Fri Aug 26 14:05:06 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.660730	99.229227	0.000000
0.733447	109.885751	0.005005
0.283399	96.396343	0.010010
0.371557	101.877873	0.015014
0.190575	95.914054	0.020019
0.547673	92.678952	0.025024
-0.099986	100.356736	0.030029
0.144929	91.827314	0.035034
-0.013763	84.129505	0.040038
-0.622702	75.429322	0.045043
-0.691257	67.844033	0.050048
-0.863517	52.365759	0.055053
-1.332333	42.141041	0.060058
-1.729671	45.353879	0.065062
-1.929754	41.389316	0.070067
-2.147794	32.637784	0.075072
-2.508891	25.284716	0.080077
-2.829665	23.192846	0.085082
-3.025508	16.108272	0.090086
-3.690189	10.080592	0.095091
-3.448956	12.118361	0.100096
-3.964779	10.015734	0.105101
-4.212131	7.833344	0.110106
-4.593410	2.720125	0.115110
-4.964413	-1.094434	0.120115
-4.812696	-0.194296	0.125120
-5.078720	4.548275	0.130125
-5.266726	-2.354020	0.135130
-5.529582	-1.588643	0.140134
-5.719039	1.269129	0.145139
-6.466047	2.242761	0.150144
-7.210342	9.366095	0.155149
-6.917445	10.038616	0.160154
-6.760512	5.430037	0.165158
-7.512358	5.806493	0.170163
-6.977237	-1.743048	0.175168
-7.796955	-1.441443	0.180173
-8.492120	-3.664835	0.185178
-8.582668	4.036894	0.190182
-8.743744	6.478974	0.195187
-8.573928	3.734940	0.200192
-8.758315	5.456175	0.205197
-9.443438	2.222015	0.210202
-9.623794	0.165231	0.215206
-10.141263	3.529639	0.220211
-9.941413	6.912072	0.225216
-10.263775	6.737621	0.230221
-10.437496	4.907586	0.235226
-10.979571	4.362397	0.240230
-11.702491	4.759659	0.245235
-11.487967	4.068196	0.250240
-12.095348	10.961414	0.255245
-12.174310	4.706504	0.260250
-11.955434	4.950803	0.265254
-12.194091	10.676171	0.270259
-12.151882	6.933311	0.275264
-12.979956	14.566384	0.280269
-13.230468	-3.765919	0.285274
-13.414198	4.788684	0.290278
-13.707008	5.716907	0.295283
-13.643171	0.274967	0.300288
-13.867444	7.870973	0.305293
-14.035486	-4.665717	0.310298
-14.483165	-4.399891	0.315302
-14.591645	3.396374	0.320307
-14.990778	-7.740802	0.325312
-15.792661	4.301471	0.330317
-16.144082	-0.500031	0.335322
-16.074740	1.469591	0.340326
-16.411363	5.843516	0.345331
-16.044663	-2.948422	0.350336
-16.231798	2.139357	0.355341
-16.017044	-2.234622	0.360346
-16.597729	-6.930825	0.365350
-17.333363	3.512983	0.370355
-17.826758	3.112070	0.375360
-18.488543	2.965157	0.380365
-18.910429	-1.635553	0.385370
-18.707364	-0.417554	0.390374
-18.402709	4.122271	0.395379
-18.544636	-3.442071	0.400384
-19.016265	4.043754	0.405389
-19.127498	6.854547	0.410394
-19.634448	-2.627077	0.415398
-20.239893	4.300636	0.420403
-20.475426	6.156381	0.425408
-20.911540	-2.969289	0.430413
-20.530338	0.562070	0.435418
-20.475265	2.790168	0.440422
-20.684955	-5.054679	0.445427
-21.381652	1.235531	0.450432
-22.038549	7.829583	0.455437
-21.766731	7.986547	0.460442
-22.147594	-0.246087	0.465446
-22.230787	6.040348	0.470451
-22.487970	-0.854340	0.475456
-22.980310	8.444316	0.480461
-23.214179	-0.946954	0.485466
-23.500513	2.267575	0.490470
-23.826870	1.131999	0.495475
-23.462060	-9.905828	0.500480
-24.119489	5.692032	0.505485
-24.275659	-0.152235	0.510490
-24.887879	0.863683	0.515494
-25.430334	5.013401	0.520499
-25.146581	-6.283880	0.525504
-25.196929	1.788061	0.530509
-25.439308	-1.075285	0.535514
-25.821013	-4.609776	0.540518
-26.366005	5.263367	0.545523
-26.212015	1.582195	0.550528
-26.286662	-6.865786	0.555533
-26.666427	2.431156	0.560538
-27.251865	-1.691688	0.565542
-27.811368	8.294443	0.570547
-27.784298	-4.592151	0.575552
-28.037184	0.714665	0.580557
-27.650935	0.119847	0.585562
-27.989845	2.254269	0.590566
-28.983734	4.069905	0.595571
-29.028444	-5.556449	0.600576
-29.468047	1.117659	0.605581
-29.274144	6.927531	0.610586
-29.304595	-9.154875	0.615590
-30.150357	2.941681	0.620595
-30.486820	-6.019173	0.625600
-30.710530	5.414240	0.630605
-31.046795	9.338874	0.635610
-31.056214	-2.754293	0.640614
-31.208366	-5.055904	0.645619
-30.597358	1.065498	0.650624
-31.209027	6.374395	0.655629
-32.092335	-3.023319	0.660634
-32.274381	-1.229686	0.665638
-32.412710	0.740632	0.670643
-32.326409	4.121761	0.675648
-33.316602	6.088678	0.680653
-33.316375	4.048069	0.685658
-33.560966	5.202894	0.690662
-33.644365	6.981169	0.695667
-33.694527	2.262472	0.700672
-34.019265	4.562360	0.705677
-34.497095	13.602503	0.710682
-34.895101	4.151370	0.715686
-35.180085	5.771213	0.720691
-35.538430	-4.176456	0.725696
-35.508830	14.718520	0.730701
-35.518165	8.240805	0.735706
-35.439425	7.893176	0.740710
-36.091292	0.025429	0.745715
-36.459093	-0.429838	0.750720
-36.738942	6.561071	0.755725
-37.094271	12.007223	0.760730
-37.079390	0.365836	0.765734
-37.172714	3.363659	0.770739
-37.660898	8.280020	0.775744
-38.406883	4.672537	0.780749
-38.622024	-1.225820	0.785754
-38.515348	-2.400346	0.790758
-39.005028	-1.982454	0.795763
-38.693053	8.415299	0.800768
-38.587553	7.237792	0.805773
-39.229457	-0.400559	0.810778
-39.651832	9.776186	0.815782
-39.888643	7.165063	0.820787
-39.656757	-0.039881	0.825792
-40.369450	2.823431	0.830797
-41.128293	1.394537	0.835802
-41.186486	0.318445	0.840806
-41.192901	7.064308	0.845811
-41.153879	-12.164082	0.850816
-41.207876	2.571055	0.855821
-42.105677	-6.020835	0.860826
-42.261977	-5.151830	0.865830
-42.851008	-0.706970	0.870835
-42.919828	-3.018392	0.875840
-42.785142	-1.745456	0.880845
-42.695613	-4.613024	0.885850
-43.083980	-6.321055	0.890854
-44.186556	-1.802564	0.895859
-44.275626	0.618812	0.900864
-44.443923	1.284049	0.905869
-44.467811	-2.002444	0.910874
-44.418324	-0.823806	0.915878
-45.061354	7.536562	0.920883
-44.847019	-0.133868	0.925888
-45.307821	0.605384	0.930893
-45.671865	1.880044	0.935898
-45.708142	-3.185650	0.940902
-46.731811	0.115208	0.945907
-46.974471	-9.625850	0.950912
-47.102380	4.507049	0.955917
-47.307807	-2.595004	0.960922
-46.932811	-6.462439	0.965926
-47.258395	-6.924279	0.970931
-47.199532	-3.722371	0.975936
-47.893593	4.554196	0.980941
-48.865682	4.528362	0.985946
-48.826185	0.624581	0.990950
-49.021410	-0.534576	0.995955
-48.935481	12.359688	1.000960
-48.905710	1.990932	1.005965
-49.101948	2.002481	1.010970
-49.361300	-9.903073	1.015974
-50.099646	1.502901	1.020979
-50.200789	-0.196069	1.025984
-50.753745	0.468949	1.030989
-50.892205	-3.055959	1.035994
-50.378171	0.056098	1.040998
-51.111801	1.824885	1.046003
-51.773439	-3.099149	1.051008
-51.900777	3.687685	1.056013
-52.256280	-4.384384	1.061018
-51.907945	-9.778870	1.066022
-52.220753	7.274388	1.071027
-52.433775	-5.615948	1.076032
-52.726447	-7.414805	1.081037
-53.039244	0.625233	1.086042
-52.835388	-5.594614	1.091046
-54.028654	3.079205	1.096051
-54.409355	-5.561559	1.101056
-54.597733	-1.125299	1.106061
-54.689434	0.141758	1.111066
-54.386949	-4.157298	1.116070
-54.485702	-0.994122	1.121075
-55.014948	-4.246220	1.126080
-55.582870	-1.035304	1.131085
-55.967023	-1.481697	1.136090
-56.206233	-9.318779	1.141094
-56.157686	-1.341331	1.146099
-55.870019	4.501395	1.151104
-56.627410	-0.781041	1.156109
-57.162792	7.606858	1.161114
-57.256611	-8.304334	1.166118
-57.669247	-4.247594	1.171123
-57.704544	-7.415254	1.176128
-57.907010	-7.352117	1.181133
-58.459684	-2.707282	1.186138
-58.607648	-8.416786	1.191142
-59.316472	3.554048	1.196147
-59.449301	-3.938944	1.201152
-59.101545	-2.205656	1.206157
-59.212318	-1.340576	1.211162
-59.172404	4.199052	1.216166
-59.950913	-5.724322	1.221171
-60.227552	-3.371815	1.226176
-60.465355	0.123049	1.231181
-60.835101	0.651977	1.236186
-60.994691	-2.575422	1.241190
-61.270766	1.649874	1.246195
-61.852857	-3.814873	1.251200
-62.071226	-3.632205	1.256205
-62.243768	-0.229758	1.261210
-62.096714	-5.086722	1.266214
-62.476335	1.492627	1.271219
-61.964905	-1.171722	1.276224
-62.813511	3.193336	1.281229
-63.287317	4.326905	1.286234
-63.309334	2.014523	1.291238
-63.600208	-3.989095	1.296243
-64.178793	0.681921	1.301248
-64.712723	5.137185	1.306253
-65.098155	2.574513	1.311258
-64.698938	-2.046477	1.316262
-65.183422	-5.033471	1.321267
-65.134312	-5.468232	1.326272
-65.033264	-6.553300	1.331277
-65.368792	0.300748	1.336282
-66.062426	-9.920565	1.341286
-66.438345	-0.450226	1.346291
-66.335341	2.475901	1.351296
-66.473919	-1.219826	1.356301
-67.321117	1.870065	1.361306
-67.546395	-8.531736	1.366310
-67.773188	-2.839857	1.371315
-68.608084	-11.922409	1.376320
-68.152324	-1.578689	1.381325
-68.250139	-3.917232	1.386330
-68.101660	-3.709427	1.391334
-68.549060	-5.250084	1.396339
-68.459044	-9.329401	1.401344
-69.343690	-2.858076	1.406349
-69.704174	2.310473	1.411354
-69.589344	-9.210429	1.416358
-69.553079	5.121525	1.421363
-70.328870	4.410254	1.426368
-70.677310	1.341968	1.431373
-70.849350	0.758148	1.436378
-71.042552	1.810063	1.441382
-71.177257	9.436411	1.446387
-71.266771	-0.078567	1.451392
-72.038841	3.774719	1.456397
-72.546483	5.593739	1.461402
-72.903286	-6.008751	1.466406
-73.043532	0.065108	1.471411
-72.501045	7.829617	1.476416
-72.700791	3.554976	1.481421
-72.746635	-0.569626	1.486426
-72.927504	-1.265962	1.491430
-74.027209	12.844250	1.496435
-73.964458	3.539672	1.501440
-74.117347	9.419356	1.506445
-74.089473	6.479132	1.511450
-75.083020	1.878849	1.516454
-75.522634	4.073242	1.521459
-75.899467	-3.008448	1.526464
-75.861081	3.009126	1.531469
-75.869230	6.585287	1.536474
-75.783025	2.196524	1.541478
-75.724230	4.658151	1.546483
-75.903333	11.785229	1.551488
-76.740629	7.144799	1.556493
-77.178286	13.571843	1.561498
-76.963535	0.716137	1.566502
-77.570290	9.981986	1.571507
-78.456817	10.664142	1.576512
-78.469459	5.667531	1.581517
-78.924894	7.826423	1.586522
-78.134985	7.469301	1.591526
-78.407466	10.124872	1.596531
-78.402243	1.518927	1.601536
-78.842214	13.223287	1.606541
-80.088310	9.029308	1.611546
-80.047803	2.664055	1.616550
-80.395085	6.096874	1.621555
-79.812379	11.757626	1.626560
-80.245043	7.569869	1.631565
-80.954704	7.667685	1.636570
-81.323593	3.564908	1.641574
-81.921558	3.844643	1.646579
-81.928272	5.193377	1.651584
-81.487340	3.372042	1.656589
-81.651973	6.624568	1.661594
-81.618051	3.151910	1.666598
-82.640362	1.336949	1.671603
-82.911318	-2.043947	1.676608
-83.252470	-2.082598	1.681613
-83.358105	5.238675	1.686618
-83.227483	0.662669	1.691622
-83.532723	6.534437	1.696627
-84.362745	7.543142	1.701632
-84.499659	5.043013	1.706637
-84.719046	11.809380	1.711642
-84.612975	7.082177	1.716646
-85.004974	2.530597	1.721651
-85.291406	4.198120	1.726656
-85.307826	11.255577	1.731661
-86.003730	9.146193	1.736666
-86.039115	4.880761	1.741670
-86.261212	9.575364	1.746675
-86.377283	2.652381	1.751680
-86.779830	6.356387	1.756685
-87.558125	10.792754	1.761690
-87.687821	4.352765	1.766694
-87.877766	5.135264	1.771699
-87.728972	-1.528411	1.776704
-87.531852	3.081936	1.781709
-87.738380	4.480762	1.786714
-88.421430	6.017057	1.791718
-88.984824	3.795295	1.796723
-89.024943	4.503847	1.801728
-88.894398	7.783177	1.806733
-89.533697	7.908002	1.811738
-90.172827	4.916613	1.816742
-90.628106	1.251216	1.821747
-90.974745	-0.419020	1.826752
-90.377148	3.018534	1.831757
-90.522811	4.107338	1.836762
-90.485323	-0.077693	1.841766
-91.625153	1.548704	1.846771
-92.186047	3.126088	1.851776
-91.995021	-3.211979	1.856781
-91.970149	5.629667	1.861786
-91.987072	-0.438751	1.866790
-92.290674	3.683268	1.871795
-92.688675	-1.038213	1.876800
-92.958866	-10.202360	1.881805
-93.656529	-2.529493	1.886810
-93.429226	-13.330775	1.891814
-93.616709	-5.898690	1.896819
-93.976667	-10.040818	1.901824
-94.461344	-8.424684	1.906829
-94.795294	-8.907366	1.911834
-95.167812	-12.981101	1.916838
-94.981580	-8.878408	1.921843
-94.995501	-8.746554	1.926848
-94.939117	-13.466016	1.931853
-96.119425	0.435280	1.936858
-96.287285	-10.389894	1.941862
-96.613054	0.395037	1.946867
-97.039048	-3.138882	1.951872
-96.781023	-8.370614	1.956877
-97.272010	-3.969494	1.961882
-96.692561	-2.389336	1.966886
-97.376629	-6.889109	1.971891
-97.810130	-9.966294	1.976896
-97.835674	-8.643102	1.981901
-98.140783	-2.986486	1.986906
-98.754669	-2.878272	1.991910
-99.205009	-7.385964	1.996915
-99.415417	-10.195624	2.006912
-99.032918	-7.391635	2.016909
-98.634651	2.039879	2.026906
-97.648856	-2.180974	2.036902
-97.059717	-8.291363	2.046899
-97.241144	-6.875713	2.056896
-96.461077	-5.701632	2.066893
-95.721377	-3.973255	2.076890
-95.517249	-3.108628	2.086886
-94.491534	-7.164640	2.096883
-94.469387	-3.604483	2.106880
-93.826506	-5.047728	2.116877
-92.825143	-0.046686	2.126874
-92.865383	-1.855555	2.136870
-92.697094	-9.493766	2.146867
-91.784061	-3.205561	2.156864
-92.020633	-7.502175	2.166861
-90.480507	-2.825764	2.176858
-90.338855	-2.854201	2.186854
-90.311681	-0.127929	2.196851
-89.699010	-2.871560	2.206848
-88.819074	-2.403584	2.216845
-87.787825	-0.302466	2.226842
-87.594873	-4.298505	2.236838
-87.636432	-4.330094	2.246835
-87.180741	-5.709349	2.256832
-86.512498	0.924239	2.266829
-85.319846	-8.001166	2.276826
-85.283003	-4.455968	2.286822
-84.893867	-7.364358	2.296819
-84.527501	-2.039540	2.306816
-83.644965	-8.439524	2.316813
-83.536333	-1.810669	2.326810
-82.924076	-8.399812	2.336806
-82.078707	-2.202436	2.346803
-82.046102	-3.902274	2.356800
-81.062741	-2.012270	2.366797
-80.364865	-0.141169	2.376794
-80.376545	-3.541498	2.386790
-80.070339	0.329214	2.396787
-79.418765	-4.035997	2.406784
-79.112186	-3.694153	2.416781
-78.100041	1.983098	2.426778
-77.668396	-5.721462	2.436774
-77.667827	-13.894239	2.446771
-76.591866	-9.322949	2.456768
-76.295063	-11.722802	2.466765
-75.982599	-3.627366	2.476762
-75.322728	-5.690956	2.486758
-74.751979	-8.548431	2.496755
-74.327890	-8.630347	2.506752
-73.434242	-7.568980	2.516749
-73.234504	-3.665853	2.526746
-73.125749	-4.775687	2.536742
-72.358001	-2.782422	2.546739
-72.047876	1.423456	2.556736
-70.985514	1.948556	2.566733
-70.282458	-11.398741	2.576730
-70.182809	-2.655636	2.586726
-70.132903	-8.720080	2.596723
-69.756326	-5.319641	2.606720
-68.742358	-5.762655	2.616717
-67.784944	-2.661719	2.626714
-67.795903	-3.217574	2.636710
-67.450773	0.685091	2.646707
-67.338694	0.439520	2.656704
-66.499075	0.048993	2.666701
-65.693390	-3.659159	2.676698
-64.949952	4.125267	2.686694
-64.595555	7.088853	2.696691
-64.456122	1.244875	2.706688
-63.670560	-2.729398	2.716685
-63.697718	3.166693	2.726682
-62.621275	6.930152	2.736678
-61.843950	1.433499	2.746675
-61.806639	-4.312216	2.756672
-61.755688	2.550530	2.766669
-60.908007	-2.979250	2.776666
-59.813289	-8.499976	2.786662
-59.724294	-3.527932	2.796659
-59.023027	-2.278226	2.806656
-58.994083	0.134171	2.816653
-58.077940	2.455946	2.826650
-57.499393	0.186447	2.836646
-57.219539	-3.636231	2.846643
-57.123635	-0.043208	2.856640
-56.498101	-1.924061	2.866637
-55.754174	-1.048449	2.876634
-54.943928	1.866334	2.886630
-54.610644	-6.519804	2.896627
-54.751515	-1.372591	2.906624
-53.639482	1.222783	2.916621
-53.286253	2.488667	2.926618
-52.995749	8.902317	2.936614
-51.958216	3.967011	2.946611
-51.909618	0.528786	2.956608
-51.265316	1.891896	2.966605
-50.253440	5.830129	2.976602
-50.074988	4.744287	2.986598
-50.397548	-1.601110	2.996595
-49.345566	5.127951	3.006592
-48.697094	6.103954	3.016589
-47.828109	10.409715	3.026586
-47.354521	4.950850	3.036582
-47.238227	7.878652	3.046579
-47.153534	-2.337724	3.056576
-46.317786	4.976184	3.066573
-45.950553	1.637228	3.076570
-44.862536	4.543609	3.086566
-44.422056	3.122375	3.096563
-44.418595	-2.899996	3.106560
-43.814609	-3.849360	3.116557
-43.001757	2.318239	3.126554
-43.071310	-2.007551	3.136550
-41.974052	0.463417	3.146547
-41.490375	0.806197	3.156544
-41.531654	3.197851	3.166541
-41.079961	-0.258788	3.176538
-40.085168	4.065396	3.186534
-39.815060	0.912618	3.196531
-39.068204	-6.087111	3.206528
-38.911499	-3.118087	3.216525
-38.050623	3.555203	3.226522
-37.332901	-4.998496	3.236518
-37.277865	-3.290222	3.246515
-36.897129	-1.429927	3.256512
-35.916349	-10.426878	3.266509
-35.673432	-4.439796	3.276506
-35.464789	0.605484	3.286502
-34.742074	-5.902661	3.296499
-34.160248	-4.080011	3.306496
-33.864583	-1.281504	3.316493
-32.991788	-4.246194	3.326490
-33.013716	-1.312710	3.336486
-32.215630	-1.551055	3.346483
-31.530172	-1.939751	3.356480
-31.278412	-8.051464	3.366477
-30.493101	5.906616	3.376474
-29.728551	1.340086	3.386470
-29.979380	0.096177	3.396467
-29.441819	7.047883	3.406464
-28.681356	-0.489308	3.416461
-28.353618	0.378249	3.426458
-27.291220	-3.616954	3.436454
-27.035776	-2.931371	3.446451
-26.476551	-7.763692	3.456448
-26.602591	-0.575625	3.466445
-25.690778	1.493411	3.476442
-25.277627	-4.377346	3.486438
-24.469479	-6.445016	3.496435
-24.170235	-10.774374	3.506432
-23.682765	0.303128	3.516429
-23.135187	-9.098362	3.526426
-22.776601	-2.131464	3.536422
-22.330933	-0.743762	3.546419
-21.353690	-3.376268	3.556416
-21.153634	-1.500511	3.566413
-21.108270	-1.029299	3.576410
-20.282513	-3.102879	3.586406
-19.324933	-4.997418	3.596403
-19.224325	-9.055106	3.606400
-18.503721	-1.355818	3.616397
-18.207910	0.771117	3.626394
-17.777642	-2.840572	3.636390
-17.149527	-6.407039	3.646387
-16.816553	-2.888939	3.656384
-15.829000	-3.993054	3.666381
-15.158945	-2.415381	3.676378
-14.855810	-0.555674	3.686374
-15.037592	0.128295	3.696371
-14.235686	-3.094611	3.706368
-13.619486	-5.331960	3.716365
-13.200437	0.646708	3.726362
-12.446704	-2.096712	3.736358
-11.821129	3.954336	3.746355
-11.638955	4.077974	3.756352
-11.459668	0.109401	3.766349
-10.356525	1.898400	3.776346
-9.824845	-2.229574	3.786342
-9.716003	-0.868620	3.796339
-9.011510	0.732200	3.806336
-8.665941	-2.679407	3.816333
-8.497965	-3.326475	3.826330
-7.906332	-1.651065	3.836326
-7.477383	-3.434788	3.846323
-6.491226	-5.941974	3.856320
-6.154661	-2.918592	3.866317
-5.721976	10.999368	3.876314
-5.480292	11.807466	3.886310
-4.848667	9.022870	3.896307
-4.212260	15.981365	3.906304
-3.936519	25.900797	3.916301
-3.423015	39.929737	3.926298
-2.597139	50.853218	3.936294
-2.446920	55.058668	3.946291
-2.254230	65.485215	3.956288
-1.699478	86.688961	3.966285
-1.074502	93.794981	3.976282
-0.856935	104.236684	3.986278
0.000000	119.646286	3.991283
-0.066597	128.283949	3.996288
-0.022787	132.269652	4.001293
0.434771	137.848699	4.006298
0.304237	153.317199	4.011302
1.142599	150.544980	4.016307
0.731201	146.730350	4.021312
0.498628	134.902779	4.026317
0.729051	132.434019	4.031322
0.403804	135.635649	4.036326
0.716317	142.518566	4.041331
0.848191	150.334420	4.046336
0.815466	154.426955	4.051341
0.837469	149.538798	4.056346
0.756182	142.993143	4.061350
0.514429	147.595935	4.066355
0.358073	155.364922	4.071360
0.631169	161.172008	4.076365
0.760454	154.884621	4.081370
0.624486	155.940288	4.086374
1.083849	161.553862	4.091379
1.126418	158.168409	4.096384
0.690676	159.767446	4.101389
0.778587	154.818407	4.106394
1.057961	149.570647	4.111398
0.906904	155.737992	4.116403
1.065014	157.358461	4.121408
0.582147	152.944369	4.126413
0.890769	153.899178	4.131418
0.357656	167.070271	4.136422
0.588806	160.577202	4.141427
0.930645	161.080761	4.146432
0.530842	162.572966	4.151437
0.777063	151.860378	4.156442
0.726424	162.428575	4.161446
1.182209	164.916999	4.166451
1.302174	165.701870	4.171456
1.453464	168.323123	4.176461
1.165599	146.889750	4.181466
0.748345	154.787941	4.186470
0.823057	153.956894	4.191475
0.979749	157.770008	4.196480
1.302358	168.242131	4.201485
1.326694	174.113262	4.206490
0.958343	158.975466	4.211494
0.774109	167.011383	4.216499
1.009353	170.755323	4.221504
1.120665	177.062155	4.226509
1.397915	181.419637	4.231514
1.439455	182.232538	4.236518
1.400386	167.090922	4.241523
1.708717	170.772864	4.246528
1.414671	166.841885	4.251533
1.311939	153.269883	4.256538
0.526071	156.710909	4.261542
0.863984	165.924670	4.266547
1.274196	170.008354	4.271552
1.456805	177.047549	4.276557
1.383754	170.741040	4.281562
1.334239	186.560777	4.286566
1.692373	182.971167	4.291571
1.554428	181.122888	4.296576
0.775925	173.689218	4.301581
1.270582	175.988098	4.306586
1.291718	184.403326	4.311590
1.318089	182.991360	4.316595
1.361989	181.013531	4.321600
1.044733	178.728111	4.326605
1.488012	176.665955	4.331610
1.393392	183.289582	4.336614
1.428540	187.675270	4.341619
1.415655	184.864744	4.346624
1.263403	186.138078	4.351629
1.272853	178.720926	4.356634
1.368220	184.783476	4.361638
1.343031	188.798917	4.366643
1.322055	186.103543	4.371648
1.230567	182.821213	4.376653
1.515471	186.437205	4.381658
1.594850	191.698673	4.386662
1.437287	193.096218	4.391667
1.952507	199.903305	4.396672
2.024400	202.141464	4.401677
1.768639	186.125594	4.406682
1.324233	188.981963	4.411686
1.548913	183.432668	4.416691
1.706329	193.940018	4.421696
1.378499	202.305186	4.426701
1.896086	196.450860	4.431706
1.461374	195.987022	4.436710
1.757639	206.232321	4.441715
1.929301	210.742289	4.446720
1.727514	194.967938	4.451725
1.865941	184.752993	4.456730
1.357806	199.378676	4.461734
1.905656	207.983983	4.466739
2.279263	212.228397	4.471744
1.856341	199.965358	4.476749
2.065990	195.557325	4.481754
1.866778	196.913899	4.486758
1.744500	200.580636	4.491763
1.360834	189.931297	4.496768
1.452754	194.105671	4.501773
1.731222	198.168746	4.506778
2.104615	210.553341	4.511782
1.792936	211.250400	4.516787
1.789006	221.381099	4.521792
1.770883	217.476749	4.526797
1.814953	221.800946	4.531802
1.681079	217.595086	4.536806
1.842717	214.089845	4.541811
1.926925	216.547547	4.546816
2.101320	216.877867	4.551821
2.002285	218.405503	4.556826
1.747328	212.779021	4.561830
1.951024	217.277675	4.566835
1.940374	217.067343	4.571840
1.807860	213.569937	4.576845
2.256186	215.771635	4.581850
1.990518	213.569924	4.586854
1.939223	212.166885	4.591859
2.229009	215.877034	4.596864
2.064079	217.009978	4.601869
2.277681	214.338186	4.606874
2.364505	211.135653	4.611878
2.183141	216.001138	4.616883
2.393901	205.945757	4.621888
1.842093	213.649793	4.626893
2.160738	203.988894	4.631898
2.345859	209.860312	4.636902
2.081728	208.654923	4.641907
1.927759	213.361121	4.646912
1.949657	214.468140	4.651917
1.966780	214.199701	4.656922
2.275911	216.068739	4.661926
2.392281	227.901755	4.666931
2.049545	219.799118	4.671936
1.977035	233.404735	4.676941
2.284922	232.192538	4.681946
2.371773	247.146393	4.686950
2.370210	233.903421	4.691955
2.666270	238.564866	4.696960
2.342998	244.021916	4.701965
2.657387	234.304717	4.706970
2.089477	223.010179	4.711974
1.742567	226.471456	4.716979
2.113519	235.809821	4.721984
2.137582	238.371800	4.726989
2.495343	237.458715	4.731994
2.406292	241.085487	4.736998
2.530717	242.806119	4.742003
2.700133	243.883844	4.747008
2.521391	244.145763	4.752013
2.665478	240.608450	4.757018
2.290672	239.015338	4.762022
2.648119	236.590060	4.767027
2.593653	235.317224	4.772032
2.500324	242.143149	4.777037
2.764849	237.460811	4.782042
2.538253	234.025505	4.787046
2.389289	237.503420	4.792051
2.637069	238.461379	4.797056
2.589995	236.972261	4.802061
2.856340	235.291979	4.807066
2.748372	239.045079	4.812070
3.047290	238.846658	4.817075
2.924035	239.966788	4.822080
2.927928	240.235072	4.827085
2.738999	227.236408	4.832090
2.355578	237.517949	4.837094
2.841008	239.210846	4.842099
3.067627	238.786405	4.847104
2.468314	238.664562	4.852109
2.507061	232.638012	4.857114
2.768516	237.311172	4.862118
2.577779	245.923929	4.867123
2.686505	234.267774	4.872128
2.732987	243.621861	4.877133
2.862448	233.772108	4.882138
2.569340	236.532163	4.887142
2.473892	237.527743	4.892147
2.742902	244.227652	4.897152
2.593637	238.451831	4.902157
2.550763	226.635791	4.907162
2.609936	242.315271	4.912166
2.406037	238.047544	4.917171
2.790286	244.362523	4.922176
2.746637	258.947573	4.927181
3.046304	260.463755	4.932186
2.809438	271.355236	4.937190
3.337276	266.432581	4.942195
3.090944	262.832666	4.947200
3.025506	260.365662	4.952205
3.499143	256.941547	4.957210
3.054647	245.830255	4.962214
2.933664	247.547968	4.967219
2.981108	233.769030	4.972224
3.010791	247.586532	4.977229
2.977811	248.116816	4.982234
3.004113	258.840766	4.987238
2.973439	253.688705	4.992243
3.107626	267.594354	4.997248
3.532167	272.166203	5.002253
3.470933	253.579539	5.007258
2.920675	250.251569	5.012262
2.595781	247.597178	5.017267
2.933397	263.625621	5.022272
3.161076	278.434192	5.027277
3.205587	268.164220	5.032282
3.501658	281.162005	5.037286
3.365930	273.163151	5.042291
3.642293	271.158610	5.047296
2.819413	269.122741	5.052301
3.226064	268.983475	5.057306
3.095445	269.620708	5.062310
3.123581	275.390043	5.067315
3.241047	268.965253	5.072320
3.053151	280.035772	5.077325
3.268249	273.089589	5.082330
3.240273	278.823370	5.087334
3.336761	286.072165	5.092339
3.369828	277.268760	5.097344
3.287917	273.254109	5.102349
3.050902	270.946692	5.107354
3.392342	266.258699	5.112358
3.152480	271.785027	5.117363
3.276927	271.107579	5.122368
3.407384	277.477903	5.127373
3.671095	262.643397	5.132378
3.444140	269.778033	5.137382
3.387544	274.263446	5.142387
3.483162	267.187175	5.147392
3.569420	276.902075	5.152397
3.517686	274.663885	5.157402
3.419095	264.159936	5.162406
3.241354	268.847704	5.167411
3.484145	270.787186	5.172416
3.001725	272.108769	5.177421
3.539747	282.167777	5.182426
3.724700	292.449439	5.187430
3.841225	290.049010	5.192435
3.601416	275.757953	5.197440
3.448858	280.210853	5.202445
3.695779	283.101966	5.207450
3.858416	277.600266	5.212454
3.758045	275.157681	5.217459
3.644687	272.764573	5.222464
3.515545	275.160590	5.227469
3.721504	258.642503	5.232474
3.308092	273.199716	5.237478
3.808770	284.893842	5.242483
3.686133	292.274832	5.247488
3.857872	286.350941	5.252493
3.898546	283.114453	5.257498
4.055118	289.101072	5.262502
3.291427	274.730234	5.267507
3.925935	278.851786	5.272512
3.720730	285.976715	5.277517
4.093798	279.521616	5.282522
3.656670	290.093118	5.287526
3.699290	291.532268	5.292531
3.943376	293.882832	5.297536
4.013396	302.008935	5.302541
4.056707	298.639157	5.307546
4.038984	285.151894	5.312550
3.741940	271.356961	5.317555
3.673563	271.339111	5.322560
3.585962	284.918644	5.327565
3.891320	285.554435	5.332570
4.080570	288.315325	5.337574
3.829083	293.308805	5.342579
4.177025	289.331625	5.347584
3.925286	289.690330	5.352589
4.219520	287.509001	5.357594
3.817493	295.790853	5.362598
4.176644	294.890204	5.367603
4.474925	289.114286	5.372608
4.112007	286.661958	5.377613
3.902804	279.930528	5.382618
3.703505	281.027700	5.387622
3.773584	294.392868	5.392627
4.072562	282.080648	5.397632
3.881497	293.490185	5.402637
4.061334	287.653616	5.407642
3.953556	288.239838	5.412646
4.026385	292.891763	5.417651
4.202377	292.816883	5.422656
3.836309	280.383588	5.427661
4.224858	283.246322	5.432666
4.190823	293.812012	5.437670
4.168384	293.613006	5.442675
4.253646	285.396245	5.447680
4.172257	290.407532	5.452685
3.715979	291.503587	5.457690
3.988253	293.606157	5.462694
4.326563	299.039310	5.467699
4.684102	305.007299	5.472704
4.316163	298.455598	5.477709
4.090264	292.337357	5.482714
4.077688	302.406175	5.487718
4.580079	313.033887	5.492723
4.402216	314.535840	5.497728
4.353155	313.164082	5.502733
4.354696	314.707704	5.507738
4.656212	315.318786	5.512742
4.414064	301.847470	5.517747
4.374627	282.941012	5.522752
4.251486	304.185399	5.527757
4.468751	304.689377	5.532762
4.774812	307.564958	5.537766
4.249712	293.976355	5.542771
4.340013	297.961184	5.547776
4.294299	312.391578	5.552781
4.194157	311.416909	5.557786
4.424882	311.782752	5.562790
4.413948	308.712479	5.567795
4.454118	316.552176	5.572800
4.641777	319.923913	5.577805
4.799297	310.303862	5.582810
4.737273	316.004991	5.587814
4.803182	308.572667	5.592819
4.789196	307.321996	5.597824
4.433758	310.262607	5.602829
4.505959	313.171436	5.607834
4.572515	313.015520	5.612838
4.558947	316.497679	5.617843
4.883344	312.910132	5.622848
4.353319	318.595544	5.627853
4.684927	311.726117	5.632858
4.620585	311.992371	5.637862
4.464546	308.194894	5.642867
4.833855	309.475615	5.647872
4.186951	308.329815	5.652877
4.655674	307.668365	5.657882
4.381386	317.986744	5.662886
4.461086	308.897657	5.667891
4.846501	298.533461	5.672896
4.871165	319.175896	5.677901
4.693435	311.196220	5.682906
4.668591	330.375257	5.687910
4.724697	332.267883	5.692915
4.943616	330.107766	5.697920
4.443849	332.909503	5.702925
4.612167	339.400503	5.707930
4.890014	333.789101	5.712934
5.026508	330.227642	5.717939
5.212818	332.229708	5.722944
4.995409	345.120828	5.727949
5.109280	328.746726	5.732954
5.146670	334.862647	5.737958
4.669517	335.712022	5.742963
4.988555	331.701369	5.747968
4.741384	332.132128	5.752973
4.837734	329.162205	5.757978
5.124793	333.622600	5.762982
4.920622	332.891913	5.767987
4.949054	329.287169	5.772992
5.140338	340.621386	5.777997
4.780180	332.217695	5.783002
4.918570	329.579742	5.788006
4.871726	336.414284	5.793011
5.340385	333.955859	5.798016
5.113420	330.394043	5.803021
5.047581	324.443856	5.808026
5.233801	337.550532	5.813030
4.996045	336.075276	5.818035
5.231486	328.939246	5.823040
5.026867	334.460106	5.828045
5.374174	338.398602	5.833050
5.079153	332.550532	5.838054
4.695390	330.867059	5.843059
5.046975	330.318758	5.848064
4.907791	345.513529	5.853069
5.138946	346.733507	5.858074
5.152517	351.211178	5.863078
5.628353	356.467914	5.868083
5.600873	358.639309	5.873088
5.193388	351.049722	5.878093
5.393295	347.709338	5.883098
5.519445	340.201183	5.888102
5.239535	338.194660	5.893107
5.251213	337.031739	5.898112
5.191621	344.510501	5.903117
5.306647	345.966855	5.908122
5.481095	353.266814	5.913126
5.209833	359.459272	5.918131
5.072089	355.060995	5.923136
5.101142	357.498831	5.928141
5.085521	361.873483	5.933146
5.453208	359.117569	5.938150
5.399974	358.806300	5.943155
5.518095	353.643697	5.948160
5.407774	365.527919	5.953165
5.419309	363.153318	5.958170
5.730070	358.131561	5.963174
5.415366	366.368213	5.968179
5.560843	360.052923	5.973184
5.373513	368.060940	5.978189
5.306009	365.866321	5.983194
5.597002	360.531270	5.988198
5.401471	363.301462	5.993203
5.298691	359.676013	5.998208
5.465018	366.936113	6.003213
5.415393	374.403844	6.008218
5.852568	379.214196	6.013222
5.698496	381.335702	6.018227
5.799224	369.611102	6.023232
5.655189	363.011862	6.028237
5.696067	361.724172	6.033242
5.736903	357.092450	6.038246
5.517874	359.296832	6.043251
5.422257	356.556106	6.048256
5.424137	356.350149	6.053261
5.699638	359.075475	6.058266
5.817106	359.933509	6.063270
5.438730	366.326142	6.068275
5.285736	368.861925	6.073280
5.466475	371.934196	6.078285
5.641630	385.321038	6.083290
5.540243	371.195011	6.088294
5.596130	381.237395	6.093299
5.717336	382.116994	6.098304
5.408127	381.076797	6.103309
5.824962	378.363847	6.108314
5.907581	378.648349	6.113318
5.715811	375.609384	6.118323
5.509187	362.214748	6.123328
5.648872	367.270729	6.128333
5.470119	361.765210	6.133338
5.755405	364.846513	6.138342
5.629581	365.315326	6.143347
5.696155	361.698310	6.148352
5.772602	365.112680	6.153357
5.313107	364.706479	6.158362
5.560678	368.018277	6.163366
5.107141	364.051975	6.168371
5.639149	364.086177	6.173376
5.244564	362.619518	6.178381
5.210676	375.247972	6.183386
5.530529	382.034928	6.188390
5.824310	386.120972	6.193395
6.095898	385.104240	6.198400
5.233313	375.260172	6.203405
5.852306	375.717423	6.208410
5.666418	367.770629	6.213414
5.427593	368.003940	6.218419
5.373858	358.198459	6.223424
5.403703	377.261465	6.228429
5.682496	386.256758	6.233434
5.624001	388.113451	6.238438
5.134886	395.102295	6.243443
6.012433	384.702555	6.248448
5.652894	383.413933	6.253453
5.419094	383.023210	6.258458
5.848235	383.763117	6.263462
5.733513	382.382595	6.268467
6.103989	375.978485	6.273472
5.689594	363.568474	6.278477
5.412528	370.657169	6.283482
5.451480	361.438361	6.288486
5.459540	356.371986	6.293491
5.497668	360.798381	6.298496
5.514518	367.287664	6.303501
5.470599	376.627423	6.308506
5.962689	370.160088	6.313510
5.432274	367.407965	6.318515
5.343242	369.494033	6.323520
5.937115	368.771967	6.328525
5.896743	372.944836	6.333530
5.761538	365.825371	6.338534
5.297587	372.617302	6.343539
5.551296	364.295186	6.348544
5.712522	365.260301	6.353549
5.455081	369.732717	6.358554
5.547098	371.145200	6.363558
5.709703	369.996742	6.368563
5.482399	359.829148	6.373568
5.567465	356.718611	6.378573
5.679251	356.299392	6.383578
5.706453	364.796017	6.388582
5.337604	373.129686	6.393587
5.605777	366.728852	6.398592
5.367579	362.494909	6.403597
5.189127	368.815287	6.408602
5.498453	375.660827	6.413606
5.328326	392.537223	6.418611
5.649063	386.416096	6.423616
5.949300	394.731021	6.428621
5.940321	396.962814	6.433626
5.558698	382.639968	6.438630
5.457553	376.600349	6.443635
5.487800	379.863730	6.448640
5.672295	392.135495	6.453645
5.803951	395.468510	6.458650
5.531965	376.541214	6.463654
5.565660	372.695199	6.468659
5.494830	371.367955	6.473664
5.590746	379.123071	6.478669
5.524189	386.175833	6.483674
5.951249	381.224546	6.488678
5.635227	372.383698	6.493683
5.780223	365.318682	6.498688
5.821026	367.609159	6.503693
5.401202	363.700882	6.508698
5.514357	351.116995	6.513702
5.083534	368.138360	6.518707
5.341938	376.349059	6.523712
5.570961	384.191019	6.528717
5.715804	380.859202	6.533722
5.848055	389.643199	6.538726
5.370399	376.496393	6.543731
5.700848	378.374783	6.548736
5.368142	383.194274	6.553741
5.691853	373.054775	6.558746
5.660966	385.037372	6.563750
5.105231	379.581051	6.568755
5.539526	386.293244	6.573760
5.682390	384.135472	6.578765
5.894785	375.101620	6.583770
5.772688	389.755938	6.588774
5.530426	385.079702	6.593779
5.963737	373.622852	6.598784
5.964565	362.239674	6.603789
5.486520	363.155627	6.608794
5.089046	361.683091	6.613798
5.516246	366.517138	6.618803
5.326391	366.075282	6.623808
5.753944	381.988591	6.628813
6.198862	387.383026	6.633818
5.552416	363.243302	6.638822
5.740999	366.485191	6.643827
5.513481	360.171029	6.648832
5.600383	360.673159	6.653837
5.559087	360.695384	6.658842
5.639477	354.940715	6.663846
5.767789	364.532058	6.668851
5.642697	358.825199	6.673856
5.605520	361.320802	6.678861
5.712057	366.258559	6.683866
5.617765	361.296703	6.688870
5.797301	365.062013	6.693875
5.654671	359.509743	6.698880
5.493923	362.771221	6.703885
5.484856	360.893366	6.708890
5.615940	354.444280	6.713894
5.581851	361.476158	6.718899
5.786497	358.941779	6.723904
5.561628	359.543071	6.728909
5.444418	358.210393	6.733914
5.942497	360.973830	6.738918
5.244200	362.556818	6.743923
5.181308	352.638872	6.748928
5.629000	355.267786	6.753933
5.422269	366.512132	6.758938
5.616675	353.820681	6.763942
5.737807	357.848179	6.768947
5.607009	362.054106	6.773952
5.480059	363.276057	6.778957
5.310085	359.923658	6.783962
5.596147	350.739146	6.788966
5.440814	361.380709	6.793971
5.501290	360.744855	6.798976
5.630565	358.984665	6.803981
5.530057	371.810148	6.808986
5.891915	360.146136	6.813990
5.721408	359.144455	6.818995
5.733050	362.768228	6.824000
5.717784	363.646929	6.829005
5.713722	362.685770	6.834010
6.020958	355.930850	6.839014
5.453014	369.107516	6.844019
5.685635	365.898074	6.849024
5.331733	362.976102	6.854029
5.723212	358.913036	6.859034
5.262775	358.035589	6.864038
5.392880	368.110702	6.869043
5.172534	364.807273	6.874048
5.418652	359.026799	6.879053
5.671668	366.017142	6.884058
5.540029	363.120675	6.889062
5.549175	361.451953	6.894067
5.628902	355.308251	6.899072
5.983586	351.994386	6.904077
5.921966	361.384349	6.909082
5.928011	357.349657	6.914086
5.440059	364.581914	6.919091
5.532652	359.913659	6.924096
5.581489	357.061859	6.929101
5.860901	366.319634	6.934106
5.995110	362.404189	6.939110
5.911312	364.090814	6.944115
5.815832	360.217459	6.949120
5.753987	363.846347	6.954125
5.576377	368.480338	6.959130
5.778813	359.653685	6.964134
5.455384	365.629645	6.969139
5.759299	366.158098	6.974144
5.565225	359.158531	6.979149
5.449008	363.124910	6.984154
5.778438	359.758029	6.989158
5.885153	361.554195	6.994163
5.172913	351.386180	6.999168
5.601892	356.520500	7.004173
5.730178	364.235769	7.009178
5.659307	348.852180	7.014182
5.458776	348.766322	7.019187
5.492481	363.111627	7.024192
5.336746	363.202289	7.029197
5.428976	366.544600	7.034202
5.646595	359.060161	7.039206
5.680310	375.525158	7.044211
5.568323	364.175362	7.049216
5.646186	371.828883	7.054221
5.580669	368.662696	7.059226
5.699828	363.781499	7.064230
5.701333	366.040130	7.069235
5.508449	368.442920	7.074240
5.518735	365.780615	7.079245
5.161491	373.400643	7.084250
5.888867	362.549740	7.089254
5.524651	371.256005	7.094259
5.586449	370.335211	7.099264
5.660739	373.993525	7.104269
5.415460	367.852965	7.109274
5.600074	365.533672	7.114278
5.609529	370.318869	7.119283
5.676171	366.350669	7.124288
5.778519	368.523997	7.129293
5.581036	363.628827	7.134298
5.737982	357.087129	7.139302
5.371519	369.004906	7.144307
5.566529	367.531868	7.149312
5.322993	366.475119	7.154317
5.396225	363.679630	7.159322
5.836252	366.857061	7.164326
5.829723	367.402212	7.169331
5.702077	363.160547	7.174336
5.801479	363.515201	7.179341
5.712358	365.136217	7.184346
5.593141	351.534994	7.189350
5.441008	355.133646	7.194355
5.171190	364.435805	7.199360
5.444356	359.834347	7.204365
5.257187	361.090984	7.209370
5.442074	356.297631	7.214374
5.133521	370.228001	7.219379
5.228506	368.704099	7.224384
5.326748	367.521371	7.229389
5.271290	365.660230	7.234394
5.833562	361.725593	7.239398
5.389238	357.542726	7.244403
5.639112	359.462133	7.249408
5.584927	353.339281	7.254413
5.529203	368.078159	7.259418
5.513970	364.179654	7.264422
5.242557	375.171488	7.269427
5.475676	387.891254	7.274432
5.927674	395.192308	7.279437
5.571200	394.200598	7.284442
5.708771	392.129068	7.289446
5.645553	382.862882	7.294451
5.340313	366.386323	7.299456
5.454073	369.089378	7.304461
5.546911	380.856558	7.309466
5.825160	380.443058	7.314470
6.162925	385.044265	7.319475
5.474103	371.316581	7.324480
5.502940	362.403062	7.329485
5.310849	370.076468	7.334490
5.604931	365.633101	7.339494
5.475830	369.231333	7.344499
5.493142	382.509872	7.349504
6.212864	381.182925	7.354509
5.849467	376.041504	7.359514
5.883276	359.325504	7.364518
5.651074	370.092934	7.369523
5.270209	365.182023	7.374528
5.611610	362.509293	7.379533
5.417467	368.930189	7.384538
5.384027	359.668870	7.389542
5.464547	369.935200	7.394547
5.754457	365.479827	7.399552
5.695168	366.567860	7.404557
5.413874	367.114663	7.409562
5.807295	362.380587	7.414566
5.411844	371.215099	7.419571
5.526408	373.380199	7.424576
5.217831	368.078387	7.429581
5.567479	373.762894	7.434586
5.684321	376.728057	7.439590
5.680589	365.896072	7.444595
5.426486	374.189730	7.449600
5.514524	368.563578	7.454605
5.743383	382.090750	7.459610
5.572551	380.238080	7.464614
5.638329	370.926505	7.469619
5.281636	372.946682	7.474624
6.027120	373.226053	7.479629
5.558024	388.592448	7.484634
5.614635	368.478226	7.489638
5.285445	373.765396	7.494643
5.615020	381.246855	7.499648
5.768098	387.797192	7.504653
5.572655	382.892207	7.509658
5.675010	368.342160	7.514662
5.684009	377.252907	7.519667
5.573625	377.478875	7.524672
5.386847	374.097452	7.529677
5.744000	377.414337	7.534682
5.812817	365.454266	7.539686
5.563331	368.368899	7.544691
5.451094	372.945256	7.549696
5.852885	363.897740	7.554701
5.775121	371.085117	7.559706
5.531176	368.917970	7.564710
5.510448	365.510695	7.569715
5.627761	377.175987	7.574720
5.762764	364.601343	7.579725
5.389855	368.414703	7.584730
5.470378	364.536090	7.589734
5.648314	365.716899	7.594739
5.601591	356.454486	7.599744
5.831631	362.477146	7.604749
5.764117	371.444095	7.609754
5.853681	364.694590	7.614758
5.707359	375.524581	7.619763
5.627546	364.527274	7.624768
6.124706	360.988747	7.629773
5.597922	366.613560	7.634778
5.758650	366.433490	7.639782
5.635401	372.893969	7.644787
5.248979	373.526742	7.649792
5.586658	361.588087	7.654797
5.367715	364.475818	7.659802
5.641819	368.925584	7.664806
5.772448	366.598878	7.669811
5.583650	369.184527	7.674816
5.428207	366.978290	7.679821
5.563353	375.113269	7.684826
5.470961	379.847888	7.689830
5.715296	371.634794	7.694835
5.505470	378.785789	7.699840
5.722321	369.836666	7.704845
5.329418	369.932617	7.709850
5.720719	372.652570	7.714854
5.625868	374.594015	7.719859
5.713664	372.878245	7.724864
5.869052	362.597283	7.729869
5.713267	380.784374	7.734874
5.416866	371.051469	7.739878
5.536616	372.057843	7.744883
5.587435	363.099774	7.749888
5.995201	365.671632	7.754893
5.575497	376.734011	7.759898
5.635464	367.904227	7.764902
5.618881	373.133234	7.769907
5.028000	368.340441	7.774912
5.711821	360.400606	7.779917
5.559949	364.334572	7.784922
5.428176	362.991507	7.789926
5.794958	357.546582	7.794931
5.549942	375.304641	7.799936
6.080306	357.204719	7.804941
5.810482	369.088467	7.809946
5.620524	360.496913	7.814950
5.155708	361.521536	7.819955
5.588665	365.769401	7.824960
5.754963	362.804400	7.829965
5.334680	368.384158	7.834970
5.387029	368.578462	7.839974
5.455004	368.583673	7.844979
5.309204	368.944868	7.849984
5.566507	364.573665	7.854989
5.347065	363.320179	7.859994
5.505186	365.782211	7.864998
5.805800	361.344156	7.870003
5.559384	366.691202	7.875008
5.422334	372.688764	7.880013
5.521585	370.129665	7.885018
5.465198	374.624561	7.890022
5.814859	374.073394	7.895027
5.656837	370.380615	7.900032
6.036073	366.809828	7.905037
5.565331	377.541637	7.910042
5.439857	369.386122	7.915046
5.498053	373.739794	7.920051
5.220617	369.784037	7.925056
5.393886	371.943160	7.930061
5.169696	371.402247	7.935066
5.309912	374.537775	7.940070
5.419971	370.717836	7.945075
5.383154	370.138259	7.950080
5.803897	371.603962	7.955085
5.639222	378.219587	7.960090
5.479149	376.488627	7.965094
5.763725	370.705326	7.970099
5.153906	371.866419	7.975104
5.601254	382.467942	7.980109
5.875203	394.295517	7.985114
5.759787	381.019542	7.990118
5.484171	379.006148	7.995136
5.584365	372.991653	8.000154
5.679120	366.529906	8.005171
5.449869	377.253726	8.010189
5.639139	382.636158	8.015206
5.686186	376.282816	8.020224
5.436683	372.162506	8.025242
5.991231	376.115360	8.030259
5.875452	382.564559	8.035277
5.440338	370.571425	8.040294
5.602750	378.810735	8.045312
5.505660	371.602568	8.050330
5.393550	371.140343	8.055347
5.585367	387.242089	8.060365
5.832666	396.235012	8.065382
5.982077	389.446026	8.070400
5.516520	379.145895	8.075418
5.767215	364.679256	8.080435
5.745935	382.149011	8.085453
5.671555	376.104894	8.090470
5.627586	369.929818	8.095488
5.224588	375.338194	8.100506
5.933210	383.135875	8.105523
5.589884	393.142202	8.110541
5.770276	392.132687	8.115558
6.088230	388.675065	8.120576
5.343438	384.227946	8.125594
5.725704	380.362701	8.130611
5.940012	389.733123	8.135629
5.776075	380.307477	8.140646
5.880624	368.577441	8.145664
5.407239	371.582710	8.150682
5.502696	368.203913	8.155699
5.846882	380.876997	8.160717
5.739562	386.434989	8.165734
5.859151	388.218217	8.170752
5.989566	395.487424	8.175770
5.751300	396.887736	8.180787
5.869548	396.007810	8.185805
6.128739	390.407189	8.190822
6.018380	377.255856	8.195840
5.699904	375.383633	8.200858
5.512690	374.475533	8.205875
5.329050	380.951075	8.210893
5.646263	395.641668	8.215910
5.845120	395.740064	8.220928
5.819633	396.835862	8.225946
5.669690	394.255778	8.230963
5.432902	394.835392	8.235981
5.743366	394.389419	8.240998
5.947003	393.477266	8.246016
5.825467	399.258370	8.251034
5.857063	397.950147	8.256051
5.534267	397.669039	8.261069
5.922245	392.209302	8.266086
5.849814	391.882902	8.271104
5.852136	394.845666	8.276122
5.912210	388.294642	8.281139
6.014579	394.599432	8.286157
6.146532	406.273683	8.291174
5.954007	384.144706	8.296192
6.176277	388.919274	8.301210
5.972678	395.136010	8.306227
5.815197	398.442376	8.311245
5.924481	394.764791	8.316262
6.055062	393.153992	8.321280
5.994508	393.863949	8.326298
5.832924	384.220195	8.331315
6.156156	388.584589	8.336333
6.115783	391.885342	8.341350
6.264140	386.563896	8.346368
5.994226	383.731108	8.351386
5.955996	395.138373	8.356403
6.062281	390.192687	8.361421
5.893030	385.198389	8.366438
5.964337	384.603469	8.371456
5.893324	389.991716	8.376474
5.737422	389.283857	8.381491
5.831452	393.889055	8.386509
5.802384	396.591632	8.391526
5.704688	392.517106	8.396544
5.933838	399.770941	8.401562
5.839177	388.131866	8.406579
5.850243	390.272800	8.411597
6.017993	400.231115	8.416614
6.399084	389.527771	8.421632
6.086266	392.580624	8.426650
5.918599	389.760316	8.431667
5.923363	394.890627	8.436685
5.726012	384.337305	8.441702
6.397738	397.764092	8.446720
5.927061	397.487075	8.451738
6.230174	384.605859	8.456755
6.007323	391.930066	8.461773
5.928309	391.948656	8.466790
6.202769	392.780013	8.471808
6.067470	401.084620	8.476826
5.691975	387.599039	8.481843
6.071110	390.638826	8.486861
6.052358	394.930241	8.491878
6.065690	392.968488	8.496896
5.946930	396.189933	8.501914
5.814705	404.118541	8.506931
6.354741	407.821210	8.511949
6.093475	406.069458	8.516966
6.347115	401.100827	8.521984
6.170497	395.239870	8.527002
5.904638	393.700263	8.532019
6.425079	396.632848	8.537037
5.885793	395.312528	8.542054
6.558507	402.917004	8.547072
6.165879	401.043701	8.552090
5.667977	397.094598	8.557107
6.298544	404.793994	8.562125
6.123581	412.079197	8.567143
6.685298	412.597600	8.572160
6.277388	406.453931	8.577178
6.194230	396.169987	8.582195
6.289887	396.240273	8.587213
6.088058	405.113789	8.592231
6.364077	391.501521	8.597248
6.335706	387.892704	8.602266
5.974288	394.973413	8.607283
6.058591	389.330597	8.612301
5.905213	411.570191	8.617319
6.456195	410.903742	8.622336
6.568267	417.036625	8.627354
6.257261	411.335435	8.632371
6.199451	403.780330	8.637389
5.916770	405.537835	8.642407
6.316504	414.819442	8.647424
6.512247	419.651794	8.652442
6.234134	423.172597	8.657459
6.400198	422.398829	8.662477
6.033429	426.293179	8.667495
6.399212	420.776932	8.672512
6.360965	413.840439	8.677530
6.635014	424.896160	8.682547
6.334224	410.089336	8.687565
6.569290	423.464215	8.692583
6.254944	400.508472	8.697600
6.326275	405.208720	8.702618
6.274082	405.223134	8.707635
6.291305	402.102652	8.712653
6.313822	405.062273	8.717671
6.315077	414.431167	8.722688
6.535968	413.844514	8.727706
6.356321	414.254294	8.732723
6.454984	406.816829	8.737741
6.427889	411.554493	8.742759
6.057539	407.651796	8.747776
6.479942	417.753499	8.752794
6.560244	415.623533	8.757811
6.721571	405.519258	8.762829
6.062104	401.588997	8.767847
6.397354	400.722620	8.772864
6.517563	415.797334	8.777882
6.593303	417.663128	8.782899
6.539176	415.348976	8.787917
6.604654	412.735349	8.792935
6.311956	397.343481	8.797952
6.181172	400.680402	8.802970
6.309563	413.920412	8.807987
6.842273	411.978771	8.813005
6.186730	418.789719	8.818023
6.642502	421.776556	8.823040
6.508355	426.922193	8.828058
6.245226	419.067705	8.833075
6.709934	415.293754	8.838093
6.145904	427.559194	8.843111
6.575419	422.370679	8.848128
6.398975	424.282049	8.853146
6.102191	425.397999	8.858163
6.457471	428.491997	8.863181
6.533036	423.014624	8.868199
6.185531	420.862908	8.873216
6.440795	421.832948	8.878234
6.384858	421.002232	8.883251
6.625005	422.290190	8.888269
6.714699	424.456755	8.893287
6.537456	413.007237	8.898304
6.793138	416.561686	8.903322
6.342970	426.338527	8.908339
6.456851	420.091522	8.913357
6.300505	423.691191	8.918375
6.177267	419.841530	8.923392
6.566162	422.595795	8.928410
6.634060	440.786989	8.933427
7.014780	437.026110	8.938445
6.644018	435.225134	8.943463
6.423898	425.334865	8.948480
7.001666	429.653326	8.953498
6.537710	431.104559	8.958515
6.717718	418.255107	8.963533
6.609180	424.753684	8.968551
6.343187	418.351242	8.973568
6.643069	436.294883	8.978586
6.553374	448.271901	8.983603
6.932043	438.569248	8.988621
6.830125	443.580489	8.993639
6.979611	446.687598	8.998656
6.943956	430.293207	9.003674
6.550204	426.605578	9.008691
6.641104	425.076690	9.013709
6.733088	431.424134	9.018727
6.790063	426.157928	9.023744
6.246915	423.585415	9.028762
6.519061	430.753677	9.033779
7.194753	444.801545	9.038797
6.596125	444.415067	9.043815
6.722774	447.251190	9.048832
7.058602	446.299518	9.053850
6.933928	444.040525	9.058867
6.880863	423.360320	9.063885
7.104681	429.100287	9.068903
6.919091	424.086432	9.073920
6.859157	428.684054	9.078938
6.473459	420.854960	9.083955
6.693763	419.946522	9.088973
6.719939	414.306437	9.093991
6.794614	417.232694	9.099008
6.800591	416.303979	9.104026
6.287994	423.360903	9.109043
6.816232	434.635817	9.114061
7.126171	446.998715	9.119079
7.091236	441.986643	9.124096
6.853298	424.778038	9.129114
6.575812	424.051240	9.134131
7.108236	431.229468	9.139149
6.889479	439.338814	9.144167
7.125333	436.181130	9.149184
7.491724	422.185557	9.154202
6.632308	416.399347	9.159219
6.548476	411.095111	9.164237
6.438661	423.778954	9.169255
6.969833	433.674392	9.174272
6.739595	442.735378	9.179290
7.036301	448.441913	9.184307
6.818782	446.594987	9.189325
7.299417	452.642097	9.194343
6.967791	445.868029	9.199360
7.125474	442.624690	9.204378
6.901189	444.265814	9.209395
7.166387	443.536568	9.214413
7.080244	437.084026	9.219431
6.697936	432.731928	9.224448
6.841607	437.638661	9.229466
7.164135	451.962417	9.234483
7.282109	443.726706	9.239501
7.279894	432.041651	9.244519
6.790773	426.551217	9.249536
7.020521	422.353121	9.254554
6.784131	424.914422	9.259571
7.032535	434.692949	9.264589
7.307698	439.677035	9.269607
7.433491	439.310304	9.274624
7.144976	423.457038	9.279642
6.858779	429.894919	9.284659
6.749477	416.976910	9.289677
6.553486	424.858655	9.294695
7.228985	437.584330	9.299712
7.405721	436.411288	9.304730
7.023966	445.268659	9.309747
6.984004	448.600916	9.314765
6.722365	442.251433	9.319783
6.799977	447.212633	9.324800
6.985207	440.162444	9.329818
7.091864	438.747861	9.334835
7.018891	438.222738	9.339853
7.513250	452.295690	9.344871
7.335272	447.230153	9.349888
7.072002	446.706258	9.354906
7.145740	448.515565	9.359923
7.151188	445.011919	9.364941
7.303747	439.194366	9.369959
6.481919	445.207589	9.374976
7.045473	446.969035	9.379994
7.058993	447.834711	9.385011
7.089978	449.458180	9.390029
7.378154	442.521343	9.395047
7.127751	443.188281	9.400064
7.092677	436.958151	9.405082
6.746441	446.368543	9.410099
6.978610	447.159153	9.415117
7.146592	448.963254	9.420135
6.902625	463.469890	9.425152
7.605860	463.464512	9.430170
7.423203	482.502607	9.435187
7.272585	457.334426	9.440205
7.121160	450.664837	9.445223
7.340401	455.941644	9.450240
7.122474	449.569574	9.455258
7.297882	464.727249	9.460275
7.543349	466.920056	9.465293
7.749950	452.387631	9.470311
7.100003	460.822886	9.475328
7.352659	445.002100	9.480346
7.317928	449.198191	9.485363
6.971823	446.806424	9.490381
7.295403	447.058963	9.495399
7.545376	455.410902	9.500416
7.241922	453.836119	9.505434
7.454953	454.866383	9.510451
6.799019	459.891307	9.515469
7.355717	467.245643	9.520487
7.793818	467.114296	9.525504
7.939392	468.644190	9.530522
7.438597	460.640504	9.535539
7.293999	451.426394	9.540557
7.444903	444.646622	9.545575
7.359714	453.167503	9.550592
7.130604	456.980469	9.555610
7.491337	453.875919	9.560627
7.272753	453.944640	9.565645
7.174512	452.883835	9.570663
7.452511	468.224346	9.575680
7.788078	470.147517	9.580698
7.513397	462.099158	9.585715
7.606787	462.217132	9.590733
7.562293	450.892081	9.595751
7.237467	455.092317	9.600768
7.382999	462.046787	9.605786
7.304981	471.185068	9.610803
7.526657	478.645217	9.615821
7.684693	471.491957	9.620839
7.337059	471.943672	9.625856
7.577149	463.944546	9.630874
7.496149	471.353993	9.635891
7.213003	471.688375	9.640909
7.560778	466.506262	9.645927
7.549595	474.466546	9.650944
7.574665	476.381259	9.655962
7.690857	473.633501	9.660979
7.120942	478.215868	9.665997
7.613777	467.772778	9.671015
7.393829	471.423382	9.676032
7.436442	468.384138	9.681050
7.606000	474.514402	9.686067
7.609591	482.844757	9.691085
7.808791	472.002434	9.696103
7.402326	480.702731	9.701120
7.461955	477.821775	9.706138
7.594919	477.857851	9.711155
7.419194	475.338572	9.716173
7.456545	472.991235	9.721191
7.734924	479.237094	9.726208
7.870289	476.824006	9.731226
8.145644	474.587929	9.736243
7.556200	475.272943	9.741261
7.529079	477.072712	9.746279
7.484834	469.095764	9.751296
7.404731	467.445182	9.756314
7.613328	470.505224	9.761331
7.330384	468.513855	9.766349
7.889818	480.869487	9.771367
7.784729	486.237824	9.776384
7.490382	480.978966	9.781402
7.977748	492.799899	9.786419
7.616317	485.796937	9.791437
7.795180	481.439501	9.796455
7.768642	485.277735	9.801472
7.919256	489.119945	9.806490
7.585146	473.422048	9.811507
7.951481	488.177649	9.816525
7.876251	477.207646	9.821543
7.820290	468.516188	9.826560
7.600871	474.315713	9.831578
7.644714	483.346668	9.836595
8.118372	487.324765	9.841613
7.593799	485.203765	9.846631
7.853538	494.753353	9.851648
7.875989	491.647819	9.856666
8.286494	489.867202	9.861683
7.807074	483.346494	9.866701
7.974451	476.529433	9.871719
7.429909	476.096665	9.876736
7.702431	488.714715	9.881754
7.910641	488.275193	9.886771
7.870742	498.534124	9.891789
8.035344	497.268298	9.896807
8.016762	496.520120	9.901824
7.917581	503.534797	9.906842
8.062703	498.488364	9.911859
7.784927	504.536815	9.916877
7.957840	499.255692	9.921895
7.933888	505.614902	9.926912
7.871850	508.221648	9.931930
8.180440	494.436980	9.936947
7.961551	506.655049	9.941965
8.195790	497.965728	9.946983
8.100140	500.057023	9.952000
7.778781	490.908281	9.957018
8.049446	486.725890	9.962035
7.836674	493.120806	9.967053
8.372422	501.993136	9.972071
7.640804	486.779977	9.977088
7.739782	490.680717	9.982106
8.215418	495.617828	9.987123
8.241896	505.187961	9.992141
8.214820	495.355954	9.997159
8.199194	499.167247	10.002176
7.843373	498.039251	10.007194
8.226700	485.650379	10.012211
7.948868	500.998568	10.017229
7.807655	495.485500	10.022247
8.066261	493.624396	10.027264
8.079140	505.389831	10.032282
8.295801	500.016693	10.037299
8.071294	503.380848	10.042317
8.594059	496.978641	10.047335
8.044764	497.499622	10.052352
7.862679	495.517792	10.057370
8.059595	492.022194	10.062387
7.930507	496.024713	10.067405
7.966407	497.862006	10.072423
8.083192	500.339928	10.077440
8.004079	494.785636	10.082458
8.213423	493.361371	10.087475
8.151470	496.867466	10.092493
8.013670	497.564209	10.097511
8.303403	495.209131	10.102528
7.924722	498.556267	10.107546
8.040806	496.666862	10.112563
7.914673	512.281763	10.117581
8.144336	507.616623	10.122599
8.148449	508.704663	10.127616
8.180129	506.803153	10.132634
8.192806	508.072888	10.137651
8.152637	516.946535	10.142669
8.354008	507.107355	10.147687
8.213135	511.600840	10.152704
8.389917	511.617472	10.157722
8.246706	499.629292	10.162739
8.389948	505.397607	10.167757
8.555158	515.738217	10.172775
8.344814	501.889179	10.177792
8.134505	506.134710	10.182810
8.092359	501.013296	10.187827
8.353863	515.368694	10.192845
8.248225	525.038300	10.197863
8.689577	521.189071	10.202880
8.260891	529.877074	10.207898
8.609865	524.650578	10.212915
8.420025	517.447326	10.217933
8.256156	501.259016	10.222951
8.516147	503.039330	10.227968
8.451853	499.473952	10.232986
8.600565	494.941334	10.238003
8.279766	493.861531	10.243021
8.119867	498.367443	10.248039
8.747900	509.229253	10.253056
8.366214	520.295615	10.258074
8.535565	510.814852	10.263091
8.339710	509.658793	10.268109
8.143892	512.276903	10.273127
8.348506	516.252715	10.278144
8.562985	519.090954	10.283162
8.476679	520.016355	10.288179
8.674004	518.483512	10.293197
8.491245	520.411654	10.298215
8.818374	520.837203	10.303232
8.603440	513.177133	10.308250
8.646326	507.240940	10.313267
8.230347	501.199475	10.318285
8.385135	518.493635	10.323303
8.357817	513.205814	10.328320
8.300592	519.437672	10.333338
8.643144	521.498610	10.338355
8.785257	515.420738	10.343373
8.275018	519.675103	10.348391
8.923646	518.838820	10.353408
8.504145	521.977730	10.358426
8.764458	531.022341	10.363443
8.740124	525.964416	10.368461
8.477209	523.016912	10.373479
8.770203	520.765459	10.378496
8.759487	529.072818	10.383514
8.728430	525.707378	10.388531
8.975121	529.301118	10.393549
8.820893	519.043947	10.398567
8.767484	522.558183	10.403584
8.626685	519.635846	10.408602
8.749661	517.212058	10.413619
8.817802	524.020819	10.418637
8.506453	519.853302	10.423655
8.938169	510.486318	10.428672
8.692955	512.310579	10.433690
8.714036	516.005712	10.438707
8.897018	526.062707	10.443725
8.452439	519.309353	10.448743
8.758839	524.651501	10.453760
8.627836	525.429235	10.458778
8.916483	516.699877	10.463795
8.764745	524.328633	10.468813
8.556557	526.683595	10.473831
8.751359	520.793169	10.478848
8.628897	527.568494	10.483866
8.744837	521.052902	10.488883
9.114538	530.364491	10.493901
8.582664	518.051822	10.498919
8.730467	520.253530	10.503936
8.511998	530.773801	10.508954
8.647366	531.775138	10.513971
8.420138	534.170933	10.518989
8.573389	530.177218	10.524007
8.741185	532.142296	10.529024
8.472775	534.200535	10.534042
8.971706	537.641400	10.539059
9.025183	549.201735	10.544077
8.851072	553.495288	10.549095
9.312375	550.775832	10.554112
8.890761	547.666848	10.559130
8.873943	533.775031	10.564147
8.995557	534.289381	10.569165
8.623585	544.303408	10.574183
9.005403	553.527920	10.579200
8.973965	559.471766	10.584218
9.045651	553.206039	10.589235
9.126527	554.846996	10.594253
9.240518	557.356917	10.599271
8.914466	539.000633	10.604288
8.946236	547.815760	10.609306
9.641231	548.278704	10.614323
9.275489	540.916645	10.619341
8.982000	531.586826	10.624359
9.179943	526.680477	10.629376
8.927581	524.637006	10.634394
8.719820	522.930558	10.639411
8.802892	532.999957	10.644429
8.905959	537.057854	10.649447
9.039911	543.670191	10.654464
9.097817	554.279984	10.659482
9.444576	555.623934	10.664499
9.276768	552.652149	10.669517
9.098524	558.584140	10.674535
9.134463	545.813831	10.679552
9.234890	553.015190	10.684570
9.449218	547.822274	10.689587
9.267290	530.137806	10.694605
9.106949	531.251453	10.699623
9.577712	527.135723	10.704640
8.951809	538.117049	10.709658
8.946741	534.274211	10.714675
9.159825	534.348303	10.719693
9.101122	537.336371	10.724711
9.569841	538.806491	10.729728
8.983228	537.026490	10.734746
9.032972	535.109542	10.739763
9.432806	544.845618	10.744781
9.279347	559.549671	10.749799
9.533905	548.692371	10.754816
9.098505	540.246141	10.759834
8.925471	543.879988	10.764851
9.264070	543.593727	10.769869
8.872009	559.379455	10.774887
9.379558	562.683289	10.779904
9.436273	559.648145	10.784922
9.226825	562.596574	10.789939
9.244986	561.019042	10.794957
8.924952	559.689818	10.799975
9.323181	566.223148	10.804992
9.406693	560.883346	10.810010
9.197567	557.204811	10.815027
9.345147	558.144290	10.820045
9.132388	550.404973	10.825063
9.249818	558.219043	10.830080
9.207552	553.978066	10.835098
9.448112	549.106100	10.840115
9.607120	548.131462	10.845133
9.394845	555.024919	10.850151
9.414868	554.425356	10.855168
9.361181	556.999253	10.860186
9.321467	561.331840	10.865203
9.295482	561.070785	10.870221
9.211155	562.952050	10.875239
9.797383	565.754505	10.880256
9.436585	567.735618	10.885274
9.788151	571.221523	10.890291
9.792206	561.312052	10.895309
9.359225	556.787939	10.900327
8.990817	563.093508	10.905344
9.749885	568.759650	10.910362
9.649757	574.247156	10.915379
9.434046	576.899928	10.920397
9.314784	586.890411	10.925415
9.490399	579.201062	10.930432
9.676040	581.592539	10.935450
9.399670	585.037365	10.940467
9.678462	581.273391	10.945485
9.305868	580.990566	10.950503
9.619900	583.466190	10.955520
9.901532	578.082913	10.960538
9.527590	588.614803	10.965555
9.760225	582.071552	10.970573
9.383272	591.786592	10.975591
9.674080	589.421868	10.980608
9.581004	579.309768	10.985626
9.508407	585.938502	10.990643
9.668069	573.612794	10.995661
9.559273	579.982085	11.000679
9.606931	574.972895	11.005696
9.906111	577.021658	11.010714
9.759539	585.643674	11.015731
9.796028	577.114487	11.020749
9.681302	577.179662	11.025767
9.662039	580.997850	11.030784
9.922344	571.256751	11.035802
9.616633	579.742602	11.040819
9.917915	573.526324	11.045837
9.705555	578.879833	11.050855
10.139456	587.588190	11.055872
9.912580	580.728336	11.060890
9.582183	582.597424	11.065907
9.448284	581.046721	11.070925
9.363249	583.701239	11.075943
9.371333	581.121769	11.080960
10.159829	590.122042	11.085978
9.983104	606.906192	11.090995
10.087792	595.116027	11.096013
9.928995	579.248736	11.101031
10.045108	584.570039	11.106048
10.004377	578.113531	11.111066
9.709520	579.850859	11.116083
9.902367	578.514359	11.121101
9.905623	585.377426	11.126119
9.841755	580.959932	11.131136
9.882525	584.383781	11.136154
9.807083	593.711065	11.141171
10.009115	606.273903	11.146189
9.847252	608.078885	11.151207
9.889788	610.536826	11.156224
10.590405	595.488728	11.161242
10.319372	594.025645	11.166259
9.833251	583.586591	11.171277
9.678772	590.714049	11.176295
9.762084	591.114448	11.181312
9.880712	603.371547	11.186330
9.774687	605.480248	11.191347
9.906499	612.313841	11.196365
9.687386	608.520091	11.201383
9.967169	607.905328	11.206400
9.800728	607.113898	11.211418
9.565096	600.242777	11.216435
10.274655	602.783048	11.221453
10.212552	603.382806	11.226471
10.069601	594.932040	11.231488
10.158078	607.869152	11.236506
10.216179	618.302234	11.241523
10.201862	612.870355	11.246541
9.953690	605.007145	11.251559
10.050935	608.744085	11.256576
10.185839	623.283377	11.261594
10.338833	628.781980	11.266611
10.510735	631.084088	11.271629
9.965522	617.448038	11.276647
10.056216	608.853594	11.281664
10.852522	614.207852	11.286682
10.190247	614.153159	11.291699
10.015720	603.034442	11.296717
10.318508	608.979913	11.301735
10.331168	609.858354	11.306752
10.482358	610.630022	11.311770
10.305254	607.015917	11.316787
10.060645	605.062744	11.321805
10.308966	609.246359	11.326823
10.311315	624.121858	11.331840
10.521245	621.529889	11.336858
10.324120	628.253764	11.341875
10.537144	619.687604	11.346893
10.375505	617.412254	11.351911
10.119655	612.510267	11.356928
10.481084	619.778309	11.361946
10.379354	628.469100	11.366963
10.514558	627.450830	11.371981
10.177631	629.343029	11.376999
10.494711	628.716147	11.382016
10.469593	623.301724	11.387034
10.249973	630.565568	11.392051
10.156303	636.386590	11.397069
10.512136	628.132694	11.402087
10.221902	632.804093	11.407104
10.399458	631.706648	11.412122
10.410978	628.025302	11.417139
10.320677	628.604205	11.422157
10.284129	632.586036	11.427175
10.300843	632.835865	11.432192
10.379809	645.348467	11.437210
9.969368	635.702299	11.442227
10.643557	644.019834	11.447245
10.633687	644.011881	11.452263
10.517962	646.500779	11.457280
10.672380	646.801749	11.462298
10.875266	648.897070	11.467315
10.324382	637.410912	11.472333
10.612490	638.953342	11.477351
10.540487	639.904923	11.482368
10.853437	643.478903	11.487386
10.855175	642.907430	11.492403
10.458941	632.627914	11.497421
10.908361	632.311774	11.502439
10.876238	636.633730	11.507456
10.839089	637.971190	11.512474
10.766091	638.348592	11.517491
10.594060	636.769109	11.522509
11.010912	631.923319	11.527527
10.521127	634.577748	11.532544
10.550984	638.886900	11.537562
10.682705	635.644412	11.542579
10.711381	639.963214	11.547597
10.661401	633.413456	11.552615
10.662626	635.148869	11.557632
10.997918	643.190978	11.562650
10.747218	646.792759	11.567667
10.508886	641.260055	11.572685
11.094997	640.673333	11.577703
10.872115	652.750117	11.582720
10.598228	646.736970	11.587738
11.140624	657.716343	11.592755
10.824834	658.147326	11.597773
10.972891	654.716105	11.602791
10.742262	649.377852	11.607808
11.215363	650.209850	11.612826
11.161153	637.160032	11.617843
10.785349	632.178890	11.622861
11.101822	633.836819	11.627879
10.719447	640.501181	11.632896
10.576572	626.982355	11.637914
10.793786	638.245867	11.642931
10.784111	645.969316	11.647949
11.233003	649.702006	11.652967
11.090097	659.323840	11.657984
11.331940	654.454801	11.663002
10.727439	642.494167	11.668019
11.018165	655.043231	11.673037
11.120720	645.809473	11.678055
11.036114	661.708362	11.683072
11.228745	660.166771	11.688090
11.254544	654.854860	11.693107
11.431708	657.960853	11.698125
11.146172	632.504173	11.703143
10.725130	637.647204	11.708160
10.447094	633.092635	11.713178
10.789389	650.850016	11.718195
10.979567	657.204341	11.723213
11.015612	651.060890	11.728231
10.938722	665.633192	11.733248
11.208236	657.992303	11.738266
11.549970	655.717467	11.743283
11.124852	659.393742	11.748301
11.326441	654.467857	11.753319
10.959005	658.819936	11.758336
11.086041	656.613240	11.763354
11.343749	657.627093	11.768371
11.461500	663.519344	11.773389
11.692579	661.801359	11.778407
11.150296	663.239559	11.783424
10.994981	665.624175	11.788442
11.215609	666.640645	11.793459
11.425305	660.886705	11.798477
11.180889	656.408944	11.803495
11.324426	662.445497	11.808512
11.223097	657.939146	11.813530
10.975030	657.769470	11.818547
11.235929	665.009004	11.823565
11.472680	662.845183	11.828583
11.298423	660.372984	11.833600
11.284672	654.663303	11.838618
11.460576	660.076301	11.843635
11.052601	659.171001	11.848653
11.547159	657.696006	11.853671
11.311810	660.512788	11.858688
11.339793	657.882874	11.863706
11.809484	662.120394	11.868723
11.302758	663.606704	11.873741
11.730454	656.736421	11.878759
11.413327	659.414463	11.883776
11.358822	657.425374	11.888794
11.325678	665.925630	11.893811
10.747831	663.484712	11.898829
11.282410	665.522080	11.903847
11.586423	679.495465	11.908864
11.690750	682.745342	11.913882
12.038648	674.555773	11.918899
11.565813	675.146902	11.923917
11.522164	655.077167	11.928935
11.448652	654.987607	11.933952
11.768583	665.973221	11.938970
11.654959	659.556434	11.943987
11.531615	655.056667	11.949005
11.796189	665.205175	11.954023
11.645692	661.157742	11.959040
11.685373	661.845792	11.964058
11.601328	658.245589	11.969075
11.480645	669.580663	11.974093
11.911425	671.716242	11.979111
11.790761	679.166663	11.984128
11.632372	680.646075	11.989146
11.658675	665.349469	11.994163
11.819989	668.315926	11.999181
11.899893	661.430366	12.004199
11.821111	663.118280	12.009216
11.617196	664.185072	12.014234
11.548609	657.878035	12.019251
12.070676	681.098358	12.024269
12.004996	676.027894	12.029287
11.631697	662.185168	12.034304
11.508366	659.796555	12.039322
12.092160	672.397828	12.044339
11.818208	673.349297	12.049357
11.956384	659.550011	12.054375
11.859434	658.037728	12.059392
11.568040	657.117433	12.064410
12.077572	668.651019	12.069427
12.040377	681.834961	12.074445
11.972567	668.629453	12.079463
11.855190	667.155063	12.084480
11.669815	665.120079	12.089498
12.059769	682.232621	12.094515
11.905696	674.225346	12.099533
11.743937	679.880265	12.104551
12.002161	680.717320	12.109568
11.970561	679.718706	12.114586
12.280846	682.217017	12.119603
11.718489	693.668210	12.124621
12.079822	687.458321	12.129639
12.440802	692.640549	12.134656
11.893109	674.975017	12.139674
12.398132	674.372518	12.144691
11.525736	675.906296	12.149709
11.893013	676.827354	12.154727
12.050446	686.273057	12.159744
11.987917	682.167743	12.164762
12.329043	690.300480	12.169779
12.093685	683.729076	12.174797
12.351931	687.302115	12.179815
12.086560	679.211184	12.184832
11.838808	683.112304	12.189850
12.394144	677.408681	12.194867
12.098219	679.565892	12.199885
12.377206	680.977206	12.204903
12.323886	683.027218	12.209920
12.089471	684.616294	12.214938
12.098747	681.149874	12.219955
12.205104	687.820208	12.224973
12.379284	678.518479	12.229991
12.466540	689.410951	12.235008
11.966148	692.117532	12.240026
12.201891	678.078985	12.245043
12.283555	676.863928	12.250061
11.953982	676.650140	12.255079
12.135709	676.189492	12.260096
12.532492	680.072308	12.265114
12.390824	681.874153	12.270131
11.816262	679.054037	12.275149
12.323537	683.348824	12.280167
12.195387	687.392265	12.285184
12.285723	681.013140	12.290202
12.506244	673.487166	12.295219
12.218382	678.751478	12.300237
12.059075	684.630071	12.305255
12.596769	693.694692	12.310272
12.489383	690.830237	12.315290
12.549052	685.093337	12.320307
12.634477	689.819867	12.325325
12.401710	672.297802	12.330343
12.478638	675.211129	12.335360
12.360212	674.551070	12.340378
12.336150	687.540474	12.345395
12.471892	699.337399	12.350413
12.597576	707.958108	12.355431
12.872088	695.668081	12.360448
12.627463	700.152522	12.365466
12.722539	688.568912	12.370483
12.618098	688.787114	12.375501
12.099331	690.202720	12.380519
12.105670	694.319893	12.385536
12.419321	699.916577	12.390554
12.732551	709.562090	12.395571
12.798423	714.073928	12.400589
12.797138	703.092272	12.405607
13.033195	700.609829	12.410624
12.548805	707.851815	12.415642
12.817805	704.234502	12.420659
12.642178	707.919278	12.425677
12.567420	696.642963	12.430695
12.730976	703.462182	12.435712
12.958344	706.175371	12.440730
12.783536	698.606800	12.445747
12.934313	704.695888	12.450765
12.888813	700.083007	12.455783
12.966052	705.580806	12.460800
13.046539	701.592071	12.465818
12.905375	688.492640	12.470835
12.860203	694.123100	12.475853
12.970295	704.863708	12.480871
12.987441	686.299207	12.485888
12.454523	682.462784	12.490906
12.511150	687.297935	12.495923
12.527392	698.321386	12.500941
12.124842	697.247987	12.505959
12.413243	702.482542	12.510976
12.421293	708.947292	12.515994
12.452954	717.342812	12.521011
13.059414	726.074861	12.526029
13.264814	730.198917	12.531047
13.444231	733.291949	12.536064
13.144126	725.427305	12.541082
12.921721	711.327525	12.546099
12.803559	709.285228	12.551117
13.164122	715.944395	12.556135
13.153616	716.138505	12.561152
13.048625	723.015322	12.566170
12.927814	721.140687	12.571187
13.089903	711.446361	12.576205
12.787259	727.038441	12.581223
12.990626	718.773529	12.586240
12.759200	727.418291	12.591258
12.895157	723.613413	12.596275
13.228473	727.282066	12.601293
13.013550	732.837985	12.606311
13.475696	718.622151	12.611328
12.951056	725.794673	12.616346
13.076028	715.112078	12.621363
13.146760	725.716820	12.626381
12.781378	725.312953	12.631399
13.130654	719.713981	12.636416
13.212774	728.057470	12.641434
13.358643	721.953697	12.646451
13.346376	722.037632	12.651469
13.115603	719.971842	12.656487
13.160351	716.297927	12.661504
13.544064	725.597971	12.666522
13.513149	718.953698	12.671539
13.345057	726.373654	12.676557
13.191281	720.546902	12.681575
13.357754	723.455762	12.686592
13.062736	729.778363	12.691610
13.362823	738.999919	12.696627
13.343289	746.993182	12.701645
13.130658	742.409467	12.706663
13.567027	745.983186	12.711680
13.568341	742.199268	12.716698
13.550896	746.440073	12.721715
13.459308	746.384884	12.726733
13.123779	752.095282	12.731751
13.417150	751.667741	12.736768
13.360693	746.529551	12.741786
13.385626	754.061472	12.746803
13.439034	750.376735	12.751821
13.145014	751.283998	12.756839
13.132259	750.421296	12.761856
13.480532	759.651139	12.766874
13.466747	755.932682	12.771891
13.393350	744.283751	12.776909
13.280077	754.046185	12.781927
14.062879	756.515117	12.786944
13.558127	756.606305	12.791962
13.705439	748.684611	12.796979
13.629466	751.164179	12.801997
13.564864	755.049422	12.807015
13.781534	754.586487	12.812032
13.664627	759.221466	12.817050
13.765051	742.925517	12.822067
13.544526	752.846655	12.827085
13.575240	766.127380	12.832103
14.169966	776.110942	12.837120
13.701974	769.569415	12.842138
13.791339	770.691533	12.847155
13.823679	761.699014	12.852173
13.912854	759.782215	12.857191
13.615665	770.018247	12.862208
13.970513	775.715834	12.867226
13.845758	775.530114	12.872243
14.176046	760.255523	12.877261
13.903885	755.482264	12.882279
13.661962	751.780394	12.887296
13.920259	754.185828	12.892314
13.874434	760.693697	12.897331
14.059146	761.318146	12.902349
13.730202	755.565991	12.907367
14.319326	757.307709	12.912384
14.234622	762.502546	12.917402
14.042533	748.887152	12.922419
13.992066	743.735407	12.927437
14.018821	755.959580	12.932455
13.799697	751.108639	12.937472
13.876522	750.383464	12.942490
13.872971	757.399131	12.947507
14.148787	760.455069	12.952525
14.029333	766.551539	12.957543
14.038516	773.741948	12.962560
14.080485	774.555875	12.967578
13.900407	771.967805	12.972595
14.359497	755.533953	12.977613
14.302280	772.217603	12.982631
14.019672	765.044473	12.987648
13.971626	766.377328	12.992666
13.937348	768.168773	12.997683
14.402085	770.788212	13.002701
14.328222	770.114900	13.007719
14.319845	775.667075	13.012736
14.419066	769.258134	13.017754
14.317561	771.511313	13.022771
14.265220	769.679660	13.027789
14.238370	780.978106	13.032807
14.202688	778.739927	13.037824
14.242009	780.791305	13.042842
14.095642	782.158404	13.047859
14.345678	766.467126	13.052877
14.123953	787.547062	13.057895
14.225773	780.642265	13.062912
14.549566	773.870163	13.067930
14.371266	763.449346	13.072947
14.397938	771.564810	13.077965
14.406443	774.555076	13.082983
14.542044	775.098812	13.088000
14.478310	773.827493	13.093018
14.122709	779.073980	13.098035
14.328526	774.459819	13.103053
14.365815	777.155279	13.108071
14.069379	774.986100	13.113088
14.266045	777.347485	13.118106
14.444239	780.964564	13.123123
14.851862	787.540694	13.128141
14.455353	787.409907	13.133159
14.454769	779.728971	13.138176
14.604201	780.390471	13.143194
14.268002	789.146248	13.148211
14.463841	799.359181	13.153229
14.782319	803.004914	13.158247
14.803795	802.919498	13.163264
14.588313	808.308275	13.168282
14.732111	801.220215	13.173299
14.708257	800.327682	13.178317
14.795171	796.094935	13.183335
14.943377	797.286787	13.188352
14.906661	803.313585	13.193370
14.831143	790.349020	13.198387
14.600812	777.992376	13.203405
14.730985	771.013743	13.208423
14.754669	784.892006	13.213440
14.891759	788.868926	13.218458
14.857290	792.752642	13.223475
14.715934	786.658854	13.228493
14.998022	803.889291	13.233511
14.382918	789.175269	13.238528
14.630634	786.886653	13.243546
14.782930	798.703156	13.248563
15.051540	792.028000	13.253581
14.924783	787.938973	13.258599
15.047126	792.558800	13.263616
14.985938	794.531157	13.268634
15.109833	796.260109	13.273651
15.070042	791.340211	13.278669
14.719756	794.717693	13.283687
14.951498	801.725144	13.288704
15.080605	797.946562	13.293722
14.849935	802.936926	13.298739
14.802046	792.202306	13.303757
15.004581	799.069140	13.308775
14.816949	798.549236	13.313792
14.987286	798.434331	13.318810
14.933415	800.945178	13.323827
15.098547	799.486749	13.328845
14.849639	805.906337	13.333863
14.692526	799.698237	13.338880
15.156227	802.683905	13.343898
15.389898	819.726241	13.348915
15.109675	813.335338	13.353933
15.318432	822.930908	13.358951
14.999551	821.838163	13.363968
15.342308	811.547624	13.368986
15.216843	823.893371	13.374003
15.482213	816.432935	13.379021
15.371464	811.741824	13.384039
15.084332	821.518741	13.389056
15.313618	813.779910	13.394074
15.196715	819.472069	13.399091
15.816101	818.400492	13.404109
15.202775	812.093010	13.409127
15.030803	814.019504	13.414144
15.684647	820.109198	13.419162
15.238711	828.430812	13.424179
15.367651	821.995135	13.429197
15.628170	825.731946	13.434215
15.579124	819.447055	13.439232
15.709656	808.545793	13.444250
15.137397	817.126904	13.449267
15.437792	808.856310	13.454285
15.809600	819.322716	13.459303
15.322963	816.296389	13.464320
15.466039	812.790177	13.469338
15.324744	821.108536	13.474355
15.341991	825.634284	13.479373
15.945795	820.891876	13.484391
15.599543	828.377482	13.489408
15.514187	818.847853	13.494426
15.405760	819.984991	13.499443
15.668214	816.431790	13.504461
15.445977	814.812772	13.509479
15.207593	817.705789	13.514496
15.905568	817.385660	13.519514
15.566697	822.077304	13.524531
15.508485	827.072381	13.529549
15.484317	815.696598	13.534567
15.413188	818.743450	13.539584
15.850864	819.072902	13.544602
15.587743	824.636354	13.549619
15.560413	821.295523	13.554637
15.535904	828.980337	13.559655
15.635922	833.373283	13.564672
16.164074	833.546642	13.569690
16.330407	833.321910	13.574707
16.093685	826.264684	13.579725
15.823501	816.890062	13.584743
16.019850	811.340117	13.589760
15.827670	813.932458	13.594778
16.239319	819.943099	13.599795
15.757828	820.302057	13.604813
15.877079	815.079687	13.609831
15.783554	820.818698	13.614848
15.927504	811.717261	13.619866
15.816808	806.278239	13.624883
15.891946	820.041223	13.629901
16.235673	837.732298	13.634919
16.287620	840.176183	13.639936
16.071397	823.964173	13.644954
15.506759	832.260090	13.649971
15.883368	838.894715	13.654989
16.159318	842.973101	13.660007
15.813696	841.291242	13.665024
16.021341	840.290082	13.670042
16.091734	838.325707	13.675059
15.786809	847.572091	13.680077
15.867110	842.033894	13.685095
15.795169	846.062307	13.690112
16.011210	842.374319	13.695130
15.827142	852.892580	13.700147
16.611548	857.731227	13.705165
16.634966	867.011703	13.710183
16.740440	855.151818	13.715200
16.407205	846.219332	13.720218
16.312697	833.406012	13.725235
16.332047	834.154037	13.730253
16.337077	841.316719	13.735271
16.129885	845.082175	13.740288
16.614893	839.865965	13.745306
16.335992	842.582263	13.750323
16.691114	841.545518	13.755341
16.637683	838.688418	13.760359
16.148826	843.091003	13.765376
16.591171	841.564164	13.770394
16.510667	841.349463	13.775411
16.357925	841.998054	13.780429
16.441532	843.739595	13.785447
16.405204	842.151588	13.790464
16.382613	835.528065	13.795482
16.407535	838.594679	13.800499
16.339402	849.113821	13.805517
16.811081	852.606327	13.810535
16.677166	866.891034	13.815552
16.521274	854.819385	13.820570
16.736574	856.461530	13.825587
16.250300	865.957060	13.830605
16.764677	864.620970	13.835623
16.579888	857.770235	13.840640
16.779115	865.701089	13.845658
16.546849	858.706271	13.850675
16.765108	864.046467	13.855693
16.774315	856.872045	13.860711
16.914778	865.004548	13.865728
16.875691	857.607277	13.870746
16.878613	862.147888	13.875763
16.734009	859.128259	13.880781
16.750229	860.365910	13.885799
16.611431	864.328999	13.890816
16.817329	864.259049	13.895834
16.929147	859.586920	13.900851
16.834871	862.552179	13.905869
16.950561	857.614366	13.910887
16.756225	868.576036	13.915904
17.013777	863.505684	13.920922
17.222619	864.388305	13.925939
16.552877	853.791493	13.930957
16.972151	859.087767	13.935975
16.596507	858.250004	13.940992
16.678707	861.307703	13.946010
17.014996	855.410917	13.951027
16.575198	865.770191	13.956045
16.929962	863.954036	13.961063
16.844315	882.573521	13.966080
17.233248	881.660895	13.971098
17.140398	891.177232	13.976115
16.860223	885.755105	13.981133
17.453978	884.450836	13.986151
17.334665	888.764338	13.991168
17.407014	888.232355	13.996186
17.461381	890.110994	14.001203
17.122229	878.689540	14.006221
17.729424	870.809796	14.011239
16.989256	866.854126	14.016256
16.877333	857.669431	14.021274
17.519239	867.560494	14.026291
17.412401	877.482936	14.031309
17.409249	879.212742	14.036327
17.344002	870.920156	14.041344
17.192836	874.828370	14.046362
17.237276	882.243702	14.051379
17.666135	889.529759	14.056397
17.815728	881.112201	14.061415
17.383076	867.344827	14.066432
17.452199	859.801322	14.071450
17.406204	857.672034	14.076467
16.902508	869.521294	14.081485
17.102946	888.708454	14.086503
17.311628	885.422381	14.091520
17.615087	883.639458	14.096538
17.516363	886.097341	14.101555
17.527594	885.559095	14.106573
17.225705	880.607398	14.111591
17.280787	890.460456	14.116608
17.559671	897.435359	14.121626
17.717948	891.954432	14.126643
17.330466	904.104349	14.131661
17.708199	891.829673	14.136679
17.513340	890.799663	14.141696
17.510296	889.320075	14.146714
17.673741	897.436392	14.151731
17.814163	913.988420	14.156749
18.209825	902.187461	14.161767
17.803376	899.483143	14.166784
18.128664	888.450526	14.171802
18.000271	884.850870	14.176819
17.761135	893.301258	14.181837
17.806426	881.917774	14.186855
17.622733	886.979740	14.191872
17.725252	880.390369	14.196890
17.744769	885.505901	14.201907
17.756280	883.765278	14.206925
17.692088	894.094489	14.211943
17.587452	900.254968	14.216960
17.599925	904.286030	14.221978
18.136635	901.460110	14.226995
18.245958	906.908796	14.232013
17.979164	914.255837	14.237031
18.191488	907.961778	14.242048
18.020429	910.194246	14.247066
18.134427	912.275037	14.252083
17.896076	927.705806	14.257101
18.126372	916.243004	14.262119
18.238592	907.774450	14.267136
17.965385	919.613102	14.272154
18.266414	907.946792	14.277171
18.106502	912.033097	14.282189
18.033621	910.034217	14.287207
17.931556	917.036883	14.292224
17.909172	918.334197	14.297242
18.378273	897.070380	14.302259
18.292029	913.891223	14.307277
18.361937	920.377975	14.312295
18.200798	906.189609	14.317312
18.149709	906.124958	14.322330
18.190205	899.845032	14.327347
18.660387	907.194088	14.332365
18.088171	903.919144	14.337383
18.175011	909.024200	14.342400
18.200175	911.181937	14.347418
18.368650	911.376584	14.352435
18.312227	914.074032	14.357453
18.113279	920.580554	14.362471
18.593821	926.659399	14.367488
18.447612	937.960750	14.372506
18.645970	928.184921	14.377523
18.589258	934.451557	14.382541
18.587529	942.309595	14.387559
18.355392	922.016446	14.392576
18.608116	932.375230	14.397594
18.952127	927.711112	14.402611
18.770920	939.765823	14.407629
18.244449	935.398176	14.412647
18.756821	925.687065	14.417664
18.436737	932.758394	14.422682
18.559138	924.231444	14.427699
18.436109	932.771068	14.432717
18.573097	936.315701	14.437735
18.668417	934.719811	14.442752
18.536948	935.775340	14.447770
18.786447	922.024788	14.452787
18.870452	924.681439	14.457805
18.958459	929.379230	14.462823
18.909498	926.982157	14.467840
18.691371	937.010319	14.472858
18.805908	928.610820	14.477875
18.656889	931.856008	14.482893
18.555204	933.396038	14.487911
18.823223	928.765841	14.492928
18.623130	938.630254	14.497946
19.034732	948.165908	14.502963
18.994669	955.543936	14.507981
19.125202	947.422799	14.512999
19.218675	939.477846	14.518016
19.438467	937.272453	14.523034
18.903084	930.208038	14.528051
19.141222	928.280650	14.533069
18.908463	926.540186	14.538087
18.857352	931.436359	14.543104
18.917834	944.807254	14.548122
19.476709	942.965624	14.553139
19.056912	945.580800	14.558157
19.187807	944.430642	14.563175
19.397082	948.298531	14.568192
18.987186	943.079616	14.573210
19.308231	949.726090	14.578227
19.166002	951.572230	14.583245
19.186290	949.161216	14.588263
19.587417	952.295505	14.593280
19.106897	944.711313	14.598298
19.416365	947.585322	14.603315
19.596595	961.672874	14.608333
19.785816	949.657879	14.613351
19.455169	925.492190	14.618368
19.173769	934.264751	14.623386
19.260068	934.257603	14.628403
19.438775	940.705333	14.633421
19.694067	944.436671	14.638439
19.675697	938.131183	14.643456
19.317618	938.057526	14.648474
19.655625	938.348852	14.653491
19.475764	938.736586	14.658509
19.514658	942.283871	14.663527
19.510917	951.814768	14.668544
19.605345	959.913457	14.673562
19.599357	962.823962	14.678579
20.036754	943.215481	14.683597
19.587509	940.823926	14.688615
19.674423	938.090122	14.693632
19.504163	946.201614	14.698650
19.614824	950.258424	14.703667
19.203277	945.989644	14.708685
19.164779	953.869190	14.713703
19.522037	950.708292	14.718720
19.339158	950.932398	14.723738
19.313789	948.796732	14.728755
19.854123	959.890220	14.733773
20.034205	969.572384	14.738791
20.075429	962.904165	14.743808
19.972278	969.938578	14.748826
20.074960	961.742878	14.753843
19.802570	956.341607	14.758861
19.406592	964.743866	14.763879
20.081437	958.996302	14.768896
20.227083	968.522884	14.773914
20.193507	979.380698	14.778931
20.068869	968.481199	14.783949
20.099705	966.560838	14.788967
20.055868	975.501555	14.793984
20.017159	980.168596	14.799002
20.245892	976.538564	14.804019
20.273268	963.586255	14.809037
19.884166	976.187746	14.814055
20.439392	967.972074	14.819072
20.161934	967.576602	14.824090
20.346650	960.299074	14.829107
20.296564	956.519957	14.834125
20.062147	962.366155	14.839143
20.318652	945.720678	14.844160
20.063221	958.973516	14.849178
20.211583	965.205078	14.854195
20.453341	967.366967	14.859213
20.546717	970.303027	14.864231
20.704450	965.273434	14.869248
20.075747	946.089709	14.874266
19.903925	951.982961	14.879283
20.284366	964.007045	14.884301
20.393332	966.965923	14.889319
20.860463	969.316781	14.894336
20.554570	965.523843	14.899354
20.483356	975.361898	14.904371
20.958670	967.543670	14.909389
20.866961	976.485530	14.914407
20.259568	949.301824	14.919424
20.263335	967.538254	14.924442
20.383009	966.178406	14.929459
20.261074	965.260111	14.934477
20.100589	977.541991	14.939495
20.437966	972.260367	14.944512
20.424018	975.705434	14.949530
20.251457	975.167400	14.954547
20.654644	974.826896	14.959565
20.779186	985.956736	14.964583
21.026051	981.967280	14.969600
20.671995	980.892625	14.974618
20.700504	970.376371	14.979635
21.023320	989.730776	14.984653
20.999265	982.400539	14.989671
20.758664	971.121469	14.994688
20.699392	974.172813	14.999706
20.879090	992.959379	15.004723
20.935167	989.283644	15.009741
20.998306	994.136799	15.014759
21.411965	982.901021	15.019776
20.940232	981.453374	15.024794
20.919158	976.710388	15.029811
21.497638	967.515971	15.034829
20.661885	969.195542	15.039847
21.070350	961.507643	15.044864
21.006794	972.912910	15.049882
21.229176	993.100293	15.054899
21.410148	990.960897	15.059917
21.003829	984.775754	15.064935
21.245906	979.250195	15.069952
21.368371	973.806376	15.074970
21.380351	970.273208	15.079987
21.336341	963.318464	15.085005
21.402152	961.758723	15.090023
21.195703	963.384494	15.095040
21.465287	965.892339	15.100058
21.120574	972.629854	15.105075
21.355603	966.669903	15.110093
21.278197	970.939032	15.115111
21.192023	966.673235	15.120128
21.107197	983.859990	15.125146
20.897301	996.439904	15.130163
21.530346	995.015903	15.135181
21.505297	990.314557	15.140199
21.297851	992.439094	15.145216
21.332003	990.726493	15.150234
21.552494	995.034451	15.155251
21.691331	990.184514	15.160269
21.560584	997.270571	15.165287
21.682056	989.324392	15.170304
21.697827	996.804195	15.175322
21.683425	1002.439429	15.180339
21.724043	993.136241	15.185357
21.517944	998.978042	15.190375
21.814075	988.783021	15.195392
21.935995	981.221777	15.200410
21.530065	991.354948	15.205427
21.733530	986.330852	15.210445
21.399715	992.858399	15.215463
21.514166	986.772051	15.220480
21.622127	984.047586	15.225498
21.176719	997.696099	15.230515
21.601816	999.703217	15.235533
21.953916	1006.654141	15.240551
22.348204	1012.364599	15.245568
22.124918	1003.850408	15.250586
22.011672	987.262461	15.255603
21.895816	985.084075	15.260621
21.879514	980.627518	15.265639
21.731964	992.042719	15.270656
22.110821	999.122015	15.275674
21.903651	1001.546306	15.280691
21.986051	1004.209530	15.285709
22.453890	1009.854888	15.290727
22.205699	1009.262357	15.295744
22.248901	1005.052146	15.300762
22.100094	1006.583740	15.305779
22.262830	1004.160008	15.310797
22.507955	1009.638074	15.315815
21.968661	990.929521	15.320832
22.469400	993.821094	15.325850
21.959643	1002.165348	15.330867
22.045832	999.387468	15.335885
22.027221	999.977311	15.340903
22.002287	1005.304922	15.345920
22.350807	1004.884568	15.350938
22.109294	1006.537892	15.355955
21.939286	1012.004855	15.360973
22.456193	1005.852684	15.365991
21.998209	1002.335878	15.371008
22.344560	1009.032081	15.376026
22.292391	1021.170896	15.381043
22.577281	1026.835277	15.386061
22.380871	1037.232493	15.391079
22.635364	1036.798376	15.396096
22.655802	1027.678191	15.401114
22.533122	1029.101579	15.406131
23.079873	1025.671328	15.411149
22.851256	1025.252471	15.416167
22.753319	1022.070916	15.421184
22.608228	1007.195172	15.426202
22.568450	1025.754017	15.431219
23.267064	1021.217697	15.436237
22.878862	1030.297264	15.441255
22.492774	1016.557237	15.446272
22.888942	1014.876630	15.451290
22.486719	1022.506730	15.456307
22.942423	1028.273902	15.461325
22.718919	1034.942077	15.466343
22.532938	1038.798943	15.471360
22.972344	1030.358283	15.476378
22.886683	1040.025057	15.481395
23.111830	1035.452000	15.486413
23.054380	1032.721724	15.491431
22.509748	1030.670051	15.496448
23.070776	1032.450885	15.501466
22.345752	1030.007583	15.506483
22.833599	1023.206689	15.511501
22.847008	1023.655850	15.516519
23.053979	1029.575357	15.521536
22.993111	1022.140384	15.526554
22.974481	1035.804528	15.531571
23.304221	1040.461555	15.536589
23.539505	1047.888267	15.541607
23.493432	1037.576088	15.546624
23.356409	1024.728225	15.551642
23.249516	1032.403863	15.556659
23.427920	1026.216027	15.561677
23.521254	1017.485278	15.566695
23.252181	1017.621821	15.571712
23.612217	1009.988778	15.576730
23.652379	1026.174674	15.581747
23.445580	1016.957333	15.586765
23.448622	1024.675810	15.591783
23.457121	1029.603754	15.596800
23.396187	1013.108622	15.601818
23.191854	1024.390675	15.606835
23.467941	1027.787439	15.611853
23.456114	1015.235666	15.616871
23.644232	1019.539203	15.621888
23.742425	1021.821280	15.626906
23.629122	1031.631207	15.631923
23.341648	1024.973117	15.636941
23.597343	1029.831015	15.641959
23.305133	1030.933666	15.646976
23.897002	1033.656425	15.651994
24.059789	1050.580633	15.657011
23.879822	1038.133917	15.662029
23.962631	1026.731875	15.667047
23.588075	1033.521396	15.672064
23.798375	1027.013019	15.677082
23.716025	1045.871998	15.682099
24.055198	1053.465572	15.687117
23.806238	1047.782918	15.692135
23.695403	1051.801654	15.697152
23.716452	1047.657997	15.702170
23.819560	1056.566409	15.707187
23.932920	1051.168165	15.712205
24.044048	1047.881472	15.717223
23.742487	1060.418900	15.722240
23.745253	1047.318885	15.727258
23.880529	1042.756663	15.732275
23.799323	1042.015057	15.737293
23.709338	1043.657415	15.742311
24.020761	1061.871287	15.747328
24.409972	1067.699317	15.752346
24.390314	1066.108694	15.757363
23.950924	1063.649317	15.762381
24.312990	1053.668052	15.767399
24.325760	1066.936017	15.772416
24.528911	1059.554594	15.777434
24.448926	1062.142126	15.782451
24.077422	1064.535208	15.787469
24.112297	1060.521937	15.792487
24.259964	1068.577673	15.797504
24.600588	1058.738598	15.802522
24.573732	1065.130017	15.807539
24.416959	1066.135845	15.812557
24.309384	1055.725935	15.817575
24.555270	1056.697471	15.822592
24.931948	1050.620766	15.827610
24.615024	1068.875673	15.832627
24.779602	1053.582451	15.837645
24.379816	1052.057325	15.842663
24.380224	1061.625505	15.847680
24.797982	1048.615509	15.852698
24.696340	1053.910897	15.857715
24.265187	1062.757329	15.862733
24.940355	1054.475608	15.867751
24.670074	1050.399399	15.872768
25.028936	1050.889449	15.877786
24.964627	1057.387681	15.882803
24.781185	1052.316510	15.887821
25.032514	1047.957120	15.892839
24.717719	1054.475417	15.897856
24.622616	1045.407925	15.902874
24.699446	1050.666057	15.907891
24.936471	1053.330460	15.912909
25.081760	1047.977738	15.917927
25.126020	1054.045660	15.922944
24.900149	1049.628027	15.927962
24.956446	1052.566718	15.932979
24.967627	1058.967992	15.937997
25.262754	1050.578188	15.943015
24.652419	1054.684162	15.948032
24.934469	1053.639848	15.953050
24.986931	1056.553891	15.958067
24.768240	1060.002450	15.963085
25.202776	1063.235698	15.968103
25.080993	1079.961247	15.973120
25.493871	1072.013841	15.978138
25.271704	1070.871308	15.983155
25.302659	1064.226740	15.988173
25.694893	1065.083974	15.993191
25.291797	1072.310293	15.998208
25.225877	1074.977686	16.003226
25.840792	1072.227925	16.008243
25.615740	1073.648322	16.013261
25.345227	1056.570406	16.018279
25.513935	1074.052285	16.023296
25.322653	1070.553899	16.028314
25.389404	1078.871544	16.033331
25.806212	1080.804224	16.038349
25.772455	1065.308346	16.043367
25.367707	1074.557766	16.048384
25.495683	1071.558776	16.053402
25.098118	1073.709768	16.058419
24.952778	1081.766949	16.063437
25.569626	1073.011468	16.068455
25.468065	1076.861510	16.073472
25.380770	1081.671840	16.078490
25.866568	1093.730101	16.083507
25.787418	1101.272063	16.088525
25.816872	1095.277806	16.093543
25.910518	1102.594052	16.098560
25.876243	1095.827086	16.103578
26.239460	1086.331613	16.108595
26.119863	1091.629807	16.113613
26.177916	1087.423576	16.118631
26.041903	1099.480825	16.123648
26.287790	1088.911722	16.128666
26.073609	1078.635160	16.133683
25.879960	1070.466612	16.138701
25.960766	1081.237253	16.143719
26.360884	1084.709390	16.148736
26.239643	1082.181541	16.153754
26.597606	1081.485164	16.158771
26.276171	1084.179718	16.163789
26.159309	1063.704359	16.168807
26.249863	1072.930310	16.173824
25.938437	1076.125071	16.178842
26.452302	1083.773509	16.183859
26.384799	1080.202202	16.188877
26.533247	1082.637407	16.193895
26.108054	1078.276046	16.198912
26.116524	1081.764980	16.203930
26.236484	1078.129772	16.208947
26.385584	1087.595921	16.213965
26.415670	1085.681975	16.218983
26.261602	1088.325225	16.224000
26.494326	1088.910653	16.229018
26.604004	1083.825393	16.234035
26.658835	1087.988755	16.239053
26.697815	1082.605238	16.244071
26.697676	1082.153962	16.249088
26.567968	1079.034147	16.254106
26.705774	1081.597239	16.259123
26.457403	1093.110252	16.264141
26.089249	1084.306156	16.269159
26.324168	1088.195330	16.274176
26.260861	1105.937423	16.279194
26.573626	1118.697976	16.284211
26.661752	1118.034142	16.289229
26.936271	1107.908690	16.294247
26.679969	1107.285860	16.299264
26.824217	1116.197364	16.304282
26.930134	1110.087056	16.309299
27.036138	1120.045921	16.314317
27.098985	1107.321511	16.319335
27.264011	1117.211225	16.324352
27.111112	1111.743966	16.329370
27.031273	1106.129635	16.334387
26.896217	1106.866999	16.339405
27.448416	1111.372646	16.344423
27.071452	1105.653100	16.349440
26.857138	1107.822900	16.354458
26.965625	1111.318357	16.359475
26.730339	1113.330480	16.364493
27.043446	1126.475989	16.369511
27.414295	1126.083714	16.374528
27.401869	1129.048896	16.379546
27.494785	1125.645105	16.384563
27.149715	1138.634326	16.389581
27.537286	1127.453011	16.394599
27.590454	1125.750059	16.399616
27.070766	1132.559058	16.404634
27.479199	1126.458448	16.409651
27.457037	1132.224318	16.414669
27.855924	1126.194621	16.419687
27.794526	1128.791891	16.424704
27.645820	1134.388118	16.429722
27.548893	1132.386646	16.434739
27.688768	1130.171581	16.439757
27.729926	1122.569204	16.444775
28.004739	1128.743266	16.449792
27.706711	1129.925723	16.454810
28.278189	1119.602551	16.459827
27.986308	1126.016321	16.464845
27.702390	1127.619455	16.469863
28.450488	1121.181942	16.474880
28.209105	1111.446077	16.479898
28.309801	1097.614418	16.484915
27.667444	1104.619229	16.489933
27.768738	1104.549786	16.494951
27.878086	1096.280403	16.499968
27.721650	1099.810795	16.504986
28.110179	1098.898221	16.510003
27.796131	1110.535078	16.515021
27.855779	1120.239232	16.520039
28.234654	1121.537201	16.525056
27.789826	1130.575142	16.530074
27.924385	1121.254105	16.535091
28.061672	1130.412850	16.540109
28.405733	1128.888668	16.545127
27.938985	1134.319819	16.550144
27.733518	1126.702190	16.555162
28.089706	1127.637623	16.560179
28.213288	1121.461445	16.565197
27.840200	1121.238646	16.570215
27.962879	1139.523010	16.575232
27.971873	1147.306886	16.580250
28.517145	1150.071632	16.585267
28.670120	1152.433559	16.590285
28.637760	1150.598756	16.595303
28.872261	1149.558684	16.600320
28.716965	1147.386419	16.605338
28.609057	1148.539276	16.610355
28.835096	1155.446770	16.615373
28.541291	1147.969117	16.620391
29.264789	1143.078602	16.625408
28.821909	1152.917818	16.630426
28.878015	1141.068585	16.635443
28.702275	1122.508415	16.640461
28.570357	1128.509120	16.645479
28.779411	1140.320169	16.650496
28.220738	1152.853512	16.655514
28.636700	1150.933128	16.660531
28.903170	1142.377330	16.665549
28.363696	1148.785477	16.670567
28.492368	1140.980120	16.675584
28.573333	1149.724770	16.680602
28.931374	1161.061360	16.685619
29.041622	1174.288982	16.690637
29.229899	1171.233250	16.695655
29.496672	1163.355888	16.700672
29.090494	1167.755147	16.705690
29.238405	1164.001962	16.710707
29.409471	1167.370924	16.715725
29.355454	1157.769962	16.720743
29.306059	1142.771908	16.725760
29.320756	1151.974997	16.730778
29.194793	1144.354450	16.735795
29.211854	1151.606901	16.740813
29.671564	1169.056188	16.745831
29.549199	1150.819034	16.750848
29.333926	1151.269091	16.755866
29.014043	1150.208038	16.760883
29.526003	1156.768061	16.765901
29.403794	1167.286343	16.770919
29.597516	1167.445505	16.775936
29.306193	1162.908647	16.780954
29.094804	1173.330365	16.785971
29.395665	1172.077990	16.790989
29.556249	1173.971680	16.796007
29.506899	1159.311273	16.801024
29.358456	1166.942946	16.806042
29.510284	1173.735770	16.811059
29.847536	1180.704853	16.816077
29.856056	1192.430396	16.821095
30.165404	1193.657145	16.826112
30.080106	1182.928113	16.831130
29.564068	1174.513069	16.836147
29.735978	1176.408150	16.841165
29.705731	1177.186003	16.846183
30.374650	1182.080591	16.851200
30.155686	1190.764662	16.856218
30.334929	1183.765605	16.861235
29.977470	1177.708485	16.866253
29.785374	1166.424895	16.871271
30.307390	1172.967580	16.876288
30.283905	1194.843946	16.881306
30.368973	1186.407889	16.886323
29.945526	1177.252597	16.891341
30.337756	1190.534157	16.896359
30.477812	1183.471773	16.901376
30.424841	1182.678428	16.906394
30.185570	1171.064511	16.911411
30.253117	1170.741549	16.916429
30.009468	1177.289838	16.921447
30.415517	1180.243522	16.926464
30.338755	1193.689622	16.931482
30.700794	1182.505936	16.936499
30.563837	1184.688947	16.941517
30.230112	1188.868649	16.946535
30.706426	1183.802015	16.951552
30.314260	1183.680015	16.956570
30.642521	1185.124724	16.961587
30.609811	1180.355093	16.966605
30.400702	1185.572579	16.971623
30.465836	1188.153313	16.976640
30.505909	1181.652448	16.981658
30.251260	1179.637658	16.986675
30.498042	1189.943869	16.991693
30.380059	1203.977059	16.996711
30.725554	1204.295626	17.001728
30.446115	1214.030534	17.006746
30.596566	1209.901406	17.011763
30.721058	1206.398010	17.016781
30.579396	1212.220381	17.021799
30.948430	1212.267041	17.026816
31.225800	1231.073365	17.031834
31.311944	1223.265126	17.036851
31.729095	1217.699612	17.041869
31.314933	1211.127449	17.046887
31.144579	1207.010399	17.051904
31.317521	1207.699813	17.056922
31.184874	1191.644868	17.061939
31.629557	1181.666448	17.066957
31.372290	1192.578156	17.071975
31.463999	1184.967881	17.076992
31.471869	1197.349931	17.082010
30.955241	1189.682892	17.087027
31.383965	1192.812928	17.092045
31.250791	1197.046612	17.097063
31.451157	1190.549189	17.102080
31.618784	1198.876430	17.107098
31.528687	1219.756503	17.112115
32.068925	1213.802599	17.117133
31.581880	1210.012566	17.122151
32.035057	1197.795361	17.127168
31.919522	1187.481286	17.132186
31.831991	1190.407680	17.137203
31.768456	1190.651077	17.142221
31.534197	1191.665820	17.147239
31.642983	1182.172040	17.152256
31.599928	1183.986983	17.157274
31.668891	1196.649853	17.162291
31.894701	1205.946332	17.167309
31.687107	1202.573536	17.172327
31.822122	1211.792637	17.177344
31.761561	1210.363003	17.182362
31.996370	1202.945034	17.187379
32.009117	1213.268763	17.192397
31.842500	1211.719943	17.197415
31.953012	1211.387134	17.202432
32.078464	1215.369118	17.207450
31.847622	1224.509489	17.212467
31.807446	1212.870858	17.217485
32.024374	1221.124162	17.222503
32.498505	1231.546478	17.227520
32.237728	1237.507323	17.232538
32.021718	1237.714500	17.237555
32.400698	1241.597056	17.242573
32.370732	1243.735015	17.247591
32.865732	1234.007507	17.252608
32.869436	1235.486973	17.257626
32.485971	1223.513622	17.262643
32.728325	1208.700460	17.267661
32.544051	1217.032007	17.272679
32.208154	1214.648012	17.277696
32.706462	1224.804630	17.282714
32.602393	1228.746613	17.287731
32.873315	1221.985730	17.292749
32.794396	1225.210589	17.297767
32.724842	1215.905503	17.302784
32.852594	1229.395527	17.307802
32.683967	1233.789374	17.312819
32.313682	1233.711303	17.317837
32.759170	1238.372452	17.322855
32.675112	1237.770136	17.327872
32.838386	1230.442188	17.332890
32.862227	1236.103100	17.337907
32.990520	1233.763594	17.342925
32.798712	1231.944140	17.347943
33.217352	1233.665115	17.352960
33.088690	1238.276801	17.357978
33.006316	1228.109018	17.362995
32.948786	1228.951081	17.368013
33.082804	1231.404332	17.373031
32.864444	1240.369199	17.378048
33.024563	1247.043996	17.383066
33.317881	1263.884968	17.388083
33.211340	1261.228572	17.393101
33.199625	1262.770402	17.398119
33.232931	1256.769179	17.403136
33.445687	1259.904450	17.408154
33.655312	1254.128239	17.413171
33.891094	1252.248521	17.418189
33.522667	1262.770481	17.423207
33.499983	1253.335002	17.428224
33.724947	1259.627324	17.433242
33.583504	1260.305728	17.438259
33.630759	1256.968982	17.443277
33.524665	1253.419427	17.448295
33.322694	1256.963251	17.453312
33.692956	1255.204605	17.458330
33.412498	1260.770891	17.463347
33.654029	1257.864643	17.468365
33.924971	1281.415185	17.473383
33.737672	1271.216376	17.478400
34.049337	1272.095633	17.483418
34.026417	1272.963867	17.488435
34.152837	1270.738257	17.493453
33.925101	1274.516468	17.498471
33.886331	1277.378480	17.503488
34.393916	1268.134987	17.508506
34.089921	1271.401209	17.513523
33.970452	1270.021767	17.518541
34.025720	1274.383920	17.523559
34.256033	1276.389840	17.528576
34.413501	1271.912467	17.533594
34.368592	1272.304443	17.538611
34.332473	1277.343543	17.543629
34.328049	1278.836902	17.548647
34.329580	1270.985011	17.553664
34.617349	1267.935863	17.558682
34.500165	1270.535528	17.563699
34.773854	1274.273539	17.568717
34.627010	1267.587151	17.573735
34.691061	1256.304647	17.578752
34.611888	1257.901161	17.583770
34.389542	1277.400718	17.588787
34.438543	1270.144195	17.593805
34.284153	1276.624974	17.598823
34.151876	1274.146153	17.603840
34.380152	1276.165013	17.608858
34.158386	1297.283427	17.613875
34.705460	1291.991152	17.618893
34.950232	1299.063042	17.623911
34.478886	1299.341533	17.628928
34.593737	1300.163071	17.633946
34.697914	1297.328695	17.638963
34.905237	1287.608079	17.643981
34.935796	1296.291221	17.648999
35.168412	1305.021804	17.654016
35.401704	1302.997301	17.659034
35.081202	1291.399108	17.664051
35.255607	1292.801509	17.669069
35.111363	1293.309938	17.674087
35.157701	1303.991406	17.679104
35.690765	1305.350590	17.684122
35.038497	1307.976766	17.689139
35.541428	1305.055057	17.694157
35.682606	1304.092623	17.699175
35.347926	1308.240943	17.704192
35.635474	1301.575271	17.709210
35.155384	1301.810942	17.714227
35.522654	1299.203846	17.719245
35.322418	1310.602207	17.724263
35.581690	1307.484906	17.729280
35.699650	1308.501621	17.734298
35.852194	1311.097165	17.739315
36.047973	1310.148321	17.744333
35.868868	1306.212491	17.749351
35.793502	1311.519644	17.754368
36.160951	1288.254628	17.759386
36.128312	1303.858822	17.764403
35.957208	1306.148150	17.769421
35.870790	1304.066128	17.774439
35.820196	1296.806165	17.779456
36.079984	1294.152689	17.784474
36.163665	1311.578611	17.789491
35.966648	1305.209289	17.794509
35.872569	1307.335147	17.799527
35.752271	1303.336514	17.804544
36.278191	1298.470408	17.809562
36.132716	1302.292622	17.814579
36.124026	1304.196902	17.819597
36.163012	1306.286263	17.824615
36.320676	1304.197795	17.829632
36.663191	1296.176039	17.834650
36.167982	1298.004588	17.839667
36.429197	1292.927233	17.844685
36.684442	1296.156881	17.849703
35.875855	1299.154532	17.854720
36.288280	1310.968745	17.859738
36.369424	1318.507932	17.864755
36.485421	1333.498874	17.869773
36.747225	1324.893223	17.874791
36.838274	1320.530320	17.879808
36.878863	1324.755915	17.884826
36.965021	1325.689220	17.889843
36.393167	1322.859109	17.894861
36.877124	1324.550988	17.899879
36.991119	1330.721757	17.904896
36.942775	1320.457104	17.909914
37.044930	1316.111408	17.914931
36.836086	1324.629867	17.919949
36.904536	1321.438132	17.924967
36.736448	1339.708012	17.929984
36.964875	1325.831043	17.935002
36.861343	1326.342601	17.940019
36.751369	1321.572339	17.945037
36.927923	1308.208388	17.950055
36.572520	1325.797363	17.955072
37.153667	1333.164034	17.960090
37.057832	1337.088980	17.965107
37.350431	1339.564893	17.970125
37.397350	1340.321271	17.975143
37.258418	1344.521172	17.980160
37.551147	1334.339108	17.985178
37.355145	1343.890682	17.990195
37.434892	1340.545706	17.995213
37.726999	1326.052905	18.000231
37.492841	1343.092843	18.005248
37.620878	1332.936422	18.010266
37.656409	1335.310347	18.015283
37.419044	1341.879808	18.020301
37.607839	1341.010944	18.025319
37.471778	1340.751238	18.030336
37.510202	1339.476596	18.035354
37.957108	1353.721755	18.040371
37.807021	1361.208599	18.045389
38.320617	1365.398429	18.050407
37.915875	1366.887850	18.055424
38.059898	1359.812157	18.060442
38.134765	1361.312112	18.065459
38.028317	1357.396517	18.070477
38.318674	1351.320527	18.075495
37.931327	1357.985929	18.080512
38.108036	1353.290944	18.085530
38.153379	1357.840856	18.090547
38.297794	1356.180481	18.095565
38.478390	1350.336175	18.100583
38.606857	1358.770574	18.105600
38.248586	1353.878016	18.110618
38.323460	1356.861202	18.115635
38.155018	1350.616803	18.120653
38.313742	1359.235840	18.125671
38.221477	1370.128278	18.130688
38.187107	1356.064982	18.135706
38.400549	1367.884967	18.140723
38.550788	1384.499021	18.145741
38.911500	1383.265716	18.150759
38.512617	1389.705707	18.155776
38.715598	1384.403862	18.160794
38.586256	1372.842126	18.165811
38.391115	1386.013311	18.170829
38.616019	1377.047305	18.175847
38.705958	1389.012765	18.180864
38.679412	1380.676046	18.185882
38.656033	1385.454416	18.190899
38.721517	1394.179506	18.195917
38.950011	1396.201502	18.200935
38.908340	1400.373650	18.205952
39.326195	1390.654913	18.210970
39.677891	1392.282184	18.215987
39.523433	1394.616269	18.221005
39.604683	1389.762567	18.226023
39.733006	1390.364261	18.231040
40.050586	1384.776329	18.236058
39.821018	1365.488980	18.241075
39.461363	1370.199781	18.246093
39.829101	1363.253357	18.251111
39.374052	1368.102087	18.256128
39.668892	1362.681805	18.261146
39.710967	1359.876023	18.266163
39.730521	1360.860725	18.271181
40.071384	1360.217493	18.276199
40.101245	1364.956010	18.281216
40.053566	1365.114889	18.286234
40.134740	1359.131426	18.291251
39.709232	1349.566109	18.296269
39.787179	1345.549224	18.301287
39.805230	1359.160568	18.306304
39.910907	1361.024956	18.311322
39.929623	1368.602287	18.316339
39.840795	1373.687491	18.321357
40.194211	1370.378795	18.326375
40.123671	1369.237882	18.331392
39.659495	1363.484493	18.336410
40.197178	1366.960514	18.341427
40.168358	1356.973668	18.346445
40.096741	1361.406091	18.351463
39.979010	1365.946681	18.356480
40.187601	1358.191901	18.361498
40.243132	1363.099991	18.366515
39.650914	1371.697097	18.371533
40.205352	1379.920017	18.376551
40.366232	1387.437352	18.381568
40.224570	1391.107512	18.386586
40.418849	1387.397554	18.391603
40.213767	1391.591988	18.396621
40.453790	1388.086348	18.401639
40.420186	1394.078147	18.406656
40.697416	1404.218796	18.411674
40.669382	1406.337538	18.416691
40.542559	1422.862220	18.421709
40.859533	1419.559190	18.426727
40.701864	1424.680373	18.431744
40.876436	1421.270124	18.436762
40.995453	1412.913881	18.441779
40.331599	1424.141500	18.446797
40.860941	1418.227095	18.451815
40.824932	1417.058711	18.456832
41.009293	1434.683675	18.461850
41.432218	1435.564552	18.466867
41.057025	1444.200487	18.471885
41.372835	1444.507902	18.476903
41.313689	1444.731683	18.481920
41.023405	1443.423005	18.486938
41.160755	1440.933738	18.491955
41.422847	1449.290571	18.496973
41.583612	1443.360959	18.501991
41.366854	1439.058575	18.507008
41.241132	1449.962582	18.512026
41.728359	1441.719412	18.517043
41.283948	1441.312051	18.522061
41.657577	1437.981261	18.527079
41.872356	1432.387229	18.532096
41.519793	1429.532426	18.537114
41.459057	1435.926097	18.542131
41.629809	1455.333087	18.547149
41.925735	1456.511452	18.552167
42.328612	1463.722896	18.557184
42.138468	1466.251897	18.562202
42.342360	1457.639419	18.567219
42.253681	1454.087113	18.572237
41.961017	1433.812271	18.577255
41.992352	1433.466539	18.582272
41.856806	1438.581126	18.587290
42.316813	1451.012878	18.592307
42.130509	1454.409133	18.597325
42.130905	1455.239031	18.602343
41.942367	1447.501863	18.607360
41.925033	1452.159388	18.612378
42.232538	1446.210085	18.617395
42.203937	1449.035827	18.622413
42.167171	1456.861677	18.627431
42.008527	1454.525791	18.632448
42.552292	1467.866017	18.637466
43.094925	1469.365737	18.642483
42.901772	1484.963521	18.647501
42.466837	1472.865469	18.652519
42.622962	1473.011553	18.657536
42.502099	1467.141561	18.662554
42.918626	1468.856576	18.667571
42.526370	1481.263251	18.672589
42.906550	1471.888010	18.677607
43.187650	1475.362976	18.682624
42.631870	1479.889746	18.687642
43.453937	1471.613364	18.692659
42.923396	1483.583975	18.697677
43.488209	1475.779995	18.702695
43.314890	1473.509508	18.707712
43.288379	1475.359776	18.712730
43.434925	1465.809473	18.717747
43.182320	1478.693024	18.722765
42.879428	1471.390221	18.727783
43.303020	1470.519508	18.732800
42.944580	1470.862473	18.737818
43.493503	1470.685465	18.742835
44.013518	1480.450683	18.747853
43.313807	1475.952082	18.752871
43.388651	1478.572372	18.757888
43.724812	1493.756390	18.762906
43.888078	1486.889091	18.767923
43.900882	1486.842892	18.772941
43.813550	1487.007946	18.777959
44.011758	1485.493819	18.782976
43.915961	1498.100504	18.787994
44.367806	1474.926248	18.793011
44.441619	1476.615727	18.798029
44.212994	1463.766029	18.803047
43.943142	1468.608043	18.808064
43.672755	1458.702932	18.813082
43.976272	1467.147999	18.818099
44.307976	1483.342568	18.823117
44.340494	1487.897666	18.828135
44.158311	1474.497926	18.833152
44.138901	1487.367267	18.838170
44.019462	1488.480915	18.843187
44.298421	1491.539648	18.848205
44.083812	1491.266921	18.853223
44.180565	1486.619065	18.858240
44.210707	1494.642799	18.863258
44.415397	1488.286607	18.868275
44.443137	1490.002196	18.873293
44.749742	1501.463779	18.878311
44.938325	1505.521207	18.883328
44.668579	1505.446415	18.888346
44.873017	1506.007860	18.893363
44.825993	1502.288111	18.898381
44.829198	1506.263947	18.903399
44.972975	1504.392215	18.908416
44.678236	1507.922129	18.913434
44.764747	1501.742125	18.918451
44.614434	1508.389613	18.923469
44.877602	1510.756522	18.928487
45.075997	1513.572178	18.933504
44.783301	1511.733689	18.938522
45.045513	1501.691982	18.943539
45.197951	1516.055703	18.948557
45.356279	1531.037064	18.953575
45.447202	1528.857975	18.958592
44.988336	1531.267875	18.963610
45.159903	1523.616620	18.968627
45.576312	1527.076841	18.973645
45.175601	1527.527376	18.978663
45.188074	1520.661450	18.983680
45.504763	1533.759366	18.988698
45.691298	1525.670273	18.993715
45.772550	1528.513638	18.998733
45.447689	1535.002118	19.003751
45.684217	1538.285217	19.008768
45.419092	1554.402360	19.013786
45.559340	1560.657485	19.018803
46.050644	1555.184465	19.023821
46.034766	1551.156895	19.028839
46.264971	1549.347443	19.033856
46.122418	1545.386934	19.038874
46.116440	1553.195410	19.043891
46.104547	1555.945982	19.048909
45.772722	1550.500134	19.053927
46.129351	1548.270206	19.058944
46.222182	1548.902678	19.063962
46.334940	1543.024690	19.068979
46.286599	1544.717415	19.073997
46.330520	1569.001125	19.079015
46.638239	1576.104352	19.084032
46.931420	1572.741881	19.089050
46.649587	1560.500009	19.094067
46.517267	1559.797898	19.099085
46.561988	1571.795768	19.104103
46.676841	1563.651546	19.109120
46.643391	1574.676964	19.114138
46.883803	1576.394163	19.119155
46.443824	1567.739868	19.124173
46.632170	1576.764659	19.129191
46.750119	1566.915792	19.134208
46.460007	1572.515237	19.139226
46.465627	1587.905436	19.144243
46.917099	1595.412329	19.149261
46.796501	1593.496542	19.154279
47.045892	1585.164103	19.159296
47.493863	1602.669294	19.164314
47.214925	1598.528033	19.169331
47.402202	1596.652675	19.174349
47.080606	1594.682975	19.179367
47.510573	1594.761177	19.184384
47.269360	1590.620356	19.189402
47.486413	1607.637633	19.194419
47.827129	1612.444584	19.199437
47.813674	1610.625725	19.204455
47.640409	1592.635889	19.209472
47.816151	1598.229083	19.214490
48.042757	1595.498677	19.219507
47.898744	1591.036604	19.224525
47.793692	1584.744383	19.229543
48.112004	1587.339406	19.234560
47.881366	1595.391165	19.239578
48.179298	1608.179626	19.244595
48.319800	1608.801522	19.249613
48.094491	1592.303043	19.254631
48.025069	1586.140976	19.259648
47.738628	1599.784132	19.264666
48.015782	1610.524523	19.269683
48.018190	1612.673265	19.274701
48.105508	1611.722356	19.279719
47.978542	1606.724286	19.284736
48.257502	1615.349974	19.289754
48.142219	1616.481918	19.294771
48.418065	1609.319328	19.299789
48.372388	1629.621754	19.304807
48.413893	1633.945112	19.309824
48.620682	1631.949946	19.314842
48.805642	1639.627743	19.319859
49.266516	1631.549539	19.324877
49.201017	1624.380127	19.329895
49.551890	1619.140395	19.334912
49.534087	1597.374032	19.339930
49.164876	1596.153371	19.344947
49.769630	1578.610469	19.349965
49.282270	1583.268625	19.354983
49.608906	1586.745991	19.360000
49.523620	1596.495060	19.365018
49.289683	1566.468797	19.370035
49.284039	1561.212005	19.375053
49.051912	1568.178371	19.380071
49.453461	1581.282045	19.385088
49.346156	1583.129124	19.390106
49.342008	1594.329876	19.395123
49.664496	1572.759873	19.400141
49.698811	1586.119546	19.405159
49.773699	1588.228597	19.410176
49.379467	1588.741241	19.415194
49.353481	1586.760231	19.420211
49.782787	1578.125223	19.425229
49.867422	1596.434915	19.430247
49.793611	1591.141390	19.435264
49.856910	1592.273931	19.440282
49.803463	1584.727112	19.445299
49.964342	1584.780937	19.450317
49.857748	1590.976673	19.455335
49.918264	1596.821340	19.460352
49.975822	1592.551950	19.465370
49.848037	1604.576701	19.470387
49.986888	1602.519531	19.475405
49.873658	1602.533981	19.480423
50.330367	1598.088832	19.485440
50.089891	1601.017014	19.490458
50.072462	1598.596006	19.495475
50.366316	1604.798829	19.500493
50.328572	1618.854566	19.505511
50.423945	1621.888255	19.510528
50.708464	1617.264780	19.515546
50.803400	1617.111117	19.520563
50.791732	1620.909411	19.525581
50.786784	1620.244271	19.530599
50.769627	1623.049323	19.535616
50.775976	1614.751554	19.540634
50.493831	1615.518151	19.545651
51.235470	1615.765582	19.550669
51.085722	1623.195678	19.555687
50.702265	1619.894365	19.560704
50.731680	1623.818809	19.565722
50.312287	1632.540612	19.570739
51.112774	1646.330161	19.575757
51.004621	1645.169839	19.580775
51.503041	1647.506450	19.585792
51.554012	1642.733135	19.590810
51.381656	1658.826460	19.595827
51.760856	1642.041308	19.600845
51.696111	1648.325224	19.605863
51.311690	1655.072334	19.610880
51.626488	1645.467336	19.615898
51.329460	1646.501344	19.620915
51.652693	1643.967329	19.625933
51.871833	1656.607144	19.630951
51.650545	1670.530550	19.635968
51.914215	1660.371759	19.640986
52.099346	1661.302296	19.646003
52.106414	1656.482162	19.651021
52.112360	1661.388587	19.656039
52.062609	1665.470535	19.661056
52.169605	1665.993507	19.666074
52.419065	1668.652911	19.671091
52.234351	1657.093299	19.676109
52.208261	1661.092666	19.681127
52.683820	1661.065938	19.686144
52.679398	1652.081850	19.691162
52.339748	1659.696165	19.696179
52.349169	1658.508069	19.701197
52.430425	1657.715895	19.706215
51.905170	1654.360912	19.711232
52.858434	1653.735934	19.716250
52.579133	1664.626113	19.721267
52.946275	1656.571959	19.726285
52.677107	1658.097101	19.731303
52.639695	1664.648172	19.736320
52.647381	1663.081641	19.741338
52.461492	1680.590922	19.746355
52.976046	1689.571294	19.751373
53.523960	1686.554157	19.756391
53.068875	1687.133083	19.761408
53.503095	1679.159995	19.766426
53.092223	1688.997678	19.771443
53.242242	1681.706324	19.776461
52.968552	1687.145453	19.781479
52.879374	1686.720648	19.786496
53.331512	1690.146936	19.791514
53.366937	1715.183266	19.796531
53.593333	1720.582416	19.801549
53.509266	1710.146371	19.806567
53.665559	1711.258129	19.811584
53.943934	1712.306697	19.816602
53.700938	1707.869474	19.821619
53.740949	1704.066703	19.826637
53.785169	1698.688495	19.831655
53.593108	1708.233339	19.836672
53.917085	1699.942883	19.841690
53.779652	1716.299072	19.846707
54.015307	1724.341406	19.851725
54.057264	1731.823753	19.856743
53.964109	1734.435523	19.861760
54.035240	1731.663029	19.866778
53.958021	1733.183539	19.871795
54.068952	1724.342404	19.876813
54.306516	1731.560761	19.881831
54.250156	1739.026858	19.886848
54.624720	1748.625517	19.891866
54.534196	1750.034488	19.896883
54.811893	1752.014150	19.901901
54.562660	1751.497496	19.906919
54.892403	1760.749680	19.911936
54.874866	1755.551489	19.916954
54.939253	1759.429491	19.921971
55.081275	1743.126151	19.926989
54.742885	1746.716558	19.932007
54.924885	1743.440795	19.937024
55.185162	1744.993968	19.942042
54.919732	1750.365557	19.947059
55.025853	1752.854783	19.952077
55.243100	1748.768781	19.957095
54.960776	1745.391736	19.962112
55.483363	1742.167090	19.967130
55.199133	1747.945558	19.972147
55.386893	1764.999105	19.977165
55.493718	1770.142324	19.982183
55.502681	1782.054383	19.987200
56.038014	1773.005132	19.992218
55.760270	1772.436109	19.997235
55.423933	1776.193464	20.002253
55.793693	1769.325465	20.007271
55.621015	1776.011250	20.012288
55.808363	1774.224227	20.017306
56.031156	1764.605088	20.022323
56.171213	1768.266178	20.027341
56.349425	1770.217148	20.032359
56.309419	1775.541024	20.037376
56.352321	1763.608224	20.042394
55.757567	1770.337630	20.047411
55.669577	1776.296999	20.052429
55.860128	1774.515789	20.057447
55.892252	1792.474087	20.062464
56.205786	1795.461215	20.067482
56.269552	1791.389632	20.072499
56.449424	1801.990646	20.077517
56.682308	1790.359618	20.082535
56.341921	1796.014298	20.087552
56.349987	1798.177960	20.092570
56.587640	1816.767020	20.097587
56.918186	1817.365646	20.102605
57.059108	1820.152429	20.107623
56.869358	1819.512899	20.112640
57.074399	1823.381639	20.117658
56.996506	1814.917007	20.122675
57.097507	1813.755669	20.127693
57.155831	1805.392913	20.132711
56.691204	1820.765007	20.137728
57.493087	1814.290473	20.142746
57.015977	1823.630442	20.147763
57.182996	1830.654689	20.152781
57.477276	1838.807872	20.157799
57.417924	1838.362639	20.162816
57.712705	1838.673337	20.167834
57.669014	1844.313396	20.172851
57.759626	1842.128006	20.177869
57.649108	1835.000234	20.182887
57.644038	1830.516469	20.187904
57.852542	1837.723613	20.192922
57.656171	1839.635079	20.197939
57.750430	1835.713377	20.202957
58.013610	1847.071488	20.207975
58.036443	1859.457979	20.212992
58.371979	1857.777269	20.218010
58.355874	1857.195911	20.223027
58.373751	1856.836487	20.228045
58.552787	1851.800172	20.233063
58.384474	1861.934709	20.238080
58.264077	1858.532432	20.243098
58.631739	1861.003044	20.248115
58.573461	1862.470121	20.253133
58.389731	1856.840170	20.258151
58.196742	1860.963399	20.263168
58.450840	1852.011546	20.268186
58.713794	1858.052005	20.273203
58.894771	1880.983010	20.278221
59.078591	1882.412396	20.283239
59.102069	1881.111640	20.288256
58.820523	1879.586966	20.293274
59.143068	1883.156549	20.298291
59.271104	1885.427779	20.303309
59.287798	1881.877917	20.308327
59.092435	1883.909156	20.313344
59.024212	1883.036100	20.318362
59.290776	1881.643846	20.323379
59.222179	1886.221100	20.328397
59.436217	1871.033090	20.333415
59.139346	1877.927603	20.338432
59.105003	1882.827738	20.343450
60.100543	1886.431399	20.348467
60.364359	1889.470467	20.353485
60.454251	1877.397727	20.358503
59.934920	1875.831178	20.363520
60.163775	1862.433423	20.368538
60.116228	1862.958370	20.373555
60.307604	1864.241407	20.378573
60.211410	1860.952129	20.383591
59.986580	1871.041821	20.388608
60.256058	1857.410520	20.393626
60.203422	1862.985704	20.398643
60.144286	1863.389376	20.403661
60.670334	1874.005966	20.408679
60.703460	1873.076104	20.413696
60.542268	1868.108536	20.418714
60.510446	1876.088439	20.423731
60.426638	1883.726134	20.428749
61.022372	1875.532146	20.433767
60.808022	1885.178387	20.438784
61.059656	1892.489296	20.443802
60.745241	1883.165179	20.448819
60.382420	1891.777310	20.453837
60.474826	1885.151273	20.458855
60.357220	1880.868059	20.463872
60.861281	1893.135466	20.468890
61.104458	1912.017265	20.473907
60.838477	1914.839012	20.478925
61.315062	1903.185747	20.483943
61.348455	1907.065451	20.488960
60.969021	1910.851634	20.493978
61.539037	1917.544918	20.498995
61.418042	1939.917079	20.504013
61.803484	1941.895767	20.509031
61.813141	1940.878035	20.514048
61.748967	1929.766554	20.519066
61.821248	1937.954347	20.524083
62.106866	1929.458311	20.529101
62.526503	1924.826344	20.534119
62.126230	1918.343275	20.539136
61.943467	1921.032142	20.544154
62.395440	1928.466513	20.549171
62.147877	1923.521845	20.554189
62.113827	1930.186103	20.559207
62.248381	1926.049817	20.564224
62.508202	1928.963277	20.569242
62.075151	1916.640559	20.574259
62.050797	1923.577869	20.579277
62.556276	1916.344689	20.584295
62.375917	1918.499832	20.589312
61.964588	1927.716001	20.594330
62.294322	1933.165400	20.599347
62.126730	1937.789640	20.604365
62.522810	1939.870816	20.609383
62.304319	1951.597487	20.614400
62.614783	1969.294868	20.619418
63.058040	1964.454078	20.624435
62.717138	1966.198705	20.629453
62.638538	1970.900619	20.634471
63.232157	1969.943450	20.639488
62.942258	1969.934911	20.644506
63.118860	1988.798753	20.649523
63.271059	1983.791827	20.654541
63.513199	1983.378548	20.659559
63.738722	1998.242539	20.664576
63.734656	1982.558196	20.669594
63.891637	1984.875428	20.674611
63.643504	1985.554690	20.679629
64.003048	1978.845999	20.684647
63.927040	1982.850054	20.689664
63.709342	1988.712918	20.694682
64.165367	1984.204663	20.699699
63.771497	1993.124646	20.704717
64.062046	1983.750470	20.709735
64.186197	1978.192470	20.714752
64.026881	1979.943541	20.719770
64.211081	1980.407163	20.724787
64.068840	1994.820306	20.729805
64.254021	1999.522185	20.734823
64.209875	2009.489145	20.739840
64.190941	2006.869493	20.744858
64.094368	2007.540938	20.749875
64.106745	2018.183939	20.754893
64.243346	2027.273822	20.759911
64.514421	2031.410049	20.764928
64.754055	2032.376302	20.769946
64.961879	2024.498273	20.774963
64.637634	2037.387069	20.779981
64.956379	2034.254071	20.784999
64.909450	2052.139727	20.790016
65.374033	2047.835260	20.795034
65.464423	2045.886574	20.800051
65.296702	2059.527376	20.805069
65.372887	2043.022566	20.810087
65.570891	2055.855311	20.815104
65.613413	2050.458327	20.820122
65.576990	2033.649152	20.825139
65.614750	2037.774367	20.830157
65.933156	2046.652910	20.835175
65.796573	2046.756206	20.840192
65.606161	2042.077173	20.845210
65.615456	2039.645632	20.850227
65.905469	2058.068994	20.855245
65.971855	2070.354173	20.860263
66.117096	2066.014211	20.865280
66.274846	2062.947301	20.870298
66.459418	2056.900167	20.875315
66.395379	2068.602867	20.880333
66.292575	2055.442806	20.885351
66.301299	2061.207322	20.890368
66.464745	2062.996516	20.895386
66.630747	2056.895466	20.900403
66.336370	2055.786202	20.905421
66.362719	2064.135845	20.910439
66.720247	2070.660290	20.915456
66.671954	2084.430845	20.920474
67.131422	2078.823763	20.925491
67.394489	2092.785699	20.930509
67.370284	2089.589317	20.935527
67.514222	2080.802831	20.940544
67.152041	2085.971824	20.945562
67.402299	2082.584381	20.950579
67.591392	2084.385364	20.955597
67.450392	2084.341018	20.960615
67.348592	2084.776585	20.965632
67.691858	2087.121633	20.970650
67.818799	2089.030127	20.975667
67.481235	2080.448002	20.980685
67.612293	2082.886052	20.985703
67.997644	2079.086240	20.990720
67.583909	2091.379911	20.995738
67.545583	2079.872975	21.000755
67.617856	2083.165971	21.005773
67.526665	2075.422841	21.010791
67.538136	2080.609399	21.015808
67.985818	2103.707458	21.020826
68.044257	2102.388618	21.025843
68.069634	2100.926597	21.030861
68.013634	2105.315745	21.035879
67.886531	2109.753836	21.040896
68.347704	2119.768420	21.045914
68.518837	2128.632062	21.050931
68.643783	2131.538151	21.055949
68.370914	2129.945829	21.060967
68.572653	2123.129104	21.065984
68.852980	2124.808583	21.071002
69.239154	2102.480068	21.076019
69.297082	2119.711965	21.081037
69.411434	2119.223901	21.086055
69.531337	2111.482605	21.091072
69.153370	2117.004374	21.096090
69.391159	2113.123384	21.101107
69.202308	2114.506665	21.106125
69.548218	2114.777848	21.111143
69.764481	2110.767660	21.116160
69.466877	2117.599259	21.121178
69.533543	2119.280444	21.126195
69.693612	2112.864704	21.131213
69.635261	2142.261973	21.136231
69.810287	2132.012571	21.141248
69.797680	2134.693913	21.146266
69.640614	2136.851767	21.151283
69.723602	2141.159321	21.156301
69.464530	2139.975125	21.161319
70.267841	2145.928395	21.166336
70.343290	2163.820357	21.171354
70.750271	2153.111931	21.176371
71.117093	2155.387046	21.181389
70.804620	2143.641873	21.186407
70.515730	2131.760485	21.191424
70.732862	2123.233994	21.196442
71.052242	2136.382430	21.201459
70.942998	2137.806969	21.206477
70.767761	2133.977656	21.211495
70.926778	2140.785511	21.216512
70.831283	2153.190629	21.221530
71.069322	2160.570039	21.226547
70.936975	2157.750261	21.231565
71.245287	2156.266276	21.236583
71.454915	2154.841838	21.241600
71.282172	2151.794810	21.246618
71.218564	2145.530653	21.251635
71.307337	2149.174559	21.256653
70.977030	2152.359825	21.261671
71.518113	2154.771918	21.266688
71.407775	2169.498986	21.271706
71.656302	2167.875977	21.276723
71.808656	2168.985222	21.281741
71.616202	2173.080036	21.286759
71.806871	2169.600865	21.291776
71.736508	2170.646950	21.296794
71.668512	2162.256356	21.301811
71.934730	2175.700290	21.306829
72.008323	2181.271700	21.311847
72.018401	2188.819165	21.316864
71.941809	2183.084062	21.321882
72.228112	2183.721150	21.326899
72.470017	2180.379174	21.331917
72.461832	2199.653879	21.336935
72.434152	2201.911523	21.341952
72.624340	2214.786627	21.346970
72.636425	2223.021793	21.351987
72.978812	2220.090221	21.357005
73.147322	2223.305139	21.362023
73.389570	2212.653885	21.367040
73.057889	2206.182124	21.372058
73.107462	2214.689175	21.377075
73.376848	2202.989077	21.382093
73.178337	2214.921102	21.387111
73.532055	2208.140646	21.392128
73.008250	2210.532342	21.397146
73.173266	2208.123873	21.402163
73.372506	2217.645935	21.407181
73.515346	2234.366080	21.412199
73.823923	2222.953372	21.417216
73.567226	2231.972043	21.422234
74.181130	2234.549544	21.427251
74.415602	2237.956177	21.432269
74.037103	2232.552101	21.437287
74.069504	2236.069094	21.442304
74.017765	2235.139804	21.447322
73.862291	2230.256455	21.452339
74.050527	2233.783901	21.457357
74.050289	2245.075975	21.462375
74.686357	2250.143244	21.467392
74.745726	2248.253018	21.472410
74.501356	2258.052464	21.477427
74.808342	2251.749507	21.482445
74.686739	2253.090769	21.487463
74.632422	2248.977503	21.492480
74.662823	2264.405454	21.497498
74.869001	2275.233040	21.502515
75.245824	2269.919648	21.507533
75.059020	2285.583417	21.512551
75.225481	2276.013801	21.517568
75.218235	2276.949075	21.522586
75.197943	2272.338174	21.527603
74.988055	2275.596236	21.532621
74.923437	2280.542221	21.537639
75.360116	2292.760432	21.542656
75.781819	2290.681237	21.547674
75.509572	2298.086501	21.552691
76.134767	2292.844892	21.557709
75.857336	2307.837942	21.562727
75.709125	2304.032789	21.567744
75.919565	2305.057255	21.572762
76.073845	2321.987151	21.577779
76.400024	2323.479620	21.582797
76.327763	2325.753688	21.587815
76.365696	2330.819427	21.592832
76.243288	2333.341159	21.597850
76.397710	2327.115581	21.602867
76.869456	2324.574129	21.607885
76.973921	2333.394601	21.612903
77.049329	2325.079438	21.617920
76.778750	2319.737433	21.622938
76.670243	2321.392259	21.627955
76.554357	2315.571708	21.632973
76.655209	2331.616789	21.637991
76.817012	2337.565856	21.643008
76.901790	2340.866420	21.648026
77.084131	2348.065221	21.653043
77.127962	2338.558849	21.658061
77.100354	2346.869684	21.663079
77.280007	2358.376832	21.668096
77.258826	2359.178572	21.673114
77.355008	2367.889891	21.678131
77.980407	2367.811432	21.683149
77.976904	2366.606365	21.688167
77.909837	2368.324175	21.693184
78.092440	2363.672193	21.698202
77.784332	2370.963143	21.703219
78.313571	2362.255393	21.708237
78.035083	2369.096736	21.713255
77.776818	2365.204556	21.718272
78.411476	2375.470001	21.723290
78.185004	2390.082779	21.728307
78.453366	2386.004454	21.733325
78.155703	2396.774851	21.738343
78.252443	2400.950931	21.743360
78.552193	2391.818122	21.748378
78.564598	2413.523125	21.753395
78.943486	2413.287375	21.758413
79.037869	2418.117118	21.763431
79.181408	2407.578953	21.768448
79.451669	2405.905200	21.773466
79.148866	2416.692190	21.778483
79.524577	2406.566030	21.783501
78.939506	2409.390194	21.788519
79.101372	2412.864973	21.793536
79.497087	2423.871436	21.798554
79.693057	2435.458149	21.803571
79.806327	2430.305672	21.808589
79.591832	2434.000008	21.813607
79.310366	2437.600624	21.818624
79.791849	2436.335823	21.823642
79.622479	2438.287332	21.828659
80.203289	2448.302410	21.833677
80.159296	2454.536038	21.838695
80.376542	2454.997684	21.843712
80.477790	2457.642412	21.848730
80.014083	2453.318266	21.853747
80.637338	2447.070148	21.858765
80.695754	2452.217945	21.863783
80.508188	2454.216473	21.868800
80.824750	2445.882644	21.873818
80.530001	2460.225225	21.878835
80.919982	2466.457566	21.883853
80.984367	2478.481388	21.888871
80.780398	2479.936483	21.893888
81.213810	2478.193137	21.898906
81.039125	2486.495376	21.903923
81.303062	2479.088126	21.908941
81.251169	2475.255315	21.913959
81.067153	2493.241656	21.918976
81.240664	2489.676726	21.923994
81.311046	2503.388098	21.929011
81.450988	2498.764815	21.934029
81.833953	2506.421626	21.939047
81.944965	2502.793835	21.944064
81.702562	2500.092131	21.949082
81.695383	2510.940454	21.954099
81.784338	2513.801713	21.959117
82.095824	2514.128759	21.964135
82.182483	2523.719010	21.969152
82.654731	2515.928993	21.974170
82.197508	2513.803568	21.979187
82.382195	2525.300571	21.984205
82.386688	2535.253939	21.989223
82.748380	2544.413188	21.994240
83.083831	2537.004248	21.999258
82.720511	2544.177622	22.004275
82.791154	2537.273847	22.009293
82.766044	2542.510418	22.014311
82.629092	2548.458730	22.019328
82.657782	2530.540655	22.024346
82.854541	2555.947545	22.029363
82.829101	2563.342896	22.034381
83.560510	2563.992755	22.039399
83.607834	2565.033164	22.044416
83.791363	2563.243503	22.049434
83.680602	2565.334234	22.054451
83.595437	2572.461157	22.059469
83.966630	2573.312278	22.064487
83.745595	2565.065251	22.069504
84.137730	2576.410060	22.074522
84.489386	2592.394233	22.079539
84.127129	2594.230613	22.084557
84.227440	2593.836248	22.089575
84.194402	2589.703810	22.094592
84.616235	2589.969493	22.099610
84.528710	2585.779263	22.104627
84.974364	2583.087193	22.109645
84.688686	2587.824665	22.114663
84.662162	2591.616009	22.119680
84.668249	2590.043335	22.124698
84.477233	2596.795399	22.129715
84.858517	2596.281544	22.134733
85.036245	2604.172337	22.139751
85.182376	2605.134244	22.144768
85.327657	2602.025000	22.149786
85.411710	2610.845630	22.154803
85.075715	2604.194502	22.159821
85.336394	2611.867241	22.164839
85.220760	2616.862290	22.169856
85.523091	2622.682267	22.174874
85.785572	2629.745618	22.179891
85.423949	2637.363767	22.184909
85.690083	2626.216208	22.189927
85.662138	2643.537723	22.194944
86.111658	2646.371270	22.199962
86.377067	2641.166641	22.204979
86.724400	2628.179091	22.209997
86.905606	2624.414106	22.215015
87.180923	2631.462835	22.220032
87.253539	2635.794216	22.225050
86.868403	2623.302590	22.230067
87.189467	2615.820112	22.235085
87.774375	2601.012432	22.240103
87.364795	2606.406719	22.245120
86.694074	2594.275181	22.250138
86.979882	2601.079251	22.255155
87.233978	2593.916500	22.260173
87.297823	2607.237621	22.265191
87.438419	2616.709063	22.270208
87.800423	2612.010149	22.275226
87.748040	2614.710379	22.280243
87.885320	2619.483001	22.285261
87.997724	2613.506881	22.290279
88.050684	2622.303954	22.295296
87.958875	2618.556228	22.300314
87.651841	2617.893900	22.305331
88.094817	2622.710453	22.310349
87.985363	2623.465983	22.315367
87.831891	2620.756726	22.320384
88.289256	2616.462717	22.325402
88.237994	2620.128521	22.330419
88.411324	2639.388063	22.335437
88.309463	2636.074276	22.340455
88.402246	2646.891339	22.345472
88.579152	2640.185589	22.350490
88.681446	2642.243158	22.355507
88.392714	2637.901192	22.360525
88.826240	2644.729620	22.365543
88.952532	2661.219193	22.370560
88.894641	2657.832280	22.375578
89.247983	2664.048303	22.380595
88.967483	2671.032095	22.385613
89.278937	2665.460500	22.390631
89.190319	2673.500098	22.395648
89.353580	2681.042856	22.400666
89.570952	2693.459601	22.405683
89.103807	2691.263110	22.410701
89.649056	2686.302099	22.415719
89.631440	2702.845676	22.420736
90.129025	2710.907640	22.425754
90.185750	2717.305573	22.430771
90.119625	2723.545897	22.435789
90.363716	2719.938372	22.440807
90.465256	2713.244329	22.445824
90.481574	2721.141368	22.450842
90.463087	2718.048134	22.455859
90.388512	2728.361085	22.460877
90.334918	2738.184742	22.465895
90.245692	2744.662217	22.470912
90.478941	2739.437319	22.475930
91.089477	2754.204121	22.480947
90.640772	2765.575814	22.485965
91.210918	2767.910878	22.490983
91.113780	2769.687062	22.496000
91.192307	2771.391711	22.501018
91.556577	2791.678969	22.506035
91.714485	2793.898324	22.511053
92.101158	2786.695919	22.516071
91.726473	2797.753125	22.521088
92.058034	2790.243693	22.526106
92.371606	2786.647429	22.531123
92.112091	2787.782966	22.536141
92.308375	2784.230212	22.541159
92.258322	2787.185747	22.546176
92.473994	2780.988349	22.551194
92.072628	2785.115828	22.556211
92.227523	2797.210985	22.561229
92.706943	2793.083928	22.566247
92.518469	2801.577824	22.571264
92.995039	2809.778815	22.576282
92.907294	2802.814383	22.581299
92.942970	2812.403257	22.586317
92.819721	2808.887624	22.591335
92.969671	2818.259877	22.596352
92.746075	2835.425832	22.601370
93.541649	2835.245133	22.606387
93.066521	2835.738842	22.611405
93.487118	2840.227551	22.616423
93.348419	2846.233042	22.621440
93.596307	2862.833267	22.626458
93.832792	2856.916649	22.631475
93.641466	2863.416376	22.636493
94.122190	2858.613700	22.641511
93.942364	2861.993431	22.646528
93.892294	2858.570545	22.651546
94.229750	2870.921375	22.656563
94.316220	2881.329271	22.661581
94.501024	2873.590166	22.666599
94.696431	2890.823493	22.671616
94.516462	2888.077291	22.676634
94.571526	2888.393771	22.681651
94.379169	2885.835708	22.686669
94.590465	2890.319143	22.691687
94.938456	2895.286271	22.696704
94.970946	2912.743816	22.701722
95.715057	2899.416559	22.706739
95.443155	2902.652828	22.711757
95.771212	2893.827810	22.716775
95.957166	2893.199179	22.721792
95.469644	2898.157523	22.726810
95.748160	2893.701929	22.731827
95.479019	2899.115467	22.736845
95.655685	2894.397995	22.741863
95.784038	2916.394850	22.746880
95.746422	2916.283908	22.751898
96.169899	2919.298295	22.756915
96.405713	2922.001042	22.761933
96.198494	2922.437261	22.766951
96.307463	2919.706035	22.771968
96.553073	2930.609937	22.776986
96.480973	2940.884751	22.782003
96.520060	2941.942245	22.787021
96.553768	2939.004963	22.792039
96.899885	2937.249918	22.797056
96.931370	2940.470519	22.802074
96.695039	2952.737156	22.807091
96.804434	2969.677808	22.812109
97.114984	2964.443965	22.817127
96.831948	2968.351072	22.822144
97.125399	2983.845994	22.827162
97.785772	2987.495759	22.832179
97.817123	2993.550570	22.837197
97.503617	2992.759834	22.842215
97.682981	2996.547612	22.847232
97.862198	3009.822665	22.852250
98.153338	3010.913511	22.857267
98.087882	3023.507075	22.862285
97.806483	3021.571984	22.867303
98.312331	3020.846202	22.872320
98.667601	3024.739156	22.877338
98.724952	3031.601051	22.882355
99.051347	3035.091365	22.887373
98.971083	3031.546903	22.892391
99.294115	3037.486881	22.897408
98.993862	3030.284022	22.902426
99.159553	3031.274468	22.907443
99.322670	3032.495712	22.912461
99.583673	3028.440481	22.917479
99.617603	3025.916601	22.922496
99.388603	3029.714312	22.927514
99.546270	3021.739505	22.932531
99.552690	3029.549849	22.937549
100.114746	3038.712875	22.942567
100.052239	3049.254526	22.947584
99.836393	3046.627506	22.952602
100.180642	3048.622202	22.957619
100.416900	3055.790801	22.962637
100.502324	3045.419116	22.967655
100.457586	3049.285983	22.972672
100.261863	3058.579624	22.977690
100.501621	3050.623584	22.982707
100.350966	3065.565966	22.987725
100.611454	3076.013159	22.992743
100.845692	3075.036144	22.997760
100.771689	3085.052535	23.002778
100.921300	3081.431243	23.007795
101.152795	3090.001913	23.012813
101.162909	3095.129010	23.017831
101.228695	3099.448941	23.022848
101.447502	3105.815466	23.027866
101.614154	3090.349753	23.032883
101.318757	3093.738051	23.037901
101.690539	3094.551233	23.042919
102.063637	3097.008549	23.047936
101.779502	3112.719753	23.052954
102.056677	3115.883196	23.057971
102.141037	3120.257051	23.062989
102.066057	3122.818851	23.068007
102.285711	3110.816606	23.073024
102.124497	3122.500405	23.078042
102.265131	3128.282600	23.083059
102.633444	3139.243273	23.088077
102.429757	3140.300703	23.093095
102.707613	3141.463061	23.098112
103.169149	3146.216900	23.103130
103.605183	3155.153428	23.108147
103.468007	3154.035399	23.113165
103.505576	3157.491802	23.118183
103.580857	3162.277378	23.123200
103.883724	3158.534370	23.128218
104.192521	3160.035929	23.133235
104.216919	3159.899550	23.138253
103.885973	3155.055893	23.143271
104.244865	3155.359791	23.148288
104.100010	3152.920538	23.153306
104.778408	3146.654128	23.158323
104.261799	3146.242180	23.163341
104.224579	3151.534469	23.168359
104.713625	3143.182933	23.173376
104.278436	3151.832182	23.178394
104.723166	3144.450165	23.183411
104.550500	3154.873316	23.188429
104.802305	3166.877887	23.193447
104.604033	3169.073840	23.198464
104.776020	3179.932547	23.203482
105.045638	3176.194711	23.208499
105.023383	3188.118877	23.213517
105.071858	3193.495676	23.218535
105.452550	3189.115630	23.223552
105.379760	3193.709650	23.228570
105.526202	3194.936657	23.233587
105.745478	3215.985507	23.238605
106.146834	3216.677313	23.243623
106.093086	3220.602430	23.248640
106.107703	3216.295153	23.253658
106.290215	3214.231002	23.258675
106.441383	3211.994988	23.263693
106.707637	3218.840211	23.268711
106.768100	3219.269478	23.273728
107.172206	3229.647059	23.278746
107.619097	3234.207522	23.283763
107.308797	3215.855495	23.288781
106.829720	3219.689026	23.293799
107.451323	3215.208342	23.298816
107.050723	3232.279143	23.303834
107.267432	3227.889901	23.308851
107.116467	3232.107897	23.313869
107.278320	3239.935163	23.318887
107.670422	3242.250670	23.323904
107.784223	3250.820804	23.328922
107.788400	3256.917808	23.333939
107.745113	3261.087485	23.338957
107.841093	3258.689625	23.343975
107.815679	3261.322631	23.348992
107.727229	3267.727582	23.354010
108.156295	3278.647319	23.359027
108.584688	3279.798873	23.364045
108.259582	3275.661252	23.369063
108.228012	3276.707674	23.374080
108.438661	3299.194013	23.379098
108.442234	3303.078662	23.384115
108.667824	3300.815269	23.389133
108.958943	3313.312490	23.394151
109.232697	3323.552613	23.399168
109.243218	3328.294661	23.404186
109.484026	3323.604964	23.409203
109.530694	3325.756489	23.414221
109.558051	3321.627104	23.419239
109.963554	3324.732732	23.424256
110.107859	3340.292212	23.429274
110.378242	3345.088491	23.434291
110.699888	3351.274971	23.439309
110.665898	3338.131660	23.444327
110.414141	3319.211773	23.449344
110.210778	3328.797109	23.454362
110.393319	3336.731662	23.459379
110.934821	3335.965599	23.464397
110.797983	3348.059206	23.469415
110.807269	3345.008882	23.474432
110.847450	3352.435371	23.479450
111.086546	3363.362644	23.484467
111.063375	3368.564436	23.489485
111.170154	3371.299967	23.494503
111.280464	3366.330741	23.499520
111.184824	3372.358108	23.504538
111.557635	3384.621728	23.509555
111.611693	3385.891538	23.514573
111.427300	3399.015182	23.519591
111.850513	3387.877414	23.524608
112.090741	3415.358670	23.529626
111.832565	3412.905463	23.534643
112.502079	3409.067446	23.539661
112.718994	3410.479179	23.544679
112.331734	3403.842045	23.549696
112.695099	3419.607358	23.554714
112.733440	3427.936831	23.559731
113.261937	3424.329073	23.564749
112.991366	3436.399374	23.569767
113.402560	3431.560031	23.574784
113.280670	3435.562083	23.579802
113.404004	3434.267761	23.584819
113.633380	3429.576661	23.589837
113.226558	3440.677137	23.594855
113.895054	3445.086373	23.599872
113.745577	3458.719082	23.604890
113.705669	3456.556974	23.609907
113.828186	3459.034417	23.614925
113.832107	3472.059359	23.619943
113.917334	3479.627228	23.624960
114.063530	3485.209833	23.629978
114.382714	3488.635079	23.634995
114.566049	3501.830949	23.640013
114.192609	3502.611835	23.645031
114.731905	3498.582608	23.650048
114.746302	3504.981099	23.655066
115.437567	3514.108471	23.660083
115.566814	3518.311313	23.665101
115.384650	3526.542602	23.670119
115.342008	3523.430896	23.675136
115.897939	3526.977100	23.680154
115.830246	3523.506332	23.685171
115.936332	3523.783318	23.690189
115.643565	3524.860952	23.695207
115.993736	3515.495635	23.700224
115.924824	3519.382147	23.705242
115.912039	3526.261463	23.710259
116.569204	3530.899731	23.715277
116.881695	3539.808343	23.720295
116.914619	3524.760759	23.725312
116.911849	3532.351819	23.730330
116.684249	3533.949549	23.735347
117.079029	3530.735020	23.740365
117.227267	3535.231591	23.745383
116.812558	3539.212976	23.750400
117.734856	3534.461310	23.755418
117.305991	3538.526959	23.760435
117.457861	3543.458523	23.765453
117.224565	3564.786551	23.770471
117.373132	3564.561400	23.775488
118.047386	3550.000999	23.780506
117.952674	3561.649478	23.785523
117.801359	3574.250483	23.790541
117.740009	3584.606051	23.795559
117.791169	3577.348259	23.800576
117.998267	3593.703014	23.805594
117.781203	3602.021833	23.810611
118.779212	3590.188457	23.815629
118.779220	3592.864896	23.820647
119.360268	3600.721740	23.825664
119.370772	3610.630580	23.830682
119.345307	3606.733445	23.835699
119.171549	3622.093349	23.840717
119.167699	3619.657329	23.845735
119.419724	3609.237288	23.850752
119.768653	3606.433880	23.855770
119.483365	3622.688575	23.860787
119.953976	3624.130263	23.865805
119.614738	3639.449665	23.870823
119.872921	3633.179076	23.875840
120.347192	3642.696951	23.880858
120.677803	3660.282398	23.885875
120.736034	3658.341702	23.890893
121.009053	3663.671057	23.895911
120.843398	3664.962470	23.900928
120.872484	3656.309877	23.905946
120.721228	3666.007215	23.910963
120.853178	3660.532700	23.915981
121.082133	3668.889419	23.920999
121.321224	3681.776900	23.926016
121.685953	3689.288715	23.931034
121.320771	3690.418664	23.936051
121.556259	3683.356222	23.941069
121.311941	3694.646177	23.946087
121.870390	3704.738037	23.951104
122.117791	3699.510658	23.956122
122.129731	3700.774423	23.961139
122.151513	3708.440640	23.966157
122.253940	3718.609819	23.971175
122.292772	3724.676336	23.976192
122.882730	3734.195185	23.981210
122.329476	3736.197132	23.986227
123.114011	3745.512100	23.991245
123.197403	3759.111936	23.996263
122.786576	3755.943890	24.001280
123.118903	3753.641729	24.006298
122.995928	3762.795000	24.011315
123.473878	3772.883650	24.016333
123.681101	3780.019184	24.021351
123.622187	3772.882606	24.026368
123.680638	3782.051828	24.031386
123.705816	3789.556582	24.036403
124.120023	3799.904515	24.041421
124.467306	3804.685788	24.046439
124.335039	3802.058268	24.051456
124.733847	3796.592665	24.056474
124.647287	3807.757128	24.061491
124.681747	3795.199357	24.066509
124.911512	3803.227764	24.071527
124.733496	3802.930363	24.076544
125.230078	3818.530097	24.081562
125.075356	3827.025531	24.086579
124.978766	3830.237826	24.091597
125.334743	3824.905132	24.096615
125.265134	3840.012287	24.101632
125.584170	3846.552845	24.106650
125.367371	3863.519874	24.111667
125.541110	3865.781086	24.116685
126.017792	3876.921025	24.121703
125.887581	3881.726160	24.126720
126.362151	3876.564363	24.131738
126.188073	3884.639899	24.136755
126.877827	3893.025980	24.141773
126.946309	3903.090079	24.146791
127.006205	3899.962344	24.151808
127.214192	3895.100860	24.156826
127.207136	3908.055232	24.161843
127.198394	3897.012810	24.166861
127.341177	3910.297356	24.171879
127.433054	3920.187384	24.176896
127.677027	3925.038431	24.181914
127.557945	3919.344107	24.186931
127.318727	3929.184689	24.191949
127.853627	3943.216214	24.196967
127.754277	3939.756607	24.201984
128.084826	3943.164389	24.207002
128.552202	3956.464715	24.212019
128.368883	3962.275522	24.217037
128.799241	3965.361611	24.222055
129.290473	3959.177720	24.227072
129.512991	3952.202413	24.232090
129.215384	3952.867353	24.237107
129.147983	3955.431247	24.242125
129.693961	3950.097341	24.247143
129.680965	3950.342374	24.252160
130.018648	3942.910418	24.257178
129.883195	3955.414531	24.262195
129.822994	3964.962133	24.267213
130.300872	3964.322735	24.272231
130.076987	3967.652717	24.277248
130.210801	3968.515617	24.282266
130.139567	3969.763943	24.287283
130.169702	3981.683632	24.292301
130.285234	3985.323745	24.297319
130.420791	3997.239656	24.302336
131.173204	3997.734806	24.307354
130.717795	4017.620812	24.312371
130.820403	4022.304517	24.317389
131.110055	4022.410899	24.322407
131.285039	4030.103901	24.327424
131.467576	4032.101792	24.332442
131.562473	4042.584798	24.337459
131.645031	4048.878182	24.342477
131.548147	4046.683842	24.347495
131.672572	4057.345324	24.352512
132.129839	4062.867052	24.357530
132.007149	4068.873613	24.362547
132.005940	4090.450193	24.367565
132.337126	4098.800664	24.372583
132.500099	4098.014600	24.377600
132.780462	4110.930681	24.382618
132.730194	4105.954690	24.387635
132.819971	4125.825372	24.392653
133.171958	4126.790032	24.397671
132.844588	4123.460579	24.402688
133.102013	4133.283918	24.407706
133.472411	4143.831404	24.412723
133.396137	4143.824318	24.417741
133.680765	4139.443219	24.422759
133.415226	4167.484123	24.427776
133.808085	4174.382595	24.432794
134.314456	4180.499569	24.437811
134.208059	4180.222574	24.442829
134.281600	4195.998970	24.447847
134.309681	4201.120428	24.452864
134.934474	4193.435353	24.457882
134.835294	4215.074679	24.462899
135.044332	4221.812410	24.467917
134.864214	4230.192047	24.472935
135.132844	4227.019132	24.477952
135.588586	4231.332280	24.482970
135.687209	4245.274149	24.487987
135.963590	4247.345831	24.493005
136.115087	4247.278032	24.498023
136.116071	4253.347463	24.503040
136.151568	4250.267655	24.508058
136.245465	4259.122280	24.513075
136.518268	4260.866263	24.518093
136.433288	4268.858659	24.523111
136.618787	4257.457518	24.528128
137.104856	4276.395520	24.533146
137.050485	4279.197311	24.538163
137.179582	4283.943243	24.543181
137.197903	4294.473038	24.548199
137.350309	4299.218501	24.553216
137.646852	4292.619767	24.558234
138.020354	4305.530955	24.563251
137.954150	4311.683462	24.568269
138.123356	4310.842761	24.573287
138.187637	4326.538648	24.578304
138.241705	4311.338770	24.583322
138.516533	4314.382852	24.588339
138.370705	4327.097154	24.593357
138.840800	4343.992409	24.598375
138.759540	4335.347203	24.603392
138.814025	4341.124263	24.608410
138.726239	4351.093000	24.613427
139.395052	4352.481797	24.618445
139.324516	4351.899363	24.623463
139.543655	4355.981090	24.628480
139.665725	4352.973007	24.633498
139.545445	4360.566928	24.638515
139.725776	4385.167778	24.643533
139.894400	4379.722056	24.648551
140.064038	4392.778675	24.653568
140.232391	4393.434212	24.658586
140.432127	4410.876638	24.663603
140.238026	4414.066341	24.668621
140.540888	4417.292300	24.673639
140.613574	4429.224598	24.678656
140.769035	4435.778212	24.683674
140.789160	4439.493241	24.688691
141.142423	4466.377730	24.693709
141.319736	4462.376244	24.698727
141.337145	4468.743044	24.703744
141.657656	4485.431306	24.708762
141.553246	4485.873647	24.713779
141.830784	4488.428100	24.718797
141.921996	4483.840306	24.723815
142.106985	4510.463829	24.728832
142.637663	4506.719798	24.733850
143.053540	4517.020538	24.738867
142.478269	4520.383234	24.743885
143.149430	4510.901145	24.748903
142.817525	4527.084999	24.753920
142.958167	4524.572703	24.758938
143.421956	4532.075761	24.763955
143.139683	4536.245063	24.768973
143.656870	4529.763396	24.773991
143.987832	4523.206565	24.779008
143.746601	4533.398144	24.784026
143.968809	4542.258182	24.789043
144.062441	4546.517311	24.794061
144.223376	4549.613885	24.799079
144.730407	4555.752980	24.804096
144.630364	4559.647718	24.809114
144.800888	4563.456143	24.814131
144.836625	4573.585684	24.819149
145.026418	4567.726281	24.824167
145.217552	4576.079841	24.829184
145.137507	4586.811346	24.834202
145.420198	4586.555832	24.839219
145.482264	4604.546995	24.844237
145.625162	4600.307795	24.849255
145.412502	4615.371584	24.854272
145.776756	4631.197790	24.859290
145.930844	4610.780361	24.864307
146.212515	4634.166345	24.869325
146.206191	4637.317383	24.874343
146.648457	4639.764145	24.879360
146.804993	4650.379944	24.884378
146.978828	4657.192759	24.889395
147.163535	4671.989563	24.894413
147.449185	4664.537007	24.899431
147.325898	4668.085028	24.904448
147.408993	4667.330314	24.909466
148.075954	4682.964242	24.914483
148.184463	4699.174372	24.919501
148.304202	4696.775781	24.924519
148.247832	4699.505351	24.929536
148.076288	4691.568438	24.934554
148.299238	4692.540595	24.939571
148.208899	4707.178240	24.944589
148.659303	4713.888045	24.949607
148.947668	4710.206950	24.954624
148.906875	4715.998964	24.959642
149.316503	4724.924604	24.964659
149.351660	4735.575133	24.969677
149.590430	4731.642930	24.974695
149.439041	4731.937927	24.979712
149.644592	4742.047437	24.984730
149.900912	4758.831169	24.989747
149.926050	4754.234654	24.994765
150.031707	4759.470448	24.999783
150.645419	4764.639769	25.004800
150.383411	4781.295898	25.009818
150.986205	4776.650475	25.014835
150.695708	4782.276220	25.019853
151.080740	4783.087421	25.024871
151.489397	4770.439151	25.029888
151.601700	4789.117086	25.034906
151.808573	4795.946904	25.039923
151.946079	4806.351122	25.044941
151.844206	4802.778111	25.049959
152.009174	4796.325936	25.054976
151.590757	4803.079506	25.059994
151.827649	4799.699954	25.065011
152.174026	4812.811426	25.070029
152.593451	4817.556488	25.075047
152.423596	4826.335667	25.080064
152.199324	4826.111734	25.085082
152.904593	4841.938690	25.090099
152.799701	4851.032879	25.095117
152.764424	4849.428570	25.100135
153.228336	4861.009851	25.105152
153.131277	4879.032372	25.110170
153.565397	4880.694485	25.115187
153.577880	4890.073437	25.120205
153.456525	4909.422317	25.125223
153.851930	4914.092232	25.130240
153.609423	4915.263126	25.135258
154.285487	4930.911634	25.140275
153.910734	4943.358990	25.145293
154.628675	4950.964695	25.150311
154.797291	4961.600891	25.155328
154.123713	4966.677141	25.160346
154.883552	4971.116727	25.165363
155.237100	4988.930318	25.170381
155.536379	4988.249253	25.175399
155.569268	4999.588397	25.180416
155.554141	5009.438863	25.185434
155.698202	5016.789890	25.190451
156.254608	5024.969998	25.195469
156.248438	5028.452508	25.200487
156.771003	5035.454218	25.205504
156.366804	5028.080509	25.210522
156.743749	5043.163332	25.215539
156.856001	5055.749582	25.220557
157.194221	5052.259514	25.225575
157.111390	5062.565611	25.230592
157.039423	5081.941706	25.235610
157.467926	5082.237963	25.240627
157.364911	5096.770575	25.245645
157.538461	5112.087136	25.250663
158.095504	5113.872175	25.255680
157.921149	5119.236892	25.260698
158.140237	5131.377281	25.265715
158.329490	5142.022996	25.270733
158.544065	5141.803333	25.275751
158.595393	5143.427217	25.280768
158.956680	5158.610425	25.285786
159.028975	5149.738907	25.290803
159.441485	5170.267539	25.295821
159.893946	5187.033756	25.300839
159.572558	5185.335077	25.305856
159.637540	5191.303319	25.310874
160.005614	5187.142559	25.315891
160.069381	5196.826176	25.320909
159.930240	5210.035623	25.325927
160.342546	5217.502792	25.330944
160.281391	5224.235615	25.335962
160.560148	5230.609341	25.340979
160.661939	5238.456294	25.345997
160.948854	5246.479601	25.351015
161.241241	5255.752033	25.356032
161.286607	5271.653699	25.361050
161.383334	5270.382329	25.366067
161.717289	5273.726706	25.371085
161.716695	5290.866579	25.376103
161.836789	5288.843479	25.381120
161.872832	5302.859035	25.386138
161.902909	5317.901395	25.391155
162.479257	5317.246625	25.396173
162.622795	5326.081417	25.401191
163.060684	5335.220758	25.406208
163.357800	5337.393504	25.411226
163.600415	5342.488195	25.416243
163.929446	5336.654216	25.421261
163.491629	5337.028538	25.426279
163.917609	5340.475390	25.431296
163.944170	5335.815377	25.436314
164.107735	5334.754553	25.441331
164.172218	5344.292938	25.446349
164.230838	5358.282926	25.451367
164.523178	5356.109897	25.456384
164.638277	5364.721866	25.461402
164.711695	5360.237630	25.466419
164.904308	5372.518032	25.471437
165.121228	5376.606648	25.476455
165.133769	5379.240365	25.481472
165.132926	5390.035769	25.486490
165.688405	5393.282549	25.491507
166.063167	5399.723456	25.496525
166.243156	5398.113993	25.501543
166.613987	5394.880774	25.506560
166.581725	5393.443243	25.511578
166.743941	5406.848966	25.516595
166.895536	5411.339169	25.521613
166.795351	5414.855329	25.526631
166.891893	5406.901617	25.531648
166.902614	5418.522247	25.536666
167.374380	5429.865930	25.541683
167.937499	5428.326232	25.546701
168.027493	5422.346362	25.551719
168.048381	5414.275008	25.556736
168.211722	5425.006993	25.561754
168.522799	5417.881607	25.566771
168.607287	5427.833582	25.571789
168.509622	5426.734510	25.576807
168.871678	5445.551002	25.581824
169.220186	5443.770097	25.586842
169.401505	5450.844038	25.591859
169.587434	5447.841615	25.596877
169.636531	5451.580749	25.601895
169.580410	5462.141750	25.606912
169.539453	5469.322904	25.611930
169.390215	5474.481797	25.616947
169.696174	5483.799581	25.621965
169.646853	5499.580457	25.626983
170.195745	5495.280997	25.632000
170.283642	5507.401028	25.637018
170.214624	5516.379484	25.642035
170.688894	5525.724746	25.647053
170.667231	5547.148415	25.652071
170.911992	5546.898796	25.657088
171.317072	5563.091933	25.662106
171.034062	5563.091780	25.667123
171.693595	5580.703644	25.672141
171.729789	5595.063466	25.677159
171.646841	5596.395797	25.682176
171.905371	5604.972923	25.687194
172.697388	5610.004250	25.692212
172.828460	5609.137862	25.697229
172.883161	5619.422862	25.702247
172.772071	5608.168061	25.707264
173.187088	5630.161466	25.712282
173.146673	5633.264322	25.717300
173.696729	5638.418555	25.722317
173.742360	5650.163317	25.727335
174.039271	5660.906212	25.732352
174.026693	5666.511055	25.737370
173.905812	5666.495129	25.742388
174.167399	5659.980258	25.747405
173.929560	5679.565895	25.752423
174.117565	5693.381325	25.757440
174.549989	5691.473696	25.762458
174.963656	5717.031187	25.767476
175.030823	5723.987273	25.772493
175.182637	5708.805731	25.777511
175.276254	5720.397865	25.782528
175.747340	5732.287931	25.787546
176.043117	5748.728681	25.792564
176.086847	5744.596197	25.797581
176.119382	5761.144231	25.802599
176.049113	5761.925354	25.807616
176.231011	5777.051781	25.812634
176.231362	5789.523384	25.817652
176.681740	5792.998092	25.822669
176.789641	5808.748444	25.827687
176.938403	5815.073170	25.832704
177.399863	5831.251455	25.837722
177.524276	5834.941063	25.842740
177.864757	5841.545296	25.847757
178.668523	5851.363422	25.852775
178.270646	5849.859671	25.857792
178.567483	5847.076660	25.862810
178.351035	5852.318726	25.867828
178.640537	5854.366456	25.872845
178.860214	5874.575524	25.877863
179.014790	5875.264827	25.882880
179.358834	5879.453716	25.887898
179.374082	5887.156594	25.892916
179.605597	5891.606064	25.897933
179.596631	5898.542504	25.902951
179.695253	5911.680719	25.907968
180.242429	5917.286875	25.912986
180.297552	5920.744230	25.918004
180.591909	5938.968859	25.923021
180.580478	5941.637956	25.928039
180.504853	5950.775485	25.933056
180.941042	5963.611809	25.938074
181.082769	5984.868506	25.943092
181.260346	5975.064775	25.948109
181.279409	5995.671379	25.953127
181.331709	5999.640561	25.958144
181.599097	5999.299029	25.963162
181.607790	6024.175037	25.968180
182.093739	6027.761048	25.973197
182.602181	6043.045194	25.978215
182.500699	6049.566793	25.983232
182.916799	6052.538670	25.988250
182.584053	6067.915921	25.993268
183.334877	6065.800851	25.998285
183.305308	6076.083445	26.003303
183.283599	6090.323250	26.008320
184.081037	6090.811462	26.013338
183.963516	6095.185901	26.018356
184.454115	6107.022669	26.023373
184.307384	6127.677330	26.028391
184.382202	6128.966198	26.033408
184.755477	6127.118240	26.038426
184.751979	6143.223986	26.043444
185.347552	6139.336944	26.048461
185.421911	6147.747288	26.053479
185.620760	6153.587679	26.058496
185.607012	6172.652831	26.063514
185.580433	6183.370638	26.068532
185.761574	6178.638994	26.073549
185.899836	6186.941550	26.078567
186.190557	6200.905520	26.083584
186.504921	6202.024518	26.088602
186.475189	6217.335778	26.093620
186.819587	6230.899987	26.098637
187.088351	6235.520516	26.103655
186.879625	6237.917333	26.108672
187.165319	6249.533562	26.113690
187.177218	6251.744511	26.118708
187.710755	6273.335127	26.123725
187.786017	6288.282867	26.128743
187.692882	6288.158450	26.133760
187.922834	6295.326161	26.138778
188.208916	6314.297429	26.143796
188.695899	6314.565666	26.148813
188.909442	6321.398177	26.153831
189.062159	6325.822142	26.158848
189.565609	6343.212825	26.163866
189.289859	6352.596367	26.168884
189.381901	6347.247213	26.173901
189.836494	6363.531212	26.178919
190.387538	6374.294939	26.183936
190.793780	6367.927758	26.188954
190.671689	6370.951912	26.193972
190.492833	6371.999345	26.198989
191.038131	6382.280998	26.204007
191.102424	6397.135834	26.209024
191.332861	6387.513055	26.214042
191.450201	6412.640996	26.219060
191.537062	6417.441414	26.224077
191.661609	6427.299310	26.229095
191.664750	6448.735959	26.234112
192.333668	6447.722661	26.239130
192.894569	6447.985706	26.244148
192.690051	6458.639834	26.249165
192.973558	6461.386199	26.254183
192.840057	6468.831533	26.259200
193.152125	6469.430049	26.264218
193.388845	6487.032859	26.269236
193.766435	6486.001782	26.274253
193.736763	6485.791721	26.279271
194.008353	6504.673900	26.284288
194.489993	6502.180848	26.289306
194.467242	6515.723513	26.294324
194.403582	6513.113327	26.299341
194.624937	6530.860623	26.304359
194.726754	6550.031288	26.309376
195.128681	6555.306705	26.314394
195.084647	6560.077031	26.319412
195.613357	6567.409836	26.324429
195.683802	6580.019432	26.329447
195.771174	6597.920236	26.334464
195.702756	6596.270425	26.339482
196.069551	6615.769241	26.344500
196.183298	6625.199611	26.349517
196.583525	6646.502064	26.354535
196.948370	6658.140955	26.359552
196.851225	6648.272307	26.364570
196.983747	6675.128137	26.369588
197.134690	6678.621225	26.374605
197.830167	6694.476580	26.379623
198.089206	6701.680961	26.384640
198.428652	6701.659657	26.389658
198.234208	6698.785699	26.394676
198.791726	6712.266578	26.399693
198.799008	6713.657547	26.404711
198.999516	6724.337160	26.409728
199.226915	6731.720099	26.414746
199.343217	6743.104162	26.419764
199.680927	6752.120917	26.424781
199.891480	6754.263118	26.429799
199.461273	6745.241774	26.434816
199.381153	6765.710006	26.439834
199.871345	6775.018709	26.444852
200.090271	6794.000932	26.449869
200.290462	6796.545660	26.454887
200.209930	6810.776242	26.459904
200.320772	6822.814655	26.464922
200.861795	6836.355016	26.469940
201.207838	6844.114125	26.474957
201.412855	6858.615965	26.479975
201.472041	6869.147199	26.484992
201.973694	6864.103466	26.490010
202.417558	6877.520086	26.495028
202.564492	6884.760933	26.500045
203.850051	6868.808443	26.505063
204.608977	6856.861828	26.510080
204.960494	6853.044203	26.515098
205.165428	6834.134779	26.520116
205.079329	6823.771860	26.525133
205.091736	6808.282806	26.530151
204.774362	6802.252265	26.535168
204.953674	6795.437282	26.540186
205.175835	6793.202406	26.545204
204.720232	6797.298188	26.550221
205.300962	6792.845105	26.555239
205.283033	6819.629869	26.560256
205.442599	6814.446846	26.565274
205.473725	6820.348288	26.570292
205.502149	6822.667220	26.575309
205.531972	6826.895780	26.580327
205.551270	6851.319845	26.585344
205.657170	6861.910095	26.590362
205.985617	6878.564595	26.595380
206.239813	6882.641435	26.600397
206.703636	6903.009351	26.605415
206.431350	6913.544865	26.610432
206.551853	6931.724948	26.615450
206.910147	6951.155997	26.620468
207.280384	6959.536434	26.625485
207.581676	6966.759595	26.630503
207.748530	6996.205436	26.635520
207.401258	6990.062686	26.640538
207.960421	7013.998846	26.645556
208.122196	7025.581197	26.650573
208.425253	7044.250685	26.655591
208.556174	7053.362922	26.660608
208.323366	7069.865060	26.665626
208.933085	7086.179219	26.670644
209.214987	7098.601566	26.675661
209.883684	7114.840275	26.680679
209.995500	7131.787593	26.685696
210.308351	7134.725215	26.690714
210.722023	7146.741948	26.695732
210.812824	7159.939100	26.700749
211.068358	7165.202761	26.705767
211.200124	7178.191512	26.710784
211.007435	7172.851722	26.715802
211.682398	7187.908867	26.720820
211.515633	7206.875802	26.725837
211.763153	7213.624437	26.730855
211.867639	7234.964149	26.735872
212.379076	7236.292451	26.740890
212.590907	7247.245251	26.745908
212.228318	7263.161655	26.750925
213.163516	7275.681293	26.755943
213.247401	7292.658363	26.760960
213.392340	7289.144299	26.765978
213.167289	7297.393435	26.770996
213.410241	7316.703928	26.776013
213.821487	7326.953320	26.781031
213.975774	7346.890079	26.786048
214.249309	7352.741324	26.791066
214.854884	7367.114910	26.796084
214.825864	7371.157031	26.801101
215.343456	7368.961327	26.806119
215.496994	7388.686739	26.811136
215.449351	7392.536038	26.816154
215.884638	7400.707668	26.821172
216.080975	7408.001011	26.826189
215.864467	7414.559943	26.831207
215.969272	7429.706055	26.836224
216.234720	7444.678795	26.841242
216.694435	7460.906152	26.846260
216.467943	7478.020107	26.851277
217.111095	7485.925803	26.856295
217.196950	7508.594624	26.861312
217.209275	7508.460093	26.866330
217.760079	7533.556811	26.871348
217.942956	7550.016760	26.876365
218.093285	7558.191785	26.881383
218.575912	7566.899105	26.886400
218.798165	7580.126603	26.891418
218.775100	7584.237296	26.896436
218.757705	7603.108775	26.901453
219.037151	7610.417671	26.906471
219.395547	7631.191110	26.911488
219.654371	7645.088539	26.916506
219.692285	7657.100971	26.921524
220.228617	7671.577127	26.926541
220.645107	7677.358867	26.931559
220.796414	7685.297027	26.936576
221.024788	7701.263864	26.941594
221.131371	7701.307228	26.946612
221.670840	7714.011899	26.951629
221.658708	7731.342112	26.956647
221.941298	7730.445723	26.961664
221.848234	7754.105564	26.966682
222.721483	7755.409145	26.971700
222.471438	7777.682310	26.976717
222.801126	7791.916080	26.981735
223.207442	7793.027178	26.986752
223.521411	7809.605856	26.991770
223.238490	7812.696325	26.996788
223.481335	7835.454756	27.001805
223.876327	7847.449602	27.006823
224.089438	7848.597097	27.011840
224.295253	7874.603524	27.016858
224.079938	7889.885091	27.021876
224.939241	7899.417871	27.026893
225.100692	7909.750677	27.031911
224.918645	7915.830879	27.036928
225.335734	7933.485921	27.041946
225.683204	7941.049543	27.046964
225.733118	7960.728562	27.051981
226.096100	7963.797420	27.056999
226.154379	7975.304931	27.062016
226.397551	7991.427564	27.067034
226.585481	8002.719175	27.072052
226.602676	8025.793943	27.077069
227.435032	8028.909702	27.082087
227.838116	8039.072368	27.087104
228.347086	8048.842874	27.092122
228.877808	8052.981105	27.097140
228.681805	8053.803998	27.102157
228.839824	8056.888998	27.107175
229.212437	8055.255630	27.112192
228.913132	8055.794694	27.117210
229.571894	8064.017066	27.122228
229.565766	8065.059801	27.127245
229.761289	8063.311939	27.132263
230.541389	8065.277228	27.137280
230.225423	8067.684662	27.142298
230.701731	8067.481046	27.147316
230.983753	8091.496489	27.152333
230.774537	8081.300406	27.157351
231.088933	8087.423340	27.162368
231.069370	8108.275104	27.167386
231.525420	8113.504664	27.172404
231.436797	8133.410640	27.177421
231.915159	8138.734600	27.182439
232.107282	8152.134522	27.187456
232.094055	8169.301154	27.192474
232.075863	8174.146800	27.197492
232.300427	8196.693849	27.202509
232.520884	8205.417033	27.207527
233.119420	8211.950380	27.212544
232.979286	8228.754827	27.217562
233.662943	8248.404941	27.222580
234.085985	8265.320634	27.227597
233.709045	8275.412294	27.232615
234.469883	8288.120782	27.237632
234.928401	8302.978924	27.242650
235.097054	8307.056772	27.247668
235.221915	8321.695372	27.252685
235.193420	8319.332016	27.257703
235.848371	8333.294575	27.262720
236.064407	8343.808548	27.267738
236.479093	8342.784226	27.272756
236.900543	8360.113825	27.277773
236.720900	8371.848047	27.282791
237.092390	8374.631518	27.287808
236.940144	8385.916342	27.292826
237.373186	8393.542597	27.297844
237.687819	8397.929228	27.302861
237.781316	8416.247578	27.307879
238.153541	8425.054578	27.312896
238.291813	8445.181285	27.317914
238.340489	8446.161839	27.322932
238.380291	8463.607780	27.327949
238.777256	8476.641399	27.332967
239.143601	8492.931561	27.337984
239.292082	8503.983371	27.343002
239.764053	8522.770131	27.348020
239.930133	8538.207535	27.353037
240.111713	8548.105048	27.358055
240.620175	8560.669908	27.363072
240.428014	8571.329646	27.368090
240.988808	8583.217076	27.373108
240.857193	8599.449104	27.378125
240.846322	8614.257449	27.383143
241.583043	8620.911498	27.388160
241.516719	8642.424659	27.393178
242.077564	8649.510206	27.398196
241.959724	8672.638377	27.403213
242.331480	8682.828377	27.408231
242.558413	8704.940000	27.413248
242.852969	8720.187071	27.418266
243.375549	8725.498004	27.423284
243.664355	8747.754743	27.428301
243.837844	8764.214082	27.433319
243.958011	8762.575758	27.438336
244.063434	8778.231174	27.443354
244.674611	8783.304177	27.448372
244.909968	8778.733911	27.453389
245.118507	8802.335509	27.458407
245.517474	8804.546489	27.463424
245.694010	8807.641361	27.468442
246.008912	8821.360465	27.473460
246.086939	8832.754937	27.478477
246.003932	8837.992859	27.483495
246.003778	8851.906263	27.488512
246.417952	8864.359725	27.493530
246.607391	8873.744736	27.498548
246.837865	8892.638928	27.503565
247.145993	8896.587851	27.508583
247.285022	8908.582197	27.513600
247.765799	8928.627694	27.518618
248.150539	8947.321125	27.523636
248.647546	8958.019018	27.528653
248.559040	8961.199380	27.533671
248.723856	8975.330292	27.538688
249.211867	8988.189085	27.543706
249.195276	9007.803802	27.548724
249.582479	9014.515567	27.553741
249.419864	9039.457053	27.558759
250.219448	9045.198525	27.563776
250.347581	9065.081229	27.568794
250.568714	9071.853598	27.573812
250.935962	9089.381750	27.578829
251.133710	9105.480858	27.583847
251.437026	9113.717999	27.588864
251.580013	9133.424819	27.593882
252.102565	9139.054751	27.598900
252.337216	9158.166408	27.603917
252.349698	9177.622077	27.608935
252.779875	9177.356179	27.613952
252.628629	9187.043805	27.618970
252.647108	9218.470586	27.623988
253.475153	9221.666156	27.629005
253.438588	9239.715109	27.634023
253.840136	9259.909059	27.639040
254.113463	9273.783359	27.644058
254.024368	9295.897532	27.649076
254.376505	9306.428751	27.654093
254.607061	9334.166681	27.659111
255.242992	9350.570331	27.664128
255.747018	9362.460788	27.669146
255.727427	9372.882586	27.674164
256.105337	9379.804307	27.679181
256.272183	9403.583653	27.684199
256.726978	9415.724914	27.689216
257.183799	9417.825931	27.694234
257.316703	9433.739672	27.699252
257.796786	9433.185010	27.704269
257.802214	9465.251997	27.709287
257.592661	9465.297227	27.714304
258.294777	9481.163434	27.719322
258.190769	9494.370485	27.724340
258.490755	9505.440350	27.729357
258.535422	9512.309814	27.734375
259.306597	9535.786866	27.739392
259.392558	9543.736000	27.744410
259.704346	9560.518654	27.749428
260.160465	9568.103918	27.754445
260.162834	9579.112817	27.759463
260.885009	9598.319518	27.764480
260.630870	9603.435908	27.769498
260.697129	9617.409005	27.774516
261.228235	9624.812127	27.779533
261.082177	9641.230435	27.784551
261.848339	9648.647487	27.789568
262.062591	9664.501402	27.794586
262.139899	9673.282297	27.799604
262.582678	9688.087175	27.804621
262.396348	9705.657894	27.809639
263.092337	9703.642529	27.814656
263.129197	9716.070063	27.819674
263.741375	9724.830855	27.824692
264.434070	9730.911227	27.829709
264.246714	9746.249958	27.834727
264.610952	9749.094757	27.839744
264.949832	9755.365984	27.844762
264.653993	9772.827524	27.849780
265.405504	9772.985184	27.854797
265.412373	9799.603073	27.859815
265.619817	9802.974298	27.864832
265.758599	9819.771492	27.869850
265.784417	9826.467199	27.874868
266.157420	9848.380639	27.879885
266.337211	9870.040028	27.884903
266.889890	9877.556713	27.889920
266.886328	9893.795194	27.894938
266.930607	9914.926364	27.899956
267.362372	9933.376673	27.904973
267.593513	9956.553145	27.909991
268.235342	9971.093620	27.915008
268.507049	9988.678542	27.920026
268.584672	10001.541944	27.925044
268.770559	10029.846712	27.930061
269.363938	10034.512383	27.935079
270.058712	10053.809071	27.940096
270.049690	10065.988239	27.945114
270.159110	10074.963236	27.950132
270.933923	10080.775196	27.955149
271.040336	10103.469255	27.960167
270.938931	10114.453581	27.965184
271.446947	10124.440038	27.970202
271.500912	10143.107241	27.975220
272.080083	10153.521505	27.980237
272.005736	10168.382017	27.985255
272.272271	10178.560808	27.990272
272.654389	10196.393955	27.995290
273.048012	10214.973619	28.000308
273.188220	10217.158753	28.005325
273.457207	10240.841177	28.010343
273.889802	10251.243585	28.015360
274.705053	10256.673581	28.020378
274.771121	10265.475450	28.025396
275.156904	10276.844997	28.030413
275.150233	10288.600859	28.035431
275.425042	10286.092154	28.040448
275.869704	10309.605234	28.045466
275.693365	10325.359498	28.050484
276.173198	10328.821021	28.055501
276.372241	10344.952576	28.060519
276.436265	10359.769597	28.065536
277.086703	10376.626561	28.070554
277.027696	10390.335577	28.075572
277.391003	10398.087187	28.080589
277.603416	10413.376857	28.085607
277.892748	10426.984308	28.090624
278.305205	10440.446305	28.095642
278.838957	10453.785235	28.100660
278.773738	10464.508384	28.105677
279.131014	10475.127875	28.110695
279.017803	10485.103892	28.115712
279.537381	10499.401751	28.120730
280.187875	10521.304356	28.125748
280.270410	10521.146243	28.130765
280.444986	10530.578610	28.135783
280.675922	10544.567813	28.140800
281.043400	10556.833926	28.145818
281.332722	10578.603384	28.150836
281.515939	10580.387189	28.155853
281.957950	10592.752232	28.160871
282.041151	10614.162303	28.165888
281.946070	10624.040849	28.170906
282.667839	10654.927997	28.175924
282.984685	10656.539449	28.180941
282.912003	10666.348224	28.185959
282.875933	10691.104877	28.190976
282.972163	10706.359199	28.195994
283.026558	10730.381925	28.201012
283.710735	10751.499671	28.206029
283.882385	10775.137937	28.211047
284.055841	10795.163834	28.216064
284.584866	10817.347767	28.221082
284.865887	10848.455411	28.226100
285.264336	10860.644282	28.231117
285.454196	10890.026430	28.236135
285.821154	10905.706071	28.241152
286.407336	10922.946115	28.246170
287.076260	10944.420091	28.251188
287.339861	10946.598731	28.256205
287.594388	10969.065548	28.261223
287.825581	10982.774023	28.266240
288.247746	10994.839306	28.271258
288.573887	11007.841530	28.276276
288.624481	11025.345029	28.281293
288.940814	11035.491277	28.286311
289.333105	11059.799671	28.291328
289.915979	11062.705361	28.296346
290.257729	11089.651853	28.301364
290.701339	11097.577546	28.306381
290.729105	11113.654336	28.311399
290.796544	11117.158110	28.316416
290.953542	11128.380662	28.321434
290.935268	11145.364534	28.326452
291.628703	11172.209031	28.331469
291.515316	11173.748580	28.336487
292.102192	11205.260725	28.341504
292.656789	11220.649344	28.346522
292.876976	11238.830766	28.351540
293.017543	11246.320601	28.356557
293.512687	11266.120099	28.361575
293.415326	11286.542327	28.366592
293.395494	11298.938694	28.371610
293.764366	11327.728462	28.376628
294.275100	11346.742550	28.381645
294.772077	11354.963167	28.386663
294.903849	11379.833532	28.391680
295.236675	11391.044655	28.396698
295.172172	11411.667144	28.401716
295.757929	11421.042262	28.406733
296.272425	11454.160659	28.411751
296.393815	11470.046356	28.416768
296.770462	11481.800126	28.421786
296.921326	11507.441290	28.426804
297.671533	11520.308384	28.431821
297.952676	11542.651759	28.436839
297.609148	11565.714454	28.441856
297.979913	11580.033154	28.446874
298.139412	11601.890325	28.451892
298.596543	11618.124890	28.456909
298.654009	11648.428751	28.461927
298.725392	11670.804935	28.466944
299.485903	11687.904873	28.471962
299.836309	11709.988214	28.476980
299.969721	11714.893276	28.481997
300.985166	11734.091263	28.487015
301.122260	11748.541199	28.492032
301.516022	11759.471502	28.497050
301.897456	11776.441082	28.502068
302.112624	11780.070389	28.507085
302.486926	11801.458601	28.512103
302.723254	11808.785344	28.517120
303.428197	11831.751444	28.522138
303.339681	11838.326737	28.527156
303.394771	11840.638988	28.532173
303.838937	11856.503180	28.537191
303.604599	11868.349157	28.542208
304.190188	11881.535789	28.547226
304.497046	11911.542323	28.552244
304.262963	11925.229197	28.557261
305.158989	11950.871789	28.562279
305.294153	11978.176959	28.567296
305.625070	11992.817943	28.572314
305.830885	12021.795203	28.577332
305.975752	12039.114458	28.582349
306.441234	12056.235404	28.587367
306.737868	12079.944273	28.592384
307.080534	12089.711232	28.597402
307.660351	12112.109832	28.602420
308.289058	12123.632146	28.607437
309.120219	12140.775181	28.612455
309.231703	12152.305411	28.617472
309.770155	12154.924528	28.622490
310.463155	12166.938930	28.627508
310.333304	12166.709666	28.632525
310.720268	12179.504303	28.637543
310.586865	12189.803295	28.642560
310.895891	12201.154389	28.647578
311.709390	12216.828764	28.652596
311.401288	12218.007158	28.657613
311.790261	12229.355297	28.662631
311.869781	12245.099757	28.667648
312.200758	12257.928425	28.672666
312.512164	12276.298744	28.677684
312.727280	12277.487259	28.682701
313.089003	12306.525943	28.687719
313.104270	12324.920311	28.692736
313.419346	12347.082529	28.697754
313.701232	12366.275378	28.702772
313.586391	12392.956954	28.707789
314.031181	12402.913429	28.712807
314.256885	12437.082676	28.717824
314.592142	12466.406765	28.722842
315.342733	12493.200050	28.727860
315.396583	12517.692494	28.732877
315.824436	12535.204980	28.737895
316.350212	12565.566878	28.742912
316.559565	12589.848899	28.747930
317.104134	12614.950302	28.752948
317.512769	12625.528286	28.757965
318.005031	12629.174616	28.762983
318.457304	12644.735069	28.768000
318.891158	12661.602556	28.773018
319.770853	12661.825562	28.778036
319.541605	12678.862612	28.783053
320.276766	12685.613112	28.788071
320.408172	12691.134506	28.793088
320.521936	12697.476509	28.798106
320.768444	12716.811008	28.803124
320.982326	12724.766842	28.808141
321.196363	12735.409919	28.813159
321.402709	12747.952022	28.818176
321.716913	12759.258439	28.823194
321.716580	12772.893747	28.828212
322.014581	12791.348759	28.833229
322.290290	12803.014867	28.838247
322.572050	12835.117236	28.843264
322.372130	12851.714101	28.848282
323.312397	12875.525868	28.853300
323.604396	12897.641803	28.858317
323.474670	12913.627813	28.863335
323.948822	12938.112209	28.868352
324.495972	12962.376856	28.873370
325.043190	12979.659600	28.878388
325.106930	13017.341339	28.883405
325.369704	13026.846494	28.888423
325.476814	13048.644031	28.893440
326.177174	13070.030292	28.898458
326.462471	13090.574899	28.903476
326.528027	13118.849382	28.908493
327.411601	13144.135552	28.913511
327.544050	13166.845053	28.918528
327.631682	13183.075341	28.923546
328.179296	13196.587754	28.928564
328.385438	13212.550148	28.933581
328.770528	13233.019374	28.938599
329.369693	13258.599446	28.943616
329.478841	13275.041199	28.948634
329.701460	13303.004139	28.953652
330.058398	13325.198886	28.958669
330.396742	13342.625007	28.963687
331.292661	13363.166424	28.968704
331.604845	13377.691404	28.973722
332.653771	13376.293349	28.978740
333.215561	13392.093158	28.983757
333.522431	13390.491683	28.988775
334.030441	13398.904114	28.993792
333.955575	13411.332544	28.998810
334.454635	13413.241135	29.003828
334.572513	13418.651164	29.008845
334.978730	13432.855232	29.013863
335.413999	13439.479011	29.018880
335.590109	13439.527359	29.023898
335.998588	13451.138462	29.028916
336.039244	13466.498414	29.033933
336.121775	13479.666595	29.038951
336.240452	13498.466006	29.043968
336.294027	13513.675564	29.048986
336.670359	13538.848602	29.054004
336.760323	13554.065158	29.059021
337.220123	13578.423146	29.064039
337.212347	13604.590813	29.069056
337.919994	13632.898734	29.074074
338.065226	13654.675244	29.079092
338.111270	13686.446279	29.084109
338.633973	13719.229489	29.089127
339.074873	13732.803112	29.094144
339.836874	13757.739554	29.099162
340.241837	13784.537960	29.104180
340.543596	13807.951358	29.109197
340.808339	13823.409346	29.114215
340.745304	13846.636422	29.119232
341.240836	13871.908190	29.124250
341.482031	13897.857497	29.129268
341.918303	13923.912262	29.134285
341.731475	13947.468214	29.139303
342.339562	13974.983706	29.144320
342.201462	14006.193402	29.149338
342.636358	14023.229319	29.154356
342.973298	14060.207423	29.159373
343.213260	14082.206526	29.164391
343.823360	14101.422676	29.169408
343.912583	14136.538379	29.174426
344.629547	14154.184208	29.179444
344.738248	14185.453673	29.184461
345.192402	14202.306746	29.189479
345.927850	14232.231299	29.194496
346.096852	14261.287203	29.199514
347.444889	14253.763326	29.204532
348.059916	14261.868945	29.209549
348.882472	14270.027525	29.214567
349.626211	14273.123428	29.219584
349.767919	14275.637240	29.224602
350.002699	14276.544916	29.229620
349.724542	14277.652452	29.234637
350.003484	14290.001111	29.239655
350.509225	14307.534697	29.244672
350.286544	14327.423910	29.249690
350.865874	14332.440241	29.254708
351.456204	14358.920061	29.259725
351.487041	14359.884756	29.264743
351.759184	14376.630525	29.269760
351.996892	14409.797210	29.274778
352.335723	14418.836466	29.279796
352.635175	14443.694238	29.284813
352.612835	14465.807257	29.289831
353.094375	14489.796698	29.294848
352.966005	14520.159361	29.299866
353.790152	14536.096136	29.304884
353.821553	14572.544878	29.309901
354.059851	14601.110486	29.314919
354.734406	14625.079523	29.319936
354.902787	14656.893138	29.324954
355.429822	14675.753307	29.329972
355.550141	14701.356191	29.334989
355.826572	14735.657489	29.340007
356.565027	14762.436939	29.345024
356.751599	14792.125698	29.350042
357.336718	14815.578336	29.355060
357.814772	14846.778755	29.360077
358.082056	14869.620893	29.365095
358.618393	14889.165139	29.370112
358.879224	14905.862605	29.375130
359.417205	14923.407533	29.380148
359.869354	14948.194820	29.385165
360.023624	14964.135183	29.390183
360.511466	14988.405347	29.395200
360.945201	15013.843006	29.400218
361.340397	15042.924894	29.405236
361.627655	15067.580100	29.410253
361.937620	15095.206792	29.415271
361.926076	15107.718058	29.420288
362.499164	15134.495354	29.425306
362.607414	15157.056253	29.430324
363.159007	15174.375063	29.435341
363.646334	15203.332316	29.440359
363.829875	15226.680596	29.445376
364.112527	15261.411385	29.450394
364.524929	15284.998869	29.455412
365.264463	15313.329601	29.460429
365.544038	15329.809763	29.465447
366.213485	15346.952472	29.470464
366.347057	15375.181825	29.475482
366.536605	15397.013438	29.480500
366.852209	15418.945462	29.485517
367.157208	15438.538921	29.490535
367.594289	15462.024877	29.495552
368.188022	15471.530268	29.500570
368.653857	15486.544575	29.505588
369.388352	15506.358638	29.510605
369.759377	15525.796629	29.515623
370.158454	15512.684652	29.520640
369.993405	15542.088231	29.525658
370.798600	15548.762541	29.530676
371.179145	15563.082741	29.535693
371.512244	15577.233477	29.540711
371.897668	15600.212853	29.545728
371.570544	15613.547351	29.550746
372.069741	15633.366595	29.555764
372.383478	15652.415694	29.560781
372.710664	15673.471371	29.565799
373.218284	15692.509276	29.570816
373.382303	15721.520808	29.575834
373.514704	15741.612031	29.580852
373.964563	15760.128405	29.585869
373.962727	15800.112458	29.590887
374.941408	15821.483765	29.595904
375.633834	15853.113566	29.600922
375.690630	15877.537242	29.605940
376.126220	15901.905136	29.610957
376.682941	15931.102196	29.615975
376.939599	15948.489735	29.620992
377.299918	15979.091307	29.626010
377.710899	15990.593036	29.631028
378.201200	16016.462232	29.636045
378.626728	16048.332881	29.641063
378.597098	16061.043402	29.646080
378.979910	16090.131971	29.651098
379.192851	16116.805639	29.656116
379.614189	16148.711850	29.661133
379.887317	16186.054588	29.666151
380.487502	16203.928954	29.671168
380.853350	16243.187119	29.676186
380.994116	16276.109994	29.681204
381.382801	16309.736545	29.686221
381.733395	16340.965565	29.691239
382.691161	16356.712515	29.696256
383.249305	16395.094610	29.701274
383.578178	16419.880891	29.706292
384.317436	16432.212968	29.711309
384.985923	16449.268385	29.716327
384.971356	16464.610923	29.721344
385.343791	16481.933545	29.726362
385.705116	16508.632034	29.731380
386.368212	16524.699778	29.736397
386.384087	16541.897936	29.741415
386.837256	16565.205873	29.746432
387.049846	16583.819993	29.751450
387.234204	16613.720380	29.756468
387.895012	16639.942883	29.761485
387.995040	16672.556938	29.766503
388.586990	16694.106292	29.771520
388.796164	16722.126878	29.776538
389.257877	16747.202428	29.781556
389.534209	16778.380553	29.786573
389.470353	16808.575719	29.791591
389.823378	16840.541091	29.796608
390.755364	16870.672915	29.801626
391.075635	16898.344824	29.806644
391.712761	16913.500985	29.811661
391.785375	16940.990418	29.816679
392.185836	16965.886281	29.821696
392.646034	16992.295262	29.826714
392.774310	17016.383934	29.831732
394.214513	17030.758200	29.836749
394.785186	17038.154939	29.841767
395.326869	17051.074068	29.846784
395.880370	17065.627464	29.851802
396.094534	17064.198047	29.856820
396.358402	17070.859258	29.861837
396.824702	17088.297313	29.866855
397.283758	17094.956572	29.871872
397.257338	17102.740032	29.876890
397.505088	17134.573834	29.881908
398.231577	17145.357537	29.886925
398.431803	17160.247110	29.891943
398.477646	17181.752532	29.896960
398.532701	17198.967287	29.901978
398.820293	17221.786961	29.906996
399.562239	17249.204218	29.912013
399.330460	17284.824181	29.917031
399.819926	17307.122957	29.922048
400.013531	17344.252911	29.927066
400.635042	17373.997984	29.932084
401.112903	17408.806502	29.937101
401.545851	17440.507745	29.942119
402.180682	17468.033588	29.947136
402.511854	17490.647806	29.952154
402.411165	17527.261705	29.957172
403.089455	17560.387366	29.962189
402.798788	17601.133962	29.967207
403.490419	17630.281019	29.972224
403.983754	17659.212621	29.977242
404.352303	17698.732339	29.982260
404.672041	17735.012698	29.987277
405.344520	17770.568586	29.992295
406.198251	17797.182728	29.997312
407.329919	17817.436413	30.002330
407.674150	17840.933421	30.007348
408.650513	17847.806158	30.012365
408.812868	17872.714993	30.017383
409.605494	17877.019960	30.022400
409.736681	17896.166035	30.027418
409.899180	17918.863871	30.032436
410.454055	17930.754985	30.037453
410.752408	17961.214586	30.042471
411.347419	17971.861292	30.047488
411.483299	17977.557248	30.052506
411.532821	18002.635431	30.057524
411.864105	18028.269924	30.062541
412.139019	18064.065131	30.067559
412.688661	18083.866420	30.072576
413.013778	18102.565567	30.077594
413.195322	18142.431172	30.082612
413.985046	18163.496536	30.087629
414.298689	18200.650511	30.092647
414.310813	18223.858550	30.097664
415.000606	18248.414110	30.102682
415.388297	18280.319616	30.107700
416.255292	18302.769243	30.112717
416.231449	18326.595791	30.117735
416.860812	18348.242252	30.122752
417.352301	18368.728848	30.127770
417.553998	18406.203880	30.132788
418.082963	18427.341715	30.137805
418.423930	18456.765722	30.142823
418.781046	18478.947473	30.147840
419.374750	18498.255885	30.152858
419.808961	18545.291189	30.157876
420.312070	18562.472150	30.162893
420.347532	18600.042928	30.167911
420.696123	18621.935566	30.172928
421.398119	18644.190166	30.177946
421.629165	18667.522591	30.182964
422.409535	18682.525179	30.187981
422.438071	18708.889996	30.192999
422.946405	18733.626043	30.198016
423.594136	18753.703354	30.203034
423.484365	18778.478827	30.208052
424.202959	18809.537680	30.213069
424.362467	18830.746108	30.218087
424.646269	18858.657093	30.223104
425.298339	18887.843795	30.228122
425.547755	18927.776257	30.233140
426.261709	18940.072825	30.238157
427.002737	18970.616719	30.243175
427.041536	18992.734897	30.248192
427.541843	19021.983332	30.253210
427.642412	19053.776869	30.258228
428.286724	19080.084231	30.263245
428.711130	19115.504317	30.268263
428.963929	19151.462914	30.273280
429.714514	19169.768336	30.278298
429.866881	19213.620810	30.283316
430.644305	19248.506037	30.288333
430.454195	19272.037425	30.293351
430.868023	19311.275403	30.298368
431.430047	19340.476803	30.303386
432.068684	19372.161823	30.308404
432.678056	19400.484096	30.313421
433.093928	19426.006183	30.318439
433.754574	19461.661785	30.323456
434.732306	19485.769752	30.328474
434.786299	19510.059463	30.333492
435.522659	19530.945093	30.338509
435.809138	19559.962279	30.343527
436.041694	19579.883958	30.348544
436.456153	19607.390292	30.353562
436.911138	19649.370789	30.358580
437.606398	19673.870446	30.363597
437.931154	19692.950251	30.368615
437.933552	19731.545530	30.373632
438.649283	19756.446445	30.378650
439.328861	19774.839307	30.383668
440.436259	19785.773683	30.388685
440.650148	19807.271648	30.393703
440.888976	19824.299017	30.398720
441.562047	19845.226427	30.403738
441.904282	19869.629659	30.408756
442.212292	19885.806032	30.413773
442.882361	19913.816344	30.418791
442.610267	19946.433819	30.423808
443.124419	19967.569320	30.428826
443.607280	19992.171941	30.433844
443.846758	20030.825671	30.438861
444.200345	20052.453789	30.443879
444.239915	20093.602765	30.448896
444.597686	20117.359456	30.453914
445.246233	20160.801961	30.458932
445.637548	20204.651052	30.463949
446.044647	20238.780684	30.468967
446.358035	20274.416018	30.473984
446.881559	20308.742460	30.479002
447.536108	20343.623506	30.484020
448.219518	20372.624333	30.489037
449.073252	20402.837027	30.494055
449.609183	20435.070481	30.499072
449.940841	20457.738625	30.504090
450.220845	20481.330959	30.509108
450.650708	20511.079089	30.514125
451.258713	20537.975339	30.519143
451.097881	20568.883275	30.524160
451.711124	20583.591131	30.529178
451.794672	20611.971752	30.534196
452.529943	20648.022265	30.539213
452.929069	20682.065457	30.544231
453.558083	20711.511208	30.549248
454.108680	20735.428176	30.554266
454.284159	20771.446019	30.559284
454.625320	20797.190030	30.564301
455.387999	20815.716257	30.569319
455.669389	20843.194501	30.574336
456.870569	20869.821952	30.579354
456.723921	20901.271569	30.584372
457.115928	20934.362257	30.589389
457.939011	20958.913129	30.594407
458.170436	20993.147244	30.599424
458.658062	21026.507522	30.604442
459.140554	21059.426378	30.609460
459.540058	21090.172082	30.614477
460.031752	21118.401439	30.619495
460.263832	21150.689692	30.624512
460.775353	21181.039002	30.629530
461.147361	21220.729605	30.634548
461.415416	21257.757495	30.639565
462.065787	21291.244528	30.644583
462.301188	21326.963417	30.649600
463.174536	21363.063251	30.654618
463.642163	21400.673224	30.659636
463.899114	21421.787154	30.664653
464.706137	21454.738288	30.669671
464.765048	21496.417938	30.674688
465.435192	21520.374119	30.679706
466.242809	21561.147546	30.684724
466.197449	21598.654524	30.689741
467.224491	21635.874572	30.694759
467.807825	21673.233270	30.699776
468.132486	21693.894658	30.704794
469.039322	21723.696741	30.709812
469.264243	21753.188008	30.714829
470.195480	21773.186384	30.719847
470.490506	21805.143668	30.724864
471.229421	21826.770623	30.729882
471.692458	21847.252667	30.734900
471.738221	21878.174725	30.739917
472.377847	21892.948963	30.744935
472.879175	21925.544091	30.749952
473.201205	21937.562369	30.754970
473.709322	21967.079373	30.759988
474.119329	21995.948245	30.765005
474.260284	22018.148711	30.770023
474.920499	22035.251408	30.775040
475.722038	22070.055774	30.780058
475.939568	22094.209488	30.785076
476.751845	22124.469203	30.790093
477.285186	22152.832571	30.795111
477.574495	22173.323044	30.800128
478.231693	22199.695785	30.805146
478.634725	22219.182894	30.810164
478.687833	22248.057147	30.815181
478.907975	22261.424721	30.820199
479.433487	22299.671902	30.825216
480.087774	22330.594714	30.830234
480.800465	22364.257113	30.835252
480.869410	22397.021432	30.840269
481.438129	22425.562927	30.845287
481.859190	22465.349499	30.850304
482.132272	22497.740993	30.855322
482.225296	22523.911336	30.860340
482.680696	22556.723175	30.865357
483.373283	22585.195067	30.870375
483.933172	22631.196978	30.875392
484.437752	22657.992173	30.880410
484.710152	22701.182912	30.885428
484.644938	22739.188010	30.890445
484.941740	22776.422796	30.895463
485.773611	22824.133127	30.900480
486.177391	22865.724062	30.905498
486.653224	22905.465078	30.910516
487.063917	22948.445260	30.915533
487.618881	22988.464792	30.920551
487.863777	23035.685673	30.925568
488.504221	23081.284316	30.930586
489.232192	23120.657927	30.935604
489.614129	23164.388688	30.940621
490.684824	23194.685640	30.945639
491.657682	23235.778026	30.950656
492.053057	23271.709326	30.955674
492.722243	23294.991682	30.960692
493.265005	23323.671212	30.965709
494.155443	23349.661633	30.970727
494.809092	23378.109133	30.975744
495.287588	23407.854064	30.980762
495.626466	23429.532416	30.985780
496.016773	23467.904006	30.990797
496.854077	23486.850830	30.995815
496.636733	23525.304490	31.000832
496.912354	23558.234441	31.005850
497.595154	23583.031593	31.010868
497.933299	23622.681737	31.015885
498.775308	23647.233016	31.020903
499.036549	23690.718322	31.025920
499.234231	23729.341573	31.030938
499.942698	23759.171292	31.035956
500.080340	23803.895680	31.040973
500.598369	23839.448721	31.045991
500.966897	23881.976188	31.051008
501.170738	23925.426708	31.056026
502.020132	23955.165271	31.061044
501.873921	24006.462033	31.066061
502.651533	24051.643438	31.071079
503.583174	24096.876798	31.076096
503.723561	24151.541706	31.081114
504.623239	24187.863777	31.086132
505.122370	24232.956242	31.091149
506.073436	24272.360597	31.096167
506.792932	24309.109055	31.101184
506.918361	24345.488753	31.106202
507.631061	24377.410436	31.111220
508.364777	24421.512588	31.116237
508.719654	24448.737944	31.121255
509.071548	24490.713194	31.126272
509.721856	24522.518435	31.131290
510.464293	24551.339272	31.136308
511.053383	24588.601459	31.141325
511.752837	24621.334477	31.146343
512.207069	24645.915761	31.151360
512.578474	24685.095201	31.156378
513.460192	24711.783900	31.161396
513.452678	24744.721970	31.166413
514.338327	24764.414502	31.171431
515.040187	24790.429846	31.176448
515.215170	24817.494126	31.181466
516.192148	24843.744767	31.186484
516.439838	24871.101135	31.191501
516.823595	24892.236936	31.196519
517.379738	24927.722787	31.201536
517.366597	24953.059714	31.206554
518.257420	24983.437954	31.211572
518.379464	25012.248607	31.216589
518.548748	25041.930362	31.221607
519.376715	25076.110252	31.226624
519.836931	25116.401591	31.231642
520.403675	25143.133581	31.236660
520.859926	25176.790110	31.241677
521.252013	25217.496712	31.246695
521.780949	25249.353602	31.251712
522.115321	25284.425918	31.256730
523.061064	25312.792790	31.261748
523.363103	25360.680156	31.266765
523.852486	25394.730031	31.271783
524.449945	25428.624105	31.276800
524.921768	25466.727738	31.281818
525.498955	25504.960394	31.286836
525.871481	25546.024609	31.291853
526.195675	25582.824308	31.296871
527.045015	25614.398070	31.301888
527.455058	25667.217693	31.306906
528.252530	25696.252805	31.311924
528.429985	25735.540328	31.316941
528.959937	25776.978652	31.321959
529.953812	25815.007995	31.326976
530.282061	25858.285345	31.331994
531.127348	25889.645298	31.337012
531.492180	25925.548205	31.342029
531.794287	25963.255772	31.347047
532.329218	25996.256804	31.352064
532.848880	26045.439087	31.357082
533.750174	26080.095903	31.362100
534.473528	26124.987082	31.367117
534.630432	26163.602412	31.372135
535.259838	26202.890007	31.377152
535.599991	26241.451679	31.382170
536.180399	26282.522954	31.387188
536.740667	26331.092900	31.392205
536.924835	26362.328993	31.397223
537.963262	26399.202274	31.402240
538.193847	26448.398943	31.407258
538.653801	26488.452912	31.412276
539.161819	26538.674690	31.417293
539.418069	26583.905048	31.422311
540.186620	26622.666198	31.427328
540.643157	26685.637550	31.432346
541.212923	26723.810475	31.437364
542.088506	26763.895088	31.442381
542.670788	26814.118629	31.447399
543.319985	26843.880011	31.452416
544.167718	26871.537533	31.457434
545.183045	26900.685832	31.462452
545.754467	26942.644666	31.467469
546.387193	26968.939043	31.472487
546.812953	26991.915994	31.477504
546.973612	27042.117256	31.482522
547.812017	27063.816579	31.487540
548.058331	27095.941594	31.492557
548.602103	27137.070872	31.497575
549.152953	27168.333289	31.502592
549.545544	27215.869670	31.507610
550.204873	27255.205217	31.512628
550.745758	27291.405477	31.517645
551.447239	27330.241628	31.522663
551.831496	27365.094907	31.527680
551.857559	27408.251973	31.532698
552.229275	27438.183832	31.537716
553.065037	27479.363153	31.542733
553.003872	27528.310809	31.547751
553.935979	27563.685893	31.552768
553.997116	27609.561987	31.557786
554.701695	27643.727524	31.562804
555.004961	27696.771325	31.567821
555.894686	27738.277751	31.572839
556.801403	27788.244627	31.577856
556.903296	27827.194033	31.582874
556.891644	27878.056226	31.587892
557.987200	27924.340834	31.592909
558.532449	27972.006910	31.597927
559.160004	28002.942650	31.602944
560.101668	28052.272689	31.607962
560.743638	28092.111878	31.612980
561.518535	28136.146229	31.617997
561.639989	28179.486015	31.623015
562.324325	28226.549547	31.628032
563.051454	28278.903147	31.633050
563.520559	28303.353845	31.638068
564.331856	28359.271984	31.643085
564.714444	28403.089880	31.648103
565.704691	28433.325112	31.653120
566.119136	28483.307125	31.658138
566.627339	28516.809434	31.663156
567.134864	28548.883440	31.668173
567.964937	28598.358588	31.673191
568.492475	28643.140455	31.678208
568.734683	28686.961852	31.683226
569.227292	28730.877097	31.688244
569.653503	28781.989413	31.693261
570.073425	28825.536933	31.698279
571.005610	28868.644519	31.703296
571.562816	28922.909803	31.708314
572.436401	28956.988028	31.713332
573.032754	28995.767876	31.718349
573.680944	29039.115977	31.723367
574.533050	29083.595452	31.728384
574.973899	29121.533797	31.733402
575.512647	29165.796759	31.738420
575.883623	29210.168105	31.743437
576.546462	29246.529839	31.748455
577.024198	29284.222552	31.753472
577.526182	29335.153791	31.758490
577.918040	29385.994845	31.763508
578.451825	29431.200966	31.768525
579.393317	29481.071765	31.773543
579.911752	29520.117574	31.778560
580.169199	29575.505810	31.783578
580.676237	29622.347321	31.788596
581.270847	29665.951607	31.793613
581.776262	29719.259953	31.798631
582.604816	29769.762173	31.803648
583.084639	29826.033013	31.808666
583.892004	29874.983818	31.813684
584.300387	29917.454557	31.818701
585.150822	29962.157437	31.823719
585.877020	30008.624373	31.828736
586.507796	30046.806670	31.833754
586.976066	30084.622428	31.838772
587.358841	30127.091265	31.843789
588.010961	30166.541007	31.848807
589.006060	30208.111906	31.853824
589.325476	30263.056188	31.858842
589.858530	30301.431163	31.863860
590.662320	30343.442994	31.868877
591.110149	30393.437109	31.873895
591.669200	30432.560504	31.878912
592.296128	30478.051525	31.883930
593.103540	30516.270408	31.888948
593.634963	30548.710456	31.893965
594.331290	30581.889756	31.898983
595.173523	30599.786858	31.904000
595.786355	30640.482592	31.909018
595.943066	30676.596945	31.914036
596.795515	30706.016260	31.919053
597.211722	30736.755148	31.924071
597.314783	30774.489957	31.929088
597.794597	30821.426934	31.934106
598.081864	30865.245962	31.939124
599.074246	30913.430837	31.944141
599.393005	30968.440314	31.949159
599.949518	31014.190012	31.954176
600.993659	31066.488735	31.959194
601.146592	31116.814973	31.964212
602.307449	31155.422519	31.969229
602.547284	31201.727647	31.974247
603.381810	31251.189531	31.979264
604.764194	31295.022312	31.984282
604.714887	31325.379397	31.989300
605.664404	31373.186408	31.994317
605.945104	31414.302018	31.999335
606.669563	31463.339039	32.004352
606.940706	31500.846717	32.009370
607.654716	31560.284529	32.014388
608.432186	31595.709624	32.019405
608.519831	31652.286714	32.024423
609.321066	31700.427322	32.029440
610.021269	31745.909727	32.034458
610.555668	31791.576084	32.039476
611.939299	31835.593144	32.044493
611.562082	31900.922894	32.049511
612.064790	31948.453097	32.054528
613.266891	31996.892325	32.059546
613.819936	32043.017816	32.064564
614.909384	32089.325417	32.069581
615.168627	32146.800111	32.074599
615.801108	32184.347599	32.079616
616.510921	32228.666364	32.084634
617.402590	32271.591411	32.089652
618.127400	32309.940261	32.094669
618.578110	32357.308806	32.099687
619.170327	32398.656030	32.104704
620.040769	32439.681863	32.109722
620.374363	32493.826982	32.114740
621.275701	32532.028647	32.119757
621.520641	32574.821089	32.124775
622.274739	32620.872310	32.129792
623.139928	32660.641343	32.134810
623.930987	32711.681305	32.139828
624.337300	32742.393097	32.144845
625.066120	32784.352012	32.149863
625.409443	32834.494721	32.154880
626.184235	32873.279365	32.159898
626.400704	32924.358720	32.164916
627.211672	32976.559475	32.169933
627.469574	33020.887057	32.174951
627.873605	33073.758315	32.179968
628.728903	33116.640190	32.184986
629.736586	33165.207237	32.190004
630.566187	33210.830751	32.195021
631.194103	33250.751644	32.200039
631.821747	33295.509049	32.205056
632.445657	33327.370057	32.210074
633.059881	33373.248728	32.215092
633.554616	33414.543597	32.220109
633.908806	33460.993999	32.225127
634.377689	33511.333736	32.230144
635.046662	33547.853811	32.235162
635.819981	33593.094948	32.240180
636.840530	33627.158005	32.245197
637.656987	33667.183108	32.250215
637.889020	33713.109376	32.255232
638.605716	33749.407419	32.260250
638.739848	33790.449376	32.265268
639.915648	33834.585212	32.270285
640.276300	33880.574013	32.275303
640.615944	33919.049003	32.280320
641.501332	33969.192234	32.285338
642.211188	34018.768614	32.290356
642.768799	34066.655464	32.295373
643.268929	34109.436607	32.300391
644.214310	34162.694192	32.305408
644.991618	34212.039246	32.310426
645.333768	34276.398256	32.315444
645.884006	34319.538724	32.320461
646.215204	34364.420428	32.325479
646.729910	34416.664569	32.330496
647.451796	34471.810199	32.335514
648.405720	34536.327664	32.340532
648.669930	34588.687097	32.345549
649.396320	34647.063268	32.350567
649.856347	34718.410598	32.355584
650.569430	34769.530938	32.360602
651.125258	34841.192540	32.365620
651.589954	34894.634290	32.370637
652.533497	34945.434665	32.375655
653.143953	35017.423458	32.380672
654.442299	35075.035258	32.385690
655.148565	35127.175468	32.390708
656.373258	35160.791943	32.395725
657.796019	35185.121275	32.400743
658.390100	35231.999796	32.405760
659.408102	35260.464021	32.410778
660.132515	35301.650970	32.415796
660.607019	35332.305355	32.420813
661.293407	35364.418958	32.425831
661.307682	35404.831478	32.430848
662.095037	35438.301505	32.435866
662.381166	35485.677441	32.440884
663.127236	35528.176590	32.445901
663.687552	35570.565640	32.450919
663.890576	35620.325852	32.455936
664.992499	35668.858726	32.460954
665.726485	35726.326216	32.465972
666.391400	35761.965573	32.470989
667.015054	35812.798864	32.476007
667.510806	35864.682813	32.481024
668.681603	35919.186961	32.486042
668.693359	35963.995332	32.491060
669.455152	36014.769666	32.496077
670.275107	36072.104575	32.501095
670.922917	36117.541391	32.506112
671.665711	36158.082206	32.511130
672.130337	36214.555988	32.516148
672.529232	36255.169493	32.521165
673.309829	36310.829264	32.526183
673.817916	36371.318116	32.531200
674.375908	36429.358685	32.536218
675.194579	36483.729409	32.541236
675.632403	36534.637617	32.546253
675.982879	36585.894667	32.551271
676.777984	36655.672497	32.556288
677.393225	36705.390047	32.561306
678.239382	36762.931402	32.566324
678.614205	36822.765708	32.571341
679.525676	36876.863740	32.576359
679.705850	36935.046702	32.581376
680.623732	36986.627393	32.586394
681.165599	37042.648723	32.591412
681.873017	37110.702811	32.596429
682.915239	37160.683761	32.601447
683.107727	37225.985566	32.606464
683.849719	37291.176734	32.611482
684.820123	37346.057192	32.616500
685.434733	37396.016734	32.621517
686.554306	37447.465969	32.626535
687.859494	37498.292039	32.631552
688.421738	37541.266462	32.636570
689.312788	37593.839241	32.641588
689.930824	37640.194502	32.646605
690.318405	37685.928106	32.651623
690.898231	37745.227208	32.656640
691.722961	37804.355558	32.661658
692.263250	37855.446989	32.666676
693.005760	37910.667898	32.671693
693.414503	37963.847836	32.676711
693.713984	38022.369294	32.681728
694.901931	38075.504092	32.686746
695.351344	38138.289865	32.691764
695.836669	38203.245530	32.696781
697.075150	38265.580016	32.701799
697.895338	38326.126989	32.706816
698.470327	38374.773352	32.711834
699.174336	38436.483293	32.716852
699.800827	38494.733805	32.721869
700.991456	38550.088956	32.726887
701.238725	38613.969957	32.731904
702.093241	38666.810323	32.736922
703.256159	38725.711501	32.741940
703.634225	38776.805081	32.746957
704.380910	38831.705198	32.751975
704.876334	38896.674030	32.756992
705.453970	38954.655146	32.762010
706.291936	39003.742599	32.767028
706.906803	39066.201779	32.772045
707.733807	39126.288305	32.777063
708.388489	39190.847478	32.782080
709.180475	39248.271137	32.787098
709.714831	39309.402897	32.792116
710.242396	39371.465499	32.797133
710.841108	39431.727538	32.802151
711.517354	39505.302183	32.807168
712.043464	39577.793760	32.812186
713.108390	39641.904657	32.817204
713.599664	39714.794200	32.822221
714.097776	39778.728130	32.827239
715.009933	39845.962176	32.832256
715.796727	39923.694891	32.837274
716.839310	39980.411133	32.842292
717.131775	40046.610260	32.847309
718.256146	40112.654790	32.852327
718.561607	40184.183533	32.857344
719.950220	40248.789712	32.862362
720.662009	40298.323463	32.867380
721.522584	40367.110248	32.872397
722.534648	40424.869568	32.877415
722.978953	40477.632760	32.882432
724.030936	40542.659021	32.887450
724.338364	40591.396291	32.892468
725.296625	40652.756763	32.897485
725.721032	40696.207949	32.902503
726.364372	40757.839090	32.907520
727.354868	40807.090290	32.912538
728.639238	40852.286237	32.917556
728.697264	40911.188281	32.922573
729.609818	40953.103069	32.927591
730.295019	41002.901861	32.932608
730.889294	41044.714587	32.937626
731.718295	41094.586068	32.942644
732.173049	41152.668079	32.947661
732.872761	41209.504148	32.952679
733.465636	41277.943368	32.957696
734.336614	41328.833411	32.962714
735.328425	41386.908335	32.967732
736.467062	41445.017477	32.972749
736.983160	41487.266962	32.977767
737.419790	41547.085755	32.982784
737.835580	41608.470117	32.987802
738.760316	41663.223187	32.992820
739.389621	41729.419257	32.997837
740.127890	41789.855838	33.002855
740.780181	41855.998116	33.007872
741.070640	41927.364141	33.012890
742.032833	41999.909732	33.017908
742.749437	42058.219019	33.022925
743.571615	42129.996254	33.027943
744.408625	42191.209156	33.032960
745.354560	42249.540174	33.037978
746.109171	42312.309473	33.042996
746.541160	42392.180725	33.048013
747.401050	42449.924817	33.053031
748.794041	42505.132054	33.058048
749.695592	42565.172189	33.063066
751.271077	42615.202898	33.068084
752.073454	42663.798160	33.073101
753.278053	42701.534392	33.078119
754.054559	42747.825297	33.083136
754.626306	42793.439787	33.088154
755.323736	42835.271497	33.093172
755.842681	42890.811837	33.098189
757.217657	42921.457007	33.103207
757.651529	42967.795387	33.108224
758.047391	43021.071916	33.113242
759.184080	43062.759781	33.118260
759.315592	43118.677253	33.123277
760.114069	43166.559510	33.128295
760.938930	43218.751413	33.133312
761.278370	43268.172748	33.138330
762.147269	43317.688874	33.143348
762.718699	43382.437848	33.148365
763.619810	43433.625357	33.153383
764.032466	43500.113482	33.158400
764.711466	43551.411741	33.163418
765.817601	43624.250209	33.168436
766.402823	43682.894180	33.173453
767.263648	43740.881864	33.178471
767.862921	43809.195136	33.183488
768.461399	43870.949524	33.188506
769.151160	43927.364053	33.193524
769.789737	43998.613009	33.198541
770.803719	44061.429136	33.203559
771.397156	44127.277453	33.208576
772.122871	44198.488184	33.213594
772.910345	44257.760020	33.218612
773.527877	44326.495836	33.223629
774.207919	44391.230849	33.228647
775.054302	44460.152840	33.233664
775.854926	44529.196025	33.238682
776.563979	44599.436527	33.243700
777.517844	44668.412012	33.248717
778.318972	44730.459838	33.253735
779.035432	44779.041495	33.258752
779.611189	44832.667573	33.263770
780.500507	44904.601501	33.268788
781.584121	44952.721552	33.273805
782.252030	45017.321112	33.278823
782.824697	45077.577397	33.283840
783.558015	45131.957708	33.288858
784.210339	45204.138238	33.293876
785.032181	45261.724797	33.298893
786.119428	45331.383709	33.303911
786.830662	45396.483671	33.308928
787.357690	45461.359471	33.313946
788.721197	45511.537270	33.318964
789.572900	45582.397551	33.323981
790.362928	45632.848339	33.328999
791.036808	45699.302367	33.334016
791.833649	45766.610402	33.339034
792.849134	45835.244637	33.344052
793.422877	45898.564626	33.349069
793.910315	45961.974137	33.354087
795.131505	46027.363445	33.359104
795.971352	46089.377389	33.364122
796.997263	46153.513324	33.369140
797.743080	46219.489584	33.374157
798.552104	46287.379264	33.379175
798.992768	46340.074778	33.384192
799.640354	46401.670376	33.389210
801.088482	46464.760961	33.394228
801.844873	46540.092552	33.399245
802.516001	46598.832027	33.404263
803.363417	46663.800601	33.409280
803.945934	46734.105455	33.414298
804.483170	46797.547527	33.419316
805.300048	46865.241621	33.424333
805.963468	46943.714094	33.429351
806.897594	47009.979661	33.434368
807.236824	47099.055030	33.439386
807.994326	47168.353452	33.444404
809.091916	47248.499081	33.449421
810.275412	47327.239866	33.454439
810.712702	47392.748844	33.459456
811.398237	47484.972871	33.464474
812.311207	47550.256429	33.469492
813.637469	47629.361942	33.474509
814.054031	47699.860117	33.479527
815.011698	47777.498896	33.484544
815.894707	47845.653778	33.489562
816.672441	47923.491877	33.494580
817.531188	48004.132857	33.499597
818.070302	48079.781762	33.504615
819.134847	48151.452071	33.509632
819.832291	48220.782042	33.514650
821.029310	48302.231816	33.519668
821.779302	48377.222568	33.524685
822.407910	48443.027446	33.529703
823.406115	48522.092244	33.534720
823.946153	48593.782330	33.539738
824.841011	48664.936593	33.544756
825.655772	48731.896389	33.549773
826.809196	48808.325154	33.554791
828.133663	48873.200499	33.559808
828.784103	48936.592973	33.564826
829.493286	49012.566467	33.569844
830.425142	49070.303787	33.574861
830.990013	49139.587599	33.579879
831.778519	49192.577239	33.584896
832.414319	49267.247054	33.589914
833.245603	49327.841369	33.594932
834.529468	49400.177407	33.599949
835.256984	49451.120951	33.604967
835.910361	49509.548060	33.609984
836.652440	49569.150945	33.615002
837.515543	49651.138353	33.620020
837.876604	49703.113831	33.625037
838.720531	49781.827399	33.630055
839.551298	49854.671957	33.635072
840.246287	49926.493948	33.640090
841.889569	49999.130236	33.645108
843.288257	50050.571692	33.650125
844.278851	50109.023759	33.655143
845.062309	50159.770363	33.660160
845.870200	50226.052294	33.665178
846.440102	50284.083118	33.670196
847.178089	50350.667331	33.675213
847.730666	50413.307233	33.680231
848.527637	50481.274586	33.685248
849.442329	50558.075362	33.690266
850.350174	50625.399502	33.695284
851.095454	50701.898122	33.700301
851.899003	50777.774194	33.705319
852.671295	50838.040017	33.710336
853.440037	50917.433525	33.715354
854.272034	50993.533657	33.720372
855.379708	51072.520617	33.725389
855.818870	51144.379904	33.730407
856.477421	51231.245104	33.735424
857.365154	51313.101728	33.740442
858.505551	51391.078649	33.745460
859.436504	51468.942908	33.750477
860.086233	51553.729009	33.755495
861.125273	51636.537631	33.760512
861.688953	51712.688223	33.765530
862.531216	51796.666976	33.770548
863.521873	51880.958285	33.775565
864.503227	51965.833473	33.780583
865.020283	52043.808384	33.785600
865.970823	52133.656039	33.790618
866.648370	52224.679161	33.795636
867.913911	52310.511117	33.800653
868.354144	52397.895561	33.805671
869.297157	52489.093530	33.810688
870.445818	52570.439401	33.815706
871.428310	52655.690258	33.820724
872.783316	52739.548305	33.825741
873.632384	52818.176495	33.830759
874.646451	52893.121860	33.835776
875.816365	52968.093827	33.840794
876.831985	53047.253701	33.845812
878.267988	53105.732592	33.850829
878.825012	53187.147401	33.855847
879.623582	53253.047117	33.860864
880.123766	53315.905498	33.865882
880.915121	53390.235362	33.870900
882.083461	53464.139764	33.875917
883.078509	53542.007307	33.880935
883.815770	53611.195411	33.885952
884.914727	53683.927993	33.890970
885.850989	53752.731174	33.895988
886.758362	53823.931016	33.901005
887.124978	53904.068070	33.906023
888.209809	53960.863574	33.911040
889.449615	54024.178240	33.916058
889.899770	54092.684735	33.921076
891.271054	54160.573441	33.926093
891.703532	54234.385992	33.931111
893.093973	54281.592000	33.936128
893.854086	54339.938721	33.941146
894.357989	54411.753693	33.946164
895.207188	54464.556096	33.951181
895.781723	54538.107017	33.956199
896.355611	54606.083166	33.961216
897.573770	54672.434133	33.966234
898.756905	54743.150860	33.971252
899.747929	54806.487374	33.976269
899.958044	54881.918617	33.981287
901.151190	54944.667155	33.986304
902.358821	55010.666330	33.991322
903.111014	55083.640738	33.996340
904.210084	55160.668442	34.001357
904.727331	55238.489408	34.006375
905.504331	55308.676187	34.011392
906.921770	55385.395602	34.016410
907.402278	55463.710310	34.021428
908.053097	55525.620867	34.026445
909.339985	55615.701617	34.031463
910.421733	55691.803467	34.036480
910.899522	55769.562705	34.041498
912.108811	55846.113502	34.046516
913.149571	55921.773147	34.051533
914.333673	56002.346969	34.056551
914.785699	56066.808635	34.061568
916.066021	56137.476429	34.066586
916.926799	56220.139115	34.071604
917.874116	56298.934497	34.076621
918.886647	56374.859451	34.081639
919.699946	56447.720953	34.086656
920.649036	56526.434540	34.091674
921.345939	56613.940214	34.096692
922.425121	56681.571520	34.101709
923.118246	56768.059426	34.106727
924.239156	56847.165020	34.111744
925.280384	56937.054848	34.116762
925.595329	57021.919087	34.121780
926.816744	57092.446991	34.126797
927.973456	57179.016111	34.131815
928.400958	57258.237331	34.136832
929.751816	57332.751961	34.141850
930.776150	57429.006787	34.146868
931.602050	57499.534168	34.151885
932.398913	57589.059430	34.156903
933.935288	57663.242421	34.161920
935.041907	57746.580959	34.166938
935.821457	57822.660696	34.171956
937.166607	57891.950195	34.176973
938.158470	57971.193511	34.181991
939.091686	58036.319747	34.187008
940.169708	58097.885663	34.192026
940.565552	58174.766745	34.197044
941.747942	58238.069934	34.202061
942.863201	58317.105308	34.207079
943.765102	58391.648806	34.212096
944.843899	58450.430675	34.217114
945.598706	58535.276089	34.222132
946.470187	58613.989618	34.227149
947.288534	58675.280971	34.232167
948.286927	58753.171387	34.237184
949.375504	58822.940222	34.242202
949.997270	58898.585878	34.247220
951.022217	58979.662851	34.252237
951.944629	59055.787533	34.257255
952.779697	59137.375619	34.262272
953.805426	59207.471814	34.267290
954.460665	59287.930125	34.272308
955.192395	59361.022023	34.277325
955.756552	59432.943964	34.282343
956.588874	59513.615976	34.287360
957.663473	59594.256873	34.292378
958.204867	59681.652319	34.297396
958.888607	59754.968075	34.302413
960.174138	59847.609380	34.307431
960.609829	59934.661405	34.312448
961.620755	60026.719511	34.317466
962.329712	60123.078465	34.322484
963.438047	60219.217390	34.327501
964.511743	60315.919096	34.332519
965.630445	60408.961954	34.337536
966.807773	60496.451220	34.342554
967.992288	60594.067244	34.347572
968.901340	60680.757076	34.352589
969.848230	60779.841354	34.357607
970.553015	60875.159508	34.362624
971.553495	60971.894195	34.367642
972.653360	61072.196488	34.372660
973.518395	61173.940978	34.377677
974.701305	61265.831390	34.382695
975.996342	61356.432378	34.387712
977.539325	61437.873652	34.392730
978.606438	61519.553849	34.397748
980.338518	61601.308049	34.402765
981.656315	61679.974665	34.407783
982.824247	61759.823256	34.412800
983.839012	61823.826522	34.417818
984.373519	61904.533786	34.422836
985.459889	61974.843704	34.427853
986.152911	62048.272490	34.432871
986.868753	62121.602991	34.437888
988.184902	62194.207251	34.442906
988.764313	62289.955532	34.447924
990.104941	62370.336273	34.452941
990.974095	62451.119836	34.457959
991.475099	62539.588892	34.462976
992.561948	62626.207262	34.467994
993.622030	62722.122943	34.473012
994.312086	62789.945771	34.478029
995.442964	62886.920888	34.483047
996.503234	62974.760034	34.488064
997.513084	63059.910607	34.493082
998.333702	63156.637546	34.498100
999.341972	63248.834732	34.503117
1000.801840	63325.465071	34.508135
1001.628085	63407.100374	34.513152
1002.949602	63498.819256	34.518170
1003.795986	63579.293513	34.523188
1005.279367	63660.953969	34.528205
1006.351327	63748.724395	34.533223
1006.983579	63821.401895	34.538240
1008.348604	63903.948857	34.543258
1009.190196	63980.734431	34.548276
1010.053532	64068.608093	34.553293
1010.892466	64141.703827	34.558311
1011.712299	64236.681494	34.563328
1012.766294	64324.368111	34.568346
1013.904973	64410.262926	34.573364
1014.673352	64501.191626	34.578381
1015.770780	64583.681197	34.583399
1016.817743	64682.467963	34.588416
1017.244267	64770.519705	34.593434
1018.060179	64869.102601	34.598452
1019.139718	64957.762403	34.603469
1020.408013	65048.754549	34.608487
1021.309858	65147.369476	34.613504
1022.386528	65233.213451	34.618522
1023.154223	65314.838767	34.623540
1023.548904	65404.733655	34.628557
1025.032189	65486.469722	34.633575
1025.644510	65587.537209	34.638592
1026.732132	65685.042721	34.643610
1027.667222	65787.269990	34.648628
1028.921784	65879.634781	34.653645
1030.401180	65957.631318	34.658663
1031.290486	66053.491383	34.663680
1032.303465	66143.507913	34.668698
1033.237045	66244.945875	34.673716
1034.750864	66334.948437	34.678733
1036.199035	66420.054853	34.683751
1036.945588	66517.008866	34.688768
1037.966644	66601.675877	34.693786
1038.771270	66709.264422	34.698804
1039.771551	66795.537126	34.703821
1040.994690	66892.038508	34.708839
1042.105037	66986.386160	34.713856
1043.071356	67073.583140	34.718874
1044.064970	67163.353046	34.723892
1045.313351	67266.582188	34.728909
1046.092678	67353.068455	34.733927
1047.095439	67454.658761	34.738944
1048.150171	67561.040650	34.743962
1049.304865	67658.315366	34.748980
1050.213273	67762.568155	34.753997
1051.666289	67875.182906	34.759015
1052.126097	67985.793680	34.764032
1053.250311	68086.063279	34.769050
1054.682823	68179.567408	34.774068
1055.255688	68274.231419	34.779085
1056.749993	68379.123659	34.784103
1057.828174	68495.446535	34.789120
1058.665100	68593.622715	34.794138
1060.493193	68697.128298	34.799156
1061.420186	68791.827736	34.804173
1062.558174	68888.299248	34.809191
1063.831891	68988.808703	34.814208
1064.574593	69083.379603	34.819226
1065.879623	69178.452184	34.824244
1066.462607	69286.902866	34.829261
1067.959445	69378.311808	34.834279
1068.899665	69478.007605	34.839296
1070.030995	69576.711576	34.844314
1071.336313	69664.409139	34.849332
1072.195978	69766.227143	34.854349
1073.556935	69854.423252	34.859367
1074.328250	69957.604487	34.864384
1075.247601	70050.106161	34.869402
1076.535990	70146.805909	34.874420
1077.775271	70259.217392	34.879437
1078.846785	70352.589291	34.884455
1079.322774	70448.606099	34.889472
1080.836058	70552.459395	34.894490
1081.973616	70651.318456	34.899508
1082.938933	70756.410328	34.904525
1083.873359	70851.084473	34.909543
1085.076113	70959.711620	34.914560
1085.973574	71055.696718	34.919578
1087.139237	71154.287351	34.924596
1088.379696	71259.756358	34.929613
1089.867388	71348.317745	34.934631
1090.728291	71449.553220	34.939648
1092.049535	71544.802909	34.944666
1093.179614	71620.072053	34.949684
1093.914524	71727.027444	34.954701
1094.630307	71812.924252	34.959719
1095.577356	71896.226994	34.964736
1096.437196	71998.351307	34.969754
1097.862610	72088.660015	34.974772
1098.863024	72180.035740	34.979789
1100.207358	72264.468341	34.984807
1101.224160	72367.798187	34.989824
1102.347118	72456.990028	34.994842
1103.810850	72553.715709	34.999860
1104.348306	72648.584782	35.004877
1105.494191	72748.273705	35.009895
1106.224799	72848.458274	35.014912
1107.271650	72951.937715	35.019930
1108.626615	73070.251744	35.024948
1109.390528	73170.052375	35.029965
1110.814035	73267.382217	35.034983
1112.384445	73369.261903	35.040000
1114.100742	73457.959458	35.045018
1115.259496	73541.918394	35.050036
1116.184720	73654.893593	35.055053
1117.559031	73745.823885	35.060071
1118.738392	73836.759501	35.065088
1119.574906	73939.325581	35.070106
1120.640513	74022.211251	35.075124
1121.420489	74136.414382	35.080141
1122.643580	74229.789103	35.085159
1123.672614	74335.556623	35.090176
1124.680244	74448.889682	35.095194
1125.849242	74547.745782	35.100212
1127.081185	74659.157529	35.105229
1128.130422	74760.249678	35.110247
1129.261193	74867.244778	35.115264
1130.547850	74972.024726	35.120282
1132.361213	75077.584427	35.125300
1133.330223	75185.707972	35.130317
1134.478029	75276.324064	35.135335
1135.440527	75373.847351	35.140352
1136.758681	75465.590240	35.145370
1138.291589	75572.398888	35.150388
1139.222445	75672.626220	35.155405
1140.542465	75764.559842	35.160423
1141.682309	75862.158628	35.165440
1142.625804	75959.927667	35.170458
1144.174515	76061.453644	35.175476
1144.907115	76158.825550	35.180493
1145.843064	76255.811473	35.185511
1147.295919	76365.080482	35.190528
1147.747217	76467.424830	35.195546
1149.236057	76565.377184	35.200564
1150.332740	76669.002572	35.205581
1151.306480	76788.494419	35.210599
1152.121008	76888.896373	35.215616
1153.410870	77012.089566	35.220634
1154.247713	77124.206369	35.225652
1155.421534	77236.575204	35.230669
1156.503022	77344.005816	35.235687
1157.504877	77463.660930	35.240704
1158.495347	77585.459197	35.245722
1159.818466	77707.586262	35.250740
1160.910715	77824.936011	35.255757
1161.982849	77948.560028	35.260775
1163.584183	78068.567856	35.265792
1164.851278	78181.128747	35.270810
1166.007217	78285.967188	35.275828
1167.145878	78407.315328	35.280845
1168.571799	78514.456229	35.285863
1169.747991	78619.685506	35.290880
1170.619163	78718.337141	35.295898
1172.544833	78812.910472	35.300916
1173.512225	78923.836166	35.305933
1174.506892	79010.751359	35.310951
1175.898440	79099.885377	35.315968
1176.624615	79199.612788	35.320986
1178.390630	79292.388350	35.326004
1179.348769	79393.068502	35.331021
1180.232228	79493.469266	35.336039
1181.437127	79602.067688	35.341056
1182.775355	79702.905174	35.346074
1183.904443	79804.472363	35.351092
1184.933789	79902.989590	35.356109
1186.195498	80014.139892	35.361127
1187.260938	80121.343140	35.366144
1188.025968	80241.503271	35.371162
1189.821317	80339.902816	35.376180
1190.975556	80457.482158	35.381197
1191.981597	80561.833133	35.386215
1193.259532	80665.572064	35.391232
1193.850335	80792.767755	35.396250
1195.297084	80902.524524	35.401268
1196.246701	81025.585910	35.406285
1197.252355	81141.088146	35.411303
1198.697294	81261.830986	35.416320
1199.589965	81398.611238	35.421338
1200.601053	81529.089609	35.426356
1201.958580	81646.654979	35.431373
1203.684681	81780.165293	35.436391
1205.012599	81894.201462	35.441408
1206.076157	82026.029637	35.446426
1207.371427	82148.193265	35.451444
1208.945816	82268.679558	35.456461
1210.313691	82381.583859	35.461479
1211.572177	82493.935488	35.466496
1212.941906	82613.492187	35.471514
1214.167573	82718.399817	35.476532
1215.339806	82842.878893	35.481549
1217.058710	82966.944000	35.486567
1218.762110	83062.263203	35.491584
1219.426070	83180.094962	35.496602
1220.899913	83277.351168	35.501620
1222.169323	83390.794307	35.506637
1223.123902	83512.383332	35.511655
1224.729355	83615.309253	35.516672
1225.284324	83728.788921	35.521690
1226.796839	83834.821720	35.526708
1227.921383	83948.162921	35.531725
1229.149847	84061.868520	35.536743
1230.825206	84168.751492	35.541760
1231.836800	84293.401297	35.546778
1233.055439	84398.417584	35.551796
1234.365663	84513.417350	35.556813
1235.359845	84632.496139	35.561831
1236.818821	84749.843171	35.566848
1237.974141	84861.117822	35.571866
1239.121542	84962.434639	35.576884
1240.564629	85079.785493	35.581901
1241.277814	85193.106950	35.586919
1242.965616	85299.409326	35.591936
1243.761257	85428.938093	35.596954
1245.303696	85535.644107	35.601972
1247.003990	85643.276300	35.606989
1247.991424	85762.221426	35.612007
1249.446632	85870.095357	35.617024
1250.226083	85984.740113	35.622042
1250.849424	86099.726412	35.627060
1252.575813	86209.903647	35.632077
1253.774863	86324.687182	35.637095
1254.734533	86416.635915	35.642112
1256.032928	86531.506178	35.647130
1257.041459	86633.306652	35.652148
1258.551943	86752.085719	35.657165
1259.557945	86869.296441	35.662183
1261.081285	86964.986098	35.667200
1261.742468	87086.534496	35.672218
1263.037241	87202.725863	35.677236
1264.335182	87324.645006	35.682253
1265.198092	87458.354155	35.687271
1266.507076	87572.415849	35.692288
1267.976343	87707.096221	35.697306
1269.210839	87832.930428	35.702324
1270.526035	87958.714595	35.707341
1271.649386	88085.302182	35.712359
1273.483304	88192.479462	35.717376
1275.348379	88314.821347	35.722394
1276.760417	88424.270166	35.727412
1277.664348	88534.140640	35.732429
1279.231851	88657.962279	35.737447
1280.648881	88773.405812	35.742464
1281.957600	88882.618958	35.747482
1282.951995	89006.518589	35.752500
1284.308950	89122.124909	35.757517
1285.737010	89243.981058	35.762535
1286.857766	89364.326758	35.767552
1288.304014	89475.231539	35.772570
1289.424809	89604.994299	35.777588
1290.928115	89720.580170	35.782605
1292.177767	89857.712435	35.787623
1293.679839	89968.496307	35.792640
1294.908477	90092.186578	35.797658
1296.352406	90213.448582	35.802676
1297.997503	90326.543425	35.807693
1298.593603	90457.189987	35.812711
1300.410816	90566.026002	35.817728
1301.637979	90680.277157	35.822746
1303.099391	90795.506177	35.827764
1304.469834	90913.690092	35.832781
1306.115841	91036.723639	35.837799
1307.215904	91144.051142	35.842816
1308.659789	91261.287133	35.847834
1309.825559	91384.396852	35.852852
1311.155823	91495.682047	35.857869
1311.945914	91619.269438	35.862887
1313.571467	91742.892057	35.867904
1314.619305	91856.212363	35.872922
1315.799636	91980.830461	35.877940
1317.039731	92107.721121	35.882957
1318.327742	92246.810140	35.887975
1319.786022	92371.145770	35.892992
1321.191588	92501.092172	35.898010
1322.346647	92621.255467	35.903028
1323.464617	92751.057585	35.908045
1324.756469	92879.971326	35.913063
1325.870183	93017.025053	35.918080
1327.414168	93149.956548	35.923098
1328.544220	93287.934195	35.928116
1329.790383	93417.491049	35.933133
1331.054269	93558.098099	35.938151
1332.488330	93699.224324	35.943168
1333.832463	93835.599436	35.948186
1335.036679	93963.048418	35.953204
1336.616975	94087.207267	35.958221
1337.327108	94231.921567	35.963239
1339.116537	94372.970222	35.968256
1340.617006	94495.026397	35.973274
1342.460372	94612.618709	35.978292
1344.063162	94716.445559	35.983309
1344.956523	94839.941170	35.988327
1346.153432	94942.551749	35.993344
1348.056824	95054.686001	35.998362
1349.425357	95176.486544	36.003380
1350.866925	95286.526018	36.008397
1352.013432	95399.197618	36.013415
1353.453395	95515.499867	36.018432
1354.621556	95624.062023	36.023450
1355.067970	95765.224655	36.028468
1356.588015	95878.942634	36.033485
1357.622412	96009.303861	36.038503
1359.080827	96151.198025	36.043520
1360.507695	96277.443015	36.048538
1361.668243	96420.259399	36.053556
1363.436889	96539.632590	36.058573
1364.192609	96683.349799	36.063591
1365.638484	96825.464462	36.068608
1367.182088	96956.802490	36.073626
1368.495433	97101.448909	36.078644
1370.259843	97250.082195	36.083661
1371.209679	97390.882227	36.088679
1372.875990	97526.564193	36.093696
1374.428929	97664.317972	36.098714
1375.838257	97806.075127	36.103732
1377.481028	97946.731750	36.108749
1378.962153	98078.388407	36.113767
1380.490336	98216.680859	36.118784
1382.112623	98345.008040	36.123802
1383.510715	98483.524730	36.128820
1385.221613	98612.473037	36.133837
1386.511880	98743.693113	36.138855
1387.516766	98872.714332	36.143872
1389.744859	98997.083384	36.148890
1391.117179	99128.279593	36.153908
1392.487056	99253.188887	36.158925
1393.661737	99382.350534	36.163943
1395.088918	99510.649384	36.168960
1396.150104	99648.564348	36.173978
1397.245909	99790.873534	36.178996
1398.695719	99920.032552	36.184013
1400.152052	100066.305559	36.189031
1401.881823	100190.097576	36.194048
1403.983083	100320.487935	36.199066
1405.619753	100445.423722	36.204084
1407.275735	100561.901029	36.209101
1408.444982	100686.618916	36.214119
1410.110230	100808.724543	36.219136
1411.616869	100920.865261	36.224154
1412.722984	101059.958286	36.229172
1413.941731	101171.422045	36.234189
1415.443723	101301.529294	36.239207
1416.693176	101418.782914	36.244224
1418.392919	101536.626124	36.249242
1419.443392	101679.876155	36.254260
1420.967087	101792.067933	36.259277
1422.457882	101920.569278	36.264295
1423.792867	102050.274450	36.269312
1425.250099	102174.902497	36.274330
1426.095889	102314.675296	36.279348
1427.348146	102444.978105	36.284365
1428.667242	102580.697373	36.289383
1429.786402	102716.727245	36.294400
1431.082630	102860.324530	36.299418
1432.260723	103007.693675	36.304436
1433.671691	103152.212582	36.309453
1435.053233	103288.001111	36.314471
1436.300041	103425.446721	36.319488
1438.114821	103557.720317	36.324506
1439.120351	103701.087565	36.329524
1440.781021	103831.167447	36.334541
1441.898044	103974.201548	36.339559
1443.365549	104105.263486	36.344576
1444.799881	104246.715214	36.349594
1445.619706	104395.972062	36.354612
1447.273094	104546.329709	36.359629
1448.756086	104702.052491	36.364647
1449.683813	104855.161744	36.369664
1451.479248	105002.697218	36.374682
1452.552241	105158.562010	36.379700
1454.245882	105306.482365	36.384717
1456.256985	105472.789912	36.389735
1457.403178	105623.992097	36.394752
1458.995935	105774.377358	36.399770
1460.288311	105948.914056	36.404788
1461.708137	106105.857730	36.409805
1463.667955	106265.938744	36.414823
1465.139818	106423.509777	36.419840
1467.494411	106560.263252	36.424858
1468.860925	106711.968554	36.429876
1470.274964	106853.053980	36.434893
1472.177161	106998.489345	36.439911
1473.831945	107145.662973	36.444928
1475.840737	107276.526180	36.449946
1477.237078	107419.518723	36.454964
1478.841440	107554.782571	36.459981
1480.840546	107689.617785	36.464999
1482.289656	107820.608224	36.470016
1484.240317	107936.976685	36.475034
1485.690068	108065.013424	36.480052
1487.486840	108187.734226	36.485069
1489.379146	108310.656165	36.490087
1490.214993	108436.887758	36.495104
1491.634459	108552.795712	36.500122
1493.176686	108685.512190	36.505140
1494.586132	108816.335055	36.510157
1496.058089	108942.329995	36.515175
1497.170733	109076.699927	36.520192
1498.842661	109204.237113	36.525210
1500.034080	109356.399792	36.530228
1501.190028	109489.927640	36.535245
1502.455159	109623.489729	36.540263
1503.767350	109765.896383	36.545280
1505.488782	109901.366758	36.550298
1506.580343	110058.633163	36.555316
1507.972240	110200.204902	36.560333
1509.879281	110345.755039	36.565351
1511.340579	110512.692465	36.570368
1512.762711	110650.723222	36.575386
1514.565154	110806.550783	36.580404
1515.900796	110956.504068	36.585421
1517.064954	111105.685743	36.590439
1518.987924	111238.086329	36.595456
1521.020795	111385.498049	36.600474
1522.440033	111538.940924	36.605492
1523.752401	111689.458930	36.610509
1525.562184	111828.232894	36.615527
1526.820304	111974.423373	36.620544
1528.456031	112105.958810	36.625562
1530.262803	112260.752171	36.630580
1531.296383	112400.295953	36.635597
1532.992728	112552.837686	36.640615
1534.284016	112697.415339	36.645632
1536.037764	112841.617222	36.650650
1537.308439	112980.073739	36.655668
1538.488639	113126.737609	36.660685
1540.371826	113259.862095	36.665703
1541.371666	113394.189879	36.670720
1542.917285	113534.723686	36.675738
1544.007216	113678.030327	36.680756
1545.765442	113826.813821	36.685773
1547.185521	113967.749325	36.690791
1548.370942	114125.640495	36.695808
1549.552169	114282.454977	36.700826
1551.381353	114426.435838	36.705844
1552.876397	114584.268124	36.710861
1554.856938	114740.123105	36.715879
1556.497615	114906.621852	36.720896
1557.625148	115054.595359	36.725914
1559.309864	115220.530630	36.730932
1560.949781	115386.904847	36.735949
1562.534020	115547.466940	36.740967
1563.783150	115708.690681	36.745984
1565.076097	115883.124217	36.751002
1566.962027	116050.934395	36.756020
1568.377694	116225.578745	36.761037
1570.116320	116388.593715	36.766055
1571.674930	116566.959025	36.771072
1573.207779	116746.458033	36.776090
1574.961241	116924.705946	36.781108
1576.287570	117105.354980	36.786125
1577.779443	117278.546477	36.791143
1579.523574	117456.151510	36.796160
1581.144664	117639.420833	36.801178
1582.938980	117818.414991	36.806196
1583.767313	118004.917032	36.811213
1585.561777	118194.009368	36.816231
1587.586349	118390.474331	36.821248
1589.325410	118570.216334	36.826266
1591.116803	118737.114651	36.831284
1592.985920	118922.266912	36.836301
1594.338176	119103.035646	36.841319
1596.052525	119277.596966	36.846336
1597.343149	119453.683742	36.851354
1599.370011	119639.791641	36.856372
1601.088769	119821.140958	36.861389
1602.709521	119989.086080	36.866407
1603.961728	120187.367578	36.871424
1605.497183	120361.327450	36.876442
1607.649515	120549.652744	36.881460
1608.976148	120730.598045	36.886477
1611.159992	120909.850531	36.891495
1612.649070	121097.812387	36.896512
1614.053406	121275.132924	36.901530
1615.597093	121450.035101	36.906548
1617.045951	121631.878908	36.911565
1618.446013	121815.659307	36.916583
1620.443331	122000.540026	36.921600
1622.197211	122182.719481	36.926618
1623.812985	122359.263601	36.931636
1625.651559	122554.434108	36.936653
1627.434669	122725.232698	36.941671
1629.209065	122898.836890	36.946688
1630.814451	123074.294878	36.951706
1632.815238	123242.588136	36.956724
1634.695869	123421.924693	36.961741
1636.216677	123585.600400	36.966759
1637.852478	123769.315164	36.971776
1639.453100	123927.296606	36.976794
1640.772055	124087.847012	36.981812
1642.225316	124285.420225	36.986829
1643.887025	124456.219787	36.991847
1645.178508	124625.656856	36.996864
1646.260516	124792.057195	37.001882
1648.164329	124953.750598	37.006900
1649.741212	125132.228700	37.011917
1651.032197	125294.551674	37.016935
1652.516076	125465.966768	37.021952
1654.178623	125637.862237	37.026970
1656.765850	125788.631107	37.031988
1658.160664	125961.521102	37.037005
1659.542653	126127.322037	37.042023
1660.931672	126307.965896	37.047040
1662.384819	126485.390844	37.052058
1664.123713	126669.013960	37.057076
1665.493165	126861.703020	37.062093
1666.732342	127048.970601	37.067111
1668.300071	127248.227775	37.072128
1669.809539	127446.340465	37.077146
1671.223842	127650.292265	37.082164
1672.682116	127865.910356	37.087181
1674.619303	128065.291583	37.092199
1676.021592	128280.844418	37.097216
1677.382002	128505.159119	37.102234
1678.979141	128714.758902	37.107252
1681.001640	128944.555350	37.112269
1682.605428	129159.891042	37.117287
1684.324184	129386.755622	37.122304
1685.976559	129598.533479	37.127322
1688.030898	129812.660496	37.132340
1689.979714	130046.877050	37.137357
1692.243523	130255.200772	37.142375
1693.910828	130476.065170	37.147392
1695.953446	130681.037736	37.152410
1698.025434	130888.112925	37.157428
1699.661212	131097.972255	37.162445
1701.239276	131293.072608	37.167463
1703.475568	131503.665184	37.172480
1705.343765	131708.428731	37.177498
1706.848408	131911.194326	37.182516
1708.631451	132115.148313	37.187533
1710.405634	132315.298109	37.192551
1712.522725	132530.367873	37.197568
1714.086930	132730.983670	37.202586
1715.741709	132929.860641	37.207604
1717.150721	133139.930104	37.212621
1718.719192	133349.341318	37.217639
1720.497503	133571.181262	37.222656
1721.623836	133783.074223	37.227674
1723.363812	134000.570015	37.232692
1725.002627	134224.211397	37.237709
1726.489994	134442.877994	37.242727
1727.696016	134676.156546	37.247744
1729.702240	134915.846699	37.252762
1731.699535	135135.490526	37.257780
1732.899972	135366.641755	37.262797
1734.805142	135596.377483	37.267815
1736.877949	135833.295889	37.272832
1738.331841	136067.355212	37.277850
1740.000094	136294.491946	37.282868
1741.920257	136534.064514	37.287885
1743.470738	136765.219163	37.292903
1745.253488	137006.693674	37.297920
1747.314794	137250.892488	37.302938
1748.771667	137473.118950	37.307956
1750.627524	137718.570453	37.312973
1751.821104	137955.497120	37.317991
1753.871922	138187.177476	37.323008
1755.158173	138439.789833	37.328026
1757.137915	138669.212116	37.333044
1759.033468	138911.783070	37.338061
1760.709370	139133.919941	37.343079
1762.770078	139360.680732	37.348096
1764.068061	139586.508017	37.353114
1766.196239	139799.174005	37.358132
1767.440443	140040.303910	37.363149
1768.653620	140266.299926	37.368167
1770.607958	140517.486938	37.373184
1771.971219	140748.309734	37.378202
1773.869668	140988.416186	37.383220
1775.712244	141243.253985	37.388237
1777.307603	141485.301038	37.393255
1779.322941	141723.806599	37.398272
1781.012979	141981.451373	37.403290
1782.835781	142234.139989	37.408308
1784.722613	142482.606463	37.413325
1786.955822	142727.682482	37.418343
1789.030320	142962.390210	37.423360
1790.694187	143212.595733	37.428378
1792.635887	143460.195605	37.433396
1794.509072	143721.057358	37.438413
1796.027696	143961.174113	37.443431
1798.007587	144206.703039	37.448448
1799.611450	144461.036306	37.453466
1801.512533	144714.994620	37.458484
1803.443708	144978.265366	37.463501
1804.850442	145232.645916	37.468519
1806.685876	145498.942270	37.473536
1808.232105	145770.336477	37.478554
1810.482067	146016.987179	37.483572
1812.944286	146272.757110	37.488589
1814.644079	146530.931587	37.493607
1816.444496	146784.192468	37.498624
1818.041477	147057.362527	37.503642
1820.173811	147319.040197	37.508660
1821.777018	147577.234943	37.513677
1823.628182	147841.319813	37.518695
1825.389988	148113.302056	37.523712
1827.038450	148382.041326	37.528730
1828.608274	148650.172263	37.533748
1830.407793	148930.961652	37.538765
1831.884727	149207.601384	37.543783
1833.428003	149483.178714	37.548800
1834.961194	149775.069591	37.553818
1836.724684	150067.205465	37.558836
1838.842282	150352.319261	37.563853
1840.417134	150646.848570	37.568871
1842.743498	150928.315338	37.573888
1844.597384	151233.987215	37.578906
1846.832180	151524.369377	37.583924
1848.841796	151823.305476	37.588941
1850.519059	152110.388342	37.593959
1852.473965	152406.200802	37.598976
1854.355999	152695.907808	37.603994
1856.381652	152976.314815	37.609012
1858.437611	153265.629592	37.614029
1860.328120	153547.571060	37.619047
1862.804287	153813.453773	37.624064
1864.909751	154092.368732	37.629082
1866.908543	154367.176083	37.634100
1868.961261	154633.001600	37.639117
1870.129890	154912.789948	37.644135
1872.051262	155172.951404	37.649152
1873.725198	155456.764003	37.654170
1875.632883	155737.901180	37.659188
1877.478152	156017.894237	37.664205
1879.243814	156295.730264	37.669223
1881.412787	156569.277546	37.674240
1883.501302	156837.633822	37.679258
1885.011929	157093.945134	37.684276
1886.884730	157355.317169	37.689293
1888.284996	157618.338052	37.694311
1889.945011	157877.206534	37.699328
1891.654875	158148.623645	37.704346
1893.272671	158417.758519	37.709364
1894.926630	158699.190446	37.714381
1896.732535	158981.907625	37.719399
1898.456877	159266.365351	37.724416
1899.706545	159557.118925	37.729434
1901.749590	159855.113654	37.734452
1903.687185	160148.670172	37.739469
1905.367111	160447.854154	37.744487
1907.196967	160737.266133	37.749504
1909.108858	161054.292114	37.754522
1910.823474	161365.345388	37.759540
1913.017137	161677.023898	37.764557
1914.707590	161992.451312	37.769575
1916.665710	162307.394276	37.774592
1918.271026	162631.293469	37.779610
1920.105872	162958.903855	37.784628
1922.102172	163291.708808	37.789645
1923.931996	163624.262058	37.794663
1926.205717	163952.697860	37.799680
1928.602936	164277.662728	37.804698
1930.524983	164596.418522	37.809716
1933.286606	164919.653923	37.814733
1935.552186	165234.817045	37.819751
1937.804898	165545.120930	37.824768
1940.116968	165837.781642	37.829786
1942.251506	166137.174997	37.834804
1944.622533	166441.116316	37.839821
1946.725058	166740.745833	37.844839
1948.447792	167047.939491	37.849856
1950.352098	167355.106252	37.854874
1952.125179	167646.296851	37.859892
1954.253491	167950.219082	37.864909
1956.158371	168258.519735	37.869927
1958.149512	168570.490419	37.874944
1959.572015	168882.550970	37.879962
1962.388846	169173.953626	37.884980
1964.917679	169456.831745	37.889997
1967.155965	169753.100895	37.895015
1969.235511	170040.482524	37.900032
1971.180656	170338.513800	37.905050
1972.650390	170636.632974	37.910068
1974.394891	170937.491309	37.915085
1975.805473	171237.818752	37.920103
1977.345931	171548.716870	37.925120
1979.206137	171868.264307	37.930138
1980.884962	172190.495118	37.935156
1982.712387	172527.319130	37.940173
1983.960671	172853.136990	37.945191
1985.982283	173189.844807	37.950208
1988.028640	173525.039201	37.955226
1990.043107	173857.560756	37.960244
1992.250070	174189.025233	37.965261
1993.788262	174528.061580	37.970279
1995.316847	174878.567165	37.975296
1997.324207	175239.716936	37.980314
1998.649754	175584.822435	37.985332
2000.836366	175944.677647	37.990349
2002.821584	176317.416395	37.995367
2005.152391	176660.617631	38.000384
2007.671940	177019.816213	38.005402
2009.201862	177379.119566	38.010420
2011.442838	177722.923277	38.015437
2013.707990	178077.162783	38.020455
2015.320531	178418.171854	38.025472
2017.100744	178761.594312	38.030490
2019.175351	179111.397831	38.035508
2020.624788	179446.163202	38.040525
2022.384994	179789.110269	38.045543
2024.359301	180141.397056	38.050560
2026.704305	180500.383328	38.055578
2028.888972	180847.966980	38.060596
2031.382389	181188.392507	38.065613
2033.927520	181531.274860	38.070631
2036.295126	181864.738037	38.075648
2038.565051	182204.440167	38.080666
2040.660413	182541.300697	38.085684
2043.412657	182875.367976	38.090701
2044.716588	183222.081673	38.095719
2046.495003	183566.665500	38.100736
2048.596059	183908.304902	38.105754
2050.328381	184267.401009	38.110772
2051.909509	184620.502445	38.115789
2053.686868	184990.668059	38.120807
2055.719515	185353.531204	38.125824
2057.352205	185727.150916	38.130842
2059.005257	186124.009082	38.135860
2061.219840	186496.779074	38.140877
2062.860237	186902.608150	38.145895
2064.862580	187267.108336	38.150912
2067.072023	187742.319637	38.155930
2068.761278	188142.989752	38.160948
2071.062277	188538.867188	38.165965
2072.886901	188949.247315	38.170983
2074.883124	189349.543880	38.176000
2077.171421	189759.753240	38.181018
2079.587624	190185.946267	38.186036
2082.035493	190579.547465	38.191053
2084.119505	191001.045373	38.196071
2086.274929	191409.808083	38.201088
2088.920255	191806.151323	38.206106
2091.269378	192198.325479	38.211124
2093.947408	192589.459091	38.216141
2096.468452	192984.860306	38.221159
2098.617787	193366.350185	38.226176
2101.015426	193750.317268	38.231194
2103.458237	194132.576617	38.236212
2105.974372	194506.519553	38.241229
2108.191744	194874.439195	38.246247
2110.028018	195249.328298	38.251264
2112.389238	195628.226360	38.256282
2114.211462	196011.425989	38.261300
2116.132000	196386.863968	38.266317
2118.210304	196776.935057	38.271335
2119.887701	197146.138761	38.276352
2121.799077	197537.863630	38.281370
2123.631010	197935.114090	38.286388
2125.659791	198321.564658	38.291405
2128.253986	198712.856190	38.296423
2130.199429	199115.705950	38.301440
2132.279190	199501.033936	38.306458
2134.243540	199904.187644	38.311476
2136.404420	200293.747100	38.316493
2138.577192	200701.061741	38.321511
2140.551052	201094.843594	38.326528
2142.207655	201484.890829	38.331546
2144.554826	201900.081393	38.336564
2146.460455	202302.538894	38.341581
2148.558285	202713.045390	38.346599
2150.955978	203123.734798	38.351616
2153.808002	203512.228824	38.356634
2155.429989	203912.549496	38.361652
2158.058311	204286.143244	38.366669
2160.135425	204660.560193	38.371687
2162.361404	205035.945411	38.376704
2164.111855	205402.514377	38.381722
2166.414336	205800.904075	38.386740
2168.408425	206170.408655	38.391757
2170.503168	206554.758947	38.396775
2172.679011	206945.956123	38.401792
2174.804126	207332.335328	38.406810
2176.561281	207718.162803	38.411828
2179.541369	208101.590546	38.416845
2181.633901	208484.572787	38.421863
2183.479335	208875.951761	38.426880
2185.531183	209276.419012	38.431898
2187.351682	209682.740272	38.436916
2189.692592	210090.022733	38.441933
2191.965598	210499.170849	38.446951
2193.288649	210913.649729	38.451968
2195.799600	211326.826618	38.456986
2197.629813	211752.837199	38.462004
2199.497389	212176.353049	38.467021
2201.938502	212610.500541	38.472039
2203.830049	213049.713277	38.477056
2206.412465	213483.230305	38.482074
2208.468584	213937.076522	38.487092
2210.287131	214366.801409	38.492109
2212.499597	214811.529915	38.497127
2214.724190	215270.533978	38.502144
2217.099455	215716.610020	38.507162
2219.440332	216170.567090	38.512180
2221.777371	216618.860192	38.517197
2224.353248	217064.245946	38.522215
2226.792779	217523.854117	38.527232
2228.974183	217977.939437	38.532250
2231.144945	218433.042970	38.537268
2233.537672	218901.271582	38.542285
2235.430201	219350.449227	38.547303
2237.824855	219816.671335	38.552320
2240.045303	220276.823918	38.557338
2242.384691	220736.094544	38.562356
2244.831568	221197.939920	38.567373
2247.231975	221652.044540	38.572391
2249.374418	222123.159429	38.577408
2251.773960	222580.414699	38.582426
2253.928528	223050.740553	38.587444
2255.937031	223517.481913	38.592461
2257.895029	223990.582281	38.597479
2260.071559	224473.784976	38.602496
2262.478139	224948.822640	38.607514
2264.167317	225433.015861	38.612532
2266.304018	225906.088679	38.617549
2268.856032	226400.487113	38.622567
2271.154546	226888.650156	38.627584
2273.953772	227370.079344	38.632602
2276.227602	227863.199882	38.637620
2278.478415	228322.841307	38.642637
2281.340815	228808.756854	38.647655
2283.117269	229296.086033	38.652672
2285.651460	229769.528094	38.657690
2287.889563	230253.533293	38.662708
2290.259632	230728.397660	38.667725
2292.637220	231213.803254	38.672743
2294.695639	231688.004242	38.677760
2297.194886	232163.762161	38.682778
2299.637333	232646.794103	38.687796
2301.525730	233136.821755	38.692813
2304.055110	233611.329052	38.697831
2306.086695	234103.569095	38.702848
2308.311154	234568.672713	38.707866
2310.479878	235032.412738	38.712884
2312.609170	235488.562678	38.717901
2314.848163	235951.147618	38.722919
2316.934506	236424.526978	38.727936
2319.846024	236876.590638	38.732954
2322.645439	237336.241493	38.737972
2324.914686	237796.101282	38.742989
2327.882144	238255.496145	38.748007
2329.977070	238719.370169	38.753024
2332.988240	239162.879701	38.758042
2335.205754	239604.479825	38.763060
2337.193533	240058.308715	38.768077
2339.764635	240516.136063	38.773095
2341.653269	240988.396382	38.778112
2343.832034	241446.283238	38.783130
2346.053065	241910.970801	38.788148
2348.589280	242386.049204	38.793165
2350.871444	242855.780753	38.798183
2353.114965	243324.120225	38.803200
2355.704599	243796.393184	38.808218
2357.708571	244277.571166	38.813236
2359.922730	244755.489215	38.818253
2362.631514	245241.458172	38.823271
2364.630641	245734.649254	38.828288
2366.957274	246227.051505	38.833306
2369.093846	246720.625251	38.838324
2371.426803	247228.189472	38.843341
2373.669672	247734.267614	38.848359
2375.674327	248253.006521	38.853376
2377.765743	248762.255332	38.858394
2380.135391	249278.013209	38.863412
2382.467485	249802.742426	38.868429
2385.147904	250324.926403	38.873447
2387.097036	250852.861834	38.878464
2389.984351	251373.333759	38.883482
2392.641073	251908.090397	38.888500
2394.806908	252422.523875	38.893517
2397.250728	252960.459862	38.898535
2399.752841	253498.715081	38.903552
2402.273338	254031.427923	38.908570
2404.358030	254573.376587	38.913588
2406.416502	255127.570764	38.918605
2409.214171	255661.783857	38.923623
2411.618121	256205.429199	38.928640
2413.826537	256740.771203	38.933658
2417.046305	257296.553890	38.938676
2419.524807	257828.064671	38.943693
2422.205401	258355.350655	38.948711
2425.168130	258881.930103	38.953728
2428.026532	259395.239028	38.958746
2431.425397	259920.095111	38.963764
2434.251593	260425.733721	38.968781
2436.831782	260926.607799	38.973799
2439.137093	261433.262940	38.978816
2441.930528	261927.622454	38.983834
2444.452744	262432.994796	38.988852
2446.586933	262939.288831	38.993869
2449.103732	263435.716708	38.998887
2451.288569	263935.622924	39.003904
2453.867875	264443.517058	39.008922
2456.163899	264934.562268	39.013940
2458.110935	265440.594234	39.018957
2460.634181	265937.009381	39.023975
2463.050068	266456.018516	39.028992
2465.176173	266965.951883	39.034010
2467.580773	267469.565809	39.039028
2469.514981	267984.197148	39.044045
2471.778656	268480.614587	39.049063
2473.898589	268985.788849	39.054080
2475.939718	269491.048875	39.059098
2478.541493	269991.088518	39.064116
2480.632354	270506.951675	39.069133
2482.499430	271008.954171	39.074151
2485.284556	271526.049588	39.079168
2487.565857	272036.972642	39.084186
2490.186567	272565.287889	39.089204
2492.325037	273109.167264	39.094221
2494.818067	273627.159281	39.099239
2496.995853	274175.648048	39.104256
2499.163107	274721.011103	39.109274
2502.054290	275271.565812	39.114292
2504.211758	275820.173932	39.119309
2506.896851	276376.950017	39.124327
2509.597118	276925.974126	39.129344
2512.983069	277477.986047	39.134362
2515.702958	278019.990301	39.139380
2518.483010	278575.110898	39.144397
2521.057009	279120.685559	39.149415
2523.561034	279673.784178	39.154432
2526.542009	280230.867728	39.159450
2529.420965	280763.457104	39.164468
2531.594600	281330.638224	39.169485
2534.179528	281878.984545	39.174503
2536.260057	282439.365884	39.179520
2538.550613	282990.263634	39.184538
2541.088710	283553.663133	39.189556
2543.218780	284132.053055	39.194573
2546.000695	284707.695854	39.199591
2548.597320	285285.038657	39.204608
2551.122400	285863.505031	39.209626
2554.778292	286419.394143	39.214644
2557.997483	286972.274136	39.219661
2560.813197	287534.480524	39.224679
2563.094306	288083.256751	39.229696
2565.827232	288650.087860	39.234714
2568.685585	289211.282956	39.239732
2571.593750	289766.498429	39.244749
2573.605321	290321.036086	39.249767
2576.320101	290882.035713	39.254784
2578.879415	291439.601379	39.259802
2581.436227	291993.582376	39.264820
2583.650287	292568.711061	39.269837
2586.048969	293133.294133	39.274855
2588.636115	293709.978947	39.279872
2590.450321	294286.270725	39.284890
2592.965332	294867.017952	39.289908
2595.329550	295467.865680	39.294925
2598.014083	296056.242287	39.299943
2600.844214	296642.863859	39.304960
2603.076146	297233.863171	39.309978
2605.712284	297828.297016	39.314996
2608.352847	298429.553241	39.320013
2611.428918	299019.336290	39.325031
2614.174022	299613.556591	39.330048
2616.041383	300220.981367	39.335066
2619.328725	300815.637442	39.340084
2621.957417	301410.719540	39.345101
2624.432319	301998.939384	39.350119
2627.483923	302594.018734	39.355136
2629.892524	303192.821614	39.360154
2632.664516	303784.960987	39.365172
2635.114128	304383.337755	39.370189
2637.423257	304990.664888	39.375207
2640.386583	305592.907728	39.380224
2643.083665	306185.285131	39.385242
2645.762246	306744.558078	39.390260
2648.302453	307317.223450	39.395277
2650.649217	307886.028748	39.400295
2653.320004	308456.782363	39.405312
2655.690314	309029.759044	39.410330
2658.118011	309614.548251	39.415348
2660.406459	310202.321798	39.420365
2662.947516	310795.379042	39.425383
2665.499205	311382.843405	39.430400
2667.882562	311987.255886	39.435418
2670.391364	312592.174124	39.440436
2672.482098	313203.900822	39.445453
2675.108684	313819.520785	39.450471
2678.064417	314442.542985	39.455488
2680.374614	315077.483991	39.460506
2683.450642	315693.237361	39.465524
2686.119292	316335.997910	39.470541
2688.835987	316964.225428	39.475559
2691.451000	317607.813602	39.480576
2694.301258	318255.111725	39.485594
2696.411777	318900.662932	39.490612
2699.096010	319559.463552	39.495629
2701.747650	320221.989601	39.500647
2704.459265	320879.065684	39.505664
2706.891289	321556.247342	39.510682
2709.516258	322215.143414	39.515700
2712.278948	322902.072356	39.520717
2715.047996	323592.845984	39.525735
2718.696868	324262.994438	39.530752
2721.189664	324943.867360	39.535770
2723.668146	325614.429735	39.540788
2726.318021	326309.845088	39.545805
2729.160541	327004.964818	39.550823
2732.129462	327683.180593	39.555840
2735.051779	328384.480124	39.560858
2738.401413	329064.389155	39.565876
2742.018101	329749.572729	39.570893
2744.819433	330422.668189	39.575911
2748.166161	331094.880686	39.580928
2750.788184	331768.716436	39.585946
2753.141816	332434.920775	39.590964
2756.125021	333102.715207	39.595981
2758.908584	333777.987124	39.600999
2761.984761	334437.778017	39.606016
2764.993822	335113.117713	39.611034
2768.086105	335772.121540	39.616052
2770.498591	336451.157168	39.621069
2773.355017	337113.826470	39.626087
2776.342533	337777.148231	39.631104
2779.049196	338445.574540	39.636122
2781.696159	339105.145671	39.641140
2784.150607	339774.347522	39.646157
2786.747744	340452.214239	39.651175
2789.488132	341132.429831	39.656192
2791.995879	341814.063449	39.661210
2794.429649	342492.829462	39.666228
2797.293129	343182.065704	39.671245
2799.993036	343870.730410	39.676263
2802.567200	344562.063761	39.681280
2805.054085	345259.787416	39.686298
2808.022743	345958.436187	39.691316
2810.837388	346669.469570	39.696333
2813.565390	347372.615035	39.701351
2816.362065	348074.670027	39.706368
2818.639043	348791.041780	39.711386
2821.517180	349500.331429	39.716404
2824.446761	350216.114275	39.721421
2826.955863	350909.938360	39.726439
2829.993185	351603.842932	39.731456
2832.505797	352296.014111	39.736474
2835.832664	352964.413909	39.741492
2839.044669	353639.739071	39.746509
2841.399877	354333.842868	39.751527
2844.400894	355010.642153	39.756544
2846.715558	355696.634944	39.761562
2849.824722	356384.593217	39.766580
2852.642238	357075.623746	39.771597
2855.689899	357759.276906	39.776615
2859.208305	358441.903717	39.781632
2861.720010	359148.880129	39.786650
2864.774491	359838.290748	39.791668
2868.191787	360523.092005	39.796685
2870.777615	361220.021639	39.801703
2873.589443	361913.554190	39.806720
2876.889536	362610.999314	39.811738
2879.542215	363312.431995	39.816756
2881.463434	364011.503426	39.821773
2884.758441	364727.223641	39.826791
2887.419048	365450.349334	39.831808
2890.148691	366174.307979	39.836826
2893.194659	366896.476030	39.841844
2896.115964	367621.661021	39.846861
2898.742124	368348.089956	39.851879
2901.726440	369073.253656	39.856896
2905.009875	369812.871872	39.861914
2907.715662	370542.577041	39.866932
2911.028466	371289.626866	39.871949
2913.598744	372029.348334	39.876967
2916.605040	372770.933204	39.881984
2919.759050	373521.773593	39.887002
2922.489505	374272.026005	39.892020
2925.480394	375015.224895	39.897037
2928.684023	375782.564509	39.902055
2931.601252	376521.426825	39.907072
2934.171281	377280.487780	39.912090
2936.977959	378041.035673	39.917108
2940.299237	378797.403461	39.922125
2943.294604	379570.442591	39.927143
2946.220095	380332.324841	39.932160
2948.979241	381100.669800	39.937178
2952.186170	381870.948762	39.942196
2955.040280	382643.969866	39.947213
2958.244949	383418.990128	39.952231
2961.210157	384178.322165	39.957248
2963.813870	384960.303459	39.962266
2966.575723	385733.347256	39.967284
2970.145155	386508.369026	39.972301
2972.447471	387304.050465	39.977319
2975.584391	388073.722899	39.982336
2978.842378	388856.570564	39.987354
2981.617578	389641.595652	39.992372
2985.111402	390426.078905	39.997389
2987.610934	391220.971404	40.002407
2991.331980	392000.912889	40.007424
2993.642389	392800.087590	40.012442
2997.008162	393595.476824	40.017460
2999.988843	394384.216466	40.022477
3002.730628	395178.587310	40.027495
3005.850017	395967.911491	40.032512
3008.680318	396777.302514	40.037530
3011.597020	397564.175159	40.042548
3014.939557	398356.371949	40.047565
3018.018366	399164.781823	40.052583
3021.847969	399938.119509	40.057600
3025.080979	400719.673785	40.062618
3028.069055	401491.977067	40.067636
3031.434285	402232.460567	40.072653
3034.750852	402976.622490	40.077671
3037.730373	403699.505337	40.082688
3040.958970	404416.658199	40.087706
3043.535571	405157.169499	40.092724
3046.763768	405881.411712	40.097741
3049.317662	406614.540740	40.102759
3052.201972	407350.326914	40.107776
3054.708587	408082.656099	40.112794
3057.492523	408838.750411	40.117812
3060.584432	409589.458175	40.122829
3063.563940	410361.003448	40.127847
3066.909937	411117.842783	40.132864
3069.725152	411894.267220	40.137882
3072.690442	412669.375817	40.142900
3075.683204	413433.929894	40.147917
3078.583837	414218.706059	40.152935
3081.812267	414990.655044	40.157952
3084.939580	415782.572356	40.162970
3087.958568	416568.913102	40.167988
3091.135618	417363.191676	40.173005
3093.960535	418164.424317	40.178023
3096.961618	418972.123289	40.183040
3100.458173	419776.527844	40.188058
3103.081681	420596.107629	40.193076
3106.734736	421398.705650	40.198093
3109.892019	422209.743920	40.203111
3112.919938	423019.910741	40.208128
3116.240594	423844.056744	40.213146
3119.025428	424670.679812	40.218164
3122.276102	425490.826239	40.223181
3125.146401	426325.660349	40.228199
3128.257568	427152.282942	40.233216
3131.032719	428001.268415	40.238234
3133.815485	428852.491441	40.243252
3137.076085	429701.986118	40.248269
3140.237855	430557.272646	40.253287
3143.151847	431414.784613	40.258304
3146.640580	432285.310764	40.263322
3149.683036	433149.347911	40.268340
3152.886564	434004.982877	40.273357
3155.651606	434889.756930	40.278375
3158.765804	435766.148624	40.283392
3162.310529	436645.212580	40.288410
3165.041095	437532.346404	40.293428
3168.514027	438425.790802	40.298445
3171.844685	439308.504173	40.303463
3174.970991	440199.493664	40.308480
3177.919455	441092.640967	40.313498
3181.072367	441987.987141	40.318516
3184.387234	442885.386749	40.323533
3187.706672	443776.377782	40.328551
3191.258148	444671.785140	40.333568
3195.067952	445559.027633	40.338586
3198.775310	446450.586547	40.343604
3202.782911	447301.451422	40.348621
3206.216188	448174.888821	40.353639
3209.703041	449042.115095	40.358656
3213.331247	449897.916318	40.363674
3216.277623	450760.043985	40.368692
3220.003008	451598.177541	40.373709
3223.116688	452454.441551	40.378727
3226.192770	453307.792483	40.383744
3229.908867	454138.840648	40.388762
3232.947615	454989.743445	40.393780
3236.180367	455827.349561	40.398797
3238.944014	456680.232259	40.403815
3241.965640	457517.891117	40.408832
3245.173140	458325.500944	40.413850
3247.548895	459147.838394	40.418868
3250.917252	459963.371113	40.423885
3253.655241	460781.991037	40.428903
3256.618135	461611.587851	40.433920
3259.499614	462445.042321	40.438938
3262.072447	463278.705778	40.443956
3265.330184	464131.747254	40.448973
3268.397677	464982.908508	40.453991
3271.177231	465857.176958	40.459008
3274.578731	466729.032922	40.464026
3277.295891	467603.976417	40.469044
3280.650991	468475.849032	40.474061
3283.805207	469380.138628	40.479079
3286.801879	470284.050126	40.484096
3290.149062	471190.378986	40.489114
3292.606603	472117.320939	40.494132
3295.832464	473039.602684	40.499149
3299.307089	473983.526001	40.504167
3302.334919	474925.648629	40.509184
3305.700868	475877.646306	40.514202
3308.516667	476839.756099	40.519220
3312.180489	477798.802581	40.524237
3315.326108	478772.742511	40.529255
3318.140045	479736.290715	40.534272
3322.033121	480723.301414	40.539290
3325.283650	481711.257377	40.544308
3328.806648	482696.135305	40.549325
3332.514152	483693.016687	40.554343
3335.546816	484680.566690	40.559360
3339.492899	485674.512218	40.564378
3343.029949	486683.169230	40.569396
3346.715165	487666.093612	40.574413
3350.434207	488662.400164	40.579431
3353.221728	489659.945138	40.584448
3357.484500	490643.998072	40.589466
3360.496698	491643.795266	40.594484
3364.535970	492634.250522	40.599501
3368.559514	493616.333432	40.604519
3371.849411	494601.235606	40.609536
3375.789242	495576.253295	40.614554
3379.328964	496564.511251	40.619572
3382.457074	497535.045114	40.624589
3386.148401	498516.100190	40.629607
3389.721480	499487.644116	40.634624
3392.946614	500461.090402	40.639642
3395.909306	501431.542787	40.644660
3399.365119	502412.724816	40.649677
3403.380351	503383.436239	40.654695
3406.941485	504370.004689	40.659712
3410.691949	505335.593153	40.664730
3413.888504	506293.906715	40.669748
3418.255805	507257.960878	40.674765
3421.772990	508219.063259	40.679783
3425.139438	509175.545927	40.684800
3428.890134	510130.998440	40.689818
3432.279840	511087.347507	40.694836
3435.872543	512036.306730	40.699853
3439.322571	512975.818884	40.704871
3442.387080	513935.644302	40.709888
3446.034323	514862.073745	40.714906
3449.267922	515818.071324	40.719924
3452.204807	516770.730246	40.724941
3455.739670	517726.548082	40.729959
3459.169197	518666.077678	40.734976
3463.052489	519614.469842	40.739994
3467.075825	520557.043739	40.745012
3469.950169	521472.379084	40.750016
3473.302194	522372.798005	40.755021
3476.560150	523222.435335	40.760026
3479.888257	524009.536386	40.765031
3482.817194	524755.797061	40.770036
3485.713695	525445.752327	40.775040
3488.612484	526066.661196	40.780045
3490.915436	526653.482668	40.785050
3493.405388	527185.700267	40.790055
3495.650541	527660.516842	40.795060
3497.713773	528095.254285	40.800064
3499.681250	528470.261427	40.805069
3500.967945	528816.053118	40.810074
3503.149188	529111.738555	40.815079
3504.444943	529379.252877	40.820084
3505.660733	529590.321760	40.825088
3506.867057	529771.475859	40.830093
3508.354951	529932.239107	40.835098
3509.827223	530047.479856	40.840103
3510.703656	530139.799188	40.845108
3511.745605	530207.366986	40.850112
3512.702853	530223.583926	40.855117
3513.287433	530242.578093	40.860122
3514.087852	530217.325557	40.865127
3514.469441	530188.562815	40.870132
3515.026297	530132.126771	40.875136
3515.737709	530056.278888	40.880141
3516.092752	529975.903482	40.885146
3516.869158	529887.001881	40.890151
3517.073389	529769.685893	40.895156
3517.248505	529643.409509	40.900160
3517.575569	529501.194695	40.905165
3517.413631	529361.421353	40.910170
3518.465381	529207.004185	40.915175
3518.423568	529032.913070	40.920180
3517.932569	528854.054804	40.925184
3518.613982	528668.061622	40.930189
3518.484731	528489.091737	40.935194
3518.447500	528294.492252	40.940199
3518.528417	528097.453997	40.945204
3518.444930	527899.380704	40.950208
3518.683720	527696.368752	40.955213
3518.628214	527490.327081	40.960218
3518.731637	527276.198598	40.965223
3518.493878	527054.211842	40.970228
3518.376426	526849.026084	40.975232
3519.044280	526617.723820	40.980237
3519.019201	526409.293168	40.985242
3518.327375	526173.107233	40.990247
3518.690599	525944.611103	40.995252
3518.585068	525723.437822	41.000256
3518.727218	525493.809745	41.005261
3518.393838	525263.244192	41.010266
3518.464915	525024.803353	41.015271
3518.055600	524800.387530	41.020276
3518.119632	524565.566739	41.025280
3518.336505	524335.705564	41.030285
3517.926905	524104.879941	41.035290
3517.756560	523870.234538	41.040295
3517.073611	523630.273940	41.045300
3517.116898	523409.895627	41.050304
3517.039461	523182.277265	41.055309
3516.709013	522963.310119	41.060314
3516.535252	522738.117653	41.065319
3516.721293	522530.651645	41.070324
3516.471574	522306.421094	41.075328
3516.126036	522094.949760	41.080333
3516.345833	521881.925869	41.085338
3516.087949	521653.956985	41.090343
3515.879370	521447.795427	41.095348
3515.678253	521240.672134	41.100352
3515.327501	521024.800830	41.105357
3515.231597	520807.072295	41.110362
3515.564867	520601.821353	41.115367
3515.086502	520393.367606	41.120372
3514.857047	520193.187026	41.125376
3514.962160	519988.768612	41.130381
3514.449378	519790.692387	41.135386
3514.182382	519587.938513	41.140391
3514.710139	519397.707729	41.145396
3513.869589	519199.875479	41.150400
3513.774067	519002.327604	41.155405
3513.489200	518825.722207	41.160410
3513.754899	518628.213494	41.165415
3513.838553	518450.134670	41.170420
3513.585745	518253.910847	41.175424
3513.169819	518067.185253	41.180429
3512.515801	517883.719957	41.185434
3512.876184	517702.765745	41.190439
3512.995810	517531.272240	41.195444
3512.676437	517352.132921	41.200448
3512.659602	517177.833537	41.205453
3512.465209	517000.031118	41.210458
3512.409144	516823.918706	41.215463
3512.369361	516654.505723	41.220468
3511.915326	516489.036550	41.225472
3512.164510	516316.701159	41.230477
3512.229688	516159.867964	41.235482
3511.875952	515990.999748	41.240487
3511.553380	515833.971125	41.245492
3511.629060	515660.495068	41.250496
3511.657456	515494.333916	41.255501
3511.120076	515335.014082	41.260506
3511.431088	515184.735564	41.265511
3511.231958	515023.393384	41.270516
3511.005464	514867.044585	41.275520
3510.862660	514707.353616	41.280525
3510.743048	514560.613941	41.285530
3510.835335	514406.277352	41.290535
3510.310278	514251.984691	41.295540
3510.072645	514109.191077	41.300544
3510.276318	513965.923977	41.305549
3510.089806	513828.211679	41.310554
3510.085602	513680.133846	41.315559
3509.821865	513545.052516	41.320564
3510.150152	513405.592086	41.325568
3509.778857	513262.255935	41.330573
3509.760531	513130.208004	41.335578
3509.850910	512999.755376	41.340583
3509.768465	512858.084423	41.345588
3509.631679	512723.882943	41.350592
3509.536544	512577.925242	41.355597
3509.824701	512462.008905	41.360602
3509.470788	512310.088334	41.365607
3509.262690	512191.120709	41.370612
3509.029135	512055.011737	41.375616
3509.077906	511920.521525	41.380621
3508.943444	511801.740822	41.385626
3508.709319	511667.645174	41.390631
3508.780392	511544.392826	41.395636
3507.979677	511431.007406	41.400640
3508.215188	511313.929918	41.405645
3508.387765	511204.929647	41.410650
3508.446100	511086.213720	41.415655
3508.439359	510968.515480	41.420660
3507.925549	510851.954162	41.425664
3508.010891	510736.811514	41.430669
3508.116374	510635.482488	41.435674
3508.186611	510504.303678	41.440679
3508.037515	510395.599322	41.445684
3507.890578	510284.321818	41.450688
3507.956435	510174.119805	41.455693
3507.604859	510063.780160	41.460698
3507.814026	509959.252931	41.465703
3507.818854	509848.957003	41.470708
3507.935989	509744.392067	41.475712
3507.428148	509631.602143	41.480717
3507.607260	509538.323053	41.485722
3507.509621	509426.173719	41.490727
3507.586815	509317.728422	41.495732
3507.073788	509218.805415	41.500736
3506.899809	509113.625450	41.505741
3507.147206	509016.398351	41.510746
3507.080727	508916.092413	41.515751
3507.140058	508818.943656	41.520756
3506.859086	508716.601800	41.525760
3506.838353	508623.398197	41.530765
3506.440219	508532.018006	41.535770
3506.393360	508438.716376	41.540775
3506.956548	508352.077857	41.545780
3506.741758	508260.465629	41.550784
3506.358053	508172.510655	41.555789
3506.522022	508081.594905	41.560794
3506.427450	507996.468849	41.565799
3506.670167	507900.747981	41.570804
3506.508090	507805.795612	41.575808
3506.344825	507707.110232	41.580813
3506.485833	507622.853194	41.585818
3506.581823	507535.273580	41.590823
3506.503862	507453.571642	41.595828
3505.935984	507361.403255	41.600832
3506.371908	507269.279831	41.605837
3505.546661	507187.541324	41.610842
3505.725460	507110.589433	41.615847
3506.016213	507022.623256	41.620852
3505.426507	506954.920191	41.625856
3505.599612	506875.395337	41.630861
3505.657653	506806.127919	41.635866
3505.392401	506724.703151	41.640871
3505.482697	506637.169334	41.645876
3505.795573	506566.902665	41.650880
3505.161501	506484.979033	41.655885
3505.373194	506412.911354	41.660890
3505.501194	506343.328132	41.665895
3505.363257	506276.005538	41.670900
3504.993299	506194.594032	41.675904
3504.892576	506124.389543	41.680909
3504.978664	506057.485067	41.685914
3504.866429	505997.219576	41.690919
3505.385006	505927.371762	41.695924
3505.054938	505858.664599	41.700928
3505.428390	505783.289542	41.705933
3505.170995	505716.689153	41.710938
3505.356255	505650.372703	41.715943
3505.108667	505578.120043	41.720948
3505.184796	505504.959031	41.725952
3505.051054	505432.738368	41.730957
3504.972908	505358.389860	41.735962
3505.061884	505298.796388	41.740967
3505.123597	505235.271908	41.745972
3505.051331	505170.103179	41.750976
3505.096206	505091.395526	41.755981
3505.280996	505032.996821	41.760986
3505.189712	504958.749180	41.765991
3505.177039	504887.818622	41.770996
3504.716858	504821.951922	41.776000
3504.684791	504748.803884	41.781005
3504.557823	504690.956804	41.786010
3504.741790	504626.351136	41.791015
3504.901851	504542.375649	41.796020
3504.549992	504502.422520	41.801024
3504.457813	504434.327365	41.806029
3504.641327	504370.628746	41.811034
3504.372194	504317.040233	41.816039
3504.483667	504256.076723	41.821044
3503.974615	504200.708830	41.826048
3504.033252	504143.335185	41.831053
3504.293868	504089.461576	41.836058
3504.437036	504031.418444	41.841063
3504.622314	503966.809607	41.846068
3504.253647	503908.996988	41.851072
3504.419678	503844.491504	41.856077
3504.449380	503785.657779	41.861082
3504.238851	503733.521131	41.866087
3504.267851	503673.476160	41.871092
3504.253461	503632.156284	41.876096
3504.020945	503562.918388	41.881101
3504.136995	503514.615135	41.886106
3504.237471	503460.814549	41.891111
3504.372633	503390.862697	41.896116
3503.907160	503350.419490	41.901120
3504.350449	503293.285334	41.906125
3504.141355	503234.789252	41.911130
3504.009534	503176.179996	41.916135
3504.050617	503115.525348	41.921140
3504.040575	503072.487680	41.926144
3503.424492	503020.916126	41.931149
3503.794230	502973.025690	41.936154
3503.995816	502918.551412	41.941159
3504.058044	502863.594043	41.946164
3503.754801	502824.133255	41.951168
3503.777184	502770.342248	41.956173
3504.134283	502711.957770	41.961178
3504.056805	502660.704774	41.966183
3503.945541	502601.989073	41.971188
3503.855246	502561.535728	41.976192
3503.832304	502510.273713	41.981197
3503.543968	502452.341833	41.986202
3503.462843	502406.638940	41.991207
3503.857280	502359.953641	41.996212
3503.862146	502319.383893	42.001216
3503.803203	502274.686312	42.006221
3503.908000	502221.839164	42.011226
3503.946342	502167.538838	42.016231
3503.897920	502122.738231	42.021236
3503.720157	502072.255652	42.026240
3503.989628	502024.226302	42.031245
3503.689100	501974.973527	42.036250
3503.592982	501916.504988	42.041255
3503.956747	501869.217357	42.046260
3503.887517	501825.024595	42.051264
3503.695687	501759.051667	42.056269
3503.906972	501725.310820	42.061274
3503.847616	501662.243579	42.066279
3503.746618	501615.279750	42.071284
3503.411540	501567.948503	42.076288
3503.635662	501513.768204	42.081293
3503.646237	501471.378569	42.086298
3503.788808	501418.017995	42.091303
3503.707258	501370.545726	42.096308
3504.007481	501314.233425	42.101312
3503.559598	501268.281241	42.106317
3503.477952	501224.492282	42.111322
3503.603781	501188.038495	42.116327
3503.769082	501127.608506	42.121332
3503.293447	501080.448930	42.126336
3503.558651	501043.569386	42.131341
3503.743672	500993.430306	42.136346
3503.504332	500953.550767	42.141351
3503.584783	500901.409093	42.146356
3503.545511	500860.993528	42.151360
3503.614258	500808.701951	42.156365
3503.800694	500767.948219	42.161370
3503.683039	500717.653432	42.166375
3503.447452	500663.289179	42.171380
3503.262486	500631.575582	42.176384
3503.603737	500574.345667	42.181389
3503.776230	500532.685076	42.186394
3503.544682	500482.457665	42.191399
3503.430789	500442.960928	42.196404
3503.366699	500390.234330	42.201408
3503.668677	500346.988624	42.206413
3503.582100	500302.592069	42.211418
3503.459788	500259.866322	42.216423
3503.796660	500209.650450	42.221428
3503.360968	500172.474040	42.226432
3503.380927	500134.873364	42.231437
3503.355702	500080.322802	42.236442
3503.312815	500040.157856	42.241447
3503.382744	499996.846289	42.246452
3503.126142	499954.847084	42.251456
3503.586805	499906.579127	42.256461
3503.171568	499863.393129	42.261466
3503.005756	499814.313939	42.266471
3503.365087	499770.653860	42.271476
3502.983972	499741.239901	42.276480
3503.287287	499701.423894	42.281485
3503.391375	499661.335973	42.286490
3502.923941	499615.230206	42.291495
3503.302794	499573.534767	42.296500
3503.216535	499530.246121	42.301504
3503.462309	499486.855210	42.306509
3503.586542	499446.612159	42.311514
3503.406442	499404.296653	42.316519
3503.783387	499358.563372	42.321524
3503.696243	499319.665065	42.326528
3503.653756	499269.101242	42.331533
3503.603623	499227.723923	42.336538
3503.520679	499178.680174	42.341543
3503.669102	499131.063888	42.346548
3503.553611	499090.402932	42.351552
3503.403206	499033.193023	42.356557
3503.509065	498993.052526	42.361562
3503.459026	498944.507578	42.366567
3503.659291	498890.926904	42.371572
3503.018278	498851.709776	42.376576
3503.409632	498816.420055	42.381581
3503.764930	498772.101505	42.386586
3503.208598	498725.804883	42.391591
3503.738363	498676.310808	42.396596
3503.319513	498627.267013	42.401600
3503.171727	498582.269100	42.406605
3503.619119	498539.601092	42.411610
3503.100164	498494.458779	42.416615
3503.660176	498449.905513	42.421620
3502.946588	498413.625902	42.426624
3503.462738	498374.782626	42.431629
3503.754200	498329.008967	42.436634
3503.031104	498288.187973	42.441639
3503.660542	498232.165884	42.446644
3503.477992	498197.367769	42.451648
3503.055310	498147.263028	42.456653
3503.168421	498111.813021	42.461658
3503.358580	498074.079624	42.466663
3503.249523	498029.275884	42.471668
3503.488131	497981.894208	42.476672
3503.120990	497938.493151	42.481677
3503.339352	497897.575042	42.486682
3503.059001	497856.835374	42.491687
3503.667761	497816.865779	42.496692
3503.206601	497774.791206	42.501696
3503.100469	497732.863167	42.506701
3503.569783	497696.952933	42.511706
3503.216038	497638.103557	42.516711
3503.304257	497590.491649	42.521716
3503.014071	497564.188638	42.526720
3502.950099	497521.698207	42.531725
3502.601669	497478.393831	42.536730
3502.932803	497447.501587	42.541735
3502.994243	497410.695086	42.546740
3502.713216	497380.907482	42.551744
3502.785401	497340.061048	42.556749
3502.592772	497308.846209	42.561754
3502.754465	497276.566638	42.566759
3503.292588	497238.272191	42.571764
3503.117168	497199.684867	42.576768
3502.838625	497157.075344	42.581773
3502.917175	497119.205441	42.586778
3502.625764	497099.716176	42.591783
3503.145382	497058.294567	42.596788
3502.920361	497026.427968	42.601792
3502.909150	496980.495313	42.606797
3503.063326	496948.418105	42.611802
3502.639916	496905.880878	42.616807
3503.078575	496868.459071	42.621812
3502.739420	496841.506178	42.626816
3502.889378	496796.052649	42.631821
3502.721344	496750.547508	42.636826
3503.030396	496730.661446	42.641831
3503.445324	496690.971362	42.646836
3503.423040	496661.949696	42.651840
3503.070632	496603.045504	42.656845
3503.006730	496571.758595	42.661850
3502.905481	496530.533082	42.666855
3503.040286	496486.595329	42.671860
3502.765970	496458.218232	42.676864
3502.711089	496419.357716	42.681869
3502.715015	496385.031097	42.686874
3502.643855	496354.300132	42.691879
3502.780898	496317.226745	42.696884
3502.448065	496288.101232	42.701888
3502.807419	496247.005173	42.706893
3502.986564	496214.720570	42.711898
3502.514341	496174.712834	42.716903
3502.768125	496140.599169	42.721908
3502.903527	496106.806730	42.726912
3502.621933	496076.410816	42.731917
3502.870030	496046.689623	42.736922
3502.934638	496014.018562	42.741927
3503.022579	495957.365388	42.746932
3503.085326	495929.288191	42.751936
3503.270612	495891.701424	42.756941
3503.221392	495860.713615	42.761946
3502.769054	495814.088767	42.766951
3502.926596	495776.152655	42.771956
3502.811294	495742.095508	42.776960
3502.835032	495710.894107	42.781965
3502.746794	495672.440677	42.786970
3502.775504	495655.726676	42.791975
3502.875967	495608.056001	42.796980
3502.763048	495579.702586	42.801985
3502.816620	495537.692986	42.806989
3503.155305	495495.184558	42.811994
3502.817263	495459.899363	42.816999
3502.893078	495423.136166	42.822004
3503.231027	495390.825060	42.827009
3502.849581	495351.608701	42.832013
3503.223551	495305.711881	42.837018
3502.994196	495261.574753	42.842023
3503.104870	495219.656335	42.847028
3502.964016	495189.590087	42.852033
3502.502309	495148.618757	42.857037
3503.033345	495119.255551	42.862042
3502.673741	495095.685071	42.867047
3502.924717	495060.206300	42.872052
3502.328614	495019.306012	42.877057
3502.360704	494992.342465	42.882061
3502.578927	494949.952194	42.887066
3502.389406	494918.630862	42.892071
3502.283725	494887.144964	42.897076
3502.383588	494859.867724	42.902081
3502.413504	494833.762468	42.907085
3502.234319	494814.050789	42.912090
3502.607655	494781.631886	42.917095
3502.531237	494750.948905	42.922100
3502.404556	494724.817341	42.927105
3502.233479	494686.273280	42.932109
3502.385608	494660.905981	42.937114
3502.320879	494628.655885	42.942119
3502.344287	494600.733758	42.947124
3502.490301	494568.400251	42.952129
3502.583400	494542.436109	42.957133
3502.438635	494514.085618	42.962138
3502.626683	494487.551262	42.967143
3502.699235	494450.331798	42.972148
3502.602248	494418.035780	42.977153
3502.613979	494405.614338	42.982157
3502.298926	494366.233589	42.987162
3502.303136	494328.721539	42.992167
3502.433174	494297.803553	42.997172
3502.642083	494274.042330	43.002177
3502.311832	494243.246343	43.007181
3502.677104	494206.889483	43.012186
3502.428690	494185.168271	43.017191
3502.387020	494139.080105	43.022196
3502.738142	494117.063551	43.027201
3502.882081	494088.010991	43.032205
3502.788584	494049.604674	43.037210
3502.438310	494027.444696	43.042215
3502.743994	493988.117817	43.047220
3502.587227	493957.597170	43.052225
3502.630679	493923.612134	43.057229
3502.808601	493885.920477	43.062234
3502.644827	493867.669298	43.067239
3502.578010	493818.655754	43.072244
3502.449305	493789.594553	43.077249
3502.524590	493759.996669	43.082253
3502.552044	493730.961542	43.087258
3502.113868	493710.985776	43.092263
3502.191642	493678.156077	43.097268
3502.423000	493644.393609	43.102273
3502.438590	493626.871555	43.107277
3502.191693	493596.010773	43.112282
3502.233933	493570.557746	43.117287
3502.301614	493543.081153	43.122292
3502.167545	493510.788943	43.127297
3502.369744	493485.613816	43.132301
3502.592812	493464.070632	43.137306
3502.157721	493429.199642	43.142311
3502.098874	493397.400376	43.147316
3502.502216	493368.659481	43.152321
3502.676343	493343.791422	43.157325
3502.583481	493313.713924	43.162330
3502.358317	493291.735344	43.167335
3502.718750	493259.820052	43.172340
3502.529301	493221.376049	43.177345
3502.344591	493194.392504	43.182349
3502.159841	493156.149564	43.187354
3502.199780	493137.916284	43.192359
3502.567570	493095.648952	43.197364
3502.595486	493066.561974	43.202369
3502.308129	493049.439822	43.207373
3502.433864	493019.277226	43.212378
3502.172515	492997.253354	43.217383
3502.433227	492959.748448	43.222388
3502.406426	492930.164810	43.227393
3502.720329	492904.062484	43.232397
3502.810272	492874.814009	43.237402
3502.469296	492847.147277	43.242407
3502.631723	492819.503141	43.247412
3502.553877	492780.333759	43.252417
3501.999707	492754.164288	43.257421
3502.420223	492719.865387	43.262426
3502.869267	492700.053158	43.267431
3502.638034	492664.037840	43.272436
3502.343117	492626.265120	43.277441
3502.546587	492593.312502	43.282445
3502.804941	492562.269982	43.287450
3502.355980	492535.073909	43.292455
3502.694154	492498.818111	43.297460
3502.360498	492468.725896	43.302465
3502.693083	492448.880966	43.307469
3503.078558	492413.122529	43.312474
3502.375681	492391.216967	43.317479
3502.673896	492348.503924	43.322484
3502.657609	492317.958076	43.327489
3502.627995	492280.042214	43.332493
3502.635004	492245.655100	43.337498
3502.105998	492218.016466	43.342503
3502.303723	492194.809120	43.347508
3502.566083	492160.988000	43.352513
3502.412185	492132.583926	43.357517
3502.644866	492106.644338	43.362522
3502.255289	492079.337209	43.367527
3502.868330	492042.128647	43.372532
3502.527397	492003.907076	43.377537
3502.635491	491972.381780	43.382541
3502.665112	491932.032094	43.387546
3502.627753	491916.586558	43.392551
3502.474300	491876.820653	43.397556
3502.627466	491849.378155	43.402561
3502.704651	491813.363300	43.407565
3502.520357	491774.207862	43.412570
3502.353818	491744.037695	43.417575
3502.323505	491724.096798	43.422580
3502.382403	491701.970696	43.427585
3502.375877	491675.461647	43.432589
3502.796100	491646.108893	43.437594
3502.465947	491614.247081	43.442599
3502.262912	491574.185119	43.447604
3502.426697	491542.953233	43.452609
3502.058009	491527.962824	43.457613
3502.453562	491485.131197	43.462618
3502.214820	491456.284586	43.467623
3502.206696	491432.098178	43.472628
3502.383931	491410.609684	43.477633
3502.036797	491379.557958	43.482637
3502.389891	491357.082592	43.487642
3502.299461	491329.121593	43.492647
3501.977861	491301.095523	43.497652
3502.111548	491267.241927	43.502657
3502.189154	491251.323349	43.507661
3502.508352	491213.754499	43.512666
3502.461786	491189.674678	43.517671
3502.610071	491161.524732	43.522676
3502.452275	491136.553188	43.527681
3502.465325	491103.172471	43.532685
3502.467530	491067.924964	43.537690
3502.138627	491047.524664	43.542695
3502.197872	491023.832093	43.547700
3502.083508	490990.521452	43.552705
3502.120394	490972.286025	43.557709
3502.150143	490947.385979	43.562714
3502.208117	490931.470119	43.567719
3501.944801	490888.082858	43.572724
3502.200462	490866.783379	43.577729
3501.996711	490845.605860	43.582733
3502.138673	490810.033015	43.587738
3502.054978	490799.138389	43.592743
3502.089926	490776.055190	43.597748
3502.108328	490753.782506	43.602753
3502.147373	490723.376313	43.607757
3502.128101	490688.333258	43.612762
3502.137143	490679.545058	43.617767
3502.226226	490648.524944	43.622772
3502.191552	490622.472916	43.627777
3502.198460	490600.504789	43.632781
3501.953527	490577.060848	43.637786
3501.851500	490546.120762	43.642791
3502.067650	490522.705985	43.647796
3502.280452	490504.240623	43.652801
3502.161460	490479.312454	43.657805
3502.315290	490451.412821	43.662810
3502.229162	490425.317961	43.667815
3502.095796	490396.856925	43.672820
3502.360475	490376.716846	43.677825
3502.102713	490359.738525	43.682829
3502.571866	490329.365611	43.687834
3502.020659	490310.362404	43.692839
3501.686244	490280.922437	43.697844
3502.133049	490254.239351	43.702849
3502.067716	490235.412942	43.707853
3502.022308	490202.039335	43.712858
3502.222029	490184.434124	43.717863
3502.448567	490160.310167	43.722868
3502.312210	490123.870014	43.727873
3502.395364	490102.091302	43.732877
3502.628381	490076.350183	43.737882
3502.249861	490051.360694	43.742887
3502.096916	490016.690393	43.747892
3502.246726	489989.851056	43.752897
3502.257779	489956.973133	43.757901
3502.346234	489930.698751	43.762906
3502.229114	489905.516841	43.767911
3502.310383	489866.567643	43.772916
3502.176849	489833.206937	43.777921
3502.210533	489818.758234	43.782925
3502.525768	489789.115214	43.787930
3502.501458	489771.998903	43.792935
3502.361231	489732.831321	43.797940
3501.880653	489701.695910	43.802945
3501.888637	489688.917646	43.807949
3502.517900	489658.518478	43.812954
3502.784532	489644.942397	43.817959
3502.274939	489605.528951	43.822964
3502.393552	489586.117588	43.827969
3502.185988	489547.263019	43.832973
3502.389810	489516.222737	43.837978
3502.658815	489488.303413	43.842983
3502.264076	489459.982297	43.847988
3502.506023	489437.319375	43.852993
3502.282133	489404.072793	43.857997
3502.384189	489361.937382	43.863002
3502.252214	489340.292061	43.868007
3502.023246	489323.308098	43.873012
3502.242095	489291.002438	43.878017
3502.004949	489278.160967	43.883021
3501.995526	489239.123268	43.888026
3502.050275	489220.933460	43.893031
3501.988694	489196.347774	43.898036
3502.072679	489169.416226	43.903041
3502.191102	489158.236450	43.908045
3502.265911	489119.993397	43.913050
3501.833635	489098.697486	43.918055
3502.213999	489068.790411	43.923060
3501.976039	489040.999661	43.928065
3501.859283	489019.452523	43.933069
3502.222913	488992.477146	43.938074
3502.115960	488993.200826	43.943079
3502.100890	488960.223805	43.948084
3502.213262	488940.206537	43.953089
3502.198050	488911.875844	43.958093
3502.474999	488879.408757	43.963098
3502.280021	488860.752334	43.968103
3502.201249	488826.926357	43.973108
3502.193843	488805.664929	43.978113
3502.042803	488771.547046	43.983117
3502.122957	488753.150707	43.988122
3501.623800	488731.258627	43.993127
3501.487761	488702.037253	43.998132
3502.373266	488687.858965	44.003137
3502.047025	488663.010571	44.008141
3501.889996	488643.489384	44.013146
3501.979846	488631.000526	44.018151
3501.514938	488598.193733	44.023156
3502.067018	488585.178358	44.028161
3501.947075	488553.428913	44.033165
3501.897454	488531.971650	44.038170
3502.212183	488503.336327	44.043175
3502.008053	488479.428244	44.048180
3502.152441	488464.304451	44.053185
3501.873113	488445.963681	44.058189
3502.133839	488406.679787	44.063194
3501.915765	488387.975872	44.068199
3501.905267	488365.047604	44.073204
3502.396197	488336.485563	44.078209
3501.943335	488324.080906	44.083213
3501.729663	488297.446671	44.088218
3502.109061	488278.195088	44.093223
3501.644863	488247.458203	44.098228
3502.034928	488230.427198	44.103233
3501.506263	488205.609557	44.108237
3501.991123	488188.311219	44.113242
3501.972911	488163.363570	44.118247
3501.779408	488155.716586	44.123252
3502.152925	488126.414817	44.128257
3502.069593	488106.073360	44.133261
3501.928397	488080.185075	44.138266
3501.627967	488063.917930	44.143271
3501.687907	488037.089140	44.148276
3502.217127	488018.318992	44.153281
3501.815338	487993.632785	44.158285
3501.935825	487977.451571	44.163290
3502.007272	487948.550021	44.168295
3502.188096	487932.965463	44.173300
3502.446470	487901.004268	44.178305
3502.036337	487879.046601	44.183309
3501.711136	487855.610953	44.188314
3501.959234	487822.388491	44.193319
3501.723323	487809.697114	44.198324
3502.331338	487786.015123	44.203329
3502.036083	487775.100742	44.208333
3501.974944	487738.289619	44.213338
3501.987881	487719.094360	44.218343
3501.607881	487694.454788	44.223348
3501.992342	487672.928771	44.228353
3502.024452	487657.266057	44.233357
3502.139364	487633.913108	44.238362
3502.179599	487610.723271	44.243367
3501.600588	487586.266019	44.248372
3501.955607	487560.804728	44.253377
3501.584739	487548.437189	44.258381
3501.764735	487522.295943	44.263386
3501.707156	487513.263737	44.268391
3501.807509	487491.983714	44.273396
3502.064944	487464.517079	44.278401
3501.841293	487444.752180	44.283405
3501.782725	487421.122846	44.288410
3501.673105	487412.351227	44.293415
3501.962359	487391.041668	44.298420
3502.363857	487365.976899	44.303425
3502.363718	487335.418513	44.308429
3502.444315	487308.282175	44.313434
3502.461360	487286.105653	44.318439
3502.126377	487252.568612	44.323444
3502.212747	487215.632259	44.328449
3502.139391	487194.530385	44.333453
3501.910384	487162.795025	44.338458
3501.801313	487152.053267	44.343463
3501.550004	487126.534078	44.348468
3501.893559	487108.296816	44.353473
3502.185753	487095.068071	44.358477
3502.176103	487072.188246	44.363482
3502.276167	487043.634113	44.368487
3501.432123	487017.045230	44.373492
3502.188797	486996.167497	44.378497
3501.970192	486975.037413	44.383501
3502.414743	486951.985708	44.388506
3501.556731	486924.540151	44.393511
3501.891499	486908.172931	44.398516
3502.019401	486878.907003	44.403521
3502.198487	486864.180323	44.408525
3501.900597	486834.980569	44.413530
3501.535361	486817.459396	44.418535
3501.402684	486800.710199	44.423540
3501.300643	486780.268869	44.428545
3501.712962	486770.203384	44.433549
3501.861611	486745.682066	44.438554
3501.578295	486735.320714	44.443559
3501.717523	486729.641708	44.448564
3501.779306	486695.637613	44.453569
3501.722718	486682.008182	44.458573
3501.890003	486651.624431	44.463578
3502.239516	486637.174085	44.468583
3501.794051	486618.705440	44.473588
3501.863815	486587.932641	44.478593
3501.975851	486564.224928	44.483597
3501.590691	486545.544762	44.488602
3501.400010	486527.895070	44.493607
3501.402422	486511.427610	44.498612
3501.983765	486493.102105	44.503617
3501.657674	486480.171096	44.508621
3501.791149	486464.188317	44.513626
3502.050163	486435.305244	44.518631
3502.065863	486424.543561	44.523636
3501.929653	486389.559345	44.528641
3501.792395	486377.609122	44.533645
3501.098899	486345.691789	44.538650
3501.731081	486337.359764	44.543655
3501.742551	486327.204828	44.548660
3501.890957	486297.934605	44.553665
3501.637500	486292.417571	44.558669
3501.450170	486263.704660	44.563674
3501.469188	486241.071703	44.568679
3501.444905	486233.498451	44.573684
3502.326249	486212.802314	44.578689
3502.160620	486218.334031	44.583693
3502.097908	486180.307094	44.588698
3502.178754	486155.290253	44.593703
3501.963973	486130.875025	44.598708
3502.182479	486113.211697	44.603713
3502.212969	486093.809621	44.608717
3502.137668	486063.512974	44.613722
3502.104369	486045.181556	44.618727
3501.972810	486017.469787	44.623732
3502.149193	485985.466855	44.628737
3502.140261	485965.515096	44.633741
3502.261672	485939.632850	44.638746
3502.229389	485916.653800	44.643751
3502.265603	485891.037302	44.648756
3502.601699	485864.161745	44.653761
3502.005295	485836.976619	44.658765
3501.929709	485806.376422	44.663770
3502.169606	485790.426899	44.668775
3501.831956	485763.100346	44.673780
3502.384825	485739.777401	44.678785
3502.210649	485716.163438	44.683789
3502.051265	485677.796700	44.688794
3502.340527	485657.343503	44.693799
3502.336726	485634.107024	44.698804
3502.335235	485591.421695	44.703809
3502.278178	485576.983111	44.708813
3502.262112	485553.849451	44.713818
3502.264930	485526.974655	44.718823
3501.994000	485505.800179	44.723828
3501.953975	485467.767956	44.728833
3502.316521	485456.042339	44.733837
3501.957036	485422.656666	44.738842
3501.905330	485400.134514	44.743847
3501.863607	485387.309883	44.748852
3502.179667	485361.244829	44.753857
3501.734075	485339.541626	44.758861
3502.137453	485318.565060	44.763866
3501.993885	485284.337227	44.768871
3502.327071	485265.897339	44.773876
3502.252797	485238.781455	44.778881
3502.330766	485213.409919	44.783885
3502.140330	485181.310854	44.788890
3502.300869	485160.927550	44.793895
3502.152020	485133.772570	44.798900
3502.150331	485098.461391	44.803905
3501.788739	485071.036304	44.808909
3501.857728	485052.283653	44.813914
3502.240730	485034.542979	44.818919
3501.591953	485020.499057	44.823924
3501.810987	484985.203789	44.828929
3501.829654	484966.761970	44.833933
3502.018075	484954.305307	44.838938
3502.159277	484928.973983	44.843943
3502.334018	484900.252709	44.848948
3502.399603	484876.094974	44.853953
3502.003376	484849.887312	44.858957
3502.046741	484823.055501	44.863962
3501.909523	484803.172723	44.868967
3502.323230	484777.243047	44.873972
3501.920576	484756.037523	44.878977
3502.097257	484735.651147	44.883981
3502.068191	484710.598553	44.888986
3502.333365	484691.208717	44.893991
3502.016508	484658.067351	44.898996
3502.096695	484640.474386	44.904001
3501.769816	484615.164870	44.909005
3501.814641	484588.029313	44.914010
3501.960268	484560.827504	44.919015
3501.700734	484552.633291	44.924020
3502.115125	484528.824887	44.929025
3502.073353	484519.586390	44.934029
3502.266079	484483.687847	44.939034
3501.745693	484463.258029	44.944039
3501.807395	484438.140351	44.949044
3502.223188	484413.270648	44.954049
3501.723690	484389.452685	44.959053
3502.085179	484377.221224	44.964058
3501.960006	484355.062621	44.969063
3501.672753	484333.383883	44.974068
3501.988468	484302.770341	44.979073
3502.090367	484294.974425	44.984077
3502.255372	484255.189648	44.989082
3501.956884	484234.169278	44.994087
3501.503919	484208.019878	44.999092
3502.074338	484194.088601	45.004097
3501.673677	484184.602632	45.009101
3501.622736	484171.020627	45.014106
3501.840382	484141.988152	45.019111
3501.875788	484127.584348	45.024116
3501.455762	484106.229076	45.029121
3501.186529	484085.153431	45.034125
3501.268410	484077.259480	45.039130
3501.313270	484054.417222	45.044135
3501.105900	484048.336485	45.049140
3501.362359	484027.178957	45.054145
3501.561236	484026.087054	45.059149
3501.428955	484000.695731	45.064154
3501.641034	483988.032529	45.069159
3501.515794	483993.053546	45.074164
3501.527705	483954.100153	45.079169
3501.230733	483952.731758	45.084173
3501.079350	483935.881322	45.089178
3501.486866	483922.328799	45.094183
3501.248844	483905.138165	45.099188
3501.391644	483887.079914	45.104193
3501.403119	483883.895278	45.109197
3501.319170	483863.043105	45.114202
3501.626889	483846.676862	45.119207
3501.499553	483846.292484	45.124212
3501.361179	483813.020496	45.129217
3501.610744	483799.542967	45.134221
3501.528880	483798.949427	45.139226
3501.662024	483767.049686	45.144231
3501.645690	483758.413035	45.149236
3501.502135	483732.012598	45.154241
3501.070698	483711.668989	45.159245
3501.121653	483700.192624	45.164250
3501.755495	483704.236742	45.169255
3501.441941	483682.813797	45.174260
3501.901434	483654.298518	45.179265
3501.524790	483650.871099	45.184269
3501.382397	483631.745452	45.189274
3501.737310	483609.106902	45.194279
3501.671495	483599.972643	45.199284
3501.959879	483582.143994	45.204289
3501.605705	483554.715068	45.209293
3501.449875	483533.671550	45.214298
3501.769384	483525.134075	45.219303
3501.710177	483508.016220	45.224308
3501.532046	483483.591111	45.229313
3501.667669	483476.395806	45.234317
3501.329592	483469.122644	45.239322
3501.775554	483452.835521	45.244327
3501.521269	483433.272339	45.249332
3501.619688	483410.622892	45.254337
3501.767732	483396.908200	45.259341
3501.498941	483373.204343	45.264346
3501.532175	483363.145123	45.269351
3501.506365	483347.284963	45.274356
3501.651028	483324.628195	45.279361
3501.968519	483314.019481	45.284365
3501.290095	483279.011564	45.289370
3501.449024	483262.718386	45.294375
3501.149881	483265.695251	45.299380
3501.504169	483245.178239	45.304385
3501.559151	483220.413303	45.309389
3501.351723	483223.173812	45.314394
3501.540624	483200.156316	45.319399
3501.326953	483185.739877	45.324404
3501.503258	483182.681019	45.329409
3501.532297	483154.838092	45.334413
3501.456510	483143.835750	45.339418
3501.594420	483133.810617	45.344423
3501.338935	483114.904027	45.349428
3501.684363	483099.895270	45.354433
3501.466465	483093.057942	45.359437
3501.368144	483068.670287	45.364442
3501.806594	483063.044426	45.369447
3501.726736	483040.119041	45.374452
3501.792050	483017.373127	45.379457
3501.867969	482998.717969	45.384461
3501.648627	482984.302226	45.389466
3501.952047	482969.552501	45.394471
3501.968811	482947.066660	45.399476
3501.668270	482925.792219	45.404481
3501.662373	482903.259316	45.409485
3501.787432	482874.440986	45.414490
3501.841258	482862.458315	45.419495
3501.156291	482850.135879	45.424500
3501.518874	482840.075596	45.429505
3501.666983	482831.463366	45.434509
3501.750863	482800.377706	45.439514
3501.962710	482790.795569	45.444519
3501.930447	482766.902408	45.449524
3502.310077	482744.561908	45.454529
3502.440198	482723.068600	45.459533
3502.016507	482692.465908	45.464538
3502.292290	482661.451160	45.469543
3502.236239	482644.129765	45.474548
3502.039116	482609.702273	45.479553
3502.246626	482586.984130	45.484557
3502.326529	482569.085718	45.489562
3502.048536	482536.742188	45.494567
3502.194297	482510.143084	45.499572
3502.507268	482489.378884	45.504577
3502.346882	482459.997902	45.509581
3501.912515	482432.427902	45.514586
3502.471160	482406.269630	45.519591
3502.157280	482388.988074	45.524596
3502.076790	482354.238713	45.529601
3501.811656	482331.947432	45.534605
3502.233373	482306.568193	45.539610
3502.143863	482276.771628	45.544615
3501.947821	482265.484223	45.549620
3502.126804	482230.896317	45.554625
3502.117707	482206.038692	45.559629
3501.952333	482188.380119	45.564634
3502.048196	482160.373443	45.569639
3501.687060	482138.147351	45.574644
3502.055609	482123.134061	45.579649
3502.085702	482101.908100	45.584653
3502.020547	482085.345406	45.589658
3502.384783	482053.658840	45.594663
3502.401426	482028.796929	45.599668
3501.822423	482000.844457	45.604673
3502.000904	481974.239352	45.609677
3501.846177	481956.225169	45.614682
3501.784211	481930.667953	45.619687
3501.668003	481915.881482	45.624692
3501.854038	481887.253956	45.629697
3502.113137	481872.156404	45.634701
3501.966561	481856.161941	45.639706
3501.834160	481828.392302	45.644711
3501.661028	481809.673427	45.649716
3501.904528	481778.661955	45.654721
3501.909529	481761.380611	45.659725
3501.818553	481744.114183	45.664730
3502.023238	481711.340139	45.669735
3501.804758	481702.177998	45.674740
3501.833131	481680.901206	45.679745
3502.170220	481652.906614	45.684749
3501.667707	481646.466638	45.689754
3502.189089	481613.693637	45.694759
3501.892646	481604.290929	45.699764
3501.945861	481569.973779	45.704769
3502.035293	481553.083295	45.709773
3501.807587	481525.732180	45.714778
3502.073321	481502.599177	45.719783
3501.842215	481480.301387	45.724788
3502.032197	481454.249428	45.729793
3502.107291	481425.031977	45.734797
3501.915314	481411.722162	45.739802
3501.885911	481389.089681	45.744807
3502.007692	481377.297416	45.749812
3501.942135	481338.854851	45.754817
3501.919979	481304.346732	45.759821
3501.655135	481236.981556	45.764826
3501.712674	481118.985478	45.769831
3501.441851	480956.269635	45.774836
3500.890831	480761.558997	45.779841
3500.543345	480498.293048	45.784845
3500.332117	480204.176440	45.789850
3500.064043	479856.244530	45.794855
3499.451934	479469.648519	45.799860
3498.629179	479027.131823	45.804865
3498.608300	478546.877601	45.809869
3497.276822	478020.821575	45.814874
3496.910147	477450.475181	45.819879
3495.631656	476835.923581	45.824884
3494.860183	476192.306825	45.829889
3494.143704	475489.312578	45.834893
3492.882834	474740.118929	45.839898
3492.025037	473952.508870	45.844903
3490.925850	473137.345480	45.849908
3489.877546	472270.159798	45.854913
3488.754690	471362.794418	45.859917
3487.189205	470413.378698	45.864922
3486.158506	469421.197216	45.869927
3484.938651	468399.958460	45.874932
3483.466757	467332.371120	45.879937
3482.211825	466224.321611	45.884941
3480.296256	465074.117925	45.889946
3479.175324	463888.303493	45.894951
3477.148840	462671.283973	45.899956
3475.793258	461414.004963	45.904961
3474.033002	460119.104601	45.909965
3472.148734	458812.336484	45.914970
3470.530612	457446.982351	45.919975
3468.621709	456039.562835	45.924980
3466.861771	454601.185003	45.929985
3465.009513	453141.648245	45.934989
3462.657092	451654.127384	45.939994
3460.476453	450123.172770	45.944999
3458.494115	448574.235871	45.950004
3456.800278	447003.957262	45.955009
3454.373682	445383.375285	45.960013
3451.735733	443746.883164	45.965018
3449.917838	442078.667770	45.970023
3447.608013	440387.029997	45.975028
3445.077267	438673.340887	45.980033
3442.908633	436926.258588	45.985037
3440.525000	435159.240446	45.990042
3437.794956	433346.461689	45.995047
3435.533985	431535.772048	46.000052
3432.549614	429686.816569	46.005057
3430.283917	427835.194632	46.010061
3427.737144	425953.691327	46.015066
3425.215557	424035.003257	46.020071
3422.520875	422112.055144	46.025076
3419.749407	420164.906687	46.030081
3417.065063	418190.130072	46.035085
3414.241512	416204.388092	46.040090
3411.519716	414187.913460	46.045095
3408.358687	412177.201581	46.050100
3405.728603	410125.792414	46.055105
3402.924463	408061.637572	46.060109
3399.720906	405982.081802	46.065114
3396.992191	403880.695250	46.070119
3393.806697	401767.057707	46.075124
3390.861055	399642.937476	46.080129
3388.188943	397492.392090	46.085133
3384.714668	395337.765757	46.090138
3381.845764	393156.504995	46.095143
3378.534750	390983.442644	46.100148
3375.644883	388782.502354	46.105153
3372.373455	386559.364360	46.110157
3368.827735	384340.135780	46.115162
3365.928089	382098.192446	46.120167
3362.410038	379857.980302	46.125172
3359.216160	377599.850899	46.130177
3355.992221	375334.017414	46.135181
3352.838444	373051.803343	46.140186
3349.403025	370769.952419	46.145191
3346.256233	368468.003697	46.150196
3342.786656	366151.106589	46.155201
3339.397414	363832.360036	46.160205
3335.871283	361512.156280	46.165210
3332.548793	359181.423285	46.170215
3328.879578	356834.884753	46.175220
3325.997009	354477.904908	46.180225
3322.419259	352123.119894	46.185229
3318.799081	349753.170891	46.190234
3315.330302	347383.027286	46.195239
3311.686452	345003.310573	46.200244
3308.449867	342619.703273	46.205249
3305.121174	340222.673790	46.210253
3301.241518	337829.790001	46.215258
3297.985346	335413.585254	46.220263
3293.974113	333015.907199	46.225268
3290.575512	330598.270551	46.230273
3286.707525	328179.437441	46.235277
3283.113282	325759.651627	46.240282
3279.601303	323336.733016	46.245287
3275.867108	320923.681354	46.250292
3272.108650	318487.930322	46.255297
3268.461768	316055.767291	46.260301
3264.780653	313626.939198	46.265306
3261.086635	311189.283439	46.270311
3257.278465	308744.930124	46.275316
3253.504470	306307.372100	46.280321
3250.069144	303858.242499	46.285325
3246.125858	301425.187837	46.290330
3242.503809	298977.083839	46.295335
3238.461550	296539.475506	46.300340
3234.639450	294106.031736	46.305345
3231.200365	291656.748651	46.310349
3226.916165	289219.439409	46.315354
3222.935020	286778.146635	46.320359
3219.330082	284343.300015	46.325364
3215.337310	281919.630809	46.330369
3211.508580	279488.624669	46.335373
3207.772775	277066.208517	46.340378
3203.995968	274619.765672	46.345383
3199.817748	272202.162587	46.350388
3196.109761	269780.524059	46.355393
3192.547205	267359.971068	46.360397
3188.416592	264948.894094	46.365402
3184.553848	262532.652192	46.370407
3180.129859	260121.920165	46.375412
3176.224518	257709.505154	46.380417
3172.376406	255315.218728	46.385421
3167.985366	252916.009324	46.390426
3164.467431	250519.223462	46.395431
3160.765629	248136.005608	46.400436
3156.632653	245755.141337	46.405441
3152.840157	243368.313225	46.410445
3148.540819	240996.794987	46.415450
3144.540957	238640.362974	46.420455
3140.475216	236286.215900	46.425460
3136.195264	233921.976751	46.430465
3133.073430	231581.767203	46.435469
3128.616615	229247.029685	46.440474
3124.750379	226903.103152	46.445479
3120.555561	224587.216712	46.450484
3116.089376	222273.768121	46.455489
3112.023588	219952.773900	46.460493
3107.771048	217661.716832	46.465498
3103.939992	215367.879407	46.470503
3100.062590	213094.717568	46.475508
3095.411389	210827.116904	46.480513
3091.430647	208568.777489	46.485517
3087.227227	206317.395959	46.490522
3083.132872	204082.244415	46.495527
3079.235972	201845.789791	46.500532
3074.762772	199636.932927	46.505537
3070.724470	197417.470926	46.510541
3065.933521	195232.896040	46.515546
3061.993883	193055.049126	46.520551
3057.746066	190879.452655	46.525556
3053.180679	188729.283456	46.530561
3049.481610	186584.394288	46.535565
3044.763352	184462.064983	46.540570
3040.158432	182345.671012	46.545575
3036.016827	180252.168874	46.550580
3031.127250	178180.143639	46.555585
3026.944493	176114.652897	46.560589
3022.137445	174085.223520	46.565594
3017.838648	172052.240912	46.570599
3013.524979	170053.608757	46.575604
3008.859859	168074.370724	46.580609
3003.871142	166110.194931	46.585613
2998.941990	164176.831299	46.590618
2994.575865	162258.112086	46.595623
2990.097812	160369.530767	46.600628
2984.889546	158506.447893	46.605633
2980.428298	156663.974749	46.610637
2974.816081	154852.740407	46.615642
2970.351470	153061.059323	46.620647
2964.998799	151236.740798	46.625652
2959.793351	149522.739062	46.630657
2954.202906	147833.755087	46.635661
2948.184013	146200.231856	46.640666
2942.342216	144617.312095	46.645671
2936.081595	143071.546567	46.650676
2929.078925	141592.946872	46.655681
2922.757281	140174.517568	46.660685
2916.010716	138811.655097	46.665690
2909.652790	137496.277182	46.670695
2903.714975	136247.089598	46.675700
2897.410000	135037.074508	46.680705
2891.884766	133879.001101	46.685709
2885.901559	132775.666143	46.690714
2880.582273	131713.229185	46.695719
2875.609683	130690.553891	46.700724
2870.409943	129714.748525	46.705729
2865.696417	128773.437124	46.710733
2861.116515	127865.018907	46.715738
2856.475098	126976.421367	46.720743
2851.686513	126127.714703	46.725748
2847.723080	125310.859618	46.730753
2843.780164	124500.949408	46.735757
2839.179740	123720.727889	46.740762
2835.164778	122962.280154	46.745767
2831.494264	122222.590288	46.750772
2827.185044	121494.154338	46.755777
2823.570713	120775.390771	46.760781
2819.831647	120074.196853	46.765786
2816.315133	119379.097891	46.770791
2812.288885	118702.453752	46.775796
2809.013494	118032.915033	46.780801
2805.220848	117367.347119	46.785805
2801.095871	116716.580564	46.790810
2797.413419	116069.049880	46.795815
2793.797063	115429.378429	46.800820
2790.031210	114802.087934	46.805825
2786.508827	114172.875726	46.810829
2782.906353	113581.462853	46.815834
2779.022363	112964.101849	46.820839
2775.524496	112377.511256	46.825844
2771.461476	111783.999912	46.830849
2767.841268	111198.223259	46.835853
2763.362071	110624.159567	46.840858
2759.914905	110055.780175	46.845863
2755.849025	109500.804541	46.850868
2751.936394	108953.136706	46.855873
2748.697924	108398.698215	46.860877
2745.109603	107875.126313	46.865882
2741.374563	107331.511876	46.870887
2737.148254	106808.030070	46.875892
2733.513782	106290.324545	46.880897
2730.072372	105767.995075	46.885901
2726.561868	105259.756479	46.890906
2722.779440	104743.889985	46.895911
2719.677807	104237.319275	46.900916
2716.104367	103738.939480	46.905921
2712.821825	103227.848875	46.910925
2709.135695	102719.714332	46.915930
2705.784771	102219.683024	46.920935
2702.227262	101712.548137	46.925940
2698.738364	101211.638494	46.930945
2695.418951	100705.410031	46.935949
2691.473377	100218.300994	46.940954
2688.418325	99709.060100	46.945959
2685.332144	99209.199040	46.950964
2681.491619	98719.109562	46.955969
2677.885030	98213.778311	46.960973
2674.683595	97718.101679	46.965978
2671.408614	97200.280141	46.970983
2668.333954	96706.594885	46.975988
2664.704717	96202.773441	46.980993
2661.756765	95688.624005	46.985997
2658.150840	95177.508252	46.991002
2654.583975	94663.090807	46.996007
2651.406436	94147.337855	47.001012
2647.687290	93632.948536	47.006017
2644.501256	93108.370014	47.011021
2640.991285	92590.089965	47.016026
2637.912469	92066.643547	47.021031
2634.218585	91548.282790	47.026036
2630.504052	91023.606428	47.031041
2627.228871	90493.839250	47.036045
2623.738756	89970.353404	47.041050
2620.430840	89442.045667	47.046055
2616.810554	88915.218907	47.051060
2613.378424	88389.884128	47.056065
2609.865660	87853.174961	47.061069
2606.333621	87332.575360	47.066074
2603.235431	86799.543380	47.071079
2599.720840	86266.001532	47.076084
2596.220128	85741.296551	47.081089
2592.641774	85190.570527	47.086093
2589.758038	84657.925578	47.091098
2586.248067	84116.521082	47.096103
2582.336663	83574.287373	47.101108
2579.204013	83036.325225	47.106113
2575.823305	82492.860856	47.111117
2572.068714	81949.922378	47.116122
2568.759834	81392.393868	47.121127
2565.463802	80850.954858	47.126132
2562.425263	80305.015306	47.131137
2559.391020	79743.641013	47.136141
2555.418303	79183.681506	47.141146
2552.106993	78617.724545	47.146151
2548.130482	78055.680168	47.151156
2544.609855	77496.802208	47.156161
2541.501492	76938.887503	47.161165
2538.002437	76383.546859	47.166170
2534.270570	75814.474891	47.171175
2530.919686	75242.510986	47.176180
2527.327896	74686.457660	47.181185
2523.995127	74121.473783	47.186189
2520.523814	73555.571020	47.191194
2516.826360	72983.023560	47.196199
2513.470838	72414.028726	47.201204
2509.988478	71847.186367	47.206209
2506.481293	71268.081783	47.211213
2503.157441	70698.166778	47.216218
2499.233327	70133.201414	47.221223
2495.981943	69550.501881	47.226228
2492.518953	68984.626352	47.231233
2489.162641	68411.592465	47.236237
2485.495150	67831.998988	47.241242
2481.425235	67260.917269	47.246247
2477.967034	66688.178924	47.251252
2474.841710	66123.069282	47.256257
2471.409519	65546.709194	47.261261
2468.079884	64976.185602	47.266266
2464.671888	64404.176543	47.271271
2461.377754	63825.359018	47.276276
2457.732368	63241.265659	47.281281
2454.296927	62659.901348	47.286285
2450.973044	62075.461643	47.291290
2447.625918	61493.387450	47.296295
2444.027232	60910.560193	47.301300
2439.999037	60328.556071	47.306305
2436.880424	59742.654854	47.311309
2433.616225	59167.857092	47.316314
2429.955300	58575.177026	47.321319
2426.814056	57986.745386	47.326324
2422.833435	57397.081818	47.331329
2419.113493	56808.807072	47.336333
2416.071785	56218.131697	47.341338
2412.338527	55631.613761	47.346343
2408.577616	55037.672465	47.351348
2404.823756	54455.367812	47.356353
2402.128178	53858.061036	47.361357
2398.642838	53282.322480	47.366362
2395.231445	52698.015948	47.371367
2391.567270	52092.556280	47.376372
2387.850778	51503.423429	47.381377
2384.891017	50898.633743	47.386381
2380.956641	50308.911782	47.391386
2377.861302	49711.018626	47.396391
2374.713979	49113.142764	47.401396
2371.211798	48510.567989	47.406401
2367.476872	47896.698486	47.411405
2364.404421	47305.955629	47.416410
2360.434363	46693.531543	47.421415
2357.062085	46088.356109	47.426420
2353.559160	45479.278958	47.431425
2350.020395	44884.359608	47.436429
2346.465346	44273.592063	47.441434
2343.092704	43670.099107	47.446439
2339.651853	43057.495492	47.451444
2335.967701	42451.313082	47.456449
2332.705858	41840.757148	47.461453
2329.265791	41227.849128	47.466458
2325.357156	40618.512106	47.471463
2322.137508	40003.708272	47.476468
2318.372676	39397.483416	47.481473
2315.072331	38783.950300	47.486477
2311.449302	38182.650856	47.491482
2307.852846	37576.026106	47.496487
2304.519834	36947.595228	47.501492
2301.399491	36342.104083	47.506497
2297.813543	35720.499943	47.511501
2294.433827	35110.006602	47.516506
2290.844422	34502.092615	47.521511
2287.350058	33881.928995	47.526516
2283.765803	33262.697670	47.531521
2279.986815	32641.740244	47.536525
2276.896191	32030.536955	47.541530
2273.026058	31413.616801	47.546535
2269.465624	30794.112723	47.551540
2265.575909	30186.770144	47.556545
2262.450318	29571.468388	47.561549
2258.987622	28962.302000	47.566554
2255.004376	28350.078973	47.571559
2251.904516	27727.015222	47.576564
2248.030784	27114.457351	47.581569
2244.538401	26502.390841	47.586573
2240.670026	25898.929666	47.591578
2237.108357	25302.237178	47.596583
2233.840228	24686.617366	47.601588
2230.295837	24099.398048	47.606593
2226.553683	23491.054170	47.611597
2222.892570	22894.081409	47.616602
2219.157418	22293.267456	47.621607
2215.730169	21698.049024	47.626612
2212.178547	21115.600285	47.631617
2208.157376	20519.325269	47.636621
2204.285539	19942.528975	47.641626
2199.945175	19375.481889	47.646631
2196.539579	18813.056134	47.651636
2192.422719	18245.101391	47.656641
2188.569352	17699.599582	47.661645
2184.244039	17156.463387	47.666650
2179.432083	16637.781559	47.671655
2175.151890	16124.369587	47.676660
2170.459493	15642.499759	47.681665
2166.230679	15148.442979	47.686669
2162.003345	14695.356932	47.691674
2157.243764	14249.754267	47.696679
2152.509905	13837.395503	47.701684
2147.598082	13440.358897	47.706689
2142.872182	13057.155864	47.711693
2138.493241	12698.277597	47.716698
2134.258657	12354.449872	47.721703
2130.154275	12019.323534	47.726708
2126.116134	11703.446767	47.731713
2122.366307	11396.995793	47.736717
2118.452916	11109.939382	47.741722
2114.822300	10827.762665	47.746727
2111.152167	10532.525899	47.751732
2107.248582	10270.469515	47.756737
2103.830252	10001.019642	47.761741
2100.291670	9735.352863	47.766746
2096.962606	9478.121403	47.771751
2093.441148	9223.484176	47.776756
2089.784102	8980.807741	47.781761
2086.628919	8740.715162	47.786765
2083.311174	8492.048043	47.791770
2080.116332	8249.657428	47.796775
2076.717874	7987.301461	47.801780
2073.032838	7753.602701	47.806785
2069.787138	7513.692081	47.811789
2066.521285	7262.678687	47.816794
2062.770244	7030.635672	47.821799
2059.676877	6789.856259	47.826804
2056.038321	6547.813467	47.831809
2052.945298	6298.767550	47.836813
2049.289050	6063.788254	47.841818
2045.887873	5825.253114	47.846823
2042.385134	5580.024616	47.851828
2038.612557	5343.490360	47.856833
2035.325584	5107.187401	47.861837
2032.084099	4872.212709	47.866842
2028.714583	4632.412946	47.871847
2025.163916	4389.296534	47.876852
2021.923868	4167.365196	47.881857
2018.346753	3920.259350	47.886861
2015.111318	3686.729378	47.891866
2011.349718	3447.028478	47.896871
2007.847858	3203.869769	47.901876
2004.309159	2975.221699	47.906881
2000.712527	2741.393126	47.911885
1997.002788	2509.306487	47.916890
1993.454592	2270.616377	47.921895
1990.053944	2045.935913	47.926900
1986.660021	1828.262359	47.931905
1982.746547	1607.362784	47.936909
1979.304575	1383.915188	47.941914
1974.851012	1166.025443	47.946919
1971.504411	953.752792	47.951924
1967.300750	746.124512	47.956929
1963.735712	554.300496	47.961933
1959.803102	364.785190	47.966938
1955.198846	202.530745	47.971943
1949.439994	71.284652	47.976948
1938.416489	101.407257	47.981953
1931.054076	109.190564	47.986957
1926.614752	103.753340	47.991962
1923.819689	104.697686	47.996967
1921.746066	103.834000	48.001972
1919.049949	106.876310	48.006977
1916.572016	102.317054	48.011981
1913.921913	107.769282	48.016986
1910.790398	101.508430	48.021991
1907.176219	94.303986	48.026996
1903.797194	110.471267	48.032001
1900.905778	110.079705	48.037005
1897.246481	99.588854	48.042010
1893.598574	101.048745	48.047015
1890.150251	100.104789	48.052020
1887.228280	100.214687	48.057025
1884.090109	98.982018	48.062029
1880.011934	101.163765	48.067034
1876.743756	101.953961	48.072039
1873.912652	97.598372	48.077044
1869.915612	98.793068	48.082049
1866.654106	99.098179	48.087053
1863.672026	91.203750	48.092058
1860.447107	91.617060	48.097063
1856.626150	84.109457	48.102068
1853.436780	97.108806	48.107073
1849.601366	96.282046	48.112077
1846.211794	98.644521	48.117082
1842.596424	102.541739	48.122087
1839.382561	96.198804	48.127092
1835.806586	95.920117	48.132097
1832.636497	90.883313	48.137101
1829.323437	96.438719	48.142106
1824.905646	102.415999	48.147111
1821.663467	95.742120	48.152116
1818.745881	98.942286	48.157121
1815.524447	97.665635	48.162125
1812.073751	91.074832	48.167130
1808.107418	101.107327	48.172135
1804.885104	91.975320	48.177140
1801.686716	95.190717	48.182145
1797.862403	97.412052	48.187149
1794.031945	90.450092	48.192154
1791.048777	95.887718	48.197159
1787.590902	90.633122	48.202164
1784.119722	100.430366	48.207169
1780.731350	96.034972	48.212173
1777.302137	96.049820	48.217178
1773.936955	93.049179	48.222183
1770.672045	90.627709	48.227188
1766.934844	96.138401	48.232193
1763.212341	89.675329	48.237197
1759.637867	86.849631	48.242202
1755.807170	96.468714	48.247207
1753.037867	92.828011	48.252212
1749.437735	92.825171	48.257217
1745.913807	95.278165	48.262221
1742.365561	95.485546	48.267226
1738.893688	96.073341	48.272231
1736.023179	86.535421	48.277236
1732.158459	87.272943	48.282241
1728.400517	98.478376	48.287245
1724.967604	98.977852	48.292250
1721.183595	88.240699	48.297255
1718.028149	93.284366	48.302260
1714.518615	93.514199	48.307265
1711.263190	89.117105	48.312269
1707.935170	86.968053	48.317274
1703.859184	96.419673	48.322279
1700.624977	89.678134	48.327284
1697.018683	89.556038	48.332289
1693.277626	93.327294	48.337293
1689.983168	91.609611	48.342298
1686.453472	93.357999	48.347303
1683.160673	90.270174	48.352308
1679.908878	93.857715	48.357313
1676.370715	99.919556	48.362317
1672.759101	96.160026	48.367322
1669.202401	94.173117	48.372327
1665.928314	89.206303	48.377332
1662.242392	96.597751	48.382337
1658.567490	106.274849	48.387341
1655.285286	96.275838	48.392346
1651.718044	102.579484	48.397351
1648.180562	96.147741	48.402356
1644.555593	93.295114	48.407361
1641.471777	93.496657	48.412365
1638.315120	89.561920	48.417370
1634.388053	91.628420	48.422375
1630.379624	91.977037	48.427380
1627.038986	90.450043	48.432385
1623.973697	92.565910	48.437389
1620.527250	89.900633	48.442394
1616.944731	87.351446	48.447399
1613.767416	90.927398	48.452404
1609.773641	85.661326	48.457409
1606.507581	88.985339	48.462413
1602.843965	91.893512	48.467418
1599.395629	90.253571	48.472423
1595.809987	89.071593	48.477428
1592.285330	86.114777	48.482433
1588.340357	89.462204	48.487437
1585.461265	85.291287	48.492442
1582.041492	91.461250	48.497447
1578.664637	86.624337	48.502452
1575.375518	85.225370	48.507457
1571.540314	89.938252	48.512461
1568.382075	88.284799	48.517466
1564.087391	94.518174	48.522471
1560.718829	92.685490	48.527476
1557.132697	94.259178	48.532481
1553.782672	96.172598	48.537485
1550.900599	83.384222	48.542490
1546.926932	89.997895	48.547495
1543.509594	82.212391	48.552500
1540.345592	96.830761	48.557505
1536.173766	87.802295	48.562509
1532.953373	81.140890	48.567514
1529.139004	88.941468	48.572519
1526.001565	83.690818	48.577524
1522.780705	79.579432	48.582529
1518.957294	85.546469	48.587533
1515.462947	82.888661	48.592538
1512.191557	90.794549	48.597543
1508.717717	83.618948	48.602548
1504.875787	80.088277	48.607553
1501.156186	86.763646	48.612557
1497.759366	89.111453	48.617562
1494.193112	93.273123	48.622567
1491.399533	91.233896	48.627572
1487.933532	93.260283	48.632577
1483.750869	89.472604	48.637581
1480.423937	90.325759	48.642586
1476.861444	92.746809	48.647591
1473.135607	83.554030	48.652596
1469.870619	84.318452	48.657601
1466.517836	90.275516	48.662605
1463.308215	80.657550	48.667610
1458.950952	89.102604	48.672615
1455.799861	77.909499	48.677620
1452.593530	88.810775	48.682625
1449.057215	80.844492	48.687629
1445.619295	80.364026	48.692634
1441.914326	85.815932	48.697639
1438.462582	83.442562	48.702644
1434.838665	71.630209	48.707649
1431.885146	88.984042	48.712653
1428.624325	81.433619	48.717658
1424.600660	78.839227	48.722663
1421.283355	84.369998	48.727668
1417.474787	95.070791	48.732673
1413.753738	87.525563	48.737677
1410.586088	73.297896	48.742682
1407.031150	81.592760	48.747687
1403.460837	85.808850	48.752692
1400.045879	76.317768	48.757697
1396.050206	70.213650	48.762701
1392.564279	76.912760	48.767706
1389.490548	88.663413	48.772711
1386.181230	87.122079	48.777716
1382.532160	87.775450	48.782721
1378.885921	78.149531	48.787725
1375.837643	82.119855	48.792730
1372.289102	87.889097	48.797735
1368.668647	84.444192	48.802740
1365.188762	81.717714	48.807745
1361.643100	82.098733	48.812749
1357.843212	75.502246	48.817754
1354.186408	83.145428	48.822759
1350.769021	74.553224	48.827764
1347.636909	76.625726	48.832769
1343.653358	84.136272	48.837773
1340.689499	83.382716	48.842778
1336.958191	88.370502	48.847783
1333.655004	81.016510	48.852788
1329.708071	81.403044	48.857793
1326.399334	91.855198	48.862797
1323.215794	78.047627	48.867802
1319.578882	83.378218	48.872807
1315.964096	76.939584	48.877812
1312.275661	84.644638	48.882817
1308.759030	90.481682	48.887821
1305.406552	85.580903	48.892826
1301.958797	84.156037	48.897831
1298.616703	85.451322	48.902836
1295.449151	81.942260	48.907841
1291.457812	83.775191	48.912845
1287.449723	76.138630	48.917850
1283.936688	83.835366	48.922855
1280.831432	86.432030	48.927860
1277.411022	79.020366	48.932865
1273.959487	86.536691	48.937869
1270.632995	81.264884	48.942874
1266.948052	82.335132	48.947879
1263.314636	86.133954	48.952884
1260.244159	78.879792	48.957889
1256.437781	85.170055	48.962893
1253.069802	81.518192	48.967898
1249.426287	89.194113	48.972903
1245.857660	80.894379	48.977908
1242.405456	81.333629	48.982913
1239.086003	87.595556	48.987917
1235.613312	77.929996	48.992922
1231.776321	82.124332	48.997927
1228.601061	81.027213	49.002932
1225.232640	77.027418	49.007937
1221.428274	79.742396	49.012941
1217.872220	78.321743	49.017946
1214.234817	88.834546	49.022951
1210.881379	80.349466	49.027956
1207.921024	79.478321	49.032961
1204.225254	89.819879	49.037965
1200.126211	79.150854	49.042970
1196.468697	91.292926	49.047975
1193.627106	93.421458	49.052980
1190.068151	81.535765	49.057985
1186.336906	81.578701	49.062989
1182.949727	82.447587	49.067994
1178.888072	89.245817	49.072999
1175.733021	88.180357	49.078004
1172.349014	82.629621	49.083009
1168.974691	84.546854	49.088013
1166.263060	85.706051	49.093018
1162.259217	89.182899	49.098023
1158.183933	92.174167	49.103028
1155.024373	78.793163	49.108033
1151.197681	88.281921	49.113037
1147.931792	78.751863	49.118042
1144.333738	85.908193	49.123047
1140.632648	82.921953	49.128052
1137.238519	74.224929	49.133057
1133.560327	95.516449	49.138061
1130.317387	79.013209	49.143066
1126.990734	86.108313	49.148071
1123.253815	89.483505	49.153076
1120.231320	74.543622	49.158081
1116.434382	87.463516	49.163085
1113.034605	83.120610	49.168090
1109.690267	89.959046	49.173095
1106.112331	85.387613	49.178100
1102.249427	84.267833	49.183105
1098.639387	92.033462	49.188109
1095.357526	81.680175	49.193114
1091.139614	84.813871	49.198119
1088.002272	80.800270	49.203124
1085.133826	82.815933	49.208129
1081.287266	77.818094	49.213133
1078.031112	78.226843	49.218138
1074.611486	78.689512	49.223143
1071.217619	73.415570	49.228148
1067.814606	73.195461	49.233153
1063.727083	86.815470	49.238157
1060.225529	78.442058	49.243162
1056.764453	77.544468	49.248167
1052.839043	86.159600	49.253172
1050.017166	76.592084	49.258177
1046.306172	86.107128	49.263181
1042.894424	72.752752	49.268186
1039.674491	75.186954	49.273191
1035.681288	87.817867	49.278196
1032.320340	77.030826	49.283201
1028.810261	81.633027	49.288205
1025.252721	79.630511	49.293210
1021.373048	91.465488	49.298215
1017.729796	82.838897	49.303220
1014.334104	72.800737	49.308225
1011.188043	77.422203	49.313229
1008.012439	72.750198	49.318234
1004.255631	79.833171	49.323239
1000.540349	79.370618	49.328244
997.415882	74.826692	49.333249
993.795049	79.079147	49.338253
990.400900	82.268120	49.343258
987.115068	83.823589	49.348263
983.621489	82.412223	49.353268
979.801346	78.416340	49.358273
976.305426	88.400935	49.363277
972.943140	74.959783	49.368282
969.551516	79.831444	49.373287
965.688437	78.281448	49.378292
962.136616	79.995380	49.383297
958.217318	78.359227	49.388301
954.888663	77.918752	49.393306
951.676598	72.603875	49.398311
948.271815	81.264516	49.403316
945.309842	82.298187	49.408321
941.564389	76.335528	49.413325
937.751794	79.083452	49.418330
934.109164	74.408227	49.423335
930.455893	78.662573	49.428340
927.395330	75.067306	49.433345
923.951653	74.948453	49.438349
920.285001	79.214375	49.443354
916.679426	78.551261	49.448359
912.741965	79.290704	49.453364
909.822002	69.244951	49.458369
905.711831	73.889953	49.463373
902.450344	73.869290	49.468378
899.524403	75.650313	49.473383
895.799981	74.967739	49.478388
892.829135	79.375281	49.483393
888.809402	75.581322	49.488397
885.168149	74.670673	49.493402
881.684771	65.022671	49.498407
878.014766	74.531336	49.503412
874.545329	69.962036	49.508417
870.866551	76.621592	49.513421
867.410639	76.235737	49.518426
864.228858	71.697590	49.523431
860.757351	80.352801	49.528436
857.209454	71.920208	49.533441
853.852967	73.701818	49.538445
850.159931	64.453447	49.543450
846.963111	69.886398	49.548455
843.040904	82.885902	49.553460
839.716961	73.415562	49.558465
835.930010	81.689619	49.563469
832.482439	83.475920	49.568474
829.150175	85.835880	49.573479
825.670999	74.475679	49.578484
822.006115	77.093056	49.583489
818.681493	82.590199	49.588493
815.674091	70.757939	49.593498
811.996498	68.182534	49.598503
808.210308	86.311338	49.603508
804.264178	73.818468	49.608513
800.350161	78.141889	49.613517
797.517079	73.160337	49.618522
794.241554	74.638291	49.623527
790.898632	90.129188	49.628532
787.306939	74.123245	49.633537
783.453356	74.397241	49.638541
779.924873	81.517451	49.643546
776.760783	80.741339	49.648551
772.889512	81.742573	49.653556
769.875670	82.240182	49.658561
766.078076	85.849474	49.663565
762.806792	78.161593	49.668570
759.478119	79.543423	49.673575
755.703463	88.859588	49.678580
752.620397	80.794402	49.683585
748.353603	74.833843	49.688589
744.735543	77.402812	49.693594
741.501891	80.101761	49.698599
737.552919	77.881815	49.703604
733.973600	81.640625	49.708609
731.000428	72.084066	49.713613
728.071399	81.420447	49.718618
724.748541	75.562881	49.723623
720.504300	69.775984	49.728628
716.835188	79.135826	49.733633
713.162297	85.006723	49.738637
710.147964	76.475278	49.743642
706.782924	76.888363	49.748647
703.142995	76.980417	49.753652
699.913882	76.470695	49.758657
695.724851	79.150698	49.763661
692.126480	79.954439	49.768666
689.185256	80.643228	49.773671
685.558091	80.148017	49.778676
682.180049	74.077592	49.783681
678.514977	82.364322	49.788685
675.103186	80.611242	49.793690
671.625145	71.528748	49.798695
667.780967	75.974184	49.803700
664.337400	75.159337	49.808705
660.837881	79.532139	49.813709
657.301741	85.258369	49.818714
653.705281	81.272010	49.823719
649.548448	80.621983	49.828724
647.056195	64.853048	49.833729
643.729031	74.843013	49.838733
640.311861	72.154329	49.843738
636.838029	70.066073	49.848743
633.114599	82.617033	49.853748
629.741775	83.809603	49.858753
626.038076	76.508594	49.863757
622.740947	73.345656	49.868762
618.620293	70.845580	49.873767
615.352324	79.671593	49.878772
611.755535	79.377303	49.883777
608.270419	80.444991	49.888781
604.836620	71.194276	49.893786
601.465314	66.018138	49.898791
597.756599	88.295108	49.903796
594.533337	72.864597	49.908801
591.233431	83.185675	49.913805
587.289881	75.263968	49.918810
584.116870	79.364491	49.923815
580.142768	82.548874	49.928820
576.886259	71.878549	49.933825
573.325693	65.001351	49.938829
569.665853	78.032779	49.943834
566.312435	70.300778	49.948839
562.571642	79.627496	49.953844
559.466034	72.401069	49.958849
556.029858	77.988359	49.963853
552.954977	76.973767	49.968858
549.256007	71.054564	49.973863
545.409009	78.385721	49.978868
541.938671	78.454559	49.983873
538.178232	70.640398	49.988877
534.864491	69.270697	49.993882
531.556718	70.899229	49.998887
527.542755	82.460901	50.003892
524.227711	69.661057	50.008897
520.667940	73.628809	50.013901
517.066717	80.504103	50.018906
513.839785	72.701801	50.023911
510.231930	77.195882	50.028916
506.762990	73.778141	50.033921
503.149153	74.173036	50.038925
499.637735	74.128056	50.043930
496.465270	65.570655	50.048935
493.215489	70.853692	50.053940
489.588613	74.414289	50.058945
485.721681	79.274564	50.063949
482.226705	77.895121	50.068954
478.643098	75.861941	50.073959
474.928842	82.482760	50.078964
471.995503	79.250554	50.083969
468.602074	81.860511	50.088973
464.907998	73.197660	50.093978
461.534452	77.304101	50.098983
457.464985	82.907736	50.103988
454.339638	71.887996	50.108993
450.925132	76.247581	50.113997
447.335725	68.061974	50.119002
444.192963	66.213264	50.124007
439.956445	75.107811	50.129012
436.652821	73.353745	50.134017
433.454301	76.221256	50.139021
430.155378	73.229464	50.144026
426.491607	64.239213	50.149031
422.315210	75.177622	50.154036
418.827269	69.292029	50.159041
415.350025	78.204413	50.164045
412.347125	76.330769	50.169050
409.151865	69.823825	50.174055
405.569310	72.010827	50.179060
401.883463	73.100299	50.184065
398.249096	70.337901	50.189069
394.801679	73.136599	50.194074
391.116153	72.274039	50.199079
387.778186	75.814980	50.204084
384.469935	70.483534	50.209089
380.850086	70.028355	50.214093
377.051712	75.153206	50.219098
373.740812	68.613654	50.224103
369.984417	69.261709	50.229108
366.658864	67.583832	50.234113
362.818701	72.057147	50.239117
359.347500	70.876496	50.244122
356.560201	62.132613	50.249127
352.794705	69.625096	50.254132
349.310937	66.462784	50.259137
345.676257	71.220478	50.264141
341.929662	78.675222	50.269146
338.506839	71.403310	50.274151
335.070950	75.361286	50.279156
331.994830	79.687185	50.284161
328.026524	76.135250	50.289165
324.615789	65.134664	50.294170
321.175427	65.224174	50.299175
317.748015	66.573971	50.304180
314.095481	62.080729	50.309185
310.549716	71.427714	50.314189
307.120944	67.715860	50.319194
303.726196	63.884819	50.324199
300.088515	73.125897	50.329204
296.415587	64.165574	50.334209
293.255999	61.566553	50.339213
289.815121	65.512654	50.344218
286.228837	70.101471	50.349223
282.587652	71.127060	50.354228
279.044597	63.971956	50.359233
275.569316	69.647612	50.364237
271.545576	77.575767	50.369242
268.086729	65.883514	50.374247
264.874399	78.082837	50.379252
262.057189	66.012288	50.384257
258.139600	59.345758	50.389261
254.666787	58.257120	50.394266
251.090865	63.369495	50.399271
247.328905	70.013575	50.404276
244.190633	70.780543	50.409281
240.574027	74.203532	50.414285
236.990535	66.874401	50.419290
233.779210	63.078089	50.424295
229.839896	65.826841	50.429300
226.294681	63.632707	50.434305
223.040389	66.765177	50.439309
219.670422	71.003958	50.444314
216.757057	67.034712	50.449319
212.503112	77.551789	50.454324
208.958894	73.997125	50.459329
205.372261	73.261563	50.464333
201.847293	64.496518	50.469338
198.777919	63.620316	50.474343
194.993949	69.989425	50.479348
191.484725	62.496888	50.484353
187.792224	67.418618	50.489357
184.309976	62.633140	50.494362
181.274006	60.479949	50.499367
177.641095	66.910959	50.504372
174.241576	66.861258	50.509377
170.593723	63.126591	50.514381
167.095358	62.674677	50.519386
163.444792	68.282723	50.524391
159.800535	69.128478	50.529396
156.523822	66.807133	50.534401
153.020579	70.402301	50.539405
149.268682	61.584018	50.544410
145.908494	62.768351	50.549415
142.640766	68.462323	50.554420
139.386672	64.577775	50.559425
135.668970	70.866972	50.564429
132.023192	75.158195	50.569434
128.496729	61.341035	50.574439
124.647312	63.724639	50.579444
121.205991	55.035176	50.584449
117.836376	67.904370	50.589453
114.189257	62.904136	50.594458
110.958864	58.237645	50.599463
107.497357	69.400118	50.604468
103.927109	57.238051	50.609473
100.434486	65.295492	50.614477
97.031233	63.000185	50.619482
93.912143	59.429974	50.624487
89.849190	71.666824	50.629492
86.646019	63.095306	50.634497
82.602071	69.349884	50.639501
78.975573	73.736184	50.644506
76.110488	68.538270	50.649511
72.390767	63.087454	50.654516
69.187138	69.087819	50.659521
65.717389	64.373181	50.664525
61.502228	72.327994	50.669530
58.493869	60.391656	50.674535
54.739620	65.746944	50.679540
51.643584	63.084283	50.684545
48.080059	52.408106	50.689549
44.531190	61.622714	50.694554
40.947802	55.150965	50.699559
37.335633	63.090986	50.704564
33.907743	53.804684	50.709569
30.421556	56.669568	50.714573
26.785620	64.328562	50.719578
23.462870	56.617210	50.724583
19.649663	60.839602	50.729588
16.536351	60.008230	50.734593
12.775544	62.548890	50.739597
9.335585	63.065476	50.744602
5.686864	55.101170	50.749607
2.534036	60.483043	50.754612