Fri Aug 26 13:57:05 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.724547	100.142940	0.000000
-0.587911	106.860293	0.005005
-0.946387	96.064777	0.010010
-0.931286	95.793543	0.015014
-1.063350	91.581157	0.020019
-1.264422	98.319450	0.025024
-1.108273	84.011245	0.030029
-1.375930	92.784644	0.035034
-1.463347	77.274213	0.040038
-1.572000	63.522929	0.045043
-2.082483	62.760906	0.050048
-1.994530	44.923222	0.055053
-2.483675	49.912559	0.060058
-2.746165	36.783178	0.065062
-2.361256	28.855283	0.070067
-3.093533	20.212349	0.075072
-3.600311	12.477075	0.080077
-4.368996	12.590458	0.085082
-4.178126	6.401152	0.090086
-4.170763	11.107537	0.095091
-5.144953	7.836180	0.100096
-5.325133	-5.343948	0.105101
-5.564101	2.842829	0.110106
-5.710561	9.645350	0.115110
-6.316863	6.414787	0.120115
-6.899472	4.227702	0.125120
-6.921891	-2.213120	0.130125
-7.055470	7.969328	0.135130
-7.150688	-2.003441	0.140134
-6.755720	-2.640691	0.145139
-7.403397	7.033363	0.150144
-7.981237	-4.898484	0.155149
-8.310540	10.623031	0.160154
-8.251990	3.587489	0.165158
-8.655644	-1.028663	0.170163
-8.934805	8.059686	0.175168
-8.832666	-0.017152	0.180173
-9.689096	4.858520	0.185178
-9.701517	-2.077386	0.190182
-10.048952	-1.494936	0.195187
-10.012024	2.574115	0.200192
-10.097788	3.479644	0.205197
-11.006805	1.909672	0.210202
-11.360519	-4.871859	0.215206
-11.211218	0.283806	0.220211
-11.626741	4.847230	0.225216
-11.320153	-3.530348	0.230221
-11.334486	-5.356674	0.235226
-11.860486	-7.815153	0.240230
-12.528137	-4.224841	0.245235
-12.887357	1.940110	0.250240
-12.597434	2.034199	0.255245
-13.073536	-1.438089	0.260250
-13.638458	1.750265	0.265254
-13.627295	-2.430616	0.270259
-14.284070	2.989753	0.275264
-14.263736	-3.464052	0.280269
-14.149214	2.253829	0.285274
-14.359080	4.966139	0.290278
-14.713313	-2.049422	0.295283
-15.311066	6.389365	0.300288
-15.431831	8.524673	0.305293
-15.949671	10.123877	0.310298
-15.888193	5.583995	0.315302
-15.903097	7.471875	0.320307
-16.497124	0.537940	0.325312
-16.880106	3.463858	0.330317
-17.445430	5.551328	0.335322
-17.550580	6.453547	0.340326
-17.212281	5.125955	0.345331
-17.199375	9.243038	0.350336
-17.474912	-0.461219	0.355341
-18.015285	1.220583	0.360346
-18.413510	7.853501	0.365350
-18.840003	-0.963577	0.370355
-18.862943	7.569205	0.375360
-18.965446	-0.678244	0.380365
-19.735244	2.643246	0.385370
-19.899612	7.360549	0.390374
-19.887398	1.933027	0.395379
-20.428876	4.766568	0.400384
-20.661696	0.481309	0.405389
-20.269281	5.535850	0.410394
-20.420255	-0.894447	0.415398
-21.021455	-4.594020	0.420403
-21.958688	9.022723	0.425408
-21.638043	4.208381	0.430413
-21.994431	2.599821	0.435418
-21.868017	3.377405	0.440422
-22.311525	8.252061	0.445427
-22.630087	8.766743	0.450432
-22.694944	0.649470	0.455437
-23.210675	9.638616	0.460442
-23.317633	11.379483	0.465446
-23.793445	8.024204	0.470451
-24.702107	11.658371	0.475456
-24.453914	3.906793	0.480461
-24.712897	0.109646	0.485466
-24.841821	-2.850404	0.490470
-24.437812	-6.004157	0.495475
-25.250836	-1.457936	0.500480
-25.207023	-3.024405	0.505485
-25.363452	-1.108163	0.510490
-25.739338	5.015093	0.515494
-25.913411	10.081908	0.520499
-26.291037	-0.024054	0.525504
-26.575411	1.114870	0.530509
-27.020684	-0.100212	0.535514
-27.323668	7.410023	0.540518
-27.452277	-4.316529	0.545523
-27.887671	2.350646	0.550528
-27.509522	2.699907	0.555533
-28.423832	-3.329975	0.560538
-28.976759	-2.614292	0.565542
-28.803916	-6.864637	0.570547
-29.060990	-5.897636	0.575552
-29.019230	-6.786766	0.580557
-28.723963	-4.146779	0.585562
-29.818358	-3.068391	0.590566
-29.875406	-6.444577	0.595571
-30.216082	3.188001	0.600576
-30.190431	3.022690	0.605581
-30.499083	2.169136	0.610586
-31.311743	12.251680	0.615590
-31.492958	9.546534	0.620595
-31.635495	12.612180	0.625600
-31.898170	-1.779433	0.630605
-31.903806	1.926097	0.635610
-32.139739	15.892383	0.640614
-31.967653	3.726716	0.645619
-32.715875	4.918879	0.650624
-33.028455	-1.780474	0.655629
-33.491959	6.286245	0.660634
-33.929309	0.397229	0.665638
-33.722242	-0.536621	0.670643
-33.579360	1.140037	0.675648
-34.108069	1.222383	0.680653
-34.796331	4.198996	0.685658
-34.867204	1.694963	0.690662
-34.961238	-1.618519	0.695667
-35.279568	0.190057	0.700672
-35.305848	-3.235211	0.705677
-35.321327	3.875931	0.710682
-36.027854	12.113364	0.715686
-36.411473	1.391425	0.720691
-36.294398	3.904139	0.725696
-36.257592	-5.288780	0.730701
-36.756629	2.947979	0.735706
-37.089278	0.620741	0.740710
-37.378111	-8.141837	0.745715
-37.839412	-4.672235	0.750720
-37.686943	-6.964277	0.755725
-38.215824	-7.587395	0.760730
-39.244322	-1.084131	0.765734
-39.116283	-9.576269	0.770739
-39.346711	5.607152	0.775744
-39.080839	-4.118124	0.780749
-39.441077	-5.675464	0.785754
-39.621286	-8.447200	0.790758
-39.420098	-6.849222	0.795763
-40.416777	-6.773104	0.800768
-40.547463	-11.542479	0.805773
-40.710691	-7.787105	0.810778
-40.620275	0.693222	0.815782
-40.950411	-7.287833	0.820787
-42.002480	0.541503	0.825792
-42.068121	-0.852906	0.830797
-42.385477	0.101335	0.835802
-42.552668	0.646232	0.840806
-42.127092	-4.152809	0.845811
-42.333301	4.803959	0.850816
-42.551951	-7.845008	0.855821
-43.052219	-3.540465	0.860826
-43.809579	-4.121682	0.865830
-43.484149	-4.868324	0.870835
-43.736181	1.691210	0.875840
-44.252656	-2.287300	0.880845
-44.700049	-7.105438	0.885850
-45.010599	-3.902908	0.890854
-45.154761	-1.852540	0.895859
-44.890782	8.258515	0.900864
-45.002359	-0.876502	0.905869
-45.920231	-1.970547	0.910874
-46.692410	5.043284	0.915878
-46.643938	2.289724	0.920883
-46.412972	-0.840251	0.925888
-46.405098	-4.875091	0.930893
-46.875719	-5.001098	0.935898
-46.881020	0.390600	0.940902
-47.467474	-10.353531	0.945907
-47.718758	-3.781461	0.950912
-47.886942	-6.596196	0.955917
-48.170667	-15.043202	0.960922
-48.515779	-2.901172	0.965926
-48.947413	-4.301868	0.970931
-49.520296	-1.688058	0.975936
-49.567025	3.014090	0.980941
-49.583200	-0.906279	0.985946
-49.863243	3.208959	0.990950
-49.465359	-2.152063	0.995955
-49.650767	2.492586	1.000960
-50.372541	2.769502	1.005965
-50.808956	-0.199616	1.010970
-51.252080	11.536919	1.015974
-51.469116	-5.604673	1.020979
-51.509091	-1.555288	1.025984
-51.235326	-3.322069	1.030989
-52.038613	1.042309	1.035994
-52.780166	5.333803	1.040998
-52.580107	-3.903514	1.046003
-52.863411	5.027293	1.051008
-52.693945	2.992023	1.056013
-53.024634	-0.841413	1.061018
-53.702172	-0.112656	1.066022
-53.990720	-3.610980	1.071027
-54.455558	0.371684	1.076032
-54.565693	5.716433	1.081037
-54.650380	-3.419605	1.086042
-54.763827	5.978284	1.091046
-54.230375	2.158993	1.096051
-55.228738	2.330283	1.101056
-55.623722	9.491023	1.106061
-55.468358	-2.475887	1.111066
-55.733440	3.652260	1.116070
-56.161578	-3.206262	1.121075
-56.855772	0.865893	1.126080
-56.932014	5.047472	1.131085
-57.189089	1.806830	1.136090
-57.306361	-5.134893	1.141094
-57.031315	-5.196672	1.146099
-57.596962	-2.011368	1.151104
-58.287686	1.130137	1.156109
-58.773554	0.709122	1.161114
-58.761889	-2.339253	1.166118
-58.561483	-6.071887	1.171123
-58.731308	-3.656869	1.176128
-58.865954	-7.122208	1.181133
-59.750265	0.408935	1.186138
-59.920204	0.698004	1.191142
-59.930122	-1.812355	1.196147
-60.002131	-4.809737	1.201152
-60.607004	-1.555054	1.206157
-60.421234	-5.152537	1.211162
-60.696532	-1.499931	1.216166
-61.100418	-4.787314	1.221171
-61.770052	4.181498	1.226176
-61.786251	3.095756	1.231181
-62.841372	2.263518	1.236186
-62.674383	-1.476569	1.241190
-62.238110	-1.841850	1.246195
-62.954518	5.577734	1.251200
-63.039582	1.487763	1.256205
-63.259618	-1.271445	1.261210
-63.496785	0.242931	1.266214
-63.522764	-4.631331	1.271219
-64.412492	-3.572153	1.276224
-64.341807	-10.916448	1.281229
-64.679821	-3.274219	1.286234
-64.530060	0.021151	1.291238
-64.765454	-7.148944	1.296243
-65.270872	3.502665	1.301248
-66.018999	-3.802726	1.306253
-66.150320	2.371030	1.311258
-66.397728	-0.472498	1.316262
-65.908489	-7.609889	1.321267
-66.587853	0.075998	1.326272
-66.489254	-4.621514	1.331277
-66.650508	-4.555251	1.336282
-67.667254	1.452655	1.341286
-67.635867	-7.837488	1.346291
-67.973562	-6.177753	1.351296
-67.630596	-3.950139	1.356301
-67.593947	0.438479	1.361306
-68.913005	-3.671322	1.366310
-68.908035	-11.321749	1.371315
-69.371946	3.300092	1.376320
-69.395001	-1.422770	1.381325
-69.131022	0.908887	1.386330
-69.826501	3.149495	1.391334
-70.164189	-5.906021	1.396339
-70.612347	2.493652	1.401344
-71.113808	-4.378762	1.406349
-70.936130	-4.877781	1.411354
-71.071770	1.587702	1.416358
-70.930321	-1.851025	1.421363
-70.946821	-2.762720	1.426368
-71.404386	-6.604872	1.431373
-71.751438	-3.994587	1.436378
-72.132514	1.335399	1.441382
-72.428197	-1.544903	1.446387
-73.070571	-2.248422	1.451392
-73.204612	2.948193	1.456397
-73.343380	4.962921	1.461402
-73.519469	2.152580	1.466406
-73.210942	-1.087543	1.471411
-74.037319	1.233555	1.476416
-74.387095	4.802848	1.481421
-74.789668	2.372607	1.486426
-75.169676	1.723147	1.491430
-74.561752	-1.860974	1.496435
-75.269977	1.707183	1.501440
-75.955384	-3.301678	1.506445
-75.977667	-1.213341	1.511450
-76.510771	1.467040	1.516454
-76.517403	-6.754201	1.521459
-76.793732	6.288252	1.526464
-76.663657	1.386528	1.531469
-76.408661	-6.394574	1.536474
-77.051598	9.261182	1.541478
-77.576152	-0.227133	1.546483
-77.580924	-1.460182	1.551488
-77.793158	-7.365261	1.556493
-78.574790	-4.965712	1.561498
-79.031393	-5.767756	1.566502
-79.018548	-7.323075	1.571507
-79.271927	2.023834	1.576512
-79.190235	-5.714467	1.581517
-79.502761	1.338521	1.586522
-79.856141	-4.354765	1.591526
-79.635231	-6.945353	1.596531
-80.390170	-8.653201	1.601536
-80.665588	-4.488068	1.606541
-80.697138	-15.777319	1.611546
-81.203782	2.334339	1.616550
-81.256412	-5.563376	1.621555
-81.939161	1.933220	1.626560
-82.308810	1.797821	1.631565
-82.403629	-2.040702	1.636570
-82.457041	0.837064	1.641574
-82.236145	-11.367823	1.646579
-82.288578	-9.164066	1.651584
-82.637210	-0.998184	1.656589
-83.349789	-6.227432	1.661594
-83.783528	-4.116159	1.666598
-83.808465	-7.854834	1.671603
-83.788538	-6.652562	1.676608
-84.353055	-8.355258	1.681613
-84.634597	-9.494595	1.686618
-85.262838	-3.044162	1.691622
-85.242915	-4.619565	1.696627
-85.272441	8.529989	1.701632
-85.458622	3.652197	1.706637
-85.507762	-6.938319	1.711642
-86.041206	-2.239483	1.716646
-86.477749	1.849502	1.721651
-86.750194	-4.198058	1.726656
-86.784929	4.377681	1.731661
-86.910916	-3.299813	1.736666
-87.163872	-0.349850	1.741670
-87.831662	-8.379565	1.746675
-88.234456	6.824361	1.751680
-88.363751	0.409674	1.756685
-88.339083	-1.017777	1.761690
-88.478277	-3.912952	1.766694
-88.406335	-2.652342	1.771699
-88.828852	-4.756785	1.776704
-89.562097	-6.945720	1.781709
-89.598347	-10.758560	1.786714
-89.878069	-14.451236	1.791718
-89.969718	-6.201987	1.796723
-90.126081	-9.240016	1.801728
-90.806279	-14.493284	1.806733
-91.199458	-14.865456	1.811738
-91.145443	-4.952667	1.816742
-91.065520	-19.014801	1.821747
-91.249314	-20.302229	1.826752
-91.959242	-25.199701	1.831757
-92.240122	-17.145612	1.836762
-92.967016	-15.301897	1.841766
-92.891953	-11.719663	1.846771
-92.696437	-6.599673	1.851776
-92.628719	-9.745355	1.856781
-93.110931	-14.304976	1.861786
-94.067530	-4.519562	1.866790
-94.322950	-14.182645	1.871795
-94.576436	-9.938674	1.876800
-94.503659	-12.278415	1.881805
-94.157831	-12.873214	1.886810
-94.524078	0.581851	1.891814
-94.627877	-4.131601	1.896819
-95.297533	-3.236398	1.901824
-95.664583	-10.230971	1.906829
-95.666401	-8.376768	1.911834
-96.015391	-7.370146	1.916838
-96.223773	-0.165702	1.921843
-96.822448	-8.437123	1.926848
-97.221410	-6.429338	1.931853
-96.783299	0.509938	1.936858
-97.391787	-1.195404	1.941862
-96.999918	-1.575917	1.946867
-98.041390	-0.834785	1.951872
-98.257385	1.040112	1.956877
-98.760060	-8.397821	1.961882
-99.105255	3.877095	1.966886
-98.550345	1.440138	1.971891
-98.898538	2.791473	1.976896
-99.561002	0.895226	1.981901
-99.775979	-1.402877	1.986906
-100.169814	1.929676	1.991910
-100.660262	-0.255936	1.996915
-100.398801	0.211007	2.006912
-99.989169	-0.891720	2.016909
-99.141701	0.465200	2.026906
-99.065597	9.807601	2.036902
-99.073498	-4.550259	2.046899
-98.324710	1.820641	2.056896
-97.409291	-2.972004	2.066893
-97.217413	2.776045	2.076890
-96.435066	-0.915699	2.086886
-96.270262	1.082852	2.096883
-96.018735	1.404862	2.106880
-95.258768	1.739571	2.116877
-94.719691	-1.112870	2.126874
-93.768129	-1.815318	2.136870
-93.345468	-6.860680	2.146867
-93.330967	-2.760723	2.156864
-93.267601	-2.247864	2.166861
-91.953983	-4.147053	2.176858
-91.656238	-1.678209	2.186854
-90.854118	2.739426	2.196851
-90.391760	3.234509	2.206848
-90.315648	4.204699	2.216845
-89.784027	1.495965	2.226842
-89.102788	-0.000664	2.236838
-88.600670	-1.814683	2.246835
-87.602782	0.108008	2.256832
-87.613554	0.283964	2.266829
-87.406992	0.058629	2.276826
-86.753800	3.419270	2.286822
-86.076756	1.755406	2.296819
-85.741412	0.458346	2.306816
-85.174164	2.866223	2.316813
-84.705252	0.145079	2.326810
-83.847853	4.937399	2.336806
-83.801028	0.577756	2.346803
-83.231713	4.223878	2.356800
-82.380747	4.310010	2.366797
-82.099305	3.170224	2.376794
-81.764401	0.621994	2.386790
-80.818121	-5.258806	2.396787
-80.638995	2.220788	2.406784
-80.522648	-5.640474	2.416781
-79.546726	0.194567	2.426778
-79.219090	-1.962904	2.436774
-78.432400	-4.971102	2.446771
-77.951582	-3.161133	2.456768
-77.815147	-13.879609	2.466765
-76.982904	-12.330258	2.476762
-76.528655	-0.268674	2.486758
-76.083002	-6.613202	2.496755
-75.656413	-0.350519	2.506752
-75.013670	3.829014	2.516749
-74.753606	-0.215384	2.526746
-73.945161	-0.800518	2.536742
-73.517890	-5.327097	2.546739
-73.598626	2.234139	2.556736
-72.417192	-0.968564	2.566733
-72.194379	-0.204942	2.576730
-71.120081	4.559943	2.586726
-70.793737	-0.562287	2.596723
-71.013948	3.273286	2.606720
-70.480941	3.475445	2.616717
-69.711526	3.346201	2.626714
-68.936084	2.965770	2.636710
-68.174572	-4.292717	2.646707
-67.888465	-4.425903	2.656704
-68.067684	-1.509008	2.666701
-67.222927	-0.024958	2.676698
-66.695285	0.418782	2.686694
-65.686069	0.074810	2.696691
-65.097929	1.139501	2.706688
-65.158493	-3.124230	2.716685
-64.985055	2.892778	2.726682
-63.923103	0.044454	2.736678
-63.589307	2.992343	2.746675
-63.408033	5.780254	2.756672
-62.476405	-3.215276	2.766669
-61.910981	-5.815235	2.776666
-61.702451	3.376672	2.786662
-61.387776	0.175880	2.796659
-60.299310	-2.467505	2.806656
-59.571391	-5.102267	2.816653
-59.488306	3.181038	2.826650
-59.200769	-8.150161	2.836646
-58.700125	3.435386	2.846643
-58.298186	1.164979	2.856640
-57.428607	2.638831	2.866637
-56.851180	1.158365	2.876634
-56.425262	-5.091228	2.886630
-56.311896	2.902270	2.896627
-55.068378	3.795230	2.906624
-55.372547	0.272656	2.916621
-54.850837	1.705639	2.926618
-54.036518	-3.166296	2.936614
-53.672474	-8.129675	2.946611
-52.641572	-0.231522	2.956608
-52.092099	-4.545886	2.966605
-52.268805	0.607008	2.976602
-51.936322	-0.642090	2.986598
-50.909884	-5.030718	2.996595
-50.753310	-9.445460	3.006592
-49.885050	-7.410722	3.016589
-49.486093	-8.397749	3.026586
-49.033366	-7.530545	3.036582
-48.457253	-6.334107	3.046579
-48.123481	-10.792276	3.056576
-47.898416	-5.895168	3.066573
-46.753388	-10.615860	3.076570
-46.792891	-6.178053	3.086566
-45.773149	-6.558508	3.096563
-45.167898	-5.702381	3.106560
-45.155213	-8.257459	3.116557
-44.622848	-13.063318	3.126554
-43.958195	-1.230887	3.136550
-43.770149	-6.588167	3.146547
-42.498659	-4.204411	3.156544
-42.277950	-9.674477	3.166541
-42.292480	-7.565644	3.176538
-41.757373	-6.685925	3.186534
-40.785957	-7.530841	3.196531
-40.607264	-2.968622	3.206528
-39.978143	-11.853694	3.216525
-39.422523	-6.510725	3.226522
-39.126420	-4.884230	3.236518
-38.450065	-7.837236	3.246515
-37.871362	-7.467968	3.256512
-37.746560	-3.445368	3.266509
-36.788675	-7.433695	3.276506
-36.125257	-7.663640	3.286502
-36.064236	-9.288607	3.296499
-35.684732	-2.844368	3.306496
-34.411151	-6.039243	3.316493
-34.471851	-2.757510	3.326490
-34.243734	-10.370089	3.336486
-33.590736	-3.040299	3.346483
-33.036744	-1.913272	3.356480
-32.426555	-3.988029	3.366477
-31.577792	-7.842161	3.376474
-31.415095	-8.811409	3.386470
-31.427972	-11.726791	3.396467
-30.717824	-6.487073	3.406464
-30.074018	-7.993711	3.416461
-28.967424	1.083712	3.426458
-28.696828	0.553812	3.436454
-28.645795	0.675798	3.446451
-28.608869	-0.590637	3.456448
-27.495237	3.867197	3.466445
-27.115331	4.606362	3.476442
-26.550747	-4.043761	3.486438
-25.973703	-6.075344	3.496435
-25.113422	-3.519861	3.506432
-24.762953	-1.604068	3.516429
-24.678237	-3.201048	3.526426
-23.969108	-9.602437	3.536422
-23.162418	-4.963773	3.546419
-23.348877	-7.386479	3.556416
-22.193566	-4.705876	3.566413
-21.819387	-11.371883	3.576410
-21.608043	-4.929971	3.586406
-21.267195	-6.284906	3.596403
-20.383158	-4.645417	3.606400
-19.959192	-2.110695	3.616397
-19.050301	-6.617231	3.626394
-18.642706	-11.666583	3.636390
-18.740584	-8.911235	3.646387
-18.298958	-5.647526	3.656384
-17.332602	-16.301994	3.666381
-17.002511	-13.933216	3.676378
-15.973148	-8.996614	3.686374
-16.103570	-3.584839	3.696371
-15.510559	-2.733141	3.706368
-14.992230	-15.988216	3.716365
-14.569523	-7.051396	3.726362
-13.632485	-5.157240	3.736358
-13.253912	-0.195334	3.746355
-12.877658	-4.324345	3.756352
-12.899927	-5.834978	3.766349
-11.650068	-2.259967	3.776346
-11.457549	-9.204958	3.786342
-11.032307	-2.102623	3.796339
-10.156665	-5.463613	3.806336
-9.971108	-1.485316	3.816333
-9.684834	-1.992315	3.826330
-8.665065	-2.676871	3.836326
-8.557053	-7.514860	3.846323
-7.880607	-7.433231	3.856320
-7.225971	-18.004319	3.866317
-7.009874	-15.887047	3.876314
-6.635867	-12.707842	3.886310
-5.722774	-3.825197	3.896307
-5.534942	3.763918	3.906304
-5.179267	13.360563	3.916301
-4.611474	9.578683	3.926298
-4.320085	22.026765	3.936294
-4.016430	30.111024	3.946291
-3.061508	39.893141	3.956288
-2.996941	54.369046	3.966285
-2.240220	68.797383	3.976282
-1.740316	80.234220	3.986278
-1.520436	94.537093	3.996275
-0.894857	112.730119	4.006272
0.000000	112.732598	4.011277
-0.493663	122.034731	4.016282
-0.144506	118.550985	4.021286
0.001314	139.256648	4.026291
0.024163	150.275340	4.031296
0.409710	151.794011	4.036301
0.578964	154.776337	4.041306
0.671176	149.848829	4.046310
0.133687	155.089324	4.051315
0.595613	146.772908	4.056320
0.400211	146.240227	4.061325
0.076653	149.387864	4.066330
0.071587	146.595161	4.071334
0.341626	154.139624	4.076339
0.487211	156.246136	4.081344
0.309582	148.880323	4.086349
0.301587	156.018836	4.091354
0.415576	142.890870	4.096358
0.162671	151.298179	4.101363
0.410235	145.938370	4.106368
0.919882	156.821164	4.111373
0.435026	159.218817	4.116378
0.728905	151.010819	4.121382
0.820295	149.870352	4.126387
0.439633	159.442805	4.131392
0.787393	148.685991	4.136397
0.187721	149.725323	4.141402
0.644964	146.275361	4.146406
0.541954	153.808307	4.151411
0.821091	146.586508	4.156416
0.718517	151.104408	4.161421
0.408354	145.888382	4.166426
0.629362	146.714517	4.171430
0.471556	156.271253	4.176435
0.654885	169.457394	4.181440
0.794193	177.904887	4.186445
0.881880	173.243826	4.191450
1.357920	167.987639	4.196454
0.767158	160.847492	4.201459
1.019839	154.041087	4.206464
0.856050	151.564153	4.211469
0.842265	158.494766	4.216474
0.730560	153.845772	4.221478
0.625439	153.172487	4.226483
0.402979	154.684585	4.231488
0.661883	159.430937	4.236493
0.903805	168.355981	4.241498
1.324104	169.587676	4.246502
1.012782	161.973762	4.251507
0.752627	157.879376	4.256512
0.506458	145.955896	4.261517
0.495246	162.525811	4.266522
1.111932	161.180173	4.271526
1.096982	168.512758	4.276531
1.037165	176.655904	4.281536
1.355843	173.493260	4.286541
0.939445	177.395656	4.291546
1.170878	166.372213	4.296550
1.035350	169.085628	4.301555
0.917499	165.586001	4.306560
1.009220	173.427148	4.311565
0.962923	172.741540	4.316570
1.425447	174.162809	4.321574
1.123833	173.488480	4.326579
1.265815	168.660782	4.331584
1.027905	165.502542	4.336589
0.909201	163.923398	4.341594
0.855494	163.915969	4.346598
0.977312	173.916383	4.351603
0.984713	181.546042	4.356608
1.414394	186.727708	4.361613
1.173876	181.285698	4.366618
0.803086	181.397239	4.371622
0.847550	182.184427	4.376627
0.538069	180.530583	4.381632
1.070685	178.261585	4.386637
0.657849	184.039487	4.391642
1.265836	191.736989	4.396646
1.165666	195.944486	4.401651
1.361166	200.004711	4.406656
1.363813	200.001163	4.411661
1.177466	209.211202	4.416666
1.235022	204.599115	4.421670
1.287282	202.436541	4.426675
1.378101	201.580890	4.431680
1.664483	207.085423	4.436685
1.399544	210.413765	4.441690
1.810435	200.893581	4.446694
1.392089	195.618455	4.451699
1.246889	187.247855	4.456704
1.096023	186.350743	4.461709
1.146352	194.049651	4.466714
1.669058	206.888759	4.471718
1.260417	209.204951	4.476723
1.650181	216.009482	4.481728
1.966098	204.871623	4.486733
1.438685	197.237555	4.491738
1.716745	193.888247	4.496742
1.480956	196.557166	4.501747
1.318792	203.042674	4.506752
1.590183	196.530725	4.511757
1.374972	203.043474	4.516762
1.397668	203.868853	4.521766
1.462221	204.118252	4.526771
1.764276	203.561899	4.531776
2.061723	202.152070	4.536781
1.654706	210.431545	4.541786
1.842907	199.734344	4.546790
1.437408	195.121591	4.551795
1.590390	198.508245	4.556800
1.616412	204.464592	4.561805
1.789678	211.211082	4.566810
2.149889	208.981578	4.571814
1.726521	198.964877	4.576819
1.400354	197.253520	4.581824
2.031814	189.723754	4.586829
1.570938	193.009834	4.591834
1.749791	193.080090	4.596838
1.554274	203.275457	4.601843
1.942144	214.297466	4.606848
2.227829	204.268440	4.611853
1.705301	201.863172	4.616858
1.632836	189.659523	4.621862
1.680351	190.344998	4.626867
1.855503	201.675359	4.631872
1.836388	202.766669	4.636877
1.604380	210.088774	4.641882
1.705652	211.683347	4.646886
1.718566	211.716165	4.651891
1.674017	209.891359	4.656896
2.032354	215.267635	4.661901
1.818099	210.653574	4.666906
1.750836	210.974116	4.671910
1.478473	222.507041	4.676915
1.572417	219.474289	4.681920
1.846646	210.715679	4.686925
1.566471	218.159180	4.691930
1.926314	223.095472	4.696934
2.232072	231.634131	4.701939
2.087274	240.027814	4.706944
2.275634	232.870733	4.711949
1.914869	227.928310	4.716954
2.183494	229.522139	4.721958
2.291859	230.432254	4.726963
2.492541	228.202277	4.731968
2.327312	220.673156	4.736973
2.164427	225.171991	4.741978
1.906620	210.807917	4.746982
2.193714	215.746042	4.751987
2.065676	223.833395	4.756992
2.006748	218.198589	4.761997
1.859533	218.569542	4.767002
2.193280	227.913745	4.772006
2.255718	226.394974	4.777011
2.237303	239.372139	4.782016
2.280179	237.764667	4.787021
2.220325	236.122570	4.792026
2.449710	233.913433	4.797030
1.907876	225.977884	4.802035
2.121186	232.990224	4.807040
2.604299	233.307330	4.812045
2.473904	237.538525	4.817050
2.174838	233.693784	4.822054
2.056636	236.037524	4.827059
2.134357	238.021736	4.832064
2.500698	228.891279	4.837069
2.022277	234.910358	4.842074
2.257004	237.230786	4.847078
2.649949	238.748312	4.852083
2.388894	233.878947	4.857088
2.397463	244.314639	4.862093
2.339911	239.568608	4.867098
2.637423	240.816262	4.872102
2.475317	240.756110	4.877107
2.191839	234.662725	4.882112
2.511592	237.067988	4.887117
2.368943	234.521314	4.892122
2.385833	233.458878	4.897126
2.531488	240.358371	4.902131
2.637873	239.228218	4.907136
2.721252	229.467952	4.912141
2.256393	231.289874	4.917146
2.748450	231.507514	4.922150
2.370445	238.757451	4.927155
2.626268	236.813110	4.932160
2.808006	236.044540	4.937165
2.641929	236.855019	4.942170
2.800833	230.756032	4.947174
2.758586	238.469374	4.952179
2.883778	229.082240	4.957184
2.578734	235.264146	4.962189
2.601538	242.514955	4.967194
2.750380	233.826475	4.972198
2.612737	234.338304	4.977203
2.634855	244.888943	4.982208
2.866915	234.545553	4.987213
2.615508	245.091324	4.992218
2.503879	240.932667	4.997222
2.399097	237.649285	5.002227
2.392396	245.198911	5.007232
2.730580	239.242847	5.012237
2.520142	240.705625	5.017242
2.852525	247.209061	5.022246
3.160942	261.574833	5.027251
2.860716	252.548146	5.032256
2.816274	240.438173	5.037261
2.890196	252.594231	5.042266
2.916948	250.448277	5.047270
2.902910	245.673324	5.052275
2.692053	257.187204	5.057280
3.289378	256.651314	5.062285
2.973294	255.767267	5.067290
2.944000	236.720135	5.072294
2.981672	241.447171	5.077299
2.746924	253.603833	5.082304
2.980102	250.881586	5.087309
2.846446	264.632833	5.092314
2.908268	269.058729	5.097318
3.219977	255.842949	5.102323
3.117607	256.735258	5.107328
3.400576	252.999204	5.112333
2.876200	262.426412	5.117338
3.300518	257.342765	5.122342
3.383174	245.171872	5.127347
3.061752	249.394847	5.132352
2.838827	235.762460	5.137357
2.646403	256.267828	5.142362
3.062683	257.186950	5.147366
3.561719	260.592502	5.152371
2.988951	258.805640	5.157376
3.377786	250.975110	5.162381
3.052493	264.009563	5.167386
3.309749	259.201857	5.172390
2.761607	259.590943	5.177395
2.626476	265.578729	5.182400
3.203114	255.630921	5.187405
3.003677	261.448388	5.192410
3.195330	263.993820	5.197414
2.956486	263.126220	5.202419
2.786937	264.452922	5.207424
3.440439	257.416396	5.212429
3.417269	269.404088	5.217434
3.426762	266.634409	5.222438
3.425193	254.919540	5.227443
2.982669	253.852703	5.232448
3.371870	256.003552	5.237453
3.251103	269.262424	5.242458
3.400934	277.667199	5.247462
3.541489	277.411230	5.252467
3.683431	272.023536	5.257472
3.480935	261.029632	5.262477
3.034344	260.811297	5.267482
3.557618	265.880340	5.272486
3.321697	254.882152	5.277491
3.558433	269.043960	5.282496
3.370675	279.573514	5.287501
3.701926	288.772607	5.292506
3.745473	268.252473	5.297510
3.347395	267.216680	5.302515
3.375408	275.621437	5.307520
3.614819	276.504824	5.312525
3.629854	283.652457	5.317530
3.558373	285.122077	5.322534
3.575208	277.953720	5.327539
3.356287	288.453330	5.332544
3.499075	289.089175	5.337549
3.378320	290.322863	5.342554
3.460771	299.348731	5.347558
3.621411	290.421110	5.352563
3.251225	288.887436	5.357568
3.776259	283.797591	5.362573
3.684645	288.889612	5.367578
3.712437	293.665655	5.372582
3.920491	282.051006	5.377587
3.355561	284.514925	5.382592
3.814081	281.311507	5.387597
3.606146	293.410239	5.392602
3.386744	286.658303	5.397606
3.853380	283.937666	5.402611
3.528740	287.094986	5.407616
4.001853	287.277611	5.412621
3.338430	286.801976	5.417626
3.930847	282.157212	5.422630
4.220530	287.923843	5.427635
3.578967	284.442458	5.432640
3.981865	288.558996	5.437645
3.853362	303.359818	5.442650
3.679956	296.755737	5.447654
3.991699	284.115723	5.452659
3.810820	292.242971	5.457664
3.814269	294.918948	5.462669
3.872854	302.391996	5.467674
3.988271	313.200227	5.472678
4.117460	309.320429	5.477683
4.067396	315.310806	5.482688
4.288369	305.930865	5.487693
4.102211	298.686538	5.492698
3.973594	287.573549	5.497702
4.027918	287.498681	5.502707
3.361039	292.648632	5.507712
3.980713	307.630356	5.512717
4.040399	311.616842	5.517722
4.655990	312.055690	5.522726
4.339415	302.721480	5.527731
3.783396	292.503921	5.532736
3.837524	298.604618	5.537741
4.014027	305.094380	5.542746
4.480689	314.968417	5.547750
4.634936	311.328322	5.552755
3.834150	315.581656	5.557760
4.101619	307.921855	5.562765
3.954868	318.290026	5.567770
4.016254	313.092030	5.572774
4.326868	319.851977	5.577779
4.312090	319.126655	5.582784
4.247844	314.482885	5.587789
4.144556	316.995153	5.592794
3.864424	313.419525	5.597798
3.991050	317.664504	5.602803
4.018953	319.004760	5.607808
4.215983	311.868443	5.612813
3.986107	322.205267	5.617818
4.012354	311.855912	5.622822
4.098451	311.877336	5.627827
4.050607	322.856522	5.632832
4.577654	329.386626	5.637837
4.692402	340.460729	5.642842
4.563741	330.505635	5.647846
4.262231	323.184347	5.652851
4.238841	321.254996	5.657856
4.341044	328.063214	5.662861
4.770920	335.867602	5.667866
4.462945	324.763533	5.672870
4.275887	326.175222	5.677875
4.462400	327.645805	5.682880
4.683617	325.064612	5.687885
4.413422	322.825680	5.692890
4.712496	320.526589	5.697894
4.341078	313.523068	5.702899
4.470274	318.416206	5.707904
4.549450	323.706268	5.712909
4.533713	342.042400	5.717914
4.938204	337.619867	5.722918
4.740380	329.279539	5.727923
4.298447	325.308328	5.732928
4.267237	327.233582	5.737933
4.494075	335.265732	5.742938
4.774890	335.199892	5.747942
4.706212	334.919553	5.752947
4.713611	344.267172	5.757952
4.930709	327.424647	5.762957
5.021141	335.490690	5.767962
5.040598	323.079651	5.772966
4.967361	323.344178	5.777971
4.734485	316.110282	5.782976
4.917487	317.745923	5.787981
4.877526	319.172674	5.792986
4.759501	314.730262	5.797990
4.606145	319.452261	5.802995
4.619296	324.581763	5.808000
4.835460	314.535025	5.813005
4.610258	314.022797	5.818010
4.619184	314.530790	5.823014
4.741282	327.619017	5.828019
4.884891	325.113181	5.833024
4.885756	316.030092	5.838029
4.853710	307.198900	5.843034
4.549944	319.388499	5.848038
5.106819	327.764722	5.853043
4.843587	341.169213	5.858048
5.494844	329.210286	5.863053
4.542686	330.848665	5.868058
5.140480	332.169793	5.873062
4.851479	327.257298	5.878067
4.987714	328.571196	5.883072
5.021142	324.861326	5.888077
5.011350	336.663486	5.893082
5.048655	325.841009	5.898086
5.122245	337.161960	5.903091
4.721561	338.119701	5.908096
5.011808	336.976734	5.913101
4.984524	335.120753	5.918106
5.040608	339.240681	5.923110
4.898263	341.224368	5.928115
4.925289	338.103940	5.933120
5.152520	337.208062	5.938125
5.110639	342.260718	5.943130
4.965856	346.551125	5.948134
4.971708	339.064919	5.953139
4.840034	343.277355	5.958144
5.317924	342.484817	5.963149
5.336955	340.567841	5.968154
5.219198	341.804229	5.973158
5.313486	351.157306	5.978163
5.001664	344.530467	5.983168
5.186182	334.776542	5.988173
4.903660	341.119490	5.993178
4.875408	343.129705	5.998182
5.083328	338.000635	6.003187
5.100282	352.237856	6.008192
5.341003	361.005000	6.013197
5.316148	375.505009	6.018202
5.359744	367.101766	6.023206
5.705811	367.032095	6.028211
4.917603	363.905716	6.033216
5.246871	360.361745	6.038221
5.338692	372.078506	6.043226
5.322836	378.436896	6.048230
5.350910	368.504833	6.053235
5.114218	371.901572	6.058240
5.284150	362.178377	6.063245
5.201601	372.925719	6.068250
5.595877	373.721725	6.073254
5.446799	366.886044	6.078259
5.063253	361.637087	6.083264
5.686012	355.889774	6.088269
5.486641	358.783998	6.093274
5.374832	354.122312	6.098278
5.500777	347.303928	6.103283
5.104036	357.302927	6.108288
5.348654	348.634280	6.113293
4.739385	350.197128	6.118298
5.358690	358.639575	6.123302
5.515953	362.898777	6.128307
5.320085	348.714769	6.133312
5.331228	344.147837	6.138317
5.100973	349.239314	6.143322
4.992824	347.759748	6.148326
5.615438	361.801440	6.153331
5.295794	369.529555	6.158336
5.444561	359.066185	6.163341
5.031822	353.919851	6.168346
5.235556	363.591247	6.173350
5.404766	370.097987	6.178355
5.446426	373.280547	6.183360
5.621866	358.542018	6.188365
5.306610	348.495745	6.193370
5.379665	343.314905	6.198374
5.477973	341.629192	6.203379
5.192454	346.678654	6.208384
5.363649	346.430568	6.213389
5.575909	346.549406	6.218394
5.000197	352.567854	6.223398
5.128118	351.652636	6.228403
5.006955	349.630939	6.233408
5.461965	344.241936	6.238413
4.997828	348.249877	6.243418
5.172827	349.605198	6.248422
5.380410	359.937207	6.253427
5.532725	360.805685	6.258432
5.354689	350.171743	6.263437
5.214734	347.162733	6.268442
5.211645	347.058839	6.273446
5.310269	343.452707	6.278451
5.189640	357.932814	6.283456
5.475079	362.763673	6.288461
5.207132	355.813627	6.293466
5.164678	360.727174	6.298470
5.269699	371.113123	6.303475
5.310513	368.487245	6.308480
5.630655	362.625697	6.313485
5.001970	355.662216	6.318490
5.326843	363.479801	6.323494
5.561337	361.560914	6.328499
5.027429	360.682302	6.333504
5.479076	366.948917	6.338509
5.502422	352.117016	6.343514
5.147134	350.138099	6.348518
5.349618	350.951310	6.353523
5.004363	350.976619	6.358528
5.188299	361.672974	6.363533
5.561541	365.968151	6.368538
5.497428	359.555835	6.373542
5.058195	356.612402	6.378547
5.349691	364.112486	6.383552
5.579324	365.487775	6.388557
5.197676	356.011811	6.393562
5.166171	352.742309	6.398566
5.154748	365.876662	6.403571
5.252042	373.932163	6.408576
5.394058	365.184571	6.413581
5.586090	369.333959	6.418586
5.734614	350.357094	6.423590
5.361481	352.351406	6.428595
5.334418	349.410238	6.433600
5.624181	346.451379	6.438605
5.528566	350.759441	6.443610
5.528713	346.969328	6.448614
5.684800	346.293331	6.453619
5.261931	348.333350	6.458624
5.416618	345.958661	6.463629
5.448954	339.717994	6.468634
5.247174	356.001390	6.473638
5.730175	350.560572	6.478643
5.510917	350.373278	6.483648
5.040690	348.345819	6.488653
5.448867	348.339242	6.493658
5.257691	346.413866	6.498662
5.387942	349.411788	6.503667
5.144705	357.112183	6.508672
5.239650	354.651884	6.513677
5.192399	349.657450	6.518682
4.747068	345.411521	6.523686
5.356844	348.913742	6.528691
5.019801	358.656677	6.533696
5.109442	352.233080	6.538701
4.987053	350.303321	6.543706
5.107716	352.119511	6.548710
5.257632	345.787770	6.553715
4.958278	351.079829	6.558720
5.219821	348.631557	6.563725
5.114980	346.534553	6.568730
5.525879	346.227001	6.573734
5.345535	347.068180	6.578739
5.276792	353.131079	6.583744
5.145652	357.561731	6.588749
5.332526	353.812145	6.593754
5.184963	354.445744	6.598758
5.433999	345.298691	6.603763
5.364555	348.264431	6.608768
5.254727	351.426282	6.613773
5.094972	354.159315	6.618778
5.469398	361.228877	6.623782
5.707366	360.717299	6.628787
5.489416	349.985169	6.633792
5.569694	349.858805	6.638797
5.554833	343.941855	6.643802
5.415326	353.748943	6.648806
5.418042	343.963209	6.653811
5.326245	344.278081	6.658816
5.171397	347.696874	6.663821
5.483016	358.667571	6.668826
5.389946	348.241861	6.673830
5.347974	347.049380	6.678835
5.106179	350.364652	6.683840
5.212691	356.482522	6.688845
5.262283	350.229674	6.693850
5.422040	352.713647	6.698854
5.515284	344.441888	6.703859
5.293740	356.539617	6.708864
5.220507	352.083895	6.713869
5.047014	350.579702	6.718874
5.180480	346.503080	6.723878
5.177131	355.061452	6.728883
5.404638	351.258085	6.733888
5.342985	342.285955	6.738893
5.103026	347.072064	6.743898
4.949591	351.737136	6.748902
5.833918	353.415445	6.753907
5.222094	345.728017	6.758912
5.342971	346.259710	6.763917
5.295999	345.852606	6.768922
5.093105	349.364299	6.773926
5.332094	347.881304	6.778931
4.999462	344.304353	6.783936
5.145941	341.630391	6.788941
4.944187	340.076816	6.793946
5.171769	346.194814	6.798950
5.523707	339.524742	6.803955
5.244430	352.235725	6.808960
4.923854	339.330296	6.813965
5.176669	355.410038	6.818970
5.051619	365.230700	6.823974
5.635134	368.328894	6.828979
5.458336	366.363313	6.833984
5.556902	371.874994	6.838989
5.187165	361.935271	6.843994
5.047395	356.626214	6.848998
5.337543	358.681769	6.854003
5.308395	365.481978	6.859008
5.574197	363.301956	6.864013
5.136996	361.221897	6.869018
5.337341	359.457021	6.874022
5.281477	359.905502	6.879027
4.764506	368.654579	6.884032
5.317201	364.392460	6.889037
5.509974	364.485859	6.894042
5.489988	374.818507	6.899046
5.716761	364.770090	6.904051
5.287143	358.237515	6.909056
4.966813	352.554781	6.914061
4.862627	360.505606	6.919066
4.819457	362.350470	6.924070
5.765099	362.253884	6.929075
5.586581	374.654970	6.934080
5.180463	371.051491	6.939085
5.281513	369.881032	6.944090
5.645316	366.695510	6.949094
5.480539	365.329161	6.954099
5.229031	359.999537	6.959104
5.673953	358.930561	6.964109
5.219186	347.412740	6.969114
4.795070	345.520469	6.974118
5.340262	353.262619	6.979123
5.095428	373.156195	6.984128
5.437764	367.262716	6.989133
5.218493	368.173231	6.994138
5.657452	370.031613	6.999142
5.588066	364.952038	7.004147
5.288702	360.835237	7.009152
5.147130	361.486885	7.014157
5.111447	357.787768	7.019162
4.933628	368.363283	7.024166
5.300132	364.060551	7.029171
5.157514	379.018654	7.034176
5.496409	372.508786	7.039181
5.581161	372.862609	7.044186
5.390216	377.761316	7.049190
5.508788	367.688615	7.054195
4.906255	370.778487	7.059200
5.287997	370.927884	7.064205
5.513534	372.778367	7.069210
5.296755	371.489717	7.074214
5.563874	369.461346	7.079219
5.264437	357.349868	7.084224
4.917540	351.658616	7.089229
5.221057	359.118863	7.094234
5.223336	371.207064	7.099238
5.546312	367.819093	7.104243
5.209045	373.939626	7.109248
5.432336	372.781771	7.114253
5.601494	369.749939	7.119258
5.336589	350.286958	7.124262
5.441772	348.777341	7.129267
5.114291	356.111207	7.134272
5.110983	352.802514	7.139277
5.211567	361.563003	7.144282
5.191352	368.497862	7.149286
5.465002	365.193501	7.154291
4.857955	382.239199	7.159296
5.173425	366.434836	7.164301
5.152678	369.933992	7.169306
4.964970	378.644464	7.174310
5.261208	369.376156	7.179315
5.334834	362.841155	7.184320
5.623683	366.636952	7.189325
5.732389	369.438919	7.194330
5.095335	366.143475	7.199334
5.379121	367.421749	7.204339
5.254236	376.271133	7.209344
5.407212	375.389978	7.214349
5.571326	377.946041	7.219354
5.376212	372.968295	7.224358
5.571317	372.899982	7.229363
5.268505	358.109367	7.234368
5.157316	346.636128	7.239373
5.192314	353.714243	7.244378
5.007373	365.464599	7.249382
5.320182	368.696690	7.254387
5.195170	373.942629	7.259392
5.268949	367.527823	7.264397
5.703439	362.467872	7.269402
5.479907	368.684588	7.274406
5.267936	361.422109	7.279411
5.461113	363.280793	7.284416
4.977551	349.353546	7.289421
5.340249	362.948496	7.294426
5.254531	363.746470	7.299430
5.221843	370.556723	7.304435
5.244630	373.128463	7.309440
5.465484	378.345863	7.314445
5.613960	374.893312	7.319450
5.054948	373.009386	7.324454
5.617665	372.061272	7.329459
5.267591	365.010116	7.334464
4.839900	366.838919	7.339469
5.197647	357.336418	7.344474
5.275667	365.796706	7.349478
5.734195	374.586891	7.354483
5.389595	372.872059	7.359488
5.287300	360.112961	7.364493
5.171621	363.193468	7.369498
5.046138	363.165578	7.374502
4.974079	365.790048	7.379507
5.073576	368.368825	7.384512
5.332936	375.642967	7.389517
5.470552	371.195540	7.394522
4.961319	372.182838	7.399526
5.311111	370.233343	7.404531
5.115414	371.137024	7.409536
5.315195	370.501679	7.414541
5.519797	366.651255	7.419546
5.426096	367.988302	7.424550
5.527970	371.813211	7.429555
5.576986	377.854620	7.434560
5.571937	369.455786	7.439565
5.583648	366.752184	7.444570
5.124059	359.733900	7.449574
5.398541	351.550976	7.454579
5.106815	358.515450	7.459584
5.339834	373.687142	7.464589
5.180395	365.717302	7.469594
5.458612	366.563015	7.474598
5.883968	369.271389	7.479603
5.333298	367.202669	7.484608
5.417504	361.577169	7.489613
5.162434	349.658101	7.494618
5.031187	353.231405	7.499622
5.604005	347.937952	7.504627
5.659059	348.761463	7.509632
5.433030	346.686492	7.514637
5.117224	351.883038	7.519642
5.145390	355.697274	7.524646
5.425164	358.143579	7.529651
5.067801	350.884759	7.534656
5.192578	351.972657	7.539661
5.471907	350.167010	7.544666
5.380732	354.809735	7.549670
5.138731	355.752262	7.554675
5.129048	360.050111	7.559680
5.096378	350.538798	7.564685
5.147455	349.028114	7.569690
5.457821	361.005066	7.574694
5.271203	354.893395	7.579699
5.194632	353.041922	7.584704
4.911143	357.461494	7.589709
5.222885	370.969472	7.594714
5.131850	372.546547	7.599718
5.522792	373.153249	7.604723
5.450795	381.225620	7.609728
5.384948	377.638761	7.614733
5.273618	385.521108	7.619738
5.620614	379.307365	7.624742
5.253252	366.760372	7.629747
5.295377	357.870152	7.634752
4.831772	355.028588	7.639757
5.296483	362.808582	7.644762
5.582377	380.227771	7.649766
5.829145	372.618621	7.654771
5.322620	356.401254	7.659776
5.404832	352.193408	7.664781
5.392000	350.360485	7.669786
5.014165	353.617847	7.674790
5.181091	353.335625	7.679795
5.039223	351.794871	7.684800
5.203556	366.983579	7.689805
5.616940	370.921336	7.694810
5.175671	365.190991	7.699814
5.010880	354.425272	7.704819
5.577749	377.099919	7.709824
5.054148	375.109240	7.714829
5.192920	380.991145	7.719834
5.283133	384.995040	7.724838
5.668993	381.195485	7.729843
5.335066	387.062405	7.734848
5.360299	376.814409	7.739853
5.270519	360.237929	7.744858
4.942348	366.809453	7.749862
5.176423	371.297140	7.754867
5.371309	381.523572	7.759872
5.328991	378.663867	7.764877
5.498061	376.878549	7.769882
5.367145	385.577019	7.774886
5.609920	376.522672	7.779891
5.181947	365.199982	7.784896
4.825645	360.535234	7.789901
5.310116	372.080131	7.794906
5.193707	380.475787	7.799910
5.799002	377.515252	7.804915
5.563023	377.124920	7.809920
5.297730	360.366961	7.814925
5.515690	354.872496	7.819930
5.050094	357.941046	7.824934
5.087464	353.202351	7.829939
5.299659	365.450851	7.834944
5.314699	374.088626	7.839949
5.452263	360.317760	7.844954
5.154884	364.018170	7.849958
5.551882	362.156238	7.854963
5.156173	351.233488	7.859968
5.437525	349.237704	7.864973
5.753696	360.960656	7.869978
5.213440	351.778304	7.874982
5.609177	350.081082	7.879987
5.224089	358.844422	7.884992
5.001988	349.343621	7.889997
5.462245	342.890797	7.895002
4.900050	357.230848	7.900006
5.383310	349.556413	7.905011
5.608500	354.671893	7.910016
5.355723	356.166582	7.915021
5.703970	356.235774	7.920026
5.275487	361.576414	7.925030
5.450763	351.665734	7.930035
5.266521	352.801745	7.935040
4.817640	358.012685	7.940045
5.211520	355.312856	7.945050
5.350156	356.540963	7.950054
5.467064	346.367294	7.955059
5.300570	358.507074	7.960064
5.510647	350.992229	7.965069
5.528632	350.312424	7.970074
5.250081	357.926569	7.975078
5.246130	354.402844	7.980083
5.153369	354.502735	7.985088
5.021649	351.524078	7.990093
5.022070	354.042350	7.995098
4.995272	356.786320	8.000102
4.955081	349.459136	8.005107
5.492794	363.159712	8.010112
4.995451	367.205054	8.015130
5.070962	381.333743	8.020147
5.208008	379.901862	8.025165
5.660468	377.095505	8.030182
5.683495	379.493389	8.035200
5.416152	375.498979	8.040218
5.524278	360.947305	8.045235
5.092830	361.569900	8.050253
5.365846	353.871848	8.055270
5.180559	368.937333	8.060288
5.308356	371.255791	8.065306
5.506318	379.013114	8.070323
5.381026	377.751460	8.075341
5.403624	375.236081	8.080358
5.105209	367.128402	8.085376
5.282997	380.821466	8.090394
5.616476	377.020673	8.095411
5.302203	380.963692	8.100429
5.357891	380.879314	8.105446
5.417112	372.444565	8.110464
5.234045	376.231462	8.115482
5.720457	369.853947	8.120499
5.538909	370.816311	8.125517
5.467618	370.556054	8.130534
5.376524	363.523727	8.135552
5.269008	373.944632	8.140570
5.557442	384.783554	8.145587
5.226603	381.890880	8.150605
5.654506	374.765119	8.155622
5.381865	373.245556	8.160640
5.351540	371.631463	8.165658
5.659996	378.547960	8.170675
5.538948	380.980900	8.175693
5.619621	374.527707	8.180710
5.369187	363.219054	8.185728
5.135349	372.365815	8.190746
5.475557	378.617841	8.195763
4.974540	379.235490	8.200781
5.608747	383.977526	8.205798
5.913488	372.036503	8.210816
5.744566	379.592186	8.215834
5.871445	378.830884	8.220851
5.614232	372.316697	8.225869
5.516968	355.395566	8.230886
5.521319	350.260698	8.235904
5.224155	351.619738	8.240922
5.305214	355.722093	8.245939
5.872258	369.758465	8.250957
5.766755	371.665147	8.255974
5.478577	355.692030	8.260992
5.341958	357.205945	8.266010
5.907918	360.800483	8.271027
5.163851	367.038295	8.276045
5.674355	371.468246	8.281062
5.988221	375.259819	8.286080
5.616082	366.693428	8.291098
5.559008	359.160371	8.296115
5.229778	362.455653	8.301133
5.532440	370.913001	8.306150
5.450721	376.549101	8.311168
5.334101	383.591740	8.316186
5.953675	371.434449	8.321203
5.761588	384.711759	8.326221
5.809701	383.318970	8.331238
5.573319	376.820472	8.336256
5.512725	379.960329	8.341274
5.805312	375.014095	8.346291
5.653056	379.588260	8.351309
5.757709	383.311428	8.356326
5.814951	380.973681	8.361344
5.919254	380.906979	8.366362
5.516237	360.571711	8.371379
5.513660	368.439143	8.376397
5.339785	364.742591	8.381414
5.660024	370.322417	8.386432
5.393553	377.621902	8.391450
5.879896	366.040751	8.396467
5.536936	380.550158	8.401485
5.659915	378.826993	8.406502
5.833735	376.303847	8.411520
5.746288	391.044865	8.416538
5.790340	376.613601	8.421555
5.819470	379.629041	8.426573
5.966634	381.259712	8.431590
6.153141	377.516513	8.436608
5.472504	366.325329	8.441626
5.757203	364.971441	8.446643
5.656814	378.237625	8.451661
5.595875	379.288502	8.456678
5.891938	376.153063	8.461696
5.616107	379.730353	8.466714
5.643442	381.635288	8.471731
5.345529	383.423613	8.476749
5.851601	382.398156	8.481766
5.963712	380.610414	8.486784
5.701307	386.189447	8.491802
5.815601	378.538186	8.496819
5.858820	380.308111	8.501837
6.069407	380.341619	8.506854
6.129240	391.844110	8.511872
6.267338	379.121183	8.516890
5.788653	366.702567	8.521907
5.618757	365.520438	8.526925
5.863356	372.765596	8.531942
5.887734	374.598410	8.536960
5.653506	371.059568	8.541978
6.200049	371.810746	8.546995
5.965588	380.064563	8.552013
5.950285	375.765837	8.557030
6.025748	376.312664	8.562048
5.473636	361.990011	8.567066
5.848542	374.936051	8.572083
5.877336	374.991553	8.577101
5.839906	380.320973	8.582119
6.071440	375.652473	8.587136
5.949641	380.013625	8.592154
5.792295	386.431479	8.597171
5.687106	383.008236	8.602189
5.781851	381.753346	8.607207
6.067800	375.763628	8.612224
5.819206	374.025737	8.617242
5.808188	378.041453	8.622259
5.668210	382.853537	8.627277
5.412882	384.751991	8.632295
5.839396	378.267041	8.637312
5.718088	383.997664	8.642330
5.913956	379.271604	8.647347
5.734744	388.599208	8.652365
5.476094	385.386041	8.657383
5.856498	393.320081	8.662400
5.788079	400.995818	8.667418
6.081023	400.678851	8.672435
6.276228	398.777190	8.677453
5.873135	402.102913	8.682471
6.356749	395.981432	8.687488
6.152243	396.906348	8.692506
6.171780	391.535587	8.697523
5.733250	389.647395	8.702541
5.488600	397.975386	8.707559
5.604656	401.333883	8.712576
5.713393	406.934028	8.717594
5.998217	403.409034	8.722611
5.781345	396.361565	8.727629
5.732408	406.110684	8.732647
5.918222	397.769816	8.737664
5.683895	405.329383	8.742682
5.862507	419.726057	8.747699
6.019601	417.527386	8.752717
6.073171	427.235311	8.757735
6.417057	426.774719	8.762752
6.615228	434.330073	8.767770
6.436971	416.310705	8.772787
6.231453	405.578825	8.777805
6.028239	406.910619	8.782823
6.122264	399.186769	8.787840
6.231951	411.438865	8.792858
6.204510	397.002938	8.797875
6.209154	396.626721	8.802893
6.256913	404.918656	8.807911
6.183053	403.598502	8.812928
6.269918	411.265845	8.817946
6.359090	401.280153	8.822963
6.431199	405.970863	8.827981
5.902194	404.636371	8.832999
6.208849	401.906357	8.838016
6.141724	402.718370	8.843034
6.432132	401.704400	8.848051
6.531644	402.458912	8.853069
5.999539	408.606935	8.858087
6.286411	400.130417	8.863104
6.339582	402.514145	8.868122
6.373891	405.860125	8.873139
6.652722	392.948027	8.878157
6.060812	402.431407	8.883175
6.396425	405.692607	8.888192
6.771632	404.147909	8.893210
6.641194	408.472545	8.898227
6.637957	396.500564	8.903245
6.106685	391.149294	8.908263
6.244790	386.318622	8.913280
6.271768	403.257094	8.918298
6.448870	391.821899	8.923315
6.035381	383.665860	8.928333
5.949995	395.992496	8.933351
6.299784	402.962525	8.938368
6.420992	401.148121	8.943386
6.636422	400.688595	8.948403
6.719986	394.225479	8.953421
6.450231	397.830227	8.958439
6.560920	381.574090	8.963456
6.494500	384.610719	8.968474
6.181400	391.122249	8.973491
6.690197	375.031340	8.978509
6.134282	389.258346	8.983527
6.173794	387.327281	8.988544
6.298512	379.775377	8.993562
6.174704	381.315700	8.998579
6.739775	382.628853	9.003597
6.246522	383.743885	9.008615
6.523113	383.218035	9.013632
6.069587	388.662732	9.018650
6.414757	390.978906	9.023667
6.355546	402.679809	9.028685
6.304932	397.402015	9.033703
6.684655	396.654992	9.038720
6.542538	399.331043	9.043738
6.062179	398.168849	9.048755
6.752626	396.881167	9.053773
6.478868	401.865555	9.058791
6.480391	397.472691	9.063808
6.529642	394.445101	9.068826
6.137927	403.013731	9.073843
6.306622	399.200722	9.078861
6.069561	405.173426	9.083879
6.279788	401.653736	9.088896
6.117594	403.875345	9.093914
6.087032	396.751533	9.098931
6.078130	400.596520	9.103949
6.131027	408.016699	9.108967
6.346319	421.726045	9.113984
6.661577	427.224617	9.119002
6.321898	424.910796	9.124019
6.805005	418.950325	9.129037
6.328453	425.989064	9.134055
6.412057	421.583414	9.139072
6.334874	432.892679	9.144090
6.399771	427.641071	9.149107
6.562105	429.925759	9.154125
6.306408	432.133529	9.159143
6.477700	431.248551	9.164160
6.546773	428.972069	9.169178
6.644365	434.422486	9.174195
6.982657	418.433821	9.179213
6.388282	424.724082	9.184231
7.182526	419.109624	9.189248
6.810235	428.154900	9.194266
6.821057	426.963564	9.199283
6.827308	419.524758	9.204301
6.389194	424.922887	9.209319
6.407539	420.868208	9.214336
6.660910	428.739996	9.219354
6.802768	428.373971	9.224371
6.810912	424.630133	9.229389
6.433148	424.105183	9.234407
6.395521	427.478146	9.239424
6.486244	423.153434	9.244442
6.396849	428.964306	9.249459
6.591465	429.309555	9.254477
6.185675	421.783430	9.259495
6.682000	427.004515	9.264512
6.665757	433.990522	9.269530
6.608249	444.851786	9.274547
6.983184	452.827728	9.279565
7.039732	439.909181	9.284583
7.146398	431.056783	9.289600
6.695223	432.225223	9.294618
6.434344	433.468172	9.299635
6.803090	428.172410	9.304653
6.639150	431.107471	9.309671
6.488013	435.580496	9.314688
6.947379	447.393183	9.319706
6.791872	444.788766	9.324723
7.230216	437.519351	9.329741
6.919417	443.487769	9.334759
6.747212	432.173203	9.339776
6.743074	435.253789	9.344794
6.859447	435.200986	9.349811
6.831102	432.620951	9.354829
6.706062	431.706375	9.359847
6.834734	423.942409	9.364864
6.741631	438.024815	9.369882
6.557168	454.431395	9.374899
6.996573	459.572993	9.379917
7.003968	457.113616	9.384935
7.140987	459.373848	9.389952
6.691257	445.467512	9.394970
6.542769	455.115399	9.399987
6.979326	443.724977	9.405005
7.066899	459.593769	9.410023
7.055680	459.522964	9.415040
7.056049	442.261516	9.420058
6.598258	442.982885	9.425075
7.083837	445.760019	9.430093
6.623626	449.183002	9.435111
6.901987	449.180714	9.440128
6.903576	454.699731	9.445146
6.960365	465.237113	9.450163
7.133178	446.563480	9.455181
6.913925	456.888228	9.460199
6.749342	455.336054	9.465216
6.938860	458.825129	9.470234
7.018946	459.532177	9.475251
7.261778	456.420791	9.480269
7.199398	463.773738	9.485287
7.137363	452.268445	9.490304
7.337326	448.759810	9.495322
6.853697	454.133478	9.500339
6.790313	449.173222	9.505357
6.875926	455.496471	9.510375
6.870176	459.236844	9.515392
7.064629	452.854267	9.520410
7.199509	449.131714	9.525427
7.027870	455.065848	9.530445
7.179344	457.270183	9.535463
7.169828	455.504527	9.540480
7.189900	458.041731	9.545498
7.037667	456.156291	9.550515
7.275030	455.434586	9.555533
7.337078	456.523121	9.560551
7.062268	453.564910	9.565568
7.376152	448.135680	9.570586
6.870819	451.603557	9.575603
7.001977	453.615405	9.580621
6.826356	452.339492	9.585639
6.901766	452.993622	9.590656
7.178733	448.939693	9.595674
6.951827	457.044054	9.600691
7.281403	442.672418	9.605709
7.232357	445.371853	9.610727
6.778166	453.211813	9.615744
7.074302	449.719761	9.620762
6.917993	457.055773	9.625779
7.112031	449.366821	9.630797
6.961857	454.477143	9.635815
7.036716	460.294008	9.640832
7.371149	450.528866	9.645850
6.902806	461.450949	9.650867
7.137384	468.864955	9.655885
7.374731	476.297468	9.660903
7.245220	479.836218	9.665920
7.467094	477.605364	9.670938
7.502688	477.098100	9.675955
7.065524	471.829978	9.680973
7.377600	466.596675	9.685991
7.507287	470.483213	9.691008
7.388574	452.426137	9.696026
7.210006	453.621559	9.701043
7.204166	453.480492	9.706061
7.576746	455.268568	9.711079
7.248471	451.517146	9.716096
7.532951	452.744609	9.721114
7.231049	459.513184	9.726131
7.471171	449.425071	9.731149
7.420132	456.965589	9.736167
7.282986	461.240792	9.741184
7.554458	456.424049	9.746202
7.479053	452.207242	9.751219
7.304797	454.184595	9.756237
7.900855	443.760214	9.761255
7.130492	462.820413	9.766272
7.645566	458.120368	9.771290
7.391930	452.997238	9.776307
7.642711	446.173569	9.781325
7.553532	456.254013	9.786343
7.289204	461.612472	9.791360
7.712063	457.314931	9.796378
7.646076	455.851543	9.801395
7.476144	461.791724	9.806413
7.638412	460.788235	9.811431
7.526767	460.228161	9.816448
7.946345	446.678758	9.821466
7.854054	452.294438	9.826483
7.669359	446.936524	9.831501
7.287609	438.349506	9.836519
7.206382	443.427000	9.841536
7.753029	442.909593	9.846554
7.609672	459.177240	9.851571
7.711884	448.763478	9.856589
7.859199	431.712680	9.861607
7.509888	434.979545	9.866624
7.728021	420.565322	9.871642
7.217439	423.630088	9.876659
7.343835	422.556450	9.881677
7.540231	434.731949	9.886695
7.717926	440.920941	9.891712
7.646950	430.625668	9.896730
7.655156	425.048388	9.901747
7.446654	424.983054	9.906765
7.108596	429.683986	9.911783
7.236833	444.804857	9.916800
7.459296	441.822870	9.921818
7.787862	448.281851	9.926835
7.381966	450.367848	9.931853
7.435825	446.033092	9.936871
7.508914	448.123404	9.941888
7.855976	446.873404	9.946906
7.758774	451.839785	9.951923
7.547931	443.418649	9.956941
7.631971	453.102911	9.961959
7.635798	450.726137	9.966976
7.717894	450.833298	9.971994
7.714085	442.140099	9.977011
7.641919	441.706416	9.982029
7.733912	451.301080	9.987047
7.383039	456.622523	9.992064
7.657892	447.608237	9.997082
7.642087	446.023433	10.002099
7.658826	451.593737	10.007117
7.774714	446.741263	10.012135
7.171961	446.699444	10.017152
7.881365	456.024422	10.022170
7.925542	474.260413	10.027187
8.056017	482.126114	10.032205
7.712622	458.171378	10.037223
7.428293	456.082453	10.042240
7.794261	471.522922	10.047258
7.534473	476.350528	10.052275
7.836684	479.948288	10.057293
7.834221	474.549370	10.062311
7.855598	476.187011	10.067328
8.004260	473.330114	10.072346
8.267248	489.329404	10.077363
8.104412	474.876627	10.082381
7.679401	462.399097	10.087399
7.878284	469.386337	10.092416
8.205423	476.135870	10.097434
8.001026	466.792268	10.102451
7.555745	460.869036	10.107469
7.909983	451.252281	10.112487
7.397079	458.318783	10.117504
7.840722	465.460407	10.122522
8.116530	471.208121	10.127539
7.827693	477.921022	10.132557
8.074665	474.228347	10.137575
7.831334	481.836683	10.142592
8.014600	486.289212	10.147610
7.994900	478.172799	10.152627
7.784709	475.501155	10.157645
8.043956	469.913176	10.162663
7.992078	479.558657	10.167680
7.662088	485.861422	10.172698
8.027264	481.938912	10.177715
7.659309	479.317076	10.182733
7.949137	470.704371	10.187751
7.625546	482.377066	10.192768
7.762922	473.021271	10.197786
8.084340	475.823969	10.202803
8.125381	486.224967	10.207821
8.061280	476.714355	10.212839
8.107664	477.070062	10.217856
8.240166	475.967070	10.222874
8.141008	477.150130	10.227891
7.917054	482.981970	10.232909
8.097669	475.209894	10.237927
8.053089	477.097634	10.242944
7.973151	481.307133	10.247962
8.049326	477.439087	10.252979
8.111709	480.850135	10.257997
8.055707	478.653078	10.263015
7.729711	486.157527	10.268032
8.145653	491.848717	10.273050
8.182276	494.200321	10.278067
8.057987	503.112352	10.283085
7.967504	504.685365	10.288103
8.533371	509.763109	10.293120
8.297098	499.834344	10.298138
8.329179	499.513811	10.303155
8.064064	507.087681	10.308173
8.393477	497.105554	10.313191
8.449256	507.100345	10.318208
8.085802	494.619519	10.323226
8.134350	500.266932	10.328243
8.163708	499.621790	10.333261
8.410012	498.974427	10.338279
8.452970	504.685826	10.343296
8.375213	495.341425	10.348314
8.248885	490.589764	10.353331
8.348683	491.842829	10.358349
8.483838	490.991876	10.363367
8.088313	487.509681	10.368384
8.197736	486.183074	10.373402
8.369195	490.953008	10.378419
8.522823	493.125456	10.383437
8.489190	497.485532	10.388455
8.044052	479.520275	10.393472
8.404069	482.711422	10.398490
8.372768	479.844675	10.403507
8.062902	496.340242	10.408525
8.377815	489.497104	10.413543
8.438633	495.183629	10.418560
8.578933	498.790823	10.423578
8.600240	501.851680	10.428595
8.426349	501.171915	10.433613
8.421297	496.890497	10.438631
8.083450	486.630431	10.443648
8.273989	494.704527	10.448666
8.711872	491.143063	10.453683
8.275054	501.419663	10.458701
8.329598	500.631751	10.463719
8.210501	506.213754	10.468736
8.501188	505.928692	10.473754
8.374529	500.129401	10.478771
8.474077	498.889533	10.483789
8.344927	498.499434	10.488807
8.388532	494.797395	10.493824
8.437313	502.328701	10.498842
8.549984	492.582285	10.503859
8.203717	490.613448	10.508877
8.439943	493.236918	10.513895
8.438614	497.752903	10.518912
8.722666	496.632625	10.523930
8.425267	496.956655	10.528947
8.402527	503.044338	10.533965
8.799432	488.034207	10.538983
8.537685	493.998161	10.544000
8.683904	494.745405	10.549018
8.786659	487.733337	10.554035
8.396853	499.100786	10.559053
8.735138	489.331867	10.564071
8.413124	490.152012	10.569088
8.594448	495.283313	10.574106
8.739795	493.925867	10.579123
8.458326	496.588917	10.584141
8.522861	495.054713	10.589159
8.487891	506.363764	10.594176
8.827073	520.877526	10.599194
8.885021	520.335224	10.604211
8.617488	506.665549	10.609229
8.989893	503.038541	10.614247
9.039076	492.667722	10.619264
8.325645	501.516852	10.624282
8.493762	497.154827	10.629299
8.760124	508.117176	10.634317
8.715354	513.378353	10.639335
8.824203	519.186790	10.644352
8.797309	523.321771	10.649370
9.036718	521.075558	10.654387
8.765288	505.797101	10.659405
8.909282	490.902080	10.664423
8.770151	503.205602	10.669440
8.732029	496.881309	10.674458
8.813939	487.101818	10.679475
8.791924	504.562386	10.684493
9.030126	498.532726	10.689511
8.600036	493.216161	10.694528
8.784303	513.408980	10.699546
9.021422	507.407887	10.704563
8.807124	520.856006	10.709581
9.032415	514.572742	10.714599
9.299367	501.059684	10.719616
8.844234	503.506787	10.724634
8.826628	499.110565	10.729651
8.897558	506.376505	10.734669
8.802699	500.884673	10.739687
8.747225	492.713866	10.744704
8.599485	511.976965	10.749722
8.572487	512.258895	10.754739
8.648023	531.042302	10.759757
8.842849	525.628431	10.764775
9.127292	523.299470	10.769792
8.777704	524.979096	10.774810
8.748949	513.597963	10.779827
8.698724	523.356814	10.784845
8.821984	525.991566	10.789863
8.981270	520.267662	10.794880
9.145942	521.513785	10.799898
9.293621	518.272042	10.804915
8.795166	525.929585	10.809933
9.069800	526.760973	10.814951
9.072401	516.151251	10.819968
8.755540	525.260527	10.824986
9.145105	523.006714	10.830003
9.055404	525.153938	10.835021
8.552952	530.972352	10.840039
9.205750	535.749403	10.845056
9.099798	545.176131	10.850074
9.098624	528.220940	10.855091
9.053301	542.709382	10.860109
8.926451	550.116582	10.865127
9.376231	541.999624	10.870144
9.204732	549.360129	10.875162
9.108367	549.230000	10.880179
9.168764	540.798144	10.885197
8.887708	543.060367	10.890215
9.354109	536.966763	10.895232
9.079277	542.383684	10.900250
9.154492	541.292763	10.905267
9.144107	543.187810	10.910285
9.116300	546.369926	10.915303
9.470844	555.595579	10.920320
9.037632	554.596439	10.925338
9.274944	545.218736	10.930355
9.715556	543.471347	10.935373
9.402146	547.171281	10.940391
9.550491	547.728856	10.945408
9.578388	550.220675	10.950426
9.401577	545.760870	10.955443
9.277587	531.844773	10.960461
9.188130	541.836950	10.965479
9.621977	538.443356	10.970496
8.919702	539.938064	10.975514
9.514254	540.445099	10.980531
9.704632	547.133905	10.985549
9.113827	533.015946	10.990567
9.299241	531.251489	10.995584
9.440988	544.148752	11.000602
9.552316	532.389206	11.005619
9.652903	552.156460	11.010637
9.730395	531.761960	11.015655
9.450511	522.060868	11.020672
9.036554	522.093791	11.025690
9.306393	523.967296	11.030707
9.524275	539.342521	11.035725
9.307265	540.259924	11.040743
9.535217	537.204486	11.045760
9.708598	549.033367	11.050778
9.544344	532.072007	11.055795
9.472239	524.888343	11.060813
9.057200	533.283949	11.065831
9.799059	528.154119	11.070848
9.487963	544.968645	11.075866
9.679845	540.312588	11.080883
9.982892	540.107649	11.085901
9.381284	528.998727	11.090919
9.467357	520.297807	11.095936
9.438608	519.166272	11.100954
9.581702	536.850463	11.105971
9.797315	539.666489	11.110989
9.341895	529.005001	11.116007
9.625366	532.469995	11.121024
9.717842	541.102154	11.126042
9.645931	546.995545	11.131059
9.576595	526.150562	11.136077
9.605931	543.290762	11.141095
9.838131	536.870721	11.146112
9.482559	536.834596	11.151130
9.496354	544.447104	11.156147
9.350934	540.045526	11.161165
9.634369	541.658150	11.166183
9.856069	535.933992	11.171200
9.623448	547.125526	11.176218
9.905908	549.833320	11.181235
10.025216	550.114561	11.186253
9.607345	551.561834	11.191271
9.870282	544.796191	11.196288
9.824522	545.197803	11.201306
9.492505	544.861378	11.206323
9.829824	542.798725	11.211341
9.901565	548.227957	11.216359
9.937348	536.656889	11.221376
9.542946	535.837893	11.226394
9.781952	544.873255	11.231411
9.859997	540.474752	11.236429
9.659438	536.274256	11.241447
9.789280	536.004770	11.246464
9.797314	535.902566	11.251482
9.892407	538.017865	11.256499
9.769197	540.066171	11.261517
9.707880	544.007708	11.266535
10.126583	537.347200	11.271552
9.855172	534.849173	11.276570
9.998678	541.879776	11.281587
9.730690	541.729033	11.286605
9.798527	550.904652	11.291623
9.974442	540.993735	11.296640
9.931406	545.992732	11.301658
9.761017	549.635686	11.306675
9.780216	539.171682	11.311693
9.691860	541.833073	11.316711
9.896012	538.929657	11.321728
9.722239	543.996344	11.326746
9.673297	546.487504	11.331763
10.273211	551.664096	11.336781
9.857098	557.929804	11.341799
10.234740	563.068427	11.346816
10.077068	559.019031	11.351834
9.989578	564.864363	11.356851
10.261405	555.497059	11.361869
9.878898	554.824526	11.366887
9.610453	561.786738	11.371904
9.729070	565.586661	11.376922
9.449556	566.472773	11.381939
10.019470	565.386875	11.386957
9.652352	577.113744	11.391975
9.775107	570.713886	11.396992
9.703176	568.525609	11.402010
10.001132	590.045131	11.407027
10.177954	597.130526	11.412045
9.999931	601.292210	11.417063
10.403883	591.645550	11.422080
10.167227	595.516573	11.427098
9.780496	593.888526	11.432115
10.246693	601.247592	11.437133
9.750895	605.935261	11.442151
10.159874	597.348124	11.447168
10.097358	597.061252	11.452186
10.077378	605.108217	11.457203
10.511901	595.235897	11.462221
10.014788	592.507926	11.467239
10.128092	601.591290	11.472256
9.884943	599.852528	11.477274
9.929377	600.476774	11.482291
10.697533	606.027959	11.487309
10.343185	613.158193	11.492327
9.858816	598.408252	11.497344
10.422613	617.254580	11.502362
10.360249	621.581291	11.507379
10.367691	616.890817	11.512397
9.987233	622.807027	11.517415
10.477671	622.509798	11.522432
10.763266	617.668723	11.527450
10.729362	621.931046	11.532467
11.054190	613.006722	11.537485
10.357233	604.067928	11.542503
10.762940	589.630675	11.547520
10.464593	593.766912	11.552538
10.161380	590.964573	11.557555
10.710886	593.296294	11.562573
10.477653	595.450095	11.567591
10.361244	588.812925	11.572608
10.191479	599.114271	11.577626
9.909206	600.174376	11.582643
10.478491	606.763187	11.587661
10.360708	615.055748	11.592679
10.356164	623.437976	11.597696
10.590171	615.329335	11.602714
10.657858	626.089169	11.607731
10.725120	619.530682	11.612749
10.935406	618.040045	11.617767
10.569244	618.232777	11.622784
10.749768	617.273772	11.627802
10.512725	622.773193	11.632819
10.618195	619.096208	11.637837
10.425968	621.527640	11.642855
10.701273	622.090695	11.647872
10.454901	620.172559	11.652890
10.610327	616.828611	11.657907
10.530853	610.488626	11.662925
10.630195	618.854677	11.667943
10.847989	615.598844	11.672960
10.700093	611.872950	11.677978
10.337076	611.976834	11.682995
10.872943	610.593289	11.688013
10.416296	616.275217	11.693031
10.421348	612.090025	11.698048
10.604685	612.986123	11.703066
10.433585	613.132706	11.708083
10.871557	609.403954	11.713101
10.527830	614.528679	11.718119
10.432777	617.759146	11.723136
11.195249	638.101913	11.728154
10.706233	639.481377	11.733171
10.960744	647.861151	11.738189
10.931810	632.137746	11.743207
10.782603	624.192903	11.748224
10.795638	620.072736	11.753242
10.883131	633.754808	11.758259
10.901379	636.093513	11.763277
11.079093	636.908440	11.768295
10.700803	631.006278	11.773312
11.101338	635.462885	11.778330
10.926213	638.743691	11.783347
10.723888	625.675974	11.788365
11.135817	633.207598	11.793383
11.078971	620.940868	11.798400
10.980689	624.856622	11.803418
10.860849	615.461908	11.808435
10.902667	620.463493	11.813453
11.127781	630.996855	11.818471
10.851765	625.097705	11.823488
11.162171	631.979286	11.828506
10.929449	639.093750	11.833523
10.960867	639.032084	11.838541
11.363188	651.033663	11.843559
11.135018	631.090568	11.848576
10.933511	622.371259	11.853594
10.975249	632.661785	11.858611
11.337900	636.796099	11.863629
11.327703	637.460409	11.868647
11.059878	625.437955	11.873664
11.341996	613.658076	11.878682
11.111279	619.756091	11.883699
11.155286	616.959644	11.888717
10.835696	616.772755	11.893735
11.038703	622.787463	11.898752
11.083060	637.243085	11.903770
11.394988	650.700886	11.908787
11.100694	646.944131	11.913805
11.389884	645.387560	11.918823
11.040223	641.005134	11.923840
11.536299	645.254371	11.928858
11.311307	640.328690	11.933875
11.113734	629.084218	11.938893
11.354720	634.165245	11.943911
11.233556	638.747259	11.948928
11.582471	640.428590	11.953946
11.170079	634.758945	11.958963
10.923331	631.452365	11.963981
11.304448	641.188302	11.968999
11.146819	641.967081	11.974016
11.434355	642.222132	11.979034
11.218265	651.555614	11.984051
11.377053	648.968501	11.989069
11.451562	654.207993	11.994087
11.790351	653.486267	11.999104
11.607919	647.440000	12.004122
11.197573	648.580007	12.009139
11.556313	645.788200	12.014157
11.575033	648.893666	12.019175
11.320660	642.025500	12.024192
11.749959	647.736751	12.029210
11.462137	654.547386	12.034227
11.443004	652.991483	12.039245
11.691497	654.385505	12.044263
11.307646	651.908123	12.049280
11.584574	649.015449	12.054298
11.666596	642.006549	12.059315
11.328551	644.741543	12.064333
11.715166	641.131229	12.069351
11.240169	657.646345	12.074368
11.731787	647.941825	12.079386
11.530956	650.052720	12.084403
11.310548	650.494149	12.089421
11.638360	649.070414	12.094439
11.538606	649.303716	12.099456
11.583629	644.048826	12.104474
11.280357	655.895189	12.109491
11.365976	647.462511	12.114509
11.730968	650.122758	12.119527
11.547240	657.570415	12.124544
11.974141	650.551995	12.129562
11.520140	654.570476	12.134579
11.641290	643.046005	12.139597
11.946588	652.023765	12.144615
11.351692	650.134644	12.149632
11.300275	651.161964	12.154650
11.366328	653.007253	12.159667
11.752277	653.294316	12.164685
11.565551	662.250861	12.169703
11.366439	672.679891	12.174720
11.927561	677.647973	12.179738
11.717831	675.115078	12.184755
11.978816	669.267999	12.189773
11.989722	662.778230	12.194791
11.835341	674.585644	12.199808
12.089236	669.026838	12.204826
12.316703	668.871534	12.209843
11.868624	654.633429	12.214861
11.853817	646.989531	12.219879
11.604793	654.005557	12.224896
11.714691	662.635062	12.229914
11.631074	676.548929	12.234931
11.708773	664.292777	12.239949
11.874394	670.912904	12.244967
11.918865	665.263633	12.249984
12.380095	668.246558	12.255002
12.046308	670.586431	12.260019
12.036705	671.556752	12.265037
12.089764	673.527137	12.270055
11.836602	666.803936	12.275072
11.999666	666.781731	12.280090
12.241807	670.836990	12.285107
11.858897	673.528483	12.290125
12.230833	661.658851	12.295143
12.411694	677.128319	12.300160
12.073232	666.161370	12.305178
12.169400	669.762847	12.310195
12.271248	669.055921	12.315213
12.302042	673.235601	12.320231
12.156453	670.878906	12.325248
12.537793	678.036628	12.330266
11.928653	660.601633	12.335283
11.803157	670.425931	12.340301
12.202228	661.142898	12.345319
12.126893	674.096143	12.350336
12.257383	668.259915	12.355354
12.236737	666.309785	12.360371
12.112571	670.267448	12.365389
12.464996	676.902671	12.370407
12.375681	672.290361	12.375424
12.492074	670.921631	12.380442
12.304631	671.263257	12.385459
12.489939	673.563334	12.390477
12.334164	672.555705	12.395495
12.236879	671.485322	12.400512
12.335429	674.168122	12.405530
12.089331	672.978903	12.410547
12.262744	666.795178	12.415565
12.319575	671.052852	12.420583
12.091822	674.427062	12.425600
12.457103	680.145135	12.430618
12.331721	675.418523	12.435635
12.434415	671.738804	12.440653
12.414104	677.027778	12.445671
12.346041	675.223880	12.450688
12.513149	673.739961	12.455706
12.269702	676.652728	12.460723
12.341617	674.255856	12.465741
12.437028	669.539049	12.470759
12.201466	675.918693	12.475776
12.523498	671.308608	12.480794
12.118360	670.791067	12.485811
12.016222	683.486570	12.490829
12.572726	681.664321	12.495847
12.570765	695.354057	12.500864
12.469432	692.545515	12.505882
12.752957	690.781546	12.510899
12.686538	690.391142	12.515917
12.555952	686.883435	12.520935
12.354502	700.705217	12.525952
12.558172	701.762250	12.530970
12.586494	693.786581	12.535987
12.389455	695.152146	12.541005
12.622269	697.769866	12.546023
12.455642	693.456756	12.551040
11.934645	690.609416	12.556058
12.236936	698.975463	12.561075
12.039063	699.659529	12.566093
12.616480	702.179416	12.571111
12.535779	711.330910	12.576128
13.090212	716.217997	12.581146
13.003071	714.735791	12.586163
13.065775	720.930162	12.591181
12.860843	721.621638	12.596199
13.469301	714.858938	12.601216
12.871294	701.442531	12.606234
13.108856	695.848391	12.611251
12.693141	696.389654	12.616269
12.899081	695.474023	12.621287
12.771923	708.192373	12.626304
12.857113	702.543062	12.631322
12.942941	697.329139	12.636339
12.634544	697.620172	12.641357
12.758873	703.464127	12.646375
12.996802	706.541784	12.651392
12.837847	721.723383	12.656410
13.050047	712.349502	12.661427
13.193599	717.581419	12.666445
12.782694	709.143971	12.671463
12.562119	719.106170	12.676480
12.682196	719.134839	12.681498
12.823584	719.930179	12.686515
12.700653	715.433541	12.691533
12.933244	710.802658	12.696551
12.985510	720.772870	12.701568
12.891446	717.748605	12.706586
12.995870	722.150355	12.711603
12.653344	726.148339	12.716621
13.134313	726.420609	12.721639
13.209600	740.578019	12.726656
13.423053	735.751300	12.731674
13.374601	727.853838	12.736691
12.884238	725.718067	12.741709
13.035928	718.736159	12.746727
12.822924	720.183104	12.751744
13.077574	746.458887	12.756762
13.432065	749.180742	12.761779
13.445530	758.093543	12.766797
13.399815	738.311263	12.771815
13.177333	737.979869	12.776832
13.275138	750.704248	12.781850
13.308063	745.492237	12.786867
13.289881	751.866464	12.791885
13.209548	756.218096	12.796903
13.302485	751.747797	12.801920
13.489957	748.439859	12.806938
13.206783	746.161377	12.811955
13.278390	752.717279	12.816973
13.415940	746.441283	12.821991
13.286700	749.645540	12.827008
13.255390	754.702728	12.832026
13.307633	747.830962	12.837043
13.245932	741.425050	12.842061
13.359021	748.804442	12.847079
13.253895	753.153621	12.852096
13.249626	758.847209	12.857114
13.479164	751.348253	12.862131
13.487973	753.328693	12.867149
13.561297	747.258351	12.872167
13.667975	747.367998	12.877184
13.696456	752.968124	12.882202
13.707568	752.265856	12.887219
13.821518	751.724295	12.892237
13.603307	752.682920	12.897255
13.707775	750.372485	12.902272
13.577834	750.702003	12.907290
13.628356	752.404558	12.912307
13.341696	748.334178	12.917325
13.169001	752.308881	12.922343
13.559017	749.385961	12.927360
13.552558	744.069632	12.932378
13.754488	741.769269	12.937395
13.550987	749.857495	12.942413
13.643520	744.058710	12.947431
13.794223	745.676240	12.952448
13.920358	752.400372	12.957466
13.995876	742.798455	12.962483
13.759255	754.284222	12.967501
13.826011	738.694142	12.972519
13.858138	742.558061	12.977536
13.689373	750.214859	12.982554
13.857187	734.284011	12.987571
14.128845	742.149936	12.992589
13.760318	745.779600	12.997607
13.987243	745.217294	13.002624
13.790898	749.252481	13.007642
14.008877	744.352474	13.012659
13.975623	748.381204	13.017677
14.014754	746.573232	13.022695
13.666978	745.251520	13.027712
13.773011	755.415345	13.032730
14.156610	745.664477	13.037747
14.054116	756.078513	13.042765
13.929601	758.379503	13.047783
13.973500	746.182205	13.052800
13.789638	740.000434	13.057818
14.069495	740.231436	13.062835
14.058966	744.553262	13.067853
14.064810	751.393949	13.072871
14.235202	741.849842	13.077888
13.776366	749.756924	13.082906
14.012112	738.820444	13.087923
13.819919	744.382345	13.092941
13.977375	760.496137	13.097959
14.010184	766.202888	13.102976
14.129916	769.488301	13.107994
14.416659	768.134066	13.113011
14.115989	766.432644	13.118029
14.195777	770.519515	13.123047
14.172547	777.797071	13.128064
14.180985	769.833930	13.133082
14.177564	768.701592	13.138099
14.551861	777.984243	13.143117
14.247733	770.372716	13.148135
14.038475	770.096065	13.153152
14.233367	780.164021	13.158170
14.630130	772.301359	13.163187
14.482291	767.385721	13.168205
14.231300	761.015585	13.173223
14.191689	758.307872	13.178240
14.085620	768.817143	13.183258
14.217754	769.314135	13.188275
14.321485	773.394123	13.193293
14.385264	765.255115	13.198311
14.687284	765.836106	13.203328
14.426563	767.382000	13.208346
14.452413	769.694294	13.213363
14.707818	760.266325	13.218381
14.329138	773.509861	13.223399
14.893786	765.674711	13.228416
14.702473	776.957785	13.233434
14.513266	771.417444	13.238451
14.303379	760.856438	13.243469
14.292878	774.310887	13.248487
14.450589	768.539813	13.253504
14.465619	775.820878	13.258522
14.620557	772.177185	13.263539
14.545329	769.096330	13.268557
14.318920	772.340966	13.273575
14.548586	766.725943	13.278592
14.110757	768.741211	13.283610
14.384299	769.206719	13.288627
14.126667	766.927414	13.293645
14.229697	782.882447	13.298663
14.501835	787.226544	13.303680
14.663954	786.106299	13.308698
14.654308	785.454597	13.313715
15.060035	785.741739	13.318733
14.922882	795.577387	13.323751
15.067910	783.326450	13.328768
15.019006	791.936563	13.333786
14.907430	783.108502	13.338803
14.824292	774.045651	13.343821
14.773342	777.771039	13.348839
14.912201	775.505737	13.353856
14.939883	777.360168	13.358874
14.561150	774.465419	13.363891
15.139328	780.396523	13.368909
15.071108	784.247673	13.373927
14.876766	768.243797	13.378944
14.752064	779.254577	13.383962
15.063982	784.195220	13.388979
15.155533	786.986421	13.393997
14.605293	786.179053	13.399015
14.979846	785.546425	13.404032
14.809137	785.759219	13.409050
15.537037	784.440435	13.414067
15.116278	789.286877	13.419085
14.897254	795.714480	13.424103
15.069162	792.118632	13.429120
15.046769	786.820549	13.434138
15.105950	790.014411	13.439155
15.271390	784.819625	13.444173
15.145817	790.945507	13.449191
15.154498	791.259755	13.454208
15.132144	786.311951	13.459226
15.178677	782.312759	13.464243
15.115267	789.369364	13.469261
14.330177	800.205274	13.474279
15.039779	786.742998	13.479296
15.030931	793.472383	13.484314
15.419567	791.821423	13.489331
15.257803	792.739704	13.494349
15.000928	787.875749	13.499367
15.156258	782.379589	13.504384
15.045097	785.117148	13.509402
14.758469	782.902313	13.514419
15.256400	796.072496	13.519437
15.344690	812.866116	13.524455
15.679374	808.399188	13.529472
15.581148	814.763811	13.534490
15.027108	798.257350	13.539507
15.533539	805.114789	13.544525
15.702115	806.259341	13.549543
15.546924	794.459070	13.554560
15.256103	799.559831	13.559578
15.357165	795.085101	13.564595
15.735008	792.792056	13.569613
15.398192	792.841369	13.574631
15.807819	793.667531	13.579648
14.982053	796.292297	13.584666
15.227250	802.152179	13.589683
15.796633	807.721753	13.594701
15.921363	812.126675	13.599719
16.008845	813.438484	13.604736
15.780617	802.577360	13.609754
15.631494	790.823483	13.614771
15.740654	793.665591	13.619789
15.326511	793.831082	13.624807
15.193260	788.594440	13.629824
15.611654	813.140742	13.634842
15.540425	816.597903	13.639859
15.432217	813.430660	13.644877
15.454204	823.894780	13.649895
15.913676	813.737597	13.654912
16.137878	824.826623	13.659930
15.732959	816.587001	13.664947
15.796852	817.410191	13.669965
15.638005	821.471114	13.674983
15.846758	811.943087	13.680000
16.226733	811.372729	13.685018
15.896125	807.340735	13.690035
16.348200	813.689103	13.695053
15.827419	815.303893	13.700071
15.968881	811.681224	13.705088
16.000686	817.687940	13.710106
15.964477	817.365411	13.715123
15.812812	813.901986	13.720141
15.623482	815.660825	13.725159
16.049360	823.316587	13.730176
15.932757	818.127835	13.735194
15.751661	817.524916	13.740211
15.997034	813.415865	13.745229
15.807935	815.139955	13.750247
15.910354	816.288497	13.755264
16.161048	811.796777	13.760282
15.860564	818.268629	13.765299
16.172098	811.795113	13.770317
16.084339	815.822876	13.775335
16.002761	817.533381	13.780352
15.813275	819.175483	13.785370
15.592449	825.786410	13.790387
16.245085	836.490010	13.795405
16.133186	846.902407	13.800423
16.205757	845.761387	13.805440
16.480143	836.636528	13.810458
16.193345	842.879046	13.815475
16.777084	831.070997	13.820493
16.192165	845.536404	13.825511
16.340137	830.176590	13.830528
16.393899	821.553136	13.835546
16.017272	824.272073	13.840563
16.553754	831.311032	13.845581
16.326973	839.996199	13.850599
16.303264	825.149100	13.855616
16.376738	827.971524	13.860634
16.144480	829.658155	13.865651
16.597043	832.680326	13.870669
16.023718	844.477344	13.875687
16.263610	840.643689	13.880704
16.476841	838.193235	13.885722
16.716107	837.108311	13.890739
16.802636	832.418090	13.895757
16.558515	847.142853	13.900775
16.796445	838.897804	13.905792
17.002681	842.740948	13.910810
16.347151	830.848145	13.915827
16.721341	830.307088	13.920845
16.685048	839.985050	13.925863
16.828917	828.343317	13.930880
16.724437	813.657122	13.935898
16.552157	812.734103	13.940915
16.645561	811.394187	13.945933
16.391218	817.707381	13.950951
16.736198	827.064049	13.955968
17.183422	833.286951	13.960986
16.725598	824.834662	13.966003
16.758773	817.413588	13.971021
16.845025	808.788236	13.976039
16.617805	806.595706	13.981056
16.443532	812.438853	13.986074
16.531639	829.387147	13.991091
17.029547	832.137178	13.996109
16.529641	836.885505	14.001127
17.002619	828.364030	14.006144
16.926028	836.129587	14.011162
16.546194	842.484418	14.016179
16.659991	831.778302	14.021197
16.685691	843.368447	14.026215
16.760229	840.216927	14.031232
16.803114	831.330080	14.036250
16.935371	842.698513	14.041267
17.185330	832.627587	14.046285
17.011378	848.086176	14.051303
16.886800	840.465597	14.056320
16.976825	836.049378	14.061338
16.767518	840.354841	14.066355
17.160379	847.573953	14.071373
17.327989	854.925966	14.076391
17.345266	858.782755	14.081408
17.101603	833.685391	14.086426
16.751445	842.459195	14.091443
17.216401	846.991030	14.096461
17.230482	850.826225	14.101479
17.360440	853.327442	14.106496
17.634277	850.861239	14.111514
17.212665	842.444328	14.116531
17.305616	832.176947	14.121549
17.113165	821.363889	14.126567
17.101037	819.264097	14.131584
17.430876	829.194309	14.136602
17.353177	845.590937	14.141619
17.297806	849.392765	14.146637
17.502951	854.564641	14.151655
17.197675	852.873395	14.156672
17.410656	850.710150	14.161690
17.463645	849.616359	14.166707
17.485419	848.110873	14.171725
17.479018	852.084953	14.176743
17.604279	856.284681	14.181760
17.580186	858.235543	14.186778
17.423657	851.673946	14.191795
17.867987	840.815379	14.196813
17.570937	830.580319	14.201831
17.315560	829.768064	14.206848
17.474952	833.893047	14.211866
17.264563	847.198796	14.216883
17.347700	853.140730	14.221901
17.382474	848.720487	14.226919
17.385343	851.680137	14.231936
17.672667	852.380180	14.236954
17.519262	852.180037	14.241971
17.061367	852.204021	14.246989
17.154230	851.091399	14.252007
17.786537	853.088380	14.257024
17.620128	850.895844	14.262042
17.424242	861.485424	14.267059
17.784991	877.785416	14.272077
17.674854	873.769572	14.277095
17.772428	877.557060	14.282112
17.975951	875.928602	14.287130
17.948429	881.101998	14.292147
18.004493	877.066588	14.297165
18.065726	870.815054	14.302183
17.830214	872.164533	14.307200
18.082599	874.984354	14.312218
18.056634	871.274134	14.317235
18.145844	864.642715	14.322253
17.926254	863.859599	14.327271
17.657369	880.869836	14.332288
17.906076	869.243310	14.337306
18.045729	872.020724	14.342323
18.135620	862.318678	14.347341
18.088525	875.857793	14.352359
18.069245	879.297411	14.357376
18.514617	873.412091	14.362394
17.873705	873.313095	14.367411
17.770115	878.220630	14.372429
17.915722	872.296777	14.377447
17.856571	874.679122	14.382464
17.935751	863.527107	14.387482
17.934336	877.620831	14.392499
17.902710	880.743643	14.397517
17.724050	882.317795	14.402535
18.260857	891.922334	14.407552
18.751593	887.008223	14.412570
19.040072	865.737911	14.417587
18.783705	861.555494	14.422605
18.717651	860.858924	14.427623
18.645555	855.145693	14.432640
19.008487	851.908244	14.437658
18.856280	856.577196	14.442675
18.585177	839.332385	14.447693
18.719109	831.109843	14.452711
18.539526	831.535452	14.457728
18.461047	821.275833	14.462746
18.290155	829.971228	14.467763
18.448080	827.627215	14.472781
18.890020	818.561481	14.477799
18.612306	825.440034	14.482816
18.803035	823.109848	14.487834
18.404011	826.794767	14.492851
18.289926	825.758548	14.497869
18.474193	831.864605	14.502887
18.249569	827.039798	14.507904
18.470338	832.174522	14.512922
18.772908	841.929110	14.517939
18.636604	846.213741	14.522957
18.837503	838.933797	14.527975
18.669687	833.996005	14.532992
18.759606	823.596560	14.538010
18.544856	837.499412	14.543027
18.838462	842.095793	14.548045
19.237487	846.186625	14.553063
18.613891	840.092218	14.558080
18.641729	829.238545	14.563098
19.006717	849.675000	14.568115
18.658721	851.553218	14.573133
18.876203	841.032919	14.578151
18.944562	853.231795	14.583168
18.669930	857.367556	14.588186
18.910679	849.901527	14.593203
19.008074	851.268598	14.598221
18.997612	847.331913	14.603239
19.063673	855.365594	14.608256
18.854329	851.188481	14.613274
18.857778	853.630502	14.618291
18.903633	855.904979	14.623309
18.699044	855.684403	14.628327
19.050878	861.174260	14.633344
18.796503	852.368398	14.638362
19.053771	856.752696	14.643379
18.889676	854.846970	14.648397
19.124023	848.215049	14.653415
18.815632	849.970339	14.658432
18.925867	862.850649	14.663450
19.218956	874.683199	14.668467
19.398949	885.488818	14.673485
19.597573	873.996316	14.678503
19.335859	882.216739	14.683520
19.171673	862.108792	14.688538
19.344731	875.029821	14.693555
19.363847	875.206749	14.698573
19.440087	873.569708	14.703591
19.081351	881.322410	14.708608
19.309282	872.561363	14.713626
19.422363	876.330658	14.718643
18.769680	881.383643	14.723661
19.298044	878.808382	14.728679
19.329533	869.844397	14.733696
19.274462	874.327821	14.738714
19.327556	869.819516	14.743731
19.106928	880.728532	14.748749
19.302678	874.983059	14.753767
19.558193	894.417310	14.758784
19.757202	896.049423	14.763802
19.734718	896.706189	14.768819
19.529069	891.550214	14.773837
19.813495	895.699924	14.778855
19.615210	895.481522	14.783872
19.868280	886.034916	14.788890
19.613240	874.707719	14.793907
19.591360	882.064000	14.798925
20.238385	882.430337	14.803943
19.957676	886.958362	14.808960
20.035630	880.183526	14.813978
19.937936	868.165976	14.818995
19.459683	872.342910	14.824013
19.825325	862.831454	14.829031
19.637587	869.948473	14.834048
19.738237	861.813147	14.839066
19.936288	880.751414	14.844083
19.590680	886.400360	14.849101
19.965390	885.259632	14.854119
19.721159	889.507429	14.859136
19.671507	897.473941	14.864154
19.648154	896.874860	14.869171
19.946387	903.764754	14.874189
20.203796	893.762059	14.879207
20.012745	892.968188	14.884224
20.376604	893.438572	14.889242
20.205859	894.569690	14.894259
20.328289	902.297977	14.899277
20.264054	891.764708	14.904295
20.138931	895.915069	14.909312
20.448230	890.934533	14.914330
20.057785	891.348794	14.919347
20.310266	890.990783	14.924365
20.204194	886.109633	14.929383
20.167179	898.299700	14.934400
19.949368	886.045226	14.939418
19.991098	886.310150	14.944435
19.943514	892.278761	14.949453
20.180092	884.822833	14.954471
19.920140	885.456612	14.959488
20.179076	884.371779	14.964506
20.458361	888.118355	14.969523
19.915371	897.149420	14.974541
20.650718	905.981459	14.979559
20.969558	910.990486	14.984576
20.960973	904.582556	14.989594
20.784555	886.704433	14.994611
20.349266	885.961211	14.999629
20.308801	884.531683	15.004647
20.344452	883.487925	15.009664
20.564439	890.831799	15.014682
20.599903	890.589625	15.019699
20.445831	885.734883	15.024717
20.643227	886.104956	15.029735
20.854404	892.901104	15.034752
20.737533	889.738353	15.039770
20.545745	881.014248	15.044787
20.585233	891.961665	15.049805
21.207855	905.014688	15.054823
20.597981	904.809876	15.059840
20.505073	899.891960	15.064858
21.209782	903.528122	15.069875
20.627582	897.351513	15.074893
20.507329	902.877016	15.079911
20.767430	910.792151	15.084928
20.686053	904.401866	15.089946
20.863398	908.965874	15.094963
20.682204	917.098039	15.099981
20.960448	913.738069	15.104999
20.942219	902.462344	15.110016
21.054451	916.267011	15.115034
21.016458	910.961854	15.120051
20.811141	916.469048	15.125069
21.476376	915.904765	15.130087
21.226492	912.216777	15.135104
21.196171	924.058688	15.140122
21.286805	923.773212	15.145139
20.954029	917.860711	15.150157
21.069127	910.329015	15.155175
21.455446	914.832087	15.160192
21.106310	917.912824	15.165210
20.965776	914.409777	15.170227
20.937478	917.074495	15.175245
21.441804	913.638300	15.180263
21.109783	914.336948	15.185280
21.032967	923.620487	15.190298
21.254431	918.180259	15.195315
20.839520	921.138696	15.200333
20.910184	911.202936	15.205351
20.907050	934.505407	15.210368
20.865720	937.796994	15.215386
21.534469	936.405359	15.220403
21.057483	941.673998	15.225421
21.306907	949.568723	15.230439
21.450857	945.254532	15.235456
21.397538	942.170236	15.240474
21.763421	937.957190	15.245491
21.653582	943.601002	15.250509
21.838331	944.260217	15.255527
21.678943	945.973382	15.260544
21.587155	944.371963	15.265562
21.617986	940.785426	15.270579
21.565094	952.024969	15.275597
21.591515	939.088661	15.280615
21.357706	951.773298	15.285632
21.273177	943.991808	15.290650
21.637899	959.839986	15.295667
21.834143	963.157703	15.300685
21.797811	964.147979	15.305703
22.305617	965.299684	15.310720
22.299861	953.873665	15.315738
22.453242	945.875255	15.320755
22.311925	945.218802	15.325773
22.097751	939.792747	15.330791
22.240681	934.099659	15.335808
21.909597	942.968370	15.340826
22.050424	932.074952	15.345843
21.941976	942.632032	15.350861
21.887041	930.169135	15.355879
22.141219	926.421598	15.360896
21.884329	933.325351	15.365914
22.066904	931.277281	15.370931
22.120310	929.138872	15.375949
21.955654	932.623224	15.380967
22.211641	937.869258	15.385984
21.718981	933.228162	15.391002
22.276578	935.688056	15.396019
21.866419	941.751003	15.401037
21.892457	942.621117	15.406055
22.272842	935.269009	15.411072
21.941606	936.317822	15.416090
22.281226	949.149858	15.421107
22.272522	966.277454	15.426125
22.575036	960.124019	15.431143
22.583572	951.109919	15.436160
22.506914	957.509104	15.441178
22.665602	940.392933	15.446195
22.090922	936.910140	15.451213
21.807978	941.627871	15.456231
22.643231	952.019092	15.461248
22.586372	955.587649	15.466266
22.179335	957.115316	15.471283
22.594839	955.195075	15.476301
22.581388	964.077458	15.481319
22.640617	953.925708	15.486336
22.146505	964.157846	15.491354
22.510633	952.768910	15.496371
22.431130	961.011492	15.501389
22.499597	952.906382	15.506407
22.595019	952.664340	15.511424
22.475541	959.631914	15.516442
22.325247	961.965346	15.521459
22.360027	964.588693	15.526477
22.859910	972.397096	15.531495
23.211790	972.468568	15.536512
22.847632	979.079777	15.541530
22.981632	974.574628	15.546547
22.946148	976.221168	15.551565
22.985710	962.440213	15.556583
23.352154	950.268294	15.561600
23.215106	957.746677	15.566618
22.952573	951.564458	15.571635
23.028922	947.787800	15.576653
22.832060	948.992414	15.581671
23.030364	941.353078	15.586688
22.825171	947.033828	15.591706
22.854305	946.628541	15.596723
23.370417	951.051455	15.601741
23.268435	961.500244	15.606759
23.195696	940.825715	15.611776
23.016740	945.975371	15.616794
23.321904	949.487562	15.621811
22.940612	948.256258	15.626829
22.681132	951.146320	15.631847
23.404943	962.552112	15.636864
23.527331	968.017767	15.641882
23.424604	969.911458	15.646899
23.580176	976.129327	15.651917
23.511136	972.422637	15.656935
23.411209	952.683272	15.661952
23.297463	956.522613	15.666970
23.499993	965.655385	15.671987
23.416448	973.002370	15.677005
23.040398	978.817028	15.682023
23.689053	967.607841	15.687040
23.561825	980.241191	15.692058
23.649763	978.510802	15.697075
23.562692	982.863537	15.702093
23.413761	976.486901	15.707111
23.787531	967.406460	15.712128
23.514671	975.679153	15.717146
23.550099	981.922043	15.722163
23.561590	966.996763	15.727181
23.619906	985.821201	15.732199
23.661111	979.228770	15.737216
23.825303	980.389795	15.742234
23.687206	972.436755	15.747251
23.840458	973.889811	15.752269
23.492091	974.354326	15.757287
23.877527	974.862377	15.762304
23.704047	976.754461	15.767322
23.757159	984.610340	15.772339
23.811654	986.066150	15.777357
23.822386	977.790140	15.782375
23.891982	975.548220	15.787392
23.884439	976.246842	15.792410
24.033253	979.310020	15.797427
23.734760	979.848819	15.802445
23.891645	1005.243974	15.807463
24.481768	995.249380	15.812480
24.246636	1011.642271	15.817498
24.120373	994.769226	15.822515
24.353428	995.865883	15.827533
24.091128	994.559245	15.832551
24.315600	986.101632	15.837568
24.299775	991.393158	15.842586
24.283375	983.727273	15.847603
24.155230	979.808881	15.852621
23.976667	993.791425	15.857639
24.428050	990.660099	15.862656
24.389343	997.895974	15.867674
24.035362	994.410365	15.872691
24.391767	1002.749196	15.877709
24.482157	1002.100845	15.882727
24.361762	994.653115	15.887744
23.967983	1003.645224	15.892762
24.423898	1000.642577	15.897779
24.082715	995.501362	15.902797
23.891334	998.137836	15.907815
24.450770	996.078420	15.912832
24.383693	1012.814369	15.917850
24.628642	1018.125260	15.922867
24.966692	1014.440384	15.927885
24.494947	1017.972566	15.932903
24.716700	1005.122560	15.937920
24.904240	1018.372793	15.942938
24.748070	1009.583120	15.947955
24.716591	1003.860361	15.952973
24.450721	1016.745693	15.957991
24.692805	1016.884752	15.963008
24.711710	1016.417941	15.968026
24.496916	1023.769603	15.973043
24.654660	1012.390672	15.978061
24.995721	1021.281002	15.983079
24.861548	1016.593537	15.988096
24.984743	1009.331933	15.993114
24.850746	1022.887847	15.998131
25.206731	1009.199599	16.003149
25.069558	1021.411656	16.008167
25.242599	1013.429089	16.013184
25.247774	1014.984098	16.018202
24.937071	1014.502334	16.023219
25.178811	1019.820037	16.028237
25.335247	1022.389738	16.033255
25.453981	1010.369953	16.038272
25.310367	1013.021082	16.043290
25.298547	1021.417253	16.048307
25.216687	1010.217638	16.053325
25.074962	1020.205598	16.058343
25.420553	1012.341332	16.063360
25.318101	1015.393145	16.068378
25.123470	1006.145566	16.073395
25.286365	1009.474796	16.078413
25.064134	1020.371524	16.083431
25.308183	1017.651165	16.088448
25.502604	1011.369377	16.093466
25.225889	1021.788603	16.098483
25.674239	1017.890897	16.103501
25.370731	1022.469841	16.108519
25.390845	1028.134472	16.113536
25.608580	1038.284224	16.118554
25.751539	1040.874960	16.123571
26.022636	1034.934671	16.128589
25.532471	1027.636016	16.133607
25.893648	1035.841578	16.138624
25.697363	1032.463950	16.143642
25.458486	1032.617933	16.148659
25.881690	1029.632997	16.153677
25.644914	1033.065483	16.158695
25.751416	1032.256834	16.163712
25.954539	1032.727002	16.168730
25.388611	1035.447043	16.173747
26.047592	1030.964282	16.178765
25.738216	1046.210603	16.183783
25.884424	1035.676040	16.188800
26.028091	1031.718473	16.193818
25.859712	1037.513438	16.198835
26.038348	1039.076155	16.203853
25.582704	1035.199274	16.208871
25.667921	1036.132761	16.213888
26.304193	1038.807634	16.218906
26.271143	1037.720916	16.223923
26.564721	1028.075427	16.228941
26.129874	1033.476385	16.233959
26.211655	1028.884680	16.238976
26.384688	1027.333538	16.243994
26.306583	1033.631991	16.249011
26.410403	1020.661483	16.254029
26.253809	1020.411341	16.259047
26.196720	1028.072961	16.264064
26.483393	1027.962085	16.269082
26.320804	1021.748501	16.274099
26.823221	1021.089647	16.279117
26.881006	1027.723541	16.284135
26.642570	1037.038613	16.289152
26.369355	1025.064064	16.294170
26.124611	1025.405150	16.299187
26.492444	1021.157067	16.304205
26.188139	1021.983945	16.309223
26.180033	1020.173833	16.314240
26.246690	1009.705319	16.319258
26.397839	1027.338252	16.324275
26.937753	1036.121891	16.329293
26.841148	1046.715058	16.334311
26.862755	1038.920157	16.339328
26.526171	1025.213496	16.344346
26.887686	1043.435376	16.349363
26.960444	1031.665728	16.354381
26.985626	1019.499558	16.359399
26.684493	1019.110977	16.364416
26.712553	1020.854924	16.369434
26.896017	1047.606131	16.374451
26.882640	1045.007898	16.379469
26.731917	1061.233060	16.384487
27.004971	1059.719991	16.389504
27.045811	1053.430543	16.394522
26.790375	1056.130646	16.399539
27.289000	1050.659848	16.404557
27.320175	1045.744663	16.409575
27.090902	1050.627632	16.414592
26.924555	1044.446184	16.419610
26.797374	1045.008804	16.424627
27.291463	1045.190677	16.429645
27.378610	1055.307122	16.434663
27.279245	1058.380552	16.439680
27.569537	1049.751717	16.444698
27.266426	1059.944705	16.449715
27.281036	1052.248717	16.454733
27.385467	1056.013085	16.459751
26.874056	1052.293203	16.464768
27.305914	1052.743538	16.469786
27.156378	1058.683897	16.474803
27.216843	1044.568269	16.479821
27.409488	1057.019329	16.484839
27.515942	1072.342938	16.489856
27.562581	1077.542714	16.494874
27.449658	1075.240837	16.499891
27.658316	1062.506437	16.504909
27.666572	1073.932193	16.509927
27.684421	1076.002778	16.514944
27.589942	1076.572931	16.519962
27.706656	1071.587616	16.524979
27.821319	1074.555144	16.529997
27.773654	1069.993049	16.535015
28.112688	1079.527499	16.540032
28.184959	1070.443456	16.545050
28.248447	1073.583050	16.550067
28.118084	1052.718549	16.555085
27.767101	1047.070768	16.560103
27.372222	1041.574988	16.565120
27.104720	1056.221515	16.570138
27.380742	1063.948050	16.575155
27.598639	1066.511344	16.580173
27.559637	1061.723843	16.585191
27.706444	1078.211962	16.590208
28.026777	1078.761711	16.595226
28.134426	1094.258719	16.600243
27.689522	1088.770713	16.605261
28.168156	1087.588547	16.610279
27.939861	1088.375192	16.615296
28.308411	1079.065136	16.620314
28.336769	1082.137619	16.625331
28.261300	1075.039462	16.630349
28.469873	1065.684895	16.635367
28.165534	1082.391579	16.640384
28.573782	1075.984960	16.645402
28.047980	1083.514456	16.650419
28.303707	1078.179296	16.655437
28.411389	1085.061059	16.660455
28.486695	1079.955959	16.665472
28.466110	1072.107653	16.670490
28.580196	1094.612610	16.675507
28.641390	1082.674318	16.680525
28.833225	1095.251761	16.685543
28.591436	1097.801425	16.690560
28.898286	1087.484815	16.695578
28.665741	1090.995547	16.700595
28.420031	1078.514912	16.705613
28.507431	1088.552443	16.710631
28.625304	1087.237099	16.715648
28.608814	1093.431307	16.720666
28.818695	1103.692771	16.725683
28.504114	1100.907898	16.730701
28.596468	1098.473073	16.735719
28.846788	1111.009864	16.740736
29.041502	1101.584854	16.745754
29.133497	1102.006055	16.750771
28.793117	1091.821770	16.755789
28.720875	1100.287345	16.760807
28.766248	1112.934941	16.765824
29.365332	1113.479160	16.770842
29.477853	1123.724236	16.775859
29.471727	1110.685574	16.780877
29.219894	1103.179369	16.785895
28.918269	1102.273317	16.790912
29.236158	1098.951320	16.795930
29.565716	1113.334523	16.800947
29.148394	1098.207657	16.805965
29.365931	1111.541650	16.810983
29.458882	1112.401354	16.816000
29.517134	1103.139598	16.821018
29.285138	1101.705159	16.826035
29.636027	1114.683882	16.831053
29.529950	1100.183889	16.836071
29.275494	1106.475111	16.841088
29.783907	1113.291338	16.846106
29.081034	1116.689112	16.851123
29.777604	1122.131689	16.856141
29.879114	1121.478446	16.861159
29.551176	1121.892447	16.866176
29.760404	1118.284410	16.871194
29.572334	1119.418240	16.876211
29.474489	1116.243018	16.881229
29.894115	1109.746254	16.886247
29.821435	1118.230840	16.891264
29.684179	1115.213231	16.896282
29.780172	1117.685061	16.901299
30.023158	1118.814893	16.906317
30.347186	1120.105674	16.911335
29.976823	1120.930218	16.916352
30.038784	1114.725821	16.921370
30.286285	1121.787799	16.926387
30.053384	1117.030473	16.931405
30.018047	1110.042817	16.936423
29.644084	1113.581883	16.941440
30.087385	1113.175224	16.946458
29.949759	1109.400289	16.951475
30.080535	1116.054409	16.956493
29.956955	1113.687916	16.961511
30.071054	1112.654021	16.966528
30.105851	1111.184355	16.971546
30.081022	1115.672597	16.976563
29.898448	1118.853666	16.981581
30.436355	1130.600933	16.986599
30.531346	1139.782097	16.991616
30.515985	1139.655130	16.996634
30.562410	1142.933091	17.001651
30.332941	1143.710454	17.006669
30.596734	1139.352311	17.011687
30.358477	1142.740867	17.016704
30.469460	1135.755666	17.021722
30.536309	1131.532328	17.026739
30.461010	1133.071474	17.031757
30.780953	1135.480037	17.036775
30.434577	1139.418752	17.041792
30.429934	1138.378097	17.046810
30.559398	1140.175694	17.051827
30.472748	1137.910745	17.056845
30.646690	1137.113682	17.061863
30.616940	1158.284131	17.066880
30.817110	1159.966581	17.071898
31.026673	1162.960373	17.076915
31.256130	1166.351851	17.081933
31.271085	1160.318858	17.086951
30.977934	1159.130619	17.091968
31.199361	1162.763186	17.096986
31.053507	1155.991533	17.102003
30.919475	1166.189815	17.107021
31.509294	1158.555700	17.112039
30.944602	1166.252230	17.117056
31.205153	1160.897360	17.122074
31.451510	1162.982871	17.127091
31.326771	1162.503707	17.132109
31.241075	1164.101279	17.137127
31.313766	1166.150713	17.142144
31.071717	1163.654336	17.147162
31.349316	1155.841618	17.152179
31.420505	1156.193477	17.157197
31.426752	1150.474265	17.162215
31.064497	1162.440598	17.167232
31.409743	1157.425990	17.172250
31.254947	1156.351909	17.177267
31.148789	1159.754615	17.182285
31.427162	1154.882962	17.187303
31.516784	1173.519689	17.192320
31.516817	1182.365367	17.197338
31.891134	1183.339057	17.202355
31.869910	1190.878399	17.207373
32.014515	1180.779499	17.212391
31.529394	1175.332441	17.217408
31.695290	1183.360194	17.222426
31.870614	1186.214154	17.227443
31.542505	1192.520030	17.232461
31.989491	1177.911774	17.237479
31.603888	1185.482600	17.242496
31.876270	1185.541205	17.247514
31.863054	1180.055385	17.252531
32.068491	1175.696852	17.257549
31.966777	1172.989278	17.262567
32.044918	1181.027537	17.267584
31.793375	1181.486449	17.272602
31.926690	1177.934401	17.277619
31.724263	1179.988802	17.282637
32.115085	1192.844599	17.287655
32.169499	1207.292807	17.292672
32.449810	1203.250812	17.297690
32.620714	1198.487397	17.302707
32.461021	1209.128352	17.307725
32.537650	1188.553355	17.312743
32.482284	1199.178061	17.317760
32.447628	1200.660392	17.322778
32.731420	1192.436442	17.327795
32.393134	1197.074494	17.332813
32.850560	1188.097681	17.337831
32.589807	1187.308336	17.342848
32.442193	1187.473357	17.347866
32.991625	1189.439101	17.352883
32.595812	1193.697947	17.357901
32.863254	1185.681672	17.362919
32.771821	1190.628424	17.367936
32.815537	1190.347093	17.372954
32.575278	1181.702970	17.377971
32.850808	1185.513310	17.382989
33.170295	1192.261152	17.388007
32.834816	1193.850280	17.393024
33.105354	1198.668095	17.398042
33.209055	1188.720725	17.403059
32.859805	1191.987717	17.408077
32.965680	1192.441473	17.413095
33.021640	1188.620601	17.418112
33.294680	1193.778850	17.423130
33.366850	1186.398887	17.428147
33.229114	1192.457374	17.433165
33.125685	1190.400156	17.438183
33.106151	1193.274988	17.443200
33.211889	1200.204436	17.448218
33.478013	1192.686976	17.453235
33.211524	1193.107189	17.458253
33.162635	1197.188947	17.463271
33.252828	1201.002899	17.468288
33.387595	1191.558772	17.473306
33.515182	1185.997380	17.478323
33.267843	1195.787289	17.483341
33.453984	1196.462076	17.488359
32.909333	1197.626182	17.493376
33.004132	1199.069423	17.498394
33.418556	1204.486527	17.503411
33.543394	1213.189713	17.508429
33.562486	1216.838015	17.513447
33.527153	1214.757569	17.518464
33.592629	1218.199835	17.523482
33.936263	1209.789835	17.528499
33.562229	1218.157287	17.533517
33.721983	1212.180627	17.538535
34.196702	1219.071567	17.543552
33.976721	1225.660420	17.548570
33.999772	1215.832888	17.553587
33.431220	1221.829073	17.558605
34.054781	1238.006427	17.563623
34.302476	1241.698037	17.568640
34.254866	1242.794226	17.573658
34.676533	1236.937724	17.578675
34.524691	1232.944071	17.583693
34.175279	1214.082700	17.588711
34.257421	1214.335025	17.593728
33.881278	1217.726129	17.598746
34.306610	1212.875760	17.603763
34.213599	1219.908743	17.608781
34.631170	1228.443283	17.613799
34.917017	1228.086383	17.618816
34.548177	1220.289078	17.623834
34.470655	1207.031089	17.628851
34.150109	1215.305006	17.633869
34.091437	1209.453872	17.638887
34.593748	1220.162175	17.643904
34.352903	1231.497429	17.648922
34.856653	1226.290867	17.653939
34.486818	1240.151907	17.658957
34.788785	1226.579199	17.663975
35.153820	1222.830120	17.668992
34.723712	1230.256415	17.674010
34.962262	1226.160956	17.679027
34.596315	1229.894456	17.684045
34.978767	1228.717789	17.689063
34.578047	1231.027130	17.694080
34.737864	1235.612886	17.699098
34.905837	1231.370625	17.704115
34.811098	1232.452061	17.709133
35.226943	1232.469394	17.714151
34.714067	1236.342536	17.719168
34.537329	1240.882864	17.724186
35.194432	1244.920984	17.729203
35.038384	1250.193393	17.734221
35.265258	1248.927338	17.739239
35.426928	1241.899490	17.744256
35.004667	1247.099738	17.749274
35.265814	1248.687496	17.754291
35.105629	1245.985859	17.759309
34.914526	1247.404190	17.764327
35.151603	1249.248159	17.769344
35.452358	1267.388211	17.774362
35.927212	1265.682760	17.779379
35.658252	1277.448452	17.784397
35.741252	1270.215092	17.789415
35.630341	1260.029697	17.794432
35.592793	1262.806360	17.799450
35.638051	1274.620959	17.804467
35.849023	1268.819341	17.809485
35.828208	1268.484940	17.814503
36.122304	1258.902362	17.819520
35.637315	1270.698529	17.824538
36.040107	1273.952588	17.829555
36.033717	1266.572201	17.834573
36.079418	1270.446744	17.839591
36.243943	1270.963954	17.844608
36.229338	1268.684614	17.849626
36.225346	1257.576861	17.854643
36.146880	1239.364396	17.859661
35.664638	1236.261625	17.864679
36.300631	1252.386564	17.869696
36.105324	1256.011451	17.874714
36.395183	1258.323729	17.879731
36.146184	1261.590904	17.884749
36.046888	1256.607611	17.889767
36.341165	1257.779959	17.894784
36.028957	1256.853456	17.899802
36.038240	1266.439347	17.904819
36.250825	1271.736419	17.909837
36.267324	1269.240798	17.914855
36.555250	1262.379476	17.919872
36.205502	1275.180224	17.924890
36.516806	1272.439888	17.929907
36.633641	1290.097359	17.934925
36.617635	1297.673803	17.939943
36.795049	1286.951198	17.944960
36.691187	1294.519229	17.949978
36.712465	1287.383833	17.954995
36.823922	1282.449771	17.960013
36.781879	1291.863787	17.965031
36.962191	1284.750969	17.970048
36.896754	1293.496442	17.975066
37.036453	1285.522101	17.980083
36.938542	1286.105418	17.985101
37.075045	1293.285731	17.990119
37.418824	1291.654334	17.995136
37.270787	1290.733826	18.000154
36.791560	1287.580083	18.005171
36.884035	1280.420982	18.010189
37.006842	1287.846422	18.015207
36.821139	1285.514824	18.020224
36.737627	1294.711236	18.025242
37.424456	1303.658327	18.030259
37.271429	1311.006802	18.035277
36.988003	1307.024152	18.040295
37.568725	1315.056806	18.045312
37.369119	1320.437003	18.050330
37.337421	1305.098442	18.055347
37.390108	1303.124201	18.060365
37.386397	1312.191433	18.065383
37.533202	1311.382809	18.070400
37.390261	1320.149829	18.075418
37.372320	1324.542378	18.080435
37.691945	1331.242915	18.085453
37.899899	1346.876006	18.090471
37.836427	1331.596018	18.095488
37.751995	1340.063604	18.100506
37.952971	1339.723072	18.105523
37.970271	1326.434452	18.110541
37.984588	1336.215257	18.115559
38.415826	1337.953267	18.120576
38.276313	1332.168328	18.125594
38.066562	1331.115415	18.130611
38.017133	1328.364963	18.135629
38.047527	1334.422567	18.140647
38.163242	1330.380923	18.145664
38.330885	1331.932754	18.150682
38.362465	1332.839894	18.155699
38.414485	1331.345437	18.160717
38.390688	1334.621744	18.165735
38.742459	1316.156023	18.170752
38.327683	1329.885273	18.175770
38.505167	1333.133397	18.180787
38.867381	1331.619047	18.185805
38.355493	1324.090121	18.190823
38.524141	1321.924254	18.195840
38.609174	1335.635652	18.200858
38.397437	1335.561349	18.205875
38.388313	1323.387690	18.210893
38.404199	1333.449117	18.215911
38.513875	1333.362641	18.220928
38.860914	1355.143691	18.225946
38.685842	1356.770974	18.230963
38.612958	1364.589833	18.235981
39.099762	1366.789410	18.240999
39.156455	1357.660310	18.246016
38.993820	1353.226496	18.251034
38.904140	1354.446007	18.256051
39.453124	1348.153079	18.261069
39.029322	1359.409602	18.266087
39.046060	1349.169568	18.271104
39.197785	1354.555036	18.276122
39.334303	1355.297515	18.281139
39.388610	1342.602726	18.286157
39.419927	1353.441246	18.291175
39.617547	1340.575821	18.296192
39.473393	1347.919774	18.301210
39.645692	1345.292588	18.306227
39.651195	1353.462156	18.311245
39.394882	1345.268578	18.316263
39.521686	1346.413358	18.321280
39.720251	1352.608887	18.326298
39.492614	1346.919714	18.331315
39.592104	1345.828121	18.336333
39.552900	1352.770727	18.341351
39.428944	1341.949843	18.346368
39.291808	1343.167274	18.351386
39.558057	1347.603945	18.356403
39.790408	1361.475463	18.361421
39.993927	1364.817369	18.366439
39.937664	1362.481387	18.371456
40.195166	1365.600294	18.376474
40.092613	1368.838376	18.381491
40.311704	1357.711606	18.386509
40.603311	1363.807446	18.391527
40.270560	1347.944518	18.396544
40.171699	1342.942199	18.401562
40.022162	1343.520932	18.406579
40.469400	1343.198862	18.411597
40.231275	1362.331785	18.416615
40.427321	1360.313127	18.421632
40.207029	1361.739168	18.426650
40.472748	1360.609069	18.431667
40.727139	1358.407758	18.436685
40.234984	1363.136081	18.441703
40.413003	1355.057913	18.446720
40.684013	1360.235461	18.451738
40.526788	1360.370422	18.456755
40.644182	1357.676042	18.461773
40.685845	1359.152816	18.466791
40.536232	1360.523671	18.471808
40.601913	1352.873250	18.476826
40.540189	1343.500660	18.481843
40.525875	1345.768789	18.486861
40.804711	1356.458321	18.491879
40.904059	1365.698882	18.496896
41.074484	1365.969023	18.501914
41.137786	1362.219555	18.506931
41.225881	1366.605073	18.511949
41.128657	1370.725954	18.516967
41.474540	1365.114739	18.521984
41.352827	1359.639446	18.527002
41.277367	1369.188093	18.532019
41.320870	1368.054722	18.537037
41.398974	1369.118723	18.542055
41.338322	1357.603161	18.547072
41.603998	1366.183509	18.552090
41.519722	1364.075951	18.557107
41.568970	1366.201642	18.562125
41.298433	1369.563708	18.567143
41.548956	1375.315653	18.572160
41.490197	1368.991108	18.577178
41.656821	1367.671309	18.582195
41.490597	1373.402932	18.587213
41.687301	1372.422434	18.592231
41.553080	1368.448097	18.597248
41.038324	1369.418210	18.602266
41.544644	1385.828549	18.607283
42.114414	1386.292135	18.612301
41.790116	1391.997882	18.617319
41.665172	1385.074562	18.622336
42.159247	1385.145989	18.627354
42.028956	1392.550918	18.632371
42.008166	1384.254380	18.637389
42.156009	1390.356834	18.642407
42.335473	1386.658703	18.647424
42.575426	1386.403621	18.652442
42.418086	1396.384755	18.657459
42.594425	1387.394802	18.662477
41.740532	1392.169986	18.667495
42.393622	1389.319613	18.672512
42.646049	1382.287047	18.677530
42.144557	1386.865351	18.682547
42.447937	1385.243391	18.687565
42.404366	1394.077028	18.692583
42.332235	1385.422408	18.697600
42.588399	1399.132458	18.702618
42.574593	1409.362652	18.707635
42.751992	1407.873915	18.712653
43.031225	1412.217061	18.717671
42.753040	1416.975201	18.722688
42.801467	1419.889982	18.727706
42.839860	1421.708099	18.732723
43.067422	1419.299517	18.737741
43.097843	1421.882585	18.742759
43.162436	1423.463092	18.747776
43.371771	1411.760292	18.752794
43.222272	1408.624618	18.757811
43.579522	1408.931943	18.762829
43.250133	1414.553283	18.767847
42.852969	1409.499559	18.772864
43.120119	1413.213422	18.777882
43.065098	1407.535224	18.782899
43.113961	1407.653878	18.787917
43.163398	1409.189406	18.792935
42.977192	1410.203042	18.797952
43.366412	1428.234810	18.802970
43.516650	1437.243422	18.807987
43.676273	1422.351502	18.813005
43.825786	1432.382711	18.818023
43.329618	1443.196115	18.823040
44.013486	1427.114873	18.828058
43.820924	1425.876240	18.833075
44.000489	1418.132320	18.838093
43.761733	1436.167194	18.843111
43.740539	1429.963011	18.848128
44.097414	1425.678669	18.853146
43.956093	1433.120047	18.858163
44.156532	1428.736984	18.863181
43.947104	1434.077718	18.868199
44.048278	1439.243862	18.873216
44.244358	1427.331675	18.878234
44.079539	1421.910410	18.883251
43.715161	1437.007836	18.888269
43.917610	1445.064731	18.893287
43.953250	1455.596525	18.898304
44.308885	1442.248830	18.903322
44.233718	1454.202219	18.908339
44.643688	1452.970760	18.913357
44.631814	1452.066913	18.918375
44.467998	1449.772912	18.923392
44.861452	1452.712875	18.928410
44.494771	1451.463480	18.933427
44.189126	1442.728424	18.938445
44.493648	1459.776169	18.943463
44.934088	1459.603481	18.948480
45.213694	1459.572599	18.953498
45.124512	1460.006238	18.958515
45.250928	1448.893840	18.963533
44.919810	1439.367482	18.968551
44.943628	1436.772868	18.973568
45.430092	1435.624175	18.978586
45.578633	1436.699304	18.983603
45.347463	1432.077324	18.988621
45.606684	1426.855126	18.993639
45.380099	1442.780021	18.998656
45.823739	1431.078597	19.003674
45.235519	1431.873957	19.008691
45.483698	1425.861367	19.013709
45.704226	1436.459039	19.018727
45.400381	1442.291006	19.023744
45.573820	1429.486087	19.028762
45.485089	1433.078637	19.033779
45.463633	1429.960894	19.038797
46.005625	1441.322721	19.043815
45.542025	1434.022917	19.048832
45.872740	1429.259806	19.053850
45.602523	1443.941787	19.058867
45.650335	1438.253881	19.063885
45.767051	1430.081081	19.068903
45.727823	1428.944808	19.073920
45.853602	1437.278726	19.078938
45.934526	1455.367989	19.083955
45.793302	1458.552147	19.088973
46.113991	1459.092386	19.093991
45.936362	1461.332308	19.099008
46.278049	1462.418392	19.104026
45.783183	1459.285988	19.109043
46.222443	1462.547028	19.114061
46.327057	1454.849476	19.119079
46.036744	1455.847765	19.124096
46.032246	1464.350303	19.129114
46.622890	1477.607545	19.134131
46.347773	1473.866562	19.139149
46.543489	1485.134007	19.144167
46.427170	1486.606986	19.149184
46.628093	1487.033328	19.154202
46.646702	1492.505835	19.159219
46.707604	1488.428507	19.164237
46.099012	1488.703173	19.169255
46.312209	1488.095645	19.174272
46.558633	1501.630563	19.179290
46.699053	1504.625710	19.184307
46.713313	1508.322162	19.189325
47.004633	1514.370761	19.194343
46.753385	1518.474631	19.199360
46.897791	1510.934963	19.204378
46.839001	1522.627068	19.209395
47.184997	1531.346471	19.214413
47.532819	1521.663868	19.219431
47.587119	1521.387195	19.224448
47.899486	1528.956794	19.229466
47.643595	1529.731975	19.234483
47.907459	1515.230851	19.239501
48.241039	1499.402900	19.244519
47.940267	1495.659596	19.249536
47.871718	1484.113623	19.254554
47.446503	1491.103759	19.259571
47.670244	1495.278839	19.264589
47.973832	1485.347520	19.269607
47.860387	1488.981799	19.274624
47.785590	1486.724426	19.279642
47.716327	1485.797955	19.284659
47.786226	1490.451426	19.289677
47.875463	1484.220564	19.294695
47.520926	1492.234810	19.299712
48.078994	1496.468292	19.304730
48.011093	1512.059269	19.309747
47.888693	1516.928882	19.314765
48.530582	1518.135490	19.319783
48.384246	1517.217861	19.324800
48.359845	1519.989361	19.329818
48.082047	1515.194736	19.334835
47.948199	1516.664135	19.339853
48.375092	1516.234776	19.344871
48.032463	1520.741042	19.349888
48.400735	1510.780703	19.354906
48.350608	1518.615021	19.359923
48.381840	1534.329441	19.364941
48.677262	1534.318188	19.369959
48.579955	1538.170873	19.374976
48.312208	1533.368367	19.379994
48.744768	1534.433996	19.385011
48.850002	1539.609005	19.390029
48.875134	1538.235483	19.395047
48.709637	1553.403029	19.400064
49.000004	1556.662022	19.405082
49.267059	1566.567708	19.410099
49.317194	1579.751388	19.415117
49.234555	1563.461157	19.420135
49.082109	1577.111883	19.425152
49.341762	1563.340378	19.430170
49.412029	1570.038804	19.435187
49.128719	1575.195421	19.440205
49.034545	1573.635341	19.445223
49.230451	1567.425712	19.450240
49.290899	1568.962696	19.455258
49.341244	1576.380603	19.460275
49.088680	1585.890668	19.465293
49.727006	1588.246566	19.470311
49.763563	1595.663473	19.475328
49.654543	1593.439818	19.480346
50.121954	1590.870792	19.485363
49.904440	1599.756859	19.490381
49.674806	1585.853230	19.495399
49.899029	1593.130462	19.500416
49.980651	1580.967745	19.505434
50.129508	1574.150048	19.510451
50.492736	1583.264430	19.515469
50.227441	1577.186565	19.520487
50.159652	1585.282442	19.525504
50.063324	1583.968854	19.530522
50.440871	1582.404758	19.535539
50.295816	1578.492022	19.540557
50.616937	1573.907094	19.545575
50.437456	1578.346948	19.550592
50.554329	1590.816491	19.555610
50.787657	1586.728075	19.560627
50.949926	1595.630751	19.565645
50.891671	1586.582547	19.570663
50.933004	1585.944969	19.575680
50.388694	1578.843866	19.580698
50.749658	1591.846615	19.585715
50.811657	1597.978285	19.590733
51.175693	1593.935789	19.595751
51.062363	1596.695900	19.600768
51.064078	1596.619921	19.605786
51.093529	1597.085586	19.610803
51.428459	1599.091086	19.615821
51.120918	1596.904650	19.620839
51.276630	1596.261887	19.625856
51.019312	1596.033731	19.630874
51.200240	1599.259277	19.635891
50.745590	1598.831466	19.640909
51.721240	1591.856632	19.645927
51.668793	1594.708251	19.650944
51.374699	1590.638833	19.655962
51.714261	1594.499253	19.660979
51.193968	1587.889877	19.665997
51.246730	1600.738644	19.671015
51.764797	1608.462446	19.676032
51.641884	1608.153402	19.681050
51.483545	1621.186531	19.686067
51.618644	1621.149746	19.691085
51.729032	1608.963596	19.696103
52.292168	1619.763659	19.701120
52.018701	1620.402722	19.706138
52.014493	1616.780479	19.711155
51.793547	1617.562846	19.716173
52.265879	1631.886370	19.721191
52.434922	1641.567512	19.726208
52.452152	1648.943268	19.731226
52.596006	1636.101781	19.736243
52.274181	1646.231743	19.741261
52.271420	1638.004865	19.746279
52.132175	1643.208500	19.751296
52.106407	1639.520180	19.756314
52.241258	1642.118579	19.761331
52.886054	1633.907649	19.766349
52.876471	1631.201440	19.771367
52.887995	1643.362368	19.776384
52.280469	1645.527231	19.781402
52.939659	1646.797428	19.786419
52.761663	1651.041405	19.791437
53.025891	1656.349486	19.796455
53.376737	1650.475473	19.801472
53.032787	1657.819102	19.806490
52.768285	1652.498496	19.811507
53.080354	1661.109633	19.816525
53.530226	1656.220611	19.821543
53.421789	1649.405073	19.826560
53.438104	1656.260257	19.831578
53.187710	1648.378048	19.836595
52.946362	1655.115555	19.841613
53.217083	1663.685793	19.846631
53.923580	1671.257206	19.851648
53.665536	1673.115190	19.856666
54.090457	1664.042213	19.861683
53.764778	1674.819744	19.866701
53.755312	1673.590457	19.871719
53.832408	1664.921935	19.876736
53.568336	1669.857829	19.881754
53.917065	1665.012954	19.886771
54.031741	1664.562774	19.891789
53.577868	1662.995573	19.896807
53.875931	1672.470448	19.901824
53.706152	1689.352413	19.906842
54.284483	1687.731801	19.911859
54.150473	1689.516826	19.916877
54.539079	1691.504511	19.921895
54.527571	1681.959820	19.926912
54.107991	1682.782583	19.931930
54.606908	1688.628503	19.936947
54.377547	1682.074783	19.941965
54.297175	1677.066335	19.946983
54.302258	1690.137189	19.952000
54.767223	1707.447375	19.957018
55.215216	1710.814402	19.962035
55.298454	1709.532808	19.967053
55.132900	1700.005780	19.972071
54.716210	1691.410969	19.977088
54.900368	1703.791219	19.982106
55.093842	1712.932097	19.987123
54.943403	1715.720096	19.992141
54.998727	1709.977284	19.997159
55.420195	1711.877802	20.002176
55.093703	1710.808327	20.007194
55.631116	1704.873691	20.012211
55.042985	1710.134611	20.017229
55.204180	1709.648784	20.022247
55.628796	1701.191231	20.027264
55.280821	1710.163939	20.032282
55.261871	1713.578419	20.037299
55.340843	1711.634756	20.042317
55.654423	1721.722637	20.047335
55.832261	1738.405356	20.052352
55.565361	1734.240151	20.057370
55.537767	1729.286589	20.062387
56.059149	1731.685962	20.067405
56.255222	1730.500411	20.072423
56.016998	1730.553309	20.077440
55.882738	1733.903693	20.082458
56.018493	1727.002769	20.087475
55.759412	1722.804790	20.092493
56.177813	1728.492842	20.097511
56.292546	1745.463110	20.102528
56.175452	1749.972189	20.107546
56.691759	1740.932283	20.112563
56.880588	1743.118340	20.117581
56.213827	1747.637258	20.122599
56.438442	1735.976049	20.127616
56.721240	1750.761533	20.132634
56.811469	1743.410088	20.137651
56.717219	1745.416151	20.142669
56.780790	1744.986549	20.147687
57.063991	1744.216632	20.152704
56.975263	1746.082977	20.157722
56.796930	1741.585237	20.162739
56.453042	1749.433834	20.167757
56.943904	1759.001817	20.172775
57.251294	1760.522461	20.177792
57.361386	1762.405191	20.182810
57.255445	1761.067839	20.187827
57.539925	1767.789793	20.192845
57.311688	1772.022685	20.197863
57.538735	1765.334756	20.202880
57.524968	1764.153470	20.207898
57.459919	1756.075095	20.212915
58.106896	1758.502255	20.217933
57.263518	1763.061298	20.222951
57.805600	1757.848615	20.227968
57.549438	1772.181531	20.232986
57.548726	1778.670173	20.238003
57.879454	1785.040941	20.243021
57.961472	1785.987590	20.248039
58.099847	1784.539612	20.253056
57.957458	1790.677923	20.258074
58.134163	1786.756072	20.263091
57.959946	1796.686407	20.268109
58.115130	1793.904025	20.273127
58.250094	1786.662365	20.278144
58.136058	1799.590894	20.283162
58.494014	1811.798989	20.288179
58.714981	1811.499518	20.293197
58.533452	1823.012109	20.298215
58.832826	1813.844991	20.303232
58.766172	1817.528858	20.308250
58.994598	1813.643131	20.313267
59.258820	1808.505253	20.318285
59.185364	1800.349269	20.323303
59.249323	1794.870180	20.328320
58.845787	1785.604227	20.333338
59.011568	1780.229213	20.338355
59.342280	1790.270284	20.343373
59.241692	1786.350579	20.348391
59.005820	1784.471706	20.353408
59.060465	1793.343899	20.358426
59.061982	1797.941824	20.363443
59.395025	1798.619010	20.368461
59.250447	1796.732234	20.373479
59.234708	1793.294792	20.378496
59.054460	1798.182955	20.383514
59.192482	1805.353772	20.388531
59.307501	1821.756007	20.393549
59.421098	1831.168166	20.398567
59.768476	1836.315029	20.403584
59.554380	1831.930134	20.408602
59.758269	1837.354964	20.413619
59.951954	1829.195246	20.418637
59.471055	1834.401635	20.423655
59.804086	1847.077551	20.428672
59.904381	1855.728067	20.433690
60.159149	1848.761227	20.438707
60.189751	1843.293629	20.443725
60.129237	1855.645804	20.448743
60.363719	1843.714737	20.453760
60.109644	1861.989117	20.458778
60.253537	1868.963379	20.463795
60.592292	1875.538064	20.468813
60.601354	1881.507654	20.473831
60.793866	1879.328537	20.478848
60.883625	1886.390131	20.483866
60.981059	1877.674157	20.488883
60.947498	1877.597357	20.493901
61.015464	1878.003383	20.498919
61.377147	1869.725968	20.503936
61.125856	1871.526115	20.508954
60.979367	1862.128580	20.513971
61.056186	1868.131799	20.518989
60.915396	1865.935147	20.524007
60.924461	1880.450924	20.529024
61.475422	1891.496053	20.534042
61.612129	1890.180874	20.539059
61.706285	1896.787338	20.544077
61.508129	1902.637714	20.549095
61.633993	1893.077834	20.554112
61.540530	1903.339649	20.559130
61.406021	1895.423509	20.564147
61.847628	1895.130712	20.569165
61.900924	1891.524707	20.574183
62.138317	1890.664083	20.579200
61.978897	1897.720295	20.584218
61.998341	1894.684468	20.589235
61.774743	1898.395942	20.594253
62.089785	1913.918180	20.599271
62.531573	1920.107598	20.604288
62.521292	1922.217377	20.609306
62.883840	1913.071932	20.614323
63.073355	1913.042453	20.619341
62.798077	1898.886901	20.624359
62.905088	1886.199299	20.629376
62.911195	1884.181752	20.634394
62.707539	1887.132702	20.639411
62.946555	1880.676403	20.644429
62.726253	1885.062726	20.649447
62.675173	1877.262996	20.654464
63.187011	1879.761708	20.659482
62.723887	1882.327008	20.664499
62.891195	1885.235980	20.669517
62.916726	1899.531451	20.674535
62.976468	1909.330745	20.679552
63.380626	1917.236524	20.684570
63.063843	1912.116491	20.689587
63.430870	1910.689710	20.694605
63.411856	1912.305369	20.699623
63.471013	1904.460061	20.704640
63.588827	1906.512023	20.709658
63.466309	1908.819161	20.714675
63.642608	1905.506438	20.719693
63.300549	1911.596980	20.724711
63.618054	1917.067264	20.729728
63.538095	1928.327415	20.734746
63.783496	1927.276187	20.739763
63.733196	1934.807747	20.744781
63.944436	1937.940270	20.749799
64.020978	1929.959695	20.754816
64.392652	1929.933415	20.759834
64.021731	1936.233593	20.764851
64.726991	1937.165269	20.769869
64.795299	1943.516989	20.774887
64.511700	1936.804355	20.779904
64.499344	1928.525186	20.784922
64.871633	1940.526003	20.789939
65.054540	1936.612621	20.794957
64.766873	1930.339296	20.799975
64.725003	1929.989225	20.804992
64.816400	1931.426743	20.810010
65.070699	1951.496678	20.815027
65.320188	1939.493780	20.820045
64.869638	1944.269428	20.825063
64.843742	1943.399299	20.830080
65.129871	1944.279462	20.835098
65.129733	1945.557658	20.840115
65.238439	1939.317294	20.845133
65.043004	1942.711957	20.850151
65.064374	1943.948933	20.855168
65.260868	1949.636891	20.860186
65.203739	1959.921485	20.865203
66.018364	1959.356008	20.870221
65.654307	1963.894124	20.875239
65.921697	1965.266374	20.880256
66.053848	1964.516809	20.885274
65.644506	1962.986829	20.890291
66.135550	1949.362045	20.895309
65.713596	1959.583515	20.900327
66.214910	1957.062810	20.905344
66.235119	1956.131852	20.910362
65.944250	1963.101254	20.915379
66.504213	1962.584894	20.920397
66.435609	1979.568150	20.925415
66.766457	1973.757108	20.930432
66.577629	1968.639228	20.935450
66.435969	1967.320045	20.940467
66.393272	1970.974966	20.945485
66.649493	1971.809292	20.950503
66.775424	1973.026835	20.955520
66.596639	1968.560667	20.960538
66.611140	1977.335056	20.965555
66.768993	1963.667459	20.970573
66.938283	1977.157941	20.975591
67.059246	1977.407390	20.980608
67.280605	1981.901703	20.985626
67.096218	1997.833145	20.990643
67.267566	2001.006605	20.995661
67.266037	2003.358037	21.000679
67.214431	1997.890567	21.005696
67.485213	2001.676575	21.010714
66.739619	2008.353861	21.015731
67.506654	1995.651785	21.020749
66.955231	1997.123118	21.025767
67.504715	2017.784666	21.030784
67.647178	2013.091738	21.035802
67.672670	2028.962127	21.040819
67.895112	2024.878462	21.045837
67.659491	2022.049590	21.050855
67.937492	2027.434536	21.055872
68.172342	2031.888891	21.060890
67.832209	2046.083614	21.065907
68.040293	2039.928732	21.070925
68.403109	2056.778617	21.075943
68.481239	2047.980355	21.080960
68.518128	2050.464673	21.085978
68.441918	2053.367404	21.090995
68.710452	2043.267657	21.096013
68.814949	2045.233343	21.101031
68.546854	2048.980179	21.106048
68.658581	2042.259607	21.111066
68.739121	2062.634442	21.116083
69.178383	2058.513856	21.121101
69.036242	2064.140960	21.126119
69.110692	2075.957856	21.131136
69.344885	2062.486590	21.136154
69.070042	2071.602732	21.141171
69.355833	2064.192304	21.146189
69.291420	2071.508359	21.151207
69.300990	2071.118716	21.156224
69.712929	2060.283391	21.161242
69.649777	2057.594925	21.166259
69.805799	2064.699925	21.171277
69.689254	2056.335928	21.176295
70.086120	2068.165740	21.181312
70.217859	2067.605592	21.186330
69.964336	2077.482155	21.191347
70.086452	2076.282849	21.196365
70.314502	2078.948856	21.201383
70.200006	2080.598332	21.206400
70.482498	2080.642745	21.211418
70.448067	2069.902158	21.216435
70.364925	2074.481775	21.221453
70.480040	2075.738880	21.226471
70.446417	2066.803367	21.231488
70.575740	2070.434682	21.236506
70.572144	2076.920726	21.241523
70.387674	2081.036418	21.246541
70.633965	2073.092470	21.251559
70.468599	2087.749186	21.256576
70.742892	2088.157809	21.261594
70.695696	2102.092363	21.266611
70.928807	2107.894596	21.271629
70.986119	2093.052763	21.276647
70.829835	2107.291497	21.281664
71.195247	2104.208081	21.286682
71.520501	2123.926320	21.291699
71.445866	2121.324843	21.296717
71.584959	2127.226931	21.301735
71.342354	2124.885146	21.306752
71.426382	2125.885151	21.311770
71.792313	2131.174384	21.316787
71.561502	2128.120673	21.321805
71.865887	2128.000724	21.326823
71.860324	2136.708884	21.331840
71.906031	2132.892564	21.336858
71.826146	2132.879782	21.341875
71.701230	2144.248059	21.346893
71.973318	2148.428389	21.351911
71.971311	2152.376827	21.356928
72.176977	2146.575752	21.361946
72.067795	2161.327928	21.366963
72.326629	2159.091113	21.371981
72.371323	2168.630948	21.376999
72.223476	2180.533019	21.382016
72.473037	2177.170968	21.387034
72.502272	2177.005490	21.392051
72.645006	2174.770970	21.397069
72.969305	2180.795726	21.402087
72.823615	2194.796183	21.407104
73.339163	2186.721896	21.412122
73.453502	2191.460154	21.417139
72.990712	2195.234177	21.422157
73.269342	2195.099302	21.427175
73.229291	2199.233563	21.432192
73.636867	2196.500191	21.437210
73.372795	2196.677040	21.442227
73.531666	2201.509358	21.447245
73.807453	2205.354594	21.452263
73.320453	2200.456648	21.457280
73.753937	2202.355350	21.462298
73.837271	2217.787690	21.467315
73.919028	2214.139317	21.472333
74.109754	2219.408516	21.477351
74.281221	2218.722251	21.482368
74.178665	2221.502872	21.487386
74.101739	2220.274583	21.492403
74.049831	2215.621332	21.497421
74.231020	2213.879462	21.502439
74.213770	2222.015098	21.507456
74.636144	2229.886621	21.512474
74.570753	2234.880103	21.517491
74.755495	2236.937463	21.522509
75.353476	2233.347577	21.527527
74.992934	2234.669282	21.532544
75.634831	2227.275930	21.537562
75.575858	2233.117367	21.542579
75.318495	2226.072319	21.547597
75.687107	2222.805339	21.552615
75.458938	2221.515386	21.557632
75.415054	2199.746096	21.562650
75.544705	2203.367919	21.567667
75.626347	2215.773953	21.572685
75.971122	2222.123756	21.577703
75.505682	2227.548768	21.582720
75.618410	2212.635089	21.587738
75.520826	2223.427931	21.592755
75.700584	2228.399023	21.597773
75.751707	2219.952038	21.602791
75.785932	2220.925087	21.607808
75.774234	2218.171778	21.612826
76.093012	2231.613931	21.617843
75.862758	2237.699799	21.622861
76.129083	2244.011328	21.627879
76.329829	2252.122505	21.632896
76.100669	2252.385442	21.637914
76.348015	2252.179693	21.642931
76.343322	2255.942370	21.647949
76.467602	2257.693549	21.652967
76.511071	2271.181751	21.657984
76.738618	2280.428075	21.663002
76.805337	2272.647704	21.668019
77.227994	2277.612552	21.673037
77.338927	2274.628692	21.678055
77.345416	2281.684471	21.683072
77.381118	2280.773176	21.688090
77.246989	2273.784665	21.693107
77.084614	2276.890206	21.698125
77.398464	2266.410874	21.703143
77.067766	2276.457361	21.708160
77.464146	2281.805018	21.713178
77.602840	2294.072828	21.718195
77.247721	2287.106095	21.723213
77.793197	2286.336349	21.728231
77.772011	2291.225129	21.733248
77.737786	2284.773356	21.738266
77.990488	2294.388176	21.743283
77.809815	2303.297260	21.748301
78.342716	2303.520449	21.753319
78.606793	2301.077662	21.758336
78.865724	2296.312875	21.763354
78.624467	2288.690906	21.768371
78.382305	2294.425177	21.773389
78.562257	2291.316953	21.778407
78.761578	2299.074904	21.783424
78.806822	2293.620668	21.788442
79.060621	2281.799918	21.793459
78.763101	2295.404348	21.798477
78.703566	2292.532237	21.803495
78.623664	2298.534753	21.808512
79.029786	2310.707287	21.813530
79.538809	2318.066713	21.818547
79.416956	2325.865212	21.823565
79.105534	2314.672115	21.828583
79.306293	2320.198572	21.833600
79.279742	2319.779832	21.838618
79.316020	2333.326008	21.843635
79.521847	2347.104588	21.848653
79.602368	2344.008680	21.853671
79.656763	2343.132343	21.858688
79.768346	2340.347197	21.863706
80.042087	2348.087271	21.868723
80.005564	2357.134893	21.873741
80.025794	2361.938345	21.878759
80.056096	2364.559439	21.883776
80.192438	2375.760947	21.888794
80.544234	2361.671508	21.893811
80.511086	2373.375958	21.898829
80.858182	2369.329615	21.903847
80.702524	2357.926036	21.908864
80.580915	2366.731275	21.913882
80.992239	2374.279516	21.918899
81.127962	2396.129455	21.923917
81.202959	2384.623671	21.928935
81.142928	2398.137551	21.933952
81.159751	2392.009171	21.938970
81.450606	2385.838129	21.943987
81.366703	2395.350766	21.949005
81.413278	2391.512164	21.954023
81.246055	2392.759598	21.959040
80.977654	2386.606195	21.964058
81.401847	2394.717364	21.969075
81.179998	2414.129760	21.974093
81.649910	2398.159863	21.979111
81.385468	2404.614050	21.984128
81.347980	2408.962568	21.989146
82.244603	2428.424917	21.994163
81.897176	2440.695926	21.999181
82.047529	2432.858280	22.004199
82.100375	2433.156213	22.009216
82.125533	2428.746544	22.014234
82.402320	2430.186800	22.019251
82.354039	2447.997364	22.024269
82.815133	2454.158715	22.029287
82.740156	2459.074852	22.034304
82.667654	2455.191655	22.039322
82.700631	2451.181577	22.044339
83.042409	2453.072492	22.049357
82.800233	2451.128253	22.054375
83.071843	2449.025122	22.059392
82.907915	2461.428532	22.064410
83.270915	2461.289987	22.069427
83.115546	2477.741234	22.074445
83.341297	2476.484738	22.079463
83.353252	2483.940559	22.084480
83.242367	2484.765791	22.089498
83.498657	2469.898978	22.094515
83.935591	2493.166527	22.099533
83.687200	2501.082640	22.104551
84.234263	2504.232410	22.109568
84.535419	2495.430765	22.114586
84.359533	2488.767429	22.119603
84.618742	2490.090498	22.124621
84.723095	2490.011159	22.129639
84.320363	2489.291198	22.134656
84.682425	2493.173560	22.139674
84.819404	2494.768141	22.144691
84.809313	2493.074961	22.149709
84.801274	2488.559986	22.154727
84.665476	2479.551806	22.159744
84.772520	2491.196634	22.164762
85.117756	2482.545933	22.169779
84.700128	2492.157921	22.174797
85.119976	2489.520431	22.179815
85.107172	2502.446330	22.184832
85.214677	2513.810215	22.189850
85.499872	2513.197757	22.194867
85.364214	2519.947536	22.199885
85.497843	2515.842872	22.204903
85.459928	2512.705410	22.209920
85.401364	2526.061357	22.214938
85.612387	2526.896436	22.219955
86.196779	2538.577435	22.224973
86.292871	2534.494391	22.229991
86.207191	2543.922171	22.235008
86.152549	2532.329172	22.240026
86.215222	2530.722496	22.245043
86.160546	2539.296478	22.250061
86.163618	2536.720714	22.255079
86.434039	2544.919013	22.260096
86.707945	2555.341770	22.265114
86.804822	2550.971402	22.270131
87.277964	2565.986721	22.275149
87.185810	2554.150222	22.280167
87.441404	2553.943187	22.285184
87.311482	2549.431392	22.290202
87.579266	2547.723348	22.295219
87.296686	2541.471107	22.300237
87.544738	2539.882908	22.305255
88.153927	2541.113619	22.310272
87.555626	2521.611068	22.315290
87.791695	2504.219404	22.320307
87.622021	2521.048484	22.325325
87.823736	2527.032479	22.330343
88.307949	2524.615352	22.335360
88.270756	2539.918402	22.340378
88.994297	2539.108300	22.345395
88.381668	2517.679654	22.350413
88.213846	2519.043963	22.355431
88.345417	2511.146087	22.360448
88.021801	2510.413807	22.365466
88.331570	2512.622159	22.370483
88.801265	2535.180872	22.375501
88.615031	2537.444358	22.380519
88.941433	2539.104131	22.385536
88.400900	2542.407459	22.390554
88.673229	2538.243323	22.395571
88.505088	2541.100481	22.400589
88.613268	2538.931259	22.405607
89.075193	2548.377933	22.410624
88.745919	2557.461768	22.415642
88.903963	2556.919602	22.420659
88.881858	2562.146293	22.425677
88.866746	2567.072075	22.430695
89.468059	2570.377524	22.435712
89.255038	2584.518165	22.440730
89.425875	2588.540782	22.445747
89.841597	2605.079969	22.450765
89.499973	2611.704048	22.455783
89.639707	2610.363098	22.460800
89.650851	2617.730733	22.465818
89.614741	2615.899570	22.470835
89.838402	2626.320724	22.475853
89.851532	2636.560051	22.480871
90.088279	2638.344253	22.485888
89.999475	2658.080207	22.490906
90.025814	2656.441304	22.495923
90.161196	2666.156648	22.500941
90.325035	2677.335127	22.505959
90.769478	2674.712717	22.510976
91.027343	2681.947284	22.515994
91.253834	2677.089611	22.521011
91.307773	2673.281362	22.526029
91.305799	2701.540949	22.531047
91.210006	2698.901653	22.536064
91.274723	2705.399381	22.541082
91.724145	2703.940775	22.546099
91.628424	2705.006671	22.551117
91.588761	2698.520879	22.556135
91.811409	2695.150299	22.561152
92.103456	2723.834395	22.566170
92.445616	2719.009198	22.571187
92.436666	2717.811320	22.576205
92.307309	2727.343834	22.581223
92.210387	2722.044157	22.586240
92.549241	2729.603831	22.591258
92.581362	2714.478205	22.596275
92.609329	2718.778735	22.601293
92.566424	2711.719041	22.606311
92.510489	2710.620004	22.611328
92.682612	2720.629481	22.616346
93.116835	2733.110377	22.621363
92.990710	2743.450348	22.626381
93.054299	2737.235667	22.631399
93.505263	2734.413403	22.636416
93.334032	2732.536989	22.641434
93.101108	2727.242704	22.646451
93.708537	2746.996599	22.651469
93.882294	2758.445006	22.656487
94.284188	2750.912069	22.661504
94.036033	2753.623915	22.666522
93.947321	2738.744317	22.671539
94.238508	2748.627967	22.676557
94.006105	2762.604495	22.681575
94.263701	2762.687503	22.686592
94.104111	2763.829624	22.691610
94.440758	2763.622592	22.696627
94.461297	2762.038236	22.701645
94.162653	2764.369749	22.706663
94.404749	2756.536615	22.711680
94.707828	2765.945014	22.716698
94.878057	2770.766250	22.721715
94.956330	2772.177475	22.726733
94.767570	2787.608484	22.731751
95.215124	2776.858710	22.736768
95.235965	2786.645605	22.741786
94.935833	2778.480281	22.746803
95.039841	2778.675573	22.751821
94.788564	2794.687569	22.756839
95.341215	2802.548530	22.761856
95.255390	2809.906093	22.766874
94.806707	2810.165342	22.771891
95.338297	2823.369662	22.776909
95.322655	2838.335067	22.781927
95.830578	2843.706556	22.786944
95.999083	2849.197170	22.791962
96.054135	2856.210897	22.796979
96.428345	2855.300523	22.801997
96.142290	2857.039901	22.807015
96.983523	2863.183239	22.812032
97.012834	2871.640152	22.817050
96.795025	2874.170551	22.822067
97.288444	2866.645409	22.827085
97.025968	2876.394405	22.832103
97.092511	2872.401100	22.837120
97.048311	2872.206020	22.842138
96.764472	2866.733413	22.847155
97.151048	2870.602573	22.852173
97.273902	2870.100593	22.857191
97.575982	2883.867757	22.862208
97.616576	2887.935967	22.867226
97.777314	2897.202480	22.872243
97.736426	2899.579094	22.877261
97.859742	2911.625640	22.882279
97.665087	2895.859765	22.887296
98.010438	2909.904259	22.892314
97.822977	2922.731410	22.897331
98.631910	2916.293317	22.902349
98.485251	2919.579574	22.907367
98.796453	2910.829816	22.912384
98.879186	2917.438435	22.917402
98.649428	2927.396979	22.922419
98.767830	2915.701044	22.927437
98.738566	2927.118045	22.932455
98.837275	2937.486244	22.937472
99.103364	2946.045196	22.942490
99.005785	2946.754757	22.947507
99.297949	2934.599371	22.952525
99.100075	2937.454909	22.957543
99.470446	2947.443115	22.962560
99.764767	2957.916582	22.967578
99.700193	2969.601064	22.972595
99.684904	2962.262392	22.977613
99.634286	2965.921905	22.982631
99.726471	2961.324928	22.987648
99.852267	2978.465072	22.992666
100.561295	2989.233786	22.997683
100.689049	2973.591232	23.002701
100.647707	2984.786068	23.007719
100.879651	2983.799998	23.012736
100.776192	2976.168906	23.017754
100.740499	2980.129083	23.022771
101.130237	2974.482137	23.027789
100.781823	2970.910054	23.032807
100.694841	2976.087001	23.037824
101.018494	2970.242043	23.042842
100.612805	2973.230937	23.047859
101.414895	2986.917175	23.052877
101.199273	2997.466904	23.057895
101.353272	2997.550263	23.062912
101.592179	2989.483973	23.067930
101.226086	2998.813625	23.072947
101.648908	3001.632501	23.077965
101.855370	3024.242281	23.082983
101.834461	3030.283198	23.088000
101.836697	3031.946147	23.093018
101.831720	3033.922674	23.098035
101.852021	3038.161352	23.103053
102.254659	3052.055013	23.108071
102.253692	3057.985527	23.113088
102.577569	3062.817637	23.118106
102.545001	3061.168932	23.123123
102.641137	3069.416700	23.128141
102.854268	3082.326776	23.133159
102.796528	3082.692435	23.138176
102.928270	3077.678976	23.143194
102.717587	3092.674959	23.148211
102.980922	3095.417685	23.153229
103.284389	3101.512275	23.158247
103.527977	3105.687799	23.163264
103.538864	3097.104641	23.168282
103.784320	3108.235965	23.173299
104.025719	3112.086751	23.178317
104.015385	3123.065385	23.183335
104.429299	3126.819880	23.188352
104.383221	3120.325466	23.193370
104.170653	3127.327312	23.198387
104.260599	3119.514554	23.203405
104.486134	3121.518324	23.208423
104.556701	3125.948032	23.213440
104.517231	3123.347246	23.218458
104.480218	3132.297496	23.223475
104.972897	3144.469746	23.228493
104.859429	3154.498681	23.233511
105.149681	3145.755228	23.238528
105.283667	3142.887568	23.243546
105.188665	3167.949434	23.248563
105.717815	3168.984348	23.253581
105.564485	3174.480983	23.258599
105.835422	3172.721892	23.263616
105.750932	3176.329910	23.268634
105.778736	3178.396033	23.273651
105.925033	3169.299401	23.278669
105.704208	3170.356397	23.283687
106.039563	3180.044040	23.288704
106.258941	3193.297243	23.293722
106.123829	3195.931588	23.298739
106.319331	3196.204167	23.303757
106.797778	3203.275201	23.308775
106.420931	3210.141692	23.313792
106.559403	3217.764333	23.318810
106.580068	3219.781074	23.323827
106.701640	3223.139246	23.328845
107.082066	3235.284849	23.333863
107.236948	3232.543323	23.338880
107.256819	3229.090593	23.343898
107.328773	3233.100345	23.348915
107.550115	3228.527378	23.353933
107.875675	3239.422226	23.358951
107.967021	3256.186104	23.363968
108.372868	3250.643874	23.368986
108.181591	3261.032159	23.374003
108.213121	3258.852692	23.379021
108.364672	3261.918994	23.384039
108.291936	3262.548951	23.389056
108.636692	3255.368721	23.394074
108.233447	3256.002794	23.399091
108.406835	3252.819680	23.404109
108.728536	3248.338392	23.409127
108.498657	3249.961752	23.414144
108.592609	3268.142346	23.419162
108.800194	3274.621193	23.424179
109.082790	3275.214766	23.429197
108.924104	3280.298811	23.434215
108.764483	3295.163922	23.439232
109.520388	3296.715867	23.444250
109.384012	3307.647958	23.449267
109.144017	3308.329208	23.454285
109.371914	3315.458231	23.459303
109.696390	3331.093852	23.464320
110.020359	3325.075142	23.469338
110.474567	3319.266557	23.474355
110.805013	3312.271590	23.479373
110.992987	3298.740316	23.484391
111.110168	3295.701659	23.489408
111.745194	3296.306642	23.494426
111.592101	3291.268034	23.499443
111.528209	3295.592472	23.504461
111.619756	3294.423095	23.509479
111.340723	3294.476034	23.514496
111.398912	3292.658527	23.519514
111.614075	3294.039013	23.524531
111.672614	3291.306166	23.529549
111.808472	3286.629716	23.534567
111.603506	3300.009031	23.539584
111.549162	3287.803204	23.544602
111.297183	3287.425851	23.549619
111.459037	3291.491054	23.554637
112.010324	3306.883036	23.559655
112.095667	3324.108712	23.564672
112.282508	3318.193414	23.569690
112.077146	3334.287113	23.574707
112.380087	3339.324552	23.579725
112.855823	3337.732398	23.584743
112.450006	3341.141141	23.589760
112.681094	3344.889429	23.594778
112.905876	3355.478109	23.599795
113.008046	3369.204178	23.604813
113.169717	3367.862913	23.609831
113.755733	3364.492446	23.614848
113.989088	3357.080183	23.619866
114.066340	3357.772009	23.624883
114.132837	3362.435965	23.629901
114.280225	3361.220016	23.634919
113.993931	3363.811643	23.639936
114.325530	3357.731768	23.644954
114.234405	3369.685761	23.649971
114.093877	3356.407583	23.654989
114.196602	3350.420154	23.660007
114.252006	3361.445510	23.665024
114.253992	3373.874215	23.670042
114.635330	3379.309761	23.675059
114.659304	3390.106471	23.680077
114.788857	3376.656826	23.685095
114.612268	3399.143658	23.690112
115.032982	3407.309485	23.695130
115.263445	3424.932434	23.700147
114.892675	3421.322711	23.705165
115.013403	3419.536484	23.710183
114.892525	3434.963790	23.715200
115.369432	3439.383967	23.720218
115.471269	3445.866715	23.725235
115.873674	3456.008028	23.730253
115.975369	3459.353557	23.735271
115.839792	3461.621896	23.740288
116.147090	3454.747257	23.745306
116.331190	3461.163548	23.750323
116.425285	3463.030012	23.755341
116.742581	3474.869988	23.760359
116.830162	3474.793257	23.765376
116.678710	3477.799460	23.770394
116.586046	3486.840611	23.775411
116.812141	3488.396157	23.780429
116.997026	3494.099039	23.785447
117.186878	3505.693757	23.790464
117.203094	3511.691181	23.795482
117.014581	3509.261885	23.800499
117.232171	3524.406170	23.805517
117.573397	3530.094191	23.810535
117.857420	3536.627511	23.815552
117.990950	3539.608293	23.820570
118.050111	3540.770060	23.825587
118.423007	3564.386683	23.830605
118.576754	3557.731596	23.835623
118.694484	3559.165147	23.840640
118.736755	3545.558531	23.845658
118.999240	3552.612827	23.850675
119.110444	3550.417764	23.855693
119.220337	3546.995144	23.860711
119.208965	3557.696459	23.865728
119.592535	3569.380994	23.870746
119.792684	3569.583420	23.875763
119.540056	3577.967781	23.880781
119.406051	3568.318067	23.885799
119.158119	3576.079924	23.890816
119.324359	3571.600668	23.895834
119.676722	3583.892905	23.900851
119.887342	3602.289232	23.905869
119.814941	3601.385232	23.910887
120.038390	3614.868515	23.915904
119.885582	3610.315829	23.920922
120.093208	3624.224515	23.925939
120.806575	3631.385392	23.930957
121.106274	3652.557993	23.935975
120.797506	3665.429808	23.940992
121.219523	3652.411013	23.946010
121.132136	3649.823924	23.951027
121.404090	3659.761570	23.956045
121.424808	3653.761559	23.961063
121.195890	3655.997111	23.966080
121.559220	3671.598574	23.971098
121.487927	3670.186247	23.976115
121.872038	3679.942319	23.981133
121.968347	3668.189368	23.986151
121.515661	3672.905831	23.991168
122.290760	3686.218063	23.996186
122.578938	3687.022248	24.001203
122.439740	3690.746198	24.006221
122.417951	3688.063672	24.011239
122.399372	3702.913473	24.016256
122.601314	3709.159795	24.021274
123.088798	3706.366415	24.026291
123.061188	3711.474360	24.031309
123.112029	3710.885727	24.036327
123.500378	3721.155627	24.041344
123.691304	3719.708783	24.046362
123.841915	3722.967840	24.051379
123.539049	3735.150728	24.056397
124.082337	3725.335512	24.061415
123.992340	3726.470013	24.066432
123.950559	3729.765338	24.071450
124.717433	3739.869004	24.076467
124.280480	3757.163786	24.081485
124.519950	3752.092336	24.086503
124.409698	3749.249981	24.091520
124.609787	3749.581824	24.096538
124.623704	3751.624925	24.101555
124.311569	3751.544144	24.106573
124.928328	3774.441330	24.111591
124.694423	3782.794465	24.116608
124.894375	3782.760206	24.121626
125.181866	3790.934324	24.126643
124.862484	3807.058821	24.131661
125.405360	3803.420397	24.136679
125.911523	3821.884559	24.141696
125.999112	3835.916253	24.146714
126.453266	3836.921854	24.151731
126.043201	3839.570694	24.156749
126.405336	3836.620060	24.161767
126.017834	3843.548419	24.166784
126.274659	3857.023530	24.171802
126.769324	3861.059141	24.176819
126.674862	3862.352159	24.181837
126.846211	3864.348668	24.186855
126.820334	3880.749472	24.191872
127.103959	3872.922014	24.196890
127.403219	3877.025927	24.201907
127.515483	3877.639728	24.206925
127.744551	3882.685665	24.211943
127.832227	3898.043022	24.216960
128.006576	3902.810265	24.221978
128.357428	3886.504089	24.226995
128.364691	3888.166335	24.232013
128.711082	3889.337061	24.237031
128.448341	3891.618939	24.242048
128.761833	3884.803142	24.247066
129.601701	3866.160969	24.252083
129.241232	3873.549099	24.257101
129.565672	3868.578013	24.262119
129.503849	3873.672394	24.267136
129.495055	3874.298730	24.272154
129.831506	3872.254778	24.277171
129.480327	3877.529929	24.282189
129.980719	3873.121667	24.287207
129.909148	3869.907146	24.292224
129.766176	3879.887421	24.297242
130.167339	3890.433173	24.302259
130.059662	3900.616277	24.307277
130.123917	3901.433242	24.312295
130.582129	3903.325124	24.317312
130.343994	3896.383737	24.322330
130.545562	3898.476545	24.327347
130.775356	3915.765516	24.332365
130.947041	3915.814565	24.337383
130.946236	3921.208772	24.342400
131.090937	3922.612903	24.347418
131.129079	3932.239914	24.352435
131.137550	3946.672233	24.357453
131.086413	3951.780753	24.362471
131.298386	3954.452702	24.367488
131.425001	3969.785120	24.372506
132.013559	3967.430467	24.377523
131.533320	3979.511727	24.382541
131.501909	3986.230042	24.387559
132.076580	3990.903419	24.392576
132.142824	4000.365121	24.397594
132.526817	4007.192364	24.402611
132.247866	4007.876547	24.407629
132.643456	4023.804702	24.412647
133.136336	4029.519771	24.417664
132.946276	4026.945457	24.422682
133.209111	4020.292153	24.427699
133.282771	4023.048772	24.432717
133.221297	4038.565190	24.437735
133.684333	4041.731476	24.442752
133.302554	4057.073682	24.447770
133.762845	4047.763595	24.452787
133.568109	4063.950977	24.457805
133.769823	4067.255798	24.462823
134.234506	4070.980496	24.467840
133.930234	4076.317839	24.472858
134.731782	4084.314212	24.477875
134.791114	4097.119554	24.482893
134.597779	4090.183742	24.487911
134.770340	4086.991142	24.492928
134.863698	4105.106391	24.497946
135.334606	4116.705089	24.502963
135.309712	4118.091452	24.507981
135.141639	4115.810393	24.512999
135.409300	4123.466961	24.518016
135.440273	4139.306796	24.523034
135.848628	4129.506058	24.528051
135.967692	4142.409447	24.533069
136.232146	4150.921884	24.538087
136.738337	4151.420707	24.543104
136.604304	4156.772601	24.548122
136.928874	4152.423210	24.553139
136.834540	4162.219314	24.558157
136.742402	4160.137900	24.563175
137.278598	4169.927374	24.568192
136.977231	4183.347602	24.573210
137.392976	4187.433450	24.578227
137.516772	4186.596720	24.583245
137.116219	4192.845480	24.588263
137.755206	4193.828638	24.593280
137.798526	4208.290459	24.598298
137.976911	4205.860760	24.603315
138.171087	4218.474753	24.608333
138.006370	4213.541855	24.613351
137.942889	4227.079737	24.618368
138.283783	4237.354164	24.623386
138.432034	4236.589376	24.628403
138.506055	4250.604567	24.633421
138.683820	4258.612915	24.638439
139.053070	4259.663323	24.643456
139.291952	4272.914284	24.648474
139.472521	4281.304121	24.653491
139.530589	4293.005085	24.658509
139.518646	4285.599070	24.663527
139.818171	4280.230898	24.668544
139.806991	4293.754374	24.673562
140.263191	4298.648282	24.678579
140.078075	4315.045865	24.683597
140.047830	4312.159402	24.688615
140.467044	4308.679011	24.693632
140.783809	4324.442950	24.698650
141.140829	4328.358062	24.703667
141.259529	4331.729514	24.708685
141.091050	4339.662395	24.713703
141.358788	4326.862829	24.718720
141.055030	4336.066679	24.723738
141.604533	4336.808115	24.728755
141.642052	4349.825350	24.733773
141.670311	4352.273454	24.738791
141.658157	4357.265547	24.743808
141.966140	4359.158775	24.748826
142.138543	4359.715884	24.753843
141.898236	4368.212320	24.758861
142.210357	4378.084139	24.763879
142.520739	4368.547877	24.768896
142.436124	4383.070789	24.773914
142.704654	4394.571765	24.778931
142.804048	4410.035048	24.783949
142.847057	4409.078319	24.788967
142.783783	4413.428179	24.793984
143.231282	4417.985745	24.799002
142.869749	4429.587995	24.804019
143.005774	4436.169936	24.809037
143.345325	4451.930438	24.814055
143.738690	4458.668016	24.819072
143.666661	4466.412336	24.824090
144.005647	4483.946828	24.829107
144.391632	4487.907968	24.834125
144.622573	4497.805117	24.839143
145.156144	4499.628517	24.844160
145.251078	4496.422680	24.849178
144.995975	4494.076214	24.854195
144.991251	4487.202419	24.859213
145.204602	4508.967084	24.864231
145.506252	4502.146587	24.869248
145.982810	4518.968450	24.874266
145.807515	4510.366262	24.879283
146.175629	4521.627712	24.884301
146.015319	4511.075711	24.889319
146.567004	4531.862913	24.894336
146.796405	4531.798818	24.899354
146.636505	4537.536772	24.904371
146.683995	4538.100710	24.909389
147.091630	4533.637292	24.914407
147.141308	4524.905379	24.919424
147.312657	4524.373711	24.924442
147.831875	4552.138411	24.929459
147.921911	4551.029160	24.934477
147.689992	4551.077921	24.939495
147.751202	4550.724375	24.944512
147.857173	4551.755820	24.949530
147.728979	4546.056459	24.954547
147.836026	4550.925887	24.959565
147.881959	4573.641512	24.964583
147.985142	4571.693773	24.969600
148.147801	4593.674752	24.974618
148.358190	4602.760812	24.979635
148.734970	4609.535749	24.984653
148.533129	4625.358598	24.989671
149.304069	4628.385516	24.994688
149.439960	4627.117614	24.999706
149.377024	4636.350406	25.004723
149.977097	4644.230048	25.009741
149.837661	4659.512937	25.014759
150.383586	4646.070121	25.019776
149.835278	4663.291567	25.024794
150.091243	4653.100786	25.029811
150.660563	4662.598140	25.034829
150.686744	4680.115239	25.039847
150.677578	4683.194180	25.044864
150.612610	4683.870323	25.049882
150.504165	4693.425869	25.054899
150.771057	4700.953390	25.059917
150.731826	4714.323727	25.064935
151.215376	4712.269408	25.069952
151.282495	4733.255383	25.074970
151.561843	4734.910065	25.079987
151.576707	4741.905532	25.085005
151.693164	4760.257727	25.090023
151.830377	4762.123925	25.095040
152.258240	4765.996540	25.100058
151.955528	4777.782395	25.105075
152.128117	4784.188323	25.110093
152.367380	4792.433533	25.115111
152.540784	4811.543923	25.120128
152.745179	4810.596767	25.125146
152.947020	4814.971732	25.130163
152.989799	4823.891457	25.135181
152.896614	4842.068049	25.140199
153.303095	4837.159682	25.145216
153.674621	4853.606813	25.150234
153.984377	4868.674747	25.155251
154.108814	4865.508442	25.160269
154.156557	4875.838343	25.165287
154.445352	4882.349315	25.170304
154.712017	4889.059434	25.175322
154.379812	4890.089678	25.180339
155.112150	4891.225635	25.185357
154.890368	4918.254027	25.190375
154.901146	4916.951925	25.195392
155.459710	4927.672635	25.200410
155.617572	4926.533862	25.205427
155.748507	4933.476611	25.210445
155.541235	4932.337870	25.215463
155.761712	4931.104125	25.220480
156.166396	4947.341010	25.225498
156.031607	4959.312319	25.230515
156.486706	4960.283120	25.235533
156.643067	4973.698951	25.240551
156.782798	4983.799954	25.245568
156.937005	4991.686036	25.250586
157.007947	4995.191306	25.255603
157.294734	5003.801674	25.260621
157.254014	5016.512768	25.265639
157.550863	5019.118001	25.270656
157.856391	5015.276403	25.275674
157.789028	5035.923830	25.280691
158.059376	5037.201167	25.285709
158.156965	5043.457885	25.290727
158.220539	5039.025817	25.295744
158.743545	5056.068214	25.300762
158.887211	5073.914612	25.305779
159.163195	5066.277220	25.310797
159.356547	5061.332532	25.315815
159.576993	5060.597504	25.320832
159.399468	5072.900658	25.325850
159.558300	5079.242547	25.330867
160.009690	5081.230314	25.335885
160.030881	5097.605952	25.340903
159.760565	5086.073298	25.345920
159.978765	5097.532054	25.350938
160.151452	5113.385397	25.355955
160.579574	5101.589327	25.360973
160.680776	5112.173027	25.365991
160.865430	5124.413514	25.371008
160.979152	5137.552022	25.376026
160.760534	5140.698372	25.381043
161.109734	5141.076471	25.386061
161.304317	5156.563449	25.391079
161.386940	5167.298427	25.396096
161.519256	5161.005929	25.401114
161.605023	5174.009931	25.406131
161.973685	5183.169492	25.411149
162.343404	5179.734521	25.416167
162.541077	5177.064954	25.421184
162.795273	5184.348448	25.426202
162.957309	5189.420971	25.431219
163.727356	5191.355982	25.436237
163.328645	5199.801711	25.441255
163.150138	5193.740670	25.446272
163.441381	5192.388570	25.451290
163.435668	5186.635215	25.456307
163.595887	5189.353284	25.461325
163.738769	5202.787166	25.466343
163.641781	5209.951739	25.471360
164.036943	5218.955681	25.476378
164.023599	5231.672132	25.481395
164.555505	5233.085525	25.486413
164.729342	5241.940860	25.491431
164.331476	5242.915059	25.496448
164.801990	5255.663515	25.501466
164.910514	5266.583910	25.506483
164.914066	5271.605374	25.511501
165.314482	5286.792115	25.516519
165.560204	5292.849092	25.521536
165.488839	5294.328005	25.526554
165.985759	5316.519809	25.531571
166.129446	5316.582692	25.536589
166.364772	5330.813499	25.541607
166.495163	5344.419882	25.546624
166.445797	5348.534217	25.551642
166.676814	5344.214892	25.556659
167.029736	5350.646606	25.561677
167.015770	5365.036199	25.566695
167.307018	5362.831827	25.571712
167.297551	5374.638698	25.576730
167.504400	5396.411753	25.581747
167.668472	5395.922228	25.586765
168.120838	5397.707862	25.591783
168.029716	5408.965607	25.596800
168.007279	5413.770200	25.601818
167.922048	5419.449459	25.606835
168.815162	5439.269154	25.611853
169.197395	5442.277818	25.616871
168.963385	5438.753715	25.621888
169.245259	5443.110059	25.626906
169.111761	5464.674192	25.631923
169.855060	5462.825560	25.636941
169.833054	5453.933909	25.641959
169.654898	5470.902782	25.646976
170.531436	5473.831336	25.651994
170.271097	5482.318784	25.657011
170.310532	5477.612592	25.662029
170.182999	5493.020588	25.667047
170.537665	5503.893334	25.672064
171.020929	5503.796027	25.677082
170.944018	5515.506168	25.682100
171.231454	5521.793468	25.687117
171.282902	5540.339651	25.692135
171.418989	5544.914423	25.697152
171.938203	5556.563345	25.702170
171.699633	5568.570151	25.707188
172.228280	5563.279567	25.712205
172.627621	5565.673218	25.717223
173.011469	5582.583105	25.722240
172.791233	5584.230420	25.727258
172.790194	5583.034276	25.732276
173.144207	5575.968486	25.737293
173.299735	5587.658267	25.742311
173.231158	5604.307174	25.747328
173.267529	5609.367814	25.752346
173.120549	5614.463314	25.757364
173.355461	5634.672945	25.762381
173.805502	5628.728546	25.767399
173.417933	5643.084984	25.772416
174.172679	5657.740229	25.777434
174.316084	5663.939523	25.782452
174.713685	5659.767799	25.787469
175.129129	5668.686736	25.792487
175.394589	5673.370818	25.797504
175.893799	5670.284915	25.802522
176.106052	5670.785357	25.807540
176.005652	5663.581947	25.812557
176.389552	5657.938240	25.817575
176.355825	5661.576727	25.822592
176.531704	5656.956569	25.827610
176.403965	5655.868530	25.832628
176.548430	5658.671193	25.837645
176.655026	5671.318772	25.842663
176.782638	5678.732653	25.847680
176.960991	5683.925880	25.852698
176.799506	5692.356999	25.857716
177.081127	5711.359946	25.862733
177.540435	5714.495546	25.867751
177.431338	5713.988567	25.872768
177.421953	5728.627104	25.877786
177.648073	5751.884333	25.882804
177.760432	5765.418080	25.887821
177.949581	5771.269378	25.892839
178.350810	5780.607253	25.897856
178.367137	5787.464004	25.902874
178.613829	5803.167538	25.907892
179.137893	5821.842448	25.912909
179.155266	5827.890964	25.917927
178.947378	5834.138695	25.922944
179.286137	5848.618958	25.927962
179.323855	5855.908015	25.932980
179.652546	5868.278096	25.937997
179.777764	5881.124944	25.943015
179.802532	5896.771568	25.948032
180.125015	5896.743486	25.953050
180.197283	5911.306324	25.958068
180.684387	5922.831060	25.963085
181.328679	5924.836239	25.968103
181.478296	5951.997736	25.973120
181.890114	5945.948705	25.978138
181.987221	5944.421595	25.983156
182.054347	5939.748852	25.988173
182.396995	5941.542154	25.993191
182.267958	5962.083437	25.998208
182.808760	5965.701982	26.003226
182.955410	5967.137537	26.008244
183.054680	5968.773021	26.013261
183.198550	5970.849803	26.018279
182.807279	5980.806754	26.023296
183.189721	5990.943132	26.028314
183.125793	5992.938629	26.033332
183.452996	6013.004890	26.038349
183.725234	6028.117508	26.043367
183.715204	6035.275179	26.048384
184.214456	6044.342242	26.053402
184.312526	6052.660514	26.058420
184.428481	6059.435567	26.063437
184.752561	6068.637240	26.068455
184.701682	6075.555069	26.073472
184.862752	6080.886836	26.078490
185.348602	6099.650055	26.083508
185.035894	6106.933793	26.088525
185.634178	6119.688219	26.093543
185.629902	6126.463076	26.098560
186.154111	6139.967704	26.103578
186.320875	6151.457229	26.108596
186.099212	6157.426273	26.113613
186.795557	6155.272377	26.118631
186.597037	6170.363705	26.123648
187.018817	6182.066079	26.128666
186.989881	6187.029720	26.133684
187.326533	6181.579452	26.138701
187.234570	6191.505702	26.143719
187.277715	6209.551949	26.148736
187.739163	6211.238396	26.153754
188.175799	6229.176051	26.158772
187.922129	6234.758677	26.163789
188.460678	6230.934210	26.168807
188.697763	6250.474974	26.173824
188.794217	6251.331226	26.178842
189.060681	6259.396095	26.183860
189.266489	6259.124174	26.188877
190.053137	6259.307927	26.193895
190.324693	6265.105517	26.198912
190.388492	6271.371075	26.203930
190.162462	6265.954722	26.208948
190.518706	6272.676661	26.213965
190.870824	6263.691645	26.218983
190.793377	6275.604383	26.224000
190.724682	6284.561119	26.229018
191.176290	6297.600510	26.234036
190.675162	6292.116495	26.239053
191.276702	6306.950794	26.244071
191.272956	6318.656372	26.249088
191.412794	6336.510917	26.254106
191.723766	6347.561432	26.259124
191.775422	6359.712973	26.264141
191.997001	6370.695346	26.269159
192.081261	6377.115589	26.274176
192.564469	6390.289021	26.279194
192.403475	6398.565710	26.284212
192.724293	6415.602982	26.289229
193.080197	6419.805985	26.294247
193.119457	6438.992632	26.299264
193.203232	6453.017472	26.304282
193.562597	6450.300450	26.309300
193.680553	6478.547253	26.314317
194.066663	6481.176683	26.319335
194.236405	6504.481529	26.324352
194.337131	6512.417635	26.329370
194.946271	6512.291260	26.334388
195.023312	6532.725338	26.339405
195.754250	6542.750946	26.344423
195.484945	6545.993815	26.349440
195.553667	6549.048318	26.354458
195.908994	6550.350416	26.359476
195.875301	6560.545585	26.364493
196.346555	6570.046584	26.369511
196.155288	6590.083714	26.374528
196.485639	6595.556584	26.379546
196.436281	6598.784159	26.384564
196.364680	6614.620021	26.389581
196.937009	6627.580875	26.394599
197.048336	6642.558061	26.399616
197.230940	6648.489578	26.404634
197.450486	6651.782627	26.409652
197.843891	6663.799088	26.414669
198.370241	6672.234055	26.419687
198.478901	6677.144839	26.424704
198.593192	6687.481190	26.429722
198.853519	6696.080698	26.434740
198.797204	6710.225404	26.439757
199.000668	6712.523435	26.444775
199.481885	6730.997604	26.449792
199.521374	6738.605570	26.454810
199.758642	6726.784505	26.459828
199.567365	6738.061818	26.464845
200.127747	6747.978352	26.469863
200.309307	6759.854237	26.474880
200.332146	6769.737673	26.479898
200.567794	6766.294872	26.484916
200.900351	6780.849447	26.489933
201.208430	6781.884279	26.494951
201.408825	6801.024121	26.499968
201.249304	6807.624524	26.504986
201.570660	6806.498064	26.510004
201.465768	6830.502690	26.515021
201.771295	6839.641349	26.520039
202.041503	6839.397276	26.525056
202.217362	6861.394721	26.530074
202.531840	6867.397325	26.535092
202.762220	6879.628716	26.540109
203.387597	6888.591332	26.545127
203.664197	6905.522302	26.550144
203.143563	6922.507958	26.555162
203.945218	6915.043656	26.560180
204.129872	6941.064727	26.565197
204.082592	6937.138759	26.570215
204.271759	6932.096360	26.575232
204.394747	6949.651075	26.580250
204.732803	6957.285254	26.585268
204.727206	6974.190773	26.590285
205.286431	6986.023791	26.595303
205.125335	6986.781276	26.600320
205.416442	7007.226752	26.605338
205.975737	7006.940826	26.610356
205.745835	7040.040986	26.615373
205.969649	7036.530528	26.620391
206.330170	7044.814705	26.625408
206.395869	7065.049107	26.630426
206.816456	7071.950733	26.635444
206.575637	7099.496716	26.640461
207.331968	7102.687334	26.645479
207.449818	7118.326824	26.650496
207.422557	7132.773544	26.655514
207.795013	7144.152748	26.660532
207.926861	7161.965147	26.665549
208.337885	7161.898027	26.670567
208.671921	7167.531493	26.675584
208.583472	7184.102853	26.680602
208.964447	7184.441328	26.685620
209.116247	7202.575813	26.690637
209.219516	7212.933118	26.695655
209.343820	7220.373394	26.700672
209.369911	7238.732680	26.705690
209.981125	7240.973610	26.710708
209.925695	7258.265969	26.715725
210.098556	7267.018264	26.720743
210.533090	7274.072481	26.725760
210.875636	7285.589018	26.730778
211.386357	7301.603144	26.735796
211.489963	7314.924735	26.740813
211.520657	7317.019291	26.745831
211.884240	7314.708721	26.750848
212.014721	7332.906635	26.755866
212.115529	7331.498795	26.760884
212.414625	7339.410690	26.765901
212.703728	7354.685936	26.770919
213.207984	7356.255338	26.775936
212.970491	7356.162909	26.780954
213.301450	7353.203944	26.785972
213.313563	7378.551676	26.790989
213.457155	7379.946780	26.796007
213.935629	7383.654237	26.801024
213.932303	7411.637242	26.806042
214.072229	7413.730587	26.811060
214.256724	7415.485522	26.816077
214.240819	7432.891853	26.821095
214.558772	7442.897019	26.826112
214.681338	7455.104541	26.831130
214.707714	7455.564523	26.836148
215.123517	7479.561539	26.841165
215.316713	7489.377800	26.846183
215.449898	7507.310287	26.851200
216.246299	7503.183396	26.856218
217.104611	7490.359126	26.861236
217.555549	7506.575309	26.866253
217.803056	7516.260011	26.871271
218.166860	7501.119803	26.876288
218.343847	7490.936584	26.881306
218.755971	7477.158960	26.886324
218.767300	7478.186367	26.891341
219.034140	7475.098463	26.896359
219.636188	7478.401562	26.901376
219.228446	7476.002705	26.906394
219.361589	7472.200063	26.911412
219.215443	7471.493605	26.916429
219.391596	7470.683303	26.921447
219.871195	7479.874104	26.926464
219.810259	7505.176559	26.931482
219.850226	7504.561086	26.936500
219.733561	7516.146106	26.941517
219.773746	7529.645042	26.946535
220.307772	7531.194040	26.951552
220.382221	7547.206852	26.956570
220.575317	7556.805339	26.961588
220.650540	7571.271174	26.966605
220.667276	7586.090228	26.971623
220.728392	7600.738226	26.976640
220.940840	7622.345745	26.981658
221.288624	7636.049423	26.986676
221.273107	7654.819687	26.991693
221.451452	7671.454128	26.996711
221.591148	7697.129695	27.001728
221.696132	7714.981539	27.006746
222.219326	7739.918722	27.011764
222.426746	7766.237326	27.016781
222.852901	7787.540272	27.021799
223.279187	7807.084810	27.026816
223.321871	7819.011415	27.031834
223.709763	7831.250488	27.036852
223.691029	7841.264093	27.041869
224.060170	7866.184391	27.046887
224.707591	7873.994933	27.051904
224.435678	7899.491780	27.056922
225.079705	7908.316247	27.061940
225.624138	7918.826252	27.066957
225.529705	7937.722741	27.071975
225.886548	7944.880865	27.076992
226.214417	7952.851684	27.082010
226.329816	7962.077330	27.087028
226.690271	7974.851140	27.092045
226.532135	7991.907621	27.097063
227.299809	7990.762118	27.102080
227.591607	7994.915484	27.107098
228.051503	7995.409010	27.112116
228.390791	8013.717152	27.117133
228.917878	8016.782620	27.122151
228.808737	8016.303996	27.127168
228.760666	8014.802475	27.132186
228.959830	8019.131275	27.137204
228.771091	8021.424236	27.142221
228.744473	8031.369719	27.147239
229.579444	8044.366457	27.152256
229.405852	8048.892204	27.157274
229.698439	8062.386961	27.162292
229.932063	8066.060069	27.167309
229.846055	8080.728196	27.172327
230.126567	8098.047967	27.177344
230.300582	8104.956802	27.182362
230.415089	8123.246380	27.187380
230.802737	8131.081691	27.192397
231.089377	8159.045943	27.197415
231.788678	8152.591538	27.202432
231.880448	8169.066272	27.207450
232.246900	8172.008397	27.212468
233.113768	8170.247610	27.217485
232.806292	8183.816937	27.222503
233.127446	8196.896936	27.227520
233.153114	8191.289289	27.232538
233.162039	8203.761246	27.237556
233.554424	8213.474272	27.242573
233.450603	8226.317382	27.247591
233.885097	8245.116054	27.252608
234.054922	8255.918194	27.257626
234.054631	8271.627570	27.262644
234.547661	8281.852185	27.267661
234.143341	8304.857219	27.272679
234.733705	8313.863873	27.277696
235.157636	8336.888380	27.282714
235.358987	8355.044700	27.287732
235.643977	8363.211796	27.292749
235.832686	8383.542150	27.297767
236.006333	8381.781931	27.302784
236.246062	8405.573948	27.307802
236.377590	8415.722323	27.312820
236.709970	8433.113259	27.317837
237.058780	8449.103082	27.322855
237.420678	8469.090863	27.327872
237.674805	8473.291245	27.332890
238.215569	8484.364101	27.337908
238.144614	8496.097314	27.342925
238.473505	8507.632530	27.347943
238.782285	8515.091965	27.352960
239.010600	8520.417132	27.357978
239.576265	8534.981006	27.362996
239.646598	8544.690676	27.368013
239.954850	8548.503801	27.373031
240.501722	8559.998799	27.378048
240.725788	8567.619827	27.383066
240.708159	8570.069326	27.388084
240.826918	8577.087968	27.393101
240.987045	8595.743446	27.398119
241.041296	8602.948936	27.403136
241.113504	8613.188739	27.408154
241.199740	8632.180936	27.413172
241.219753	8641.308118	27.418189
241.437744	8664.292483	27.423207
241.923806	8676.292683	27.428224
242.053941	8693.301773	27.433242
242.233387	8712.270070	27.438260
242.810061	8727.946836	27.443277
243.305641	8743.175304	27.448295
243.760957	8765.958679	27.453312
243.876693	8771.749753	27.458330
243.636256	8781.321662	27.463348
244.132568	8792.521595	27.468365
244.389957	8803.913430	27.473383
244.525967	8823.728393	27.478400
244.665149	8829.923103	27.483418
245.152312	8843.804879	27.488436
245.221000	8858.518995	27.493453
245.156606	8872.963388	27.498471
245.518118	8879.843323	27.503488
245.848817	8905.336137	27.508506
245.676482	8919.516386	27.513524
246.298926	8930.134798	27.518541
246.487175	8948.839925	27.523559
246.890837	8966.229737	27.528576
246.762558	8982.606856	27.533594
246.887351	8999.607588	27.538612
247.473323	9010.200152	27.543629
247.842045	9044.830322	27.548647
247.894696	9049.033789	27.553664
248.781136	9066.910507	27.558682
248.966330	9071.399587	27.563700
249.529555	9084.483571	27.568717
249.465962	9095.609843	27.573735
249.627239	9104.705789	27.578752
250.232574	9123.030442	27.583770
250.611042	9132.613519	27.588788
250.973272	9123.312984	27.593805
251.064737	9137.635445	27.598823
251.228857	9144.044222	27.603840
251.819664	9147.775596	27.608858
251.663817	9159.572960	27.613876
252.090892	9165.899763	27.618893
251.937938	9174.264844	27.623911
252.400488	9184.548379	27.628928
252.984820	9183.901772	27.633946
253.278921	9191.663699	27.638964
253.748289	9186.390791	27.643981
253.034165	9201.223895	27.648999
253.825317	9211.333156	27.654016
253.993396	9217.318281	27.659034
254.558627	9244.183149	27.664052
254.668911	9239.490222	27.669069
254.509959	9254.495825	27.674087
254.575452	9275.181005	27.679104
255.259668	9278.951536	27.684122
255.233247	9283.359954	27.689140
255.395104	9299.865828	27.694157
255.486561	9312.281483	27.699175
255.708401	9331.881567	27.704192
256.320478	9348.532081	27.709210
256.476274	9359.826416	27.714228
256.244229	9376.340011	27.719245
256.512156	9399.004951	27.724263
256.984301	9409.381834	27.729280
257.650324	9433.077232	27.734298
257.702234	9452.467109	27.739316
258.167559	9460.009901	27.744333
258.282808	9477.066231	27.749351
258.196791	9496.225049	27.754368
258.627640	9510.015063	27.759386
258.978472	9526.750610	27.764404
258.937399	9527.502139	27.769421
259.743248	9551.501115	27.774439
259.795178	9566.568855	27.779456
260.658664	9571.823854	27.784474
260.553500	9581.119377	27.789492
261.135555	9591.712887	27.794509
261.422043	9598.030153	27.799527
261.502159	9606.810629	27.804544
261.964446	9606.751314	27.809562
262.059404	9627.369154	27.814580
262.129113	9624.431562	27.819597
261.805007	9631.576382	27.824615
262.162910	9646.808088	27.829632
262.712888	9656.288962	27.834650
263.232773	9686.148292	27.839668
263.337766	9689.908054	27.844685
263.696654	9705.316460	27.849703
263.397320	9714.279195	27.854720
264.065565	9726.299074	27.859738
264.054773	9744.606605	27.864756
264.453191	9755.010946	27.869773
264.568315	9774.893324	27.874791
264.929183	9790.841387	27.879808
264.883932	9788.603638	27.884826
264.892573	9829.470120	27.889844
265.422293	9840.529726	27.894861
265.831434	9863.738403	27.899879
265.799205	9879.545676	27.904896
266.330349	9891.400727	27.909914
266.930182	9911.634023	27.914932
267.411272	9931.784795	27.919949
267.105497	9943.770176	27.924967
267.422398	9961.408072	27.929984
267.796537	9971.374293	27.935002
267.543019	9989.498842	27.940020
268.171524	10003.334226	27.945037
268.563939	10030.044015	27.950055
268.758619	10051.344566	27.955072
269.184319	10061.782720	27.960090
269.144239	10092.863361	27.965108
269.284345	10114.156693	27.970125
269.985580	10132.795779	27.975143
270.135478	10143.494774	27.980160
270.513517	10164.719549	27.985178
270.465195	10190.023707	27.990196
271.036592	10189.890574	27.995213
271.365424	10215.142363	28.000231
271.607643	10231.478686	28.005248
272.117920	10246.147255	28.010266
272.175001	10266.332828	28.015284
272.511772	10285.556087	28.020301
273.120422	10294.832399	28.025319
273.291111	10297.129670	28.030336
273.737433	10322.638005	28.035354
273.834443	10335.953327	28.040372
274.121566	10349.602159	28.045389
274.555682	10353.506572	28.050407
274.538025	10378.266302	28.055424
275.060897	10388.092768	28.060442
275.263648	10396.690340	28.065460
275.309420	10416.808374	28.070477
275.735413	10430.972401	28.075495
275.790775	10449.674469	28.080512
276.214432	10471.081935	28.085530
276.416405	10475.243533	28.090548
276.919924	10494.677852	28.095565
277.484734	10494.271051	28.100583
277.639444	10523.399230	28.105600
277.416248	10531.153848	28.110618
277.685729	10553.128483	28.115636
278.336931	10559.951316	28.120653
278.742377	10580.120882	28.125671
278.500109	10588.560492	28.130688
279.052723	10602.281843	28.135706
279.416577	10612.313158	28.140724
279.466828	10625.617023	28.145741
280.061186	10635.694557	28.150759
280.252113	10647.186280	28.155776
280.416898	10647.394303	28.160794
280.878681	10667.056320	28.165812
280.960848	10676.247445	28.170829
281.343239	10687.100003	28.175847
281.420555	10700.854377	28.180864
282.021235	10703.438388	28.185882
282.427215	10714.634605	28.190900
282.382010	10730.062570	28.195917
283.148410	10733.413301	28.200935
283.248858	10746.712594	28.205952
283.777860	10753.958676	28.210970
283.807290	10759.675399	28.215988
284.326224	10782.138761	28.221005
284.565408	10781.890003	28.226023
284.353268	10782.500871	28.231040
284.763703	10797.854797	28.236058
285.198384	10819.728249	28.241076
285.165171	10836.430044	28.246093
285.098127	10845.445563	28.251111
285.325547	10863.161394	28.256128
285.631074	10879.636830	28.261146
285.656118	10906.540841	28.266164
286.148077	10930.950422	28.271181
286.303619	10938.949361	28.276199
286.451384	10966.999459	28.281216
287.182628	10984.826416	28.286234
287.548183	11005.829912	28.291252
287.813053	11034.060801	28.296269
288.260699	11052.923425	28.301287
288.403208	11056.169267	28.306304
288.562593	11078.319536	28.311322
288.784574	11099.430742	28.316340
289.447583	11118.250431	28.321357
289.800885	11134.229242	28.326375
290.050419	11159.958810	28.331392
290.341613	11175.789450	28.336410
290.782141	11200.340005	28.341428
291.002043	11214.268325	28.346445
291.729316	11230.656309	28.351463
291.637310	11247.850723	28.356480
291.745883	11264.388737	28.361498
292.054168	11279.007472	28.366516
292.432236	11300.906090	28.371533
292.706750	11312.003148	28.376551
292.995446	11332.409574	28.381568
293.507379	11350.517312	28.386586
293.563595	11373.091314	28.391604
294.004548	11383.104726	28.396621
294.360157	11389.137137	28.401639
294.680845	11412.566755	28.406656
294.733876	11429.735598	28.411674
295.505273	11431.326925	28.416692
295.230417	11449.459366	28.421709
296.008840	11463.973477	28.426727
295.715433	11476.178941	28.431744
296.313213	11492.145257	28.436762
296.817032	11516.651642	28.441780
296.610606	11528.710980	28.446797
297.064348	11539.704489	28.451815
297.274061	11563.110524	28.456832
297.486753	11580.343061	28.461850
297.752087	11595.259228	28.466868
298.162492	11612.015794	28.471885
299.110315	11621.483101	28.476903
299.118897	11645.782573	28.481920
299.514873	11662.932972	28.486938
299.552916	11667.698198	28.491956
299.898599	11686.110012	28.496973
300.600620	11688.207906	28.501991
300.338300	11702.230608	28.507008
300.891601	11719.201844	28.512026
301.034013	11727.585235	28.517044
301.145993	11752.733930	28.522061
301.619135	11757.058843	28.527079
301.687156	11778.933664	28.532096
302.118772	11797.171171	28.537114
302.736497	11805.398500	28.542132
302.674143	11818.509183	28.547149
303.037621	11822.535422	28.552167
303.270758	11843.418382	28.557184
303.569480	11868.639204	28.562202
304.052144	11883.903839	28.567220
304.178068	11910.496768	28.572237
304.621936	11923.936049	28.577255
304.614046	11947.998496	28.582272
304.523551	11962.588278	28.587290
305.073125	11976.977378	28.592308
305.133725	12021.402382	28.597325
305.376919	12035.450834	28.602343
305.848186	12053.395071	28.607360
306.186685	12080.634043	28.612378
306.859192	12098.562782	28.617396
307.108733	12123.254800	28.622413
307.560968	12130.892291	28.627431
307.575763	12168.883130	28.632448
308.214134	12186.804638	28.637466
308.533896	12199.931881	28.642484
308.732573	12225.099288	28.647501
309.279324	12241.519423	28.652519
309.427809	12261.102428	28.657536
309.689183	12283.115092	28.662554
310.369293	12294.212742	28.667572
310.591877	12317.810334	28.672589
311.430863	12339.774189	28.677607
311.533869	12338.570884	28.682624
312.120701	12361.761319	28.687642
312.707013	12355.812520	28.692660
312.760309	12377.816639	28.697677
313.177131	12395.078141	28.702695
313.168043	12405.481096	28.707712
313.145389	12414.970430	28.712730
313.772936	12423.108087	28.717748
313.509160	12439.578796	28.722765
313.825230	12458.182284	28.727783
314.262958	12478.809900	28.732800
314.687473	12502.101564	28.737818
314.774606	12516.591493	28.742836
315.086729	12545.875142	28.747853
315.254102	12564.729242	28.752871
315.711221	12586.187601	28.757888
316.047808	12611.719300	28.762906
316.439690	12623.000959	28.767924
316.414852	12649.488937	28.772941
316.854938	12670.122711	28.777959
317.001523	12687.739172	28.782976
317.068283	12707.651141	28.787994
317.821860	12739.070483	28.793012
318.335481	12765.285328	28.798029
318.762008	12778.791076	28.803047
318.686181	12799.571626	28.808064
319.195439	12834.730084	28.813082
319.513147	12843.440354	28.818100
319.780662	12873.110390	28.823117
319.938811	12889.654747	28.828135
320.490943	12914.218592	28.833152
320.412046	12934.071373	28.838170
321.549366	12943.067761	28.843188
322.308580	12951.901972	28.848205
322.289105	12953.319730	28.853223
322.766805	12970.259660	28.858240
322.666877	12975.867727	28.863258
323.107176	12986.898916	28.868276
323.204695	13005.672756	28.873293
322.964982	13026.659065	28.878311
323.562448	13049.207654	28.883328
324.021994	13063.283191	28.888346
324.121738	13086.600877	28.893364
324.285169	13105.434027	28.898381
324.728645	13132.383446	28.903399
325.087604	13164.373346	28.908416
325.240435	13187.281845	28.913434
325.801994	13207.581512	28.918452
325.773580	13237.367665	28.923469
326.839881	13249.087856	28.928487
327.261527	13260.191582	28.933504
327.386959	13282.236051	28.938522
328.362618	13297.557715	28.943540
328.437338	13303.915524	28.948557
328.613970	13322.901571	28.953575
328.995979	13335.356765	28.958592
329.290962	13352.723376	28.963610
329.850725	13364.007765	28.968628
329.704337	13390.376757	28.973645
330.436279	13405.648032	28.978663
330.291839	13426.619951	28.983680
330.342366	13452.462585	28.988698
330.858614	13462.358020	28.993716
331.453283	13492.691781	28.998733
331.570134	13511.564167	29.003751
332.071618	13534.510387	29.008768
332.246655	13558.192722	29.013786
332.486504	13569.795462	29.018804
332.965174	13592.770567	29.023821
333.368896	13600.782530	29.028839
333.898488	13623.402374	29.033856
334.435935	13648.086304	29.038874
334.883385	13654.291465	29.043892
335.294406	13680.473029	29.048909
335.625193	13690.056401	29.053927
335.828270	13696.849101	29.058944
336.262092	13719.825027	29.063962
336.558509	13738.202309	29.068980
336.644944	13755.393334	29.073997
336.940537	13767.284364	29.079015
337.295800	13779.949281	29.084032
337.235720	13799.841094	29.089050
337.895170	13817.985090	29.094068
338.069290	13840.730011	29.099085
338.655135	13861.996094	29.104103
338.762013	13879.626164	29.109120
338.932553	13899.469546	29.114138
339.432738	13919.271102	29.119156
339.555304	13942.782083	29.124173
339.693488	13968.030707	29.129191
340.571226	13988.762004	29.134208
340.439221	14027.458399	29.139226
340.670531	14044.598710	29.144244
341.163026	14065.658496	29.149261
341.320712	14092.587459	29.154279
341.980164	14118.680424	29.159296
342.429827	14141.692292	29.164314
342.822481	14166.314174	29.169332
342.929857	14184.023398	29.174349
343.463799	14204.208433	29.179367
344.082538	14211.962962	29.184384
344.704715	14228.047813	29.189402
345.175197	14237.271806	29.194420
345.411861	14247.782783	29.199437
345.419321	14257.419937	29.204455
345.652986	14270.290437	29.209472
346.028667	14286.047381	29.214490
346.469539	14302.893184	29.219508
346.560524	14327.053796	29.224525
346.573405	14353.898301	29.229543
347.048269	14359.505716	29.234560
347.523424	14396.222987	29.239578
347.327699	14413.537486	29.244596
347.957942	14448.414834	29.249613
348.324643	14475.289694	29.254631
348.621323	14506.454670	29.259648
348.570211	14532.172485	29.264666
349.513869	14554.972151	29.269684
349.525898	14592.728272	29.274701
349.851334	14624.627956	29.279719
350.777732	14649.843201	29.284736
350.733399	14664.784742	29.289754
351.034306	14689.645810	29.294772
351.360584	14713.227089	29.299789
351.720086	14748.090291	29.304807
352.416894	14769.564344	29.309824
352.501085	14795.542521	29.314842
352.864397	14821.290951	29.319860
353.628742	14843.026171	29.324877
353.655290	14867.807018	29.329895
354.000722	14890.990770	29.334912
354.642963	14915.407386	29.339930
355.458088	14931.314363	29.344948
355.692954	14951.442535	29.349965
355.971438	14971.273389	29.354983
356.904421	14987.234703	29.360000
357.611477	15009.875947	29.365018
357.719372	15013.077332	29.370036
358.289094	15030.307964	29.375053
358.330882	15041.525563	29.380071
358.689427	15052.207500	29.385088
358.748585	15068.942869	29.390106
358.945513	15081.658572	29.395124
359.168564	15094.376533	29.400141
359.321377	15124.232174	29.405159
359.998447	15143.909568	29.410176
360.115370	15175.738418	29.415194
360.384378	15181.558143	29.420212
360.689843	15205.042210	29.425229
361.056579	15236.396440	29.430247
361.527514	15258.499950	29.435264
361.699237	15287.155948	29.440282
361.669482	15317.261387	29.445300
362.534801	15346.548513	29.450317
362.929752	15368.802941	29.455335
363.236152	15385.073737	29.460352
363.710980	15427.882080	29.465370
363.876188	15437.880575	29.470388
364.564217	15463.083480	29.475405
364.620354	15497.641560	29.480423
365.002092	15514.639764	29.485440
365.284189	15546.544580	29.490458
365.684043	15579.350165	29.495476
366.096387	15599.167149	29.500493
366.349730	15629.266905	29.505511
366.887897	15641.137135	29.510528
367.515393	15668.149939	29.515546
367.627538	15688.130606	29.520564
367.909127	15707.570118	29.525581
367.941783	15733.415472	29.530599
368.279389	15750.035448	29.535616
368.555148	15789.916293	29.540634
368.729162	15808.223042	29.545652
369.565762	15824.986478	29.550669
369.658872	15868.906943	29.555687
370.067049	15889.795538	29.560704
370.721538	15913.595660	29.565722
370.860444	15943.660035	29.570740
371.381657	15967.619938	29.575757
371.924704	15999.311177	29.580775
372.761632	16014.805088	29.585792
373.477587	16033.261397	29.590810
373.988438	16053.546740	29.595828
374.455289	16061.183551	29.600845
374.170982	16090.713962	29.605863
374.975119	16095.999017	29.610880
375.409874	16114.508657	29.615898
375.568286	16121.631328	29.620916
376.166869	16133.716702	29.625933
376.263762	16164.081689	29.630951
376.751098	16177.444587	29.635968
377.304415	16190.768797	29.640986
377.567630	16219.787791	29.646004
377.800718	16235.821216	29.651021
378.293722	16254.988337	29.656039
378.601979	16271.022722	29.661056
378.578592	16291.173561	29.666074
378.994308	16313.729060	29.671092
379.807115	16329.770222	29.676109
379.648261	16354.231280	29.681127
379.982056	16381.085521	29.686144
380.129902	16409.131032	29.691162
380.532969	16448.424920	29.696180
380.934412	16478.117631	29.701197
381.402635	16497.178308	29.706215
381.706309	16530.313177	29.711232
382.053025	16558.744856	29.716250
382.470348	16592.234831	29.721268
382.993747	16617.884957	29.726285
383.362112	16651.208944	29.731303
383.819651	16668.521691	29.736320
384.448758	16696.710630	29.741338
385.010588	16706.758587	29.746356
386.102300	16721.013205	29.751373
386.485329	16733.802104	29.756391
386.938893	16745.373509	29.761408
387.420221	16747.250516	29.766426
387.992968	16762.252388	29.771444
388.488316	16759.010546	29.776461
389.076034	16778.773024	29.781479
389.186604	16789.080783	29.786496
389.623022	16786.555602	29.791514
389.470914	16789.371373	29.796532
389.945143	16808.241919	29.801549
389.799612	16817.392512	29.806567
390.413370	16846.335772	29.811584
390.662319	16861.732403	29.816602
390.762540	16887.815152	29.821620
391.074439	16902.390292	29.826637
391.531844	16939.067837	29.831655
391.875343	16957.052401	29.836672
392.142313	16973.678119	29.841690
392.192494	17012.244797	29.846708
392.662425	17034.157849	29.851725
393.113035	17060.663215	29.856743
393.087716	17082.107004	29.861760
393.699223	17105.293078	29.866778
393.614053	17133.356971	29.871796
394.522999	17151.929607	29.876813
395.206177	17185.774041	29.881831
395.765219	17217.524816	29.886848
396.118180	17229.664915	29.891866
395.955597	17264.557126	29.896884
396.499904	17279.522770	29.901901
396.707795	17307.016977	29.906919
396.932936	17338.564092	29.911936
397.857759	17367.822942	29.916954
397.592463	17400.814157	29.921972
398.389417	17423.235803	29.926989
398.986139	17461.247670	29.932007
399.224425	17498.209918	29.937024
400.018604	17516.557566	29.942042
399.751818	17555.522117	29.947060
400.315204	17570.045976	29.952077
400.915140	17600.786591	29.957095
401.181593	17636.891904	29.962112
401.647925	17668.619952	29.967130
401.928607	17693.832355	29.972148
402.400596	17726.671442	29.977165
403.104921	17763.043633	29.982183
403.617189	17789.224542	29.987200
403.856706	17817.096743	29.992218
403.983953	17836.906728	29.997236
404.814645	17863.872040	30.002253
405.270414	17897.465693	30.007271
405.322106	17932.594233	30.012288
406.072344	17964.979786	30.017306
406.396164	17996.244129	30.022324
407.045164	18021.854464	30.027341
407.281848	18055.615162	30.032359
407.474113	18081.404075	30.037376
408.025001	18101.906454	30.042394
408.516510	18129.152365	30.047412
409.300471	18147.451667	30.052429
410.134281	18166.728730	30.057447
410.745587	18191.498636	30.062464
411.226957	18195.340477	30.067482
411.623391	18210.554133	30.072500
412.039276	18222.208102	30.077517
412.227328	18247.650438	30.082535
412.463201	18273.622338	30.087552
413.042115	18287.796867	30.092570
413.109055	18311.710385	30.097588
413.218639	18340.298480	30.102605
413.860509	18354.299004	30.107623
414.113633	18383.686079	30.112640
414.361651	18411.077689	30.117658
414.201522	18436.321781	30.122676
415.308511	18465.980365	30.127693
416.359475	18479.399263	30.132711
416.381777	18506.485007	30.137728
417.156694	18518.304371	30.142746
417.392195	18540.321965	30.147764
417.308378	18560.948913	30.152781
417.707939	18586.213464	30.157799
417.858782	18625.036179	30.162816
418.680071	18634.946834	30.167834
419.054301	18675.105767	30.172852
419.372075	18702.657502	30.177869
419.546736	18726.194663	30.182887
419.973837	18756.363859	30.187904
420.637258	18777.430649	30.192922
421.042866	18806.895707	30.197940
421.323811	18831.856849	30.202957
421.827097	18855.109256	30.207975
421.870432	18885.970154	30.212992
422.374786	18906.019449	30.218010
422.551544	18938.647534	30.223028
423.041189	18972.054568	30.228045
423.806175	18997.149048	30.233063
424.181943	19027.187670	30.238080
424.401814	19055.848095	30.243098
424.944223	19090.839160	30.248116
425.352546	19113.392768	30.253133
425.961771	19148.209276	30.258151
426.469306	19174.986657	30.263168
426.518956	19200.931930	30.268186
427.000592	19223.600606	30.273204
427.218998	19259.912270	30.278221
427.815594	19296.221985	30.283239
428.589987	19328.675553	30.288256
429.127008	19341.480116	30.293274
429.503307	19376.901890	30.298292
429.835287	19412.924496	30.303309
430.433324	19438.443555	30.308327
430.831887	19471.328618	30.313344
431.645478	19486.036090	30.318362
431.843641	19506.721225	30.323380
432.250356	19529.307155	30.328397
433.068210	19555.209120	30.333415
432.993054	19579.493796	30.338432
433.591472	19617.339050	30.343450
433.760548	19647.145459	30.348468
434.336129	19673.900297	30.353485
434.661626	19705.982132	30.358503
435.217727	19735.071368	30.363520
435.825178	19759.148915	30.368538
435.832043	19794.837451	30.373556
436.198171	19829.421355	30.378573
436.599698	19858.547475	30.383591
436.972946	19897.533957	30.388608
437.493791	19927.740919	30.393626
437.732434	19963.450541	30.398644
438.018332	20003.619648	30.403661
438.356598	20036.312877	30.408679
439.085889	20069.299091	30.413696
439.492279	20101.779650	30.418714
439.904880	20145.833825	30.423732
440.650810	20169.549149	30.428749
441.637659	20190.870386	30.433767
442.106432	20215.134353	30.438784
442.864533	20247.301361	30.443802
442.926558	20274.857228	30.448820
443.249679	20311.293541	30.453837
443.995821	20328.185555	30.458855
444.320499	20358.297362	30.463872
444.759326	20382.484064	30.468890
445.183304	20414.090512	30.473908
445.498929	20449.245683	30.478925
445.771797	20469.225219	30.483943
446.280742	20499.074787	30.488960
446.804118	20522.345013	30.493978
447.330465	20555.957546	30.498996
447.613213	20585.747688	30.504013
448.106642	20616.004209	30.509031
447.975834	20646.181050	30.514048
448.670782	20671.661364	30.519066
449.275114	20713.633572	30.524084
449.358878	20753.203869	30.529101
450.173196	20783.113739	30.534119
450.403635	20814.055962	30.539136
450.420869	20847.647162	30.544154
451.374662	20874.982905	30.549172
451.541468	20909.151155	30.554189
452.353963	20942.296482	30.559207
452.670222	20976.422628	30.564224
453.325767	20997.834234	30.569242
453.369092	21026.164893	30.574260
453.828982	21063.112046	30.579277
454.569003	21088.686979	30.584295
455.158642	21119.377897	30.589312
455.450038	21145.180702	30.594330
456.098590	21181.883886	30.599348
456.230470	21210.497985	30.604365
457.011980	21236.881716	30.609383
456.987884	21280.722101	30.614400
457.361780	21312.925401	30.619418
458.296528	21341.357836	30.624436
458.384375	21382.198754	30.629453
458.974245	21401.952975	30.634471
459.685568	21442.115665	30.639488
459.925692	21479.634877	30.644506
460.732310	21514.968256	30.649524
460.893769	21552.563038	30.654541
461.613047	21565.903030	30.659559
462.796003	21584.737390	30.664576
462.976471	21600.815032	30.669594
463.999579	21628.697061	30.674612
464.474231	21659.741603	30.679629
465.036574	21672.670125	30.684647
465.206972	21699.250710	30.689664
465.738363	21720.739301	30.694682
466.132326	21743.481416	30.699700
466.284869	21769.350886	30.704717
466.663286	21795.551699	30.709735
466.954126	21837.499290	30.714752
467.209089	21858.645636	30.719770
467.874719	21886.128748	30.724788
468.400287	21921.847813	30.729805
469.164667	21948.525820	30.734823
469.475406	21991.822813	30.739840
469.448296	22021.764467	30.744858
470.063301	22044.883225	30.749876
470.395414	22072.860820	30.754893
470.839293	22102.065821	30.759911
471.228935	22143.543741	30.764928
472.008839	22177.764074	30.769946
472.115777	22220.290829	30.774964
472.831977	22258.514602	30.779981
473.456278	22289.416785	30.784999
473.853063	22319.191799	30.790016
474.233431	22353.733702	30.795034
474.669728	22382.479033	30.800052
475.012671	22418.593912	30.805069
475.796515	22452.681416	30.810087
476.262300	22486.951187	30.815104
476.838163	22513.621395	30.820122
477.706075	22541.787948	30.825140
478.282297	22570.960402	30.830157
478.799827	22593.033428	30.835175
479.121210	22622.574206	30.840192
479.766295	22633.165172	30.845210
480.616725	22662.680519	30.850228
480.638925	22688.065980	30.855245
481.482353	22708.881512	30.860263
481.653816	22742.578303	30.865280
482.058363	22761.149529	30.870298
483.028277	22768.777027	30.875316
483.192255	22789.376158	30.880333
483.816049	22811.079031	30.885351
483.995412	22829.192509	30.890368
484.300948	22851.020797	30.895386
484.998392	22870.279514	30.900404
484.913568	22908.938871	30.905421
485.327661	22939.072300	30.910439
485.847955	22970.225538	30.915456
486.145318	22995.119915	30.920474
486.591980	23018.619880	30.925492
487.007184	23060.468559	30.930509
487.362032	23093.391766	30.935527
488.046699	23139.084798	30.940544
487.944668	23179.371326	30.945562
488.768011	23210.850582	30.950580
488.756002	23256.658661	30.955597
489.408664	23301.017426	30.960615
489.976715	23345.319953	30.965632
490.461983	23382.482343	30.970650
491.234990	23422.942772	30.975668
492.069020	23459.008372	30.980685
492.379778	23494.845865	30.985703
492.937224	23529.735075	30.990720
493.423639	23567.618006	30.995738
493.727167	23593.706478	31.000756
494.362959	23639.054401	31.005773
494.848065	23678.062544	31.010791
495.402819	23714.064659	31.015808
496.024408	23758.473517	31.020826
496.600345	23800.330327	31.025844
496.822532	23837.825204	31.030861
497.295789	23861.758049	31.035879
498.031010	23903.918877	31.040896
498.513265	23942.864791	31.045914
499.484224	23974.499216	31.050932
499.696382	24012.128686	31.055949
500.507186	24046.935126	31.060967
501.334373	24075.552548	31.065984
501.415226	24104.286198	31.071002
502.062108	24131.364598	31.076020
502.316437	24181.948609	31.081037
502.587387	24206.791741	31.086055
503.118819	24240.839465	31.091072
503.658476	24283.941519	31.096090
504.007402	24319.344841	31.101108
504.533760	24353.475698	31.106125
505.219867	24396.416170	31.111143
505.727771	24431.889733	31.116160
505.974879	24474.424765	31.121178
506.659085	24510.465041	31.126196
507.000209	24563.197729	31.131213
507.595128	24588.591244	31.136231
508.551976	24632.684442	31.141248
508.964506	24668.836811	31.146266
509.300767	24698.517383	31.151284
509.550625	24744.136442	31.156301
509.824392	24775.153939	31.161319
510.605560	24815.957179	31.166336
510.710418	24868.910718	31.171354
511.793693	24908.990932	31.176372
512.431915	24938.675408	31.181389
513.053657	24983.105926	31.186407
513.570588	25015.571029	31.191424
514.285845	25055.999528	31.196442
514.580030	25086.698352	31.201460
515.230034	25128.413705	31.206477
515.383211	25155.456601	31.211495
516.003575	25187.021139	31.216512
516.700633	25219.932500	31.221530
517.389316	25252.883136	31.226548
517.731331	25280.086390	31.231565
518.311932	25308.680773	31.236583
519.025578	25331.364591	31.241600
519.623612	25365.606090	31.246618
520.154726	25387.528432	31.251636
520.199378	25422.033126	31.256653
520.291760	25453.016713	31.261671
520.884415	25486.880077	31.266688
521.508520	25534.572403	31.271706
521.900243	25559.676479	31.276724
522.474862	25594.686698	31.281741
522.942124	25644.672479	31.286759
523.667833	25680.771599	31.291776
523.607736	25719.242946	31.296794
524.368123	25753.074327	31.301812
524.580922	25802.556614	31.306829
525.088466	25839.284041	31.311847
525.941554	25888.117039	31.316864
526.004222	25940.599665	31.321882
526.762005	25991.874563	31.326900
527.410367	26033.743729	31.331917
527.612207	26085.648919	31.336935
528.310265	26119.648617	31.341952
528.991628	26176.541612	31.346970
529.164841	26219.047603	31.351988
530.045374	26269.608909	31.357005
530.657102	26313.399296	31.362023
531.257428	26365.849887	31.367040
531.849105	26405.598826	31.372058
532.423985	26441.008635	31.377076
533.010260	26487.280792	31.382093
533.406809	26533.216032	31.387111
534.385062	26577.847375	31.392128
534.950397	26623.788144	31.397146
535.388791	26656.129082	31.402164
535.731766	26693.913852	31.407181
536.432599	26730.353690	31.412199
537.082071	26763.641551	31.417216
537.560509	26820.498431	31.422234
538.387679	26849.480066	31.427252
539.422805	26878.795936	31.432269
539.515844	26914.919919	31.437287
540.218175	26956.965883	31.442304
540.708142	26995.069621	31.447322
541.281468	27021.638803	31.452340
541.659961	27058.925754	31.457357
542.005206	27102.696136	31.462375
542.629817	27130.230785	31.467392
542.748922	27176.811095	31.472410
543.739813	27216.840775	31.477428
544.292527	27260.004058	31.482445
544.552177	27301.784682	31.487463
545.241926	27342.670482	31.492480
545.421590	27394.171664	31.497498
546.028914	27429.938410	31.502516
546.315270	27477.043237	31.507533
547.123443	27525.659659	31.512551
547.812398	27568.581179	31.517568
548.318555	27611.000339	31.522586
549.989253	27638.865817	31.527604
550.674659	27654.825480	31.532621
550.925663	27690.338458	31.537639
551.958356	27713.727418	31.542656
551.888675	27741.345701	31.547674
552.581889	27770.855142	31.552692
553.168987	27801.461934	31.557709
553.384117	27841.209109	31.562727
554.024500	27855.709603	31.567744
554.445265	27894.034378	31.572762
554.613528	27923.556237	31.577780
555.255056	27962.997094	31.582797
555.445449	27999.493397	31.587815
556.137743	28028.295464	31.592832
556.591883	28075.546212	31.597850
557.082929	28112.223450	31.602868
558.010522	28149.528052	31.607885
557.954839	28194.804277	31.612903
558.941102	28237.819980	31.617920
559.153357	28283.332795	31.622938
559.565158	28328.245795	31.627956
560.162751	28366.847319	31.632973
560.860171	28419.300748	31.637991
560.958757	28465.362594	31.643008
561.871646	28515.823341	31.648026
562.148010	28565.814446	31.653044
562.842096	28603.086703	31.658061
563.390388	28666.998041	31.663079
563.884435	28712.499547	31.668096
564.484178	28767.193957	31.673114
565.187572	28808.162749	31.678132
566.212844	28840.548539	31.683149
566.560585	28887.994712	31.688167
568.256589	28914.663392	31.693184
569.262870	28941.546931	31.698202
569.766446	28970.594616	31.703220
570.594499	28987.588689	31.708237
571.272594	29020.035133	31.713255
571.830834	29042.665144	31.718272
571.992727	29073.169380	31.723290
572.664752	29102.115180	31.728308
573.346679	29116.192935	31.733325
573.760898	29161.480321	31.738343
574.329633	29188.217393	31.743360
574.997637	29222.220653	31.748378
575.232178	29249.780973	31.753396
575.717440	29278.402130	31.758413
575.958028	29312.952463	31.763431
576.425940	29345.191950	31.768448
576.707810	29391.075646	31.773466
577.222942	29435.854898	31.778484
578.092441	29483.214906	31.783501
578.180910	29523.162057	31.788519
578.823029	29570.804181	31.793536
579.626418	29623.914227	31.798554
579.725760	29665.914276	31.803572
580.592294	29713.009795	31.808589
580.615229	29772.550071	31.813607
580.864397	29828.755725	31.818624
581.817124	29867.696701	31.823642
582.872778	29921.179112	31.828660
584.124311	29954.662916	31.833677
584.398433	30004.493533	31.838695
585.499029	30032.008578	31.843712
586.029138	30077.968943	31.848730
586.227364	30119.019000	31.853748
587.005876	30151.198760	31.858765
587.498193	30200.502836	31.863783
588.076758	30238.750549	31.868800
588.712887	30276.357255	31.873818
589.043344	30319.441506	31.878836
589.791918	30355.349419	31.883853
590.256685	30396.093045	31.888871
591.188660	30440.613639	31.893888
591.615861	30486.388657	31.898906
591.595782	30518.333001	31.903924
592.513925	30547.008641	31.908941
592.888635	30594.005750	31.913959
593.182882	30644.131880	31.918976
593.810871	30671.898351	31.923994
594.593616	30731.051298	31.929012
595.299657	30764.381134	31.934029
595.480882	30812.224308	31.939047
595.731254	30859.848225	31.944064
596.303216	30915.854880	31.949082
596.884009	30967.498563	31.954100
597.956160	31013.028956	31.959117
598.073836	31072.627770	31.964135
598.564297	31124.203728	31.969152
599.400026	31170.909131	31.974170
599.427785	31240.320654	31.979188
600.412873	31294.702622	31.984205
601.287103	31345.682064	31.989223
601.962790	31400.321085	31.994240
602.753686	31453.317683	31.999258
603.148639	31510.042548	32.004276
604.314627	31554.080285	32.009293
604.605039	31606.984507	32.014311
605.570080	31657.988511	32.019328
605.924330	31701.147795	32.024346
606.500108	31754.305083	32.029364
607.440210	31804.175439	32.034381
608.070162	31849.555257	32.039399
608.623554	31894.751120	32.044416
609.383983	31941.842961	32.049434
609.751002	31994.641419	32.054452
610.607295	32033.127373	32.059469
611.046143	32093.222785	32.064487
611.755909	32145.386672	32.069504
612.180922	32196.065154	32.074522
612.690414	32239.030702	32.079540
613.513769	32280.164737	32.084557
614.360778	32337.036428	32.089575
615.342188	32374.915611	32.094592
616.189638	32408.194471	32.099610
616.617439	32461.680052	32.104628
617.522977	32497.156331	32.109645
618.055801	32542.375770	32.114663
618.425792	32577.474060	32.119680
618.934269	32618.430196	32.124698
619.099005	32672.071062	32.129716
620.048694	32711.473051	32.134733
620.213796	32768.458396	32.139751
620.807271	32816.115571	32.144768
621.737093	32867.608495	32.149786
622.304474	32928.653567	32.154804
622.940606	32970.779053	32.159821
623.838599	33013.900666	32.164839
624.634335	33055.476752	32.169856
625.751266	33095.182177	32.174874
626.131682	33138.624858	32.179892
626.529129	33176.741815	32.184909
627.244580	33228.376476	32.189927
627.754558	33270.452663	32.194944
628.646311	33313.449426	32.199962
629.013914	33364.089106	32.204980
629.557864	33402.777946	32.209997
629.957609	33452.394976	32.215015
630.747589	33491.595705	32.220032
631.513579	33543.830203	32.225050
631.859597	33594.334713	32.230068
632.572962	33640.103741	32.235085
633.180911	33682.481613	32.240103
633.571371	33737.177489	32.245120
634.331247	33773.570047	32.250138
634.619338	33823.281203	32.255156
634.849372	33858.940822	32.260173
635.545218	33908.462259	32.265191
635.729370	33966.408881	32.270208
636.724072	34024.033491	32.275226
637.131274	34083.646413	32.280244
637.979223	34123.844551	32.285261
638.331038	34175.860593	32.290279
638.971227	34244.295310	32.295296
639.796054	34297.730099	32.300314
640.390977	34365.135385	32.305332
640.952812	34411.226836	32.310349
641.621196	34477.546235	32.315367
642.386286	34536.175327	32.320384
643.208377	34584.173959	32.325402
644.172873	34644.175899	32.330420
645.420049	34676.681705	32.335437
646.808331	34704.929518	32.340455
647.310793	34751.637918	32.345472
648.125071	34789.357821	32.350490
648.466876	34824.546454	32.355508
649.610498	34877.850896	32.360525
650.022379	34906.718848	32.365543
650.256523	34944.491403	32.370560
651.194542	34979.454708	32.375578
651.837020	35021.741390	32.380596
652.294224	35061.199177	32.385613
653.689847	35097.811194	32.390631
653.877533	35135.003318	32.395648
654.547578	35158.419251	32.400666
654.702639	35208.318773	32.405684
655.446808	35243.913347	32.410701
656.467187	35293.931272	32.415719
657.039556	35338.998838	32.420736
657.232509	35384.536541	32.425754
657.911717	35431.041894	32.430772
658.268116	35482.763278	32.435789
658.909688	35537.418412	32.440807
659.698570	35588.927307	32.445824
660.146157	35641.652850	32.450842
661.514239	35677.271161	32.455860
662.589892	35719.972340	32.460877
663.257379	35766.366445	32.465895
663.636967	35814.626446	32.470912
664.609990	35851.564796	32.475930
664.835280	35894.430318	32.480948
665.284931	35951.417918	32.485965
665.862164	36002.252604	32.490983
666.459864	36048.190295	32.496000
666.933254	36098.244690	32.501018
667.689704	36163.208887	32.506036
668.004215	36217.885074	32.511053
668.850297	36265.099744	32.516071
669.358485	36324.500930	32.521088
669.978975	36374.640567	32.526106
670.656976	36433.092463	32.531124
671.060635	36496.512873	32.536141
671.904297	36545.593839	32.541159
672.716209	36606.061388	32.546176
673.891800	36655.995137	32.551194
673.993172	36719.577084	32.556212
674.320608	36777.382633	32.561229
675.325027	36829.929594	32.566247
675.659801	36888.505724	32.571264
676.470444	36956.050075	32.576282
677.042776	37016.758426	32.581300
677.800597	37074.346024	32.586317
678.218408	37115.072081	32.591335
678.838618	37185.138151	32.596352
679.855001	37231.822595	32.601370
680.527357	37289.411431	32.606388
681.019434	37343.348331	32.611405
681.786462	37399.929971	32.616423
682.412211	37464.305119	32.621440
682.743395	37514.429239	32.626458
683.782436	37576.331194	32.631476
684.283379	37653.094831	32.636493
685.001809	37705.011865	32.641511
685.634271	37764.347123	32.646528
686.619944	37828.768512	32.651546
687.279265	37882.661766	32.656564
687.877021	37952.006644	32.661581
688.625979	37994.592513	32.666599
689.497528	38065.709977	32.671616
690.383825	38124.070838	32.676634
691.085875	38185.628632	32.681652
691.982297	38243.488682	32.686669
692.764529	38302.359465	32.691687
692.896175	38363.551266	32.696704
693.743392	38417.732793	32.701722
694.244774	38479.088692	32.706740
694.711196	38540.007553	32.711757
695.481427	38596.730971	32.716775
696.152991	38670.392061	32.721792
697.101749	38738.394805	32.726810
697.750752	38809.138331	32.731828
698.283463	38875.644315	32.736845
699.502160	38928.713236	32.741863
700.628055	38975.194718	32.746880
701.935313	39034.801540	32.751898
702.907858	39082.533941	32.756916
703.157669	39140.168222	32.761933
704.063119	39183.737572	32.766951
704.590070	39231.767326	32.771968
705.469513	39273.519639	32.776986
705.991012	39333.104156	32.782004
706.364754	39384.655202	32.787021
707.281564	39434.711602	32.792039
708.151420	39494.160124	32.797056
709.015328	39538.267866	32.802074
709.315875	39587.124146	32.807092
710.079950	39656.284195	32.812109
710.754096	39704.077070	32.817127
711.303845	39761.470271	32.822144
712.128828	39818.884019	32.827162
712.389656	39883.044948	32.832180
712.853319	39937.131897	32.837197
713.278172	39997.188618	32.842215
714.105793	40070.368528	32.847232
714.948612	40132.681500	32.852250
715.880654	40189.902490	32.857268
716.617409	40258.404679	32.862285
717.430738	40316.219979	32.867303
717.803409	40388.624345	32.872320
718.637449	40450.509551	32.877338
720.026835	40499.723295	32.882356
720.976222	40563.924504	32.887373
721.432083	40613.707550	32.892391
722.247849	40663.257604	32.897408
722.923863	40724.567386	32.902426
723.694994	40779.727966	32.907444
724.292083	40830.697464	32.912461
725.288884	40880.782696	32.917479
726.037805	40924.601266	32.922496
727.103346	40977.540945	32.927514
727.461943	41015.058160	32.932532
727.995183	41065.449981	32.937549
728.694174	41098.012958	32.942567
729.417227	41145.105707	32.947584
730.098640	41207.257151	32.952602
730.664927	41254.646490	32.957620
731.083440	41320.817251	32.962637
731.949470	41366.901607	32.967655
732.483844	41432.643579	32.972672
732.841517	41487.478194	32.977690
733.595120	41541.302634	32.982708
734.481702	41614.535474	32.987725
735.251904	41678.944946	32.992743
735.582676	41750.259878	32.997760
736.433751	41804.411319	33.002778
736.706849	41878.651283	33.007796
737.477928	41942.612346	33.012813
738.350014	42011.832630	33.017831
739.114107	42093.213315	33.022848
739.639002	42165.941404	33.027866
740.300303	42234.923242	33.032884
741.167915	42317.838200	33.037901
742.246602	42381.562915	33.042919
743.251013	42459.536451	33.047936
744.175039	42528.351817	33.052954
745.002881	42595.575867	33.057972
745.334853	42664.958185	33.062989
746.570648	42736.369452	33.068007
747.468265	42802.678818	33.073024
748.502124	42868.587681	33.078042
749.308163	42930.534860	33.083060
749.779636	42993.008664	33.088077
750.998393	43036.758320	33.093095
751.275861	43113.892269	33.098112
752.025322	43170.573907	33.103130
753.442253	43224.413063	33.108148
754.091158	43290.819539	33.113165
755.387563	43326.101137	33.118183
756.458904	43376.787674	33.123200
757.420931	43417.371256	33.128218
758.627341	43466.171082	33.133236
758.866244	43501.579629	33.138253
759.507735	43539.936306	33.143271
760.035132	43593.187449	33.148288
760.690571	43641.421945	33.153306
761.698415	43687.406868	33.158324
761.808493	43753.443202	33.163341
762.346257	43807.003178	33.168359
762.850316	43870.467440	33.173376
763.630312	43926.684526	33.178394
764.442487	43994.516169	33.183412
764.982574	44060.612983	33.188429
765.810590	44127.677213	33.193447
766.853023	44202.393479	33.198464
766.982535	44253.171709	33.203482
767.613347	44318.951554	33.208500
768.285288	44406.768976	33.213517
768.959212	44470.025074	33.218535
769.691619	44554.519180	33.223552
770.466418	44639.645874	33.228570
771.514464	44698.467205	33.233588
772.268699	44769.371735	33.238605
773.316179	44838.788638	33.243623
774.435945	44909.143325	33.248640
774.869566	44978.352597	33.253658
775.995959	45038.478334	33.258676
776.603548	45111.279132	33.263693
777.471113	45161.583985	33.268711
778.662407	45209.542378	33.273728
779.548278	45256.732419	33.278746
780.227772	45296.054026	33.283764
780.735408	45358.902067	33.288781
781.625511	45412.670410	33.293799
782.813415	45455.872995	33.298816
783.240881	45522.409168	33.303834
783.750252	45571.075428	33.308852
784.498700	45632.191472	33.313869
785.194977	45689.918904	33.318887
785.956355	45749.224105	33.323904
786.494719	45817.179828	33.328922
787.100192	45883.550197	33.333940
787.912316	45945.681956	33.338957
788.974276	46006.490861	33.343975
789.534000	46075.525752	33.348992
790.079303	46159.669178	33.354010
790.979610	46228.746410	33.359028
791.446635	46296.044147	33.364045
792.605591	46369.794322	33.369063
793.515988	46439.749931	33.374080
794.143360	46513.020320	33.379098
795.015003	46577.225793	33.384116
795.637294	46660.669580	33.389133
796.459628	46734.650480	33.394151
798.072393	46782.533985	33.399168
799.019535	46861.468114	33.404186
800.062086	46917.006599	33.409204
800.658978	46982.603445	33.414221
801.502600	47050.110507	33.419239
802.272999	47109.107914	33.424256
802.804355	47182.161359	33.429274
803.662618	47246.592236	33.434292
804.353665	47332.096451	33.439309
804.852097	47396.318070	33.444327
805.882408	47465.669861	33.449344
806.421031	47545.675841	33.454362
807.216301	47611.635857	33.459380
808.030546	47687.303917	33.464397
808.609642	47774.807349	33.469415
809.416188	47852.147296	33.474432
809.807185	47934.657540	33.479450
810.892255	48012.169772	33.484468
812.102927	48092.199592	33.489485
812.646986	48167.810091	33.494503
814.215759	48233.120090	33.499520
815.448161	48293.345580	33.504538
817.068837	48342.901344	33.509556
817.887202	48410.416393	33.514573
818.584666	48465.164653	33.519591
819.776844	48514.021990	33.524608
820.146559	48588.054099	33.529626
820.643660	48643.434995	33.534644
821.576133	48702.569484	33.539661
822.017941	48763.362146	33.544679
822.553328	48830.188610	33.549696
823.328437	48893.251588	33.554714
824.218305	48963.781260	33.559732
825.133679	49035.256174	33.564749
825.808272	49105.319990	33.569767
826.584857	49176.190611	33.574784
827.575634	49254.012779	33.579802
827.993079	49316.335439	33.584820
828.811413	49386.156305	33.589837
829.688206	49456.271969	33.594855
830.530411	49526.880393	33.599872
830.997101	49607.075635	33.604890
831.760028	49677.399504	33.609908
832.780598	49748.929869	33.614925
833.325844	49815.422354	33.619943
834.219225	49880.310758	33.624960
835.180107	49954.894280	33.629978
836.019491	50026.042466	33.634996
836.565692	50106.100537	33.640013
837.356761	50174.713280	33.645031
838.347684	50245.060341	33.650048
838.616981	50325.086354	33.655066
839.814180	50405.373132	33.660084
840.653974	50472.739086	33.665101
841.331143	50547.640758	33.670119
842.789450	50624.838020	33.675136
843.653610	50706.613937	33.680154
844.195041	50786.384070	33.685172
845.289742	50860.924391	33.690189
845.505803	50938.385676	33.695207
846.676320	51018.027047	33.700224
847.713991	51099.315462	33.705242
848.900977	51164.509780	33.710260
850.321735	51243.499235	33.715277
850.997748	51319.067952	33.720295
851.865983	51388.906113	33.725312
852.547810	51463.594905	33.730330
853.278154	51542.155033	33.735348
853.999308	51617.635443	33.740365
854.952348	51689.213982	33.745383
855.791408	51771.067174	33.750400
856.186801	51848.427658	33.755418
857.083639	51930.671045	33.760436
857.814407	52014.003586	33.765453
858.672622	52097.506411	33.770471
859.978994	52177.839302	33.775488
860.940377	52257.270718	33.780506
862.140406	52327.034746	33.785524
863.409230	52397.060359	33.790541
864.128354	52475.391271	33.795559
864.906651	52545.310188	33.800576
866.038226	52629.651908	33.805594
866.772259	52700.514668	33.810612
867.914863	52764.967407	33.815629
868.299974	52834.176421	33.820647
869.046795	52905.676910	33.825664
869.967061	52986.705464	33.830682
870.788918	53068.319115	33.835700
871.527598	53146.244260	33.840717
872.286377	53220.907730	33.845735
873.456693	53297.424700	33.850752
874.827691	53366.374251	33.855770
875.600620	53444.972136	33.860788
876.170848	53511.572581	33.865805
877.272732	53594.454343	33.870823
877.972422	53663.237168	33.875840
878.803300	53742.769888	33.880858
879.356091	53817.638179	33.885876
880.666968	53889.680336	33.890893
881.881914	53967.654307	33.895911
882.659541	54044.215859	33.900928
883.930388	54110.905113	33.905946
885.148933	54166.693166	33.910964
886.787336	54228.800997	33.915981
887.665421	54281.851653	33.920999
888.208837	54328.715040	33.926016
889.073154	54393.854719	33.931034
889.845707	54441.973595	33.936052
891.008319	54497.612939	33.941069
891.428702	54548.773726	33.946087
892.689916	54597.481308	33.951104
893.037122	54653.279589	33.956122
893.440964	54710.904358	33.961140
894.148603	54760.046497	33.966157
894.616823	54826.350135	33.971175
895.726520	54889.959532	33.976192
896.233517	54965.041102	33.981210
896.880025	55035.968837	33.986228
897.647638	55104.340290	33.991245
898.077399	55187.452526	33.996263
899.294982	55269.398244	34.001280
900.040987	55356.954960	34.006298
901.125882	55436.301974	34.011316
901.877944	55518.631109	34.016333
902.294861	55614.568171	34.021351
903.413797	55690.284551	34.026368
904.119007	55777.431492	34.031386
905.075112	55869.596158	34.036404
906.136616	55957.561629	34.041421
907.320496	56063.209293	34.046439
908.327423	56135.799246	34.051456
909.409501	56227.749506	34.056474
910.380966	56314.160823	34.061492
911.553131	56396.478233	34.066509
912.378796	56485.450647	34.071527
913.342796	56566.636576	34.076544
914.278175	56642.365575	34.081562
915.199187	56734.811186	34.086580
916.423065	56812.552650	34.091597
917.230996	56902.674880	34.096615
918.054933	56975.827491	34.101632
920.133117	57043.342321	34.106650
920.916327	57116.792828	34.111668
922.252270	57177.082148	34.116685
923.044372	57255.961838	34.121703
924.084464	57325.961748	34.126720
924.880896	57384.171097	34.131738
925.834777	57460.380802	34.136756
927.255130	57515.145356	34.141773
928.276649	57579.813618	34.146791
929.392829	57641.593973	34.151808
929.812722	57709.805517	34.156826
930.676931	57778.125303	34.161844
931.629935	57837.248069	34.166861
932.431224	57913.299425	34.171879
932.919038	57966.817785	34.176896
933.689161	58056.241383	34.181914
934.296620	58135.083083	34.186932
935.439717	58206.246737	34.191949
935.903293	58295.801220	34.196967
936.794924	58369.472859	34.201984
937.851705	58447.916524	34.207002
938.641685	58547.927554	34.212020
939.410379	58626.511582	34.217037
940.558855	58711.467252	34.222055
941.485609	58802.141409	34.227072
942.324620	58893.044759	34.232090
943.004851	58984.916234	34.237108
944.377282	59066.192608	34.242125
945.129849	59157.319274	34.247143
946.029755	59245.030802	34.252160
946.613787	59336.874279	34.257178
947.450536	59431.489030	34.262196
948.523435	59521.636775	34.267213
949.632093	59613.311021	34.272231
950.601016	59701.791981	34.277248
951.448381	59787.671764	34.282266
952.368766	59892.484803	34.287284
953.336739	59967.858395	34.292301
954.225179	60062.258677	34.297319
955.215710	60143.230987	34.302336
956.331805	60221.398983	34.307354
957.006876	60305.224961	34.312372
957.889212	60384.372985	34.317389
959.112602	60473.101970	34.322407
960.283761	60552.458768	34.327424
961.488751	60630.759822	34.332442
962.190123	60716.583314	34.337460
963.329543	60797.161160	34.342477
964.437028	60880.617972	34.347495
965.454779	60967.405864	34.352512
966.618852	61037.814973	34.357530
967.540499	61121.782602	34.362548
968.253060	61198.161887	34.367565
969.449054	61270.927743	34.372583
970.397300	61366.602388	34.377600
971.593756	61452.648898	34.382618
972.477116	61543.207074	34.387636
973.282925	61628.618711	34.392653
973.908020	61706.399458	34.397671
974.876930	61796.881951	34.402688
976.056790	61889.110686	34.407706
976.710692	61973.743248	34.412724
977.719336	62068.999767	34.417741
978.690286	62164.034635	34.422759
979.823864	62245.327115	34.427776
981.159053	62336.748407	34.432794
981.996712	62429.861683	34.437812
983.045658	62515.896885	34.442829
984.330953	62608.327123	34.447847
985.271065	62682.611927	34.452864
986.644942	62771.927159	34.457882
987.449556	62855.558084	34.462900
988.683408	62939.217432	34.467917
989.865159	63026.980908	34.472935
990.474510	63104.996397	34.477952
991.712189	63178.894529	34.482970
992.731838	63263.474567	34.487988
993.735525	63347.766178	34.493005
994.608779	63424.374217	34.498023
995.293257	63508.146318	34.503040
996.595713	63586.618842	34.508058
997.849974	63670.404085	34.513076
998.886860	63750.659356	34.518093
999.803327	63840.581396	34.523111
1000.350421	63920.280398	34.528128
1001.769823	64003.851139	34.533146
1002.440284	64101.098930	34.538164
1003.612201	64175.187514	34.543181
1004.401786	64264.959905	34.548199
1005.083249	64353.116130	34.553216
1006.307532	64441.536361	34.558234
1007.118931	64528.957610	34.563252
1008.239871	64621.262638	34.568269
1008.791501	64719.442955	34.573287
1009.995542	64816.597804	34.578304
1011.112137	64906.024041	34.583322
1012.196718	64995.461911	34.588340
1013.085817	65085.247070	34.593357
1013.952098	65185.437762	34.598375
1015.202922	65290.082942	34.603392
1016.055635	65382.191943	34.608410
1016.867681	65470.983852	34.613428
1017.580733	65574.270461	34.618445
1018.982480	65665.047827	34.623463
1019.872536	65752.556049	34.628480
1021.180317	65846.077371	34.633498
1022.046528	65924.998654	34.638516
1023.240546	66022.172377	34.643533
1023.817460	66107.267771	34.648551
1024.767791	66191.596237	34.653568
1026.588214	66275.865521	34.658586
1027.470205	66359.375800	34.663604
1028.584207	66438.728622	34.668621
1029.863214	66523.304599	34.673639
1031.012216	66603.595842	34.678656
1031.923967	66676.624317	34.683674
1033.198307	66763.702672	34.688692
1033.891696	66835.100463	34.693709
1034.958011	66923.515997	34.698727
1035.429177	67017.323820	34.703744
1036.657432	67101.637374	34.708762
1037.618746	67204.531090	34.713780
1038.274957	67281.982409	34.718797
1039.518209	67387.055304	34.723815
1039.997518	67492.108254	34.728832
1041.095039	67587.808758	34.733850
1042.353292	67687.847019	34.738868
1043.184121	67801.197797	34.743885
1044.782502	67906.546791	34.748903
1045.507966	68003.281826	34.753920
1046.826666	68087.787169	34.758938
1048.392035	68187.444002	34.763956
1049.511201	68272.189958	34.768973
1050.895408	68357.692729	34.773991
1051.710318	68472.011367	34.779008
1053.045945	68546.821738	34.784026
1054.182006	68647.693228	34.789044
1055.221426	68738.981178	34.794061
1056.274369	68821.288855	34.799079
1057.203788	68910.378405	34.804096
1058.355315	69007.019240	34.809114
1059.104601	69103.070866	34.814132
1059.746915	69202.451080	34.819149
1061.106199	69300.985572	34.824167
1061.658233	69408.143559	34.829184
1063.105928	69502.251694	34.834202
1063.875470	69596.516386	34.839220
1064.547073	69712.148218	34.844237
1065.767756	69805.969859	34.849255
1066.812739	69920.651684	34.854272
1067.802153	70023.115392	34.859290
1068.830493	70135.856805	34.864308
1070.174792	70242.571981	34.869325
1071.832236	70352.765871	34.874343
1073.086082	70443.120956	34.879360
1074.735556	70527.608131	34.884378
1076.375459	70610.634324	34.889396
1077.555523	70706.751480	34.894413
1079.053083	70776.173341	34.899431
1079.522782	70860.256335	34.904448
1080.673420	70952.503613	34.909466
1081.829820	71026.361209	34.914484
1082.701709	71113.409271	34.919501
1083.714226	71191.760376	34.924519
1084.451834	71279.564448	34.929536
1085.437380	71367.165579	34.934554
1086.501448	71466.685099	34.939572
1087.234300	71561.874486	34.944589
1088.008058	71661.667904	34.949607
1089.059142	71752.363040	34.954624
1090.209479	71856.936622	34.959642
1091.298814	71964.015145	34.964660
1091.989216	72057.731117	34.969677
1093.041546	72142.538103	34.974695
1094.020270	72255.486357	34.979712
1095.217278	72323.958552	34.984730
1096.644509	72431.138363	34.989748
1097.486814	72529.341233	34.994765
1098.359060	72615.824275	34.999783
1099.728829	72719.315895	35.004800
1100.653309	72810.553668	35.009818
1101.728653	72902.743522	35.014836
1102.996916	73006.366055	35.019853
1103.885160	73107.337693	35.024871
1104.922308	73204.157513	35.029888
1105.904874	73308.256333	35.034906
1107.173256	73409.549924	35.039924
1108.298330	73511.132192	35.044941
1109.401724	73609.222431	35.049959
1110.566011	73724.415269	35.054976
1112.011213	73816.956042	35.059994
1113.306313	73926.809671	35.065012
1113.893050	74040.130535	35.070029
1115.395120	74138.084671	35.075047
1116.537417	74247.887411	35.080064
1117.378185	74346.768553	35.085082
1118.564824	74454.335978	35.090100
1119.616636	74572.298576	35.095117
1120.852366	74664.266910	35.100135
1121.693053	74778.830683	35.105152
1123.001317	74893.879493	35.110170
1124.182792	75002.387246	35.115188
1125.332611	75110.583701	35.120205
1126.555024	75224.532629	35.125223
1127.409813	75330.293223	35.130240
1128.527017	75450.440848	35.135258
1129.837053	75568.494299	35.140276
1131.040605	75681.523419	35.145293
1132.547627	75789.198328	35.150311
1133.768778	75894.156761	35.155328
1134.673797	76004.446965	35.160346
1136.058393	76113.218923	35.165364
1137.021005	76221.866995	35.170381
1138.865973	76328.009395	35.175399
1139.452448	76426.114396	35.180416
1140.677629	76536.002250	35.185434
1141.998492	76639.453315	35.190452
1143.123055	76751.080460	35.195469
1144.254254	76860.198878	35.200487
1145.331427	76966.007261	35.205504
1146.595239	77074.827215	35.210522
1147.552700	77175.398017	35.215540
1149.117500	77267.121321	35.220557
1150.864044	77351.026028	35.225575
1152.483334	77441.766029	35.230592
1153.795706	77530.970637	35.235610
1155.318767	77616.823781	35.240628
1156.897033	77698.082847	35.245645
1157.656045	77776.784088	35.250663
1158.723369	77865.888587	35.255680
1159.773319	77954.489364	35.260698
1160.983643	78027.699196	35.265716
1161.315829	78133.932102	35.270733
1162.689404	78216.542047	35.275751
1163.664089	78304.332246	35.280768
1165.174290	78394.129616	35.285786
1166.013631	78482.980242	35.290804
1166.787071	78573.754316	35.295821
1167.690631	78672.666808	35.300839
1168.854285	78773.515430	35.305856
1169.751652	78876.230115	35.310874
1171.029420	78969.080617	35.315892
1171.806562	79060.666499	35.320909
1172.622014	79159.505774	35.325927
1173.482778	79266.648919	35.330944
1174.502366	79380.013379	35.335962
1175.576980	79481.828596	35.340980
1176.996851	79598.932243	35.345997
1177.636691	79691.631096	35.351015
1178.795408	79809.789785	35.356032
1179.921499	79927.840036	35.361050
1181.232537	80039.020792	35.366068
1182.581419	80165.284833	35.371085
1183.779233	80266.817708	35.376103
1185.461981	80383.896421	35.381120
1186.372545	80505.542680	35.386138
1187.979892	80615.184663	35.391156
1188.961925	80735.857946	35.396173
1189.783945	80838.921030	35.401191
1191.128176	80962.566871	35.406208
1192.515793	81079.466396	35.411226
1193.878324	81197.092473	35.416244
1194.871121	81313.509645	35.421261
1196.478084	81438.687712	35.426279
1197.766504	81543.720590	35.431296
1199.007853	81665.915879	35.436314
1200.482190	81774.240129	35.441332
1201.633077	81898.452321	35.446349
1202.706812	82001.049726	35.451367
1203.889846	82121.647009	35.456384
1204.480921	82235.925978	35.461402
1205.921045	82349.528446	35.466420
1207.024721	82480.478296	35.471437
1208.241482	82602.934877	35.476455
1209.816214	82731.291226	35.481472
1210.951961	82855.788731	35.486490
1212.467943	82972.207344	35.491508
1213.673282	83102.523407	35.496525
1214.766151	83217.754528	35.501543
1216.075176	83328.720562	35.506560
1217.589273	83448.131633	35.511578
1218.720142	83557.960612	35.516596
1220.122365	83674.450493	35.521613
1221.553014	83798.640147	35.526631
1222.494726	83914.277735	35.531648
1223.889111	84033.165055	35.536666
1225.403887	84138.869222	35.541684
1226.551955	84247.519800	35.546701
1227.836681	84359.925432	35.551719
1228.732078	84483.073670	35.556736
1230.314632	84588.388822	35.561754
1232.090279	84697.323552	35.566772
1233.579358	84797.332205	35.571789
1234.696061	84895.245084	35.576807
1236.026433	85003.375980	35.581824
1236.591260	85111.854523	35.586842
1238.412394	85213.827658	35.591860
1239.065474	85326.512789	35.596877
1240.417900	85437.492919	35.601895
1241.402515	85548.404013	35.606912
1242.811258	85653.914851	35.611930
1244.435239	85751.903740	35.616948
1245.510211	85858.975183	35.621965
1246.562884	85966.341938	35.626983
1248.263046	86071.226048	35.632000
1248.893411	86185.527355	35.637018
1250.391291	86293.586324	35.642036
1251.497611	86404.722517	35.647053
1253.190920	86509.203784	35.652071
1254.526073	86594.264573	35.657088
1255.773136	86701.489746	35.662106
1256.353712	86786.339079	35.667124
1257.384272	86882.117869	35.672141
1258.365457	86980.274322	35.677159
1259.464012	87094.126162	35.682176
1260.525543	87214.054141	35.687194
1261.956153	87316.133479	35.692212
1262.976069	87429.390603	35.697229
1264.024359	87553.034984	35.702247
1265.093341	87658.973477	35.707264
1266.486174	87779.016943	35.712282
1267.565543	87904.229337	35.717300
1268.644134	88027.136000	35.722317
1269.834862	88165.029963	35.727335
1271.362260	88287.538371	35.732352
1272.472930	88425.940247	35.737370
1273.605256	88563.211532	35.742388
1274.811520	88692.044581	35.747405
1276.112635	88829.569632	35.752423
1277.526103	88961.007542	35.757440
1278.840845	89104.019090	35.762458
1280.295091	89236.136211	35.767476
1281.730903	89370.715355	35.772493
1283.196811	89509.675309	35.777511
1284.721073	89626.626272	35.782528
1285.885954	89763.061621	35.787546
1287.418077	89891.443618	35.792564
1289.429366	90007.851364	35.797581
1290.948572	90130.279954	35.802599
1292.416403	90242.299516	35.807616
1293.619667	90377.806545	35.812634
1295.076312	90485.557808	35.817652
1296.482856	90607.460930	35.822669
1297.211086	90736.389911	35.827687
1298.996945	90835.194325	35.832704
1300.263397	90954.155030	35.837722
1301.249082	91073.033170	35.842740
1302.707987	91191.014327	35.847757
1304.113755	91317.166171	35.852775
1305.602550	91427.919515	35.857792
1306.322775	91549.261566	35.862810
1307.728453	91668.761078	35.867828
1309.088669	91799.155141	35.872845
1310.238301	91929.379758	35.877863
1311.439966	92038.621120	35.882880
1313.117293	92175.710093	35.887898
1314.423737	92305.265535	35.892916
1315.435410	92431.711507	35.897933
1316.629241	92570.461808	35.902951
1318.097113	92687.534853	35.907968
1319.594495	92814.477165	35.912986
1320.166268	92947.470404	35.918004
1321.858762	93073.749700	35.923021
1322.724173	93219.487068	35.928039
1324.508572	93349.238724	35.933056
1325.797772	93481.159341	35.938074
1326.847393	93608.453491	35.943092
1328.476542	93743.605098	35.948109
1329.401200	93886.700048	35.953127
1331.141169	94018.058491	35.958144
1332.488338	94160.683354	35.963162
1333.838371	94294.157023	35.968180
1334.833899	94427.711799	35.973197
1336.012011	94568.019960	35.978215
1337.234497	94694.924117	35.983232
1339.795313	94801.961108	35.988250
1342.168835	94916.037082	35.993268
1343.582022	95016.751000	35.998285
1344.764363	95118.578587	36.003303
1346.286265	95209.389386	36.008320
1347.261300	95324.229583	36.013338
1347.977075	95423.380207	36.018356
1349.522708	95532.212882	36.023373
1350.664436	95640.867969	36.028391
1351.751067	95743.498391	36.033408
1352.763147	95860.502341	36.038426
1353.676387	95982.769881	36.043444
1354.969129	96098.970494	36.048461
1356.086166	96240.715409	36.053479
1357.575447	96368.966544	36.058496
1358.719972	96498.387351	36.063514
1360.223682	96630.972497	36.068532
1361.318212	96767.855703	36.073549
1362.367922	96916.040926	36.078567
1363.906996	97050.713904	36.083584
1365.351628	97195.631895	36.088602
1366.735691	97328.682275	36.093620
1367.930649	97474.020697	36.098637
1369.424157	97625.867032	36.103655
1370.940675	97763.145230	36.108672
1372.685621	97909.857846	36.113690
1373.611819	98061.515686	36.118708
1374.845379	98209.817802	36.123725
1376.486248	98361.974320	36.128743
1378.004432	98496.466552	36.133760
1379.379298	98651.112473	36.138778
1381.088864	98790.380680	36.143796
1383.114894	98919.331912	36.148813
1385.122273	99045.155350	36.153831
1386.970692	99163.435830	36.158848
1388.567242	99280.006513	36.163866
1389.455005	99407.945239	36.168884
1391.133621	99529.638298	36.173901
1392.318201	99663.325318	36.178919
1393.572463	99785.972805	36.183936
1394.805169	99913.859855	36.188954
1396.454033	100045.637985	36.193972
1397.945999	100167.007542	36.198989
1399.090681	100298.763761	36.204007
1400.552001	100428.506215	36.209024
1402.233341	100552.269155	36.214042
1403.190067	100682.357395	36.219060
1404.544929	100816.238206	36.224077
1405.913513	100957.571947	36.229095
1407.322188	101088.504269	36.234112
1408.574305	101226.408947	36.239130
1409.926610	101368.495002	36.244148
1411.515067	101497.334487	36.249165
1412.935763	101630.574505	36.254183
1414.405583	101754.298878	36.259200
1416.484835	101888.616507	36.264218
1417.784121	102009.389034	36.269236
1419.581714	102145.982914	36.274253
1420.642694	102283.490746	36.279271
1422.128688	102399.963077	36.284288
1423.575850	102528.663798	36.289306
1424.595686	102651.181082	36.294324
1426.249848	102778.481294	36.299341
1427.446531	102914.677440	36.304359
1428.948720	103048.392314	36.309376
1430.381886	103174.181667	36.314394
1431.349682	103312.570441	36.319412
1433.020291	103442.837460	36.324429
1434.123785	103589.358678	36.329447
1435.485016	103721.716227	36.334464
1436.892241	103838.763761	36.339482
1438.158896	103967.371389	36.344500
1439.502076	104091.098885	36.349517
1440.560306	104224.862245	36.354535
1441.941500	104350.118945	36.359552
1443.584984	104493.910174	36.364570
1444.772219	104628.555288	36.369588
1446.261328	104750.804412	36.374605
1447.094921	104898.058064	36.379623
1448.631082	105042.958772	36.384640
1450.075146	105179.987874	36.389658
1451.198921	105336.974075	36.394676
1452.977997	105480.228572	36.399693
1454.216880	105637.464525	36.404711
1455.904838	105790.294893	36.409728
1457.011865	105936.914585	36.414746
1458.608694	106101.489220	36.419764
1460.444959	106255.845531	36.424781
1461.713397	106414.804944	36.429799
1463.285472	106575.987539	36.434816
1464.733085	106729.835902	36.439834
1466.055023	106888.675081	36.444852
1467.437945	107057.801718	36.449869
1469.159381	107221.449411	36.454887
1470.700493	107386.533453	36.459904
1472.427386	107539.327578	36.464922
1473.647784	107706.656762	36.469940
1475.389548	107870.253666	36.474957
1477.165020	108013.417943	36.479975
1478.720399	108167.763208	36.484992
1480.538908	108320.115407	36.490010
1482.311457	108476.545900	36.495028
1484.362168	108616.017831	36.500045
1486.075822	108751.599090	36.505063
1487.586237	108896.076351	36.510080
1489.632970	109027.244673	36.515098
1491.049803	109173.703178	36.520116
1492.751287	109298.420989	36.525133
1494.213812	109443.148915	36.530151
1495.131210	109574.875506	36.535168
1497.207353	109702.098008	36.540186
1498.636591	109832.046645	36.545204
1500.050480	109964.711916	36.550221
1501.372800	110112.089430	36.555239
1502.740022	110236.456819	36.560256
1504.373320	110372.386602	36.565274
1505.674753	110521.531783	36.570292
1506.871802	110652.419972	36.575309
1508.298781	110793.925259	36.580327
1509.788139	110951.577612	36.585344
1511.308435	111094.337727	36.590362
1512.501613	111248.550081	36.595380
1514.194940	111407.631103	36.600397
1515.584872	111553.114549	36.605415
1516.806394	111708.858978	36.610432
1518.779784	111861.101021	36.615450
1519.946071	112019.214221	36.620468
1521.318568	112165.615979	36.625485
1522.768853	112325.360345	36.630503
1523.898208	112483.709625	36.635520
1525.548171	112641.826389	36.640538
1526.836016	112808.966488	36.645556
1528.525031	112974.345509	36.650573
1529.713958	113141.591326	36.655591
1531.402415	113306.413940	36.660608
1533.017231	113472.910161	36.665626
1533.762149	113646.213505	36.670644
1535.635937	113811.871985	36.675661
1536.935435	113979.117149	36.680679
1538.341300	114140.474478	36.685696
1539.932250	114294.067290	36.690714
1541.384951	114469.521915	36.695732
1543.009923	114615.019206	36.700749
1544.976993	114760.628709	36.705767
1546.215143	114930.906304	36.710784
1548.191550	115094.969289	36.715802
1549.006533	115265.732839	36.720820
1550.848683	115423.869865	36.725837
1552.761931	115588.084398	36.730855
1554.088674	115743.741029	36.735872
1555.893262	115910.738844	36.740890
1557.416784	116081.839809	36.745908
1559.219435	116238.984500	36.750925
1561.269416	116389.762351	36.755943
1562.729484	116549.523723	36.760960
1564.375010	116701.253632	36.765978
1566.387966	116858.533099	36.770996
1567.847494	117024.625686	36.776013
1569.606384	117174.678327	36.781031
1570.730301	117348.789927	36.786048
1572.562991	117510.755123	36.791066
1573.801717	117666.890120	36.796084
1575.622666	117830.418634	36.801101
1576.880177	117995.570310	36.806119
1578.788120	118153.252079	36.811136
1580.340526	118319.970144	36.816154
1581.909278	118489.794005	36.821172
1583.260182	118666.933240	36.826189
1584.848729	118836.438470	36.831207
1586.215243	119006.105858	36.836224
1587.950093	119176.135257	36.841242
1589.352164	119349.730784	36.846260
1590.681056	119525.317264	36.851277
1592.176489	119710.924755	36.856295
1593.771751	119905.942241	36.861312
1595.452332	120075.172275	36.866330
1596.795786	120262.239451	36.871348
1598.772548	120437.856120	36.876365
1600.885296	120626.023064	36.881383
1602.125097	120814.440957	36.886400
1604.052485	120994.088945	36.891418
1605.624327	121165.027780	36.896436
1607.424006	121343.695152	36.901453
1609.216240	121520.474423	36.906471
1610.563884	121712.723476	36.911488
1612.225632	121880.695820	36.916506
1613.812917	122066.148095	36.921524
1615.150841	122245.576471	36.926541
1616.629824	122430.857048	36.931559
1618.381485	122617.833966	36.936576
1620.127754	122800.968901	36.941594
1621.906988	122983.731674	36.946612
1623.356370	123178.750209	36.951629
1625.354384	123352.511895	36.956647
1626.800990	123543.219523	36.961664
1628.695908	123707.700158	36.966682
1630.417382	123883.283221	36.971700
1632.125879	124063.727783	36.976717
1634.506976	124225.940227	36.981735
1635.683292	124399.085901	36.986752
1637.438993	124563.249210	36.991770
1639.055663	124733.473425	36.996788
1641.337814	124891.124272	37.001805
1643.160047	125054.251652	37.006823
1644.894678	125211.544954	37.011840
1646.961801	125350.150910	37.016858
1648.702190	125485.217954	37.021876
1650.080945	125610.649323	37.026893
1652.608182	125722.467391	37.031911
1654.309615	125841.556780	37.036928
1656.062610	125956.287021	37.041946
1657.636830	126071.603620	37.046964
1659.028359	126211.713194	37.051981
1660.343871	126335.723060	37.056999
1661.556189	126468.236744	37.062016
1663.093466	126609.238438	37.067034
1664.491294	126745.022692	37.072052
1665.559071	126900.637485	37.077069
1667.035743	127050.378650	37.082087
1668.328993	127212.556693	37.087104
1669.529000	127385.318115	37.092122
1671.122621	127555.621155	37.097140
1672.313309	127740.159052	37.102157
1673.874283	127904.657935	37.107175
1674.897962	128100.286589	37.112192
1676.413374	128291.703593	37.117210
1677.860714	128488.206985	37.122228
1679.547666	128688.023468	37.127245
1680.784627	128895.688325	37.132263
1682.220182	129111.088035	37.137280
1684.016504	129321.218120	37.142298
1685.597560	129537.168305	37.147316
1687.118120	129757.709258	37.152333
1689.014773	129975.985159	37.157351
1690.631085	130208.186273	37.162368
1692.514676	130428.077883	37.167386
1694.046478	130652.123583	37.172404
1696.130465	130881.832182	37.177421
1697.968688	131098.130910	37.182439
1699.496820	131338.231181	37.187456
1701.577180	131542.542233	37.192474
1703.834431	131768.739354	37.197492
1705.096512	131995.929976	37.202509
1706.816349	132205.946585	37.207527
1708.536324	132439.869246	37.212544
1710.131477	132673.330425	37.217562
1712.033964	132898.522810	37.222580
1713.694790	133128.791364	37.227597
1715.621163	133347.688764	37.232615
1717.836126	133575.132648	37.237632
1719.604643	133797.140229	37.242650
1721.660767	134012.417102	37.247668
1723.282717	134240.388132	37.252685
1725.430299	134444.055140	37.257703
1727.363464	134651.334778	37.262720
1728.813194	134861.114250	37.267738
1730.591895	135068.140703	37.272756
1732.114760	135300.345392	37.277773
1734.428671	135511.008549	37.282791
1736.008381	135733.105910	37.287808
1737.512908	135947.297839	37.292826
1738.968374	136155.686615	37.297844
1740.660416	136385.256513	37.302861
1742.303762	136603.985498	37.307879
1744.010216	136828.086148	37.312896
1745.045063	137058.256617	37.317914
1746.969314	137286.792416	37.322932
1748.713492	137520.940934	37.327949
1750.510545	137749.016610	37.332967
1752.072472	137985.391216	37.337984
1753.778105	138226.414616	37.343002
1755.369140	138462.863265	37.348020
1757.175207	138698.061386	37.353037
1759.274201	138926.349657	37.358055
1760.789526	139148.232425	37.363072
1762.300294	139375.802254	37.368090
1764.406846	139579.600050	37.373108
1766.203496	139795.845595	37.378125
1768.146439	139998.655424	37.383143
1770.041302	140207.933133	37.388160
1771.362774	140430.727753	37.393178
1773.414695	140644.767330	37.398196
1774.845360	140866.227152	37.403213
1776.662873	141098.326188	37.408231
1778.528037	141314.974075	37.413248
1779.550454	141553.151096	37.418266
1781.543865	141781.279153	37.423284
1783.201806	142025.476673	37.428301
1784.665330	142257.737906	37.433319
1786.493348	142505.261835	37.438336
1788.561972	142735.413261	37.443354
1790.934214	142983.108735	37.448372
1792.626077	143221.760836	37.453389
1794.152962	143460.338238	37.458407
1795.886373	143702.247908	37.463424
1797.574543	143941.475181	37.468442
1799.707451	144190.432353	37.473460
1801.706110	144428.344476	37.478477
1803.848952	144672.200432	37.483495
1805.886255	144916.619750	37.488512
1807.460187	145157.977472	37.493530
1809.329654	145408.060506	37.498548
1811.120513	145657.040111	37.503565
1812.488275	145897.887692	37.508583
1814.532892	146150.739387	37.513600
1816.418840	146403.388569	37.518618
1818.802507	146642.748867	37.523636
1820.551855	146901.577519	37.528653
1822.264633	147141.666477	37.533671
1824.194886	147388.716251	37.538688
1825.826062	147635.001427	37.543706
1827.986887	147881.421110	37.548724
1829.902239	148137.678883	37.553741
1831.217010	148375.614265	37.558759
1833.138778	148640.250679	37.563776
1834.545732	148902.303051	37.568794
1836.797098	149152.116281	37.573812
1838.526721	149400.679129	37.578829
1840.855319	149641.991058	37.583847
1843.200085	149897.632035	37.588864
1844.703431	150151.767772	37.593882
1846.872530	150398.045558	37.598900
1848.813689	150648.827966	37.603917
1850.368650	150895.203600	37.608935
1852.127696	151139.124156	37.613952
1853.812210	151413.458144	37.618970
1855.972234	151667.739956	37.623988
1857.508905	151932.693684	37.629005
1858.941324	152191.241948	37.634023
1861.141631	152451.829832	37.639040
1862.504933	152712.714227	37.644058
1864.570667	152977.095554	37.649076
1866.459727	153228.430975	37.654093
1868.628217	153496.289568	37.659111
1870.108032	153758.201601	37.664128
1871.557052	154024.321361	37.669146
1873.659061	154284.552242	37.674164
1875.256348	154560.654370	37.679181
1876.486685	154837.335405	37.684199
1878.140482	155105.789460	37.689216
1879.867717	155398.758763	37.694234
1881.699765	155677.241639	37.699252
1883.257965	155953.102638	37.704269
1884.990764	156228.138016	37.709287
1886.945462	156502.721231	37.714304
1888.515037	156783.979566	37.719322
1890.411410	157051.401958	37.724340
1892.474503	157335.505886	37.729357
1894.561413	157606.988835	37.734375
1896.550271	157880.798744	37.739392
1898.659669	158144.092450	37.744410
1901.159584	158424.160061	37.749428
1902.858848	158701.421028	37.754445
1905.022002	158963.541999	37.759463
1907.090955	159235.822176	37.764480
1908.746742	159514.667810	37.769498
1911.115735	159787.893970	37.774516
1912.936411	160081.112928	37.779533
1914.583322	160356.231326	37.784551
1916.582143	160630.407492	37.789568
1918.292004	160916.550893	37.794586
1920.251091	161198.606933	37.799604
1922.232582	161487.706806	37.804621
1924.271760	161774.158326	37.809639
1925.494602	162062.198193	37.814656
1928.267757	162343.104273	37.819674
1931.145264	162598.883007	37.824692
1933.512542	162878.699279	37.829709
1935.068848	163157.081378	37.834727
1937.287894	163429.927643	37.839744
1939.193056	163709.705153	37.844762
1941.425320	163976.508328	37.849780
1943.377203	164254.465346	37.854797
1945.130394	164536.491845	37.859815
1946.742153	164816.002304	37.864832
1947.912860	165101.105466	37.869850
1949.690063	165399.103823	37.874868
1951.292548	165697.676636	37.879885
1953.158412	166003.230923	37.884903
1954.694468	166305.181310	37.889920
1956.153874	166617.962450	37.894938
1958.349195	166934.883854	37.899956
1959.905964	167261.999970	37.904973
1961.528680	167588.523310	37.909991
1963.746898	167922.827524	37.915008
1965.332687	168256.774667	37.920026
1967.487001	168588.565302	37.925044
1969.454232	168929.668110	37.930061
1971.453783	169257.562567	37.935079
1974.423925	169576.419478	37.940096
1976.592100	169907.909325	37.945114
1979.031991	170220.299846	37.950132
1981.260434	170533.283290	37.955149
1983.649707	170854.178870	37.960167
1985.324752	171177.536015	37.965184
1986.838556	171495.180410	37.970202
1989.281623	171819.627062	37.975220
1991.310150	172128.877162	37.980237
1992.813485	172454.602872	37.985255
1994.735461	172777.928448	37.990272
1996.440126	173106.609549	37.995290
1998.185097	173435.907966	38.000308
2000.264188	173773.802997	38.005325
2001.749180	174117.798046	38.010343
2004.038803	174452.806210	38.015360
2005.258160	174792.121902	38.020378
2007.450359	175136.773185	38.025396
2009.533670	175475.944616	38.030413
2011.421165	175818.055821	38.035431
2013.923002	176140.517619	38.040448
2016.186873	176468.160514	38.045466
2018.110798	176780.746637	38.050484
2020.336066	177094.556873	38.055501
2022.289958	177418.569239	38.060519
2024.333201	177730.226059	38.065536
2026.027098	178061.570263	38.070554
2028.392797	178370.741137	38.075572
2030.322808	178691.282673	38.080589
2032.295075	179011.590246	38.085607
2034.138265	179327.017396	38.090624
2036.226724	179651.753772	38.095642
2038.676812	179971.253964	38.100660
2040.696210	180299.432133	38.105677
2042.690903	180630.409100	38.110695
2044.826738	180946.990151	38.115712
2046.846285	181295.744159	38.120730
2048.729347	181627.199296	38.125748
2050.759948	181957.388157	38.130765
2052.344211	182307.178863	38.135783
2054.397168	182639.830286	38.140800
2056.382851	182986.538652	38.145818
2058.245911	183332.708600	38.150836
2061.130590	183665.411959	38.155853
2063.568275	184006.491387	38.160871
2065.453838	184355.328354	38.165888
2067.517108	184694.868333	38.170906
2069.542033	185034.237651	38.175924
2071.718516	185396.748422	38.180941
2073.825895	185744.996963	38.185959
2076.049037	186083.424600	38.190976
2078.129634	186426.142615	38.195994
2079.981450	186849.692703	38.201012
2081.813262	187218.232400	38.206029
2083.447544	187580.022449	38.211047
2085.512219	187943.956512	38.216064
2087.189322	188323.014151	38.221082
2089.329742	188692.399883	38.226100
2091.145317	189066.383994	38.231117
2092.945767	189457.694500	38.236135
2095.000920	189838.298708	38.241152
2096.976734	190222.066162	38.246170
2099.172570	190622.590212	38.251188
2101.656721	191010.040416	38.256205
2103.655096	191403.282594	38.261223
2105.977840	191794.316556	38.266240
2108.326749	192191.418460	38.271258
2109.869292	192582.906613	38.276276
2112.297364	192971.743530	38.281293
2114.214289	193373.412422	38.286311
2116.548794	193754.595297	38.291328
2118.999468	194145.947024	38.296346
2121.781243	194524.725699	38.301364
2123.894209	194915.700495	38.306381
2126.202244	195304.690201	38.311399
2128.474710	195684.059498	38.316416
2130.629484	196064.616638	38.321434
2132.652477	196444.280895	38.326452
2134.940723	196824.235130	38.331469
2137.016463	197213.037800	38.336487
2139.439776	197590.077297	38.341504
2141.691018	197962.521456	38.346522
2143.685815	198330.967597	38.351540
2146.012938	198714.705624	38.356557
2148.117556	199090.960307	38.361575
2150.366307	199456.067444	38.366592
2152.624408	199830.191695	38.371610
2155.113394	200186.956712	38.376628
2157.239819	200560.442735	38.381645
2159.362236	200902.660188	38.386663
2161.179201	201258.871710	38.391680
2163.585547	201602.621370	38.396698
2165.285532	201943.458787	38.401716
2167.227015	202281.592054	38.406733
2168.977969	202644.192758	38.411751
2170.885702	202997.599521	38.416768
2173.246280	203358.354044	38.421786
2175.321158	203720.804915	38.426804
2177.802426	204081.516682	38.431821
2180.224375	204451.129310	38.436839
2182.423817	204806.704179	38.441856
2184.375495	205180.151000	38.446874
2185.947306	205548.602487	38.451892
2188.014591	205925.665319	38.456909
2189.697147	206321.713886	38.461927
2191.781996	206717.344955	38.466944
2193.719188	207109.595737	38.471962
2195.696841	207526.024632	38.476980
2197.591492	207929.511646	38.481997
2199.813179	208344.786343	38.487015
2201.477383	208765.661032	38.492032
2203.757732	209178.717994	38.497050
2205.391388	209622.284016	38.502068
2207.934566	210046.783802	38.507085
2210.231436	210495.277989	38.512103
2212.288824	210932.912145	38.517120
2214.727158	211374.018795	38.522138
2216.810877	211817.035779	38.527156
2219.924473	212243.838138	38.532173
2221.855625	212680.783321	38.537191
2224.474410	213134.413881	38.542208
2226.781547	213575.772826	38.547226
2229.219563	214009.694121	38.552244
2232.144998	214440.491666	38.557261
2234.568895	214882.469210	38.562279
2236.582977	215306.957068	38.567296
2239.174064	215737.706540	38.572314
2241.525437	216160.593197	38.577332
2244.298296	216584.710280	38.582349
2246.418965	217007.278021	38.587367
2248.950722	217435.015373	38.592384
2251.861791	217847.604158	38.597402
2253.694998	218269.226990	38.602420
2256.017103	218680.968148	38.607437
2258.265797	219105.956491	38.612455
2260.002132	219540.246513	38.617472
2262.109595	219948.948062	38.622490
2264.369446	220391.134019	38.627508
2266.571700	220820.982850	38.632525
2269.076957	221246.491474	38.637543
2271.456649	221675.805048	38.642560
2273.964403	222101.212062	38.647578
2275.855749	222520.338753	38.652596
2278.065161	222959.078842	38.657613
2280.416390	223395.815480	38.662631
2282.316534	223831.657080	38.667648
2285.014544	224260.515502	38.672666
2286.662369	224698.911545	38.677684
2288.919935	225140.667710	38.682701
2290.931522	225592.141153	38.687719
2293.061932	226030.081138	38.692736
2295.467895	226486.650245	38.697754
2297.411346	226936.559215	38.702772
2299.836105	227387.663435	38.707789
2302.212781	227845.888206	38.712807
2304.591608	228297.278845	38.717824
2306.551152	228743.323548	38.722842
2308.684432	229178.061669	38.727860
2310.736431	229614.488955	38.732877
2313.101172	230051.019821	38.737895
2315.181311	230492.700995	38.742912
2317.603470	230924.395750	38.747930
2319.358739	231376.517265	38.752948
2321.879502	231826.995136	38.757965
2324.394073	232272.621516	38.762983
2326.451748	232717.963036	38.768000
2328.610812	233184.246690	38.773018
2330.812509	233651.844325	38.778036
2333.365823	234103.306163	38.783053
2335.687972	234575.863369	38.788071
2337.823617	235039.456166	38.793088
2340.595301	235506.506032	38.798106
2342.613570	235988.203598	38.803124
2344.882877	236464.577542	38.808141
2347.721573	236942.767566	38.813159
2349.605620	237426.541927	38.818176
2352.678001	237896.158685	38.823194
2355.209202	238374.724877	38.828212
2357.864847	238851.111699	38.833229
2360.764588	239319.254470	38.838247
2363.137785	239783.896570	38.843264
2365.663888	240234.872482	38.848282
2368.568612	240711.471612	38.853300
2370.991000	241170.108586	38.858317
2373.865870	241620.037224	38.863335
2376.324477	242077.346008	38.868352
2378.870004	242533.979952	38.873370
2380.794830	243005.240267	38.878388
2382.970119	243473.285280	38.883405
2385.335747	243950.622661	38.888423
2387.442288	244427.313473	38.893440
2389.689385	244889.527086	38.898458
2392.524850	245363.028649	38.903476
2395.062147	245821.003590	38.908493
2397.479373	246292.408874	38.913511
2399.817043	246762.860125	38.918528
2402.531858	247237.341383	38.923546
2404.457542	247714.763961	38.928564
2406.769742	248196.519813	38.933581
2409.029240	248664.717671	38.938599
2411.010439	249162.399018	38.943616
2413.286720	249652.539340	38.948634
2415.413430	250156.647387	38.953652
2417.494994	250657.611078	38.958669
2420.122516	251165.677081	38.963687
2421.772333	251678.415201	38.968704
2424.050662	252184.652560	38.973722
2426.308973	252705.878483	38.978740
2428.825501	253231.888775	38.983757
2431.373579	253748.544484	38.988775
2434.164468	254269.656667	38.993792
2436.479896	254794.651181	38.998810
2438.814228	255321.723717	39.003828
2441.596507	255847.302066	39.008845
2444.246529	256378.614242	39.013863
2446.628538	256905.774837	39.018880
2449.507861	257425.388031	39.023898
2451.619006	257948.954222	39.028916
2453.843513	258465.769408	39.033933
2457.083319	258991.086095	39.038951
2459.771911	259496.800871	39.043968
2462.664072	260009.339992	39.048986
2464.888728	260530.464519	39.054004
2467.180090	261041.187657	39.059021
2469.502306	261536.155656	39.064039
2472.147362	262034.932080	39.069056
2474.444690	262525.251441	39.074074
2476.531756	263017.049156	39.079092
2478.805279	263516.994357	39.084109
2481.142361	264011.110859	39.089127
2483.185412	264515.760817	39.094144
2485.449951	265020.856485	39.099162
2488.646861	265522.248719	39.104180
2490.879722	266010.301621	39.109197
2493.753902	266520.832062	39.114215
2496.062639	267037.391231	39.119232
2498.701078	267542.390789	39.124250
2501.297314	268051.331090	39.129268
2503.840459	268557.406955	39.134285
2506.344476	269072.528027	39.139303
2508.836208	269601.896572	39.144320
2511.303103	270098.731119	39.149338
2513.488874	270636.497329	39.154356
2515.715185	271177.250990	39.159373
2518.337080	271695.996344	39.164391
2520.392196	272238.878241	39.169408
2522.997861	272784.160046	39.174426
2525.325824	273333.189628	39.179444
2527.636319	273882.573983	39.184461
2530.589468	274429.492878	39.189479
2532.729074	274990.782315	39.194496
2535.671476	275549.835127	39.199514
2538.045523	276103.182236	39.204532
2540.528077	276670.857480	39.209549
2543.718367	277227.269774	39.214567
2546.497702	277788.846667	39.219584
2549.124409	278343.916646	39.224602
2551.858193	278911.003402	39.229620
2554.362394	279479.950160	39.234637
2557.126719	280051.086945	39.239655
2559.553658	280616.177155	39.244672
2561.913010	281176.169288	39.249690
2564.551892	281751.528073	39.254708
2566.721547	282316.797668	39.259725
2569.429747	282887.946626	39.264743
2572.031083	283469.315963	39.269760
2574.176549	284054.560510	39.274778
2576.960651	284628.349955	39.279796
2579.300339	285225.540131	39.284813
2582.122433	285813.610165	39.289831
2584.309015	286399.183962	39.294848
2587.119842	286995.218806	39.299866
2589.715569	287576.198797	39.304884
2592.085328	288182.042264	39.309901
2595.024683	288770.804372	39.314919
2597.618289	289377.922264	39.319936
2600.422111	289964.993338	39.324954
2603.080424	290565.031102	39.329972
2605.888503	291171.489128	39.334989
2608.858385	291749.910248	39.340007
2611.930333	292341.792369	39.345024
2614.634629	292913.464675	39.350042
2617.334682	293496.303822	39.355060
2619.724029	294084.517516	39.360077
2622.608364	294667.240455	39.365095
2625.301294	295255.903124	39.370112
2627.427723	295828.551505	39.375130
2630.337828	296414.579063	39.380148
2632.896445	297001.721692	39.385165
2635.298585	297588.171793	39.390183
2637.805757	298172.619253	39.395200
2640.479017	298762.086941	39.400218
2643.184833	299337.656489	39.405236
2645.463413	299905.441955	39.410253
2648.120338	300455.011126	39.415271
2650.855200	301011.721653	39.420288
2653.717142	301563.100959	39.425306
2656.237999	302119.833381	39.430324
2658.756224	302685.369278	39.435341
2661.512658	303246.064224	39.440359
2664.096934	303813.126300	39.445376
2666.196286	304380.206925	39.450394
2669.364542	304946.988095	39.455412
2672.222393	305524.472779	39.460429
2675.289040	306071.914450	39.465447
2677.903622	306641.174515	39.470464
2680.402060	307212.223082	39.475482
2683.459013	307777.593915	39.480500
2686.570827	308348.635570	39.485517
2689.222963	308910.731316	39.490535
2691.427429	309494.439924	39.495552
2694.049676	310081.782310	39.500570
2696.358128	310658.759886	39.505588
2698.901950	311265.263288	39.510605
2701.404475	311848.668599	39.515623
2703.921846	312455.338615	39.520640
2706.287024	313069.105649	39.525658
2708.617146	313681.093473	39.530676
2711.097691	314291.400135	39.535693
2713.957567	314918.187091	39.540711
2716.326779	315560.573828	39.545728
2718.815612	316199.608256	39.550746
2721.754408	316834.401560	39.555764
2724.274104	317476.889872	39.560781
2727.167545	318123.675699	39.565799
2729.710390	318773.780283	39.570816
2732.545051	319434.259723	39.575834
2735.799913	320105.017365	39.580852
2738.217199	320769.779305	39.585869
2740.991162	321421.863722	39.590887
2743.780388	322084.263549	39.595904
2746.745473	322741.880538	39.600922
2749.399120	323403.341890	39.605940
2752.215139	324081.793531	39.610957
2755.361145	324748.992925	39.615975
2758.449231	325415.074102	39.620992
2760.749101	326076.826845	39.626010
2763.606854	326746.753425	39.631028
2766.470318	327420.093226	39.636045
2769.304098	328086.119321	39.641063
2772.374008	328769.958850	39.646080
2775.097714	329433.442363	39.651098
2778.306268	330099.503116	39.656116
2781.005994	330772.101016	39.661133
2784.169641	331433.655471	39.666151
2787.394287	332097.345453	39.671168
2790.089974	332760.954047	39.676186
2793.556760	333404.593205	39.681204
2796.280744	334059.498803	39.686221
2799.466385	334702.753691	39.691239
2802.140120	335356.858079	39.696256
2804.764501	336003.932157	39.701274
2807.661913	336657.547563	39.706292
2810.271856	337321.519825	39.711309
2812.583383	337972.615667	39.716327
2815.260397	338617.961299	39.721344
2817.938794	339284.043017	39.726362
2820.670778	339944.524037	39.731380
2823.437940	340616.273961	39.736397
2826.024167	341278.705857	39.741415
2828.696516	341932.057605	39.746432
2831.473642	342576.326735	39.751450
2833.834715	343224.326090	39.756468
2836.312686	343878.026685	39.761485
2838.836068	344531.200616	39.766503
2841.689126	345174.876950	39.771520
2844.141247	345839.727857	39.776538
2846.792506	346484.628054	39.781556
2849.971748	347159.838420	39.786573
2852.912428	347832.511176	39.791591
2855.600289	348500.772178	39.796608
2858.217513	349178.514156	39.801626
2861.351953	349844.827465	39.806644
2863.898470	350530.539824	39.811661
2866.556043	351222.407165	39.816679
2869.563797	351912.455788	39.821696
2872.146456	352618.097886	39.826714
2875.352926	353321.320217	39.831732
2878.311363	354030.472896	39.836749
2881.210469	354732.570981	39.841767
2884.130064	355435.436164	39.846784
2887.148168	356152.238839	39.851802
2890.422978	356854.687300	39.856820
2893.415422	357577.900213	39.861837
2896.418170	358284.946922	39.866855
2900.011755	358991.479818	39.871872
2902.532827	359707.516811	39.876890
2905.681546	360411.044192	39.881908
2908.575453	361123.567744	39.886925
2911.866542	361837.634773	39.891943
2914.907198	362558.009512	39.896960
2917.315982	363278.617197	39.901978
2920.922130	363999.046342	39.906996
2923.376436	364710.361140	39.912013
2926.836437	365429.105198	39.917031
2929.842054	366140.223329	39.922048
2932.369668	366869.213978	39.927066
2935.541451	367596.236006	39.932084
2938.315693	368316.459400	39.937101
2941.236402	369038.947780	39.942119
2944.348536	369775.350122	39.947136
2947.160488	370498.553009	39.952154
2950.316904	371238.609676	39.957172
2953.214582	371969.362741	39.962189
2956.285543	372696.522449	39.967207
2959.404577	373432.675289	39.972224
2962.382321	374161.584423	39.977242
2965.879632	374880.132631	39.982260
2969.019207	375614.602165	39.987277
2972.355982	376328.070204	39.992295
2976.312806	377029.085725	39.997312
2979.368984	377749.272984	40.002330
2982.396525	378457.387440	40.007348
2985.213986	379164.705144	40.012365
2987.931231	379868.523969	40.017383
2991.048516	380576.289148	40.022400
2993.763764	381289.492847	40.027418
2996.615313	382001.060175	40.032436
2999.616073	382715.573447	40.037453
3002.240888	383435.393459	40.042471
3005.571169	384142.243233	40.047488
3008.499703	384859.114236	40.052506
3011.266432	385568.012997	40.057524
3014.359542	386290.212244	40.062541
3017.058028	387021.163464	40.067559
3019.912562	387741.408396	40.072576
3022.764272	388471.736451	40.077594
3025.617877	389207.917301	40.082612
3028.535879	389929.152652	40.087629
3031.281160	390618.187344	40.092647
3034.964102	391317.235013	40.097664
3037.481965	392006.266140	40.102682
3040.234825	392696.051399	40.107700
3043.389793	393408.438265	40.112717
3046.028655	394114.504845	40.117735
3049.385488	394819.375765	40.122752
3052.082927	395546.554665	40.127770
3055.383869	396261.821339	40.132788
3058.461209	396978.012556	40.137805
3061.409208	397713.287587	40.142823
3064.307319	398436.398005	40.147840
3066.951290	399168.485637	40.152858
3069.896064	399913.968324	40.157876
3072.829422	400658.062225	40.162893
3075.297055	401424.323997	40.167911
3078.216658	402179.607865	40.172928
3080.543170	402958.139878	40.177946
3083.438205	403750.576190	40.182964
3086.318041	404546.580543	40.187981
3089.382855	405350.574743	40.192999
3091.978938	406163.570433	40.198016
3095.431828	406986.422916	40.203034
3098.052619	407805.781847	40.208052
3101.335064	408625.766643	40.213069
3104.780221	409455.764796	40.218087
3107.829487	410292.370815	40.223104
3110.690942	411119.867179	40.228122
3114.243579	411955.926533	40.233140
3118.023962	412803.149369	40.238157
3121.687808	413634.270031	40.243175
3125.557155	414451.567101	40.248192
3128.909648	415297.544331	40.253210
3132.744199	416115.238518	40.258228
3135.898480	416923.497929	40.263245
3138.957103	417746.813825	40.268263
3142.111706	418559.866109	40.273280
3145.291972	419384.262221	40.278298
3148.351739	420204.750443	40.283316
3151.681439	421030.271943	40.288333
3154.822406	421862.363841	40.293351
3158.239561	422695.693916	40.298368
3160.888792	423521.777787	40.303386
3164.014999	424354.175508	40.308404
3167.279541	425183.736833	40.313421
3170.429312	426025.719441	40.318439
3173.426092	426866.174038	40.323456
3176.594652	427696.000922	40.328474
3180.140974	428542.972877	40.333492
3183.014094	429377.325545	40.338509
3186.337037	430219.408045	40.343527
3189.600253	431058.532297	40.348544
3192.969350	431897.199934	40.353562
3196.801506	432731.109806	40.358580
3200.568562	433558.929453	40.363597
3203.896532	434389.005783	40.368615
3207.074155	435200.927873	40.373632
3210.704223	436025.024820	40.378650
3213.536772	436842.439389	40.383668
3216.903221	437662.969756	40.388685
3219.780951	438488.441866	40.393703
3223.163155	439305.513612	40.398720
3226.353966	440126.520511	40.403738
3229.094150	440964.889953	40.408756
3232.630988	441777.283553	40.413773
3235.166870	442612.428368	40.418791
3238.367926	443442.936535	40.423808
3241.935864	444271.734039	40.428826
3244.374057	445089.558275	40.433844
3247.513084	445888.852833	40.438861
3249.896636	446692.674418	40.443879
3252.712646	447497.504343	40.448896
3255.595135	448327.689525	40.453914
3258.989502	449141.799900	40.458932
3262.247743	449977.910469	40.463949
3265.145662	450827.974122	40.468967
3267.878045	451674.488871	40.473984
3271.201919	452537.027435	40.479002
3274.207291	453404.622188	40.484020
3277.559853	454264.800389	40.489037
3280.117146	455148.886997	40.494055
3283.740635	456026.503955	40.499072
3286.947137	456914.842457	40.504090
3290.109311	457809.350658	40.509108
3293.998414	458704.809952	40.514125
3297.015852	459615.145355	40.519143
3300.443797	460525.419193	40.524160
3303.384176	461435.316864	40.529178
3306.619794	462348.753157	40.534196
3310.167034	463272.990467	40.539213
3313.734003	464210.090380	40.544231
3317.115160	465143.282433	40.549248
3320.394252	466073.764787	40.554266
3323.373639	467011.556580	40.559284
3326.910813	467940.078751	40.564301
3330.152317	468893.058122	40.569319
3333.441278	469852.128428	40.574336
3336.936403	470802.537081	40.579354
3340.435683	471762.169238	40.584372
3344.172542	472714.698591	40.589389
3347.816159	473671.220647	40.594407
3351.302409	474612.987567	40.599424
3355.074720	475570.738606	40.604442
3358.541421	476523.186473	40.609460
3362.506449	477461.132485	40.614477
3366.148187	478408.248224	40.619495
3369.436332	479345.079525	40.624512
3373.383973	480292.186339	40.629530
3376.664992	481235.711120	40.634548
3380.325284	482163.698470	40.639565
3383.719079	483101.146465	40.644583
3387.469845	484035.509412	40.649600
3390.796536	484976.079930	40.654618
3393.619051	485917.729814	40.659636
3397.091561	486847.028437	40.664653
3400.577978	487794.757930	40.669671
3403.900169	488737.870005	40.674688
3407.869892	489664.955367	40.679706
3410.800602	490603.932420	40.684724
3414.477868	491536.791709	40.689741
3417.873882	492488.523490	40.694759
3421.324187	493432.733116	40.699776
3424.590621	494375.904611	40.704794
3427.549879	495328.832969	40.709812
3431.104264	496274.961237	40.714829
3434.426743	497221.266484	40.719847
3438.250295	498179.264006	40.724864
3442.148919	499123.897245	40.729882
3445.061549	500068.874628	40.734900
3449.127161	501007.017503	40.739917
3452.561294	501958.686929	40.744935
3455.615507	502894.096889	40.749952
3459.150290	503838.782208	40.754970
3462.372035	504785.718638	40.759988
3466.545221	505735.765434	40.765005
3469.732769	506668.974509	40.770010
3473.041010	507562.546913	40.775015
3476.098074	508405.412422	40.780020
3479.738358	509193.566616	40.785024
3482.753121	509924.937161	40.790029
3486.186166	510608.649448	40.795034
3488.666282	511227.173271	40.800039
3491.543913	511790.694712	40.805044
3494.120132	512301.799884	40.810048
3496.593957	512758.597938	40.815053
3498.594219	513177.387328	40.820058
3500.590482	513528.300738	40.825063
3502.949611	513839.419481	40.830068
3504.826168	514100.844797	40.835072
3506.399133	514319.357843	40.840077
3508.071142	514512.593860	40.845082
3509.078022	514633.736450	40.850087
3510.727877	514739.552688	40.855092
3511.585014	514818.116467	40.860096
3512.522882	514862.637654	40.865101
3514.078996	514887.199324	40.870106
3514.422301	514879.029246	40.875111
3515.097035	514835.467174	40.880116
3515.880070	514789.115313	40.885120
3516.507823	514705.127636	40.890125
3516.906911	514612.453212	40.895130
3517.310164	514503.594134	40.900135
3517.896549	514381.042972	40.905140
3518.205324	514239.476493	40.910144
3518.747374	514096.511007	40.915149
3518.886867	513930.465009	40.920154
3518.868272	513751.584964	40.925159
3519.203025	513561.555454	40.930164
3519.115475	513370.479827	40.935168
3519.739174	513172.433720	40.940173
3519.577135	512975.868435	40.945178
3519.248164	512764.956121	40.950183
3519.719828	512544.587831	40.955188
3519.392401	512339.316168	40.960192
3519.420391	512107.412619	40.965197
3519.434402	511885.138581	40.970202
3519.644627	511664.897933	40.975207
3519.829688	511420.805907	40.980212
3519.273536	511196.491721	40.985216
3519.845901	510951.877402	40.990221
3519.276791	510713.336672	40.995226
3519.171852	510475.879544	41.000231
3519.187114	510228.414357	41.005236
3518.985652	509995.502920	41.010240
3518.918011	509751.522036	41.015245
3518.864675	509505.113885	41.020250
3518.770616	509265.970326	41.025255
3518.608398	509011.299231	41.030260
3518.613786	508774.855383	41.035264
3518.849020	508523.795491	41.040269
3518.762361	508287.307375	41.045274
3518.046501	508045.566704	41.050279
3518.120794	507791.744736	41.055284
3517.906882	507544.469914	41.060288
3517.657454	507309.756233	41.065293
3517.666744	507080.345293	41.070298
3517.105562	506839.064412	41.075303
3516.876363	506606.656356	41.080308
3516.814027	506378.254120	41.085312
3516.708663	506137.293973	41.090317
3516.903975	505909.348590	41.095322
3516.348816	505691.807578	41.100327
3516.518250	505465.877033	41.105332
3516.317071	505239.395206	41.110336
3515.959624	505010.411635	41.115341
3515.853328	504799.244742	41.120346
3515.353053	504568.813279	41.125351
3515.707021	504342.079530	41.130356
3515.072899	504139.360079	41.135360
3514.906044	503914.920551	41.140365
3515.152551	503721.593865	41.145370
3514.830616	503509.735215	41.150375
3514.873036	503296.101261	41.155380
3514.849431	503090.597885	41.160384
3514.404847	502880.565501	41.165389
3514.416594	502672.426904	41.170394
3513.864282	502485.868387	41.175399
3514.139442	502274.504190	41.180404
3513.640383	502083.542249	41.185408
3513.436936	501887.788501	41.190413
3513.428548	501689.377774	41.195418
3513.399802	501499.394634	41.200423
3513.554925	501303.829518	41.205428
3512.981504	501117.609905	41.210432
3513.002224	500933.414930	41.215437
3512.884769	500748.936339	41.220442
3512.694377	500571.582336	41.225447
3512.746063	500382.177665	41.230452
3512.389969	500208.983224	41.235456
3512.348195	500031.094855	41.240461
3512.232483	499848.370938	41.245466
3512.190283	499671.336202	41.250471
3512.182705	499496.615499	41.255476
3511.916899	499339.193415	41.260480
3511.658502	499156.483055	41.265485
3512.018295	498985.282448	41.270490
3511.500218	498814.923047	41.275495
3511.613059	498643.706410	41.280500
3511.327588	498488.095225	41.285504
3511.075723	498315.013561	41.290509
3511.157305	498159.190354	41.295514
3510.535126	498000.698943	41.300519
3510.692336	497836.734244	41.305524
3510.403763	497689.948126	41.310528
3510.134214	497537.403374	41.315533
3510.090232	497381.389570	41.320538
3509.775590	497241.366829	41.325543
3510.085586	497096.450240	41.330548
3509.743578	496952.693717	41.335552
3509.342928	496818.889085	41.340557
3509.242319	496674.032247	41.345562
3509.222140	496542.841269	41.350567
3509.675760	496402.135753	41.355572
3509.168348	496269.806668	41.360576
3509.004016	496119.754894	41.365581
3509.259935	495993.109794	41.370586
3508.797903	495869.503246	41.375591
3509.015016	495740.186521	41.380596
3508.712141	495618.521898	41.385600
3508.806500	495487.758096	41.390605
3508.690067	495364.951768	41.395610
3508.773443	495228.230404	41.400615
3508.801713	495103.985867	41.405620
3508.437717	494978.034386	41.410624
3508.581332	494856.092106	41.415629
3508.362148	494735.467410	41.420634
3508.385523	494608.796219	41.425639
3508.099853	494484.140994	41.430644
3507.845182	494370.788839	41.435648
3507.870517	494254.161102	41.440653
3507.868185	494131.781229	41.445658
3507.383886	494032.649111	41.450663
3507.712414	493910.872279	41.455668
3507.562577	493798.155804	41.460672
3507.621952	493691.111138	41.465677
3507.661234	493581.493894	41.470682
3507.220710	493468.113321	41.475687
3507.248168	493365.564845	41.480692
3507.419623	493260.367776	41.485696
3507.626578	493152.236000	41.490701
3507.342250	493039.736705	41.495706
3507.310777	492937.244959	41.500711
3507.316084	492828.384861	41.505716
3506.946729	492716.653746	41.510720
3507.086203	492614.335161	41.515725
3507.039542	492512.549770	41.520730
3507.082178	492413.678383	41.525735
3507.204989	492310.653424	41.530740
3507.027358	492209.896229	41.535744
3506.828622	492105.102129	41.540749
3506.729122	492010.390712	41.545754
3506.505358	491898.933828	41.550759
3506.513423	491800.265768	41.555764
3506.493758	491722.152948	41.560768
3506.334739	491618.207698	41.565773
3506.276125	491538.585121	41.570778
3506.222097	491445.428447	41.575783
3506.205026	491345.549417	41.580788
3506.178452	491248.095051	41.585792
3506.059156	491167.672011	41.590797
3506.063996	491072.837474	41.595802
3505.596323	490983.226637	41.600807
3505.744570	490892.155977	41.605812
3505.697444	490813.992233	41.610816
3505.635032	490734.113515	41.615821
3505.904963	490651.859713	41.620826
3505.677443	490569.733374	41.625831
3505.896875	490482.891096	41.630836
3505.733343	490397.572405	41.635840
3505.837189	490309.787629	41.640845
3505.754130	490234.555483	41.645850
3505.525252	490146.417535	41.650855
3505.855245	490060.969651	41.655860
3505.630153	489983.586828	41.660864
3505.431175	489910.694161	41.665869
3505.713013	489824.696926	41.670874
3505.375530	489747.835406	41.675879
3505.575189	489659.526942	41.680884
3505.226891	489587.716504	41.685888
3505.246460	489510.545709	41.690893
3505.306699	489428.822937	41.695898
3505.258039	489357.217297	41.700903
3505.409135	489271.792815	41.705908
3505.130989	489194.060703	41.710912
3505.153334	489123.553995	41.715917
3505.403942	489047.658002	41.720922
3505.041545	488968.271210	41.725927
3505.020606	488899.689368	41.730932
3504.916056	488816.827348	41.735936
3505.051025	488752.311479	41.740941
3505.215683	488677.285605	41.745946
3505.105185	488604.574932	41.750951
3505.015287	488536.911290	41.755956
3505.248683	488452.681552	41.760960
3504.881460	488385.565456	41.765965
3504.703512	488309.884001	41.770970
3504.634847	488246.003759	41.775975
3505.297322	488165.746213	41.780980
3504.997056	488091.244372	41.785984
3504.980471	488024.425676	41.790989
3505.054528	487946.480876	41.795994
3505.000821	487884.970663	41.800999
3505.011430	487803.903515	41.806004
3504.703414	487738.795694	41.811008
3504.485790	487666.551805	41.816013
3504.768728	487592.310341	41.821018
3504.553652	487536.783895	41.826023
3504.837817	487461.834481	41.831028
3504.649161	487388.372546	41.836032
3504.432365	487323.198254	41.841037
3504.360364	487259.011353	41.846042
3504.597627	487186.239823	41.851047
3504.594602	487126.335007	41.856052
3504.609182	487060.012361	41.861056
3504.266003	486994.553274	41.866061
3504.162647	486944.209921	41.871066
3504.023416	486875.738436	41.876071
3504.128769	486811.117974	41.881076
3504.579338	486749.777294	41.886080
3504.347388	486695.715269	41.891085
3504.668165	486625.201122	41.896090
3503.957217	486560.555097	41.901095
3503.989919	486506.855324	41.906100
3503.901936	486456.305930	41.911104
3503.992905	486393.403382	41.916109
3503.859064	486334.223017	41.921114
3503.975663	486273.286001	41.926119
3504.046175	486219.882422	41.931124
3503.651585	486160.388370	41.936128
3503.840749	486100.045541	41.941133
3504.080831	486048.686050	41.946138
3503.977987	485994.702500	41.951143
3504.195285	485934.809274	41.956148
3504.009380	485880.282590	41.961152
3503.846193	485823.074896	41.966157
3504.000038	485759.200197	41.971162
3503.707889	485712.973906	41.976167
3503.834505	485649.456596	41.981172
3503.776412	485594.100766	41.986176
3503.650829	485530.622212	41.991181
3504.015548	485476.058931	41.996186
3503.769683	485430.632847	42.001191
3504.031750	485374.569702	42.006196
3503.857473	485326.454811	42.011200
3503.500801	485274.023730	42.016205
3503.562014	485213.040631	42.021210
3503.483914	485165.415441	42.026215
3503.809928	485104.491742	42.031220
3503.934673	485060.421377	42.036224
3503.359759	485004.689205	42.041229
3503.898939	484957.219904	42.046234
3503.508030	484911.309688	42.051239
3503.580290	484848.302724	42.056244
3503.856071	484799.712017	42.061248
3503.489324	484742.127853	42.066253
3503.800281	484688.631050	42.071258
3503.473297	484641.396606	42.076263
3503.192281	484584.253182	42.081268
3503.467550	484535.813284	42.086272
3503.347552	484489.960699	42.091277
3503.656190	484448.082819	42.096282
3503.623846	484396.204526	42.101287
3503.793104	484333.786610	42.106292
3503.732688	484289.187151	42.111296
3503.550454	484234.300455	42.116301
3503.725289	484179.054880	42.121306
3503.363230	484133.036828	42.126311
3503.859735	484080.165818	42.131316
3503.671719	484021.136592	42.136320
3503.403134	483971.415508	42.141325
3503.782175	483923.109115	42.146330
3503.413331	483875.828333	42.151335
3503.620753	483822.597264	42.156340
3503.664191	483778.839041	42.161344
3503.369507	483726.342556	42.166349
3503.280791	483666.791315	42.171354
3503.624641	483627.785489	42.176359
3503.532916	483570.760445	42.181364
3503.352542	483523.499784	42.186368
3503.413266	483474.837357	42.191373
3503.724093	483424.216002	42.196378
3503.201627	483369.177106	42.201383
3503.245194	483319.051702	42.206388
3503.339295	483271.697043	42.211392
3503.001108	483232.038514	42.216397
3503.284300	483179.096596	42.221402
3503.156833	483149.055026	42.226407
3503.074863	483095.209701	42.231412
3503.331135	483052.477315	42.236416
3503.211951	482998.890067	42.241421
3503.123070	482957.120561	42.246426
3503.016585	482925.256427	42.251431
3503.190378	482871.218957	42.256436
3503.005676	482828.251432	42.261440
3502.958467	482785.161344	42.266445
3503.281342	482735.748473	42.271450
3503.036925	482700.520182	42.276455
3502.787937	482645.638273	42.281460
3503.010166	482608.164579	42.286464
3503.056237	482566.120401	42.291469
3503.278159	482531.880194	42.296474
3502.925975	482484.441018	42.301479
3503.220892	482443.823031	42.306484
3503.195916	482398.151603	42.311488
3503.173445	482354.450167	42.316493
3503.398712	482298.684824	42.321498
3503.111621	482267.655873	42.326503
3503.173729	482215.351411	42.331508
3503.367899	482173.788398	42.336512
3503.064005	482130.989083	42.341517
3502.932967	482077.552102	42.346522
3503.020873	482032.114675	42.351527
3503.251874	481984.077960	42.356532
3503.066985	481943.230175	42.361536
3502.975307	481904.439407	42.366541
3503.062646	481861.881641	42.371546
3503.016162	481822.578361	42.376551
3503.018822	481779.225104	42.381556
3502.860074	481736.705292	42.386560
3502.876662	481698.655087	42.391565
3502.984476	481655.285125	42.396570
3503.027568	481609.600806	42.401575
3502.948515	481563.884833	42.406580
3502.899655	481516.243936	42.411584
3503.179914	481475.272020	42.416589
3503.021224	481433.509311	42.421594
3502.898577	481389.467071	42.426599
3503.025276	481348.468192	42.431604
3502.981681	481307.748353	42.436608
3502.954555	481268.996498	42.441613
3503.172953	481220.858351	42.446618
3502.919225	481185.931279	42.451623
3503.071118	481137.297927	42.456628
3502.784058	481090.501285	42.461632
3502.943056	481057.328786	42.466637
3503.076042	481019.460944	42.471642
3502.815781	480973.165086	42.476647
3502.865311	480926.820884	42.481652
3502.729109	480885.457464	42.486656
3502.507659	480855.779834	42.491661
3502.716715	480801.022313	42.496666
3502.987359	480777.533807	42.501671
3502.936122	480727.667521	42.506676
3502.844714	480693.573128	42.511680
3502.715294	480646.497977	42.516685
3502.914662	480603.262462	42.521690
3502.778007	480566.294528	42.526695
3502.769633	480519.705480	42.531700
3502.632964	480490.620352	42.536704
3502.457492	480458.863005	42.541709
3502.752563	480408.335434	42.546714
3502.788842	480367.550201	42.551719
3502.615045	480346.404173	42.556724
3502.370560	480305.207676	42.561728
3502.380602	480273.269490	42.566733
3502.792828	480234.497253	42.571738
3502.687835	480196.159137	42.576743
3502.455886	480159.558809	42.581748
3502.518743	480130.189302	42.586752
3502.409876	480095.237267	42.591757
3502.693009	480047.641331	42.596762
3502.465149	480005.481329	42.601767
3502.609349	479983.577860	42.606772
3502.544316	479948.214409	42.611776
3502.621057	479912.020276	42.616781
3502.696016	479881.132405	42.621786
3502.524873	479841.590907	42.626791
3502.733910	479810.429364	42.631796
3502.693096	479773.747865	42.636800
3502.510927	479738.806448	42.641805
3502.989963	479703.408320	42.646810
3502.892923	479657.891753	42.651815
3502.723853	479617.692421	42.656820
3502.765978	479579.178310	42.661824
3502.937828	479538.622516	42.666829
3502.896750	479491.125892	42.671834
3502.691136	479448.101843	42.676839
3502.802397	479411.800123	42.681844
3502.835761	479368.991347	42.686848
3502.535820	479338.362900	42.691853
3502.525301	479299.553087	42.696858
3502.577647	479265.028952	42.701863
3502.577512	479228.137714	42.706868
3502.978129	479188.151858	42.711872
3502.377604	479153.122640	42.716877
3502.407323	479116.731860	42.721882
3502.513282	479088.414977	42.726887
3502.291551	479058.430792	42.731892
3502.615322	479015.070504	42.736896
3502.441530	478987.807709	42.741901
3502.576137	478937.098265	42.746906
3502.922687	478908.389863	42.751911
3502.781938	478859.542355	42.756916
3502.845034	478824.459679	42.761920
3502.723429	478794.914251	42.766925
3502.840655	478750.170332	42.771930
3502.821007	478712.169104	42.776935
3503.019331	478663.167153	42.781940
3502.377227	478634.511027	42.786945
3502.653830	478601.719381	42.791949
3502.697741	478555.268028	42.796954
3502.212028	478520.977619	42.801959
3502.239961	478489.033050	42.806964
3502.496710	478461.045353	42.811969
3502.500345	478436.685234	42.816973
3502.601511	478392.650349	42.821978
3502.712124	478348.917104	42.826983
3502.577617	478313.762973	42.831988
3502.787900	478280.980987	42.836993
3502.225361	478255.495757	42.841997
3502.571276	478207.985611	42.847002
3502.663250	478170.117335	42.852007
3502.386175	478135.642008	42.857012
3502.444477	478097.930419	42.862017
3502.814485	478065.931769	42.867021
3502.575659	478029.125430	42.872026
3502.033452	477990.900555	42.877031
3502.214289	477963.782978	42.882036
3502.657922	477933.743670	42.887041
3502.528906	477901.569644	42.892045
3502.641770	477856.823892	42.897050
3502.518300	477824.901551	42.902055
3502.278299	477788.701325	42.907060
3502.628285	477766.206829	42.912065
3502.532924	477721.695263	42.917069
3502.313179	477689.484386	42.922074
3502.057645	477645.957812	42.927079
3502.292192	477614.383666	42.932084
3502.088532	477577.924600	42.937089
3502.433508	477551.488358	42.942093
3502.633186	477518.099957	42.947098
3502.266555	477489.095647	42.952103
3502.272978	477446.942931	42.957108
3502.827342	477417.946799	42.962113
3502.394274	477383.948995	42.967117
3502.612115	477352.629641	42.972122
3502.432423	477318.844980	42.977127
3502.286348	477274.542227	42.982132
3502.345518	477239.456671	42.987137
3502.329460	477223.942679	42.992141
3502.345119	477174.661321	42.997146
3502.286912	477151.825141	43.002151
3502.361634	477123.155826	43.007156
3502.459177	477091.601967	43.012161
3502.359391	477048.959299	43.017165
3502.632969	477006.511134	43.022170
3502.111433	476979.299011	43.027175
3501.998311	476951.113507	43.032180
3502.329576	476920.685437	43.037185
3501.799606	476894.636980	43.042189
3502.230556	476870.763953	43.047194
3502.221040	476831.695250	43.052199
3502.249807	476794.591703	43.057204
3502.163974	476773.781033	43.062209
3502.209726	476739.353538	43.067213
3502.332561	476719.167397	43.072218
3502.488145	476682.347119	43.077223
3502.135236	476648.587996	43.082228
3502.283368	476620.563434	43.087233
3502.073814	476595.020615	43.092237
3502.341740	476555.149898	43.097242
3502.227120	476529.086755	43.102247
3502.406525	476492.616147	43.107252
3502.689227	476465.075820	43.112257
3502.080950	476428.980364	43.117261
3502.347720	476392.293754	43.122266
3502.467535	476363.312792	43.127271
3502.364975	476336.691463	43.132276
3502.181898	476293.099384	43.137281
3502.203432	476276.567715	43.142285
3502.489385	476234.671580	43.147290
3502.528595	476203.731596	43.152295
3502.312557	476169.343616	43.157300
3502.484056	476125.999180	43.162305
3502.257367	476101.570251	43.167309
3502.507684	476068.120402	43.172314
3502.363969	476036.551462	43.177319
3502.121655	475996.253295	43.182324
3502.319020	475962.255457	43.187329
3502.017854	475938.444425	43.192333
3502.488734	475907.133418	43.197338
3502.366407	475863.328531	43.202343
3502.170803	475836.063743	43.207348
3502.256959	475805.469514	43.212353
3502.257721	475771.148037	43.217357
3502.447408	475749.888788	43.222362
3502.293169	475714.934199	43.227367
3502.265700	475687.339711	43.232372
3502.729928	475655.372135	43.237377
3502.083523	475620.493928	43.242381
3502.698620	475582.588673	43.247386
3502.353024	475555.144559	43.252391
3502.149735	475519.691701	43.257396
3501.967027	475493.688020	43.262401
3502.318914	475468.258231	43.267405
3502.392333	475433.469795	43.272410
3502.265856	475400.582674	43.277415
3502.155503	475365.115013	43.282420
3502.316805	475330.818163	43.287425
3502.186675	475303.491735	43.292429
3502.324917	475270.815897	43.297434
3502.371827	475233.200433	43.302439
3502.272548	475202.633915	43.307444
3502.531253	475175.095115	43.312449
3502.090135	475144.986072	43.317453
3502.415289	475104.091874	43.322458
3502.365565	475086.104147	43.327463
3502.267917	475054.020618	43.332468
3502.646595	475021.256310	43.337473
3502.276300	474992.601894	43.342477
3502.521485	474945.856000	43.347482
3502.367708	474923.941414	43.352487
3502.219144	474892.472083	43.357492
3502.408572	474854.277510	43.362497
3502.361125	474818.647208	43.367501
3502.450810	474786.230695	43.372506
3502.471404	474754.128170	43.377511
3502.048520	474728.565029	43.382516
3502.510166	474691.288166	43.387521
3502.205438	474658.022864	43.392525
3502.389931	474628.826514	43.397530
3502.274461	474588.757836	43.402535
3502.081925	474556.233126	43.407540
3502.434160	474529.234730	43.412545
3502.255098	474496.808906	43.417549
3502.490630	474456.280871	43.422554
3502.303240	474422.188005	43.427559
3502.185794	474388.690799	43.432564
3502.107441	474359.029351	43.437569
3502.287401	474334.534458	43.442573
3502.437987	474301.601981	43.447578
3502.158840	474273.892584	43.452583
3502.003012	474242.119805	43.457588
3502.535924	474210.644202	43.462593
3501.904087	474177.176052	43.467597
3501.833654	474136.037651	43.472602
3502.219852	474110.044314	43.477607
3501.995978	474080.859970	43.482612
3501.920427	474051.703045	43.487617
3502.284147	474033.144284	43.492621
3502.095621	474001.325568	43.497626
3502.243672	473972.588678	43.502631
3502.127391	473940.253073	43.507636
3502.311989	473904.736306	43.512641
3501.998191	473876.526091	43.517645
3502.271977	473847.617754	43.522650
3502.148550	473817.355690	43.527655
3501.824396	473794.151703	43.532660
3501.878576	473763.811348	43.537665
3502.122433	473734.553594	43.542669
3502.141695	473705.987933	43.547674
3501.881434	473687.626984	43.552679
3502.206487	473670.489325	43.557684
3502.715911	473624.911784	43.562689
3502.200813	473596.176314	43.567693
3502.322779	473562.892913	43.572698
3502.539170	473523.123832	43.577703
3502.435861	473498.873974	43.582708
3502.484821	473457.159176	43.587713
3502.324517	473427.357111	43.592717
3502.525303	473387.387909	43.597722
3502.390464	473361.626118	43.602727
3502.105961	473328.051605	43.607732
3502.197493	473295.429602	43.612737
3502.336287	473264.266270	43.617741
3502.279312	473227.622852	43.622746
3502.263056	473199.415711	43.627751
3502.213744	473177.988054	43.632756
3502.358465	473133.224214	43.637761
3502.115028	473106.518367	43.642765
3502.173274	473074.153876	43.647770
3502.263422	473045.171579	43.652775
3502.215783	473014.289557	43.657780
3502.661585	472986.010144	43.662785
3502.393886	472958.094491	43.667789
3502.099271	472921.184026	43.672794
3502.242523	472888.957607	43.677799
3501.613421	472853.514607	43.682804
3502.178660	472830.676401	43.687809
3502.103471	472805.157226	43.692813
3502.337735	472769.781919	43.697818
3502.348877	472733.025673	43.702823
3502.282065	472702.095485	43.707828
3502.834104	472661.159822	43.712833
3502.037361	472626.804105	43.717837
3502.190402	472595.940618	43.722842
3502.467952	472569.102259	43.727847
3501.876546	472542.904647	43.732852
3502.190363	472506.353575	43.737857
3502.104634	472481.846677	43.742861
3502.125671	472440.133616	43.747866
3502.184697	472415.806323	43.752871
3501.939188	472389.756868	43.757876
3502.173169	472361.054316	43.762881
3502.191579	472335.064820	43.767885
3502.265439	472307.246572	43.772890
3502.351330	472268.455334	43.777895
3502.429012	472250.444633	43.782900
3502.264724	472212.905586	43.787905
3501.716798	472183.515466	43.792909
3501.977304	472149.752593	43.797914
3501.932138	472120.031332	43.802919
3501.915987	472098.597094	43.807924
3502.243073	472072.154677	43.812929
3502.021930	472050.600599	43.817933
3502.074595	471999.730377	43.822938
3502.226308	471969.775970	43.827943
3501.986596	471936.494968	43.832948
3502.077441	471907.864453	43.837953
3502.209366	471894.799707	43.842957
3502.019879	471854.432445	43.847962
3502.160868	471824.985034	43.852967
3501.908120	471798.581846	43.857972
3502.239886	471773.250525	43.862977
3501.902017	471741.703423	43.867981
3501.811520	471711.027839	43.872986
3502.028681	471684.551343	43.877991
3501.971313	471660.038797	43.882996
3502.151982	471634.124056	43.888001
3502.086450	471605.871266	43.893005
3501.944544	471582.029038	43.898010
3502.111433	471549.644617	43.903015
3502.297213	471527.470364	43.908020
3502.320984	471490.759916	43.913025
3502.124913	471468.796686	43.918029
3502.252400	471432.322769	43.923034
3502.424246	471393.516078	43.928039
3501.942678	471362.293968	43.933044
3502.153775	471334.857196	43.938049
3502.067369	471302.107214	43.943053
3502.055246	471280.469033	43.948058
3502.183955	471249.404545	43.953063
3502.126850	471215.638609	43.958068
3501.991250	471190.530799	43.963073
3502.019455	471159.785150	43.968077
3502.198599	471129.066515	43.973082
3502.126230	471092.673504	43.978087
3501.607108	471080.720652	43.983092
3501.844091	471048.627703	43.988097
3501.708983	471017.300459	43.993101
3501.947391	470993.701564	43.998106
3501.832275	470979.107113	44.003111
3501.854171	470955.744103	44.008116
3502.376403	470923.808770	44.013121
3502.207713	470901.183209	44.018125
3502.017104	470868.296889	44.023130
3502.210477	470842.277795	44.028135
3502.095185	470804.475078	44.033140
3502.133748	470772.210215	44.038145
3502.034673	470754.326500	44.043149
3501.866867	470726.442047	44.048154
3502.158163	470694.795019	44.053159
3502.170529	470666.932990	44.058164
3502.485156	470621.781893	44.063169
3502.261693	470598.759934	44.068173
3502.305017	470561.336479	44.073178
3502.446657	470529.712422	44.078183
3502.084611	470504.638800	44.083188
3502.463285	470481.472413	44.088193
3502.243019	470443.331255	44.093197
3502.050316	470401.545132	44.098202
3502.175776	470375.232485	44.103207
3502.253224	470353.326324	44.108212
3502.239504	470310.450276	44.113217
3501.965474	470289.963952	44.118221
3501.984568	470259.116906	44.123226
3501.934737	470226.510778	44.128231
3502.041449	470198.431017	44.133236
3501.766823	470170.410549	44.138241
3501.939679	470153.141201	44.143245
3502.030093	470118.389327	44.148250
3502.282332	470097.669176	44.153255
3501.752020	470058.361819	44.158260
3502.106948	470027.714903	44.163265
3502.016821	470012.003276	44.168269
3502.054264	469970.635329	44.173274
3502.287089	469945.114328	44.178279
3502.381876	469925.176938	44.183284
3502.325753	469888.576471	44.188289
3502.118042	469861.101281	44.193293
3501.994646	469827.292241	44.198298
3502.233167	469798.230543	44.203303
3502.132119	469773.823109	44.208308
3501.983999	469742.343761	44.213313
3502.034488	469708.911946	44.218317
3502.303445	469682.676995	44.223322
3502.083232	469647.921900	44.228327
3501.852239	469623.382766	44.233332
3501.921249	469585.194603	44.238337
3502.058301	469564.491708	44.243341
3501.698648	469543.360416	44.248346
3501.954199	469516.014826	44.253351
3501.712963	469494.511080	44.258356
3501.810340	469457.177837	44.263361
3501.859966	469442.050719	44.268365
3501.719656	469415.019396	44.273370
3502.010619	469393.634968	44.278375
3501.550271	469360.989876	44.283380
3501.645875	469343.782269	44.288385
3501.614207	469323.712130	44.293389
3501.781264	469306.695634	44.298394
3501.996212	469272.428270	44.303399
3501.666691	469254.730487	44.308404
3502.058457	469218.463373	44.313409
3502.005962	469203.402495	44.318413
3501.658125	469166.491848	44.323418
3502.217109	469141.323391	44.328423
3502.046713	469120.364376	44.333428
3502.012502	469082.696791	44.338433
3501.880034	469060.922714	44.343437
3501.978621	469034.258136	44.348442
3502.141029	469009.960278	44.353447
3501.780130	468979.979059	44.358452
3501.889631	468954.172310	44.363457
3501.966888	468920.431325	44.368461
3501.729990	468895.487480	44.373466
3502.064414	468882.287697	44.378471
3501.862820	468859.158765	44.383476
3501.620761	468823.596239	44.388481
3501.662924	468798.962804	44.393485
3502.001440	468790.667467	44.398490
3502.010051	468754.610667	44.403495
3501.965338	468730.091786	44.408500
3502.067271	468704.589239	44.413505
3501.730065	468671.721345	44.418509
3501.628740	468647.868548	44.423514
3501.777483	468618.616472	44.428519
3501.548536	468606.566089	44.433524
3501.781119	468572.800225	44.438529
3501.984984	468549.354919	44.443533
3501.761019	468530.830823	44.448538
3502.136946	468497.447055	44.453543
3501.872391	468473.720547	44.458548
3501.795492	468445.514670	44.463553
3501.698619	468416.249888	44.468557
3501.544804	468395.287374	44.473562
3501.304455	468368.522757	44.478567
3501.282895	468361.395777	44.483572
3501.573440	468342.589126	44.488577
3501.515702	468316.200568	44.493581
3501.771152	468296.033934	44.498586
3501.944210	468274.868691	44.503591
3501.962687	468250.490978	44.508596
3501.896324	468227.390690	44.513601
3501.823606	468198.678039	44.518605
3501.896047	468183.293368	44.523610
3502.179497	468152.502393	44.528615
3501.932887	468129.531159	44.533620
3501.866947	468101.221850	44.538625
3501.869932	468071.182358	44.543629
3501.773072	468047.125719	44.548634
3501.900980	468018.533249	44.553639
3502.048966	467997.776123	44.558644
3501.998277	467963.395677	44.563649
3501.584568	467937.820478	44.568653
3501.714627	467918.886608	44.573658
3501.932048	467882.289706	44.578663
3501.790692	467869.567728	44.583668
3501.955079	467838.693557	44.588673
3501.927619	467825.043533	44.593677
3501.646660	467787.006827	44.598682
3501.810126	467770.191601	44.603687
3501.481225	467746.018919	44.608692
3501.685773	467721.206899	44.613697
3501.953401	467688.900370	44.618701
3501.625240	467660.631115	44.623706
3501.609548	467655.728091	44.628711
3501.269051	467621.594323	44.633716
3501.642779	467603.077327	44.638721
3501.629565	467586.238837	44.643725
3501.590570	467567.735453	44.648730
3501.571012	467536.535338	44.653735
3501.296607	467513.314714	44.658740
3501.593127	467493.899304	44.663745
3501.864368	467481.416259	44.668749
3501.676801	467463.391033	44.673754
3501.754104	467435.665172	44.678759
3501.554099	467415.467200	44.683764
3501.659130	467389.001267	44.688769
3501.647162	467374.033567	44.693773
3501.508840	467344.773346	44.698778
3501.815707	467336.077628	44.703783
3501.652933	467311.221011	44.708788
3501.946462	467282.955517	44.713793
3501.409241	467259.219129	44.718797
3501.394870	467242.077031	44.723802
3501.679243	467214.672593	44.728807
3501.405528	467197.924821	44.733812
3501.859833	467174.438607	44.738817
3501.892184	467144.999756	44.743821
3501.396660	467126.870366	44.748826
3501.593258	467096.141527	44.753831
3501.645213	467079.848696	44.758836
3501.868793	467053.616652	44.763841
3501.750120	467040.030753	44.768845
3501.562477	467018.667173	44.773850
3501.601708	466989.429273	44.778855
3501.198011	466967.391211	44.783860
3501.425948	466947.277800	44.788865
3501.649631	466931.312120	44.793869
3501.724342	466907.024837	44.798874
3501.840725	466888.395371	44.803879
3501.542317	466867.807451	44.808884
3501.793359	466838.131730	44.813889
3501.909103	466812.927581	44.818893
3501.607299	466787.788370	44.823898
3501.740495	466769.560754	44.828903
3501.628416	466752.382782	44.833908
3501.788371	466719.029059	44.838913
3501.821811	466697.883540	44.843917
3501.532813	466679.418074	44.848922
3501.641594	466649.814731	44.853927
3501.520454	466635.925435	44.858932
3501.801760	466599.821529	44.863937
3501.612348	466595.956732	44.868941
3501.485384	466568.412943	44.873946
3501.448496	466546.570121	44.878951
3501.280892	466524.393582	44.883956
3501.551121	466510.443279	44.888961
3501.877474	466485.458742	44.893965
3501.693752	466459.744329	44.898970
3501.707855	466437.134793	44.903975
3501.451283	466416.640957	44.908980
3501.821280	466389.879330	44.913985
3501.473096	466374.609020	44.918989
3501.364995	466357.328871	44.923994
3501.469009	466335.514423	44.928999
3501.456081	466322.467821	44.934004
3501.199401	466294.336851	44.939009
3501.625859	466277.681503	44.944013
3501.538644	466259.639359	44.949018
3501.496216	466238.403912	44.954023
3501.134204	466223.742533	44.959028
3501.547053	466192.422041	44.964033
3501.515825	466179.327598	44.969037
3501.325256	466154.220700	44.974042
3501.430617	466144.544187	44.979047
3501.141260	466129.416229	44.984052
3501.167187	466102.353647	44.989057
3501.163055	466102.253164	44.994061
3501.292008	466082.912770	44.999066
3501.338120	466067.833707	45.004071
3501.179522	466055.568219	45.009076
3501.593187	466026.978446	45.014081
3501.446692	466027.153002	45.019085
3501.535435	465994.871035	45.024090
3501.587674	465971.900896	45.029095
3501.524716	465957.698519	45.034100
3501.268834	465936.698215	45.039105
3501.440905	465914.012813	45.044109
3501.293461	465896.890042	45.049114
3501.282221	465886.574019	45.054119
3501.427115	465860.655816	45.059124
3501.633403	465852.430179	45.064129
3501.485054	465831.008387	45.069133
3501.443917	465807.192733	45.074138
3501.759287	465782.360591	45.079143
3501.955154	465763.565772	45.084148
3501.857701	465728.479907	45.089153
3501.286863	465718.756641	45.094157
3501.752018	465687.528223	45.099162
3501.857101	465664.448284	45.104167
3501.400726	465636.954221	45.109172
3501.749249	465611.256837	45.114177
3501.642483	465590.435207	45.119181
3501.499131	465585.197392	45.124186
3501.510338	465552.673748	45.129191
3501.470080	465533.207317	45.134196
3501.451202	465520.717380	45.139201
3501.247538	465501.731547	45.144205
3501.159540	465488.746556	45.149210
3501.334191	465464.391049	45.154215
3501.372968	465443.040800	45.159220
3501.801961	465429.166052	45.164225
3502.125678	465405.090736	45.169229
3501.679832	465388.823144	45.174234
3501.697002	465360.951466	45.179239
3501.387070	465343.347624	45.184244
3501.644841	465324.643840	45.189249
3501.915809	465299.615577	45.194253
3501.331755	465283.167072	45.199258
3501.349337	465251.855757	45.204263
3501.620785	465236.336246	45.209268
3501.727949	465213.457681	45.214273
3501.424744	465199.848422	45.219277
3501.136013	465172.125191	45.224282
3501.575363	465146.261224	45.229287
3501.485627	465144.606086	45.234292
3501.352790	465117.465462	45.239297
3501.606622	465104.022342	45.244301
3501.571884	465074.387972	45.249306
3502.042289	465048.367283	45.254311
3501.745369	465030.912829	45.259316
3501.870371	465001.152312	45.264321
3501.759128	464975.323182	45.269325
3501.616996	464958.046885	45.274330
3501.975485	464940.338606	45.279335
3501.483707	464907.740244	45.284340
3501.349385	464884.443586	45.289345
3501.689587	464878.877401	45.294349
3501.463684	464851.143863	45.299354
3501.743884	464832.081978	45.304359
3501.504690	464815.225284	45.309364
3501.665418	464792.540134	45.314369
3501.612622	464760.631887	45.319373
3501.120700	464753.627143	45.324378
3501.503539	464724.736470	45.329383
3501.229290	464711.678700	45.334388
3501.364661	464699.568798	45.339393
3501.697920	464681.712431	45.344397
3501.293063	464661.998240	45.349402
3501.163711	464630.506308	45.354407
3501.640387	464623.350783	45.359412
3501.429408	464593.692410	45.364417
3501.339602	464579.088394	45.369421
3501.221790	464563.780583	45.374426
3501.313632	464530.534275	45.379431
3501.132639	464529.904907	45.384436
3501.009756	464512.523995	45.389441
3501.332878	464494.871334	45.394445
3501.280126	464482.942296	45.399450
3501.416269	464457.073875	45.404455
3501.479005	464437.539566	45.409460
3501.265143	464438.078692	45.414465
3500.976161	464403.879758	45.419469
3501.224871	464402.424790	45.424474
3501.073976	464383.480063	45.429479
3501.423105	464374.017510	45.434484
3501.543358	464351.135737	45.439489
3501.203954	464328.780702	45.444493
3501.269858	464303.782872	45.449498
3501.352640	464298.256554	45.454503
3501.363222	464278.325519	45.459508
3501.199529	464250.075488	45.464513
3501.131930	464236.428784	45.469517
3501.170569	464224.080682	45.474522
3501.426575	464202.796222	45.479527
3501.253562	464198.422493	45.484532
3501.160500	464177.242903	45.489537
3501.427623	464156.411899	45.494541
3501.242165	464152.495337	45.499546
3501.317124	464112.877414	45.504551
3501.560769	464110.209222	45.509556
3501.341280	464092.337082	45.514561
3501.194147	464071.975100	45.519565
3501.425158	464061.417929	45.524570
3501.681867	464034.366690	45.529575
3501.611518	464027.093707	45.534580
3501.625161	463990.570605	45.539585
3501.626145	463981.111425	45.544589
3501.569441	463958.762490	45.549594
3501.836830	463939.145175	45.554599
3501.794361	463918.867888	45.559604
3501.676170	463890.357257	45.564609
3501.586680	463866.394631	45.569613
3501.420863	463852.864068	45.574618
3501.684034	463828.593592	45.579623
3501.288764	463817.627889	45.584628
3501.559872	463787.083740	45.589633
3501.639264	463763.904029	45.594637
3501.234959	463742.215904	45.599642
3501.572997	463721.778002	45.604647
3501.475313	463703.734743	45.609652
3501.229355	463684.702857	45.614657
3501.469775	463665.797600	45.619661
3501.199605	463638.473629	45.624666
3501.553148	463628.908805	45.629671
3501.538905	463611.510059	45.634676
3501.492876	463585.263978	45.639681
3501.703640	463564.592769	45.644685
3501.631084	463560.860839	45.649690
3501.652006	463526.358980	45.654695
3501.692263	463514.263030	45.659700
3501.633923	463489.080992	45.664705
3501.815575	463467.301332	45.669709
3501.824950	463443.676815	45.674714
3501.722119	463416.731124	45.679719
3501.487081	463388.946019	45.684724
3501.432471	463361.537472	45.689729
3501.594496	463340.620649	45.694733
3501.373521	463337.063521	45.699738
3501.522956	463303.805838	45.704743
3501.685190	463283.344180	45.709748
3501.499827	463267.893949	45.714753
3501.568388	463255.034631	45.719757
3501.686061	463237.311460	45.724762
3501.531278	463216.544955	45.729767
3501.438059	463187.826912	45.734772
3501.366838	463166.592072	45.739777
3501.669865	463148.991723	45.744781
3501.475214	463130.305329	45.749786
3501.305748	463112.727882	45.754791
3501.182658	463091.399848	45.759796
3501.129275	463080.734565	45.764801
3501.636618	463059.358973	45.769805
3501.244840	463041.411359	45.774810
3501.370386	463012.304875	45.779815
3501.411266	462944.867151	45.784820
3501.132363	462825.071235	45.789825
3501.376349	462669.023360	45.794829
3500.774386	462472.888523	45.799834
3500.824941	462204.612021	45.804839
3500.175199	461903.354841	45.809844
3499.503304	461561.775281	45.814849
3499.196160	461166.909878	45.819853
3498.536075	460724.937786	45.824858
3498.151754	460253.212571	45.829863
3497.378846	459715.810987	45.834868
3496.693877	459153.484985	45.839873
3495.956679	458535.084840	45.844877
3494.966699	457876.069184	45.849882
3494.415914	457161.448405	45.854887
3493.256179	456418.807039	45.859892
3492.163248	455625.465396	45.864897
3491.266019	454787.115606	45.869901
3489.444634	453929.991172	45.874906
3488.459799	453010.387662	45.879911
3487.404305	452069.842264	45.884916
3485.658706	451077.822726	45.889921
3484.351093	450042.194325	45.894925
3482.839400	448968.061763	45.899930
3481.608060	447867.190460	45.904935
3479.917711	446729.058030	45.909940
3478.463430	445545.447900	45.914945
3476.952738	444325.512322	45.919949
3475.219804	443066.788838	45.924954
3473.556132	441767.300115	45.929959
3471.505118	440457.398018	45.934964
3469.543671	439090.557281	45.939969
3467.830536	437707.824716	45.944973
3465.668481	436300.035044	45.949978
3463.831750	434845.327678	45.954983
3461.889428	433360.227232	45.959988
3459.576480	431854.903363	45.964993
3457.641872	430306.532529	45.969997
3455.230973	428742.555477	45.975002
3453.197553	427137.240799	45.980007
3450.851627	425502.801641	45.985012
3448.587297	423859.650695	45.990017
3446.409713	422186.138503	45.995021
3444.021445	420473.533779	46.000026
3441.507722	418741.539304	46.005031
3438.920333	416995.620169	46.010036
3436.459345	415223.774632	46.015041
3433.963539	413403.047341	46.020045
3431.169873	411584.190945	46.025050
3428.555745	409734.312903	46.030055
3426.126837	407879.532613	46.035060
3423.532098	405995.450665	46.040065
3420.900136	404082.142811	46.045069
3417.893342	402157.264088	46.050074
3415.308191	400205.515713	46.055079
3412.409341	398235.939644	46.060084
3409.378536	396260.940412	46.065089
3406.517685	394255.751037	46.070093
3403.462675	392248.343500	46.075098
3400.827604	390209.558255	46.080103
3397.999150	388157.408156	46.085108
3394.806407	386090.166822	46.090113
3392.109580	383994.774882	46.095117
3389.097207	381902.790587	46.100122
3385.842404	379783.985549	46.105127
3382.640184	377663.935421	46.110132
3379.444644	375530.686462	46.115137
3376.349306	373366.341029	46.120141
3372.990210	371211.773728	46.125146
3369.815512	369025.992054	46.130151
3366.855045	366851.314813	46.135156
3363.250641	364657.796514	46.140161
3360.364126	362445.376051	46.145165
3356.875801	360222.313095	46.150170
3353.401678	357990.214919	46.155175
3350.252952	355748.245978	46.160180
3346.828242	353503.109270	46.165185
3343.471565	351240.645303	46.170189
3340.068922	348979.632298	46.175194
3336.436357	346706.195414	46.180199
3333.057385	344432.209622	46.185204
3329.514795	342144.825821	46.190209
3326.458401	339844.909491	46.195213
3322.492754	337551.572957	46.200218
3319.043220	335243.388585	46.205223
3315.704280	332921.640549	46.210228
3311.911361	330610.326033	46.215233
3308.520239	328286.118873	46.220237
3304.899142	325975.827893	46.225242
3301.580000	323633.534295	46.230247
3297.775721	321296.959564	46.235252
3293.970625	318952.649923	46.240257
3290.601279	316611.123799	46.245261
3286.568861	314261.767263	46.250266
3283.037419	311920.661108	46.255271
3279.377072	309566.557574	46.260276
3275.861931	307212.419447	46.265281
3271.900817	304866.867543	46.270285
3268.031351	302511.650744	46.275290
3264.689188	300145.888713	46.280295
3261.251498	297784.035699	46.285300
3257.199095	295424.165367	46.290305
3253.777050	293061.047348	46.295309
3248.994208	290691.863281	46.300314
3245.394308	288337.272711	46.305319
3241.736052	285963.691165	46.310324
3237.664671	283612.469041	46.315329
3234.305832	281256.398669	46.320333
3230.651257	278908.318914	46.325338
3226.588776	276553.916588	46.330343
3222.842237	274198.555957	46.335348
3218.729958	271852.760371	46.340353
3215.136048	269500.074334	46.345357
3211.474134	267152.941669	46.350362
3207.218610	264796.449256	46.355367
3203.150778	262455.917476	46.360372
3199.031151	260124.282934	46.365377
3195.237396	257787.407874	46.370381
3191.083260	255462.566218	46.375386
3187.532957	253133.058249	46.380391
3183.756707	250818.447374	46.385396
3179.642097	248506.708673	46.390401
3175.379937	246185.514658	46.395405
3171.669313	243873.580142	46.400410
3167.481867	241567.171831	46.405415
3163.928480	239266.018139	46.410420
3159.963070	236979.275409	46.415425
3155.463580	234688.144396	46.420429
3151.657588	232412.200830	46.425434
3147.940354	230133.102335	46.430439
3143.904788	227870.067856	46.435444
3139.693139	225610.292706	46.440449
3135.894426	223356.387769	46.445453
3130.917492	221112.754890	46.450458
3127.426915	218884.712630	46.455463
3122.974425	216647.073846	46.460468
3118.793294	214439.839051	46.465473
3114.711213	212232.373109	46.470477
3110.672758	210038.007202	46.475482
3106.306590	207860.341454	46.480487
3102.318404	205670.387624	46.485492
3098.457532	203512.424756	46.490497
3094.097458	201354.666775	46.495501
3089.794024	199207.496521	46.500506
3085.246262	197083.568751	46.505511
3081.645697	194956.902212	46.510516
3076.751779	192853.873986	46.515521
3072.758417	190746.463057	46.520525
3067.919148	188669.626753	46.525530
3063.515019	186605.315771	46.530535
3059.802946	184563.549753	46.535540
3055.139711	182532.337308	46.540545
3050.558935	180511.417135	46.545549
3045.992444	178514.423424	46.550554
3041.196651	176535.118146	46.555559
3037.057631	174581.778910	46.560564
3032.557668	172645.729322	46.565569
3027.946263	170717.039988	46.570573
3023.432390	168811.094993	46.575578
3018.670834	166934.414383	46.580583
3014.116522	165075.967155	46.585588
3008.852777	163245.442384	46.590593
3004.237140	161432.789203	46.595597
2999.102599	159653.360618	46.600602
2994.120403	157905.383447	46.605607
2989.406475	156177.956676	46.610612
2984.158888	154495.079717	46.615617
2978.311120	152836.780002	46.620621
2973.019230	151163.184600	46.625626
2967.267990	149558.773077	46.630631
2961.321920	148029.530856	46.635636
2954.280094	146564.661944	46.640641
2948.186720	145141.295918	46.645645
2941.790103	143781.242979	46.650650
2935.572190	142454.739147	46.655655
2929.705449	141196.872014	46.660660
2923.632937	139982.188197	46.665665
2917.923691	138806.664971	46.670669
2912.576138	137682.946169	46.675674
2907.220807	136610.755113	46.680679
2902.073142	135561.812440	46.685684
2897.201633	134559.971841	46.690689
2892.300257	133595.520797	46.695693
2887.772459	132659.782176	46.700698
2883.571327	131740.447947	46.705703
2878.598328	130853.029134	46.710708
2874.242301	129999.597466	46.715713
2870.047909	129160.442316	46.720717
2865.978483	128347.156379	46.725722
2861.724184	127555.169320	46.730727
2857.932936	126769.256011	46.735732
2853.660031	126016.591171	46.740737
2850.082591	125268.499777	46.745741
2846.237524	124533.335026	46.750746
2842.637063	123809.846513	46.755751
2838.540752	123089.805847	46.760756
2834.902408	122391.098461	46.765761
2831.029644	121698.925953	46.770765
2827.125169	121014.706306	46.775770
2823.674916	120327.948161	46.780775
2819.851687	119664.952021	46.785780
2816.126374	119011.413380	46.790785
2812.530885	118360.002118	46.795789
2808.719798	117710.555771	46.800794
2804.479373	117077.731109	46.805799
2800.880003	116453.654943	46.810804
2796.617882	115848.931233	46.815809
2793.259453	115240.401992	46.820813
2789.399230	114641.344779	46.825818
2785.884911	114045.028141	46.830823
2782.130553	113457.023289	46.835828
2777.831215	112882.386909	46.840833
2774.008338	112312.682336	46.845837
2769.952991	111754.453124	46.850842
2766.344164	111198.413552	46.855847
2762.935548	110647.030238	46.860852
2759.335546	110111.844403	46.865857
2755.476161	109575.931556	46.870861
2751.979707	109037.262503	46.875866
2748.275839	108509.503758	46.880871
2745.230433	107970.920880	46.885876
2741.299695	107453.167759	46.890881
2737.678266	106925.166151	46.895885
2734.200240	106404.167577	46.900890
2730.352458	105890.378732	46.905895
2727.276034	105365.761468	46.910900
2723.411609	104857.736688	46.915905
2720.096331	104346.252854	46.920909
2717.047516	103834.519272	46.925914
2713.539159	103309.785275	46.930919
2710.168253	102793.490968	46.935924
2707.046078	102294.147598	46.940929
2703.679105	101766.746829	46.945933
2699.812252	101254.112803	46.950938
2696.711596	100728.581172	46.955943
2693.244123	100208.834599	46.960948
2689.764434	99694.538046	46.965953
2686.632366	99167.015801	46.970957
2683.352443	98641.711238	46.975962
2679.556632	98114.640056	46.980967
2676.279649	97580.227363	46.985972
2672.849962	97057.755495	46.990977
2669.280294	96521.792224	46.995981
2665.968416	95990.652532	47.000986
2662.211697	95465.131791	47.005991
2659.175569	94919.492919	47.010996
2655.407702	94387.879640	47.016001
2652.104077	93848.540694	47.021005
2649.175640	93319.737884	47.026010
2645.738430	92789.854324	47.031015
2642.376820	92246.981907	47.036020
2638.494176	91698.088431	47.041025
2635.065558	91150.544641	47.046029
2631.810794	90604.521164	47.051034
2628.693160	90061.370486	47.056039
2624.793705	89500.639754	47.061044
2621.205231	88952.017483	47.066049
2618.309950	88399.562176	47.071053
2614.587627	87846.229505	47.076058
2610.919638	87294.652019	47.081063
2607.590843	86733.427606	47.086068
2603.909037	86187.183578	47.091073
2600.628086	85629.504728	47.096077
2597.076237	85069.338037	47.101082
2593.734793	84511.334464	47.106087
2590.333041	83939.491961	47.111092
2586.793239	83386.012661	47.116097
2583.547069	82819.287642	47.121101
2580.375960	82255.356781	47.126106
2576.449327	81687.617070	47.131111
2573.482089	81116.411604	47.136116
2569.759739	80540.610268	47.141121
2565.985816	79968.270895	47.146125
2562.712774	79403.066874	47.151130
2559.011213	78826.053064	47.156135
2555.637381	78246.523695	47.161140
2552.133145	77675.320136	47.166145
2548.343321	77106.852642	47.171149
2545.005297	76527.277864	47.176154
2541.664822	75953.595698	47.181159
2538.232341	75380.028898	47.186164
2534.711218	74814.615435	47.191169
2531.125713	74233.147321	47.196173
2528.221517	73654.506450	47.201178
2524.472140	73067.743163	47.206183
2520.714730	72484.181256	47.211188
2516.833589	71909.120772	47.216193
2513.959212	71319.466615	47.221197
2510.502381	70747.031937	47.226202
2506.777391	70162.983201	47.231207
2503.587636	69566.097967	47.236212
2499.915316	68990.675561	47.241217
2496.740072	68404.060653	47.246221
2493.171209	67805.973710	47.251226
2489.850265	67219.414846	47.256231
2486.347398	66627.146909	47.261236
2482.641003	66041.595490	47.266241
2479.113536	65444.135065	47.271245
2475.793245	64858.950774	47.276250
2472.550227	64256.440980	47.281255
2469.072784	63653.468046	47.286260
2465.373900	63058.363135	47.291265
2462.136370	62451.757991	47.296269
2458.413803	61860.480622	47.301274
2454.796205	61265.482219	47.306279
2451.643322	60655.677783	47.311284
2447.904029	60059.236207	47.316289
2444.761873	59456.414993	47.321293
2441.246062	58849.250362	47.326298
2437.432969	58253.346754	47.331303
2434.176856	57647.599534	47.336308
2430.681966	57034.138366	47.341313
2427.000554	56434.699684	47.346317
2423.564229	55826.266443	47.351322
2420.076910	55218.021632	47.356327
2416.606312	54609.865933	47.361332
2413.087497	54008.496328	47.366337
2409.789839	53396.500353	47.371341
2406.227719	52789.623919	47.376346
2402.775722	52178.191276	47.381351
2399.431437	51560.509478	47.386356
2395.956175	50954.231869	47.391361
2392.449560	50344.873167	47.396365
2388.484068	49727.070539	47.401370
2384.814292	49100.421863	47.406375
2381.784333	48487.898468	47.411380
2378.387463	47876.856654	47.416385
2374.850330	47264.166007	47.421389
2371.406023	46657.629427	47.426394
2367.963079	46035.488460	47.431399
2364.518832	45416.085552	47.436404
2360.732897	44796.378763	47.441409
2357.358777	44184.856360	47.446413
2354.042348	43560.842976	47.451418
2350.083602	42948.557768	47.456423
2346.825130	42327.265096	47.461428
2343.231165	41709.802243	47.466433
2339.949040	41090.108014	47.471437
2336.573611	40462.038403	47.476442
2332.638779	39842.569888	47.481447
2329.375784	39211.881274	47.486452
2325.852393	38600.499486	47.491457
2322.227569	37980.991562	47.496461
2318.995844	37351.436496	47.501466
2315.375595	36746.030906	47.506471
2312.275012	36110.209607	47.511476
2308.718109	35490.224331	47.516481
2304.660788	34865.080165	47.521485
2301.214222	34240.594696	47.526490
2297.727825	33622.643475	47.531495
2294.182591	32987.695062	47.536500
2290.577369	32370.997105	47.541505
2287.108761	31741.721782	47.546509
2283.985448	31122.437931	47.551514
2279.701895	30508.752658	47.556519
2276.572696	29882.427821	47.561524
2272.884380	29270.955453	47.566529
2269.869345	28648.851878	47.571533
2266.460403	28030.199627	47.576538
2262.548269	27403.907532	47.581543
2259.122873	26782.900487	47.586548
2255.664399	26158.407378	47.591553
2251.674181	25533.598135	47.596557
2248.044079	24917.653938	47.601562
2244.511079	24301.795871	47.606567
2240.997581	23691.275402	47.611572
2237.455971	23077.312638	47.616577
2233.639087	22462.835167	47.621581
2230.175557	21854.631164	47.626586
2226.318737	21254.900382	47.631591
2223.066654	20645.262753	47.636596
2219.152079	20044.786012	47.641601
2215.462339	19462.762620	47.646605
2211.777860	18867.334389	47.651610
2207.602689	18283.762245	47.656615
2203.329779	17718.216124	47.661620
2198.713182	17166.521162	47.666625
2194.491963	16614.976752	47.671629
2190.476158	16085.166498	47.676634
2185.953750	15564.505494	47.681639
2182.441703	15044.749433	47.686644
2177.996263	14545.555720	47.691649
2174.378315	14047.728035	47.696653
2170.408706	13551.149032	47.701658
2166.050449	13065.290593	47.706663
2162.705901	12594.220270	47.711668
2158.824830	12127.249917	47.716673
2155.013065	11669.100029	47.721677
2151.606613	11210.046667	47.726682
2147.946360	10774.026020	47.731687
2144.771505	10332.390877	47.736692
2140.630399	9886.393169	47.741697
2136.906192	9451.369294	47.746701
2133.571739	9011.828741	47.751706
2129.967797	8592.088170	47.756711
2126.772095	8170.236243	47.761716
2123.319142	7748.478282	47.766721
2119.641602	7316.083110	47.771725
2116.259593	6897.346633	47.776730
2112.401791	6484.058133	47.781735
2108.821240	6058.617924	47.786740
2104.885839	5651.857522	47.791745
2101.258249	5238.934733	47.796749
2097.607275	4846.069182	47.801754
2094.073574	4453.934348	47.806759
2090.717342	4058.176088	47.811764
2086.636841	3682.553669	47.816769
2082.528019	3314.382684	47.821773
2077.877241	2961.229176	47.826778
2073.202238	2611.282160	47.831783
2069.368126	2277.914365	47.836788
2064.624285	1960.406981	47.841793
2060.583483	1659.751634	47.846797
2056.347236	1373.053092	47.851802
2052.159783	1100.646021	47.856807
2047.331297	827.270328	47.861812
2043.385471	579.809020	47.866817
2039.371098	349.249968	47.871821
2034.950792	136.334721	47.876826
2026.113161	47.610728	47.881831
2013.725738	109.560610	47.886836
2006.990476	112.155930	47.891841
2003.094376	118.713278	47.896845
2000.894637	116.157693	47.901850
1999.191680	121.222121	47.906855
1998.085294	105.275196	47.911860
1995.961663	110.319671	47.916865
1992.808649	116.112807	47.921869
1989.894273	119.521325	47.926874
1986.531497	118.706462	47.931879
1983.231855	112.481308	47.936884
1979.800540	111.329104	47.941889
1976.234205	112.001234	47.946893
1973.110504	109.962771	47.951898
1969.886863	118.775595	47.956903
1966.688480	113.088334	47.961908
1963.616945	114.759120	47.966913
1959.883166	112.024678	47.971917
1956.812095	105.175505	47.976922
1952.871925	109.990175	47.981927
1949.898362	113.012440	47.986932
1946.863398	104.775105	47.991937
1943.437122	110.743645	47.996941
1939.743038	101.166240	48.001946
1936.125431	101.030114	48.006951
1933.024241	103.622994	48.011956
1929.499040	104.962597	48.016961
1926.287039	110.869315	48.021965
1923.003184	106.116005	48.026970
1919.300216	116.325862	48.031975
1915.901031	107.518799	48.036980
1912.446116	108.607021	48.041985
1908.777692	112.835243	48.046989
1905.573602	104.852022	48.051994
1902.138576	105.440447	48.056999
1899.014251	98.634373	48.062004
1895.732171	106.330004	48.067009
1891.610151	111.581100	48.072013
1888.412295	106.365162	48.077018
1885.245167	107.275721	48.082023
1881.713937	106.705382	48.087028
1877.823240	107.965833	48.092033
1873.977696	109.042089	48.097037
1871.350241	103.379880	48.102042
1867.628053	116.218609	48.107047
1864.129689	99.391160	48.112052
1860.500343	103.714538	48.117057
1857.121477	103.326130	48.122061
1853.846758	98.909925	48.127066
1850.442840	106.020251	48.132071
1847.022482	98.978687	48.137076
1843.541299	102.541862	48.142081
1839.857446	99.385219	48.147085
1836.525189	105.057557	48.152090
1832.993685	100.624374	48.157095
1829.285148	98.338431	48.162100
1826.231509	101.544003	48.167105
1822.304372	99.905843	48.172109
1819.249170	100.817968	48.177114
1815.631319	106.629669	48.182119
1812.498091	99.461165	48.187124
1808.981116	101.378455	48.192129
1805.233068	98.535523	48.197133
1801.662691	92.479085	48.202138
1798.043946	101.552708	48.207143
1794.841836	102.952765	48.212148
1791.497529	97.838728	48.217153
1787.556722	102.795872	48.222157
1784.197632	90.293712	48.227162
1780.931689	91.368352	48.232167
1777.282255	97.684832	48.237172
1773.861517	92.937030	48.242177
1769.818259	96.363065	48.247181
1766.694998	88.797557	48.252186
1763.281426	97.304579	48.257191
1759.904488	96.207208	48.262196
1756.485104	90.620816	48.267201
1752.860041	93.146545	48.272205
1750.064856	98.732131	48.277210
1746.009998	98.183192	48.282215
1742.952289	105.913506	48.287220
1739.351178	103.803839	48.292225
1735.441610	99.698425	48.297229
1731.907157	87.299501	48.302234
1728.485028	98.930434	48.307239
1724.779009	91.006385	48.312244
1721.446800	96.798938	48.317249
1717.971287	106.182461	48.322253
1714.680169	98.737993	48.327258
1710.936239	99.266945	48.332263
1707.618823	96.233617	48.337268
1704.330707	103.860588	48.342273
1700.786046	99.106771	48.347277
1697.010014	93.028573	48.352282
1693.633283	106.636089	48.357287
1690.057058	96.227313	48.362292
1686.518239	90.650028	48.367297
1682.661728	99.539198	48.372301
1679.822225	94.520612	48.377306
1676.150163	101.666347	48.382311
1672.797073	94.168258	48.387316
1669.558455	98.111298	48.392321
1665.030618	102.001898	48.397325
1662.272616	96.945318	48.402330
1658.692866	92.940441	48.407335
1655.417289	99.508782	48.412340
1651.789838	92.189439	48.417345
1647.872138	99.436680	48.422349
1644.831969	93.987429	48.427354
1641.049192	98.252442	48.432359
1637.928912	91.192681	48.437364
1634.310772	93.948292	48.442369
1630.805765	97.401292	48.447373
1627.125547	90.624833	48.452378
1623.530087	95.923696	48.457383
1620.084777	93.976453	48.462388
1616.471207	87.784400	48.467393
1613.270080	96.271013	48.472397
1609.760282	96.624330	48.477402
1606.206231	100.496247	48.482407
1602.821638	91.310491	48.487412
1599.589816	98.969829	48.492417
1595.772620	102.446113	48.497421
1592.341718	98.959069	48.502426
1588.544765	102.391075	48.507431
1585.237547	99.729491	48.512436
1582.036757	93.821201	48.517441
1578.193679	100.465218	48.522445
1574.867230	98.154635	48.527450
1571.145490	98.664328	48.532455
1567.834120	96.224852	48.537460
1564.502528	101.941387	48.542465
1560.619843	100.340631	48.547469
1557.314355	95.113017	48.552474
1553.589212	106.949301	48.557479
1550.170406	102.267662	48.562484
1547.139626	89.986529	48.567489
1543.434398	108.140791	48.572493
1540.184361	94.485933	48.577498
1536.214045	107.113337	48.582503
1532.400852	95.425373	48.587508
1529.291593	99.841824	48.592513
1525.589370	100.531978	48.597517
1522.513574	98.685417	48.602522
1518.682490	103.856450	48.607527
1515.003508	97.744190	48.612532
1511.969427	93.100753	48.617537
1508.248986	101.487867	48.622541
1504.828542	94.680484	48.627546
1500.911653	105.445643	48.632551
1497.941700	97.748743	48.637556
1494.453101	86.832834	48.642561
1490.920882	107.576544	48.647565
1487.388198	96.123334	48.652570
1483.887377	91.875245	48.657575
1480.636460	90.932291	48.662580
1477.161423	87.588173	48.667585
1473.144349	96.426409	48.672589
1469.739034	82.979238	48.677594
1465.808836	93.635733	48.682599
1462.879564	89.779570	48.687604
1459.536685	92.539806	48.692609
1456.071319	93.879623	48.697613
1452.468692	91.846156	48.702618
1448.925914	99.316619	48.707623
1445.043447	90.417187	48.712628
1441.392069	90.011123	48.717633
1437.974992	89.056072	48.722637
1434.993278	84.258966	48.727642
1431.378950	88.671776	48.732647
1427.671536	91.618465	48.737652
1424.917757	83.606366	48.742657
1420.915863	93.046506	48.747661
1417.227368	88.315119	48.752666
1413.904075	98.709478	48.757671
1410.407570	93.084518	48.762676
1407.143239	84.180633	48.767681
1403.040057	99.220468	48.772685
1399.698069	93.517675	48.777690
1395.915245	96.514069	48.782695
1392.703203	98.292181	48.787700
1389.676003	86.526206	48.792705
1385.392207	91.062203	48.797709
1382.149927	87.618594	48.802714
1378.466303	90.941227	48.807719
1375.399442	93.326319	48.812724
1372.001408	84.538161	48.817729
1368.464442	91.362326	48.822733
1364.867764	85.259430	48.827738
1361.275025	87.802303	48.832743
1357.879549	82.133156	48.837748
1354.339159	84.212309	48.842753
1350.715378	89.234025	48.847757
1347.143241	80.409699	48.852762
1343.959057	95.743078	48.857767
1340.299659	90.820515	48.862772
1337.221198	87.348249	48.867777
1333.007047	94.148109	48.872781
1329.578503	89.547112	48.877786
1326.298759	90.323384	48.882791
1322.635472	92.519745	48.887796
1319.405670	82.506371	48.892801
1315.774956	89.689972	48.897805
1312.309616	86.353857	48.902810
1308.997743	93.706126	48.907815
1305.447176	89.361403	48.912820
1301.963277	83.377003	48.917825
1298.106889	83.983609	48.922829
1294.497433	74.427965	48.927834
1291.133820	86.195308	48.932839
1287.384520	80.945070	48.937844
1284.178141	78.691764	48.942849
1280.645382	84.025175	48.947853
1277.499681	89.162303	48.952858
1274.031444	80.843828	48.957863
1270.669186	85.400907	48.962868
1266.930643	82.249689	48.967873
1262.881913	91.051731	48.972877
1259.428460	84.287493	48.977882
1255.725616	89.505015	48.982887
1252.328934	92.786159	48.987892
1249.490401	87.372016	48.992897
1245.787175	97.597727	48.997901
1242.589620	85.045228	49.002906
1239.106358	87.700782	49.007911
1235.155057	95.513245	49.012916
1231.697852	89.002689	49.017921
1228.154738	87.975531	49.022925
1224.387439	90.858793	49.027930
1221.212934	89.799570	49.032935
1217.715491	82.311374	49.037940
1214.523397	76.107567	49.042945
1210.503126	83.975053	49.047949
1207.197989	88.494772	49.052954
1203.662906	90.800899	49.057959
1200.178912	98.841177	49.062964
1196.683611	87.363231	49.067969
1193.066818	93.500654	49.072973
1189.801957	81.414216	49.077978
1186.083193	87.811114	49.082983
1182.498411	88.074906	49.087988
1179.624188	91.328515	49.092993
1175.758379	89.117753	49.097997
1172.100757	85.833732	49.103002
1168.389025	88.300233	49.108007
1164.547067	90.979990	49.113012
1161.425287	78.596048	49.118017
1158.164247	89.632435	49.123021
1154.537813	80.645757	49.128026
1151.439279	78.976780	49.133031
1148.183927	85.424930	49.138036
1144.568257	86.304127	49.143041
1140.738289	81.854227	49.148045
1136.954018	87.017994	49.153050
1133.451710	84.842405	49.158055
1130.031469	99.247597	49.163060
1126.505201	93.510256	49.168065
1123.027525	91.998372	49.173069
1119.213277	92.696514	49.178074
1116.275898	92.176184	49.183079
1112.405685	84.818794	49.188084
1109.464259	85.694282	49.193089
1105.476964	92.110838	49.198093
1101.998390	89.668971	49.203098
1099.021678	89.021891	49.208103
1095.312810	92.750266	49.213108
1091.595859	82.616614	49.218113
1087.949935	90.438495	49.223117
1084.724148	85.043525	49.228122
1080.998484	95.310697	49.233127
1077.416337	95.320995	49.238132
1074.449486	81.707587	49.243137
1070.339972	87.045370	49.248141
1067.305922	93.427442	49.253146
1063.546592	86.356515	49.258151
1060.129612	86.262014	49.263156
1056.728534	83.346193	49.268161
1052.958721	86.005239	49.273165
1049.526341	81.740234	49.278170
1045.815033	90.445472	49.283175
1042.012987	92.922880	49.288180
1038.844004	83.096240	49.293185
1035.223905	86.839274	49.298189
1031.806367	82.790255	49.303194
1028.585181	90.669408	49.308199
1025.232739	85.892100	49.313204
1022.330426	84.315977	49.318209
1018.451018	86.894012	49.323213
1014.849150	82.478228	49.328218
1010.813430	82.654048	49.333223
1007.067577	83.477595	49.338228
1004.126342	81.445636	49.343233
1000.153947	89.359467	49.348237
997.344540	77.572327	49.353242
993.707485	90.875498	49.358247
989.866110	94.728910	49.363252
986.634292	85.158828	49.368257
982.845038	86.685144	49.373261
979.510664	80.028966	49.378266
976.170458	89.884968	49.383271
972.193585	95.369790	49.388276
969.161251	88.783651	49.393281
965.180666	90.773177	49.398285
961.788906	96.549727	49.403290
958.390506	86.005855	49.408295
955.038852	81.563786	49.413300
951.736039	88.069953	49.418305
948.040395	97.905360	49.423309
944.375940	92.002902	49.428314
940.928283	84.108380	49.433319
937.467874	86.763567	49.438324
934.245049	81.997734	49.443329
930.547050	95.892513	49.448333
927.054185	92.775865	49.453338
923.550585	83.260757	49.458343
919.792239	80.033581	49.463348
916.705784	68.318063	49.468353
912.934302	76.982049	49.473357
909.274644	72.243093	49.478362
905.896154	82.215781	49.483367
902.405109	84.929523	49.488372
899.119933	89.753033	49.493377
895.462297	91.375928	49.498381
891.918278	86.748681	49.503386
888.338829	87.669722	49.508391
884.578737	83.231133	49.513396
881.524323	76.107460	49.518401
877.576409	90.705511	49.523405
874.570990	78.787559	49.528410
871.013782	81.046541	49.533415
867.426943	90.178491	49.538420
864.023740	77.813110	49.543425
860.688959	82.384921	49.548429
856.729386	86.259907	49.553434
853.301891	78.510958	49.558439
850.047418	79.065048	49.563444
846.801680	76.027003	49.568449
842.832110	89.685647	49.573453
839.465909	82.917390	49.578458
835.979016	78.784287	49.583463
832.192447	82.790528	49.588468
829.001733	77.447087	49.593473
824.977655	91.088909	49.598477
821.546353	86.450455	49.603482
818.461126	89.088378	49.608487
814.638323	84.463414	49.613492
811.331680	83.035675	49.618497
807.987573	86.504818	49.623501
804.622148	92.270949	49.628506
801.078998	76.219534	49.633511
797.340160	82.477215	49.638516
793.679746	85.638102	49.643521
790.107316	81.638540	49.648525
787.157186	88.713061	49.653530
783.542740	78.190206	49.658535
780.085890	82.189417	49.663540
776.556687	85.159042	49.668545
772.137640	78.978625	49.673549
769.215554	79.544256	49.678554
765.715582	73.053098	49.683559
762.487878	79.718420	49.688564
759.054844	73.384517	49.693569
755.258015	77.170904	49.698573
751.867818	73.604880	49.703578
748.390309	75.282006	49.708583
744.846575	80.905057	49.713588
741.369806	77.045633	49.718593
737.829250	80.004373	49.723597
734.258580	78.791747	49.728602
730.680230	71.344712	49.733607
726.958154	80.918484	49.738612
723.878428	71.185583	49.743617
720.351838	82.320255	49.748621
717.011045	85.444049	49.753626
713.416122	75.421197	49.758631
709.442926	85.081519	49.763636
706.636619	77.865470	49.768641
703.028617	83.625076	49.773645
699.335109	80.751665	49.778650
695.666508	81.316457	49.783655
691.815373	81.523697	49.788660
688.707467	75.914293	49.793665
684.957589	87.188130	49.798669
681.604826	84.907066	49.803674
678.442665	82.340075	49.808679
675.088899	95.187874	49.813684
671.562060	73.720903	49.818689
667.633911	77.312612	49.823693
664.316061	76.101768	49.828698
660.488972	81.895482	49.833703
656.985638	88.116514	49.838708
653.765076	81.449002	49.843713
650.278834	81.026819	49.848717
646.470794	87.532561	49.853722
643.221330	82.043274	49.858727
639.518139	82.278109	49.863732
636.508819	82.572602	49.868737
632.840103	90.853626	49.873741
629.093072	83.926397	49.878746
626.183153	78.127998	49.883751
621.869179	85.829279	49.888756
618.203272	78.718587	49.893761
614.797539	78.884973	49.898765
611.505937	79.827675	49.903770
608.413486	79.363176	49.908775
604.906474	83.177228	49.913780
601.609869	76.613311	49.918785
597.798003	77.171945	49.923789
594.043822	78.996560	49.928794
590.806326	81.601261	49.933799
586.613951	80.409511	49.938804
583.435895	73.124809	49.943809
580.056561	76.925312	49.948813
576.786033	78.355106	49.953818
573.559788	77.506490	49.958823
569.435492	79.929714	49.963828
565.963561	77.714675	49.968833
562.625504	81.866250	49.973837
558.852575	78.473729	49.978842
555.627866	77.716622	49.983847
552.098133	84.150573	49.988852
548.349580	73.452503	49.993857
544.978222	82.272516	49.998861
541.988667	82.662017	50.003866
538.430827	83.057730	50.008871
534.228225	75.755367	50.013876
531.360101	76.401204	50.018881
527.873475	74.840175	50.023885
524.037829	83.052279	50.028890
520.731336	71.042076	50.033895
517.084935	83.682332	50.038900
513.835207	77.614157	50.043905
510.197716	83.217022	50.048909
505.988164	88.443886	50.053914
503.115262	80.564374	50.058919
499.058910	76.152992	50.063924
495.831831	79.948784	50.068929
492.506386	78.438596	50.073933
489.119420	75.704154	50.078938
485.997459	70.438651	50.083943
482.309482	69.994113	50.088948
478.587323	70.174976	50.093953
474.929604	77.584284	50.098957
471.298700	77.466211	50.103962
468.039408	77.220687	50.108967
464.494913	78.304012	50.113972
461.187044	70.194843	50.118977
457.518907	73.742933	50.123981
453.666097	74.355417	50.128986
450.482644	77.654052	50.133991
446.840908	72.184742	50.138996
443.691106	72.403053	50.144001
440.827121	72.140282	50.149005
436.835944	71.170329	50.154010
433.201972	68.721117	50.159015
429.020097	68.065584	50.164020
425.402633	72.830128	50.169025
421.975874	70.829536	50.174029
419.071004	76.093733	50.179034
415.753738	68.558660	50.184039
412.056640	73.753207	50.189044
408.644429	72.538105	50.194049
405.379978	71.597385	50.199053
401.830428	72.172155	50.204058
398.166591	60.110055	50.209063
394.397468	72.604902	50.214068
391.003627	66.828100	50.219073
387.519932	75.558042	50.224077
383.999449	81.338850	50.229082
380.302233	69.503401	50.234087
376.482328	67.886716	50.239092
373.507158	70.830237	50.244097
369.855437	69.304425	50.249101
366.285156	75.491607	50.254106
363.035952	72.520609	50.259111
359.434072	77.323862	50.264116
355.742423	70.097015	50.269121
352.304656	76.023130	50.274125
348.657874	67.773763	50.279130
345.604610	66.331951	50.284135
341.648480	69.776197	50.289140
338.539555	65.467281	50.294145
335.093965	74.336822	50.299149
331.560687	74.326954	50.304154
327.902986	71.520795	50.309159
324.485766	72.533705	50.314164
320.904740	67.526355	50.319169
317.104026	82.006582	50.324173
313.521661	79.090622	50.329178
310.404054	74.371783	50.334183
306.902258	78.608983	50.339188
303.463268	70.887243	50.344193
299.992481	65.505241	50.349197
296.159195	73.622081	50.354202
292.859416	68.555132	50.359207
289.012044	78.727385	50.364212
285.739032	75.519667	50.369217
282.470430	71.969587	50.374221
278.872005	79.916993	50.379226
275.755213	72.103969	50.384231
272.063349	72.128290	50.389236
268.112357	82.443225	50.394241
264.691478	79.780534	50.399245
260.583891	82.169563	50.404250
257.797146	72.473397	50.409255
254.003582	78.116401	50.414260
251.087583	67.510246	50.419265
247.762422	76.332571	50.424269
243.816518	78.743885	50.429274
240.513266	83.902444	50.434279
237.141715	77.739393	50.439284
233.216127	70.628085	50.444289
229.745499	77.948174	50.449293
225.984554	78.226858	50.454298
223.110391	76.178228	50.459303
219.207746	73.732915	50.464308
215.722290	76.243384	50.469313
212.116257	79.781835	50.474317
208.628109	75.275720	50.479322
205.567416	66.058804	50.484327
201.881762	73.491463	50.489332
198.197552	74.957232	50.494337
194.864020	72.303101	50.499341
191.466833	70.095466	50.504346
187.983451	67.955034	50.509351
183.673647	73.944165	50.514356
180.586797	62.709749	50.519361
177.284389	76.909921	50.524365
173.652068	78.905438	50.529370
170.270190	70.845814	50.534375
166.915914	76.970911	50.539380
163.691646	71.964992	50.544385
159.895114	76.282894	50.549389
156.189878	76.578225	50.554394
153.037671	65.910793	50.559399
149.285504	78.200539	50.564404
146.088957	75.594688	50.569409
142.278720	75.204036	50.574413
138.303525	78.091310	50.579418
134.760446	69.889117	50.584423
131.709048	77.441327	50.589428
128.293162	67.893760	50.594433
124.949736	77.142867	50.599437
121.190367	77.266303	50.604442
118.020334	66.301106	50.609447
113.814113	75.564323	50.614452
110.363783	68.429667	50.619457
107.493651	66.684138	50.624461
103.631540	72.514993	50.629466
100.023064	69.463936	50.634471
96.116726	72.508168	50.639476
92.790148	79.831151	50.644481
89.473918	70.002328	50.649485
86.227705	76.958468	50.654490
83.351592	69.025757	50.659495
79.210368	69.847710	50.664500
75.587972	69.826445	50.669505
71.962639	69.384871	50.674509
68.185763	68.647362	50.679514
65.094803	72.757348	50.684519
62.064913	78.502930	50.689524
58.135796	75.270854	50.694529
54.583241	66.462733	50.699533
51.124068	70.348483	50.704538
47.408037	73.904079	50.709543
43.999819	70.869307	50.714548
40.524752	69.417281	50.719553
37.378256	67.613552	50.724557
33.604097	78.226826	50.729562
30.585808	67.975155	50.734567
26.722650	74.910299	50.739572
23.170409	68.348332	50.744577
19.563882	69.985524	50.749581
16.001668	79.132665	50.754586
12.528713	73.826980	50.759591
8.759945	83.202431	50.764596
5.304767	78.175544	50.769601
2.123946	72.033463	50.774605