Fri Aug 26 13:59:46 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.934239	109.680986	0.000000
1.330167	100.770596	0.005005
1.277067	100.978196	0.010010
1.002678	86.759154	0.015014
0.996166	81.635061	0.020019
0.539312	77.327709	0.025024
0.445274	65.355274	0.030029
0.058681	51.865552	0.035034
-0.214003	47.953463	0.040038
-0.700322	33.381495	0.045043
-0.889930	36.647452	0.050048
-1.554198	22.748584	0.055053
-1.957160	9.868863	0.060058
-2.610669	7.452372	0.065062
-2.404161	11.643709	0.070067
-2.791108	16.443120	0.075072
-2.641147	5.606449	0.080077
-3.330249	-1.034293	0.085082
-3.882568	-10.211426	0.090086
-3.778298	-8.082689	0.095091
-3.969046	1.969456	0.100096
-3.896631	-5.251742	0.105101
-4.206319	-2.204369	0.110106
-4.669591	-5.647026	0.115110
-4.744843	-14.265705	0.120115
-5.059459	-5.216135	0.125120
-5.528643	-5.829574	0.130125
-5.913569	-1.843538	0.135130
-6.080762	-0.333736	0.140134
-6.151983	-10.800613	0.145139
-6.618856	-8.317205	0.150144
-7.514922	-7.851813	0.155149
-7.469787	-7.861982	0.160154
-7.387933	-2.468038	0.165158
-7.983036	-13.894185	0.170163
-7.760237	-2.232864	0.175168
-7.722619	-8.420459	0.180173
-7.720255	-10.300010	0.185178
-8.279061	-6.906977	0.190182
-8.685345	-7.542863	0.195187
-9.048991	-1.971992	0.200192
-9.028612	-10.317671	0.205197
-9.290904	-1.567301	0.210202
-10.402705	-3.229089	0.215206
-10.270315	-9.785767	0.220211
-10.595629	-15.100632	0.225216
-10.544891	-10.679411	0.230221
-10.699909	-5.874989	0.235226
-10.731585	-8.445241	0.240230
-11.111323	-2.606119	0.245235
-11.667908	-2.990822	0.250240
-11.912141	-8.498641	0.255245
-11.925177	-10.429575	0.260250
-12.490620	-9.806860	0.265254
-12.482731	-8.381264	0.270259
-13.239583	-9.278932	0.275264
-13.658889	-5.917109	0.280269
-13.459020	-5.182605	0.285274
-13.693583	-5.389663	0.290278
-13.657470	-6.211484	0.295283
-13.492792	-6.221284	0.300288
-14.163423	-16.518903	0.305293
-14.670033	-12.719561	0.310298
-15.368244	-8.767004	0.315302
-15.086291	-10.671104	0.320307
-15.388243	-3.350854	0.325312
-15.198234	-17.392189	0.330317
-15.519333	-9.268559	0.335322
-16.159835	-8.039392	0.340326
-16.179757	-11.623839	0.345331
-16.225087	3.473819	0.350336
-16.502471	1.296151	0.355341
-17.253825	-4.996387	0.360346
-17.657927	2.681444	0.365350
-17.506106	-9.756310	0.370355
-17.730699	-5.896476	0.375360
-18.039856	-8.151451	0.380365
-18.694262	-0.738361	0.385370
-19.006947	1.496424	0.390374
-18.737234	-17.071841	0.395379
-19.508739	-10.035977	0.400384
-19.496542	-2.018019	0.405389
-19.173987	-13.371914	0.410394
-19.498610	-4.399878	0.415398
-19.828981	-6.423768	0.420403
-20.279122	1.223266	0.425408
-20.593870	-5.694050	0.430413
-20.526444	-12.588613	0.435418
-20.982349	-2.621733	0.440422
-21.642272	-9.004432	0.445427
-22.262271	3.743533	0.450432
-22.098441	-10.009002	0.455437
-21.899821	-3.794874	0.460442
-22.012057	0.512523	0.465446
-22.305246	-10.100121	0.470451
-23.217175	2.743914	0.475456
-23.382582	-0.144027	0.480461
-23.323384	0.846489	0.485466
-23.238198	3.417945	0.490470
-23.382500	-4.832495	0.495475
-24.516473	-2.691294	0.500480
-24.640281	2.269617	0.505485
-24.944545	-10.606471	0.510490
-25.010967	-2.592092	0.515494
-24.969052	-11.380869	0.520499
-25.145174	-2.476244	0.525504
-25.551529	-0.328112	0.530509
-26.068357	-8.808440	0.535514
-26.723821	0.990203	0.540518
-26.365782	-2.089965	0.545523
-26.405292	3.942950	0.550528
-26.457920	-7.276606	0.555533
-26.598428	-10.472132	0.560538
-27.511425	-2.306960	0.565542
-27.561791	-6.266305	0.570547
-27.772127	-5.619788	0.575552
-27.968191	-5.883459	0.580557
-28.579609	-13.469564	0.585562
-29.065920	1.007078	0.590566
-29.398404	-8.969883	0.595571
-29.477032	1.393822	0.600576
-29.555415	-4.370766	0.605581
-29.624058	-10.548142	0.610586
-29.901979	-6.044112	0.615590
-29.436515	-8.698095	0.620595
-30.144231	-2.551653	0.625600
-30.906165	-11.996691	0.630605
-30.649798	-9.474036	0.635610
-31.184604	0.464002	0.640614
-30.951441	-9.515609	0.645619
-31.670689	-5.357303	0.650624
-32.416320	-3.482203	0.655629
-32.517967	-4.273084	0.660634
-32.985838	-3.735160	0.665638
-32.401379	-2.114607	0.670643
-32.540099	-0.308692	0.675648
-32.921726	-7.955886	0.680653
-32.792999	-8.501072	0.685658
-33.763827	-4.575668	0.690662
-33.981552	-5.633204	0.695667
-33.978219	-5.810866	0.700672
-34.024502	-6.793858	0.705677
-34.634442	1.982167	0.710682
-35.203674	3.035729	0.715686
-35.389445	-13.085722	0.720691
-35.805390	-2.210772	0.725696
-35.678185	-1.218191	0.730701
-35.783087	-8.133378	0.735706
-35.869857	2.453050	0.740710
-36.167563	-14.505156	0.745715
-36.784243	-6.588596	0.750720
-36.839574	-13.894299	0.755725
-36.799621	-8.696308	0.760730
-37.285383	-4.700901	0.765734
-38.093949	-9.295141	0.770739
-38.545432	-11.945556	0.775744
-38.642370	-0.512856	0.780749
-38.699873	-12.899032	0.785754
-38.815821	-10.144408	0.790758
-38.765666	-8.212883	0.795763
-38.749962	-6.785340	0.800768
-38.838860	-9.719992	0.805773
-39.423615	-6.727865	0.810778
-40.241716	-5.085081	0.815782
-39.758167	-8.827009	0.820787
-40.147801	-0.860379	0.825792
-40.385516	-2.835422	0.830797
-41.190127	-4.817110	0.835802
-41.582500	3.921877	0.840806
-41.355592	-8.565530	0.845811
-41.791193	-0.123523	0.850816
-41.897718	-6.358275	0.855821
-41.852254	-3.400998	0.860826
-42.612007	1.307762	0.865830
-42.814151	-13.969608	0.870835
-42.965160	0.862935	0.875840
-43.531244	-8.615761	0.880845
-43.208127	-8.748303	0.885850
-43.292432	-6.511115	0.890854
-43.643387	-9.699183	0.895859
-44.318545	-3.874175	0.900864
-44.440977	-9.780593	0.905869
-44.673525	-4.729991	0.910874
-44.766628	3.750436	0.915878
-45.011937	-10.871669	0.920883
-45.690376	-3.831312	0.925888
-45.829172	0.287238	0.930893
-45.625023	-6.318576	0.935898
-46.147241	5.085434	0.940902
-46.099422	-0.524803	0.945907
-47.255360	-7.519945	0.950912
-47.230387	-3.638859	0.955917
-47.171788	-2.322395	0.960922
-47.638358	3.182247	0.965926
-47.199159	-6.788317	0.970931
-47.417741	-3.530511	0.975936
-48.055180	-5.430663	0.980941
-48.642768	-2.501367	0.985946
-48.944696	7.017613	0.990950
-49.140215	-3.287547	0.995955
-48.954885	5.029311	1.000960
-49.208632	-1.059137	1.005965
-49.757403	-6.143065	1.010970
-50.675119	-7.167540	1.015974
-50.259747	-0.341778	1.020979
-50.710335	-5.368229	1.025984
-50.810725	-4.156720	1.030989
-50.582757	-7.862017	1.035994
-51.142102	0.286055	1.040998
-51.002573	-13.320327	1.046003
-51.778611	-5.100555	1.051008
-51.732686	-7.141906	1.056013
-51.729630	-2.052059	1.061018
-52.562741	-1.770468	1.066022
-52.937412	-15.967480	1.071027
-53.262357	-6.024159	1.076032
-53.481187	-3.968498	1.081037
-53.366263	-10.351618	1.086042
-53.525523	1.720351	1.091046
-53.619264	-8.648107	1.096051
-53.993233	-2.610575	1.101056
-54.916832	-2.539514	1.106061
-54.897796	-1.564890	1.111066
-55.033512	5.188495	1.116070
-55.069162	-8.267233	1.121075
-55.177397	-11.281128	1.126080
-55.995412	-0.251831	1.131085
-56.487099	-5.942575	1.136090
-56.794827	-3.863582	1.141094
-56.587125	-9.887837	1.146099
-56.556891	-1.110252	1.151104
-56.838430	-1.072723	1.156109
-56.553602	-2.850725	1.161114
-57.261497	-1.503500	1.166118
-57.465014	-4.790452	1.171123
-58.024931	-4.026233	1.176128
-58.429970	-5.013476	1.181133
-58.163288	-11.413896	1.186138
-58.435966	-1.250929	1.191142
-58.811071	-12.198813	1.196147
-59.323271	-14.118464	1.201152
-59.609135	-3.494716	1.206157
-59.181725	-12.859185	1.211162
-60.070519	-3.527236	1.216166
-60.678841	-15.387900	1.221171
-61.149526	-11.012042	1.226176
-61.043863	-4.878352	1.231181
-60.943951	-12.730227	1.236186
-61.292245	-8.537934	1.241190
-60.941681	-7.934457	1.246195
-61.232237	-3.558170	1.251200
-61.767985	-10.415763	1.256205
-61.794208	-12.094716	1.261210
-62.377226	-15.009377	1.266214
-62.362413	-9.016562	1.271219
-62.927610	-10.086433	1.276224
-63.251933	-4.781106	1.281229
-63.168368	-5.214859	1.286234
-63.369509	-4.462210	1.291238
-63.991460	-9.389214	1.296243
-64.624097	-9.002800	1.301248
-64.977942	-3.762476	1.306253
-64.819427	0.113636	1.311258
-65.359244	-3.082990	1.316262
-64.980084	-7.428739	1.321267
-65.136156	-9.853075	1.326272
-65.262965	-4.834756	1.331277
-65.962335	-7.405447	1.336282
-66.460616	-7.568280	1.341286
-66.627127	-10.101719	1.346291
-66.778473	-5.481362	1.351296
-66.786231	-5.109986	1.356301
-67.202939	-10.565638	1.361306
-67.578960	-3.796986	1.366310
-67.945861	-5.201441	1.371315
-68.296095	-6.314272	1.376320
-68.237232	-10.249494	1.381325
-68.342243	-8.129301	1.386330
-68.594001	-6.150768	1.391334
-68.916178	-14.329214	1.396339
-69.231827	-6.646180	1.401344
-69.849696	0.862457	1.406349
-69.517927	-4.668606	1.411354
-69.976189	-8.605568	1.416358
-70.410376	-11.214383	1.421363
-70.962371	-8.227358	1.426368
-70.726016	-6.052751	1.431373
-71.129030	-10.608897	1.436378
-71.179118	-2.249062	1.441382
-70.928058	-14.493459	1.446387
-71.617362	-8.242323	1.451392
-72.042843	-2.769390	1.456397
-72.235216	-8.611135	1.461402
-72.582253	-3.678744	1.466406
-72.423634	-10.948159	1.471411
-72.325962	-3.408569	1.476416
-73.389558	-5.229713	1.481421
-73.385937	-13.265903	1.486426
-73.841884	-0.609925	1.491430
-73.955604	-2.911147	1.496435
-74.143581	-2.761639	1.501440
-74.853553	-11.050543	1.506445
-74.748153	-6.118997	1.511450
-75.260241	-6.678299	1.516454
-75.227742	-8.647959	1.521459
-75.530914	1.728558	1.526464
-75.475592	-1.554405	1.531469
-75.789343	-12.426422	1.536474
-76.508751	-9.539876	1.541478
-76.143882	-8.261608	1.546483
-77.039903	-7.021129	1.551488
-77.633924	-1.971191	1.556493
-77.146585	-11.553791	1.561498
-77.132434	-3.599415	1.566502
-77.726834	1.567637	1.571507
-77.956008	2.520798	1.576512
-78.620469	2.611621	1.581517
-78.530324	-9.281868	1.586522
-78.473606	-9.148314	1.591526
-78.866326	-7.916599	1.596531
-79.307776	-10.736247	1.601536
-79.867627	-8.263672	1.606541
-79.708244	-3.365840	1.611546
-80.050362	-5.460663	1.616550
-79.898730	-9.903857	1.621555
-80.591955	-11.380885	1.626560
-80.994497	-6.987163	1.631565
-81.410493	-6.735716	1.636570
-81.610136	-3.158168	1.641574
-81.632824	-12.759428	1.646579
-81.483561	-11.824063	1.651584
-81.662816	-7.474599	1.656589
-81.790988	-13.414919	1.661594
-82.715186	-1.170073	1.666598
-83.045227	-5.563580	1.671603
-83.218419	2.296585	1.676608
-83.422951	6.020424	1.681613
-83.367716	-8.657963	1.686618
-83.724490	-2.629437	1.691622
-84.123966	-4.139547	1.696627
-84.676414	-7.236132	1.701632
-84.865337	-7.744514	1.706637
-84.709804	-7.148636	1.711642
-85.114276	-5.516471	1.716646
-84.999038	-3.354644	1.721651
-84.736773	-9.988485	1.726656
-85.746768	-9.438915	1.731661
-85.611961	-18.147238	1.736666
-86.057264	-5.091140	1.741670
-86.734877	-10.335330	1.746675
-87.340171	-3.236763	1.751680
-87.756917	-1.245196	1.756685
-87.253137	-7.998896	1.761690
-87.628175	6.090272	1.766694
-87.466418	-6.194006	1.771699
-87.477800	-3.069698	1.776704
-88.011849	-6.109039	1.781709
-88.448040	-14.051440	1.786714
-89.216951	-0.723498	1.791718
-88.996967	-3.971988	1.796723
-89.009490	-0.062919	1.801728
-89.382337	-5.126781	1.806733
-89.865656	-5.965799	1.811738
-89.934859	-5.410856	1.816742
-90.407810	-9.424620	1.821747
-90.392675	-7.294661	1.826752
-90.457967	-8.565748	1.831757
-91.019012	2.357102	1.836762
-91.616599	7.132360	1.841766
-91.938493	2.750236	1.846771
-92.091591	-0.652129	1.851776
-92.076871	6.590342	1.856781
-91.657354	-7.046980	1.861786
-92.545879	-2.878136	1.866790
-92.892799	2.108020	1.871795
-93.161524	-0.463287	1.876800
-93.450018	0.100491	1.881805
-93.242456	0.273832	1.886810
-93.379443	-1.299293	1.891814
-94.275211	-0.403690	1.896819
-94.793013	-8.273276	1.901824
-94.896173	1.736751	1.906829
-94.712974	-7.403040	1.911834
-95.120567	-2.056275	1.916838
-95.012966	-9.472763	1.921843
-95.545552	-11.541093	1.926848
-96.095256	-2.499215	1.931853
-96.327740	-6.018928	1.936858
-96.888133	-1.932810	1.941862
-96.848841	-6.146549	1.946867
-97.099839	-2.614787	1.951872
-96.929683	5.334283	1.956877
-97.092057	-4.991851	1.961882
-97.291022	-4.236376	1.966886
-97.248843	-7.156635	1.971891
-98.119918	0.495826	1.976896
-98.310077	-2.438877	1.981901
-98.384435	-14.695876	1.986906
-98.498768	0.532732	1.991910
-98.793056	-4.002379	1.996915
-99.632803	-2.465799	2.006912
-99.280477	-4.782346	2.016909
-98.621908	4.795626	2.026906
-98.273822	-8.977804	2.036902
-97.280301	0.972485	2.046899
-96.908634	-6.567430	2.056896
-96.875026	2.458471	2.066893
-96.159090	-4.048529	2.076890
-95.762765	-0.220268	2.086886
-94.673808	-7.219321	2.096883
-94.523464	-2.019162	2.106880
-94.192046	-3.027364	2.116877
-93.610582	-4.093505	2.126874
-93.102517	-4.809274	2.136870
-92.794795	2.982896	2.146867
-91.652055	5.526062	2.156864
-91.543268	-2.001434	2.166861
-91.273314	-2.509073	2.176858
-90.357244	1.599381	2.186854
-89.842469	-2.228108	2.196851
-89.699338	-3.393887	2.206848
-89.314320	-3.298575	2.216845
-88.577619	-7.749807	2.226842
-87.993076	-1.860175	2.236838
-87.397785	-8.886897	2.246835
-87.096318	-5.506350	2.256832
-86.786441	-6.292627	2.266829
-85.740901	-7.624253	2.276826
-85.558806	-6.515361	2.286822
-85.322161	-0.641250	2.296819
-84.512303	-4.061703	2.306816
-84.572033	-4.343787	2.316813
-83.390696	-4.701902	2.326810
-83.119934	-6.587613	2.336806
-82.650335	-7.940435	2.346803
-81.796645	-2.935315	2.356800
-81.683220	-6.861864	2.366797
-81.068486	-10.920318	2.376794
-80.934358	-7.577070	2.386790
-79.678926	-8.976221	2.396787
-79.085666	0.548566	2.406784
-78.890142	-8.459075	2.416781
-79.181660	-5.784458	2.426778
-78.188754	-1.694303	2.436774
-77.638736	-8.821677	2.446771
-76.843430	-12.236695	2.456768
-76.182054	-2.541957	2.466765
-75.973208	-4.307159	2.476762
-75.750865	-4.975274	2.486758
-75.034492	-4.906211	2.496755
-74.736665	-10.074698	2.506752
-73.777883	-1.167505	2.516749
-73.123078	-4.684188	2.526746
-73.213111	-4.413543	2.536742
-72.748266	-6.719100	2.546739
-72.037253	-5.987155	2.556736
-71.589239	-7.650217	2.566733
-70.688531	-8.658362	2.576730
-70.343915	-6.171486	2.586726
-70.396546	-6.293124	2.596723
-69.512391	-5.493107	2.606720
-68.915412	-8.275384	2.616717
-68.642821	-1.123953	2.626714
-67.594267	-1.211145	2.636710
-67.490743	-6.979751	2.646707
-67.368579	2.941493	2.656704
-66.601847	-4.143602	2.666701
-65.902088	-5.734992	2.676698
-65.596997	-6.960833	2.686694
-65.018638	3.073108	2.696691
-64.799261	1.287259	2.706688
-63.377286	-9.802453	2.716685
-63.061255	-0.944064	2.726682
-63.300642	-0.498116	2.736678
-62.884827	0.514201	2.746675
-62.088468	1.549627	2.756672
-61.682159	0.133802	2.766669
-60.651204	-1.135366	2.776666
-60.819425	1.089248	2.786662
-60.285321	2.298551	2.796659
-59.287758	3.489544	2.806656
-59.120105	5.224722	2.816653
-58.019025	5.705872	2.826650
-57.516380	1.864433	2.836646
-57.808326	4.044958	2.846643
-57.227990	5.025324	2.856640
-56.103265	4.134349	2.866637
-56.205233	1.879031	2.876634
-55.580401	2.665575	2.886630
-54.710686	6.103364	2.896627
-54.350334	-6.952915	2.906624
-54.139382	-13.527001	2.916621
-53.312205	-4.567640	2.926618
-52.929296	-0.753126	2.936614
-52.848617	-0.277820	2.946611
-51.778460	-1.147627	2.956608
-51.471983	-3.384179	2.966605
-50.835827	2.237671	2.976602
-50.252553	-1.328062	2.986598
-50.155517	1.609164	2.996595
-49.556785	4.018463	3.006592
-48.868957	4.538616	3.016589
-48.491651	0.060979	3.026586
-47.901660	4.736541	3.036582
-47.316301	13.103192	3.046579
-47.168344	4.707979	3.056576
-46.544575	0.816003	3.066573
-46.050597	10.292903	3.076570
-45.239347	5.921924	3.086566
-44.861583	4.618245	3.096563
-44.483563	3.659805	3.106560
-44.472961	5.314902	3.116557
-43.135156	3.510133	3.126554
-42.904903	-3.035286	3.136550
-42.357617	-5.784485	3.146547
-41.911251	-5.942636	3.156544
-41.709274	-6.550561	3.166541
-40.914135	-5.901403	3.176538
-40.431437	-4.291302	3.186534
-40.052943	3.043208	3.196531
-39.119163	0.103957	3.206528
-38.688557	-7.771410	3.216525
-38.495075	-2.533618	3.226522
-38.219069	-8.775724	3.236518
-37.526351	-4.657834	3.246515
-37.125461	3.366915	3.256512
-36.085346	1.415266	3.266509
-35.840046	-1.103188	3.276506
-35.558002	-5.043323	3.286502
-34.494798	-2.966092	3.296499
-34.222722	-1.120464	3.306496
-34.341467	-4.377329	3.316493
-33.191920	-8.528556	3.326490
-32.643178	-5.984765	3.336486
-32.742678	0.955349	3.346483
-31.983623	-0.366515	3.356480
-31.206714	-1.143149	3.366477
-31.025274	-6.984074	3.376474
-30.332308	-0.522127	3.386470
-29.821744	2.464751	3.396467
-29.648322	-4.711694	3.406464
-28.902424	-4.362135	3.416461
-28.351592	-1.897861	3.426458
-28.134235	-2.992838	3.436454
-27.285613	-1.522071	3.446451
-26.959470	0.530542	3.456448
-26.358519	-1.137326	3.466445
-25.237287	-1.973905	3.476442
-25.332118	-3.948409	3.486438
-25.369600	-3.936194	3.496435
-24.463548	1.748169	3.506432
-23.994151	-2.132442	3.516429
-23.153096	-5.652782	3.526426
-22.630589	-2.059567	3.536422
-22.330429	-8.086864	3.546419
-22.044702	-8.413233	3.556416
-21.491286	-14.293066	3.566413
-20.886498	-0.648900	3.576410
-20.528864	-12.006871	3.586406
-19.541530	-6.031067	3.596403
-19.152198	-8.277351	3.606400
-18.976037	-5.254246	3.616397
-18.862675	-2.547636	3.626394
-18.111009	-1.853696	3.636390
-17.197898	-4.213209	3.646387
-16.909217	-6.570529	3.656384
-16.559928	-8.088344	3.666381
-15.580094	-3.375281	3.676378
-15.269266	-10.550944	3.686374
-15.083476	2.822687	3.696371
-14.216051	-11.744341	3.706368
-13.955165	-5.265804	3.716365
-13.426750	-9.792308	3.726362
-12.643610	0.285778	3.736358
-12.140835	0.068161	3.746355
-12.015365	1.949286	3.756352
-11.331683	-2.914996	3.766349
-10.935054	-2.773975	3.776346
-10.297373	-0.576638	3.786342
-9.739384	-0.520926	3.796339
-9.160204	-3.373290	3.806336
-9.180504	-7.481753	3.816333
-8.653520	-0.325578	3.826330
-7.643851	-2.646274	3.836326
-7.364726	-3.237701	3.846323
-6.691442	0.715331	3.856320
-6.241593	-6.244402	3.866317
-6.269778	-5.096433	3.876314
-5.361413	6.226070	3.886310
-5.098906	6.052198	3.896307
-4.351634	13.497186	3.906304
-4.018285	16.232902	3.916301
-3.658804	21.622249	3.926298
-3.137888	33.866708	3.936294
-2.422449	51.576857	3.946291
-2.187990	49.585921	3.956288
-1.670209	58.454114	3.966285
-1.264188	73.317177	3.976282
-0.294941	77.692967	3.986278
-0.195899	88.466811	3.996275
0.040236	101.794667	4.006272
0.000000	113.178217	4.011277
0.443129	129.414780	4.016282
0.753318	133.219854	4.021286
0.938769	141.394395	4.026291
0.976871	152.455005	4.031296
1.177853	151.635980	4.036301
0.763891	156.031521	4.041306
1.376376	161.583337	4.046310
1.729727	163.483493	4.051315
1.441499	172.655592	4.056320
1.459564	174.940138	4.061325
1.470677	171.417259	4.066330
1.700984	167.869743	4.071334
1.426956	172.854090	4.076339
1.199372	177.293382	4.081344
1.819708	171.002343	4.086349
1.766267	174.462255	4.091354
1.584070	178.970409	4.096358
1.726777	177.935835	4.101363
1.558351	171.827713	4.106368
1.617938	159.201725	4.111373
1.707449	169.428622	4.116378
1.516743	167.174163	4.121382
1.252766	159.340901	4.126387
1.159509	169.586764	4.131392
1.853275	161.914423	4.136397
1.571449	166.852528	4.141402
1.794473	170.800891	4.146406
1.853908	173.904716	4.151411
1.617734	180.098022	4.156416
1.788204	168.315284	4.161421
1.630032	176.837564	4.166426
1.583762	170.884425	4.171430
1.759024	173.299516	4.176435
1.756793	176.109229	4.181440
1.809476	169.792679	4.186445
1.709432	177.113204	4.191450
1.812925	176.945256	4.196454
2.133339	171.659507	4.201459
1.696597	182.832031	4.206464
1.690398	171.510221	4.211469
1.308867	175.960827	4.216474
1.604811	176.547506	4.221478
1.991083	172.811195	4.226483
1.795535	175.312494	4.231488
2.110275	176.231596	4.236493
1.863629	177.013483	4.241498
1.895170	181.270066	4.246502
2.158806	177.271281	4.251507
1.968689	175.124294	4.256512
1.793993	172.557301	4.261517
1.656843	172.888717	4.266522
2.122120	192.187491	4.271526
2.585796	188.980115	4.276531
1.895814	179.991991	4.281536
2.044460	174.577965	4.286541
2.416284	174.671951	4.291546
2.201104	171.013466	4.296550
1.883034	166.165642	4.301555
1.763629	176.213105	4.306560
2.032189	170.508333	4.311565
1.627493	179.935845	4.316570
2.043463	192.222099	4.321574
2.425053	193.994479	4.326579
2.375997	197.039270	4.331584
2.751177	194.279095	4.336589
2.601828	190.082022	4.341594
1.965218	175.264424	4.346598
2.140258	169.124972	4.351603
2.315966	169.578515	4.356608
2.106244	167.431418	4.361613
2.108460	165.846093	4.366618
2.261006	171.915602	4.371622
2.345605	178.039982	4.376627
1.670856	183.153161	4.381632
2.604051	190.056561	4.386637
2.281829	199.939467	4.391642
2.462671	205.764141	4.396646
2.296614	201.775306	4.401651
2.436145	198.093225	4.406656
2.780863	203.977803	4.411661
2.226648	192.772941	4.416666
2.070626	182.853814	4.421670
2.507336	181.086947	4.426675
2.418648	192.477363	4.431680
2.484428	199.389273	4.436685
2.623031	208.061510	4.441690
2.455564	189.108689	4.446694
2.407309	187.123107	4.451699
1.834434	189.885631	4.456704
2.446823	198.635953	4.461709
2.443679	206.058458	4.466714
2.342029	202.236762	4.471718
2.404922	206.779528	4.476723
2.446689	200.439357	4.481728
2.793832	198.904728	4.486733
2.618064	204.908308	4.491738
2.110986	208.486312	4.496742
2.500723	199.750839	4.501747
2.667645	213.062952	4.506752
2.447438	201.888336	4.511757
2.509253	206.231958	4.516762
2.668136	204.982897	4.521766
2.765864	202.205809	4.526771
2.517715	203.421356	4.531776
2.362303	198.924675	4.536781
2.598268	209.989315	4.541786
2.823064	196.897825	4.546790
2.747819	199.184248	4.551795
2.890487	203.584882	4.556800
2.883171	209.280669	4.561805
2.759600	206.234323	4.566810
2.618243	200.194741	4.571814
2.846357	200.608488	4.576819
2.600935	204.939836	4.581824
2.606823	194.084354	4.586829
2.870749	202.575728	4.591834
2.599857	204.285187	4.596838
2.724291	211.086732	4.601843
2.771701	220.671659	4.606848
2.904272	217.411427	4.611853
2.806611	228.107252	4.616858
3.436036	226.360995	4.621862
2.997332	208.883533	4.626867
2.899232	202.030476	4.631872
2.995885	198.832787	4.636877
2.782616	201.849364	4.641882
2.844411	204.304272	4.646886
2.882987	206.917815	4.651891
3.053697	223.367719	4.656896
3.091115	218.442386	4.661901
3.151271	213.247765	4.666906
3.015416	209.273208	4.671910
2.789194	215.483960	4.676915
2.864662	223.159982	4.681920
3.198162	229.843564	4.686925
3.099660	223.367041	4.691930
3.125174	225.751672	4.696934
3.195522	224.813781	4.701939
3.294124	228.430361	4.706944
3.066476	213.495274	4.711949
2.918848	212.069314	4.716954
3.252570	216.595225	4.721958
3.305135	218.656111	4.726963
2.855207	218.485745	4.731968
3.443474	220.422097	4.736973
3.061132	229.058397	4.741978
3.416128	222.103150	4.746982
3.183924	208.140028	4.751987
2.874268	219.242169	4.756992
3.421999	230.903672	4.761997
3.245724	227.207481	4.767002
3.545841	229.096951	4.772006
3.278538	222.982060	4.777011
2.807047	226.086301	4.782016
3.075026	228.186414	4.787021
3.247667	226.419529	4.792026
3.286757	232.076461	4.797030
3.148797	222.670181	4.802035
2.968480	229.629911	4.807040
3.336208	232.777492	4.812045
3.458487	231.676495	4.817050
3.306802	229.580464	4.822054
3.122307	228.397519	4.827059
3.372988	229.313943	4.832064
3.162884	223.857684	4.837069
3.211096	224.555701	4.842074
3.224995	221.459475	4.847078
3.523515	226.756481	4.852083
3.471882	248.024518	4.857088
3.471602	244.361031	4.862093
3.492452	248.359873	4.867098
3.693376	248.091334	4.872102
3.733074	238.606766	4.877107
3.601729	234.609355	4.882112
3.394041	226.248455	4.887117
3.526315	234.940673	4.892122
3.667840	242.913297	4.897126
3.542580	238.101870	4.902131
3.334530	234.106911	4.907136
3.717512	238.672614	4.912141
3.813063	246.462576	4.917146
3.433654	243.446565	4.922150
3.730485	239.053464	4.927155
3.918207	256.190433	4.932160
3.917122	244.924726	4.937165
3.719978	233.686389	4.942170
3.581563	233.331482	4.947174
3.791537	226.746819	4.952179
3.311772	238.255099	4.957184
3.562177	243.366617	4.962189
3.902157	235.806275	4.967194
3.895315	244.197461	4.972198
4.070210	249.064478	4.977203
3.733132	238.945724	4.982208
3.889531	230.455370	4.987213
3.775956	223.914756	4.992218
3.407510	234.538852	4.997222
4.108193	231.474897	5.002227
4.084101	250.369048	5.007232
4.225071	238.669948	5.012237
3.636279	235.759303	5.017242
3.583090	229.930606	5.022246
4.297743	248.848937	5.027251
3.873735	225.114559	5.032256
3.655739	234.155534	5.037261
3.924976	229.671821	5.042266
3.853973	247.687442	5.047270
4.177741	247.697163	5.052275
4.039988	256.516853	5.057280
4.100049	240.157580	5.062285
3.968894	249.491920	5.067290
3.792726	259.937401	5.072294
3.825750	247.087701	5.077299
3.633979	251.885259	5.082304
4.225224	248.942742	5.087309
4.298323	255.144869	5.092314
4.105013	251.236194	5.097318
4.416081	250.722721	5.102323
4.066961	259.116586	5.107328
4.063398	254.735452	5.112333
4.030168	251.409282	5.117338
3.814644	261.933657	5.122342
4.074995	256.154207	5.127347
3.916912	257.210205	5.132352
4.103484	249.866727	5.137357
4.133054	253.993923	5.142362
4.170122	258.338247	5.147366
3.914691	249.690547	5.152371
4.055731	252.421018	5.157376
4.085751	245.364503	5.162381
4.073082	255.338446	5.167386
4.083306	253.378551	5.172390
4.334792	253.117959	5.177395
4.208625	252.476413	5.182400
4.320595	258.925584	5.187405
4.306181	250.749711	5.192410
4.274720	262.311592	5.197414
4.440640	266.490326	5.202419
4.219812	266.195706	5.207424
4.234321	266.164996	5.212429
4.627994	269.919136	5.217434
4.540532	281.641606	5.222438
4.685784	258.593657	5.227443
3.995433	263.611212	5.232448
4.700303	256.892537	5.237453
4.535463	253.678605	5.242458
4.286706	255.033452	5.247462
4.601927	255.642443	5.252467
4.254258	249.350234	5.257472
4.828774	262.943766	5.262477
4.784659	252.247891	5.267482
4.117117	247.856244	5.272486
4.400251	247.505305	5.277491
4.595560	273.679770	5.282496
4.987140	265.554571	5.287501
4.798252	256.228968	5.292506
4.291435	260.556735	5.297510
4.437421	256.395920	5.302515
4.481835	250.975953	5.307520
4.534687	263.818656	5.312525
4.997206	271.722334	5.317530
4.581522	267.974826	5.322534
4.512221	252.803085	5.327539
4.460663	279.490548	5.332544
4.483758	272.359172	5.337549
4.444889	274.526048	5.342554
4.534529	284.069633	5.347558
4.878052	277.998822	5.352563
4.728390	286.421756	5.357568
4.888675	277.231597	5.362573
4.957714	275.484002	5.367578
5.073316	277.883087	5.372582
5.198835	269.663272	5.377587
4.857793	264.040729	5.382592
4.532483	258.880801	5.387597
4.689850	261.738443	5.392602
4.615185	269.507463	5.397606
4.850447	272.340324	5.402611
4.998409	278.154323	5.407616
4.825907	275.694539	5.412621
4.594323	272.699799	5.417626
4.702719	280.513086	5.422630
4.752953	278.452049	5.427635
4.471836	280.036559	5.432640
4.648699	283.754858	5.437645
5.134524	278.256666	5.442650
4.200649	282.239650	5.447654
4.541204	278.032717	5.452659
4.661393	295.041036	5.457664
4.837413	298.730996	5.462669
4.897690	303.581073	5.467674
4.823926	310.831123	5.472678
5.036012	312.452739	5.477683
5.075902	303.654629	5.482688
4.821017	303.767100	5.487693
5.384041	300.496780	5.492698
4.867908	310.811728	5.497702
4.912031	309.618493	5.502707
5.045851	315.004443	5.507712
4.956631	311.816691	5.512717
5.055598	309.134304	5.517722
4.923852	310.651268	5.522726
5.410851	300.878728	5.527731
5.460492	302.788222	5.532736
5.408173	308.715670	5.537741
5.688575	307.618522	5.542746
4.864615	315.238473	5.547750
5.629928	309.766357	5.552755
5.174606	310.517467	5.557760
5.098776	301.117290	5.562765
5.496739	310.008618	5.567770
5.428790	306.700498	5.572774
5.330350	302.669476	5.577779
5.273928	304.589156	5.582784
5.411934	305.247886	5.587789
5.215911	306.977334	5.592794
5.067484	303.289446	5.597798
5.372798	294.361432	5.602803
4.963152	307.032571	5.607808
5.039271	300.339009	5.612813
5.183137	305.346912	5.617818
4.897859	304.967415	5.622822
5.232008	303.716369	5.627827
5.261748	319.932050	5.632832
5.210683	329.779137	5.637837
5.482288	329.562867	5.642842
5.395789	332.717914	5.647846
5.556794	326.802052	5.652851
5.205579	332.953213	5.657856
5.602798	336.690997	5.662861
5.743663	330.775106	5.667866
5.184586	338.489865	5.672870
5.894220	328.891450	5.677875
5.851427	330.764720	5.682880
5.287224	326.875811	5.687885
5.653296	330.558333	5.692890
5.174137	330.775325	5.697894
5.321613	332.846757	5.702899
5.166246	329.112489	5.707904
5.414701	338.558611	5.712909
5.482226	332.768031	5.717914
5.586513	332.302570	5.722918
5.688671	341.879038	5.727923
5.633529	335.882933	5.732928
5.357658	338.757423	5.737933
5.878779	333.161971	5.742938
5.605169	332.584506	5.747942
5.772846	332.393909	5.752947
5.586117	334.602795	5.757952
5.824362	349.042839	5.762957
5.899567	336.464913	5.767962
5.750071	341.341334	5.772966
5.796292	329.951150	5.777971
5.666547	340.750113	5.782976
5.675341	348.721305	5.787981
6.039992	353.533497	5.792986
5.869176	352.626820	5.797990
5.683103	337.454205	5.802995
5.893958	349.895889	5.808000
5.854132	355.691696	5.813005
5.908369	359.552488	5.818010
6.021194	365.150527	5.823014
6.116222	355.992635	5.828019
5.698036	353.172465	5.833024
5.798506	357.127297	5.838029
5.837912	357.225585	5.843034
5.620227	357.927042	5.848038
5.893063	356.963945	5.853043
6.144101	359.101512	5.858048
5.801177	361.097443	5.863053
5.680753	357.538060	5.868058
5.941603	360.620048	5.873062
5.848899	358.828026	5.878067
5.933575	364.803765	5.883072
6.142048	357.583381	5.888077
6.177635	355.464505	5.893082
5.891747	368.299914	5.898086
5.911145	360.419278	5.903091
5.617860	364.909975	5.908096
5.747902	366.284945	5.913101
6.054433	369.280730	5.918106
6.132823	377.756783	5.923110
6.538811	383.030777	5.928115
6.118330	377.942578	5.933120
6.054315	380.907474	5.938125
6.160486	374.316772	5.943130
6.250216	378.969297	5.948134
6.455086	374.242473	5.953139
6.046819	382.009699	5.958144
6.225694	386.420560	5.963149
6.101806	386.787879	5.968154
6.517539	389.070648	5.973158
6.472323	384.433378	5.978163
6.428726	373.772150	5.983168
6.179112	366.338351	5.988173
6.337161	364.836313	5.993178
5.957491	380.331193	5.998182
6.201451	375.199655	6.003187
6.277846	389.380197	6.008192
6.619477	391.598575	6.013197
6.507073	388.281543	6.018202
6.070327	390.871044	6.023206
6.467293	386.332604	6.028211
6.421626	393.954796	6.033216
6.332117	384.487103	6.038221
6.475652	389.514063	6.043226
6.268469	386.993226	6.048230
6.654038	383.826449	6.053235
6.535347	389.441559	6.058240
6.532847	393.431414	6.063245
6.283266	373.292134	6.068250
6.136569	381.138855	6.073254
6.221555	387.351832	6.078259
6.129647	393.823303	6.083264
6.038304	394.451307	6.088269
6.597242	390.359042	6.093274
6.338319	397.473443	6.098278
6.888680	392.752933	6.103283
6.492256	388.401295	6.108288
6.390700	396.386525	6.113293
6.452219	389.109916	6.118298
6.509397	386.446679	6.123302
6.330440	381.681539	6.128307
6.386915	369.280510	6.133312
5.942142	370.570973	6.138317
6.303730	378.082294	6.143322
6.461114	395.050116	6.148326
6.144726	392.179289	6.153331
6.409821	383.988310	6.158336
6.234449	381.481503	6.163341
6.136809	372.635170	6.168346
6.102764	391.293742	6.173350
6.512313	384.301465	6.178355
6.491913	391.739390	6.183360
6.455419	385.727710	6.188365
6.923858	384.373493	6.193370
6.539240	389.833857	6.198374
6.504339	375.495039	6.203379
6.522927	373.733143	6.208384
6.304838	374.384044	6.213389
6.300074	362.334235	6.218394
6.204652	369.192218	6.223398
6.398073	376.435496	6.228403
6.271487	384.557494	6.233408
6.155179	383.050715	6.238413
6.776943	388.933348	6.243418
6.383518	386.726241	6.248422
6.371566	375.553892	6.253427
6.609313	375.137251	6.258432
6.012045	366.239000	6.263437
6.308874	361.428260	6.268442
6.252534	389.325170	6.273446
6.360275	380.880284	6.278451
6.548853	386.453881	6.283456
6.287812	388.161822	6.288461
6.830413	375.394039	6.293466
6.616217	363.544514	6.298470
6.474221	357.919424	6.303475
6.081041	360.793199	6.308480
5.868201	365.518140	6.313485
6.330754	378.929879	6.318490
6.469611	391.601098	6.323494
6.659450	382.868187	6.328499
6.393960	373.332988	6.333504
6.123458	367.180581	6.338509
6.326399	375.096246	6.343514
6.309355	381.394708	6.348518
6.577252	394.381192	6.353523
6.543000	380.671848	6.358528
6.153102	381.482375	6.363533
6.441631	376.131929	6.368538
6.189190	383.564850	6.373542
6.098367	389.153475	6.378547
6.348643	393.031208	6.383552
6.575124	393.932426	6.388557
6.649561	394.246721	6.393562
6.377756	393.485478	6.398566
6.207654	386.007655	6.403571
6.603398	391.843223	6.408576
6.164431	383.875757	6.413581
6.080903	377.229169	6.418586
5.923619	391.468242	6.423590
6.634206	391.541123	6.428595
6.796560	393.857015	6.433600
6.659992	389.373171	6.438605
6.531105	377.671703	6.443610
5.966216	375.149614	6.448614
6.405090	381.500476	6.453619
6.216078	386.345097	6.458624
6.350680	394.027805	6.463629
6.724019	390.037202	6.468634
6.590224	388.792570	6.473638
6.207670	375.558233	6.478643
5.847057	373.292237	6.483648
6.052618	381.539687	6.488653
6.242837	388.331058	6.493658
6.187409	390.405614	6.498662
6.552177	389.200415	6.503667
6.513709	398.707061	6.508672
6.550687	398.517829	6.513677
6.758491	388.782384	6.518682
6.524282	391.460572	6.523686
6.280834	388.407549	6.528691
6.552939	388.479098	6.533696
6.398228	386.430976	6.538701
6.069160	367.996664	6.543706
6.397522	389.895395	6.548710
6.350586	387.843147	6.553715
6.698537	392.417507	6.558720
6.182872	381.437474	6.563725
6.725043	376.813154	6.568730
6.083617	385.524669	6.573734
6.381365	378.448563	6.578739
6.319822	387.610787	6.583744
6.108719	390.358143	6.588749
6.398983	390.107330	6.593754
6.473969	396.179500	6.598758
6.286972	389.925499	6.603763
6.045211	384.141929	6.608768
5.964975	395.123040	6.613773
6.584651	391.467401	6.618778
6.226366	398.685857	6.623782
6.332486	388.985225	6.628787
6.431886	391.864569	6.633792
5.990889	390.743695	6.638797
6.410364	390.254468	6.643802
6.404770	390.578060	6.648806
6.384185	395.171836	6.653811
6.442374	389.199196	6.658816
5.935169	388.939671	6.663821
6.606152	378.230457	6.668826
5.953035	392.328433	6.673830
6.297105	386.880752	6.678835
6.378050	389.604783	6.683840
6.468846	394.481771	6.688845
6.484499	388.949182	6.693850
6.218924	396.725835	6.698854
5.997130	392.359662	6.703859
6.359474	384.431948	6.708864
6.022160	388.489749	6.713869
6.259227	391.360313	6.718874
6.291009	406.920868	6.723878
6.452526	408.980631	6.728883
6.445729	404.853060	6.733888
6.345249	414.328241	6.738893
6.542885	397.716452	6.743898
6.025645	398.455058	6.748902
6.046445	404.054783	6.753907
6.512254	419.098523	6.758912
6.846494	420.457523	6.763917
6.598361	404.275796	6.768922
6.394280	403.051597	6.773926
6.312075	393.329665	6.778931
6.377241	392.901930	6.783936
6.348580	392.865286	6.788941
6.293624	387.353183	6.793946
6.275957	394.467985	6.798950
6.268199	392.691207	6.803955
6.320652	398.406222	6.808960
6.104688	397.807125	6.813965
6.334020	406.076195	6.818970
6.529404	412.180244	6.823974
6.429825	412.996191	6.828979
6.816168	401.423293	6.833984
6.561164	407.983438	6.838989
6.305385	396.595941	6.843994
6.120879	392.644736	6.848998
6.252668	386.454996	6.854003
6.294542	384.616708	6.859008
6.319720	399.456957	6.864013
6.523342	398.083860	6.869018
6.287085	405.074514	6.874022
6.500195	402.722351	6.879027
6.124104	389.417396	6.884032
6.256534	411.514337	6.889037
6.774602	414.600578	6.894042
6.363140	403.259462	6.899046
6.326132	395.061731	6.904051
6.401747	387.447574	6.909056
6.255859	394.534884	6.914061
6.079401	386.058316	6.919066
6.531296	408.146641	6.924070
6.645871	402.532208	6.929075
6.290278	389.369593	6.934080
6.143880	398.975300	6.939085
6.588353	396.055611	6.944090
6.603122	404.291649	6.949094
6.637088	403.913064	6.954099
6.500252	392.038820	6.959104
6.185423	398.478564	6.964109
6.534411	390.695294	6.969114
6.285855	393.571867	6.974118
6.036615	388.605698	6.979123
6.431029	387.244024	6.984128
6.464795	384.480031	6.989133
6.700380	381.102492	6.994138
6.343066	388.093005	6.999142
6.487322	385.893931	7.004147
6.177119	392.937222	7.009152
6.213989	394.250772	7.014157
6.504378	393.107772	7.019162
6.498243	394.513438	7.024166
6.185380	400.876947	7.029171
6.753964	394.635016	7.034176
6.293440	396.785300	7.039181
6.584374	394.338765	7.044186
6.341527	393.082637	7.049190
6.110993	387.983844	7.054195
6.405561	388.766895	7.059200
6.055705	393.696672	7.064205
6.106129	392.970679	7.069210
6.240095	397.211367	7.074214
6.021877	397.691448	7.079219
6.743397	406.323643	7.084224
6.713883	405.208304	7.089229
6.449591	396.919411	7.094234
6.357167	404.422338	7.099238
6.169100	396.023502	7.104243
6.084005	390.797661	7.109248
6.253561	400.774950	7.114253
6.556710	403.037285	7.119258
6.371080	403.477492	7.124262
6.517916	401.904431	7.129267
6.685358	396.613959	7.134272
6.384008	389.593162	7.139277
6.256142	388.274840	7.144282
6.116435	390.286590	7.149286
6.242656	393.088992	7.154291
6.344626	387.188630	7.159296
6.175798	404.374927	7.164301
6.596876	412.035186	7.169306
6.492443	412.060959	7.174310
6.435234	399.699755	7.179315
6.687704	394.475138	7.184320
6.321054	395.070077	7.189325
6.412985	394.676140	7.194330
6.439071	404.273977	7.199334
6.396308	391.945330	7.204339
6.377941	394.675333	7.209344
6.674431	392.686671	7.214349
6.532983	389.393143	7.219354
6.827935	395.193786	7.224358
6.403054	397.192990	7.229363
6.522452	393.501349	7.234368
6.406225	387.976639	7.239373
6.859882	388.114833	7.244378
6.729883	389.992195	7.249382
6.476821	386.668590	7.254387
6.312744	384.925642	7.259392
6.362945	391.286403	7.264397
6.463449	387.246532	7.269402
6.290998	383.182723	7.274406
6.041925	380.238143	7.279411
6.432931	392.762538	7.284416
6.350724	399.115444	7.289421
6.397033	396.333677	7.294426
6.523529	406.944090	7.299430
6.624327	391.603379	7.304435
6.638255	377.307576	7.309440
6.063340	369.342302	7.314445
6.073605	369.872229	7.319450
5.990604	379.740134	7.324454
6.064887	386.789997	7.329459
6.291461	385.577840	7.334464
5.984332	398.685494	7.339469
6.409202	394.047796	7.344474
6.467548	403.403331	7.349478
6.626626	394.915646	7.354483
6.808971	400.743314	7.359488
6.613965	403.222414	7.364493
6.753778	394.911732	7.369498
6.300845	396.235104	7.374502
6.378042	396.169323	7.379507
6.290893	401.694106	7.384512
6.102866	394.285508	7.389517
6.425151	391.270951	7.394522
6.558239	397.482769	7.399526
6.175882	391.566065	7.404531
6.538938	387.358767	7.409536
6.140526	394.055129	7.414541
6.601870	393.388542	7.419546
6.320403	383.026933	7.424550
6.273276	390.997359	7.429555
6.783328	398.330551	7.434560
6.251621	384.508833	7.439565
6.396618	385.542959	7.444570
6.428155	389.809084	7.449574
6.256005	383.641358	7.454579
6.537274	382.097987	7.459584
6.225941	384.544576	7.464589
6.303479	377.585013	7.469594
6.326806	387.129487	7.474598
6.620072	387.732410	7.479603
6.647334	377.408156	7.484608
5.858384	376.920418	7.489613
6.368218	384.475098	7.494618
6.465070	393.951181	7.499622
6.564489	386.937588	7.504627
6.706545	379.069484	7.509632
6.334373	379.352075	7.514637
6.099942	364.908293	7.519642
6.324882	370.605934	7.524646
6.456036	366.542314	7.529651
6.406470	364.392403	7.534656
6.350427	372.838765	7.539661
6.259691	363.469350	7.544666
6.353346	366.270491	7.549670
6.014435	370.951788	7.554675
6.606376	378.414589	7.559680
6.516266	383.218501	7.564685
6.233857	382.452582	7.569690
6.348314	377.717688	7.574694
6.550069	383.292395	7.579699
6.613503	369.830439	7.584704
6.062490	359.482337	7.589709
6.026640	365.682483	7.594714
6.187321	378.413569	7.599718
6.233937	381.231527	7.604723
6.758477	380.586739	7.609728
6.485708	395.251914	7.614733
6.474029	391.460460	7.619738
6.458116	379.213062	7.624742
6.090896	383.303992	7.629747
6.418977	379.839287	7.634752
6.275456	385.834743	7.639757
6.570115	383.007984	7.644762
6.536659	389.989202	7.649766
6.323233	381.100782	7.654771
6.380737	377.355507	7.659776
6.077860	372.103469	7.664781
6.660807	375.486482	7.669786
6.541639	374.986209	7.674790
6.372867	370.418800	7.679795
6.352835	373.908350	7.684800
5.806613	379.049027	7.689805
6.164346	378.414392	7.694810
6.294603	378.286566	7.699814
6.395525	390.122143	7.704819
6.454478	386.050778	7.709824
6.319994	390.257331	7.714829
6.380150	394.278559	7.719834
6.255167	397.692706	7.724838
6.624570	400.074438	7.729843
6.502102	389.033180	7.734848
6.311190	403.464157	7.739853
6.070883	392.843036	7.744858
6.667935	398.441622	7.749862
6.612950	390.202400	7.754867
6.644064	389.314901	7.759872
6.047203	380.460872	7.764877
6.311706	386.522513	7.769882
6.320557	392.237987	7.774886
6.206777	401.743706	7.779891
6.622809	393.785483	7.784896
6.171036	400.717943	7.789901
6.350470	395.868524	7.794906
6.487615	392.038081	7.799910
6.046318	398.586099	7.804915
6.518777	402.043267	7.809920
6.671545	398.248354	7.814925
6.598849	398.648831	7.819930
6.367521	382.711277	7.824934
6.431889	392.448678	7.829939
6.363343	382.408254	7.834944
5.954034	384.759368	7.839949
6.361696	388.612595	7.844954
6.533247	389.243959	7.849958
6.322864	391.624212	7.854963
6.662432	388.755659	7.859968
6.110198	388.563255	7.864973
6.401030	386.104081	7.869978
6.898388	388.402615	7.874982
6.200095	380.149665	7.879987
6.146948	383.875323	7.884992
6.317438	392.201004	7.889997
6.358345	396.582729	7.895002
6.324748	391.418472	7.900006
6.137869	396.927144	7.905011
6.556344	393.938737	7.910016
6.378802	389.556184	7.915021
6.399158	394.330245	7.920026
6.394979	390.537623	7.925030
6.278267	401.837625	7.930035
6.571739	391.313729	7.935040
6.501067	399.022072	7.940045
6.402391	377.248961	7.945050
6.326275	372.277988	7.950054
6.192910	382.387851	7.955059
6.642901	381.501573	7.960064
6.263354	383.892345	7.965069
6.296535	387.870315	7.970074
6.553693	395.552925	7.975078
6.303583	391.896669	7.980083
6.492046	390.630335	7.985088
6.084413	382.775049	7.990093
6.308820	383.325418	7.995098
6.398084	388.265916	8.000102
6.187835	391.876834	8.005107
6.616958	391.803715	8.010112
6.545256	404.617988	8.015130
6.410052	385.294962	8.020147
6.421328	378.836785	8.025165
5.998342	387.116800	8.030182
6.511436	388.952410	8.035200
6.321427	394.823112	8.040218
6.301925	403.542061	8.045235
6.779277	402.063498	8.050253
6.560818	395.376009	8.055270
6.343484	373.831587	8.060288
6.278907	378.240626	8.065306
6.286447	389.082260	8.070323
6.549275	389.438972	8.075341
6.536188	389.816552	8.080358
6.348009	383.692369	8.085376
6.506597	394.415820	8.090394
6.393769	393.814902	8.095411
6.392420	401.278234	8.100429
6.128210	399.539608	8.105446
6.357615	393.864775	8.110464
6.429549	398.164207	8.115482
6.385997	400.701837	8.120499
6.467866	388.549349	8.125517
6.465044	400.882067	8.130534
6.262826	401.891823	8.135552
6.270069	399.650209	8.140570
6.736863	401.549831	8.145587
6.574075	400.634816	8.150605
6.315188	396.800013	8.155622
6.753612	397.094673	8.160640
6.731118	397.265446	8.165658
6.772302	401.301436	8.170675
6.593041	393.796845	8.175693
6.364935	403.198335	8.180710
6.647235	401.797476	8.185728
6.501772	399.784755	8.190746
6.313269	406.276888	8.195763
6.404160	398.521960	8.200781
6.399048	403.679101	8.205798
6.732630	390.114716	8.210816
6.687426	394.460785	8.215834
6.677029	402.067530	8.220851
6.946848	390.365435	8.225869
6.651342	398.859126	8.230886
6.874500	398.840180	8.235904
6.833545	410.714963	8.240922
7.049341	395.073563	8.245939
6.802270	389.618077	8.250957
6.315237	384.726946	8.255974
6.210345	376.800549	8.260992
6.924657	389.308767	8.266010
6.509133	393.778763	8.271027
6.741818	390.306060	8.276045
6.442387	388.484561	8.281062
7.001474	387.453998	8.286080
6.909129	381.362229	8.291098
6.456285	376.692984	8.296115
6.455689	369.614997	8.301133
6.588743	377.123660	8.306150
6.817888	383.724319	8.311168
6.664639	380.614649	8.316186
6.679870	387.403241	8.321203
7.031885	379.074361	8.326221
6.626211	378.373880	8.331238
6.332349	379.946985	8.336256
6.801143	385.326967	8.341274
6.515748	398.814465	8.346291
6.988524	388.109513	8.351309
6.742672	397.311802	8.356326
6.712235	387.297394	8.361344
6.812564	387.594204	8.366362
6.475429	389.158269	8.371379
6.491475	385.981216	8.376397
6.593165	398.300815	8.381414
6.679284	401.585078	8.386432
6.806430	400.179975	8.391450
6.468397	397.771224	8.396467
6.597128	395.759991	8.401485
6.978758	401.932993	8.406502
6.809762	401.893058	8.411520
6.874370	393.274422	8.416538
7.023225	396.965460	8.421555
6.729307	399.289619	8.426573
6.518785	404.084288	8.431590
6.689937	400.365556	8.436608
6.713129	398.926148	8.441626
6.734244	394.587027	8.446643
6.752643	401.876879	8.451661
6.621712	400.508802	8.456678
6.905181	395.059069	8.461696
6.911457	400.949702	8.466714
6.904793	400.023002	8.471731
6.389758	394.287360	8.476749
6.523351	402.001066	8.481766
6.550815	399.282957	8.486784
6.922052	405.296640	8.491802
6.905703	416.902522	8.496819
6.950934	408.141735	8.501837
6.637933	414.438671	8.506854
6.974798	421.663169	8.511872
7.028135	414.857620	8.516890
6.874741	420.372352	8.521907
6.730047	416.396696	8.526925
6.861313	426.199815	8.531942
6.880070	432.987875	8.536960
6.854037	431.903251	8.541978
7.178968	431.581296	8.546995
7.393293	424.012255	8.552013
6.877113	413.937768	8.557030
6.826570	410.155726	8.562048
6.916565	404.404771	8.567066
6.669784	416.106486	8.572083
7.128670	420.572883	8.577101
7.237163	435.958741	8.582119
6.768938	416.529748	8.587136
7.200029	413.540521	8.592154
6.945894	414.091325	8.597171
6.794410	415.787426	8.602189
6.887445	423.617904	8.607207
6.954900	425.762732	8.612224
7.277319	434.952299	8.617242
6.971092	436.249637	8.622259
6.807305	426.432685	8.627277
6.933714	432.273068	8.632295
7.065356	429.996303	8.637312
7.110292	421.614234	8.642330
6.512373	432.474427	8.647347
6.641142	437.866342	8.652365
6.744049	432.580403	8.657383
6.529420	434.261092	8.662400
6.720838	436.386620	8.667418
6.838429	434.001595	8.672435
6.896560	450.307289	8.677453
7.217139	451.421834	8.682471
7.422842	457.464464	8.687488
7.156494	440.765211	8.692506
6.883655	445.168825	8.697523
7.146407	435.421151	8.702541
7.143840	447.671815	8.707559
7.183837	449.593714	8.712576
7.220998	440.304018	8.717594
6.797413	444.223042	8.722611
7.133645	448.440312	8.727629
7.288129	450.918715	8.732647
7.379784	456.168098	8.737664
7.224182	439.811349	8.742682
7.018885	432.657916	8.747699
7.063312	429.353365	8.752717
7.257317	440.412140	8.757735
6.819001	443.872732	8.762752
7.250198	450.931083	8.767770
7.216963	455.701318	8.772787
7.360877	450.680376	8.777805
7.463927	446.177013	8.782823
7.125087	440.890427	8.787840
7.278618	426.252724	8.792858
7.002626	438.031582	8.797875
7.273355	446.310908	8.802893
7.668810	448.985310	8.807911
6.907575	444.531311	8.812928
7.085500	434.534926	8.817946
7.457970	445.351333	8.822963
7.371228	444.935691	8.827981
6.977899	441.128122	8.832999
7.230474	451.947422	8.838016
7.407402	442.449780	8.843034
7.533647	453.746320	8.848051
7.261189	447.130332	8.853069
7.255117	439.889076	8.858087
7.010822	440.848584	8.863104
7.378161	441.624504	8.868122
7.431277	454.494478	8.873139
7.270189	448.896205	8.878157
7.318763	450.548538	8.883175
7.203260	452.731322	8.888192
7.372694	448.602612	8.893210
7.580383	453.878108	8.898227
7.212382	441.088761	8.903245
7.509882	438.142418	8.908263
7.270713	437.182492	8.913280
7.610595	433.033559	8.918298
7.036132	432.454025	8.923315
7.117785	433.343850	8.928333
7.217266	437.260324	8.933351
7.384621	451.396859	8.938368
7.969728	453.255976	8.943386
7.530558	455.858366	8.948403
7.062257	447.265874	8.953421
7.543924	450.838837	8.958439
7.489865	444.469700	8.963456
7.481370	445.922645	8.968474
7.391206	442.519132	8.973491
7.550964	448.982303	8.978509
7.314322	447.027952	8.983527
7.454694	446.741043	8.988544
7.918838	435.138045	8.993562
7.666463	431.526273	8.998579
7.247315	425.927162	9.003597
7.510993	431.638880	9.008615
7.191116	429.246232	9.013632
7.507663	427.953642	9.018650
7.166829	434.349588	9.023667
7.286938	453.002907	9.028685
7.596769	450.824622	9.033703
7.795779	461.276745	9.038720
7.742450	448.318484	9.043738
7.338482	442.707537	9.048755
7.451794	457.859146	9.053773
7.745278	452.044936	9.058791
7.331270	445.141734	9.063808
7.818538	448.840051	9.068826
7.655411	438.985121	9.073843
7.260297	434.900135	9.078861
7.450159	446.764249	9.083879
7.294504	456.160799	9.088896
7.662453	459.350701	9.093914
7.637463	452.333281	9.098931
7.462699	454.424311	9.103949
7.540497	457.896063	9.108967
7.603946	451.382401	9.113984
7.701119	452.863073	9.119002
7.826214	449.362932	9.124019
7.357750	448.362969	9.129037
7.842297	445.750403	9.134055
7.594446	444.842318	9.139072
7.472017	449.336118	9.144090
7.673664	454.300145	9.149107
7.586000	451.025624	9.154125
7.455117	453.621037	9.159143
7.417965	465.583622	9.164160
7.329433	451.438002	9.169178
7.636429	457.067248	9.174195
7.575433	455.382180	9.179213
7.564319	447.968145	9.184231
7.539166	455.166974	9.189248
7.761860	449.881314	9.194266
7.433339	452.166688	9.199283
7.388333	454.404765	9.204301
7.676211	456.597324	9.209319
7.327558	459.393894	9.214336
7.701722	467.038617	9.219354
7.867528	472.945459	9.224371
7.885328	477.373254	9.229389
8.122452	471.012417	9.234407
7.533868	462.126235	9.239424
7.829208	456.447428	9.244442
7.751598	456.147124	9.249459
7.489162	465.389898	9.254477
8.024851	465.641014	9.259495
7.932436	466.952400	9.264512
7.955048	457.911101	9.269530
7.667057	452.225293	9.274547
7.395803	459.869521	9.279565
8.231388	463.646147	9.284583
7.715448	475.314072	9.289600
7.785886	471.494248	9.294618
8.093493	466.712890	9.299635
7.866782	461.566622	9.304653
7.928925	452.323521	9.309671
7.552119	445.174697	9.314688
7.963486	460.693292	9.319706
7.887958	458.152148	9.324723
7.803645	461.639673	9.329741
8.295655	466.757301	9.334759
8.104671	461.750631	9.339776
8.015980	456.043258	9.344794
7.943381	448.285362	9.349811
7.844954	453.072057	9.354829
7.868688	449.480404	9.359847
7.833875	449.072456	9.364864
7.863259	447.000949	9.369882
7.739499	447.746040	9.374899
7.374121	452.362870	9.379917
7.885275	458.086556	9.384935
7.941190	477.753394	9.389952
7.818979	477.750354	9.394970
8.038639	474.686743	9.399987
7.871697	478.016731	9.405005
7.862444	476.497166	9.410023
7.942028	481.953554	9.415040
8.265601	482.856205	9.420058
8.285150	480.581108	9.425075
8.080236	478.643903	9.430093
8.079801	475.516735	9.435111
8.220457	484.065627	9.440128
8.052472	478.796607	9.445146
7.815173	467.470050	9.450163
7.777544	474.617184	9.455181
8.225903	472.145942	9.460199
7.895836	480.941684	9.465216
7.962090	474.373931	9.470234
8.295739	474.359872	9.475251
8.057222	475.084963	9.480269
8.404782	478.237020	9.485287
8.178516	479.894280	9.490304
8.084945	476.892060	9.495322
8.034780	466.369462	9.500339
7.391881	472.080340	9.505357
7.888008	475.158774	9.510375
8.049139	482.508483	9.515392
7.932926	483.331292	9.520410
7.687053	484.666572	9.525427
7.798108	483.601623	9.530445
8.125156	485.245314	9.535463
8.005036	474.007802	9.540480
8.071102	476.793450	9.545498
8.151648	476.692573	9.550515
7.843001	483.679944	9.555533
8.229077	487.163662	9.560551
8.265267	493.280031	9.565568
8.398749	499.081467	9.570586
8.312228	498.864596	9.575603
7.904754	493.850599	9.580621
8.307824	507.158408	9.585639
8.575521	505.261220	9.590656
8.157090	490.103474	9.595674
8.422102	482.892574	9.600691
7.988160	481.445442	9.605709
8.182944	488.382834	9.610727
8.298485	493.092047	9.615744
8.172808	486.557328	9.620762
8.375004	484.439977	9.625779
7.961217	493.763133	9.630797
8.596293	496.775758	9.635815
8.413336	488.325003	9.640832
8.144575	489.057959	9.645850
8.540611	486.727399	9.650867
8.441600	490.759993	9.655885
8.468744	474.576721	9.660903
8.354517	481.044694	9.665920
8.391928	473.178145	9.670938
8.332106	471.070034	9.675955
8.124616	471.291701	9.680973
8.338550	470.277004	9.685991
8.294822	472.309766	9.691008
8.641336	475.417806	9.696026
8.590666	477.656768	9.701043
8.376624	482.647655	9.706061
8.489744	478.950566	9.711079
8.484737	478.768339	9.716096
8.205099	483.090973	9.721114
8.566389	482.290007	9.726131
8.171107	480.890503	9.731149
8.524721	472.147940	9.736167
8.454347	477.248995	9.741184
8.196235	483.613145	9.746202
8.553568	485.170074	9.751219
8.249624	476.766562	9.756237
8.431045	471.749242	9.761255
8.409625	480.029890	9.766272
8.226254	479.673472	9.771290
8.702427	495.308233	9.776307
8.762526	497.634088	9.781325
8.085723	482.242034	9.786343
8.427134	491.065772	9.791360
8.308412	502.463596	9.796378
8.675768	506.628700	9.801395
8.270413	512.977917	9.806413
8.277874	505.813419	9.811431
8.566511	503.925593	9.816448
8.585971	509.309303	9.821466
8.602302	510.262949	9.826483
8.662464	509.470998	9.831501
8.654804	498.140225	9.836519
8.423144	503.316890	9.841536
8.439800	510.461898	9.846554
8.761384	500.809165	9.851571
8.518533	513.409696	9.856589
8.548909	506.790715	9.861607
8.718567	506.278349	9.866624
8.755367	508.610989	9.871642
8.577343	507.603670	9.876659
8.609010	509.302820	9.881677
8.886590	500.464789	9.886695
8.884691	500.051714	9.891712
8.703789	509.502713	9.896730
8.809238	502.553323	9.901747
8.719827	507.474323	9.906765
8.498953	511.383890	9.911783
8.589470	509.719405	9.916800
8.457621	497.574873	9.921818
8.643674	499.748579	9.926835
8.777878	502.608826	9.931853
8.591014	504.108481	9.936871
9.037939	497.456205	9.941888
8.869033	503.004935	9.946906
8.575351	499.936042	9.951923
8.703079	501.001725	9.956941
8.506980	503.446361	9.961959
8.596061	503.587140	9.966976
8.804220	510.490902	9.971994
8.598737	505.628481	9.977011
8.408702	503.212451	9.982029
8.771613	510.499199	9.987047
8.902804	509.768770	9.992064
8.755834	509.700160	9.997082
8.875169	503.616416	10.002099
8.644701	504.700001	10.007117
8.561440	511.425083	10.012135
8.729960	515.539100	10.017152
8.622867	510.090183	10.022170
8.542456	508.338708	10.027187
8.975684	514.333310	10.032205
9.018805	519.624981	10.037223
9.235309	508.985102	10.042240
8.816858	511.603208	10.047258
9.021537	503.025823	10.052275
8.949308	507.350883	10.057293
8.761799	512.918290	10.062311
8.888683	508.834060	10.067328
8.699462	522.098404	10.072346
8.962363	510.561403	10.077363
9.200609	509.224197	10.082381
8.833764	509.076217	10.087399
8.929860	506.514655	10.092416
9.065024	511.302865	10.097434
8.786666	512.633737	10.102451
9.063187	506.342490	10.107469
8.827712	504.615158	10.112487
9.181560	508.230124	10.117504
8.734365	512.771349	10.122522
8.940823	507.475577	10.127539
8.921693	503.268922	10.132557
8.698214	509.608755	10.137575
8.787170	520.898520	10.142592
8.933498	532.210917	10.147610
9.094185	533.612282	10.152627
9.383914	535.526864	10.157645
9.020615	534.911293	10.162663
9.354293	537.405987	10.167680
8.991634	539.144445	10.172698
9.259116	539.175401	10.177715
9.215253	512.627311	10.182733
8.910640	509.194062	10.187751
9.153521	517.392554	10.192768
9.167481	528.432080	10.197786
8.944831	518.794648	10.202803
9.143472	524.645905	10.207821
9.157460	523.447751	10.212839
9.109500	519.412830	10.217856
8.918291	524.258170	10.222874
8.944736	524.219362	10.227891
9.551290	518.886539	10.232909
9.497009	527.279618	10.237927
9.214311	519.765833	10.242944
9.155560	518.717853	10.247962
8.959236	511.995318	10.252979
9.338791	513.349982	10.257997
9.320648	527.474436	10.263015
9.266018	518.826969	10.268032
9.167977	510.659614	10.273050
9.129040	520.634446	10.278067
9.414844	521.637650	10.283085
9.229975	519.145078	10.288103
9.258986	518.036099	10.293120
9.079408	522.699754	10.298138
9.098241	525.704195	10.303155
9.763951	515.969473	10.308173
9.285058	519.789832	10.313191
9.084906	514.737239	10.318208
9.092880	526.850623	10.323226
9.650992	527.786185	10.328243
9.673235	526.533099	10.333261
9.111004	523.278806	10.338279
9.255510	511.520407	10.343296
8.881654	513.853872	10.348314
9.142631	520.910352	10.353331
9.082448	523.368542	10.358349
9.059677	534.353833	10.363367
9.351286	531.651379	10.368384
9.413780	530.896933	10.373402
9.461023	532.432721	10.378419
9.687856	517.591035	10.383437
9.195021	524.932133	10.388455
9.546361	517.748802	10.393472
9.367290	522.680610	10.398490
9.408556	520.783962	10.403507
9.307202	525.653180	10.408525
9.314409	526.904879	10.413543
9.422188	518.714943	10.418560
9.056339	526.834655	10.423578
9.113258	523.124217	10.428595
9.504200	527.566507	10.433613
9.403294	533.890420	10.438631
9.649443	525.297101	10.443648
9.287924	537.578469	10.448666
9.438374	528.252155	10.453683
9.822534	525.954996	10.458701
9.428274	531.267434	10.463719
9.860902	533.125055	10.468736
9.792545	527.780550	10.473754
9.619070	529.641024	10.478771
9.903005	529.252870	10.483789
9.627793	524.505438	10.488807
9.445009	515.704364	10.493824
9.556175	523.181785	10.498842
9.494042	529.326098	10.503859
9.697130	516.239506	10.508877
9.677973	525.551726	10.513895
9.587169	520.434771	10.518912
9.751640	530.084461	10.523930
9.311657	528.960144	10.528947
9.325225	526.039061	10.533965
9.403109	535.108969	10.538983
9.616401	527.259192	10.544000
9.526765	532.631494	10.549018
9.532635	541.043616	10.554035
9.915726	543.877741	10.559053
9.859403	543.318511	10.564071
9.708501	526.320349	10.569088
9.605479	530.893196	10.574106
9.406581	532.735538	10.579123
9.840307	541.585952	10.584141
9.581896	539.994726	10.589159
9.583333	551.932427	10.594176
9.923908	548.540722	10.599194
9.874266	551.076166	10.604211
10.024133	541.847761	10.609229
9.894810	543.455220	10.614247
10.043670	545.003588	10.619264
9.879830	534.646966	10.624282
9.387258	531.627968	10.629299
9.831105	534.127598	10.634317
9.767217	541.430319	10.639335
9.935494	545.818924	10.644352
10.376746	538.978175	10.649370
9.754301	534.114397	10.654387
9.774847	531.769714	10.659405
9.303227	534.506550	10.664423
9.810287	547.570989	10.669440
10.087715	543.314996	10.674458
9.802263	551.352777	10.679475
9.835548	533.786310	10.684493
9.834247	543.932012	10.689511
9.695753	541.015668	10.694528
10.059376	541.539718	10.699546
9.526721	540.893712	10.704563
10.243580	548.759657	10.709581
9.753673	549.173613	10.714599
9.507994	548.833205	10.719616
9.760417	540.087430	10.724634
9.791506	546.362395	10.729651
9.807369	549.108537	10.734669
9.840384	552.599902	10.739687
10.038411	550.489504	10.744704
9.760195	542.987633	10.749722
10.007675	549.042724	10.754739
9.937471	543.973045	10.759757
10.161895	551.047852	10.764775
9.958945	551.376106	10.769792
10.126127	554.963342	10.774810
10.018779	556.860859	10.779827
9.977495	555.074886	10.784845
10.077447	562.326861	10.789863
10.388797	566.308202	10.794880
10.103840	553.906614	10.799898
10.117671	552.809464	10.804915
10.234105	546.331698	10.809933
10.028951	541.879453	10.814951
10.168290	545.584627	10.819968
10.152274	538.142916	10.824986
10.221664	545.396487	10.830003
10.313033	540.320587	10.835021
10.238055	551.209880	10.840039
10.122421	546.598536	10.845056
10.231251	552.978159	10.850074
10.095200	544.318111	10.855091
9.579551	543.000456	10.860109
9.842118	558.848404	10.865127
10.213287	558.172124	10.870144
10.356335	566.641792	10.875162
10.117291	576.966534	10.880179
10.346390	568.921781	10.885197
10.414003	575.026975	10.890215
10.405176	583.555010	10.895232
10.231187	578.107021	10.900250
10.158116	579.626833	10.905267
10.385789	576.142252	10.910285
10.286155	567.741600	10.915303
10.340895	577.152790	10.920320
10.468757	572.181648	10.925338
10.222831	577.035521	10.930355
10.489112	565.794592	10.935373
10.469725	574.497828	10.940391
10.238244	579.314741	10.945408
10.547396	575.725959	10.950426
10.642351	578.866873	10.955443
10.152476	570.877259	10.960461
10.546899	565.583761	10.965479
9.944068	573.210238	10.970496
10.279486	562.182599	10.975514
10.021298	569.761726	10.980531
10.040828	569.660881	10.985549
10.543727	573.315767	10.990567
10.034079	566.616748	10.995584
10.387531	570.601003	11.000602
10.320550	566.351292	11.005619
10.349442	568.899756	11.010637
10.529705	567.697800	11.015655
10.121487	578.055194	11.020672
10.370318	577.991228	11.025690
10.711374	591.166750	11.030707
10.255026	577.245548	11.035725
10.297605	593.026797	11.040743
10.306276	594.555973	11.045760
10.734324	593.394328	11.050778
10.750729	604.887939	11.055795
10.596699	600.127931	11.060813
10.878715	614.694850	11.065831
10.610177	604.288218	11.070848
10.812983	592.195654	11.075866
10.407864	582.248940	11.080883
10.588146	583.786108	11.085901
10.609116	588.071431	11.090919
10.813378	596.575762	11.095936
10.477005	584.418834	11.100954
10.469351	589.532246	11.105971
10.706119	597.993649	11.110989
10.855276	599.377881	11.116007
10.601535	608.319585	11.121024
11.271898	595.059200	11.126042
10.821477	583.601657	11.131059
10.621861	575.551069	11.136077
10.617708	573.235471	11.141095
10.482420	569.889451	11.146112
10.530726	575.284468	11.151130
10.315013	581.903973	11.156147
10.588105	588.671428	11.161165
11.014388	597.024431	11.166183
10.661839	594.138250	11.171200
10.412394	595.344711	11.176218
10.746534	600.553227	11.181235
10.901522	599.677084	11.186253
10.796640	603.265666	11.191271
10.511789	607.320909	11.196288
10.968534	598.136210	11.201306
10.824742	602.393543	11.206323
10.747161	601.604100	11.211341
10.915508	603.932049	11.216359
10.768108	602.582299	11.221376
11.082114	597.408606	11.226394
10.805343	597.483277	11.231411
10.919832	605.370453	11.236429
11.117056	599.953020	11.241447
10.664614	601.727553	11.246464
10.718159	603.483263	11.251482
10.798513	599.494616	11.256499
10.818015	604.152542	11.261517
10.953953	595.213446	11.266535
10.764436	609.068012	11.271552
10.824906	606.590876	11.276570
10.898422	604.095930	11.281587
10.716569	600.271179	11.286605
10.888096	605.000106	11.291623
10.729206	623.425654	11.296640
10.786812	618.982970	11.301658
10.913219	629.320268	11.306675
10.804727	628.374697	11.311693
11.293064	626.105485	11.316711
10.974290	629.402339	11.321728
11.116547	630.052373	11.326746
11.415279	622.728873	11.331763
11.011683	629.608013	11.336781
11.203697	626.277291	11.341799
10.792206	631.422034	11.346816
11.136454	620.904206	11.351834
11.359104	630.888862	11.356851
11.052030	633.224566	11.361869
11.601047	627.143305	11.366887
11.171963	630.072340	11.371904
11.276311	634.303669	11.376922
11.333595	629.864188	11.381939
11.248899	625.566730	11.386957
11.458173	624.903032	11.391975
11.051537	615.208990	11.396992
11.164351	615.544883	11.402010
11.052289	620.030801	11.407027
11.153890	629.756603	11.412045
11.547040	628.508874	11.417063
11.064053	636.659497	11.422080
11.230822	627.822877	11.427098
11.592528	628.126330	11.432115
11.278439	633.164394	11.437133
11.278001	627.051920	11.442151
11.030962	637.548349	11.447168
11.024359	627.523784	11.452186
11.612855	632.885203	11.457203
11.130642	637.779038	11.462221
11.476690	620.883286	11.467239
11.210070	625.446916	11.472256
11.151724	629.359604	11.477274
11.312833	634.408885	11.482291
11.303901	627.972698	11.487309
11.458103	619.908026	11.492327
11.097523	635.218772	11.497344
11.159487	630.822742	11.502362
11.452705	631.963649	11.507379
10.930859	633.199901	11.512397
11.624942	624.224380	11.517415
11.346759	633.532806	11.522432
11.332719	626.627218	11.527450
11.528330	633.413065	11.532467
11.235038	629.129150	11.537485
11.449965	629.982456	11.542503
11.291590	625.791140	11.547520
11.340038	627.055359	11.552538
11.954584	638.023534	11.557555
11.308949	633.579890	11.562573
11.603640	640.536499	11.567591
11.452669	651.885793	11.572608
11.610128	647.137232	11.577626
11.737315	650.143757	11.582643
11.538670	643.569850	11.587661
11.562625	627.566810	11.592679
11.347078	640.049574	11.597696
12.056103	649.065454	11.602714
12.083931	643.485041	11.607731
11.816701	634.520338	11.612749
11.972074	635.013701	11.617767
11.771493	633.164163	11.622784
11.640482	627.245582	11.627802
11.622030	630.019168	11.632819
11.482811	625.556637	11.637837
11.468939	626.221512	11.642855
11.317390	631.032304	11.647872
11.348767	632.030949	11.652890
11.912890	644.679492	11.657907
11.424820	659.148605	11.662925
11.957253	659.094130	11.667943
11.824301	661.118716	11.672960
11.971514	652.714303	11.677978
12.126622	646.255724	11.682995
11.570428	639.459787	11.688013
11.493443	628.502629	11.693031
11.718124	639.982769	11.698048
11.958701	646.600680	11.703066
12.139009	642.104173	11.708083
11.681604	656.151959	11.713101
12.008725	650.184130	11.718119
11.938616	656.036250	11.723136
11.700428	654.814236	11.728154
11.943874	658.897686	11.733171
11.717408	655.389127	11.738189
12.169265	651.497255	11.743207
11.839996	655.262790	11.748224
11.943497	655.420260	11.753242
11.829990	652.534719	11.758259
11.683418	659.146643	11.763277
11.947828	655.283956	11.768295
12.224539	660.801221	11.773312
11.965721	658.307520	11.778330
12.088472	652.876421	11.783347
11.844982	659.692776	11.788365
12.150748	648.776994	11.793383
12.201044	652.757977	11.798400
11.888540	648.426557	11.803418
12.242971	653.022881	11.808435
11.804661	651.746822	11.813453
11.802176	659.346133	11.818471
11.789411	655.233122	11.823488
11.762973	655.597008	11.828506
12.112483	652.083976	11.833523
11.589093	656.192148	11.838541
11.997726	649.198652	11.843559
11.576264	656.544470	11.848576
11.670882	661.856567	11.853594
12.264825	665.733974	11.858611
12.031664	679.888870	11.863629
12.265586	668.826477	11.868647
12.187742	683.096044	11.873664
12.081627	679.534029	11.878682
12.067657	678.258170	11.883699
12.266486	677.753880	11.888717
12.077022	676.325470	11.893735
12.303997	679.584697	11.898752
11.974932	679.736935	11.903770
12.201373	668.035102	11.908787
12.330493	672.521349	11.913805
12.213758	679.725061	11.918823
12.337477	670.008374	11.923840
12.461229	677.534391	11.928858
12.363094	678.742544	11.933875
12.152342	681.419851	11.938893
12.264274	667.492148	11.943911
12.266533	677.356515	11.948928
12.186324	674.342714	11.953946
12.296577	677.452863	11.958963
12.325091	678.833794	11.963981
12.543275	675.738822	11.968999
12.486440	672.995928	11.974016
12.218295	678.683235	11.979034
12.454532	675.815818	11.984051
12.329217	673.250837	11.989069
12.338455	671.722065	11.994087
12.119988	675.511377	11.999104
12.164597	685.094609	12.004122
12.529669	692.560970	12.009139
12.751629	705.852946	12.014157
13.029221	694.651199	12.019175
12.729052	674.195402	12.024192
12.449079	672.976737	12.029210
12.798494	666.020856	12.034227
12.736406	678.271478	12.039245
12.564852	666.669480	12.044263
12.390673	661.171005	12.049280
12.728037	669.768252	12.054298
12.500337	667.657855	12.059315
12.387559	669.086030	12.064333
12.397725	674.890944	12.069351
12.666513	666.764231	12.074368
12.428093	668.568562	12.079386
12.660547	674.121123	12.084403
12.743285	679.684375	12.089421
12.738246	685.551618	12.094439
12.952096	671.892055	12.099456
12.518193	667.784652	12.104474
13.293185	669.901397	12.109491
12.593935	672.228741	12.114509
12.733864	673.049546	12.119527
12.551077	665.532766	12.124544
12.223341	673.924311	12.129562
12.833728	684.669108	12.134579
12.610489	705.907018	12.139597
12.792257	698.065230	12.144615
12.841741	707.303744	12.149632
12.456244	695.504671	12.154650
13.100438	693.561467	12.159667
13.008844	701.562820	12.164685
13.012178	695.601210	12.169703
13.173262	686.169019	12.174720
13.236565	670.762552	12.179738
13.039820	661.452357	12.184755
12.896245	669.761580	12.189773
12.461324	672.603171	12.194791
12.769093	659.178295	12.199808
13.103233	678.073071	12.204826
12.543513	669.134956	12.209843
12.918752	681.273311	12.214861
12.984570	687.552386	12.219879
12.876721	685.745207	12.224896
12.911504	688.052938	12.229914
12.971439	684.512404	12.234931
13.054349	694.219062	12.239949
13.277360	697.289568	12.244967
13.139596	696.967068	12.249984
13.258819	693.890656	12.255002
13.488568	683.485289	12.260019
13.312704	680.072984	12.265037
12.531447	679.926411	12.270055
12.857587	673.359145	12.275072
12.580992	681.625971	12.280090
12.950867	684.831393	12.285107
13.218814	693.988551	12.290125
13.222049	699.336977	12.295143
13.549082	696.329191	12.300160
13.161315	695.906765	12.305178
12.910434	687.154077	12.310195
13.121157	694.281565	12.315213
12.998403	695.569290	12.320231
13.083540	690.992918	12.325248
13.147227	687.641141	12.330266
12.608511	690.763974	12.335283
12.699651	695.981952	12.340301
12.887650	699.187293	12.345319
13.437584	698.334857	12.350336
13.523378	711.465007	12.355354
13.289650	702.387760	12.360371
13.241528	694.613322	12.365389
13.377100	686.409515	12.370407
13.646696	697.185290	12.375424
13.226522	698.954808	12.380442
13.819684	694.999902	12.385459
13.342947	692.136196	12.390477
12.709507	697.700510	12.395495
13.494033	686.094803	12.400512
13.498872	701.058387	12.405530
13.222102	693.859174	12.410547
13.331122	698.578924	12.415565
13.386081	713.967046	12.420583
13.475822	705.098201	12.425600
13.579165	722.454264	12.430618
13.347227	723.474977	12.435635
13.897372	723.057994	12.440653
13.508823	714.579183	12.445671
13.281280	699.116992	12.450688
13.664025	713.557861	12.455706
13.801477	714.631509	12.460723
13.689525	701.369778	12.465741
13.248207	701.400642	12.470759
13.588501	696.876057	12.475776
13.411344	703.530628	12.480794
13.555427	716.134172	12.485811
13.639688	717.796752	12.490829
13.565945	720.017246	12.495847
13.654228	717.056097	12.500864
13.953919	716.372006	12.505882
13.881404	716.134018	12.510899
13.652403	694.395370	12.515917
13.333747	702.577238	12.520935
13.901628	704.943977	12.525952
13.436155	707.976517	12.530970
13.710949	719.041820	12.535987
13.979367	715.932708	12.541005
13.783873	725.919407	12.546023
14.030191	711.869763	12.551040
13.352588	707.443700	12.556058
13.400529	706.732536	12.561075
13.582058	713.261839	12.566093
13.522022	725.467995	12.571111
13.594330	725.819664	12.576128
13.670563	716.182926	12.581146
13.420095	720.280176	12.586163
13.702869	713.890056	12.591181
13.404989	724.760513	12.596199
13.957537	721.888020	12.601216
13.400226	735.695811	12.606234
13.869095	742.028913	12.611251
13.664652	749.609215	12.616269
13.847542	746.365096	12.621287
13.946499	747.488920	12.626304
14.129675	759.060803	12.631322
14.111017	752.200065	12.636339
13.902071	745.062853	12.641357
14.038672	761.517556	12.646375
14.337171	751.464351	12.651392
14.310130	752.393205	12.656410
14.039645	754.420281	12.661427
14.335931	749.432334	12.666445
13.864439	748.899869	12.671463
14.398935	733.192774	12.676480
13.881726	733.475288	12.681498
13.876033	739.367897	12.686515
14.247622	738.723102	12.691533
13.867806	750.177514	12.696551
14.270571	745.741017	12.701568
13.817344	745.224643	12.706586
13.798860	740.793776	12.711603
14.537065	742.761628	12.716621
14.560984	744.143280	12.721639
14.639088	745.939361	12.726656
14.333327	751.837669	12.731674
13.948441	734.749510	12.736691
14.349661	739.385908	12.741709
14.101792	750.895514	12.746727
14.264526	748.424525	12.751744
14.327140	747.859394	12.756762
14.112235	753.708843	12.761779
14.182970	749.298796	12.766797
14.114484	751.903472	12.771815
14.050771	747.312392	12.776832
14.225374	753.375744	12.781850
14.240158	757.854569	12.786867
14.304152	751.110346	12.791885
14.236317	749.634592	12.796903
14.578546	744.876171	12.801920
14.384540	751.457646	12.806938
14.137669	754.771729	12.811955
14.381780	752.830851	12.816973
14.255631	753.642597	12.821991
14.311101	755.183434	12.827008
14.272085	756.767385	12.832026
14.093740	758.742246	12.837043
14.471091	761.962297	12.842061
14.768827	768.823811	12.847079
15.117640	777.614982	12.852096
14.747830	768.842902	12.857114
14.574596	758.244622	12.862131
14.602323	752.436979	12.867149
14.245288	757.655328	12.872167
14.095902	754.500810	12.877184
14.108423	760.939683	12.882202
14.750439	761.868507	12.887219
14.836943	767.169275	12.892237
14.579087	772.148131	12.897255
14.464430	773.699680	12.902272
14.634806	769.409809	12.907290
14.554104	775.929472	12.912307
14.885997	769.402300	12.917325
14.617394	774.076726	12.922343
14.409022	772.843750	12.927360
14.715272	769.728738	12.932378
14.657053	776.377441	12.937395
14.545649	772.917213	12.942413
14.892038	768.603094	12.947431
14.952887	763.235246	12.952448
14.822513	769.074696	12.957466
14.498365	774.130143	12.962483
14.901068	760.630452	12.967501
14.709405	770.004371	12.972519
14.722130	775.395522	12.977536
14.798051	768.094031	12.982554
14.632246	771.275578	12.987571
15.005498	771.154372	12.992589
14.732358	772.506540	12.997607
15.024238	765.859371	13.002624
14.884353	768.068079	13.007642
14.671477	782.469199	13.012659
15.318276	790.718535	13.017677
15.097772	787.461478	13.022695
14.865845	783.325757	13.027712
15.034045	773.557907	13.032730
14.818321	772.922506	13.037747
15.005198	782.010283	13.042765
15.025231	796.078514	13.047783
14.977060	798.446511	13.052800
15.261008	793.346867	13.057818
14.961027	803.498196	13.062835
15.434589	796.390395	13.067853
15.236191	800.214477	13.072871
14.755250	799.980119	13.077888
15.048836	798.899356	13.082906
14.729296	800.722641	13.087923
14.933503	800.154396	13.092941
14.935688	803.114139	13.097959
14.805650	801.657532	13.102976
15.174724	802.199676	13.107994
15.109783	802.844108	13.113011
15.180724	802.082024	13.118029
14.904953	799.076560	13.123047
15.428957	810.772132	13.128064
15.460291	799.460341	13.133082
15.115649	805.535129	13.138099
15.361627	792.596287	13.143117
15.467427	793.715893	13.148135
15.363440	793.372354	13.153152
15.772813	796.884063	13.158170
15.222503	803.091854	13.163187
15.571559	799.430546	13.168205
15.375198	792.338691	13.173223
15.039302	796.310408	13.178240
15.249116	797.994471	13.183258
15.177089	799.558320	13.188275
15.392876	803.403119	13.193293
15.739892	810.660908	13.198311
15.972514	812.467651	13.203328
15.666670	801.855279	13.208346
15.676921	805.567983	13.213363
15.553606	793.655442	13.218381
15.613349	791.781135	13.223399
15.543918	797.557458	13.228416
15.478314	789.908774	13.233434
15.232920	791.976126	13.238451
15.254961	796.046744	13.243469
15.546952	799.652467	13.248487
15.828844	806.147243	13.253504
15.773568	805.199689	13.258522
15.472998	803.703363	13.263539
15.596243	797.502148	13.268557
15.508454	802.378796	13.273575
15.651249	815.209822	13.278592
15.906485	816.243049	13.283610
15.574058	820.753860	13.288627
15.861974	817.979357	13.293645
15.803236	814.551946	13.298663
15.623350	825.375691	13.303680
15.702902	812.522705	13.308698
15.928769	809.458071	13.313715
16.151191	816.063093	13.318733
16.111650	818.268807	13.323751
15.802126	811.383907	13.328768
15.945004	796.479323	13.333786
15.703015	796.223540	13.338803
15.750119	802.742248	13.343821
16.262183	809.040247	13.348839
16.015130	815.065131	13.353856
15.895208	791.450663	13.358874
16.144332	791.670666	13.363891
15.910738	787.661432	13.368909
16.365443	794.122986	13.373927
15.720882	794.554714	13.378944
16.004544	793.447094	13.383962
15.941385	793.946085	13.388979
16.065247	790.357709	13.393997
16.223102	791.664864	13.399015
16.009422	794.632970	13.404032
15.769288	789.384558	13.409050
15.903922	802.295738	13.414067
15.897014	814.250693	13.419085
15.755645	810.021973	13.424103
15.655829	816.939091	13.429120
15.973824	811.070458	13.434138
15.698376	822.379282	13.439155
15.959548	815.172002	13.444173
15.975540	818.303162	13.449191
15.803308	819.589131	13.454208
16.228200	830.321874	13.459226
16.181063	832.759140	13.464243
16.009018	846.494409	13.469261
16.513515	839.075670	13.474279
16.314503	842.843053	13.479296
16.501939	841.838773	13.484314
16.414270	840.918350	13.489331
16.445589	837.117161	13.494349
16.468824	834.311284	13.499367
15.982212	840.711137	13.504384
16.041993	846.454735	13.509402
16.840794	839.880087	13.514419
16.588978	849.017267	13.519437
16.565373	841.365178	13.524455
16.378622	840.911450	13.529472
16.591699	835.646108	13.534490
16.251034	832.265745	13.539507
16.283718	834.927263	13.544525
16.460903	842.883676	13.549543
16.407952	837.284222	13.554560
16.373452	838.384651	13.559578
16.570562	842.611054	13.564595
16.637601	840.464213	13.569613
16.575361	839.337865	13.574631
16.272565	845.923689	13.579648
16.670963	837.192910	13.584666
16.374237	841.470955	13.589683
16.489657	844.936925	13.594701
16.698924	837.886036	13.599719
16.369066	844.097387	13.604736
16.458653	841.735602	13.609754
16.289937	834.923441	13.614771
16.364003	833.255177	13.619789
17.099768	848.458523	13.624807
16.495320	850.086337	13.629824
16.817438	845.378357	13.634842
16.549740	858.923406	13.639859
16.672162	859.497643	13.644877
17.124777	863.090993	13.649895
16.927616	863.793882	13.654912
17.396088	858.327827	13.659930
17.283614	850.806332	13.664947
16.720319	844.077692	13.669965
16.882041	836.368349	13.674983
16.892308	835.988085	13.680000
16.633731	836.634265	13.685018
16.833726	837.013392	13.690035
16.616216	843.365036	13.695053
17.117726	841.923702	13.700071
16.913931	846.493385	13.705088
17.040390	845.833105	13.710106
17.250822	850.773785	13.715123
16.986678	843.316932	13.720141
17.298632	835.855590	13.725159
16.939298	841.386738	13.730176
17.123014	838.205588	13.735194
17.011764	842.129716	13.740211
16.731561	845.417448	13.745229
16.961326	855.719851	13.750247
17.218066	863.364093	13.755264
17.031594	872.399596	13.760282
17.176572	868.470253	13.765299
16.834925	870.473708	13.770317
17.300016	870.701111	13.775335
16.997782	877.015467	13.780352
17.031697	871.869525	13.785370
17.185094	860.081111	13.790387
17.059724	873.862781	13.795405
17.409300	865.748645	13.800423
17.329874	866.934964	13.805440
17.324055	865.386429	13.810458
17.398040	873.926955	13.815475
17.186285	874.966624	13.820493
17.499080	868.388742	13.825511
17.711030	870.293381	13.830528
17.684716	869.767337	13.835546
17.838251	867.749033	13.840563
17.451370	867.459005	13.845581
17.721464	862.718096	13.850599
17.808414	850.886386	13.855616
17.586386	853.448712	13.860634
17.560232	848.113319	13.865651
17.193328	848.694317	13.870669
17.271187	841.578681	13.875687
16.983789	859.898253	13.880704
17.042381	863.960040	13.885722
17.561263	865.820046	13.890739
17.265699	868.198168	13.895757
17.373327	867.158977	13.900775
17.646635	868.385048	13.905792
17.469896	870.776228	13.910810
17.748126	867.286875	13.915827
17.500208	871.831876	13.920845
17.922104	865.694589	13.925863
18.027457	866.855294	13.930880
17.384088	867.668680	13.935898
17.759942	865.347526	13.940915
17.156229	869.348335	13.945933
17.574680	870.955741	13.950951
18.010812	878.237552	13.955968
18.231878	888.841123	13.960986
18.094836	869.969125	13.966003
17.957260	873.966785	13.971021
18.092225	867.624869	13.976039
17.837694	874.922696	13.981056
17.789902	873.323893	13.986074
18.057825	859.889291	13.991091
17.841846	871.939951	13.996109
18.139237	865.396025	14.001127
17.623234	862.175496	14.006144
17.495874	873.953589	14.011162
17.913701	865.481697	14.016179
17.794763	870.461041	14.021197
18.242311	883.765363	14.026215
17.994391	879.976084	14.031232
17.781651	879.564270	14.036250
18.361740	882.762245	14.041267
18.137698	883.579771	14.046285
17.868624	874.867691	14.051303
18.087791	884.780451	14.056320
18.067265	903.882162	14.061338
18.242774	898.310233	14.066355
18.195189	894.587587	14.071373
18.149796	894.818733	14.076391
18.349815	901.992152	14.081408
17.942193	902.361745	14.086426
18.415676	893.931665	14.091443
18.187522	902.333058	14.096461
18.378174	898.106270	14.101479
18.080207	894.387895	14.106496
18.169671	899.328488	14.111514
18.304332	888.464447	14.116531
18.292026	901.600544	14.121549
18.488286	898.553127	14.126567
18.502687	893.539603	14.131584
18.038150	895.104613	14.136602
18.086046	888.072517	14.141619
18.059739	896.508751	14.146637
18.203739	894.110086	14.151655
18.266386	891.559989	14.156672
18.443305	894.281108	14.161690
18.551678	888.120046	14.166707
18.254045	894.847093	14.171725
18.517873	892.379279	14.176743
18.650550	894.034337	14.181760
18.210948	897.451036	14.186778
18.625726	889.951572	14.191795
18.406735	895.413549	14.196813
18.627631	905.717362	14.201831
18.988094	912.168387	14.206848
18.671385	909.813049	14.211866
18.518921	902.976241	14.216883
18.586492	891.646127	14.221901
18.792473	889.676459	14.226919
18.748072	890.914129	14.231936
18.725602	897.232270	14.236954
18.765623	885.647679	14.241971
18.435976	898.268307	14.246989
18.482576	911.994830	14.252007
18.622095	916.637307	14.257024
18.573390	918.147043	14.262042
18.876101	917.421450	14.267059
18.557033	917.433280	14.272077
18.965969	911.787135	14.277095
19.006558	917.019359	14.282112
18.734481	917.301578	14.287130
19.128528	916.855248	14.292147
18.697487	928.368241	14.297165
18.690297	918.018563	14.302183
18.901906	915.906007	14.307200
18.581587	928.250654	14.312218
18.911221	915.999272	14.317235
18.937601	918.658628	14.322253
19.087227	916.764002	14.327271
19.077041	917.750199	14.332288
19.035140	919.972072	14.337306
19.020549	919.725062	14.342323
19.211056	921.131283	14.347341
18.979466	921.015887	14.352359
18.964084	922.135434	14.357376
19.165185	938.902144	14.362394
19.678344	927.426894	14.367411
19.487371	927.077960	14.372429
19.000209	916.181332	14.377447
19.104093	913.227189	14.382464
18.973779	921.935243	14.387482
19.464700	927.151003	14.392499
19.633024	927.187932	14.397517
19.214928	929.477845	14.402535
19.351865	925.177365	14.407552
19.292110	926.133411	14.412570
19.551835	933.158694	14.417587
19.580325	917.063171	14.422605
19.299872	919.350587	14.427623
19.413206	920.364889	14.432640
19.079104	922.872093	14.437658
19.419745	927.290759	14.442675
19.711551	930.426332	14.447693
19.591137	941.133593	14.452711
19.703471	933.463455	14.457728
19.510739	934.279263	14.462746
19.370576	930.198646	14.467763
19.154081	931.523073	14.472781
19.065337	932.108100	14.477799
19.420170	933.577098	14.482816
19.239646	938.619697	14.487834
18.935113	938.411518	14.492851
19.319348	940.279874	14.497869
19.203635	952.911412	14.502887
19.976229	955.606066	14.507904
19.827265	961.003513	14.512922
19.776607	959.793305	14.517939
20.281005	955.157899	14.522957
19.960485	943.960759	14.527975
20.217300	930.947547	14.532992
19.949446	925.558246	14.538010
19.846620	926.735589	14.543027
19.575628	920.359032	14.548045
19.336117	922.617984	14.553063
19.843701	924.643854	14.558080
19.734513	938.331538	14.563098
19.906889	940.952388	14.568115
20.025179	950.224496	14.573133
19.915202	949.673606	14.578151
20.375886	950.393993	14.583168
20.191557	935.899992	14.588186
20.034964	923.001644	14.593203
20.120378	920.012506	14.598221
19.877409	926.194579	14.603239
20.120970	926.437540	14.608256
19.833599	917.336976	14.613274
19.877377	925.809649	14.618291
19.757190	935.207239	14.623309
19.943577	943.787102	14.628327
20.048896	943.521422	14.633344
20.075633	950.384175	14.638362
20.532550	945.601534	14.643379
20.125797	948.924767	14.648397
20.349723	949.325416	14.653415
20.288393	954.071757	14.658432
20.359095	940.541571	14.663450
20.351985	945.206886	14.668467
20.334370	950.792158	14.673485
20.306642	951.598055	14.678503
20.571891	956.126294	14.683520
20.278632	959.015301	14.688538
20.021232	954.732029	14.693555
20.450489	950.982465	14.698573
20.394962	953.954375	14.703591
20.571575	944.895164	14.708608
20.083464	948.928483	14.713626
19.870977	950.571016	14.718643
20.426779	948.281794	14.723661
20.254277	953.947985	14.728679
20.322590	949.898020	14.733696
20.695435	963.008909	14.738714
20.323106	969.725524	14.743731
20.596987	973.233118	14.748749
20.673270	985.516056	14.753767
20.825010	972.986224	14.758784
20.675078	977.326651	14.763802
20.658033	967.237249	14.768819
20.764229	975.050143	14.773837
20.611386	979.015490	14.778855
20.972618	971.966134	14.783872
20.768344	977.056622	14.788890
20.942880	976.641313	14.793907
20.600929	962.780890	14.798925
20.773850	969.870195	14.803943
20.654697	968.648560	14.808960
20.579111	969.846910	14.813978
20.918888	971.939938	14.818995
20.809864	973.115093	14.824013
20.477518	983.006480	14.829031
20.613851	973.290819	14.834048
20.507647	979.300140	14.839066
20.458917	971.241659	14.844083
21.009562	972.856895	14.849101
21.037813	988.233633	14.854119
21.354006	977.435946	14.859136
21.245902	971.002453	14.864154
21.234190	979.101944	14.869171
21.314102	977.928209	14.874189
20.635008	976.860025	14.879207
20.858354	970.087753	14.884224
20.558536	973.482702	14.889242
21.169947	989.286188	14.894259
21.345029	985.213280	14.899277
21.222598	1001.449764	14.904295
21.659845	992.624499	14.909312
21.613382	981.955855	14.914330
20.994141	970.824142	14.919347
21.243432	970.081618	14.924365
21.003005	974.382487	14.929383
21.523233	982.547480	14.934400
21.523275	983.169177	14.939418
21.438939	976.432185	14.944435
21.519651	968.315683	14.949453
21.246988	966.770817	14.954471
21.310293	968.035904	14.959488
21.481340	976.949524	14.964506
21.523934	978.173655	14.969523
21.870986	968.923796	14.974541
21.653603	961.973999	14.979559
21.710368	961.570715	14.984576
21.888198	962.903175	14.989594
21.282704	959.967955	14.994611
21.599864	958.353347	14.999629
21.317200	969.328878	15.004647
21.482391	961.101399	15.009664
21.476437	964.097149	15.014682
21.596512	985.831039	15.019699
21.766561	980.711207	15.024717
21.787692	996.647628	15.029735
21.881668	989.362170	15.034752
21.639967	978.468311	15.039770
21.545486	993.731621	15.044787
21.426101	989.341648	15.049805
22.046628	996.749430	15.054823
22.048548	988.913425	15.059840
22.323190	987.056130	15.064858
21.759048	981.564623	15.069875
21.842905	981.049824	15.074893
21.838761	986.197517	15.079911
21.865123	985.044742	15.084928
21.503533	995.284665	15.089946
21.877808	995.923835	15.094963
21.676806	988.270900	15.099981
21.548663	994.129010	15.104999
21.465511	978.397947	15.110016
22.313598	987.430218	15.115034
22.118591	995.570879	15.120051
21.980948	985.162578	15.125069
21.780423	985.531486	15.130087
22.164756	1006.877125	15.135104
22.367311	1005.141504	15.140122
22.354499	1008.813660	15.145139
22.197826	999.490737	15.150157
22.143493	1003.065218	15.155175
22.459626	1005.215578	15.160192
22.374960	993.154878	15.165210
22.186317	997.756953	15.170227
22.514975	982.766485	15.175245
22.373042	986.282018	15.180263
22.263958	977.103174	15.185280
22.469365	980.350036	15.190298
22.227650	983.590776	15.195315
22.393503	978.528401	15.200333
22.544293	988.205716	15.205351
22.403326	986.154359	15.210368
22.195099	984.186056	15.215386
22.149581	999.198755	15.220403
22.431466	1007.435581	15.225421
22.793759	1014.728945	15.230439
22.496200	1011.890936	15.235456
22.643248	1012.593887	15.240474
22.830590	1013.713434	15.245491
22.522374	1000.557775	15.250509
22.448402	1008.357710	15.255527
22.614011	1017.890725	15.260544
23.004435	1013.165754	15.265562
22.847550	1009.608422	15.270579
22.540123	1010.047622	15.275597
22.519101	1019.240472	15.280615
22.612863	1017.726912	15.285632
23.001576	1010.865763	15.290650
22.851600	1015.291412	15.295667
22.878856	1010.856511	15.300685
22.919599	1011.080560	15.305703
22.814434	1005.391354	15.310720
22.608018	996.167694	15.315738
22.618182	1003.260262	15.320755
22.966638	1004.032838	15.325773
22.985925	1004.206579	15.330791
22.795421	1005.265036	15.335808
23.116630	1010.516712	15.340826
22.877320	1001.891452	15.345843
22.731643	1012.466992	15.350861
22.779833	1011.474915	15.355879
22.636225	1013.851489	15.360896
23.212193	1022.326552	15.365914
23.091211	1036.088730	15.370931
23.209831	1030.172173	15.375949
23.334648	1030.667149	15.380967
23.563155	1033.882023	15.385984
23.248454	1031.128730	15.391002
23.215256	1034.965009	15.396019
23.318285	1027.955832	15.401037
23.189498	1030.610962	15.406055
23.221895	1029.785443	15.411072
23.299051	1029.852346	15.416090
23.151358	1034.198750	15.421107
23.088668	1036.319734	15.426125
23.500480	1034.131813	15.431143
23.220336	1037.498465	15.436160
23.269927	1032.208027	15.441178
23.469593	1035.184398	15.446195
23.050258	1035.659957	15.451213
23.247922	1033.448575	15.456231
23.235957	1031.153068	15.461248
23.444958	1044.100182	15.466266
23.284409	1051.288775	15.471283
23.316078	1053.843188	15.476301
23.467247	1058.061016	15.481319
23.633631	1065.618429	15.486336
23.818519	1050.489345	15.491354
23.820043	1058.618370	15.496371
23.775738	1055.387478	15.501389
23.945770	1056.932596	15.506407
24.131533	1056.938408	15.511424
23.917908	1051.442797	15.516442
23.990167	1063.653833	15.521459
23.903218	1053.805637	15.526477
24.198378	1039.773376	15.531495
23.729683	1030.391722	15.536512
23.843406	1026.145324	15.541530
23.847797	1045.426341	15.546547
23.856771	1043.787127	15.551565
23.943448	1052.382566	15.556583
23.739071	1046.345882	15.561600
23.854666	1052.462703	15.566618
23.938820	1059.906686	15.571635
24.066754	1051.817508	15.576653
24.256377	1050.301642	15.581671
23.993657	1051.519667	15.586688
24.089334	1041.687224	15.591706
24.159016	1046.870776	15.596723
23.877881	1047.943347	15.601741
24.341134	1041.834274	15.606759
23.787829	1045.647395	15.611776
24.298177	1041.954613	15.616794
24.336964	1044.381686	15.621811
24.432863	1046.717817	15.626829
24.030921	1042.539079	15.631847
23.905506	1058.113370	15.636864
24.470630	1045.326624	15.641882
24.246152	1049.139040	15.646899
24.564453	1043.327086	15.651917
24.453809	1041.327805	15.656935
24.349191	1049.504909	15.661952
24.595582	1040.892370	15.666970
24.417049	1051.561410	15.671987
24.362842	1050.821956	15.677005
24.313175	1046.771403	15.682023
24.621814	1066.910777	15.687040
24.717059	1061.149325	15.692058
24.287328	1071.513509	15.697075
24.563506	1068.728172	15.702093
24.805776	1074.557039	15.707111
24.623045	1069.470018	15.712128
24.421831	1066.295112	15.717146
24.878994	1076.858880	15.722163
24.633285	1088.081192	15.727181
24.746451	1075.973855	15.732199
24.604447	1084.115771	15.737216
24.541101	1078.142323	15.742234
24.734896	1083.672631	15.747251
24.680683	1084.227041	15.752269
25.145031	1069.947511	15.757287
24.677565	1075.842700	15.762304
24.747603	1082.238021	15.767322
24.829433	1074.452652	15.772339
24.948609	1083.027268	15.777357
25.010309	1075.535363	15.782375
24.558007	1083.589893	15.787392
24.791952	1099.228187	15.792410
24.753707	1107.814701	15.797427
24.816338	1104.873261	15.802445
25.065467	1105.105891	15.807463
24.777693	1107.697424	15.812480
25.423368	1101.594642	15.817498
25.236423	1100.443513	15.822515
25.295775	1107.266535	15.827533
25.293204	1100.715579	15.832551
25.311222	1103.429913	15.837568
25.032664	1098.061160	15.842586
25.122324	1103.898018	15.847603
25.015570	1103.949375	15.852621
25.253247	1095.454930	15.857639
25.137386	1104.744640	15.862656
25.490713	1123.782068	15.867674
26.071552	1117.616793	15.872691
25.812055	1114.520380	15.877709
26.138121	1090.406892	15.882727
25.464785	1094.674207	15.887744
25.482088	1100.954670	15.892762
25.839994	1092.454131	15.897779
25.364948	1095.551341	15.902797
25.366070	1096.791405	15.907815
25.278139	1097.455205	15.912832
25.337773	1090.033043	15.917850
25.587866	1086.844671	15.922867
25.721973	1089.496747	15.927885
26.002671	1090.926808	15.932903
25.853524	1092.408016	15.937920
25.481712	1089.733033	15.942938
25.760467	1095.691924	15.947955
25.798532	1102.982156	15.952973
26.111373	1110.661952	15.957991
26.167174	1100.005717	15.963008
26.032649	1088.912068	15.968026
25.929117	1089.145957	15.973043
25.774049	1090.284108	15.978061
25.864270	1078.969283	15.983079
25.905205	1091.207305	15.988096
26.093890	1105.249523	15.993114
26.061210	1103.559984	15.998131
26.082159	1110.458414	16.003149
26.129970	1104.455027	16.008167
26.334980	1111.924396	16.013184
26.125197	1100.021958	16.018202
26.410262	1097.209987	16.023219
26.337666	1096.056832	16.028237
26.536768	1082.213062	16.033255
26.249735	1083.103518	16.038272
26.308594	1076.804935	16.043290
26.310529	1081.121743	16.048307
26.052732	1079.539839	16.053325
26.481546	1080.123183	16.058343
26.492668	1081.453206	16.063360
26.392958	1082.377613	16.068378
26.657817	1077.015776	16.073395
26.176766	1085.494500	16.078413
26.330257	1073.743799	16.083431
26.521288	1082.881576	16.088448
26.315261	1094.886656	16.093466
26.409558	1106.627236	16.098483
26.465153	1101.727159	16.103501
26.690121	1105.829368	16.108519
26.727533	1108.013669	16.113536
26.447844	1114.734849	16.118554
26.744506	1107.966889	16.123571
26.567632	1113.816847	16.128589
26.789763	1106.921637	16.133607
26.539546	1108.560592	16.138624
26.612324	1103.919768	16.143642
26.733691	1103.626341	16.148659
26.744594	1111.378393	16.153677
26.776878	1098.598831	16.158695
26.780602	1106.604461	16.163712
26.848380	1104.268127	16.168730
26.746920	1105.271701	16.173747
26.759277	1106.270178	16.178765
26.881289	1104.685941	16.183783
27.070024	1126.967885	16.188800
27.139697	1124.902650	16.193818
27.208373	1122.269531	16.198835
27.092694	1119.008716	16.203853
27.133492	1106.085813	16.208871
26.857498	1115.675013	16.213888
26.976133	1128.753022	16.218906
27.116795	1127.702361	16.223923
27.195677	1134.149971	16.228941
27.234382	1129.261983	16.233959
27.107165	1128.129954	16.238976
27.164007	1125.653311	16.243994
27.164637	1130.869729	16.249011
26.838888	1137.803214	16.254029
27.384582	1121.784768	16.259047
27.303659	1130.873395	16.264064
27.317473	1128.103652	16.269082
27.442896	1123.116958	16.274099
27.646012	1133.095470	16.279117
27.308698	1125.324846	16.284135
27.484609	1118.323221	16.289152
27.521053	1126.292207	16.294170
27.508778	1128.676749	16.299187
27.691803	1123.693709	16.304205
27.699260	1124.232207	16.309223
27.494094	1121.474469	16.314240
27.170770	1126.334229	16.319258
27.364615	1137.967813	16.324275
27.473376	1150.491959	16.329293
27.796950	1146.755653	16.334311
28.202498	1146.642040	16.339328
27.879480	1157.087488	16.344346
27.713468	1153.607287	16.349363
27.510676	1148.239346	16.354381
27.553557	1142.050524	16.359399
27.670719	1144.184543	16.364416
27.987203	1151.636573	16.369434
28.173105	1144.317804	16.374451
28.028069	1148.685913	16.379469
27.934129	1151.960479	16.384487
27.951224	1150.323146	16.389504
28.060400	1148.977587	16.394522
27.868481	1142.809543	16.399539
27.940675	1149.169838	16.404557
28.390071	1154.338483	16.409575
28.594882	1152.378436	16.414592
28.263041	1156.955510	16.419610
28.203381	1148.097083	16.424627
28.434452	1150.898172	16.429645
28.298319	1150.070485	16.434663
28.136358	1144.901314	16.439680
28.564339	1148.441754	16.444698
28.607261	1154.995956	16.449715
28.289887	1147.739765	16.454733
28.613942	1150.097191	16.459751
28.391615	1143.615147	16.464768
28.301321	1150.284762	16.469786
28.609762	1150.527092	16.474803
28.715267	1147.547412	16.479821
28.547402	1141.574437	16.484839
28.630923	1143.877795	16.489856
28.236279	1149.237811	16.494874
28.492061	1156.692982	16.499891
28.918641	1164.534972	16.504909
28.989955	1164.533357	16.509927
29.095498	1167.464446	16.514944
28.660639	1162.842683	16.519962
29.178003	1144.502818	16.524979
29.018501	1139.544702	16.529997
28.822258	1137.959520	16.535015
28.854892	1137.518964	16.540032
28.722062	1141.626397	16.545050
28.742312	1140.518744	16.550067
28.775781	1147.598274	16.555085
29.196099	1164.116472	16.560103
29.301764	1164.879520	16.565120
28.857792	1151.978413	16.570138
29.161881	1149.813562	16.575155
29.094177	1151.698657	16.580173
28.864062	1146.041483	16.585191
29.417723	1149.369854	16.590208
29.217198	1160.623046	16.595226
29.239345	1163.630233	16.600243
29.102178	1157.601981	16.605261
29.221779	1164.049574	16.610279
29.296038	1159.654656	16.615296
29.120273	1161.146325	16.620314
29.557038	1167.642368	16.625331
29.310105	1163.773979	16.630349
28.951995	1174.079735	16.635367
29.060195	1162.932470	16.640384
29.138742	1170.266920	16.645402
29.375200	1164.218363	16.650419
29.423880	1156.693738	16.655437
28.941158	1157.598887	16.660455
29.663981	1160.310791	16.665472
29.657949	1181.629057	16.670490
29.879752	1174.970556	16.675507
29.735452	1173.162691	16.680525
29.508805	1165.056085	16.685543
29.677298	1157.291900	16.690560
29.338917	1175.802769	16.695578
29.236651	1179.911763	16.700595
29.550166	1188.604494	16.705613
29.725174	1187.046712	16.710631
30.392009	1183.114944	16.715648
29.813464	1197.402919	16.720666
29.762043	1193.652406	16.725683
30.101273	1191.955447	16.730701
29.778130	1191.743850	16.735719
29.833351	1188.020915	16.740736
29.987711	1183.730283	16.745754
29.846046	1181.353966	16.750771
29.886599	1184.310954	16.755789
29.768462	1187.245314	16.760807
30.407458	1188.120984	16.765824
30.506514	1174.103372	16.770842
30.229980	1175.358269	16.775859
30.239419	1181.551623	16.780877
30.008222	1181.262595	16.785895
30.403603	1183.754087	16.790912
30.447864	1189.553861	16.795930
30.283401	1181.475434	16.800947
30.383016	1178.951099	16.805965
30.325096	1196.960734	16.810983
30.775089	1196.884382	16.816000
30.216303	1190.461018	16.821018
30.355069	1189.786187	16.826035
30.780559	1195.327793	16.831053
30.426517	1206.040030	16.836071
30.464775	1205.680646	16.841088
30.396462	1204.293290	16.846106
30.460536	1200.606844	16.851123
30.326234	1201.457747	16.856141
30.393127	1209.018089	16.861159
30.372854	1199.825302	16.866176
30.643788	1206.265127	16.871194
30.347045	1194.502396	16.876211
30.588441	1204.017399	16.881229
30.591793	1216.400214	16.886247
30.906797	1225.966884	16.891264
30.768239	1227.635802	16.896282
30.785424	1216.199718	16.901299
30.958999	1219.861834	16.906317
30.961919	1222.635341	16.911335
31.195180	1210.376671	16.916352
31.077952	1233.719394	16.921370
30.811270	1218.048251	16.926387
31.136915	1220.654747	16.931405
31.266706	1221.259407	16.936423
31.229243	1222.508643	16.941440
31.182003	1215.951976	16.946458
31.109813	1219.327309	16.951475
31.222959	1217.526693	16.956493
30.969007	1222.991058	16.961511
31.479045	1219.102629	16.966528
31.091484	1216.483727	16.971546
31.298315	1221.604951	16.976563
31.494181	1211.037295	16.981581
31.212843	1214.202195	16.986599
31.223812	1209.640394	16.991616
31.302381	1213.086927	16.996634
31.284810	1226.918358	17.001651
31.139337	1227.881455	17.006669
31.142038	1235.581190	17.011687
31.309789	1228.662842	17.016704
31.290027	1236.189350	17.021722
31.151868	1237.700417	17.026739
31.658539	1251.661683	17.031757
31.472259	1256.222431	17.036775
31.897241	1259.791763	17.041792
31.596677	1264.859456	17.046810
31.968795	1265.148678	17.051827
32.267588	1267.386977	17.056845
32.189601	1268.674083	17.061863
32.416393	1260.806103	17.066880
32.248649	1248.814969	17.071898
31.908899	1241.839933	17.076915
32.468615	1232.859783	17.081933
32.171975	1234.780531	17.086951
32.297822	1231.945992	17.091968
31.896929	1231.408830	17.096986
32.230473	1239.808134	17.102003
32.382845	1231.374244	17.107021
32.390995	1243.137794	17.112039
32.178044	1238.626628	17.117056
31.982024	1227.400457	17.122074
32.113720	1229.967723	17.127091
32.330909	1234.891679	17.132109
32.452685	1247.467515	17.137127
32.343558	1237.935094	17.142144
32.425482	1249.633514	17.147162
32.131260	1242.869139	17.152179
32.636006	1250.427598	17.157197
32.567802	1254.805860	17.162215
32.334881	1254.539190	17.167232
32.364576	1255.916827	17.172250
32.569638	1257.096748	17.177267
33.166291	1253.119088	17.182285
32.497392	1259.149840	17.187303
32.539429	1256.789092	17.192320
32.563460	1251.325844	17.197338
32.587373	1254.648352	17.202355
32.930940	1248.134968	17.207373
32.440760	1257.312624	17.212391
32.728781	1254.162498	17.217408
32.903820	1254.687531	17.222426
32.973396	1257.523249	17.227443
32.929927	1262.235333	17.232461
32.810516	1259.805047	17.237479
32.641216	1259.686261	17.242496
32.995541	1268.634608	17.247514
33.419999	1276.038321	17.252531
33.629806	1268.797830	17.257549
32.950343	1258.334873	17.262567
33.049792	1249.732489	17.267584
33.061672	1253.394540	17.272602
33.076272	1264.655329	17.277619
33.489361	1266.582344	17.282637
33.345448	1277.675317	17.287655
33.222184	1276.110318	17.292672
33.244452	1274.601556	17.297690
33.244972	1278.754530	17.302707
33.434492	1267.417814	17.307725
33.228051	1287.075901	17.312743
33.497823	1275.540492	17.317760
33.577003	1273.063506	17.322778
33.552945	1274.648329	17.327795
33.622518	1282.407100	17.332813
33.530341	1286.211591	17.337831
33.585525	1279.358087	17.342848
33.851018	1270.398481	17.347866
33.583887	1283.404122	17.352883
33.527490	1279.130503	17.357901
33.679397	1275.903735	17.362919
33.737726	1281.142772	17.367936
34.007093	1276.190428	17.372954
33.686474	1278.613531	17.377971
33.721798	1282.625388	17.382989
33.562532	1282.956319	17.388007
33.656991	1297.373120	17.393024
33.782081	1301.825440	17.398042
33.806164	1303.311252	17.403059
34.104714	1304.116858	17.408077
33.886057	1298.830237	17.413095
34.212428	1301.278841	17.418112
34.101704	1300.923717	17.423130
34.288769	1305.183353	17.428147
34.468846	1309.529284	17.433165
33.941268	1305.218565	17.438183
34.189013	1300.121259	17.443200
34.334921	1292.647710	17.448218
34.014251	1305.857363	17.453235
34.584945	1313.837927	17.458253
34.348477	1323.010829	17.463271
34.164637	1322.900618	17.468288
34.445351	1321.973307	17.473306
34.632000	1325.358854	17.478323
34.427748	1318.406872	17.483341
34.466288	1327.316053	17.488359
34.479393	1321.046597	17.493376
34.514557	1319.182373	17.498394
34.550991	1320.546343	17.503411
34.642907	1304.140794	17.508429
34.852287	1315.712115	17.513447
34.614167	1322.632028	17.518464
34.551644	1322.061116	17.523482
34.495106	1322.770529	17.528499
34.798541	1337.533523	17.533517
35.139297	1337.505737	17.538535
35.043412	1338.464275	17.543552
35.021772	1329.653487	17.548570
35.221935	1334.652706	17.553587
35.376400	1332.511129	17.558605
35.445580	1332.935881	17.563623
35.262680	1330.944661	17.568640
35.452149	1311.803608	17.573658
35.082928	1313.741977	17.578675
35.352048	1307.792428	17.583693
35.144189	1317.244895	17.588711
34.872533	1315.355858	17.593728
35.219067	1317.665626	17.598746
35.185212	1333.926491	17.603763
35.322567	1328.811650	17.608781
35.095096	1333.883761	17.613799
35.405102	1341.706109	17.618816
35.554323	1326.326723	17.623834
35.434000	1339.612505	17.628851
35.247520	1335.374904	17.633869
35.379432	1331.314951	17.638887
35.884302	1327.099100	17.643904
35.868515	1335.439230	17.648922
35.853438	1335.946528	17.653939
35.749919	1331.011201	17.658957
36.166098	1340.022537	17.663975
35.612340	1347.237756	17.668992
36.059336	1340.995414	17.674010
35.598036	1343.910644	17.679027
35.717161	1339.776940	17.684045
35.727473	1335.887396	17.689063
35.587517	1345.474474	17.694080
36.090736	1344.563012	17.699098
36.359790	1356.487988	17.704115
35.710601	1359.413539	17.709133
36.153934	1361.354790	17.714151
36.386544	1356.180929	17.719168
36.377629	1356.974448	17.724186
36.123683	1360.703156	17.729203
36.407020	1362.016063	17.734221
35.939205	1363.853023	17.739239
35.863158	1367.670799	17.744256
36.157044	1352.587604	17.749274
36.119977	1367.577207	17.754291
36.316085	1362.948672	17.759309
36.672104	1368.094048	17.764327
36.361275	1385.553113	17.769344
36.662663	1380.264394	17.774362
36.613167	1387.622025	17.779379
36.589354	1378.454944	17.784397
36.981954	1379.268001	17.789415
36.911936	1385.347564	17.794432
37.255223	1365.942662	17.799450
37.072971	1369.278355	17.804467
37.071061	1353.711037	17.809485
36.580138	1352.383156	17.814503
36.550667	1355.174350	17.819520
36.906663	1361.222290	17.824538
37.345927	1364.038336	17.829555
37.084888	1365.063615	17.834573
36.687706	1358.365719	17.839591
36.870805	1370.136828	17.844608
37.092619	1367.748075	17.849626
36.867392	1374.097954	17.854643
37.217232	1379.635617	17.859661
37.092418	1373.043632	17.864679
36.892000	1375.732057	17.869696
37.183907	1369.526474	17.874714
37.042573	1375.456191	17.879731
37.160417	1375.381060	17.884749
37.239599	1375.040548	17.889767
36.854350	1384.448086	17.894784
37.287455	1389.108094	17.899802
37.538969	1392.941148	17.904819
37.462930	1397.169185	17.909837
37.322112	1392.659372	17.914855
37.128583	1398.455211	17.919872
37.474677	1387.545323	17.924890
37.514717	1393.456274	17.929907
37.643784	1397.655534	17.934925
37.814387	1392.096839	17.939943
37.510326	1397.941445	17.944960
38.060230	1384.251106	17.949978
37.687856	1399.539096	17.954995
37.786513	1399.151370	17.960013
38.275547	1399.687481	17.965031
37.903213	1388.390829	17.970048
38.318522	1383.333682	17.975066
38.144628	1381.066498	17.980083
37.859927	1393.074559	17.985101
38.158961	1380.527820	17.990119
37.872402	1392.406782	17.995136
38.456074	1402.026392	18.000154
38.271671	1404.958481	18.005171
38.379315	1416.094426	18.010189
38.619398	1409.231019	18.015207
38.055058	1403.610021	18.020224
38.456677	1407.337656	18.025242
38.231075	1413.365713	18.030259
38.598282	1408.114076	18.035277
38.629811	1409.030689	18.040295
38.367021	1413.767492	18.045312
38.088334	1405.198660	18.050330
38.475991	1402.651537	18.055347
38.516450	1411.999121	18.060365
38.732322	1409.740676	18.065383
38.600856	1407.687790	18.070400
38.793994	1407.291665	18.075418
38.647293	1413.692448	18.080435
38.577177	1418.257242	18.085453
38.499687	1404.866543	18.090471
38.622793	1412.225713	18.095488
39.116902	1428.265607	18.100506
39.301340	1435.867704	18.105523
38.774794	1436.091719	18.110541
39.259039	1430.821852	18.115559
39.139914	1438.499617	18.120576
39.404702	1436.309293	18.125594
39.247985	1437.091113	18.130611
39.285204	1430.047843	18.135629
39.296276	1433.403942	18.140647
39.390665	1433.430293	18.145664
39.340999	1437.707884	18.150682
39.339584	1434.830010	18.155699
39.424805	1435.451084	18.160717
39.425571	1430.777205	18.165735
39.803116	1440.763447	18.170752
39.608082	1433.746869	18.175770
39.608001	1435.040793	18.180787
39.381848	1432.336766	18.185805
39.625511	1430.929222	18.190823
39.513325	1436.911225	18.195840
39.408674	1436.375271	18.200858
39.892627	1432.118471	18.205875
39.630066	1436.609090	18.210893
39.754222	1431.395287	18.215911
39.540652	1439.005705	18.220928
39.310141	1429.842377	18.225946
39.441324	1428.742681	18.230963
39.520706	1450.660200	18.235981
40.106770	1449.521238	18.240999
40.201809	1451.456767	18.246016
40.255853	1445.818372	18.251034
40.521496	1446.622796	18.256051
40.466709	1458.790767	18.261069
40.426102	1438.536677	18.266087
40.299262	1421.028981	18.271104
40.172688	1425.649904	18.276122
40.098367	1424.941969	18.281139
40.329685	1438.608580	18.286157
40.707968	1439.853062	18.291175
40.746213	1442.302365	18.296192
40.639366	1423.712259	18.301210
40.541310	1412.549614	18.306227
40.253108	1426.637932	18.311245
40.640369	1423.178833	18.316263
40.665376	1433.507140	18.321280
40.738631	1437.115491	18.326298
40.890215	1432.834699	18.331315
40.558057	1444.417836	18.336333
40.681494	1438.292109	18.341351
40.524142	1439.698882	18.346368
40.549573	1447.041717	18.351386
41.021485	1441.224653	18.356403
40.513228	1436.282884	18.361421
40.840186	1427.745978	18.366439
40.642178	1440.996594	18.371456
40.807114	1435.022198	18.376474
40.783792	1444.537520	18.381491
40.786694	1462.951368	18.386509
41.341230	1467.589334	18.391527
41.020815	1461.456965	18.396544
41.095120	1474.292819	18.401562
41.268178	1471.526631	18.406579
41.124435	1467.519032	18.411597
41.349843	1465.218070	18.416615
41.405477	1466.020479	18.421632
41.474588	1458.464143	18.426650
41.631739	1458.442853	18.431667
41.177614	1465.361738	18.436685
41.306251	1465.723587	18.441703
41.592196	1477.440885	18.446720
41.589608	1493.368821	18.451738
41.898262	1484.465505	18.456755
41.872827	1488.373258	18.461773
41.856126	1483.575851	18.466791
41.716239	1483.824872	18.471808
41.657485	1485.115312	18.476826
41.870104	1479.752021	18.481843
41.830019	1483.034042	18.486861
41.671434	1482.632717	18.491879
41.934964	1477.192072	18.496896
41.952437	1483.564163	18.501914
42.316674	1482.128374	18.506931
41.959442	1483.790336	18.511949
41.994463	1481.998701	18.516967
42.159899	1482.080263	18.521984
42.327620	1493.408876	18.527002
42.394882	1495.752681	18.532019
42.298988	1500.356224	18.537037
42.144719	1512.908953	18.542055
41.938994	1508.459710	18.547072
42.199764	1510.678713	18.552090
42.794977	1498.953634	18.557107
42.557298	1509.032546	18.562125
42.571749	1514.609847	18.567143
42.584642	1508.551800	18.572160
42.548724	1513.761397	18.577178
42.816055	1501.576119	18.582195
42.653551	1513.713561	18.587213
42.653214	1511.031169	18.592231
42.262259	1505.749221	18.597248
42.879441	1536.870756	18.602266
42.976892	1532.273317	18.607283
42.880186	1535.936553	18.612301
43.031229	1537.017604	18.617319
42.882285	1535.286165	18.622336
42.837526	1526.753437	18.627354
43.199440	1532.746866	18.632371
43.072803	1539.412817	18.637389
42.923037	1533.339061	18.642407
43.275799	1529.206807	18.647424
42.989792	1536.118479	18.652442
43.377987	1527.811836	18.657459
43.283754	1538.711041	18.662477
43.065458	1544.223601	18.667495
43.671458	1544.918234	18.672512
43.625985	1554.058361	18.677530
43.544712	1550.154628	18.682547
43.511610	1554.432823	18.687565
43.610434	1554.572095	18.692583
43.709107	1555.225794	18.697600
43.797818	1549.086500	18.702618
44.002740	1546.296405	18.707635
43.852247	1548.087133	18.712653
44.001119	1558.001745	18.717671
44.113140	1562.099555	18.722688
43.841100	1556.893752	18.727706
43.813004	1548.380511	18.732723
44.010538	1558.656782	18.737741
44.011728	1556.340224	18.742759
43.830679	1547.850797	18.747776
43.923549	1557.332310	18.752794
44.074555	1542.457396	18.757811
43.941407	1540.767679	18.762829
43.733107	1558.564404	18.767847
44.071941	1567.114521	18.772864
44.318584	1580.280230	18.777882
44.659524	1568.373785	18.782899
44.459852	1574.470443	18.787917
44.519597	1578.595331	18.792935
44.674660	1568.646053	18.797952
44.314831	1577.844604	18.802970
44.860843	1572.618729	18.807987
44.603575	1584.035658	18.813005
44.973231	1573.481757	18.818023
45.325526	1572.429678	18.823040
44.649408	1569.940857	18.828058
44.586401	1575.246210	18.833075
44.810629	1572.109117	18.838093
45.191803	1571.652154	18.843111
45.075489	1560.233479	18.848128
44.859626	1572.846334	18.853146
45.116368	1562.395227	18.858163
44.805351	1571.226408	18.863181
44.686169	1573.454082	18.868199
45.255177	1572.472406	18.873216
45.073064	1595.178754	18.878234
45.389896	1589.808672	18.883251
45.103244	1593.943314	18.888269
44.939111	1601.637623	18.893287
45.244463	1598.494207	18.898304
44.735867	1595.275543	18.903322
45.209940	1600.333178	18.908339
45.736478	1616.532297	18.913357
45.690970	1619.758382	18.918375
46.123283	1621.341610	18.923392
45.917358	1620.275454	18.928410
45.973177	1614.939692	18.933427
45.977070	1599.308138	18.938445
45.384237	1589.920268	18.943463
45.752353	1592.498115	18.948480
45.947345	1618.976990	18.953498
46.005374	1605.798574	18.958515
46.100005	1619.029005	18.963533
45.968452	1624.834203	18.968551
46.425392	1620.985515	18.973568
45.965434	1621.593646	18.978586
45.985871	1619.258304	18.983603
46.006669	1612.141779	18.988621
45.911548	1619.897936	18.993639
45.858295	1612.322716	18.998656
45.918097	1607.996211	19.003674
45.791963	1610.660481	19.008691
46.170773	1631.821535	19.013709
46.477633	1639.988494	19.018727
46.348122	1639.784614	19.023744
46.451433	1646.556816	19.028762
46.603113	1645.728476	19.033779
46.600254	1640.395531	19.038797
46.386628	1637.844160	19.043815
46.739705	1638.650760	19.048832
46.407510	1646.226085	19.053850
46.749475	1657.928468	19.058867
47.005489	1660.908796	19.063885
46.646708	1674.414994	19.068903
46.908103	1659.150404	19.073920
46.966725	1674.500914	19.078938
47.073659	1662.056472	19.083955
47.275766	1656.779974	19.088973
46.801032	1663.850469	19.093991
47.205009	1660.120474	19.099008
47.238486	1667.190742	19.104026
47.276332	1660.819483	19.109043
47.367044	1655.383601	19.114061
47.191323	1653.545864	19.119079
47.461270	1663.075603	19.124096
47.574151	1675.504800	19.129114
47.743300	1682.279389	19.134131
48.071171	1670.444340	19.139149
47.864084	1658.872474	19.144167
47.977543	1652.404238	19.149184
47.854804	1654.474683	19.154202
47.863612	1643.547724	19.159219
47.857925	1645.795607	19.164237
47.612797	1650.024784	19.169255
48.057333	1648.974119	19.174272
47.754842	1654.424081	19.179290
48.089195	1665.537507	19.184307
48.191386	1674.765161	19.189325
48.003080	1679.499905	19.194343
48.132132	1672.199240	19.199360
48.216280	1677.112474	19.204378
48.055126	1676.493789	19.209395
48.273334	1662.529827	19.214413
48.002154	1669.486580	19.219431
48.334269	1663.700678	19.224448
48.093596	1667.783995	19.229466
48.545298	1673.564672	19.234483
48.353342	1667.428011	19.239501
48.391187	1676.236486	19.244519
48.416485	1686.413411	19.249536
48.660232	1699.822662	19.254554
48.715294	1700.063425	19.259571
48.839507	1700.732088	19.264589
48.693273	1709.389355	19.269607
48.750111	1701.803268	19.274624
49.039539	1693.537173	19.279642
48.735872	1691.930796	19.284659
48.878070	1687.411559	19.289677
49.086678	1688.802400	19.294695
49.149009	1696.950651	19.299712
48.862642	1696.013782	19.304730
48.818985	1698.314921	19.309747
49.310144	1699.361964	19.314765
49.281682	1717.657878	19.319783
48.921496	1723.918437	19.324800
49.013845	1720.126493	19.329818
49.085070	1722.883131	19.334835
49.466034	1720.084535	19.339853
49.224931	1720.964715	19.344871
49.340846	1717.494158	19.349888
49.243242	1724.442842	19.354906
49.129140	1736.598146	19.359923
49.553458	1741.360603	19.364941
49.475598	1747.725540	19.369959
49.706463	1743.937272	19.374976
49.862388	1748.517450	19.379994
49.957186	1745.813900	19.385011
50.144395	1750.032593	19.390029
49.841961	1742.963185	19.395047
50.077856	1739.376111	19.400064
50.140552	1742.945142	19.405082
49.890701	1747.424392	19.410099
50.373653	1746.291999	19.415117
50.391227	1760.588598	19.420135
50.558932	1763.841475	19.425152
50.404415	1756.783746	19.430170
50.425825	1759.772214	19.435187
50.490406	1766.840833	19.440205
50.494274	1769.216636	19.445223
50.554289	1764.467171	19.450240
50.803418	1767.761021	19.455258
50.524276	1775.883577	19.460275
50.844630	1760.922154	19.465293
50.638085	1766.003751	19.470311
50.847094	1761.253181	19.475328
50.890829	1760.848752	19.480346
50.795029	1765.897328	19.485363
51.034425	1765.784336	19.490381
51.102595	1763.750820	19.495399
51.142462	1763.814064	19.500416
51.316720	1756.528417	19.505434
51.046998	1754.572758	19.510451
51.221263	1753.258046	19.515469
51.182796	1766.127447	19.520487
51.276483	1760.728940	19.525504
50.862748	1753.945107	19.530522
50.776942	1775.560532	19.535539
51.438199	1775.662732	19.540557
51.426861	1781.730138	19.545575
51.580035	1779.203691	19.550592
51.768789	1775.418817	19.555610
51.749284	1774.090090	19.560627
52.080705	1765.003205	19.565645
51.951562	1770.041194	19.570663
51.907063	1765.475264	19.575680
52.111040	1766.516529	19.580698
52.020111	1769.090132	19.585715
52.254475	1759.163116	19.590733
52.055872	1766.313739	19.595751
52.596627	1766.302153	19.600768
52.639289	1762.271777	19.605786
52.556974	1754.243418	19.610803
52.541625	1742.253471	19.615821
52.448228	1742.921302	19.620839
52.259123	1738.128577	19.625856
51.729733	1730.289760	19.630874
52.001359	1734.763557	19.635891
52.704619	1738.299128	19.640909
52.415974	1762.644398	19.645927
52.553245	1754.515577	19.650944
52.669703	1744.834150	19.655962
52.309629	1761.973037	19.660979
52.610429	1755.986849	19.665997
52.618155	1764.326674	19.671015
52.509204	1755.059043	19.676032
52.683904	1749.243972	19.681050
52.174959	1766.778437	19.686067
53.056559	1769.768682	19.691085
53.212005	1772.534307	19.696103
53.165992	1769.925261	19.701120
53.534818	1770.256033	19.706138
53.346779	1771.879054	19.711155
53.398585	1771.795269	19.716173
53.418839	1777.737831	19.721191
53.373919	1776.362567	19.726208
53.291394	1770.464459	19.731226
53.287239	1780.548191	19.736243
53.430966	1770.840413	19.741261
53.446924	1780.671699	19.746279
53.467349	1776.225049	19.751296
53.578204	1773.689412	19.756314
53.646941	1767.531062	19.761331
53.567602	1764.239223	19.766349
53.552849	1770.935178	19.771367
53.531053	1784.663555	19.776384
53.939720	1799.158077	19.781402
53.683178	1801.404010	19.786419
53.733470	1800.070726	19.791437
54.103704	1796.734132	19.796455
53.952557	1804.306582	19.801472
54.108289	1800.943422	19.806490
54.205539	1804.241990	19.811507
54.376179	1790.089670	19.816525
54.417383	1798.594716	19.821543
54.165248	1791.599511	19.826560
54.423363	1808.995654	19.831578
54.322191	1819.653107	19.836595
54.633297	1822.987812	19.841613
54.556665	1816.631166	19.846631
54.573265	1830.524018	19.851648
54.964297	1830.270648	19.856666
55.002067	1830.681368	19.861683
54.849921	1834.053486	19.866701
55.316245	1814.471147	19.871719
54.752817	1824.241182	19.876736
54.819571	1825.897124	19.881754
54.873082	1826.037141	19.886771
55.087858	1808.049831	19.891789
54.736921	1818.664117	19.896807
54.822640	1823.220531	19.901824
55.505363	1834.289292	19.906842
55.231731	1838.431430	19.911859
55.447442	1830.549145	19.916877
55.308074	1830.807558	19.921895
55.421062	1838.117986	19.926912
55.765751	1830.083073	19.931930
55.462128	1838.840648	19.936947
55.887729	1836.363298	19.941965
55.769115	1835.087869	19.946983
55.236075	1843.079567	19.952000
55.731445	1849.633010	19.957018
55.617190	1836.219308	19.962035
55.404672	1836.561696	19.967053
55.575990	1839.653073	19.972071
55.706320	1851.398002	19.977088
55.894678	1848.626218	19.982106
55.771092	1860.716809	19.987123
55.795331	1857.194225	19.992141
55.777558	1855.821040	19.997159
55.657198	1866.162762	20.002176
56.439894	1878.661389	20.007194
56.622395	1886.109341	20.012211
56.582988	1879.267179	20.017229
56.658705	1885.658748	20.022247
56.566494	1888.011654	20.027264
56.772870	1877.637635	20.032282
56.936899	1877.993983	20.037299
56.705265	1875.521123	20.042317
56.784879	1877.111950	20.047335
56.446483	1875.678226	20.052352
56.785086	1871.267223	20.057370
56.537026	1877.491442	20.062387
56.825087	1873.908843	20.067405
57.115730	1874.567380	20.072423
56.950711	1894.917141	20.077440
57.164961	1898.295344	20.082458
57.199399	1906.653168	20.087475
57.117295	1902.260320	20.092493
57.413393	1901.844999	20.097511
57.248565	1899.579493	20.102528
57.387635	1903.679481	20.107546
57.494265	1900.191399	20.112563
57.251860	1903.227277	20.117581
57.329284	1899.365033	20.122599
57.213688	1921.553337	20.127616
57.745110	1905.605845	20.132634
57.516785	1922.594981	20.137651
57.889567	1925.292076	20.142669
57.954386	1917.994999	20.147687
57.933522	1927.292437	20.152704
57.668187	1929.798540	20.157722
58.056748	1924.025858	20.162739
58.287217	1925.324949	20.167757
58.091060	1921.584193	20.172775
58.532094	1927.798975	20.177792
58.534928	1930.746181	20.182810
58.221291	1925.534123	20.187827
58.105911	1929.547497	20.192845
58.805898	1937.536617	20.197863
58.767691	1949.241576	20.202880
58.663289	1947.970237	20.207898
58.558928	1944.909486	20.212915
58.665191	1939.376418	20.217933
58.572269	1943.793413	20.222951
58.469086	1943.291929	20.227968
58.512640	1949.451835	20.232986
59.167694	1938.499821	20.238003
58.810318	1938.890011	20.243021
58.944835	1946.967175	20.248039
58.844249	1962.863448	20.253056
58.875568	1960.785153	20.258074
59.279007	1964.809280	20.263091
59.170735	1974.057233	20.268109
59.294381	1973.949638	20.273127
58.966131	1969.958029	20.278144
59.320267	1969.764053	20.283162
59.673088	1972.413768	20.288179
59.598539	1983.692047	20.293197
60.002898	1983.098916	20.298215
59.738326	1976.165537	20.303232
59.916342	1962.873499	20.308250
60.225207	1957.028005	20.313267
60.157820	1959.752610	20.318285
59.806383	1964.080466	20.323303
59.893991	1964.006885	20.328320
60.108195	1956.796991	20.333338
60.517362	1954.713519	20.338355
59.970629	1962.915693	20.343373
60.416057	1948.379624	20.348391
60.486136	1950.659932	20.353408
59.924649	1950.958821	20.358426
60.262197	1952.518963	20.363443
60.254088	1967.731788	20.368461
60.623302	1972.231477	20.373479
60.252617	1983.843052	20.378496
60.524265	1972.051273	20.383514
60.976099	1976.130986	20.388531
60.827748	1973.398984	20.393549
60.686204	1970.520749	20.398567
60.741641	1980.494327	20.403584
60.719766	1978.560017	20.408602
61.072745	1974.058385	20.413619
61.136345	1973.477282	20.418637
61.199984	1977.304999	20.423655
60.850011	1982.121799	20.428672
61.061085	1997.420449	20.433690
61.453516	2001.664057	20.438707
61.659454	2005.857804	20.443725
61.461640	1996.016880	20.448743
61.805622	1995.190143	20.453760
62.012591	2002.239844	20.458778
61.936358	1996.148169	20.463795
61.783504	1991.946203	20.468813
61.698483	1985.259430	20.473831
61.877273	1993.298163	20.478848
61.721483	1986.417273	20.483866
62.084375	1991.381873	20.488883
61.660845	1997.084322	20.493901
61.937373	1990.502209	20.498919
61.819038	1994.434004	20.503936
61.721798	1984.608987	20.508954
61.649325	1979.548720	20.513971
61.954869	2002.369015	20.518989
62.309923	2008.685578	20.524007
62.083019	2018.759943	20.529024
61.764600	2018.610717	20.534042
62.118473	2016.813568	20.539059
62.393740	2033.490864	20.544077
62.539881	2036.497829	20.549095
62.621711	2046.700873	20.554112
62.645761	2048.688547	20.559130
62.934265	2041.672187	20.564147
62.411206	2051.467618	20.569165
62.406729	2050.650949	20.574183
62.648177	2056.723274	20.579200
62.880648	2065.574225	20.584218
62.941397	2071.122399	20.589235
62.830239	2070.748391	20.594253
63.228003	2068.395270	20.599271
63.696488	2065.908057	20.604288
63.277381	2062.545981	20.609306
63.486159	2059.139798	20.614323
63.164242	2060.209309	20.619341
63.643879	2068.340097	20.624359
63.819204	2080.321178	20.629376
64.083633	2085.755590	20.634394
64.488238	2078.064704	20.639411
64.428365	2073.882957	20.644429
64.168372	2069.748148	20.649447
64.539459	2055.766389	20.654464
64.213859	2054.150770	20.659482
64.470781	2051.942661	20.664499
64.583909	2056.845176	20.669517
64.170169	2058.563326	20.674535
64.309949	2057.620051	20.679552
64.237241	2055.807261	20.684570
64.405593	2051.589985	20.689587
64.236339	2060.090053	20.694605
64.355757	2046.639811	20.699623
64.541755	2052.667117	20.704640
64.357006	2051.108466	20.709658
64.296610	2043.698284	20.714675
64.463773	2056.397018	20.719693
64.186724	2066.280392	20.724711
64.524363	2070.239046	20.729728
64.702110	2082.506942	20.734746
65.019406	2076.489676	20.739763
64.653651	2082.069542	20.744781
65.188065	2088.613840	20.749799
65.467299	2097.151400	20.754816
65.435686	2113.409469	20.759834
65.500708	2100.794514	20.764851
65.046116	2099.129543	20.769869
65.228338	2094.111644	20.774887
65.390118	2099.407401	20.779904
65.215336	2105.920105	20.784922
65.328322	2101.272762	20.789939
65.648365	2108.787759	20.794957
65.285662	2112.751315	20.799975
65.615839	2125.011288	20.804992
65.853133	2131.276798	20.810010
65.937363	2121.505506	20.815027
65.897539	2130.455692	20.820045
66.213550	2125.300184	20.825063
66.087064	2132.275615	20.830080
65.619538	2132.746077	20.835098
66.143787	2141.453804	20.840115
66.380732	2143.929073	20.845133
66.508003	2142.568000	20.850151
66.809722	2150.177390	20.855168
66.874815	2138.490248	20.860186
67.082465	2144.829809	20.865203
66.818114	2153.467809	20.870221
66.660765	2141.572290	20.875239
66.794027	2141.267527	20.880256
66.730399	2142.457782	20.885274
66.651811	2140.216689	20.890291
66.679729	2146.013006	20.895309
66.738911	2146.360436	20.900327
67.014262	2163.097803	20.905344
67.343811	2162.936057	20.910362
67.375162	2166.143962	20.915379
67.052907	2167.235623	20.920397
67.237195	2163.861637	20.925415
67.289738	2164.661403	20.930432
67.325324	2170.727947	20.935450
67.502956	2165.060616	20.940467
67.280322	2177.911648	20.945485
67.756753	2182.000203	20.950503
68.160030	2182.751674	20.955520
67.817551	2187.731473	20.960538
67.856859	2184.645157	20.965555
67.798759	2190.811505	20.970573
67.834162	2185.699669	20.975591
68.105415	2179.209831	20.980608
67.959592	2179.746977	20.985626
67.928197	2187.016908	20.990643
68.193738	2194.303730	20.995661
68.289601	2212.148427	21.000679
68.440843	2206.456788	21.005696
67.975115	2211.872369	21.010714
68.558096	2207.880851	21.015731
68.537347	2208.183920	21.020749
68.388930	2206.853140	21.025767
68.663058	2216.420397	21.030784
68.839132	2221.994846	21.035802
69.119517	2227.815002	21.040819
69.095487	2228.692968	21.045837
69.285831	2235.016320	21.050855
69.299623	2223.744230	21.055872
69.017775	2229.314234	21.060890
69.499260	2226.083323	21.065907
69.419589	2229.639901	21.070925
69.285513	2229.130595	21.075943
69.822112	2229.618302	21.080960
69.882866	2224.044892	21.085978
69.667378	2232.006257	21.090995
69.622449	2228.718442	21.096013
69.838709	2216.988778	21.101031
69.865467	2224.464275	21.106048
69.756281	2220.564741	21.111066
69.827287	2217.363025	21.116083
69.989492	2231.650106	21.121101
70.353839	2248.701918	21.126119
70.262660	2256.675499	21.131136
70.295387	2250.929710	21.136154
70.206874	2242.883161	21.141171
70.587903	2248.589819	21.146189
70.369340	2248.803760	21.151207
70.509457	2239.071042	21.156224
70.195322	2242.083429	21.161242
70.400156	2246.580378	21.166259
70.576038	2249.336583	21.171277
70.489150	2264.760752	21.176295
70.909856	2265.512669	21.181312
70.896857	2266.988555	21.186330
71.170909	2266.238970	21.191347
71.148469	2266.930488	21.196365
71.083417	2272.245833	21.201383
71.273559	2269.786149	21.206400
70.972715	2278.496166	21.211418
71.154274	2267.974299	21.216435
71.439995	2280.017225	21.221453
71.093139	2283.050493	21.226471
71.331923	2286.563814	21.231488
71.630373	2285.977696	21.236506
71.497873	2291.290924	21.241523
71.909252	2291.675046	21.246541
71.646729	2298.779024	21.251559
72.060441	2298.559990	21.256576
71.894048	2303.032696	21.261594
71.970957	2307.480146	21.266611
72.017157	2308.142043	21.271629
72.083396	2317.467150	21.276647
72.603696	2309.310003	21.281664
72.305353	2310.874502	21.286682
72.451869	2321.058164	21.291699
72.435507	2312.798367	21.296717
72.272080	2323.311169	21.301735
72.390596	2315.308097	21.306752
72.427308	2325.966475	21.311770
72.757850	2339.444749	21.316787
73.288135	2344.029916	21.321805
73.117313	2341.967269	21.326823
73.257525	2335.254766	21.331840
73.243154	2348.026154	21.336858
73.271204	2339.450143	21.341875
73.460292	2336.536152	21.346893
73.008176	2338.859940	21.351911
73.441904	2331.110760	21.356928
73.537077	2326.396701	21.361946
73.637759	2323.704771	21.366963
73.808611	2326.906765	21.371981
73.712214	2333.767130	21.376999
73.548953	2336.677143	21.382016
73.749883	2330.816772	21.387034
73.660400	2337.534043	21.392051
73.741260	2325.957940	21.397069
73.470141	2329.298178	21.402087
73.902800	2337.370128	21.407104
73.622838	2347.493965	21.412122
73.769657	2356.216377	21.417139
74.019561	2348.827189	21.422157
73.840410	2367.910979	21.427175
74.528081	2364.303939	21.432192
75.316944	2354.362849	21.437210
75.394968	2357.651890	21.442227
75.740387	2339.463815	21.447245
75.224335	2342.229929	21.452263
75.344803	2333.106169	21.457280
75.191990	2327.089425	21.462298
75.301034	2324.352009	21.467315
75.485229	2330.799436	21.472333
75.043714	2329.656300	21.477351
75.016269	2322.184064	21.482368
74.855152	2331.494081	21.487386
74.873910	2325.895619	21.492403
75.238187	2324.718550	21.497421
75.536092	2337.633827	21.502439
75.473009	2351.624702	21.507456
75.410815	2358.063160	21.512474
75.326940	2354.629898	21.517491
75.748067	2358.196898	21.522509
75.176573	2362.170924	21.527527
75.638187	2359.375454	21.532544
75.584296	2379.566444	21.537562
75.823318	2385.396247	21.542579
75.777116	2381.016628	21.547597
75.376782	2385.592053	21.552615
75.939458	2399.166782	21.557632
76.232116	2408.040093	21.562650
76.131997	2405.666611	21.567667
76.264865	2406.378137	21.572685
76.398679	2429.998936	21.577703
76.746306	2425.356005	21.582720
76.619057	2434.484066	21.587738
76.706306	2442.414169	21.592755
76.748467	2433.198403	21.597773
76.803448	2433.830533	21.602791
76.900615	2430.476374	21.607808
76.899183	2444.306233	21.612826
76.886483	2456.515670	21.617843
77.122344	2455.200786	21.622861
77.221247	2457.568195	21.627879
77.496078	2454.637680	21.632896
77.574852	2454.290900	21.637914
77.443932	2459.001134	21.642931
78.043662	2463.259918	21.647949
77.545293	2471.909258	21.652967
77.559297	2469.407538	21.657984
77.728816	2479.556149	21.663002
77.807907	2480.929346	21.668019
77.773591	2479.072663	21.673037
77.776386	2485.946046	21.678055
77.790421	2476.538964	21.683072
78.150949	2489.286800	21.688090
78.347609	2506.942516	21.693107
78.417036	2500.275688	21.698125
78.083510	2505.273116	21.703143
78.217497	2496.907769	21.708160
78.440829	2502.266651	21.713178
78.373831	2506.982726	21.718195
78.658703	2508.131369	21.723213
78.781041	2513.016796	21.728231
79.138757	2518.992276	21.733248
79.193808	2522.051378	21.738266
79.263731	2529.144716	21.743283
78.884481	2521.042314	21.748301
78.883778	2522.939214	21.753319
78.867539	2524.693355	21.758336
79.067290	2533.388676	21.763354
79.253273	2546.959046	21.768371
79.558489	2542.057582	21.773389
79.269063	2541.162170	21.778407
79.877202	2544.649596	21.783424
79.912472	2552.849791	21.788442
79.710458	2566.123953	21.793459
80.029010	2556.786190	21.798477
80.082126	2566.280739	21.803495
80.028748	2561.712832	21.808512
79.791873	2568.598314	21.813530
80.226834	2568.246572	21.818547
80.311175	2560.403358	21.823565
80.332540	2590.855739	21.828583
80.468320	2590.878804	21.833600
80.801368	2592.534386	21.838618
80.585475	2598.072143	21.843635
81.020905	2592.724327	21.848653
80.774374	2600.532886	21.853671
80.942225	2594.355665	21.858688
81.335159	2590.406277	21.863706
80.880071	2594.573684	21.868723
81.263118	2591.799879	21.873741
81.183424	2594.109900	21.878759
81.022908	2606.695928	21.883776
81.256535	2609.859796	21.888794
81.410535	2616.204721	21.893811
81.638058	2609.342813	21.898829
81.460146	2613.318735	21.903847
81.646397	2621.012581	21.908864
81.866665	2613.908786	21.913882
81.628659	2630.104776	21.918899
81.960913	2633.991805	21.923917
82.218540	2637.903079	21.928935
82.202447	2633.594455	21.933952
82.203148	2631.186309	21.938970
82.243497	2629.444227	21.943987
82.316881	2629.833640	21.949005
82.346439	2631.498605	21.954023
82.216289	2638.512675	21.959040
82.349572	2649.948376	21.964058
82.528414	2660.701598	21.969075
82.982101	2654.126377	21.974093
83.091461	2650.337900	21.979111
83.025985	2651.790428	21.984128
83.362984	2651.539150	21.989146
82.825538	2654.718927	21.994163
82.852586	2651.356707	21.999181
83.583106	2656.829189	22.004199
83.853450	2662.464843	22.009216
83.709948	2645.722305	22.014234
83.553686	2651.506433	22.019251
83.543957	2640.240899	22.024269
83.744301	2650.754065	22.029287
84.079527	2666.235943	22.034304
84.408383	2660.680622	22.039322
84.350333	2660.535035	22.044339
84.306127	2644.676510	22.049357
84.248056	2637.092138	22.054375
84.064791	2630.818081	22.059392
84.458852	2635.531838	22.064410
84.247044	2662.612122	22.069427
84.485967	2662.032105	22.074445
84.526689	2665.743607	22.079463
84.441057	2661.114419	22.084480
84.477423	2657.930642	22.089498
84.465825	2669.003875	22.094515
84.469962	2671.269294	22.099533
84.847053	2685.551686	22.104551
84.461389	2692.820170	22.109568
84.695825	2692.234539	22.114586
85.060723	2692.420764	22.119603
85.031109	2693.129195	22.124621
85.253791	2702.158726	22.129639
85.484758	2716.422864	22.134656
85.519796	2717.821875	22.139674
85.282418	2712.228454	22.144691
85.389376	2717.308850	22.149709
85.577325	2708.786669	22.154727
85.730016	2723.315484	22.159744
85.829200	2741.807182	22.164762
85.705000	2743.328825	22.169779
85.839476	2739.555356	22.174797
85.957842	2739.994577	22.179815
86.116266	2754.175358	22.184832
86.192953	2762.287143	22.189850
86.303723	2759.315844	22.194867
86.446718	2769.080553	22.199885
86.615765	2764.796726	22.204903
86.553859	2770.225346	22.209920
87.201098	2777.872735	22.214938
86.954649	2782.935584	22.219955
87.308713	2786.623575	22.224973
87.226268	2784.168389	22.229991
87.235709	2789.510161	22.235008
87.442873	2782.114826	22.240026
87.360438	2790.115686	22.245043
87.327282	2783.799268	22.250061
87.431769	2787.409343	22.255079
87.330377	2792.061413	22.260096
87.311884	2778.224962	22.265114
87.637938	2795.387408	22.270131
87.836661	2796.536859	22.275149
88.144574	2808.718710	22.280167
87.669905	2821.227556	22.285184
88.116411	2813.002770	22.290202
88.221363	2811.623029	22.295219
88.290620	2808.083780	22.300237
88.391717	2801.156269	22.305255
88.117286	2811.935968	22.310272
88.343211	2822.823980	22.315290
88.565272	2830.534433	22.320307
88.634907	2828.592096	22.325325
88.797080	2830.362674	22.330343
88.861452	2828.683110	22.335360
88.580575	2824.772302	22.340378
89.032142	2842.562246	22.345395
88.992665	2852.734139	22.350413
89.380099	2852.976824	22.355431
89.469609	2849.983571	22.360448
89.515644	2849.913304	22.365466
89.402612	2847.481808	22.370483
89.391968	2855.364214	22.375501
89.438214	2853.375018	22.380519
89.521995	2854.785387	22.385536
89.930289	2861.415884	22.390554
90.167668	2865.008439	22.395571
89.881837	2857.317411	22.400589
90.317418	2856.413255	22.405607
90.083082	2863.752929	22.410624
90.107640	2856.392306	22.415642
90.327890	2855.758381	22.420659
90.164546	2852.176436	22.425677
90.319613	2861.320724	22.430695
90.479699	2879.670528	22.435712
90.867034	2886.102308	22.440730
90.611667	2880.555820	22.445747
90.353536	2892.081022	22.450765
90.750745	2886.035264	22.455783
90.959925	2897.279410	22.460800
91.142020	2910.310970	22.465818
91.835128	2903.436427	22.470835
91.352687	2910.306618	22.475853
91.495864	2904.104728	22.480871
91.322755	2921.976228	22.485888
91.649771	2905.586263	22.490906
91.576351	2909.236685	22.495923
91.227717	2921.953216	22.500941
91.453480	2934.242626	22.505959
91.708799	2934.669998	22.510976
91.635520	2939.324041	22.515994
91.961229	2954.198524	22.521011
92.439720	2949.800197	22.526029
92.718626	2953.515705	22.531047
92.764735	2950.093652	22.536064
92.948326	2951.157099	22.541082
93.083146	2960.175190	22.546099
92.742929	2962.039781	22.551117
92.738631	2955.731434	22.556135
92.691330	2960.169980	22.561152
92.862884	2950.883305	22.566170
93.296357	2960.836444	22.571187
93.113553	2973.508257	22.576205
93.701808	2985.848572	22.581223
93.597245	2980.373257	22.586240
93.871583	2980.400000	22.591258
93.999495	2982.494694	22.596275
93.550266	2982.154365	22.601293
94.032979	2977.660690	22.606311
93.562033	2978.633524	22.611328
94.106676	2976.853922	22.616346
94.116931	2983.562217	22.621363
93.980738	2973.995210	22.626381
94.123426	2973.692123	22.631399
94.135747	2988.669081	22.636416
94.170534	2995.275722	22.641434
94.519371	3007.735386	22.646451
94.415852	3003.162548	22.651469
95.082742	2998.930555	22.656487
94.937865	3001.171874	22.661504
94.889092	2995.937201	22.666522
94.776068	2996.904807	22.671539
94.730360	3018.253530	22.676557
95.145951	3020.148790	22.681575
95.438604	3032.513067	22.686592
95.390102	3034.862474	22.691610
95.385341	3020.714400	22.696627
95.377899	3026.895240	22.701645
95.541047	3018.604014	22.706663
95.129624	3032.659120	22.711680
95.803030	3040.630785	22.716698
95.995558	3043.494985	22.721715
95.810161	3050.656686	22.726733
96.006971	3045.598378	22.731751
95.938402	3051.305859	22.736768
96.008941	3047.131985	22.741786
95.982300	3060.281368	22.746803
96.273553	3072.453367	22.751821
96.246019	3066.435806	22.756839
96.829482	3068.708917	22.761856
96.684760	3074.270456	22.766874
97.071536	3062.390604	22.771891
96.545985	3075.059042	22.776909
97.000928	3085.280334	22.781927
97.555656	3088.154428	22.786944
97.626802	3085.334426	22.791962
97.502367	3079.827458	22.796979
97.765633	3081.910558	22.801997
97.566715	3070.996134	22.807015
97.489538	3074.246348	22.812032
97.563886	3082.339705	22.817050
97.652735	3078.109319	22.822067
97.523507	3090.955928	22.827085
98.050462	3101.055553	22.832103
97.825758	3099.162169	22.837120
97.909358	3107.140476	22.842138
98.314426	3104.864990	22.847155
98.167893	3114.261512	22.852173
98.513330	3112.153115	22.857191
98.425601	3131.589592	22.862208
98.459644	3128.352439	22.867226
98.579792	3127.809837	22.872243
98.408271	3138.857761	22.877261
98.919282	3154.123325	22.882279
99.114348	3147.430385	22.887296
98.670337	3155.017439	22.892314
99.178632	3154.976196	22.897331
99.259026	3168.942212	22.902349
99.536562	3182.473560	22.907367
99.462340	3192.000890	22.912384
99.584222	3189.485431	22.917402
99.716548	3178.699269	22.922419
99.874894	3175.527970	22.927437
99.644873	3176.567455	22.932455
100.124032	3191.825386	22.937472
100.011204	3213.563528	22.942490
100.295286	3201.175654	22.947507
100.500407	3219.490388	22.952525
100.518386	3209.255399	22.957543
100.492190	3209.111160	22.962560
100.568267	3210.756311	22.967578
100.944057	3210.599985	22.972595
100.783456	3222.040776	22.977613
100.735546	3225.128653	22.982631
101.019143	3226.542659	22.987648
100.696676	3230.083582	22.992666
100.881854	3230.338826	22.997683
101.085722	3242.821224	23.002701
100.993115	3243.359584	23.007719
101.560459	3248.179083	23.012736
101.119111	3266.253651	23.017754
101.409624	3268.376718	23.022771
101.505319	3275.475806	23.027789
101.680890	3274.634206	23.032807
102.187712	3270.499664	23.037824
102.602349	3286.522041	23.042842
102.791154	3279.100955	23.047859
102.641801	3268.472216	23.052877
102.665207	3258.072234	23.057895
102.729340	3256.238017	23.062912
102.696006	3266.093572	23.067930
102.760822	3271.660422	23.072947
102.793340	3285.160559	23.077965
102.978441	3288.568814	23.082983
103.312159	3282.974671	23.088000
103.134786	3283.482044	23.093018
103.455959	3279.029227	23.098035
103.482732	3291.403517	23.103053
103.501112	3290.415957	23.108071
103.585553	3274.694654	23.113088
103.628891	3287.082143	23.118106
103.689371	3298.327599	23.123123
103.690463	3310.106230	23.128141
103.821106	3314.665498	23.133159
104.141378	3311.803518	23.138176
103.959826	3313.611880	23.143194
103.986775	3318.364038	23.148211
104.286746	3332.371742	23.153229
104.174519	3343.707238	23.158247
104.585607	3328.563110	23.163264
104.554629	3336.057528	23.168282
104.588918	3346.230839	23.173299
104.930502	3356.129069	23.178317
104.578595	3367.858544	23.183335
105.079780	3358.763364	23.188352
104.811810	3365.767612	23.193370
104.786595	3380.766521	23.198387
105.185216	3391.842611	23.203405
105.153266	3396.575554	23.208423
105.240076	3402.205299	23.213440
105.184748	3417.344642	23.218458
105.532181	3407.635828	23.223475
105.612431	3422.321670	23.228493
105.818370	3431.527765	23.233511
106.396223	3433.962763	23.238528
106.526668	3429.725819	23.243546
106.835003	3423.592722	23.248563
106.693057	3431.498979	23.253581
106.744657	3435.060606	23.258599
106.917053	3428.178565	23.263616
106.836037	3423.062410	23.268634
107.160371	3431.972327	23.273651
107.151467	3440.650076	23.278669
107.479576	3446.930314	23.283687
107.643712	3445.875865	23.288704
107.621855	3454.157958	23.293722
107.849857	3448.324573	23.298739
107.646113	3450.672954	23.303757
107.791549	3446.392642	23.308775
108.015705	3442.049576	23.313792
107.669619	3445.335411	23.318810
107.406869	3445.739301	23.323827
107.661761	3462.247509	23.328845
107.956994	3473.554367	23.333863
108.238176	3471.695803	23.338880
108.171675	3474.325813	23.343898
108.655842	3488.806795	23.348915
108.912850	3491.891431	23.353933
108.742615	3500.992006	23.358951
109.109690	3494.562527	23.363968
108.733042	3500.807325	23.368986
108.926180	3496.491168	23.374003
109.019946	3496.123098	23.379021
108.600156	3503.334095	23.384039
109.017112	3504.484334	23.389056
109.145944	3518.872322	23.394074
109.414285	3517.681710	23.399091
109.736170	3524.657308	23.404109
109.574772	3533.829116	23.409127
110.219325	3539.738187	23.414144
110.312702	3530.097267	23.419162
110.281681	3524.847051	23.424179
110.728680	3525.790618	23.429197
110.250569	3535.665070	23.434215
110.663296	3524.112276	23.439232
110.514212	3530.252218	23.444250
111.094594	3529.366516	23.449267
110.935078	3525.793309	23.454285
110.964166	3529.049153	23.459303
111.109323	3528.966607	23.464320
111.044093	3530.122484	23.469338
110.997346	3541.997089	23.474355
111.134536	3541.170920	23.479373
111.272650	3558.167671	23.484391
111.681433	3553.009939	23.489408
111.769113	3564.816287	23.494426
111.546378	3567.505353	23.499443
111.705517	3579.445770	23.504461
111.381062	3581.367937	23.509479
111.965349	3578.452185	23.514496
111.874217	3593.777155	23.519514
111.947263	3600.851492	23.524531
112.382032	3603.810629	23.529549
112.248750	3611.273746	23.534567
112.854946	3615.866362	23.539584
112.974981	3624.760840	23.544602
113.235297	3627.655611	23.549619
113.405470	3625.015793	23.554637
113.294510	3625.894737	23.559655
113.701190	3620.248100	23.564672
113.587678	3619.602990	23.569690
113.449935	3619.094213	23.574707
113.620885	3616.397464	23.579725
113.596245	3625.112469	23.584743
113.869056	3634.238819	23.589760
113.894518	3645.818190	23.594778
114.190311	3650.036209	23.599795
113.967689	3648.218191	23.604813
113.990039	3651.907508	23.609831
114.402850	3646.831185	23.614848
114.357397	3654.618360	23.619866
114.508419	3667.402810	23.624883
114.957484	3674.071449	23.629901
114.740073	3681.500349	23.634919
115.003350	3673.559355	23.639936
115.102452	3672.789610	23.644954
115.147472	3688.446959	23.649971
115.158896	3688.757669	23.654989
115.145071	3699.364761	23.660007
115.311846	3700.102624	23.665024
115.240893	3706.287273	23.670042
115.805263	3707.944821	23.675059
115.867038	3720.244518	23.680077
115.760796	3725.800266	23.685095
115.979419	3721.208652	23.690112
116.074212	3726.490071	23.695130
116.097252	3736.071983	23.700147
116.395875	3743.404785	23.705165
116.194154	3749.814964	23.710183
116.702514	3745.247672	23.715200
116.072456	3753.627750	23.720218
116.402337	3753.828910	23.725235
116.619613	3769.895072	23.730253
116.453871	3770.851989	23.735271
117.030355	3779.082104	23.740288
117.396577	3789.787892	23.745306
117.340904	3800.051216	23.750323
117.192755	3798.322587	23.755341
117.312629	3806.263994	23.760359
118.017080	3814.316391	23.765376
118.103887	3818.251362	23.770394
118.157804	3815.048867	23.775411
118.334125	3802.046111	23.780429
118.044551	3816.508948	23.785447
118.709849	3817.551106	23.790464
118.732762	3813.914720	23.795482
118.567897	3810.762069	23.800499
118.788734	3825.057071	23.805517
118.968360	3829.608844	23.810535
119.249172	3824.672959	23.815552
119.097509	3831.466748	23.820570
119.422728	3829.882198	23.825587
119.746292	3821.559316	23.830605
118.952757	3823.283102	23.835623
119.124467	3827.416326	23.840640
119.672888	3837.901244	23.845658
119.827319	3846.869382	23.850675
120.188814	3846.939372	23.855693
120.246059	3854.615958	23.860711
120.341653	3854.878846	23.865728
120.026371	3846.551259	23.870746
120.246383	3862.926390	23.875763
120.102312	3875.062554	23.880781
120.268295	3878.035178	23.885799
120.409742	3889.236834	23.890816
120.732219	3892.286096	23.895834
120.722532	3900.604374	23.900851
121.208612	3897.637581	23.905869
121.051681	3901.493737	23.910887
121.302216	3925.682235	23.915904
121.449329	3923.629874	23.920922
121.143171	3925.703884	23.925939
121.837467	3932.924661	23.930957
121.411043	3946.503059	23.935975
122.072492	3947.141822	23.940992
122.007680	3951.302430	23.946010
122.103963	3936.718122	23.951027
122.241223	3956.297209	23.956045
122.417954	3962.582259	23.961063
122.639407	3964.962351	23.966080
122.871754	3959.882474	23.971098
122.761767	3955.597621	23.976115
123.129315	3966.666279	23.981133
123.037725	3983.967478	23.986151
123.088016	3986.522566	23.991168
123.272211	3983.656417	23.996186
123.278998	3992.171017	24.001203
123.363792	3986.451288	24.006221
123.697785	4003.260148	24.011239
123.693271	4011.495608	24.016256
124.200612	4015.636589	24.021274
123.963969	4012.110012	24.026291
124.026247	4009.723658	24.031309
124.205720	4017.801068	24.036327
124.137122	4028.034971	24.041344
124.607024	4032.850918	24.046362
124.464872	4038.150380	24.051379
124.724339	4036.572894	24.056397
124.780884	4041.588919	24.061415
124.991650	4042.468293	24.066432
125.172650	4059.894407	24.071450
125.202383	4061.224910	24.076467
125.295473	4062.438235	24.081485
125.156740	4058.331430	24.086503
125.358454	4075.176733	24.091520
125.734971	4074.518438	24.096538
125.957275	4083.545566	24.101555
126.178637	4076.491528	24.106573
126.055174	4084.827604	24.111591
126.442107	4074.247459	24.116608
126.893012	4071.305053	24.121626
126.776543	4083.402340	24.126643
127.087701	4094.568232	24.131661
127.175770	4092.995332	24.136679
127.171227	4083.325174	24.141696
127.082550	4094.155624	24.146714
126.859888	4093.240267	24.151731
127.250922	4085.367578	24.156749
127.283740	4094.856625	24.161767
127.446482	4103.896193	24.166784
127.903563	4108.067115	24.171802
127.632791	4116.760708	24.176819
127.896706	4123.619313	24.181837
127.841005	4115.970823	24.186855
127.543645	4120.530650	24.191872
127.681085	4129.277477	24.196890
127.855664	4154.633314	24.201907
128.061460	4165.885093	24.206925
128.341147	4171.352484	24.211943
128.248478	4176.050897	24.216960
128.500612	4195.138911	24.221978
128.699261	4205.075645	24.226995
129.126205	4207.723626	24.232013
129.399666	4216.449318	24.237031
129.711785	4220.784870	24.242048
129.887340	4216.392372	24.247066
129.624285	4220.981603	24.252083
130.056193	4222.258971	24.257101
129.744113	4213.482518	24.262119
130.056761	4221.892793	24.267136
130.388273	4240.479268	24.272154
130.355720	4243.631210	24.277171
130.586138	4249.485055	24.282189
130.671699	4248.439638	24.287207
130.550674	4250.611114	24.292224
130.690865	4267.118979	24.297242
131.104698	4276.965436	24.302259
131.231309	4263.963775	24.307277
131.664894	4267.882731	24.312295
131.458421	4269.865508	24.317312
131.919198	4260.889796	24.322330
131.707372	4273.579664	24.327347
131.733151	4281.535930	24.332365
132.042615	4287.124974	24.337383
132.278982	4290.493875	24.342400
132.339856	4293.915350	24.347418
132.211380	4297.300022	24.352435
132.286120	4295.656584	24.357453
132.549021	4303.058304	24.362471
132.485912	4304.876730	24.367488
132.998283	4308.625611	24.372506
132.762812	4314.069093	24.377523
132.772492	4324.284663	24.382541
133.089997	4328.979225	24.387559
133.409989	4326.776805	24.392576
133.746529	4325.695465	24.397594
133.833136	4323.630384	24.402611
133.943520	4318.919749	24.407629
133.860170	4325.078133	24.412647
133.762263	4339.606236	24.417664
134.319661	4341.631066	24.422682
134.367736	4340.926052	24.427699
134.324487	4348.359673	24.432717
134.560477	4341.154907	24.437735
134.324369	4346.156610	24.442752
134.479159	4361.702761	24.447770
134.653148	4368.578616	24.452787
135.018193	4369.730683	24.457805
135.187681	4372.134702	24.462823
135.245095	4385.470812	24.467840
135.629479	4393.071443	24.472858
135.607840	4385.300751	24.477875
135.629522	4394.182514	24.482893
135.705170	4392.008660	24.487911
136.036186	4414.815428	24.492928
136.263830	4410.405305	24.497946
136.218924	4414.095780	24.502963
136.477653	4419.800080	24.507981
136.459500	4417.675546	24.512999
136.366572	4447.905819	24.518016
136.866365	4449.245232	24.523034
136.966195	4448.323836	24.528051
137.047522	4459.816122	24.533069
137.191042	4459.626512	24.538087
137.169120	4474.234427	24.543104
137.185169	4468.291678	24.548122
137.245442	4482.754235	24.553139
137.462519	4491.141639	24.558157
137.785599	4494.538111	24.563175
137.809631	4502.355866	24.568192
137.872018	4505.748738	24.573210
138.389008	4521.462738	24.578227
138.151804	4526.508850	24.583245
138.716525	4537.439844	24.588263
138.386456	4544.722506	24.593280
138.747758	4556.796226	24.598298
138.717843	4554.241084	24.603315
138.870847	4568.020121	24.608333
139.029233	4574.030479	24.613351
139.091685	4582.211583	24.618368
139.579991	4600.123802	24.623386
139.952674	4590.296795	24.628403
140.245221	4598.950261	24.633421
140.301120	4605.696241	24.638439
140.156976	4615.598192	24.643456
140.439070	4596.183561	24.648474
140.561839	4599.219847	24.653491
140.485953	4616.534987	24.658509
140.909960	4620.190374	24.663527
141.010697	4626.443298	24.668544
141.004973	4622.129429	24.673562
140.886534	4633.229971	24.678579
140.870127	4645.147921	24.683597
141.573470	4655.593415	24.688615
141.455298	4656.962771	24.693632
141.568295	4656.231855	24.698650
141.503339	4673.286523	24.703667
141.318588	4685.697856	24.708685
141.527227	4682.098664	24.713703
141.580436	4692.942101	24.718720
142.023474	4708.585711	24.723738
141.999571	4719.242316	24.728755
142.043129	4727.360143	24.733773
142.717089	4735.199910	24.738791
142.619704	4750.599429	24.743808
142.847512	4740.103644	24.748826
143.498976	4749.525124	24.753843
143.716542	4739.838974	24.758861
143.668063	4736.342931	24.763879
143.829996	4742.109750	24.768896
144.257871	4731.630167	24.773914
144.359656	4725.951748	24.778931
144.758682	4732.748516	24.783949
144.715452	4726.240446	24.788967
144.737517	4722.809176	24.793984
144.814982	4725.991419	24.799002
145.215176	4737.298511	24.804019
144.874305	4746.486249	24.809037
145.449923	4741.867205	24.814055
144.991824	4747.901005	24.819072
145.116818	4743.071199	24.824090
145.465077	4744.042833	24.829107
145.527592	4744.831693	24.834125
145.592595	4751.339580	24.839143
145.866607	4763.717418	24.844160
146.034693	4762.955826	24.849178
145.966960	4764.175299	24.854195
145.578021	4782.025424	24.859213
146.092050	4789.801735	24.864231
146.514437	4799.716588	24.869248
146.230917	4808.617663	24.874266
146.885501	4816.100651	24.879283
146.757038	4825.214325	24.884301
146.836204	4823.286073	24.889319
147.177614	4840.530144	24.894336
147.546208	4850.245075	24.899354
147.410403	4853.937166	24.904371
147.356696	4856.830524	24.909389
147.089947	4863.841472	24.914407
147.505068	4878.668904	24.919424
147.588542	4893.361753	24.924442
147.613575	4899.822257	24.929459
147.858878	4918.508074	24.934477
148.650264	4918.457482	24.939495
148.285015	4935.110934	24.944512
148.516372	4945.974133	24.949530
149.051606	4960.549355	24.954547
148.792342	4962.849757	24.959565
149.492882	4976.606987	24.964583
149.338629	4981.261536	24.969600
149.463851	4987.744350	24.974618
149.639997	4984.131219	24.979635
149.972425	4995.821485	24.984653
150.244322	5002.177305	24.989671
150.084598	5004.727357	24.994688
150.168939	5013.410281	24.999706
150.523057	5020.649740	25.004723
150.484861	5029.948319	25.009741
150.622074	5032.767791	25.014759
150.652504	5052.175308	25.019776
150.913912	5058.122441	25.024794
151.268248	5064.500169	25.029811
151.672677	5062.660135	25.034829
151.504185	5068.200733	25.039847
151.667778	5086.274465	25.044864
151.954440	5082.994476	25.049882
152.016696	5084.948128	25.054899
151.992609	5097.681940	25.059917
151.933875	5104.853138	25.064935
152.193776	5096.921519	25.069952
152.536827	5112.401126	25.074970
152.311529	5125.466149	25.079987
152.879027	5134.137037	25.085005
152.986733	5126.891960	25.090023
153.146648	5131.150421	25.095040
153.382806	5156.592768	25.100058
153.468533	5146.680723	25.105075
153.214869	5149.961941	25.110093
153.657917	5152.165650	25.115111
153.763343	5162.742406	25.120128
154.248505	5166.486236	25.125146
154.468609	5181.262210	25.130163
154.424667	5174.034411	25.135181
154.896984	5178.875543	25.140199
154.919408	5207.024779	25.145216
154.602246	5198.062405	25.150234
155.219728	5205.163084	25.155251
155.117981	5204.250939	25.160269
155.164043	5208.009480	25.165287
155.640306	5227.846498	25.170304
155.730634	5232.475658	25.175322
155.866739	5227.252589	25.180339
155.550010	5242.872907	25.185357
155.933291	5245.489964	25.190375
155.679825	5257.779812	25.195392
156.356633	5266.222260	25.200410
156.823823	5277.478225	25.205427
156.419681	5288.901419	25.210445
156.485342	5284.475271	25.215463
157.120097	5302.813608	25.220480
157.177879	5302.596304	25.225498
157.367275	5303.081349	25.230515
157.291955	5318.825129	25.235533
157.895073	5329.005689	25.240551
157.856264	5330.757303	25.245568
157.983669	5337.804918	25.250586
158.353785	5337.460074	25.255603
158.312138	5357.721927	25.260621
158.356195	5352.658352	25.265639
158.301196	5361.981813	25.270656
158.628237	5374.853699	25.275674
158.659706	5377.427697	25.280691
158.886254	5387.240788	25.285709
159.350632	5398.999153	25.290727
159.672690	5401.950887	25.295744
159.619490	5409.597978	25.300762
160.013500	5399.757747	25.305779
159.910766	5421.989383	25.310797
160.061167	5428.604165	25.315815
160.577655	5425.982770	25.320832
160.858860	5423.590554	25.325850
161.006979	5415.306886	25.330867
161.163946	5426.974244	25.335885
161.362619	5415.115829	25.340903
161.632053	5428.568053	25.345920
161.589521	5441.828961	25.350938
161.594333	5442.964585	25.355955
161.848043	5445.942749	25.360973
161.974240	5437.873972	25.365991
161.916327	5439.761145	25.371008
162.327184	5445.644103	25.376026
162.113104	5445.235540	25.381043
162.018659	5454.735643	25.386061
162.253149	5456.801407	25.391079
162.100237	5469.448213	25.396096
162.423524	5485.351036	25.401114
162.830266	5485.776995	25.406131
162.634692	5501.826901	25.411149
162.728668	5516.919500	25.416167
163.378133	5512.724370	25.421184
163.135509	5532.184380	25.426202
163.488786	5528.534095	25.431219
163.611687	5542.886737	25.436237
164.066899	5550.113826	25.441255
164.241675	5558.464119	25.446272
164.087768	5569.889565	25.451290
164.455038	5559.860861	25.456307
164.512614	5571.610072	25.461325
164.822722	5592.915903	25.466343
165.205212	5584.961829	25.471360
164.866531	5597.612394	25.476378
165.429451	5604.178798	25.481395
165.554835	5612.710417	25.486413
165.692158	5615.975037	25.491431
166.091689	5625.060569	25.496448
165.993799	5635.887058	25.501466
166.204201	5632.451547	25.506483
166.078350	5637.171285	25.511501
166.411580	5650.740004	25.516519
166.830290	5656.123071	25.521536
167.210576	5654.296208	25.526554
167.217820	5659.976923	25.531571
167.391008	5665.306677	25.536589
167.640477	5671.650442	25.541607
167.663661	5682.669599	25.546624
167.529579	5692.299102	25.551642
167.795313	5688.785522	25.556659
168.057653	5708.744755	25.561677
167.892254	5717.053385	25.566695
168.407016	5711.294582	25.571712
168.449485	5734.009044	25.576730
168.723850	5733.555994	25.581747
168.881826	5731.025096	25.586765
168.752928	5742.049027	25.591783
169.289271	5762.221343	25.596800
169.006908	5766.817122	25.601818
169.126608	5776.028368	25.606835
169.729731	5790.123357	25.611853
169.534585	5794.181570	25.616871
170.041065	5806.921659	25.621888
169.928485	5817.819987	25.626906
170.101313	5819.810166	25.631923
170.337360	5840.812157	25.636941
170.460160	5847.248307	25.641959
170.675796	5854.957898	25.646976
170.853972	5863.364620	25.651994
171.206504	5873.212022	25.657011
171.415537	5881.724430	25.662029
171.198013	5889.892893	25.667047
171.841253	5895.638807	25.672064
171.723011	5908.877119	25.677082
172.388194	5911.380939	25.682100
172.617145	5915.565705	25.687117
172.507791	5917.656646	25.692135
172.834893	5926.393752	25.697152
172.842027	5935.717302	25.702170
172.724756	5945.300129	25.707188
173.189068	5954.050609	25.712205
173.222633	5965.273500	25.717223
173.551802	5969.448989	25.722240
173.465586	5975.744111	25.727258
173.741135	5981.493635	25.732276
173.924506	5991.923004	25.737293
174.053798	6001.849425	25.742311
173.883709	6012.254919	25.747328
174.296580	6020.151680	25.752346
174.691054	6020.993083	25.757364
174.481451	6036.628967	25.762381
174.751967	6046.246171	25.767399
175.067225	6056.430922	25.772416
174.687398	6063.854513	25.777434
175.457020	6080.815286	25.782452
175.225783	6081.536299	25.787469
175.753628	6100.346645	25.792487
176.301716	6101.988019	25.797504
176.031186	6099.154457	25.802522
176.350467	6113.063453	25.807540
176.731532	6119.983493	25.812557
176.560189	6125.619553	25.817575
176.689371	6122.079800	25.822592
176.511502	6137.130006	25.827610
177.558490	6140.556134	25.832628
177.667637	6141.792353	25.837645
177.826422	6161.187381	25.842663
177.948098	6160.041534	25.847680
178.241941	6167.720141	25.852698
178.031635	6161.865744	25.857716
178.592236	6173.789560	25.862733
178.500054	6190.515281	25.867751
178.923883	6186.140477	25.872768
179.224649	6188.319117	25.877786
178.961264	6190.866532	25.882804
179.661753	6206.660753	25.887821
179.630189	6208.247176	25.892839
179.965489	6218.580418	25.897856
180.119187	6212.003276	25.902874
179.978009	6230.245547	25.907892
180.329299	6234.910093	25.912909
180.291973	6233.261832	25.917927
180.454540	6231.405677	25.922944
180.821641	6242.526305	25.927962
180.899271	6249.900846	25.932980
181.059909	6247.842963	25.937997
180.924086	6270.989905	25.943015
181.103235	6284.744076	25.948032
181.785581	6285.928944	25.953050
181.298383	6302.927764	25.958068
181.857442	6298.061535	25.963085
181.852620	6321.244966	25.968103
181.980773	6326.187340	25.973120
182.032530	6335.254769	25.978138
182.563306	6353.373606	25.983156
182.468679	6350.171696	25.988173
183.310001	6377.387132	25.993191
183.445833	6390.289507	25.998208
183.452676	6387.147552	26.003226
183.586252	6392.155391	26.008244
183.972574	6393.938776	26.013261
184.212443	6410.328898	26.018279
184.524899	6403.903746	26.023296
184.773798	6409.079880	26.028314
184.620492	6415.420322	26.033332
185.070946	6421.142755	26.038349
185.041134	6430.346042	26.043367
185.078113	6431.322040	26.048384
185.690452	6442.063685	26.053402
185.528545	6466.032521	26.058420
185.858874	6457.022381	26.063437
185.568887	6450.719417	26.068455
186.058069	6457.496485	26.073472
186.371826	6475.857574	26.078490
186.229044	6484.036762	26.083508
186.469974	6492.105707	26.088525
186.478096	6505.874045	26.093543
186.506779	6506.115825	26.098560
187.327692	6514.072385	26.103578
186.855983	6527.233593	26.108596
187.045633	6529.622134	26.113613
187.429395	6542.315553	26.118631
187.706351	6556.843881	26.123648
187.688951	6554.914698	26.128666
187.902596	6572.634872	26.133684
188.046185	6585.005847	26.138701
188.376547	6596.687994	26.143719
188.530517	6608.833241	26.148736
188.701820	6618.185244	26.153754
188.449530	6627.394857	26.158772
189.151361	6642.074920	26.163789
188.988495	6657.473615	26.168807
189.606199	6658.365526	26.173824
190.036442	6668.810512	26.178842
189.861446	6672.101849	26.183860
190.380669	6680.856758	26.188877
189.876455	6696.760045	26.193895
190.371853	6717.227058	26.198912
190.838261	6721.444489	26.203930
190.899777	6722.549266	26.208948
191.190925	6745.071587	26.213965
191.155422	6759.238345	26.218983
191.329801	6764.369360	26.224000
191.750138	6771.100442	26.229018
191.582003	6782.702481	26.234036
192.036557	6787.745688	26.239053
192.172723	6807.479540	26.244071
192.108469	6806.201605	26.249088
192.610013	6831.286137	26.254106
192.821608	6840.284737	26.259124
193.455123	6846.802721	26.264141
193.597793	6852.462722	26.269159
193.686524	6861.177410	26.274176
193.847320	6863.529450	26.279194
193.931003	6877.848209	26.284212
194.180317	6879.223652	26.289229
194.673714	6891.736092	26.294247
194.865046	6905.324681	26.299264
195.076472	6908.675857	26.304282
194.833834	6906.478653	26.309300
195.039795	6908.994132	26.314317
195.410150	6924.145882	26.319335
195.525803	6937.206466	26.324352
196.201271	6930.004867	26.329370
195.705085	6947.150894	26.334388
195.783453	6954.131005	26.339405
196.209514	6960.987538	26.344423
196.526703	6977.009413	26.349440
196.811553	6982.195897	26.354458
196.764758	6989.422797	26.359476
196.936392	6995.561323	26.364493
197.205029	7011.354028	26.369511
197.428040	7011.221468	26.374528
197.617194	7038.798285	26.379546
197.834996	7044.806524	26.384564
198.254807	7048.769272	26.389581
198.247842	7064.901670	26.394599
198.493420	7071.192863	26.399616
198.661347	7071.700242	26.404634
198.527548	7090.775617	26.409652
198.962776	7096.210207	26.414669
199.123078	7092.927438	26.419687
199.491876	7104.578673	26.424704
199.824499	7104.934138	26.429722
200.022731	7110.509805	26.434740
200.351495	7119.439791	26.439757
200.909099	7127.222953	26.444775
200.782223	7124.319511	26.449792
201.100055	7116.823113	26.454810
201.172072	7121.323017	26.459828
201.470777	7110.363411	26.464845
201.606161	7114.563021	26.469863
201.648141	7111.961602	26.474880
202.038237	7114.612597	26.479898
201.953571	7130.618250	26.484916
202.312488	7134.230620	26.489933
202.213129	7123.999069	26.494951
201.885232	7141.267446	26.499968
202.472759	7158.099734	26.504986
202.823563	7165.103804	26.510004
203.227009	7180.424240	26.515021
203.372039	7195.926979	26.520039
203.510156	7189.314032	26.525056
203.763671	7186.805942	26.530074
204.154297	7209.158662	26.535092
204.332352	7204.821883	26.540109
204.589972	7212.077242	26.545127
204.295980	7212.656540	26.550144
204.830541	7214.132813	26.555162
204.796093	7230.465360	26.560180
205.404883	7239.661179	26.565197
205.303218	7247.515464	26.570215
205.406226	7260.205740	26.575232
205.979772	7256.887017	26.580250
205.707055	7263.902965	26.585268
205.504784	7285.776697	26.590285
206.074420	7297.336807	26.595303
206.281970	7307.608477	26.600320
206.297601	7312.780146	26.605338
205.992502	7339.417858	26.610356
206.458822	7353.731083	26.615373
206.949232	7370.783883	26.620391
207.155374	7393.285510	26.625408
207.717990	7401.781461	26.630426
208.017902	7412.392380	26.635444
208.416628	7420.487678	26.640461
208.551363	7422.143021	26.645479
208.613384	7431.878652	26.650496
209.158791	7429.230379	26.655514
208.895283	7442.422963	26.660532
209.303879	7450.251560	26.665549
209.158645	7454.529662	26.670567
209.333577	7468.430596	26.675584
209.451635	7471.136625	26.680602
209.513386	7495.318220	26.685620
209.975771	7501.471630	26.690637
210.232689	7514.425396	26.695655
210.519664	7534.442769	26.700672
210.949466	7533.668732	26.705690
210.913965	7551.463368	26.710708
210.985215	7572.051040	26.715725
211.216218	7579.073921	26.720743
211.373453	7599.916573	26.725760
212.026184	7603.641138	26.730778
212.042036	7610.296601	26.735796
212.264664	7623.587258	26.740813
212.695227	7625.793218	26.745831
212.890268	7632.215592	26.750848
213.050375	7642.182302	26.755866
213.410238	7648.436960	26.760884
213.714913	7650.608855	26.765901
213.849609	7657.271088	26.770919
213.915906	7669.582219	26.775936
214.148048	7665.562074	26.780954
213.954205	7676.979264	26.785972
214.531802	7692.351938	26.790989
215.377531	7684.940439	26.796007
215.205399	7685.453424	26.801024
215.449907	7693.929585	26.806042
215.267483	7692.347980	26.811060
215.643157	7703.575499	26.816077
216.020669	7710.913411	26.821095
215.633638	7722.098682	26.826112
216.147127	7731.978854	26.831130
216.070194	7739.567474	26.836148
216.035109	7751.821835	26.841165
216.261587	7759.347441	26.846183
216.625794	7783.027727	26.851200
216.746618	7795.188391	26.856218
217.196579	7812.105837	26.861236
217.125867	7829.287464	26.866253
217.354709	7847.707346	26.871271
217.576069	7872.319187	26.876288
217.902325	7877.126959	26.881306
218.006484	7881.539965	26.886324
218.236070	7896.547117	26.891341
219.071682	7899.132024	26.896359
218.897829	7911.423880	26.901376
219.534721	7925.057507	26.906394
219.606448	7935.284378	26.911412
219.991429	7944.174445	26.916429
220.440322	7946.128192	26.921447
220.548601	7961.987721	26.926464
220.731825	7976.014027	26.931482
220.798455	7984.240202	26.936500
220.928305	7992.046133	26.941517
221.203266	8000.609246	26.946535
221.211924	8020.799916	26.951552
221.542692	8028.792413	26.956570
221.746810	8045.748349	26.961588
221.970119	8052.352731	26.966605
222.154505	8060.418543	26.971623
222.194699	8070.170537	26.976640
222.567879	8088.767079	26.981658
222.787003	8097.323146	26.986676
223.020653	8116.838024	26.991693
222.965667	8126.099748	26.996711
223.114780	8156.146929	27.001728
223.566856	8151.322131	27.006746
223.813742	8167.472800	27.011764
223.876103	8182.102124	27.016781
224.122578	8200.787959	27.021799
224.104435	8209.965064	27.026816
224.883166	8214.677224	27.031834
225.329197	8233.717180	27.036852
225.513572	8247.803496	27.041869
225.968886	8267.751261	27.046887
225.715024	8271.020434	27.051904
226.315860	8285.348171	27.056922
226.252688	8282.952380	27.061940
226.660389	8302.702389	27.066957
226.857573	8309.787641	27.071975
226.834113	8320.613595	27.076992
226.984560	8324.890063	27.082010
227.043158	8336.135763	27.087028
226.917777	8369.790313	27.092045
227.759604	8366.012899	27.097063
227.972390	8390.039558	27.102080
227.812839	8408.160566	27.107098
228.444945	8426.502458	27.112116
228.477914	8438.083700	27.117133
228.963633	8451.154043	27.122151
228.986081	8454.462313	27.127168
229.535965	8465.015981	27.132186
229.766616	8477.924003	27.137204
229.498858	8482.016209	27.142221
229.803175	8483.244302	27.147239
230.061168	8514.856800	27.152256
230.075858	8529.402266	27.157274
230.593057	8540.930283	27.162292
230.621999	8545.800305	27.167309
231.121852	8562.495994	27.172327
231.111520	8578.087226	27.177344
231.109046	8590.160270	27.182362
231.407874	8606.435834	27.187380
231.893644	8615.784096	27.192397
232.524075	8625.949624	27.197415
232.523856	8656.620713	27.202432
232.587237	8662.795593	27.207450
232.704031	8670.840625	27.212468
233.068123	8697.385581	27.217485
233.619329	8695.263464	27.222503
234.319609	8703.539693	27.227520
234.490963	8718.225085	27.232538
234.744219	8711.609454	27.237556
234.967928	8726.217246	27.242573
235.241694	8721.164338	27.247591
235.416560	8730.324280	27.252608
235.354216	8736.108336	27.257626
235.863542	8738.589467	27.262644
235.740314	8756.373666	27.267661
235.705710	8764.663307	27.272679
236.203175	8784.876580	27.277696
236.515074	8779.520951	27.282714
236.644126	8793.439499	27.287732
236.688226	8822.560139	27.292749
237.172392	8820.805199	27.297767
237.450533	8836.323324	27.302784
237.290827	8845.964779	27.307802
237.832528	8870.152382	27.312820
238.161547	8882.129807	27.317837
238.398414	8888.189354	27.322855
238.713033	8904.147010	27.327872
238.479142	8901.676689	27.332890
238.917483	8925.249030	27.337908
239.160281	8935.067809	27.342925
239.138655	8945.218217	27.347943
239.479996	8967.006148	27.352960
239.800919	8980.629766	27.357978
240.568350	8989.883854	27.362996
240.750197	9013.979284	27.368013
240.826239	9011.315466	27.373031
241.113181	9019.940332	27.378048
241.489756	9023.692400	27.383066
241.678247	9026.368749	27.388084
241.728765	9053.783895	27.393101
241.686803	9053.250577	27.398119
242.061244	9064.267590	27.403136
242.540052	9084.597754	27.408154
242.652905	9086.414513	27.413172
242.609398	9112.508907	27.418189
243.038679	9112.921984	27.423207
243.416996	9140.159937	27.428224
243.661492	9142.101436	27.433242
243.724344	9165.817786	27.438260
243.819263	9173.762257	27.443277
244.379956	9193.811433	27.448295
244.778148	9206.125589	27.453312
244.480565	9221.039090	27.458330
244.899356	9227.461915	27.463348
244.607960	9239.842410	27.468365
244.716227	9249.764387	27.473383
245.058236	9273.446886	27.478400
244.825870	9295.728643	27.483418
245.362986	9315.008109	27.488436
245.495363	9342.616154	27.493453
245.979580	9362.203839	27.498471
246.659672	9388.694276	27.503488
246.485206	9406.442874	27.508506
246.838568	9419.622912	27.513524
247.237284	9437.105498	27.518541
247.792000	9454.794291	27.523559
248.223320	9458.642113	27.528576
248.505471	9472.164784	27.533594
248.783404	9484.279999	27.538612
248.804664	9503.024315	27.543629
249.261506	9518.745668	27.548647
249.898964	9514.974588	27.553664
249.407723	9540.570988	27.558682
250.173448	9542.188275	27.563700
250.191693	9573.382107	27.568717
250.644753	9559.868075	27.573735
250.419753	9574.252772	27.578752
250.817326	9586.759869	27.583770
250.811279	9604.053050	27.588788
251.085438	9632.283530	27.593805
251.347491	9645.140120	27.598823
251.843112	9655.642931	27.603840
251.737797	9676.528801	27.608858
252.084402	9696.608696	27.613876
252.347192	9722.116368	27.618893
253.135540	9731.367574	27.623911
253.428216	9743.755346	27.628928
253.448405	9763.144173	27.633946
253.647185	9764.742399	27.638964
253.947220	9783.172070	27.643981
254.752651	9792.079661	27.648999
254.928905	9789.513793	27.654016
255.068622	9823.214953	27.659034
255.452853	9818.772849	27.664052
255.675476	9830.893745	27.669069
255.954357	9845.629594	27.674087
255.682649	9846.634889	27.679104
256.124203	9860.224588	27.684122
256.339237	9863.345262	27.689140
256.051590	9886.596148	27.694157
256.617673	9898.294213	27.699175
257.425447	9919.660188	27.704192
257.092592	9933.389449	27.709210
257.913133	9942.919906	27.714228
258.039432	9958.522599	27.719245
258.167257	9968.934456	27.724263
258.272737	9976.956559	27.729280
258.266734	9997.798912	27.734298
258.763567	10016.188704	27.739316
258.970068	10031.245386	27.744333
259.015574	10041.944786	27.749351
259.754227	10057.123866	27.754368
259.889433	10071.607576	27.759386
260.469307	10080.998764	27.764404
260.773927	10100.552044	27.769421
260.595009	10111.557954	27.774439
261.259470	10119.126842	27.779456
261.550108	10134.119991	27.784474
261.565459	10131.301281	27.789492
262.160014	10149.218177	27.794509
261.999643	10160.578008	27.799527
262.441408	10173.991093	27.804544
263.066089	10187.088392	27.809562
262.980065	10179.438937	27.814580
263.020240	10188.604783	27.819597
262.998725	10209.228775	27.824615
263.035695	10217.956263	27.829632
263.374152	10246.029271	27.834650
263.713198	10259.442622	27.839668
263.900578	10273.590002	27.844685
263.933337	10294.805535	27.849703
264.214587	10309.108825	27.854720
264.392504	10331.267955	27.859738
264.911281	10352.455248	27.864756
264.818306	10371.331888	27.869773
264.936615	10399.714092	27.874791
265.635074	10413.150534	27.879808
265.622164	10440.103991	27.884826
266.235021	10457.396330	27.889844
266.627549	10466.150672	27.894861
266.878465	10495.759546	27.899879
267.460645	10500.796541	27.904896
267.751554	10519.117854	27.909914
267.807132	10522.948621	27.914932
267.960599	10543.722553	27.919949
268.135544	10566.911739	27.924967
268.773954	10574.203861	27.929984
268.863745	10595.426644	27.935002
269.179387	10615.648121	27.940020
269.757555	10633.217563	27.945037
269.747092	10639.439328	27.950055
270.225979	10658.255644	27.955072
270.195119	10671.032249	27.960090
270.955683	10688.917506	27.965108
271.339214	10701.133901	27.970125
271.356442	10716.391105	27.975143
271.773526	10715.006386	27.980160
272.062114	10739.267408	27.985178
272.759446	10735.107874	27.990196
273.253777	10735.892915	27.995213
273.731267	10744.252111	28.000231
275.041519	10712.748497	28.005248
275.220773	10724.551512	28.010266
274.920575	10704.794855	28.015284
275.457909	10696.201948	28.020301
275.211534	10699.347237	28.025319
275.528722	10697.665486	28.030336
275.374113	10698.763104	28.035354
275.386700	10692.487355	28.040372
275.674924	10702.719937	28.045389
275.707295	10722.363617	28.050407
276.058425	10725.993698	28.055424
276.056059	10742.987407	28.060442
276.343553	10748.477658	28.065460
276.685228	10777.652912	28.070477
276.629491	10798.661775	28.075495
277.461910	10800.657163	28.080512
276.750314	10818.029739	28.085530
276.860055	10831.463416	28.090548
277.608224	10859.637750	28.095565
276.860170	10883.580416	28.100583
277.285996	10907.965535	28.105600
277.618429	10939.150627	28.110618
278.319379	10967.389309	28.115636
278.941218	10991.627194	28.120653
278.773109	11019.720240	28.125671
279.658094	11033.885889	28.130688
279.892161	11056.138177	28.135706
279.768667	11075.042381	28.140724
279.913337	11087.106767	28.145741
280.210435	11123.267566	28.150759
280.685883	11131.680932	28.155776
280.607807	11159.697020	28.160794
280.984001	11173.998822	28.165812
281.810340	11184.555211	28.170829
281.977762	11202.271233	28.175847
282.636074	11215.439803	28.180864
282.855728	11221.152309	28.185882
282.955844	11244.211897	28.190900
283.495450	11255.520251	28.195917
283.949108	11278.635354	28.200935
284.251649	11279.737615	28.205952
284.548343	11290.395467	28.210970
284.611970	11292.475867	28.215988
285.184373	11307.116656	28.221005
285.273807	11333.562892	28.226023
285.129485	11332.906512	28.231040
285.562202	11353.609453	28.236058
285.848447	11374.894105	28.241076
286.200677	11387.706284	28.246093
286.350470	11412.864430	28.251111
286.715809	11413.584331	28.256128
286.613061	11439.574374	28.261146
287.054990	11462.407350	28.266164
287.582977	11467.010989	28.271181
287.654199	11491.360506	28.276199
287.831267	11513.338032	28.281216
288.377767	11529.078703	28.286234
288.275306	11549.356811	28.291252
289.215727	11567.675919	28.296269
289.426049	11591.852347	28.301287
289.408442	11604.655944	28.306304
289.793432	11622.591098	28.311322
290.237647	11634.018734	28.316340
290.917143	11643.616236	28.321357
290.961924	11655.355520	28.326375
291.486475	11677.557008	28.331392
291.660332	11680.494944	28.336410
292.027905	11706.304776	28.341428
292.575673	11718.890969	28.346445
292.679631	11732.566171	28.351463
292.558233	11741.271662	28.356480
293.151455	11762.906822	28.361498
293.185591	11776.675024	28.366516
293.635102	11794.862381	28.371533
293.663676	11806.910571	28.376551
293.848969	11825.293815	28.381568
294.240695	11848.182442	28.386586
294.442352	11864.659130	28.391604
294.725400	11873.102786	28.396621
294.918854	11897.853765	28.401639
295.353691	11921.638853	28.406656
295.664708	11939.216384	28.411674
295.917349	11960.105913	28.416692
296.466976	11978.843079	28.421709
296.817902	11993.231541	28.426727
297.005265	12008.551724	28.431744
297.347246	12037.836254	28.436762
297.395535	12053.478103	28.441780
297.665671	12063.568995	28.446797
297.932536	12093.260013	28.451815
298.274018	12112.414953	28.456832
298.242440	12133.683636	28.461850
298.908208	12153.672280	28.466868
299.402263	12173.125611	28.471885
299.315954	12197.260585	28.476903
299.971583	12213.136412	28.481920
300.234780	12232.616273	28.486938
300.583834	12247.339937	28.491956
301.017180	12252.087971	28.496973
300.993047	12273.661949	28.501991
301.238550	12288.935417	28.507008
302.020468	12296.471123	28.512026
301.834844	12310.968623	28.517044
302.121705	12324.224226	28.522061
302.503149	12345.450951	28.527079
302.450488	12364.361212	28.532096
303.176167	12381.644088	28.537114
303.538963	12407.635618	28.542132
303.979861	12409.707931	28.547149
304.289738	12428.523922	28.552167
304.240590	12445.545402	28.557184
304.649885	12465.233273	28.562202
304.772518	12477.532498	28.567220
305.729190	12494.552160	28.572237
305.687605	12517.209078	28.577255
305.758190	12525.509272	28.582272
306.438764	12537.131177	28.587290
306.454298	12566.489458	28.592308
306.545258	12579.418914	28.597325
306.880031	12604.104613	28.602343
307.463401	12621.349869	28.607360
307.973287	12633.588907	28.612378
308.258351	12662.444343	28.617396
308.588867	12667.824256	28.622413
308.425285	12694.090754	28.627431
308.566456	12714.698488	28.632448
309.380028	12732.195363	28.637466
309.482747	12746.225165	28.642484
310.059544	12769.354513	28.647501
310.470687	12780.450115	28.652519
310.612197	12802.093643	28.657536
310.724334	12812.916879	28.662554
311.150630	12835.450814	28.667572
311.884044	12830.906277	28.672589
312.616584	12862.581732	28.677607
312.702099	12864.573639	28.682624
313.260013	12873.044424	28.687642
313.547825	12895.350524	28.692660
313.830627	12904.344140	28.697677
314.284059	12902.802035	28.702695
314.465878	12924.748893	28.707712
314.641988	12929.429783	28.712730
314.982744	12946.034180	28.717748
315.183781	12947.528124	28.722765
315.369585	12959.580994	28.727783
315.472415	12980.674975	28.732800
316.447911	12994.190146	28.737818
316.276666	13011.796394	28.742836
316.604109	13016.286381	28.747853
316.748211	13027.619489	28.752871
317.033055	13047.737861	28.757888
317.382543	13060.586347	28.762906
317.757399	13080.924421	28.767924
318.154609	13088.665602	28.772941
318.153285	13114.923213	28.777959
318.781132	13128.909441	28.782976
319.214288	13140.971286	28.787994
319.303031	13165.626552	28.793012
319.759362	13178.218488	28.798029
319.847823	13190.166662	28.803047
320.143820	13209.396116	28.808064
320.801586	13216.645213	28.813082
320.721914	13243.332036	28.818100
320.959529	13266.085332	28.823117
321.519622	13277.739085	28.828135
321.566285	13296.647449	28.833152
322.068715	13311.888063	28.838170
322.278296	13333.341604	28.843188
322.199171	13347.586478	28.848205
322.557515	13371.641097	28.853223
322.544242	13387.119953	28.858240
323.091778	13411.694639	28.863258
323.144090	13439.213820	28.868276
323.810304	13464.269045	28.873293
323.925163	13492.997513	28.878311
324.377261	13505.732433	28.883328
324.773138	13532.437207	28.888346
324.615234	13561.666140	28.893364
325.146108	13582.972049	28.898381
325.977750	13610.281728	28.903399
326.266004	13632.171784	28.908416
326.630350	13646.164682	28.913434
327.179618	13669.441528	28.918452
327.667694	13684.732047	28.923469
328.081565	13699.440440	28.928487
328.118667	13723.987629	28.933504
328.811902	13732.927217	28.938522
329.074916	13759.280360	28.943540
328.926017	13774.989071	28.948557
329.601704	13787.133574	28.953575
329.927438	13812.428588	28.958592
330.814847	13820.087439	28.963610
330.980194	13842.044242	28.968628
331.415137	13839.882825	28.973645
331.672194	13864.670695	28.978663
331.812286	13875.483872	28.983680
332.184480	13890.072584	28.988698
332.049456	13899.005405	28.993716
332.748151	13921.245590	28.998733
332.842084	13937.033476	29.003751
333.023926	13963.469015	29.008768
333.407256	13987.687900	29.013786
333.937933	14006.868997	29.018804
334.366685	14015.177245	29.023821
334.871300	14043.027950	29.028839
334.757803	14057.714511	29.033856
335.131955	14066.684986	29.038874
335.515071	14086.204936	29.043892
335.897217	14118.796025	29.048909
336.048170	14129.730818	29.053927
336.590858	14156.160976	29.058944
336.881946	14165.993935	29.063962
337.164558	14188.498167	29.068980
337.462940	14206.651380	29.073997
337.607189	14226.072867	29.079015
337.908251	14250.428058	29.084032
338.707718	14270.698149	29.089050
338.992705	14290.170426	29.094068
338.907868	14312.829910	29.099085
339.364197	14328.305901	29.104103
340.165157	14355.021406	29.109120
340.618852	14375.130693	29.114138
341.136744	14383.311536	29.119156
341.580688	14391.882860	29.124173
341.951478	14402.897276	29.129191
341.955332	14423.297711	29.134208
342.444477	14435.885378	29.139226
342.828981	14452.872730	29.144244
342.680663	14471.038895	29.149261
343.228051	14492.816967	29.154279
342.974260	14514.899805	29.159296
343.995758	14522.762292	29.164314
343.854546	14541.915894	29.169332
344.032458	14562.744143	29.174349
344.678341	14579.798290	29.179367
344.829839	14606.141548	29.184384
345.080981	14624.814125	29.189402
345.335285	14632.451866	29.194420
345.614286	14662.631378	29.199437
345.784398	14678.297486	29.204455
346.079594	14708.417703	29.209472
346.619784	14736.904983	29.214490
346.890239	14760.845566	29.219508
347.058316	14791.715228	29.224525
347.478718	14811.002734	29.229543
348.019918	14841.760701	29.234560
348.327229	14865.856742	29.239578
348.592434	14881.246088	29.244596
348.952195	14919.911962	29.249613
349.480065	14946.721346	29.254631
349.658202	14961.331619	29.259648
350.183391	14987.513008	29.264666
350.553442	15012.670079	29.269684
350.550830	15041.722359	29.274701
351.249287	15062.864885	29.279719
351.414256	15095.677791	29.284736
351.723812	15114.439657	29.289754
352.034188	15144.836120	29.294772
352.142796	15170.261489	29.299789
352.496842	15201.958729	29.304807
353.105633	15241.653951	29.309824
353.678929	15270.771672	29.314842
354.235988	15300.893114	29.319860
354.175765	15330.621182	29.324877
354.850327	15345.839795	29.329895
355.153682	15371.876230	29.334912
355.383203	15406.198719	29.339930
355.992113	15423.622576	29.344948
356.137428	15453.789412	29.349965
356.824249	15476.405940	29.354983
356.925116	15499.334795	29.360000
357.588356	15518.162010	29.365018
357.805931	15539.768393	29.370036
358.404397	15567.177199	29.375053
358.870764	15582.371566	29.380071
359.209955	15610.190314	29.385088
359.595300	15631.988602	29.390106
360.114982	15645.472420	29.395124
359.916767	15675.835209	29.400141
360.403988	15700.930731	29.405159
360.736861	15728.542189	29.410176
361.063272	15749.383356	29.415194
361.713283	15764.719824	29.420212
361.652807	15799.448210	29.425229
362.573203	15805.239353	29.430247
362.733791	15833.989500	29.435264
363.483618	15839.412422	29.440282
363.982913	15870.996570	29.445300
364.010620	15885.877317	29.450317
364.530078	15904.544116	29.455335
364.812468	15915.374198	29.460352
365.250244	15937.464711	29.465370
365.763966	15953.694241	29.470388
365.711941	15982.010282	29.475405
366.091798	15985.905372	29.480423
366.713462	15993.735975	29.485440
367.507269	15999.019448	29.490458
368.036576	16011.071311	29.495476
368.770766	16022.544896	29.500493
369.302151	16004.965119	29.505511
369.819731	16008.361868	29.510528
369.602930	16022.775456	29.515546
370.238554	16018.981291	29.520564
370.371595	16037.746280	29.525581
370.930558	16030.114056	29.530599
370.997403	16038.451109	29.535616
371.092829	16040.160718	29.540634
370.963505	16044.491981	29.545652
370.988466	16062.297898	29.550669
371.735356	16084.150958	29.555687
371.731781	16102.071897	29.560704
372.094126	16122.813127	29.565722
372.225269	16138.739168	29.570740
372.312444	16182.645499	29.575757
372.571379	16202.723871	29.580775
373.282577	16238.160403	29.585792
373.360100	16266.469329	29.590810
374.135196	16287.604442	29.595828
374.119647	16329.259397	29.600845
374.543911	16356.576440	29.605863
375.253112	16376.322750	29.610880
375.620217	16408.970629	29.615898
375.776752	16429.150456	29.620916
376.105630	16457.313147	29.625933
376.448476	16479.384322	29.630951
377.067938	16513.957613	29.635968
377.671502	16539.216152	29.640986
378.031605	16569.177594	29.646004
378.185686	16596.622317	29.651021
378.703824	16625.504334	29.656039
379.188912	16654.963214	29.661056
379.237850	16681.347405	29.666074
379.547176	16712.226602	29.671092
380.041163	16739.309086	29.676109
380.468908	16775.539289	29.681127
381.167989	16796.083536	29.686144
381.377990	16821.119456	29.691162
381.983599	16845.743232	29.696180
382.065832	16874.491345	29.701197
382.869167	16905.388697	29.706215
383.295475	16923.091870	29.711232
383.307371	16947.972447	29.716250
383.884439	16971.659604	29.721268
384.400149	16994.721488	29.726285
384.736623	17016.718469	29.731303
385.238744	17044.049637	29.736320
385.820625	17058.336501	29.741338
386.427895	17080.095571	29.746356
386.315898	17104.360781	29.751373
386.970676	17118.475258	29.756391
387.287770	17143.267514	29.761408
387.389210	17171.081321	29.766426
387.961475	17190.265466	29.771444
387.874953	17214.116242	29.776461
388.302841	17241.743513	29.781479
389.274465	17263.758762	29.786496
389.560086	17281.048290	29.791514
389.880588	17299.674778	29.796532
390.509559	17313.392284	29.801549
391.224048	17333.176661	29.806567
391.921369	17343.617625	29.811584
392.743348	17351.231249	29.816602
393.265459	17359.400085	29.821620
393.198776	17371.406616	29.826637
393.678812	17373.782931	29.831655
394.543178	17388.509321	29.836672
394.337040	17399.959567	29.841690
394.310771	17411.015426	29.846708
394.668471	17417.150510	29.851725
394.865677	17428.831725	29.856743
394.920631	17458.185080	29.861760
395.003812	17479.697704	29.866778
395.837307	17493.216095	29.871796
395.539257	17522.520271	29.876813
396.016005	17540.907886	29.881831
396.879782	17559.617452	29.886848
396.897236	17583.878905	29.891866
397.411514	17601.310004	29.896884
397.585387	17628.825765	29.901901
397.882908	17654.035499	29.906919
398.097073	17684.059300	29.911936
398.696739	17711.256203	29.916954
399.076884	17737.192294	29.921972
399.493803	17766.464497	29.926989
399.730918	17798.563264	29.932007
400.552911	17827.633519	29.937024
400.509272	17856.510084	29.942042
400.876873	17891.267199	29.947060
401.037704	17928.381318	29.952077
401.473517	17959.280725	29.957095
402.026758	17997.540484	29.962112
401.925682	18026.072476	29.967130
402.885133	18067.648886	29.972148
403.263697	18092.909749	29.977165
403.980414	18120.758642	29.982183
404.446227	18141.571226	29.987200
404.846269	18179.349809	29.992218
405.425368	18201.250355	29.997236
405.827144	18239.850042	30.002253
406.004088	18265.951141	30.007271
406.594783	18291.438251	30.012288
406.705886	18330.146544	30.017306
407.729179	18362.521849	30.022324
407.911991	18391.667192	30.027341
408.366379	18418.003270	30.032359
408.917805	18443.869421	30.037376
409.004328	18473.061464	30.042394
409.500939	18487.558507	30.047412
409.758430	18523.692149	30.052429
409.973897	18555.852398	30.057447
410.645257	18581.302062	30.062464
411.103973	18627.266148	30.067482
411.433760	18650.311576	30.072500
412.030901	18692.710152	30.077517
411.995345	18715.484024	30.082535
412.800381	18745.379578	30.087552
413.350136	18792.176429	30.092570
413.657225	18814.795994	30.097588
414.144152	18842.688018	30.102605
413.869457	18867.205037	30.107623
414.555910	18888.198871	30.112640
414.802236	18921.618436	30.117658
415.512177	18969.534260	30.122676
415.924382	18990.532995	30.127693
415.965385	19027.029792	30.132711
416.775737	19055.749919	30.137728
417.251672	19100.076178	30.142746
417.831891	19125.382804	30.147764
418.524087	19153.338083	30.152781
418.423762	19184.209190	30.157799
418.720512	19212.314564	30.162816
419.370797	19243.568007	30.167834
420.059836	19271.422864	30.172852
420.772115	19297.783165	30.177869
421.264814	19315.882529	30.182887
422.417805	19314.982834	30.187904
422.729470	19354.609599	30.192922
423.308250	19347.058286	30.197940
424.019184	19348.501789	30.202957
423.773269	19373.046553	30.207975
424.177624	19376.584731	30.212992
424.100462	19393.465113	30.218010
424.622578	19403.725989	30.223028
425.106814	19419.495522	30.228045
424.742199	19448.190664	30.233063
425.553024	19472.830068	30.238080
425.555809	19494.524862	30.243098
426.272840	19526.197978	30.248116
426.774475	19550.872980	30.253133
426.609745	19582.462336	30.258151
427.514331	19610.865362	30.263168
427.773466	19642.692084	30.268186
428.052422	19673.005811	30.273204
428.204660	19704.868229	30.278221
428.485965	19740.122244	30.283239
429.224845	19775.456716	30.288256
429.641068	19810.329736	30.293274
430.006027	19848.988893	30.298292
430.495538	19879.939858	30.303309
430.723240	19906.957670	30.308327
431.346190	19952.482336	30.313344
431.593281	19991.059037	30.318362
432.415859	20019.026853	30.323380
432.694406	20059.380450	30.328397
432.929231	20092.506869	30.333415
433.630840	20130.450788	30.338432
433.924722	20172.482812	30.343450
434.109546	20207.512607	30.348468
435.259334	20225.598974	30.353485
435.693114	20279.575755	30.358503
436.231321	20294.130852	30.363520
436.299606	20330.910150	30.368538
436.924981	20348.061068	30.373556
437.569528	20389.419799	30.378573
438.062814	20422.285408	30.383591
439.053652	20437.231366	30.388608
439.590772	20465.762344	30.393626
439.649070	20482.034995	30.398644
440.437949	20503.570622	30.403661
440.825614	20538.417796	30.408679
441.135687	20553.874184	30.413696
441.409512	20581.852419	30.418714
441.565186	20611.150621	30.423732
442.121401	20643.273902	30.428749
442.589978	20679.315495	30.433767
443.273379	20692.698383	30.438784
443.292644	20734.774367	30.443802
443.606844	20759.764394	30.448820
443.976857	20779.804945	30.453837
444.311981	20815.216791	30.458855
445.040325	20844.546235	30.463872
445.456525	20884.033463	30.468890
445.754658	20916.317415	30.473908
446.634009	20945.465546	30.478925
447.081568	20978.794121	30.483943
447.545247	21004.734200	30.488960
447.888106	21035.615051	30.493978
448.135864	21065.834700	30.498996
449.141958	21088.291215	30.504013
449.362493	21113.839648	30.509031
449.892256	21136.364054	30.514048
449.970639	21173.952102	30.519066
450.128492	21200.837251	30.524084
450.724957	21235.413062	30.529101
451.152289	21265.301782	30.534119
451.729593	21298.364285	30.539136
452.121559	21322.300395	30.544154
452.313368	21350.039758	30.549172
452.592404	21375.768974	30.554189
452.869368	21410.356922	30.559207
453.722338	21437.494328	30.564224
454.448083	21463.741727	30.569242
455.086432	21489.339334	30.574260
455.876497	21513.776040	30.579277
455.956241	21548.862498	30.584295
456.337651	21569.508650	30.589312
456.892157	21595.928208	30.594330
456.937699	21615.445146	30.599348
457.840492	21644.085192	30.604365
458.155001	21677.934824	30.609383
458.387462	21711.569821	30.614400
459.127187	21743.097670	30.619418
459.426850	21776.008326	30.624436
460.106865	21792.216866	30.629453
460.466789	21811.508138	30.634471
460.599751	21838.492810	30.639488
461.069729	21875.894864	30.644506
461.694626	21915.162116	30.649524
462.267041	21936.859390	30.654541
462.697551	21979.727016	30.659559
462.866496	22016.797087	30.664576
463.615979	22040.198200	30.669594
463.943852	22077.117271	30.674612
464.548934	22107.402944	30.679629
464.847479	22148.351668	30.684647
465.051405	22194.730278	30.689664
465.778726	22220.485589	30.694682
466.184036	22260.211063	30.699700
466.797715	22280.600648	30.704717
466.919296	22322.859971	30.709735
467.685196	22343.238561	30.714752
468.559758	22384.527772	30.719770
468.817626	22419.436397	30.724788
469.112910	22458.136810	30.729805
469.685188	22493.009256	30.734823
469.795987	22529.413235	30.739840
470.733172	22569.517797	30.744858
470.709824	22606.208189	30.749876
471.368608	22634.110453	30.754893
472.311511	22674.365989	30.759911
472.485452	22702.963071	30.764928
473.415292	22737.647589	30.769946
473.585109	22774.068106	30.774964
474.242685	22789.408964	30.779981
474.520341	22831.676670	30.784999
475.169277	22866.019694	30.790016
475.097332	22891.925585	30.795034
475.729285	22929.816244	30.800052
476.069569	22959.740040	30.805069
476.613438	22995.552989	30.810087
477.411630	23034.125684	30.815104
477.804225	23063.769780	30.820122
478.100773	23099.330749	30.825140
478.872675	23122.792846	30.830157
479.349599	23165.895936	30.835175
479.450692	23200.729240	30.840192
479.959844	23239.366289	30.845210
480.331205	23281.923676	30.850228
480.811373	23316.401178	30.855245
481.637851	23358.641437	30.860263
481.946535	23390.725584	30.865280
482.448576	23424.744899	30.870298
482.601280	23467.128195	30.875316
483.471888	23485.185213	30.880333
484.199350	23516.585102	30.885351
484.672486	23544.151045	30.890368
485.132889	23566.335158	30.895386
485.414853	23597.020963	30.900404
486.051021	23617.553765	30.905421
486.834513	23645.968845	30.910439
486.926017	23679.850298	30.915456
487.636336	23701.426935	30.920474
487.819805	23736.924499	30.925492
488.382688	23772.274593	30.930509
488.756362	23803.812162	30.935527
489.324948	23832.690667	30.940544
489.556067	23868.237920	30.945562
489.996916	23908.555164	30.950580
490.990018	23925.089549	30.955597
491.341052	23948.567590	30.960615
491.894882	23991.546753	30.965632
492.477260	24016.644492	30.970650
492.683500	24068.531156	30.975668
493.258067	24096.612890	30.980685
493.623464	24127.798383	30.985703
494.005860	24156.055461	30.990720
494.975545	24193.112365	30.995738
495.320616	24238.386858	31.000756
495.577634	24270.145543	31.005773
495.995624	24316.571612	31.010791
496.436067	24349.591007	31.015808
496.963939	24377.023197	31.020826
498.164111	24397.740734	31.025844
499.306788	24420.761167	31.030861
500.239185	24444.168245	31.035879
500.809284	24470.949417	31.040896
501.381523	24467.953449	31.045914
502.015956	24498.920698	31.050932
502.186571	24503.374591	31.055949
502.588442	24521.214835	31.060967
502.452849	24542.835604	31.065984
503.056796	24569.858096	31.071002
503.223839	24599.027722	31.076020
503.455460	24629.533372	31.081037
504.237625	24665.249035	31.086055
504.897840	24693.097097	31.091072
505.121757	24722.732007	31.096090
505.220624	24764.191162	31.101108
506.057937	24796.764028	31.106125
506.168940	24831.952528	31.111143
506.453665	24879.038917	31.116160
506.780156	24912.449832	31.121178
507.505742	24948.212727	31.126196
508.198942	24977.610650	31.131213
508.987299	25017.054496	31.136231
509.287959	25059.064243	31.141248
509.855319	25092.020871	31.146266
510.146459	25130.145723	31.151284
510.897488	25155.762124	31.156301
511.787241	25207.147201	31.161319
512.038366	25240.880057	31.166336
512.796857	25274.944759	31.171354
513.330196	25311.894722	31.176372
513.771275	25332.794605	31.181389
514.168457	25375.276600	31.186407
514.162302	25417.650844	31.191424
515.057846	25455.340961	31.196442
515.584342	25499.345087	31.201460
515.836589	25539.846653	31.206477
516.310665	25572.553165	31.211495
516.831948	25614.991069	31.216512
517.266424	25649.328039	31.221530
517.292411	25689.776654	31.226548
517.945346	25723.492006	31.231565
518.684048	25758.609691	31.236583
518.671336	25799.311021	31.241600
519.570443	25849.634564	31.246618
520.103757	25888.816479	31.251636
520.378391	25934.699830	31.256653
521.016960	25965.668703	31.261671
521.421650	26012.454680	31.266688
521.855978	26050.325151	31.271706
522.606230	26099.876192	31.276724
522.848040	26146.055848	31.281741
523.360265	26192.718064	31.286759
523.787156	26242.471472	31.291776
524.511715	26289.638051	31.296794
525.469901	26338.866592	31.301812
525.512108	26383.738036	31.306829
526.047365	26429.354421	31.311847
526.762611	26470.518896	31.316864
527.140684	26516.772987	31.321882
528.098734	26563.088576	31.326900
528.929926	26602.750068	31.331917
529.731436	26635.350453	31.336935
530.047730	26680.666530	31.341952
530.393748	26715.398292	31.346970
531.783492	26741.005764	31.351988
532.522561	26766.284799	31.357005
533.267430	26793.471629	31.362023
533.881253	26827.087477	31.367040
534.151884	26848.660120	31.372058
535.197838	26879.111930	31.377076
535.511670	26894.439943	31.382093
535.987490	26920.758732	31.387111
536.123434	26945.322907	31.392128
536.568798	26972.765169	31.397146
537.111244	27006.424027	31.402164
537.656058	27038.995505	31.407181
538.744666	27065.187485	31.412199
538.746374	27089.696890	31.417216
539.251446	27120.106863	31.422234
540.057453	27159.444720	31.427252
540.193649	27194.228929	31.432269
540.834495	27229.351770	31.437287
540.834028	27260.567480	31.442304
541.632124	27300.956002	31.447322
542.110463	27342.626835	31.452340
542.270190	27370.215227	31.457357
542.849138	27412.989229	31.462375
543.115029	27465.071292	31.467392
543.857151	27508.123466	31.472410
544.257358	27549.832169	31.477428
544.961983	27606.592859	31.482445
545.505966	27640.442142	31.487463
545.752124	27690.208284	31.492480
546.561179	27731.651460	31.497498
546.900255	27777.971386	31.502516
547.195441	27828.058893	31.507533
548.247719	27876.442236	31.512551
548.833784	27916.808110	31.517568
549.397793	27960.565259	31.522586
550.014036	28001.451200	31.527604
550.519183	28048.061910	31.532621
551.256052	28088.392007	31.537639
551.403458	28128.851872	31.542656
552.238915	28174.551862	31.547674
552.450068	28216.544183	31.552692
553.071018	28256.608235	31.557709
554.138009	28281.420958	31.562727
554.748817	28319.489418	31.567744
555.494916	28348.466865	31.572762
556.085736	28372.721770	31.577780
556.724821	28405.476704	31.582797
557.300059	28436.256961	31.587815
557.742010	28466.982166	31.592832
558.261801	28494.421220	31.597850
558.528814	28530.375623	31.602868
558.757221	28574.097847	31.607885
559.407899	28606.617435	31.612903
559.786839	28641.846698	31.617920
560.211183	28685.721958	31.622938
561.070035	28735.938850	31.627956
561.392510	28783.793253	31.632973
561.825531	28819.539022	31.637991
562.578594	28868.508566	31.643008
563.000781	28914.995117	31.648026
563.491789	28960.162662	31.653044
563.921339	29011.433102	31.658061
564.404998	29050.085269	31.663079
564.817891	29100.593711	31.668096
565.374771	29156.351426	31.673114
566.202229	29205.101608	31.678132
566.485126	29264.612602	31.683149
567.055747	29309.831733	31.688167
567.550725	29364.442932	31.693184
568.642213	29422.949906	31.698202
569.735058	29462.462473	31.703220
570.267379	29509.495790	31.708237
570.811619	29545.124377	31.713255
571.311106	29589.666216	31.718272
572.105182	29630.211688	31.723290
572.998460	29665.703976	31.728308
573.283477	29724.640765	31.733325
573.493821	29755.871716	31.738343
574.408171	29798.535297	31.743360
575.234256	29842.609656	31.748378
575.745740	29878.187031	31.753396
575.797068	29929.929515	31.758413
576.649114	29966.680313	31.763431
577.053947	30013.001385	31.768448
577.811443	30060.304322	31.773466
578.675345	30097.799399	31.778484
578.897212	30146.936866	31.783501
579.195109	30177.990479	31.788519
580.212369	30237.181371	31.793536
580.501552	30282.452779	31.798554
581.311627	30316.372532	31.803572
583.494210	30323.188358	31.808589
585.344680	30329.101389	31.813607
586.382444	30345.849028	31.818624
586.676014	30355.354665	31.823642
587.258105	30355.036508	31.828660
587.364463	30371.328650	31.833677
587.705560	30377.533557	31.838695
587.904913	30388.975521	31.843712
588.469133	30409.829858	31.848730
588.859720	30437.746758	31.853748
588.608094	30460.017679	31.858765
589.238798	30499.894968	31.863783
589.792603	30517.577776	31.868800
589.664655	30556.593484	31.873818
590.627612	30590.306575	31.878836
590.676937	30636.848748	31.883853
590.878157	30680.794615	31.888871
591.517602	30728.288141	31.893888
592.047721	30779.635837	31.898906
592.512600	30818.907425	31.903924
592.474918	30870.109848	31.908941
593.100126	30925.722656	31.913959
593.462616	30980.700125	31.918976
593.865047	31035.330167	31.923994
594.608344	31085.014514	31.929012
595.334302	31147.730149	31.934029
595.775820	31202.228117	31.939047
596.463239	31260.784260	31.944064
597.248336	31306.638145	31.949082
598.125096	31355.467930	31.954100
598.693351	31407.974404	31.959117
599.582233	31453.799816	31.964135
600.447966	31504.553413	31.969152
600.653613	31551.673854	31.974170
601.626395	31606.798197	31.979188
602.476257	31649.437723	31.984205
602.790165	31692.280881	31.989223
603.781534	31741.555212	31.994240
604.136559	31799.070981	31.999258
604.903996	31833.145265	32.004276
605.204557	31881.895306	32.009293
606.099236	31923.049150	32.014311
606.874886	31954.005771	32.019328
607.666112	32009.557716	32.024346
608.493637	32052.334303	32.029364
609.169294	32095.058760	32.034381
609.550807	32127.063185	32.039399
609.956685	32156.648962	32.044416
610.554240	32216.018330	32.049434
611.400048	32255.701151	32.054452
611.811292	32312.937754	32.059469
612.302926	32350.684529	32.064487
612.643771	32402.078352	32.069504
613.036975	32458.098052	32.074522
613.646496	32510.278476	32.079540
614.310591	32557.943047	32.084557
615.015154	32611.291116	32.089575
615.942046	32653.933357	32.094592
616.186458	32710.179198	32.099610
616.922771	32764.148585	32.104628
617.348421	32817.471060	32.109645
617.940289	32879.688077	32.114663
618.377052	32929.013629	32.119680
619.217258	32992.406142	32.124698
619.605880	33041.537150	32.129716
620.200884	33105.429683	32.134733
621.378054	33153.995658	32.139751
622.034883	33193.090125	32.144768
622.433079	33254.175149	32.149786
623.964096	33295.763702	32.154804
624.384169	33340.762197	32.159821
625.155281	33386.091790	32.164839
625.990908	33426.328450	32.169856
626.332316	33476.220161	32.174874
627.198117	33505.862697	32.179892
627.519624	33556.965229	32.184909
628.058084	33596.774316	32.189927
628.858230	33633.381647	32.194944
629.185773	33691.931105	32.199962
629.800860	33733.087796	32.204980
630.348175	33782.429761	32.209997
630.796465	33828.916957	32.215015
631.896464	33879.292150	32.220032
632.150668	33940.869438	32.225050
632.786097	33986.177196	32.230068
633.277648	34042.641033	32.235085
634.318443	34082.157883	32.240103
635.183745	34119.305962	32.245120
635.693534	34152.602243	32.250138
636.504249	34178.859211	32.255156
637.115319	34218.664497	32.260173
637.833280	34265.976844	32.265191
638.291158	34290.537581	32.270208
638.633804	34339.071838	32.275226
639.162357	34386.963992	32.280244
639.613466	34430.859893	32.285261
640.316418	34468.539658	32.290279
640.944998	34522.454478	32.295296
641.483666	34574.790170	32.300314
641.857054	34615.031522	32.305332
642.385058	34673.906567	32.310349
642.461216	34736.082922	32.315367
643.291342	34785.117669	32.320384
643.734529	34866.533648	32.325402
644.624746	34911.835349	32.330420
645.180834	34973.741692	32.335437
645.664457	35043.986373	32.340455
646.424355	35100.556691	32.345472
647.086405	35183.425638	32.350490
647.758549	35236.248004	32.355508
648.841294	35292.597867	32.360525
649.598449	35343.744402	32.365543
650.979276	35397.519063	32.370560
651.381607	35452.609568	32.375578
652.271975	35488.889949	32.380596
653.266891	35543.818892	32.385613
653.818555	35582.459968	32.390631
654.642426	35627.381522	32.395648
655.567682	35675.619502	32.400666
655.858480	35707.826872	32.405684
656.910891	35753.098807	32.410701
657.312987	35793.888020	32.415719
658.212325	35839.734056	32.420736
658.547275	35890.441810	32.425754
659.089375	35934.301378	32.430772
660.094990	35959.328880	32.435789
660.662598	36007.724459	32.440807
661.502729	36054.711976	32.445824
662.061531	36096.925324	32.450842
662.605971	36144.920155	32.455860
663.184542	36186.416112	32.460877
663.665262	36239.403561	32.465895
664.558034	36278.498642	32.470912
664.855504	36334.063014	32.475930
665.413473	36377.320343	32.480948
666.140624	36430.921177	32.485965
666.889360	36488.110272	32.490983
667.595635	36530.503861	32.496000
668.131827	36583.445594	32.501018
668.403560	36636.023949	32.506036
669.176657	36685.470330	32.511053
669.694639	36746.319176	32.516071
670.351212	36799.995158	32.521088
670.778716	36865.518577	32.526106
671.247091	36921.576374	32.531124
672.107299	36992.628828	32.536141
672.897001	37051.147250	32.541159
673.310641	37104.735352	32.546176
674.076058	37178.806713	32.551194
674.891376	37237.795902	32.556212
675.201275	37297.489938	32.561229
675.985512	37355.169048	32.566247
676.875717	37420.963599	32.571264
677.319652	37482.395166	32.576282
677.827794	37544.955118	32.581300
678.849915	37586.928561	32.586317
679.485716	37660.338844	32.591335
680.699209	37704.135478	32.596352
680.982734	37752.256747	32.601370
682.113332	37804.653688	32.606388
684.096653	37824.959353	32.611405
684.569912	37863.167809	32.616423
685.219880	37905.282016	32.621440
686.089324	37935.259020	32.626458
686.550492	37975.138954	32.631476
687.212574	38018.560458	32.636493
687.410125	38053.555575	32.641511
688.110025	38093.626211	32.646528
688.742922	38137.090439	32.651546
689.132609	38190.185427	32.656564
689.788333	38232.400557	32.661581
690.002922	38288.444528	32.666599
690.458447	38352.071061	32.671616
691.399531	38408.261517	32.676634
692.180016	38472.723126	32.681652
692.891923	38522.493137	32.686669
693.837768	38576.691346	32.691687
695.579891	38602.612769	32.696704
696.483560	38647.243698	32.701722
697.063726	38685.120791	32.706740
697.919475	38717.074012	32.711757
698.707038	38762.286063	32.716775
699.804246	38796.092604	32.721792
700.583691	38823.239187	32.726810
701.075898	38860.314520	32.731828
701.587953	38893.086678	32.736845
701.787785	38930.416330	32.741863
702.645413	38964.658828	32.746880
703.158481	39014.290188	32.751898
703.531768	39064.854050	32.756916
703.953835	39113.740949	32.761933
704.566581	39163.508907	32.766951
705.274199	39213.799738	32.771968
705.801302	39278.277906	32.776986
706.394922	39329.415178	32.782004
707.536097	39371.474762	32.787021
707.656643	39433.752731	32.792039
708.434123	39500.500812	32.797056
709.303232	39559.677722	32.802074
709.868029	39616.574949	32.807092
710.702805	39664.848663	32.812109
710.964585	39730.387642	32.817127
711.902024	39787.853385	32.822144
712.858585	39853.632400	32.827162
713.323678	39922.264379	32.832180
714.252819	39971.681388	32.837197
714.364168	40035.632070	32.842215
715.302536	40098.568824	32.847232
716.049281	40168.504769	32.852250
716.527005	40233.556314	32.857268
717.476372	40296.397067	32.862285
718.175270	40368.731637	32.867303
718.879016	40430.516931	32.872320
719.605036	40491.951102	32.877338
720.106548	40564.576343	32.882356
720.831609	40630.083860	32.887373
721.918993	40699.241197	32.892391
722.813760	40750.777639	32.897408
723.847097	40810.710283	32.902426
724.401472	40870.306570	32.907444
725.423805	40915.796466	32.912461
726.234848	40969.844573	32.917479
726.822368	41023.231930	32.922496
727.657693	41076.998251	32.927514
728.068188	41128.117670	32.932532
729.281578	41171.244655	32.937549
730.000704	41212.867560	32.942567
730.961566	41262.725278	32.947584
731.684510	41306.592943	32.952602
732.155766	41351.625631	32.957620
733.008594	41388.453090	32.962637
733.466251	41445.460321	32.967655
733.926851	41487.142967	32.972672
734.174178	41542.184649	32.977690
734.729076	41601.656361	32.982708
735.265929	41666.329826	32.987725
735.990153	41733.630635	32.992743
736.734025	41794.679896	32.997760
738.030206	41867.135166	33.002778
738.798356	41925.771336	33.007796
739.356157	41994.053870	33.012813
739.831825	42063.342376	33.017831
740.451255	42120.579166	33.022848
741.132175	42200.297184	33.027866
741.874289	42267.906758	33.032884
742.703088	42332.928874	33.037901
743.491230	42404.611165	33.042919
743.953431	42477.685284	33.047936
744.944120	42545.054622	33.052954
745.476906	42623.285604	33.057972
746.583883	42682.939946	33.062989
747.012242	42764.071814	33.068007
747.756501	42830.443108	33.073024
749.576267	42893.446777	33.078042
750.882372	42947.093802	33.083060
751.895244	42996.776595	33.088077
753.877817	43016.600276	33.093095
755.289730	43055.222012	33.098112
755.902229	43086.087355	33.103130
756.119147	43130.992511	33.108148
756.709486	43154.688879	33.113165
757.076351	43196.648685	33.118183
757.613026	43240.568189	33.123200
758.356292	43284.980597	33.128218
758.721508	43332.393085	33.133236
759.859327	43370.425539	33.138253
760.206824	43425.816867	33.143271
760.532927	43487.093984	33.148288
761.507931	43528.934453	33.153306
761.819377	43596.355816	33.158324
762.713751	43650.992115	33.163341
763.423773	43704.430169	33.168359
763.936128	43758.405135	33.173376
764.739703	43826.009919	33.178394
765.361532	43892.776651	33.183412
765.992332	43956.626264	33.188429
766.787850	44029.634654	33.193447
767.094989	44103.971709	33.198464
768.194678	44164.725460	33.203482
769.036979	44241.174536	33.208500
769.776131	44296.051648	33.213517
770.553759	44366.249168	33.218535
771.219246	44429.854380	33.223552
772.027300	44492.855647	33.228570
772.652517	44574.355675	33.233588
773.510213	44642.371996	33.238605
774.496749	44709.350074	33.243623
774.836772	44780.603789	33.248640
775.851133	44846.021888	33.253658
776.624358	44922.072901	33.258676
777.269827	44990.566105	33.263693
778.161023	45056.857939	33.268711
778.756090	45115.871091	33.273728
779.562387	45176.445559	33.278746
780.098107	45245.582860	33.283764
781.152671	45298.888880	33.288781
783.150480	45336.487209	33.293799
783.785262	45389.922050	33.298816
784.686770	45439.943936	33.303834
785.107552	45499.073790	33.308852
785.833495	45543.588297	33.313869
786.625309	45602.717599	33.318887
787.093614	45663.807777	33.323904
788.050644	45721.273319	33.328922
788.707191	45779.279190	33.333940
789.555549	45843.372348	33.338957
790.465219	45903.306445	33.343975
790.994307	45964.742224	33.348992
791.507205	46032.379972	33.354010
791.955170	46108.852549	33.359028
792.280959	46178.170901	33.364045
793.662911	46251.538081	33.369063
794.129887	46337.642763	33.374080
795.089461	46417.990428	33.379098
795.920696	46488.920075	33.384116
796.376825	46564.108765	33.389133
797.321603	46632.440203	33.394151
798.092800	46707.580326	33.399168
799.644391	46777.829410	33.404186
800.489766	46846.702030	33.409204
801.550845	46904.805986	33.414221
802.770090	46972.368235	33.419239
803.461000	47039.013411	33.424256
804.393697	47092.519797	33.429274
805.266776	47159.250840	33.434292
806.573895	47217.652586	33.439309
807.500426	47277.511808	33.444327
808.483653	47320.136224	33.449344
808.985306	47363.575847	33.454362
809.623588	47426.928099	33.459380
810.071739	47482.946421	33.464397
810.920564	47548.448780	33.469415
811.503638	47623.077181	33.474432
812.079790	47678.930559	33.479450
812.702334	47748.884451	33.484468
813.776791	47816.857670	33.489485
814.439083	47892.316023	33.494503
815.033547	47969.942468	33.499520
815.492024	48036.671048	33.504538
816.514728	48118.039805	33.509556
817.002192	48192.906387	33.514573
817.923208	48274.633160	33.519591
818.561986	48352.937269	33.524608
819.194000	48433.615126	33.529626
820.198018	48518.486763	33.534644
820.703578	48603.113657	33.539661
821.700686	48682.932097	33.544679
822.598109	48774.116187	33.549696
823.581197	48842.505271	33.554714
824.586118	48918.748802	33.559732
825.465319	49003.907395	33.564749
826.747554	49071.579977	33.569767
827.253019	49152.571102	33.574784
828.443773	49213.058597	33.579802
829.499175	49286.271342	33.584820
830.383813	49361.459536	33.589837
831.462271	49421.636075	33.594855
831.934052	49483.305424	33.599872
833.323738	49538.359761	33.604890
833.950607	49590.793475	33.609908
835.127571	49654.479315	33.614925
835.646226	49696.256795	33.619943
836.532860	49759.785664	33.624960
837.250005	49814.141849	33.629978
837.874912	49871.815145	33.634996
839.238924	49922.065986	33.640013
839.843691	49982.254467	33.645031
840.446378	50038.020918	33.650048
841.358121	50078.852137	33.655066
842.039472	50151.170511	33.660084
842.726098	50216.376784	33.665101
843.699323	50276.369488	33.670119
844.177600	50352.585890	33.675136
845.106353	50416.964167	33.680154
845.708613	50494.224678	33.685172
846.193639	50561.677775	33.690189
847.256508	50628.743748	33.695207
847.505116	50722.548438	33.700224
848.811816	50789.247914	33.705242
849.264413	50866.621549	33.710260
850.091125	50949.663288	33.715277
851.109089	51027.158250	33.720295
851.893757	51115.737092	33.725312
853.153654	51191.094310	33.730330
854.170113	51276.784107	33.735348
854.626240	51357.860280	33.740365
855.707367	51429.721813	33.745383
856.521932	51517.367427	33.750400
857.488232	51588.348848	33.755418
858.412475	51675.617329	33.760436
858.910336	51761.693361	33.765453
860.208594	51835.990036	33.770471
860.873952	51914.245199	33.775488
861.990939	51990.025893	33.780506
863.286065	52072.777285	33.785524
864.167237	52147.494222	33.790541
864.973856	52212.035715	33.795559
865.620737	52294.648361	33.800576
866.581392	52364.133410	33.805594
867.381143	52435.991241	33.810612
868.244900	52516.381575	33.815629
869.319634	52592.170810	33.820647
869.974990	52679.333053	33.825664
870.794739	52759.743732	33.830682
871.670305	52836.298772	33.835700
872.532891	52929.377707	33.840717
873.217274	53001.875355	33.845735
873.859493	53082.707100	33.850752
875.041460	53154.064704	33.855770
876.619536	53230.157325	33.860788
877.708650	53308.629629	33.865805
878.689764	53372.103083	33.870823
879.903407	53439.425806	33.875840
881.151043	53484.292204	33.880858
882.326681	53536.624120	33.885876
883.133649	53597.619460	33.890893
884.068002	53654.190913	33.895911
885.183344	53715.075278	33.900928
885.500100	53768.458957	33.905946
886.560747	53826.675412	33.910964
887.254148	53890.688638	33.915981
887.824496	53941.021125	33.920999
888.352325	54015.419362	33.926016
889.289018	54088.406321	33.931034
890.279198	54147.609056	33.936052
891.006961	54216.787823	33.941069
891.893431	54279.886129	33.946087
892.384397	54343.008201	33.951104
893.462430	54417.201828	33.956122
893.912357	54479.533313	33.961140
894.327105	54543.946068	33.966157
895.348450	54612.586703	33.971175
895.817040	54681.402175	33.976192
896.752745	54762.453472	33.981210
897.649642	54839.106650	33.986228
898.193132	54917.023782	33.991245
899.585951	55007.585716	33.996263
900.012481	55090.546265	34.001280
900.878916	55186.500253	34.006298
902.019910	55268.856603	34.011316
902.678676	55359.742986	34.016333
903.627492	55431.390601	34.021351
904.270784	55521.887655	34.026368
905.400500	55621.688057	34.031386
906.480079	55708.833458	34.036404
907.322626	55804.097534	34.041421
908.418785	55898.044157	34.046439
909.433592	55974.334587	34.051456
910.075965	56062.846689	34.056474
911.371445	56140.403969	34.061492
911.834797	56235.241498	34.066509
913.310736	56325.112038	34.071527
914.018943	56416.836471	34.076544
914.689870	56509.687232	34.081562
916.089055	56602.368034	34.086580
917.159159	56680.670969	34.091597
918.147284	56758.455309	34.096615
919.012575	56853.004892	34.101632
920.135690	56937.844347	34.106650
921.325989	57015.028463	34.111668
922.160682	57106.811800	34.116685
922.721619	57185.201975	34.121703
923.956321	57268.101266	34.126720
925.065169	57360.488444	34.131738
926.029555	57426.994254	34.136756
927.052899	57528.496352	34.141773
927.896688	57600.850361	34.146791
929.087027	57676.334115	34.151808
929.619259	57755.914139	34.156826
930.981932	57832.504447	34.161844
931.331821	57923.296770	34.166861
932.369860	58006.203908	34.171879
933.148828	58087.987108	34.176896
934.064876	58178.236570	34.181914
934.802993	58269.146978	34.186932
935.917270	58359.828289	34.191949
936.898864	58442.714069	34.196967
938.426213	58525.945566	34.201984
939.457197	58596.412646	34.207002
940.753309	58668.819710	34.212020
941.936415	58746.048482	34.217037
942.569429	58815.711044	34.222055
943.895879	58887.189968	34.227072
944.421971	58957.230350	34.232090
945.739925	59034.989704	34.237108
946.021558	59111.157394	34.242125
946.886757	59184.677422	34.247143
947.409205	59271.473109	34.252160
948.448856	59369.378993	34.257178
949.699887	59424.256545	34.262196
950.841397	59511.766893	34.267213
951.782429	59593.890738	34.272231
952.722196	59662.229429	34.277248
953.622217	59739.195287	34.282266
954.548743	59806.542713	34.287284
955.471186	59887.651390	34.292301
957.028380	59932.114639	34.297319
958.564671	59980.176420	34.302336
959.302976	60035.685839	34.307354
960.563476	60092.386349	34.312372
960.990923	60148.463441	34.317389
961.626998	60219.009368	34.322407
962.256306	60275.599679	34.327424
963.106369	60359.784744	34.332442
963.855190	60423.078901	34.337460
964.503827	60504.175283	34.342477
965.407007	60582.668772	34.347495
966.018550	60667.081915	34.352512
966.523753	60760.557144	34.357530
967.422275	60843.660270	34.362548
968.858413	60916.925750	34.367565
970.561035	60989.080227	34.372583
972.765399	61055.738466	34.377600
973.752098	61123.219416	34.382618
974.876220	61186.083666	34.387636
975.835649	61249.271218	34.392653
976.521530	61316.109566	34.397671
977.613194	61380.770734	34.402688
978.435762	61461.659642	34.407706
979.817727	61529.586579	34.412724
980.517414	61604.931044	34.417741
981.350326	61681.052583	34.422759
982.254028	61739.762097	34.427776
982.814848	61823.484479	34.432794
983.916451	61896.697350	34.437812
984.424410	61980.036029	34.442829
985.270306	62062.018383	34.447847
986.438268	62137.873955	34.452864
986.422475	62240.627252	34.457882
987.640912	62325.103541	34.462900
988.483351	62419.615038	34.467917
989.037832	62522.071837	34.472935
990.286259	62619.211244	34.477952
990.890378	62728.953619	34.482970
992.369490	62830.482811	34.487988
993.180370	62936.167846	34.493005
993.854173	63049.205223	34.498023
994.974904	63148.310000	34.503040
995.820072	63247.742935	34.508058
997.106702	63357.938926	34.513076
998.002018	63459.352658	34.518093
998.624899	63574.160214	34.523111
1000.310368	63679.440057	34.528128
1000.899242	63799.976735	34.533146
1002.413544	63892.300169	34.538164
1003.121516	64001.088731	34.543181
1004.052596	64098.922707	34.548199
1005.716066	64204.043594	34.553216
1007.022972	64303.472170	34.558234
1008.527480	64384.543009	34.563252
1009.678632	64479.273830	34.568269
1010.617853	64562.611006	34.573287
1011.957910	64651.666053	34.578304
1012.948795	64740.408583	34.583322
1013.845747	64825.386555	34.588340
1014.876846	64908.489001	34.593357
1015.545018	65006.310467	34.598375
1016.456587	65087.431561	34.603392
1017.531629	65176.352457	34.608410
1018.618693	65265.733954	34.613428
1019.492302	65352.762229	34.618445
1020.487900	65451.927266	34.623463
1021.720899	65532.651559	34.628480
1022.499924	65624.532368	34.633498
1023.329621	65699.729693	34.638516
1024.551693	65776.562886	34.643533
1025.216726	65854.951827	34.648551
1026.296139	65937.809568	34.653568
1026.927034	66034.640513	34.658586
1028.035568	66115.139129	34.663604
1029.033456	66205.949678	34.668621
1030.185681	66298.787831	34.673639
1031.338896	66378.488932	34.678656
1032.298079	66477.986554	34.683674
1033.125602	66572.661656	34.688692
1034.264556	66668.029393	34.693709
1035.225027	66767.559606	34.698727
1036.260635	66860.360983	34.703744
1036.968689	66960.228812	34.708762
1037.847720	67048.192777	34.713780
1038.934139	67154.143894	34.718797
1039.750341	67257.769563	34.723815
1041.030274	67368.648948	34.728832
1042.258452	67468.311176	34.733850
1043.199614	67577.749975	34.738868
1044.147473	67684.978499	34.743885
1045.315701	67800.150922	34.748903
1046.252223	67899.993195	34.753920
1047.394686	68017.728563	34.758938
1048.256682	68124.820336	34.763956
1049.382285	68231.605593	34.768973
1050.535041	68342.116430	34.773991
1051.661045	68446.407835	34.779008
1052.710384	68558.778229	34.784026
1053.718714	68666.362351	34.789044
1054.914976	68778.881794	34.794061
1056.715037	68874.325811	34.799079
1058.393758	68963.634525	34.804096
1059.497351	69053.102723	34.809114
1060.400106	69150.137431	34.814132
1061.483545	69240.394569	34.819149
1062.517004	69351.973073	34.824167
1064.240858	69427.194157	34.829184
1065.367561	69514.779769	34.834202
1066.077874	69603.481602	34.839220
1066.826093	69691.595294	34.844237
1068.200823	69786.469359	34.849255
1069.200106	69884.378282	34.854272
1069.944083	69978.851000	34.859290
1070.744257	70073.549602	34.864308
1071.898462	70171.543139	34.869325
1072.994006	70280.279181	34.874343
1074.132123	70368.784064	34.879360
1075.071767	70472.561753	34.884378
1075.877176	70568.439132	34.889396
1077.458000	70671.205967	34.894413
1078.200081	70773.407214	34.899431
1079.299964	70873.108898	34.904448
1080.393682	70967.961361	34.909466
1081.070044	71082.129477	34.914484
1082.542109	71174.682146	34.919501
1083.708227	71273.070577	34.924519
1085.518704	71368.864106	34.929536
1086.548379	71463.348390	34.934554
1087.509327	71559.464825	34.939572
1088.452760	71642.476086	34.944589
1089.680813	71746.885185	34.949607
1090.473167	71845.789887	34.954624
1091.386098	71943.840294	34.959642
1092.323199	72038.695682	34.964660
1093.808222	72126.145635	34.969677
1094.493361	72227.158218	34.974695
1095.246707	72313.418162	34.979712
1096.869860	72393.324316	34.984730
1097.643891	72485.091023	34.989748
1099.290211	72563.841540	34.994765
1100.360080	72652.890379	34.999783
1101.797245	72736.018219	35.004800
1102.627658	72822.533807	35.009818
1103.607619	72900.565792	35.014836
1105.001282	72992.934421	35.019853
1105.495763	73079.845112	35.024871
1106.833704	73168.473991	35.029888
1107.684950	73265.816966	35.034906
1108.853734	73360.476385	35.039924
1110.055009	73449.494786	35.044941
1111.032329	73548.795046	35.049959
1111.975207	73647.771723	35.054976
1112.955270	73736.445540	35.059994
1114.176585	73837.887448	35.065012
1115.556866	73936.113150	35.070029
1116.722872	74038.147070	35.075047
1117.922984	74139.910082	35.080064
1119.221694	74231.512498	35.085082
1119.856994	74339.532634	35.090100
1121.243160	74435.099343	35.095117
1122.162885	74540.074102	35.100135
1123.442453	74630.034239	35.105152
1125.213060	74731.520709	35.110170
1125.430903	74838.695855	35.115188
1126.878775	74939.916688	35.120205
1127.561854	75047.020250	35.125223
1129.271956	75146.199722	35.130240
1130.095344	75253.890267	35.135258
1131.351925	75364.566501	35.140276
1131.806410	75467.983297	35.145293
1133.415566	75588.979681	35.150311
1134.610260	75702.225640	35.155328
1135.556024	75810.722712	35.160346
1136.379757	75925.091373	35.165364
1137.626488	76029.324363	35.170381
1138.488628	76156.760433	35.175399
1139.983738	76269.480660	35.180416
1141.300793	76381.456371	35.185434
1142.494793	76499.202643	35.190452
1143.894838	76603.895339	35.195469
1145.282423	76724.069917	35.200487
1146.199492	76825.139769	35.205504
1147.827303	76924.123241	35.210522
1148.425052	77034.782188	35.215540
1150.319265	77142.364243	35.220557
1151.337534	77252.211231	35.225575
1153.536556	77321.274989	35.230592
1155.291167	77409.739005	35.235610
1156.515518	77492.762710	35.240628
1157.618337	77577.629745	35.245645
1158.966800	77664.447657	35.250663
1159.799322	77742.529324	35.255680
1160.510205	77822.226303	35.260698
1161.549076	77908.611800	35.265716
1162.749345	78000.749044	35.270733
1163.460678	78094.191501	35.275751
1164.503312	78192.865290	35.280768
1165.649938	78283.529671	35.285786
1166.289402	78394.301643	35.290804
1167.643613	78486.948623	35.295821
1168.571894	78597.638454	35.300839
1169.763938	78693.845815	35.305856
1170.928985	78779.986388	35.310874
1172.183480	78876.032646	35.315892
1173.237959	78964.445977	35.320909
1174.423159	79057.627924	35.325927
1176.378029	79125.695435	35.330944
1178.549705	79190.245524	35.335962
1179.492769	79268.897078	35.340980
1180.210963	79354.766952	35.345997
1181.399220	79435.901868	35.351015
1182.430813	79510.410354	35.356032
1183.606484	79591.370324	35.361050
1183.980172	79681.614865	35.366068
1185.562458	79765.210496	35.371085
1186.400412	79855.028611	35.376103
1187.267148	79954.382196	35.381120
1188.341076	80045.355071	35.386138
1189.391443	80151.205268	35.391156
1190.737099	80246.241250	35.396173
1191.395693	80358.500390	35.401191
1192.527425	80474.119664	35.406208
1193.929973	80579.713968	35.411226
1194.556491	80698.516755	35.416244
1195.999868	80808.501786	35.421261
1197.322373	80930.149163	35.426279
1198.467394	81044.210406	35.431296
1199.497001	81155.996914	35.436314
1200.995340	81274.843819	35.441332
1202.153616	81389.537880	35.446349
1203.430041	81506.659247	35.451367
1204.826080	81624.142574	35.456384
1206.080840	81748.071913	35.461402
1206.767571	81864.387012	35.466420
1208.067598	81979.960971	35.471437
1209.599206	82118.862554	35.476455
1210.178833	82236.070079	35.481472
1211.760914	82349.333738	35.486490
1213.055874	82484.574331	35.491508
1214.181670	82597.707289	35.496525
1215.401668	82727.195832	35.501543
1216.344754	82859.515509	35.506560
1217.832300	82986.885685	35.511578
1219.205199	83117.745939	35.516596
1220.750775	83240.508904	35.521613
1222.056022	83364.766905	35.526631
1223.084353	83484.101730	35.531648
1224.165452	83593.837265	35.536666
1225.282714	83726.754725	35.541684
1226.611135	83849.465425	35.546701
1227.605968	83983.796907	35.551719
1229.038698	84114.297651	35.556736
1230.591694	84227.547992	35.561754
1231.765742	84352.793699	35.566772
1233.224582	84483.190696	35.571789
1234.062904	84616.155709	35.576807
1235.484673	84738.564261	35.581824
1236.797205	84857.923941	35.586842
1238.020586	84989.550969	35.591860
1239.166927	85110.939604	35.596877
1240.242391	85230.844578	35.601895
1241.273307	85358.980651	35.606912
1242.901276	85479.079427	35.611930
1244.054016	85613.115183	35.616948
1245.625194	85721.223993	35.621965
1246.825647	85851.071849	35.626983
1248.289902	85973.884524	35.632000
1249.712927	86090.127573	35.637018
1250.912069	86212.323601	35.642036
1252.177055	86324.600616	35.647053
1253.598774	86440.503136	35.652071
1254.176106	86559.147942	35.657088
1255.661174	86660.671647	35.662106
1256.691596	86774.051344	35.667124
1258.069484	86892.066022	35.672141
1259.152788	86993.070512	35.677159
1260.584005	87100.838759	35.682176
1262.082066	87205.733106	35.687194
1263.346917	87327.036539	35.692212
1264.360532	87436.683143	35.697229
1265.382831	87541.019137	35.702247
1266.938944	87653.800862	35.707264
1268.031086	87773.371578	35.712282
1268.850498	87877.791039	35.717300
1270.218404	88016.809956	35.722317
1271.653829	88134.402498	35.727335
1272.934409	88268.265819	35.732352
1274.277368	88380.221778	35.737370
1275.572121	88513.310977	35.742388
1276.241870	88635.295382	35.747405
1278.051584	88770.295202	35.752423
1279.206274	88899.149891	35.757440
1280.316744	89017.924416	35.762458
1281.768749	89143.388252	35.767476
1283.350975	89268.756313	35.772493
1284.898355	89399.731810	35.777511
1286.257151	89527.087387	35.782528
1287.421756	89637.935288	35.787546
1288.901330	89765.171701	35.792564
1290.027526	89893.059304	35.797581
1291.819114	90015.951993	35.802599
1292.654401	90144.773086	35.807616
1294.517749	90256.731170	35.812634
1296.339911	90366.326151	35.817652
1297.568399	90491.108073	35.822669
1299.039937	90610.048198	35.827687
1300.122906	90715.209709	35.832704
1301.885066	90833.459133	35.837722
1302.770897	90941.757165	35.842740
1304.259326	91054.967919	35.847757
1305.504317	91166.645441	35.852775
1306.476725	91297.630035	35.857792
1307.681268	91409.758339	35.862810
1309.051342	91543.292924	35.867828
1310.275113	91651.857758	35.872845
1311.714754	91770.237108	35.877863
1312.931509	91900.615954	35.882880
1313.913796	92022.679595	35.887898
1315.004011	92152.255400	35.892916
1316.369556	92273.867499	35.897933
1317.955249	92394.178389	35.902951
1319.309726	92535.818657	35.907968
1320.901574	92648.170100	35.912986
1322.203203	92778.488809	35.918004
1323.575415	92907.960572	35.923021
1324.955671	93016.632678	35.928039
1326.075979	93141.670524	35.933056
1327.162121	93265.332661	35.938074
1328.517396	93390.018083	35.943092
1329.620729	93526.239240	35.948109
1330.936551	93656.698908	35.953127
1331.879664	93794.898119	35.958144
1333.151973	93921.601248	35.963162
1334.580318	94067.660667	35.968180
1335.902896	94199.743989	35.973197
1337.318423	94337.479180	35.978215
1338.964767	94465.533266	35.983232
1340.470828	94597.855914	35.988250
1341.585245	94724.536220	35.993268
1343.140536	94848.828841	35.998285
1344.512156	94961.717376	36.003303
1345.473175	95078.016539	36.008320
1346.286902	95190.194191	36.013338
1347.458082	95312.317580	36.018356
1349.013527	95439.413831	36.023373
1350.528752	95559.165014	36.028391
1352.851436	95674.303798	36.033408
1354.870762	95766.040201	36.038426
1356.426231	95868.674142	36.043444
1357.878496	95981.883402	36.048461
1359.761221	96090.374047	36.053479
1360.246656	96194.633329	36.058496
1361.230469	96311.567345	36.063514
1362.891165	96422.527477	36.068532
1363.954493	96531.121838	36.073549
1365.404394	96649.176111	36.078567
1366.273857	96780.491634	36.083584
1367.480021	96905.645395	36.088602
1368.743760	97021.993414	36.093620
1369.760826	97156.887572	36.098637
1371.231464	97280.049515	36.103655
1373.353846	97400.245642	36.108672
1374.946761	97522.996535	36.113690
1376.547473	97642.235318	36.118708
1377.778940	97765.563146	36.123725
1379.341290	97892.262620	36.128743
1380.283470	98023.356493	36.133760
1381.116341	98143.616715	36.138778
1382.862116	98272.038533	36.143796
1384.056397	98412.133254	36.148813
1385.095832	98545.939646	36.153831
1386.330621	98691.150717	36.158848
1387.711415	98843.147229	36.163866
1388.966161	98985.504227	36.168884
1389.879923	99124.885121	36.173901
1391.893520	99268.469029	36.178919
1393.101250	99418.378137	36.183936
1394.547043	99564.473085	36.188954
1395.771527	99711.477874	36.193972
1397.336373	99860.179828	36.198989
1399.130383	99994.901687	36.204007
1400.497459	100158.595106	36.209024
1401.336100	100301.086086	36.214042
1403.343179	100448.479526	36.219060
1404.518400	100590.361580	36.224077
1406.324557	100740.107625	36.229095
1407.500443	100893.616324	36.234112
1409.304419	101029.697461	36.239130
1411.147550	101168.448096	36.244148
1412.361509	101302.707858	36.249165
1414.477709	101441.353766	36.254183
1415.562757	101579.007062	36.259200
1416.905161	101704.018908	36.264218
1418.454166	101849.448838	36.269236
1419.870384	101988.345479	36.274253
1421.449804	102122.082635	36.279271
1422.614686	102254.731137	36.284288
1423.793655	102397.545984	36.289306
1425.277375	102527.255306	36.294324
1426.528510	102660.982362	36.299341
1428.768272	102781.902982	36.304359
1430.459362	102921.103103	36.309376
1432.106088	103043.131267	36.314394
1433.930727	103162.038613	36.319412
1435.927451	103265.375584	36.324429
1437.269691	103383.255768	36.329447
1438.639324	103501.918189	36.334464
1439.427528	103600.943361	36.339482
1440.718901	103699.167819	36.344500
1441.837401	103807.258261	36.349517
1443.446871	103911.405575	36.354535
1444.568549	104029.969009	36.359552
1445.836998	104137.504669	36.364570
1447.376843	104247.039757	36.369588
1448.172466	104373.072385	36.374605
1449.333608	104497.172088	36.379623
1450.741699	104623.503385	36.384640
1451.710951	104760.617392	36.389658
1453.414408	104888.843636	36.394676
1454.440181	105033.101063	36.399693
1455.869226	105180.909961	36.404711
1457.104551	105320.825022	36.409728
1458.392840	105476.277458	36.414746
1459.939013	105619.442040	36.419764
1461.068965	105775.922185	36.424781
1462.430785	105937.692417	36.429799
1463.816655	106094.020083	36.434816
1464.962621	106255.559156	36.439834
1466.474214	106420.186687	36.444852
1468.104079	106585.608120	36.449869
1470.252574	106746.613091	36.454887
1471.815937	106908.141017	36.459904
1473.460549	107060.958532	36.464922
1475.397372	107213.426927	36.469940
1476.907022	107373.925645	36.474957
1478.184114	107527.499858	36.479975
1479.599659	107691.045286	36.484992
1481.139629	107836.198284	36.490010
1482.453104	108001.916738	36.495028
1483.936337	108161.954074	36.500045
1485.422765	108328.547493	36.505063
1486.800730	108487.677044	36.510080
1488.137752	108657.211838	36.515098
1490.178013	108811.154850	36.520116
1491.873327	108983.932462	36.525133
1493.469121	109138.681592	36.530151
1495.326682	109281.229697	36.535168
1497.582307	109422.435654	36.540186
1499.235177	109566.513137	36.545204
1500.500263	109712.097210	36.550221
1502.057532	109856.596563	36.555239
1503.624215	110001.678381	36.560256
1504.466952	110152.871685	36.565274
1506.524261	110296.762414	36.570292
1507.830322	110447.517116	36.575309
1509.454684	110597.094282	36.580327
1510.843669	110755.649116	36.585344
1511.836279	110913.885912	36.590362
1513.115848	111064.279612	36.595380
1514.401746	111223.144264	36.600397
1516.491297	111380.743197	36.605415
1518.319621	111529.658482	36.610432
1519.534669	111684.249815	36.615450
1521.114456	111846.064406	36.620468
1522.769659	111999.244328	36.625485
1523.993068	112152.682342	36.630503
1525.530004	112311.956652	36.635520
1527.059045	112471.537269	36.640538
1529.075032	112625.754378	36.645556
1530.684756	112767.923942	36.650573
1532.441405	112918.289258	36.655591
1534.086081	113065.578165	36.660608
1535.186311	113222.958744	36.665626
1536.673642	113362.714709	36.670644
1537.964401	113516.490492	36.675661
1539.394466	113653.631239	36.680679
1540.872667	113790.600142	36.685696
1541.821568	113944.811428	36.690714
1543.475590	114074.436209	36.695732
1544.555573	114228.476105	36.700749
1545.723809	114377.074722	36.705767
1547.242025	114530.629159	36.710784
1548.973918	114704.963473	36.715802
1550.637535	114857.317152	36.720820
1551.867370	115011.197517	36.725837
1553.164799	115192.349087	36.730855
1554.794722	115359.168697	36.735872
1556.416988	115531.849847	36.740890
1557.911411	115682.749365	36.745908
1559.996939	115858.835127	36.750925
1561.565122	116032.909511	36.755943
1563.292022	116192.932252	36.760960
1564.722607	116374.665021	36.765978
1566.336242	116533.755609	36.770996
1567.949716	116702.245374	36.776013
1569.890867	116867.387178	36.781031
1571.894511	117021.776971	36.786048
1573.366786	117187.487830	36.791066
1574.905182	117364.046397	36.796084
1577.166554	117512.880688	36.801101
1578.640370	117663.956347	36.806119
1580.291163	117815.334849	36.811136
1582.049242	117976.260944	36.816154
1583.672169	118128.697810	36.821172
1585.779531	118285.816407	36.826189
1587.015617	118430.247657	36.831207
1588.787171	118582.878855	36.836224
1590.112739	118746.628008	36.841242
1591.705471	118894.087776	36.846260
1593.011739	119061.570457	36.851277
1594.559435	119231.058479	36.856295
1596.044447	119394.493866	36.861312
1597.324044	119567.969961	36.866330
1599.080026	119736.857010	36.871348
1600.520410	119902.990634	36.876365
1601.723290	120080.413209	36.881383
1603.617548	120255.559913	36.886400
1604.981212	120441.597402	36.891418
1606.360701	120605.916937	36.896436
1608.271554	120786.327664	36.901453
1609.654507	120973.506350	36.906471
1611.503275	121145.835437	36.911488
1613.025036	121334.313498	36.916506
1614.495618	121515.696782	36.921524
1615.895294	121704.436653	36.926541
1617.549463	121890.232912	36.931559
1618.914120	122076.645952	36.936576
1620.261544	122265.650370	36.941594
1622.163461	122454.303003	36.946612
1624.044343	122648.858558	36.951629
1625.627136	122840.911677	36.956647
1627.848297	123021.804543	36.961664
1629.112237	123208.505018	36.966682
1631.159425	123390.428814	36.971700
1632.812993	123568.215721	36.976717
1634.723374	123747.955127	36.981735
1636.327745	123925.916206	36.986752
1637.942879	124111.259617	36.991770
1639.805930	124281.012279	36.996788
1641.164151	124451.744943	37.001805
1642.860749	124638.486267	37.006823
1644.595256	124802.463598	37.011840
1645.805543	124991.946347	37.016858
1647.383784	125149.504818	37.021876
1649.195192	125316.681897	37.026893
1650.248687	125479.245616	37.031911
1652.255786	125647.395828	37.036928
1653.749756	125822.286998	37.041946
1655.200214	125988.089454	37.046964
1656.868441	126158.971383	37.051981
1658.125874	126337.529942	37.056999
1659.651155	126511.543819	37.062016
1661.781703	126689.942652	37.067034
1663.797670	126863.450306	37.072052
1665.620425	127045.755378	37.077069
1666.912588	127219.643613	37.082087
1668.288032	127392.974080	37.087104
1670.150934	127579.576143	37.092122
1671.501192	127771.422475	37.097140
1673.059335	127950.207658	37.102157
1674.611938	128149.585773	37.107175
1676.807950	128327.600880	37.112192
1678.600968	128514.446393	37.117210
1681.514336	128675.933977	37.122228
1683.657018	128837.453324	37.127245
1685.484858	129013.853924	37.132263
1687.153994	129184.316839	37.137280
1688.284730	129363.580592	37.142298
1689.835946	129536.232857	37.147316
1691.618744	129711.425380	37.152333
1692.866670	129901.280061	37.157351
1693.991929	130079.494622	37.162368
1695.863262	130285.963793	37.167386
1697.070156	130467.821371	37.172404
1698.789073	130668.289373	37.177421
1699.893113	130889.015258	37.182439
1701.401344	131089.619529	37.187456
1703.258828	131302.807759	37.192474
1704.325175	131519.203409	37.197492
1705.898270	131740.647331	37.202509
1707.646579	131970.896193	37.207527
1709.348648	132192.753759	37.212544
1710.999317	132411.359524	37.217562
1712.932686	132641.583139	37.222580
1714.337052	132877.638236	37.227597
1715.776243	133108.321881	37.232615
1717.518212	133338.071405	37.237632
1719.650746	133570.299100	37.242650
1721.707649	133814.974875	37.247668
1723.823933	134032.792988	37.252685
1725.078469	134263.346460	37.257703
1727.566064	134496.779969	37.262720
1728.925350	134720.581619	37.267738
1730.728843	134950.444132	37.272756
1732.537513	135165.676314	37.277773
1734.323482	135403.487348	37.282791
1735.976245	135625.687056	37.287808
1737.922680	135854.021909	37.292826
1740.408854	136060.879411	37.297844
1742.831903	136259.918229	37.302861
1744.077991	136482.616884	37.307879
1746.181023	136696.820758	37.312896
1747.937533	136908.414726	37.317914
1749.468352	137112.075609	37.322932
1750.901227	137327.478061	37.327949
1752.184642	137548.957871	37.332967
1754.557031	137765.510520	37.337984
1755.968002	137987.708602	37.343002
1757.758735	138206.092377	37.348020
1759.231982	138411.189246	37.353037
1761.195707	138634.763762	37.358055
1763.053494	138841.211288	37.363072
1764.373541	139043.949012	37.368090
1765.393242	139251.708985	37.373108
1767.353062	139449.577307	37.378125
1769.310622	139664.515515	37.383143
1770.885969	139879.120782	37.388160
1772.607439	140097.854106	37.393178
1774.049192	140321.746310	37.398196
1776.181002	140526.521470	37.403213
1777.532644	140747.790031	37.408231
1779.255112	140965.943411	37.413248
1781.282810	141190.548015	37.418266
1782.939652	141423.117851	37.423284
1785.237490	141656.248980	37.428301
1786.564605	141882.704516	37.433319
1788.366201	142108.858822	37.438336
1789.928563	142350.192009	37.443354
1791.209673	142582.013647	37.448372
1793.350527	142824.312517	37.453389
1794.974386	143062.669882	37.458407
1796.766187	143313.757165	37.463424
1798.970146	143559.831890	37.468442
1800.130566	143795.447410	37.473460
1802.284215	144052.916754	37.478477
1804.204606	144295.472914	37.483495
1806.164241	144538.531815	37.488512
1808.441564	144782.202427	37.493530
1810.104562	145035.311060	37.498548
1812.091841	145284.042541	37.503565
1813.209104	145535.817122	37.508583
1815.027182	145796.837939	37.513600
1816.984453	146054.348093	37.518618
1818.368010	146318.536092	37.523636
1820.463136	146573.095506	37.528653
1822.169548	146842.719017	37.533671
1823.603832	147120.306349	37.538688
1825.819948	147380.676735	37.543706
1827.541664	147649.565907	37.548724
1829.528242	147919.925665	37.553741
1831.224893	148184.645632	37.558759
1833.098393	148448.235145	37.563776
1835.065388	148723.361866	37.568794
1836.730834	149002.700210	37.573812
1838.267410	149270.116042	37.578829
1840.513498	149548.998797	37.583847
1842.284608	149821.648486	37.588864
1844.113169	150104.572046	37.593882
1846.003626	150389.315282	37.598900
1847.782099	150663.313570	37.603917
1850.066442	150945.751728	37.608935
1851.860668	151221.552835	37.613952
1854.466751	151477.287585	37.618970
1856.102139	151767.040870	37.623988
1858.237786	152037.220499	37.629005
1860.313264	152301.774843	37.634023
1862.044664	152565.762013	37.639040
1863.825579	152830.872473	37.644058
1865.862642	153098.153051	37.649076
1867.761778	153354.336541	37.654093
1869.390947	153623.968005	37.659111
1871.933257	153885.601061	37.664128
1873.789361	154136.476023	37.669146
1875.625127	154398.284880	37.674164
1877.536922	154662.583856	37.679181
1879.646304	154908.967149	37.684199
1881.080705	155170.410403	37.689216
1883.526158	155424.944104	37.694234
1885.019534	155682.445256	37.699252
1886.616060	155906.748233	37.704269
1888.477208	156157.326561	37.709287
1890.128590	156394.990178	37.714304
1891.771753	156640.056984	37.719322
1893.054715	156885.168176	37.724340
1894.696380	157142.779617	37.729357
1896.693388	157411.000471	37.734375
1898.033022	157668.013763	37.739392
1899.864415	157927.401736	37.744410
1901.342832	158206.459426	37.749428
1903.099144	158487.874510	37.754445
1904.829191	158774.373011	37.759463
1906.572790	159068.767110	37.764480
1908.382206	159355.014783	37.769498
1910.105643	159652.677490	37.774516
1912.173411	159948.498010	37.779533
1914.220329	160260.166991	37.784551
1916.202174	160551.801602	37.789568
1918.362873	160836.300277	37.794586
1921.044960	161129.237799	37.799604
1922.718134	161424.491956	37.804621
1924.737281	161722.867558	37.809639
1926.336053	162037.915975	37.814656
1928.161158	162326.853607	37.819674
1930.743124	162624.320604	37.824692
1932.506665	162918.183760	37.829709
1934.465077	163222.111196	37.834727
1936.418349	163535.931040	37.839744
1938.611561	163835.317710	37.844762
1940.318844	164136.939711	37.849780
1942.394227	164441.527492	37.854797
1944.369640	164742.755031	37.859815
1946.250889	165070.013299	37.864832
1947.842087	165373.830041	37.869850
1949.757424	165680.479792	37.874868
1952.157355	166000.666131	37.879885
1953.849974	166309.854592	37.884903
1955.914479	166634.781129	37.889920
1958.075349	166945.346989	37.894938
1959.601028	167270.741280	37.899956
1961.464561	167585.825523	37.904973
1963.529062	167916.979482	37.909991
1965.448200	168230.610529	37.915008
1967.874559	168553.191551	37.920026
1969.328153	168886.908334	37.925044
1971.297197	169214.413772	37.930061
1973.403498	169537.760081	37.935079
1975.666550	169857.693294	37.940096
1978.062086	170176.985131	37.945114
1979.948357	170505.271111	37.950132
1981.719080	170826.758067	37.955149
1984.197027	171142.028905	37.960167
1986.257733	171467.473181	37.965184
1988.293824	171784.758209	37.970202
1990.120090	172100.693195	37.975220
1992.439862	172414.698841	37.980237
1995.136713	172733.370622	37.985255
1996.365092	173048.970866	37.990272
1998.535853	173352.375559	37.995290
2000.368996	173665.128779	38.000308
2002.272272	173984.919650	38.005325
2005.034086	174293.150084	38.010343
2006.153513	174606.970473	38.015360
2008.784861	174909.776185	38.020378
2010.679224	175238.068465	38.025396
2012.308617	175546.975211	38.030413
2014.392733	175862.948729	38.035431
2016.345862	176174.893130	38.040448
2018.563495	176471.407266	38.045466
2020.007435	176769.122234	38.050484
2021.535116	177076.031536	38.055501
2023.547280	177380.199902	38.060519
2025.153481	177695.556382	38.065536
2029.654962	177941.688461	38.070554
2032.317633	178202.380563	38.075572
2034.048975	178501.720429	38.080589
2036.138044	178782.795866	38.085607
2037.492692	179067.161175	38.090624
2039.323081	179363.313943	38.095642
2041.112158	179660.490039	38.100660
2042.449251	179966.220258	38.105677
2044.285728	180274.058005	38.110695
2045.494442	180594.693371	38.115712
2047.313100	180916.200068	38.120730
2048.937851	181263.567752	38.125748
2050.439719	181603.158693	38.130765
2052.372640	181958.887787	38.135783
2053.729271	182323.343319	38.140800
2055.574866	182665.449865	38.145818
2057.808422	183042.089877	38.150836
2059.338572	183426.358804	38.155853
2061.012232	183802.707970	38.160871
2063.039407	184188.756676	38.165888
2065.487210	184572.988925	38.170906
2067.819882	184969.813039	38.175924
2069.577712	185372.392172	38.180941
2071.994899	185843.955866	38.185959
2073.971229	186245.539296	38.190976
2076.136921	186625.302212	38.195994
2078.298325	187029.247415	38.201012
2080.375548	187426.197010	38.206029
2083.123255	187807.753187	38.211047
2085.876761	188196.370932	38.216064
2088.302612	188576.303544	38.221082
2090.994614	188948.957094	38.226100
2094.143084	189313.082682	38.231117
2097.414232	189660.959752	38.236135
2099.430979	190007.763115	38.241152
2101.605805	190361.654983	38.246170
2103.449801	190720.044473	38.251188
2105.265080	191080.598566	38.256205
2107.637782	191440.305005	38.261223
2108.992861	191800.526515	38.266240
2111.075627	192156.419364	38.271258
2113.106411	192523.421430	38.276276
2114.923900	192894.013891	38.281293
2117.116196	193248.343427	38.286311
2119.291719	193615.097599	38.291328
2121.159378	193990.054447	38.296346
2123.277890	194358.572300	38.301364
2125.700881	194724.478306	38.306381
2127.789881	195097.244822	38.311399
2130.249709	195472.571000	38.316416
2131.542894	195843.710770	38.321434
2133.602383	196219.888770	38.326452
2135.835484	196590.731880	38.331469
2137.990017	196968.802231	38.336487
2139.343745	197345.601137	38.341504
2141.513910	197735.279610	38.346522
2143.806696	198121.790236	38.351540
2145.225833	198522.154799	38.356557
2147.813576	198920.458831	38.361575
2149.182416	199319.918880	38.366592
2151.439614	199735.448171	38.371610
2153.576657	200132.453779	38.376628
2155.313277	200529.903730	38.381645
2157.311217	200917.788182	38.386663
2159.608058	201312.155407	38.391680
2161.417145	201693.161671	38.396698
2163.368749	202083.088238	38.401716
2165.089960	202493.830707	38.406733
2167.549965	202883.654554	38.411751
2169.620993	203299.831392	38.416768
2171.384594	203718.419472	38.421786
2173.373427	204127.041023	38.426804
2175.739905	204549.398348	38.431821
2178.021675	204977.841044	38.436839
2179.990128	205394.952988	38.441856
2182.073766	205824.241246	38.446874
2184.534628	206249.991505	38.451892
2186.363476	206687.958204	38.456909
2188.703098	207123.737863	38.461927
2190.746928	207560.656761	38.466944
2193.158564	207996.045894	38.471962
2195.950168	208440.623471	38.476980
2198.196870	208871.848402	38.481997
2200.957070	209299.412336	38.487015
2203.296807	209740.531595	38.492032
2205.621023	210160.874113	38.497050
2208.330772	210584.942415	38.502068
2210.417831	211017.567635	38.507085
2212.977829	211434.318987	38.512103
2215.457384	211861.575113	38.517120
2217.501616	212290.525440	38.522138
2219.506569	212708.152505	38.527156
2222.360844	213138.883227	38.532173
2224.521661	213568.299847	38.537191
2226.636163	213980.576760	38.542208
2229.245636	214403.472091	38.547226
2231.910771	214818.458706	38.552244
2234.202339	215242.573063	38.557261
2236.623115	215642.254753	38.562279
2238.907175	216063.779984	38.567296
2241.143835	216484.169847	38.572314
2243.182674	216911.094288	38.577332
2245.143791	217346.058849	38.582349
2247.152726	217757.644781	38.587367
2249.278338	218200.561322	38.592384
2251.056709	218635.326801	38.597402
2253.574821	219070.409359	38.602420
2255.665257	219520.699559	38.607437
2257.746739	219954.351854	38.612455
2259.966759	220398.982796	38.617472
2262.130604	220852.234709	38.622490
2264.257225	221298.684387	38.627508
2266.170570	221750.527734	38.632525
2268.426798	222196.474993	38.637543
2270.749899	222658.365777	38.642560
2272.384396	223119.246116	38.647578
2274.744790	223573.256143	38.652596
2276.909163	224049.169713	38.657613
2278.630100	224516.337175	38.662631
2281.291330	225000.709372	38.667648
2283.770116	225473.779786	38.672666
2286.520798	225949.805592	38.677684
2288.830308	226428.973948	38.682701
2290.900722	226899.821535	38.687719
2293.220728	227369.360019	38.692736
2295.460837	227846.938549	38.697754
2297.790214	228314.722506	38.702772
2299.966446	228802.091301	38.707789
2302.407495	229281.949920	38.712807
2305.677144	229736.656404	38.717824
2308.597666	230190.299248	38.722842
2310.412126	230620.285029	38.727860
2312.938477	231055.266013	38.732877
2315.520411	231486.859376	38.737895
2318.290451	231903.942937	38.742912
2320.375288	232332.361431	38.747930
2322.985851	232743.677172	38.752948
2324.620428	233175.112007	38.757965
2326.362671	233610.568978	38.762983
2328.715564	234051.163758	38.768000
2330.591314	234500.012451	38.773018
2333.020837	234938.003308	38.778036
2335.232508	235390.838068	38.783053
2337.091963	235852.948741	38.788071
2339.406736	236309.068957	38.793088
2341.660149	236776.350428	38.798106
2344.339339	237238.357297	38.803124
2346.751630	237705.993915	38.808141
2348.719647	238183.987509	38.813159
2350.877047	238662.255786	38.818176
2352.758860	239144.452978	38.823194
2354.976694	239648.190105	38.828212
2357.114863	240149.500043	38.833229
2359.667857	240632.454082	38.838247
2362.338314	241127.176165	38.843264
2364.497606	241621.900674	38.848282
2366.535390	242123.451228	38.853300
2369.152178	242641.778417	38.858317
2371.382401	243155.769914	38.863335
2374.629434	243653.420267	38.868352
2377.455024	244147.705716	38.873370
2380.043418	244646.548721	38.878388
2382.196476	245152.012290	38.883405
2384.534946	245659.274806	38.888423
2387.346537	246163.261692	38.893440
2389.718862	246662.666972	38.898458
2392.137052	247159.548979	38.903476
2394.711311	247663.721367	38.908493
2397.036159	248165.238543	38.913511
2399.534661	248666.143064	38.918528
2401.697397	249184.321273	38.923546
2404.375313	249689.614999	38.928564
2406.893601	250203.518042	38.933581
2409.517285	250702.746050	38.938599
2412.092773	251211.023193	38.943616
2414.090010	251713.851082	38.948634
2416.272718	252224.040472	38.953652
2418.542479	252746.712350	38.958669
2421.098043	253259.177245	38.963687
2424.077245	253775.765728	38.968704
2426.285587	254279.949368	38.973722
2428.367762	254800.636448	38.978740
2430.945658	255320.660230	38.983757
2433.152627	255837.285210	38.988775
2435.785306	256362.148176	38.993792
2437.561154	256893.645113	38.998810
2440.337546	257412.994923	39.003828
2443.120349	257934.322921	39.008845
2445.783967	258449.113927	39.013863
2449.033186	258960.636598	39.018880
2451.420366	259470.945070	39.023898
2454.805743	259969.208631	39.028916
2456.975772	260471.570911	39.033933
2459.298212	260970.452899	39.038951
2461.890554	261465.506120	39.043968
2464.202073	261975.104336	39.048986
2466.804084	262465.681297	39.054004
2469.110686	262972.253163	39.059021
2470.867621	263468.240361	39.064039
2473.380140	263960.500968	39.069056
2475.122778	264452.269537	39.074074
2477.792450	264936.855934	39.079092
2479.817964	265430.963445	39.084109
2481.606570	265925.308654	39.089127
2483.735511	266429.986688	39.094144
2486.279095	266954.865952	39.099162
2488.023648	267469.910493	39.104180
2490.315910	268003.992231	39.109197
2492.531814	268534.120752	39.114215
2494.646203	269077.697836	39.119232
2497.376060	269634.738625	39.124250
2499.911130	270180.504292	39.129268
2502.191096	270729.100189	39.134285
2504.626018	271282.189455	39.139303
2507.383854	271841.599847	39.144320
2509.534395	272415.425339	39.149338
2511.968635	272977.875777	39.154356
2514.766568	273551.720029	39.159373
2517.686717	274100.322326	39.164391
2521.011073	274660.743821	39.169408
2524.195990	275226.491135	39.174426
2526.813888	275791.840288	39.179444
2529.355576	276345.997677	39.184461
2531.665863	276910.066326	39.189479
2534.400860	277466.623926	39.194496
2536.672086	278054.384840	39.199514
2538.596535	278615.149151	39.204532
2541.359314	279204.704144	39.209549
2543.949674	279785.799475	39.214567
2546.281322	280362.969008	39.219584
2549.083759	280954.002504	39.224602
2551.732508	281535.481488	39.229620
2553.861977	282123.969306	39.234637
2556.434621	282727.873759	39.239655
2559.272686	283312.940383	39.244672
2561.559344	283906.874198	39.249690
2564.216151	284509.861629	39.254708
2566.926180	285114.765436	39.259725
2569.690386	285711.885252	39.264743
2572.299712	286313.924741	39.269760
2575.139006	286916.100823	39.274778
2577.734841	287505.435476	39.279796
2581.070580	288091.221809	39.284813
2583.493078	288681.740951	39.289831
2586.813267	289265.919474	39.294848
2589.868442	289840.510602	39.299866
2592.156802	290417.983521	39.304884
2594.971501	290994.607528	39.309901
2597.573616	291573.696816	39.314919
2600.107883	292146.469041	39.319936
2603.058764	292729.961941	39.324954
2605.817655	293305.912930	39.329972
2608.621021	293880.505858	39.334989
2610.565884	294463.580020	39.340007
2613.602200	295027.309748	39.345024
2616.245663	295604.830664	39.350042
2618.710544	296180.875735	39.355060
2621.525921	296744.851790	39.360077
2624.169312	297318.420446	39.365095
2626.812756	297891.094752	39.370112
2629.379884	298451.842915	39.375130
2631.772001	299020.406671	39.380148
2635.230991	299570.519811	39.385165
2638.306862	300154.756392	39.390183
2640.927413	300708.644367	39.395200
2643.275570	301262.315238	39.400218
2645.358316	301819.118859	39.405236
2647.761156	302355.405852	39.410253
2650.093724	302890.175247	39.415271
2652.624881	303428.208439	39.420288
2654.963133	303977.740226	39.425306
2657.114294	304519.324496	39.430324
2659.732754	305075.350380	39.435341
2662.068079	305638.725004	39.440359
2664.334373	306198.956541	39.445376
2666.572795	306782.056994	39.450394
2668.890567	307363.386894	39.455412
2671.593968	307954.422544	39.460429
2673.744999	308560.817593	39.465447
2676.375379	309169.770373	39.470464
2678.801547	309781.590163	39.475482
2680.863037	310397.367811	39.480500
2683.588213	311012.831265	39.485517
2686.252074	311642.662126	39.490535
2689.028287	312283.634746	39.495552
2692.024946	312929.335891	39.500570
2694.607498	313575.549418	39.505588
2697.543637	314224.592236	39.510605
2699.707662	314878.466659	39.515623
2702.219259	315531.592424	39.520640
2705.029327	316192.047570	39.525658
2707.564903	316861.519704	39.530676
2710.558908	317532.230148	39.535693
2713.216816	318201.663143	39.540711
2716.001868	318870.025733	39.545728
2719.433065	319538.759736	39.550746
2721.964763	320215.540881	39.555764
2725.115165	320875.644594	39.560781
2728.328480	321548.746057	39.565799
2731.041820	322211.891468	39.570816
2734.256182	322874.441015	39.575834
2737.151752	323545.251036	39.580852
2740.585294	324210.967868	39.585869
2743.425352	324869.890105	39.590887
2745.887961	325526.881418	39.595904
2748.904074	326185.019305	39.600922
2751.602768	326851.213595	39.605940
2754.720817	327490.361214	39.610957
2757.177929	328156.064042	39.615975
2760.529661	328810.148767	39.620992
2763.403244	329467.696762	39.626010
2765.792389	330121.300638	39.631028
2768.929995	330774.726367	39.636045
2771.725030	331441.361146	39.641063
2774.369198	332086.368121	39.646080
2776.992935	332752.372605	39.651098
2779.257034	333425.778170	39.656116
2782.149351	334077.689047	39.661133
2784.659881	334749.206179	39.666151
2787.221005	335422.808824	39.671168
2790.269400	336104.516749	39.676186
2792.784124	336776.554656	39.681204
2795.865996	337445.270600	39.686221
2798.626060	338128.938930	39.691239
2801.142399	338808.396440	39.696256
2804.099865	339476.434809	39.701274
2806.326609	340174.097513	39.706292
2808.997888	340859.604603	39.711309
2812.441972	341548.630351	39.716327
2815.411738	342231.477367	39.721344
2818.160556	342913.102720	39.726362
2821.048721	343602.352043	39.731380
2823.860414	344278.970003	39.736397
2825.945786	344966.719259	39.741415
2828.630988	345657.074794	39.746432
2831.544545	346323.644781	39.751450
2833.882661	346984.915167	39.756468
2837.322530	347649.500484	39.761485
2839.583144	348318.465426	39.766503
2842.095448	348989.837356	39.771520
2844.944894	349659.292160	39.776538
2847.554808	350341.194992	39.781556
2850.432588	351018.351168	39.786573
2853.697650	351713.941994	39.791591
2856.374540	352401.825611	39.796608
2859.543904	353076.484628	39.801626
2861.996032	353768.151609	39.806644
2865.366500	354460.700095	39.811661
2868.274000	355145.801234	39.816679
2871.261912	355834.145285	39.821696
2874.037755	356535.486892	39.826714
2876.721695	357246.333392	39.831732
2879.507085	357944.371469	39.836749
2882.809482	358659.195853	39.841767
2885.526258	359365.374741	39.846784
2888.404213	360074.655329	39.851802
2890.918628	360803.087857	39.856820
2894.143345	361512.306068	39.861837
2897.323445	362231.044618	39.866855
2900.398494	362942.203838	39.871872
2903.938910	363660.750357	39.876890
2906.666545	364379.709978	39.881908
2909.901899	365081.237825	39.886925
2912.791861	365798.540663	39.891943
2915.781560	366506.509547	39.896960
2919.422919	367221.632799	39.901978
2921.954021	367936.682953	39.906996
2925.141181	368648.369531	39.912013
2928.133149	369369.571181	39.917031
2930.870549	370087.981400	39.922048
2934.051944	370801.971278	39.927066
2937.041937	371530.896866	39.932084
2939.598262	372248.088989	39.937101
2942.359990	372979.824573	39.942119
2945.379937	373702.936984	39.947136
2948.442010	374433.903108	39.952154
2950.645382	375182.084235	39.957172
2953.562767	375914.451916	39.962189
2956.191180	376676.307385	39.967207
2958.760214	377412.919270	39.972224
2962.260587	378167.858254	39.977242
2965.258137	378920.827600	39.982260
2968.562129	379672.967964	39.987277
2971.262540	380433.640939	39.992295
2974.264653	381198.626841	39.997312
2977.353604	381951.495254	40.002330
2980.213166	382710.988038	40.007348
2983.073775	383478.031062	40.012365
2985.997518	384249.979974	40.017383
2988.605120	385025.804252	40.022400
2991.643614	385799.359960	40.027418
2994.444278	386589.440118	40.032436
2997.271087	387364.652265	40.037453
3000.339514	388140.284002	40.042471
3003.052860	388940.331337	40.047488
3006.332601	389721.552955	40.052506
3009.175286	390509.679554	40.057524
3012.172429	391297.199880	40.062541
3015.760725	392093.717405	40.067559
3018.784218	392883.461149	40.072576
3022.273295	393666.828273	40.077594
3025.591510	394448.221958	40.082612
3028.906548	395216.123277	40.087629
3031.936525	395954.275065	40.092647
3034.608408	396702.787494	40.097664
3038.030820	397430.808329	40.102682
3040.627492	398177.969558	40.107700
3043.475689	398911.906278	40.112717
3046.815203	399648.021433	40.117735
3049.332041	400394.466284	40.122752
3052.664482	401135.394828	40.127770
3055.208412	401889.481030	40.132788
3058.009628	402640.566899	40.137805
3060.866434	403408.220173	40.142823
3063.154594	404183.426393	40.147840
3066.283188	404953.060275	40.152858
3069.206541	405743.347394	40.157876
3072.239608	406535.765696	40.162893
3074.940511	407331.699270	40.167911
3077.833389	408146.752421	40.172928
3082.143472	408935.395260	40.177946
3085.317882	409726.109383	40.182964
3088.641022	410526.941691	40.187981
3091.979005	411317.320080	40.192999
3095.349353	412116.923136	40.198016
3098.497348	412910.561714	40.203034
3101.912235	413716.877884	40.208052
3105.180367	414502.395680	40.213069
3108.603166	415300.962026	40.218087
3111.613067	416108.060631	40.223104
3114.835971	416904.473494	40.228122
3117.526747	417706.351127	40.233140
3120.253375	418517.397666	40.238157
3123.604678	419328.366228	40.243175
3126.750054	420153.445202	40.248192
3129.946435	420974.791839	40.253210
3132.560350	421799.685802	40.258228
3135.387211	422634.879847	40.263245
3138.689631	423467.741075	40.268263
3141.731321	424305.260719	40.273280
3145.252469	425124.873954	40.278298
3148.456698	425969.428750	40.283316
3151.538212	426814.523429	40.288333
3154.621113	427656.953535	40.293351
3157.929231	428516.500871	40.298368
3161.136467	429359.850833	40.303386
3164.489889	430216.790116	40.308404
3167.584973	431063.117846	40.313421
3170.708663	431915.773193	40.318439
3174.026979	432768.563308	40.323456
3177.385297	433607.512754	40.328474
3180.671389	434468.521812	40.333492
3184.138538	435322.945409	40.338509
3187.387062	436165.490022	40.343527
3190.941912	437017.702279	40.348544
3194.145529	437859.067678	40.353562
3197.634430	438703.534593	40.358580
3201.247579	439557.746074	40.363597
3204.613231	440391.748955	40.368615
3207.491100	441242.866111	40.373632
3210.463605	442074.278903	40.378650
3213.692102	442915.263026	40.383668
3216.766808	443751.939477	40.388685
3219.813121	444611.614937	40.393703
3223.039246	445453.342704	40.398720
3226.293875	446290.330456	40.403738
3229.836486	447132.941879	40.408756
3232.741251	447985.865141	40.413773
3236.007631	448816.220403	40.418791
3239.194695	449673.211569	40.423808
3242.326758	450504.721868	40.428826
3245.341655	451317.732127	40.433844
3248.556640	452122.697022	40.438861
3252.481527	452918.780872	40.443879
3255.801656	453726.685894	40.448896
3258.593953	454533.323575	40.453914
3261.817994	455338.039844	40.458932
3264.637897	456146.164053	40.463949
3268.382982	456946.989961	40.468967
3271.480115	457774.630311	40.473984
3274.428790	458592.412608	40.479002
3277.910159	459420.318272	40.484020
3280.514185	460252.105554	40.489037
3283.925369	461088.470425	40.494055
3286.446427	461933.359767	40.499072
3289.196852	462796.033572	40.504090
3292.420091	463653.897622	40.509108
3295.310402	464543.908248	40.514125
3298.920802	465414.538380	40.519143
3301.819112	466307.027361	40.524160
3305.050200	467187.915548	40.529178
3308.430099	468087.801006	40.534196
3311.323441	469004.459132	40.539213
3314.671118	469916.859937	40.544231
3318.093990	470838.125182	40.549248
3321.662890	471750.944451	40.554266
3325.278469	472674.900402	40.559284
3328.484827	473596.548007	40.564301
3331.592214	474533.638159	40.569319
3335.062452	475471.272901	40.574336
3338.436262	476414.060832	40.579354
3341.926952	477348.456914	40.584372
3345.122175	478292.119724	40.589389
3348.746801	479231.123044	40.594407
3352.034061	480184.034717	40.599424
3355.744300	481126.037158	40.604442
3359.222329	482077.746077	40.609460
3362.507273	483041.773939	40.614477
3365.903989	483990.254491	40.619495
3369.433994	484962.792598	40.624512
3372.526894	485921.632701	40.629530
3376.160706	486886.878696	40.634548
3379.566262	487856.482510	40.639565
3382.815789	488815.570902	40.644583
3386.768813	489771.718931	40.649600
3390.231450	490735.438482	40.654618
3394.138256	491691.271039	40.659636
3397.603892	492645.802135	40.664653
3400.994201	493598.018029	40.669671
3404.625914	494564.286002	40.674688
3407.537723	495527.279973	40.679706
3410.932453	496478.001873	40.684724
3414.531217	497440.110034	40.689741
3418.282216	498405.001260	40.694759
3421.816571	499363.117125	40.699776
3425.355490	500319.206346	40.704794
3428.835438	501280.275390	40.709812
3432.182295	502245.780932	40.714829
3435.723466	503189.953699	40.719847
3439.090186	504150.799295	40.724864
3442.478386	505101.009943	40.729882
3446.253965	506060.556841	40.734900
3449.135997	507028.832170	40.739917
3452.672186	507987.129201	40.744935
3455.988923	508947.659318	40.749952
3459.140131	509920.021410	40.754970
3462.379646	510882.091594	40.759988
3465.592249	511855.466901	40.765005
3468.827685	512822.287984	40.770010
3472.356272	513745.584336	40.775015
3475.561958	514624.705857	40.780020
3478.740641	515448.019963	40.785024
3481.523297	516238.126851	40.790029
3484.374527	516964.463899	40.795034
3487.478899	517634.825038	40.800039
3489.667312	518264.772873	40.805044
3492.489275	518824.789647	40.810048
3494.841406	519342.068846	40.815053
3497.213354	519799.706850	40.820058
3499.118417	520222.629903	40.825063
3501.232191	520584.178954	40.830068
3503.543921	520900.637190	40.835072
3504.608080	521185.283960	40.840077
3506.841453	521411.592788	40.845082
3508.012798	521603.193700	40.850087
3509.172765	521759.975077	40.855092
3510.704107	521874.723433	40.860096
3511.621577	521975.508106	40.865101
3512.766993	522050.609258	40.870106
3513.493391	522089.395459	40.875111
3514.051795	522095.052761	40.880116
3515.182245	522075.326510	40.885120
3515.583991	522054.857037	40.890125
3516.479970	521996.217456	40.895130
3516.815040	521918.870139	40.900135
3517.255357	521836.971041	40.905140
3517.644518	521724.745338	40.910144
3517.944118	521614.497822	40.915149
3518.595258	521487.062193	40.920154
3519.251099	521343.247794	40.925159
3519.190503	521191.581597	40.930164
3519.399411	521011.400571	40.935168
3519.188004	520844.586086	40.940173
3519.525518	520670.729919	40.945178
3519.489908	520481.307602	40.950183
3519.890754	520291.613141	40.955188
3520.009276	520093.241635	40.960192
3519.406607	519897.398446	40.965197
3520.075230	519683.514259	40.970202
3520.072068	519479.810694	40.975207
3520.046080	519264.163300	40.980212
3520.050138	519041.653568	40.985216
3520.135634	518809.853981	40.990221
3520.132181	518582.297940	40.995226
3520.172228	518359.368258	41.000231
3519.932520	518113.898262	41.005236
3519.887691	517894.048727	41.010240
3519.088578	517664.383458	41.015245
3519.780514	517430.046680	41.020250
3519.789916	517195.106427	41.025255
3519.526289	516962.573737	41.030260
3519.813404	516717.601588	41.035264
3519.254345	516490.399644	41.040269
3519.215133	516246.225988	41.045274
3519.045891	516004.689553	41.050279
3518.859171	515777.165826	41.055284
3519.071838	515535.360080	41.060288
3518.286514	515306.056486	41.065293
3518.292709	515077.533347	41.070298
3518.280621	514836.708185	41.075303
3518.113732	514609.666254	41.080308
3517.617698	514372.487784	41.085312
3517.518755	514148.301419	41.090317
3517.295325	513920.904067	41.095322
3517.184365	513715.518338	41.100327
3516.952199	513483.779195	41.105332
3516.807786	513268.509882	41.110336
3516.672622	513065.286361	41.115341
3516.780418	512838.626471	41.120346
3516.324689	512625.563777	41.125351
3516.125809	512420.626396	41.130356
3516.113104	512205.471413	41.135360
3515.950367	512012.019039	41.140365
3516.079793	511789.221409	41.145370
3516.017224	511585.662464	41.150375
3515.614601	511379.833837	41.155380
3515.676681	511171.307632	41.160384
3515.723613	510976.497184	41.165389
3515.712102	510772.918474	41.170394
3515.473850	510577.793860	41.175399
3515.095298	510376.182837	41.180404
3514.866116	510176.008179	41.185408
3514.895188	509975.034003	41.190413
3514.340453	509786.352491	41.195418
3514.745369	509597.216515	41.200423
3514.005874	509409.819537	41.205428
3514.094089	509220.576486	41.210432
3514.324856	509036.806158	41.215437
3513.929704	508845.716758	41.220442
3513.801868	508660.131200	41.225447
3513.806109	508491.368688	41.230452
3513.764856	508303.646615	41.235456
3513.791463	508124.183410	41.240461
3513.019469	507945.951864	41.245466
3513.085348	507766.478015	41.250471
3512.724888	507593.272410	41.255476
3512.936994	507425.877188	41.260480
3512.540754	507272.748739	41.265485
3512.716534	507101.219138	41.270490
3512.517073	506929.745859	41.275495
3512.481240	506770.452339	41.280500
3512.387705	506610.510245	41.285504
3512.009031	506451.922281	41.290509
3512.058613	506283.227349	41.295514
3512.115025	506132.286214	41.300519
3511.648981	505973.050725	41.305524
3511.642039	505826.656367	41.310528
3511.825632	505670.040526	41.315533
3511.561595	505523.884863	41.320538
3511.238727	505359.272789	41.325543
3510.762128	505222.026016	41.330548
3510.910299	505070.807146	41.335552
3510.401460	504938.708503	41.340557
3510.631197	504790.147817	41.345562
3510.751795	504649.573805	41.350567
3510.398300	504506.953237	41.355572
3510.711790	504379.362995	41.360576
3510.400967	504241.273804	41.365581
3510.573468	504112.946353	41.370586
3510.544989	503973.852054	41.375591
3510.130997	503842.283542	41.380596
3509.934537	503703.212766	41.385600
3510.215853	503573.652672	41.390605
3509.850963	503445.100163	41.395610
3509.868992	503302.863931	41.400615
3510.029212	503190.373197	41.405620
3510.179711	503066.782704	41.410624
3509.901664	502927.717141	41.415629
3509.694705	502808.771636	41.420634
3509.719918	502683.582727	41.425639
3509.394144	502560.566593	41.430644
3509.520435	502433.038712	41.435648
3509.642829	502308.941525	41.440653
3509.370361	502188.386421	41.445658
3509.479288	502065.046131	41.450663
3509.316438	501944.270098	41.455668
3509.368356	501817.152048	41.460672
3509.060406	501703.864774	41.465677
3508.593828	501579.752072	41.470682
3509.047312	501470.583257	41.475687
3508.658474	501361.140999	41.480692
3508.608854	501245.135442	41.485696
3508.445217	501139.895339	41.490701
3508.613005	501020.119887	41.495706
3508.509311	500922.387939	41.500711
3508.320589	500815.837335	41.505716
3508.547574	500709.423120	41.510720
3508.279725	500599.703978	41.515725
3508.093944	500491.636595	41.520730
3508.300780	500387.998760	41.525735
3507.775175	500290.328225	41.530740
3507.802493	500181.872121	41.535744
3507.881106	500090.364054	41.540749
3508.355172	499989.760275	41.545754
3508.070527	499881.350484	41.550759
3507.609031	499788.965694	41.555764
3507.845430	499678.555542	41.560768
3507.771025	499580.709108	41.565773
3507.476612	499488.346885	41.570778
3507.940930	499400.256822	41.575783
3507.352989	499302.488438	41.580788
3507.360103	499202.153784	41.585792
3507.526934	499120.063761	41.590797
3507.233079	499026.588195	41.595802
3507.048410	498939.858114	41.600807
3506.869126	498849.341357	41.605812
3507.131718	498761.581673	41.610816
3506.959868	498670.154171	41.615821
3506.658026	498584.802956	41.620826
3506.900584	498501.334944	41.625831
3506.962832	498416.380343	41.630836
3507.187471	498338.213803	41.635840
3506.947177	498250.176009	41.640845
3506.564309	498164.582595	41.645850
3507.043282	498073.352941	41.650855
3506.820511	497996.516048	41.655860
3506.660236	497904.627715	41.660864
3507.054447	497826.734915	41.665869
3506.859853	497749.387602	41.670874
3506.938567	497656.804360	41.675879
3506.568874	497578.019616	41.680884
3506.593797	497491.803601	41.685888
3506.318386	497420.776593	41.690893
3505.995884	497334.866103	41.695898
3506.316569	497257.436023	41.700903
3505.910409	497193.999734	41.705908
3506.426678	497103.212563	41.710912
3506.168772	497038.187748	41.715917
3506.185926	496970.999791	41.720922
3505.897472	496899.013228	41.725927
3506.124737	496827.804187	41.730932
3506.344817	496759.624611	41.735936
3506.168577	496688.326254	41.740941
3505.857789	496597.311329	41.745946
3506.056685	496521.764060	41.750951
3505.986042	496460.897316	41.755956
3505.577498	496394.378732	41.760960
3505.602673	496316.383957	41.765965
3505.284532	496254.040486	41.770970
3505.673663	496185.428120	41.775975
3505.668651	496125.054583	41.780980
3505.830058	496044.210278	41.785984
3505.683387	495985.322153	41.790989
3505.440215	495917.008863	41.795994
3505.611686	495851.811052	41.800999
3505.428839	495797.218715	41.806004
3505.659312	495725.700989	41.811008
3505.514301	495668.729653	41.816013
3505.341208	495611.207164	41.821018
3505.700114	495534.115502	41.826023
3505.754533	495478.778319	41.831028
3505.953013	495402.316727	41.836032
3505.765321	495332.982459	41.841037
3505.509776	495264.112775	41.846042
3505.664503	495191.392667	41.851047
3505.191480	495150.877513	41.856052
3505.558038	495068.077592	41.861056
3505.646890	495014.550745	41.866061
3505.390660	494949.667953	41.871066
3505.304401	494880.770151	41.876071
3505.106058	494826.631019	41.881076
3505.061942	494748.487338	41.886080
3504.958035	494699.179606	41.891085
3505.366005	494636.514410	41.896090
3505.354476	494576.085109	41.901095
3504.749473	494524.683897	41.906100
3505.071664	494464.303184	41.911104
3504.650835	494410.146674	41.916109
3504.806279	494358.677040	41.921114
3505.205897	494303.988582	41.926119
3504.879464	494252.997462	41.931124
3504.885183	494189.484224	41.936128
3505.460356	494144.915727	41.941133
3505.024026	494087.731236	41.946138
3505.031206	494017.805160	41.951143
3505.070524	493963.878350	41.956148
3505.139637	493897.476210	41.961152
3504.974859	493848.629530	41.966157
3505.313958	493793.696184	41.971162
3505.267816	493730.946391	41.976167
3504.797871	493677.299748	41.981172
3505.186183	493614.683815	41.986176
3504.885941	493555.809979	41.991181
3505.132354	493499.526773	41.996186
3505.080634	493435.716335	42.001191
3504.893239	493385.861875	42.006196
3504.820579	493331.647274	42.011200
3504.651963	493280.880726	42.016205
3504.887050	493229.798734	42.021210
3504.704552	493170.147705	42.026215
3504.718652	493120.412477	42.031220
3505.199917	493066.464153	42.036224
3504.827913	493019.363696	42.041229
3504.821057	492955.695706	42.046234
3505.112709	492901.422857	42.051239
3504.856352	492842.034473	42.056244
3504.779735	492780.901168	42.061248
3504.678208	492736.433790	42.066253
3504.598469	492682.419910	42.071258
3504.983964	492629.797712	42.076263
3504.523275	492577.710945	42.081268
3504.731929	492523.651616	42.086272
3504.748455	492478.660179	42.091277
3504.533211	492425.171387	42.096282
3504.949830	492380.975776	42.101287
3504.915935	492327.761375	42.106292
3504.852865	492259.605290	42.111296
3504.774701	492212.911017	42.116301
3504.569496	492156.794043	42.121306
3504.828033	492101.564080	42.126311
3504.787214	492055.216964	42.131316
3504.750031	492001.597968	42.136320
3504.654457	491944.352268	42.141325
3504.742593	491890.511398	42.146330
3504.752862	491839.712141	42.151335
3504.704555	491790.891131	42.156340
3504.935896	491727.231368	42.161344
3505.009347	491685.308906	42.166349
3504.823953	491634.943369	42.171354
3504.919419	491567.314931	42.176359
3504.917684	491520.455131	42.181364
3504.940514	491458.493044	42.186368
3504.713210	491408.183767	42.191373
3504.629067	491355.125238	42.196378
3504.824947	491304.800260	42.201383
3504.758647	491243.103642	42.206388
3504.498953	491195.626517	42.211392
3504.789554	491138.216669	42.216397
3504.775112	491094.084368	42.221402
3505.018842	491038.802324	42.226407
3504.537180	490998.125779	42.231412
3504.318731	490941.450867	42.236416
3504.519690	490884.457988	42.241421
3504.497196	490844.214556	42.246426
3504.934082	490792.638415	42.251431
3504.478889	490743.523847	42.256436
3504.277038	490685.936423	42.261440
3504.520151	490649.337542	42.266445
3504.343374	490594.826294	42.271450
3504.340387	490529.531485	42.276455
3504.515634	490501.275170	42.281460
3504.696823	490462.009011	42.286464
3504.523959	490405.779494	42.291469
3504.095868	490356.558452	42.296474
3504.063707	490307.730138	42.301479
3503.774953	490274.748111	42.306484
3503.965308	490217.148372	42.311488
3504.069343	490186.478541	42.316493
3503.720747	490144.920487	42.321498
3504.164000	490093.694481	42.326503
3504.148278	490059.103979	42.331508
3503.863786	490016.727586	42.336512
3504.024886	489978.372318	42.341517
3503.688140	489935.801827	42.346522
3503.929076	489880.869501	42.351527
3504.190059	489845.174924	42.356532
3503.785091	489808.169850	42.361536
3504.024728	489773.286451	42.366541
3503.927297	489736.334348	42.371546
3503.606094	489686.235965	42.376551
3503.359953	489660.518255	42.381556
3504.000106	489615.976774	42.386560
3503.724068	489581.122677	42.391565
3503.728175	489545.265361	42.396570
3504.218305	489498.878292	42.401575
3503.906606	489455.949039	42.406580
3503.992357	489405.129865	42.411584
3503.846529	489375.103313	42.416589
3503.783416	489332.337040	42.421594
3503.957884	489293.422429	42.426599
3503.802518	489251.932867	42.431604
3503.887930	489219.243845	42.436608
3504.228857	489183.333262	42.441613
3503.857349	489142.230561	42.446618
3503.986058	489097.110602	42.451623
3503.578061	489056.568891	42.456628
3503.843158	489018.750566	42.461632
3503.784021	488972.396864	42.466637
3503.435774	488944.976683	42.471642
3503.642644	488901.460124	42.476647
3503.557182	488878.089802	42.481652
3503.692957	488827.563946	42.486656
3503.841536	488802.035884	42.491661
3503.682420	488766.303142	42.496666
3503.880431	488722.181390	42.501671
3503.664684	488684.538072	42.506676
3503.760812	488640.886487	42.511680
3503.915878	488605.003466	42.516685
3503.654402	488568.074054	42.521690
3503.878404	488526.068930	42.526695
3503.589927	488495.153735	42.531700
3504.011081	488459.329977	42.536704
3503.662551	488415.898461	42.541709
3503.569189	488380.407114	42.546714
3503.689538	488348.518891	42.551719
3503.749898	488315.326766	42.556724
3504.008757	488270.790190	42.561728
3503.817803	488233.293420	42.566733
3503.771749	488195.672996	42.571738
3504.149900	488151.622579	42.576743
3503.782754	488122.739155	42.581748
3503.634263	488080.588742	42.586752
3503.635493	488034.778379	42.591757
3503.539864	488001.205787	42.596762
3503.914394	487969.630773	42.601767
3503.782599	487922.881129	42.606772
3503.668077	487882.593674	42.611776
3503.865994	487845.641536	42.616781
3503.652756	487813.450551	42.621786
3503.378217	487772.985676	42.626791
3503.551052	487747.805638	42.631796
3503.329299	487709.958818	42.636800
3503.767305	487676.201456	42.641805
3503.701739	487647.068168	42.646810
3503.848302	487613.356020	42.651815
3503.664086	487571.108745	42.656820
3503.712380	487534.128630	42.661824
3503.817916	487495.220167	42.666829
3503.652789	487452.312974	42.671834
3503.872597	487415.204864	42.676839
3503.705691	487377.601235	42.681844
3503.679492	487338.662365	42.686848
3503.725377	487302.136653	42.691853
3503.515667	487268.125617	42.696858
3503.716753	487232.686808	42.701863
3503.720046	487203.693493	42.706868
3503.523249	487154.325087	42.711872
3503.611419	487119.610734	42.716877
3503.555013	487086.989733	42.721882
3504.133920	487050.633031	42.726887
3504.000185	487020.852522	42.731892
3503.678938	486980.443332	42.736896
3503.839874	486937.180893	42.741901
3503.543446	486896.868643	42.746906
3503.532042	486856.259377	42.751911
3503.566204	486826.603899	42.756916
3503.689329	486785.670443	42.761920
3503.394408	486747.580075	42.766925
3503.509331	486714.325482	42.771930
3503.496148	486679.019763	42.776935
3503.634531	486645.963419	42.781940
3503.410341	486601.648702	42.786945
3503.413908	486584.322483	42.791949
3503.555737	486542.627787	42.796954
3503.886728	486512.622438	42.801959
3503.868739	486476.458291	42.806964
3503.471733	486448.839169	42.811969
3503.383899	486411.018818	42.816973
3503.604003	486382.040727	42.821978
3503.901719	486337.441982	42.826983
3503.707005	486307.467528	42.831988
3503.662508	486268.478280	42.836993
3503.815460	486228.094347	42.841997
3503.339188	486188.869006	42.847002
3503.402839	486156.075808	42.852007
3503.559511	486128.319438	42.857012
3503.689312	486084.503797	42.862017
3503.523429	486049.220396	42.867021
3503.744932	486021.807344	42.872026
3504.042951	485976.601340	42.877031
3503.412374	485942.349776	42.882036
3503.539150	485911.566808	42.887041
3503.578706	485872.866567	42.892045
3503.315457	485831.637099	42.897050
3503.549318	485799.574376	42.902055
3503.536042	485774.925220	42.907060
3503.214493	485741.231298	42.912065
3503.680286	485703.373574	42.917069
3503.633645	485681.760367	42.922074
3503.916748	485635.848474	42.927079
3503.780124	485603.994544	42.932084
3503.902766	485566.644523	42.937089
3503.938236	485514.304810	42.942093
3503.558033	485488.853527	42.947098
3503.787293	485449.415483	42.952103
3503.881928	485417.474665	42.957108
3503.975657	485362.043891	42.962113
3504.103140	485329.845200	42.967117
3503.855565	485287.803578	42.972122
3503.931844	485245.458864	42.977127
3503.336837	485210.745488	42.982132
3503.635616	485177.105355	42.987137
3503.611796	485136.897627	42.992141
3503.423647	485106.010510	42.997146
3503.567645	485072.192166	43.002151
3503.058225	485033.827837	43.007156
3502.893358	485013.090886	43.012161
3503.238537	484973.027381	43.017165
3503.183520	484962.932460	43.022170
3503.206843	484928.778958	43.027175
3503.085017	484898.739907	43.032180
3503.130827	484858.874245	43.037185
3503.346231	484835.804578	43.042189
3503.261671	484812.377410	43.047194
3503.407313	484769.161793	43.052199
3502.796560	484748.493873	43.057204
3503.175405	484710.899846	43.062209
3503.103431	484682.368168	43.067213
3503.161874	484662.606367	43.072218
3503.132489	484629.167666	43.077223
3503.034258	484593.819895	43.082228
3503.202768	484566.816663	43.087233
3503.160372	484536.714030	43.092237
3503.150856	484516.760543	43.097242
3503.844173	484483.663739	43.102247
3503.373117	484457.568146	43.107252
3502.905541	484423.641479	43.112257
3503.735808	484391.483034	43.117261
3502.996022	484361.892740	43.122266
3503.153426	484329.182119	43.127271
3503.344104	484301.467701	43.132276
3503.195041	484273.553503	43.137281
3503.460533	484246.282023	43.142285
3503.201310	484217.071349	43.147290
3503.443540	484178.739493	43.152295
3503.082131	484141.006679	43.157300
3503.357690	484124.140579	43.162305
3503.460109	484080.121446	43.167309
3503.340223	484068.015219	43.172314
3503.588600	484031.349219	43.177319
3503.249227	483982.700143	43.182324
3503.298273	483949.449857	43.187329
3503.230613	483921.017149	43.192333
3503.072068	483898.105323	43.197338
3503.490248	483869.091707	43.202343
3502.981294	483834.159767	43.207348
3503.257747	483810.270739	43.212353
3503.337634	483772.923050	43.217357
3503.291576	483750.145066	43.222362
3503.437097	483723.750205	43.227367
3503.234697	483691.700491	43.232372
3503.207761	483659.471842	43.237377
3503.429435	483630.842015	43.242381
3503.006771	483606.556246	43.247386
3503.326016	483567.756204	43.252391
3503.545225	483542.309489	43.257396
3503.371038	483507.930987	43.262401
3503.327231	483474.542568	43.267405
3503.783284	483441.328906	43.272410
3503.658691	483401.991248	43.277415
3503.504419	483364.426405	43.282420
3503.132706	483328.107857	43.287425
3503.431674	483301.941018	43.292429
3503.039292	483277.296361	43.297434
3503.753661	483238.737153	43.302439
3503.745966	483205.544631	43.307444
3503.597669	483167.372105	43.312449
3503.374972	483122.693529	43.317453
3503.299433	483103.910545	43.322458
3503.243025	483070.422174	43.327463
3503.695178	483040.643877	43.332468
3503.108970	483014.513253	43.337473
3503.442468	482976.871573	43.342477
3503.092693	482956.009077	43.347482
3503.150686	482908.355813	43.352487
3503.110049	482889.567139	43.357492
3503.321668	482858.360721	43.362497
3503.216026	482829.982456	43.367501
3503.195085	482809.321216	43.372506
3503.172963	482756.122254	43.377511
3503.505222	482743.641489	43.382516
3503.431922	482702.929918	43.387521
3503.144633	482661.796815	43.392525
3503.068325	482636.697760	43.397530
3503.486290	482596.768392	43.402535
3503.394246	482574.349522	43.407540
3503.531748	482543.052958	43.412545
3503.771412	482504.616337	43.417549
3503.528696	482479.037669	43.422554
3503.348459	482445.415651	43.427559
3503.423022	482416.099129	43.432564
3503.140568	482382.745511	43.437569
3503.277419	482353.621284	43.442573
3503.145033	482328.126252	43.447578
3503.359661	482294.391936	43.452583
3503.021210	482270.949925	43.457588
3503.135694	482236.826859	43.462593
3503.411059	482211.621871	43.467597
3503.175814	482179.826793	43.472602
3503.203080	482147.384482	43.477607
3503.375649	482117.496357	43.482612
3503.265997	482084.923642	43.487617
3503.436523	482053.014637	43.492621
3502.860196	482016.724876	43.497626
3503.144466	481985.050669	43.502631
3503.174939	481968.877237	43.507636
3503.382090	481940.499211	43.512641
3503.254968	481908.838340	43.517645
3503.174171	481880.505014	43.522650
3503.562034	481844.064812	43.527655
3503.136891	481823.869390	43.532660
3502.973524	481787.919058	43.537665
3503.559866	481750.639310	43.542669
3503.242571	481725.020486	43.547674
3503.545044	481690.968034	43.552679
3503.310332	481661.597173	43.557684
3503.253372	481632.703879	43.562689
3503.117636	481595.586654	43.567693
3503.282378	481565.648168	43.572698
3503.245933	481531.496526	43.577703
3503.321528	481502.733951	43.582708
3503.601202	481470.655192	43.587713
3503.349549	481437.648469	43.592717
3503.552206	481412.150338	43.597722
3503.407852	481375.690813	43.602727
3503.235698	481341.610404	43.607732
3503.245115	481310.836606	43.612737
3503.257367	481281.376072	43.617741
3503.407469	481246.689486	43.622746
3503.596242	481224.528164	43.627751
3503.280683	481177.988888	43.632756
3503.095794	481156.289854	43.637761
3503.213131	481122.568161	43.642765
3502.938341	481097.446997	43.647770
3503.043292	481078.027134	43.652775
3503.206132	481051.018711	43.657780
3503.350879	481030.531462	43.662785
3503.265297	480990.827961	43.667789
3503.158358	480957.191344	43.672794
3502.920299	480919.684201	43.677799
3502.648621	480908.407635	43.682804
3502.796233	480876.954584	43.687809
3502.971087	480850.348193	43.692813
3502.822059	480832.837191	43.697818
3502.766053	480814.250545	43.702823
3503.119111	480783.725426	43.707828
3503.116342	480759.875199	43.712833
3502.769177	480727.690346	43.717837
3502.860317	480704.482328	43.722842
3503.170739	480672.851941	43.727847
3503.280565	480640.191543	43.732852
3503.168719	480615.499036	43.737857
3503.212954	480590.125290	43.742861
3503.093249	480568.061579	43.747866
3503.109650	480540.771878	43.752871
3503.059015	480513.189371	43.757876
3503.033672	480487.371499	43.762881
3503.196290	480445.101397	43.767885
3502.788472	480431.268534	43.772890
3503.202388	480385.472446	43.777895
3502.932937	480363.633880	43.782900
3502.911012	480344.940311	43.787905
3503.045156	480310.759474	43.792909
3503.077775	480296.403161	43.797914
3503.184101	480282.085898	43.802919
3503.113272	480245.157517	43.807924
3502.837144	480209.625385	43.812929
3503.191616	480172.782252	43.817933
3502.838032	480149.945821	43.822938
3503.130954	480121.904903	43.827943
3503.292719	480091.812480	43.832948
3503.177415	480067.928186	43.837953
3503.390021	480034.745208	43.842957
3503.119748	479999.717027	43.847962
3503.393752	479984.211130	43.852967
3503.472640	479949.734908	43.857972
3503.231951	479910.507625	43.862977
3503.248960	479885.490720	43.867981
3502.853699	479856.141470	43.872986
3503.080323	479823.713878	43.877991
3503.164235	479798.383220	43.882996
3502.959513	479777.089645	43.888001
3502.874189	479743.851350	43.893005
3503.077664	479724.566094	43.898010
3503.197568	479687.455126	43.903015
3503.266911	479659.852457	43.908020
3502.612327	479641.357574	43.913025
3502.847865	479619.894208	43.918029
3503.113344	479603.984987	43.923034
3503.061176	479567.254257	43.928039
3503.242853	479540.088714	43.933044
3502.950806	479519.819082	43.938049
3503.092272	479486.696560	43.943053
3502.682522	479461.897000	43.948058
3502.755280	479434.445013	43.953063
3502.955779	479418.495182	43.958068
3502.992238	479392.969117	43.963073
3503.160243	479363.480765	43.968077
3503.233867	479335.169366	43.973082
3503.230719	479308.588079	43.978087
3503.845012	479265.132750	43.983092
3503.305134	479238.837012	43.988097
3503.375932	479196.982151	43.993101
3503.026765	479181.016544	43.998106
3503.097649	479146.843036	44.003111
3503.065086	479119.760647	44.008116
3502.907442	479089.817097	44.013121
3503.121522	479058.046865	44.018125
3502.680907	479040.882469	44.023130
3503.194336	479013.310642	44.028135
3502.953953	478990.050625	44.033140
3502.830536	478962.325126	44.038145
3502.858372	478940.084572	44.043149
3502.669896	478922.072219	44.048154
3502.991838	478886.595658	44.053159
3502.991831	478858.092716	44.058164
3502.915476	478846.177832	44.063169
3503.449338	478812.639081	44.068173
3503.405800	478786.568578	44.073178
3503.036241	478752.058458	44.078183
3503.387373	478724.511387	44.083188
3502.870843	478703.871340	44.088193
3503.186573	478661.623189	44.093197
3503.344641	478634.560845	44.098202
3502.649638	478606.165601	44.103207
3503.207931	478572.622542	44.108212
3502.876608	478554.126619	44.113217
3503.305858	478523.029370	44.118221
3502.994117	478504.631418	44.123226
3503.099793	478462.819733	44.128231
3503.243352	478441.217472	44.133236
3503.218826	478427.727514	44.138241
3503.212290	478387.853559	44.143245
3502.997084	478361.354223	44.148250
3503.242485	478321.036586	44.153255
3503.301379	478296.010656	44.158260
3502.798565	478276.732471	44.163265
3502.964365	478247.292929	44.168269
3503.373226	478221.201640	44.173274
3503.106426	478196.681088	44.178279
3503.064923	478168.284446	44.183284
3503.006772	478140.901133	44.188289
3503.111164	478112.127910	44.193293
3503.346921	478082.373940	44.198298
3503.454165	478054.004486	44.203303
3503.148592	478026.760559	44.208308
3503.312028	478000.302780	44.213313
3503.291645	477958.458846	44.218317
3503.401640	477930.695226	44.223322
3503.431376	477898.547044	44.228327
3503.553406	477860.673373	44.233332
3503.197623	477835.256384	44.238337
3502.951369	477799.309873	44.243341
3503.453070	477775.123949	44.248346
3503.113523	477745.155630	44.253351
3502.900013	477718.756041	44.258356
3502.776433	477689.613205	44.263361
3503.131455	477650.793042	44.268365
3503.115182	477642.607943	44.273370
3503.090690	477616.835806	44.278375
3503.264340	477580.419130	44.283380
3503.018313	477557.107352	44.288385
3502.876842	477520.992283	44.293389
3502.720675	477495.948021	44.298394
3502.557877	477472.825334	44.303399
3502.672198	477450.367073	44.308404
3502.600497	477436.125490	44.313409
3502.881087	477399.590677	44.318413
3502.830896	477385.952205	44.323418
3502.449970	477361.094332	44.328423
3503.015135	477343.468335	44.333428
3502.844557	477316.707605	44.338433
3502.850973	477295.428386	44.343437
3502.842223	477264.346301	44.348442
3503.101964	477239.843424	44.353447
3503.038723	477207.809404	44.358452
3503.117383	477183.385162	44.363457
3502.894291	477149.101484	44.368461
3502.974748	477128.063234	44.373466
3502.841420	477102.711545	44.378471
3502.929697	477077.375874	44.383476
3502.491084	477063.191055	44.388481
3502.999170	477038.447052	44.393485
3502.700808	477014.232850	44.398490
3502.518313	476986.007672	44.403495
3502.623301	476961.275734	44.408500
3502.544494	476950.775023	44.413505
3502.892668	476925.651385	44.418509
3502.963656	476914.824080	44.423514
3502.332227	476879.693586	44.428519
3502.775746	476865.421863	44.433524
3502.700889	476847.894917	44.438529
3502.734583	476813.065124	44.443533
3502.588409	476792.466049	44.448538
3502.816714	476771.505410	44.453543
3503.266180	476742.726568	44.458548
3502.739415	476732.093245	44.463553
3502.832896	476689.369020	44.468557
3502.779728	476679.066317	44.473562
3502.563419	476652.159958	44.478567
3502.763752	476631.304578	44.483572
3502.465170	476608.403946	44.488577
3502.764805	476592.233685	44.493581
3503.262707	476554.702785	44.498586
3502.764592	476528.648783	44.503591
3502.954429	476507.845421	44.508596
3502.677446	476483.627087	44.513601
3502.742829	476461.326688	44.518605
3502.973606	476438.040168	44.523610
3503.140782	476417.189670	44.528615
3503.034728	476380.914880	44.533620
3503.013786	476362.873562	44.538625
3502.849593	476328.578960	44.543629
3502.993368	476308.287959	44.548634
3502.922207	476280.751846	44.553639
3503.011996	476258.497913	44.558644
3502.891380	476237.388692	44.563649
3502.981717	476209.675689	44.568653
3503.078513	476187.370021	44.573658
3502.886369	476159.245978	44.578663
3503.087859	476118.626346	44.583668
3502.979075	476104.389349	44.588673
3502.980273	476078.711828	44.593677
3502.787930	476057.967355	44.598682
3502.924401	476035.705848	44.603687
3503.037647	476006.674730	44.608692
3502.903378	475982.332338	44.613697
3502.729228	475947.886833	44.618701
3502.842570	475924.769483	44.623706
3502.890423	475912.226521	44.628711
3503.002022	475876.017813	44.633716
3503.034403	475863.881594	44.638721
3503.015711	475821.273607	44.643725
3502.828836	475797.444588	44.648730
3502.724743	475779.061726	44.653735
3502.913470	475747.389952	44.658740
3502.882588	475728.287979	44.663745
3503.053667	475690.907015	44.668749
3502.966930	475673.582823	44.673754
3502.853363	475651.460788	44.678759
3503.110033	475631.353554	44.683764
3502.988322	475608.070136	44.688769
3503.121570	475566.954256	44.693773
3502.825488	475548.651553	44.698778
3502.697074	475521.325238	44.703783
3503.187920	475504.012079	44.708788
3502.645979	475485.343180	44.713793
3503.000852	475450.308807	44.718797
3502.874565	475432.687221	44.723802
3502.683378	475405.269381	44.728807
3502.795910	475380.281094	44.733812
3502.607581	475354.126426	44.738817
3502.779209	475334.840829	44.743821
3502.787085	475309.767622	44.748826
3502.640534	475293.412748	44.753831
3502.847371	475263.910789	44.758836
3502.487354	475247.841830	44.763841
3502.933370	475211.124649	44.768845
3502.967057	475188.524125	44.773850
3503.007187	475166.124761	44.778855
3503.184485	475139.862301	44.783860
3502.922045	475110.989127	44.788865
3503.023715	475085.041641	44.793869
3502.841274	475063.687753	44.798874
3502.511410	475044.024903	44.803879
3502.958926	475012.159766	44.808884
3503.012204	474997.492173	44.813889
3502.859983	474964.557632	44.818893
3502.553492	474937.409685	44.823898
3502.812729	474917.402261	44.828903
3502.820642	474887.020675	44.833908
3502.668671	474863.184841	44.838913
3502.807537	474855.328027	44.843917
3502.887094	474843.941947	44.848922
3502.651463	474813.800320	44.853927
3502.889770	474788.538795	44.858932
3502.613827	474765.733110	44.863937
3502.761040	474738.564776	44.868941
3502.549949	474712.564259	44.873946
3502.773781	474700.549023	44.878951
3502.966670	474672.766867	44.883956
3502.808611	474651.509739	44.888961
3502.807823	474617.590465	44.893965
3502.708890	474599.357104	44.898970
3502.277481	474576.878648	44.903975
3502.551867	474554.492533	44.908980
3502.454415	474542.021667	44.913985
3502.793294	474519.777121	44.918989
3502.821715	474499.855650	44.923994
3502.809176	474476.351404	44.928999
3502.743276	474445.272758	44.934004
3502.619850	474432.401440	44.939009
3502.370512	474401.755665	44.944013
3502.724868	474396.544314	44.949018
3502.281521	474373.511368	44.954023
3502.696171	474342.812708	44.959028
3502.933656	474337.518421	44.964033
3502.567799	474306.081772	44.969037
3502.966211	474293.028036	44.974042
3502.611586	474267.049137	44.979047
3502.902955	474243.851123	44.984052
3502.812208	474218.842120	44.989057
3502.821533	474191.744877	44.994061
3503.024169	474173.261899	44.999066
3502.489299	474149.181283	45.004071
3502.978213	474127.873341	45.009076
3503.079047	474116.685647	45.014081
3502.978498	474085.106179	45.019085
3503.041088	474063.156762	45.024090
3502.793412	474031.802294	45.029095
3503.046598	474009.064858	45.034100
3502.785260	473979.734515	45.039105
3502.649127	473949.525240	45.044109
3502.819981	473923.059596	45.049114
3502.416838	473908.613699	45.054119
3502.829915	473880.189285	45.059124
3502.659376	473861.207941	45.064129
3502.394670	473841.230166	45.069133
3502.526915	473830.037386	45.074138
3503.041263	473795.379036	45.079143
3503.073218	473771.007439	45.084148
3502.745702	473752.758140	45.089153
3502.858139	473721.852566	45.094157
3502.960045	473703.283622	45.099162
3502.793854	473675.606186	45.104167
3502.543267	473652.693876	45.109172
3502.609620	473632.815989	45.114177
3502.817456	473603.058078	45.119181
3502.816895	473585.263250	45.124186
3502.315758	473559.154351	45.129191
3503.129260	473530.818677	45.134196
3502.727679	473515.866646	45.139201
3502.608662	473485.451625	45.144205
3503.123344	473471.064729	45.149210
3502.528149	473444.616403	45.154215
3502.564577	473431.365533	45.159220
3502.633742	473406.734826	45.164225
3502.544014	473380.561619	45.169229
3502.773678	473356.006968	45.174234
3502.527640	473344.063846	45.179239
3502.652978	473322.255326	45.184244
3502.493643	473298.317222	45.189249
3502.412050	473289.027869	45.194253
3502.385531	473262.945746	45.199258
3502.361488	473248.490821	45.204263
3502.593386	473234.299385	45.209268
3502.378380	473216.133083	45.214273
3502.421693	473200.454314	45.219277
3502.487855	473175.722614	45.224282
3502.404896	473162.186772	45.229287
3503.031970	473139.389938	45.234292
3502.398719	473116.637528	45.239297
3502.705840	473102.939825	45.244301
3502.609593	473073.228264	45.249306
3502.652617	473063.363280	45.254311
3502.791686	473031.542251	45.259316
3502.748489	473009.152870	45.264321
3502.438906	472993.427706	45.269325
3503.043982	472966.640155	45.274330
3502.596401	472943.353052	45.279335
3502.689789	472914.774475	45.284340
3502.403493	472900.461162	45.289345
3502.760576	472879.323769	45.294349
3502.722800	472867.904004	45.299354
3502.551343	472839.417064	45.304359
3502.371036	472818.160992	45.309364
3502.634184	472813.013886	45.314369
3502.632126	472773.782547	45.319373
3502.302316	472754.015789	45.324378
3502.272177	472737.791884	45.329383
3502.217714	472722.228982	45.334388
3501.996346	472724.639607	45.339393
3502.455061	472704.396189	45.344397
3502.703182	472680.444327	45.349402
3502.184262	472657.622924	45.354407
3502.228809	472642.095096	45.359412
3502.447011	472625.630207	45.364417
3502.798696	472610.054554	45.369421
3502.856375	472593.564055	45.374426
3502.617499	472571.659535	45.379431
3502.326669	472551.583123	45.384436
3502.259542	472534.303073	45.389441
3502.256246	472501.037005	45.394445
3502.606902	472495.370610	45.399450
3502.041940	472472.151654	45.404455
3502.544353	472457.866890	45.409460
3502.428794	472443.223261	45.414465
3502.308421	472419.884489	45.419469
3502.642712	472412.046642	45.424474
3502.825603	472399.024927	45.429479
3502.676984	472370.230267	45.434484
3502.520972	472357.969064	45.439489
3502.624179	472331.561915	45.444493
3502.649111	472308.149814	45.449498
3502.574307	472287.028304	45.454503
3502.354950	472263.603595	45.459508
3502.444958	472249.635614	45.464513
3502.421515	472233.106817	45.469517
3502.711390	472198.935025	45.474522
3502.568682	472191.474649	45.479527
3502.576478	472165.688776	45.484532
3502.641271	472149.803421	45.489537
3502.831881	472132.685071	45.494541
3502.804926	472099.624100	45.499546
3502.533041	472087.026815	45.504551
3502.717258	472066.117504	45.509556
3502.901462	472043.489175	45.514561
3502.767684	472019.039626	45.519565
3502.650503	471990.188844	45.524570
3502.457907	471976.062371	45.529575
3502.505537	471947.388102	45.534580
3502.677804	471927.693887	45.539585
3502.501481	471910.682963	45.544589
3502.520887	471886.108259	45.549594
3502.741021	471880.613641	45.554599
3502.504648	471850.213827	45.559604
3502.605955	471837.204360	45.564609
3502.424467	471815.694367	45.569613
3502.575368	471790.745142	45.574618
3502.205417	471777.101130	45.579623
3502.826981	471745.253069	45.584628
3502.536730	471740.596219	45.589633
3502.152519	471714.466159	45.594637
3502.426464	471698.193901	45.599642
3502.530800	471685.234402	45.604647
3502.778901	471655.213872	45.609652
3502.780914	471641.865783	45.614657
3502.610274	471612.618174	45.619661
3502.333596	471590.414857	45.624666
3502.253533	471576.321087	45.629671
3502.484649	471567.184330	45.634676
3502.359344	471543.238351	45.639681
3502.474232	471524.007621	45.644685
3502.213642	471518.486568	45.649690
3502.331020	471492.530900	45.654695
3502.301130	471485.406566	45.659700
3502.309638	471475.647115	45.664705
3502.280560	471446.832224	45.669709
3502.697906	471433.419334	45.674714
3502.223716	471410.134176	45.679719
3502.422842	471389.069999	45.684724
3502.382729	471384.070758	45.689729
3502.876061	471360.028243	45.694733
3502.746742	471338.003896	45.699738
3502.794849	471321.463042	45.704743
3502.660041	471296.456402	45.709748
3502.660367	471283.866698	45.714753
3502.567450	471266.690441	45.719757
3503.078511	471235.111391	45.724762
3502.430157	471206.796934	45.729767
3502.818021	471193.894048	45.734772
3502.813136	471177.765786	45.739777
3502.507011	471147.274395	45.744781
3503.041507	471129.899240	45.749786
3502.629527	471110.446643	45.754791
3502.728594	471082.723523	45.759796
3502.689508	471060.836446	45.764801
3502.601297	471051.698533	45.769805
3502.757211	471017.595684	45.774810
3502.722270	470980.438188	45.779815
3502.957333	470902.333871	45.784820
3502.492529	470782.624072	45.789825
3502.390511	470623.114474	45.794829
3502.256258	470405.055714	45.799834
3501.594448	470152.388981	45.804839
3501.587301	469851.124368	45.809844
3500.832625	469498.898532	45.814849
3500.265610	469102.894997	45.819853
3500.118299	468652.707872	45.824858
3498.931310	468176.626511	45.829863
3498.830008	467644.025294	45.834868
3497.994706	467068.331216	45.839873
3497.416590	466448.525819	45.844877
3496.521817	465779.787510	45.849882
3495.051280	465078.690445	45.854887
3494.347735	464332.881997	45.859892
3493.382561	463547.625447	45.864897
3492.044959	462712.461161	45.869901
3491.272375	461841.299931	45.874906
3489.717018	460919.117879	45.879911
3488.907985	459958.621336	45.884916
3487.275152	458962.881937	45.889921
3485.658807	457933.331680	45.894925
3484.545708	456844.738797	45.899930
3482.938878	455752.612244	45.904935
3481.327591	454587.437763	45.909940
3479.408156	453409.631215	45.914945
3477.767132	452178.402693	45.919949
3476.601630	450919.983316	45.924954
3474.714810	449619.518535	45.929959
3472.720142	448295.788759	45.934964
3471.259569	446943.727607	45.939969
3468.838206	445546.244470	45.944973
3467.316613	444120.055168	45.949978
3465.204262	442670.804672	45.954983
3462.813833	441175.040262	45.959988
3461.065504	439661.682806	45.964993
3458.606796	438109.866403	45.969997
3456.364514	436539.601211	45.975002
3454.257120	434942.992674	45.980007
3451.985485	433310.353385	45.985012
3449.733529	431655.885930	45.990017
3447.332804	429975.456575	45.995021
3445.415675	428261.156466	46.000026
3442.729915	426539.580598	46.005031
3439.991169	424781.926080	46.010036
3438.139244	423000.256182	46.015041
3435.212127	421194.820709	46.020045
3432.882815	419365.151718	46.025050
3430.127343	417508.817605	46.030055
3427.779259	415643.635607	46.035060
3424.963380	413743.520325	46.040065
3422.349755	411830.576157	46.045069
3419.539990	409894.058751	46.050074
3416.612784	407950.997031	46.055079
3414.146353	405962.894473	46.060084
3411.074199	403973.391155	46.065089
3407.886952	401971.806769	46.070093
3405.419325	399941.110942	46.075098
3402.428557	397897.377305	46.080103
3399.621440	395830.901406	46.085108
3396.629332	393754.376643	46.090113
3393.401625	391659.180252	46.095117
3390.668176	389552.151729	46.100122
3387.197169	387433.812136	46.105127
3384.222890	385296.935949	46.110132
3381.257319	383137.559587	46.115137
3378.062665	380972.680042	46.120141
3375.503423	378799.522767	46.125146
3371.772797	376604.933883	46.130151
3368.374573	374398.709779	46.135156
3365.171438	372187.806491	46.140161
3361.822069	369967.909196	46.145165
3358.585892	367734.506622	46.150170
3355.100221	365494.667473	46.155175
3351.786969	363237.934651	46.160180
3348.724400	360977.737940	46.165185
3344.973710	358716.716102	46.170189
3341.901956	356433.386033	46.175194
3338.436371	354137.723941	46.180199
3335.036957	351842.393721	46.185204
3331.783611	349536.632809	46.190209
3327.882599	347233.836410	46.195213
3324.527619	344915.567387	46.200218
3320.813241	342599.002345	46.205223
3317.593317	340264.610115	46.210228
3313.788795	337926.544667	46.215233
3310.392002	335595.920160	46.220237
3306.987949	333247.754178	46.225242
3303.085772	330908.676767	46.230247
3299.337477	328547.889868	46.235252
3296.067520	326187.447647	46.240257
3292.331822	323840.219892	46.245261
3288.304229	321466.167065	46.250266
3284.763927	319111.979827	46.255271
3281.095624	316749.111292	46.260276
3277.966429	314380.818200	46.265281
3273.955569	312011.649885	46.270285
3270.017386	309634.157632	46.275290
3266.307177	307260.101951	46.280295
3262.359342	304882.331416	46.285300
3258.931864	302508.671484	46.290305
3255.189404	300127.446354	46.295309
3251.433329	297737.949669	46.300314
3247.332960	295368.209107	46.305319
3243.634407	292987.822831	46.310324
3240.141262	290611.486094	46.315329
3236.116660	288245.096047	46.320333
3232.598021	285856.571502	46.325338
3228.564390	283476.469994	46.330343
3224.337648	281111.772433	46.335348
3220.762612	278743.486008	46.340353
3216.634536	276380.534279	46.345357
3213.073595	274012.358217	46.350362
3209.168490	271645.518999	46.355367
3205.179972	269288.967905	46.360372
3201.284995	266920.629756	46.365377
3197.196164	264582.287784	46.370381
3193.125507	262236.582607	46.375386
3189.372471	259888.130489	46.380391
3185.753276	257543.915231	46.385396
3181.768070	255212.625647	46.390401
3177.800871	252877.779680	46.395405
3173.876215	250535.581848	46.400410
3169.680032	248207.247338	46.405415
3165.990979	245872.360780	46.410420
3162.291957	243561.974712	46.415425
3157.638481	241246.900407	46.420429
3153.748797	238935.201589	46.425434
3149.719649	236651.038909	46.430439
3145.639144	234354.034018	46.435444
3142.126602	232072.312885	46.440449
3137.832674	229797.785685	46.445453
3133.923488	227517.539361	46.450458
3129.327101	225264.293065	46.455463
3125.318787	223009.555061	46.460468
3121.173269	220760.470462	46.465473
3117.116674	218522.686390	46.470477
3113.165479	216298.928070	46.475482
3108.828620	214089.427229	46.480487
3104.363642	211875.299515	46.485492
3100.790545	209686.416037	46.490497
3096.257370	207501.266306	46.495501
3092.522429	205324.036014	46.500506
3088.209964	203156.673318	46.505511
3084.330776	201001.187785	46.510516
3080.187242	198846.331778	46.515521
3075.632786	196721.595210	46.520525
3071.510287	194592.188656	46.525530
3067.011854	192479.529678	46.530535
3062.892417	190387.143792	46.535540
3058.724998	188290.015880	46.540545
3053.917691	186236.367923	46.545549
3049.827133	184173.125782	46.550554
3045.189432	182149.785522	46.555559
3040.894960	180124.194818	46.560564
3036.153570	178120.845950	46.565569
3031.495228	176143.119649	46.570573
3027.164658	174169.641780	46.575578
3022.587330	172236.643998	46.580583
3018.385914	170304.667768	46.585588
3013.774546	168402.007259	46.590593
3008.971029	166518.533810	46.595597
3004.531418	164644.398055	46.600602
2999.218697	162814.287201	46.605607
2994.712610	160993.635716	46.610612
2989.870903	159198.162464	46.615617
2984.895298	157449.840748	46.620621
2979.986372	155710.252259	46.625626
2974.755190	154013.565111	46.630631
2969.405878	152350.811201	46.635636
2964.293758	150690.653429	46.640641
2958.381409	149042.250962	46.645645
2952.531575	147491.006932	46.650650
2945.889150	146005.998644	46.655655
2939.683423	144555.142884	46.660660
2933.357656	143156.961048	46.665665
2926.926034	141824.845086	46.670669
2920.902194	140534.154436	46.675674
2914.789771	139307.991979	46.680679
2909.291868	138120.098870	46.685684
2903.676386	136972.062316	46.690689
2898.144294	135875.832527	46.695693
2893.031772	134816.342228	46.700698
2888.064493	133792.690432	46.705703
2882.700528	132815.861232	46.710708
2878.020279	131866.411602	46.715713
2873.084560	130950.859102	46.720717
2868.733468	130055.587551	46.725722
2864.578099	129193.312776	46.730727
2860.308162	128351.730325	46.735732
2856.118489	127537.588282	46.740737
2851.724568	126745.307533	46.745741
2847.730242	125975.492522	46.750746
2844.138065	125215.168534	46.755751
2840.022512	124469.096005	46.760756
2835.856995	123737.086117	46.765761
2831.924410	123022.667954	46.770765
2828.314689	122319.785679	46.775770
2825.119081	121624.952644	46.780775
2821.064247	120939.078832	46.785780
2817.621560	120252.816657	46.790785
2813.844016	119588.911637	46.795789
2810.250281	118917.346742	46.800794
2806.482275	118270.300117	46.805799
2802.738783	117615.224023	46.810804
2799.422477	116976.712784	46.815809
2795.386298	116351.116639	46.820813
2791.658696	115716.849059	46.825818
2787.846027	115098.182019	46.830823
2784.048392	114487.838814	46.835828
2780.061287	113878.590628	46.840833
2775.901454	113289.977534	46.845837
2772.208334	112693.532762	46.850842
2768.429736	112123.951287	46.855847
2764.856215	111551.880405	46.860852
2760.964840	110994.400282	46.865857
2756.669816	110438.936956	46.870861
2753.315337	109881.899377	46.875866
2749.338860	109350.000134	46.880871
2745.562859	108811.759323	46.885876
2741.838435	108279.112546	46.890881
2738.284661	107760.647640	46.895885
2734.859792	107239.055878	46.900890
2731.419171	106717.817732	46.905895
2727.662586	106202.268238	46.910900
2724.472920	105691.062135	46.915905
2721.064484	105170.986772	46.920909
2717.789264	104656.504548	46.925914
2714.118883	104146.299201	46.930919
2710.597386	103628.604239	46.935924
2707.095509	103126.523491	46.940929
2703.601797	102613.454152	46.945933
2700.563860	102098.415257	46.950938
2696.450717	101596.236831	46.955943
2693.079900	101087.925906	46.960948
2690.369759	100566.466816	46.965953
2686.729045	100057.921653	46.970957
2683.576679	99542.991772	46.975962
2680.050194	99029.462842	46.980967
2676.542405	98509.940442	46.985972
2673.317827	97990.395129	46.990977
2669.575324	97475.908073	46.995981
2666.020235	96948.894881	47.000986
2663.081397	96430.550717	47.005991
2659.416786	95903.978732	47.010996
2655.758324	95383.489091	47.016001
2652.242580	94866.887235	47.021005
2648.742824	94340.150820	47.026010
2645.868539	93820.899648	47.031015
2642.600307	93295.936772	47.036020
2639.211565	92751.598120	47.041025
2635.791425	92227.630230	47.046029
2632.449063	91684.561382	47.051034
2628.876650	91143.240710	47.056039
2624.953583	90613.063995	47.061044
2621.902749	90063.867338	47.066049
2618.053604	89532.008359	47.071053
2614.916370	88978.715780	47.076058
2611.615939	88444.567413	47.081063
2607.875708	87908.883614	47.086068
2604.777842	87357.076307	47.091073
2601.155364	86814.495498	47.096077
2598.007919	86264.838127	47.101082
2594.500983	85715.424934	47.106087
2590.908617	85165.108077	47.111092
2587.696034	84601.962928	47.116097
2583.800841	84059.425312	47.121101
2580.781522	83496.309885	47.126106
2577.067952	82940.655780	47.131111
2573.792378	82378.974218	47.136116
2570.350782	81817.850425	47.141121
2566.736464	81256.815486	47.146125
2563.327070	80695.785268	47.151130
2560.083263	80139.630589	47.156135
2556.225652	79570.817826	47.161140
2552.906234	78999.481685	47.166145
2549.062899	78436.265707	47.171149
2545.847693	77865.940169	47.176154
2542.143684	77302.103428	47.181159
2538.725596	76738.538624	47.186164
2535.321827	76171.630555	47.191169
2531.886795	75598.376824	47.196173
2528.581742	75028.696171	47.201178
2524.761609	74466.511146	47.206183
2521.522241	73892.856929	47.211188
2518.573254	73317.404782	47.216193
2514.576938	72740.477326	47.221197
2511.339946	72156.790656	47.226202
2507.878618	71572.808968	47.231207
2503.902800	70996.995706	47.236212
2500.478903	70416.963678	47.241217
2497.003111	69842.793050	47.246221
2493.914202	69260.328632	47.251226
2490.201092	68688.137620	47.256231
2486.847051	68110.774331	47.261236
2483.533158	67526.124212	47.266241
2480.044215	66941.152863	47.271245
2476.416824	66346.885732	47.276250
2472.966808	65756.781402	47.281255
2469.161425	65182.137946	47.286260
2466.156913	64586.260128	47.291265
2462.703283	63998.564897	47.296269
2458.873203	63406.937270	47.301274
2455.485665	62817.901308	47.306279
2452.147935	62226.973972	47.311284
2448.607500	61624.294607	47.316289
2445.233259	61035.939908	47.321293
2441.851830	60443.868988	47.326298
2438.552741	59847.294050	47.331303
2434.946486	59252.735943	47.336308
2431.567322	58648.708618	47.341313
2427.884673	58064.953403	47.346317
2424.527086	57459.239177	47.351322
2420.990817	56850.167083	47.356327
2417.612918	56250.203347	47.361332
2413.958822	55644.162355	47.366337
2410.522361	55036.681751	47.371341
2407.190915	54443.513229	47.376346
2404.234289	53835.462186	47.381351
2399.973651	53219.687053	47.386356
2396.596853	52605.725414	47.391361
2393.022839	52000.812293	47.396365
2389.867804	51388.066162	47.401370
2386.458088	50771.373175	47.406375
2382.846025	50158.400828	47.411380
2379.172080	49550.960160	47.416385
2375.886980	48933.028359	47.421389
2372.233758	48311.739138	47.426394
2369.093380	47707.264457	47.431399
2365.223467	47087.780213	47.436404
2362.323608	46472.943946	47.441409
2358.356163	45854.574161	47.446413
2354.948129	45231.371618	47.451418
2351.519797	44617.245432	47.456423
2347.441731	43993.407972	47.461428
2344.704882	43367.013976	47.466433
2340.907989	42755.995943	47.471437
2337.532475	42128.239882	47.476442
2334.104671	41508.518226	47.481447
2330.512821	40893.620392	47.486452
2326.880714	40265.310808	47.491457
2323.451743	39638.357209	47.496461
2319.855917	39018.396345	47.501466
2316.190168	38394.945500	47.506471
2312.832678	37777.151381	47.511476
2309.466213	37151.857777	47.516481
2305.486115	36535.521238	47.521485
2302.424632	35916.897888	47.526490
2298.717978	35286.241187	47.531495
2294.842470	34655.369623	47.536500
2291.607870	34041.810134	47.541505
2288.184145	33421.313054	47.546509
2284.785821	32796.951381	47.551514
2281.403769	32177.448021	47.556519
2277.671697	31547.351000	47.561524
2274.444803	30921.168132	47.566529
2271.031472	30305.673719	47.571533
2267.258814	29678.738810	47.576538
2263.623025	29056.871317	47.581543
2260.087242	28434.481139	47.586548
2256.531094	27801.391446	47.591553
2252.955959	27189.950685	47.596557
2249.459734	26567.294502	47.601562
2245.999641	25950.943544	47.606567
2242.244258	25339.466279	47.611572
2238.968852	24711.060951	47.616577
2235.137275	24087.177680	47.621581
2231.904991	23468.979373	47.626586
2228.280320	22857.500467	47.631591
2224.482805	22246.966818	47.636596
2220.973136	21625.878896	47.641601
2217.330577	21018.551713	47.646605
2213.584441	20402.334325	47.651610
2210.209982	19803.687262	47.656615
2206.323027	19202.097973	47.661620
2202.978712	18590.657166	47.666625
2198.907087	17999.147360	47.671629
2195.091829	17402.802351	47.676634
2190.659623	16830.587022	47.681639
2185.990751	16275.331349	47.686644
2182.000967	15718.849286	47.691649
2177.812389	15184.999532	47.696653
2173.741965	14643.737343	47.701658
2169.563009	14104.875658	47.706663
2165.364691	13601.890788	47.711668
2161.552092	13090.406112	47.716673
2157.529592	12599.102860	47.721677
2153.646573	12117.468503	47.726682
2149.824315	11643.536009	47.731687
2145.814624	11182.987779	47.736692
2142.446586	10716.928394	47.741697
2138.650520	10261.228697	47.746701
2134.787137	9817.756391	47.751706
2131.306708	9376.798954	47.756711
2127.129140	8935.355901	47.761716
2123.593446	8493.484780	47.766721
2120.178358	8075.989405	47.771725
2116.488803	7662.360044	47.776730
2112.487829	7240.353790	47.781735
2108.234302	6840.370377	47.786740
2104.424511	6448.137411	47.791745
2099.863873	6085.541112	47.796749
2095.349132	5728.786902	47.801754
2091.611504	5381.086691	47.806759
2087.241732	5049.982145	47.811764
2083.194095	4715.159470	47.816769
2079.310737	4403.509816	47.821773
2075.104086	4100.431286	47.826778
2071.191222	3804.821154	47.831783
2067.388287	3530.219324	47.836788
2063.479264	3247.148432	47.841793
2059.732280	2983.890126	47.846797
2055.905224	2725.071652	47.851802
2052.545381	2466.177860	47.856807
2048.413671	2226.047589	47.861812
2044.953165	1974.802011	47.866817
2041.338044	1735.521812	47.871821
2037.552249	1503.978792	47.876826
2034.229100	1282.703316	47.881831
2030.559477	1058.023209	47.886836
2027.220326	836.955070	47.891841
2023.410648	629.478700	47.896845
2019.289737	425.232782	47.901850
2015.514137	217.423718	47.906855
2010.209441	62.492814	47.911860
1998.616970	92.488872	47.916865
1990.521380	99.718778	47.921869
1985.200390	99.831928	47.926874
1982.089041	100.192797	47.931879
1980.585380	99.297393	47.936884
1978.296218	102.880679	47.941889
1975.792161	104.861768	47.946893
1973.126444	106.102398	47.951898
1970.115661	102.148125	47.956903
1966.835346	106.825293	47.961908
1963.972627	108.957115	47.966913
1960.461782	101.069075	47.971917
1956.725395	105.624238	47.976922
1953.993115	99.415184	47.981927
1950.004593	107.850340	47.986932
1947.264935	93.641397	47.991937
1943.905580	103.079604	47.996941
1940.297550	105.485609	48.001946
1936.904535	96.367533	48.006951
1933.532463	108.639248	48.011956
1930.073776	99.559865	48.016961
1927.051400	101.855740	48.021965
1923.505053	98.718808	48.026970
1920.341036	99.818697	48.031975
1915.970766	107.724816	48.036980
1912.485939	93.103514	48.041985
1909.321764	97.446236	48.046989
1905.944868	106.842882	48.051994
1903.146116	100.368936	48.056999
1899.945647	101.015761	48.062004
1896.693063	99.576318	48.067009
1892.872152	102.420413	48.072013
1889.511978	107.021430	48.077018
1886.039162	97.374786	48.082023
1881.935100	104.600404	48.087028
1878.973779	103.394037	48.092033
1875.200784	97.128670	48.097037
1871.896114	108.070624	48.102042
1868.903161	105.100665	48.107047
1865.306286	101.620429	48.112052
1861.934012	105.353308	48.117057
1857.968229	102.518940	48.122061
1854.091565	106.270211	48.127066
1851.313790	94.696265	48.132071
1847.471585	109.784087	48.137076
1844.577479	96.216123	48.142081
1841.120335	100.401967	48.147085
1837.104480	102.064705	48.152090
1834.159062	97.135341	48.157095
1830.243021	104.413954	48.162100
1827.040288	96.253359	48.167105
1823.375237	101.271982	48.172109
1819.919447	103.882088	48.177114
1816.621728	91.857568	48.182119
1813.051057	96.146502	48.187124
1809.327343	94.017939	48.192129
1805.703471	90.374238	48.197133
1802.284108	98.546807	48.202138
1799.215949	98.818711	48.207143
1796.100516	110.711963	48.212148
1792.704475	99.794226	48.217153
1789.221962	105.850612	48.222157
1785.056223	103.610515	48.227162
1782.078019	100.442120	48.232167
1777.778452	108.906709	48.237172
1774.773325	100.130078	48.242177
1771.392383	94.297248	48.247181
1768.017490	91.605042	48.252186
1764.507602	91.417359	48.257191
1760.907596	101.260010	48.262196
1757.493256	101.718673	48.267201
1753.937502	99.813907	48.272205
1750.321903	91.926389	48.277210
1747.012529	92.020707	48.282215
1743.474530	95.162461	48.287220
1740.230960	85.761739	48.292225
1736.538358	94.040107	48.297229
1732.819472	97.099285	48.302234
1729.407270	89.018766	48.307239
1725.890277	97.427990	48.312244
1722.422802	97.255856	48.317249
1719.082381	94.203954	48.322253
1715.695996	97.610010	48.327258
1712.212053	88.357432	48.332263
1708.580031	95.322926	48.337268
1705.041462	89.679152	48.342273
1701.647780	88.258526	48.347277
1697.913091	92.623612	48.352282
1694.796073	92.567775	48.357287
1690.635330	92.766133	48.362292
1687.946782	89.040146	48.367297
1684.720266	88.754584	48.372301
1680.808307	84.848859	48.377306
1676.958686	83.458070	48.382311
1673.339178	90.826569	48.387316
1670.250007	91.127063	48.392321
1666.490231	91.487639	48.397325
1663.256521	88.972785	48.402330
1659.900986	85.217738	48.407335
1656.329830	91.968118	48.412340
1652.686681	90.307917	48.417345
1649.197942	90.177064	48.422349
1645.256034	87.886331	48.427354
1642.714369	90.553484	48.432359
1638.979912	89.666785	48.437364
1635.378642	86.513127	48.442369
1632.018597	84.473514	48.447373
1628.336294	89.396753	48.452378
1624.780089	82.455455	48.457383
1621.026848	86.949981	48.462388
1617.211553	84.364303	48.467393
1614.113425	86.108844	48.472397
1611.032331	85.414682	48.477402
1607.937496	88.534924	48.482407
1604.119731	82.732144	48.487412
1600.150073	83.666387	48.492417
1596.719186	80.185664	48.497421
1592.782626	92.959665	48.502426
1589.568701	87.736771	48.507431
1585.960952	91.490494	48.512436
1583.036374	90.022176	48.517441
1579.454372	87.428665	48.522445
1576.058837	89.947150	48.527450
1572.504323	88.336438	48.532455
1568.682944	85.457488	48.537460
1565.255378	83.292352	48.542465
1561.827749	86.116385	48.547469
1558.171218	83.025121	48.552474
1555.074122	81.887373	48.557479
1551.376728	88.211322	48.562484
1548.052148	79.300964	48.567489
1544.059074	83.450014	48.572493
1540.676041	88.905636	48.577498
1537.379391	77.596010	48.582503
1533.750155	90.306356	48.587508
1530.622933	79.770777	48.592513
1527.011065	81.301061	48.597517
1523.325803	77.322111	48.602522
1519.774445	78.127981	48.607527
1515.784323	80.061983	48.612532
1512.769582	82.587641	48.617537
1509.381438	78.135348	48.622541
1505.763385	85.010087	48.627546
1502.783195	79.175035	48.632551
1498.582579	84.390922	48.637556
1494.984777	87.409123	48.642561
1491.926571	79.472862	48.647565
1488.184688	79.039746	48.652570
1485.313835	77.806681	48.657575
1481.908587	82.566584	48.662580
1478.081290	73.737650	48.667585
1474.539538	74.162386	48.672589
1470.656000	77.506630	48.677594
1467.405153	76.990761	48.682599
1463.600652	90.883137	48.687604
1460.137316	81.311030	48.692609
1456.618576	76.907544	48.697613
1452.805659	75.226336	48.702618
1449.730909	65.378627	48.707623
1446.438674	81.396358	48.712628
1442.962395	81.889998	48.717633
1439.636825	70.701954	48.722637
1435.713179	86.523743	48.727642
1432.624965	81.673606	48.732647
1428.798493	79.940727	48.737652
1425.140996	75.748665	48.742657
1421.944419	87.686161	48.747661
1418.501122	82.173133	48.752666
1415.016285	75.265055	48.757671
1411.130904	96.202923	48.762676
1407.842341	85.401414	48.767681
1404.175126	81.543054	48.772685
1400.627525	87.157172	48.777690
1397.571078	80.245691	48.782695
1393.840830	91.921412	48.787700
1390.490216	90.560551	48.792705
1387.369663	81.415986	48.797709
1383.201193	85.750534	48.802714
1380.005736	80.790548	48.807719
1376.099505	84.777400	48.812724
1372.938340	83.080176	48.817729
1369.243143	83.367457	48.822733
1365.434560	83.178850	48.827738
1362.424731	88.497298	48.832743
1358.341379	81.093938	48.837748
1355.227203	81.319258	48.842753
1352.254117	81.620691	48.847757
1348.289919	86.546696	48.852762
1345.097598	84.604392	48.857767
1341.216999	81.370866	48.862772
1337.883033	72.601211	48.867777
1334.780102	84.179285	48.872781
1330.831311	82.696408	48.877786
1327.224968	73.747691	48.882791
1323.391999	79.466339	48.887796
1320.316359	81.764211	48.892801
1317.161700	76.981379	48.897805
1313.313791	87.938271	48.902810
1310.070311	85.453451	48.907815
1306.256935	84.550601	48.912820
1302.564701	87.365220	48.917825
1299.158073	81.122016	48.922829
1295.761430	86.940429	48.927834
1292.360802	82.727385	48.932839
1288.430581	87.154569	48.937844
1285.160858	79.292392	48.942849
1282.030630	89.273888	48.947853
1277.908133	86.615850	48.952858
1274.812051	78.986071	48.957863
1271.271891	87.152139	48.962868
1267.283997	84.397223	48.967873
1264.486209	84.260098	48.972877
1260.970239	85.803954	48.977882
1257.451611	85.022907	48.982887
1253.720452	89.836718	48.987892
1250.379325	89.202046	48.992897
1246.735667	89.604702	48.997901
1243.073370	89.469267	49.002906
1239.752877	80.688037	49.007911
1236.343907	90.722413	49.012916
1233.099693	81.812254	49.017921
1229.382573	77.120145	49.022925
1225.631647	82.832358	49.027930
1222.420672	81.516220	49.032935
1218.854146	85.168640	49.037940
1215.028271	81.641882	49.042945
1211.743909	80.416260	49.047949
1208.258970	87.687902	49.052954
1204.670216	85.421350	49.057959
1201.148608	90.395532	49.062964
1197.985520	88.926412	49.067969
1194.587439	78.581748	49.072973
1190.799091	82.395246	49.077978
1187.041385	81.537528	49.082983
1183.063213	83.343156	49.087988
1179.802269	84.167129	49.092993
1176.992601	83.044789	49.097997
1173.050631	84.395538	49.103002
1170.211547	79.788226	49.108007
1166.300352	92.700645	49.113012
1162.568427	81.708775	49.118017
1159.657007	74.224275	49.123021
1155.689303	85.047959	49.128026
1152.030032	85.598585	49.133031
1148.116174	83.850871	49.138036
1144.973114	90.098047	49.143041
1141.976350	79.257501	49.148045
1138.122130	80.161170	49.153050
1134.768163	80.572528	49.158055
1131.385641	79.162882	49.163060
1128.163368	84.900379	49.168065
1124.579416	79.747805	49.173069
1120.441135	88.342332	49.178074
1117.002727	77.659119	49.183079
1113.672274	71.388273	49.188084
1109.841883	78.286589	49.193089
1106.704973	79.888512	49.198093
1103.059147	82.901565	49.203098
1099.674958	74.253662	49.208103
1096.241660	79.049590	49.213108
1092.789675	76.094227	49.218113
1089.396407	76.900841	49.223117
1085.580692	84.666891	49.228122
1082.360580	73.323298	49.233127
1079.024610	81.387987	49.238132
1074.868626	77.706995	49.243137
1071.693080	80.115347	49.248141
1067.818654	74.568246	49.253146
1064.480848	77.305570	49.258151
1061.227030	76.321979	49.263156
1057.366112	70.440591	49.268161
1054.321545	72.942449	49.273165
1050.632540	78.047097	49.278170
1047.133563	75.434406	49.283175
1043.684858	84.402477	49.288180
1039.942060	81.603117	49.293185
1037.320514	78.591260	49.298189
1033.009413	86.193985	49.303194
1029.514999	74.206579	49.308199
1025.611284	75.880414	49.313204
1022.367156	77.878676	49.318209
1019.253359	69.574670	49.323213
1016.121282	78.113811	49.328218
1012.464354	65.689814	49.333223
1008.721205	78.107842	49.338228
1004.547677	78.823953	49.343233
1001.502747	75.896987	49.348237
997.767117	79.714949	49.353242
994.553195	74.742075	49.358247
991.009835	81.019930	49.363252
987.648197	77.984080	49.368257
984.421341	70.349399	49.373261
980.752396	87.852579	49.378266
977.332425	77.802426	49.383271
973.288120	77.172842	49.388276
969.578370	78.509613	49.393281
966.388373	80.847459	49.398285
962.931487	83.970316	49.403290
959.543113	72.478938	49.408295
956.257758	81.127361	49.413300
952.397158	76.062171	49.418305
948.895376	77.315952	49.423309
945.269372	81.708464	49.428314
941.729624	77.333634	49.433319
938.859280	73.743599	49.438324
935.566057	73.832318	49.443329
931.785955	72.607969	49.448333
927.705081	81.513101	49.453338
924.753573	73.177521	49.458343
921.131080	74.434277	49.463348
917.523653	76.258151	49.468353
913.993327	83.296430	49.473357
910.027041	83.733527	49.478362
907.051494	74.060289	49.483367
903.641986	78.751290	49.488372
899.859788	79.909525	49.493377
896.399363	70.881232	49.498381
893.215077	76.182566	49.503386
889.590839	74.323369	49.508391
886.152332	77.775558	49.513396
882.456204	83.504575	49.518401
878.956520	69.664107	49.523405
875.294316	82.275179	49.528410
872.192837	69.834348	49.533415
868.671680	70.464745	49.538420
864.965453	76.378826	49.543425
861.372758	73.144850	49.548429
857.396362	79.537577	49.553434
854.505304	74.175951	49.558439
851.223567	73.870595	49.563444
847.303409	76.641644	49.568449
844.193682	70.380774	49.573453
840.160045	77.896028	49.578458
836.693477	74.620275	49.583463
833.355910	85.001038	49.588468
829.680052	85.709304	49.593473
826.893989	76.424190	49.598477
823.134908	79.439080	49.603482
819.393614	72.839939	49.608487
815.900912	71.349411	49.613492
812.046450	72.771999	49.618497
808.914850	77.365964	49.623501
805.390382	79.967856	49.628506
802.213574	83.540664	49.633511
798.496315	74.833936	49.638516
794.764623	80.074961	49.643521
791.505599	77.181348	49.648525
787.734232	81.580684	49.653530
784.393937	68.509512	49.658535
781.081903	70.015341	49.663540
777.169895	76.024736	49.668545
774.079127	70.175369	49.673549
770.477038	74.380678	49.678554
766.790069	74.252306	49.683559
763.455948	74.489776	49.688564
759.483975	72.931497	49.693569
756.239349	79.178682	49.698573
752.579443	80.510882	49.703578
749.541806	86.381007	49.708583
746.269841	81.818991	49.713588
742.747559	82.054118	49.718593
739.046145	69.690889	49.723597
735.457855	76.817292	49.728602
731.877151	76.859040	49.733607
728.237107	78.719649	49.738612
724.545082	73.283417	49.743617
721.370215	71.256218	49.748621
717.716992	69.540761	49.753626
714.212642	70.405835	49.758631
710.498177	70.588627	49.763636
707.248625	77.969178	49.768641
704.216691	72.528268	49.773645
700.857055	73.861186	49.778650
697.179963	82.152996	49.783655
693.559836	73.620991	49.788660
689.723765	69.883939	49.793665
686.154156	75.403453	49.798669
682.352071	73.856703	49.803674
678.994004	73.439866	49.808679
675.874921	71.381843	49.813684
672.292545	74.125638	49.818689
668.818083	73.363099	49.823693
665.190746	69.754905	49.828698
661.616733	75.290925	49.833703
657.965465	76.814776	49.838708
654.775426	80.611112	49.843713
651.585805	65.830278	49.848717
647.679134	72.503224	49.853722
644.303110	76.502514	49.858727
640.707316	80.355689	49.863732
637.092104	78.463486	49.868737
633.844886	69.180599	49.873741
629.981437	82.107734	49.878746
626.576165	73.630879	49.883751
623.649273	64.772681	49.888756
619.847092	72.916290	49.893761
616.485509	75.204951	49.898765
612.564683	73.964591	49.903770
609.622809	79.367408	49.908775
605.973900	67.992597	49.913780
602.261553	71.228019	49.918785
598.700897	71.453319	49.923789
594.798215	75.461837	49.928794
591.531288	71.316669	49.933799
588.219177	78.349470	49.938804
584.502534	85.473722	49.943809
581.494404	66.706893	49.948813
577.783108	67.904749	49.953818
574.146207	73.877661	49.958823
570.829864	73.840311	49.963828
566.945117	72.736707	49.968833
563.558776	74.130744	49.973837
560.097196	76.786145	49.978842
556.635670	74.727665	49.983847
553.450093	64.492426	49.988852
549.410217	76.323921	49.993857
546.342655	76.731887	49.998861
542.534498	75.527780	50.003866
539.281654	75.888662	50.008871
535.858995	75.244623	50.013876
532.116082	77.159234	50.018881
528.973996	69.894243	50.023885
525.493854	67.924085	50.028890
521.688575	71.651698	50.033895
518.354515	64.565290	50.038900
514.154338	71.268120	50.043905
511.005629	67.942936	50.048909
507.355285	70.833367	50.053914
503.895394	72.732394	50.058919
500.870396	70.843240	50.063924
496.879705	72.597117	50.068929
493.652306	59.663465	50.073933
489.718868	69.852264	50.078938
486.607457	75.192898	50.083943
483.305773	73.492349	50.088948
479.672323	75.196941	50.093953
476.212160	62.935425	50.098957
472.743223	65.769146	50.103962
469.267051	66.012947	50.108967
465.815379	68.707943	50.113972
461.667430	72.207342	50.118977
458.625181	65.534248	50.123981
454.764233	68.084159	50.128986
451.738721	79.691309	50.133991
448.171520	78.699635	50.138996
444.553274	83.293460	50.144001
441.415690	70.045282	50.149005
437.569697	71.495073	50.154010
433.886416	68.262613	50.159015
430.946351	76.892102	50.164020
427.052088	81.886394	50.169025
423.793686	73.358242	50.174029
419.902164	75.302329	50.179034
416.762843	70.615319	50.184039
413.213394	70.177692	50.189044
409.111908	73.154187	50.194049
405.946346	72.128465	50.199053
402.543959	65.438683	50.204058
398.763984	75.499198	50.209063
395.704917	68.135889	50.214068
392.057564	75.347439	50.219073
388.631703	69.717977	50.224077
385.001706	81.552111	50.229082
381.370503	73.822304	50.234087
378.040482	69.876815	50.239092
374.356096	70.668722	50.244097
371.261124	74.273115	50.249101
367.602722	63.924870	50.254106
363.927475	68.942014	50.259111
360.741704	66.442013	50.264116
356.789968	74.128047	50.269121
353.301990	62.823155	50.274125
350.120560	74.524178	50.279130
346.336861	68.089917	50.284135
343.398612	67.990570	50.289140
339.556335	72.087785	50.294145
336.144044	71.853436	50.299149
332.161357	70.970755	50.304154
328.605643	67.465360	50.309159
325.341844	65.509007	50.314164
321.974190	70.066992	50.319169
318.757818	68.976428	50.324173
315.071378	60.881929	50.329178
311.525715	68.371872	50.334183
307.754287	64.431842	50.339188
304.277929	70.057089	50.344193
301.052654	68.904640	50.349197
297.128438	61.521023	50.354202
293.424398	63.695358	50.359207
290.415137	68.817628	50.364212
286.913260	83.615156	50.369217
283.677961	75.191000	50.374221
279.902154	70.789760	50.379226
276.700499	74.268406	50.384231
273.149161	65.327163	50.389236
269.319240	79.666411	50.394241
266.186880	66.553502	50.399245
262.175245	74.723420	50.404250
258.827231	69.005935	50.409255
255.894223	72.651561	50.414260
251.455680	71.362150	50.419265
248.351051	64.502658	50.424269
244.634211	71.826274	50.429274
241.373473	66.566592	50.434279
237.876144	68.025402	50.439284
234.385422	76.990559	50.444289
231.135850	72.694056	50.449293
227.296757	62.415103	50.454298
223.608024	75.463740	50.459303
220.357661	68.177700	50.464308
216.789785	78.932850	50.469313
213.299723	68.245227	50.474317
209.598468	70.406486	50.479322
206.170000	73.844523	50.484327
203.314624	72.878100	50.489332
199.185681	75.264131	50.494337
196.012602	72.509083	50.499341
192.598705	78.596004	50.504346
188.747054	75.231616	50.509351
185.293055	73.209985	50.514356
181.516250	76.135962	50.519361
178.249847	72.750060	50.524365
174.876719	74.053504	50.529370
171.687989	69.301463	50.534375
167.839357	70.381555	50.539380
164.413907	65.400623	50.544385
160.581377	67.373525	50.549389
157.248649	80.910891	50.554394
153.964568	74.677284	50.559399
150.445874	79.995937	50.564404
146.779878	76.650106	50.569409
143.514158	71.356415	50.574413
139.611483	71.223752	50.579418
135.603626	78.146613	50.584423
132.478914	70.575279	50.589428
129.021622	72.432818	50.594433
126.004352	64.155083	50.599437
122.382744	68.578625	50.604442
118.609620	76.461493	50.609447
115.329872	65.877189	50.614452
111.610077	70.278055	50.619457
108.419476	55.064099	50.624461
104.907076	63.602375	50.629466
101.587907	73.591165	50.634471
98.250446	64.970992	50.639476
93.943913	70.121252	50.644481
90.887585	64.962646	50.649485
87.221614	67.475921	50.654490
83.499089	68.988795	50.659495
79.883566	64.980243	50.664500
76.278048	69.818888	50.669505
73.061511	70.142539	50.674509
69.889865	63.091042	50.679514
66.024694	64.015541	50.684519
63.141324	63.385679	50.689524
58.982408	75.343301	50.694529
55.567995	66.513661	50.699533
52.312947	70.399264	50.704538
48.550119	72.646059	50.709543
45.195246	59.760836	50.714548
41.601014	66.470611	50.719553
38.073578	73.226935	50.724557
34.726652	70.527454	50.729562
31.025605	72.685541	50.734567
27.845748	59.874310	50.739572
24.330084	66.518073	50.744577
20.601976	61.916476	50.749581
17.352527	61.571401	50.754586
13.432683	66.177426	50.759591
10.127822	71.266650	50.764596
6.552957	72.478143	50.769601
3.308875	63.160104	50.774605