Fri Aug 26 13:49:07 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
0.425295	116.789541	0.000000
0.602399	110.153112	0.005005
0.733655	108.436990	0.010010
0.999499	118.864196	0.015014
1.074180	107.744986	0.020019
0.441582	105.878883	0.025024
0.261684	103.629093	0.030029
0.350233	93.055046	0.035034
0.104391	87.500011	0.040038
-0.048929	69.162057	0.045043
-0.386535	72.517515	0.050048
-0.823852	62.329073	0.055053
-1.140362	54.776131	0.060058
-1.327509	52.673005	0.065062
-1.434321	45.448074	0.070067
-1.868982	44.307273	0.075072
-1.844416	47.286807	0.080077
-2.192945	33.285014	0.085082
-2.574031	37.479274	0.090086
-2.583356	15.683233	0.095091
-2.933320	21.910031	0.100096
-3.275986	7.328398	0.105101
-3.439775	6.721208	0.110106
-4.124580	4.100806	0.115110
-4.337801	-2.838627	0.120115
-4.602644	7.554085	0.125120
-4.264365	5.502030	0.130125
-5.042375	1.187774	0.135130
-5.296772	0.113817	0.140134
-5.562766	-9.471692	0.145139
-5.679401	-1.544392	0.150144
-6.215295	-4.592923	0.155149
-6.810053	-10.748475	0.160154
-7.155378	-0.286291	0.165158
-7.254571	-9.458025	0.170163
-7.102809	-8.703362	0.175168
-7.053994	-1.947059	0.180173
-7.164309	-4.302578	0.185178
-8.476128	-0.207015	0.190182
-8.704592	-0.218861	0.195187
-8.889687	-4.910159	0.200192
-8.844768	-7.501810	0.205197
-8.851578	-5.618347	0.210202
-8.921766	-1.241556	0.215206
-9.130105	-5.935562	0.220211
-9.514114	-13.436837	0.225216
-10.124370	-2.499987	0.230221
-10.303447	-22.652928	0.235226
-10.529447	-9.162745	0.240230
-10.581985	-11.375403	0.245235
-10.704492	-10.764691	0.250240
-11.218489	-16.660742	0.255245
-11.606706	-13.379675	0.260250
-11.728016	-5.306121	0.265254
-11.454435	-8.246576	0.270259
-11.589474	-9.993988	0.275264
-12.517748	-15.373137	0.280269
-12.539441	-4.505781	0.285274
-12.653681	-5.857814	0.290278
-12.915802	-4.744491	0.295283
-13.932477	10.080488	0.300288
-13.998554	-2.971868	0.305293
-14.255644	-4.203587	0.310298
-14.839448	-1.366612	0.315302
-14.371848	-3.508401	0.320307
-14.800343	2.999527	0.325312
-14.744998	-10.163474	0.330317
-14.475689	-9.066458	0.335322
-15.570324	-6.694094	0.340326
-15.582671	-15.588291	0.345331
-16.061693	-2.498454	0.350336
-16.095917	-10.699573	0.355341
-16.672776	-4.601967	0.360346
-17.388262	0.675697	0.365350
-17.164483	-10.007925	0.370355
-17.703897	-10.452230	0.375360
-17.714582	-6.815506	0.380365
-17.339742	-11.337728	0.385370
-17.737403	1.429408	0.390374
-17.633345	-5.043750	0.395379
-18.238789	-3.250571	0.400384
-18.650616	-3.923542	0.405389
-18.790825	-12.674450	0.410394
-18.908677	-3.155651	0.415398
-19.567765	-2.682849	0.420403
-19.958142	-2.119012	0.425408
-20.435364	0.751987	0.430413
-20.771890	-7.835485	0.435418
-20.570419	7.451539	0.440422
-20.413142	0.796093	0.445427
-20.281897	-0.711217	0.450432
-21.182458	3.908753	0.455437
-21.689629	0.270476	0.460442
-22.003899	-2.480379	0.465446
-21.957000	-2.826153	0.470451
-21.815793	-2.835447	0.475456
-22.295919	-1.647054	0.480461
-22.980116	-4.919258	0.485466
-23.558664	0.957159	0.490470
-23.291707	-1.194518	0.495475
-23.125469	1.645896	0.500480
-23.288121	1.797803	0.505485
-23.584786	-2.309832	0.510490
-24.368281	4.503297	0.515494
-24.351457	-3.389408	0.520499
-24.486862	-6.316803	0.525504
-25.570538	-4.752874	0.530509
-25.721002	-7.551377	0.535514
-25.531607	2.742134	0.540518
-25.629797	-7.132085	0.545523
-25.902715	-7.953229	0.550528
-26.508680	-4.211166	0.555533
-26.203812	-6.783182	0.560538
-26.808274	-7.116123	0.565542
-27.012522	-18.024151	0.570547
-27.447139	-13.568477	0.575552
-28.028603	-5.261934	0.580557
-27.971057	-14.049958	0.585562
-28.374618	-9.576973	0.590566
-27.910763	-11.578978	0.595571
-28.104524	-9.185534	0.600576
-28.689715	-5.845325	0.605581
-29.160198	-7.625928	0.610586
-29.328486	-13.544168	0.615590
-29.183416	-9.722896	0.620595
-29.212558	-12.660506	0.625600
-29.932940	-4.351315	0.630605
-30.054046	-10.159848	0.635610
-30.819006	-3.305317	0.640614
-31.003284	-3.804916	0.645619
-31.127691	-5.794421	0.650624
-31.228418	-7.588304	0.655629
-31.142888	-13.223372	0.660634
-32.136933	-8.332594	0.665638
-32.078194	-12.226653	0.670643
-32.402292	-13.710519	0.675648
-32.828576	-1.688714	0.680653
-32.740657	-9.747504	0.685658
-32.468451	-14.494181	0.690662
-32.717419	-15.211490	0.695667
-33.370028	-9.608273	0.700672
-34.019833	-1.041160	0.705677
-34.132310	-4.823143	0.710682
-34.130784	3.525506	0.715686
-34.482526	-4.357268	0.720691
-34.767974	-2.800567	0.725696
-35.092126	1.403802	0.730701
-34.960944	-7.281799	0.735706
-35.291012	1.257678	0.740710
-35.929888	3.404064	0.745715
-36.282764	3.579261	0.750720
-36.664760	17.011496	0.755725
-36.593021	1.466875	0.760730
-36.872763	3.184034	0.765734
-36.738434	-0.443396	0.770739
-36.734134	4.927836	0.775744
-37.738511	-0.306593	0.780749
-37.526551	-7.106586	0.785754
-37.868863	-6.417360	0.790758
-38.207741	-9.809764	0.795763
-38.284107	-4.622121	0.800768
-39.289960	-0.890560	0.805773
-39.133350	-0.029087	0.810778
-39.849614	-2.024514	0.815782
-39.421303	-5.612297	0.820787
-39.611859	-8.746230	0.825792
-39.579539	4.419013	0.830797
-40.035901	-1.773906	0.835802
-40.662275	-0.822160	0.840806
-41.093559	-3.611741	0.845811
-40.966646	-11.265328	0.850816
-41.313410	-5.728712	0.855821
-41.316129	-8.382545	0.860826
-42.006699	5.939253	0.865830
-42.323172	2.521212	0.870835
-42.580098	-7.961018	0.875840
-42.892252	-0.095022	0.880845
-42.727746	-6.033443	0.885850
-42.910172	-10.642899	0.890854
-42.708901	-15.353222	0.895859
-43.152277	-3.591339	0.900864
-44.047295	-1.702455	0.905869
-43.722818	-12.275206	0.910874
-44.311684	-1.917471	0.915878
-44.631714	-7.210995	0.920883
-44.884721	-10.958442	0.925888
-45.369979	-3.672915	0.930893
-45.535697	-10.205302	0.935898
-45.224463	-5.862591	0.940902
-45.869741	-9.052270	0.945907
-45.512594	-7.643076	0.950912
-46.463615	0.670391	0.955917
-46.633117	-5.788644	0.960922
-46.945832	0.429182	0.965926
-47.299296	-4.390918	0.970931
-46.859493	-2.934483	0.975936
-47.351879	-1.304434	0.980941
-47.365739	-7.379593	0.985946
-48.050991	1.275295	0.990950
-48.482689	-0.653711	0.995955
-48.391650	-6.824293	1.000960
-48.909901	-2.937705	1.005965
-48.697562	-3.236475	1.010970
-49.985031	-7.433440	1.015974
-50.179980	2.951547	1.020979
-50.380450	-10.965695	1.025984
-50.505249	3.489466	1.030989
-50.210137	2.146461	1.035994
-50.383467	-1.790557	1.040998
-50.118157	-5.647179	1.046003
-50.596410	-1.637110	1.051008
-51.299558	-5.573890	1.056013
-51.253781	-9.045166	1.061018
-51.769915	-9.376040	1.066022
-52.405645	2.010849	1.071027
-52.720380	2.006108	1.076032
-53.029892	-1.163087	1.081037
-53.079934	1.723655	1.086042
-53.658075	5.894806	1.091046
-53.828062	0.419737	1.096051
-53.435169	-1.150456	1.101056
-53.320501	-0.820272	1.106061
-53.203119	-4.419753	1.111066
-54.349089	-4.747471	1.116070
-54.776219	-4.646130	1.121075
-54.538719	-9.444350	1.126080
-54.763371	-9.257480	1.131085
-54.677683	-11.371441	1.136090
-55.534868	-5.363062	1.141094
-55.970290	-3.450828	1.146099
-55.794976	-7.682565	1.151104
-56.084791	-4.182709	1.156109
-56.862636	-15.687936	1.161114
-57.183565	-15.713858	1.166118
-57.514106	-12.150717	1.171123
-57.458938	-19.413492	1.176128
-57.668802	-14.954850	1.181133
-57.837605	-14.223039	1.186138
-57.859767	-7.120345	1.191142
-57.643334	-5.132440	1.196147
-58.545197	-6.339694	1.201152
-58.950639	-3.973400	1.206157
-58.811704	-15.558097	1.211162
-58.851375	-3.852745	1.216166
-59.317268	-7.598682	1.221171
-59.856025	-8.046252	1.226176
-60.232239	-5.444072	1.231181
-60.245805	-14.676586	1.236186
-60.121210	-1.225171	1.241190
-61.178750	-2.268986	1.246195
-61.185058	-5.668880	1.251200
-61.411918	4.303475	1.256205
-61.455612	-8.499266	1.261210
-61.671023	-1.505681	1.266214
-61.987340	-3.028723	1.271219
-62.462582	-12.262119	1.276224
-63.271427	-8.621342	1.281229
-63.174958	-2.963919	1.286234
-63.107667	-3.632396	1.291238
-63.099593	-6.025328	1.296243
-63.243093	-4.699528	1.301248
-63.584748	-3.947131	1.306253
-63.926222	-3.770545	1.311258
-64.888976	0.134634	1.316262
-65.096630	-9.235335	1.321267
-64.832997	-9.779365	1.326272
-64.795727	-13.590988	1.331277
-64.798251	-15.134413	1.336282
-65.825686	-3.085449	1.341286
-66.243854	-3.722631	1.346291
-66.112499	-18.150257	1.351296
-66.598788	-8.267226	1.356301
-66.305671	-8.670318	1.361306
-66.287005	-9.758316	1.366310
-66.903085	-6.305734	1.371315
-67.372048	-6.868571	1.376320
-67.826485	-8.639016	1.381325
-67.662201	-15.032963	1.386330
-67.523479	-7.142264	1.391334
-68.729082	-7.973207	1.396339
-69.030740	-14.373697	1.401344
-69.472213	-2.441276	1.406349
-69.248981	-7.224620	1.411354
-69.735157	-3.548663	1.416358
-69.420546	4.668983	1.421363
-69.154044	-2.696303	1.426368
-69.956200	2.828964	1.431373
-70.620337	-3.597347	1.436378
-70.371770	-4.651540	1.441382
-70.482688	-11.293694	1.446387
-70.692078	-15.465530	1.451392
-71.715571	-8.238567	1.456397
-71.891016	-13.260380	1.461402
-72.183871	-5.131648	1.466406
-72.061462	-2.316048	1.471411
-71.834370	-5.185991	1.476416
-72.437545	-1.593054	1.481421
-73.416922	-5.692460	1.486426
-73.746768	-2.607135	1.491430
-73.489759	-1.492386	1.496435
-73.411234	-10.286838	1.501440
-73.660277	3.602391	1.506445
-73.703540	-9.842634	1.511450
-73.877832	-13.311280	1.516454
-74.965675	-12.066229	1.521459
-75.044251	-10.782174	1.526464
-75.185718	-15.432805	1.531469
-75.180006	-5.392268	1.536474
-75.492635	-3.967371	1.541478
-76.278687	-4.253055	1.546483
-75.980506	-12.458470	1.551488
-76.590220	-0.686507	1.556493
-76.064520	-8.174403	1.561498
-76.572929	-4.545603	1.566502
-77.037833	-8.468857	1.571507
-77.994484	-12.998890	1.576512
-78.117748	-3.077471	1.581517
-78.013977	-5.826975	1.586522
-78.338953	-6.042085	1.591526
-78.186794	-2.123844	1.596531
-78.392522	-5.891307	1.601536
-78.314857	-5.046016	1.606541
-79.111750	-14.254637	1.611546
-79.296611	-8.138976	1.616550
-79.696921	-2.242859	1.621555
-79.655735	-0.828761	1.626560
-80.420067	-4.471285	1.631565
-80.752343	-3.998748	1.636570
-81.224208	-7.041426	1.641574
-81.198731	-8.690448	1.646579
-81.027138	-11.308148	1.651584
-81.197585	-2.322146	1.656589
-81.491175	-10.255095	1.661594
-81.453815	-2.475159	1.666598
-81.969980	-4.508066	1.671603
-82.482152	-5.102139	1.676608
-82.931642	-8.341283	1.681613
-82.855742	-12.535393	1.686618
-83.201559	-4.246561	1.691622
-83.278531	-4.879921	1.696627
-83.243077	-9.564427	1.701632
-84.210663	0.985147	1.706637
-84.333687	-1.773337	1.711642
-84.074653	-4.736835	1.716646
-84.121043	1.784360	1.721651
-84.854959	-3.333993	1.726656
-85.441858	0.984048	1.731661
-85.471339	9.666543	1.736666
-85.363718	-3.147104	1.741670
-85.784371	3.840474	1.746675
-85.950948	2.097972	1.751680
-86.824493	-2.581039	1.756685
-86.950395	2.560534	1.761690
-87.072365	-3.374409	1.766694
-87.084934	1.679919	1.771699
-87.061134	-8.823870	1.776704
-87.404462	-6.353356	1.781709
-88.183968	-2.502019	1.786714
-88.474543	0.903047	1.791718
-88.957407	-1.948101	1.796723
-88.606815	-13.290515	1.801728
-88.908749	-9.010518	1.806733
-88.838783	-9.480103	1.811738
-88.982521	-4.854591	1.816742
-89.723078	3.347015	1.821747
-89.864542	-4.714022	1.826752
-90.238967	-0.859319	1.831757
-90.203680	-7.568528	1.836762
-90.813440	-0.111762	1.841766
-90.733980	5.057947	1.846771
-91.233936	-7.072659	1.851776
-91.830892	8.189979	1.856781
-91.776161	-2.714084	1.861786
-91.864033	-1.884146	1.866790
-92.002409	-4.339693	1.871795
-91.925880	-5.088700	1.876800
-92.755917	-1.859059	1.881805
-93.084618	-7.208175	1.886810
-93.358009	-7.747680	1.891814
-93.497112	-1.680270	1.896819
-93.318250	-11.575472	1.901824
-93.502390	-2.805630	1.906829
-94.325975	-1.332813	1.911834
-94.553366	5.067874	1.916838
-94.786688	4.272202	1.921843
-94.454001	-3.188806	1.926848
-95.052922	-4.319845	1.931853
-95.477879	2.111602	1.936858
-95.916045	-1.872761	1.941862
-96.107944	4.430653	1.946867
-95.914495	-1.237037	1.951872
-96.091564	-4.034560	1.956877
-96.598348	-1.624014	1.961882
-97.164003	-8.885037	1.966886
-97.335635	-4.353255	1.971891
-97.201285	-3.823664	1.976896
-97.610503	6.686429	1.981901
-97.670744	-4.696422	1.986906
-98.536092	-2.748884	1.991910
-99.405750	1.401218	1.996915
-98.631031	2.453495	2.006912
-98.114423	-1.028967	2.016909
-97.871530	-9.638480	2.026906
-97.983565	-11.258657	2.036902
-97.006861	-3.700501	2.046899
-96.605496	-4.402794	2.056896
-95.813295	-4.136440	2.066893
-95.148024	-13.099977	2.076890
-94.943522	-12.463362	2.086886
-94.753567	-3.531471	2.096883
-94.092145	-9.291874	2.106880
-93.496731	-6.755325	2.116877
-92.608589	-3.858888	2.126874
-92.338340	-8.414850	2.136870
-92.224966	-8.207523	2.146867
-91.239849	-1.977937	2.156864
-91.085935	-9.727823	2.166861
-90.625162	-5.925408	2.176858
-89.875917	0.106495	2.186854
-89.523816	-1.319863	2.196851
-88.603385	2.220923	2.206848
-88.075222	-1.801845	2.216845
-88.213545	-3.392589	2.226842
-87.634996	-8.474875	2.236838
-86.953136	-1.884470	2.246835
-86.610758	-6.153900	2.256832
-85.744335	-1.572038	2.266829
-85.263696	-3.594930	2.276826
-85.091107	-4.942655	2.286822
-84.221002	-8.781086	2.296819
-84.070914	-6.510973	2.306816
-83.602593	-7.692509	2.316813
-82.800559	-6.182784	2.326810
-82.516505	-5.083401	2.336806
-81.773962	-2.310008	2.346803
-81.186838	-4.989352	2.356800
-80.833037	-4.851136	2.366797
-80.766905	-5.355519	2.376794
-79.793015	-8.291479	2.386790
-79.706108	-3.170111	2.396787
-78.922684	-1.505439	2.406784
-78.502830	-14.235160	2.416781
-77.688452	-6.277942	2.426778
-77.087111	-7.343977	2.436774
-76.901854	-9.137151	2.446771
-76.645173	-10.745049	2.456768
-75.785063	-14.889188	2.466765
-75.496890	-9.998723	2.476762
-74.556428	-14.646366	2.486758
-73.871889	-15.034799	2.496755
-74.247669	-10.943748	2.506752
-73.840337	-14.048077	2.516749
-72.647555	-8.430512	2.526746
-72.851149	-10.745997	2.536742
-71.643756	-5.602692	2.546739
-71.487134	-11.876856	2.556736
-70.973574	-12.118295	2.566733
-70.123961	-8.943438	2.576730
-69.860615	-10.568212	2.586726
-69.727279	-10.154925	2.596723
-68.474899	-9.592769	2.606720
-68.226232	-14.664870	2.616717
-68.021921	-9.514268	2.626714
-66.884119	-5.380123	2.636710
-67.051793	-2.987677	2.646707
-66.702906	-8.623396	2.656704
-65.797451	-11.583545	2.666701
-65.433833	-10.220961	2.676698
-65.014991	-10.358957	2.686694
-64.148949	-4.389587	2.696691
-63.888603	-8.145749	2.706688
-63.438991	-13.417027	2.716685
-62.704455	-8.849474	2.726682
-62.263124	-10.419600	2.736678
-62.279033	-9.175315	2.746675
-61.687622	-11.516383	2.756672
-60.655935	-12.114084	2.766669
-60.145125	-13.875586	2.776666
-60.211588	-3.528990	2.786662
-59.474931	-3.393366	2.796659
-58.582979	-5.657689	2.806656
-58.584802	-9.639118	2.816653
-57.608355	-10.171199	2.826650
-57.278584	-1.562004	2.836646
-56.849764	-5.965266	2.846643
-56.169181	-9.254687	2.856640
-55.652189	-11.131189	2.866637
-55.590897	-9.230541	2.876634
-55.053739	-4.039897	2.886630
-54.508459	-9.085326	2.896627
-54.104958	-4.016418	2.906624
-53.173691	-6.793693	2.916621
-52.717555	-8.762086	2.926618
-52.070073	-10.373812	2.936614
-51.394707	-9.414549	2.946611
-51.262408	-7.331727	2.956608
-50.944589	-15.544274	2.966605
-50.469133	-11.531909	2.976602
-50.038918	-10.759381	2.986598
-49.542839	-6.595008	2.996595
-48.920217	-11.871050	3.006592
-48.266565	-7.997298	3.016589
-47.305958	-3.553637	3.026586
-47.497746	-3.153082	3.036582
-46.777539	-4.766629	3.046579
-46.387116	-9.325465	3.056576
-45.617441	-4.985120	3.066573
-45.254116	-0.600511	3.076570
-45.060968	1.403148	3.086566
-43.990908	5.313436	3.096563
-43.924446	-0.116761	3.106560
-43.446793	-0.463478	3.116557
-42.660189	-6.579150	3.126554
-42.186276	-4.587529	3.136550
-42.185561	3.512222	3.146547
-40.996858	-5.051329	3.156544
-40.780031	-2.997506	3.166541
-40.469533	-2.326710	3.176538
-39.664021	0.737813	3.186534
-39.369847	-0.685862	3.196531
-38.670153	-3.465094	3.206528
-37.948710	-5.981625	3.216525
-37.906451	-5.684032	3.226522
-37.737535	-7.538016	3.236518
-36.558601	-9.593606	3.246515
-36.360852	-11.841704	3.256512
-36.039835	-10.529505	3.266509
-34.953487	-8.424172	3.276506
-34.727464	-8.874257	3.286502
-34.452483	-2.141305	3.296499
-33.703096	-7.104478	3.306496
-33.211730	-5.226443	3.316493
-32.897198	-4.233171	3.326490
-32.244977	-1.892356	3.336486
-31.988358	-4.973222	3.346483
-31.139318	-7.813718	3.356480
-30.757377	-9.289069	3.366477
-30.504440	-5.216714	3.376474
-29.703335	2.457488	3.386470
-29.203187	-1.196635	3.396467
-28.997968	-12.578352	3.406464
-27.827836	-7.647812	3.416461
-27.653365	-1.931878	3.426458
-27.630228	1.007380	3.436454
-26.543097	-7.793771	3.446451
-26.277981	-3.184804	3.456448
-25.922816	-2.356242	3.466445
-25.076845	-2.437201	3.476442
-24.760091	-7.149288	3.486438
-24.530859	-6.057206	3.496435
-23.450705	-3.659480	3.506432
-23.131015	-4.155826	3.516429
-23.021061	-3.460140	3.526426
-22.343348	-0.983916	3.536422
-21.881730	3.176323	3.546419
-20.738593	-1.525052	3.556416
-20.400584	-6.474858	3.566413
-20.256693	-2.220803	3.576410
-20.127728	-0.935719	3.586406
-19.432582	-2.415489	3.596403
-18.527492	2.020981	3.606400
-18.383466	-5.359920	3.616397
-17.420922	-1.917549	3.626394
-16.913620	7.642831	3.636390
-16.895046	1.691084	3.646387
-16.294384	2.791856	3.656384
-15.534895	1.146851	3.666381
-15.549908	7.883780	3.676378
-14.983824	0.924988	3.686374
-14.608503	0.096876	3.696371
-13.304495	-1.056389	3.706368
-12.831025	0.251081	3.716365
-13.019447	-0.571617	3.726362
-12.378929	-0.002887	3.736358
-11.833199	-4.418018	3.746355
-11.381393	1.824923	3.756352
-10.180363	-2.910808	3.766349
-9.722444	4.629937	3.776346
-10.034815	-4.437975	3.786342
-9.349871	2.117113	3.796339
-8.617726	3.086545	3.806336
-8.169833	-7.069050	3.816333
-7.978974	3.018918	3.826330
-7.480941	0.705058	3.836326
-6.730852	4.199516	3.846323
-6.002274	0.953303	3.856320
-5.805058	4.125210	3.866317
-5.230609	2.588207	3.876314
-4.713054	14.231338	3.886310
-4.283032	10.876391	3.896307
-4.112483	22.979020	3.906304
-3.518686	27.806076	3.916301
-3.197356	47.909027	3.926298
-2.796107	52.978305	3.936294
-2.485925	74.356439	3.946291
-1.545697	83.976164	3.956288
-1.435849	94.130649	3.966285
-0.544283	114.201911	3.976282
0.000000	127.882125	3.981286
-0.134058	132.939590	3.986291
0.448415	132.089658	3.991296
0.054578	147.206908	3.996301
0.366503	137.246607	4.001306
0.346666	150.185972	4.006310
0.495012	145.784394	4.011315
0.379519	149.064156	4.016320
0.173093	143.737078	4.021325
0.428621	148.869928	4.026330
0.392250	157.382736	4.031334
0.424498	157.425207	4.036339
0.434515	149.865678	4.041344
0.778719	163.191285	4.046349
1.288915	166.563452	4.051354
0.788625	162.114169	4.056358
0.510996	133.573683	4.061363
0.799128	151.916097	4.066368
0.262664	153.613132	4.071373
0.773235	154.090480	4.076378
0.654387	159.794138	4.081382
0.959547	164.008128	4.086387
1.011566	158.574369	4.091392
0.394851	153.225750	4.096397
0.666326	160.102467	4.101402
0.983512	171.758706	4.106406
0.872473	161.845264	4.111411
0.425840	163.427075	4.116416
0.652178	162.876194	4.121421
1.055505	163.373404	4.126426
0.903166	168.139504	4.131430
1.181523	163.825244	4.136435
1.378254	167.641676	4.141440
0.656482	159.648764	4.146445
0.729341	146.172879	4.151450
0.846806	157.255943	4.156454
1.344836	158.820384	4.161459
1.035946	158.517346	4.166464
0.298371	155.351496	4.171469
0.890341	159.505010	4.176474
0.778685	171.822789	4.181478
1.160367	172.329697	4.186483
1.083547	173.895058	4.191488
1.320955	167.062562	4.196493
1.647815	169.014313	4.201498
1.213057	165.912040	4.206502
1.191599	153.811213	4.211507
0.855343	151.035284	4.216512
0.811682	150.988336	4.221517
1.146209	153.030637	4.226522
1.202796	162.459094	4.231526
1.166943	160.721530	4.236531
0.958087	157.039936	4.241536
0.876266	167.106860	4.246541
1.196992	166.329316	4.251546
0.863628	165.909870	4.256550
0.926360	163.691897	4.261555
1.047680	163.207985	4.266560
1.211811	166.662506	4.271565
1.495985	169.139745	4.276570
1.320887	171.217105	4.281574
1.300641	165.263099	4.286579
1.395607	158.566676	4.291584
1.240116	173.494982	4.296589
1.123314	167.606627	4.301594
1.350807	169.678250	4.306598
1.385034	171.545852	4.311603
1.318582	172.302863	4.316608
1.136589	174.884320	4.321613
1.366472	165.961808	4.326618
0.870942	166.776133	4.331622
1.342142	166.294692	4.336627
1.650918	159.849709	4.341632
1.265938	169.887908	4.346637
1.240910	166.427620	4.351642
1.424996	167.895413	4.356646
1.434726	170.551420	4.361651
1.665983	169.379692	4.366656
0.913582	180.003436	4.371661
1.276699	170.076275	4.376666
1.130662	179.593234	4.381670
1.570397	185.693972	4.386675
1.794922	190.486821	4.391680
2.085817	186.382570	4.396685
1.790519	173.675812	4.401690
1.474973	184.541581	4.406694
1.592975	178.483791	4.411699
1.696109	166.594504	4.416704
1.617189	172.573516	4.421709
1.721771	172.569924	4.426714
0.972641	179.437879	4.431718
1.394241	175.528410	4.436723
1.336974	185.123297	4.441728
1.593143	188.762805	4.446733
1.595309	192.834156	4.451738
1.909159	201.738535	4.456742
1.940461	196.175117	4.461747
2.063636	195.624478	4.466752
1.552225	186.418750	4.471757
1.992822	166.798681	4.476762
1.571076	178.592120	4.481766
1.637228	168.249300	4.486771
1.550290	180.408216	4.491776
1.524879	190.567608	4.496781
1.918514	193.097409	4.501786
1.692002	188.086649	4.506790
1.990672	197.784309	4.511795
2.223694	193.084805	4.516800
2.133738	191.352498	4.521805
1.827279	176.116534	4.526810
1.974333	171.730970	4.531814
1.736700	179.107729	4.536819
1.921351	180.088228	4.541824
1.671308	179.288823	4.546829
2.013966	186.284177	4.551834
2.033571	194.687050	4.556838
1.902479	194.024143	4.561843
1.984769	198.326624	4.566848
1.624309	200.034224	4.571853
1.664640	192.479447	4.576858
1.574236	197.216930	4.581862
1.725113	194.827045	4.586867
1.723157	190.645006	4.591872
1.762282	190.645278	4.596877
2.091956	195.757107	4.601882
2.075217	198.214764	4.606886
1.991381	205.241729	4.611891
1.843112	197.580277	4.616896
2.389287	200.776010	4.621901
2.391208	196.125141	4.626906
2.457552	200.395305	4.631910
2.045589	199.690710	4.636915
1.831662	197.363951	4.641920
1.829786	203.520798	4.646925
1.755922	192.744194	4.651930
2.192519	207.694234	4.656934
2.005582	224.449759	4.661939
2.341574	221.423621	4.666944
2.530220	226.630181	4.671949
2.748602	222.714378	4.676954
2.526239	214.760741	4.681958
2.248962	207.578104	4.686963
2.091662	203.195627	4.691968
2.050631	200.674273	4.696973
2.456189	199.497551	4.701978
2.246578	204.392798	4.706982
2.272872	204.132483	4.711987
2.542198	199.243832	4.716992
2.283618	202.659773	4.721997
2.134084	206.314996	4.727002
2.113022	213.132879	4.732006
2.381891	221.370407	4.737011
2.478611	224.237500	4.742016
2.329937	226.171549	4.747021
2.670793	215.991570	4.752026
2.286867	216.848631	4.757030
2.276653	229.824520	4.762035
2.603417	223.617154	4.767040
2.448626	224.286682	4.772045
2.655130	222.486069	4.777050
2.374648	227.284791	4.782054
2.579580	234.627468	4.787059
2.615148	224.387451	4.792064
2.248018	229.576143	4.797069
2.441038	224.104592	4.802074
2.470851	228.589254	4.807078
2.458942	226.316457	4.812083
2.618900	223.548676	4.817088
2.641902	226.443065	4.822093
2.566822	228.384639	4.827098
2.744486	231.128401	4.832102
2.439474	222.637147	4.837107
2.769017	215.584648	4.842112
2.459277	218.907320	4.847117
2.631077	220.095462	4.852122
2.333406	226.061095	4.857126
2.478758	230.866282	4.862131
2.580943	223.659358	4.867136
2.404046	228.261623	4.872141
2.795503	220.152303	4.877146
2.454520	218.895666	4.882150
2.346542	222.784861	4.887155
2.666704	235.136688	4.892160
2.591157	242.725514	4.897165
3.186115	239.418613	4.902170
2.865774	253.657660	4.907174
3.090254	246.972676	4.912179
2.746352	233.343319	4.917184
2.904463	231.698932	4.922189
2.626495	228.255869	4.927194
2.941170	240.656009	4.932198
2.897987	248.651077	4.937203
3.402805	243.292323	4.942208
3.001146	236.758613	4.947213
2.934333	232.235493	4.952218
2.965189	229.063879	4.957222
2.500867	227.446803	4.962227
2.965623	230.860858	4.967232
2.911042	241.727159	4.972237
3.169488	244.243214	4.977242
2.623344	241.506277	4.982246
2.842684	240.602150	4.987251
3.426306	246.041442	4.992256
3.322786	257.940406	4.997261
3.087449	250.865114	5.002266
2.819979	235.850815	5.007270
2.558129	237.666448	5.012275
3.180100	251.894817	5.017280
3.082922	252.394028	5.022285
3.147843	248.369238	5.027290
2.886552	243.066492	5.032294
2.981997	252.555383	5.037299
3.544169	240.047259	5.042304
3.217170	253.243326	5.047309
3.314493	249.763972	5.052314
3.390489	254.228795	5.057318
3.179178	253.951691	5.062323
3.118366	251.139187	5.067328
2.971556	258.770751	5.072333
3.062475	251.815501	5.077338
2.728929	251.111349	5.082342
3.001863	258.718688	5.087347
2.896495	244.745305	5.092352
3.269873	257.797529	5.097357
3.075841	248.887194	5.102362
3.150862	253.374314	5.107366
3.048779	250.612528	5.112371
3.388477	256.463116	5.117376
3.142025	273.547485	5.122381
3.594426	271.464977	5.127386
3.690336	272.952835	5.132390
3.262488	262.876695	5.137395
3.433272	254.314510	5.142400
3.256636	263.747695	5.147405
3.377750	269.249514	5.152410
3.446274	276.660902	5.157414
3.457183	274.387710	5.162419
3.834938	275.259057	5.167424
3.406205	273.807274	5.172429
3.681551	263.738706	5.177434
3.499845	259.742821	5.182438
3.303946	253.923700	5.187443
3.550342	258.260754	5.192448
3.328329	260.316955	5.197453
3.903528	260.967739	5.202458
3.597407	268.402653	5.207462
3.468596	255.676242	5.212467
3.709677	258.859378	5.217472
2.997969	259.428961	5.222477
3.382127	260.777027	5.227482
3.553644	268.317905	5.232486
3.889092	273.030232	5.237491
3.984228	269.424668	5.242496
3.801585	275.230042	5.247501
3.903349	269.083001	5.252506
3.658972	255.874720	5.257510
3.197049	267.453014	5.262515
3.524286	269.945709	5.267520
3.724762	271.205318	5.272525
3.693468	267.420126	5.277530
3.833223	273.349306	5.282534
3.518420	282.294659	5.287539
3.878493	274.392677	5.292544
3.809191	279.990584	5.297549
3.807862	279.481474	5.302554
3.838904	277.866359	5.307558
3.670224	275.671747	5.312563
3.677792	275.366891	5.317568
3.491997	285.763276	5.322573
3.874842	271.742332	5.327578
4.088110	268.630893	5.332582
3.927565	278.877813	5.337587
4.149869	274.834840	5.342592
3.869560	271.354169	5.347597
3.858896	275.804016	5.352602
3.664881	279.712947	5.357606
4.015640	285.084105	5.362611
3.865794	279.289441	5.367616
3.840906	287.332297	5.372621
3.744310	288.166771	5.377626
3.874081	290.712359	5.382630
3.710450	289.776110	5.387635
4.134570	278.909264	5.392640
3.713478	290.028808	5.397645
4.258232	293.291217	5.402650
4.284870	301.768974	5.407654
3.948530	291.007868	5.412659
4.235641	287.834309	5.417664
4.398742	290.355726	5.422669
4.043461	286.409006	5.427674
3.953714	284.686149	5.432678
3.930098	289.970068	5.437683
4.238790	292.914897	5.442688
3.887200	297.870239	5.447693
4.264057	300.326739	5.452698
4.054002	298.606794	5.457702
4.276925	304.466088	5.462707
4.319210	300.935184	5.467712
4.470769	313.468338	5.472717
4.678610	304.286602	5.477722
4.314699	288.243253	5.482726
4.162516	284.979907	5.487731
4.197029	279.422290	5.492736
3.931446	285.914447	5.497741
4.299376	302.153391	5.502746
4.027583	304.780485	5.507750
4.296467	303.995189	5.512755
4.441610	300.435615	5.517760
4.529450	321.707335	5.522765
4.307885	305.512097	5.527770
4.022707	307.698358	5.532774
4.487775	306.426944	5.537779
4.604108	301.780380	5.542784
4.077766	308.708607	5.547789
3.929921	308.554496	5.552794
4.190754	305.872235	5.557798
3.943424	306.926328	5.562803
4.077660	305.469146	5.567808
4.084376	318.009036	5.572813
4.307222	324.665602	5.577818
4.395267	332.029681	5.582822
3.968741	339.660539	5.587827
4.713856	328.300768	5.592832
4.719425	335.421430	5.597837
4.797606	333.375034	5.602842
4.658130	334.263641	5.607846
4.225177	336.321057	5.612851
4.577407	332.109148	5.617856
4.577074	334.750928	5.622861
4.949216	331.855183	5.627866
4.526164	332.107746	5.632870
4.342393	342.310863	5.637875
4.690990	331.224794	5.642880
4.520084	334.124082	5.647885
4.654027	336.681682	5.652890
4.925836	336.690019	5.657894
4.642376	339.081657	5.662899
4.649442	333.996524	5.667904
4.665173	337.290689	5.672909
4.573742	335.507979	5.677914
4.872887	333.123464	5.682918
4.344854	330.576678	5.687923
4.677017	332.647843	5.692928
4.329630	333.695369	5.697933
4.342094	333.453024	5.702938
4.681893	342.321797	5.707942
5.015225	355.981431	5.712947
5.129982	351.059858	5.717952
4.830605	350.575004	5.722957
4.724890	339.006017	5.727962
5.122296	346.432666	5.732966
4.993362	341.450962	5.737971
4.866415	339.993315	5.742976
4.818804	333.916964	5.747981
4.731711	342.099242	5.752986
5.152741	339.559710	5.757990
4.745232	347.934245	5.762995
5.004971	350.655755	5.768000
5.032249	359.139768	5.773005
5.244732	353.744240	5.778010
4.995823	337.382390	5.783014
4.854435	337.382295	5.788019
4.742446	356.574980	5.793024
4.826469	361.269530	5.798029
5.140906	351.656727	5.803034
5.313678	347.048819	5.808038
5.094265	355.473164	5.813043
5.315893	353.426578	5.818048
5.216592	361.598110	5.823053
5.084986	354.247202	5.828058
5.158982	351.998979	5.833062
5.208531	348.723194	5.838067
5.173359	338.766204	5.843072
4.995202	337.955598	5.848077
5.134574	350.867157	5.853082
5.146047	344.895497	5.858086
4.745726	353.249933	5.863091
4.619308	350.947493	5.868096
4.636040	346.670760	5.873101
4.848827	351.164928	5.878106
5.295332	351.456109	5.883110
5.185750	352.548867	5.888115
5.337792	351.905145	5.893120
5.138900	357.640310	5.898125
4.954714	361.386380	5.903130
5.198826	364.939217	5.908134
5.371552	380.778361	5.913139
5.754488	376.438277	5.918144
5.779812	381.974027	5.923149
5.396759	373.358812	5.928154
5.122008	361.544050	5.933158
4.913469	358.289465	5.938163
5.471057	370.816388	5.943168
5.392861	372.774281	5.948173
5.431653	379.870806	5.953178
5.685404	381.071510	5.958182
5.342469	389.280988	5.963187
5.698113	377.175078	5.968192
5.388857	375.875525	5.973197
5.215696	375.570333	5.978202
5.745167	375.769503	5.983206
5.655390	381.389612	5.988211
5.895444	377.846883	5.993216
5.656712	376.912831	5.998221
5.180767	367.461044	6.003226
5.157352	369.771070	6.008230
5.449195	380.706903	6.013235
5.724609	379.721273	6.018240
5.378150	376.766565	6.023245
5.303048	382.605849	6.028250
5.225449	378.868971	6.033254
5.313160	380.044907	6.038259
5.648323	385.975337	6.043264
5.491285	382.133770	6.048269
5.189988	387.201527	6.053274
5.241021	382.457543	6.058278
5.394129	386.325106	6.063283
5.385421	382.789470	6.068288
5.303580	384.539127	6.073293
5.532087	377.306145	6.078298
5.508055	382.564846	6.083302
5.564225	387.472545	6.088307
5.600319	384.110265	6.093312
5.411001	390.407090	6.098317
5.266490	385.510056	6.103322
5.776016	383.390168	6.108326
5.465534	390.756210	6.113331
5.648257	386.602318	6.118336
5.732736	385.886858	6.123341
5.971410	388.747694	6.128346
5.973341	386.646726	6.133350
5.964841	381.624113	6.138355
5.600457	370.595246	6.143360
5.677393	361.395897	6.148365
5.360675	360.451842	6.153370
5.232571	363.879137	6.158374
5.302691	362.314876	6.163379
5.411454	375.595045	6.168384
5.762282	379.333747	6.173389
5.492361	381.213926	6.178394
5.891319	383.610049	6.183398
5.589583	374.343104	6.188403
5.417603	358.820294	6.193408
5.343212	363.666057	6.198413
5.390620	357.600214	6.203418
5.328870	366.518865	6.208422
5.496172	371.994542	6.213427
5.720289	382.969394	6.218432
5.592724	372.463631	6.223437
5.492471	367.967828	6.228442
5.493083	354.363831	6.233446
5.519132	364.021772	6.238451
5.458426	364.423560	6.243456
5.660390	361.639727	6.248461
5.040543	356.737616	6.253466
5.515913	364.863967	6.258470
5.610065	387.226262	6.263475
5.909192	385.094840	6.268480
5.698169	367.736822	6.273485
5.388924	365.130656	6.278490
5.294153	358.242241	6.283494
5.398820	367.074870	6.288499
5.369836	351.384272	6.293504
5.466878	357.895925	6.298509
5.451522	366.801024	6.303514
5.574804	375.254278	6.308518
5.311313	379.056991	6.313523
5.658745	377.376787	6.318528
5.652957	375.928746	6.323533
5.335085	361.437872	6.328538
5.836013	356.801015	6.333542
5.359722	361.753645	6.338547
5.175257	348.061411	6.343552
5.163554	363.799543	6.348557
5.369925	377.485289	6.353562
5.693273	377.691242	6.358566
5.693156	388.900324	6.363571
5.794558	385.619623	6.368576
5.545323	381.267235	6.373581
5.201251	369.466424	6.378586
5.673128	373.866475	6.383590
5.389231	391.054862	6.388595
5.694571	378.425280	6.393600
5.452085	366.573853	6.398605
5.734856	375.726765	6.403610
5.654269	369.611245	6.408614
5.227236	363.894512	6.413619
5.486843	355.096989	6.418624
5.363373	361.468972	6.423629
5.086617	372.948903	6.428634
5.891142	383.975756	6.433638
5.654261	388.979701	6.438643
5.651222	385.035063	6.443648
5.178967	376.987385	6.448653
5.432650	380.681102	6.453658
5.780289	379.870886	6.458662
5.361069	383.596607	6.463667
5.562941	385.067976	6.468672
5.569669	381.729251	6.473677
5.273732	385.075114	6.478682
5.552042	389.438870	6.483686
5.495643	389.583727	6.488691
5.884002	376.539429	6.493696
5.621238	366.247706	6.498701
5.843568	367.083146	6.503706
5.403877	364.399216	6.508710
5.166586	367.011456	6.513715
5.369838	364.436227	6.518720
5.273915	368.209684	6.523725
5.388358	379.343977	6.528730
5.692821	377.679954	6.533734
5.747076	389.418402	6.538739
5.521481	378.709601	6.543744
5.630062	359.571280	6.548749
5.193329	366.612126	6.553754
5.472858	361.038481	6.558758
5.627668	383.998759	6.563763
5.669183	370.650968	6.568768
5.522027	363.973184	6.573773
5.376080	365.163352	6.578778
5.579183	353.030590	6.583782
5.347810	362.447040	6.588787
5.135834	356.424746	6.593792
5.518160	370.016653	6.598797
5.457871	383.509807	6.603802
5.749604	379.883102	6.608806
5.478780	389.995398	6.613811
5.812092	384.843636	6.618816
5.449126	368.622900	6.623821
5.061636	366.740752	6.628826
5.528237	372.261576	6.633830
5.459931	376.293323	6.638835
5.681177	381.225937	6.643840
5.955624	381.961517	6.648845
5.236493	367.365436	6.653850
5.396663	369.321016	6.658854
5.600595	369.672110	6.663859
5.738157	366.278217	6.668864
5.498196	356.659982	6.673869
5.120387	363.697979	6.678874
5.345868	373.014831	6.683878
5.510950	391.288067	6.688883
5.563567	382.731563	6.693888
5.788392	377.508111	6.698893
5.464944	389.166163	6.703898
5.471484	374.634259	6.708902
5.320153	373.091822	6.713907
5.700680	378.069237	6.718912
5.751219	375.169775	6.723917
5.349778	363.264007	6.728922
5.735935	366.623888	6.733926
5.332852	366.572791	6.738931
5.227874	362.742104	6.743936
5.371354	368.297418	6.748941
5.345615	382.111054	6.753946
5.424759	385.423829	6.758950
5.499232	400.648710	6.763955
5.890439	382.124413	6.768960
5.915797	390.162656	6.773965
5.360447	385.465627	6.778970
5.345636	372.069659	6.783974
4.956122	373.591975	6.788979
5.405887	386.860187	6.793984
5.789885	388.325346	6.798989
5.576550	388.662315	6.803994
5.820868	394.803043	6.808998
5.587779	382.368020	6.814003
5.529192	369.532518	6.819008
5.656880	362.103271	6.824013
5.433691	362.438610	6.829018
5.468998	364.505378	6.834022
5.324021	366.540106	6.839027
5.445298	365.290578	6.844032
5.732002	370.864722	6.849037
5.761096	369.502998	6.854042
5.823836	362.128155	6.859046
5.368384	372.968367	6.864051
5.400305	359.096903	6.869056
5.332512	358.674067	6.874061
5.509797	364.752456	6.879066
5.645562	357.454829	6.884070
5.425373	362.500460	6.889075
5.584034	358.903969	6.894080
5.815930	362.249903	6.899085
5.605749	364.421331	6.904090
5.570127	354.935795	6.909094
5.597959	352.884581	6.914099
5.659169	361.211453	6.919104
5.692278	362.962193	6.924109
5.391945	359.886412	6.929114
5.072525	360.920095	6.934118
5.067629	353.188796	6.939123
5.578241	361.322314	6.944128
5.727246	357.325536	6.949133
4.991804	359.069387	6.954138
5.535439	359.864293	6.959142
5.400399	352.308279	6.964147
5.399849	360.097446	6.969152
5.737276	354.644500	6.974157
5.298499	361.701481	6.979162
5.449123	355.325344	6.984166
5.672232	358.887777	6.989171
5.447687	364.076454	6.994176
5.584464	357.753091	6.999181
5.089826	362.332096	7.004186
5.627516	372.875312	7.009190
5.435700	383.310656	7.014195
5.713169	371.359288	7.019200
5.403787	375.026778	7.024205
5.051064	377.100180	7.029210
5.530966	378.518769	7.034214
5.529789	380.705112	7.039219
5.409729	381.543244	7.044224
5.662726	384.468287	7.049229
5.335682	376.749171	7.054234
5.598164	379.558843	7.059238
5.537000	388.376174	7.064243
5.525903	385.334449	7.069248
5.783604	385.063412	7.074253
5.795179	382.957779	7.079258
6.084349	363.674279	7.084262
5.776358	365.629984	7.089267
5.657144	355.347554	7.094272
5.647151	361.239968	7.099277
5.220926	357.120783	7.104282
5.300069	361.078949	7.109286
5.592490	361.216952	7.114291
5.458565	364.714755	7.119296
5.146619	360.441737	7.124301
5.111264	369.277187	7.129306
5.603421	359.684165	7.134310
5.695320	359.340868	7.139315
5.407070	367.026137	7.144320
5.234972	362.237807	7.149325
5.251077	369.926310	7.154330
6.043597	371.539830	7.159334
5.858612	365.314017	7.164339
5.444359	361.246751	7.169344
5.640501	358.751722	7.174349
5.629532	356.311085	7.179354
5.603780	351.512627	7.184358
5.592172	357.205978	7.189363
5.799153	359.173251	7.194368
5.574524	360.242794	7.199373
5.798476	363.406470	7.204378
5.824691	359.874892	7.209382
5.461454	370.121786	7.214387
5.321763	367.369001	7.219392
5.620022	354.759520	7.224397
5.192511	357.499451	7.229402
5.578029	364.491366	7.234406
5.250807	362.916205	7.239411
5.237144	368.862976	7.244416
5.532630	359.227810	7.249421
5.348873	366.830372	7.254426
5.460485	354.487230	7.259430
5.263666	361.645742	7.264435
5.444731	357.808485	7.269440
5.568756	357.491823	7.274445
5.283933	355.321612	7.279450
5.750046	361.392994	7.284454
5.373679	366.402833	7.289459
5.553407	355.811270	7.294464
5.781782	352.912596	7.299469
5.765451	360.125261	7.304474
5.654731	354.495322	7.309478
5.241016	359.425553	7.314483
4.918451	350.892678	7.319488
4.971565	354.200009	7.324493
4.859541	370.247991	7.329498
5.181393	371.302051	7.334502
5.627729	380.929365	7.339507
5.600089	383.334961	7.344512
5.268361	383.699855	7.349517
5.423487	379.673645	7.354522
5.652002	385.709264	7.359526
5.755323	380.735680	7.364531
5.593338	384.645974	7.369536
5.828434	388.019888	7.374541
5.749590	385.273445	7.379546
5.450710	372.649358	7.384550
5.509356	371.963230	7.389555
5.410881	379.767652	7.394560
5.438247	366.864987	7.399565
5.654749	379.571571	7.404570
5.896668	372.725639	7.409574
5.431124	363.683517	7.414579
5.321849	365.877199	7.419584
5.631167	353.218542	7.424589
5.455456	364.012029	7.429594
5.540327	359.727848	7.434598
5.414059	364.195716	7.439603
5.428332	364.408663	7.444608
5.620295	358.057726	7.449613
5.563699	356.453085	7.454618
5.387026	352.459559	7.459622
5.677274	355.014972	7.464627
5.305885	354.354672	7.469632
5.645215	358.376729	7.474637
5.452421	360.485339	7.479642
5.369605	350.042223	7.484646
5.380649	358.854624	7.489651
5.325270	361.672655	7.494656
5.902433	369.118781	7.499661
5.639813	363.895297	7.504666
5.769218	360.531148	7.509670
5.701294	361.013153	7.514675
5.619683	355.445119	7.519680
5.836254	353.873875	7.524685
5.852852	356.506695	7.529690
5.733293	356.984085	7.534694
5.632915	355.525463	7.539699
5.181179	352.077794	7.544704
5.705152	344.416014	7.549709
5.544958	357.386873	7.554714
5.459734	349.617464	7.559718
5.417314	356.084392	7.564723
5.454660	362.216205	7.569728
5.472278	352.311099	7.574733
5.255073	360.602226	7.579738
5.304544	357.911738	7.584742
5.343046	349.945897	7.589747
4.884298	352.810911	7.594752
5.763883	351.484447	7.599757
5.455107	361.011022	7.604762
5.403298	362.044167	7.609766
5.629115	349.265638	7.614771
5.712428	357.095529	7.619776
5.915172	349.110444	7.624781
5.280949	362.031727	7.629786
5.779706	359.593984	7.634790
5.442496	354.638377	7.639795
5.644291	356.907009	7.644800
5.804895	350.067419	7.649805
5.674578	358.563314	7.654810
5.669222	354.324819	7.659814
5.698781	356.104583	7.664819
5.477663	353.794742	7.669824
5.660645	357.907580	7.674829
5.646512	359.653020	7.679834
5.547327	351.521957	7.684838
5.644476	343.249600	7.689843
5.010512	353.086226	7.694848
5.646907	356.695041	7.699853
5.171670	363.397037	7.704858
5.245356	358.984885	7.709862
5.189735	359.714907	7.714867
5.041128	355.511370	7.719872
5.405458	352.170756	7.724877
4.900221	355.881391	7.729882
4.724587	357.095163	7.734886
5.082816	369.814475	7.739891
5.407285	376.347671	7.744896
5.619766	380.383157	7.749901
5.469082	382.260589	7.754906
5.828709	387.257080	7.759910
5.632481	384.876921	7.764915
5.591129	390.707789	7.769920
6.011999	386.349141	7.774925
5.667441	374.020063	7.779930
5.317922	365.187663	7.784934
5.420798	354.674504	7.789939
5.324718	354.689500	7.794944
5.890085	362.159606	7.799949
5.572052	364.702161	7.804954
5.772881	356.473765	7.809958
5.969196	358.132656	7.814963
5.571376	359.982126	7.819968
5.847343	355.747285	7.824973
5.588494	357.122708	7.829978
5.817741	354.195425	7.834982
5.992277	356.560049	7.839987
5.754747	355.363223	7.844992
5.658322	333.785995	7.849997
5.412475	346.010893	7.855002
5.145365	333.913390	7.860006
5.270570	350.304063	7.865011
5.266721	358.906815	7.870016
5.750028	351.159616	7.875021
5.741941	361.594814	7.880026
5.482400	362.426188	7.885030
5.273947	361.142578	7.890035
5.280638	366.020010	7.895040
5.564626	354.099277	7.900045
5.395340	354.185781	7.905050
5.388753	350.267013	7.910054
5.717092	358.916119	7.915059
5.380011	357.345658	7.920064
5.695622	354.813046	7.925069
5.493309	361.175159	7.930074
5.483220	358.259829	7.935078
5.532392	355.952196	7.940083
5.399895	355.738748	7.945088
5.989136	356.384186	7.950093
5.500090	356.849501	7.955098
5.420589	356.488599	7.960102
5.642382	358.611751	7.965107
6.032868	357.171615	7.970112
5.792129	340.966675	7.975117
5.401703	336.813447	7.980122
5.372547	336.534647	7.985139
5.260585	333.544799	7.990157
4.926380	339.703018	7.995174
5.284425	351.787031	8.000192
5.150645	352.041414	8.005210
5.497419	356.960740	8.010227
5.604127	360.727771	8.015245
5.478214	357.856850	8.020262
5.775320	353.332782	8.025280
5.475823	361.028710	8.030298
5.467715	362.118704	8.035315
5.494395	360.741886	8.040333
5.795658	361.581751	8.045350
5.888713	353.760257	8.050368
5.935595	362.415215	8.055386
5.443857	364.776495	8.060403
5.659245	364.257029	8.065421
5.557728	363.029551	8.070438
5.644892	353.738448	8.075456
5.492926	361.726970	8.080474
5.580444	364.764881	8.085491
5.879883	351.941128	8.090509
5.595894	367.517421	8.095526
5.988868	366.165618	8.100544
5.647736	352.195123	8.105562
5.639069	341.154947	8.110579
5.590552	346.770099	8.115597
5.252115	339.378691	8.120614
5.813061	358.559692	8.125632
5.458828	362.243863	8.130650
5.631893	367.723541	8.135667
5.735732	363.766020	8.140685
5.164995	370.465979	8.145702
5.461380	362.253081	8.150720
5.767833	360.406692	8.155738
5.595841	361.001522	8.160755
5.653526	360.872664	8.165773
5.476897	357.277532	8.170790
5.802347	353.127727	8.175808
5.655194	361.746627	8.180826
5.304994	364.205784	8.185843
5.571032	358.130824	8.190861
5.416474	367.240002	8.195878
5.462314	362.164950	8.200896
5.517392	364.898659	8.205914
5.448152	361.949490	8.210931
5.791074	367.308052	8.215949
5.530617	385.187468	8.220966
6.053408	387.072072	8.225984
5.823403	384.438248	8.231002
5.693592	374.616058	8.236019
6.138749	370.842066	8.241037
5.891752	369.921246	8.246054
5.989944	354.175148	8.251072
5.533092	354.725972	8.256090
5.765680	353.787284	8.261107
5.676636	362.236199	8.266125
5.650293	364.963652	8.271142
6.070348	360.527732	8.276160
6.049193	361.427263	8.281178
5.806413	367.886821	8.286195
6.057115	354.016672	8.291213
5.555374	356.079723	8.296230
5.900164	352.147802	8.301248
5.876602	354.868509	8.306266
5.638521	364.113760	8.311283
5.878119	361.977994	8.316301
5.759050	352.684290	8.321318
5.906347	350.073773	8.326336
5.684181	354.630425	8.331354
5.769141	356.160340	8.336371
5.647438	359.186647	8.341389
6.033042	377.063289	8.346406
6.104706	376.332683	8.351424
6.156638	371.682690	8.356442
5.569121	366.845096	8.361459
5.571935	358.703153	8.366477
6.183502	371.104293	8.371494
5.915841	375.608077	8.376512
6.148816	371.545246	8.381530
5.594079	378.728685	8.386547
6.117663	362.998394	8.391565
6.111580	368.802594	8.396582
6.107964	360.481780	8.401600
6.137540	358.441827	8.406618
5.945259	364.350752	8.411635
5.885075	362.523579	8.416653
5.635654	358.756753	8.421670
6.059547	357.759879	8.426688
5.964207	357.427641	8.431706
5.768307	367.155449	8.436723
6.157429	360.471220	8.441741
5.770651	367.268762	8.446758
6.095661	374.899018	8.451776
6.038266	366.425637	8.456794
5.822723	367.992873	8.461811
6.188979	370.069097	8.466829
6.097346	367.880766	8.471846
6.059398	366.889530	8.476864
5.677250	360.151825	8.481882
5.725429	377.538235	8.486899
5.959761	378.028779	8.491917
6.023500	378.829891	8.496934
6.086554	386.983752	8.501952
6.398617	385.246934	8.506970
6.225115	387.792186	8.511987
6.132452	380.182624	8.517005
6.237247	383.716440	8.522022
6.157348	361.904523	8.527040
6.074283	353.693907	8.532058
6.069306	355.790060	8.537075
6.027998	350.832716	8.542093
5.687446	358.143736	8.547110
6.096026	370.674305	8.552128
6.067160	377.163673	8.557146
5.878303	379.215879	8.562163
5.983578	372.386502	8.567181
6.207819	382.373935	8.572199
6.600578	384.660617	8.577216
6.416998	376.370971	8.582234
6.171442	375.560373	8.587251
5.922112	358.574568	8.592269
6.446537	367.237222	8.597287
6.232207	364.029791	8.602304
6.188521	357.201522	8.607322
5.879011	361.200605	8.612339
6.267570	368.038366	8.617357
5.941102	373.040429	8.622375
6.296575	385.569810	8.627392
6.248588	384.993525	8.632410
6.068648	393.147354	8.637427
6.281379	382.344068	8.642445
6.040188	390.753572	8.647463
6.100099	384.464556	8.652480
6.178480	386.115412	8.657498
6.258513	389.163960	8.662515
6.581866	394.979990	8.667533
6.445575	392.773364	8.672551
6.745798	382.234151	8.677568
6.160436	364.748422	8.682586
5.704494	362.623125	8.687603
6.269332	381.500603	8.692621
6.569749	393.012979	8.697639
6.118939	376.774856	8.702656
6.263776	373.527280	8.707674
5.752310	374.525241	8.712691
6.319326	378.788622	8.717709
6.203929	384.161747	8.722727
6.195586	388.076077	8.727744
6.568339	387.203923	8.732762
6.070054	386.413740	8.737779
6.194063	383.791066	8.742797
6.341972	377.605110	8.747815
6.252443	378.688848	8.752832
6.574771	379.288761	8.757850
6.389267	381.687566	8.762867
6.683118	364.869634	8.767885
6.345911	378.311545	8.772903
6.391507	380.134754	8.777920
6.718708	380.393100	8.782938
6.605043	377.387732	8.787955
6.136497	362.427262	8.792973
6.195310	370.300924	8.797991
6.323301	379.590167	8.803008
6.058437	380.208925	8.808026
6.331311	385.467951	8.813043
6.426357	383.922704	8.818061
6.342545	383.402488	8.823079
6.361245	388.795759	8.828096
6.441427	378.082536	8.833114
5.660576	393.177663	8.838131
6.423375	391.203418	8.843149
6.420609	389.518773	8.848167
6.494435	386.174959	8.853184
6.643796	386.918562	8.858202
6.204582	380.612590	8.863219
6.570537	378.163675	8.868237
6.659915	382.611870	8.873255
6.236561	389.894772	8.878272
6.627745	384.860613	8.883290
6.157306	378.815111	8.888307
6.382114	382.323929	8.893325
6.184053	384.191386	8.898343
6.028369	392.347750	8.903360
6.403009	407.149379	8.908378
6.398852	409.314836	8.913395
6.776855	407.561438	8.918413
6.586482	411.576695	8.923431
6.657642	412.067400	8.928448
6.899338	407.021798	8.933466
6.732280	405.867635	8.938483
6.550747	391.774434	8.943501
6.508634	381.588309	8.948519
6.422282	388.070853	8.953536
6.193098	394.266386	8.958554
6.599537	403.174634	8.963571
6.705018	417.945600	8.968589
6.493396	418.937903	8.973607
6.694271	419.234851	8.978624
6.978987	410.215903	8.983642
6.205833	407.136494	8.988659
6.586364	415.499701	8.993677
6.595383	411.402306	8.998695
6.677134	422.768874	9.003712
6.613357	420.219612	9.008730
6.838880	417.600061	9.013747
6.372755	411.900997	9.018765
6.849444	413.025960	9.023783
6.671484	421.280474	9.028800
6.676498	416.003490	9.033818
6.514875	424.709875	9.038835
6.710146	417.623483	9.043853
6.611142	419.276715	9.048871
6.371650	423.861328	9.053888
6.729211	413.837007	9.058906
6.355675	426.205380	9.063923
6.665782	424.961144	9.068941
6.542586	419.858747	9.073959
6.228618	423.795425	9.078976
6.381248	415.223052	9.083994
6.698683	425.823973	9.089011
6.443705	421.843415	9.094029
6.862568	422.573459	9.099047
6.398289	426.432560	9.104064
6.815618	435.787231	9.109082
7.007579	444.511154	9.114099
6.855450	439.145026	9.119117
6.757747	429.645993	9.124135
6.561913	426.416737	9.129152
6.888993	443.374798	9.134170
7.229663	434.009471	9.139187
6.913394	417.968103	9.144205
6.530303	412.685278	9.149223
6.593700	422.505282	9.154240
6.722381	427.849884	9.159258
7.141365	437.529331	9.164275
6.996993	432.461784	9.169293
6.854845	417.179063	9.174311
6.951309	418.353760	9.179328
6.609785	409.867794	9.184346
7.059833	417.686874	9.189363
6.664215	420.787395	9.194381
6.958872	411.119991	9.199399
6.664536	425.587159	9.204416
6.966529	425.398172	9.209434
7.544414	431.013646	9.214451
7.180557	409.914879	9.219469
6.851258	413.522599	9.224487
6.408515	417.908494	9.229504
6.933327	409.770456	9.234522
7.047262	404.429182	9.239539
6.747375	410.761954	9.244557
6.887064	416.104840	9.249575
6.580144	419.620718	9.254592
6.837700	421.537156	9.259610
7.090618	433.157933	9.264627
7.146933	436.412144	9.269645
7.023764	430.186329	9.274663
6.542588	433.218126	9.279680
6.914105	427.767316	9.284698
6.950158	439.058963	9.289715
6.681908	425.932244	9.294733
6.717344	436.962067	9.299751
6.487991	441.144337	9.304768
6.847672	435.856306	9.309786
6.688150	437.582075	9.314803
7.184197	439.104794	9.319821
7.219745	427.685314	9.324839
6.972508	444.978936	9.329856
6.823331	427.084423	9.334874
6.871648	432.441539	9.339891
6.870100	447.342797	9.344909
7.185417	451.493913	9.349927
6.962617	459.452483	9.354944
7.102873	456.180360	9.359962
7.568851	465.054124	9.364979
7.262950	462.899143	9.369997
7.103806	445.274393	9.375015
6.883240	439.789539	9.380032
7.115222	446.478149	9.385050
7.256962	442.587289	9.390067
7.175662	447.942502	9.395085
6.931984	437.816128	9.400103
6.934008	446.427620	9.405120
7.193021	451.414283	9.410138
7.367520	453.817004	9.415155
7.194686	448.611879	9.420173
7.174339	443.834273	9.425191
7.227317	442.434419	9.430208
7.094077	444.597889	9.435226
6.727156	443.733604	9.440243
7.033790	461.404887	9.445261
7.207988	472.100717	9.450279
7.282571	466.816042	9.455296
7.233103	460.225308	9.460314
7.434012	469.862990	9.465331
7.414006	468.461875	9.470349
7.310046	460.364911	9.475367
7.233988	461.433934	9.480384
7.513962	454.419542	9.485402
7.045073	442.277057	9.490419
7.039706	447.718272	9.495437
7.491570	457.250605	9.500455
7.512052	460.362083	9.505472
6.908484	445.302651	9.510490
7.257832	448.927785	9.515507
6.959694	472.707914	9.520525
7.302345	468.997197	9.525543
7.424446	466.557835	9.530560
7.684473	463.106125	9.535578
7.445481	460.492623	9.540595
7.135029	465.514307	9.545613
7.192750	466.597214	9.550631
7.263866	472.947980	9.555648
7.195147	459.979508	9.560666
7.161834	463.181409	9.565683
7.250453	466.156054	9.570701
7.295829	470.557476	9.575719
7.131849	466.237707	9.580736
6.998766	464.668015	9.585754
7.109971	462.861482	9.590771
7.057475	462.541505	9.595789
7.224360	455.806639	9.600807
7.438348	465.786248	9.605824
7.493450	474.029745	9.610842
7.928110	475.442110	9.615859
7.478683	482.079044	9.620877
7.608882	472.847447	9.625895
7.745487	465.978443	9.630912
7.934113	470.474321	9.635930
7.678790	462.265230	9.640947
7.820769	464.524699	9.645965
7.720017	464.969592	9.650983
7.778275	469.466834	9.656000
7.443753	463.002528	9.661018
7.545138	461.390019	9.666035
7.375354	471.028615	9.671053
7.606360	467.915922	9.676071
7.723509	468.756057	9.681088
7.434680	466.008309	9.686106
7.197787	469.027324	9.691123
7.118221	473.691186	9.696141
7.353272	475.951944	9.701159
7.412801	469.786028	9.706176
7.162069	463.936651	9.711194
7.446875	461.579251	9.716211
7.243460	470.945386	9.721229
7.237642	465.319796	9.726247
7.526044	470.516473	9.731264
7.335272	463.786799	9.736282
7.594527	477.694469	9.741299
7.469246	494.072944	9.746317
7.691589	492.043986	9.751335
7.757212	489.717552	9.756352
7.670942	493.685063	9.761370
8.010872	489.435147	9.766387
7.847605	480.268172	9.771405
7.537706	480.764563	9.776423
7.878506	477.123557	9.781440
7.605899	472.921680	9.786458
7.870685	474.272135	9.791475
7.737402	478.871782	9.796493
7.645867	471.568104	9.801511
7.966152	477.542421	9.806528
7.603969	469.977940	9.811546
7.819027	473.756525	9.816563
7.496917	476.662583	9.821581
7.532685	469.717763	9.826599
7.697964	463.204041	9.831616
8.013972	477.304836	9.836634
7.709388	467.598163	9.841651
7.969981	469.640359	9.846669
7.799716	476.180180	9.851687
7.839368	466.170615	9.856704
7.808383	467.279956	9.861722
7.704174	460.748235	9.866739
7.536666	459.638317	9.871757
7.599010	463.869847	9.876775
8.042171	465.378712	9.881792
7.669646	472.940899	9.886810
7.813400	460.535764	9.891827
7.647775	463.780356	9.896845
7.578312	463.627114	9.901863
7.851538	473.102067	9.906880
8.136165	485.636237	9.911898
8.001098	477.559887	9.916915
7.715673	481.681473	9.921933
8.035162	477.920714	9.926951
7.929553	467.349968	9.931968
7.951833	465.582525	9.936986
7.828554	460.858808	9.942003
8.043224	475.032181	9.947021
7.882245	461.929757	9.952039
7.891417	455.604436	9.957056
7.319317	460.957177	9.962074
7.705915	473.219855	9.967091
8.098554	480.240053	9.972109
7.861081	486.127653	9.977127
8.053253	485.028002	9.982144
8.224330	490.214551	9.987162
7.789889	489.316597	9.992179
7.961003	492.291024	9.997197
7.777687	490.738618	10.002215
7.806366	487.714224	10.007232
7.878064	495.680605	10.012250
8.099339	489.590480	10.017267
8.104316	494.859693	10.022285
7.796203	497.981316	10.027303
7.933789	488.508731	10.032320
8.091034	495.284731	10.037338
8.086537	493.215356	10.042355
8.187188	483.881061	10.047373
7.994233	495.621791	10.052391
8.306473	498.665761	10.057408
8.125138	495.715088	10.062426
8.450155	496.286186	10.067443
8.325366	491.591097	10.072461
8.315214	485.442336	10.077479
8.546708	478.151473	10.082496
8.019705	481.357664	10.087514
8.015625	470.547057	10.092531
7.995046	467.299973	10.097549
7.972511	480.790794	10.102567
8.321415	484.024703	10.107584
8.153273	491.233198	10.112602
8.191256	484.562570	10.117619
8.034813	489.102712	10.122637
8.037986	494.346961	10.127655
8.347395	490.016594	10.132672
7.879256	501.803329	10.137690
8.061977	495.668714	10.142707
7.955111	489.108996	10.147725
7.733279	496.625640	10.152743
8.061580	481.866036	10.157760
8.336186	492.214901	10.162778
8.348444	486.769518	10.167795
8.123866	486.100810	10.172813
8.198714	486.698235	10.177831
8.177171	480.036877	10.182848
8.000019	498.427275	10.187866
8.016148	494.215150	10.192883
8.493610	490.811628	10.197901
8.294922	495.424618	10.202919
8.265159	488.534173	10.207936
8.200679	491.236027	10.212954
8.360385	491.596189	10.217971
8.493347	487.952827	10.222989
8.421636	486.951063	10.228007
8.395334	483.610198	10.233024
8.076524	497.226051	10.238042
8.306216	490.544507	10.243059
8.214664	491.824217	10.248077
7.951312	490.483079	10.253095
8.395698	502.793581	10.258112
8.714211	510.175611	10.263130
8.218079	506.778510	10.268147
8.598929	507.886845	10.273165
8.474510	505.656267	10.278183
8.414623	509.004319	10.283200
8.550200	501.412814	10.288218
8.372936	491.815688	10.293235
8.355237	493.708720	10.298253
8.314707	507.069824	10.303271
8.507615	514.758577	10.308288
8.575235	523.400917	10.313306
8.234921	514.624392	10.318323
8.182502	510.303021	10.323341
8.527597	517.737717	10.328359
9.102256	513.141994	10.333376
8.576767	509.471765	10.338394
8.289552	503.706947	10.343411
8.798439	501.784846	10.348429
8.867667	512.339261	10.353447
8.358266	501.496864	10.358464
8.368602	502.246339	10.363482
8.688612	508.132352	10.368499
8.416403	501.421655	10.373517
8.292660	512.798186	10.378535
8.689330	507.059426	10.383552
8.784278	523.450974	10.388570
8.463265	511.335908	10.393587
8.576505	503.110437	10.398605
8.418397	513.545621	10.403623
8.518841	512.106815	10.408640
8.435566	523.120462	10.413658
8.889008	522.450324	10.418675
8.665466	513.936472	10.423693
8.863646	514.713503	10.428711
8.907494	518.326259	10.433728
8.745947	512.557651	10.438746
8.376376	505.660149	10.443763
8.437206	511.425577	10.448781
8.672973	513.752497	10.453799
8.829123	513.958586	10.458816
8.830342	525.034815	10.463834
8.497980	529.419328	10.468851
8.760114	514.064112	10.473869
8.650853	511.436715	10.478887
8.809709	514.993696	10.483904
8.473708	518.962226	10.488922
8.334555	515.424340	10.493939
8.564781	524.773478	10.498957
8.620134	514.351205	10.503975
8.755952	517.605674	10.508992
8.792626	512.910685	10.514010
8.531444	518.767276	10.519027
8.853229	521.102894	10.524045
8.693280	517.268458	10.529063
8.653656	518.344434	10.534080
8.778946	525.986918	10.539098
8.625426	524.893752	10.544115
8.816364	522.203835	10.549133
8.908405	523.464430	10.554151
8.721322	526.024439	10.559168
8.770825	538.629968	10.564186
8.953664	544.442679	10.569203
9.016803	539.607869	10.574221
8.880819	549.392717	10.579239
9.004395	541.654748	10.584256
9.134975	540.640419	10.589274
8.852110	530.447513	10.594291
8.803658	521.398335	10.599309
8.635928	528.849767	10.604327
8.609045	543.556243	10.609344
8.958365	542.968584	10.614362
9.008933	540.193227	10.619379
9.357016	540.798604	10.624397
9.023781	545.858570	10.629415
8.958554	545.780404	10.634432
9.514377	539.537193	10.639450
8.481002	545.450906	10.644467
9.338470	539.242777	10.649485
9.287628	542.450577	10.654503
8.727693	527.740872	10.659520
9.176606	529.930472	10.664538
8.869624	544.891989	10.669555
9.007756	533.260818	10.674573
9.107259	541.825623	10.679591
8.819104	543.710279	10.684608
8.929586	541.856516	10.689626
8.903613	552.391064	10.694643
9.009908	546.088458	10.699661
8.787770	549.300840	10.704679
8.849494	541.310581	10.709696
8.850843	546.782337	10.714714
9.001386	545.165323	10.719731
9.206036	537.919639	10.724749
9.055797	539.669218	10.729767
8.730294	541.449241	10.734784
9.240597	551.442721	10.739802
9.158715	550.051234	10.744819
9.249010	559.933395	10.749837
9.195255	558.711090	10.754855
8.962636	561.726299	10.759872
9.612077	558.456926	10.764890
9.196698	563.453951	10.769907
9.176599	551.553927	10.774925
8.703193	551.858036	10.779943
8.829645	571.065892	10.784960
9.494089	563.221612	10.789978
9.683953	562.040268	10.794995
9.671469	574.661784	10.800013
9.673286	562.101961	10.805031
8.981173	550.581111	10.810048
9.496741	559.876373	10.815066
9.358639	559.364604	10.820083
9.027505	544.193246	10.825101
8.912585	553.526711	10.830119
9.252995	562.426387	10.835136
9.453285	568.602447	10.840154
9.330837	567.128915	10.845171
9.535811	567.784975	10.850189
9.465438	559.405037	10.855207
9.344098	563.838752	10.860224
9.445781	557.997587	10.865242
9.289876	566.163531	10.870259
9.316401	570.653117	10.875277
9.821764	570.867948	10.880295
9.636991	574.576269	10.885312
9.523075	577.412060	10.890330
9.296262	569.668675	10.895347
9.381041	574.767704	10.900365
9.771961	572.624131	10.905383
9.210834	573.544632	10.910400
9.167850	568.092047	10.915418
9.147272	570.828101	10.920435
9.105444	574.817110	10.925453
9.234935	570.208637	10.930471
9.463193	567.254137	10.935488
9.439544	566.301688	10.940506
9.323038	574.316340	10.945523
9.493197	563.175604	10.950541
9.735558	566.637547	10.955559
9.717693	569.291131	10.960576
9.683397	565.481300	10.965594
9.612261	566.748370	10.970611
9.536240	569.237447	10.975629
9.539930	558.274105	10.980647
9.721457	560.300220	10.985664
9.747075	570.665808	10.990682
9.457354	570.764600	10.995699
9.491526	561.885566	11.000717
9.879510	567.751548	11.005735
9.331674	569.017103	11.010752
9.641210	558.665677	11.015770
9.638982	567.019125	11.020787
9.294837	571.029958	11.025805
9.741431	569.742372	11.030823
9.769835	582.013559	11.035840
9.944882	593.368866	11.040858
10.033858	578.962012	11.045875
9.541759	568.347245	11.050893
9.649945	573.865489	11.055911
9.652625	576.462228	11.060928
9.794752	571.375280	11.065946
9.568086	576.159897	11.070963
9.758289	575.795819	11.075981
10.172710	587.135942	11.080999
10.044014	577.641656	11.086016
10.253469	564.847539	11.091034
9.733452	565.613321	11.096051
9.587023	572.992031	11.101069
9.933098	569.709932	11.106087
10.003180	567.016735	11.111104
9.972382	562.196545	11.116122
9.938068	568.895105	11.121139
9.755964	577.737292	11.126157
10.049013	571.295152	11.131175
10.055877	566.166152	11.136192
9.969126	564.254735	11.141210
10.032863	567.413144	11.146227
9.744093	573.517034	11.151245
9.850472	566.191970	11.156263
9.722110	576.120807	11.161280
10.015123	568.681479	11.166298
10.144093	561.911453	11.171315
9.860787	564.353911	11.176333
10.149008	564.577305	11.181351
10.225729	574.038727	11.186368
9.816857	568.586308	11.191386
9.973145	573.645801	11.196403
9.786791	573.678009	11.201421
10.162463	565.698815	11.206439
9.819500	578.886164	11.211456
10.194292	571.812784	11.216474
10.327116	568.876299	11.221491
10.073111	568.496179	11.226509
10.377525	572.453369	11.231527
10.225863	573.625685	11.236544
10.202216	570.319102	11.241562
10.336709	568.531022	11.246579
10.347883	572.521246	11.251597
10.421450	564.781586	11.256615
10.071214	573.066149	11.261632
10.106342	568.257782	11.266650
9.944263	563.123530	11.271667
10.113344	566.962941	11.276685
10.060347	571.916169	11.281703
9.831709	575.088544	11.286720
9.831101	576.354101	11.291738
9.894479	568.048005	11.296755
9.994741	575.094828	11.301773
10.015289	561.190928	11.306791
10.039539	569.590745	11.311808
10.021222	569.514742	11.316826
9.994063	580.068426	11.321843
9.679603	590.748895	11.326861
10.186898	589.451857	11.331879
10.067566	596.065839	11.336896
10.372835	590.404397	11.341914
10.375190	590.874263	11.346931
10.261597	591.567301	11.351949
10.627802	585.426177	11.356967
10.544920	584.965768	11.361984
10.818888	593.178398	11.367002
10.572846	599.313513	11.372019
10.547011	590.336514	11.377037
10.582701	579.702679	11.382055
10.148966	575.245010	11.387072
10.414610	581.726466	11.392090
10.460515	580.583313	11.397107
10.134624	578.431429	11.402125
10.378855	584.780527	11.407143
10.326971	596.698167	11.412160
10.538049	591.559454	11.417178
10.506660	600.744245	11.422195
10.334307	597.135775	11.427213
10.936370	586.259125	11.432231
10.673598	586.956456	11.437248
10.164696	575.107275	11.442266
10.155213	583.222028	11.447283
9.991475	595.299088	11.452301
10.060783	598.213647	11.457319
9.941243	606.099404	11.462336
10.045338	593.084994	11.467354
10.536619	595.179647	11.472371
10.161947	600.186122	11.477389
10.621621	606.081979	11.482407
10.348621	614.411337	11.487424
10.637516	613.501738	11.492442
10.620677	616.880976	11.497459
10.529085	612.682439	11.502477
10.826352	621.102886	11.507495
10.498739	618.121321	11.512512
10.425852	612.203182	11.517530
10.754612	604.868723	11.522547
10.526031	622.030229	11.527565
10.526655	613.352045	11.532583
10.657381	625.083487	11.537600
10.624392	617.164743	11.542618
11.022703	608.579271	11.547635
11.022865	619.204460	11.552653
11.317864	615.491665	11.557671
10.899847	609.516813	11.562688
10.907377	601.986227	11.567706
10.842956	595.593423	11.572723
10.762661	608.124540	11.577741
10.919671	602.552446	11.582759
10.414529	592.586609	11.587776
10.722875	604.066330	11.592794
11.035003	604.778289	11.597811
10.914422	605.554463	11.602829
10.739091	598.071283	11.607847
10.746451	593.873123	11.612864
10.547065	602.014296	11.617882
10.874353	592.496342	11.622899
10.736780	607.381044	11.627917
10.892717	608.442357	11.632935
10.940445	614.979844	11.637952
10.329156	613.847497	11.642970
10.636633	609.754078	11.647987
10.670503	619.215885	11.653005
10.795729	615.232889	11.658023
10.924625	617.803672	11.663040
10.884676	622.521362	11.668058
10.786586	612.296485	11.673075
10.574943	619.732703	11.678093
10.389828	620.705111	11.683111
10.774417	624.387908	11.688128
10.603195	642.667082	11.693146
11.007374	643.718147	11.698163
11.065738	644.800965	11.703181
10.886495	641.079954	11.708199
11.166525	644.009048	11.713216
10.838376	640.816132	11.718234
11.270899	644.592452	11.723251
11.287827	646.906127	11.728269
11.266248	646.941081	11.733287
11.285086	650.564070	11.738304
11.114661	652.073815	11.743322
11.403078	646.351865	11.748339
11.220251	625.221501	11.753357
11.077368	626.360896	11.758375
10.905767	612.057700	11.763392
10.901013	634.438578	11.768410
11.199015	637.970764	11.773427
11.038858	641.173512	11.778445
11.048547	646.849120	11.783463
11.515842	644.987127	11.788480
11.357071	647.340781	11.793498
11.293972	641.509467	11.798515
11.040616	638.973911	11.803533
11.273700	650.093009	11.808551
11.373927	647.167898	11.813568
11.363627	648.368700	11.818586
11.161360	640.684576	11.823603
11.079708	646.740465	11.828621
11.495746	642.027401	11.833639
11.618711	641.711658	11.838656
11.092261	645.933922	11.843674
11.335742	654.211286	11.848691
11.439616	647.839596	11.853709
11.297992	634.491043	11.858727
11.261360	648.176681	11.863744
11.157598	648.868191	11.868762
11.342822	651.414430	11.873779
11.254199	644.053425	11.878797
11.005816	652.732406	11.883815
11.313773	648.749353	11.888832
11.260734	640.322498	11.893850
11.347821	639.740953	11.898867
11.343430	649.426475	11.903885
11.158456	652.465838	11.908903
11.105415	642.546343	11.913920
11.405790	645.822550	11.918938
11.645138	643.986580	11.923955
11.885139	644.908579	11.928973
11.470616	644.550294	11.933991
11.503711	637.612137	11.939008
11.226826	643.023105	11.944026
11.447963	644.269920	11.949043
11.743554	658.396128	11.954061
11.535791	648.879401	11.959079
11.775683	653.010751	11.964096
11.338242	648.907077	11.969114
11.299971	649.200241	11.974131
11.932710	661.825498	11.979149
11.885263	657.175125	11.984167
11.788666	648.878120	11.989184
11.243725	650.114829	11.994202
11.557700	654.827914	11.999219
11.800082	665.734143	12.004237
11.827386	670.589692	12.009255
11.856260	664.826099	12.014272
11.472259	674.166810	12.019290
12.146357	673.534892	12.024307
11.203572	661.308256	12.029325
11.422349	664.496189	12.034343
11.654498	666.375585	12.039360
11.747477	671.747910	12.044378
11.613409	670.430808	12.049395
11.713737	682.476279	12.054413
11.845539	680.089025	12.059431
12.242513	664.778955	12.064448
11.457983	686.331444	12.069466
11.529888	682.344112	12.074483
11.469441	677.834609	12.079501
11.482531	677.564374	12.084519
11.692382	672.103948	12.089536
11.585161	680.353880	12.094554
11.774886	676.461810	12.099571
11.589600	680.978090	12.104589
11.838161	698.548201	12.109607
11.847950	689.278438	12.114624
11.822528	697.212694	12.119642
11.849487	695.280404	12.124659
11.936669	696.216732	12.129677
11.726116	696.341067	12.134695
12.065683	691.333793	12.139712
11.821617	695.650953	12.144730
11.743601	698.708383	12.149747
12.263993	693.455212	12.154765
11.926258	698.743132	12.159783
12.199115	699.350760	12.164800
11.961715	708.501412	12.169818
11.912655	696.391213	12.174835
12.093067	701.506945	12.179853
12.043007	704.648383	12.184871
12.319606	686.873502	12.189888
12.165709	699.353028	12.194906
12.010304	692.194899	12.199923
12.120386	696.488476	12.204941
12.033408	698.660551	12.209959
12.239936	700.061119	12.214976
12.501563	707.101805	12.219994
12.480401	702.242208	12.225011
12.136773	697.088848	12.230029
12.053273	698.932189	12.235047
12.093264	698.503137	12.240064
12.272628	696.099009	12.245082
12.185304	694.689423	12.250099
12.118463	691.853431	12.255117
12.052358	692.460186	12.260135
12.059054	688.950049	12.265152
12.328822	689.539223	12.270170
12.170121	696.023676	12.275187
12.247601	695.421535	12.280205
11.931679	698.118389	12.285223
12.322908	692.374106	12.290240
12.482152	699.222454	12.295258
12.610145	690.562269	12.300275
12.404576	695.678137	12.305293
12.075748	698.111922	12.310311
12.375327	691.226924	12.315328
12.134620	701.861264	12.320346
12.278428	714.786738	12.325363
12.715180	715.457208	12.330381
12.294396	723.557171	12.335399
12.532666	713.194662	12.340416
12.686271	722.344401	12.345434
12.524319	707.761924	12.350451
12.561852	695.792872	12.355469
12.129398	694.108830	12.360487
12.372703	711.717641	12.365504
12.622759	711.978537	12.370522
12.175247	714.336131	12.375539
12.556648	719.486845	12.380557
12.397689	722.427498	12.385575
12.984347	723.352330	12.390592
12.864983	726.179525	12.395610
12.841588	725.574155	12.400627
12.570354	719.251375	12.405645
12.427726	726.291896	12.410663
12.870583	722.445608	12.415680
12.879256	722.460073	12.420698
12.518906	712.279128	12.425715
12.341585	701.719408	12.430733
12.454182	715.943578	12.435751
12.499862	716.747518	12.440768
12.777349	715.577766	12.445786
12.344061	719.406859	12.450803
12.689024	726.478757	12.455821
12.478172	721.216358	12.460839
13.014530	709.254836	12.465856
12.625460	723.598144	12.470874
12.661953	718.199408	12.475891
12.533607	722.747857	12.480909
12.813009	718.816570	12.485927
12.913479	729.726000	12.490944
12.868840	718.176812	12.495962
12.890143	724.349237	12.500979
12.987817	717.767055	12.505997
12.818199	720.226546	12.511015
12.952213	715.768804	12.516032
13.158177	715.733618	12.521050
12.782603	723.817074	12.526067
13.384614	716.907069	12.531085
12.839150	721.103910	12.536103
12.984284	719.623417	12.541120
13.087841	718.802627	12.546138
12.823008	719.768518	12.551155
12.977202	724.105725	12.556173
12.796609	730.776630	12.561191
12.929547	724.835874	12.566208
12.860114	721.198732	12.571226
12.594688	720.145067	12.576243
12.883357	726.746065	12.581261
13.014868	725.797850	12.586279
12.853300	722.414886	12.591296
12.855287	728.322086	12.596314
12.860410	728.384439	12.601331
13.189686	727.721003	12.606349
13.200595	743.141260	12.611367
13.291790	739.472793	12.616384
13.502546	731.992559	12.621402
12.861136	726.967602	12.626419
13.070561	724.284244	12.631437
12.999038	729.956744	12.636455
13.284116	738.398079	12.641472
13.174744	743.896602	12.646490
13.277417	747.194143	12.651507
13.136092	745.215467	12.656525
13.434739	747.677791	12.661543
13.421252	745.420444	12.666560
13.394163	731.470180	12.671578
13.532253	728.905221	12.676595
13.154125	716.448625	12.681613
13.110047	727.500475	12.686631
13.363406	741.462916	12.691648
13.172070	746.320970	12.696666
13.287099	746.707028	12.701683
13.474843	746.778817	12.706701
13.199456	750.472881	12.711719
13.330212	748.041601	12.716736
13.717846	740.303457	12.721754
13.601145	738.447177	12.726771
13.669526	736.379049	12.731789
13.317150	729.911114	12.736807
12.852885	726.871914	12.741824
13.433788	743.156446	12.746842
13.271539	749.897084	12.751859
13.589448	745.467506	12.756877
13.393637	746.239621	12.761895
13.340941	756.573330	12.766912
13.468116	753.827036	12.771930
13.374285	750.468234	12.776947
13.738283	745.548657	12.781965
13.381077	753.013905	12.786983
13.627846	751.943605	12.792000
13.482512	744.304219	12.797018
13.264801	747.626397	12.802035
13.580178	749.543335	12.807053
13.698337	754.996969	12.812071
13.502613	749.823721	12.817088
13.848583	753.389486	12.822106
13.731157	756.187983	12.827123
13.753286	748.311089	12.832141
13.735640	749.885415	12.837159
13.433512	750.421626	12.842176
13.710504	749.390801	12.847194
13.272281	751.756421	12.852211
13.596254	746.098330	12.857229
13.583661	760.862719	12.862247
13.534432	766.613808	12.867264
13.975951	773.358277	12.872282
13.930506	773.892393	12.877299
13.914141	763.500075	12.882317
14.016277	761.672834	12.887335
14.101501	756.484243	12.892352
13.903998	744.608555	12.897370
13.813124	749.015482	12.902387
13.689763	748.722311	12.907405
13.562021	754.627628	12.912423
13.506882	761.086514	12.917440
13.724823	777.064682	12.922458
14.327859	783.070817	12.927475
14.049394	783.085809	12.932493
14.151792	785.010665	12.937511
13.721804	776.462560	12.942528
14.157843	776.000244	12.947546
14.021078	766.608096	12.952563
14.099483	766.507566	12.957581
14.126430	780.628362	12.962599
13.920907	777.952799	12.967616
14.130277	774.957026	12.972634
13.985104	775.115362	12.977651
13.899959	771.909832	12.982669
14.203408	771.610167	12.987687
14.110260	777.787807	12.992704
14.233030	776.796771	12.997722
13.969901	780.548891	13.002739
14.029613	784.493737	13.007757
14.258449	772.699970	13.012775
14.226576	790.544201	13.017792
14.089362	779.915077	13.022810
13.982461	769.997585	13.027827
14.017359	767.145739	13.032845
14.169694	771.571608	13.037863
13.912985	774.451751	13.042880
14.037309	775.697871	13.047898
14.071059	784.759009	13.052915
14.361485	773.959168	13.057933
14.153349	773.732843	13.062951
14.213067	777.879652	13.067968
14.445664	776.944097	13.072986
14.395889	784.427762	13.078003
14.102449	779.127713	13.083021
14.918940	784.393735	13.088039
14.614177	785.709818	13.093056
14.209822	773.979923	13.098074
14.339170	773.085689	13.103091
13.986614	766.545187	13.108109
14.053428	782.575293	13.113127
14.038808	803.102361	13.118144
14.429991	795.963226	13.123162
14.431413	801.075298	13.128179
14.723497	792.518900	13.133197
14.718305	791.623523	13.138215
14.500185	797.258911	13.143232
15.200448	798.175526	13.148250
14.810472	802.998254	13.153267
14.569119	791.621653	13.158285
14.680724	781.758494	13.163303
14.399028	782.676522	13.168320
14.559311	796.852308	13.173338
14.352980	794.725963	13.178355
14.720228	796.773681	13.183373
14.605677	802.156267	13.188391
14.497839	800.951833	13.193408
14.684578	789.145674	13.198426
14.980998	801.409996	13.203443
15.010216	804.362389	13.208461
14.591976	797.106288	13.213479
14.700164	813.739032	13.218496
14.961724	803.394934	13.223514
14.746564	799.048340	13.228531
14.727490	799.843431	13.233549
14.807736	801.831697	13.238567
14.600616	802.564550	13.243584
15.127245	794.044215	13.248602
14.831520	800.578442	13.253619
15.142392	801.038148	13.258637
14.958978	791.116778	13.263655
14.827366	806.256331	13.268672
14.761794	801.949560	13.273690
14.988113	808.869555	13.278707
15.226397	801.691110	13.283725
15.156456	794.794180	13.288743
14.808521	784.352491	13.293760
14.849300	779.997609	13.298778
14.829261	793.409385	13.303795
14.901170	792.410488	13.308813
15.043633	802.259416	13.313831
14.988365	808.547930	13.318848
14.826059	807.064806	13.323866
14.736097	800.243572	13.328883
14.813356	805.640475	13.333901
14.972159	796.489462	13.338919
14.373536	802.057866	13.343936
14.594663	801.193522	13.348954
14.789634	819.728278	13.353971
14.865337	825.674524	13.358989
15.140468	822.169901	13.364007
14.761558	830.720972	13.369024
15.085384	822.156462	13.374042
14.968743	825.519721	13.379059
14.978706	827.228606	13.384077
15.240068	823.906003	13.389095
15.072043	836.640282	13.394112
15.179185	829.078312	13.399130
15.452131	831.014488	13.404147
14.979767	832.621751	13.409165
15.271959	832.825596	13.414183
14.975912	833.805820	13.419200
15.030128	840.834672	13.424218
15.280646	845.093797	13.429235
14.886504	849.484852	13.434253
15.480891	845.012203	13.439271
15.639367	850.835119	13.444288
15.503752	853.888921	13.449306
15.664646	860.860148	13.454323
15.377317	857.439936	13.459341
15.350775	855.219320	13.464359
15.565100	856.634465	13.469376
15.409666	856.153787	13.474394
15.549607	854.592042	13.479411
15.631795	861.032739	13.484429
15.742974	859.503874	13.489447
15.759899	861.609300	13.494464
15.312058	858.409733	13.499482
15.329595	846.468940	13.504499
15.179517	858.787041	13.509517
15.551530	857.933914	13.514535
15.503093	858.039320	13.519552
15.465822	857.612826	13.524570
15.389460	850.092041	13.529587
15.446913	853.854222	13.534605
15.838717	843.341504	13.539623
15.444082	848.928653	13.544640
15.652196	854.431426	13.549658
15.549571	846.005883	13.554675
15.221880	856.199434	13.559693
15.812975	863.441343	13.564711
16.066716	865.746578	13.569728
16.022614	867.441795	13.574746
16.190088	864.032819	13.579763
15.890760	860.456688	13.584781
16.156083	844.299138	13.589799
15.890237	850.917091	13.594816
15.771367	839.928478	13.599834
16.273588	835.347108	13.604851
16.144226	845.771699	13.609869
15.971224	841.314391	13.614887
15.754221	845.138237	13.619904
15.703168	847.484613	13.624922
15.906332	845.575363	13.629939
15.767724	847.989018	13.634957
15.817099	843.115245	13.639975
15.779468	847.255137	13.644992
15.588918	861.438261	13.650010
16.152535	863.581643	13.655027
16.239458	865.682482	13.660045
16.308302	875.088488	13.665063
16.442702	871.785644	13.670080
16.054197	866.607664	13.675098
16.074027	859.911321	13.680115
16.210976	872.241546	13.685133
16.204348	862.036998	13.690151
16.004566	857.921518	13.695168
16.123913	872.971563	13.700186
16.544403	867.282627	13.705203
15.960143	863.135492	13.710221
16.152633	860.776634	13.715239
16.178499	867.655281	13.720256
15.933722	877.015445	13.725274
16.601002	872.951152	13.730291
15.887196	877.196328	13.735309
15.858217	878.138129	13.740327
15.965572	878.058336	13.745344
15.870338	875.154153	13.750362
16.202577	870.498257	13.755379
16.054454	876.125927	13.760397
16.527750	885.156549	13.765415
16.511324	892.196421	13.770432
16.564002	890.761866	13.775450
16.776427	876.102027	13.780467
16.391927	872.744277	13.785485
16.036760	867.785163	13.790503
16.425963	874.872324	13.795520
16.612464	890.262212	13.800538
16.707828	881.465008	13.805555
16.409569	866.133626	13.810573
16.839950	874.861663	13.815591
16.226836	871.997088	13.820608
16.478673	876.401179	13.825626
16.727581	884.526331	13.830643
16.885194	889.939149	13.835661
16.495762	884.262704	13.840679
16.825035	866.731901	13.845696
16.398848	871.301515	13.850714
17.016435	869.381387	13.855731
16.727595	869.192871	13.860749
16.743802	861.193777	13.865767
16.529439	849.478430	13.870784
16.475895	866.423576	13.875802
17.287753	871.785017	13.880819
16.884431	867.597087	13.885837
16.591771	857.736869	13.890855
17.034880	860.246143	13.895872
17.131566	864.620740	13.900890
16.797232	854.113778	13.905907
16.492673	853.732055	13.910925
16.665732	852.619579	13.915943
17.193141	867.341004	13.920960
16.969550	853.777836	13.925978
16.778144	856.632047	13.930995
17.127678	855.006113	13.936013
17.043486	865.922287	13.941031
17.097324	854.685873	13.946048
16.801280	854.586840	13.951066
17.319104	853.000974	13.956083
17.128930	847.833145	13.961101
16.796861	846.688865	13.966119
16.905496	848.325587	13.971136
16.832708	861.224932	13.976154
17.290093	867.455739	13.981171
17.079893	882.891608	13.986189
17.099615	868.290180	13.991207
17.274511	872.053014	13.996224
16.974253	891.280317	14.001242
17.173389	883.751336	14.006259
16.934450	879.083385	14.011277
16.706056	881.110246	14.016295
17.209859	880.848811	14.021312
17.001786	886.902375	14.026330
17.005416	873.493158	14.031347
16.923446	884.241744	14.036365
17.092252	883.085748	14.041383
17.383459	884.410031	14.046400
16.948801	881.126359	14.051418
17.210321	887.753734	14.056435
17.445801	903.287483	14.061453
17.451903	896.902525	14.066471
17.570777	900.503678	14.071488
17.438024	903.815813	14.076506
17.311901	885.958272	14.081523
18.009389	897.576406	14.086541
17.633936	893.431467	14.091559
17.413076	883.806203	14.096576
17.400183	886.774633	14.101594
17.471325	884.743926	14.106611
17.373557	874.083358	14.111629
17.376883	874.534146	14.116647
17.703845	891.123433	14.121664
17.443691	895.114950	14.126682
17.830205	893.480099	14.131699
17.220142	896.904416	14.136717
17.622452	902.575780	14.141735
17.843547	896.867388	14.146752
17.514071	905.066822	14.151770
17.707627	902.714105	14.156787
17.845031	905.589711	14.161805
17.728994	902.613024	14.166823
17.779984	898.783532	14.171840
17.787102	905.542038	14.176858
17.901354	908.342356	14.181875
17.742258	889.319169	14.186893
17.592320	899.002242	14.191911
17.820901	905.893522	14.196928
17.513388	906.288569	14.201946
17.794665	896.484133	14.206963
17.920550	904.016236	14.211981
17.910829	912.607692	14.216999
18.157044	899.192244	14.222016
17.801283	902.895698	14.227034
17.802667	902.314865	14.232051
17.769183	902.222288	14.237069
17.887237	907.035371	14.242087
17.510760	899.807438	14.247104
17.974697	900.846060	14.252122
18.254201	904.207614	14.257139
18.118033	898.318166	14.262157
17.777042	900.693913	14.267175
17.786574	897.495710	14.272192
17.903279	909.068581	14.277210
17.980483	902.394846	14.282227
17.813107	906.987288	14.287245
18.174997	920.191374	14.292263
18.043503	919.915245	14.297280
18.307847	918.545561	14.302298
18.231047	927.074886	14.307315
18.179570	924.069210	14.312333
17.986293	927.242452	14.317351
18.265403	932.674237	14.322368
18.060555	929.496783	14.327386
18.130401	924.717628	14.332403
18.460629	917.038838	14.337421
17.839654	924.327479	14.342439
18.601701	919.894978	14.347456
18.441542	923.088309	14.352474
18.186548	917.826413	14.357491
18.285362	924.144626	14.362509
18.241957	936.840639	14.367527
18.494292	926.788235	14.372544
18.048215	937.789198	14.377562
18.107887	931.982854	14.382579
18.761747	932.546949	14.387597
18.414893	938.953490	14.392615
18.705163	925.698417	14.397632
18.350320	933.762962	14.402650
18.672660	938.440107	14.407667
18.622952	937.239236	14.412685
18.428761	939.036722	14.417703
18.944825	945.895880	14.422720
18.504932	939.182723	14.427738
18.670141	936.673472	14.432755
18.725920	946.564378	14.437773
18.195075	952.482029	14.442791
18.620577	945.542615	14.447808
18.769116	957.138962	14.452826
18.859964	956.522108	14.457843
18.844676	947.820992	14.462861
18.562197	955.423009	14.467879
18.950433	948.640872	14.472896
19.136193	955.898592	14.477914
19.234192	948.887094	14.482931
18.678150	940.222839	14.487949
18.243041	941.682302	14.492967
18.460116	949.361169	14.497984
18.612127	948.668522	14.503002
18.495371	948.412188	14.508019
19.087807	944.656171	14.513037
19.092824	945.359157	14.518055
19.035113	937.295799	14.523072
19.082749	942.312356	14.528090
19.009760	943.431421	14.533107
19.633975	940.027056	14.538125
19.504898	942.609650	14.543143
19.368562	943.252595	14.548160
19.159737	949.735477	14.553178
19.075469	943.276212	14.558195
19.301467	939.735036	14.563213
19.326453	946.238318	14.568231
19.081520	949.063008	14.573248
19.545874	937.519635	14.578266
19.098962	947.621350	14.583283
19.483124	940.009890	14.588301
19.260489	936.282950	14.593319
19.373461	929.035604	14.598336
19.079479	924.161620	14.603354
19.095730	936.807321	14.608371
19.616966	943.798214	14.613389
19.234479	949.011126	14.618407
19.649108	945.655170	14.623424
19.363714	944.980133	14.628442
19.419854	940.682780	14.633459
19.617432	925.160540	14.638477
19.004153	925.814628	14.643495
19.655222	941.157475	14.648512
19.749605	945.011754	14.653530
19.502112	938.208682	14.658547
19.562500	933.323702	14.663565
19.518638	930.048602	14.668583
19.615742	927.177579	14.673600
19.213768	920.284960	14.678618
19.140913	943.150189	14.683635
19.451436	937.481508	14.688653
19.358946	947.038901	14.693671
19.517219	946.007614	14.698688
19.581413	947.616551	14.703706
19.545679	949.673383	14.708723
19.410524	940.473392	14.713741
19.319155	948.430652	14.718759
19.476061	953.553272	14.723776
19.782971	959.173236	14.728794
19.797518	973.087836	14.733811
19.749493	964.672671	14.738829
19.610381	971.296183	14.743847
19.859102	969.543926	14.748864
20.329183	958.731780	14.753882
20.087403	973.844447	14.758899
20.158526	966.512085	14.763917
20.039612	950.477377	14.768935
19.830443	943.968132	14.773952
19.719078	957.078676	14.778970
19.844454	973.112458	14.783987
19.779573	959.082694	14.789005
19.986730	969.928324	14.794023
19.928555	961.937610	14.799040
20.179336	969.103163	14.804058
19.962549	963.510263	14.809075
19.885263	960.827329	14.814093
20.193834	960.346986	14.819111
20.252007	963.099240	14.824128
20.557383	961.316073	14.829146
20.232849	960.691310	14.834163
20.245664	956.271313	14.839181
20.341447	969.936582	14.844199
20.012708	957.203889	14.849216
20.173763	964.288738	14.854234
20.251011	958.384976	14.859251
20.481598	967.683799	14.864269
20.400169	968.368688	14.869287
20.559070	966.510498	14.874304
20.466430	964.397988	14.879322
20.217677	963.960237	14.884339
20.450316	955.046951	14.889357
20.289347	958.789514	14.894375
20.578925	960.817788	14.899392
20.532200	951.086481	14.904410
20.392592	959.126994	14.909427
20.392735	954.402863	14.914445
20.613583	955.179541	14.919463
20.429327	959.970280	14.924480
20.490390	962.712618	14.929498
20.659283	964.380993	14.934515
20.938095	952.677153	14.939533
20.783220	952.565607	14.944551
20.574068	956.921574	14.949568
20.471988	956.164348	14.954586
20.376923	958.688001	14.959603
20.481779	951.214696	14.964621
20.592857	961.220073	14.969639
20.584331	953.316305	14.974656
20.574677	945.314888	14.979674
20.355717	949.410453	14.984691
20.668808	948.228833	14.989709
20.487511	958.857232	14.994727
20.437046	964.299315	14.999744
21.004768	968.307114	15.004762
20.931416	984.684266	15.009779
20.904178	979.150210	15.014797
21.206478	979.674370	15.019815
20.870766	969.129685	15.024832
21.062187	963.788803	15.029850
21.029373	973.040278	15.034867
20.895988	971.839810	15.039885
20.926851	980.481783	15.044903
20.727668	981.570007	15.049920
21.041401	974.190401	15.054938
20.874360	982.380359	15.059955
21.105307	973.006588	15.064973
21.219608	974.001823	15.069991
21.100330	971.303335	15.075008
21.047909	974.672402	15.080026
20.823852	978.061881	15.085043
21.114378	981.828825	15.090061
21.210783	976.938226	15.095079
20.998412	979.824122	15.100096
20.832884	972.591717	15.105114
20.872691	985.145424	15.110131
21.149865	997.236156	15.115149
21.344591	999.604245	15.120167
20.953473	998.349230	15.125184
21.552287	1003.655522	15.130202
21.205229	1011.526389	15.135219
21.289907	995.466253	15.140237
21.400113	1001.445055	15.145255
21.310555	993.594910	15.150272
21.548320	997.944418	15.155290
21.391878	995.194910	15.160307
21.343362	994.388318	15.165325
21.439399	988.951827	15.170343
21.150213	995.854330	15.175360
21.413537	993.326639	15.180378
21.530138	1005.966232	15.185395
21.425465	1004.193256	15.190413
21.872189	999.708846	15.195431
21.628075	1015.424660	15.200448
21.632279	1007.064457	15.205466
22.057970	1010.236016	15.210483
21.907703	1002.830813	15.215501
22.033454	990.544876	15.220519
21.685622	1001.246565	15.225536
21.817655	990.502811	15.230554
21.750217	997.616938	15.235571
21.472841	998.209261	15.240589
21.853970	989.193945	15.245607
21.372730	1005.315892	15.250624
21.692679	1008.589120	15.255642
21.964955	1010.386567	15.260659
22.207639	1011.311324	15.265677
22.301570	1013.720353	15.270695
22.500731	1017.268005	15.275712
22.274101	995.875781	15.280730
22.433606	996.018239	15.285747
22.267443	982.786852	15.290765
22.343335	982.803475	15.295783
21.933530	994.553049	15.300800
22.299695	981.910956	15.305818
22.119564	987.426882	15.310835
22.289997	989.009814	15.315853
21.893812	981.428318	15.320871
21.999287	983.617799	15.325888
22.362930	989.058530	15.330906
21.964717	988.309540	15.335923
21.878800	995.833634	15.340941
22.201618	994.865087	15.345959
22.332277	1009.099302	15.350976
22.421173	1012.389570	15.355994
22.464984	1011.164666	15.361011
22.612083	1012.609225	15.366029
22.510285	993.971474	15.371047
22.315057	998.476759	15.376064
22.486140	993.202149	15.381082
22.290951	1000.834775	15.386099
22.444976	1012.793216	15.391117
22.433568	1013.643927	15.396135
22.486914	1022.203526	15.401152
22.792918	1021.310178	15.406170
22.823964	1013.128827	15.411187
22.667767	1014.589050	15.416205
22.791912	1012.569012	15.421223
22.507093	1011.161748	15.426240
22.368151	1008.248570	15.431258
22.741714	1017.575650	15.436275
22.296812	1019.367998	15.441293
22.639831	1008.989008	15.446311
22.765729	1020.349085	15.451328
22.780529	1014.950481	15.456346
22.841544	1021.211498	15.461363
22.672732	1018.192517	15.466381
23.125431	1006.464725	15.471399
22.795858	1012.704503	15.476416
22.491875	1007.945660	15.481434
22.858584	1007.042861	15.486451
22.413692	1021.638092	15.491469
22.860234	1014.742712	15.496487
22.929738	1017.916081	15.501504
23.004330	1008.563480	15.506522
22.922148	1013.745433	15.511539
22.482626	1016.745595	15.516557
23.102110	1029.452073	15.521575
23.418234	1031.829666	15.526592
23.352506	1031.035220	15.531610
23.318662	1022.254907	15.536627
23.101786	1012.985552	15.541645
23.071186	1007.549839	15.546663
23.378637	1021.289487	15.551680
23.206795	1024.759206	15.556698
23.566051	1015.681011	15.561715
23.328481	1006.762015	15.566733
23.547649	1006.844691	15.571751
23.069617	997.947359	15.576768
23.208998	999.869637	15.581786
23.298426	1002.522359	15.586803
23.405090	1011.313488	15.591821
23.749977	1008.533259	15.596839
23.805215	1004.974477	15.601856
23.560189	994.295739	15.606874
23.728785	994.853340	15.611891
23.626412	1003.225740	15.616909
23.631446	992.994055	15.621927
23.269926	998.790686	15.626944
23.432268	998.178478	15.631962
23.655529	992.854719	15.636979
23.633865	990.920500	15.641997
23.621162	992.651865	15.647015
23.531459	994.493047	15.652032
23.571334	995.155894	15.657050
23.779050	1000.832341	15.662067
23.284214	1000.107861	15.667085
23.683156	1001.213412	15.672103
23.679077	1013.480487	15.677120
23.844830	1021.650206	15.682138
23.859965	1016.223148	15.687155
23.576125	1026.959070	15.692173
24.042572	1029.631989	15.697191
24.306146	1030.673413	15.702208
24.011134	1020.365354	15.707226
24.195654	1017.717387	15.712243
24.169574	1027.819896	15.717261
24.233848	1017.945040	15.722279
24.160285	1006.955581	15.727296
23.949350	1007.603831	15.732314
23.921414	993.634559	15.737331
23.689804	1010.626501	15.742349
24.077330	1017.038648	15.747367
24.085532	1015.645722	15.752384
23.990914	1017.484515	15.757402
24.375388	1029.148316	15.762419
23.856579	1021.863600	15.767437
23.832138	1022.492281	15.772455
23.998115	1022.946151	15.777472
23.622902	1014.875388	15.782490
24.086840	1019.789281	15.787507
24.212156	1031.458719	15.792525
24.297715	1039.928107	15.797543
24.129542	1043.965294	15.802560
24.193711	1049.474761	15.807578
24.337153	1047.764134	15.812595
24.268662	1045.439574	15.817613
24.206473	1042.908910	15.822631
24.628054	1030.586352	15.827648
24.350749	1051.334484	15.832666
24.664603	1046.075499	15.837683
24.522599	1041.588069	15.842701
24.630970	1043.335301	15.847719
24.950131	1033.445998	15.852736
24.603525	1053.867257	15.857754
24.509570	1043.906571	15.862771
24.384182	1044.876014	15.867789
24.631952	1038.412353	15.872807
24.741709	1040.591708	15.877824
24.775482	1048.545307	15.882842
25.099102	1048.334014	15.887859
24.775516	1041.735251	15.892877
25.104153	1045.597260	15.897895
25.079934	1042.574697	15.902912
25.011809	1046.571062	15.907930
24.973789	1039.732182	15.912947
24.709509	1049.603550	15.917965
24.755263	1045.777997	15.922983
24.889087	1047.912580	15.928000
24.664680	1044.940120	15.933018
24.853793	1046.144614	15.938035
24.680430	1051.798360	15.943053
25.030217	1061.877080	15.948071
25.428261	1066.495136	15.953088
25.180790	1066.259152	15.958106
25.168925	1069.091755	15.963123
25.364733	1062.251173	15.968141
25.268746	1070.247075	15.973159
25.570798	1064.870003	15.978176
25.045488	1059.681709	15.983194
25.230181	1054.338691	15.988211
25.464351	1062.680811	15.993229
25.361185	1066.865671	15.998247
25.202341	1053.525796	16.003264
25.002149	1061.326482	16.008282
25.176907	1060.677625	16.013299
25.115350	1067.355369	16.018317
25.154028	1074.475094	16.023335
25.028119	1071.140160	16.028352
25.045602	1071.490920	16.033370
25.373564	1060.887030	16.038387
25.462752	1077.273674	16.043405
25.346274	1088.422226	16.048423
25.677761	1095.562641	16.053440
25.846814	1094.996722	16.058458
25.708950	1092.701891	16.063475
25.654559	1083.123183	16.068493
25.622840	1078.429227	16.073511
25.752856	1090.748060	16.078528
25.841408	1095.155537	16.083546
25.958975	1089.624147	16.088563
25.946257	1094.164155	16.093581
26.028028	1098.241334	16.098599
26.114738	1091.799575	16.103616
25.903668	1092.072313	16.108634
25.879612	1089.791322	16.113651
25.996974	1093.862958	16.118669
25.890431	1089.840204	16.123687
25.990289	1088.950547	16.128704
25.642216	1090.926638	16.133722
26.082433	1087.292121	16.138739
26.186193	1100.826862	16.143757
26.208337	1087.367265	16.148775
26.345908	1084.149094	16.153792
26.233883	1088.953868	16.158810
26.082346	1093.272495	16.163827
26.083834	1084.360420	16.168845
25.972884	1090.862829	16.173863
26.009764	1084.479323	16.178880
26.000713	1085.746231	16.183898
26.157865	1090.389176	16.188915
26.171364	1094.003619	16.193933
25.930410	1087.786445	16.198951
26.290611	1083.239747	16.203968
26.097112	1089.407874	16.208986
26.506697	1086.336696	16.214003
26.295697	1086.682006	16.219021
26.681704	1094.647055	16.224039
26.454227	1086.695267	16.229056
26.568218	1091.095627	16.234074
26.968114	1093.725270	16.239091
26.698766	1084.019085	16.244109
26.425071	1090.701465	16.249127
26.759876	1089.071492	16.254144
26.214586	1089.424668	16.259162
26.381393	1096.559167	16.264179
26.806482	1098.389635	16.269197
26.618294	1109.536742	16.274215
27.161806	1106.002902	16.279232
26.931922	1110.128607	16.284250
27.034065	1107.875301	16.289267
26.886846	1085.817361	16.294285
26.759591	1088.806786	16.299303
26.978827	1090.044462	16.304320
26.886901	1099.106393	16.309338
27.186994	1102.354328	16.314355
26.810670	1100.768803	16.319373
26.544735	1102.618500	16.324391
26.725635	1106.787543	16.329408
26.575522	1110.821934	16.334426
26.992736	1111.946737	16.339443
27.286547	1108.521201	16.344461
26.869740	1099.841500	16.349479
26.957667	1094.813334	16.354496
26.902277	1099.842820	16.359514
27.100453	1095.965123	16.364531
27.352643	1106.103244	16.369549
26.831198	1105.572249	16.374567
27.349961	1125.032043	16.379584
27.317049	1131.058418	16.384602
27.593527	1127.032824	16.389619
27.646727	1126.055756	16.394637
27.840529	1123.018169	16.399655
27.483838	1106.745789	16.404672
27.241060	1109.087337	16.409690
27.149841	1106.264540	16.414707
27.569517	1121.703532	16.419725
27.563663	1131.108680	16.424743
27.654106	1125.751913	16.429760
27.427492	1129.750883	16.434778
27.576105	1131.595999	16.439795
27.686720	1129.069975	16.444813
27.543670	1132.014529	16.449831
27.395581	1129.648703	16.454848
27.319856	1134.738169	16.459866
27.398945	1126.653426	16.464883
27.537005	1125.666302	16.469901
27.610933	1125.339252	16.474919
27.532039	1131.423278	16.479936
27.602081	1149.554956	16.484954
27.941052	1154.772363	16.489971
28.144633	1148.208246	16.494989
27.925062	1147.096923	16.500007
28.214442	1143.132433	16.505024
28.526096	1145.917833	16.510042
28.181332	1134.642319	16.515059
28.433159	1133.539652	16.520077
28.035241	1127.902318	16.525095
28.145246	1116.764291	16.530112
28.146856	1116.372762	16.535130
28.007260	1111.127554	16.540147
28.304868	1110.585799	16.545165
28.334056	1115.311790	16.550183
28.243963	1110.235598	16.555200
28.230871	1115.949616	16.560218
27.981415	1108.348376	16.565235
28.056745	1117.829239	16.570253
28.297795	1140.418632	16.575271
28.449666	1137.671591	16.580288
28.519650	1141.813730	16.585306
28.356776	1143.581114	16.590323
28.718390	1140.066120	16.595341
28.664150	1142.365694	16.600359
28.786158	1136.293961	16.605376
28.510429	1126.304727	16.610394
28.441702	1122.739975	16.615411
28.691632	1129.280883	16.620429
28.843624	1138.689862	16.625447
28.861580	1117.574988	16.630464
28.656917	1118.279069	16.635482
28.471963	1120.816741	16.640499
28.771202	1119.791899	16.645517
28.261934	1135.296640	16.650535
28.660921	1137.828603	16.655552
28.866307	1134.066538	16.660570
28.611153	1134.440813	16.665587
28.866648	1143.316132	16.670605
28.671028	1140.468560	16.675623
28.932738	1136.915474	16.680640
29.109647	1137.528589	16.685658
28.695519	1142.932674	16.690675
28.977004	1138.303545	16.695693
28.775309	1146.322251	16.700711
29.086348	1145.210364	16.705728
28.942729	1150.360898	16.710746
29.295865	1163.162589	16.715763
29.487673	1150.863101	16.720781
29.381265	1160.034614	16.725799
28.952839	1150.217462	16.730816
29.359692	1146.638620	16.735834
29.227896	1153.791231	16.740851
29.691114	1154.612232	16.745869
29.095863	1161.253185	16.750887
29.121831	1165.152877	16.755904
29.649235	1156.442903	16.760922
29.483857	1159.798034	16.765939
29.738775	1143.966876	16.770957
29.540097	1160.698215	16.775975
29.671409	1159.743698	16.780992
29.857722	1156.085583	16.786010
29.417636	1160.395504	16.791027
29.616864	1146.081478	16.796045
29.204974	1162.823924	16.801063
29.438292	1144.452573	16.806080
29.562859	1152.284785	16.811098
29.213876	1150.941149	16.816115
29.552739	1153.602394	16.821133
29.477198	1147.633997	16.826151
29.699223	1156.123218	16.831168
29.620294	1160.992285	16.836186
29.673084	1175.371300	16.841203
29.762812	1180.851582	16.846221
29.852363	1187.966588	16.851239
29.383730	1188.882183	16.856256
29.631141	1184.646509	16.861274
29.704687	1190.429112	16.866291
29.885740	1184.038902	16.871309
29.652308	1187.773861	16.876327
29.892097	1199.422430	16.881344
30.602226	1198.033811	16.886362
30.607149	1200.848041	16.891379
30.358918	1183.523607	16.896397
30.065086	1180.669229	16.901415
30.312501	1181.769982	16.906432
30.530121	1166.582080	16.911450
30.114407	1174.940231	16.916467
30.148595	1181.423230	16.921485
30.147579	1191.840663	16.926503
30.510908	1203.924434	16.931520
30.537947	1203.118692	16.936538
30.226384	1207.724193	16.941555
30.708298	1209.419594	16.946573
30.804711	1202.812183	16.951591
30.634141	1201.800524	16.956608
30.638175	1200.193639	16.961626
30.685450	1204.869501	16.966643
30.933522	1199.529195	16.971661
30.955364	1200.993271	16.976679
30.571073	1184.122363	16.981696
30.480215	1188.052872	16.986714
30.652899	1199.257457	16.991731
30.719750	1198.767406	16.996749
30.593290	1202.084928	17.001767
30.569817	1197.995567	17.006784
30.965260	1190.953441	17.011802
30.790098	1209.170694	17.016819
30.879632	1202.643249	17.021837
30.921435	1206.294333	17.026855
30.706469	1199.385112	17.031872
31.021267	1200.166108	17.036890
30.697315	1204.540009	17.041907
30.793569	1214.068158	17.046925
31.035286	1221.866382	17.051943
31.232794	1224.246691	17.056960
31.393526	1223.874566	17.061978
31.472130	1229.375529	17.066995
31.492541	1226.863535	17.072013
31.416901	1227.717945	17.077031
31.271554	1227.342983	17.082048
31.593030	1223.960454	17.087066
31.600770	1219.430729	17.092083
31.957392	1222.704599	17.097101
31.639612	1198.274676	17.102119
31.723171	1193.865696	17.107136
31.883400	1186.377359	17.112154
31.700073	1195.488283	17.117171
31.731423	1193.539477	17.122189
32.097566	1190.598121	17.127207
31.396176	1191.269091	17.132224
31.564984	1181.156965	17.137242
31.788692	1186.499624	17.142259
31.782545	1196.706421	17.147277
31.685905	1190.826501	17.152295
31.651607	1194.921774	17.157312
31.990865	1191.031557	17.162330
31.727265	1198.668607	17.167347
31.467845	1194.101590	17.172365
31.901509	1192.484618	17.177383
31.453033	1200.525992	17.182400
32.046182	1205.684905	17.187418
31.875440	1217.839215	17.192435
31.942905	1222.319435	17.197453
31.955217	1222.538460	17.202471
32.169067	1218.102877	17.207488
32.200270	1222.434109	17.212506
32.350574	1220.261653	17.217523
32.169319	1217.960939	17.222541
31.978511	1217.880231	17.227559
31.819423	1216.557516	17.232576
32.437285	1214.615219	17.237594
32.010075	1222.230416	17.242611
32.065789	1213.448689	17.247629
32.673735	1216.162722	17.252647
32.476978	1215.581170	17.257664
32.442603	1210.638285	17.262682
32.386119	1218.706998	17.267699
32.254385	1216.114553	17.272717
32.322011	1223.479138	17.277735
32.702117	1241.774073	17.282752
32.379715	1234.919434	17.287770
32.693193	1245.827574	17.292787
32.620905	1242.970251	17.297805
32.605551	1238.885928	17.302823
32.506332	1243.934901	17.307840
32.290317	1239.761900	17.312858
32.492157	1237.758142	17.317875
32.600533	1244.418961	17.322893
32.573012	1250.775895	17.327911
32.291920	1258.983737	17.332928
33.017755	1256.980444	17.337946
33.079376	1262.891159	17.342963
32.763212	1256.597273	17.347981
33.065713	1255.688680	17.352999
32.879751	1270.707701	17.358016
33.254261	1254.883072	17.363034
33.183868	1262.556340	17.368051
33.073599	1263.627582	17.373069
33.162700	1256.898213	17.378087
32.914935	1265.138739	17.383104
33.088924	1253.217495	17.388122
33.072238	1262.700138	17.393139
33.312060	1283.055600	17.398157
33.542166	1289.713263	17.403175
33.279870	1296.021560	17.408192
33.755341	1283.901877	17.413210
33.280391	1272.637077	17.418227
33.164785	1288.443576	17.423245
33.678024	1274.954713	17.428263
33.782689	1289.679193	17.433280
33.860759	1287.271823	17.438298
33.845273	1282.171343	17.443315
33.886197	1287.154328	17.448333
33.713376	1271.828311	17.453351
33.638524	1274.096397	17.458368
33.861045	1270.704020	17.463386
34.107495	1279.729138	17.468403
34.003020	1273.272900	17.473421
33.857339	1263.515804	17.478439
33.909756	1263.040622	17.483456
34.079996	1270.588066	17.488474
33.523633	1265.685411	17.493491
33.431502	1272.803492	17.498509
33.805069	1275.752842	17.503527
33.850017	1272.258724	17.508544
33.951667	1273.776652	17.513562
34.056330	1277.392718	17.518579
33.852108	1276.133830	17.523597
34.010709	1270.624397	17.528615
34.119337	1292.171097	17.533632
34.452154	1298.607644	17.538650
34.465984	1299.211442	17.543667
34.383121	1299.546272	17.548685
34.595528	1296.931793	17.553703
34.417192	1289.215260	17.558720
34.149138	1286.303202	17.563738
34.442900	1291.120591	17.568755
34.608700	1300.069914	17.573773
34.549583	1297.586071	17.578791
34.624927	1304.693869	17.583808
34.631399	1306.759949	17.588826
34.636646	1298.882285	17.593843
34.737004	1296.357834	17.598861
34.999525	1297.610877	17.603879
34.591449	1294.947837	17.608896
34.722367	1288.376048	17.613914
34.807915	1292.815600	17.618931
34.937289	1288.475203	17.623949
34.834585	1288.522789	17.628967
35.080902	1298.671402	17.633984
35.226215	1294.943903	17.639002
35.336984	1286.134633	17.644019
34.825589	1298.376750	17.649037
35.140693	1287.872557	17.654055
35.191291	1294.239434	17.659072
35.523619	1298.236623	17.664090
35.659318	1281.035354	17.669107
35.414112	1268.119017	17.674125
35.846834	1268.190537	17.679143
35.160911	1270.389662	17.684160
34.963034	1263.708129	17.689178
35.178205	1265.826918	17.694195
34.673223	1266.738708	17.699213
35.077732	1278.345905	17.704231
35.351792	1281.102466	17.709248
35.165284	1285.454987	17.714266
35.213802	1287.432468	17.719283
35.241042	1294.348936	17.724301
35.698766	1288.019754	17.729319
35.523824	1284.840736	17.734336
35.438873	1289.780204	17.739354
36.015820	1295.519178	17.744371
35.568627	1294.348611	17.749389
35.852064	1295.238635	17.754407
36.023802	1306.635939	17.759424
35.526545	1295.513453	17.764442
35.656974	1298.683699	17.769459
35.568852	1311.888715	17.774477
35.865207	1308.532172	17.779495
35.971064	1315.745676	17.784512
35.943140	1314.143756	17.789530
36.320751	1307.091738	17.794547
35.832520	1310.834835	17.799565
35.863730	1303.824129	17.804583
35.835772	1315.757459	17.809600
36.162980	1309.262398	17.814618
35.922176	1304.215927	17.819635
36.081830	1330.800860	17.824653
36.416746	1328.129432	17.829671
36.646113	1338.410095	17.834688
36.594433	1336.013452	17.839706
36.598935	1321.928419	17.844723
36.232989	1322.635528	17.849741
36.295185	1332.314210	17.854759
36.353770	1340.450269	17.859776
36.249269	1339.172694	17.864794
36.707004	1336.460052	17.869811
36.269726	1345.383374	17.874829
36.629420	1338.255238	17.879847
36.443816	1337.804490	17.884864
36.551653	1343.622829	17.889882
36.674297	1336.714639	17.894899
36.385178	1338.309193	17.899917
36.682930	1336.435658	17.904935
36.811504	1339.896534	17.909952
37.245577	1346.677096	17.914970
37.187713	1346.174901	17.919987
36.907726	1341.686788	17.925005
36.847049	1323.083315	17.930023
37.037173	1330.627688	17.935040
36.994747	1344.349477	17.940058
37.232374	1349.440709	17.945075
36.975059	1355.823991	17.950093
37.243916	1341.205477	17.955111
37.487589	1349.593589	17.960128
37.455444	1348.525656	17.965146
37.512823	1339.197651	17.970163
37.681310	1342.989986	17.975181
37.377059	1335.728539	17.980199
37.691974	1330.096920	17.985216
37.236225	1332.351734	17.990234
37.569033	1334.755174	17.995251
37.481806	1347.878026	18.000269
37.617265	1347.617131	18.005287
37.895901	1343.152495	18.010304
37.681950	1337.618995	18.015322
37.882263	1333.763004	18.020339
37.618420	1334.176506	18.025357
37.742719	1336.997418	18.030375
37.590000	1336.181788	18.035392
37.694634	1337.721348	18.040410
37.910788	1336.810416	18.045427
37.864592	1344.180149	18.050445
37.921906	1345.881712	18.055463
37.702978	1349.017998	18.060480
37.658934	1359.565305	18.065498
37.775226	1345.270343	18.070515
37.757475	1344.269596	18.075533
37.963391	1363.835166	18.080551
38.037772	1371.375487	18.085568
38.112943	1377.334623	18.090586
38.103897	1373.031536	18.095603
38.159959	1377.239015	18.100621
37.893361	1369.267944	18.105639
38.338229	1366.005033	18.110656
38.136374	1377.959168	18.115674
38.407367	1363.987245	18.120691
38.293745	1367.911871	18.125709
38.347225	1376.427439	18.130727
38.792847	1380.422786	18.135744
39.117704	1388.473228	18.140762
38.904388	1364.137266	18.145779
38.842195	1359.466915	18.150797
38.540877	1360.870865	18.155815
39.003635	1352.398080	18.160832
38.897279	1364.873826	18.165850
38.719228	1360.212046	18.170867
38.456852	1351.918433	18.175885
38.806561	1366.907783	18.180903
39.357538	1373.733270	18.185920
38.875753	1375.256838	18.190938
39.047248	1382.226619	18.195955
38.864805	1374.592740	18.200973
38.912993	1383.219588	18.205991
39.446550	1378.929849	18.211008
39.074290	1385.627685	18.216026
38.992006	1383.945859	18.221043
39.000287	1381.969065	18.226061
39.106472	1386.818840	18.231079
39.306234	1372.312045	18.236096
39.251052	1390.384570	18.241114
39.302415	1383.683120	18.246131
39.235781	1380.200042	18.251149
39.339242	1377.245906	18.256167
39.364538	1374.584807	18.261184
39.187115	1379.781695	18.266202
39.548271	1386.841870	18.271219
39.086754	1397.845520	18.276237
39.469013	1404.167110	18.281255
39.698054	1398.861266	18.286272
39.575811	1405.491780	18.291290
39.668866	1406.465101	18.296307
39.648376	1401.109745	18.301325
39.528453	1397.540286	18.306343
39.644247	1406.901393	18.311360
40.012079	1421.559762	18.316378
40.081233	1421.599525	18.321395
40.219983	1430.149180	18.326413
40.334905	1429.070967	18.331431
40.541657	1416.832085	18.336448
40.391491	1409.836953	18.341466
40.141904	1402.892017	18.346483
40.576475	1398.431492	18.351501
40.202279	1398.309908	18.356519
40.506968	1403.734699	18.361536
40.153164	1402.587454	18.366554
39.883278	1408.881193	18.371571
40.138666	1408.383873	18.376589
40.439613	1425.567849	18.381607
41.071510	1414.206368	18.386624
40.830454	1421.407655	18.391642
40.393063	1426.903810	18.396659
40.597262	1422.548575	18.401677
40.474617	1422.498279	18.406695
40.685527	1407.715162	18.411712
40.314345	1419.092927	18.416730
40.650183	1414.376369	18.421747
40.647215	1419.934273	18.426765
40.650553	1420.148386	18.431783
40.541268	1411.120850	18.436800
40.573060	1428.170008	18.441818
40.730569	1436.398007	18.446835
40.577864	1437.472710	18.451853
40.701076	1426.868923	18.456871
41.023360	1437.504409	18.461888
40.980219	1438.549430	18.466906
41.381738	1435.643552	18.471923
41.207374	1441.985547	18.476941
40.826200	1456.457602	18.481959
41.535166	1459.398944	18.486976
41.497914	1464.911707	18.491994
41.761815	1461.926265	18.497011
41.617281	1462.901867	18.502029
41.672706	1456.199757	18.507047
41.631837	1447.142616	18.512064
41.053939	1442.088629	18.517082
41.298506	1451.477048	18.522099
41.484082	1457.011920	18.527117
41.542663	1456.608357	18.532135
41.811674	1454.518377	18.537152
42.042580	1457.246970	18.542170
41.920980	1454.463563	18.547187
42.278896	1454.761327	18.552205
41.994475	1460.836439	18.557223
42.253818	1459.060391	18.562240
42.012487	1457.614762	18.567258
42.011236	1452.470991	18.572275
42.568604	1450.168856	18.577293
42.162054	1463.231056	18.582311
42.224222	1454.587061	18.587328
42.294285	1460.076802	18.592346
42.138618	1447.834366	18.597363
42.394900	1448.119551	18.602381
42.123506	1459.989893	18.607399
42.457140	1457.122984	18.612416
42.465398	1458.611288	18.617434
42.509268	1458.989506	18.622451
42.893415	1448.509183	18.627469
42.565039	1450.362325	18.632487
42.307634	1455.843090	18.637504
42.243826	1452.902360	18.642522
42.146348	1450.399223	18.647539
42.398593	1452.559599	18.652557
42.252639	1456.161072	18.657575
42.277839	1457.965476	18.662592
42.571687	1468.195150	18.667610
42.376356	1478.848134	18.672627
42.788636	1469.815102	18.677645
42.612213	1481.342465	18.682663
42.949479	1472.497839	18.687680
42.699332	1476.285953	18.692698
43.001048	1483.390134	18.697715
43.061227	1490.907470	18.702733
43.059922	1495.919179	18.707751
43.440861	1493.139574	18.712768
43.659840	1494.929591	18.717786
43.483840	1504.112116	18.722803
43.418532	1490.066222	18.727821
43.157008	1493.306995	18.732839
43.407875	1492.453768	18.737856
43.863732	1496.952482	18.742874
43.565884	1498.453734	18.747891
43.683828	1492.616044	18.752909
43.465549	1493.161312	18.757927
43.476635	1489.634553	18.762944
43.843011	1501.875845	18.767962
43.742473	1500.786992	18.772979
43.938759	1492.172591	18.777997
44.016764	1501.233515	18.783015
43.608743	1494.571990	18.788032
44.031695	1501.395369	18.793050
43.833002	1499.747436	18.798067
44.075719	1495.957392	18.803085
43.708203	1490.583454	18.808103
43.783508	1494.996250	18.813120
43.857016	1494.454662	18.818138
43.948652	1489.504703	18.823155
44.054942	1501.205815	18.828173
44.194937	1521.381431	18.833191
44.017055	1519.364178	18.838208
44.336658	1516.565717	18.843226
44.221768	1527.079972	18.848243
44.513294	1522.505986	18.853261
44.329815	1524.415472	18.858279
44.292281	1525.999274	18.863296
44.315550	1512.002688	18.868314
44.004555	1522.266602	18.873331
44.442089	1522.586686	18.878349
44.759124	1531.550449	18.883367
44.833849	1537.124696	18.888384
45.323894	1532.036955	18.893402
45.077472	1519.392028	18.898419
45.098719	1507.942524	18.903437
44.969749	1510.490469	18.908455
44.907681	1501.076835	18.913472
45.144373	1505.492908	18.918490
44.956571	1513.695810	18.923507
45.037872	1494.359988	18.928525
45.128756	1499.253203	18.933543
44.984277	1515.077021	18.938560
45.387744	1518.766536	18.943578
45.362154	1534.726497	18.948595
45.599431	1520.658714	18.953613
45.548252	1509.987355	18.958631
44.889400	1511.200828	18.963648
45.089653	1520.091248	18.968666
45.381243	1527.575726	18.973683
45.670040	1526.113825	18.978701
45.657574	1523.733142	18.983719
45.509339	1533.602489	18.988736
45.821824	1526.017720	18.993754
45.442023	1536.443836	18.998771
45.473468	1525.974201	19.003789
45.468311	1531.848065	19.008807
45.511661	1531.342729	19.013824
45.784526	1535.664814	19.018842
45.758505	1551.631170	19.023859
46.124687	1553.366716	19.028877
46.202646	1556.750307	19.033895
45.908587	1552.589383	19.038912
46.280732	1555.867210	19.043930
46.166536	1558.150926	19.048947
46.106242	1551.813941	19.053965
46.169426	1554.821130	19.058983
46.151483	1555.486689	19.064000
46.341790	1549.214831	19.069018
46.188662	1554.761442	19.074035
46.219120	1543.272611	19.079053
46.047680	1554.660388	19.084071
46.126900	1562.360984	19.089088
46.666616	1562.680939	19.094106
46.725358	1570.081765	19.099123
46.602159	1574.553889	19.104141
46.750559	1565.738622	19.109159
46.737457	1574.678067	19.114176
46.723605	1569.510978	19.119194
46.463078	1572.461272	19.124211
46.375800	1570.073295	19.129229
46.752060	1575.808893	19.134247
46.703719	1590.885653	19.139264
47.015693	1589.243411	19.144282
46.947852	1601.634429	19.149299
47.234654	1593.905305	19.154317
47.586053	1594.216710	19.159335
47.478741	1584.870037	19.164352
47.187441	1578.606879	19.169370
47.286910	1588.134728	19.174387
47.716068	1587.906999	19.179405
47.323770	1581.848916	19.184423
47.444435	1587.248766	19.189440
47.591894	1585.019903	19.194458
47.593670	1582.586501	19.199475
47.370442	1587.247774	19.204493
47.535883	1587.531326	19.209511
47.602588	1583.497265	19.214528
47.738103	1583.564567	19.219546
47.776287	1585.698328	19.224563
47.640429	1582.566820	19.229581
48.349963	1591.690413	19.234599
47.937524	1597.908582	19.239616
48.064556	1590.147529	19.244634
48.053989	1604.918614	19.249651
48.382358	1596.570781	19.254669
48.292979	1576.794378	19.259687
47.828740	1583.579192	19.264704
48.299022	1581.479952	19.269722
48.099244	1597.381882	19.274739
48.180403	1592.442994	19.279757
48.463751	1605.306364	19.284775
48.592586	1609.117552	19.289792
48.389200	1600.811482	19.294810
48.456071	1606.920314	19.299827
48.241048	1606.284787	19.304845
48.613960	1606.968390	19.309863
48.309729	1606.684429	19.314880
48.823716	1607.813135	19.319898
48.388364	1610.049028	19.324915
48.609161	1595.816491	19.329933
48.474069	1599.914926	19.334951
48.401022	1626.564933	19.339968
48.812487	1623.891011	19.344986
48.906565	1628.386125	19.350003
48.734114	1630.035125	19.355021
48.820104	1627.831606	19.360039
48.523865	1639.352479	19.365056
48.652666	1649.431225	19.370074
49.219645	1646.969777	19.375091
48.928733	1657.240109	19.380109
49.186760	1646.785619	19.385127
49.064381	1649.398830	19.390144
49.375565	1651.909824	19.395162
49.310925	1658.540931	19.400179
49.591400	1656.417584	19.405197
50.018081	1663.076339	19.410215
49.842263	1662.693488	19.415232
50.029670	1658.167237	19.420250
49.960831	1642.199851	19.425267
49.597850	1647.185861	19.430285
49.869222	1654.932321	19.435303
49.837217	1659.352397	19.440320
50.711716	1660.920447	19.445338
50.187548	1648.391256	19.450355
50.039930	1644.620929	19.455373
50.223682	1644.841670	19.460391
49.877657	1644.131862	19.465408
49.939585	1650.506570	19.470426
50.035002	1662.585028	19.475443
50.168396	1666.900458	19.480461
50.334057	1664.823389	19.485479
50.307032	1669.331057	19.490496
49.965855	1668.970795	19.495514
50.454727	1661.339571	19.500531
50.558806	1661.437015	19.505549
50.650487	1659.396711	19.510567
50.774894	1667.150279	19.515584
51.040463	1657.221638	19.520602
51.056779	1656.490130	19.525619
50.385354	1658.229443	19.530637
51.051351	1655.260262	19.535655
50.658466	1657.416964	19.540672
50.716268	1657.938187	19.545690
51.371139	1674.871636	19.550707
51.052588	1681.416049	19.555725
51.235128	1667.173633	19.560743
51.235887	1677.676282	19.565760
51.325620	1675.257576	19.570778
51.765268	1678.436552	19.575795
51.200264	1673.825468	19.580813
51.250306	1659.512167	19.585831
51.333647	1677.572883	19.590848
51.436740	1667.887288	19.595866
52.028080	1668.237078	19.600883
51.557445	1654.235226	19.605901
51.817888	1650.499196	19.610919
51.672519	1646.930492	19.615936
51.730270	1646.912071	19.620954
51.737926	1652.812382	19.625971
51.761716	1665.564726	19.630989
51.998902	1660.459513	19.636007
51.889545	1677.641341	19.641024
51.975652	1676.703302	19.646042
51.805164	1669.502945	19.651059
51.822053	1671.901968	19.656077
52.150732	1668.931653	19.661095
52.154268	1664.901097	19.666112
52.035164	1663.527941	19.671130
52.086733	1664.542450	19.676147
51.963055	1671.460470	19.681165
52.259245	1672.118150	19.686183
52.019754	1670.817387	19.691200
52.566211	1685.905764	19.696218
52.568851	1693.927615	19.701235
52.428729	1699.958251	19.706253
52.734614	1693.412721	19.711271
52.936655	1686.987506	19.716288
52.712841	1689.600736	19.721306
53.098709	1687.691355	19.726323
52.679483	1700.623155	19.731341
52.834011	1689.821828	19.736359
52.567294	1692.094593	19.741376
52.719514	1691.894202	19.746394
52.673713	1689.275685	19.751411
52.499917	1697.454399	19.756429
52.619223	1700.875762	19.761447
52.775542	1707.655526	19.766464
52.880289	1703.000119	19.771482
53.522281	1710.221830	19.776499
53.196744	1710.850077	19.781517
53.364494	1727.048358	19.786535
53.523146	1735.361526	19.791552
53.522304	1731.965968	19.796570
54.018941	1735.113990	19.801587
53.925104	1734.721528	19.806605
53.983893	1724.932345	19.811623
53.872884	1721.260445	19.816640
53.992888	1716.448021	19.821658
53.715996	1719.826931	19.826675
53.810977	1724.230408	19.831693
53.928021	1719.137571	19.836711
54.085483	1729.833609	19.841728
54.262615	1723.847770	19.846746
54.237030	1726.114555	19.851763
53.930012	1727.538356	19.856781
54.629194	1720.218354	19.861799
54.606875	1727.496163	19.866816
54.355063	1727.743694	19.871834
54.672966	1715.765020	19.876851
54.940179	1717.522303	19.881869
54.670723	1723.771903	19.886887
54.240361	1722.627088	19.891904
54.353788	1725.197285	19.896922
54.781396	1714.205100	19.901939
54.910970	1728.518957	19.906957
54.921205	1711.731292	19.911975
54.847578	1723.504744	19.916992
54.597696	1724.809193	19.922010
54.980329	1714.840203	19.927027
54.461147	1727.588765	19.932045
54.613545	1722.118029	19.937063
54.632528	1728.237514	19.942080
55.067512	1742.683716	19.947098
55.144647	1744.514778	19.952115
55.043309	1746.938531	19.957133
55.389873	1736.855221	19.962151
55.329183	1745.413988	19.967168
55.120299	1748.091176	19.972186
55.643355	1734.751921	19.977203
55.377033	1745.204673	19.982221
54.971678	1740.859056	19.987239
55.116581	1741.401435	19.992256
55.645859	1768.633234	19.997274
56.084899	1766.422069	20.002291
55.651811	1773.931114	20.007309
55.922425	1775.302855	20.012327
55.903400	1771.288411	20.017344
55.405877	1762.090764	20.022362
55.978865	1760.477298	20.027379
55.794359	1774.679142	20.032397
55.996965	1764.138536	20.037415
55.999550	1768.423862	20.042432
55.975310	1790.017098	20.047450
56.234122	1788.913305	20.052467
56.069047	1789.478701	20.057485
56.408084	1792.742791	20.062503
56.670743	1780.311915	20.067520
56.548038	1787.201425	20.072538
56.589196	1778.901381	20.077555
56.340534	1780.751612	20.082573
56.578374	1784.397540	20.087591
56.519851	1787.338510	20.092608
56.731932	1807.228664	20.097626
57.149976	1799.128714	20.102643
57.168278	1804.045936	20.107661
57.239307	1800.563434	20.112679
57.261098	1786.743592	20.117696
57.458607	1797.730089	20.122714
57.557687	1777.905185	20.127731
57.365372	1769.458454	20.132749
57.532586	1777.969130	20.137767
57.233633	1776.507198	20.142784
57.171857	1776.548412	20.147802
57.663838	1773.423264	20.152819
57.717997	1792.990843	20.157837
57.777794	1793.587501	20.162855
57.852309	1785.269636	20.167872
57.617396	1779.714014	20.172890
57.906929	1784.724705	20.177907
57.469093	1792.957196	20.182925
57.602800	1788.959995	20.187943
57.961746	1798.801017	20.192960
57.666346	1790.231466	20.197978
58.100991	1788.481743	20.202995
57.558697	1792.283850	20.208013
57.809561	1789.764300	20.213031
58.081585	1798.154522	20.218048
58.033999	1808.936182	20.223066
57.902639	1808.978763	20.228083
58.180228	1817.570105	20.233101
58.600215	1815.636463	20.238119
58.648086	1812.937070	20.243136
58.419661	1814.926169	20.248154
58.841734	1814.380796	20.253171
58.598073	1817.767173	20.258189
58.502010	1821.395666	20.263207
58.637453	1818.202942	20.268224
58.410603	1821.103850	20.273242
58.881822	1835.781179	20.278259
59.125876	1839.830106	20.283277
59.056554	1839.784130	20.288295
59.504161	1835.630745	20.293312
59.374432	1839.892507	20.298330
59.508062	1820.447197	20.303347
58.971024	1823.134461	20.308365
58.854462	1828.211547	20.313383
59.346221	1816.773798	20.318400
59.280854	1835.754101	20.323418
59.355711	1826.325288	20.328435
59.451321	1823.063023	20.333453
59.354497	1828.424222	20.338471
59.288703	1821.964918	20.343488
59.523040	1826.637066	20.348506
59.556215	1825.751443	20.353523
59.718723	1838.548586	20.358541
59.666430	1835.656495	20.363559
60.208709	1840.331196	20.368576
59.689760	1843.179754	20.373594
59.861821	1841.360452	20.378611
59.980103	1838.716366	20.383629
60.278144	1840.614033	20.388647
60.012665	1846.162447	20.393664
60.241129	1841.632914	20.398682
60.203074	1858.361989	20.403699
60.689332	1863.705002	20.408717
60.696481	1868.055916	20.413735
60.493079	1869.589831	20.418752
60.283074	1867.441836	20.423770
60.671267	1866.043331	20.428787
60.532305	1861.618337	20.433805
61.029469	1870.377496	20.438823
60.784362	1863.826170	20.443840
60.705992	1868.834203	20.448858
60.736618	1871.979063	20.453875
60.748944	1872.172847	20.458893
60.917736	1872.619990	20.463911
61.452477	1883.399395	20.468928
61.353626	1895.593467	20.473946
61.393290	1891.563547	20.478963
61.332148	1890.976637	20.483981
61.223636	1893.417306	20.488999
61.623819	1885.572570	20.494016
61.221889	1888.674324	20.499034
61.060299	1889.740969	20.504051
61.088001	1903.010442	20.509069
61.312575	1909.255775	20.514087
61.757857	1912.115169	20.519104
61.702380	1917.940188	20.524122
61.951847	1913.309533	20.529139
61.775166	1907.574386	20.534157
61.530580	1914.729082	20.539175
62.166456	1909.015752	20.544192
62.295229	1910.403276	20.549210
62.142871	1915.665846	20.554227
62.106446	1932.555689	20.559245
62.100298	1934.639587	20.564263
62.662337	1933.586408	20.569280
63.085339	1930.989542	20.574298
62.782716	1938.986446	20.579315
63.050857	1928.435539	20.584333
62.722805	1919.738461	20.589351
63.027871	1911.015401	20.594368
62.746254	1908.212653	20.599386
62.681074	1907.575877	20.604403
62.749228	1912.838829	20.609421
63.027675	1929.348274	20.614439
63.196544	1929.858525	20.619456
63.367033	1934.610072	20.624474
63.379571	1929.893221	20.629491
62.819475	1931.643629	20.634509
62.943625	1936.935741	20.639527
63.127644	1930.232368	20.644544
63.158937	1929.050377	20.649562
63.027086	1941.183344	20.654579
63.054735	1932.967385	20.659597
63.035692	1932.194032	20.664615
63.119599	1945.072920	20.669632
63.308682	1947.697644	20.674650
63.175205	1950.470423	20.679667
63.434768	1963.274636	20.684685
63.448124	1979.582395	20.689703
63.727961	1971.721644	20.694720
63.660207	1978.583737	20.699738
63.840678	1987.531122	20.704755
64.276560	1977.348561	20.709773
63.971900	1989.631547	20.714791
64.344483	1988.254398	20.719808
64.291304	2007.012071	20.724826
64.591787	1996.771681	20.729843
64.795464	1996.291866	20.734861
64.495948	1995.505371	20.739879
64.782892	1994.810612	20.744896
64.648120	1994.613874	20.749914
64.782570	2003.464286	20.754931
64.799434	2000.356266	20.759949
64.929483	1996.845601	20.764967
65.160918	2005.624108	20.769984
64.912993	1999.354048	20.775002
64.986236	1996.578090	20.780019
65.032887	1992.685920	20.785037
64.788561	1999.525017	20.790055
64.767912	1997.688364	20.795072
64.969592	2013.389298	20.800090
65.108598	2025.527490	20.805107
65.413014	2023.883231	20.810125
65.047296	2030.223667	20.815143
65.343967	2025.683468	20.820160
65.499068	2016.535563	20.825178
65.243109	2035.523660	20.830195
65.830799	2039.411829	20.835213
65.925608	2052.080805	20.840231
65.834764	2047.613558	20.845248
66.168386	2042.288086	20.850266
66.015047	2041.384153	20.855283
66.300751	2039.540826	20.860301
66.228007	2046.974945	20.865319
66.197932	2033.633222	20.870336
66.234948	2033.832632	20.875354
66.147124	2035.512675	20.880371
66.607310	2026.115285	20.885389
66.303911	2028.387492	20.890407
66.631281	2037.062711	20.895424
66.818947	2048.300214	20.900442
66.773493	2060.157867	20.905459
67.238958	2055.171641	20.910477
66.922400	2040.788874	20.915495
66.837616	2040.448647	20.920512
66.941456	2049.594194	20.925530
67.069964	2060.926126	20.930547
67.439804	2049.655540	20.935565
67.320967	2054.994987	20.940583
67.451058	2044.989390	20.945600
67.507037	2048.524827	20.950618
67.201292	2056.339224	20.955635
67.399833	2050.103780	20.960653
67.316106	2054.917031	20.965671
67.127273	2051.670607	20.970688
67.633040	2037.699476	20.975706
67.182077	2047.130226	20.980723
67.706467	2048.718108	20.985741
67.543400	2056.576566	20.990759
67.301284	2066.473447	20.995776
67.805919	2070.159949	21.000794
68.013562	2084.843806	21.005811
68.028832	2072.523831	21.010829
67.648041	2083.133463	21.015847
67.924286	2082.254166	21.020864
68.388978	2087.799428	21.025882
68.522883	2100.951523	21.030899
68.526391	2102.964507	21.035917
68.500955	2101.295854	21.040935
68.731334	2095.733965	21.045952
69.040285	2098.501001	21.050970
68.677983	2102.057389	21.055987
68.867075	2095.694006	21.061005
68.413991	2093.754250	21.066023
68.702386	2094.873929	21.071040
69.009857	2086.702699	21.076058
68.809714	2094.743679	21.081075
69.066266	2102.896602	21.086093
69.219747	2096.352563	21.091111
68.892405	2103.103635	21.096128
69.090565	2110.031678	21.101146
69.319457	2111.722381	21.106163
69.435297	2118.890473	21.111181
69.769766	2122.786525	21.116199
69.579060	2121.143602	21.121216
69.977643	2112.257555	21.126234
69.474726	2117.622104	21.131251
69.884225	2114.481336	21.136269
69.770532	2113.164109	21.141287
69.469767	2111.866540	21.146304
69.924344	2111.994627	21.151322
70.072309	2142.139341	21.156339
70.170106	2137.292391	21.161357
70.547785	2129.810831	21.166375
70.181057	2139.648255	21.171392
70.419096	2130.743011	21.176410
70.277420	2134.296614	21.181427
70.120286	2130.928470	21.186445
70.669019	2131.092393	21.191463
70.404273	2134.718808	21.196480
70.027476	2130.273970	21.201498
70.543527	2153.686563	21.206515
70.891403	2150.441769	21.211533
71.187662	2157.433457	21.216551
71.146980	2157.821699	21.221568
71.080069	2160.214899	21.226586
71.158267	2153.733055	21.231603
71.291314	2150.433343	21.236621
71.426923	2151.630464	21.241639
71.220192	2153.385838	21.246656
71.228648	2150.206514	21.251674
71.763628	2158.429728	21.256691
71.640511	2167.194085	21.261709
71.927927	2169.854027	21.266727
71.848157	2169.102743	21.271744
71.734330	2174.037483	21.276762
71.927137	2172.224385	21.281779
72.049457	2163.015234	21.286797
72.220580	2163.307380	21.291815
72.082611	2169.066425	21.296832
71.978832	2169.726435	21.301850
71.983895	2175.898736	21.306867
72.187752	2169.943303	21.311885
71.955864	2163.004781	21.316903
71.955478	2161.903450	21.321920
72.341244	2160.915575	21.326938
72.438586	2184.346060	21.331955
72.481923	2191.146754	21.336973
72.690338	2183.132921	21.341991
72.526914	2185.496968	21.347008
73.002246	2184.536174	21.352026
72.509619	2194.317486	21.357043
72.409799	2188.769107	21.362061
72.408956	2198.843102	21.367079
72.763435	2208.479908	21.372096
73.341843	2207.462038	21.377114
73.081688	2216.863168	21.382131
73.432909	2214.419457	21.387149
73.279742	2212.088992	21.392167
73.430387	2219.775596	21.397184
73.467083	2223.399280	21.402202
73.140263	2238.923907	21.407219
73.614413	2236.268540	21.412237
73.989972	2236.459427	21.417255
74.119890	2234.719234	21.422272
74.466685	2240.061983	21.427290
74.123236	2239.029840	21.432307
74.527345	2233.434548	21.437325
74.876747	2228.860840	21.442343
74.614632	2232.130241	21.447360
74.552852	2219.553904	21.452378
74.402060	2220.382189	21.457395
74.579871	2215.428082	21.462413
74.470397	2229.186237	21.467431
74.595705	2220.418427	21.472448
74.451239	2226.339456	21.477466
74.639529	2230.144677	21.482483
74.609832	2228.656566	21.487501
74.561584	2228.995491	21.492519
74.638175	2253.524418	21.497536
74.959807	2240.995674	21.502554
74.812221	2250.164689	21.507571
74.677860	2250.627481	21.512589
75.083235	2255.970582	21.517607
75.293377	2278.499956	21.522624
75.259658	2276.504354	21.527642
75.191707	2279.049219	21.532659
74.965217	2277.342421	21.537677
75.458568	2283.328276	21.542695
75.679894	2296.959236	21.547712
75.784166	2297.340692	21.552730
76.090029	2309.298455	21.557747
76.306288	2308.693590	21.562765
76.112575	2301.291453	21.567783
75.867699	2302.576228	21.572800
76.270985	2298.846228	21.577818
76.572531	2295.924220	21.582835
76.088249	2297.334636	21.587853
76.079397	2288.363606	21.592871
76.063581	2308.286644	21.597888
76.654716	2321.386649	21.602906
76.751904	2329.949518	21.607923
76.539427	2324.800511	21.612941
76.845722	2316.869215	21.617959
76.853097	2325.045255	21.622976
76.900654	2315.497352	21.627994
76.594073	2321.320570	21.633011
76.523135	2324.708554	21.638029
76.811643	2334.605023	21.643047
76.937354	2338.716673	21.648064
76.933641	2340.632972	21.653082
76.815929	2346.278460	21.658099
77.262077	2366.934416	21.663117
77.727804	2365.751033	21.668135
77.539365	2369.605470	21.673152
77.665495	2371.170178	21.678170
77.897934	2367.283716	21.683187
77.743436	2370.817270	21.688205
78.095076	2361.351394	21.693223
77.760065	2366.519451	21.698240
77.872385	2360.641326	21.703258
78.136579	2373.419866	21.708275
78.468008	2378.294806	21.713293
78.477136	2378.047254	21.718311
78.490367	2393.967223	21.723328
78.828516	2393.955640	21.728346
78.730354	2392.781150	21.733363
78.424969	2389.578059	21.738381
78.748534	2382.818075	21.743399
78.882789	2383.740851	21.748416
78.923765	2380.515395	21.753434
79.060667	2384.054078	21.758451
78.873659	2387.182418	21.763469
78.854420	2378.888343	21.768487
78.917064	2391.549943	21.773504
79.181227	2398.833919	21.778522
79.362740	2400.380538	21.783539
79.421732	2411.578338	21.788557
79.524719	2404.486593	21.793575
79.610359	2415.623439	21.798592
79.582925	2412.175085	21.803610
79.813884	2402.488121	21.808627
79.485020	2410.322051	21.813645
79.513620	2424.794207	21.818663
79.410426	2431.545218	21.823680
79.462379	2432.020035	21.828698
79.964048	2432.724654	21.833715
80.050679	2448.080942	21.838733
80.403633	2446.473272	21.843751
80.238728	2446.656784	21.848768
80.515739	2452.408118	21.853786
80.573942	2456.205237	21.858803
80.498521	2452.521334	21.863821
80.696785	2452.424226	21.868839
80.693424	2460.693524	21.873856
80.711003	2475.186373	21.878874
80.885968	2477.216887	21.883891
81.078040	2475.823624	21.888909
81.451400	2471.034672	21.893927
81.321433	2478.522064	21.898944
81.457948	2475.998131	21.903962
81.669453	2471.228067	21.908979
81.401204	2473.491700	21.913997
81.400346	2472.690244	21.919015
81.562769	2473.510803	21.924032
81.704783	2476.237614	21.929050
81.876492	2466.824946	21.934067
81.968264	2479.598846	21.939085
81.895382	2497.132411	21.944103
82.245493	2493.306502	21.949120
82.177599	2491.455062	21.954138
82.466767	2489.361825	21.959155
82.254275	2493.207409	21.964173
82.672912	2486.385244	21.969191
82.742269	2490.325810	21.974208
82.573716	2489.888156	21.979226
82.831527	2485.300240	21.984243
82.563593	2486.929467	21.989261
82.557037	2481.063499	21.994279
82.886181	2486.462723	21.999296
82.952677	2497.621537	22.004314
83.013354	2491.555737	22.009331
82.785704	2493.219721	22.014349
82.786186	2488.242651	22.019367
82.965647	2500.529511	22.024384
82.948577	2499.440225	22.029402
83.459900	2504.372404	22.034419
82.825229	2505.923022	22.039437
82.983120	2504.692879	22.044455
83.180619	2527.297122	22.049472
83.302813	2524.769100	22.054490
83.683209	2529.863691	22.059507
83.796197	2535.912007	22.064525
83.667079	2545.330779	22.069543
83.549316	2551.926303	22.074560
83.887975	2555.616658	22.079578
84.073611	2556.837578	22.084595
84.092719	2558.223291	22.089613
84.300984	2567.210823	22.094631
84.425965	2578.777177	22.099648
84.431442	2581.342213	22.104666
84.652891	2573.796425	22.109683
84.305914	2575.507399	22.114701
84.671813	2580.096141	22.119719
84.750652	2594.364938	22.124736
85.033282	2603.643889	22.129754
85.401790	2600.664066	22.134771
85.203124	2598.233329	22.139789
85.415945	2601.529845	22.144807
85.547226	2603.279977	22.149824
85.415523	2603.328924	22.154842
85.826839	2604.104426	22.159859
85.392045	2605.270458	22.164877
85.617372	2599.592427	22.169895
85.835072	2583.939374	22.174912
85.858175	2585.889397	22.179930
86.236438	2594.831539	22.184947
86.230419	2602.429082	22.189965
86.414373	2604.240446	22.194983
86.301784	2610.317596	22.200000
86.148569	2612.979932	22.205018
86.177287	2613.534116	22.210035
86.393150	2618.660662	22.215053
86.372788	2609.618674	22.220071
86.530142	2608.183465	22.225088
86.470434	2612.835324	22.230106
86.655610	2626.314363	22.235123
86.825023	2633.259709	22.240141
86.960801	2634.141233	22.245159
87.098812	2641.460729	22.250176
86.941581	2645.313522	22.255194
86.999074	2640.059270	22.260211
87.060163	2661.179490	22.265229
87.255829	2668.218600	22.270247
87.295492	2666.766994	22.275264
87.343692	2670.691958	22.280282
87.418133	2663.184801	22.285299
87.619109	2668.155876	22.290317
87.695386	2686.054596	22.295335
88.052821	2680.643172	22.300352
87.916389	2686.297993	22.305370
88.256464	2678.620075	22.310387
88.452377	2680.675756	22.315405
88.129047	2682.544016	22.320423
88.753722	2681.449485	22.325440
88.453717	2686.056719	22.330458
88.483320	2681.848292	22.335475
88.006630	2684.264334	22.340493
87.934420	2687.621023	22.345511
88.355450	2703.190574	22.350528
88.885638	2701.851957	22.355546
88.967676	2694.545591	22.360563
89.096674	2707.493753	22.365581
89.261551	2720.310095	22.370599
89.736549	2725.017599	22.375616
89.461906	2734.272920	22.380634
89.541757	2734.762338	22.385651
89.381279	2730.779170	22.390669
89.535464	2730.556370	22.395687
89.743037	2723.407187	22.400704
89.943344	2726.513156	22.405722
89.785691	2717.520894	22.410739
89.998193	2721.893696	22.415757
89.812432	2722.080457	22.420775
89.660573	2731.004210	22.425792
90.302538	2739.813843	22.430810
90.395381	2749.598984	22.435827
90.321882	2752.324675	22.440845
90.306142	2752.851068	22.445863
90.812669	2746.248670	22.450880
90.597755	2747.437285	22.455898
90.661418	2745.880942	22.460915
91.007874	2758.164072	22.465933
91.090314	2769.513092	22.470951
91.325349	2770.729492	22.475968
90.821183	2770.142096	22.480986
91.227767	2767.576073	22.486003
91.465368	2759.172401	22.491021
91.108253	2772.581333	22.496039
91.508680	2762.233422	22.501056
91.450170	2761.920651	22.506074
91.395583	2776.854203	22.511091
92.013967	2780.879781	22.516109
91.875747	2779.629444	22.521127
92.141385	2778.868541	22.526144
92.554907	2771.412696	22.531162
92.892692	2770.255521	22.536179
92.897553	2766.997745	22.541197
92.688944	2772.676456	22.546215
92.700225	2764.917137	22.551232
92.723168	2772.106267	22.556250
92.732779	2769.396907	22.561267
92.620019	2774.312708	22.566285
92.584393	2775.482879	22.571303
92.778325	2763.977282	22.576320
92.665107	2768.953118	22.581338
93.291719	2779.409470	22.586355
93.153866	2788.113302	22.591373
92.896093	2791.628301	22.596391
93.218427	2791.013217	22.601408
93.342561	2796.375020	22.606426
93.085453	2788.938367	22.611443
93.609592	2809.560599	22.616461
93.527402	2816.194866	22.621479
94.008641	2824.051183	22.626496
93.663532	2826.481474	22.631514
93.819773	2818.731123	22.636531
93.918470	2821.729841	22.641549
93.750278	2836.160378	22.646567
94.405985	2840.177003	22.651584
94.520656	2840.092909	22.656602
94.728523	2847.546792	22.661619
94.892873	2839.618430	22.666637
94.528480	2841.912857	22.671655
95.134057	2835.010958	22.676672
94.743681	2836.671904	22.681690
94.823122	2839.055032	22.686707
94.965958	2835.668456	22.691725
94.866545	2838.903167	22.696743
94.958955	2848.274982	22.701760
95.043180	2849.003584	22.706778
95.010341	2852.938049	22.711795
95.173092	2862.747084	22.716813
95.343858	2875.127081	22.721831
95.572321	2883.511973	22.726848
95.495522	2889.627830	22.731866
95.899650	2890.284534	22.736883
96.089091	2885.628259	22.741901
95.889586	2881.004138	22.746919
96.387080	2871.114464	22.751936
96.536193	2881.904018	22.756954
96.428759	2887.494422	22.761971
96.854640	2895.750744	22.766989
96.661777	2904.141277	22.772007
97.209877	2898.027857	22.777024
96.952211	2902.600148	22.782042
96.748771	2888.738778	22.787059
96.932526	2896.098597	22.792077
97.062220	2897.830068	22.797095
96.980453	2890.574375	22.802112
97.219066	2896.196120	22.807130
97.001830	2897.523974	22.812147
97.241342	2897.073274	22.817165
97.603252	2922.303528	22.822183
97.726713	2916.189937	22.827200
97.460677	2921.678802	22.832218
97.591657	2923.832992	22.837235
97.590996	2923.921502	22.842253
97.580849	2938.491632	22.847271
97.963879	2940.085826	22.852288
98.045265	2946.707298	22.857306
98.089547	2949.493583	22.862323
98.317170	2960.848525	22.867341
98.369428	2965.214775	22.872359
98.699711	2975.445954	22.877376
98.392478	2970.529283	22.882394
98.728855	2973.705637	22.887411
98.641256	2965.068451	22.892429
98.692537	2986.357853	22.897447
98.887389	2990.771342	22.902464
98.786049	3001.278039	22.907482
99.069630	2996.294625	22.912499
99.551050	3007.878351	22.917517
99.334688	3022.635304	22.922535
99.798612	3025.592973	22.927552
99.828635	3017.982120	22.932570
99.496681	3020.596598	22.937587
99.864144	3014.845810	22.942605
100.066246	3015.666530	22.947623
100.218032	3024.748300	22.952640
100.198486	3038.445732	22.957658
100.410885	3040.483108	22.962675
100.720751	3035.748079	22.967693
100.491096	3038.173046	22.972711
100.692761	3036.661471	22.977728
100.876669	3031.321144	22.982746
100.614331	3033.681765	22.987763
100.536394	3035.227805	22.992781
100.776557	3054.436410	22.997799
101.335230	3053.715087	23.002816
101.344825	3053.603167	23.007834
101.211339	3061.473238	23.012851
101.485556	3047.856144	23.017869
101.718877	3059.156608	23.022887
101.653068	3049.701712	23.027904
101.901720	3049.369518	23.032922
101.851257	3052.628206	23.037939
101.934941	3047.814769	23.042957
101.845003	3054.115782	23.047975
101.704793	3076.501871	23.052992
102.333285	3075.561374	23.058010
101.908421	3078.600620	23.063027
101.826689	3079.396099	23.068045
102.121718	3087.874874	23.073063
102.842724	3090.928242	23.078080
102.946553	3101.633451	23.083098
102.789837	3107.209503	23.088115
103.235344	3096.343091	23.093133
102.924745	3102.419675	23.098151
103.228474	3091.793112	23.103168
103.285250	3089.051111	23.108186
103.067958	3104.161761	23.113203
103.456706	3112.518648	23.118221
103.346860	3125.491673	23.123239
103.462116	3123.179263	23.128256
103.357211	3125.629005	23.133274
103.317518	3134.289317	23.138291
103.475459	3141.757408	23.143309
103.568498	3149.453380	23.148327
103.775167	3147.136203	23.153344
103.872327	3159.205932	23.158362
103.612253	3174.137089	23.163379
104.434978	3167.488464	23.168397
104.745415	3188.567326	23.173415
104.935807	3192.290366	23.178432
104.938641	3189.237978	23.183450
104.906541	3194.898809	23.188467
104.985423	3184.297730	23.193485
104.988183	3187.166264	23.198503
105.194969	3185.470823	23.203520
105.211966	3190.656900	23.208538
105.393809	3214.687864	23.213555
105.658538	3214.498346	23.218573
105.548803	3211.425608	23.223591
105.642229	3213.645646	23.228608
105.646026	3201.181500	23.233626
105.860586	3217.727330	23.238643
106.509910	3223.259984	23.243661
106.723210	3235.696731	23.248679
106.740123	3226.083680	23.253696
106.854351	3216.635383	23.258714
106.386332	3211.667932	23.263731
106.284912	3219.760322	23.268749
106.789041	3223.384024	23.273767
106.808643	3230.201432	23.278784
106.914786	3228.158700	23.283802
107.108893	3230.871204	23.288819
107.141919	3232.437858	23.293837
107.686586	3235.603922	23.298855
107.403282	3258.495406	23.303872
107.476437	3254.002324	23.308890
107.129354	3260.119358	23.313907
107.442704	3255.708813	23.318925
107.569022	3251.163269	23.323943
107.348227	3266.855331	23.328960
107.657815	3269.114313	23.333978
107.767767	3277.202225	23.338995
107.847539	3277.224560	23.344013
108.509526	3284.601610	23.349031
108.854293	3286.855116	23.354048
108.775577	3296.152812	23.359066
108.879350	3296.499650	23.364083
108.580667	3293.052328	23.369101
109.209380	3294.920763	23.374119
109.040096	3296.755633	23.379136
109.172841	3291.760904	23.384154
109.116712	3298.864714	23.389171
109.192132	3292.408142	23.394189
109.148880	3294.071894	23.399207
108.802336	3295.896488	23.404224
109.478055	3305.322909	23.409242
109.482096	3313.755567	23.414259
109.383107	3317.624684	23.419277
109.491191	3330.305121	23.424295
109.531254	3340.038834	23.429312
109.939208	3341.869053	23.434330
109.847912	3351.307607	23.439347
109.978732	3357.646948	23.444365
110.385438	3373.310840	23.449383
110.362612	3376.457975	23.454400
110.621162	3370.039143	23.459418
110.681844	3376.168478	23.464435
110.936255	3393.210096	23.469453
111.014163	3402.521335	23.474471
110.945036	3397.128768	23.479488
111.501763	3402.284529	23.484506
111.596057	3406.836868	23.489523
111.164354	3395.500866	23.494541
111.679634	3409.992728	23.499559
111.598042	3414.348365	23.504576
112.092787	3421.798852	23.509594
111.676917	3426.266504	23.514611
112.038524	3420.727963	23.519629
112.306169	3434.826004	23.524647
112.083339	3422.075059	23.529664
112.405040	3428.564608	23.534682
112.048295	3443.507883	23.539699
112.321514	3440.899408	23.544717
112.491004	3444.531069	23.549735
112.674566	3466.848296	23.554752
112.929373	3471.555563	23.559770
112.649595	3470.914267	23.564787
113.207791	3469.078871	23.569805
113.656922	3474.746926	23.574823
113.111547	3487.175720	23.579840
113.458151	3492.831338	23.584858
113.530819	3492.952621	23.589875
113.758993	3481.217146	23.594893
114.297490	3485.640378	23.599911
114.242165	3489.849915	23.604928
114.008445	3484.760691	23.609946
114.341316	3495.004389	23.614963
114.335277	3501.358776	23.619981
115.029453	3503.207573	23.624999
114.795284	3501.154670	23.630016
115.042173	3506.308202	23.635034
115.028436	3513.301342	23.640051
114.878599	3511.086968	23.645069
115.510712	3496.362803	23.650087
114.965977	3503.223991	23.655104
115.329700	3496.671960	23.660122
115.248473	3498.155428	23.665139
115.313479	3502.911191	23.670157
115.336324	3515.434595	23.675175
115.153967	3518.385659	23.680192
115.583235	3516.103215	23.685210
115.725875	3526.824727	23.690227
115.915919	3539.176931	23.695245
116.311973	3537.679236	23.700263
115.795241	3550.756947	23.705280
116.205747	3554.994970	23.710298
116.354293	3554.119706	23.715315
116.286510	3551.595869	23.720333
116.365156	3561.787655	23.725351
116.391702	3579.739194	23.730368
116.617665	3576.497348	23.735386
116.639296	3586.956834	23.740403
116.987659	3595.736854	23.745421
117.271426	3597.491748	23.750439
117.129321	3605.685332	23.755456
117.161612	3608.296838	23.760474
117.628331	3624.999469	23.765491
117.369833	3623.909828	23.770509
117.629985	3625.851462	23.775527
117.802811	3629.236457	23.780544
117.993575	3631.387737	23.785562
118.232622	3647.314688	23.790579
118.480311	3648.311401	23.795597
118.646137	3639.394562	23.800615
118.839937	3648.091361	23.805632
118.632663	3645.911162	23.810650
118.811802	3645.226815	23.815667
118.867128	3658.010384	23.820685
119.090996	3657.678882	23.825703
119.122649	3664.990104	23.830720
119.209256	3661.189196	23.835738
119.278879	3660.133685	23.840755
119.714547	3682.493990	23.845773
119.927084	3678.095882	23.850791
120.033468	3684.780015	23.855808
119.863777	3691.472414	23.860826
120.156258	3687.999256	23.865843
120.006611	3691.383970	23.870861
120.379450	3690.142375	23.875879
120.347379	3699.376204	23.880896
120.247755	3703.005630	23.885914
120.793934	3705.789640	23.890931
120.633337	3706.695268	23.895949
120.824628	3703.733389	23.900967
120.849131	3712.087298	23.905984
120.738026	3728.416022	23.911002
121.413048	3727.133690	23.916019
121.534885	3733.278875	23.921037
121.329700	3728.627012	23.926055
121.050788	3737.990823	23.931072
121.336688	3748.324040	23.936090
121.839228	3753.280028	23.941107
121.727533	3755.604663	23.946125
122.035767	3771.953356	23.951143
122.012926	3777.909614	23.956160
122.049256	3782.710947	23.961178
122.468526	3775.007610	23.966195
122.789937	3770.349499	23.971213
123.313210	3772.982431	23.976231
123.639424	3779.679716	23.981248
123.571302	3763.713486	23.986266
123.907017	3741.570772	23.991283
123.374616	3756.648965	23.996301
123.780862	3743.566289	24.001319
123.708415	3741.810116	24.006336
123.252701	3739.094151	24.011354
124.050930	3757.869436	24.016371
123.723315	3768.613807	24.021389
123.701858	3774.582474	24.026407
123.793726	3773.520337	24.031424
124.133441	3772.249176	24.036442
124.241601	3771.749469	24.041459
124.312913	3786.566413	24.046477
124.608755	3787.290512	24.051495
124.568738	3795.307319	24.056512
124.890552	3796.693342	24.061530
124.738074	3802.098512	24.066547
124.646040	3803.375375	24.071565
125.138215	3807.695432	24.076583
125.282367	3819.897162	24.081600
125.268422	3822.815741	24.086618
125.235786	3816.284274	24.091635
125.219232	3830.622560	24.096653
125.394788	3840.537448	24.101671
125.681069	3845.202038	24.106688
125.809576	3855.761822	24.111706
126.422866	3867.420261	24.116723
126.288867	3869.653695	24.121741
126.596956	3867.487919	24.126759
126.649760	3872.274085	24.131776
126.490986	3879.362542	24.136794
126.498195	3869.270909	24.141811
126.771575	3882.847626	24.146829
126.814551	3887.831015	24.151847
127.052709	3898.288533	24.156864
127.085980	3905.145099	24.161882
127.509361	3898.012353	24.166899
127.215241	3920.451857	24.171917
127.325396	3924.733575	24.176935
127.594227	3929.233622	24.181952
127.869507	3947.781211	24.186970
128.133627	3943.741135	24.191987
127.970768	3954.718780	24.197005
128.232594	3944.574837	24.202023
128.485089	3947.960114	24.207040
128.327666	3966.029055	24.212058
128.844400	3964.020159	24.217075
128.622849	3962.785869	24.222093
129.162006	3961.909739	24.227111
129.131235	3970.894160	24.232128
129.362413	3979.705237	24.237146
129.381270	3989.515196	24.242163
129.644853	3988.691439	24.247181
129.982180	3984.946116	24.252199
129.800802	3987.622507	24.257216
129.725729	3990.686350	24.262234
130.182296	3990.116612	24.267251
130.172014	4001.534503	24.272269
130.452910	4006.291506	24.277287
130.504917	4004.976746	24.282304
130.553734	4005.549938	24.287322
130.740370	4012.347949	24.292339
130.522970	4020.556599	24.297357
130.637306	4030.168651	24.302375
131.218922	4029.500535	24.307392
130.955952	4035.181792	24.312410
131.262711	4029.702107	24.317427
131.286837	4048.863345	24.322445
131.760631	4055.121127	24.327463
131.901773	4052.823506	24.332480
132.000234	4053.767725	24.337498
132.076307	4049.232960	24.342515
131.773746	4051.543161	24.347533
132.149199	4067.575498	24.352551
132.395043	4079.139781	24.357568
132.555913	4077.593440	24.362586
132.678595	4069.658401	24.367603
132.584931	4073.975044	24.372621
132.817860	4078.010431	24.377639
133.304705	4088.113711	24.382656
133.142513	4095.609947	24.387674
133.602840	4097.801378	24.392691
133.185635	4098.857447	24.397709
133.115416	4097.770026	24.402727
133.491622	4108.452364	24.407744
133.709898	4122.975261	24.412762
133.819477	4114.944397	24.417779
133.683338	4124.226209	24.422797
134.047026	4131.716335	24.427815
134.350059	4148.242933	24.432832
134.308512	4153.754032	24.437850
134.541044	4148.749844	24.442867
134.677045	4155.243318	24.447885
134.818287	4160.448206	24.452903
135.235127	4173.914430	24.457920
134.973239	4174.640160	24.462938
135.333728	4174.205315	24.467955
135.106358	4177.750566	24.472973
135.178071	4193.271638	24.477991
135.391693	4198.929246	24.483008
135.178072	4202.349265	24.488026
135.847562	4219.077691	24.493043
136.339456	4222.520437	24.498061
135.911290	4225.383632	24.503079
136.272424	4224.945529	24.508096
136.377368	4244.365835	24.513114
136.808943	4235.211637	24.518131
136.870638	4243.610503	24.523149
137.203130	4238.439224	24.528167
137.285823	4239.486910	24.533184
137.118612	4236.056811	24.538202
137.685109	4244.923127	24.543219
137.707514	4252.557972	24.548237
137.919841	4258.673467	24.553255
137.849675	4255.979460	24.558272
137.933832	4270.567546	24.563290
138.372891	4263.990886	24.568307
138.047279	4262.554990	24.573325
137.950138	4270.183204	24.578343
138.256437	4276.126257	24.583360
138.181983	4286.714736	24.588378
138.142897	4291.152343	24.593395
138.886058	4295.079933	24.598413
138.905041	4313.838242	24.603431
139.088622	4302.380623	24.608448
139.453095	4330.563622	24.613466
139.427337	4327.379771	24.618483
140.160939	4324.342827	24.623501
140.061542	4332.204987	24.628519
140.168855	4332.563921	24.633536
139.883543	4326.870162	24.638554
140.048490	4324.666648	24.643571
140.192394	4343.591763	24.648589
140.450274	4349.498191	24.653607
140.770893	4356.108185	24.658624
140.410879	4353.105781	24.663642
140.601218	4351.232882	24.668659
141.203711	4366.403176	24.673677
140.954104	4379.761839	24.678695
141.027070	4367.544940	24.683712
141.043977	4384.895918	24.688730
141.505156	4382.425332	24.693747
141.357277	4398.709885	24.698765
141.414346	4402.034139	24.703783
141.508021	4403.149564	24.708800
141.886713	4429.209438	24.713818
142.010743	4425.007998	24.718835
142.253344	4417.634905	24.723853
142.272357	4440.184118	24.728871
142.179702	4449.743398	24.733888
142.476240	4452.979877	24.738906
142.682515	4456.665987	24.743923
142.712317	4469.185813	24.748941
142.998181	4483.720572	24.753959
143.214149	4477.860342	24.758976
143.245620	4493.028111	24.763994
143.894277	4496.515944	24.769011
143.862804	4494.068386	24.774029
143.634483	4503.771915	24.779047
143.996735	4507.329591	24.784064
144.187763	4526.755736	24.789082
144.349843	4525.587933	24.794099
144.463727	4528.849707	24.799117
144.409863	4535.679046	24.804135
144.794447	4535.852778	24.809152
144.676122	4549.699303	24.814170
144.877806	4547.600515	24.819187
145.386008	4544.781699	24.824205
145.180460	4557.698054	24.829223
145.706128	4566.785520	24.834240
145.604478	4573.158325	24.839258
145.466920	4577.134720	24.844275
145.823843	4578.739442	24.849293
145.866590	4590.177855	24.854311
146.521822	4591.013323	24.859328
146.517956	4594.517545	24.864346
146.337482	4603.907508	24.869363
147.025397	4604.397000	24.874381
147.089669	4618.556037	24.879399
147.343735	4610.508771	24.884416
147.491169	4615.968494	24.889434
147.197130	4611.238701	24.894451
147.646300	4619.129208	24.899469
147.623056	4634.870608	24.904487
148.180429	4633.600221	24.909504
147.862880	4635.038509	24.914522
147.836765	4630.642607	24.919539
148.008883	4639.346416	24.924557
147.901771	4657.285114	24.929575
148.453912	4651.937483	24.934592
148.570049	4654.119444	24.939610
148.849501	4669.090932	24.944627
148.858423	4672.255444	24.949645
148.895441	4683.391793	24.954663
149.233466	4675.965863	24.959680
149.589031	4689.495671	24.964698
149.363324	4694.385389	24.969715
149.727175	4691.772095	24.974733
149.635775	4690.902571	24.979751
149.876265	4693.759583	24.984768
150.488229	4714.641778	24.989786
149.825508	4710.891028	24.994803
150.453897	4717.317513	24.999821
150.310829	4725.675885	25.004839
151.019888	4734.381366	25.009856
151.193815	4745.035603	25.014874
150.875101	4743.447086	25.019891
151.113435	4751.474638	25.024909
151.061112	4750.087689	25.029927
151.413462	4771.979387	25.034944
151.668277	4774.849963	25.039962
151.683927	4784.449373	25.044979
151.960092	4779.911680	25.049997
152.073176	4797.188108	25.055015
152.487692	4787.146179	25.060032
152.811191	4790.605784	25.065050
152.922066	4791.339786	25.070067
153.007466	4787.841845	25.075085
152.596483	4796.687016	25.080103
152.906821	4791.178137	25.085120
153.268154	4792.116189	25.090138
153.147476	4810.445389	25.095155
153.661712	4806.937494	25.100173
153.419837	4801.164225	25.105191
153.802514	4810.747539	25.110208
153.789204	4812.820259	25.115226
154.050040	4825.900925	25.120243
154.211337	4823.963058	25.125261
154.096718	4834.236155	25.130279
154.577207	4825.721112	25.135296
154.694415	4845.231689	25.140314
154.743946	4852.089240	25.145331
155.242768	4860.808576	25.150349
154.707370	4860.106019	25.155367
155.449325	4867.004123	25.160384
155.530881	4873.121248	25.165402
155.917119	4888.852774	25.170419
155.558392	4885.143039	25.175437
155.570026	4885.665232	25.180455
155.648702	4894.336366	25.185472
156.031830	4909.658059	25.190490
156.111828	4914.187752	25.195507
156.203962	4920.751460	25.200525
155.994555	4931.954736	25.205543
156.242902	4940.286988	25.210560
156.945843	4956.139713	25.215578
156.692135	4962.047080	25.220595
157.400776	4976.983568	25.225613
157.323991	4987.086725	25.230631
157.893011	4994.021272	25.235648
158.416379	4979.331779	25.240666
158.336964	4982.074508	25.245683
158.589412	4984.352074	25.250701
158.443783	4994.185030	25.255719
158.786912	4997.758407	25.260736
159.078195	5001.933270	25.265754
158.726294	5003.809368	25.270771
159.072108	4998.376971	25.275789
158.690718	5008.754829	25.280807
158.959925	5019.864705	25.285824
159.299247	5027.845092	25.290842
159.091607	5038.287453	25.295859
159.543477	5045.540123	25.300877
159.519567	5058.759982	25.305895
159.714269	5061.460046	25.310912
159.979847	5077.264182	25.315930
160.267148	5079.138620	25.320947
160.119543	5088.858301	25.325965
160.296217	5099.382904	25.330983
160.441252	5108.804517	25.336000
160.970284	5113.387453	25.341018
160.939052	5132.908824	25.346035
161.304495	5132.930877	25.351053
161.515954	5142.118057	25.356071
161.753655	5151.866165	25.361088
161.668956	5152.769515	25.366106
161.594251	5159.564456	25.371123
161.979264	5171.994742	25.376141
162.429628	5183.770940	25.381159
162.293754	5175.159152	25.386176
162.560397	5174.508474	25.391194
162.428594	5196.681234	25.396211
162.810380	5201.669052	25.401229
162.949534	5204.889136	25.406247
163.382630	5201.583189	25.411264
163.595312	5209.185656	25.416282
163.490727	5223.762860	25.421299
163.793016	5228.185425	25.426317
163.723417	5229.256879	25.431335
163.801469	5234.904354	25.436352
164.479417	5241.339094	25.441370
164.139888	5258.875818	25.446387
164.207755	5251.526436	25.451405
164.150179	5258.284025	25.456423
164.355716	5286.594264	25.461440
164.860185	5279.580929	25.466458
164.603646	5297.332036	25.471475
165.072680	5309.853501	25.476493
164.834614	5315.042020	25.481511
165.265065	5346.552754	25.486528
165.813599	5338.680278	25.491546
165.577759	5358.666188	25.496563
166.003693	5359.430075	25.501581
166.435272	5359.599658	25.506599
166.451713	5362.914632	25.511616
167.099458	5377.583158	25.516634
167.363227	5376.276366	25.521651
167.865249	5377.593424	25.526669
167.949694	5378.587242	25.531687
167.740839	5380.532646	25.536704
167.944675	5376.744692	25.541722
167.811619	5373.612085	25.546739
168.005637	5375.343251	25.551757
168.325950	5380.735254	25.556775
168.005896	5390.324119	25.561792
168.329446	5386.889995	25.566810
168.193739	5403.602838	25.571827
168.763882	5415.414200	25.576845
168.568873	5422.606751	25.581863
168.477477	5434.757860	25.586880
169.174343	5442.745895	25.591898
169.053035	5458.465397	25.596915
168.861500	5463.627774	25.601933
169.218298	5471.343645	25.606951
169.619004	5486.003373	25.611968
169.733395	5497.049261	25.616986
170.012815	5515.143270	25.622003
170.133750	5523.798655	25.627021
170.486502	5521.003894	25.632039
170.727916	5531.262987	25.637056
171.295266	5541.619700	25.642074
171.179266	5546.079057	25.647091
171.374800	5548.207729	25.652109
171.789739	5544.677276	25.657127
172.382423	5553.783216	25.662144
172.605540	5557.861498	25.667162
172.747824	5566.387317	25.672180
172.632980	5560.404634	25.677197
173.177453	5558.558549	25.682215
172.971874	5553.940997	25.687232
173.276209	5547.668942	25.692250
173.346808	5551.546853	25.697268
173.166719	5549.636808	25.702285
173.462540	5549.483466	25.707303
173.394939	5545.485214	25.712320
173.943184	5548.076647	25.717338
173.976682	5550.221077	25.722356
173.675565	5566.410583	25.727373
173.661930	5568.915887	25.732391
173.837092	5585.700447	25.737408
174.140325	5589.763107	25.742426
174.225450	5602.022576	25.747444
173.950747	5611.156265	25.752461
174.590976	5622.511776	25.757479
174.537487	5627.507505	25.762496
174.798277	5639.452403	25.767514
174.996817	5663.386167	25.772532
175.144425	5666.188350	25.777549
175.590345	5682.637285	25.782567
175.485870	5700.406145	25.787584
175.867843	5692.663616	25.792602
176.016364	5715.674048	25.797620
176.103726	5720.038654	25.802637
176.500845	5720.510325	25.807655
176.597894	5733.522448	25.812672
177.210691	5729.812797	25.817690
177.511208	5741.672663	25.822708
177.365686	5749.337438	25.827725
177.382358	5755.401830	25.832743
177.195751	5762.883613	25.837760
177.395630	5773.449186	25.842778
177.782029	5784.885353	25.847796
178.106260	5785.895524	25.852813
178.686746	5796.976353	25.857831
178.581050	5816.970913	25.862848
178.843644	5811.415499	25.867866
179.036253	5809.785157	25.872884
179.305623	5827.259193	25.877901
179.356415	5833.106806	25.882919
179.318914	5833.289451	25.887936
179.653999	5847.678751	25.892954
179.776625	5861.734975	25.897972
179.691960	5860.627600	25.902989
180.233524	5866.136818	25.908007
180.266781	5886.734828	25.913024
180.503601	5885.886747	25.918042
180.494716	5889.373060	25.923060
180.576728	5901.661625	25.928077
181.347970	5905.376867	25.933095
181.473048	5921.803368	25.938112
181.498183	5924.204829	25.943130
181.987344	5932.493732	25.948148
182.056407	5935.813244	25.953165
182.402803	5939.784034	25.958183
182.466455	5956.920898	25.963200
182.638104	5954.220557	25.968218
182.582334	5949.655339	25.973236
182.791332	5957.182935	25.978253
182.953586	5963.433067	25.983271
182.951433	5977.628758	25.988288
183.223835	5981.134427	25.993306
183.419009	6003.904369	25.998324
183.334444	6010.079306	26.003341
183.921404	6010.171044	26.008359
184.140598	6022.763465	26.013376
183.942856	6030.897357	26.018394
184.320283	6028.644774	26.023412
184.488712	6053.780102	26.028429
185.014363	6059.269760	26.033447
185.012392	6066.041088	26.038464
185.105104	6087.738047	26.043482
185.095637	6093.244739	26.048500
185.178755	6098.190919	26.053517
185.577239	6107.093781	26.058535
185.788957	6113.465686	26.063552
186.065076	6118.530186	26.068570
186.112856	6136.821866	26.073588
186.082227	6143.367248	26.078605
186.596973	6134.094984	26.083623
186.595985	6140.399002	26.088640
186.761183	6150.181030	26.093658
186.744698	6159.669372	26.098676
187.058713	6176.224519	26.103693
187.443102	6175.034628	26.108711
187.684961	6184.018733	26.113728
187.823127	6202.302720	26.118746
187.998710	6202.868872	26.123764
188.063109	6207.606500	26.128781
188.801903	6217.876931	26.133799
188.923980	6225.771717	26.138816
188.918366	6231.486190	26.143834
188.949193	6221.863073	26.148852
188.832182	6235.597034	26.153869
189.404435	6247.165546	26.158887
189.276662	6255.468574	26.163904
189.646757	6264.906254	26.168922
190.169006	6272.094796	26.173940
190.021802	6278.399529	26.178957
190.341876	6286.055174	26.183975
190.280273	6295.932568	26.188992
190.466851	6312.163602	26.194010
190.582343	6327.667054	26.199028
190.900396	6332.519900	26.204045
191.491195	6336.316989	26.209063
191.672130	6344.584621	26.214080
191.941041	6344.615396	26.219098
192.547003	6349.966372	26.224116
192.761360	6364.766306	26.229133
193.169768	6372.465055	26.234151
192.955996	6369.641571	26.239168
192.865736	6369.018010	26.244186
193.061390	6362.822574	26.249204
193.063203	6369.729162	26.254221
193.136760	6383.534579	26.259239
193.430032	6386.831893	26.264256
193.539093	6391.669943	26.269274
194.040331	6407.741588	26.274292
193.895828	6419.977380	26.279309
194.080120	6425.599214	26.284327
194.444647	6439.132090	26.289344
194.523767	6446.948428	26.294362
194.830503	6451.986157	26.299380
194.940559	6468.955286	26.304397
194.740336	6468.980182	26.309415
195.304664	6486.165861	26.314432
195.102698	6510.639754	26.319450
195.756135	6519.042245	26.324468
195.649242	6529.217234	26.329485
195.936307	6541.086028	26.334503
196.094893	6546.566693	26.339520
196.344359	6559.827153	26.344538
197.182538	6567.140246	26.349556
197.267736	6580.344221	26.354573
197.670317	6573.832393	26.359591
197.615313	6573.073910	26.364608
197.462324	6589.010816	26.369626
197.724431	6593.253725	26.374644
197.906049	6601.663420	26.379661
198.127231	6608.387578	26.384679
198.244925	6630.194935	26.389696
197.982263	6632.079398	26.394714
198.513080	6643.998699	26.399732
198.984805	6663.929540	26.404749
199.328511	6674.413265	26.409767
199.424820	6685.506883	26.414784
199.222114	6695.194959	26.419802
199.803981	6688.026985	26.424820
199.979862	6704.490475	26.429837
199.948881	6706.815544	26.434855
199.789540	6716.840965	26.439872
200.458307	6736.545490	26.444890
200.483855	6740.266517	26.449908
200.307957	6747.036764	26.454925
200.690974	6757.201898	26.459943
200.781375	6769.846454	26.464960
200.953838	6792.507272	26.469978
201.212965	6796.513934	26.474996
201.565644	6812.378622	26.480013
201.992774	6824.175286	26.485031
202.372788	6840.566079	26.490048
202.323613	6843.550606	26.495066
202.778486	6856.129007	26.500084
203.379308	6869.691706	26.505101
203.128660	6876.202155	26.510119
203.322498	6876.655001	26.515136
203.803171	6898.826016	26.520154
203.938322	6901.128402	26.525172
203.628678	6907.963726	26.530189
204.049505	6921.466096	26.535207
204.236247	6924.347615	26.540224
204.424911	6934.508381	26.545242
204.716885	6953.059596	26.550260
204.910988	6957.691992	26.555277
205.162256	6968.657482	26.560295
205.430940	6978.379648	26.565312
205.123890	6988.794402	26.570330
205.795713	6997.503618	26.575348
205.892659	7000.699025	26.580365
206.101964	7007.450434	26.585383
206.593951	7018.132247	26.590400
206.912933	7019.897782	26.595418
207.303905	7031.081477	26.600436
207.174083	7039.394648	26.605453
207.127300	7046.362723	26.610471
207.294410	7052.145265	26.615488
207.634006	7059.324675	26.620506
207.902311	7066.388915	26.625524
208.075502	7088.462819	26.630541
208.440238	7093.289660	26.635559
208.465077	7103.349754	26.640576
208.753806	7118.347068	26.645594
208.607703	7122.423206	26.650612
209.050207	7140.730199	26.655629
209.202258	7147.108598	26.660647
209.757765	7154.424899	26.665664
209.493284	7181.737934	26.670682
209.975985	7177.205379	26.675700
210.251481	7194.285166	26.680717
210.319422	7204.790031	26.685735
210.786691	7204.597360	26.690752
210.428061	7227.442419	26.695770
210.794360	7238.993118	26.700788
210.992861	7246.396606	26.705805
211.107344	7260.092136	26.710823
211.307002	7265.396152	26.715840
211.606001	7290.885357	26.720858
211.877743	7299.859045	26.725876
212.184526	7302.077937	26.730893
212.384665	7315.195096	26.735911
212.777934	7325.444185	26.740928
212.738588	7345.777337	26.745946
213.231157	7347.626369	26.750964
213.288408	7368.174957	26.755981
213.389773	7359.117966	26.760999
213.872507	7368.658642	26.766016
213.945683	7385.384969	26.771034
214.179334	7382.829453	26.776052
214.630775	7383.930402	26.781069
214.764580	7403.703150	26.786087
215.231362	7410.282033	26.791104
215.174347	7412.251362	26.796122
215.350957	7412.097628	26.801140
215.277869	7420.111707	26.806157
215.240665	7439.797470	26.811175
215.926410	7446.837906	26.816192
216.214112	7460.061498	26.821210
216.271932	7465.138261	26.826228
216.431902	7478.583792	26.831245
216.332240	7490.535511	26.836263
216.675643	7498.907803	26.841280
217.123682	7511.102579	26.846298
217.327656	7522.123118	26.851316
217.581434	7533.877778	26.856333
217.724831	7552.657930	26.861351
217.736184	7562.306821	26.866368
217.756051	7571.831273	26.871386
218.346734	7592.716930	26.876404
219.005902	7593.239408	26.881421
218.575958	7602.925456	26.886439
219.395245	7619.333794	26.891456
219.194720	7626.758520	26.896474
219.763134	7633.994082	26.901492
220.389335	7639.699022	26.906509
220.131835	7645.961413	26.911527
220.710773	7654.192928	26.916544
220.465485	7657.855287	26.921562
221.085016	7668.773333	26.926580
221.260399	7678.999718	26.931597
221.283295	7690.812523	26.936615
221.924415	7691.293618	26.941632
221.701166	7689.813093	26.946650
222.070366	7714.007092	26.951668
222.430618	7712.022164	26.956685
222.360931	7721.573264	26.961703
222.847310	7724.727108	26.966720
222.697619	7733.602461	26.971738
222.713437	7750.584290	26.976756
223.163902	7764.161591	26.981773
223.203313	7771.400645	26.986791
223.668214	7784.350642	26.991808
223.783303	7797.279343	26.996826
224.046015	7815.577118	27.001844
224.417670	7818.821450	27.006861
224.508484	7816.114481	27.011879
224.830356	7827.994476	27.016896
225.282752	7841.571535	27.021914
225.151668	7857.304085	27.026932
225.549772	7860.291751	27.031949
225.528966	7878.845245	27.036967
225.614675	7887.630354	27.041984
225.940745	7899.891734	27.047002
226.045035	7913.453588	27.052020
226.578604	7921.310296	27.057037
226.406676	7944.913258	27.062055
227.186153	7944.728801	27.067072
227.259297	7957.465257	27.072090
227.405387	7975.793976	27.077108
227.649930	7970.957355	27.082125
227.844475	7988.233587	27.087143
228.077081	8001.494560	27.092160
228.036376	8017.266844	27.097178
228.350405	8029.653307	27.102196
228.945542	8028.645166	27.107213
228.574866	8056.901023	27.112231
228.988562	8064.021938	27.117248
228.967960	8071.254667	27.122266
229.004965	8092.722740	27.127284
229.894057	8103.343364	27.132301
229.678074	8116.412228	27.137319
230.116481	8132.956093	27.142336
230.445508	8147.449170	27.147354
230.773855	8158.381273	27.152372
230.893925	8164.139920	27.157389
230.829739	8177.873421	27.162407
231.214820	8196.446124	27.167424
231.478203	8207.644088	27.172442
231.529549	8224.396675	27.177460
232.042845	8228.967070	27.182477
231.728742	8250.407907	27.187495
232.165967	8264.404366	27.192512
232.541174	8281.119211	27.197530
233.010851	8298.258189	27.202548
233.456530	8307.549405	27.207565
233.955121	8326.136138	27.212583
234.002683	8328.417613	27.217600
234.544622	8341.832721	27.222618
234.711918	8360.130107	27.227636
235.122287	8353.818493	27.232653
235.095927	8351.596929	27.237671
235.299934	8360.878442	27.242688
235.667373	8373.455714	27.247706
235.887109	8373.961394	27.252724
236.004391	8384.017266	27.257741
236.237294	8403.980867	27.262759
236.278892	8399.147317	27.267776
236.811962	8413.409944	27.272794
236.853911	8428.203658	27.277812
236.910307	8432.718956	27.282829
237.020167	8456.335527	27.287847
237.401051	8466.637696	27.292864
237.355619	8480.520040	27.297882
237.636428	8497.540227	27.302900
238.223303	8505.410986	27.307917
238.346656	8510.604118	27.312935
238.529676	8531.481698	27.317952
238.995543	8538.509434	27.322970
239.309250	8552.433788	27.327988
239.583255	8564.665832	27.333005
239.291075	8569.838433	27.338023
239.857307	8586.908977	27.343040
239.940629	8597.488012	27.348058
240.359533	8610.505738	27.353076
240.860884	8619.756874	27.358093
240.724895	8637.362998	27.363111
241.121820	8643.628024	27.368128
241.237238	8649.074996	27.373146
241.411093	8659.614715	27.378164
241.907498	8666.779814	27.383181
242.433659	8688.687029	27.388199
242.396763	8688.705439	27.393216
243.125941	8688.250987	27.398234
242.773948	8714.392849	27.403252
242.887452	8708.903977	27.408269
243.476548	8728.629364	27.413287
244.014050	8726.793532	27.418304
244.035416	8733.540109	27.423322
243.912749	8745.682489	27.428340
244.356866	8758.364899	27.433357
244.131264	8759.612386	27.438375
244.743556	8769.329362	27.443392
245.230172	8780.897028	27.448410
245.291439	8791.725862	27.453428
245.517334	8802.402788	27.458445
245.418691	8813.572241	27.463463
245.438318	8823.368888	27.468480
245.883284	8834.359007	27.473498
245.463492	8847.801086	27.478516
246.113315	8869.341981	27.483533
246.530896	8886.745344	27.488551
246.363027	8903.052793	27.493568
247.347530	8919.452359	27.498586
247.277498	8929.461919	27.503604
248.024248	8946.113209	27.508621
248.241703	8956.987280	27.513639
248.200655	8965.521124	27.518656
249.196022	8974.761828	27.523674
248.728745	8984.296551	27.528692
249.141732	8996.560915	27.533709
249.444205	9008.378393	27.538727
249.702606	9023.173612	27.543744
250.340791	9032.713054	27.548762
250.025536	9045.485472	27.553780
250.156552	9055.908958	27.558797
250.162153	9063.374782	27.563815
250.443441	9086.750782	27.568832
250.703412	9101.403748	27.573850
250.727211	9123.187632	27.578868
251.312200	9137.480623	27.583885
252.076210	9146.605889	27.588903
252.258022	9158.158104	27.593920
252.521424	9146.479820	27.598938
253.342866	9166.579934	27.603956
253.810029	9161.032712	27.608973
254.182010	9160.318146	27.613991
254.304784	9169.044423	27.619008
254.777109	9159.382607	27.624026
254.902014	9165.560718	27.629044
255.028236	9168.887702	27.634061
255.043855	9181.997033	27.639079
254.825364	9188.042340	27.644096
255.348950	9187.780903	27.649114
255.058299	9215.101016	27.654132
255.637905	9222.209179	27.659149
255.300397	9220.408499	27.664167
255.519977	9244.596229	27.669184
255.945515	9259.608720	27.674202
256.128947	9288.900988	27.679220
256.474409	9295.439453	27.684237
256.709048	9318.188413	27.689255
256.623820	9337.397468	27.694272
256.840570	9358.046569	27.699290
257.554251	9376.926066	27.704308
258.072005	9391.554914	27.709325
258.320839	9397.259170	27.714343
258.262135	9420.770612	27.719360
258.508642	9433.698943	27.724378
259.017631	9448.528105	27.729396
259.527312	9468.181401	27.734413
259.870438	9476.409406	27.739431
259.476400	9481.080333	27.744448
260.000335	9495.342063	27.749466
260.116060	9510.469292	27.754484
260.373207	9530.155657	27.759501
260.814429	9547.420201	27.764519
261.062246	9557.948917	27.769536
261.162035	9573.062893	27.774554
261.368555	9591.285931	27.779572
261.662813	9613.151416	27.784589
261.881556	9619.128791	27.789607
261.834504	9641.590493	27.794624
262.260295	9653.985905	27.799642
262.645543	9677.917929	27.804660
262.670172	9696.762953	27.809677
262.684729	9706.646101	27.814695
263.109513	9727.051689	27.819712
263.517197	9737.359868	27.824730
263.767204	9757.852687	27.829748
263.966138	9776.487534	27.834765
264.516162	9790.600196	27.839783
264.894804	9818.123249	27.844800
265.300711	9826.215345	27.849818
265.103605	9846.822074	27.854836
265.235103	9855.875674	27.859853
266.258012	9874.417067	27.864871
266.298234	9888.612330	27.869888
266.555345	9897.902135	27.874906
266.638981	9906.808503	27.879924
266.738991	9927.264874	27.884941
267.441531	9943.462982	27.889959
268.025950	9955.789698	27.894976
268.213763	9974.631699	27.899994
268.550519	9988.569333	27.905012
268.955985	9991.995070	27.910029
269.688978	10002.303267	27.915047
269.426764	10009.943774	27.920064
269.627133	10004.961953	27.925082
270.591110	10014.290161	27.930100
270.693121	10023.686266	27.935117
271.097302	10018.776902	27.940135
271.033389	10014.821305	27.945152
271.497402	10021.865685	27.950170
271.410821	10033.283420	27.955188
271.648770	10041.960604	27.960205
271.511937	10039.598170	27.965223
272.048034	10067.696971	27.970240
272.417647	10066.439683	27.975258
272.582671	10083.144679	27.980276
272.878638	10089.643771	27.985293
273.451814	10106.727270	27.990311
272.982199	10128.737545	27.995328
273.603900	10127.314713	28.000346
273.761507	10144.516620	28.005364
273.812977	10145.850511	28.010381
274.225586	10172.036406	28.015399
274.548756	10194.548487	28.020416
274.916886	10210.176896	28.025434
275.203253	10218.764533	28.030452
275.279601	10235.404538	28.035469
275.728867	10246.710564	28.040487
275.858378	10259.326163	28.045504
276.193345	10273.658959	28.050522
276.555080	10278.329241	28.055540
276.710279	10301.849540	28.060557
277.093670	10316.500038	28.065575
277.146548	10330.002205	28.070592
277.488031	10337.299426	28.075610
277.576553	10356.561416	28.080628
277.893657	10377.518078	28.085645
278.303575	10384.921487	28.090663
278.394279	10405.382989	28.095680
278.705764	10414.895077	28.100698
278.693778	10441.055890	28.105716
279.024877	10459.708733	28.110733
279.881220	10473.161693	28.115751
279.675749	10485.428608	28.120768
280.094411	10507.241046	28.125786
280.197685	10514.550164	28.130804
280.237729	10542.379597	28.135821
280.747923	10544.857699	28.140839
280.603747	10577.928737	28.145856
281.032643	10599.610236	28.150874
281.592442	10612.676899	28.155892
281.877855	10631.324398	28.160909
282.248213	10648.733611	28.165927
282.582596	10673.461033	28.170944
282.940183	10687.307540	28.175962
283.476016	10683.681524	28.180980
283.732537	10704.900581	28.185997
284.798941	10721.620532	28.191015
284.339879	10727.605909	28.196032
284.865785	10734.640925	28.201050
285.266354	10751.354053	28.206068
285.456474	10757.484652	28.211085
285.790001	10773.447295	28.216103
285.970535	10787.836104	28.221120
286.002407	10791.560120	28.226138
286.681472	10803.269594	28.231156
286.362444	10820.473708	28.236173
286.744445	10826.173460	28.241191
286.891371	10847.637078	28.246208
287.186057	10864.448886	28.251226
287.618201	10886.726973	28.256244
287.601024	10907.218451	28.261261
287.979614	10924.667688	28.266279
287.925602	10943.703033	28.271296
288.450171	10967.558192	28.276314
289.038482	10982.931948	28.281332
289.099822	11003.490244	28.286349
289.415343	11026.582339	28.291367
289.932903	11033.426162	28.296384
290.073900	11059.049353	28.301402
290.635453	11081.077028	28.306420
290.814673	11097.032397	28.311437
291.024777	11103.873592	28.316455
291.545392	11131.799589	28.321472
291.961987	11145.599360	28.326490
291.990393	11165.676706	28.331508
292.195996	11181.950106	28.336525
292.735549	11197.906297	28.341543
292.813908	11216.532938	28.346560
293.177380	11225.926833	28.351578
293.436265	11241.159480	28.356596
293.922102	11264.812653	28.361613
294.307665	11269.839434	28.366631
294.499622	11287.299121	28.371648
294.668728	11297.591633	28.376666
295.050894	11318.832874	28.381684
295.547066	11336.807286	28.386701
295.845276	11344.244257	28.391719
296.323565	11361.387888	28.396736
296.453517	11362.876997	28.401754
296.978775	11375.984308	28.406772
297.115255	11395.239902	28.411789
296.864193	11396.554674	28.416807
297.360343	11412.656738	28.421824
297.701023	11436.402193	28.426842
297.975310	11449.952795	28.431860
298.467597	11472.288526	28.436877
298.303279	11488.682934	28.441895
298.523152	11503.400872	28.446912
299.112249	11532.892431	28.451930
299.527232	11546.525399	28.456948
299.496461	11566.805000	28.461965
299.722874	11570.157865	28.466983
300.049239	11586.583324	28.472000
300.167272	11609.561637	28.477018
300.325669	11622.874642	28.482036
300.627665	11649.082989	28.487053
301.295867	11673.207186	28.492071
302.031318	11688.912268	28.497088
301.852348	11713.199984	28.502106
302.521708	11707.405820	28.507124
302.992477	11731.488204	28.512141
303.257168	11732.997416	28.517159
303.514637	11756.869905	28.522176
303.752035	11771.225357	28.527194
303.834399	11783.138863	28.532212
304.282499	11800.338118	28.537229
304.628775	11819.766731	28.542247
304.530400	11830.770593	28.547264
304.608752	11854.986855	28.552282
305.428699	11868.471755	28.557300
305.373151	11888.645043	28.562317
306.025341	11911.221645	28.567335
306.116918	11939.171435	28.572352
306.159900	11959.642067	28.577370
306.731930	11970.443752	28.582388
307.265326	11989.379235	28.587405
307.739744	11998.269969	28.592423
307.856505	12019.092309	28.597440
308.172654	12039.495238	28.602458
308.761891	12054.212941	28.607476
309.263471	12081.350748	28.612493
309.486522	12089.096537	28.617511
310.106477	12102.322237	28.622528
309.711410	12119.119408	28.627546
310.276262	12130.812766	28.632564
310.265589	12150.710947	28.637581
310.618906	12166.996940	28.642599
310.928501	12178.467980	28.647616
310.990750	12208.569957	28.652634
311.704765	12226.122915	28.657652
311.770236	12249.994345	28.662669
311.964193	12263.918019	28.667687
312.372717	12286.030934	28.672704
312.901109	12305.586424	28.677722
313.370025	12316.947488	28.682740
313.688321	12338.212459	28.687757
314.010449	12361.447268	28.692775
314.231748	12376.775106	28.697792
314.563379	12393.421493	28.702810
315.058811	12410.197121	28.707828
315.011673	12433.240048	28.712845
315.586640	12449.782288	28.717863
316.313130	12457.190919	28.722880
316.202829	12475.980805	28.727898
316.689965	12487.092832	28.732916
316.695119	12508.087817	28.737933
317.076459	12527.006465	28.742951
317.426227	12544.635376	28.747968
317.857340	12565.264124	28.752986
318.309074	12571.837723	28.758004
318.655119	12584.503279	28.763021
319.006427	12598.418492	28.768039
319.414832	12609.454433	28.773056
319.451387	12619.878827	28.778074
319.873502	12634.323019	28.783092
319.793203	12646.192925	28.788109
320.604535	12657.131429	28.793127
320.846584	12674.859333	28.798144
321.549445	12690.819794	28.803162
321.840804	12686.353604	28.808180
321.846770	12698.232217	28.813197
321.957684	12719.637271	28.818215
322.327636	12731.168723	28.823232
322.702262	12751.550691	28.828250
322.774926	12755.691887	28.833268
322.853343	12761.600542	28.838285
323.193457	12791.710717	28.843303
323.446423	12801.526805	28.848320
323.754170	12823.801300	28.853338
324.405622	12843.486609	28.858356
324.769194	12857.084325	28.863373
325.092612	12885.056267	28.868391
325.533170	12896.677878	28.873408
325.329635	12925.312952	28.878426
325.872076	12933.757765	28.883444
326.205397	12950.704373	28.888461
326.446234	12974.726258	28.893479
326.868584	12987.231789	28.898496
327.098242	13010.064963	28.903514
327.617789	13030.910975	28.908532
327.780552	13051.594666	28.913549
328.031013	13071.784736	28.918567
328.651901	13086.690951	28.923584
328.864910	13109.428945	28.928602
329.169507	13126.677020	28.933620
329.659709	13149.921372	28.938637
329.592802	13168.610455	28.943655
330.624647	13190.744234	28.948672
330.594687	13202.972963	28.953690
330.721648	13215.843576	28.958708
331.380830	13249.874227	28.963725
331.497480	13273.091624	28.968743
331.730476	13281.338457	28.973760
332.095958	13321.329637	28.978778
332.127434	13332.285737	28.983796
332.863059	13356.660547	28.988813
332.910117	13385.904669	28.993831
333.617970	13397.753396	28.998848
333.523481	13426.002778	29.003866
334.010906	13446.690041	29.008884
334.427454	13464.198889	29.013901
334.649821	13489.215881	29.018919
335.130785	13507.201057	29.023936
335.297001	13535.337383	29.028954
335.557004	13559.158079	29.033972
336.155451	13587.312454	29.038989
336.314394	13606.232073	29.044007
337.301796	13627.195382	29.049024
337.482261	13643.323245	29.054042
338.205036	13651.907677	29.059060
338.491425	13668.135914	29.064077
338.359948	13696.069348	29.069095
339.295669	13701.595354	29.074112
339.704595	13709.751826	29.079130
340.130557	13719.162507	29.084148
340.436290	13740.383647	29.089165
340.736830	13754.863416	29.094183
340.958243	13771.954502	29.099200
340.402658	13779.961158	29.104218
341.063743	13809.186130	29.109236
341.367746	13820.381142	29.114253
341.389126	13848.748907	29.119271
342.023845	13856.421860	29.124288
342.024526	13886.150825	29.129306
342.606372	13921.858973	29.134324
343.187289	13936.089963	29.139341
342.981448	13959.667889	29.144359
343.798208	13975.150645	29.149376
343.796733	13997.847307	29.154394
343.989927	14010.581830	29.159412
344.620867	14032.036887	29.164429
344.879603	14048.569764	29.169447
345.141912	14064.593662	29.174464
345.872355	14099.435827	29.179482
345.524717	14110.934573	29.184500
346.293781	14131.269255	29.189517
346.937058	14159.752252	29.194535
347.210569	14188.062323	29.199552
347.431457	14204.721233	29.204570
347.486256	14223.417673	29.209588
348.348817	14248.178099	29.214605
348.485688	14257.097191	29.219623
348.849484	14278.047778	29.224640
349.370865	14309.265881	29.229658
349.595105	14322.864240	29.234676
349.764542	14337.093273	29.239693
350.292650	14371.774799	29.244711
350.608413	14394.378333	29.249728
350.826922	14409.594566	29.254746
351.069390	14439.839413	29.259764
351.447599	14448.032568	29.264781
351.887024	14465.254556	29.269799
353.163874	14479.788158	29.274816
353.582477	14486.421275	29.279834
354.216062	14503.723604	29.284852
354.878987	14507.738552	29.289869
354.653020	14515.451027	29.294887
355.196109	14526.407120	29.299904
355.710849	14539.894089	29.304922
355.546894	14555.684748	29.309940
356.062612	14556.084524	29.314957
356.043334	14571.565287	29.319975
356.423437	14587.552341	29.324992
356.772933	14608.230767	29.330010
356.730474	14632.175693	29.335028
357.418921	14643.832426	29.340045
357.767815	14672.996801	29.345063
358.414690	14681.947227	29.350080
358.153001	14711.847812	29.355098
358.584873	14728.363802	29.360116
359.170249	14742.553649	29.365133
359.183261	14765.397403	29.370151
359.446055	14793.552140	29.375168
359.908530	14816.313348	29.380186
360.429628	14842.804672	29.385204
360.910891	14857.970884	29.390221
360.905744	14889.297177	29.395239
361.289580	14904.260682	29.400256
361.794494	14929.298748	29.405274
361.824102	14946.998692	29.410292
362.958372	14949.847640	29.415309
363.021768	14985.190047	29.420327
363.362152	15006.558800	29.425344
363.760954	15020.506301	29.430362
363.862985	15048.598015	29.435380
364.393681	15055.700236	29.440397
364.746960	15091.326159	29.445415
365.427750	15118.781511	29.450432
365.752305	15128.565555	29.455450
365.929575	15148.355512	29.460468
366.094709	15167.793663	29.465485
366.285372	15199.983745	29.470503
366.918074	15212.499058	29.475520
367.311164	15244.310300	29.480538
367.615011	15258.686482	29.485556
368.318305	15265.566104	29.490573
368.226677	15300.484766	29.495591
368.549654	15321.142830	29.500608
369.230034	15333.388669	29.505626
369.018935	15366.573249	29.510644
369.446111	15381.397738	29.515661
369.773831	15404.992290	29.520679
370.017248	15431.890858	29.525696
370.478706	15462.949641	29.530714
370.925331	15481.491567	29.535732
371.344100	15503.717187	29.540749
371.869581	15526.646297	29.545767
372.181326	15538.090619	29.550784
372.452375	15572.043742	29.555802
372.499816	15594.766273	29.560820
373.483419	15614.712265	29.565837
373.471089	15647.345276	29.570855
374.204585	15675.661746	29.575872
374.701385	15689.373403	29.580890
374.832984	15720.010217	29.585908
375.226880	15744.033884	29.590925
375.754342	15766.662939	29.595943
376.345984	15786.632234	29.600960
376.522222	15814.501916	29.605978
376.941969	15833.939005	29.610996
377.395268	15847.303821	29.616013
378.082183	15863.244181	29.621031
378.327462	15884.300262	29.626048
378.963027	15905.946214	29.631066
379.082555	15918.974571	29.636084
379.248578	15928.951097	29.641101
379.542457	15968.014658	29.646119
380.125885	15992.441819	29.651136
380.797729	16004.070392	29.656154
380.735181	16031.355376	29.661172
381.612788	16051.384654	29.666189
381.641100	16058.407548	29.671207
381.945807	16090.170793	29.676224
382.175930	16111.141049	29.681242
382.293986	16137.396877	29.686260
382.722598	16167.182792	29.691277
382.895406	16188.007296	29.696295
383.515981	16222.962046	29.701312
384.000915	16250.604278	29.706330
384.570029	16286.985258	29.711348
385.204721	16310.848973	29.716365
385.645504	16330.867590	29.721383
385.756172	16353.060046	29.726400
386.371559	16370.142663	29.731418
386.744009	16389.139191	29.736436
386.896112	16408.552207	29.741453
387.554456	16438.877604	29.746471
387.835811	16472.606474	29.751488
388.155214	16491.273414	29.756506
388.101842	16522.688847	29.761524
388.342562	16544.965505	29.766541
389.146564	16568.155710	29.771559
389.215007	16608.417965	29.776576
389.718444	16629.065139	29.781594
390.337804	16664.782062	29.786612
390.840884	16679.940011	29.791629
391.284356	16702.532714	29.796647
391.894170	16731.012131	29.801664
392.307140	16751.010250	29.806682
392.584368	16771.165335	29.811700
392.855698	16795.837932	29.816717
393.278950	16813.478317	29.821735
393.627330	16832.460081	29.826752
393.908734	16850.905879	29.831770
393.787344	16880.655347	29.836788
394.422037	16891.728039	29.841805
395.181222	16919.372759	29.846823
395.235585	16947.111453	29.851840
395.512130	16957.933570	29.856858
395.412389	16991.710046	29.861876
395.886763	17023.833755	29.866893
396.189092	17058.473188	29.871911
396.863647	17091.990324	29.876928
397.343091	17119.334605	29.881946
397.747568	17153.560337	29.886964
398.314857	17188.964174	29.891981
398.863655	17204.601830	29.896999
399.439589	17237.929270	29.902016
399.836378	17253.060001	29.907034
400.270062	17274.710503	29.912052
400.706917	17309.724261	29.917069
401.268333	17336.977127	29.922087
401.344377	17362.262023	29.927104
401.762740	17386.078633	29.932122
402.330448	17405.036293	29.937140
402.640824	17429.172988	29.942157
402.758286	17456.002405	29.947175
402.984157	17482.745493	29.952192
403.447986	17516.722580	29.957210
404.409112	17545.325391	29.962228
404.533187	17572.851984	29.967245
404.940031	17594.879736	29.972263
405.199221	17622.451695	29.977280
405.935075	17641.377093	29.982298
406.395019	17674.571735	29.987316
407.111054	17705.945119	29.992333
407.366307	17718.482935	29.997351
407.348715	17742.149912	30.002368
408.212649	17766.001859	30.007386
408.691674	17788.460800	30.012404
409.132042	17813.490576	30.017421
409.744435	17830.931883	30.022439
410.036503	17849.945528	30.027456
410.559033	17866.358515	30.032474
410.821607	17888.465918	30.037492
411.735827	17901.943611	30.042509
411.977861	17924.224819	30.047527
412.233803	17948.032664	30.052544
412.855152	17963.002648	30.057562
413.377530	17988.304160	30.062580
413.720527	17996.065272	30.067597
414.118364	18008.947482	30.072615
414.511856	18035.658924	30.077632
414.642218	18042.701400	30.082650
414.979008	18077.874269	30.087668
414.739021	18100.420240	30.092685
415.364965	18121.852244	30.097703
415.605050	18155.751576	30.102720
415.914106	18178.717550	30.107738
416.068593	18203.906050	30.112756
416.387720	18243.996866	30.117773
417.036069	18280.599862	30.122791
417.565300	18323.273526	30.127808
417.847327	18346.117558	30.132826
418.047871	18384.357177	30.137844
418.205131	18421.782347	30.142861
419.344529	18443.747562	30.147879
419.510283	18489.460003	30.152896
420.037009	18515.740732	30.157914
420.695691	18549.051236	30.162932
421.302729	18579.849168	30.167949
421.560387	18599.822845	30.172967
421.917628	18627.532590	30.177984
422.238833	18646.567752	30.183002
422.909359	18674.412000	30.188020
422.975034	18695.824466	30.193037
423.767438	18718.305193	30.198055
423.870703	18748.499529	30.203072
423.965114	18781.620308	30.208090
424.662230	18811.343238	30.213108
424.838272	18851.268059	30.218125
425.554238	18872.427861	30.223143
425.838991	18906.763781	30.228160
426.232569	18932.497222	30.233178
426.735298	18965.472618	30.238196
426.711056	19006.079649	30.243213
427.600813	19035.867698	30.248231
428.091757	19071.214215	30.253248
429.125104	19093.139822	30.258266
429.582529	19118.850935	30.263284
429.530222	19146.833663	30.268301
430.483501	19170.622896	30.273319
430.890177	19190.100156	30.278336
431.494870	19209.805633	30.283354
432.103569	19230.710866	30.288372
432.639261	19250.483986	30.293389
433.522611	19258.654263	30.298407
433.560855	19282.459732	30.303424
433.705265	19304.700864	30.308442
434.468141	19317.571341	30.313460
434.769700	19339.314220	30.318477
435.317666	19347.833681	30.323495
435.163009	19378.738826	30.328512
435.520236	19401.174375	30.333530
435.833907	19429.327972	30.338548
436.116795	19461.858288	30.343565
436.551301	19493.815408	30.348583
436.791565	19536.839978	30.353600
437.818841	19561.793278	30.358618
438.160592	19586.486901	30.363636
438.184891	19623.189582	30.368653
438.776749	19652.759606	30.373671
438.694575	19685.637748	30.378688
439.213555	19717.664216	30.383706
439.796856	19757.072607	30.388724
440.115193	19792.403081	30.393741
440.945722	19828.102450	30.398759
441.122314	19869.103309	30.403776
441.540627	19905.195523	30.408794
441.808022	19938.739910	30.413812
441.846226	19978.480007	30.418829
442.710712	20006.472870	30.423847
443.458045	20051.788859	30.428864
443.859500	20078.982035	30.433882
444.373156	20121.042908	30.438900
444.772456	20163.475483	30.443917
445.621822	20188.533101	30.448935
445.917924	20221.012080	30.453952
446.204847	20242.290712	30.458970
447.097728	20279.939784	30.463988
447.180872	20309.703725	30.469005
448.140466	20341.820574	30.474023
448.298216	20374.037034	30.479040
448.523089	20399.034192	30.484058
449.060229	20434.856163	30.489076
449.104913	20471.279265	30.494093
449.983903	20508.463402	30.499111
450.111722	20528.781492	30.504128
450.622057	20550.316312	30.509146
451.161685	20574.961424	30.514164
451.879683	20622.248236	30.519181
452.436813	20633.104543	30.524199
453.152417	20667.193261	30.529216
453.203998	20688.540607	30.534234
453.680969	20693.274503	30.539252
454.147009	20723.516507	30.544269
454.673543	20746.735970	30.549287
455.395909	20763.891116	30.554304
455.864296	20789.659589	30.559322
455.976327	20813.284842	30.564340
456.189767	20838.246432	30.569357
456.656138	20878.976838	30.574375
457.248122	20905.414907	30.579392
457.220635	20944.156273	30.584410
458.027238	20977.732224	30.589428
458.439885	21010.238596	30.594445
458.716204	21035.841428	30.599463
459.363746	21063.856946	30.604480
459.495914	21111.267730	30.609498
460.159541	21138.611112	30.614516
460.608654	21171.889225	30.619533
461.146927	21210.441946	30.624551
461.401721	21247.825755	30.629568
461.879399	21289.319769	30.634586
462.278706	21318.960201	30.639604
462.712372	21367.076548	30.644621
463.391117	21404.053462	30.649639
463.953347	21430.913885	30.654656
464.354972	21471.137490	30.659674
464.841909	21496.272163	30.664692
465.442838	21533.792181	30.669709
466.130904	21570.786913	30.674727
466.668262	21598.561291	30.679744
467.450001	21621.748379	30.684762
468.545772	21645.872286	30.689780
468.922393	21667.782984	30.694797
469.195835	21677.104420	30.699815
469.557963	21699.725078	30.704832
470.080915	21723.767658	30.709850
470.414426	21744.282449	30.714868
470.687890	21782.915428	30.719885
471.177265	21810.918725	30.724903
471.925877	21827.982259	30.729920
471.785315	21857.852874	30.734938
472.655041	21874.998691	30.739956
472.405791	21918.287928	30.744973
473.077010	21949.820454	30.749991
473.542208	21987.842679	30.755008
473.597379	22028.374100	30.760026
474.443122	22062.653495	30.765044
474.800204	22096.029639	30.770061
475.347392	22138.045384	30.775079
475.733224	22171.771023	30.780096
476.331711	22207.605632	30.785114
476.765997	22240.622477	30.790132
477.109962	22279.460287	30.795149
477.530994	22314.994147	30.800167
478.521054	22344.550473	30.805184
478.790374	22385.283078	30.810202
479.315177	22413.389132	30.815220
479.764530	22447.996292	30.820237
480.427091	22481.685698	30.825255
480.893081	22509.162853	30.830272
481.523927	22544.158963	30.835290
481.973969	22578.039587	30.840308
482.328244	22608.276612	30.845325
482.976696	22629.280389	30.850343
483.774664	22644.997370	30.855360
483.779947	22684.615360	30.860378
484.689122	22688.536841	30.865396
484.780197	22719.402658	30.870413
485.071327	22751.886589	30.875431
485.707929	22776.898495	30.880448
486.242040	22812.782137	30.885466
486.310571	22829.175198	30.890484
486.685095	22869.279494	30.895501
486.995616	22908.622934	30.900519
487.497132	22931.071651	30.905536
487.893877	22972.802965	30.910554
488.462050	23005.282095	30.915572
489.018061	23060.587061	30.920589
489.416999	23089.155994	30.925607
489.731489	23125.712603	30.930624
490.255218	23176.169979	30.935642
491.083903	23203.149308	30.940660
491.566449	23247.275364	30.945677
492.122038	23291.232173	30.950695
492.940009	23308.374659	30.955712
493.144540	23357.454096	30.960730
493.998781	23380.271784	30.965748
494.622172	23411.839365	30.970765
495.325577	23437.656860	30.975783
495.967054	23476.128429	30.980800
496.255299	23501.991682	30.985818
496.882920	23528.756313	30.990836
497.364335	23563.177176	30.995853
497.646037	23586.058956	31.000871
498.362433	23611.198514	31.005888
498.725829	23655.824277	31.010906
498.851292	23680.070138	31.015924
499.610867	23713.569602	31.020941
500.005295	23747.347138	31.025959
500.455399	23782.051295	31.030976
500.629757	23811.787356	31.035994
501.300489	23849.642136	31.041012
501.989577	23888.928582	31.046029
502.300082	23931.142954	31.051047
502.986504	23959.055422	31.056064
503.189372	24005.059266	31.061082
503.768393	24044.647519	31.066100
504.511024	24082.289334	31.071117
504.908669	24117.583612	31.076135
505.392064	24144.870746	31.081152
505.854815	24189.665496	31.086170
506.657948	24227.816347	31.091188
506.696089	24260.222060	31.096205
507.472875	24297.290227	31.101223
508.453427	24324.538128	31.106240
508.599399	24356.206808	31.111258
509.053023	24397.628929	31.116276
509.884692	24437.235505	31.121293
510.200616	24473.566869	31.126311
510.916395	24498.537022	31.131328
511.113190	24534.849128	31.136346
512.072288	24567.756544	31.141364
512.201471	24601.937025	31.146381
512.721044	24637.693516	31.151399
513.081754	24668.678363	31.156416
513.752892	24701.523398	31.161434
514.296653	24744.840675	31.166452
514.962560	24781.086516	31.171469
514.733922	24816.264666	31.176487
515.239255	24859.942063	31.181504
516.033712	24895.169622	31.186522
516.551299	24929.991660	31.191540
516.953529	24970.310736	31.196557
516.975625	25007.169094	31.201575
517.587985	25053.882584	31.206592
518.133620	25087.474539	31.211610
518.457225	25127.332204	31.216628
519.289072	25172.880601	31.221645
519.757410	25208.071006	31.226663
520.730590	25240.977340	31.231680
521.286557	25285.210226	31.236698
521.576151	25327.740461	31.241716
522.164933	25351.138906	31.246733
522.733563	25394.485313	31.251751
523.205918	25434.946077	31.256768
523.647019	25482.199119	31.261786
524.048197	25517.154054	31.266804
524.792653	25550.880145	31.271821
525.063583	25595.177047	31.276839
525.805905	25635.109570	31.281856
526.376431	25675.757768	31.286874
526.765441	25712.130557	31.291892
527.613425	25763.624666	31.296909
527.763507	25806.607377	31.301927
528.281943	25828.867131	31.306944
528.885417	25877.998080	31.311962
529.171194	25922.830575	31.316980
530.289472	25954.521048	31.321997
531.048530	25995.526052	31.327015
531.685086	26022.874061	31.332032
532.072888	26067.469800	31.337050
532.528535	26109.249053	31.342068
533.199407	26136.553955	31.347085
533.223179	26182.925629	31.352103
533.957085	26218.108059	31.357120
534.671674	26258.286293	31.362138
535.088433	26300.274234	31.367156
535.983830	26333.314548	31.372173
536.121920	26381.008708	31.377191
536.742309	26406.861925	31.382208
537.389563	26445.641664	31.387226
537.607366	26490.574482	31.392244
538.546032	26526.901095	31.397261
538.919339	26570.084521	31.402279
539.632941	26614.630751	31.407296
540.417736	26647.315918	31.412314
540.819396	26678.594530	31.417332
541.093948	26723.411591	31.422349
541.747981	26755.093438	31.427367
542.382802	26791.341427	31.432384
542.577863	26835.690785	31.437402
542.761690	26881.508255	31.442420
544.198746	26900.763177	31.447437
544.055403	26958.816948	31.452455
545.314644	26992.737083	31.457472
545.736691	27017.553856	31.462490
545.760082	27059.762616	31.467508
546.833213	27116.148543	31.472525
547.433188	27153.755127	31.477543
547.884979	27188.534434	31.482560
548.084726	27221.810905	31.487578
548.799619	27265.347133	31.492596
549.352685	27296.906502	31.497613
549.600820	27336.287304	31.502631
550.393172	27370.874861	31.507648
550.810925	27404.945649	31.512666
551.227382	27454.899583	31.517684
551.986313	27500.401392	31.522701
552.459973	27539.475706	31.527719
553.174355	27581.925599	31.532736
553.678357	27618.833789	31.537754
553.999542	27654.658123	31.542772
554.512521	27683.904766	31.547789
554.852383	27720.099210	31.552807
555.500211	27758.502154	31.557824
556.217952	27803.044034	31.562842
556.656597	27838.439581	31.567860
557.588743	27877.063945	31.572877
557.804914	27919.952369	31.577895
558.537745	27961.553245	31.582912
559.162830	27994.455065	31.587930
559.573711	28036.093573	31.592948
560.709018	28067.740475	31.597965
561.288767	28105.807047	31.602983
561.695852	28129.970179	31.608000
562.476986	28173.163057	31.613018
562.973590	28204.555653	31.618036
563.505049	28235.690051	31.623053
564.133321	28278.540358	31.628071
564.711292	28305.180033	31.633088
565.398708	28334.349893	31.638106
565.942495	28372.991414	31.643124
566.431944	28408.639189	31.648141
566.790558	28451.102038	31.653159
567.308424	28482.649768	31.658176
567.785741	28514.703190	31.663194
568.171807	28562.926405	31.668212
568.628792	28595.994420	31.673229
569.285878	28642.127743	31.678247
569.882255	28701.221686	31.683264
570.532051	28739.651458	31.688282
570.601310	28792.810429	31.693300
571.219069	28832.086016	31.698317
571.799465	28886.714236	31.703335
572.295691	28937.133443	31.708352
573.048319	28983.840493	31.713370
573.380796	29038.090542	31.718388
574.178862	29085.030939	31.723405
574.574179	29133.216135	31.728423
575.017862	29186.703409	31.733440
576.109461	29234.356953	31.738458
576.727839	29294.296178	31.743476
577.594487	29326.713762	31.748493
577.931915	29369.365121	31.753511
578.444909	29420.579340	31.758528
578.766606	29468.328000	31.763546
579.521980	29510.238251	31.768564
580.504997	29553.889334	31.773581
581.551599	29581.848329	31.778599
582.233807	29624.130497	31.783616
583.296913	29652.112303	31.788634
583.655855	29692.270522	31.793652
583.989122	29728.690788	31.798669
584.934138	29760.711279	31.803687
585.094717	29799.737524	31.808704
585.742123	29832.980168	31.813722
586.219079	29872.924417	31.818740
586.873526	29907.740025	31.823757
587.563712	29942.038122	31.828775
587.433929	29983.853258	31.833792
588.271440	30014.620347	31.838810
588.073147	30059.044266	31.843828
588.888657	30100.807298	31.848845
589.697024	30146.142962	31.853863
590.045693	30197.011752	31.858880
590.799298	30255.630578	31.863898
591.334530	30290.952123	31.868916
592.361968	30322.417041	31.873933
592.744740	30365.543819	31.878951
593.117401	30407.243669	31.883968
593.856471	30445.220258	31.888986
594.216192	30483.432966	31.894004
594.764124	30519.960282	31.899021
595.246658	30567.446249	31.904039
596.147582	30606.301878	31.909056
596.761780	30647.724405	31.914074
597.418187	30690.271956	31.919092
597.564335	30730.313616	31.924109
598.324999	30775.304099	31.929127
599.274703	30822.319684	31.934144
600.058302	30862.401435	31.939162
600.824943	30910.248529	31.944180
601.157190	30948.769802	31.949197
601.609079	30978.688088	31.954215
602.178149	31031.509538	31.959232
602.938219	31068.934046	31.964250
603.472784	31113.808751	31.969268
603.964042	31164.474407	31.974285
604.610689	31200.437595	31.979303
605.127799	31253.217129	31.984320
605.611833	31303.119352	31.989338
606.107442	31349.170105	31.994356
606.585170	31395.394425	31.999373
607.363685	31447.634361	32.004391
607.481975	31505.464303	32.009408
608.252393	31545.391393	32.014426
608.933591	31610.258386	32.019444
609.794619	31660.861372	32.024461
610.661135	31711.217084	32.029479
611.347742	31769.572486	32.034496
611.976878	31811.235241	32.039514
612.668283	31860.006559	32.044532
613.070119	31906.471411	32.049549
613.873333	31954.176149	32.054567
613.994273	31996.424122	32.059584
614.825304	32050.680342	32.064602
615.615063	32108.375825	32.069620
616.219316	32159.955615	32.074637
616.584272	32199.150544	32.079655
617.181073	32262.212049	32.084672
618.171588	32313.346462	32.089690
618.560148	32359.371868	32.094708
619.382227	32412.492503	32.099725
620.059187	32461.476101	32.104743
620.517967	32516.942061	32.109760
621.178886	32562.426091	32.114778
621.513353	32607.088622	32.119796
622.198513	32663.916865	32.124813
622.987844	32722.530790	32.129831
623.482426	32774.160785	32.134848
624.359304	32831.364242	32.139866
624.544106	32888.700882	32.144884
625.139376	32944.797893	32.149901
625.991791	32994.766946	32.154919
626.426456	33060.328003	32.159936
626.925125	33110.662180	32.164954
627.342820	33163.424104	32.169972
628.410948	33221.110943	32.174989
629.104838	33282.187934	32.180007
629.600544	33345.970201	32.185024
630.165351	33394.840685	32.190042
630.673646	33452.963030	32.195060
631.126424	33509.336622	32.200077
631.862527	33567.701996	32.205095
632.381683	33631.127440	32.210112
633.671199	33686.517757	32.215130
634.201841	33722.693030	32.220148
634.812282	33768.882988	32.225165
635.801623	33816.765323	32.230183
636.032382	33867.339014	32.235200
636.807990	33913.421389	32.240218
637.168368	33961.642214	32.245236
637.573559	34015.660041	32.250253
638.274294	34064.188487	32.255271
638.674894	34121.602384	32.260288
639.227037	34176.773702	32.265306
640.080249	34243.936080	32.270324
640.514092	34303.703541	32.275341
641.341879	34342.387868	32.280359
641.698728	34410.336155	32.285376
642.556273	34471.429066	32.290394
643.587392	34545.841836	32.295412
643.702832	34600.848317	32.300429
644.738027	34651.469371	32.305447
645.437145	34726.446584	32.310464
645.953799	34782.516488	32.315482
646.175940	34837.702975	32.320500
646.631587	34900.212717	32.325517
647.497367	34958.176089	32.330535
647.855431	35037.228659	32.335552
648.671073	35110.134248	32.340570
649.294534	35174.983342	32.345588
649.689825	35241.777598	32.350605
650.092186	35310.948295	32.355623
650.824848	35396.506841	32.360640
652.137379	35458.663547	32.365658
653.017275	35517.397628	32.370676
654.013441	35585.920382	32.375693
654.622085	35648.060765	32.380711
654.961149	35719.253294	32.385728
656.020076	35774.647068	32.390746
656.676189	35839.221231	32.395764
656.952464	35914.407581	32.400781
657.661697	35956.597223	32.405799
658.378866	36031.816520	32.410816
658.848692	36095.623777	32.415834
659.924388	36163.415205	32.420852
660.106280	36228.582855	32.425869
660.959068	36301.935692	32.430887
661.398155	36366.115279	32.435904
662.202617	36421.398602	32.440922
663.015176	36501.884431	32.445940
663.358434	36568.153502	32.450957
664.038553	36630.450030	32.455975
664.545671	36709.131529	32.460992
665.387671	36773.432990	32.466010
666.420284	36850.907692	32.471028
666.243113	36925.428391	32.476045
667.377320	36997.671199	32.481063
668.053959	37074.462315	32.486080
668.905043	37139.288291	32.491098
669.484812	37214.027293	32.496116
670.153171	37279.729456	32.501133
670.975903	37346.375253	32.506151
671.216296	37419.169643	32.511168
672.061391	37486.994856	32.516186
672.666126	37563.938035	32.521204
673.527558	37623.123437	32.526221
674.690939	37691.582675	32.531239
674.908681	37766.367314	32.536256
675.847645	37829.860110	32.541274
676.539530	37892.095249	32.546292
676.773191	37960.997280	32.551309
677.393096	38023.288269	32.556327
678.153123	38091.444813	32.561344
678.679448	38154.528542	32.566362
679.903673	38224.902364	32.571380
680.401375	38295.484369	32.576397
681.270852	38346.803997	32.581415
681.636209	38419.563354	32.586432
682.363738	38480.688019	32.591450
683.048115	38545.120516	32.596468
683.675759	38610.422056	32.601485
684.461082	38683.161192	32.606503
685.235593	38747.289374	32.611520
685.734934	38804.112420	32.616538
686.352899	38878.067126	32.621556
686.877719	38949.785326	32.626573
687.589371	39010.534540	32.631591
688.250995	39084.691842	32.636608
688.969150	39163.115502	32.641626
689.866898	39217.386030	32.646644
690.449061	39294.123900	32.651661
691.156402	39361.590715	32.656679
691.748303	39433.445526	32.661696
692.446547	39512.252987	32.666714
693.268036	39584.161094	32.671732
693.647376	39659.894706	32.676749
694.673686	39739.998930	32.681767
695.146372	39812.436393	32.686784
695.903711	39888.478753	32.691802
697.036454	39960.156258	32.696820
697.253464	40048.691093	32.701837
698.087776	40107.223511	32.706855
698.542863	40188.708431	32.711872
699.145133	40261.323266	32.716890
700.235223	40346.061721	32.721908
700.682167	40429.256335	32.726925
701.668790	40496.151971	32.731943
702.305578	40572.253435	32.736960
702.867128	40649.543190	32.741978
703.885720	40724.169116	32.746996
704.272844	40810.334259	32.752013
705.387051	40883.794826	32.757031
705.823339	40966.449257	32.762048
706.560038	41040.316956	32.767066
707.612111	41118.164448	32.772084
708.194891	41194.643306	32.777101
709.272017	41260.584863	32.782119
709.990363	41331.502895	32.787136
710.988929	41403.142796	32.792154
712.385915	41462.419772	32.797172
712.576358	41524.332315	32.802189
713.519628	41579.815965	32.807207
714.172366	41645.122725	32.812224
714.569031	41717.616299	32.817242
715.356290	41780.960882	32.822260
716.095203	41849.189442	32.827277
716.760301	41915.323606	32.832295
717.448476	41973.706693	32.837312
717.905609	42059.568599	32.842330
719.310108	42112.287492	32.847348
719.550016	42179.329823	32.852365
719.916188	42250.621887	32.857383
720.580404	42311.254877	32.862400
721.391375	42403.166413	32.867418
721.804887	42466.027225	32.872436
722.829319	42543.340154	32.877453
723.508247	42617.905243	32.882471
723.944680	42678.479831	32.887488
724.204992	42759.859172	32.892506
725.061832	42840.083370	32.897524
726.151960	42915.831458	32.902541
726.294935	42982.182931	32.907559
727.417873	43050.678009	32.912576
727.963765	43119.111329	32.917594
728.765919	43192.039985	32.922612
729.075618	43265.191016	32.927629
729.900207	43348.394837	32.932647
730.731845	43436.385941	32.937664
731.341558	43521.578306	32.942682
732.277978	43589.452607	32.947700
732.963018	43678.466860	32.952717
733.900521	43760.282100	32.957735
734.404639	43827.990398	32.962752
735.217808	43908.124067	32.967770
736.304586	43977.177937	32.972788
737.057797	44063.109070	32.977805
737.466223	44143.078886	32.982823
738.440763	44227.028020	32.987840
738.943275	44305.054560	32.992858
739.645825	44382.057159	32.997876
740.675215	44460.596808	33.002893
741.228052	44543.113673	33.007911
742.445254	44627.937400	33.012928
742.602607	44702.894319	33.017946
743.872855	44784.199777	33.022964
744.680170	44854.242367	33.027981
745.406682	44930.136175	33.032999
746.119010	45005.652919	33.038016
746.887511	45088.979525	33.043034
748.206150	45167.963707	33.048052
748.617566	45240.719545	33.053069
749.323550	45317.364282	33.058087
750.158153	45396.816810	33.063104
750.804150	45469.435665	33.068122
751.460435	45548.517974	33.073140
751.890447	45631.728501	33.078157
752.793554	45703.789387	33.083175
753.737195	45787.907348	33.088192
754.322627	45872.258507	33.093210
754.974253	45951.671903	33.098228
755.855446	46035.408316	33.103245
756.664113	46120.876954	33.108263
757.565565	46199.727295	33.113280
758.014952	46296.999619	33.118298
758.638055	46376.842791	33.123316
760.019332	46465.038622	33.128333
760.358531	46549.253527	33.133351
761.292389	46626.841459	33.138368
761.970749	46718.924305	33.143386
762.519758	46790.778108	33.148404
763.710366	46881.440764	33.153421
764.387877	46965.370496	33.158439
765.082550	47040.302185	33.163456
765.793545	47128.940239	33.168474
766.731464	47205.757747	33.173492
767.802431	47287.710613	33.178509
768.340591	47361.984510	33.183527
769.569568	47437.353088	33.188544
770.516885	47511.721939	33.193562
771.254146	47583.061839	33.198580
772.388216	47650.013041	33.203597
772.713773	47721.221351	33.208615
773.742396	47787.936325	33.213632
774.414330	47862.924889	33.218650
775.100997	47936.778996	33.223668
775.984117	48001.834447	33.228685
777.017578	48064.918161	33.233703
777.899549	48124.995298	33.238720
778.463319	48189.310201	33.243738
778.941989	48245.293995	33.248756
779.661033	48319.232875	33.253773
780.390516	48383.459267	33.258791
781.013879	48447.487260	33.263808
781.115329	48530.038393	33.268826
782.219302	48596.788300	33.273844
782.984615	48674.782752	33.278861
783.407376	48740.462388	33.283879
784.551371	48819.043694	33.288896
785.078675	48912.126927	33.293914
785.815858	48983.313069	33.298932
786.443754	49064.493554	33.303949
786.962431	49152.524125	33.308967
788.168207	49235.487953	33.313984
788.618448	49326.920952	33.319002
789.137076	49403.475844	33.324020
790.298844	49499.803219	33.329037
791.217652	49596.637002	33.334055
792.012675	49682.671617	33.339072
792.392356	49773.181013	33.344090
792.989542	49857.026358	33.349108
794.126007	49957.225306	33.354125
794.835815	50048.899160	33.359143
795.807198	50142.354819	33.364160
796.556601	50239.407493	33.369178
797.117276	50326.341466	33.374196
797.966075	50404.025117	33.379213
799.007689	50517.578609	33.384231
800.144363	50608.422673	33.389248
800.847129	50695.342246	33.394266
801.981910	50794.286012	33.399284
802.662906	50880.121407	33.404301
803.260348	50969.962567	33.409319
804.188475	51047.863817	33.414336
804.909309	51152.333915	33.419354
805.627053	51240.670506	33.424372
806.832071	51323.249701	33.429389
807.625352	51419.775347	33.434407
808.554065	51513.717751	33.439424
809.411288	51595.263760	33.444442
810.018256	51682.841019	33.449460
811.011801	51777.634922	33.454477
812.067688	51864.510246	33.459495
812.682099	51946.234490	33.464512
813.425406	52036.303848	33.469530
814.284144	52107.999579	33.474548
815.638414	52193.526228	33.479565
816.015566	52286.621150	33.484583
816.992263	52361.950282	33.489600
817.788205	52462.257390	33.494618
818.481700	52551.545551	33.499636
819.536670	52639.056672	33.504653
820.394727	52719.897804	33.509671
821.239736	52807.954781	33.514688
822.086382	52900.042573	33.519706
822.809361	52981.481457	33.524724
823.893475	53063.123845	33.529741
823.909735	53145.268118	33.534759
824.989120	53230.803398	33.539776
825.784287	53315.130328	33.544794
826.538613	53400.014441	33.549812
827.373246	53492.568367	33.554829
828.574479	53589.014185	33.559847
829.390316	53668.093361	33.564864
829.956145	53761.671016	33.569882
830.950578	53848.468375	33.574900
831.575364	53929.748658	33.579917
832.225971	54005.753989	33.584935
832.999705	54080.209021	33.589952
834.113829	54170.640199	33.594970
834.325688	54245.385715	33.599988
835.536892	54340.440895	33.605005
836.046662	54432.409957	33.610023
837.061150	54518.232138	33.615040
837.558835	54600.895069	33.620058
838.537694	54688.014356	33.625076
839.701014	54778.864198	33.630093
840.184962	54868.408952	33.635111
841.283698	54961.370517	33.640128
842.402629	55053.879998	33.645146
842.952616	55138.441476	33.650164
843.895829	55224.783584	33.655181
844.491514	55328.722258	33.660199
845.414867	55405.430054	33.665216
845.940880	55493.736594	33.670234
846.834841	55600.477801	33.675252
848.101904	55695.175343	33.680269
848.776566	55797.895046	33.685287
849.742891	55878.432734	33.690304
850.683954	55977.732332	33.695322
851.387335	56068.544803	33.700340
852.646242	56161.157056	33.705357
853.378584	56257.604489	33.710375
854.610054	56335.134342	33.715392
855.787067	56434.437088	33.720410
856.339167	56521.724471	33.725428
857.620022	56602.709283	33.730445
858.048290	56685.643425	33.735463
858.936688	56773.145183	33.740480
859.972952	56866.763130	33.745498
861.101971	56959.506291	33.750516
861.855716	57046.707243	33.755533
862.434008	57141.758247	33.760551
863.103067	57225.739006	33.765568
864.003990	57309.709282	33.770586
864.531072	57422.180084	33.775604
865.469706	57508.031195	33.780621
866.583806	57602.342410	33.785639
867.347773	57703.923523	33.790656
868.371350	57796.388874	33.795674
869.254233	57898.458617	33.800692
870.498230	57976.909548	33.805709
870.801230	58081.582964	33.810727
871.858462	58183.209056	33.815744
872.637005	58275.005529	33.820762
873.773191	58368.601119	33.825780
874.861308	58461.305813	33.830797
875.750886	58558.636763	33.835815
876.189888	58645.955799	33.840832
877.578458	58735.931190	33.845850
878.021413	58832.959342	33.850868
879.113307	58921.165105	33.855885
879.885275	59015.440166	33.860903
880.704174	59107.752524	33.865920
881.634805	59201.617522	33.870938
882.325809	59298.102574	33.875956
883.666785	59385.454763	33.880973
884.378581	59486.747680	33.885991
885.030655	59580.385338	33.891008
886.114332	59666.645618	33.896026
886.798195	59764.994503	33.901044
887.655764	59858.183494	33.906061
888.478209	59958.074981	33.911079
889.539642	60054.081289	33.916096
890.591190	60128.644812	33.921114
891.206522	60222.379271	33.926132
891.942077	60310.569591	33.931149
892.911031	60397.040205	33.936167
893.756982	60479.169114	33.941184
894.916736	60564.110482	33.946202
895.418011	60657.959312	33.951220
896.388839	60745.874049	33.956237
897.187176	60837.803717	33.961255
897.976523	60927.108258	33.966272
899.134607	61020.166285	33.971290
899.788869	61119.841835	33.976308
900.734568	61212.110770	33.981325
901.366368	61304.758068	33.986343
902.175142	61413.652423	33.991360
903.404390	61508.733134	33.996378
904.255094	61614.520171	34.001396
905.352773	61704.355571	34.006413
906.162026	61800.730810	34.011431
906.995894	61895.982173	34.016448
908.443552	61996.658193	34.021466
909.194486	62103.621265	34.026484
910.126613	62199.080057	34.031501
911.225407	62293.627052	34.036519
912.206207	62381.090310	34.041536
913.381204	62480.873881	34.046554
913.935536	62571.360405	34.051572
915.306204	62667.645304	34.056589
916.070820	62764.050238	34.061607
917.128291	62864.866496	34.066624
918.375181	62953.208250	34.071642
918.820255	63052.221497	34.076660
919.631312	63139.954411	34.081677
920.624291	63241.377291	34.086695
921.581544	63338.241909	34.091712
922.744316	63429.953579	34.096730
923.161173	63535.170651	34.101748
924.001622	63619.994993	34.106765
925.193272	63721.414226	34.111783
925.879690	63833.421230	34.116800
926.913173	63921.337512	34.121818
928.046444	64023.583705	34.126836
928.895388	64123.677848	34.131853
929.957748	64220.447233	34.136871
930.558019	64315.370728	34.141888
931.887319	64418.613591	34.146906
932.631813	64527.056808	34.151924
933.464388	64626.857966	34.156941
934.551966	64729.943486	34.161959
935.140186	64824.516260	34.166976
936.349110	64917.732936	34.171994
937.150004	65032.823256	34.177012
938.208557	65141.169590	34.182029
939.213015	65238.736946	34.187047
940.257181	65346.244392	34.192064
941.166567	65439.395671	34.197082
941.898850	65543.989621	34.202100
943.009829	65639.889562	34.207117
943.741473	65740.622513	34.212135
944.800903	65846.002486	34.217152
945.872768	65935.546926	34.222170
946.885617	66040.042277	34.227188
947.437088	66146.768794	34.232205
948.745719	66241.766556	34.237223
949.661137	66348.285321	34.242240
950.674444	66442.025580	34.247258
951.210415	66550.997458	34.252276
952.425966	66651.361137	34.257293
953.375147	66746.663661	34.262311
954.117816	66848.627568	34.267328
955.129289	66931.910602	34.272346
956.147067	67025.791608	34.277364
957.160018	67114.304706	34.282381
958.313444	67205.828985	34.287399
958.713410	67305.910659	34.292416
959.805037	67398.622894	34.297434
960.417293	67496.842484	34.302452
960.868710	67600.140020	34.307469
962.457233	67704.318333	34.312487
963.348744	67813.683469	34.317504
964.354772	67902.801876	34.322522
965.422923	68005.587162	34.327540
966.467103	68105.204452	34.332557
967.753593	68210.387915	34.337575
968.362918	68322.686378	34.342592
969.586118	68428.171843	34.347610
970.649092	68531.491905	34.352628
971.448615	68629.870305	34.357645
972.676979	68731.082280	34.362663
973.162026	68829.478735	34.367680
974.537852	68946.403123	34.372698
975.222802	69044.117102	34.377716
976.635391	69158.003770	34.382733
977.650395	69250.797942	34.387751
978.586677	69363.999834	34.392768
980.045885	69453.439318	34.397786
980.725540	69560.495702	34.402804
981.803551	69670.390578	34.407821
982.428402	69771.928528	34.412839
983.122958	69876.698036	34.417856
984.529649	69975.006042	34.422874
985.774860	70086.092411	34.427892
986.760785	70195.902534	34.432909
987.606571	70298.997519	34.437927
988.554906	70401.943974	34.442944
989.746191	70504.074157	34.447962
990.670272	70613.015489	34.452980
991.281359	70721.949007	34.457997
992.533022	70822.373994	34.463015
993.789736	70927.319849	34.468032
994.869129	71026.012054	34.473050
995.893253	71138.150498	34.478068
996.735713	71234.664046	34.483085
998.224156	71341.969137	34.488103
998.954358	71440.881904	34.493120
1000.008470	71540.352541	34.498138
1001.014907	71642.807243	34.503156
1001.990595	71755.209167	34.508173
1003.086053	71842.921383	34.513191
1003.961475	71956.935575	34.518208
1004.661446	72057.489171	34.523226
1006.151931	72158.692677	34.528244
1006.860294	72266.971547	34.533261
1008.040673	72368.376113	34.538279
1008.609492	72480.755812	34.543296
1009.588614	72580.356044	34.548314
1010.768474	72681.546583	34.553332
1011.692872	72793.935592	34.558349
1012.754579	72903.289300	34.563367
1013.930551	73005.418937	34.568384
1014.616557	73109.917721	34.573402
1016.234650	73218.185536	34.578420
1016.638791	73334.254884	34.583437
1017.516535	73434.304746	34.588455
1018.543869	73543.717109	34.593472
1019.465315	73645.331531	34.598490
1021.079381	73739.821583	34.603508
1021.666497	73847.492487	34.608525
1022.922162	73932.590165	34.613543
1023.658644	74033.753552	34.618560
1024.875500	74141.492279	34.623578
1025.981530	74247.868075	34.628596
1026.609586	74346.744276	34.633613
1027.687727	74449.186011	34.638631
1028.924779	74548.386149	34.643648
1029.914707	74642.064576	34.648666
1031.029336	74742.475132	34.653684
1031.646553	74851.462706	34.658701
1033.159245	74951.229424	34.663719
1034.083895	75061.195986	34.668736
1035.038613	75160.885672	34.673754
1036.415685	75265.500659	34.678772
1037.115718	75373.489459	34.683789
1038.577289	75467.718024	34.688807
1039.506024	75582.892133	34.693824
1040.319789	75689.496478	34.698842
1041.603082	75795.230142	34.703860
1042.596827	75909.774847	34.708877
1043.641685	76012.785075	34.713895
1044.393706	76134.613906	34.718912
1045.534322	76230.073136	34.723930
1046.527705	76347.533195	34.728948
1047.124450	76467.918301	34.733965
1048.496067	76578.467504	34.738983
1049.856052	76692.958515	34.744000
1050.852572	76806.771877	34.749018
1052.043836	76916.197795	34.754036
1052.791600	77035.865202	34.759053
1053.704488	77152.365874	34.764071
1054.654766	77270.165989	34.769088
1055.978111	77382.385435	34.774106
1057.303461	77501.787635	34.779124
1058.051085	77624.358557	34.784141
1059.385554	77736.299036	34.789159
1060.340178	77860.941659	34.794176
1061.675592	77972.743612	34.799194
1062.995742	78079.417859	34.804212
1063.676448	78200.050903	34.809229
1065.366574	78320.704708	34.814247
1066.350462	78429.434219	34.819264
1067.107127	78536.577999	34.824282
1068.291438	78647.228080	34.829300
1069.312421	78764.326864	34.834317
1070.384900	78879.454532	34.839335
1071.775843	78986.083276	34.844352
1072.493432	79098.784093	34.849370
1073.685093	79206.838242	34.854388
1074.511267	79328.049006	34.859405
1075.427326	79437.996570	34.864423
1076.583078	79559.017690	34.869440
1077.861029	79681.958634	34.874458
1078.985989	79785.071950	34.879476
1079.922132	79904.329796	34.884493
1080.877522	80024.218602	34.889511
1082.078316	80136.899105	34.894528
1083.840784	80237.862503	34.899546
1086.251248	80329.020924	34.904564
1087.981358	80418.689245	34.909581
1089.207767	80489.685982	34.914599
1090.590397	80562.926358	34.919616
1091.350239	80645.005597	34.924634
1092.595861	80718.888500	34.929652
1093.332949	80815.110619	34.934669
1094.367074	80880.842538	34.939687
1095.474230	80949.692563	34.944704
1096.198547	81019.463865	34.949722
1097.110082	81104.282759	34.954740
1097.576918	81181.759521	34.959757
1098.551951	81265.986228	34.964775
1099.714326	81353.845512	34.969792
1100.399858	81442.754848	34.974810
1101.495092	81531.651373	34.979828
1102.295678	81630.349647	34.984845
1103.392483	81726.873657	34.989863
1103.976336	81833.448903	34.994880
1104.987882	81931.557930	34.999898
1105.881288	82035.957241	35.004916
1107.239236	82145.479267	35.009933
1108.163028	82260.922793	35.014951
1109.488777	82377.697918	35.019968
1110.213105	82496.138223	35.024986
1111.359976	82605.264110	35.030004
1112.095120	82727.023253	35.035021
1113.165280	82842.991188	35.040039
1114.551116	82968.210399	35.045056
1115.272774	83083.435341	35.050074
1116.977223	83210.341855	35.055092
1118.163209	83328.599746	35.060109
1119.398406	83449.485920	35.065127
1120.533708	83567.676672	35.070144
1121.651900	83698.604472	35.075162
1123.021586	83804.228558	35.080180
1124.227481	83919.292816	35.085197
1125.460966	84039.814312	35.090215
1126.345449	84153.231670	35.095232
1127.297250	84278.207437	35.100250
1128.623697	84398.158459	35.105268
1129.832303	84512.173000	35.110285
1131.140577	84637.551001	35.115303
1132.089805	84753.532862	35.120320
1133.271226	84877.677227	35.125338
1134.293435	84998.210300	35.130356
1135.450221	85120.915042	35.135373
1136.883069	85230.272553	35.140391
1138.269827	85352.714406	35.145408
1139.184357	85479.690591	35.150426
1140.203729	85598.655372	35.155444
1141.270970	85718.639578	35.160461
1141.926022	85843.883751	35.165479
1143.346575	85965.892111	35.170496
1144.331128	86087.031154	35.175514
1145.750065	86223.917310	35.180532
1146.693689	86352.552781	35.185549
1148.176531	86474.756335	35.190567
1149.445063	86600.757291	35.195584
1150.659627	86733.660694	35.200602
1151.860711	86851.829346	35.205620
1153.250381	86973.403229	35.210637
1154.223345	87105.357518	35.215655
1155.422253	87214.594192	35.220672
1156.421335	87339.917975	35.225690
1157.332675	87468.728133	35.230708
1158.882174	87587.656549	35.235725
1159.739892	87705.907445	35.240743
1161.500681	87831.469592	35.245760
1162.577883	87951.993684	35.250778
1163.841063	88074.707002	35.255796
1164.703559	88192.908424	35.260813
1165.912428	88312.463060	35.265831
1167.399713	88422.647806	35.270848
1168.273516	88546.652941	35.275866
1169.516477	88648.816752	35.280884
1170.514967	88775.908254	35.285901
1171.602744	88883.558990	35.290919
1173.025009	88988.408046	35.295936
1173.717007	89101.494468	35.300954
1175.173087	89207.124754	35.305972
1176.145546	89317.963255	35.310989
1176.795003	89435.303022	35.316007
1178.193551	89551.969038	35.321024
1179.129823	89673.282469	35.326042
1180.366535	89795.829623	35.331060
1181.731296	89917.330817	35.336077
1183.138376	90032.920164	35.341095
1184.579879	90144.626559	35.346112
1185.507467	90272.191737	35.351130
1186.584328	90388.949121	35.356148
1187.444426	90518.186074	35.361165
1188.735884	90638.016034	35.366183
1190.432679	90750.610125	35.371200
1191.660002	90886.495839	35.376218
1192.544894	91001.891389	35.381236
1193.850469	91133.127464	35.386253
1195.135949	91259.842688	35.391271
1196.774838	91379.976396	35.396288
1197.781333	91503.833757	35.401306
1199.100917	91621.749500	35.406324
1200.204946	91733.793166	35.411341
1201.386932	91870.159313	35.416359
1202.860188	91975.847394	35.421376
1203.845831	92115.667218	35.426394
1205.068625	92248.746107	35.431412
1206.098934	92361.627396	35.436429
1207.188457	92498.036107	35.441447
1208.264025	92620.645200	35.446464
1209.940081	92752.705166	35.451482
1211.351043	92890.637235	35.456500
1212.186825	93010.674275	35.461517
1213.603406	93136.971356	35.466535
1215.287808	93255.875978	35.471552
1216.546553	93389.042977	35.476570
1217.376889	93511.414976	35.481588
1218.737043	93634.072565	35.486605
1219.749131	93753.007718	35.491623
1221.947503	93888.527577	35.496640
1222.706308	94013.346294	35.501658
1223.839577	94132.149978	35.506676
1225.426486	94253.076295	35.511693
1226.439354	94373.965686	35.516711
1228.022964	94480.456469	35.521728
1229.333372	94601.668020	35.526746
1230.649896	94707.225168	35.531764
1232.183540	94820.366728	35.536781
1233.360107	94940.877951	35.541799
1234.636288	95059.637610	35.546816
1235.675757	95162.704360	35.551834
1236.652466	95288.913961	35.556852
1238.105473	95396.936610	35.561869
1239.266712	95514.625807	35.566887
1240.234166	95630.989320	35.571904
1241.261952	95757.915385	35.576922
1242.543953	95872.887221	35.581940
1243.956174	95997.612227	35.586957
1245.116003	96110.880052	35.591975
1246.534206	96232.284002	35.596992
1247.552470	96346.918359	35.602010
1248.829126	96471.805793	35.607028
1250.314491	96592.744352	35.612045
1251.093710	96716.987658	35.617063
1251.993772	96834.887268	35.622080
1253.060927	96948.603534	35.627098
1254.302990	97066.171903	35.632116
1255.723938	97187.819971	35.637133
1256.316577	97319.992000	35.642151
1257.181485	97435.110542	35.647168
1258.470113	97562.434302	35.652186
1259.542444	97688.676713	35.657204
1261.181249	97813.120129	35.662221
1262.714921	97957.254405	35.667239
1263.855789	98088.025948	35.672256
1265.002750	98221.256353	35.677274
1266.280719	98347.634177	35.682292
1267.498796	98480.220762	35.687309
1268.855663	98624.816597	35.692327
1270.403750	98760.040467	35.697344
1271.692114	98892.376965	35.702362
1272.788888	99027.545446	35.707380
1274.164258	99158.449683	35.712397
1274.822491	99296.818787	35.717415
1276.574623	99441.432856	35.722432
1278.229644	99577.632355	35.727450
1278.958486	99722.837993	35.732468
1280.514927	99857.012982	35.737485
1281.541414	100011.516770	35.742503
1283.281763	100145.398111	35.747520
1284.368115	100291.653600	35.752538
1285.413791	100431.919608	35.757556
1286.849596	100576.828886	35.762573
1288.233709	100726.602397	35.767591
1289.700927	100869.403605	35.772608
1291.470736	101016.811081	35.777626
1292.751114	101152.936083	35.782644
1294.027684	101289.379193	35.787661
1295.238184	101425.009095	35.792679
1296.495137	101562.850975	35.797696
1297.964318	101705.731616	35.802714
1298.983696	101854.426066	35.807732
1300.539979	101994.847542	35.812749
1301.874725	102142.429249	35.817767
1303.548791	102283.594322	35.822784
1304.765017	102417.794806	35.827802
1305.574355	102555.000548	35.832820
1307.394376	102702.559952	35.837837
1308.672046	102837.006150	35.842855
1310.099050	102991.271537	35.847872
1311.634138	103123.485451	35.852890
1313.121583	103264.075203	35.857908
1313.963919	103397.767332	35.862925
1315.075357	103538.974639	35.867943
1316.140612	103692.082440	35.872960
1317.590771	103828.128702	35.877978
1318.956332	103979.314615	35.882996
1320.646972	104114.322983	35.888013
1321.847119	104269.288929	35.893031
1323.235716	104401.150362	35.898048
1324.521284	104544.984756	35.903066
1325.827621	104689.475853	35.908084
1326.968191	104829.809230	35.913101
1328.329521	104973.671711	35.918119
1329.930628	105118.765420	35.923136
1331.061172	105272.314076	35.928154
1332.264595	105410.104216	35.933172
1334.053075	105539.917212	35.938189
1335.026312	105695.216690	35.943207
1336.591622	105831.963222	35.948224
1338.283539	105973.775141	35.953242
1339.257236	106111.844815	35.958260
1340.690594	106244.835002	35.963277
1341.664181	106386.164507	35.968295
1343.007033	106510.382715	35.973312
1344.509527	106630.417522	35.978330
1345.790659	106761.468041	35.983348
1347.397872	106895.942629	35.988365
1348.451009	107023.732843	35.993383
1349.647828	107158.170902	35.998400
1351.177809	107297.807213	36.003418
1352.224932	107420.451707	36.008436
1353.601665	107552.821801	36.013453
1354.914456	107697.730488	36.018471
1356.404491	107832.975135	36.023488
1357.724798	107968.918792	36.028506
1358.894854	108115.677433	36.033524
1360.368469	108237.763924	36.038541
1361.526875	108398.816501	36.043559
1362.534549	108538.488425	36.048576
1364.001254	108692.963876	36.053594
1364.936661	108845.468435	36.058612
1366.625860	108995.383588	36.063629
1368.240036	109152.450370	36.068647
1369.573579	109301.699394	36.073664
1371.240523	109454.447827	36.078682
1372.268232	109609.693132	36.083700
1374.217215	109754.194377	36.088717
1375.823363	109904.202455	36.093735
1376.992839	110053.645084	36.098752
1378.697749	110206.365532	36.103770
1379.986146	110352.633305	36.108788
1381.322844	110499.185839	36.113805
1383.082458	110655.805571	36.118823
1383.916439	110805.569925	36.123840
1385.576873	110949.639110	36.128858
1386.955547	111111.773195	36.133876
1388.410667	111259.667380	36.138893
1389.952860	111403.072010	36.143911
1391.081808	111553.237475	36.148928
1393.039085	111693.598476	36.153946
1394.543603	111851.290426	36.158964
1395.655717	111991.695378	36.163981
1396.839145	112139.318466	36.168999
1398.064211	112292.807428	36.174016
1399.614900	112441.338430	36.179034
1401.063124	112601.071575	36.184052
1402.793141	112746.646374	36.189069
1404.393521	112885.862812	36.194087
1405.743692	113035.530834	36.199104
1407.570015	113176.311189	36.204122
1408.761048	113330.837151	36.209140
1410.500627	113475.944168	36.214157
1412.307415	113607.661354	36.219175
1413.259977	113750.038425	36.224192
1414.726585	113885.703089	36.229210
1415.514460	114032.380910	36.234228
1417.071782	114172.243139	36.239245
1418.257429	114326.469804	36.244263
1419.643283	114475.592872	36.249280
1421.191214	114625.693262	36.254298
1422.833991	114779.901425	36.259316
1424.030421	114925.555355	36.264333
1425.749902	115073.246502	36.269351
1426.783896	115222.998117	36.274368
1428.128737	115369.011198	36.279386
1429.565195	115520.426275	36.284404
1430.511031	115679.452121	36.289421
1432.480227	115832.535836	36.294439
1433.309469	115989.222092	36.299456
1434.810240	116136.114452	36.304474
1436.140994	116294.486919	36.309492
1437.455749	116438.365428	36.314509
1438.705579	116576.889503	36.319527
1440.107165	116731.460460	36.324544
1441.543858	116883.020595	36.329562
1443.087334	117036.365796	36.334580
1444.354864	117186.938807	36.339597
1445.380180	117347.367312	36.344615
1446.640585	117510.068357	36.349632
1448.883057	117663.459539	36.354650
1449.801302	117827.052346	36.359668
1451.264066	117993.376943	36.364685
1452.523318	118157.603042	36.369703
1453.990356	118319.730018	36.374720
1455.636911	118484.620248	36.379738
1457.047286	118649.865060	36.384756
1458.853144	118820.947191	36.389773
1460.344571	118984.785586	36.394791
1461.584010	119164.214876	36.399808
1463.398509	119329.729539	36.404826
1464.620251	119508.414825	36.409844
1466.210561	119680.029060	36.414861
1467.435536	119843.671612	36.419879
1468.838015	120013.261679	36.424896
1470.785511	120193.752577	36.429914
1471.922478	120374.535379	36.434932
1473.706638	120540.199526	36.439949
1475.512760	120711.505714	36.444967
1476.970894	120889.221951	36.449984
1478.761857	121057.741358	36.455002
1479.937879	121225.989347	36.460020
1481.562879	121399.559328	36.465037
1482.965247	121568.724949	36.470055
1484.286933	121751.527728	36.475072
1486.089373	121913.173697	36.480090
1487.570554	122088.900249	36.485108
1489.117493	122264.947174	36.490125
1490.946921	122428.278220	36.495143
1492.115352	122616.170357	36.500160
1494.339018	122752.256489	36.505178
1495.917884	122929.176718	36.510196
1496.816503	123103.641126	36.515213
1498.721425	123262.600034	36.520231
1500.307905	123428.675083	36.525248
1502.120583	123589.971147	36.530266
1503.358146	123760.795622	36.535284
1504.865725	123921.912175	36.540301
1506.995790	124083.947366	36.545319
1508.084153	124252.539078	36.550336
1509.704376	124403.415154	36.555354
1511.177747	124575.322781	36.560372
1512.310619	124744.556626	36.565389
1513.808266	124913.620231	36.570407
1515.203861	125087.343591	36.575424
1516.859528	125254.481097	36.580442
1517.992710	125427.904236	36.585460
1518.826531	125596.909101	36.590477
1521.040029	125777.650564	36.595495
1522.215839	125965.392367	36.600512
1523.459341	126142.277490	36.605530
1524.926550	126318.113632	36.610548
1526.382529	126515.570371	36.615565
1528.121428	126681.888845	36.620583
1529.348368	126878.190427	36.625600
1531.008150	127068.805305	36.630618
1532.496405	127252.216227	36.635636
1533.778153	127429.443497	36.640653
1535.075210	127620.878601	36.645671
1536.371617	127800.706019	36.650688
1537.797746	127971.874094	36.655706
1539.639044	128149.905455	36.660724
1541.045647	128334.754844	36.665741
1543.126161	128507.091994	36.670759
1544.452655	128685.028146	36.675776
1545.769240	128855.658658	36.680794
1547.449426	129041.953018	36.685812
1548.507874	129228.205413	36.690829
1550.382169	129411.121697	36.695847
1551.735373	129593.054120	36.700864
1553.561365	129776.119069	36.705882
1555.221281	129969.487718	36.710900
1556.703906	130156.363321	36.715917
1558.315309	130341.671787	36.720935
1559.946650	130526.774950	36.725952
1561.646867	130714.202779	36.730970
1563.536605	130904.418671	36.735988
1565.076718	131098.407426	36.741005
1567.035257	131271.751808	36.746023
1568.371277	131465.456785	36.751040
1569.950515	131658.845636	36.756058
1571.462783	131835.370362	36.761076
1572.877457	132028.266261	36.766093
1574.463722	132210.262360	36.771111
1575.740545	132421.198977	36.776128
1577.673006	132616.326197	36.781146
1579.257565	132803.540020	36.786164
1580.568161	132996.989331	36.791181
1582.530613	133190.845587	36.796199
1584.101302	133387.352176	36.801216
1585.559603	133578.522467	36.806234
1587.381297	133765.246690	36.811252
1589.156961	133959.160781	36.816269
1591.072120	134154.690885	36.821287
1592.507248	134350.512278	36.826304
1594.092332	134546.412707	36.831322
1596.044359	134734.250053	36.836340
1597.681865	134925.360193	36.841357
1599.549395	135112.450931	36.846375
1600.735022	135308.302671	36.851392
1602.573881	135504.091662	36.856410
1604.027496	135704.065517	36.861428
1605.544027	135898.053737	36.866445
1606.693916	136090.462909	36.871463
1608.574151	136274.739429	36.876480
1610.041345	136476.529189	36.881498
1611.646438	136667.626376	36.886516
1613.148084	136883.320444	36.891533
1614.941593	137078.679152	36.896551
1616.448454	137286.582789	36.901568
1617.803093	137483.864244	36.906586
1619.584565	137685.711940	36.911604
1621.124256	137897.864359	36.916621
1622.808167	138102.647761	36.921639
1624.091957	138310.679562	36.926656
1625.798472	138525.917968	36.931674
1627.150967	138733.230315	36.936692
1628.797688	138947.845462	36.941709
1630.304560	139154.666110	36.946727
1631.786745	139383.725092	36.951744
1633.326830	139588.829277	36.956762
1635.238736	139814.193998	36.961780
1636.612236	140030.506377	36.966797
1638.248187	140242.261029	36.971815
1639.959662	140468.967195	36.976832
1641.265971	140686.092529	36.981850
1643.205929	140899.059169	36.986868
1644.131208	141115.243180	36.991885
1646.417304	141316.279153	36.996903
1648.138945	141518.926736	37.001920
1649.764589	141734.687249	37.006938
1651.427774	141927.129367	37.011956
1652.976773	142137.586044	37.016973
1654.724235	142353.381116	37.021991
1656.104172	142560.134724	37.027008
1657.470336	142774.620351	37.032026
1659.298928	142985.608279	37.037044
1660.105997	143210.310528	37.042061
1662.351191	143423.697630	37.047079
1663.888022	143650.915440	37.052096
1665.095368	143889.976055	37.057114
1667.289266	144116.827212	37.062132
1668.955346	144348.203648	37.067149
1670.415100	144571.452467	37.072167
1672.325256	144811.867669	37.077184
1673.859312	145047.392725	37.082202
1674.871490	145283.266639	37.087220
1676.766185	145527.101792	37.092237
1678.916012	145772.091465	37.097255
1680.540327	146008.736542	37.102272
1682.589275	146244.288562	37.107290
1684.173167	146488.976306	37.112308
1685.835907	146725.187183	37.117325
1687.737447	146968.926622	37.122343
1689.494809	147211.725029	37.127360
1690.872996	147452.260867	37.132378
1692.908928	147689.496930	37.137396
1694.094664	147932.501908	37.142413
1696.077426	148175.675899	37.147431
1697.844694	148423.834715	37.152448
1699.257427	148690.708258	37.157466
1701.137754	148936.617965	37.162484
1702.517592	149181.794367	37.167501
1704.161655	149444.053569	37.172519
1705.955538	149700.807362	37.177536
1707.951139	149947.884256	37.182554
1709.885839	150208.134547	37.187572
1711.801316	150465.469654	37.192589
1713.324502	150697.099738	37.197607
1715.056353	150971.144764	37.202624
1717.004771	151223.515260	37.207642
1719.017196	151470.393399	37.212660
1720.685159	151728.712323	37.217677
1722.585712	151972.563699	37.222695
1724.497429	152216.554045	37.227712
1725.708492	152474.884111	37.232730
1727.726492	152717.273415	37.237748
1729.300181	152972.807514	37.242765
1730.994215	153234.379009	37.247783
1732.752614	153481.978427	37.252800
1734.388446	153735.373756	37.257818
1736.257491	153977.398181	37.262836
1737.687557	154236.527388	37.267853
1739.775536	154484.574969	37.272871
1742.264083	154741.980360	37.277888
1743.617002	154997.202530	37.282906
1745.928135	155245.066346	37.287924
1747.657702	155492.818632	37.292941
1749.284966	155730.838610	37.297959
1751.219962	155971.959889	37.302976
1752.398732	156215.446791	37.307994
1754.281322	156457.923852	37.313012
1755.597126	156721.131551	37.318029
1757.165361	156972.101571	37.323047
1759.159115	157209.753151	37.328064
1760.358333	157447.389702	37.333082
1761.890747	157693.303139	37.338100
1763.611341	157933.856458	37.343117
1765.211348	158173.617035	37.348135
1766.929796	158412.484182	37.353152
1768.284086	158677.421040	37.358170
1770.345472	158921.543341	37.363188
1771.677331	159173.587665	37.368205
1773.185375	159434.352583	37.373223
1774.716949	159702.008459	37.378240
1776.258760	159976.824048	37.383258
1777.909402	160248.843639	37.388276
1779.955370	160531.784417	37.393293
1781.524463	160806.053528	37.398311
1783.306261	161094.116150	37.403328
1785.097537	161381.378796	37.408346
1786.941811	161661.474164	37.413364
1788.338244	161950.286232	37.418381
1790.096420	162246.038664	37.423399
1792.112286	162537.689698	37.428416
1793.782268	162833.014207	37.433434
1795.300896	163127.347949	37.438452
1797.424619	163436.379664	37.443469
1799.191628	163742.687928	37.448487
1801.183453	164039.910315	37.453504
1802.878698	164354.345405	37.458522
1805.104933	164650.099390	37.463540
1806.754446	164955.111156	37.468557
1808.752405	165253.175976	37.473575
1810.459853	165564.491572	37.478592
1811.770154	165867.592332	37.483610
1813.941956	166175.346944	37.488628
1816.298682	166489.562104	37.493645
1818.048140	166795.963225	37.498663
1820.181860	167092.872275	37.503680
1821.942671	167398.652163	37.508698
1823.970181	167701.814438	37.513716
1826.096644	167999.998163	37.518733
1827.952153	168303.342167	37.523751
1830.125166	168603.882819	37.528768
1832.199190	168902.662568	37.533786
1834.066370	169192.283095	37.538804
1835.942103	169490.296240	37.543821
1837.528019	169794.044044	37.548839
1839.502110	170085.289444	37.553856
1841.379675	170388.384869	37.558874
1842.813465	170683.183087	37.563892
1844.590283	170981.560538	37.568909
1846.562785	171281.749858	37.573927
1849.108973	171576.505468	37.578944
1851.479207	171869.791316	37.583962
1852.994098	172154.894527	37.588980
1855.172322	172449.494959	37.593997
1856.833011	172743.008893	37.599015
1858.908325	173018.669940	37.604032
1860.407972	173314.534798	37.609050
1862.363598	173613.859805	37.614068
1864.426888	173892.979633	37.619085
1865.986716	174186.400447	37.624103
1867.987096	174470.573180	37.629120
1869.863928	174764.505512	37.634138
1871.731630	175069.830480	37.639156
1873.522723	175358.356280	37.644173
1874.837631	175648.011166	37.649191
1876.610465	175945.925815	37.654208
1878.390731	176245.414972	37.659226
1880.093378	176546.517283	37.664244
1881.930822	176843.942599	37.669261
1884.026086	177136.389196	37.674279
1886.245584	177404.004821	37.679296
1887.628047	177683.053175	37.684314
1889.223299	177969.053493	37.689332
1891.444355	178250.944644	37.694349
1893.117242	178540.160218	37.699367
1895.012543	178827.462754	37.704384
1896.369257	179127.066163	37.709402
1898.320432	179420.533506	37.714420
1900.261430	179723.171899	37.719437
1902.023899	180033.255200	37.724455
1903.575673	180327.905211	37.729472
1905.514909	180643.677592	37.734490
1906.894189	180955.728555	37.739508
1908.956107	181278.316070	37.744525
1910.914498	181594.317358	37.749543
1912.752126	181917.043620	37.754560
1914.774187	182242.637691	37.759578
1917.020141	182553.060692	37.764596
1919.170782	182878.459173	37.769613
1921.037609	183207.280933	37.774631
1922.822258	183532.560822	37.779648
1924.971213	183860.172581	37.784666
1926.811521	184181.280621	37.789684
1928.969933	184505.616649	37.794701
1930.493741	184847.171338	37.799719
1932.361027	185171.859646	37.804736
1934.628096	185521.657218	37.809754
1935.978477	185844.040635	37.814772
1938.048413	186249.266863	37.819789
1939.535964	186604.777296	37.824807
1941.591401	186958.346410	37.829824
1943.624446	187318.752659	37.834842
1945.149674	187658.589335	37.839860
1947.564821	188012.639383	37.844877
1949.484670	188372.025422	37.849895
1952.000500	188724.309551	37.854912
1953.882256	189088.301239	37.859930
1955.710891	189441.558206	37.864948
1957.681833	189792.203336	37.869965
1959.564791	190150.457883	37.874983
1961.562498	190501.202638	37.880000
1963.799254	190866.592617	37.885018
1965.440528	191223.846703	37.890036
1967.808183	191575.832537	37.895053
1970.246401	191936.597009	37.900071
1972.005505	192291.930929	37.905088
1973.802581	192646.497959	37.910106
1975.737568	192999.495107	37.915124
1978.263308	193351.690096	37.920141
1980.170232	193699.588033	37.925159
1982.355514	194051.787164	37.930176
1984.547873	194404.570386	37.935194
1986.813006	194748.757678	37.940212
1989.391523	195079.053479	37.945229
1991.360021	195427.124284	37.950247
1993.393097	195751.892976	37.955264
1995.594198	196092.639138	37.960282
1997.622544	196417.029134	37.965300
1999.780489	196746.581618	37.970317
2001.939438	197072.883328	37.975335
2004.219151	197406.914476	37.980352
2005.860053	197725.068198	37.985370
2007.580462	198073.844678	37.990388
2009.933497	198390.085502	37.995405
2011.289301	198724.390469	38.000423
2013.467747	199052.141482	38.005440
2015.729077	199373.123394	38.010458
2016.785472	199693.429836	38.015476
2018.862380	200003.671328	38.020493
2020.564615	200328.146093	38.025511
2022.486995	200640.851480	38.030528
2024.264060	200966.484387	38.035546
2025.826754	201298.451053	38.040564
2027.823443	201634.567617	38.045581
2029.371316	201980.255170	38.050599
2031.527857	202311.648772	38.055616
2033.248169	202664.575941	38.060634
2034.993796	203017.449076	38.065652
2037.011262	203372.261999	38.070669
2039.107378	203740.450530	38.075687
2040.733053	204110.008547	38.080704
2042.654841	204474.440675	38.085722
2044.617489	204843.160200	38.090740
2046.561546	205221.460164	38.095757
2048.482573	205603.955902	38.100775
2050.562219	205994.124749	38.105792
2052.728678	206378.336548	38.110810
2054.884912	206783.914533	38.115828
2056.656752	207151.753439	38.120845
2059.103399	207548.167987	38.125863
2061.527280	207940.496888	38.130880
2063.660437	208336.275732	38.135898
2065.364649	208729.810319	38.140916
2067.596629	209107.767455	38.145933
2070.064825	209511.498131	38.150951
2072.043413	209917.642763	38.155968
2074.378125	210307.626899	38.160986
2076.376850	210706.859929	38.166004
2078.478387	211104.019876	38.171021
2081.037788	211492.421156	38.176039
2082.984122	211882.950661	38.181056
2085.288171	212283.992883	38.186074
2087.299907	212688.561421	38.191092
2089.744769	213091.538867	38.196109
2091.775744	213484.089542	38.201127
2093.311838	213886.447303	38.206144
2095.939511	214281.319397	38.211162
2097.874552	214658.466330	38.216180
2100.655272	215055.906642	38.221197
2103.136447	215450.142311	38.226215
2105.451210	215839.348925	38.231232
2107.611208	216223.118180	38.236250
2109.932191	216608.640998	38.241268
2111.988916	216993.798821	38.246285
2113.760259	217373.717376	38.251303
2115.910522	217765.923553	38.256320
2118.340153	218149.144383	38.261338
2120.013572	218544.397623	38.266356
2121.891733	218915.256897	38.271373
2124.312816	219307.955531	38.276391
2126.514169	219704.118149	38.281408
2128.779702	220087.365789	38.286426
2130.664806	220492.063017	38.291444
2132.843226	220882.818816	38.296461
2134.719051	221275.908258	38.301479
2136.705737	221667.303956	38.306496
2139.324591	222065.511332	38.311514
2140.980016	222454.799545	38.316532
2143.359189	222854.035261	38.321549
2145.269349	223244.808320	38.326567
2147.204720	223648.736869	38.331584
2149.917090	224036.997284	38.336602
2151.799851	224439.486150	38.341620
2154.000982	224835.904757	38.346637
2156.076738	225219.463039	38.351655
2157.940714	225600.005815	38.356672
2160.489337	225970.712281	38.361690
2163.396750	226329.346768	38.366708
2165.672410	226685.488344	38.371725
2167.647440	227053.769032	38.376743
2170.016773	227412.436378	38.381760
2172.505871	227766.791748	38.386778
2174.384112	228133.842552	38.391796
2176.599217	228484.709269	38.396813
2178.818500	228850.614468	38.401831
2181.001339	229207.328971	38.406848
2183.578710	229570.891875	38.411866
2185.176058	229932.778088	38.416884
2187.090521	230302.439264	38.421901
2189.012269	230678.323146	38.426919
2190.826096	231063.445316	38.431936
2193.043858	231443.118788	38.436954
2194.826351	231846.460110	38.441972
2196.591923	232246.501312	38.446989
2198.788363	232640.429070	38.452007
2200.482113	233063.573123	38.457024
2202.889873	233468.162497	38.462042
2204.893311	233891.562571	38.467060
2207.000097	234311.084821	38.472077
2208.950958	234733.806457	38.477095
2210.816171	235170.487741	38.482112
2213.106806	235603.368025	38.487130
2215.231992	236043.793132	38.492148
2217.169964	236493.773300	38.497165
2219.674717	236930.962876	38.502183
2221.601836	237395.830239	38.507200
2223.934632	237848.440105	38.512218
2225.836567	238315.342454	38.517236
2228.342912	238763.859498	38.522253
2230.837425	239230.058619	38.527271
2232.937291	239695.607151	38.532288
2234.721103	240162.423504	38.537306
2236.831616	240632.719330	38.542324
2239.263687	241104.259888	38.547341
2241.861093	241574.706947	38.552359
2243.786720	242058.187979	38.557376
2246.468767	242528.137457	38.562394
2249.289192	242989.960883	38.567412
2251.926591	243451.202225	38.572429
2254.794628	243918.732129	38.577447
2257.140747	244382.760465	38.582464
2259.780666	244843.515925	38.587482
2261.698429	245290.360369	38.592500
2264.333269	245740.648673	38.597517
2267.375099	246176.697879	38.602535
2269.425710	246630.479115	38.607552
2271.774909	247072.730815	38.612570
2273.884422	247525.586303	38.617588
2276.340490	247964.415351	38.622605
2278.445192	248408.403948	38.627623
2281.386606	248830.796163	38.632640
2285.778811	249217.169603	38.637658
2289.149617	249616.656345	38.642676
2291.197452	250020.691841	38.647693
2293.564464	250411.010299	38.652711
2295.865064	250796.232342	38.657728
2298.606315	251174.399323	38.662746
2300.554384	251565.796317	38.667764
2302.415699	251955.122887	38.672781
2304.805008	252342.664391	38.677799
2306.322512	252731.915513	38.682816
2308.361661	253115.216644	38.687834
2310.578185	253505.449266	38.692852
2312.398151	253892.033930	38.697869
2314.164676	254272.199283	38.702887
2315.770264	254659.780523	38.707904
2318.175796	255043.781616	38.712922
2319.531417	255438.639033	38.717940
2321.743591	255856.019993	38.722957
2323.713640	256260.203313	38.727975
2325.893027	256680.533378	38.732992
2327.816345	257097.371212	38.738010
2330.190134	257529.606818	38.743028
2332.315025	257966.502677	38.748045
2334.590177	258400.147749	38.753063
2336.474579	258846.984310	38.758080
2338.842875	259294.759981	38.763098
2340.679382	259749.652721	38.768116
2342.769721	260221.293935	38.773133
2344.985316	260684.328473	38.778151
2346.836910	261166.290207	38.783168
2349.700464	261643.622027	38.788186
2352.352640	262124.540751	38.793204
2354.031047	262612.949541	38.798221
2356.896239	263096.751928	38.803239
2359.001802	263585.928134	38.808256
2361.464693	264071.846178	38.813274
2364.312483	264569.487460	38.818292
2367.174353	265063.720695	38.823309
2369.154291	265550.392876	38.828327
2371.745194	266051.013373	38.833344
2374.353816	266541.367466	38.838362
2376.817498	267038.243825	38.843380
2379.632448	267528.916542	38.848397
2382.569388	268012.405417	38.853415
2385.202709	268499.113938	38.858432
2388.096246	268983.036472	38.863450
2390.547978	269457.450167	38.868468
2392.938596	269945.103366	38.873485
2395.732656	270421.795500	38.878503
2397.960511	270911.399161	38.883520
2400.650054	271380.457810	38.888538
2402.941182	271851.836390	38.893556
2405.233209	272337.485668	38.898573
2408.110575	272808.945691	38.903591
2409.874731	273284.919310	38.908608
2412.064541	273762.678037	38.913626
2414.827644	274242.148045	38.918644
2416.967787	274727.604309	38.923661
2419.599782	275212.346298	38.928679
2421.768009	275698.884575	38.933696
2424.157236	276191.023537	38.938714
2426.896307	276683.003487	38.943732
2428.739753	277187.766975	38.948749
2430.877555	277673.917151	38.953767
2433.047148	278186.572394	38.958784
2435.479707	278686.714188	38.963802
2437.797811	279184.686566	38.968820
2439.987891	279696.363592	38.973837
2442.516412	280214.282441	38.978855
2444.586606	280739.887472	38.983872
2447.010159	281262.691188	38.988890
2449.053901	281788.496053	38.993908
2451.697862	282318.216010	38.998925
2453.884098	282843.991064	39.003943
2456.348351	283373.096375	39.008960
2458.549121	283903.686186	39.013978
2460.850841	284446.292780	39.018996
2463.038259	284991.579229	39.024013
2466.182453	285527.367836	39.029031
2468.655994	286056.425940	39.034048
2471.579873	286568.930000	39.039066
2474.289407	287059.092746	39.044084
2476.343728	287565.249425	39.049101
2478.809903	288067.757855	39.054119
2481.369576	288579.033480	39.059136
2484.080914	289081.470571	39.064154
2486.936801	289574.587970	39.069172
2489.617047	290084.817249	39.074189
2492.244639	290564.479747	39.079207
2495.224530	291058.378852	39.084224
2498.511638	291542.400047	39.089242
2501.899405	292014.874514	39.094260
2504.369357	292500.132569	39.099277
2506.657235	292976.350845	39.104295
2508.791071	293462.796109	39.109312
2511.050611	293949.903413	39.114330
2513.172982	294431.670922	39.119348
2515.264633	294929.028336	39.124365
2517.835705	295432.400333	39.129383
2520.453220	295936.497060	39.134400
2522.918391	296438.759761	39.139418
2525.380452	296955.972354	39.144436
2527.719400	297459.642160	39.149453
2530.277656	297977.744518	39.154471
2532.358690	298500.206922	39.159488
2534.468040	299034.516012	39.164506
2536.803437	299560.254696	39.169524
2538.779504	300113.513024	39.174541
2541.629969	300644.314777	39.179559
2544.285119	301206.367125	39.184576
2546.363806	301766.777087	39.189594
2549.073237	302313.095397	39.194612
2551.678455	302868.690105	39.199629
2554.212084	303434.139668	39.204647
2557.354199	303992.837551	39.209664
2559.708980	304551.448902	39.214682
2562.632809	305106.843373	39.219700
2564.940975	305673.928294	39.224717
2567.697272	306231.900469	39.229735
2569.852418	306805.418766	39.234752
2572.310082	307381.244121	39.239770
2575.319205	307950.123577	39.244788
2577.675626	308535.393896	39.249805
2580.089378	309099.631581	39.254823
2583.202707	309683.882048	39.259840
2584.920334	310262.987103	39.264858
2588.162160	310842.533328	39.269876
2590.480654	311431.226623	39.274893
2593.116570	312021.081539	39.279911
2596.197780	312605.910567	39.284928
2598.716229	313191.733589	39.289946
2601.811783	313761.926837	39.294964
2603.961954	314358.375984	39.299981
2606.502108	314947.802756	39.304999
2608.794767	315539.265403	39.310016
2611.358046	316144.103616	39.315034
2614.071552	316719.775899	39.320052
2616.360828	317327.737021	39.325069
2618.557881	317933.039539	39.330087
2621.748584	318537.189433	39.335104
2623.907202	319143.242657	39.340122
2626.843516	319742.492379	39.345140
2629.499955	320351.318894	39.350157
2632.198039	320960.993120	39.355175
2635.125558	321555.575214	39.360192
2637.679253	322157.819767	39.365210
2640.715576	322752.495042	39.370228
2643.138945	323347.764787	39.375245
2645.403757	323920.493056	39.380263
2648.139925	324501.285093	39.385280
2650.651298	325070.685867	39.390298
2653.541768	325628.170484	39.395316
2656.022701	326210.069124	39.400333
2658.610642	326786.030994	39.405351
2661.014443	327360.262628	39.410368
2663.425849	327948.819884	39.415386
2665.950654	328543.795134	39.420404
2668.892003	329133.495594	39.425421
2671.520967	329708.394062	39.430439
2674.589569	330307.266641	39.435456
2676.821854	330903.393381	39.440474
2679.812272	331502.792481	39.445492
2682.512855	332108.138346	39.450509
2684.797097	332707.171921	39.455527
2687.628734	333303.675550	39.460544
2689.866836	333926.644680	39.465562
2692.611635	334540.087997	39.470580
2695.494949	335164.382144	39.475597
2697.841870	335788.368805	39.480615
2700.134444	336428.359427	39.485632
2702.740838	337066.666692	39.490650
2705.233736	337712.716882	39.495668
2708.353392	338358.886357	39.500685
2711.492635	338993.728763	39.505703
2714.203111	339637.478680	39.510720
2717.155655	340293.074779	39.515738
2719.735981	340936.339612	39.520756
2722.086090	341594.490979	39.525773
2724.794594	342259.853150	39.530791
2727.754372	342908.272800	39.535808
2730.224216	343576.005620	39.540826
2732.876454	344241.440077	39.545844
2735.220063	344916.419698	39.550861
2737.820492	345600.652974	39.555879
2740.667851	346291.402034	39.560896
2743.149320	346978.745160	39.565914
2745.929827	347668.107044	39.570932
2748.572065	348350.553637	39.575949
2751.478451	349052.799574	39.580967
2753.942967	349744.880724	39.585984
2756.686956	350454.728954	39.591002
2759.586236	351162.788074	39.596020
2762.455543	351877.124387	39.601037
2765.070477	352584.334607	39.606055
2768.340396	353294.571166	39.611072
2771.141423	354009.605905	39.616090
2773.879714	354715.786290	39.621108
2776.918601	355435.720879	39.626125
2779.713929	356139.882990	39.631143
2782.727948	356851.651109	39.636160
2785.357357	357564.350016	39.641178
2788.301897	358263.497460	39.646196
2792.259725	358940.468359	39.651213
2796.477753	359608.917373	39.656231
2799.911067	360279.729757	39.661248
2802.769281	360960.324783	39.666266
2805.376955	361620.818071	39.671284
2808.661687	362292.495837	39.676301
2811.117477	362947.280531	39.681319
2814.073062	363609.576514	39.686336
2816.699442	364261.618987	39.691354
2819.370715	364919.367728	39.696372
2821.810540	365590.772417	39.701389
2824.676853	366248.942333	39.706407
2827.142608	366914.610226	39.711424
2829.794038	367578.535955	39.716442
2832.669572	368202.043138	39.721460
2835.493627	368832.310627	39.726477
2838.074413	369467.746001	39.731495
2840.668186	370104.178654	39.736512
2843.264085	370752.049728	39.741530
2845.866600	371385.031272	39.746548
2848.991247	372015.738172	39.751565
2851.727535	372665.899373	39.756583
2854.484544	373312.875012	39.761600
2856.751869	373973.694359	39.766618
2859.468693	374628.322039	39.771636
2861.918525	375299.063053	39.776653
2864.134592	375992.320461	39.781671
2866.970219	376680.270358	39.786688
2869.745795	377363.474808	39.791706
2871.967227	378074.841280	39.796724
2874.900738	378789.396374	39.801741
2877.670937	379512.240764	39.806759
2880.403744	380233.602058	39.811776
2883.223726	380962.047513	39.816794
2886.032598	381697.186477	39.821812
2889.189930	382429.667027	39.826829
2891.515381	383192.091627	39.831847
2894.497640	383934.763583	39.836864
2897.393618	384688.697366	39.841882
2900.414086	385448.870084	39.846900
2903.306913	386214.509932	39.851917
2906.017756	386980.610749	39.856935
2909.021671	387736.007184	39.861952
2912.296418	388517.394791	39.866970
2914.811743	389303.383218	39.871988
2918.201887	390080.703045	39.877005
2921.738354	390851.898984	39.882023
2925.091991	391627.859058	39.887040
2928.006213	392404.470518	39.892058
2931.136122	393183.757869	39.897076
2934.210462	393948.446707	39.902093
2936.989301	394727.941435	39.907111
2940.228398	395489.669701	39.912128
2943.397650	396254.067801	39.917146
2946.703561	397018.673195	39.922164
2950.224267	397802.558885	39.927181
2953.242033	398568.222061	39.932199
2956.288410	399340.132774	39.937216
2958.805378	400108.506400	39.942234
2961.653600	400881.966067	39.947252
2964.826760	401648.870507	39.952269
2967.389163	402422.981046	39.957287
2970.540583	403192.772981	39.962304
2973.634335	403972.973731	39.967322
2976.633781	404736.157793	39.972340
2980.068858	405498.033760	39.977357
2983.247947	406265.895253	39.982375
2986.562602	407023.183792	39.987392
2989.433526	407788.612042	39.992410
2992.490698	408548.874349	39.997428
2995.646575	409312.384113	40.002445
2998.038896	410073.355238	40.007463
3001.029236	410836.483727	40.012480
3003.645369	411607.536378	40.017498
3006.799980	412367.904326	40.022516
3010.694561	413115.786574	40.027533
3014.107546	413880.614249	40.032551
3017.496030	414632.923760	40.037568
3020.544037	415384.703408	40.042586
3022.613513	416143.437500	40.047604
3026.105559	416894.740666	40.052621
3028.877803	417640.009112	40.057639
3031.664416	418376.600271	40.062656
3034.278294	419097.514070	40.067674
3036.832129	419819.626145	40.072692
3039.493325	420552.872911	40.077709
3042.216477	421293.416822	40.082727
3045.077223	422036.744634	40.087744
3047.990376	422781.301636	40.092762
3050.954305	423527.745181	40.097780
3054.633681	424276.325464	40.102797
3057.378682	425038.776206	40.107815
3060.496122	425792.899208	40.112832
3063.499226	426559.550030	40.117850
3066.353969	427325.133078	40.122868
3069.359670	428094.606558	40.127885
3072.046902	428884.472121	40.132903
3075.399236	429660.049025	40.137920
3078.520510	430443.617998	40.142938
3081.409847	431244.731159	40.147956
3084.546227	432032.177111	40.152973
3087.475862	432833.674009	40.157991
3090.491516	433645.636707	40.163008
3093.474816	434457.267278	40.168026
3096.719890	435268.368254	40.173044
3099.828559	436085.722365	40.178061
3103.061609	436908.075364	40.183079
3106.111606	437720.517921	40.188096
3109.184442	438560.357954	40.193114
3112.311374	439383.327925	40.198132
3115.953385	440210.021538	40.203149
3119.015847	441045.761469	40.208167
3122.073317	441871.614054	40.213184
3125.646166	442709.321947	40.218202
3128.883041	443546.690783	40.223220
3132.462227	444367.653628	40.228237
3135.738399	445206.607985	40.233255
3139.155399	446017.723902	40.238272
3142.299311	446853.845659	40.243290
3145.001121	447688.937347	40.248308
3148.333358	448513.540258	40.253325
3151.838543	449350.349359	40.258343
3154.719673	450178.127744	40.263360
3157.918595	451012.533951	40.268378
3161.130796	451861.339188	40.273396
3164.406937	452696.210070	40.278413
3167.393277	453540.779862	40.283431
3170.244452	454389.015566	40.288448
3173.455823	455235.589502	40.293466
3176.835726	456091.939479	40.298484
3180.156132	456936.193237	40.303501
3183.385045	457789.757726	40.308519
3186.623043	458636.566289	40.313536
3189.491021	459484.854505	40.318554
3192.427422	460345.000050	40.323572
3196.110975	461198.779311	40.328589
3199.363275	462053.087621	40.333607
3202.260565	462909.224780	40.338624
3205.630316	463764.387479	40.343642
3208.704670	464633.376819	40.348660
3212.307795	465485.287906	40.353677
3215.338427	466355.910273	40.358695
3218.368347	467215.894042	40.363712
3221.964960	468071.659412	40.368730
3224.890714	468936.816307	40.373748
3228.298792	469799.633651	40.378765
3231.226183	470668.683976	40.383783
3234.661993	471520.613780	40.388800
3238.083953	472386.470110	40.393818
3241.321382	473232.088264	40.398836
3244.524774	474058.103334	40.403853
3248.383570	474863.452881	40.408871
3251.861620	475660.250283	40.413888
3255.303756	476468.155695	40.418906
3258.664733	477278.553645	40.423924
3261.780276	478087.890006	40.428941
3264.723163	478890.558158	40.433959
3267.487826	479699.413321	40.438976
3270.690666	480519.650826	40.443994
3273.334792	481349.811055	40.449012
3276.409243	482175.778200	40.454029
3279.547112	483014.996190	40.459047
3282.503553	483863.318266	40.464064
3285.690983	484719.267698	40.469082
3288.530292	485584.696709	40.474100
3291.636146	486457.945994	40.479117
3294.787192	487333.960000	40.484135
3298.153814	488218.908075	40.489152
3301.416293	489102.712816	40.494170
3304.794223	489991.384746	40.499188
3308.232313	490888.558016	40.504205
3311.650446	491776.212253	40.509223
3314.719490	492681.294198	40.514240
3317.878137	493589.027065	40.519258
3320.701709	494509.598049	40.524276
3324.670222	495425.754610	40.529293
3328.070826	496348.236862	40.534311
3331.236557	497284.896204	40.539328
3334.276670	498214.618377	40.544346
3337.630886	499145.894093	40.549364
3341.313445	500078.972306	40.554381
3344.849353	501015.889421	40.559399
3348.190605	501962.188433	40.564416
3351.974230	502905.790019	40.569434
3354.655661	503861.277455	40.574452
3358.209742	504804.136156	40.579469
3361.757053	505769.375830	40.584487
3364.758664	506736.295539	40.589504
3368.232499	507690.447858	40.594522
3371.465121	508657.452344	40.599540
3374.643298	509634.309097	40.604557
3378.291762	510604.938423	40.609575
3381.732657	511594.193255	40.614592
3385.028153	512561.220997	40.619610
3388.554161	513545.797672	40.624628
3392.079657	514521.102026	40.629645
3395.613876	515504.331260	40.634663
3399.090601	516481.767348	40.639680
3402.708754	517467.055453	40.644698
3406.340019	518449.756896	40.649716
3410.144583	519426.177418	40.654733
3413.639616	520402.374829	40.659751
3417.222747	521382.609566	40.664768
3420.615419	522355.867072	40.669786
3424.004548	523338.954761	40.674804
3427.147541	524315.023736	40.679821
3430.826844	525293.148743	40.684839
3433.859578	526272.458019	40.689856
3437.636454	527250.624596	40.694874
3441.345275	528235.410691	40.699892
3444.931503	529214.064097	40.704909
3448.455584	530194.462384	40.709927
3451.719392	531177.790906	40.714944
3455.468665	532157.102676	40.719962
3458.521628	533134.239391	40.724980
3461.881052	534116.426615	40.729997
3465.525905	535092.670345	40.735015
3468.293420	536067.298232	40.740020
3472.513172	537014.496484	40.745024
3475.307446	537908.248414	40.750029
3478.423517	538754.432661	40.755034
3481.534129	539526.137794	40.760039
3484.656322	540270.421464	40.765044
3487.254325	540943.698687	40.770048
3490.037258	541591.855756	40.775053
3492.069667	542153.915709	40.780058
3494.744905	542675.554005	40.785063
3497.092654	543148.927997	40.790068
3498.969877	543566.016724	40.795072
3501.265102	543943.840762	40.800077
3502.858066	544261.099304	40.805082
3504.840816	544536.187853	40.810087
3506.289503	544785.147531	40.815092
3507.828658	544984.091573	40.820096
3508.781019	545157.622800	40.825101
3509.826947	545286.271983	40.830106
3511.386753	545386.371889	40.835111
3512.198711	545463.752758	40.840116
3513.443561	545497.408596	40.845120
3514.253222	545513.075695	40.850125
3514.865509	545490.648866	40.855130
3515.569889	545467.302329	40.860135
3516.423919	545421.298970	40.865140
3516.897238	545339.090584	40.870144
3516.943151	545250.359209	40.875149
3517.745801	545150.041553	40.880154
3518.416026	545007.392547	40.885159
3518.514695	544874.236747	40.890164
3519.030105	544720.945181	40.895168
3519.108579	544558.363894	40.900173
3519.544467	544382.596344	40.905178
3520.123494	544197.196437	40.910183
3519.914533	544017.801775	40.915188
3520.205974	543801.052030	40.920192
3520.057739	543600.564855	40.925197
3520.304542	543391.058728	40.930202
3520.425639	543168.539467	40.935207
3520.412086	542936.931695	40.940212
3520.197692	542704.696898	40.945216
3520.179739	542476.653149	40.950221
3520.331772	542241.133002	40.955226
3520.522920	541999.816652	40.960231
3520.324814	541765.549530	40.965236
3520.326118	541504.229262	40.970240
3520.205161	541260.532303	40.975245
3519.853911	541022.753250	40.980250
3519.985251	540775.385017	40.985255
3519.625970	540522.251588	40.990260
3519.911689	540267.201290	40.995264
3519.762859	540025.145289	41.000269
3519.134822	539768.465984	41.005274
3519.512750	539518.367862	41.010279
3519.003565	539266.591285	41.015284
3518.895160	539017.867327	41.020288
3518.585407	538776.517032	41.025293
3519.108403	538524.263172	41.030298
3518.551298	538276.701664	41.035303
3518.733185	538039.941133	41.040308
3518.443061	537791.624079	41.045312
3518.264592	537537.295760	41.050317
3517.929194	537299.243110	41.055322
3517.882876	537055.504068	41.060327
3517.503585	536806.628094	41.065332
3517.762002	536572.143662	41.070336
3517.446443	536327.577002	41.075341
3517.253240	536092.248070	41.080346
3516.900380	535862.073810	41.085351
3516.904857	535629.323031	41.090356
3516.800855	535390.997551	41.095360
3516.845062	535159.943532	41.100365
3516.605785	534933.862643	41.105370
3516.450032	534699.559478	41.110375
3516.064864	534481.648320	41.115380
3515.940131	534263.843973	41.120384
3515.884044	534038.776035	41.125389
3515.518411	533822.814041	41.130394
3515.599413	533607.181684	41.135399
3515.376558	533391.895083	41.140404
3514.934997	533172.460275	41.145408
3515.048689	532963.004566	41.150413
3515.345998	532751.956146	41.155418
3514.909000	532528.633013	41.160423
3514.421975	532325.956749	41.165428
3514.461459	532126.166001	41.170432
3514.242445	531918.910238	41.175437
3513.904887	531715.748046	41.180442
3514.249943	531520.029213	41.185447
3513.636896	531332.915741	41.190452
3513.606539	531119.223133	41.195456
3513.950641	530938.500974	41.200461
3513.481882	530746.421945	41.205466
3513.079544	530555.890772	41.210471
3513.169139	530360.597146	41.215476
3512.922272	530172.402928	41.220480
3512.892097	529994.999164	41.225485
3512.584479	529814.866466	41.230490
3512.354594	529622.381246	41.235495
3512.400440	529446.519354	41.240500
3512.223890	529274.768900	41.245504
3512.282190	529109.778385	41.250509
3511.890908	528935.538860	41.255514
3511.966440	528757.900470	41.260519
3511.371997	528593.810848	41.265524
3511.488428	528427.745106	41.270528
3511.418270	528265.735441	41.275533
3511.418691	528105.677029	41.280538
3511.430041	527939.470390	41.285543
3511.234576	527788.101457	41.290548
3511.184959	527610.315969	41.295552
3510.859196	527460.373820	41.300557
3510.234616	527302.467979	41.305562
3510.363570	527154.113735	41.310567
3510.366781	527011.166875	41.315572
3510.498960	526858.980776	41.320576
3510.569580	526711.235080	41.325581
3510.291838	526562.987867	41.330586
3510.202548	526417.429717	41.335591
3510.163071	526265.616113	41.340596
3510.190152	526116.812758	41.345600
3509.697941	525979.523197	41.350605
3509.828353	525835.234167	41.355610
3509.804274	525693.637433	41.360615
3509.561511	525557.463293	41.365620
3509.447868	525409.127280	41.370624
3509.276271	525277.221075	41.375629
3509.066041	525150.155676	41.380634
3509.694245	525011.170482	41.385639
3509.344288	524876.466975	41.390644
3509.466159	524745.769267	41.395648
3509.226723	524613.413649	41.400653
3509.273867	524470.734889	41.405658
3509.225910	524343.737310	41.410663
3508.742156	524222.700746	41.415668
3508.785724	524089.792101	41.420672
3508.772669	523959.309213	41.425677
3508.514879	523826.142559	41.430682
3508.947358	523701.633550	41.435687
3508.483720	523587.490369	41.440692
3508.855231	523459.260331	41.445696
3508.525791	523329.777805	41.450701
3507.971760	523210.556802	41.455706
3507.947152	523087.473566	41.460711
3507.830278	522978.763071	41.465716
3508.352378	522869.599571	41.470720
3507.915780	522758.972048	41.475725
3507.856858	522646.924435	41.480730
3507.883152	522526.750495	41.485735
3507.812516	522416.315131	41.490740
3507.647477	522297.478960	41.495744
3507.437081	522186.458815	41.500749
3507.629504	522081.320807	41.505754
3507.803352	521971.448398	41.510759
3507.479531	521870.873612	41.515764
3507.322583	521755.054696	41.520768
3507.321443	521648.734101	41.525773
3506.913334	521553.561707	41.530778
3507.443002	521432.745387	41.535783
3507.005253	521346.243222	41.540788
3507.133849	521238.740230	41.545792
3507.183745	521135.935005	41.550797
3506.849662	521027.091376	41.555802
3507.090855	520927.379071	41.560807
3506.872268	520834.490140	41.565812
3506.626005	520729.762614	41.570816
3506.601347	520646.920741	41.575821
3506.687095	520551.815613	41.580826
3506.820359	520446.321328	41.585831
3506.604591	520358.266482	41.590836
3507.132668	520253.717140	41.595840
3506.851288	520156.398618	41.600845
3506.270723	520068.449050	41.605850
3506.781152	519967.780672	41.610855
3506.724754	519882.973643	41.615860
3506.718294	519777.697481	41.620864
3506.584193	519683.376416	41.625869
3506.399853	519593.547834	41.630874
3506.480487	519497.327377	41.635879
3505.640598	519404.474928	41.640884
3506.127359	519314.489672	41.645888
3506.307960	519226.013012	41.650893
3505.974755	519141.597216	41.655898
3506.088229	519052.121900	41.660903
3505.931671	518968.685520	41.665908
3505.739259	518885.405406	41.670912
3505.814368	518799.361564	41.675917
3505.639104	518721.924157	41.680922
3506.031526	518635.628304	41.685927
3505.566929	518553.094118	41.690932
3506.008779	518471.779206	41.695936
3506.069645	518380.190822	41.700941
3505.759661	518311.289873	41.705946
3505.971812	518226.027513	41.710951
3505.646553	518137.068081	41.715956
3506.023060	518047.696450	41.720960
3506.186011	517970.958188	41.725965
3505.720204	517882.119771	41.730970
3505.609575	517796.703348	41.735975
3505.511133	517719.197893	41.740980
3505.827562	517644.399663	41.745984
3505.414918	517561.800993	41.750989
3505.368067	517492.804562	41.755994
3505.607298	517407.482480	41.760999
3505.320283	517326.677418	41.766004
3505.088240	517253.726586	41.771008
3505.326836	517177.526563	41.776013
3505.048942	517097.676440	41.781018
3505.052803	517022.368987	41.786023
3504.867448	516963.371896	41.791028
3504.840582	516887.564418	41.796032
3504.969041	516810.875428	41.801037
3504.978902	516748.873016	41.806042
3505.074245	516679.951180	41.811047
3504.819596	516612.948552	41.816052
3505.029943	516546.125278	41.821056
3504.950931	516468.156049	41.826061
3504.851130	516409.949799	41.831066
3505.318938	516326.450544	41.836071
3505.072811	516265.090689	41.841076
3504.970532	516185.661612	41.846080
3504.398835	516121.881718	41.851085
3504.772909	516060.928537	41.856090
3505.181520	515990.240559	41.861095
3504.853227	515922.187408	41.866100
3504.708803	515842.410035	41.871104
3504.960374	515778.651670	41.876109
3504.597614	515707.981455	41.881114
3505.025930	515645.001547	41.886119
3504.842081	515573.395396	41.891124
3504.988300	515504.812637	41.896128
3504.921322	515428.952947	41.901133
3504.551812	515366.549628	41.906138
3504.734628	515291.961036	41.911143
3504.623856	515232.138306	41.916148
3504.639922	515169.069139	41.921152
3504.642020	515102.523333	41.926157
3504.300618	515043.239807	41.931162
3504.461160	514977.424947	41.936167
3504.319468	514918.361876	41.941172
3504.328560	514858.770946	41.946176
3504.649046	514795.047728	41.951181
3504.235231	514737.488250	41.956186
3504.232558	514679.612479	41.961191
3504.144273	514622.808506	41.966196
3504.280234	514563.398221	41.971200
3504.341264	514505.511809	41.976205
3504.045866	514441.479476	41.981210
3504.372333	514380.627119	41.986215
3504.558759	514318.888795	41.991220
3504.364834	514262.200613	41.996224
3504.418814	514196.600286	42.001229
3503.890350	514150.198288	42.006234
3504.286130	514082.477141	42.011239
3504.324306	514023.180589	42.016244
3504.101226	513963.722768	42.021248
3504.089117	513903.778103	42.026253
3503.940319	513847.585379	42.031258
3504.097812	513787.865910	42.036263
3504.313646	513739.733332	42.041268
3504.218396	513675.918406	42.046272
3504.068169	513623.455971	42.051277
3503.924726	513566.152059	42.056282
3504.221088	513505.300548	42.061287
3504.123634	513458.980421	42.066292
3504.042182	513402.472897	42.071296
3504.101568	513335.657588	42.076301
3504.174961	513287.948969	42.081306
3504.449126	513221.755150	42.086311
3504.345902	513161.670198	42.091316
3504.231426	513103.149778	42.096320
3504.318421	513043.942289	42.101325
3504.348430	512980.911412	42.106330
3504.249819	512914.219505	42.111335
3504.076965	512859.892118	42.116340
3503.993874	512797.936864	42.121344
3503.830285	512743.405892	42.126349
3503.748934	512698.038741	42.131354
3504.022256	512637.892931	42.136359
3503.743439	512590.438419	42.141364
3503.864879	512531.273812	42.146368
3504.069788	512475.323034	42.151373
3504.120218	512425.547692	42.156378
3504.179209	512363.013739	42.161383
3503.994132	512307.828903	42.166388
3503.886607	512257.220339	42.171392
3503.986906	512204.562296	42.176397
3503.922376	512154.350060	42.181402
3504.075038	512096.439353	42.186407
3504.051556	512044.405059	42.191412
3503.827713	511982.115110	42.196416
3504.020837	511931.408155	42.201421
3503.658615	511878.871282	42.206426
3503.713742	511811.847627	42.211431
3503.486174	511769.223175	42.216436
3503.809789	511721.924088	42.221440
3503.913803	511662.708086	42.226445
3503.655191	511618.474377	42.231450
3503.827498	511558.793473	42.236455
3503.763597	511509.940332	42.241460
3503.847048	511467.417840	42.246464
3503.783494	511405.655069	42.251469
3503.468487	511363.395974	42.256474
3503.559022	511309.324122	42.261479
3503.338177	511266.344100	42.266484
3503.656222	511216.220242	42.271488
3503.806450	511161.432545	42.276493
3503.705644	511115.710286	42.281498
3503.596823	511063.332625	42.286503
3503.483419	511023.612961	42.291508
3503.608771	510965.348824	42.296512
3503.916479	510915.830641	42.301517
3503.687629	510864.429058	42.306522
3503.663441	510807.700399	42.311527
3503.369025	510766.142300	42.316532
3503.385337	510712.180553	42.321536
3503.535432	510665.510054	42.326541
3502.930406	510620.419366	42.331546
3503.502991	510571.665625	42.336551
3503.738919	510528.713120	42.341556
3503.473324	510480.997235	42.346560
3503.604221	510425.604511	42.351565
3503.383409	510374.704185	42.356570
3503.767875	510326.987480	42.361575
3503.192367	510282.193694	42.366580
3503.276564	510242.541930	42.371584
3503.407439	510193.300873	42.376589
3503.200992	510152.937616	42.381594
3503.376107	510108.581214	42.386599
3503.522639	510068.162786	42.391604
3503.366252	510017.553729	42.396608
3503.705396	509964.497077	42.401613
3503.341470	509927.587053	42.406618
3503.320586	509875.594733	42.411623
3503.412405	509824.189873	42.416628
3503.435183	509784.344645	42.421632
3503.593042	509736.106441	42.426637
3503.453899	509685.039610	42.431642
3503.585564	509635.090415	42.436647
3503.316627	509601.039442	42.441652
3503.194940	509556.071853	42.446656
3503.339486	509505.666294	42.451661
3502.871484	509468.367790	42.456666
3502.840871	509421.872587	42.461671
3502.961459	509381.859698	42.466676
3502.873253	509344.098292	42.471680
3503.224529	509301.678871	42.476685
3503.139679	509263.311513	42.481690
3503.312437	509219.305720	42.486695
3503.235658	509173.522967	42.491700
3503.258480	509132.717629	42.496704
3503.453497	509089.565361	42.501709
3503.347392	509044.845892	42.506714
3502.987786	509002.788370	42.511719
3503.187956	508958.928806	42.516724
3503.091695	508921.571007	42.521728
3503.542342	508869.753779	42.526733
3503.186497	508835.008376	42.531738
3503.078660	508785.900421	42.536743
3503.331768	508740.871909	42.541748
3503.093534	508689.917766	42.546752
3503.125350	508650.320111	42.551757
3503.079850	508606.548119	42.556762
3503.474395	508566.591164	42.561767
3503.302443	508528.790171	42.566772
3502.914904	508471.049460	42.571776
3502.732519	508437.537019	42.576781
3502.818173	508411.548420	42.581786
3503.255759	508365.783883	42.586791
3502.983223	508316.245985	42.591796
3502.897757	508283.474665	42.596800
3503.209059	508242.470551	42.601805
3503.032205	508207.493998	42.606810
3503.126859	508160.016821	42.611815
3503.146933	508124.706789	42.616820
3502.985980	508088.466503	42.621824
3503.069742	508042.705543	42.626829
3502.750305	508000.588348	42.631834
3502.987123	507950.616836	42.636839
3503.336849	507924.384494	42.641844
3503.083113	507870.403454	42.646848
3502.893246	507826.550637	42.651853
3502.989428	507795.212669	42.656858
3502.966737	507750.324806	42.661863
3503.001480	507713.599150	42.666868
3502.921582	507677.546960	42.671872
3502.939952	507626.448175	42.676877
3502.694755	507585.932285	42.681882
3502.807267	507552.472740	42.686887
3503.090732	507509.554097	42.691892
3502.671443	507471.687890	42.696896
3502.894365	507440.783385	42.701901
3502.908387	507417.578366	42.706906
3503.034595	507365.453040	42.711911
3502.901043	507333.746273	42.716916
3502.688353	507291.913008	42.721920
3502.897922	507248.450220	42.726925
3503.057501	507211.602956	42.731930
3503.196950	507176.625080	42.736935
3503.146898	507131.487309	42.741940
3503.106372	507083.876241	42.746944
3503.095092	507040.598511	42.751949
3502.879410	507011.728581	42.756954
3503.120041	506968.966300	42.761959
3503.260671	506919.409671	42.766964
3503.092108	506884.428564	42.771968
3503.385018	506844.432137	42.776973
3503.391334	506808.717427	42.781978
3503.255749	506755.773071	42.786983
3503.123588	506709.940531	42.791988
3503.013835	506676.009075	42.796993
3503.002182	506628.240659	42.801997
3503.076518	506587.369533	42.807002
3503.372783	506540.662676	42.812007
3503.182913	506493.325094	42.817012
3503.011118	506461.319666	42.822017
3503.172046	506411.304110	42.827021
3503.307100	506375.517837	42.832026
3503.146814	506330.092009	42.837031
3503.178000	506294.372140	42.842036
3502.975173	506250.264249	42.847041
3503.160615	506212.300581	42.852045
3502.663482	506173.938574	42.857050
3502.877692	506129.916751	42.862055
3502.769007	506094.722603	42.867060
3502.508108	506051.581603	42.872065
3502.937737	506017.362861	42.877069
3502.658399	505978.815099	42.882074
3502.849311	505941.253428	42.887079
3502.919571	505906.787666	42.892084
3502.707428	505865.605927	42.897089
3502.983814	505828.989146	42.902093
3502.834432	505788.806353	42.907098
3503.006734	505750.944397	42.912103
3502.909412	505706.112148	42.917108
3502.782864	505670.869288	42.922113
3502.590537	505632.811524	42.927117
3502.767020	505600.548179	42.932122
3502.524538	505558.966696	42.937127
3502.569195	505519.862800	42.942132
3502.341248	505499.820074	42.947137
3502.773643	505467.920190	42.952141
3502.299578	505437.523389	42.957146
3502.769708	505403.448221	42.962151
3502.741313	505360.369849	42.967156
3502.553224	505337.394687	42.972161
3503.020896	505295.146996	42.977165
3502.911206	505259.345564	42.982170
3502.848008	505216.070379	42.987175
3502.769182	505184.854803	42.992180
3502.534543	505153.764304	42.997185
3502.906246	505116.727276	43.002189
3502.788581	505084.659889	43.007194
3502.587913	505040.598375	43.012199
3502.888039	505000.999263	43.017204
3502.203664	504972.399935	43.022209
3502.381168	504927.623379	43.027213
3502.733374	504903.403097	43.032218
3502.494123	504855.361470	43.037223
3502.876851	504825.939944	43.042228
3502.738859	504799.626407	43.047233
3503.083412	504768.898996	43.052237
3502.955196	504733.502736	43.057242
3502.918950	504681.695595	43.062247
3502.882601	504647.546095	43.067252
3502.582013	504608.745691	43.072257
3502.721356	504564.377548	43.077261
3502.778359	504539.849433	43.082266
3502.745369	504487.637475	43.087271
3502.847793	504459.520102	43.092276
3502.416147	504419.326937	43.097281
3503.056771	504379.319963	43.102285
3503.015549	504336.593673	43.107290
3502.918623	504307.548437	43.112295
3503.115955	504270.233649	43.117300
3502.693814	504231.097973	43.122305
3503.257795	504187.318467	43.127309
3503.006838	504156.581511	43.132314
3502.559710	504124.664151	43.137319
3502.728560	504076.253693	43.142324
3502.758488	504043.051047	43.147329
3502.803930	504002.378849	43.152333
3502.040132	503974.698042	43.157338
3502.547678	503937.334117	43.162343
3503.045957	503896.692060	43.167348
3502.722592	503871.162470	43.172353
3502.749647	503826.254534	43.177357
3502.607154	503795.853104	43.182362
3502.293064	503753.520719	43.187367
3502.664211	503726.318723	43.192372
3502.348600	503686.155902	43.197377
3502.416992	503658.042259	43.202381
3502.163968	503631.441756	43.207386
3502.557547	503592.530585	43.212391
3502.699135	503561.125816	43.217396
3502.588108	503536.723047	43.222401
3502.756236	503496.736695	43.227405
3502.558220	503462.205898	43.232410
3502.645407	503434.896176	43.237415
3502.796625	503398.191765	43.242420
3502.546823	503370.379352	43.247425
3502.797617	503321.247231	43.252429
3502.490591	503294.452686	43.257434
3502.313021	503261.785084	43.262439
3502.442257	503223.670889	43.267444
3502.450876	503195.565646	43.272449
3501.782627	503158.281760	43.277453
3502.425493	503137.343382	43.282458
3502.636440	503110.316523	43.287463
3502.667764	503081.299311	43.292468
3502.388366	503049.858027	43.297473
3502.723260	503006.161044	43.302477
3502.270061	502975.049381	43.307482
3502.848653	502935.199428	43.312487
3502.469045	502905.236672	43.317492
3501.893161	502873.437484	43.322497
3502.405621	502846.312755	43.327501
3502.383623	502818.362913	43.332506
3502.441976	502780.662238	43.337511
3502.723211	502752.665083	43.342516
3502.134748	502729.445307	43.347521
3502.414697	502689.187031	43.352525
3502.364307	502660.433978	43.357530
3502.469181	502633.523651	43.362535
3502.207436	502595.569556	43.367540
3501.929531	502573.360821	43.372545
3502.359809	502543.069452	43.377549
3502.126085	502522.367510	43.382554
3502.185944	502495.615305	43.387559
3502.348304	502459.310443	43.392564
3502.302842	502442.514855	43.397569
3502.405947	502400.819997	43.402573
3502.575753	502382.779833	43.407578
3502.375113	502341.283446	43.412583
3502.681681	502304.501624	43.417588
3502.333186	502275.138226	43.422593
3502.460246	502240.503461	43.427597
3502.365010	502210.696848	43.432602
3502.581765	502175.543375	43.437607
3502.749326	502141.053448	43.442612
3502.211913	502109.095209	43.447617
3502.472769	502080.847628	43.452621
3502.486210	502055.312870	43.457626
3502.372843	502018.141529	43.462631
3502.903989	501991.163675	43.467636
3502.876469	501965.534212	43.472641
3502.493882	501923.207115	43.477645
3502.274814	501884.538069	43.482650
3502.451079	501853.578340	43.487655
3502.709914	501817.155935	43.492660
3502.353383	501787.288189	43.497665
3502.784666	501745.388994	43.502669
3502.600406	501716.503516	43.507674
3502.391821	501682.171952	43.512679
3502.234462	501653.584929	43.517684
3502.226473	501622.047843	43.522689
3502.589138	501587.374855	43.527693
3501.996410	501569.200030	43.532698
3502.105873	501535.726937	43.537703
3502.197025	501512.702218	43.542708
3502.394127	501493.294231	43.547713
3502.441156	501454.683553	43.552717
3502.879749	501418.232175	43.557722
3502.499385	501377.568390	43.562727
3502.587668	501361.154435	43.567732
3502.314454	501317.345141	43.572737
3502.654131	501295.492503	43.577741
3502.561823	501253.723832	43.582746
3502.507558	501224.867608	43.587751
3502.794306	501184.099469	43.592756
3502.477328	501160.633072	43.597761
3502.744820	501119.110802	43.602765
3502.723592	501087.877396	43.607770
3502.692288	501048.874123	43.612775
3502.606568	501012.251001	43.617780
3502.692321	500979.083098	43.622785
3502.601133	500948.163060	43.627789
3502.538658	500922.638123	43.632794
3502.389930	500876.789573	43.637799
3502.601983	500837.949722	43.642804
3502.329105	500809.177156	43.647809
3502.426089	500771.868963	43.652813
3502.426842	500742.044396	43.657818
3502.367677	500707.283560	43.662823
3502.426699	500693.548030	43.667828
3502.061199	500665.041915	43.672833
3502.433253	500623.804751	43.677837
3502.222472	500602.591847	43.682842
3502.293772	500566.044098	43.687847
3502.265920	500531.479831	43.692852
3502.183301	500512.214995	43.697857
3502.442533	500474.123812	43.702861
3502.295988	500461.429361	43.707866
3502.131962	500430.469092	43.712871
3502.384276	500396.617891	43.717876
3502.173292	500369.702054	43.722881
3502.455328	500333.120928	43.727885
3502.483894	500305.259310	43.732890
3502.346292	500279.038411	43.737895
3502.726356	500240.978283	43.742900
3502.548193	500216.479436	43.747905
3502.076386	500181.579693	43.752909
3502.272056	500147.585330	43.757914
3502.393889	500119.910710	43.762919
3502.384749	500085.443406	43.767924
3502.622723	500064.563621	43.772929
3502.529158	500022.690680	43.777933
3502.608783	499993.054175	43.782938
3502.555219	499961.924321	43.787943
3502.559117	499933.662094	43.792948
3502.199138	499899.349881	43.797953
3502.140197	499866.757105	43.802957
3502.530714	499829.602695	43.807962
3502.675168	499802.933308	43.812967
3502.509846	499776.312077	43.817972
3502.126573	499743.214349	43.822977
3502.464021	499718.836302	43.827981
3502.579750	499682.430832	43.832986
3502.271630	499643.870621	43.837991
3502.409888	499613.012983	43.842996
3502.469576	499583.984373	43.848001
3502.370651	499554.576638	43.853005
3502.448581	499524.838511	43.858010
3502.395202	499500.319043	43.863015
3502.120882	499452.618214	43.868020
3502.135777	499440.755724	43.873025
3502.102038	499404.877512	43.878029
3501.935613	499375.227574	43.883034
3502.321526	499349.024478	43.888039
3502.895624	499320.773276	43.893044
3502.308764	499289.119343	43.898049
3502.340727	499262.315067	43.903053
3502.332987	499235.516921	43.908058
3502.246608	499205.450426	43.913063
3502.471492	499166.250846	43.918068
3502.319365	499149.013825	43.923073
3502.771506	499115.128564	43.928077
3502.470400	499077.373290	43.933082
3502.478013	499039.065174	43.938087
3502.715583	499012.884562	43.943092
3502.320907	498975.547350	43.948097
3502.257716	498934.877862	43.953101
3502.188115	498919.242792	43.958106
3501.950117	498899.242946	43.963111
3502.373269	498851.784920	43.968116
3501.851659	498830.113098	43.973121
3502.562801	498792.149100	43.978125
3502.208875	498763.183226	43.983130
3501.922025	498751.013834	43.988135
3502.146924	498713.529068	43.993140
3501.988062	498688.822770	43.998145
3502.184645	498656.490366	44.003149
3502.146938	498633.783990	44.008154
3502.107070	498607.544885	44.013159
3502.291733	498579.857578	44.018164
3502.266509	498558.360470	44.023169
3502.183390	498525.263750	44.028173
3502.520289	498490.637899	44.033178
3502.068881	498463.806438	44.038183
3502.691253	498444.580590	44.043188
3502.019865	498417.076661	44.048193
3502.411897	498389.104363	44.053197
3502.356334	498367.207915	44.058202
3502.031500	498330.665754	44.063207
3502.494271	498303.439378	44.068212
3502.263762	498273.696239	44.073217
3502.515297	498226.565738	44.078221
3502.297736	498207.571232	44.083226
3502.154293	498179.076183	44.088231
3502.402331	498143.302456	44.093236
3502.320334	498118.431816	44.098241
3502.099877	498075.563583	44.103245
3501.985991	498055.139483	44.108250
3502.048194	498028.933935	44.113255
3502.012589	497996.787633	44.118260
3502.216287	497977.273010	44.123265
3502.244678	497949.760258	44.128269
3502.277786	497921.540081	44.133274
3502.157568	497898.946357	44.138279
3502.638729	497873.331503	44.143284
3502.162088	497842.868676	44.148289
3501.918789	497802.930723	44.153293
3502.201306	497783.706426	44.158298
3501.819701	497743.789835	44.163303
3501.810141	497723.248089	44.168308
3501.809402	497701.644968	44.173313
3501.867519	497680.991682	44.178317
3502.106337	497656.676040	44.183322
3501.724242	497631.699851	44.188327
3501.801946	497608.519654	44.193332
3501.887136	497590.436269	44.198337
3501.612393	497555.802449	44.203341
3502.092730	497536.193719	44.208346
3501.947402	497518.448970	44.213351
3502.358660	497481.689202	44.218356
3502.199699	497469.397892	44.223361
3502.088387	497431.608851	44.228365
3501.769491	497405.007214	44.233370
3502.113112	497388.347169	44.238375
3502.253870	497352.487265	44.243380
3502.025876	497337.783732	44.248385
3502.290386	497301.349209	44.253389
3502.084877	497280.938292	44.258394
3502.040955	497257.574565	44.263399
3502.445647	497218.240862	44.268404
3502.112288	497196.133517	44.273409
3502.177642	497172.348837	44.278413
3501.954040	497154.969168	44.283418
3501.742352	497132.085641	44.288423
3502.033627	497107.559023	44.293428
3501.831007	497085.734030	44.298433
3502.262919	497051.291923	44.303437
3502.087631	497032.390275	44.308442
3502.074347	497005.336541	44.313447
3502.062466	496977.222512	44.318452
3501.903353	496959.125892	44.323457
3501.780800	496921.135383	44.328461
3502.034132	496904.438366	44.333466
3501.735631	496873.693423	44.338471
3502.139259	496845.211618	44.343476
3501.619377	496833.177853	44.348481
3502.116604	496807.710088	44.353485
3501.966488	496775.982768	44.358490
3501.793952	496745.470347	44.363495
3501.796682	496715.182982	44.368500
3501.941977	496706.023825	44.373505
3502.086183	496683.336612	44.378509
3501.772971	496648.858084	44.383514
3502.039341	496632.259689	44.388519
3502.001809	496605.713783	44.393524
3502.236502	496585.283881	44.398529
3502.475210	496550.719239	44.403533
3502.248128	496519.356698	44.408538
3501.957849	496495.727229	44.413543
3502.292325	496478.158960	44.418548
3502.224807	496462.722874	44.423553
3502.010199	496422.120487	44.428557
3501.815394	496398.627443	44.433562
3501.862633	496381.406634	44.438567
3501.906902	496352.676927	44.443572
3501.503228	496340.321797	44.448577
3501.769913	496303.026323	44.453581
3502.019830	496286.177703	44.458586
3501.820972	496256.829405	44.463591
3501.870476	496240.314798	44.468596
3501.681501	496223.483923	44.473601
3501.883418	496205.784520	44.478605
3501.864405	496177.972963	44.483610
3502.135550	496155.315669	44.488615
3502.206715	496117.292949	44.493620
3501.990257	496097.841227	44.498625
3501.945546	496075.182481	44.503629
3501.870075	496041.624672	44.508634
3501.818473	496026.639980	44.513639
3502.031687	495988.090017	44.518644
3501.675725	495985.015635	44.523649
3501.822196	495956.925507	44.528653
3502.010693	495942.509139	44.533658
3501.940604	495917.380532	44.538663
3502.077687	495883.637846	44.543668
3501.666979	495867.901176	44.548673
3501.885630	495847.270830	44.553677
3502.141342	495814.468671	44.558682
3501.920756	495801.529304	44.563687
3502.074932	495783.332012	44.568692
3502.045697	495763.749754	44.573697
3502.002004	495727.712691	44.578701
3502.204163	495705.166409	44.583706
3502.353891	495676.671390	44.588711
3502.385241	495646.730760	44.593716
3501.778797	495622.846203	44.598721
3501.748070	495596.650805	44.603725
3501.967731	495580.108985	44.608730
3501.876132	495548.268964	44.613735
3502.059660	495516.739439	44.618740
3502.061265	495505.279711	44.623745
3502.100556	495461.202373	44.628749
3501.996866	495447.436784	44.633754
3501.728129	495427.840870	44.638759
3502.111907	495398.046828	44.643764
3501.910959	495376.370500	44.648769
3501.696381	495345.306425	44.653773
3502.026263	495330.816980	44.658778
3501.860604	495315.344488	44.663783
3501.917923	495278.836269	44.668788
3501.820096	495260.324169	44.673793
3501.595971	495235.268861	44.678797
3501.748280	495208.589945	44.683802
3501.824063	495191.868149	44.688807
3501.982719	495169.075406	44.693812
3501.864479	495161.723234	44.698817
3501.817970	495129.572398	44.703821
3501.666940	495117.126447	44.708826
3501.668524	495103.091738	44.713831
3501.999928	495080.322461	44.718836
3502.044320	495053.962965	44.723841
3501.899305	495030.359037	44.728845
3502.040203	494998.582627	44.733850
3501.644575	494981.479595	44.738855
3502.000096	494945.378512	44.743860
3501.738509	494930.677812	44.748865
3502.029388	494907.813610	44.753869
3502.023801	494886.308105	44.758874
3501.494996	494862.460725	44.763879
3501.878254	494844.176153	44.768884
3501.769061	494829.199214	44.773889
3501.848257	494803.035797	44.778893
3501.847311	494774.865407	44.783898
3501.953445	494744.557929	44.788903
3501.975421	494722.896444	44.793908
3502.028607	494707.742660	44.798913
3501.979304	494682.053393	44.803917
3502.224300	494650.613439	44.808922
3502.000870	494638.127868	44.813927
3501.995032	494598.800627	44.818932
3502.002327	494586.430565	44.823937
3501.928732	494556.100187	44.828941
3501.947218	494528.330192	44.833946
3501.502384	494504.065284	44.838951
3502.066223	494489.336673	44.843956
3501.716098	494465.864739	44.848961
3501.780690	494436.623305	44.853965
3501.866946	494413.790188	44.858970
3501.911406	494404.746280	44.863975
3502.163174	494372.850312	44.868980
3501.541990	494350.531075	44.873985
3501.534878	494327.712355	44.878989
3501.952055	494311.390825	44.883994
3501.598631	494295.391138	44.888999
3501.659523	494271.804452	44.894004
3501.622812	494241.871588	44.899009
3501.951333	494239.700059	44.904013
3501.987882	494195.871837	44.909018
3501.811825	494182.873643	44.914023
3501.451184	494150.769578	44.919028
3501.676897	494149.169392	44.924033
3501.936440	494113.939515	44.929037
3501.856548	494097.947538	44.934042
3501.796132	494081.397153	44.939047
3502.171964	494046.552920	44.944052
3501.975322	494030.225626	44.949057
3501.938900	493997.969805	44.954061
3501.850824	493979.151669	44.959066
3501.468822	493952.250727	44.964071
3501.891597	493923.861331	44.969076
3501.577293	493927.343449	44.974081
3501.701646	493884.156991	44.979085
3501.549643	493871.912102	44.984090
3501.533343	493855.253625	44.989095
3501.845803	493825.871449	44.994100
3501.704008	493815.896893	44.999105
3501.859971	493787.144851	45.004109
3501.650980	493764.104244	45.009114
3502.054156	493752.227260	45.014119
3501.916155	493729.427995	45.019124
3501.572536	493710.396844	45.024129
3501.797613	493690.873264	45.029133
3501.883293	493660.465792	45.034138
3501.466000	493651.796215	45.039143
3501.407212	493624.137542	45.044148
3501.526379	493620.988727	45.049153
3501.635866	493598.807105	45.054157
3501.819601	493570.353259	45.059162
3501.399770	493558.907126	45.064167
3501.539986	493534.600087	45.069172
3501.718210	493516.295310	45.074177
3501.358116	493500.548253	45.079181
3501.610562	493476.021698	45.084186
3501.400152	493470.652117	45.089191
3501.453121	493438.482157	45.094196
3501.803396	493432.066013	45.099201
3501.743006	493409.355161	45.104205
3502.002077	493369.831993	45.109210
3501.867400	493357.836435	45.114215
3501.732266	493337.156694	45.119220
3501.696896	493320.248141	45.124225
3501.756133	493304.334644	45.129229
3501.792289	493271.763023	45.134234
3501.754675	493256.722878	45.139239
3501.829601	493241.715695	45.144244
3501.682393	493216.392574	45.149249
3501.789933	493194.614579	45.154253
3501.936147	493166.165805	45.159258
3501.677624	493152.321209	45.164263
3501.838541	493126.748027	45.169268
3501.605633	493113.151862	45.174273
3501.693178	493081.632133	45.179277
3501.479832	493059.449459	45.184282
3501.569378	493052.720291	45.189287
3501.693430	493031.949306	45.194292
3501.454036	493013.002030	45.199297
3501.591747	492986.725347	45.204301
3501.957479	492978.185984	45.209306
3501.749405	492954.184657	45.214311
3501.945128	492938.401007	45.219316
3501.806504	492917.721230	45.224321
3501.734118	492893.698692	45.229325
3502.077443	492872.388451	45.234330
3501.516207	492858.439216	45.239335
3501.960934	492821.915200	45.244340
3501.811415	492815.172636	45.249345
3501.568367	492788.702400	45.254349
3502.149669	492753.873681	45.259354
3501.631104	492735.726874	45.264359
3501.607280	492712.302390	45.269364
3501.638683	492688.364356	45.274369
3501.874756	492682.622061	45.279373
3501.956826	492659.433477	45.284378
3501.701560	492639.074419	45.289383
3501.972287	492615.502965	45.294388
3502.098698	492588.267992	45.299393
3501.625009	492556.279079	45.304397
3501.815174	492542.010651	45.309402
3501.510538	492528.778564	45.314407
3501.714521	492509.559687	45.319412
3501.906935	492484.687406	45.324417
3501.898545	492459.189927	45.329421
3501.729337	492439.473612	45.334426
3501.578624	492418.542565	45.339431
3502.028640	492391.509343	45.344436
3501.771190	492367.666240	45.349441
3501.982804	492346.274764	45.354445
3502.206026	492316.499577	45.359450
3501.973405	492297.095903	45.364455
3501.772241	492270.618235	45.369460
3501.679021	492253.364028	45.374465
3501.857543	492243.187098	45.379469
3501.609683	492208.890096	45.384474
3501.681874	492204.586942	45.389479
3501.926701	492180.463407	45.394484
3501.709931	492153.785988	45.399489
3501.627591	492133.096372	45.404493
3501.834736	492114.532918	45.409498
3501.790598	492098.583737	45.414503
3502.050333	492064.712358	45.419508
3501.789528	492051.069076	45.424513
3501.440926	492021.937725	45.429517
3501.912773	492006.211118	45.434522
3501.486293	491981.888763	45.439527
3501.404958	491967.914512	45.444532
3501.887243	491951.378313	45.449537
3501.484726	491932.354067	45.454541
3501.837182	491904.123285	45.459546
3501.603646	491879.568762	45.464551
3501.835494	491865.697165	45.469556
3501.687490	491840.220362	45.474561
3501.725065	491824.005701	45.479565
3501.939514	491797.815990	45.484570
3501.646292	491793.165622	45.489575
3502.113100	491763.957378	45.494580
3501.688951	491735.847130	45.499585
3501.578288	491713.343518	45.504589
3501.680827	491698.078022	45.509594
3501.404567	491674.337737	45.514599
3501.699647	491653.538235	45.519604
3501.566050	491638.511407	45.524609
3501.661750	491618.601306	45.529613
3501.932150	491605.278923	45.534618
3501.759484	491576.775774	45.539623
3501.848369	491558.280535	45.544628
3501.908804	491544.334326	45.549633
3501.757875	491522.089173	45.554637
3502.216495	491492.679695	45.559642
3501.638618	491471.005865	45.564647
3501.626203	491455.303547	45.569652
3501.984538	491433.635465	45.574657
3501.752413	491408.877970	45.579661
3502.279586	491376.730800	45.584666
3501.469476	491364.939748	45.589671
3501.788643	491333.481308	45.594676
3501.953449	491306.238043	45.599681
3501.627899	491302.551989	45.604685
3501.942750	491273.618927	45.609690
3501.995369	491251.745675	45.614695
3501.665987	491225.185127	45.619700
3501.960838	491210.949648	45.624705
3501.696467	491187.863207	45.629709
3501.663954	491168.729920	45.634714
3501.749386	491142.306665	45.639719
3501.819141	491119.319617	45.644724
3501.794129	491094.781863	45.649729
3501.487046	491080.336945	45.654733
3501.456130	491064.990581	45.659738
3501.585182	491049.922294	45.664743
3501.706290	491023.695270	45.669748
3501.727687	491003.189951	45.674753
3501.752197	490993.036145	45.679757
3501.734704	490952.590216	45.684762
3501.845294	490939.544604	45.689767
3501.803545	490914.453686	45.694772
3501.735231	490911.080991	45.699777
3501.695561	490876.597066	45.704781
3501.802196	490850.523488	45.709786
3501.633985	490833.178328	45.714791
3501.602600	490817.023815	45.719796
3501.530810	490799.663612	45.724801
3501.625074	490786.115425	45.729805
3501.738110	490770.796861	45.734810
3501.475525	490743.265601	45.739815
3501.759957	490722.819967	45.744820
3501.637150	490687.086083	45.749825
3501.590254	490622.555951	45.754829
3501.745513	490494.870051	45.759834
3501.188047	490335.529602	45.764839
3501.145763	490122.172790	45.769844
3500.929296	489880.256328	45.774849
3499.986929	489576.331155	45.779853
3500.173352	489224.902489	45.784858
3499.658787	488828.827543	45.789863
3498.951127	488390.549128	45.794868
3498.506512	487899.082932	45.799873
3497.538392	487378.841424	45.804877
3497.167713	486791.864643	45.809882
3496.171820	486174.503054	45.814887
3495.228609	485515.483577	45.819892
3494.094867	484820.496819	45.824897
3492.793815	484075.388678	45.829901
3491.887552	483273.597615	45.834906
3490.669529	482450.593020	45.839911
3489.436075	481576.463213	45.844916
3488.077887	480672.642177	45.849921
3486.785787	479728.280912	45.854925
3485.457547	478737.576442	45.859930
3483.845248	477713.042515	45.864935
3482.230418	476652.607291	45.869940
3480.849574	475562.191757	45.874945
3478.914627	474423.208831	45.879949
3477.221135	473253.269573	45.884954
3475.638209	472056.786674	45.889959
3474.002129	470808.751801	45.894964
3472.267710	469542.837935	45.899969
3470.083402	468238.969192	45.904973
3468.321108	466894.573907	45.909978
3466.124906	465530.007535	45.914983
3464.436092	464119.018602	45.919988
3462.160367	462681.596628	45.924993
3460.116791	461222.211996	45.929997
3457.925134	459725.841497	45.935002
3455.743422	458213.147250	45.940007
3453.341726	456663.363092	45.945012
3451.361500	455090.652078	45.950017
3448.642349	453495.594539	45.955021
3446.427524	451868.020116	45.960026
3443.711345	450216.632830	45.965031
3441.645756	448541.956764	45.970036
3438.714740	446855.564292	45.975041
3436.017499	445145.686355	45.980045
3433.866229	443403.659938	45.985050
3430.986747	441657.278170	45.990055
3428.348956	439866.324785	45.995060
3425.555749	438063.625109	46.000065
3422.881982	436254.149986	46.005069
3420.594103	434406.444555	46.010074
3417.470794	432556.159236	46.015079
3414.280644	430676.621155	46.020084
3411.550156	428774.380850	46.025089
3408.575471	426871.439255	46.030093
3405.755456	424950.551835	46.035098
3402.736445	423015.318983	46.040103
3399.992484	421050.708203	46.045108
3397.007384	419082.804933	46.050113
3393.846060	417091.671217	46.055117
3390.925656	415090.575427	46.060122
3387.478017	413077.709011	46.065127
3384.420917	411058.203172	46.070132
3381.669387	409017.106486	46.075137
3378.207609	406967.611617	46.080141
3375.273862	404902.371669	46.085146
3371.793086	402820.587746	46.090151
3368.442441	400725.450757	46.095156
3365.455619	398637.781957	46.100161
3361.823957	396525.258696	46.105165
3359.080282	394411.038807	46.110170
3355.255349	392291.369494	46.115175
3351.720499	390154.894375	46.120180
3348.608960	388006.236610	46.125185
3344.786878	385862.278044	46.130189
3341.962027	383710.670340	46.135194
3338.371166	381553.567601	46.140199
3334.929016	379385.140017	46.145204
3331.811406	377192.788200	46.150209
3328.225840	375015.188849	46.155213
3324.859474	372810.785716	46.160218
3320.977488	370619.776360	46.165223
3317.453954	368411.086499	46.170228
3314.112166	366199.046671	46.175233
3310.369350	363983.063447	46.180237
3306.935199	361763.511011	46.185242
3303.052320	359536.976716	46.190247
3299.580977	357315.501735	46.195252
3295.639365	355092.694982	46.200257
3291.869056	352866.501815	46.205261
3288.675757	350627.201360	46.210266
3284.718141	348410.898588	46.215271
3280.997381	346166.393892	46.220276
3277.345373	343930.984474	46.225281
3273.762156	341696.741606	46.230285
3270.162800	339454.018560	46.235290
3266.227256	337217.310782	46.240295
3262.568935	334976.175910	46.245300
3258.897116	332726.515529	46.250305
3254.811929	330490.038265	46.255309
3251.504847	328251.886994	46.260314
3247.531800	326006.768946	46.265319
3243.818792	323759.298761	46.270324
3240.308326	321526.863681	46.275329
3236.118510	319278.617946	46.280333
3232.676722	317036.424389	46.285338
3228.716900	314805.165515	46.290343
3224.557455	312559.604975	46.295348
3221.118508	310314.079534	46.300353
3216.931210	308085.488998	46.305357
3213.386618	305846.086007	46.310362
3209.555862	303626.098575	46.315367
3205.903418	301396.368833	46.320372
3202.161792	299168.393447	46.325377
3197.868001	296941.432892	46.330381
3194.160448	294716.305557	46.335386
3189.963348	292496.770964	46.340391
3186.420238	290280.236128	46.345396
3182.762232	288071.609619	46.350401
3178.373905	285870.328761	46.355405
3174.337156	283661.106101	46.360410
3170.733734	281460.657646	46.365415
3167.016659	279270.879612	46.370420
3163.414187	277068.061377	46.375425
3159.061811	274891.015106	46.380429
3155.479212	272703.734500	46.385434
3151.249708	270527.856050	46.390439
3147.149945	268340.905361	46.395444
3143.386847	266178.297898	46.400449
3138.885393	264025.512012	46.405453
3135.188911	261854.630115	46.410458
3131.410779	259710.559949	46.415463
3127.186165	257563.796245	46.420468
3123.923414	255416.719688	46.425473
3119.408130	253291.094792	46.430477
3115.533110	251147.538369	46.435482
3111.580266	249026.656981	46.440487
3107.386528	246917.706370	46.445492
3103.560958	244808.242508	46.450497
3099.812157	242715.198425	46.455501
3095.592449	240604.050511	46.460506
3091.798183	238511.845242	46.465511
3087.719531	236435.028226	46.470516
3084.185089	234358.038868	46.475521
3080.045153	232297.180107	46.480525
3076.008794	230231.331993	46.485530
3072.030269	228175.377685	46.490535
3067.833491	226129.693422	46.495540
3063.738891	224080.070655	46.500545
3059.417895	222055.291689	46.505549
3055.993827	220028.797796	46.510554
3051.837743	218019.283983	46.515559
3047.777302	216014.525602	46.520564
3043.686752	214013.652730	46.525569
3039.292870	212031.430564	46.530573
3035.499944	210058.831506	46.535578
3031.498898	208085.006381	46.540583
3027.207345	206141.626484	46.545588
3023.254043	204185.019854	46.550593
3018.894176	202252.588814	46.555597
3015.085990	200329.872755	46.560602
3010.884913	198409.227245	46.565607
3006.593206	196503.034512	46.570612
3002.661931	194609.646592	46.575617
2998.343401	192729.741205	46.580621
2994.678447	190845.280789	46.585626
2990.047771	188991.609752	46.590631
2985.858424	187138.537569	46.595636
2981.725664	185301.276699	46.600641
2977.096115	183490.506749	46.605645
2972.950469	181677.760232	46.610650
2968.646863	179896.723656	46.615655
2964.772495	178112.498606	46.620660
2960.584147	176352.789819	46.625665
2955.823649	174605.148691	46.630669
2951.611010	172876.250302	46.635674
2947.511639	171166.315065	46.640679
2942.989512	169461.958425	46.645684
2938.594876	167780.318326	46.650689
2934.126923	166121.196459	46.655693
2929.758687	164473.351435	46.660698
2925.267164	162847.090021	46.665703
2920.843279	161235.381538	46.670708
2916.202589	159654.905318	46.675713
2911.407426	158087.984631	46.680717
2906.985618	156546.806138	46.685722
2902.124198	155024.253737	46.690727
2896.951485	153537.652968	46.695732
2892.557197	152074.386153	46.700737
2887.104837	150640.770018	46.705741
2882.042083	149196.009095	46.710746
2876.675770	147790.069665	46.715751
2871.305358	146458.735561	46.720756
2866.010104	145165.202998	46.725761
2860.030376	143910.834810	46.730765
2854.531981	142702.610627	46.735770
2848.870912	141539.291755	46.740775
2843.341930	140405.968821	46.745780
2837.864340	139314.497631	46.750785
2832.207808	138269.186260	46.755789
2827.194890	137252.970480	46.760794
2821.948955	136274.559716	46.765799
2817.362204	135329.627466	46.770804
2812.623759	134418.883219	46.775809
2807.828841	133527.464530	46.780813
2803.288618	132679.657316	46.785818
2798.879793	131849.120906	46.790823
2794.473742	131047.144882	46.795828
2790.673230	130259.654344	46.800833
2786.247178	129489.384207	46.805837
2782.484816	128743.256149	46.810842
2778.386873	128014.962912	46.815847
2774.423842	127299.444432	46.820852
2770.918986	126587.975331	46.825857
2767.150005	125906.118590	46.830861
2763.195204	125209.383040	46.835866
2759.847714	124532.049803	46.840871
2756.160545	123859.066913	46.845876
2753.041464	123195.240319	46.850881
2749.039600	122544.585359	46.855885
2745.615374	121895.262909	46.860890
2741.679578	121246.590396	46.865895
2738.139904	120602.547008	46.870900
2734.697244	119959.224112	46.875905
2730.817970	119342.189400	46.880909
2727.248973	118711.166170	46.885914
2724.039494	118101.422972	46.890919
2720.540186	117472.889217	46.895924
2716.910767	116855.385599	46.900929
2713.154806	116253.081872	46.905933
2709.684040	115646.928837	46.910938
2706.181126	115046.131225	46.915943
2702.111511	114446.130963	46.920948
2698.425442	113860.995572	46.925953
2694.465916	113284.367502	46.930957
2690.669992	112691.664623	46.935962
2687.002611	112122.587568	46.940967
2683.397534	111550.649171	46.945972
2679.684252	110988.539288	46.950977
2675.527091	110439.704320	46.955981
2671.772344	109893.955532	46.960986
2667.891757	109346.429512	46.965991
2664.400756	108818.912889	46.970996
2660.728008	108284.173421	46.976001
2656.737103	107764.937805	46.981005
2652.991911	107241.641873	46.986010
2649.338746	106728.102758	46.991015
2645.384551	106228.843221	46.996020
2641.922395	105714.806586	47.001025
2638.333790	105219.331342	47.006029
2634.887458	104707.773667	47.011034
2631.650848	104216.288019	47.016039
2627.968344	103724.040037	47.021044
2624.773499	103236.096069	47.026049
2620.884129	102741.924605	47.031053
2617.584451	102239.864371	47.036058
2614.063946	101748.904340	47.041063
2610.377745	101262.998044	47.046068
2607.401037	100765.689230	47.051073
2603.778274	100282.533085	47.056077
2600.597109	99784.546656	47.061082
2597.369108	99295.255853	47.066087
2593.724871	98804.207124	47.071092
2590.547847	98300.015458	47.076097
2587.053133	97805.362116	47.081101
2583.684826	97296.767969	47.086106
2579.889128	96793.166737	47.091111
2576.429071	96309.460793	47.096116
2573.313867	95802.884719	47.101121
2569.638890	95303.927096	47.106125
2565.958945	94794.214752	47.111130
2563.065516	94291.491919	47.116135
2559.520278	93793.872697	47.121140
2555.812084	93288.103469	47.126145
2552.523826	92785.453972	47.131149
2549.417966	92275.744829	47.136154
2545.950978	91763.622652	47.141159
2542.186219	91248.264535	47.146164
2538.748201	90726.206378	47.151169
2535.597568	90226.652779	47.156173
2531.928241	89700.506344	47.161178
2528.793729	89195.847080	47.166183
2525.204943	88684.202973	47.171188
2521.669064	88144.989635	47.176193
2518.214684	87634.714918	47.181197
2515.182831	87112.657010	47.186202
2511.611945	86597.844826	47.191207
2507.717760	86071.518614	47.196212
2504.428651	85547.534211	47.201217
2500.905198	85022.007807	47.206221
2497.653095	84497.579354	47.211226
2494.051238	83970.750489	47.216231
2490.300820	83444.843646	47.221236
2487.342345	82911.011101	47.226241
2484.143518	82380.731867	47.231245
2480.466725	81834.659182	47.236250
2476.843257	81288.372842	47.241255
2473.314007	80759.864876	47.246260
2469.942491	80228.382900	47.251265
2466.299242	79698.642608	47.256269
2462.772786	79155.837621	47.261274
2459.235173	78620.297144	47.266279
2455.617509	78081.883813	47.271284
2452.288571	77546.573066	47.276289
2448.470938	77002.344542	47.281293
2444.870533	76461.496607	47.286298
2441.609864	75932.747289	47.291303
2437.860824	75396.210765	47.296308
2434.733188	74854.521312	47.301313
2431.257615	74323.055914	47.306317
2427.851430	73772.225078	47.311322
2424.636885	73245.515112	47.316327
2421.054062	72703.825793	47.321332
2417.902963	72148.481122	47.326337
2414.477569	71601.431456	47.331341
2410.808166	71051.142576	47.336346
2407.438794	70493.797170	47.341351
2403.847657	69947.283966	47.346356
2400.278373	69390.164677	47.351361
2396.714415	68843.346719	47.356365
2393.695843	68288.323783	47.361370
2390.222314	67720.491287	47.366375
2386.436046	67172.023189	47.371380
2383.377625	66609.444664	47.376385
2379.424914	66059.376044	47.381389
2376.431998	65492.641824	47.386394
2372.670826	64930.971542	47.391399
2368.959458	64366.538770	47.396404
2365.617082	63807.037148	47.401409
2361.915355	63250.491690	47.406413
2358.262502	62685.230950	47.411418
2354.749571	62125.133583	47.416423
2351.464164	61564.074239	47.421428
2348.254413	61001.835509	47.426433
2344.664196	60436.711643	47.431437
2341.423274	59859.882908	47.436442
2337.889817	59300.297297	47.441447
2334.281219	58742.861991	47.446452
2330.975487	58173.767702	47.451457
2327.331781	57604.016060	47.456461
2323.591683	57028.645818	47.461466
2320.389021	56449.309973	47.466471
2316.514653	55884.831511	47.471476
2313.274689	55317.495108	47.476481
2309.778194	54750.960821	47.481485
2306.324754	54182.542797	47.486490
2303.324770	53610.692822	47.491495
2299.626598	53033.071860	47.496500
2296.142989	52455.158962	47.501505
2292.555025	51877.168763	47.506509
2289.127909	51307.902885	47.511514
2286.043671	50718.324293	47.516519
2281.671145	50138.704351	47.521524
2278.296923	49552.042426	47.526529
2274.904362	48987.014809	47.531533
2271.423306	48403.208798	47.536538
2268.115741	47825.333687	47.541543
2264.811368	47244.663093	47.546548
2261.449708	46655.175245	47.551553
2258.055616	46067.838759	47.556557
2253.975372	45480.047270	47.561562
2250.376278	44899.977592	47.566567
2247.173991	44327.686686	47.571572
2243.648032	43735.517175	47.576577
2240.132769	43154.592083	47.581581
2236.450574	42567.075469	47.586586
2233.000587	41986.304081	47.591591
2229.701999	41414.845321	47.596596
2226.404864	40814.171283	47.601601
2222.559966	40233.717010	47.606605
2219.186483	39646.915350	47.611610
2216.055257	39054.062469	47.616615
2212.455593	38468.836819	47.621620
2208.650024	37880.933019	47.626625
2205.129211	37296.868080	47.631629
2201.837401	36708.973465	47.636634
2198.554527	36116.757636	47.641639
2194.555948	35526.850266	47.646644
2191.341944	34937.090733	47.651649
2187.198783	34348.576140	47.656653
2183.775134	33770.722359	47.661658
2180.209612	33184.337160	47.666663
2176.548496	32593.045844	47.671668
2173.249613	32010.378830	47.676673
2169.698298	31425.885074	47.681677
2166.117033	30849.448470	47.686682
2162.571331	30263.104337	47.691687
2158.888616	29684.535921	47.696692
2155.668484	29101.811704	47.701697
2151.995940	28520.074269	47.706701
2148.562828	27944.291601	47.711706
2144.742612	27365.398162	47.716711
2141.180377	26791.733861	47.721716
2137.607786	26213.366968	47.726721
2133.802032	25643.688823	47.731725
2129.963106	25072.948518	47.736730
2126.405183	24521.554983	47.741735
2122.246370	23972.044054	47.746740
2118.766830	23409.258833	47.751745
2114.612620	22874.703283	47.756749
2110.612328	22338.225010	47.761754
2105.864595	21825.784943	47.766759
2101.218410	21330.027686	47.771764
2097.287086	20836.319020	47.776769
2092.912720	20361.118129	47.781773
2088.312952	19902.191886	47.786778
2084.399258	19444.772133	47.791783
2079.740336	19022.733272	47.796788
2075.805890	18595.048806	47.801793
2071.578805	18182.163860	47.806797
2067.421968	17785.262393	47.811802
2063.534132	17397.345850	47.816807
2059.530756	17032.859419	47.821812
2055.165626	16664.300674	47.826817
2051.204953	16329.044951	47.831821
2046.513520	16011.726326	47.836826
2042.449846	15686.288479	47.841831
2038.100393	15409.215685	47.846836
2033.905250	15105.085970	47.851841
2029.982936	14830.760422	47.856845
2025.943401	14570.708110	47.861850
2022.547541	14321.599554	47.866855
2019.113054	14068.919399	47.871860
2015.574639	13816.021326	47.876865
2012.192903	13579.277487	47.881869
2008.520141	13350.775489	47.886874
2005.003143	13102.600938	47.891879
2001.130000	12876.510324	47.896884
1997.935790	12641.316173	47.901889
1994.721303	12416.917279	47.906893
1991.358863	12200.290796	47.911898
1988.339547	11971.805111	47.916903
1984.912466	11746.193663	47.921908
1981.532257	11519.567777	47.926913
1978.045942	11298.842918	47.931917
1974.634370	11076.323625	47.936922
1971.789859	10841.046936	47.941927
1967.737214	10616.090939	47.946932
1964.616205	10376.219299	47.951937
1961.468775	10159.431015	47.956941
1957.939804	9923.041061	47.961946
1954.587826	9690.643426	47.966951
1950.820185	9470.145421	47.971956
1947.622341	9237.368619	47.976961
1943.988577	9007.264426	47.981965
1940.510771	8777.341393	47.986970
1937.105513	8556.478174	47.991975
1933.415138	8330.088147	47.996980
1930.052683	8099.145916	48.001985
1926.710386	7878.622838	48.006989
1922.809620	7661.528423	48.011994
1919.640533	7439.208067	48.016999
1916.128203	7214.301083	48.022004
1913.140679	6985.118498	48.027009
1909.299129	6766.069533	48.032013
1905.417006	6545.254027	48.037018
1902.362298	6321.853361	48.042023
1898.386075	6100.469218	48.047028
1895.249290	5883.549126	48.052033
1891.147224	5671.895977	48.057037
1887.475524	5453.133797	48.062042
1884.023042	5227.333679	48.067047
1880.400985	5017.255869	48.072052
1877.385919	4802.725286	48.077057
1873.529827	4600.742465	48.082061
1869.865468	4409.045053	48.087066
1866.691300	4178.702128	48.092071
1862.946061	3972.984524	48.097076
1859.720770	3768.124988	48.102081
1856.139595	3560.215801	48.107085
1852.298102	3359.272978	48.112090
1848.787618	3152.537767	48.117095
1844.896278	2950.373207	48.122100
1841.632526	2760.320645	48.127105
1837.881852	2562.096947	48.132109
1834.365020	2359.921876	48.137114
1830.759574	2164.284031	48.142119
1827.162264	1979.749677	48.147124
1823.795025	1786.230436	48.152129
1820.127262	1595.398815	48.157133
1816.464838	1413.050929	48.162138
1812.590306	1236.050123	48.167143
1808.952415	1062.424908	48.172148
1805.011808	887.715840	48.177153
1801.218536	725.919252	48.182157
1797.059797	570.540241	48.187162
1793.454573	409.106417	48.192167
1789.169432	270.786585	48.197172
1784.128646	160.982974	48.202177
1778.246071	108.124894	48.207181
1770.035598	112.373528	48.212186
1764.590756	109.123991	48.217191
1760.415572	107.451688	48.222196
1757.249044	104.837799	48.227201
1754.593821	106.820295	48.232205
1751.876666	104.348434	48.237210
1749.349861	108.133240	48.242215
1746.177415	109.911502	48.247220
1743.409937	104.562172	48.252225
1740.032480	108.061763	48.257229
1736.070191	109.077119	48.262234
1732.902264	106.545706	48.267239
1729.052672	101.583095	48.272244
1725.913477	110.525148	48.277249
1722.475927	105.545861	48.282253
1718.776893	112.774899	48.287258
1715.816235	112.878236	48.292263
1712.159009	111.928905	48.297268
1709.519409	108.885001	48.302273
1706.294645	107.605775	48.307277
1702.370121	106.552517	48.312282
1699.076337	100.054425	48.317287
1695.274338	106.609799	48.322292
1691.976558	107.031359	48.327297
1688.676503	109.516011	48.332301
1685.192407	112.003999	48.337306
1682.051931	111.436145	48.342311
1677.925103	110.575726	48.347316
1674.681785	107.632117	48.352321
1671.142366	100.675557	48.357325
1667.872666	111.387453	48.362330
1664.859018	99.233348	48.367335
1661.187006	103.297636	48.372340
1657.604137	102.903042	48.377345
1654.021922	104.349624	48.382349
1650.585184	93.650244	48.387354
1647.096430	101.118630	48.392359
1643.461211	101.355435	48.397364
1640.563448	102.682834	48.402369
1637.150341	97.880088	48.407373
1633.484941	103.094937	48.412378
1629.690368	101.091333	48.417383
1626.349202	106.996026	48.422388
1622.879379	102.474187	48.427393
1619.046949	97.084985	48.432397
1615.811263	98.003079	48.437402
1612.646777	94.860551	48.442407
1609.001925	98.727628	48.447412
1606.104804	97.577748	48.452417
1602.195034	102.349751	48.457421
1598.088733	106.383563	48.462426
1595.115677	102.771485	48.467431
1591.423287	109.031397	48.472436
1588.045224	102.283851	48.477441
1584.883942	100.061463	48.482445
1581.230731	97.007660	48.487450
1577.928428	89.811737	48.492455
1574.115812	96.134651	48.497460
1570.627580	104.273664	48.502465
1567.163656	99.330142	48.507469
1563.703794	98.473494	48.512474
1560.245343	97.069306	48.517479
1556.916793	101.580008	48.522484
1553.581248	99.460676	48.527489
1550.305645	96.756221	48.532493
1546.375270	97.782446	48.537498
1543.152298	90.665928	48.542503
1539.578138	98.973335	48.547508
1535.613295	100.681958	48.552513
1532.049832	94.766860	48.557517
1528.928864	95.249498	48.562522
1525.699690	89.424738	48.567527
1521.598453	100.196450	48.572532
1518.149623	95.212623	48.577537
1514.921646	93.810532	48.582541
1511.570093	96.138698	48.587546
1508.554238	95.130692	48.592551
1504.739048	105.282091	48.597556
1501.028948	97.092972	48.602561
1497.426063	90.915102	48.607565
1493.910269	98.058675	48.612570
1490.487623	82.652715	48.617575
1486.852949	101.998200	48.622580
1483.672526	99.291592	48.627585
1480.189527	84.053212	48.632589
1476.324377	104.086293	48.637594
1473.657976	89.448460	48.642599
1469.624004	98.564579	48.647604
1465.915927	89.327970	48.652609
1462.510910	97.011113	48.657613
1458.943222	97.765763	48.662618
1455.459884	104.334822	48.667623
1451.671611	98.018136	48.672628
1448.777690	94.896787	48.677633
1445.210669	109.470380	48.682637
1441.620313	103.072268	48.687642
1438.355256	98.385708	48.692647
1434.815641	103.397496	48.697652
1430.794255	91.026976	48.702657
1427.439680	97.829088	48.707661
1424.097476	94.673115	48.712666
1420.698420	87.938358	48.717671
1417.123425	97.425957	48.722676
1413.715048	99.206163	48.727681
1410.091087	104.588579	48.732685
1406.557992	92.357194	48.737690
1403.405234	88.599108	48.742695
1399.456075	100.448118	48.747700
1395.913087	104.055751	48.752705
1392.334738	93.928944	48.757709
1389.224733	91.407538	48.762714
1385.608762	91.600245	48.767719
1382.429725	103.936819	48.772724
1378.592531	89.427456	48.777729
1375.800252	96.951955	48.782733
1372.272840	100.430616	48.787738
1367.949768	92.416024	48.792743
1364.274215	106.816684	48.797748
1361.132496	103.857298	48.802753
1358.285302	92.683403	48.807757
1354.082006	97.675112	48.812762
1350.507055	86.965668	48.817767
1347.226386	94.411163	48.822772
1343.770844	94.487157	48.827777
1340.245242	87.256427	48.832781
1336.485807	90.087846	48.837786
1333.398292	94.760354	48.842791
1329.684911	95.464929	48.847796
1326.366830	91.694620	48.852801
1322.574779	90.816939	48.857805
1319.166169	88.022486	48.862810
1315.842253	85.910864	48.867815
1312.156851	86.943274	48.872820
1308.847147	94.595767	48.877825
1305.267902	93.631181	48.882829
1301.433249	89.887498	48.887834
1297.964493	89.478344	48.892839
1294.805475	84.772139	48.897844
1291.786139	86.763878	48.902849
1288.385728	88.871878	48.907853
1284.205698	91.616911	48.912858
1280.420875	95.967697	48.917863
1277.312195	85.150892	48.922868
1273.836568	83.777884	48.927873
1270.507246	87.491468	48.932877
1266.605167	92.255967	48.937882
1263.238649	89.521407	48.942887
1259.497998	91.264762	48.947892
1255.889535	86.217238	48.952897
1252.675914	89.824231	48.957901
1249.037844	93.348598	48.962906
1245.950577	84.221043	48.967911
1242.434380	85.287233	48.972916
1238.689774	91.824200	48.977921
1235.134694	84.237417	48.982925
1231.478390	86.053065	48.987930
1228.174765	83.738983	48.992935
1224.719415	91.784300	48.997940
1221.584073	86.846632	49.002945
1218.065650	88.466817	49.007949
1214.443082	85.509533	49.012954
1210.646500	84.502860	49.017959
1207.049880	93.291488	49.022964
1203.607860	90.916694	49.027969
1200.166964	85.979135	49.032973
1196.892579	91.303984	49.037978
1193.554259	75.008631	49.042983
1189.804175	82.666397	49.047988
1186.181306	85.631592	49.052993
1182.822849	86.255627	49.057997
1178.868899	91.227520	49.063002
1175.762645	82.985602	49.068007
1172.193948	86.306191	49.073012
1168.669550	85.209701	49.078017
1165.070406	76.395953	49.083021
1161.874291	84.505319	49.088026
1158.031634	80.636359	49.093031
1154.293696	82.986730	49.098036
1150.924242	88.130229	49.103041
1147.843294	84.009829	49.108045
1144.401643	92.824957	49.113050
1141.158896	90.979126	49.118055
1137.577279	87.743400	49.123060
1133.585376	86.776630	49.128065
1130.611624	78.678610	49.133069
1126.557803	85.032763	49.138074
1123.317654	78.134121	49.143079
1119.618465	82.272275	49.148084
1116.033265	89.119786	49.153089
1112.573771	80.834791	49.158093
1109.014509	86.045802	49.163098
1105.612342	84.867019	49.168103
1102.192681	73.545016	49.173108
1098.860807	81.102887	49.178113
1095.191238	83.774809	49.183117
1091.528026	79.036386	49.188122
1087.997361	75.621900	49.193127
1084.394883	87.986408	49.198132
1081.158153	84.222453	49.203137
1077.794708	86.248789	49.208141
1074.066793	79.277386	49.213146
1070.701096	83.028282	49.218151
1067.131852	82.966983	49.223156
1063.339211	79.178836	49.228161
1060.284560	78.993145	49.233165
1056.378734	92.028121	49.238170
1053.058187	76.290009	49.243175
1049.771653	85.258157	49.248180
1046.179612	72.514030	49.253185
1042.696645	80.835725	49.258189
1039.135981	86.575294	49.263194
1035.945693	77.536580	49.268199
1032.354340	81.142275	49.273204
1028.883111	85.849216	49.278209
1025.656386	81.520576	49.283213
1021.643995	85.473379	49.288218
1018.435296	82.799705	49.293223
1014.836104	83.325192	49.298228
1011.204669	79.980185	49.303233
1007.208432	75.027865	49.308237
1003.879546	86.210860	49.313242
1000.792363	81.398604	49.318247
997.268350	84.661633	49.323252
993.427490	83.475223	49.328257
990.218848	82.449824	49.333261
986.352197	88.325610	49.338266
982.988031	91.086043	49.343271
979.258721	82.669068	49.348276
976.150355	75.765756	49.353281
972.645328	84.122526	49.358285
968.862075	88.808442	49.363290
965.592232	80.493952	49.368295
962.097700	83.299988	49.373300
958.165040	80.609305	49.378305
955.156297	73.187464	49.383309
951.957470	83.037284	49.388314
948.595460	80.915819	49.393319
944.958938	85.408057	49.398324
941.452541	85.969727	49.403329
937.475572	87.025417	49.408333
933.551042	82.818067	49.413338
930.442359	77.104356	49.418343
926.799735	86.710056	49.423348
923.465109	86.634399	49.428353
920.164056	81.950357	49.433357
916.618343	87.532587	49.438362
913.524845	84.695464	49.443367
909.766511	91.712305	49.448372
905.952500	84.089959	49.453377
902.789521	87.094321	49.458381
898.924295	91.770858	49.463386
895.297623	89.127462	49.468391
892.010573	82.764492	49.473396
888.591810	85.106334	49.478401
884.918843	82.881426	49.483405
881.670902	87.313181	49.488410
878.339414	90.644326	49.493415
874.454885	89.246436	49.498420
870.917341	80.970471	49.503425
867.437139	81.664110	49.508429
863.886403	87.971609	49.513434
860.797128	75.307444	49.518439
857.029199	84.559337	49.523444
853.811145	84.351649	49.528449
850.054235	89.903487	49.533453
846.490409	89.009322	49.538458
842.904770	75.062045	49.543463
839.261503	83.544741	49.548468
835.557889	82.033276	49.553473
832.493617	77.476901	49.558477
828.748589	88.038159	49.563482
825.531758	78.551210	49.568487
822.423304	83.489589	49.573492
818.842575	82.534787	49.578497
815.188495	77.807642	49.583501
811.442277	81.934161	49.588506
807.990499	81.209218	49.593511
804.314415	79.152482	49.598516
800.814255	88.957469	49.603521
797.724485	71.927519	49.608525
793.969009	75.005138	49.613530
790.519607	67.984110	49.618535
786.684629	71.580294	49.623540
783.399563	79.890175	49.628545
780.415114	76.045865	49.633549
776.488876	77.131643	49.638554
772.972142	79.330562	49.643559
769.352459	75.034660	49.648564
765.787094	82.258743	49.653569
762.530981	74.650821	49.658573
759.047869	82.798549	49.663578
755.873998	80.413711	49.668583
752.450144	73.518421	49.673588
748.457325	74.446892	49.678593
744.855886	73.916093	49.683597
741.164994	76.711589	49.688602
737.615539	68.826643	49.693607
734.026182	68.180072	49.698612
730.614812	72.555021	49.703617
727.228007	63.401435	49.708621
723.919125	76.147332	49.713626
720.747925	79.434555	49.718631
717.007171	75.331511	49.723636
713.598331	83.401243	49.728641
709.513129	83.796784	49.733645
706.236979	81.984681	49.738650
703.052484	72.647746	49.743655
699.518313	74.264107	49.748660
695.578045	81.236516	49.753665
692.322001	77.086493	49.758669
688.694833	80.814850	49.763674
685.537235	72.644291	49.768679
682.500095	78.011328	49.773684
678.287087	77.300501	49.778689
675.004429	71.477878	49.783693
671.305406	71.421012	49.788698
668.042759	71.172832	49.793703
664.309939	65.875859	49.798708
660.690039	77.161102	49.803713
657.354179	75.570269	49.808717
653.558485	83.133928	49.813722
650.183209	78.926544	49.818727
647.364486	72.237621	49.823732
643.531449	73.830913	49.828737
639.651644	72.378542	49.833741
635.984849	80.766836	49.838746
632.663819	71.198076	49.843751
629.069512	74.370843	49.848756
625.815449	65.225086	49.853761
622.450767	65.926079	49.858765
618.669201	76.663866	49.863770
615.539965	74.620104	49.868775
611.907216	68.469187	49.873780
608.288170	69.004141	49.878785
604.934425	64.761780	49.883789
601.618234	79.444985	49.888794
597.993619	70.217714	49.893799
594.050285	81.562803	49.898804
590.657189	80.215000	49.903809
587.555891	78.628788	49.908813
584.013887	80.913917	49.913818
580.378673	72.472890	49.918823
576.755799	73.438703	49.923828
573.155212	75.520988	49.928833
569.886979	78.728419	49.933837
566.315686	71.463822	49.938842
562.924053	74.592390	49.943847
559.109033	84.256580	49.948852
555.792297	69.337398	49.953857
552.038871	77.270959	49.958861
548.525366	84.853971	49.963866
545.186226	83.086496	49.968871
542.001106	72.034980	49.973876
538.412356	75.776352	49.978881
534.970889	77.697832	49.983885
531.137965	83.647497	49.988890
527.807714	78.227765	49.993895
524.542682	77.612988	49.998900
520.446834	83.059434	50.003905
517.346805	75.348166	50.008909
513.774008	78.587198	50.013914
510.213756	72.975492	50.018919
506.737704	73.522999	50.023924
502.486577	79.657990	50.028929
499.971615	71.776553	50.033933
496.197538	75.024776	50.038938
492.920349	74.212585	50.043943
489.478887	77.719067	50.048948
485.744058	78.695994	50.053953
482.089616	81.419407	50.058957
478.308149	81.663297	50.063962
475.071147	77.750782	50.068967
471.545505	77.992810	50.073972
468.198498	76.536612	50.078977
464.841704	75.439432	50.083981
461.274199	78.595391	50.088986
457.770106	75.967782	50.093991
454.205657	75.630575	50.098996
450.610668	74.225640	50.104001
446.914737	69.539878	50.109005
443.553305	70.072712	50.114010
440.315709	76.442218	50.119015
436.607153	71.410419	50.124020
433.066830	77.918800	50.129025
429.622765	75.202759	50.134029
426.455974	69.042611	50.139034
423.279615	74.175081	50.144039
419.151201	75.118380	50.149044
415.252868	68.255895	50.154049
412.202271	62.058680	50.159053
408.798758	73.227988	50.164058
405.177200	67.372754	50.169063
401.490091	80.895693	50.174068
397.649977	78.098949	50.179073
394.601380	64.802157	50.184077
390.713787	81.665503	50.189082
387.511699	78.231608	50.194087
384.077637	69.566324	50.199092
380.620429	80.478248	50.204097
377.524329	82.646527	50.209101
373.760588	82.606106	50.214106
370.110649	88.445045	50.219111
366.545761	87.029108	50.224116
362.901741	73.141661	50.229121
359.407792	71.138896	50.234125
356.181030	84.166239	50.239130
352.631785	73.222070	50.244135
348.895266	72.285261	50.249140
345.312821	76.924153	50.254145
342.334565	73.752804	50.259149
338.619400	78.791999	50.264154
335.149384	82.160579	50.269159
331.502185	75.806325	50.274164
327.802632	76.432942	50.279169
324.617953	79.092730	50.284173
320.990621	86.839008	50.289178
317.683857	81.086634	50.294183
314.139477	79.199289	50.299188
310.392684	73.246513	50.304193
307.161180	74.202050	50.309197
303.493418	76.978177	50.314202
299.851488	79.943266	50.319207
296.302535	77.765580	50.324212
292.438180	78.886081	50.329217
289.597957	76.348128	50.334221
285.883949	75.078803	50.339226
282.637833	80.323383	50.344231
279.211090	71.233050	50.349236
275.672429	72.397757	50.354241
272.222715	73.665673	50.359245
268.290293	81.642944	50.364250
264.807946	77.423821	50.369255
261.613200	74.602554	50.374260
258.337411	78.431271	50.379265
254.690853	68.742434	50.384269
250.967225	73.245133	50.389274
247.472067	71.239409	50.394279
243.728742	75.080806	50.399284
240.252790	78.045371	50.404289
237.109880	65.674434	50.409293
233.459415	74.895417	50.414298
229.970405	64.444928	50.419303
226.531878	70.057977	50.424308
223.107015	61.334354	50.429313
219.317927	55.112950	50.434317
215.878816	69.992449	50.439322
212.343780	61.713075	50.444327
208.855542	69.567409	50.449332
205.434268	74.023040	50.454337
202.323351	63.355509	50.459341
198.221956	65.737265	50.464346
194.677745	66.371352	50.469351
191.440111	76.144980	50.474356
188.049983	72.541083	50.479361
184.453814	63.372752	50.484365
180.761960	69.642160	50.489370
176.937173	61.417396	50.494375
174.039854	64.943592	50.499380
170.604495	67.275439	50.504385
167.146798	64.014252	50.509389
163.309485	68.300548	50.514394
159.486333	63.286647	50.519399
156.424245	66.870135	50.524404
152.896676	65.128894	50.529409
149.866011	58.178837	50.534413
146.107137	58.292712	50.539418
142.171797	54.492146	50.544423
138.842657	62.498878	50.549428
135.418728	71.738379	50.554433
131.811268	65.026817	50.559437
128.214189	71.135946	50.564442
124.638860	65.824047	50.569447
121.485822	58.390027	50.574452
117.569698	71.186182	50.579457
114.333477	64.204860	50.584461
111.050722	72.795979	50.589466
107.245649	64.349868	50.594471
103.667006	64.084523	50.599476
100.211188	64.606789	50.604481
97.091839	66.693297	50.609485
93.385522	73.926719	50.614490
90.014217	71.057040	50.619495
86.342251	65.377392	50.624500
82.726726	67.417771	50.629505
79.422155	60.057970	50.634509
75.556662	79.179889	50.639514
71.914653	75.865157	50.644519
68.809640	72.270672	50.649524
65.484879	71.690566	50.654529
61.990651	68.745122	50.659533
58.295578	78.415977	50.664538
54.685299	69.730745	50.669543
51.266660	64.087591	50.674548
47.672946	78.469167	50.679553
44.219938	76.880843	50.684557
40.844499	70.285029	50.689562
37.136793	65.316451	50.694567
33.800890	61.757923	50.699572
30.359529	74.230237	50.704577
26.804145	73.803100	50.709581
23.373989	74.830729	50.714586
19.667090	68.065071	50.719591
16.356590	66.802567	50.724596
12.642429	73.761979	50.729601
9.144078	61.484405	50.734605
5.821473	72.153929	50.739610
2.593845	71.245507	50.744615