Fri Aug 26 14:02:27 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.973010	98.775763	0.000000
0.725496	115.657628	0.005005
1.083849	112.567852	0.010010
1.022847	102.684543	0.015014
0.500525	92.585172	0.020019
1.001260	93.136753	0.025024
0.480202	91.009618	0.030029
0.159769	81.888028	0.035034
0.014960	79.559949	0.040038
-0.352754	75.437980	0.045043
-0.350314	58.660696	0.050048
-0.545635	61.794629	0.055053
-0.711920	54.854122	0.060058
-0.709923	38.747620	0.065062
-1.499781	29.993365	0.070067
-1.554279	23.816887	0.075072
-1.642258	22.463863	0.080077
-2.243768	7.485867	0.085082
-2.643332	1.720615	0.090086
-3.237482	0.740620	0.095091
-3.217569	-3.416373	0.100096
-3.939796	-6.211340	0.105101
-4.052664	-8.351398	0.110106
-3.649085	-9.132407	0.115110
-4.702405	-10.097855	0.120115
-4.892288	-10.546027	0.125120
-5.244787	-22.152358	0.130125
-4.894746	-20.425753	0.135130
-5.181761	-20.302000	0.140134
-5.704348	-13.766829	0.145139
-5.719093	-9.243711	0.150144
-6.437018	-10.982690	0.155149
-6.688048	-14.689385	0.160154
-6.884722	-20.192001	0.165158
-6.764439	-9.758076	0.170163
-6.611729	-11.683228	0.175168
-7.678244	-7.866356	0.180173
-8.073825	-21.145875	0.185178
-8.080381	-18.430474	0.190182
-8.234713	-7.270445	0.195187
-8.163545	-17.307138	0.200192
-8.625100	-4.264361	0.205197
-8.998692	-1.738576	0.210202
-9.149095	-10.219061	0.215206
-9.422587	-6.490859	0.220211
-9.403200	-12.596573	0.225216
-10.083723	-7.909687	0.230221
-10.923057	-9.335544	0.235226
-10.915569	-8.783097	0.240230
-11.407571	-2.967668	0.245235
-10.919844	-5.599856	0.250240
-11.123723	-1.825546	0.255245
-10.713423	-7.938343	0.260250
-11.054689	-13.709503	0.265254
-11.994537	-3.499644	0.270259
-12.291478	-12.855788	0.275264
-12.208668	-7.398766	0.280269
-12.751350	-13.771295	0.285274
-13.159708	-14.330979	0.290278
-13.708148	-9.180620	0.295283
-13.962656	-6.983414	0.300288
-13.895394	-9.426755	0.305293
-13.782865	-12.845217	0.310298
-13.425501	-9.297493	0.315302
-14.496335	-5.979803	0.320307
-15.074131	-10.243042	0.325312
-15.062902	-13.101586	0.330317
-15.520169	-2.818173	0.335322
-14.979202	-8.897532	0.340326
-15.824714	-7.351765	0.345331
-16.374015	-12.464133	0.350336
-16.697186	-6.624373	0.355341
-16.837983	-10.737360	0.360346
-16.642091	-14.415566	0.365350
-16.969404	-9.932365	0.370355
-16.863663	-12.634788	0.375360
-16.702498	-7.490512	0.380365
-17.768669	-9.390397	0.385370
-18.061510	-17.073609	0.390374
-18.674928	-8.559672	0.395379
-18.292560	-7.262028	0.400384
-18.672287	-4.855507	0.405389
-19.112769	-10.984529	0.410394
-19.562433	-12.888657	0.415398
-19.763512	-4.840701	0.420403
-19.631920	-9.758536	0.425408
-20.179502	-9.287340	0.430413
-20.269396	-14.075780	0.435418
-20.047638	-20.001035	0.440422
-20.632677	-9.102968	0.445427
-20.878448	-18.147547	0.450432
-21.115730	-10.321739	0.455437
-21.217063	-6.158450	0.460442
-22.073984	-16.661225	0.465446
-22.602761	0.631303	0.470451
-22.569448	-8.475715	0.475456
-22.747751	-6.340993	0.480461
-22.865663	-9.508449	0.485466
-22.891683	-8.356020	0.490470
-22.822357	-5.506905	0.495475
-22.741256	-15.494526	0.500480
-23.625360	-9.538959	0.505485
-24.467196	0.155785	0.510490
-24.259802	-21.829054	0.515494
-24.446096	-4.134291	0.520499
-25.201437	-1.387723	0.525504
-25.626419	-5.709555	0.530509
-25.400973	-1.669907	0.535514
-25.696467	-6.163755	0.540518
-25.933594	2.221999	0.545523
-25.857978	-4.512546	0.550528
-25.867482	-1.897921	0.555533
-26.086231	-6.916229	0.560538
-26.622867	-9.018779	0.565542
-27.354488	-4.633974	0.570547
-27.103385	-16.992323	0.575552
-27.291522	-9.319694	0.580557
-28.032832	0.308779	0.585562
-28.258645	-6.856543	0.590566
-28.439325	-5.955271	0.595571
-28.487775	-13.714498	0.600576
-28.796548	-14.564923	0.605581
-28.764481	-12.184555	0.610586
-28.981347	-13.248599	0.615590
-29.699300	-3.832564	0.620595
-30.114781	-15.568291	0.625600
-30.019337	-4.330097	0.630605
-30.298843	-5.011078	0.635610
-30.129374	-8.571280	0.640614
-30.848314	-2.527535	0.645619
-31.162182	-6.034629	0.650624
-31.395908	-7.437722	0.655629
-31.711050	-4.111145	0.660634
-31.451830	-10.219400	0.665638
-31.993517	3.164876	0.670643
-32.532664	-9.734803	0.675648
-32.670844	-0.206563	0.680653
-33.192217	-8.376197	0.685658
-33.254223	-18.585134	0.690662
-33.228434	-12.432727	0.695667
-32.947808	-8.442800	0.700672
-33.446881	-12.794221	0.705677
-34.088827	-12.254551	0.710682
-34.058957	-12.765410	0.715686
-34.492535	-1.568229	0.720691
-34.539601	-5.237081	0.725696
-35.217127	-9.152609	0.730701
-35.558657	-2.737371	0.735706
-35.455908	-9.972830	0.740710
-35.935848	-5.019791	0.745715
-35.677821	-16.249797	0.750720
-36.305317	-9.461018	0.755725
-37.200128	-20.957600	0.760730
-37.344955	-15.692922	0.765734
-37.453430	-5.584036	0.770739
-37.162468	-4.496779	0.775744
-37.499282	-6.222331	0.780749
-37.397294	-11.508866	0.785754
-37.213300	-19.067008	0.790758
-38.146466	-10.183761	0.795763
-38.728295	-13.307458	0.800768
-38.528823	-8.979041	0.805773
-39.085604	-10.353980	0.810778
-39.581531	-9.185334	0.815782
-40.151658	-8.710627	0.820787
-40.261310	-12.739880	0.825792
-40.127259	-4.177811	0.830797
-40.389376	-14.542249	0.835802
-40.019329	-14.609381	0.840806
-40.518623	-6.486523	0.845811
-41.037152	-6.162214	0.850816
-41.330612	-3.538178	0.855821
-41.723739	0.480725	0.860826
-41.481166	-13.062664	0.865830
-41.849312	-0.521632	0.870835
-42.323988	-8.208170	0.875840
-42.735341	-9.504516	0.880845
-43.267674	-7.482345	0.885850
-43.147974	-13.496111	0.890854
-43.252004	-7.342471	0.895859
-43.173977	-11.198472	0.900864
-43.338088	-10.631963	0.905869
-44.132733	-7.531275	0.910874
-44.388087	-19.842403	0.915878
-44.844083	-15.820042	0.920883
-44.485270	-13.357675	0.925888
-44.942299	-11.122610	0.930893
-45.224456	-11.170450	0.935898
-45.424610	-5.134716	0.940902
-45.866263	-1.301240	0.945907
-46.176535	-13.451967	0.950912
-46.960591	-9.441799	0.955917
-46.882373	-9.185093	0.960922
-46.940126	-16.322796	0.965926
-47.362848	-9.214735	0.970931
-47.480078	-2.578166	0.975936
-47.390342	-7.578066	0.980941
-47.910953	-4.766808	0.985946
-47.403243	-6.421378	0.990950
-47.782246	-13.274954	0.995955
-48.744902	-6.146098	1.000960
-48.979742	-0.136599	1.005965
-49.033743	2.146444	1.010970
-49.119104	-2.898959	1.015974
-50.135634	-6.897741	1.020979
-50.440176	-16.141968	1.025984
-50.480436	-11.564262	1.030989
-50.707686	-6.593622	1.035994
-50.639842	-11.080766	1.040998
-50.834933	-10.019068	1.046003
-50.674751	-7.680792	1.051008
-50.558641	-14.877201	1.056013
-51.496005	-6.252718	1.061018
-51.353092	-16.072796	1.066022
-51.795491	-6.221957	1.071027
-52.691379	-5.993913	1.076032
-53.372116	-13.854001	1.081037
-53.667827	-15.256933	1.086042
-52.596618	-12.918139	1.091046
-53.294545	-7.820434	1.096051
-53.620661	-15.675627	1.101056
-53.652653	-7.926074	1.106061
-54.020712	-1.513033	1.111066
-54.230656	-7.795003	1.116070
-54.941705	-6.216389	1.121075
-55.110497	-16.829464	1.126080
-54.782426	-14.827366	1.131085
-55.253398	-5.652261	1.136090
-55.229614	-13.704297	1.141094
-55.908069	-6.189437	1.146099
-56.421391	-17.909925	1.151104
-56.560408	-13.098552	1.156109
-56.549425	-12.043631	1.161114
-56.304776	-12.638549	1.166118
-57.319340	-3.998881	1.171123
-57.741583	-10.228814	1.176128
-57.474779	-15.509372	1.181133
-57.851604	-11.040609	1.186138
-58.024178	-10.444310	1.191142
-58.040274	-1.283081	1.196147
-58.698206	-10.162251	1.201152
-59.340049	-3.016909	1.206157
-59.120552	-8.366031	1.211162
-59.383011	-11.352798	1.216166
-59.599415	-5.776427	1.221171
-59.516278	-16.223090	1.226176
-60.185139	-16.084175	1.231181
-61.057107	-2.784518	1.236186
-60.575345	-14.517578	1.241190
-61.325906	-7.551456	1.246195
-60.870614	-8.754953	1.251200
-60.834543	-9.038996	1.256205
-61.110944	0.010908	1.261210
-61.793372	-9.547796	1.266214
-62.225005	-2.330782	1.271219
-62.551335	-9.942343	1.276224
-62.285695	-9.480709	1.281229
-63.085107	2.238487	1.286234
-63.174478	-12.123219	1.291238
-63.826633	-4.675726	1.296243
-63.907544	-2.755477	1.301248
-64.204986	-7.090837	1.306253
-64.619601	3.154299	1.311258
-64.224448	-9.090444	1.316262
-64.402021	-5.766305	1.321267
-64.537491	-7.396660	1.326272
-64.886089	2.120050	1.331277
-65.838283	0.702276	1.336282
-65.878586	-7.478984	1.341286
-65.690072	-5.281156	1.346291
-65.707443	-6.208588	1.351296
-66.581543	-6.800155	1.356301
-66.875030	-5.115718	1.361306
-66.723735	-7.733487	1.366310
-67.129082	-8.730221	1.371315
-67.108534	-8.385445	1.376320
-67.154038	-9.378097	1.381325
-68.043887	-10.587285	1.386330
-68.245109	-1.941380	1.391334
-68.485683	-2.837224	1.396339
-68.441857	-8.994195	1.401344
-68.310373	-11.403242	1.406349
-69.304044	-13.580158	1.411354
-69.551740	-20.577556	1.416358
-69.311001	-10.387011	1.421363
-69.924797	-13.429802	1.426368
-69.772375	-7.382530	1.431373
-70.845180	-5.491335	1.436378
-70.936057	-8.052417	1.441382
-70.987084	-8.920826	1.446387
-71.356327	-9.711217	1.451392
-71.324481	-5.619283	1.456397
-71.596693	0.010069	1.461402
-71.734554	-7.323963	1.466406
-72.502778	-3.069495	1.471411
-72.984833	-11.479355	1.476416
-72.718620	-13.263996	1.481421
-72.967685	-7.233304	1.486426
-72.721781	-9.736094	1.491430
-72.694543	-5.425151	1.496435
-73.646580	-9.861064	1.501440
-74.100155	-10.113159	1.506445
-74.506441	-3.630895	1.511450
-74.461968	-11.942407	1.516454
-74.612721	-3.124033	1.521459
-74.854417	-13.112011	1.526464
-75.278699	-18.398857	1.531469
-75.959946	-10.940510	1.536474
-75.813090	-15.190026	1.541478
-75.878588	-6.391255	1.546483
-76.108060	-10.408178	1.551488
-75.875651	-11.418791	1.556493
-76.228184	-11.126655	1.561498
-76.951219	-9.615774	1.566502
-77.397178	-5.591811	1.571507
-77.622681	-9.406879	1.576512
-77.797618	-8.974720	1.581517
-77.845040	-7.625978	1.586522
-77.602619	-11.314591	1.591526
-78.574482	-6.892381	1.596531
-78.660818	-5.676779	1.601536
-78.907228	-12.010015	1.606541
-79.253024	-8.045938	1.611546
-79.177197	-13.100616	1.616550
-79.753475	-14.652845	1.621555
-80.369660	-9.210376	1.626560
-80.393660	-7.798844	1.631565
-80.324420	-2.678221	1.636570
-80.340416	-19.202621	1.641574
-80.385372	-6.721408	1.646579
-80.965258	-7.263874	1.651584
-81.424609	-17.132541	1.656589
-81.881372	-9.471873	1.661594
-81.243361	-15.537865	1.666598
-82.492800	-12.999095	1.671603
-83.060534	-1.420374	1.676608
-83.063935	-11.008871	1.681613
-83.413295	1.168578	1.686618
-83.067645	-13.238712	1.691622
-83.321585	-11.136505	1.696627
-83.135817	-6.053008	1.701632
-83.408550	-8.772429	1.706637
-84.403950	-0.695709	1.711642
-84.605165	-9.804170	1.716646
-84.827694	-6.055431	1.721651
-85.236246	-7.418648	1.726656
-84.656742	-18.572156	1.731661
-85.395837	-2.224458	1.736666
-85.717768	-4.632510	1.741670
-86.277645	-4.896527	1.746675
-86.425948	-4.816516	1.751680
-85.868372	-9.386237	1.756685
-86.515395	-11.190034	1.761690
-87.006270	-12.597378	1.766694
-87.614707	-14.679255	1.771699
-87.702640	-11.761367	1.776704
-87.542282	-12.191306	1.781709
-88.000734	-11.404968	1.786714
-87.774872	-14.341219	1.791718
-88.656580	-13.223234	1.796723
-89.198810	-8.285808	1.801728
-88.859629	-2.919323	1.806733
-89.338646	-8.542487	1.811738
-89.315676	-16.686138	1.816742
-89.058123	-14.688880	1.821747
-90.089660	-7.523992	1.826752
-90.474235	-14.841752	1.831757
-90.838531	-12.387016	1.836762
-90.675873	-10.998220	1.841766
-90.612717	-3.355228	1.846771
-90.827969	-7.507238	1.851776
-91.209592	-12.158507	1.856781
-91.991772	4.100996	1.861786
-92.107306	-13.375986	1.866790
-92.429559	1.587574	1.871795
-92.531055	-9.912308	1.876800
-92.384094	-6.901283	1.881805
-92.808005	-3.428062	1.886810
-93.125837	-13.366219	1.891814
-93.482260	-11.441037	1.896819
-93.800074	-4.067748	1.901824
-93.692479	-13.559633	1.906829
-94.438234	-8.451318	1.911834
-94.787899	-9.972394	1.916838
-95.204292	-7.604456	1.921843
-95.306054	0.706435	1.926848
-95.223328	-14.302136	1.931853
-95.753332	-10.220797	1.936858
-95.474932	-21.665930	1.941862
-95.615171	-15.854659	1.946867
-95.801460	-17.957973	1.951872
-96.514570	-15.803255	1.956877
-96.864697	-13.179890	1.961882
-96.818208	-8.827655	1.966886
-96.840439	-2.598171	1.971891
-97.744116	-10.569073	1.976896
-98.179463	-18.252235	1.981901
-98.252275	-6.162141	1.986906
-98.472634	-7.791932	1.991910
-98.468210	-10.541851	1.996915
-98.800266	-12.883238	2.006912
-98.593757	-9.269429	2.016909
-97.936443	-10.509025	2.026906
-97.531768	-14.458842	2.036902
-96.864494	-11.379257	2.046899
-96.142748	-10.452681	2.056896
-95.713835	-13.120189	2.066893
-96.059320	-8.780560	2.076890
-95.199849	-9.462441	2.086886
-94.446890	-7.688615	2.096883
-93.833562	-4.987088	2.106880
-93.298035	-8.580324	2.116877
-93.126747	-8.065369	2.126874
-92.704277	-3.195932	2.136870
-91.703977	-13.596049	2.146867
-91.792632	-14.922229	2.156864
-90.892947	-7.431390	2.166861
-90.449996	-7.915376	2.176858
-90.158513	-0.963375	2.186854
-89.012235	-7.147849	2.196851
-88.946317	-9.039773	2.206848
-88.819834	-9.401628	2.216845
-87.897849	-7.882193	2.226842
-87.424598	-11.696974	2.236838
-87.231253	-6.177330	2.246835
-86.378458	-6.078919	2.256832
-86.150440	-7.498755	2.266829
-85.239623	-1.416101	2.276826
-84.749160	-7.260887	2.286822
-84.505740	-12.246775	2.296819
-84.217023	-3.818199	2.306816
-83.508438	-6.494408	2.316813
-83.007537	-3.398420	2.326810
-82.178466	-6.853635	2.336806
-82.215699	-4.022306	2.346803
-81.690672	-5.209629	2.356800
-81.004886	-7.518003	2.366797
-80.601077	-7.305337	2.376794
-79.620060	-8.608005	2.386790
-79.120322	-11.099647	2.396787
-79.155770	-0.260666	2.406784
-78.693601	-5.458005	2.416781
-78.385336	-2.008918	2.426778
-77.316941	-4.335685	2.436774
-76.646692	-7.709153	2.446771
-76.568832	-9.029584	2.456768
-76.024324	-12.259933	2.466765
-75.262255	-16.116515	2.476762
-75.101915	-12.758435	2.486758
-74.143938	-10.389326	2.496755
-73.796302	-13.608029	2.506752
-73.652165	-6.794640	2.516749
-73.027737	-12.863015	2.526746
-72.060296	-18.034488	2.536742
-72.035552	-11.341890	2.546739
-71.476878	-13.925067	2.556736
-70.736004	-8.598375	2.566733
-70.683511	-4.216175	2.576730
-69.976205	-5.308338	2.586726
-69.197637	-13.161951	2.596723
-69.158913	-12.341263	2.606720
-68.315123	-8.012579	2.616717
-67.763349	-14.361070	2.626714
-67.397486	-9.188224	2.636710
-66.964829	-15.784254	2.646707
-66.333011	-11.283188	2.656704
-66.298278	-12.128086	2.666701
-65.280256	-2.577660	2.676698
-64.804416	-7.599737	2.686694
-64.614762	0.844267	2.696691
-63.618750	-6.048549	2.706688
-63.431627	-6.695435	2.716685
-62.798308	-11.605819	2.726682
-61.958081	-5.670559	2.736678
-61.453998	-8.609522	2.746675
-61.601111	-8.006980	2.756672
-61.634637	-10.669009	2.766669
-60.745459	-8.900552	2.776666
-59.400809	-10.836356	2.786662
-59.072618	-7.070434	2.796659
-58.922524	-6.143546	2.806656
-58.813030	-9.375854	2.816653
-57.828318	-5.620289	2.826650
-57.302736	-13.573891	2.836646
-57.021783	-13.342097	2.846643
-55.938972	-11.660806	2.856640
-55.875647	-11.563015	2.866637
-55.989527	-3.866845	2.876634
-54.738866	-7.146956	2.886630
-54.418121	-4.342854	2.896627
-53.867031	-7.957520	2.906624
-53.195448	-4.397112	2.916621
-53.054824	-7.684951	2.926618
-51.977741	-6.943574	2.936614
-51.493610	-1.241128	2.946611
-51.961223	-5.894573	2.956608
-50.901937	-6.224273	2.966605
-50.220576	-8.044133	2.976602
-50.120046	-7.923625	2.986598
-49.427771	-5.399108	2.996595
-48.686919	-5.432148	3.006592
-48.578746	-3.868361	3.016589
-47.686375	-7.292252	3.026586
-47.014994	-6.931184	3.036582
-47.229959	-8.563973	3.046579
-46.503197	-5.066007	3.056576
-46.060090	-3.513189	3.066573
-45.111501	-3.524722	3.076570
-44.271336	-6.104213	3.086566
-44.003205	-2.069188	3.096563
-44.025596	-0.409048	3.106560
-44.002515	1.465751	3.116557
-43.167792	-0.729602	3.126554
-41.932494	-4.431792	3.136550
-41.232435	0.818900	3.146547
-41.510364	1.980319	3.156544
-41.313227	-3.207434	3.166541
-40.556207	-3.768829	3.176538
-39.952039	-4.493319	3.186534
-38.740595	1.802284	3.196531
-38.562723	-6.033830	3.206528
-38.162059	-2.782854	3.216525
-38.353902	-2.417260	3.226522
-37.703463	-6.224786	3.236518
-36.781927	-6.745273	3.246515
-35.962277	-1.468854	3.256512
-35.427494	-7.326877	3.266509
-35.625363	0.366535	3.276506
-35.183679	-0.760296	3.286502
-34.278902	-9.995670	3.296499
-34.100367	-10.783765	3.306496
-33.141773	-14.170450	3.316493
-32.836392	-8.452845	3.326490
-32.626761	-16.946445	3.336486
-31.892803	-10.139360	3.346483
-31.485605	-8.989584	3.356480
-30.311104	-0.131899	3.366477
-29.820031	1.020658	3.376474
-29.735663	-8.343566	3.386470
-29.602773	-0.419727	3.396467
-29.245550	-3.776136	3.406464
-28.436037	1.029877	3.416461
-27.605154	1.071515	3.426458
-26.817194	-0.125068	3.436454
-26.787132	0.662125	3.446451
-26.602025	3.905484	3.456448
-25.829829	-2.651554	3.466445
-25.405408	-0.741044	3.476442
-24.728423	-5.639223	3.486438
-24.174898	-4.299993	3.496435
-23.793795	-7.131114	3.506432
-23.506270	-3.640784	3.516429
-22.786770	-0.670690	3.526426
-22.284911	-1.100493	3.536422
-21.855460	-3.657217	3.546419
-20.993142	2.860634	3.556416
-20.874531	-0.759556	3.566413
-20.562855	-2.015026	3.576410
-19.570077	-1.555116	3.586406
-19.409447	-3.832408	3.596403
-18.892177	-9.323420	3.606400
-18.042085	-9.002847	3.616397
-17.750318	-7.543670	3.626394
-17.454291	-5.594163	3.636390
-16.458776	-10.576779	3.646387
-16.225822	-7.543604	3.656384
-16.095094	-6.002335	3.666381
-15.211299	-8.490420	3.676378
-14.747224	-5.395030	3.686374
-14.442973	-4.222889	3.696371
-13.736631	0.890616	3.706368
-13.432267	-4.168119	3.716365
-12.674032	-0.073188	3.726362
-12.397809	-1.405498	3.736358
-11.662435	-0.709114	3.746355
-10.926427	-3.848909	3.756352
-11.054535	3.931843	3.766349
-10.582467	-2.930081	3.776346
-9.479970	-4.913709	3.786342
-9.212111	-6.456952	3.796339
-9.001497	0.298578	3.806336
-8.143064	0.972635	3.816333
-7.763647	-0.568972	3.826330
-7.512914	3.826715	3.836326
-6.375157	-3.636183	3.846323
-6.244660	-5.908784	3.856320
-5.902214	-7.729726	3.866317
-5.220947	-0.889090	3.876314
-4.864740	1.095396	3.886310
-4.116715	5.939494	3.896307
-3.869940	12.467660	3.906304
-3.855283	8.461356	3.916301
-3.376786	24.602260	3.926298
-2.492960	44.696721	3.936294
-2.161204	49.466264	3.946291
-1.794145	63.869646	3.956288
-1.085692	80.301072	3.966285
-0.594988	94.571190	3.976282
-0.317086	102.789270	3.986278
0.000000	117.446052	3.991283
0.251964	125.936045	3.996288
0.593721	126.252959	4.001293
1.174514	130.607461	4.006298
0.948531	134.423205	4.011302
0.939666	126.328730	4.016307
1.316476	127.896163	4.021312
1.077829	126.614044	4.026317
1.398214	124.039528	4.031322
0.679894	121.965248	4.036326
0.587889	117.949035	4.041331
0.913539	132.482819	4.046336
1.153381	146.577569	4.051341
1.348602	142.136990	4.056346
1.039703	145.725207	4.061350
0.919726	141.944292	4.066355
0.696713	146.892171	4.071360
0.831293	147.598837	4.076365
1.348982	145.313130	4.081370
0.982795	152.488382	4.086374
1.148486	147.324754	4.091379
0.872702	148.323096	4.096384
0.906894	141.749964	4.101389
0.908514	143.540325	4.106394
1.140663	149.451858	4.111398
1.154680	154.087595	4.116403
1.282282	163.179085	4.121408
1.379420	166.134627	4.126413
1.650639	163.757581	4.131418
1.252384	161.143093	4.136422
1.258407	151.771328	4.141427
1.564598	152.944808	4.146432
0.949712	154.625518	4.151437
1.297716	153.808864	4.156442
1.359144	172.044189	4.161446
1.663783	166.036366	4.166451
1.289663	158.650463	4.171456
1.280831	166.772966	4.176461
1.834920	165.187089	4.181466
1.486538	160.960853	4.186470
1.608160	145.373455	4.191475
1.281389	151.065134	4.196480
1.292796	153.638563	4.201485
1.498422	166.526969	4.206490
1.673200	160.760825	4.211494
1.533934	150.345523	4.216499
1.612999	150.877339	4.221504
1.438396	150.711514	4.226509
1.470780	144.325320	4.231514
1.521663	159.224600	4.236518
1.597898	169.273193	4.241523
1.801828	154.270906	4.246528
1.515796	155.622012	4.251533
1.500010	160.297191	4.256538
1.681600	167.478909	4.261542
1.763034	160.272007	4.266547
1.804326	155.570660	4.271552
1.373820	150.819388	4.276557
1.982664	156.928532	4.281562
1.670507	161.032939	4.286566
1.675050	152.477631	4.291571
1.684398	154.023187	4.296576
1.465172	156.752744	4.301581
1.853374	158.679064	4.306586
1.811791	161.380964	4.311590
1.780830	167.909258	4.316595
1.669608	174.041936	4.321600
1.806696	164.377681	4.326605
1.840025	163.388564	4.331610
2.065264	175.407076	4.336614
1.619026	160.765435	4.341619
1.896964	161.022684	4.346624
1.783550	173.252106	4.351629
2.028073	168.129981	4.356634
1.821614	165.251519	4.361638
2.093986	159.928913	4.366643
1.901222	157.943639	4.371648
1.597095	153.485893	4.376653
2.032206	157.587845	4.381658
2.050304	167.132973	4.386662
1.787211	167.389040	4.391667
2.097507	165.281150	4.396672
2.245797	168.567241	4.401677
2.307945	156.652630	4.406682
1.826927	154.573036	4.411686
1.362459	143.822402	4.416691
1.751875	153.391965	4.421696
1.638083	162.093942	4.426701
2.125524	160.527933	4.431706
1.743183	173.223158	4.436710
1.820975	174.802350	4.441715
2.026824	168.177173	4.446720
1.843736	166.766181	4.451725
1.956524	164.132235	4.456730
2.028458	166.069834	4.461734
2.097502	162.860583	4.466739
2.443806	161.591788	4.471744
2.150800	179.888633	4.476749
2.095086	168.640918	4.481754
1.983878	175.602478	4.486758
2.051531	164.889202	4.491763
2.110773	170.141146	4.496768
2.166845	175.305002	4.501773
2.302613	189.064822	4.506778
2.809193	188.008347	4.511782
2.571950	167.845176	4.516787
2.405029	162.597292	4.521792
1.971372	166.502324	4.526797
2.158944	162.363480	4.531802
2.171869	176.041178	4.536806
1.913890	165.853153	4.541811
2.169548	181.742436	4.546816
2.709783	180.228316	4.551821
2.832754	180.585622	4.556826
2.448061	182.983450	4.561830
2.103271	173.071522	4.566835
2.390595	171.486051	4.571840
2.250857	175.724964	4.576845
2.858071	178.243595	4.581850
2.570385	168.113976	4.586854
2.820509	173.434276	4.591859
2.718790	165.060018	4.596864
2.279565	169.386686	4.601869
2.517382	160.750763	4.606874
2.719476	162.278964	4.611878
2.397342	166.622201	4.616883
2.429422	173.058426	4.621888
2.281707	171.610290	4.626893
2.584568	162.948420	4.631898
2.706700	170.341872	4.636902
2.557396	166.714210	4.641907
2.919220	172.333486	4.646912
2.378192	169.636824	4.651917
2.672384	169.100625	4.656922
2.206251	168.318982	4.661926
2.525558	162.761282	4.666931
2.770476	172.492555	4.671936
2.227754	172.542229	4.676941
2.658505	178.938530	4.681946
2.779076	178.954533	4.686950
2.678479	192.548681	4.691955
3.103788	193.760564	4.696960
2.709842	181.451887	4.701965
3.073127	162.077890	4.706970
2.859756	159.308070	4.711974
2.861891	168.425424	4.716979
2.563630	167.446806	4.721984
2.752742	153.370620	4.726989
2.681872	163.650916	4.731994
2.495705	171.826342	4.736998
3.180537	178.312794	4.742003
3.248412	173.370028	4.747008
2.952012	173.811610	4.752013
2.685674	167.911668	4.757018
2.508163	168.416996	4.762022
2.624247	167.335901	4.767027
2.908362	182.024885	4.772032
2.868831	189.620681	4.777037
3.185606	190.631168	4.782042
3.307108	192.855274	4.787046
3.077280	190.644819	4.792051
2.511993	175.183326	4.797056
2.734585	189.926187	4.802061
3.062289	184.933471	4.807066
2.950029	193.999049	4.812070
2.735201	196.927239	4.817075
3.162460	191.669091	4.822080
2.827949	190.980847	4.827085
3.220906	189.831334	4.832090
3.228199	200.630979	4.837094
2.973719	192.868938	4.842099
3.184806	187.555865	4.847104
3.073014	196.969376	4.852109
3.202771	187.182866	4.857114
2.955007	195.987975	4.862118
2.879571	188.830795	4.867123
3.178020	186.209067	4.872128
3.236757	195.257512	4.877133
3.366483	185.104022	4.882138
3.135240	187.651962	4.887142
3.357156	191.106924	4.892147
3.538277	188.943214	4.897152
3.118304	181.760588	4.902157
3.300178	186.019031	4.907162
2.813876	192.358806	4.912166
2.836142	196.569337	4.917171
3.149642	192.771539	4.922176
3.102353	193.386303	4.927181
3.291203	194.192086	4.932186
3.287467	196.195252	4.937190
3.242514	201.137569	4.942195
3.213086	199.240753	4.947200
3.071086	205.004919	4.952205
3.306930	187.460363	4.957210
3.174705	195.529327	4.962214
3.151963	207.902839	4.967219
3.481439	205.795122	4.972224
3.404669	218.445966	4.977229
3.658049	220.469213	4.982234
3.307676	206.720585	4.987238
3.473393	218.438353	4.992243
3.756747	211.510034	4.997248
3.234092	206.345996	5.002253
3.565967	209.726896	5.007258
3.504575	200.621859	5.012262
3.552475	213.987264	5.017267
3.427269	208.017879	5.022272
3.277585	221.221068	5.027277
3.198296	210.840684	5.032282
3.303372	222.346438	5.037286
3.184424	215.003037	5.042291
3.310611	207.428488	5.047296
2.859453	220.833635	5.052301
3.266314	221.017031	5.057306
3.577846	232.300826	5.062310
3.560793	230.509645	5.067315
3.373992	236.524401	5.072320
4.155343	229.325553	5.077325
4.016428	229.989385	5.082330
3.710568	227.278245	5.087334
3.306549	226.325581	5.092339
3.739183	224.891483	5.097344
3.924582	237.099734	5.102349
3.548386	232.355803	5.107354
3.647668	239.594657	5.112358
3.550328	230.817898	5.117363
3.933118	241.647688	5.122368
3.704631	241.037845	5.127373
3.812551	238.714687	5.132378
3.921564	239.991638	5.137382
3.826750	248.874196	5.142387
4.121638	237.309265	5.147392
3.858795	237.913300	5.152397
3.847967	225.817019	5.157402
3.927180	232.910302	5.162406
3.722607	230.756020	5.167411
4.258237	234.174801	5.172416
3.772711	234.459173	5.177421
4.106964	238.228841	5.182426
3.857878	238.533347	5.187430
3.758573	238.400090	5.192435
3.882292	231.904733	5.197440
3.834916	230.978796	5.202445
3.767932	228.344357	5.207450
3.861553	236.833747	5.212454
3.592940	235.910619	5.217459
4.033258	233.035847	5.222464
3.839529	240.475342	5.227469
3.850228	239.964297	5.232474
4.177439	238.103696	5.237478
3.724681	234.349264	5.242483
3.868817	237.161462	5.247488
4.035702	249.543443	5.252493
4.394593	252.034311	5.257498
4.063548	250.193941	5.262502
4.126379	251.911508	5.267507
4.477645	246.298188	5.272512
3.892165	253.428531	5.277517
3.988716	245.988291	5.282522
4.250268	258.668745	5.287526
4.416290	258.421412	5.292531
4.511010	251.857797	5.297536
4.163337	253.490585	5.302541
4.064942	236.108749	5.307546
3.845233	240.869483	5.312550
4.209030	256.045984	5.317555
4.451799	257.653281	5.322560
4.064581	269.593211	5.327565
4.510634	258.678597	5.332570
4.397060	264.799018	5.337574
4.734716	263.050681	5.342579
4.244287	253.854232	5.347584
4.314521	262.407386	5.352589
4.275081	266.608558	5.357594
4.520070	263.988815	5.362598
4.210628	261.581943	5.367603
4.263974	261.915290	5.372608
4.379019	257.983865	5.377613
4.482538	258.679553	5.382618
4.601296	253.750988	5.387622
4.233064	258.787946	5.392627
4.597934	251.679243	5.397632
4.776023	269.295403	5.402637
4.760700	260.616589	5.407642
4.438456	254.459572	5.412646
4.593152	255.008089	5.417651
4.765265	245.793908	5.422656
3.965382	246.326537	5.427661
4.692470	253.167099	5.432666
4.249955	261.062945	5.437670
4.343857	273.064008	5.442675
4.394455	260.679736	5.447680
4.166513	260.477923	5.452685
4.315990	256.250077	5.457690
4.530685	247.579748	5.462694
4.522097	259.501849	5.467699
4.540320	256.154964	5.472704
4.202002	259.004317	5.477709
4.714268	265.014642	5.482714
5.219448	286.483890	5.487718
4.904998	265.807456	5.492723
4.814038	255.840142	5.497728
4.692451	262.986846	5.502733
4.582011	256.410881	5.507738
4.499829	255.028463	5.512742
4.744826	259.894015	5.517747
4.727679	250.149326	5.522752
4.716232	265.216584	5.527757
4.737720	274.410072	5.532762
4.936463	273.218027	5.537766
4.599571	277.500315	5.542771
5.049977	274.595492	5.547776
4.989974	284.994386	5.552781
4.631890	274.878830	5.557786
4.661924	265.481121	5.562790
4.783323	284.839826	5.567795
4.846196	278.546911	5.572800
4.731522	287.508510	5.577805
5.110536	283.611909	5.582810
4.961551	284.270983	5.587814
4.707612	285.923980	5.592819
4.821448	284.624934	5.597824
4.789555	286.588202	5.602829
4.746246	276.885536	5.607834
4.596389	281.217796	5.612838
5.104778	285.555137	5.617843
5.259095	283.648686	5.622848
4.767284	299.499432	5.627853
4.791899	290.225937	5.632858
4.657317	286.292244	5.637862
4.996508	300.972751	5.642867
5.549279	300.114718	5.647872
4.943593	298.370887	5.652877
5.036078	288.991914	5.657882
5.344508	306.698547	5.662886
5.366234	307.274096	5.667891
5.219104	289.010797	5.672896
4.702699	294.694083	5.677901
4.872290	304.880075	5.682906
5.464410	305.034628	5.687910
5.320830	310.738964	5.692915
5.679212	305.039097	5.697920
5.019354	303.642215	5.702925
5.177110	291.858158	5.707930
5.458334	301.409846	5.712934
5.165657	298.468857	5.717939
5.165097	295.191326	5.722944
5.663141	310.365955	5.727949
5.319728	303.687043	5.732954
5.383225	294.432802	5.737958
5.189256	298.278397	5.742963
5.113092	291.073834	5.747968
5.316290	300.685125	5.752973
5.483852	303.145679	5.757978
5.712393	304.926035	5.762982
5.106329	296.864353	5.767987
5.283529	298.690666	5.772992
5.210224	309.123282	5.777997
5.605368	312.181144	5.783002
5.487336	315.002536	5.788006
5.530228	312.243412	5.793011
5.504369	310.494722	5.798016
5.566277	320.915784	5.803021
5.630673	308.149685	5.808026
5.357281	300.706911	5.813030
5.378081	314.706187	5.818035
5.851504	304.983163	5.823040
5.995801	304.476625	5.828045
5.302657	297.867985	5.833050
5.546593	289.857459	5.838054
5.004817	294.643042	5.843059
5.382687	297.963014	5.848064
5.580107	316.129858	5.853069
5.388976	309.373450	5.858074
5.753288	317.526509	5.863078
5.451425	314.741969	5.868083
5.563691	307.372022	5.873088
5.428840	312.761794	5.878093
5.318979	313.383140	5.883098
5.726606	314.401635	5.888102
5.522587	314.563086	5.893107
5.496907	311.384375	5.898112
5.567446	307.330157	5.903117
5.785271	303.974331	5.908122
5.852414	305.425482	5.913126
5.549632	311.122968	5.918131
6.254686	315.543590	5.923136
5.784349	315.439627	5.928141
5.597500	317.686448	5.933146
5.574986	318.246740	5.938150
5.750880	331.899184	5.943155
5.973072	332.880114	5.948160
5.971333	342.244929	5.953165
5.919590	331.410940	5.958170
5.757636	326.295110	5.963174
5.523528	344.206471	5.968179
6.014247	334.177022	5.973184
5.965258	340.761970	5.978189
6.004100	334.105786	5.983194
6.222957	336.827273	5.988198
6.184947	339.025615	5.993203
5.980644	321.755096	5.998208
5.769841	322.841405	6.003213
5.771320	323.413780	6.008218
6.419835	329.491497	6.013222
5.918241	331.901219	6.018227
5.854607	323.634850	6.023232
5.691085	323.799487	6.028237
6.096761	329.791630	6.033242
5.903169	323.241241	6.038246
5.858416	328.639135	6.043251
6.394373	336.129574	6.048256
5.904238	313.908075	6.053261
5.791008	316.124452	6.058266
5.938867	311.922155	6.063270
6.033614	313.663232	6.068275
5.885573	309.219110	6.073280
5.954264	315.504156	6.078285
5.998056	313.516835	6.083290
5.913444	307.566406	6.088294
6.013985	320.003057	6.093299
6.222531	307.135423	6.098304
5.435500	317.524148	6.103309
5.959804	323.247885	6.108314
6.426142	326.626854	6.113318
5.729101	327.595883	6.118323
5.773484	304.500247	6.123328
5.614708	324.740999	6.128333
5.719342	330.061852	6.133338
5.941844	332.779607	6.138342
5.703708	342.893063	6.143347
5.950561	329.905555	6.148352
6.017553	338.516197	6.153357
6.113455	335.805762	6.158362
5.978562	336.563883	6.163366
5.704258	342.301237	6.168371
6.057398	340.015816	6.173376
5.984748	329.425524	6.178381
6.139823	325.361303	6.183386
5.889474	337.400190	6.188390
5.676571	339.258771	6.193395
6.228852	335.743300	6.198400
5.948589	338.827232	6.203405
5.668257	329.408210	6.208410
5.976693	332.748490	6.213414
5.981937	339.505324	6.218419
5.949674	334.922948	6.223424
6.155307	340.095203	6.228429
6.122647	338.018544	6.233434
5.784326	340.440810	6.238438
5.963354	342.039056	6.243443
6.057953	339.575592	6.248448
5.881206	342.190998	6.253453
5.931088	332.951511	6.258458
5.851396	337.089366	6.263462
5.984004	339.817955	6.268467
5.907185	328.351966	6.273472
5.966319	330.392814	6.278477
5.982776	337.008699	6.283482
6.318177	337.845454	6.288486
5.892506	346.760592	6.293491
5.932146	328.436536	6.298496
5.954889	328.692394	6.303501
5.713366	326.509052	6.308506
5.707955	326.076441	6.313510
5.728568	338.734355	6.318515
5.904275	334.761831	6.323520
5.959720	338.182631	6.328525
5.894800	337.202473	6.333530
6.024163	338.922345	6.338534
5.983095	338.662962	6.343539
6.011785	334.096406	6.348544
6.167112	334.243037	6.353549
6.099892	345.149283	6.358554
6.282195	334.841990	6.363558
5.869249	337.161981	6.368563
6.116445	334.418500	6.373568
6.172866	332.672816	6.378573
6.208337	341.329495	6.383578
5.932129	334.374356	6.388582
5.982205	341.247595	6.393587
6.229981	331.344556	6.398592
6.238960	328.059207	6.403597
5.867968	313.111499	6.408602
5.795436	312.784251	6.413606
5.667969	321.191047	6.418611
6.129161	331.432892	6.423616
6.060626	329.111886	6.428621
5.937329	328.533117	6.433626
5.778020	325.413174	6.438630
5.530057	326.467304	6.443635
6.246230	335.005343	6.448640
6.114404	333.058017	6.453645
6.301901	337.647810	6.458650
6.030474	316.202165	6.463654
5.479734	317.698899	6.468659
5.961964	328.934033	6.473664
6.123830	328.858186	6.478669
6.087055	335.014129	6.483674
6.018251	322.730660	6.488678
6.088274	316.066465	6.493683
5.839961	309.676459	6.498688
5.971822	311.541469	6.503693
5.544394	315.186139	6.508698
6.222733	321.183282	6.513702
6.154986	335.500076	6.518707
5.860300	320.290549	6.523712
6.018436	318.032328	6.528717
5.708740	321.057566	6.533722
6.003747	329.401752	6.538726
6.047707	333.507699	6.543731
5.942675	327.041595	6.548736
5.978661	322.024660	6.553741
6.176086	323.898446	6.558746
6.233914	324.053929	6.563750
5.859098	318.468215	6.568755
5.976814	306.627108	6.573760
6.337860	311.243656	6.578765
5.503907	322.693201	6.583770
5.621653	312.718671	6.588774
5.649401	320.534997	6.593779
6.143190	332.651007	6.598784
6.293924	337.698934	6.603789
6.268059	332.318308	6.608794
6.051867	316.754882	6.613798
5.729193	321.310209	6.618803
5.589382	317.548163	6.623808
5.699929	322.830128	6.628813
5.967080	331.602589	6.633818
6.221719	333.043531	6.638822
5.946393	335.895744	6.643827
5.758628	326.690097	6.648832
6.046659	332.058326	6.653837
5.751191	341.339161	6.658842
6.392610	339.325227	6.663846
5.836546	331.325346	6.668851
5.699988	322.557812	6.673856
5.971499	339.536246	6.678861
5.823718	344.858439	6.683866
6.232474	338.049749	6.688870
5.913200	341.589002	6.693875
6.062119	332.694758	6.698880
6.049635	329.909452	6.703885
5.694564	325.333047	6.708890
6.008771	327.416437	6.713894
5.898564	330.872517	6.718899
6.277076	329.484803	6.723904
5.987852	316.419421	6.728909
5.592338	328.661234	6.733914
5.991179	329.253997	6.738918
6.031496	339.574030	6.743923
6.239415	344.246065	6.748928
6.028120	326.603313	6.753933
5.695560	321.359025	6.758938
5.910350	318.073271	6.763942
6.036672	327.588981	6.768947
6.032779	319.835323	6.773952
5.756407	329.923088	6.778957
5.970679	335.173089	6.783962
5.992625	335.951082	6.788966
5.971888	331.243528	6.793971
5.933748	334.343544	6.798976
6.057403	338.481376	6.803981
5.832121	339.168150	6.808986
6.100598	326.218406	6.813990
5.634668	330.156971	6.818995
6.107548	333.522267	6.824000
6.424143	338.544370	6.829005
5.980739	330.855974	6.834010
5.367345	324.595570	6.839014
5.488057	334.618349	6.844019
5.752890	336.026067	6.849024
6.161607	339.151422	6.854029
6.096946	346.868255	6.859034
6.239930	345.558338	6.864038
5.957983	339.796808	6.869043
6.126261	343.611323	6.874048
6.444651	340.116448	6.879053
6.020696	336.813084	6.884058
6.033061	310.685268	6.889062
5.707315	317.740396	6.894067
5.554670	313.720925	6.899072
5.883645	322.265460	6.904077
5.950534	336.653040	6.909082
6.252449	341.038361	6.914086
5.821614	332.639337	6.919091
6.173601	335.874763	6.924096
6.227495	329.754067	6.929101
5.773429	319.605974	6.934106
6.333703	322.603327	6.939110
5.751308	312.411945	6.944115
5.786511	317.746768	6.949120
5.884043	312.631669	6.954125
5.639595	316.940701	6.959130
6.076560	328.923189	6.964134
6.149511	342.759346	6.969139
6.054642	339.322487	6.974144
6.154797	328.961551	6.979149
5.582854	323.580530	6.984154
5.884831	327.624157	6.989158
5.748324	339.110654	6.994163
5.987194	338.235055	6.999168
5.807641	342.388459	7.004173
6.081515	346.072640	7.009178
6.016962	351.214200	7.014182
6.133220	342.075104	7.019187
5.882798	341.832498	7.024192
5.634535	333.414540	7.029197
6.070510	349.949769	7.034202
6.005982	343.686157	7.039206
6.083855	348.318330	7.044211
5.978294	337.552826	7.049216
6.144664	338.327315	7.054221
5.745858	338.724735	7.059226
5.820721	343.591490	7.064230
5.699238	353.101503	7.069235
6.054001	348.212096	7.074240
6.472424	345.856399	7.079245
5.863252	336.077290	7.084250
5.810258	335.028838	7.089254
5.900715	341.063735	7.094259
5.935646	344.585805	7.099264
5.926231	342.091080	7.104269
5.934452	342.463092	7.109274
6.080169	338.261123	7.114278
5.960317	338.292413	7.119283
6.275173	341.008445	7.124288
6.249721	328.588510	7.129293
5.882171	328.183810	7.134298
5.893267	323.879419	7.139302
5.609543	322.528375	7.144307
5.780496	332.135212	7.149312
6.217082	336.948810	7.154317
6.015368	344.285190	7.159322
5.879195	327.247664	7.164326
5.919552	339.415293	7.169331
6.000903	343.521748	7.174336
6.472492	338.114289	7.179341
5.884106	329.831544	7.184346
6.161650	318.462247	7.189350
5.521189	326.265556	7.194355
5.754881	331.028486	7.199360
5.922074	329.727456	7.204365
5.752033	337.571422	7.209370
6.012544	345.481231	7.214374
5.984917	352.625997	7.219379
6.220462	350.257644	7.224384
5.980763	336.925112	7.229389
5.249098	329.790955	7.234394
5.991267	337.546676	7.239398
6.054114	347.591127	7.244403
6.137835	342.244055	7.249408
5.940390	343.397887	7.254413
5.893339	353.820115	7.259418
5.852175	347.325077	7.264422
6.059063	345.701495	7.269427
5.940406	343.559132	7.274432
5.889697	338.584164	7.279437
5.838810	349.608090	7.284442
5.871737	342.566852	7.289446
5.774267	343.904432	7.294451
5.590436	348.900050	7.299456
5.880432	337.696478	7.304461
6.033495	350.298977	7.309466
6.087897	342.090151	7.314470
5.798858	350.085525	7.319475
5.978490	351.547638	7.324480
6.176133	349.343373	7.329485
5.941639	355.599709	7.334490
6.254934	349.865720	7.339494
5.500673	348.496187	7.344499
5.769838	348.738987	7.349504
5.794985	348.472459	7.354509
5.486425	351.798077	7.359514
5.929971	339.691085	7.364518
5.844929	357.528633	7.369523
5.691755	358.422476	7.374528
6.094641	353.712234	7.379533
5.425300	354.563057	7.384538
5.984429	364.134784	7.389542
6.108944	368.266162	7.394547
6.065603	365.697623	7.399552
6.081590	358.681162	7.404557
5.808819	354.923991	7.409562
6.200907	350.167975	7.414566
5.898096	352.277834	7.419571
6.029930	351.842837	7.424576
6.011842	349.336807	7.429581
5.646023	347.185470	7.434586
5.927563	350.963369	7.439590
5.801943	358.246779	7.444595
6.226890	365.982301	7.449600
6.341854	359.431313	7.454605
5.999770	351.806226	7.459610
6.326834	342.748202	7.464614
6.036051	351.015927	7.469619
6.268698	356.585772	7.474624
6.432817	346.006062	7.479629
6.459851	346.036628	7.484634
6.425123	348.313552	7.489638
5.906804	339.390315	7.494643
6.027953	326.896937	7.499648
6.021279	329.204291	7.504653
5.792061	327.050671	7.509658
5.907578	330.107781	7.514662
5.883498	333.585253	7.519667
6.270873	344.683307	7.524672
6.162028	326.129275	7.529677
6.019060	327.825109	7.534682
6.046958	320.556876	7.539686
5.803211	337.175777	7.544691
5.486544	327.360622	7.549696
5.602328	329.452761	7.554701
6.045421	347.179596	7.559706
6.191166	345.277636	7.564710
6.238018	341.885149	7.569715
5.980239	345.427483	7.574720
6.113696	331.245929	7.579725
5.846559	331.433026	7.584730
6.120057	319.583475	7.589734
5.931646	326.240743	7.594739
5.516677	318.895933	7.599744
5.995556	328.904072	7.604749
5.684994	341.803373	7.609754
5.881758	344.784561	7.614758
5.885646	339.896003	7.619763
5.702115	347.292827	7.624768
5.940764	341.073761	7.629773
5.787984	349.535130	7.634778
6.010365	348.209688	7.639782
5.992654	352.236658	7.644787
6.023723	348.482800	7.649792
6.300861	348.208675	7.654797
6.294256	354.236543	7.659802
5.975582	346.288279	7.664806
6.152363	339.955461	7.669811
5.739123	336.650428	7.674816
5.592998	344.873481	7.679821
5.677738	350.342968	7.684826
6.335174	357.007756	7.689830
6.344892	340.029760	7.694835
5.846474	349.588967	7.699840
6.352056	340.689808	7.704845
5.788187	344.871412	7.709850
5.552185	336.574927	7.714854
5.848104	336.664868	7.719859
6.148281	349.238134	7.724864
6.262207	348.834398	7.729869
6.052922	331.884180	7.734874
6.051094	322.358526	7.739878
5.737086	328.007146	7.744883
5.847246	326.778270	7.749888
6.223737	330.503418	7.754893
6.017225	341.434512	7.759898
6.017732	320.379951	7.764902
5.970195	330.489034	7.769907
5.962250	331.910749	7.774912
6.414448	321.570934	7.779917
6.051016	327.929592	7.784922
5.959119	324.549220	7.789926
6.051970	332.225703	7.794931
6.098158	321.376472	7.799936
6.079428	323.581300	7.804941
5.702634	333.096253	7.809946
6.025861	323.782576	7.814950
5.649151	329.485251	7.819955
5.574724	326.519767	7.824960
5.696766	320.382138	7.829965
5.727266	330.409469	7.834970
5.929545	336.718015	7.839974
6.336508	349.995981	7.844979
6.165318	338.709191	7.849984
6.500919	326.505122	7.854989
5.957279	331.154965	7.859994
5.933780	325.543023	7.864998
5.890395	328.419232	7.870003
5.743065	327.053279	7.875008
6.116147	323.024717	7.880013
5.844264	330.134738	7.885018
5.910756	324.746063	7.890022
5.777890	323.808122	7.895027
6.023610	321.444517	7.900032
6.090550	305.302353	7.905037
5.953929	324.302648	7.910042
6.000324	326.753597	7.915046
5.952576	319.070043	7.920051
5.956185	324.596445	7.925056
6.084946	320.662871	7.930061
5.946245	323.895600	7.935066
6.273136	317.539418	7.940070
5.760851	318.191784	7.945075
5.622134	319.956556	7.950080
6.209022	329.292992	7.955085
5.943911	326.929828	7.960090
6.033660	318.525687	7.965094
5.860216	311.747543	7.970099
6.096222	317.883155	7.975104
6.175456	320.651688	7.980109
5.677267	330.182376	7.985114
5.437741	320.576674	7.990118
5.699276	315.938552	7.995136
5.493296	319.776289	8.000154
6.067296	335.840584	8.005171
6.196016	352.501213	8.010189
5.602338	350.343650	8.015206
6.328510	348.460250	8.020224
6.146859	352.799108	8.025242
6.302335	346.081768	8.030259
5.574703	333.133855	8.035277
5.862240	328.813177	8.040294
6.142454	340.208700	8.045312
5.878208	356.065871	8.050330
6.036892	358.963261	8.055347
6.118266	356.397654	8.060365
5.859539	354.591863	8.065382
6.133776	356.994760	8.070400
6.010502	353.580592	8.075418
6.636285	359.693432	8.080435
5.844198	353.186734	8.085453
6.047024	332.772874	8.090470
6.143699	329.741010	8.095488
5.840354	326.550534	8.100506
6.255149	333.806998	8.105523
6.051758	335.672063	8.110541
5.860010	336.481334	8.115558
6.273511	342.264321	8.120576
6.056765	352.888361	8.125594
5.924381	333.284044	8.130611
6.079319	345.809859	8.135629
6.106663	351.706618	8.140646
6.533495	350.920651	8.145664
5.896573	342.493260	8.150682
6.203429	335.869114	8.155699
6.075427	338.277833	8.160717
6.110720	347.512017	8.165734
6.368968	349.835355	8.170752
5.985892	347.733362	8.175770
5.705627	349.036071	8.180787
5.915048	361.383010	8.185805
6.049888	355.972159	8.190822
6.351689	350.910835	8.195840
6.410713	363.549421	8.200858
6.522809	356.819897	8.205875
6.505925	352.644435	8.210893
6.325035	350.116507	8.215910
6.365557	333.290631	8.220928
6.345370	333.584067	8.225946
6.456146	328.211682	8.230963
6.019323	339.135052	8.235981
5.842342	330.714947	8.240998
5.917985	325.291232	8.246016
5.837923	333.341072	8.251034
6.086086	343.223727	8.256051
6.168626	352.217039	8.261069
6.132506	352.317306	8.266086
6.136763	355.873023	8.271104
5.954833	349.867743	8.276122
5.955629	346.453194	8.281139
5.679729	353.558442	8.286157
5.705878	353.084155	8.291174
6.282281	357.289210	8.296192
5.867382	363.904890	8.301210
6.116013	370.073299	8.306227
6.303063	379.716194	8.311245
5.986098	378.758869	8.316262
6.388732	381.911755	8.321280
6.194686	393.299106	8.326298
6.782357	379.032429	8.331315
6.435229	377.060527	8.336333
6.610794	378.254401	8.341350
6.336757	365.175884	8.346368
6.404395	364.221791	8.351386
6.781428	356.169828	8.356403
6.110790	356.611871	8.361421
5.818725	351.807103	8.366438
6.306481	360.614259	8.371456
5.990245	372.945224	8.376474
6.331710	376.397952	8.381491
6.413691	375.823458	8.386509
6.182356	374.802310	8.391526
6.335023	379.048100	8.396544
5.856403	381.448302	8.401562
6.351326	378.486961	8.406579
6.408484	377.547122	8.411597
6.219126	380.628085	8.416614
6.102010	378.790776	8.421632
5.921954	382.716004	8.426650
5.931089	368.179668	8.431667
6.253377	387.757561	8.436685
6.740348	400.275898	8.441702
6.824161	397.962357	8.446720
6.476209	392.506748	8.451738
6.473245	387.420285	8.456755
6.619934	381.180802	8.461773
6.431506	387.530869	8.466790
6.223377	374.934364	8.471808
6.068226	380.774344	8.476826
6.226280	393.694163	8.481843
6.633541	406.830799	8.486861
6.152218	411.216329	8.491878
6.733077	412.924585	8.496896
6.736291	408.947942	8.501914
6.541748	407.864263	8.506931
6.561068	399.886909	8.511949
6.307246	401.093991	8.516966
6.671639	395.451737	8.521984
6.590003	402.160704	8.527002
6.665691	401.350515	8.532019
6.562410	393.426965	8.537037
6.104721	392.223319	8.542054
6.737787	388.688230	8.547072
6.499731	403.458980	8.552090
6.635631	403.194810	8.557107
6.779412	401.701867	8.562125
6.480438	394.468315	8.567143
6.573642	382.563309	8.572160
6.446469	393.571038	8.577178
6.569861	395.240071	8.582195
6.664974	394.051337	8.587213
6.623152	405.768427	8.592231
6.811651	394.987765	8.597248
6.278923	392.754440	8.602266
6.509541	387.287643	8.607283
6.735623	403.503993	8.612301
6.600771	403.796349	8.617319
6.753623	400.405450	8.622336
6.445950	402.447697	8.627354
6.601065	401.369534	8.632371
6.674809	397.394535	8.637389
6.661001	405.446715	8.642407
6.854775	405.918267	8.647424
6.510255	412.620833	8.652442
6.752622	406.953395	8.657459
6.826852	398.585659	8.662477
7.122112	411.095984	8.667495
6.859462	391.272055	8.672512
6.799761	387.879540	8.677530
6.199906	391.876442	8.682547
6.634223	377.403281	8.687565
6.379565	386.692096	8.692583
6.926082	392.539592	8.697600
7.026961	408.245292	8.702618
7.164054	398.756980	8.707635
6.787719	381.885513	8.712653
6.624912	380.594933	8.717671
6.485733	369.022748	8.722688
6.620817	382.144940	8.727706
6.277329	374.602762	8.732723
6.740165	393.499250	8.737741
6.978053	399.353777	8.742759
6.820415	402.685413	8.747776
6.855252	407.274586	8.752794
6.602438	393.640506	8.757811
6.890162	393.652484	8.762829
6.695266	400.328594	8.767847
6.990678	394.154309	8.772864
6.678964	401.498670	8.777882
6.870198	413.674917	8.782899
6.936705	409.641084	8.787917
6.897947	395.566596	8.792935
6.573731	383.461506	8.797952
6.755190	391.035176	8.802970
6.810967	405.681287	8.807987
7.056170	402.465348	8.813005
6.774977	405.835155	8.818023
7.059627	400.025444	8.823040
6.791539	394.497443	8.828058
6.761030	399.191458	8.833075
7.040369	397.377623	8.838093
6.803548	398.777708	8.843111
6.819582	396.518899	8.848128
6.870690	397.419743	8.853146
6.898795	399.444422	8.858163
7.342623	402.713969	8.863181
6.831200	399.328669	8.868199
6.557213	382.302419	8.873216
6.978280	378.087164	8.878234
6.922109	396.060967	8.883251
7.245405	393.536580	8.888269
7.057853	397.705963	8.893287
6.739171	383.722402	8.898304
6.793902	384.644770	8.903322
6.804868	386.321839	8.908339
7.382379	394.730050	8.913357
7.173081	392.806111	8.918375
7.194582	380.681908	8.923392
6.793135	377.487763	8.928410
6.836465	368.083490	8.933427
6.976254	371.368812	8.938445
7.503929	390.753793	8.943463
7.161592	378.768286	8.948480
7.166602	372.481441	8.953498
6.970260	376.917262	8.958515
7.122710	372.620761	8.963533
7.123999	376.555620	8.968551
7.074446	377.872902	8.973568
7.355037	373.771033	8.978586
7.042617	372.696242	8.983603
7.034681	367.509578	8.988621
6.767106	363.947471	8.993639
6.983209	372.550788	8.998656
6.836867	367.824308	9.003674
6.711641	369.595160	9.008691
7.035644	360.311285	9.013709
6.810710	375.553314	9.018727
7.093111	383.433140	9.023744
7.385095	387.963337	9.028762
6.961000	398.218920	9.033779
7.295377	392.126928	9.038797
7.290631	387.826497	9.043815
7.029376	379.318510	9.048832
7.053682	370.772376	9.053850
6.900650	379.212275	9.058867
7.233450	396.150423	9.063885
7.219015	393.915292	9.068903
7.139836	402.763404	9.073920
7.099175	394.205286	9.078938
7.252531	397.286539	9.083955
7.218502	393.631262	9.088973
7.279060	395.723468	9.093991
7.166583	403.200903	9.099008
7.285839	399.890970	9.104026
6.713963	399.222628	9.109043
7.047631	399.890140	9.114061
6.854424	401.264501	9.119079
7.045592	401.389338	9.124096
7.036738	393.548911	9.129114
6.897032	400.342653	9.134131
6.872977	398.967355	9.139149
6.819890	406.284074	9.144167
6.817933	403.886061	9.149184
7.476030	408.428686	9.154202
7.382900	425.515225	9.159219
7.467770	411.897979	9.164237
7.168641	412.238001	9.169255
6.822811	424.551520	9.174272
7.588249	425.363236	9.179290
7.262713	434.918719	9.184307
7.552679	427.669193	9.189325
7.857818	419.783022	9.194343
7.205035	412.932736	9.199360
7.482897	397.190102	9.204378
7.110857	409.558182	9.209395
7.162167	395.949328	9.214413
7.476204	399.974348	9.219431
7.354390	404.111408	9.224448
7.174301	400.620875	9.229466
7.552032	415.541899	9.234483
7.036616	410.311165	9.239501
7.331358	423.859788	9.244519
7.231629	421.227699	9.249536
7.589310	421.320300	9.254554
7.591718	423.017639	9.259571
7.438668	424.865409	9.264589
7.108826	413.322881	9.269607
7.738829	427.033891	9.274624
8.045884	417.882007	9.279642
7.519613	407.856376	9.284659
7.611312	394.900766	9.289677
7.432038	397.046091	9.294695
7.302984	395.358954	9.299712
7.625525	397.552375	9.304730
7.330664	404.531214	9.309747
6.835979	392.891294	9.314765
6.804771	403.899866	9.319783
7.535966	418.481852	9.324800
7.815134	422.143094	9.329818
7.581034	430.494658	9.334835
7.626585	429.259992	9.339853
7.847268	413.743986	9.344871
7.433560	414.979119	9.349888
7.324923	397.463229	9.354906
7.464219	412.635959	9.359923
7.754909	420.397751	9.364941
7.465542	408.694297	9.369959
7.506517	419.388698	9.374976
8.117509	406.364850	9.379994
7.630758	407.065428	9.385011
7.510309	398.854228	9.390029
7.374565	398.790135	9.395047
7.198572	400.786634	9.400064
7.537972	409.228768	9.405082
7.683404	420.250872	9.410099
7.880256	416.919388	9.415117
8.116877	403.726623	9.420135
7.739568	404.829862	9.425152
7.982950	399.272717	9.430170
7.569814	397.011303	9.435187
7.793078	394.502490	9.440205
7.667929	393.338583	9.445223
7.333820	402.298966	9.450240
7.588585	397.913949	9.455258
7.763561	402.213072	9.460275
7.766930	402.414484	9.465293
7.538908	399.464718	9.470311
7.432617	398.417789	9.475328
7.666682	396.746696	9.480346
7.530553	399.163001	9.485363
7.508684	394.483401	9.490381
7.729558	393.975640	9.495399
7.361122	395.929521	9.500416
7.290272	399.872462	9.505434
7.534470	421.109798	9.510451
7.895142	416.288586	9.515469
7.769413	425.904468	9.520487
7.479136	423.289424	9.525504
7.468193	418.557627	9.530522
7.841283	420.320323	9.535539
7.888138	424.812960	9.540557
7.832612	422.259191	9.545575
7.988258	422.686190	9.550592
8.276181	413.969611	9.555610
8.039580	418.345441	9.560627
7.764057	411.013561	9.565645
8.140201	411.156933	9.570663
7.743732	400.994338	9.575680
7.845396	389.056454	9.580698
7.728962	398.033434	9.585715
7.607616	405.509095	9.590733
8.097854	412.567662	9.595751
7.661962	416.706291	9.600768
8.065910	407.192204	9.605786
7.938144	407.417189	9.610803
7.534109	392.724266	9.615821
8.064800	398.599474	9.620839
8.095263	414.502326	9.625856
7.915933	409.919818	9.630874
7.752353	399.058278	9.635891
7.793642	412.545373	9.640909
8.057476	418.020345	9.645927
7.969870	415.294855	9.650944
8.177325	404.864669	9.655962
7.921783	409.079352	9.660979
7.613268	403.611289	9.665997
7.884600	414.181463	9.671015
7.913809	421.479063	9.676032
7.761383	427.208187	9.681050
8.215989	427.733799	9.686067
7.902867	432.121547	9.691085
8.202044	423.122357	9.696103
7.985771	429.375793	9.701120
8.273246	419.630538	9.706138
7.860983	416.905106	9.711155
7.831195	407.332324	9.716173
7.804964	414.581752	9.721191
7.595228	422.509817	9.726208
7.675223	426.978361	9.731226
7.914020	424.605974	9.736243
7.484611	431.596305	9.741261
7.786137	432.003747	9.746279
7.790695	432.391157	9.751296
7.690839	430.655292	9.756314
8.013101	429.560571	9.761331
7.595475	441.408776	9.766349
7.903377	437.829635	9.771367
8.179590	438.424046	9.776384
8.547937	445.615208	9.781402
8.356638	446.803093	9.786419
8.071692	452.972559	9.791437
8.438527	447.156348	9.796455
7.940802	445.438248	9.801472
8.161576	447.054257	9.806490
8.110778	447.655403	9.811507
8.117055	448.878795	9.816525
8.136425	445.931527	9.821543
8.381334	452.924171	9.826560
8.245396	454.744034	9.831578
8.357791	454.044887	9.836595
7.904278	444.052087	9.841613
8.225747	440.054287	9.846631
8.142260	439.350927	9.851648
8.232019	448.870158	9.856666
8.227589	452.272619	9.861683
7.991074	456.478040	9.866701
7.954452	452.450788	9.871719
7.702805	451.653694	9.876736
7.767100	453.540207	9.881754
8.091714	449.664986	9.886771
8.160012	449.102087	9.891789
7.762898	444.076975	9.896807
7.980185	460.787029	9.901824
7.962503	469.748670	9.906842
8.286865	469.584539	9.911859
8.802478	476.550822	9.916877
8.639622	484.544196	9.921895
8.207567	460.915593	9.926912
8.162564	460.398735	9.931930
8.538384	471.451269	9.936947
8.146544	472.121293	9.941965
8.609964	465.280227	9.946983
8.148716	462.205825	9.952000
8.231997	476.560548	9.957018
8.523365	476.127012	9.962035
8.454468	477.232727	9.967053
8.186650	468.596336	9.972071
8.181717	481.768803	9.977088
8.471969	472.026243	9.982106
8.784843	473.037806	9.987123
8.518819	479.406297	9.992141
8.514804	472.789478	9.997159
8.187288	462.789673	10.002176
7.906728	486.690117	10.007194
8.324429	479.168230	10.012211
8.384213	486.442163	10.017229
8.629414	483.661690	10.022247
8.403867	486.874533	10.027264
8.627612	482.121957	10.032282
8.846300	480.216576	10.037299
8.334863	480.700104	10.042317
8.256245	480.516668	10.047335
8.267844	475.371110	10.052352
8.637777	481.100969	10.057370
8.570943	479.148528	10.062387
8.561884	481.551371	10.067405
8.470945	482.070410	10.072423
8.508657	475.996177	10.077440
8.559925	476.578278	10.082458
8.742940	471.639551	10.087475
8.863806	482.211103	10.092493
8.779897	483.205553	10.097511
8.395038	478.459376	10.102528
8.592370	479.725604	10.107546
8.797918	473.751467	10.112563
8.740456	472.933606	10.117581
8.749307	470.720085	10.122599
8.663752	455.128652	10.127616
8.305420	459.526601	10.132634
8.663961	454.910828	10.137651
8.966959	474.820009	10.142669
8.706471	462.420934	10.147687
8.557398	459.092810	10.152704
8.681942	465.514091	10.157722
8.421724	453.004532	10.162739
8.481666	468.296956	10.167757
9.092987	474.711876	10.172775
8.902696	466.830240	10.177792
8.524319	466.005542	10.182810
8.718399	463.302457	10.187827
8.761370	472.144208	10.192845
8.483262	460.574659	10.197863
8.836033	462.798094	10.202880
8.985659	466.504760	10.207898
8.848856	460.221030	10.212915
8.500899	453.913376	10.217933
8.423327	469.590112	10.222951
8.871331	474.133908	10.227968
8.611359	486.778068	10.232986
8.725855	476.106705	10.238003
8.664034	475.242187	10.243021
8.511326	475.549947	10.248039
8.775939	482.463798	10.253056
8.755799	486.935325	10.258074
8.488677	471.135473	10.263091
8.754421	481.129072	10.268109
8.661334	475.258233	10.273127
8.924726	474.781717	10.278144
8.538197	485.343911	10.283162
8.825816	481.938325	10.288179
8.817579	480.986573	10.293197
8.564643	472.720231	10.298215
8.769404	483.707891	10.303232
9.007672	501.632802	10.308250
8.884804	496.549198	10.313267
8.689460	494.070834	10.318285
8.760635	499.080388	10.323303
8.947522	504.567367	10.328320
8.640072	514.707030	10.333338
9.145292	507.837350	10.338355
9.198084	507.936397	10.343373
9.063221	502.261394	10.348391
9.063995	504.233538	10.353408
9.294020	510.218709	10.358426
9.183696	499.067961	10.363443
8.411333	490.705766	10.368461
9.073011	498.141600	10.373479
9.327971	505.981573	10.378496
8.817437	511.280507	10.383514
9.066752	498.991372	10.388531
9.004611	504.965227	10.393549
9.091471	508.315618	10.398567
9.077508	501.716114	10.403584
9.178406	506.913538	10.408602
9.306141	500.755857	10.413619
8.714054	484.709956	10.418637
9.076116	497.206785	10.423655
9.404336	493.176365	10.428672
9.020807	489.616509	10.433690
9.541315	481.668377	10.438707
9.418749	482.176562	10.443725
9.285066	485.895786	10.448743
9.603590	473.687407	10.453760
9.270976	479.438290	10.458778
9.055337	476.511829	10.463795
8.917780	477.722905	10.468813
8.828445	481.873860	10.473831
9.342347	475.166935	10.478848
8.927619	473.947127	10.483866
9.052979	479.162824	10.488883
9.207637	482.423762	10.493901
9.214057	473.530085	10.498919
9.316368	474.618611	10.503936
9.022994	474.986140	10.508954
9.071810	475.129986	10.513971
9.213414	472.864239	10.518989
8.825400	473.145522	10.524007
9.329773	478.658798	10.529024
9.367102	487.883270	10.534042
9.181536	487.006461	10.539059
9.014742	488.982604	10.544077
9.282642	491.673671	10.549095
9.208547	490.138907	10.554112
9.232477	503.291118	10.559130
9.642479	499.418370	10.564147
9.691383	499.385485	10.569165
9.276309	503.984775	10.574183
9.314718	487.752347	10.579200
9.453652	495.316903	10.584218
9.556400	500.233183	10.589235
9.307120	493.417868	10.594253
9.580427	479.095919	10.599271
9.248624	470.614650	10.604288
9.070965	480.427987	10.609306
9.719400	484.432518	10.614323
9.394046	492.119851	10.619341
9.128460	497.396422	10.624359
9.453496	492.681719	10.629376
9.177848	509.105665	10.634394
9.351094	505.111994	10.639411
9.997141	494.872233	10.644429
9.545445	509.663710	10.649447
9.656750	497.680074	10.654464
9.017971	488.457675	10.659482
9.421509	490.029453	10.664499
9.386890	501.660282	10.669517
9.377971	501.216697	10.674535
9.977452	494.982412	10.679552
9.684073	501.983148	10.684570
9.566665	492.389251	10.689587
9.465444	483.335612	10.694605
9.401966	503.311350	10.699623
9.453455	507.086951	10.704640
9.527955	506.516773	10.709658
9.509569	505.557132	10.714675
9.708593	500.877825	10.719693
9.353588	505.243711	10.724711
9.391704	500.923957	10.729728
9.641334	506.814560	10.734746
9.641972	500.294831	10.739763
9.595700	499.964354	10.744781
9.323966	502.149332	10.749799
9.677942	500.254442	10.754816
9.490143	499.355890	10.759834
9.375815	496.426275	10.764851
9.761111	490.455704	10.769869
9.419821	499.663395	10.774887
9.793928	501.750975	10.779904
9.420844	500.168091	10.784922
9.237166	508.341435	10.789939
9.431854	501.431747	10.794957
9.749428	515.062088	10.799975
9.546092	517.665590	10.804992
9.521872	520.679842	10.810010
9.800179	522.649802	10.815027
9.866667	521.219374	10.820045
10.081800	527.923206	10.825063
9.988322	517.918487	10.830080
9.572170	517.831783	10.835098
9.698609	520.251402	10.840115
10.071836	526.236372	10.845133
9.742575	525.706968	10.850151
9.628807	513.319726	10.855168
9.617544	520.771985	10.860186
9.696979	524.865116	10.865203
10.083674	524.006499	10.870221
9.974114	530.347493	10.875239
9.862689	527.808723	10.880256
9.736741	526.531327	10.885274
9.815624	532.158202	10.890291
10.010849	524.175494	10.895309
10.105710	526.271841	10.900327
10.033179	528.233312	10.905344
9.915177	523.246768	10.910362
9.838839	529.828731	10.915379
10.019884	522.207978	10.920397
9.854576	525.698615	10.925415
10.073188	535.917323	10.930432
10.059095	527.654792	10.935450
10.179120	523.240233	10.940467
10.039166	509.149854	10.945485
9.842400	506.734823	10.950503
9.930958	506.048853	10.955520
9.874773	512.933771	10.960538
9.982441	525.110482	10.965555
10.301773	517.913150	10.970573
9.904999	522.459104	10.975591
10.089367	515.244918	10.980608
10.348480	530.812486	10.985626
9.951388	515.474624	10.990643
9.873370	510.027442	10.995661
9.773776	529.352454	11.000679
9.777679	531.478743	11.005696
10.107375	527.277680	11.010714
9.877854	530.099846	11.015731
9.988241	524.440297	11.020749
10.074872	536.585579	11.025767
9.909409	530.126413	11.030784
9.986330	525.570247	11.035802
10.300452	527.297956	11.040819
10.157389	516.862320	11.045837
10.003739	533.586017	11.050855
9.965526	529.319164	11.055872
9.996209	522.984089	11.060890
10.002827	529.297527	11.065907
10.351148	517.343243	11.070925
10.061398	520.932146	11.075943
9.784321	528.242765	11.080960
9.601704	540.275342	11.085978
9.891190	547.245304	11.090995
10.231809	545.993090	11.096013
10.092295	551.969541	11.101031
10.076799	558.482084	11.106048
10.129658	544.768739	11.111066
10.126046	551.238405	11.116083
10.174391	548.905121	11.121101
10.215698	555.945283	11.126119
10.375786	557.750624	11.131136
10.332586	548.498578	11.136154
10.255935	551.432640	11.141171
10.411754	551.304217	11.146189
10.218133	546.657630	11.151207
10.294178	552.190282	11.156224
10.373881	543.566016	11.161242
10.302546	542.065530	11.166259
10.479144	538.850781	11.171277
10.057362	559.213714	11.176295
10.108800	568.006859	11.181312
10.760310	575.059316	11.186330
10.527302	579.724948	11.191347
10.565357	575.102241	11.196365
10.646366	571.132383	11.201383
10.423406	556.770880	11.206400
10.312691	550.886982	11.211418
10.207058	561.986131	11.216435
10.454213	565.560873	11.221453
10.961070	572.525402	11.226471
10.762405	567.494603	11.231488
10.676370	554.569704	11.236506
10.311056	548.772782	11.241523
10.295269	535.777003	11.246541
10.534116	557.463440	11.251559
10.596945	559.290235	11.256576
10.646334	564.915400	11.261594
10.127081	569.051264	11.266611
10.553823	560.126814	11.271629
10.907728	566.928970	11.276647
10.510637	570.610331	11.281664
11.012563	572.261469	11.286682
10.602211	564.420364	11.291699
10.865854	560.453630	11.296717
11.135150	550.313520	11.301735
10.924497	542.753743	11.306752
10.974877	543.831425	11.311770
10.910355	551.787430	11.316787
10.977734	548.362475	11.321805
10.754325	546.652146	11.326823
10.921432	544.467623	11.331840
10.834315	548.883325	11.336858
10.990021	549.408143	11.341875
11.122341	544.341596	11.346893
10.644368	533.027171	11.351911
10.672980	547.078052	11.356928
10.891555	543.907257	11.361946
10.829627	542.187565	11.366963
10.855607	541.195769	11.371981
10.604273	543.825682	11.376999
10.679239	549.166005	11.382016
10.596055	541.226637	11.387034
10.361103	555.122907	11.392051
10.711603	551.208922	11.397069
10.602003	550.575892	11.402087
10.486958	546.728079	11.407104
10.903167	542.627146	11.412122
10.895565	543.183703	11.417139
10.870250	545.611175	11.422157
10.992141	547.722251	11.427175
10.855358	550.801369	11.432192
11.182536	547.578952	11.437210
11.047700	557.237347	11.442227
10.780660	553.233324	11.447245
10.980510	552.034584	11.452263
11.025016	554.814089	11.457280
10.650233	552.351032	11.462298
10.401205	556.567891	11.467315
10.737810	549.023888	11.472333
10.949738	553.162667	11.477351
10.712864	549.744059	11.482368
11.248833	560.683355	11.487386
11.193793	559.934537	11.492403
11.082952	544.899206	11.497421
10.728956	549.378549	11.502439
10.797464	565.067338	11.507456
10.755871	575.042571	11.512474
11.090914	576.609244	11.517491
10.982206	570.772362	11.522509
11.281427	573.666840	11.527527
10.846096	578.162010	11.532544
11.395391	565.229700	11.537562
11.065959	578.714683	11.542579
11.041834	574.272064	11.547597
11.023800	573.037820	11.552615
11.140220	568.993025	11.557632
11.376242	564.913831	11.562650
11.446358	572.899373	11.567667
11.163321	573.104354	11.572685
11.231877	564.974099	11.577703
11.002482	583.356898	11.582720
11.044321	585.486754	11.587738
11.248402	582.450747	11.592755
11.053817	580.802197	11.597773
11.300472	583.881579	11.602791
11.317279	580.931532	11.607808
11.271392	576.624839	11.612826
11.125644	576.473943	11.617843
10.992638	573.067561	11.622861
11.469439	570.683344	11.627879
10.827105	574.541738	11.632896
11.399271	575.071142	11.637914
11.219745	585.834686	11.642931
11.319086	576.194374	11.647949
11.319879	583.471219	11.652967
11.018571	578.967618	11.657984
11.489107	569.878561	11.663002
11.379268	573.783431	11.668019
11.569779	579.080528	11.673037
11.415528	578.621700	11.678055
11.393672	576.908389	11.683072
11.359099	573.912696	11.688090
11.798966	578.713397	11.693107
11.663536	571.817211	11.698125
11.651631	571.146880	11.703143
11.430696	574.106566	11.708160
11.700391	572.786501	11.713178
11.575401	575.788051	11.718195
11.450782	579.758337	11.723213
11.474310	572.130531	11.728231
11.337428	567.497194	11.733248
11.416929	568.683948	11.738266
11.144512	575.006134	11.743283
11.469011	573.510285	11.748301
11.270792	567.157187	11.753319
11.570103	577.565319	11.758336
11.427704	584.394263	11.763354
11.493965	596.457554	11.768371
11.897152	601.308151	11.773389
11.798440	594.286324	11.778407
11.362515	588.642388	11.783424
11.884822	591.429555	11.788442
11.657790	586.917543	11.793459
11.474235	580.091961	11.798477
11.652699	585.971580	11.803495
11.747459	599.598809	11.808512
11.722883	594.989003	11.813530
11.679789	587.661886	11.818547
11.571441	606.966256	11.823565
12.017037	602.447340	11.828583
11.977715	594.415915	11.833600
11.684547	585.385798	11.838618
11.490873	580.202745	11.843635
11.157744	589.967768	11.848653
11.523749	585.824151	11.853671
11.503352	603.420224	11.858688
11.871592	598.869173	11.863706
11.973935	604.811142	11.868723
11.875403	605.766851	11.873741
12.015275	603.977865	11.878759
12.145351	608.104155	11.883776
12.121265	596.744267	11.888794
12.093116	599.494067	11.893811
11.753358	601.355147	11.898829
11.954082	596.271623	11.903847
11.871295	594.378455	11.908864
11.782960	593.319252	11.913882
11.890825	598.051732	11.918899
11.921291	601.338340	11.923917
12.129351	602.744911	11.928935
12.195651	598.057842	11.933952
12.015487	590.433341	11.938970
11.600704	589.951963	11.943987
11.891136	587.981753	11.949005
12.073557	586.164055	11.954023
12.143870	592.473910	11.959040
12.253243	601.882876	11.964058
12.251717	603.110649	11.969075
11.813917	583.260129	11.974093
12.161354	584.193737	11.979111
12.008172	584.375345	11.984128
12.043256	590.182619	11.989146
12.117278	588.220859	11.994163
11.920967	601.562061	11.999181
11.781550	596.013964	12.004199
11.804557	611.870818	12.009216
11.236900	604.016319	12.014234
11.874360	600.919145	12.019251
11.759211	602.833613	12.024269
11.863824	604.022770	12.029287
12.098812	611.632379	12.034304
11.923174	620.817497	12.039322
12.221234	615.135012	12.044339
11.979331	618.776441	12.049357
12.357010	607.319281	12.054375
12.048570	616.433559	12.059392
11.942085	614.487277	12.064410
12.243430	620.186836	12.069427
11.978741	614.257465	12.074445
12.064894	611.116743	12.079463
12.356971	609.919418	12.084480
12.420300	610.319771	12.089498
12.813245	604.026091	12.094515
12.439221	618.417416	12.099533
12.616866	620.380970	12.104551
12.497018	612.242159	12.109568
12.695436	608.140408	12.114586
12.444900	609.596292	12.119603
12.507356	616.017827	12.124621
12.373372	610.932765	12.129639
12.520096	618.950579	12.134656
12.324198	612.871649	12.139674
12.513378	616.130392	12.144691
12.321093	619.281277	12.149709
12.570767	611.839142	12.154727
12.535264	606.214904	12.159744
12.244309	614.130455	12.164762
12.751258	603.180170	12.169779
12.336306	617.353813	12.174797
12.484851	603.991584	12.179815
12.602838	607.501242	12.184832
12.577753	610.963751	12.189850
12.594923	607.073250	12.194867
12.461333	617.015495	12.199885
12.266996	606.745574	12.204903
12.225515	614.786378	12.209920
12.373574	622.699849	12.214938
12.368982	609.541333	12.219955
12.663619	616.049790	12.224973
12.597348	611.045700	12.229991
12.342544	615.695801	12.235008
12.532478	621.292791	12.240026
12.413571	611.913648	12.245043
12.329778	620.368126	12.250061
12.398080	615.096939	12.255079
12.723001	627.508128	12.260096
12.556530	633.321552	12.265114
13.059500	634.391887	12.270131
12.822862	633.273723	12.275149
12.594138	630.005304	12.280167
12.942858	621.323337	12.285184
12.896553	626.401709	12.290202
12.805043	624.213262	12.295219
12.534364	621.711897	12.300237
12.320588	622.319490	12.305255
12.560581	635.949380	12.310272
12.881705	644.201976	12.315290
12.768703	641.180615	12.320307
12.517048	653.852000	12.325325
12.709989	645.954797	12.330343
12.919312	640.775251	12.335360
12.429402	655.247762	12.340378
13.052785	648.252338	12.345395
13.026032	647.783124	12.350413
13.206908	646.063487	12.355431
13.278166	645.354959	12.360448
13.215560	644.133962	12.365466
13.119188	645.042002	12.370483
12.989467	656.223852	12.375501
12.896465	648.895013	12.380519
12.911763	651.101589	12.385536
12.431738	654.568670	12.390554
13.160315	652.631219	12.395571
12.898994	654.069851	12.400589
12.939904	649.721225	12.405607
13.158224	644.502408	12.410624
12.792281	637.601064	12.415642
13.177234	648.147376	12.420659
12.698792	648.660482	12.425677
12.728365	647.750169	12.430695
12.916787	650.601953	12.435712
12.858812	647.600425	12.440730
13.458119	654.134041	12.445747
12.948591	666.375387	12.450765
13.294627	661.995029	12.455783
12.903121	655.990719	12.460800
12.700141	665.356835	12.465818
13.312874	667.265276	12.470835
13.041507	671.482484	12.475853
13.183613	671.854795	12.480871
13.182661	671.507792	12.485888
12.946220	678.114737	12.490906
13.427886	674.988160	12.495923
13.054305	666.049414	12.500941
13.136878	673.916302	12.505959
13.411579	671.566693	12.510976
13.180323	676.355150	12.515994
13.352155	678.190232	12.521011
12.966511	689.102691	12.526029
13.421219	675.342458	12.531047
13.543868	680.003233	12.536064
13.576700	676.637280	12.541082
13.499485	670.009694	12.546099
13.397694	673.206457	12.551117
13.616203	678.723279	12.556135
13.632885	667.688346	12.561152
13.343730	683.969394	12.566170
13.688845	670.103156	12.571187
13.522417	674.758447	12.576205
13.257094	677.788175	12.581223
13.605142	674.941169	12.586240
13.402356	681.138946	12.591258
13.561806	675.676831	12.596275
13.332140	677.284100	12.601293
13.219567	672.549124	12.606311
13.609923	672.078082	12.611328
13.525466	680.788303	12.616346
13.357455	662.962671	12.621363
13.409736	671.780981	12.626381
13.349982	669.559183	12.631399
13.412351	673.162717	12.636416
13.438348	677.052772	12.641434
13.538936	676.462749	12.646451
13.741140	686.377997	12.651469
13.905645	693.462146	12.656487
13.536530	677.513894	12.661504
13.842250	686.011895	12.666522
13.916772	680.698696	12.671539
13.685514	669.673965	12.676557
13.458958	671.258659	12.681575
13.621827	679.264520	12.686592
13.555411	694.854514	12.691610
13.660061	698.536674	12.696627
13.720647	705.706433	12.701645
13.515212	700.957507	12.706663
13.899926	698.732773	12.711680
13.201849	700.138428	12.716698
13.704565	695.522236	12.721715
13.530738	700.229177	12.726733
13.120836	695.748764	12.731751
13.566224	704.906660	12.736768
14.207821	711.717726	12.741786
14.200791	711.128679	12.746803
13.939940	702.648874	12.751821
13.811704	696.322703	12.756839
14.243501	692.695820	12.761856
13.791912	698.061368	12.766874
13.867168	697.907619	12.771891
14.062988	697.078713	12.776909
13.831168	698.291857	12.781927
13.680436	692.928521	12.786944
14.293935	715.112222	12.791962
13.785946	707.172650	12.796979
14.362960	709.780911	12.801997
13.792933	700.453025	12.807015
14.449942	707.646686	12.812032
13.939037	702.973720	12.817050
14.271320	690.835632	12.822067
14.021222	695.260967	12.827085
13.991321	691.469291	12.832103
13.969317	697.531633	12.837120
14.066381	708.905418	12.842138
14.278533	709.825383	12.847155
14.398879	710.971074	12.852173
14.214914	703.463877	12.857191
14.118570	689.353943	12.862208
13.952198	698.597616	12.867226
14.166649	713.515912	12.872243
14.597463	716.131158	12.877261
14.129703	707.456355	12.882279
14.281570	702.626553	12.887296
14.327122	706.308449	12.892314
14.404643	706.968518	12.897331
14.471448	691.441516	12.902349
14.275660	690.266497	12.907367
14.181319	689.463834	12.912384
14.101854	695.670817	12.917402
14.079756	707.265119	12.922419
14.659915	712.987567	12.927437
14.401679	723.854965	12.932455
14.550997	724.765780	12.937472
14.572007	722.815414	12.942490
14.352897	710.788407	12.947507
14.614350	708.434545	12.952525
14.429963	710.962543	12.957543
14.467940	703.076820	12.962560
14.518205	698.827707	12.967578
14.308072	697.916844	12.972595
14.638647	703.728640	12.977613
14.384960	721.957579	12.982631
14.633172	712.956712	12.987648
14.720194	715.133195	12.992666
14.271548	713.969142	12.997683
14.792706	715.437425	13.002701
14.762225	721.781952	13.007719
14.520286	711.169099	13.012736
14.708990	714.528917	13.017754
14.398757	718.032688	13.022771
14.514242	711.801104	13.027789
14.872947	716.712305	13.032807
14.844014	721.030630	13.037824
14.858472	716.367380	13.042842
14.414103	707.931925	13.047859
14.703811	711.266549	13.052877
14.470958	718.175898	13.057895
15.046594	718.840461	13.062912
14.808216	711.363822	13.067930
14.625130	721.547354	13.072947
15.015613	717.835383	13.077965
14.631990	716.149982	13.082983
14.744424	716.448022	13.088000
14.648753	710.609064	13.093018
14.648293	719.751180	13.098035
14.947562	717.643886	13.103053
14.833575	717.658452	13.108071
14.992653	713.799480	13.113088
14.806864	718.486198	13.118106
14.579015	720.304620	13.123123
14.620871	714.920760	13.128141
14.688831	715.465557	13.133159
14.778031	724.186630	13.138176
14.746243	720.963269	13.143194
14.786592	720.089143	13.148211
14.858395	711.879423	13.153229
14.467601	720.261830	13.158247
14.957894	738.362329	13.163264
14.901356	734.196107	13.168282
14.868525	744.599246	13.173299
15.111789	742.074648	13.178317
15.016086	737.583174	13.183335
15.095473	733.013949	13.188352
15.237034	730.846003	13.193370
15.225121	734.038251	13.198387
15.295577	736.431904	13.203405
14.964970	740.926587	13.208423
15.180224	731.583714	13.213440
15.198051	737.280118	13.218458
14.920539	735.616063	13.223475
15.089155	736.189368	13.228493
15.117935	733.874885	13.233511
15.069073	737.012928	13.238528
15.193525	738.710230	13.243546
14.819381	746.493629	13.248563
15.361011	736.730720	13.253581
14.666363	746.441665	13.258599
14.950075	749.799320	13.263616
15.497361	750.954278	13.268634
15.084833	749.368046	13.273651
15.848162	749.763554	13.278669
15.235759	742.461897	13.283687
15.653748	736.533490	13.288704
15.614163	737.145523	13.293722
15.251918	735.450481	13.298739
15.222443	730.806690	13.303757
15.398759	737.141115	13.308775
15.412493	745.040842	13.313792
15.665669	731.457106	13.318810
14.969483	741.679512	13.323827
15.015235	745.815807	13.328845
15.930041	756.172393	13.333863
15.947233	756.513663	13.338880
15.755814	751.087220	13.343898
15.402874	735.054349	13.348915
15.684172	731.914779	13.353933
15.525459	729.900879	13.358951
15.604524	733.457647	13.363968
15.501491	735.928802	13.368986
15.578832	738.659044	13.374003
15.875420	740.421061	13.379021
15.750871	735.482812	13.384039
15.548245	725.324563	13.389056
15.692620	734.412579	13.394074
15.820378	733.348124	13.399091
15.843905	730.636840	13.404109
15.760614	739.365842	13.409127
15.782051	731.432190	13.414144
15.538970	725.452082	13.419162
15.473240	730.691293	13.424179
15.859841	740.943923	13.429197
15.711295	752.794619	13.434215
16.029904	753.903133	13.439232
16.032461	748.033091	13.444250
15.617787	750.309780	13.449267
16.261457	750.638715	13.454285
15.933657	736.261831	13.459303
15.788790	733.059230	13.464320
15.939752	731.539896	13.469338
15.626579	727.240068	13.474355
16.110823	742.267857	13.479373
15.968806	731.440624	13.484391
15.916550	734.740136	13.489408
15.875960	742.708278	13.494426
16.153202	750.459686	13.499443
16.006986	748.671049	13.504461
16.038745	741.253321	13.509479
15.781574	749.346702	13.514496
16.066132	753.366925	13.519514
15.915610	755.488882	13.524531
16.065166	746.948313	13.529549
16.360770	760.298250	13.534567
16.449785	763.619951	13.539584
16.190087	739.146813	13.544602
16.081343	733.376153	13.549619
16.729435	725.931897	13.554637
16.610326	728.493914	13.559655
16.260371	727.008391	13.564672
16.248777	726.356940	13.569690
16.159425	726.474964	13.574707
16.090346	718.107301	13.579725
16.280717	723.906220	13.584743
16.122964	726.597326	13.589760
16.133023	725.816275	13.594778
15.915484	718.980152	13.599795
15.952764	724.244348	13.604813
16.664802	732.969435	13.609831
16.285626	741.192257	13.614848
16.277903	738.356454	13.619866
16.473467	741.891929	13.624883
16.483738	747.100378	13.629901
16.595323	745.038080	13.634919
16.497405	731.720439	13.639936
16.453524	727.675321	13.644954
16.036694	737.466078	13.649971
16.474766	735.192008	13.654989
16.652603	746.610044	13.660007
16.371591	749.588579	13.665024
16.408979	747.799758	13.670042
16.414678	754.028214	13.675059
16.116565	754.017800	13.680077
16.125911	746.755034	13.685095
15.951040	752.260545	13.690112
16.304333	750.690773	13.695130
16.085275	749.241671	13.700147
16.198727	767.170505	13.705165
16.538129	769.443396	13.710183
16.610983	779.438793	13.715200
16.547299	772.035912	13.720218
16.538296	772.614784	13.725235
16.259146	775.504674	13.730253
16.642773	767.770227	13.735271
16.677134	770.750155	13.740288
16.630788	774.626249	13.745306
16.627114	782.714890	13.750323
16.855940	774.445980	13.755341
16.764720	774.024669	13.760359
16.705583	776.337521	13.765376
16.678285	771.185311	13.770394
16.716896	774.429658	13.775411
17.084772	785.587763	13.780429
16.788917	774.008151	13.785447
16.903433	784.893287	13.790464
17.029726	789.323157	13.795482
16.846006	785.596435	13.800499
17.181216	784.285088	13.805517
17.192006	779.903251	13.810535
17.190193	782.134598	13.815552
17.135311	774.440020	13.820570
17.246833	777.205971	13.825587
17.196962	779.154474	13.830605
17.073036	779.167431	13.835623
16.975589	778.589304	13.840640
17.055830	769.106491	13.845658
16.924118	772.295308	13.850675
17.027853	777.811096	13.855693
17.085830	767.116801	13.860711
17.018782	774.350640	13.865728
16.901238	770.149728	13.870746
17.082814	777.082934	13.875763
16.869463	772.982142	13.880781
16.855296	786.882087	13.885799
17.126127	790.573105	13.890816
17.267127	793.804670	13.895834
17.276845	799.262522	13.900851
16.868729	801.026970	13.905869
17.480681	792.556394	13.910887
17.035193	801.092517	13.915904
17.164534	794.726207	13.920922
17.364308	797.538378	13.925939
17.313070	795.596097	13.930957
17.542159	790.650109	13.935975
17.166738	790.718002	13.940992
17.599977	791.915965	13.946010
17.418326	793.026633	13.951027
17.230944	791.705135	13.956045
17.083894	788.591223	13.961063
17.421629	792.278137	13.966080
17.019938	791.236152	13.971098
17.183072	793.160960	13.976115
17.397735	808.303359	13.981133
17.693983	812.246038	13.986151
17.949826	815.993043	13.991168
17.665091	790.078413	13.996186
17.770246	793.823629	14.001203
17.274038	797.996981	14.006221
17.667022	798.699453	14.011239
17.501345	796.289009	14.016256
17.629579	796.411025	14.021274
17.573001	800.657937	14.026291
17.647313	817.570463	14.031309
17.625132	819.069703	14.036327
17.795696	821.952696	14.041344
18.165193	813.415720	14.046362
17.577437	802.758827	14.051379
17.616856	807.808125	14.056397
17.855988	807.142880	14.061415
17.640477	814.841651	14.066432
17.724003	821.234734	14.071450
17.822673	822.560527	14.076467
17.874461	828.519909	14.081485
17.713840	826.471582	14.086503
17.836577	818.563143	14.091520
17.943331	821.462383	14.096538
17.970192	812.940885	14.101555
17.830133	818.286366	14.106573
18.144249	817.060351	14.111591
18.058825	814.022044	14.116608
18.045419	817.208227	14.121626
18.369600	810.174120	14.126643
18.097340	820.437862	14.131661
17.988794	815.336158	14.136679
18.017389	827.926164	14.141696
18.341181	814.189363	14.146714
18.315740	817.292215	14.151731
17.914792	810.702358	14.156749
18.048541	799.579691	14.161767
18.075878	809.982968	14.166784
18.126136	813.660999	14.171802
18.097439	811.734140	14.176819
17.638655	816.296135	14.181837
18.052874	808.512727	14.186855
17.974935	820.428212	14.191872
18.231637	824.809386	14.196890
18.279543	813.097333	14.201907
17.927651	818.043461	14.206925
18.265874	810.925119	14.211943
18.242254	824.066036	14.216960
17.948421	819.125719	14.221978
18.135295	818.885165	14.226995
18.205486	822.238210	14.232013
18.413806	824.847089	14.237031
17.963325	833.106301	14.242048
18.158686	842.823891	14.247066
18.627028	829.821946	14.252083
18.571622	855.877902	14.257101
18.620313	842.382722	14.262119
18.617581	841.748821	14.267136
18.725271	839.570357	14.272154
18.860892	837.744142	14.277171
18.492341	824.493814	14.282189
18.718194	809.137601	14.287207
18.518874	818.010936	14.292224
18.216625	815.151551	14.297242
18.461707	820.970385	14.302259
18.551054	837.950015	14.307277
18.735090	839.754812	14.312295
18.847877	840.207429	14.317312
18.438873	836.045569	14.322330
18.856717	833.200294	14.327347
18.583101	848.096866	14.332365
18.564401	830.452941	14.337383
18.387722	846.195930	14.342400
18.669832	836.953043	14.347418
19.086121	832.943549	14.352435
18.625664	845.120573	14.357453
18.842242	834.420479	14.362471
18.831627	832.667524	14.367488
18.589557	842.611006	14.372506
18.778421	838.605362	14.377523
18.622510	844.874790	14.382541
18.962415	845.295202	14.387559
18.509347	842.910563	14.392576
18.642900	847.998863	14.397594
19.173560	857.632700	14.402611
18.930169	868.507341	14.407629
19.109082	861.962879	14.412647
19.421734	856.401119	14.417664
18.931818	847.982154	14.422682
19.041775	833.789493	14.427699
18.760900	839.478789	14.432717
19.166770	848.185332	14.437735
19.263122	858.637851	14.442752
19.074954	860.595272	14.447770
19.315983	854.217863	14.452787
19.362301	857.224346	14.457805
19.113782	843.942692	14.462823
18.942107	841.984445	14.467840
19.397243	852.832368	14.472858
19.379677	840.612952	14.477875
19.272448	842.283221	14.482893
18.951257	842.891767	14.487911
19.590315	858.239524	14.492928
19.280212	849.069901	14.497946
19.484979	849.381969	14.502963
19.448677	835.306750	14.507981
19.432379	828.672776	14.512999
19.000242	832.728866	14.518016
19.393224	836.221000	14.523034
19.557390	855.107678	14.528051
19.413517	854.827103	14.533069
19.721933	851.541283	14.538087
19.636192	848.708142	14.543104
19.659922	835.333615	14.548122
19.553113	822.910361	14.553139
19.444009	827.260128	14.558157
19.579708	827.415695	14.563175
19.642604	828.261078	14.568192
19.862095	824.133907	14.573210
19.304604	820.266562	14.578227
19.636788	825.658436	14.583245
19.698788	823.591227	14.588263
19.686876	825.073090	14.593280
19.518920	828.927105	14.598298
19.709578	838.648581	14.603315
19.884873	851.951048	14.608333
19.309450	839.701725	14.613351
19.775962	848.534523	14.618368
19.736926	848.688894	14.623386
19.983064	843.636098	14.628403
19.915510	851.024678	14.633421
19.984232	854.324310	14.638439
19.927196	851.792805	14.643456
19.979723	855.419998	14.648474
19.978886	850.355162	14.653491
19.586840	841.128875	14.658509
19.798514	845.794768	14.663527
19.764502	849.369164	14.668544
19.557080	850.717371	14.673562
20.226678	850.729854	14.678579
19.839935	849.493039	14.683597
19.880590	856.344078	14.688615
19.876077	847.729622	14.693632
19.638768	851.569194	14.698650
19.827402	848.668088	14.703667
19.836575	850.727324	14.708685
20.130595	849.728491	14.713703
20.276232	855.446058	14.718720
20.003033	860.102242	14.723738
20.331801	866.769576	14.728755
20.096987	865.619556	14.733773
20.214858	862.530654	14.738791
20.369844	875.413432	14.743808
20.430751	864.418828	14.748826
20.095198	860.832492	14.753843
20.425515	859.487189	14.758861
20.311574	864.105955	14.763879
20.457433	861.684867	14.768896
20.614123	860.044712	14.773914
20.132188	850.406393	14.778931
20.704309	842.961294	14.783949
20.471234	844.528084	14.788967
20.511366	848.794663	14.793984
20.024843	847.904735	14.799002
20.435539	864.278950	14.804019
20.496737	870.656593	14.809037
20.620331	872.581254	14.814055
20.752008	870.310692	14.819072
20.431083	869.956699	14.824090
20.735501	863.768228	14.829107
20.688717	857.404071	14.834125
20.529843	847.794347	14.839143
20.485869	843.503070	14.844160
20.490652	862.894242	14.849178
20.616756	866.210188	14.854195
20.919978	869.681591	14.859213
20.865411	867.982812	14.864231
20.801933	857.386265	14.869248
20.712330	855.008149	14.874266
20.856177	858.321331	14.879283
20.798027	847.970108	14.884301
20.765942	857.521152	14.889319
20.989987	852.411834	14.894336
20.638854	851.343040	14.899354
20.864762	860.674040	14.904371
20.667966	858.937447	14.909389
20.797911	862.909186	14.914407
20.936198	859.387928	14.919424
20.889676	864.254967	14.924442
20.625398	868.379602	14.929459
20.957580	863.092503	14.934477
20.600349	854.555049	14.939495
20.861577	857.584875	14.944512
20.680529	876.077210	14.949530
20.912531	862.963718	14.954547
20.957606	858.838449	14.959565
20.773208	868.855016	14.964583
20.896555	867.428330	14.969600
21.324392	890.562631	14.974618
21.330812	885.730178	14.979635
21.146731	893.616589	14.984653
20.952561	889.405489	14.989671
21.295653	886.881107	14.994688
21.285560	880.662704	14.999706
21.245255	890.196111	15.004723
21.285202	885.853889	15.009741
21.574023	885.638485	15.014759
21.686392	893.557634	15.019776
21.343649	894.513512	15.024794
21.458647	898.670619	15.029811
21.599744	891.668141	15.034829
21.285797	882.697910	15.039847
21.601169	881.749399	15.044864
21.264350	878.980591	15.049882
21.098217	884.958142	15.054899
21.267705	882.517593	15.059917
20.971337	889.689355	15.064935
21.105239	888.100082	15.069952
21.214421	895.123499	15.074970
21.242844	890.530611	15.079987
21.401072	897.145615	15.085005
21.401532	918.983216	15.090023
21.729009	916.054170	15.095040
21.302319	919.680251	15.100058
21.690270	916.782815	15.105075
22.349792	909.816376	15.110093
22.203170	915.030367	15.115111
22.021529	906.279361	15.120128
21.738370	893.870891	15.125146
21.808851	894.295383	15.130163
22.235563	881.422956	15.135181
21.791274	894.380118	15.140199
21.739239	878.211907	15.145216
22.078455	880.876153	15.150234
21.801587	889.016844	15.155251
21.872515	871.661873	15.160269
21.707477	881.217851	15.165287
21.589683	882.640467	15.170304
21.904116	898.319662	15.175322
22.031902	907.037973	15.180339
22.219523	905.525539	15.185357
22.350285	906.155236	15.190375
22.368633	890.506220	15.195392
22.137180	886.048467	15.200410
22.041651	881.840945	15.205427
22.090403	878.485097	15.210445
21.587704	885.146197	15.215463
22.018250	886.407701	15.220480
22.163732	893.292925	15.225498
22.518054	913.197762	15.230515
22.426840	900.147190	15.235533
22.157121	897.623546	15.240551
21.966834	896.545484	15.245568
22.250826	895.090629	15.250586
22.015431	901.508149	15.255603
22.112344	900.581027	15.260621
22.268084	909.181381	15.265639
22.187926	903.942690	15.270656
22.007741	911.730675	15.275674
22.104479	912.649686	15.280691
22.268015	897.748058	15.285709
22.119534	898.556929	15.290727
22.219308	911.359969	15.295744
22.743943	923.872812	15.300762
22.629340	928.744158	15.305779
22.836091	920.608003	15.310797
22.420949	921.650892	15.315815
22.813450	917.140164	15.320832
22.684556	903.783037	15.325850
22.737143	903.232038	15.330867
22.748217	898.070661	15.335885
22.600075	902.903041	15.340903
22.397850	905.607409	15.345920
22.967660	916.904567	15.350938
22.793016	923.012842	15.355955
22.601995	923.828336	15.360973
22.489193	924.028906	15.365991
22.987538	929.701049	15.371008
22.893215	927.784396	15.376026
22.663271	940.184366	15.381043
23.079783	924.845705	15.386061
22.849630	929.327951	15.391079
22.728615	924.152419	15.396096
22.963396	930.279000	15.401114
22.656441	928.054633	15.406131
22.614728	928.644913	15.411149
23.107379	922.193590	15.416167
23.154397	922.520753	15.421184
22.825578	919.564504	15.426202
22.583344	924.910146	15.431219
22.894967	925.480127	15.436237
22.948286	934.579268	15.441255
22.997832	944.385886	15.446272
23.386907	942.668519	15.451290
23.335079	951.092931	15.456307
23.690363	943.429091	15.461325
23.619545	938.106887	15.466343
23.283121	921.714677	15.471360
23.438369	928.522657	15.476378
23.316654	922.179610	15.481395
23.372751	926.579419	15.486413
23.269048	923.329349	15.491431
23.021292	927.533474	15.496448
23.329170	925.547889	15.501466
22.931932	934.815007	15.506483
23.094845	931.848466	15.511501
23.381542	945.720626	15.516519
23.601491	945.175125	15.521536
23.254161	940.123185	15.526554
23.260748	942.223859	15.531571
23.541345	937.730549	15.536589
23.205874	957.910088	15.541607
23.252071	943.847185	15.546624
23.405865	943.728542	15.551642
23.356839	948.687511	15.556659
23.612067	936.791622	15.561677
23.504775	952.476567	15.566695
23.628476	967.229328	15.571712
24.249072	964.813204	15.576730
23.968656	948.194503	15.581747
23.988909	936.644462	15.586765
24.043207	934.808808	15.591783
24.050244	933.232972	15.596800
24.169415	933.321687	15.601818
23.705021	939.026964	15.606835
24.005730	929.153142	15.611853
24.163439	932.748196	15.616871
24.163783	937.718410	15.621888
24.098097	928.542249	15.626906
23.874414	933.121317	15.631923
23.682470	938.345527	15.636941
24.032132	938.079626	15.641959
23.766406	931.626457	15.646976
23.972564	933.014417	15.651994
24.026399	941.296143	15.657011
23.863466	931.462948	15.662029
23.901304	939.248558	15.667047
24.285372	951.183715	15.672064
24.826658	945.794608	15.677082
24.222140	945.749851	15.682099
24.207136	937.597722	15.687117
24.229459	935.587169	15.692135
24.345470	934.085883	15.697152
24.770956	930.090714	15.702170
24.788781	936.648699	15.707187
24.522256	924.310199	15.712205
24.472750	928.944197	15.717223
24.675227	931.497198	15.722240
24.403326	927.986142	15.727258
24.317922	930.031711	15.732275
24.713268	930.099517	15.737293
24.214347	941.588333	15.742311
23.987956	935.337317	15.747328
24.015292	928.002249	15.752346
24.166708	942.261535	15.757363
24.428748	949.447364	15.762381
24.581996	951.064465	15.767399
24.492034	957.311043	15.772416
24.597284	955.315978	15.777434
24.706672	963.002097	15.782451
24.785970	957.123193	15.787469
25.023147	953.119469	15.792487
24.690346	956.409053	15.797504
24.930823	950.293622	15.802522
24.974051	959.697298	15.807539
24.700625	957.739101	15.812557
24.860352	959.866425	15.817575
24.789243	958.116565	15.822592
25.122571	954.826847	15.827610
24.876503	962.918596	15.832627
24.946719	956.608770	15.837645
24.800300	957.777077	15.842663
24.697195	955.467320	15.847680
24.997618	945.312671	15.852698
25.206531	951.452754	15.857715
25.133348	947.651984	15.862733
25.181839	945.034609	15.867751
24.549926	958.737383	15.872768
25.224374	950.793479	15.877786
24.863403	956.558397	15.882803
25.220930	949.973471	15.887821
24.958555	951.134585	15.892839
24.883964	949.722932	15.897856
25.403252	956.486866	15.902874
25.461214	973.402087	15.907891
25.257031	960.779305	15.912909
25.483911	962.407034	15.917927
25.248885	967.865174	15.922944
25.567346	956.906150	15.927962
25.261655	967.960963	15.932979
25.407910	975.657126	15.937997
25.519428	971.174353	15.943015
25.156663	978.602637	15.948032
25.367970	967.985333	15.953050
25.633764	973.226646	15.958067
25.418641	966.023985	15.963085
25.664457	967.614053	15.968103
25.760734	979.934858	15.973120
25.828174	968.702491	15.978138
25.538153	972.572386	15.983155
25.699018	973.064858	15.988173
26.022719	975.993460	15.993191
25.943006	977.129292	15.998208
25.535913	974.030589	16.003226
25.542622	965.628918	16.008243
25.684357	973.814925	16.013261
25.553713	973.573313	16.018279
25.593426	976.969001	16.023296
25.716540	976.012550	16.028314
25.695402	981.408991	16.033331
25.748971	965.214792	16.038349
25.955262	975.318910	16.043367
25.718211	976.062680	16.048384
25.791304	975.754634	16.053402
25.904996	989.155156	16.058419
25.825155	993.752868	16.063437
26.115218	994.275716	16.068455
26.247536	999.708230	16.073472
26.145618	992.670966	16.078490
26.155198	998.192015	16.083507
26.195452	992.382294	16.088525
26.317367	991.687956	16.093543
26.322524	1000.071962	16.098560
26.346942	1000.071290	16.103578
26.181525	998.620127	16.108595
26.458567	994.405063	16.113613
26.573802	1001.727376	16.118631
26.585666	1000.116070	16.123648
26.388576	997.887211	16.128666
26.549369	994.463406	16.133683
26.267615	998.041690	16.138701
26.237789	990.248446	16.143719
26.427322	1003.088069	16.148736
26.590879	993.923519	16.153754
26.434468	988.996472	16.158771
26.006515	987.646144	16.163789
26.498377	985.994818	16.168807
26.296493	995.278888	16.173824
26.358483	993.236907	16.178842
26.534288	995.913989	16.183859
26.820266	997.980636	16.188877
26.651296	988.460770	16.193895
26.690836	996.476509	16.198912
27.001982	999.937236	16.203930
26.852384	1003.614865	16.208947
26.722544	995.562639	16.213965
26.975490	1004.059543	16.218983
26.992440	1007.023287	16.224000
26.689414	993.936197	16.229018
26.749314	997.142556	16.234035
26.948011	1006.405288	16.239053
27.070599	997.313386	16.244071
27.180960	1013.100193	16.249088
27.261022	1007.833371	16.254106
27.174608	993.513369	16.259123
27.005349	983.075226	16.264141
26.916064	1003.140748	16.269159
26.849143	1007.121081	16.274176
27.047106	1003.530543	16.279194
27.013833	1010.967499	16.284211
27.057095	1006.410140	16.289229
27.530861	998.421722	16.294247
27.585597	1008.322240	16.299264
27.350031	1011.435752	16.304282
27.396419	1005.757614	16.309299
27.281779	1009.628613	16.314317
27.563098	1003.917053	16.319335
27.374504	1004.571230	16.324352
27.405888	1002.395159	16.329370
27.654424	1006.247483	16.334387
27.531811	1005.114697	16.339405
27.478002	1005.315550	16.344423
27.324466	1004.042415	16.349440
27.755349	1003.587145	16.354458
27.516629	1003.602197	16.359475
27.617695	1006.559156	16.364493
27.738241	1008.178199	16.369511
27.436297	1010.879174	16.374528
27.752436	1000.722047	16.379546
27.628259	1001.650213	16.384563
27.427320	1001.558398	16.389581
27.618383	1007.492999	16.394599
27.428595	1003.483158	16.399616
27.544072	1014.384064	16.404634
27.542171	1012.086945	16.409651
27.843005	1028.478417	16.414669
27.732416	1024.673987	16.419687
27.783226	1027.465208	16.424704
27.779458	1032.322481	16.429722
28.009399	1029.332865	16.434739
27.697730	1030.962400	16.439757
27.857449	1028.406588	16.444775
27.777300	1023.786389	16.449792
27.976675	1021.221249	16.454810
28.133975	1026.069222	16.459827
27.747263	1019.606456	16.464845
28.295845	1032.137738	16.469863
28.291491	1035.174230	16.474880
28.272679	1047.888537	16.479898
28.676873	1036.688901	16.484915
28.155388	1030.013589	16.489933
28.318092	1022.130394	16.494951
28.475914	1038.118115	16.499968
28.232148	1039.459371	16.504986
28.465561	1041.710931	16.510003
28.274280	1044.104351	16.515021
28.683398	1046.782984	16.520039
28.558319	1037.543432	16.525056
28.589736	1038.081306	16.530074
28.506019	1026.916617	16.535091
28.759401	1049.936278	16.540109
28.504943	1037.605288	16.545127
28.196235	1037.798492	16.550144
28.433705	1036.852635	16.555162
28.704874	1036.693627	16.560179
28.644765	1045.431793	16.565197
28.916586	1038.841243	16.570215
28.703486	1042.762293	16.575232
28.597527	1044.233570	16.580250
28.942803	1028.817550	16.585267
28.978168	1045.613282	16.590285
29.116007	1038.724861	16.595303
29.072978	1035.746186	16.600320
28.897649	1034.022012	16.605338
29.041857	1036.413690	16.610355
28.794916	1038.973564	16.615373
28.925051	1040.225049	16.620391
28.868514	1034.124275	16.625408
28.896019	1035.644199	16.630426
29.038544	1029.430384	16.635443
28.842026	1039.732952	16.640461
28.983661	1040.001204	16.645479
29.381006	1041.220553	16.650496
29.271964	1035.815909	16.655514
28.939418	1042.002457	16.660531
29.192498	1045.746785	16.665549
29.405306	1031.496928	16.670567
29.094224	1032.160710	16.675584
29.114949	1044.890948	16.680602
29.661714	1055.292391	16.685619
29.251021	1066.218447	16.690637
29.571609	1068.759391	16.695655
29.475995	1068.348224	16.700672
29.534525	1064.463806	16.705690
29.873619	1066.118254	16.710707
29.670568	1066.613740	16.715725
29.923223	1047.055983	16.720743
29.437354	1048.229810	16.725760
29.473003	1042.654315	16.730778
29.410213	1046.280568	16.735795
29.565331	1057.418322	16.740813
29.386858	1060.059056	16.745831
29.951145	1060.854788	16.750848
29.613362	1065.969200	16.755866
30.090851	1051.829594	16.760883
29.864369	1057.289586	16.765901
30.432532	1052.473768	16.770919
30.256487	1059.446986	16.775936
30.182717	1058.098312	16.780954
29.843934	1036.783373	16.785971
29.932307	1046.104327	16.790989
30.256447	1059.285947	16.796007
30.276023	1049.518944	16.801024
30.183174	1038.873214	16.806042
29.912891	1028.264583	16.811059
30.294137	1040.096100	16.816077
30.393886	1050.178980	16.821095
30.477590	1038.697887	16.826112
30.047998	1032.484785	16.831130
30.026387	1020.016570	16.836147
30.247675	1032.627212	16.841165
30.409696	1048.557485	16.846183
30.854753	1040.074908	16.851200
30.336465	1036.611659	16.856218
30.217747	1021.059606	16.861235
29.815676	1035.474569	16.866253
30.397105	1046.877297	16.871271
30.225740	1048.339823	16.876288
29.999198	1043.231179	16.881306
30.141377	1057.375232	16.886323
29.953579	1051.304356	16.891341
30.214217	1058.105445	16.896359
30.385698	1060.032138	16.901376
30.524753	1082.776156	16.906394
30.780529	1073.865447	16.911411
30.844776	1079.923957	16.916429
31.048667	1077.739954	16.921447
30.700034	1072.700802	16.926464
30.702534	1073.571379	16.931482
30.973476	1085.631536	16.936499
31.124789	1082.793007	16.941517
30.705208	1092.249875	16.946535
30.871032	1080.269981	16.951552
30.926164	1071.639818	16.956570
30.934826	1080.708117	16.961587
31.069682	1074.015804	16.966605
30.805796	1068.351240	16.971623
31.239025	1071.770884	16.976640
30.911319	1078.316448	16.981658
31.186471	1076.399057	16.986675
31.052894	1077.738939	16.991693
31.126541	1077.396092	16.996711
31.102441	1071.400707	17.001728
30.932563	1079.720484	17.006746
31.245297	1073.606384	17.011763
31.068754	1090.551916	17.016781
31.017340	1087.883803	17.021799
31.678976	1095.992076	17.026816
31.353999	1104.774666	17.031834
31.490089	1104.166478	17.036851
31.786776	1101.504126	17.041869
31.474871	1109.151761	17.046887
31.557133	1094.357296	17.051904
31.959712	1098.586438	17.056922
31.513044	1100.224374	17.061939
31.536775	1105.020582	17.066957
31.771174	1097.182996	17.071975
31.662353	1098.815668	17.076992
31.938260	1093.467836	17.082010
32.106128	1101.340567	17.087027
31.857186	1098.703207	17.092045
31.714888	1101.451922	17.097063
32.237031	1093.137197	17.102080
31.848543	1081.660168	17.107098
31.750319	1085.184649	17.112115
31.758003	1085.521094	17.117133
31.826981	1095.157515	17.122151
32.170795	1092.724509	17.127168
32.088211	1106.436542	17.132186
32.053588	1098.830187	17.137203
32.268458	1102.050307	17.142221
32.270972	1091.351830	17.147239
32.100308	1095.468253	17.152256
31.998921	1096.983004	17.157274
31.873069	1096.765890	17.162291
32.222657	1103.092404	17.167309
32.125548	1096.477223	17.172327
32.068142	1093.608074	17.177344
32.006852	1102.355919	17.182362
32.035693	1092.227692	17.187379
32.164357	1104.335260	17.192397
32.339206	1115.561496	17.197415
32.445585	1112.171386	17.202432
32.363936	1116.961914	17.207450
32.640270	1116.959890	17.212467
32.624956	1116.905445	17.217485
32.515160	1122.839591	17.222503
32.574060	1110.093692	17.227520
32.697046	1123.726396	17.232538
32.614674	1123.120663	17.237555
32.691953	1125.134613	17.242573
32.314144	1122.435263	17.247591
32.725464	1116.668714	17.252608
32.614441	1120.138391	17.257626
32.845707	1112.799898	17.262643
32.686386	1114.323670	17.267661
32.712301	1119.024868	17.272679
32.656146	1117.929065	17.277696
32.373165	1129.501144	17.282714
32.801309	1136.897870	17.287731
33.290439	1129.418238	17.292749
33.048577	1146.178334	17.297767
33.437834	1141.573382	17.302784
33.127767	1147.462979	17.307802
33.478930	1141.879355	17.312819
33.489981	1136.336063	17.317837
33.207536	1142.559025	17.322855
33.507144	1134.916396	17.327872
33.451155	1137.762131	17.332890
33.407657	1143.629158	17.337907
33.588698	1135.206576	17.342925
33.236388	1133.879173	17.347943
33.437520	1130.802508	17.352960
33.617211	1129.783592	17.357978
33.239598	1130.110600	17.362995
33.383682	1126.127643	17.368013
33.469096	1131.324505	17.373031
33.688370	1134.502920	17.378048
33.403034	1137.529529	17.383066
33.627920	1133.546613	17.388083
33.728322	1132.066675	17.393101
33.773685	1132.075366	17.398119
33.717633	1134.192126	17.403136
33.655986	1136.811526	17.408154
33.711594	1137.064773	17.413171
33.833029	1132.637220	17.418189
33.557641	1138.852771	17.423207
33.403221	1146.605289	17.428224
33.749337	1156.460524	17.433242
33.667745	1159.853043	17.438259
33.992228	1158.679039	17.443277
34.023491	1162.306451	17.448295
34.103154	1160.621458	17.453312
34.003798	1153.795169	17.458330
34.009576	1160.509745	17.463347
34.113046	1152.465304	17.468365
34.129653	1166.379688	17.473383
34.356410	1155.236007	17.478400
33.995802	1154.468467	17.483418
33.958762	1160.886756	17.488435
34.306150	1172.048295	17.493453
34.339490	1183.063078	17.498471
34.800968	1189.640444	17.503488
34.421756	1177.982028	17.508506
34.276674	1180.737500	17.513523
34.587733	1174.137636	17.518541
34.421725	1164.449957	17.523559
34.763393	1169.950913	17.528576
34.895273	1179.050570	17.533594
34.837330	1178.324268	17.538611
35.278788	1169.577104	17.543629
34.858540	1161.327023	17.548647
34.844349	1160.524483	17.553664
34.672597	1152.917364	17.558682
34.717872	1161.011179	17.563699
34.778561	1169.487603	17.568717
34.717512	1173.261932	17.573735
34.567223	1171.467575	17.578752
35.000690	1166.518064	17.583770
34.697498	1179.387193	17.588787
35.039084	1170.090693	17.593805
35.005047	1167.296788	17.598823
35.565577	1172.432312	17.603840
35.413438	1172.200355	17.608858
35.134800	1168.024430	17.613875
35.491772	1170.496608	17.618893
35.232356	1169.558679	17.623911
35.298993	1169.986933	17.628928
35.386241	1170.446691	17.633946
35.310034	1175.037572	17.638963
35.283548	1165.050461	17.643981
35.384664	1173.473256	17.648999
35.389378	1170.130522	17.654016
35.319554	1168.367818	17.659034
35.203360	1164.864030	17.664051
35.219539	1163.387735	17.669069
35.092105	1169.536080	17.674087
35.461361	1174.587777	17.679104
35.723422	1182.404853	17.684122
35.580140	1193.103161	17.689139
35.554123	1193.293378	17.694157
35.910315	1194.547547	17.699175
35.636518	1189.878560	17.704192
36.049961	1189.713179	17.709210
35.679801	1196.072892	17.714227
35.612694	1186.524436	17.719245
35.655294	1201.037556	17.724263
35.702996	1198.505473	17.729280
35.958817	1189.733553	17.734298
35.588985	1190.734689	17.739315
35.866530	1200.717389	17.744333
36.253668	1213.188729	17.749351
36.285044	1218.084762	17.754368
36.384649	1219.486179	17.759386
36.264095	1217.431568	17.764403
36.415597	1214.864387	17.769421
36.575028	1213.968541	17.774439
36.331520	1198.953311	17.779456
36.493845	1190.988051	17.784474
36.285763	1212.858481	17.789491
36.403483	1219.284253	17.794509
36.778455	1214.618391	17.799527
36.698761	1208.013081	17.804544
36.777481	1193.039206	17.809562
36.462924	1192.933521	17.814579
36.288618	1191.502661	17.819597
36.572092	1207.799172	17.824615
36.570226	1219.327541	17.829632
36.815963	1209.133921	17.834650
36.788535	1209.153944	17.839667
36.846228	1206.093288	17.844685
37.062021	1210.256865	17.849703
36.652852	1213.615190	17.854720
36.717080	1208.600081	17.859738
36.645492	1210.365821	17.864755
36.762386	1201.555566	17.869773
36.941394	1204.686615	17.874791
36.621146	1200.999996	17.879808
36.862246	1194.736062	17.884826
36.932996	1210.453474	17.889843
36.869133	1217.929993	17.894861
36.976590	1229.277246	17.899879
37.188674	1231.241818	17.904896
37.179994	1220.911077	17.909914
36.997509	1217.666907	17.914931
37.323820	1226.316597	17.919949
37.260498	1231.000160	17.924967
36.955274	1234.459070	17.929984
37.487477	1225.079215	17.935002
37.450369	1226.501918	17.940019
37.312956	1233.579642	17.945037
37.257423	1226.320470	17.950055
37.397124	1238.379074	17.955072
37.450652	1238.733631	17.960090
37.543696	1247.911953	17.965107
37.696906	1242.999745	17.970125
37.996785	1245.944725	17.975143
37.694644	1244.944016	17.980160
37.905993	1249.875153	17.985178
37.905215	1247.470532	17.990195
37.976325	1236.814935	17.995213
38.171583	1244.216408	18.000231
37.783007	1248.066993	18.005248
37.953513	1242.552491	18.010266
37.866102	1239.407123	18.015283
37.753229	1235.028649	18.020301
37.980530	1231.998385	18.025319
38.006655	1236.068423	18.030336
38.520200	1221.897822	18.035354
38.574996	1231.473410	18.040371
38.432082	1227.535114	18.045389
38.547222	1224.373992	18.050407
38.265190	1229.113697	18.055424
38.441791	1224.876348	18.060442
38.435667	1235.941489	18.065459
38.569657	1226.503713	18.070477
38.914830	1234.844358	18.075495
38.270400	1230.523399	18.080512
38.666419	1231.654605	18.085530
38.629953	1235.854308	18.090547
38.462693	1231.014089	18.095565
38.815542	1229.131922	18.100583
38.521350	1234.463656	18.105600
38.533972	1233.047869	18.110618
38.188911	1233.663299	18.115635
38.658396	1241.773155	18.120653
38.602484	1247.670550	18.125671
38.643592	1245.502404	18.130688
38.843760	1250.779264	18.135706
39.049647	1251.886426	18.140723
39.186470	1254.313997	18.145741
39.262084	1249.615839	18.150759
39.097266	1255.280886	18.155776
39.457437	1248.805891	18.160794
39.521900	1251.232104	18.165811
39.442609	1252.367888	18.170829
39.260403	1244.071238	18.175847
39.129374	1249.923526	18.180864
39.251890	1245.265404	18.185882
39.502213	1247.924611	18.190899
39.334692	1246.811425	18.195917
39.208045	1249.671335	18.200935
39.354277	1251.235908	18.205952
39.560001	1254.167146	18.210970
39.429426	1249.491624	18.215987
39.251432	1248.591507	18.221005
39.504680	1248.820294	18.226023
39.422084	1249.085593	18.231040
39.816448	1258.021347	18.236058
39.968828	1269.307983	18.241075
39.751813	1272.055734	18.246093
39.994354	1270.402177	18.251111
39.462256	1270.567047	18.256128
39.966899	1272.284102	18.261146
39.941220	1266.664437	18.266163
40.231895	1273.489334	18.271181
40.081943	1278.281072	18.276199
39.852805	1279.408630	18.281216
40.240193	1264.673814	18.286234
40.022104	1274.272976	18.291251
40.269151	1273.868414	18.296269
40.309729	1267.629363	18.301287
40.372717	1274.290895	18.306304
40.146416	1266.322991	18.311322
40.239003	1267.441483	18.316339
39.816754	1268.299305	18.321357
40.005677	1268.708522	18.326375
40.088541	1281.789017	18.331392
40.420022	1268.565065	18.336410
40.201775	1273.777689	18.341427
40.031071	1296.986774	18.346445
40.970858	1296.742599	18.351463
40.630523	1286.400341	18.356480
41.168295	1289.204148	18.361498
41.397431	1291.487964	18.366515
40.724585	1278.783290	18.371533
40.949127	1264.389409	18.376551
40.651807	1278.750389	18.381568
41.091021	1283.283141	18.386586
41.157549	1278.374951	18.391603
40.919072	1266.969119	18.396621
41.131490	1267.844892	18.401639
40.542443	1275.873418	18.406656
41.318442	1280.634600	18.411674
41.313545	1274.923335	18.416691
41.272596	1281.673635	18.421709
41.523200	1285.273233	18.426727
41.009469	1274.563503	18.431744
41.553082	1278.937988	18.436762
41.601877	1280.637655	18.441779
41.320810	1287.927115	18.446797
41.272664	1274.443528	18.451815
41.093858	1287.347017	18.456832
41.209087	1280.376816	18.461850
41.506161	1274.618536	18.466867
41.137748	1278.961450	18.471885
41.068180	1274.330070	18.476903
40.947612	1285.766511	18.481920
41.302227	1297.248896	18.486938
41.534183	1306.506606	18.491955
41.452895	1303.726348	18.496973
41.687013	1303.102891	18.501991
41.635888	1310.325001	18.507008
41.469566	1308.735098	18.512026
41.907401	1317.099224	18.517043
41.759767	1328.580931	18.522061
42.167637	1326.974211	18.527079
42.055772	1327.629076	18.532096
42.071453	1329.930352	18.537114
42.363865	1324.734516	18.542131
42.271102	1327.374567	18.547149
42.637626	1327.869743	18.552167
42.269248	1324.654496	18.557184
42.219801	1322.109119	18.562202
42.422805	1327.492858	18.567219
42.530990	1335.681099	18.572237
42.586756	1318.309119	18.577255
42.551934	1325.418244	18.582272
42.346834	1324.639108	18.587290
42.760784	1317.073272	18.592307
42.511043	1327.977585	18.597325
42.561904	1330.033541	18.602343
42.505320	1328.079411	18.607360
42.282722	1321.679344	18.612378
42.856510	1324.714236	18.617395
42.410584	1332.726815	18.622413
42.690423	1328.309266	18.627431
42.933693	1327.769590	18.632448
42.746273	1331.604654	18.637466
43.065744	1337.064937	18.642483
42.829092	1345.092276	18.647501
43.105875	1344.222334	18.652519
42.983215	1347.012211	18.657536
43.282559	1349.761631	18.662554
43.302389	1343.762471	18.667571
43.252877	1353.316494	18.672589
43.459503	1350.819606	18.677607
43.249978	1354.825374	18.682624
43.318291	1353.830098	18.687642
43.323757	1348.985045	18.692659
43.342059	1343.263834	18.697677
43.644588	1344.772523	18.702695
43.573747	1347.390230	18.707712
43.621636	1350.901482	18.712730
43.843448	1336.416449	18.717747
44.014191	1353.311316	18.722765
44.188122	1344.378501	18.727783
43.840227	1341.876431	18.732800
43.723122	1338.044546	18.737818
43.793054	1337.232056	18.742835
43.798784	1335.277690	18.747853
44.090821	1336.611287	18.752871
44.230284	1336.756806	18.757888
43.955275	1339.406299	18.762906
43.770432	1334.663463	18.767923
43.824153	1347.246770	18.772941
43.844360	1342.847549	18.777959
43.997558	1335.189759	18.782976
43.728578	1342.455269	18.787994
44.308818	1350.765681	18.793011
43.982922	1362.410865	18.798029
44.172993	1360.957973	18.803047
44.086007	1359.096936	18.808064
44.151184	1363.091494	18.813082
44.370088	1357.629381	18.818099
44.873960	1371.174571	18.823117
44.549367	1360.331199	18.828135
44.362022	1361.449099	18.833152
44.342991	1363.055192	18.838170
44.867796	1375.994364	18.843187
44.884468	1384.862755	18.848205
44.882905	1382.316225	18.853223
44.797228	1380.615928	18.858240
44.474031	1387.075695	18.863258
44.951605	1379.679809	18.868275
44.532888	1379.868053	18.873293
44.563107	1384.729598	18.878311
45.005386	1381.227179	18.883328
44.646068	1381.475602	18.888346
44.934301	1386.356937	18.893363
45.025345	1399.969579	18.898381
45.298022	1398.339720	18.903399
45.488575	1408.112018	18.908416
45.431662	1406.599745	18.913434
45.333834	1397.560891	18.918451
45.434422	1401.922332	18.923469
45.557244	1400.934346	18.928487
45.603812	1399.178744	18.933504
45.564591	1410.810884	18.938522
45.590383	1400.155933	18.943539
45.653891	1403.857269	18.948557
45.729069	1399.607267	18.953575
46.063001	1396.680295	18.958592
45.633704	1401.562896	18.963610
45.912262	1397.792472	18.968627
45.996697	1408.165119	18.973645
45.418166	1405.604274	18.978663
45.780940	1396.298047	18.983680
46.030087	1402.823344	18.988698
45.878062	1390.160578	18.993715
46.058184	1393.218903	18.998733
46.227354	1396.802800	19.003751
46.344392	1382.801105	19.008768
46.082655	1391.179511	19.013786
46.192821	1390.278703	19.018803
45.949545	1400.216371	19.023821
45.852809	1400.322926	19.028839
46.248872	1414.437203	19.033856
46.441975	1424.455267	19.038874
46.660337	1424.998760	19.043891
46.429713	1425.022018	19.048909
46.345613	1431.495068	19.053927
46.828101	1426.253830	19.058944
46.518882	1421.852230	19.063962
46.689513	1424.012627	19.068979
46.672159	1425.470141	19.073997
46.483036	1427.787536	19.079015
46.655070	1425.217128	19.084032
46.718828	1435.473089	19.089050
47.294293	1439.669085	19.094067
47.258004	1449.495658	19.099085
47.293594	1442.761857	19.104103
47.203029	1417.699712	19.109120
47.244357	1423.859740	19.114138
47.144780	1420.883493	19.119155
47.129940	1428.002170	19.124173
47.186008	1437.391476	19.129191
47.452279	1434.257281	19.134208
47.214866	1446.358961	19.139226
47.465232	1444.678922	19.144243
47.460474	1433.558490	19.149261
47.331525	1440.584484	19.154279
47.212337	1440.915443	19.159296
47.043598	1448.424167	19.164314
47.163281	1434.904861	19.169331
47.369419	1451.134741	19.174349
47.302507	1463.206731	19.179367
47.830052	1456.784498	19.184384
47.603339	1460.953913	19.189402
48.064927	1463.315170	19.194419
48.085285	1457.757706	19.199437
48.046890	1459.612977	19.204455
47.942894	1463.334093	19.209472
48.017809	1464.531089	19.214490
47.993483	1455.777410	19.219507
48.271828	1457.996781	19.224525
47.512099	1456.966317	19.229543
48.222276	1466.446303	19.234560
47.922716	1478.636577	19.239578
48.364541	1477.554738	19.244595
48.515983	1484.319342	19.249613
48.411739	1484.903598	19.254631
48.830338	1485.810397	19.259648
48.891483	1493.169738	19.264666
48.936086	1487.649516	19.269683
48.575149	1476.155317	19.274701
48.417400	1488.190974	19.279719
48.894731	1478.308284	19.284736
48.859084	1483.003384	19.289754
49.129029	1484.283626	19.294771
48.824200	1486.486499	19.299789
48.714730	1486.620283	19.304807
48.977558	1482.038085	19.309824
48.991559	1483.424448	19.314842
49.246924	1489.065174	19.319859
49.127289	1478.316054	19.324877
49.082075	1483.975174	19.329895
49.269872	1479.171126	19.334912
49.148650	1490.194385	19.339930
49.111955	1476.248110	19.344947
49.077683	1478.834895	19.349965
48.916464	1476.859169	19.354983
49.342297	1492.161780	19.360000
49.248206	1497.235216	19.365018
49.387559	1504.449839	19.370035
49.454870	1506.531658	19.375053
49.470233	1509.041291	19.380071
49.684584	1488.968299	19.385088
49.720237	1499.212893	19.390106
49.235944	1496.706791	19.395123
49.539813	1511.375148	19.400141
49.739650	1516.055684	19.405159
50.221660	1516.488703	19.410176
49.594968	1520.439537	19.415194
49.708093	1523.031782	19.420211
50.319408	1512.837876	19.425229
49.822621	1515.862755	19.430247
50.245699	1516.797262	19.435264
50.093528	1518.742838	19.440282
50.170621	1517.935537	19.445299
50.007050	1527.930294	19.450317
50.120091	1525.346966	19.455335
50.514828	1529.306031	19.460352
50.433017	1538.893585	19.465370
50.582551	1533.016180	19.470387
50.666230	1535.925441	19.475405
50.438732	1545.292680	19.480423
50.429141	1540.203763	19.485440
50.536251	1549.484194	19.490458
50.550993	1539.553571	19.495475
50.610735	1539.029841	19.500493
50.910745	1555.008511	19.505511
51.705914	1544.388324	19.510528
51.393591	1536.345329	19.515546
51.186603	1527.351807	19.520563
51.800479	1520.811968	19.525581
51.440268	1516.191063	19.530599
50.993773	1523.806180	19.535616
51.285811	1520.882554	19.540634
51.286865	1526.357757	19.545651
51.294980	1525.191961	19.550669
51.297614	1530.925699	19.555687
51.279214	1526.567158	19.560704
51.238521	1528.312339	19.565722
51.654953	1542.117429	19.570739
51.800702	1536.543574	19.575757
51.637508	1547.705948	19.580775
51.554521	1550.237212	19.585792
52.023036	1543.893568	19.590810
52.018155	1540.716362	19.595827
51.856652	1540.157649	19.600845
51.879325	1547.715509	19.605863
52.184932	1541.813801	19.610880
51.897106	1541.855433	19.615898
51.563702	1547.755106	19.620915
52.123524	1543.931393	19.625933
51.867104	1546.363425	19.630951
51.991368	1543.355463	19.635968
51.985089	1548.317410	19.640986
51.944865	1548.910636	19.646003
52.217724	1551.212925	19.651021
52.294730	1571.530911	19.656039
52.564752	1556.848843	19.661056
52.536161	1573.939058	19.666074
52.514322	1568.119882	19.671091
52.686263	1558.691801	19.676109
52.456913	1572.398640	19.681127
52.532085	1562.610076	19.686144
52.897549	1563.982751	19.691162
52.726780	1571.479219	19.696179
52.822537	1559.642459	19.701197
52.809085	1564.413021	19.706215
53.087500	1547.482686	19.711232
53.500566	1561.398770	19.716250
53.383310	1567.050198	19.721267
53.511710	1553.207549	19.726285
53.258762	1555.746340	19.731303
53.308281	1550.231644	19.736320
53.221275	1556.096113	19.741338
53.237950	1557.052870	19.746355
53.207065	1547.946712	19.751373
53.039713	1552.671803	19.756391
53.451068	1563.811007	19.761408
53.341166	1573.352459	19.766426
53.460563	1577.729950	19.771443
53.712814	1569.516987	19.776461
53.882882	1584.572316	19.781479
53.769912	1570.322257	19.786496
54.097433	1578.533266	19.791514
54.290636	1576.609647	19.796531
54.080173	1568.572869	19.801549
53.822332	1570.206694	19.806567
54.071296	1574.128504	19.811584
54.217236	1577.368911	19.816602
53.987324	1579.156181	19.821619
53.728740	1571.587649	19.826637
53.946107	1575.208260	19.831655
54.013678	1575.917249	19.836672
54.300887	1591.427724	19.841690
54.285441	1592.275873	19.846707
54.583336	1588.764335	19.851725
54.464845	1593.251453	19.856743
54.679105	1599.239447	19.861760
54.602753	1598.758995	19.866778
54.347965	1597.921309	19.871795
54.688207	1592.878898	19.876813
54.401295	1591.938915	19.881831
54.491784	1606.246090	19.886848
54.867318	1607.582487	19.891866
54.860674	1625.672898	19.896883
55.199289	1627.734581	19.901901
55.014536	1624.074116	19.906919
55.053924	1622.360636	19.911936
55.321737	1623.432933	19.916954
54.955099	1628.018655	19.921971
55.199424	1620.696857	19.926989
55.265619	1627.152890	19.932007
55.191665	1620.593870	19.937024
55.418647	1624.228774	19.942042
55.390039	1618.906106	19.947059
55.473355	1623.828878	19.952077
55.229402	1626.972205	19.957095
55.190372	1641.211209	19.962112
56.090025	1639.505803	19.967130
55.866757	1644.249092	19.972147
55.862913	1643.911987	19.977165
55.807275	1646.899763	19.982183
55.936646	1650.571961	19.987200
55.929229	1633.010692	19.992218
55.847041	1641.424378	19.997235
56.032410	1628.661574	20.002253
55.860865	1640.699481	20.007271
55.842618	1637.956693	20.012288
56.075811	1646.699982	20.017306
56.051010	1662.625177	20.022323
56.518336	1657.824898	20.027341
56.580772	1662.179720	20.032359
56.687945	1661.506587	20.037376
56.851461	1664.018423	20.042394
56.615653	1659.419138	20.047411
56.933498	1654.070922	20.052429
57.004037	1660.605187	20.057447
57.068090	1650.395420	20.062464
57.454434	1635.253355	20.067482
56.993699	1629.417283	20.072499
56.780025	1614.542228	20.077517
56.776323	1627.604896	20.082535
56.999595	1633.316938	20.087552
57.141499	1640.572246	20.092570
57.301567	1646.347782	20.097587
57.445102	1648.203151	20.102605
57.448450	1640.751601	20.107623
57.293939	1643.303481	20.112640
57.427525	1646.031418	20.117658
57.196696	1647.506407	20.122675
57.252787	1649.586833	20.127693
57.442077	1652.716360	20.132711
57.130644	1657.410262	20.137728
57.555713	1657.602837	20.142746
57.419001	1666.671977	20.147763
57.508935	1672.471065	20.152781
57.588237	1676.444560	20.157799
57.344480	1676.839099	20.162816
57.515898	1666.754621	20.167834
57.859249	1686.718840	20.172851
58.341668	1697.064406	20.177869
58.065344	1695.463191	20.182887
58.195386	1696.512760	20.187904
58.367057	1703.883383	20.192922
58.203200	1704.388562	20.197939
58.685290	1690.594883	20.202957
58.692698	1697.470358	20.207975
58.428823	1697.905900	20.212992
58.706679	1694.507918	20.218010
58.430098	1691.281467	20.223027
58.308308	1692.524883	20.228045
58.560473	1688.559688	20.233063
58.391957	1687.692787	20.238080
58.629230	1687.854640	20.243098
58.617821	1696.235240	20.248115
58.917030	1706.786066	20.253133
59.034984	1712.987913	20.258151
58.781211	1722.293062	20.263168
59.141049	1712.065611	20.268186
59.111723	1719.937760	20.273203
59.109997	1715.365132	20.278221
59.096729	1705.656533	20.283239
59.204323	1718.253805	20.288256
59.380638	1704.151108	20.293274
59.265289	1716.884078	20.298291
59.206392	1715.271100	20.303309
59.654031	1728.055283	20.308327
59.474902	1739.646301	20.313344
59.887483	1742.163553	20.318362
59.928525	1747.190774	20.323379
59.710558	1733.625980	20.328397
59.570787	1740.044692	20.333415
59.879413	1744.165538	20.338432
59.642522	1735.097670	20.343450
59.511002	1734.635271	20.348467
59.913149	1731.082228	20.353485
59.963059	1744.243934	20.358503
59.976717	1757.433385	20.363520
60.239039	1758.812667	20.368538
60.404811	1757.246759	20.373555
60.315334	1756.074051	20.378573
60.576863	1751.343660	20.383591
60.509342	1754.790907	20.388608
60.445755	1754.646143	20.393626
60.619866	1755.430073	20.398643
60.378195	1759.339947	20.403661
60.716512	1754.108438	20.408679
60.341610	1767.932764	20.413696
60.845805	1774.077653	20.418714
61.091203	1778.520785	20.423731
61.007747	1782.838389	20.428749
60.774317	1776.465092	20.433767
61.097730	1776.670341	20.438784
61.338860	1772.545895	20.443802
61.162642	1778.313870	20.448819
61.303835	1784.644671	20.453837
61.159870	1779.141094	20.458855
61.119588	1781.343840	20.463872
61.243039	1792.373373	20.468890
61.282205	1803.078355	20.473907
61.732312	1802.383384	20.478925
61.880350	1794.599965	20.483943
61.760663	1801.040819	20.488960
62.086621	1788.675747	20.493978
62.082434	1795.654053	20.498995
62.083366	1796.455480	20.504013
62.162700	1789.465422	20.509031
61.855897	1797.926776	20.514048
62.269887	1797.849671	20.519066
62.507940	1796.247259	20.524083
62.137842	1796.822422	20.529101
62.010347	1802.204111	20.534119
62.099019	1799.842295	20.539136
62.497749	1802.920305	20.544154
62.365363	1804.828116	20.549171
62.593265	1809.419151	20.554189
62.786646	1812.286131	20.559207
62.866103	1819.589105	20.564224
62.872286	1818.653971	20.569242
62.965909	1819.860701	20.574259
63.038687	1828.761603	20.579277
62.941169	1821.650741	20.584295
62.948717	1819.481438	20.589312
62.742357	1812.627373	20.594330
62.762803	1810.317204	20.599347
63.112766	1818.360723	20.604365
63.277974	1805.954393	20.609383
63.091923	1815.776081	20.614400
63.192448	1801.681952	20.619418
63.229670	1810.503171	20.624435
63.178578	1815.724642	20.629453
63.231179	1820.727993	20.634471
63.422159	1828.398627	20.639488
63.595862	1836.845150	20.644506
63.650253	1826.507394	20.649523
63.756866	1834.872841	20.654541
64.150993	1819.584237	20.659559
63.747110	1832.564189	20.664576
63.730128	1831.566387	20.669594
63.507282	1822.404767	20.674611
63.683197	1830.917216	20.679629
63.839548	1839.647317	20.684647
63.936625	1848.910530	20.689664
64.374340	1858.903378	20.694682
64.548143	1857.957924	20.699699
64.168123	1863.189594	20.704717
64.592358	1855.460980	20.709735
64.183186	1855.499413	20.714752
64.265462	1858.661418	20.719770
64.434906	1860.875704	20.724787
64.501470	1876.221957	20.729805
65.180472	1880.405095	20.734823
65.105231	1880.902794	20.739840
65.312521	1873.703427	20.744858
65.476214	1875.662982	20.749875
65.445210	1877.908478	20.754893
65.349289	1851.565259	20.759911
65.252266	1847.951050	20.764928
65.411221	1845.915966	20.769946
65.115997	1845.747304	20.774963
65.417134	1855.455291	20.779981
65.497089	1857.061797	20.784999
65.540381	1863.792889	20.790016
65.291877	1870.667247	20.795034
65.482125	1870.400909	20.800051
65.344127	1876.472243	20.805069
65.396396	1871.449343	20.810087
65.545895	1871.864712	20.815104
65.587560	1880.353904	20.820122
65.915847	1877.026934	20.825139
66.076910	1884.033197	20.830157
66.235164	1886.182954	20.835175
66.144078	1888.437806	20.840192
66.018851	1885.001556	20.845210
66.456543	1884.573611	20.850227
66.019257	1893.582362	20.855245
66.493960	1882.415404	20.860263
66.445087	1881.274237	20.865280
66.572346	1874.005277	20.870298
66.714999	1885.123399	20.875315
66.710192	1896.759965	20.880333
66.873191	1900.537436	20.885351
66.718880	1900.536188	20.890368
66.733506	1902.171804	20.895386
66.743450	1902.053462	20.900403
66.928348	1894.743959	20.905421
66.967110	1900.914019	20.910439
66.867133	1896.577556	20.915456
66.919898	1898.046282	20.920474
67.266466	1902.846092	20.925491
67.357986	1924.724398	20.930509
67.445487	1928.557812	20.935527
67.371464	1927.045003	20.940544
67.265202	1933.354422	20.945562
67.706282	1922.306287	20.950579
67.434915	1930.645418	20.955597
67.492463	1921.051913	20.960615
67.807531	1923.003684	20.965632
67.827296	1923.982071	20.970650
67.964690	1924.452978	20.975667
67.995468	1931.839318	20.980685
68.083647	1931.538376	20.985703
68.040600	1940.122839	20.990720
67.831204	1943.604835	20.995738
68.601524	1943.484876	21.000755
68.194445	1948.086444	21.005773
68.626386	1944.632865	21.010791
68.630113	1933.857951	21.015808
68.478729	1940.827673	21.020826
68.637178	1944.514340	21.025843
68.495378	1939.799356	21.030861
68.650142	1944.228237	21.035879
68.637527	1940.910148	21.040896
68.254988	1947.742286	21.045914
68.589008	1959.042107	21.050931
68.760394	1965.503976	21.055949
68.975450	1964.801412	21.060967
68.994058	1965.101458	21.065984
68.870671	1967.815802	21.071002
69.372443	1967.519895	21.076019
69.006955	1974.456690	21.081037
68.717055	1987.359045	21.086055
69.076449	1987.893223	21.091072
68.916872	1999.490833	21.096090
69.608778	1995.643306	21.101107
70.014214	2006.935194	21.106125
69.996241	2022.670291	21.111143
70.335189	2015.781742	21.116160
70.256792	2018.097753	21.121178
70.266064	2001.363534	21.126195
70.073478	1997.518011	21.131213
70.258444	2000.982802	21.136231
69.935899	2009.045903	21.141248
70.144234	2019.222883	21.146266
70.684095	2010.317973	21.151283
70.325060	2016.527915	21.156301
70.393518	2015.690376	21.161319
70.488906	2013.586272	21.166336
70.380552	2017.235595	21.171354
70.399501	2020.486387	21.176371
70.328367	2019.822067	21.181389
70.569965	2032.531246	21.186407
70.914640	2028.516858	21.191424
70.490736	2040.673222	21.196442
70.637649	2034.938078	21.201459
70.733388	2038.975369	21.206477
71.116629	2049.762634	21.211495
71.242983	2058.207166	21.216512
70.896474	2054.972600	21.221530
71.771482	2054.173594	21.226547
71.268992	2061.008671	21.231565
71.438643	2064.318061	21.236583
71.881353	2054.093293	21.241600
71.872307	2051.973884	21.246618
71.765033	2048.115068	21.251635
71.696152	2061.544822	21.256653
71.504266	2057.150043	21.261671
71.716841	2062.485176	21.266688
72.126031	2065.422743	21.271706
72.354720	2060.552210	21.276723
72.381920	2074.456186	21.281741
72.148705	2065.273963	21.286759
72.583277	2063.631463	21.291776
72.515026	2064.039712	21.296794
72.847952	2058.300847	21.301811
72.963018	2069.439159	21.306829
72.678597	2060.896099	21.311847
73.127185	2057.307358	21.316864
72.496037	2058.901513	21.321882
72.647415	2058.350877	21.326899
72.899207	2056.023593	21.331917
72.834084	2063.005179	21.336935
72.935591	2049.949006	21.341952
72.649608	2063.772340	21.346970
72.979323	2062.745795	21.351987
72.874319	2054.985880	21.357005
72.860349	2073.832156	21.362023
73.298509	2068.225233	21.367040
73.485248	2084.184143	21.372058
73.468766	2089.239352	21.377075
73.637431	2074.427466	21.382093
73.688502	2076.723328	21.387111
74.055597	2075.984465	21.392128
73.772692	2069.751315	21.397146
74.025603	2078.018355	21.402163
74.671218	2073.142870	21.407181
73.931154	2069.773907	21.412199
74.028262	2072.359259	21.417216
74.235060	2068.085449	21.422234
74.499332	2067.955912	21.427251
74.317787	2071.525119	21.432269
74.109776	2071.153519	21.437287
74.693517	2080.773447	21.442304
74.139270	2097.674593	21.447322
74.556556	2105.597303	21.452339
74.603588	2107.631854	21.457357
74.254858	2100.061352	21.462375
74.607834	2095.919419	21.467392
74.463236	2113.040835	21.472410
74.724106	2108.597644	21.477427
74.913207	2111.926107	21.482445
74.990050	2120.618229	21.487463
75.210038	2119.473058	21.492480
75.065649	2112.656569	21.497498
75.229006	2122.360906	21.502515
75.404215	2135.086806	21.507533
75.166598	2143.038910	21.512551
75.481322	2133.304260	21.517568
75.781731	2138.729887	21.522586
75.810941	2134.502648	21.527603
75.822173	2137.155031	21.532621
75.711060	2136.907205	21.537639
75.671278	2138.958431	21.542656
75.947560	2157.788008	21.547674
76.217203	2158.680165	21.552691
76.244896	2169.248290	21.557709
76.203318	2158.000589	21.562727
76.376990	2160.974840	21.567744
76.467055	2164.391319	21.572762
76.153153	2164.342331	21.577779
76.181955	2163.709785	21.582797
76.206530	2176.664306	21.587815
76.391256	2181.691370	21.592832
76.575927	2185.329821	21.597850
76.292732	2185.443318	21.602867
76.762845	2189.920998	21.607885
77.432800	2193.471271	21.612903
77.915709	2189.896096	21.617920
77.890274	2170.096371	21.622938
78.098809	2174.545342	21.627955
78.378486	2164.140756	21.632973
78.015604	2163.692275	21.637991
78.336437	2146.666404	21.643008
78.159132	2135.332545	21.648026
78.226093	2124.879046	21.653043
78.194145	2126.443035	21.658061
77.699703	2132.330100	21.663079
77.970117	2125.912948	21.668096
77.768921	2134.780916	21.673114
77.655018	2140.324700	21.678131
77.765353	2131.426642	21.683149
77.555122	2141.902400	21.688167
77.778518	2149.340897	21.693184
77.938442	2156.293793	21.698202
77.707850	2163.020300	21.703219
78.050363	2170.837911	21.708237
78.573036	2186.731987	21.713255
78.576221	2179.605302	21.718272
78.821343	2179.942672	21.723290
78.933763	2179.704226	21.728307
78.986666	2186.036293	21.733325
78.871335	2186.309856	21.738343
78.924883	2187.074705	21.743360
78.673763	2192.090731	21.748378
78.855418	2202.622282	21.753395
79.169395	2206.152238	21.758413
78.926438	2210.876649	21.763431
79.106793	2209.683992	21.768448
79.203746	2209.163917	21.773466
78.983733	2225.088446	21.778483
79.351138	2232.302574	21.783501
79.911232	2241.355040	21.788519
80.005063	2230.187202	21.793536
80.175814	2236.229525	21.798554
80.008425	2237.988189	21.803571
80.138316	2229.109129	21.808589
79.711036	2239.852279	21.813607
80.077051	2242.152779	21.818624
80.140555	2265.127831	21.823642
80.435729	2262.863197	21.828659
80.781558	2270.045984	21.833677
80.290769	2274.171490	21.838695
80.590018	2265.682634	21.843712
80.719015	2260.729733	21.848730
80.297459	2273.921050	21.853747
80.811703	2264.565543	21.858765
80.709292	2285.180533	21.863783
80.834496	2288.881915	21.868800
80.983992	2282.486690	21.873818
80.866370	2292.686171	21.878835
81.066510	2295.757316	21.883853
80.768215	2296.122487	21.888871
81.047491	2305.985611	21.893888
81.497346	2314.013803	21.898906
81.520112	2323.105785	21.903923
81.523213	2314.650389	21.908941
81.575300	2313.420888	21.913959
81.857303	2319.758360	21.918976
82.177694	2329.072266	21.923994
82.242877	2326.026032	21.929011
82.274343	2328.407034	21.934029
81.966463	2337.032920	21.939047
82.462278	2334.396193	21.944064
82.245009	2334.777153	21.949082
82.148780	2327.205114	21.954099
82.575463	2332.617452	21.959117
82.849371	2324.785803	21.964135
82.803300	2323.805127	21.969152
82.742904	2326.670673	21.974170
82.424814	2334.120964	21.979187
82.804538	2318.849958	21.984205
82.715388	2339.453479	21.989223
83.188157	2345.922215	21.994240
82.909322	2349.481376	21.999258
82.638915	2356.072134	22.004275
83.086189	2348.103024	22.009293
83.025936	2351.110571	22.014311
83.441584	2362.347443	22.019328
83.517172	2365.005620	22.024346
83.554472	2380.094914	22.029363
83.844823	2376.369791	22.034381
83.694721	2374.123974	22.039399
83.789852	2375.112744	22.044416
83.823908	2369.107869	22.049434
83.865659	2366.099992	22.054451
84.083877	2371.510083	22.059469
83.837605	2380.928021	22.064487
84.055611	2386.761053	22.069504
84.487863	2402.214935	22.074522
84.328447	2403.413761	22.079539
84.480552	2391.378318	22.084557
84.145857	2404.663511	22.089575
84.497792	2404.353056	22.094592
84.738374	2413.572127	22.099610
85.102501	2423.942846	22.104627
84.973627	2415.160791	22.109645
85.078417	2423.561513	22.114663
84.834529	2425.429941	22.119680
85.206952	2425.624413	22.124698
84.995592	2428.507167	22.129715
85.157880	2424.543180	22.134733
85.624233	2440.007565	22.139751
85.707370	2447.240791	22.144768
85.776448	2445.601510	22.149786
85.767979	2443.182145	22.154803
86.368098	2444.063891	22.159821
85.790984	2439.921512	22.164839
85.976061	2441.697907	22.169856
86.226811	2438.496523	22.174874
85.979349	2439.598600	22.179891
86.036936	2431.434487	22.184909
86.202377	2444.259964	22.189927
86.096911	2438.052712	22.194944
86.465437	2451.818626	22.199962
86.402796	2459.172390	22.204979
86.488968	2461.406028	22.209997
86.272161	2461.708018	22.215015
86.493393	2466.653735	22.220032
86.440339	2475.359941	22.225050
86.692733	2480.417583	22.230067
87.025846	2480.555055	22.235085
87.318575	2477.643793	22.240103
87.138098	2479.265654	22.245120
87.349009	2482.404586	22.250138
87.540171	2493.395605	22.255155
87.753785	2501.820449	22.260173
88.022482	2505.281770	22.265191
88.085960	2500.089679	22.270208
88.342056	2494.539375	22.275226
88.187064	2491.590512	22.280243
88.351895	2484.470100	22.285261
88.050823	2479.461013	22.290279
88.132012	2489.310895	22.295296
88.319036	2492.115854	22.300314
88.007985	2493.808542	22.305331
88.489470	2495.059080	22.310349
88.674659	2489.346236	22.315367
88.523683	2493.330517	22.320384
88.460304	2490.398951	22.325402
88.372494	2494.635348	22.330419
88.399761	2493.229806	22.335437
88.705048	2503.265726	22.340455
88.719800	2510.853630	22.345472
89.112006	2510.839881	22.350490
88.761412	2510.578839	22.355507
88.891907	2518.675781	22.360525
89.336893	2526.859473	22.365543
89.201023	2538.475833	22.370560
89.177551	2537.838789	22.375578
89.168578	2543.268523	22.380595
89.502984	2536.980128	22.385613
89.404071	2549.092548	22.390631
89.679409	2555.525823	22.395648
89.692399	2548.889806	22.400666
89.622716	2563.484635	22.405683
90.186252	2569.560597	22.410701
90.344783	2573.335750	22.415719
90.304876	2582.901558	22.420736
90.614196	2585.946286	22.425754
90.322693	2591.729315	22.430771
90.687088	2580.418141	22.435789
91.006530	2581.397248	22.440807
90.503252	2587.995943	22.445824
90.920534	2584.453001	22.450842
90.567916	2588.231995	22.455859
91.022988	2600.198234	22.460877
90.914854	2609.370706	22.465895
90.971447	2619.233957	22.470912
91.429880	2606.519469	22.475930
91.351786	2608.425224	22.480947
91.420956	2609.386489	22.485965
91.326252	2613.081148	22.490983
91.266000	2632.758943	22.496000
91.813219	2634.488443	22.501018
91.926993	2639.255264	22.506035
91.852180	2627.971413	22.511053
92.100017	2639.805830	22.516071
91.934924	2645.076852	22.521088
92.445375	2648.500562	22.526106
92.974449	2638.202052	22.531123
93.482346	2632.839736	22.536141
93.588265	2619.107069	22.541159
93.168363	2614.179566	22.546176
93.428295	2603.537942	22.551194
93.372836	2603.152046	22.556211
93.494089	2606.860422	22.561229
93.239084	2608.705352	22.566247
93.612076	2606.939838	22.571264
93.502219	2584.915168	22.576282
93.122219	2584.431468	22.581299
93.104211	2596.386147	22.586317
93.408855	2606.867227	22.591335
93.302434	2606.410365	22.596352
93.172590	2601.481890	22.601370
93.429177	2607.151186	22.606387
93.475894	2619.875345	22.611405
93.911566	2629.600681	22.616423
93.582499	2628.178017	22.621440
93.704971	2636.077432	22.626458
93.690110	2643.234469	22.631475
93.870908	2657.433743	22.636493
94.126945	2655.011040	22.641511
94.074602	2665.071171	22.646528
94.264335	2672.092216	22.651546
94.876318	2686.293815	22.656563
94.567570	2684.000069	22.661581
95.505838	2665.312176	22.666599
95.402806	2668.765127	22.671616
95.800871	2662.836035	22.676634
95.800179	2663.038104	22.681651
95.340190	2657.873814	22.686669
95.472910	2641.217615	22.691687
95.521119	2638.129786	22.696704
95.452661	2641.075539	22.701722
95.334879	2663.123044	22.706739
95.633168	2673.280079	22.711757
95.580119	2665.934722	22.716775
95.606721	2672.703433	22.721792
95.572055	2666.652349	22.726810
96.030081	2677.440975	22.731827
95.743229	2685.662935	22.736845
96.028034	2691.356269	22.741863
96.066074	2690.217299	22.746880
96.161816	2694.273674	22.751898
96.217349	2711.178294	22.756915
95.948143	2714.474075	22.761933
96.380491	2708.407076	22.766951
96.365815	2724.173836	22.771968
96.766644	2734.958777	22.776986
96.745949	2750.789619	22.782003
96.685522	2756.489382	22.787021
97.036182	2753.427034	22.792039
97.176273	2767.149855	22.797056
97.597744	2776.640777	22.802074
97.768410	2764.924113	22.807091
97.401228	2769.579642	22.812109
97.563515	2766.496122	22.817127
97.549073	2768.963232	22.822144
97.820298	2774.879632	22.827162
97.955306	2776.316689	22.832179
97.917826	2790.862504	22.837197
98.565336	2783.000894	22.842215
98.280325	2785.396513	22.847232
98.493267	2772.309840	22.852250
98.696921	2774.380048	22.857267
98.467308	2778.026311	22.862285
98.719897	2770.538643	22.867303
98.671603	2780.197388	22.872320
98.533861	2791.482816	22.877338
98.996794	2798.458220	22.882355
98.933171	2800.712066	22.887373
99.455163	2791.995762	22.892391
99.163695	2806.233966	22.897408
99.337460	2784.044963	22.902426
99.567388	2800.284990	22.907443
99.545268	2816.826228	22.912461
99.773560	2818.589621	22.917479
99.979839	2828.025704	22.922496
99.908601	2824.126393	22.927514
99.899700	2828.555727	22.932531
99.542047	2826.976538	22.937549
99.896387	2825.759909	22.942567
100.230544	2847.377484	22.947584
100.284776	2840.371989	22.952602
100.203061	2842.884300	22.957619
99.814065	2850.528896	22.962637
100.512512	2855.207901	22.967655
100.363944	2866.974786	22.972672
100.700873	2861.452813	22.977690
100.834747	2867.299101	22.982707
100.696786	2879.234771	22.987725
101.352936	2882.124557	22.992743
101.570533	2892.452084	22.997760
101.626460	2892.749492	23.002778
101.654394	2886.590748	23.007795
101.548082	2884.410639	23.012813
101.923399	2881.663195	23.017831
101.821163	2891.857464	23.022848
102.055415	2884.271609	23.027866
102.172386	2880.945795	23.032883
101.846776	2890.755082	23.037901
102.136279	2882.794519	23.042919
102.006810	2888.435640	23.047936
102.159389	2892.798820	23.052954
102.391082	2903.376646	23.057971
102.387329	2909.698852	23.062989
102.355772	2911.329126	23.068007
102.722254	2920.481516	23.073024
102.586370	2913.076364	23.078042
103.131657	2926.007164	23.083059
103.124396	2941.056527	23.088077
103.283481	2938.611008	23.093095
102.874560	2943.541347	23.098112
102.825991	2941.131314	23.103130
102.945194	2944.461348	23.108147
102.852395	2960.373034	23.113165
103.412662	2961.519814	23.118183
103.536073	2974.825630	23.123200
103.825273	2983.298898	23.128218
103.800210	2980.708458	23.133235
104.032397	2995.647996	23.138253
103.775737	2990.079532	23.143271
103.987719	2991.542497	23.148288
104.442050	3006.766224	23.153306
104.666759	3014.637263	23.158323
104.393184	3010.823067	23.163341
104.729594	3010.843256	23.168359
104.888899	3017.370509	23.173376
104.916879	3023.738312	23.178394
105.185220	3025.391339	23.183411
105.017249	3038.534265	23.188429
105.179902	3035.371740	23.193447
105.394321	3028.328608	23.198464
105.458131	3035.101131	23.203482
105.660192	3027.753780	23.208499
105.500159	3041.485665	23.213517
106.078157	3040.332039	23.218535
106.113845	3048.819560	23.223552
106.202020	3043.427788	23.228570
106.378432	3043.330862	23.233587
106.529927	3054.574579	23.238605
106.417583	3044.135837	23.243623
106.766167	3045.476542	23.248640
106.792591	3053.245913	23.253658
106.943058	3034.468833	23.258675
106.858263	3048.267912	23.263693
106.833793	3043.635365	23.268711
106.741711	3049.340150	23.273728
106.627245	3054.051089	23.278746
106.966833	3054.566293	23.283763
107.027509	3066.325979	23.288781
107.218962	3068.650610	23.293799
107.350849	3070.141831	23.298816
106.994498	3089.664234	23.303834
107.517306	3083.639836	23.308851
107.531605	3096.198949	23.313869
107.659029	3091.220816	23.318887
108.031205	3112.315188	23.323904
108.276306	3121.966310	23.328922
108.267704	3116.602208	23.333939
108.365645	3117.555865	23.338957
108.605967	3109.179939	23.343975
108.565087	3108.069010	23.348992
108.496954	3113.135705	23.354010
108.934136	3104.940592	23.359027
108.801350	3123.408796	23.364045
108.778108	3127.865686	23.369063
108.709759	3133.576270	23.374080
108.910061	3141.302827	23.379098
109.347062	3135.610540	23.384115
109.047363	3139.337223	23.389133
109.255512	3153.182301	23.394151
109.243035	3158.562269	23.399168
109.093832	3169.874967	23.404186
109.578787	3173.274344	23.409203
109.883878	3182.060846	23.414221
110.214379	3189.855525	23.419239
110.604661	3185.653881	23.424256
110.102916	3185.662538	23.429274
110.438699	3181.611407	23.434291
110.456975	3184.720488	23.439309
110.318035	3184.701065	23.444327
110.623370	3191.934714	23.449344
110.588086	3209.141151	23.454362
110.687963	3204.729069	23.459379
111.023105	3204.954605	23.464397
111.041436	3215.010353	23.469415
111.410541	3218.737077	23.474432
111.202854	3234.745797	23.479450
111.454852	3226.333281	23.484467
111.462013	3234.992606	23.489485
111.833576	3218.409153	23.494503
112.370007	3224.082417	23.499520
112.393382	3223.624268	23.504538
112.435923	3216.910812	23.509555
112.465344	3218.689427	23.514573
112.483706	3211.790369	23.519591
112.456364	3219.741770	23.524608
112.411436	3236.561529	23.529626
112.877686	3235.472633	23.534643
112.848534	3246.189113	23.539661
112.960233	3253.206755	23.544679
113.155339	3242.464382	23.549696
112.909859	3244.449919	23.554714
112.829365	3239.377871	23.559731
113.006901	3251.798056	23.564749
113.259366	3253.150586	23.569767
113.460323	3262.998027	23.574784
113.429901	3270.265045	23.579802
113.540413	3273.883703	23.584819
113.429655	3285.285172	23.589837
113.903875	3288.364315	23.594855
114.251876	3290.257457	23.599872
113.955420	3296.890488	23.604890
113.886183	3301.809068	23.609907
114.382223	3307.441306	23.614925
114.417196	3324.204520	23.619943
114.752649	3322.754088	23.624960
114.266249	3320.920312	23.629978
114.660857	3332.034824	23.634995
114.827338	3335.774183	23.640013
114.921647	3337.798357	23.645031
114.794805	3334.961750	23.650048
115.150846	3352.000088	23.655066
115.530674	3352.259699	23.660083
115.704048	3353.548803	23.665101
115.900836	3353.562326	23.670119
116.249446	3352.532769	23.675136
115.811515	3356.830190	23.680154
115.985100	3358.554813	23.685171
116.032380	3361.612067	23.690189
116.285353	3372.006954	23.695207
116.469370	3374.679961	23.700224
116.430112	3376.737560	23.705242
116.531733	3369.269992	23.710259
116.752630	3365.334548	23.715277
116.621698	3364.900419	23.720295
116.933962	3370.700161	23.725312
117.091854	3386.917216	23.730330
117.110105	3394.782692	23.735347
117.084180	3388.991966	23.740365
117.828583	3381.440099	23.745383
117.789757	3376.645580	23.750400
117.925306	3377.457680	23.755418
117.828236	3377.731574	23.760435
118.648198	3369.407310	23.765453
118.600489	3377.245174	23.770471
119.035990	3368.822959	23.775488
118.588784	3370.915665	23.780506
118.840094	3371.599276	23.785523
118.683014	3373.842495	23.790541
118.726111	3376.499568	23.795559
118.617798	3362.474603	23.800576
118.487401	3385.134097	23.805594
118.635517	3383.053186	23.810611
119.218397	3383.549460	23.815629
119.051733	3396.408387	23.820647
119.194939	3400.725807	23.825664
119.051545	3406.179887	23.830682
119.043006	3412.452516	23.835699
119.257656	3422.727153	23.840717
119.389636	3429.394526	23.845735
119.902991	3428.869554	23.850752
120.250751	3438.965667	23.855770
120.240201	3438.351828	23.860787
120.938094	3446.856372	23.865805
120.263070	3447.561117	23.870823
120.775873	3445.792694	23.875840
120.691855	3447.547963	23.880858
120.515327	3446.341353	23.885875
121.158632	3445.972895	23.890893
120.599039	3457.902000	23.895911
120.717285	3459.319629	23.900928
121.053908	3464.746335	23.905946
121.315051	3468.865508	23.910963
121.488741	3462.690187	23.915981
121.423824	3480.990382	23.920999
121.831084	3484.367197	23.926016
121.992049	3484.610387	23.931034
121.605609	3492.829282	23.936051
121.647554	3487.526636	23.941069
121.508724	3503.950960	23.946087
122.009806	3513.653969	23.951104
122.159834	3512.888879	23.956122
122.471163	3524.852868	23.961139
122.512591	3528.924201	23.966157
122.483209	3535.392646	23.971175
122.861329	3529.046601	23.976192
122.910945	3536.203424	23.981210
122.794226	3554.811597	23.986227
123.203978	3550.644713	23.991245
122.951825	3549.269967	23.996263
123.585430	3565.110123	24.001280
123.880322	3583.647930	24.006298
123.801405	3590.597538	24.011315
123.822994	3583.448495	24.016333
123.979711	3582.565581	24.021351
123.982012	3581.700397	24.026368
124.286938	3601.985200	24.031386
124.480797	3611.294224	24.036403
124.500089	3605.531107	24.041421
124.331315	3609.127034	24.046439
124.443037	3607.986003	24.051456
124.534591	3614.246275	24.056474
124.714477	3623.914133	24.061491
124.856354	3623.200808	24.066509
124.850449	3626.342136	24.071527
124.892349	3634.175628	24.076544
125.152642	3653.694165	24.081562
125.408384	3659.644830	24.086579
125.556202	3662.449766	24.091597
125.348487	3666.506263	24.096615
125.762187	3683.324471	24.101632
126.385954	3682.504555	24.106650
126.126577	3692.575400	24.111667
126.430026	3682.245144	24.116685
126.335493	3693.262442	24.121703
126.375218	3705.019495	24.126720
126.609368	3698.979867	24.131738
126.823753	3703.172654	24.136755
126.920780	3705.332164	24.141773
127.078999	3724.762515	24.146791
127.064414	3726.017784	24.151808
127.508324	3731.399462	24.156826
127.773609	3730.032515	24.161843
127.854008	3725.885307	24.166861
127.772884	3728.261930	24.171879
127.996669	3733.119226	24.176896
128.431634	3737.574365	24.181914
128.583241	3743.070992	24.186931
128.541511	3745.147954	24.191949
128.593320	3752.411833	24.196967
128.618139	3742.225923	24.201984
129.056659	3739.575823	24.207002
128.679038	3747.237963	24.212019
128.734034	3740.430842	24.217037
128.649473	3751.819059	24.222055
129.205385	3761.614665	24.227072
128.862110	3766.241476	24.232090
129.067742	3772.332542	24.237107
129.540346	3781.929662	24.242125
129.834812	3790.430899	24.247143
129.524479	3789.911066	24.252160
129.811411	3792.735394	24.257178
129.830549	3804.391561	24.262195
130.146808	3815.502788	24.267213
130.226611	3817.469307	24.272231
130.248055	3815.101912	24.277248
130.433974	3828.114565	24.282266
130.597603	3837.800851	24.287283
130.929999	3824.126693	24.292301
130.530487	3838.350968	24.297319
130.801040	3845.063202	24.302336
131.043310	3853.806158	24.307354
131.398885	3860.075910	24.312371
131.250051	3854.790233	24.317389
131.235413	3868.553767	24.322407
131.445177	3879.432270	24.327424
131.745421	3884.511266	24.332442
131.622895	3887.989579	24.337459
132.161697	3893.526969	24.342477
132.086333	3909.616685	24.347495
131.987510	3907.179627	24.352512
132.676061	3918.416020	24.357530
132.651238	3925.814994	24.362547
133.012919	3925.225248	24.367565
133.235904	3936.613043	24.372583
133.139238	3931.145628	24.377600
133.046799	3925.563930	24.382618
133.246484	3935.430875	24.387635
133.411275	3938.520431	24.392653
133.636852	3946.865185	24.397671
133.578607	3948.818491	24.402688
133.741522	3945.823050	24.407706
133.955494	3958.556833	24.412723
134.177529	3959.014618	24.417741
134.079413	3970.988993	24.422759
134.048511	3974.932812	24.427776
134.400666	3975.007366	24.432794
134.370549	3981.873776	24.437811
134.842616	3986.796643	24.442829
135.333256	4005.051905	24.447847
135.277770	4002.983685	24.452864
135.407982	3999.952294	24.457882
135.527965	3998.128196	24.462899
135.721220	3985.785436	24.467917
135.851384	3980.282690	24.472935
135.645637	3997.276541	24.477952
135.880415	3997.703936	24.482970
136.017607	4015.360887	24.487987
136.467954	4014.754179	24.493005
136.363025	4015.329152	24.498023
136.418645	4023.103864	24.503040
136.346253	4027.044685	24.508058
136.538042	4037.525234	24.513075
136.756453	4031.977170	24.518093
137.245579	4033.378135	24.523111
136.910558	4037.296721	24.528128
137.256757	4047.582796	24.533146
137.798613	4044.903939	24.538163
138.124340	4052.292575	24.543181
137.879066	4048.669440	24.548199
137.956163	4045.788345	24.553216
138.279195	4044.024161	24.558234
138.268075	4041.339866	24.563251
138.199227	4045.248576	24.568269
138.245269	4052.718632	24.573287
138.452961	4060.911565	24.578304
138.580436	4065.496723	24.583322
138.849969	4072.348077	24.588339
138.790758	4075.589315	24.593357
139.417029	4091.020760	24.598375
139.223293	4089.759971	24.603392
139.272022	4088.006927	24.608410
139.275386	4094.426286	24.613427
139.311649	4094.076578	24.618445
139.545669	4115.919585	24.623463
139.420519	4123.567826	24.628480
139.514767	4127.662633	24.633498
140.091553	4146.677921	24.638515
140.135691	4147.049781	24.643533
140.340786	4146.752694	24.648551
140.830157	4159.232270	24.653568
140.798326	4174.658932	24.658586
140.616922	4166.698527	24.663603
140.919581	4172.108641	24.668621
140.839229	4171.218421	24.673639
141.047307	4191.051831	24.678656
141.239766	4184.589274	24.683674
141.477883	4199.314259	24.688691
141.785063	4204.026133	24.693709
141.697462	4215.923282	24.698727
141.418961	4215.650984	24.703744
142.243478	4209.970626	24.708762
141.884036	4226.780304	24.713779
142.116572	4232.990434	24.718797
142.431254	4241.738086	24.723815
142.529482	4247.713470	24.728832
142.619848	4239.900100	24.733850
142.604189	4273.028151	24.738867
142.796022	4265.896521	24.743885
143.256706	4271.171591	24.748903
143.332424	4283.882940	24.753920
143.783765	4278.330100	24.758938
144.079773	4292.348599	24.763955
144.117513	4293.753578	24.768973
144.027418	4289.888448	24.773991
144.017310	4299.295866	24.779008
144.084858	4288.781050	24.784026
144.276314	4293.100642	24.789043
144.220707	4307.098143	24.794061
144.792434	4308.454707	24.799079
144.846598	4313.799393	24.804096
144.961506	4304.814330	24.809114
144.723570	4329.060448	24.814131
145.023050	4329.935447	24.819149
145.276969	4326.111440	24.824167
145.654889	4339.504893	24.829184
145.995204	4344.909197	24.834202
146.083547	4360.178427	24.839219
145.751222	4353.753325	24.844237
146.055185	4356.145829	24.849255
146.144140	4358.215140	24.854272
146.051094	4376.719470	24.859290
146.453222	4376.991410	24.864307
146.622969	4375.326813	24.869325
146.653223	4388.282040	24.874343
146.710420	4404.244241	24.879360
146.903562	4403.914292	24.884378
147.141410	4416.837219	24.889395
147.345302	4423.241256	24.894413
147.417816	4432.099300	24.899431
147.710731	4434.133710	24.904448
147.970220	4441.207714	24.909466
147.949923	4450.032871	24.914483
147.730911	4456.957277	24.919501
148.307752	4447.253171	24.924519
148.766709	4466.059883	24.929536
149.097846	4464.164988	24.934554
149.300390	4471.342560	24.939571
149.036586	4462.185966	24.944589
149.117992	4465.667359	24.949607
149.115635	4474.331917	24.954624
149.414954	4481.317670	24.959642
149.473827	4492.005403	24.964659
149.510386	4494.063949	24.969677
149.831657	4491.368870	24.974695
149.480998	4502.562260	24.979712
149.880438	4509.507185	24.984730
149.980189	4524.639054	24.989747
150.481211	4535.684084	24.994765
150.643457	4543.679148	24.999783
150.443580	4553.823272	25.004800
150.826459	4548.978568	25.009818
151.002915	4558.499112	25.014835
150.844240	4567.730949	25.019853
151.221569	4574.628840	25.024871
151.178508	4585.348279	25.029888
151.501207	4585.790408	25.034906
151.885931	4594.372664	25.039923
151.858991	4608.353309	25.044941
151.858698	4602.195219	25.049959
152.180900	4623.314923	25.054976
152.372744	4624.948447	25.059994
153.060887	4618.111862	25.065011
153.190232	4613.628566	25.070029
153.493790	4598.888300	25.075047
153.344919	4606.474153	25.080064
153.553475	4604.418413	25.085082
153.564338	4602.257729	25.090099
153.387834	4600.299816	25.095117
153.436612	4605.727493	25.100135
153.459854	4614.530170	25.105152
153.590155	4625.459372	25.110170
153.824637	4627.165167	25.115187
153.917271	4631.295060	25.120205
154.213422	4644.632030	25.125223
154.229310	4656.162996	25.130240
154.279745	4656.780084	25.135258
154.796596	4669.984864	25.140275
154.578269	4679.803665	25.145293
155.163431	4681.303361	25.150311
155.490236	4693.227840	25.155328
155.635442	4697.024454	25.160346
155.758389	4703.630577	25.165363
155.542397	4710.059054	25.170381
155.774977	4703.807858	25.175399
156.123041	4717.493473	25.180416
156.378034	4729.517536	25.185434
156.493781	4729.347982	25.190451
156.704968	4729.738036	25.195469
156.909531	4728.617201	25.200487
156.590529	4733.796004	25.205504
156.754532	4748.340434	25.210522
157.151849	4738.600996	25.215539
156.959459	4755.363059	25.220557
157.546722	4771.713364	25.225575
157.486329	4776.665688	25.230592
157.406157	4784.386115	25.235610
158.156930	4784.089286	25.240627
158.177162	4792.280172	25.245645
158.414501	4792.988110	25.250663
158.942578	4789.326490	25.255680
158.840891	4788.524784	25.260698
159.131474	4793.334090	25.265715
158.265456	4799.077852	25.270733
158.949390	4813.108957	25.275751
158.918940	4818.280736	25.280768
159.107102	4836.703877	25.285786
159.222813	4829.337677	25.290803
159.212053	4844.540678	25.295821
159.672415	4852.249576	25.300839
159.908079	4856.953818	25.305856
159.817129	4861.415363	25.310874
160.365886	4873.513730	25.315891
159.899546	4895.069005	25.320909
160.380130	4890.786628	25.325927
160.711136	4905.021104	25.330944
160.836823	4910.859861	25.335962
161.160550	4912.703298	25.340979
161.422306	4929.183334	25.345997
161.342665	4932.844557	25.351015
161.612692	4931.072760	25.356032
161.322621	4934.416379	25.361050
161.706998	4951.218240	25.366067
161.679706	4961.622958	25.371085
161.846675	4962.973149	25.376103
162.435387	4975.387321	25.381120
162.427711	4984.851533	25.386138
162.683925	4985.468159	25.391155
162.963917	4987.940235	25.396173
163.455169	4997.418312	25.401191
163.608303	4997.350255	25.406208
163.401821	5003.565873	25.411226
163.685852	4996.037671	25.416243
163.767909	5004.433667	25.421261
163.725194	5003.758497	25.426279
164.055210	5015.922580	25.431296
163.923585	5022.369596	25.436314
164.284839	5027.032234	25.441331
164.061950	5035.898687	25.446349
164.293007	5039.132783	25.451367
164.548736	5053.129734	25.456384
164.875935	5061.945278	25.461402
165.170050	5068.266055	25.466419
165.215839	5075.187347	25.471437
165.511231	5069.327118	25.476455
165.581719	5071.342570	25.481472
165.508757	5096.722451	25.486490
165.716579	5107.071709	25.491507
165.846691	5112.193323	25.496525
166.153919	5115.608119	25.501543
166.367188	5135.170298	25.506560
166.369648	5136.340943	25.511578
166.546402	5144.012052	25.516595
166.731080	5150.596101	25.521613
166.939795	5165.578969	25.526631
167.078006	5175.468787	25.531648
167.302121	5185.319985	25.536666
167.542447	5191.415599	25.541683
167.449864	5214.324012	25.546701
167.985804	5212.526571	25.551719
168.095576	5220.255488	25.556736
168.137538	5242.319144	25.561754
168.315774	5233.339546	25.566771
168.499661	5242.578364	25.571789
168.686927	5256.611384	25.576807
168.824177	5260.725005	25.581824
169.065393	5273.171388	25.586842
169.693921	5282.151611	25.591859
169.489439	5287.991389	25.596877
169.596222	5297.422161	25.601895
169.946089	5299.637193	25.606912
170.443349	5315.960968	25.611930
170.755685	5309.173168	25.616947
170.714885	5321.350996	25.621965
170.820434	5307.796268	25.626983
170.968094	5303.713984	25.632000
170.752961	5310.101504	25.637018
171.101222	5320.454271	25.642035
171.674613	5318.859319	25.647053
171.733450	5324.714930	25.652071
171.846758	5318.317956	25.657088
171.753745	5321.119610	25.662106
172.109793	5328.522989	25.667123
171.836892	5335.999038	25.672141
172.059669	5338.057097	25.677159
172.423151	5350.058368	25.682176
172.539545	5375.140853	25.687194
172.702436	5372.899590	25.692212
172.501392	5377.630924	25.697229
173.177442	5392.345515	25.702247
173.320200	5391.654081	25.707264
172.931727	5396.032660	25.712282
173.319549	5405.135646	25.717300
173.677535	5417.866975	25.722317
173.698243	5431.528339	25.727335
174.075477	5439.136795	25.732352
174.200103	5452.033897	25.737370
174.283970	5449.972224	25.742388
174.820963	5466.002704	25.747405
174.532203	5469.036875	25.752423
175.109613	5476.753069	25.757440
174.807477	5479.798794	25.762458
175.245563	5490.421762	25.767476
175.804752	5500.356695	25.772493
175.854845	5507.874068	25.777511
176.066522	5498.769184	25.782528
175.845516	5504.270698	25.787546
176.624392	5519.790085	25.792564
176.435462	5527.025868	25.797581
176.323009	5533.618438	25.802599
176.648898	5523.062687	25.807616
176.610990	5543.573497	25.812634
176.936017	5557.629493	25.817652
177.136952	5556.108292	25.822669
176.996518	5573.096603	25.827687
177.191059	5575.591533	25.832704
177.229191	5592.911909	25.837722
177.746977	5610.792094	25.842740
177.893742	5611.504697	25.847757
177.994437	5631.624709	25.852775
178.380699	5633.815178	25.857792
178.161290	5647.027976	25.862810
178.439765	5656.432203	25.867828
178.812296	5670.897558	25.872845
179.029782	5684.837819	25.877863
179.493223	5672.581270	25.882880
179.724387	5682.485302	25.887898
179.748054	5687.020745	25.892916
180.023513	5702.460837	25.897933
180.214619	5708.409616	25.902951
180.268242	5710.793928	25.907968
180.383531	5724.617555	25.912986
180.349887	5735.317266	25.918004
181.151835	5736.177240	25.923021
180.778585	5752.434915	25.928039
181.236589	5763.039159	25.933056
181.533479	5764.931056	25.938074
181.514861	5783.014872	25.943092
181.698744	5785.227398	25.948109
181.699609	5788.304914	25.953127
182.221307	5800.524909	25.958144
182.224126	5811.888186	25.963162
182.226100	5814.457322	25.968180
182.365143	5831.478120	25.973197
182.167259	5840.565188	25.978215
182.739183	5855.877182	25.983232
182.738408	5863.945558	25.988250
183.024867	5873.654845	25.993268
183.606004	5880.600420	25.998285
183.499653	5890.598149	26.003303
184.239609	5904.867595	26.008320
184.311073	5906.655713	26.013338
184.445602	5914.523118	26.018356
184.471447	5912.779775	26.023373
184.957531	5941.691274	26.028391
185.126753	5925.098978	26.033408
185.039999	5939.970653	26.038426
185.167354	5942.719154	26.043444
185.878296	5947.428600	26.048461
185.572352	5961.049675	26.053479
185.900622	5965.231571	26.058496
186.073090	5973.168854	26.063514
186.248393	5983.994012	26.068532
186.381806	5990.671576	26.073549
186.382591	5996.476466	26.078567
186.352892	5989.227135	26.083584
186.830929	6009.213057	26.088602
186.870503	6015.737939	26.093620
187.299907	6012.975297	26.098637
187.435867	6034.245590	26.103655
187.807833	6038.752148	26.108672
187.913676	6033.612426	26.113690
187.708424	6033.249776	26.118708
188.039150	6052.207521	26.123725
187.860467	6058.608566	26.128743
188.410074	6068.100217	26.133760
188.747043	6090.620877	26.138778
188.604024	6089.443593	26.143796
189.036048	6091.718536	26.148813
189.094946	6118.856501	26.153831
189.382724	6112.255313	26.158848
189.662696	6122.335071	26.163866
189.587067	6134.850313	26.168884
189.981894	6134.504719	26.173901
189.691939	6153.148837	26.178919
189.993485	6165.864224	26.183936
190.650852	6180.203566	26.188954
190.683018	6181.435943	26.193972
191.020824	6174.050406	26.198989
191.670879	6192.324092	26.204007
192.232010	6189.487253	26.209024
192.091308	6206.135275	26.214042
192.101427	6204.612162	26.219060
192.437094	6196.159997	26.224077
192.365200	6205.265511	26.229095
192.688925	6204.227049	26.234112
192.789926	6217.974358	26.239130
192.833914	6222.093247	26.244148
193.306730	6222.174286	26.249165
193.290694	6224.181241	26.254183
193.608435	6228.266981	26.259200
193.458424	6242.564768	26.264218
193.420143	6247.128935	26.269236
194.055851	6248.330486	26.274253
193.878466	6269.024815	26.279271
194.656338	6256.324340	26.284288
195.269410	6260.016874	26.289306
195.574716	6274.215388	26.294324
195.759927	6272.516646	26.299341
195.614432	6276.283090	26.304359
195.705747	6270.255381	26.309376
196.020524	6276.639653	26.314394
195.871131	6275.791644	26.319412
196.088095	6278.620945	26.324429
196.385209	6292.091556	26.329447
196.220534	6290.144244	26.334464
196.465006	6298.076773	26.339482
196.423814	6304.396521	26.344500
196.801456	6315.345051	26.349517
196.758430	6335.175703	26.354535
196.896884	6338.847446	26.359552
196.935742	6356.436752	26.364570
196.867076	6377.912921	26.369588
197.635257	6376.271772	26.374605
197.795239	6406.421696	26.379623
197.656448	6407.260864	26.384640
198.235554	6420.924420	26.389658
197.877964	6443.878791	26.394676
198.951085	6445.750925	26.399693
198.928807	6463.021554	26.404711
199.248435	6465.490820	26.409728
199.819116	6481.895757	26.414746
199.859737	6495.747376	26.419764
200.530703	6484.670155	26.424781
200.377644	6485.798808	26.429799
200.422499	6490.324839	26.434816
200.547050	6492.499338	26.439834
200.459005	6496.247412	26.444852
200.785877	6495.786124	26.449869
200.591808	6514.535636	26.454887
200.484019	6520.117685	26.459904
201.285318	6529.721915	26.464922
200.732184	6552.653202	26.469940
201.399181	6568.134085	26.474957
201.542783	6574.996524	26.479975
202.112926	6585.858425	26.484992
202.107597	6598.113658	26.490010
202.137684	6620.625928	26.495028
202.529652	6621.344592	26.500045
202.795142	6639.460785	26.505063
203.133319	6641.216921	26.510080
203.140849	6653.858467	26.515098
203.043520	6671.892282	26.520116
203.747898	6668.253354	26.525133
203.710726	6696.272081	26.530151
203.873851	6706.667088	26.535168
204.031569	6722.315780	26.540186
204.309937	6738.643344	26.545204
204.484556	6739.746251	26.550221
204.623619	6755.476794	26.555239
205.149840	6770.973454	26.560256
205.820607	6773.811100	26.565274
206.072010	6771.757920	26.570292
206.233056	6771.552886	26.575309
206.391357	6787.536160	26.580327
206.687940	6792.474491	26.585344
207.322204	6791.946399	26.590362
207.478635	6794.340101	26.595380
207.588816	6788.249306	26.600397
207.449133	6794.922331	26.605415
207.785351	6790.769323	26.610432
208.359092	6798.110999	26.615450
207.938850	6808.117059	26.620468
208.336402	6803.683017	26.625485
208.387327	6815.329850	26.630503
208.435974	6822.118776	26.635520
208.967284	6833.236256	26.640538
208.895495	6837.199687	26.645556
208.787326	6841.607573	26.650573
209.231831	6858.379739	26.655591
209.261334	6858.097324	26.660608
209.251889	6871.953866	26.665626
209.466290	6890.210846	26.670644
209.771492	6898.244668	26.675661
210.314574	6911.500662	26.680679
210.130597	6915.825665	26.685696
210.685411	6933.647720	26.690714
210.643518	6943.077236	26.695732
210.794069	6956.381748	26.700749
211.392368	6969.613404	26.705767
211.330257	6971.763356	26.710784
211.508838	6989.988131	26.715802
211.358143	6999.636650	26.720820
211.895571	7015.652644	26.725837
211.961094	7026.776467	26.730855
211.946288	7047.503186	26.735872
212.281908	7059.326828	26.740890
212.815183	7073.383140	26.745908
212.975333	7080.116920	26.750925
213.151547	7097.515085	26.755943
213.335937	7108.191123	26.760960
213.763183	7119.277627	26.765978
214.072330	7129.280793	26.770996
214.095745	7133.046370	26.776013
214.322583	7137.351661	26.781031
214.401870	7151.974336	26.786048
214.474240	7158.178836	26.791066
214.518646	7175.594439	26.796084
214.612662	7185.151291	26.801101
215.234931	7201.176337	26.806119
215.470511	7221.807448	26.811136
216.005836	7236.488620	26.816154
216.053552	7240.866019	26.821172
215.780343	7248.832205	26.826189
216.439399	7263.399430	26.831207
216.664855	7258.493291	26.836224
217.014530	7277.528279	26.841242
217.020167	7292.244609	26.846260
217.350516	7302.860155	26.851277
217.724914	7316.957174	26.856295
217.660785	7323.997451	26.861312
218.313391	7333.287473	26.866330
217.970934	7345.160045	26.871348
218.311525	7347.919756	26.876365
218.673453	7364.708399	26.881383
218.919153	7373.667184	26.886400
219.627430	7376.470676	26.891418
219.454477	7390.182594	26.896436
219.528618	7390.281516	26.901453
220.095581	7404.616956	26.906471
220.081448	7420.573961	26.911488
220.439032	7427.226620	26.916506
220.673125	7444.212023	26.921524
220.403510	7448.831446	26.926541
220.856714	7467.089704	26.931559
220.725883	7467.381539	26.936576
221.346209	7489.045331	26.941594
221.530923	7500.586534	26.946612
221.824396	7506.229530	26.951629
222.372313	7510.955298	26.956647
222.560387	7527.761687	26.961664
222.748487	7526.112891	26.966682
223.218316	7535.314668	26.971700
222.741005	7542.990753	26.976717
223.516393	7558.600820	26.981735
223.127282	7584.377472	26.986752
223.855149	7581.839627	26.991770
224.132247	7594.348303	26.996788
223.967645	7602.692345	27.001805
224.282222	7603.151606	27.006823
224.189183	7624.569889	27.011840
224.590253	7627.717998	27.016858
225.109167	7646.171404	27.021876
225.155266	7656.354716	27.026893
225.939190	7655.127724	27.031911
226.254901	7657.604077	27.036928
226.660956	7655.498311	27.041946
226.727750	7660.453712	27.046964
226.463549	7668.349223	27.051981
227.015907	7675.132653	27.056999
227.562374	7673.159713	27.062016
228.199674	7678.468267	27.067034
228.229790	7684.670054	27.072052
228.065968	7681.816424	27.077069
228.261710	7682.442563	27.082087
228.226110	7692.117722	27.087104
228.260325	7697.823238	27.092122
228.261392	7708.414519	27.097140
228.306046	7716.353517	27.102157
228.688721	7739.405768	27.107175
228.561366	7740.221116	27.112192
228.764702	7756.472875	27.117210
229.011153	7767.808905	27.122228
229.256666	7783.375381	27.127245
229.594554	7796.073617	27.132263
229.392196	7833.271758	27.137280
229.800964	7840.090232	27.142298
230.336835	7857.398397	27.147316
230.083257	7868.218830	27.152333
230.581537	7876.617642	27.157351
230.963039	7909.939854	27.162368
231.270112	7913.661428	27.167386
231.578380	7931.257654	27.172404
231.887882	7944.673885	27.177421
232.369441	7955.282053	27.182439
232.544864	7973.445156	27.187456
232.391434	7972.054696	27.192474
233.113836	7983.941840	27.197492
232.850811	7993.961948	27.202509
233.445321	8006.781383	27.207527
233.221175	8033.622136	27.212544
233.447672	8046.359986	27.217562
233.725254	8055.576170	27.222580
234.230155	8069.795515	27.227597
234.349690	8082.474274	27.232615
234.492312	8095.840829	27.237632
234.913028	8104.892690	27.242650
235.503889	8128.872742	27.247668
235.529508	8133.799954	27.252685
235.578424	8137.498626	27.257703
235.997196	8149.373165	27.262720
236.150481	8169.235216	27.267738
236.421989	8170.705124	27.272756
236.359321	8188.078372	27.277773
236.849276	8206.738899	27.282791
236.716610	8219.665380	27.287808
237.183767	8235.134591	27.292826
237.832071	8245.890603	27.297844
237.581059	8265.253752	27.302861
238.104470	8276.070267	27.307879
238.313002	8297.360298	27.312896
238.841404	8297.344305	27.317914
238.697405	8314.742963	27.322932
238.998015	8329.919323	27.327949
239.240916	8346.455890	27.332967
239.404914	8362.016603	27.337984
239.817610	8365.516619	27.343002
240.516471	8367.191515	27.348020
240.499075	8378.973100	27.353037
241.184137	8388.138640	27.358055
241.316906	8397.254417	27.363072
241.669580	8391.125340	27.368090
241.773603	8403.165857	27.373108
241.749220	8414.156134	27.378125
242.114021	8419.084286	27.383143
242.310198	8425.288882	27.388160
242.565656	8437.264803	27.393178
242.500456	8437.442252	27.398196
242.638794	8449.973112	27.403213
242.957404	8459.549330	27.408231
242.811275	8479.489900	27.413248
243.250412	8495.178372	27.418266
243.600235	8498.183072	27.423284
244.217863	8518.118432	27.428301
244.752123	8520.756616	27.433319
245.082458	8517.374462	27.438336
245.415330	8527.109505	27.443354
245.658821	8533.281514	27.448372
245.541291	8536.895682	27.453389
245.931655	8534.369216	27.458407
245.732070	8534.744382	27.463424
246.260269	8533.891800	27.468442
246.543244	8536.853244	27.473460
246.653157	8551.885838	27.478477
246.881632	8551.926012	27.483495
246.393665	8564.747039	27.488512
246.539863	8579.540383	27.493530
247.451350	8579.736259	27.498548
247.209237	8604.815835	27.503565
247.272767	8620.168256	27.508583
247.861287	8629.863552	27.513600
248.125906	8647.713510	27.518618
248.424719	8654.315782	27.523636
248.743309	8685.991724	27.528653
249.106220	8688.735537	27.533671
248.913159	8697.242357	27.538688
249.346639	8716.354186	27.543706
249.681479	8725.593363	27.548724
249.717830	8744.372411	27.553741
250.263158	8755.293138	27.558759
250.661871	8770.328304	27.563776
250.668230	8781.891764	27.568794
251.119822	8800.312612	27.573812
251.215983	8807.331656	27.578829
251.244202	8826.108896	27.583847
251.712428	8839.728381	27.588864
252.018672	8861.439533	27.593882
252.640741	8865.058590	27.598900
252.700972	8887.868866	27.603917
252.757242	8896.128590	27.608935
253.012359	8907.100903	27.613952
253.031760	8918.905517	27.618970
253.409472	8927.374096	27.623988
253.678118	8963.295158	27.629005
253.954141	8971.410203	27.634023
254.317635	8982.851888	27.639040
254.228006	8996.994024	27.644058
254.860012	9002.370091	27.649076
255.250056	9018.925395	27.654093
255.115510	9024.029323	27.659111
255.580490	9041.378053	27.664128
255.608437	9054.068582	27.669146
256.160231	9072.423587	27.674164
256.355790	9075.828101	27.679181
256.783154	9090.085564	27.684199
257.019765	9103.198271	27.689216
257.121814	9124.126974	27.694234
257.791402	9122.197863	27.699252
257.844063	9141.959810	27.704269
258.066058	9152.419650	27.709287
258.511409	9172.230995	27.714304
258.312674	9183.507762	27.719322
258.746995	9198.626134	27.724340
259.060221	9212.389998	27.729357
259.047354	9227.739031	27.734375
259.223228	9233.280894	27.739392
259.556371	9255.793403	27.744410
259.710270	9262.910975	27.749428
260.210779	9290.335312	27.754445
260.332622	9298.859682	27.759463
260.697187	9315.460262	27.764480
260.792906	9338.353969	27.769498
261.246632	9354.268220	27.774516
261.054271	9364.132833	27.779533
261.649256	9376.609015	27.784551
261.719154	9394.215332	27.789568
262.158249	9413.285964	27.794586
262.845826	9419.076569	27.799604
262.935644	9425.736913	27.804621
263.056122	9445.984309	27.809639
263.291310	9450.187813	27.814656
263.709703	9458.877623	27.819674
263.963997	9464.893559	27.824692
264.233318	9490.721901	27.829709
264.585656	9493.694802	27.834727
264.449845	9499.177924	27.839744
264.606330	9516.325708	27.844762
264.956357	9535.909176	27.849780
265.781271	9540.352399	27.854797
266.274653	9552.955022	27.859815
266.470689	9555.213474	27.864832
266.801411	9550.703940	27.869850
266.788776	9567.300327	27.874868
267.203811	9576.514816	27.879885
267.427681	9585.815902	27.884903
267.609981	9597.996557	27.889920
267.790795	9617.003421	27.894938
268.147252	9618.387606	27.899956
268.518638	9635.075814	27.904973
268.474562	9641.570803	27.909991
268.791843	9655.817425	27.915008
269.154495	9666.432464	27.920026
269.656536	9669.227382	27.925044
270.384840	9665.745178	27.930061
270.489945	9679.292367	27.935079
270.874062	9675.450145	27.940096
270.786489	9691.887817	27.945114
271.044095	9699.431429	27.950132
271.068123	9705.625369	27.955149
271.046002	9722.144439	27.960167
271.483506	9740.161129	27.965184
271.750883	9760.480716	27.970202
271.727215	9764.683548	27.975220
271.559872	9778.427933	27.980237
272.263443	9804.735315	27.985255
272.734473	9823.981364	27.990272
272.508263	9847.159457	27.995290
273.057633	9856.978316	28.000308
273.103434	9873.988954	28.005325
273.122928	9893.318001	28.010343
273.813196	9915.636792	28.015360
273.757335	9935.425951	28.020378
273.972653	9954.140473	28.025396
274.643593	9977.024347	28.030413
275.004932	9995.211008	28.035431
275.374506	10016.620024	28.040448
275.223440	10033.974032	28.045466
276.272137	10040.194840	28.050484
276.613225	10056.512424	28.055501
276.800171	10064.771268	28.060519
277.512353	10069.828906	28.065536
277.558557	10083.467651	28.070554
277.880194	10099.308387	28.075572
278.174909	10111.418203	28.080589
278.185445	10111.637550	28.085607
278.546680	10130.045373	28.090624
278.799024	10141.498765	28.095642
278.701999	10157.142670	28.100660
279.208196	10174.151368	28.105677
279.136942	10196.042833	28.110695
279.568204	10205.390876	28.115712
279.481309	10224.746302	28.120730
279.590851	10251.478321	28.125748
280.236732	10262.662135	28.130765
280.312237	10285.980084	28.135783
281.048554	10293.522029	28.140800
280.759401	10313.287919	28.145818
281.227273	10324.764702	28.150836
281.690042	10340.031131	28.155853
281.949571	10363.020577	28.160871
282.409559	10372.080068	28.165888
282.396385	10386.542882	28.170906
283.049029	10410.333149	28.175924
283.254629	10426.031201	28.180941
283.201339	10433.825586	28.185959
283.558501	10458.043960	28.190976
283.734524	10474.037137	28.195994
284.207071	10489.665268	28.201012
284.684788	10505.870410	28.206029
284.693413	10526.392145	28.211047
284.976210	10537.531614	28.216064
285.047393	10551.731988	28.221082
285.444783	10577.908162	28.226100
286.238268	10588.879748	28.231117
286.408578	10602.818450	28.236135
286.907442	10617.410116	28.241152
287.188379	10632.916641	28.246170
287.336244	10651.721302	28.251188
287.842586	10659.068708	28.256205
288.189525	10672.714740	28.261223
288.484721	10678.115320	28.266240
288.748543	10697.034585	28.271258
288.786864	10711.249669	28.276276
289.051612	10713.977496	28.281293
289.291776	10746.821626	28.286311
289.459404	10754.786985	28.291328
289.621321	10769.892214	28.296346
289.797942	10793.261362	28.301364
290.517749	10805.428590	28.306381
290.239500	10838.890358	28.311399
290.719750	10848.992045	28.316416
291.328468	10869.935398	28.321434
291.227411	10882.502014	28.326452
291.602658	10900.763175	28.331469
291.925977	10926.345136	28.336487
292.337980	10936.170166	28.341504
292.870519	10960.930234	28.346522
293.201718	10979.106762	28.351540
293.388790	10993.996705	28.356557
293.738003	11014.459637	28.361575
293.909104	11032.395912	28.366592
294.242075	11043.177392	28.371610
294.081005	11064.673383	28.376628
294.620110	11075.883784	28.381645
295.096538	11096.004935	28.386663
296.250992	11082.298461	28.391680
297.279562	11092.188617	28.396698
297.596013	11094.924238	28.401716
297.905961	11091.614263	28.406733
297.802177	11099.138927	28.411751
298.171661	11091.493910	28.416768
298.434637	11093.723184	28.421786
298.342526	11103.159475	28.426804
298.604820	11103.544878	28.431821
298.596877	11121.029173	28.436839
298.902309	11129.109010	28.441856
298.951889	11129.587522	28.446874
299.301827	11156.757037	28.451892
299.363366	11161.786816	28.456909
299.604973	11180.214301	28.461927
299.786604	11187.805078	28.466944
300.091695	11209.629667	28.471962
299.931516	11228.476551	28.476980
300.489986	11235.882379	28.481997
300.714264	11264.568279	28.487015
300.732927	11281.928597	28.492032
300.958495	11292.622743	28.497050
301.017939	11325.391827	28.502068
301.822578	11343.296078	28.507085
302.087749	11360.198138	28.512103
302.704402	11386.966504	28.517120
303.100726	11409.572825	28.522138
302.907262	11433.979230	28.527156
303.338805	11446.299115	28.532173
303.886544	11472.832043	28.537191
304.029158	11494.887501	28.542208
304.515151	11508.771417	28.547226
304.620987	11540.807415	28.552244
304.827900	11553.070771	28.557261
305.200218	11576.176770	28.562279
305.299774	11597.866458	28.567296
305.892514	11622.820117	28.572314
306.044641	11643.405990	28.577332
306.386036	11662.642546	28.582349
306.873373	11688.193699	28.587367
307.041146	11704.460768	28.592384
307.333794	11723.367112	28.597402
307.552414	11748.401286	28.602420
307.932673	11768.051862	28.607437
308.272311	11803.010590	28.612455
308.757210	11812.041644	28.617472
309.481040	11826.583446	28.622490
309.555588	11848.201533	28.627508
310.180836	11874.741911	28.632525
310.021167	11883.349182	28.637543
310.456249	11904.895418	28.642560
311.042559	11920.690179	28.647578
311.315106	11940.850297	28.652596
311.828009	11949.545506	28.657613
311.643880	11969.820958	28.662631
312.551024	11989.819179	28.667648
312.765907	11996.865150	28.672666
313.179188	12013.858416	28.677684
313.625376	12015.989811	28.682701
313.832526	12031.439516	28.687719
314.098036	12038.708129	28.692736
314.762300	12054.895049	28.697754
314.501070	12079.085490	28.702772
315.317608	12097.070712	28.707789
315.343590	12103.865099	28.712807
315.235063	12110.367821	28.717824
315.620295	12120.743920	28.722842
315.673348	12148.109504	28.727860
315.942461	12165.302182	28.732877
316.774372	12179.101166	28.737895
316.856721	12196.471360	28.742912
317.594643	12218.643396	28.747930
317.733706	12233.478645	28.752948
318.140072	12246.342941	28.757965
318.423760	12256.014971	28.762983
318.595318	12285.714787	28.768000
318.791765	12300.316958	28.773018
318.626045	12319.727869	28.778036
319.175160	12339.318020	28.783053
319.660957	12362.022080	28.788071
319.706556	12382.675872	28.793088
320.092170	12409.434303	28.798106
320.414003	12426.956889	28.803124
321.276478	12441.752307	28.808141
321.284509	12454.906117	28.813159
321.139009	12479.044319	28.818176
321.743152	12486.857198	28.823194
322.124656	12514.993190	28.828212
322.189020	12528.946662	28.833229
322.619537	12544.693577	28.838247
322.702448	12558.805229	28.843264
322.874931	12585.164480	28.848282
323.314367	12613.263181	28.853300
323.426489	12632.321697	28.858317
323.732778	12664.887325	28.863335
324.233786	12685.025304	28.868352
324.597603	12707.868767	28.873370
325.121198	12730.150561	28.878388
325.853344	12737.820464	28.883405
325.901885	12759.873105	28.888423
326.479099	12777.258368	28.893440
326.662302	12795.459699	28.898458
327.422162	12813.868103	28.903476
327.619490	12826.086416	28.908493
328.002365	12845.295622	28.913511
328.433820	12858.980616	28.918528
328.420593	12877.184186	28.923546
328.716791	12890.770264	28.928564
328.857421	12924.969452	28.933581
329.059099	12940.695485	28.938599
329.456358	12959.618365	28.943616
330.179709	12991.977527	28.948634
330.126174	13004.945520	28.953652
330.450170	13020.962043	28.958669
330.614146	13046.366443	28.963687
330.989167	13077.014756	28.968704
331.545482	13100.476081	28.973722
331.828175	13131.233591	28.978740
332.795655	13124.315696	28.983757
333.115722	13143.487616	28.988775
333.310269	13168.988473	28.993792
333.706285	13182.492907	28.998810
334.098202	13200.557926	29.003828
334.340923	13216.423060	29.008845
334.872913	13237.598899	29.013863
334.954159	13256.763905	29.018880
335.347847	13267.865630	29.023898
335.344832	13284.915383	29.028916
335.460963	13301.539237	29.033933
335.834568	13327.546111	29.038951
336.617194	13349.740944	29.043968
337.214555	13368.648872	29.048986
337.700290	13386.860515	29.054004
338.015798	13378.556667	29.059021
338.185859	13411.931106	29.064039
338.204533	13434.848129	29.069056
338.607822	13442.177942	29.074074
338.764286	13463.352498	29.079092
338.821540	13481.261465	29.084109
339.417538	13501.410793	29.089127
339.394516	13534.708138	29.094144
339.846151	13546.410483	29.099162
340.413394	13570.334904	29.104180
340.548445	13604.791981	29.109197
341.018415	13619.652594	29.114215
341.310783	13640.938823	29.119232
341.796913	13662.665442	29.124250
342.097413	13686.745224	29.129268
343.108569	13700.062683	29.134285
343.862071	13697.276895	29.139303
344.041408	13710.183854	29.144320
344.247477	13712.021246	29.149338
344.596156	13727.965052	29.154356
344.528257	13732.185131	29.159373
344.928806	13743.096592	29.164391
345.509289	13757.914846	29.169408
345.836536	13761.915517	29.174426
345.978441	13780.746341	29.179444
346.062075	13796.001982	29.184461
346.474732	13802.187299	29.189479
346.411199	13836.429393	29.194496
346.951753	13848.039133	29.199514
347.065180	13868.800834	29.204532
347.172057	13885.748754	29.209549
347.886861	13912.000162	29.214567
347.656529	13929.335364	29.219584
348.270942	13964.312165	29.224602
348.794411	13999.397930	29.229620
348.995878	14007.024654	29.234637
349.527143	14050.288484	29.239655
349.456356	14073.128624	29.244672
349.507167	14096.865682	29.249690
350.203678	14117.540036	29.254708
350.337402	14156.381633	29.259725
350.665596	14188.908579	29.264743
351.360097	14218.751081	29.269760
351.857794	14237.309064	29.274778
352.587530	14249.792795	29.279796
352.853899	14285.215968	29.284813
353.205635	14296.577473	29.289831
353.521893	14318.940792	29.294848
354.115417	14337.281841	29.299866
354.422749	14367.437495	29.304884
354.530133	14388.090173	29.309901
355.234547	14391.283802	29.314919
355.984826	14410.671097	29.319936
356.080165	14422.227339	29.324954
356.602979	14441.965883	29.329972
357.028893	14460.225771	29.334989
357.157894	14471.906283	29.340007
357.445136	14495.145952	29.345024
358.012504	14514.002851	29.350042
358.273087	14527.181944	29.355060
358.586711	14552.476640	29.360077
358.846859	14555.821572	29.365095
358.907979	14588.280249	29.370112
359.243140	14611.831568	29.375130
359.591552	14629.863670	29.380148
360.097632	14646.901709	29.385165
360.595588	14668.842392	29.390183
360.788367	14704.363071	29.395200
361.183596	14721.914257	29.400218
361.736969	14743.303205	29.405236
361.896598	14770.393863	29.410253
362.345135	14787.115701	29.415271
362.747905	14820.854310	29.420288
363.055592	14835.554814	29.425306
363.104739	14852.136767	29.430324
363.774776	14878.538600	29.435341
363.693387	14903.086777	29.440359
363.942153	14933.062957	29.445376
364.350536	14952.586146	29.450394
364.999677	14988.882691	29.455412
365.070275	15004.747695	29.460429
365.971018	15028.640987	29.465447
366.162125	15055.954538	29.470464
366.084136	15088.262024	29.475482
366.886519	15104.815360	29.480500
366.750217	15138.117357	29.485517
367.580922	15158.203485	29.490535
367.669174	15191.439034	29.495552
367.925278	15214.460198	29.500570
368.587699	15230.217463	29.505588
368.840317	15262.783277	29.510605
369.222063	15298.983081	29.515623
369.517084	15313.982797	29.520640
370.094380	15335.116030	29.525658
370.500044	15354.321074	29.530676
370.740734	15374.129774	29.535693
371.185346	15399.386253	29.540711
371.283254	15421.664849	29.545728
371.464168	15447.104564	29.550746
372.204221	15477.652552	29.555764
372.560957	15507.139091	29.560781
373.077476	15536.777662	29.565799
372.898072	15554.984400	29.570816
373.149592	15583.761042	29.575834
373.966297	15614.559450	29.580852
374.043626	15649.733505	29.585869
374.969059	15672.518373	29.590887
375.182459	15704.945766	29.595904
375.891399	15725.367276	29.600922
376.280467	15748.453658	29.605940
376.501745	15778.618625	29.610957
376.817399	15796.919069	29.615975
377.256828	15826.146880	29.620992
377.359038	15843.255182	29.626010
378.137767	15866.738996	29.631028
378.420310	15904.796676	29.636045
378.997143	15914.488106	29.641063
379.426543	15940.442496	29.646080
379.381961	15969.531113	29.651098
379.982514	15986.182962	29.656116
379.970323	16023.301369	29.661133
380.681914	16044.881913	29.666151
381.316501	16084.274805	29.671168
381.215239	16107.226347	29.676186
381.958314	16127.952491	29.681204
382.059768	16154.075083	29.686221
382.314043	16181.437258	29.691239
382.677039	16207.866624	29.696256
383.541720	16230.172073	29.701274
384.006591	16253.518881	29.706292
384.404601	16288.094629	29.711309
384.990198	16303.425730	29.716327
385.104407	16321.388508	29.721344
385.368367	16341.595700	29.726362
385.949750	16363.645363	29.731380
386.051061	16389.844100	29.736397
386.883191	16418.174709	29.741415
387.190391	16437.569882	29.746432
387.333804	16461.803962	29.751450
387.960398	16483.821458	29.756468
388.333188	16508.032521	29.761485
388.365495	16541.604436	29.766503
388.902815	16558.639321	29.771520
389.097864	16586.898807	29.776538
389.973069	16598.707647	29.781556
390.402792	16635.417331	29.786573
390.743816	16649.498150	29.791591
391.373832	16665.763836	29.796608
391.311964	16694.726747	29.801626
391.842225	16714.974993	29.806644
392.163804	16746.534529	29.811661
392.459951	16772.848743	29.816679
393.061585	16782.069305	29.821696
393.370616	16802.964824	29.826714
393.860482	16818.775534	29.831732
394.253782	16839.042075	29.836749
394.187205	16856.859783	29.841767
394.627318	16882.232624	29.846784
395.339635	16914.467527	29.851802
395.944642	16922.313698	29.856820
396.218905	16938.865569	29.861837
396.235614	16968.085128	29.866855
396.902313	16987.266966	29.871872
397.033091	17014.084186	29.876890
397.609710	17027.531652	29.881908
397.781359	17057.633710	29.886925
398.356766	17065.585621	29.891943
398.375923	17096.763257	29.896960
398.673269	17124.982340	29.901978
399.066757	17150.890264	29.906996
399.125878	17190.807732	29.912013
399.682812	17217.508354	29.917031
400.607476	17251.722739	29.922048
400.667172	17282.565879	29.927066
401.322377	17302.065674	29.932084
401.831726	17325.858532	29.937101
401.970760	17349.235290	29.942119
402.397063	17372.279927	29.947136
403.091697	17409.098297	29.952154
403.387360	17436.844317	29.957172
403.915969	17464.105596	29.962189
403.833801	17504.961691	29.967207
404.207273	17535.797447	29.972224
404.315347	17560.916494	29.977242
404.965716	17591.396533	29.982260
405.452459	17632.578104	29.987277
405.748188	17657.200591	29.992295
406.944558	17683.729665	29.997312
408.462622	17686.942490	30.002330
409.199167	17697.383817	30.007348
409.541765	17706.673580	30.012365
409.764625	17722.406575	30.017383
410.100524	17712.966905	30.022400
410.281682	17736.925074	30.027418
410.872542	17743.390319	30.032436
411.176575	17762.774688	30.037453
410.965599	17780.659950	30.042471
411.268067	17797.391367	30.047488
411.348137	17820.480966	30.052506
411.914546	17845.011016	30.057524
412.311482	17882.498884	30.062541
412.747575	17899.291711	30.067559
413.131454	17923.913450	30.072576
413.658978	17952.972851	30.077594
413.891141	17969.601651	30.082612
414.285259	17995.599054	30.087629
414.789055	18019.216750	30.092647
415.123186	18046.101663	30.097664
415.513220	18081.771609	30.102682
416.261157	18104.612276	30.107700
416.480477	18120.800993	30.112717
416.795951	18153.519853	30.117735
417.350461	18170.610348	30.122752
417.774138	18200.690746	30.127770
417.961724	18222.519568	30.132788
418.552471	18250.893617	30.137805
418.935313	18279.969717	30.142823
419.259551	18299.882139	30.147840
419.612908	18330.100033	30.152858
419.980327	18349.329822	30.157876
420.662035	18373.577264	30.162893
420.730947	18404.641867	30.167911
421.454580	18423.866815	30.172928
421.532967	18449.048493	30.177946
422.361202	18471.346428	30.182964
422.933741	18489.040873	30.187981
422.724628	18518.809643	30.192999
423.404078	18526.815457	30.198016
424.352743	18560.598842	30.203034
424.330048	18575.246249	30.208052
424.526599	18606.790386	30.213069
424.731172	18623.790458	30.218087
424.728936	18650.210542	30.223104
425.201474	18694.845940	30.228122
425.862280	18718.522174	30.233140
426.230250	18749.957729	30.238157
426.505974	18780.813847	30.243175
427.536612	18810.478506	30.248192
427.819423	18834.877071	30.253210
428.551982	18857.297746	30.258228
428.967025	18878.137943	30.263245
429.519048	18914.624441	30.268263
429.673332	18940.748896	30.273280
429.815042	18971.670404	30.278298
430.473998	19003.364314	30.283316
430.965173	19026.606147	30.288333
431.001239	19060.393489	30.293351
431.778016	19078.587358	30.298368
432.405590	19113.937930	30.303386
432.750339	19146.641272	30.308404
433.369128	19168.934712	30.313421
433.224186	19202.510409	30.318439
433.940665	19226.930401	30.323456
434.874782	19246.432966	30.328474
435.432405	19269.399402	30.333492
436.146706	19291.766563	30.338509
436.214510	19312.421211	30.343527
436.931084	19330.675232	30.348544
437.211057	19366.990129	30.353562
437.639571	19385.560709	30.358580
438.121651	19394.684262	30.363597
438.299142	19434.174109	30.368615
438.776336	19456.072951	30.373632
439.506922	19484.452307	30.378650
439.769866	19505.563250	30.383668
440.002987	19526.982111	30.388685
440.376271	19567.983288	30.393703
440.813864	19589.616780	30.398720
441.343338	19615.791135	30.403738
441.636169	19643.114301	30.408756
442.122079	19671.374075	30.413773
442.107348	19709.934095	30.418791
442.582865	19739.275937	30.423808
443.212393	19767.576671	30.428826
444.043091	19791.783738	30.433844
444.144261	19824.759900	30.438861
443.980284	19865.542083	30.443879
444.301823	19905.079955	30.448896
444.841502	19940.426757	30.453914
445.176272	19984.353681	30.458932
446.270805	20019.254125	30.463949
446.001219	20061.310428	30.468967
446.964336	20095.985067	30.473984
447.238977	20129.711847	30.479002
447.327271	20171.308321	30.484020
448.002639	20206.078497	30.489037
448.091129	20248.995567	30.494055
448.651900	20289.311996	30.499072
449.417537	20328.004468	30.504090
449.635811	20368.646056	30.509108
451.027836	20401.820270	30.514125
451.252467	20433.179766	30.519143
451.404677	20456.634027	30.524160
451.681851	20495.377601	30.529178
451.987618	20532.423547	30.534196
452.924120	20555.048201	30.539213
453.199157	20589.931927	30.544231
454.123672	20617.903656	30.549248
454.298404	20656.947813	30.554266
454.995528	20687.248528	30.559284
455.041211	20714.883348	30.564301
455.555062	20750.747407	30.569319
456.053141	20777.667433	30.574336
456.356515	20821.013531	30.579354
456.925377	20842.627976	30.584372
457.530297	20879.109913	30.589389
458.305610	20919.090965	30.594407
458.953216	20938.551376	30.599424
459.516919	20959.572840	30.604442
459.828385	20997.673925	30.609460
460.299539	21010.338162	30.614477
460.792623	21038.061743	30.619495
460.829432	21070.380283	30.624512
461.599063	21102.256241	30.629530
461.815415	21130.275765	30.634548
462.551592	21159.225332	30.639565
462.551028	21189.376388	30.644583
463.318363	21209.791452	30.649600
464.274241	21242.839126	30.654618
463.998986	21254.836246	30.659636
464.943635	21292.567643	30.664653
465.080042	21329.439272	30.669671
465.420750	21352.353471	30.674688
465.999050	21403.139005	30.679706
465.966557	21436.302962	30.684724
466.724406	21469.931548	30.689741
467.131563	21510.356541	30.694759
467.719729	21540.991459	30.699776
468.026272	21583.397298	30.704794
468.287753	21611.157743	30.709812
469.009364	21656.222376	30.714829
469.082289	21687.658039	30.719847
469.699436	21738.760633	30.724864
470.753317	21781.979374	30.729882
470.980958	21820.221472	30.734900
471.622389	21843.765509	30.739917
471.945881	21881.853796	30.744935
472.594110	21910.875031	30.749952
473.158897	21940.951860	30.754970
473.505350	21979.618069	30.759988
474.173532	22015.024428	30.765005
474.544178	22052.871917	30.770023
475.443471	22077.292287	30.775040
476.164210	22094.802650	30.780058
476.739574	22126.457769	30.785076
477.226920	22138.747415	30.790093
477.968152	22165.208142	30.795111
478.056249	22186.235454	30.800128
478.520931	22208.935472	30.805146
478.622892	22233.732909	30.810164
479.377349	22257.108197	30.815181
480.008503	22281.336773	30.820199
480.105120	22315.322489	30.825216
480.990251	22328.908845	30.830234
481.204235	22358.497517	30.835252
481.590594	22387.016813	30.840269
482.017653	22417.058942	30.845287
482.169997	22460.868150	30.850304
482.903525	22482.420853	30.855322
482.779957	22512.390878	30.860340
483.150550	22540.950762	30.865357
484.035905	22572.760538	30.870375
483.857985	22597.229194	30.875392
484.573556	22645.494324	30.880410
485.006777	22687.225659	30.885428
485.525693	22717.841592	30.890445
485.882240	22756.078070	30.895463
486.337904	22800.068286	30.900480
487.166870	22830.692996	30.905498
487.483179	22863.489103	30.910516
487.543784	22899.655114	30.915533
488.423426	22955.572881	30.920551
488.790465	22985.694724	30.925568
489.421731	23025.190645	30.930586
489.565744	23072.604278	30.935604
489.997069	23112.580143	30.940621
490.900360	23145.436991	30.945639
491.438120	23189.396333	30.950656
492.498939	23222.841725	30.955674
492.502910	23253.355402	30.960692
493.263377	23290.108258	30.965709
494.035816	23325.424906	30.970727
494.449969	23353.694825	30.975744
495.184803	23376.158237	30.980762
495.640523	23414.513245	30.985780
496.453598	23445.501565	30.990797
496.894071	23471.928715	30.995815
496.735901	23501.444328	31.000832
497.681167	23537.202058	31.005850
498.210699	23575.798648	31.010868
499.043684	23595.062213	31.015885
499.745264	23612.071380	31.020903
500.590676	23650.637899	31.025920
501.007347	23673.258603	31.030938
500.679658	23704.304855	31.035956
501.082572	23720.583359	31.040973
501.853083	23749.961085	31.045991
501.961861	23776.579298	31.051008
502.412502	23811.839483	31.056026
502.653476	23852.212980	31.061044
503.489801	23887.122574	31.066061
503.819322	23921.409697	31.071079
504.150743	23968.183327	31.076096
504.652758	23999.922369	31.081114
504.971195	24050.597170	31.086132
505.733389	24079.926125	31.091149
506.212964	24122.481078	31.096167
506.878189	24170.037357	31.101184
507.358997	24198.133799	31.106202
507.958203	24235.444328	31.111220
508.652660	24268.051178	31.116237
509.008143	24303.794675	31.121255
509.620217	24342.594758	31.126272
510.507975	24371.348495	31.131290
510.923853	24410.172934	31.136308
511.436555	24426.788807	31.141325
511.955940	24455.972855	31.146343
512.568619	24498.084491	31.151360
513.280820	24532.098231	31.156378
513.255374	24555.231120	31.161396
513.598376	24592.594841	31.166413
514.151787	24626.172144	31.171431
514.358814	24666.110213	31.176448
515.178931	24701.181743	31.181466
515.753217	24722.591048	31.186484
516.602634	24761.652011	31.191501
517.454865	24793.590574	31.196519
517.331670	24818.489477	31.201536
517.772345	24842.466459	31.206554
518.426784	24874.176844	31.211572
519.073178	24902.905727	31.216589
520.033192	24909.821453	31.221607
520.445885	24943.914118	31.226624
520.977397	24970.752491	31.231642
521.043020	24996.911403	31.236660
521.678068	25017.919755	31.241677
522.349017	25048.995894	31.246695
522.161326	25088.225268	31.251712
522.776214	25115.057174	31.256730
523.336276	25152.318633	31.261748
523.761989	25192.318501	31.266765
524.211129	25231.758676	31.271783
524.301188	25254.482575	31.276800
524.659230	25295.238896	31.281818
525.487868	25341.432763	31.286836
525.770203	25380.589536	31.291853
526.555804	25425.640120	31.296871
526.950642	25473.184714	31.301888
527.748629	25508.261105	31.306906
528.116651	25553.933117	31.311924
528.825479	25599.526899	31.316941
529.524208	25639.820101	31.321959
529.698870	25681.515794	31.326976
530.620316	25722.810930	31.331994
531.179736	25762.475130	31.337012
531.786228	25813.874239	31.342029
532.257381	25844.262258	31.347047
532.751371	25878.274337	31.352064
533.315076	25921.382478	31.357082
533.865048	25958.526927	31.362100
534.344968	25997.540385	31.367117
535.014931	26036.897205	31.372135
535.812032	26081.745235	31.377152
536.626075	26100.002993	31.382170
537.607975	26136.195748	31.387188
538.162514	26171.090000	31.392205
538.926480	26176.785351	31.397223
539.199291	26218.100322	31.402240
539.503689	26249.823136	31.407258
540.215632	26276.199092	31.412276
540.433029	26305.748841	31.417293
541.239997	26340.768409	31.422311
541.239820	26368.443495	31.427328
541.645910	26413.694414	31.432346
542.277490	26442.851247	31.437364
542.428824	26490.290791	31.442381
543.120563	26519.160290	31.447399
543.308987	26571.726096	31.452416
544.130224	26612.311856	31.457434
545.223383	26639.115584	31.462452
545.860590	26667.330180	31.467469
546.886641	26696.122609	31.472487
547.241343	26733.791851	31.477504
548.083798	26755.338542	31.482522
548.411977	26786.685612	31.487540
548.508247	26812.658828	31.492557
549.176283	26849.754941	31.497575
549.972601	26885.573447	31.502592
550.509775	26918.405016	31.507610
551.029474	26941.822349	31.512628
551.443512	26977.864854	31.517645
551.723029	27005.592073	31.522663
551.817471	27045.514467	31.527680
552.396372	27090.499832	31.532698
553.205875	27131.056860	31.537716
553.362841	27166.608824	31.542733
553.912621	27202.327226	31.547751
553.942574	27251.196858	31.552768
554.699334	27279.147208	31.557786
555.037805	27324.872069	31.562804
555.477438	27368.046856	31.567821
556.265225	27405.548803	31.572839
557.157760	27451.984053	31.577856
557.522527	27485.424848	31.582874
557.916497	27532.911225	31.587892
558.760501	27579.322720	31.592909
559.221200	27620.895720	31.597927
559.593144	27668.284716	31.602944
559.953582	27716.181244	31.607962
560.601499	27765.088638	31.612980
561.391911	27813.247120	31.617997
562.627614	27847.330339	31.623015
562.811218	27895.861579	31.628032
563.350146	27931.690402	31.633050
564.052763	27982.688193	31.638068
564.406107	28022.711253	31.643085
565.074220	28066.414478	31.648103
565.776409	28109.707980	31.653120
565.785393	28150.360064	31.658138
566.377674	28194.612612	31.663156
566.957828	28257.335777	31.668173
567.238499	28305.524213	31.673191
567.755951	28357.322876	31.678208
568.496285	28404.946985	31.683226
569.147402	28454.588726	31.688244
569.911213	28512.505705	31.693261
570.632537	28556.795837	31.698279
570.916121	28599.814232	31.703296
571.560355	28659.166069	31.708314
572.352554	28706.846015	31.713332
573.038543	28759.656055	31.718349
573.809847	28808.407690	31.723367
574.501787	28852.545021	31.728384
574.971206	28902.696514	31.733402
575.518898	28936.718006	31.738420
576.009996	28993.895031	31.743437
576.984495	29026.440698	31.748455
577.364686	29079.703700	31.753472
577.581816	29117.379810	31.758490
578.442287	29166.409176	31.763508
578.790692	29220.012495	31.768525
579.621185	29265.981156	31.773543
580.408779	29314.149943	31.778560
580.419155	29365.100929	31.783578
581.086898	29402.372408	31.788596
581.552078	29452.032875	31.793613
582.144101	29493.045647	31.798631
583.233734	29545.137501	31.803648
583.580779	29593.546192	31.808666
584.263959	29636.624657	31.813684
585.257094	29683.434910	31.818701
586.068524	29720.425439	31.823719
586.392162	29759.489409	31.828736
587.004674	29799.001524	31.833754
588.197489	29819.940679	31.838772
588.843501	29858.923050	31.843789
589.627312	29893.939705	31.848807
589.961028	29925.082145	31.853824
590.748598	29966.311944	31.858842
591.232537	29990.294606	31.863860
591.179425	30026.516358	31.868877
592.172093	30058.896492	31.873895
592.412508	30090.774313	31.878912
592.883575	30130.005671	31.883930
593.467400	30163.688557	31.888948
593.814046	30200.499460	31.893965
594.178451	30229.880306	31.898983
594.885652	30273.019578	31.904000
595.053869	30319.163232	31.909018
595.695937	30359.221767	31.914036
596.343264	30411.707057	31.919053
596.492716	30454.434160	31.924071
597.405033	30496.852957	31.929088
598.004314	30550.679862	31.934106
598.542780	30597.714690	31.939124
599.137100	30647.964784	31.944141
599.834040	30696.226780	31.949159
600.849719	30740.994155	31.954176
601.109504	30794.400448	31.959194
601.655327	30835.960404	31.964212
602.465588	30893.440701	31.969229
602.951863	30937.469140	31.974247
603.503618	30977.896933	31.979264
603.768467	31027.187818	31.984282
604.604700	31079.695971	31.989300
605.626265	31126.467155	31.994317
606.766932	31161.240772	31.999335
607.740781	31191.760796	32.004352
608.182650	31224.715261	32.009370
608.660364	31265.957970	32.014388
609.367118	31310.743065	32.019405
609.948441	31343.530617	32.024423
610.622627	31382.922382	32.029440
611.040848	31432.525397	32.034458
611.606196	31467.041407	32.039476
612.038495	31502.216663	32.044493
612.806606	31556.607810	32.049511
613.371515	31603.590237	32.054528
613.633306	31643.375419	32.059546
614.135345	31690.026463	32.064564
614.712900	31745.604623	32.069581
615.248683	31795.746508	32.074599
616.283314	31851.664704	32.079616
617.279523	31899.958781	32.084634
617.887577	31929.721344	32.089652
618.703704	31973.896610	32.094669
619.107636	32023.813025	32.099687
619.849518	32061.463395	32.104704
620.038108	32107.652115	32.109722
620.886910	32144.603245	32.114740
621.021167	32193.108047	32.119757
621.713162	32232.770490	32.124775
622.368866	32284.981070	32.129792
623.029817	32339.138078	32.134810
623.349974	32393.019544	32.139828
623.952323	32447.097450	32.144845
624.439181	32499.081978	32.149863
625.520632	32547.876362	32.154880
626.068545	32596.551617	32.159898
626.601931	32639.330924	32.164916
627.263315	32689.866334	32.169933
627.729311	32744.351873	32.174951
628.717430	32777.855961	32.179968
629.284905	32836.744975	32.184986
630.059146	32886.953518	32.190004
630.814189	32931.393205	32.195021
631.777797	32975.566605	32.200039
632.512607	33011.380097	32.205056
632.968713	33062.511024	32.210074
633.713901	33108.242313	32.215092
634.381957	33141.411166	32.220109
634.893556	33170.343366	32.225127
635.482449	33202.304484	32.230144
635.985977	33242.668327	32.235162
637.004910	33270.598666	32.240180
637.599714	33301.686569	32.245197
637.941092	33331.834045	32.250215
638.547591	33369.773384	32.255232
638.914503	33419.408085	32.260250
639.767912	33446.030458	32.265268
639.922924	33500.876167	32.270285
640.215732	33546.255253	32.275303
641.178966	33579.050098	32.280320
641.777591	33640.907950	32.285338
642.589851	33679.732538	32.290356
643.355334	33720.119746	32.295373
643.596226	33772.411264	32.300391
643.754237	33819.335583	32.305408
644.532826	33875.551958	32.310426
645.608456	33929.572668	32.315444
646.042972	33990.926027	32.320461
646.071510	34054.043467	32.325479
647.032758	34101.380772	32.330496
647.405195	34162.516692	32.335514
648.194168	34222.443598	32.340532
648.721231	34284.004688	32.345549
649.363390	34350.631253	32.350567
650.455969	34407.912917	32.355584
650.743302	34468.563502	32.360602
651.568327	34531.906119	32.365620
652.628844	34589.642163	32.370637
652.994262	34647.897535	32.375655
653.904975	34701.800487	32.380672
654.598284	34767.389839	32.385690
655.462790	34813.137884	32.390708
656.267159	34874.297145	32.395725
657.054960	34932.784712	32.400743
657.873482	34980.879634	32.405760
658.408086	35038.351035	32.410778
658.966014	35085.209595	32.415796
659.642370	35139.061630	32.420813
660.232910	35192.332832	32.425831
660.961712	35238.242023	32.430848
661.512867	35284.507748	32.435866
662.082739	35333.660133	32.440884
662.712706	35384.232212	32.445901
663.590611	35445.938080	32.450919
664.524020	35501.306415	32.455936
665.085597	35555.057245	32.460954
665.366912	35598.197957	32.465972
666.218651	35658.214013	32.470989
666.929926	35727.856461	32.476007
667.950852	35766.936944	32.481024
668.450484	35825.136728	32.486042
668.845379	35875.550566	32.491060
670.039475	35929.918366	32.496077
670.375670	35975.915566	32.501095
671.216068	36020.911232	32.506112
672.259664	36071.749353	32.511130
672.882983	36106.516899	32.516148
673.865427	36147.342881	32.521165
674.651670	36197.728177	32.526183
675.264648	36237.751925	32.531200
675.507459	36286.723485	32.536218
676.065966	36328.880407	32.541236
676.662068	36374.566121	32.546253
677.299364	36425.379817	32.551271
678.148891	36475.559906	32.556288
678.632007	36526.309321	32.561306
679.106316	36564.863031	32.566324
680.081358	36601.682216	32.571341
680.251348	36644.880322	32.576359
681.111206	36692.656542	32.581376
681.693466	36744.826388	32.586394
682.124778	36798.606967	32.591412
682.465601	36840.754528	32.596429
683.391837	36897.575623	32.601447
683.964188	36950.487325	32.606464
684.381884	37006.629094	32.611482
684.883954	37060.260207	32.616500
686.247879	37116.223348	32.621517
686.782533	37179.125866	32.626535
687.279399	37233.738328	32.631552
687.917317	37295.392076	32.636570
688.916454	37347.391004	32.641588
689.734187	37405.495002	32.646605
690.524403	37463.729908	32.651623
691.028374	37512.948176	32.656640
691.952685	37568.127286	32.661658
692.350573	37625.955779	32.666676
693.117891	37683.461335	32.671693
693.743938	37750.878858	32.676711
694.539012	37807.368680	32.681728
694.986784	37869.262354	32.686746
695.589641	37936.955980	32.691764
696.538354	37986.276836	32.696781
697.093003	38055.584506	32.701799
698.023127	38109.923081	32.706816
699.130935	38161.344278	32.711834
699.815443	38219.351075	32.716852
700.753757	38255.407358	32.721869
701.650680	38325.130560	32.726887
702.338952	38372.197386	32.731904
703.270684	38425.088405	32.736922
703.722565	38470.870610	32.741940
704.556476	38522.493400	32.746957
705.105253	38579.782433	32.751975
705.833146	38613.918064	32.756992
706.301165	38673.344671	32.762010
707.688995	38712.272261	32.767028
708.439619	38755.023780	32.772045
709.336491	38802.400556	32.777063
709.847189	38842.558929	32.782080
710.908948	38894.615100	32.787098
711.409135	38940.144157	32.792116
712.042070	38979.967570	32.797133
712.523583	39036.035151	32.802151
713.238519	39078.337554	32.807168
713.982361	39140.277329	32.812186
713.963153	39180.082476	32.817204
714.531832	39225.082918	32.822221
715.356320	39292.215102	32.827239
716.039372	39347.891658	32.832256
717.327344	39412.479428	32.837274
717.403636	39479.248046	32.842292
718.146839	39531.557709	32.847309
718.477206	39593.253274	32.852327
719.260493	39654.650845	32.857344
719.755443	39719.065752	32.862362
721.044698	39787.575318	32.867380
721.487375	39843.271595	32.872397
722.166154	39909.473448	32.877415
722.887020	39968.307738	32.882432
724.006880	40031.962269	32.887450
724.480522	40093.750787	32.892468
725.259000	40143.792409	32.897485
726.036613	40211.446993	32.902503
727.049560	40265.841348	32.907520
727.690883	40309.163157	32.912538
728.365705	40363.585096	32.917556
729.150624	40405.069705	32.922573
729.482467	40455.485133	32.927591
729.800618	40522.990863	32.932608
730.755550	40581.891566	32.937626
731.352180	40643.396883	32.942644
731.750271	40705.072413	32.947661
732.707567	40766.989930	32.952679
733.519477	40830.049660	32.957696
734.640044	40886.838381	32.962714
734.981137	40953.962414	32.967732
736.101755	41012.813194	32.972749
736.363496	41089.746445	32.977767
736.973195	41145.318865	32.982784
738.037126	41202.996319	32.987802
738.692108	41270.142030	32.992820
739.741750	41337.106346	32.997837
740.319923	41407.262230	33.002855
741.154280	41466.690053	33.007872
741.795285	41535.204845	33.012890
742.551125	41598.914300	33.017908
743.509432	41663.212230	33.022925
743.836875	41729.777883	33.027943
744.926922	41793.233492	33.032960
746.132420	41841.650366	33.037978
747.119015	41904.338150	33.042996
748.231566	41956.722639	33.048013
748.955936	42008.326501	33.053031
749.818764	42066.676329	33.058048
750.482327	42115.886535	33.063066
751.265566	42180.655964	33.068084
752.088734	42222.220295	33.073101
753.006206	42270.442614	33.078119
753.782287	42336.674631	33.083136
754.181598	42376.698748	33.088154
754.587910	42425.469011	33.093172
755.406839	42486.268153	33.098189
756.114625	42537.622849	33.103207
756.818828	42615.030182	33.108224
757.614196	42667.611215	33.113242
758.667445	42732.726055	33.118260
759.203641	42788.680925	33.123277
759.763997	42852.968390	33.128295
760.395526	42916.106479	33.133312
760.989975	42974.013475	33.138330
761.888895	43046.123343	33.143348
762.554768	43108.396442	33.148365
763.537329	43166.452251	33.153383
764.245002	43236.119441	33.158400
765.542466	43288.826197	33.163418
766.144982	43346.941641	33.168436
767.270503	43407.518497	33.173453
768.068193	43454.686798	33.178471
768.384495	43515.731473	33.183488
769.898439	43557.418498	33.188506
770.163419	43622.829451	33.193524
771.151059	43678.962982	33.198541
771.505174	43734.777814	33.203559
772.670250	43788.410868	33.208576
773.277014	43835.502174	33.213594
774.297208	43897.804568	33.218612
774.931348	43955.391697	33.223629
775.387347	44020.331323	33.228647
776.057408	44082.480007	33.233664
776.794785	44135.756690	33.238682
777.698877	44190.810253	33.243700
778.514388	44233.328359	33.248717
779.464131	44279.930773	33.253735
780.043473	44337.274411	33.258752
780.576038	44383.878732	33.263770
781.208796	44448.994506	33.268788
781.912684	44504.048384	33.273805
782.966455	44554.658117	33.278823
783.386078	44613.418914	33.283840
783.828690	44663.542095	33.288858
784.553950	44736.392945	33.293876
785.207023	44802.967767	33.298893
785.815205	44866.190951	33.303911
786.487326	44938.032330	33.308928
787.657585	44998.227038	33.313946
788.114975	45078.477271	33.318964
789.207452	45144.029557	33.323981
790.420202	45203.402209	33.328999
791.400132	45262.722703	33.334016
793.173798	45313.715495	33.339034
794.152942	45367.337027	33.344052
794.975601	45415.448123	33.349069
795.617207	45456.528092	33.354087
796.244237	45526.765348	33.359104
797.198987	45569.542661	33.364122
797.750491	45634.598636	33.369140
798.357724	45687.355280	33.374157
799.003113	45747.077051	33.379175
799.751576	45806.264226	33.384192
800.368125	45869.590158	33.389210
800.854405	45932.904918	33.394228
801.429236	46001.551366	33.399245
802.138454	46076.148672	33.404263
803.192297	46147.447427	33.409280
803.817520	46216.200553	33.414298
804.537329	46303.543562	33.419316
805.167158	46372.966993	33.424333
806.129657	46456.572169	33.429351
806.928933	46531.808538	33.434368
807.636796	46605.724610	33.439386
808.533053	46683.185779	33.444404
809.367393	46753.135234	33.449421
810.297234	46835.133768	33.454439
811.230902	46914.639542	33.459456
812.086175	46982.669658	33.464474
813.397562	47055.411500	33.469492
814.069564	47117.821356	33.474509
815.309240	47188.057000	33.479527
815.949674	47256.950108	33.484544
816.695503	47327.554062	33.489562
817.491759	47387.028959	33.494580
817.978990	47461.412359	33.499597
819.364056	47516.955937	33.504615
820.068523	47591.748785	33.509632
821.394034	47650.522017	33.514650
822.043643	47719.997123	33.519668
822.510883	47777.721275	33.524685
823.272854	47834.982159	33.529703
823.755193	47902.870655	33.534720
824.728952	47986.473416	33.539738
825.485518	48049.840610	33.544756
826.181644	48116.893018	33.549773
827.165622	48185.665883	33.554791
827.944422	48268.123319	33.559808
829.108290	48328.308960	33.564826
830.324486	48388.606817	33.569844
831.423673	48449.391209	33.574861
832.511757	48503.199371	33.579879
833.208900	48564.837467	33.584896
833.944424	48605.959167	33.589914
834.785462	48657.161664	33.594932
835.355962	48709.355372	33.599949
835.971308	48760.732419	33.604967
836.609741	48823.468522	33.609984
837.383616	48872.923170	33.615002
838.040380	48945.374407	33.620020
838.562828	49007.825395	33.625037
839.600892	49069.879959	33.630055
840.054178	49144.868855	33.635072
840.792695	49203.674217	33.640090
841.497196	49283.717446	33.645108
842.216733	49358.596004	33.650125
843.352900	49433.574448	33.655143
844.150360	49506.328226	33.660160
844.816634	49576.983181	33.665178
845.701799	49661.105693	33.670196
846.014249	49743.444923	33.675213
847.273608	49816.817410	33.680231
848.103114	49907.946994	33.685248
848.876711	49982.097910	33.690266
850.018257	50069.585884	33.695284
850.504694	50149.172580	33.700301
851.633551	50226.850037	33.705319
852.226529	50319.207541	33.710336
853.535897	50402.564441	33.715354
854.398897	50473.564826	33.720372
855.255148	50560.219620	33.725389
856.743106	50635.090286	33.730407
857.452793	50713.043428	33.735424
858.200205	50794.559459	33.740442
859.056544	50870.769328	33.745460
859.678473	50950.786929	33.750477
861.028775	51033.962582	33.755495
861.364855	51107.742325	33.760512
862.348652	51182.832449	33.765530
863.240467	51261.126070	33.770548
863.906125	51345.605270	33.775565
865.046111	51429.099812	33.780583
865.722891	51499.505938	33.785600
866.329685	51584.077426	33.790618
867.532318	51672.416163	33.795636
868.223077	51751.812064	33.800653
869.594371	51839.074836	33.805671
870.612351	51916.737275	33.810688
871.412421	51995.243809	33.815706
871.969412	52060.943681	33.820724
872.862774	52149.117241	33.825741
874.044686	52224.875927	33.830759
874.765793	52304.174080	33.835776
875.829592	52384.298689	33.840794
876.745072	52457.903946	33.845812
877.633113	52534.867334	33.850829
878.583239	52608.334794	33.855847
879.644698	52690.605883	33.860864
880.330423	52774.150662	33.865882
881.261415	52849.842872	33.870900
881.805941	52927.221705	33.875917
882.450054	53006.401349	33.880935
883.719480	53091.482628	33.885952
884.358937	53163.241080	33.890970
885.569612	53246.035088	33.895988
886.483531	53324.578998	33.901005
886.938925	53403.751397	33.906023
888.178828	53483.093025	33.911040
888.807631	53560.302636	33.916058
889.925466	53636.442898	33.921076
890.552588	53722.607278	33.926093
891.681762	53785.109597	33.931111
892.579673	53857.937334	33.936128
892.975551	53933.779625	33.941146
893.966945	53991.007426	33.946164
895.050805	54073.317858	33.951181
896.011838	54146.623921	33.956199
896.614557	54226.668414	33.961216
897.361208	54288.554516	33.966234
898.523571	54368.506047	33.971252
899.094422	54459.048268	33.976269
899.908419	54527.986695	33.981287
900.928752	54614.593056	33.986304
901.820151	54702.251299	33.991322
903.090280	54778.460148	33.996340
903.843987	54862.792802	34.001357
904.847244	54941.075078	34.006375
905.544927	55016.785277	34.011392
906.331157	55104.809439	34.016410
907.497269	55179.953638	34.021428
908.698730	55263.869967	34.026445
909.929823	55328.480510	34.031463
911.326265	55404.716015	34.036480
911.992675	55468.718720	34.041498
913.257361	55537.052024	34.046516
914.584057	55586.181774	34.051533
915.683824	55658.395106	34.056551
916.755406	55716.551220	34.061568
917.670611	55778.655470	34.066586
918.796707	55829.601580	34.071604
919.442519	55896.196994	34.076621
920.316065	55958.320856	34.081639
921.094127	56028.446353	34.086656
921.941180	56097.181692	34.091674
922.992963	56154.202822	34.096692
923.537801	56226.054933	34.101709
924.681916	56286.992062	34.106727
925.590834	56351.010024	34.111744
926.341086	56435.994328	34.116762
927.358179	56490.711710	34.121780
928.072462	56569.044340	34.126797
928.906727	56627.340883	34.131815
929.844747	56700.202769	34.136832
930.400272	56782.509930	34.141850
931.275082	56859.388230	34.146868
932.363242	56939.119489	34.151885
933.025468	57012.499916	34.156903
934.268143	57089.486243	34.161920
934.881631	57180.462558	34.166938
935.924579	57249.284642	34.171956
936.935965	57334.851721	34.176973
937.473988	57417.840979	34.181991
938.215327	57501.419110	34.187008
938.748057	57600.156192	34.192026
939.895406	57671.134066	34.197044
941.078004	57776.011076	34.202061
942.160629	57864.777756	34.207079
942.983703	57944.294132	34.212096
943.635484	58032.628502	34.217114
944.929267	58118.799980	34.222132
945.741163	58209.527787	34.227149
946.955213	58290.237610	34.232167
948.036662	58378.848140	34.237184
948.713083	58466.053674	34.242202
949.812388	58553.339267	34.247220
950.491605	58639.260163	34.252237
951.572201	58726.182198	34.257255
952.491137	58812.098040	34.262272
953.252310	58899.089406	34.267290
954.396805	58964.356186	34.272308
955.192269	59052.804837	34.277325
956.184766	59130.393618	34.282343
957.149466	59208.170526	34.287360
958.138295	59287.532605	34.292378
959.055885	59360.310786	34.297396
959.816847	59454.652626	34.302413
960.577393	59533.937116	34.307431
961.782495	59615.981941	34.312448
962.610189	59694.167831	34.317466
963.938674	59787.669413	34.322484
964.449342	59865.386181	34.327501
965.467417	59960.227971	34.332519
966.834336	60042.204739	34.337536
967.787291	60132.411418	34.342554
969.042720	60218.292515	34.347572
969.869913	60301.841634	34.352589
970.705524	60387.465864	34.357607
971.582824	60473.925753	34.362624
972.614921	60561.425247	34.367642
973.759217	60641.071365	34.372660
975.364813	60725.722409	34.377677
976.334699	60817.384828	34.382695
977.265362	60896.849821	34.387712
978.154691	60977.359598	34.392730
979.282424	61051.103898	34.397748
980.243690	61138.135411	34.402765
980.905679	61229.954908	34.407783
982.295040	61305.083474	34.412800
983.129852	61383.824365	34.417818
983.922265	61458.862754	34.422836
984.531798	61539.183718	34.427853
985.771738	61629.199320	34.432871
987.558825	61723.162307	34.437888
987.821534	61812.697693	34.442906
989.011883	61894.094134	34.447924
990.022193	61978.956105	34.452941
990.494389	62065.016230	34.457959
991.833136	62158.158120	34.462976
992.983036	62241.442053	34.467994
994.392247	62321.305589	34.473012
995.483471	62401.661995	34.478029
996.205149	62487.222652	34.483047
998.055133	62555.706240	34.488064
998.851359	62636.995563	34.493082
999.862343	62711.592274	34.498100
1001.017718	62797.346035	34.503117
1001.694125	62875.521295	34.508135
1002.634670	62939.773261	34.513152
1003.112348	63038.572551	34.518170
1004.440468	63113.184409	34.523188
1005.588251	63193.123104	34.528205
1005.800154	63286.356017	34.533223
1007.020188	63367.050006	34.538240
1007.671497	63469.255078	34.543258
1008.605111	63560.749746	34.548276
1009.456602	63651.491542	34.553293
1010.323525	63751.340909	34.558311
1011.408664	63841.477278	34.563328
1012.523798	63937.813278	34.568346
1013.433723	64030.326250	34.573364
1014.621194	64134.134528	34.578381
1015.600367	64235.570010	34.583399
1016.445759	64337.286285	34.588416
1017.747307	64423.548341	34.593434
1018.880903	64510.539548	34.598452
1020.125104	64595.500662	34.603469
1021.243991	64685.723451	34.608487
1022.324251	64756.092872	34.613504
1023.055557	64854.410376	34.618522
1024.155901	64931.044672	34.623540
1024.838388	65002.818839	34.628557
1026.049346	65093.319981	34.633575
1026.645251	65175.826298	34.638592
1027.597128	65266.229110	34.643610
1028.774114	65350.361228	34.648628
1029.616321	65435.792938	34.653645
1030.298631	65529.448454	34.658663
1031.237261	65629.192839	34.663680
1032.586432	65725.708195	34.668698
1033.509302	65823.904698	34.673716
1034.770200	65908.329507	34.678733
1035.558277	66012.682544	34.683751
1036.663630	66111.250618	34.688768
1037.707205	66208.752395	34.693786
1038.647253	66315.621818	34.698804
1040.057970	66403.044933	34.703821
1040.758516	66517.898153	34.708839
1042.046291	66606.259134	34.713856
1043.310594	66710.635884	34.718874
1044.535550	66790.574019	34.723892
1046.380538	66892.341270	34.728909
1047.194750	66971.603144	34.733927
1048.428301	67052.883012	34.738944
1049.764548	67139.820078	34.743962
1050.630339	67231.142362	34.748980
1051.676666	67322.867408	34.753997
1052.304470	67419.108945	34.759015
1053.870352	67505.441683	34.764032
1054.851832	67588.066779	34.769050
1055.582146	67674.447841	34.774068
1056.705509	67768.182251	34.779085
1057.243250	67876.095903	34.784103
1058.555757	67957.341036	34.789120
1059.831767	68056.580221	34.794138
1060.866810	68141.750409	34.799156
1062.214094	68238.598510	34.804173
1063.063392	68339.811043	34.809191
1064.347493	68423.791033	34.814208
1065.327245	68520.729066	34.819226
1066.108746	68613.570021	34.824244
1067.477176	68709.466844	34.829261
1068.972051	68801.374304	34.834279
1069.996109	68885.833175	34.839296
1070.966259	68975.385183	34.844314
1071.798425	69063.660949	34.849332
1073.107195	69155.592310	34.854349
1073.426170	69262.684693	34.859367
1074.773504	69359.612989	34.864384
1075.986762	69467.656113	34.869402
1076.586968	69566.392113	34.874420
1077.842596	69650.760454	34.879437
1079.089226	69754.861075	34.884455
1080.013747	69853.231084	34.889472
1081.160036	69961.590632	34.894490
1082.273273	70058.690958	34.899508
1083.201029	70144.606319	34.904525
1084.099087	70261.123543	34.909543
1085.363902	70334.955976	34.914560
1086.947221	70431.243658	34.919578
1087.970956	70541.480034	34.924596
1089.149010	70634.127200	34.929613
1089.912830	70734.589870	34.934631
1091.351766	70821.802001	34.939648
1092.314568	70925.843842	34.944666
1093.444976	71011.090953	34.949684
1094.702888	71101.004442	34.954701
1095.563737	71187.585889	34.959719
1096.202368	71274.518832	34.964736
1097.206951	71353.517569	34.969754
1098.036245	71452.073080	34.974772
1099.336654	71538.308639	34.979789
1099.821289	71639.198188	34.984807
1100.864023	71742.964869	34.989824
1102.329953	71842.993215	34.994842
1103.253234	71950.097559	34.999860
1104.474098	72052.330585	35.004877
1105.312644	72149.646085	35.009895
1106.436069	72255.036042	35.014912
1107.450638	72359.316150	35.019930
1108.752911	72471.619732	35.024948
1109.734440	72577.944973	35.029965
1110.847951	72684.300761	35.034983
1112.209531	72791.973575	35.040000
1113.553176	72890.821710	35.045018
1114.486186	73005.236862	35.050036
1115.988616	73107.290827	35.055053
1117.014650	73219.273280	35.060071
1118.345086	73313.223409	35.065088
1119.437611	73416.507621	35.070106
1120.241123	73527.702732	35.075124
1122.244057	73631.086721	35.080141
1123.501261	73728.824169	35.085159
1124.553349	73819.310940	35.090176
1125.730877	73917.770781	35.095194
1126.509632	74015.330433	35.100212
1127.980083	74117.038606	35.105229
1128.935995	74219.764557	35.110247
1130.115021	74322.164851	35.115264
1131.427338	74419.858256	35.120282
1132.715085	74523.711691	35.125300
1133.891328	74616.246457	35.130317
1135.136966	74714.052648	35.135335
1136.235534	74822.648609	35.140352
1137.542180	74906.829528	35.145370
1138.637914	75002.633461	35.150388
1139.920372	75097.813340	35.155405
1140.979310	75196.283683	35.160423
1141.949212	75293.526908	35.165440
1142.860891	75390.690879	35.170458
1143.768382	75488.071189	35.175476
1145.160279	75582.463075	35.180493
1146.238447	75688.545008	35.185511
1147.404309	75802.011209	35.190528
1148.295751	75908.313075	35.195546
1148.835243	76009.843993	35.200564
1150.652688	76123.159455	35.205581
1151.746229	76223.933581	35.210599
1152.739056	76335.642888	35.215616
1154.110450	76438.059301	35.220634
1155.003347	76553.129216	35.225652
1155.908343	76655.188357	35.230669
1157.368329	76767.536101	35.235687
1158.565402	76881.939361	35.240704
1159.817225	76983.185702	35.245722
1160.908869	77086.142139	35.250740
1162.503667	77200.738183	35.255757
1163.503726	77298.959327	35.260775
1164.545738	77413.490298	35.265792
1165.790772	77512.054110	35.270810
1166.583324	77623.647870	35.275828
1168.145624	77716.893232	35.280845
1169.445016	77820.326818	35.285863
1170.575854	77941.344808	35.290880
1171.543235	78023.726041	35.295898
1172.315580	78121.162166	35.300916
1173.626557	78215.677148	35.305933
1175.022768	78320.807746	35.310951
1176.561587	78405.672811	35.315968
1177.883790	78481.235390	35.320986
1178.495581	78569.095602	35.326004
1180.086759	78661.554256	35.331021
1181.245610	78758.071037	35.336039
1182.642481	78856.831416	35.341056
1183.765933	78942.459555	35.346074
1184.842014	79043.702871	35.351092
1185.980074	79135.840926	35.356109
1187.420218	79230.706680	35.361127
1188.542364	79322.873174	35.366144
1189.854980	79412.185224	35.371162
1191.379815	79501.173151	35.376180
1192.120741	79603.978262	35.381197
1192.624927	79699.396709	35.386215
1194.304838	79793.986370	35.391232
1195.911029	79889.373298	35.396250
1196.892612	79999.959098	35.401268
1197.855907	80099.386844	35.406285
1199.267245	80200.430182	35.411303
1200.127637	80294.921071	35.416320
1201.524743	80390.050876	35.421338
1202.764374	80497.760618	35.426356
1203.657140	80601.952060	35.431373
1204.703243	80716.065362	35.436391
1205.563268	80828.548419	35.441408
1207.246085	80937.774537	35.446426
1208.087239	81055.759933	35.451444
1209.417429	81174.290508	35.456461
1210.569277	81289.479263	35.461479
1211.469098	81408.027137	35.466496
1212.661592	81533.574250	35.471514
1214.047227	81651.401386	35.476532
1215.246519	81768.979287	35.481549
1216.357562	81886.698114	35.486567
1217.564319	82006.581742	35.491584
1219.286458	82109.648781	35.496602
1220.656909	82234.284434	35.501620
1221.995605	82345.013964	35.506637
1223.522397	82451.685589	35.511655
1224.570294	82581.364963	35.516672
1226.073377	82683.872706	35.521690
1226.900180	82808.367450	35.526708
1227.877205	82915.924619	35.531725
1229.139091	83037.552532	35.536743
1230.557148	83150.148061	35.541760
1232.207130	83262.251804	35.546778
1233.152311	83380.205393	35.551796
1234.516115	83488.224016	35.556813
1236.500299	83584.628990	35.561831
1237.666584	83691.069973	35.566848
1238.972796	83800.758590	35.571866
1240.102763	83909.740164	35.576884
1241.174228	84017.856982	35.581901
1242.924426	84119.444493	35.586919
1243.917450	84231.312199	35.591936
1245.067454	84319.638827	35.596954
1246.221432	84428.428579	35.601972
1247.010367	84528.595978	35.606989
1248.126941	84647.681180	35.612007
1249.412449	84760.202329	35.617024
1250.515621	84870.838967	35.622042
1252.033056	84992.384750	35.627060
1253.383501	85092.973562	35.632077
1254.652340	85183.400439	35.637095
1255.699086	85285.621098	35.642112
1257.226670	85373.613431	35.647130
1258.146019	85472.065862	35.652148
1259.373676	85581.241321	35.657165
1260.248730	85683.971628	35.662183
1261.446468	85795.357383	35.667200
1262.815687	85892.093930	35.672218
1263.767590	86000.363529	35.677236
1264.871650	86118.861192	35.682253
1266.025157	86230.128788	35.687271
1267.476556	86347.597603	35.692288
1268.987896	86461.382749	35.697306
1269.871879	86575.177286	35.702324
1271.391895	86698.757333	35.707341
1272.819243	86814.495732	35.712359
1274.060572	86936.967022	35.717376
1275.614580	87050.722487	35.722394
1276.764430	87174.172086	35.727412
1277.933708	87288.039048	35.732429
1279.129861	87408.415773	35.737447
1280.226903	87527.363784	35.742464
1281.611606	87639.449813	35.747482
1282.874491	87774.010617	35.752500
1283.943435	87893.255950	35.757517
1285.592160	88013.108508	35.762535
1286.522643	88145.948612	35.767552
1288.139897	88277.149038	35.772570
1289.315712	88403.045570	35.777588
1290.301290	88541.923720	35.782605
1291.734576	88667.591216	35.787623
1292.776883	88804.928373	35.792640
1294.466287	88931.368183	35.797658
1295.900532	89061.637446	35.802676
1297.234792	89202.542780	35.807693
1298.905124	89325.033279	35.812711
1299.865960	89453.679767	35.817728
1301.070752	89581.160932	35.822746
1302.838529	89698.619250	35.827764
1303.993867	89841.126934	35.832781
1305.815707	89956.385387	35.837799
1307.118967	90083.688624	35.842816
1308.840726	90202.055897	35.847834
1310.320654	90317.787187	35.852852
1311.918261	90433.601996	35.857869
1313.585959	90537.518576	35.862887
1314.778008	90652.358128	35.867904
1315.833635	90762.454073	35.872922
1317.475556	90872.801355	35.877940
1318.611132	90993.468215	35.882957
1319.924915	91090.864143	35.887975
1321.240452	91202.847659	35.892992
1322.530601	91307.522732	35.898010
1323.933047	91421.762153	35.903028
1325.021295	91538.598375	35.908045
1326.524034	91643.393613	35.913063
1327.859397	91757.999621	35.918080
1329.098533	91868.375224	35.923098
1330.696638	91972.320270	35.928116
1331.807816	92088.141117	35.933133
1333.137747	92211.963817	35.938151
1334.175441	92319.824900	35.943168
1335.197843	92434.177996	35.948186
1336.416012	92551.720342	35.953204
1337.431472	92682.133880	35.958221
1338.900830	92802.236353	35.963239
1340.071358	92921.701387	35.968256
1341.493660	93043.840060	35.973274
1342.685245	93156.521841	35.978292
1343.824387	93269.934656	35.983309
1345.253209	93374.354458	35.988327
1346.614510	93493.310396	35.993344
1347.841398	93601.311335	35.998362
1349.400069	93710.832696	36.003380
1350.529100	93838.952019	36.008397
1351.800606	93950.318767	36.013415
1353.249825	94074.764203	36.018432
1354.502779	94199.595592	36.023450
1355.566543	94326.155398	36.028468
1356.684899	94452.453723	36.033485
1358.239717	94583.171653	36.038503
1358.800518	94713.956127	36.043520
1360.682264	94848.642352	36.048538
1362.214249	94984.625790	36.053556
1363.315772	95121.424676	36.058573
1364.794965	95251.105138	36.063591
1366.064641	95398.184237	36.068608
1367.781156	95543.179062	36.073626
1369.363803	95671.805779	36.078644
1370.053789	95814.223703	36.083661
1371.639375	95952.079036	36.088679
1372.739063	96094.383765	36.093696
1374.423760	96235.545989	36.098714
1375.836188	96377.955442	36.103732
1377.535663	96524.060283	36.108749
1378.862910	96658.206843	36.113767
1380.589072	96787.158065	36.118784
1382.357403	96923.937117	36.123802
1383.847742	97064.347402	36.128820
1384.925828	97200.918188	36.133837
1386.025292	97349.858332	36.138855
1387.685854	97490.015843	36.143872
1388.998325	97633.194444	36.148890
1390.520901	97762.625021	36.153908
1392.162562	97904.498639	36.158925
1393.344665	98041.525898	36.163943
1395.123690	98187.296472	36.168960
1396.252114	98322.786746	36.173978
1397.861855	98455.401116	36.178996
1399.423699	98586.958641	36.184013
1400.850962	98720.743432	36.189031
1402.174272	98858.791735	36.194048
1403.254132	99001.074610	36.199066
1405.037221	99141.055533	36.204084
1406.258399	99283.203573	36.209101
1407.539224	99417.166196	36.214119
1408.776864	99557.423993	36.219136
1410.851491	99691.441689	36.224154
1412.054568	99832.403315	36.229172
1413.640027	99966.916649	36.234189
1415.065309	100096.270411	36.239207
1416.728338	100237.605930	36.244224
1417.778865	100374.562234	36.249242
1419.839198	100483.534668	36.254260
1421.092976	100617.519170	36.259277
1422.604198	100746.063467	36.264295
1424.085823	100876.121529	36.269312
1425.282188	101017.761289	36.274330
1426.865214	101143.582940	36.279348
1428.184027	101273.338311	36.284365
1429.559526	101390.939922	36.289383
1431.169631	101530.717252	36.294400
1432.347914	101670.714529	36.299418
1434.116517	101807.489037	36.304436
1435.003016	101931.621853	36.309453
1435.897003	102060.165981	36.314471
1437.942634	102191.612175	36.319488
1439.203150	102311.073338	36.324506
1440.419127	102431.340601	36.329524
1441.698708	102556.200655	36.334541
1443.336810	102681.106807	36.339559
1444.811490	102804.707630	36.344576
1445.830257	102938.319837	36.349594
1447.432936	103061.356523	36.354612
1448.245043	103205.626616	36.359629
1449.533823	103345.791327	36.364647
1450.929312	103479.714767	36.369664
1452.178726	103628.013863	36.374682
1453.419237	103775.186591	36.379700
1454.947194	103931.507431	36.384717
1456.087722	104093.911813	36.389735
1457.713270	104235.993102	36.394752
1459.054111	104407.839060	36.399770
1460.656070	104561.831065	36.404788
1461.953931	104724.061872	36.409805
1463.203768	104881.140480	36.414823
1465.018723	105054.145849	36.419840
1465.793479	105215.129119	36.424858
1468.116587	105368.581485	36.429876
1469.556889	105549.699162	36.434893
1471.498191	105703.592866	36.439911
1473.022418	105870.257175	36.444928
1474.705782	106026.652345	36.449946
1476.427998	106173.430943	36.454964
1478.049668	106333.526939	36.459981
1479.300556	106501.213239	36.464999
1481.528797	106644.428151	36.470016
1482.843327	106792.997349	36.475034
1484.392383	106946.374465	36.480052
1486.111569	107092.929262	36.485069
1487.685318	107235.310199	36.490087
1489.816300	107374.650514	36.495104
1491.044781	107525.708929	36.500122
1492.448665	107670.172312	36.505140
1494.067057	107808.668511	36.510157
1495.593086	107941.511505	36.515175
1497.081451	108086.381942	36.520192
1498.681826	108238.159110	36.525210
1500.277659	108377.510703	36.530228
1501.852135	108529.445350	36.535245
1503.167783	108670.895994	36.540263
1504.751014	108806.662649	36.545280
1505.743864	108954.428966	36.550298
1507.637847	109100.305702	36.555316
1509.247482	109243.653089	36.560333
1510.439459	109394.738035	36.565351
1511.992100	109534.075634	36.570368
1513.356082	109688.000981	36.575386
1515.705905	109820.634190	36.580404
1517.029175	109962.545415	36.585421
1518.231636	110114.303941	36.590439
1520.431620	110238.250077	36.595456
1522.046384	110371.126592	36.600474
1523.659957	110506.844414	36.605492
1524.962609	110638.400933	36.610509
1526.415993	110771.405529	36.615527
1528.182055	110906.403678	36.620544
1529.797662	111042.034474	36.625562
1531.276664	111171.270176	36.630580
1532.549521	111307.373828	36.635597
1533.830982	111452.138244	36.640615
1536.222211	111561.488032	36.645632
1538.104400	111691.056009	36.650650
1539.877099	111797.915718	36.655668
1541.272762	111914.307761	36.660685
1541.913064	112014.369360	36.665703
1543.345675	112127.560518	36.670720
1544.728182	112242.738218	36.675738
1546.270035	112358.969457	36.680756
1547.244228	112488.909935	36.685773
1548.462123	112614.069854	36.690791
1550.204896	112741.329843	36.695808
1551.430086	112880.376490	36.700826
1552.577548	113023.215076	36.705844
1553.883773	113176.898232	36.710861
1555.489949	113309.850474	36.715879
1557.742543	113454.826950	36.720896
1558.766538	113608.099305	36.725914
1559.894490	113759.453755	36.730932
1561.498149	113912.624495	36.735949
1562.964126	114072.716643	36.740967
1564.294366	114226.349788	36.745984
1565.518279	114398.732488	36.751002
1567.101395	114569.817184	36.756020
1568.703556	114741.191423	36.761037
1569.938759	114916.479177	36.766055
1571.393580	115083.071135	36.771072
1572.975569	115260.386562	36.776090
1574.798370	115438.781475	36.781108
1576.720838	115613.965592	36.786125
1577.990154	115793.107891	36.791143
1580.130970	115971.684185	36.796160
1581.177163	116144.597389	36.801178
1582.586373	116320.701842	36.806196
1584.599967	116508.166203	36.811213
1586.402786	116683.653045	36.816231
1588.177598	116862.607684	36.821248
1590.198169	117038.823322	36.826266
1591.949148	117206.038292	36.831284
1593.965024	117379.224870	36.836301
1595.488117	117550.586378	36.841319
1597.130185	117718.492829	36.846336
1598.642423	117875.841865	36.851354
1600.447819	118054.632551	36.856372
1601.422304	118222.924204	36.861389
1602.959558	118401.859742	36.866407
1604.723108	118575.205255	36.871424
1606.406457	118747.346362	36.876442
1608.143064	118924.642450	36.881460
1609.949405	119100.863031	36.886477
1611.498286	119276.515649	36.891495
1612.944208	119451.639671	36.896512
1614.837489	119631.667186	36.901530
1616.264265	119811.945740	36.906548
1618.107203	119967.717146	36.911565
1620.116158	120139.788490	36.916583
1621.543887	120315.655003	36.921600
1623.406988	120489.830907	36.926618
1624.680346	120654.636507	36.931636
1626.127529	120827.445284	36.936653
1627.691547	121000.680621	36.941671
1629.252355	121181.655077	36.946688
1630.854659	121358.983309	36.951706
1632.216734	121540.447029	36.956724
1633.754819	121717.799574	36.961741
1635.301827	121909.663439	36.966759
1636.989596	122089.899295	36.971776
1638.499098	122277.077242	36.976794
1639.758608	122470.219077	36.981812
1641.529117	122654.478610	36.986829
1643.323260	122844.101306	36.991847
1644.856975	123028.221844	36.996864
1646.229211	123215.006986	37.001882
1647.988843	123372.428734	37.006900
1649.546996	123549.570757	37.011917
1650.824344	123723.141817	37.016935
1652.470686	123902.872280	37.021952
1654.082902	124091.818849	37.026970
1656.051617	124271.843320	37.031988
1657.755377	124445.046689	37.037005
1659.028985	124631.815765	37.042023
1660.652375	124805.857798	37.047040
1662.215934	125006.893475	37.052058
1663.825409	125197.609061	37.057076
1665.421228	125385.054599	37.062093
1667.050441	125599.302172	37.067111
1669.057227	125785.810239	37.072128
1670.608236	125979.316942	37.077146
1671.944028	126179.442397	37.082164
1674.033991	126376.482780	37.087181
1675.233294	126583.596429	37.092199
1677.620289	126783.408992	37.097216
1678.832727	126970.337899	37.102234
1680.838914	127183.735843	37.107252
1682.425276	127387.367838	37.112269
1683.845780	127590.722164	37.117287
1685.566497	127798.648862	37.122304
1687.792047	128012.435616	37.127322
1689.228521	128214.547174	37.132340
1691.275718	128419.025991	37.137357
1692.832466	128632.044597	37.142375
1695.344599	128824.374693	37.147392
1696.960680	129027.895907	37.152410
1698.799366	129229.112396	37.157428
1700.334293	129417.765672	37.162445
1701.724732	129634.088638	37.167463
1703.450968	129846.401885	37.172480
1705.131919	130044.525634	37.177498
1706.501527	130261.184926	37.182516
1708.306530	130467.424238	37.187533
1709.808160	130694.367752	37.192551
1711.438760	130905.762259	37.197568
1713.099749	131123.687443	37.202586
1714.408631	131351.514537	37.207604
1716.295217	131571.563864	37.212621
1718.315684	131802.061309	37.217639
1719.871878	132026.998614	37.222656
1721.916900	132248.143300	37.227674
1723.312347	132487.560114	37.232692
1724.777212	132701.158931	37.237709
1726.518441	132929.637584	37.242727
1728.592439	133153.789554	37.247744
1730.415891	133377.042696	37.252762
1732.337331	133607.933071	37.257780
1734.116398	133826.005676	37.262797
1736.124007	134044.652856	37.267815
1737.853693	134267.531739	37.272832
1739.950581	134484.111573	37.277850
1741.432618	134713.236182	37.282868
1743.404362	134920.092367	37.287885
1745.248934	135150.139859	37.292903
1746.750299	135360.966888	37.297920
1748.635917	135578.003648	37.302938
1749.934318	135799.269599	37.307956
1751.631967	136014.446988	37.312973
1754.160634	136235.231738	37.317991
1755.984331	136449.871304	37.323008
1757.888521	136657.126658	37.328026
1759.453807	136873.610372	37.333044
1761.462063	137073.821311	37.338061
1763.152691	137273.486138	37.343079
1764.723968	137458.665862	37.348096
1766.251545	137652.330014	37.353114
1767.571690	137859.262931	37.358132
1769.589237	138063.930922	37.363149
1771.052538	138261.985700	37.368167
1773.088938	138470.002738	37.373184
1774.394857	138671.840045	37.378202
1775.638117	138894.182778	37.383220
1777.842403	139097.849099	37.388237
1779.214002	139314.209393	37.393255
1780.670453	139539.923030	37.398272
1782.562565	139758.463254	37.403290
1783.995305	139996.276826	37.408308
1786.038454	140212.650932	37.413325
1787.110881	140449.799487	37.418343
1788.810882	140694.174117	37.423360
1790.990857	140934.261940	37.428378
1792.497061	141183.187164	37.433396
1794.467019	141417.129624	37.438413
1796.143158	141670.104714	37.443431
1797.894047	141925.049303	37.448448
1799.670849	142169.191027	37.453466
1801.552488	142427.189160	37.458484
1803.512037	142672.650235	37.463501
1805.977528	142915.470145	37.468519
1807.771703	143163.421537	37.473536
1809.762144	143405.911682	37.478554
1812.020061	143654.136037	37.483572
1813.636641	143895.379541	37.488589
1815.262729	144134.465154	37.493607
1816.635626	144398.416329	37.498624
1818.719432	144652.422115	37.503642
1820.337954	144906.730057	37.508660
1822.012082	145156.436157	37.513677
1823.938651	145417.374682	37.518695
1825.425108	145671.389731	37.523712
1828.162567	145936.570789	37.528730
1829.753017	146194.113364	37.533748
1831.454099	146457.833830	37.538765
1833.409119	146717.302285	37.543783
1834.875494	146982.724667	37.548800
1837.061821	147246.145189	37.553818
1838.692171	147517.256389	37.558836
1840.515667	147774.097883	37.563853
1842.900123	148039.281242	37.568871
1844.244566	148310.504525	37.573888
1845.966273	148569.929691	37.578906
1848.055262	148840.125947	37.583924
1849.618246	149114.974889	37.588941
1851.919547	149366.304546	37.593959
1853.758505	149646.431629	37.598976
1855.598192	149910.896809	37.603994
1857.638540	150184.077635	37.609012
1859.468293	150448.204291	37.614029
1861.586902	150704.353993	37.619047
1863.604184	150976.323865	37.624064
1865.477157	151241.742380	37.629082
1867.508243	151509.066984	37.634100
1869.180808	151764.059824	37.639117
1871.053798	152028.695152	37.644135
1873.023845	152288.734245	37.649152
1875.224079	152539.485035	37.654170
1877.155066	152799.177178	37.659188
1879.024777	153049.385102	37.664205
1880.979525	153305.229677	37.669223
1882.592969	153573.822457	37.674240
1884.359938	153832.795974	37.679258
1885.804574	154075.623254	37.684276
1887.383619	154315.980695	37.689293
1889.470587	154560.512638	37.694311
1890.889329	154812.042575	37.699328
1892.661885	155055.686196	37.704346
1894.063200	155316.221277	37.709364
1895.837361	155574.846128	37.714381
1897.494421	155847.987389	37.719399
1898.630948	156123.191284	37.724416
1900.531416	156404.701018	37.729434
1902.052936	156690.434912	37.734452
1903.968258	156988.930519	37.739469
1906.010970	157280.044859	37.744487
1907.669957	157576.285570	37.749504
1909.695980	157874.958821	37.754522
1911.845870	158175.899368	37.759540
1913.492242	158470.711936	37.764557
1915.635953	158772.875142	37.769575
1917.548538	159080.153866	37.774592
1919.435295	159387.323901	37.779610
1921.516190	159691.354927	37.784628
1923.655433	160000.050244	37.789645
1925.913982	160298.140599	37.794663
1927.683211	160615.605586	37.799680
1929.662696	160906.772496	37.804698
1931.651812	161224.054001	37.809716
1933.602336	161533.078264	37.814733
1936.174544	161825.388643	37.819751
1938.373910	162138.528610	37.824768
1940.634341	162430.192019	37.829786
1942.863272	162729.212552	37.834804
1944.794295	163029.118765	37.839821
1946.698971	163321.311318	37.844839
1948.412786	163627.386246	37.849856
1950.533173	163920.017657	37.854874
1952.520799	164219.146063	37.859892
1954.295289	164525.317294	37.864909
1955.863069	164831.712550	37.869927
1957.836675	165150.793151	37.874944
1959.794844	165458.476326	37.879962
1961.760052	165779.326010	37.884980
1963.161399	166093.992899	37.889997
1965.346327	166402.546515	37.895015
1967.461232	166722.082288	37.900032
1969.546324	167038.678555	37.905050
1971.625228	167354.743970	37.910068
1973.361880	167684.284584	37.915085
1975.298693	167993.556828	37.920103
1977.495146	168318.648448	37.925120
1979.273441	168647.069757	37.930138
1981.120631	168967.292281	37.935156
1983.130206	169290.131955	37.940173
1985.355002	169618.323162	37.945191
1986.928094	169957.397194	37.950208
1988.320305	170278.216919	37.955226
1990.914314	170616.551045	37.960244
1992.954891	170947.138584	37.965261
1995.241180	171269.194784	37.970279
1997.121180	171607.047769	37.975296
1999.018174	171922.615470	37.980314
2001.240087	172259.554736	37.985332
2002.974313	172598.412552	37.990349
2005.258872	172932.818211	37.995367
2006.453758	173275.838913	38.000384
2008.678056	173600.416085	38.005402
2011.123835	173929.988489	38.010420
2012.916027	174259.790974	38.015437
2015.302946	174578.048717	38.020455
2017.708546	174895.720720	38.025472
2019.547658	175197.901629	38.030490
2021.489267	175493.820254	38.035508
2023.382084	175799.245770	38.040525
2024.926855	176104.929771	38.045543
2027.437963	176416.585073	38.050560
2029.043448	176737.410986	38.055578
2031.018301	177044.364854	38.060596
2032.991573	177366.621657	38.065613
2035.094885	177686.726119	38.070631
2036.868816	178015.518026	38.075648
2038.760754	178343.759496	38.080666
2040.611236	178669.418162	38.085684
2042.470295	179014.683413	38.090701
2044.262949	179344.620355	38.095719
2046.602505	179699.235954	38.100736
2048.142083	180046.815364	38.105754
2049.947607	180397.351665	38.110772
2051.628367	180752.073986	38.115789
2053.721672	181109.476464	38.120807
2055.544328	181494.123693	38.125824
2057.701524	181861.652957	38.130842
2059.987662	182219.766285	38.135860
2062.037977	182600.699940	38.140877
2064.269513	182967.028260	38.145895
2066.061290	183345.389114	38.150912
2067.834711	183731.119904	38.155930
2069.971610	184121.392822	38.160948
2072.253727	184507.301507	38.165965
2074.472610	184895.736032	38.170983
2076.446800	185287.969202	38.176000
2078.942798	185668.845504	38.181018
2081.149672	186048.625270	38.186036
2083.579557	186430.505274	38.191053
2085.955048	186803.708573	38.196071
2088.051138	187249.243532	38.201088
2090.457512	187635.551104	38.206106
2092.545676	188020.131622	38.211124
2094.673136	188402.218222	38.216141
2096.679011	188787.271465	38.221159
2098.860077	189162.062626	38.226176
2100.820519	189542.578985	38.231194
2102.903390	189938.851031	38.236212
2104.839942	190320.567532	38.241229
2106.534669	190710.197017	38.246247
2109.254185	191080.897473	38.251264
2111.984397	191467.879103	38.256282
2114.169233	191853.219639	38.261300
2116.310001	192241.184531	38.266317
2118.061666	192623.038858	38.271335
2120.132232	193003.269896	38.276352
2121.935281	193395.228109	38.281370
2123.731953	193784.851654	38.286388
2125.616303	194169.001537	38.291405
2128.227091	194571.455273	38.296423
2130.223514	194968.392216	38.301440
2131.790243	195369.461417	38.306458
2134.215925	195780.558654	38.311476
2136.274860	196178.810324	38.316493
2138.306290	196595.813685	38.321511
2140.172471	197003.648665	38.326528
2141.939305	197411.830502	38.331546
2144.103866	197823.330023	38.336564
2146.192544	198239.262417	38.341581
2148.523350	198657.241248	38.346599
2150.945595	199071.777761	38.351616
2152.722215	199487.838388	38.356634
2154.917024	199898.754651	38.361652
2156.725070	200304.346942	38.366669
2158.910274	200707.341354	38.371687
2160.796789	201101.746506	38.376704
2162.924448	201508.409763	38.381722
2164.964254	201903.224799	38.386740
2167.029615	202323.058111	38.391757
2169.164456	202731.933176	38.396775
2171.313626	203141.594437	38.401792
2173.438501	203558.830373	38.406810
2176.032785	203972.336232	38.411828
2178.079111	204393.320461	38.416845
2180.113901	204812.783255	38.421863
2182.568870	205236.652453	38.426880
2184.912036	205661.987921	38.431898
2187.186414	206088.351104	38.436916
2189.203923	206505.838716	38.441933
2191.429476	206939.171640	38.446951
2193.636578	207367.097462	38.451968
2195.398801	207790.774824	38.456986
2198.097375	208214.231050	38.462004
2200.574021	208649.712889	38.467021
2203.329412	209070.799327	38.472039
2205.540599	209495.603855	38.477056
2207.834196	209918.643454	38.482074
2209.978444	210346.432018	38.487092
2212.079347	210768.867908	38.492109
2214.194420	211216.629473	38.497127
2216.566872	211652.970947	38.502144
2218.737165	212073.416547	38.507162
2221.440859	212508.945647	38.512180
2223.895609	212932.218779	38.517197
2226.512852	213363.520136	38.522215
2228.652411	213787.300714	38.527232
2230.281596	214225.666750	38.532250
2232.745026	214647.822957	38.537268
2234.909591	215094.388348	38.542285
2236.900512	215539.330044	38.547303
2239.064968	215974.972850	38.552320
2241.044341	216426.674731	38.557338
2243.160694	216865.653843	38.562356
2245.390620	217321.864933	38.567373
2247.312307	217780.105932	38.572391
2249.668613	218241.836258	38.577408
2251.247135	218706.685691	38.582426
2253.743794	219160.265683	38.587444
2255.758039	219637.699212	38.592461
2257.809883	220111.773910	38.597479
2260.038434	220591.003843	38.602496
2262.000854	221072.333217	38.607514
2264.333827	221557.771458	38.612532
2266.678384	222047.780874	38.617549
2269.175649	222529.561237	38.622567
2271.827641	223007.303868	38.627584
2273.882294	223499.061057	38.632602
2276.539146	223968.953365	38.637620
2278.865631	224454.342878	38.642637
2280.888752	224928.449458	38.647655
2283.533531	225413.179873	38.652672
2285.669464	225900.098044	38.657690
2287.423136	226391.191168	38.662708
2290.030850	226875.851134	38.667725
2292.334250	227369.703874	38.672743
2295.049049	227853.153038	38.677760
2296.954926	228345.848042	38.682778
2299.138584	228834.104765	38.687796
2301.410598	229323.922616	38.692813
2304.244085	229809.918490	38.697831
2306.683108	230276.871688	38.702848
2308.746966	230751.478840	38.707866
2311.389567	231208.949566	38.712884
2313.117731	231676.317461	38.717901
2315.032141	232135.475981	38.722919
2317.380655	232606.811327	38.727936
2319.363383	233069.159432	38.732954
2322.583655	233519.323918	38.737972
2325.512069	233984.851993	38.742989
2327.654525	234445.471986	38.748007
2329.988891	234903.470476	38.753024
2332.422617	235382.589015	38.758042
2334.626660	235841.343522	38.763060
2336.778547	236306.685206	38.768077
2339.067011	236772.360734	38.773095
2341.556342	237230.078470	38.778112
2344.150622	237701.649691	38.783130
2346.528386	238171.501112	38.788148
2348.838294	238651.650884	38.793165
2351.137581	239131.903201	38.798183
2353.441870	239607.403534	38.803200
2355.539584	240101.505191	38.808218
2357.742011	240576.181485	38.813236
2359.799017	241075.647895	38.818253
2362.044804	241568.860181	38.823271
2364.771550	242053.029325	38.828288
2367.201505	242569.200994	38.833306
2369.265611	243066.376126	38.838324
2371.380983	243574.872033	38.843341
2373.845659	244084.531806	38.848359
2376.182884	244595.150167	38.853376
2378.231696	245115.338321	38.858394
2380.203703	245635.994406	38.863412
2382.921656	246156.914134	38.868429
2385.085958	246695.980032	38.873447
2387.864412	247228.471188	38.878464
2389.915601	247767.119862	38.883482
2392.171440	248292.068569	38.888500
2394.780762	248831.109923	38.893517
2397.248056	249368.215763	38.898535
2399.165977	249907.463025	38.903552
2401.666477	250460.512927	38.908570
2404.411902	250998.992851	38.913588
2406.888268	251543.761767	38.918605
2409.458578	252105.863736	38.923623
2412.068912	252642.962008	38.928640
2413.838416	253198.046693	38.933658
2416.511613	253751.947211	38.938676
2419.243176	254308.656128	38.943693
2421.626182	254863.537420	38.948711
2423.904469	255410.202773	38.953728
2425.973886	255966.931978	38.958746
2428.694610	256531.330301	38.963764
2431.254474	257088.562762	38.968781
2433.904307	257648.598356	38.973799
2437.140475	258182.275781	38.978816
2439.656143	258740.701798	38.983834
2442.135919	259290.469278	38.988852
2444.444445	259837.365275	38.993869
2446.778304	260383.873837	38.998887
2449.571630	260927.514340	39.003904
2451.446408	261484.096932	39.008922
2454.425187	262028.414599	39.013940
2456.376785	262579.518872	39.018957
2458.667677	263132.624995	39.023975
2461.210982	263681.421903	39.028992
2463.986962	264247.222893	39.034010
2466.841399	264769.626504	39.039028
2469.896258	265299.971695	39.044045
2472.033154	265824.589824	39.049063
2474.792959	266335.621448	39.054080
2477.329537	266836.855856	39.059098
2479.277360	267343.208318	39.064116
2482.269699	267852.672049	39.069133
2484.433891	268367.163895	39.074151
2487.094229	268863.619141	39.079168
2489.188251	269381.748406	39.084186
2491.207303	269912.179144	39.089204
2493.683694	270424.274566	39.094221
2496.178324	270947.590108	39.099239
2498.499392	271460.440412	39.104256
2500.716595	272005.279379	39.109274
2502.934882	272548.006845	39.114292
2505.690145	273089.860066	39.119309
2507.710875	273634.643267	39.124327
2510.365818	274182.422713	39.129344
2512.851856	274739.850234	39.134362
2515.091970	275297.261512	39.139380
2517.789794	275856.502524	39.144397
2520.004047	276433.719249	39.149415
2522.589812	276997.236395	39.154432
2524.972610	277586.532480	39.159450
2527.291924	278154.755698	39.164468
2530.000787	278739.065641	39.169485
2532.212438	279329.594180	39.174503
2534.607145	279916.128043	39.179520
2537.213358	280521.467390	39.184538
2539.700470	281122.554070	39.189556
2542.164990	281720.388892	39.194573
2544.518478	282345.458674	39.199591
2547.038794	282950.512035	39.204608
2549.807033	283551.814205	39.209626
2552.635429	284170.623443	39.214644
2555.423672	284785.802216	39.219661
2557.713816	285408.848715	39.224679
2560.547203	286020.530586	39.229696
2563.740418	286630.805136	39.234714
2566.439045	287242.776220	39.239732
2569.020760	287844.349080	39.244749
2571.535948	288462.964777	39.249767
2574.155143	289072.899856	39.254784
2576.859638	289692.515427	39.259802
2579.739502	290304.556518	39.264820
2582.350648	290907.441988	39.269837
2585.069665	291520.791236	39.274855
2587.807569	292131.973304	39.279872
2590.228315	292739.009278	39.284890
2592.938782	293357.571939	39.289908
2595.688759	293962.183188	39.294925
2597.899650	294578.449804	39.299943
2600.673663	295194.063831	39.304960
2603.322924	295807.126553	39.309978
2606.203312	296431.114747	39.314996
2608.543411	297043.120821	39.320013
2610.828114	297663.735538	39.325031
2613.853125	298273.413069	39.330048
2616.680699	298885.526540	39.335066
2619.345685	299507.483467	39.340084
2621.784449	300116.622815	39.345101
2624.404472	300734.206351	39.350119
2626.895836	301343.146150	39.355136
2629.492921	301965.161861	39.360154
2631.768716	302592.018269	39.365172
2634.738079	303218.378570	39.370189
2636.858262	303831.612504	39.375207
2639.462778	304454.663990	39.380224
2642.284475	305071.556510	39.385242
2645.088144	305669.126995	39.390260
2647.630291	306257.694483	39.395277
2650.014813	306855.646259	39.400295
2652.352828	307450.476013	39.405312
2654.760628	308051.405156	39.410330
2657.173127	308669.002779	39.415348
2659.957183	309272.472949	39.420365
2662.438436	309886.186416	39.425383
2664.816810	310513.309734	39.430400
2667.118607	311133.304606	39.435418
2669.738219	311779.942957	39.440436
2672.757735	312409.555885	39.445453
2675.218850	313053.511116	39.450471
2677.805465	313689.240171	39.455488
2680.600285	314328.176729	39.460506
2683.285860	314977.653883	39.465524
2686.248650	315616.292578	39.470541
2688.907307	316277.302867	39.475559
2691.396563	316933.051136	39.480576
2693.924897	317588.732961	39.485594
2696.022784	318251.501682	39.490612
2698.993595	318930.010715	39.495629
2701.334732	319615.281313	39.500647
2704.043758	320297.387943	39.505664
2706.822594	320982.137404	39.510682
2709.363724	321665.568007	39.515700
2712.171008	322363.816048	39.520717
2715.081336	323059.803531	39.525735
2717.980289	323769.102734	39.530752
2721.075329	324457.400520	39.535770
2724.126804	325160.105735	39.540788
2726.593922	325859.413749	39.545805
2729.216328	326556.884143	39.550823
2731.547520	327264.612800	39.555840
2734.948630	327967.265758	39.560858
2737.653442	328688.332720	39.565876
2740.174457	329386.023315	39.570893
2743.465400	330101.239463	39.575911
2746.097904	330807.640167	39.580928
2748.943747	331514.070922	39.585946
2751.913897	332231.251176	39.590964
2754.693421	332943.906710	39.595981
2757.454304	333658.378284	39.600999
2759.986050	334365.540800	39.606016
2762.927313	335073.235072	39.611034
2765.834946	335798.855271	39.616052
2769.056952	336516.751795	39.621069
2771.919138	337226.801626	39.626087
2774.747263	337933.088941	39.631104
2777.646244	338635.648274	39.636122
2780.343842	339351.668214	39.641140
2783.283018	340053.813141	39.646157
2786.254645	340772.678788	39.651175
2789.530849	341463.583674	39.656192
2793.227766	342133.663379	39.661210
2796.298629	342817.446832	39.666228
2799.743242	343488.478155	39.671245
2802.589519	344168.896897	39.676263
2805.140299	344854.927375	39.681280
2808.264572	345519.907857	39.686298
2810.678345	346203.421931	39.691316
2813.474136	346864.597939	39.696333
2816.174149	347530.923534	39.701351
2819.011677	348203.350975	39.706368
2822.057201	348870.179262	39.711386
2824.675341	349542.639041	39.716404
2827.453030	350208.366261	39.721421
2830.429798	350866.391596	39.726439
2833.111313	351506.041853	39.731456
2835.386396	352138.846297	39.736474
2837.685186	352792.830549	39.741492
2840.168450	353433.614301	39.746509
2842.975406	354084.678805	39.751527
2845.341158	354748.956506	39.756544
2847.843041	355409.979349	39.761562
2850.307926	356086.078077	39.766580
2852.714950	356769.522897	39.771597
2854.924164	357460.842029	39.776615
2857.292684	358167.634883	39.781632
2860.436976	358885.520385	39.786650
2862.701974	359599.089875	39.791668
2864.734215	360328.800065	39.796685
2867.826337	361065.399586	39.801703
2870.586634	361807.203398	39.806720
2873.342450	362558.925117	39.811738
2876.176932	363319.131610	39.816756
2879.085128	364071.703690	39.821773
2882.006498	364849.218291	39.826791
2884.939706	365615.305882	39.831808
2887.968972	366389.822781	39.836826
2890.948110	367168.381444	39.841844
2894.326531	367952.026508	39.846861
2897.865818	368716.923709	39.851879
2900.474507	369503.433376	39.856896
2903.284337	370282.592184	39.861914
2905.692719	371081.099794	39.866932
2908.771579	371863.897561	39.871949
2911.827160	372653.441907	39.876967
2915.070899	373459.048324	39.881984
2918.683712	374237.413993	39.887002
2922.217517	375024.662343	39.892020
2924.821674	375796.680112	39.897037
2927.793631	376600.412033	39.902055
2930.535790	377398.633218	39.907072
2933.893755	378173.505464	39.912090
2936.785170	378985.005924	39.917108
2939.691703	379765.500173	39.922125
2942.376008	380564.369865	39.927143
2945.552434	381370.332032	39.932160
2948.714475	382162.645059	39.937178
2951.757733	382964.348802	39.942196
2954.800257	383751.135801	39.947213
2958.303900	384542.866766	39.952231
2960.955531	385332.147975	39.957248
2964.687193	386135.975267	39.962266
2967.670657	386927.611642	39.967284
2970.482407	387711.197286	39.972301
2973.171480	388503.234977	39.977319
2975.771794	389303.591906	39.982336
2978.784790	390092.110270	39.987354
2981.697069	390900.722639	39.992372
2985.215079	391696.909364	39.997389
2988.077184	392487.146623	40.002407
2991.202255	393283.747762	40.007424
2994.761333	394069.369280	40.012442
2997.647523	394862.107501	40.017460
3000.755790	395669.214111	40.022477
3004.109475	396464.003525	40.027495
3006.653534	397251.045422	40.032512
3009.785338	398021.820744	40.037530
3012.694087	398819.435127	40.042548
3015.668240	399607.900547	40.047565
3019.082114	400390.550991	40.052583
3021.935991	401187.941028	40.057600
3025.091021	401964.909460	40.062618
3028.248257	402745.394224	40.067636
3031.316927	403497.321231	40.072653
3034.452568	404240.457489	40.077671
3037.032232	404989.324060	40.082688
3039.688823	405741.595099	40.087706
3042.544303	406499.983842	40.092724
3045.142909	407245.078252	40.097741
3048.097094	408005.981323	40.102759
3050.978992	408770.866964	40.107776
3054.051831	409542.172989	40.112794
3057.068441	410325.300265	40.117812
3059.542931	411103.677479	40.122829
3062.668105	411896.546947	40.127847
3065.333879	412692.039120	40.132864
3068.480940	413497.797878	40.137882
3071.369669	414310.497122	40.142900
3073.918728	415123.420791	40.147917
3077.280972	415942.965121	40.152935
3080.132108	416775.556741	40.157952
3083.025861	417595.970031	40.162970
3085.917896	418437.290579	40.167988
3088.420469	419294.113969	40.173005
3091.973409	420145.428630	40.178023
3094.928766	421008.078739	40.183040
3097.945602	421867.750368	40.188058
3100.860489	422738.577235	40.193076
3103.968582	423627.034635	40.198093
3107.242522	424503.596040	40.203111
3110.673624	425382.168171	40.208128
3113.750459	426268.340976	40.213146
3116.871850	427153.254554	40.218164
3119.846500	428050.284741	40.223181
3123.023244	428935.919762	40.228199
3126.785319	429830.826330	40.233216
3130.153733	430719.991391	40.238234
3133.424516	431615.146289	40.243252
3136.463864	432509.336064	40.248269
3139.741541	433402.234869	40.253287
3142.866179	434311.136798	40.258304
3145.770539	435210.630853	40.263322
3149.021981	436117.255074	40.268340
3152.493875	437029.714176	40.273357
3155.742739	437925.237624	40.278375
3158.885504	438836.701421	40.283392
3162.352502	439732.408806	40.288410
3165.618156	440641.644460	40.293428
3168.972668	441555.773017	40.298445
3172.160108	442453.970475	40.303463
3175.216046	443365.884618	40.308480
3178.424475	444276.214848	40.313498
3181.833884	445174.902538	40.318516
3184.987980	446093.333709	40.323533
3188.266934	446991.599120	40.328551
3191.695501	447891.463488	40.333568
3195.365937	448783.115389	40.338586
3198.872244	449678.132035	40.343604
3202.332359	450579.624964	40.348621
3205.858375	451449.404681	40.353639
3209.237763	452335.321041	40.358656
3212.560780	453215.901034	40.363674
3216.128415	454099.327190	40.368692
3219.089394	454978.462165	40.373709
3222.310321	455831.516477	40.378727
3225.578624	456711.627248	40.383744
3228.835749	457589.878290	40.388762
3232.025971	458456.890869	40.393780
3235.404965	459346.339320	40.398797
3238.781420	460190.575730	40.403815
3241.678218	461060.631807	40.408832
3244.594941	461894.409972	40.413850
3248.002015	462727.314160	40.418868
3250.439080	463565.222602	40.423885
3253.640634	464397.319844	40.428903
3256.657998	465255.386637	40.433920
3259.352397	466107.456546	40.438938
3262.256130	466968.681966	40.443956
3265.011532	467832.811641	40.448973
3268.378322	468696.649894	40.453991
3271.630760	469575.440720	40.459008
3274.659572	470455.581224	40.464026
3277.607501	471355.002551	40.469044
3280.679454	472249.060080	40.474061
3283.863491	473159.036257	40.479079
3287.266289	474066.355796	40.484096
3290.053848	474987.837938	40.489114
3293.240925	475915.557844	40.494132
3296.534178	476857.122070	40.499149
3299.996008	477786.001678	40.504167
3303.228154	478723.079486	40.509184
3306.114086	479680.519760	40.514202
3309.556763	480635.043254	40.519220
3312.968173	481606.145608	40.524237
3316.097408	482569.521070	40.529255
3319.071924	483543.292618	40.534272
3321.828927	484528.677203	40.539290
3325.246055	485527.097790	40.544308
3328.424890	486521.309035	40.549325
3331.925472	487518.327983	40.554343
3335.401762	488539.718660	40.559360
3338.622197	489556.345627	40.564378
3342.385619	490560.378603	40.569396
3345.759093	491584.300560	40.574413
3348.991508	492596.490569	40.579431
3352.575348	493613.090049	40.584448
3355.966202	494653.972677	40.589466
3359.346432	495677.966271	40.594484
3362.475435	496713.961819	40.599501
3365.788393	497756.199695	40.604519
3369.492579	498791.154237	40.609536
3372.786042	499836.117040	40.614554
3376.501387	500869.060261	40.619572
3380.191855	501917.989780	40.624589
3383.538649	502949.785261	40.629607
3386.853308	503991.174244	40.634624
3390.304743	505029.698830	40.639642
3393.725682	506074.543088	40.644660
3397.350616	507123.907869	40.649677
3401.272429	508154.735553	40.654695
3405.151356	509192.336419	40.659712
3408.692990	510215.627495	40.664730
3412.672354	511236.260935	40.669748
3415.941356	512265.681772	40.674765
3419.292634	513289.029097	40.679783
3422.740975	514308.061725	40.684800
3426.414517	515332.766884	40.689818
3430.045075	516346.139767	40.694836
3433.845394	517360.366687	40.699853
3437.194973	518373.884725	40.704871
3441.315445	519385.950714	40.709888
3444.575212	520387.067102	40.714906
3448.499774	521372.726447	40.719924
3451.327862	522371.601680	40.724941
3454.942793	523392.894592	40.729959
3458.646307	524379.021084	40.734976
3461.649544	525386.488224	40.739994
3465.508209	526381.989098	40.745012
3468.848227	527369.750442	40.750016
3472.479695	528300.398330	40.755021
3475.720120	529186.975784	40.760026
3478.823395	530025.121299	40.765031
3482.356712	530815.662127	40.770036
3484.455485	531536.540839	40.775040
3487.397463	532208.057569	40.780045
3490.275331	532844.709809	40.785050
3492.299524	533417.375505	40.790055
3495.322105	533933.175223	40.795060
3497.043997	534392.372800	40.800064
3498.818232	534813.238085	40.805069
3500.676873	535183.135152	40.810074
3502.107569	535522.332877	40.815079
3504.733674	535799.021097	40.820084
3506.259365	536038.174454	40.825088
3507.681226	536247.642952	40.830093
3509.589655	536409.921123	40.835098
3510.122467	536541.306134	40.840103
3511.271509	536639.324726	40.845108
3511.908346	536722.373214	40.850112
3512.365715	536765.536548	40.855117
3513.336760	536782.347003	40.860122
3513.703095	536783.296593	40.865127
3514.852438	536762.934937	40.870132
3516.015169	536728.025430	40.875136
3515.980757	536681.323231	40.880141
3516.453731	536597.296421	40.885146
3516.563389	536507.688396	40.890151
3517.185749	536398.923924	40.895156
3517.943628	536285.305472	40.900160
3517.947773	536148.398214	40.905165
3518.442957	536010.356067	40.910170
3518.465640	535860.808986	40.915175
3518.637057	535693.065967	40.920180
3518.749586	535517.427164	40.925184
3518.796732	535344.262634	40.930189
3519.048263	535157.674212	40.935194
3518.919491	534966.309797	40.940199
3519.122416	534773.078719	40.945204
3519.115368	534578.266546	40.950208
3519.629360	534358.099403	40.955213
3519.605270	534152.862953	40.960218
3519.328128	533932.710981	40.965223
3519.409976	533721.561147	40.970228
3519.622627	533501.023545	40.975232
3519.401048	533281.455962	40.980237
3519.494566	533055.693453	40.985242
3519.169893	532830.243820	40.990247
3519.081060	532589.548641	40.995252
3519.014679	532365.913598	41.000256
3519.338362	532134.510577	41.005261
3519.056028	531898.565530	41.010266
3518.649711	531665.354451	41.015271
3518.463751	531424.300350	41.020276
3518.462932	531210.051048	41.025280
3518.308069	530974.875071	41.030285
3518.358169	530746.057995	41.035290
3517.905616	530526.781955	41.040295
3518.037536	530282.686325	41.045300
3517.687733	530059.509016	41.050304
3517.728610	529836.921761	41.055309
3517.677688	529608.553730	41.060314
3516.937569	529378.828533	41.065319
3517.255785	529155.733317	41.070324
3517.472407	528938.592786	41.075328
3517.084023	528714.038820	41.080333
3517.083598	528487.657932	41.085338
3516.954306	528265.926704	41.090343
3516.844462	528040.209884	41.095348
3516.484106	527830.292680	41.100352
3516.253277	527606.551529	41.105357
3516.540119	527392.094378	41.110362
3516.144893	527177.739886	41.115367
3515.824610	526964.478374	41.120372
3515.909367	526758.856987	41.125376
3515.957541	526533.895759	41.130381
3515.803795	526321.806879	41.135386
3515.553607	526122.826413	41.140391
3515.557146	525911.210215	41.145396
3515.352515	525703.149211	41.150400
3514.824377	525498.057021	41.155405
3515.006139	525293.909081	41.160410
3515.161422	525104.320842	41.165415
3514.576711	524898.925963	41.170420
3514.179956	524698.989835	41.175424
3514.268469	524505.927415	41.180429
3514.354198	524314.071736	41.185434
3513.755142	524124.284676	41.190439
3513.905297	523934.479093	41.195444
3513.847744	523750.799272	41.200448
3513.479878	523572.505701	41.205453
3513.433552	523375.971595	41.210458
3513.359907	523197.425716	41.215463
3512.936694	523015.505745	41.220468
3512.767621	522854.151081	41.225472
3513.217471	522669.722486	41.230477
3512.905956	522491.304999	41.235482
3512.537545	522319.343485	41.240487
3512.505690	522140.122019	41.245492
3512.538675	521971.721484	41.250496
3511.914819	521808.863018	41.255501
3512.289362	521635.416663	41.260506
3511.623086	521478.859455	41.265511
3511.782004	521307.306856	41.270516
3511.303141	521159.031184	41.275520
3511.793364	520989.841764	41.280525
3511.439888	520832.522899	41.285530
3511.274490	520689.131723	41.290535
3511.276094	520534.626521	41.295540
3510.932465	520395.140246	41.300544
3511.088076	520237.180906	41.305549
3510.692727	520072.854902	41.310554
3510.703251	519941.523229	41.315559
3510.636817	519793.067616	41.320564
3510.190730	519640.335351	41.325568
3510.374374	519496.121286	41.330573
3510.710769	519359.693560	41.335578
3510.093591	519233.240490	41.340583
3510.278663	519090.533845	41.345588
3510.279850	518948.207112	41.350592
3510.028854	518804.103746	41.355597
3509.923477	518662.849008	41.360602
3509.708354	518539.502138	41.365607
3509.701207	518403.370293	41.370612
3509.665934	518281.605941	41.375616
3509.664219	518144.210624	41.380621
3509.610527	518006.922818	41.385626
3509.742928	517885.784078	41.390631
3509.489408	517748.474368	41.395636
3509.265310	517628.245683	41.400640
3509.051763	517502.621016	41.405645
3509.201658	517374.418391	41.410650
3509.010482	517252.921160	41.415655
3509.091228	517130.372418	41.420660
3508.743317	517008.191723	41.425664
3508.495013	516901.469311	41.430669
3508.767398	516778.736384	41.435674
3508.219192	516655.726793	41.440679
3508.199502	516547.302598	41.445684
3508.566453	516436.145734	41.450688
3507.982902	516318.381095	41.455693
3508.400076	516222.841431	41.460698
3508.178841	516111.723063	41.465703
3508.224415	516001.923350	41.470708
3507.874881	515883.866521	41.475712
3507.910918	515780.922349	41.480717
3508.151566	515664.939468	41.485722
3507.664074	515564.494886	41.490727
3508.119978	515465.667186	41.495732
3507.747311	515360.716582	41.500736
3508.077174	515252.177375	41.505741
3507.887326	515145.482650	41.510746
3507.464478	515043.158921	41.515751
3507.878124	514943.325787	41.520756
3508.050081	514840.807172	41.525760
3507.508302	514739.860887	41.530765
3507.846998	514625.870604	41.535770
3507.561680	514534.713844	41.540775
3507.392461	514429.522839	41.545780
3507.426059	514331.458565	41.550784
3507.660194	514235.479883	41.555789
3507.458945	514130.644507	41.560794
3507.064081	514039.551947	41.565799
3507.414946	513936.998797	41.570804
3507.191319	513843.760766	41.575808
3507.045787	513746.173985	41.580813
3507.445312	513648.400864	41.585818
3507.106205	513552.254563	41.590823
3507.210957	513454.122591	41.595828
3506.988277	513365.973552	41.600832
3507.024193	513268.506436	41.605837
3507.057427	513180.770177	41.610842
3506.682740	513089.466557	41.615847
3506.898648	512987.179498	41.620852
3506.865659	512907.972972	41.625856
3506.586031	512817.661199	41.630861
3506.734065	512722.845159	41.635866
3506.249018	512652.430521	41.640871
3506.381134	512557.162029	41.645876
3506.422513	512475.823723	41.650880
3506.128407	512390.906681	41.655885
3506.168415	512302.710025	41.660890
3506.127783	512235.299954	41.665895
3505.986054	512154.542928	41.670900
3505.738655	512082.676556	41.675904
3506.071220	511994.029029	41.680909
3506.277979	511910.039609	41.685914
3506.276505	511838.486685	41.690919
3505.848916	511760.494821	41.695924
3506.109391	511684.261203	41.700928
3506.123300	511610.738115	41.705933
3505.998754	511525.285159	41.710938
3505.959577	511456.711298	41.715943
3505.635403	511369.977367	41.720948
3505.759233	511294.771427	41.725952
3505.881753	511230.911446	41.730957
3506.008291	511148.543613	41.735962
3505.939036	511074.677656	41.740967
3505.975285	510981.783453	41.745972
3505.927592	510922.386240	41.750976
3506.062324	510837.594737	41.755981
3505.867373	510746.348672	41.760986
3506.033984	510681.571605	41.765991
3505.574656	510601.611474	41.770996
3505.855826	510525.872629	41.776000
3505.879008	510455.619979	41.781005
3505.832780	510373.224046	41.786010
3505.409732	510300.115090	41.791015
3505.523726	510229.746317	41.796020
3505.558180	510168.366321	41.801024
3505.040192	510098.397821	41.806029
3505.550545	510022.418873	41.811034
3505.313639	509963.601795	41.816039
3505.423317	509887.028852	41.821044
3505.081815	509827.975322	41.826048
3505.167984	509757.406785	41.831053
3505.418162	509686.055880	41.836058
3504.881114	509622.795552	41.841063
3505.145142	509564.756218	41.846068
3505.081492	509497.134825	41.851072
3504.856104	509434.480789	41.856077
3504.672802	509367.936505	41.861082
3504.595347	509312.218802	41.866087
3504.879919	509252.359352	41.871092
3505.060352	509197.458451	41.876096
3504.781940	509135.265248	41.881101
3504.760357	509067.282202	41.886106
3504.290368	509011.271347	41.891111
3504.712679	508955.171852	41.896116
3504.705570	508907.107799	41.901120
3504.760158	508843.852779	41.906125
3504.593455	508787.743405	41.911130
3504.552828	508734.287314	41.916135
3504.517439	508669.481989	41.921140
3505.024120	508619.168233	41.926144
3504.854342	508566.589030	41.931149
3504.667958	508496.611406	41.936154
3504.783417	508443.382112	41.941159
3504.675432	508374.551743	41.946164
3504.911331	508310.812185	41.951168
3504.694662	508261.265412	41.956173
3504.968188	508197.317736	41.961178
3504.311850	508140.525413	41.966183
3504.640785	508084.436998	41.971188
3504.194100	508030.688365	41.976192
3504.287144	507979.528806	41.981197
3504.623507	507912.947241	41.986202
3504.794551	507858.496557	41.991207
3504.548471	507800.579800	41.996212
3504.663156	507741.043032	42.001216
3504.665717	507691.964550	42.006221
3504.943106	507635.125779	42.011226
3504.755156	507582.243106	42.016231
3504.567932	507524.416943	42.021236
3504.779635	507467.184196	42.026240
3504.609545	507410.868129	42.031245
3504.613229	507346.454198	42.036250
3504.579750	507288.300501	42.041255
3504.734436	507229.915518	42.046260
3504.912057	507170.164796	42.051264
3504.303685	507115.176804	42.056269
3504.358275	507045.810265	42.061274
3504.456873	506998.379038	42.066279
3504.350767	506950.222867	42.071284
3504.768211	506897.747865	42.076288
3503.949576	506840.067613	42.081293
3504.462505	506785.105627	42.086298
3504.091525	506744.001585	42.091303
3503.797698	506690.829408	42.096308
3504.323338	506636.621525	42.101312
3503.785195	506590.397786	42.106317
3504.451227	506538.134995	42.111322
3504.368733	506492.495807	42.116327
3504.101952	506438.460926	42.121332
3504.011980	506385.962110	42.126336
3503.654756	506335.673817	42.131341
3504.342898	506299.397716	42.136346
3503.887465	506248.317277	42.141351
3503.971520	506193.318859	42.146356
3504.131526	506153.088943	42.151360
3503.855217	506104.149269	42.156365
3503.633944	506041.126470	42.161370
3503.821540	506009.417207	42.166375
3503.960938	505960.664582	42.171380
3504.530535	505919.764918	42.176384
3503.800707	505872.963322	42.181389
3503.981083	505819.915888	42.186394
3503.703844	505770.218513	42.191399
3503.836162	505727.772048	42.196404
3503.988802	505678.713718	42.201408
3503.750250	505626.689254	42.206413
3504.166310	505580.465093	42.211418
3504.202620	505551.149388	42.216423
3503.979821	505495.540215	42.221428
3503.908614	505443.035011	42.226432
3503.330978	505397.267578	42.231437
3503.834593	505357.435987	42.236442
3503.535168	505309.354806	42.241447
3503.925788	505262.528197	42.246452
3504.188413	505219.505011	42.251456
3503.988828	505185.533528	42.256461
3504.134961	505140.762522	42.261466
3503.556339	505090.857438	42.266471
3503.826907	505043.292056	42.271476
3503.926122	505001.605329	42.276480
3504.019900	504960.322925	42.281485
3503.810990	504904.860643	42.286490
3503.736287	504857.600623	42.291495
3503.664921	504821.993923	42.296500
3503.743910	504768.403419	42.301504
3503.515074	504726.615590	42.306509
3503.891989	504674.037833	42.311514
3503.916092	504642.956394	42.316519
3503.821589	504594.285965	42.321524
3504.135535	504543.735569	42.326528
3504.134527	504493.940325	42.331533
3503.859114	504450.191336	42.336538
3503.716497	504408.742324	42.341543
3503.679683	504352.897966	42.346548
3503.669212	504309.813647	42.351552
3503.456657	504289.564988	42.356557
3503.448781	504229.074056	42.361562
3503.522060	504194.755050	42.366567
3503.614501	504156.144516	42.371572
3503.650546	504116.886771	42.376576
3503.682165	504082.119905	42.381581
3503.809591	504025.895548	42.386586
3503.930240	503990.206452	42.391591
3503.543123	503949.096879	42.396596
3503.915338	503890.210332	42.401600
3503.460460	503851.986872	42.406605
3503.836566	503803.644160	42.411610
3503.852961	503762.673078	42.416615
3503.724722	503718.646689	42.421620
3503.747514	503675.353477	42.426624
3503.903716	503640.112068	42.431629
3503.719309	503594.984047	42.436634
3503.751414	503545.281273	42.441639
3503.587824	503509.130669	42.446644
3503.702886	503456.690122	42.451648
3503.523260	503421.197707	42.456653
3503.846212	503384.920625	42.461658
3504.178420	503332.748568	42.466663
3503.831132	503287.897208	42.471668
3504.102853	503239.770671	42.476672
3503.550419	503195.960062	42.481677
3503.930991	503138.683733	42.486682
3503.937828	503099.377303	42.491687
3503.589667	503048.420129	42.496692
3503.791538	503002.120101	42.501696
3503.463850	502967.810110	42.506701
3503.768130	502918.264649	42.511706
3503.541762	502879.397565	42.516711
3503.958029	502844.971514	42.521716
3503.895239	502803.555915	42.526720
3503.609718	502753.849384	42.531725
3503.695160	502710.038951	42.536730
3503.773034	502672.637693	42.541735
3503.790708	502630.855874	42.546740
3503.854281	502581.043967	42.551744
3503.573588	502543.496341	42.556749
3503.536313	502490.319118	42.561754
3503.580012	502451.459314	42.566759
3503.301411	502412.346808	42.571764
3503.441073	502363.935154	42.576768
3503.399876	502329.074476	42.581773
3504.044347	502294.611606	42.586778
3503.287953	502252.091344	42.591783
3503.056504	502210.296617	42.596788
3503.611950	502171.507805	42.601792
3503.465600	502140.144738	42.606797
3503.297526	502101.619707	42.611802
3503.513496	502062.025614	42.616807
3503.192598	502020.244258	42.621812
3503.564434	501979.566026	42.626816
3503.413296	501937.707555	42.631821
3503.713059	501891.085977	42.636826
3503.554084	501857.049858	42.641831
3503.595771	501810.871867	42.646836
3503.435421	501769.115263	42.651840
3503.318665	501731.792323	42.656845
3503.171726	501688.519571	42.661850
3503.410153	501660.728791	42.666855
3502.555777	501628.314183	42.671860
3503.262602	501592.174720	42.676864
3502.858053	501552.776721	42.681869
3503.264949	501524.000693	42.686874
3502.947114	501497.910937	42.691879
3502.761356	501456.359233	42.696884
3503.515149	501425.762861	42.701888
3502.936214	501388.712807	42.706893
3503.317115	501345.609205	42.711898
3503.070925	501317.590407	42.716903
3503.180204	501284.570911	42.721908
3503.217135	501237.433047	42.726912
3503.059507	501207.684523	42.731917
3502.871138	501160.884248	42.736922
3503.236899	501133.224033	42.741927
3502.982054	501095.466778	42.746932
3503.271628	501057.877022	42.751936
3502.987339	501040.612303	42.756941
3502.830958	501000.518162	42.761946
3503.419916	500969.744630	42.766951
3503.017298	500930.849278	42.771956
3503.268381	500894.324830	42.776960
3503.040794	500874.477430	42.781965
3503.195973	500833.425995	42.786970
3503.186556	500804.814258	42.791975
3503.245453	500766.098969	42.796980
3503.252438	500725.625398	42.801985
3502.650734	500693.976811	42.806989
3503.262728	500661.634643	42.811994
3502.938338	500631.204383	42.816999
3502.926695	500597.445173	42.822004
3502.959363	500564.940616	42.827009
3502.585463	500537.545766	42.832013
3503.346739	500499.830704	42.837018
3502.935942	500473.804039	42.842023
3503.077570	500432.804049	42.847028
3503.269710	500400.728499	42.852033
3502.935674	500367.775909	42.857037
3503.376778	500326.426224	42.862042
3503.393714	500293.973976	42.867047
3502.948036	500246.958472	42.872052
3503.522998	500230.215140	42.877057
3503.230247	500195.842683	42.882061
3503.403414	500151.102486	42.887066
3503.140750	500120.257821	42.892071
3503.069639	500080.652545	42.897076
3503.311705	500049.073120	42.902081
3502.672104	500000.724393	42.907085
3502.782594	499980.116627	42.912090
3503.542623	499946.639566	42.917095
3503.145771	499915.411612	42.922100
3503.510733	499869.278089	42.927105
3502.823592	499832.240905	42.932109
3503.172346	499796.707862	42.937114
3503.399657	499768.460995	42.942119
3502.888070	499733.717760	42.947124
3503.276740	499698.632479	42.952129
3502.981033	499654.468404	42.957133
3503.353368	499618.022831	42.962138
3503.366553	499585.216314	42.967143
3503.043446	499557.458439	42.972148
3502.924924	499526.287277	42.977153
3503.012456	499492.257735	42.982157
3502.617239	499462.996838	42.987162
3503.229116	499423.031154	42.992167
3502.913841	499392.697828	42.997172
3502.996703	499361.898731	43.002177
3502.901340	499331.531057	43.007181
3502.988006	499292.252377	43.012186
3503.063851	499257.164248	43.017191
3503.004440	499229.061897	43.022196
3503.188190	499197.186892	43.027201
3502.903931	499165.031356	43.032205
3502.890435	499130.612935	43.037210
3502.932953	499094.116443	43.042215
3502.586621	499066.563130	43.047220
3503.051545	499040.397632	43.052225
3502.791219	499006.622974	43.057229
3502.747084	498969.786363	43.062234
3502.933455	498941.392861	43.067239
3502.806247	498911.887273	43.072244
3502.617874	498879.060068	43.077249
3502.684071	498862.394348	43.082253
3502.594691	498832.277063	43.087258
3503.028171	498808.791010	43.092263
3502.833956	498777.175792	43.097268
3503.120888	498733.523926	43.102273
3502.818474	498712.372973	43.107277
3503.147781	498674.720437	43.112282
3502.953238	498643.761113	43.117287
3502.801759	498618.296444	43.122292
3502.824217	498580.035283	43.127297
3502.886620	498557.868371	43.132301
3503.088482	498515.945143	43.137306
3503.104032	498492.372204	43.142311
3502.863703	498458.744587	43.147316
3503.057681	498413.390176	43.152321
3503.366858	498389.821854	43.157325
3503.380203	498345.353375	43.162330
3503.267247	498313.522622	43.167335
3503.266129	498285.762702	43.172340
3503.150407	498245.503255	43.177345
3502.801580	498214.213722	43.182349
3502.776089	498184.589897	43.187354
3502.721083	498158.150425	43.192359
3502.799673	498128.914079	43.197364
3503.017680	498093.094418	43.202369
3502.784200	498064.966450	43.207373
3502.997408	498035.254707	43.212378
3503.000419	498000.982490	43.217383
3502.727374	497968.216897	43.222388
3502.605144	497932.247893	43.227393
3502.724765	497916.935589	43.232397
3502.279275	497879.149215	43.237402
3502.684937	497862.429536	43.242407
3502.873985	497834.790596	43.247412
3503.033913	497796.455529	43.252417
3502.776977	497783.826361	43.257421
3502.678933	497745.733204	43.262426
3502.473465	497703.467248	43.267431
3502.387909	497682.281064	43.272436
3502.667064	497644.583223	43.277441
3502.390313	497634.935041	43.282445
3502.618439	497593.711751	43.287450
3502.585153	497583.167569	43.292455
3502.064502	497562.200344	43.297460
3502.532479	497536.031701	43.302465
3502.478967	497510.095587	43.307469
3502.505018	497489.951746	43.312474
3502.522617	497471.878696	43.317479
3502.498267	497437.357047	43.322484
3502.828681	497400.104887	43.327489
3502.527388	497377.588985	43.332493
3502.562277	497349.367412	43.337498
3502.761963	497329.246808	43.342503
3502.576012	497300.302364	43.347508
3502.620522	497262.438155	43.352513
3502.833641	497243.375348	43.357517
3502.919794	497212.975048	43.362522
3502.787028	497187.605943	43.367527
3502.517688	497158.775150	43.372532
3502.889709	497124.695857	43.377537
3502.542248	497096.785684	43.382541
3502.501667	497076.399261	43.387546
3502.543005	497045.753206	43.392551
3502.736463	497026.743656	43.397556
3503.015586	496994.344267	43.402561
3502.856140	496973.471426	43.407565
3502.894408	496935.001620	43.412570
3503.120970	496909.121823	43.417575
3502.761710	496876.013872	43.422580
3502.793350	496836.838154	43.427585
3502.863078	496803.511851	43.432589
3502.865961	496778.221890	43.437594
3503.018520	496754.624850	43.442599
3502.514161	496723.760175	43.447604
3502.921662	496699.870985	43.452609
3502.822170	496672.527162	43.457613
3502.721117	496639.580415	43.462618
3503.008574	496618.435615	43.467623
3502.698157	496579.261963	43.472628
3502.919245	496537.279640	43.477633
3502.811607	496508.775767	43.482637
3502.741822	496485.717689	43.487642
3502.996922	496453.371332	43.492647
3502.694057	496427.017806	43.497652
3502.892073	496394.528767	43.502657
3502.657428	496367.861643	43.507661
3502.793428	496334.624931	43.512666
3502.844466	496303.773910	43.517671
3502.721889	496278.098780	43.522676
3503.248325	496247.577503	43.527681
3502.631757	496214.255709	43.532685
3502.378213	496195.718492	43.537690
3502.677093	496165.686777	43.542695
3502.446523	496147.448805	43.547700
3502.597037	496121.831867	43.552705
3502.704301	496098.947556	43.557709
3502.491847	496074.144224	43.562714
3502.500367	496032.344990	43.567719
3502.670783	496007.936293	43.572724
3502.930463	495989.117030	43.577729
3502.454629	495962.284784	43.582733
3502.255922	495930.058385	43.587738
3502.680332	495905.509033	43.592743
3502.489151	495873.937595	43.597748
3502.877266	495852.170266	43.602753
3502.400816	495828.316264	43.607757
3502.453474	495803.824594	43.612762
3502.547381	495773.622057	43.617767
3502.349420	495741.647540	43.622772
3502.634587	495725.953836	43.627777
3502.888858	495698.755091	43.632781
3502.877224	495662.359496	43.637786
3502.830320	495634.551236	43.642791
3502.584912	495612.831659	43.647796
3503.036194	495572.931031	43.652801
3502.309793	495544.622554	43.657805
3502.620076	495521.453349	43.662810
3502.654019	495499.488206	43.667815
3502.593127	495483.949063	43.672820
3502.697037	495446.828205	43.677825
3502.745751	495423.245207	43.682829
3502.579149	495390.507813	43.687834
3502.771760	495365.337365	43.692839
3502.732887	495337.173918	43.697844
3502.740153	495298.755172	43.702849
3502.859973	495273.444447	43.707853
3502.394486	495252.970186	43.712858
3502.935905	495218.658222	43.717863
3502.723831	495199.204603	43.722868
3502.758002	495152.350556	43.727873
3503.045499	495126.761070	43.732877
3502.899411	495100.986593	43.737882
3502.985696	495061.595746	43.742887
3502.553897	495036.572392	43.747892
3502.742805	495007.464163	43.752897
3502.704621	494984.903675	43.757901
3502.718151	494955.772152	43.762906
3502.715465	494924.169362	43.767911
3502.558318	494892.590540	43.772916
3502.900244	494862.852404	43.777921
3502.988758	494838.202109	43.782925
3502.986472	494808.416459	43.787930
3502.998739	494781.809030	43.792935
3502.674188	494749.094803	43.797940
3503.018429	494713.853147	43.802945
3502.485894	494680.009975	43.807949
3502.568211	494663.387500	43.812954
3503.013522	494633.683305	43.817959
3502.687221	494615.811744	43.822964
3502.300621	494581.541755	43.827969
3502.648148	494537.110801	43.832973
3502.748338	494515.285354	43.837978
3502.878367	494492.243571	43.842983
3502.627432	494463.253211	43.847988
3502.614170	494434.478239	43.852993
3502.544700	494409.044043	43.857997
3502.459044	494372.353895	43.863002
3502.720249	494354.844973	43.868007
3502.455655	494331.359488	43.873012
3502.436291	494303.443481	43.878017
3502.434514	494282.239398	43.883021
3502.805335	494248.810025	43.888026
3502.640119	494228.136164	43.893031
3502.171869	494199.229594	43.898036
3502.854945	494174.788603	43.903041
3502.732781	494149.160216	43.908045
3502.439787	494117.903814	43.913050
3502.992866	494103.024995	43.918055
3502.601341	494069.007030	43.923060
3502.894181	494050.180160	43.928065
3502.616779	494017.406501	43.933069
3502.639818	493998.924475	43.938074
3502.862062	493959.862975	43.943079
3502.376998	493930.554599	43.948084
3502.785459	493892.524187	43.953089
3502.346385	493868.964148	43.958093
3502.434974	493856.378834	43.963098
3502.420624	493820.181113	43.968103
3502.314921	493801.769365	43.973108
3502.707295	493776.716617	43.978113
3502.813521	493764.633364	43.983117
3502.676433	493731.332360	43.988122
3502.507028	493694.603090	43.993127
3502.264983	493675.758007	43.998132
3502.368874	493642.166862	44.003137
3502.379620	493623.837752	44.008141
3502.257323	493603.711724	44.013146
3502.571183	493584.729532	44.018151
3502.254725	493562.008239	44.023156
3502.805849	493534.456423	44.028161
3502.683200	493508.927991	44.033165
3502.788602	493468.823119	44.038170
3502.627479	493449.561244	44.043175
3502.560059	493423.519179	44.048180
3503.093097	493393.748382	44.053185
3502.899453	493361.869064	44.058189
3503.140671	493332.850413	44.063194
3502.947074	493297.386176	44.068199
3502.615125	493269.870311	44.073204
3502.703480	493244.662024	44.078209
3502.350916	493216.492898	44.083213
3502.605614	493184.947356	44.088218
3502.799103	493157.147558	44.093223
3502.536032	493131.488863	44.098228
3502.814907	493109.179145	44.103233
3502.711495	493085.313184	44.108237
3502.793257	493047.987847	44.113242
3502.489144	493012.792587	44.118247
3502.495920	492995.422652	44.123252
3502.318267	492954.249650	44.128257
3502.547468	492943.156420	44.133261
3502.676460	492912.589197	44.138266
3502.657131	492885.478398	44.143271
3502.580875	492870.999241	44.148276
3502.928097	492829.794713	44.153281
3502.382588	492793.980115	44.158285
3502.379393	492784.336694	44.163290
3502.433059	492760.445773	44.168295
3502.601031	492738.304237	44.173300
3502.233950	492711.247238	44.178305
3502.599373	492685.994898	44.183309
3502.387733	492653.460477	44.188314
3502.622416	492634.893342	44.193319
3502.642362	492614.743851	44.198324
3502.411642	492581.101415	44.203329
3502.619245	492559.104925	44.208333
3502.535288	492538.214115	44.213338
3502.823894	492500.804738	44.218343
3502.548263	492480.196136	44.223348
3502.696786	492452.452525	44.228353
3502.799617	492420.979504	44.233357
3502.419751	492387.208363	44.238362
3502.222163	492356.236392	44.243367
3502.566078	492343.458599	44.248372
3502.683047	492323.849044	44.253377
3502.732193	492293.292987	44.258381
3502.628231	492261.801319	44.263386
3502.987986	492233.923448	44.268391
3502.226712	492211.673272	44.273396
3502.613660	492179.145663	44.278401
3502.614338	492144.304887	44.283405
3502.235428	492133.053220	44.288410
3502.680902	492095.163980	44.293415
3502.507490	492085.647587	44.298420
3502.576646	492050.846432	44.303425
3502.218436	492028.735239	44.308429
3502.246896	492010.754862	44.313434
3502.294329	491981.006345	44.318439
3502.164599	491955.678349	44.323444
3502.129514	491938.263211	44.328449
3502.346195	491921.667283	44.333453
3502.328780	491905.562215	44.338458
3502.527829	491879.728478	44.343463
3502.103775	491853.183744	44.348468
3502.458009	491825.003008	44.353473
3502.499160	491799.092715	44.358477
3502.630968	491776.854404	44.363482
3502.470390	491742.542741	44.368487
3502.492185	491731.783865	44.373492
3502.405626	491706.499227	44.378497
3502.775174	491683.466355	44.383501
3502.410917	491665.597172	44.388506
3502.713370	491626.668610	44.393511
3502.366725	491603.242109	44.398516
3502.524487	491575.343958	44.403521
3502.467837	491547.832591	44.408525
3502.289531	491523.672830	44.413530
3502.508836	491492.230240	44.418535
3502.458494	491476.533805	44.423540
3502.491394	491452.290567	44.428545
3502.659908	491433.429275	44.433549
3502.601197	491414.401332	44.438554
3502.591087	491378.449548	44.443559
3502.454245	491362.110002	44.448564
3502.590304	491326.135347	44.453569
3502.328638	491305.522962	44.458573
3502.448208	491280.710499	44.463578
3502.680379	491253.204148	44.468583
3502.325018	491240.231258	44.473588
3502.406550	491205.981692	44.478593
3502.665290	491182.056356	44.483597
3502.497178	491158.449890	44.488602
3502.439834	491118.364077	44.493607
3502.269842	491106.372170	44.498612
3502.408612	491075.446218	44.503617
3502.332187	491046.472592	44.508621
3502.538990	491036.542887	44.513626
3502.678556	491011.878365	44.518631
3502.413269	490978.439716	44.523636
3502.272245	490959.121022	44.528641
3502.446031	490932.330141	44.533645
3502.377441	490910.374228	44.538650
3502.413919	490884.210602	44.543655
3502.447778	490864.157602	44.548660
3502.386700	490841.139961	44.553665
3502.280333	490803.989833	44.558669
3502.364100	490794.937586	44.563674
3502.770386	490769.978673	44.568679
3502.705777	490745.294990	44.573684
3502.763272	490715.491915	44.578689
3502.595604	490692.743127	44.583693
3502.325354	490667.485334	44.588698
3502.251544	490641.136456	44.593703
3502.010972	490632.437575	44.598708
3502.239496	490592.154387	44.603713
3502.513635	490577.568000	44.608717
3502.646527	490549.671828	44.613722
3502.828106	490524.747479	44.618727
3502.344252	490498.260163	44.623732
3502.772423	490472.287370	44.628737
3502.534473	490439.146270	44.633741
3502.366608	490414.175118	44.638746
3502.631974	490381.359565	44.643751
3502.374804	490367.461651	44.648756
3502.531513	490342.540872	44.653761
3502.428858	490319.781407	44.658765
3502.495122	490295.127124	44.663770
3502.440181	490269.431162	44.668775
3502.525001	490247.803915	44.673780
3502.322184	490220.312878	44.678785
3502.537462	490204.775789	44.683789
3502.400975	490172.022318	44.688794
3502.858550	490154.427460	44.693799
3502.310984	490123.606367	44.698804
3502.414835	490090.966822	44.703809
3502.443482	490061.267951	44.708813
3502.411095	490047.183261	44.713818
3502.609029	490016.599446	44.718823
3502.404096	490000.319525	44.723828
3502.317556	489980.233590	44.728833
3502.444381	489963.598998	44.733837
3501.981437	489932.814849	44.738842
3502.134202	489902.692345	44.743847
3502.227159	489887.476974	44.748852
3502.261440	489856.110282	44.753857
3502.129376	489843.303449	44.758861
3501.956995	489830.856389	44.763866
3502.289687	489798.635118	44.768871
3502.109179	489793.714026	44.773876
3502.057698	489767.208649	44.778881
3502.614658	489747.173774	44.783885
3502.271142	489726.218460	44.788890
3502.304455	489702.022858	44.793895
3502.354066	489681.006306	44.798900
3502.254011	489659.154480	44.803905
3502.430411	489641.097763	44.808909
3502.005066	489616.266368	44.813914
3502.406463	489583.629934	44.818919
3502.283891	489570.164863	44.823924
3502.048212	489550.808600	44.828929
3502.536727	489531.541629	44.833933
3502.274606	489508.351239	44.838938
3502.271706	489487.645606	44.843943
3502.116433	489454.944013	44.848948
3502.017105	489440.364149	44.853953
3502.190972	489410.792917	44.858957
3501.805619	489401.964349	44.863962
3502.359704	489378.949767	44.868967
3502.085845	489360.912281	44.873972
3502.023653	489342.740830	44.878977
3502.189762	489321.705653	44.883981
3502.179559	489308.626889	44.888986
3502.380745	489280.263229	44.893991
3502.515366	489262.869109	44.898996
3502.373131	489230.266010	44.904001
3502.411594	489201.877022	44.909005
3502.121326	489176.518852	44.914010
3502.446056	489165.458495	44.919015
3502.256839	489150.033779	44.924020
3502.006800	489122.750116	44.929025
3502.368624	489096.835805	44.934029
3502.427020	489086.170363	44.939034
3502.584410	489050.288001	44.944039
3502.167480	489021.717022	44.949044
3502.071081	489007.388808	44.954049
3502.396075	488987.944581	44.959053
3502.518451	488967.117738	44.964058
3502.707254	488943.452281	44.969063
3502.281879	488927.407531	44.974068
3502.293960	488905.537172	44.979073
3502.544806	488879.942790	44.984077
3502.527359	488853.430525	44.989082
3502.389052	488820.825938	44.994087
3502.353732	488799.518356	44.999092
3502.176046	488762.778371	45.004097
3502.483290	488750.912355	45.009101
3502.095454	488736.578733	45.014106
3502.383593	488698.351962	45.019111
3502.222704	488688.225417	45.024116
3502.420239	488665.416761	45.029121
3502.179257	488631.363091	45.034125
3501.953527	488613.923294	45.039130
3502.076761	488597.489792	45.044135
3502.375612	488576.230908	45.049140
3502.425158	488559.707821	45.054145
3502.500308	488535.604867	45.059149
3502.531998	488513.781401	45.064154
3502.534807	488481.659188	45.069159
3502.330313	488465.377554	45.074164
3502.183298	488447.571776	45.079169
3502.493304	488409.239866	45.084173
3502.386966	488397.336923	45.089178
3502.615994	488368.260148	45.094183
3502.213911	488353.625344	45.099188
3502.494923	488322.671658	45.104193
3502.206357	488304.382675	45.109197
3501.789719	488283.083204	45.114202
3502.370787	488261.072874	45.119207
3501.779414	488242.830937	45.124212
3501.562651	488223.167002	45.129217
3502.170957	488205.142390	45.134221
3502.138013	488198.278556	45.139226
3501.978131	488173.049946	45.144231
3502.145113	488152.013022	45.149236
3502.181204	488137.966416	45.154241
3502.147848	488111.859396	45.159245
3501.859806	488091.650803	45.164250
3502.421088	488069.946322	45.169255
3502.243181	488040.629205	45.174260
3502.201867	488036.544508	45.179265
3502.151322	488008.167151	45.184269
3502.263149	487984.007112	45.189274
3502.036397	487960.758353	45.194279
3502.129799	487955.996072	45.199284
3502.360394	487933.383210	45.204289
3502.627397	487906.016912	45.209293
3502.259908	487897.235196	45.214298
3502.730285	487860.139652	45.219303
3502.388152	487841.656418	45.224308
3502.696033	487810.192434	45.229313
3502.362331	487793.172566	45.234317
3502.252017	487765.662700	45.239322
3502.169802	487734.309772	45.244327
3502.333069	487717.212485	45.249332
3501.901130	487688.994903	45.254337
3502.248205	487676.869316	45.259341
3502.070447	487659.471472	45.264346
3502.575090	487638.482316	45.269351
3502.218532	487616.566460	45.274356
3502.359279	487588.663646	45.279361
3502.031754	487561.035685	45.284365
3502.264061	487553.322142	45.289370
3502.906550	487521.906516	45.294375
3502.238744	487509.938725	45.299380
3502.145448	487476.314081	45.304385
3502.336828	487457.090740	45.309389
3501.656539	487434.315831	45.314394
3502.352043	487420.772068	45.319399
3502.303488	487406.737964	45.324404
3502.189563	487376.854015	45.329409
3502.405684	487363.990915	45.334413
3502.118615	487333.982296	45.339418
3502.138135	487305.087636	45.344423
3502.191819	487292.502303	45.349428
3501.968059	487267.635709	45.354433
3502.404586	487256.354540	45.359437
3502.095714	487234.178165	45.364442
3502.119943	487203.716769	45.369447
3502.189048	487187.340687	45.374452
3502.233682	487172.786766	45.379457
3502.518087	487155.114389	45.384461
3502.441392	487130.174177	45.389466
3502.105325	487103.051823	45.394471
3502.440187	487088.301127	45.399476
3502.384691	487075.934649	45.404481
3502.214288	487050.806847	45.409485
3502.049660	487019.364260	45.414490
3501.841042	487000.859233	45.419495
3502.063849	486989.459594	45.424500
3502.326171	486960.981101	45.429505
3502.242144	486940.234130	45.434509
3502.080320	486912.781259	45.439514
3502.009883	486903.245589	45.444519
3501.931521	486881.638968	45.449524
3502.160163	486877.764509	45.454529
3502.439828	486845.141181	45.459533
3502.085058	486828.376074	45.464538
3502.277397	486807.232338	45.469543
3502.130478	486788.363874	45.474548
3501.838021	486764.769942	45.479553
3501.941530	486737.174445	45.484557
3501.928879	486738.590716	45.489562
3502.181297	486716.831366	45.494567
3502.286492	486694.589777	45.499572
3502.315003	486673.016744	45.504577
3502.289961	486643.370094	45.509581
3502.148900	486628.490970	45.514586
3502.217332	486608.224947	45.519591
3502.353628	486588.352434	45.524596
3502.265152	486563.413135	45.529601
3502.315013	486544.513749	45.534605
3501.727059	486526.420765	45.539610
3502.005442	486506.829111	45.544615
3502.148710	486501.806057	45.549620
3501.986095	486481.171721	45.554625
3502.256366	486461.227684	45.559629
3502.125451	486440.891436	45.564634
3502.092032	486422.762550	45.569639
3502.122766	486396.743663	45.574644
3501.969907	486382.775367	45.579649
3502.104289	486348.405643	45.584653
3502.180346	486344.302231	45.589658
3502.326573	486321.144483	45.594663
3502.357734	486300.378724	45.599668
3502.234113	486283.779105	45.604673
3502.110429	486259.450950	45.609677
3502.086063	486246.775880	45.614682
3502.401787	486217.075383	45.619687
3502.463862	486194.688241	45.624692
3502.223737	486177.247908	45.629697
3502.411784	486148.981526	45.634701
3502.169117	486140.987593	45.639706
3502.456247	486104.775065	45.644711
3502.305145	486089.038247	45.649716
3502.038280	486065.742343	45.654721
3502.354480	486021.998523	45.659725
3502.259934	486014.436101	45.664730
3502.195884	485994.745542	45.669735
3501.998931	485971.236559	45.674740
3501.938831	485957.607042	45.679745
3502.275725	485937.045789	45.684749
3502.256816	485913.458498	45.689754
3502.298743	485897.337845	45.694759
3502.403235	485864.285070	45.699764
3502.203040	485842.898007	45.704769
3502.587213	485819.399392	45.709773
3502.080624	485801.747524	45.714778
3501.951278	485781.763765	45.719783
3502.088194	485771.993068	45.724788
3502.168976	485761.928010	45.729793
3502.151093	485731.924888	45.734797
3502.189236	485720.755108	45.739802
3502.214521	485687.310160	45.744807
3502.442605	485681.061278	45.749812
3502.006947	485646.324059	45.754817
3502.437372	485626.303507	45.759821
3502.137408	485553.153254	45.764826
3501.987827	485429.665412	45.769831
3502.101124	485265.570963	45.774836
3501.466548	485063.248656	45.779841
3501.285851	484800.433614	45.784845
3500.530813	484496.126378	45.789850
3500.627852	484143.787520	45.794855
3499.812235	483746.871254	45.799860
3499.043241	483315.177906	45.804865
3498.559300	482829.064028	45.809869
3497.600770	482300.920638	45.814874
3497.414585	481726.254588	45.819879
3496.531230	481116.709274	45.824884
3495.496456	480449.658451	45.829889
3494.657793	479757.736545	45.834893
3493.574762	479021.451242	45.839898
3492.593096	478221.183985	45.844903
3491.863885	477396.779287	45.849908
3490.631435	476523.129416	45.854913
3489.392519	475604.850078	45.859917
3487.674254	474650.651535	45.864922
3486.926723	473648.320770	45.869927
3485.085554	472617.179746	45.874932
3484.032471	471551.571040	45.879937
3482.460726	470439.708032	45.884941
3480.896918	469286.708118	45.889946
3479.233505	468096.524314	45.894951
3477.665096	466869.927944	45.899956
3475.716977	465610.626947	45.904961
3474.103131	464313.596872	45.909965
3472.745212	462993.309395	45.914970
3470.521885	461625.043828	45.919975
3468.619018	460227.476380	45.924980
3466.497495	458798.812345	45.929985
3464.879114	457334.884193	45.934989
3462.868734	455844.578149	45.939994
3460.741211	454324.302725	45.944999
3458.631032	452770.284542	45.950004
3456.467181	451186.728226	45.955009
3454.770515	449575.216499	45.960013
3452.200779	447929.521539	45.965018
3449.646881	446258.357790	45.970023
3447.593405	444572.126290	45.975028
3445.061762	442853.149901	45.980033
3443.052653	441108.001295	45.985037
3440.257063	439342.298096	45.990042
3437.896309	437549.614937	45.995047
3435.193202	435723.024508	46.000052
3432.409163	433895.310509	46.005057
3429.926221	432029.829374	46.010061
3427.190962	430152.756797	46.015066
3425.065807	428247.840075	46.020071
3422.569983	426329.063127	46.025076
3419.744570	424382.325084	46.030081
3416.951729	422408.070366	46.035085
3414.034508	420425.431855	46.040090
3411.241580	418412.363887	46.045095
3408.335389	416387.000623	46.050100
3405.527882	414356.255750	46.055105
3402.825401	412285.638707	46.060109
3399.808593	410211.575897	46.065114
3396.808114	408104.999287	46.070119
3393.831074	405998.777353	46.075124
3390.386814	403869.699225	46.080129
3387.715337	401739.489684	46.085133
3384.557933	399582.870512	46.090138
3381.669097	397409.819540	46.095143
3378.193895	395222.955033	46.100148
3375.123044	393035.827780	46.105153
3372.365862	390833.579432	46.110157
3368.925589	388620.958634	46.115162
3365.477734	386364.398043	46.120167
3362.345817	384128.280348	46.125172
3359.048525	381882.191645	46.130177
3355.902619	379619.454730	46.135181
3352.706065	377348.328399	46.140186
3349.278423	375066.174568	46.145191
3345.932971	372761.920341	46.150196
3342.050030	370462.333613	46.155201
3339.243325	368149.688235	46.160205
3335.350848	365826.861367	46.165210
3332.120307	363497.494797	46.170215
3328.889683	361166.724723	46.175220
3324.864535	358829.188206	46.180225
3321.820559	356470.657246	46.185229
3317.992886	354118.627342	46.190234
3314.811906	351759.026914	46.195239
3311.540282	349390.879197	46.200244
3307.342723	347017.493519	46.205249
3303.861702	344639.735160	46.210253
3300.433886	342252.497300	46.215258
3296.813960	339883.638292	46.220263
3293.180130	337492.245722	46.225268
3289.561416	335097.845621	46.230273
3285.826963	332698.095858	46.235277
3282.315678	330301.008993	46.240282
3278.635695	327894.694735	46.245287
3274.866437	325487.638797	46.250292
3271.072514	323088.305811	46.255297
3267.443936	320669.576308	46.260301
3263.619414	318254.328541	46.265306
3260.165568	315848.152352	46.270311
3256.523908	313433.556989	46.275316
3252.507398	311023.933068	46.280321
3249.043576	308595.626792	46.285325
3245.290247	306187.197836	46.290330
3241.366931	303760.891401	46.295335
3238.108057	301336.252466	46.300340
3233.582446	298911.879990	46.305345
3229.951581	296492.888174	46.310349
3226.151423	294086.014054	46.315354
3222.352019	291652.594579	46.320359
3218.685716	289238.914931	46.325364
3214.416001	286824.958599	46.330369
3210.658995	284411.955523	46.335373
3206.505518	282015.148055	46.340378
3202.679146	279609.808757	46.345383
3198.708551	277205.714139	46.350388
3194.724310	274812.599186	46.355393
3190.941958	272415.717486	46.360397
3187.049515	270035.440094	46.365402
3183.186989	267652.168339	46.370407
3179.072716	265268.368242	46.375412
3175.211032	262898.683239	46.380417
3171.122363	260518.159768	46.385421
3167.492911	258163.440819	46.390426
3163.567345	255792.451045	46.395431
3159.598386	253425.756046	46.400436
3155.121091	251071.963102	46.405441
3151.775118	248717.170297	46.410445
3147.739117	246387.743190	46.415450
3143.306700	244040.751970	46.420455
3139.447385	241698.027462	46.425460
3134.930600	239391.447240	46.430465
3131.250834	237070.583895	46.435469
3127.416019	234764.883707	46.440474
3123.144381	232465.046683	46.445479
3119.221501	230174.009910	46.450484
3115.542082	227901.216346	46.455489
3111.397211	225617.591726	46.460493
3106.977091	223355.429573	46.465498
3102.877493	221082.752769	46.470503
3098.829767	218831.060172	46.475508
3094.437640	216589.438980	46.480513
3090.683456	214343.934931	46.485517
3086.259128	212119.356981	46.490522
3082.217644	209918.828944	46.495527
3078.254460	207719.478992	46.500532
3074.091344	205524.205385	46.505537
3070.093306	203341.943816	46.510541
3065.445410	201163.705945	46.515546
3061.449701	199005.131912	46.520551
3057.227445	196853.423152	46.525556
3052.870358	194726.215519	46.530561
3048.817417	192587.968263	46.535565
3044.498674	190479.440937	46.540570
3040.015749	188389.745015	46.545575
3036.051695	186307.672987	46.550580
3031.709401	184231.354583	46.555585
3027.151788	182180.449316	46.560589
3022.646308	180148.244853	46.565594
3018.127135	178135.872581	46.570599
3013.762991	176125.203816	46.575604
3009.350260	174148.454535	46.580609
3004.818127	172172.384220	46.585613
3000.180180	170236.823940	46.590618
2995.586970	168312.993190	46.595623
2990.876176	166412.336001	46.600628
2985.711835	164529.978448	46.605633
2981.247174	162673.530933	46.610637
2976.756233	160848.158803	46.615642
2971.699568	159046.270086	46.620647
2967.003566	157267.974567	46.625652
2961.722329	155519.209459	46.630657
2956.602983	153793.188517	46.635661
2951.545201	152110.491926	46.640666
2945.869172	150434.763602	46.645671
2940.016620	148777.617165	46.650676
2934.441774	147221.222502	46.655681
2928.330585	145694.262566	46.660685
2922.064516	144243.552151	46.665690
2915.538577	142832.991550	46.670695
2909.527119	141471.376689	46.675700
2903.151799	140157.886540	46.680705
2896.854456	138914.103147	46.685709
2891.074649	137713.884754	46.690714
2885.240277	136557.953556	46.695719
2879.719154	135461.909940	46.700724
2874.323399	134395.425542	46.705729
2869.547871	133360.774975	46.710733
2864.435644	132375.545621	46.715738
2859.852967	131423.444327	46.720743
2855.406726	130499.505744	46.725748
2850.656880	129604.012970	46.730753
2846.104295	128734.126238	46.735757
2841.626996	127894.709280	46.740762
2837.591962	127088.946740	46.745767
2833.303457	126293.083969	46.750772
2828.894760	125512.670649	46.755777
2825.182430	124752.233963	46.760781
2821.191681	124013.349045	46.765786
2817.407189	123287.163844	46.770791
2813.942826	122566.677884	46.775796
2809.660928	121869.961818	46.780801
2806.209665	121186.151590	46.785805
2802.520006	120515.145896	46.790810
2798.619985	119829.585397	46.795815
2795.106443	119162.111180	46.800820
2791.323540	118518.127260	46.805825
2787.619251	117866.550342	46.810829
2784.293235	117228.557553	46.815834
2780.642274	116599.222177	46.820839
2776.928545	115957.394890	46.825844
2772.887503	115340.310502	46.830849
2769.132206	114728.049233	46.835853
2765.363403	114116.881079	46.840858
2761.427964	113528.051044	46.845863
2758.036105	112934.924702	46.850868
2753.858674	112351.606092	46.855873
2750.646974	111772.939968	46.860877
2746.480875	111201.170210	46.865882
2742.534216	110640.779862	46.870887
2738.802097	110086.772712	46.875892
2734.861741	109544.503102	46.880897
2731.130702	109002.539868	46.885901
2727.338997	108477.795323	46.890906
2723.732648	107949.991492	46.895911
2720.370292	107424.331633	46.900916
2716.421421	106904.199333	46.905921
2712.670695	106382.353368	46.910925
2709.218205	105881.850794	46.915930
2705.550389	105367.342414	46.920935
2702.245583	104861.009885	46.925940
2699.215658	104361.862369	46.930945
2695.673134	103854.285442	46.935949
2692.101583	103357.118502	46.940954
2688.570281	102852.554947	46.945959
2685.404537	102342.311320	46.950964
2681.741823	101842.842546	46.955969
2678.378064	101329.302571	46.960973
2675.050628	100833.572010	46.965978
2671.533319	100326.846262	46.970983
2668.237736	99822.368989	46.975988
2665.161295	99320.076971	46.980993
2661.654378	98808.569212	46.985997
2658.411516	98292.796369	46.991002
2654.721978	97773.326808	46.996007
2651.370269	97252.288120	47.001012
2647.663067	96745.839248	47.006017
2644.359450	96227.872757	47.011021
2641.109872	95716.578197	47.016026
2637.951794	95203.028455	47.021031
2634.399045	94678.251419	47.026036
2630.747775	94166.549235	47.031041
2627.219910	93641.773204	47.036045
2623.995060	93120.694861	47.041050
2620.495195	92589.667863	47.046055
2617.330554	92056.946075	47.051060
2613.682336	91546.748459	47.056065
2610.254816	91003.399970	47.061069
2606.810090	90480.698486	47.066074
2603.407377	89947.898474	47.071079
2599.826808	89411.476436	47.076084
2596.378986	88874.509778	47.081089
2593.073831	88340.592561	47.086093
2589.865044	87808.537607	47.091098
2586.178507	87260.571496	47.096103
2582.956302	86723.469139	47.101108
2579.350364	86189.078839	47.106113
2575.847772	85631.319773	47.111117
2572.320577	85088.171788	47.116122
2568.783311	84557.484959	47.121127
2565.823091	83997.919977	47.126132
2561.831156	83455.764382	47.131137
2558.643390	82912.261785	47.136141
2555.151045	82362.567368	47.141146
2551.869002	81803.857732	47.146151
2548.395757	81249.202740	47.151156
2544.510267	80698.014213	47.156161
2541.366226	80143.177454	47.161165
2537.958726	79588.494349	47.166170
2534.568472	79031.558872	47.171175
2530.919149	78472.973034	47.176180
2527.432150	77915.363894	47.181185
2524.043946	77354.715367	47.186189
2520.777060	76788.496893	47.191194
2516.869914	76228.828552	47.196199
2513.876707	75666.616644	47.201204
2509.993536	75106.586787	47.206209
2506.657424	74536.121175	47.211213
2503.044882	73961.482084	47.216218
2499.431070	73404.709380	47.221223
2496.193800	72825.693534	47.226228
2492.087349	72269.948234	47.231233
2488.920007	71708.837106	47.236237
2485.738881	71140.261410	47.241242
2481.971316	70572.335271	47.246247
2479.109911	70000.179430	47.251252
2475.096014	69431.453097	47.256257
2471.664671	68850.974497	47.261261
2468.220417	68292.976229	47.266266
2464.835912	67706.714092	47.271271
2461.730125	67127.125077	47.276276
2457.750088	66556.070294	47.281281
2454.718870	65979.853562	47.286285
2450.938386	65401.722721	47.291290
2447.425963	64821.633882	47.296295
2444.183350	64233.455841	47.301300
2440.287848	63662.827747	47.306305
2437.079279	63077.521250	47.311309
2433.740163	62497.497348	47.316314
2430.155069	61913.761913	47.321319
2427.016934	61332.820130	47.326324
2423.440018	60748.171752	47.331329
2419.626940	60156.269957	47.336333
2416.440350	59569.374249	47.341338
2412.458362	58978.142835	47.346343
2409.174958	58382.146881	47.351348
2405.673107	57796.827890	47.356353
2402.418863	57209.980784	47.361357
2398.598143	56615.584170	47.366362
2395.568658	56031.376759	47.371367
2391.867624	55441.622407	47.376372
2388.512078	54844.507404	47.381377
2385.018889	54255.232367	47.386381
2381.290985	53643.321899	47.391386
2378.116614	53059.787621	47.396391
2374.817298	52467.805614	47.401396
2371.147231	51868.994400	47.406401
2367.727129	51269.068607	47.411405
2364.226006	50659.167499	47.416410
2360.418504	50059.872506	47.421415
2357.135780	49460.067428	47.426420
2353.451983	48853.001776	47.431425
2349.800605	48258.860862	47.436429
2346.972438	47644.368399	47.441434
2343.232033	47054.680815	47.446439
2339.900257	46445.645788	47.451444
2336.138344	45846.365678	47.456449
2332.827545	45235.958513	47.461453
2329.254353	44628.475233	47.466458
2325.651990	44023.980831	47.471463
2322.331093	43418.545895	47.476468
2318.607778	42813.893976	47.481473
2315.250105	42199.905848	47.486477
2311.920335	41590.058336	47.491482
2308.290839	40983.730035	47.496487
2305.059924	40373.235226	47.501492
2301.504663	39758.293722	47.506497
2297.824344	39138.291662	47.511501
2294.751356	38537.853809	47.516506
2291.046353	37921.979690	47.521511
2287.480682	37297.200815	47.526516
2283.992681	36695.801223	47.531521
2280.539092	36077.722163	47.536525
2277.119926	35457.246861	47.541530
2273.482542	34839.916982	47.546535
2270.297593	34220.658468	47.551540
2266.505838	33609.397568	47.556545
2262.632814	32994.839510	47.561549
2259.396547	32373.291899	47.566554
2255.864327	31762.602224	47.571559
2252.353700	31144.404272	47.576564
2248.449311	30519.073948	47.581569
2244.831034	29910.619584	47.586573
2241.420372	29301.358724	47.591578
2237.959656	28697.434056	47.596583
2234.633859	28078.171280	47.601588
2230.889106	27469.726588	47.606593
2226.951168	26862.153873	47.611597
2223.789423	26247.109585	47.616602
2220.068678	25651.324647	47.621607
2216.716511	25034.769241	47.626612
2212.787410	24440.465433	47.631617
2209.830129	23831.640289	47.636621
2206.012718	23233.490341	47.641626
2202.651858	22630.079908	47.646631
2198.785202	22038.004516	47.651636
2194.831074	21437.338988	47.656641
2191.423335	20835.390488	47.661645
2187.758908	20241.367490	47.666650
2183.679675	19664.814051	47.671655
2179.746684	19092.707566	47.676660
2174.876832	18542.114584	47.681665
2170.662118	17998.832798	47.686669
2166.666212	17451.307826	47.691674
2162.232740	16935.263184	47.696679
2158.466889	16413.134244	47.701684
2153.991725	15916.752550	47.706689
2149.868564	15408.309476	47.711693
2146.099522	14927.279423	47.716698
2141.895948	14464.797453	47.721703
2138.221665	13978.213587	47.726708
2134.149835	13531.083075	47.731713
2130.394791	13086.788487	47.736717
2126.591433	12653.516450	47.741722
2122.422544	12217.807081	47.746727
2119.037444	11788.513552	47.751732
2115.146773	11373.984531	47.756737
2111.517526	10966.837811	47.761741
2107.991838	10569.240560	47.766746
2103.911056	10168.158008	47.771751
2100.068682	9776.739422	47.776756
2095.707325	9412.312005	47.781761
2091.536228	9047.751340	47.786765
2087.905738	8694.217271	47.791770
2083.673516	8361.746422	47.796775
2079.904885	8011.567140	47.801780
2075.884506	7700.870089	47.806785
2072.141255	7384.232440	47.811789
2068.111085	7080.013464	47.816794
2064.027353	6779.605725	47.821799
2060.427810	6489.900650	47.826804
2057.165744	6215.493687	47.831809
2053.370227	5933.106936	47.836813
2049.716828	5662.323180	47.841818
2045.324739	5396.247146	47.846823
2041.876976	5128.790672	47.851828
2038.107780	4868.812199	47.856833
2034.659030	4627.825278	47.861837
2031.311158	4373.079395	47.866842
2027.624613	4130.015900	47.871847
2024.335373	3882.482682	47.876852
2020.565446	3652.339777	47.881857
2016.415981	3423.043621	47.886861
2013.378501	3187.030458	47.891866
2009.579529	2963.887547	47.896871
2006.174903	2749.055298	47.901876
2002.571002	2532.519512	47.906881
1999.218390	2307.824959	47.911885
1995.998194	2091.086063	47.916890
1992.071836	1879.708818	47.921895
1988.690659	1655.802066	47.926900
1985.437754	1447.697928	47.931905
1981.185471	1232.481061	47.936909
1978.323443	1023.602818	47.941914
1974.130844	827.810953	47.946919
1970.701568	623.682860	47.951924
1966.858748	435.342273	47.956929
1962.920074	251.476315	47.961933
1958.383717	94.302632	47.966938
1947.664579	96.198663	47.971943
1939.062759	114.504404	47.976948
1933.948213	114.813167	47.981953
1930.199905	122.625612	47.986957
1928.181857	117.605632	47.991962
1925.718325	118.776785	47.996967
1923.695607	111.501802	48.001972
1920.915803	114.933618	48.006977
1917.354898	109.669716	48.011981
1914.171532	108.744625	48.016986
1911.025454	117.706681	48.021991
1907.865818	107.587294	48.026996
1904.923755	103.264781	48.032001
1901.160865	105.368980	48.037005
1898.050993	99.414798	48.042010
1894.004660	115.347430	48.047015
1890.738111	113.217255	48.052020
1887.101567	108.417541	48.057025
1884.072197	110.584748	48.062029
1881.097699	109.943524	48.067034
1877.778450	113.690250	48.072039
1873.979179	114.265711	48.077044
1870.697877	116.313942	48.082049
1867.249298	120.817945	48.087053
1863.782906	114.780046	48.092058
1860.004650	111.464028	48.097063
1856.911228	106.272908	48.102068
1853.947753	115.497605	48.107073
1850.105188	108.372990	48.112077
1846.806801	106.412289	48.117082
1843.108587	107.544657	48.122087
1839.613833	109.727350	48.127092
1836.495510	103.477100	48.132097
1832.813865	109.460030	48.137101
1829.984455	100.342782	48.142106
1825.647165	107.908373	48.147111
1822.449200	104.375497	48.152116
1819.001094	102.605778	48.157121
1815.518209	106.074257	48.162125
1812.262008	101.269142	48.167130
1808.607780	111.218268	48.172135
1805.042866	109.150358	48.177140
1802.024011	93.529531	48.182145
1798.189644	106.081953	48.187149
1794.925436	95.779553	48.192154
1791.476753	102.128015	48.197159
1787.985619	106.581695	48.202164
1784.415474	108.330041	48.207169
1780.800743	112.034176	48.212173
1777.293913	103.272300	48.217178
1773.811025	104.247776	48.222183
1770.730759	102.971298	48.227188
1767.257123	104.685642	48.232193
1763.560801	109.607851	48.237197
1760.422225	105.932863	48.242202
1756.612774	106.494099	48.247207
1753.050564	103.391240	48.252212
1749.542904	99.387726	48.257217
1745.993971	111.905217	48.262221
1742.781430	101.926970	48.267226
1739.024880	117.941045	48.272231
1735.754503	105.839455	48.277236
1732.406412	110.511317	48.282241
1728.735918	116.021124	48.287245
1725.933731	103.701137	48.292250
1722.110819	113.429749	48.297255
1718.548053	100.519471	48.302260
1715.102125	103.020434	48.307265
1711.376184	106.792500	48.312269
1708.361932	97.656585	48.317274
1704.189869	107.876128	48.322279
1700.519857	106.935050	48.327284
1697.401553	98.764444	48.332289
1693.967648	100.826946	48.337293
1690.708505	103.118509	48.342298
1686.717063	108.055017	48.347303
1683.117658	105.676117	48.352308
1679.734776	106.427230	48.357313
1676.472184	110.446717	48.362317
1673.213774	99.719496	48.367322
1669.753184	108.850719	48.372327
1666.519762	100.217150	48.377332
1663.219029	109.630374	48.382337
1659.440345	101.053197	48.387341
1655.856328	98.662416	48.392346
1652.230871	100.201085	48.397351
1648.510381	97.056437	48.402356
1645.202537	109.599675	48.407361
1641.496239	104.247711	48.412365
1638.388514	101.324062	48.417370
1634.379848	96.920820	48.422375
1631.022955	91.789722	48.427380
1627.889253	98.361243	48.432385
1623.984022	98.333131	48.437389
1621.039532	89.607149	48.442394
1617.414170	93.471131	48.447399
1614.172927	96.066791	48.452404
1610.534458	96.576119	48.457409
1606.493237	98.315542	48.462413
1603.512547	90.341832	48.467418
1599.466476	91.256282	48.472423
1596.268053	97.765112	48.477428
1592.608763	95.186740	48.482433
1589.024198	97.073385	48.487437
1586.026393	99.213549	48.492442
1581.989176	97.358379	48.497447
1578.702775	87.280935	48.502452
1575.469361	89.255292	48.507457
1571.709947	88.973540	48.512461
1568.219697	88.251267	48.517466
1564.588412	92.856481	48.522471
1561.228336	95.926214	48.527476
1557.782502	81.447567	48.532481
1554.586009	94.887773	48.537485
1550.684911	89.797097	48.542490
1547.160752	89.368001	48.547495
1543.664033	91.617457	48.552500
1540.606097	89.230229	48.557505
1536.549885	96.049738	48.562509
1533.793361	87.876637	48.567514
1529.754625	91.536048	48.572519
1526.399531	90.960419	48.577524
1522.854151	93.641387	48.582529
1519.049412	89.200096	48.587533
1515.804294	89.679847	48.592538
1512.341362	96.669604	48.597543
1508.887896	95.637896	48.602548
1505.395126	94.311754	48.607553
1501.598097	101.002342	48.612557
1498.338363	90.243727	48.617562
1494.868208	84.633577	48.622567
1491.335415	87.837762	48.627572
1487.872841	93.207646	48.632577
1484.306921	95.119870	48.637581
1481.149543	90.460768	48.642586
1477.048931	95.597773	48.647591
1473.930012	83.320818	48.652596
1470.576097	88.683281	48.657601
1466.673525	93.182031	48.662605
1463.544316	90.144690	48.667610
1459.664326	88.600417	48.672615
1456.321912	86.966146	48.677620
1452.736702	87.976556	48.682625
1449.113041	96.082809	48.687629
1445.909458	81.313385	48.692634
1442.543866	83.317815	48.697639
1439.062348	84.622130	48.702644
1435.741934	86.277850	48.707649
1431.955852	84.870822	48.712653
1428.277264	83.137021	48.717658
1424.678854	86.924053	48.722663
1421.479624	81.910814	48.727668
1418.115086	78.293187	48.732673
1414.261056	89.130767	48.737677
1410.911704	78.683512	48.742682
1407.137956	80.283246	48.747687
1403.799491	84.982093	48.752692
1400.473952	73.430170	48.757697
1396.940631	96.043742	48.762701
1393.610780	84.277352	48.767706
1389.661634	87.751990	48.772711
1386.415310	85.239080	48.777716
1383.154152	87.037438	48.782721
1379.125382	88.338353	48.787725
1375.678580	82.778369	48.792730
1372.303254	89.729183	48.797735
1368.796908	92.587581	48.802740
1365.639165	82.294004	48.807745
1361.998593	92.348565	48.812749
1358.091572	77.084387	48.817754
1354.685288	92.164398	48.822759
1351.150084	86.032891	48.827764
1348.116338	84.151275	48.832769
1344.163516	84.222349	48.837773
1340.820458	81.607444	48.842778
1337.221334	86.444942	48.847783
1333.828588	89.810835	48.852788
1330.585932	90.366148	48.857793
1326.671078	85.068844	48.862797
1323.272164	75.670179	48.867802
1319.439758	89.104953	48.872807
1316.305341	87.612325	48.877812
1312.978438	84.229294	48.882817
1309.553135	86.651147	48.887821
1306.104634	82.094330	48.892826
1302.113919	81.930866	48.897831
1298.869834	85.488752	48.902836
1295.477546	82.745477	48.907841
1291.595940	87.354868	48.912845
1288.137371	83.267848	48.917850
1284.944604	84.704399	48.922855
1281.595348	80.467490	48.927860
1278.461964	68.585134	48.932865
1274.396361	88.162134	48.937869
1270.592471	83.492963	48.942874
1266.990061	83.148842	48.947879
1263.484651	87.753462	48.952884
1260.280651	84.395600	48.957889
1256.824681	81.349036	48.962893
1253.356532	74.748376	48.967898
1249.974064	89.675981	48.972903
1246.338884	90.912484	48.977908
1243.125724	80.108709	48.982913
1239.549197	84.167590	48.987917
1235.944009	85.734777	48.992922
1232.153970	93.180411	48.997927
1228.648787	88.183181	49.002932
1225.232408	81.631412	49.007937
1221.701540	81.241360	49.012941
1218.134229	79.265642	49.017946
1214.716930	84.824641	49.022951
1211.311548	80.893865	49.027956
1208.040256	77.514848	49.032961
1204.122516	79.257235	49.037965
1200.291114	77.917401	49.042970
1197.563752	83.872037	49.047975
1194.030366	81.720202	49.052980
1190.530347	78.060420	49.057985
1186.511868	88.382609	49.062989
1183.399048	84.868197	49.067994
1179.880826	73.577259	49.072999
1176.114712	83.546958	49.078004
1172.705403	76.696712	49.083009
1169.059293	82.731081	49.088013
1165.841818	78.695135	49.093018
1162.308364	76.062435	49.098023
1158.590307	77.647197	49.103028
1155.226034	75.285551	49.108033
1151.713802	81.011186	49.113037
1148.317025	74.488017	49.118042
1144.961321	76.449805	49.123047
1141.034834	84.331123	49.128052
1137.937796	82.978227	49.133057
1133.969726	90.682526	49.138061
1131.148658	75.069042	49.143066
1127.108198	84.727113	49.148071
1123.461499	80.220156	49.153076
1120.367299	75.022937	49.158081
1116.516850	81.329556	49.163085
1113.630481	78.722686	49.168090
1110.137307	86.561868	49.173095
1106.253378	80.924438	49.178100
1102.486683	83.159007	49.183105
1099.037981	85.609828	49.188109
1095.836139	83.564583	49.193114
1092.194173	75.459779	49.198119
1088.497767	80.704732	49.203124
1085.671832	77.392446	49.208129
1081.794494	75.025252	49.213133
1078.336436	82.245212	49.218138
1074.890019	79.659084	49.223143
1071.000845	82.852337	49.228148
1067.881566	79.009923	49.233153
1063.830486	83.569783	49.238157
1060.778303	78.891203	49.243162
1057.056646	77.622888	49.248167
1053.445885	83.044334	49.253172
1050.286679	79.464396	49.258177
1046.749578	90.752515	49.263181
1043.300797	84.496877	49.268186
1039.874475	79.968285	49.273191
1035.858763	86.430347	49.278196
1032.504353	81.786159	49.283201
1028.924288	80.113002	49.288205
1025.276179	82.838473	49.293210
1022.065753	88.241899	49.298215
1018.627057	82.908493	49.303220
1015.378582	75.887708	49.308225
1011.430520	88.018063	49.313229
1008.120103	79.336491	49.318234
1004.394040	79.350163	49.323239
1001.361387	87.380252	49.328244
997.717871	73.732925	49.333249
994.474523	79.100346	49.338253
990.698902	82.690374	49.343258
986.959957	79.396835	49.348263
983.424268	81.899172	49.353268
980.178123	79.107880	49.358273
976.800741	79.630415	49.363277
973.081601	80.740813	49.368282
970.067364	83.889629	49.373287
966.244784	79.818190	49.378292
962.748470	82.247962	49.383297
959.003782	82.868803	49.388301
955.393383	80.317708	49.393306
952.253067	81.657540	49.398311
948.445544	72.695866	49.403316
944.778815	76.395494	49.408321
941.476155	79.374078	49.413325
938.188753	79.502969	49.418330
934.572761	76.832528	49.423335
931.236558	84.368879	49.428340
927.531313	69.712473	49.433345
924.090965	84.269433	49.438349
920.814911	80.786794	49.443354
917.004741	78.314257	49.448359
913.490585	79.395916	49.453364
910.114101	79.076779	49.458369
906.548308	78.625763	49.463373
903.311237	86.868005	49.468378
899.284223	74.893877	49.473383
895.422745	69.955330	49.478388
892.611729	80.978564	49.483393
889.114483	87.840812	49.488397
885.967233	76.713646	49.493402
882.397286	82.846907	49.498407
878.548510	85.872543	49.503412
874.878282	72.438207	49.508417
871.293336	77.975866	49.513421
867.805872	76.348426	49.518426
864.648865	77.228966	49.523431
861.000933	82.558138	49.528436
857.539542	77.351677	49.533441
853.970926	77.533843	49.538445
850.575649	87.540741	49.543450
847.241042	80.479607	49.548455
843.375546	76.981169	49.553460
839.885133	80.934929	49.558465
836.142285	77.736932	49.563469
833.126049	84.271211	49.568474
829.518439	79.824654	49.573479
825.806761	80.519464	49.578484
822.930776	80.562179	49.583489
818.780172	78.025594	49.588493
815.144660	85.149809	49.593498
811.850063	84.457276	49.598503
808.091496	83.197904	49.603508
805.025021	77.885685	49.608513
801.537323	82.914678	49.613517
798.209982	76.301666	49.618522
794.698438	79.350743	49.623527
791.149081	76.394710	49.628532
787.935028	82.782618	49.633537
783.980428	82.955276	49.638541
780.485426	75.792578	49.643546
776.640524	79.301663	49.648551
773.013175	88.844828	49.653556
770.189734	79.973602	49.658561
765.938388	79.774850	49.663565
762.669688	76.240471	49.668570
759.618129	73.902962	49.673575
756.200851	83.799392	49.678580
752.885520	70.600901	49.683585
749.197827	84.256750	49.688589
745.538501	86.914395	49.693594
741.938969	70.991925	49.698599
737.747214	78.427353	49.703604
734.894564	76.713765	49.708609
731.532234	82.735625	49.713613
728.090666	77.225550	49.718618
724.550680	70.810167	49.723623
720.990250	65.837444	49.728628
717.841517	70.522616	49.733633
713.817184	76.603237	49.738637
710.288905	63.412601	49.743642
706.550930	68.891837	49.748647
703.303227	70.694487	49.753652
700.045039	68.196168	49.758657
696.237047	71.528677	49.763661
693.034741	67.594841	49.768666
689.416753	66.626808	49.773671
685.900648	71.457754	49.778676
682.208873	66.087878	49.783681
678.555575	70.339083	49.788685
675.274337	64.013143	49.793690
671.800501	74.035432	49.798695
668.561259	67.149311	49.803700
664.865147	72.821346	49.808705
661.353437	77.471282	49.813709
657.687501	68.209227	49.818714
654.414998	77.782571	49.823719
650.561183	84.219461	49.828724
647.353247	70.020372	49.833729
644.040821	87.335128	49.838733
640.222291	79.498335	49.843738
636.934653	76.925516	49.848743
633.192428	73.249740	49.853748
629.810890	74.915049	49.858753
626.531154	67.203193	49.863757
622.811757	77.807864	49.868762
619.575215	65.622174	49.873767
615.783369	68.986978	49.878772
612.714185	64.937521	49.883777
608.930454	73.831167	49.888781
604.764704	68.838802	49.893786
601.466159	69.270016	49.898791
597.673470	66.206365	49.903796
595.176132	60.065286	49.908801
591.284286	71.797759	49.913805
587.864002	70.507905	49.918810
584.331963	65.682641	49.923815
580.617471	65.055505	49.928820
577.479772	67.391522	49.933825
573.809490	64.780209	49.938829
570.204420	67.049783	49.943834
566.982918	67.342460	49.948839
563.041226	75.441308	49.953844
559.759462	67.128682	49.958849
556.377091	75.770030	49.963853
552.514478	76.551645	49.968858
549.152377	69.827036	49.973863
545.716015	74.006519	49.978868
542.596940	65.988101	49.983873
539.086833	71.564753	49.988877
535.104375	70.995156	49.993882
531.809020	66.303894	49.998887
528.167321	81.920390	50.003892
524.721788	76.170529	50.008897
520.937201	80.480153	50.013901
517.519365	70.935901	50.018906
514.206283	72.210925	50.023911
510.415649	75.268676	50.028916
507.574052	65.745451	50.033921
504.080878	76.726187	50.038925
499.906348	76.543992	50.043930
496.660936	74.110149	50.048935
492.868205	79.246763	50.053940
490.252469	70.900064	50.058945
486.475486	67.128488	50.063949
482.516386	63.432720	50.068954
478.592807	64.891371	50.073959
475.107641	82.150753	50.078964
471.910726	65.162798	50.083969
468.692928	75.012362	50.088973
465.096450	65.024548	50.093978
462.174201	72.066216	50.098983
458.331649	74.224082	50.103988
455.136930	64.562856	50.108993
450.907750	68.160273	50.113997
447.730131	69.211740	50.119002
444.175794	63.978696	50.124007
440.338324	68.704673	50.129012
437.099648	67.870608	50.134017
433.464055	65.975233	50.139021
430.458598	69.651056	50.144026
426.913131	66.416073	50.149031
423.065381	71.978862	50.154036
419.370223	75.926571	50.159041
415.979260	67.067839	50.164045
412.636424	66.860581	50.169050
409.283184	68.249434	50.174055
405.304287	72.478591	50.179060
402.063892	67.867376	50.184065
398.630897	64.016956	50.189069
395.121921	66.461410	50.194074
391.994195	58.852484	50.199079
387.926330	64.810200	50.204084
384.542961	61.391806	50.209089
380.744824	69.439845	50.214093
377.614431	61.613042	50.219098
374.323766	60.565623	50.224103
370.729377	79.708569	50.229108
367.197576	64.832328	50.234113
363.186832	71.784039	50.239117
359.948029	68.390596	50.244122
356.843093	66.131053	50.249127
353.082720	64.767631	50.254132
349.930610	67.991741	50.259137
345.902423	64.389010	50.264141
342.423178	65.503266	50.269146
338.947201	67.502840	50.274151
335.592304	73.874736	50.279156
331.926406	70.471861	50.284161
328.095586	70.163420	50.289165
324.478932	69.214213	50.294170
321.474941	68.372100	50.299175
317.867242	76.801776	50.304180
314.614552	70.278470	50.309185
311.205275	72.932034	50.314189
307.488119	72.308516	50.319194
304.220644	63.943099	50.324199
300.217426	75.382887	50.329204
297.011494	69.500858	50.334209
293.501002	65.539136	50.339213
289.866033	68.813117	50.344218
286.968651	63.756227	50.349223
283.100373	71.679157	50.354228
279.445765	67.414016	50.359233
275.844629	62.555274	50.364237
272.328037	68.553726	50.369242
268.933608	66.377228	50.374247
265.234572	75.115348	50.379252
262.004303	69.926792	50.384257
258.205121	74.102679	50.389261
254.904114	66.229695	50.394266
251.560367	71.859564	50.399271
248.185555	68.291166	50.404276
244.519748	59.845413	50.409281
240.968200	60.085112	50.414285
237.446724	57.374760	50.419290
234.153843	66.135063	50.424295
230.158523	65.732029	50.429300
226.878623	64.866447	50.434305
223.366246	65.492344	50.439309
219.609713	64.394094	50.444314
216.350491	65.644949	50.449319
212.861677	63.714103	50.454324
209.820231	67.654968	50.459329
206.209001	63.474835	50.464333
202.265290	63.747122	50.469338
198.932747	67.011993	50.474343
195.148374	68.490139	50.479348
191.816118	60.701127	50.484353
188.545197	69.125831	50.489357
184.952891	64.566279	50.494362
181.706588	66.666152	50.499367
177.975430	73.479444	50.504372
174.344456	61.291995	50.509377
170.828536	68.761454	50.514381
167.270883	73.399606	50.519386
163.929928	64.026957	50.524391
160.058075	73.060900	50.529396
156.862252	63.599221	50.534401
153.338621	62.037627	50.539405
149.795461	63.636407	50.544410
146.517965	63.469632	50.549415
143.096405	67.852486	50.554420
139.290434	59.172322	50.559425
135.606052	61.552370	50.564429
132.276260	62.681349	50.569434
129.068157	55.543719	50.574439
124.975695	68.509639	50.579444
121.777540	68.305204	50.584449
118.586850	71.070287	50.589453
114.849289	66.966784	50.594458
111.546859	69.401261	50.599463
107.806478	71.638177	50.604468
104.505587	66.517591	50.609473
100.816869	66.889395	50.614477
97.089247	63.961231	50.619482
93.956684	57.833709	50.624487
89.821888	59.844140	50.629492
86.671022	61.834255	50.634497
83.172276	68.367767	50.639501
79.998825	73.300441	50.644506
76.364505	57.342458	50.649511
72.763006	65.480124	50.654516
69.248343	64.053184	50.659521
65.965400	69.585019	50.664525
62.060981	65.795398	50.669530
58.891594	62.438653	50.674535
54.929871	70.236950	50.679540
51.748417	66.170260	50.684545
48.467736	59.844350	50.689549
44.769070	64.039411	50.694554
41.380040	60.546028	50.699559
37.454485	73.666298	50.704564
34.139781	65.150106	50.709569
30.815563	66.347830	50.714573
27.485368	58.400350	50.719578
24.092730	57.160057	50.724583
20.180931	62.758168	50.729588
16.698628	55.748671	50.734593
13.239965	60.940883	50.739597
9.855299	64.615674	50.744602
6.246003	55.262699	50.749607
2.189985	61.614070	50.754612