Fri Aug 26 13:51:46 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.566879	95.953385	0.000000
0.437045	100.776045	0.005005
0.781848	94.021743	0.010010
0.241232	85.352087	0.015014
0.384041	76.091990	0.020019
-0.241606	74.417766	0.025024
-0.560770	64.910072	0.030029
-0.743933	66.893739	0.035034
-0.945680	69.617431	0.040038
-0.909588	52.654648	0.045043
-1.032068	53.483624	0.050048
-1.463871	39.548553	0.055053
-1.658748	32.606226	0.060058
-2.030540	19.076266	0.065062
-2.150705	20.205426	0.070067
-2.461164	17.507731	0.075072
-2.878270	17.683412	0.080077
-3.512947	9.449204	0.085082
-3.786076	11.807527	0.090086
-3.891040	9.536568	0.095091
-3.817118	2.406875	0.100096
-4.471417	0.208791	0.105101
-4.877761	0.297378	0.110106
-4.911312	3.694037	0.115110
-5.132528	6.582097	0.120115
-5.329439	6.929131	0.125120
-5.879432	5.692372	0.130125
-6.342725	-0.951894	0.135130
-6.756391	2.858275	0.140134
-6.906074	0.249443	0.145139
-6.803147	5.175037	0.150144
-6.800871	9.344375	0.155149
-6.589122	4.043954	0.160154
-7.449617	8.208422	0.165158
-7.970805	10.440858	0.170163
-7.708006	2.032119	0.175168
-8.259054	4.844986	0.180173
-8.141922	-7.925876	0.185178
-8.906007	3.348098	0.190182
-9.492978	-0.407488	0.195187
-10.026454	-5.300823	0.200192
-10.283079	3.492939	0.205197
-9.882976	-0.979460	0.210202
-9.999628	2.990102	0.215206
-10.099073	1.044139	0.220211
-9.836941	0.819846	0.225216
-10.346293	-0.894622	0.230221
-11.088992	-2.803705	0.235226
-11.501675	-0.724200	0.240230
-11.092044	1.027963	0.245235
-11.592964	5.595174	0.250240
-12.332782	5.647100	0.255245
-12.408053	-3.291110	0.260250
-12.537410	0.379884	0.265254
-12.608195	-3.816726	0.270259
-12.655662	-10.725040	0.275264
-13.467372	-0.797691	0.280269
-13.817267	5.561935	0.285274
-13.862652	4.132720	0.290278
-14.214016	7.218207	0.295283
-13.996512	8.389701	0.300288
-14.683775	14.767058	0.305293
-15.298101	5.333827	0.310298
-15.534769	10.223714	0.315302
-15.219783	6.267585	0.320307
-15.344701	11.991094	0.325312
-15.455566	18.750091	0.330317
-15.413760	0.422939	0.335322
-16.151428	8.845527	0.340326
-16.699512	14.992414	0.345331
-16.513797	4.744944	0.350336
-16.820300	15.821136	0.355341
-17.565382	1.586873	0.360346
-17.851706	10.875626	0.365350
-18.363693	6.760363	0.370355
-18.292256	9.947694	0.375360
-18.955404	13.977037	0.380365
-18.392004	8.764228	0.385370
-18.587277	3.720161	0.390374
-18.356864	14.203409	0.395379
-19.021781	13.629927	0.400384
-19.574120	12.662443	0.405389
-20.045966	-1.234723	0.410394
-20.141926	1.643325	0.415398
-19.978175	7.464250	0.420403
-20.550332	5.000286	0.425408
-21.042801	12.856371	0.430413
-21.275394	13.680343	0.435418
-21.426134	5.709300	0.440422
-21.567078	5.569911	0.445427
-21.469725	4.700582	0.450432
-21.910239	13.851997	0.455437
-22.375740	13.630268	0.460442
-22.991818	1.321560	0.465446
-22.907694	9.556088	0.470451
-22.913233	3.213860	0.475456
-23.130388	5.092085	0.480461
-23.401639	3.106436	0.485466
-23.675605	2.266447	0.490470
-24.501805	14.268245	0.495475
-24.219722	5.385120	0.500480
-24.208284	-4.487208	0.505485
-24.688030	-2.988863	0.510490
-25.126452	1.350324	0.515494
-25.664615	5.489915	0.520499
-25.914306	8.597535	0.525504
-26.148038	6.783208	0.530509
-25.957331	0.676172	0.535514
-26.024228	14.423132	0.540518
-26.421481	3.918430	0.545523
-26.715674	-3.378563	0.550528
-26.960090	10.392870	0.555533
-26.907694	-4.693190	0.560538
-27.129686	5.582091	0.565542
-27.992686	4.229558	0.570547
-28.028301	-2.592022	0.575552
-28.493977	6.348180	0.580557
-28.363815	-1.438813	0.585562
-28.759994	7.772133	0.590566
-29.592364	5.592284	0.595571
-29.762825	-4.061905	0.600576
-29.868574	1.693415	0.605581
-29.967007	-2.040161	0.610586
-30.116602	3.136713	0.615590
-30.328510	7.390015	0.620595
-30.006324	-2.445278	0.625600
-30.617639	9.836260	0.630605
-31.079083	1.970541	0.635610
-31.413899	4.161304	0.640614
-31.589486	4.334181	0.645619
-31.467346	7.228890	0.650624
-32.210545	3.912065	0.655629
-32.817594	8.103508	0.660634
-32.817969	0.004657	0.665638
-33.110034	10.537614	0.670643
-32.597566	-2.158766	0.675648
-32.928942	4.511177	0.680653
-33.417071	7.178211	0.685658
-33.874415	0.124911	0.690662
-34.708765	0.235847	0.695667
-34.350552	10.028501	0.700672
-34.675127	8.029008	0.705677
-34.557975	1.829024	0.710682
-34.921345	6.507692	0.715686
-35.834365	4.571346	0.720691
-36.104493	3.588397	0.725696
-36.279786	6.396542	0.730701
-35.974179	-0.936894	0.735706
-36.075804	4.504584	0.740710
-36.182120	3.258856	0.745715
-36.810269	7.469403	0.750720
-36.955912	10.538678	0.755725
-37.310316	8.217975	0.760730
-37.884097	6.535683	0.765734
-37.669290	9.191346	0.770739
-37.761984	1.056250	0.775744
-38.563959	4.794005	0.780749
-38.736076	3.397177	0.785754
-38.941038	10.487184	0.790758
-39.245079	4.713434	0.795763
-38.897275	6.171514	0.800768
-39.508865	9.417736	0.805773
-40.124538	2.623196	0.810778
-40.417699	6.158348	0.815782
-40.612106	10.567109	0.820787
-40.869707	7.468896	0.825792
-40.646984	16.779629	0.830797
-40.615483	14.984114	0.835802
-41.383911	7.137718	0.840806
-42.003893	11.116048	0.845811
-41.881214	2.637382	0.850816
-41.983182	9.198843	0.855821
-42.205071	3.447103	0.860826
-42.300578	6.084643	0.865830
-42.952288	3.898812	0.870835
-43.380274	6.730483	0.875840
-43.753402	9.961722	0.880845
-43.514085	10.288292	0.885850
-43.184042	3.976070	0.890854
-44.148276	5.356867	0.895859
-44.584259	1.264573	0.900864
-44.744755	10.271151	0.905869
-44.603572	5.911828	0.910874
-44.794716	11.731065	0.915878
-45.450064	7.840597	0.920883
-45.778510	8.695312	0.925888
-46.580634	8.725304	0.930893
-46.340319	11.759795	0.935898
-46.401237	9.706597	0.940902
-46.680580	10.689703	0.945907
-46.540343	12.933048	0.950912
-46.966152	20.851520	0.955917
-47.478079	10.772780	0.960922
-47.643397	7.577945	0.965926
-48.199353	13.580528	0.970931
-48.002299	1.161039	0.975936
-48.306705	10.284932	0.980941
-48.388412	9.965483	0.985946
-48.983334	9.928414	0.990950
-49.508728	1.515853	0.995955
-49.441801	9.199419	1.000960
-49.792933	7.881081	1.005965
-49.694203	9.586741	1.010970
-49.844780	11.831074	1.015974
-50.431250	6.038025	1.020979
-50.877741	6.281555	1.025984
-50.989157	4.539929	1.030989
-51.082527	6.553899	1.035994
-51.161613	7.420408	1.040998
-51.500034	9.178314	1.046003
-51.931775	8.631800	1.051008
-52.581616	8.986083	1.056013
-52.370061	16.827461	1.061018
-52.188031	4.884856	1.066022
-52.509662	5.842910	1.071027
-53.175576	0.859469	1.076032
-53.654433	5.435899	1.081037
-54.113995	9.984016	1.086042
-53.819879	2.013314	1.091046
-53.988522	20.686088	1.096051
-54.011820	6.807665	1.101056
-54.743974	10.281459	1.106061
-55.544083	8.713498	1.111066
-55.436915	10.674100	1.116070
-55.504485	10.577068	1.121075
-55.414615	14.571422	1.126080
-55.539402	15.157154	1.131085
-56.313375	7.596350	1.136090
-56.667522	15.975044	1.141094
-56.857097	15.036498	1.146099
-56.682982	10.776447	1.151104
-57.073705	14.760210	1.156109
-57.280024	11.536957	1.161114
-57.081679	5.729278	1.166118
-57.929646	7.784811	1.171123
-58.047515	10.602997	1.176128
-58.651985	15.369823	1.181133
-58.626674	15.881567	1.186138
-58.485476	5.688487	1.191142
-59.351576	17.886315	1.196147
-59.600090	12.730320	1.201152
-59.692250	17.259198	1.206157
-59.867325	12.819406	1.211162
-60.200377	13.937421	1.216166
-60.447457	10.628769	1.221171
-60.826234	9.586809	1.226176
-61.344079	11.847197	1.231181
-61.536518	10.649679	1.236186
-61.319300	13.785839	1.241190
-61.416124	12.007141	1.246195
-61.589785	12.666920	1.251200
-61.790647	10.964530	1.256205
-62.287749	17.587515	1.261210
-62.630451	2.025151	1.266214
-62.722206	14.529504	1.271219
-63.445392	12.772403	1.276224
-64.200940	11.051977	1.281229
-63.416945	1.802818	1.286234
-63.766328	4.963923	1.291238
-64.126728	21.591204	1.296243
-64.004665	11.530810	1.301248
-64.692998	6.696387	1.306253
-65.631661	15.416016	1.311258
-65.641534	17.103786	1.316262
-65.833996	13.176047	1.321267
-65.579998	8.074686	1.326272
-66.097156	10.271694	1.331277
-65.971109	16.876747	1.336282
-66.123696	15.454731	1.341286
-66.308010	13.866819	1.346291
-66.776878	13.525396	1.351296
-67.412360	12.896714	1.356301
-67.262583	5.454667	1.361306
-67.033756	0.996282	1.366310
-68.015332	4.527892	1.371315
-68.504133	0.791823	1.376320
-69.218508	6.088269	1.381325
-69.010489	5.755346	1.386330
-68.931050	8.751611	1.391334
-69.295327	10.016852	1.396339
-69.175779	8.410102	1.401344
-69.497643	8.175500	1.406349
-69.492015	6.921833	1.411354
-69.994235	2.400108	1.416358
-70.468170	15.422693	1.421363
-70.255434	8.439061	1.426368
-71.481985	13.359690	1.431373
-71.562829	4.691258	1.436378
-71.747827	0.199233	1.441382
-72.015371	6.574508	1.446387
-71.788187	3.891180	1.451392
-71.904035	13.824080	1.456397
-72.000020	10.593140	1.461402
-72.815020	10.033537	1.466406
-73.105534	11.157583	1.471411
-73.126142	6.684251	1.476416
-73.316542	7.216927	1.481421
-73.490027	7.974751	1.486426
-73.590187	5.598646	1.491430
-74.371820	12.860695	1.496435
-74.488161	7.930886	1.501440
-74.523103	1.495166	1.506445
-74.532085	8.684367	1.511450
-75.123397	6.302479	1.516454
-75.729572	19.083074	1.521459
-75.634495	7.505172	1.526464
-75.896751	9.741584	1.531469
-76.127077	5.949452	1.536474
-75.924345	9.537103	1.541478
-76.822199	14.501463	1.546483
-76.964903	5.754081	1.551488
-77.285071	12.650061	1.556493
-77.377480	4.198559	1.561498
-77.395941	3.787008	1.566502
-78.670179	17.424565	1.571507
-78.610598	3.365570	1.576512
-78.755611	5.450854	1.581517
-78.754904	6.115120	1.586522
-78.929620	2.706622	1.591526
-78.915303	11.704961	1.596531
-79.059270	5.700653	1.601536
-80.232946	8.224499	1.606541
-80.417462	5.355346	1.611546
-80.274697	0.350396	1.616550
-80.362732	1.148698	1.621555
-80.701204	1.182427	1.626560
-80.405360	-5.184574	1.631565
-80.971498	-0.904594	1.636570
-81.760446	8.623758	1.641574
-81.796513	7.654984	1.646579
-81.933759	-5.576120	1.651584
-81.812805	-4.443377	1.656589
-82.601494	1.361329	1.661594
-83.283564	-2.800210	1.666598
-83.497612	4.351317	1.671603
-83.253187	-7.781319	1.676608
-83.406427	-7.010830	1.681613
-83.274305	-2.728842	1.686618
-83.758132	2.727852	1.691622
-84.140045	-3.514641	1.696627
-84.702572	1.704378	1.701632
-84.907977	3.352991	1.706637
-84.984458	5.035312	1.711642
-84.989017	-0.690153	1.716646
-85.502486	5.157120	1.721651
-85.644139	-2.679293	1.726656
-86.110598	-1.746144	1.731661
-86.474831	5.280076	1.736666
-86.476383	9.174770	1.741670
-86.367063	5.082992	1.746675
-86.428938	0.043470	1.751680
-87.443944	9.591201	1.756685
-87.743764	2.813923	1.761690
-87.549786	0.964639	1.766694
-88.035828	10.230702	1.771699
-88.073320	5.045017	1.776704
-88.703077	6.386393	1.781709
-89.073510	1.619530	1.786714
-89.033159	-2.040744	1.791718
-89.509406	7.132046	1.796723
-89.405496	1.649110	1.801728
-89.417650	-0.237678	1.806733
-89.634946	1.643731	1.811738
-90.061632	-3.487680	1.816742
-90.805781	2.832091	1.821747
-90.844065	4.587556	1.826752
-91.041500	5.301655	1.831757
-91.233366	-2.121994	1.836762
-91.213864	1.430911	1.841766
-91.935001	11.853507	1.846771
-92.075053	1.251822	1.851776
-92.245355	4.460971	1.856781
-92.213936	2.383906	1.861786
-92.596848	-4.611376	1.866790
-93.368517	9.219996	1.871795
-93.651056	5.809305	1.876800
-93.891776	5.071705	1.881805
-94.246402	3.836167	1.886810
-94.198636	8.688092	1.891814
-94.332322	8.917719	1.896819
-94.263260	6.303302	1.901824
-94.572736	9.863139	1.906829
-94.819913	6.193850	1.911834
-94.998188	8.433004	1.916838
-96.062792	15.321511	1.921843
-95.616540	7.934540	1.926848
-95.858051	8.142992	1.931853
-95.914137	13.162943	1.936858
-96.052928	3.045098	1.941862
-97.093311	7.762739	1.946867
-96.972117	3.684931	1.951872
-97.185278	10.377593	1.956877
-97.615355	13.133663	1.961882
-97.522519	7.943504	1.966886
-97.967495	4.520140	1.971891
-98.266749	6.708530	1.976896
-98.570876	5.794148	1.981901
-98.872178	6.084673	1.986906
-98.532166	-0.864989	1.991910
-99.194223	10.317171	1.996915
-99.852209	6.231656	2.006912
-99.432791	11.317041	2.016909
-98.821233	15.552079	2.026906
-98.406495	11.990395	2.036902
-97.672847	6.871237	2.046899
-97.669646	3.126552	2.056896
-97.079448	0.342145	2.066893
-96.369790	5.683268	2.076890
-95.570901	6.702441	2.086886
-95.217503	5.741480	2.096883
-95.043249	7.513620	2.106880
-94.341311	7.081247	2.116877
-93.823189	7.573950	2.126874
-93.013037	11.391608	2.136870
-92.512377	9.074121	2.146867
-92.208126	4.338590	2.156864
-92.022323	11.753757	2.166861
-91.341020	7.149580	2.176858
-91.148933	8.003481	2.186854
-90.180163	12.002342	2.196851
-89.482717	11.367936	2.206848
-89.512937	12.487692	2.216845
-88.671775	11.153023	2.226842
-88.445934	10.772605	2.236838
-87.889992	7.930176	2.246835
-86.936581	6.007846	2.256832
-86.807976	7.517841	2.266829
-86.406058	9.058137	2.276826
-85.441207	10.434760	2.286822
-85.352165	11.722841	2.296819
-85.163770	12.038809	2.306816
-84.129339	6.160089	2.316813
-83.940245	3.149873	2.326810
-83.148599	5.247188	2.336806
-82.525415	3.705715	2.346803
-82.076515	7.595458	2.356800
-81.828013	-1.205042	2.366797
-81.066470	6.855385	2.376794
-80.782928	4.970833	2.386790
-80.567120	7.088117	2.396787
-79.469904	3.084398	2.406784
-79.439084	0.292055	2.416781
-78.792745	8.870916	2.426778
-78.152448	5.087220	2.436774
-77.902943	8.231925	2.446771
-76.727516	8.688809	2.456768
-76.233363	11.532504	2.466765
-76.549973	8.075189	2.476762
-76.244776	0.425235	2.486758
-75.406413	1.159505	2.496755
-74.938942	3.972509	2.506752
-74.161194	7.129998	2.516749
-73.923201	12.075745	2.526746
-72.948821	9.104812	2.536742
-72.392255	4.675273	2.546739
-72.194095	7.789960	2.556736
-72.017328	3.077446	2.566733
-71.215791	5.008502	2.576730
-70.979055	11.617482	2.586726
-70.102098	11.778727	2.596723
-69.708554	3.114026	2.606720
-69.550139	8.084833	2.616717
-68.675875	5.709176	2.626714
-68.136112	9.600611	2.636710
-67.753026	8.562171	2.646707
-67.120777	13.871005	2.656704
-66.650617	1.478672	2.666701
-66.209578	-0.712327	2.676698
-65.490258	-0.523371	2.686694
-65.191560	1.428958	2.696691
-64.815137	2.789498	2.706688
-63.942123	3.600733	2.716685
-63.959069	8.836421	2.726682
-63.552414	6.574750	2.736678
-62.603711	6.588614	2.746675
-62.363343	6.598727	2.756672
-61.316651	0.467852	2.766669
-61.294318	10.794239	2.776666
-60.858926	2.762896	2.786662
-59.808824	3.125256	2.796659
-59.703167	1.021320	2.806656
-59.435958	1.622781	2.816653
-58.257721	-1.598461	2.826650
-58.137542	5.221895	2.836646
-58.161288	3.892017	2.846643
-56.833502	5.737969	2.856640
-56.710549	10.229642	2.866637
-56.597468	2.074259	2.876634
-55.491739	5.342235	2.886630
-55.093535	1.786294	2.896627
-54.869387	-0.063669	2.906624
-54.002993	-2.222696	2.916621
-53.550329	9.072524	2.926618
-53.379908	1.855353	2.936614
-52.817140	-1.995462	2.946611
-52.321415	3.619718	2.956608
-51.320305	-1.328847	2.966605
-50.883882	-1.510811	2.976602
-50.609835	-2.548111	2.986598
-50.565632	6.083323	2.996595
-49.680186	-4.970379	3.006592
-49.248124	-1.141368	3.016589
-48.344872	1.540433	3.026586
-48.096998	6.738056	3.036582
-47.832088	9.395707	3.046579
-46.893395	3.845495	3.056576
-46.727016	6.011656	3.066573
-46.342935	3.924556	3.076570
-45.245164	0.703171	3.086566
-45.005721	-3.829039	3.096563
-44.781479	5.740509	3.106560
-44.551105	3.905414	3.116557
-43.734396	-3.472567	3.126554
-43.403550	-0.536924	3.136550
-42.191962	1.596375	3.146547
-42.025751	1.532507	3.156544
-42.035170	1.790580	3.166541
-40.737966	3.460736	3.176538
-40.676185	2.896794	3.186534
-40.307296	4.404222	3.196531
-39.361962	-0.627522	3.206528
-38.743626	2.450255	3.216525
-38.949041	3.217165	3.226522
-38.529509	12.848174	3.236518
-37.650469	6.566009	3.246515
-37.276898	6.444514	3.256512
-36.426228	4.142221	3.266509
-36.150987	5.692739	3.276506
-35.739992	5.166288	3.286502
-34.639242	6.189146	3.296499
-34.433763	1.823774	3.306496
-34.530566	2.877873	3.316493
-33.438903	5.140713	3.326490
-33.118191	5.211175	3.336486
-32.810467	5.730303	3.346483
-31.816179	5.619866	3.356480
-31.319202	2.191093	3.366477
-31.298545	4.937456	3.376474
-30.988097	1.730955	3.386470
-30.034591	-1.746724	3.396467
-29.955895	1.836376	3.406464
-29.137225	4.819607	3.416461
-28.683364	3.757478	3.426458
-27.683546	5.071641	3.436454
-27.229363	4.015797	3.446451
-27.241399	0.498388	3.456448
-26.912587	1.121935	3.466445
-26.235286	5.410092	3.476442
-25.967378	4.278717	3.486438
-24.899951	5.984651	3.496435
-24.412529	2.823451	3.506432
-24.144783	4.809110	3.516429
-23.385477	4.073211	3.526426
-23.236997	-3.188058	3.536422
-22.803217	-5.894260	3.546419
-21.987815	-2.533565	3.556416
-21.718457	-2.049644	3.566413
-21.021660	4.475037	3.576410
-20.326866	10.290468	3.586406
-20.069062	1.279447	3.596403
-19.805788	2.781145	3.606400
-18.847743	-3.443629	3.616397
-18.921507	2.361586	3.626394
-17.876978	-3.905162	3.636390
-17.044874	-3.014698	3.646387
-16.990423	3.587819	3.656384
-17.088656	-4.316092	3.666381
-16.391933	2.604561	3.676378
-15.554915	3.548111	3.686374
-14.703470	-1.183922	3.696371
-14.163531	-2.272124	3.706368
-14.182212	-0.010628	3.716365
-14.030606	3.652984	3.726362
-13.109038	3.287783	3.736358
-12.607520	3.102020	3.746355
-12.100604	5.424229	3.756352
-11.551268	-1.357779	3.766349
-11.213834	2.457459	3.776346
-10.603640	2.476514	3.786342
-9.779652	5.930905	3.796339
-9.702055	5.079408	3.806336
-8.673180	8.764818	3.816333
-8.026928	7.482672	3.826330
-7.970490	10.761974	3.836326
-8.242214	10.202442	3.846323
-7.447174	3.562736	3.856320
-6.296622	1.638223	3.866317
-5.503753	4.505101	3.876314
-5.798080	2.374745	3.886310
-5.323107	3.609074	3.896307
-4.647428	13.656354	3.906304
-4.011723	17.190746	3.916301
-3.843797	17.839342	3.926298
-3.474431	31.836925	3.936294
-2.499011	40.586312	3.946291
-2.213450	46.912119	3.956288
-1.940337	56.676822	3.966285
-1.877235	59.932922	3.976282
-1.275095	78.050326	3.986278
-0.636387	95.126214	3.996275
-0.093146	119.480548	4.006272
0.000000	129.123883	4.011277
0.213422	129.277322	4.016282
0.312470	146.041995	4.021286
0.543058	149.577886	4.026291
1.048327	167.101886	4.031296
0.919924	172.917736	4.036301
1.401608	161.326988	4.041306
1.146789	170.550811	4.046310
1.427694	168.596229	4.051315
1.385902	171.760092	4.056320
1.411975	169.047941	4.061325
1.633952	172.452303	4.066330
1.353284	168.658479	4.071334
1.587199	165.758949	4.076339
1.382108	180.951209	4.081344
1.332141	169.607744	4.086349
1.371987	162.065688	4.091354
1.166311	170.500432	4.096358
1.563838	160.298986	4.101363
1.541406	165.456109	4.106368
1.273256	161.698302	4.111373
1.567043	160.766745	4.116378
1.354427	163.153631	4.121382
1.848909	164.326303	4.126387
0.999327	160.304693	4.131392
1.165720	171.376955	4.136397
1.706860	163.661938	4.141402
1.603947	171.210674	4.146406
1.859422	173.189331	4.151411
1.635605	163.692049	4.156416
1.000844	152.809794	4.161421
1.499737	164.016939	4.166426
1.758612	174.195303	4.171430
2.108655	165.108532	4.176435
1.478926	161.729717	4.181440
1.207658	160.993701	4.186445
1.536575	169.943144	4.191450
1.542442	172.716783	4.196454
1.785743	175.687566	4.201459
1.605044	182.808667	4.206464
1.814049	187.730451	4.211469
1.910277	177.136155	4.216474
1.297298	173.042903	4.221478
1.758757	175.334330	4.226483
1.676464	178.501337	4.231488
1.609364	185.351658	4.236493
1.858435	180.425014	4.241498
1.801337	182.699106	4.246502
1.596568	183.749702	4.251507
1.607102	187.259752	4.256512
1.669916	187.136092	4.261517
1.858043	183.455933	4.266522
1.660801	184.021315	4.271526
1.685644	178.414593	4.276531
1.706471	189.623423	4.281536
1.364656	187.911323	4.286541
1.672806	183.323484	4.291546
1.519342	191.690000	4.296550
1.671517	184.057680	4.301555
1.700417	187.049192	4.306560
1.836615	198.942400	4.311565
2.056382	194.339847	4.316570
1.930074	195.321281	4.321574
1.880263	186.878872	4.326579
1.784981	184.951222	4.331584
2.065187	208.182773	4.336589
2.226766	203.813898	4.341594
1.847250	192.860240	4.346598
2.155857	190.790615	4.351603
2.133817	190.449217	4.356608
1.530168	177.980265	4.361613
1.927638	196.394252	4.366618
2.173933	207.735663	4.371622
2.215189	201.658154	4.376627
2.058067	199.553474	4.381632
2.273733	202.724712	4.386637
2.540167	195.001834	4.391642
2.007293	196.337628	4.396646
2.229825	181.060407	4.401651
1.795338	189.622532	4.406656
2.084395	195.794161	4.411661
2.199980	201.556213	4.416666
1.953847	209.263302	4.421670
1.959930	194.032425	4.426675
2.272164	201.206496	4.431680
2.160462	212.834598	4.436685
2.063953	199.217347	4.441690
2.112719	197.833567	4.446694
2.537370	199.175298	4.451699
2.452402	205.547530	4.456704
2.361368	199.623493	4.461709
2.438719	197.640491	4.466714
2.308456	202.675212	4.471718
2.197972	201.151715	4.476723
2.390856	198.030783	4.481728
1.964976	210.375335	4.486733
2.594674	200.403467	4.491738
2.374215	210.545754	4.496742
2.581567	196.915995	4.501747
2.460732	208.381005	4.506752
2.454880	214.019604	4.511757
2.707443	200.825718	4.516762
2.411377	208.325451	4.521766
2.532195	207.480932	4.526771
2.809504	204.365836	4.531776
2.085181	194.313729	4.536781
1.947355	199.476173	4.541786
1.875550	205.666027	4.546790
2.113315	204.708389	4.551795
2.599307	201.222289	4.556800
2.298502	211.130319	4.561805
2.573711	204.285574	4.566810
2.074766	209.333407	4.571814
2.160385	211.385971	4.576819
2.550439	219.563474	4.581824
2.571716	225.802115	4.586829
3.004747	221.527010	4.591834
2.149545	222.305564	4.596838
2.377473	221.738590	4.601843
2.282027	226.995682	4.606848
2.579003	235.545180	4.611853
2.702201	231.011435	4.616858
2.653658	238.890248	4.621862
2.965329	233.909552	4.626867
2.744347	232.880972	4.631872
2.748640	235.373297	4.636877
2.937821	234.303003	4.641882
2.679005	231.372613	4.646886
2.785935	231.517324	4.651891
2.823549	229.723998	4.656896
2.772404	225.663478	4.661901
3.371884	233.492013	4.666906
2.507348	234.936395	4.671910
3.024327	230.550142	4.676915
2.846513	227.186372	4.681920
2.905181	229.999253	4.686925
3.317510	234.557207	4.691930
2.710531	224.670306	4.696934
2.807003	225.588583	4.701939
3.215187	232.652818	4.706944
3.111135	230.906859	4.711949
2.975283	217.975911	4.716954
2.358295	224.465784	4.721958
2.616493	218.430420	4.726963
3.067945	227.670856	4.731968
3.055358	238.207891	4.736973
2.886810	233.241853	4.741978
2.843079	243.495844	4.746982
2.891255	233.649299	4.751987
3.214522	238.477379	4.756992
2.942075	230.237287	4.761997
3.029710	223.329992	4.767002
3.189105	238.759775	4.772006
3.097595	236.572111	4.777011
3.337408	239.236570	4.782016
2.840830	242.116921	4.787021
2.962299	231.398443	4.792026
3.042420	243.591471	4.797030
3.005469	239.000403	4.802035
3.065807	238.045079	4.807040
2.660160	234.564923	4.812045
2.736124	234.499325	4.817050
2.857321	238.681838	4.822054
2.904835	237.658909	4.827059
3.091031	244.915896	4.832064
3.201078	255.541412	4.837069
3.342380	249.514747	4.842074
3.217333	254.615108	4.847078
3.486140	258.005868	4.852083
3.532164	256.537090	4.857088
3.074581	240.568460	4.862093
3.223926	231.313592	4.867098
3.341499	250.457733	4.872102
3.151425	248.041809	4.877107
3.527467	261.963604	4.882112
3.401578	253.105910	4.887117
3.657007	245.324613	4.892122
3.094703	241.441749	4.897126
3.164074	242.563559	4.902131
3.287839	262.396432	4.907136
3.124028	252.453170	4.912141
3.460596	256.608483	4.917146
3.334544	260.076539	4.922150
3.522567	254.678500	4.927155
3.536306	258.207047	4.932160
3.375558	267.425764	4.937165
3.430025	258.710825	4.942170
3.194469	259.617526	4.947174
3.194113	258.121169	4.952179
3.505402	257.762673	4.957184
3.242351	264.801718	4.962189
3.555219	261.070484	4.967194
3.403762	269.063408	4.972198
3.422910	262.201562	4.977203
3.786571	263.600250	4.982208
3.663340	264.853286	4.987213
3.760588	264.221237	4.992218
3.458253	261.756353	4.997222
3.664251	257.693754	5.002227
3.791193	257.674001	5.007232
3.399579	254.194820	5.012237
3.619051	251.686658	5.017242
3.614833	257.056102	5.022246
3.408694	250.985458	5.027251
3.617061	259.327306	5.032256
3.907131	274.407751	5.037261
3.803909	265.644596	5.042266
3.254223	268.669259	5.047270
3.574439	270.169621	5.052275
3.581325	272.832388	5.057280
3.641665	276.802927	5.062285
3.911666	281.664621	5.067290
3.640340	279.536585	5.072294
3.951611	274.071895	5.077299
4.193956	272.104323	5.082304
4.013685	274.508334	5.087309
4.279882	269.623291	5.092314
4.129588	276.787150	5.097318
3.612318	267.904966	5.102323
4.002351	261.346035	5.107328
3.912555	278.443950	5.112333
4.041996	262.712926	5.117338
3.616305	269.315397	5.122342
3.754827	269.278023	5.127347
4.108902	274.420849	5.132352
4.009271	276.473789	5.137357
3.818043	290.936336	5.142362
3.806934	280.732006	5.147366
4.002729	279.078560	5.152371
4.072561	277.776913	5.157376
3.956406	283.094192	5.162381
3.972053	283.234134	5.167386
3.925505	281.336851	5.172390
4.206423	283.865206	5.177395
4.163684	280.350683	5.182400
3.798661	276.617426	5.187405
4.227925	281.166427	5.192410
3.781893	280.666420	5.197414
3.839993	279.043903	5.202419
4.002388	281.188923	5.207424
4.129768	288.436102	5.212429
4.231358	278.476814	5.217434
3.836198	279.946193	5.222438
3.971850	276.220402	5.227443
4.173617	279.548839	5.232448
4.074205	294.237534	5.237453
4.652829	284.213460	5.242458
4.032138	283.740647	5.247462
3.996235	285.625481	5.252467
4.287500	299.816764	5.257472
4.339613	304.383365	5.262477
4.537849	306.418405	5.267482
4.333635	296.709196	5.272486
4.377379	285.442813	5.277491
4.142274	293.372843	5.282496
4.345371	306.470566	5.287501
4.594665	315.033854	5.292506
4.159753	298.504832	5.297510
4.505711	304.025409	5.302515
4.380217	296.948793	5.307520
4.087800	297.788420	5.312525
4.230243	305.552107	5.317530
4.628349	311.349300	5.322534
4.425612	303.398872	5.327539
4.718743	303.789834	5.332544
4.653315	318.223326	5.337549
4.736256	297.991242	5.342554
4.157218	294.354576	5.347558
4.256235	305.184316	5.352563
4.723160	305.345743	5.357568
4.597114	318.656070	5.362573
4.823806	313.710728	5.367578
4.547079	310.596455	5.372582
4.540308	310.787343	5.377587
4.695085	302.455391	5.382592
4.360855	302.491622	5.387597
4.336194	304.390527	5.392602
4.638971	313.132146	5.397606
4.707409	325.763639	5.402611
4.832914	311.260701	5.407616
4.611881	320.188280	5.412621
4.769240	308.834592	5.417626
4.765891	321.682900	5.422630
4.569338	315.936602	5.427635
4.780905	311.667483	5.432640
4.384690	310.745274	5.437645
4.556069	312.493436	5.442650
4.897453	308.093377	5.447654
4.661498	310.221329	5.452659
4.688712	302.871002	5.457664
4.491466	310.940675	5.462669
5.021580	297.437754	5.467674
4.906902	315.656363	5.472678
5.166223	309.952982	5.477683
4.753429	305.755765	5.482688
4.514025	320.355548	5.487693
4.721686	310.398709	5.492698
4.647874	310.527270	5.497702
4.420762	310.186162	5.502707
4.898202	305.388440	5.507712
4.652613	320.356175	5.512717
4.919474	312.857802	5.517722
4.995670	313.614728	5.522726
4.697864	308.944035	5.527731
5.190678	313.043397	5.532736
4.714457	312.699947	5.537741
4.667242	316.851753	5.542746
4.843239	325.435950	5.547750
4.894181	336.203593	5.552755
5.626214	327.082575	5.557760
5.451577	338.359896	5.562765
4.981303	318.406908	5.567770
5.113460	316.317285	5.572774
5.074715	310.812169	5.577779
4.872484	310.634863	5.582784
4.517164	317.707277	5.587789
5.165835	324.879636	5.592794
5.055924	339.348543	5.597798
5.251655	339.966639	5.602803
5.506264	337.475140	5.607808
5.260456	343.663660	5.612813
5.367166	338.037814	5.617818
5.225411	333.909120	5.622822
5.028479	319.491178	5.627827
5.033612	314.089959	5.632832
5.052809	328.345770	5.637837
5.234700	329.643052	5.642842
5.156472	333.034076	5.647846
5.167508	342.396925	5.652851
5.395160	337.460918	5.657856
5.341237	331.455130	5.662861
5.474232	330.902933	5.667866
5.471703	332.466207	5.672870
4.943029	345.098935	5.677875
5.241111	332.160453	5.682880
5.305049	335.791929	5.687885
5.542709	337.839817	5.692890
5.213142	333.259482	5.697894
5.326313	335.497592	5.702899
5.218711	332.493023	5.707904
4.895731	334.669328	5.712909
5.384075	335.494961	5.717914
5.438690	338.058559	5.722918
5.340150	336.213656	5.727923
4.987849	336.388741	5.732928
4.896480	335.846167	5.737933
5.574313	336.768845	5.742938
5.431708	340.767833	5.747942
5.554287	353.118838	5.752947
5.454548	342.744777	5.757952
5.497772	348.375778	5.762957
5.551788	349.993523	5.767962
5.620944	356.474688	5.772966
5.524817	365.449280	5.777971
5.856462	349.670879	5.782976
5.274900	366.076664	5.787981
5.265879	347.412222	5.792986
5.443991	350.696900	5.797990
5.305426	355.831031	5.802995
5.375729	358.303605	5.808000
5.509200	360.870747	5.813005
5.874394	352.996385	5.818010
5.994543	349.421686	5.823014
5.217722	349.628066	5.828019
5.559908	353.266843	5.833024
5.557177	359.737056	5.838029
5.351157	345.921611	5.843034
5.484588	351.139941	5.848038
5.547783	384.330052	5.853043
6.004594	382.866907	5.858048
6.018997	387.853847	5.863053
6.303821	377.647678	5.868058
6.017118	377.122861	5.873062
5.662515	365.399600	5.878067
5.824248	365.228900	5.883072
5.383060	361.890292	5.888077
5.726608	365.592133	5.893082
6.269252	379.965801	5.898086
6.001243	382.984591	5.903091
5.807893	368.044040	5.908096
5.555839	375.796414	5.913101
6.100600	374.148737	5.918106
6.414149	383.208247	5.923110
5.900140	370.791640	5.928115
5.854452	360.959638	5.933120
5.845405	370.417377	5.938125
5.779738	381.041853	5.943130
5.886485	392.057102	5.948134
5.859463	383.892620	5.953139
5.822775	383.059961	5.958144
5.707565	394.840586	5.963149
5.835489	383.431323	5.968154
6.084001	384.348082	5.973158
6.233925	389.367705	5.978163
5.985562	382.664520	5.983168
6.107276	390.532711	5.988173
6.196399	384.080696	5.993178
6.400568	386.038892	5.998182
6.356738	387.276412	6.003187
6.511609	383.901942	6.008192
6.577633	384.862932	6.013197
6.301215	379.840883	6.018202
6.205802	377.527260	6.023206
6.396490	374.305401	6.028211
6.271203	368.525844	6.033216
5.687510	366.262936	6.038221
6.135540	370.147825	6.043226
6.270900	383.509248	6.048230
6.243425	391.894205	6.053235
6.351571	377.181948	6.058240
6.067524	380.133633	6.063245
6.090653	368.310431	6.068250
5.982988	376.359859	6.073254
5.699108	384.120355	6.078259
6.045289	382.772511	6.083264
6.081166	385.952792	6.088269
6.103572	389.720458	6.093274
6.195410	391.980879	6.098278
5.824714	394.658159	6.103283
5.948432	383.945567	6.108288
5.821307	390.197880	6.113293
6.271806	382.288077	6.118298
6.134607	390.690118	6.123302
5.944889	396.556716	6.128307
6.248188	388.616046	6.133312
5.813336	386.959540	6.138317
6.244786	382.861810	6.143322
6.445711	375.022506	6.148326
6.292345	383.186618	6.153331
6.481198	389.206240	6.158336
6.270617	386.869419	6.163341
6.231491	386.198489	6.168346
6.221625	392.150976	6.173350
6.203776	386.854551	6.178355
6.656679	386.780884	6.183360
6.477992	385.799493	6.188365
6.559553	389.972394	6.193370
6.569636	380.669529	6.198374
5.737584	367.903815	6.203379
5.667462	375.653173	6.208384
5.583262	387.985777	6.213389
6.166833	388.220791	6.218394
6.441826	389.747188	6.223398
5.968643	398.536897	6.228403
6.132699	385.578115	6.233408
6.186828	390.827786	6.238413
6.228343	391.735646	6.243418
6.252128	398.100506	6.248422
6.292381	392.959547	6.253427
6.493286	399.733422	6.258432
6.298463	396.093861	6.263437
6.143762	389.784209	6.268442
6.511823	387.749596	6.273446
6.013883	382.837965	6.278451
6.023960	367.976470	6.283456
5.932500	383.901010	6.288461
6.454710	376.571659	6.293466
6.118293	379.904815	6.298470
6.217388	385.008280	6.303475
6.524762	381.347478	6.308480
6.147863	377.141492	6.313485
5.834922	372.308626	6.318490
6.094834	372.926222	6.323494
6.037884	392.474169	6.328499
6.407551	382.941313	6.333504
6.213528	385.417081	6.338509
6.256996	376.631032	6.343514
6.010882	374.432621	6.348518
5.901372	374.598377	6.353523
6.334999	383.291184	6.358528
6.292028	387.309470	6.363533
6.314558	376.685402	6.368538
6.042655	372.491543	6.373542
6.027788	370.658919	6.378547
6.113992	375.403725	6.383552
6.300529	381.126316	6.388557
6.197620	379.019502	6.393562
6.022173	379.701717	6.398566
5.883977	390.097050	6.403571
6.323779	385.153308	6.408576
6.203579	386.127475	6.413581
6.191070	388.366177	6.418586
6.499506	388.365622	6.423590
5.776068	375.658921	6.428595
6.339570	369.746812	6.433600
6.215486	381.275713	6.438605
6.014884	375.052305	6.443610
6.359453	386.144416	6.448614
5.873599	379.560465	6.453619
6.593176	381.001822	6.458624
6.195405	374.397831	6.463629
5.870444	376.890821	6.468634
6.083867	372.127860	6.473638
6.070038	390.719980	6.478643
6.603032	383.680007	6.483648
6.372551	383.858271	6.488653
5.942575	373.734923	6.493658
5.897738	363.270046	6.498662
6.208169	379.850170	6.503667
6.404833	376.678000	6.508672
6.250970	372.978283	6.513677
6.387036	367.784448	6.518682
6.071164	364.954667	6.523686
6.064341	367.822059	6.528691
6.353210	354.239599	6.533696
6.143208	363.817206	6.538701
6.449847	366.338404	6.543706
6.016668	364.121664	6.548710
5.813407	370.502882	6.553715
5.995313	365.558171	6.558720
5.850126	363.151062	6.563725
6.244372	381.173443	6.568730
6.485661	381.537678	6.573734
6.059548	369.901477	6.578739
6.452819	372.089654	6.583744
6.271573	359.298547	6.588749
6.227761	369.498841	6.593754
6.399831	366.014130	6.598758
6.117836	356.503657	6.603763
6.743891	367.131156	6.608768
6.300415	370.291157	6.613773
5.976547	363.096705	6.618778
6.239105	367.421752	6.623782
6.032392	373.850965	6.628787
6.523640	365.444450	6.633792
6.275486	368.608840	6.638797
6.058499	360.227178	6.643802
6.397394	359.952965	6.648806
6.264931	372.596790	6.653811
6.309219	356.812503	6.658816
6.436802	368.586946	6.663821
6.243303	365.513489	6.668826
6.274355	362.917590	6.673830
6.184241	368.863582	6.678835
6.345728	362.972939	6.683840
6.078273	356.310701	6.688845
6.177909	342.760876	6.693850
6.155846	345.893224	6.698854
6.124101	352.747597	6.703859
6.061420	351.185007	6.708864
6.203760	359.157538	6.713869
6.273179	351.829092	6.718874
6.084812	358.207987	6.723878
6.024283	355.341615	6.728883
6.167302	361.314580	6.733888
6.174589	364.461345	6.738893
6.264978	360.619199	6.743898
5.981351	348.587511	6.748902
6.286987	363.830121	6.753907
6.204615	353.007267	6.758912
6.390845	353.772373	6.763917
6.027594	351.199904	6.768922
5.966098	341.911367	6.773926
6.334547	361.601852	6.778931
6.117967	354.118622	6.783936
5.982778	357.429935	6.788941
6.101007	364.336890	6.793946
6.291133	356.024719	6.798950
6.400198	362.189629	6.803955
6.089060	350.750672	6.808960
5.897386	348.316002	6.813965
5.963330	353.506875	6.818970
6.473068	355.477603	6.823974
6.069796	357.305750	6.828979
6.264772	357.721487	6.833984
6.368803	357.667336	6.838989
6.209868	347.397401	6.843994
6.213108	342.138834	6.848998
6.223668	341.311475	6.854003
6.056872	332.833427	6.859008
5.973578	338.212044	6.864013
6.126051	357.847568	6.869018
6.262110	346.240913	6.874022
6.285958	352.694330	6.879027
6.340289	345.111977	6.884032
6.060748	352.337118	6.889037
5.921615	338.890909	6.894042
6.113092	345.447937	6.899046
6.035927	362.354143	6.904051
6.424168	349.746455	6.909056
6.446047	361.208325	6.914061
5.848589	339.117469	6.919066
6.011250	339.019390	6.924070
6.143480	358.211984	6.929075
6.414132	355.350995	6.934080
6.279476	353.094105	6.939085
6.042459	353.700486	6.944090
6.183296	343.035872	6.949094
5.956763	355.675349	6.954099
6.114940	360.045119	6.959104
5.971468	365.777958	6.964109
6.123726	367.415209	6.969114
6.208184	370.293699	6.974118
6.341676	369.390253	6.979123
5.816802	369.275835	6.984128
6.186320	366.253921	6.989133
6.383595	371.715413	6.994138
6.430576	358.262358	6.999142
6.271964	366.417789	7.004147
6.210678	358.208035	7.009152
5.991279	351.437078	7.014157
5.999328	350.701857	7.019162
5.924201	358.603845	7.024166
6.052262	362.348727	7.029171
6.537269	366.854272	7.034176
6.428588	369.860907	7.039181
6.151678	364.538386	7.044186
6.140397	352.321926	7.049190
6.079244	359.918022	7.054195
5.985430	349.264629	7.059200
6.074721	360.905826	7.064205
6.347388	357.655387	7.069210
6.479534	363.946417	7.074214
6.244308	355.611888	7.079219
6.106234	344.762911	7.084224
6.074129	352.550632	7.089229
5.986969	349.160069	7.094234
5.834140	347.250853	7.099238
6.082543	357.171529	7.104243
6.390006	360.616400	7.109248
6.279772	368.659897	7.114253
6.250308	360.878616	7.119258
6.461461	353.585049	7.124262
6.119934	354.065335	7.129267
6.027731	338.476320	7.134272
5.958104	353.378721	7.139277
5.890915	359.118663	7.144282
6.264259	355.944297	7.149286
6.086220	364.169189	7.154291
5.984839	368.006743	7.159296
6.163572	364.264735	7.164301
6.381252	363.202650	7.169306
6.556811	363.453734	7.174310
6.061873	364.109764	7.179315
6.195667	362.817135	7.184320
6.206834	361.632182	7.189325
5.955513	358.488635	7.194330
5.921567	359.458862	7.199334
6.070546	362.295668	7.204339
6.315008	367.670720	7.209344
5.843988	373.634890	7.214349
5.844108	372.900903	7.219354
6.150634	364.504167	7.224358
6.317006	372.843116	7.229363
6.100507	365.198519	7.234368
6.071661	373.539390	7.239373
5.948869	365.557505	7.244378
6.220233	371.127682	7.249382
6.225312	367.118486	7.254387
6.442578	358.741978	7.259392
6.096662	368.856432	7.264397
6.283888	369.988374	7.269402
6.436545	363.112029	7.274406
6.164975	370.895913	7.279411
6.059962	363.996412	7.284416
6.285023	372.601466	7.289421
6.036171	362.592291	7.294426
6.354196	364.627669	7.299430
6.128123	363.916245	7.304435
6.245180	362.455381	7.309440
6.026567	369.326200	7.314445
6.071048	370.084903	7.319450
6.364429	359.478785	7.324454
6.031765	370.948407	7.329459
6.082244	364.856751	7.334464
6.279688	370.621932	7.339469
5.866809	371.948547	7.344474
5.800538	366.210421	7.349478
6.093065	370.597241	7.354483
6.426488	360.481590	7.359488
6.265725	363.508988	7.364493
6.187311	368.127565	7.369498
6.278468	368.322189	7.374502
5.818855	378.473333	7.379507
6.153136	364.709790	7.384512
6.051072	366.914978	7.389517
6.117546	361.187823	7.394522
6.301583	357.767689	7.399526
6.059159	371.545421	7.404531
5.954361	370.217173	7.409536
5.903550	365.700995	7.414541
5.954026	369.043514	7.419546
6.155437	363.447207	7.424550
6.241709	364.196239	7.429555
6.041796	360.453075	7.434560
6.138281	365.636034	7.439565
5.721039	369.045046	7.444570
6.469019	375.180086	7.449574
6.296454	369.455345	7.454579
6.311188	358.351618	7.459584
6.132122	363.700863	7.464589
6.144367	364.860048	7.469594
6.235301	368.715114	7.474598
6.022873	373.500089	7.479603
5.992294	365.165330	7.484608
6.288213	374.126342	7.489613
5.973652	367.819442	7.494618
6.171333	364.539548	7.499622
6.009098	367.725362	7.504627
5.912747	359.789982	7.509632
6.372802	372.626287	7.514637
6.025383	358.962560	7.519642
6.187325	363.303271	7.524646
5.809234	374.340213	7.529651
5.955509	384.298951	7.534656
6.118827	393.388185	7.539661
6.021637	398.487413	7.544666
6.496643	393.421131	7.549670
6.232021	394.164687	7.554675
6.541598	388.883721	7.559680
6.664325	382.081631	7.564685
6.433762	369.779078	7.569690
6.370451	367.549043	7.574694
6.043209	367.745535	7.579699
6.018408	363.282255	7.584704
6.109506	362.951712	7.589709
6.016549	361.514056	7.594714
6.352953	361.505983	7.599718
6.276560	367.010082	7.604723
6.559559	357.025669	7.609728
6.458018	362.897509	7.614733
6.206235	373.750272	7.619738
6.478980	367.345603	7.624742
6.290898	365.011610	7.629747
6.312125	362.777903	7.634752
6.335510	363.514581	7.639757
6.140589	364.788278	7.644762
6.235802	363.941410	7.649766
6.044919	364.638684	7.654771
6.319295	365.899423	7.659776
5.906774	365.223355	7.664781
5.796099	369.220542	7.669786
6.453271	368.400073	7.674790
6.232663	373.043953	7.679795
6.034985	368.901813	7.684800
6.374984	367.491658	7.689805
6.337511	369.943049	7.694810
6.566002	359.900683	7.699814
5.979510	352.734471	7.704819
5.951396	349.540355	7.709824
6.088361	353.476835	7.714829
5.784307	367.941193	7.719834
6.064726	351.759483	7.724838
6.068368	366.267680	7.729843
6.263619	352.633359	7.734848
6.054305	360.834646	7.739853
6.242061	367.762414	7.744858
6.162558	358.701296	7.749862
6.082697	360.213338	7.754867
6.273193	365.090597	7.759872
6.332193	360.598452	7.764877
6.036676	368.060201	7.769882
6.415205	364.160538	7.774886
6.312540	358.994384	7.779891
6.486574	365.294711	7.784896
6.129462	363.945638	7.789901
5.975255	362.220130	7.794906
6.337532	358.895629	7.799910
6.168108	360.817078	7.804915
5.860161	356.711091	7.809920
6.275283	362.553108	7.814925
6.173684	368.542015	7.819930
6.400966	361.132041	7.824934
5.901065	355.429796	7.829939
6.011714	360.354287	7.834944
6.546995	353.241206	7.839949
6.138788	354.437380	7.844954
6.084170	349.820560	7.849958
6.264495	363.896292	7.854963
5.869504	350.233651	7.859968
6.050230	362.006142	7.864973
6.039907	363.301717	7.869978
6.403702	362.084007	7.874982
6.236127	367.377680	7.879987
6.557305	370.181349	7.884992
5.978496	352.146610	7.889997
5.776992	358.657262	7.895002
6.105880	355.037408	7.900006
6.002342	366.189783	7.905011
6.390606	365.749699	7.910016
6.419007	364.169763	7.915021
6.351445	371.725734	7.920026
6.336898	357.254055	7.925030
5.970461	361.484047	7.930035
6.087796	353.679912	7.935040
6.319434	344.630467	7.940045
6.016529	354.225697	7.945050
6.150321	345.865355	7.950054
6.005631	356.606523	7.955059
6.259796	357.361052	7.960064
6.103148	355.158205	7.965069
6.181654	361.584133	7.970074
6.240671	362.628470	7.975078
6.107572	367.331490	7.980083
6.016044	364.106117	7.985088
6.263194	358.746296	7.990093
5.977495	369.072834	7.995098
6.310766	361.187620	8.000102
6.126549	373.409239	8.005107
6.244381	364.184518	8.010112
5.974871	368.060144	8.015130
5.999772	361.798654	8.020147
6.440170	368.180216	8.025165
5.971836	363.251463	8.030182
6.026247	371.924158	8.035200
5.614548	368.293019	8.040218
5.900444	370.331238	8.045235
6.055704	369.032199	8.050253
6.531880	373.536901	8.055270
6.230601	370.715347	8.060288
6.445099	364.007792	8.065306
6.460715	374.605154	8.070323
6.242038	375.008423	8.075341
5.909767	368.764672	8.080358
6.348144	373.417263	8.085376
6.495552	361.103121	8.090394
6.296913	374.223639	8.095411
6.246860	368.036929	8.100429
6.376344	374.258630	8.105446
6.245231	370.953014	8.110464
6.627015	372.730164	8.115482
6.474892	381.949389	8.120499
6.752743	365.667231	8.125517
6.357061	358.000699	8.130534
6.030974	352.213559	8.135552
6.192762	346.407261	8.140570
5.705280	358.616582	8.145587
5.929828	359.809175	8.150605
6.000527	372.026267	8.155622
6.335220	365.602939	8.160640
6.074275	362.693059	8.165658
5.765864	368.364432	8.170675
5.871464	363.788109	8.175693
6.136681	366.362849	8.180710
6.052424	375.789243	8.185728
6.360370	379.897284	8.190746
6.210266	386.572753	8.195763
7.024952	381.576770	8.200781
6.673946	386.084038	8.205798
5.968161	376.420926	8.210816
6.093724	371.033649	8.215834
6.187661	382.303595	8.220851
6.524738	385.646593	8.225869
6.638065	393.404457	8.230886
6.164927	389.748167	8.235904
6.485976	395.864314	8.240922
5.908479	394.237571	8.245939
6.815450	389.769988	8.250957
6.476048	398.428276	8.255974
6.258038	398.351783	8.260992
6.615532	392.922078	8.266010
6.626580	403.892535	8.271027
6.387167	383.566473	8.276045
6.065780	381.846210	8.281062
6.236950	386.344757	8.286080
6.361077	394.517485	8.291098
6.299153	394.116904	8.296115
6.406345	387.640631	8.301133
6.396836	385.647759	8.306150
6.446328	388.126709	8.311168
6.759338	385.528230	8.316186
6.594153	394.153079	8.321203
6.807194	388.436613	8.326221
6.534752	388.428552	8.331238
6.410297	394.036580	8.336256
6.828452	395.959540	8.341274
6.208667	395.547992	8.346291
6.708287	399.121292	8.351309
6.610136	394.440991	8.356326
6.399615	391.782019	8.361344
7.109873	396.221880	8.366362
6.890379	387.783171	8.371379
6.568294	372.708356	8.376397
6.306570	376.485392	8.381414
6.180265	370.831233	8.386432
6.611054	364.370854	8.391450
6.215295	373.315600	8.396467
6.524615	380.235100	8.401485
6.695395	390.003625	8.406502
6.736143	382.183930	8.411520
6.711795	369.685097	8.416538
6.523428	370.383431	8.421555
6.752588	373.468688	8.426573
6.344294	363.238585	8.431590
6.215169	374.338139	8.436608
6.496034	386.655056	8.441626
6.747487	390.468954	8.446643
6.794956	389.940894	8.451661
6.831587	384.797822	8.456678
6.516075	387.570274	8.461696
6.507649	380.846931	8.466714
6.614940	393.194033	8.471731
6.482063	389.355385	8.476749
6.844678	386.938521	8.481766
6.321849	400.586034	8.486784
6.371843	385.816175	8.491802
6.694328	391.199989	8.496819
6.672908	393.364949	8.501837
6.926310	387.721090	8.506854
6.536852	393.468203	8.511872
6.939748	392.566085	8.516890
6.360416	394.821065	8.521907
6.758259	385.213323	8.526925
6.753002	395.877061	8.531942
6.541023	393.142581	8.536960
6.751529	392.283039	8.541978
6.514913	396.715699	8.546995
6.719250	382.972640	8.552013
7.072960	392.381344	8.557030
6.603909	394.653866	8.562048
6.965099	391.454624	8.567066
6.880063	392.818490	8.572083
6.398188	391.886878	8.577101
6.630873	390.272842	8.582119
6.655128	391.928944	8.587136
6.517551	394.496977	8.592154
6.737680	399.186711	8.597171
6.724702	398.787977	8.602189
6.410303	389.287970	8.607207
6.476382	392.793077	8.612224
6.774020	388.663349	8.617242
6.618007	393.692497	8.622259
6.557272	411.433518	8.627277
6.847573	413.856045	8.632295
7.011578	416.440239	8.637312
7.340204	416.597358	8.642330
6.861899	409.164562	8.647347
6.795743	402.052589	8.652365
6.931291	398.497177	8.657383
6.708028	396.528118	8.662400
6.647546	396.023177	8.667418
6.815685	402.522877	8.672435
6.826433	405.758904	8.677453
7.122951	411.137300	8.682471
6.869109	409.835685	8.687488
6.749618	399.743622	8.692506
6.713621	405.413616	8.697523
6.604473	404.559664	8.702541
7.144769	414.204403	8.707559
7.115979	420.422361	8.712576
6.787625	411.044431	8.717594
7.341599	413.211320	8.722611
7.108966	406.469230	8.727629
7.022709	383.560096	8.732647
6.817792	396.195639	8.737664
6.636260	387.498569	8.742682
7.022735	398.704044	8.747699
6.877485	401.658262	8.752717
7.044738	402.449545	8.757735
6.782125	410.568890	8.762752
7.069082	407.923973	8.767770
7.351167	409.252770	8.772787
6.714742	407.278613	8.777805
6.963733	399.344441	8.782823
6.983660	417.991202	8.787840
7.029188	410.445291	8.792858
7.015201	416.553651	8.797875
6.911516	414.392412	8.802893
7.145448	416.056894	8.807911
6.965036	414.948962	8.812928
7.098646	415.272137	8.817946
7.114604	413.429923	8.822963
6.923443	414.797691	8.827981
7.218581	409.898371	8.832999
6.733555	406.717275	8.838016
6.961492	410.967162	8.843034
7.270092	415.693615	8.848051
6.586542	416.702567	8.853069
7.320427	418.134582	8.858087
7.133630	413.767864	8.863104
6.983404	416.839618	8.868122
7.476671	414.099466	8.873139
7.315413	417.005688	8.878157
7.035567	411.283909	8.883175
7.377894	411.183287	8.888192
6.852857	402.527069	8.893210
7.436752	408.974662	8.898227
6.861797	396.488958	8.903245
7.351551	399.918634	8.908263
6.929891	400.814231	8.913280
6.842754	413.863771	8.918298
7.026438	421.121567	8.923315
6.932062	424.708464	8.928333
7.469191	413.971389	8.933351
7.184884	423.368998	8.938368
6.977664	419.450405	8.943386
7.205484	416.025783	8.948403
7.137791	413.698002	8.953421
7.423419	413.498916	8.958439
7.150870	425.886246	8.963456
7.236520	418.248883	8.968474
7.573444	412.497343	8.973491
7.410157	412.194591	8.978509
7.284157	419.822479	8.983527
7.408430	424.498743	8.988544
7.249493	418.060738	8.993562
7.349854	395.321339	8.998579
6.818440	401.983602	9.003597
7.056710	411.643807	9.008615
6.949913	415.065387	9.013632
7.048770	416.280708	9.018650
7.186931	415.195756	9.023667
7.330881	415.356383	9.028685
7.202631	417.440154	9.033703
7.109804	412.370876	9.038720
7.242617	419.844865	9.043738
7.263703	417.364412	9.048755
7.039666	422.498828	9.053773
7.026984	418.303806	9.058791
7.103691	421.498010	9.063808
7.616021	413.762660	9.068826
7.360972	410.813987	9.073843
7.249406	423.772668	9.078861
7.433462	418.319469	9.083879
7.194394	416.324467	9.088896
7.238941	417.579801	9.093914
7.212580	411.884823	9.098931
7.467748	415.322626	9.103949
7.158206	415.986183	9.108967
7.263748	425.420920	9.113984
7.641134	441.342374	9.119002
7.712909	435.805670	9.124019
7.262871	431.470466	9.129037
7.151873	418.499120	9.134055
7.432809	425.120115	9.139072
7.459433	439.777119	9.144090
7.680802	444.981042	9.149107
6.984569	440.359137	9.154125
7.074296	443.592341	9.159143
7.349215	446.856670	9.164160
7.578837	448.591250	9.169178
7.856612	448.282939	9.174195
7.564190	455.529675	9.179213
7.740066	451.046524	9.184231
7.822642	449.771418	9.189248
7.243471	442.934953	9.194266
7.620481	442.936223	9.199283
7.206880	429.210448	9.204301
7.484886	438.056635	9.209319
7.613027	455.301257	9.214336
7.504595	453.014526	9.219354
7.567828	449.173732	9.224371
7.371174	451.908755	9.229389
7.467150	455.254592	9.234407
7.385769	457.217467	9.239424
7.012171	449.623192	9.244442
7.251057	450.785157	9.249459
7.313603	450.242126	9.254477
7.217610	445.305868	9.259495
7.485068	445.538779	9.264512
7.551765	441.394506	9.269530
7.718023	448.453065	9.274547
7.320485	458.385849	9.279565
7.710338	447.450788	9.284583
7.850991	449.931331	9.289600
7.799692	450.295919	9.294618
7.858753	446.891255	9.299635
7.682036	451.005348	9.304653
7.679029	441.993292	9.309671
7.972240	441.805647	9.314688
7.579629	445.303289	9.319706
7.739335	444.091911	9.324723
7.588935	446.441053	9.329741
7.255060	449.172195	9.334759
7.978879	444.023093	9.339776
7.742821	445.413632	9.344794
7.859691	446.727132	9.349811
7.813339	450.663145	9.354829
7.673419	450.221061	9.359847
7.805683	453.450800	9.364864
7.741997	446.527763	9.369882
7.855537	445.310950	9.374899
7.613221	448.100416	9.379917
7.833919	446.311525	9.384935
7.590946	444.216147	9.389952
7.652135	449.593326	9.394970
7.596901	452.057034	9.399987
7.737898	450.858035	9.405005
7.935796	452.774272	9.410023
7.533097	452.508794	9.415040
7.626215	443.188295	9.420058
7.756212	443.897022	9.425075
7.958226	447.841700	9.430093
7.917607	450.785946	9.435111
7.807228	454.744552	9.440128
7.623043	459.901175	9.445146
7.895658	451.316392	9.450163
8.152120	454.091314	9.455181
7.934525	444.203840	9.460199
7.793743	440.782957	9.465216
7.653691	443.597524	9.470234
7.754192	433.619506	9.475251
7.582964	429.960381	9.480269
7.671295	443.680021	9.485287
7.871410	441.162224	9.490304
7.405307	450.146361	9.495322
7.639767	458.238826	9.500339
7.563010	468.052246	9.505357
8.155529	472.220138	9.510375
8.049521	465.297372	9.515392
7.417263	472.297239	9.520410
7.784263	470.731707	9.525427
7.827465	471.258298	9.530445
8.119132	473.090513	9.535463
7.905479	469.210778	9.540480
7.899412	471.875106	9.545498
7.959773	470.571902	9.550515
8.136971	463.232675	9.555533
7.964505	468.034042	9.560551
7.851720	457.994548	9.565568
7.509211	468.161755	9.570586
8.005951	460.188982	9.575603
7.641159	465.973301	9.580621
7.672895	467.628245	9.585639
7.881266	464.629500	9.590656
7.802970	467.904648	9.595674
8.463583	480.588518	9.600691
8.201341	472.358387	9.605709
8.056473	473.475966	9.610727
8.354679	462.018705	9.615744
8.130522	469.955373	9.620762
7.988334	470.201574	9.625779
7.913102	469.058330	9.630797
7.997824	473.109633	9.635815
8.228368	458.469386	9.640832
8.182903	474.737559	9.645850
7.831346	460.891652	9.650867
8.238335	464.419430	9.655885
8.144018	467.886411	9.660903
8.585440	459.619309	9.665920
8.343578	465.775788	9.670938
8.341445	456.085123	9.675955
8.482188	467.363614	9.680973
8.068302	471.303209	9.685991
8.219586	457.224387	9.691008
8.294185	465.064048	9.696026
8.290122	469.492074	9.701043
8.056746	465.303001	9.706061
8.055220	469.572850	9.711079
8.255817	467.162267	9.716096
8.001079	472.992565	9.721114
8.390218	466.267248	9.726131
8.143788	463.604389	9.731149
8.169158	463.243862	9.736167
8.541575	460.251132	9.741184
8.086302	470.230780	9.746202
8.396219	466.982705	9.751219
8.311222	467.841666	9.756237
8.364151	473.280096	9.761255
8.523496	467.234310	9.766272
8.169925	472.805455	9.771290
8.385565	476.429296	9.776307
8.485131	471.954866	9.781325
8.412090	473.054950	9.786343
8.451316	463.364153	9.791360
8.293368	452.381842	9.796378
8.228533	443.054380	9.801395
8.210283	445.291433	9.806413
8.037377	461.017730	9.811431
8.313077	458.661723	9.816448
8.006120	475.311420	9.821466
7.957481	473.775889	9.826483
7.911099	469.223202	9.831501
7.806437	478.204724	9.836519
8.070078	467.264057	9.841536
8.085744	476.479296	9.846554
8.348314	494.611855	9.851571
8.666227	495.038873	9.856589
8.304224	488.190668	9.861607
8.645174	478.664314	9.866624
8.509070	481.490894	9.871642
8.259050	486.436879	9.876659
8.107152	475.750244	9.881677
8.064443	484.797860	9.886695
8.409703	487.599985	9.891712
8.471430	503.870430	9.896730
8.352675	495.725240	9.901747
8.658837	505.119317	9.906765
8.412119	504.741194	9.911783
8.635658	498.767450	9.916800
8.702476	504.642364	9.921818
8.488921	503.343937	9.926835
8.829041	495.480736	9.931853
8.518697	498.810952	9.936871
8.670865	490.446867	9.941888
8.411191	479.218458	9.946906
8.085394	478.186805	9.951923
8.793257	492.131901	9.956941
8.532058	497.846454	9.961959
8.668011	504.385915	9.966976
8.658506	509.651049	9.971994
8.638725	494.431237	9.977011
8.564791	477.866094	9.982029
8.571780	487.975740	9.987047
8.863332	489.186310	9.992064
8.546472	485.669763	9.997082
7.989636	477.122597	10.002099
8.307238	480.733720	10.007117
8.617286	497.959528	10.012135
8.857095	494.286883	10.017152
9.132043	494.506006	10.022170
8.525919	498.604920	10.027187
8.717248	489.508936	10.032205
8.654264	493.791515	10.037223
8.583383	485.654654	10.042240
8.787447	498.539002	10.047258
8.619332	494.210380	10.052275
8.696681	492.061968	10.057293
8.781091	493.961166	10.062311
8.615194	493.103423	10.067328
8.702390	491.994845	10.072346
8.806995	494.114951	10.077363
8.909038	497.510342	10.082381
8.484977	490.804335	10.087399
8.922446	489.376146	10.092416
8.951725	488.465926	10.097434
8.629838	472.346472	10.102451
8.595789	467.492078	10.107469
8.381488	483.291108	10.112487
8.598106	495.220491	10.117504
8.389767	491.399882	10.122522
8.456862	496.719354	10.127539
8.655299	494.353282	10.132557
8.953711	500.652863	10.137575
8.955406	489.932838	10.142592
8.803214	502.490822	10.147610
8.749137	491.738456	10.152627
8.675885	488.344918	10.157645
8.584649	489.924341	10.162663
8.855468	490.920399	10.167680
8.839513	497.543466	10.172698
8.605341	496.440745	10.177715
8.864127	493.714999	10.182733
8.531248	506.421033	10.187751
8.711124	497.358385	10.192768
8.897697	510.813484	10.197786
9.072223	522.496985	10.202803
9.321392	510.580289	10.207821
9.018599	508.424793	10.212839
8.712140	486.244057	10.217856
8.679843	494.987114	10.222874
8.809493	498.955692	10.227891
8.959127	508.270005	10.232909
9.102622	515.543565	10.237927
8.901763	524.120384	10.242944
8.861564	523.659617	10.247962
9.213219	526.498621	10.252979
9.358148	514.872694	10.257997
8.859232	499.276218	10.263015
8.593452	492.349917	10.268032
9.005444	507.675934	10.273050
8.743251	515.378714	10.278067
9.015569	525.772105	10.283085
8.801698	527.029813	10.288103
8.999700	522.969214	10.293120
8.890655	520.411182	10.298138
8.909530	524.491683	10.303155
9.085722	516.385765	10.308173
8.926735	529.923082	10.313191
9.019811	519.406553	10.318208
9.463255	514.152769	10.323226
9.211139	515.804577	10.328243
9.381794	516.210344	10.333261
9.343808	529.277561	10.338279
9.107325	532.795091	10.343296
9.193046	526.085436	10.348314
8.991899	524.125541	10.353331
9.057134	520.555808	10.358349
8.842281	520.784922	10.363367
8.772974	516.125344	10.368384
9.226275	517.875596	10.373402
8.902405	524.316251	10.378419
9.338674	518.236798	10.383437
9.240651	522.916142	10.388455
9.111503	524.441513	10.393472
9.396482	523.835446	10.398490
9.358353	528.638004	10.403507
9.321985	519.018904	10.408525
8.963876	519.768917	10.413543
9.226072	520.696895	10.418560
8.899168	522.732716	10.423578
8.835455	522.490195	10.428595
9.199658	523.317087	10.433613
8.859137	536.128469	10.438631
9.368013	544.074111	10.443648
9.361965	540.717435	10.448666
9.694615	550.574450	10.453683
9.500767	540.213030	10.458701
9.294716	529.676799	10.463719
9.021368	523.351239	10.468736
9.861015	539.207120	10.473754
9.026873	539.144509	10.478771
9.150032	525.745325	10.483789
9.323430	537.334342	10.488807
9.384761	545.848261	10.493824
9.704767	550.001798	10.498842
9.390396	541.076038	10.503859
9.135222	530.036237	10.508877
9.198859	547.830610	10.513895
9.296868	540.913917	10.518912
9.548618	549.268808	10.523930
9.549744	549.947113	10.528947
9.558719	548.604568	10.533965
9.652968	544.077301	10.538983
9.441671	551.513408	10.544000
9.393015	550.438601	10.549018
9.255109	557.509848	10.554035
9.339582	548.809152	10.559053
9.363634	548.947424	10.564071
9.379135	555.713931	10.569088
9.647690	549.909878	10.574106
9.633512	554.904366	10.579123
9.403352	549.408325	10.584141
9.688715	554.662274	10.589159
9.613701	559.707259	10.594176
9.881246	552.719986	10.599194
9.533737	552.786726	10.604211
9.579032	554.897140	10.609229
9.517957	547.667557	10.614247
9.144454	556.974986	10.619264
9.540230	556.645145	10.624282
9.512053	567.192639	10.629299
9.742543	548.601426	10.634317
9.332941	553.584898	10.639335
9.533411	563.613973	10.644352
9.735857	557.933815	10.649370
9.414603	560.852349	10.654387
9.720733	563.259809	10.659405
9.713367	556.766598	10.664423
9.781277	560.031622	10.669440
9.692540	549.559161	10.674458
9.680402	553.893796	10.679475
9.567174	543.882723	10.684493
10.020950	551.953707	10.689511
9.668619	556.748390	10.694528
9.602300	550.602017	10.699546
9.669678	557.281557	10.704563
9.724000	543.476528	10.709581
9.865460	547.979743	10.714599
9.780296	552.590823	10.719616
9.438154	547.481431	10.724634
9.565597	549.667412	10.729651
9.625586	549.323583	10.734669
9.660538	546.257155	10.739687
9.753950	554.945956	10.744704
9.706239	557.111874	10.749722
9.572378	560.367289	10.754739
9.872863	549.483949	10.759757
10.129376	548.528878	10.764775
9.524824	552.684362	10.769792
9.997254	553.371334	10.774810
9.704087	557.610875	10.779827
9.661245	557.734317	10.784845
9.814117	560.361290	10.789863
10.041262	564.491421	10.794880
9.767249	562.486065	10.799898
9.707309	563.031873	10.804915
10.019370	572.816371	10.809933
10.065859	570.615952	10.814951
9.917971	570.288709	10.819968
10.004155	558.807595	10.824986
9.571646	566.215036	10.830003
9.816079	572.106498	10.835021
10.203117	576.000307	10.840039
9.989150	578.517147	10.845056
10.217678	581.163900	10.850074
10.099128	572.605250	10.855091
9.977062	573.217533	10.860109
10.163303	551.856215	10.865127
10.105747	559.176874	10.870144
10.148004	540.217362	10.875162
9.544621	550.157001	10.880179
9.791377	565.082779	10.885197
10.161283	576.309881	10.890215
9.992288	588.914722	10.895232
10.147058	583.043171	10.900250
9.919299	583.217493	10.905267
10.104325	591.860492	10.910285
10.270073	579.423429	10.915303
10.194103	577.829031	10.920320
10.278243	581.552260	10.925338
10.317644	568.519520	10.930355
9.689158	570.737996	10.935373
10.262097	568.550282	10.940391
10.055991	571.375153	10.945408
10.227585	573.964500	10.950426
10.361741	578.115424	10.955443
9.852327	580.088153	10.960461
9.954456	578.825773	10.965479
10.031766	587.870533	10.970496
10.301133	583.439062	10.975514
10.277049	575.326431	10.980531
10.271717	585.071993	10.985549
10.459997	578.015004	10.990567
10.214122	572.313129	10.995584
10.296460	576.219666	11.000602
10.227857	574.854486	11.005619
10.274675	573.278839	11.010637
10.460671	563.950127	11.015655
10.109052	575.870211	11.020672
10.016753	574.657036	11.025690
10.227295	578.436321	11.030707
10.232593	574.617143	11.035725
10.510659	570.528289	11.040743
9.966138	573.248067	11.045760
10.223555	572.195029	11.050778
10.330457	577.631399	11.055795
10.059149	579.832132	11.060813
10.369065	574.457115	11.065831
9.844773	569.208827	11.070848
9.962087	571.134467	11.075866
10.270419	572.131000	11.080883
10.485141	591.918369	11.085901
10.713939	584.195533	11.090919
10.257048	585.001953	11.095936
10.206729	577.634989	11.100954
10.043953	586.351071	11.105971
10.056958	599.606052	11.110989
10.639881	593.910823	11.116007
10.404044	604.897753	11.121024
10.696002	598.888078	11.126042
10.757656	592.008583	11.131059
10.958605	595.738873	11.136077
10.872696	585.379555	11.141095
10.716314	580.878678	11.146112
10.546875	589.882965	11.151130
10.327695	579.951482	11.156147
10.224729	571.005414	11.161165
10.138597	570.498150	11.166183
10.397554	589.877859	11.171200
10.936298	593.243144	11.176218
10.790305	603.875272	11.181235
10.574108	598.238193	11.186253
10.793211	586.606982	11.191271
10.289588	579.989065	11.196288
10.239670	588.277338	11.201306
10.176625	593.323624	11.206323
10.224949	601.132723	11.211341
10.680687	600.793545	11.216359
10.507294	603.597550	11.221376
10.416475	593.440955	11.226394
10.915110	599.860869	11.231411
10.445378	601.982051	11.236429
10.921951	596.953449	11.241447
10.925624	596.596297	11.246464
10.766493	601.013787	11.251482
10.652739	596.970154	11.256499
10.277376	599.092421	11.261517
10.533060	597.017212	11.266535
11.013950	598.529656	11.271552
10.453183	596.976025	11.276570
10.984192	596.360052	11.281587
10.536279	601.652447	11.286605
10.848020	605.453849	11.291623
10.413246	605.628846	11.296640
10.536321	624.247140	11.301658
10.901297	626.528687	11.306675
11.051766	625.198819	11.311693
11.079892	624.670608	11.316711
10.902847	614.259194	11.321728
10.869733	606.252092	11.326746
10.697361	594.189542	11.331763
10.929494	607.369388	11.336781
10.896272	616.251498	11.341799
10.982840	623.025900	11.346816
10.734528	609.586664	11.351834
11.099142	616.226258	11.356851
10.984468	622.785850	11.361869
10.902842	609.418487	11.366887
10.925036	621.608591	11.371904
10.990719	616.290521	11.376922
11.091483	611.131086	11.381939
11.069783	618.130619	11.386957
11.309108	609.446806	11.391975
11.035575	598.567605	11.396992
10.971690	597.599303	11.402010
10.697957	598.449787	11.407027
10.798347	600.024630	11.412045
11.104038	610.154108	11.417063
10.884559	619.844672	11.422080
11.056281	622.607570	11.427098
11.399321	620.241057	11.432115
10.939869	620.609238	11.437133
11.485924	624.317359	11.442151
11.021969	605.903634	11.447168
11.024798	591.418648	11.452186
10.919718	596.957454	11.457203
10.594093	614.171898	11.462221
10.966361	620.037160	11.467239
11.301605	620.650824	11.472256
11.142320	626.444222	11.477274
11.528957	619.176460	11.482291
11.126515	626.292077	11.487309
11.009061	618.960795	11.492327
11.463102	623.301756	11.497344
11.411014	629.517104	11.502362
11.248507	629.144801	11.507379
10.965799	631.486166	11.512397
11.017475	619.126794	11.517415
11.179248	619.556036	11.522432
10.964312	626.358449	11.527450
11.498476	622.002501	11.532467
11.503686	628.404579	11.537485
11.266883	631.915867	11.542503
11.307976	633.667196	11.547520
11.185018	627.725267	11.552538
11.449486	621.338026	11.557555
11.294536	625.515040	11.562573
11.497330	621.494696	11.567591
11.477271	626.707861	11.572608
11.137366	625.454342	11.577626
11.105322	630.912362	11.582643
11.113841	628.771494	11.587661
11.198219	634.583759	11.592679
11.115402	628.515664	11.597696
11.601694	626.707493	11.602714
11.197553	623.753596	11.607731
11.245639	626.696683	11.612749
11.172300	624.328729	11.617767
11.429431	625.989619	11.622784
11.419789	622.125422	11.627802
11.328347	615.137216	11.632819
11.395659	627.721070	11.637837
11.473560	633.875157	11.642855
11.636478	625.177988	11.647872
11.454630	631.423006	11.652890
11.793328	626.841880	11.657907
11.439688	629.759156	11.662925
11.395589	627.048991	11.667943
11.514437	635.740183	11.672960
11.430371	638.795362	11.677978
11.762386	639.242279	11.682995
11.752991	653.267619	11.688013
11.628225	647.307031	11.693031
11.817742	628.586420	11.698048
11.558694	623.792260	11.703066
11.729482	621.155932	11.708083
11.503385	624.416252	11.713101
11.429356	623.642025	11.718119
11.852503	631.847197	11.723136
11.689649	644.350139	11.728154
11.638432	633.862320	11.733171
11.778070	633.461908	11.738189
11.587749	630.790288	11.743207
11.545351	638.146487	11.748224
11.764369	647.847686	11.753242
11.596779	646.737744	11.758259
11.976636	645.337447	11.763277
12.016876	644.094165	11.768295
11.996323	640.676614	11.773312
11.623093	634.893566	11.778330
11.666860	630.658148	11.783347
11.387947	627.760489	11.788365
11.602320	642.262201	11.793383
12.180555	646.167281	11.798400
11.915119	641.535051	11.803418
12.164583	630.744808	11.808435
11.975925	631.585203	11.813453
11.546667	633.337184	11.818471
11.859192	631.511887	11.823488
11.970261	644.858927	11.828506
11.738328	639.057033	11.833523
11.740905	640.038061	11.838541
11.940076	639.416950	11.843559
12.206746	639.100898	11.848576
11.871254	650.608281	11.853594
11.953937	647.840506	11.858611
12.037746	643.033983	11.863629
12.053395	651.428837	11.868647
11.856340	647.477054	11.873664
11.931726	642.416232	11.878682
12.043521	634.433891	11.883699
12.100249	639.332159	11.888717
12.235885	633.469882	11.893735
11.912691	628.076661	11.898752
11.711982	639.553585	11.903770
11.706279	648.545031	11.908787
11.883578	645.712034	11.913805
11.827350	648.879641	11.918823
11.906247	647.056005	11.923840
11.519678	650.637949	11.928858
11.689034	647.661027	11.933875
12.410095	649.984962	11.938893
11.820785	643.093195	11.943911
12.237908	642.614867	11.948928
11.717982	645.725287	11.953946
12.001518	654.425559	11.958963
12.392486	667.997271	11.963981
12.426954	675.092218	11.968999
12.440193	664.581723	11.974016
12.316055	654.370322	11.979034
12.049157	648.602270	11.984051
12.247627	655.583316	11.989069
11.979668	661.339998	11.994087
12.146845	653.743487	11.999104
11.993984	669.132344	12.004122
12.070181	663.519144	12.009139
12.415756	653.947797	12.014157
12.361862	662.921508	12.019175
12.563694	664.887646	12.024192
12.416377	671.966716	12.029210
12.431855	664.671520	12.034227
12.206446	671.898443	12.039245
12.119833	671.069371	12.044263
12.466418	670.807145	12.049280
12.511892	672.775538	12.054298
12.370862	667.921967	12.059315
12.530317	670.639446	12.064333
12.127263	668.499541	12.069351
12.619066	668.072699	12.074368
12.446213	667.014066	12.079386
12.685027	668.333842	12.084403
12.744133	658.642999	12.089421
12.248093	659.720595	12.094439
12.424925	662.097709	12.099456
12.290139	672.541947	12.104474
12.018359	662.429266	12.109491
12.320461	669.482542	12.114509
12.130976	670.480852	12.119527
12.312243	669.117785	12.124544
12.197035	670.331740	12.129562
12.525043	668.320999	12.134579
12.340955	667.503948	12.139597
12.380867	682.733419	12.144615
12.839748	688.944968	12.149632
13.083028	682.400064	12.154650
12.815755	673.318587	12.159667
13.006822	664.967297	12.164685
12.530669	679.065330	12.169703
12.597390	657.350123	12.174720
12.293488	668.303509	12.179738
12.610725	664.325296	12.184755
12.910432	657.787394	12.189773
12.738641	668.070140	12.194791
12.900996	665.842203	12.199808
12.981505	671.058657	12.204826
12.678070	668.679187	12.209843
12.626650	670.564839	12.214861
12.781340	665.286544	12.219879
12.700137	663.683486	12.224896
12.690366	671.833009	12.229914
12.968720	662.900105	12.234931
12.851184	666.203489	12.239949
12.695559	658.688791	12.244967
12.832663	664.215156	12.249984
13.120150	670.147282	12.255002
12.556295	660.862688	12.260019
12.608529	662.350363	12.265037
12.818666	658.821155	12.270055
12.616497	674.072532	12.275072
12.705958	674.636106	12.280090
12.961618	685.013250	12.285107
12.856149	689.192041	12.290125
12.869182	696.621682	12.295143
13.024877	692.965249	12.300160
13.011304	684.137745	12.305178
13.059202	690.236564	12.310195
13.039336	693.139751	12.315213
12.916028	697.728407	12.320231
12.852588	689.880618	12.325248
13.112165	692.853902	12.330266
13.211499	695.473452	12.335283
12.985214	687.562659	12.340301
13.101007	691.678600	12.345319
13.293222	701.980428	12.350336
13.032599	689.215211	12.355354
12.955362	693.146619	12.360371
13.209421	682.573373	12.365389
12.950713	692.910689	12.370407
13.223177	691.697517	12.375424
13.483182	691.675981	12.380442
13.020969	688.794229	12.385459
13.022173	679.267019	12.390477
12.770072	682.805943	12.395495
13.018718	697.592688	12.400512
13.267902	697.623328	12.405530
13.340980	696.113007	12.410547
13.577510	681.695699	12.415565
13.433295	695.606369	12.420583
13.365227	696.374345	12.425600
13.163897	697.122046	12.430618
13.174060	697.253014	12.435635
13.366418	689.311752	12.440653
13.171894	698.891180	12.445671
13.306739	692.691348	12.450688
13.333480	691.513278	12.455706
13.236984	697.410527	12.460723
13.512907	687.569150	12.465741
13.289191	697.178368	12.470759
13.269226	691.943036	12.475776
13.578538	693.128765	12.480794
13.341765	691.445789	12.485811
13.042346	695.354988	12.490829
13.236686	692.642402	12.495847
13.122228	695.774904	12.500864
13.406915	700.041270	12.505882
13.091386	699.191035	12.510899
13.435648	694.602714	12.515917
13.586566	703.494066	12.520935
13.397990	697.114221	12.525952
13.399200	696.340900	12.530970
13.043981	701.981797	12.535987
13.484907	695.585991	12.541005
13.252877	705.363759	12.546023
13.282424	699.215031	12.551040
13.387225	706.504161	12.556058
13.703828	718.332923	12.561075
13.546661	710.480784	12.566093
13.700817	716.316924	12.571111
13.663790	715.281320	12.576128
13.820638	715.092815	12.581146
13.469035	725.684447	12.586163
13.705396	721.867131	12.591181
13.360525	725.193297	12.596199
13.514362	723.544172	12.601216
13.531084	729.152414	12.606234
13.351932	728.934174	12.611251
13.480922	714.779728	12.616269
13.308860	724.535547	12.621287
13.089034	721.874818	12.626304
13.759888	721.596817	12.631322
13.577108	724.787297	12.636339
13.508491	734.561728	12.641357
14.220016	744.643875	12.646375
13.875481	743.662459	12.651392
13.863893	736.636527	12.656410
13.742282	737.829394	12.661427
13.888855	742.587473	12.666445
14.057944	743.138652	12.671463
13.738011	733.995917	12.676480
13.903313	729.296599	12.681498
14.029972	749.514406	12.686515
13.868733	737.623589	12.691533
13.910725	727.320012	12.696551
13.763372	732.543560	12.701568
13.947260	738.551797	12.706586
13.939308	748.834326	12.711603
14.092648	744.761696	12.716621
14.101157	747.344904	12.721639
13.894906	744.252882	12.726656
14.143270	742.077814	12.731674
13.746671	745.405726	12.736691
14.114785	737.146754	12.741709
14.107658	742.787115	12.746727
14.013851	744.373272	12.751744
14.074665	740.245623	12.756762
14.112972	746.715173	12.761779
14.441249	742.678420	12.766797
13.940974	733.835154	12.771815
13.952130	747.582823	12.776832
14.229228	739.240194	12.781850
13.883896	744.983703	12.786867
13.958317	739.291864	12.791885
14.251018	742.708108	12.796903
14.056504	738.156326	12.801920
14.177044	746.673745	12.806938
14.172691	749.757556	12.811955
14.193426	740.927839	12.816973
14.439880	737.872627	12.821991
14.036184	747.055473	12.827008
14.456262	746.661887	12.832026
14.271861	753.948728	12.837043
14.240452	748.087176	12.842061
14.289655	739.180446	12.847079
14.258989	737.604225	12.852096
14.712514	740.856579	12.857114
14.346996	741.869678	12.862131
14.316885	738.541957	12.867149
14.291678	736.737676	12.872167
13.867515	748.808020	12.877184
14.197991	742.937462	12.882202
14.261464	739.475253	12.887219
14.462279	730.440783	12.892237
14.368028	739.969908	12.897255
14.412801	751.891506	12.902272
14.669212	746.663619	12.907290
14.264760	742.608410	12.912307
14.275399	742.856066	12.917325
14.522024	739.460012	12.922343
14.618471	735.030181	12.927360
14.800667	735.446779	12.932378
14.593817	741.673639	12.937395
14.531086	740.102411	12.942413
14.783175	740.527061	12.947431
14.400496	742.303357	12.952448
14.774175	739.376655	12.957466
14.394429	741.698430	12.962483
14.484518	743.571525	12.967501
14.531385	737.625208	12.972519
14.303393	744.454944	12.977536
14.666213	739.945770	12.982554
14.557334	755.217404	12.987571
14.785336	761.493327	12.992589
15.158884	757.121330	12.997607
14.762524	755.261228	13.002624
14.913844	741.977414	13.007642
14.586439	739.652158	13.012659
14.529987	737.066972	13.017677
14.829245	739.769006	13.022695
14.751665	741.819681	13.027712
14.937037	741.229116	13.032730
14.956397	732.797234	13.037747
14.717421	740.218795	13.042765
15.035348	742.135309	13.047783
14.679534	737.845318	13.052800
14.757936	728.893022	13.057818
14.978435	739.487104	13.062835
14.833661	738.484053	13.067853
15.120078	740.790469	13.072871
14.751204	749.368310	13.077888
14.793074	741.232712	13.082906
14.744693	753.285576	13.087923
14.826970	747.911237	13.092941
15.221831	754.135932	13.097959
15.221951	756.183978	13.102976
15.231665	750.372825	13.107994
15.040743	750.178508	13.113011
15.000721	744.444526	13.118029
15.218720	748.068056	13.123047
14.999195	733.260980	13.128064
15.066441	740.634863	13.133082
15.132868	746.869668	13.138099
14.962485	751.339438	13.143117
15.385569	750.923294	13.148135
14.945324	745.134865	13.153152
15.251475	744.954671	13.158170
15.038414	750.775415	13.163187
15.112975	751.003651	13.168205
15.134187	763.449617	13.173223
15.131467	758.779608	13.178240
15.548403	760.399851	13.183258
15.021000	765.619466	13.188275
15.471158	761.715207	13.193293
15.290274	756.407084	13.198311
15.156009	755.758991	13.203328
15.182040	763.483272	13.208346
15.305487	760.630240	13.213363
15.194998	759.669185	13.218381
15.250829	763.797635	13.223399
15.300927	763.786691	13.228416
15.159126	768.378243	13.233434
15.148858	756.574358	13.238451
15.359221	761.792710	13.243469
15.454533	751.297786	13.248487
15.088705	764.469867	13.253504
15.313241	763.570255	13.258522
15.465453	761.113519	13.263539
15.194632	769.168035	13.268557
15.292544	764.801082	13.273575
14.997336	753.442338	13.278592
15.231403	770.459340	13.283610
15.446542	780.874406	13.288627
15.486341	787.996970	13.293645
15.500151	778.694955	13.298663
15.536725	784.571514	13.303680
15.500101	785.078986	13.308698
15.925299	797.537814	13.313715
15.577207	788.487794	13.318733
15.649370	783.465303	13.323751
15.686157	792.122012	13.328768
15.742695	792.271007	13.333786
15.903339	782.570599	13.338803
15.570567	785.418380	13.343821
15.882072	786.499636	13.348839
15.552171	781.896340	13.353856
15.540878	781.118650	13.358874
15.818461	781.858059	13.363891
15.710499	793.585721	13.368909
15.736808	781.088179	13.373927
15.624832	785.025016	13.378944
15.642310	784.419566	13.383962
15.626584	780.111327	13.388979
15.829761	777.684522	13.393997
15.798252	774.375946	13.399015
15.466364	785.715602	13.404032
15.773689	776.134367	13.409050
15.538009	780.809965	13.414067
15.362644	783.914097	13.419085
15.888884	779.398404	13.424103
15.762206	790.936480	13.429120
15.887849	800.150543	13.434138
16.278021	800.582097	13.439155
16.119663	794.465749	13.444173
16.104971	785.310175	13.449191
15.759455	784.789643	13.454208
16.084473	781.719037	13.459226
16.054658	786.564549	13.464243
15.889017	798.007714	13.469261
16.203502	793.345111	13.474279
16.309791	796.594735	13.479296
15.985220	783.252444	13.484314
15.936183	786.996451	13.489331
15.838567	800.688515	13.494349
16.264046	804.036763	13.499367
16.484598	807.047699	13.504384
16.232053	800.990193	13.509402
16.047647	788.831557	13.514419
16.341705	805.144997	13.519437
16.175277	779.044787	13.524455
16.254546	784.820028	13.529472
16.149675	785.019399	13.534490
16.370428	785.063933	13.539507
16.141588	796.362307	13.544525
16.185493	799.975085	13.549543
16.516408	808.197855	13.554560
16.331772	804.405044	13.559578
16.331955	801.410255	13.564595
16.166714	804.787362	13.569613
16.239095	799.755365	13.574631
16.417158	809.510364	13.579648
16.043868	809.174031	13.584666
16.372174	808.078386	13.589683
16.097841	820.800773	13.594701
16.466283	806.552170	13.599719
16.161496	803.873099	13.604736
16.384569	806.331393	13.609754
16.492846	809.236737	13.614771
16.135626	808.610733	13.619789
16.243713	805.696970	13.624807
16.157343	811.005717	13.629824
16.701090	824.061470	13.634842
16.595368	818.482857	13.639859
16.218741	819.261011	13.644877
17.163756	820.458223	13.649895
16.800534	810.028345	13.654912
16.718337	807.204167	13.659930
16.600592	796.385793	13.664947
16.641804	805.811814	13.669965
16.555690	803.338531	13.674983
16.389525	807.921264	13.680000
16.977630	823.964884	13.685018
16.680545	814.856418	13.690035
16.843625	825.936004	13.695053
16.811407	809.509220	13.700071
16.756044	807.523440	13.705088
16.554627	816.987243	13.710106
17.062761	819.618900	13.715123
16.673586	820.910234	13.720141
16.797026	822.989578	13.725159
17.197257	824.252677	13.730176
17.117465	817.900032	13.735194
16.850871	804.883204	13.740211
16.717257	807.848299	13.745229
16.885841	802.788700	13.750247
16.827680	802.337033	13.755264
16.861200	820.521365	13.760282
17.020912	821.664125	13.765299
17.120830	830.601350	13.770317
16.837772	827.000579	13.775335
17.138345	826.865432	13.780352
17.308051	827.899342	13.785370
17.233562	807.092695	13.790387
16.629053	808.979272	13.795405
17.150008	812.047576	13.800423
17.388982	813.272666	13.805440
17.214787	803.346677	13.810458
16.976161	803.863510	13.815475
16.804954	813.827522	13.820493
17.199888	823.119586	13.825511
17.278821	825.505653	13.830528
17.333579	822.161547	13.835546
16.893065	793.816095	13.840563
16.968667	824.452633	13.845581
16.954912	823.470202	13.850599
17.250403	825.163007	13.855616
17.266562	837.884359	13.860634
17.201597	829.023760	13.865651
17.437944	843.411766	13.870669
17.369751	827.325072	13.875687
17.306446	832.674415	13.880704
17.207134	828.167746	13.885722
17.203733	831.699535	13.890739
17.386990	835.770293	13.895757
17.093190	836.765919	13.900775
17.370183	831.850375	13.905792
17.367840	835.830112	13.910810
17.616423	827.242580	13.915827
17.687537	836.288431	13.920845
17.374677	826.453444	13.925863
17.618573	829.164112	13.930880
17.416832	831.792690	13.935898
17.630054	828.518582	13.940915
17.710030	832.450789	13.945933
17.386415	838.355045	13.950951
17.312817	825.598479	13.955968
17.103065	832.920856	13.960986
17.517857	824.730313	13.966003
17.144444	824.207812	13.971021
17.180221	822.700132	13.976039
17.565737	845.487524	13.981056
17.535112	859.219694	13.986074
17.522375	848.719445	13.991091
17.516443	849.831194	13.996109
17.336825	852.888664	14.001127
17.766594	849.801737	14.006144
17.484847	860.461466	14.011162
17.744483	852.853630	14.016179
17.680454	862.643196	14.021197
17.860005	860.447271	14.026215
17.949235	849.719712	14.031232
17.750735	853.988764	14.036250
18.209496	852.342643	14.041267
17.989115	856.766577	14.046285
18.228012	862.636907	14.051303
18.323880	851.031023	14.056320
17.814423	853.262557	14.061338
17.743015	847.669125	14.066355
17.998466	852.921509	14.071373
17.881963	849.878610	14.076391
18.009107	853.314341	14.081408
18.074860	859.189538	14.086426
18.287006	855.716781	14.091443
18.182227	856.585152	14.096461
18.061363	857.774755	14.101479
18.156057	855.358518	14.106496
18.060886	860.738076	14.111514
18.144392	852.482339	14.116531
17.885201	859.285419	14.121549
17.679772	852.829249	14.126567
18.125896	852.516811	14.131584
17.991921	858.981667	14.136602
18.360285	855.797005	14.141619
18.107468	849.849974	14.146637
17.956457	848.917314	14.151655
18.320298	854.351633	14.156672
18.194237	852.468372	14.161690
18.291645	856.167502	14.166707
18.273841	856.227089	14.171725
18.044100	857.354750	14.176743
18.192658	854.942750	14.181760
18.056352	862.862759	14.186778
18.138634	862.824714	14.191795
17.971374	877.076776	14.196813
18.437783	881.725137	14.201831
18.538825	877.941479	14.206848
18.239756	875.791669	14.211866
18.329734	884.730468	14.216883
18.312954	879.750199	14.221901
18.331916	880.239552	14.226919
18.326990	883.399213	14.231936
18.074685	881.986873	14.236954
18.065837	874.824763	14.241971
18.475028	880.618094	14.246989
18.725313	890.219886	14.252007
19.015755	879.571432	14.257024
18.699917	876.114606	14.262042
18.671425	881.092479	14.267059
18.491424	873.584641	14.272077
18.520577	877.202887	14.277095
18.251954	869.951840	14.282112
18.520447	886.098925	14.287130
18.968478	892.236498	14.292147
18.969359	893.189403	14.297165
18.634036	886.807093	14.302183
19.213582	886.849412	14.307200
19.105706	883.009920	14.312218
18.980095	878.087621	14.317235
18.898496	873.638140	14.322253
18.533618	873.354144	14.327271
18.791122	872.578779	14.332288
18.576973	870.093864	14.337306
18.413610	878.046493	14.342323
18.940419	888.441498	14.347341
18.345438	901.614644	14.352359
18.739309	899.145510	14.357376
18.533461	907.420340	14.362394
18.599866	895.961022	14.367411
19.321584	899.588205	14.372429
19.090692	909.855046	14.377447
19.440903	902.154195	14.382464
18.973446	901.605308	14.387482
19.217210	905.654039	14.392499
18.925248	902.111441	14.397517
19.068390	908.608907	14.402535
19.400484	899.733789	14.407552
19.121953	900.752288	14.412570
19.249420	899.268194	14.417587
19.111615	891.375092	14.422605
19.201274	899.670180	14.427623
19.212591	893.003529	14.432640
19.099022	890.502951	14.437658
19.202809	897.476744	14.442675
18.999745	896.763619	14.447693
18.983801	898.448117	14.452711
19.273687	893.830343	14.457728
19.285411	895.968114	14.462746
19.172368	894.127001	14.467763
19.246099	909.054762	14.472781
19.426360	918.695873	14.477799
19.403203	915.780436	14.482816
19.293842	917.261735	14.487834
19.386985	925.859244	14.492851
19.810302	922.217899	14.497869
19.695780	913.926695	14.502887
19.314305	903.228211	14.507904
19.339911	898.765189	14.512922
19.733095	909.430313	14.517939
19.317035	901.637333	14.522957
19.690289	920.100223	14.527975
19.825834	909.942916	14.532992
19.197142	899.472269	14.538010
19.595961	910.625655	14.543027
19.726612	908.333198	14.548045
19.560993	922.291557	14.553063
19.987491	922.121025	14.558080
19.741056	915.592324	14.563098
19.374052	910.578214	14.568115
19.687840	908.818964	14.573133
19.741005	924.052890	14.578151
19.608551	921.485822	14.583168
19.645004	931.881460	14.588186
19.828864	930.262355	14.593203
20.144920	919.906528	14.598221
20.009957	924.923081	14.603239
19.975049	933.755120	14.608256
19.902568	924.106710	14.613274
20.227419	925.444667	14.618291
19.759204	909.095141	14.623309
19.771894	911.011862	14.628327
20.034530	911.946104	14.633344
19.822026	917.283988	14.638362
19.942289	919.736215	14.643379
20.134137	917.746646	14.648397
19.978724	936.945102	14.653415
19.794647	925.401690	14.658432
20.226807	921.604338	14.663450
19.936019	915.069920	14.668467
20.264073	920.263684	14.673485
20.322860	924.467448	14.678503
20.133929	925.623473	14.683520
20.147045	918.139197	14.688538
19.818572	932.252304	14.693555
20.192091	927.529983	14.698573
20.067770	922.806282	14.703591
19.807867	925.683765	14.708608
19.673567	918.045719	14.713626
19.825466	924.557606	14.718643
20.148106	928.395250	14.723661
20.238173	944.425004	14.728679
19.993251	942.992575	14.733696
20.355728	945.817340	14.738714
20.401082	950.594390	14.743731
20.344266	946.169435	14.748749
20.209637	950.731516	14.753767
20.177518	945.434887	14.758784
20.479042	941.484305	14.763802
20.166588	941.943210	14.768819
20.363427	949.637823	14.773837
20.554364	944.126588	14.778855
20.518565	941.913690	14.783872
20.744749	943.503691	14.788890
20.406259	948.365749	14.793907
20.907936	951.105727	14.798925
20.441179	948.937836	14.803943
20.262778	946.134926	14.808960
20.429271	942.271638	14.813978
20.206366	945.111806	14.818995
20.691120	956.046718	14.824013
20.767460	969.393097	14.829031
20.414733	981.566083	14.834048
20.745413	973.600003	14.839066
20.904260	980.113984	14.844083
21.264166	964.143548	14.849101
21.148058	954.107447	14.854119
20.963538	942.592494	14.859136
20.950508	938.021871	14.864154
20.813168	939.668471	14.869171
20.823530	940.256992	14.874189
20.883154	950.696370	14.879207
20.745461	948.773885	14.884224
21.101546	941.513905	14.889242
20.469121	946.838285	14.894259
20.969413	941.020115	14.899277
21.358278	950.070199	14.904295
20.801633	949.828681	14.909312
21.261118	941.618504	14.914330
20.731339	940.230426	14.919347
21.056852	944.096027	14.924365
21.428750	948.604490	14.929383
21.234791	940.578100	14.934400
21.115238	940.423160	14.939418
20.888416	945.539225	14.944435
21.031774	950.752287	14.949453
21.420159	962.046183	14.954471
21.202562	968.804960	14.959488
21.262774	962.035997	14.964506
21.162601	965.018002	14.969523
21.502535	968.259683	14.974541
21.314439	958.338927	14.979559
20.777837	948.365142	14.984576
20.922389	955.253718	14.989594
20.987794	961.397240	14.994611
21.261007	958.495613	14.999629
21.002164	956.898096	15.004647
21.023455	968.119764	15.009664
21.223011	953.922584	15.014682
21.423496	969.291399	15.019699
21.379228	973.113596	15.024717
21.312282	984.030283	15.029735
21.448351	983.942838	15.034752
21.952802	988.837764	15.039770
21.427636	985.486091	15.044787
21.835162	983.510271	15.049805
21.655506	989.199662	15.054823
21.608618	983.728599	15.059840
21.929805	983.422988	15.064858
21.260401	981.898859	15.069875
21.432723	979.631462	15.074893
21.818840	981.354352	15.079911
21.508179	995.322728	15.084928
22.155460	983.681397	15.089946
21.795013	991.194556	15.094963
21.663455	981.703633	15.099981
21.662298	988.870523	15.104999
21.593613	988.729753	15.110016
22.255842	985.240543	15.115034
21.959875	985.210898	15.120051
21.873447	981.222881	15.125069
21.802101	981.060435	15.130087
21.921721	992.282589	15.135104
22.111618	984.152234	15.140122
21.719454	983.064613	15.145139
21.873040	989.626753	15.150157
21.826153	985.222332	15.155175
21.590441	983.532850	15.160192
22.102461	981.196785	15.165210
21.742602	978.987001	15.170227
21.812928	985.764070	15.175245
21.887035	988.614805	15.180263
21.836459	1000.138012	15.185280
22.339268	1000.621462	15.190298
22.216321	1016.659201	15.195315
21.935908	1011.385432	15.200333
22.511982	1010.055542	15.205351
22.256564	1012.935496	15.210368
22.471238	999.499617	15.215386
22.340847	1003.919043	15.220403
22.573797	994.118902	15.225421
22.527181	976.987318	15.230439
22.162783	985.990601	15.235456
22.211378	981.293609	15.240474
21.944956	979.675180	15.245491
21.685432	996.324289	15.250509
22.156324	1004.850398	15.255527
22.230519	1006.883784	15.260544
22.429985	992.014413	15.265562
22.442077	1001.754334	15.270579
22.284277	1001.567479	15.275597
22.518249	995.494117	15.280615
22.267674	1006.000759	15.285632
22.701219	1001.796083	15.290650
22.433444	1013.570862	15.295667
22.736006	1015.887424	15.300685
23.080439	1018.686608	15.305703
22.556268	1010.348688	15.310720
23.082668	1006.192669	15.315738
22.852874	1002.924389	15.320755
22.556039	1002.490943	15.325773
22.806401	1001.047666	15.330791
22.673082	1007.689196	15.335808
23.029219	1002.896980	15.340826
22.781310	1001.872102	15.345843
22.817618	1006.360247	15.350861
22.999577	994.226479	15.355879
22.914091	1003.104296	15.360896
22.886978	1005.109274	15.365914
22.572612	1001.260881	15.370931
23.007752	1009.685264	15.375949
23.217116	1007.513081	15.380967
22.866463	1003.345295	15.385984
23.050736	1001.334807	15.391002
23.077821	1006.524964	15.396019
22.890669	1006.257474	15.401037
23.282630	1016.818713	15.406055
23.239193	1021.972519	15.411072
23.367511	1024.991541	15.416090
23.307866	1006.129450	15.421107
23.114179	1004.821580	15.426125
23.042121	1000.096032	15.431143
23.387488	1000.815430	15.436160
23.287368	997.063067	15.441178
23.192421	1001.562179	15.446195
22.749773	1003.963207	15.451213
23.438065	1011.628666	15.456231
23.447773	1026.351902	15.461248
23.559522	1022.534989	15.466266
23.320224	1028.656549	15.471283
23.377567	1026.343933	15.476301
23.479208	1021.581869	15.481319
23.613987	1024.719804	15.486336
23.525912	1025.948493	15.491354
23.660852	1033.466590	15.496371
23.345924	1022.189637	15.501389
23.661644	1019.997737	15.506407
23.367485	1026.607512	15.511424
23.291783	1026.177505	15.516442
23.604204	1022.247299	15.521459
23.564251	1027.059742	15.526477
23.785083	1018.839350	15.531495
23.555445	1025.091947	15.536512
23.612500	1026.989150	15.541530
23.010975	1020.089669	15.546547
23.304606	1030.224421	15.551565
23.504355	1027.829674	15.556583
23.444610	1022.420560	15.561600
23.419166	1030.064611	15.566618
23.371944	1048.558388	15.571635
23.719024	1052.692050	15.576653
24.029479	1049.276533	15.581671
23.709721	1051.718393	15.586688
23.750416	1054.700571	15.591706
24.004520	1050.905668	15.596723
23.892112	1059.544712	15.601741
24.239542	1052.077755	15.606759
24.107004	1059.508122	15.611776
24.060396	1055.397125	15.616794
24.024218	1047.314564	15.621811
23.891408	1051.226302	15.626829
23.827764	1052.331270	15.631847
23.733473	1060.434171	15.636864
23.822372	1059.568286	15.641882
23.875685	1044.794209	15.646899
24.067772	1064.352102	15.651917
24.422283	1072.438779	15.656935
24.075332	1081.597182	15.661952
24.446064	1076.692221	15.666970
24.884220	1072.467877	15.671987
24.503033	1063.309262	15.677005
24.531385	1047.797465	15.682023
24.108484	1049.816734	15.687040
24.364119	1048.732389	15.692058
24.385717	1052.285576	15.697075
24.606036	1045.949239	15.702093
24.615832	1039.118670	15.707111
24.479833	1050.689923	15.712128
24.264755	1053.257495	15.717146
24.276143	1045.167529	15.722163
24.208749	1050.779501	15.727181
25.028182	1057.392629	15.732199
24.745049	1056.054501	15.737216
24.276909	1056.846913	15.742234
24.589336	1059.319732	15.747251
24.725157	1074.910142	15.752269
24.823306	1071.148984	15.757287
24.780083	1070.956912	15.762304
24.846101	1063.480117	15.767322
24.761137	1068.107078	15.772339
24.649134	1077.430867	15.777357
24.748154	1072.782804	15.782375
24.568532	1071.131917	15.787392
24.839122	1079.042318	15.792410
25.131075	1077.576781	15.797427
25.024053	1067.532889	15.802445
25.193031	1064.265627	15.807463
25.187645	1069.202085	15.812480
24.876644	1051.562491	15.817498
25.178007	1049.445405	15.822515
24.910119	1052.459849	15.827533
25.092320	1055.025525	15.832551
25.377838	1063.009333	15.837568
25.346594	1042.066291	15.842586
25.174336	1036.160303	15.847603
24.800572	1037.805853	15.852621
25.035792	1036.084069	15.857639
25.433297	1046.896924	15.862656
25.099852	1045.926387	15.867674
25.245789	1046.629501	15.872691
25.257521	1047.470273	15.877709
24.990654	1040.534458	15.882727
25.213700	1054.609130	15.887744
25.663358	1062.655743	15.892762
25.677306	1049.872762	15.897779
25.140151	1046.538722	15.902797
25.330737	1041.096939	15.907815
25.147313	1056.241584	15.912832
25.367530	1058.018714	15.917850
25.380317	1045.848135	15.922867
25.139929	1056.280637	15.927885
25.049669	1059.955382	15.932903
25.264777	1050.789139	15.937920
25.038975	1070.099681	15.942938
25.195477	1053.094188	15.947955
25.132161	1074.916666	15.952973
25.663232	1078.961729	15.957991
25.731779	1086.095715	15.963008
25.834865	1080.582337	15.968026
25.795888	1083.655819	15.973043
25.608476	1091.170481	15.978061
25.753587	1086.685649	15.983079
25.719691	1083.017630	15.988096
25.507168	1085.815179	15.993114
25.900553	1082.853797	15.998131
25.775150	1082.851243	16.003149
25.765028	1083.578656	16.008167
25.916662	1082.507345	16.013184
25.774674	1083.823326	16.018202
25.603672	1089.299966	16.023219
25.738487	1077.833035	16.028237
25.609044	1083.773411	16.033255
25.668704	1095.424681	16.038272
25.875456	1102.758060	16.043290
26.187842	1104.678633	16.048307
26.163087	1104.316430	16.053325
26.264936	1105.127395	16.058343
26.362680	1101.962733	16.063360
26.201537	1098.194604	16.068378
26.279260	1099.801422	16.073395
26.459504	1102.648273	16.078413
26.333151	1097.063318	16.083431
26.337012	1101.676457	16.088448
26.012322	1100.079712	16.093466
26.439768	1097.614790	16.098483
26.595865	1099.591254	16.103501
26.362537	1097.185031	16.108519
26.465382	1099.636839	16.113536
26.365260	1088.831322	16.118554
26.417246	1096.166703	16.123571
26.661331	1094.888497	16.128589
26.240618	1099.577207	16.133607
26.795619	1107.711579	16.138624
26.338920	1108.486433	16.143642
26.285307	1103.849503	16.148659
26.382967	1090.592719	16.153677
26.336970	1099.581199	16.158695
26.818447	1089.953746	16.163712
26.791205	1100.337310	16.168730
26.769370	1099.693790	16.173747
26.756283	1097.802380	16.178765
26.585408	1098.747323	16.183783
26.585684	1101.764204	16.188800
26.208726	1115.351681	16.193818
26.820908	1114.511617	16.198835
26.975564	1124.926834	16.203853
26.611210	1128.480168	16.208871
26.767084	1127.269341	16.213888
27.018305	1127.965533	16.218906
27.277770	1124.359127	16.223923
27.166266	1117.291797	16.228941
26.930792	1126.016304	16.233959
27.466560	1117.257689	16.238976
27.388208	1124.474521	16.243994
27.388670	1124.556511	16.249011
27.278254	1113.815697	16.254029
26.926478	1102.901031	16.259047
27.080556	1098.440047	16.264064
27.113411	1124.586791	16.269082
27.161597	1121.350948	16.274099
27.104187	1125.591786	16.279117
26.974244	1116.068982	16.284135
27.362234	1116.848020	16.289152
27.227582	1119.308406	16.294170
27.518559	1119.373565	16.299187
27.425999	1119.949715	16.304205
26.954052	1119.792836	16.309223
27.484775	1121.979214	16.314240
27.018348	1120.186787	16.319258
26.995710	1116.447581	16.324275
27.221571	1125.538913	16.329293
27.530101	1139.237428	16.334311
28.058218	1134.453114	16.339328
27.441589	1140.630305	16.344346
27.380584	1146.929272	16.349363
27.760616	1144.386520	16.354381
27.612269	1144.952422	16.359399
27.748983	1144.653440	16.364416
27.708867	1144.230512	16.369434
27.760241	1151.509208	16.374451
27.823271	1144.023377	16.379469
27.683017	1155.551179	16.384487
27.866601	1148.087602	16.389504
28.057298	1147.559311	16.394522
28.121929	1142.859780	16.399539
28.457236	1140.415510	16.404557
28.096062	1155.133482	16.409575
28.008148	1135.300520	16.414592
27.978115	1134.165974	16.419610
27.886352	1138.705650	16.424627
28.082475	1144.642693	16.429645
28.130215	1147.002102	16.434663
27.991035	1139.920137	16.439680
28.122015	1150.875537	16.444698
28.068102	1138.715280	16.449715
28.125576	1136.573041	16.454733
27.677315	1143.336239	16.459751
28.230709	1140.157432	16.464768
28.194943	1144.716793	16.469786
28.104948	1142.515464	16.474803
28.315368	1141.447620	16.479821
28.124702	1142.638642	16.484839
27.864703	1137.563627	16.489856
27.733954	1145.044243	16.494874
28.443626	1163.000576	16.499891
28.541277	1163.231534	16.504909
28.851096	1165.376574	16.509927
29.032889	1158.717994	16.514944
28.283357	1165.625936	16.519962
28.714019	1160.799984	16.524979
28.941830	1157.873835	16.529997
28.765733	1157.715074	16.535015
28.810544	1155.672633	16.540032
28.871556	1153.936936	16.545050
28.646170	1144.403731	16.550067
28.551334	1148.890240	16.555085
28.678514	1164.239079	16.560103
28.899539	1158.852481	16.565120
28.881970	1161.433497	16.570138
28.923554	1157.722153	16.575155
29.117035	1150.559988	16.580173
29.043474	1146.484725	16.585191
28.785126	1137.035550	16.590208
28.435333	1143.953829	16.595226
28.809541	1150.071428	16.600243
29.009486	1157.342773	16.605261
28.830380	1161.066085	16.610279
29.033772	1151.396690	16.615296
29.142215	1153.986488	16.620314
29.181196	1155.267987	16.625331
29.048395	1153.382587	16.630349
28.954371	1166.291740	16.635367
28.767157	1158.226333	16.640384
28.861332	1163.484984	16.645402
28.768106	1164.108576	16.650419
29.190114	1168.685032	16.655437
29.288429	1184.477035	16.660455
29.477238	1173.405576	16.665472
29.344213	1178.380873	16.670490
29.405981	1179.835549	16.675507
29.473471	1182.886160	16.680525
29.695610	1185.745436	16.685543
29.730021	1183.341697	16.690560
29.525549	1181.145563	16.695578
29.021901	1181.318664	16.700595
29.704602	1178.836080	16.705613
29.460588	1175.989701	16.710631
29.634568	1165.289782	16.715648
29.518369	1181.932529	16.720666
29.645255	1177.778713	16.725683
29.632230	1165.072433	16.730701
29.476405	1169.473769	16.735719
29.888513	1174.613497	16.740736
29.743612	1175.122059	16.745754
29.987321	1179.095122	16.750771
30.533483	1179.063747	16.755789
29.816176	1181.365551	16.760807
30.119528	1175.713668	16.765824
29.598643	1176.154537	16.770842
29.792558	1176.676619	16.775859
29.888480	1168.822741	16.780877
29.399895	1186.110445	16.785895
29.746537	1200.977025	16.790912
30.064876	1206.393291	16.795930
30.028443	1203.094869	16.800947
29.951029	1193.257734	16.805965
30.028791	1202.056585	16.810983
30.133952	1200.736885	16.816000
30.378647	1196.750914	16.821018
29.986262	1200.346495	16.826035
30.177663	1195.636680	16.831053
29.984347	1199.346433	16.836071
29.993038	1214.391873	16.841088
30.454764	1219.059988	16.846106
30.550532	1227.975968	16.851123
30.487918	1224.022058	16.856141
30.598731	1230.852878	16.861159
30.810518	1224.918591	16.866176
30.775038	1217.788891	16.871194
30.534276	1232.163133	16.876211
30.710450	1213.232548	16.881229
30.697979	1223.787452	16.886247
30.753409	1215.258209	16.891264
30.704784	1203.207536	16.896282
30.648341	1201.023066	16.901299
30.857073	1206.330166	16.906317
30.777929	1215.342800	16.911335
30.994453	1209.556103	16.916352
30.987408	1205.199073	16.921370
30.630029	1201.414137	16.926387
30.685746	1199.792868	16.931405
30.566162	1211.232283	16.936423
30.563431	1223.685453	16.941440
31.110968	1216.632238	16.946458
31.057860	1221.885437	16.951475
30.970700	1219.140861	16.956493
31.145804	1216.885624	16.961511
31.196804	1222.561268	16.966528
31.224189	1219.032001	16.971546
31.084227	1222.916488	16.976563
31.025600	1219.754061	16.981581
30.977781	1216.138675	16.986599
30.889512	1214.328385	16.991616
31.060725	1221.566361	16.996634
30.904138	1223.212827	17.001651
31.386988	1230.528517	17.006669
31.393096	1241.336158	17.011687
31.426881	1237.834294	17.016704
31.653645	1241.923618	17.021722
31.557030	1247.398191	17.026739
31.608172	1231.201035	17.031757
31.755020	1239.070814	17.036775
31.958530	1239.859645	17.041792
31.832266	1223.828972	17.046810
31.522134	1220.033521	17.051827
31.586752	1209.161256	17.056845
31.451285	1203.413585	17.061863
31.339382	1217.019831	17.066880
31.894932	1229.644859	17.071898
32.084593	1236.971486	17.076915
32.015851	1230.736893	17.081933
32.090343	1232.183281	17.086951
31.505388	1222.444087	17.091968
31.555561	1227.637025	17.096986
31.829229	1233.688257	17.102003
32.086976	1234.386593	17.107021
32.029941	1231.886632	17.112039
31.919298	1241.475382	17.117056
32.173680	1242.704415	17.122074
31.917750	1233.541990	17.127091
32.476421	1233.729573	17.132109
32.179015	1228.209077	17.137127
32.102246	1239.310485	17.142144
32.381387	1230.784274	17.147162
32.184789	1226.942742	17.152179
32.108123	1225.869099	17.157197
32.546885	1232.437421	17.162215
32.293666	1230.892652	17.167232
32.389764	1226.109305	17.172250
32.333920	1238.756947	17.177267
32.259087	1235.085803	17.182285
32.242974	1234.968403	17.187303
31.858433	1233.128501	17.192320
32.433741	1228.901700	17.197338
32.344239	1250.719004	17.202355
32.701084	1246.257971	17.207373
32.477463	1255.419351	17.212391
32.600597	1260.269581	17.217408
32.483856	1247.636195	17.222426
32.616698	1249.742527	17.227443
32.660933	1253.131285	17.232461
32.997943	1258.626710	17.237479
32.892092	1257.134733	17.242496
32.843379	1254.024405	17.247514
32.704434	1256.725318	17.252531
32.753106	1251.453889	17.257549
32.619058	1261.677452	17.262567
32.575227	1261.842078	17.267584
32.894660	1254.821207	17.272602
32.714647	1247.095463	17.277619
32.871366	1252.114030	17.282637
33.235114	1266.129094	17.287655
33.197570	1278.944328	17.292672
33.366807	1271.539737	17.297690
32.886730	1272.435002	17.302707
33.418474	1269.619304	17.307725
33.604156	1282.339826	17.312743
33.296327	1265.810365	17.317760
33.155736	1252.136120	17.322778
33.309254	1271.466717	17.327795
33.307324	1274.834264	17.332813
33.331156	1282.259313	17.337831
33.088070	1277.973729	17.342848
33.389980	1278.851383	17.347866
33.431546	1281.164434	17.352883
33.714977	1272.612288	17.357901
33.652534	1275.156127	17.362919
33.162993	1275.525847	17.367936
33.860141	1276.244135	17.372954
33.592873	1276.497197	17.377971
33.252453	1275.767573	17.382989
33.466910	1275.402836	17.388007
33.266329	1275.036446	17.393024
33.503498	1286.966317	17.398042
33.941796	1299.600183	17.403059
33.784432	1300.874393	17.408077
33.929398	1302.464449	17.413095
33.687858	1305.345444	17.418112
34.114799	1304.780367	17.423130
34.083411	1306.353699	17.428147
34.095949	1299.812938	17.433165
34.403039	1306.793107	17.438183
34.225811	1297.984468	17.443200
34.346410	1294.866707	17.448218
34.020202	1295.210997	17.453235
33.830478	1290.017699	17.458253
34.073060	1295.183856	17.463271
33.992450	1297.291869	17.468288
34.193249	1297.951738	17.473306
34.219353	1308.529089	17.478323
33.842097	1295.532286	17.483341
34.140776	1301.163081	17.488359
34.336687	1319.294237	17.493376
34.322411	1322.771012	17.498394
34.635990	1325.966369	17.503411
35.053595	1323.982632	17.508429
35.102688	1314.236187	17.513447
34.825495	1317.447784	17.518464
34.698416	1297.270445	17.523482
34.307447	1298.871359	17.528499
34.454363	1312.380576	17.533517
34.741325	1314.728009	17.538535
34.706134	1320.057341	17.543552
34.704030	1314.582360	17.548570
35.084965	1316.889915	17.553587
34.957964	1321.567668	17.558605
35.250608	1317.252313	17.563623
34.985348	1325.031658	17.568640
35.150574	1312.824539	17.573658
35.092197	1308.090467	17.578675
34.963433	1315.226864	17.583693
35.021627	1312.929857	17.588711
35.038770	1311.715371	17.593728
35.493980	1317.252372	17.598746
35.466981	1315.391507	17.603763
35.224231	1307.650259	17.608781
35.212125	1297.380021	17.613799
35.163537	1306.630940	17.618816
35.376110	1303.625090	17.623834
35.420759	1309.393268	17.628851
34.930460	1312.123647	17.633869
35.427773	1314.050165	17.638887
35.365145	1322.520639	17.643904
35.771248	1307.202267	17.648922
35.707513	1312.756948	17.653939
35.494450	1313.834703	17.658957
35.491867	1321.074532	17.663975
35.363848	1322.656599	17.668992
35.307442	1314.195214	17.674010
35.483554	1312.069196	17.679027
35.239483	1311.031080	17.684045
35.638403	1310.719673	17.689063
35.653130	1319.468436	17.694080
35.415897	1330.620131	17.699098
35.708325	1340.849923	17.704115
35.388552	1338.365607	17.709133
36.186305	1334.564897	17.714151
35.785166	1335.763455	17.719168
35.924002	1335.719759	17.724186
35.896139	1330.457067	17.729203
35.915921	1335.721041	17.734221
35.832855	1327.134412	17.739239
35.890525	1331.871778	17.744256
36.428448	1340.444418	17.749274
36.158844	1336.172416	17.754291
35.726608	1341.203811	17.759309
36.097008	1351.544545	17.764327
36.084432	1350.552434	17.769344
36.023387	1359.063705	17.774362
36.327951	1353.787118	17.779379
36.339949	1353.457058	17.784397
36.636397	1349.661811	17.789415
36.693673	1349.630815	17.794432
36.550925	1346.891718	17.799450
36.637227	1355.291683	17.804467
36.761331	1357.352052	17.809485
36.917166	1348.538868	17.814503
36.909802	1354.438236	17.819520
36.930349	1348.767213	17.824538
36.971342	1351.585292	17.829555
36.789099	1350.878375	17.834573
36.900414	1352.221209	17.839591
36.664430	1350.825225	17.844608
37.002985	1345.335065	17.849626
36.961192	1357.671335	17.854643
36.721948	1349.967391	17.859661
36.904486	1349.102693	17.864679
36.903191	1349.061881	17.869696
36.737515	1350.495179	17.874714
37.085090	1343.425710	17.879731
37.003127	1353.155221	17.884749
37.338241	1366.947604	17.889767
37.334183	1368.800710	17.894784
37.272130	1360.087717	17.899802
37.405086	1355.131339	17.904819
36.943704	1366.074957	17.909837
37.461185	1365.300121	17.914855
37.516829	1373.663843	17.919872
37.405108	1376.209056	17.924890
37.560822	1374.266089	17.929907
37.744827	1378.377881	17.934925
37.338435	1388.151611	17.939943
37.614989	1383.103440	17.944960
37.269584	1380.572616	17.949978
37.698633	1378.372496	17.954995
37.382317	1386.071454	17.960013
37.466344	1378.285609	17.965031
37.484970	1374.959648	17.970048
37.738482	1373.241296	17.975066
37.679812	1374.007837	17.980083
37.458104	1375.269980	17.985101
37.507922	1377.755328	17.990119
37.684916	1391.613374	17.995136
37.974609	1389.788401	18.000154
38.447980	1396.644887	18.005171
38.150039	1403.504700	18.010189
38.376530	1396.185818	18.015207
38.396326	1388.381566	18.020224
38.131396	1394.851227	18.025242
38.381444	1384.454915	18.030259
38.158461	1382.921204	18.035277
38.170255	1387.059810	18.040295
38.205696	1390.935959	18.045312
38.498502	1390.584268	18.050330
38.586654	1388.658129	18.055347
38.188819	1399.058541	18.060365
38.247077	1391.933112	18.065383
38.464959	1394.348115	18.070400
38.144022	1392.047011	18.075418
38.423078	1387.983064	18.080435
38.183348	1389.371090	18.085453
38.244211	1383.876817	18.090471
38.338870	1389.245913	18.095488
38.396990	1410.188358	18.100506
39.261464	1407.649040	18.105523
38.604288	1415.751377	18.110541
38.591173	1415.835482	18.115559
38.688841	1409.843162	18.120576
38.624947	1415.072849	18.125594
38.946280	1417.525398	18.130611
38.582100	1409.354884	18.135629
38.665998	1412.090553	18.140647
39.130089	1425.323255	18.145664
38.967008	1428.188899	18.150682
39.583822	1429.497217	18.155699
39.072488	1434.941743	18.160717
39.408100	1436.202325	18.165735
39.667458	1437.332767	18.170752
39.423570	1421.594786	18.175770
39.553079	1405.792371	18.180787
38.940687	1408.980433	18.185805
39.313854	1419.358646	18.190823
39.329492	1422.010269	18.195840
39.303044	1423.535506	18.200858
39.999412	1416.452729	18.205875
39.611918	1431.389622	18.210893
39.690199	1432.747073	18.215911
39.676507	1433.131071	18.220928
39.488360	1432.254655	18.225946
39.838502	1429.041171	18.230963
39.800062	1434.882287	18.235981
39.578931	1422.798364	18.240999
39.921330	1421.602658	18.246016
39.892767	1429.496675	18.251034
39.655688	1423.868895	18.256051
39.904925	1417.237589	18.261069
39.841481	1413.015522	18.266087
40.071171	1427.947838	18.271104
39.721487	1419.427922	18.276122
40.207147	1413.899059	18.281139
39.912524	1416.469599	18.286157
40.045599	1417.695441	18.291175
40.304283	1415.685944	18.296192
40.439582	1416.737870	18.301210
40.564280	1410.772899	18.306227
40.205539	1416.518711	18.311245
40.106993	1419.434267	18.316263
40.547024	1426.494772	18.321280
40.477699	1425.909126	18.326298
40.571168	1422.117065	18.331315
40.557025	1425.969383	18.336333
40.537107	1429.825757	18.341351
40.910027	1431.938914	18.346368
40.720288	1426.975953	18.351386
40.710756	1416.260275	18.356403
40.710364	1416.979875	18.361421
40.684634	1426.262011	18.366439
41.027152	1432.741251	18.371456
40.409611	1438.095015	18.376474
40.718229	1439.047373	18.381491
40.780059	1445.302074	18.386509
40.862315	1441.915700	18.391527
41.099665	1440.676388	18.396544
40.761237	1447.479404	18.401562
41.199974	1440.670261	18.406579
40.990418	1442.419669	18.411597
40.869169	1436.653929	18.416615
41.235042	1431.484540	18.421632
41.294383	1446.351876	18.426650
41.178090	1433.238602	18.431667
41.246165	1445.816604	18.436685
41.556140	1455.601914	18.441703
41.507412	1449.095883	18.446720
41.311263	1461.014441	18.451738
41.603672	1455.692379	18.456755
41.528297	1465.711262	18.461773
41.380502	1451.681377	18.466791
41.477500	1451.306522	18.471808
41.690227	1455.704196	18.476826
41.721664	1459.678814	18.481843
41.959133	1460.768484	18.486861
42.213141	1467.261517	18.491879
41.978878	1453.431287	18.496896
41.929069	1460.631188	18.501914
41.800431	1451.685518	18.506931
41.950044	1457.462648	18.511949
41.807739	1466.870254	18.516967
42.033517	1458.421671	18.521984
41.844939	1462.891295	18.527002
41.774368	1460.948836	18.532019
41.770531	1453.381767	18.537037
41.664229	1456.200705	18.542055
42.033460	1471.897134	18.547072
41.975299	1480.408013	18.552090
42.023864	1481.126305	18.557107
42.267480	1481.467087	18.562125
42.226796	1496.498362	18.567143
42.356051	1483.346821	18.572160
42.462859	1485.160587	18.577178
42.176755	1490.352309	18.582195
42.281188	1488.578261	18.587213
42.367553	1504.340851	18.592231
42.390112	1507.685693	18.597248
42.723261	1504.692595	18.602266
42.419366	1504.847220	18.607283
42.992082	1501.592758	18.612301
42.566690	1509.580153	18.617319
42.828718	1505.379974	18.622336
42.785068	1504.323265	18.627354
42.946209	1504.790498	18.632371
43.130741	1504.865922	18.637389
42.777761	1506.132732	18.642407
43.020155	1502.077624	18.647424
42.990794	1510.284229	18.652442
42.842811	1504.323812	18.657459
43.586924	1507.385898	18.662477
43.082239	1518.964363	18.667495
43.516722	1506.992904	18.672512
43.041899	1507.590712	18.677530
43.084748	1509.051517	18.682547
43.391446	1518.341905	18.687565
43.355408	1522.371224	18.692583
43.540552	1524.002382	18.697600
43.182090	1522.764310	18.702618
43.305100	1524.455635	18.707635
43.791865	1530.631582	18.712653
43.783793	1524.049765	18.717671
43.756523	1520.377468	18.722688
43.812878	1529.460684	18.727706
43.855904	1518.594748	18.732723
44.208429	1515.548137	18.737741
44.124494	1518.953745	18.742759
44.077056	1515.426602	18.747776
43.970142	1522.032653	18.752794
44.247381	1511.572074	18.757811
44.286732	1515.753757	18.762829
44.486716	1524.050895	18.767847
44.007584	1520.221730	18.772864
44.314301	1522.850140	18.777882
44.046516	1523.466207	18.782899
44.157049	1519.327482	18.787917
44.215855	1520.088363	18.792935
44.242831	1511.607590	18.797952
44.143904	1515.924413	18.802970
43.948778	1521.300797	18.807987
44.572385	1517.820656	18.813005
44.104384	1519.092752	18.818023
44.181796	1533.521841	18.823040
44.924802	1545.862285	18.828058
44.625906	1548.199977	18.833075
45.107878	1538.313428	18.838093
44.737391	1540.810590	18.843111
45.008871	1549.352231	18.848128
45.109695	1544.107310	18.853146
44.625487	1541.235152	18.858163
45.100682	1534.000570	18.863181
44.739422	1546.475072	18.868199
45.048732	1534.728213	18.873216
45.065895	1537.108214	18.878234
45.265672	1541.331199	18.883251
45.416845	1535.014922	18.888269
45.032987	1543.728021	18.893287
44.898079	1535.774221	18.898304
44.922044	1534.385086	18.903322
45.069938	1537.404304	18.908339
44.898157	1532.646803	18.913357
45.163178	1539.781940	18.918375
45.106504	1550.022023	18.923392
45.832048	1557.530440	18.928410
45.236582	1559.535606	18.933427
45.483748	1568.175717	18.938445
45.909035	1567.765526	18.943463
45.957482	1550.123122	18.948480
45.877718	1561.004287	18.953498
45.399794	1564.373414	18.958515
45.919366	1556.680627	18.963533
45.650425	1556.826655	18.968551
45.826193	1556.692001	18.973568
45.850691	1564.498921	18.978586
45.490770	1570.872979	18.983603
45.795845	1557.548840	18.988621
45.804596	1567.560994	18.993639
45.570954	1554.191343	18.998656
45.658602	1563.115067	19.003674
45.452237	1577.070814	19.008691
46.094759	1577.030750	19.013709
46.021152	1585.219032	19.018727
45.998657	1580.974770	19.023744
46.015789	1598.168354	19.028762
46.177370	1599.042627	19.033779
46.426367	1602.955001	19.038797
46.982305	1598.860521	19.043815
47.115672	1597.801492	19.048832
47.521958	1583.448546	19.053850
46.981523	1572.439886	19.058867
47.389838	1561.725337	19.063885
46.930576	1562.822504	19.068903
46.954172	1562.171893	19.073920
47.121272	1561.631485	19.078938
47.215363	1571.352639	19.083955
47.271251	1565.123772	19.088973
46.944873	1572.177427	19.093991
46.951704	1562.727765	19.099008
46.831569	1554.938915	19.104026
46.644937	1562.349510	19.109043
46.904112	1564.294198	19.114061
47.069285	1561.191542	19.119079
46.853509	1553.774194	19.124096
47.049813	1569.863712	19.129114
47.245406	1582.885867	19.134131
46.835920	1582.561464	19.139149
47.120045	1584.417061	19.144167
47.226866	1588.774452	19.149184
47.397850	1578.541819	19.154202
47.516947	1584.857081	19.159219
47.758199	1588.016409	19.164237
47.793036	1596.951528	19.169255
48.046719	1603.469909	19.174272
47.756286	1586.946908	19.179290
47.889916	1579.162720	19.184307
48.044076	1579.489029	19.189325
47.797226	1578.205173	19.194343
47.966606	1596.621613	19.199360
48.106301	1598.297724	19.204378
48.039672	1613.481462	19.209395
48.279369	1607.138754	19.214413
48.071274	1607.871764	19.219431
48.334996	1597.305940	19.224448
48.542757	1594.546947	19.229466
48.319376	1604.046145	19.234483
48.622577	1607.946925	19.239501
48.518433	1604.305515	19.244519
48.160804	1608.223974	19.249536
48.542522	1603.888371	19.254554
48.152870	1602.371121	19.259571
48.597049	1599.250266	19.264589
48.424538	1598.510264	19.269607
48.422719	1612.560426	19.274624
48.383785	1606.346308	19.279642
48.280063	1609.556194	19.284659
48.488491	1603.540253	19.289677
48.793980	1618.258953	19.294695
48.608506	1626.556191	19.299712
48.896905	1625.214242	19.304730
48.917586	1635.953581	19.309747
48.872264	1629.901397	19.314765
49.296138	1627.200271	19.319783
49.322712	1627.435991	19.324800
49.236052	1627.948121	19.329818
48.995559	1630.623875	19.334835
49.535756	1628.308588	19.339853
49.329214	1629.353788	19.344871
49.012479	1636.570072	19.349888
49.273113	1629.829613	19.354906
49.198788	1637.528872	19.359923
49.661400	1621.702807	19.364941
49.350022	1626.541892	19.369959
49.474489	1641.361380	19.374976
49.342072	1644.238063	19.379994
49.355446	1650.563497	19.385011
49.741966	1646.463825	19.390029
49.583402	1650.537497	19.395047
49.298512	1654.564564	19.400064
49.780584	1652.627560	19.405082
49.599157	1657.746228	19.410099
49.965024	1663.953668	19.415117
49.913902	1675.057666	19.420135
50.110358	1681.657570	19.425152
50.580111	1676.355170	19.430170
50.204646	1675.744595	19.435187
50.412956	1669.324699	19.440205
50.471943	1666.948627	19.445223
50.496188	1678.470091	19.450240
50.518809	1665.660072	19.455258
50.670943	1674.532785	19.460275
50.758722	1670.372321	19.465293
50.727638	1662.351805	19.470311
50.690293	1673.696659	19.475328
50.741633	1671.646831	19.480346
50.765361	1669.879019	19.485363
50.855330	1664.973430	19.490381
51.049066	1664.400469	19.495399
50.976861	1677.477012	19.500416
50.956613	1667.027944	19.505434
50.664990	1674.467556	19.510451
50.970735	1671.150486	19.515469
50.956363	1671.610336	19.520487
50.789290	1674.101092	19.525504
50.837169	1669.997334	19.530522
50.849837	1665.334159	19.535539
50.839444	1665.746051	19.540557
51.105294	1687.489628	19.545575
51.010990	1689.820731	19.550592
51.495310	1693.444017	19.555610
51.520018	1694.633101	19.560627
51.267375	1701.504910	19.565645
51.292949	1688.347269	19.570663
51.440251	1691.918882	19.575680
51.395816	1683.449146	19.580698
51.516425	1690.808803	19.585715
51.608899	1704.408847	19.590733
51.839118	1712.755015	19.595751
51.852979	1714.472820	19.600768
51.998693	1702.621931	19.605786
51.669812	1705.687006	19.610803
51.872252	1706.520208	19.615821
52.012085	1710.493784	19.620839
52.320323	1705.617319	19.625856
52.010082	1703.254546	19.630874
52.209889	1704.012417	19.635891
52.179549	1711.607028	19.640909
52.343997	1700.984014	19.645927
52.269595	1700.711582	19.650944
52.779402	1706.173932	19.655962
52.355688	1706.700671	19.660979
52.388769	1698.840565	19.665997
52.468189	1696.647504	19.671015
52.616560	1696.586545	19.676032
52.762616	1700.729567	19.681050
52.456324	1704.791537	19.686067
52.473666	1724.775002	19.691085
52.736195	1731.358325	19.696103
52.640590	1724.316681	19.701120
52.917045	1725.068931	19.706138
53.201367	1710.302518	19.711155
53.417789	1712.039280	19.716173
53.337189	1705.131009	19.721191
53.900731	1705.324154	19.726208
53.604954	1704.388740	19.731226
53.684785	1680.634706	19.736243
53.544270	1681.316172	19.741261
53.514187	1673.431197	19.746279
53.391007	1679.209846	19.751296
53.639130	1671.205816	19.756314
53.178170	1668.828644	19.761331
53.850675	1673.012774	19.766349
53.873788	1675.682207	19.771367
53.102670	1674.041303	19.776384
53.277875	1690.866376	19.781402
53.557843	1699.346807	19.786419
53.382821	1698.490424	19.791437
53.980466	1701.670025	19.796455
53.894317	1702.866902	19.801472
53.510947	1705.012634	19.806490
53.951143	1704.537002	19.811507
53.993737	1721.051384	19.816525
54.466957	1723.158429	19.821543
54.388644	1733.698639	19.826560
54.526661	1720.782250	19.831578
54.618855	1716.987168	19.836595
54.480484	1710.813742	19.841613
54.376484	1697.471136	19.846631
54.412100	1711.051635	19.851648
54.668739	1712.103622	19.856666
54.623856	1717.141086	19.861683
54.751416	1723.429833	19.866701
54.588462	1723.663503	19.871719
54.533601	1717.656957	19.876736
54.806575	1715.755658	19.881754
54.990405	1717.472247	19.886771
54.621120	1730.140636	19.891789
54.852945	1716.253413	19.896807
54.842751	1720.969890	19.901824
54.715285	1720.137661	19.906842
55.060736	1720.588828	19.911859
54.643501	1725.251912	19.916877
55.191577	1736.713948	19.921895
55.179157	1745.669123	19.926912
55.258369	1750.308569	19.931930
55.313065	1741.763409	19.936947
55.208244	1746.311584	19.941965
55.294828	1738.771343	19.946983
55.134704	1739.544228	19.952000
55.117958	1745.606136	19.957018
55.626785	1747.698172	19.962035
55.800935	1763.857587	19.967053
55.913598	1761.031322	19.972071
55.697593	1759.824703	19.977088
55.856922	1756.240073	19.982106
56.022713	1760.897601	19.987123
55.934398	1756.590960	19.992141
55.934003	1755.606398	19.997159
55.761006	1754.756009	20.002176
55.861822	1759.161715	20.007194
56.074808	1762.644219	20.012211
55.778706	1764.489186	20.017229
55.973597	1762.899848	20.022247
56.101657	1774.389431	20.027264
55.931903	1784.372693	20.032282
56.359187	1781.295463	20.037299
56.501448	1784.053662	20.042317
56.219405	1779.802424	20.047335
56.363643	1792.715961	20.052352
56.181741	1801.766981	20.057370
56.335107	1797.706731	20.062387
56.507072	1804.342053	20.067405
56.612233	1807.112343	20.072423
56.722553	1802.986209	20.077440
56.649719	1813.257362	20.082458
56.606336	1822.135343	20.087475
56.801348	1828.644005	20.092493
56.984532	1832.939073	20.097511
57.300167	1842.146186	20.102528
57.178750	1824.507865	20.107546
57.498854	1834.613709	20.112563
57.778989	1832.509305	20.117581
57.415121	1836.899014	20.122599
57.734941	1823.411430	20.127616
57.345664	1838.639282	20.132634
57.584588	1828.948210	20.137651
57.393545	1837.034967	20.142669
57.824868	1832.300255	20.147687
57.720296	1829.933847	20.152704
57.660096	1842.942367	20.157722
58.419497	1847.185595	20.162739
58.065243	1852.656284	20.167757
58.411829	1841.228478	20.172775
58.487145	1832.067820	20.177792
58.154233	1831.198143	20.182810
58.343667	1824.064742	20.187827
58.062936	1826.162949	20.192845
58.086290	1823.647233	20.197863
58.036196	1835.685316	20.202880
58.188858	1844.368678	20.207898
58.502077	1845.156236	20.212915
58.238658	1850.685367	20.217933
58.228216	1851.835752	20.222951
58.245855	1846.426963	20.227968
58.296470	1850.108340	20.232986
58.759649	1865.904102	20.238003
58.810213	1876.102429	20.243021
59.097693	1879.409251	20.248039
59.154055	1883.998640	20.253056
59.038561	1882.735336	20.258074
58.928730	1872.069715	20.263091
59.099397	1880.235879	20.268109
59.238284	1879.696699	20.273127
58.952710	1878.008582	20.278144
58.863502	1880.616635	20.283162
59.013289	1868.540933	20.288179
58.984565	1876.750763	20.293197
59.135978	1897.982222	20.298215
59.347101	1905.413084	20.303232
59.234549	1905.960812	20.308250
59.677518	1902.104767	20.313267
59.778204	1893.517659	20.318285
59.801703	1894.347171	20.323303
60.086946	1898.496972	20.328320
59.764144	1898.995381	20.333338
60.014988	1892.196386	20.338355
59.725777	1895.640337	20.343373
59.783530	1892.103054	20.348391
59.530936	1891.372352	20.353408
59.566818	1901.857011	20.358426
59.990123	1912.527517	20.363443
60.124953	1923.526977	20.368461
59.932347	1923.402336	20.373479
60.354897	1917.198312	20.378496
60.221507	1912.813442	20.383514
60.441368	1911.535794	20.388531
60.261556	1921.100962	20.393549
60.363947	1933.478299	20.398567
60.805898	1938.932351	20.403584
60.745536	1951.622228	20.408602
60.737810	1939.214384	20.413619
60.744169	1945.888165	20.418637
61.028406	1941.791728	20.423655
60.834474	1953.296843	20.428672
60.841659	1949.982024	20.433690
61.173393	1942.397216	20.438707
61.244548	1935.361084	20.443725
60.843173	1954.245466	20.448743
61.119547	1940.215430	20.453760
60.930134	1954.657999	20.458778
61.392381	1959.717563	20.463795
61.926225	1965.687510	20.468813
61.826778	1963.755803	20.473831
62.054844	1960.611727	20.478848
61.876492	1957.631917	20.483866
62.038597	1949.360280	20.488883
62.114474	1945.280502	20.493901
61.899369	1942.473681	20.498919
61.936489	1932.738230	20.503936
61.448928	1941.189948	20.508954
61.932006	1944.355872	20.513971
61.967426	1950.207748	20.518989
61.940270	1955.494993	20.524007
62.123954	1960.294960	20.529024
62.324241	1971.230606	20.534042
62.467556	1956.283966	20.539059
62.396167	1964.087054	20.544077
61.733128	1958.954628	20.549095
62.250062	1965.394283	20.554112
62.668069	1982.396431	20.559130
62.877086	1982.288158	20.564147
62.849516	1980.705034	20.569165
62.727518	1983.892585	20.574183
62.948697	1976.564826	20.579200
62.741665	1983.265533	20.584218
62.742032	1978.619971	20.589235
63.157680	1984.949167	20.594253
62.831787	1987.130166	20.599271
62.428399	1979.672420	20.604288
62.597611	1991.610188	20.609306
63.073053	1996.585655	20.614323
63.145728	2001.904709	20.619341
63.314828	2005.728622	20.624359
63.401867	2007.763278	20.629376
63.413057	2013.113999	20.634394
63.390679	2009.914229	20.639411
63.442385	2005.001881	20.644429
63.239307	2011.705139	20.649447
63.865375	2014.760448	20.654464
63.901525	2027.062953	20.659482
63.756557	2019.744844	20.664499
64.333112	2016.849469	20.669517
64.305404	2017.039995	20.674535
64.494956	2006.261407	20.679552
64.516703	2006.106548	20.684570
64.353403	1998.033880	20.689587
64.151221	1995.887782	20.694605
63.965408	1987.301053	20.699623
64.363261	1990.098387	20.704640
64.337772	1996.114402	20.709658
64.621722	2013.124828	20.714675
65.189448	2003.732777	20.719693
64.655006	2004.586044	20.724711
64.661951	1999.611236	20.729728
64.514582	2007.142139	20.734746
64.729618	2015.310925	20.739763
65.146074	2006.349539	20.744781
64.860899	2000.422939	20.749799
65.422155	2000.338723	20.754816
64.756199	2009.357910	20.759834
64.876188	2005.359617	20.764851
65.023081	2000.577623	20.769869
64.889204	2007.206987	20.774887
64.930976	2009.122454	20.779904
65.177700	2017.204253	20.784922
65.358526	2023.664701	20.789939
65.560216	2026.243264	20.794957
65.238556	2021.445849	20.799975
65.561071	2023.762594	20.804992
65.535310	2026.685851	20.810010
65.602519	2022.200291	20.815027
65.666939	2030.774402	20.820045
65.749604	2046.048876	20.825063
65.980654	2050.415442	20.830080
65.933613	2057.198569	20.835098
66.090349	2056.893300	20.840115
66.051152	2058.038707	20.845133
65.965850	2059.882442	20.850151
66.311015	2045.339820	20.855168
66.036454	2058.164112	20.860186
66.283277	2062.629215	20.865203
66.808921	2073.908760	20.870221
66.952717	2087.725178	20.875239
66.405365	2078.465671	20.880256
66.983548	2075.753079	20.885274
66.908118	2076.882036	20.890291
67.141876	2072.200112	20.895309
67.080242	2084.009775	20.900327
66.778809	2071.253075	20.905344
67.021031	2068.671688	20.910362
67.015007	2072.103142	20.915379
66.892399	2067.312595	20.920397
66.822143	2077.548783	20.925415
67.185874	2074.411968	20.930432
67.317236	2069.051681	20.935450
66.928311	2066.003648	20.940467
67.443046	2076.653706	20.945485
67.163814	2090.908390	20.950503
67.507448	2083.492091	20.955520
67.452584	2094.376016	20.960538
67.394739	2095.612695	20.965555
67.913402	2091.997300	20.970573
67.810637	2090.066096	20.975591
67.716922	2103.603910	20.980608
68.384483	2120.987077	20.985626
67.826529	2112.398264	20.990643
68.275965	2119.807892	20.995661
68.301387	2120.428823	21.000679
68.572133	2114.469283	21.005696
68.545889	2113.441387	21.010714
68.638842	2110.065845	21.015731
68.751354	2103.493444	21.020749
68.486044	2118.336143	21.025767
68.723739	2107.922400	21.030784
68.837353	2100.002240	21.035802
68.450765	2104.887878	21.040819
68.609138	2102.808713	21.045837
68.717731	2111.770478	21.050855
68.742835	2108.538050	21.055872
68.661611	2106.073292	21.060890
68.723276	2108.613705	21.065907
69.094571	2110.667235	21.070925
69.167774	2126.694367	21.075943
69.205971	2124.428774	21.080960
68.989947	2129.429880	21.085978
68.924414	2145.614335	21.090995
69.456748	2134.122707	21.096013
69.315145	2130.969882	21.101031
69.455595	2148.274190	21.106048
69.567329	2149.459223	21.111066
69.716219	2160.147355	21.116083
69.877630	2159.049212	21.121101
69.947845	2163.093692	21.126119
70.129957	2158.653327	21.131136
69.920757	2152.569674	21.136154
69.793952	2157.878804	21.141171
70.102744	2149.170807	21.146189
69.769985	2162.067353	21.151207
70.164433	2153.311302	21.156224
70.293379	2170.746817	21.161242
70.216228	2181.302890	21.166259
70.755411	2174.080181	21.171277
70.693721	2164.830225	21.176295
70.705216	2168.075924	21.181312
70.838296	2166.767587	21.186330
70.822077	2163.219675	21.191347
70.873417	2169.308998	21.196365
70.970167	2170.742529	21.201383
71.061453	2178.829667	21.206400
71.292494	2187.074939	21.211418
71.109987	2199.231716	21.216435
71.351536	2188.599565	21.221453
71.156045	2193.581713	21.226471
71.362673	2192.495464	21.231488
71.358499	2192.442474	21.236506
71.124342	2187.946986	21.241523
71.620312	2184.836903	21.246541
71.651772	2193.053288	21.251559
71.348765	2201.817236	21.256576
71.931826	2206.056448	21.261594
72.053367	2213.501387	21.266611
72.082252	2215.750259	21.271629
72.343542	2217.382250	21.276647
71.776958	2216.836126	21.281664
72.154427	2211.683644	21.286682
71.712315	2218.559902	21.291699
72.131237	2213.890140	21.296717
72.058143	2219.108871	21.301735
72.290897	2222.007691	21.306752
72.453000	2233.429150	21.311770
72.089183	2237.231938	21.316787
72.280799	2246.073541	21.321805
72.363415	2241.781197	21.326823
72.615745	2240.807756	21.331840
73.039971	2243.708328	21.336858
72.767176	2254.907163	21.341875
72.813543	2261.748411	21.346893
73.053804	2262.036081	21.351911
73.051146	2266.003563	21.356928
73.216341	2262.263276	21.361946
73.102892	2261.166893	21.366963
73.144914	2258.951183	21.371981
73.131697	2260.518614	21.376999
73.390628	2256.394486	21.382016
73.497398	2261.525262	21.387034
73.653073	2277.893158	21.392051
73.840821	2277.797663	21.397069
73.954062	2287.304775	21.402087
74.083814	2277.049760	21.407104
74.094573	2265.301565	21.412122
73.909176	2284.515605	21.417139
73.938517	2281.790598	21.422157
74.080040	2273.007592	21.427175
74.043767	2274.288264	21.432192
74.167193	2281.388936	21.437210
73.874183	2284.691534	21.442227
73.932351	2290.808238	21.447245
74.414841	2300.346235	21.452263
74.451332	2308.123209	21.457280
74.782307	2295.476181	21.462298
74.484940	2302.787551	21.467315
74.625434	2306.754846	21.472333
74.958355	2314.163760	21.477351
74.856237	2325.257166	21.482368
75.079998	2327.759749	21.487386
75.384409	2327.403080	21.492403
75.265748	2327.749788	21.497421
75.399088	2326.356187	21.502439
75.413847	2328.417914	21.507456
75.505552	2318.566452	21.512474
75.370198	2328.778203	21.517491
75.403269	2327.144579	21.522509
75.243066	2330.180341	21.527527
74.666851	2330.061770	21.532544
75.256569	2342.174158	21.537562
75.359513	2344.054889	21.542579
75.600694	2354.267995	21.547597
75.970204	2365.051296	21.552615
75.620360	2377.029108	21.557632
76.318701	2370.968193	21.562650
76.118539	2371.599007	21.567667
76.344217	2366.848833	21.572685
76.678191	2369.378447	21.577703
77.167601	2370.009203	21.582720
77.049916	2355.784559	21.587738
77.201063	2348.928326	21.592755
77.531314	2352.705132	21.597773
77.353629	2342.804075	21.602791
77.137325	2347.278236	21.607808
77.360198	2350.705665	21.612826
77.716431	2348.706125	21.617843
77.414869	2338.953753	21.622861
77.527433	2328.010223	21.627879
77.477957	2321.911112	21.632896
77.434900	2322.646859	21.637914
77.278659	2325.237010	21.642931
77.174800	2335.320778	21.647949
77.296567	2337.403717	21.652967
77.218959	2344.163308	21.657984
77.510204	2343.631953	21.663002
77.469145	2345.929603	21.668019
77.433543	2339.452764	21.673037
77.820062	2352.145936	21.678055
77.793813	2359.891673	21.683072
78.209959	2356.951788	21.688090
77.922078	2373.931660	21.693107
77.979132	2369.236143	21.698125
78.063845	2364.817204	21.703143
77.707467	2366.977746	21.708160
78.105340	2380.912631	21.713178
78.203735	2384.624551	21.718195
78.137149	2392.218782	21.723213
78.418778	2394.671337	21.728231
78.284997	2397.242221	21.733248
78.793114	2402.802887	21.738266
78.690377	2404.226468	21.743283
78.950437	2407.695458	21.748301
79.102567	2414.056367	21.753319
79.096224	2419.621392	21.758336
79.370887	2410.991169	21.763354
79.056000	2417.620463	21.768371
79.403341	2416.089388	21.773389
79.593657	2416.214413	21.778407
79.247493	2440.493780	21.783424
79.480961	2445.188291	21.788442
79.408538	2437.940772	21.793459
79.563647	2436.635297	21.798477
79.891243	2431.831366	21.803495
79.528853	2445.796301	21.808512
79.982748	2444.983984	21.813530
80.245035	2456.191159	21.818547
80.165791	2463.869447	21.823565
80.064003	2455.480863	21.828583
80.075233	2456.691032	21.833600
80.191236	2463.676160	21.838618
80.178734	2461.033385	21.843635
80.446636	2478.330793	21.848653
80.781670	2474.690260	21.853671
80.772923	2483.780940	21.858688
80.945690	2479.663865	21.863706
81.097799	2478.371478	21.868723
80.758670	2479.595169	21.873741
81.108513	2470.287295	21.878759
81.509204	2470.688855	21.883776
81.371135	2468.573746	21.888794
80.946689	2467.658323	21.893811
81.348728	2468.570946	21.898829
81.532656	2476.984644	21.903847
81.690338	2486.144094	21.908864
82.000510	2491.820818	21.913882
81.942232	2496.267256	21.918899
81.794934	2498.499410	21.923917
82.362414	2489.700476	21.928935
82.268037	2494.499695	21.933952
82.027417	2491.570519	21.938970
82.098698	2487.503958	21.943987
81.820021	2488.418417	21.949005
82.455378	2487.984970	21.954023
82.289008	2483.882823	21.959040
82.180615	2490.199108	21.964058
82.543880	2491.045181	21.969075
82.419546	2491.395932	21.974093
82.712079	2498.353589	21.979111
82.838884	2504.693225	21.984128
83.025559	2507.188984	21.989146
82.968638	2505.285314	21.994163
82.728370	2505.288017	21.999181
83.083027	2506.031283	22.004199
82.826205	2514.122274	22.009216
82.924713	2513.122272	22.014234
82.902391	2523.490116	22.019251
83.080351	2532.510725	22.024269
83.278050	2533.057507	22.029287
83.382188	2538.545403	22.034304
83.449615	2537.698572	22.039322
84.011688	2534.805371	22.044339
83.715216	2538.373660	22.049357
83.878440	2530.679132	22.054375
84.070938	2551.680893	22.059392
84.068485	2554.597451	22.064410
84.181843	2557.256121	22.069427
83.820332	2551.912462	22.074445
83.972715	2552.857648	22.079463
84.259793	2560.040256	22.084480
84.343022	2553.248172	22.089498
84.650917	2556.643468	22.094515
84.487630	2573.742995	22.099533
84.892164	2575.453710	22.104551
85.082976	2576.093092	22.109568
84.915049	2577.239638	22.114586
85.155166	2567.794152	22.119603
85.144921	2577.102879	22.124621
85.472639	2573.356160	22.129639
85.268557	2569.619651	22.134656
85.638523	2573.967874	22.139674
85.547630	2567.733106	22.144691
85.083654	2576.149888	22.149709
85.378136	2561.684171	22.154727
85.317125	2586.563168	22.159744
85.695840	2591.588579	22.164762
86.004358	2583.906123	22.169779
86.062580	2593.986894	22.174797
86.054526	2592.709968	22.179815
86.095988	2591.191786	22.184832
85.983409	2596.681881	22.189850
86.267334	2587.936515	22.194867
86.150360	2601.146943	22.199885
86.635639	2603.886580	22.204903
86.174748	2613.398041	22.209920
86.525559	2620.349829	22.214938
86.601737	2611.624172	22.219955
86.535962	2619.729650	22.224973
86.714209	2616.208180	22.229991
86.837535	2623.097550	22.235008
86.754099	2628.889252	22.240026
87.164343	2630.949404	22.245043
87.314712	2633.362465	22.250061
87.326937	2638.571190	22.255079
87.460863	2631.745935	22.260096
87.638193	2636.474485	22.265114
87.618782	2630.541014	22.270131
87.503942	2642.046880	22.275149
87.672598	2638.037714	22.280167
88.136785	2650.892589	22.285184
87.959022	2656.310793	22.290202
88.081258	2652.122645	22.295219
88.203450	2647.596808	22.300237
88.272351	2648.507655	22.305255
88.315633	2651.477073	22.310272
88.317331	2654.430874	22.315290
88.491828	2646.437874	22.320307
88.519409	2654.506741	22.325325
88.312770	2642.618564	22.330343
88.388869	2656.720536	22.335360
88.408082	2669.335412	22.340378
88.765848	2672.435765	22.345395
88.688538	2687.786191	22.350413
88.725722	2675.153077	22.355431
89.029029	2683.463073	22.360448
89.239058	2690.367373	22.365466
89.435973	2690.358819	22.370483
89.410868	2695.598621	22.375501
89.483804	2700.201420	22.380519
89.935167	2698.086038	22.385536
89.571102	2699.326250	22.390554
89.751001	2696.782883	22.395571
89.741212	2699.618549	22.400589
89.871927	2689.593539	22.405607
90.162647	2697.848692	22.410624
89.860924	2686.666465	22.415642
89.985950	2691.870268	22.420659
90.017109	2702.406628	22.425677
90.505248	2718.476993	22.430695
90.381325	2716.498518	22.435712
90.208687	2720.000220	22.440730
91.069266	2708.614925	22.445747
90.831602	2704.457550	22.450765
90.954044	2706.275318	22.455783
91.344738	2702.121106	22.460800
90.863304	2709.502328	22.465818
91.274101	2701.279994	22.470835
91.037999	2709.178484	22.475853
91.168433	2709.555850	22.480871
91.404139	2723.917070	22.485888
91.304494	2729.193736	22.490906
91.487038	2725.640016	22.495923
91.613253	2726.971167	22.500941
91.622031	2726.458532	22.505959
91.727808	2731.671655	22.510976
91.913250	2730.235195	22.515994
91.572881	2736.679209	22.521011
91.726485	2749.948613	22.526029
92.023713	2755.886234	22.531047
92.328097	2755.636868	22.536064
92.153019	2749.475109	22.541082
92.665113	2755.281439	22.546099
92.725087	2765.712356	22.551117
93.063371	2767.376596	22.556135
93.121595	2765.268763	22.561152
92.980080	2773.237767	22.566170
93.084297	2765.748002	22.571187
92.915724	2763.467179	22.576205
92.795736	2767.301549	22.581223
93.074115	2767.529640	22.586240
93.277079	2765.052105	22.591258
93.135833	2751.954372	22.596275
93.408843	2776.178820	22.601293
93.334788	2780.097567	22.606311
93.838801	2781.117417	22.611328
93.525770	2780.137289	22.616346
93.838598	2783.105791	22.621363
93.874386	2784.384749	22.626381
93.831334	2781.254337	22.631399
94.261188	2800.792895	22.636416
93.865670	2812.317322	22.641434
94.342306	2817.627377	22.646451
93.917375	2815.058230	22.651469
93.790341	2814.806598	22.656487
93.756297	2825.305841	22.661504
94.161435	2838.037489	22.666522
94.259080	2838.347374	22.671539
94.641264	2846.307465	22.676557
94.700151	2852.070768	22.681575
95.122852	2859.188197	22.686592
94.862388	2860.418602	22.691610
95.564694	2858.541867	22.696627
95.468108	2865.181521	22.701645
95.216504	2862.803151	22.706663
95.532488	2857.969354	22.711680
95.514563	2879.641788	22.716698
95.767623	2875.344849	22.721715
95.765975	2880.713608	22.726733
95.770305	2888.243354	22.731751
96.012057	2879.618032	22.736768
95.779126	2890.359735	22.741786
96.030278	2883.891707	22.746803
95.829908	2885.324215	22.751821
96.428530	2896.867499	22.756839
96.533296	2907.957459	22.761856
96.583681	2908.271546	22.766874
96.828113	2903.057523	22.771891
97.021162	2903.952211	22.776909
96.778180	2900.363713	22.781927
97.042061	2898.593107	22.786944
96.845721	2906.289815	22.791962
97.121395	2898.896387	22.796979
97.118664	2908.784835	22.801997
97.054481	2926.743504	22.807015
97.479248	2923.325617	22.812032
97.351465	2933.119930	22.817050
97.448933	2930.579895	22.822067
97.507238	2927.029698	22.827085
97.822055	2946.349619	22.832103
98.033135	2939.411240	22.837120
98.356860	2951.395026	22.842138
98.039469	2945.646712	22.847155
97.908971	2949.324952	22.852173
98.185266	2940.905680	22.857191
98.520050	2937.400806	22.862208
98.417813	2944.003496	22.867226
98.348144	2951.762560	22.872243
98.698047	2959.292186	22.877261
98.749968	2964.447485	22.882279
98.680461	2961.832447	22.887296
98.896763	2967.975260	22.892314
99.124869	2969.328439	22.897331
99.152720	2974.509581	22.902349
99.128937	2991.644595	22.907367
99.401372	2984.961759	22.912384
99.207605	2983.660065	22.917402
99.485928	2985.302100	22.922419
99.576379	2991.877964	22.927437
99.325473	2997.717952	22.932455
99.733608	3006.403133	22.937472
100.056453	3007.107189	22.942490
100.222724	3002.328224	22.947507
100.444069	2999.459595	22.952525
100.401068	3008.410694	22.957543
100.841182	2997.409447	22.962560
100.530533	3000.197320	22.967578
100.456848	2994.815028	22.972595
100.855255	3006.708322	22.977613
100.837367	3015.690232	22.982631
101.368948	3020.635154	22.987648
101.048498	3027.410718	22.992666
100.902512	3025.492454	22.997683
101.467896	3017.362684	23.002701
101.450395	3021.720845	23.007719
101.415628	3017.841105	23.012736
101.165678	3028.819092	23.017754
101.191508	3022.004207	23.022771
101.611527	3041.143733	23.027789
101.432413	3044.747502	23.032807
101.948212	3046.188453	23.037824
102.118347	3048.014612	23.042842
101.774840	3044.659507	23.047859
102.042965	3035.695456	23.052877
101.988434	3044.613651	23.057895
102.283635	3052.284390	23.062912
102.385845	3066.354214	23.067930
102.174977	3066.314465	23.072947
102.879359	3067.397821	23.077965
102.554611	3071.431408	23.082983
102.959916	3072.958998	23.088000
102.865327	3071.960624	23.093018
102.752776	3079.726419	23.098035
102.952656	3084.079156	23.103053
103.556013	3090.474204	23.108071
103.589300	3083.929561	23.113088
103.266373	3092.444554	23.118106
103.463197	3084.091242	23.123123
103.753603	3078.901572	23.128141
103.924430	3090.893477	23.133159
104.515104	3095.074908	23.138176
104.618723	3094.995665	23.143194
104.267603	3082.050299	23.148211
104.543486	3078.750247	23.153229
104.475614	3082.911117	23.158247
104.712563	3087.763061	23.163264
104.855689	3090.148907	23.168282
105.125677	3091.369330	23.173299
105.035251	3088.672316	23.178317
104.671611	3089.858833	23.183335
104.903700	3091.814220	23.188352
105.073795	3097.572913	23.193370
104.950378	3092.210959	23.198387
105.323076	3086.468779	23.203405
105.006367	3088.313929	23.208423
105.249392	3095.345807	23.213440
105.335219	3112.672175	23.218458
105.377896	3115.575486	23.223475
105.844402	3114.044738	23.228493
105.622956	3115.265929	23.233511
105.844939	3125.460372	23.238528
105.962233	3136.952506	23.243546
105.791571	3145.456442	23.248563
106.076568	3144.891321	23.253581
105.790044	3160.145322	23.258599
106.376511	3157.781613	23.263616
106.522679	3170.124584	23.268634
106.322966	3169.578117	23.273651
106.790538	3176.612940	23.278669
107.086422	3189.560685	23.283687
106.838844	3188.295759	23.288704
107.132069	3191.381003	23.293722
106.930829	3196.026616	23.298739
107.352750	3193.852639	23.303757
107.467546	3205.638727	23.308775
107.359375	3208.704409	23.313792
107.757313	3207.664062	23.318810
107.645006	3211.942345	23.323827
107.886224	3204.844521	23.328845
108.077286	3219.358271	23.333863
108.424519	3230.767324	23.338880
108.479697	3227.703600	23.343898
108.464629	3230.830537	23.348915
108.658139	3220.987980	23.353933
109.421173	3230.350240	23.358951
109.256000	3219.742930	23.363968
109.317664	3211.833525	23.368986
109.567402	3198.179079	23.374003
109.589318	3187.429039	23.379021
109.463760	3190.835132	23.384039
109.086574	3185.522128	23.389056
109.404473	3183.746240	23.394074
109.118313	3181.366894	23.399091
109.514196	3183.804928	23.404109
109.850606	3199.113471	23.409127
109.667371	3203.030370	23.414144
109.869405	3202.020525	23.419162
109.694025	3212.469407	23.424179
110.078115	3199.144375	23.429197
110.323882	3191.506148	23.434215
110.330571	3198.382338	23.439232
110.567973	3194.643241	23.444250
109.975560	3201.259219	23.449267
110.250234	3213.225569	23.454285
110.639848	3219.436169	23.459303
110.556691	3220.799956	23.464320
110.864742	3217.340219	23.469338
110.871031	3233.997363	23.474355
111.228918	3242.501114	23.479373
111.472607	3242.658866	23.484391
111.109207	3244.195687	23.489408
111.462411	3247.309477	23.494426
111.536246	3250.776065	23.499443
111.542956	3258.248785	23.504461
111.800849	3272.985728	23.509479
111.888434	3268.840705	23.514496
111.767030	3271.419254	23.519514
112.089521	3278.432519	23.524531
112.203222	3267.178938	23.529549
111.905281	3279.158736	23.534567
112.179331	3288.956959	23.539584
112.487275	3283.789749	23.544602
112.357209	3290.220154	23.549619
112.712421	3301.085152	23.554637
112.941935	3299.013711	23.559655
112.919931	3316.653743	23.564672
113.222732	3312.793974	23.569690
113.033517	3318.826454	23.574707
113.091215	3336.602436	23.579725
113.357715	3338.192691	23.584743
112.825780	3339.320210	23.589760
113.169196	3343.836875	23.594778
113.361889	3360.020094	23.599795
113.983378	3359.304737	23.604813
113.720140	3366.671191	23.609831
114.122833	3391.649540	23.614848
114.659474	3386.976931	23.619866
114.638606	3395.927933	23.624883
114.579549	3385.446031	23.629901
114.908510	3388.513122	23.634919
115.202991	3387.397344	23.639936
115.416873	3388.367717	23.644954
115.213330	3394.392985	23.649971
115.234584	3384.757059	23.654989
115.248170	3391.524938	23.660007
115.427889	3391.313911	23.665024
115.675158	3378.549753	23.670042
115.438978	3390.608382	23.675059
115.727119	3400.464439	23.680077
116.012046	3402.635723	23.685095
115.944688	3409.608737	23.690112
116.116114	3402.461735	23.695130
116.281263	3401.236689	23.700147
116.360685	3400.804565	23.705165
116.199102	3395.622051	23.710183
116.412562	3403.425602	23.715200
116.696314	3411.798948	23.720218
116.455655	3425.755158	23.725235
116.930657	3418.835472	23.730253
117.389386	3411.526957	23.735271
117.154785	3418.286144	23.740288
117.287035	3415.494444	23.745306
117.192745	3411.103118	23.750323
117.443195	3422.776699	23.755341
117.566538	3414.059090	23.760359
117.105892	3422.292688	23.765376
117.280979	3433.274182	23.770394
117.667807	3441.236972	23.775411
117.988559	3435.067216	23.780429
118.174112	3434.741658	23.785447
117.890624	3452.230007	23.790464
118.348936	3459.660906	23.795482
118.432997	3471.552951	23.800499
118.802006	3468.320391	23.805517
118.603749	3478.738271	23.810535
118.469164	3470.884556	23.815552
118.735209	3461.210477	23.820570
118.492844	3483.707628	23.825587
118.616983	3490.938073	23.830605
119.025124	3491.354281	23.835623
119.164173	3519.451137	23.840640
119.218667	3515.409052	23.845658
119.085243	3518.065256	23.850675
118.729170	3515.400068	23.855693
119.429282	3529.850595	23.860711
119.701465	3540.195268	23.865728
119.970816	3555.565054	23.870746
120.265290	3559.827430	23.875763
120.130785	3571.488449	23.880781
120.509597	3561.702074	23.885799
120.062606	3567.847363	23.890816
120.653079	3573.600728	23.895834
120.958396	3583.981297	23.900851
120.917892	3584.937632	23.905869
121.004943	3583.579548	23.910887
120.863253	3594.424244	23.915904
121.027550	3595.553847	23.920922
121.314357	3617.504814	23.925939
121.490913	3609.517380	23.930957
121.565619	3612.958652	23.935975
121.712929	3628.173910	23.940992
122.053983	3631.245472	23.946010
122.145456	3634.090770	23.951027
122.303652	3633.737906	23.956045
122.328666	3625.351125	23.961063
122.394339	3628.680184	23.966080
122.565707	3638.339930	23.971098
122.848694	3654.891258	23.976115
122.987081	3651.596728	23.981133
122.835140	3648.719834	23.986151
122.881178	3658.383323	23.991168
123.250755	3651.893426	23.996186
123.005699	3652.600709	24.001203
122.753856	3660.252724	24.006221
123.080890	3670.194404	24.011239
123.059679	3681.541171	24.016256
123.683104	3684.928588	24.021274
123.904794	3691.904053	24.026291
123.804925	3696.309919	24.031309
124.107221	3693.709482	24.036327
124.254815	3703.013154	24.041344
124.494334	3712.614986	24.046362
124.612054	3724.561926	24.051379
124.809937	3723.117139	24.056397
124.895153	3721.797205	24.061415
124.807233	3727.968706	24.066432
124.927506	3720.696981	24.071450
125.217970	3717.167295	24.076467
124.920930	3714.900039	24.081485
125.185311	3717.339683	24.086503
125.195824	3737.954543	24.091520
125.761481	3732.204210	24.096538
126.018797	3732.735438	24.101555
125.896068	3737.517308	24.106573
126.063864	3726.097207	24.111591
126.206001	3725.573249	24.116608
126.673903	3721.993844	24.121626
126.757940	3724.101756	24.126643
126.350974	3724.382909	24.131661
126.629578	3733.669357	24.136679
126.464755	3753.771818	24.141696
126.639539	3746.983967	24.146714
126.785960	3745.806001	24.151731
127.155127	3760.683832	24.156749
126.989245	3763.439812	24.161767
127.132350	3774.454900	24.166784
127.297061	3781.612864	24.171802
127.471765	3778.621969	24.176819
128.030743	3785.172521	24.181837
127.756600	3787.149989	24.186855
127.760604	3805.597603	24.191872
128.088037	3811.123717	24.196890
128.092052	3806.881114	24.201907
127.556252	3817.367523	24.206925
127.943906	3833.129439	24.211943
128.118448	3839.660958	24.216960
128.417897	3843.622784	24.221978
128.550716	3837.570527	24.226995
128.905374	3856.020411	24.232013
128.880989	3853.395062	24.237031
129.213959	3878.650068	24.242048
129.321612	3885.286706	24.247066
129.499939	3880.401476	24.252083
129.295746	3890.479642	24.257101
129.864877	3890.637233	24.262119
129.774037	3899.864504	24.267136
130.047633	3900.784578	24.272154
129.978912	3911.545510	24.277171
130.032192	3916.779776	24.282189
130.552300	3920.880858	24.287207
130.640367	3930.118166	24.292224
130.734046	3937.113656	24.297242
130.757279	3928.013697	24.302259
131.098496	3933.357795	24.307277
131.158221	3929.554679	24.312295
131.407951	3943.346563	24.317312
131.500596	3951.557383	24.322330
131.381449	3947.030920	24.327347
131.310943	3962.002620	24.332365
131.479747	3957.557573	24.337383
131.839293	3975.867944	24.342400
131.946680	3975.554547	24.347418
132.295245	3972.624926	24.352435
132.546964	3978.166036	24.357453
132.299641	3974.827343	24.362471
132.418459	3981.594841	24.367488
132.764582	3989.112865	24.372506
132.640301	3995.706746	24.377523
132.560478	4005.143826	24.382541
132.680070	4000.097270	24.387559
132.807488	4025.384483	24.392576
133.067580	4031.719689	24.397594
133.218577	4026.317889	24.402611
133.416955	4016.843425	24.407629
134.004361	4019.829355	24.412647
134.411683	4030.932871	24.417664
134.501568	4025.628962	24.422682
134.709889	4010.601057	24.427699
134.569230	4007.813880	24.432717
134.902044	3993.618802	24.437735
134.474879	3996.191402	24.442752
134.581668	4006.700969	24.447770
135.034962	4021.897327	24.452787
135.183085	4030.162671	24.457805
135.332660	4022.261318	24.462823
135.280609	4027.483609	24.467840
135.136219	4039.645161	24.472858
135.453178	4029.997571	24.477875
135.208634	4030.717413	24.482893
135.395225	4040.542288	24.487911
135.801757	4046.387569	24.492928
135.774943	4055.677546	24.497946
135.795244	4057.359854	24.502963
135.832673	4077.832034	24.507981
136.168069	4071.524063	24.512999
136.112847	4080.521784	24.518016
135.958592	4096.368302	24.523034
136.280804	4101.456594	24.528051
136.418036	4112.040390	24.533069
136.549298	4130.714714	24.538087
136.572722	4125.938756	24.543104
136.751805	4148.001829	24.548122
137.040865	4150.952168	24.553139
137.282785	4162.201456	24.558157
137.484455	4185.504643	24.563175
137.621444	4183.744201	24.568192
137.564208	4191.849056	24.573210
138.255657	4192.966064	24.578227
138.714649	4192.291759	24.583245
139.102864	4188.585792	24.588263
139.638908	4186.529654	24.593280
139.013660	4189.764382	24.598298
139.669482	4183.860993	24.603315
139.628839	4187.225644	24.608333
139.703477	4186.967843	24.613351
139.858370	4186.618640	24.618368
139.629423	4189.501287	24.623386
140.246147	4180.520272	24.628403
140.066778	4185.844495	24.633421
140.156906	4173.429342	24.638439
140.205611	4176.057287	24.643456
139.723000	4176.135593	24.648474
140.342637	4175.016490	24.653491
140.081867	4176.306998	24.658509
140.543859	4191.672586	24.663527
140.451182	4200.073343	24.668544
140.525566	4208.239778	24.673562
140.729898	4205.692396	24.678579
140.623915	4226.802554	24.683597
140.996709	4230.844580	24.688615
141.101917	4236.610584	24.693632
140.929012	4248.682027	24.698650
141.193887	4252.532543	24.703667
141.066543	4266.954675	24.708685
141.591469	4272.387057	24.713703
141.683929	4285.682896	24.718720
141.747967	4304.273176	24.723738
142.091629	4312.255699	24.728755
142.179751	4312.409276	24.733773
142.433092	4317.300034	24.738791
142.494126	4323.076100	24.743808
142.528637	4334.414601	24.748826
142.837724	4328.770310	24.753843
143.119756	4344.299769	24.758861
143.034972	4357.231869	24.763879
143.166481	4360.235178	24.768896
142.986891	4360.648224	24.773914
143.682743	4360.912346	24.778931
143.751555	4382.150131	24.783949
143.802715	4373.452768	24.788967
144.338095	4367.618573	24.793984
144.674002	4379.140591	24.799002
144.904830	4380.935344	24.804019
144.934355	4378.932794	24.809037
144.950385	4372.475591	24.814055
145.116958	4368.453741	24.819072
145.264212	4392.589473	24.824090
145.380010	4386.590184	24.829107
145.613804	4382.882968	24.834125
145.508420	4388.031602	24.839143
145.695572	4382.210586	24.844160
145.482486	4391.002626	24.849178
145.651389	4397.936082	24.854195
145.920177	4407.448507	24.859213
145.623839	4416.117798	24.864231
146.190920	4429.242001	24.869248
146.056466	4440.338585	24.874266
145.930460	4446.516260	24.879283
146.400741	4466.511163	24.884301
146.576388	4464.021870	24.889319
147.085335	4475.561197	24.894336
147.003590	4488.830649	24.899354
147.316057	4484.997536	24.904371
147.439936	4488.507072	24.909389
147.691452	4503.905695	24.914407
148.329429	4501.240256	24.919424
148.071909	4515.045268	24.924442
148.127108	4510.892377	24.929459
147.992117	4506.803819	24.934477
148.216064	4522.582357	24.939495
148.627353	4519.182055	24.944512
148.882997	4530.391560	24.949530
148.847585	4531.634381	24.954547
149.003808	4538.907597	24.959565
149.004886	4543.316890	24.964583
149.345384	4547.600744	24.969600
149.567928	4557.846413	24.974618
149.253675	4558.270959	24.979635
149.615873	4571.559732	24.984653
149.767074	4579.253544	24.989671
150.368781	4571.278403	24.994688
150.129287	4584.749242	24.999706
150.445034	4598.752296	25.004723
150.415580	4598.772675	25.009741
150.110262	4605.281334	25.014759
150.739846	4612.572416	25.019776
150.879145	4631.236537	25.024794
150.905549	4637.188539	25.029811
151.144804	4631.128916	25.034829
151.628203	4637.745207	25.039847
151.959467	4645.960224	25.044864
151.754998	4658.895391	25.049882
151.324289	4658.855143	25.054899
151.867130	4661.456728	25.059917
151.663744	4676.077252	25.064935
151.853320	4680.820217	25.069952
152.019547	4683.704545	25.074970
152.305546	4703.305444	25.079987
152.421704	4707.078207	25.085005
152.736149	4708.932571	25.090023
152.882625	4702.978904	25.095040
153.041973	4719.623056	25.100058
153.274814	4726.183697	25.105075
153.861509	4727.935705	25.110093
153.745029	4729.169067	25.115111
153.822706	4734.822729	25.120128
153.676935	4743.301445	25.125146
154.185604	4753.512147	25.130163
154.449298	4762.754101	25.135181
154.332650	4750.632728	25.140199
154.169734	4754.041773	25.145216
154.488810	4770.597975	25.150234
154.735813	4769.158085	25.155251
154.817512	4769.978669	25.160269
155.417248	4788.438697	25.165287
155.565804	4790.735544	25.170304
155.875474	4785.251999	25.175322
155.919351	4777.650852	25.180339
156.018285	4784.216580	25.185357
156.293653	4783.378303	25.190375
156.493745	4781.216584	25.195392
155.926058	4784.515051	25.200410
156.422898	4801.068856	25.205427
157.017766	4796.333166	25.210445
156.932304	4812.321106	25.215463
157.060542	4808.623926	25.220480
156.767835	4806.147533	25.225498
156.960342	4812.525100	25.230515
157.607914	4826.454573	25.235533
157.277546	4835.337686	25.240551
157.755762	4836.096539	25.245568
157.825837	4845.191920	25.250586
157.824168	4850.176185	25.255603
158.204188	4852.241305	25.260621
157.606788	4863.189273	25.265639
158.097156	4876.010103	25.270656
158.298461	4886.186667	25.275674
158.444350	4896.602284	25.280691
159.151705	4902.852380	25.285709
158.916571	4903.943248	25.290727
158.822783	4912.625431	25.295744
159.406956	4931.220598	25.300762
158.994996	4937.285138	25.305779
159.391474	4947.510261	25.310797
159.621186	4953.926276	25.315815
159.717991	4958.762668	25.320832
160.223845	4975.918111	25.325850
160.111538	4984.202342	25.330867
160.451577	4976.820143	25.335885
160.527304	4998.786714	25.340903
161.145872	4999.943531	25.345920
161.186149	5010.880689	25.350938
160.969270	5009.898089	25.355955
161.533331	5013.967329	25.360973
162.110726	5030.947551	25.365991
162.324779	5022.268707	25.371008
162.218354	5030.763526	25.376026
162.398570	5030.290419	25.381043
162.827294	5014.327780	25.386061
162.287513	5018.250077	25.391079
162.568847	5019.617222	25.396096
162.568896	5029.509555	25.401114
163.000097	5043.678053	25.406131
162.940689	5044.987774	25.411149
162.686209	5047.969225	25.416167
163.025117	5046.496066	25.421184
162.849106	5060.250923	25.426202
163.000033	5073.219434	25.431219
163.432604	5081.867096	25.436237
163.680987	5094.163904	25.441255
163.578485	5098.447418	25.446272
163.788208	5100.570645	25.451290
164.391715	5112.831116	25.456307
164.340215	5107.309011	25.461325
164.581893	5121.466043	25.466343
164.844506	5135.679798	25.471360
164.664909	5148.901837	25.476378
165.326094	5140.579447	25.481395
165.556671	5135.224901	25.486413
165.807887	5143.357914	25.491431
165.850184	5148.117618	25.496448
165.628189	5162.492069	25.501466
165.748268	5163.357199	25.506483
166.412965	5153.793760	25.511501
166.531006	5176.277933	25.516519
166.480367	5174.382471	25.521536
166.943377	5183.991325	25.526554
166.663185	5181.910647	25.531571
167.134571	5199.371534	25.536589
167.293987	5201.786690	25.541607
167.518016	5212.528067	25.546624
167.411731	5201.698939	25.551642
167.723508	5216.640565	25.556659
168.195927	5222.412843	25.561677
167.992933	5230.225205	25.566695
168.124577	5231.495726	25.571712
168.352021	5236.693789	25.576730
168.444255	5251.110925	25.581747
168.763333	5249.315719	25.586765
168.625802	5253.270134	25.591783
169.246409	5263.236430	25.596800
169.178071	5277.268242	25.601818
169.434872	5282.370209	25.606835
169.587002	5281.178631	25.611853
169.816188	5295.088380	25.616871
170.015162	5304.176548	25.621888
169.880379	5301.779663	25.626906
169.544892	5310.591204	25.631923
170.233639	5327.825827	25.636941
170.287976	5332.470072	25.641959
170.496587	5347.099590	25.646976
170.724472	5355.485695	25.651994
170.868978	5361.413234	25.657011
171.068708	5375.624343	25.662029
171.503018	5381.045918	25.667047
171.514227	5389.797207	25.672064
171.564116	5397.131514	25.677082
171.664113	5419.344179	25.682100
171.780256	5406.270734	25.687117
172.364060	5429.320322	25.692135
172.419101	5432.556672	25.697152
172.637874	5440.559138	25.702170
172.481036	5452.104894	25.707188
172.813524	5467.355999	25.712205
172.700059	5470.025162	25.717223
173.133612	5490.232090	25.722240
173.696269	5481.994329	25.727258
173.539900	5488.533773	25.732276
174.240264	5496.470755	25.737293
174.104905	5507.198816	25.742311
174.260560	5503.456192	25.747328
174.445769	5506.069391	25.752346
173.976961	5512.597512	25.757364
174.369730	5522.173291	25.762381
174.625904	5538.383299	25.767399
174.730748	5537.214849	25.772416
175.201100	5548.653550	25.777434
175.353570	5557.272447	25.782452
175.459751	5563.698441	25.787469
175.718772	5564.163173	25.792487
175.880939	5581.628379	25.797504
176.358928	5580.367110	25.802522
176.321701	5582.876063	25.807540
176.319320	5583.081621	25.812557
176.210574	5594.705206	25.817575
176.460297	5605.638522	25.822592
176.658329	5606.785098	25.827610
177.090290	5632.547970	25.832628
177.274989	5626.130350	25.837645
177.514028	5625.060951	25.842663
177.718153	5630.496343	25.847680
178.016079	5646.431639	25.852698
177.955686	5653.341300	25.857716
177.974120	5642.508275	25.862733
178.557597	5658.335994	25.867751
178.624195	5679.108469	25.872768
178.831261	5671.604648	25.877786
178.865893	5682.716700	25.882804
178.783665	5691.148084	25.887821
179.249381	5696.476481	25.892839
178.943198	5716.391631	25.897856
179.490702	5721.805156	25.902874
179.664678	5734.271812	25.907892
179.688863	5737.610874	25.912909
180.284678	5741.823697	25.917927
180.482978	5753.778370	25.922944
180.686032	5745.530190	25.927962
180.594570	5748.041296	25.932980
180.597020	5755.913438	25.937997
181.114052	5770.722554	25.943015
181.296415	5774.333715	25.948032
181.361192	5783.348320	25.953050
181.644915	5803.099121	25.958068
181.891597	5801.728646	25.963085
182.346003	5812.150418	25.968103
182.223730	5823.223852	25.973120
182.159062	5823.918912	25.978138
182.425584	5832.933697	25.983156
182.723773	5847.287675	25.988173
182.848553	5859.099190	25.993191
182.802170	5864.299029	25.998208
183.169622	5871.704037	26.003226
183.141962	5887.166238	26.008244
183.671698	5881.288252	26.013261
183.787553	5900.680189	26.018279
184.118055	5899.836437	26.023296
184.024401	5900.523387	26.028314
184.069340	5917.123316	26.033332
184.203990	5916.682535	26.038349
184.686504	5925.881544	26.043367
184.775777	5953.298626	26.048384
185.360021	5947.737263	26.053402
185.353585	5954.127266	26.058420
185.342152	5964.305989	26.063437
185.750400	5962.228519	26.068455
185.644599	5981.430932	26.073472
185.970411	5970.717158	26.078490
186.301599	5989.687400	26.083508
186.610877	5985.087413	26.088525
186.613782	5986.914656	26.093543
186.731828	5997.436251	26.098560
187.461341	6006.435859	26.103578
187.261805	6014.352186	26.108596
187.768557	6016.381929	26.113613
188.003174	6007.708885	26.118631
187.680131	6016.600900	26.123648
187.961019	6012.302048	26.128666
187.675804	6021.061910	26.133684
188.092687	6036.808571	26.138701
188.374369	6037.771693	26.143719
187.996771	6051.366127	26.148736
188.332285	6050.139636	26.153754
188.526253	6069.065036	26.158772
188.725243	6085.006650	26.163789
188.862738	6086.371019	26.168807
188.867601	6109.315894	26.173824
189.431454	6117.176547	26.178842
189.507468	6139.665296	26.183860
189.528671	6155.603084	26.188877
189.777749	6162.941411	26.193895
189.979076	6175.924958	26.198912
190.619101	6185.705655	26.203930
190.760188	6197.647430	26.208948
190.980047	6210.366114	26.213965
191.079894	6218.782021	26.218983
191.219049	6229.881289	26.224000
191.683651	6221.238629	26.229018
191.969210	6237.990787	26.234036
192.196785	6256.462903	26.239053
192.308354	6246.997640	26.244071
192.406009	6255.518075	26.249088
192.835666	6265.852418	26.254106
193.262992	6272.717947	26.259124
192.951854	6278.322141	26.264141
193.351823	6280.210705	26.269159
192.971123	6290.147217	26.274176
193.511356	6299.059642	26.279194
193.773206	6306.111938	26.284212
194.147750	6323.336449	26.289229
194.235365	6324.339271	26.294247
194.249391	6326.177443	26.299264
194.646687	6332.776196	26.304282
194.821798	6347.493809	26.309300
194.994467	6349.124197	26.314317
195.279293	6358.366831	26.319335
195.611774	6361.733770	26.324352
195.560719	6366.644064	26.329370
195.645743	6372.189765	26.334388
195.726287	6392.256940	26.339405
196.154083	6398.623686	26.344423
195.893242	6406.322446	26.349440
196.241573	6420.353399	26.354458
196.482085	6415.315760	26.359476
196.926579	6437.286629	26.364493
197.247126	6445.485192	26.369511
197.392324	6448.145793	26.374528
197.782924	6452.529629	26.379546
198.080815	6465.820332	26.384564
197.918217	6464.453552	26.389581
197.845463	6463.123292	26.394599
198.191670	6482.479983	26.399616
198.209729	6491.442233	26.404634
198.508445	6496.878942	26.409652
198.888265	6501.217117	26.414669
199.177552	6510.964207	26.419687
199.522204	6527.445425	26.424704
199.239308	6530.463105	26.429722
199.614134	6542.012007	26.434740
199.777391	6544.717162	26.439757
200.262891	6540.320041	26.444775
199.932344	6554.336835	26.449792
200.457622	6570.518493	26.454810
200.562650	6559.381024	26.459828
200.579451	6577.065532	26.464845
200.595147	6595.889807	26.469863
201.117603	6594.612079	26.474880
201.303570	6613.949664	26.479898
201.382447	6617.457149	26.484916
201.350353	6632.797559	26.489933
201.839753	6646.926680	26.494951
202.030753	6657.055332	26.499968
202.083748	6670.390625	26.504986
202.440566	6666.401788	26.510004
202.427201	6687.077373	26.515021
203.015366	6689.615381	26.520039
202.737971	6709.435583	26.525056
202.717983	6712.118784	26.530074
203.115336	6723.345461	26.535092
203.196571	6747.813426	26.540109
203.793409	6744.566921	26.545127
203.776600	6770.631714	26.550144
204.040083	6776.585386	26.555162
204.885534	6791.985025	26.560180
204.804410	6808.030859	26.565197
205.061292	6810.926667	26.570215
205.305472	6819.759170	26.575232
205.336376	6829.350939	26.580250
205.898071	6821.728301	26.585268
206.343256	6848.137969	26.590285
205.967644	6860.258481	26.595303
206.209174	6857.060961	26.600320
206.763546	6868.367455	26.605338
207.222084	6868.719086	26.610356
207.282082	6878.751455	26.615373
207.433905	6870.744347	26.620391
207.492794	6877.430709	26.625408
207.619342	6890.019182	26.630426
207.653887	6894.471186	26.635444
208.070623	6899.046781	26.640461
208.119514	6909.254519	26.645479
208.504206	6925.714079	26.650496
208.256664	6937.164405	26.655514
208.406855	6938.627879	26.660532
208.483919	6953.257070	26.665549
209.110402	6977.624669	26.670567
209.440665	6991.680973	26.675584
209.472328	7000.183618	26.680602
209.998968	7007.277037	26.685620
209.874468	7005.010911	26.690637
210.325212	7023.104966	26.695655
210.537953	7038.126642	26.700672
210.477838	7049.165884	26.705690
210.957442	7056.831714	26.710708
211.120684	7070.497382	26.715725
211.117737	7079.750460	26.720743
211.405189	7092.563409	26.725760
211.417351	7096.633815	26.730778
211.588551	7098.665415	26.735796
211.889740	7124.018271	26.740813
212.086295	7134.184204	26.745831
212.244647	7146.720550	26.750848
212.302391	7166.826847	26.755866
213.097288	7168.076322	26.760884
212.784515	7186.087371	26.765901
213.115003	7199.493493	26.770919
213.195656	7208.231684	26.775936
213.302082	7222.341954	26.780954
213.878344	7229.497185	26.785972
214.121537	7246.316843	26.790989
214.267798	7253.510618	26.796007
214.155613	7267.478175	26.801024
214.548437	7278.181863	26.806042
215.222259	7287.083447	26.811060
215.195460	7307.663960	26.816077
215.335280	7305.915407	26.821095
215.798285	7313.422930	26.826112
215.877812	7337.898261	26.831130
216.409996	7327.091588	26.836148
216.185955	7344.798548	26.841165
216.355065	7352.089823	26.846183
216.235162	7353.459637	26.851200
216.678907	7377.237474	26.856218
217.046361	7386.909726	26.861236
217.354830	7403.927719	26.866253
217.579993	7411.024036	26.871271
217.832431	7419.419896	26.876288
218.089090	7435.637827	26.881306
218.236750	7435.330731	26.886324
218.747098	7453.659011	26.891341
218.733300	7465.142725	26.896359
218.946920	7464.515986	26.901376
219.191286	7481.998623	26.906394
219.613817	7487.018584	26.911412
219.568408	7490.469821	26.916429
220.121156	7507.885530	26.921447
220.017965	7520.548086	26.926464
220.475649	7523.100214	26.931482
220.637361	7526.790704	26.936500
220.506358	7540.085824	26.941517
220.672141	7548.473136	26.946535
221.131427	7552.960192	26.951552
221.466568	7571.211690	26.956570
221.800071	7569.417174	26.961588
221.897526	7586.929096	26.966605
221.691520	7600.437978	26.971623
222.318315	7612.715454	26.976640
222.385488	7615.255785	26.981658
222.618289	7628.058676	26.986676
223.028133	7650.980312	26.991693
223.318034	7665.564306	26.996711
223.328235	7667.352698	27.001728
223.328125	7670.932663	27.006746
223.854470	7691.961008	27.011764
223.880984	7697.285764	27.016781
224.072094	7724.143494	27.021799
224.520678	7717.952399	27.026816
224.285632	7742.887644	27.031834
224.536210	7738.545757	27.036852
225.209704	7765.934576	27.041869
225.319384	7770.555039	27.046887
225.965414	7792.534042	27.051904
225.765761	7805.098162	27.056922
225.830820	7806.518136	27.061940
226.030258	7825.712839	27.066957
226.242669	7834.367675	27.071975
226.746382	7847.819912	27.076992
226.477147	7859.170008	27.082010
227.304542	7866.160114	27.087028
227.612976	7876.432161	27.092045
228.061507	7893.902345	27.097063
228.646766	7894.066953	27.102080
228.667200	7898.287782	27.107098
228.917701	7894.324705	27.112116
229.077260	7883.932456	27.117133
228.883116	7910.294814	27.122151
229.266579	7916.245963	27.127168
229.739584	7919.228265	27.132186
229.795944	7916.008881	27.137204
230.029421	7924.054345	27.142221
230.081137	7940.607697	27.147239
230.332693	7938.819590	27.152256
230.170954	7947.447493	27.157274
230.658865	7950.155981	27.162292
230.944958	7965.533203	27.167309
230.756806	7978.196673	27.172327
231.237384	7988.296763	27.177344
231.497436	7996.480185	27.182362
231.520718	8004.848850	27.187380
231.932165	8013.690615	27.192397
232.148374	8043.010496	27.197415
232.663441	8036.354341	27.202432
232.282145	8045.830971	27.207450
232.454944	8068.240719	27.212468
232.900928	8079.700589	27.217485
232.854665	8104.111284	27.222503
233.084537	8105.679256	27.227520
233.696700	8123.114713	27.232538
233.945026	8144.912967	27.237556
234.283692	8147.389004	27.242573
234.444062	8161.276921	27.247591
235.178608	8168.070080	27.252608
235.430985	8174.281654	27.257626
235.821698	8173.674676	27.262644
236.600949	8182.872827	27.267661
236.231348	8199.545674	27.272679
236.551348	8202.981197	27.277696
236.568213	8200.216206	27.282714
236.811041	8187.651433	27.287732
237.092583	8199.951485	27.292749
237.110603	8221.627836	27.297767
237.715325	8213.739056	27.302784
237.679105	8222.770584	27.307802
237.909050	8237.471705	27.312820
237.956376	8248.258163	27.317837
238.419344	8258.733671	27.322855
238.591608	8265.747001	27.327872
239.045426	8271.412653	27.332890
238.970319	8280.106149	27.337908
239.367672	8286.992891	27.342925
239.064067	8297.281535	27.347943
239.391633	8309.991223	27.352960
239.607884	8319.769590	27.357978
239.909637	8341.307197	27.362996
240.050030	8349.361026	27.368013
239.810483	8367.213447	27.373031
240.111804	8371.422224	27.378048
240.336392	8401.767407	27.383066
240.393684	8415.093825	27.388084
240.640179	8437.148430	27.393101
241.099092	8467.517224	27.398119
241.733024	8475.064911	27.403136
242.071339	8493.250532	27.408154
242.346494	8514.060046	27.413172
242.952661	8518.079330	27.418189
242.568788	8537.163536	27.423207
242.973482	8544.364938	27.428224
243.182178	8560.701825	27.433242
243.155634	8564.718598	27.438260
243.395913	8590.010344	27.443277
243.850808	8614.517330	27.448295
244.481952	8615.675596	27.453312
244.629513	8640.432516	27.458330
244.722055	8655.597353	27.463348
245.487182	8650.101739	27.468365
245.630979	8662.916050	27.473383
246.030736	8677.007025	27.478400
246.572270	8663.075764	27.483418
246.622845	8664.801140	27.488436
247.003896	8663.662105	27.493453
247.212265	8667.607599	27.498471
247.393356	8671.538398	27.503488
247.437019	8684.734536	27.508506
247.453875	8689.480179	27.513524
247.550347	8692.934809	27.518541
247.864877	8711.414800	27.523559
248.039504	8706.228942	27.528576
248.189747	8721.135440	27.533594
248.164652	8748.148291	27.538612
248.503374	8755.697856	27.543629
248.561503	8767.783660	27.548647
248.775288	8782.945511	27.553664
249.263653	8801.745810	27.558682
249.081751	8824.347454	27.563700
249.673231	8843.444295	27.568717
249.527505	8862.605416	27.573735
249.689382	8875.647530	27.578752
250.668811	8897.654877	27.583770
250.577208	8920.712990	27.588788
251.188576	8935.358443	27.593805
251.399475	8951.802676	27.598823
251.547241	8958.826398	27.603840
251.700102	8979.204006	27.608858
252.168471	8989.859046	27.613876
252.715871	8987.557526	27.618893
252.639736	9009.211573	27.623911
253.211770	9018.855992	27.628928
253.451306	9030.253882	27.633946
253.746041	9048.535235	27.638964
254.274171	9050.539898	27.643981
254.255444	9073.804700	27.648999
254.436456	9070.628851	27.654016
254.880993	9080.807768	27.659034
254.761413	9098.604329	27.664052
255.444008	9095.811331	27.669069
254.966976	9116.890173	27.674087
255.370002	9130.905213	27.679104
255.941948	9144.379348	27.684122
255.928229	9164.262162	27.689140
256.569126	9174.887293	27.694157
256.623374	9195.810896	27.699175
257.326257	9203.607039	27.704192
257.363558	9205.132472	27.709210
257.116330	9225.462138	27.714228
257.642006	9231.966181	27.719245
257.625826	9250.564500	27.724263
258.098969	9260.047639	27.729280
258.300429	9277.194526	27.734298
258.407085	9287.902895	27.739316
258.803682	9302.376859	27.744333
259.307259	9319.271532	27.749351
259.267809	9327.050695	27.754368
259.778473	9337.052127	27.759386
260.092042	9359.422582	27.764404
260.504911	9363.617379	27.769421
260.565257	9381.765063	27.774439
260.752585	9399.570961	27.779456
261.208890	9402.508751	27.784474
260.872833	9424.127975	27.789492
261.334884	9426.490262	27.794509
261.848918	9450.951263	27.799527
261.800026	9461.560818	27.804544
262.046391	9474.517584	27.809562
261.934956	9489.929552	27.814580
262.423207	9503.675872	27.819597
263.023226	9531.463936	27.824615
262.989975	9538.402401	27.829632
263.257329	9545.341426	27.834650
264.013868	9572.151700	27.839668
263.960576	9584.498490	27.844685
264.217259	9591.164514	27.849703
264.677491	9599.750026	27.854720
265.020240	9616.856287	27.859738
264.919535	9634.132634	27.864756
265.449561	9637.759893	27.869773
265.879291	9649.138026	27.874791
265.908215	9664.424097	27.879808
266.104423	9669.833507	27.884826
266.506709	9686.659039	27.889844
266.900184	9690.073931	27.894861
267.229196	9701.916106	27.899879
267.400161	9715.219449	27.904896
267.759230	9734.583875	27.909914
267.986404	9750.622154	27.914932
268.096112	9750.744006	27.919949
268.168405	9760.198249	27.924967
268.304973	9779.158502	27.929984
268.506080	9794.465233	27.935002
268.958464	9819.195215	27.940020
269.737455	9831.327348	27.945037
269.643017	9845.698219	27.950055
269.962398	9864.825850	27.955072
270.283264	9878.841620	27.960090
270.122028	9895.603524	27.965108
270.718109	9908.199890	27.970125
271.201788	9926.215897	27.975143
270.990764	9938.742186	27.980160
271.605308	9951.875605	27.985178
271.977039	9960.058299	27.990196
272.475296	9968.401265	27.995213
273.012398	9981.890908	28.000231
273.116755	9994.645978	28.005248
273.618862	9987.375474	28.010266
273.748166	10014.877614	28.015284
273.825935	10022.162065	28.020301
274.252378	10028.808133	28.025319
274.034064	10046.062128	28.030336
274.669936	10049.095201	28.035354
275.088395	10061.223626	28.040372
275.118285	10067.091599	28.045389
274.987260	10086.564266	28.050407
275.473638	10100.273434	28.055424
275.700457	10112.119153	28.060442
275.793481	10137.268599	28.065460
276.214087	10147.035062	28.070477
275.991112	10159.907509	28.075495
276.111351	10193.984899	28.080512
276.703880	10210.512914	28.085530
276.891740	10226.219888	28.090548
277.312991	10243.904929	28.095565
277.705689	10265.187500	28.100583
277.626202	10296.524015	28.105600
278.273363	10293.698473	28.110618
278.963972	10313.788599	28.115636
279.338081	10333.085004	28.120653
279.721928	10341.682753	28.125671
280.118098	10349.609225	28.130688
280.788355	10346.843227	28.135706
280.655402	10365.242981	28.140724
281.036742	10367.513763	28.145741
281.570002	10373.110865	28.150759
281.268103	10370.009978	28.155776
281.505511	10376.101488	28.160794
281.775698	10395.407822	28.165812
281.668744	10405.474413	28.170829
282.037923	10419.871427	28.175847
281.962457	10431.391840	28.180864
282.530223	10446.326286	28.185882
282.381890	10458.666350	28.190900
282.616242	10482.218724	28.195917
283.067326	10499.984613	28.200935
283.280456	10521.030212	28.205952
283.609324	10525.939295	28.210970
284.046616	10566.371208	28.215988
284.624315	10576.435496	28.221005
284.833349	10596.259901	28.226023
284.808430	10609.000786	28.231040
285.458539	10625.586513	28.236058
285.169586	10637.894912	28.241076
285.847967	10653.165934	28.246093
286.404408	10669.794700	28.251111
287.150663	10676.261756	28.256128
287.332049	10689.096874	28.261146
288.029759	10690.983756	28.266164
287.869112	10699.047585	28.271181
288.260923	10712.942429	28.276199
288.301410	10718.812114	28.281216
288.377925	10733.539103	28.286234
288.441573	10755.378652	28.291252
288.953503	10772.639612	28.296269
289.046068	10783.309990	28.301287
289.134497	10811.883728	28.306304
289.993115	10825.690194	28.311322
289.878618	10845.268433	28.316340
289.904342	10861.184317	28.321357
290.630840	10883.432327	28.326375
291.104200	10900.355248	28.331392
291.860382	10907.982786	28.336410
291.796059	10926.966011	28.341428
291.803766	10935.676272	28.346445
292.390980	10950.304979	28.351463
292.334848	10959.325149	28.356480
292.914389	10967.254912	28.361498
293.348855	10980.202389	28.366516
293.342415	11003.079318	28.371533
293.539417	11018.731860	28.376551
293.949960	11031.364191	28.381568
294.208278	11048.756457	28.386586
294.091006	11066.816609	28.391604
294.606797	11082.593236	28.396621
294.920676	11101.464080	28.401639
295.205677	11116.869349	28.406656
295.486060	11123.958498	28.411674
295.839313	11152.494684	28.416692
296.046915	11162.793729	28.421709
296.710889	11184.906589	28.426727
296.777378	11199.572356	28.431744
297.470878	11216.799145	28.436762
297.513418	11223.489622	28.441780
297.945192	11238.205906	28.446797
298.776313	11258.489889	28.451815
298.724684	11272.201585	28.456832
299.236832	11267.461359	28.461850
299.501978	11290.694206	28.466868
299.790466	11298.710472	28.471885
300.004577	11291.503248	28.476903
300.623140	11312.417154	28.481920
300.834502	11311.351747	28.486938
300.994495	11312.624596	28.491956
301.277941	11331.374109	28.496973
301.666805	11339.873656	28.501991
301.630632	11347.934173	28.507008
301.708958	11345.992736	28.512026
302.147294	11362.586830	28.517044
302.325852	11367.835291	28.522061
302.228995	11382.946585	28.527079
302.406971	11408.198189	28.532096
302.883869	11417.460822	28.537114
303.048453	11437.384609	28.542132
303.591571	11449.292450	28.547149
303.739019	11475.019372	28.552167
304.199419	11486.457008	28.557184
304.195526	11498.459514	28.562202
304.814840	11515.972838	28.567220
305.067695	11538.541660	28.572237
305.448895	11554.892215	28.577255
305.723318	11576.715696	28.582272
305.625439	11590.655856	28.587290
306.489903	11604.907211	28.592308
306.784426	11628.063279	28.597325
307.286319	11631.673212	28.602343
307.227392	11665.759076	28.607360
307.576420	11679.456058	28.612378
307.977166	11695.901579	28.617396
308.109763	11722.221622	28.622413
308.744156	11731.652506	28.627431
308.988476	11760.168687	28.632448
309.244082	11769.327013	28.637466
309.381250	11790.145889	28.642484
309.461654	11811.886175	28.647501
309.782055	11820.548166	28.652519
310.244251	11844.480432	28.657536
310.017167	11869.988333	28.662554
310.568404	11886.678990	28.667572
310.563122	11923.939858	28.672589
311.303799	11942.183047	28.677607
311.400754	11967.002789	28.682624
311.642054	11977.161258	28.687642
312.397367	12014.310209	28.692660
312.653984	12036.869572	28.697677
313.123077	12056.443475	28.702695
313.347823	12077.662688	28.707712
313.787131	12099.862130	28.712730
314.207470	12113.115728	28.717748
314.162528	12136.783135	28.722765
315.435360	12145.132799	28.727783
315.766621	12157.143543	28.732800
316.224972	12171.240678	28.737818
316.747422	12184.311072	28.742836
316.277277	12196.882367	28.747853
316.451812	12204.209442	28.752871
316.955548	12225.379073	28.757888
317.401020	12237.406822	28.762906
317.807544	12257.754837	28.767924
317.892320	12275.683649	28.772941
318.551129	12290.513827	28.777959
319.096887	12291.878255	28.782976
319.326584	12304.710118	28.787994
319.723058	12312.624750	28.793012
319.717556	12321.208244	28.798029
320.183561	12330.722486	28.803047
320.063724	12351.954604	28.808064
320.368053	12363.893889	28.813082
320.997874	12379.338089	28.818100
321.231388	12398.885871	28.823117
321.304374	12397.791425	28.828135
321.515724	12425.701153	28.833152
321.896104	12430.271160	28.838170
322.003197	12453.239544	28.843188
321.846470	12476.956358	28.848205
322.251535	12487.181182	28.853223
322.784066	12501.746991	28.858240
323.246481	12520.596141	28.863258
324.211813	12538.167074	28.868276
323.821381	12550.565149	28.873293
324.677649	12568.528861	28.878311
324.913932	12578.480026	28.883328
325.321967	12605.686801	28.888346
325.300821	12613.871831	28.893364
325.219832	12635.979233	28.898381
325.908816	12655.169017	28.903399
326.249116	12678.682396	28.908416
326.479298	12687.352518	28.913434
327.142172	12706.956929	28.918452
327.034430	12724.331954	28.923469
327.502106	12745.956189	28.928487
328.038000	12767.099319	28.933504
328.099359	12783.699680	28.938522
328.789573	12797.881185	28.943540
328.366135	12827.456593	28.948557
328.862023	12841.049458	28.953575
329.381271	12866.161472	28.958592
329.653709	12893.525559	28.963610
330.326360	12913.940217	28.968628
330.351863	12934.809322	28.973645
330.783567	12942.750314	28.978663
331.644175	12950.599273	28.983680
331.927205	12981.407004	28.988698
332.743198	12988.571366	28.993716
333.072766	13003.813357	28.998733
333.450439	13008.920756	29.003751
333.772890	13022.982848	29.008768
333.852039	13036.552315	29.013786
334.205517	13045.301299	29.018804
334.217685	13069.933595	29.023821
334.140918	13079.305354	29.028839
334.954452	13101.255092	29.033856
335.075988	13127.900922	29.038874
335.165590	13139.833077	29.043892
335.474939	13165.546579	29.048909
335.403719	13188.448883	29.053927
335.856753	13204.069703	29.058944
336.126603	13229.562076	29.063962
336.949465	13263.276711	29.068980
336.997137	13277.280719	29.073997
337.397051	13293.377247	29.079015
338.318822	13323.915571	29.084032
338.820492	13334.776338	29.089050
339.160650	13334.426553	29.094068
339.371552	13356.208305	29.099085
339.559843	13370.323122	29.104103
340.002410	13385.058359	29.109120
340.283597	13409.301848	29.114138
340.733366	13412.847614	29.119156
341.011661	13442.447365	29.124173
341.440629	13459.335299	29.129191
341.377122	13465.307295	29.134208
341.868582	13493.392890	29.139226
342.503663	13502.530878	29.144244
342.442118	13523.849975	29.149261
342.759571	13540.445868	29.154279
343.379300	13552.456805	29.159296
343.156302	13581.496920	29.164314
343.818976	13587.273795	29.169332
343.805323	13606.378149	29.174349
344.091004	13643.271849	29.179367
344.949914	13656.350889	29.184384
344.724701	13675.684040	29.189402
345.348920	13695.857610	29.194420
345.452782	13718.038553	29.199437
345.820762	13731.231969	29.204455
347.086201	13737.448742	29.209472
347.159936	13758.857570	29.214490
347.530353	13771.895897	29.219508
347.577038	13783.168814	29.224525
347.475238	13798.273337	29.229543
348.277798	13825.369924	29.234560
348.279628	13848.198494	29.239578
348.814328	13858.574412	29.244596
349.529783	13889.019453	29.249613
349.612522	13905.484836	29.254631
349.552303	13930.786377	29.259648
349.966572	13958.695202	29.264666
350.460113	13973.028216	29.269684
350.573957	14002.016533	29.274701
350.797352	14030.100446	29.279719
351.327168	14045.334209	29.284736
351.600084	14064.527046	29.289754
352.300704	14092.757815	29.294772
352.387824	14119.950415	29.299789
352.878401	14144.080140	29.304807
353.443299	14166.461420	29.309824
353.562842	14194.763857	29.314842
353.774309	14217.803400	29.319860
354.065761	14254.106842	29.324877
354.606393	14277.063632	29.329895
355.191197	14298.188232	29.334912
355.399719	14335.259509	29.339930
355.735249	14354.506052	29.344948
356.420506	14370.881194	29.349965
356.499674	14395.138448	29.354983
356.965838	14403.444183	29.360000
357.174023	14444.191692	29.365018
357.978685	14457.532379	29.370036
358.696059	14485.707439	29.375053
358.943368	14502.817228	29.380071
359.243286	14517.708195	29.385088
359.598673	14532.157883	29.390106
359.892789	14551.161585	29.395124
360.369923	14570.736848	29.400141
360.424645	14584.999687	29.405159
360.617870	14597.001895	29.410176
360.647242	14615.282622	29.415194
361.544081	14649.875634	29.420212
361.871742	14662.396988	29.425229
361.602627	14696.044163	29.430247
362.428077	14716.670684	29.435264
362.721253	14738.848610	29.440282
363.058770	14764.424098	29.445300
363.462940	14778.759004	29.450317
363.862393	14805.954490	29.455335
364.991560	14820.700806	29.460352
365.087237	14839.145122	29.465370
365.676571	14855.131378	29.470388
366.027112	14860.881446	29.475405
366.608444	14877.030031	29.480423
366.982776	14885.312378	29.485440
367.003761	14900.885012	29.490458
367.222125	14915.728984	29.495476
367.513942	14931.430018	29.500493
367.816511	14951.541311	29.505511
368.210041	14963.190436	29.510528
368.250723	14990.549418	29.515546
368.488479	14997.880368	29.520564
369.174388	15021.181787	29.525581
369.594290	15041.552825	29.530599
369.738412	15050.486924	29.535616
369.764785	15079.266271	29.540634
370.458878	15090.707617	29.545652
370.572792	15120.010285	29.550669
370.979112	15146.567240	29.555687
371.534086	15164.065553	29.560704
371.497969	15196.189837	29.565722
372.030498	15222.389324	29.570740
372.446367	15239.277726	29.575757
372.624831	15276.541847	29.580775
373.257422	15296.434741	29.585792
373.447374	15326.787042	29.590810
374.093690	15347.716901	29.595828
373.970407	15363.144987	29.600845
374.682982	15395.475186	29.605863
374.843878	15420.551630	29.610880
375.295307	15449.638032	29.615898
375.763673	15468.839757	29.620916
376.304851	15500.037747	29.625933
376.463616	15529.166674	29.630951
376.997527	15543.851472	29.635968
377.082503	15571.716024	29.640986
377.365352	15597.032690	29.646004
378.182537	15628.974326	29.651021
378.619713	15648.250568	29.656039
379.375788	15670.499636	29.661056
379.471988	15696.265539	29.666074
380.066013	15715.166865	29.671092
380.383527	15736.053591	29.676109
380.613674	15761.631341	29.681127
381.127377	15794.482708	29.686144
381.727720	15812.966254	29.691162
381.857272	15830.926196	29.696180
382.618242	15846.194902	29.701197
382.762632	15865.106368	29.706215
383.432970	15879.605954	29.711232
383.830696	15904.131362	29.716250
384.348223	15925.284036	29.721268
384.480099	15936.456532	29.726285
384.740714	15962.787800	29.731303
385.035110	15976.385863	29.736320
385.489458	16007.181304	29.741338
386.071520	16018.135321	29.746356
386.445414	16040.649610	29.751373
386.444170	16063.632909	29.756391
386.727806	16077.766475	29.761408
387.870110	16105.062932	29.766426
388.122349	16111.318225	29.771444
388.753789	16132.333378	29.776461
388.528693	16160.114409	29.781479
388.909532	16173.888655	29.786496
389.199353	16196.220398	29.791514
389.365637	16215.687829	29.796532
389.867860	16252.057010	29.801549
389.652570	16275.857157	29.806567
390.524216	16301.361026	29.811584
390.928400	16330.348739	29.816602
391.203137	16356.940495	29.821620
391.922884	16380.412019	29.826637
392.108280	16401.282139	29.831655
392.267959	16436.536398	29.836672
392.528026	16456.918037	29.841690
393.166912	16484.915613	29.846708
393.994465	16505.897487	29.851725
394.760090	16524.163329	29.856743
395.001934	16527.025099	29.861760
395.364385	16543.547122	29.866778
395.980353	16558.715796	29.871796
396.425392	16564.489570	29.876813
396.367380	16587.494967	29.881831
396.793938	16599.819010	29.886848
397.018680	16622.540391	29.891866
397.192603	16651.160159	29.896884
397.611342	16670.986710	29.901901
398.076917	16691.383982	29.906919
398.733348	16715.386914	29.911936
398.782259	16741.082623	29.916954
398.934135	16773.963574	29.921972
399.471616	16793.414862	29.926989
399.829530	16831.238382	29.932007
400.372191	16850.186728	29.937024
400.873502	16874.520379	29.942042
400.989527	16897.072660	29.947060
401.809201	16922.313821	29.952077
401.913600	16953.983305	29.957095
402.290908	16977.445703	29.962112
402.348082	17012.107390	29.967130
402.892302	17042.947355	29.972148
403.914339	17056.944580	29.977165
403.936632	17099.255389	29.982183
404.097938	17121.851420	29.987200
404.703415	17151.848181	29.992218
405.087009	17183.525113	29.997236
405.907619	17207.146190	30.002253
405.722141	17240.686891	30.007271
406.423711	17270.207733	30.012288
407.068739	17298.012869	30.017306
407.185284	17327.031073	30.022324
407.846381	17347.120652	30.027341
407.740167	17380.203903	30.032359
408.550475	17401.748505	30.037376
409.122337	17427.246849	30.042394
409.809435	17457.679894	30.047412
410.094745	17485.244398	30.052429
410.421628	17499.707086	30.057447
411.023972	17525.298729	30.062464
411.206097	17552.538269	30.067482
411.282903	17580.072196	30.072500
412.365350	17601.647304	30.077517
412.336333	17633.698751	30.082535
412.587976	17654.064020	30.087552
413.188054	17683.345451	30.092570
413.248505	17709.748177	30.097588
413.658949	17733.601161	30.102605
414.556347	17769.084139	30.107623
414.695752	17799.088136	30.112640
415.155311	17818.107228	30.117658
415.394345	17842.277624	30.122676
415.784509	17872.640682	30.127693
416.340512	17902.700011	30.132711
416.875944	17933.204797	30.137728
417.702773	17951.130815	30.142746
418.125450	17984.167506	30.147764
418.601963	18001.427939	30.152781
419.147767	18021.482474	30.157799
419.584783	18045.767600	30.162816
420.193242	18058.977111	30.167834
420.684920	18078.048316	30.172852
421.133787	18098.775022	30.177869
421.928857	18113.635923	30.182887
421.778585	18126.862522	30.187904
422.140309	18135.517807	30.192922
422.293705	18160.043067	30.197940
422.874075	18172.037784	30.202957
422.774017	18200.721456	30.207975
422.963709	18220.774782	30.212992
423.474681	18237.474135	30.218010
423.684276	18273.633680	30.223028
424.421709	18278.263232	30.228045
425.245081	18289.032526	30.233063
426.433550	18299.012172	30.238080
426.967153	18310.098236	30.243098
427.529360	18307.250029	30.248116
428.108794	18305.510999	30.253133
428.532006	18328.099256	30.258151
428.807566	18330.235866	30.263168
429.172155	18334.045360	30.268186
429.001014	18339.940868	30.273204
429.772378	18346.157136	30.278221
430.099699	18364.950978	30.283239
430.156047	18376.010300	30.288256
430.574943	18398.668803	30.293274
430.724848	18426.764281	30.298292
430.875477	18445.914214	30.303309
431.342654	18468.628456	30.308327
431.256526	18504.790250	30.313344
432.160985	18531.245908	30.318362
432.161926	18562.289754	30.323380
432.738353	18582.017914	30.328397
433.334629	18626.103201	30.333415
433.535520	18655.056567	30.338432
434.030519	18690.262740	30.343450
434.485037	18721.173052	30.348468
434.905684	18757.060578	30.353485
435.170479	18789.958968	30.358503
435.272155	18815.333342	30.363520
436.134952	18852.959029	30.368538
436.618817	18883.669187	30.373556
437.142486	18923.464191	30.378573
437.716081	18954.457418	30.383591
437.873967	18990.379963	30.388608
438.549895	19011.445038	30.393626
438.713111	19044.852447	30.398644
439.115595	19077.666712	30.403661
439.821197	19110.301174	30.408679
440.223371	19145.882729	30.413696
440.817018	19173.208947	30.418714
441.241126	19220.841323	30.423732
441.756359	19248.186171	30.428749
442.378878	19267.907855	30.433767
442.576772	19298.378892	30.438784
443.094366	19329.362482	30.443802
443.008393	19361.135034	30.448820
443.545100	19397.814342	30.453837
444.231217	19429.605798	30.458855
444.496560	19465.076566	30.463872
444.881466	19497.508893	30.468890
445.732783	19531.403883	30.473908
446.134860	19560.137743	30.478925
446.599364	19593.202252	30.483943
446.888742	19618.959109	30.488960
447.898313	19644.010006	30.493978
448.248689	19678.033781	30.498996
448.642243	19707.325153	30.504013
449.076763	19741.026364	30.509031
449.242451	19761.154513	30.514048
449.785920	19794.200752	30.519066
449.883235	19827.885112	30.524084
450.640313	19857.486554	30.529101
451.255447	19892.467711	30.534119
451.580909	19916.342928	30.539136
452.035509	19929.394452	30.544154
452.240935	19961.103661	30.549172
452.908550	19985.614350	30.554189
453.447531	20009.020505	30.559207
453.921796	20041.667271	30.564224
454.317529	20062.126358	30.569242
454.851481	20095.597892	30.574260
455.425042	20111.556233	30.579277
455.669518	20148.516213	30.584295
456.079186	20180.749965	30.589312
456.709747	20202.695276	30.594330
456.969235	20230.201358	30.599348
456.840887	20248.802603	30.604365
457.377662	20283.070087	30.609383
457.855238	20316.613957	30.614400
458.720047	20345.712880	30.619418
459.042153	20374.612022	30.624436
459.552781	20408.049814	30.629453
460.159554	20442.458315	30.634471
460.534095	20471.475798	30.639488
461.106688	20505.902368	30.644506
461.870845	20533.008088	30.649524
462.130108	20555.194823	30.654541
462.341613	20592.552497	30.659559
463.159535	20626.764180	30.664576
463.797514	20657.061416	30.669594
464.296179	20687.026571	30.674612
464.264788	20713.321304	30.679629
465.307546	20727.678112	30.684647
465.622247	20757.912105	30.689664
466.119202	20787.024726	30.694682
466.895196	20815.778041	30.699700
467.195691	20841.004050	30.704717
467.981220	20864.195938	30.709735
468.265291	20888.849608	30.714752
469.054748	20903.978893	30.719770
469.434126	20925.502890	30.724788
469.576064	20951.600367	30.729805
470.302010	20968.205419	30.734823
470.581530	20993.826621	30.739840
470.729284	21019.007136	30.744858
471.128569	21047.219202	30.749876
471.531035	21081.496357	30.754893
472.120089	21113.495215	30.759911
472.344732	21152.671576	30.764928
472.807735	21178.586688	30.769946
473.309933	21206.890373	30.774964
473.349203	21241.205393	30.779981
474.124032	21279.847755	30.784999
474.584735	21321.300216	30.790016
474.925939	21345.699149	30.795034
475.775232	21385.202060	30.800052
476.188520	21417.784793	30.805069
476.985055	21448.393444	30.810087
477.295118	21469.518134	30.815104
477.984906	21508.572244	30.820122
478.516260	21536.018879	30.825140
478.691564	21562.895457	30.830157
479.113159	21595.376097	30.835175
478.990259	21634.550656	30.840192
479.699340	21659.031714	30.845210
480.278746	21697.307257	30.850228
480.481307	21736.955786	30.855245
481.312426	21764.002237	30.860263
482.008010	21803.492007	30.865280
482.378316	21835.285991	30.870298
482.958902	21858.788976	30.875316
483.566720	21888.688425	30.880333
484.161796	21901.220232	30.885351
484.513420	21928.385787	30.890368
484.833685	21965.343705	30.895386
485.399212	21986.839887	30.900404
485.885857	22020.606406	30.905421
486.567624	22037.623633	30.910439
486.876103	22072.662739	30.915456
487.286645	22090.644749	30.920474
487.992120	22106.754785	30.925492
488.638916	22136.515851	30.930509
488.820921	22165.439438	30.935527
489.496194	22197.395044	30.940544
490.059701	22221.671995	30.945562
490.034026	22253.029125	30.950580
491.076371	22282.425539	30.955597
491.709446	22285.006107	30.960615
492.504600	22313.366877	30.965632
492.614885	22337.663978	30.970650
492.863385	22361.535196	30.975668
493.325295	22401.308971	30.980685
493.764175	22423.931118	30.985703
494.084040	22465.793352	30.990720
494.223861	22498.521543	30.995738
494.774774	22537.087496	31.000756
495.087502	22571.798251	31.005773
495.830671	22608.584118	31.010791
496.162442	22658.785677	31.015808
496.382868	22696.171227	31.020826
497.140752	22733.966043	31.025844
497.779580	22773.510822	31.030861
498.634118	22797.161843	31.035879
499.073208	22842.102536	31.040896
499.061484	22875.986016	31.045914
499.927761	22919.242755	31.050932
499.912066	22965.783693	31.055949
500.557923	22995.792637	31.060967
501.079933	23039.912052	31.065984
501.582405	23091.610988	31.071002
502.159615	23120.487084	31.076020
502.377428	23177.898638	31.081037
503.049486	23213.812048	31.086055
503.530537	23258.431204	31.091072
504.016459	23297.166727	31.096090
504.875299	23337.771565	31.101108
505.484502	23387.331473	31.106125
506.588913	23408.707397	31.111143
507.583547	23426.125767	31.116160
507.997787	23457.163554	31.121178
508.693801	23481.851119	31.126196
508.638963	23513.454903	31.131213
509.556711	23535.081190	31.136231
509.726968	23563.755883	31.141248
510.241021	23594.266501	31.146266
510.952495	23620.411539	31.151284
511.053759	23644.345137	31.156301
511.335769	23682.898308	31.161319
511.754833	23723.591356	31.166336
512.097013	23760.321723	31.171354
512.674514	23794.254058	31.176372
513.028047	23839.570519	31.181389
513.572262	23861.855632	31.186407
514.615843	23893.326936	31.191424
515.066507	23917.983728	31.196442
515.869567	23951.091320	31.201460
516.189509	23981.948711	31.206477
517.237341	24016.092570	31.211495
517.735048	24040.761148	31.216512
517.910723	24067.830642	31.221530
518.443138	24085.024546	31.226548
518.956388	24117.191731	31.231565
519.502493	24136.588964	31.236583
520.028659	24166.504565	31.241600
520.798623	24180.331322	31.246618
521.389186	24187.121076	31.251636
521.641555	24217.477491	31.256653
522.265756	24246.796578	31.261671
522.703457	24270.627999	31.266688
522.530947	24301.170751	31.271706
523.279713	24319.051577	31.276724
523.607361	24355.955926	31.281741
524.195396	24381.963199	31.286759
524.463410	24420.260883	31.291776
524.873034	24458.460762	31.296794
525.362170	24492.382767	31.301812
525.654453	24535.726064	31.306829
526.364476	24576.249170	31.311847
527.102816	24628.300861	31.316864
527.327621	24669.221982	31.321882
528.160792	24706.509597	31.326900
528.307003	24753.092696	31.331917
528.515650	24802.971260	31.336935
529.205836	24839.466172	31.341952
530.313524	24878.354436	31.346970
531.246231	24914.641105	31.351988
531.225162	24957.143048	31.357005
531.872338	24995.231137	31.362023
532.083906	25042.493561	31.367040
532.925888	25088.994403	31.372058
533.709700	25129.886317	31.377076
534.473521	25165.327634	31.382093
534.628069	25198.247553	31.387111
535.293571	25233.786451	31.392128
535.641016	25277.438746	31.397146
536.474655	25300.148062	31.402164
537.012135	25340.111852	31.407181
537.594963	25371.044215	31.412199
538.018740	25403.505463	31.417216
538.576185	25453.704205	31.422234
539.372471	25494.986742	31.427252
539.757512	25540.624455	31.432269
540.185440	25569.723249	31.437287
540.675779	25610.750307	31.442304
541.025910	25649.050194	31.447322
541.641405	25691.195482	31.452340
541.972989	25732.512932	31.457357
542.535460	25775.469260	31.462375
543.116411	25804.620410	31.467392
543.414841	25852.661189	31.472410
544.460503	25902.165709	31.477428
544.945614	25943.813601	31.482445
544.874875	25983.412007	31.487463
546.055641	26038.804874	31.492480
546.352305	26079.028817	31.497498
546.848996	26123.462336	31.502516
547.514576	26172.224066	31.507533
548.152397	26211.990691	31.512551
549.762061	26213.237936	31.517568
550.321239	26240.749933	31.522586
551.121188	26267.093221	31.527604
551.774170	26284.061691	31.532621
552.084317	26311.056399	31.537639
553.054890	26339.351359	31.542656
553.297351	26365.604604	31.547674
553.905719	26396.149053	31.552692
554.238477	26419.942487	31.557709
554.489050	26447.553369	31.562727
554.833069	26475.408861	31.567744
554.735844	26500.666045	31.572762
555.428433	26535.122309	31.577780
555.599863	26574.614656	31.582797
556.442744	26603.669308	31.587815
557.048391	26645.249325	31.592832
557.246011	26687.885196	31.597850
557.905186	26721.234651	31.602868
558.323789	26765.207736	31.607885
558.802426	26809.588697	31.612903
559.389792	26853.447221	31.617920
559.452954	26906.482095	31.622938
559.991870	26952.712101	31.627956
561.045156	27003.874017	31.632973
560.986818	27053.603792	31.637991
561.968371	27098.829840	31.643008
562.497791	27151.204994	31.648026
563.126889	27200.373058	31.653044
563.589443	27254.433744	31.658061
563.897419	27307.033379	31.663079
564.796834	27354.288943	31.668096
565.221097	27394.691568	31.673114
566.188656	27439.010436	31.678132
566.935782	27495.890554	31.683149
567.060623	27547.122534	31.688167
567.771990	27588.277210	31.693184
568.456777	27640.363986	31.698202
569.196963	27689.060876	31.703220
569.866174	27733.508998	31.708237
570.153535	27788.773970	31.713255
571.357610	27816.307806	31.718272
572.204439	27860.760158	31.723290
572.879840	27884.704227	31.728308
573.310288	27925.208071	31.733325
573.612900	27963.273242	31.738343
575.008896	27992.465001	31.743360
575.468113	28038.899504	31.748378
575.798313	28071.746194	31.753396
576.350620	28101.581410	31.758413
576.921584	28133.764992	31.763431
577.595278	28178.093299	31.768448
577.881467	28218.790839	31.773466
578.411068	28256.745377	31.778484
579.215604	28298.165091	31.783501
579.143895	28340.542971	31.788519
580.328945	28362.290875	31.793536
581.146313	28399.929097	31.798554
581.759713	28442.244779	31.803572
582.252930	28480.312848	31.808589
582.687387	28524.849809	31.813607
583.238355	28556.973967	31.818624
583.594203	28614.019254	31.823642
583.931064	28644.508229	31.828660
584.951851	28681.186167	31.833677
585.407880	28739.189592	31.838695
586.054917	28772.361009	31.843712
586.423378	28820.056597	31.848730
587.130585	28846.310229	31.853748
588.100678	28880.215300	31.858765
588.374641	28919.456051	31.863783
589.235471	28955.141744	31.868800
590.093490	28999.032293	31.873818
590.292257	29034.732700	31.878836
590.755150	29075.176891	31.883853
591.510705	29117.756280	31.888871
591.929408	29137.456279	31.893888
592.540094	29190.203276	31.898906
592.938518	29221.524198	31.903924
593.652119	29250.046535	31.908941
593.878546	29291.539300	31.913959
594.254823	29336.712853	31.918976
594.745700	29368.594807	31.923994
595.373099	29406.586825	31.929012
596.015892	29454.961768	31.934029
596.104529	29503.606399	31.939047
597.035845	29545.046834	31.944064
597.677328	29591.336394	31.949082
598.019176	29644.493026	31.954100
598.651711	29687.244454	31.959117
598.911796	29743.125770	31.964135
599.815988	29786.524104	31.969152
600.424912	29847.351320	31.974170
600.840463	29894.409974	31.979188
601.646225	29941.932639	31.984205
602.052736	29995.497303	31.989223
602.878757	30051.613732	31.994240
603.797745	30098.695620	31.999258
604.231581	30145.006111	32.004276
605.203159	30198.843642	32.009293
605.622287	30251.635830	32.014311
606.255743	30291.524889	32.019328
607.115587	30342.643127	32.024346
607.792370	30391.090837	32.029364
608.903149	30423.440514	32.034381
609.432344	30460.242419	32.039399
610.109264	30506.288317	32.044416
610.753004	30540.436581	32.049434
611.372388	30585.562390	32.054452
612.164132	30614.896225	32.059469
612.670637	30663.219373	32.064487
613.197009	30695.394961	32.069504
613.131678	30739.793289	32.074522
614.041426	30788.730337	32.079540
615.127712	30819.105878	32.084557
615.451026	30867.369524	32.089575
616.207539	30908.233072	32.094592
617.224720	30944.112813	32.099610
617.617476	30977.226240	32.104628
618.083551	31018.520823	32.109645
618.405146	31065.944456	32.114663
618.878710	31113.281325	32.119680
620.091272	31160.699226	32.124698
620.296394	31202.629015	32.129716
620.688807	31248.663967	32.134733
620.909509	31303.822353	32.139751
621.683862	31353.439251	32.144768
622.023106	31415.754374	32.149786
622.694216	31475.445161	32.154804
623.362521	31521.020548	32.159821
623.575546	31579.746213	32.164839
624.309179	31629.123569	32.169856
625.586750	31676.975045	32.174874
626.314209	31735.071088	32.179892
627.039535	31769.562693	32.184909
627.625264	31834.931976	32.189927
628.625622	31882.277098	32.194944
629.187717	31926.517078	32.199962
629.348522	31976.686139	32.204980
630.148183	32021.647941	32.209997
630.696055	32074.184513	32.215015
631.060934	32121.294056	32.220032
631.577625	32178.083944	32.225050
632.149775	32226.678678	32.230068
633.091426	32274.185555	32.235085
633.931161	32321.379674	32.240103
634.648008	32366.241321	32.245120
635.607808	32412.215814	32.250138
635.703750	32453.374897	32.255156
636.632125	32495.087233	32.260173
637.237332	32529.282708	32.265191
637.647017	32574.944921	32.270208
638.386972	32621.655827	32.275226
638.524459	32660.147341	32.280244
639.370696	32701.891845	32.285261
639.645722	32757.393334	32.290279
639.894497	32808.138641	32.295296
640.731537	32864.001781	32.300314
641.567987	32922.766945	32.305332
642.838738	32965.191884	32.310349
643.059035	33022.074465	32.315367
643.699158	33068.833524	32.320384
644.497392	33126.208046	32.325402
645.164643	33185.417543	32.330420
645.866212	33227.893690	32.335437
646.432483	33275.682560	32.340455
646.851612	33341.316419	32.345472
647.494959	33390.016577	32.350490
648.218484	33443.072955	32.355508
649.019961	33497.862243	32.360525
649.357299	33550.587039	32.365543
649.797964	33608.549608	32.370560
650.933496	33655.586899	32.375578
651.778693	33712.178088	32.380596
652.203439	33769.821149	32.385613
652.783791	33828.306291	32.390631
653.711107	33881.743001	32.395648
654.328000	33925.491874	32.400666
654.822860	33986.399551	32.405684
655.876014	34039.330257	32.410701
656.502774	34099.819424	32.415719
656.954742	34149.151759	32.420736
658.230464	34193.854461	32.425754
658.377616	34251.010978	32.430772
659.363298	34296.296450	32.435789
659.721663	34356.549953	32.440807
660.464796	34400.729054	32.445824
661.451555	34446.672215	32.450842
661.785158	34501.979529	32.455860
663.007503	34537.681794	32.460877
663.978843	34584.892148	32.465895
664.541313	34632.672055	32.470912
665.377396	34674.586459	32.475930
665.954585	34709.453720	32.480948
666.447871	34755.556567	32.485965
667.311709	34788.735482	32.490983
667.678539	34844.101747	32.496000
668.639353	34880.882207	32.501018
669.047374	34927.441282	32.506036
669.842818	34969.166599	32.511053
670.697640	35016.762770	32.516071
671.106712	35060.799260	32.521088
672.035353	35102.333396	32.526106
672.338422	35147.322316	32.531124
673.334908	35179.298864	32.536141
673.947137	35239.799890	32.541159
674.322274	35274.288565	32.546176
675.076922	35306.922576	32.551194
675.775417	35356.630335	32.556212
676.604372	35389.948404	32.561229
677.136439	35446.491840	32.566247
677.580616	35483.195708	32.571264
678.250113	35527.856518	32.576282
678.739418	35582.845256	32.581300
679.720164	35626.635863	32.586317
680.013734	35663.622722	32.591335
680.377644	35718.232996	32.596352
681.063946	35758.048407	32.601370
681.452549	35818.617513	32.606388
682.335345	35854.558233	32.611405
682.777595	35921.739304	32.616423
683.623921	35976.148686	32.621440
684.254879	36024.142379	32.626458
684.834738	36076.525912	32.631476
685.138797	36132.234109	32.636493
686.177893	36191.956912	32.641511
686.729928	36250.661832	32.646528
687.736582	36307.715397	32.651546
688.150604	36359.948402	32.656564
688.981698	36413.981898	32.661581
690.070020	36470.966282	32.666599
690.139781	36529.588970	32.671616
690.985299	36588.685427	32.676634
691.564986	36649.176568	32.681652
692.601963	36707.630211	32.686669
693.433713	36768.114068	32.691687
694.024897	36835.015590	32.696704
694.658891	36885.375607	32.701722
694.900879	36954.355271	32.706740
695.772647	37014.624932	32.711757
696.529846	37076.866470	32.716775
697.042141	37144.325038	32.721792
697.880001	37209.361920	32.726810
698.711705	37272.774879	32.731828
699.324070	37330.170786	32.736845
700.435149	37392.389772	32.741863
701.053831	37456.898753	32.746880
701.901582	37518.280156	32.751898
702.773881	37577.767230	32.756916
703.985615	37621.279378	32.761933
704.517897	37675.406850	32.766951
705.147737	37737.151619	32.771968
705.747949	37786.715946	32.776986
706.298815	37842.086659	32.782004
706.853836	37907.814685	32.787021
707.623266	37965.851809	32.792039
708.087608	38035.527541	32.797056
708.817576	38076.175187	32.802074
709.650521	38147.716248	32.807092
710.231115	38207.370626	32.812109
710.862979	38264.462471	32.817127
711.770111	38339.540139	32.822144
711.978149	38394.946674	32.827162
713.356557	38454.496514	32.832180
714.519740	38500.635985	32.837197
715.255131	38558.376475	32.842215
716.112254	38619.380152	32.847232
717.302369	38664.896065	32.852250
717.577520	38717.175410	32.857268
718.411676	38764.492284	32.862285
719.062825	38814.392534	32.867303
719.094748	38874.703308	32.872320
720.046954	38938.665245	32.877338
720.791743	38997.391955	32.882356
721.380405	39054.283935	32.887373
721.981315	39104.704905	32.892391
722.617521	39172.074666	32.897408
723.523053	39228.582616	32.902426
724.348386	39282.870877	32.907444
724.730479	39351.716272	32.912461
725.592459	39407.384070	32.917479
726.097052	39465.953405	32.922496
726.868710	39511.327558	32.927514
727.484920	39581.389376	32.932532
728.038415	39639.572132	32.937549
728.843773	39686.648877	32.942567
729.752503	39741.115025	32.947584
730.132434	39799.287284	32.952602
730.838050	39857.914923	32.957620
731.183024	39921.639123	32.962637
732.106857	39982.825988	32.967655
732.665485	40049.224002	32.972672
733.721645	40116.543977	32.977690
735.126319	40161.858898	32.982708
736.228528	40205.342733	32.987725
737.663456	40245.113185	32.992743
738.470014	40288.156252	32.997760
738.943543	40334.685266	33.002778
739.530302	40379.622034	33.007796
739.963687	40435.637458	33.012813
740.756326	40481.219075	33.017831
741.079874	40538.055035	33.022848
741.967473	40597.136982	33.027866
742.624531	40653.839112	33.032884
743.261867	40717.374676	33.037901
744.382857	40774.030197	33.042919
744.901818	40841.303233	33.047936
745.295696	40891.387451	33.052954
745.927031	40947.632674	33.057972
746.870779	41015.055148	33.062989
747.550377	41067.909636	33.068007
747.908121	41147.787902	33.073024
748.816403	41211.061372	33.078042
749.485641	41276.927310	33.083060
750.202465	41347.617924	33.088077
750.706438	41410.569118	33.093095
751.477599	41489.758155	33.098112
752.562202	41555.768982	33.103130
753.236458	41627.934417	33.108148
753.828177	41697.374403	33.113165
754.523012	41762.725530	33.118183
755.291397	41849.214862	33.123200
756.305688	41919.848368	33.128218
756.893418	41983.983526	33.133236
757.707773	42060.954278	33.138253
758.841069	42124.929025	33.143271
759.604041	42202.110662	33.148288
759.925391	42264.700606	33.153306
761.061821	42341.318618	33.158324
761.746352	42412.738714	33.163341
762.636602	42465.430963	33.168359
763.550509	42540.775082	33.173376
764.508874	42603.608367	33.178394
766.106879	42660.580335	33.183412
767.086666	42688.750457	33.188429
768.937829	42724.014279	33.193447
770.397028	42758.232322	33.198464
771.273897	42784.116339	33.203482
771.858170	42814.916091	33.208500
772.344258	42844.225846	33.213517
773.207871	42881.617016	33.218535
773.588372	42913.941304	33.223552
773.842060	42953.527411	33.228570
774.693428	42993.962965	33.233588
774.900671	43048.755288	33.238605
775.282909	43088.770697	33.243623
775.668970	43151.618737	33.248640
776.621018	43197.162223	33.253658
776.864479	43247.768584	33.258676
777.320838	43323.686282	33.263693
777.894539	43370.516076	33.268711
778.507408	43439.882370	33.273728
779.298935	43501.321049	33.278746
779.878862	43562.324781	33.283764
780.811828	43634.488149	33.288781
781.956689	43694.069704	33.293799
782.558702	43752.123010	33.298816
783.213212	43818.074752	33.303834
784.446651	43866.643522	33.308852
784.633441	43940.903825	33.313869
785.548697	44003.893288	33.318887
786.396880	44077.418569	33.323904
787.249099	44152.322373	33.328922
788.241557	44211.600131	33.333940
788.757546	44275.196491	33.338957
789.628216	44334.683295	33.343975
790.270101	44401.467353	33.348992
791.056368	44476.534324	33.354010
791.732121	44543.414742	33.359028
792.571775	44610.016831	33.364045
794.207267	44658.594330	33.369063
795.391765	44723.201179	33.374080
796.147506	44783.383895	33.379098
797.505728	44829.810003	33.384116
797.732938	44892.371428	33.389133
798.797263	44950.969471	33.394151
799.342877	45015.474205	33.399168
799.879736	45083.326692	33.404186
800.583606	45140.399962	33.409204
800.986459	45202.397243	33.414221
801.740560	45272.772014	33.419239
802.571992	45354.192119	33.424256
803.771211	45422.518159	33.429274
803.995825	45481.273612	33.434292
804.653314	45564.600274	33.439309
805.388610	45629.690843	33.444327
806.519481	45706.821088	33.449344
806.837071	45787.405530	33.454362
808.254813	45847.595600	33.459380
808.955011	45936.116757	33.464397
809.885805	45996.604430	33.469415
810.913491	46062.080894	33.474432
811.548358	46147.772770	33.479450
812.465540	46220.914824	33.484468
813.234759	46281.327203	33.489485
814.169783	46344.130422	33.494503
815.065942	46428.005120	33.499520
815.583715	46492.480485	33.504538
816.937465	46563.588334	33.509556
817.579462	46639.785736	33.514573
818.373115	46705.895148	33.519591
819.081228	46780.811213	33.524608
819.810034	46852.554968	33.529626
820.748102	46929.086822	33.534644
821.243828	47017.511216	33.539661
821.846489	47092.988775	33.544679
823.071334	47168.268516	33.549696
823.818105	47244.470629	33.554714
824.522373	47320.679616	33.559732
826.033845	47377.000241	33.564749
827.803250	47420.653790	33.569767
829.243922	47468.786934	33.574784
829.971329	47524.091263	33.579802
830.553355	47570.485726	33.584820
831.366184	47627.548353	33.589837
832.669316	47663.158391	33.594855
833.981002	47705.719714	33.599872
834.287416	47747.792324	33.604890
834.589691	47782.685322	33.609908
835.478473	47828.703597	33.614925
836.313257	47868.948125	33.619943
836.898985	47910.983885	33.624960
837.279218	47966.862097	33.629978
838.321254	48007.802139	33.634996
838.729760	48070.685798	33.640013
839.266785	48125.559407	33.645031
840.130592	48182.071428	33.650048
840.764481	48251.461997	33.655066
841.196688	48304.739120	33.660084
841.547786	48378.975859	33.665101
842.464891	48456.433478	33.670119
843.234593	48534.591240	33.675136
843.713780	48610.276541	33.680154
844.820391	48684.871159	33.685172
845.298586	48771.995529	33.690189
846.789904	48853.926565	33.695207
847.762264	48918.395011	33.700224
848.920897	48993.330505	33.705242
849.714294	49064.514462	33.710260
850.163019	49149.632989	33.715277
851.320170	49221.981860	33.720295
851.907588	49297.658919	33.725312
852.794236	49387.183142	33.730330
853.623009	49462.361324	33.735348
854.551165	49535.442775	33.740365
855.278937	49629.718776	33.745383
856.151953	49710.901345	33.750400
856.750894	49800.921174	33.755418
857.948218	49882.749821	33.760436
858.369718	49962.674924	33.765453
859.289554	50055.878841	33.770471
860.311742	50127.315199	33.775488
861.582767	50223.672886	33.780506
862.265144	50310.461302	33.785524
863.453922	50397.430625	33.790541
864.386360	50473.639940	33.795559
865.254637	50544.633353	33.800576
865.942175	50628.429472	33.805594
866.714779	50706.992802	33.810612
867.728314	50800.969712	33.815629
868.714004	50873.350481	33.820647
869.670703	50953.910679	33.825664
870.445682	51044.932971	33.830682
871.170716	51128.497290	33.835700
872.249893	51199.883814	33.840717
873.275445	51272.892354	33.845735
874.316740	51347.493145	33.850752
875.159131	51421.827757	33.855770
876.607421	51492.379471	33.860788
877.435507	51567.001505	33.865805
878.258198	51645.547574	33.870823
879.287567	51713.994895	33.875840
879.644367	51789.007373	33.880858
880.482363	51856.289027	33.885876
881.709225	51930.881795	33.890893
882.531919	52006.455196	33.895911
883.985991	52067.706419	33.900928
885.274429	52124.408819	33.905946
885.968860	52185.550812	33.910964
886.760185	52253.897575	33.915981
887.453146	52326.151284	33.920999
888.324493	52391.220988	33.926016
888.754416	52460.029577	33.931034
889.808428	52524.830772	33.936052
890.334204	52602.502469	33.941069
890.945731	52674.023275	33.946087
891.988850	52734.865655	33.951104
892.459823	52815.216857	33.956122
893.329389	52885.616114	33.961140
893.997592	52953.319688	33.966157
894.844013	53026.216087	33.971175
895.813798	53093.328938	33.976192
896.593543	53171.178135	33.981210
897.197088	53251.832917	33.986228
898.425682	53331.770555	33.991245
899.235602	53422.733438	33.996263
900.306089	53497.222679	34.001280
901.170013	53583.703991	34.006298
902.130390	53655.097561	34.011316
902.763631	53745.114701	34.016333
903.362997	53830.302913	34.021351
904.322590	53914.884827	34.026368
905.881083	53999.133356	34.031386
906.709819	54088.608815	34.036404
907.474315	54167.412895	34.041421
908.586756	54235.829370	34.046439
910.072497	54306.731819	34.051456
910.928309	54391.059495	34.056474
911.690829	54469.554818	34.061492
912.892630	54544.855926	34.066509
914.093581	54621.442022	34.071527
915.070455	54690.899755	34.076544
915.955994	54756.625623	34.081562
916.695197	54840.131408	34.086580
917.599589	54917.561983	34.091597
918.558623	54979.783848	34.096615
920.122703	55052.663420	34.101632
920.915247	55125.308931	34.106650
921.535053	55197.658811	34.111668
922.567590	55269.697861	34.116685
923.516607	55332.675285	34.121703
925.235172	55391.337386	34.126720
925.887177	55454.728414	34.131738
926.953331	55530.028466	34.136756
927.658232	55593.310376	34.141773
928.518434	55670.737638	34.146791
929.470003	55735.544654	34.151808
930.322761	55803.822572	34.156826
931.204311	55869.938191	34.161844
932.608868	55941.617607	34.166861
933.129108	56017.295295	34.171879
934.240717	56068.351740	34.176896
935.258746	56145.920526	34.181914
935.744278	56217.572961	34.186932
936.568207	56282.996226	34.191949
937.119190	56367.232832	34.196967
937.959713	56446.304795	34.201984
938.934517	56526.166187	34.207002
939.695637	56604.257434	34.212020
940.851772	56689.198392	34.217037
941.192387	56781.797782	34.222055
942.173923	56858.539174	34.227072
942.969979	56953.561862	34.232090
943.914282	57046.796115	34.237108
944.680175	57136.862448	34.242125
945.380018	57231.445539	34.247143
946.365757	57332.477924	34.252160
947.293886	57425.444026	34.257178
948.355671	57511.446858	34.262196
949.430155	57618.029752	34.267213
950.025938	57708.118380	34.272231
951.068187	57803.150413	34.277248
951.981470	57895.785211	34.282266
952.960136	57985.258323	34.287284
954.001125	58080.266331	34.292301
954.578639	58164.821576	34.297319
955.889458	58254.630060	34.302336
956.730175	58340.360141	34.307354
957.515771	58433.232071	34.312372
958.820278	58514.225984	34.317389
959.521371	58612.864988	34.322407
960.637055	58687.445740	34.327424
961.241595	58778.138278	34.332442
962.544947	58875.671926	34.337460
964.058265	58956.717100	34.342477
965.093614	59050.672812	34.347495
965.720931	59120.761149	34.352512
967.077140	59205.015269	34.357530
967.964561	59298.836736	34.362548
968.966468	59380.235099	34.367565
969.717293	59478.306568	34.372583
971.008398	59567.369794	34.377600
971.993771	59645.777787	34.382618
973.230798	59734.755103	34.387636
974.295647	59813.638638	34.392653
974.906998	59894.669110	34.397671
976.501176	59984.769043	34.402688
977.345336	60075.403809	34.407706
978.200654	60160.486105	34.412724
979.160417	60233.475501	34.417741
979.780437	60328.994597	34.422759
981.235646	60404.939291	34.427776
982.059475	60478.273391	34.432794
982.950436	60574.181691	34.437812
984.084791	60663.691088	34.442829
985.090429	60753.271487	34.447847
986.193017	60832.006856	34.452864
987.311474	60919.835942	34.457882
988.505062	61017.262334	34.462900
989.432626	61089.442749	34.467917
990.581557	61169.216415	34.472935
991.731909	61253.465354	34.477952
992.956061	61331.930212	34.482970
993.854250	61404.894707	34.487988
994.912027	61478.391614	34.493005
995.689627	61562.231219	34.498023
996.785502	61636.900045	34.503040
997.687140	61721.480484	34.508058
998.209975	61806.525299	34.513076
999.227092	61888.341100	34.518093
1000.333768	61974.536307	34.523111
1001.310723	62059.777171	34.528128
1001.934632	62149.820878	34.533146
1002.956080	62244.500003	34.538164
1004.160029	62335.587195	34.543181
1004.915790	62423.218569	34.548199
1005.786046	62512.199758	34.553216
1006.810748	62606.430317	34.558234
1007.497397	62705.537518	34.563252
1008.844644	62797.578967	34.568269
1009.378901	62887.778580	34.573287
1010.280269	63000.527017	34.578304
1011.742112	63095.476352	34.583322
1012.691239	63202.115797	34.588340
1013.917182	63284.581061	34.593357
1014.572909	63372.528889	34.598375
1015.869316	63478.254523	34.603392
1017.093965	63577.958819	34.608410
1017.775989	63678.229097	34.613428
1019.250044	63772.508083	34.618445
1019.762642	63863.974382	34.623463
1020.821710	63947.645302	34.628480
1022.170555	64021.212070	34.633498
1022.832585	64119.391803	34.638516
1024.196309	64186.436199	34.643533
1025.417267	64266.987306	34.648551
1026.343269	64351.256381	34.653568
1027.694807	64431.547127	34.658586
1028.479226	64515.781819	34.663604
1029.641019	64586.214004	34.668621
1030.774017	64669.552965	34.673639
1031.478174	64755.744502	34.678656
1032.919842	64834.642399	34.683674
1033.814289	64921.925439	34.688692
1035.254573	64994.600852	34.693709
1036.651140	65074.791688	34.698727
1037.073733	65152.956561	34.703744
1038.269551	65226.791267	34.708762
1038.777867	65310.596785	34.713780
1039.783692	65403.834224	34.718797
1040.553664	65489.986378	34.723815
1041.524504	65580.146733	34.728832
1042.513047	65672.305255	34.733850
1043.505630	65773.586515	34.738868
1044.508891	65867.706083	34.743885
1045.451929	65967.951208	34.748903
1046.717900	66064.487079	34.753920
1048.282703	66144.066337	34.758938
1050.091009	66230.534227	34.763956
1051.380478	66313.664338	34.768973
1052.005931	66390.218668	34.773991
1052.898658	66479.837245	34.779008
1054.097014	66558.252921	34.784026
1055.251715	66647.483094	34.789044
1055.901821	66735.367586	34.794061
1057.044015	66829.861642	34.799079
1057.785090	66924.950318	34.804096
1059.155567	67009.083111	34.809114
1060.305118	67097.498921	34.814132
1061.338958	67183.514458	34.819149
1062.194330	67283.024987	34.824167
1062.745742	67384.368685	34.829184
1063.895197	67478.180220	34.834202
1064.964568	67578.715946	34.839220
1066.035575	67675.560540	34.844237
1067.283799	67774.771237	34.849255
1068.238103	67874.211685	34.854272
1069.936602	67952.414509	34.859290
1070.932041	68040.110446	34.864308
1073.184226	68123.508168	34.869325
1074.188429	68190.701460	34.874343
1075.763982	68269.006702	34.879360
1076.671071	68338.298615	34.884378
1077.424269	68410.590566	34.889396
1078.977545	68494.813771	34.894413
1079.778298	68573.468487	34.899431
1080.705630	68656.478985	34.904448
1081.751744	68717.310050	34.909466
1082.506657	68813.726931	34.914484
1083.534736	68893.024741	34.919501
1084.587324	68967.164868	34.924519
1085.170452	69060.671441	34.929536
1085.923491	69145.819154	34.934554
1086.496477	69241.993683	34.939572
1088.012315	69349.653556	34.944589
1089.175221	69445.249458	34.949607
1089.556170	69548.914059	34.954624
1090.794175	69639.642365	34.959642
1092.035755	69749.892057	34.964660
1093.286820	69836.458880	34.969677
1094.282038	69929.575183	34.974695
1095.486928	70018.239383	34.979712
1096.287075	70099.539322	34.984730
1097.056905	70194.616620	34.989748
1098.139664	70282.946135	34.994765
1099.569460	70371.988126	34.999783
1099.947191	70466.228280	35.004800
1101.596688	70568.192428	35.009818
1102.205072	70664.183082	35.014836
1103.199560	70772.613895	35.019853
1104.466493	70877.038732	35.024871
1105.397249	70984.403854	35.029888
1106.771849	71098.387293	35.034906
1107.606668	71203.311295	35.039924
1108.821987	71299.665743	35.044941
1110.168359	71396.633388	35.049959
1110.991524	71505.119236	35.054976
1112.487639	71610.917134	35.059994
1113.737597	71724.910038	35.065012
1114.985748	71821.463934	35.070029
1116.056509	71929.697692	35.075047
1117.067636	72039.828286	35.080064
1118.136027	72145.517604	35.085082
1119.164407	72251.264236	35.090100
1120.478908	72352.787203	35.095117
1121.802009	72465.936024	35.100135
1122.605246	72575.683260	35.105152
1124.161472	72671.951680	35.110170
1125.318357	72783.911852	35.115188
1126.165260	72897.947240	35.120205
1127.535532	72995.955638	35.125223
1128.572032	73109.645785	35.130240
1129.499959	73209.585681	35.135258
1131.017598	73327.242235	35.140276
1132.086943	73445.374397	35.145293
1133.173630	73552.054426	35.150311
1133.900614	73670.354871	35.155328
1135.245492	73778.414204	35.160346
1136.512527	73895.111669	35.165364
1137.867126	74000.966501	35.170381
1139.087529	74100.876888	35.175399
1140.095180	74220.795356	35.180416
1141.521597	74321.105152	35.185434
1142.962222	74422.692410	35.190452
1143.835790	74539.897261	35.195469
1145.424533	74642.868266	35.200487
1146.256009	74751.822106	35.205504
1147.470888	74842.248956	35.210522
1148.473823	74959.650838	35.215540
1149.986147	75068.892652	35.220557
1151.351542	75166.251132	35.225575
1152.448745	75272.341063	35.230592
1153.653584	75367.445258	35.235610
1154.481853	75474.717855	35.240628
1155.266286	75575.486946	35.245645
1157.035654	75673.493727	35.250663
1157.994376	75782.229268	35.255680
1159.417234	75880.037397	35.260698
1160.592623	75985.535286	35.265716
1161.119085	76088.360506	35.270733
1162.776708	76181.167690	35.275751
1163.566073	76288.487578	35.280768
1164.727346	76399.043481	35.285786
1165.854641	76510.479166	35.290804
1168.326137	76584.578165	35.295821
1169.899859	76675.854696	35.300839
1170.661659	76760.949551	35.305856
1171.931845	76849.031059	35.310874
1172.986935	76920.450606	35.315892
1174.244848	76997.412472	35.320909
1175.401928	77073.047492	35.325927
1176.064140	77159.945220	35.330944
1177.075700	77232.449108	35.335962
1178.313507	77325.160878	35.340980
1178.784135	77414.597435	35.345997
1180.156981	77506.934109	35.351015
1180.724399	77613.559049	35.356032
1181.777923	77704.983345	35.361050
1183.069531	77804.567003	35.366068
1184.039567	77915.032156	35.371085
1185.110811	78022.669710	35.376103
1186.236082	78133.238259	35.381120
1187.673688	78237.247247	35.386138
1189.049541	78345.206028	35.391156
1190.052662	78454.946124	35.396173
1191.492676	78557.638462	35.401191
1192.111580	78678.789988	35.406208
1193.621612	78785.146078	35.411226
1195.043244	78897.559157	35.416244
1196.046672	79009.759084	35.421261
1197.470816	79119.765677	35.426279
1198.631283	79239.669872	35.431296
1200.147624	79336.525708	35.436314
1201.372085	79448.490317	35.441332
1202.496531	79554.884057	35.446349
1204.090039	79653.185891	35.451367
1205.142642	79763.062846	35.456384
1206.764062	79876.132925	35.461402
1207.961033	79977.778860	35.466420
1209.176366	80087.023664	35.471437
1210.833279	80185.102144	35.476455
1211.587037	80287.907733	35.481472
1213.629096	80371.142184	35.486490
1215.350064	80455.187008	35.491508
1216.532969	80544.636874	35.496525
1217.645234	80634.275391	35.501543
1218.532621	80732.298212	35.506560
1220.192614	80827.819299	35.511578
1221.468895	80909.970978	35.516596
1222.368684	81005.598332	35.521613
1223.217017	81095.304750	35.526631
1224.462316	81206.335662	35.531648
1225.256957	81308.365812	35.536666
1226.450109	81408.851970	35.541684
1227.357774	81522.331228	35.546701
1228.232574	81626.263164	35.551719
1229.294820	81745.952720	35.556736
1230.415279	81862.808375	35.561754
1231.813010	81978.405058	35.566772
1232.651945	82097.320002	35.571789
1233.809921	82222.216655	35.576807
1235.112751	82349.549284	35.581824
1236.305340	82465.053195	35.586842
1237.652098	82586.741908	35.591860
1238.920747	82703.755362	35.596877
1240.462561	82823.020081	35.601895
1241.877694	82944.408276	35.606912
1243.041139	83053.748734	35.611930
1244.260221	83180.046505	35.616948
1245.083292	83306.279775	35.621965
1246.704299	83424.305670	35.626983
1247.934976	83554.138349	35.632000
1249.115072	83659.943483	35.637018
1250.490814	83779.782904	35.642036
1251.577524	83905.876431	35.647053
1252.397401	84018.340369	35.652071
1253.807021	84130.282150	35.657088
1255.160755	84241.282758	35.662106
1257.128392	84327.138006	35.667124
1258.280870	84432.785583	35.672141
1259.766291	84530.905885	35.677159
1260.783388	84641.859079	35.682176
1261.657201	84736.894871	35.687194
1263.313828	84849.371213	35.692212
1264.197192	84972.231955	35.697229
1265.183375	85069.329418	35.702247
1266.332201	85183.672741	35.707264
1267.658459	85311.078312	35.712282
1269.106838	85425.337955	35.717300
1270.236587	85551.203930	35.722317
1271.355533	85667.707956	35.727335
1272.232029	85792.765418	35.732352
1273.749831	85905.951754	35.737370
1275.354255	86028.806132	35.742388
1276.518732	86160.168816	35.747405
1277.806873	86264.978339	35.752423
1279.184494	86402.568754	35.757440
1280.360962	86525.922690	35.762458
1281.620088	86645.779524	35.767476
1282.834270	86785.399342	35.772493
1284.575621	86901.367928	35.777511
1285.645120	87027.427092	35.782528
1286.487052	87157.197120	35.787546
1288.273636	87288.632802	35.792564
1289.419808	87427.936803	35.797581
1290.796226	87547.449608	35.802599
1292.274489	87683.205597	35.807616
1293.471528	87812.923259	35.812634
1295.084979	87923.225922	35.817652
1296.100980	88066.025452	35.822669
1297.659947	88191.519213	35.827687
1299.071672	88323.169950	35.832704
1300.155785	88449.004843	35.837722
1301.447787	88566.215841	35.842740
1303.142251	88705.288482	35.847757
1304.241160	88832.136524	35.852775
1305.814665	88954.513763	35.857792
1307.217610	89070.277462	35.862810
1308.683597	89200.288860	35.867828
1309.993355	89326.865417	35.872845
1311.389743	89451.071842	35.877863
1312.910028	89570.684511	35.882880
1314.285963	89688.495196	35.887898
1316.033047	89794.868045	35.892916
1316.898801	89913.430710	35.897933
1318.586731	90027.113388	35.902951
1320.219474	90143.162331	35.907968
1321.633263	90253.808921	35.912986
1323.205825	90355.978025	35.918004
1323.799013	90476.537059	35.923021
1325.103133	90591.358871	35.928039
1326.715692	90697.958656	35.933056
1327.746402	90818.146797	35.938074
1328.738326	90924.235653	35.943092
1329.770765	91053.473473	35.948109
1331.097856	91189.154965	35.953127
1332.678246	91301.655212	35.958144
1333.759403	91427.769293	35.963162
1335.157024	91545.558562	35.968180
1336.113389	91686.686420	35.973197
1337.323378	91811.730111	35.978215
1338.428148	91941.898360	35.983232
1340.013077	92071.270004	35.988250
1341.959547	92177.100625	35.993268
1343.445908	92290.151506	35.998285
1344.780252	92394.734694	36.003303
1345.936323	92485.670385	36.008320
1347.456488	92604.788182	36.013338
1348.800884	92717.736008	36.018356
1350.127350	92823.082362	36.023373
1351.183422	92933.274808	36.028391
1352.402226	93043.036737	36.033408
1353.530158	93166.666553	36.038426
1354.719038	93285.078097	36.043444
1355.824359	93413.921719	36.048461
1357.039429	93540.251871	36.053479
1358.212136	93670.391585	36.058496
1359.318062	93793.761187	36.063514
1361.162131	93933.874046	36.068532
1361.930745	94071.493190	36.073549
1363.006317	94213.425387	36.078567
1364.572466	94354.077745	36.083584
1365.643820	94501.893173	36.088602
1367.023834	94650.206302	36.093620
1368.575827	94790.824828	36.098637
1370.025299	94933.728836	36.103655
1371.953327	95081.362994	36.108672
1373.459872	95219.100548	36.113690
1375.686270	95335.368440	36.118708
1377.507007	95468.647125	36.123725
1379.216394	95593.882024	36.128743
1380.958134	95709.554947	36.133760
1381.998040	95830.040225	36.138778
1383.269769	95951.034942	36.143796
1384.780226	96091.032033	36.148813
1385.921909	96208.650874	36.153831
1387.361625	96330.863150	36.158848
1388.385842	96464.282743	36.163866
1389.679055	96587.177973	36.168884
1390.989521	96733.711861	36.173901
1392.008133	96871.925614	36.178919
1393.574243	97004.958933	36.183936
1395.085823	97138.571734	36.188954
1396.477570	97282.370136	36.193972
1398.078893	97420.837861	36.198989
1399.290290	97552.483598	36.204007
1401.198382	97672.549259	36.209024
1402.568187	97813.818207	36.214042
1404.404757	97944.366826	36.219060
1405.452533	98069.613169	36.224077
1407.109197	98198.745705	36.229095
1408.793351	98336.228439	36.234112
1409.659414	98465.814709	36.239130
1410.933960	98587.148705	36.244148
1412.267466	98721.062112	36.249165
1413.567848	98862.245110	36.254183
1414.927803	98991.528459	36.259200
1416.440179	99136.812368	36.264218
1418.102148	99267.583746	36.269236
1419.566132	99393.429715	36.274253
1421.182970	99526.668538	36.279271
1422.669185	99660.207145	36.284288
1424.057881	99793.292426	36.289306
1425.573838	99920.793098	36.294324
1427.207118	100054.411871	36.299341
1428.218962	100177.276032	36.304359
1430.143634	100303.091889	36.309376
1431.207228	100440.921117	36.314394
1432.389827	100569.008693	36.319412
1433.880626	100702.170574	36.324429
1435.725126	100831.246443	36.329447
1437.347237	100948.617850	36.334464
1438.607560	101062.166590	36.339482
1439.900305	101187.982821	36.344500
1440.922707	101292.454035	36.349517
1442.159601	101414.577896	36.354535
1443.454868	101531.951569	36.359552
1444.605998	101659.820140	36.364570
1445.526955	101782.894693	36.369588
1447.193920	101927.875486	36.374605
1448.616163	102058.834915	36.379623
1450.263807	102193.842173	36.384640
1451.641564	102332.416555	36.389658
1453.242674	102452.433721	36.394676
1455.059224	102590.408406	36.399693
1456.377586	102722.502349	36.404711
1457.982169	102857.189397	36.409728
1459.345947	103001.867123	36.414746
1460.792210	103139.242456	36.419764
1462.175488	103282.866055	36.424781
1463.275609	103423.821108	36.429799
1464.724851	103551.853492	36.434816
1465.945109	103711.441508	36.439834
1467.345148	103855.648204	36.444852
1468.864114	104011.425546	36.449869
1470.005802	104164.954764	36.454887
1471.528919	104321.519006	36.459904
1472.548499	104476.349244	36.464922
1473.964916	104644.330116	36.469940
1475.908575	104799.005340	36.474957
1477.406294	104962.093651	36.479975
1479.835532	105114.919656	36.484992
1481.617892	105270.953493	36.490010
1483.229027	105422.259908	36.495028
1485.275085	105561.441098	36.500045
1486.382369	105709.023371	36.505063
1488.267404	105857.131896	36.510080
1489.372451	106001.900921	36.515098
1490.804997	106134.434378	36.520116
1492.491168	106285.745662	36.525133
1493.336650	106440.054112	36.530151
1494.898750	106589.255846	36.535168
1496.095239	106745.083353	36.540186
1497.703518	106897.182958	36.545204
1499.315155	107049.916722	36.550221
1502.103090	107176.080770	36.555239
1506.038014	107267.183676	36.560256
1507.745028	107388.279851	36.565274
1509.043495	107498.002477	36.570292
1510.406686	107601.514729	36.575309
1511.791176	107724.488251	36.580327
1512.971027	107831.516819	36.585344
1514.304853	107946.852772	36.590362
1515.391452	108073.246890	36.595380
1516.435032	108198.659090	36.600397
1517.747946	108330.877313	36.605415
1519.290329	108452.269153	36.610432
1520.478859	108590.290073	36.615450
1521.939715	108717.084799	36.620468
1524.058377	108829.942943	36.625485
1525.380164	108963.480997	36.630503
1526.909830	109094.920238	36.635520
1528.364256	109226.054664	36.640538
1529.688575	109359.758698	36.645556
1531.065102	109492.047533	36.650573
1532.139668	109633.653684	36.655591
1533.370535	109766.448109	36.660608
1534.406897	109922.441697	36.665626
1535.958078	110078.647518	36.670644
1537.461710	110214.495392	36.675661
1538.267264	110356.006840	36.680679
1539.873455	110502.225826	36.685696
1541.326884	110651.068879	36.690714
1542.440460	110803.972788	36.695732
1544.041439	110951.640134	36.700749
1545.543122	111098.841653	36.705767
1546.836883	111262.016908	36.710784
1547.990863	111412.177933	36.715802
1549.745061	111585.314197	36.720820
1551.260535	111752.857755	36.725837
1552.727854	111923.656144	36.730855
1554.662302	112081.130073	36.735872
1556.151786	112246.004117	36.740890
1557.564572	112419.933127	36.745908
1559.612023	112577.315564	36.750925
1561.094236	112751.210013	36.755943
1562.696613	112914.496980	36.760960
1564.615006	113091.787426	36.765978
1565.733441	113262.405537	36.770996
1567.185987	113437.550786	36.776013
1568.706947	113613.802290	36.781031
1570.566181	113787.135760	36.786048
1572.387860	113960.628095	36.791066
1573.524333	114139.656064	36.796084
1574.771669	114310.309779	36.801101
1576.316943	114498.825939	36.806119
1578.265338	114676.728242	36.811136
1580.003399	114860.295339	36.816154
1581.763076	115044.620967	36.821172
1583.950390	115219.761898	36.826189
1585.421355	115397.577134	36.831207
1586.767899	115576.427244	36.836224
1588.561920	115759.000843	36.841242
1589.871271	115936.856519	36.846260
1591.523419	116109.281982	36.851277
1593.184962	116308.202312	36.856295
1594.748672	116473.946425	36.861312
1596.485473	116661.632116	36.866330
1597.967641	116837.499276	36.871348
1600.208986	117000.641611	36.876365
1601.541047	117185.399608	36.881383
1603.957610	117347.767854	36.886400
1606.138358	117526.205793	36.891418
1607.195096	117694.000217	36.896436
1608.963230	117859.769401	36.901453
1610.406194	118035.787815	36.906471
1612.139953	118200.967707	36.911488
1613.492285	118372.511663	36.916506
1615.205687	118543.974833	36.921524
1617.048754	118716.940698	36.926541
1618.390363	118882.412917	36.931559
1620.400124	119050.103087	36.936576
1622.413699	119214.520845	36.941594
1623.896716	119375.736633	36.946612
1625.740560	119529.641440	36.951629
1627.369242	119694.450969	36.956647
1628.694217	119860.145657	36.961664
1630.417393	120023.546594	36.966682
1631.531067	120192.852665	36.971700
1633.599916	120365.080519	36.976717
1635.071112	120529.423440	36.981735
1636.841132	120688.925688	36.986752
1638.573145	120845.149128	36.991770
1640.270970	121012.439777	36.996788
1641.952372	121164.752741	37.001805
1643.134319	121335.613446	37.006823
1644.522735	121495.799977	37.011840
1646.194095	121666.979202	37.016858
1647.130579	121839.909947	37.021876
1648.920382	121980.767183	37.026893
1650.841036	122140.201203	37.031911
1652.123044	122298.174974	37.036928
1654.161906	122458.391068	37.041946
1655.419331	122625.909406	37.046964
1657.019755	122785.230976	37.051981
1658.471008	122954.902452	37.056999
1659.690776	123121.046027	37.062016
1661.358614	123295.658017	37.067034
1662.894009	123479.069913	37.072052
1664.669170	123655.975588	37.077069
1666.050706	123835.417053	37.082087
1667.134252	124035.659840	37.087104
1668.915698	124222.500117	37.092122
1670.757576	124404.929812	37.097140
1672.961467	124599.419203	37.102157
1674.876324	124789.907641	37.107175
1676.403304	124972.262065	37.112192
1678.016619	125157.902305	37.117210
1679.287825	125360.279154	37.122228
1681.032648	125561.086309	37.127245
1682.645990	125750.205332	37.132263
1683.963247	125966.621936	37.137280
1685.549645	126171.300778	37.142298
1687.027383	126388.925246	37.147316
1689.026646	126595.026291	37.152333
1690.862336	126828.608012	37.157351
1692.006554	127034.159257	37.162368
1693.971170	127247.995261	37.167386
1695.852664	127456.478722	37.172404
1697.709657	127667.428334	37.177421
1700.041452	127878.000633	37.182439
1701.624919	128088.817341	37.187456
1703.790181	128287.542452	37.192474
1705.694128	128500.912250	37.197492
1707.792926	128700.690032	37.202509
1709.452249	128891.897041	37.207527
1711.372155	129093.303153	37.212544
1713.017485	129281.938561	37.217562
1714.349854	129490.137031	37.222580
1715.974454	129698.291045	37.227597
1717.582207	129911.270037	37.232615
1719.183834	130117.983291	37.237632
1721.173860	130322.543608	37.242650
1722.489755	130536.205550	37.247668
1724.554512	130751.388757	37.252685
1726.095352	130962.480228	37.257703
1728.119704	131154.173529	37.262720
1730.174849	131353.767606	37.267738
1732.089094	131562.177464	37.272756
1734.233758	131756.646130	37.277773
1736.239126	131957.151616	37.282791
1737.262397	132159.739516	37.287808
1738.799661	132360.078641	37.292826
1740.245910	132572.524992	37.297844
1742.242420	132784.835983	37.302861
1743.632235	132986.406348	37.307879
1745.017638	133203.724979	37.312896
1746.530704	133413.766855	37.317914
1747.899893	133641.558389	37.322932
1749.487631	133875.712276	37.327949
1751.047551	134104.707334	37.332967
1752.579361	134333.010053	37.337984
1754.323289	134562.867066	37.343002
1756.172757	134805.994367	37.348020
1758.319243	135027.568558	37.353037
1760.096139	135252.424442	37.358055
1761.616944	135467.512457	37.363072
1763.484091	135676.291728	37.368090
1765.644052	135880.140957	37.373108
1767.728701	136087.987331	37.378125
1769.363055	136293.963239	37.383143
1771.038335	136508.283480	37.388160
1772.696549	136705.857013	37.393178
1774.212817	136927.640124	37.398196
1775.798473	137140.962107	37.403213
1777.277425	137365.811388	37.408231
1778.722189	137597.798825	37.413248
1780.977573	137820.829037	37.418266
1782.443304	138050.632809	37.423284
1784.011173	138286.728808	37.428301
1785.600501	138523.076471	37.433319
1787.477258	138766.614033	37.438336
1789.528431	138996.597856	37.443354
1791.142805	139249.391929	37.448372
1793.092768	139489.013220	37.453389
1794.986219	139726.068354	37.458407
1796.366583	139975.818953	37.463424
1798.646649	140211.179264	37.468442
1800.961549	140448.984623	37.473460
1803.053688	140683.196284	37.478477
1804.685394	140919.257468	37.483495
1806.523731	141155.452637	37.488512
1808.535540	141389.934074	37.493530
1810.274687	141633.000134	37.498548
1812.011565	141878.910570	37.503565
1814.000821	142120.645665	37.508583
1815.353109	142380.236084	37.513600
1816.776351	142622.645559	37.518618
1819.317577	142862.635872	37.523636
1820.871337	143117.223847	37.528653
1823.143971	143355.100834	37.533671
1824.942864	143606.683387	37.538688
1826.945379	143857.131362	37.543706
1828.800165	144097.983326	37.548724
1830.867634	144341.595529	37.553741
1832.983557	144580.264283	37.558759
1834.795891	144828.893742	37.563776
1836.765936	145056.456735	37.568794
1838.523506	145299.461846	37.573812
1840.002471	145533.068635	37.578829
1842.162748	145779.909823	37.583847
1843.872689	146036.277935	37.588864
1845.258457	146284.600170	37.593882
1846.830818	146534.798407	37.598900
1848.780665	146800.855279	37.603917
1850.498422	147049.484930	37.608935
1851.669977	147315.462508	37.613952
1853.549582	147571.481865	37.618970
1855.602601	147844.547003	37.623988
1856.951185	148118.649769	37.629005
1858.910207	148393.763227	37.634023
1860.650668	148671.412619	37.639040
1862.673086	148945.846379	37.644058
1864.246635	149227.205591	37.649076
1865.625776	149503.773219	37.654093
1867.807084	149785.116949	37.659111
1869.155618	150079.792599	37.664128
1871.590011	150358.764418	37.669146
1873.747665	150641.372938	37.674164
1875.705155	150931.998178	37.679181
1877.730318	151212.066244	37.684199
1879.380453	151509.723758	37.689216
1881.323646	151778.129515	37.694234
1883.624833	152055.772559	37.699252
1884.929375	152316.080288	37.704269
1887.070038	152573.847311	37.709287
1888.347357	152845.052945	37.714304
1890.391888	153100.476330	37.719322
1891.962590	153375.497795	37.724340
1893.455095	153644.198504	37.729357
1895.637052	153917.134535	37.734375
1897.928807	154194.573878	37.739392
1899.628314	154462.065705	37.744410
1901.432064	154743.861592	37.749428
1903.298635	155023.948060	37.754445
1904.954727	155300.666579	37.759463
1906.870128	155597.999793	37.764480
1909.131871	155865.372562	37.769498
1912.482257	156126.204501	37.774516
1914.925181	156379.752537	37.779533
1917.725491	156626.632168	37.784551
1920.191139	156859.905489	37.789568
1922.451249	157094.595442	37.794586
1924.826304	157343.816610	37.799604
1926.130427	157590.882349	37.804621
1927.764716	157832.603975	37.809639
1929.227888	158094.931640	37.814656
1931.171141	158334.474459	37.819674
1932.599986	158597.723693	37.824692
1933.938678	158866.865915	37.829709
1935.798799	159139.355858	37.834727
1936.959750	159412.996837	37.839744
1938.908575	159689.055463	37.844762
1940.459167	159980.094273	37.849780
1942.297281	160269.528176	37.854797
1944.454055	160552.959686	37.859815
1946.327765	160845.983531	37.864832
1948.197241	161147.083762	37.869850
1950.280283	161436.916598	37.874868
1952.104987	161737.391834	37.879885
1953.725860	162039.233264	37.884903
1955.652757	162347.414465	37.889920
1957.298229	162671.371082	37.894938
1959.299710	162980.737119	37.899956
1961.248424	163289.884317	37.904973
1963.356423	163609.990247	37.909991
1965.547542	163921.527650	37.915008
1967.513520	164237.303990	37.920026
1969.144032	164562.897424	37.925044
1970.791261	164878.409020	37.930061
1973.158509	165205.808070	37.935079
1975.232976	165537.977337	37.940096
1978.657963	165807.420776	37.945114
1981.305297	166103.890174	37.950132
1982.939663	166422.458148	37.955149
1985.378557	166723.914330	37.960167
1986.888169	167024.729266	37.965184
1988.406540	167329.645183	37.970202
1990.575842	167630.994911	37.975220
1992.104333	167948.126250	37.980237
1994.222067	168245.588717	37.985255
1996.156886	168567.293962	37.990272
1998.030650	168869.482187	37.995290
2000.316813	169183.530034	38.000308
2001.882453	169490.022338	38.005325
2003.657075	169806.615750	38.010343
2005.327784	170129.359465	38.015360
2007.531884	170459.563772	38.020378
2009.122689	170784.100422	38.025396
2010.934069	171113.708514	38.030413
2012.973674	171431.372349	38.035431
2014.788658	171768.106032	38.040448
2016.602138	172072.894422	38.045466
2018.585561	172402.405209	38.050484
2019.865115	172724.167117	38.055501
2021.728844	173044.328430	38.060519
2023.659981	173379.603613	38.065536
2025.559283	173710.771106	38.070554
2027.351798	174046.908790	38.075572
2029.429918	174385.974775	38.080589
2031.924190	174727.377364	38.085607
2033.944064	175049.554240	38.090624
2035.592013	175404.564045	38.095642
2037.767486	175756.902890	38.100660
2039.615577	176105.256187	38.105677
2041.532887	176449.562148	38.110695
2043.507647	176814.228682	38.115712
2045.467956	177181.489531	38.120730
2047.565931	177546.495644	38.125748
2049.579198	177916.799083	38.130765
2051.707576	178272.076564	38.135783
2053.904428	178639.941851	38.140800
2056.118158	179014.714133	38.145818
2058.364964	179378.689000	38.150836
2060.757721	179759.303408	38.155853
2062.497084	180122.522205	38.160871
2064.881528	180494.378893	38.165888
2066.844072	180862.391521	38.170906
2069.183623	181240.760107	38.175924
2071.873609	181599.265282	38.180941
2074.084650	181958.684528	38.185959
2076.757040	182315.366556	38.190976
2079.070318	182663.140236	38.195994
2081.333843	183013.691365	38.201012
2083.219373	183377.509821	38.206029
2085.635736	183733.602072	38.211047
2087.648167	184093.034925	38.216064
2089.301179	184458.798533	38.221082
2091.525793	184806.187366	38.226100
2093.444649	185158.882581	38.231117
2095.881625	185526.306037	38.236135
2097.967882	185894.750578	38.241152
2099.483330	186263.590076	38.246170
2101.943938	186627.127740	38.251188
2103.505360	187000.890176	38.256205
2105.767353	187446.730275	38.261223
2107.953655	187805.895197	38.266240
2109.623640	188192.547929	38.271258
2111.837937	188574.900968	38.276276
2114.123149	188942.537793	38.281293
2116.249592	189314.010541	38.286311
2118.035635	189692.141509	38.291328
2120.316895	190066.107256	38.296346
2123.146301	190437.702908	38.301364
2125.501575	190814.606005	38.306381
2127.760601	191183.524191	38.311399
2130.082129	191559.317325	38.316416
2131.940389	191938.511213	38.321434
2133.838957	192291.588216	38.326452
2135.559079	192674.844607	38.331469
2137.339433	193043.563592	38.336487
2139.113850	193431.106603	38.341504
2140.900319	193832.187614	38.346522
2142.705175	194227.653409	38.351540
2145.016885	194628.223353	38.356557
2147.497251	195029.555713	38.361575
2149.389926	195428.466033	38.366592
2150.765538	195832.360460	38.371610
2153.200868	196228.394551	38.376628
2155.364180	196627.342479	38.381645
2157.438537	197017.516471	38.386663
2159.392847	197398.413247	38.391680
2161.633423	197793.847027	38.396698
2163.853813	198173.510562	38.401716
2165.920458	198561.581590	38.406733
2168.149822	198956.258184	38.411751
2170.091151	199338.279678	38.416768
2171.933665	199748.945522	38.421786
2174.397488	200161.624121	38.426804
2175.846728	200561.328805	38.431821
2177.976119	200966.415496	38.436839
2180.345988	201379.111836	38.441856
2182.124829	201800.182327	38.446874
2184.640169	202220.783611	38.451892
2186.486963	202649.136094	38.456909
2188.681759	203085.361036	38.461927
2190.699596	203509.370557	38.466944
2192.606680	203959.512173	38.471962
2195.300795	204389.921539	38.476980
2197.329954	204846.346140	38.481997
2199.294841	205286.955887	38.487015
2201.999758	205732.277982	38.492032
2203.778221	206178.761356	38.497050
2206.462377	206629.423241	38.502068
2209.702573	207072.810501	38.507085
2211.734094	207506.250956	38.512103
2214.136641	207934.045834	38.517120
2216.883913	208377.690237	38.522138
2219.158344	208818.411495	38.527156
2221.360910	209248.551599	38.532173
2223.498819	209683.529144	38.537191
2225.753817	210116.583969	38.542208
2227.650224	210564.632505	38.547226
2229.915738	211009.194891	38.552244
2232.155880	211455.260750	38.557261
2234.916834	211885.064238	38.562279
2237.659388	212321.044281	38.567296
2239.796225	212765.045133	38.572314
2242.050924	213206.462513	38.577332
2244.203751	213649.293553	38.582349
2246.416419	214080.176145	38.587367
2249.012643	214514.657716	38.592384
2251.071552	214964.719707	38.597402
2253.449604	215401.471812	38.602420
2255.216679	215829.834628	38.607437
2257.545790	216291.922900	38.612455
2259.880973	216735.440524	38.617472
2262.385400	217187.391737	38.622490
2264.794507	217629.806359	38.627508
2267.271561	218063.548071	38.632525
2269.599108	218504.858377	38.637543
2271.599476	218949.217620	38.642560
2273.603634	219396.421853	38.647578
2276.409473	219839.360792	38.652596
2278.549014	220285.807853	38.657613
2280.790682	220733.077626	38.662631
2283.675061	221151.947541	38.667648
2285.725588	221595.360712	38.672666
2288.104408	222038.418151	38.677684
2290.141619	222486.940005	38.682701
2292.208620	222927.836168	38.687719
2294.330629	223376.421348	38.692736
2296.715774	223820.469179	38.697754
2298.403530	224277.276879	38.702772
2300.376655	224725.301242	38.707789
2302.229147	225196.182720	38.712807
2304.557699	225655.863153	38.717824
2306.696282	226129.570821	38.722842
2308.712866	226577.385284	38.727860
2310.953439	227023.716822	38.732877
2313.260143	227468.056494	38.737895
2315.552802	227925.405167	38.742912
2317.691784	228382.574421	38.747930
2319.766265	228842.471820	38.752948
2322.422658	229296.308553	38.757965
2324.381586	229772.837859	38.762983
2327.047160	230227.917584	38.768000
2328.741787	230704.462173	38.773018
2331.113906	231178.081214	38.778036
2333.914152	231652.598689	38.783053
2336.525960	232109.489408	38.788071
2339.409905	232573.831626	38.793088
2341.752564	233047.809611	38.798106
2343.554805	233528.349304	38.803124
2346.035766	233995.826954	38.808141
2347.967087	234483.534976	38.813159
2350.970252	234959.466137	38.818176
2353.748484	235422.806104	38.823194
2356.059375	235910.072456	38.828212
2358.629256	236386.120269	38.833229
2360.812658	236866.698700	38.838247
2363.550641	237353.287090	38.843264
2365.922036	237820.625088	38.848282
2368.421577	238303.921383	38.853300
2370.817220	238782.609685	38.858317
2372.880410	239261.145773	38.863335
2375.209263	239752.366923	38.868352
2377.724153	240241.576833	38.873370
2380.211689	240734.067200	38.878388
2382.434981	241220.653420	38.883405
2384.467065	241727.921408	38.888423
2386.498292	242220.505442	38.893440
2388.955987	242736.139066	38.898458
2391.063298	243247.609197	38.903476
2393.727929	243758.051569	38.908493
2396.134225	244266.754791	38.913511
2398.606343	244772.855501	38.918528
2400.846087	245289.762032	38.923546
2403.352754	245802.637505	38.928564
2405.871654	246316.221070	38.933581
2407.885405	246834.302006	38.938599
2410.812320	247352.620496	38.943616
2412.888695	247884.939755	38.948634
2415.435291	248415.685563	38.953652
2418.450797	248928.041679	38.958669
2420.380850	249459.718626	38.963687
2423.235923	249979.285506	38.968704
2424.912514	250513.284837	38.973722
2427.257940	251043.723673	38.978740
2429.983199	251568.614823	38.983757
2432.336956	252097.245340	38.988775
2435.342809	252611.725343	38.993792
2437.927400	253142.018284	38.998810
2440.923021	253657.232977	39.003828
2443.832570	254166.337470	39.008845
2445.826859	254674.007710	39.013863
2448.967504	255174.766354	39.018880
2451.436667	255690.411278	39.023898
2454.095707	256209.072861	39.028916
2456.718405	256706.985367	39.033933
2458.659096	257215.645178	39.038951
2461.034534	257722.457281	39.043968
2463.554351	258239.303649	39.048986
2465.653827	258742.268308	39.054004
2468.284899	259257.543716	39.059021
2470.195937	259774.681644	39.064039
2472.627948	260268.240887	39.069056
2474.724857	260757.506774	39.074074
2477.789897	261232.091030	39.079092
2480.589125	261701.507680	39.084109
2483.160509	262186.782057	39.089127
2485.703385	262659.003231	39.094144
2488.156283	263144.114092	39.099162
2490.492570	263633.025503	39.104180
2493.200309	264112.606060	39.109197
2495.041990	264604.460175	39.114215
2497.610680	265096.402053	39.119232
2500.087462	265598.160000	39.124250
2501.950466	266108.138720	39.129268
2504.497054	266622.834297	39.134285
2506.792109	267124.485987	39.139303
2509.348752	267637.396840	39.144320
2511.837407	268154.709532	39.149338
2514.117777	268676.394996	39.154356
2516.809694	269199.588254	39.159373
2519.091274	269735.439936	39.164391
2521.161050	270281.810860	39.169408
2523.379060	270824.523582	39.174426
2525.536395	271372.576016	39.179444
2528.395516	271931.563808	39.184461
2530.936833	272489.607036	39.189479
2533.265570	273045.851195	39.194496
2536.111158	273609.630453	39.199514
2538.384928	274178.929908	39.204532
2541.187987	274742.174942	39.209549
2543.599938	275326.302179	39.214567
2546.038312	275896.630967	39.219584
2549.093178	276475.392937	39.224602
2551.914836	277046.822218	39.229620
2554.222723	277621.933561	39.234637
2556.651348	278204.259667	39.239655
2558.951051	278782.004922	39.244672
2561.711909	279375.723860	39.249690
2563.966947	279958.901780	39.254708
2566.502681	280549.929301	39.259725
2568.786456	281156.329697	39.264743
2571.478584	281757.862026	39.269760
2574.317671	282367.924372	39.274778
2576.360745	282980.289325	39.279796
2579.096773	283585.227796	39.284813
2581.449041	284207.463022	39.289831
2584.035961	284817.061120	39.294848
2586.629263	285438.232105	39.299866
2588.678879	286069.004384	39.304884
2591.295664	286710.931458	39.309901
2594.219854	287330.789375	39.314919
2596.768003	287950.725419	39.319936
2599.714130	288584.076774	39.324954
2602.384049	289215.382836	39.329972
2605.957895	289834.328785	39.334989
2608.951072	290442.339336	39.340007
2611.774980	291056.235677	39.345024
2614.530356	291661.706968	39.350042
2616.775470	292286.040651	39.355060
2619.445894	292902.989445	39.360077
2622.432091	293506.350038	39.365095
2624.828902	294114.341062	39.370112
2627.278431	294725.288256	39.375130
2629.571113	295348.414942	39.380148
2632.459891	295946.764305	39.385165
2634.819181	296563.342749	39.390183
2637.397454	297197.880832	39.395200
2640.550508	297803.532419	39.400218
2642.926788	298410.618582	39.405236
2645.961159	298990.355014	39.410253
2648.779544	299571.413781	39.415271
2651.328076	300140.170381	39.420288
2653.720815	300720.699376	39.425306
2656.301251	301300.329840	39.430324
2659.035074	301872.288990	39.435341
2662.279542	302456.220870	39.440359
2664.784293	303032.315768	39.445376
2667.070699	303607.448340	39.450394
2669.404127	304206.479995	39.455412
2672.021627	304786.117379	39.460429
2674.669225	305387.117290	39.465447
2677.202910	305988.914794	39.470464
2679.553192	306589.185311	39.475482
2681.487770	307200.022177	39.480500
2684.316362	307820.738855	39.485517
2686.619225	308450.159793	39.490535
2689.230133	309097.241812	39.495552
2692.051173	309728.977094	39.500570
2694.413711	310377.959073	39.505588
2696.913099	311024.652069	39.510605
2699.922047	311668.338195	39.515623
2702.768902	312310.340307	39.520640
2705.669810	312965.700807	39.525658
2708.104930	313631.149783	39.530676
2710.908375	314295.212160	39.535693
2713.745312	314952.204278	39.540711
2716.623563	315615.093858	39.545728
2719.472769	316284.145307	39.550746
2721.747480	316955.204981	39.555764
2724.246263	317602.161441	39.560781
2727.120567	318298.434776	39.565799
2729.709171	318996.543355	39.570816
2732.753268	319661.224874	39.575834
2735.599260	320350.237605	39.580852
2738.675414	321030.778700	39.585869
2741.190198	321719.059753	39.590887
2743.802387	322410.308774	39.595904
2747.126150	323091.920224	39.600922
2749.847905	323789.676202	39.605940
2752.808570	324469.291732	39.610957
2756.221227	325153.824318	39.615975
2758.755193	325838.938938	39.620992
2761.808815	326515.918058	39.626010
2764.717790	327198.718596	39.631028
2767.585654	327864.971552	39.636045
2771.103265	328537.023802	39.641063
2773.945385	329206.404356	39.646080
2777.223245	329868.196075	39.651098
2780.172864	330520.513922	39.656116
2783.263227	331181.120168	39.661133
2786.622828	331822.874661	39.666151
2789.145072	332466.397715	39.671168
2791.938811	333121.232697	39.676186
2794.816054	333773.075346	39.681204
2797.694063	334411.335025	39.686221
2800.512537	335053.398164	39.691239
2803.270324	335707.635656	39.696256
2805.559022	336355.542334	39.701274
2808.161026	337006.635676	39.706292
2810.914090	337665.354242	39.711309
2813.393339	338318.371063	39.716327
2816.043966	338990.423404	39.721344
2818.655191	339644.207362	39.726362
2821.268595	340316.266029	39.731380
2823.887097	340975.604395	39.736397
2826.486054	341645.484278	39.741415
2829.045233	342322.129223	39.746432
2831.721345	342963.642629	39.751450
2834.147825	343620.424994	39.756468
2836.543941	344268.602396	39.761485
2839.356951	344918.503263	39.766503
2841.963487	345591.906829	39.771520
2844.578557	346257.865533	39.776538
2846.771900	346933.614417	39.781556
2849.504292	347615.808197	39.786573
2852.527251	348310.393356	39.791591
2854.922783	349009.701953	39.796608
2857.748418	349710.424847	39.801626
2860.566897	350435.095183	39.806644
2863.133550	351148.125200	39.811661
2866.417099	351853.877966	39.816679
2869.347710	352579.294352	39.821696
2872.321089	353293.025036	39.826714
2875.660313	354009.243484	39.831732
2878.512860	354730.566639	39.836749
2881.947262	355457.106652	39.841767
2884.559593	356181.805720	39.846784
2887.511803	356910.617931	39.851802
2890.499321	357635.731767	39.856820
2893.052264	358377.069160	39.861837
2896.501348	359126.005941	39.866855
2898.805742	359864.760385	39.871872
2902.132467	360598.293575	39.876890
2905.314200	361347.698715	39.881908
2908.222684	362079.613316	39.886925
2911.597781	362820.029561	39.891943
2914.460889	363560.456314	39.896960
2917.952045	364297.243875	39.901978
2921.115201	365031.428223	39.906996
2923.730885	365757.544134	39.912013
2927.204652	366502.565976	39.917031
2929.920300	367244.189395	39.922048
2932.953376	367982.044456	39.927066
2936.744033	368706.433419	39.932084
2940.026996	369436.026943	39.937101
2943.077298	370162.343746	39.942119
2945.811046	370886.486605	39.947136
2948.991836	371616.774323	39.952154
2952.020974	372336.247456	39.957172
2953.880699	373077.825456	39.962189
2956.891270	373808.563326	39.967207
2960.128755	374545.656262	39.972224
2963.159923	375277.947828	39.977242
2966.335412	376020.330776	39.982260
2969.044248	376757.699310	39.987277
2972.234354	377497.100676	39.992295
2975.196575	378234.009229	39.997312
2978.109928	378970.651690	40.002330
2981.263586	379713.822199	40.007348
2983.819512	380454.481156	40.012365
2986.851076	381201.554756	40.017383
2989.661415	381950.135786	40.022400
2993.026634	382696.025504	40.027418
2996.024812	383447.674690	40.032436
2998.880846	384188.509821	40.037453
3001.804364	384935.998921	40.042471
3004.714431	385695.725304	40.047488
3007.576319	386441.634958	40.052506
3010.351577	387213.289631	40.057524
3013.153162	387970.584106	40.062541
3016.048275	388740.628473	40.067559
3018.450060	389511.865228	40.072576
3021.209412	390298.315578	40.077594
3024.094748	391082.974225	40.082612
3026.951104	391850.142658	40.087629
3029.491778	392615.715799	40.092647
3032.192285	393377.796888	40.097664
3035.518933	394126.896044	40.102682
3039.256483	394888.869316	40.107700
3042.005839	395668.185889	40.112717
3044.877647	396421.536932	40.117735
3047.717519	397194.562344	40.122752
3050.533651	397963.921275	40.127770
3054.041924	398732.590516	40.132788
3056.837744	399523.669005	40.137805
3059.738184	400308.832624	40.142823
3062.571839	401101.724482	40.147840
3065.341148	401893.991775	40.152858
3068.437973	402700.099518	40.157876
3071.414308	403511.916752	40.162893
3074.202521	404318.774587	40.167911
3076.910012	405142.114507	40.172928
3080.089873	405962.365145	40.177946
3083.669322	406792.239695	40.182964
3086.954734	407618.789457	40.187981
3090.566351	408440.197727	40.192999
3093.313696	409262.519627	40.198016
3097.131568	410093.852909	40.203034
3100.344097	410922.466204	40.208052
3103.560813	411755.853773	40.213069
3107.178865	412575.487414	40.218087
3110.380054	413395.003148	40.223104
3113.851951	414218.796116	40.228122
3117.313078	415039.068776	40.233140
3120.848737	415856.364534	40.238157
3124.530245	416658.381226	40.243175
3128.005156	417466.266928	40.248192
3131.199735	418280.639238	40.253210
3134.655038	419081.081718	40.258228
3137.543170	419886.487472	40.263245
3140.590831	420690.067260	40.268263
3143.512626	421500.462417	40.273280
3146.661834	422313.167078	40.278298
3149.737254	423121.502466	40.283316
3152.337283	423949.245817	40.288333
3155.542603	424763.007517	40.293351
3158.802880	425592.098170	40.298368
3161.870941	426424.268755	40.303386
3165.092867	427242.528837	40.308404
3168.026537	428086.481472	40.313421
3171.207540	428914.689100	40.318439
3173.995846	429766.277003	40.323456
3177.232379	430607.042609	40.328474
3180.045433	431462.344590	40.333492
3182.880391	432319.122186	40.338509
3185.914432	433168.907250	40.343527
3189.279153	434040.537268	40.348544
3192.155140	434905.078613	40.353562
3195.586452	435766.311220	40.358580
3199.007839	436629.275377	40.363597
3202.319927	437493.682975	40.368615
3205.373035	438369.460162	40.373632
3208.463888	439242.866956	40.378650
3212.144998	440101.439658	40.383668
3215.354851	440971.767085	40.388685
3218.893526	441833.869654	40.393703
3221.948802	442698.937499	40.398720
3225.463061	443566.671867	40.403738
3228.850034	444435.294558	40.408756
3231.905759	445305.897686	40.413773
3234.968645	446160.549214	40.418791
3238.149302	447039.686985	40.423808
3241.275491	447897.479541	40.428826
3244.566031	448744.853824	40.433844
3247.206769	449571.434665	40.438861
3250.113208	450407.429027	40.443879
3253.395408	451250.950139	40.448896
3256.103684	452091.390426	40.453914
3259.779779	452943.706700	40.458932
3262.875300	453789.711352	40.463949
3265.897500	454643.360099	40.468967
3269.550573	455501.260947	40.473984
3271.889601	456371.236769	40.479002
3275.556855	457244.495754	40.484020
3278.472976	458122.067382	40.489037
3281.509246	459003.764788	40.494055
3285.480817	459878.307238	40.499072
3288.813635	460764.511264	40.504090
3292.360976	461651.342496	40.509108
3295.334456	462544.322400	40.514125
3298.727732	463436.937769	40.519143
3302.044492	464344.452116	40.524160
3305.222485	465253.099562	40.529178
3308.735853	466152.010132	40.534196
3312.182414	467063.796713	40.539213
3315.434676	467977.329108	40.544231
3319.084735	468871.985828	40.549248
3322.489371	469784.537368	40.554266
3326.175122	470692.455543	40.559284
3330.074891	471608.207852	40.564301
3332.996741	472515.286488	40.569319
3336.537239	473435.833204	40.574336
3339.976615	474350.897760	40.579354
3343.720949	475265.005894	40.584372
3346.800429	476183.450998	40.589389
3350.309520	477102.129540	40.594407
3353.515903	478008.804504	40.599424
3356.472695	478943.342385	40.604442
3360.255652	479856.576834	40.609460
3363.639690	480794.517665	40.614477
3367.295921	481714.468483	40.619495
3370.096019	482640.142915	40.624512
3373.634141	483572.148376	40.629530
3377.802988	484504.201410	40.634548
3380.950289	485446.535564	40.639565
3383.914491	486375.891975	40.644583
3386.922479	487337.832372	40.649600
3390.245013	488273.668451	40.654618
3393.728202	489224.131617	40.659636
3397.018941	490182.927028	40.664653
3400.030689	491132.588499	40.669671
3403.682196	492083.500912	40.674688
3407.032716	493051.875673	40.679706
3410.102023	494022.497757	40.684724
3413.005681	494999.125169	40.689741
3417.071523	495963.272022	40.694759
3420.862210	496930.621267	40.699776
3423.969144	497909.139882	40.704794
3427.528206	498881.481967	40.709812
3430.637325	499860.222569	40.714829
3433.941513	500838.766522	40.719847
3437.774878	501826.775709	40.724864
3441.208871	502815.735899	40.729882
3444.635058	503789.984910	40.734900
3447.611344	504780.038965	40.739917
3451.372970	505763.310712	40.744935
3454.815962	506751.344211	40.749952
3458.461821	507734.095436	40.754970
3461.878174	508722.599612	40.759988
3465.140210	509716.139323	40.765005
3468.942555	510686.830915	40.770010
3472.375184	511622.185403	40.775015
3475.248768	512517.881539	40.780020
3478.465440	513352.257161	40.785024
3481.403034	514136.713357	40.790029
3484.040107	514888.805967	40.795034
3486.955263	515567.364631	40.800039
3489.450117	516191.311522	40.805044
3491.992804	516769.402449	40.810048
3494.356710	517291.496528	40.815053
3496.967918	517771.949266	40.820058
3498.814994	518185.519775	40.825063
3500.502380	518562.461323	40.830068
3502.403292	518899.846091	40.835072
3504.081860	519190.638662	40.840077
3505.553927	519438.921750	40.845082
3506.941201	519646.493026	40.850087
3507.969728	519826.298373	40.855092
3509.456513	519972.769049	40.860096
3510.642600	520095.800873	40.865101
3511.241428	520175.936332	40.870106
3512.508508	520229.510232	40.875111
3513.249982	520273.086840	40.880116
3514.327739	520267.224576	40.885120
3515.165009	520251.875187	40.890125
3515.470836	520218.113689	40.895130
3516.305634	520149.245440	40.900135
3516.585252	520079.757704	40.905140
3516.915940	519986.676628	40.910144
3517.376278	519883.898750	40.915149
3517.751305	519769.340656	40.920154
3518.276744	519647.198692	40.925159
3518.453968	519495.375476	40.930164
3518.638544	519341.936690	40.935168
3518.670115	519184.689705	40.940173
3518.826141	519016.787348	40.945178
3519.620525	518829.782907	40.950183
3519.127623	518648.016259	40.955188
3519.292249	518457.677485	40.960192
3519.327905	518264.332018	40.965197
3519.237391	518057.142748	40.970202
3519.794071	517848.085508	40.975207
3519.747734	517645.923461	40.980212
3519.804964	517422.521864	40.985216
3519.619689	517202.380323	40.990221
3519.660300	516988.652128	40.995226
3519.953796	516750.030436	41.000231
3519.637796	516522.538844	41.005236
3519.390503	516285.051796	41.010240
3519.485273	516064.243509	41.015245
3519.254947	515837.332160	41.020250
3519.413882	515598.156896	41.025255
3519.064827	515373.071192	41.030260
3519.294082	515137.254621	41.035264
3518.972091	514906.914117	41.040269
3519.013134	514676.614107	41.045274
3519.107092	514432.992250	41.050279
3518.752405	514199.973013	41.055284
3518.731830	513956.763932	41.060288
3518.516781	513730.723115	41.065293
3518.007921	513497.111029	41.070298
3518.160254	513258.047590	41.075303
3517.950379	513035.624898	41.080308
3517.905234	512804.903848	41.085312
3517.628668	512587.576969	41.090317
3517.377668	512355.771214	41.095322
3517.379087	512127.048627	41.100327
3516.982175	511899.947453	41.105332
3516.724797	511677.409623	41.110336
3516.652451	511466.185447	41.115341
3516.768854	511243.128702	41.120346
3516.792779	511029.613723	41.125351
3516.041159	510815.510169	41.130356
3516.147497	510602.984444	41.135360
3516.047926	510383.376845	41.140365
3515.653586	510183.429439	41.145370
3516.017709	509968.483732	41.150375
3515.337027	509760.001420	41.155380
3515.102302	509570.712198	41.160384
3515.079437	509367.871121	41.165389
3514.828201	509166.222665	41.170394
3514.907946	508966.738986	41.175399
3514.718373	508779.651283	41.180404
3514.573499	508581.710206	41.185408
3514.566801	508383.190042	41.190413
3514.372280	508207.746633	41.195418
3514.558413	508003.188976	41.200423
3514.124797	507820.716515	41.205428
3514.201878	507626.560958	41.210432
3513.962495	507436.991683	41.215437
3513.690631	507254.789417	41.220442
3513.855279	507075.745194	41.225447
3513.546608	506896.469714	41.230452
3513.474887	506704.947751	41.235456
3513.041471	506537.793626	41.240461
3513.212028	506353.039195	41.245466
3513.086037	506192.391010	41.250471
3512.747821	506009.375998	41.255476
3512.829567	505836.433075	41.260480
3512.675260	505672.201725	41.265485
3512.508263	505501.059104	41.270490
3512.595121	505330.984799	41.275495
3512.421691	505175.326956	41.280500
3512.375766	505005.521692	41.285504
3511.883635	504841.484724	41.290509
3511.643725	504682.653509	41.295514
3511.689587	504517.772357	41.300519
3511.347083	504373.887277	41.305524
3511.249358	504206.451849	41.310528
3511.401545	504068.036491	41.315533
3511.178501	503923.472421	41.320538
3511.081621	503761.329287	41.325543
3510.919978	503619.628487	41.330548
3511.073787	503457.897015	41.335552
3511.118621	503312.528300	41.340557
3510.668964	503166.528683	41.345562
3510.919907	503022.588198	41.350567
3510.535501	502888.331990	41.355572
3510.573291	502741.343991	41.360576
3510.731370	502606.849375	41.365581
3510.388071	502464.560002	41.370586
3510.440160	502326.496717	41.375591
3510.142102	502200.193200	41.380596
3510.199550	502058.392524	41.385600
3510.169691	501918.420623	41.390605
3509.672819	501784.827656	41.395610
3509.910149	501654.146888	41.400615
3509.710504	501527.368039	41.405620
3509.443304	501389.093201	41.410624
3509.526727	501270.392483	41.415629
3509.341510	501143.557574	41.420634
3509.343574	501013.916920	41.425639
3509.331246	500891.241383	41.430644
3508.965643	500765.642384	41.435648
3509.026710	500649.766088	41.440653
3508.963591	500533.554938	41.445658
3508.958466	500403.455778	41.450663
3508.541249	500299.056361	41.455668
3508.962141	500177.367185	41.460672
3508.857827	500076.349202	41.465677
3508.482518	499952.712912	41.470682
3508.937082	499827.381939	41.475687
3508.403075	499728.800397	41.480692
3508.674343	499609.653177	41.485696
3508.128760	499501.937116	41.490701
3508.258915	499390.128042	41.495706
3508.583003	499276.168214	41.500711
3508.202663	499173.067218	41.505716
3508.199898	499060.065029	41.510720
3508.327756	498961.577203	41.515725
3508.038480	498854.371668	41.520730
3508.216374	498744.821438	41.525735
3507.593769	498652.403941	41.530740
3507.968031	498531.465417	41.535744
3507.723754	498424.148791	41.540749
3507.759845	498331.172517	41.545754
3507.555248	498226.523332	41.550759
3507.461464	498146.335811	41.555764
3507.305291	498046.068997	41.560768
3507.004736	497936.990987	41.565773
3507.211674	497861.853011	41.570778
3507.345586	497756.491638	41.575783
3507.141268	497678.337759	41.580788
3506.843411	497587.427754	41.585792
3507.174619	497492.381241	41.590797
3506.929187	497405.701915	41.595802
3507.387269	497316.085932	41.600807
3506.974030	497224.686880	41.605812
3507.247615	497129.697475	41.610816
3506.989869	497034.487277	41.615821
3506.980349	496953.321083	41.620826
3506.995691	496861.701658	41.625831
3506.820439	496769.051283	41.630836
3506.553361	496681.159593	41.635840
3506.639034	496595.484035	41.640845
3506.902512	496516.342589	41.645850
3506.745589	496423.687197	41.650855
3506.758772	496340.747330	41.655860
3506.667400	496262.719820	41.660864
3506.926786	496169.947577	41.665869
3506.436770	496086.377866	41.670874
3506.581474	496009.170453	41.675879
3506.539523	495916.948327	41.680884
3506.692959	495837.113643	41.685888
3506.745102	495756.537068	41.690893
3506.626343	495672.200506	41.695898
3507.025599	495585.915014	41.700903
3506.522976	495498.759713	41.705908
3506.357668	495409.784512	41.710912
3506.498155	495331.413127	41.715917
3506.285649	495258.296042	41.720922
3506.460425	495167.196651	41.725927
3506.384303	495089.211082	41.730932
3506.014076	495013.896047	41.735936
3505.872990	494948.036040	41.740941
3505.738413	494871.774896	41.745946
3505.875485	494793.249754	41.750951
3505.975046	494722.555235	41.755956
3505.792604	494646.906209	41.760960
3505.986504	494574.277861	41.765965
3505.646785	494503.398232	41.770970
3505.724157	494434.321347	41.775975
3505.589571	494365.933449	41.780980
3505.850100	494286.578646	41.785984
3505.635694	494219.010281	41.790989
3505.640574	494155.294991	41.795994
3505.748186	494077.225048	41.800999
3505.688213	494005.340260	41.806004
3505.830419	493929.637079	41.811008
3505.734377	493860.079645	41.816013
3505.728505	493799.545259	41.821018
3505.656701	493721.652843	41.826023
3505.434940	493658.324123	41.831028
3505.523414	493584.495639	41.836032
3505.773562	493512.812670	41.841037
3505.412309	493457.078187	41.846042
3505.749789	493383.512901	41.851047
3505.571624	493318.509799	41.856052
3505.559406	493247.977168	41.861056
3505.628967	493174.452547	41.866061
3505.321603	493113.911814	41.871066
3505.437760	493035.330202	41.876071
3505.374367	492974.649960	41.881076
3505.529651	492903.332276	41.886080
3505.600608	492833.996546	41.891085
3505.505784	492771.603663	41.896090
3505.442417	492698.652804	41.901095
3505.293071	492638.842944	41.906100
3505.535683	492580.486623	41.911104
3505.563243	492508.934480	41.916109
3505.363663	492451.858293	41.921114
3505.532875	492382.353710	41.926119
3505.349022	492324.365717	41.931124
3505.138466	492249.971281	41.936128
3505.650819	492185.310259	41.941133
3505.436998	492128.790491	41.946138
3505.413955	492049.366988	41.951143
3505.290503	491985.763438	41.956148
3504.849926	491928.116832	41.961152
3505.108732	491860.060238	41.966157
3504.723954	491805.131197	41.971162
3505.039368	491741.660302	41.976167
3505.311476	491683.649382	41.981172
3504.991091	491618.610560	41.986176
3504.956826	491547.669417	41.991181
3504.846792	491501.735268	41.996186
3504.717204	491440.806659	42.001191
3505.089506	491381.365092	42.006196
3504.879709	491323.781254	42.011200
3505.040851	491265.180035	42.016205
3504.761217	491205.031275	42.021210
3505.178035	491140.330146	42.026215
3504.760723	491092.877155	42.031220
3504.646270	491033.964444	42.036224
3504.690815	490970.330468	42.041229
3504.739956	490919.320000	42.046234
3504.742092	490861.095443	42.051239
3504.613254	490810.011306	42.056244
3504.737537	490754.443741	42.061248
3504.819615	490691.661227	42.066253
3504.461955	490640.965618	42.071258
3504.353453	490587.605115	42.076263
3504.474888	490535.117630	42.081268
3504.287444	490479.951061	42.086272
3504.527921	490430.222155	42.091277
3504.136043	490385.136464	42.096282
3504.447090	490330.396776	42.101287
3504.477602	490279.993052	42.106292
3504.462151	490227.273301	42.111296
3504.555263	490176.455490	42.116301
3504.330165	490133.767117	42.121306
3504.513205	490078.490934	42.126311
3504.302521	490021.811291	42.131316
3504.463675	489967.548128	42.136320
3504.448736	489914.675709	42.141325
3504.832379	489863.963145	42.146330
3504.813692	489804.626738	42.151335
3504.437668	489767.970517	42.156340
3504.620752	489711.733459	42.161344
3504.586399	489657.550114	42.166349
3504.283432	489609.165640	42.171354
3504.662954	489553.604461	42.176359
3504.376621	489499.005240	42.181364
3504.264097	489443.217210	42.186368
3504.322317	489394.119308	42.191373
3504.168038	489354.649917	42.196378
3504.271606	489304.736620	42.201383
3504.510656	489256.115167	42.206388
3504.560808	489193.482936	42.211392
3504.273724	489147.367186	42.216397
3504.241183	489104.393436	42.221402
3504.030069	489045.084010	42.226407
3504.311347	489000.141973	42.231412
3504.183940	488954.051294	42.236416
3504.191001	488913.899094	42.241421
3503.960264	488868.531300	42.246426
3504.244677	488814.699389	42.251431
3504.327974	488768.676370	42.256436
3504.476911	488720.521778	42.261440
3504.039049	488667.054267	42.266445
3503.876654	488629.857004	42.271450
3504.156557	488573.701690	42.276455
3504.182152	488530.515253	42.281460
3504.499807	488480.010378	42.286464
3504.611253	488436.153736	42.291469
3503.954881	488385.143537	42.296474
3504.057889	488338.964636	42.301479
3503.917221	488290.601222	42.306484
3503.707160	488240.531220	42.311488
3504.178674	488191.213612	42.316493
3504.152219	488157.883084	42.321498
3504.286463	488105.082184	42.326503
3504.395681	488064.810840	42.331508
3504.302178	488011.994551	42.336512
3504.032927	487961.629802	42.341517
3503.827855	487919.033117	42.346522
3503.970944	487871.230314	42.351527
3504.031621	487824.197810	42.356532
3503.931310	487789.362725	42.361536
3504.175477	487732.250225	42.366541
3504.069838	487692.364896	42.371546
3504.021099	487642.520376	42.376551
3504.152348	487609.669201	42.381556
3503.809664	487565.678697	42.386560
3504.054638	487513.060561	42.391565
3504.024082	487473.971127	42.396570
3504.052140	487424.113946	42.401575
3503.903274	487371.203043	42.406580
3504.132803	487332.022265	42.411584
3504.179287	487288.071425	42.416589
3503.915572	487239.723837	42.421594
3504.095010	487182.922425	42.426599
3504.082983	487143.425183	42.431604
3504.043271	487105.194912	42.436608
3504.181568	487058.249001	42.441613
3503.742777	487016.241794	42.446618
3503.786959	486963.804553	42.451623
3503.640707	486929.227218	42.456628
3503.672242	486877.650341	42.461632
3503.767154	486842.429146	42.466637
3503.538365	486808.874612	42.471642
3503.928049	486759.161045	42.476647
3503.987684	486719.449515	42.481652
3503.865412	486676.179837	42.486656
3503.705277	486629.228544	42.491661
3503.472513	486589.663203	42.496666
3503.635225	486549.733145	42.501671
3503.711688	486512.139982	42.506676
3503.916882	486478.870782	42.511680
3503.877228	486431.799113	42.516685
3503.908223	486392.646836	42.521690
3503.704156	486343.680991	42.526695
3503.666590	486307.266872	42.531700
3503.276345	486265.906729	42.536704
3503.484090	486227.534742	42.541709
3503.656517	486198.715220	42.546714
3503.640966	486154.922335	42.551719
3503.746222	486116.464992	42.556724
3503.673772	486076.519788	42.561728
3503.838636	486029.667634	42.566733
3503.650453	485986.456789	42.571738
3503.901187	485947.622787	42.576743
3503.542333	485915.905063	42.581748
3503.238970	485874.429319	42.586752
3503.711367	485829.448256	42.591757
3503.663824	485793.792199	42.596762
3503.636270	485757.425739	42.601767
3504.058911	485720.332440	42.606772
3503.860959	485678.334615	42.611776
3503.817138	485639.596190	42.616781
3503.662379	485600.218231	42.621786
3503.583523	485558.252061	42.626791
3503.649312	485527.174676	42.631796
3503.621192	485477.976638	42.636800
3503.776731	485442.793327	42.641805
3503.368442	485413.961676	42.646810
3503.679207	485365.013640	42.651815
3503.671885	485323.086216	42.656820
3503.526159	485286.585487	42.661824
3503.806007	485235.772742	42.666829
3503.846679	485215.660761	42.671834
3503.879105	485159.683039	42.676839
3504.055157	485121.868925	42.681844
3503.871355	485083.858130	42.686848
3503.779226	485031.789152	42.691853
3503.759382	484996.581602	42.696858
3503.726344	484948.494029	42.701863
3503.614343	484911.734579	42.706868
3503.947496	484882.584487	42.711872
3504.099161	484831.588292	42.716877
3503.859200	484787.220235	42.721882
3504.131736	484733.577963	42.726887
3503.875727	484682.038494	42.731892
3503.860741	484657.185708	42.736896
3503.736213	484600.977798	42.741901
3503.615998	484564.067245	42.746906
3503.670952	484529.352182	42.751911
3503.718493	484482.412562	42.756916
3503.516950	484446.726845	42.761920
3503.689994	484411.437430	42.766925
3503.557260	484378.620454	42.771930
3503.915576	484331.429939	42.776935
3503.539789	484296.932944	42.781940
3503.453455	484256.833642	42.786945
3503.729050	484219.759636	42.791949
3503.530239	484185.588494	42.796954
3503.979548	484138.787396	42.801959
3503.774280	484093.098426	42.806964
3503.866546	484060.548887	42.811969
3503.723569	484017.679152	42.816973
3503.534891	483976.332034	42.821978
3503.773554	483936.332893	42.826983
3503.720410	483890.063923	42.831988
3503.563741	483855.380286	42.836993
3503.840905	483809.059675	42.841997
3503.464501	483777.542380	42.847002
3503.662945	483737.700552	42.852007
3503.676609	483697.432681	42.857012
3503.311890	483663.488294	42.862017
3503.359777	483621.092982	42.867021
3503.157075	483581.616310	42.872026
3503.035353	483548.593778	42.877031
3503.459532	483514.526304	42.882036
3503.280620	483493.789473	42.887041
3503.475436	483446.369106	42.892045
3503.483120	483418.934162	42.897050
3503.374033	483377.219408	42.902055
3503.375182	483334.931636	42.907060
3503.447446	483301.373165	42.912065
3503.500795	483264.634609	42.917069
3503.350582	483228.382353	42.922074
3503.650562	483201.002588	42.927079
3503.431181	483155.616200	42.932084
3503.489401	483121.352199	42.937089
3503.701734	483085.144239	42.942093
3503.528378	483049.804595	42.947098
3503.425174	482998.943100	42.952103
3503.482353	482969.377656	42.957108
3503.240329	482936.119927	42.962113
3503.418187	482902.544167	42.967117
3503.463567	482864.290180	42.972122
3503.301961	482818.540150	42.977127
3503.313492	482793.882359	42.982132
3503.051383	482758.909540	42.987137
3503.480684	482713.724072	42.992141
3503.524213	482687.899063	42.997146
3503.345661	482635.027107	43.002151
3503.454040	482611.263411	43.007156
3503.380851	482584.142736	43.012161
3503.668842	482537.109312	43.017165
3503.366113	482506.588489	43.022170
3503.404454	482467.576743	43.027175
3503.284858	482424.193728	43.032180
3503.516342	482401.168444	43.037185
3503.476679	482358.480172	43.042189
3503.641038	482328.341051	43.047194
3503.727355	482283.258240	43.052199
3503.685006	482245.066916	43.057204
3503.660086	482216.523353	43.062209
3503.348714	482167.510499	43.067213
3503.403319	482136.983876	43.072218
3503.485224	482095.488611	43.077223
3503.497386	482056.479914	43.082228
3503.543597	482032.270270	43.087233
3503.810980	481975.840323	43.092237
3503.551550	481945.109557	43.097242
3503.468021	481905.509047	43.102247
3503.272416	481864.056353	43.107252
3503.278290	481831.515612	43.112257
3503.456561	481788.387651	43.117261
3503.209050	481765.233859	43.122266
3503.422395	481727.001483	43.127271
3503.447716	481686.979257	43.132276
3503.407155	481653.940091	43.137281
3503.565372	481619.505656	43.142285
3503.450200	481589.964427	43.147290
3503.163167	481548.120898	43.152295
3503.537013	481507.387106	43.157300
3503.245527	481473.578147	43.162305
3503.457125	481431.858830	43.167309
3503.356477	481411.662875	43.172314
3503.458886	481372.790022	43.177319
3503.477155	481330.292052	43.182324
3503.226936	481292.484460	43.187329
3503.590408	481257.663586	43.192333
3503.293810	481229.716329	43.197338
3503.389879	481197.412887	43.202343
3503.527680	481154.946372	43.207348
3502.898215	481114.721401	43.212353
3503.440825	481081.135511	43.217357
3503.141348	481049.348088	43.222362
3503.134082	481016.908764	43.227367
3503.238375	480989.100817	43.232372
3503.487247	480951.366332	43.237377
3503.386287	480914.343093	43.242381
3502.892882	480883.848780	43.247386
3502.965926	480847.859455	43.252391
3503.490405	480813.012543	43.257396
3503.102323	480774.315599	43.262401
3503.471858	480746.567012	43.267405
3503.161746	480716.852352	43.272410
3503.061165	480679.070530	43.277415
3503.215318	480646.655857	43.282420
3503.124931	480609.428129	43.287425
3503.512305	480581.777539	43.292429
3503.104068	480551.976774	43.297434
3502.952125	480510.463183	43.302439
3503.454031	480480.621717	43.307444
3503.063109	480449.352632	43.312449
3503.235423	480415.519756	43.317453
3503.193657	480385.762713	43.322458
3503.354256	480357.035306	43.327463
3503.237267	480321.529143	43.332468
3503.101162	480286.733332	43.337473
3503.458384	480260.046993	43.342477
3503.301179	480228.185239	43.347482
3503.264212	480185.339044	43.352487
3503.212429	480154.673530	43.357492
3503.290140	480118.075415	43.362497
3503.384189	480076.724536	43.367501
3503.070832	480055.246072	43.372506
3503.071716	480017.851145	43.377511
3503.303878	479986.484182	43.382516
3503.276711	479949.346127	43.387521
3503.179101	479920.455971	43.392525
3503.046690	479885.254430	43.397530
3503.022988	479848.166131	43.402535
3503.292606	479817.803687	43.407540
3503.058083	479787.873376	43.412545
3503.195939	479752.275741	43.417549
3503.191277	479727.716729	43.422554
3503.294243	479687.727876	43.427559
3503.282167	479643.966717	43.432564
3503.040526	479619.545484	43.437569
3503.079535	479593.160212	43.442573
3503.309399	479566.391453	43.447578
3503.113591	479541.053335	43.452583
3502.961672	479505.601309	43.457588
3503.091241	479476.978202	43.462593
3503.352879	479433.780292	43.467597
3502.978694	479409.177217	43.472602
3502.854667	479369.425025	43.477607
3503.098609	479347.656734	43.482612
3502.999668	479322.303192	43.487617
3503.341474	479283.691155	43.492621
3502.851775	479247.533074	43.497626
3503.092192	479217.982602	43.502631
3502.871157	479186.381361	43.507636
3502.941700	479155.391656	43.512641
3503.080286	479124.441838	43.517645
3502.797162	479099.217674	43.522650
3503.029634	479064.614501	43.527655
3503.273378	479024.046164	43.532660
3502.827207	479003.799819	43.537665
3503.185363	478971.754263	43.542669
3503.143678	478948.816986	43.547674
3502.975225	478919.380120	43.552679
3503.323583	478881.625216	43.557684
3502.846236	478859.159901	43.562689
3503.225386	478827.009712	43.567693
3503.188541	478796.137091	43.572698
3503.160608	478769.255491	43.577703
3502.992544	478730.317150	43.582708
3502.890059	478711.179317	43.587713
3502.917906	478655.633918	43.592717
3503.143289	478633.463233	43.597722
3503.146802	478616.987304	43.602727
3503.063848	478577.984807	43.607732
3502.335671	478546.713899	43.612737
3502.960104	478519.629284	43.617741
3502.820441	478482.353681	43.622746
3503.128103	478465.779728	43.627751
3502.903925	478432.610779	43.632756
3502.703374	478414.144850	43.637761
3503.098938	478377.088944	43.642765
3503.397712	478352.985973	43.647770
3503.012124	478307.560928	43.652775
3503.265208	478279.725068	43.657780
3503.101526	478252.964797	43.662785
3502.990153	478226.297419	43.667789
3503.259681	478190.877951	43.672794
3503.229372	478152.169453	43.677799
3502.894141	478122.959222	43.682804
3502.847059	478105.580924	43.687809
3502.914925	478066.856942	43.692813
3502.907254	478041.335532	43.697818
3502.797171	478012.090061	43.702823
3502.953566	477970.825071	43.707828
3502.826636	477953.459032	43.712833
3502.918105	477923.373392	43.717837
3503.324504	477889.953566	43.722842
3503.084823	477859.868796	43.727847
3502.988667	477822.837580	43.732852
3503.081781	477792.953600	43.737857
3502.837583	477772.775335	43.742861
3502.824965	477741.442031	43.747866
3502.813202	477711.018268	43.752871
3502.703321	477681.367831	43.757876
3502.734445	477667.262051	43.762881
3502.989719	477630.681111	43.767885
3502.927433	477608.806472	43.772890
3502.909650	477579.950175	43.777895
3502.839298	477550.647133	43.782900
3502.562931	477525.874291	43.787905
3502.839831	477501.015314	43.792909
3502.906388	477475.380365	43.797914
3502.819100	477456.390282	43.802919
3502.591550	477415.133059	43.807924
3502.577006	477403.359077	43.812929
3502.831124	477369.961860	43.817933
3502.711823	477343.445865	43.822938
3502.716914	477318.578360	43.827943
3502.961076	477292.005719	43.832948
3502.923419	477265.375805	43.837953
3502.964843	477232.415737	43.842957
3502.888378	477205.741220	43.847962
3502.809886	477172.648061	43.852967
3502.568784	477141.045878	43.857972
3502.716140	477122.221054	43.862977
3502.919403	477100.658196	43.867981
3502.850558	477073.577929	43.872986
3502.639753	477043.335497	43.877991
3502.834614	477014.141829	43.882996
3502.991525	476992.788211	43.888001
3503.031219	476965.033809	43.893005
3502.900198	476933.161367	43.898010
3502.815965	476901.079408	43.903015
3503.151431	476882.123943	43.908020
3503.164477	476853.564798	43.913025
3502.970408	476820.387809	43.918029
3502.711493	476788.636069	43.923034
3502.584284	476755.246364	43.928039
3502.690908	476729.755616	43.933044
3502.576064	476715.267358	43.938049
3502.828153	476681.565756	43.943053
3502.772893	476658.728384	43.948058
3502.999719	476624.070252	43.953063
3502.908213	476603.917292	43.958068
3502.612088	476582.886347	43.963073
3502.895277	476551.555223	43.968077
3502.855237	476525.328804	43.973082
3502.626620	476498.424061	43.978087
3502.890180	476464.467494	43.983092
3502.744443	476444.575497	43.988097
3502.624567	476416.592251	43.993101
3502.849671	476394.974500	43.998106
3502.619841	476370.495893	44.003111
3502.950963	476337.539448	44.008116
3503.002958	476313.977260	44.013121
3502.633551	476282.443891	44.018125
3502.736781	476262.866744	44.023130
3502.769836	476236.173568	44.028135
3503.088705	476208.526050	44.033140
3502.863077	476193.094190	44.038145
3502.910906	476155.177428	44.043149
3503.185514	476122.684249	44.048154
3502.716400	476102.083959	44.053159
3503.039438	476062.607772	44.058164
3503.027972	476043.806398	44.063169
3502.837287	476006.482408	44.068173
3502.618574	475982.456396	44.073178
3502.440605	475943.260064	44.078183
3502.943865	475932.516447	44.083188
3502.701819	475911.526752	44.088193
3502.817951	475877.490793	44.093197
3502.501766	475867.784489	44.098202
3502.362467	475830.654281	44.103207
3502.890199	475804.995442	44.108212
3502.781439	475773.976529	44.113217
3502.666021	475744.929930	44.118221
3502.506002	475730.043434	44.123226
3502.686956	475711.211727	44.128231
3502.968204	475677.655124	44.133236
3502.817744	475657.611244	44.138241
3502.391265	475620.676881	44.143245
3502.674172	475592.528426	44.148250
3502.550994	475579.000842	44.153255
3502.781704	475545.300184	44.158260
3502.852851	475532.298347	44.163265
3502.595838	475510.703882	44.168269
3502.601201	475480.930342	44.173274
3502.862504	475463.703377	44.178279
3502.831717	475422.460952	44.183284
3502.581749	475402.482786	44.188289
3502.457112	475372.678726	44.193293
3502.300120	475350.866290	44.198298
3502.475154	475329.912028	44.203303
3502.804142	475306.456905	44.208308
3502.331852	475293.084503	44.213313
3502.673637	475261.489006	44.218317
3502.532542	475241.038760	44.223322
3502.496537	475211.978841	44.228327
3502.750890	475195.561453	44.233332
3502.875689	475170.368697	44.238337
3502.856165	475148.484046	44.243341
3502.876567	475121.790989	44.248346
3502.734508	475089.310015	44.253351
3502.720018	475067.828864	44.258356
3502.533833	475038.084312	44.263361
3502.322005	475021.233796	44.268365
3502.660641	474994.187711	44.273370
3502.726777	474970.267509	44.278375
3502.728479	474941.706730	44.283380
3502.531396	474919.798849	44.288385
3502.891842	474891.889854	44.293389
3502.596223	474866.357647	44.298394
3502.609970	474848.612501	44.303399
3502.442655	474819.521758	44.308404
3502.889070	474806.410389	44.313409
3503.051650	474774.589076	44.318413
3502.666489	474750.132172	44.323418
3502.620755	474727.442224	44.328423
3503.069510	474698.305945	44.333428
3502.752938	474664.941364	44.338433
3502.643437	474644.131591	44.343437
3502.620192	474612.237773	44.348442
3502.790695	474595.984477	44.353447
3502.792888	474557.717200	44.358452
3502.558011	474544.206128	44.363457
3502.495327	474513.531474	44.368461
3502.521373	474496.491741	44.373466
3502.494472	474479.763536	44.378471
3502.988676	474453.096747	44.383476
3502.630612	474427.674665	44.388481
3502.797649	474391.302290	44.393485
3502.643971	474369.841869	44.398490
3502.505834	474339.987450	44.403495
3502.293149	474311.762228	44.408500
3501.997442	474301.242964	44.413505
3502.244005	474286.443518	44.418509
3502.536234	474265.823502	44.423514
3502.544081	474248.533581	44.428519
3502.313980	474215.002958	44.433524
3502.318709	474196.095805	44.438529
3502.270572	474174.719806	44.443533
3502.774314	474156.897651	44.448538
3502.499224	474137.427347	44.453543
3502.654782	474113.542514	44.458548
3502.314990	474094.334987	44.463553
3502.805661	474075.604836	44.468557
3502.912449	474044.549054	44.473562
3502.687566	474018.903394	44.478567
3502.568557	474003.149527	44.483572
3502.830188	473985.263754	44.488577
3502.473082	473947.455366	44.493581
3502.468019	473916.720061	44.498586
3502.592125	473898.147853	44.503591
3502.392400	473879.777675	44.508596
3502.395725	473858.443803	44.513601
3502.299871	473836.518699	44.518605
3502.665387	473803.703389	44.523610
3502.504871	473790.685647	44.528615
3502.702076	473769.018168	44.533620
3503.023469	473742.427656	44.538625
3502.708735	473717.604354	44.543629
3502.622526	473681.623669	44.548634
3502.300578	473676.466759	44.553639
3502.409430	473633.428661	44.558644
3502.770636	473627.558784	44.563649
3502.747755	473602.790998	44.568653
3502.767305	473578.673772	44.573658
3502.107572	473554.510554	44.578663
3502.576157	473527.593461	44.583668
3502.382292	473496.633969	44.588673
3502.888759	473479.467853	44.593677
3502.730206	473454.670399	44.598682
3502.458819	473442.630162	44.603687
3502.559595	473417.488970	44.608692
3502.643343	473397.608055	44.613697
3502.652162	473369.650048	44.618701
3502.567732	473341.453731	44.623706
3502.698916	473328.794663	44.628711
3502.926144	473299.437572	44.633716
3502.703654	473277.733638	44.638721
3502.620762	473249.081927	44.643725
3502.906458	473223.203890	44.648730
3502.891854	473196.715327	44.653735
3502.900570	473161.982595	44.658740
3502.616570	473138.518614	44.663745
3502.705002	473110.143330	44.668749
3502.507494	473079.486941	44.673754
3502.459443	473065.793895	44.678759
3502.718405	473044.520284	44.683764
3502.496913	473019.074736	44.688769
3502.649562	472994.025929	44.693773
3502.776074	472964.532239	44.698778
3502.533666	472942.527621	44.703783
3502.591701	472916.482300	44.708788
3502.754982	472898.964529	44.713793
3502.770390	472870.044074	44.718797
3502.546337	472841.868617	44.723802
3502.235497	472825.840120	44.728807
3502.685751	472801.553606	44.733812
3502.530556	472776.147917	44.738817
3502.387983	472770.002232	44.743821
3502.421398	472736.478102	44.748826
3502.059220	472729.759897	44.753831
3502.152013	472690.917995	44.758836
3502.104570	472682.987991	44.763841
3502.197204	472663.660920	44.768845
3502.203407	472646.167321	44.773850
3502.637566	472634.876157	44.778855
3502.679170	472598.064273	44.783860
3502.495630	472584.846918	44.788865
3502.632231	472562.226680	44.793869
3502.966966	472535.126550	44.798874
3502.565319	472515.724548	44.803879
3502.519452	472488.936353	44.808884
3502.386973	472466.964543	44.813889
3502.264332	472439.278181	44.818893
3502.716328	472424.596747	44.823898
3502.485853	472405.774668	44.828903
3502.893195	472374.820599	44.833908
3502.560846	472348.582330	44.838913
3502.414954	472324.640663	44.843917
3502.233371	472295.294821	44.848922
3502.457517	472282.569916	44.853927
3502.737141	472251.382698	44.858932
3502.722903	472238.998203	44.863937
3502.630423	472205.088107	44.868941
3502.376671	472183.084226	44.873946
3502.278859	472163.331174	44.878951
3502.158270	472148.991386	44.883956
3502.241625	472121.171312	44.888961
3502.170139	472107.228314	44.893965
3502.181322	472099.845046	44.898970
3501.949465	472084.663022	44.903975
3502.372210	472054.312652	44.908980
3502.205890	472040.687706	44.913985
3502.379408	472022.762932	44.918989
3502.488047	472005.454941	44.923994
3502.508883	471981.385707	44.928999
3502.405883	471954.554967	44.934004
3502.451570	471931.391854	44.939009
3502.512595	471920.309940	44.944013
3502.737724	471895.147048	44.949018
3502.539021	471882.588751	44.954023
3503.067933	471850.199115	44.959028
3502.695209	471823.561809	44.964033
3502.654066	471796.923422	44.969037
3502.612664	471766.442507	44.974042
3502.382033	471750.552147	44.979047
3502.497345	471716.406462	44.984052
3502.330221	471698.281543	44.989057
3502.462037	471684.357107	44.994061
3502.588329	471656.175641	44.999066
3502.481278	471633.086433	45.004071
3502.822649	471618.017013	45.009076
3502.490015	471584.496919	45.014081
3502.497711	471564.018882	45.019085
3502.712863	471539.615399	45.024090
3502.690277	471526.473260	45.029095
3502.444902	471495.568538	45.034100
3502.419772	471471.809069	45.039105
3502.593948	471452.568998	45.044109
3502.720494	471427.370168	45.049114
3502.180364	471409.201851	45.054119
3502.415143	471380.446862	45.059124
3502.376015	471368.975674	45.064129
3502.744184	471347.430057	45.069133
3502.667402	471318.774003	45.074138
3502.481784	471308.842396	45.079143
3502.764369	471282.203355	45.084148
3502.386896	471251.976022	45.089153
3502.495220	471237.043640	45.094157
3502.543863	471197.497202	45.099162
3502.403483	471186.092203	45.104167
3502.383367	471160.157365	45.109172
3502.471634	471146.947109	45.114177
3502.289749	471121.694682	45.119181
3502.707071	471100.444461	45.124186
3502.293904	471077.907721	45.129191
3502.475617	471054.064898	45.134196
3502.452682	471032.023549	45.139201
3502.548662	471017.345696	45.144205
3502.669529	470987.798755	45.149210
3502.222779	470970.474971	45.154215
3502.429570	470943.594365	45.159220
3502.476966	470925.738580	45.164225
3502.358528	470907.099587	45.169229
3502.341138	470881.821193	45.174234
3502.493683	470870.067018	45.179239
3502.479138	470844.333062	45.184244
3502.397224	470825.941105	45.189249
3502.450537	470799.741458	45.194253
3502.336355	470780.444346	45.199258
3502.545931	470765.445216	45.204263
3502.257855	470735.304143	45.209268
3502.570034	470708.811255	45.214273
3502.445179	470696.897871	45.219277
3502.818284	470662.861565	45.224282
3502.431748	470649.016913	45.229287
3502.805362	470627.924572	45.234292
3502.796648	470602.745525	45.239297
3502.714280	470588.752363	45.244301
3502.829004	470547.929997	45.249306
3502.383578	470539.302434	45.254311
3502.450092	470497.172798	45.259316
3502.589195	470493.106088	45.264321
3502.329453	470456.032897	45.269325
3502.367688	470441.666898	45.274330
3502.259202	470422.317914	45.279335
3502.317411	470402.032820	45.284340
3502.450794	470377.994282	45.289345
3502.110584	470360.501582	45.294349
3502.096945	470339.064622	45.299354
3501.937435	470319.672894	45.304359
3502.547031	470303.043611	45.309364
3502.712325	470293.714114	45.314369
3502.533937	470262.341566	45.319373
3502.638111	470238.256805	45.324378
3502.415500	470223.779513	45.329383
3502.600757	470179.759708	45.334388
3502.590092	470171.569940	45.339393
3501.987146	470151.640244	45.344397
3502.351072	470128.981273	45.349402
3502.636150	470109.570678	45.354407
3502.529526	470098.715881	45.359412
3502.554439	470063.872920	45.364417
3502.421444	470044.679000	45.369421
3502.472502	470029.097089	45.374426
3502.311324	470013.042541	45.379431
3502.658318	469971.019606	45.384436
3502.659415	469960.249085	45.389441
3502.822815	469934.637711	45.394445
3502.347198	469907.861604	45.399450
3502.402903	469885.604219	45.404455
3502.722097	469866.895944	45.409460
3502.544293	469841.337521	45.414465
3502.386656	469825.181107	45.419469
3502.458921	469796.853162	45.424474
3502.263060	469789.956164	45.429479
3502.424399	469763.232400	45.434484
3502.204292	469747.237328	45.439489
3502.230980	469733.277034	45.444493
3502.657899	469705.045441	45.449498
3502.036198	469682.488667	45.454503
3502.065705	469661.145242	45.459508
3502.239143	469649.488077	45.464513
3502.150367	469623.005272	45.469517
3502.462037	469610.618643	45.474522
3502.459200	469595.499805	45.479527
3502.373478	469562.038287	45.484532
3502.351576	469547.529167	45.489537
3502.436989	469523.446281	45.494541
3502.391866	469503.024462	45.499546
3502.232211	469481.305708	45.504551
3501.888666	469473.976460	45.509556
3502.109312	469449.922989	45.514561
3502.037713	469427.482529	45.519565
3502.134946	469419.022764	45.524570
3502.045976	469397.292901	45.529575
3502.175751	469391.811500	45.534580
3502.002440	469379.955269	45.539585
3501.890812	469352.059712	45.544589
3502.153795	469333.207880	45.549594
3501.953350	469324.137017	45.554599
3501.820300	469307.672867	45.559604
3502.268639	469291.573334	45.564609
3501.814458	469289.115665	45.569613
3502.189639	469264.886176	45.574618
3502.289268	469247.273279	45.579623
3502.427799	469232.132109	45.584628
3502.164239	469219.278460	45.589633
3502.107590	469212.308989	45.594637
3502.186578	469187.114130	45.599642
3502.412559	469179.443287	45.604647
3502.419695	469166.193501	45.609652
3502.254322	469134.968483	45.614657
3501.909151	469123.037676	45.619661
3502.413875	469099.748573	45.624666
3502.132867	469080.778834	45.629671
3502.142779	469064.595602	45.634676
3502.235502	469043.342677	45.639681
3502.204944	469034.801466	45.644685
3502.103366	469015.601459	45.649690
3502.214389	468994.396192	45.654695
3502.178702	468976.045543	45.659700
3502.158544	468954.557229	45.664705
3502.232520	468942.004817	45.669709
3502.308448	468922.928785	45.674714
3502.121193	468910.164157	45.679719
3502.295921	468895.927277	45.684724
3502.248463	468865.340789	45.689729
3502.271510	468858.662178	45.694733
3502.068869	468833.915153	45.699738
3502.287379	468812.389516	45.704743
3502.145002	468797.999622	45.709748
3502.342808	468767.273650	45.714753
3502.156002	468752.738925	45.719757
3502.539266	468738.520028	45.724762
3502.435815	468716.083558	45.729767
3502.496226	468698.375043	45.734772
3502.807256	468675.924590	45.739777
3502.366276	468657.535517	45.744781
3502.737764	468630.220962	45.749786
3502.481153	468613.067379	45.754791
3502.509622	468586.817514	45.759796
3502.325059	468556.454068	45.764801
3502.509632	468537.360686	45.769805
3502.546291	468511.311705	45.774810
3502.662298	468497.589316	45.779815
3502.038904	468419.960719	45.784820
3502.326870	468299.660476	45.789825
3501.867718	468136.996310	45.794829
3501.802622	467934.014531	45.799834
3501.309911	467679.665103	45.804839
3500.882140	467377.459705	45.809844
3500.688076	467036.270504	45.814849
3499.695632	466642.701573	45.819853
3499.044172	466218.977316	45.824858
3498.384718	465733.589152	45.829863
3497.810177	465213.627942	45.834868
3496.947905	464650.499112	45.839873
3496.208959	464033.562548	45.844877
3495.264195	463385.019877	45.849882
3494.362218	462695.419653	45.854887
3493.272125	461961.504587	45.859892
3492.126469	461181.680081	45.864897
3491.281147	460374.452569	45.869901
3490.434912	459501.007125	45.874906
3488.715905	458602.809054	45.879911
3487.438626	457663.153900	45.884916
3485.987909	456681.270596	45.889921
3484.341310	455661.052523	45.894925
3483.048661	454612.631046	45.899930
3481.746072	453534.387795	45.904935
3479.795953	452388.454086	45.909940
3478.418383	451214.212511	45.914945
3476.614310	450017.078254	45.919949
3474.848462	448763.611483	45.924954
3472.649788	447500.809100	45.929959
3471.130966	446208.799737	45.934964
3469.150339	444874.690804	45.939969
3467.115840	443507.930907	45.944973
3465.313951	442097.377475	45.949978
3463.258328	440677.032164	45.954983
3461.057304	439225.652844	45.959988
3459.023052	437733.914249	45.964993
3456.403049	436218.643099	45.969997
3454.779543	434676.700523	45.975002
3452.176885	433108.591210	45.980007
3449.679526	431526.252022	45.985012
3447.305059	429904.085505	45.990017
3444.763259	428252.061771	45.995021
3442.425287	426582.382848	46.000026
3439.717579	424902.130062	46.005031
3437.052769	423192.886286	46.010036
3435.239526	421454.418272	46.015041
3432.186402	419705.602848	46.020045
3429.276880	417921.782389	46.025050
3426.665991	416133.910258	46.030055
3424.302264	414321.049138	46.035060
3421.514398	412480.914796	46.040065
3418.418617	410639.251936	46.045069
3415.746062	408749.277224	46.050074
3412.786078	406863.041630	46.055079
3409.910882	404956.490941	46.060084
3407.136556	403034.084548	46.065089
3404.134710	401086.331032	46.070093
3400.971096	399126.512236	46.075098
3398.190676	397166.977138	46.080103
3394.876405	395184.369005	46.085108
3391.868908	393191.802415	46.090113
3389.119617	391179.130980	46.095117
3385.706104	389152.181748	46.100122
3382.618512	387117.069998	46.105127
3379.958166	385065.553773	46.110132
3376.477881	382997.368295	46.115137
3372.985939	380927.393799	46.120141
3369.963813	378834.326113	46.125146
3366.610342	376742.338632	46.130151
3363.476789	374628.310348	46.135156
3360.406760	372513.803657	46.140161
3357.037515	370392.831149	46.145165
3353.830721	368254.880117	46.150170
3350.481834	366103.121701	46.155175
3346.936662	363947.448035	46.160180
3343.529862	361777.618701	46.165185
3339.907882	359605.073297	46.170189
3336.587881	357434.612995	46.175194
3332.955795	355246.917913	46.180199
3329.454006	353055.974656	46.185204
3326.039780	350856.580659	46.190209
3322.356386	348657.893437	46.195213
3318.739761	346443.541487	46.200218
3315.326018	344239.386215	46.205223
3311.748959	342019.502911	46.210228
3308.469873	339798.288335	46.215233
3304.509960	337575.770129	46.220237
3301.546309	335344.594344	46.225242
3297.638418	333118.670902	46.230247
3294.070437	330878.981976	46.235252
3289.922611	328629.639105	46.240257
3286.659284	326391.961150	46.245261
3283.138442	324137.893371	46.250266
3279.203131	321915.593341	46.255271
3275.040768	319652.658313	46.260276
3271.615300	317404.527520	46.265281
3268.109094	315161.206507	46.270285
3264.301996	312906.422523	46.275290
3260.328977	310657.815668	46.280295
3256.865933	308407.192042	46.285300
3253.280630	306155.568733	46.290305
3248.990163	303902.988222	46.295309
3245.511469	301638.960317	46.300314
3241.895201	299387.151987	46.305319
3238.046186	297134.932116	46.310324
3234.433753	294880.219544	46.315329
3230.413531	292635.437370	46.320333
3226.630310	290373.378428	46.325338
3222.664279	288133.923706	46.330343
3218.833261	285887.752378	46.335348
3214.795230	283637.694768	46.340353
3211.059067	281399.127978	46.345357
3207.214505	279163.284995	46.350362
3203.257842	276932.359017	46.355367
3199.149651	274692.890129	46.360372
3195.502881	272472.386110	46.365377
3191.467140	270250.485822	46.370381
3187.361825	268025.130524	46.375386
3183.668831	265825.429516	46.380391
3180.033054	263609.043801	46.385396
3176.052558	261394.270564	46.390401
3171.628751	259197.196690	46.395405
3167.825257	256998.153262	46.400410
3163.916686	254807.442245	46.405415
3160.080055	252616.762350	46.410420
3156.053337	250435.503382	46.415425
3151.900476	248249.880400	46.420429
3148.170595	246071.907542	46.425434
3144.198247	243914.960005	46.430439
3140.076588	241747.751345	46.435444
3136.096138	239589.187110	46.440449
3132.296254	237450.215358	46.445453
3127.979582	235298.474691	46.450458
3124.301347	233172.627633	46.455463
3120.222876	231049.075950	46.460468
3116.067007	228915.139123	46.465473
3112.097343	226810.382840	46.470477
3108.450210	224698.927813	46.475482
3103.898453	222607.913553	46.480487
3099.888424	220509.712527	46.485492
3096.110417	218426.482243	46.490497
3091.752824	216357.052158	46.495501
3087.892921	214304.873173	46.500506
3083.544762	212246.669538	46.505511
3079.431546	210198.452401	46.510516
3075.487737	208179.844286	46.515521
3071.470796	206156.273379	46.520525
3067.490452	204127.622898	46.525530
3063.404866	202119.944722	46.530535
3059.311787	200119.650998	46.535540
3055.062141	198128.982219	46.540545
3050.713170	196164.891616	46.545549
3046.654411	194181.964441	46.550554
3042.408641	192223.441830	46.555559
3037.969663	190287.823004	46.560564
3033.849534	188358.731516	46.565569
3029.725241	186449.511392	46.570573
3025.608487	184541.980308	46.575578
3021.234362	182650.822480	46.580583
3016.773046	180775.935738	46.585588
3012.552297	178911.795328	46.590593
3008.261104	177069.577314	46.595597
3003.964811	175236.935732	46.600602
2999.604090	173424.637761	46.605607
2995.124663	171621.184025	46.610612
2990.984260	169837.693482	46.615617
2985.794259	168081.306945	46.620621
2981.860755	166332.558619	46.625626
2977.357119	164611.615727	46.630631
2972.683185	162910.523590	46.635636
2967.854653	161219.657036	46.640641
2963.270697	159562.729682	46.645645
2958.534305	157928.232549	46.650650
2953.582984	156306.349370	46.655655
2948.614540	154729.451492	46.660660
2943.284030	153175.929685	46.665665
2938.309794	151659.071630	46.670669
2933.843997	150084.096506	46.675674
2928.425046	148615.342499	46.680679
2922.573673	147193.384283	46.685684
2916.758884	145823.884565	46.690689
2910.944502	144493.955761	46.695693
2905.367124	143193.913788	46.700698
2899.477760	141950.345509	46.705703
2893.532204	140741.285101	46.710708
2888.163473	139587.637509	46.715713
2882.398245	138471.687930	46.720717
2876.487791	137384.832774	46.725722
2871.408505	136354.105446	46.730727
2865.928588	135356.324166	46.735732
2861.344840	134394.949003	46.740737
2856.363533	133469.924732	46.745741
2851.519695	132572.782879	46.750746
2847.073956	131702.120237	46.755751
2842.563140	130853.160945	46.760756
2838.367350	130037.674559	46.765761
2834.012715	129239.286057	46.770765
2830.162796	128458.311089	46.775770
2826.150322	127703.578251	46.780775
2821.999703	126965.403021	46.785780
2818.188532	126229.134208	46.790785
2814.098643	125521.971916	46.795789
2810.408374	124824.985543	46.800794
2806.729149	124133.872693	46.805799
2802.874982	123453.812965	46.810804
2799.212349	122783.705967	46.815809
2795.445585	122117.759814	46.820813
2791.862700	121466.625031	46.825818
2788.197786	120820.638975	46.830823
2784.550948	120194.270724	46.835828
2781.104572	119541.697250	46.840833
2777.687393	118910.812375	46.845837
2773.983350	118275.862435	46.850842
2770.439770	117651.236534	46.855847
2766.893719	117040.380209	46.860852
2763.143850	116424.517358	46.865857
2759.414584	115830.163727	46.870861
2755.839878	115217.078391	46.875866
2752.037662	114635.966734	46.880871
2748.026103	114036.612598	46.885876
2744.264534	113448.380363	46.890881
2740.490695	112887.445266	46.895885
2736.486275	112316.879072	46.900890
2733.064383	111755.283865	46.905895
2729.215344	111202.701963	46.910900
2725.663770	110647.031042	46.915905
2721.865663	110114.520692	46.920909
2717.641239	109570.324776	46.925914
2714.172099	109035.275062	46.930919
2710.370788	108521.795820	46.935924
2706.481405	107995.218164	46.940929
2703.133301	107491.294649	46.945933
2699.429086	106974.314604	46.950938
2695.890233	106457.736142	46.955943
2691.904600	105961.803301	46.960948
2688.518493	105452.741934	46.965953
2685.341830	104961.858906	46.970957
2681.552750	104460.680261	46.975962
2677.995169	103958.773961	46.980967
2674.668408	103468.762405	46.985972
2671.027194	102963.261430	46.990977
2667.368707	102476.811685	46.995981
2664.326638	101986.714212	47.000986
2660.831824	101499.757730	47.005991
2657.033239	101005.534661	47.010996
2654.203553	100509.643103	47.016001
2651.052682	100025.654710	47.021005
2647.534641	99523.111018	47.026010
2643.982769	99021.482811	47.031015
2640.509454	98527.018265	47.036020
2637.246421	98028.982816	47.041025
2633.925280	97527.431137	47.046029
2630.515607	97011.133687	47.051034
2626.850940	96509.943909	47.056039
2623.421582	96010.695288	47.061044
2619.981358	95502.039640	47.066049
2616.813827	94995.205200	47.071053
2613.269647	94488.030998	47.076058
2609.782024	93981.631463	47.081063
2606.314485	93467.320516	47.086068
2603.087648	92943.234443	47.091073
2599.523743	92433.479545	47.096077
2595.788631	91916.351880	47.101082
2592.572268	91397.729189	47.106087
2589.424478	90881.861960	47.111092
2585.955281	90363.804636	47.116097
2582.723816	89850.547437	47.121101
2579.151465	89319.386535	47.126106
2575.813581	88791.730689	47.131111
2572.399649	88267.831353	47.136116
2569.056204	87733.309118	47.141121
2565.349689	87206.209051	47.146125
2561.937564	86667.791189	47.151130
2558.115637	86132.191124	47.156135
2554.701735	85605.404741	47.161140
2551.498375	85064.799010	47.166145
2547.697729	84533.938248	47.171149
2544.354519	84006.776249	47.176154
2540.934467	83467.618928	47.181159
2537.265149	82934.074375	47.186164
2533.893447	82392.224221	47.191169
2530.514190	81854.323304	47.196173
2527.135197	81317.753612	47.201178
2523.688921	80775.260227	47.206183
2519.760149	80238.784041	47.211188
2516.562742	79683.139801	47.216193
2512.828228	79143.809420	47.221197
2509.639577	78610.818478	47.226202
2506.311371	78061.526722	47.231207
2502.634829	77522.523851	47.236212
2499.779460	76964.684025	47.241217
2495.846421	76429.933629	47.246221
2492.430976	75873.803491	47.251226
2489.074179	75321.129841	47.256231
2485.641976	74767.958598	47.261236
2482.366496	74210.406008	47.266241
2478.573698	73662.748725	47.271245
2475.108809	73091.166423	47.276250
2471.715503	72537.514695	47.281255
2467.805904	71984.831035	47.286260
2464.635144	71415.880248	47.291265
2461.232738	70863.026939	47.296269
2457.855638	70300.468308	47.301274
2454.101437	69728.242257	47.306279
2450.285467	69178.625065	47.311284
2447.184502	68616.021842	47.316289
2443.670602	68058.611521	47.321293
2440.167519	67498.355134	47.326298
2436.753662	66930.264206	47.331303
2433.159839	66381.268941	47.336308
2429.704553	65807.369861	47.341313
2426.138669	65247.883644	47.346317
2422.523474	64674.809504	47.351322
2419.318337	64108.082249	47.356327
2416.065113	63543.082558	47.361332
2412.567118	62966.760666	47.366337
2409.227097	62408.172167	47.371341
2405.388954	61840.985694	47.376346
2402.167025	61262.902513	47.381351
2398.377564	60691.895471	47.386356
2395.123396	60123.889804	47.391361
2391.576832	59545.320132	47.396365
2388.014771	58970.123405	47.401370
2384.828290	58381.607285	47.406375
2381.348065	57820.810108	47.411380
2377.629699	57237.702915	47.416385
2374.287672	56659.246562	47.421389
2370.822217	56080.150844	47.426394
2367.189738	55493.519682	47.431399
2363.647324	54917.268540	47.436404
2360.453428	54335.768484	47.441409
2356.720885	53754.975613	47.446413
2353.201810	53171.911733	47.451418
2349.705259	52585.128660	47.456423
2346.210822	52019.402018	47.461428
2342.879758	51423.208370	47.466433
2339.303791	50839.126894	47.471437
2335.726732	50252.167830	47.476442
2332.620943	49666.698071	47.481447
2328.859103	49080.165549	47.486452
2325.605330	48492.611230	47.491457
2322.263297	47901.337317	47.496461
2318.534778	47307.551223	47.501466
2314.815789	46717.831885	47.506471
2311.544061	46128.109073	47.511476
2308.009519	45530.902088	47.516481
2304.161780	44948.542310	47.521485
2300.757535	44353.299692	47.526490
2296.939548	43763.324616	47.531495
2293.753663	43179.424168	47.536500
2290.436086	42594.164573	47.541505
2287.101010	41998.511474	47.546509
2283.428982	41406.744051	47.551514
2280.458331	40811.142522	47.556519
2276.762357	40222.891784	47.561524
2273.185768	39620.544081	47.566529
2269.879273	39017.777971	47.571533
2266.235293	38420.888468	47.576538
2262.661580	37812.770647	47.581543
2258.877149	37214.922080	47.586548
2255.584064	36618.363998	47.591553
2251.949974	36016.569783	47.596557
2248.595029	35426.970649	47.601562
2244.975282	34826.241147	47.606567
2241.638092	34237.794297	47.611572
2238.007042	33633.512819	47.616577
2234.578130	33034.623773	47.621581
2230.876490	32443.533061	47.626586
2227.622776	31840.759345	47.631591
2223.856572	31245.181056	47.636596
2220.504271	30646.570466	47.641601
2216.369126	30055.127129	47.646605
2213.039645	29463.150778	47.651610
2209.710284	28867.161130	47.656615
2205.976078	28281.986329	47.661620
2202.201748	27683.622699	47.666625
2198.786209	27100.073374	47.671629
2195.016862	26509.372557	47.676634
2191.629276	25928.678539	47.681639
2187.492747	25359.934186	47.686644
2183.764551	24775.778287	47.691649
2179.256424	24224.908186	47.696653
2174.991680	23685.697758	47.701658
2171.178838	23137.473629	47.706663
2166.862091	22611.230466	47.711668
2162.825971	22081.460752	47.716673
2158.864571	21575.702001	47.721677
2154.764918	21068.945196	47.726682
2151.611755	20568.863560	47.731687
2147.047946	20083.684184	47.736692
2143.303871	19603.956873	47.741697
2139.248103	19125.759305	47.746701
2135.616700	18656.627996	47.751706
2132.085484	18194.301009	47.756711
2128.208494	17748.410778	47.761716
2124.709958	17294.634465	47.766721
2120.870814	16853.914260	47.771725
2117.443457	16411.369969	47.776730
2113.829313	15964.435092	47.781735
2110.213296	15533.076709	47.786740
2106.491918	15092.144264	47.791745
2103.252987	14656.975898	47.796749
2099.647844	14235.023430	47.801754
2096.035543	13803.276109	47.806759
2092.191789	13386.366167	47.811764
2089.046204	12952.073932	47.816769
2085.285276	12542.144224	47.821773
2081.672639	12118.546291	47.826778
2078.419973	11700.881897	47.831783
2074.687156	11304.001684	47.836788
2071.446673	10885.163241	47.841793
2068.095248	10484.812688	47.846797
2064.592332	10082.740628	47.851802
2061.314014	9652.891442	47.856807
2057.653899	9257.192397	47.861812
2053.898728	8845.221938	47.866817
2049.928500	8448.309644	47.871821
2046.096933	8053.058620	47.876826
2042.242195	7656.680246	47.881831
2037.722554	7294.934160	47.886836
2033.193440	6923.337981	47.891841
2029.232053	6572.371698	47.896845
2025.211362	6235.846455	47.901850
2021.417260	5905.612099	47.906855
2017.345685	5591.525590	47.911860
2013.246845	5276.299975	47.916865
2009.221860	4974.562035	47.921869
2005.524631	4677.591322	47.926874
2001.514834	4397.306546	47.931879
1997.391124	4124.692234	47.936884
1993.964531	3843.524657	47.941889
1989.742262	3576.601330	47.946893
1986.197377	3317.607466	47.951898
1982.768334	3064.237957	47.956903
1979.068849	2825.583294	47.961908
1975.463775	2575.257207	47.966913
1971.894775	2334.282090	47.971917
1968.301174	2101.521621	47.976922
1964.803770	1858.697095	47.981927
1961.061294	1634.426463	47.986932
1957.775883	1399.766723	47.991937
1953.552914	1176.041721	47.996941
1949.819778	961.643131	48.001946
1946.871432	747.770398	48.006951
1943.188201	543.294002	48.011956
1939.250715	333.825993	48.016961
1934.761765	155.181816	48.021965
1926.362973	83.160371	48.026970
1915.766300	115.019887	48.031975
1909.076239	121.626086	48.036980
1905.141955	117.344146	48.041985
1902.872666	116.735571	48.046989
1900.289266	122.262871	48.051994
1898.496826	118.561897	48.056999
1895.589339	131.210543	48.062004
1892.958874	114.671926	48.067009
1890.066575	121.326129	48.072013
1886.363903	117.859183	48.077018
1883.365017	113.779673	48.082023
1879.685583	117.285101	48.087028
1876.190236	123.039754	48.092033
1873.208515	111.310877	48.097037
1869.675778	118.956921	48.102042
1866.566708	106.463268	48.107047
1863.322089	113.406416	48.112052
1860.146011	112.271430	48.117057
1856.632618	115.842765	48.122061
1852.678266	116.901140	48.127066
1849.171105	108.259575	48.132071
1845.662403	107.141559	48.137076
1842.383123	106.633234	48.142081
1839.522174	112.535918	48.147085
1836.017983	107.478380	48.152090
1832.940515	101.117419	48.157095
1829.292372	111.714182	48.162100
1825.810398	111.436718	48.167105
1822.419396	106.216034	48.172109
1818.605048	120.046673	48.177114
1815.215002	114.876458	48.182119
1811.702292	113.401568	48.187124
1808.292823	112.707867	48.192129
1805.403512	120.048130	48.197133
1801.863057	119.476054	48.202138
1798.538401	109.040740	48.207143
1795.126616	121.625497	48.212148
1791.140688	109.897907	48.217153
1788.154314	109.903975	48.222157
1784.283011	111.338566	48.227162
1780.820276	106.515025	48.232167
1776.979460	112.535415	48.237172
1773.635764	110.711527	48.242177
1770.827630	114.040224	48.247181
1767.011734	118.582449	48.252186
1763.742021	107.898149	48.257191
1760.033215	106.912524	48.262196
1756.598762	112.910798	48.267201
1753.376753	105.718140	48.272205
1749.759681	111.425301	48.277210
1746.261149	106.281474	48.282215
1742.595590	107.184181	48.287220
1739.059535	105.997667	48.292225
1735.719379	104.363054	48.297229
1732.231033	112.173030	48.302234
1729.214996	105.327963	48.307239
1725.366782	109.027345	48.312244
1721.703112	109.050249	48.317249
1718.662461	102.458949	48.322253
1715.015702	103.909217	48.327258
1711.757259	103.875380	48.332263
1707.878112	107.845328	48.337268
1704.244552	111.368936	48.342273
1700.858957	113.990258	48.347277
1697.409852	112.777560	48.352282
1694.288076	102.747284	48.357287
1690.878283	103.088176	48.362292
1687.425331	106.444471	48.367297
1683.940157	106.939463	48.372301
1680.112784	113.419667	48.377306
1676.431118	107.380549	48.382311
1673.105122	120.496107	48.387316
1669.636551	115.056563	48.392321
1666.196736	107.540318	48.397325
1662.730397	100.461632	48.402330
1659.525765	103.779279	48.407335
1655.764470	101.299074	48.412340
1652.243402	100.319042	48.417345
1648.989110	97.411920	48.422349
1645.172184	109.781317	48.427354
1641.614331	96.743803	48.432359
1638.027571	105.344202	48.437364
1634.692135	112.212906	48.442369
1631.500147	98.887498	48.447373
1628.117416	102.906736	48.452378
1624.728116	100.299035	48.457383
1620.841305	113.777116	48.462388
1617.633625	104.611259	48.467393
1613.842778	105.726464	48.472397
1610.475898	107.136343	48.477402
1606.861656	102.222514	48.482407
1603.011207	101.970785	48.487412
1599.510664	101.911364	48.492417
1596.285940	97.256446	48.497421
1592.270240	109.084149	48.502426
1589.638719	102.343768	48.507431
1585.916198	100.452313	48.512436
1582.584872	99.483884	48.517441
1579.379887	94.756295	48.522445
1575.899875	99.793569	48.527450
1571.908055	90.139180	48.532455
1568.208914	102.167541	48.537460
1564.714927	91.040474	48.542465
1561.372354	101.156244	48.547469
1557.971357	106.424828	48.552474
1554.833547	91.642033	48.557479
1551.067491	100.763876	48.562484
1547.500890	96.804407	48.567489
1544.286748	96.798490	48.572493
1540.436288	105.810088	48.577498
1536.745646	100.240619	48.582503
1533.026035	100.053953	48.587508
1529.962774	106.658836	48.592513
1526.531860	89.877916	48.597517
1523.131078	96.294889	48.602522
1520.156550	95.444935	48.607527
1516.176928	104.577876	48.612532
1512.347258	100.697320	48.617537
1508.871623	98.378313	48.622541
1505.114919	93.929592	48.627546
1501.773749	97.122968	48.632551
1498.253760	102.258217	48.637556
1494.617081	96.496861	48.642561
1491.602171	96.058150	48.647565
1487.828568	96.677144	48.652570
1484.948328	90.048259	48.657575
1481.628278	100.014993	48.662580
1477.490122	106.907402	48.667585
1474.109699	104.880457	48.672589
1470.513936	94.129910	48.677594
1467.122653	93.329010	48.682599
1463.495342	92.384516	48.687604
1459.858194	93.972512	48.692609
1456.546831	86.512245	48.697613
1452.657363	95.659624	48.702618
1449.972374	90.635986	48.707623
1446.292101	91.752977	48.712628
1442.564287	93.541745	48.717633
1439.242690	88.977856	48.722637
1435.363202	96.949952	48.727642
1432.362175	87.318544	48.732647
1428.696891	95.779308	48.737652
1425.022384	88.714083	48.742657
1421.560079	87.724930	48.747661
1417.886473	96.813402	48.752666
1414.606476	87.972051	48.757671
1411.275097	97.402719	48.762676
1407.166642	91.319348	48.767681
1403.981708	96.415104	48.772685
1400.381114	97.785448	48.777690
1396.715938	98.539433	48.782695
1393.855221	103.331632	48.787700
1390.442249	103.128890	48.792705
1386.796508	105.936255	48.797709
1383.035203	104.367230	48.802714
1379.443292	99.035514	48.807719
1375.755393	100.672546	48.812724
1372.429211	100.971979	48.817729
1369.476642	94.661245	48.822733
1365.758049	102.380516	48.827738
1361.998334	83.303358	48.832743
1357.787579	87.464144	48.837748
1354.420631	95.229918	48.842753
1351.536595	93.473733	48.847757
1347.818079	96.510722	48.852762
1345.004737	85.584639	48.857767
1341.673873	92.797476	48.862772
1337.693674	93.603664	48.867777
1334.018006	90.838096	48.872781
1330.550587	95.389377	48.877786
1327.063560	92.679867	48.882791
1323.486390	83.131830	48.887796
1319.849446	87.557639	48.892801
1316.610119	88.102982	48.897805
1312.934481	95.527671	48.902810
1309.861663	97.182864	48.907815
1306.105770	94.094434	48.912820
1302.226260	98.096103	48.917825
1298.844379	90.105844	48.922829
1295.727808	95.573772	48.927834
1292.204305	88.927982	48.932839
1288.629491	96.166139	48.937844
1284.907140	94.069056	48.942849
1281.838080	91.639337	48.947853
1278.031187	89.789527	48.952858
1274.419550	88.785669	48.957863
1270.804049	93.913649	48.962868
1267.704141	95.810339	48.967873
1264.363500	87.142965	48.972877
1260.550198	93.589356	48.977882
1257.211514	86.848368	48.982887
1253.687441	91.734332	48.987892
1249.556102	89.030211	48.992897
1246.604148	90.223678	48.997901
1242.630534	93.218127	49.002906
1239.211636	90.517006	49.007911
1235.829316	96.282560	49.012916
1232.667179	94.759496	49.017921
1229.100818	85.456561	49.022925
1225.578179	93.623051	49.027930
1222.336375	89.616236	49.032935
1218.508740	92.667057	49.037940
1214.839356	88.533812	49.042945
1211.864318	81.280660	49.047949
1208.120704	94.334646	49.052954
1204.629442	82.729515	49.057959
1200.831605	86.354653	49.062964
1197.043300	96.928938	49.067969
1193.855397	83.473286	49.072973
1190.525662	90.347437	49.077978
1187.439023	84.105057	49.082983
1183.290042	83.596130	49.087988
1179.914468	84.197493	49.092993
1176.547117	83.554248	49.097997
1172.979408	92.284564	49.103002
1169.348237	90.110029	49.108007
1166.017802	92.292541	49.113012
1162.579775	88.613664	49.118017
1159.126475	83.700164	49.123021
1155.638821	97.606472	49.128026
1151.895948	92.282472	49.133031
1148.576147	87.133062	49.138036
1144.919717	92.384478	49.143041
1141.293070	83.461096	49.148045
1137.778708	85.877878	49.153050
1134.239511	88.950246	49.158055
1131.042409	96.303620	49.163060
1127.199736	95.807130	49.168065
1124.448989	88.645624	49.173069
1120.779399	87.900736	49.178074
1117.019933	78.264060	49.183079
1113.582847	85.575693	49.188084
1109.949953	103.633225	49.193089
1106.706234	89.917361	49.198093
1102.992440	93.323787	49.203098
1099.461574	90.001048	49.208103
1096.252506	95.233452	49.213108
1092.031335	102.353936	49.218113
1088.739346	100.430329	49.223117
1085.196095	97.811857	49.228122
1081.557090	95.926449	49.233127
1078.608110	92.617539	49.238132
1074.964252	93.352421	49.243137
1071.779134	87.229788	49.248141
1068.031829	96.892880	49.253146
1064.611935	88.291660	49.258151
1060.818575	92.953804	49.263156
1057.000637	90.039581	49.268161
1053.594305	81.401455	49.273165
1050.367347	87.250399	49.278170
1047.147057	88.052226	49.283175
1043.588475	81.797911	49.288180
1039.890629	89.235558	49.293185
1036.595816	85.183239	49.298189
1032.865450	92.002704	49.303194
1029.389835	84.027085	49.308199
1025.867181	88.397162	49.313204
1022.287719	95.360815	49.318209
1019.032278	85.082562	49.323213
1015.495553	85.648918	49.328218
1011.862908	80.023056	49.333223
1008.653306	78.773156	49.338228
1004.704168	84.797789	49.343233
1001.799727	88.995709	49.348237
997.520759	89.886407	49.353242
993.750315	82.254075	49.358247
990.781597	80.074523	49.363252
986.928984	90.158958	49.368257
983.708245	81.397046	49.373261
980.267300	84.169401	49.378266
976.906995	87.723289	49.383271
973.587341	88.470990	49.388276
970.156920	83.892472	49.393281
966.591354	88.734294	49.398285
962.509575	92.096776	49.403290
959.176565	89.455088	49.408295
955.859533	82.960712	49.413300
952.221459	90.351097	49.418305
948.876097	80.890434	49.423309
945.252252	88.927158	49.428314
941.739137	87.499889	49.433319
938.476135	91.082926	49.438324
934.611795	93.468787	49.443329
931.676697	84.358705	49.448333
927.698211	86.224508	49.453338
924.370497	94.385978	49.458343
920.809693	89.176042	49.463348
916.801754	92.251795	49.468353
914.088049	83.926648	49.473357
910.331997	94.565520	49.478362
906.905627	90.078126	49.483367
903.650706	79.923202	49.488372
899.831170	96.079926	49.493377
896.218621	89.754942	49.498381
892.709396	93.891991	49.503386
888.723392	87.372048	49.508391
885.701761	81.764987	49.513396
882.487596	82.913882	49.518401
878.688339	81.274907	49.523405
875.069432	86.707156	49.528410
871.969763	83.912102	49.533415
868.136504	87.827516	49.538420
864.931948	99.165137	49.543425
861.437277	88.202834	49.548429
857.808371	79.824015	49.553434
854.515640	85.765462	49.558439
850.904928	86.014331	49.563444
847.293742	91.644694	49.568449
843.867665	93.035383	49.573453
840.210180	86.499111	49.578458
836.284608	87.746098	49.583463
832.974723	82.655304	49.588468
829.351979	92.251558	49.593473
826.545495	83.789012	49.598477
822.727836	92.245046	49.603482
819.454157	87.493458	49.608487
816.084872	91.589747	49.613492
811.828505	86.624145	49.618497
808.713973	80.231147	49.623501
804.995704	85.960436	49.628506
801.899154	83.835605	49.633511
798.158894	81.731888	49.638516
794.771533	77.520010	49.643521
791.206317	75.427010	49.648525
787.548791	82.953303	49.653530
783.982433	77.380436	49.658535
780.380053	76.856079	49.663540
777.059246	86.430640	49.668545
773.920271	78.380523	49.673549
770.412641	88.357481	49.678554
766.670371	84.571003	49.683559
763.331358	72.932783	49.688564
759.836808	74.761236	49.693569
756.149654	76.012246	49.698573
752.712940	87.613785	49.703578
748.831566	86.079358	49.708583
745.711627	84.299852	49.713588
741.781569	76.733547	49.718593
738.637620	73.293688	49.723597
735.239312	76.439069	49.728602
731.611579	75.260621	49.733607
728.149138	64.100361	49.738612
724.385668	75.702140	49.743617
721.417664	72.567081	49.748621
717.858882	84.969049	49.753626
714.259074	73.738423	49.758631
710.899265	67.174826	49.763636
706.836028	80.243763	49.768641
703.661010	74.673265	49.773645
699.983120	71.737299	49.778650
696.275612	78.929701	49.783655
693.062139	72.545799	49.788660
689.760733	78.058346	49.793665
686.626555	74.357552	49.798669
682.358493	76.391846	49.803674
679.038419	76.592328	49.808679
675.757943	69.953113	49.813684
671.975751	73.465135	49.818689
668.851875	76.384308	49.823693
665.048288	74.141777	49.828698
661.340477	76.794358	49.833703
657.791989	71.405390	49.838708
654.074682	75.476775	49.843713
651.295303	71.293659	49.848717
647.538965	81.432718	49.853722
644.305468	79.487411	49.858727
640.691487	74.124459	49.863732
637.064109	80.640020	49.868737
633.768220	72.253699	49.873741
629.847111	74.661085	49.878746
625.937158	72.109260	49.883751
622.880534	68.377422	49.888756
619.288695	77.554426	49.893761
616.178206	63.102966	49.898765
612.655632	67.909646	49.903770
609.088170	70.404346	49.908775
605.676518	64.054478	49.913780
602.188895	69.191068	49.918785
598.681806	66.525915	49.923789
595.024270	72.350164	49.928794
591.442926	71.866849	49.933799
588.023001	70.421960	49.938804
584.367333	72.259695	49.943809
581.092653	70.497974	49.948813
577.789053	71.452021	49.953818
574.059454	79.688719	49.958823
570.728072	74.332405	49.963828
566.606431	79.077332	49.968833
563.108582	77.033987	49.973837
559.859854	80.807816	49.978842
556.231504	77.835687	49.983847
553.133345	79.178523	49.988852
549.548230	74.864596	49.993857
546.262606	70.146552	49.998861
542.606490	77.223399	50.003866
538.886011	77.144555	50.008871
535.522923	79.879523	50.013876
531.638622	82.189445	50.018881
528.476039	78.436149	50.023885
524.840329	76.300380	50.028890
521.595889	71.683494	50.033895
518.457646	74.576443	50.038900
514.610975	66.323348	50.043905
511.063197	79.834051	50.048909
507.128980	73.587694	50.053914
503.592759	79.934055	50.058919
500.355981	67.356190	50.063924
496.728430	74.216627	50.068929
493.112495	64.424874	50.073933
489.913188	68.763637	50.078938
486.412813	71.061249	50.083943
482.851269	66.288099	50.088948
479.291099	73.505032	50.093953
476.033726	67.045750	50.098957
472.380131	74.909962	50.103962
468.632440	77.999032	50.108967
465.574925	77.279165	50.113972
461.446295	77.206926	50.118977
458.912009	69.610049	50.123981
454.906209	78.032117	50.128986
451.387544	80.569857	50.133991
447.686966	68.412211	50.138996
444.074899	80.398547	50.144001
440.786328	75.222246	50.149005
437.434268	71.283334	50.154010
434.039347	71.359461	50.159015
430.786333	75.725573	50.164020
426.769718	71.061240	50.169025
423.264275	73.720307	50.174029
420.043646	73.158714	50.179034
416.326988	67.932009	50.184039
412.992093	73.019530	50.189044
409.165334	68.161134	50.194049
405.824780	71.927125	50.199053
402.477044	69.341595	50.204058
398.553751	73.732967	50.209063
395.308319	74.418559	50.214068
391.504202	74.998145	50.219073
388.500617	65.016174	50.224077
384.557806	76.582614	50.229082
381.191851	85.613741	50.234087
377.851338	70.498973	50.239092
374.368222	81.781885	50.244097
370.740840	67.198986	50.249101
367.187463	69.833885	50.254106
363.682048	82.515446	50.259111
360.319716	80.723109	50.264116
356.812726	85.207861	50.269121
353.293855	77.514350	50.274125
350.082796	75.571918	50.279130
346.516823	74.099181	50.284135
342.658075	66.702192	50.289140
339.372733	74.578684	50.294145
336.176566	72.289097	50.299149
332.655752	71.802722	50.304154
328.791858	74.603024	50.309159
325.133816	68.089090	50.314164
321.360680	70.609515	50.319169
318.068964	58.682476	50.324173
314.803562	67.429032	50.329178
310.955957	73.127878	50.334183
307.525714	77.625994	50.339188
304.315627	78.252312	50.344193
300.854879	77.680663	50.349197
297.202914	78.087882	50.354202
293.660966	71.489443	50.359207
290.079546	74.859523	50.364212
286.602661	78.311403	50.369217
283.184076	75.373099	50.374221
279.420079	76.689915	50.379226
276.009427	81.529825	50.384231
272.616498	72.285512	50.389236
268.557210	80.725416	50.394241
265.672871	72.933137	50.399245
262.563964	74.489643	50.404250
258.907511	85.954568	50.409255
255.794330	73.746644	50.414260
251.863211	77.800741	50.419265
248.310487	78.312736	50.424269
244.611279	83.349429	50.429274
241.036880	79.204725	50.434279
237.669540	72.781586	50.439284
233.921572	72.764012	50.444289
230.659191	83.006521	50.449293
226.924493	76.672213	50.454298
223.562640	76.284488	50.459303
220.213579	76.173175	50.464308
216.288258	80.365575	50.469313
213.230867	73.141234	50.474317
209.821810	75.396190	50.479322
206.075348	77.732149	50.484327
202.653541	69.270610	50.489332
198.724855	71.037008	50.494337
195.475434	78.205585	50.499341
192.207424	79.546432	50.504346
188.879559	83.383235	50.509351
185.711211	66.220138	50.514356
181.790764	74.072135	50.519361
178.324813	79.689432	50.524365
174.500077	81.078993	50.529370
171.061659	79.289040	50.534375
167.210920	70.135010	50.539380
163.744122	68.960064	50.544385
160.599278	69.307331	50.549389
157.279755	68.052511	50.554394
153.809118	74.698727	50.559399
150.216412	71.056750	50.564404
145.952799	70.594303	50.569409
142.879790	67.665494	50.574413
139.449514	66.798068	50.579418
136.131821	78.691128	50.584423
133.158539	76.252978	50.589428
129.139838	79.678503	50.594433
125.788157	64.698420	50.599437
121.817131	69.353512	50.604442
118.060616	74.402302	50.609447
115.214666	67.641757	50.614452
111.280870	78.029930	50.619457
107.702414	67.836971	50.624461
104.589332	71.659323	50.629466
100.936363	72.243892	50.634471
97.643086	68.567960	50.639476
94.308202	75.113954	50.644481
90.574703	78.504572	50.649485
87.154534	67.641588	50.654490
83.769509	83.294069	50.659495
80.232492	76.992287	50.664500
76.098592	75.930708	50.669505
73.004404	70.635627	50.674509
69.654955	62.577294	50.679514
65.891140	71.391975	50.684519
62.390007	66.644296	50.689524
58.593048	68.510424	50.694529
54.988864	67.363212	50.699533
51.772218	61.388037	50.704538
48.569162	68.422856	50.709543
45.068919	59.524329	50.714548
41.260778	73.936091	50.719553
38.283536	75.269649	50.724557
34.757264	71.221892	50.729562
31.051268	68.204997	50.734567
27.676757	59.865847	50.739572
23.726216	71.949184	50.744577
20.341222	69.619445	50.749581
16.786089	67.164340	50.754586
13.332614	70.891007	50.759591
10.123405	68.151098	50.764596
6.651389	68.270923	50.769601
3.040663	71.221670	50.774605