Fri Aug 26 13:54:26 2022

Number of Points = 9924

Depth (nm)	Load (N)	Time (s)
2.992247	99.321185	0.000000
2.845414	87.894775	0.005005
2.428311	90.591900	0.010010
2.244425	84.283737	0.015014
2.440891	90.510884	0.020019
2.290542	80.546637	0.025024
2.446115	64.647200	0.030029
2.023077	68.930237	0.035034
1.445363	53.262037	0.040038
1.296514	57.012013	0.045043
1.050385	39.359206	0.050048
0.684039	25.818895	0.055053
0.205332	39.465504	0.060058
-0.072177	23.940407	0.065062
-0.753884	19.161892	0.070067
-0.717112	27.039995	0.075072
-0.701760	11.981823	0.080077
-0.634885	17.498319	0.085082
-1.013945	4.326987	0.090086
-1.432218	7.024281	0.095091
-1.708052	-2.205398	0.100096
-1.957825	-4.207042	0.105101
-2.636168	-7.344142	0.110106
-2.383522	-2.508287	0.115110
-3.082114	-4.993689	0.120115
-3.514816	-14.138828	0.125120
-3.544959	-6.765995	0.130125
-3.697876	-13.297236	0.135130
-3.970805	-7.117258	0.140134
-4.157287	-15.076403	0.145139
-4.782615	-11.106726	0.150144
-5.131352	-10.565211	0.155149
-5.487339	-6.662778	0.160154
-5.286257	-12.897971	0.165158
-5.071061	-0.868490	0.170163
-5.638723	-12.387495	0.175168
-5.670234	-10.848205	0.180173
-6.798377	-3.465761	0.185178
-6.795969	-14.061157	0.190182
-6.883882	-10.909119	0.195187
-7.255123	-6.700602	0.200192
-6.953986	-11.233516	0.205197
-7.110139	-11.285114	0.210202
-7.488969	-16.107613	0.215206
-7.746637	-11.303033	0.220211
-8.090450	-15.026873	0.225216
-8.671822	-9.820729	0.230221
-9.153253	-6.534657	0.235226
-9.508950	-19.478662	0.240230
-9.507614	-9.076800	0.245235
-9.415979	-5.952717	0.250240
-9.395874	-10.378602	0.255245
-9.628324	-17.871860	0.260250
-10.094394	-16.378802	0.265254
-10.764439	-7.988883	0.270259
-10.947672	-10.007213	0.275264
-10.650638	-16.842618	0.280269
-11.167516	-11.209934	0.285274
-11.874327	-12.403288	0.290278
-11.945707	-8.678042	0.295283
-12.244203	-5.758962	0.300288
-12.247102	-5.524384	0.305293
-12.166053	-4.369602	0.310298
-12.457445	-7.086076	0.315302
-12.929822	-3.466067	0.320307
-13.481418	-5.721263	0.325312
-13.313598	-7.791088	0.330317
-13.776679	-2.834306	0.335322
-14.503883	-0.715315	0.340326
-15.185797	-3.905642	0.345331
-14.695164	0.523013	0.350336
-14.671056	-9.553762	0.355341
-15.333220	-6.397733	0.360346
-15.506764	-7.645643	0.365350
-15.721155	-5.609660	0.370355
-15.823999	-3.436026	0.375360
-15.486206	-10.825089	0.380365
-16.198356	-3.238505	0.385370
-16.587922	-4.332563	0.390374
-16.942160	-5.814922	0.395379
-17.426435	-4.081755	0.400384
-17.008509	-4.213245	0.405389
-17.249010	-3.511417	0.410394
-17.734555	-6.093262	0.415398
-18.285763	-4.599602	0.420403
-18.395491	-3.867517	0.425408
-18.471725	-6.709236	0.430413
-18.528393	-8.193635	0.435418
-19.008546	-7.201403	0.440422
-19.077675	-5.615128	0.445427
-19.613307	-15.342167	0.450432
-19.751771	-11.334404	0.455437
-19.851301	-9.145468	0.460442
-20.797896	2.277156	0.465446
-21.185637	-4.160580	0.470451
-21.318611	-12.631074	0.475456
-21.310294	-20.690145	0.480461
-21.657237	-4.397138	0.485466
-21.438243	-13.498216	0.490470
-21.158308	-4.591841	0.495475
-21.673231	-3.024739	0.500480
-22.580873	-7.793377	0.505485
-22.797879	-2.868581	0.510490
-22.876306	-11.176733	0.515494
-22.823009	-7.439262	0.520499
-23.049533	-6.613065	0.525504
-23.505850	-7.209528	0.530509
-24.188691	-3.126495	0.535514
-24.066262	-7.406967	0.540518
-24.168169	-6.884900	0.545523
-24.127985	2.084116	0.550528
-24.764781	-10.297290	0.555533
-25.465873	-12.333063	0.560538
-25.667855	-5.743368	0.565542
-25.582670	-12.656516	0.570547
-25.900267	-13.265087	0.575552
-25.709437	-12.535508	0.580557
-26.222947	-6.058655	0.585562
-27.053330	-11.921286	0.590566
-26.944145	-2.140469	0.595571
-27.585310	-9.620711	0.600576
-27.298789	-7.479228	0.605581
-27.059159	-6.238409	0.610586
-27.351066	-6.809853	0.615590
-28.080059	-13.219762	0.620595
-29.014614	-7.588481	0.625600
-28.675819	-5.673429	0.630605
-29.080754	-13.680814	0.635610
-29.007325	-11.009462	0.640614
-28.932135	-7.575946	0.645619
-29.380684	-8.686129	0.650624
-29.734800	-17.432225	0.655629
-30.283633	-9.051689	0.660634
-30.402936	-11.646265	0.665638
-30.333348	-19.502911	0.670643
-31.440787	-8.039433	0.675648
-31.380565	-13.445964	0.680653
-31.732706	-4.713250	0.685658
-31.814211	3.853948	0.690662
-31.774397	-5.719090	0.695667
-32.205657	-5.620290	0.700672
-31.889938	-9.190564	0.705677
-32.534762	-7.821528	0.710682
-32.664976	-7.013490	0.715686
-32.608865	-5.269551	0.720691
-33.593357	-0.399259	0.725696
-33.497127	-9.272423	0.730701
-34.086807	-2.290181	0.735706
-34.480809	-4.079549	0.740710
-34.617003	-15.517036	0.745715
-35.039725	3.720470	0.750720
-35.070821	-10.982446	0.755725
-35.140990	-3.878619	0.760730
-35.174008	-9.169397	0.765734
-35.078794	-11.942900	0.770739
-35.685799	-5.432508	0.775744
-35.643208	-2.139443	0.780749
-36.264307	7.071736	0.785754
-36.745302	-7.725643	0.790758
-37.330837	-2.588449	0.795763
-37.711494	-0.422178	0.800768
-37.378967	-6.351983	0.805773
-37.939770	-1.620422	0.810778
-37.929156	-5.491193	0.815782
-37.918805	-2.626527	0.820787
-38.385161	-4.066120	0.825792
-38.334208	-4.646656	0.830797
-38.411712	1.920497	0.835802
-39.074478	-5.550055	0.840806
-39.296881	4.636720	0.845811
-39.679083	-4.022754	0.850816
-39.283809	-4.144390	0.855821
-40.788680	-0.768569	0.860826
-40.874485	-2.444578	0.865830
-40.837758	-1.349331	0.870835
-40.926071	3.061900	0.875840
-40.788091	-5.564674	0.880845
-41.003204	1.827469	0.885850
-41.584008	1.171297	0.890854
-41.916754	1.352831	0.895859
-42.322529	3.864687	0.900864
-42.079389	-3.452695	0.905869
-42.270095	0.325932	0.910874
-42.992894	-8.505129	0.915878
-43.695088	-9.060146	0.920883
-43.900133	-6.373908	0.925888
-43.575933	-4.026328	0.930893
-43.952458	-5.600125	0.935898
-44.230761	-1.627533	0.940902
-43.952238	-3.031248	0.945907
-44.519314	1.005289	0.950912
-44.497707	-4.933052	0.955917
-44.846818	-5.210861	0.960922
-45.213064	-5.919421	0.965926
-46.032887	-10.246165	0.970931
-46.836204	0.831456	0.975936
-45.932094	-8.116876	0.980941
-46.245859	0.170119	0.985946
-46.638703	2.755889	0.990950
-46.778109	-1.809671	0.995955
-46.826629	-5.652252	1.000960
-47.366779	-7.684610	1.005965
-48.047091	-8.489798	1.010970
-48.415389	-7.439054	1.015974
-48.260695	-9.234761	1.020979
-48.667083	-5.685137	1.025984
-48.001463	-6.763158	1.030989
-48.431442	-4.225389	1.035994
-49.250141	-3.275354	1.040998
-49.330782	-11.630613	1.046003
-49.628762	-8.126341	1.051008
-49.813654	-5.038295	1.056013
-49.935110	-4.589112	1.061018
-50.400239	-2.213543	1.066022
-51.061655	-10.158848	1.071027
-51.333280	-1.100160	1.076032
-51.195162	6.047168	1.081037
-51.589055	-2.101140	1.086042
-51.515482	-6.374004	1.091046
-51.391033	-11.730426	1.096051
-52.263149	-1.591187	1.101056
-52.489243	-6.696885	1.106061
-52.593552	1.443606	1.111066
-52.929155	-4.616280	1.116070
-52.731931	-12.230219	1.121075
-53.897144	1.089825	1.126080
-53.999087	-0.855744	1.131085
-54.078545	-9.002387	1.136090
-54.369499	-9.896670	1.141094
-53.983482	-9.773264	1.146099
-54.274229	-1.015309	1.151104
-54.488419	-10.861995	1.156109
-55.319489	-11.033127	1.161114
-55.302238	-3.120365	1.166118
-55.471928	-9.006773	1.171123
-55.855006	-9.209693	1.176128
-56.415781	-14.063970	1.181133
-56.686989	0.815752	1.186138
-56.606049	-7.058483	1.191142
-56.734784	-8.319697	1.196147
-57.256949	-7.286123	1.201152
-57.110236	-11.554555	1.206157
-57.961346	-2.253788	1.211162
-58.257231	-2.270974	1.216166
-58.189849	-11.946373	1.221171
-58.400541	-9.287729	1.226176
-58.450114	-16.157747	1.231181
-58.844997	-11.800024	1.236186
-58.785907	-13.030372	1.241190
-59.421401	-13.431264	1.246195
-59.667493	-6.796740	1.251200
-59.884296	-21.470729	1.256205
-60.049776	-5.139545	1.261210
-60.814306	-10.689735	1.266214
-61.108975	-11.846022	1.271219
-61.609777	-8.965044	1.276224
-61.490784	-15.200108	1.281229
-61.249027	-8.875651	1.286234
-61.399233	-1.673945	1.291238
-61.675299	-18.401403	1.296243
-62.049850	0.350885	1.301248
-62.388897	-7.141594	1.306253
-62.663186	-13.498915	1.311258
-62.998129	-7.350412	1.316262
-62.958581	-12.120995	1.321267
-63.098420	-4.873449	1.326272
-63.599896	-13.055619	1.331277
-64.275826	-7.515225	1.336282
-64.749350	-0.275832	1.341286
-64.826097	-12.121192	1.346291
-64.788704	-11.725215	1.351296
-64.493180	-14.849433	1.356301
-64.562161	-9.242196	1.361306
-65.385250	-8.370568	1.366310
-65.297180	-10.592485	1.371315
-65.736034	-5.006748	1.376320
-65.949452	-13.584932	1.381325
-66.675949	-13.984309	1.386330
-66.846583	-9.607718	1.391334
-66.961596	-8.957066	1.396339
-67.128648	-9.174639	1.401344
-67.030637	-10.505956	1.406349
-67.855984	-4.882189	1.411354
-68.246289	-13.711231	1.416358
-68.506435	-14.069328	1.421363
-68.694732	-1.992848	1.426368
-68.719144	-9.705151	1.431373
-68.466155	-10.870781	1.436378
-69.300535	-1.088581	1.441382
-69.685599	-12.898590	1.446387
-70.025509	-5.145348	1.451392
-70.357912	-24.398105	1.456397
-70.540224	-12.294092	1.461402
-70.621355	-2.515283	1.466406
-70.738337	-16.341142	1.471411
-70.664134	-6.254339	1.476416
-70.674271	-7.821910	1.481421
-71.568020	-11.425322	1.486426
-71.593415	-9.675022	1.491430
-71.874469	-17.467580	1.496435
-72.080798	-4.872622	1.501440
-72.481638	-9.318383	1.506445
-72.722904	-10.160292	1.511450
-73.211478	-2.975503	1.516454
-73.095961	-13.196213	1.521459
-73.620645	-8.533551	1.526464
-73.389938	-6.054361	1.531469
-74.066791	-10.593182	1.536474
-74.098682	-4.846192	1.541478
-74.637059	-16.910727	1.546483
-74.563526	-5.273636	1.551488
-74.667322	-8.414772	1.556493
-75.333866	-8.934210	1.561498
-75.968049	-10.993054	1.566502
-75.946959	-7.978207	1.571507
-76.552024	-11.942932	1.576512
-76.304161	-16.796566	1.581517
-76.400114	-2.428173	1.586522
-76.399329	-5.063591	1.591526
-76.308342	-11.629640	1.596531
-77.145064	-5.020209	1.601536
-77.472828	-9.325493	1.606541
-77.869835	-3.211616	1.611546
-77.979861	-5.883563	1.616550
-77.965853	-18.473850	1.621555
-78.881568	-6.132260	1.626560
-79.082628	-8.559087	1.631565
-79.460802	-7.124004	1.636570
-79.537817	-8.355307	1.641574
-79.578002	-4.862700	1.646579
-79.367309	-7.344146	1.651584
-79.654456	-10.852188	1.656589
-79.876921	-3.231123	1.661594
-80.750828	-12.383487	1.666598
-80.866679	-7.256153	1.671603
-80.889843	-6.110454	1.676608
-80.750078	-7.653910	1.681613
-81.676123	-11.249130	1.686618
-82.328267	-2.827199	1.691622
-82.110585	-18.435674	1.696627
-82.448076	-7.123716	1.701632
-82.516456	-15.556807	1.706637
-82.370184	-3.348932	1.711642
-82.612517	-6.528606	1.716646
-83.251166	-10.098974	1.721651
-83.879207	-7.255130	1.726656
-84.011518	-6.896003	1.731661
-84.116599	-0.390996	1.736666
-83.901959	-1.139382	1.741670
-83.938052	-15.253072	1.746675
-84.777097	-6.286369	1.751680
-85.285315	-9.222171	1.756685
-85.135082	-6.439396	1.761690
-85.532400	-8.879956	1.766694
-85.424376	-7.770502	1.771699
-85.937032	-14.675981	1.776704
-86.483309	-12.158069	1.781709
-87.070454	-4.353678	1.786714
-87.047556	-4.743190	1.791718
-86.941847	-5.857415	1.796723
-87.172815	-3.916925	1.801728
-87.025818	-6.442235	1.806733
-87.312957	-6.302601	1.811738
-88.212000	-7.728604	1.816742
-88.159626	-13.532529	1.821747
-88.764272	-6.693488	1.826752
-88.692618	-13.367253	1.831757
-88.791259	-6.246342	1.836762
-89.441998	-7.866025	1.841766
-89.474913	-14.627908	1.846771
-89.909627	-0.507315	1.851776
-89.919184	-13.296408	1.856781
-90.056109	-7.555211	1.861786
-90.487727	-6.905881	1.866790
-90.771400	-8.547916	1.871795
-91.245850	-2.751000	1.876800
-91.187548	-8.419814	1.881805
-91.169998	-2.826049	1.886810
-91.863902	-4.189083	1.891814
-92.043968	-7.887798	1.896819
-92.885828	-0.929566	1.901824
-92.553944	-10.475309	1.906829
-92.590611	-11.228856	1.911834
-92.844001	-4.476141	1.916838
-92.798664	-10.769336	1.921843
-93.971394	-11.270070	1.926848
-94.003245	-19.085609	1.931853
-94.235893	-12.481654	1.936858
-94.596252	-15.994113	1.941862
-94.359896	-15.227333	1.946867
-94.450216	-16.390126	1.951872
-94.542117	-13.749980	1.956877
-95.162242	-7.604530	1.961882
-95.721079	-8.608957	1.966886
-95.584682	-18.431131	1.971891
-96.108133	-8.188003	1.976896
-95.999914	-8.549672	1.981901
-96.813873	-9.606122	1.986906
-97.164454	-11.250393	1.991910
-97.319636	-13.314216	1.996915
-97.435210	-8.931422	2.006912
-96.645683	-13.736164	2.016909
-96.204753	-13.690746	2.026906
-95.813021	-10.447804	2.036902
-95.718351	-4.659301	2.046899
-95.721525	-5.590074	2.056896
-94.718459	-8.407079	2.066893
-93.843601	-14.672741	2.076890
-93.388290	-3.495130	2.086886
-93.151084	-6.173884	2.096883
-92.918737	-8.566788	2.106880
-91.877124	-9.112225	2.116877
-91.839121	-3.628499	2.126874
-90.718261	-12.558482	2.136870
-90.614885	-8.523067	2.146867
-90.282194	-3.607893	2.156864
-89.666765	-4.093308	2.166861
-88.945788	-3.603669	2.176858
-88.053382	-6.960958	2.186854
-87.989573	-1.623796	2.196851
-88.077172	-3.960550	2.206848
-87.078224	-7.895108	2.216845
-86.354445	-8.058450	2.226842
-86.030391	-5.153416	2.236838
-85.096201	-4.136293	2.246835
-85.071116	-0.902783	2.256832
-84.961603	-0.986322	2.266829
-83.745592	-4.793126	2.276826
-83.544714	-5.552937	2.286822
-83.458616	-6.836553	2.296819
-82.229153	-4.078826	2.306816
-81.900252	-8.279678	2.316813
-81.903233	-5.738691	2.326810
-80.779597	-6.810065	2.336806
-80.616545	-10.395903	2.346803
-79.711316	-12.944258	2.356800
-79.405364	-9.624606	2.366797
-79.412562	-5.296384	2.376794
-78.433640	-16.694071	2.386790
-78.020730	-13.704674	2.396787
-77.664248	-14.514054	2.406784
-76.642783	-17.270569	2.416781
-76.556813	-17.863607	2.426778
-76.432697	-12.618197	2.436774
-75.490904	-10.629777	2.446771
-75.096769	-10.820985	2.456768
-74.231020	-7.483959	2.466765
-73.675133	-8.438424	2.476762
-73.541088	-12.111608	2.486758
-73.265672	-11.387875	2.496755
-72.557503	-10.250033	2.506752
-72.192485	-9.451555	2.516749
-71.172558	-11.219511	2.526746
-70.802390	-8.065073	2.536742
-70.771658	-12.476083	2.546739
-70.116465	-14.304453	2.556736
-69.301990	-11.307890	2.566733
-69.169585	-9.763632	2.576730
-68.119550	-16.601413	2.586726
-67.918017	-8.561481	2.596723
-67.427190	-9.958796	2.606720
-67.163838	-5.891270	2.616717
-66.567246	-10.586781	2.626714
-66.050621	-14.465246	2.636710
-65.168005	-11.324076	2.646707
-64.865937	-13.699326	2.656704
-65.056332	-9.475624	2.666701
-63.786487	-14.329811	2.676698
-63.491175	-22.060573	2.686694
-62.961458	-17.366139	2.696691
-62.354038	-17.527202	2.706688
-62.189536	-15.617322	2.716685
-61.526210	-16.496651	2.726682
-60.972515	-13.424640	2.736678
-60.501617	-12.458922	2.746675
-59.541162	-14.610411	2.756672
-59.416200	-15.754364	2.766669
-59.024805	-14.475336	2.776666
-58.588274	-17.039410	2.786662
-57.988481	-14.142463	2.796659
-57.452485	-10.608380	2.806656
-56.773559	-15.848882	2.816653
-56.713294	-14.125504	2.826650
-56.223878	-16.719986	2.836646
-55.141600	-16.701568	2.846643
-55.315619	-16.082081	2.856640
-54.354661	-7.821447	2.866637
-54.153789	-14.941982	2.876634
-53.335367	-17.343778	2.886630
-52.539522	-10.185135	2.896627
-52.432433	-12.675741	2.906624
-52.265692	-13.297194	2.916621
-51.452693	-16.632614	2.926618
-51.034735	-13.114998	2.936614
-50.111684	-14.354703	2.946611
-49.440894	-9.061364	2.956608
-49.660706	-6.084319	2.966605
-49.261656	-6.779956	2.976602
-48.344833	-10.559180	2.986598
-48.077735	-13.286936	2.996595
-47.333681	-16.174480	3.006592
-46.590557	-8.614833	3.016589
-46.448428	-11.690583	3.026586
-46.208207	-12.776457	3.036582
-45.044768	-12.609123	3.046579
-44.813385	-16.173923	3.056576
-44.751208	-11.834330	3.066573
-43.881504	-13.129083	3.076570
-43.370950	-11.178051	3.086566
-43.248827	-14.342549	3.096563
-42.246227	-15.464765	3.106560
-42.108817	-16.601152	3.116557
-41.160835	-9.922343	3.126554
-40.589871	-13.387966	3.136550
-40.653973	-14.717885	3.146547
-40.270700	-10.631018	3.156544
-39.516878	-6.611347	3.166541
-38.550615	-10.087836	3.176538
-38.151084	-13.200495	3.186534
-38.002756	-16.435594	3.196531
-37.622894	-9.589137	3.206528
-36.689516	-14.625344	3.216525
-36.514629	-15.210054	3.226522
-36.061179	-9.686477	3.236518
-34.921342	-13.668312	3.246515
-34.760178	-10.611207	3.256512
-34.915897	-10.596431	3.266509
-33.903747	-17.431481	3.276506
-33.367206	-9.918861	3.286502
-32.845933	-11.333586	3.296499
-31.994036	-10.794641	3.306496
-31.978521	-9.856218	3.316493
-31.969649	-12.147806	3.326490
-30.692315	-11.380505	3.336486
-30.318466	-19.075982	3.346483
-29.731754	-13.649180	3.356480
-28.987389	-17.015094	3.366477
-28.878745	-12.293109	3.376474
-28.663094	-15.887137	3.386470
-27.881210	-17.925294	3.396467
-27.411965	-18.638194	3.406464
-27.167543	-13.493873	3.416461
-26.359746	-13.505574	3.426458
-25.905472	-11.726338	3.436454
-24.985754	-17.213398	3.446451
-24.811740	-13.670469	3.456448
-24.561963	-14.938389	3.466445
-23.982283	-8.496829	3.476442
-23.379538	-17.507694	3.486438
-22.949823	-13.786007	3.496435
-21.968388	-9.472334	3.506432
-21.574736	-5.691179	3.516429
-21.589277	-8.558811	3.526426
-21.087736	-9.270404	3.536422
-20.255636	-10.432594	3.546419
-20.057157	-14.198172	3.556416
-19.004970	-5.498757	3.566413
-18.502303	-8.662320	3.576410
-18.611277	-11.641956	3.586406
-18.204100	-9.586133	3.596403
-17.243481	-15.288629	3.606400
-16.992533	-21.666217	3.616397
-15.864237	-13.710393	3.626394
-15.580335	-14.346920	3.636390
-15.265497	-15.507765	3.646387
-15.164222	-15.767412	3.656384
-14.345660	-9.537267	3.666381
-13.918971	-17.526066	3.676378
-13.206310	-23.646101	3.686374
-12.572148	-21.631955	3.696371
-12.179276	-14.749511	3.706368
-11.971026	-14.446125	3.716365
-11.464972	-9.545270	3.726362
-10.663975	-17.490981	3.736358
-10.612011	-12.864704	3.746355
-10.035684	-9.070812	3.756352
-9.728736	-10.306453	3.766349
-8.761203	-13.450531	3.776346
-8.593051	-7.378869	3.786342
-8.095761	-15.394500	3.796339
-7.318350	-5.100132	3.806336
-6.703483	-1.568822	3.816333
-6.329909	-2.830676	3.826330
-5.942313	4.119119	3.836326
-5.557097	2.529179	3.846323
-5.144697	12.215173	3.856320
-4.629917	16.861261	3.866317
-4.150659	21.547727	3.876314
-3.282670	31.774162	3.886310
-3.057089	29.828951	3.896307
-2.467480	47.219730	3.906304
-2.279166	53.738088	3.916301
-1.749156	66.123690	3.926298
-1.531936	74.683894	3.936294
-0.349405	92.555757	3.946291
0.107481	101.677356	3.956288
0.000000	108.646222	3.961293
0.257869	115.256111	3.966298
0.830436	119.153199	3.971302
0.686376	127.252485	3.976307
0.943558	123.026929	3.981312
0.899060	131.683340	3.986317
0.767742	125.870001	3.991322
1.002327	127.842422	3.996326
0.867626	129.650883	4.001331
1.077888	120.709279	4.006336
1.191518	131.916293	4.011341
1.196018	123.136434	4.016346
0.940710	120.626287	4.021350
0.952754	125.468002	4.026355
1.122328	121.414270	4.031360
0.914050	124.686309	4.036365
1.222185	133.607347	4.041370
1.041433	133.888600	4.046374
0.988886	137.003521	4.051379
1.361254	133.797711	4.056384
0.910800	133.570478	4.061389
1.003149	130.778417	4.066394
1.178657	131.782463	4.071398
1.032130	136.674179	4.076403
1.172084	130.799620	4.081408
1.388280	130.557174	4.086413
1.406998	136.191933	4.091418
1.566122	128.615500	4.096422
1.464453	129.703830	4.101427
1.371884	127.807405	4.106432
1.317777	131.042787	4.111437
1.240610	133.478188	4.116442
1.330526	127.839205	4.121446
0.920207	131.541325	4.126451
1.302675	127.631610	4.131456
1.156641	134.108246	4.136461
1.066093	139.953002	4.141466
1.258078	129.429241	4.146470
1.268675	135.020972	4.151475
1.471431	130.379957	4.156480
1.476741	135.621345	4.161485
1.186498	144.274895	4.166490
1.455289	135.257734	4.171494
1.303926	140.393806	4.176499
1.483502	139.903968	4.181504
1.739346	138.355081	4.186509
1.406996	141.023198	4.191514
1.715943	135.036907	4.196518
1.271446	134.463906	4.201523
1.189478	130.433518	4.206528
1.036007	138.499475	4.211533
1.354811	142.151348	4.216538
1.996108	153.216109	4.221542
1.837807	146.733103	4.226547
1.664369	128.527901	4.231552
1.418528	136.864496	4.236557
1.334643	140.737250	4.241562
1.955121	144.804049	4.246566
1.621213	140.945759	4.251571
1.457836	128.759455	4.256576
1.503327	141.267860	4.261581
1.771561	149.432674	4.266586
1.980308	145.021670	4.271590
1.322148	140.055962	4.276595
1.650648	146.170825	4.281600
2.032140	157.285531	4.286605
1.868789	148.689977	4.291610
1.508775	138.979799	4.296614
1.687210	143.773466	4.301619
1.744021	145.425565	4.306624
1.797273	145.622929	4.311629
1.765988	143.280374	4.316634
1.909906	130.549528	4.321638
1.865606	146.096383	4.326643
1.572225	132.959070	4.331648
1.759915	147.735836	4.336653
1.894019	148.635602	4.341658
2.122203	159.986145	4.346662
2.122919	146.989688	4.351667
1.944185	134.878535	4.356672
1.678799	142.452568	4.361677
1.605474	134.203662	4.366682
1.848047	144.628164	4.371686
1.983633	150.918594	4.376691
2.237682	151.461172	4.381696
1.984274	150.719217	4.386701
1.902627	134.688978	4.391706
1.997070	137.350754	4.396710
1.945393	150.510192	4.401715
2.361423	148.898400	4.406720
2.414384	146.466799	4.411725
1.800822	139.716165	4.416730
1.590567	130.014312	4.421734
1.788204	140.752684	4.426739
2.182197	136.293858	4.431744
2.333232	154.107131	4.436749
2.065712	143.452429	4.441754
2.454389	146.840331	4.446758
1.926016	141.756341	4.451763
1.921803	136.903946	4.456768
2.280780	144.842664	4.461773
2.091057	148.924882	4.466778
2.269470	145.407592	4.471782
2.214311	158.675144	4.476787
2.185950	131.630198	4.481792
2.231194	145.701497	4.486797
2.064057	143.604714	4.491802
2.370171	147.144672	4.496806
2.433471	146.745702	4.501811
1.867083	143.774636	4.506816
1.958733	146.022407	4.511821
2.247640	154.623755	4.516826
2.129530	148.529949	4.521830
1.856650	158.022339	4.526835
2.467780	155.506996	4.531840
2.338084	158.228982	4.536845
1.902372	160.650611	4.541850
2.070845	153.446025	4.546854
2.241502	152.799392	4.551859
2.390847	148.068614	4.556864
2.308220	152.852312	4.561869
2.060036	151.517937	4.566874
2.363240	152.736215	4.571878
2.322356	154.808475	4.576883
2.573118	154.212643	4.581888
2.143957	150.815259	4.586893
2.330649	158.806116	4.591898
2.820009	177.439910	4.596902
2.572751	159.682757	4.601907
2.581715	155.043435	4.606912
2.238052	161.266121	4.611917
2.783888	165.075635	4.616922
2.892649	162.882111	4.621926
2.463217	165.169888	4.626931
2.154924	153.357297	4.631936
2.458120	164.019139	4.636941
2.668203	169.149562	4.641946
2.885272	180.236100	4.646950
2.640203	179.097387	4.651955
2.700236	168.948478	4.656960
2.632817	160.885297	4.661965
2.470545	146.702531	4.666970
2.853812	158.769227	4.671974
2.219235	169.406241	4.676979
2.890441	162.866841	4.681984
2.953174	167.887332	4.686989
3.056650	162.768233	4.691994
2.742217	149.308327	4.696998
2.644194	150.604893	4.702003
2.784839	144.420182	4.707008
2.646781	147.583219	4.712013
2.625181	153.724121	4.717018
2.587135	168.330412	4.722022
2.937162	179.601887	4.727027
2.776070	177.412413	4.732032
3.020895	167.481500	4.737037
3.024475	178.110908	4.742042
3.033088	162.604415	4.747046
2.517314	155.458909	4.752051
2.602664	157.881665	4.757056
2.805381	170.245392	4.762061
2.917226	173.027847	4.767066
2.878858	173.922830	4.772070
3.043230	173.634670	4.777075
3.339358	179.580583	4.782080
3.107465	175.228687	4.787085
2.930830	165.986639	4.792090
2.923273	151.754471	4.797094
2.874128	168.418876	4.802099
3.076159	171.873807	4.807104
3.231848	174.168557	4.812109
3.036926	168.934568	4.817114
2.829509	157.409982	4.822118
2.680709	162.773446	4.827123
3.106054	168.673926	4.832128
3.019707	168.472258	4.837133
2.718596	176.789003	4.842138
3.311051	170.707940	4.847142
2.781749	178.617300	4.852147
2.960831	172.692344	4.857152
2.959491	169.807298	4.862157
3.006640	181.141751	4.867162
3.082124	178.013794	4.872166
2.575550	180.750171	4.877171
3.138992	178.700983	4.882176
3.174205	175.984247	4.887181
2.872981	189.027548	4.892186
3.370220	191.262795	4.897190
3.684959	194.697018	4.902195
3.393616	188.617515	4.907200
2.996588	172.585727	4.912205
2.959416	179.874313	4.917210
3.109609	182.663454	4.922214
3.459419	199.085442	4.927219
3.388468	198.941486	4.932224
3.515669	198.864752	4.937229
3.459677	189.157829	4.942234
3.415341	179.066293	4.947238
3.099499	179.349598	4.952243
3.272559	190.610670	4.957248
3.505031	201.100051	4.962253
3.664291	201.825064	4.967258
3.476937	179.955272	4.972262
3.220858	187.765150	4.977267
3.483725	200.027786	4.982272
3.691869	201.327305	4.987277
3.373564	195.394363	4.992282
3.376154	193.005400	4.997286
3.392720	198.444366	5.002291
3.553930	192.269091	5.007296
3.905121	195.647020	5.012301
3.358636	186.712477	5.017306
3.372220	190.832651	5.022310
3.125840	191.029213	5.027315
3.419205	200.357535	5.032320
3.526890	195.177661	5.037325
3.821836	200.487865	5.042330
3.851720	198.145270	5.047334
3.710820	197.778092	5.052339
3.708422	194.652768	5.057344
3.524265	197.456004	5.062349
3.592495	200.694497	5.067354
4.036465	201.058813	5.072358
3.712813	204.962585	5.077363
3.867480	193.448036	5.082368
3.823869	188.975075	5.087373
3.319954	186.601700	5.092378
3.729378	196.709197	5.097382
3.598229	197.621791	5.102387
3.732434	197.249744	5.107392
3.853022	196.686833	5.112397
3.617232	198.412967	5.117402
4.242570	194.275603	5.122406
3.510385	200.650540	5.127411
3.630707	197.620001	5.132416
3.655374	200.998151	5.137421
3.641359	204.394979	5.142426
3.816549	205.395915	5.147430
3.915516	210.581616	5.152435
3.737739	201.051833	5.157440
3.860398	207.701790	5.162445
3.694445	205.592161	5.167450
3.968982	206.299226	5.172454
3.626367	209.563724	5.177459
4.080506	205.231555	5.182464
3.993906	204.890723	5.187469
3.946912	211.469023	5.192474
3.996187	197.984089	5.197478
4.248563	202.734623	5.202483
4.039537	206.424399	5.207488
3.870288	211.547459	5.212493
3.935047	204.374819	5.217498
4.100349	198.157777	5.222502
3.637221	202.697018	5.227507
3.885072	208.141104	5.232512
4.015324	208.389754	5.237517
3.560714	207.463993	5.242522
4.584151	217.225971	5.247526
4.408162	214.402911	5.252531
4.231864	204.914023	5.257536
4.185826	204.437165	5.262541
4.167305	203.775693	5.267546
4.454373	199.349318	5.272550
4.278621	200.765554	5.277555
4.311227	203.693226	5.282560
3.852119	207.048626	5.287565
3.603703	208.314829	5.292570
4.128114	205.917382	5.297574
4.112559	216.464372	5.302579
4.035530	217.764001	5.307584
4.360606	221.310513	5.312589
4.297413	229.432055	5.317594
4.630369	223.217375	5.322598
4.342547	231.734553	5.327603
4.406943	227.858520	5.332608
4.580888	224.281801	5.337613
4.115665	224.439671	5.342618
4.175181	212.326171	5.347622
4.213071	221.181764	5.352627
4.520392	222.098855	5.357632
4.308913	223.409927	5.362637
3.978835	226.881279	5.367642
4.322386	224.328496	5.372646
4.113451	240.476858	5.377651
4.660714	226.015880	5.382656
4.650313	229.038835	5.387661
4.607749	233.398710	5.392666
4.613023	222.214281	5.397670
4.350203	231.290701	5.402675
4.345146	224.056159	5.407680
4.735754	223.590408	5.412685
4.311276	225.602181	5.417690
4.752733	229.924659	5.422694
4.464806	224.724116	5.427699
4.627826	217.501372	5.432704
4.696836	221.752125	5.437709
4.595540	229.591705	5.442714
4.720285	214.288544	5.447718
4.853754	225.887990	5.452723
4.585601	223.348191	5.457728
4.540414	235.310809	5.462733
4.585374	228.312081	5.467738
4.858705	222.650838	5.472742
4.515318	230.670478	5.477747
4.750623	221.142805	5.482752
4.833842	220.544584	5.487757
4.342115	229.786355	5.492762
4.958479	221.746394	5.497766
4.681770	238.458951	5.502771
4.757088	232.236926	5.507776
4.726088	226.110548	5.512781
4.916310	230.260176	5.517786
4.934089	213.347536	5.522790
4.256141	223.940717	5.527795
4.590333	231.323360	5.532800
4.829090	228.391432	5.537805
4.716342	224.853022	5.542810
5.212994	223.130596	5.547814
4.877738	223.027791	5.552819
4.700029	232.429475	5.557824
4.583180	223.380564	5.562829
4.654847	225.745350	5.567834
4.943157	216.266374	5.572838
4.891820	228.315364	5.577843
4.776539	219.345304	5.582848
4.834679	222.626500	5.587853
4.912356	239.325008	5.592858
4.992669	249.679925	5.597862
5.113093	245.162428	5.602867
5.193386	241.201662	5.607872
4.983135	223.343773	5.612877
4.624226	236.908607	5.617882
5.042244	239.260596	5.622886
4.918333	246.907556	5.627891
5.005221	246.685242	5.632896
5.470110	244.211638	5.637901
5.465453	249.888037	5.642906
5.262823	235.426751	5.647910
4.910011	233.156391	5.652915
4.734490	241.823764	5.657920
4.969345	247.551454	5.662925
5.124945	238.456952	5.667930
5.418665	239.584966	5.672934
5.251167	247.203912	5.677939
5.064627	248.340264	5.682944
5.017932	246.607523	5.687949
4.946934	256.198244	5.692954
5.197990	244.523125	5.697958
5.081920	245.487157	5.702963
5.114891	243.827432	5.707968
5.000501	248.929306	5.712973
4.774290	255.921495	5.717978
4.662788	241.534600	5.722982
5.385231	258.521872	5.727987
5.326987	254.174556	5.732992
5.589660	263.618420	5.737997
5.414702	258.517335	5.743002
5.132978	243.479911	5.748006
5.270090	261.077164	5.753011
5.451473	267.480725	5.758016
5.240774	262.299784	5.763021
5.167643	266.088634	5.768026
5.306393	266.054394	5.773030
5.530134	271.945170	5.778035
5.424926	271.752764	5.783040
5.402802	262.442318	5.788045
5.333010	269.406995	5.793050
5.485181	265.457178	5.798054
5.331636	273.023344	5.803059
5.661424	270.361967	5.808064
5.831619	263.147578	5.813069
5.545754	272.031459	5.818074
5.521857	266.267786	5.823078
5.243987	274.802417	5.828083
5.259399	272.481047	5.833088
5.664708	273.256338	5.838093
5.392422	278.123381	5.843098
5.503957	260.743690	5.848102
5.543010	275.202026	5.853107
5.510705	272.970342	5.858112
5.525775	272.189744	5.863117
5.583938	263.638738	5.868122
5.390760	264.554666	5.873126
5.506794	276.530174	5.878131
5.350718	284.014482	5.883136
6.085059	282.137987	5.888141
5.823824	288.041004	5.893146
5.796410	275.384185	5.898150
5.748657	270.623952	5.903155
5.697761	270.435745	5.908160
5.914128	267.719263	5.913165
5.920299	267.167837	5.918170
5.897050	265.463081	5.923174
5.754834	266.010413	5.928179
5.850113	267.431912	5.933184
6.027134	256.208066	5.938189
5.750599	275.568638	5.943194
5.638186	270.290136	5.948198
5.798195	273.805413	5.953203
6.185929	283.378508	5.958208
5.993636	275.451774	5.963213
5.973475	275.714353	5.968218
5.863128	268.015305	5.973222
5.808100	272.234764	5.978227
5.766526	272.041942	5.983232
5.812235	277.688362	5.988237
5.750915	282.063824	5.993242
6.042536	275.393662	5.998246
5.836125	277.061446	6.003251
5.608506	274.439400	6.008256
5.967276	273.165536	6.013261
6.180431	289.729106	6.018266
6.109977	282.163043	6.023270
5.882155	279.303751	6.028275
5.744010	273.636956	6.033280
5.885437	282.821302	6.038285
5.990070	279.676135	6.043290
5.995947	261.499824	6.048294
6.036966	269.668433	6.053299
5.493131	275.134565	6.058304
6.001096	265.573908	6.063309
5.643693	270.552276	6.068314
5.890063	273.608026	6.073318
5.919065	281.601345	6.078323
5.901574	277.165422	6.083328
6.155496	267.688610	6.088333
5.707682	272.870877	6.093338
5.676849	269.623419	6.098342
6.112933	288.126421	6.103347
5.901513	277.102244	6.108352
5.860418	267.810567	6.113357
6.043273	275.982405	6.118362
5.777621	269.079478	6.123366
5.554997	277.036043	6.128371
5.612960	280.029381	6.133376
6.143772	288.621603	6.138381
5.749512	293.396913	6.143386
5.838494	288.985538	6.148390
5.917583	291.934460	6.153395
6.246365	285.932376	6.158400
6.418153	293.099890	6.163405
5.928072	283.400392	6.168410
5.943635	263.422430	6.173414
5.793705	263.755832	6.178419
5.539913	265.487939	6.183424
6.000675	269.984588	6.188429
5.483288	277.404928	6.193434
5.969458	277.367214	6.198438
6.048105	288.054601	6.203443
5.847188	282.593726	6.208448
6.236004	284.646553	6.213453
5.643993	273.336793	6.218458
5.945385	274.118771	6.223462
5.957528	275.334920	6.228467
5.832461	274.367337	6.233472
5.914208	274.142659	6.238477
5.675721	291.111900	6.243482
5.977303	285.300709	6.248486
6.165933	288.352796	6.253491
5.594842	272.484058	6.258496
6.191610	271.720457	6.263501
5.983041	276.634526	6.268506
5.977985	266.397622	6.273510
5.818471	269.402672	6.278515
6.123713	269.984739	6.283520
5.661927	253.402987	6.288525
5.499205	267.753530	6.293530
6.094167	272.956934	6.298534
6.059758	274.933289	6.303539
5.841579	273.356956	6.308544
5.901836	260.189798	6.313549
5.703961	271.783916	6.318554
5.728872	270.818292	6.323558
6.306935	280.896417	6.328563
6.185320	276.666528	6.333568
5.901911	264.568420	6.338573
5.748803	269.116355	6.343578
5.732153	256.356635	6.348582
5.869269	258.306282	6.353587
5.576651	273.199063	6.358592
5.860951	264.242696	6.363597
6.207550	281.952883	6.368602
5.977951	280.289744	6.373606
5.954349	270.508133	6.378611
5.602546	268.572963	6.383616
6.207527	260.167769	6.388621
5.566894	267.898354	6.393626
5.608694	269.578111	6.398630
6.018502	285.997166	6.403635
5.938511	296.861114	6.408640
5.973389	283.460613	6.413645
6.103887	293.934290	6.418650
5.854509	269.479814	6.423654
5.773162	271.273655	6.428659
5.944252	277.052411	6.433664
6.111579	280.073012	6.438669
5.920060	278.739296	6.443674
6.232013	272.540524	6.448678
5.796826	284.608188	6.453683
5.877161	274.351657	6.458688
5.976433	274.000866	6.463693
5.453350	267.530319	6.468698
5.772059	275.244415	6.473702
5.968680	286.739157	6.478707
5.977314	283.618427	6.483712
5.861672	268.083733	6.488717
5.963367	278.527085	6.493722
5.913671	274.010758	6.498726
5.808067	269.468336	6.503731
5.723396	269.766269	6.508736
5.958138	278.081887	6.513741
6.057825	285.684559	6.518746
5.734919	282.732505	6.523750
5.806068	278.637115	6.528755
6.135408	286.514073	6.533760
5.792405	275.548348	6.538765
5.938796	278.875924	6.543770
6.233278	280.408775	6.548774
6.046276	267.900192	6.553779
5.831650	272.071735	6.558784
5.606907	269.696011	6.563789
5.604361	275.865625	6.568794
6.178453	277.601709	6.573798
6.040143	267.553227	6.578803
5.826920	268.060996	6.583808
6.061516	258.242354	6.588813
6.009300	273.762081	6.593818
6.171787	263.537056	6.598822
6.033158	263.552330	6.603827
5.858742	279.651061	6.608832
6.305276	271.254714	6.613837
6.143161	271.748198	6.618842
5.905433	271.987705	6.623846
5.911186	270.771969	6.628851
5.632142	276.082981	6.633856
6.029194	268.950325	6.638861
5.845942	274.009145	6.643866
6.197997	271.809364	6.648870
6.110133	266.068306	6.653875
5.384366	263.663024	6.658880
5.566181	266.845880	6.663885
5.615094	268.012011	6.668890
5.609112	259.626015	6.673894
6.210657	265.378874	6.678899
5.868339	264.397662	6.683904
5.807003	262.379303	6.688909
5.512253	261.393849	6.693914
5.948508	264.125808	6.698918
5.757362	264.832616	6.703923
5.612229	274.428563	6.708928
6.210245	263.885796	6.713933
5.971753	274.866156	6.718938
6.029497	266.511362	6.723942
5.942897	272.168890	6.728947
5.775816	277.452979	6.733952
5.915977	268.171044	6.738957
5.863426	271.292317	6.743962
5.878580	266.057228	6.748966
5.464420	270.354748	6.753971
5.764512	271.165403	6.758976
6.652131	278.550482	6.763981
6.112380	282.057654	6.768986
5.870450	278.918990	6.773990
5.979923	273.163023	6.778995
5.801556	274.880223	6.784000
6.114650	268.542072	6.789005
5.734072	271.878929	6.794010
6.158172	274.925989	6.799014
5.968282	272.048137	6.804019
5.838095	278.104751	6.809024
6.230940	271.029696	6.814029
5.589457	271.461777	6.819034
5.924470	264.136306	6.824038
5.720958	267.293737	6.829043
5.533925	271.559058	6.834048
5.892640	260.322739	6.839053
5.530904	268.399034	6.844058
5.736528	267.671024	6.849062
5.922224	270.590690	6.854067
5.666616	277.666558	6.859072
6.069383	272.386935	6.864077
5.618273	277.307130	6.869082
6.133080	294.127452	6.874086
5.954471	286.043562	6.879091
5.828200	285.553884	6.884096
6.186927	282.008494	6.889101
5.712473	279.836159	6.894106
5.786990	277.360057	6.899110
5.991437	285.629776	6.904115
5.599606	287.475124	6.909120
6.238892	288.236131	6.914125
6.043947	287.969113	6.919130
5.943369	275.516671	6.924134
6.032402	275.717957	6.929139
5.579460	284.086865	6.934144
6.012644	270.466174	6.939149
5.731535	271.550813	6.944154
5.742467	264.048015	6.949158
6.050066	291.840644	6.954163
6.191548	290.629083	6.959168
6.062311	277.431306	6.964173
6.079698	279.943752	6.969178
5.957361	278.229113	6.974182
6.095531	267.144184	6.979187
5.795126	281.538321	6.984192
6.091026	265.237213	6.989197
5.753028	267.830300	6.994202
5.766384	276.904872	6.999206
6.042760	271.799949	7.004211
5.806891	279.891453	7.009216
5.980964	273.062427	7.014221
6.067102	275.197180	7.019226
5.716516	278.326893	7.024230
5.955118	280.849189	7.029235
5.444353	275.667508	7.034240
6.080217	261.844427	7.039245
5.884860	272.473228	7.044250
5.967438	273.156400	7.049254
6.155679	268.416371	7.054259
6.242393	277.112533	7.059264
6.146093	272.173200	7.064269
5.772173	282.975339	7.069274
5.677000	271.926738	7.074278
5.596021	272.341152	7.079283
5.668662	275.759303	7.084288
5.805692	261.811412	7.089293
5.554000	276.267562	7.094298
5.529691	274.540823	7.099302
5.925036	277.677780	7.104307
6.233616	285.295384	7.109312
5.836744	279.868183	7.114317
5.985221	275.808209	7.119322
5.591925	280.798496	7.124326
5.929672	275.503687	7.129331
5.385172	278.230165	7.134336
5.736020	295.370239	7.139341
5.842422	292.756295	7.144346
6.046354	297.985788	7.149350
6.338122	300.876289	7.154355
6.017592	295.313813	7.159360
6.083658	282.743673	7.164365
5.967073	283.021265	7.169370
5.653280	281.342761	7.174374
5.915827	282.254173	7.179379
5.477756	283.379070	7.184384
6.275859	292.173282	7.189389
5.852128	295.684538	7.194394
5.663884	290.800644	7.199398
6.086059	295.341272	7.204403
5.877972	308.075934	7.209408
6.112597	288.984472	7.214413
5.627684	292.305941	7.219418
5.882739	294.917424	7.224422
6.145168	288.565008	7.229427
5.952037	289.170888	7.234432
6.114353	274.788788	7.239437
6.035130	274.690411	7.244442
6.049153	277.288800	7.249446
5.937832	277.752230	7.254451
5.726823	280.904503	7.259456
5.806498	273.682058	7.264461
5.831905	274.937269	7.269466
5.661737	270.756069	7.274470
5.865800	273.150867	7.279475
5.648368	273.722565	7.284480
5.724215	282.297037	7.289485
5.871853	292.986340	7.294490
5.971102	292.679844	7.299494
6.103365	296.838512	7.304499
5.898931	289.625494	7.309504
5.956404	284.383811	7.314509
5.731056	284.504334	7.319514
5.979718	285.974717	7.324518
6.175464	283.792945	7.329523
5.640417	285.825103	7.334528
5.910788	279.015882	7.339533
5.674150	286.288112	7.344538
6.067146	294.980888	7.349542
6.047367	285.049980	7.354547
5.774845	286.101646	7.359552
5.778323	286.651605	7.364557
6.178131	289.645503	7.369562
5.584227	288.978702	7.374566
5.889747	282.148189	7.379571
6.187550	298.679605	7.384576
6.079755	286.304207	7.389581
5.511745	285.699813	7.394586
5.758726	286.461791	7.399590
6.149644	285.597364	7.404595
5.381092	296.986128	7.409600
6.205076	289.157416	7.414605
6.122365	295.178170	7.419610
6.097385	287.294983	7.424614
5.895453	282.362603	7.429619
5.496742	279.327441	7.434624
5.790895	280.445899	7.439629
5.835046	298.636620	7.444634
5.622688	296.344383	7.449638
6.128986	301.473017	7.454643
6.169400	293.070290	7.459648
6.154999	289.095783	7.464653
5.932474	292.139121	7.469658
5.831598	282.426482	7.474662
5.946534	273.243383	7.479667
5.758746	274.734265	7.484672
5.817075	267.780895	7.489677
5.777155	282.707104	7.494682
6.226029	288.698873	7.499686
6.010168	276.058739	7.504691
5.583288	278.368279	7.509696
5.733680	280.119713	7.514701
5.995127	282.160734	7.519706
5.954514	285.830633	7.524710
5.777033	287.917849	7.529715
5.659046	293.358811	7.534720
5.797846	294.510949	7.539725
5.794336	298.965997	7.544730
5.790560	294.524772	7.549734
5.982193	294.355750	7.554739
5.942270	306.716222	7.559744
6.048831	290.074419	7.564749
6.156400	304.196250	7.569754
6.343605	293.815502	7.574758
6.198574	286.922261	7.579763
5.809149	276.669267	7.584768
5.717403	275.693333	7.589773
5.676976	279.420148	7.594778
5.541458	286.284336	7.599782
5.945668	281.760609	7.604787
6.048982	293.250900	7.609792
6.246784	286.313772	7.614797
5.765988	283.329355	7.619802
6.178403	273.536802	7.624806
5.925624	273.883055	7.629811
5.696514	283.884379	7.634816
5.250466	274.181194	7.639821
5.728095	294.436748	7.644826
5.887477	288.492675	7.649830
6.147526	296.114675	7.654835
6.243727	296.336992	7.659840
6.402718	283.676453	7.664845
5.770935	285.489560	7.669850
5.687081	274.727091	7.674854
5.692756	270.882338	7.679859
5.730711	280.680731	7.684864
5.957864	281.888713	7.689869
6.042564	291.613396	7.694874
6.398710	278.662742	7.699878
6.093988	274.480345	7.704883
5.731009	271.113762	7.709888
6.050350	259.352073	7.714893
5.850314	261.126428	7.719898
5.911267	273.993181	7.724902
5.971380	270.329774	7.729907
5.783735	274.531917	7.734912
5.930935	270.241194	7.739917
5.817345	268.816254	7.744922
5.533218	265.010296	7.749926
5.691044	261.749284	7.754931
5.399096	281.944314	7.759936
6.204645	279.917529	7.764941
6.142486	288.541965	7.769946
5.744172	281.071241	7.774950
5.931493	281.168641	7.779955
5.705118	281.415871	7.784960
5.883893	284.036066	7.789965
6.110874	298.015916	7.794970
6.121427	290.415091	7.799974
5.963430	270.672947	7.804979
5.763886	278.749304	7.809984
6.195312	273.999883	7.814989
5.912251	280.061317	7.819994
5.725543	281.748180	7.824998
5.677389	277.361324	7.830003
5.755633	279.000606	7.835008
6.299542	271.041506	7.840013
6.149919	281.903633	7.845018
5.925370	270.141199	7.850022
6.106817	264.203189	7.855027
5.956454	270.547674	7.860032
5.904489	265.639405	7.865037
5.792363	279.498035	7.870042
5.729461	274.610448	7.875046
6.051522	266.837748	7.880051
5.879421	274.447932	7.885056
6.124002	271.439161	7.890061
5.646496	270.444196	7.895066
6.100883	273.122715	7.900070
5.939821	273.011770	7.905075
5.645820	269.884379	7.910080
6.035985	269.883759	7.915085
5.986866	263.355237	7.920090
5.916201	265.637786	7.925094
5.818006	267.060935	7.930099
5.921979	265.235132	7.935104
6.199301	262.736947	7.940109
6.234968	267.682588	7.945114
6.081169	268.472164	7.950118
6.238810	268.580512	7.955123
6.223343	267.810997	7.960128
5.901812	265.787566	7.965146
5.992377	262.043539	7.970163
6.189641	263.312958	7.975181
6.038204	248.192738	7.980198
5.716520	245.522698	7.985216
5.678297	241.407431	7.990234
5.765018	251.548723	7.995251
5.980862	263.528576	8.000269
6.161179	265.996615	8.005286
5.830165	257.622664	8.010304
6.108731	262.341140	8.015322
6.232513	253.069608	8.020339
5.974880	251.806468	8.025357
5.826676	249.453379	8.030374
5.724778	252.369275	8.035392
6.114833	256.155261	8.040410
5.662545	250.760166	8.045427
5.782061	263.483966	8.050445
6.020791	269.657076	8.055462
5.794492	273.258180	8.060480
6.242111	268.556051	8.065498
5.767875	271.154403	8.070515
5.834210	272.059222	8.075533
5.794057	280.137573	8.080550
5.791049	275.048039	8.085568
6.100327	274.334066	8.090586
6.097295	276.559270	8.095603
5.811024	271.876736	8.100621
5.901540	265.879602	8.105638
6.117460	272.365515	8.110656
6.069048	277.087570	8.115674
6.021798	273.074680	8.120691
5.963562	274.576374	8.125709
5.913151	280.305384	8.130726
5.976732	279.238368	8.135744
5.982351	278.050996	8.140762
6.125246	280.136721	8.145779
5.535219	276.457635	8.150797
5.651520	275.524413	8.155814
6.155603	298.942727	8.160832
6.043504	298.537344	8.165850
6.081985	301.724864	8.170867
6.081714	309.538258	8.175885
6.444022	306.629177	8.180902
5.875705	299.920458	8.185920
6.328221	296.110602	8.190938
6.164838	293.343329	8.195955
6.126860	290.446083	8.200973
6.068914	287.308965	8.205990
5.941335	302.049840	8.211008
5.999569	295.221482	8.216026
6.226193	299.534667	8.221043
6.400061	294.168294	8.226061
6.383235	299.191532	8.231078
5.954973	293.827396	8.236096
6.190667	295.172880	8.241114
6.373596	298.401022	8.246131
6.148021	296.703722	8.251149
6.109636	297.826807	8.256166
5.784042	301.481244	8.261184
6.171475	302.389717	8.266202
6.459907	297.848057	8.271219
6.042871	304.868008	8.276237
6.381296	301.000180	8.281254
6.318330	300.849064	8.286272
6.349409	306.871491	8.291290
6.416563	292.247344	8.296307
6.044372	304.463940	8.301325
6.219227	301.612446	8.306342
6.277296	295.756046	8.311360
6.176126	293.796393	8.316378
6.516384	290.322735	8.321395
6.243603	298.623497	8.326413
6.320938	292.274976	8.331430
6.304911	291.851479	8.336448
6.214017	301.181057	8.341466
6.703662	286.374376	8.346483
5.991842	292.692336	8.351501
6.056383	290.561724	8.356518
6.262781	293.439093	8.361536
5.960861	290.775435	8.366554
6.390959	299.746201	8.371571
6.336956	303.254216	8.376589
6.021787	295.887581	8.381606
6.480027	294.737028	8.386624
6.172673	291.187486	8.391642
6.370142	290.765460	8.396659
6.185521	296.493282	8.401677
6.190383	294.040621	8.406694
6.568166	295.016864	8.411712
6.317685	296.330753	8.416730
6.220334	296.349083	8.421747
6.078905	300.321965	8.426765
6.127562	291.276693	8.431782
6.074522	292.219034	8.436800
6.281107	290.448137	8.441818
6.344583	305.834573	8.446835
6.268193	300.475606	8.451853
6.766463	307.741189	8.456870
6.471210	299.008221	8.461888
6.274052	301.172138	8.466906
6.234326	301.131006	8.471923
6.579946	318.347967	8.476941
6.724536	305.289568	8.481958
6.528131	309.580263	8.486976
6.506230	309.791962	8.491994
6.500289	297.744718	8.497011
6.241365	305.046147	8.502029
6.279792	301.288140	8.507046
6.561761	304.330459	8.512064
6.175342	300.764825	8.517082
6.681819	310.209670	8.522099
6.525110	316.958732	8.527117
6.353703	315.063658	8.532134
6.814497	308.592316	8.537152
6.858995	307.225329	8.542170
6.664082	299.981972	8.547187
6.295689	306.312734	8.552205
6.621500	298.606472	8.557223
6.765205	293.516179	8.562240
6.567567	305.188075	8.567258
6.557889	300.187929	8.572275
6.495840	299.058426	8.577293
6.206205	299.393856	8.582311
6.204711	305.806341	8.587328
6.265418	304.291672	8.592346
6.657133	305.612865	8.597363
7.014771	313.970105	8.602381
6.881324	307.319900	8.607399
6.790464	295.639310	8.612416
6.498192	297.827503	8.617434
6.776047	292.429161	8.622451
6.681888	304.870697	8.627469
6.592537	297.437346	8.632487
6.405083	304.342660	8.637504
6.334943	301.655536	8.642522
6.747272	296.586531	8.647539
6.346693	298.472869	8.652557
6.263386	293.269607	8.657575
6.502745	294.125399	8.662592
6.703491	313.008992	8.667610
7.163860	314.868576	8.672627
6.589693	302.117738	8.677645
6.521386	293.415705	8.682663
6.849636	304.554467	8.687680
6.901235	310.996555	8.692698
6.552133	295.200209	8.697715
6.479948	302.160155	8.702733
6.489917	308.088045	8.707751
6.865119	310.595170	8.712768
6.808509	324.873760	8.717786
7.304281	313.628812	8.722803
6.752439	302.389199	8.727821
6.616236	300.823142	8.732839
6.826182	300.667402	8.737856
6.434602	302.934170	8.742874
6.419406	303.842219	8.747891
6.358355	304.561757	8.752909
7.023452	313.915640	8.757927
6.950418	318.726741	8.762944
6.864390	313.195711	8.767962
6.839433	302.423143	8.772979
6.366152	304.816235	8.777997
6.386537	307.864571	8.783015
6.292187	317.481857	8.788032
6.651521	320.307017	8.793050
7.012772	310.752344	8.798067
6.731909	316.409955	8.803085
6.935775	318.154851	8.808103
7.087599	316.272563	8.813120
6.986037	320.652630	8.818138
6.935844	322.951450	8.823155
6.754188	323.175399	8.828173
6.904332	312.258805	8.833191
6.916736	316.949311	8.838208
7.022742	333.402064	8.843226
7.241212	319.830406	8.848243
6.832435	329.777506	8.853261
6.906031	322.145214	8.858279
6.831347	312.945576	8.863296
6.752487	319.152372	8.868314
6.737651	317.841957	8.873331
6.743569	327.812847	8.878349
6.946027	326.815718	8.883367
7.215518	315.280970	8.888384
6.738544	322.281859	8.893402
7.236848	329.695761	8.898419
7.107201	324.635397	8.903437
6.853030	315.160762	8.908455
7.037140	311.111842	8.913472
6.959319	324.216685	8.918490
6.842202	314.184254	8.923507
6.817644	309.025486	8.928525
6.679779	321.470682	8.933543
6.958541	318.533583	8.938560
6.823505	320.403825	8.943578
6.908878	318.923181	8.948595
7.011497	315.221445	8.953613
6.760663	322.796162	8.958631
7.082082	321.954071	8.963648
7.003060	319.934166	8.968666
7.132267	318.194247	8.973683
6.804327	320.981256	8.978701
6.735343	316.195455	8.983719
6.996638	317.205615	8.988736
6.608474	323.539461	8.993754
6.938911	314.491328	8.998771
6.804760	317.797243	9.003789
6.766090	316.926016	9.008807
7.297916	319.913657	9.013824
6.934567	316.366517	9.018842
6.893508	318.136924	9.023859
7.098702	325.987759	9.028877
7.025001	332.988977	9.033895
7.280915	331.724763	9.038912
7.082952	328.230761	9.043930
6.958073	318.335229	9.048947
6.965228	335.021112	9.053965
7.467896	338.836917	9.058983
7.128446	329.164125	9.064000
7.202433	334.214257	9.069018
7.252335	330.801577	9.074035
7.226087	323.251099	9.079053
6.909039	321.350300	9.084071
7.127064	319.568152	9.089088
6.974062	330.015041	9.094106
7.276822	334.007129	9.099123
7.287492	332.762165	9.104141
7.148653	330.486499	9.109159
7.538850	326.298197	9.114176
6.917478	323.539114	9.119194
7.152679	321.385082	9.124211
7.237394	316.947716	9.129229
6.848426	330.444971	9.134247
7.294526	335.197339	9.139264
7.308794	346.845736	9.144282
7.146619	341.231884	9.149299
7.624036	349.176037	9.154317
7.195886	333.966290	9.159335
7.254800	333.474323	9.164352
6.990575	331.284447	9.169370
7.116369	337.011286	9.174387
7.247646	342.885588	9.179405
7.272684	342.398895	9.184423
7.811800	345.341227	9.189440
7.463437	344.732800	9.194458
7.464739	337.219049	9.199475
7.275311	324.562918	9.204493
7.372231	321.360658	9.209511
7.206372	320.550256	9.214528
7.195451	315.256827	9.219546
7.041206	317.290995	9.224563
7.205518	327.193044	9.229581
7.458616	334.979623	9.234599
7.750828	327.584676	9.239616
7.381559	333.312858	9.244634
7.222227	332.056496	9.249651
7.167293	325.886339	9.254669
7.425264	345.726680	9.259687
7.528779	344.079117	9.264704
7.348882	341.639437	9.269722
7.133154	334.351973	9.274739
7.419678	323.373114	9.279757
7.250840	334.289505	9.284775
8.007526	340.202124	9.289792
7.603415	324.998109	9.294810
7.395548	327.633887	9.299827
7.424371	323.422959	9.304845
7.102667	327.199866	9.309863
7.509571	323.150967	9.314880
7.519196	337.889444	9.319898
7.627592	332.037818	9.324915
7.599549	327.434979	9.329933
7.065951	327.148867	9.334951
7.598317	323.074122	9.339968
7.383211	335.913186	9.344986
7.698009	340.193719	9.350003
7.524813	333.540227	9.355021
7.176874	323.322835	9.360039
7.625301	332.827221	9.365056
7.638155	346.448108	9.370074
7.396677	336.378226	9.375091
7.705192	339.760382	9.380109
7.512857	338.259863	9.385127
7.401664	328.775582	9.390144
7.774950	334.047343	9.395162
7.451454	342.261352	9.400179
7.654633	325.508036	9.405197
7.667562	329.576805	9.410215
7.665296	317.658356	9.415232
7.669660	322.829772	9.420250
7.323595	318.692993	9.425267
7.600215	320.896751	9.430285
7.586383	329.759934	9.435303
7.811735	331.277436	9.440320
7.412854	323.993247	9.445338
7.388598	327.846911	9.450355
7.812272	332.788952	9.455373
8.003252	348.553183	9.460391
7.990799	338.204657	9.465408
7.881583	319.849589	9.470426
7.596034	321.411924	9.475443
7.553205	313.684160	9.480461
7.503261	316.339527	9.485479
7.712132	315.985149	9.490496
7.595759	317.928219	9.495514
7.407810	316.632135	9.500531
7.520326	315.791014	9.505549
7.788656	331.795638	9.510567
7.823281	325.169748	9.515584
7.611331	331.271045	9.520602
7.709290	342.445687	9.525619
7.945374	342.588817	9.530637
7.793411	333.006746	9.535655
7.586634	319.141556	9.540672
7.571320	336.313751	9.545690
7.865768	342.184737	9.550707
8.226893	332.030501	9.555725
7.773160	334.859186	9.560743
7.729798	318.368312	9.565760
7.717908	329.118260	9.570778
7.612718	318.099413	9.575795
7.479861	335.914723	9.580813
7.486156	340.640899	9.585831
7.545439	344.538361	9.590848
7.799587	348.945099	9.595866
7.674891	345.736316	9.600883
7.941319	337.335576	9.605901
7.638213	351.359092	9.610919
8.040040	339.301977	9.615936
8.159008	336.670607	9.620954
8.094970	348.921301	9.625971
8.010534	338.281042	9.630989
7.580150	345.489269	9.636007
7.797177	342.072655	9.641024
7.861518	333.289994	9.646042
7.892285	338.867536	9.651059
7.845383	337.789317	9.656077
7.796501	335.329240	9.661095
7.868933	340.499530	9.666112
8.017362	344.553517	9.671130
7.404881	345.166420	9.676147
8.072589	340.969619	9.681165
7.568022	340.962993	9.686183
7.853214	344.828438	9.691200
7.729278	340.527688	9.696218
7.715261	344.846796	9.701235
7.940239	335.998098	9.706253
8.104490	353.931260	9.711271
7.993746	348.464025	9.716288
7.828201	351.938927	9.721306
7.883706	364.675921	9.726323
8.392266	363.337657	9.731341
8.229466	355.552819	9.736359
7.910600	348.521235	9.741376
7.762436	349.932800	9.746394
8.003435	348.153384	9.751411
8.015007	354.081039	9.756429
7.928591	355.950026	9.761447
8.326247	359.501333	9.766464
8.315086	361.314424	9.771482
7.970316	351.165947	9.776499
8.102802	345.862803	9.781517
7.878091	350.340941	9.786535
7.957090	361.610060	9.791552
8.339572	364.949148	9.796570
8.133542	374.381893	9.801587
8.351121	354.688407	9.806605
8.202571	362.856253	9.811623
7.869034	348.408050	9.816640
8.398907	356.375595	9.821658
8.128008	345.306797	9.826675
8.266925	346.373879	9.831693
8.263087	342.729736	9.836711
8.216442	342.847462	9.841728
8.575243	336.275231	9.846746
8.217788	339.101549	9.851763
8.234209	327.423168	9.856781
7.802467	336.278843	9.861799
7.880567	337.162900	9.866816
8.044140	343.843172	9.871834
8.203438	358.002970	9.876851
8.410112	350.716001	9.881869
8.500144	361.932912	9.886887
8.275507	356.218333	9.891904
8.013266	350.487522	9.896922
8.069711	350.229455	9.901939
8.542515	355.864404	9.906957
8.436487	349.083689	9.911975
8.022482	339.561347	9.916992
8.354312	348.247652	9.922010
8.191722	364.193172	9.927027
8.144952	364.134203	9.932045
8.229826	367.071527	9.937063
8.406693	366.826268	9.942080
8.307228	368.719376	9.947098
8.173860	368.320458	9.952115
8.471866	357.674289	9.957133
8.530841	363.686080	9.962151
8.714270	364.847214	9.967168
8.699355	352.583591	9.972186
8.174833	351.235771	9.977203
8.002053	347.810425	9.982221
8.595841	355.108490	9.987239
8.342950	357.602967	9.992256
8.531276	349.826575	9.997274
8.280456	349.676306	10.002291
8.520785	353.510870	10.007309
8.421282	350.992404	10.012327
8.722144	362.630901	10.017344
8.667040	345.687419	10.022362
8.306935	339.066181	10.027379
8.452313	338.538662	10.032397
8.382702	343.768936	10.037415
8.155002	340.121780	10.042432
7.969245	344.271978	10.047450
8.176513	365.287820	10.052467
8.379340	365.480308	10.057485
8.416474	366.446480	10.062503
8.432397	369.656458	10.067520
8.597003	359.952504	10.072538
8.399785	362.659208	10.077555
8.950144	361.074608	10.082573
8.311024	358.539177	10.087591
8.329170	362.859593	10.092608
8.874348	363.727730	10.097626
8.516969	358.920552	10.102643
8.394106	361.233847	10.107661
8.367720	367.637607	10.112679
8.575519	363.016972	10.117696
8.592880	361.212417	10.122714
8.566525	368.622821	10.127731
8.559375	364.764605	10.132749
8.646865	374.438813	10.137767
8.450077	373.506999	10.142784
8.994986	362.093432	10.147802
8.664273	371.059619	10.152819
8.964370	372.473974	10.157837
8.818665	365.547959	10.162855
8.561988	374.758228	10.167872
8.376139	364.559755	10.172890
8.603383	364.858888	10.177907
8.498172	364.780617	10.182925
8.643628	355.335254	10.187943
8.665571	363.388197	10.192960
8.464853	368.607335	10.197978
8.122231	370.191182	10.202995
8.448239	376.202425	10.208013
8.972964	389.768894	10.213031
8.878612	401.951764	10.218048
8.738233	390.143129	10.223066
8.481077	381.293741	10.228083
8.868143	381.022065	10.233101
9.133043	383.590554	10.238119
8.772941	381.876323	10.243136
8.758010	362.591395	10.248154
8.599234	368.984212	10.253171
8.893250	377.004267	10.258189
8.983574	385.926997	10.263207
8.685987	372.666010	10.268224
8.757777	366.510820	10.273242
8.982039	380.897195	10.278259
8.898368	381.121667	10.283277
8.990767	364.095244	10.288295
8.439106	373.427176	10.293312
9.253471	378.327334	10.298330
9.053644	377.061495	10.303347
8.876156	363.816527	10.308365
8.839205	363.566691	10.313383
8.762145	362.751929	10.318400
8.557806	360.893534	10.323418
8.979214	378.493208	10.328435
9.453918	382.682586	10.333453
9.196258	376.121119	10.338471
8.889180	366.026722	10.343488
8.983362	356.119151	10.348506
8.818083	364.832372	10.353523
8.728699	360.668241	10.358541
8.854075	363.173248	10.363559
9.172227	376.778181	10.368576
9.450543	375.381096	10.373594
8.853272	374.416967	10.378611
8.838120	364.763087	10.383629
8.703943	364.698793	10.388647
8.861386	379.792966	10.393664
8.892439	371.763355	10.398682
9.156527	380.655873	10.403699
9.114710	380.094385	10.408717
9.209668	380.818038	10.413735
8.993390	389.586546	10.418752
9.129216	376.321188	10.423770
9.184296	381.787666	10.428787
8.977458	386.635397	10.433805
9.286449	378.385793	10.438823
8.690667	389.188819	10.443840
9.242553	383.056699	10.448858
9.393138	384.298683	10.453875
9.062503	388.405179	10.458893
9.350316	376.990608	10.463911
9.276465	368.687013	10.468928
8.812285	366.118032	10.473946
9.135035	370.741299	10.478963
9.091294	381.720288	10.483981
9.124158	383.747422	10.488999
9.236481	389.918165	10.494016
8.916910	383.224331	10.499034
9.109634	389.947416	10.504051
8.995533	392.688518	10.509069
8.993388	386.513277	10.514087
8.932955	394.118336	10.519104
9.080608	384.767284	10.524122
9.421855	390.223921	10.529139
8.713410	385.499797	10.534157
8.840730	386.038539	10.539175
8.849698	393.755863	10.544192
9.295401	400.594190	10.549210
9.544888	404.282180	10.554227
9.115573	408.492403	10.559245
9.605491	412.815113	10.564263
8.956296	409.694292	10.569280
9.231754	412.731333	10.574298
9.616754	412.321129	10.579315
9.271885	415.404263	10.584333
9.456934	418.884549	10.589351
9.455584	413.469685	10.594368
9.593558	405.098380	10.599386
9.128176	395.527205	10.604403
8.961885	402.416640	10.609421
9.656477	408.364196	10.614439
9.311561	425.859180	10.619456
9.507033	413.408131	10.624474
9.576537	416.313145	10.629491
9.232043	419.500357	10.634509
9.287503	408.604757	10.639527
9.443773	420.489856	10.644544
9.461203	407.435403	10.649562
9.180186	408.905526	10.654579
9.240694	411.209211	10.659597
9.186751	408.611063	10.664615
9.328802	412.173777	10.669632
9.438467	412.122008	10.674650
9.479136	410.291729	10.679667
9.383269	415.889012	10.684685
9.331165	404.057156	10.689703
9.529090	410.422851	10.694720
9.339427	405.498034	10.699738
9.717925	408.689436	10.704755
9.331446	416.130684	10.709773
9.562176	402.834752	10.714791
9.797651	413.177026	10.719808
9.700642	417.423870	10.724826
9.799387	412.924338	10.729843
9.958372	409.762889	10.734861
9.746714	405.655653	10.739879
9.428160	409.536223	10.744896
9.534693	405.060725	10.749914
9.549990	405.676867	10.754931
9.648978	415.437665	10.759949
9.597256	409.039772	10.764967
9.267203	413.477527	10.769984
9.531724	407.614191	10.775002
9.636123	404.202479	10.780019
9.307341	415.074397	10.785037
9.831337	408.732027	10.790055
9.154231	421.680952	10.795072
9.456554	435.742808	10.800090
9.793434	440.745728	10.805107
9.480449	443.959595	10.810125
10.160484	444.617401	10.815143
9.846127	439.244952	10.820160
9.684214	433.959218	10.825178
9.919661	441.578186	10.830195
9.652606	439.912576	10.835213
10.037236	444.305332	10.840231
10.030920	445.830513	10.845248
10.005427	435.487117	10.850266
9.679326	422.189509	10.855283
9.390287	428.590006	10.860301
9.803191	430.930340	10.865319
9.845662	442.167329	10.870336
9.935186	444.141469	10.875354
9.780184	440.419860	10.880371
9.761278	447.892251	10.885389
10.066313	433.237262	10.890407
9.838092	444.304971	10.895424
9.834591	440.840627	10.900442
9.901543	435.812734	10.905459
9.601409	440.681316	10.910477
10.285133	440.798931	10.915495
10.027906	438.923517	10.920512
9.667991	437.474326	10.925530
9.935471	438.518242	10.930547
9.925865	443.631911	10.935565
9.959563	444.844763	10.940583
10.092821	445.691837	10.945600
9.930493	438.241388	10.950618
10.011914	437.401947	10.955635
9.960185	445.551601	10.960653
10.021343	437.791815	10.965671
9.864133	447.033969	10.970688
9.867606	444.155490	10.975706
10.195317	437.364011	10.980723
10.112435	430.668019	10.985741
10.155147	438.430599	10.990759
10.216773	439.781107	10.995776
9.898957	442.610736	11.000794
10.288588	437.643050	11.005811
9.911531	441.838834	11.010829
10.289048	429.899047	11.015847
10.378532	436.013405	11.020864
10.102789	433.771663	11.025882
10.182585	432.336058	11.030899
10.083542	439.366508	11.035917
9.864511	439.747749	11.040935
10.396517	435.341692	11.045952
9.906866	436.904258	11.050970
10.205327	426.422071	11.055987
10.429436	441.972953	11.061005
10.053163	433.060039	11.066023
10.371163	431.158177	11.071040
9.861273	437.722445	11.076058
10.150560	427.210129	11.081075
9.889177	432.792164	11.086093
10.203478	434.870154	11.091111
10.107452	430.098000	11.096128
10.248696	435.917135	11.101146
10.503460	435.678680	11.106163
10.185934	439.423403	11.111181
10.467688	432.007951	11.116199
10.413695	436.349083	11.121216
10.532199	441.701569	11.126234
10.212188	429.898786	11.131251
10.314026	441.012928	11.136269
10.466262	436.817471	11.141287
10.604668	430.361567	11.146304
10.494595	432.739149	11.151322
10.720583	434.486923	11.156339
10.183792	439.928813	11.161357
10.392110	430.211703	11.166375
10.113140	433.142575	11.171392
10.351346	438.236592	11.176410
9.688908	431.463586	11.181427
10.400676	434.265448	11.186445
10.158163	436.729920	11.191463
10.298238	433.347359	11.196480
10.335951	443.414344	11.201498
10.758084	428.797930	11.206515
10.549747	436.855203	11.211533
10.340328	441.091154	11.216551
10.693850	431.834250	11.221568
10.538129	434.465080	11.226586
9.916217	441.315021	11.231603
10.231224	435.781470	11.236621
10.001741	443.602210	11.241639
10.571537	446.751211	11.246656
10.561286	465.762488	11.251674
10.606538	458.614211	11.256691
10.314063	464.617643	11.261709
10.325815	463.132672	11.266727
10.386753	458.165667	11.271744
9.971425	466.668573	11.276762
10.615084	469.339040	11.281779
10.453616	470.642239	11.286797
10.554132	462.172602	11.291815
10.678051	462.251151	11.296832
10.393377	459.064100	11.301850
10.694564	462.579958	11.306867
10.311309	467.628739	11.311885
10.748603	474.623032	11.316903
10.719350	463.036876	11.321920
10.736936	469.332846	11.326938
10.651203	460.642912	11.331955
10.680452	469.685641	11.336973
10.521891	470.729623	11.341991
10.983884	475.343861	11.347008
10.655948	474.688069	11.352026
11.052222	473.963699	11.357043
10.923178	471.538174	11.362061
10.782725	464.576591	11.367079
10.655005	464.419777	11.372096
10.653236	462.835930	11.377114
10.964051	463.551223	11.382131
10.960833	466.789445	11.387149
10.565969	462.357286	11.392167
10.892593	450.475900	11.397184
10.524418	470.032035	11.402202
10.999535	473.189471	11.407219
11.130497	480.553338	11.412237
10.577528	469.193880	11.417255
10.784472	474.835548	11.422272
10.769017	482.670316	11.427290
11.176365	479.246134	11.432307
10.918673	482.359885	11.437325
10.907719	475.851484	11.442343
11.068743	472.033329	11.447360
10.792887	469.801068	11.452378
10.872352	467.743847	11.457395
10.997091	487.769185	11.462413
10.942955	493.249546	11.467431
11.198909	497.473011	11.472448
11.079432	489.378425	11.477466
10.854046	480.454617	11.482483
11.182693	477.777956	11.487501
10.726187	473.528954	11.492519
11.067223	476.849271	11.497536
11.234042	490.506255	11.502554
11.427948	481.406715	11.507571
10.998123	469.529489	11.512589
10.898435	476.354936	11.517607
11.245642	471.608431	11.522624
11.070774	463.377322	11.527642
10.922236	476.004160	11.532659
11.368939	474.227416	11.537677
11.028322	472.005237	11.542695
10.881751	464.883668	11.547712
10.919980	475.199887	11.552730
11.060623	486.711940	11.557747
11.226351	491.864592	11.562765
11.030710	495.899604	11.567783
11.433986	495.492866	11.572800
11.283442	492.467953	11.577818
11.284877	499.864618	11.582835
11.545335	494.866538	11.587853
11.231272	482.917633	11.592871
11.135817	465.462791	11.597888
10.919552	478.261114	11.602906
11.073775	482.487791	11.607923
11.136455	495.195361	11.612941
11.180396	498.577717	11.617959
11.105630	492.530505	11.622976
11.191278	499.052562	11.627994
11.350528	499.851412	11.633011
11.734714	501.079123	11.638029
11.033559	497.357334	11.643047
11.399505	492.746755	11.648064
11.057497	498.221448	11.653082
11.492687	490.406559	11.658099
11.571175	487.525861	11.663117
11.196784	496.429487	11.668135
11.308052	489.968320	11.673152
11.191726	491.598991	11.678170
11.132415	495.675890	11.683187
11.427391	490.672437	11.688205
11.421508	490.263134	11.693223
11.188540	496.074284	11.698240
11.144035	484.004517	11.703258
11.358444	490.531769	11.708275
11.283796	494.936089	11.713293
11.444428	507.931360	11.718311
11.593033	512.067405	11.723328
11.514171	511.647375	11.728346
11.522260	507.231358	11.733363
11.517993	517.696224	11.738381
11.345202	515.782410	11.743399
11.769148	508.657198	11.748416
11.759701	514.092740	11.753434
11.749297	508.833885	11.758451
11.654781	500.826922	11.763469
11.312170	492.546180	11.768487
11.643652	497.666716	11.773504
11.332402	498.257967	11.778522
11.733965	520.512318	11.783539
11.881477	515.721157	11.788557
11.605899	522.974777	11.793575
11.783259	510.207760	11.798592
11.438684	511.839258	11.803610
11.662203	517.459426	11.808627
11.889143	517.092764	11.813645
11.724046	529.924181	11.818663
11.520972	520.400457	11.823680
11.725732	518.658223	11.828698
11.650617	523.996700	11.833715
11.606794	509.919806	11.838733
11.736898	537.808281	11.843751
11.728046	523.034840	11.848768
11.652961	529.805986	11.853786
11.648459	525.780073	11.858803
11.793156	521.491100	11.863821
11.773759	525.883670	11.868839
11.989739	522.647058	11.873856
11.967119	522.798913	11.878874
11.899071	527.893305	11.883891
11.873032	525.480135	11.888909
11.501879	518.929974	11.893927
11.689015	521.662063	11.898944
11.726518	521.889760	11.903962
11.893895	523.533065	11.908979
11.957191	521.759209	11.913997
11.409200	522.235849	11.919015
11.603538	527.232586	11.924032
11.641212	524.768473	11.929050
11.294127	526.719086	11.934067
11.932138	540.908633	11.939085
11.758747	545.536613	11.944103
11.556269	543.797825	11.949120
11.698623	551.033720	11.954138
12.067774	548.991345	11.959155
12.334348	544.800150	11.964173
12.027213	541.222123	11.969191
11.778245	541.844702	11.974208
12.452054	536.804343	11.979226
12.012360	541.454851	11.984243
11.760807	537.416909	11.989261
11.811466	548.308723	11.994279
12.188654	538.956565	11.999296
12.122114	543.170294	12.004314
12.348598	551.197787	12.009331
12.035002	548.144605	12.014349
11.874156	544.139874	12.019367
12.089675	538.618626	12.024384
12.159598	538.976970	12.029402
12.030722	546.472834	12.034419
12.059175	532.744416	12.039437
11.993784	548.340466	12.044455
12.362979	558.393773	12.049472
12.050702	557.833366	12.054490
12.114468	567.299942	12.059507
12.216393	559.435930	12.064525
12.573837	570.551379	12.069543
12.579762	562.127980	12.074560
12.130902	548.136208	12.079578
12.197450	547.551532	12.084595
12.507826	547.014096	12.089613
12.283255	544.578188	12.094631
12.022230	537.045239	12.099648
11.878553	551.489039	12.104666
12.376948	559.388996	12.109683
12.513703	567.351575	12.114701
12.408329	574.433555	12.119719
12.592956	571.498449	12.124736
12.729069	566.854211	12.129754
12.611987	569.996575	12.134771
12.483700	553.446126	12.139789
12.505663	555.474976	12.144807
12.018013	550.889992	12.149824
12.447818	552.779606	12.154842
12.674355	563.265365	12.159859
12.552399	559.699525	12.164877
12.330069	551.927025	12.169895
12.605944	562.900542	12.174912
12.988124	561.733414	12.179930
12.236066	558.720096	12.184947
12.490903	556.417819	12.189965
12.429711	564.256588	12.194983
12.747744	562.297906	12.200000
12.633493	555.717200	12.205018
12.109746	556.644483	12.210035
12.429390	558.727968	12.215053
12.588610	562.581517	12.220071
12.961279	576.373767	12.225088
12.600223	568.433518	12.230106
12.539843	562.251504	12.235123
12.923674	562.270652	12.240141
12.524953	566.826428	12.245159
12.544238	563.740349	12.250176
12.530065	560.463829	12.255194
12.489732	562.701186	12.260211
12.126823	560.605538	12.265229
12.428141	571.985337	12.270247
12.241917	571.077113	12.275264
12.790007	567.855054	12.280282
12.524964	583.314969	12.285299
12.574826	570.154366	12.290317
12.595507	579.021767	12.295335
12.574579	595.238915	12.300352
12.565279	593.542624	12.305370
12.502764	596.973131	12.310387
12.699140	588.706252	12.315405
12.659074	596.608015	12.320423
12.944972	595.231822	12.325440
13.018982	596.608815	12.330458
13.176030	600.317550	12.335475
13.546769	594.466016	12.340493
12.989889	596.682821	12.345511
13.453361	593.650650	12.350528
12.654710	583.370744	12.355546
12.510372	579.903056	12.360563
12.921047	585.645578	12.365581
13.371236	597.210489	12.370599
13.017508	598.975959	12.375616
13.172031	595.767837	12.380634
12.828491	594.467556	12.385651
13.142370	590.133291	12.390669
12.963769	596.415671	12.395687
13.182811	592.613704	12.400704
13.404149	585.289643	12.405722
13.031369	578.354721	12.410739
13.101146	562.549721	12.415757
12.766065	573.612057	12.420775
12.747828	571.623683	12.425792
12.881349	584.771548	12.430810
12.723120	594.979575	12.435827
12.924252	591.092037	12.440845
12.843922	583.991663	12.445863
12.990291	594.739221	12.450880
13.115380	585.640875	12.455898
12.858047	589.527730	12.460915
13.240701	585.277429	12.465933
12.717016	593.342848	12.470951
13.011606	592.107307	12.475968
13.578329	605.266632	12.480986
12.811779	599.175619	12.486003
13.549031	608.524735	12.491021
13.490665	605.794708	12.496039
13.019220	599.780820	12.501056
13.059738	600.178456	12.506074
13.149273	616.454161	12.511091
13.405714	615.221403	12.516109
13.421588	618.529260	12.521127
13.314259	616.056154	12.526144
13.629238	623.413519	12.531162
13.340188	622.129997	12.536179
13.224443	613.192207	12.541197
13.507710	620.071688	12.546215
13.148438	614.759826	12.551232
13.380207	619.271097	12.556250
13.366762	621.804066	12.561267
13.560383	611.994475	12.566285
13.242175	618.162905	12.571303
13.434572	621.702045	12.576320
13.727523	622.464305	12.581338
13.580168	625.453608	12.586355
13.755068	610.130798	12.591373
13.587269	613.404138	12.596391
13.599987	621.528059	12.601408
13.828747	615.389367	12.606426
13.796533	617.417193	12.611443
13.288034	607.931508	12.616461
13.141264	603.555358	12.621479
13.289732	617.158493	12.626496
13.573432	611.418332	12.631514
13.584937	613.846434	12.636531
13.597803	612.698935	12.641549
13.530021	621.961968	12.646567
13.421600	625.734131	12.651584
13.366765	619.361892	12.656602
13.670636	623.716777	12.661619
13.705962	620.391514	12.666637
13.927864	620.274934	12.671655
13.827644	623.673448	12.676672
13.748633	622.694882	12.681690
14.135573	616.714592	12.686707
13.864276	617.324872	12.691725
13.798903	615.356454	12.696743
13.797893	625.719894	12.701760
13.718610	627.635133	12.706778
13.621570	619.972480	12.711795
13.665380	622.976198	12.716813
13.850185	617.336636	12.721831
13.584816	623.613601	12.726848
13.880750	611.358204	12.731866
13.593972	624.764035	12.736883
13.509941	623.353922	12.741901
13.993095	617.077795	12.746919
13.876365	629.772370	12.751936
13.768110	635.134974	12.756954
13.914848	631.896501	12.761971
13.694448	632.656641	12.766989
14.170506	639.932131	12.772007
13.925825	642.447459	12.777024
14.275077	645.378380	12.782042
13.996559	636.705753	12.787059
14.119751	640.378743	12.792077
14.240951	639.488920	12.797095
13.681579	626.596693	12.802112
13.793692	634.263349	12.807130
13.982466	639.065331	12.812147
14.163635	636.424232	12.817165
14.060445	635.929094	12.822183
14.014857	641.196739	12.827200
14.107808	632.475745	12.832218
14.010843	641.118507	12.837235
13.943973	642.145066	12.842253
14.303993	641.704036	12.847271
14.076249	644.756349	12.852288
14.141378	640.170479	12.857306
14.171859	634.782149	12.862323
13.880665	631.801201	12.867341
14.105047	640.403397	12.872359
13.514787	643.124003	12.877376
13.876394	643.354887	12.882394
14.274626	664.587494	12.887411
14.570513	665.466060	12.892429
14.633361	670.786256	12.897447
14.109191	667.418713	12.902464
14.459636	661.336796	12.907482
14.638159	655.013416	12.912499
14.295702	650.686656	12.917517
14.584997	633.973289	12.922535
14.511324	640.911509	12.927552
14.486461	639.779350	12.932570
14.060815	630.643657	12.937587
13.851058	641.961068	12.942605
14.517305	655.906479	12.947623
14.162612	666.435459	12.952640
14.893641	659.174016	12.957658
14.860881	662.722975	12.962675
15.060664	647.004953	12.967693
14.543995	635.687071	12.972711
14.516814	644.104382	12.977728
14.575590	635.770545	12.982746
14.214997	632.453277	12.987763
14.249818	640.826220	12.992781
14.900540	650.346615	12.997799
14.668664	648.836447	13.002816
14.603011	644.009016	13.007834
14.389139	640.902423	13.012851
14.266536	645.039702	13.017869
14.629694	657.344011	13.022887
14.570183	666.520576	13.027904
14.943371	664.326086	13.032922
15.201598	658.668768	13.037939
14.595346	646.992455	13.042957
14.569712	636.715234	13.047975
14.476720	653.439097	13.052992
14.713697	656.302297	13.058010
14.972948	658.855927	13.063027
14.730796	660.159078	13.068045
14.853889	655.056113	13.073063
14.597662	657.794139	13.078080
14.687247	655.804746	13.083098
14.582423	656.228168	13.088115
14.615012	657.737843	13.093133
14.518750	661.126281	13.098151
14.527995	667.221654	13.103168
14.477759	661.908997	13.108186
14.667558	659.960803	13.113203
14.428445	672.283157	13.118221
15.006615	683.288575	13.123239
14.677006	690.667436	13.128256
14.884419	688.113759	13.133274
14.949330	681.400973	13.138291
15.007801	699.537139	13.143309
14.975863	688.831694	13.148327
15.063148	691.869679	13.153344
14.856441	687.468127	13.158362
14.957246	688.257152	13.163379
14.952854	682.729075	13.168397
15.133158	682.887205	13.173415
14.985638	693.686892	13.178432
15.335735	683.603599	13.183450
15.216600	691.274726	13.188467
15.153701	692.480546	13.193485
15.002196	686.457838	13.198503
14.963782	683.787807	13.203520
15.269783	688.375897	13.208538
14.774297	687.907125	13.213555
15.093681	687.100048	13.218573
15.100579	678.654352	13.223591
15.032279	694.935769	13.228608
15.120429	690.261098	13.233626
15.206877	687.492733	13.238643
14.982363	695.622067	13.243661
15.096698	691.366182	13.248679
15.021630	694.041295	13.253696
15.429170	703.716342	13.258714
15.656623	718.361260	13.263731
15.384332	709.627670	13.268749
15.339024	695.954790	13.273767
15.186379	699.478242	13.278784
15.522726	699.154500	13.283802
15.331350	702.346324	13.288819
15.632499	712.151545	13.293837
15.797061	696.136016	13.298855
15.430231	701.226485	13.303872
15.350750	693.920815	13.308890
15.571175	689.067765	13.313907
15.253664	695.545371	13.318925
15.344561	693.069792	13.323943
15.632864	707.408592	13.328960
15.471899	698.717632	13.333978
15.748718	702.470854	13.338995
15.426648	703.104821	13.344013
15.619751	702.670843	13.349031
15.449417	706.307500	13.354048
15.488129	712.669691	13.359066
15.632251	710.176356	13.364083
15.508086	718.078645	13.369101
15.493914	713.943745	13.374119
15.894422	721.653896	13.379136
15.644033	723.614720	13.384154
15.872841	716.955295	13.389171
16.030622	722.838219	13.394189
15.775689	713.581233	13.399207
15.472218	711.640409	13.404224
15.832766	717.201437	13.409242
15.815618	716.882242	13.414259
15.822105	720.797474	13.419277
15.888550	718.284675	13.424295
15.932525	713.052006	13.429312
15.374883	697.757970	13.434330
15.803144	704.248849	13.439347
15.929931	713.557373	13.444365
15.574317	716.307726	13.449383
15.831719	724.699701	13.454400
15.540471	711.989721	13.459418
15.778668	706.856197	13.464435
15.607774	714.819407	13.469453
15.647704	717.034820	13.474471
15.637557	722.161276	13.479488
15.863618	715.653753	13.484506
16.014997	718.953154	13.489523
15.734064	721.729749	13.494541
16.140977	725.181863	13.499559
15.992540	720.929015	13.504576
15.825180	720.967713	13.509594
16.153761	730.838099	13.514611
16.196477	745.432910	13.519629
16.122204	744.381019	13.524647
16.245015	735.570121	13.529664
15.852814	738.613343	13.534682
16.144948	730.116901	13.539699
16.270059	744.061430	13.544717
15.975006	737.250039	13.549735
16.087157	753.604397	13.554752
15.672624	747.455369	13.559770
15.967779	744.029670	13.564787
16.157278	739.907234	13.569805
16.269919	748.656263	13.574823
16.210860	747.737698	13.579840
16.371763	749.940592	13.584858
16.453774	741.514728	13.589875
16.434473	750.416841	13.594893
16.375473	742.969111	13.599911
16.372740	744.594742	13.604928
16.196080	751.479614	13.609946
16.442942	747.398736	13.614963
16.437978	755.408710	13.619981
16.257469	752.038135	13.624999
16.385115	742.961401	13.630016
15.947550	747.182455	13.635034
16.008847	745.134342	13.640051
16.045860	754.892353	13.645069
16.496039	761.149473	13.650087
16.901436	768.489665	13.655104
16.940305	770.478039	13.660122
16.905605	752.259242	13.665139
16.548448	751.036806	13.670157
16.497245	744.023349	13.675175
16.128579	739.321963	13.680192
16.327650	748.325770	13.685210
16.330166	751.850320	13.690227
16.561242	768.441787	13.695245
16.618720	769.543665	13.700263
16.850025	773.922507	13.705280
16.675991	780.254732	13.710298
17.090288	766.377699	13.715315
16.780094	777.022888	13.720333
16.711358	770.239362	13.725351
16.705008	756.443608	13.730368
16.320210	765.197514	13.735386
17.086493	765.239165	13.740403
16.993170	768.945892	13.745421
16.922932	776.707271	13.750439
16.732541	754.202011	13.755456
16.786948	766.787989	13.760474
17.145504	765.226907	13.765491
16.745461	763.859673	13.770509
16.843781	759.148688	13.775527
16.880356	752.686432	13.780544
16.724687	773.797134	13.785562
16.695070	769.989664	13.790579
16.874584	769.381081	13.795597
16.785296	775.062656	13.800615
17.240510	775.739702	13.805632
16.905906	774.507441	13.810650
17.191137	782.598473	13.815667
17.131787	773.071171	13.820685
17.220533	767.847293	13.825703
17.350616	764.368399	13.830720
16.955789	760.049766	13.835738
16.897404	754.791997	13.840755
16.973856	760.690752	13.845773
17.034248	770.924799	13.850791
17.293007	766.561205	13.855808
16.904564	770.632609	13.860826
17.169054	756.731572	13.865843
17.137499	766.203628	13.870861
16.968254	766.804335	13.875879
17.169353	758.505085	13.880896
16.934986	772.871668	13.885914
17.085129	775.865169	13.890931
16.982974	773.725740	13.895949
16.877697	761.160334	13.900967
17.070097	767.050505	13.905984
16.819901	777.812582	13.911002
17.415280	783.908252	13.916019
17.662633	798.083092	13.921037
16.864853	789.447058	13.926055
17.414099	788.212880	13.931072
16.853212	791.156146	13.936090
17.425678	788.151153	13.941107
17.361532	800.825039	13.946125
17.153638	800.930007	13.951143
17.595147	790.548407	13.956160
17.437921	797.887849	13.961178
17.419921	796.707276	13.966195
17.330820	795.174866	13.971213
17.210175	798.384095	13.976231
17.728434	787.529812	13.981248
17.277611	802.018481	13.986266
17.285621	794.339396	13.991283
17.328572	803.550570	13.996301
17.667965	814.883572	14.001319
17.870032	807.641314	14.006336
18.103889	822.522000	14.011354
17.553197	796.948621	14.016371
17.681268	800.914367	14.021389
17.751915	802.607471	14.026407
17.712696	795.349138	14.031424
17.571600	810.821509	14.036442
17.926068	814.660492	14.041459
17.946994	815.345198	14.046477
17.663441	805.404673	14.051495
17.981786	799.633812	14.056512
17.284055	809.749240	14.061530
18.166622	809.334142	14.066547
18.075480	816.798999	14.071565
17.783624	805.512276	14.076583
17.647115	806.467639	14.081600
17.747587	819.680782	14.086618
18.073760	811.289452	14.091635
17.955378	822.368694	14.096653
17.859872	821.250678	14.101671
17.819668	814.251259	14.106688
17.971846	817.664160	14.111706
18.090036	825.790687	14.116723
18.250125	827.274213	14.121741
17.873213	827.515946	14.126759
18.074038	818.910605	14.131776
17.860801	822.430892	14.136794
18.024461	818.053692	14.141811
18.247027	821.749116	14.146829
18.113754	821.574229	14.151847
18.213692	821.536596	14.156864
18.127404	821.004108	14.161882
17.954667	818.115136	14.166899
18.030714	815.206363	14.171917
17.889352	827.150697	14.176935
18.004323	818.631305	14.181952
17.896578	823.612044	14.186970
17.970829	827.715560	14.191987
18.007365	815.560369	14.197005
17.886193	832.859973	14.202023
17.714429	844.695447	14.207040
18.104586	843.839475	14.212058
18.191519	844.592798	14.217075
18.261944	842.028870	14.222093
18.058126	853.853562	14.227111
18.339787	844.298373	14.232128
18.038493	844.405259	14.237146
18.442469	855.235939	14.242163
18.602471	865.015885	14.247181
18.366143	862.783730	14.252199
18.291213	857.058304	14.257216
18.459727	868.408478	14.262234
18.383120	874.586715	14.267251
18.538141	862.697061	14.272269
18.608401	866.233175	14.277287
18.674123	863.243954	14.282304
18.721422	865.256272	14.287322
18.804236	864.631184	14.292339
18.974035	861.442726	14.297357
18.667411	869.215703	14.302375
18.814144	852.956663	14.307392
18.548579	845.720928	14.312410
18.757078	853.401072	14.317427
18.971663	849.763842	14.322445
18.970298	844.591840	14.327463
18.727569	833.360565	14.332480
18.442924	833.509039	14.337498
18.380580	856.044316	14.342515
18.702092	855.909071	14.347533
18.852986	868.303378	14.352551
18.757484	863.329060	14.357568
18.877385	864.828313	14.362586
18.404130	868.606838	14.367603
18.896075	860.375863	14.372621
18.928912	876.136782	14.377639
18.911597	850.716961	14.382656
18.548046	866.337622	14.387674
18.939222	864.301249	14.392691
19.124280	857.951534	14.397709
18.722147	864.603318	14.402727
19.062496	860.990684	14.407744
19.070252	856.599879	14.412762
19.288102	863.530666	14.417779
19.275272	854.788164	14.422797
18.882034	869.510912	14.427815
19.172131	868.945067	14.432832
19.248720	861.747569	14.437850
19.201359	867.567809	14.442867
19.353519	866.957170	14.447885
18.983538	863.590828	14.452903
19.784070	858.205610	14.457920
19.505112	871.342171	14.462938
19.112822	868.137088	14.467955
19.286251	874.787623	14.472973
18.858611	872.825089	14.477991
19.335082	859.850309	14.483008
19.333792	862.438222	14.488026
19.243098	876.271292	14.493043
19.185038	868.652954	14.498061
19.092704	872.088156	14.503079
19.120661	859.353617	14.508096
19.533452	880.770404	14.513114
19.439220	885.651228	14.518131
19.549548	885.567798	14.523149
19.682326	887.816112	14.528167
19.386464	869.360153	14.533184
19.430835	879.366388	14.538202
19.535581	891.300849	14.543219
19.703410	884.786552	14.548237
19.563787	878.929183	14.553255
19.728350	872.749907	14.558272
19.540537	877.995586	14.563290
19.368819	881.402125	14.568307
19.750934	884.239609	14.573325
19.050414	889.874379	14.578343
19.679083	886.895332	14.583360
19.937034	881.376840	14.588378
18.979841	890.194680	14.593395
19.441506	883.965987	14.598413
19.711491	885.369293	14.603431
19.551431	889.395698	14.608448
19.827786	890.242604	14.613466
19.620514	891.874848	14.618483
19.513721	896.016035	14.623501
19.744424	901.180780	14.628519
19.748066	908.864442	14.633536
20.219759	913.571957	14.638554
20.042478	903.311882	14.643571
19.887043	895.522504	14.648589
19.820023	901.333193	14.653607
20.143205	906.199526	14.658624
20.537002	898.072175	14.663642
20.163648	897.600159	14.668659
20.279014	890.005301	14.673677
20.043151	895.813875	14.678695
20.137926	888.578822	14.683712
20.271938	889.428956	14.688730
19.990279	887.876026	14.693747
20.166013	886.498029	14.698765
20.127634	893.374049	14.703783
20.181192	888.427008	14.708800
20.246034	885.062387	14.713818
20.088905	882.369785	14.718835
20.032072	881.700169	14.723853
20.071692	889.453959	14.728871
20.251365	889.388133	14.733888
20.078356	880.626378	14.738906
19.975139	884.669177	14.743923
20.149194	893.702199	14.748941
20.122890	916.396039	14.753959
20.117622	915.396508	14.758976
20.372350	913.334039	14.763994
20.176533	912.572454	14.769011
20.016820	911.417093	14.774029
20.197168	914.917143	14.779047
20.254637	915.182761	14.784064
20.431890	904.570846	14.789082
20.209215	915.634827	14.794099
20.390740	903.744174	14.799117
20.414630	921.371565	14.804135
20.487699	921.855656	14.809152
20.709609	933.494198	14.814170
20.608926	945.719450	14.819187
20.732282	929.410332	14.824205
20.828139	917.662393	14.829223
20.595614	916.366893	14.834240
20.479947	904.273208	14.839258
20.591856	911.927392	14.844275
20.688142	921.761470	14.849293
20.611186	930.559043	14.854311
20.647530	936.530372	14.859328
20.929990	939.061495	14.864346
20.727794	945.073121	14.869363
21.232300	937.379787	14.874381
20.816444	939.195987	14.879399
21.099138	937.839202	14.884416
20.939327	920.207745	14.889434
20.492534	924.269334	14.894451
20.485900	925.147679	14.899469
20.844546	933.038006	14.904487
21.035373	934.601960	14.909504
20.975219	930.101792	14.914522
20.452795	934.534913	14.919539
20.752492	932.298185	14.924557
20.958688	936.466387	14.929575
21.008903	939.273506	14.934592
20.935392	942.251364	14.939610
20.464143	939.869587	14.944627
21.136916	940.168791	14.949645
21.214727	933.520173	14.954663
21.030351	942.577468	14.959680
20.910311	933.886333	14.964698
21.376029	954.824763	14.969715
21.203788	953.289505	14.974733
21.274255	956.200769	14.979751
21.329107	959.991761	14.984768
21.505637	955.956499	14.989786
21.654294	950.814756	14.994803
21.417730	934.940360	14.999821
21.527517	933.162382	15.004839
21.382475	936.858262	15.009856
21.120647	928.126091	15.014874
21.035456	935.653186	15.019891
21.164311	945.109829	15.024909
21.549686	968.790501	15.029927
21.525013	957.017122	15.034944
21.720421	958.826513	15.039962
21.670974	961.336734	15.044979
21.476843	943.735843	15.049997
21.349691	944.566683	15.055015
21.396703	954.421074	15.060032
21.652874	955.031289	15.065050
21.666214	960.845265	15.070067
21.616095	959.354107	15.075085
21.760024	960.035446	15.080103
21.695971	959.912894	15.085120
21.908763	951.532840	15.090138
21.430510	958.666717	15.095155
21.736728	957.284177	15.100173
21.843823	958.324694	15.105191
21.688352	968.131725	15.110208
21.893892	953.523359	15.115226
21.871702	963.498981	15.120243
21.841828	961.701719	15.125261
21.890404	946.840092	15.130279
21.407697	962.242708	15.135296
21.832332	957.203159	15.140314
21.788374	958.352399	15.145331
21.860654	954.860378	15.150349
21.960937	956.700358	15.155367
21.881395	956.564440	15.160384
21.998441	950.313642	15.165402
21.841521	958.741834	15.170419
21.947555	961.051125	15.175437
21.954453	961.794824	15.180455
21.744277	963.033059	15.185472
21.968595	960.454621	15.190490
21.748767	963.471043	15.195507
21.842023	966.113677	15.200525
22.295075	980.758400	15.205543
22.031273	983.238883	15.210560
22.351534	978.565867	15.215578
22.235359	983.301815	15.220595
22.206373	977.588130	15.225613
22.222480	983.638363	15.230631
22.094177	985.274100	15.235648
22.147477	981.056051	15.240666
22.274254	981.632766	15.245683
22.365907	982.353802	15.250701
22.342271	985.604764	15.255719
22.169471	996.083527	15.260736
22.301740	976.058661	15.265754
21.980388	987.630346	15.270771
22.447674	988.340234	15.275789
22.386374	981.000058	15.280807
22.099765	989.767188	15.285824
22.702637	1002.283717	15.290842
22.626246	1001.828577	15.295859
22.583282	985.387516	15.300877
22.412556	991.719301	15.305895
22.748139	1003.210804	15.310912
22.594854	1015.267571	15.315930
22.539576	1010.630926	15.320947
22.634950	1004.765330	15.325965
22.517594	1006.733873	15.330983
23.003788	1016.223279	15.336000
23.245663	1010.593642	15.341018
22.852174	1011.907758	15.346035
22.910679	1003.693710	15.351053
23.026590	987.745454	15.356071
23.063835	979.944975	15.361088
22.869368	982.676590	15.366106
22.695414	985.632225	15.371123
22.689061	985.948806	15.376141
22.894207	987.305412	15.381159
22.777691	1001.271985	15.386176
23.128076	1006.885178	15.391194
23.090557	1016.314115	15.396211
22.677177	1006.759759	15.401229
22.937326	1007.965794	15.406247
22.827848	1015.764943	15.411264
22.924464	1009.552019	15.416282
22.988587	1010.406729	15.421299
22.767676	1008.961093	15.426317
23.089710	1004.805337	15.431335
23.137653	1008.095650	15.436352
22.908784	1011.025127	15.441370
22.872039	1009.074298	15.446387
23.130005	1014.862827	15.451405
23.106539	1021.619811	15.456423
23.326554	1028.506144	15.461440
23.651617	1025.347131	15.466458
23.450656	1020.120950	15.471475
23.244797	1013.361836	15.476493
23.373384	1020.792567	15.481511
23.182229	1029.936168	15.486528
23.495924	1027.927620	15.491546
23.405305	1030.920780	15.496563
23.299503	1033.717491	15.501581
23.740974	1033.273238	15.506599
23.681501	1032.963783	15.511616
23.484121	1034.468270	15.516634
23.715994	1027.041405	15.521651
23.626173	1035.493899	15.526669
23.757586	1018.463933	15.531687
23.447186	1019.026666	15.536704
23.641979	1021.855468	15.541722
23.698343	1030.745940	15.546739
23.211397	1029.395371	15.551757
23.843410	1011.848820	15.556775
23.368726	1020.812502	15.561792
23.587445	1028.579492	15.566810
23.384736	1023.429320	15.571827
23.357226	1028.870987	15.576845
23.528666	1017.493061	15.581863
23.390645	1034.072816	15.586880
24.086207	1038.186940	15.591898
23.832458	1049.836501	15.596915
23.916898	1057.719084	15.601933
24.261268	1047.794266	15.606951
23.983791	1051.542347	15.611968
24.000828	1029.872277	15.616986
23.913931	1033.757937	15.622003
23.849141	1047.075873	15.627021
24.063466	1042.472982	15.632039
23.865794	1056.527971	15.637056
23.997438	1049.937199	15.642074
23.855084	1052.528169	15.647091
23.989543	1060.825837	15.652109
24.549171	1048.914087	15.657127
24.222453	1055.822440	15.662144
24.105832	1054.180685	15.667162
24.525523	1051.347756	15.672179
24.234882	1057.486798	15.677197
24.329599	1052.722649	15.682215
24.011649	1056.413917	15.687232
23.692527	1048.773033	15.692250
24.276381	1049.108174	15.697267
23.918495	1049.744572	15.702285
24.437680	1053.318124	15.707303
24.601978	1073.536774	15.712320
24.470510	1065.254448	15.717338
24.749821	1054.219460	15.722355
24.366310	1058.656229	15.727373
24.433077	1055.931896	15.732391
24.456204	1065.468180	15.737408
24.725135	1072.413185	15.742426
24.633316	1067.119504	15.747443
24.839278	1076.466383	15.752461
24.517757	1062.934055	15.757479
24.484957	1076.603634	15.762496
24.627384	1073.239521	15.767514
24.626584	1073.350115	15.772531
24.735738	1077.542927	15.777549
24.533165	1067.630672	15.782567
24.792050	1073.081410	15.787584
24.547871	1078.840846	15.792602
24.739237	1071.000552	15.797619
24.607753	1082.413350	15.802637
24.526400	1070.935895	15.807655
24.578298	1075.080817	15.812672
24.536730	1078.287252	15.817690
24.582026	1088.369199	15.822707
24.822802	1109.519557	15.827725
25.093806	1108.259252	15.832743
25.040679	1106.800108	15.837760
24.840421	1105.935066	15.842778
25.226245	1100.308236	15.847795
25.083486	1104.988395	15.852813
25.195416	1102.348541	15.857831
25.354400	1099.641401	15.862848
24.999482	1111.221548	15.867866
25.121079	1093.735452	15.872883
25.153594	1110.143560	15.877901
25.555316	1099.865805	15.882919
25.273960	1109.231771	15.887936
25.126166	1107.954622	15.892954
25.567990	1098.689938	15.897971
25.137160	1099.230399	15.902989
25.266966	1095.035124	15.908007
25.616545	1097.139259	15.913024
25.423928	1093.814684	15.918042
25.266401	1094.262101	15.923059
25.113452	1099.660204	15.928077
25.271903	1090.537473	15.933095
25.211168	1088.476763	15.938112
25.536665	1094.289517	15.943130
25.666210	1091.470199	15.948147
25.590632	1095.584481	15.953165
25.746585	1102.360898	15.958183
25.724665	1097.476042	15.963200
25.352117	1098.364031	15.968218
25.403373	1102.938244	15.973235
25.933296	1113.897793	15.978253
25.608331	1118.148738	15.983271
25.965547	1124.429929	15.988288
26.031162	1117.170921	15.993306
26.057720	1113.862711	15.998323
25.843071	1117.197085	16.003341
25.886189	1109.193665	16.008359
25.747286	1117.918925	16.013376
25.672456	1115.620568	16.018394
25.829784	1113.876195	16.023411
25.841395	1127.851320	16.028429
25.982575	1121.852322	16.033447
25.981927	1121.019316	16.038464
26.023878	1126.892006	16.043482
26.051487	1111.433909	16.048499
25.905148	1119.854218	16.053517
26.156655	1111.853066	16.058535
26.004877	1117.257304	16.063552
25.953754	1122.475460	16.068570
26.214393	1118.225097	16.073587
26.088399	1117.799767	16.078605
26.147429	1115.376428	16.083623
26.206567	1118.081202	16.088640
25.984212	1125.500346	16.093658
26.193305	1115.549216	16.098675
26.390109	1138.300119	16.103693
26.591699	1135.450643	16.108711
26.622183	1148.867429	16.113728
26.574392	1129.681460	16.118746
26.341831	1115.835443	16.123763
26.217772	1131.204454	16.128781
26.008367	1134.096206	16.133799
26.323849	1126.384885	16.138816
26.411148	1144.794724	16.143834
26.702769	1136.929324	16.148851
26.772553	1134.157173	16.153869
26.470671	1137.123284	16.158887
26.783648	1133.994535	16.163904
26.883207	1142.206158	16.168922
26.775772	1136.081763	16.173939
26.461914	1134.360257	16.178957
26.825346	1138.898498	16.183975
27.136835	1131.266691	16.188992
26.824651	1133.035211	16.194010
26.960231	1126.055637	16.199027
26.633642	1133.765566	16.204045
26.731324	1139.746347	16.209063
26.664702	1134.925245	16.214080
26.827277	1137.434038	16.219098
27.009721	1131.198240	16.224115
26.595171	1130.164592	16.229133
26.854247	1132.674137	16.234151
26.849310	1136.143120	16.239168
26.746817	1143.218565	16.244186
27.039049	1156.146483	16.249203
27.266407	1161.179282	16.254221
27.248722	1161.929973	16.259239
27.294801	1155.273589	16.264256
27.282733	1162.316028	16.269274
27.330908	1152.964284	16.274291
27.167649	1154.185760	16.279309
27.485024	1157.437307	16.284327
27.456957	1159.717011	16.289344
27.292043	1169.165863	16.294362
27.711807	1151.238815	16.299379
27.160538	1147.922734	16.304397
27.193634	1148.848553	16.309415
27.689468	1151.052997	16.314432
27.727881	1153.101445	16.319450
27.490988	1148.556157	16.324467
27.653462	1151.910715	16.329485
27.593896	1150.503062	16.334503
27.603089	1140.245374	16.339520
27.623654	1152.556030	16.344538
27.868644	1144.341285	16.349555
27.797849	1134.828194	16.354573
27.523202	1129.272629	16.359591
27.459496	1135.931781	16.364608
27.766898	1158.277330	16.369626
27.937593	1153.526570	16.374643
27.931919	1148.850609	16.379661
28.157439	1147.089303	16.384679
28.212084	1137.619796	16.389696
27.728823	1128.448635	16.394714
27.943475	1123.842517	16.399731
27.823015	1129.661600	16.404749
27.680391	1133.426572	16.409767
27.764878	1141.217667	16.414784
27.903081	1155.498148	16.419802
27.738003	1150.739708	16.424819
27.797050	1154.053566	16.429837
27.784846	1149.826741	16.434855
28.036983	1138.433018	16.439872
27.846670	1155.289268	16.444890
28.127073	1146.993269	16.449907
28.250134	1156.293138	16.454925
27.793266	1152.044027	16.459943
28.246298	1149.657168	16.464960
28.072078	1179.853568	16.469978
28.338757	1181.052287	16.474995
28.555184	1175.249837	16.480013
28.043875	1173.653743	16.485031
28.161004	1169.596124	16.490048
28.236093	1176.306264	16.495066
28.389232	1174.821311	16.500083
28.337137	1181.769005	16.505101
28.368296	1171.394271	16.510119
28.559827	1169.644567	16.515136
28.489441	1178.548535	16.520154
28.385999	1177.687350	16.525171
28.287068	1176.355252	16.530189
28.732221	1177.119087	16.535207
28.792623	1170.457312	16.540224
28.407221	1173.957136	16.545242
28.668224	1174.326768	16.550259
28.617278	1182.183148	16.555277
28.506293	1187.218141	16.560295
29.120205	1186.456704	16.565312
28.851310	1196.540294	16.570330
29.082600	1188.797874	16.575347
29.471594	1183.899509	16.580365
29.336065	1176.252076	16.585383
29.041768	1168.742973	16.590400
29.020591	1168.784157	16.595418
28.868542	1172.803066	16.600435
29.216515	1173.215961	16.605453
29.319531	1169.813786	16.610471
29.033673	1156.111733	16.615488
29.068982	1165.652486	16.620506
28.989155	1164.582499	16.625523
29.076320	1166.165770	16.630541
28.903841	1174.710094	16.635559
29.194899	1161.350556	16.640576
29.227638	1179.879379	16.645594
29.286299	1181.400817	16.650611
29.207772	1191.410584	16.655629
29.113694	1198.538389	16.660647
29.639320	1193.748136	16.665664
29.406524	1194.683797	16.670682
29.509078	1197.334486	16.675699
29.647679	1187.523679	16.680717
29.383086	1187.930963	16.685735
29.303290	1180.173865	16.690752
29.311793	1195.235116	16.695770
28.842732	1191.215111	16.700787
29.394550	1190.037311	16.705805
29.096078	1182.756069	16.710823
29.560970	1191.709246	16.715840
29.618777	1209.259058	16.720858
29.977392	1213.826471	16.725875
30.161404	1208.306766	16.730893
29.762618	1205.225708	16.735911
29.807476	1189.256777	16.740928
29.539501	1190.229473	16.745946
29.943275	1206.002358	16.750963
30.050610	1210.848733	16.755981
29.987430	1213.673550	16.760999
29.866995	1208.753510	16.766016
29.752693	1220.207902	16.771034
29.821929	1213.617319	16.776051
30.142776	1203.096478	16.781069
29.786834	1211.577866	16.786087
30.220236	1198.874632	16.791104
30.273594	1215.064999	16.796122
29.953518	1215.720762	16.801139
30.300149	1205.571444	16.806157
30.159173	1207.105033	16.811175
30.166130	1210.938249	16.816192
29.792357	1212.549109	16.821210
29.994308	1205.776921	16.826227
30.104761	1206.523441	16.831245
30.044703	1214.434903	16.836263
30.258072	1229.925031	16.841280
30.239144	1235.728341	16.846298
30.496894	1240.043222	16.851315
30.566333	1232.408033	16.856333
30.322996	1236.469572	16.861351
30.473605	1232.353077	16.866368
30.560421	1228.861895	16.871386
30.497487	1227.991245	16.876403
30.482165	1229.145511	16.881421
30.606577	1227.194814	16.886439
30.593509	1227.048543	16.891456
30.419746	1242.646294	16.896474
30.478088	1237.326028	16.901491
30.712391	1229.119219	16.906509
30.470493	1226.881573	16.911527
31.022880	1232.911510	16.916544
31.249495	1243.072611	16.921562
31.064857	1238.099443	16.926579
31.189909	1232.304890	16.931597
31.112756	1229.091701	16.936615
30.869410	1224.193949	16.941632
31.019145	1235.506256	16.946650
30.947879	1234.412842	16.951667
31.318248	1237.062864	16.956685
30.956447	1227.121663	16.961703
30.952305	1229.640646	16.966720
31.122491	1226.982236	16.971738
30.860413	1228.982804	16.976755
31.379168	1238.584024	16.981773
31.410881	1248.904862	16.986791
31.311398	1245.253335	16.991808
31.493649	1254.373626	16.996826
31.499010	1260.116358	17.001843
31.753207	1250.808225	17.006861
31.498197	1237.388484	17.011879
31.237645	1232.061065	17.016896
31.443292	1235.853884	17.021914
31.299829	1246.637494	17.026931
31.705796	1248.840164	17.031949
31.626718	1262.943124	17.036967
31.776278	1240.835598	17.041984
31.862557	1247.398857	17.047002
31.565068	1246.905551	17.052019
31.658891	1249.709085	17.057037
31.485878	1244.996036	17.062055
31.906898	1240.177877	17.067072
31.922301	1248.920201	17.072090
32.105049	1249.567106	17.077107
32.106793	1242.665129	17.082125
31.691249	1246.803975	17.087143
31.783564	1251.125681	17.092160
31.697798	1250.176534	17.097178
31.330301	1249.489002	17.102195
31.972958	1241.698289	17.107213
31.875522	1245.068085	17.112231
31.992035	1247.801815	17.117248
32.008556	1239.348043	17.122266
31.760566	1250.999994	17.127283
31.591795	1251.483879	17.132301
31.939880	1266.643797	17.137319
32.074213	1270.501375	17.142336
32.410358	1268.719678	17.147354
32.118776	1269.664496	17.152371
32.270960	1269.454627	17.157389
32.399266	1279.596341	17.162407
32.226298	1280.349123	17.167424
32.112662	1273.796457	17.172442
32.101216	1276.177730	17.177459
32.546102	1278.134503	17.182477
32.079623	1276.200060	17.187495
32.440802	1280.565120	17.192512
32.815933	1291.864460	17.197530
32.497938	1291.557382	17.202547
32.677585	1281.948415	17.207565
32.723976	1290.272525	17.212583
32.603336	1302.643140	17.217600
32.680288	1302.426049	17.222618
33.196172	1293.840854	17.227635
33.161061	1283.274401	17.232653
32.978969	1273.633398	17.237671
32.814441	1264.772303	17.242688
33.069591	1267.670642	17.247706
32.564926	1276.487641	17.252723
32.763944	1272.382535	17.257741
33.115578	1284.938382	17.262759
32.876611	1289.015031	17.267776
33.317454	1291.581506	17.272794
33.253818	1297.669507	17.277811
32.972571	1282.855796	17.282829
33.118448	1279.232333	17.287847
33.064275	1284.561464	17.292864
33.085737	1278.192890	17.297882
32.884199	1288.635274	17.302899
33.434621	1284.500699	17.307917
33.117552	1291.316121	17.312935
33.035364	1279.576730	17.317952
33.202621	1291.757346	17.322970
33.049866	1294.189024	17.327987
33.509281	1289.964476	17.333005
33.120991	1296.655290	17.338023
33.167906	1293.672081	17.343040
33.283377	1304.049337	17.348058
33.266483	1315.188823	17.353075
33.550998	1311.938243	17.358093
33.458278	1314.209098	17.363111
33.276618	1326.358855	17.368128
34.057473	1314.279942	17.373146
33.818226	1326.609079	17.378163
33.942194	1312.085704	17.383181
33.635625	1318.205225	17.388199
33.932921	1324.874513	17.393216
33.923673	1312.170690	17.398234
33.835127	1321.270062	17.403251
34.142631	1326.546050	17.408269
33.969403	1323.114273	17.413287
33.777635	1321.493660	17.418304
34.078123	1311.947913	17.423322
33.613986	1318.789400	17.428339
34.233671	1318.058618	17.433357
34.061483	1322.591937	17.438375
34.218848	1340.236830	17.443392
34.440319	1336.327030	17.448410
34.127094	1331.604230	17.453427
34.227969	1332.061913	17.458445
34.443905	1342.855896	17.463463
34.435624	1348.095850	17.468480
34.585673	1334.205871	17.473498
34.441914	1335.957655	17.478515
34.805902	1330.009104	17.483533
34.369097	1307.617249	17.488551
34.432005	1310.482410	17.493568
34.534316	1311.059790	17.498586
34.351253	1320.669338	17.503603
34.478019	1329.833021	17.508621
34.731106	1328.524998	17.513639
34.808060	1334.076726	17.518656
34.926612	1336.156899	17.523674
34.594315	1336.019305	17.528691
35.188559	1327.396648	17.533709
35.014861	1307.374866	17.538727
34.729298	1314.441013	17.543744
34.924055	1303.472685	17.548762
34.667275	1307.690967	17.553779
34.913627	1325.410354	17.558797
34.601156	1326.658229	17.563815
34.950522	1326.016871	17.568832
34.737965	1330.704801	17.573850
34.746693	1334.843881	17.578867
35.090634	1327.311080	17.583885
35.003912	1322.713963	17.588903
34.733297	1336.007357	17.593920
35.180907	1324.406356	17.598938
35.080037	1318.609080	17.603955
35.107418	1331.609920	17.608973
35.317423	1341.016270	17.613991
35.383532	1343.890406	17.619008
35.378325	1337.854167	17.624026
35.346740	1351.441716	17.629043
35.527546	1338.878697	17.634061
35.828686	1341.713084	17.639079
35.442010	1351.366974	17.644096
35.912456	1338.556887	17.649114
35.638222	1344.977496	17.654131
35.322498	1351.660188	17.659149
35.603569	1339.059468	17.664167
35.592125	1333.311380	17.669184
35.635270	1345.991040	17.674202
35.337112	1347.681658	17.679219
35.401235	1349.397921	17.684237
35.601061	1337.482039	17.689255
35.450032	1350.138285	17.694272
35.530023	1350.684427	17.699290
35.778065	1366.522727	17.704307
36.300226	1369.767676	17.709325
36.195892	1365.766584	17.714343
36.089172	1364.400970	17.719360
36.486922	1357.408890	17.724378
36.358387	1360.985522	17.729395
36.385243	1364.563208	17.734413
36.335086	1351.600638	17.739431
36.105393	1353.365803	17.744448
36.533080	1350.411662	17.749466
36.439152	1344.193574	17.754483
36.219437	1337.546947	17.759501
36.167975	1343.437409	17.764519
36.401672	1353.767885	17.769536
36.196494	1353.528447	17.774554
36.730916	1361.748204	17.779571
36.676473	1366.547226	17.784589
36.855482	1355.016427	17.789607
36.760058	1358.417490	17.794624
36.567948	1359.185878	17.799642
36.976161	1362.691565	17.804659
36.670311	1359.027964	17.809677
36.973794	1355.897499	17.814695
36.538211	1357.985056	17.819712
36.683406	1348.889503	17.824730
36.478643	1355.299299	17.829747
36.297751	1362.488024	17.834765
36.560163	1352.582109	17.839783
36.292195	1349.032533	17.844800
37.061544	1364.265801	17.849818
37.273481	1379.216638	17.854835
36.895584	1363.183983	17.859853
36.931477	1361.726737	17.864871
37.358339	1373.463045	17.869888
37.304880	1369.668627	17.874906
37.272122	1361.235093	17.879923
37.055466	1360.864899	17.884941
37.441886	1354.095491	17.889959
36.738112	1368.245303	17.894976
37.313216	1369.702129	17.899994
37.284513	1374.105823	17.905011
37.386295	1367.194534	17.910029
37.461645	1368.902740	17.915047
37.136250	1373.974324	17.920064
37.222700	1366.734061	17.925082
37.055482	1372.008236	17.930099
37.157934	1377.650682	17.935117
37.570228	1385.820037	17.940135
37.769722	1392.955861	17.945152
38.013436	1396.509257	17.950170
38.137685	1385.703336	17.955187
37.972529	1381.509737	17.960205
37.625099	1369.732688	17.965223
37.870126	1384.340706	17.970240
37.768281	1387.114766	17.975258
37.782810	1391.836783	17.980275
37.826140	1386.619795	17.985293
38.399270	1394.596855	17.990311
38.156118	1389.503366	17.995328
38.056430	1395.019499	18.000346
38.125556	1383.739321	18.005363
38.039887	1391.355045	18.010381
38.191134	1387.897982	18.015399
38.279400	1393.911873	18.020416
38.139058	1387.328609	18.025434
38.131469	1393.108114	18.030451
38.039464	1393.942970	18.035469
38.551212	1386.819520	18.040487
38.353558	1388.627037	18.045504
38.565026	1393.189004	18.050522
38.747633	1396.054477	18.055539
38.461927	1389.288717	18.060557
38.293228	1384.272001	18.065575
38.177096	1395.527974	18.070592
38.399148	1391.321424	18.075610
38.517549	1401.190194	18.080627
38.631798	1408.033181	18.085645
38.876341	1414.420381	18.090663
38.829107	1414.203689	18.095680
38.910427	1411.240349	18.100698
39.089130	1408.448042	18.105715
38.838685	1409.604214	18.110733
38.984176	1405.049817	18.115751
38.744677	1409.107641	18.120768
38.824705	1406.163439	18.125786
39.194338	1414.377319	18.130803
38.960921	1416.531237	18.135821
38.724071	1408.880543	18.140839
38.672192	1416.030267	18.145856
38.832802	1411.804876	18.150874
39.238468	1439.651860	18.155891
39.499162	1436.180903	18.160909
39.960426	1427.004541	18.165927
39.458521	1431.977391	18.170944
39.080642	1426.586129	18.175962
39.302039	1433.952090	18.180979
39.583295	1435.527256	18.185997
39.448789	1429.665753	18.191015
39.749864	1436.489131	18.196032
39.465875	1437.615813	18.201050
39.695587	1439.252654	18.206067
39.341553	1436.615871	18.211085
39.633610	1436.680870	18.216103
39.502602	1435.366370	18.221120
39.869126	1424.364913	18.226138
39.783955	1426.281154	18.231155
39.955237	1430.423350	18.236173
39.868237	1422.957604	18.241191
40.010204	1425.024674	18.246208
39.617774	1430.138270	18.251226
40.013810	1431.935408	18.256243
39.815634	1439.057426	18.261261
40.121215	1441.146361	18.266279
40.292596	1451.931569	18.271296
39.912410	1449.440868	18.276314
40.271618	1452.218894	18.281331
39.993860	1463.967138	18.286349
40.054889	1451.353260	18.291367
40.021869	1460.115851	18.296384
39.977216	1457.945296	18.301402
40.174637	1459.186376	18.306419
40.066388	1472.202125	18.311437
40.450586	1470.955730	18.316455
40.433436	1484.743107	18.321472
40.629862	1486.050616	18.326490
41.155977	1487.398314	18.331507
40.857870	1491.746151	18.336525
40.758309	1481.186460	18.341543
40.489908	1471.438865	18.346560
40.512309	1479.867786	18.351578
40.766659	1477.546533	18.356595
40.824576	1490.823604	18.361613
41.029451	1486.562901	18.366631
40.958509	1482.461909	18.371648
40.876625	1483.146868	18.376666
41.165998	1486.661615	18.381683
40.956267	1492.952312	18.386701
40.786536	1498.116461	18.391719
41.005945	1489.583645	18.396736
41.064534	1482.278245	18.401754
41.185284	1474.628651	18.406771
40.800224	1481.454732	18.411789
41.066381	1486.513141	18.416807
41.325892	1495.460580	18.421824
41.074661	1506.945943	18.426842
41.283359	1495.681834	18.431859
41.526413	1505.266163	18.436877
41.836961	1506.189828	18.441895
41.615790	1500.944560	18.446912
41.482132	1499.157091	18.451930
41.539707	1500.293714	18.456947
41.823399	1508.546265	18.461965
41.921070	1503.876211	18.466983
41.878321	1499.392124	18.472000
41.680523	1503.831645	18.477018
41.767404	1489.960847	18.482035
42.146149	1497.491687	18.487053
42.131449	1496.973279	18.492071
42.121842	1500.802825	18.497088
42.370472	1500.735729	18.502106
41.839421	1500.502844	18.507123
41.734272	1508.172145	18.512141
41.946768	1496.579236	18.517159
41.718844	1499.284580	18.522176
42.131771	1513.689835	18.527194
42.642631	1519.906219	18.532211
42.067239	1514.517280	18.537229
42.343851	1519.829694	18.542247
42.605072	1521.086092	18.547264
42.099341	1526.214199	18.552282
42.408856	1523.862260	18.557299
42.337826	1526.991310	18.562317
42.275932	1522.750042	18.567335
42.328653	1527.182123	18.572352
42.222918	1528.113798	18.577370
42.610851	1514.918796	18.582387
42.291605	1525.843553	18.587405
42.132664	1526.313291	18.592423
42.370913	1540.594284	18.597440
42.677295	1539.804975	18.602458
43.007173	1542.044776	18.607475
42.875582	1537.830135	18.612493
42.963181	1537.488306	18.617511
43.194247	1533.646397	18.622528
43.321344	1541.733994	18.627546
43.306715	1541.714198	18.632563
43.149035	1543.506040	18.637581
42.900632	1526.888179	18.642599
43.283738	1529.119691	18.647616
42.972795	1540.324035	18.652634
43.362382	1539.427096	18.657651
43.233078	1538.547829	18.662669
43.125896	1532.325427	18.667687
43.168538	1535.540923	18.672704
43.344833	1545.053616	18.677722
43.707806	1546.300485	18.682739
43.554853	1557.448682	18.687757
43.711073	1556.666973	18.692775
44.254354	1561.959972	18.697792
43.415147	1556.438523	18.702810
43.778249	1555.930720	18.707827
43.714642	1561.311897	18.712845
44.114461	1562.183795	18.717863
43.775219	1559.658301	18.722880
43.810742	1567.495077	18.727898
44.097684	1554.931160	18.732915
44.154468	1562.568961	18.737933
44.014587	1559.327608	18.742951
43.962763	1554.182191	18.747968
43.977044	1564.957213	18.752986
44.222424	1555.148514	18.758003
43.848801	1558.113239	18.763021
43.985639	1566.385526	18.768039
44.186617	1554.106398	18.773056
44.144126	1556.801815	18.778074
44.311671	1555.387172	18.783091
44.042261	1565.174400	18.788109
44.445912	1572.919147	18.793127
44.680479	1573.409671	18.798144
44.596190	1581.463925	18.803162
44.832377	1585.981067	18.808179
44.456788	1589.028156	18.813197
44.630105	1581.199916	18.818215
44.917133	1572.530298	18.823232
44.627952	1582.314302	18.828250
44.305782	1573.644857	18.833267
44.463533	1576.214424	18.838285
44.096388	1576.909086	18.843303
44.752563	1592.188574	18.848320
44.900023	1603.583522	18.853338
45.184281	1599.812214	18.858355
45.271371	1604.765991	18.863373
44.919499	1595.861315	18.868391
45.225869	1599.594348	18.873408
45.289377	1603.403065	18.878426
45.426516	1599.316986	18.883443
45.417095	1607.050321	18.888461
45.281773	1607.942424	18.893479
45.426237	1606.521903	18.898496
45.234066	1606.539217	18.903514
45.277828	1601.104346	18.908531
45.201214	1609.413042	18.913549
45.189496	1604.640070	18.918567
45.223781	1604.906153	18.923584
45.378349	1619.828254	18.928602
45.821120	1618.809419	18.933619
45.770480	1624.333766	18.938637
45.537054	1629.697221	18.943655
45.992498	1623.854257	18.948672
45.497393	1628.447397	18.953690
45.872627	1634.249429	18.958707
46.085116	1635.292512	18.963725
46.035722	1628.278425	18.968743
46.541158	1617.788562	18.973760
46.091571	1630.097008	18.978778
46.435550	1620.818886	18.983795
46.380097	1622.717898	18.988813
45.962315	1624.856363	18.993831
46.317933	1630.134418	18.998848
46.515629	1630.409774	19.003866
46.548242	1612.002889	19.008883
46.628059	1620.388222	19.013901
46.543068	1625.570772	19.018919
47.038843	1605.763164	19.023936
46.504323	1612.442148	19.028954
46.752271	1613.536515	19.033971
46.854650	1617.837808	19.038989
46.524313	1620.578050	19.044007
46.764272	1615.418746	19.049024
46.405882	1618.901827	19.054042
46.587480	1619.952874	19.059059
46.713048	1614.429521	19.064077
46.595969	1614.103778	19.069095
46.873497	1623.370374	19.074112
46.915984	1637.158050	19.079130
47.096514	1639.490546	19.084147
47.116589	1639.105578	19.089165
46.964457	1639.842507	19.094183
47.170767	1645.976962	19.099200
47.204998	1648.916072	19.104218
47.054511	1640.377657	19.109235
47.254181	1641.624712	19.114253
47.084692	1648.859114	19.119271
47.067054	1652.292303	19.124288
47.162346	1660.507985	19.129306
47.401684	1657.662016	19.134323
47.853969	1655.792771	19.139341
47.822005	1660.089744	19.144359
47.592486	1653.999958	19.149376
47.701414	1667.221881	19.154394
47.572260	1657.913261	19.159411
47.668102	1659.258535	19.164429
47.454617	1665.347901	19.169447
47.599358	1650.549612	19.174464
47.883888	1665.479920	19.179482
47.825325	1680.009212	19.184499
47.854136	1687.162261	19.189517
48.183632	1681.206341	19.194535
48.636732	1674.079285	19.199552
47.950390	1683.423397	19.204570
48.377230	1675.587203	19.209587
48.635551	1673.681881	19.214605
48.187017	1678.744320	19.219623
48.261671	1671.164937	19.224640
48.677862	1675.010278	19.229658
48.411848	1674.360577	19.234675
48.569009	1672.559370	19.239693
48.607664	1681.828473	19.244711
48.954431	1672.755021	19.249728
48.901940	1674.069741	19.254746
48.636029	1675.992058	19.259763
48.932489	1674.547867	19.264781
48.916874	1680.133051	19.269799
49.215072	1670.726329	19.274816
49.210444	1666.094250	19.279834
49.043878	1669.616904	19.284851
49.264970	1670.560818	19.289869
49.012916	1674.481799	19.294887
49.241139	1674.843922	19.299904
48.813030	1671.546436	19.304922
48.840565	1674.625451	19.309939
49.099024	1666.458864	19.314957
48.833024	1670.909045	19.319975
48.877737	1670.627540	19.324992
48.820837	1676.913442	19.330010
48.767369	1692.581221	19.335027
49.072366	1694.370470	19.340045
49.177499	1702.572015	19.345063
49.323413	1697.402083	19.350080
49.301735	1707.204467	19.355098
49.525881	1714.866769	19.360115
49.957454	1718.308929	19.365133
49.690693	1720.004159	19.370151
50.168237	1718.503368	19.375168
49.711123	1715.282975	19.380186
49.873522	1714.976835	19.385203
50.414108	1713.298967	19.390221
50.131998	1721.750166	19.395239
50.182038	1710.172945	19.400256
50.248510	1708.057643	19.405274
50.053194	1714.141042	19.410291
50.543023	1706.885176	19.415309
50.413921	1709.224862	19.420327
50.477094	1708.148358	19.425344
50.576823	1696.806411	19.430362
50.432029	1705.305652	19.435379
50.786118	1698.695787	19.440397
50.382739	1700.866733	19.445415
51.050864	1692.289204	19.450432
50.679125	1704.285772	19.455450
50.614528	1695.610879	19.460467
51.093943	1695.930738	19.465485
50.697062	1706.908719	19.470503
50.619870	1700.337599	19.475520
50.935277	1701.834888	19.480538
50.791891	1707.518870	19.485555
51.112512	1692.387043	19.490573
50.539433	1701.347448	19.495591
50.766930	1696.751806	19.500608
51.027965	1705.670710	19.505626
51.384462	1722.249852	19.510643
51.377573	1724.917659	19.515661
51.300519	1729.186955	19.520679
51.408405	1727.822614	19.525696
51.792603	1722.776524	19.530714
51.545470	1724.970484	19.535731
51.795595	1721.081386	19.540749
51.644057	1729.600624	19.545767
51.551620	1722.309172	19.550784
51.900125	1720.459234	19.555802
51.588606	1726.159932	19.560819
51.895501	1714.757317	19.565837
51.897698	1713.147494	19.570855
52.119461	1709.979198	19.575872
51.907448	1703.280741	19.580890
51.682715	1708.343059	19.585907
52.059973	1716.748401	19.590925
52.066274	1708.002502	19.595943
52.233755	1712.713414	19.600960
52.282472	1708.701038	19.605978
51.862595	1713.935755	19.610995
52.105450	1713.471917	19.616013
51.921045	1718.679440	19.621031
51.866328	1710.122925	19.626048
51.865682	1711.849308	19.631066
51.867156	1718.100889	19.636083
52.035200	1735.154362	19.641101
52.327322	1735.127832	19.646119
52.499222	1733.567327	19.651136
52.832997	1738.094561	19.656154
52.547757	1738.262068	19.661171
52.771382	1729.018408	19.666189
52.546967	1727.885690	19.671207
52.427561	1737.977869	19.676224
52.775579	1755.915391	19.681242
52.621644	1758.965868	19.686259
53.185651	1757.274883	19.691277
53.261686	1759.977123	19.696295
53.147591	1764.362650	19.701312
53.203442	1751.427467	19.706330
53.203120	1763.407273	19.711347
53.187056	1752.361038	19.716365
53.100741	1750.140128	19.721383
53.286150	1752.345644	19.726400
53.419679	1748.436822	19.731418
53.477842	1755.244493	19.736435
53.687847	1771.960101	19.741453
53.863149	1775.356963	19.746471
53.501759	1777.972672	19.751488
53.999889	1776.149926	19.756506
53.761529	1777.465190	19.761523
53.511242	1786.602604	19.766541
54.042568	1781.233781	19.771559
54.237288	1777.002994	19.776576
54.255055	1779.739556	19.781594
53.924359	1785.310711	19.786611
54.237568	1770.905826	19.791629
54.011549	1777.252809	19.796647
54.272115	1773.863860	19.801664
54.382920	1768.803517	19.806682
53.921008	1781.356989	19.811699
54.045661	1783.871778	19.816717
54.395146	1778.360850	19.821735
54.198842	1778.931087	19.826752
54.124352	1775.291339	19.831770
54.187371	1798.038668	19.836787
54.393365	1801.402353	19.841805
54.588706	1797.212491	19.846823
55.036790	1803.353540	19.851840
54.746531	1802.650802	19.856858
54.457043	1810.241633	19.861875
54.970320	1805.061811	19.866893
54.953009	1799.074639	19.871911
54.689686	1799.866756	19.876928
54.686232	1799.513851	19.881946
54.478306	1822.899860	19.886963
54.966347	1826.295378	19.891981
55.200728	1826.754379	19.896999
55.162585	1825.236037	19.902016
55.477588	1820.715104	19.907034
55.217712	1831.712857	19.912051
55.641973	1820.515970	19.917069
55.519662	1819.528300	19.922087
55.414922	1830.000111	19.927104
55.741426	1821.715558	19.932122
55.780462	1821.034135	19.937139
55.573321	1818.052523	19.942157
55.495374	1832.439786	19.947175
55.589132	1845.869337	19.952192
55.775163	1846.623053	19.957210
55.768118	1850.458587	19.962227
55.721237	1852.949598	19.967245
55.615201	1844.634545	19.972263
55.673615	1859.707522	19.977280
56.014695	1847.497900	19.982298
55.951850	1856.691376	19.987315
56.002071	1872.330545	19.992333
56.313803	1873.285605	19.997351
56.164247	1874.413474	20.002368
56.411906	1864.566380	20.007386
56.517186	1872.054747	20.012403
56.689721	1870.301621	20.017421
56.646257	1874.294314	20.022439
56.433764	1883.725704	20.027456
56.735799	1877.139657	20.032474
56.561541	1876.153760	20.037491
56.733732	1871.241626	20.042509
56.780377	1869.662740	20.047527
56.978620	1888.321170	20.052544
57.549052	1880.860174	20.057562
57.244306	1874.065634	20.062579
57.035979	1869.389476	20.067597
56.972326	1862.671016	20.072615
56.994618	1886.927009	20.077632
57.530423	1876.893030	20.082650
57.503946	1878.550864	20.087667
57.577053	1878.132387	20.092685
57.807298	1881.312425	20.097703
57.215235	1886.728639	20.102720
57.509856	1885.354148	20.107738
57.741178	1885.952487	20.112755
57.567660	1883.271751	20.117773
57.624313	1883.483861	20.122791
57.513564	1885.874364	20.127808
57.631616	1880.219551	20.132826
57.493971	1884.031243	20.137843
57.736696	1895.812346	20.142861
58.129326	1896.372947	20.147879
57.812148	1915.509297	20.152896
58.137789	1908.531386	20.157914
57.975941	1912.223772	20.162931
58.287889	1914.463257	20.167949
58.559160	1905.281518	20.172967
58.068496	1910.546248	20.177984
58.556737	1905.010521	20.183002
58.712316	1910.878402	20.188019
58.587536	1909.906891	20.193037
58.906924	1915.225388	20.198055
58.652609	1906.112856	20.203072
58.755248	1900.716065	20.208090
58.815214	1903.493415	20.213107
58.535555	1903.385490	20.218125
58.843971	1902.213984	20.223143
58.928407	1913.770426	20.228160
58.750077	1922.849368	20.233178
58.924615	1925.858200	20.238195
58.567280	1929.751445	20.243213
59.310172	1921.335742	20.248231
59.236576	1939.844039	20.253248
59.498035	1936.180355	20.258266
59.024985	1928.660891	20.263283
59.086077	1933.034963	20.268301
59.296718	1922.410934	20.273319
59.157187	1936.618514	20.278336
59.352210	1938.847804	20.283354
59.590784	1947.606219	20.288371
60.101300	1953.535621	20.293389
59.612582	1955.969201	20.298407
59.896427	1953.068918	20.303424
59.937460	1960.365345	20.308442
59.826148	1953.404954	20.313459
59.772679	1948.120820	20.318477
60.111032	1945.013228	20.323495
59.943055	1950.697960	20.328512
60.030446	1950.573914	20.333530
59.685328	1944.350542	20.338547
59.564399	1958.337486	20.343565
60.174404	1951.267946	20.348583
59.859157	1965.468192	20.353600
60.106242	1955.494901	20.358618
59.946889	1957.826706	20.363635
60.271165	1973.682080	20.368653
60.351526	1987.404168	20.373671
60.343376	1989.387376	20.378688
60.665581	1988.223185	20.383706
60.888452	1992.477406	20.388723
60.666406	1984.663208	20.393741
60.848847	1990.466970	20.398759
60.887475	2012.621899	20.403776
61.178284	2004.560579	20.408794
61.672797	2003.170737	20.413811
61.909379	1995.610188	20.418829
61.725445	1975.273657	20.423847
61.755210	1979.453795	20.428864
61.568003	1973.145865	20.433882
61.930017	1985.571198	20.438899
61.529277	1980.492607	20.443917
61.739252	1976.978948	20.448935
61.571509	1974.284676	20.453952
61.315940	1966.816544	20.458970
62.361627	1969.140620	20.463987
61.795788	1970.178668	20.469005
61.629399	1967.768219	20.474023
61.543586	1964.748756	20.479040
61.646274	1974.434090	20.484058
61.870022	1989.121659	20.489075
62.016840	1995.202379	20.494093
62.255111	1992.817289	20.499111
62.226569	1999.884715	20.504128
62.551839	2000.932353	20.509146
62.572531	1994.399534	20.514163
62.195578	2002.029311	20.519181
62.272898	1989.983740	20.524199
62.267153	1992.714528	20.529216
62.440794	1989.828241	20.534234
62.318584	1995.256543	20.539251
62.278662	2007.340513	20.544269
62.375893	2015.758036	20.549287
62.412740	2027.366144	20.554304
62.596176	2031.825338	20.559322
62.790523	2027.503027	20.564339
62.880295	2046.348931	20.569357
62.877866	2050.998020	20.574375
62.923617	2057.839298	20.579392
63.245986	2049.728860	20.584410
63.160495	2043.070540	20.589427
62.953683	2058.226005	20.594445
63.516315	2041.389868	20.599463
63.100706	2049.795732	20.604480
63.070839	2056.093337	20.609498
63.671656	2073.622575	20.614515
63.397607	2077.670149	20.619533
63.738938	2073.536391	20.624551
63.784051	2072.888728	20.629568
63.638971	2074.672349	20.634586
63.620715	2066.299343	20.639603
63.530748	2074.578775	20.644621
63.927374	2077.859181	20.649639
64.174303	2095.358328	20.654656
64.114676	2095.973570	20.659674
64.418029	2087.632536	20.664691
64.382706	2093.296660	20.669709
64.950993	2097.011111	20.674727
64.628564	2093.491955	20.679744
64.993036	2084.339797	20.684762
64.659456	2073.835126	20.689779
64.431432	2071.768789	20.694797
64.533898	2076.985403	20.699815
64.334575	2088.062251	20.704832
64.601903	2090.204560	20.709850
64.730101	2089.064257	20.714867
64.634192	2095.331132	20.719885
65.050244	2092.044153	20.724903
65.041805	2090.543255	20.729920
64.955795	2083.638836	20.734938
65.024299	2099.060753	20.739955
64.842110	2107.294595	20.744973
65.270981	2106.375734	20.749991
65.254247	2115.050900	20.755008
65.113738	2111.326683	20.760026
65.291702	2113.694357	20.765043
65.284466	2124.539340	20.770061
65.652245	2126.303079	20.775079
65.314690	2139.566463	20.780096
65.467096	2140.890343	20.785114
65.812545	2137.933100	20.790131
65.606664	2141.174775	20.795149
66.002338	2124.134171	20.800167
66.127401	2136.747987	20.805184
65.803075	2134.668233	20.810202
65.977294	2131.914383	20.815219
65.986709	2150.075442	20.820237
66.335851	2152.561643	20.825255
66.471650	2156.744249	20.830272
66.436269	2156.538326	20.835290
66.520954	2152.425572	20.840307
66.417902	2158.867159	20.845325
66.521668	2153.788868	20.850343
66.776925	2159.770706	20.855360
66.525991	2155.205253	20.860378
66.723639	2150.702510	20.865395
66.434811	2164.204490	20.870413
66.751349	2176.318285	20.875431
66.896640	2184.605322	20.880448
66.631270	2189.241735	20.885466
67.361766	2190.504017	20.890483
67.357180	2187.923172	20.895501
67.570155	2182.057815	20.900519
67.356250	2186.591536	20.905536
67.216179	2177.069739	20.910554
67.079721	2173.575264	20.915571
67.025916	2189.694832	20.920589
67.495112	2197.281318	20.925607
67.670810	2207.394090	20.930624
67.493682	2205.285097	20.935642
67.800046	2204.401085	20.940659
67.430186	2208.940156	20.945677
67.817621	2204.751851	20.950695
67.967340	2211.239312	20.955712
68.166205	2224.400305	20.960730
68.291330	2223.853795	20.965747
68.479913	2220.595896	20.970765
68.471669	2222.124685	20.975783
68.574324	2226.968909	20.980800
68.440718	2218.837865	20.985818
68.663256	2217.790169	20.990835
68.449847	2219.833763	20.995853
68.409618	2217.779198	21.000871
68.754728	2218.290401	21.005888
68.691281	2223.977881	21.010906
68.915925	2210.807792	21.015923
68.544895	2218.752334	21.020941
69.105791	2219.744363	21.025959
69.108110	2220.242662	21.030976
68.778923	2222.316907	21.035994
69.124374	2206.969330	21.041011
69.055078	2218.796070	21.046029
69.234244	2232.449311	21.051047
69.575902	2240.295525	21.056064
69.281733	2238.817010	21.061082
69.507891	2244.427846	21.066099
69.557030	2246.206492	21.071117
69.853763	2238.721687	21.076135
69.552573	2238.459313	21.081152
69.389179	2247.359359	21.086170
69.690053	2230.311322	21.091187
69.514087	2239.557322	21.096205
69.937407	2242.707364	21.101223
70.127175	2256.750314	21.106240
70.103130	2266.793227	21.111258
70.334441	2257.396612	21.116275
70.411229	2266.944119	21.121293
70.143572	2259.686041	21.126311
70.153260	2262.550173	21.131328
70.260133	2267.081310	21.136346
70.097472	2261.902451	21.141363
70.305936	2279.600281	21.146381
70.348226	2291.229805	21.151399
70.972595	2288.424782	21.156416
70.616930	2290.856626	21.161434
70.661095	2295.100871	21.166451
70.814808	2292.536393	21.171469
70.674890	2293.179922	21.176487
71.339103	2305.608924	21.181504
71.131450	2308.532150	21.186522
71.300775	2311.302005	21.191539
71.210657	2311.966185	21.196557
71.441194	2306.685067	21.201575
71.475588	2301.825830	21.206592
71.641734	2297.271147	21.211610
71.849977	2280.780313	21.216627
72.125787	2289.495227	21.221645
72.267471	2285.124247	21.226663
72.594433	2279.402066	21.231680
72.304615	2283.108140	21.236698
72.347994	2281.229909	21.241715
72.491594	2282.432087	21.246733
72.125720	2273.421948	21.251751
72.414433	2262.533084	21.256768
72.027743	2261.378257	21.261786
72.607764	2270.531818	21.266803
72.732725	2277.799528	21.271821
72.520321	2279.533687	21.276839
72.775785	2270.152240	21.281856
72.382628	2277.226048	21.286874
72.662440	2276.870058	21.291891
72.764181	2276.491298	21.296909
72.386797	2281.520735	21.301927
72.882712	2276.529685	21.306944
72.593832	2276.221210	21.311962
72.621667	2274.219160	21.316979
72.827953	2281.313255	21.321997
72.651508	2294.078273	21.327015
72.770276	2296.843373	21.332032
72.849964	2302.514904	21.337050
73.165246	2303.267453	21.342067
73.332476	2300.609345	21.347085
73.241421	2327.944885	21.352103
73.933117	2327.755154	21.357120
73.844147	2330.824017	21.362138
74.239645	2320.369798	21.367155
74.168332	2326.178462	21.372173
73.673079	2321.729905	21.377191
74.098004	2320.619134	21.382208
73.902353	2320.056287	21.387226
73.922342	2317.926059	21.392243
74.158026	2315.825368	21.397261
74.251745	2327.857187	21.402279
74.205109	2314.243237	21.407296
74.361678	2311.529979	21.412314
74.519218	2311.578056	21.417331
74.241400	2331.257863	21.422349
74.030485	2344.119806	21.427367
75.020547	2346.023381	21.432384
74.788868	2348.890392	21.437402
74.445950	2344.200348	21.442419
74.542320	2341.095648	21.447437
75.062456	2348.816287	21.452455
75.161658	2357.366216	21.457472
74.920599	2371.722500	21.462490
74.938017	2371.953349	21.467507
75.138680	2368.920775	21.472525
75.101536	2370.100604	21.477543
75.101158	2362.526299	21.482560
75.335281	2379.371272	21.487578
75.453913	2388.612509	21.492595
75.755799	2391.790953	21.497613
75.646225	2394.806227	21.502631
75.853294	2391.147764	21.507648
75.757969	2400.939903	21.512666
75.576675	2397.957325	21.517683
75.979386	2395.530800	21.522701
75.841072	2423.315683	21.527719
75.918981	2424.638559	21.532736
75.891771	2418.349744	21.537754
75.959056	2418.045778	21.542771
76.247948	2426.477838	21.547789
76.386967	2441.551378	21.552807
76.581968	2443.859635	21.557824
76.438916	2451.188080	21.562842
76.525598	2442.022183	21.567859
76.597543	2449.929418	21.572877
76.649894	2452.556551	21.577895
76.701670	2459.753673	21.582912
76.972487	2470.773339	21.587930
77.124878	2475.565703	21.592947
77.156949	2467.228859	21.597965
77.023524	2470.696012	21.602983
77.326715	2472.340446	21.608000
77.173856	2472.345327	21.613018
77.256489	2476.836107	21.618035
77.458245	2485.089244	21.623053
77.460339	2495.446974	21.628071
77.571403	2498.446849	21.633088
77.727509	2496.879270	21.638106
77.424058	2484.649638	21.643123
78.165557	2492.850304	21.648141
77.817559	2491.894578	21.653159
78.070748	2491.994040	21.658176
78.273704	2502.980107	21.663194
78.615277	2509.106425	21.668211
78.751658	2508.507657	21.673229
78.513996	2507.509503	21.678247
78.386975	2508.857980	21.683264
78.391457	2514.437139	21.688282
78.319790	2519.027697	21.693299
78.575823	2508.737104	21.698317
78.867489	2511.415354	21.703335
78.861489	2505.034839	21.708352
79.160688	2508.683968	21.713370
79.159973	2501.781888	21.718387
79.339187	2502.744992	21.723405
79.192020	2508.038470	21.728423
79.192598	2496.414790	21.733440
79.487034	2502.106601	21.738458
79.252703	2510.692752	21.743475
79.586267	2523.217570	21.748493
79.533635	2519.668948	21.753511
79.441559	2529.372282	21.758528
79.524192	2527.023979	21.763546
79.381774	2521.321149	21.768563
79.741896	2526.696608	21.773581
79.928553	2538.430056	21.778599
79.938853	2544.989842	21.783616
80.110850	2547.134424	21.788634
79.958889	2540.419991	21.793651
80.396980	2536.949607	21.798669
80.492964	2537.616381	21.803687
80.563370	2541.335856	21.808704
80.585041	2549.310927	21.813722
80.668717	2558.986914	21.818739
81.016418	2560.561306	21.823757
80.883490	2574.361236	21.828775
80.706426	2570.604743	21.833792
81.231241	2567.076667	21.838810
81.117486	2567.971771	21.843827
80.876264	2565.964239	21.848845
81.006746	2572.675748	21.853863
81.078662	2568.886803	21.858880
81.397600	2561.284790	21.863898
81.247608	2570.299682	21.868915
81.576399	2578.267978	21.873933
81.464845	2591.221933	21.878951
81.848173	2594.236244	21.883968
81.620393	2597.197367	21.888986
81.648178	2596.366178	21.894003
82.048296	2598.509966	21.899021
82.011542	2593.989954	21.904039
82.066893	2591.260854	21.909056
82.195169	2600.036762	21.914074
81.756801	2595.301549	21.919091
82.161710	2612.236923	21.924109
82.520159	2611.133328	21.929127
82.402018	2618.659949	21.934144
82.394359	2615.385193	21.939162
82.284792	2621.799555	21.944179
82.618215	2626.065120	21.949197
82.449388	2640.467181	21.954215
82.682885	2638.057502	21.959232
82.947484	2632.881446	21.964250
82.541085	2634.330238	21.969267
82.757826	2641.489126	21.974285
82.916795	2644.251176	21.979303
83.170851	2653.534587	21.984320
83.485505	2657.500101	21.989338
83.149697	2651.385493	21.994355
83.422119	2646.814176	21.999373
83.576506	2661.093342	22.004391
83.765089	2659.362890	22.009408
83.631873	2661.548695	22.014426
83.738403	2675.333512	22.019443
83.987145	2676.004912	22.024461
83.855926	2682.107063	22.029479
83.961324	2679.341752	22.034496
84.116789	2671.370639	22.039514
83.941057	2679.695264	22.044531
84.409356	2678.255801	22.049549
84.703930	2697.799550	22.054567
84.455227	2699.627769	22.059584
84.560234	2704.487537	22.064602
84.501668	2701.043952	22.069619
84.923578	2698.740640	22.074637
85.104732	2703.746355	22.079655
84.883178	2704.083847	22.084672
85.129726	2705.939110	22.089690
84.982187	2695.076878	22.094707
85.014441	2693.004660	22.099725
84.948678	2714.431883	22.104743
85.378668	2719.490385	22.109760
85.271148	2714.750969	22.114778
85.403811	2728.440233	22.119795
85.648700	2726.558986	22.124813
85.597725	2726.746835	22.129831
85.788599	2745.451490	22.134848
85.782576	2747.241930	22.139866
85.622218	2747.052302	22.144883
85.841813	2743.805262	22.149901
86.244882	2752.680484	22.154919
86.002269	2758.787379	22.159936
86.448494	2767.725323	22.164954
86.490175	2770.104834	22.169971
86.723073	2775.105669	22.174989
86.791602	2781.514452	22.180007
86.537686	2776.658945	22.185024
86.861379	2773.888038	22.190042
86.735674	2769.384988	22.195059
86.648341	2769.168210	22.200077
86.480469	2781.225280	22.205095
86.877134	2792.007782	22.210112
87.448193	2791.167745	22.215130
87.194132	2799.854943	22.220147
87.053340	2800.296638	22.225165
87.407849	2798.969565	22.230183
87.560023	2797.156399	22.235200
87.679188	2804.065434	22.240218
87.660700	2819.024947	22.245235
87.487345	2818.742660	22.250253
87.913367	2816.138866	22.255271
88.246563	2805.059697	22.260288
88.369489	2803.803396	22.265306
88.690796	2798.328106	22.270323
88.855665	2791.011938	22.275341
88.824001	2783.792649	22.280359
88.699065	2793.570676	22.285376
88.938117	2789.474772	22.290394
88.864306	2785.945175	22.295411
88.741361	2790.243960	22.300429
88.983148	2786.450613	22.305447
89.070378	2783.681803	22.310464
89.045144	2786.904937	22.315482
88.939659	2792.845314	22.320499
88.861647	2787.454291	22.325517
89.021495	2785.905041	22.330535
89.065237	2788.438881	22.335552
89.101861	2783.613883	22.340570
89.040083	2797.494433	22.345587
89.142786	2803.762193	22.350605
89.374132	2806.740237	22.355623
89.512136	2808.470387	22.360640
89.789117	2808.910158	22.365658
89.633626	2833.185644	22.370675
89.707884	2838.829785	22.375693
89.892440	2842.386370	22.380711
89.788758	2850.276941	22.385728
89.927959	2843.198298	22.390746
89.966791	2858.761200	22.395763
90.037793	2858.087386	22.400781
90.499518	2862.771727	22.405799
90.111583	2865.530591	22.410816
90.397770	2871.504696	22.415834
90.478171	2896.078084	22.420851
90.660877	2887.941673	22.425869
91.106912	2895.358479	22.430887
90.856550	2900.273628	22.435904
91.337545	2901.271827	22.440922
91.300413	2913.324410	22.445939
91.292309	2913.717044	22.450957
91.934769	2918.698338	22.455975
92.243958	2921.222429	22.460992
91.727032	2915.978605	22.466010
91.914911	2920.162750	22.471027
91.836240	2917.369253	22.476045
91.849794	2913.788155	22.481063
91.823213	2912.649806	22.486080
92.378276	2902.994147	22.491098
92.052842	2911.591516	22.496115
91.728504	2905.598123	22.501133
92.106719	2921.231326	22.506151
92.130981	2937.926445	22.511168
92.272553	2938.295776	22.516186
92.414359	2944.399692	22.521203
92.799027	2932.804299	22.526221
92.659177	2945.892315	22.531239
92.740482	2961.177269	22.536256
93.057189	2971.972328	22.541274
93.026996	2972.071729	22.546291
93.099013	2970.226841	22.551309
93.335389	2971.067451	22.556327
93.205502	2964.014875	22.561344
93.418632	2975.854952	22.566362
93.309301	2986.915186	22.571379
93.414514	2991.374174	22.576397
93.556558	2990.588300	22.581415
93.627091	2995.560821	22.586432
93.830723	2999.029252	22.591450
94.009421	3019.440385	22.596467
93.676629	3010.677211	22.601485
94.086880	3006.933336	22.606503
93.896250	3014.888014	22.611520
94.500887	3014.071145	22.616538
94.542397	3026.203087	22.621555
95.083071	3031.872511	22.626573
95.236143	3023.573380	22.631591
94.955202	3029.553777	22.636608
95.029140	3026.007441	22.641626
95.361905	3026.716271	22.646643
95.099729	3024.033386	22.651661
95.219630	3018.573606	22.656679
95.286505	3020.172826	22.661696
95.501992	3008.060875	22.666714
95.409247	3022.508206	22.671731
95.590094	3018.525464	22.676749
95.449938	3012.765316	22.681767
95.376853	3020.392397	22.686784
95.813348	3009.495854	22.691802
95.781173	3016.337006	22.696819
95.881857	3030.069353	22.701837
96.095339	3040.356612	22.706855
95.926175	3039.373011	22.711872
96.405900	3026.471909	22.716890
96.163586	3033.023862	22.721907
95.989340	3030.444062	22.726925
96.681982	3043.708678	22.731943
96.802532	3048.499841	22.736960
96.853911	3052.654771	22.741978
96.843513	3057.422138	22.746995
97.250463	3062.216056	22.752013
97.245976	3049.816402	22.757031
97.144954	3061.787505	22.762048
97.574892	3056.740235	22.767066
97.504823	3052.989075	22.772083
97.436386	3055.808688	22.777101
97.482763	3050.511839	22.782119
97.356580	3063.840834	22.787136
97.166841	3067.443114	22.792154
97.560495	3069.966701	22.797171
97.901286	3072.593202	22.802189
98.307109	3071.094002	22.807207
97.955824	3081.128354	22.812224
98.543256	3087.592170	22.817242
98.772635	3095.598268	22.822259
98.525469	3097.950203	22.827277
98.807849	3095.100465	22.832295
98.740111	3089.679346	22.837312
98.773944	3095.143651	22.842330
98.600949	3097.970082	22.847347
98.701988	3094.959209	22.852365
98.922222	3089.824648	22.857383
98.785515	3106.238841	22.862400
99.159976	3115.083980	22.867418
99.192733	3120.135008	22.872435
99.117290	3128.412664	22.877453
99.020511	3127.619781	22.882471
99.208707	3141.019818	22.887488
99.423869	3150.732463	22.892506
99.665519	3153.014613	22.897523
99.520833	3157.162220	22.902541
99.444194	3163.129790	22.907559
99.527213	3179.910669	22.912576
99.645279	3172.352298	22.917594
100.237112	3190.979211	22.922611
100.547201	3204.773772	22.927629
100.769857	3199.288471	22.932647
100.480706	3193.665083	22.937664
100.532482	3193.606541	22.942682
100.862912	3200.501772	22.947699
100.843345	3199.018295	22.952717
101.160582	3193.600330	22.957735
101.143054	3212.199048	22.962752
101.326023	3211.252141	22.967770
101.484046	3219.360932	22.972787
101.417012	3221.296632	22.977805
101.775039	3214.054372	22.982823
101.657704	3214.814351	22.987840
101.754615	3219.208410	22.992858
102.053163	3215.677564	22.997875
102.120402	3209.711475	23.002893
101.809988	3212.183737	23.007911
101.834794	3216.888855	23.012928
101.647478	3213.496779	23.017946
102.138657	3230.529772	23.022963
101.882835	3232.867292	23.027981
102.234320	3234.434844	23.032999
102.224815	3231.213917	23.038016
102.597040	3254.164287	23.043034
102.687569	3247.162499	23.048051
102.844232	3264.834649	23.053069
102.722106	3255.931247	23.058087
102.931161	3265.038924	23.063104
102.870290	3262.772834	23.068122
103.523675	3272.922301	23.073139
103.601611	3270.792406	23.078157
103.830025	3272.401216	23.083175
103.597513	3278.361531	23.088192
103.600429	3268.472871	23.093210
103.880118	3267.599275	23.098227
103.790872	3268.840930	23.103245
104.046932	3277.379500	23.108263
104.152696	3296.356785	23.113280
104.306075	3299.432267	23.118298
104.403935	3300.647949	23.123315
104.180137	3306.496451	23.128333
104.676597	3295.448373	23.133351
104.558948	3301.750614	23.138368
104.682008	3307.945945	23.143386
104.934451	3320.941594	23.148403
104.783887	3323.581510	23.153421
105.096900	3320.638594	23.158439
105.110677	3317.893764	23.163456
104.705476	3323.906229	23.168474
105.153868	3334.800940	23.173491
104.924508	3350.062000	23.178509
105.180057	3348.292652	23.183527
105.667734	3375.984699	23.188544
105.382171	3383.054811	23.193562
105.562960	3374.931105	23.198579
105.300275	3387.991223	23.203597
105.885060	3396.800600	23.208615
106.063098	3408.933637	23.213632
106.126433	3414.627003	23.218650
106.618883	3405.836149	23.223667
106.626606	3420.116660	23.228685
106.877225	3426.074395	23.233703
106.710295	3430.440148	23.238720
106.935184	3430.553492	23.243738
106.989978	3423.607698	23.248755
106.937869	3428.403750	23.253773
107.203316	3417.962833	23.258791
106.907816	3425.659432	23.263808
107.256870	3443.440676	23.268826
107.401655	3442.752197	23.273843
107.317646	3450.409566	23.278861
107.348498	3450.079693	23.283879
107.336650	3459.670040	23.288896
107.782270	3476.120152	23.293914
108.093254	3473.824547	23.298931
107.975603	3477.560870	23.303949
108.139667	3489.847634	23.308967
108.398603	3494.784648	23.313984
108.440140	3499.386237	23.319002
108.857421	3492.977343	23.324019
108.538210	3501.261561	23.329037
108.666546	3488.784113	23.334055
108.984248	3486.525334	23.339072
108.780117	3490.022629	23.344090
109.357782	3504.113473	23.349107
109.283480	3507.322281	23.354125
109.663465	3505.587199	23.359143
109.563688	3515.270170	23.364160
109.071828	3521.596031	23.369178
109.395226	3513.292250	23.374195
109.735595	3514.025166	23.379213
110.113330	3525.988319	23.384231
110.201889	3530.415316	23.389248
110.337725	3540.361456	23.394266
110.367471	3537.112270	23.399283
110.350366	3532.197595	23.404301
110.156509	3531.609180	23.409319
110.388182	3523.294425	23.414336
110.265906	3532.643195	23.419354
110.758747	3541.264961	23.424371
110.811718	3559.991935	23.429389
110.958219	3564.432013	23.434407
111.351927	3556.426573	23.439424
111.463347	3562.175623	23.444442
111.493689	3557.736453	23.449459
111.358680	3563.040972	23.454477
111.591210	3559.002722	23.459495
111.845974	3564.593738	23.464512
111.601786	3581.911991	23.469530
111.818444	3583.958216	23.474547
112.039126	3587.152673	23.479565
111.885279	3579.027320	23.484583
111.681790	3586.365635	23.489600
111.786650	3603.310787	23.494618
112.427228	3605.565603	23.499635
112.375962	3606.747712	23.504653
112.251678	3617.116295	23.509671
112.437862	3625.157760	23.514688
112.469024	3640.034476	23.519706
112.898667	3630.088649	23.524723
113.835423	3628.670866	23.529741
114.178182	3616.942687	23.534759
114.158033	3612.344085	23.539776
114.199446	3610.567020	23.544794
114.367304	3605.655090	23.549811
114.452113	3610.101628	23.554829
114.452151	3608.750781	23.559847
114.571476	3612.806888	23.564864
114.184441	3604.471644	23.569882
114.427835	3597.957226	23.574899
114.089524	3601.229248	23.579917
114.311421	3604.136305	23.584935
114.364452	3594.732032	23.589952
114.532206	3606.494372	23.594970
114.410889	3608.788904	23.599987
114.550238	3621.335260	23.605005
114.563627	3629.204788	23.610023
114.790939	3640.528632	23.615040
114.790321	3640.916960	23.620058
114.984261	3645.425421	23.625075
115.607197	3658.180571	23.630093
115.210674	3664.327515	23.635111
115.519381	3657.414691	23.640128
115.712275	3673.853834	23.645146
115.889578	3670.581650	23.650163
115.857776	3681.803832	23.655181
116.004573	3679.672637	23.660199
116.350651	3673.502014	23.665216
116.039247	3687.317959	23.670234
116.304713	3686.058342	23.675251
116.578219	3686.255650	23.680269
116.414283	3699.155432	23.685287
116.420020	3700.091955	23.690304
116.409022	3701.779110	23.695322
116.693206	3713.337174	23.700339
116.669779	3718.927364	23.705357
116.914108	3727.868816	23.710375
116.794809	3740.237744	23.715392
116.863886	3747.284345	23.720410
117.635614	3749.222075	23.725427
117.397217	3753.659001	23.730445
117.772725	3757.703661	23.735463
118.004070	3754.552455	23.740480
117.761267	3774.645008	23.745498
118.130539	3775.124093	23.750515
118.371333	3782.159754	23.755533
118.425883	3778.486883	23.760551
118.617837	3777.996204	23.765568
118.447226	3782.858144	23.770586
118.782297	3798.284204	23.775603
119.169448	3796.368074	23.780621
119.052294	3788.192726	23.785639
119.526240	3797.016400	23.790656
119.435001	3793.675537	23.795674
119.719434	3795.761734	23.800691
119.591833	3787.736356	23.805709
119.577704	3793.549214	23.810727
119.643329	3784.193382	23.815744
119.820215	3804.858187	23.820762
120.300178	3806.569912	23.825779
120.084537	3804.621382	23.830797
120.301979	3812.604408	23.835815
120.268917	3813.086165	23.840832
120.370535	3818.991480	23.845850
120.221998	3808.144512	23.850867
120.390502	3824.830620	23.855885
120.556740	3839.850596	23.860903
120.973071	3834.966199	23.865920
120.645802	3841.149764	23.870938
120.640982	3861.274799	23.875955
120.899926	3865.375507	23.880973
120.563105	3879.116648	23.885991
121.183286	3889.934450	23.891008
121.093652	3902.841747	23.896026
121.644469	3898.640241	23.901043
121.810181	3914.499926	23.906061
121.899615	3919.968450	23.911079
122.102015	3911.421355	23.916096
121.830780	3914.165363	23.921114
122.015470	3934.194692	23.926131
122.581603	3930.801955	23.931149
122.431494	3945.549333	23.936167
122.728683	3947.153809	23.941184
122.535412	3959.266120	23.946202
123.012313	3962.196658	23.951219
123.017665	3971.601535	23.956237
123.050973	3973.206066	23.961255
123.587051	3966.633322	23.966272
123.744149	3974.275469	23.971290
123.694302	3971.117504	23.976307
124.118394	3977.455574	23.981325
123.651177	3992.801553	23.986343
123.801544	3989.101096	23.991360
123.742123	3989.908903	23.996378
123.743685	3986.790275	24.001395
124.222134	4008.658248	24.006413
124.395403	4023.948723	24.011431
124.291415	4021.723969	24.016448
124.271336	4019.975376	24.021466
124.628912	4028.691032	24.026483
125.041878	4040.390226	24.031501
124.754537	4045.399818	24.036519
124.965584	4035.389958	24.041536
125.133799	4051.167310	24.046554
125.350851	4046.468542	24.051571
125.606150	4058.084981	24.056589
125.604851	4061.973749	24.061607
125.837577	4065.917614	24.066624
125.643863	4064.581117	24.071642
125.682822	4066.434124	24.076659
126.320158	4072.915779	24.081677
126.035286	4086.882555	24.086695
126.072897	4088.435926	24.091712
126.471149	4086.161376	24.096730
126.709428	4098.462252	24.101747
126.689010	4106.371970	24.106765
126.664133	4111.223934	24.111783
126.869521	4110.825843	24.116800
126.789939	4116.882562	24.121818
127.250540	4126.986778	24.126835
127.140455	4133.745795	24.131853
127.294901	4143.919780	24.136871
127.642603	4146.516958	24.141888
127.566339	4160.265090	24.146906
128.019021	4162.262009	24.151923
128.421984	4161.905752	24.156941
128.079317	4155.236187	24.161959
128.577137	4148.647240	24.166976
128.975013	4150.128744	24.171994
129.059429	4154.307192	24.177011
129.564301	4158.211863	24.182029
129.406589	4145.813217	24.187047
129.508082	4139.573202	24.192064
129.565915	4134.261627	24.197082
129.477153	4130.661498	24.202099
129.993681	4123.873956	24.207117
129.602146	4128.539975	24.212135
129.586888	4140.457408	24.217152
129.797347	4151.307595	24.222170
129.675153	4148.277647	24.227187
130.063117	4150.126825	24.232205
130.198144	4151.027461	24.237223
130.213434	4172.633175	24.242240
130.269430	4187.888390	24.247258
130.401203	4183.963534	24.252275
130.438646	4176.874962	24.257293
130.633458	4188.226304	24.262311
131.046093	4203.823702	24.267328
131.163979	4210.992294	24.272346
130.423573	4211.966104	24.277363
131.041753	4220.221489	24.282381
131.044648	4237.748092	24.287399
131.372639	4230.595325	24.292416
131.807168	4244.750068	24.297434
131.437100	4255.873768	24.302451
131.650301	4264.665673	24.307469
131.355802	4263.228069	24.312487
131.787982	4278.872990	24.317504
132.209859	4290.533084	24.322522
132.304607	4290.729824	24.327539
132.213868	4297.283884	24.332557
132.768452	4314.481631	24.337575
132.805187	4317.363974	24.342592
132.869275	4321.141614	24.347610
133.022227	4326.186892	24.352627
133.328961	4337.817599	24.357645
133.293063	4343.968595	24.362663
133.374776	4341.153062	24.367680
133.797900	4338.776763	24.372698
133.931983	4336.224521	24.377715
134.188930	4330.881888	24.382733
133.887608	4341.584613	24.387751
134.150946	4353.187367	24.392768
134.262514	4352.036887	24.397786
134.074673	4362.677768	24.402803
134.453572	4353.162396	24.407821
134.766473	4376.416972	24.412839
135.006395	4376.041907	24.417856
135.192819	4383.221991	24.422874
134.959758	4382.718559	24.427891
135.231058	4384.172444	24.432909
135.416318	4388.546721	24.437927
135.522799	4394.366245	24.442944
135.630794	4405.712303	24.447962
135.657049	4417.364634	24.452979
136.014398	4405.191786	24.457997
136.063102	4416.215665	24.463015
136.511578	4421.959858	24.468032
136.650460	4418.365262	24.473050
136.240675	4431.916175	24.478067
136.410052	4428.282109	24.483085
136.757672	4437.280428	24.488103
136.805246	4445.217586	24.493120
137.087579	4445.997455	24.498138
136.885655	4458.278733	24.503155
137.264812	4459.166627	24.508173
137.256679	4470.306703	24.513191
137.186882	4483.943601	24.518208
137.372375	4476.522538	24.523226
137.613486	4496.019750	24.528243
137.677707	4500.816913	24.533261
137.551191	4507.064138	24.538279
137.824480	4528.286064	24.543296
137.703318	4530.025167	24.548314
138.125026	4533.283187	24.553331
138.722848	4552.150462	24.558349
138.654708	4553.278445	24.563367
139.075640	4556.593405	24.568384
139.069985	4563.847655	24.573402
139.230975	4579.771787	24.578419
139.473459	4579.203780	24.583437
139.212037	4587.078634	24.588455
139.808958	4590.221006	24.593472
139.797859	4595.957897	24.598490
139.877276	4605.010683	24.603507
140.133725	4598.541220	24.608525
140.284556	4603.350177	24.613543
140.525507	4612.693455	24.618560
140.921998	4614.427725	24.623578
140.921977	4627.949707	24.628595
141.000408	4622.508527	24.633613
141.384985	4621.340777	24.638631
141.703722	4619.473091	24.643648
141.862278	4615.891175	24.648666
141.647642	4617.657465	24.653683
141.719192	4615.500000	24.658701
141.624709	4610.069962	24.663719
141.545863	4605.448682	24.668736
141.728919	4617.878452	24.673754
141.766525	4638.698463	24.678771
141.917775	4640.745524	24.683789
142.064794	4639.706294	24.688807
142.208416	4659.790167	24.693824
142.798870	4664.549633	24.698842
142.494017	4668.814056	24.703859
142.442135	4664.583113	24.708877
142.292337	4684.024601	24.713895
142.963301	4690.943142	24.718912
143.254290	4699.877812	24.723930
142.970527	4715.426255	24.728947
143.399467	4729.051973	24.733965
143.553379	4724.921544	24.738983
143.630940	4726.140483	24.744000
144.064985	4737.470706	24.749018
143.855640	4752.177459	24.754035
144.415494	4747.784970	24.759053
144.401782	4751.688443	24.764071
144.639633	4766.174076	24.769088
144.993331	4765.184727	24.774106
145.017033	4775.745568	24.779123
144.931164	4773.830385	24.784141
145.274692	4770.513187	24.789159
145.262069	4781.650998	24.794176
145.732959	4784.955066	24.799194
145.960268	4792.510873	24.804211
145.782995	4791.616817	24.809229
145.571924	4794.585163	24.814247
145.533346	4795.610710	24.819264
146.124947	4803.870502	24.824282
146.158982	4816.007967	24.829299
146.213591	4815.870068	24.834317
146.515856	4828.783294	24.839335
146.406679	4843.970084	24.844352
147.002878	4826.355968	24.849370
146.841079	4856.319869	24.854387
147.083493	4866.603666	24.859405
147.126825	4857.367539	24.864423
146.859291	4869.318416	24.869440
147.537727	4887.845223	24.874458
147.655425	4894.341795	24.879475
147.502870	4903.891685	24.884493
147.901699	4908.037138	24.889511
148.167734	4922.625826	24.894528
148.390966	4931.710043	24.899546
148.269558	4939.276014	24.904563
148.154823	4946.970364	24.909581
149.021057	4956.270128	24.914599
148.948042	4979.329890	24.919616
149.421767	4962.867876	24.924634
149.245808	4971.316689	24.929651
149.316823	4972.157891	24.934669
149.532621	4975.798416	24.939687
149.944710	4994.066937	24.944704
149.887786	4989.650472	24.949722
149.771934	4992.304163	24.954739
150.258006	5003.550697	24.959757
150.553982	5014.940468	24.964775
150.394776	5018.538380	24.969792
150.667319	5009.209673	24.974810
150.644576	5025.188054	24.979827
151.044287	5038.490284	24.984845
151.003025	5035.898959	24.989863
150.921908	5049.711650	24.994880
151.406824	5060.497557	24.999898
151.235177	5064.807619	25.004915
151.476089	5077.680070	25.009933
151.502162	5079.222697	25.014951
151.508055	5103.375094	25.019968
151.962068	5098.544468	25.024986
152.484034	5107.310807	25.030003
152.219162	5115.420005	25.035021
152.301648	5123.907563	25.040039
152.517439	5132.058723	25.045056
153.025417	5125.815057	25.050074
153.324163	5126.968022	25.055091
153.718806	5128.816264	25.060109
153.519035	5119.005497	25.065127
153.615289	5132.894799	25.070144
153.657432	5132.881942	25.075162
153.552654	5130.707678	25.080179
153.606761	5129.010557	25.085197
154.096932	5141.276081	25.090215
153.956279	5154.387913	25.095232
154.226027	5155.791600	25.100250
154.207954	5176.759782	25.105267
154.420930	5183.058548	25.110285
154.924960	5190.281042	25.115303
154.898741	5205.512035	25.120320
155.248731	5206.843261	25.125338
155.173325	5206.665629	25.130355
155.244399	5213.169574	25.135373
155.747313	5218.564646	25.140391
155.660321	5226.797711	25.145408
155.844629	5230.124384	25.150426
156.275185	5234.372294	25.155443
156.278318	5252.067134	25.160461
156.359018	5254.292543	25.165479
156.565389	5254.771783	25.170496
156.558285	5252.945294	25.175514
156.692899	5277.595548	25.180531
156.739277	5289.646182	25.185549
157.162242	5294.324572	25.190567
156.954141	5300.950926	25.195584
157.600699	5309.518045	25.200602
157.938650	5318.041676	25.205619
157.844002	5334.100966	25.210637
158.301363	5328.808909	25.215655
157.879499	5333.486267	25.220672
158.118643	5335.582853	25.225690
158.593917	5355.208670	25.230707
158.592074	5364.675364	25.235725
158.882560	5359.908007	25.240743
158.841601	5374.244986	25.245760
159.342292	5387.743238	25.250778
159.484212	5393.077775	25.255795
159.522934	5395.205572	25.260813
159.769680	5393.222756	25.265831
159.366925	5403.522078	25.270848
160.097497	5401.710143	25.275866
159.694600	5406.731785	25.280883
160.007978	5417.781352	25.285901
160.204491	5436.702561	25.290919
160.001541	5445.427257	25.295936
160.147665	5454.119705	25.300954
160.518637	5473.395731	25.305971
160.770256	5480.919633	25.310989
161.211998	5490.838158	25.316007
161.331352	5501.097283	25.321024
161.601304	5491.206870	25.326042
161.890549	5513.314451	25.331059
161.982985	5523.085359	25.336077
162.164185	5511.892475	25.341095
161.963544	5520.272784	25.346112
162.074821	5528.721326	25.351130
162.168377	5538.605704	25.356147
162.522254	5541.173716	25.361165
162.943826	5543.743815	25.366183
163.159870	5558.044082	25.371200
163.869375	5556.257508	25.376218
163.919062	5553.781368	25.381235
163.915624	5558.311568	25.386253
164.238807	5542.494311	25.391271
164.296648	5548.735286	25.396288
164.279291	5547.308090	25.401306
164.237701	5549.858760	25.406323
164.187190	5555.920901	25.411341
164.534185	5549.588519	25.416359
164.209938	5550.863759	25.421376
164.694519	5560.889289	25.426394
165.153635	5578.428228	25.431411
164.749004	5578.769019	25.436429
164.617004	5577.981510	25.441447
164.794008	5596.574485	25.446464
165.141437	5610.122016	25.451482
165.587275	5625.986935	25.456499
165.541543	5625.056574	25.461517
165.778023	5633.997035	25.466535
165.842359	5652.273013	25.471552
166.013987	5659.376993	25.476570
166.167605	5668.062064	25.481587
166.283803	5671.595130	25.486605
166.657092	5673.213168	25.491623
166.921113	5689.103293	25.496640
167.201817	5698.576675	25.501658
167.484479	5714.403945	25.506675
168.071148	5718.334102	25.511693
168.455874	5716.121435	25.516711
168.043320	5717.322051	25.521728
168.158705	5726.546564	25.526746
168.539591	5733.510670	25.531763
168.257295	5727.658148	25.536781
168.337677	5743.362263	25.541799
168.927605	5745.271707	25.546816
168.614870	5750.885469	25.551834
169.035110	5764.488068	25.556851
168.769318	5784.018234	25.561869
169.336589	5795.953383	25.566887
169.321841	5801.927967	25.571904
169.692285	5806.466308	25.576922
169.567253	5812.697966	25.581939
169.753749	5829.427311	25.586957
169.627800	5833.856703	25.591975
170.055755	5861.978527	25.596992
170.172208	5860.300041	25.602010
170.874955	5864.382615	25.607027
171.250397	5878.610968	25.612045
171.203533	5884.221257	25.617063
171.457174	5881.097781	25.622080
171.660133	5895.921190	25.627098
172.519495	5900.998974	25.632115
172.449640	5899.330551	25.637133
172.623006	5895.910223	25.642151
172.616388	5899.954885	25.647168
172.799926	5899.506499	25.652186
172.622280	5904.654194	25.657203
172.672894	5906.745476	25.662221
173.173864	5911.844338	25.667239
173.054557	5918.384489	25.672256
173.207055	5926.757354	25.677274
172.840552	5933.800019	25.682292
172.771395	5953.192426	25.687309
173.492296	5950.719056	25.692327
173.824107	5966.658845	25.697344
173.527599	5976.165419	25.702362
174.197724	5978.993606	25.707380
173.973147	5998.858500	25.712397
174.229257	6003.427318	25.717415
174.309452	6006.675645	25.722432
174.343579	6026.342460	25.727450
174.734416	6029.472982	25.732468
174.671441	6049.549518	25.737485
175.107990	6054.945704	25.742503
175.542377	6065.951572	25.747520
175.431910	6089.034352	25.752538
176.104010	6071.028426	25.757556
176.310420	6077.675755	25.762573
176.635330	6088.392487	25.767591
176.920374	6094.563553	25.772608
177.242070	6097.591212	25.777626
178.027183	6092.074293	25.782644
177.422028	6101.537443	25.787661
177.558961	6095.698448	25.792679
177.923154	6092.024252	25.797696
177.824232	6091.158967	25.802714
177.960026	6082.678044	25.807732
177.816824	6087.804644	25.812749
178.254775	6094.049761	25.817767
178.352285	6103.955926	25.822784
178.327040	6117.874366	25.827802
178.289703	6117.046841	25.832820
178.534434	6136.254839	25.837837
178.909630	6134.750696	25.842855
178.949623	6148.674786	25.847872
178.801200	6173.654416	25.852890
179.354939	6172.927421	25.857908
179.307898	6187.228105	25.862925
179.750732	6188.633337	25.867943
179.866858	6195.534672	25.872960
180.082847	6214.049604	25.877978
180.277910	6216.446726	25.882996
180.410224	6237.818864	25.888013
180.656036	6230.485554	25.893031
181.058508	6243.100085	25.898048
181.010729	6264.225662	25.903066
180.955269	6267.984440	25.908084
181.293903	6280.359559	25.913101
181.684012	6285.188529	25.918119
182.128624	6292.247099	25.923136
181.766191	6299.030422	25.928154
182.427785	6309.780097	25.933172
182.464647	6318.417366	25.938189
182.615666	6323.772856	25.943207
182.983490	6333.390839	25.948224
182.980932	6355.626948	25.953242
183.176125	6347.717485	25.958260
183.131350	6348.930328	25.963277
183.075279	6360.754555	25.968295
183.605441	6373.194618	25.973312
183.692992	6384.841823	25.978330
183.890713	6389.205173	25.983348
183.960648	6400.148031	25.988365
184.417905	6417.864844	25.993383
184.372105	6419.841771	25.998400
184.485024	6438.082561	26.003418
184.836217	6448.883802	26.008436
184.925655	6457.828621	26.013453
185.115071	6463.402300	26.018471
185.417373	6472.304516	26.023488
185.533965	6484.483903	26.028506
185.808108	6492.377209	26.033524
186.079193	6502.963670	26.038541
185.844777	6503.120138	26.043559
186.313367	6519.569443	26.048576
186.184928	6533.876758	26.053594
186.378552	6529.111553	26.058612
186.789415	6542.511008	26.063629
187.150823	6556.634748	26.068647
187.174216	6553.278684	26.073664
187.254175	6575.407511	26.078682
187.659920	6578.510553	26.083700
187.778818	6587.150960	26.088717
188.107704	6601.077767	26.093735
188.571646	6603.947626	26.098752
188.560695	6604.463895	26.103770
188.794194	6600.386945	26.108788
188.835506	6625.154561	26.113805
188.922062	6628.316777	26.118823
189.174997	6627.081012	26.123840
189.338487	6641.945897	26.128858
189.686047	6652.971953	26.133876
189.617835	6647.575097	26.138893
189.771079	6668.600395	26.143911
190.042498	6669.331557	26.148928
190.090926	6685.859054	26.153946
190.655470	6701.665392	26.158964
191.017619	6701.700572	26.163981
190.950852	6713.949697	26.168999
191.482505	6705.482618	26.174016
191.650762	6718.304407	26.179034
191.982945	6718.164318	26.184052
191.956992	6713.603716	26.189069
192.193606	6725.549918	26.194087
192.601357	6732.150356	26.199104
192.552799	6745.416298	26.204122
192.703838	6745.613773	26.209140
192.913863	6745.495859	26.214157
192.763940	6751.848511	26.219175
192.854383	6766.920590	26.224192
193.120817	6785.974367	26.229210
193.326500	6783.846272	26.234228
193.579094	6800.417848	26.239245
193.469637	6813.333449	26.244263
193.765710	6819.531456	26.249280
193.920315	6834.205318	26.254298
194.235559	6841.637801	26.259316
194.462393	6857.749394	26.264333
194.401385	6866.822010	26.269351
194.656287	6884.128831	26.274368
194.844888	6894.346391	26.279386
195.083518	6910.399372	26.284404
195.607081	6908.723701	26.289421
195.626648	6925.429531	26.294439
195.818306	6930.179083	26.299456
196.187147	6941.022062	26.304474
196.482933	6950.370633	26.309492
196.986083	6956.369137	26.314509
196.767535	6967.975979	26.319527
196.782030	6980.493584	26.324544
197.076023	6986.155316	26.329562
197.030401	6992.479186	26.334580
197.422799	7009.054440	26.339597
197.291664	7019.539668	26.344615
197.458254	7033.353173	26.349632
197.713413	7045.662887	26.354650
198.285296	7060.101497	26.359668
198.665729	7065.099493	26.364685
198.422477	7078.831627	26.369703
198.847384	7090.294172	26.374720
198.823418	7105.501142	26.379738
199.203037	7120.900994	26.384756
199.778733	7119.592850	26.389773
199.667584	7116.844798	26.394791
200.483597	7133.145862	26.399808
200.443615	7138.455565	26.404826
200.314304	7146.143637	26.409844
200.813012	7140.939330	26.414861
200.718460	7145.856614	26.419879
201.114542	7155.934686	26.424896
200.769965	7175.709048	26.429914
201.409151	7167.016665	26.434932
201.675150	7166.214474	26.439949
201.892722	7187.176686	26.444967
201.728218	7191.015766	26.449984
202.218539	7196.602802	26.455002
202.336413	7203.245385	26.460020
202.581369	7210.515336	26.465037
202.422778	7223.066368	26.470055
202.796515	7229.707007	26.475072
202.962385	7247.750950	26.480090
202.760597	7252.779663	26.485108
203.497998	7268.449091	26.490125
203.119898	7288.727575	26.495143
203.632285	7295.757042	26.500160
203.837220	7308.624044	26.505178
204.432164	7321.474531	26.510196
204.490411	7324.363471	26.515213
204.674651	7342.038451	26.520231
204.797643	7352.995716	26.525248
204.993014	7360.819583	26.530266
205.222730	7370.765831	26.535284
205.279714	7377.035977	26.540301
205.344313	7399.310247	26.545319
205.607089	7402.612476	26.550336
206.019875	7417.597021	26.555354
206.190725	7440.022113	26.560372
206.845106	7446.972708	26.565389
206.583851	7469.733445	26.570407
206.811344	7468.940393	26.575424
207.102542	7488.783422	26.580442
207.402592	7494.772685	26.585460
207.794494	7500.829729	26.590477
207.774131	7515.461925	26.595495
207.905986	7529.022346	26.600512
208.144577	7535.346351	26.605530
208.295977	7549.393062	26.610548
208.553245	7551.310299	26.615565
208.428763	7580.139526	26.620583
208.798401	7581.095359	26.625600
209.083323	7607.720513	26.630618
209.474441	7614.497490	26.635636
209.876882	7619.811060	26.640653
209.622217	7638.583808	26.645671
210.027759	7644.970251	26.650688
210.190562	7658.251299	26.655706
209.933237	7671.859789	26.660724
210.547987	7681.080152	26.665741
210.755534	7704.143863	26.670759
210.867126	7712.662818	26.675776
211.244714	7714.845463	26.680794
211.068067	7740.816579	26.685812
211.573814	7756.247839	26.690829
211.523339	7768.845548	26.695847
211.679671	7784.375429	26.700864
212.180472	7803.283282	26.705882
212.441425	7813.243849	26.710900
213.006846	7816.521132	26.715917
213.063322	7830.658604	26.720935
213.196908	7837.980870	26.725952
213.639643	7851.723585	26.730970
213.409851	7855.828681	26.735988
214.016028	7870.022663	26.741005
213.863704	7881.787087	26.746023
214.018526	7893.920418	26.751040
214.346812	7905.505853	26.756058
214.439079	7909.462953	26.761076
214.971679	7924.050424	26.766093
215.209642	7931.435400	26.771111
215.228515	7945.042131	26.776128
215.787659	7957.251462	26.781146
215.602197	7964.260399	26.786164
215.735317	7970.379986	26.791181
215.690735	7979.747348	26.796199
216.005476	7997.674139	26.801216
216.169056	8007.915157	26.806234
216.853613	8033.102268	26.811252
216.838556	8042.256704	26.816269
217.154196	8049.617007	26.821287
217.430081	8074.230090	26.826304
217.833965	8073.267487	26.831322
217.865571	8088.794944	26.836340
218.277929	8094.208132	26.841357
218.410843	8114.651051	26.846375
218.703679	8128.470980	26.851392
218.727463	8139.317879	26.856410
218.951119	8154.787079	26.861428
219.050815	8162.291541	26.866445
219.195049	8170.578323	26.871463
219.671214	8189.162081	26.876480
219.944640	8197.520314	26.881498
219.715275	8209.527403	26.886516
220.186948	8220.838152	26.891533
220.525751	8238.366806	26.896551
220.717491	8258.406100	26.901568
221.307424	8264.056881	26.906586
220.896699	8276.559487	26.911604
221.584262	8295.340902	26.916621
221.926839	8307.467373	26.921639
221.902883	8312.380291	26.926656
221.942761	8325.273701	26.931674
221.802873	8344.247132	26.936692
222.412655	8363.694231	26.941709
222.637564	8373.670185	26.946727
222.842004	8388.425925	26.951744
223.410383	8398.471542	26.956762
223.112018	8414.963030	26.961780
223.497670	8430.378826	26.966797
223.499594	8446.435274	26.971815
224.144075	8454.691657	26.976832
224.635961	8465.607936	26.981850
224.810939	8480.668257	26.986868
225.258005	8488.586015	26.991885
225.452531	8482.951978	26.996903
225.488986	8506.542145	27.001920
225.926656	8503.301181	27.006938
225.530391	8526.658822	27.011956
226.070011	8525.987614	27.016973
226.159423	8533.954760	27.021991
226.471377	8545.723093	27.027008
226.775515	8550.231403	27.032026
226.675747	8571.118314	27.037044
227.047354	8585.538794	27.042061
227.452149	8597.131696	27.047079
227.283342	8620.018367	27.052096
227.740846	8623.760904	27.057114
228.209444	8636.553057	27.062132
228.476069	8644.416891	27.067149
228.915409	8651.114132	27.072167
229.271177	8653.145592	27.077184
229.692185	8647.299447	27.082202
229.713970	8655.513955	27.087220
229.933856	8657.152993	27.092237
230.175335	8651.767318	27.097255
230.307733	8656.141380	27.102272
230.293715	8659.578485	27.107290
230.598094	8680.093205	27.112308
230.883928	8675.647744	27.117325
231.159275	8681.050866	27.122343
231.205295	8701.990999	27.127360
231.285849	8700.507271	27.132378
231.406491	8705.716647	27.137396
231.662460	8714.144131	27.142413
232.177018	8718.913332	27.147431
232.209181	8730.337021	27.152448
232.600386	8746.879302	27.157466
232.956874	8757.542168	27.162484
232.837955	8750.823450	27.167501
233.379080	8776.494846	27.172519
233.110429	8778.674048	27.177536
233.972294	8785.725451	27.182554
233.629875	8804.490945	27.187572
234.338975	8810.675837	27.192589
234.420200	8827.537961	27.197607
234.555212	8836.318987	27.202624
234.744245	8835.484510	27.207642
234.583571	8858.354424	27.212660
235.219646	8858.893150	27.217677
235.230126	8883.728589	27.222695
235.262682	8891.799455	27.227712
235.609693	8903.452060	27.232730
235.811421	8930.294132	27.237748
236.203966	8937.112420	27.242765
236.362003	8946.278241	27.247783
236.728325	8958.256216	27.252800
237.081698	8980.512694	27.257818
237.183869	8995.711056	27.262836
237.560458	8999.996668	27.267853
237.744920	9015.156977	27.272871
237.977231	9032.617723	27.277888
238.373340	9040.019566	27.282906
238.472012	9047.881306	27.287924
238.875142	9068.630498	27.292941
238.885884	9067.694326	27.297959
238.913097	9095.012122	27.302976
239.651102	9095.206642	27.307994
239.787621	9117.244474	27.313012
240.386441	9122.572108	27.318029
240.665534	9123.722081	27.323047
240.728358	9139.517076	27.328064
241.061259	9142.606644	27.333082
240.987828	9157.238931	27.338100
240.960087	9160.091032	27.343117
241.670479	9173.587849	27.348135
241.865736	9201.403730	27.353152
242.306866	9201.372955	27.358170
242.585729	9203.201762	27.363188
242.392224	9232.877806	27.368205
242.189954	9231.510683	27.373223
242.615688	9254.144558	27.378240
243.100107	9264.257393	27.383258
243.255853	9274.165671	27.388276
243.352180	9295.067070	27.393293
244.246463	9307.989162	27.398311
243.586469	9317.367768	27.403328
244.355791	9323.439272	27.408346
244.841296	9335.026387	27.413364
245.056488	9343.735184	27.418381
245.161969	9344.833271	27.423399
245.386303	9371.419887	27.428416
245.416747	9355.259758	27.433434
245.551257	9380.041824	27.438452
245.671821	9387.991859	27.443469
245.956085	9401.068976	27.448487
246.375258	9416.511950	27.453504
246.687825	9438.892150	27.458522
246.964691	9450.720196	27.463540
247.219859	9459.081844	27.468557
247.256195	9466.445155	27.473575
247.434761	9485.714311	27.478592
247.728290	9496.529481	27.483610
247.809779	9518.866822	27.488628
248.074036	9537.513346	27.493645
248.500554	9549.618094	27.498663
248.524135	9563.660980	27.503680
248.868712	9595.637544	27.508698
249.229304	9600.080493	27.513716
249.299762	9617.519630	27.518733
249.474193	9637.357891	27.523751
249.749411	9664.259044	27.528768
250.096629	9671.915019	27.533786
250.461829	9688.544279	27.538804
250.656317	9711.069481	27.543821
250.931044	9723.977819	27.548839
251.374810	9732.840649	27.553856
251.571939	9750.512771	27.558874
251.808654	9766.050746	27.563892
252.129604	9777.673229	27.568909
252.505358	9787.541216	27.573927
252.220238	9813.402675	27.578944
252.644016	9817.737963	27.583962
253.106370	9842.074943	27.588980
253.144775	9857.072400	27.593997
253.683034	9865.484877	27.599015
253.956532	9888.563147	27.604032
254.176163	9900.611930	27.609050
254.761439	9910.008498	27.614068
254.858020	9923.781393	27.619085
255.431608	9932.589377	27.624103
255.476426	9948.672021	27.629120
255.679391	9952.969100	27.634138
256.057692	9968.242089	27.639156
255.866450	9973.680345	27.644173
256.579298	9988.370839	27.649191
256.564322	10011.696241	27.654208
256.780633	10015.625009	27.659226
256.877459	10031.478616	27.664244
256.916565	10054.918788	27.669261
257.435101	10056.363061	27.674279
257.708667	10090.015440	27.679296
258.312830	10089.694069	27.684314
258.217971	10119.349854	27.689332
258.268523	10134.879232	27.694349
258.908226	10136.238344	27.699367
258.992879	10162.743647	27.704384
259.200356	10179.426319	27.709402
259.460868	10192.968664	27.714420
259.308775	10219.823483	27.719437
260.006253	10238.318015	27.724455
260.103505	10261.241061	27.729472
260.145387	10269.074271	27.734490
260.828250	10284.704246	27.739508
260.610466	10306.621836	27.744525
261.323528	10318.139409	27.749543
261.513708	10339.459929	27.754560
261.710265	10342.248875	27.759578
262.687860	10362.275447	27.764596
262.571831	10382.908022	27.769613
262.705488	10386.309826	27.774631
262.593282	10409.568772	27.779648
263.095982	10416.607261	27.784666
263.824192	10411.757835	27.789684
264.280090	10433.226536	27.794701
264.580256	10415.413230	27.799719
264.732162	10432.395259	27.804736
265.391585	10443.150860	27.809754
265.729655	10440.698631	27.814772
265.976172	10440.091939	27.819789
266.385777	10434.528022	27.824807
266.061782	10443.725426	27.829824
266.383727	10460.469463	27.834842
266.610721	10456.537923	27.839860
266.697922	10470.678940	27.844877
267.030244	10476.945159	27.849895
267.546055	10488.600899	27.854912
267.747603	10507.314992	27.859930
267.734965	10511.197418	27.864948
267.922656	10518.891209	27.869965
267.980306	10536.708932	27.874983
268.694309	10548.112836	27.880000
268.737222	10559.880133	27.885018
268.876264	10570.710509	27.890036
268.967893	10586.057054	27.895053
269.486379	10592.802672	27.900071
269.516061	10617.763734	27.905088
269.928706	10633.101386	27.910106
270.338391	10648.796300	27.915124
270.100676	10667.752599	27.920141
270.442999	10674.787739	27.925159
270.758055	10689.275497	27.930176
270.780121	10707.853547	27.935194
271.380714	10722.457905	27.940212
271.496977	10746.107954	27.945229
271.864313	10763.044116	27.950247
272.302459	10786.669363	27.955264
272.420946	10797.954586	27.960282
272.731373	10820.851446	27.965300
272.769358	10833.487982	27.970317
273.136461	10850.039049	27.975335
273.612445	10871.830347	27.980352
274.165720	10901.048620	27.985370
274.330752	10905.705462	27.990388
274.709427	10922.232690	27.995405
274.767867	10935.478659	28.000423
275.408887	10954.004796	28.005440
275.596689	10964.486803	28.010458
276.043222	10978.635411	28.015476
275.826027	10990.566617	28.020493
276.503041	11015.654768	28.025511
276.534215	11012.596646	28.030528
276.753782	11022.900079	28.035546
277.160052	11043.957266	28.040564
277.407419	11079.560521	28.045581
277.809221	11066.110217	28.050599
277.924934	11090.654357	28.055616
277.975332	11102.866038	28.060634
278.744561	11114.754263	28.065652
278.974469	11126.211787	28.070669
279.165918	11147.814051	28.075687
279.305854	11156.017584	28.080704
279.358790	11178.134018	28.085722
279.748408	11189.061515	28.090740
279.676813	11211.121595	28.095757
280.141876	11231.674111	28.100775
280.587018	11239.208133	28.105792
280.668895	11257.591124	28.110810
280.739654	11270.816467	28.115828
281.150739	11293.818222	28.120845
281.466427	11307.933773	28.125863
282.042530	11331.778205	28.130880
282.656833	11337.441930	28.135898
283.433358	11336.916888	28.140916
283.700020	11351.712661	28.145933
283.680803	11345.848963	28.150951
284.292310	11343.631912	28.155968
284.336948	11365.440420	28.160986
284.577573	11377.736337	28.166004
284.358418	11375.591768	28.171021
284.979262	11396.009698	28.176039
285.490141	11390.448679	28.181056
285.284803	11407.752447	28.186074
285.812093	11424.588525	28.191092
285.990377	11432.726216	28.196109
286.239260	11450.126658	28.201127
286.457060	11457.996130	28.206144
286.426173	11478.682966	28.211162
286.684249	11496.748265	28.216180
287.347295	11493.133846	28.221197
288.089444	11498.259876	28.226215
288.723313	11514.912093	28.231232
288.922834	11517.823900	28.236250
289.223736	11517.874955	28.241268
289.180668	11530.177248	28.246285
289.268573	11542.077092	28.251303
289.740460	11542.180468	28.256320
289.635935	11562.891491	28.261338
289.749143	11562.283417	28.266356
290.005398	11589.777610	28.271373
290.183422	11603.150682	28.276391
290.626801	11623.460714	28.281408
290.931211	11644.970184	28.286426
291.017236	11660.845800	28.291444
291.376513	11681.134254	28.296461
291.692616	11697.665596	28.301479
291.998782	11713.311213	28.306496
291.995913	11740.887018	28.311514
291.962965	11766.336160	28.316532
292.489684	11784.138880	28.321549
292.508391	11806.873962	28.326567
292.836074	11831.285029	28.331584
293.420146	11863.875508	28.336602
294.268004	11885.578517	28.341620
294.313565	11908.972644	28.346637
294.549397	11922.532718	28.351655
294.824740	11945.682713	28.356672
295.115552	11967.646212	28.361690
295.385750	11986.319521	28.366708
295.690874	12005.344225	28.371725
296.149822	12021.083146	28.376743
296.381938	12033.305034	28.381760
296.388248	12064.141741	28.386778
297.213306	12077.104967	28.391796
297.129018	12103.566695	28.396813
297.093444	12126.563227	28.401831
297.926828	12137.008536	28.406848
297.972593	12164.062690	28.411866
298.657081	12182.498023	28.416884
298.754996	12200.500520	28.421901
298.937382	12216.939460	28.426919
299.428569	12235.427043	28.431936
299.520905	12256.240804	28.436954
300.303060	12277.341906	28.441972
300.408484	12291.670922	28.446989
300.567189	12307.532612	28.452007
300.795681	12312.028356	28.457024
300.803998	12336.069825	28.462042
301.421442	12347.344613	28.467060
301.452698	12376.450682	28.472077
301.785854	12388.019213	28.477095
302.191236	12410.533781	28.482112
302.421302	12437.145973	28.487130
302.597308	12454.366071	28.492148
302.830931	12482.212443	28.497165
303.141976	12497.125361	28.502183
303.315445	12517.067876	28.507200
303.717740	12546.833249	28.512218
304.030824	12562.595333	28.517236
304.277282	12595.811196	28.522253
304.475392	12612.709065	28.527271
305.388797	12643.190771	28.532288
305.327334	12650.538983	28.537306
306.022694	12671.470891	28.542324
306.588814	12700.023683	28.547341
307.188035	12707.540627	28.552359
307.566901	12718.255963	28.557376
307.572008	12738.228082	28.562394
307.975276	12750.228009	28.567412
308.246519	12761.711676	28.572429
308.458113	12776.905552	28.577447
309.032009	12793.773499	28.582464
308.888822	12812.376202	28.587482
309.550030	12826.934877	28.592500
309.727919	12836.336353	28.597517
309.924929	12859.082839	28.602535
310.330032	12884.973699	28.607552
310.642240	12899.514135	28.612570
310.666772	12925.161150	28.617588
310.782902	12939.498466	28.622605
310.987055	12955.666249	28.627623
311.750313	12972.703818	28.632640
311.701030	12994.001482	28.637658
312.162958	13016.062720	28.642676
312.586031	13034.706954	28.647693
312.713933	13053.542420	28.652711
312.860335	13072.624493	28.657728
312.900510	13096.740917	28.662746
313.627180	13120.396817	28.667764
313.959375	13142.494189	28.672781
314.069453	13171.507109	28.677799
314.693186	13190.199203	28.682816
315.076809	13217.117005	28.687834
315.326290	13240.465247	28.692852
316.206253	13253.812317	28.697869
316.117216	13270.493377	28.702887
316.955389	13282.874353	28.707904
316.951701	13299.674782	28.712922
317.393263	13315.828017	28.717940
317.703451	13344.920575	28.722957
318.165799	13356.750639	28.727975
318.467640	13367.434127	28.732992
318.498032	13384.361957	28.738010
318.768440	13392.621943	28.743028
318.919248	13410.607887	28.748045
319.423679	13427.329323	28.753063
320.022485	13443.679240	28.758080
320.401049	13458.045566	28.763098
320.148648	13473.931187	28.768116
320.727479	13493.631626	28.773133
320.703256	13508.903857	28.778151
321.297476	13529.296676	28.783168
321.175622	13547.385199	28.788186
321.720477	13566.329947	28.793204
322.190458	13591.384303	28.798221
322.168137	13603.495243	28.803239
322.597514	13603.583151	28.808256
322.629884	13642.243695	28.813274
322.926455	13662.626154	28.818292
323.607526	13675.019215	28.823309
323.701744	13704.297529	28.828327
324.190807	13723.096382	28.833344
325.293463	13724.633177	28.838362
325.980831	13721.238770	28.843380
326.594791	13720.593723	28.848397
326.516710	13729.268116	28.853415
327.056744	13747.607473	28.858432
327.237130	13753.547916	28.863450
327.598757	13756.220095	28.868468
327.890143	13764.082236	28.873485
327.841933	13781.515297	28.878503
328.372019	13782.509647	28.883520
328.913747	13795.761338	28.888538
328.972931	13807.341815	28.893556
329.569435	13810.375337	28.898573
329.738878	13828.144036	28.903591
329.739525	13837.346232	28.908608
329.661193	13848.231288	28.913626
329.722331	13872.604390	28.918644
330.384418	13885.764772	28.923661
330.140128	13909.380190	28.928679
330.620484	13932.137541	28.933696
330.969501	13954.905893	28.938714
331.612680	13976.134751	28.943732
331.889682	14000.360723	28.948749
331.847514	14029.256551	28.953767
332.169010	14047.128102	28.958784
332.684389	14076.278263	28.963802
333.135233	14095.348708	28.968820
333.751604	14109.624822	28.973837
334.237991	14139.606990	28.978855
334.284432	14155.269807	28.983872
335.068635	14178.346479	28.988890
335.346651	14184.710821	28.993908
335.723219	14201.847601	28.998925
335.935775	14225.884940	29.003943
336.411163	14235.275535	29.008960
337.271754	14250.527459	29.013978
337.617621	14252.216860	29.018996
337.975603	14247.446215	29.024013
338.404279	14263.352784	29.029031
338.376256	14269.736378	29.034048
338.890352	14279.007280	29.039066
339.016827	14306.301418	29.044084
339.343446	14310.311817	29.049101
339.322964	14332.658126	29.054119
339.778331	14333.509397	29.059136
339.935091	14362.747411	29.064154
339.926832	14379.271600	29.069172
340.355123	14399.596450	29.074189
340.328753	14424.081782	29.079207
340.588411	14445.557201	29.084224
340.917985	14459.720326	29.089242
341.753395	14494.332120	29.094260
341.616967	14517.353574	29.099277
342.193012	14550.679461	29.104295
342.535886	14573.787426	29.109312
342.938335	14596.567178	29.114330
343.133733	14620.898231	29.119348
343.578209	14640.980805	29.124365
343.635335	14660.968957	29.129383
344.080732	14677.928073	29.134400
344.110541	14702.881890	29.139418
344.721947	14732.299180	29.144436
345.198160	14743.508968	29.149453
345.299324	14777.973466	29.154471
345.692808	14798.569442	29.159488
345.850453	14818.128398	29.164506
346.242877	14843.843898	29.169524
346.869327	14870.805200	29.174541
347.391766	14888.699949	29.179559
347.742729	14918.770751	29.184576
347.847305	14929.501623	29.189594
348.017197	14969.529879	29.194612
348.544653	14993.452842	29.199629
348.997763	15020.700310	29.204647
349.287412	15048.589106	29.209664
349.774357	15066.404277	29.214682
350.255162	15099.499617	29.219700
350.383585	15111.995451	29.224717
350.931323	15145.254149	29.229735
351.021815	15161.034104	29.234752
351.166084	15190.654313	29.239770
351.348711	15220.420189	29.244788
352.164549	15255.090105	29.249805
352.522449	15282.011685	29.254823
352.592665	15301.947939	29.259840
353.045630	15336.570276	29.264858
353.144004	15370.202511	29.269876
353.955235	15391.406792	29.274893
354.154666	15417.759490	29.279911
354.679672	15443.407786	29.284928
354.938679	15470.720856	29.289946
355.024043	15506.395571	29.294964
355.864539	15535.674215	29.299981
355.699021	15554.981045	29.304999
356.073936	15584.925997	29.310016
356.769041	15619.808025	29.315034
356.931980	15645.497169	29.320052
357.705843	15669.531057	29.325069
357.799149	15699.816907	29.330087
358.334131	15734.010304	29.335104
358.921337	15743.406347	29.340122
359.349219	15767.418424	29.345140
360.151584	15770.868694	29.350157
360.244504	15803.640331	29.355175
360.719625	15817.327015	29.360192
361.025828	15840.192720	29.365210
361.178133	15861.894895	29.370228
361.713081	15886.326296	29.375245
362.262420	15899.963586	29.380263
362.267836	15923.823707	29.385280
362.504480	15948.352161	29.390298
362.947839	15975.473020	29.395316
363.239791	15996.016615	29.400333
363.552284	16014.017747	29.405351
363.440451	16038.992201	29.410368
364.125040	16074.192527	29.415386
364.475711	16098.062282	29.420404
365.239252	16106.189829	29.425421
365.840004	16126.006447	29.430439
366.475987	16145.381750	29.435456
367.005698	16166.400163	29.440474
367.017770	16176.520785	29.445492
367.252363	16185.251841	29.450509
367.707885	16203.271943	29.455527
368.220111	16228.433739	29.460544
368.601073	16226.422587	29.465562
368.352362	16255.145485	29.470580
368.826911	16269.161051	29.475597
368.902865	16279.562352	29.480615
369.614387	16305.258569	29.485632
370.046591	16318.535390	29.490650
370.163569	16352.450707	29.495668
370.321865	16372.036417	29.500685
370.927507	16391.742007	29.505703
370.694827	16415.374503	29.510720
371.678420	16428.180236	29.515738
371.657033	16457.256527	29.520756
372.361611	16475.023341	29.525773
372.498267	16499.776522	29.530791
373.109486	16530.396804	29.535808
373.941965	16543.968365	29.540826
374.315640	16563.192266	29.545844
374.166144	16584.042097	29.550861
374.341526	16609.503191	29.555879
374.648505	16643.067283	29.560896
375.078883	16655.523433	29.565914
375.424261	16693.446574	29.570932
375.719440	16719.138678	29.575949
376.179622	16750.790365	29.580967
376.554746	16783.614495	29.585984
376.599835	16809.070869	29.591002
377.341016	16846.171506	29.596020
377.629138	16870.993179	29.601037
378.140570	16900.369362	29.606055
378.099149	16928.400874	29.611072
378.893066	16949.975965	29.616090
379.137283	16987.024745	29.621108
379.448101	17010.358581	29.626125
379.831350	17044.290516	29.631143
380.001414	17073.972788	29.636160
380.753575	17110.554234	29.641178
380.956208	17147.050741	29.646196
381.528245	17170.224081	29.651213
381.733267	17186.954375	29.656231
382.124357	17228.983832	29.661248
382.485956	17256.119230	29.666266
382.829119	17292.720476	29.671284
383.406700	17317.450283	29.676301
384.614661	17347.400954	29.681319
384.655369	17379.270589	29.686336
384.967635	17397.800531	29.691354
385.134169	17428.557803	29.696372
385.718433	17454.070066	29.701389
386.081560	17480.305354	29.706407
386.616171	17508.339629	29.711424
387.102912	17528.257569	29.716442
387.006147	17561.188074	29.721460
387.495510	17589.570637	29.726477
388.097508	17607.253396	29.731495
388.334382	17633.104250	29.736512
388.926526	17658.293381	29.741530
389.446997	17672.009075	29.746548
390.011086	17698.282863	29.751565
390.841383	17720.649122	29.756583
390.622165	17733.374508	29.761600
391.661515	17747.729637	29.766618
392.150178	17769.182607	29.771636
392.254872	17782.085017	29.776653
392.438127	17791.835550	29.781671
393.109949	17811.668115	29.786688
393.067574	17825.326247	29.791706
393.113898	17845.325715	29.796724
393.143231	17880.249170	29.801741
393.799745	17896.009584	29.806759
394.293252	17921.921947	29.811776
394.939393	17943.660140	29.816794
395.034780	17955.477546	29.821812
395.152987	17991.682406	29.826829
395.687101	18014.979536	29.831847
395.776533	18037.208811	29.836864
396.556857	18057.852303	29.841882
396.552204	18089.862834	29.846900
396.950945	18114.299324	29.851917
397.381805	18136.387115	29.856935
397.297958	18174.740078	29.861952
398.194090	18196.351194	29.866970
398.763971	18220.514798	29.871988
399.222710	18250.886750	29.877005
399.601199	18274.720128	29.882023
399.476564	18312.839654	29.887040
400.223606	18331.763975	29.892058
401.066039	18369.139223	29.897076
401.377776	18397.348469	29.902093
401.917349	18417.259102	29.907111
402.467550	18437.332355	29.912128
403.117389	18461.370098	29.917146
403.449440	18477.440515	29.922164
403.776388	18509.715988	29.927181
404.022864	18523.898214	29.932199
404.393740	18550.127431	29.937216
405.271998	18572.645149	29.942234
405.501996	18593.873971	29.947252
405.654703	18607.565459	29.952269
406.410762	18631.845894	29.957287
406.451446	18660.135626	29.962304
407.101420	18669.794990	29.967322
407.594275	18700.080209	29.972340
407.825171	18731.726618	29.977357
408.394390	18733.286892	29.982375
408.494384	18765.888729	29.987392
408.794337	18781.711694	29.992410
409.178716	18812.007658	29.997428
409.352840	18832.556826	30.002445
409.751471	18870.975038	30.007463
410.185295	18900.473746	30.012480
411.062737	18928.102924	30.017498
411.310537	18958.932104	30.022516
411.620908	18991.836401	30.027533
412.177183	18995.748861	30.032551
412.693899	19027.597642	30.037568
412.925429	19054.348326	30.042586
413.518680	19076.411909	30.047604
413.666085	19101.362594	30.052621
414.504554	19125.801396	30.057639
414.448037	19151.030280	30.062656
415.077337	19174.250811	30.067674
415.573421	19198.976762	30.072692
415.452740	19239.239179	30.077709
416.509735	19266.765075	30.082727
416.813775	19296.499391	30.087744
416.895711	19323.678067	30.092762
417.261915	19354.375721	30.097780
417.509299	19382.413203	30.102797
418.157544	19403.318770	30.107815
418.093063	19441.690169	30.112832
418.708826	19472.949345	30.117850
419.643213	19505.207717	30.122868
419.839369	19538.257074	30.127885
419.907209	19555.506717	30.132903
420.528955	19597.941332	30.137920
421.179314	19612.497405	30.142938
421.592823	19637.059869	30.147956
422.003664	19657.964762	30.152973
422.777196	19679.773523	30.157991
423.068472	19706.357856	30.163008
423.590606	19719.291334	30.168026
424.298622	19747.491390	30.173044
424.407573	19771.836089	30.178061
424.894678	19795.079499	30.183079
425.049951	19809.883378	30.188096
425.086685	19832.160815	30.193114
425.554147	19871.777001	30.198132
425.663115	19889.235344	30.203149
426.296501	19917.851611	30.208167
426.407723	19958.648019	30.213184
427.023723	19992.485703	30.218202
427.751260	20023.008117	30.223220
427.981528	20059.603728	30.228237
428.580781	20082.608893	30.233255
428.953773	20112.415852	30.238272
429.446788	20149.994238	30.243290
429.915137	20173.721186	30.248308
430.117715	20204.660463	30.253325
430.788467	20226.688014	30.258343
431.426014	20277.006517	30.263360
431.255376	20292.076311	30.268378
432.431949	20320.520153	30.273396
432.398594	20360.891327	30.278413
433.126825	20385.570007	30.283431
433.462198	20417.379793	30.288448
433.854092	20453.527668	30.293466
434.209072	20477.613811	30.298484
434.310822	20514.230279	30.303501
435.043442	20545.352938	30.308519
435.501893	20583.765211	30.313536
435.929662	20613.501224	30.318554
436.422829	20641.173707	30.323572
436.892931	20682.206386	30.328589
437.160662	20711.158739	30.333607
437.366462	20743.166134	30.338624
438.138823	20786.079017	30.343642
439.035188	20819.823940	30.348660
438.738913	20854.392730	30.353677
439.372813	20879.074083	30.358695
439.906113	20909.823986	30.363712
441.056555	20933.445668	30.368730
441.565474	20953.205715	30.373748
441.858178	20992.200596	30.378765
442.358055	21013.769131	30.383783
442.804977	21047.856102	30.388800
442.989540	21073.940808	30.393818
443.596152	21086.394490	30.398836
443.757713	21123.141785	30.403853
444.271476	21148.436099	30.408871
444.693002	21173.561575	30.413888
445.374468	21199.758640	30.418906
446.030402	21239.537801	30.423924
446.542401	21261.945060	30.428941
446.774142	21280.864021	30.433959
447.080404	21311.611989	30.438976
447.448835	21331.767072	30.443994
447.571246	21363.921146	30.449012
448.382838	21401.502883	30.454029
448.919600	21413.171532	30.459047
449.532544	21445.558975	30.464064
449.798308	21476.768430	30.469082
450.076879	21501.430063	30.474100
450.448319	21531.858627	30.479117
450.743982	21558.324740	30.484135
451.057932	21586.348696	30.489152
451.399271	21621.501960	30.494170
452.124711	21637.987624	30.499188
451.858877	21677.399376	30.504205
452.279167	21704.604500	30.509223
453.252776	21742.300673	30.514240
453.420358	21773.020403	30.519258
453.706036	21808.327991	30.524276
454.037557	21845.561974	30.529293
455.046073	21879.228076	30.534311
455.352126	21915.777436	30.539328
455.527152	21946.180350	30.544346
456.544588	21982.372662	30.549364
457.477033	22008.399043	30.554381
457.910656	22035.526726	30.559399
458.385532	22049.555902	30.564416
458.727510	22073.178450	30.569434
459.181791	22103.980434	30.574452
459.470689	22138.649933	30.579469
460.015891	22163.706871	30.584487
460.317001	22198.804241	30.589504
460.832890	22238.360796	30.594522
461.176556	22265.256372	30.599540
461.185859	22305.997692	30.604557
461.395210	22333.956852	30.609575
462.116096	22380.407052	30.614592
463.031677	22418.366302	30.619610
463.436807	22455.589975	30.624628
463.659917	22492.456613	30.629645
464.320995	22520.579506	30.634663
464.670746	22564.023327	30.639680
465.457307	22600.189529	30.644698
465.459260	22635.707054	30.649716
466.023831	22666.833960	30.654733
466.275384	22708.732646	30.659751
467.121462	22735.778124	30.664768
467.216229	22781.903380	30.669786
467.706480	22820.289790	30.674804
468.572902	22847.363847	30.679821
469.288416	22890.903096	30.684839
470.255912	22924.722704	30.689856
470.526371	22947.674993	30.694874
471.088644	22967.788933	30.699892
471.772471	22995.668842	30.704909
472.596007	23020.929974	30.709927
473.644049	23024.374925	30.714944
473.965532	23042.125245	30.719962
474.612822	23054.832920	30.724980
474.999317	23079.460765	30.729997
475.116647	23092.680654	30.735015
475.373022	23107.610292	30.740032
475.832188	23134.937713	30.745050
476.381580	23160.279615	30.750068
476.676670	23184.334159	30.755085
476.777036	23205.562877	30.760103
477.182214	23231.824613	30.765120
477.413920	23264.817824	30.770138
478.034735	23302.862574	30.775156
478.243209	23336.472462	30.780173
478.701550	23368.893448	30.785191
479.438604	23392.354962	30.790208
480.003416	23434.869911	30.795226
480.547902	23457.407307	30.800244
480.676488	23488.616017	30.805261
481.027492	23516.763321	30.810279
481.727630	23546.587737	30.815296
482.011278	23595.257338	30.820314
482.488015	23617.685401	30.825332
482.746538	23660.690851	30.830349
483.447850	23668.467931	30.835367
484.424990	23702.641237	30.840384
484.318763	23730.632537	30.845402
485.017165	23764.596577	30.850420
485.508774	23793.291106	30.855437
486.012455	23829.554145	30.860455
486.466924	23852.188152	30.865472
486.916996	23885.976208	30.870490
487.293791	23918.056911	30.875508
487.762629	23954.597327	30.880525
488.066698	23972.515488	30.885543
488.789928	24004.416014	30.890560
489.014389	24049.784673	30.895578
489.870674	24074.618662	30.900596
489.926472	24113.650257	30.905613
490.071250	24151.056664	30.910631
490.769801	24174.266007	30.915648
491.058909	24218.045168	30.920666
491.439904	24267.882962	30.925684
492.289540	24309.464417	30.930701
492.460935	24359.202363	30.935719
493.180948	24396.715578	30.940736
493.864131	24440.187424	30.945754
494.454831	24478.580355	30.950772
494.798228	24518.136709	30.955789
495.282059	24559.440706	30.960807
496.258151	24604.832640	30.965824
496.312128	24638.727870	30.970842
497.053631	24675.498892	30.975860
497.536379	24722.623585	30.980877
498.049498	24756.359064	30.985895
498.815338	24798.681321	30.990912
498.874886	24846.289272	30.995930
499.183698	24881.541845	31.000948
500.189685	24924.395736	31.005965
500.284513	24966.367805	31.010983
501.110450	24997.148014	31.016000
501.647707	25037.054385	31.021018
501.955473	25079.334795	31.026036
502.962347	25115.730379	31.031053
503.172979	25156.869595	31.036071
503.653486	25187.507966	31.041088
503.997806	25231.470335	31.046106
504.465833	25273.359669	31.051124
505.234739	25320.959429	31.056141
505.239468	25353.719681	31.061159
506.056087	25402.108480	31.066176
506.059691	25445.903173	31.071194
506.975556	25483.514330	31.076212
507.497499	25524.725909	31.081229
508.247520	25573.479392	31.086247
508.620262	25606.896891	31.091264
509.296103	25645.240887	31.096282
509.818909	25686.882406	31.101300
510.679168	25725.387437	31.106317
511.487533	25752.190099	31.111335
511.869560	25782.907907	31.116352
512.240170	25828.321038	31.121370
512.643439	25864.344285	31.126388
513.177194	25898.463980	31.131405
513.666173	25942.424344	31.136423
514.246743	25960.490836	31.141440
514.623830	25997.245177	31.146458
515.043402	26031.743105	31.151476
515.392995	26067.775073	31.156493
515.946088	26106.948000	31.161511
516.716894	26138.199896	31.166528
516.915297	26163.973125	31.171546
517.879662	26197.691338	31.176564
518.692160	26220.790520	31.181581
519.005348	26255.071555	31.186599
519.722379	26270.039281	31.191616
520.232186	26300.238714	31.196634
520.589207	26324.432751	31.201652
521.041839	26350.697517	31.206669
521.497846	26380.071211	31.211687
521.698835	26408.182735	31.216704
522.303504	26443.031750	31.221722
522.653078	26482.129651	31.226740
523.313346	26515.933658	31.231757
523.671240	26549.108553	31.236775
524.183575	26586.057794	31.241792
524.863760	26636.828172	31.246810
525.415563	26667.065856	31.251828
526.164965	26697.487706	31.256845
526.273231	26739.404497	31.261863
526.991244	26766.608102	31.266880
527.262150	26812.620417	31.271898
527.428965	26843.088941	31.276916
527.828286	26886.003541	31.281933
528.361843	26944.609185	31.286951
529.228308	26984.588250	31.291968
529.641721	27039.401824	31.296986
530.212427	27092.939662	31.302004
530.705663	27126.979261	31.307021
531.384212	27173.997049	31.312039
531.751279	27217.574675	31.317056
532.569860	27251.557515	31.322074
532.987875	27304.468699	31.327092
533.677768	27345.961225	31.332109
534.020215	27391.426495	31.337127
534.454999	27431.163952	31.342144
534.699057	27484.178529	31.347162
535.280293	27532.760772	31.352180
536.333894	27571.643732	31.357197
536.714696	27629.990722	31.362215
537.361225	27677.444446	31.367232
537.821909	27715.117988	31.372250
538.360009	27754.839995	31.377268
538.789883	27799.274985	31.382285
539.165354	27857.794109	31.387303
540.221918	27893.795114	31.392320
540.620422	27931.541942	31.397338
541.048363	27983.498962	31.402356
541.902216	28011.530035	31.407373
542.496276	28065.799978	31.412391
543.175679	28107.125040	31.417408
543.919417	28152.877169	31.422426
544.312828	28193.539031	31.427444
544.887297	28229.356541	31.432461
545.188595	28268.863594	31.437479
545.722480	28308.271311	31.442496
546.141591	28350.907821	31.447514
546.993077	28388.648184	31.452532
547.827274	28424.969175	31.457549
548.227616	28465.504089	31.462567
548.732822	28502.704434	31.467584
549.572643	28539.795870	31.472602
549.682424	28590.716820	31.477620
550.095438	28609.557602	31.482637
550.663871	28660.483172	31.487655
551.469387	28687.757903	31.492672
552.312366	28726.701145	31.497690
552.797617	28766.755709	31.502708
553.450796	28802.309144	31.507725
553.683875	28836.398426	31.512743
554.381659	28864.834216	31.517760
554.752616	28892.366493	31.522778
555.034939	28933.849858	31.527796
556.084570	28959.462517	31.532813
556.424026	28997.922116	31.537831
556.883325	29037.178511	31.542848
557.740444	29068.680644	31.547866
557.916998	29106.521086	31.552884
558.705556	29144.411703	31.557901
558.730530	29183.205044	31.562919
559.155781	29214.907371	31.567936
559.998094	29268.326477	31.572954
560.338593	29298.070020	31.577972
561.389903	29336.887182	31.582989
561.452551	29379.853129	31.588007
561.961309	29420.524761	31.593024
562.846043	29466.504400	31.598042
563.485425	29512.572906	31.603060
564.085479	29549.210469	31.608077
564.502938	29587.090146	31.613095
565.126867	29623.781014	31.618112
565.436770	29674.869455	31.623130
566.310776	29723.259634	31.628148
567.053561	29767.460564	31.633165
567.384410	29809.886299	31.638183
567.549317	29848.962522	31.643200
568.256939	29900.052818	31.648218
568.974637	29947.285823	31.653236
569.519254	29991.303168	31.658253
569.730580	30046.004569	31.663271
570.489706	30096.347767	31.668288
570.883811	30148.385084	31.673306
571.078323	30201.351207	31.678324
571.817500	30250.876140	31.683341
572.437259	30310.103820	31.688359
572.989959	30361.339481	31.693376
573.951150	30408.630458	31.698394
574.436227	30465.224645	31.703412
575.290146	30507.146867	31.708429
576.256787	30556.207280	31.713447
576.542202	30596.720049	31.718464
577.047773	30642.350465	31.723482
577.693792	30695.822805	31.728500
578.723817	30738.179536	31.733517
579.379159	30790.595012	31.738535
579.653757	30828.315896	31.743552
580.795091	30872.937578	31.748570
580.957244	30913.046626	31.753588
581.913930	30945.636059	31.758605
582.521539	30977.356965	31.763623
582.989009	31007.475140	31.768640
583.600210	31050.453995	31.773658
584.190678	31096.103805	31.778676
584.834699	31139.475986	31.783693
585.049254	31180.898574	31.788711
585.328257	31221.615852	31.793728
586.420526	31256.827039	31.798746
587.123913	31304.311919	31.803764
587.661621	31339.533721	31.808781
588.016221	31386.409330	31.813799
588.672699	31424.615501	31.818816
588.973547	31467.529750	31.823834
589.505862	31517.191070	31.828852
590.110513	31551.448257	31.833869
590.244230	31599.357539	31.838887
590.795328	31652.404620	31.843904
591.614494	31700.744764	31.848922
591.792654	31760.310853	31.853940
592.709467	31793.223913	31.858957
593.442248	31848.854045	31.863975
593.510370	31884.971689	31.868992
594.427048	31931.034038	31.874010
594.933290	31979.708021	31.879028
595.181334	32018.490926	31.884045
596.110309	32069.988328	31.889063
596.554779	32123.451479	31.894080
597.165425	32169.347059	31.899098
597.870035	32217.472335	31.904116
598.233745	32266.320900	31.909133
599.040851	32320.195915	31.914151
599.650761	32375.296589	31.919168
600.445049	32422.662407	31.924186
600.753463	32480.497068	31.929204
601.293987	32521.100319	31.934221
602.122329	32574.549123	31.939239
602.685379	32628.633619	31.944256
603.287788	32670.890184	31.949274
603.946427	32732.325077	31.954292
604.639126	32784.170803	31.959309
605.916771	32823.174240	31.964327
606.745863	32861.229743	31.969344
607.123404	32917.183555	31.974362
607.455955	32968.573726	31.979380
608.153975	33002.945210	31.984397
608.922299	33047.857236	31.989415
609.416658	33089.290641	31.994432
610.149883	33142.882150	31.999450
610.512297	33191.157777	32.004468
611.030876	33239.687375	32.009485
611.718152	33290.213890	32.014503
612.112548	33337.991754	32.019520
612.820832	33381.668392	32.024538
613.529211	33435.454181	32.029556
614.316114	33488.918099	32.034573
615.230305	33524.938481	32.039591
616.372518	33566.094958	32.044608
616.988069	33591.806242	32.049626
617.631843	33636.972843	32.054644
618.225533	33667.606285	32.059661
618.900163	33697.379996	32.064679
619.415637	33734.803116	32.069696
620.010168	33773.415219	32.074714
620.717961	33812.559797	32.079732
621.290922	33855.942378	32.084749
621.822996	33892.553948	32.089767
622.126371	33933.740577	32.094784
622.662119	33966.653173	32.099802
623.058602	34021.241372	32.104820
623.733905	34062.781304	32.109837
624.711632	34104.539778	32.114855
625.399243	34148.493093	32.119872
625.877659	34191.884764	32.124890
626.936667	34234.484361	32.129908
627.219066	34277.976271	32.134925
627.914278	34315.106906	32.139943
628.381151	34362.515445	32.144960
629.232906	34401.758837	32.149978
629.646869	34451.002990	32.154996
629.889795	34486.396121	32.160013
630.677124	34536.789938	32.165031
631.150061	34597.386710	32.170048
631.709860	34630.922528	32.175066
632.299068	34687.334941	32.180084
632.937392	34732.359329	32.185101
633.695933	34780.532686	32.190119
633.952905	34822.366853	32.195136
634.519643	34861.124377	32.200154
634.812354	34905.671844	32.205172
635.728105	34952.493381	32.210189
636.609547	35009.619874	32.215207
636.846261	35067.321083	32.220224
637.613972	35105.978223	32.225242
637.861957	35161.724244	32.230260
639.031296	35213.659840	32.235277
639.487724	35258.429147	32.240295
640.026620	35311.733984	32.245312
640.738220	35365.075297	32.250330
641.189013	35420.695588	32.255348
642.311303	35471.564280	32.260365
642.730356	35523.769183	32.265383
643.024465	35582.702122	32.270400
643.777633	35642.992712	32.275418
644.719498	35695.356916	32.280436
645.375003	35743.630706	32.285453
646.342091	35787.809489	32.290471
647.054493	35834.234685	32.295488
647.855461	35879.368978	32.300506
648.378071	35934.631681	32.305524
648.989709	35984.676931	32.310541
649.247241	36032.298845	32.315559
650.073914	36093.375958	32.320576
650.690074	36147.467557	32.325594
651.406284	36196.390513	32.330612
651.945570	36253.061467	32.335629
652.755464	36301.615995	32.340647
653.328122	36356.954204	32.345664
654.086546	36415.393532	32.350682
654.683128	36469.855734	32.355700
655.153631	36525.583343	32.360717
655.607803	36589.742289	32.365735
656.163093	36644.451642	32.370752
657.216739	36689.327014	32.375770
658.153750	36755.611733	32.380788
658.786791	36812.452951	32.385805
659.628855	36856.128601	32.390823
660.275716	36915.364415	32.395840
661.653399	36954.486410	32.400858
661.907694	37001.971886	32.405876
662.520320	37058.494455	32.410893
662.964273	37104.957893	32.415911
663.654619	37161.310555	32.420928
664.247248	37215.376913	32.425946
665.176284	37270.877008	32.430964
665.641886	37321.447672	32.435981
666.398244	37372.327297	32.440999
666.642533	37433.189071	32.446016
667.142984	37481.838724	32.451034
668.066398	37541.747760	32.456052
668.703726	37594.372718	32.461069
669.388555	37651.081638	32.466087
669.540700	37716.524044	32.471104
670.615157	37769.897103	32.476122
671.194763	37828.823423	32.481140
671.519457	37896.383160	32.486157
672.413673	37948.893117	32.491175
673.128434	38011.820628	32.496192
673.837090	38070.234290	32.501210
674.410233	38132.671996	32.506228
675.350724	38195.387846	32.511245
676.081603	38251.623244	32.516263
676.210246	38316.685398	32.521280
677.123277	38373.645265	32.526298
677.939779	38428.723226	32.531316
678.288070	38481.926539	32.536333
679.182885	38537.808336	32.541351
679.380029	38599.060171	32.546368
680.401957	38647.580697	32.551386
681.359095	38710.738117	32.556404
681.845065	38764.837631	32.561421
682.833131	38815.482251	32.566439
683.390897	38871.626067	32.571456
683.972737	38922.093873	32.576474
684.876916	38979.676450	32.581492
685.414323	39039.447394	32.586509
685.946530	39093.964230	32.591527
686.573966	39147.840321	32.596544
686.933833	39206.880507	32.601562
687.951710	39259.513539	32.606580
688.633366	39328.286968	32.611597
689.104266	39382.112124	32.616615
689.914600	39448.557685	32.621632
690.728897	39504.081411	32.626650
691.580629	39561.958283	32.631668
692.147002	39630.111900	32.636685
692.744772	39694.245115	32.641703
693.542180	39749.898581	32.646720
694.225453	39816.124738	32.651738
694.868755	39880.150231	32.656756
695.070298	39948.298401	32.661773
696.040663	40017.326305	32.666791
697.044195	40087.810132	32.671808
697.617120	40151.259240	32.676826
698.121142	40216.104244	32.681844
699.237001	40279.665257	32.686861
699.491691	40350.064135	32.691879
700.421154	40414.501997	32.696896
700.963303	40484.186196	32.701914
701.909000	40548.988734	32.706932
702.538127	40617.394973	32.711949
703.230822	40688.011350	32.716967
704.176635	40754.534684	32.721984
705.068679	40813.420504	32.727002
705.832600	40866.229782	32.732020
706.533589	40930.363225	32.737037
707.913486	40985.473828	32.742055
708.581943	41038.753739	32.747072
708.852002	41102.682824	32.752090
709.560832	41157.164697	32.757108
710.148819	41225.534978	32.762125
711.127468	41280.727764	32.767143
711.992433	41334.850580	32.772160
712.858672	41386.645926	32.777178
713.570534	41438.313639	32.782196
714.351189	41499.122321	32.787213
715.035794	41544.609164	32.792231
715.547000	41597.971839	32.797248
716.188160	41656.563789	32.802266
716.931555	41709.972811	32.807284
717.524724	41767.383511	32.812301
718.348232	41833.688838	32.817319
718.947776	41895.304740	32.822336
719.513443	41958.823480	32.827354
720.349556	42013.882190	32.832372
720.951422	42080.520025	32.837389
721.919862	42129.859898	32.842407
722.421347	42186.185471	32.847424
723.120279	42249.412344	32.852442
723.897010	42314.505736	32.857460
724.180258	42381.921429	32.862477
725.347647	42439.914924	32.867495
726.064135	42487.789527	32.872512
726.671856	42539.324252	32.877530
727.655365	42593.766939	32.882548
727.926551	42650.996054	32.887565
728.853618	42707.212437	32.892583
729.590271	42764.767854	32.897600
730.003775	42822.044831	32.902618
730.797665	42884.626260	32.907636
731.692276	42936.920518	32.912653
732.384330	42984.154863	32.917671
732.896487	43049.873509	32.922688
733.799262	43107.739184	32.927706
734.719485	43164.615597	32.932724
735.028883	43240.695074	32.937741
735.790277	43309.746922	32.942759
736.522239	43363.655094	32.947776
737.344143	43432.052751	32.952794
737.861724	43497.461956	32.957812
738.698416	43568.261262	32.962829
739.166436	43633.684910	32.967847
740.197111	43696.478459	32.972864
740.593268	43769.832765	32.977882
741.594779	43838.621180	32.982900
742.453245	43903.023416	32.987917
743.047964	43976.594179	32.992935
743.923891	44051.569889	32.997952
744.204080	44125.171131	33.002970
745.322709	44202.627023	33.007988
745.951544	44265.484738	33.013005
746.878927	44331.117246	33.018023
748.119196	44397.036485	33.023040
748.463101	44473.665122	33.028058
749.456582	44524.701648	33.033076
750.376524	44603.537171	33.038093
751.254002	44670.759800	33.043111
752.089235	44721.214172	33.048128
752.537191	44798.302135	33.053146
753.386137	44850.519465	33.058164
754.243970	44921.876437	33.063181
754.822781	44983.143619	33.068199
755.821643	45045.370315	33.073216
756.486133	45114.657929	33.078234
757.517020	45171.642448	33.083252
757.693746	45243.663124	33.088269
758.488274	45314.221532	33.093287
759.608111	45373.558491	33.098304
760.199489	45449.633256	33.103322
761.196438	45504.587054	33.108340
761.791647	45579.877284	33.113357
762.790649	45642.327020	33.118375
763.414707	45708.852120	33.123392
763.944319	45777.169647	33.128410
765.427676	45836.482876	33.133428
765.694173	45902.779554	33.138445
766.674892	45966.650011	33.143463
767.543637	46024.458992	33.148480
768.074341	46090.190053	33.153498
769.008277	46150.234874	33.158516
769.872292	46220.102129	33.163533
770.369068	46275.597468	33.168551
771.460486	46331.405233	33.173568
771.979370	46393.761003	33.178586
772.592827	46462.668525	33.183604
773.674825	46523.178390	33.188621
774.761303	46572.168166	33.193639
775.341015	46634.768173	33.198656
776.237310	46705.365724	33.203674
776.907728	46765.522797	33.208692
777.857901	46819.361070	33.213709
778.347026	46885.910660	33.218727
778.821354	46923.691871	33.223744
779.608858	46994.319915	33.228762
780.170312	47051.837765	33.233780
780.678639	47105.745504	33.238797
781.493468	47171.093883	33.243815
782.702141	47226.847660	33.248832
782.853260	47291.344459	33.253850
783.773897	47360.112014	33.258868
784.415899	47423.507935	33.263885
784.881413	47494.826612	33.268903
785.873057	47565.804237	33.273920
786.648740	47649.835120	33.278938
787.927797	47703.086575	33.283956
788.963395	47771.166900	33.288973
789.871585	47824.976150	33.293991
790.862740	47896.125697	33.299008
791.444990	47954.610533	33.304026
792.286297	48017.743018	33.309044
793.197339	48080.042396	33.314061
794.093343	48137.662761	33.319079
794.822087	48202.761811	33.324096
795.392666	48263.583702	33.329114
795.998624	48323.609444	33.334132
796.579772	48394.204386	33.339149
797.598573	48462.498174	33.344167
798.202933	48527.022826	33.349184
798.906643	48607.886233	33.354202
799.728733	48682.050676	33.359220
800.583808	48759.784731	33.364237
801.654582	48841.781221	33.369255
802.007705	48907.054635	33.374272
802.270583	48985.425732	33.379290
803.418801	49055.055047	33.384308
804.606321	49149.966127	33.389325
805.282378	49213.646441	33.394343
806.554054	49291.785631	33.399360
807.098267	49376.225871	33.404378
807.948722	49441.809324	33.409396
808.996886	49514.169789	33.414413
809.431549	49587.657251	33.419431
810.155964	49661.106170	33.424448
811.022768	49744.668740	33.429466
811.559311	49823.873208	33.434484
813.002780	49890.744889	33.439501
814.157660	49972.080673	33.444519
815.471132	50023.839057	33.449536
815.869534	50093.044139	33.454554
817.116766	50148.533349	33.459572
817.878154	50219.352620	33.464589
818.828925	50286.580539	33.469607
819.671045	50347.049355	33.474624
820.816842	50408.856673	33.479642
821.766005	50456.579168	33.484660
822.809916	50511.847825	33.489677
823.285951	50567.477078	33.494695
823.912487	50617.869531	33.499712
824.567426	50672.844810	33.504730
825.498321	50734.819326	33.509748
826.631186	50801.957135	33.514765
826.761582	50867.631443	33.519783
827.565409	50916.756832	33.524800
828.037350	50993.906405	33.529818
829.159108	51067.835775	33.534836
829.590912	51131.685973	33.539853
830.344049	51193.784301	33.544871
831.250850	51268.804423	33.549888
831.881574	51337.489878	33.554906
832.597210	51410.218110	33.559924
833.371755	51475.028267	33.564941
833.968417	51551.325081	33.569959
834.841828	51614.171421	33.574976
835.622289	51693.356996	33.579994
836.294172	51760.461784	33.585012
837.223035	51828.336671	33.590029
837.954711	51909.808443	33.595047
839.057588	51973.967781	33.600064
839.340144	52056.889364	33.605082
840.130165	52137.169615	33.610100
840.869741	52210.162382	33.615117
841.888128	52294.368646	33.620135
843.066995	52382.612522	33.625152
843.757338	52455.354292	33.630170
844.648961	52545.408891	33.635188
845.772530	52620.209811	33.640205
846.125578	52705.989140	33.645223
847.161619	52787.144516	33.650240
847.715521	52872.633758	33.655258
848.946541	52951.095397	33.660276
850.193407	53027.934937	33.665293
850.946723	53111.312188	33.670311
851.986825	53191.696353	33.675328
853.100973	53270.405058	33.680346
853.572222	53346.499474	33.685364
854.462995	53421.604968	33.690381
855.022044	53511.442964	33.695399
855.972726	53581.376113	33.700416
856.817710	53673.808946	33.705434
857.607894	53753.056951	33.710452
858.974745	53832.620446	33.715469
859.843437	53913.299544	33.720487
861.060915	53989.811433	33.725504
861.593509	54063.905310	33.730522
862.481681	54150.302707	33.735540
863.491245	54226.632579	33.740557
864.204069	54300.939613	33.745575
865.476403	54375.134473	33.750592
866.175485	54445.596625	33.755610
867.465477	54519.282942	33.760628
868.552136	54582.736889	33.765645
869.110831	54660.062260	33.770663
870.171003	54729.709673	33.775680
871.253226	54802.068657	33.780698
872.050495	54873.712835	33.785716
872.996996	54929.855124	33.790733
873.710318	55008.391573	33.795751
874.125551	55077.260777	33.800768
875.285213	55151.083265	33.805786
876.033470	55227.608933	33.810804
876.736886	55297.642627	33.815821
877.567572	55371.200595	33.820839
878.891984	55440.182462	33.825856
879.972168	55514.145023	33.830874
880.647228	55580.804606	33.835892
881.564066	55654.710763	33.840909
882.326469	55731.337111	33.845927
883.287424	55805.053344	33.850944
884.332180	55880.788207	33.855962
884.482907	55947.979763	33.860980
885.649624	56023.278413	33.865997
886.322492	56107.248348	33.871015
887.136727	56184.165529	33.876032
887.872572	56268.866673	33.881050
888.754757	56346.450960	33.886068
889.659874	56421.120758	33.891085
890.470224	56507.127508	33.896103
891.331513	56579.722497	33.901120
892.311793	56660.399916	33.906138
892.920126	56731.351308	33.911156
893.891508	56801.499607	33.916173
894.671159	56874.652472	33.921191
895.573293	56954.058311	33.926208
896.374232	57034.891487	33.931226
897.496987	57106.365151	33.936244
898.434865	57186.025677	33.941261
899.754139	57252.266883	33.946279
900.456956	57329.692419	33.951296
901.183918	57406.500544	33.956314
902.168764	57500.053060	33.961332
902.989313	57563.626010	33.966349
904.101884	57638.798948	33.971367
904.892565	57721.756237	33.976384
906.214793	57801.934918	33.981402
906.344994	57871.141360	33.986420
907.462620	57950.846064	33.991437
908.433357	58035.751069	33.996455
909.194562	58119.290263	34.001472
910.369156	58203.626155	34.006490
910.917515	58292.863631	34.011508
912.319594	58362.449450	34.016525
912.854669	58455.075688	34.021543
914.048479	58534.093242	34.026560
914.691249	58616.196879	34.031578
915.708008	58710.059261	34.036596
916.695489	58783.894459	34.041613
917.434275	58881.421111	34.046631
918.238445	58971.444079	34.051648
918.851933	59046.002872	34.056666
919.984413	59153.273461	34.061684
921.804517	59224.866393	34.066701
922.689247	59311.858976	34.071719
923.460645	59401.331655	34.076736
924.707091	59492.464984	34.081754
925.770538	59569.512438	34.086772
926.844283	59646.159776	34.091789
927.734308	59721.753610	34.096807
928.432743	59800.428331	34.101824
929.772599	59866.300075	34.106842
930.061934	59956.584063	34.111860
930.851206	60038.289932	34.116877
931.886004	60117.729836	34.121895
932.900312	60205.946048	34.126912
933.592463	60283.483974	34.131930
934.423093	60374.849905	34.136948
935.776941	60463.077490	34.141965
936.398943	60555.945062	34.146983
937.526809	60633.144095	34.152000
938.561696	60716.345797	34.157018
939.685579	60805.401635	34.162036
940.992458	60878.971934	34.167053
941.863608	60954.224385	34.172071
943.090670	61023.807098	34.177088
943.817949	61100.323042	34.182106
944.690118	61188.596574	34.187124
945.684803	61268.090768	34.192141
946.867178	61330.882997	34.197159
947.529113	61409.252081	34.202176
948.467013	61484.223580	34.207194
949.299982	61563.743904	34.212212
950.487234	61642.171218	34.217229
951.249118	61716.544154	34.222247
952.057323	61797.936445	34.227264
953.001129	61879.611739	34.232282
953.835644	61971.546387	34.237300
954.848274	62035.867069	34.242317
955.589363	62098.172900	34.247335
956.241167	62185.699377	34.252352
957.521538	62264.835813	34.257370
958.026175	62339.573510	34.262388
958.802595	62416.725241	34.267405
960.086737	62506.825767	34.272423
960.446074	62590.379513	34.277440
961.773590	62679.239518	34.282458
962.738870	62749.855381	34.287476
963.598080	62838.022889	34.292493
964.365589	62927.888851	34.297511
965.382232	63012.652080	34.302528
966.181592	63101.551500	34.307546
967.399655	63197.615372	34.312564
968.480038	63293.257917	34.317581
969.782763	63372.103214	34.322599
970.714447	63466.604772	34.327616
971.526665	63545.729546	34.332634
973.061782	63635.826758	34.337652
974.251673	63705.840631	34.342669
975.354498	63779.020863	34.347687
976.545108	63854.928779	34.352704
977.593342	63929.485353	34.357722
978.100148	64011.166055	34.362740
978.881220	64089.923899	34.367757
980.327021	64182.202061	34.372775
980.656541	64273.489483	34.377792
981.653689	64355.747042	34.382810
982.428035	64446.269475	34.387828
983.580903	64540.183565	34.392845
984.852274	64621.797892	34.397863
985.924787	64697.726751	34.402880
986.929335	64788.872989	34.407898
987.417322	64888.481973	34.412916
988.486531	64978.352669	34.417933
989.460414	65063.832241	34.422951
990.240312	65160.073157	34.427968
991.752089	65244.311062	34.432986
992.498596	65345.913838	34.438004
993.279580	65433.134044	34.443021
994.610377	65531.367181	34.448039
995.296165	65629.834053	34.453056
996.657578	65716.705319	34.458074
997.477718	65816.304253	34.463092
998.665526	65910.559897	34.468109
999.813620	65998.326365	34.473127
1000.776681	66089.243183	34.478144
1001.437774	66185.158288	34.483162
1002.908456	66282.163321	34.488180
1003.520362	66381.511989	34.493197
1004.456985	66467.337667	34.498215
1005.507050	66574.640542	34.503232
1006.627515	66651.580817	34.508250
1007.679737	66749.007324	34.513268
1009.079295	66840.118472	34.518285
1010.111056	66924.784920	34.523303
1010.705718	67017.851749	34.528320
1011.881036	67105.028992	34.533338
1012.828869	67195.591254	34.538356
1013.898199	67295.397796	34.543373
1014.869579	67391.737678	34.548391
1015.963272	67485.811214	34.553408
1017.230937	67565.396888	34.558426
1017.929479	67656.145213	34.563444
1018.742709	67746.983644	34.568461
1020.199930	67828.642702	34.573479
1021.225520	67922.766436	34.578496
1022.739346	67994.812212	34.583514
1023.493339	68079.551054	34.588532
1024.634895	68149.762061	34.593549
1025.647664	68227.895209	34.598567
1026.287585	68303.598285	34.603584
1027.120860	68374.187139	34.608602
1027.932223	68462.824970	34.613620
1028.901201	68539.193003	34.618637
1029.959437	68623.557033	34.623655
1030.885120	68723.796734	34.628672
1032.376269	68797.519885	34.633690
1033.410695	68893.874596	34.638708
1034.106723	68970.868924	34.643725
1035.477935	69046.441359	34.648743
1036.294666	69143.755341	34.653760
1037.523866	69225.770932	34.658778
1038.504491	69321.059191	34.663796
1039.431187	69414.633907	34.668813
1040.444962	69494.353728	34.673831
1041.623173	69593.310102	34.678848
1042.498313	69673.564947	34.683866
1043.501639	69771.206838	34.688884
1044.398307	69869.448247	34.693901
1045.587139	69965.263689	34.698919
1046.319195	70060.973287	34.703936
1047.500043	70160.748258	34.708954
1048.688227	70254.032016	34.713972
1049.465659	70351.844228	34.718989
1050.503475	70461.381501	34.724007
1051.430880	70560.963167	34.729024
1052.347394	70669.443718	34.734042
1053.340248	70771.808524	34.739060
1054.367173	70876.954640	34.744077
1055.416638	70981.730396	34.749095
1056.707630	71103.730972	34.754112
1057.862741	71203.108669	34.759130
1058.960253	71312.830194	34.764148
1059.809454	71421.058382	34.769165
1060.972189	71520.271454	34.774183
1062.216354	71637.152516	34.779200
1063.473056	71739.290062	34.784218
1064.333333	71847.758922	34.789236
1066.049703	71945.215634	34.794253
1067.130225	72049.471555	34.799271
1068.487177	72152.329683	34.804288
1069.394571	72239.249299	34.809306
1070.913697	72337.574076	34.814324
1071.433397	72442.995402	34.819341
1072.632304	72535.772677	34.824359
1073.842814	72638.452851	34.829376
1074.618414	72731.550013	34.834394
1075.761859	72827.832624	34.839412
1076.608231	72919.095593	34.844429
1078.167419	73009.196674	34.849447
1078.859713	73133.541672	34.854464
1080.274283	73227.503711	34.859482
1081.232432	73322.639051	34.864500
1082.350182	73425.691361	34.869517
1083.446323	73522.971796	34.874535
1084.054124	73625.065655	34.879552
1084.923049	73718.151755	34.884570
1086.458248	73824.129799	34.889588
1087.397783	73927.756434	34.894605
1088.460814	74031.997554	34.899623
1089.240244	74135.611920	34.904640
1090.762532	74239.541709	34.909658
1091.729209	74337.934568	34.914676
1092.916802	74448.871046	34.919693
1093.990257	74539.635575	34.924711
1095.168341	74632.651412	34.929728
1096.620458	74714.098457	34.934746
1097.258414	74801.967718	34.939764
1098.392723	74895.738605	34.944781
1099.533243	74994.727479	34.949799
1100.150343	75085.210228	34.954816
1101.581220	75182.989273	34.959834
1102.953960	75261.651007	34.964852
1104.026841	75357.117739	34.969869
1104.994174	75447.458525	34.974887
1106.116228	75546.490307	34.979904
1107.177151	75643.555937	34.984922
1108.493183	75738.555500	34.989940
1109.289561	75838.538401	34.994957
1110.545772	75926.391104	34.999975
1111.626934	76029.028454	35.004992
1112.761541	76118.509426	35.010010
1114.076542	76230.269456	35.015028
1114.997521	76329.588754	35.020045
1116.183164	76422.368926	35.025063
1117.144200	76538.758200	35.030080
1118.052770	76630.682835	35.035098
1119.110785	76738.431416	35.040116
1120.176495	76851.866906	35.045133
1121.506369	76955.051754	35.050151
1122.528780	77076.437436	35.055168
1123.393603	77173.361730	35.060186
1124.656001	77282.993461	35.065204
1125.645832	77398.203841	35.070221
1127.229173	77505.734346	35.075239
1128.261603	77622.193148	35.080256
1129.658488	77734.212641	35.085274
1131.017666	77838.688395	35.090292
1132.105716	77942.839381	35.095309
1133.296150	78043.883836	35.100327
1134.338770	78158.519145	35.105344
1135.619752	78264.668211	35.110362
1137.095850	78368.000326	35.115380
1137.784994	78490.077568	35.120397
1138.942519	78581.767331	35.125415
1140.155508	78682.937312	35.130432
1141.139900	78789.413275	35.135450
1142.672595	78891.433711	35.140468
1143.813460	79006.614674	35.145485
1145.079009	79109.792324	35.150503
1146.241326	79203.599049	35.155520
1147.305598	79313.345750	35.160538
1148.641947	79408.696987	35.165556
1149.503404	79513.890013	35.170573
1151.060557	79607.978708	35.175591
1152.273444	79710.799408	35.180608
1153.862650	79806.188670	35.185626
1154.859440	79903.494787	35.190644
1155.693343	80005.374731	35.195661
1156.982952	80101.014344	35.200679
1158.043827	80208.218663	35.205696
1158.902947	80315.163412	35.210714
1160.108614	80421.775910	35.215732
1161.276582	80522.959629	35.220749
1162.179697	80627.947685	35.225767
1162.786989	80750.085638	35.230784
1164.003111	80862.500702	35.235802
1165.042819	80969.977301	35.240820
1166.298091	81082.387156	35.245837
1167.813768	81187.890099	35.250855
1169.376070	81292.626014	35.255872
1170.134118	81399.704674	35.260890
1171.464950	81484.915600	35.265908
1172.586487	81587.504052	35.270925
1173.906124	81684.386039	35.275943
1174.757227	81783.862559	35.280960
1175.884245	81875.529933	35.285978
1177.165865	81968.073096	35.290996
1177.880264	82083.814618	35.296013
1179.088145	82189.255208	35.301031
1179.905472	82287.522456	35.306048
1181.236045	82400.052565	35.311066
1182.610095	82508.648647	35.316084
1183.284388	82626.805942	35.321101
1184.689515	82742.949453	35.326119
1185.703119	82858.571556	35.331136
1186.843315	82978.203559	35.336154
1188.334828	83091.940382	35.341172
1189.289061	83217.962824	35.346189
1190.020077	83335.835496	35.351207
1191.724788	83450.731589	35.356224
1193.252764	83574.626366	35.361242
1194.327737	83682.868043	35.366260
1195.281563	83803.748903	35.371277
1196.773855	83926.814507	35.376295
1198.296235	84043.920727	35.381312
1199.148777	84164.400745	35.386330
1200.714552	84287.659199	35.391348
1202.036104	84407.345002	35.396365
1202.981285	84517.637383	35.401383
1204.358519	84630.080358	35.406400
1206.004723	84753.860480	35.411418
1207.095840	84872.545069	35.416436
1208.123767	84985.145174	35.421453
1209.823828	85104.078055	35.426471
1211.157585	85220.559543	35.431488
1212.290517	85335.248096	35.436506
1213.820660	85431.920017	35.441524
1215.097235	85561.742013	35.446541
1216.162360	85671.868093	35.451559
1217.098864	85772.130868	35.456576
1218.108200	85886.752150	35.461594
1219.644539	85990.052179	35.466612
1220.544382	86112.915244	35.471629
1221.679152	86230.065355	35.476647
1223.206155	86351.666019	35.481664
1224.194700	86470.512527	35.486682
1225.694702	86585.934551	35.491700
1226.807820	86705.155455	35.496717
1227.939362	86824.107869	35.501735
1229.450612	86936.881101	35.506752
1230.303909	87064.748189	35.511770
1231.471697	87175.776378	35.516788
1232.873741	87310.427394	35.521805
1234.068196	87433.541631	35.526823
1235.198347	87542.029959	35.531840
1236.258201	87667.231704	35.536858
1237.814279	87787.275135	35.541876
1238.832087	87912.712574	35.546893
1240.008229	88039.405821	35.551911
1241.295426	88159.099778	35.556928
1242.816226	88281.811947	35.561946
1244.072684	88398.064727	35.566964
1245.005986	88520.501829	35.571981
1246.247093	88640.382333	35.576999
1247.503914	88765.849565	35.582016
1249.009608	88907.259017	35.587034
1250.356198	89024.450695	35.592052
1251.719587	89128.713843	35.597069
1252.669242	89254.661837	35.602087
1253.926532	89368.523111	35.607104
1254.859552	89485.603562	35.612122
1256.355902	89584.296812	35.617140
1257.436397	89706.753925	35.622157
1258.820077	89812.270959	35.627175
1259.952781	89908.208435	35.632192
1260.611243	90031.936533	35.637210
1262.319207	90147.200741	35.642228
1263.398931	90270.408017	35.647245
1264.695995	90387.473366	35.652263
1266.200072	90502.707314	35.657280
1267.364338	90625.535362	35.662298
1268.663121	90746.961552	35.667316
1270.033161	90863.142923	35.672333
1271.069201	90989.477673	35.677351
1272.418255	91117.120326	35.682368
1273.618618	91243.988214	35.687386
1274.775682	91359.368182	35.692404
1276.151967	91493.699992	35.697421
1278.038911	91612.287888	35.702439
1279.417598	91730.245616	35.707456
1280.573498	91859.214225	35.712474
1281.744372	91978.903596	35.717492
1283.103807	92109.603295	35.722509
1284.346479	92228.154473	35.727527
1285.792250	92351.021778	35.732544
1287.069317	92475.259319	35.737562
1288.259899	92594.770611	35.742580
1289.711582	92723.088484	35.747597
1291.250950	92851.621391	35.752615
1292.453604	92968.128417	35.757632
1293.888686	93097.008129	35.762650
1294.996724	93222.479112	35.767668
1296.369701	93337.047165	35.772685
1297.977240	93473.075493	35.777703
1299.252562	93593.654861	35.782720
1300.342568	93719.967227	35.787738
1301.901707	93836.244625	35.792756
1303.203784	93954.146843	35.797773
1304.014125	94080.402822	35.802791
1305.491426	94200.332059	35.807808
1307.190376	94335.297952	35.812826
1308.246761	94465.256364	35.817844
1309.499862	94592.117306	35.822861
1310.572881	94721.972809	35.827879
1312.109101	94839.499738	35.832896
1313.572790	94973.440313	35.837914
1314.597850	95102.430276	35.842932
1315.862573	95231.953868	35.847949
1317.275779	95361.480240	35.852967
1318.504351	95487.600812	35.857984
1319.771392	95625.453533	35.863002
1321.145089	95751.425829	35.868020
1322.734386	95885.629651	35.873037
1324.337648	96019.045978	35.878055
1325.844842	96138.902009	35.883072
1326.830370	96276.078900	35.888090
1328.171189	96395.175904	35.893108
1329.718537	96515.267970	35.898125
1330.802775	96640.997359	35.903143
1332.718357	96771.402090	35.908160
1333.723245	96890.591292	35.913178
1334.987900	97010.615169	35.918196
1336.659111	97129.714241	35.923213
1337.510009	97262.099426	35.928231
1338.760333	97379.845210	35.933248
1340.311909	97514.467515	35.938266
1341.671547	97633.997279	35.943284
1343.245172	97746.522124	35.948301
1344.170558	97865.575266	35.953319
1345.191618	97974.498058	35.958336
1346.468433	98092.736759	35.963354
1347.348967	98219.746451	35.968372
1348.494363	98341.733474	35.973389
1350.014069	98466.223411	35.978407
1351.503760	98593.951096	35.983424
1352.635308	98720.873010	35.988442
1353.818903	98852.186218	35.993460
1355.022952	98984.789834	35.998477
1356.423772	99125.476669	36.003495
1357.973232	99259.029145	36.008512
1359.337021	99388.592425	36.013530
1360.334889	99527.708396	36.018548
1361.577159	99672.631137	36.023565
1363.229033	99811.938119	36.028583
1364.956282	99945.161522	36.033600
1366.235554	100090.181803	36.038618
1367.611495	100228.709505	36.043636
1369.403685	100368.161860	36.048653
1370.520174	100507.770699	36.053671
1372.203629	100646.493202	36.058688
1373.422223	100788.559496	36.063706
1375.094040	100910.144719	36.068724
1376.588899	101051.180300	36.073741
1378.257606	101188.081815	36.078759
1379.960784	101312.465466	36.083776
1381.683489	101449.486455	36.088794
1382.562477	101575.191119	36.093812
1383.989032	101707.441652	36.098829
1384.930688	101843.444840	36.103847
1386.624462	101983.312465	36.108864
1387.787280	102113.133451	36.113882
1389.098984	102257.321588	36.118900
1390.450686	102386.974797	36.123917
1391.961678	102528.280487	36.128935
1393.641376	102666.720563	36.133952
1394.943086	102810.316796	36.138970
1396.184061	102945.377786	36.143988
1397.381134	103077.415985	36.149005
1398.684771	103237.445201	36.154023
1400.336125	103382.751831	36.159040
1401.911916	103532.394309	36.164058
1403.242981	103665.187399	36.169076
1404.219392	103806.366222	36.174093
1405.511113	103957.601650	36.179111
1407.599754	104085.701422	36.184128
1409.252884	104237.084731	36.189146
1410.525060	104387.437621	36.194164
1411.966132	104525.529549	36.199181
1413.154039	104667.921653	36.204199
1414.347489	104810.440292	36.209216
1416.029597	104953.504763	36.214234
1417.112523	105105.690791	36.219252
1418.798289	105240.197364	36.224269
1419.794712	105396.201987	36.229287
1421.547511	105536.202188	36.234304
1422.829993	105692.379209	36.239322
1424.154389	105837.519164	36.244340
1425.853919	105985.961465	36.249357
1427.216194	106130.310641	36.254375
1429.243105	106263.500221	36.259392
1430.766170	106402.817022	36.264410
1432.245978	106536.092827	36.269428
1433.847943	106670.098257	36.274445
1435.047280	106812.307426	36.279463
1436.663857	106940.821218	36.284480
1437.822846	107076.342716	36.289498
1439.195069	107196.235014	36.294516
1440.739209	107311.650238	36.299533
1441.866833	107440.191292	36.304551
1443.417691	107564.178143	36.309568
1444.548362	107686.227356	36.314586
1445.770770	107813.436305	36.319604
1447.176668	107956.531061	36.324621
1448.320058	108092.376011	36.329639
1449.619667	108229.313065	36.334656
1451.442721	108364.152984	36.339674
1452.670541	108520.249999	36.344692
1454.065123	108658.086974	36.349709
1455.439541	108807.847502	36.354727
1456.631908	108959.107981	36.359744
1458.375762	109112.515106	36.364762
1459.487191	109254.710003	36.369780
1461.308835	109395.146418	36.374797
1462.577804	109557.366575	36.379815
1464.101243	109706.384960	36.384832
1465.774160	109858.386134	36.389850
1467.174986	110022.692989	36.394868
1468.697618	110172.968921	36.399885
1469.864306	110336.134335	36.404903
1471.556233	110497.164380	36.409920
1473.263842	110655.288686	36.414938
1474.581219	110812.599420	36.419956
1476.241856	110964.366343	36.424973
1477.649318	111122.881861	36.429991
1479.491647	111283.029739	36.435008
1480.837301	111427.809386	36.440026
1482.207217	111590.847511	36.445044
1483.860866	111749.834783	36.450061
1485.163155	111911.629409	36.455079
1486.867750	112066.551981	36.460096
1488.469337	112221.199574	36.465114
1489.563448	112380.733298	36.470132
1491.908519	112536.686920	36.475149
1493.410012	112697.769270	36.480167
1495.283610	112844.362128	36.485184
1496.792987	112989.731371	36.490202
1498.223363	113147.098235	36.495220
1500.027227	113291.966302	36.500237
1500.987256	113435.926336	36.505255
1502.443572	113587.571338	36.510272
1504.560350	113741.650673	36.515290
1505.707339	113893.839720	36.520308
1507.393778	114043.662579	36.525325
1509.310370	114194.578988	36.530343
1510.022570	114344.060098	36.535360
1511.873287	114490.219298	36.540378
1513.254306	114649.604241	36.545396
1514.618117	114802.930158	36.550413
1516.827192	114953.195410	36.555431
1518.296691	115094.229059	36.560448
1519.396343	115234.851544	36.565466
1520.689538	115405.858388	36.570484
1522.558316	115547.985792	36.575501
1524.199064	115703.758258	36.580519
1525.363965	115864.310916	36.585536
1526.805774	116011.313499	36.590554
1528.117723	116170.335291	36.595572
1529.546274	116326.663426	36.600589
1531.006446	116488.276286	36.605607
1532.511283	116643.300173	36.610624
1534.074695	116793.216812	36.615642
1535.146227	116967.005010	36.620660
1536.784843	117130.279800	36.625677
1538.408119	117280.315916	36.630695
1539.866907	117429.325485	36.635712
1541.603581	117571.493884	36.640730
1542.870271	117722.576608	36.645748
1544.111244	117869.097742	36.650765
1545.259864	118036.613061	36.655783
1546.833646	118184.960848	36.660800
1548.514424	118339.089175	36.665818
1549.881470	118509.299666	36.670836
1551.484500	118665.585039	36.675853
1553.245270	118838.627717	36.680871
1554.316040	119002.963011	36.685888
1556.021975	119177.575933	36.690906
1557.183628	119342.443973	36.695924
1559.165223	119505.269756	36.700941
1560.744557	119681.528298	36.705959
1562.507216	119845.797588	36.710976
1564.352454	120023.335511	36.715994
1565.710042	120197.182808	36.721012
1567.347314	120365.406084	36.726029
1569.086806	120545.106593	36.731047
1570.425458	120722.853438	36.736064
1572.121239	120894.367972	36.741082
1573.560993	121069.043612	36.746100
1575.348395	121255.602525	36.751117
1577.049967	121428.983219	36.756135
1578.782114	121606.748981	36.761152
1580.194606	121786.062157	36.766170
1581.687285	121961.456621	36.771188
1583.200311	122146.172401	36.776205
1585.196663	122323.557799	36.781223
1586.610081	122508.011708	36.786240
1588.372486	122680.601987	36.791258
1590.113649	122866.833275	36.796276
1591.817605	123034.423416	36.801293
1593.490290	123218.041102	36.806311
1594.370196	123390.061441	36.811328
1596.106942	123584.377586	36.816346
1597.368984	123774.810589	36.821364
1599.160891	123964.882943	36.826381
1600.895618	124149.966841	36.831399
1602.635169	124341.812485	36.836416
1604.150339	124525.168938	36.841434
1605.887545	124708.834195	36.846452
1607.293133	124904.958989	36.851469
1608.956613	125098.646899	36.856487
1610.713402	125275.562614	36.861504
1612.244942	125468.981052	36.866522
1613.634585	125660.456103	36.871540
1615.317164	125850.110358	36.876557
1617.263701	126045.052761	36.881575
1618.578754	126228.029429	36.886592
1620.700957	126425.153777	36.891610
1622.242100	126615.049278	36.896628
1624.143460	126803.506736	36.901645
1625.857769	126980.322290	36.906663
1627.323363	127169.242541	36.911680
1629.344293	127354.017404	36.916698
1630.607387	127556.596726	36.921716
1632.033892	127741.871825	36.926733
1633.606824	127933.468521	36.931751
1634.973428	128120.911446	36.936768
1636.689625	128308.376928	36.941786
1637.911048	128509.051609	36.946804
1640.012019	128697.778432	36.951821
1641.868670	128885.922451	36.956839
1643.217398	129072.598498	36.961856
1645.012253	129257.658060	36.966874
1646.317180	129431.109433	36.971892
1647.764810	129625.245519	36.976909
1649.534922	129798.664063	36.981927
1650.763353	129972.560945	36.986944
1652.468065	130155.265864	36.991962
1653.836182	130338.671037	36.996980
1655.465129	130543.199825	37.001997
1656.779922	130739.315615	37.007015
1658.223694	130934.003861	37.012032
1660.087656	131136.773339	37.017050
1661.282732	131342.604218	37.022068
1662.920682	131547.796183	37.027085
1664.447576	131741.891493	37.032103
1666.077768	131966.106357	37.037120
1667.699447	132185.387924	37.042138
1669.656351	132399.923696	37.047156
1670.858926	132624.513038	37.052173
1673.401583	132835.584643	37.057191
1674.606319	133058.056885	37.062208
1676.501060	133262.975894	37.067226
1678.258651	133492.165434	37.072244
1679.995387	133704.026469	37.077261
1681.776636	133934.686532	37.082279
1682.955967	134153.323523	37.087296
1684.484668	134379.063823	37.092314
1686.800029	134613.489059	37.097332
1688.270707	134833.314889	37.102349
1689.981018	135055.528142	37.107367
1691.549114	135293.144038	37.112384
1693.803693	135514.348538	37.117402
1695.724582	135736.354735	37.122420
1697.945001	135963.454641	37.127437
1699.655979	136175.889742	37.132455
1701.064578	136386.837460	37.137472
1703.161784	136598.744912	37.142490
1704.931936	136827.898806	37.147508
1706.632965	137058.206687	37.152525
1708.597173	137278.792420	37.157543
1710.349839	137488.689176	37.162560
1712.302362	137699.951679	37.167578
1713.780462	137917.849722	37.172596
1715.447508	138136.937631	37.177613
1716.991708	138352.923923	37.182631
1718.682121	138575.791924	37.187648
1720.005902	138800.126671	37.192666
1721.571104	139028.523890	37.197684
1723.367745	139250.769442	37.202701
1725.142949	139483.577822	37.207719
1727.065286	139722.747774	37.212736
1728.532152	139949.553075	37.217754
1730.093708	140177.194996	37.222772
1732.111689	140405.020784	37.227789
1734.428795	140637.572827	37.232807
1735.660917	140864.748987	37.237824
1737.232991	141087.431511	37.242842
1739.030486	141331.134229	37.247860
1740.527909	141565.595078	37.252877
1742.536449	141792.692853	37.257895
1744.410493	142031.767652	37.262912
1746.340094	142258.968736	37.267930
1747.772851	142478.392338	37.272948
1749.652700	142720.629733	37.277965
1751.507858	142941.119195	37.282983
1753.175645	143178.822974	37.288000
1754.967428	143397.598317	37.293018
1757.112379	143626.079443	37.298036
1758.483351	143865.292249	37.303053
1760.590155	144083.881989	37.308071
1761.837868	144296.628608	37.313088
1763.920269	144501.555026	37.318106
1765.615403	144718.434774	37.323124
1767.359078	144928.847750	37.328141
1768.697884	145135.923189	37.333159
1770.133489	145352.592226	37.338176
1771.831513	145580.631471	37.343194
1773.408068	145807.484900	37.348212
1774.818197	146032.905649	37.353229
1776.899333	146261.357929	37.358247
1778.767923	146503.843858	37.363264
1780.374926	146727.295112	37.368282
1781.948752	146971.834510	37.373300
1783.506900	147214.968648	37.378317
1785.366217	147457.155888	37.383335
1786.958875	147712.433693	37.388352
1788.749981	147962.985599	37.393370
1790.291543	148213.526774	37.398388
1791.916257	148472.078007	37.403405
1793.827295	148723.592221	37.408423
1795.519713	148991.756601	37.413440
1797.156292	149253.851121	37.418458
1799.092451	149515.633756	37.423476
1800.718184	149792.151838	37.428493
1802.744688	150055.382756	37.433511
1804.868818	150336.535219	37.438528
1806.168402	150605.352720	37.443546
1808.238909	150885.970579	37.448564
1809.784538	151153.737040	37.453581
1811.637148	151425.836271	37.458599
1814.047664	151713.869209	37.463616
1815.885391	151983.028632	37.468634
1817.591490	152265.665090	37.473652
1819.475841	152543.908622	37.478669
1821.727606	152823.454595	37.483687
1823.431556	153100.142267	37.488704
1825.048825	153383.674100	37.493722
1826.730792	153662.538619	37.498740
1828.879820	153948.389689	37.503757
1830.786450	154226.320749	37.508775
1832.510372	154499.051626	37.513792
1834.407483	154766.755342	37.518810
1837.379440	155037.593528	37.523828
1839.049219	155309.130735	37.528845
1841.053242	155574.587377	37.533863
1842.832828	155841.044942	37.538880
1844.835671	156118.868621	37.543898
1846.369689	156387.613826	37.548916
1848.448741	156669.744403	37.553933
1849.982948	156929.973984	37.558951
1851.752178	157203.078655	37.563968
1853.495872	157474.639795	37.568986
1855.701641	157739.985960	37.574004
1857.103701	158025.986020	37.579021
1859.331231	158300.116143	37.584039
1860.704447	158578.265145	37.589056
1862.720465	158871.562152	37.594074
1864.578744	159138.149195	37.599092
1866.358500	159422.852946	37.604109
1868.090816	159706.232402	37.609127
1870.043670	159981.872794	37.614144
1871.970045	160256.998027	37.619162
1873.718269	160533.269401	37.624180
1875.574446	160821.979448	37.629197
1877.700468	161105.354795	37.634215
1879.305512	161387.555639	37.639232
1881.047932	161676.008008	37.644250
1882.965222	161946.660500	37.649268
1884.947050	162222.077697	37.654285
1886.653829	162491.711515	37.659303
1888.160368	162763.040784	37.664320
1889.407888	163031.897717	37.669338
1891.244714	163306.542275	37.674356
1892.904200	163601.821223	37.679373
1894.539725	163888.941658	37.684391
1895.868555	164183.893805	37.689408
1897.566832	164486.712189	37.694426
1899.799055	164790.426465	37.699444
1901.280472	165097.978991	37.704461
1903.422116	165399.488277	37.709479
1905.745235	165716.663440	37.714496
1907.409143	166037.903986	37.719514
1909.352668	166337.797740	37.724532
1911.189683	166658.227077	37.729549
1913.274048	166974.810413	37.734567
1914.967247	167288.980218	37.739584
1916.996724	167626.930941	37.744602
1918.679081	167942.997196	37.749620
1920.679934	168268.779207	37.754637
1922.607979	168594.307414	37.759655
1924.580576	168925.746979	37.764672
1926.503849	169257.449697	37.769690
1928.364419	169586.383032	37.774708
1930.322113	169917.537448	37.779725
1932.636721	170257.170364	37.784743
1934.488317	170580.865627	37.789760
1936.349882	170927.835002	37.794778
1938.577501	171266.317948	37.799796
1940.596563	171604.911073	37.804813
1942.650366	171942.281354	37.809831
1944.701139	172279.285383	37.814848
1946.650750	172624.801369	37.819866
1948.764233	172960.820929	37.824884
1951.005755	173294.688806	37.829901
1952.640087	173640.093342	37.834919
1954.814433	173962.470330	37.839936
1956.768171	174310.748620	37.844954
1958.683910	174643.530139	37.849972
1960.818315	174995.846668	37.854989
1962.783229	175327.086922	37.860007
1964.736816	175668.069763	37.865024
1966.243260	176020.361516	37.870042
1968.262738	176360.041782	37.875060
1970.062199	176709.294105	37.880077
1972.145677	177060.103687	37.885095
1973.953229	177407.503722	37.890112
1975.880586	177762.759583	37.895130
1978.305396	178112.885510	37.900148
1980.039607	178474.523654	37.905165
1982.486634	178810.553580	37.910183
1984.991946	179155.312413	37.915200
1987.066813	179484.824964	37.920218
1989.145438	179830.186206	37.925236
1991.320752	180168.346225	37.930253
1993.232297	180506.370794	37.935271
1995.245217	180851.136669	37.940288
1996.916123	181198.928637	37.945306
1998.688082	181537.258153	37.950324
2000.412832	181896.625870	37.955341
2002.238052	182238.632387	37.960359
2004.424763	182579.796550	37.965376
2006.453636	182939.120943	37.970394
2008.617899	183283.821512	37.975412
2010.373766	183653.274270	37.980429
2011.898210	184003.182102	37.985447
2013.970623	184339.950961	37.990464
2015.567853	184689.468939	37.995482
2017.675117	185030.044553	38.000500
2019.637957	185366.681564	38.005517
2021.375774	185717.603604	38.010535
2023.213261	186064.015691	38.015552
2025.096288	186417.863844	38.020570
2027.176389	186784.915594	38.025588
2029.091827	187202.310551	38.030605
2030.824906	187551.232989	38.035623
2033.283889	187910.940031	38.040640
2035.257967	188271.663534	38.045658
2037.591388	188624.305980	38.050676
2039.231876	188989.249339	38.055693
2041.264897	189356.622006	38.060711
2044.015620	189723.630184	38.065728
2045.752096	190084.193376	38.070746
2047.675270	190454.558527	38.075764
2049.726543	190827.089357	38.080781
2051.840519	191192.626523	38.085799
2054.242171	191562.590530	38.090816
2056.203669	191933.386206	38.095834
2057.995512	192300.094534	38.100852
2059.974630	192698.373256	38.105869
2061.785497	193070.745285	38.110887
2064.581268	193442.457131	38.115904
2066.438044	193828.515316	38.120922
2068.501846	194219.190832	38.125940
2070.930966	194607.676989	38.130957
2072.850011	194986.413448	38.135975
2074.905547	195370.006783	38.140992
2076.392173	195774.213989	38.146010
2078.645605	196161.309557	38.151028
2080.924293	196558.867673	38.156045
2083.023068	196946.472136	38.161063
2085.510016	197341.967944	38.166080
2087.326408	197743.995818	38.171098
2089.346614	198130.320236	38.176116
2091.927634	198538.327706	38.181133
2093.757051	198927.833716	38.186151
2095.909991	199322.345357	38.191168
2098.061789	199725.240838	38.196186
2100.128357	200125.813638	38.201204
2102.099840	200523.023769	38.206221
2104.283985	200932.674245	38.211239
2106.247814	201339.235561	38.216256
2108.080409	201749.908064	38.221274
2110.068125	202157.178910	38.226292
2112.207071	202580.506908	38.231309
2114.319805	202993.653620	38.236327
2116.826252	203409.788318	38.241344
2118.974504	203824.607977	38.246362
2121.241522	204226.657957	38.251380
2123.397033	204641.757730	38.256397
2125.558938	205054.926797	38.261415
2127.873417	205465.075459	38.266432
2129.735156	205881.442914	38.271450
2132.061561	206290.321254	38.276468
2134.371520	206696.281617	38.281485
2136.571791	207102.132811	38.286503
2139.339166	207511.757768	38.291520
2141.269784	207924.155628	38.296538
2143.399542	208316.912019	38.301556
2145.679262	208722.702972	38.306573
2147.365747	209129.069603	38.311591
2150.368354	209527.560299	38.316608
2152.296365	209927.692262	38.321626
2154.323433	210329.867106	38.326644
2156.481820	210717.110343	38.331661
2158.323895	211095.181925	38.336679
2160.542153	211466.946230	38.341696
2162.815581	211846.856956	38.346714
2164.470839	212220.488101	38.351732
2166.443938	212604.663528	38.356749
2167.920935	212993.844939	38.361767
2170.263018	213388.785833	38.366784
2172.010487	213792.533194	38.371802
2174.253875	214198.236152	38.376820
2176.252246	214612.487954	38.381837
2178.228423	215015.845483	38.386855
2180.208191	215439.729124	38.391872
2182.051501	215865.971609	38.396890
2183.720213	216290.006178	38.401908
2185.800458	216718.829256	38.406925
2187.842424	217165.034945	38.411943
2190.310433	217607.796039	38.416960
2191.823649	218057.666794	38.421978
2194.210354	218518.325688	38.426996
2196.550025	218971.523523	38.432013
2198.749728	219432.796547	38.437031
2200.756227	219878.476525	38.442048
2203.166522	220356.611076	38.447066
2205.135839	220827.040937	38.452084
2207.616194	221295.740277	38.457101
2209.432639	221759.005107	38.462119
2212.035608	222228.600378	38.467136
2214.559815	222713.120293	38.472154
2216.590458	223186.971279	38.477172
2218.847160	223653.648685	38.482189
2220.992989	224156.645909	38.487207
2223.326030	224626.842824	38.492224
2225.739384	225110.720117	38.497242
2228.314596	225594.800902	38.502260
2230.363132	226074.695781	38.507277
2233.108230	226544.727072	38.512295
2236.072128	227015.257763	38.517312
2238.054858	227492.469941	38.522330
2240.756859	227969.366860	38.527348
2243.321633	228439.298897	38.532365
2245.434413	228900.460523	38.537383
2248.060505	229362.050188	38.542400
2250.450780	229826.165968	38.547418
2252.477640	230293.284967	38.552436
2254.586407	230750.585031	38.557453
2256.919760	231233.152288	38.562471
2259.339037	231689.234907	38.567488
2262.068398	232157.031015	38.572506
2264.331890	232624.264190	38.577524
2266.210371	233084.875688	38.582541
2268.376571	233558.245609	38.587559
2270.568646	234012.786798	38.592576
2273.143890	234485.558731	38.597594
2275.420577	234951.339792	38.602612
2277.267392	235415.840870	38.607629
2279.560423	235890.560535	38.612647
2281.493449	236360.483558	38.617664
2284.159830	236838.141636	38.622682
2286.199895	237320.291414	38.627700
2288.830685	237778.875628	38.632717
2291.056331	238260.207717	38.637735
2293.381085	238738.017986	38.642752
2295.492496	239209.179605	38.647770
2297.990497	239681.017040	38.652788
2300.051664	240158.053205	38.657805
2302.431904	240631.965106	38.662823
2304.587611	241099.103033	38.667840
2306.989599	241564.677620	38.672858
2309.295005	242021.045012	38.677876
2311.379578	242480.951596	38.682893
2313.583011	242936.342457	38.687911
2315.606021	243388.407317	38.692928
2317.821200	243842.473642	38.697946
2320.012559	244307.466077	38.702964
2322.178264	244768.016006	38.707981
2324.204249	245261.915349	38.712999
2326.356975	245719.112060	38.718016
2328.285103	246207.232536	38.723034
2330.483152	246704.531020	38.728052
2332.921730	247188.479802	38.733069
2334.804886	247690.117819	38.738087
2337.162461	248196.456341	38.743104
2339.514503	248697.917047	38.748122
2341.853283	249203.900042	38.753140
2344.161047	249712.274221	38.758157
2346.106736	250224.513580	38.763175
2348.648141	250745.955865	38.768192
2351.602278	251268.805586	38.773210
2353.696940	251783.963542	38.778228
2356.562902	252290.363126	38.783245
2358.898357	252815.132942	38.788263
2361.232020	253336.192564	38.793280
2363.595605	253863.672327	38.798298
2365.632200	254413.910077	38.803316
2368.419659	254925.825042	38.808333
2370.876066	255456.078659	38.813351
2373.241336	255981.314969	38.818368
2376.322222	256502.018072	38.823386
2379.105502	257029.547548	38.828404
2382.463127	257543.497596	38.833421
2384.464652	258053.973510	38.838439
2387.310484	258572.190218	38.843456
2389.801912	259069.707579	38.848474
2391.928823	259588.793941	38.853492
2394.268527	260098.218188	38.858509
2396.882608	260615.471671	38.863527
2398.969836	261116.294713	38.868544
2401.384556	261643.353759	38.873562
2403.591722	262173.160474	38.878580
2406.212495	262696.778954	38.883597
2408.319294	263211.051636	38.888615
2410.674022	263724.622925	38.893632
2413.311223	264246.326459	38.898650
2415.289277	264778.492969	38.903668
2417.918688	265305.526361	38.908685
2420.517855	265835.127090	38.913703
2422.909569	266368.973594	38.918720
2424.850712	266906.367038	38.923738
2427.422785	267439.290812	38.928756
2429.991811	267989.635603	38.933773
2432.347549	268519.513917	38.938791
2434.535513	269063.841646	38.943808
2436.711826	269604.256740	38.948826
2439.415620	270153.704504	38.953844
2441.750025	270693.174326	38.958861
2443.885185	271245.954961	38.963879
2446.380438	271796.288794	38.968896
2448.884743	272336.382663	38.973914
2450.787200	272902.827614	38.978932
2453.700547	273452.628857	38.983949
2456.005477	274022.864179	38.988967
2458.118360	274572.935154	38.993984
2460.897655	275134.809800	38.999002
2463.045398	275700.994721	39.004020
2465.673740	276261.894716	39.009037
2468.421603	276813.274109	39.014055
2470.876734	277346.714993	39.019072
2473.398518	277875.062776	39.024090
2475.597862	278405.895154	39.029108
2478.443881	278932.712384	39.034125
2480.594021	279462.503956	39.039143
2483.295033	279995.482071	39.044160
2485.905626	280516.280976	39.049178
2488.374275	281053.477885	39.054196
2490.660787	281592.197511	39.059213
2492.878663	282132.295147	39.064231
2495.309844	282684.874847	39.069248
2498.025692	283221.534822	39.074266
2499.826739	283780.603376	39.079284
2502.495655	284327.267387	39.084301
2504.608845	284889.122603	39.089319
2507.066885	285460.188060	39.094336
2509.891276	286031.267922	39.099354
2512.605182	286600.836613	39.104372
2514.996778	287170.780736	39.109389
2517.783435	287742.232817	39.114407
2520.277073	288323.882341	39.119424
2523.063407	288892.683694	39.124442
2525.234082	289469.117145	39.129460
2527.909852	290048.742293	39.134477
2530.463332	290636.582504	39.139495
2532.875869	291217.101215	39.144512
2535.516989	291796.969584	39.149530
2537.901294	292398.581237	39.154548
2540.756242	292984.016424	39.159565
2543.572144	293576.611989	39.164583
2545.781009	294159.470418	39.169600
2548.684224	294746.505908	39.174618
2551.130797	295345.209463	39.179636
2553.715681	295951.476655	39.184653
2556.233223	296554.777551	39.189671
2558.528984	297152.140403	39.194688
2561.333603	297761.807197	39.199706
2563.624390	298371.852057	39.204724
2566.195002	298984.512444	39.209741
2568.714523	299607.608198	39.214759
2571.242755	300214.219467	39.219776
2574.790997	300808.885892	39.224794
2577.683622	301422.382984	39.229812
2580.027568	302022.706958	39.234829
2582.885149	302617.232470	39.239847
2585.155846	303224.713114	39.244864
2587.911088	303826.551993	39.249882
2590.183428	304441.278482	39.254900
2593.117180	305056.199379	39.259917
2595.662502	305663.126555	39.264935
2597.825877	306281.985678	39.269952
2600.800920	306893.425820	39.274970
2603.812211	307495.714870	39.279988
2606.340190	308106.448290	39.285005
2609.058476	308717.880673	39.290023
2611.308228	309334.150274	39.295040
2614.456492	309933.190101	39.300058
2616.562905	310547.740662	39.305076
2618.979010	311165.103295	39.310093
2621.877563	311780.327003	39.315111
2624.363225	312401.698388	39.320128
2626.815411	313017.305417	39.325146
2629.252699	313638.515679	39.330164
2631.811314	314259.774892	39.335181
2634.375563	314885.440890	39.340199
2636.835171	315518.550706	39.345216
2639.976557	316139.186150	39.350234
2642.342170	316755.061131	39.355252
2645.038357	317347.680646	39.360269
2647.487168	317943.756772	39.365287
2650.027643	318549.834680	39.370304
2652.670435	319140.281426	39.375322
2655.272540	319750.647241	39.380340
2657.593512	320339.224562	39.385357
2660.093861	320951.314870	39.390375
2662.406051	321564.516870	39.395392
2665.607972	322169.857501	39.400410
2667.850402	322792.720592	39.405428
2670.189934	323420.786497	39.410445
2673.085913	324048.908611	39.415463
2675.547448	324696.601232	39.420480
2677.947070	325332.976805	39.425498
2680.481776	325984.418372	39.430516
2683.109946	326632.764891	39.435533
2685.445266	327271.403689	39.440551
2687.871521	327943.204392	39.445568
2690.552488	328604.069870	39.450586
2693.105393	329281.029386	39.455604
2695.969840	329957.370638	39.460621
2698.855700	330630.855431	39.465639
2701.745854	331327.921550	39.470656
2704.324101	331998.741270	39.475674
2706.951349	332699.933251	39.480692
2709.846248	333382.577302	39.485709
2713.151856	334070.066469	39.490727
2716.160258	334753.911077	39.495744
2718.796595	335424.280590	39.500762
2721.872367	336119.225683	39.505780
2724.225573	336807.243809	39.510797
2727.113131	337499.072149	39.515815
2730.105646	338191.758802	39.520832
2733.084999	338880.528151	39.525850
2735.943873	339570.190814	39.530868
2738.576388	340269.614965	39.535885
2741.453980	340953.236866	39.540903
2743.903071	341652.915920	39.545920
2746.619852	342347.061222	39.550938
2749.613139	343038.004892	39.555956
2751.990671	343754.442251	39.560973
2754.848710	344454.204295	39.565991
2757.688565	345162.678686	39.571008
2760.722183	345860.051549	39.576026
2763.803263	346561.460091	39.581044
2767.035100	347255.425963	39.586061
2770.135832	347935.958260	39.591079
2773.195386	348626.980963	39.596096
2776.230655	349318.981946	39.601114
2778.905818	349996.774268	39.606132
2781.474850	350690.923478	39.611149
2784.664530	351372.714807	39.616167
2787.205373	352067.041853	39.621184
2789.614002	352759.625091	39.626202
2792.024095	353450.215568	39.631220
2794.935376	354148.876732	39.636237
2797.656441	354842.988675	39.641255
2799.874021	355548.495940	39.646272
2802.516173	356254.884611	39.651290
2805.561091	356963.298708	39.656308
2808.424315	357669.189892	39.661325
2811.617612	358368.143849	39.666343
2813.965381	359074.716735	39.671360
2817.298396	359791.943670	39.676378
2820.174161	360483.547580	39.681396
2822.858583	361197.090693	39.686413
2825.665791	361887.202903	39.691431
2828.084273	362595.862206	39.696448
2831.030407	363273.729293	39.701466
2834.134963	363953.203601	39.706484
2836.656781	364633.259785	39.711501
2839.133183	365312.268158	39.716519
2841.269029	365999.296753	39.721536
2844.364177	366682.333087	39.726554
2846.790991	367374.859059	39.731572
2849.263384	368078.663400	39.736589
2852.514388	368789.475271	39.741607
2855.108654	369490.007539	39.746624
2857.807902	370198.411976	39.751642
2860.597770	370926.067176	39.756660
2863.365683	371646.536238	39.761677
2866.283576	372377.731685	39.766695
2868.805580	373117.355873	39.771712
2871.361465	373848.290061	39.776730
2874.400160	374597.573722	39.781748
2877.220638	375346.972113	39.786765
2879.989201	376103.983398	39.791783
2882.969777	376875.228373	39.796800
2885.305870	377628.818830	39.801818
2888.442846	378392.877409	39.806836
2891.468073	379160.148472	39.811853
2894.499715	379936.388531	39.816871
2897.670473	380719.119068	39.821888
2900.563985	381499.361828	39.826906
2903.626254	382274.540046	39.831924
2906.249607	383064.225226	39.836941
2909.525184	383852.087884	39.841959
2912.382980	384642.549270	39.846976
2915.040966	385429.193247	39.851994
2918.642815	386226.124838	39.857012
2921.129574	387022.166590	39.862029
2924.394302	387823.607719	39.867047
2927.058002	388620.027078	39.872064
2930.114420	389418.258934	39.877082
2932.959827	390210.750286	39.882100
2935.918847	391028.669602	39.887117
2939.074130	391836.049337	39.892135
2942.796167	392633.136553	39.897152
2945.581009	393434.343503	39.902170
2948.802671	394239.506474	39.907188
2951.848758	395045.277396	39.912205
2954.514929	395843.688611	39.917223
2957.965501	396653.139497	39.922240
2960.946913	397470.533241	39.927258
2963.985589	398271.589156	39.932276
2966.732938	399080.762514	39.937293
2969.735779	399884.249349	39.942311
2972.266045	400706.763673	39.947328
2975.455168	401513.759005	39.952346
2978.546519	402315.882340	39.957364
2981.676513	403121.565117	39.962381
2985.212521	403930.496603	39.967399
2987.999073	404739.212283	39.972416
2991.162604	405545.006412	39.977434
2994.133201	406355.659853	39.982452
2996.656482	407164.228262	39.987469
2999.946554	407971.636038	39.992487
3003.059974	408766.088431	39.997504
3005.861886	409583.734632	40.002522
3008.874853	410390.034725	40.007540
3012.235982	411186.891066	40.012557
3015.090796	411998.013561	40.017575
3018.002430	412811.069976	40.022592
3021.143913	413614.296488	40.027610
3024.690500	414405.390384	40.032628
3027.228763	415208.347689	40.037645
3030.319053	415977.096014	40.042663
3033.843229	416730.018294	40.047680
3037.050168	417480.181310	40.052698
3040.236977	418241.194966	40.057716
3042.831946	419004.144463	40.062733
3045.791242	419758.411899	40.067751
3048.730756	420533.237946	40.072768
3051.182090	421291.928601	40.077786
3054.248515	422059.749710	40.082804
3057.034877	422850.239512	40.087821
3060.209122	423636.239394	40.092839
3063.494388	424423.506383	40.097856
3065.658848	425216.175614	40.102874
3068.791611	426008.157583	40.107892
3071.934768	426805.516403	40.112909
3075.699688	427610.127791	40.117927
3078.563398	428404.686031	40.122944
3081.494095	429206.936403	40.127962
3084.702711	430012.801150	40.132980
3088.072928	430820.427580	40.137997
3091.227348	431629.823522	40.143015
3094.382968	432449.092141	40.148032
3097.843254	433252.409435	40.153050
3101.320101	434060.087788	40.158068
3104.088299	434883.205643	40.163085
3107.051938	435700.345560	40.168103
3110.425757	436515.517260	40.173120
3113.719754	437339.307197	40.178138
3116.469884	438154.657631	40.183156
3119.686722	438989.655715	40.188173
3122.902295	439817.746064	40.193191
3125.923770	440664.068126	40.198208
3128.595254	441500.707012	40.203226
3131.726310	442341.783388	40.208244
3134.852298	443190.500639	40.213261
3137.729616	444052.754777	40.218279
3140.762016	444905.549886	40.223296
3143.721569	445778.165883	40.228314
3146.876478	446639.851544	40.233332
3149.939528	447512.469698	40.238349
3153.089819	448379.275468	40.243367
3156.387132	449261.468905	40.248384
3159.062757	450146.392125	40.253402
3162.715278	451028.292185	40.258420
3165.841126	451916.642865	40.263437
3169.430017	452791.397196	40.268455
3172.688022	453676.357731	40.273472
3175.821630	454568.663655	40.278490
3179.389243	455439.453591	40.283508
3182.290260	456339.227189	40.288525
3185.549846	457227.592425	40.293543
3188.697482	458112.295755	40.298560
3191.360698	459008.283872	40.303578
3194.572859	459905.805443	40.308596
3197.814732	460807.464009	40.313613
3201.264032	461713.281535	40.318631
3204.491061	462624.888235	40.323648
3207.508060	463523.864786	40.328666
3210.575155	464417.488215	40.333684
3213.926130	465335.337106	40.338701
3217.006305	466241.272346	40.343719
3220.144142	467148.461094	40.348736
3223.033366	468064.516908	40.353754
3226.564185	468978.656936	40.358772
3229.884243	469898.982865	40.363789
3233.210392	470810.733120	40.368807
3236.342080	471714.293154	40.373824
3239.331901	472618.329568	40.378842
3242.879295	473497.369360	40.383860
3246.053181	474381.209751	40.388877
3249.375617	475252.323304	40.393895
3252.924301	476119.623638	40.398912
3256.102179	476993.236556	40.403930
3259.446145	477852.963094	40.408948
3262.198152	478740.510597	40.413965
3265.102014	479602.630602	40.418983
3268.662063	480492.172068	40.424000
3271.310703	481376.361881	40.429018
3274.936666	482275.166680	40.434036
3277.942275	483180.265278	40.439053
3280.969114	484085.610351	40.444071
3284.426540	485001.064529	40.449088
3287.318425	485907.886190	40.454106
3291.136752	486808.665936	40.459124
3294.446127	487731.084951	40.464141
3297.796669	488650.419347	40.469159
3301.527075	489565.760419	40.474176
3304.139265	490504.743396	40.479194
3307.640279	491435.672495	40.484212
3310.873531	492357.923115	40.489229
3314.132076	493301.013099	40.494247
3318.064657	494249.226370	40.499264
3320.822111	495195.598371	40.504282
3324.426418	496131.053436	40.509300
3327.957545	497082.572273	40.514317
3331.117397	498029.757823	40.519335
3335.035964	498982.402564	40.524352
3338.401451	499949.065515	40.529370
3341.968421	500892.076170	40.534388
3345.419212	501845.814783	40.539405
3349.093347	502798.298287	40.544423
3352.538584	503742.551516	40.549440
3355.325342	504711.452691	40.554458
3359.069430	505659.257172	40.559476
3362.604927	506605.169529	40.564493
3366.826847	507544.824436	40.569511
3370.399242	508486.832328	40.574528
3373.552018	509441.016587	40.579546
3377.688740	510384.570593	40.584564
3380.904812	511333.334842	40.589581
3383.513319	512287.359947	40.594599
3387.206718	513236.825849	40.599616
3390.260904	514198.294867	40.604634
3393.415731	515147.361690	40.609652
3396.896916	516112.804634	40.614669
3400.087799	517083.956565	40.619687
3403.060098	518046.979525	40.624704
3406.245158	519018.698756	40.629722
3409.882339	519999.778632	40.634740
3413.117934	520982.910757	40.639757
3416.683033	521969.237161	40.644775
3420.136182	522942.090384	40.649792
3423.525442	523938.451231	40.654810
3426.605189	524923.178579	40.659828
3430.182771	525915.543573	40.664845
3433.880589	526901.636013	40.669863
3437.375228	527884.421120	40.674880
3440.598651	528891.186701	40.679898
3443.962621	529888.460325	40.684916
3447.373786	530890.673185	40.689933
3450.431641	531898.287967	40.694951
3453.877905	532901.043722	40.699968
3456.951444	533908.851461	40.704986
3461.194771	534918.055422	40.710004
3464.330486	535933.176452	40.715021
3468.163638	536929.978154	40.720026
3471.344952	537893.730254	40.725031
3474.762333	538807.754143	40.730036
3477.973463	539666.744941	40.735040
3481.346216	540469.599770	40.740045
3484.470545	541224.090958	40.745050
3486.984339	541901.405033	40.750055
3489.819457	542552.170486	40.755060
3492.097466	543135.780353	40.760064
3495.032692	543658.041166	40.765069
3496.726472	544138.873749	40.770074
3499.247542	544564.631433	40.775079
3501.041984	544959.403165	40.780084
3503.061261	545288.489697	40.785088
3504.689318	545575.430076	40.790093
3505.835503	545824.365520	40.795098
3507.690864	546015.397644	40.800103
3509.214829	546185.103639	40.805108
3510.438502	546326.237353	40.810112
3511.803370	546433.701810	40.815117
3512.514185	546495.802951	40.820122
3513.515272	546536.735930	40.825127
3514.423218	546563.249464	40.830132
3515.305106	546549.382517	40.835136
3515.999328	546507.682882	40.840141
3516.401877	546458.534922	40.845146
3517.351809	546388.882755	40.850151
3517.331810	546291.217009	40.855156
3518.252620	546177.712503	40.860160
3518.537195	546068.681547	40.865165
3518.915507	545926.641827	40.870170
3519.382046	545772.214133	40.875175
3519.698849	545614.437997	40.880180
3519.915735	545413.017958	40.885184
3520.326328	545236.964726	40.890189
3520.019584	545034.714689	40.895194
3520.365232	544835.830477	40.900199
3520.517825	544629.478456	40.905204
3520.965406	544417.845842	40.910208
3520.829013	544193.423306	40.915213
3520.710546	543967.183053	40.920218
3520.698800	543739.563901	40.925223
3520.570634	543508.286501	40.930228
3520.563850	543275.979830	40.935232
3520.678475	543030.369100	40.940237
3520.733195	542790.246370	40.945242
3520.738630	542542.228318	40.950247
3520.482122	542304.961989	40.955252
3520.465026	542047.026742	40.960256
3520.713730	541801.169850	40.965261
3519.858850	541547.631178	40.970266
3520.334709	541284.672990	40.975271
3520.017801	541043.417510	40.980276
3520.427995	540792.232799	40.985280
3519.982576	540533.981010	40.990285
3519.817219	540281.970018	40.995290
3519.804083	540032.697821	41.000295
3519.353565	539779.412914	41.005300
3519.478341	539518.736973	41.010304
3519.226294	539272.556529	41.015309
3518.705425	539029.080218	41.020314
3518.610413	538763.793317	41.025319
3519.029887	538535.056896	41.030324
3518.738846	538282.220524	41.035328
3518.398534	538038.042902	41.040333
3518.205004	537797.008365	41.045338
3518.094242	537549.262755	41.050343
3517.945420	537317.422237	41.055348
3517.799201	537078.631572	41.060352
3517.768863	536833.225062	41.065357
3517.294212	536593.318828	41.070362
3517.298253	536363.802826	41.075367
3516.964158	536125.526934	41.080372
3516.995100	535905.914283	41.085376
3516.779666	535669.423497	41.090381
3516.433900	535449.257626	41.095386
3516.479850	535215.335295	41.100391
3516.335746	535008.973246	41.105396
3516.046193	534793.317823	41.110400
3516.146300	534563.654029	41.115405
3516.009107	534352.196058	41.120410
3516.156454	534120.553736	41.125415
3515.747592	533914.013989	41.130420
3515.455961	533686.811981	41.135424
3515.481520	533470.984733	41.140429
3515.239604	533266.523111	41.145434
3515.245145	533061.063183	41.150439
3514.806539	532853.806293	41.155444
3514.555659	532642.841523	41.160448
3514.255818	532435.556353	41.165453
3514.264588	532228.874385	41.170458
3514.415836	532037.422911	41.175463
3514.210201	531848.541674	41.180468
3513.676877	531657.946397	41.185472
3513.964119	531469.385767	41.190477
3513.476776	531274.094993	41.195482
3513.854336	531082.040376	41.200487
3513.144735	530904.553369	41.205492
3512.801998	530705.404667	41.210496
3513.509203	530528.598462	41.215501
3512.901637	530353.857640	41.220506
3512.936921	530169.194862	41.225511
3512.369964	529997.011151	41.230516
3512.328687	529828.469877	41.235520
3512.135798	529662.971556	41.240525
3512.025061	529493.731762	41.245530
3512.037987	529321.499294	41.250535
3512.026135	529150.829606	41.255540
3512.080061	528989.967939	41.260544
3512.272956	528821.679461	41.265549
3512.042053	528655.418923	41.270554
3512.214393	528481.992304	41.275559
3511.825789	528317.867300	41.280564
3511.641957	528148.218643	41.285568
3511.540080	527994.420095	41.290573
3511.034890	527842.697144	41.295578
3510.746407	527682.527541	41.300583
3511.013810	527531.889584	41.305588
3510.390216	527387.483030	41.310592
3510.595538	527226.626644	41.315597
3510.146799	527088.535995	41.320602
3510.008847	526937.954348	41.325607
3510.044872	526809.405868	41.330612
3510.403441	526657.937856	41.335616
3510.247882	526523.371977	41.340621
3510.158936	526381.238666	41.345626
3510.021961	526233.066678	41.350631
3509.812765	526112.407613	41.355636
3509.566374	525961.428765	41.360640
3509.811718	525833.090113	41.365645
3509.272449	525701.547639	41.370650
3509.908663	525561.106165	41.375655
3509.658382	525432.740025	41.380660
3509.346832	525303.878426	41.385664
3509.530841	525173.427186	41.390669
3509.268246	525042.641155	41.395674
3509.521235	524899.884651	41.400679
3508.942213	524776.298771	41.405684
3508.564167	524650.413463	41.410688
3508.925258	524534.034214	41.415693
3508.865355	524419.331585	41.420698
3508.996721	524293.817051	41.425703
3508.759038	524158.585099	41.430708
3508.855021	524053.225699	41.435712
3508.973537	523920.253393	41.440717
3508.284450	523816.979143	41.445722
3508.155164	523684.849154	41.450727
3508.273493	523581.044386	41.455732
3508.310757	523456.997719	41.460736
3508.124559	523340.088660	41.465741
3507.894051	523241.121910	41.470746
3508.140776	523127.468919	41.475751
3508.293395	523017.910718	41.480756
3507.975959	522913.916675	41.485760
3507.742144	522801.494543	41.490765
3507.672453	522695.898327	41.495770
3507.623813	522576.996186	41.500775
3507.750331	522483.863419	41.505780
3507.074974	522381.936393	41.510784
3507.646587	522276.438632	41.515789
3507.532788	522188.379897	41.520794
3507.528610	522078.284178	41.525799
3507.400611	521978.485970	41.530804
3507.484683	521880.367225	41.535808
3507.173003	521773.592105	41.540813
3506.788794	521683.606988	41.545818
3507.115054	521585.398018	41.550823
3506.816811	521493.634625	41.555828
3506.619229	521393.389405	41.560832
3507.036668	521307.409020	41.565837
3506.763522	521217.806634	41.570842
3507.008243	521116.885844	41.575847
3506.803712	521022.685889	41.580852
3506.717758	520936.529522	41.585856
3506.972350	520828.953322	41.590861
3506.641351	520755.583162	41.595866
3506.641142	520657.619823	41.600871
3506.644677	520573.110179	41.605876
3506.345736	520477.510109	41.610880
3506.623453	520389.126741	41.615885
3506.472165	520295.770134	41.620890
3506.593168	520221.520434	41.625895
3506.188247	520119.735804	41.630900
3506.163311	520039.813196	41.635904
3506.174517	519954.794550	41.640909
3506.122837	519880.368272	41.645914
3506.022881	519797.784936	41.650919
3505.983322	519715.695663	41.655924
3506.053119	519638.275767	41.660928
3506.286272	519554.379199	41.665933
3506.165463	519475.980099	41.670938
3506.011015	519384.583206	41.675943
3506.249956	519318.777010	41.680948
3505.835927	519233.467236	41.685952
3505.832978	519152.326427	41.690957
3505.698141	519074.935166	41.695962
3505.362365	519005.890572	41.700967
3505.564871	518930.058761	41.705972
3505.220978	518854.563551	41.710976
3506.080339	518782.610270	41.715981
3505.738970	518722.133076	41.720986
3505.744660	518636.804645	41.725991
3505.602601	518572.112538	41.730996
3505.763319	518487.363855	41.736000
3505.591723	518411.940183	41.741005
3505.598961	518335.732243	41.746010
3505.614101	518262.042735	41.751015
3505.438429	518184.299957	41.756020
3505.389883	518112.333220	41.761024
3505.906579	518045.973636	41.766029
3505.255879	517970.672481	41.771034
3505.617273	517899.044052	41.776039
3505.251631	517827.780401	41.781044
3505.090477	517762.885815	41.786048
3505.732307	517692.321543	41.791053
3505.368129	517629.474071	41.796058
3505.401614	517554.870621	41.801063
3505.289557	517475.551376	41.806068
3504.991116	517407.752998	41.811072
3505.490844	517343.912896	41.816077
3505.252964	517283.262005	41.821082
3505.056932	517204.357498	41.826087
3505.119665	517148.044521	41.831092
3505.225697	517074.939343	41.836096
3505.350460	516998.403225	41.841101
3505.226077	516932.390038	41.846106
3505.037242	516860.035292	41.851111
3505.374926	516800.048801	41.856116
3504.877356	516736.109027	41.861120
3505.110715	516668.375457	41.866125
3504.881224	516612.761055	41.871130
3505.164694	516543.406020	41.876135
3505.078430	516480.560436	41.881140
3504.613234	516414.698609	41.886144
3505.132555	516351.808609	41.891149
3505.063046	516291.227947	41.896154
3505.395634	516223.980836	41.901159
3505.061162	516153.207714	41.906164
3504.946615	516087.592211	41.911168
3504.963872	516020.141124	41.916173
3505.117759	515959.524237	41.921178
3504.851258	515881.076781	41.926183
3504.970220	515823.993468	41.931188
3504.680221	515763.747258	41.936192
3504.852226	515700.051342	41.941197
3504.620433	515642.064044	41.946202
3504.760617	515581.800507	41.951207
3505.127940	515520.997244	41.956212
3504.746262	515452.143511	41.961216
3504.651932	515385.362036	41.966221
3504.851413	515340.010256	41.971226
3504.674210	515281.912123	41.976231
3504.696631	515223.328964	41.981236
3504.525365	515160.339341	41.986240
3504.891648	515098.122808	41.991245
3504.522451	515049.682524	41.996250
3504.658625	514991.332747	42.001255
3504.718925	514929.415138	42.006260
3504.695981	514866.451507	42.011264
3504.919615	514804.205435	42.016269
3504.487146	514743.573621	42.021274
3504.565930	514682.206589	42.026279
3504.579213	514626.193479	42.031284
3504.139136	514575.544297	42.036288
3504.461956	514512.121924	42.041293
3504.687087	514467.822017	42.046298
3504.459757	514403.526859	42.051303
3504.935574	514351.726014	42.056308
3504.406655	514291.157639	42.061312
3504.669955	514224.617400	42.066317
3504.466199	514167.274959	42.071322
3504.132657	514107.734130	42.076327
3504.599825	514064.504443	42.081332
3504.642216	514008.736391	42.086336
3504.690398	513940.514074	42.091341
3504.316165	513888.188347	42.096346
3504.337231	513838.422643	42.101351
3504.375813	513784.166819	42.106356
3504.092524	513724.465268	42.111360
3504.443522	513671.874614	42.116365
3504.560026	513609.236496	42.121370
3504.189669	513548.287265	42.126375
3504.466952	513509.623111	42.131380
3503.877609	513459.093908	42.136384
3504.444569	513390.788160	42.141389
3504.454111	513346.619060	42.146394
3504.567196	513300.416910	42.151399
3504.155071	513229.640892	42.156404
3504.579364	513184.902536	42.161408
3504.314870	513117.279452	42.166413
3504.308611	513065.447987	42.171418
3504.560831	512996.634653	42.176423
3504.120442	512953.593160	42.181428
3504.029973	512904.396099	42.186432
3504.530879	512851.274802	42.191437
3504.308107	512790.954762	42.196442
3504.184692	512736.972168	42.201447
3504.427386	512681.974372	42.206452
3504.469574	512631.848106	42.211456
3504.621638	512581.855829	42.216461
3503.938944	512519.085053	42.221466
3504.169216	512469.735700	42.226471
3504.275277	512415.766574	42.231476
3503.989467	512366.345894	42.236480
3504.029327	512311.277353	42.241485
3504.050844	512268.464402	42.246490
3504.284575	512206.961475	42.251495
3504.330947	512151.084506	42.256500
3504.309828	512101.924244	42.261504
3504.322352	512046.556366	42.266509
3504.066737	512001.314922	42.271514
3504.218621	511945.571986	42.276519
3504.147773	511894.653863	42.281524
3503.969188	511844.559123	42.286528
3503.994963	511778.397125	42.291533
3503.801929	511739.750825	42.296538
3503.858426	511688.055749	42.301543
3503.955665	511649.111899	42.306548
3503.931124	511598.941881	42.311552
3504.014518	511541.443077	42.316557
3503.703033	511504.982890	42.321562
3503.887026	511452.208147	42.326567
3503.729676	511405.890525	42.331572
3503.796537	511362.260913	42.336576
3504.121519	511318.943988	42.341581
3504.056344	511276.746614	42.346586
3504.216962	511224.478924	42.351591
3504.014767	511165.762333	42.356596
3503.841740	511114.151281	42.361600
3503.797899	511066.806316	42.366605
3503.734598	511033.079817	42.371610
3503.757310	510977.403552	42.376615
3504.085681	510934.286624	42.381620
3503.705741	510894.255075	42.386624
3503.891818	510830.332938	42.391629
3503.672652	510788.107626	42.396634
3503.898008	510731.138125	42.401639
3503.748954	510688.296452	42.406644
3503.525217	510645.617558	42.411648
3503.604883	510601.681009	42.416653
3503.667095	510560.369389	42.421658
3503.465020	510520.611672	42.426663
3503.514879	510481.318940	42.431668
3503.536330	510439.509006	42.436672
3503.889677	510390.940057	42.441677
3503.739199	510346.584649	42.446682
3503.526284	510297.094881	42.451687
3503.954363	510250.884063	42.456692
3503.456087	510208.448285	42.461696
3503.824358	510152.714975	42.466701
3503.708290	510118.944058	42.471706
3503.554241	510071.259864	42.476711
3503.785944	510029.516856	42.481716
3503.790460	509991.036716	42.486720
3503.983806	509944.861422	42.491725
3503.928638	509899.228970	42.496730
3503.961507	509851.161918	42.501735
3503.718422	509808.786085	42.506740
3503.720538	509754.167259	42.511744
3503.668274	509708.836334	42.516749
3503.590265	509666.131786	42.521754
3503.936707	509608.684998	42.526759
3503.945164	509565.815391	42.531764
3503.707898	509528.380279	42.536768
3503.910552	509478.419493	42.541773
3503.570595	509440.445356	42.546778
3503.786775	509390.482154	42.551783
3503.784538	509334.097186	42.556788
3503.405452	509291.488788	42.561792
3503.762078	509245.084055	42.566797
3503.730970	509215.029903	42.571802
3503.680858	509166.267342	42.576807
3503.936818	509116.145674	42.581812
3503.243127	509076.258635	42.586816
3503.725690	509017.930863	42.591821
3503.327026	508987.429068	42.596826
3503.376267	508947.627797	42.601831
3503.714084	508898.703074	42.606836
3503.641391	508861.946682	42.611840
3503.772318	508809.725076	42.616845
3503.495743	508781.977823	42.621850
3503.326717	508729.348670	42.626855
3503.497385	508690.133015	42.631860
3503.421152	508653.477504	42.636864
3503.746472	508599.005657	42.641869
3503.658302	508559.174239	42.646874
3503.721987	508515.788479	42.651879
3503.485591	508474.870272	42.656884
3503.393467	508437.712302	42.661888
3503.232930	508396.025500	42.666893
3503.028227	508345.821474	42.671898
3502.961870	508308.608717	42.676903
3503.424579	508269.043823	42.681908
3503.183296	508241.390891	42.686912
3503.420268	508200.448666	42.691917
3503.569132	508159.469595	42.696922
3503.535400	508119.830221	42.701927
3503.219275	508074.333354	42.706932
3503.055937	508032.141529	42.711936
3503.755521	507990.874516	42.716941
3503.453176	507950.973836	42.721946
3503.457229	507909.058231	42.726951
3503.800746	507874.907790	42.731956
3503.244034	507835.046365	42.736960
3503.563139	507788.642697	42.741965
3503.510089	507752.737842	42.746970
3503.245039	507713.284647	42.751975
3503.377748	507667.968829	42.756980
3503.489080	507628.759470	42.761984
3503.854075	507579.573762	42.766989
3503.634616	507552.773576	42.771994
3503.480484	507509.620393	42.776999
3503.511302	507461.293328	42.782004
3503.485828	507420.843661	42.787009
3503.419413	507368.042158	42.792013
3503.082515	507330.061872	42.797018
3503.275389	507288.316816	42.802023
3503.493049	507245.861598	42.807028
3503.294212	507220.570825	42.812033
3503.119358	507176.108367	42.817037
3503.040002	507143.081251	42.822042
3503.115326	507100.849517	42.827047
3503.453202	507061.401570	42.832052
3503.384420	507034.274305	42.837057
3503.479657	506988.861268	42.842061
3503.361350	506942.119362	42.847066
3503.497641	506898.364258	42.852071
3503.584353	506870.001853	42.857076
3503.515003	506824.815677	42.862081
3503.431928	506777.411987	42.867085
3503.671436	506744.485656	42.872090
3503.626706	506697.176619	42.877095
3503.620894	506662.774966	42.882100
3503.411047	506608.025654	42.887105
3503.398568	506562.527131	42.892109
3503.060585	506529.337060	42.897114
3503.111692	506497.145693	42.902119
3503.260450	506446.779057	42.907124
3503.417618	506410.131874	42.912129
3503.407527	506367.709479	42.917133
3502.908967	506335.451948	42.922138
3503.027144	506298.255652	42.927143
3503.378302	506251.438425	42.932148
3503.208672	506220.087906	42.937153
3503.361370	506174.057987	42.942157
3503.282663	506138.859285	42.947162
3503.250518	506101.282303	42.952167
3503.513527	506061.490122	42.957172
3503.562890	506029.297971	42.962177
3503.620140	505980.457307	42.967181
3503.329377	505940.952748	42.972186
3503.073610	505903.006472	42.977191
3503.428268	505863.149030	42.982196
3503.281396	505822.057907	42.987201
3503.497272	505777.933854	42.992205
3503.459969	505746.309467	42.997210
3503.366755	505704.352058	43.002215
3503.435727	505663.479126	43.007220
3503.201537	505636.475834	43.012225
3503.332533	505579.752536	43.017229
3503.398165	505547.304530	43.022234
3503.432763	505505.377094	43.027239
3503.606747	505460.400968	43.032244
3503.300401	505431.995974	43.037249
3503.631337	505379.377510	43.042253
3503.758677	505350.904867	43.047258
3503.284008	505300.530306	43.052263
3503.419267	505258.838727	43.057268
3503.159669	505211.104162	43.062273
3503.302621	505177.583860	43.067277
3503.164059	505141.685730	43.072282
3503.072538	505102.450542	43.077287
3503.354385	505077.333411	43.082292
3503.201189	505034.929327	43.087297
3503.188115	504991.494321	43.092301
3503.040570	504952.620588	43.097306
3503.040933	504913.723732	43.102311
3503.050738	504871.646950	43.107316
3502.829265	504848.877993	43.112321
3503.254185	504816.826474	43.117325
3503.312011	504780.795979	43.122330
3502.940115	504734.288108	43.127335
3503.290042	504693.419138	43.132340
3503.331122	504655.978317	43.137345
3503.331776	504612.136419	43.142349
3502.979090	504584.796423	43.147354
3503.060230	504544.019306	43.152359
3503.221331	504510.847781	43.157364
3503.017546	504479.751016	43.162369
3503.081922	504438.471694	43.167373
3503.292518	504412.759069	43.172378
3503.120824	504376.813728	43.177383
3503.259304	504336.531617	43.182388
3502.772243	504303.964995	43.187393
3503.182400	504253.449059	43.192397
3503.098685	504235.248842	43.197402
3502.804185	504187.516299	43.202407
3503.080450	504149.129414	43.207412
3502.672336	504116.600534	43.212417
3503.271467	504084.268010	43.217421
3503.075031	504054.178236	43.222426
3502.783844	504015.526127	43.227431
3502.809732	503984.039377	43.232436
3502.935363	503953.747916	43.237441
3503.019543	503911.253119	43.242445
3503.167492	503882.572545	43.247450
3503.576615	503848.957269	43.252455
3503.612377	503810.808723	43.257460
3503.225184	503781.807592	43.262465
3503.440536	503736.113272	43.267469
3503.211077	503697.904790	43.272474
3503.152091	503648.569729	43.277479
3503.019472	503619.982745	43.282484
3503.157027	503582.423207	43.287489
3502.909508	503548.051683	43.292493
3502.836511	503519.757951	43.297498
3503.049010	503473.659605	43.302503
3502.982830	503435.223197	43.307508
3502.950544	503413.633446	43.312513
3503.278060	503374.832883	43.317517
3503.062658	503341.666796	43.322522
3502.955362	503306.061945	43.327527
3503.060819	503257.658610	43.332532
3502.833236	503231.406596	43.337537
3503.026969	503196.662835	43.342541
3503.184042	503157.585475	43.347546
3503.180068	503112.528782	43.352551
3503.238292	503089.663056	43.357556
3503.463898	503057.487271	43.362561
3502.871174	503015.498820	43.367565
3502.944633	502979.612752	43.372570
3503.010798	502946.099200	43.377575
3503.131659	502913.132085	43.382580
3503.050743	502891.952775	43.387585
3502.923018	502847.469539	43.392589
3502.980572	502809.365409	43.397594
3502.924932	502769.916443	43.402599
3503.591656	502730.657706	43.407604
3503.008109	502705.216989	43.412609
3502.898233	502659.065292	43.417613
3502.536550	502623.548800	43.422618
3502.594719	502597.301623	43.427623
3502.791879	502567.046577	43.432628
3502.595154	502535.793140	43.437633
3502.989873	502507.424640	43.442637
3503.088875	502469.313164	43.447642
3503.163565	502436.200771	43.452647
3503.056618	502411.240414	43.457652
3502.817229	502378.933644	43.462657
3503.208363	502345.519507	43.467661
3502.980784	502301.807013	43.472666
3502.587225	502260.239502	43.477671
3502.956379	502231.521226	43.482676
3502.511343	502205.654398	43.487681
3502.946662	502177.228476	43.492685
3502.845209	502140.408814	43.497690
3503.006666	502112.630896	43.502695
3503.194758	502060.375757	43.507700
3503.239238	502038.822466	43.512705
3503.048153	501991.924379	43.517709
3502.636786	501974.630117	43.522714
3502.853280	501936.246654	43.527719
3502.888457	501898.395909	43.532724
3502.856258	501868.780623	43.537729
3502.908849	501841.473272	43.542733
3503.041369	501806.130171	43.547738
3503.224557	501771.536013	43.552743
3503.374568	501731.749450	43.557748
3503.026492	501705.664796	43.562753
3502.835839	501670.119347	43.567757
3502.992399	501639.919147	43.572762
3502.972289	501598.342083	43.577767
3502.873743	501565.305119	43.582772
3502.782204	501538.322395	43.587777
3502.730659	501500.282260	43.592781
3502.809862	501475.594094	43.597786
3502.872253	501441.774877	43.602791
3503.127147	501412.971840	43.607796
3502.539391	501381.120751	43.612801
3502.912925	501345.385788	43.617805
3502.731165	501311.251023	43.622810
3503.034133	501270.934771	43.627815
3502.834673	501234.683150	43.632820
3502.915520	501210.196128	43.637825
3503.274759	501159.424999	43.642829
3503.176410	501137.337502	43.647834
3502.820152	501105.803026	43.652839
3502.903576	501067.437975	43.657844
3503.240629	501045.333048	43.662849
3502.954996	500998.194144	43.667853
3502.811062	500969.553219	43.672858
3502.471395	500936.249564	43.677863
3502.530845	500906.567589	43.682868
3502.388513	500879.086906	43.687873
3502.742594	500846.482513	43.692877
3502.171045	500818.866651	43.697882
3502.461901	500802.773783	43.702887
3502.546006	500769.151479	43.707892
3502.235765	500749.417726	43.712897
3502.365446	500724.114857	43.717901
3502.273198	500695.061632	43.722906
3502.226747	500670.391653	43.727911
3502.683067	500648.822677	43.732916
3502.628518	500625.516431	43.737921
3502.886661	500595.449650	43.742925
3502.678137	500567.726354	43.747930
3502.109286	500537.333957	43.752935
3502.744895	500512.305247	43.757940
3502.463554	500483.634283	43.762945
3502.997887	500449.133734	43.767949
3502.806154	500434.074401	43.772954
3502.727643	500396.742093	43.777959
3502.649628	500372.379315	43.782964
3502.655394	500331.400191	43.787969
3502.829177	500304.272959	43.792973
3502.455719	500274.858927	43.797978
3502.658369	500250.199940	43.802983
3502.707803	500219.609734	43.807988
3502.435271	500191.643351	43.812993
3502.324919	500167.386195	43.817997
3502.878407	500139.947239	43.823002
3502.342802	500113.737506	43.828007
3502.500830	500077.982506	43.833012
3502.274548	500068.328114	43.838017
3502.452064	500027.624211	43.843021
3502.686695	500012.296226	43.848026
3502.617697	499976.879109	43.853031
3502.597280	499941.151543	43.858036
3502.996939	499920.347319	43.863041
3502.854074	499890.442423	43.868045
3502.793460	499860.070458	43.873050
3502.552003	499828.414413	43.878055
3502.546189	499795.762744	43.883060
3502.741581	499765.552616	43.888065
3502.487449	499731.324473	43.893069
3502.749796	499700.700048	43.898074
3502.548299	499678.121709	43.903079
3502.764160	499643.618351	43.908084
3502.545586	499616.803239	43.913089
3502.361132	499585.440607	43.918093
3502.602657	499565.922200	43.923098
3502.348159	499542.897682	43.928103
3502.670986	499516.957042	43.933108
3502.454175	499489.232985	43.938113
3502.571596	499458.782013	43.943117
3502.633041	499431.216422	43.948122
3502.333414	499412.942807	43.953127
3502.185020	499396.714869	43.958132
3502.352961	499364.691297	43.963137
3502.526809	499339.177279	43.968141
3502.431451	499315.471538	43.973146
3502.628419	499286.471442	43.978151
3502.652555	499256.741139	43.983156
3502.541307	499232.533040	43.988161
3502.556163	499210.021249	43.993165
3502.317995	499184.873896	43.998170
3502.598267	499152.428622	44.003175
3502.685129	499122.890166	44.008180
3502.589093	499091.815537	44.013185
3502.784749	499065.439657	44.018189
3502.584550	499038.519684	44.023194
3502.514364	499008.096970	44.028199
3502.749174	498971.469321	44.033204
3502.550472	498948.536126	44.038209
3502.746045	498915.346447	44.043213
3502.886601	498889.231178	44.048218
3502.815673	498874.252378	44.053223
3502.696918	498842.373221	44.058228
3502.543449	498805.755108	44.063233
3502.658834	498780.249216	44.068237
3503.062510	498754.900303	44.073242
3502.937256	498719.438425	44.078247
3503.202243	498679.171407	44.083252
3502.751834	498648.352869	44.088257
3502.803166	498623.563275	44.093261
3502.739881	498583.700381	44.098266
3502.287428	498556.970193	44.103271
3502.797949	498522.973538	44.108276
3502.567246	498500.347453	44.113281
3502.686190	498467.723882	44.118285
3502.729982	498440.562954	44.123290
3502.220872	498405.866665	44.128295
3502.457818	498385.035114	44.133300
3502.710935	498355.418770	44.138305
3502.674647	498324.383690	44.143309
3502.618773	498295.875238	44.148314
3502.705478	498277.994343	44.153319
3502.573050	498243.794257	44.158324
3502.286192	498214.816860	44.163329
3502.175775	498191.565904	44.168333
3502.655293	498169.838256	44.173338
3502.606195	498144.356855	44.178343
3502.234558	498111.304099	44.183348
3502.282880	498085.555069	44.188353
3502.537418	498060.076747	44.193357
3502.395911	498032.691531	44.198362
3502.271453	498000.003851	44.203367
3502.263486	497985.620034	44.208372
3502.511360	497955.145643	44.213377
3502.456168	497931.380940	44.218381
3502.621839	497903.897210	44.223386
3502.739590	497885.001522	44.228391
3502.729992	497853.809873	44.233396
3502.925685	497825.614683	44.238401
3502.985264	497789.566579	44.243405
3502.583440	497761.918520	44.248410
3502.720135	497737.416997	44.253415
3502.628053	497700.180878	44.258420
3502.886565	497671.117544	44.263425
3502.745870	497633.384070	44.268429
3502.813198	497612.375921	44.273434
3502.416066	497571.855581	44.278439
3502.823351	497545.393567	44.283444
3502.863106	497520.200113	44.288449
3502.669248	497496.304859	44.293453
3502.706371	497463.287989	44.298458
3502.176465	497439.646840	44.303463
3502.502754	497410.269589	44.308468
3502.624229	497391.776497	44.313473
3502.443446	497360.055205	44.318477
3502.710406	497337.652744	44.323482
3502.330359	497302.227097	44.328487
3502.895060	497277.658208	44.333492
3502.621310	497253.875947	44.338497
3502.407088	497219.231919	44.343501
3502.805975	497192.114384	44.348506
3502.479880	497166.573443	44.353511
3502.429059	497131.449491	44.358516
3502.583059	497110.730002	44.363521
3502.485861	497090.705775	44.368525
3502.531457	497058.191450	44.373530
3502.074569	497037.718352	44.378535
3502.455243	496996.419188	44.383540
3502.149706	496976.881523	44.388545
3502.231039	496961.018964	44.393549
3502.727962	496930.655136	44.398554
3502.541991	496907.565342	44.403559
3502.265195	496866.317647	44.408564
3502.486536	496851.392262	44.413569
3502.712899	496832.528804	44.418573
3502.771938	496799.305127	44.423578
3502.782952	496771.389053	44.428583
3502.598304	496743.907199	44.433588
3502.744163	496713.294686	44.438593
3502.023688	496697.354702	44.443597
3502.387210	496664.184297	44.448602
3502.009338	496652.330187	44.453607
3502.292164	496612.155705	44.458612
3502.508885	496606.468385	44.463617
3502.348309	496578.831043	44.468621
3502.303118	496550.771862	44.473626
3501.982178	496518.414345	44.478631
3502.418419	496502.092234	44.483636
3502.327211	496483.176791	44.488641
3502.260857	496450.325196	44.493645
3502.587821	496430.940780	44.498650
3502.206798	496404.447959	44.503655
3502.497499	496372.954054	44.508660
3502.447872	496354.637729	44.513665
3502.209842	496323.983189	44.518669
3502.387395	496290.184651	44.523674
3502.076807	496277.259694	44.528679
3502.326824	496245.115610	44.533684
3502.025513	496233.703568	44.538689
3502.058995	496219.311579	44.543693
3502.590118	496193.837481	44.548698
3502.467955	496171.392848	44.553703
3502.560971	496146.996448	44.558708
3502.490601	496118.687965	44.563713
3502.053409	496090.234588	44.568717
3502.615058	496063.039180	44.573722
3502.250857	496043.913253	44.578727
3502.302058	496012.405370	44.583732
3502.078747	495998.557935	44.588737
3502.690022	495973.323390	44.593741
3502.489694	495945.792012	44.598746
3502.138048	495924.240891	44.603751
3502.342276	495900.785919	44.608756
3502.456443	495876.840112	44.613761
3502.313497	495854.953527	44.618765
3502.521313	495815.596260	44.623770
3502.575441	495802.664614	44.628775
3502.378749	495761.754745	44.633780
3502.507379	495739.421876	44.638785
3502.776017	495718.026340	44.643789
3502.783264	495684.555814	44.648794
3502.575620	495656.823111	44.653799
3502.486397	495623.468423	44.658804
3502.813461	495603.880984	44.663809
3502.597384	495577.310533	44.668813
3502.661354	495535.097421	44.673818
3502.422189	495512.821446	44.678823
3502.556394	495481.955792	44.683828
3502.121240	495460.770369	44.688833
3502.540585	495443.339110	44.693837
3502.358947	495419.438597	44.698842
3502.074653	495401.914853	44.703847
3502.259226	495375.887489	44.708852
3502.247449	495356.907764	44.713857
3502.355325	495326.348782	44.718861
3502.292852	495303.186785	44.723866
3501.917021	495280.275446	44.728871
3502.093128	495254.602569	44.733876
3501.840792	495231.621454	44.738881
3502.116293	495220.926606	44.743885
3502.494675	495187.700108	44.748890
3502.106575	495177.108492	44.753895
3502.355500	495146.274774	44.758900
3502.222964	495126.253389	44.763905
3501.939991	495106.962161	44.768909
3502.165979	495092.337189	44.773914
3502.311264	495063.740716	44.778919
3502.444107	495035.600481	44.783924
3502.292176	495007.252087	44.788929
3502.397095	494985.224680	44.793933
3502.659023	494962.415545	44.798938
3502.241527	494938.197570	44.803943
3502.049548	494911.420240	44.808948
3502.418673	494885.363300	44.813953
3502.627707	494868.872818	44.818957
3502.392611	494835.841970	44.823962
3502.183433	494808.562284	44.828967
3502.296902	494786.886648	44.833972
3502.346286	494765.119982	44.838977
3502.220252	494733.838909	44.843981
3502.595730	494712.526274	44.848986
3502.398306	494697.512436	44.853991
3502.797572	494663.524243	44.858996
3502.619719	494656.483994	44.864001
3502.156572	494632.827964	44.869005
3502.327575	494585.950847	44.874010
3502.532535	494573.247089	44.879015
3502.700977	494539.345018	44.884020
3502.479885	494523.678374	44.889025
3502.653938	494491.643295	44.894029
3502.536962	494463.187453	44.899034
3502.142155	494438.965134	44.904039
3502.128448	494403.778463	44.909044
3502.247277	494387.957807	44.914049
3502.423619	494368.796091	44.919053
3502.593160	494346.656713	44.924058
3502.400060	494317.758062	44.929063
3502.225393	494295.621685	44.934068
3502.497639	494273.112810	44.939073
3502.442059	494242.274121	44.944077
3502.316598	494221.190198	44.949082
3502.153931	494191.630238	44.954087
3502.380930	494162.766888	44.959092
3502.245407	494138.251297	44.964097
3502.405799	494123.938507	44.969101
3502.660564	494082.297434	44.974106
3502.076233	494068.049991	44.979111
3502.230620	494035.209196	44.984116
3502.227505	494020.719802	44.989121
3502.118715	493988.980096	44.994125
3502.331058	493981.575881	44.999130
3502.116757	493958.435419	45.004135
3502.705813	493934.008690	45.009140
3502.594812	493911.054031	45.014145
3502.260805	493877.784012	45.019149
3502.699040	493863.579201	45.024154
3502.244249	493835.427170	45.029159
3502.201423	493804.383641	45.034164
3502.271090	493780.441391	45.039169
3502.459088	493765.013219	45.044173
3502.637966	493732.925275	45.049178
3502.066621	493709.284614	45.054183
3501.899440	493680.027275	45.059188
3502.142314	493662.167005	45.064193
3501.949773	493641.749054	45.069197
3502.149125	493630.661009	45.074202
3502.017814	493606.446822	45.079207
3502.373921	493588.972755	45.084212
3502.275887	493563.642565	45.089217
3501.757975	493543.073155	45.094221
3502.184200	493519.731361	45.099226
3501.889542	493505.488791	45.104231
3502.014834	493482.850128	45.109236
3502.089699	493466.833383	45.114241
3502.095891	493445.071516	45.119245
3502.208539	493417.183822	45.124250
3502.046329	493402.415648	45.129255
3502.243683	493370.021113	45.134260
3502.151690	493361.401710	45.139265
3501.954543	493336.238027	45.144269
3502.276165	493319.677829	45.149274
3502.298420	493300.690193	45.154279
3502.187009	493277.684135	45.159284
3502.107714	493249.775508	45.164289
3502.478619	493234.116368	45.169293
3502.421989	493209.738448	45.174298
3502.022271	493199.702621	45.179303
3502.416273	493168.387836	45.184308
3502.575939	493146.803614	45.189313
3502.543662	493119.089389	45.194317
3502.868202	493082.736182	45.199322
3502.818258	493053.711829	45.204327
3502.631333	493020.316033	45.209332
3502.565427	492988.315077	45.214337
3502.390274	492972.387201	45.219341
3502.479432	492937.383036	45.224346
3502.654132	492921.501647	45.229351
3502.551749	492882.184919	45.234356
3502.592442	492855.115238	45.239361
3502.384131	492833.082913	45.244365
3502.876767	492802.559880	45.249370
3502.530968	492773.682007	45.254375
3502.817553	492740.817804	45.259380
3502.637568	492717.973034	45.264385
3502.467634	492690.733865	45.269389
3502.755857	492651.103288	45.274394
3502.477639	492629.283511	45.279399
3502.476561	492594.141112	45.284404
3503.104309	492571.725841	45.289409
3502.608442	492554.181179	45.294413
3503.049830	492530.179089	45.299418
3502.549878	492490.266798	45.304423
3502.438230	492463.371595	45.309428
3502.594735	492435.020818	45.314433
3502.478244	492409.085635	45.319437
3502.534515	492378.781126	45.324442
3502.400047	492351.283357	45.329447
3502.260707	492327.421806	45.334452
3502.694869	492298.674112	45.339457
3502.441500	492283.868528	45.344461
3502.492108	492242.203624	45.349466
3502.327647	492218.850743	45.354471
3502.350679	492197.437901	45.359476
3502.328971	492172.143977	45.364481
3502.113327	492150.818703	45.369485
3502.397208	492119.872328	45.374490
3502.468530	492100.471589	45.379495
3502.313196	492072.825076	45.384500
3502.545327	492046.784524	45.389505
3502.370825	492016.464702	45.394509
3502.528477	491990.183172	45.399514
3502.293028	491960.478653	45.404519
3502.539505	491940.646496	45.409524
3502.553742	491920.244517	45.414529
3502.295462	491891.704790	45.419533
3502.460519	491867.189204	45.424538
3502.457286	491853.808619	45.429543
3502.449061	491823.361544	45.434548
3502.527092	491795.779198	45.439553
3502.546162	491770.074293	45.444557
3502.522758	491741.194760	45.449562
3501.986755	491723.655372	45.454567
3502.179207	491703.679825	45.459572
3502.190383	491666.715524	45.464577
3501.983832	491652.507976	45.469581
3502.452078	491621.026935	45.474586
3502.213808	491603.946031	45.479591
3502.063130	491577.459283	45.484596
3502.185382	491562.645033	45.489601
3502.045848	491540.044656	45.494605
3502.397250	491521.508512	45.499610
3502.100381	491500.346443	45.504615
3502.115861	491468.733556	45.509620
3502.587401	491450.734087	45.514625
3502.488657	491435.550133	45.519629
3502.534726	491394.237064	45.524634
3502.183268	491369.700054	45.529639
3502.316460	491355.691841	45.534644
3502.274668	491319.088405	45.539649
3502.182871	491309.205380	45.544653
3502.471753	491277.852528	45.549658
3501.980765	491260.154104	45.554663
3502.259272	491231.226614	45.559668
3502.486365	491207.407259	45.564673
3502.160537	491184.835340	45.569677
3502.365904	491168.694848	45.574682
3502.108717	491144.950755	45.579687
3502.017708	491140.470688	45.584692
3502.349352	491100.374805	45.589697
3501.940056	491089.430102	45.594701
3502.375555	491048.408969	45.599706
3501.622642	491037.164216	45.604711
3501.660125	491019.130784	45.609716
3502.448320	490993.405867	45.614721
3502.191535	490981.073916	45.619725
3502.263107	490957.682351	45.624730
3501.844101	490954.818700	45.629735
3501.998549	490916.618321	45.634740
3502.204612	490900.830921	45.639745
3501.850750	490880.232328	45.644749
3502.413219	490853.128354	45.649754
3502.019372	490835.717302	45.654759
3502.460697	490813.580929	45.659764
3502.552804	490787.509498	45.664769
3501.984616	490766.287623	45.669773
3502.388678	490734.915724	45.674778
3502.225996	490728.073258	45.679783
3502.027075	490686.392390	45.684788
3501.863452	490664.854923	45.689793
3501.906655	490658.939864	45.694797
3502.143739	490636.077533	45.699802
3502.151499	490626.885552	45.704807
3501.824301	490590.476262	45.709812
3501.914332	490577.282028	45.714817
3501.733880	490565.846842	45.719821
3502.162846	490532.652682	45.724826
3502.109200	490511.905870	45.729831
3501.866320	490451.697961	45.734836
3501.700928	490335.978538	45.739841
3501.372481	490174.681839	45.744845
3501.162530	489957.005865	45.749850
3500.738581	489709.260956	45.754855
3500.636276	489416.766960	45.759860
3500.391501	489068.937177	45.764865
3499.647073	488675.166897	45.769869
3499.138364	488235.742192	45.774874
3498.390381	487761.844904	45.779879
3497.919902	487223.287423	45.784884
3497.417719	486656.530294	45.789889
3496.161302	486037.385645	45.794893
3495.342922	485376.270076	45.799898
3494.231710	484668.290682	45.804903
3493.623723	483918.824025	45.809908
3492.419531	483132.481374	45.814913
3491.628525	482315.466477	45.819917
3490.573059	481428.012790	45.824922
3488.956093	480511.085684	45.829927
3487.620346	479547.367152	45.834932
3486.726483	478547.032595	45.839937
3485.099077	477513.240218	45.844941
3483.758909	476433.694150	45.849946
3481.809112	475326.773011	45.854951
3480.407485	474174.800324	45.859956
3478.852383	472980.858834	45.864961
3476.835514	471756.110786	45.869965
3475.299329	470499.998537	45.874970
3473.443518	469219.314836	45.879975
3471.859530	467891.407629	45.884980
3470.304129	466522.069645	45.889985
3468.121557	465117.817017	45.894989
3466.169652	463692.823470	45.899994
3464.061499	462234.952916	45.904999
3461.894218	460725.311439	45.910004
3460.115446	459201.106835	45.915009
3457.785745	457657.067957	45.920013
3455.361337	456066.146198	45.925018
3453.394521	454474.249346	45.930023
3450.758125	452843.439988	45.935028
3448.608800	451177.983065	45.940033
3445.806657	449500.322563	45.945037
3443.518520	447791.693484	45.950042
3441.064812	446068.903597	45.955047
3438.779875	444313.060252	45.960052
3436.222178	442540.278384	45.965057
3433.426600	440750.599780	45.970061
3431.065509	438922.337745	45.975066
3428.447896	437081.325021	45.980071
3425.730755	435213.602464	45.985076
3423.054518	433320.003466	45.990081
3420.204677	431415.301679	45.995085
3417.227210	429486.920113	46.000090
3414.618190	427544.710492	46.005095
3411.792591	425587.545174	46.010100
3409.006124	423606.307749	46.015105
3406.101164	421603.197740	46.020109
3403.483271	419594.626331	46.025114
3400.317500	417563.178842	46.030119
3397.454390	415508.160539	46.035124
3394.137874	413444.544889	46.040129
3391.031193	411369.489372	46.045133
3388.098821	409274.679140	46.050138
3384.863092	407169.418563	46.055143
3381.820204	405051.803258	46.060148
3378.785009	402930.284167	46.065153
3374.978194	400790.673258	46.070157
3372.278090	398639.222596	46.075162
3368.982207	396476.348669	46.080167
3365.953840	394299.073916	46.085172
3362.661831	392115.703682	46.090177
3359.293595	389922.808179	46.095181
3355.883924	387705.733655	46.100186
3352.396234	385485.352251	46.105191
3349.192685	383263.488475	46.110196
3345.602388	381027.272841	46.115201
3342.337589	378794.015281	46.120205
3339.307337	376538.995705	46.125210
3335.625704	374287.267036	46.130215
3332.101143	372017.953399	46.135220
3328.680628	369745.567569	46.140225
3324.943262	367474.293081	46.145229
3321.765269	365175.691746	46.150234
3318.417197	362890.581176	46.155239
3314.727609	360579.249192	46.160244
3311.209866	358280.013969	46.165249
3307.122097	355981.101945	46.170253
3304.038092	353659.267945	46.175258
3300.298824	351344.407855	46.180263
3296.550589	349018.935539	46.185268
3293.216770	346692.701141	46.190273
3289.317685	344372.190977	46.195277
3285.908708	342045.904667	46.200282
3282.066037	339715.818803	46.205287
3278.213221	337371.392589	46.210292
3274.762696	335040.791621	46.215297
3271.071527	332706.343752	46.220301
3267.591248	330364.191335	46.225306
3263.651308	328024.971207	46.230311
3259.925996	325687.997040	46.235316
3256.530732	323338.474136	46.240321
3252.536591	321003.769794	46.245325
3249.028577	318649.272042	46.250330
3245.405885	316290.849383	46.255335
3241.201018	313951.401206	46.260340
3237.590718	311595.634822	46.265345
3233.464503	309248.331417	46.270349
3229.935191	306899.142810	46.275354
3225.977152	304556.553605	46.280359
3222.060712	302217.236967	46.285364
3218.186568	299868.470395	46.290369
3214.324845	297535.153564	46.295373
3210.764420	295190.010742	46.300378
3206.609875	292864.441813	46.305383
3202.841142	290535.694721	46.310388
3199.097572	288201.257191	46.315393
3195.035379	285883.308068	46.320397
3191.127392	283560.265976	46.325402
3187.320677	281244.795084	46.330407
3183.182436	278929.863104	46.335412
3179.760120	276609.785085	46.340417
3175.519462	274310.315056	46.345421
3171.645872	272001.482232	46.350426
3167.652784	269701.112354	46.355431
3163.609647	267411.388115	46.360436
3160.184732	265125.410275	46.365441
3156.101040	262837.141868	46.370445
3152.282757	260556.398792	46.375450
3147.948256	258279.155117	46.380455
3143.987704	255998.705118	46.385460
3140.262786	253734.784234	46.390465
3136.143792	251465.210461	46.395469
3132.302302	249200.680059	46.400474
3128.510717	246949.737697	46.405479
3124.272109	244710.299220	46.410484
3120.334211	242476.470113	46.415489
3116.555631	240252.426622	46.420493
3112.288433	238011.708765	46.425498
3108.262803	235801.704531	46.430503
3104.302431	233585.896711	46.435508
3100.401279	231377.227059	46.440513
3095.989088	229191.603300	46.445517
3092.323058	226999.721371	46.450522
3088.001498	224823.960038	46.455527
3083.819210	222658.009164	46.460532
3080.094975	220486.591143	46.465537
3075.786125	218346.214887	46.470541
3071.600736	216199.384119	46.475546
3067.508283	214076.668470	46.480551
3063.365362	211948.956257	46.485556
3059.272605	209829.070289	46.490561
3054.779566	207743.314911	46.495565
3051.114904	205652.738248	46.500570
3046.408443	203578.389744	46.505575
3042.560363	201514.856451	46.510580
3038.227561	199460.337259	46.515585
3034.049327	197412.799004	46.520589
3029.904447	195391.896803	46.525594
3025.762497	193369.725727	46.530599
3021.357015	191369.350032	46.535604
3016.895940	189381.239830	46.540609
3012.542094	187409.496320	46.545613
3008.671862	185459.103798	46.550618
3003.858190	183515.770746	46.555623
2999.915127	181594.061184	46.560628
2995.480310	179674.785139	46.565633
2990.888750	177787.402403	46.570637
2986.864005	175899.273095	46.575642
2982.495223	174042.684836	46.580647
2977.824883	172195.352784	46.585652
2973.391258	170375.028454	46.590657
2968.887908	168568.291294	46.595661
2964.170149	166774.005905	46.600666
2959.523775	165015.536519	46.605671
2954.822172	163266.044365	46.610676
2950.025517	161554.734536	46.615681
2945.176984	159870.067144	46.620685
2940.627959	158200.671853	46.625690
2935.083383	156565.038899	46.630695
2929.682928	154965.903667	46.635700
2924.967415	153412.088466	46.640705
2919.045552	151803.361928	46.645709
2913.469143	150302.389381	46.650714
2907.608960	148854.567231	46.655719
2901.627358	147453.465990	46.660724
2896.014118	146096.843195	46.665729
2889.899290	144800.393183	46.670733
2883.733237	143534.649353	46.675738
2878.290595	142320.483409	46.680743
2872.442377	141155.357585	46.685748
2867.250557	140025.311656	46.690753
2861.423118	138950.608396	46.695757
2856.706984	137901.697987	46.700762
2851.310032	136897.699477	46.705767
2846.931513	135915.573444	46.710772
2842.248692	134963.348383	46.715777
2837.503913	134051.836286	46.720781
2833.090297	133162.311703	46.725786
2828.936709	132300.534407	46.730791
2824.551337	131461.847361	46.735796
2820.811716	130637.335711	46.740801
2816.449293	129834.841025	46.745805
2812.057011	129055.770877	46.750810
2808.461439	128286.105514	46.755815
2804.230393	127538.659704	46.760820
2800.584612	126795.855139	46.765825
2796.636157	126071.935270	46.770829
2793.430304	125362.933599	46.775834
2789.526801	124638.930465	46.780839
2785.460539	123946.888800	46.785844
2782.221348	123247.608233	46.790849
2778.594397	122570.567681	46.795853
2774.582716	121896.714460	46.800858
2771.126497	121233.036692	46.805863
2767.354455	120572.039143	46.810868
2763.950807	119921.665179	46.815873
2760.153549	119272.291795	46.820877
2756.217906	118619.199569	46.825882
2752.677148	117991.489977	46.830887
2748.967842	117362.163939	46.835892
2745.456399	116740.396399	46.840897
2741.275562	116124.796105	46.845901
2737.502273	115516.161608	46.850906
2733.381568	114912.702795	46.855911
2729.484491	114327.821409	46.860916
2725.831929	113733.616694	46.865921
2721.678453	113174.490704	46.870925
2718.252342	112603.740767	46.875930
2714.698452	112040.228827	46.880935
2710.782566	111486.788155	46.885940
2707.375371	110935.069599	46.890945
2703.203018	110391.920663	46.895949
2699.744950	109851.885479	46.900954
2696.067916	109316.469505	46.905959
2692.488365	108787.746428	46.910964
2688.830570	108250.614843	46.915969
2685.103369	107736.919402	46.920973
2681.914834	107204.803474	46.925978
2677.979311	106681.570910	46.930983
2674.442497	106172.280490	46.935988
2671.310475	105659.515165	46.940993
2667.849039	105145.626667	46.945997
2664.672087	104634.358470	46.951002
2661.208301	104126.282429	46.956007
2656.979966	103606.803970	46.961012
2653.832327	103096.330128	46.966017
2650.522208	102574.843681	46.971021
2647.391396	102064.802601	46.976026
2643.797076	101553.570521	46.981031
2640.347373	101034.596073	46.986036
2637.365406	100518.976111	46.991041
2633.836051	100010.185760	46.996045
2630.642332	99487.586610	47.001050
2626.834448	98963.884124	47.006055
2623.469798	98444.747390	47.011060
2620.175006	97912.784798	47.016065
2616.413204	97381.564645	47.021069
2613.208512	96865.008714	47.026074
2609.700501	96336.143162	47.031079
2606.339276	95818.586684	47.036084
2603.400867	95288.137904	47.041089
2599.950592	94750.089615	47.046093
2596.265453	94207.868307	47.051098
2592.816950	93692.584643	47.056103
2589.192048	93145.632817	47.061108
2586.120252	92602.963142	47.066113
2583.000263	92069.967679	47.071117
2579.485902	91518.478841	47.076122
2575.701646	90969.557883	47.081127
2571.949095	90430.298529	47.086132
2569.324398	89880.302173	47.091137
2565.331063	89333.286018	47.096141
2562.055743	88783.538189	47.101146
2558.485781	88235.536175	47.106151
2554.974168	87685.553305	47.111156
2551.688023	87130.044559	47.116161
2548.128535	86584.930201	47.121165
2544.860667	86026.962231	47.126170
2541.043907	85457.656949	47.131175
2537.535862	84901.196256	47.136180
2534.652902	84349.273044	47.141185
2530.615689	83797.324118	47.146189
2527.054251	83231.313271	47.151194
2523.948047	82676.217869	47.156199
2520.472307	82113.074038	47.161204
2516.929685	81542.800564	47.166209
2513.534413	80983.871152	47.171213
2510.056629	80409.152263	47.176218
2506.849405	79842.760562	47.181223
2503.110704	79283.778915	47.186228
2499.546200	78714.112768	47.191233
2495.946530	78142.025351	47.196237
2492.638367	77573.219248	47.201242
2489.154205	76990.787147	47.206247
2485.914161	76428.293475	47.211252
2482.705976	75852.522843	47.216257
2478.983738	75270.266275	47.221261
2475.292708	74692.550943	47.226266
2471.645760	74105.342596	47.231271
2468.414343	73533.155439	47.236276
2464.566898	72948.111681	47.241281
2461.133949	72386.215231	47.246285
2457.912902	71801.467552	47.251290
2454.504951	71217.587262	47.256295
2450.688764	70638.709923	47.261300
2447.374387	70060.110124	47.266305
2443.883216	69476.497518	47.271309
2440.700391	68893.992707	47.276314
2437.265088	68308.639315	47.281319
2433.576064	67723.814799	47.286324
2430.482088	67133.128320	47.291329
2426.418880	66551.372206	47.296333
2423.156389	65960.529640	47.301338
2419.665179	65370.548871	47.306343
2415.944007	64784.368766	47.311348
2412.529614	64189.351426	47.316353
2409.039527	63607.504088	47.321357
2405.666298	63021.488744	47.326362
2401.991977	62432.379864	47.331367
2398.602754	61838.715698	47.336372
2395.064496	61240.126302	47.341377
2391.755889	60653.744435	47.346381
2388.475279	60050.517685	47.351386
2384.641826	59456.440790	47.356391
2381.192965	58868.657715	47.361396
2378.057286	58263.441132	47.366401
2374.390043	57674.293313	47.371405
2370.818317	57072.036152	47.376410
2367.449936	56479.476489	47.381415
2363.615339	55884.231408	47.386420
2360.581252	55287.595007	47.391425
2356.974966	54689.095869	47.396429
2353.789228	54081.220359	47.401434
2350.445716	53476.411201	47.406439
2346.389201	52872.223397	47.411444
2343.240179	52262.390881	47.416449
2339.747802	51660.899792	47.421453
2336.115136	51047.057367	47.426458
2332.956426	50443.522346	47.431463
2329.071949	49835.904231	47.436468
2325.569751	49222.521349	47.441473
2322.089482	48622.204877	47.446477
2318.644766	48006.834979	47.451482
2315.259203	47409.402548	47.456487
2311.656080	46808.544151	47.461492
2308.444470	46176.862643	47.466497
2304.239444	45581.578439	47.471501
2301.194469	44959.316599	47.476506
2297.576170	44349.926856	47.481511
2294.356886	43752.736906	47.486516
2290.986066	43131.065079	47.491521
2287.112209	42528.702352	47.496525
2283.496275	41909.943800	47.501530
2280.008544	41306.666675	47.506535
2276.275284	40699.646392	47.511540
2272.802512	40083.630856	47.516545
2268.975715	39483.696754	47.521549
2265.219549	38883.070849	47.526554
2261.803134	38282.174176	47.531559
2257.897838	37687.158422	47.536564
2254.223041	37096.288302	47.541569
2250.296303	36514.145840	47.546573
2245.942996	35936.852657	47.551578
2241.921843	35377.063319	47.556583
2237.893553	34822.620782	47.561588
2234.321546	34269.186656	47.566593
2229.833719	33736.801136	47.571597
2225.750811	33194.630454	47.576602
2221.801081	32686.539576	47.581607
2217.661039	32175.366033	47.586612
2214.211121	31663.184972	47.591617
2210.326404	31167.226257	47.596621
2206.726212	30675.126366	47.601626
2203.052872	30166.996983	47.606631
2199.114190	29696.254002	47.611636
2195.381176	29212.897994	47.616641
2191.754287	28746.608556	47.621645
2187.995789	28279.425043	47.626650
2184.744209	27810.494110	47.631655
2180.961904	27350.052428	47.636660
2177.622557	26880.598959	47.641665
2174.049131	26428.927848	47.646669
2170.365318	25975.085380	47.651674
2167.144283	25518.019461	47.656679
2163.181206	25065.951617	47.661684
2160.112287	24613.729445	47.666689
2156.231728	24162.809518	47.671693
2152.624173	23711.344106	47.676698
2149.739426	23283.533501	47.681703
2146.044764	22834.154122	47.686708
2142.633652	22381.719011	47.691713
2139.420228	21941.141203	47.696717
2135.983669	21493.069691	47.701722
2132.312254	21045.811378	47.706727
2128.975427	20605.979373	47.711732
2125.867434	20156.385892	47.716737
2121.937642	19710.940090	47.721741
2118.677919	19270.137935	47.726746
2115.455896	18816.406260	47.731751
2111.577459	18370.881712	47.736756
2108.108616	17916.088392	47.741761
2104.340103	17467.527395	47.746765
2100.800338	17018.013386	47.751770
2097.296637	16577.911991	47.756775
2093.831000	16134.122639	47.761780
2090.485569	15688.193849	47.766785
2086.922291	15240.336721	47.771789
2083.183462	14801.667819	47.776794
2079.662167	14362.345075	47.781799
2076.137091	13920.322876	47.786804
2072.914509	13471.352460	47.791809
2069.184625	13033.102853	47.796813
2065.926860	12602.786906	47.801818
2062.365623	12158.709281	47.806823
2058.941531	11721.876609	47.811828
2055.341086	11285.053036	47.816833
2051.593216	10855.768156	47.821837
2047.841308	10420.855979	47.826842
2043.879346	9996.258439	47.831847
2040.324803	9569.499027	47.836852
2036.630527	9144.439251	47.841857
2032.434401	8745.387270	47.846861
2028.229238	8337.755069	47.851866
2024.124051	7951.971185	47.856871
2019.966768	7586.152588	47.861876
2016.114754	7205.111444	47.866881
2011.594814	6856.862831	47.871885
2007.373231	6503.757511	47.876890
2003.223275	6165.987514	47.881895
1999.263044	5847.976892	47.886900
1995.225806	5531.803474	47.891905
1991.398830	5231.941715	47.896909
1987.186959	4934.727078	47.901914
1982.874528	4652.295407	47.906919
1979.239672	4382.385733	47.911924
1975.287136	4097.995339	47.916929
1971.779276	3843.101760	47.921933
1967.759829	3593.740368	47.926938
1964.547502	3329.621983	47.931943
1960.480939	3096.899944	47.936948
1957.158891	2851.689848	47.941953
1953.476703	2621.148061	47.946957
1950.211586	2387.361216	47.951962
1946.506937	2162.195159	47.956967
1943.082882	1935.855533	47.961972
1939.429667	1701.112881	47.966977
1935.843275	1490.345714	47.971981
1932.104590	1269.328314	47.976986
1928.751434	1059.605661	47.981991
1924.905135	842.527183	47.986996
1921.475968	630.192254	47.992001
1917.751718	440.115468	47.997005
1913.960152	237.722096	48.002010
1909.412826	64.039063	48.007015
1898.131991	82.891476	48.012020
1889.436525	96.504211	48.017025
1883.805646	102.594400	48.022029
1880.716455	113.986864	48.027034
1878.628281	102.283432	48.032039
1875.912875	105.885600	48.037044
1874.069329	108.918646	48.042049
1871.037123	107.403773	48.047053
1867.992182	111.120504	48.052058
1865.026571	102.021335	48.057063
1861.846226	107.704824	48.062068
1858.670674	97.844240	48.067073
1855.461807	107.569066	48.072077
1851.894562	98.930529	48.077082
1848.827546	95.889840	48.082087
1845.003456	113.777889	48.087092
1841.300426	97.697284	48.092097
1838.044590	102.430753	48.097101
1834.758788	103.625527	48.102106
1831.760340	100.172377	48.107111
1828.484380	112.584148	48.112116
1824.892750	102.611157	48.117121
1821.018307	99.705628	48.122125
1817.058848	110.445771	48.127130
1814.385719	104.600840	48.132135
1811.067868	100.593134	48.137140
1808.150186	100.164579	48.142145
1804.793477	112.237745	48.147149
1801.151544	102.513030	48.152154
1797.614235	96.394485	48.157159
1793.541193	102.577576	48.162164
1790.273070	100.514143	48.167169
1787.024366	97.330898	48.172173
1783.256297	106.604926	48.177178
1780.300971	99.234721	48.182183
1776.528579	94.918119	48.187188
1773.569468	102.658388	48.192193
1770.325747	99.540807	48.197197
1766.333264	105.192513	48.202202
1763.245198	92.733580	48.207207
1759.624560	98.504578	48.212212
1756.295454	98.867715	48.217217
1752.574709	94.574715	48.222221
1748.840081	95.273046	48.227226
1745.766018	94.232930	48.232231
1741.889759	99.202167	48.237236
1739.128302	92.997680	48.242241
1735.679052	102.190448	48.247245
1731.875203	97.571867	48.252250
1728.142567	91.138891	48.257255
1724.488284	98.860808	48.262260
1720.799002	98.479587	48.267265
1717.788699	87.011459	48.272269
1714.709269	89.844559	48.277274
1711.631609	84.907320	48.282279
1707.828898	85.809237	48.287284
1704.372843	92.797957	48.292289
1700.746300	85.203213	48.297293
1697.119162	95.777731	48.302298
1693.507037	87.690369	48.307303
1689.964229	97.100174	48.312308
1686.495485	79.069114	48.317313
1683.434806	87.245959	48.322317
1679.718391	89.871323	48.327322
1676.062612	84.571657	48.332327
1672.451748	98.895800	48.337332
1669.042510	90.773698	48.342337
1665.728572	85.310099	48.347341
1661.839364	88.487533	48.352346
1659.151232	81.648397	48.357351
1655.262178	90.814701	48.362356
1652.022676	82.093557	48.367361
1648.523258	85.207160	48.372365
1645.045229	92.322686	48.377370
1641.458888	92.377861	48.382375
1637.634968	95.934272	48.387380
1634.465209	81.346257	48.392385
1630.823431	88.094969	48.397389
1627.276942	97.935612	48.402394
1624.071129	86.652953	48.407399
1620.278867	93.630729	48.412404
1616.639285	87.847667	48.417409
1613.577403	83.214863	48.422413
1609.920801	100.042286	48.427418
1606.690074	86.858956	48.432423
1602.781236	92.640015	48.437428
1599.575272	83.284082	48.442433
1596.095875	84.414094	48.447437
1592.592377	85.484583	48.452442
1589.420023	80.925924	48.457447
1585.497132	91.710986	48.462452
1582.012562	88.975758	48.467457
1578.350174	88.691605	48.472461
1574.958157	96.312594	48.477466
1572.043373	90.682478	48.482471
1568.000949	98.904566	48.487476
1564.170147	84.824405	48.492481
1561.148811	85.737595	48.497485
1557.469500	85.057451	48.502490
1553.924245	82.423421	48.507495
1550.510695	89.434002	48.512500
1547.643508	98.128057	48.517505
1544.139209	80.855527	48.522509
1539.953337	94.649074	48.527514
1537.099680	92.122532	48.532519
1532.936229	98.927138	48.537524
1529.538101	89.174023	48.542529
1526.049530	85.107507	48.547533
1522.288673	85.556846	48.552538
1518.956700	87.198584	48.557543
1515.546411	90.570403	48.562548
1512.244524	88.388871	48.567553
1508.758674	94.148391	48.572557
1505.246676	96.191468	48.577562
1501.900521	96.095380	48.582567
1498.239403	99.142415	48.587572
1494.835578	91.136556	48.592577
1490.925253	80.387516	48.597581
1487.781541	83.417292	48.602586
1484.131675	79.141774	48.607591
1480.821315	82.396802	48.612596
1477.160186	87.079472	48.617601
1473.790498	90.932184	48.622605
1470.353804	90.767934	48.627610
1466.563266	92.183663	48.632615
1462.911245	82.612448	48.637620
1459.446146	80.484800	48.642625
1456.093839	94.616832	48.647629
1452.672673	90.318374	48.652634
1449.328540	79.259758	48.657639
1445.883489	86.702344	48.662644
1442.336641	85.061976	48.667649
1438.685474	83.279661	48.672653
1434.987800	89.613146	48.677658
1431.788818	86.637337	48.682663
1427.950235	96.226057	48.687668
1425.012210	84.715097	48.692673
1421.406073	82.827701	48.697677
1417.496469	86.387972	48.702682
1414.318420	83.089373	48.707687
1410.671011	92.053561	48.712692
1407.406192	88.591301	48.717697
1403.776382	91.516413	48.722701
1399.991284	92.713006	48.727706
1396.799355	81.902786	48.732711
1393.245663	95.651719	48.737716
1389.674824	85.561688	48.742721
1386.202749	85.194150	48.747725
1382.716726	87.812150	48.752730
1379.216048	74.984099	48.757735
1375.908030	91.184617	48.762740
1372.182925	79.138130	48.767745
1368.820657	85.409920	48.772749
1364.993228	79.798503	48.777754
1361.516514	75.739657	48.782759
1358.213569	87.111584	48.787764
1354.671213	86.429127	48.792769
1351.313095	80.662408	48.797773
1347.662932	88.750680	48.802778
1344.717237	80.654561	48.807783
1340.940333	83.181801	48.812788
1337.379095	79.449319	48.817793
1333.989077	80.245909	48.822797
1329.939923	87.140299	48.827802
1326.612024	80.416607	48.832807
1323.053659	85.674902	48.837812
1319.498342	84.099141	48.842817
1316.235964	83.847665	48.847821
1312.347961	86.619986	48.852826
1309.242945	86.325034	48.857831
1305.627131	92.351562	48.862836
1302.377799	81.980557	48.867841
1299.026230	82.090971	48.872845
1295.148717	93.438440	48.877850
1291.678727	86.078820	48.882855
1287.938072	88.806063	48.887860
1284.871083	79.188114	48.892865
1281.562003	76.412955	48.897869
1277.633517	84.275637	48.902874
1274.018011	88.650668	48.907879
1270.734328	75.972359	48.912884
1267.614348	80.137384	48.917889
1263.716015	76.099886	48.922893
1259.821846	81.565474	48.927898
1256.654041	76.063371	48.932903
1253.004337	86.622419	48.937908
1249.532471	77.554707	48.942913
1246.366192	76.218951	48.947917
1242.423297	83.644124	48.952922
1239.450962	78.839246	48.957927
1235.626504	78.618321	48.962932
1232.323354	73.346093	48.967937
1229.051914	73.750921	48.972941
1225.293554	82.286299	48.977946
1221.496444	74.468258	48.982951
1217.991772	78.629891	48.987956
1214.571932	71.477615	48.992961
1211.269616	81.175847	48.997965
1207.992555	84.017594	49.002970
1204.250016	72.467398	49.007975
1200.758246	75.994285	49.012980
1197.606621	74.033007	49.017985
1193.578894	69.367106	49.022989
1189.752576	75.458037	49.027994
1186.745239	69.779112	49.032999
1182.950179	77.412223	49.038004
1179.686114	82.333658	49.043009
1176.328025	69.360077	49.048013
1172.711130	74.086499	49.053018
1169.401603	72.412389	49.058023
1165.465932	79.586508	49.063028
1161.961284	77.015809	49.068033
1158.483851	70.135094	49.073037
1154.763408	73.982310	49.078042
1151.778296	77.477793	49.083047
1148.333284	78.513910	49.088052
1145.068924	73.074309	49.093057
1141.665572	70.750433	49.098061
1137.632024	74.782426	49.103066
1134.090634	70.809610	49.108071
1130.454023	66.484628	49.113076
1127.111831	78.947803	49.118081
1123.431603	78.505129	49.123085
1119.878700	83.405090	49.128090
1117.001034	79.025246	49.133095
1113.045363	79.973179	49.138100
1109.979013	76.100424	49.143105
1106.381130	71.459375	49.148109
1102.363826	75.004800	49.153114
1098.842192	71.108005	49.158119
1095.195311	84.716410	49.163124
1091.714965	75.621575	49.168129
1089.005849	75.768047	49.173133
1085.168332	78.051650	49.178138
1081.755794	67.253693	49.183143
1078.170886	79.463590	49.188148
1074.599701	79.003948	49.193153
1071.113451	77.259284	49.198157
1067.136653	82.623856	49.203162
1064.015484	81.217824	49.208167
1060.510922	79.842999	49.213172
1057.179514	69.174783	49.218177
1053.905546	73.838343	49.223181
1050.193903	89.355044	49.228186
1046.528551	80.921751	49.233191
1042.877171	85.602933	49.238196
1039.301180	74.466600	49.243201
1036.113277	75.149502	49.248205
1032.666501	75.046978	49.253210
1029.535871	72.095382	49.258215
1025.468025	78.995862	49.263220
1022.035160	69.096403	49.268225
1018.396830	73.117507	49.273229
1014.978668	74.972017	49.278234
1011.299029	64.955956	49.283239
1008.382868	75.634932	49.288244
1004.873972	77.974956	49.293249
1001.114107	76.747444	49.298253
997.463742	74.155158	49.303258
993.990920	75.790393	49.308263
990.293290	75.394735	49.313268
986.797888	75.495935	49.318273
983.299303	68.735599	49.323277
979.931713	80.886361	49.328282
976.975233	66.743021	49.333287
973.162871	68.206489	49.338292
969.620496	75.003030	49.343297
966.193657	67.883524	49.348301
962.581869	69.069004	49.353306
959.220492	61.736837	49.358311
955.313929	71.858151	49.363316
952.049302	73.644475	49.368321
948.859243	74.087282	49.373325
945.216759	80.026232	49.378330
941.387963	72.507401	49.383335
937.907549	79.212044	49.388340
934.565846	71.677502	49.393345
931.038080	67.841797	49.398349
927.228869	78.526916	49.403354
923.929234	65.999865	49.408359
920.489040	69.502927	49.413364
916.964138	78.947918	49.418369
913.619128	74.422557	49.423373
909.834746	72.702176	49.428378
906.335814	77.074906	49.433383
902.848288	78.127157	49.438388
899.282745	75.632411	49.443393
895.965307	71.226145	49.448397
892.670037	84.147080	49.453402
889.093541	71.207560	49.458407
885.586880	79.710100	49.463412
881.885000	74.167807	49.468417
878.494857	81.026078	49.473421
874.789770	82.159654	49.478426
871.229184	58.271332	49.483431
867.924855	72.047863	49.488436
864.854331	76.265324	49.493441
861.066250	77.332730	49.498445
857.325622	76.171844	49.503450
854.028153	68.510212	49.508455
850.479732	72.678683	49.513460
846.663373	73.181029	49.518465
843.662539	68.636904	49.523469
839.790014	69.413743	49.528474
836.840745	65.228580	49.533479
832.891421	66.672257	49.538484
829.430626	68.466984	49.543489
826.007273	61.334308	49.548493
821.939621	61.907413	49.553498
819.234999	63.366135	49.558503
815.568249	72.213127	49.563508
811.727140	73.209701	49.568513
808.236806	67.694602	49.573517
804.756059	71.526683	49.578522
801.501177	57.018563	49.583527
797.735141	65.023652	49.588532
794.397475	63.148331	49.593537
790.959555	63.123549	49.598541
787.382521	74.705814	49.603546
783.891754	67.900005	49.608551
780.377873	76.900370	49.613556
777.281925	75.721395	49.618561
773.800083	62.175567	49.623565
769.693259	66.652426	49.628570
766.197517	69.126463	49.633575
762.668539	68.508433	49.638580
759.428816	59.477452	49.643585
756.036944	65.997480	49.648589
751.900704	71.538753	49.653594
748.616033	59.414368	49.658599
745.468625	68.376664	49.663604
741.702453	60.063537	49.668609
738.779874	61.537213	49.673613
734.660743	64.978306	49.678618
731.494878	64.844744	49.683623
727.553174	65.768405	49.688628
724.128468	69.155181	49.693633
721.086998	62.918507	49.698637
716.698610	67.369602	49.703642
713.678292	65.505000	49.708647
710.436390	67.809816	49.713652
706.901009	65.209167	49.718657
703.285432	68.309290	49.723661
699.913550	72.244653	49.728666
696.446770	57.095682	49.733671
692.367508	69.635629	49.738676
689.238991	66.250327	49.743681
686.089994	59.201516	49.748685
682.598437	65.281498	49.753690
678.934540	63.785999	49.758695
675.192163	53.627927	49.763700
671.757792	65.254416	49.768705
668.704324	58.181247	49.773709
664.515248	69.415874	49.778714
661.267603	63.961096	49.783719
657.252243	63.004356	49.788724
653.870098	61.949042	49.793729
650.648353	60.289807	49.798733
646.966989	60.518071	49.803738
644.087352	49.624605	49.808743
640.767354	56.490944	49.813748
636.670378	53.658201	49.818753
633.581782	57.312191	49.823757
629.681955	64.357380	49.828762
626.510162	62.026000	49.833767
622.662557	67.215476	49.838772
618.870724	62.671140	49.843777
615.534343	59.305554	49.848781
611.775979	65.686497	49.853786
608.734296	63.119735	49.858791
605.470553	63.542413	49.863796
602.191884	65.343612	49.868801
598.736556	63.821984	49.873805
594.704945	63.310697	49.878810
591.322898	63.555645	49.883815
587.531255	56.828354	49.888820
584.071873	58.556449	49.893825
580.517338	55.591816	49.898829
576.744941	55.055998	49.903834
573.878838	57.609200	49.908839
570.366652	50.249967	49.913844
566.523032	64.914018	49.918849
563.228782	57.701185	49.923853
559.803500	56.111613	49.928858
556.012316	60.640594	49.933863
552.632413	56.636405	49.938868
548.837766	52.680965	49.943873
545.832308	55.452011	49.948877
541.769898	61.984692	49.953882
538.786588	56.767189	49.958887
535.192093	60.379726	49.963892
531.544977	66.458627	49.968897
528.377507	59.286173	49.973901
524.198524	66.811415	49.978906
520.959919	63.370512	49.983911
517.675371	64.919541	49.988916
514.307547	66.430917	49.993921
510.651887	64.165389	49.998925
507.111605	66.709660	50.003930
503.950538	60.194257	50.008935
500.093171	64.129287	50.013940
496.826276	58.778773	50.018945
493.147774	64.185538	50.023949
489.420730	73.595577	50.028954
485.988308	62.009929	50.033959
482.818283	65.069185	50.038964
479.110881	57.493592	50.043969
475.784055	52.645945	50.048973
472.036554	62.391349	50.053978
468.482539	64.801725	50.058983
465.097207	63.500167	50.063988
461.325319	68.953111	50.068993
458.191955	68.210260	50.073997
454.685231	67.595136	50.079002
451.326378	63.420010	50.084007
447.575056	67.569486	50.089012
443.790750	64.172421	50.094017
440.502512	65.162064	50.099021
436.832559	63.528343	50.104026
433.591347	58.952104	50.109031
430.338208	60.088140	50.114036
426.745602	70.119476	50.119041
423.660419	64.516063	50.124045
419.480391	63.129428	50.129050
415.975680	54.937015	50.134055
412.280505	64.085836	50.139060
408.638913	64.757181	50.144065
405.489059	54.453143	50.149069
401.934237	67.332223	50.154074
398.539537	62.381261	50.159079
394.938951	63.561902	50.164084
391.429499	63.156013	50.169089
387.758787	65.094197	50.174093
384.054169	65.215389	50.179098
380.755777	62.116000	50.184103
377.409611	63.228562	50.189108
373.869475	71.584481	50.194113
370.534595	66.244570	50.199117
367.020953	58.781199	50.204122
363.773876	63.959464	50.209127
359.983735	65.821335	50.214132
356.606348	63.977568	50.219137
353.276069	64.837730	50.224141
349.612795	62.563922	50.229146
345.923493	63.119321	50.234151
342.415386	69.296817	50.239156
338.909508	70.285556	50.244161
335.584249	58.705407	50.249165
331.950341	65.111290	50.254170
328.329936	68.683592	50.259175
325.044787	66.736888	50.264180
321.466148	72.659619	50.269185
317.655014	59.994052	50.274189
314.007125	62.627862	50.279194
310.772002	60.682863	50.284199
307.396965	54.343174	50.289204
304.025542	60.635429	50.294209
300.645842	50.765821	50.299213
296.745365	60.962146	50.304218
293.481660	54.314069	50.309223
289.835287	62.759294	50.314228
286.009463	53.035071	50.319233
282.868938	54.216865	50.324237
279.267321	63.018944	50.329242
276.077742	60.184198	50.334247
272.497536	54.521845	50.339252
269.056166	51.947758	50.344257
265.607761	53.266069	50.349261
261.963729	62.150680	50.354266
258.557638	52.465518	50.359271
254.841064	55.236574	50.364276
250.974289	58.859895	50.369281
247.907368	52.548176	50.374285
244.527750	68.924302	50.379290
240.804837	64.318687	50.384295
237.401392	60.381488	50.389300
233.847341	62.396439	50.394305
230.476972	61.620917	50.399309
226.584633	66.719325	50.404314
223.127238	56.210113	50.409319
219.749964	56.533458	50.414324
216.408390	66.010044	50.419329
213.250858	56.912596	50.424333
209.406163	61.785295	50.429338
205.884998	54.604696	50.434343
202.360097	55.881143	50.439348
198.548710	59.125699	50.444353
195.135399	51.526528	50.449357
191.881029	60.726952	50.454362
188.124809	57.847566	50.459367
184.823365	58.064200	50.464372
181.621792	56.373417	50.469377
177.882688	51.185062	50.474381
173.857477	55.443645	50.479386
170.902200	59.023138	50.484391
167.389633	56.419024	50.489396
163.733725	71.512594	50.494401
160.811340	56.149300	50.499405
156.957923	59.963536	50.504410
153.584360	48.311867	50.509415
149.770079	50.902001	50.514420
145.857922	54.709565	50.519425
142.634817	54.493242	50.524429
138.872022	52.956280	50.529434
135.584963	52.240566	50.534439
132.424861	55.212892	50.539444
128.835673	55.888773	50.544449
125.313564	53.317788	50.549453
121.838712	61.195335	50.554458
118.509480	58.796796	50.559463
114.781274	57.406308	50.564468
111.305979	62.689726	50.569473
108.135236	58.156353	50.574477
103.989001	59.988281	50.579482
100.466121	53.864634	50.584487
97.048210	52.932024	50.589492
93.461098	63.633215	50.594497
89.851281	56.643607	50.599501
86.414997	55.966952	50.604506
83.453559	53.536465	50.609511
79.876442	57.399438	50.614516
76.557710	54.954980	50.619521
73.129078	50.591476	50.624525
69.165593	65.429221	50.629530
65.882109	57.797206	50.634535
62.182556	55.788517	50.639540
58.366399	57.600698	50.644545
55.308031	49.085779	50.649549
51.439044	54.819627	50.654554
47.860327	47.641698	50.659559
44.585262	53.257766	50.664564
41.153039	66.430970	50.669569
37.715942	54.330486	50.674573
34.645293	54.106259	50.679578
30.701774	61.022268	50.684583
26.852589	55.784644	50.689588
23.614265	62.559221	50.694593
20.064795	58.347413	50.699597
16.679067	58.469628	50.704602
13.115320	57.999485	50.709607
9.527380	50.342123	50.714612
6.036344	64.549508	50.719617
2.830738	58.224625	50.724621