031	51002.943106	47.486465
2318.540557	50403.785022	47.491469
2315.749785	49811.233973	47.496474
2311.908115	49210.787185	47.501479
2308.019258	48608.206935	47.506484
2305.112643	48004.493934	47.511489
2301.541433	47400.633987	47.516493
2298.193326	46790.666831	47.521498
2294.311241	46182.930174	47.526503
2290.748724	45580.747408	47.531508
2287.465498	44976.216252	47.536513
2283.959326	44363.466717	47.541517
2280.701955	43761.215676	47.546522
2277.079647	43149.995165	47.551527
2273.406804	42548.108049	47.556532
2270.221518	41929.922489	47.561537
2266.548161	41319.806853	47.566541
2262.986682	40708.841157	47.571546
2259.252436	40093.386089	47.576551
2256.044130	39487.941088	47.581556
2252.277958	38873.356095	47.586561
2248.734465	38261.213756	47.591565
2245.254655	37646.213379	47.596570
2241.861873	37034.957333	47.601575
2238.362084	36428.115818	47.606580
2234.848483	35817.401508	47.611585
2231.059310	35208.535188	47.616589
2227.967521	34595.083669	47.621594
2224.413363	33985.296842	47.626599
2220.831658	33369.218957	47.631604
2217.289938	32749.134530	47.636609
2213.743239	32151.714843	47.641613
2210.067184	31537.156968	47.646618
2206.586807	30934.317715	47.651623
2202.855737	30319.170696	47.656628
2199.735101	29704.606062	47.661633
2196.061066	29099.144491	47.666637
2192.560091	28483.458828	47.671642
2189.354144	27880.019897	47.676647
2185.696207	27270.510094	47.681652
2182.185606	26654.120755	47.686657
2178.150850	26051.283265	47.691661
2174.662291	25441.352233	47.696666
2171.397880	24832.462844	47.701671
2167.922316	24226.260352	47.706676
2164.193900	23616.067285	47.711681
2160.476865	23016.185704	47.716685
2157.373845	22415.954244	47.721690
2153.356601	21809.947552	47.726695
2149.782676	21204.523893	47.731700
2146.227156	20610.074416	47.736705
2142.340683	20021.509197	47.741709
2138.993439	19421.381539	47.746714
2135.224909	18831.541615	47.751719
2131.250060	18249.560992	47.756724
2127.333387	17686.519344	47.761729
2122.726601	17127.578738	47.766733
2118.558776	16564.852657	47.771738
2114.351138	16023.478333	47.776743
2109.931642	15490.723550	47.781748
2105.804076	14961.940307	47.786753
2101.995025	14456.668992	47.791757
2098.021999	13947.380819	47.796762
2093.638777	13458.027355	47.801767
2089.979213	12992.448207	47.806772
2086.351080	12510.479644	47.811777
2082.750014	12045.962597	47.816781
2079.386714	11583.620158	47.821786
2075.522725	11123.494310	47.826791
2071.887663	10678.029091	47.831796
2068.235569	10221.308046	47.836801
2064.555949	9773.459225	47.841805
2061.152216	9340.255818	47.846810
2057.212871	8894.355098	47.851815
2053.172651	8464.648485	47.856820
2049.734861	8039.365187	47.861825
2045.785011	7617.982060	47.866829
2043.005920	7197.629036	47.871834
2039.371114	6785.812053	47.876839
2035.886229	6370.382576	47.881844
2032.340078	5951.215498	47.886849
2028.554922	5542.266463	47.891853
2025.096423	5129.006704	47.896858
2021.419249	4726.002274	47.901863
2017.999201	4322.235764	47.906868
2014.125983	3927.674854	47.911873
2010.501846	3541.943868	47.916877
2007.261198	3136.849988	47.921882
2003.642226	2754.470123	47.926887
1999.833516	2366.078107	47.931892
1996.438361	1981.259276	47.936897
1992.703358	1599.380802	47.941901
1988.368705	1231.575637	47.946906
1984.626888	873.161507	47.951911
1979.837080	524.114809	47.956916
1973.436687	259.496829	47.961921
1963.685972	92.507845	47.966925
1950.131276	87.638293	47.971930
1940.889676	94.470760	47.976935
1935.354822	99.688630	47.981940
1932.562080	92.356378	47.986945
1930.697070	97.404883	47.991949
1929.496230	86.382756	47.996954
1928.202315	87.599704	48.001959
1925.474302	93.339334	48.006964
1923.262726	78.652754	48.011969
1919.927638	92.487894	48.016973
1916.684535	85.124500	48.021978
1913.505994	88.906309	48.026983
1910.169022	81.294940	48.031988
1906.782973	77.633194	48.036993
1903.402272	82.420888	48.041997
1900.084472	78.748522	48.047002
1897.184327	75.628078	48.052007
1893.248102	85.235143	48.057012
1890.319751	71.235927	48.062017
1886.825617	77.189701	48.067021
1883.649021	71.932489	48.072026
1880.362511	72.918563	48.077031
1877.107733	79.319132	48.082036
1874.049951	67.706522	48.087041
1869.951682	86.523053	48.092045
1866.302641	83.335671	48.097050
1863.495127	88.793449	48.102055
1860.311048	81.477826	48.107060
1856.628481	74.749146	48.112065
1853.053851	77.605525	48.117069
1850.038749	72.592097	48.122074
1846.538678	68.410277	48.127079
1842.784967	79.902977	48.132084
1839.543267	75.589196	48.137089
1835.787126	77.920176	48.142093
1832.466160	78.402259	48.147098
1829.111547	81.417383	48.152103
1825.771255	90.925374	48.157108
1822.646444	90.766333	48.162113
1818.922667	83.895375	48.167117
1815.698786	77.117458	48.172122
1811.790916	80.212362	48.177127
1808.215530	86.548941	48.182132
1804.878874	82.534675	48.187137
1801.683415	83.772336	48.192141
1797.995224	77.389384	48.197146
1794.469972	78.621426	48.202151
1791.307880	80.891590	48.207156
1787.946894	75.925675	48.212161
1784.136956	83.080194	48.217165
1781.031175	84.588633	48.222170
1777.430337	68.954067	48.227175
1773.741402	81.347832	48.232180
1770.722741	78.831131	48.237185
1766.885680	81.633448	48.242189
1763.624718	71.083846	48.247194
1759.928480	88.195837	48.252199
1756.530760	89.841462	48.257204
1753.003919	86.144699	48.262209
1749.369683	85.970039	48.267213
1746.465890	74.020273	48.272218
1742.614818	71.158577	48.277223
1738.847758	72.886996	48.282228
1735.869402	70.307080	48.287233
1732.128175	78.966320	48.292237
1728.938852	71.461714	48.297242
1725.610229	81.587970	48.302247
1721.910954	86.241760	48.307252
1718.673092	79.744438	48.312257
1714.497951	74.281998	48.317261
1711.350566	70.747644	48.322266
1707.733005	65.910259	48.327271
1704.336220	78.198440	48.332276
1701.179543	71.947911	48.337281
1697.411378	79.548340	48.342285
1694.009685	80.381516	48.347290
1690.678882	74.809811	48.352295
1686.935557	74.598354	48.357300
1683.424579	72.654989	48.362305
1679.403804	74.473520	48.367309
1676.380468	78.430495	48.372314
1673.197144	71.446974	48.377319
1669.441462	84.483869	48.382324
1666.311654	78.706880	48.387329
1662.515124	81.218163	48.392333
1659.044636	91.157700	48.397338
1655.699975	73.379422	48.402343
1651.990615	73.906152	48.407348
1648.713596	73.593648	48.412353
1645.085299	86.800540	48.417357
1641.366052	80.261094	48.422362
1638.079414	84.401419	48.427367
1634.490858	75.525805	48.432372
1631.449933	74.066097	48.437377
1627.684956	77.825298	48.442381
1624.147516	73.788523	48.447386
1620.788399	73.957028	48.452391
1616.976733	87.243079	48.457396
1613.605061	75.170008	48.462401
1609.921088	79.568325	48.467405
1606.880893	76.074245	48.472410
1603.762583	69.931652	48.477415
1599.533575	85.693398	48.482420
1595.819534	73.841295	48.487425
1592.625888	80.479127	48.492429
1589.512626	74.607827	48.497434
1585.937513	78.546284	48.502439
1582.422746	74.651515	48.507444
1579.080660	69.325189	48.512449
1575.248764	75.369509	48.517453
1571.695304	74.505263	48.522458
1568.229921	77.711646	48.527463
1564.247537	77.192565	48.532468
1561.091703	68.354019	48.537473
1557.791545	74.015026	48.542477
1554.262592	67.923699	48.547482
1550.952030	76.905047	48.552487
1547.030652	87.623430	48.557492
1543.857527	72.868290	48.562497
1539.968192	81.955542	48.567501
1536.935032	82.864245	48.572506
1533.730950	74.627985	48.577511
1529.809305	83.081199	48.582516
1526.402007	69.115475	48.587521
1522.587648	72.268610	48.592525
1519.343107	71.561928	48.597530
1515.810787	75.683551	48.602535
1512.309250	77.946455	48.607540
1509.215355	76.355800	48.612545
1505.167853	82.712089	48.617549
1501.776984	78.155815	48.622554
1498.356737	75.043599	48.627559
1494.810115	75.677889	48.632564
1491.717455	63.941067	48.637569
1488.041794	75.930970	48.642573
1484.092775	74.818258	48.647578
1480.875512	65.236327	48.652583
1476.858799	78.475193	48.657588
1473.762110	74.907665	48.662593
1470.511883	75.024434	48.667597
1466.747728	71.794910	48.672602
1463.236703	75.710745	48.677607
1459.861895	77.542647	48.682612
1456.671561	70.117332	48.687617
1453.056887	67.139787	48.692621
1449.140804	72.292399	48.697626
1445.989858	68.869360	48.702631
1442.440635	69.608462	48.707636
1438.843785	71.196521	48.712641
1435.104051	73.806547	48.717645
1431.713992	70.379599	48.722650
1428.338373	66.668835	48.727655
1424.887908	73.356134	48.732660
1421.486866	58.566906	48.737665
1417.767914	67.292283	48.742669
1414.464117	63.250810	48.747674
1411.119487	61.572645	48.752679
1406.962278	71.112870	48.757684
1403.921911	72.237836	48.762689
1400.516856	62.289689	48.767693
1396.834083	65.874761	48.772698
1393.301268	67.433874	48.777703
1389.531151	78.963927	48.782708
1386.549002	66.874570	48.787713
1382.742983	63.724341	48.792717
1379.112323	64.694419	48.797722
1375.814693	63.375931	48.802727
1372.523641	75.328116	48.807732
1369.399350	64.102431	48.812737
1365.413528	66.092719	48.817741
1361.582548	72.662080	48.822746
1358.246697	77.161248	48.827751
1354.738875	71.487434	48.832756
1351.296610	67.274535	48.837761
1347.692432	66.013255	48.842765
1344.199463	70.688736	48.847770
1341.099499	66.036589	48.852775
1336.837040	76.232267	48.857780
1333.802324	80.652929	48.862785
1330.113928	80.198846	48.867789
1326.833838	76.875013	48.872794
1323.798358	69.748313	48.877799
1320.094114	72.450900	48.882804
1316.716885	71.334629	48.887809
1312.614789	70.679191	48.892813
1308.988640	82.376659	48.897818
1305.727747	67.651055	48.902823
1302.470922	69.050162	48.907828
1299.182067	61.285878	48.912833
1295.649425	72.348702	48.917837
1291.830054	76.432763	48.922842
1288.282602	70.787273	48.927847
1284.683317	73.182466	48.932852
1281.650412	63.457983	48.937857
1277.866727	65.701548	48.942861
1274.564324	74.184930	48.947866
1270.687161	72.162571	48.952871
1267.193224	69.337096	48.957876
1263.650625	62.608875	48.962881
1260.229875	73.214531	48.967885
1256.542829	67.119386	48.972890
1253.431567	63.582629	48.977895
1249.669346	71.384624	48.982900
1246.428572	70.936805	48.987905
1242.841943	72.355615	48.992909
1239.308189	63.446239	48.997914
1236.013800	70.520530	49.002919
1232.363501	71.582264	49.007924
1228.943323	68.296069	49.012929
1225.301924	76.389302	49.017933
1221.392689	72.698350	49.022938
1218.307305	66.341884	49.027943
1214.920690	73.582390	49.032948
1211.278932	63.493955	49.037953
1207.765487	66.805917	49.042957
1204.369575	63.243873	49.047962
1201.094015	67.420459	49.052967
1196.992170	70.928412	49.057972
1193.856777	60.574506	49.062977
1190.273437	65.463375	49.067981
1186.754074	68.406109	49.072986
1183.459420	56.159802	49.077991
1179.544071	65.447256	49.082996
1175.921895	64.454548	49.088001
1172.632078	69.614099	49.093005
1168.971495	65.074549	49.098010
1166.036241	60.501191	49.103015
1162.182334	71.288163	49.108020
1159.048199	57.773545	49.113025
1155.802867	68.905540	49.118029
1151.590662	63.509077	49.123034
1148.134281	68.549026	49.128039
1144.548811	76.728467	49.133044
1141.225385	72.544554	49.138049
1137.619252	74.456782	49.143053
1134.107700	64.038054	49.148058
1130.927717	77.149841	49.153063
1127.436950	73.662679	49.158068
1123.889097	62.506137	49.163073
1120.294297	69.519628	49.168077
1116.628065	65.676976	49.173082
1113.379386	63.316372	49.178087
1109.873034	62.302480	49.183092
1106.353168	63.445162	49.188097
1102.774371	69.671569	49.193101
1098.893934	63.533789	49.198106
1095.631776	63.279137	49.203111
1092.037813	64.452336	49.208116
1088.749801	57.526334	49.213121
1085.048677	70.754036	49.218125
1081.533174	68.776647	49.223130
1078.279643	61.307451	49.228135
1074.932146	69.101845	49.233140
1071.126732	65.217590	49.238145
1067.639446	63.302249	49.243149
1064.274713	61.975259	49.248154
1060.796803	56.622699	49.253159
1057.595315	54.305377	49.258164
1053.783798	57.682731	49.263169
1050.068200	68.830981	49.268173
1046.760537	62.942568	49.273178
1043.491560	64.659958	49.278183
1039.299152	70.020123	49.283188
1035.938104	63.133970	49.288193
1032.446295	60.713148	49.293197
1029.015287	62.591799	49.298202
1025.829438	57.146327	49.303207
1022.487171	66.129452	49.308212
1018.891223	55.360065	49.313217
1014.857585	61.223851	49.318221
1011.153595	61.357515	49.323226
1007.944330	67.130946	49.328231
1004.424279	72.202963	49.333236
1001.081171	63.766981	49.338241
997.694606	75.167733	49.343245
994.535810	62.691510	49.348250
990.705933	62.971320	49.353255
987.066392	62.576111	49.358260
983.474940	63.464199	49.363265
979.970857	61.576794	49.368269
976.638010	73.051438	49.373274
973.476099	73.499350	49.378279
969.722514	67.984074	49.383284
966.144396	63.064732	49.388289
962.342576	63.431924	49.393293
959.239276	56.913779	49.398298
956.090675	61.861539	49.403303
952.055382	64.944714	49.408308
948.477227	59.870361	49.413313
944.708274	65.787863	49.418317
941.652011	64.343270	49.423322
938.228094	62.032112	49.428327
934.727469	66.863833	49.433332
931.231784	66.674022	49.438337
927.827582	73.078903	49.443341
924.128362	68.178418	49.448346
920.332831	64.881094	49.453351
916.607641	67.852727	49.458356
913.618158	64.581789	49.463361
910.501759	57.790451	49.468365
906.425193	66.903702	49.473370
902.783369	59.498144	49.478375
899.120757	69.265114	49.483380
896.104956	58.886323	49.488385
892.785820	61.222124	49.493389
889.421765	55.361499	49.498394
886.009077	60.790123	49.503399
882.130186	55.636049	49.508404
878.709335	62.141595	49.513409
875.025231	67.565016	49.518413
871.111851	65.959631	49.523418
867.889139	56.192009	49.528423
864.387247	64.725435	49.533428
861.053806	57.129516	49.538433
857.422602	58.545813	49.543437
854.021083	59.081655	49.548442
850.518993	62.904395	49.553447
847.080012	69.741790	49.558452
843.757233	57.322768	49.563457
839.897969	60.603174	49.568461
836.389038	65.692452	49.573466
832.888270	58.451607	49.578471
829.702798	61.937169	49.583476
826.151510	60.870197	49.588481
822.452974	59.658473	49.593485
818.587463	65.929529	49.598490
815.351958	58.919471	49.603495
811.949346	68.241020	49.608500
808.515518	66.962781	49.613505
804.802220	59.786662	49.618509
801.758439	66.056351	49.623514
798.715372	62.385655	49.628519
794.570833	60.987104	49.633524
791.023194	65.921064	49.638529
787.245405	61.890191	49.643533
783.433147	64.986120	49.648538
780.354465	51.795145	49.653543
776.995988	57.072971	49.658548
774.045840	64.068385	49.663553
769.895461	65.052996	49.668557
766.030814	64.752966	49.673562
762.930334	52.248742	49.678567
759.150496	60.480598	49.683572
756.000734	57.063794	49.688577
752.766955	59.392648	49.693581
748.862722	62.578826	49.698586
745.705831	55.249668	49.703591
742.032828	63.600933	49.708596
738.261167	60.144903	49.713601
734.370395	57.624882	49.718605
731.053467	62.437513	49.723610
728.198234	51.935689	49.728615
724.468537	63.570182	49.733620
721.140592	61.500373	49.738625
717.969867	59.497836	49.743629
714.093264	58.895963	49.748634
710.970308	50.821230	49.753639
706.829097	62.124324	49.758644
703.333823	50.611692	49.763649
699.713518	55.765771	49.768653
696.212251	58.857589	49.773658
692.654720	55.263833	49.778663
689.156764	54.131632	49.783668
685.670253	53.453219	49.788673
682.089445	59.597709	49.793677
678.902007	52.709905	49.798682
675.723622	53.619146	49.803687
671.830100	65.503765	49.808692
668.488788	54.312012	49.813697
664.662306	57.739189	49.818701
661.111744	64.989423	49.823706
658.028774	58.373252	49.828711
654.104476	55.330131	49.833716
650.654840	59.097268	49.838721
647.196913	56.778791	49.843725
643.885086	62.043039	49.848730
640.190572	56.354119	49.853735
636.835426	64.228813	49.858740
633.490036	55.283909	49.863745
629.704633	50.988502	49.868749
626.633472	63.649913	49.873754
623.231129	55.036572	49.878759
619.137628	61.422227	49.883764
615.955436	45.858835	49.888769
612.589514	53.108797	49.893773
608.969746	55.137095	49.898778
605.054537	53.487745	49.903783
601.258805	70.941026	49.908788
597.855948	51.337175	49.913793
594.630119	58.619114	49.918797
591.252261	62.314974	49.923802
588.585884	54.441260	49.928807
584.304909	61.349636	49.933812
580.963182	61.689545	49.938817
577.429604	65.915835	49.943821
573.436514	56.461184	49.948826
570.102739	54.158193	49.953831
566.839028	64.407227	49.958836
563.382419	55.084192	49.963841
559.761942	54.103957	49.968845
555.952612	53.652982	49.973850
552.585943	49.618260	49.978855
548.944881	52.605307	49.983860
546.011154	44.292348	49.988865
542.801656	44.883752	49.993869
539.014544	56.514530	49.998874
535.542687	59.117744	50.003879
531.908313	49.787592	50.008884
528.167732	55.998094	50.013889
524.896818	52.609676	50.018893
520.920981	47.518218	50.023898
517.752251	46.021586	50.028903
514.273800	55.687132	50.033908
510.255942	48.283250	50.038913
507.025756	47.166335	50.043917
503.283887	41.219070	50.048922
500.230824	48.037529	50.053927
496.381133	50.709057	50.058932
493.106627	46.324650	50.063937
489.898207	48.421797	50.068941
486.369861	53.830490	50.073946
482.842486	51.193829	50.078951
479.311168	55.710833	50.083956
475.459188	50.891158	50.088961
472.320896	47.330247	50.093965
468.460925	52.110380	50.098970
465.019139	46.891502	50.103975
461.907481	46.879242	50.108980
458.413175	56.085365	50.113985
454.443668	52.625385	50.118989
450.971323	53.824016	50.123994
447.599136	57.338676	50.128999
443.914228	54.413343	50.134004
440.685317	52.287029	50.139009
437.158416	53.997177	50.144013
433.586752	45.293183	50.149018
430.150060	51.510165	50.154023
426.746815	54.729114	50.159028
422.899876	54.992674	50.164033
419.593776	56.991145	50.169037
416.211983	52.455776	50.174042
413.042274	59.089929	50.179047
408.986073	56.731754	50.184052
405.490978	49.433166	50.189057
402.196064	47.680955	50.194061
398.445766	60.451257	50.199066
395.110506	41.944237	50.204071
391.427923	59.316617	50.209076
388.130067	57.697738	50.214081
384.589201	50.374643	50.219085
380.920839	54.299240	50.224090
377.784343	52.111093	50.229095
374.143338	58.679419	50.234100
370.627965	50.036274	50.239105
367.241395	51.167779	50.244109
363.398394	52.338706	50.249114
360.398422	46.627133	50.254119
356.747720	66.155337	50.259124
352.875107	53.553119	50.264129
349.279441	49.145969	50.269133
345.867698	55.862097	50.274138
342.973701	45.647955	50.279143
338.873103	55.150947	50.284148
335.313929	54.683205	50.289153
331.675863	52.664897	50.294157
328.569201	50.339238	50.299162
325.269543	37.707949	50.304167
321.801556	51.089174	50.309172
317.974078	44.465594	50.314177
314.416165	49.106971	50.319181
310.828951	60.760424	50.324186
307.482679	53.761378	50.329191
303.938828	55.768402	50.334196
300.481932	49.014366	50.339201
297.040970	49.353941	50.344205
293.199005	63.236311	50.349210
289.914515	54.085850	50.354215
286.329955	52.321802	50.359220
283.140738	48.974486	50.364225
279.545361	56.434196	50.369229
276.216332	51.643872	50.374234
272.784092	52.991300	50.379239
268.867951	54.837997	50.384244
265.252910	54.094233	50.389249
261.877596	52.468451	50.394253
258.273688	61.685324	50.399258
255.016684	53.024123	50.404263
251.271327	60.276239	50.409268
247.779502	48.238010	50.414273
244.874805	48.402357	50.419277
240.752170	59.772186	50.424282
237.520227	47.484698	50.429287
233.172957	57.956220	50.434292
230.119522	50.139666	50.439297
226.956293	46.000563	50.444301
223.637823	52.142210	50.449306
220.424679	50.873989	50.454311
216.731447	60.743829	50.459316
213.415590	52.784642	50.464321
209.752013	48.008451	50.469325
205.640691	55.830059	50.474330
202.515630	44.357984	50.479335
198.231064	55.386040	50.484340
195.380230	52.039836	50.489345
191.983434	49.914388	50.494349
188.277787	56.527594	50.499354
185.498041	45.982494	50.504359
181.401823	53.362003	50.509364
177.670239	48.134513	50.514369
174.257617	45.040289	50.519373
171.096697	55.048710	50.524378
167.560007	45.782526	50.529383
163.281178	52.026241	50.534388
160.265311	49.335305	50.539393
156.979115	47.888648	50.544397
153.137007	53.656260	50.549402
150.100227	40.360843	50.554407
146.375945	56.043992	50.559412
143.037652	52.485796	50.564417
139.588941	48.821411	50.569421
135.393361	44.390648	50.574426
132.137081	45.922664	50.579431
128.727395	41.995950	50.584436
125.132097	40.654368	50.589441
121.970472	38.669483	50.594445
118.195763	45.666755	50.599450
115.356177	37.620788	50.604455
111.712100	49.014186	50.609460
107.754491	49.839173	50.614465
104.124313	44.652857	50.619469
100.559692	46.542921	50.624474
97.725955	48.755777	50.629479
94.106811	55.105595	50.634484
90.206967	53.659577	50.639489
86.499923	47.890464	50.644493
83.097681	47.838075	50.649498
79.829070	41.070589	50.654503
76.046200	46.531601	50.659508
72.547303	49.398497	50.664513
69.256952	47.247004	50.669517
65.314276	56.171794	50.674522
62.654986	43.801519	50.679527
58.559175	47.001790	50.684532
55.214682	47.740818	50.689537
51.870330	55.386082	50.694541
48.350400	51.261416	50.699546
45.023632	38.979254	50.704551
40.862794	46.330872	50.709556
37.513039	46.207044	50.714561
34.420762	39.763279	50.719565
30.711565	52.878358	50.724570
27.748354	45.664711	50.729575
23.730285	50.219581	50.734580
20.105775	48.651617	50.739585
16.894572	48.132909	50.744589
13.099314	46.129638	50.749594
9.964090	37.446373	50.754599
6.057491	43.065857	50.759604
2.730155	49.240538	50.764609